Wed Jun 15 16:44:35 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.255444	116.301861	0.000000
1.182636	101.157828	0.005005
1.017413	80.403099	0.010010
1.149445	85.441765	0.015014
1.146356	90.493588	0.020019
0.971822	58.296891	0.025024
0.206680	62.177839	0.030029
0.121582	50.962587	0.035034
-0.193887	22.481768	0.040038
-0.274182	22.832446	0.045043
-0.844049	6.463495	0.050048
-0.944832	15.822224	0.055053
-1.421954	-5.336291	0.060058
-1.347909	-17.830984	0.065062
-2.158612	-1.429643	0.070067
-2.687962	-16.263830	0.075072
-2.757568	-23.482501	0.080077
-3.065356	-19.522577	0.085082
-2.879011	-26.839179	0.090086
-3.446420	-18.177132	0.095091
-4.026107	-18.053379	0.100096
-4.749035	-23.808006	0.105101
-4.834150	-11.040922	0.110106
-4.355280	-16.073597	0.115110
-4.866824	-3.265433	0.120115
-4.638579	-3.811234	0.125120
-4.766720	-14.315193	0.130125
-5.467261	-22.050177	0.135130
-5.780103	-29.904962	0.140134
-6.140654	-6.987915	0.145139
-5.988552	-7.456422	0.150144
-6.898179	-35.624782	0.155149
-7.651979	-29.714032	0.160154
-7.508417	-10.219344	0.165158
-7.271423	-4.865323	0.170163
-7.703097	-24.918599	0.175168
-8.034155	-20.815246	0.180173
-8.269150	-13.441887	0.185178
-8.018597	-22.885639	0.190182
-8.442776	-19.481681	0.195187
-8.398291	-6.992193	0.200192
-9.444864	-6.483213	0.205197
-9.840675	-21.785339	0.210202
-9.196060	-35.901041	0.215206
-9.716651	-9.362423	0.220211
-9.599723	-9.234626	0.225216
-9.959767	-10.707937	0.230221
-10.873559	-2.512940	0.235226
-10.809826	-15.676817	0.240230
-11.363795	-19.991917	0.245235
-11.300681	-32.217166	0.250240
-11.364074	-17.548738	0.255245
-12.063243	-3.048873	0.260250
-12.321174	-31.811454	0.265254
-12.596210	-10.066839	0.270259
-12.322450	-24.344204	0.275264
-12.550435	-21.196988	0.280269
-12.798136	-8.934635	0.285274
-13.468361	-11.774221	0.290278
-14.265873	-16.550095	0.295283
-14.093500	-24.751014	0.300288
-14.293484	-19.638379	0.305293
-14.263695	-8.836063	0.310298
-14.110400	-21.980604	0.315302
-14.586551	-22.198108	0.320307
-15.280251	-19.477711	0.325312
-15.627331	-11.833297	0.330317
-16.101453	-23.420808	0.335322
-15.786499	-21.564521	0.340326
-15.955413	-19.773773	0.345331
-16.247011	-30.089521	0.350336
-16.210797	-29.021414	0.355341
-17.068205	-24.138095	0.360346
-17.496542	-26.214087	0.365350
-17.597105	-17.175519	0.370355
-17.843477	-27.352451	0.375360
-17.628895	-26.703273	0.380365
-17.913746	-7.319095	0.385370
-17.900780	-11.584161	0.390374
-18.833006	-16.907744	0.395379
-19.159276	-17.152582	0.400384
-19.144811	-12.193166	0.405389
-19.366263	-17.652558	0.410394
-19.092319	-6.997818	0.415398
-19.941809	-5.147866	0.420403
-20.380456	-16.499957	0.425408
-20.566389	-16.378732	0.430413
-20.716668	-8.009538	0.435418
-20.755163	-18.607321	0.440422
-21.069170	-6.451989	0.445427
-21.227689	2.267875	0.450432
-21.149864	-20.435372	0.455437
-21.898018	-33.840505	0.460442
-22.419418	-25.498377	0.465446
-22.631337	-10.908582	0.470451
-22.556419	-26.335448	0.475456
-22.569357	-23.922969	0.480461
-22.967366	-18.923110	0.485466
-23.328504	-21.887066	0.490470
-23.780460	-25.194293	0.495475
-23.640374	-17.700034	0.500480
-23.938331	-21.871493	0.505485
-24.728834	-10.048474	0.510490
-24.926770	1.239923	0.515494
-25.527860	-7.606761	0.520499
-25.005856	-28.269329	0.525504
-25.447749	-24.464608	0.530509
-25.615811	-1.279584	0.535514
-25.749371	-6.740582	0.540518
-25.707223	-15.307168	0.545523
-25.973901	-40.361287	0.550528
-26.912581	-22.745410	0.555533
-27.121913	-23.243855	0.560538
-27.091499	-43.409175	0.565542
-27.303109	-21.615873	0.570547
-27.194320	-19.392687	0.575552
-28.020568	-11.183258	0.580557
-28.622364	-30.439564	0.585562
-28.506340	-28.642933	0.590566
-28.811759	-9.041398	0.595571
-28.691119	-12.322513	0.600576
-28.738412	-25.233058	0.605581
-29.423730	-29.056598	0.610586
-30.030251	-20.709870	0.615590
-30.302116	-2.771411	0.620595
-30.588286	-14.565970	0.625600
-30.575655	-28.860644	0.630605
-31.201385	-22.695538	0.635610
-30.837162	-14.747164	0.640614
-30.891903	-24.035009	0.645619
-31.072879	-3.307675	0.650624
-31.134848	-3.240081	0.655629
-31.860945	-9.444502	0.660634
-32.113438	-24.045162	0.665638
-32.451812	-23.152591	0.670643
-32.371557	-35.816186	0.675648
-32.911010	-23.061234	0.680653
-33.622356	-16.480786	0.685658
-33.761675	-26.297596	0.690662
-34.034542	-4.275846	0.695667
-34.114212	-18.257662	0.700672
-34.279144	-23.432132	0.705677
-34.385245	-13.331915	0.710682
-34.056370	-10.588147	0.715686
-34.568483	-0.613676	0.720691
-34.806663	-26.038105	0.725696
-35.154004	-20.174004	0.730701
-35.694983	-14.993078	0.735706
-35.574331	-20.215238	0.740710
-36.794824	-5.626361	0.745715
-37.051618	-13.698159	0.750720
-36.772502	-24.974232	0.755725
-36.954282	-13.556825	0.760730
-37.127419	-7.572158	0.765734
-37.295228	-20.835077	0.770739
-37.783159	-31.840951	0.775744
-37.699570	-24.652039	0.780749
-38.206092	-17.705533	0.785754
-38.315829	-31.467912	0.790758
-38.687209	-7.049477	0.795763
-38.753345	-6.731226	0.800768
-38.732219	-15.697501	0.805773
-39.331756	-24.587734	0.810778
-39.708284	-27.488576	0.815782
-40.195307	-16.870853	0.820787
-40.421231	-4.018252	0.825792
-40.083104	-9.563019	0.830797
-40.353037	-15.600647	0.835802
-40.586869	-32.913085	0.840806
-41.545388	-8.743669	0.845811
-41.707809	-5.896218	0.850816
-41.845930	-15.282546	0.855821
-42.309027	-21.111871	0.860826
-42.107601	-17.498298	0.865830
-42.313657	-19.738671	0.870835
-42.251730	-27.944713	0.875840
-42.997730	-7.750902	0.880845
-43.371405	-7.300049	0.885850
-43.318982	-24.734872	0.890854
-43.699255	-31.845374	0.895859
-43.647978	-17.532381	0.900864
-44.008292	-6.670531	0.905869
-44.988360	-16.872110	0.910874
-44.883807	-38.579971	0.915878
-45.152631	-14.358426	0.920883
-44.993154	-12.323742	0.925888
-45.268680	2.257239	0.930893
-45.338181	-6.688736	0.935898
-45.520032	-21.331651	0.940902
-46.626040	-6.727071	0.945907
-46.759505	7.808934	0.950912
-46.675068	-22.054792	0.955917
-47.012094	-12.306160	0.960922
-46.902885	-12.653643	0.965926
-47.320492	7.440540	0.970931
-48.100563	1.706205	0.975936
-47.930511	-21.546638	0.980941
-48.570797	-13.344661	0.985946
-48.212474	-12.797860	0.990950
-48.556278	7.545339	0.995955
-48.713369	-9.805847	1.000960
-49.297482	-22.536231	1.005965
-49.926155	-17.553690	1.010970
-49.926669	-17.360318	1.015974
-50.166200	-17.396649	1.020979
-50.056179	-19.297832	1.025984
-50.216047	-33.715412	1.030989
-50.579763	-8.740508	1.035994
-50.294912	-8.943304	1.040998
-51.241550	-4.289278	1.046003
-51.652547	-10.796427	1.051008
-51.969223	-21.648508	1.056013
-51.595884	-14.491891	1.061018
-51.482640	-19.681852	1.066022
-52.671360	-21.771268	1.071027
-53.175831	-18.501809	1.076032
-53.034454	-17.152286	1.081037
-53.351786	2.684426	1.086042
-53.339788	-15.760759	1.091046
-53.504168	-25.572241	1.096051
-53.838206	-26.716622	1.101056
-54.392884	-17.609421	1.106061
-54.943035	-14.401267	1.111066
-54.959871	-11.827647	1.116070
-55.194817	-20.394403	1.121075
-55.268741	-14.970560	1.126080
-54.833042	-14.510530	1.131085
-55.512306	-12.661086	1.136090
-55.662550	-15.154632	1.141094
-56.500757	-3.621042	1.146099
-56.761681	-21.351017	1.151104
-56.467736	-27.368484	1.156109
-56.648261	-4.092335	1.161114
-57.080464	-1.117436	1.166118
-57.744687	-8.314093	1.171123
-58.268214	-0.094019	1.176128
-58.049685	-13.804322	1.181133
-58.443843	2.089801	1.186138
-58.425175	-6.987343	1.191142
-58.414653	-5.956421	1.196147
-58.907147	-10.911626	1.201152
-59.179636	-28.354695	1.206157
-59.613983	-1.688179	1.211162
-59.649521	-6.852273	1.216166
-59.919509	-24.569796	1.221171
-60.065474	-16.620368	1.226176
-60.231152	-13.919855	1.231181
-61.320779	-3.877268	1.236186
-61.617496	-17.806539	1.241190
-61.520085	-28.067406	1.246195
-61.791847	-6.699373	1.251200
-61.586385	8.641201	1.256205
-62.037917	-9.199435	1.261210
-61.858562	-27.092918	1.266214
-62.052109	-9.619507	1.271219
-62.493607	-3.073981	1.276224
-62.919378	-18.759612	1.281229
-63.549778	-22.258311	1.286234
-63.491318	-15.963607	1.291238
-63.445494	-15.106907	1.296243
-63.482917	-10.710272	1.301248
-64.392793	8.590181	1.306253
-64.569922	-5.832855	1.311258
-64.500830	-0.643646	1.316262
-64.588497	-2.165619	1.321267
-65.304378	-9.900923	1.326272
-66.267133	-16.454689	1.331277
-66.531006	-6.708476	1.336282
-66.193521	4.603297	1.341286
-66.341126	-2.513313	1.346291
-66.513864	-17.838979	1.351296
-66.409958	-9.851235	1.356301
-66.830419	-16.327814	1.361306
-66.768488	-20.084658	1.366310
-67.345272	4.064007	1.371315
-68.286482	-1.915855	1.376320
-68.145684	-10.880896	1.381325
-68.448718	11.914600	1.386330
-68.540518	-2.176098	1.391334
-68.552488	-10.803284	1.396339
-68.624645	-7.408669	1.401344
-69.392929	-17.124197	1.406349
-69.675354	-10.227547	1.411354
-69.666779	-15.505859	1.416358
-69.887213	-20.809554	1.421363
-69.988347	-3.837238	1.426368
-70.357896	-11.780310	1.431373
-70.905562	-9.704718	1.436378
-71.463465	-0.096841	1.441382
-71.371154	0.233992	1.446387
-71.601308	-22.901309	1.451392
-71.789235	-11.693200	1.456397
-71.873498	-0.488504	1.461402
-71.656024	-4.644331	1.466406
-72.629700	-20.774066	1.471411
-73.037869	-21.269932	1.476416
-73.041125	-17.879702	1.481421
-73.695072	7.333179	1.486426
-73.455254	-10.887657	1.491430
-73.378024	-23.143253	1.496435
-74.042793	-18.561855	1.501440
-74.715318	-10.842843	1.506445
-75.092317	-15.143778	1.511450
-74.662432	-26.383899	1.516454
-74.987151	-21.152105	1.521459
-75.033263	-6.139497	1.526464
-74.954324	-6.302049	1.531469
-75.635531	-4.257161	1.536474
-75.919712	-7.771254	1.541478
-76.354833	-8.599738	1.546483
-76.620632	3.769089	1.551488
-76.047977	-14.704039	1.556493
-77.159215	-0.172868	1.561498
-77.424637	-9.761390	1.566502
-77.866146	4.522478	1.571507
-77.973352	-4.731351	1.576512
-77.981309	-14.968597	1.581517
-78.229573	-11.606729	1.586522
-78.088221	-18.550711	1.591526
-79.040991	-10.115088	1.596531
-79.584948	-12.020449	1.601536
-79.767631	-11.937146	1.606541
-80.045581	-8.920661	1.611546
-79.824084	-22.700791	1.616550
-79.576878	-26.591929	1.621555
-79.712486	-17.710241	1.626560
-79.710085	-10.441815	1.631565
-80.660140	-6.107228	1.636570
-80.876350	-4.062541	1.641574
-81.277962	5.647156	1.646579
-81.800059	6.383556	1.651584
-81.724697	-18.368237	1.656589
-82.764163	-21.550939	1.661594
-82.667402	-1.797767	1.666598
-82.505485	-14.368135	1.671603
-83.084798	-3.226536	1.676608
-83.038741	-16.137317	1.681613
-83.105241	0.080757	1.686618
-83.076320	-3.464564	1.691622
-83.370642	12.234123	1.696627
-84.255216	-1.853298	1.701632
-84.456087	-23.041833	1.706637
-84.852955	-7.738753	1.711642
-84.837093	-2.034500	1.716646
-84.548284	-14.067408	1.721651
-84.888024	-29.141928	1.726656
-85.651434	-23.144847	1.731661
-86.448734	5.795754	1.736666
-86.385462	0.315644	1.741670
-87.043796	-13.073360	1.746675
-87.001832	-7.016129	1.751680
-86.524253	-9.168741	1.756685
-86.453075	-14.176851	1.761690
-86.609487	2.931365	1.766694
-87.198879	-4.150009	1.771699
-87.871625	3.982174	1.776704
-87.525876	-2.082138	1.781709
-88.245489	7.158379	1.786714
-88.908119	5.077608	1.791718
-89.124273	-7.309737	1.796723
-89.337209	-24.254819	1.801728
-89.173140	-23.497467	1.806733
-89.238738	4.125932	1.811738
-89.435738	-9.512935	1.816742
-89.949617	-19.273561	1.821747
-90.732587	-9.142764	1.826752
-90.668731	-9.763300	1.831757
-90.966497	-5.105040	1.836762
-90.995159	-10.143310	1.841766
-90.772155	2.501827	1.846771
-91.333000	-12.380208	1.851776
-92.269006	-18.379759	1.856781
-92.691437	-10.918705	1.861786
-92.297555	-2.468099	1.866790
-92.573209	-2.582011	1.871795
-92.869559	-10.278234	1.876800
-92.526774	-12.823865	1.881805
-92.890545	-13.167164	1.886810
-93.501494	-11.174233	1.891814
-94.205981	5.510129	1.896819
-94.321377	-10.470354	1.901824
-94.281643	-7.740655	1.906829
-94.841574	-7.072380	1.911834
-94.592265	-8.437759	1.916838
-94.600628	-1.458259	1.921843
-95.563151	7.212085	1.926848
-95.528033	-11.791798	1.931853
-96.468735	-6.489761	1.936858
-96.550888	-5.807722	1.941862
-96.330240	-14.819791	1.946867
-96.448561	0.764862	1.951872
-95.962585	-0.106452	1.956877
-97.229402	-6.595068	1.961882
-97.633601	-4.717096	1.966886
-97.952637	-1.325674	1.971891
-97.821556	5.033879	1.976896
-97.622000	-12.241587	1.981901
-98.051912	-5.235528	1.986906
-98.228194	-5.882568	1.991910
-98.646868	-15.902780	1.996915
-99.453106	-9.572710	2.006912
-99.023427	-5.981090	2.016909
-98.055978	-7.989807	2.026906
-98.167019	-8.066491	2.036902
-97.024616	-15.320155	2.046899
-96.473399	-12.100348	2.056896
-96.610352	-7.435364	2.066893
-95.970461	-9.132842	2.076890
-95.026775	-16.977505	2.086886
-95.304439	-7.810367	2.096883
-93.984464	-10.826343	2.106880
-93.748002	-11.687419	2.116877
-93.650894	-17.135333	2.126874
-92.362321	-11.864709	2.136870
-91.908114	-8.335319	2.146867
-92.027132	-12.951317	2.156864
-91.343714	-18.888748	2.166861
-91.242197	-16.313973	2.176858
-90.155995	-15.368103	2.186854
-89.212953	-12.598953	2.196851
-89.147135	-21.770324	2.206848
-89.132901	-17.665474	2.216845
-88.707056	-15.895262	2.226842
-87.925711	-7.186619	2.236838
-87.186134	-12.852624	2.246835
-86.296458	-7.507083	2.256832
-86.325083	-5.901577	2.266829
-86.136089	-15.047974	2.276826
-85.140326	-10.942957	2.286822
-85.012619	-24.070977	2.296819
-83.882559	-0.024327	2.306816
-83.658772	-11.064400	2.316813
-83.255044	-7.404682	2.326810
-83.030901	0.833648	2.336806
-81.835220	-15.712867	2.346803
-81.425579	-8.221392	2.356800
-81.196096	-7.112498	2.366797
-81.423883	-13.460459	2.376794
-80.058815	-13.039914	2.386790
-79.828599	-7.604151	2.396787
-79.351002	-12.294256	2.406784
-78.306009	-9.524569	2.416781
-78.082566	-9.804098	2.426778
-77.931184	-18.843628	2.436774
-77.189093	-4.280719	2.446771
-76.560622	-14.453290	2.456768
-76.575351	8.286281	2.466765
-75.773007	-18.252266	2.476762
-75.031961	-4.967388	2.486758
-74.993684	-17.151589	2.496755
-74.042412	-1.792281	2.506752
-73.589254	-12.260246	2.516749
-73.396531	-21.602231	2.526746
-72.669192	-10.866955	2.536742
-71.822819	-5.639497	2.546739
-71.689528	-16.026545	2.556736
-71.734015	-17.881254	2.566733
-70.768963	4.437507	2.576730
-70.096538	-11.564926	2.586726
-69.775218	-15.328602	2.596723
-68.607490	-4.403962	2.606720
-68.965659	-8.215156	2.616717
-68.632110	-11.644636	2.626714
-67.129297	-14.237067	2.636710
-67.143953	-1.836047	2.646707
-67.189491	-16.483988	2.656704
-66.331648	-1.421947	2.666701
-65.631183	-24.081377	2.676698
-65.471525	-9.523158	2.686694
-64.551160	-21.412613	2.696691
-63.886862	-19.630051	2.706688
-63.661744	-21.779010	2.716685
-63.619112	-25.535246	2.726682
-62.629071	-8.402089	2.736678
-62.479589	-18.058532	2.746675
-61.540440	-9.474538	2.756672
-60.977162	-15.403373	2.766669
-60.947412	-5.393746	2.776666
-59.863031	-29.203204	2.786662
-59.388960	-6.409905	2.796659
-59.161201	-16.068816	2.806656
-59.225246	-17.702600	2.816653
-58.021484	-11.716276	2.826650
-57.723313	-9.460141	2.836646
-57.385586	-9.916196	2.846643
-56.120258	-23.987041	2.856640
-56.005014	3.535794	2.866637
-55.901144	-11.166477	2.876634
-55.323583	-16.970059	2.886630
-54.403435	-12.782610	2.896627
-54.177179	-22.391093	2.906624
-53.929971	-11.638987	2.916621
-53.349013	-7.554108	2.926618
-52.741835	-15.700611	2.936614
-52.176613	-12.702090	2.946611
-51.600728	-22.979651	2.956608
-51.315452	-16.513318	2.966605
-50.698922	-12.604798	2.976602
-49.976866	5.644241	2.986598
-49.630977	-12.909531	2.996595
-49.067431	-0.002148	3.006592
-48.444042	-16.703778	3.016589
-48.177536	-13.119461	3.026586
-48.025811	0.378385	3.036582
-46.889995	-19.718066	3.046579
-46.461509	-10.918606	3.056576
-46.426390	-12.555148	3.066573
-45.797122	-20.567710	3.076570
-45.040822	-9.094845	3.086566
-44.624423	-9.466808	3.096563
-43.877636	-9.147053	3.106560
-43.273308	-7.809715	3.116557
-43.190130	-14.806738	3.126554
-43.241352	-10.943923	3.136550
-41.835067	-4.407913	3.146547
-41.428673	-10.708577	3.156544
-41.311804	-7.689295	3.166541
-40.971417	-2.215532	3.176538
-40.410650	-16.704104	3.186534
-39.517024	4.133737	3.196531
-38.709669	-17.585383	3.206528
-38.634456	-1.321927	3.216525
-38.644459	-7.164420	3.226522
-37.690842	-7.190272	3.236518
-37.090425	-11.723082	3.246515
-36.519735	-14.372538	3.256512
-35.539597	-6.607510	3.266509
-35.423377	-13.790056	3.276506
-35.388000	-6.542321	3.286502
-34.883408	-17.736164	3.296499
-34.045908	-8.046900	3.306496
-33.745716	-13.263870	3.316493
-33.239927	-8.360193	3.326490
-32.378833	0.123520	3.336486
-32.116143	-23.402493	3.346483
-31.764215	-9.808743	3.356480
-30.841153	-1.207757	3.366477
-30.598532	-0.716280	3.376474
-30.227585	-21.690243	3.386470
-29.243294	-11.210373	3.396467
-28.645770	-10.674726	3.406464
-28.854393	-4.926815	3.416461
-28.792320	-14.467280	3.426458
-27.647307	-4.821325	3.436454
-27.015481	-18.842794	3.446451
-26.569677	-10.626279	3.456448
-25.720714	-16.003867	3.466445
-25.545010	-10.349597	3.476442
-25.412993	-16.836337	3.486438
-24.417882	-11.197473	3.496435
-23.846378	-5.104479	3.506432
-23.888322	-10.191818	3.516429
-23.204687	-4.851030	3.526426
-22.596932	-14.029498	3.536422
-22.332938	-15.848268	3.546419
-21.304677	-6.694261	3.556416
-20.860188	-16.605400	3.566413
-20.900164	-2.614015	3.576410
-19.946414	-18.357434	3.586406
-19.318458	-4.089839	3.596403
-18.949382	-6.525027	3.606400
-18.987396	-8.296951	3.616397
-17.981013	4.302480	3.626394
-17.416812	-8.881596	3.636390
-17.214417	-9.122778	3.646387
-16.436378	-10.246004	3.656384
-16.079055	-5.414981	3.666381
-16.007323	-11.358591	3.676378
-14.984202	-4.269147	3.686374
-14.630417	-3.986275	3.696371
-14.037015	-15.032120	3.706368
-13.086114	2.696610	3.716365
-12.765754	-5.844009	3.726362
-12.911181	-4.427312	3.736358
-12.530726	-23.763037	3.746355
-11.292812	-5.063016	3.756352
-11.227039	-11.248620	3.766349
-10.538944	-8.429718	3.776346
-9.613527	0.615457	3.786342
-9.329029	-10.175873	3.796339
-9.494928	-21.231946	3.806336
-8.722114	3.201800	3.816333
-8.064323	-19.677470	3.826330
-7.711540	-16.893434	3.836326
-6.468762	-14.783520	3.846323
-6.060705	-15.483012	3.856320
-6.105592	-0.450153	3.866317
-5.974905	-14.172895	3.876314
-5.222955	0.008829	3.886310
-4.712029	-17.450269	3.896307
-4.145247	-4.418862	3.906304
-3.520641	4.782800	3.916301
-3.306358	4.141109	3.926298
-3.046212	3.402351	3.936294
-2.637106	31.504288	3.946291
-1.826112	47.063060	3.956288
-1.570492	50.945708	3.966285
-0.984858	79.239712	3.976282
-0.433732	96.184586	3.986278
-0.005466	116.371743	3.996275
0.000000	129.316643	4.001280
0.480031	140.428988	4.006285
0.586590	155.319763	4.011290
0.719904	153.626109	4.016294
0.527636	159.157961	4.021299
0.932010	180.152329	4.026304
0.894175	183.237090	4.031309
0.942040	181.027229	4.036314
0.732337	183.593889	4.041318
0.959426	182.575656	4.046323
1.014240	176.863183	4.051328
1.138254	183.511936	4.056333
1.140409	194.990477	4.061338
1.138977	194.019379	4.066342
1.124420	205.907781	4.071347
1.465348	196.882906	4.076352
1.731354	207.160998	4.081357
1.047782	209.765625	4.086362
1.198336	206.222348	4.091366
1.584111	205.257005	4.096371
1.374886	225.941677	4.101376
1.655660	222.467730	4.106381
1.399650	219.823033	4.111386
1.242805	183.181153	4.116390
1.122528	200.995689	4.121395
1.444702	217.829552	4.126400
1.587711	216.777368	4.131405
1.540266	218.773380	4.136410
1.512644	222.033926	4.141414
1.572929	231.027417	4.146419
1.817839	199.176412	4.151424
1.636350	193.485719	4.156429
1.121871	205.603423	4.161434
1.838223	201.983218	4.166438
1.647410	186.465074	4.171443
1.200326	183.339589	4.176448
1.470363	212.102066	4.181453
1.435806	223.313715	4.186458
1.933683	216.655772	4.191462
1.846284	210.204444	4.196467
1.881579	210.753541	4.201472
1.597357	208.058265	4.206477
1.214376	206.171840	4.211482
1.475948	204.645499	4.216486
1.205296	199.594664	4.221491
1.362329	224.241034	4.226496
1.597176	233.185159	4.231501
1.168808	227.570666	4.236506
1.595929	211.547038	4.241510
1.537269	213.608726	4.246515
1.140074	231.662679	4.251520
1.525181	232.667032	4.256525
1.314623	233.333900	4.261530
1.882350	227.512872	4.266534
1.899947	252.321323	4.271539
1.930363	251.001568	4.276544
1.766816	237.286206	4.281549
1.884331	226.637018	4.286554
2.111545	244.273411	4.291558
1.744281	239.969207	4.296563
1.946545	243.352267	4.301568
1.762709	249.839240	4.306573
1.552756	237.772838	4.311578
1.819302	217.850967	4.316582
1.723842	250.440529	4.321587
1.511649	230.270444	4.326592
1.821237	236.154719	4.331597
1.768095	252.532845	4.336602
1.977439	236.564809	4.341606
1.895182	236.055022	4.346611
1.735965	240.051326	4.351616
2.004691	274.315267	4.356621
1.962232	282.490027	4.361626
2.518856	271.456813	4.366630
2.388275	256.976796	4.371635
1.968265	258.495273	4.376640
2.259680	251.995138	4.381645
2.074468	246.514173	4.386650
2.295936	233.574774	4.391654
1.886307	251.303494	4.396659
1.999046	245.334706	4.401664
2.108791	236.237824	4.406669
2.055896	259.585629	4.411674
2.342818	239.453894	4.416678
2.212596	238.800511	4.421683
2.249822	240.256645	4.426688
1.867026	253.418211	4.431693
1.902535	262.584402	4.436698
2.506275	263.200752	4.441702
2.336487	271.396251	4.446707
2.321955	276.859808	4.451712
2.320854	264.848146	4.456717
2.183402	253.751093	4.461722
2.281291	253.037127	4.466726
2.444488	268.346387	4.471731
2.288061	263.644510	4.476736
2.255954	258.050147	4.481741
2.071319	262.233549	4.486746
2.713543	270.971679	4.491750
2.410424	292.434106	4.496755
2.295289	275.949568	4.501760
2.703400	284.899125	4.506765
2.356585	271.966993	4.511770
2.355208	237.697134	4.516774
2.443153	253.646802	4.521779
2.072879	289.033722	4.526784
2.534682	287.852400	4.531789
2.252520	278.200554	4.536794
2.668321	277.097367	4.541798
2.490422	294.708728	4.546803
2.439229	277.153063	4.551808
2.277850	265.582403	4.556813
2.195122	285.906807	4.561818
2.507189	284.523636	4.566822
2.221286	280.222548	4.571827
2.371045	290.980590	4.576832
2.557579	298.396107	4.581837
2.317504	284.379453	4.586842
2.546035	278.304708	4.591846
2.552849	275.059704	4.596851
2.312158	295.511239	4.601856
2.645567	285.106689	4.606861
2.303064	290.871363	4.611866
2.740484	291.184435	4.616870
3.138688	316.425007	4.621875
2.801091	313.476032	4.626880
2.881227	293.032738	4.631885
2.680131	295.010253	4.636890
2.436420	280.116932	4.641894
2.508796	283.885475	4.646899
2.890982	302.734745	4.651904
2.775325	311.630793	4.656909
2.596662	322.415509	4.661914
2.863395	312.752444	4.666918
2.906168	309.318303	4.671923
3.154529	316.952178	4.676928
3.244817	288.473652	4.681933
2.527519	296.177032	4.686938
2.629048	298.252607	4.691942
2.877304	286.883939	4.696947
2.881996	302.182335	4.701952
3.235249	315.368317	4.706957
2.527141	308.509416	4.711962
2.771615	307.661922	4.716966
2.860078	317.716299	4.721971
3.161969	307.161671	4.726976
3.444763	292.009290	4.731981
3.172569	290.887214	4.736986
3.192593	289.981815	4.741990
2.809508	296.551847	4.746995
2.827407	286.091614	4.752000
3.161380	269.725228	4.757005
2.803416	277.834240	4.762010
2.873834	292.235912	4.767014
3.107330	300.037569	4.772019
2.869573	295.602942	4.777024
2.762572	293.300379	4.782029
2.907793	319.557695	4.787034
3.206970	320.781047	4.792038
3.056847	310.998059	4.797043
2.903182	299.554735	4.802048
3.140370	326.035788	4.807053
2.832539	334.196326	4.812058
2.887607	307.022184	4.817062
3.002174	310.102403	4.822067
3.171316	316.084396	4.827072
3.073454	290.992850	4.832077
2.978245	320.646379	4.837082
3.239577	325.554653	4.842086
3.136817	315.549967	4.847091
3.199489	304.640480	4.852096
3.022190	313.356424	4.857101
2.844794	340.106170	4.862106
3.384299	339.045671	4.867110
3.268547	335.310999	4.872115
3.434766	344.444985	4.877120
3.274065	361.867038	4.882125
3.020015	361.359099	4.887130
2.967157	345.367891	4.892134
3.263727	344.792044	4.897139
3.083776	356.568802	4.902144
3.140139	336.055689	4.907149
3.413570	355.849299	4.912154
3.413374	354.920208	4.917158
3.337378	351.950092	4.922163
2.897128	337.184094	4.927168
3.416090	349.366306	4.932173
3.324147	359.699116	4.937178
3.755174	365.869674	4.942182
3.593374	377.610401	4.947187
3.537913	387.919246	4.952192
3.473389	358.942845	4.957197
3.339235	378.938692	4.962202
3.564674	355.832568	4.967206
3.686167	355.445857	4.972211
3.544884	367.718153	4.977216
3.511232	378.517319	4.982221
3.757038	374.694675	4.987226
3.470589	379.840080	4.992230
3.771281	396.654410	4.997235
3.739648	378.205098	5.002240
4.000463	369.847989	5.007245
3.407386	358.920954	5.012250
3.434172	371.085376	5.017254
3.648101	374.042253	5.022259
3.592599	372.276691	5.027264
3.558940	372.228333	5.032269
3.333998	387.339155	5.037274
3.774121	383.242118	5.042278
3.492671	372.190378	5.047283
3.452474	366.078129	5.052288
3.707653	369.133347	5.057293
3.719911	381.591683	5.062298
3.802762	380.669583	5.067302
3.961271	370.186943	5.072307
3.403671	375.132016	5.077312
3.853387	375.342931	5.082317
3.867475	378.002461	5.087322
3.858797	384.816072	5.092326
4.008208	379.814927	5.097331
3.679600	378.574418	5.102336
3.832540	380.362630	5.107341
4.096444	378.821780	5.112346
3.973781	375.657933	5.117350
3.990367	394.014022	5.122355
3.845886	393.566894	5.127360
4.067851	370.934536	5.132365
3.871805	372.604332	5.137370
4.158981	375.086347	5.142374
4.275401	393.565229	5.147379
3.985401	381.093970	5.152384
4.227878	362.196303	5.157389
4.121447	367.971121	5.162394
4.165256	379.255067	5.167398
4.212998	378.831121	5.172403
3.980855	359.500105	5.177408
4.127421	362.642916	5.182413
3.850187	377.458040	5.187418
3.916585	367.611120	5.192422
3.878160	385.960507	5.197427
3.777732	368.268454	5.202432
3.861898	372.060323	5.207437
4.104186	396.565133	5.212442
4.112665	390.795919	5.217446
4.048958	406.572328	5.222451
3.858468	422.180103	5.227456
4.307496	409.702407	5.232461
4.330281	422.818697	5.237466
4.294043	423.482611	5.242470
4.186592	415.153880	5.247475
3.948697	412.204490	5.252480
4.446630	419.844427	5.257485
3.876942	422.980133	5.262490
4.378300	401.796771	5.267494
4.167191	401.695859	5.272499
3.930807	410.508335	5.277504
4.211566	397.802760	5.282509
4.416521	408.608782	5.287514
4.145202	425.320966	5.292518
4.013186	420.358225	5.297523
4.128466	397.128683	5.302528
4.258185	417.173900	5.307533
4.368808	437.090604	5.312538
4.551816	432.605640	5.317542
4.554777	443.500803	5.322547
4.419210	446.153410	5.327552
4.695184	434.949629	5.332557
4.315981	449.684900	5.337562
4.491244	440.007573	5.342566
4.823705	433.602284	5.347571
4.746902	413.328692	5.352576
4.571853	422.785471	5.357581
4.493771	425.530183	5.362586
4.682812	413.181864	5.367590
4.596017	403.577558	5.372595
4.057478	422.753837	5.377600
4.463258	414.483628	5.382605
4.734707	429.937043	5.387610
4.571393	446.526145	5.392614
4.557851	430.686286	5.397619
4.509737	438.167678	5.402624
4.740439	431.682432	5.407629
4.545888	444.817788	5.412634
4.568534	449.202855	5.417638
4.871194	435.891084	5.422643
4.562654	440.651684	5.427648
4.844876	436.589013	5.432653
4.661213	464.845681	5.437658
4.453461	457.742539	5.442662
4.885654	452.889370	5.447667
4.425661	453.658037	5.452672
5.059949	428.123583	5.457677
4.697900	439.223188	5.462682
4.394211	446.854050	5.467686
4.592750	445.983558	5.472691
4.739613	446.760749	5.477696
4.929669	441.818763	5.482701
4.717086	446.824334	5.487706
4.546976	422.290925	5.492710
4.811652	434.273637	5.497715
4.547606	449.226042	5.502720
4.780599	445.338319	5.507725
4.709216	441.763990	5.512730
5.258852	450.594865	5.517734
5.200324	454.691780	5.522739
4.948942	465.147191	5.527744
5.058704	446.126734	5.532749
5.199132	446.753168	5.537754
5.007984	433.334388	5.542758
4.844150	457.417014	5.547763
4.972080	455.263035	5.552768
5.233531	442.750018	5.557773
5.116638	430.841015	5.562778
5.141703	439.226066	5.567782
5.218158	441.607964	5.572787
4.902475	458.147384	5.577792
5.149557	437.065576	5.582797
5.134024	442.447578	5.587802
5.271973	439.485791	5.592806
5.158165	454.520308	5.597811
4.818662	449.983579	5.602816
4.997114	436.433480	5.607821
4.858298	449.756926	5.612826
4.910748	457.848817	5.617830
5.119699	460.686084	5.622835
5.044908	460.998968	5.627840
5.566932	454.817548	5.632845
5.312985	470.756072	5.637850
5.196094	474.174168	5.642854
5.222554	452.340793	5.647859
5.110630	454.620451	5.652864
5.609135	458.525680	5.657869
5.109935	459.292343	5.662874
4.997516	468.390966	5.667878
5.252881	473.082852	5.672883
5.090338	494.252231	5.677888
5.724692	476.606033	5.682893
5.379058	466.345241	5.687898
5.002255	465.624675	5.692902
5.162133	481.813064	5.697907
5.278649	486.413369	5.702912
5.250772	474.091377	5.707917
4.967266	463.913938	5.712922
5.539428	485.564042	5.717926
5.436835	472.747739	5.722931
5.274379	466.318374	5.727936
5.472762	466.005863	5.732941
5.066451	471.029941	5.737946
5.389520	474.065181	5.742950
5.300577	466.756349	5.747955
5.099542	469.275851	5.752960
5.684249	482.458650	5.757965
5.627965	501.358627	5.762970
5.691209	521.840636	5.767974
5.815423	502.322306	5.772979
5.465409	480.492804	5.777984
5.654224	483.500119	5.782989
5.346989	481.488484	5.787994
5.584352	490.464012	5.792998
5.671733	499.924625	5.798003
5.656833	502.750652	5.803008
5.837545	486.097139	5.808013
5.681676	507.053042	5.813018
5.635353	491.060700	5.818022
5.853373	491.655274	5.823027
5.559356	490.697192	5.828032
5.748533	486.448444	5.833037
5.752390	499.500649	5.838042
5.652588	493.633674	5.843046
5.928285	498.501650	5.848051
5.459811	511.797256	5.853056
5.903092	501.006640	5.858061
5.508740	501.642631	5.863066
6.086442	496.058782	5.868070
5.999726	502.941868	5.873075
5.756282	517.976365	5.878080
6.230258	509.225465	5.883085
5.715436	492.458809	5.888090
5.509428	487.501565	5.893094
5.839036	510.331377	5.898099
5.707990	509.326830	5.903104
5.971489	508.724086	5.908109
5.877146	510.235332	5.913114
6.038170	495.946123	5.918118
6.035478	496.564051	5.923123
6.065467	513.456883	5.928128
5.986124	515.237133	5.933133
5.895457	508.303727	5.938138
5.737698	498.268353	5.943142
6.017102	517.322011	5.948147
5.828154	518.453013	5.953152
6.100259	501.936891	5.958157
5.894666	491.239898	5.963162
5.942732	486.172797	5.968166
6.082116	509.142853	5.973171
5.656490	517.880418	5.978176
5.968676	507.703552	5.983181
5.781426	496.362011	5.988186
6.062593	508.911260	5.993190
6.097640	493.868872	5.998195
5.906639	505.456882	6.003200
6.269233	492.362346	6.008205
6.119275	500.528647	6.013210
6.127278	515.602481	6.018214
5.995848	518.691925	6.023219
5.929586	501.610232	6.028224
6.096239	501.148086	6.033229
6.088871	527.056109	6.038234
5.914147	528.033632	6.043238
6.458905	533.402882	6.048243
6.257090	516.662308	6.053248
6.115778	521.309472	6.058253
6.128028	500.565783	6.063258
6.135261	494.449393	6.068262
6.060270	517.421248	6.073267
5.890346	522.943421	6.078272
6.417188	507.870652	6.083277
6.443381	523.489383	6.088282
6.275434	519.947568	6.093286
5.990251	509.754985	6.098291
6.167848	503.889713	6.103296
6.367233	512.280919	6.108301
6.039263	495.055344	6.113306
6.317497	491.929494	6.118310
6.384885	506.452319	6.123315
6.135990	505.791012	6.128320
6.565630	499.702478	6.133325
6.388792	504.841452	6.138330
6.412020	499.082090	6.143334
6.490844	502.347598	6.148339
6.122878	509.950640	6.153344
6.346229	505.983109	6.158349
6.266476	508.703844	6.163354
6.189307	509.423653	6.168358
6.302272	488.745610	6.173363
6.222650	480.407213	6.178368
6.162479	479.328018	6.183373
6.169679	479.967986	6.188378
6.170305	462.465102	6.193382
6.058466	481.541542	6.198387
5.643462	470.033554	6.203392
6.006615	484.835883	6.208397
6.283131	505.070827	6.213402
5.961024	504.194924	6.218406
6.252752	497.549126	6.223411
5.864119	500.377331	6.228416
6.451430	492.373127	6.233421
6.441636	501.835199	6.238426
6.071984	516.464882	6.243430
6.381379	514.990192	6.248435
6.227550	489.099438	6.253440
5.974100	471.706401	6.258445
5.774509	493.754843	6.263450
6.089853	497.956702	6.268454
6.521252	492.396341	6.273459
5.806389	499.583387	6.278464
6.001094	501.332158	6.283469
6.047451	493.745651	6.288474
6.141430	508.540596	6.293478
6.280204	504.648205	6.298483
6.024507	515.251350	6.303488
6.221228	519.375649	6.308493
5.978641	520.656090	6.313498
6.029623	501.589344	6.318502
6.234383	490.977345	6.323507
6.241378	514.285554	6.328512
6.316965	520.218670	6.333517
5.999720	510.377545	6.338522
6.041667	495.740053	6.343526
6.246644	500.767296	6.348531
5.906892	506.185536	6.353536
6.345292	505.028190	6.358541
6.543632	505.741338	6.363546
6.165318	491.655989	6.368550
6.119340	488.234401	6.373555
5.869324	509.073577	6.378560
5.963308	492.242715	6.383565
6.039352	488.540136	6.388570
5.963909	512.195791	6.393574
6.227440	508.989799	6.398579
6.227336	514.949232	6.403584
6.118527	499.413396	6.408589
6.042983	494.798012	6.413594
5.928080	513.407897	6.418598
6.331504	524.044180	6.423603
5.810139	512.400731	6.428608
5.938013	497.237939	6.433613
6.250199	518.042424	6.438618
5.904892	509.200712	6.443622
6.133528	492.434113	6.448627
6.353395	509.395593	6.453632
6.001788	506.266395	6.458637
6.533205	505.340793	6.463642
6.090190	516.149205	6.468646
6.383424	510.736560	6.473651
6.055120	509.666849	6.478656
6.218663	499.226202	6.483661
6.240906	501.347363	6.488666
6.448689	518.412458	6.493670
6.216169	512.743791	6.498675
6.469959	517.270320	6.503680
6.524040	490.634243	6.508685
5.968830	494.499643	6.513690
5.979339	493.960213	6.518694
5.976825	469.716089	6.523699
6.037267	475.919128	6.528704
6.383189	511.082258	6.533709
6.220273	480.115862	6.538714
6.194523	484.051898	6.543718
6.162035	485.421224	6.548723
5.832481	480.497815	6.553728
6.055863	475.843791	6.558733
6.003993	480.711144	6.563738
5.926331	510.283813	6.568742
6.224702	499.323596	6.573747
6.174495	490.490937	6.578752
6.335432	506.994262	6.583757
5.980232	518.570943	6.588762
6.114310	515.407452	6.593766
6.221083	499.958215	6.598771
6.031640	511.420491	6.603776
6.478324	513.680747	6.608781
6.305280	512.432473	6.613786
5.884431	480.077012	6.618790
6.088365	479.977059	6.623795
6.107883	500.919360	6.628800
6.215575	512.821535	6.633805
6.434535	497.623468	6.638810
6.080145	482.421811	6.643814
6.462251	487.352696	6.648819
6.028618	467.339145	6.653824
5.928239	469.053219	6.658829
6.103754	487.741350	6.663834
6.062031	486.176221	6.668838
6.081038	478.189486	6.673843
5.870057	484.598672	6.678848
6.181253	503.708616	6.683853
6.076559	521.222709	6.688858
5.896657	507.370120	6.693862
6.343134	516.011510	6.698867
5.892820	516.483324	6.703872
5.887642	527.573935	6.708877
6.211152	517.807444	6.713882
6.004163	497.727989	6.718886
6.462624	493.321587	6.723891
6.082489	518.405825	6.728896
6.202534	522.132220	6.733901
6.348049	513.136986	6.738906
5.974563	505.151273	6.743910
6.306291	502.414529	6.748915
6.030463	508.388451	6.753920
6.308217	508.544032	6.758925
6.573288	503.963608	6.763930
6.046253	494.841389	6.768934
6.190502	474.350462	6.773939
5.789207	469.855604	6.778944
6.321688	479.771603	6.783949
6.321134	492.800857	6.788954
5.817740	486.504771	6.793958
5.779107	494.948815	6.798963
5.801650	507.794626	6.803968
6.169051	519.354391	6.808973
6.297514	511.283850	6.813978
5.785878	497.994428	6.818982
6.115113	505.741304	6.823987
6.106504	514.047617	6.828992
6.024821	531.189071	6.833997
6.069675	507.994477	6.839002
5.732195	504.221333	6.844006
5.943968	504.700732	6.849011
6.235798	515.466529	6.854016
6.386744	510.697602	6.859021
6.327391	504.865370	6.864026
5.997161	512.782392	6.869030
6.621467	514.836812	6.874035
6.233193	515.203474	6.879040
6.445900	503.091973	6.884045
6.379874	515.992774	6.889050
6.237533	528.267050	6.894054
6.524876	506.550100	6.899059
6.127719	504.726253	6.904064
6.339744	482.149532	6.909069
6.138851	486.367644	6.914074
5.955223	482.951443	6.919078
6.024440	472.347058	6.924083
5.820218	503.326740	6.929088
6.058923	509.310533	6.934093
6.240194	511.932890	6.939098
6.475965	509.586967	6.944102
6.336285	513.040505	6.949107
5.852336	501.874951	6.954112
5.951825	481.811457	6.959117
6.544481	511.060768	6.964122
5.837826	492.398412	6.969126
6.173243	479.280954	6.974131
5.720423	507.502670	6.979136
5.961121	522.603757	6.984141
6.418784	503.757463	6.989146
6.211124	495.233055	6.994150
5.863733	517.654086	6.999155
5.988136	522.122290	7.004160
6.167272	506.898635	7.009165
6.420751	502.954636	7.014170
6.244194	513.416260	7.019174
6.452172	506.552770	7.024179
5.996647	514.918930	7.029184
6.296374	500.945259	7.034189
6.158621	500.199787	7.039194
6.000169	497.283814	7.044198
6.349518	494.357220	7.049203
6.127922	492.256952	7.054208
6.015878	481.623918	7.059213
6.197145	486.805119	7.064218
6.264579	478.902716	7.069222
6.537157	472.848138	7.074227
6.246496	490.436333	7.079232
6.064974	480.316213	7.084237
6.092569	468.579614	7.089242
5.656705	477.179458	7.094246
5.739321	488.430337	7.099251
6.002551	499.732763	7.104256
6.372859	503.056346	7.109261
6.584099	501.470917	7.114266
6.789375	499.660075	7.119270
6.798321	474.020834	7.124275
6.453906	467.659123	7.129280
6.395445	474.207054	7.134285
6.341019	487.736772	7.139290
6.399115	484.721288	7.144294
6.605633	451.324754	7.149299
6.192410	445.100102	7.154304
6.074371	460.157717	7.159309
6.090556	459.321404	7.164314
5.787276	453.233063	7.169318
5.872599	452.717968	7.174323
5.891735	465.616392	7.179328
6.243830	460.763437	7.184333
6.394870	459.047189	7.189338
5.963525	471.977051	7.194342
6.342199	459.112105	7.199347
6.190178	485.414881	7.204352
6.073922	464.874187	7.209357
5.977595	464.921221	7.214362
5.926947	488.695659	7.219366
6.203175	491.481762	7.224371
6.206598	476.128646	7.229376
6.246963	465.164331	7.234381
6.150420	475.756833	7.239386
5.827561	464.523154	7.244390
6.279697	461.395109	7.249395
5.955016	479.749297	7.254400
6.004389	489.310690	7.259405
6.127859	469.322563	7.264410
6.061917	468.362799	7.269414
6.044673	471.546513	7.274419
5.872667	489.166594	7.279424
5.926271	480.181340	7.284429
6.367561	468.576041	7.289434
5.850286	466.066416	7.294438
5.921888	475.162254	7.299443
5.780171	492.880224	7.304448
5.836357	486.050311	7.309453
6.308217	473.798444	7.314458
5.801262	477.688321	7.319462
5.955686	482.022421	7.324467
5.688728	497.233813	7.329472
6.070682	494.727896	7.334477
6.313427	487.565287	7.339482
6.414821	499.108721	7.344486
6.509507	512.513099	7.349491
6.009250	498.270920	7.354496
6.192361	467.762905	7.359501
6.371408	474.072810	7.364506
6.000651	494.530124	7.369510
6.102214	485.377624	7.374515
5.658075	482.560655	7.379520
5.867075	487.561974	7.384525
5.690542	516.193313	7.389530
6.181744	529.567298	7.394534
6.008973	513.853795	7.399539
6.169986	494.789887	7.404544
6.368451	508.726585	7.409549
6.508867	524.065811	7.414554
6.070861	519.620706	7.419558
6.320302	500.714517	7.424563
6.425869	515.517419	7.429568
6.262786	508.439227	7.434573
6.239475	501.653321	7.439578
5.888882	483.255211	7.444582
6.195576	483.317127	7.449587
6.018064	496.503278	7.454592
6.387856	516.897333	7.459597
6.284342	504.198449	7.464602
5.740078	481.899416	7.469606
6.207115	494.839168	7.474611
5.934870	505.605443	7.479616
5.983149	491.272919	7.484621
6.275465	509.287141	7.489626
6.183956	513.849325	7.494630
6.156320	517.130258	7.499635
6.181173	527.433719	7.504640
6.211740	513.429839	7.509645
6.237396	501.118512	7.514650
6.033114	499.292485	7.519654
6.137595	505.201684	7.524659
6.038495	528.932302	7.529664
6.186674	517.816166	7.534669
6.025632	519.461648	7.539674
5.851078	514.433596	7.544678
6.030942	500.982349	7.549683
5.987057	513.232451	7.554688
6.163792	522.725861	7.559693
6.237805	516.671131	7.564698
6.428966	508.779044	7.569702
6.200522	507.473831	7.574707
5.836614	515.318290	7.579712
6.210816	515.615771	7.584717
6.462184	496.026422	7.589722
6.326246	509.778074	7.594726
6.385295	488.071254	7.599731
5.996510	497.517825	7.604736
5.755057	503.787436	7.609741
6.192846	492.695078	7.614746
5.995660	521.958035	7.619750
6.227874	511.907533	7.624755
6.038817	507.135210	7.629760
6.141696	515.790764	7.634765
5.980791	516.590407	7.639770
6.256776	506.970675	7.644774
6.027685	511.436821	7.649779
6.530604	515.043810	7.654784
6.345555	519.209002	7.659789
5.879608	515.261168	7.664794
5.807050	508.037505	7.669798
6.244746	491.977310	7.674803
6.082161	520.553179	7.679808
6.373508	521.831605	7.684813
6.269778	514.889603	7.689818
5.999778	496.063636	7.694822
5.789275	505.581371	7.699827
5.797368	507.425399	7.704832
6.187839	503.513018	7.709837
6.326673	504.001017	7.714842
6.117975	528.349728	7.719846
6.243502	527.282951	7.724851
6.050946	517.910810	7.729856
6.295134	511.116800	7.734861
6.333959	518.773862	7.739866
6.157791	505.971564	7.744870
6.318611	514.347639	7.749875
6.381494	519.407938	7.754880
6.379191	507.939543	7.759885
6.382060	482.564487	7.764890
6.297170	493.387689	7.769894
6.397706	482.278664	7.774899
5.927111	471.319370	7.779904
5.905678	477.338050	7.784909
5.988123	496.514297	7.789914
5.846128	480.799786	7.794918
6.106061	466.755678	7.799923
6.186087	481.931713	7.804928
6.269377	490.885351	7.809933
5.998140	487.348182	7.814938
6.159332	490.688070	7.819942
6.529362	494.753930	7.824947
6.307428	469.530478	7.829952
6.124753	476.488303	7.834957
6.207507	488.169859	7.839962
5.945031	492.437215	7.844966
6.229820	472.991134	7.849971
5.948628	462.818837	7.854976
6.127146	475.040048	7.859981
6.379992	484.830317	7.864986
6.196257	490.837449	7.869990
6.377536	471.409068	7.874995
6.126622	491.374934	7.880000
6.031208	480.774863	7.885005
6.225830	469.235778	7.890010
5.926492	470.907363	7.895014
5.990886	481.344241	7.900019
6.127790	491.462741	7.905024
5.818296	480.100079	7.910029
6.028427	491.371222	7.915034
6.029840	474.910121	7.920038
6.145616	491.811837	7.925043
5.801988	503.740645	7.930048
5.927749	510.622755	7.935053
6.336199	503.423581	7.940058
5.935845	514.110214	7.945062
6.312245	513.952067	7.950067
5.905148	514.734389	7.955072
6.120634	517.892281	7.960077
6.140116	528.030801	7.965082
6.237123	521.309644	7.970086
6.331177	508.525429	7.975091
6.105711	519.953908	7.980096
6.273473	518.130717	7.985101
6.247705	516.984573	7.990106
5.957156	523.864557	7.995110
6.490417	507.049179	8.000115
6.330026	515.667522	8.005133
5.927565	495.388889	8.010150
5.982920	497.265562	8.015168
5.568150	513.797658	8.020186
5.969726	502.711938	8.025203
5.963317	520.121269	8.030221
5.937528	522.615021	8.035238
6.127487	504.677547	8.040256
5.774043	513.347322	8.045274
5.937275	522.842089	8.050291
6.038452	523.784094	8.055309
6.168716	512.828611	8.060326
6.320827	517.194293	8.065344
5.946520	513.511782	8.070362
5.909323	503.982105	8.075379
6.149351	531.554509	8.080397
6.414395	546.710091	8.085414
6.675613	525.613576	8.090432
6.321720	531.138264	8.095450
6.476724	534.624490	8.100467
6.445680	513.860755	8.105485
6.684949	506.587687	8.110502
6.738242	513.499488	8.115520
6.500465	529.452903	8.120538
6.468214	514.659033	8.125555
6.321044	524.896337	8.130573
6.584471	511.600905	8.135590
6.299344	491.302789	8.140608
6.110770	499.604561	8.145626
6.345196	528.021050	8.150643
6.339891	507.123777	8.155661
6.384740	500.071073	8.160678
6.256480	485.797185	8.165696
6.095052	514.134815	8.170714
6.641806	513.086802	8.175731
6.450615	487.444174	8.180749
6.320817	488.244673	8.185766
6.218814	475.602503	8.190784
6.171803	486.039507	8.195802
6.398434	499.188186	8.200819
5.971866	505.560169	8.205837
5.928948	510.114431	8.210854
6.529820	500.658985	8.215872
6.111054	514.003578	8.220890
6.383987	516.887800	8.225907
6.405581	507.797785	8.230925
6.375964	513.542718	8.235942
6.466288	511.494848	8.240960
6.476771	530.070948	8.245978
6.253317	505.208697	8.250995
6.228812	517.224819	8.256013
6.146805	535.769668	8.261030
6.523409	514.735868	8.266048
6.387136	509.099804	8.271066
6.512021	516.808699	8.276083
6.664611	522.997112	8.281101
6.646984	511.212178	8.286118
6.784498	528.456239	8.291136
6.668669	536.761852	8.296154
6.581230	506.512205	8.301171
6.710844	498.453160	8.306189
6.243491	502.589018	8.311206
6.169726	493.353792	8.316224
6.161597	533.120430	8.321242
6.306638	511.882155	8.326259
6.449870	503.577815	8.331277
6.132308	506.620524	8.336294
6.714490	510.829922	8.341312
6.176055	516.901884	8.346330
6.502240	514.918353	8.351347
6.466601	502.709752	8.356365
6.195955	513.034069	8.361382
6.446140	499.733554	8.366400
6.470410	500.286216	8.371418
6.213886	514.380843	8.376435
6.357075	523.982339	8.381453
6.134567	497.049864	8.386470
6.381983	521.392917	8.391488
6.214258	556.402901	8.396506
6.857475	542.680117	8.401523
6.769968	527.506696	8.406541
6.615259	524.636570	8.411558
6.816016	513.912970	8.416576
6.613144	522.215149	8.421594
6.508594	510.563444	8.426611
6.693833	490.539861	8.431629
6.316013	500.780334	8.436646
6.250872	533.589291	8.441664
6.615630	541.018765	8.446682
6.632055	523.195060	8.451699
6.836878	528.290800	8.456717
6.900213	553.120297	8.461734
6.879821	527.366919	8.466752
6.432649	508.249759	8.471770
6.456068	506.270902	8.476787
6.750268	520.895314	8.481805
6.259436	521.420828	8.486822
6.720483	542.875781	8.491840
6.796049	538.023365	8.496858
6.595258	532.660773	8.501875
6.950447	532.607627	8.506893
6.579899	528.643075	8.511910
6.394740	502.780786	8.516928
6.370174	515.207724	8.521946
6.716235	537.585843	8.526963
6.692313	529.605289	8.531981
6.799842	539.718450	8.536998
6.784446	550.356808	8.542016
6.901862	557.914049	8.547034
6.889853	552.270914	8.552051
6.722101	529.978612	8.557069
6.687438	531.582057	8.562087
6.930156	543.931099	8.567104
6.404285	526.186872	8.572122
6.468702	527.076406	8.577139
6.983287	526.350253	8.582157
6.851957	553.681691	8.587175
6.596687	550.583463	8.592192
7.032868	539.632116	8.597210
6.924517	537.563546	8.602227
6.561609	533.492052	8.607245
6.196396	535.144317	8.612263
7.023676	538.166791	8.617280
6.674959	554.962939	8.622298
6.646380	547.984338	8.627315
6.912212	531.365119	8.632333
6.645735	541.425356	8.637351
6.586725	566.538502	8.642368
6.798175	555.859746	8.647386
6.713281	535.451535	8.652403
6.889072	542.804295	8.657421
6.664082	564.549961	8.662439
6.779897	542.993728	8.667456
6.712127	531.364070	8.672474
6.763296	526.203672	8.677491
6.417782	540.058573	8.682509
6.598232	543.538136	8.687527
6.578317	545.095458	8.692544
6.686732	550.998154	8.697562
6.874232	559.086673	8.702579
6.766958	570.359149	8.707597
7.032863	579.113859	8.712615
7.183568	564.903610	8.717632
7.255523	562.017963	8.722650
6.977296	567.261338	8.727667
6.930928	540.726723	8.732685
6.600281	546.389760	8.737703
7.067127	553.964528	8.742720
7.055293	537.225979	8.747738
6.810682	539.002172	8.752755
7.317886	540.541755	8.757773
6.800004	547.962903	8.762791
6.983617	539.959657	8.767808
7.143779	548.055639	8.772826
6.856566	538.880553	8.777843
6.993444	540.842157	8.782861
6.952850	552.068571	8.787879
6.941786	548.499106	8.792896
6.972853	529.833446	8.797914
6.824733	526.537745	8.802931
6.934480	538.704877	8.807949
6.977101	561.787814	8.812967
6.919107	560.831273	8.817984
7.025645	550.783760	8.823002
7.096161	570.784426	8.828019
7.398299	572.747358	8.833037
6.869591	556.431215	8.838055
7.053200	531.230863	8.843072
7.161521	536.640501	8.848090
6.593726	554.701540	8.853107
7.520496	557.666250	8.858125
7.322007	552.637526	8.863143
7.079105	547.046325	8.868160
7.361942	540.659882	8.873178
6.856091	545.461671	8.878195
6.815818	537.725281	8.883213
6.914798	540.403773	8.888231
6.965888	543.646420	8.893248
7.399473	568.805296	8.898266
7.243198	566.394642	8.903283
7.097165	546.556008	8.908301
7.246816	553.057330	8.913319
7.118294	553.515888	8.918336
7.070563	543.381306	8.923354
7.180726	552.052617	8.928371
6.993110	549.025962	8.933389
7.380016	551.888995	8.938407
7.306517	543.204819	8.943424
6.993003	559.545281	8.948442
7.025509	565.458658	8.953459
7.159649	549.906459	8.958477
7.380180	560.512233	8.963495
7.265528	579.776894	8.968512
7.363967	560.656489	8.973530
7.213573	538.823970	8.978547
7.236739	536.908223	8.983565
7.157568	544.783887	8.988583
7.319865	543.274259	8.993600
7.296368	534.967050	8.998618
6.938742	545.509346	9.003635
7.523420	559.320752	9.008653
7.088576	555.928570	9.013671
7.424605	551.139868	9.018688
7.272017	540.914281	9.023706
7.028295	537.520628	9.028723
7.146547	546.041035	9.033741
7.393905	561.555064	9.038759
7.695439	572.077794	9.043776
7.456011	551.984190	9.048794
7.427284	537.265482	9.053811
7.341823	533.964147	9.058829
7.235286	554.948702	9.063847
7.088330	539.694174	9.068864
7.422636	516.490418	9.073882
6.927253	534.103468	9.078899
7.088084	552.335253	9.083917
7.477707	564.462158	9.088935
7.216734	569.367246	9.093952
7.616479	559.785105	9.098970
7.488198	568.798795	9.103987
7.673773	563.557921	9.109005
7.612460	557.118434	9.114023
7.153405	544.216895	9.119040
7.069970	525.739406	9.124058
7.012258	551.115820	9.129075
7.506988	557.537389	9.134093
7.395843	568.303166	9.139111
7.261913	571.539594	9.144128
7.214063	549.479838	9.149146
7.021743	571.420846	9.154163
7.218971	579.105024	9.159181
7.346763	583.364932	9.164199
6.994423	570.289384	9.169216
7.500613	552.975783	9.174234
7.475804	572.461448	9.179251
7.392829	587.374172	9.184269
7.564041	572.038795	9.189287
7.097297	575.247765	9.194304
7.642364	565.292786	9.199322
7.395373	563.666395	9.204339
7.286979	562.298715	9.209357
7.754724	571.062674	9.214375
7.427875	572.244560	9.219392
7.379297	559.251561	9.224410
7.425226	577.321015	9.229427
7.650629	577.997387	9.234445
7.667685	581.518129	9.239463
7.519620	574.632963	9.244480
7.606320	555.458711	9.249498
7.437273	566.984828	9.254515
7.579679	587.012600	9.259533
7.704370	589.919071	9.264551
7.510570	570.775608	9.269568
7.850483	562.332563	9.274586
7.500692	568.967102	9.279603
7.402737	556.243116	9.284621
7.865453	577.085808	9.289639
7.514420	575.726539	9.294656
7.610682	562.452883	9.299674
7.579983	559.960964	9.304691
7.581838	559.434272	9.309709
7.490225	590.939039	9.314727
7.455583	596.969597	9.319744
7.710016	598.897908	9.324762
7.537730	614.375462	9.329779
7.607304	605.859385	9.334797
7.589489	612.836905	9.339815
7.697442	613.705571	9.344832
7.880309	595.685623	9.349850
8.014446	612.313777	9.354867
7.659093	586.915470	9.359885
7.949340	597.656362	9.364903
7.586138	604.222286	9.369920
7.932892	580.635773	9.374938
7.598435	570.725280	9.379955
7.389042	569.792479	9.384973
7.833609	584.685326	9.389991
7.914950	582.552144	9.395008
7.792863	574.851987	9.400026
7.663591	578.038741	9.405043
7.652771	597.991583	9.410061
7.607909	586.695109	9.415079
7.373109	595.269164	9.420096
7.871760	603.716508	9.425114
7.734721	619.626899	9.430131
7.786537	608.390201	9.435149
7.864427	607.980236	9.440167
7.723461	602.444983	9.445184
7.711118	595.395980	9.450202
7.739211	589.521563	9.455219
7.532251	598.918050	9.460237
7.725009	594.899752	9.465255
7.628262	605.512725	9.470272
7.706623	608.211955	9.475290
7.565215	591.878215	9.480307
7.240867	586.722780	9.485325
7.848011	599.627516	9.490343
7.940899	634.473287	9.495360
8.113611	617.183529	9.500378
8.065754	612.337021	9.505395
8.022904	606.910714	9.510413
8.176011	579.506391	9.515431
7.845690	596.779233	9.520448
7.968984	594.155591	9.525466
7.834367	603.530878	9.530483
7.662038	604.100190	9.535501
8.209701	587.666850	9.540519
7.975479	612.246585	9.545536
8.227395	611.618250	9.550554
8.050175	604.307987	9.555571
8.061657	590.786676	9.560589
7.984325	585.680356	9.565607
7.868491	605.461343	9.570624
7.750133	599.120315	9.575642
8.134441	606.241064	9.580659
8.051799	606.950730	9.585677
8.318175	597.792658	9.590695
7.913784	622.482888	9.595712
7.665506	606.557630	9.600730
7.633968	592.277007	9.605747
7.757348	596.851044	9.610765
7.950119	607.785462	9.615783
7.933342	614.144873	9.620800
8.218590	625.134965	9.625818
8.238449	626.956120	9.630835
7.864199	608.845989	9.635853
8.296242	618.186385	9.640871
7.843380	616.286614	9.645888
7.765862	609.550457	9.650906
8.105476	618.127407	9.655923
7.856020	636.481509	9.660941
8.045062	626.944575	9.665959
7.884170	615.600443	9.670976
7.753226	624.507549	9.675994
8.407601	650.911118	9.681011
8.403277	642.224506	9.686029
8.325106	626.602027	9.691047
8.365616	640.779047	9.696064
8.459803	624.596442	9.701082
8.154656	621.246869	9.706099
8.288532	636.359570	9.711117
8.006689	623.824631	9.716135
8.444656	633.746181	9.721152
8.209246	625.403193	9.726170
8.265442	612.944552	9.731187
8.043149	632.511636	9.736205
8.147766	622.509360	9.741223
8.303873	611.901997	9.746240
8.351870	633.211517	9.751258
8.362140	624.395471	9.756275
8.018527	608.605716	9.761293
8.315398	607.399244	9.766311
8.119005	627.226830	9.771328
8.128774	625.222759	9.776346
8.595389	619.454159	9.781363
8.270479	625.660221	9.786381
8.380666	627.924787	9.791399
8.120138	601.888517	9.796416
8.397046	591.109476	9.801434
8.517261	608.443076	9.806451
8.017227	615.576444	9.811469
8.237092	616.999392	9.816487
8.089105	613.180370	9.821504
8.409617	605.782246	9.826522
8.516208	609.353633	9.831539
8.377972	619.432382	9.836557
8.603448	624.778314	9.841575
8.448820	608.402659	9.846592
8.143492	609.787431	9.851610
8.541922	626.733044	9.856627
8.484255	623.686769	9.861645
8.485678	588.135161	9.866663
8.165495	601.515099	9.871680
8.277276	614.107034	9.876698
8.210022	616.029271	9.881715
8.289619	622.591595	9.886733
8.355361	614.147878	9.891751
8.462080	628.675460	9.896768
8.773058	636.359567	9.901786
8.504145	619.205367	9.906803
8.581304	612.576583	9.911821
8.795159	622.469430	9.916839
8.286466	605.130132	9.921856
8.265028	613.773141	9.926874
8.471484	628.184660	9.931891
8.760625	623.401814	9.936909
8.905279	610.079481	9.941927
8.265291	599.892382	9.946944
8.393894	618.534872	9.951962
8.610453	626.560077	9.956979
8.516943	618.886957	9.961997
8.857038	596.790969	9.967015
8.533960	605.317430	9.972032
8.447236	618.264128	9.977050
8.572322	606.874023	9.982067
8.435331	613.472825	9.987085
8.865323	609.039242	9.992103
8.823542	616.010588	9.997120
8.703534	623.956311	10.002138
8.716565	591.842078	10.007155
8.505545	584.133585	10.012173
8.554084	595.384366	10.017191
8.552424	606.873012	10.022208
8.290356	606.744656	10.027226
8.446343	599.505183	10.032243
8.496193	619.918663	10.037261
8.924566	614.115451	10.042279
8.736993	625.356073	10.047296
8.664284	627.898826	10.052314
8.699260	616.692651	10.057331
8.681631	618.926284	10.062349
8.831186	611.240158	10.067367
8.512260	609.652906	10.072384
8.394945	628.809342	10.077402
8.992578	615.672507	10.082419
8.971088	622.482476	10.087437
8.736046	608.164818	10.092455
8.823606	617.634365	10.097472
8.254268	607.440998	10.102490
8.596280	604.422550	10.107507
8.500970	628.783840	10.112525
8.884333	622.366384	10.117543
8.934028	614.024700	10.122560
8.862389	626.096420	10.127578
9.103650	629.188992	10.132595
8.926478	636.776357	10.137613
8.929449	610.029390	10.142631
8.679522	597.557684	10.147648
8.612115	607.358851	10.152666
9.121109	617.980560	10.157683
8.540829	624.045604	10.162701
8.757352	608.551858	10.167719
8.994818	611.341396	10.172736
8.974375	629.945459	10.177754
9.264040	623.094890	10.182771
8.960223	595.109340	10.187789
8.830166	595.980341	10.192807
8.654440	592.457559	10.197824
8.638694	602.034301	10.202842
8.703759	617.871539	10.207859
8.775477	632.867182	10.212877
8.745383	616.396843	10.217895
9.083072	621.203902	10.222912
8.737786	619.414566	10.227930
8.807044	626.987673	10.232947
8.787961	633.655261	10.237965
9.024867	638.567440	10.242983
8.769927	643.566804	10.248000
8.597199	625.625655	10.253018
8.880339	627.067471	10.258035
8.568408	635.906389	10.263053
8.775115	615.533717	10.268071
8.819215	627.775335	10.273088
8.906645	659.104831	10.278106
9.503945	649.024072	10.283123
8.981826	632.591043	10.288141
8.885000	639.179478	10.293159
8.985363	629.889319	10.298176
8.825987	658.297722	10.303194
8.971357	671.607085	10.308211
9.483817	673.156047	10.313229
9.303840	650.905045	10.318247
9.195542	631.550875	10.323264
8.992579	624.695812	10.328282
9.020705	629.920466	10.333299
8.912011	624.226960	10.338317
9.150301	633.096474	10.343335
9.187360	659.510166	10.348352
9.225438	664.947890	10.353370
9.403624	638.092020	10.358387
9.246228	623.361921	10.363405
8.951501	632.255657	10.368423
9.336583	642.668593	10.373440
8.963780	637.014892	10.378458
8.923263	629.966789	10.383475
9.034755	647.774678	10.388493
9.346157	661.828921	10.393511
8.901909	655.792836	10.398528
9.211997	664.191277	10.403546
9.412876	670.171726	10.408563
9.361270	647.428681	10.413581
9.517750	644.861045	10.418599
9.575187	655.372512	10.423616
9.184475	653.278757	10.428634
9.376533	624.202332	10.433651
9.268804	629.470689	10.438669
9.222283	632.154940	10.443687
9.129174	609.538855	10.448704
9.151533	625.094459	10.453722
9.377293	644.664662	10.458739
9.599573	643.705980	10.463757
9.304305	616.782757	10.468775
9.237033	622.875100	10.473792
8.900592	636.674374	10.478810
9.144938	642.419641	10.483827
9.609508	638.162274	10.488845
9.716999	646.105541	10.493863
9.588608	645.088798	10.498880
9.069191	658.329611	10.503898
9.424494	635.174849	10.508915
9.489656	610.725922	10.513933
9.187751	624.760156	10.518951
9.631281	632.311759	10.523968
9.442077	623.722226	10.528986
9.230230	627.779291	10.534003
9.519177	636.990141	10.539021
9.434068	636.020463	10.544039
9.832492	630.678860	10.549056
9.346902	636.628486	10.554074
9.554485	627.354261	10.559091
9.262546	617.369404	10.564109
9.214115	642.381251	10.569127
9.417192	655.543207	10.574144
9.414102	651.359675	10.579162
9.344974	651.661216	10.584179
9.233332	666.045143	10.589197
9.616011	657.798565	10.594215
9.468656	645.375206	10.599232
9.288627	662.388803	10.604250
9.528039	672.424368	10.609267
9.579357	665.448156	10.614285
9.184522	649.531426	10.619303
9.671604	640.473138	10.624320
9.489736	668.873864	10.629338
9.662554	662.894520	10.634355
9.772278	650.571056	10.639373
9.647357	650.349090	10.644391
10.042181	650.781878	10.649408
9.615921	678.655350	10.654426
9.869252	665.692169	10.659443
9.793700	648.011928	10.664461
9.667034	657.760338	10.669479
9.820097	671.520175	10.674496
9.480930	660.139248	10.679514
9.453140	638.584768	10.684531
9.687078	642.580074	10.689549
9.511359	648.602183	10.694567
9.631849	667.114516	10.699584
9.321612	662.872122	10.704602
9.581954	646.613626	10.709619
9.441270	647.656516	10.714637
9.506668	660.441535	10.719655
9.701681	659.062377	10.724672
9.479693	657.457723	10.729690
9.855168	671.914561	10.734707
10.228499	671.782356	10.739725
10.082379	665.450807	10.744743
9.946225	662.496509	10.749760
9.880357	662.956130	10.754778
9.661211	648.444127	10.759795
9.844907	637.771278	10.764813
9.615271	659.541560	10.769831
9.793756	665.047198	10.774848
9.814201	654.511915	10.779866
9.739511	659.417636	10.784883
9.985353	650.156263	10.789901
9.627586	632.869726	10.794919
9.870427	639.941744	10.799936
9.709426	673.679091	10.804954
10.291515	684.419835	10.809971
10.361303	654.554725	10.814989
9.852263	638.371426	10.820007
10.164396	651.319447	10.825024
9.967185	665.055491	10.830042
9.953448	640.686368	10.835059
10.239809	627.693555	10.840077
9.993629	651.911749	10.845095
10.138719	665.008415	10.850112
10.033106	661.017758	10.855130
9.831937	650.168901	10.860147
9.840253	628.703028	10.865165
9.808891	648.878561	10.870183
9.854882	660.484240	10.875200
9.841238	658.592962	10.880218
9.773701	631.635821	10.885235
9.732847	646.759201	10.890253
9.915976	673.581436	10.895271
10.242637	676.305080	10.900288
10.292009	663.674933	10.905306
10.099535	655.579292	10.910323
10.247157	667.707797	10.915341
9.831641	662.416558	10.920359
10.126099	664.554149	10.925376
10.141682	680.818118	10.930394
9.940989	678.168200	10.935411
10.445000	661.622147	10.940429
10.244045	678.800100	10.945447
10.346329	666.281155	10.950464
10.058446	650.466993	10.955482
9.963744	644.599267	10.960499
10.330811	646.630000	10.965517
9.966125	670.089183	10.970535
10.154200	676.994135	10.975552
10.127415	664.430200	10.980570
9.989036	669.944219	10.985587
10.038500	675.969273	10.990605
9.978869	684.183222	10.995623
10.156696	666.473682	11.000640
10.094225	671.662152	11.005658
10.208702	668.384819	11.010675
10.011510	683.365417	11.015693
10.231746	680.407815	11.020711
10.155042	680.719859	11.025728
10.229618	670.359624	11.030746
9.936394	677.292651	11.035763
10.385129	668.358565	11.040781
10.331464	681.868596	11.045799
10.144723	679.740934	11.050816
10.338768	668.042519	11.055834
10.364909	670.541392	11.060851
10.306684	679.808556	11.065869
10.260763	673.938072	11.070887
10.433932	676.348492	11.075904
10.581690	674.890945	11.080922
10.171357	666.525774	11.085939
10.767873	664.646723	11.090957
10.532227	690.424521	11.095975
10.413705	678.595321	11.100992
10.356816	673.414060	11.106010
10.435008	660.761441	11.111027
10.491642	668.030930	11.116045
10.515097	681.288715	11.121063
10.465155	677.051026	11.126080
10.398781	666.808253	11.131098
10.328374	650.251554	11.136115
10.659588	674.112235	11.141133
10.313356	697.326547	11.146151
10.803596	678.071777	11.151168
10.657341	662.706411	11.156186
10.357072	665.339417	11.161203
10.379552	677.207092	11.166221
10.648099	670.818136	11.171239
10.377506	666.716393	11.176256
10.797256	672.711054	11.181274
10.353893	680.302775	11.186291
10.739658	698.604817	11.191309
10.645993	688.934003	11.196327
10.797497	673.519125	11.201344
10.717146	672.029017	11.206362
10.518369	687.499806	11.211379
10.511564	668.555963	11.216397
10.416771	671.745404	11.221415
10.663592	686.805542	11.226432
10.932354	717.046720	11.231450
10.660352	709.982027	11.236467
10.977281	685.718971	11.241485
10.873597	672.752102	11.246503
10.469241	672.850747	11.251520
10.608409	659.559780	11.256538
10.403151	679.753759	11.261555
10.859169	703.112889	11.266573
10.954205	697.433610	11.271591
11.243746	705.430660	11.276608
10.960101	697.846876	11.281626
10.675653	678.420110	11.286643
10.774419	659.762882	11.291661
10.839500	668.250522	11.296679
10.955228	684.102581	11.301696
11.097912	678.864919	11.306714
10.715945	664.790817	11.311731
10.770884	645.000317	11.316749
10.968882	664.268916	11.321767
10.746916	671.547940	11.326784
10.937842	670.629764	11.331802
10.699517	659.688937	11.336819
10.607747	654.793389	11.341837
10.556540	669.355961	11.346855
10.526071	678.621096	11.351872
11.064604	693.236587	11.356890
10.763668	703.251458	11.361907
11.304801	688.443647	11.366925
11.124112	702.313080	11.371943
11.010281	704.082144	11.376960
10.692490	688.025314	11.381978
10.720673	706.862510	11.386995
11.189833	700.435075	11.392013
11.298273	692.925440	11.397031
10.924201	692.374078	11.402048
11.141287	703.747635	11.407066
11.075739	704.359328	11.412083
10.966690	682.317661	11.417101
11.010196	667.106412	11.422119
11.284807	681.158389	11.427136
11.161061	686.164327	11.432154
10.883952	690.340528	11.437171
11.359824	667.054111	11.442189
11.473483	665.653269	11.447207
10.997446	675.599839	11.452224
11.087008	658.144298	11.457242
10.752004	662.115453	11.462259
10.917901	669.174124	11.467277
10.828347	670.796692	11.472295
11.155180	701.932425	11.477312
11.155313	701.148898	11.482330
11.111634	696.659055	11.487347
11.499489	697.780210	11.492365
11.456168	712.182311	11.497383
11.185072	684.946988	11.502400
11.249521	674.323142	11.507418
11.020527	684.923192	11.512435
11.029473	690.855468	11.517453
11.222865	697.351592	11.522471
11.118475	693.736901	11.527488
11.031933	705.449926	11.532506
11.094253	711.429771	11.537523
11.208428	690.451102	11.542541
11.116417	698.982824	11.547559
11.264245	695.827301	11.552576
11.554868	692.946427	11.557594
11.330534	710.820709	11.562611
11.204465	699.593955	11.567629
11.280638	697.966494	11.572647
11.037800	698.002826	11.577664
11.252135	691.881312	11.582682
11.474228	716.375967	11.587699
11.573362	714.364497	11.592717
11.503517	698.549283	11.597735
11.454079	694.821111	11.602752
11.671772	700.815620	11.607770
11.474135	710.097280	11.612787
11.432152	712.914224	11.617805
11.500547	696.947658	11.622823
11.442153	688.949790	11.627840
11.618035	698.083619	11.632858
11.419725	717.624414	11.637875
11.390196	703.801202	11.642893
11.768916	691.685448	11.647911
11.630853	699.905281	11.652928
11.866586	719.343257	11.657946
11.493851	710.712076	11.662963
11.852291	687.908785	11.667981
12.057733	679.334987	11.672999
11.457940	693.925165	11.678016
11.691161	666.197001	11.683034
11.408718	669.535037	11.688051
11.524720	690.389033	11.693069
11.754018	693.454960	11.698087
11.388717	708.284967	11.703104
11.523579	700.245317	11.708122
11.687022	700.190895	11.713139
11.545773	689.025597	11.718157
11.966263	701.231050	11.723175
11.775707	713.164364	11.728192
11.656333	690.199446	11.733210
11.660530	683.895398	11.738227
11.573132	704.231994	11.743245
12.067776	689.141984	11.748263
11.671930	685.580281	11.753280
11.562555	689.837002	11.758298
11.725998	695.517530	11.763315
11.712419	681.421304	11.768333
11.811439	700.927309	11.773351
11.746066	690.759826	11.778368
11.988860	682.616546	11.783386
11.811008	690.911041	11.788403
11.517186	684.409753	11.793421
11.593126	697.790045	11.798439
11.701131	704.318190	11.803456
11.916235	711.369241	11.808474
11.703515	705.911834	11.813491
11.583248	700.230447	11.818509
11.617352	691.300317	11.823527
11.571300	703.786161	11.828544
11.639397	708.660430	11.833562
11.795330	712.339798	11.838579
11.918587	692.574255	11.843597
11.639521	706.724050	11.848615
11.831055	707.115848	11.853632
11.893126	693.402966	11.858650
11.814379	706.366625	11.863667
11.993822	713.291520	11.868685
12.195484	706.621653	11.873703
11.678104	714.534790	11.878720
12.002500	710.182096	11.883738
11.911755	722.845767	11.888755
12.046327	735.634867	11.893773
12.319319	714.870110	11.898791
12.174462	711.719459	11.903808
11.830916	708.559331	11.908826
11.991878	707.486502	11.913843
11.971811	725.520300	11.918861
12.104840	710.701190	11.923879
11.943156	737.506424	11.928896
12.284120	720.475972	11.933914
12.299547	709.897692	11.938931
12.033399	719.765721	11.943949
12.125769	736.604007	11.948967
11.842597	738.178679	11.953984
12.081788	722.751031	11.959002
11.926461	718.579354	11.964019
11.933491	723.592130	11.969037
12.369063	711.035488	11.974055
12.021573	709.710159	11.979072
12.375827	725.745127	11.984090
12.275792	729.229756	11.989107
12.136574	723.587702	11.994125
12.433441	702.329189	11.999143
12.183896	727.179776	12.004160
12.221673	715.552413	12.009178
12.183854	710.785492	12.014195
12.040416	745.307282	12.019213
12.205196	721.247021	12.024231
12.143173	710.783382	12.029248
12.094739	721.462448	12.034266
12.164443	721.671087	12.039283
12.245009	720.078026	12.044301
12.401555	713.272245	12.049319
12.414349	711.781009	12.054336
12.422525	726.207479	12.059354
12.486999	740.713414	12.064371
12.543129	727.401179	12.069389
12.834386	700.626684	12.074407
12.401609	713.833942	12.079424
12.423411	718.127737	12.084442
12.445044	718.536788	12.089459
12.212454	725.980837	12.094477
12.732955	724.919733	12.099495
12.393808	730.701730	12.104512
12.387984	726.519416	12.109530
12.417467	708.025605	12.114547
12.290005	717.385413	12.119565
12.365450	736.930389	12.124583
12.669928	739.502929	12.129600
12.833907	721.435574	12.134618
12.812982	712.097217	12.139635
12.514145	729.439198	12.144653
12.682815	717.326549	12.149671
12.675210	720.301745	12.154688
12.331645	718.760765	12.159706
12.711500	704.928645	12.164723
12.171366	703.669886	12.169741
12.942884	727.509548	12.174759
12.703047	741.472921	12.179776
12.845684	711.460264	12.184794
13.125338	697.487370	12.189811
12.696073	714.291689	12.194829
12.770682	717.263433	12.199847
12.831220	717.344094	12.204864
12.687032	710.630619	12.209882
12.797636	708.126542	12.214899
12.646698	716.100055	12.219917
12.992130	703.452143	12.224935
12.743192	700.621564	12.229952
12.832715	703.935432	12.234970
13.194823	702.975583	12.239987
12.540025	717.753073	12.245005
12.692748	716.421143	12.250023
12.803322	701.536972	12.255040
12.844058	726.204684	12.260058
12.894172	709.264815	12.265075
12.808334	704.937604	12.270093
12.963847	706.387627	12.275111
12.890270	715.339621	12.280128
12.543586	708.967794	12.285146
12.954768	699.279669	12.290163
12.525836	698.376940	12.295181
12.982341	721.644902	12.300199
12.970586	750.978826	12.305216
12.993203	747.666866	12.310234
13.220332	722.482426	12.315251
13.017626	710.451719	12.320269
12.955676	709.114823	12.325287
12.933529	718.512725	12.330304
12.916734	728.403906	12.335322
13.077251	718.449204	12.340339
12.733143	733.022652	12.345357
12.745596	758.172224	12.350375
12.996185	745.227928	12.355392
12.844802	751.327235	12.360410
13.243493	735.717648	12.365427
12.904408	744.909251	12.370445
12.905483	751.299027	12.375463
12.988016	736.849852	12.380480
12.893610	734.353179	12.385498
13.250828	722.963101	12.390515
12.834840	744.818911	12.395533
13.051164	734.094651	12.400551
13.100215	730.235166	12.405568
13.230664	731.431037	12.410586
13.224887	742.787529	12.415603
13.201800	747.238120	12.420621
13.271671	721.071378	12.425639
13.189369	722.854619	12.430656
13.159668	742.742186	12.435674
13.440781	757.143162	12.440691
13.315701	753.016956	12.445709
13.517035	734.421112	12.450727
13.363491	728.503054	12.455744
13.234696	730.961416	12.460762
13.302161	731.695874	12.465779
13.206319	724.685111	12.470797
13.241590	738.517904	12.475815
13.734770	747.317712	12.480832
13.130449	739.768795	12.485850
13.717989	738.444614	12.490867
13.429007	753.595722	12.495885
13.258534	726.178387	12.500903
13.165891	723.558820	12.505920
13.299491	746.423809	12.510938
13.694753	756.081604	12.515955
13.454755	769.969460	12.520973
13.659491	766.927123	12.525991
13.524641	758.806554	12.531008
13.639668	747.690275	12.536026
13.496658	750.341293	12.541043
13.072312	745.037216	12.546061
13.905437	736.069286	12.551079
13.885197	750.223187	12.556096
13.598697	727.208096	12.561114
13.661267	729.306675	12.566131
13.293296	733.203790	12.571149
13.677830	731.717737	12.576167
13.525269	734.185635	12.581184
13.630246	754.542758	12.586202
13.953800	752.746590	12.591219
13.279408	748.463097	12.596237
13.555614	765.839486	12.601255
13.796437	748.261333	12.606272
13.828324	760.532429	12.611290
13.856160	760.143229	12.616307
14.035488	758.006622	12.621325
13.560775	745.865859	12.626343
13.659281	748.311359	12.631360
13.679417	742.705350	12.636378
14.145689	737.798735	12.641395
13.693253	746.699410	12.646413
13.750094	752.700054	12.651431
13.986550	745.880857	12.656448
13.577018	730.235296	12.661466
14.169908	734.506651	12.666483
13.477600	758.643760	12.671501
13.908377	757.817403	12.676519
14.268137	759.144628	12.681536
13.953663	764.177288	12.686554
13.812191	746.656998	12.691571
13.667741	740.658123	12.696589
14.208076	738.541663	12.701607
14.084924	740.095007	12.706624
13.792968	754.016526	12.711642
13.931265	744.917219	12.716659
14.034514	761.841016	12.721677
13.787259	752.316671	12.726695
14.009942	752.666128	12.731712
13.755777	752.974732	12.736730
13.874364	757.491161	12.741747
13.661939	747.122018	12.746765
13.788784	755.374462	12.751783
14.023672	776.097344	12.756800
13.776279	761.049101	12.761818
14.121917	742.358160	12.766835
13.832051	764.581732	12.771853
13.810525	770.808367	12.776871
14.235994	754.770729	12.781888
13.814630	756.414387	12.786906
14.110783	779.250398	12.791923
14.330021	777.174203	12.796941
14.197266	786.268956	12.801959
14.184811	771.743441	12.806976
14.116725	767.277980	12.811994
14.266114	753.796808	12.817011
14.433411	753.322866	12.822029
14.203832	763.847989	12.827047
14.433721	757.421597	12.832064
14.337661	764.120167	12.837082
14.479916	742.970196	12.842099
14.331470	751.308277	12.847117
14.201484	764.490534	12.852135
14.515488	757.412126	12.857152
14.128446	758.979561	12.862170
14.076486	739.639559	12.867187
14.373336	755.684832	12.872205
14.144115	790.835106	12.877223
14.759638	767.506862	12.882240
14.410450	772.568483	12.887258
14.450187	768.167071	12.892275
14.744342	784.154173	12.897293
14.403142	772.335426	12.902311
14.500693	756.157737	12.907328
14.525184	762.112661	12.912346
14.518921	746.489001	12.917363
14.366780	762.972750	12.922381
14.415084	777.767143	12.927399
14.792136	757.038761	12.932416
14.302445	759.623481	12.937434
14.559835	774.607963	12.942451
14.962023	785.883196	12.947469
14.492551	772.167162	12.952487
14.376467	752.816780	12.957504
14.666717	782.367518	12.962522
14.535617	783.538326	12.967539
15.058775	774.000995	12.972557
14.870393	784.228358	12.977575
14.725877	755.390130	12.982592
14.529186	755.268385	12.987610
14.554135	753.521071	12.992627
14.703137	770.892115	12.997645
14.463854	769.358497	13.002663
14.764974	775.112046	13.007680
14.731230	770.222615	13.012698
14.822310	786.789295	13.017715
14.762876	790.558784	13.022733
14.592368	772.749148	13.027751
14.916376	778.549690	13.032768
15.091838	809.989423	13.037786
14.596766	805.752245	13.042803
15.052530	781.727048	13.047821
14.699296	788.457697	13.052839
14.865829	789.459864	13.057856
14.760082	807.013364	13.062874
14.771314	790.048640	13.067891
14.796180	766.125768	13.072909
14.716161	780.696357	13.077927
14.457703	789.101739	13.082944
14.706259	788.480938	13.087962
14.658816	781.091581	13.092979
14.746569	767.973441	13.097997
14.840559	773.121232	13.103015
15.182559	801.679860	13.108032
14.879506	790.677804	13.113050
14.959380	793.638853	13.118067
15.118712	799.181948	13.123085
14.970269	823.443400	13.128103
15.329833	813.284431	13.133120
15.286270	797.466640	13.138138
15.252162	777.519765	13.143155
15.310763	786.270479	13.148173
15.072718	785.408425	13.153191
15.096402	774.745687	13.158208
15.127688	784.740444	13.163226
14.928728	783.916014	13.168243
15.202406	764.984838	13.173261
15.054926	770.901864	13.178279
15.286921	778.171946	13.183296
15.277095	809.042457	13.188314
15.447993	801.841062	13.193331
15.377619	783.000176	13.198349
15.259742	769.551448	13.203367
15.048118	773.895739	13.208384
15.239931	781.516564	13.213402
15.527123	787.668672	13.218419
15.555987	773.298489	13.223437
15.252538	784.242220	13.228455
15.210592	791.779271	13.233472
15.207899	778.391893	13.238490
15.664599	780.030178	13.243507
15.541092	787.536425	13.248525
15.372743	786.524406	13.253543
15.354898	771.244964	13.258560
15.202052	793.892962	13.263578
15.274931	802.675077	13.268595
15.528907	785.561414	13.273613
15.463311	797.711284	13.278631
15.649443	808.524240	13.283648
15.814676	803.215898	13.288666
15.449334	806.625718	13.293683
15.735605	799.199506	13.298701
15.397654	807.303552	13.303719
15.407592	792.618453	13.308736
15.761153	809.078018	13.313754
15.652780	796.838889	13.318771
16.089057	807.440573	13.323789
15.516779	799.116357	13.328807
15.657262	801.679208	13.333824
15.743860	783.302703	13.338842
15.350074	787.120655	13.343859
15.627867	789.989662	13.348877
15.487874	803.997403	13.353895
15.544274	803.020566	13.358912
15.535010	786.845833	13.363930
15.403527	798.153080	13.368947
15.766951	815.597473	13.373965
15.342610	816.329371	13.378983
15.524605	791.677826	13.384000
15.428681	797.849461	13.389018
15.557876	823.568471	13.394035
15.882255	826.262705	13.399053
15.734261	824.355527	13.404071
16.104703	813.326487	13.409088
16.283713	826.012085	13.414106
16.076831	816.480044	13.419123
16.146006	799.652742	13.424141
16.141290	800.481295	13.429159
15.784107	788.978872	13.434176
16.045449	797.343033	13.439194
15.815822	786.910778	13.444211
16.037173	799.476592	13.449229
15.905300	805.640002	13.454247
15.827923	782.117659	13.459264
15.890782	794.612246	13.464282
15.780736	819.632890	13.469299
16.002673	823.347921	13.474317
15.998125	827.743812	13.479335
15.713793	848.268811	13.484352
16.455503	845.296933	13.489370
16.095737	825.283960	13.494387
16.198887	832.165626	13.499405
16.464311	817.459636	13.504423
16.279209	819.528604	13.509440
16.452439	833.007670	13.514458
16.362944	844.093698	13.519475
16.252831	826.525331	13.524493
15.918016	809.805023	13.529511
16.005603	817.327371	13.534528
16.269008	824.796365	13.539546
15.978747	834.552833	13.544563
16.588576	817.949666	13.549581
16.458850	819.266471	13.554599
16.517692	819.370144	13.559616
16.393853	825.146607	13.564634
16.419516	821.043491	13.569651
16.594649	830.364187	13.574669
16.130546	836.542266	13.579687
16.338489	818.132973	13.584704
16.540466	815.136150	13.589722
16.293093	830.952328	13.594739
16.565125	827.262314	13.599757
16.513232	830.436826	13.604775
16.778414	810.047247	13.609792
16.797178	810.025097	13.614810
16.280721	809.509167	13.619827
16.361296	797.073011	13.624845
16.144646	807.755926	13.629863
16.282667	832.846495	13.634880
16.544301	826.751846	13.639898
16.201770	821.721056	13.644915
16.602323	818.274696	13.649933
16.278188	828.381057	13.654951
16.437751	829.115454	13.659968
16.419790	815.604516	13.664986
16.293353	820.857727	13.670003
16.464339	830.408674	13.675021
16.706903	844.606317	13.680039
16.687962	839.906197	13.685056
17.072337	841.222966	13.690074
16.659919	852.876599	13.695091
16.935900	846.708232	13.700109
16.643232	832.710040	13.705127
16.573719	819.892378	13.710144
17.005093	838.244517	13.715162
16.935502	863.455938	13.720179
17.284335	840.889969	13.725197
16.708840	817.681617	13.730215
16.456506	823.493189	13.735232
16.656135	825.327070	13.740250
16.858580	839.141775	13.745267
17.066903	856.796246	13.750285
17.164521	842.112846	13.755303
17.527284	829.981120	13.760320
17.239645	803.901556	13.765338
16.876211	821.301646	13.770355
17.153729	814.397012	13.775373
16.948915	803.961038	13.780391
16.954738	802.837088	13.785408
17.028350	802.225517	13.790426
16.554599	809.003150	13.795443
16.817936	813.390684	13.800461
17.312075	828.398284	13.805479
17.333940	839.288296	13.810496
17.330342	813.891014	13.815514
17.073277	810.622405	13.820531
17.029859	812.107181	13.825549
17.376532	810.653060	13.830567
17.471352	794.793708	13.835584
17.335671	800.991004	13.840602
17.050822	818.472764	13.845619
17.459431	813.017633	13.850637
17.307334	795.025645	13.855655
17.003955	815.415399	13.860672
17.346159	806.714921	13.865690
16.766437	804.565985	13.870707
17.183060	819.145656	13.875725
17.547133	830.834594	13.880743
17.382759	828.256875	13.885760
17.757273	839.418248	13.890778
17.521982	826.731984	13.895795
17.347643	791.465867	13.900813
17.515532	800.613477	13.905831
17.223042	815.654626	13.910848
17.470350	801.637979	13.915866
17.122456	803.775075	13.920883
17.385754	822.877516	13.925901
17.465328	818.011557	13.930919
17.368296	824.587511	13.935936
17.450662	826.960318	13.940954
17.505387	825.655792	13.945971
17.651973	843.505932	13.950989
17.500034	827.184799	13.956007
17.442346	840.096482	13.961024
17.611830	837.269548	13.966042
17.774739	832.935633	13.971059
17.624768	820.641565	13.976077
17.882893	825.600187	13.981095
17.422836	840.935713	13.986112
17.823782	848.367624	13.991130
17.642205	852.739936	13.996147
17.427706	830.851959	14.001165
17.500168	834.531473	14.006183
17.461301	838.360060	14.011200
17.671329	834.315721	14.016218
17.097437	847.226418	14.021235
17.531175	841.608702	14.026253
17.692698	860.721218	14.031271
17.920593	857.004543	14.036288
18.588559	852.045572	14.041306
18.072528	848.644696	14.046323
18.014131	852.435087	14.051341
18.259021	828.386511	14.056359
18.007291	815.438278	14.061376
18.265123	817.974851	14.066394
18.140699	844.706910	14.071411
17.947082	834.506503	14.076429
18.306610	811.986041	14.081447
17.981212	825.911774	14.086464
18.338085	846.920026	14.091482
17.977058	836.456118	14.096499
17.948571	817.866663	14.101517
18.366211	813.705562	14.106535
17.862928	836.550179	14.111552
18.101581	838.197640	14.116570
17.794975	830.660093	14.121587
17.715596	824.507261	14.126605
18.031151	813.814467	14.131623
17.814211	827.165044	14.136640
18.275445	825.447763	14.141658
17.961914	829.358341	14.146675
18.424518	852.647045	14.151693
18.140936	844.312292	14.156711
18.141466	829.545762	14.161728
18.677956	833.915222	14.166746
18.348752	838.313795	14.171763
18.297590	846.115319	14.176781
18.495239	822.916757	14.181799
18.346130	822.059487	14.186816
18.101765	820.571967	14.191834
18.285296	842.340357	14.196851
18.500914	849.261304	14.201869
18.252456	833.903600	14.206887
18.127798	859.717167	14.211904
18.400811	859.322774	14.216922
18.535492	859.529927	14.221939
18.370007	870.740314	14.226957
18.496652	871.017872	14.231975
18.152827	860.614770	14.236992
18.276410	850.555977	14.242010
18.493379	854.793845	14.247027
18.555891	857.301301	14.252045
18.555064	859.246736	14.257063
18.387407	850.490762	14.262080
18.420070	856.808648	14.267098
18.725401	872.759361	14.272115
18.259865	866.763805	14.277133
18.227808	864.096614	14.282151
18.172644	873.183515	14.287168
18.800645	886.405930	14.292186
18.891063	887.092815	14.297203
18.697651	887.093821	14.302221
18.925403	867.984920	14.307239
18.930569	897.806162	14.312256
19.051196	883.944493	14.317274
18.913649	872.257915	14.322291
18.976584	883.683353	14.327309
19.050732	874.296321	14.332327
19.108323	870.561243	14.337344
19.139988	849.717808	14.342362
18.829424	851.679200	14.347379
18.573441	843.581949	14.352397
18.774324	849.253396	14.357415
18.960671	875.995851	14.362432
18.792022	873.202352	14.367450
18.889810	879.609164	14.372467
19.048111	897.551600	14.377485
19.264367	879.294757	14.382503
18.992944	878.022671	14.387520
19.214779	860.870841	14.392538
19.432255	874.856770	14.397555
19.200991	893.022000	14.402573
19.389130	881.685033	14.407591
19.081280	855.320312	14.412608
19.056834	869.475216	14.417626
19.125489	887.845142	14.422643
19.128535	886.788950	14.427661
19.162205	889.987613	14.432679
19.262077	891.007002	14.437696
19.461266	874.715664	14.442714
19.401935	886.928727	14.447731
19.486500	880.236906	14.452749
19.314044	857.406263	14.457767
19.375022	870.841232	14.462784
19.575877	881.018409	14.467802
19.233256	867.831872	14.472819
19.117580	853.910092	14.477837
19.431403	852.853911	14.482855
19.476413	885.067620	14.487872
19.554027	878.394070	14.492890
19.423756	873.842323	14.497907
19.082616	887.722301	14.502925
19.677013	884.324582	14.507943
19.580726	876.387783	14.512960
19.389791	881.873663	14.517978
19.174137	881.804546	14.522995
19.194071	886.700509	14.528013
19.383382	872.950105	14.533031
19.268619	863.380672	14.538048
19.337043	879.870411	14.543066
19.520916	873.085332	14.548083
19.189062	866.842842	14.553101
19.762535	879.218481	14.558119
19.392936	893.526285	14.563136
19.788185	914.057052	14.568154
20.040942	914.410694	14.573171
20.100713	903.868937	14.578189
20.172048	870.390995	14.583207
19.610785	866.382101	14.588224
19.806129	875.989961	14.593242
19.866947	880.109091	14.598259
19.503405	875.363768	14.603277
19.640464	862.410976	14.608295
20.037059	892.372490	14.613312
20.036795	905.570037	14.618330
20.041104	893.998350	14.623347
19.551154	896.952921	14.628365
20.164948	906.539866	14.633383
20.057807	904.216978	14.638400
20.034014	894.443270	14.643418
20.427538	898.794752	14.648435
19.736605	895.003784	14.653453
20.051382	897.601611	14.658471
20.045430	904.124665	14.663488
19.763266	892.044854	14.668506
19.985154	910.496151	14.673523
19.745495	906.973036	14.678541
19.860468	909.961764	14.683559
20.133812	920.222141	14.688576
19.960325	905.004004	14.693594
20.165536	889.467168	14.698611
19.815140	910.041544	14.703629
20.154845	894.942299	14.708647
19.943546	893.687238	14.713664
19.818994	912.010204	14.718682
20.282198	921.335504	14.723699
20.613612	919.755483	14.728717
20.572717	922.832257	14.733735
20.467460	921.796518	14.738752
20.646400	926.310798	14.743770
20.500303	912.603682	14.748787
20.174500	904.516559	14.753805
20.714966	909.242379	14.758823
20.735475	905.621167	14.763840
20.336269	908.393957	14.768858
20.519848	896.960120	14.773875
20.356215	913.327064	14.778893
20.490003	898.321966	14.783911
20.664100	899.024839	14.788928
20.799143	907.924956	14.793946
20.626292	914.044899	14.798963
20.408367	911.997436	14.803981
20.483487	904.323758	14.808999
20.789342	911.203253	14.814016
20.793576	908.666144	14.819034
21.160859	917.732758	14.824051
20.708215	892.511689	14.829069
21.025259	883.712793	14.834087
20.515540	897.500000	14.839104
20.363554	889.210486	14.844122
20.684500	894.252721	14.849139
20.618464	908.660336	14.854157
20.833727	919.309149	14.859175
21.109082	912.506476	14.864192
21.017813	917.356865	14.869210
21.222538	922.628202	14.874227
20.938635	910.312799	14.879245
20.875702	890.071011	14.884263
20.628553	889.929264	14.889280
20.523713	907.057938	14.894298
20.845928	915.275330	14.899315
20.740682	940.664379	14.904333
20.743307	922.405691	14.909351
21.036097	910.211961	14.914368
20.998254	913.124787	14.919386
21.096429	924.363376	14.924403
21.099347	929.234908	14.929421
21.318192	927.131896	14.934439
21.285458	936.639429	14.939456
21.232396	932.345112	14.944474
21.446266	928.858828	14.949491
21.441063	926.919283	14.954509
21.381691	900.007746	14.959527
21.290207	904.864662	14.964544
21.152357	929.953452	14.969562
21.346091	941.365879	14.974579
21.302727	918.234454	14.979597
21.192410	921.360585	14.984615
21.620558	922.955388	14.989632
21.423566	926.464645	14.994650
21.548372	917.106017	14.999667
21.015858	930.381996	15.004685
21.115472	931.475034	15.009703
21.224287	919.902294	15.014720
21.169451	921.480676	15.019738
21.258013	929.442472	15.024755
21.146252	930.933634	15.029773
21.029271	927.907628	15.034791
21.639334	937.102692	15.039808
21.780115	963.435221	15.044826
22.065687	959.951152	15.049843
21.866422	927.078388	15.054861
21.663664	908.419910	15.059879
21.451406	917.855353	15.064896
21.232848	941.615522	15.069914
21.797348	933.188593	15.074931
21.998207	936.991660	15.079949
22.075019	932.810492	15.084967
21.935657	921.638709	15.089984
21.644880	931.842945	15.095002
21.866359	918.741150	15.100019
21.988987	906.629071	15.105037
21.769285	907.589490	15.110055
21.849744	915.723144	15.115072
21.750372	910.547739	15.120090
21.927492	911.769663	15.125107
22.167126	927.869936	15.130125
22.209008	930.733773	15.135143
22.095578	919.140787	15.140160
21.803679	911.928833	15.145178
22.119298	921.540757	15.150195
22.248179	900.910656	15.155213
21.963558	900.831877	15.160231
22.133696	905.941448	15.165248
21.893896	928.433291	15.170266
21.935911	912.936094	15.175283
21.748867	912.841092	15.180301
22.076312	926.198915	15.185319
22.152578	946.101117	15.190336
22.045944	954.477368	15.195354
22.519620	925.644211	15.200371
22.354035	947.832162	15.205389
21.899065	951.619035	15.210407
21.940590	930.810662	15.215424
21.936097	947.868286	15.220442
22.371380	955.540673	15.225459
22.468327	941.877893	15.230477
22.259376	934.831703	15.235495
22.290641	938.808822	15.240512
22.336448	956.115361	15.245530
22.392617	933.190833	15.250547
22.443693	930.090316	15.255565
22.321059	941.362848	15.260583
22.247220	948.794645	15.265600
22.235051	952.951047	15.270618
22.249336	931.998098	15.275635
22.512793	942.269570	15.280653
22.400628	967.310684	15.285671
22.917557	962.787752	15.290688
22.786920	964.839965	15.295706
22.679575	950.716772	15.300723
22.661969	968.525804	15.305741
22.609901	968.778087	15.310759
22.837378	956.146803	15.315776
22.871284	949.431244	15.320794
22.866637	954.614782	15.325811
23.055537	966.982212	15.330829
22.757000	969.506645	15.335847
22.910102	939.896727	15.340864
22.483670	928.478162	15.345882
22.595001	958.651668	15.350899
23.020831	956.754936	15.355917
22.379606	973.211396	15.360935
23.033681	982.315377	15.365952
22.676254	977.214673	15.370970
23.130115	971.715797	15.375987
23.357839	971.773654	15.381005
22.923872	958.707420	15.386023
23.046607	957.904702	15.391040
22.900234	966.913842	15.396058
22.970640	983.906781	15.401075
23.049896	976.021905	15.406093
22.942656	971.935102	15.411111
23.206733	954.507062	15.416128
23.185118	969.470832	15.421146
23.230922	972.127782	15.426163
22.779145	960.876135	15.431181
22.882209	969.168738	15.436199
23.230729	964.935084	15.441216
22.909623	993.053398	15.446234
23.164301	986.999097	15.451251
23.773737	980.269893	15.456269
23.647552	997.559932	15.461287
23.522940	973.915408	15.466304
23.670892	963.578273	15.471322
23.444809	973.885596	15.476339
23.114993	963.904803	15.481357
23.332090	960.948650	15.486375
23.997646	960.310594	15.491392
23.436150	945.166671	15.496410
23.614467	939.798161	15.501427
23.614008	947.556918	15.506445
23.458127	966.191742	15.511463
23.547578	961.976005	15.516480
23.437505	957.402101	15.521498
23.688793	968.910425	15.526515
23.616075	958.395739	15.531533
23.684995	975.092139	15.536551
23.841156	972.390185	15.541568
23.797965	974.802164	15.546586
23.644859	977.125445	15.551603
23.892025	966.844433	15.556621
23.557522	962.689801	15.561639
23.796211	962.065508	15.566656
23.891169	991.560857	15.571674
23.867681	981.961998	15.576691
24.032285	966.786133	15.581709
23.843861	985.027443	15.586727
24.121291	991.972877	15.591744
24.132042	987.207782	15.596762
24.134653	968.012566	15.601779
23.737262	960.695907	15.606797
23.610670	977.964934	15.611815
23.860349	993.822142	15.616832
23.892689	991.711368	15.621850
23.788141	970.799749	15.626867
24.062069	976.680081	15.631885
23.865212	986.034006	15.636903
23.905941	1001.158819	15.641920
23.890066	990.858283	15.646938
23.934910	972.986257	15.651955
24.281028	990.237501	15.656973
23.984036	1028.331234	15.661991
24.167761	1018.592625	15.667008
24.321764	1010.240302	15.672026
24.536109	1016.873002	15.677043
24.650175	1009.771061	15.682061
24.372771	1017.548337	15.687079
24.371432	1015.807600	15.692096
24.459512	1014.626056	15.697114
24.641018	1013.985627	15.702131
24.679540	999.320820	15.707149
24.017090	1005.552407	15.712167
24.418411	1010.848359	15.717184
24.660846	1008.372435	15.722202
24.573094	995.465931	15.727219
24.588312	1009.739181	15.732237
24.594852	1004.662256	15.737255
24.841803	995.344896	15.742272
25.053990	1012.895171	15.747290
25.076387	1016.927404	15.752307
24.853928	975.224595	15.757325
24.773797	966.382160	15.762343
24.607318	980.365117	15.767360
24.711768	989.744824	15.772378
24.877858	977.733845	15.777395
24.722539	979.904677	15.782413
24.406193	981.053664	15.787431
24.885980	997.131741	15.792448
24.959491	1004.007460	15.797466
24.719898	1013.434958	15.802483
25.033956	1010.446168	15.807501
24.882919	1003.898515	15.812519
24.971050	1010.604835	15.817536
25.005535	1011.296713	15.822554
24.999678	994.737263	15.827571
24.955071	984.957097	15.832589
24.906969	1010.739965	15.837607
25.035316	1005.259347	15.842624
25.073393	987.765394	15.847642
25.012487	995.671727	15.852659
25.204717	992.482435	15.857677
24.850279	988.262603	15.862695
25.197646	997.570783	15.867712
25.168978	1004.739499	15.872730
24.597250	1003.182368	15.877747
25.311240	1010.090306	15.882765
25.113903	1024.948729	15.887783
25.386840	1029.465514	15.892800
25.591821	1019.701940	15.897818
25.600621	1024.902172	15.902835
25.880533	1023.631166	15.907853
25.561895	1025.062748	15.912871
25.510264	1013.500904	15.917888
25.233795	1005.521514	15.922906
25.297914	1003.687994	15.927923
25.802317	1015.607831	15.932941
25.408898	1023.612522	15.937959
25.439546	1023.746538	15.942976
25.547293	1020.166381	15.947994
25.673192	1019.669654	15.953011
26.093059	1019.809806	15.958029
25.693651	1044.535317	15.963047
25.653637	1045.318449	15.968064
26.094701	1024.175193	15.973082
25.580089	1012.537042	15.978099
25.827816	1018.613503	15.983117
25.852485	1026.850703	15.988135
25.838100	1022.893387	15.993152
25.916353	1019.079779	15.998170
25.975331	1032.999352	16.003187
26.041632	1030.727881	16.008205
26.112260	1020.624099	16.013223
25.600522	1007.817094	16.018240
25.850295	1008.883257	16.023258
25.990424	1032.385403	16.028275
26.305500	1019.256149	16.033293
26.114168	1021.827621	16.038311
26.052477	1020.727998	16.043328
26.260488	1021.986843	16.048346
25.980287	1019.022428	16.053363
26.246166	1017.669118	16.058381
26.247746	1025.524698	16.063399
26.027734	1023.759678	16.068416
25.872304	1030.876046	16.073434
26.142346	1032.135367	16.078451
26.078115	1014.494158	16.083469
26.220081	1009.088556	16.088487
26.147088	1028.618363	16.093504
26.522412	1019.466145	16.098522
26.151580	1025.425295	16.103539
26.219908	1036.967938	16.108557
26.364398	1029.012723	16.113575
26.408013	1006.950500	16.118592
26.488039	1009.370266	16.123610
26.440101	1049.560743	16.128627
26.785057	1032.578582	16.133645
26.849857	1040.863771	16.138663
26.719556	1023.287098	16.143680
26.662294	1020.255042	16.148698
26.723884	1022.571879	16.153715
26.692095	1020.451822	16.158733
26.637880	1009.617316	16.163751
26.541428	1025.183197	16.168768
26.628455	1022.412954	16.173786
26.694039	1033.333961	16.178803
26.757934	1012.723993	16.183821
26.970260	1031.659376	16.188839
26.881136	1039.627271	16.193856
26.601211	1041.342148	16.198874
26.747640	1033.954381	16.203891
26.651637	1017.297603	16.208909
26.543007	1029.332359	16.213927
26.796964	1050.504221	16.218944
26.768206	1037.737304	16.223962
26.722209	1026.877787	16.228979
26.735903	1032.308946	16.233997
26.720998	1033.281187	16.239015
27.084111	1051.553451	16.244032
27.740403	1067.840664	16.249050
27.252520	1054.247761	16.254067
27.312497	1052.956221	16.259085
27.138472	1047.782184	16.264103
27.196083	1043.383053	16.269120
27.119867	1037.527667	16.274138
26.874031	1045.259421	16.279155
27.369071	1056.398184	16.284173
27.296648	1083.028881	16.289191
27.417141	1077.662794	16.294208
27.470176	1058.850177	16.299226
27.609009	1071.257552	16.304243
27.577232	1084.411458	16.309261
27.592142	1078.760531	16.314279
27.520040	1056.795365	16.319296
27.753627	1071.237359	16.324314
27.653218	1068.264971	16.329331
27.798337	1064.138211	16.334349
27.480992	1041.622008	16.339367
27.408273	1051.494989	16.344384
27.633947	1053.394361	16.349402
27.457227	1067.278031	16.354419
27.523033	1070.853512	16.359437
27.768621	1061.059290	16.364455
27.697415	1072.781870	16.369472
27.668769	1053.792646	16.374490
27.426822	1065.825550	16.379507
27.745369	1065.282128	16.384525
27.809625	1070.888659	16.389543
27.585201	1065.291752	16.394560
27.918029	1059.679120	16.399578
27.792047	1072.833527	16.404595
27.645436	1090.161978	16.409613
27.842009	1091.230149	16.414631
27.783407	1081.625714	16.419648
28.037855	1085.808548	16.424666
28.174691	1098.691946	16.429683
27.936407	1103.899383	16.434701
28.483279	1088.124631	16.439719
27.871291	1072.676305	16.444736
28.129840	1079.247237	16.449754
27.892524	1090.953788	16.454771
28.431661	1092.314378	16.459789
28.449184	1078.244429	16.464807
28.396713	1067.315695	16.469824
28.165094	1077.079749	16.474842
28.230320	1098.739740	16.479859
28.271535	1093.695727	16.484877
28.522087	1092.950306	16.489895
28.348550	1079.387894	16.494912
28.453647	1083.649528	16.499930
28.376405	1091.136963	16.504947
28.426709	1072.640647	16.509965
28.439810	1083.748763	16.514983
28.587671	1111.790192	16.520000
28.967322	1116.480561	16.525018
29.127911	1099.111180	16.530035
28.904955	1077.587149	16.535053
28.778793	1084.004093	16.540071
28.789843	1083.245802	16.545088
28.622577	1075.793445	16.550106
28.685749	1076.989933	16.555123
28.615156	1075.039330	16.560141
28.745767	1074.097641	16.565159
28.899266	1081.488392	16.570176
28.818254	1078.118898	16.575194
28.644937	1071.869903	16.580211
28.468822	1087.702812	16.585229
28.856885	1076.780682	16.590247
28.756281	1098.318115	16.595264
28.890450	1097.719452	16.600282
28.823592	1103.810147	16.605299
28.711898	1118.892074	16.610317
28.999262	1109.523685	16.615335
28.905464	1095.260358	16.620352
28.862947	1119.269892	16.625370
29.029674	1118.090006	16.630387
29.464295	1115.960658	16.635405
29.579335	1136.700590	16.640423
29.167002	1129.063661	16.645440
29.394373	1117.561906	16.650458
29.310220	1114.809799	16.655475
29.388547	1106.425132	16.660493
29.243409	1108.776145	16.665511
29.189615	1135.535122	16.670528
29.673526	1118.304664	16.675546
29.463844	1139.752528	16.680563
29.499888	1137.765107	16.685581
29.697142	1128.245989	16.690599
29.464279	1133.201814	16.695616
29.850764	1128.497684	16.700634
29.708114	1135.042835	16.705651
29.567017	1147.200146	16.710669
29.911100	1118.168116	16.715687
29.713790	1124.693070	16.720704
29.368021	1132.494027	16.725722
29.861383	1138.539588	16.730739
29.932208	1126.866893	16.735757
30.092367	1122.575172	16.740775
29.661686	1128.399012	16.745792
29.819938	1142.610078	16.750810
29.954445	1143.094166	16.755827
29.787166	1133.428838	16.760845
30.097089	1109.956232	16.765863
29.711521	1139.186180	16.770880
29.752529	1129.359399	16.775898
29.921321	1126.644211	16.780915
29.789681	1117.463731	16.785933
30.300745	1127.914633	16.790951
30.140398	1147.254869	16.795968
30.163470	1139.751544	16.800986
30.417614	1124.007909	16.806003
30.260550	1118.619580	16.811021
30.225208	1119.970210	16.816039
30.439484	1134.366059	16.821056
30.086497	1121.238184	16.826074
30.120169	1120.614210	16.831091
29.900981	1135.755245	16.836109
30.306766	1133.670907	16.841127
29.964629	1149.984748	16.846144
30.136218	1168.839062	16.851162
30.703497	1155.291728	16.856179
30.479369	1150.833243	16.861197
30.641899	1141.995183	16.866215
30.616551	1154.010469	16.871232
30.763287	1141.383321	16.876250
30.870401	1155.017068	16.881267
30.778383	1154.622276	16.886285
30.825959	1147.588504	16.891303
30.962608	1169.360680	16.896320
31.139649	1148.414881	16.901338
31.319203	1128.121192	16.906355
30.572087	1124.318587	16.911373
30.592820	1126.731048	16.916391
30.742877	1142.525857	16.921408
30.889745	1132.567435	16.926426
31.157339	1145.193988	16.931443
31.200862	1156.727340	16.936461
31.326965	1163.255940	16.941479
30.921825	1133.244217	16.946496
30.725402	1103.057152	16.951514
30.952796	1122.429716	16.956531
30.682408	1157.157229	16.961549
31.004501	1141.372630	16.966567
31.189824	1134.960629	16.971584
31.021635	1139.416616	16.976602
31.027870	1154.875056	16.981619
31.149132	1164.916007	16.986637
31.119831	1143.094395	16.991655
31.035708	1138.064290	16.996672
31.096731	1135.188803	17.001690
31.184610	1152.797297	17.006707
31.067589	1165.433697	17.011725
31.493366	1177.031032	17.016743
31.427714	1194.992130	17.021760
31.696453	1189.956736	17.026778
31.882347	1170.572060	17.031795
31.484568	1183.567392	17.036813
31.749383	1161.854790	17.041831
31.726756	1157.321677	17.046848
31.492146	1183.081044	17.051866
31.781740	1187.229070	17.056883
31.867135	1187.572788	17.061901
31.953176	1167.819865	17.066919
31.976884	1161.584229	17.071936
31.778904	1167.527661	17.076954
31.898622	1191.059919	17.081971
31.768676	1179.628874	17.086989
31.728197	1153.713724	17.092007
31.987219	1170.409723	17.097024
31.291365	1161.894951	17.102042
31.649438	1183.359166	17.107059
31.929746	1186.284021	17.112077
31.992222	1171.011767	17.117095
32.014510	1167.564371	17.122112
31.596644	1158.424768	17.127130
31.863046	1178.913519	17.132147
31.733991	1211.057196	17.137165
32.229816	1188.848814	17.142183
32.224903	1190.930957	17.147200
31.955492	1197.411473	17.152218
32.390282	1201.091521	17.157235
32.110484	1197.501466	17.162253
32.282625	1203.415829	17.167271
32.611600	1197.601568	17.172288
32.357213	1199.159719	17.177306
32.251241	1190.592521	17.182323
32.415022	1217.776601	17.187341
32.474062	1192.418523	17.192359
32.466438	1188.092221	17.197376
32.401170	1213.438512	17.202394
32.641482	1231.719871	17.207411
32.517098	1221.101364	17.212429
32.546000	1202.215903	17.217447
32.685903	1213.963041	17.222464
32.805361	1230.881334	17.227482
32.850515	1219.552396	17.232499
33.192949	1212.464259	17.237517
33.174600	1205.270726	17.242535
33.204584	1217.883467	17.247552
33.130623	1221.670223	17.252570
33.265774	1195.693112	17.257587
33.073347	1186.848442	17.262605
33.174418	1171.725284	17.267623
33.242140	1173.996063	17.272640
33.145230	1176.549695	17.277658
33.326233	1180.509414	17.282675
32.813676	1198.859253	17.287693
32.822195	1186.642315	17.292711
33.080414	1174.608578	17.297728
32.884844	1184.544948	17.302746
33.386552	1208.231478	17.307763
33.313846	1219.036920	17.312781
33.562247	1218.374407	17.317799
33.461437	1216.324375	17.322816
33.178851	1209.628039	17.327834
33.440818	1195.419973	17.332851
33.144751	1206.919345	17.337869
33.060158	1219.805881	17.342887
33.397281	1220.445125	17.347904
33.207837	1218.869571	17.352922
33.533823	1191.141756	17.357939
33.282995	1206.104275	17.362957
33.346651	1211.665988	17.367975
33.585904	1212.757029	17.372992
33.513078	1229.481165	17.378010
33.985011	1241.569721	17.383027
33.713801	1243.762200	17.388045
33.746238	1261.259734	17.393063
34.195290	1244.612712	17.398080
33.931988	1236.734322	17.403098
34.032779	1231.593727	17.408115
33.982543	1239.579703	17.413133
34.161682	1222.785817	17.418151
34.328435	1229.221528	17.423168
33.814767	1240.328540	17.428186
34.325864	1227.170652	17.433203
34.154848	1226.348270	17.438221
34.103416	1226.267165	17.443239
34.246080	1237.338928	17.448256
34.269065	1255.139421	17.453274
34.503637	1240.384298	17.458291
34.428061	1211.250221	17.463309
33.995069	1205.264895	17.468327
34.249199	1228.422525	17.473344
33.922150	1242.892775	17.478362
34.780300	1222.609137	17.483379
34.551840	1232.671810	17.488397
34.401302	1247.976669	17.493415
34.586919	1233.477024	17.498432
34.389628	1224.990630	17.503450
34.354962	1246.343990	17.508467
34.288360	1249.175531	17.513485
34.337846	1233.833035	17.518503
34.591226	1213.202308	17.523520
33.922990	1232.602669	17.528538
34.511604	1252.383901	17.533555
34.636030	1256.995948	17.538573
34.650789	1271.648367	17.543591
34.931488	1272.394159	17.548608
34.854138	1263.153450	17.553626
35.198805	1239.942754	17.558643
35.202112	1246.456552	17.563661
35.249775	1261.277695	17.568679
35.189716	1258.655898	17.573696
35.165097	1253.317075	17.578714
35.413575	1239.477844	17.583731
35.235239	1245.603155	17.588749
34.772780	1241.247103	17.593767
35.198799	1228.277444	17.598784
35.337579	1241.092547	17.603802
35.085511	1255.380282	17.608819
35.116135	1277.219826	17.613837
35.296689	1267.842718	17.618855
35.586458	1247.520228	17.623872
35.088547	1252.908873	17.628890
35.659738	1262.771920	17.633907
35.255920	1256.865887	17.638925
35.260362	1269.626853	17.643943
35.666160	1258.301759	17.648960
35.301372	1250.292824	17.653978
35.414600	1249.570678	17.658995
35.664390	1269.749084	17.664013
35.523067	1266.948536	17.669031
35.485873	1238.284724	17.674048
35.432646	1244.110784	17.679066
35.549164	1260.386834	17.684083
35.762218	1262.306621	17.689101
35.850689	1271.693275	17.694119
35.967836	1279.689792	17.699136
35.850222	1297.680558	17.704154
35.828713	1283.486487	17.709171
36.154381	1266.442704	17.714189
35.833345	1264.787437	17.719207
36.363292	1271.827559	17.724224
36.094086	1286.271170	17.729242
36.514470	1273.879631	17.734259
36.511943	1265.973188	17.739277
36.143166	1271.334399	17.744295
36.323804	1272.026959	17.749312
36.294127	1291.238328	17.754330
36.145336	1273.305746	17.759347
35.964418	1272.190185	17.764365
36.060653	1290.204645	17.769383
36.305054	1281.270317	17.774400
36.522534	1278.715620	17.779418
36.298861	1257.307076	17.784435
36.433051	1283.769170	17.789453
36.404252	1294.321896	17.794471
36.376318	1281.578059	17.799488
36.223598	1264.501448	17.804506
36.182695	1285.109218	17.809523
36.694087	1306.882839	17.814541
36.585656	1312.552240	17.819559
37.111372	1285.540583	17.824576
36.516157	1291.787151	17.829594
36.544261	1301.832564	17.834611
36.973716	1312.339492	17.839629
36.820286	1312.587079	17.844647
37.020590	1294.635948	17.849664
36.419755	1299.202148	17.854682
36.623125	1287.437857	17.859699
36.651970	1292.218331	17.864717
36.693572	1334.065850	17.869735
37.212319	1331.634451	17.874752
37.130120	1320.180945	17.879770
37.352378	1311.981487	17.884787
37.426378	1327.044052	17.889805
37.150662	1340.516475	17.894823
37.444760	1327.022005	17.899840
37.503367	1326.536290	17.904858
37.399907	1327.540404	17.909875
37.614946	1326.455645	17.914893
37.344576	1328.960425	17.919911
37.682057	1316.962876	17.924928
37.703593	1321.029477	17.929946
37.320889	1329.325696	17.934963
37.747673	1312.976306	17.939981
37.869857	1322.901389	17.944999
37.787679	1332.126363	17.950016
37.796178	1332.365987	17.955034
37.933403	1310.898714	17.960051
37.870982	1309.623738	17.965069
37.341098	1321.389241	17.970087
37.692442	1330.764768	17.975104
37.895009	1312.573632	17.980122
37.526803	1312.284502	17.985139
37.826765	1329.734166	17.990157
37.634333	1321.844021	17.995175
37.735480	1319.036852	18.000192
37.578444	1334.623908	18.005210
37.791235	1344.911012	18.010227
38.065131	1348.326019	18.015245
38.058088	1359.688099	18.020263
38.327478	1348.265724	18.025280
38.280887	1344.034774	18.030298
38.186708	1347.544849	18.035315
38.088956	1345.635895	18.040333
38.219883	1349.323782	18.045351
37.976588	1337.248903	18.050368
38.446561	1352.645574	18.055386
38.419771	1330.839318	18.060403
38.707517	1339.080546	18.065421
38.331084	1345.837607	18.070439
38.470075	1337.944544	18.075456
38.440979	1351.177647	18.080474
38.332628	1374.567602	18.085491
39.085294	1379.043397	18.090509
39.132379	1371.799907	18.095527
39.475581	1360.062343	18.100544
39.045223	1338.914658	18.105562
38.959464	1341.455748	18.110579
39.273598	1321.823855	18.115597
38.905519	1324.205049	18.120615
39.052124	1339.189502	18.125632
39.426962	1331.136237	18.130650
39.150805	1320.098650	18.135667
39.186765	1321.746499	18.140685
39.016275	1326.810752	18.145703
38.990453	1325.841860	18.150720
39.411611	1325.988888	18.155738
38.683519	1333.453020	18.160755
39.144609	1330.130864	18.165773
39.369884	1343.491867	18.170791
39.301527	1347.704894	18.175808
39.530203	1361.648779	18.180826
39.282647	1368.453633	18.185843
39.510512	1348.576966	18.190861
39.543018	1360.236871	18.195879
39.274643	1370.228294	18.200896
39.488504	1378.578777	18.205914
39.481994	1352.492065	18.210931
39.478789	1355.489978	18.215949
39.531152	1369.882989	18.220967
39.589581	1376.678907	18.225984
39.560908	1360.273757	18.231002
39.673925	1360.512740	18.236019
39.742780	1355.016341	18.241037
39.456058	1373.368135	18.246055
39.839378	1386.238991	18.251072
39.696918	1372.410809	18.256090
39.762047	1381.481087	18.261107
40.082986	1395.191991	18.266125
39.745150	1397.632259	18.271143
39.813945	1380.436746	18.276160
40.173976	1367.737166	18.281178
40.230440	1379.740488	18.286195
40.355451	1388.571695	18.291213
40.224720	1379.274593	18.296231
40.257479	1381.630887	18.301248
40.303827	1378.691063	18.306266
40.193201	1374.299859	18.311283
40.199196	1377.697248	18.316301
40.549391	1392.966542	18.321319
40.440183	1407.137820	18.326336
40.621197	1412.047678	18.331354
40.699726	1421.845916	18.336371
41.214512	1404.084958	18.341389
40.916262	1394.656117	18.346407
40.813576	1390.661143	18.351424
40.573124	1380.965043	18.356442
40.556829	1379.898138	18.361459
40.729304	1396.154361	18.366477
41.003968	1399.686451	18.371495
40.775769	1407.112095	18.376512
41.357574	1409.843406	18.381530
41.008057	1402.574908	18.386547
41.103669	1409.430921	18.391565
40.968829	1423.884340	18.396583
41.093031	1395.707030	18.401600
41.226398	1386.779771	18.406618
41.206102	1398.148990	18.411635
41.446807	1409.802474	18.416653
41.290832	1418.041790	18.421671
41.229584	1396.188392	18.426688
41.479812	1392.775505	18.431706
41.314825	1410.527733	18.436723
41.414605	1398.960749	18.441741
41.320675	1407.188921	18.446759
41.207669	1400.031504	18.451776
41.475129	1382.936200	18.456794
41.047864	1388.637258	18.461811
41.151841	1405.441695	18.466829
41.358302	1418.636029	18.471847
41.641911	1435.064831	18.476864
41.941196	1428.378913	18.481882
41.820501	1421.717625	18.486899
41.858571	1413.159267	18.491917
41.522409	1432.494082	18.496935
41.848119	1436.432022	18.501952
42.141651	1417.753887	18.506970
41.666757	1435.714701	18.511987
41.876172	1432.963915	18.517005
41.819468	1431.626975	18.522023
41.664473	1434.876806	18.527040
42.104131	1429.307200	18.532058
42.470045	1435.422159	18.537075
42.342670	1464.372221	18.542093
42.553810	1468.886655	18.547111
42.508783	1462.921350	18.552128
42.742763	1436.972961	18.557146
42.284197	1434.971292	18.562163
42.272073	1438.737649	18.567181
42.499729	1439.257131	18.572199
42.593489	1460.391875	18.577216
42.560508	1472.499106	18.582234
42.769851	1466.036256	18.587251
42.910443	1438.835664	18.592269
42.757648	1456.274681	18.597287
42.733978	1443.123303	18.602304
43.037119	1450.990969	18.607322
42.619143	1447.709449	18.612339
42.738818	1454.431910	18.617357
43.041500	1456.941697	18.622375
42.759018	1451.973886	18.627392
42.964909	1452.015575	18.632410
42.625712	1460.013500	18.637427
42.743280	1458.457939	18.642445
42.883846	1452.964120	18.647463
42.826028	1451.084373	18.652480
42.832514	1450.233433	18.657498
42.681081	1473.892806	18.662515
43.115448	1464.237173	18.667533
43.158227	1470.211394	18.672551
43.106477	1499.285412	18.677568
43.372847	1478.430282	18.682586
43.141349	1462.808372	18.687603
43.335592	1468.390716	18.692621
43.561750	1483.927394	18.697639
43.297544	1497.470084	18.702656
44.015701	1490.539960	18.707674
43.526553	1505.554157	18.712691
44.093978	1491.852896	18.717709
44.252389	1476.211019	18.722727
43.751127	1476.760817	18.727744
44.261471	1467.337749	18.732762
44.168829	1465.647572	18.737779
44.275541	1454.731126	18.742797
44.022641	1448.911668	18.747815
44.322315	1445.148648	18.752832
44.227492	1449.947344	18.757850
44.110556	1468.815267	18.762867
44.153959	1452.495723	18.767885
44.418951	1445.201428	18.772903
44.274918	1460.514871	18.777920
44.252967	1464.513319	18.782938
44.235439	1460.854374	18.787955
44.081074	1455.180602	18.792973
44.315827	1451.960375	18.797991
44.038853	1457.762874	18.803008
44.219256	1461.055986	18.808026
44.423218	1483.778101	18.813043
44.172953	1493.402027	18.818061
44.482856	1495.808386	18.823079
44.656590	1485.627430	18.828096
44.361280	1463.448619	18.833114
44.475821	1483.687740	18.838131
44.648407	1498.187748	18.843149
45.002347	1495.051042	18.848167
44.916810	1504.260340	18.853184
45.187306	1496.595212	18.858202
45.156339	1515.209373	18.863219
45.033284	1502.880687	18.868237
45.225978	1495.199289	18.873255
44.875233	1485.318834	18.878272
44.987640	1498.593824	18.883290
45.312345	1525.414925	18.888307
45.020964	1512.576762	18.893325
45.324642	1498.606155	18.898343
45.160028	1519.292742	18.903360
45.358410	1521.157125	18.908378
45.198291	1507.311960	18.913395
45.405799	1497.578465	18.918413
45.827086	1506.156987	18.923431
45.719209	1512.891195	18.928448
45.733386	1515.362564	18.933466
45.662054	1509.103129	18.938483
45.602289	1496.471927	18.943501
46.008495	1499.223908	18.948519
45.656339	1510.596388	18.953536
45.728949	1513.114092	18.958554
45.793457	1508.153968	18.963571
45.785451	1508.866691	18.968589
45.763843	1507.566553	18.973607
45.511123	1505.613222	18.978624
45.678138	1513.579579	18.983642
46.243108	1521.133208	18.988659
45.830254	1519.639609	18.993677
46.198902	1528.316488	18.998695
46.142682	1545.044424	19.003712
46.185394	1511.291522	19.008730
46.051871	1524.380452	19.013747
46.170954	1534.234842	19.018765
46.596448	1533.573951	19.023783
46.175213	1539.360170	19.028800
46.362471	1532.907240	19.033818
46.440868	1522.198235	19.038835
46.396792	1517.340088	19.043853
46.713971	1535.493091	19.048871
46.653523	1557.034078	19.053888
46.627451	1555.486499	19.058906
47.080666	1539.273711	19.063923
47.017325	1544.167705	19.068941
47.103496	1570.112950	19.073959
47.077555	1543.193771	19.078976
46.763882	1528.119312	19.083994
46.980648	1536.863411	19.089011
47.131352	1559.350004	19.094029
47.072215	1563.927630	19.099047
46.842761	1551.574172	19.104064
46.955666	1537.013241	19.109082
46.950330	1552.161662	19.114099
46.930417	1542.875867	19.119117
46.996688	1548.626796	19.124135
47.177882	1565.702939	19.129152
47.060572	1567.609064	19.134170
47.765045	1563.909705	19.139187
47.421610	1594.565041	19.144205
47.353964	1591.323905	19.149223
47.477632	1588.178589	19.154240
47.634514	1593.657727	19.159258
47.556547	1585.022996	19.164275
47.595932	1574.474108	19.169293
47.736215	1576.743978	19.174311
47.861576	1571.989184	19.179328
47.629887	1568.117822	19.184346
47.867382	1577.001696	19.189363
47.848073	1572.854836	19.194381
47.927140	1569.733917	19.199399
48.048902	1585.727127	19.204416
48.130680	1597.935645	19.209434
48.174368	1617.829640	19.214451
48.335633	1614.119563	19.219469
48.758257	1590.413963	19.224487
48.426634	1592.972696	19.229504
48.303331	1603.318958	19.234522
48.408370	1620.753145	19.239539
48.406233	1610.980615	19.244557
48.689255	1594.858773	19.249575
48.509972	1601.122443	19.254592
48.429252	1610.360628	19.259610
48.883603	1602.949946	19.264627
49.090410	1587.275653	19.269645
48.894304	1583.976334	19.274663
48.901836	1601.933394	19.279680
48.727209	1602.098778	19.284698
48.747593	1595.166123	19.289715
48.754431	1605.889811	19.294733
48.746757	1608.330659	19.299751
48.652680	1610.721331	19.304768
48.513973	1597.248942	19.309786
48.522758	1584.947703	19.314803
48.581108	1613.854171	19.319821
48.922527	1618.866697	19.324839
48.829450	1643.004477	19.329856
49.094144	1628.205232	19.334874
49.049028	1618.867071	19.339891
48.971109	1634.057679	19.344909
49.293576	1634.011125	19.349927
49.561912	1647.471259	19.354944
49.787891	1649.273433	19.359962
49.955234	1654.199996	19.364979
49.941547	1648.226094	19.369997
49.952229	1633.370218	19.375015
49.624525	1622.658186	19.380032
49.677952	1643.729195	19.385050
49.879882	1651.059672	19.390067
49.901757	1651.746504	19.395085
50.445144	1634.666925	19.400103
50.527419	1640.707211	19.405120
50.154378	1641.330686	19.410138
50.188771	1621.457001	19.415155
49.936272	1612.466236	19.420173
50.111888	1615.055892	19.425191
49.999557	1629.808478	19.430208
50.221359	1625.193111	19.435226
50.370611	1649.246477	19.440243
50.062413	1654.546836	19.445261
50.539919	1643.285971	19.450279
50.610922	1639.321273	19.455296
50.457097	1638.553987	19.460314
50.603812	1643.510722	19.465331
50.513705	1651.355107	19.470349
50.572465	1636.625409	19.475367
50.347797	1630.394903	19.480384
50.413596	1635.269554	19.485402
50.617760	1669.806843	19.490419
50.902128	1675.550120	19.495437
51.156098	1651.831851	19.500455
51.240916	1670.909644	19.505472
50.898361	1689.704809	19.510490
50.937954	1690.632365	19.515507
51.177847	1673.584592	19.520525
51.097365	1665.890684	19.525543
50.816826	1672.296974	19.530560
51.089562	1668.579682	19.535578
51.270375	1663.935061	19.540595
51.181859	1668.731405	19.545613
51.412241	1666.096282	19.550631
51.458896	1668.749769	19.555648
51.564943	1679.560833	19.560666
51.817863	1692.804507	19.565683
51.802954	1703.021037	19.570701
51.616578	1701.545396	19.575719
52.167628	1686.884170	19.580736
51.944813	1675.930996	19.585754
52.183652	1656.340836	19.590771
51.872665	1659.486696	19.595789
51.609325	1665.007157	19.600807
52.238653	1654.105565	19.605824
51.967770	1669.778492	19.610842
52.090967	1691.568692	19.615859
52.240598	1694.976661	19.620877
52.337075	1681.731618	19.625895
52.715688	1682.022957	19.630912
52.032001	1668.643808	19.635930
52.021177	1663.747253	19.640947
51.898085	1678.232625	19.645965
51.945839	1689.099874	19.650983
52.021026	1687.082198	19.656000
52.044866	1698.492860	19.661018
52.542365	1708.889922	19.666035
52.460835	1714.890882	19.671053
52.360333	1720.322361	19.676071
52.293734	1727.282176	19.681088
52.489571	1715.806243	19.686106
53.024476	1704.900045	19.691123
52.651173	1725.667646	19.696141
52.689088	1712.885998	19.701159
52.949850	1715.525369	19.706176
52.953395	1739.525017	19.711194
53.131607	1740.415893	19.716211
52.892681	1737.620267	19.721229
53.115780	1732.002300	19.726247
53.132717	1738.896162	19.731264
53.360804	1738.466368	19.736282
53.520242	1736.576467	19.741299
53.331712	1724.339605	19.746317
53.312980	1721.547154	19.751335
53.449776	1732.931895	19.756352
53.069955	1749.871370	19.761370
53.480100	1748.277274	19.766387
53.438359	1752.623387	19.771405
53.664376	1772.856277	19.776423
53.982316	1762.474278	19.781440
53.624145	1756.487784	19.786458
53.762822	1749.727008	19.791475
54.065424	1751.432199	19.796493
54.251793	1766.095997	19.801511
54.557849	1755.559010	19.806528
54.007128	1758.344881	19.811546
54.689559	1748.574767	19.816563
54.457805	1744.150038	19.821581
54.521326	1749.930724	19.826599
54.906097	1753.964872	19.831616
54.755701	1743.217551	19.836634
54.605657	1742.452292	19.841651
54.521615	1757.675425	19.846669
54.587998	1732.670383	19.851687
54.686850	1736.222846	19.856704
54.663153	1759.116723	19.861722
54.869166	1741.151137	19.866739
54.748365	1764.270867	19.871757
55.118559	1751.196237	19.876775
54.910625	1728.525928	19.881792
54.779788	1749.644359	19.886810
54.975906	1737.428258	19.891827
54.840198	1749.995310	19.896845
54.873064	1754.104830	19.901863
54.941949	1738.055912	19.906880
54.941687	1753.483853	19.911898
54.820768	1768.178750	19.916915
54.931976	1778.820759	19.921933
54.866561	1776.656458	19.926951
54.933525	1769.252931	19.931968
55.006746	1779.457016	19.936986
55.494026	1794.834546	19.942003
55.578262	1792.808473	19.947021
55.683734	1800.034612	19.952039
55.611659	1813.376180	19.957056
55.365636	1824.515549	19.962074
55.542997	1806.943914	19.967091
55.409440	1805.415547	19.972109
55.570795	1816.237644	19.977127
56.071569	1798.425112	19.982144
56.155239	1793.116524	19.987162
56.076848	1819.534079	19.992179
56.149092	1799.670046	19.997197
55.884424	1787.752937	20.002215
56.376824	1806.211296	20.007232
56.050597	1820.647414	20.012250
56.188947	1818.527175	20.017267
56.136869	1818.141314	20.022285
56.526851	1829.900938	20.027303
56.918386	1816.682006	20.032320
56.757415	1843.942710	20.037338
56.952289	1815.132895	20.042355
56.891214	1810.215764	20.047373
56.841534	1828.502164	20.052391
57.271968	1834.418768	20.057408
56.923431	1820.197546	20.062426
56.830008	1794.504484	20.067443
56.979901	1790.828718	20.072461
56.881700	1817.625452	20.077479
56.963275	1804.337400	20.082496
57.179452	1828.335214	20.087514
57.168571	1821.294162	20.092531
57.079951	1812.223355	20.097549
56.683050	1810.416619	20.102567
57.299406	1817.605087	20.107584
56.887807	1830.101183	20.112602
57.372750	1828.634061	20.117619
57.445994	1841.671873	20.122637
57.465063	1857.763817	20.127655
57.705981	1843.319997	20.132672
57.791758	1854.895900	20.137690
57.701479	1866.500708	20.142707
57.932553	1844.029283	20.147725
57.503814	1844.890566	20.152743
58.060275	1851.375900	20.157760
57.708031	1851.373234	20.162778
57.710570	1837.382410	20.167795
57.871816	1854.109092	20.172813
57.815575	1878.831395	20.177831
58.357381	1870.558662	20.182848
58.189353	1870.269897	20.187866
58.146879	1865.209741	20.192883
58.259533	1872.390739	20.197901
58.176288	1872.383280	20.202919
58.592887	1856.885519	20.207936
58.343152	1858.027693	20.212954
58.551797	1867.307667	20.217971
58.773924	1864.448722	20.222989
58.595989	1860.685800	20.228007
58.832302	1888.275442	20.233024
58.893953	1894.659819	20.238042
58.791796	1901.636807	20.243059
59.368925	1906.769601	20.248077
59.147966	1900.638550	20.253095
59.511256	1880.513269	20.258112
58.889407	1888.115688	20.263130
59.203927	1899.501691	20.268147
59.354749	1893.784803	20.273165
59.518653	1879.400812	20.278183
59.674141	1885.096779	20.283200
59.387606	1905.984708	20.288218
59.313728	1905.804671	20.293235
59.506568	1892.190834	20.298253
59.103527	1883.108568	20.303271
59.507066	1892.181583	20.308288
59.290484	1904.911112	20.313306
59.355122	1885.102447	20.318323
59.167591	1899.383954	20.323341
59.509816	1916.911838	20.328359
59.429418	1917.688107	20.333376
59.586411	1917.598733	20.338394
59.620022	1940.338261	20.343411
59.868707	1930.382868	20.348429
59.952019	1941.551448	20.353447
60.020072	1936.964052	20.358464
60.250895	1947.698891	20.363482
60.301159	1962.097332	20.368499
60.503867	1938.950369	20.373517
60.438034	1938.371047	20.378535
60.708852	1946.188120	20.383552
60.483285	1943.847936	20.388570
60.361068	1935.010517	20.393587
60.855944	1935.078655	20.398605
60.665565	1952.718405	20.403623
60.738977	1954.350391	20.408640
60.837198	1958.545408	20.413658
61.076814	1962.014340	20.418675
61.687452	1957.815337	20.423693
61.231147	1964.418870	20.428711
61.057365	1962.964248	20.433728
61.305403	1955.585621	20.438746
61.084020	1948.499192	20.443763
61.226431	1970.187715	20.448781
60.901939	1968.277477	20.453799
61.186266	1965.823805	20.458816
61.068008	1973.612290	20.463834
61.355725	1970.166906	20.468851
61.814524	1953.200836	20.473869
62.016239	1964.066949	20.478887
61.858698	1975.925821	20.483904
61.804808	1971.908461	20.488922
61.913982	1963.014388	20.493939
62.052356	1953.217043	20.498957
61.880702	1973.394184	20.503975
62.462693	1999.219353	20.508992
62.504932	1990.724933	20.514010
62.273773	1968.810621	20.519027
62.501332	1950.397712	20.524045
62.236371	1960.898208	20.529063
62.539736	1957.328119	20.534080
62.614470	1973.847813	20.539098
62.696907	1963.082331	20.544115
62.742092	1940.562462	20.549133
62.193081	1965.893299	20.554151
62.426331	1976.142022	20.559168
62.667953	1972.114308	20.564186
62.931266	1971.230937	20.569203
63.008395	1987.309487	20.574221
62.953767	1987.915883	20.579239
63.045872	1982.577100	20.584256
63.025336	1984.747153	20.589274
62.877821	1964.206462	20.594291
62.975471	1960.983003	20.599309
62.985774	1979.842829	20.604327
62.981842	1991.909751	20.609344
63.040028	1988.251552	20.614362
62.988670	1996.013150	20.619379
63.118209	2011.712170	20.624397
63.174600	1999.301373	20.629415
63.459093	2002.976835	20.634432
63.720743	2003.658898	20.639450
63.482891	2011.641147	20.644467
63.808685	2016.475319	20.649485
63.835919	2029.121657	20.654503
63.791807	2024.947479	20.659520
64.021055	2024.373320	20.664538
63.770547	2029.860792	20.669555
64.158492	2012.866805	20.674573
64.028676	2036.570512	20.679591
64.508672	2049.322528	20.684608
64.487923	2025.365174	20.689626
64.656842	2022.827827	20.694643
64.418205	2023.075825	20.699661
64.396919	2029.886190	20.704679
64.387634	2024.569264	20.709696
64.451749	2025.313885	20.714714
64.174294	2027.332931	20.719731
64.486362	2029.064045	20.724749
64.539388	2038.004749	20.729767
64.447095	2038.954415	20.734784
65.048357	2050.254473	20.739802
64.623870	2061.854626	20.744819
64.874963	2046.029955	20.749837
64.933225	2067.433561	20.754855
64.945376	2078.075417	20.759872
65.165245	2063.353129	20.764890
65.231030	2072.084007	20.769907
65.355159	2083.874473	20.774925
65.471465	2106.880059	20.779943
65.351320	2104.458268	20.784960
65.553734	2088.139031	20.789978
65.568441	2085.668094	20.794995
65.447165	2107.265763	20.800013
65.306177	2112.842234	20.805031
65.687075	2081.354709	20.810048
66.044263	2081.967946	20.815066
66.093482	2104.006643	20.820083
66.142203	2096.526658	20.825101
66.267645	2118.120377	20.830119
66.421195	2104.455966	20.835136
66.362833	2095.739277	20.840154
66.222964	2103.124385	20.845171
66.526108	2097.668618	20.850189
66.353224	2112.691075	20.855207
66.163407	2111.942406	20.860224
66.344900	2097.687071	20.865242
66.203953	2100.012053	20.870259
66.765987	2091.725725	20.875277
66.835455	2098.063431	20.880295
67.011485	2093.998796	20.885312
66.863612	2102.993203	20.890330
66.594970	2094.202620	20.895347
66.694712	2110.439443	20.900365
67.033259	2124.321783	20.905383
67.073409	2132.058389	20.910400
66.994501	2121.011836	20.915418
67.169106	2129.940277	20.920435
67.254473	2129.078627	20.925453
67.359739	2137.266204	20.930471
67.363279	2117.615931	20.935488
67.421693	2120.306917	20.940506
67.168173	2141.504416	20.945523
67.552107	2141.751982	20.950541
67.528698	2145.086695	20.955559
67.346980	2174.768307	20.960576
67.755423	2163.694135	20.965594
67.718228	2148.720398	20.970611
67.924809	2140.751691	20.975629
67.667105	2172.110912	20.980647
68.017903	2196.753771	20.985664
68.286767	2176.000710	20.990682
68.407563	2170.218615	20.995699
68.381816	2170.721543	21.000717
68.455939	2189.446988	21.005735
68.506133	2179.098422	21.010752
68.874649	2153.634278	21.015770
68.356351	2166.499592	21.020787
68.554059	2195.559098	21.025805
68.654772	2200.447054	21.030823
68.453029	2182.708048	21.035840
68.851673	2161.628595	21.040858
68.738074	2185.614249	21.045875
69.146017	2192.831825	21.050893
69.183312	2179.400399	21.055911
69.461843	2185.112556	21.060928
69.384127	2189.147963	21.065946
69.027270	2193.229300	21.070963
69.410552	2198.295129	21.075981
69.491648	2200.082833	21.080999
69.364598	2203.337261	21.086016
69.733271	2202.814945	21.091034
69.335337	2215.911746	21.096051
69.351214	2198.602133	21.101069
69.436668	2209.721252	21.106087
69.657774	2205.243009	21.111104
69.697033	2198.397597	21.116122
69.804159	2222.251478	21.121139
69.784408	2222.911657	21.126157
69.762326	2222.643051	21.131175
70.106923	2228.962017	21.136192
70.185877	2234.314326	21.141210
70.323056	2237.810976	21.146227
70.107143	2204.889600	21.151245
70.391051	2225.403040	21.156263
70.491863	2259.462070	21.161280
70.591115	2254.137758	21.166298
70.502211	2267.793275	21.171315
70.536909	2261.803167	21.176333
70.964099	2247.831645	21.181351
70.806995	2270.488630	21.186368
71.080385	2240.334955	21.191386
70.887196	2252.016399	21.196403
70.898341	2266.096448	21.201421
71.042348	2247.457563	21.206439
71.027466	2260.181314	21.211456
71.326748	2277.798978	21.216474
71.683205	2289.418065	21.221491
71.708434	2287.895295	21.226509
71.732997	2273.359876	21.231527
71.443636	2281.290058	21.236544
71.561007	2268.589389	21.241562
71.561430	2276.608275	21.246579
71.356919	2286.959066	21.251597
71.734081	2274.217825	21.256615
71.596152	2277.382448	21.261632
72.021904	2293.956571	21.266650
72.114727	2309.210562	21.271667
71.972639	2311.663400	21.276685
72.264183	2306.590712	21.281703
71.967479	2292.182956	21.286720
72.523525	2297.777952	21.291738
72.144258	2303.617057	21.296755
71.929331	2296.923034	21.301773
72.153920	2318.404999	21.306791
72.314193	2338.859014	21.311808
72.931492	2339.289836	21.316826
73.007642	2325.627981	21.321843
72.814035	2341.126152	21.326861
72.797874	2331.885511	21.331879
72.765665	2326.243976	21.336896
72.896845	2313.020406	21.341914
72.916888	2335.289612	21.346931
72.669885	2343.733016	21.351949
73.437308	2339.470511	21.356967
73.440856	2348.808582	21.361984
73.628142	2355.426384	21.367002
73.616643	2362.067197	21.372019
73.625750	2369.038214	21.377037
73.707347	2353.178353	21.382055
73.758069	2357.329368	21.387072
73.974092	2356.098633	21.392090
73.578186	2356.229241	21.397107
73.685136	2366.651040	21.402125
73.997880	2353.044341	21.407143
73.602869	2355.004618	21.412160
73.954276	2371.733213	21.417178
73.926992	2375.520216	21.422195
74.217930	2399.735175	21.427213
74.535624	2395.519809	21.432231
74.274027	2388.784253	21.437248
74.393202	2387.695286	21.442266
74.566866	2399.974875	21.447283
74.379370	2405.573504	21.452301
74.540217	2385.644672	21.457319
74.352684	2402.772739	21.462336
74.721382	2421.030960	21.467354
75.282010	2429.897756	21.472371
75.034566	2431.354995	21.477389
75.211501	2411.590176	21.482407
75.455029	2415.537524	21.487424
75.205792	2406.006862	21.492442
75.527021	2405.361595	21.497459
75.180744	2426.856166	21.502477
75.460562	2403.226350	21.507495
75.271036	2409.350429	21.512512
75.365972	2430.328272	21.517530
75.665170	2436.295434	21.522547
76.091076	2444.047673	21.527565
75.930035	2454.178632	21.532583
75.599439	2441.395766	21.537600
75.844195	2449.220062	21.542618
76.238172	2444.161893	21.547635
76.156655	2435.785791	21.552653
76.371984	2427.006171	21.557671
76.228264	2441.488880	21.562688
76.186844	2466.056061	21.567706
76.303041	2459.282648	21.572723
76.196070	2464.296429	21.577741
76.399564	2475.999783	21.582759
76.743662	2478.633488	21.587776
76.661507	2469.948466	21.592794
76.768780	2461.717700	21.597811
76.789044	2460.708449	21.602829
76.849982	2488.900502	21.607847
77.134067	2478.251119	21.612864
77.037265	2477.415320	21.617882
77.637923	2492.251574	21.622899
77.692495	2509.054561	21.627917
77.398143	2499.672416	21.632935
77.644837	2492.453672	21.637952
77.862929	2479.492719	21.642970
77.971827	2492.065520	21.647987
77.087669	2491.934539	21.653005
77.337726	2487.269373	21.658023
77.683236	2489.998698	21.663040
77.555572	2486.844541	21.668058
77.922853	2483.995546	21.673075
77.626207	2503.267211	21.678093
77.854270	2495.594331	21.683111
77.941872	2529.279232	21.688128
78.167214	2519.675393	21.693146
78.162727	2497.525852	21.698163
78.192833	2507.418600	21.703181
78.338543	2534.331373	21.708199
78.344697	2553.107069	21.713216
78.477063	2537.135299	21.718234
78.530712	2531.436398	21.723251
78.833706	2533.570486	21.728269
78.940911	2547.755375	21.733287
79.169655	2547.657980	21.738304
78.702101	2530.757945	21.743322
79.441297	2556.876929	21.748339
78.842544	2545.627432	21.753357
79.420739	2563.275308	21.758375
79.321980	2571.458549	21.763392
79.193416	2568.072079	21.768410
79.510122	2570.787087	21.773427
79.306491	2579.472628	21.778445
79.687426	2554.347943	21.783463
79.561246	2581.451570	21.788480
79.651743	2591.311561	21.793498
79.844329	2588.953550	21.798515
79.784490	2590.116456	21.803533
79.761268	2598.584036	21.808551
79.892131	2600.825306	21.813568
79.825470	2589.697073	21.818586
80.263274	2595.693748	21.823603
80.374735	2619.365371	21.828621
80.903808	2611.054789	21.833639
80.674140	2615.206544	21.838656
80.480107	2633.887091	21.843674
80.773822	2625.865159	21.848691
80.777963	2630.481949	21.853709
81.083484	2605.847328	21.858727
80.924582	2613.368582	21.863744
80.930333	2627.973595	21.868762
81.446608	2617.066687	21.873779
80.763034	2609.389887	21.878797
81.144698	2624.597840	21.883815
81.301147	2647.355513	21.888832
81.405147	2649.824031	21.893850
81.331095	2626.627686	21.898867
81.453295	2656.977126	21.903885
81.521207	2663.451819	21.908903
81.841596	2656.129889	21.913920
81.739208	2667.899090	21.918938
82.168068	2651.759326	21.923955
81.940721	2679.480740	21.928973
82.245869	2680.275118	21.933991
82.441252	2660.296529	21.939008
82.362155	2663.866017	21.944026
82.575432	2669.680957	21.949043
82.607617	2668.457547	21.954061
82.509135	2655.822931	21.959079
82.772098	2661.572580	21.964096
82.583743	2670.691215	21.969114
82.859889	2652.324057	21.974131
82.552918	2659.498594	21.979149
82.559406	2646.534087	21.984167
82.832197	2677.552284	21.989184
82.992418	2681.847869	21.994202
83.191093	2675.687217	21.999219
83.550190	2698.005632	22.004237
83.611771	2686.664039	22.009255
83.203879	2682.611597	22.014272
83.269539	2696.003798	22.019290
83.450965	2680.920495	22.024307
83.307878	2705.590081	22.029325
83.370174	2682.965919	22.034343
83.855733	2695.661266	22.039360
83.608825	2712.540863	22.044378
83.983745	2705.788755	22.049395
83.806331	2732.111067	22.054413
83.913493	2724.373418	22.059431
84.131113	2713.094789	22.064448
83.967379	2726.021056	22.069466
84.444566	2738.335592	22.074483
84.180187	2753.320945	22.079501
84.380034	2736.462741	22.084519
84.816896	2728.287002	22.089536
84.281952	2745.583077	22.094554
84.631609	2748.424347	22.099571
84.895280	2741.315855	22.104589
85.087290	2744.938384	22.109607
85.219906	2758.234942	22.114624
85.266445	2774.147740	22.119642
85.442894	2765.333216	22.124659
85.411275	2765.486886	22.129677
85.277318	2785.882256	22.134695
85.578736	2765.564793	22.139712
85.437085	2764.789729	22.144730
85.602070	2773.982303	22.149747
85.558131	2777.823331	22.154765
85.628158	2769.622372	22.159783
85.688728	2772.881050	22.164800
85.911115	2801.553031	22.169818
85.875499	2794.376466	22.174835
86.013224	2792.921660	22.179853
86.244097	2782.283419	22.184871
86.362046	2784.977970	22.189888
86.124726	2802.942548	22.194906
86.266657	2826.987948	22.199923
86.487566	2831.446160	22.204941
86.743262	2807.420946	22.209959
86.805333	2820.198774	22.214976
86.619239	2837.359364	22.219994
86.764717	2831.489688	22.225011
86.885734	2830.172463	22.230029
86.925790	2830.092470	22.235047
87.407243	2855.080496	22.240064
87.300303	2869.278629	22.245082
87.508713	2852.519855	22.250099
87.539148	2847.893430	22.255117
87.815529	2866.152871	22.260135
87.941182	2861.001523	22.265152
87.691106	2855.899468	22.270170
87.886683	2833.406388	22.275187
87.827287	2848.554785	22.280205
87.639692	2841.533412	22.285223
88.064260	2845.942624	22.290240
88.055754	2865.895772	22.295258
88.337710	2873.798969	22.300275
88.553790	2863.905343	22.305293
88.581680	2858.673313	22.310311
88.654945	2872.339965	22.315328
88.262048	2881.245311	22.320346
88.361160	2864.035748	22.325363
88.575826	2877.958728	22.330381
88.816960	2878.232859	22.335399
88.880306	2879.517539	22.340416
88.684587	2895.958620	22.345434
88.717980	2905.655633	22.350451
88.775127	2918.245994	22.355469
88.943741	2903.141956	22.360487
89.141739	2906.303947	22.365504
89.260853	2920.940697	22.370522
89.727334	2913.804912	22.375539
89.356946	2931.947120	22.380557
89.555909	2930.460728	22.385575
89.791825	2918.882507	22.390592
89.588837	2925.617007	22.395610
90.276712	2940.008827	22.400627
90.194530	2931.035002	22.405645
90.050207	2932.708288	22.410663
90.214564	2950.828684	22.415680
90.149745	2952.838594	22.420698
90.343863	2940.527789	22.425715
90.368232	2954.972969	22.430733
90.360721	2954.296777	22.435751
90.745312	2956.498338	22.440768
90.430234	2976.253303	22.445786
90.903427	2962.457764	22.450803
90.965403	2954.026767	22.455821
91.235178	2970.512450	22.460839
91.566083	2981.071063	22.465856
91.168919	2967.744888	22.470874
91.347197	2963.181193	22.475891
91.540648	2964.632154	22.480909
90.999533	2968.296557	22.485927
91.713565	2989.917652	22.490944
91.914571	2986.615590	22.495962
92.025214	2994.966791	22.500979
92.358895	2995.266768	22.505997
92.041060	3014.094989	22.511015
92.317169	2996.443089	22.516032
92.095490	2994.522914	22.521050
92.139603	2987.021311	22.526067
92.554580	3006.618677	22.531085
92.318874	3010.650290	22.536103
92.458833	2976.815017	22.541120
92.235733	2988.839025	22.546138
92.337971	3008.968720	22.551155
92.235129	3019.185893	22.556173
92.356797	3029.319130	22.561191
92.691776	3039.127397	22.566208
92.834388	3050.357055	22.571226
92.851140	3053.076838	22.576243
92.868210	3048.621636	22.581261
92.936646	3048.891831	22.586279
93.554835	3064.026692	22.591296
93.406093	3093.107744	22.596314
93.569284	3081.126900	22.601331
93.649157	3092.117182	22.606349
93.483710	3096.787131	22.611367
93.776085	3074.254873	22.616384
93.897173	3105.668643	22.621402
93.872923	3118.879241	22.626419
94.595575	3105.466322	22.631437
94.529252	3130.788197	22.636455
94.892294	3110.833481	22.641472
94.777447	3090.470215	22.646490
94.805830	3109.990665	22.651507
94.892753	3108.706804	22.656525
94.813607	3109.471017	22.661543
94.973312	3102.137244	22.666560
94.761775	3107.154537	22.671578
94.904588	3116.170687	22.676595
95.251628	3113.449909	22.681613
95.349072	3118.215976	22.686631
95.193507	3088.149928	22.691648
95.339750	3116.193027	22.696666
95.529878	3123.641305	22.701683
95.724181	3127.314721	22.706701
95.486750	3125.347728	22.711719
95.743102	3111.823098	22.716736
95.663783	3127.512794	22.721754
95.301672	3138.511976	22.726771
95.759168	3138.003005	22.731789
95.301261	3162.510997	22.736807
95.915495	3157.834464	22.741824
96.048327	3183.567365	22.746842
96.016482	3177.367646	22.751859
96.511534	3168.724434	22.756877
96.436709	3183.660183	22.761895
96.418769	3196.872167	22.766912
96.717990	3196.168309	22.771930
96.706261	3211.443423	22.776947
97.171025	3222.557580	22.781965
97.087263	3228.083859	22.786983
97.187655	3220.099273	22.792000
97.321372	3230.787875	22.797018
97.536309	3238.580694	22.802035
97.428719	3213.912196	22.807053
97.265187	3215.994547	22.812071
97.723458	3222.286875	22.817088
97.852280	3243.261605	22.822106
97.912994	3251.727877	22.827123
98.460166	3226.278403	22.832141
98.074837	3231.649615	22.837159
97.863614	3246.385939	22.842176
98.173359	3239.302083	22.847194
98.330626	3239.172015	22.852211
98.888067	3241.833784	22.857229
98.404994	3260.154231	22.862247
98.762208	3261.153008	22.867264
98.780701	3260.600248	22.872282
98.697856	3276.210568	22.877299
98.964172	3257.476048	22.882317
99.072561	3253.313342	22.887335
99.272550	3266.227788	22.892352
99.588521	3268.202177	22.897370
99.432274	3254.460984	22.902387
99.303672	3261.945659	22.907405
99.305630	3295.051567	22.912423
99.660273	3286.243716	22.917440
99.795641	3298.896062	22.922458
99.543161	3301.235223	22.927475
100.087293	3284.223874	22.932493
99.929411	3305.473008	22.937511
100.087882	3316.589030	22.942528
100.053291	3316.460942	22.947546
100.087721	3313.115477	22.952563
100.366456	3317.005279	22.957581
100.152294	3321.847108	22.962599
100.184318	3343.184586	22.967616
100.522131	3355.736014	22.972634
100.686865	3342.383589	22.977651
100.999432	3328.482391	22.982669
100.530432	3357.663313	22.987687
101.249381	3383.055824	22.992704
101.244853	3378.813524	22.997722
101.116353	3363.191848	23.002739
101.176634	3368.491050	23.007757
101.335438	3390.580009	23.012775
101.571331	3411.254822	23.017792
101.804530	3395.530044	23.022810
101.820608	3385.886238	23.027827
102.114331	3399.583262	23.032845
102.578416	3397.406033	23.037863
102.466255	3391.132697	23.042880
102.606847	3387.904305	23.047898
102.384918	3392.716341	23.052915
102.518240	3394.128662	23.057933
102.532965	3395.459605	23.062951
102.496711	3404.544287	23.067968
102.723855	3391.940293	23.072986
102.650226	3396.771718	23.078003
102.695599	3405.853542	23.083021
102.831109	3432.638874	23.088039
102.652748	3445.068797	23.093056
103.115893	3439.856175	23.098074
103.139077	3427.413401	23.103091
103.443281	3440.215506	23.108109
103.454453	3462.229957	23.113127
103.355116	3473.180641	23.118144
103.868317	3447.910811	23.123162
103.570815	3456.617472	23.128179
103.881865	3466.378593	23.133197
104.199853	3496.229661	23.138215
104.023696	3484.279974	23.143232
104.350052	3474.996223	23.148250
104.058840	3480.546242	23.153267
104.448824	3496.300485	23.158285
104.613318	3507.542804	23.163303
104.429660	3496.438760	23.168320
105.148758	3507.604397	23.173338
104.869996	3521.702004	23.178355
104.980415	3512.237001	23.183373
105.019655	3510.531103	23.188391
105.059864	3502.894278	23.193408
105.270836	3521.809933	23.198426
105.323435	3545.763744	23.203443
105.439572	3546.761238	23.208461
105.220155	3548.397986	23.213479
105.461690	3536.307987	23.218496
105.892023	3555.002215	23.223514
105.776791	3569.635788	23.228531
106.239641	3566.794624	23.233549
106.064561	3579.348708	23.238567
105.971110	3572.453951	23.243584
106.406683	3583.849155	23.248602
106.413043	3598.174498	23.253619
106.722125	3590.207005	23.258637
106.670622	3583.186425	23.263655
106.539505	3590.649826	23.268672
106.956381	3586.705128	23.273690
106.797599	3598.788857	23.278707
107.131447	3610.993146	23.283725
107.218439	3625.233347	23.288743
107.318147	3610.960409	23.293760
107.478936	3603.914779	23.298778
107.296306	3625.354449	23.303795
107.622250	3616.705078	23.308813
107.621303	3635.087628	23.313831
107.604698	3643.725737	23.318848
107.959677	3643.360257	23.323866
107.948935	3653.951181	23.328883
108.352554	3639.498483	23.333901
108.518941	3631.622062	23.338919
108.281678	3637.978116	23.343936
108.363175	3653.531152	23.348954
108.297061	3672.794131	23.353971
108.938657	3671.358733	23.358989
108.668221	3678.887910	23.364007
108.854817	3684.380702	23.369024
109.014412	3672.132299	23.374042
108.933469	3692.184895	23.379059
109.262125	3702.062539	23.384077
109.774564	3701.880275	23.389095
109.496390	3696.906589	23.394112
109.895056	3676.255745	23.399130
109.380903	3695.080620	23.404147
109.592896	3711.502634	23.409165
110.070614	3697.626766	23.414183
110.077706	3711.798562	23.419200
110.429269	3714.385191	23.424218
110.548364	3715.370398	23.429235
110.507423	3717.846307	23.434253
110.632583	3726.854315	23.439271
110.811967	3721.920360	23.444288
110.738277	3726.202924	23.449306
110.539992	3742.668947	23.454323
110.914418	3716.354762	23.459341
110.766764	3713.484539	23.464359
110.921783	3737.816970	23.469376
110.944201	3738.331771	23.474394
111.256463	3743.728234	23.479411
111.185528	3757.860214	23.484429
111.484431	3749.709689	23.489447
111.185143	3757.276937	23.494464
111.666022	3769.538153	23.499482
111.888884	3779.377623	23.504499
111.802256	3773.298323	23.509517
112.034216	3782.423155	23.514535
112.129668	3808.074304	23.519552
112.486503	3797.579700	23.524570
111.986909	3791.146022	23.529587
112.398027	3801.367165	23.534605
112.351652	3808.887923	23.539623
112.606504	3824.769155	23.544640
112.927791	3833.710765	23.549658
112.745374	3843.982179	23.554675
113.153986	3816.561265	23.559693
113.478454	3841.404799	23.564711
113.348274	3873.578136	23.569728
113.463118	3859.647918	23.574746
113.725867	3854.960759	23.579763
113.553238	3863.787949	23.584781
113.875216	3878.061007	23.589799
113.740254	3881.777397	23.594816
114.348327	3863.905299	23.599834
114.279332	3865.215473	23.604851
114.179937	3882.302466	23.609869
114.365690	3883.980560	23.614887
114.357081	3887.835513	23.619904
114.548306	3891.742284	23.624922
114.494830	3902.054041	23.629939
114.934199	3901.675202	23.634957
115.318778	3913.545188	23.639975
115.203830	3930.925732	23.644992
115.334411	3913.237981	23.650010
115.409336	3923.452163	23.655027
115.276774	3917.473697	23.660045
115.740473	3922.951099	23.665063
115.491571	3927.162479	23.670080
115.798779	3934.810886	23.675098
115.992461	3935.636350	23.680115
115.808615	3929.898623	23.685133
116.234652	3934.741741	23.690151
115.984043	3949.509452	23.695168
116.153008	3955.588289	23.700186
115.923278	3948.602701	23.705203
115.943525	3954.639580	23.710221
116.330131	3986.393527	23.715239
116.280360	4003.521664	23.720256
116.308242	4004.046595	23.725274
116.601577	4001.477445	23.730291
116.727964	4013.415366	23.735309
117.079567	4034.133701	23.740327
116.904507	4042.813765	23.745344
117.226344	4030.532563	23.750362
117.215860	4035.314385	23.755379
117.467513	4046.809610	23.760397
117.712118	4040.932546	23.765415
117.844502	4063.548064	23.770432
117.876753	4064.467136	23.775450
118.304004	4053.134194	23.780467
118.282878	4063.521024	23.785485
118.541536	4076.518576	23.790503
118.722959	4083.490633	23.795520
118.652383	4092.294004	23.800538
119.013971	4094.383005	23.805555
118.947879	4083.002826	23.810573
118.971871	4084.003181	23.815591
118.983279	4091.000185	23.820608
119.081001	4086.441007	23.825626
118.990175	4115.725030	23.830643
119.286475	4114.726552	23.835661
119.702257	4093.362126	23.840679
119.736584	4103.887057	23.845696
120.066751	4126.490458	23.850714
120.240230	4133.069382	23.855731
120.578070	4128.109510	23.860749
120.778778	4121.166493	23.865767
121.015293	4125.641402	23.870784
120.582055	4117.770512	23.875802
120.845939	4109.147854	23.880819
120.620607	4128.642028	23.885837
120.737359	4133.506789	23.890855
121.021612	4132.276060	23.895872
121.142106	4125.414009	23.900890
121.150164	4132.066721	23.905907
120.996948	4131.234246	23.910925
121.240468	4127.327704	23.915943
121.152397	4146.377981	23.920960
121.403071	4164.785722	23.925978
121.658743	4178.809003	23.930995
121.729698	4192.493937	23.936013
121.657136	4198.885601	23.941031
121.577559	4207.296841	23.946048
121.910549	4209.372081	23.951066
122.124606	4206.433730	23.956083
122.460362	4209.101400	23.961101
122.659782	4201.563311	23.966119
122.539670	4214.966071	23.971136
122.745892	4245.578754	23.976154
123.021199	4233.998752	23.981171
122.787017	4252.234361	23.986189
122.920979	4246.644388	23.991207
122.875445	4262.452088	23.996224
123.330214	4280.854195	24.001242
123.422028	4269.949342	24.006259
123.432595	4273.119950	24.011277
123.822815	4291.775639	24.016295
123.878451	4321.978727	24.021312
123.943874	4309.935336	24.026330
124.011976	4305.948684	24.031347
124.019918	4325.847850	24.036365
124.467611	4327.560071	24.041383
124.217714	4325.929024	24.046400
124.330496	4351.476047	24.051418
124.264697	4339.647616	24.056435
124.768138	4344.561930	24.061453
125.017133	4356.277502	24.066471
124.850704	4373.228480	24.071488
125.031578	4364.784352	24.076506
125.575556	4384.473372	24.081523
125.393926	4390.025291	24.086541
125.542949	4397.962262	24.091559
125.686523	4393.115506	24.096576
125.621446	4414.304369	24.101594
125.973240	4419.779181	24.106611
125.747843	4412.582830	24.111629
126.191651	4409.987570	24.116647
126.559914	4428.766340	24.121664
126.434657	4440.397363	24.126682
126.874975	4433.846886	24.131699
126.940149	4444.819300	24.136717
127.164768	4456.173631	24.141735
127.136950	4451.830754	24.146752
127.434044	4448.057796	24.151770
127.808209	4426.656877	24.156787
127.220462	4431.618061	24.161805
127.483663	4447.319031	24.166823
127.758488	4467.085700	24.171840
128.107039	4469.192656	24.176858
128.206744	4464.188170	24.181875
128.036047	4470.386718	24.186893
128.361008	4476.994301	24.191911
128.192116	4483.326804	24.196928
128.135230	4495.609939	24.201946
128.550697	4482.724736	24.206963
128.379502	4497.647164	24.211981
128.569428	4503.229065	24.216999
128.962923	4513.435484	24.222016
128.566706	4535.515428	24.227034
129.127106	4559.032971	24.232051
129.002304	4545.105517	24.237069
129.321753	4529.463370	24.242087
129.376829	4567.212127	24.247104
129.702131	4553.861459	24.252122
129.566274	4566.565958	24.257139
129.955036	4585.859631	24.262157
129.967208	4585.961202	24.267175
129.915198	4595.319653	24.272192
130.257713	4597.334712	24.277210
130.385937	4612.244388	24.282227
130.435907	4615.329816	24.287245
130.593344	4621.046260	24.292263
130.903289	4621.083275	24.297280
130.899536	4629.693235	24.302298
131.519405	4653.659356	24.307315
131.491744	4644.934184	24.312333
131.588698	4651.114563	24.317351
132.099277	4668.838629	24.322368
131.746036	4659.266866	24.327386
132.119540	4644.301882	24.332403
132.176564	4656.466717	24.337421
132.485372	4664.289235	24.342439
132.262998	4666.845667	24.347456
132.460507	4657.438411	24.352474
132.748178	4668.595081	24.357491
132.359877	4673.247799	24.362509
132.794348	4668.565880	24.367527
132.497908	4683.557212	24.372544
132.619476	4686.874521	24.377562
133.012956	4698.075934	24.382579
132.836385	4713.802596	24.387597
132.470481	4707.794665	24.392615
133.220083	4731.271365	24.397632
133.173762	4735.834524	24.402650
133.336457	4755.265761	24.407667
133.454718	4770.290621	24.412685
133.668370	4776.278146	24.417703
134.151076	4776.627558	24.422720
133.921076	4809.544912	24.427738
134.240009	4810.638705	24.432755
134.291670	4800.644440	24.437773
134.349353	4814.680933	24.442791
134.632606	4846.245455	24.447808
134.749997	4842.823748	24.452826
134.942464	4828.945583	24.457843
135.310115	4827.641180	24.462861
135.587849	4858.962153	24.467879
135.835240	4866.118938	24.472896
135.656797	4850.885115	24.477914
136.066563	4853.998542	24.482931
135.557458	4864.416537	24.487949
136.273121	4849.433010	24.492967
136.372241	4857.756020	24.497984
136.720100	4873.372174	24.503002
136.912397	4878.884135	24.508019
136.790007	4871.813856	24.513037
136.870500	4875.840355	24.518055
136.853298	4877.408196	24.523072
136.895291	4894.496957	24.528090
136.856545	4882.480571	24.533107
137.074650	4895.117796	24.538125
137.127819	4909.300789	24.543143
137.538640	4915.284136	24.548160
137.481133	4925.636215	24.553178
137.824492	4945.205949	24.558195
137.644310	4936.427468	24.563213
137.790110	4962.337365	24.568231
138.044863	4963.446499	24.573248
137.822673	4967.625397	24.578266
138.436600	4954.725124	24.583283
138.652176	4995.108253	24.588301
138.809603	5014.241865	24.593319
138.908533	5005.001476	24.598336
138.854074	5000.849856	24.603354
139.045366	5000.873801	24.608371
139.163097	5021.491156	24.613389
139.621612	5040.025832	24.618407
139.817535	5018.050399	24.623424
139.967548	5018.768178	24.628442
140.322364	5039.160554	24.633459
140.484691	5053.742182	24.638477
140.644571	5068.205329	24.643495
140.725443	5060.182865	24.648512
140.733586	5056.825620	24.653530
140.476070	5060.324152	24.658547
140.852160	5048.483584	24.663565
140.881865	5063.468634	24.668583
141.159601	5058.137295	24.673600
141.412855	5072.364936	24.678618
141.398533	5081.047759	24.683635
141.685327	5104.077869	24.688653
141.677714	5101.318501	24.693671
141.858028	5091.200823	24.698688
141.873477	5091.121538	24.703706
142.340821	5097.246800	24.708723
142.299006	5120.165087	24.713741
141.848577	5132.835803	24.718759
142.194287	5108.685853	24.723776
142.086229	5134.412782	24.728794
142.351848	5133.096080	24.733811
142.369135	5147.767511	24.738829
142.430320	5157.140273	24.743847
142.647716	5153.965758	24.748864
142.743483	5182.996940	24.753882
142.972157	5201.313877	24.758899
143.359078	5202.722455	24.763917
143.112167	5198.753766	24.768935
143.416996	5218.056978	24.773952
144.073319	5249.352797	24.778970
144.092882	5234.431557	24.783987
143.961852	5250.965821	24.789005
144.027186	5260.110789	24.794023
144.571842	5241.248754	24.799040
144.154528	5259.212250	24.804058
144.404331	5278.356908	24.809075
145.091894	5289.745596	24.814093
144.883330	5281.872814	24.819111
145.429541	5288.715060	24.824128
145.480624	5295.543054	24.829146
145.839334	5303.994675	24.834163
145.855717	5326.095360	24.839181
145.843341	5315.248724	24.844199
146.000980	5317.812158	24.849216
146.200410	5331.982000	24.854234
146.573475	5343.554981	24.859251
146.553792	5337.723068	24.864269
146.180176	5355.148730	24.869287
146.720950	5359.394979	24.874304
146.450942	5365.227602	24.879322
146.899289	5362.533404	24.884339
147.057594	5387.365139	24.889357
147.277148	5380.292068	24.894375
147.821051	5403.715980	24.899392
147.698692	5402.005473	24.904410
147.611243	5394.906741	24.909427
147.916967	5409.041373	24.914445
148.125814	5413.728716	24.919463
148.606672	5421.086954	24.924480
148.497890	5429.730459	24.929498
148.383764	5442.008837	24.934515
148.498167	5421.447929	24.939533
148.602977	5449.219016	24.944551
148.596720	5458.434988	24.949568
148.740956	5471.106542	24.954586
148.670913	5488.967644	24.959603
149.432195	5493.586173	24.964621
149.230061	5511.992375	24.969639
149.557189	5508.048447	24.974656
149.736390	5511.743434	24.979674
149.970688	5527.612485	24.984691
149.890351	5527.592334	24.989709
149.954180	5545.718007	24.994727
150.684969	5560.836918	24.999744
150.630821	5563.860208	25.004762
150.545339	5560.156497	25.009779
151.092633	5576.865652	25.014797
150.697954	5589.204676	25.019815
151.316562	5590.964003	25.024832
151.221263	5602.452747	25.029850
151.301583	5599.738213	25.034867
151.545809	5595.785519	25.039885
151.339164	5625.486025	25.044903
151.967418	5613.591160	25.049920
152.225004	5653.803695	25.054938
152.118580	5660.466527	25.059955
152.301078	5647.055448	25.064973
152.245500	5643.635373	25.069991
152.403909	5655.564148	25.075008
152.623661	5685.187227	25.080026
152.722309	5687.545498	25.085043
152.992687	5689.884056	25.090061
153.260518	5703.417706	25.095079
153.560134	5702.589854	25.100096
153.536766	5708.715334	25.105114
153.663700	5709.667286	25.110131
154.167101	5700.110823	25.115149
154.359070	5726.875826	25.120167
154.488819	5732.490951	25.125184
154.522730	5738.876677	25.130202
154.881008	5723.461578	25.135219
154.836710	5709.646951	25.140237
154.655074	5738.753746	25.145255
154.643818	5748.529012	25.150272
154.958378	5755.035312	25.155290
154.951105	5753.035263	25.160307
155.358813	5768.268787	25.165325
155.490180	5780.360797	25.170343
155.926928	5789.857330	25.175360
156.030911	5791.150107	25.180378
156.023470	5806.304617	25.185395
156.017222	5818.374904	25.190413
156.238713	5820.821172	25.195431
156.071825	5824.710828	25.200448
156.500902	5849.978904	25.205466
156.068285	5851.227664	25.210483
156.554816	5865.330080	25.215501
156.791477	5895.489774	25.220519
156.946578	5879.593493	25.225536
157.202620	5906.535631	25.230554
156.886324	5921.573951	25.235571
157.558127	5930.137578	25.240589
157.599712	5948.809557	25.245607
158.116245	5944.566097	25.250624
158.200064	5962.700763	25.255642
158.170210	5978.972212	25.260659
158.795022	5971.055876	25.265677
158.551041	5986.208303	25.270695
159.218006	6017.417291	25.275712
159.339967	6007.735465	25.280730
159.620759	6000.690187	25.285747
159.519203	6004.115911	25.290765
159.707769	6012.769667	25.295783
159.605941	6021.070986	25.300800
159.985281	6032.749751	25.305818
159.657808	6023.583546	25.310835
160.107020	6029.835806	25.315853
160.224830	6072.042343	25.320871
160.504787	6063.713221	25.325888
160.713064	6070.564011	25.330906
160.755641	6077.213425	25.335923
161.058435	6076.692139	25.340941
161.061936	6081.645127	25.345959
161.140384	6094.848177	25.350976
161.344299	6109.265248	25.355994
161.311541	6120.052253	25.361011
161.669843	6125.987264	25.366029
161.864659	6128.683283	25.371047
162.046462	6157.154775	25.376064
162.498814	6154.834224	25.381082
162.300121	6144.088669	25.386099
162.585181	6148.121464	25.391117
162.712576	6178.996667	25.396135
162.712973	6182.274471	25.401152
162.914480	6194.604839	25.406170
162.955540	6201.321491	25.411187
163.450563	6200.676307	25.416205
163.545930	6210.885071	25.421223
163.704259	6217.531168	25.426240
163.877001	6221.151795	25.431258
163.753869	6224.420489	25.436275
164.025201	6241.605521	25.441293
164.021997	6255.122223	25.446311
164.382370	6253.783868	25.451328
164.905716	6266.989150	25.456346
164.955052	6276.154289	25.461363
165.036608	6254.358628	25.466381
165.084636	6270.287955	25.471399
165.139837	6279.814757	25.476416
165.469775	6296.531858	25.481434
165.432566	6327.453450	25.486451
165.676280	6312.827246	25.491469
165.844395	6320.592738	25.496487
165.711563	6328.033516	25.501504
166.384079	6345.775267	25.506522
166.273469	6361.956511	25.511539
166.854061	6355.398205	25.516557
166.718563	6363.051664	25.521575
166.736357	6377.598171	25.526592
167.214939	6385.618332	25.531610
167.270914	6382.810826	25.536627
167.840076	6384.329577	25.541645
167.617105	6397.285019	25.546663
167.909889	6432.995282	25.551680
168.123402	6425.869190	25.556698
168.169161	6418.135324	25.561715
168.365288	6406.102187	25.566733
168.647106	6443.123074	25.571751
168.750480	6460.975532	25.576768
169.006892	6448.482356	25.581786
169.002924	6451.040788	25.586803
169.455870	6462.518326	25.591821
169.522814	6488.055166	25.596839
169.342046	6489.040290	25.601856
169.810783	6479.462309	25.606874
169.685241	6503.595400	25.611891
170.018778	6505.945697	25.616909
170.283537	6508.869228	25.621927
170.249357	6505.863975	25.626944
170.354952	6542.355888	25.631962
170.300682	6554.164964	25.636979
170.748127	6558.356094	25.641997
170.887639	6565.461010	25.647015
171.251220	6555.138859	25.652032
171.444744	6561.085513	25.657050
171.438655	6595.557204	25.662067
171.632314	6603.532813	25.667085
172.059248	6593.206470	25.672103
172.025101	6612.791459	25.677120
172.082091	6629.496135	25.682138
172.092091	6619.181570	25.687156
172.294155	6646.310695	25.692173
172.655170	6673.363991	25.697191
173.088827	6656.682624	25.702208
173.493766	6666.613344	25.707226
173.222800	6682.122122	25.712244
173.322945	6674.577591	25.717261
173.704937	6687.390398	25.722279
173.961131	6703.300340	25.727296
174.094617	6704.871423	25.732314
173.911925	6705.575350	25.737332
173.960312	6717.777870	25.742349
174.240252	6748.412431	25.747367
174.566208	6743.768308	25.752384
174.684106	6728.459665	25.757402
174.886851	6745.314812	25.762420
174.937334	6763.269673	25.767437
175.209599	6766.951946	25.772455
175.344405	6774.814517	25.777472
175.708555	6770.341262	25.782490
175.715989	6795.803781	25.787508
175.728628	6817.206713	25.792525
176.151946	6820.029293	25.797543
176.140286	6833.604985	25.802560
176.492297	6840.510721	25.807578
176.564016	6843.192161	25.812596
176.842072	6859.151018	25.817613
177.011940	6881.179323	25.822631
176.791148	6889.220801	25.827648
177.254169	6885.783279	25.832666
177.046248	6909.081284	25.837684
177.390476	6928.739600	25.842701
178.057625	6939.699358	25.847719
177.642669	6939.615185	25.852736
178.252118	6939.779524	25.857754
178.174193	6969.567622	25.862772
178.520649	6964.169554	25.867789
178.351988	6990.483640	25.872807
178.478447	7001.113824	25.877824
178.825892	7003.783991	25.882842
179.090274	7041.742764	25.887860
179.605701	7052.349665	25.892877
179.932179	7045.654691	25.897895
179.800842	7051.450062	25.902912
180.212570	7059.731653	25.907930
180.570105	7058.919759	25.912948
180.789057	7077.698050	25.917965
181.037528	7077.903528	25.922983
180.923242	7080.824825	25.928000
180.729487	7068.939863	25.933018
180.845674	7097.049052	25.938036
181.200836	7113.547082	25.943053
181.560402	7131.983261	25.948071
181.826140	7143.339455	25.953088
182.328317	7148.523423	25.958106
182.468760	7139.882484	25.963124
182.611615	7149.273268	25.968141
182.676637	7157.003447	25.973159
182.492365	7175.394474	25.978176
183.003145	7186.999231	25.983194
183.112526	7193.532554	25.988212
182.973229	7202.137977	25.993229
183.280799	7207.198977	25.998247
183.524485	7221.356923	26.003264
183.820620	7225.566936	26.008282
184.010605	7221.591692	26.013300
183.861649	7241.322438	26.018317
184.268741	7272.269348	26.023335
184.307244	7295.626438	26.028352
184.716070	7280.257377	26.033370
184.851127	7288.708838	26.038388
184.927769	7305.305065	26.043405
185.357495	7307.383254	26.048423
185.162674	7327.083096	26.053440
185.662666	7341.333469	26.058458
186.105515	7331.185539	26.063476
186.210690	7338.355150	26.068493
186.531037	7355.319889	26.073511
186.199253	7376.840344	26.078528
186.698943	7361.893267	26.083546
186.873609	7359.447532	26.088564
187.088702	7369.418338	26.093581
187.561875	7382.214681	26.098599
187.762420	7395.412830	26.103616
187.581495	7375.876657	26.108634
187.301171	7367.898121	26.113652
187.796534	7393.318005	26.118669
187.883801	7406.892417	26.123687
188.096717	7416.974654	26.128704
188.179556	7410.469412	26.133722
188.146541	7423.871555	26.138740
188.263101	7441.537883	26.143757
188.469173	7460.714100	26.148775
188.718364	7487.908954	26.153792
188.548678	7509.383906	26.158810
189.046450	7534.031050	26.163828
189.306135	7516.943587	26.168845
189.459986	7524.034362	26.173863
189.391142	7555.364455	26.178880
189.883354	7558.461664	26.183898
190.133782	7579.640489	26.188916
189.933988	7615.796313	26.193933
190.548025	7611.631202	26.198951
190.758473	7632.473336	26.203968
190.946183	7637.696826	26.208986
191.085724	7657.541871	26.214004
191.621716	7676.593750	26.219021
191.923528	7661.382970	26.224039
191.646028	7673.989353	26.229056
192.349806	7697.788399	26.234074
192.304543	7709.973694	26.239092
192.431025	7722.498404	26.244109
192.890066	7718.461255	26.249127
192.912327	7723.694784	26.254144
193.356362	7753.559180	26.259162
193.661295	7772.531221	26.264180
193.789198	7759.303770	26.269197
193.810658	7757.459771	26.274215
194.021343	7782.096460	26.279232
193.972923	7775.781289	26.284250
193.989150	7783.779335	26.289268
194.580428	7818.585011	26.294285
194.634981	7834.850739	26.299303
194.824573	7831.488120	26.304320
194.653957	7834.590156	26.309338
194.927786	7849.346952	26.314356
195.228434	7881.515240	26.319373
195.413609	7882.295863	26.324391
195.884105	7894.402385	26.329408
195.817547	7914.931539	26.334426
196.477134	7912.266990	26.339444
196.711026	7918.969056	26.344461
197.017747	7936.518677	26.349479
197.255630	7963.964303	26.354496
197.372205	7959.772612	26.359514
197.513488	7946.050572	26.364532
197.303280	7958.267249	26.369549
197.763048	7981.851876	26.374567
197.730723	7988.943695	26.379584
197.969298	7974.041546	26.384602
198.376772	8004.783498	26.389620
197.934909	8026.890856	26.394637
198.325861	8031.796588	26.399655
198.436379	8029.926817	26.404672
198.566790	8049.422614	26.409690
198.911742	8062.473029	26.414708
199.111632	8088.805238	26.419725
199.585700	8098.545492	26.424743
199.397979	8118.786993	26.429760
199.450153	8132.120534	26.434778
199.729591	8132.172850	26.439796
199.697736	8136.796432	26.444813
200.212083	8166.043570	26.449831
200.503404	8181.102575	26.454848
200.602735	8195.864901	26.459866
200.839336	8190.976010	26.464884
200.954946	8216.955352	26.469901
201.517077	8228.027090	26.474919
201.483034	8237.880522	26.479936
201.836906	8253.052910	26.484954
202.081759	8256.873953	26.489972
202.232036	8273.863059	26.494989
202.378438	8294.651285	26.500007
202.408228	8304.426481	26.505024
202.522645	8315.310780	26.510042
203.110976	8319.227877	26.515060
203.581126	8339.706711	26.520077
204.016858	8347.749930	26.525095
204.049814	8343.639685	26.530112
204.413954	8347.888384	26.535130
204.579453	8348.196587	26.540148
204.622349	8361.238877	26.545165
204.877907	8376.274838	26.550183
205.142726	8379.991803	26.555200
205.140031	8398.161693	26.560218
205.368004	8392.481862	26.565236
205.627885	8404.477876	26.570253
205.637050	8415.205579	26.575271
205.754848	8435.004005	26.580288
205.383664	8442.008675	26.585306
205.794055	8449.702510	26.590324
205.986173	8490.375364	26.595341
206.184422	8511.712131	26.600359
206.479009	8525.188672	26.605376
206.588290	8547.366361	26.610394
207.093649	8544.656310	26.615412
206.731896	8575.641457	26.620429
207.149856	8585.905578	26.625447
207.411923	8602.569410	26.630464
207.427938	8612.326595	26.635482
208.065497	8649.645958	26.640500
208.366175	8671.123534	26.645517
208.785406	8668.783684	26.650535
208.989905	8673.480209	26.655552
209.198329	8693.120643	26.660570
209.683615	8685.590671	26.665588
209.504229	8701.000452	26.670605
209.904908	8722.787640	26.675623
210.344465	8750.259596	26.680640
210.117471	8747.217644	26.685658
210.645537	8721.280804	26.690676
210.852499	8742.822794	26.695693
211.022634	8780.611130	26.700711
211.212399	8772.071414	26.705728
211.466076	8769.720310	26.710746
211.960789	8770.404157	26.715764
211.924303	8802.614276	26.720781
211.872039	8803.551529	26.725799
212.238533	8805.854599	26.730816
212.267209	8819.873088	26.735834
212.831191	8841.437347	26.740852
212.657920	8848.055863	26.745869
212.923593	8851.614492	26.750887
213.465329	8861.595285	26.755904
213.352249	8901.409157	26.760922
213.673299	8897.456733	26.765940
213.692246	8885.388366	26.770957
214.247141	8899.199481	26.775975
214.095858	8921.461702	26.780992
214.150871	8941.824821	26.786010
214.207293	8933.102272	26.791028
214.692955	8947.830613	26.796045
214.927597	8969.065109	26.801063
215.244080	8975.227073	26.806080
214.962269	9004.834142	26.811098
215.394284	9019.671439	26.816116
215.312307	9028.626746	26.821133
215.682169	9029.028792	26.826151
216.119391	9056.074783	26.831168
215.954711	9084.597799	26.836186
216.210467	9090.271283	26.841204
216.950717	9106.978722	26.846221
217.356303	9120.242892	26.851239
217.750330	9089.141164	26.856256
218.090915	9097.387941	26.861274
218.462251	9132.248613	26.866292
218.484614	9139.406736	26.871309
218.391435	9140.133387	26.876327
218.513681	9136.939932	26.881344
218.940425	9148.932572	26.886362
219.192001	9150.899466	26.891380
219.263836	9164.279462	26.896397
219.206943	9192.162647	26.901415
219.460826	9183.457743	26.906432
219.724257	9191.704715	26.911450
220.000232	9232.460927	26.916468
220.114498	9234.183514	26.921485
220.638475	9257.392413	26.926503
220.938044	9277.714773	26.931520
220.700026	9283.857417	26.936538
220.945009	9288.960152	26.941556
221.084951	9296.277710	26.946573
221.451276	9316.412662	26.951591
221.815838	9329.171831	26.956608
221.664878	9350.616260	26.961626
222.218174	9356.203663	26.966644
222.012198	9387.320608	26.971661
222.176721	9404.925289	26.976679
222.364640	9422.008653	26.981696
222.690401	9437.100187	26.986714
222.825948	9459.054280	26.991732
223.230698	9481.422327	26.996749
223.474701	9503.805149	27.001767
223.955631	9530.370576	27.006784
224.134241	9533.650745	27.011802
224.357604	9540.577356	27.016820
224.607250	9562.864813	27.021837
224.642421	9565.770932	27.026855
225.050836	9594.555402	27.031872
225.211064	9616.279583	27.036890
225.770229	9625.752319	27.041908
225.929168	9623.114291	27.046925
226.149670	9645.065632	27.051943
226.230796	9664.628275	27.056960
226.354505	9671.668289	27.061978
226.759107	9671.147013	27.066996
227.273382	9692.981359	27.072013
227.173094	9704.310874	27.077031
227.697386	9692.148161	27.082048
228.021968	9712.711904	27.087066
227.890811	9742.263951	27.092084
228.263122	9748.248438	27.097101
228.305057	9740.109121	27.102119
228.744265	9743.784208	27.107136
228.677364	9784.115663	27.112154
229.292770	9772.831026	27.117172
229.199787	9788.244127	27.122189
229.283130	9815.137219	27.127207
229.615710	9809.233239	27.132224
230.060610	9820.078150	27.137242
229.818351	9852.564633	27.142260
229.816002	9867.980165	27.147277
230.297193	9889.235023	27.152295
230.410231	9880.707389	27.157312
230.366489	9909.714428	27.162330
230.956945	9935.923749	27.167348
230.825601	9964.000175	27.172365
231.501211	9967.416502	27.177383
231.670664	9978.204636	27.182400
231.836897	10013.489450	27.187418
231.937539	10018.162578	27.192436
232.583610	10033.007209	27.197453
232.855026	10049.125962	27.202471
233.157556	10054.788915	27.207488
233.753657	10083.147072	27.212506
233.613940	10066.805753	27.217524
233.956712	10077.690558	27.222541
234.199972	10106.169276	27.227559
234.352743	10103.636947	27.232576
234.611493	10103.702148	27.237594
234.705461	10133.324061	27.242612
234.756236	10164.269355	27.247629
234.836483	10169.860377	27.252647
235.251424	10169.656384	27.257664
235.091119	10214.334159	27.262682
235.521364	10242.782229	27.267700
235.945857	10260.169259	27.272717
236.074793	10271.102916	27.277735
236.667802	10289.329361	27.282752
236.376704	10302.648979	27.287770
236.560113	10321.329093	27.292788
236.908292	10339.982793	27.297805
237.067220	10372.627753	27.302823
237.529092	10384.427274	27.307840
237.837600	10398.591543	27.312858
237.794599	10431.577967	27.317876
237.760994	10463.727178	27.322893
237.946674	10478.330069	27.327911
238.664361	10485.510188	27.332928
239.042530	10520.618541	27.337946
239.087660	10550.391083	27.342964
239.687189	10552.852045	27.347981
239.963650	10585.113324	27.352999
240.219868	10598.119847	27.358016
240.547236	10597.753089	27.363034
240.653609	10606.352063	27.368052
241.238477	10640.926351	27.373069
241.085170	10655.056084	27.378087
241.388250	10646.510033	27.383104
241.827993	10664.421162	27.388122
242.226760	10682.369802	27.393140
243.022392	10674.044832	27.398157
242.965423	10704.266972	27.403175
243.326900	10717.309765	27.408192
243.331726	10699.523706	27.413210
243.499813	10694.055389	27.418228
243.730069	10726.627063	27.423245
243.471810	10740.259847	27.428263
244.027479	10739.334703	27.433280
243.840027	10776.643364	27.438298
244.069804	10780.591970	27.443316
244.470443	10783.908185	27.448333
244.751814	10820.865374	27.453351
244.870079	10842.716320	27.458368
245.090631	10861.920266	27.463386
245.193869	10863.629888	27.468404
245.274902	10867.558979	27.473421
245.408944	10914.315300	27.478439
245.544332	10932.076151	27.483456
245.893039	10940.547833	27.488474
246.014614	10962.329078	27.493492
246.671797	10988.496818	27.498509
246.891709	11002.612459	27.503527
247.499371	11003.483347	27.508544
247.927919	11039.180028	27.513562
248.007414	11052.779332	27.518580
248.436138	11046.577801	27.523597
248.701475	11057.752558	27.528615
248.986151	11057.013957	27.533632
249.299744	11076.587193	27.538650
249.618158	11110.551149	27.543668
249.933540	11099.501052	27.548685
250.186866	11089.475786	27.553703
250.091567	11125.609739	27.558720
250.265218	11133.257354	27.563738
250.374007	11140.439121	27.568756
250.915280	11153.545518	27.573773
250.913673	11162.094889	27.578791
251.158257	11171.858420	27.583808
251.418603	11198.578879	27.588826
251.285583	11240.817826	27.593844
251.700075	11240.561122	27.598861
251.904769	11259.879236	27.603879
252.225493	11277.908398	27.608896
252.420553	11313.898703	27.613914
252.430748	11332.323466	27.618932
252.855311	11347.279974	27.623949
252.762453	11378.755498	27.628967
253.256601	11390.693015	27.633984
253.603530	11401.885255	27.639002
253.756423	11448.167389	27.644020
254.401796	11477.762144	27.649037
254.832354	11487.789754	27.654055
254.865987	11486.016570	27.659072
254.952435	11516.046401	27.664090
255.026893	11544.303505	27.669108
255.686253	11546.330944	27.674125
255.892917	11568.894569	27.679143
256.189425	11597.784656	27.684160
256.687794	11592.015694	27.689178
256.632504	11629.102848	27.694196
257.334103	11649.774597	27.699213
257.652100	11656.320200	27.704231
258.029185	11673.361339	27.709248
258.571485	11663.892956	27.714266
258.479383	11674.118894	27.719284
258.873958	11698.643064	27.724301
259.136414	11705.753221	27.729319
258.967987	11703.524997	27.734336
259.403771	11736.919476	27.739354
259.525956	11733.705033	27.744372
259.730773	11756.203058	27.749389
259.919291	11771.970164	27.754407
260.359050	11789.933762	27.759424
260.518507	11790.070522	27.764442
260.704705	11812.863168	27.769460
260.976400	11840.758145	27.774477
260.988984	11853.969009	27.779495
261.233405	11868.629641	27.784512
261.596749	11882.414355	27.789530
261.961866	11884.899294	27.794548
262.389344	11910.472363	27.799565
262.441166	11952.452626	27.804583
262.463051	11949.658040	27.809600
263.352466	11957.958220	27.814618
263.040216	11963.694280	27.819636
263.676073	11984.152027	27.824653
263.982623	12015.877131	27.829671
263.947255	12017.830349	27.834688
264.322809	12023.814378	27.839706
264.370574	12037.163741	27.844724
264.660112	12075.523906	27.849741
264.820669	12098.886020	27.854759
265.112625	12110.929170	27.859776
265.466323	12115.253880	27.864794
265.585419	12131.243930	27.869812
265.950927	12156.760671	27.874829
266.031572	12186.339754	27.879847
266.126792	12211.545956	27.884864
266.176181	12212.226344	27.889882
266.248752	12251.168698	27.894900
267.211060	12270.941089	27.899917
267.641623	12299.678739	27.904935
267.304817	12317.402553	27.909952
267.996636	12344.189926	27.914970
268.244857	12380.867876	27.919988
268.734372	12395.271072	27.925005
268.916708	12396.012221	27.930023
269.039799	12425.256229	27.935040
269.585288	12442.439738	27.940058
269.627103	12462.733124	27.945076
270.189701	12493.722051	27.950093
270.264954	12512.330427	27.955111
270.395085	12536.812916	27.960128
270.913811	12532.971899	27.965146
270.792359	12576.810077	27.970164
271.372659	12603.955844	27.975181
271.275906	12616.274721	27.980199
271.833662	12638.334386	27.985216
272.427383	12650.416319	27.990234
272.717795	12679.817490	27.995252
272.911229	12700.284650	28.000269
273.444916	12721.329794	28.005287
273.317997	12727.501090	28.010304
273.629751	12739.246021	28.015322
273.881999	12774.464426	28.020340
274.576866	12771.627839	28.025357
274.527963	12809.402046	28.030375
274.777499	12817.620900	28.035392
275.267431	12832.059872	28.040410
275.531422	12866.082238	28.045428
275.895129	12883.355339	28.050445
275.750986	12886.903020	28.055463
276.233116	12895.936673	28.060480
276.636115	12920.209227	28.065498
276.868034	12959.910834	28.070516
277.024739	12956.902364	28.075533
277.529367	12966.635848	28.080551
277.495587	13006.702891	28.085568
277.876571	13026.362705	28.090586
277.949149	13049.510698	28.095604
278.220139	13052.672344	28.100621
278.788243	13076.800475	28.105639
278.884784	13103.367615	28.110656
279.284241	13112.275607	28.115674
279.266332	13146.802858	28.120692
279.507616	13172.960960	28.125709
279.792951	13184.545929	28.130727
279.903890	13213.709871	28.135744
280.005165	13228.638831	28.140762
280.064900	13248.909765	28.145780
280.549043	13293.206041	28.150797
280.788035	13311.989185	28.155815
281.142402	13335.455007	28.160832
281.752246	13340.231698	28.165850
282.283314	13367.044977	28.170868
282.431734	13393.669415	28.175885
282.670357	13412.378682	28.180903
282.977897	13427.982793	28.185920
283.421466	13432.613661	28.190938
283.965323	13469.574564	28.195956
283.707009	13492.131840	28.200973
284.231925	13494.292048	28.205991
284.079212	13504.592188	28.211008
284.578146	13534.951563	28.216026
284.734754	13567.521485	28.221044
285.070410	13579.143331	28.226061
285.510013	13618.352156	28.231079
285.812270	13631.917633	28.236096
286.019512	13642.816236	28.241114
286.150489	13671.144952	28.246132
286.638009	13702.054862	28.251149
286.885594	13725.703554	28.256167
287.172661	13753.194363	28.261184
287.779823	13745.793955	28.266202
288.102831	13781.217166	28.271220
288.566007	13786.156096	28.276237
288.865617	13813.154897	28.281255
289.072162	13842.986455	28.286272
289.412417	13855.631942	28.291290
289.703742	13845.404878	28.296308
290.026553	13863.260916	28.301325
290.456355	13875.535518	28.306343
290.545534	13915.025131	28.311360
290.932016	13914.277468	28.316378
291.510153	13921.037864	28.321396
291.337704	13957.720364	28.326413
291.762844	13967.651160	28.331431
291.801516	13993.516321	28.336448
292.347966	14001.542552	28.341466
292.269960	14009.213420	28.346484
292.090820	14041.033003	28.351501
292.764386	14072.503781	28.356519
293.081739	14113.957341	28.361536
293.410560	14115.059635	28.366554
293.294334	14149.364976	28.371572
293.710634	14176.526315	28.376589
294.191286	14200.486221	28.381607
293.905315	14241.948391	28.386624
294.631352	14264.935020	28.391642
294.872838	14294.333040	28.396660
295.027239	14321.648193	28.401677
295.776694	14334.848870	28.406695
295.705299	14349.891697	28.411712
296.233392	14366.444331	28.416730
297.132725	14394.783680	28.421748
297.278604	14415.865174	28.426765
297.891940	14430.441986	28.431783
298.044790	14433.305123	28.436800
298.509275	14448.751145	28.441818
298.598873	14478.039078	28.446836
298.799925	14497.386113	28.451853
298.885363	14511.117363	28.456871
299.340105	14520.107611	28.461888
299.403383	14528.800112	28.466906
299.469012	14573.184802	28.471924
299.893844	14611.378961	28.476941
300.305467	14627.303466	28.481959
300.071648	14627.868441	28.486976
300.714104	14643.817857	28.491994
300.862253	14685.719992	28.497012
300.961235	14714.516736	28.502029
301.539205	14716.000221	28.507047
301.507949	14755.432992	28.512064
301.983872	14776.701525	28.517082
302.407896	14788.684683	28.522100
302.619641	14814.016735	28.527117
302.946919	14852.909896	28.532135
303.215330	14877.914377	28.537152
303.369272	14890.778976	28.542170
303.802094	14927.415676	28.547188
304.184764	14969.350710	28.552205
304.680260	14971.188218	28.557223
304.606343	14996.748966	28.562240
305.162803	15019.035089	28.567258
305.434362	15051.883686	28.572276
305.331149	15064.385923	28.577293
306.012606	15111.112853	28.582311
306.291199	15140.167479	28.587328
306.693223	15145.926904	28.592346
307.223959	15169.380438	28.597364
307.378403	15212.608159	28.602381
308.078916	15235.102428	28.607399
308.192957	15247.313630	28.612416
308.586586	15254.311507	28.617434
308.855616	15290.679831	28.622452
309.151730	15315.694593	28.627469
309.897107	15335.334056	28.632487
309.674945	15340.716040	28.637504
310.236153	15364.612361	28.642522
310.785494	15376.969213	28.647540
310.766129	15427.747713	28.652557
311.365898	15412.531583	28.657575
311.253006	15438.737682	28.662592
311.733133	15464.850581	28.667610
311.999247	15501.976269	28.672628
312.001866	15514.658349	28.677645
312.420957	15524.261752	28.682663
312.566739	15562.428612	28.687680
312.594605	15602.124718	28.692698
312.981018	15634.593070	28.697716
313.404739	15665.750503	28.702733
314.135759	15680.682486	28.707751
314.022050	15706.846602	28.712768
314.786883	15737.415175	28.717786
315.417405	15750.948688	28.722804
315.640128	15765.739372	28.727821
315.813487	15779.203453	28.732839
316.120088	15814.999428	28.737856
316.409851	15852.530162	28.742874
316.683516	15853.491984	28.747892
317.005823	15871.876671	28.752909
317.291339	15915.207525	28.757927
317.630125	15939.745007	28.762944
317.958597	15952.940919	28.767962
318.473153	15963.942391	28.772980
318.733516	15991.608458	28.777997
319.074160	16032.005644	28.783015
319.177837	16045.090633	28.788032
319.439657	16069.114672	28.793050
320.146209	16088.763040	28.798068
320.160328	16096.150193	28.803085
320.635431	16135.182746	28.808103
321.079099	16152.586393	28.813120
321.110771	16155.718851	28.818138
321.625161	16176.563674	28.823156
321.951684	16186.660266	28.828173
322.293610	16220.180396	28.833191
322.593709	16232.014898	28.838208
322.824610	16255.175986	28.843226
323.272768	16277.595199	28.848244
323.434616	16278.670076	28.853261
323.739395	16282.299559	28.858279
324.097221	16312.799350	28.863296
324.235536	16321.284998	28.868314
324.690949	16354.421040	28.873332
324.934728	16374.195060	28.878349
324.950656	16400.865236	28.883367
325.690091	16413.019699	28.888384
326.030587	16439.461389	28.893402
326.177013	16482.260421	28.898420
326.286206	16495.294430	28.903437
326.699743	16503.793016	28.908455
326.796914	16536.957092	28.913472
326.906052	16585.823674	28.918490
327.448544	16615.825464	28.923508
327.501337	16636.433517	28.928525
328.085285	16659.484848	28.933543
328.552511	16697.402691	28.938560
328.642412	16739.508852	28.943578
329.128376	16758.614515	28.948596
329.290813	16790.884203	28.953613
329.608375	16822.083451	28.958631
329.826074	16862.711035	28.963648
330.261764	16896.869523	28.968666
330.854372	16916.071224	28.973684
330.689390	16940.747021	28.978701
331.425183	16991.656215	28.983719
331.530040	17034.726751	28.988736
331.876597	17055.835251	28.993754
332.430870	17076.632086	28.998772
332.696488	17126.375905	29.003789
333.200023	17149.839945	29.008807
333.639452	17182.496472	29.013824
333.995461	17193.759799	29.018842
334.808145	17228.739270	29.023860
334.822014	17249.914013	29.028877
335.270550	17280.589749	29.033895
335.503655	17303.952115	29.038912
335.632962	17327.856480	29.043930
336.220490	17348.402307	29.048948
336.498552	17374.673006	29.053965
337.070987	17413.462436	29.058983
337.288117	17445.393410	29.064000
337.345451	17462.956843	29.069018
337.722305	17498.350892	29.074036
337.862931	17535.114228	29.079053
338.248813	17563.854425	29.084071
338.665494	17581.043409	29.089088
338.673742	17616.481271	29.094106
339.336832	17647.845660	29.099124
339.427407	17700.594166	29.104141
340.049105	17702.745275	29.109159
340.420240	17743.463172	29.114176
340.739451	17790.873876	29.119194
340.872260	17818.735900	29.124212
341.055215	17833.505082	29.129229
341.544138	17855.048157	29.134247
341.915089	17897.646730	29.139264
342.092443	17938.141797	29.144282
342.458126	17970.687568	29.149300
343.174529	17990.409106	29.154317
343.641295	18016.324984	29.159335
344.036997	18048.722526	29.164352
344.080961	18080.164806	29.169370
344.791889	18086.165829	29.174388
345.081449	18098.711096	29.179405
345.327075	18143.666797	29.184423
345.565849	18153.514319	29.189440
346.135912	18185.733597	29.194458
346.362999	18199.245961	29.199476
346.357747	18223.856316	29.204493
346.959144	18257.126556	29.209511
347.224022	18293.187026	29.214528
347.267938	18312.254052	29.219546
347.859751	18323.499693	29.224564
347.985335	18360.243718	29.229581
348.953109	18407.270084	29.234599
349.061891	18430.687692	29.239616
349.328178	18448.658977	29.244634
350.129118	18460.850523	29.249652
350.043580	18503.835002	29.254669
349.817363	18529.486320	29.259687
350.945820	18556.693357	29.264704
351.047567	18600.189344	29.269722
351.248152	18604.066680	29.274740
351.492441	18637.177598	29.279757
352.190456	18681.149016	29.284775
352.502407	18716.772347	29.289792
352.863639	18751.631054	29.294810
353.302602	18776.299673	29.299828
353.836570	18794.774046	29.304845
353.660761	18821.776149	29.309863
354.104359	18861.772416	29.314880
354.695322	18906.107302	29.319898
354.612808	18917.693296	29.324916
355.115441	18964.656241	29.329933
355.530904	18984.556363	29.334951
356.286998	19011.430047	29.339968
356.711634	19055.266364	29.344986
356.824967	19071.636964	29.350004
356.799064	19105.830595	29.355021
357.402482	19147.271747	29.360039
358.035060	19156.348676	29.365056
358.302095	19185.819058	29.370074
358.779135	19232.150205	29.375092
359.165658	19264.947288	29.380109
359.651856	19279.689741	29.385127
360.240810	19292.142326	29.390144
360.486604	19332.571195	29.395162
360.919677	19356.459850	29.400180
361.320789	19376.098011	29.405197
361.671692	19386.252451	29.410215
361.909019	19415.570529	29.415232
361.891030	19456.448367	29.420250
362.358487	19472.940556	29.425268
362.540473	19516.673170	29.430285
362.773686	19550.470261	29.435303
363.548992	19557.544075	29.440320
363.352436	19589.468736	29.445338
363.903915	19634.300739	29.450356
364.088272	19661.991857	29.455373
364.411768	19704.103269	29.460391
365.089148	19739.361069	29.465408
365.022647	19766.903076	29.470426
365.509939	19798.373120	29.475444
365.957116	19842.575072	29.480461
366.509824	19892.262483	29.485479
367.283599	19905.515699	29.490496
367.438206	19939.816793	29.495514
367.400006	19958.479994	29.500532
368.016331	19988.729535	29.505549
368.302919	20025.475888	29.510567
368.930113	20046.764126	29.515584
369.071038	20066.360970	29.520602
369.718753	20088.329982	29.525620
369.878468	20123.037295	29.530637
370.052897	20150.138182	29.535655
370.445033	20177.505798	29.540672
371.045938	20214.214832	29.545690
371.294102	20230.966264	29.550708
371.779014	20244.998880	29.555725
372.042636	20295.162435	29.560743
372.158956	20315.487166	29.565760
372.193642	20359.566329	29.570778
372.756157	20392.831539	29.575796
373.691379	20416.135927	29.580813
374.024516	20457.401176	29.585831
374.406581	20473.383554	29.590848
374.980340	20504.631005	29.595866
375.233071	20534.746144	29.600884
375.717981	20542.733767	29.605901
375.720617	20579.342247	29.610919
376.471233	20612.266286	29.615936
376.529371	20660.404610	29.620954
376.897200	20671.944232	29.625972
377.527765	20710.686109	29.630989
377.443066	20734.985441	29.636007
378.087728	20750.934166	29.641024
378.437413	20796.355950	29.646042
378.495464	20853.249954	29.651060
379.229998	20891.082854	29.656077
379.192169	20910.617218	29.661095
379.667293	20946.382336	29.666112
380.103702	20991.476628	29.671130
380.402334	21031.402774	29.676148
381.290015	21060.553271	29.681165
381.470762	21089.276746	29.686183
382.359064	21117.656388	29.691200
382.301240	21146.411490	29.696218
382.835632	21162.474988	29.701236
382.902304	21222.434916	29.706253
383.118585	21278.263807	29.711271
383.644398	21288.652207	29.716288
384.027590	21307.431749	29.721306
384.623907	21345.424088	29.726324
384.756085	21399.050842	29.731341
385.074281	21447.663968	29.736359
385.806054	21454.285483	29.741376
385.943746	21486.945201	29.746394
386.269938	21552.024661	29.751412
386.885440	21575.651493	29.756429
386.687112	21632.093928	29.761447
387.619691	21670.064565	29.766464
387.897900	21693.859210	29.771482
388.127258	21733.079622	29.776500
388.616367	21771.483178	29.781517
389.051325	21822.647726	29.786535
389.439705	21838.537364	29.791552
389.234450	21885.035922	29.796570
389.820024	21934.706669	29.801588
390.688006	21961.533559	29.806605
390.684409	22007.909286	29.811623
391.296752	22057.103033	29.816640
391.414697	22088.558030	29.821658
392.150503	22129.027837	29.826676
392.679223	22159.324182	29.831693
392.972953	22204.798458	29.836711
393.668835	22234.242819	29.841728
393.932669	22260.356519	29.846746
394.556791	22306.091793	29.851764
395.029107	22308.980789	29.856781
395.294672	22342.693079	29.861799
395.475270	22366.400758	29.866816
396.088762	22388.495132	29.871834
396.341695	22432.887399	29.876852
396.792871	22459.992045	29.881869
396.954643	22485.084031	29.886887
397.034511	22532.727558	29.891904
397.693901	22559.372308	29.896922
397.883204	22606.296412	29.901940
398.140407	22633.527974	29.906957
398.484757	22663.792629	29.911975
399.083252	22723.796209	29.916992
399.196933	22778.486721	29.922010
399.925164	22807.975624	29.927028
400.172095	22836.565045	29.932045
400.234991	22885.978117	29.937063
400.675396	22941.714050	29.942080
401.168448	22990.331153	29.947098
401.221591	23027.538898	29.952116
401.770058	23059.894189	29.957133
402.276075	23107.394852	29.962151
403.002293	23163.267190	29.967168
403.776225	23202.256037	29.972186
403.878615	23233.824536	29.977204
404.393475	23272.727063	29.982221
404.610148	23330.886633	29.987239
405.306472	23358.302241	29.992256
405.702736	23403.340300	29.997274
405.975357	23447.307890	30.002292
406.512913	23475.943412	30.007309
406.748432	23538.604968	30.012327
407.135043	23578.476936	30.017344
407.559156	23614.539983	30.022362
407.972467	23661.701209	30.027380
408.400471	23685.644215	30.032397
408.781199	23746.731153	30.037415
409.378229	23765.265287	30.042432
409.754549	23792.795956	30.047450
409.870248	23849.395777	30.052468
410.707398	23906.977116	30.057485
410.954041	23936.348898	30.062503
411.526257	23962.633460	30.067520
411.970971	24021.311150	30.072538
412.128893	24050.984741	30.077556
413.080690	24094.395632	30.082573
413.036064	24154.398611	30.087591
413.629221	24174.195178	30.092608
413.957108	24196.723826	30.097626
414.293047	24246.013797	30.102644
414.878651	24296.423113	30.107661
415.305827	24348.315615	30.112679
415.597206	24369.638047	30.117696
415.974022	24391.329531	30.122714
416.416687	24451.057559	30.127732
416.816767	24505.848272	30.132749
417.281946	24544.880199	30.137767
417.228492	24581.372656	30.142784
418.176173	24616.376949	30.147802
418.583143	24675.425793	30.152820
419.170730	24720.938743	30.157837
419.524890	24746.951511	30.162855
419.932188	24778.202911	30.167872
420.489342	24827.358701	30.172890
420.879777	24873.784450	30.177908
421.533746	24889.153780	30.182925
422.113186	24903.592540	30.187943
422.372405	24951.463980	30.192960
423.019904	24960.196326	30.197978
423.091134	25008.978808	30.202996
423.477180	25023.101155	30.208013
424.244686	25042.117829	30.213031
424.469773	25075.279375	30.218048
424.761141	25107.343645	30.223066
424.975232	25135.450441	30.228084
425.425653	25161.908363	30.233101
425.632368	25213.647572	30.238119
426.000919	25236.880440	30.243136
426.113470	25268.569322	30.248154
426.253911	25323.952716	30.253172
426.765369	25386.009475	30.258189
426.912975	25412.651836	30.263207
427.383468	25469.548517	30.268224
427.856838	25515.861411	30.273242
428.185250	25584.907565	30.278260
428.758058	25649.995242	30.283277
429.618776	25694.060749	30.288295
429.734698	25719.209270	30.293312
430.602275	25772.692206	30.298330
430.594557	25831.868768	30.303348
431.297507	25864.749508	30.308365
431.658806	25930.451897	30.313383
432.252329	25975.830053	30.318400
432.990591	25991.788819	30.323418
433.430719	26053.041414	30.328436
434.067344	26102.752288	30.333453
434.203884	26137.868492	30.338471
434.838796	26178.681651	30.343488
435.780015	26211.178372	30.348506
436.133270	26252.673711	30.353524
436.675040	26271.566642	30.358541
437.275482	26310.163997	30.363559
437.254360	26345.573166	30.368576
438.180421	26377.263769	30.373594
438.165873	26403.511864	30.378612
439.060059	26435.753445	30.383629
439.403769	26482.618649	30.388647
439.682154	26502.457327	30.393664
441.004936	26517.593088	30.398682
441.493252	26569.431827	30.403700
441.747551	26584.245845	30.408717
442.039145	26604.517685	30.413735
442.352904	26630.177328	30.418752
442.817712	26660.463938	30.423770
443.132163	26682.201773	30.428788
443.091514	26735.539729	30.433805
443.780704	26749.585057	30.438823
443.945747	26786.568114	30.443840
444.597703	26827.968207	30.448858
444.690859	26872.775408	30.453876
445.038649	26906.292411	30.458893
445.085508	26931.171859	30.463911
445.626190	26982.903858	30.468928
446.256888	27029.691621	30.473946
446.175578	27078.038453	30.478964
446.769776	27135.732398	30.483981
447.159537	27186.477539	30.488999
447.582538	27214.969578	30.494016
448.002188	27259.241310	30.499034
448.290239	27332.014959	30.504052
449.127013	27392.237008	30.509069
449.638906	27444.646951	30.514087
449.802709	27485.914805	30.519104
450.483318	27520.193337	30.524122
450.807438	27562.283313	30.529140
451.386821	27602.044584	30.534157
452.014914	27653.773635	30.539175
452.168731	27702.827735	30.544192
453.084811	27730.286675	30.549210
452.981814	27771.879995	30.554228
453.290013	27826.759660	30.559245
454.079808	27861.733652	30.564263
454.246722	27903.087155	30.569280
454.848018	27939.533842	30.574298
455.058929	28008.781106	30.579316
455.740729	28052.629945	30.584333
456.255284	28086.665791	30.589351
456.593626	28139.967592	30.594368
457.031985	28195.700620	30.599386
457.681824	28247.418409	30.604404
458.120680	28282.918039	30.609421
458.705233	28329.262784	30.614439
459.198019	28380.164765	30.619456
459.599329	28427.675532	30.624474
459.860702	28471.746288	30.629492
460.877887	28516.029807	30.634509
461.333103	28565.727346	30.639527
461.571035	28620.403515	30.644544
462.079020	28640.304527	30.649562
462.250169	28697.297678	30.654580
462.598428	28748.533733	30.659597
463.301878	28788.059621	30.664615
463.951207	28838.993877	30.669632
464.438898	28881.668832	30.674650
464.967843	28928.447045	30.679668
465.572003	28985.694511	30.684685
466.231310	29021.045699	30.689703
466.560531	29046.032974	30.694720
467.121895	29102.004115	30.699738
467.696603	29154.692786	30.704756
467.836647	29185.509071	30.709773
468.597877	29226.496317	30.714791
468.711819	29280.570512	30.719808
469.474734	29299.524895	30.724826
470.025093	29345.190389	30.729844
470.333545	29399.901542	30.734861
470.673389	29443.949206	30.739879
470.459919	29493.337194	30.744896
471.318173	29520.717081	30.749914
471.754946	29591.059496	30.754932
472.065520	29648.471213	30.759949
472.593480	29687.835738	30.764967
472.732153	29746.774503	30.769984
473.847840	29791.931419	30.775002
474.494328	29857.300500	30.780020
475.393303	29899.689230	30.785037
475.799941	29924.497806	30.790055
475.727997	29959.757206	30.795072
476.187837	29997.244189	30.800090
476.605503	30071.638847	30.805108
477.248068	30108.464999	30.810125
477.966671	30140.468127	30.815143
478.643943	30182.862628	30.820160
479.525270	30239.566911	30.825178
479.812064	30269.616432	30.830196
480.064199	30310.646182	30.835213
480.542019	30346.629417	30.840231
480.259486	30390.100922	30.845248
481.012044	30450.549476	30.850266
481.128402	30485.804077	30.855284
481.606397	30554.276121	30.860301
482.280535	30603.839265	30.865319
482.729891	30650.692068	30.870336
483.108082	30678.373908	30.875354
483.357202	30750.979142	30.880372
483.558716	30797.630378	30.885389
484.498763	30837.932605	30.890407
484.916929	30914.160449	30.895424
485.249821	30952.178356	30.900442
485.659954	30986.745064	30.905460
486.234743	31049.480613	30.910477
486.606767	31120.067058	30.915495
487.070552	31171.915822	30.920512
487.675631	31209.053351	30.925530
488.007006	31271.104336	30.930548
488.485883	31300.890468	30.935565
489.465382	31350.954217	30.940583
489.605605	31433.132640	30.945600
490.072629	31486.956643	30.950618
490.756303	31535.706957	30.955636
490.643911	31602.211155	30.960653
491.367148	31656.681091	30.965671
491.937372	31719.656412	30.970688
492.111618	31776.649708	30.975706
493.065235	31838.804992	30.980724
493.518920	31897.200561	30.985741
494.495831	31929.186406	30.990759
494.688466	31995.386180	30.995776
495.309246	32047.760551	31.000794
495.596184	32117.096854	31.005812
496.294174	32174.708462	31.010829
496.797919	32217.978928	31.015847
497.531174	32284.633131	31.020864
497.864993	32347.488868	31.025882
498.586432	32388.758326	31.030900
498.834639	32443.138816	31.035917
499.516893	32497.614991	31.040935
499.959209	32542.590579	31.045952
500.599399	32602.494128	31.050970
501.100001	32660.931821	31.055988
501.478778	32704.410273	31.061005
502.104457	32732.149144	31.066023
502.790913	32811.754586	31.071040
503.297424	32868.441005	31.076058
503.863829	32919.057041	31.081076
504.032208	32967.227613	31.086093
504.610685	33004.830830	31.091111
505.176548	33075.128134	31.096128
505.400870	33139.033320	31.101146
506.017045	33180.877313	31.106164
506.290636	33221.900898	31.111181
507.068062	33279.534571	31.116199
507.408833	33348.507180	31.121216
508.485746	33390.953904	31.126234
509.224130	33438.258634	31.131252
509.235497	33501.613473	31.136269
509.348388	33554.461156	31.141287
509.712580	33611.921234	31.146304
510.228728	33659.793321	31.151322
511.028338	33725.545995	31.156340
511.450974	33786.171021	31.161357
512.326144	33821.811829	31.166375
512.655378	33892.624755	31.171392
513.019508	33939.166004	31.176410
513.984985	33984.345991	31.181428
514.570454	34028.187973	31.186445
515.438257	34074.535957	31.191463
515.775173	34142.029383	31.196480
516.306072	34182.280706	31.201498
517.002698	34216.377369	31.206516
517.696414	34255.844722	31.211533
518.503401	34271.014180	31.216551
519.059341	34307.052617	31.221568
519.461749	34344.993839	31.226586
519.819412	34377.070671	31.231604
520.078153	34424.015544	31.236621
520.685195	34465.564357	31.241639
520.763077	34501.325612	31.246656
521.095986	34530.649131	31.251674
521.508815	34593.872166	31.256692
521.796939	34654.143763	31.261709
521.990632	34687.163268	31.266727
522.439974	34729.742127	31.271744
522.705431	34813.654235	31.276762
523.290390	34887.079359	31.281780
523.405376	34955.306715	31.286797
524.138154	35009.296406	31.291815
524.555883	35072.779079	31.296832
525.287013	35149.405906	31.301850
525.819738	35228.167312	31.306868
526.104069	35280.616351	31.311885
526.889301	35359.172553	31.316903
527.463689	35430.743149	31.321920
527.820634	35489.024622	31.326938
528.507182	35548.056480	31.331956
528.961261	35648.362228	31.336973
529.660748	35700.261152	31.341991
530.589031	35753.851632	31.347008
531.200775	35828.446905	31.352026
532.013696	35895.451869	31.357044
532.286002	35950.479750	31.362061
532.823473	36010.263532	31.367079
533.115146	36081.810870	31.372096
533.791351	36138.972021	31.377114
534.040701	36198.425360	31.382132
534.259615	36291.051964	31.387149
534.886372	36356.186609	31.392167
535.412698	36412.896904	31.397184
535.903318	36476.568197	31.402202
536.309614	36557.745157	31.407220
536.881685	36654.455471	31.412237
537.627255	36724.475675	31.417255
538.249157	36780.208883	31.422272
538.639302	36860.938631	31.427290
539.439782	36944.295914	31.432308
540.005186	37028.913665	31.437325
540.379095	37072.406811	31.442343
541.072569	37128.220798	31.447360
541.477110	37226.940509	31.452378
542.621443	37284.409854	31.457396
543.237453	37346.223744	31.462413
544.379123	37402.153905	31.467431
545.029114	37457.717333	31.472448
545.641648	37511.390500	31.477466
546.072286	37570.749035	31.482484
546.330552	37616.727272	31.487501
546.902598	37658.879464	31.492519
547.788350	37726.728187	31.497536
547.871366	37792.292392	31.502554
548.493224	37831.375616	31.507572
548.677655	37883.277601	31.512589
549.116246	37941.146492	31.517607
550.199960	38009.840916	31.522624
550.588994	38085.110415	31.527642
551.625246	38114.980092	31.532660
551.694827	38165.746811	31.537677
552.265818	38237.815229	31.542695
553.046368	38304.014041	31.547712
553.338566	38351.658033	31.552730
553.906736	38390.612482	31.557748
553.954814	38445.833401	31.562765
554.607109	38502.283347	31.567783
555.106027	38570.738820	31.572800
555.234677	38639.886903	31.577818
555.769031	38690.294299	31.582836
556.204367	38760.799759	31.587853
556.689644	38826.118243	31.592871
557.444431	38904.057544	31.597888
557.238170	38979.454351	31.602906
558.499760	39049.142767	31.607924
559.076550	39112.304220	31.612941
559.511853	39188.627966	31.617959
559.833056	39263.146665	31.622976
560.451032	39339.829076	31.627994
560.707716	39412.856748	31.633012
561.398833	39496.995095	31.638029
561.849697	39569.571564	31.643047
562.990593	39632.793161	31.648064
563.705142	39709.095075	31.653082
565.053804	39777.515775	31.658100
565.657700	39842.319667	31.663117
566.105048	39883.481376	31.668135
566.781509	39943.993857	31.673152
567.149804	40022.784557	31.678170
567.558095	40065.591205	31.683188
568.032063	40148.581708	31.688205
568.768988	40216.268703	31.693223
569.655124	40272.060624	31.698240
569.923295	40355.840410	31.703258
570.577966	40392.651256	31.708276
571.239970	40453.199388	31.713293
571.990275	40519.019937	31.718311
572.554978	40596.578139	31.723328
572.908562	40657.881750	31.728346
573.326060	40711.217897	31.733364
573.926706	40797.779194	31.738381
574.337288	40858.401765	31.743399
575.196325	40908.786968	31.748416
575.870190	40986.559218	31.753434
576.466576	41050.181865	31.758452
576.872407	41112.576803	31.763469
577.334766	41187.948104	31.768487
578.069574	41237.972811	31.773504
578.185533	41319.673683	31.778522
579.317764	41373.509229	31.783540
579.591831	41436.236369	31.788557
580.187504	41537.084976	31.793575
581.339329	41607.609426	31.798592
581.861856	41656.095255	31.803610
582.382320	41691.245329	31.808628
582.768038	41780.943322	31.813645
583.124455	41855.416330	31.818663
583.856920	41909.512035	31.823680
584.564128	41980.142924	31.828698
585.382634	42041.993086	31.833716
585.428719	42103.775323	31.838733
585.514893	42174.989334	31.843751
586.334602	42253.566763	31.848768
586.622649	42324.864809	31.853786
587.248858	42416.896812	31.858804
587.970168	42501.192424	31.863821
588.508193	42559.160640	31.868839
589.231381	42654.527026	31.873856
589.702982	42725.865761	31.878874
590.614573	42778.918000	31.883892
591.211736	42860.154839	31.888909
591.844718	42944.031449	31.893927
592.655366	42999.143394	31.898944
593.036157	43058.783811	31.903962
593.429379	43122.611373	31.908980
593.730783	43189.999361	31.913997
594.409083	43242.955732	31.919015
594.987104	43321.726022	31.924032
595.418257	43417.450807	31.929050
596.101396	43487.864187	31.934068
596.862752	43541.603217	31.939085
597.206088	43617.086243	31.944103
598.077477	43705.700082	31.949120
598.478928	43789.691393	31.954138
598.755673	43848.098276	31.959156
599.439080	43940.829283	31.964173
600.176445	44012.239601	31.969191
600.725025	44090.730761	31.974208
601.152955	44173.459835	31.979226
602.031924	44236.876394	31.984244
602.652899	44325.907087	31.989261
603.240349	44409.305400	31.994279
604.445336	44480.753949	31.999296
605.271872	44570.405363	32.004314
605.604906	44648.899764	32.009332
606.328773	44692.684822	32.014349
606.869291	44758.646799	32.019367
607.344801	44849.247820	32.024384
607.946532	44928.942904	32.029402
608.575411	45005.075830	32.034420
609.170161	45082.086059	32.039437
609.628793	45154.945409	32.044455
610.089776	45226.484986	32.049472
610.809277	45314.168698	32.054490
611.480927	45397.939564	32.059508
611.982319	45464.216752	32.064525
612.500731	45556.509525	32.069543
613.422582	45624.757371	32.074560
614.334985	45710.845137	32.079578
615.263772	45785.226846	32.084596
616.429841	45830.728536	32.089613
616.817038	45908.736260	32.094631
617.634946	45971.114326	32.099648
618.134518	46034.744929	32.104666
618.578746	46082.627039	32.109684
619.014503	46151.980051	32.114701
619.639713	46239.819459	32.119719
620.298002	46307.279816	32.124736
620.771825	46363.092029	32.129754
621.322870	46443.401858	32.134772
622.162148	46529.076087	32.139789
622.722104	46612.040481	32.144807
623.031977	46666.851385	32.149824
623.596562	46738.809057	32.154842
624.130441	46824.039370	32.159860
624.543131	46899.906322	32.164877
625.233300	46977.296982	32.169895
626.013706	47045.399732	32.174912
626.449485	47144.013042	32.179930
626.742339	47226.222283	32.184948
627.404497	47304.177787	32.189965
627.582764	47398.038783	32.194983
628.341630	47499.117105	32.200000
629.092435	47574.040530	32.205018
630.109016	47653.846084	32.210036
630.715471	47743.151256	32.215053
631.217829	47829.490163	32.220071
632.149316	47913.368321	32.225088
632.644630	47993.119316	32.230106
633.038588	48054.074496	32.235124
633.927387	48138.210156	32.240141
634.551049	48233.927897	32.245159
635.150997	48295.705553	32.250176
635.826909	48361.992598	32.255194
635.887107	48442.246793	32.260212
636.811668	48541.620324	32.265229
637.084890	48622.108503	32.270247
637.890118	48697.788413	32.275264
638.170379	48789.201756	32.280282
638.636894	48888.153840	32.285300
639.350319	48968.144499	32.290317
639.726318	49081.922334	32.295335
640.338885	49178.019306	32.300352
641.208901	49271.652226	32.305370
641.855824	49355.839574	32.310388
642.729760	49469.610132	32.315405
643.100381	49571.723655	32.320423
644.529057	49646.603359	32.325440
644.915010	49728.691283	32.330458
645.501216	49825.585358	32.335476
646.521737	49925.651358	32.340493
646.968011	50013.897924	32.345511
647.610758	50085.741776	32.350528
648.306432	50181.018518	32.355546
648.881922	50279.776703	32.360564
649.670720	50383.325552	32.365581
650.213551	50470.648793	32.370599
651.194303	50549.622995	32.375616
651.746632	50643.034081	32.380634
652.204694	50755.662024	32.385652
653.162152	50840.366793	32.390669
653.933988	50914.797843	32.395687
654.533935	50995.564242	32.400704
655.193072	51106.111455	32.405722
656.188459	51206.298869	32.410740
656.861218	51260.715766	32.415757
657.661593	51362.938453	32.420775
658.301824	51448.099391	32.425792
658.866630	51529.363362	32.430810
659.594717	51609.514299	32.435828
660.099644	51675.162139	32.440845
660.884020	51774.146209	32.445863
661.315122	51871.215247	32.450880
661.730851	51952.717233	32.455898
662.435206	52034.623527	32.460916
663.446770	52130.843196	32.465933
663.679330	52208.093916	32.470951
664.470605	52298.893313	32.475968
665.336957	52402.607676	32.480986
665.787072	52483.045042	32.486004
666.769826	52567.775385	32.491021
666.991763	52672.485117	32.496039
667.772215	52758.598326	32.501056
668.530980	52840.312724	32.506074
669.209850	52935.132191	32.511092
669.821234	53030.490725	32.516109
670.067166	53147.472646	32.521127
670.970729	53219.168321	32.526144
671.537372	53330.988037	32.531162
671.940786	53426.237581	32.536180
672.596848	53509.898444	32.541197
673.467213	53615.122106	32.546215
674.189159	53733.794564	32.551232
674.876895	53826.737623	32.556250
675.143897	53913.250312	32.561268
675.948837	54008.227944	32.566285
676.258677	54129.478785	32.571303
677.104505	54219.933924	32.576320
678.306426	54308.100694	32.581338
678.519524	54380.492728	32.586356
679.810273	54477.717180	32.591373
680.643133	54575.213575	32.596391
681.382640	54654.058118	32.601408
682.283479	54719.426664	32.606426
682.904396	54815.619986	32.611444
683.416240	54908.976318	32.616461
684.153828	54999.225535	32.621479
684.631048	55070.673121	32.626496
685.486039	55158.831556	32.631514
685.858630	55258.138381	32.636532
686.600215	55326.675085	32.641549
687.011864	55439.104276	32.646567
687.665918	55531.347159	32.651584
688.571831	55617.073287	32.656602
689.641858	55698.078651	32.661620
690.330925	55803.988506	32.666637
690.986916	55899.555926	32.671655
691.409881	55992.780494	32.676672
692.029099	56081.051525	32.681690
692.480138	56182.769809	32.686708
693.363738	56280.114717	32.691725
694.241060	56375.142476	32.696743
694.729937	56490.401688	32.701760
695.428401	56575.553434	32.706778
695.849143	56692.960558	32.711796
697.102475	56770.800045	32.716813
697.260570	56879.387467	32.721831
698.054522	56996.153507	32.726848
698.712512	57089.546649	32.731866
699.078388	57201.001552	32.736884
700.232663	57314.272893	32.741901
701.273778	57405.456075	32.746919
701.537960	57505.600911	32.751936
702.671208	57617.487451	32.756954
703.453269	57735.839412	32.761972
704.237778	57818.334942	32.766989
705.062299	57906.119020	32.772007
705.201350	58021.824064	32.777024
706.251275	58125.784983	32.782042
706.792388	58218.754160	32.787060
707.705699	58308.484093	32.792077
708.714223	58420.490555	32.797095
709.043277	58528.268989	32.802112
709.818142	58630.060156	32.807130
710.427204	58724.397943	32.812148
711.282731	58806.209768	32.817165
711.971446	58911.049568	32.822183
712.497735	59037.710103	32.827200
713.475044	59130.990646	32.832218
713.779098	59228.193051	32.837236
714.495596	59342.148582	32.842253
715.305732	59461.574093	32.847271
716.264547	59552.509042	32.852288
716.631726	59638.866093	32.857306
717.397778	59751.672055	32.862324
717.853596	59867.392399	32.867341
718.603040	59965.535888	32.872359
719.632616	60087.993648	32.877376
720.549177	60167.639864	32.882394
721.338652	60271.225317	32.887412
722.160457	60381.346312	32.892429
723.340532	60465.714859	32.897447
723.518091	60571.267081	32.902464
724.591987	60675.420623	32.907482
725.352491	60771.417690	32.912500
725.809302	60857.354445	32.917517
726.538103	60947.000348	32.922535
726.963961	61040.324004	32.927552
727.643564	61125.966023	32.932570
728.202826	61222.276533	32.937588
729.188926	61319.831468	32.942605
729.967107	61418.520805	32.947623
730.504828	61516.283446	32.952640
731.743863	61597.493573	32.957658
732.423443	61708.321530	32.962676
732.946572	61791.249519	32.967693
733.542485	61884.378377	32.972711
734.154613	61986.061832	32.977728
734.806532	62089.698338	32.982746
735.386545	62184.689203	32.987764
736.039529	62300.801790	32.992781
736.868572	62418.320568	32.997799
737.746236	62516.739739	33.002816
738.163843	62606.457055	33.007834
738.247117	62729.618044	33.012852
739.516969	62863.112872	33.017869
740.135396	62969.691875	33.022887
740.559461	63083.716918	33.027904
741.395275	63208.936952	33.032922
742.570278	63337.059552	33.037940
743.317632	63436.319999	33.042957
744.194406	63566.067005	33.047975
744.806115	63679.975924	33.052992
745.865773	63783.212464	33.058010
746.154256	63913.400124	33.063028
747.007371	64040.297292	33.068045
747.850322	64148.520279	33.073063
748.948812	64250.558229	33.078080
749.942070	64367.877875	33.083098
750.494547	64471.719930	33.088116
751.561331	64603.104437	33.093133
752.234225	64712.843813	33.098151
752.832387	64807.806013	33.103168
753.965482	64923.873250	33.108186
754.154917	65041.746659	33.113204
754.851900	65151.971098	33.118221
755.768249	65264.745069	33.123239
756.080499	65375.761122	33.128256
757.189386	65497.821338	33.133274
757.584636	65647.584138	33.138292
758.162100	65743.217769	33.143309
759.114424	65872.246349	33.148327
759.485039	65994.696904	33.153344
760.791233	66107.328949	33.158362
761.398944	66246.606162	33.163380
762.065798	66375.489082	33.168397
763.374856	66490.537385	33.173415
763.819862	66611.190449	33.178432
764.682338	66725.182326	33.183450
765.466876	66859.813717	33.188468
766.003970	66967.052742	33.193485
767.385916	67090.777705	33.198503
767.840551	67208.063429	33.203520
768.341388	67330.083181	33.208538
769.143128	67481.410404	33.213556
769.954771	67592.773113	33.218573
771.028145	67694.863897	33.223591
771.742971	67817.066103	33.228608
772.780533	67934.386097	33.233626
773.571871	68072.545314	33.238644
774.228975	68181.559791	33.243661
775.441066	68278.048571	33.248679
775.780252	68389.613673	33.253696
776.749866	68507.023973	33.258714
777.428028	68610.240230	33.263732
778.346588	68703.555375	33.268749
779.588124	68784.926354	33.273767
780.377480	68906.939309	33.278784
780.929448	69002.611141	33.283802
781.933482	69103.449587	33.288820
782.347531	69215.563058	33.293837
783.488246	69294.657821	33.298855
783.893831	69406.798999	33.303872
784.509025	69503.202346	33.308890
785.239206	69618.085371	33.313908
785.757389	69740.647397	33.318925
786.416321	69836.893323	33.323943
786.846254	69952.169146	33.328960
787.937181	70074.101159	33.333978
788.682898	70190.919329	33.338996
789.316186	70332.122589	33.344013
790.082585	70429.940362	33.349031
791.069810	70566.743354	33.354048
791.965542	70694.451843	33.359066
792.596958	70802.662278	33.364084
793.140662	70921.490431	33.369101
794.142423	71043.664058	33.374119
794.893785	71180.307651	33.379136
795.275438	71301.712660	33.384154
796.419727	71437.003231	33.389172
797.158741	71589.653919	33.394189
797.810275	71701.349382	33.399207
798.501304	71817.553302	33.404224
799.198549	71961.159483	33.409242
800.005356	72111.475964	33.414260
801.271761	72247.472328	33.419277
802.287792	72378.522181	33.424295
803.004974	72499.151495	33.429312
804.008145	72618.811122	33.434330
804.938578	72757.610366	33.439348
805.849052	72891.285858	33.444365
806.654543	72999.952961	33.449383
807.590260	73137.976071	33.454400
808.361358	73262.913129	33.459418
809.140472	73388.677924	33.464436
809.672634	73512.125688	33.469453
810.675467	73634.927354	33.474471
811.110981	73781.402819	33.479488
812.153288	73892.754347	33.484506
813.133067	74015.454501	33.489524
814.043566	74146.127911	33.494541
815.241986	74272.296572	33.499559
815.992842	74407.474900	33.504576
816.834977	74509.851774	33.509594
817.634537	74643.765169	33.514612
818.278777	74765.374123	33.519629
818.981463	74894.960797	33.524647
820.197841	75029.199819	33.529664
820.474489	75154.052441	33.534682
821.498884	75263.346173	33.539700
822.104796	75383.181648	33.544717
823.257800	75515.827928	33.549735
823.734875	75654.625865	33.554752
824.737577	75790.738797	33.559770
825.617672	75889.144556	33.564788
825.937429	76022.981288	33.569805
827.137440	76160.493160	33.574823
827.615304	76311.405535	33.579840
828.485478	76449.523885	33.584858
829.365356	76577.270023	33.589876
829.949123	76695.649204	33.594893
830.834245	76830.352479	33.599911
831.477920	76966.196862	33.604928
832.334446	77074.920298	33.609946
833.399150	77187.942012	33.614964
833.686713	77332.163861	33.619981
834.979230	77474.981150	33.624999
835.965998	77597.890138	33.630016
836.735659	77719.311482	33.635034
837.387706	77839.469057	33.640052
837.925352	77985.513290	33.645069
839.104838	78132.818610	33.650087
839.507694	78250.951462	33.655104
840.313812	78382.805973	33.660122
841.434360	78534.424437	33.665140
841.950353	78688.964577	33.670157
842.669624	78816.977969	33.675175
843.604413	78959.642604	33.680192
844.382466	79104.756440	33.685210
845.224272	79235.256643	33.690228
846.344647	79398.563049	33.695245
847.355315	79540.453590	33.700263
848.077458	79670.881244	33.705280
849.003654	79817.493279	33.710298
850.465136	79964.530225	33.715316
850.899268	80108.980041	33.720333
851.262374	80238.717626	33.725351
852.451979	80402.557622	33.730368
852.951930	80550.566830	33.735386
853.910925	80680.834794	33.740404
854.451187	80849.915073	33.745421
855.733271	80980.795596	33.750439
856.643719	81152.302895	33.755456
857.225260	81315.699686	33.760474
858.488587	81458.863767	33.765492
859.146943	81613.489272	33.770509
859.999069	81757.146963	33.775527
861.061819	81901.934706	33.780544
861.779430	82065.276534	33.785562
862.708092	82210.847483	33.790580
863.654925	82354.676801	33.795597
864.533824	82513.535617	33.800615
865.516598	82678.027351	33.805632
866.252515	82825.677334	33.810650
867.674731	82954.003230	33.815668
868.446594	83126.952819	33.820685
869.118176	83259.048128	33.825703
870.300603	83407.564430	33.830720
871.465510	83559.899211	33.835738
872.620511	83686.103545	33.840756
873.285291	83819.247047	33.845773
874.476833	83950.798727	33.850791
875.281340	84109.896119	33.855808
875.956008	84251.138071	33.860826
877.177751	84363.385768	33.865844
877.686602	84514.386554	33.870861
878.602271	84654.015955	33.875879
879.555848	84784.580547	33.880896
879.909039	84923.380814	33.885914
880.900205	85076.918500	33.890932
881.652408	85222.114033	33.895949
882.648870	85360.760128	33.900967
883.444032	85527.682240	33.905984
884.317083	85690.461404	33.911002
885.114583	85805.810373	33.916020
885.576419	85944.813990	33.921037
886.784969	86099.271636	33.926055
887.952976	86264.726673	33.931072
888.551876	86417.724395	33.936090
889.794340	86534.768740	33.941108
890.148042	86663.867676	33.946125
891.556979	86806.250531	33.951143
892.463708	86932.652954	33.956160
892.882841	87080.661119	33.961178
893.675097	87235.258376	33.966196
894.673466	87372.581252	33.971213
895.337266	87500.962983	33.976231
896.172227	87637.801912	33.981248
896.975082	87800.392416	33.986266
897.803639	87973.856393	33.991284
898.586147	88130.131616	33.996301
899.347324	88264.917385	34.001319
900.326280	88416.017954	34.006336
901.173441	88590.154150	34.011354
902.417711	88745.465087	34.016372
903.380692	88899.659235	34.021389
904.363299	89044.948276	34.026407
905.192563	89205.715547	34.031424
906.127465	89375.894679	34.036442
907.237666	89522.336229	34.041460
907.639751	89677.988560	34.046477
908.787710	89834.031321	34.051495
909.843244	90011.756834	34.056512
910.195956	90173.033370	34.061530
911.195131	90351.916097	34.066548
911.801674	90520.398560	34.071565
912.171538	90681.485897	34.076583
913.012805	90853.450348	34.081600
914.272326	91059.170679	34.086618
915.346452	91234.738111	34.091636
915.977699	91411.310210	34.096653
917.026288	91581.701631	34.101671
918.264273	91768.206472	34.106688
919.036698	91962.358340	34.111706
920.361700	92131.898036	34.116724
921.078445	92287.730727	34.121741
921.896278	92466.931458	34.126759
923.412490	92659.485329	34.131776
924.128137	92840.072690	34.136794
925.203321	92991.724557	34.141812
925.979365	93166.678267	34.146829
927.222342	93346.055871	34.151847
928.435849	93515.636439	34.156864
929.135306	93700.289675	34.161882
930.557529	93864.756216	34.166900
931.669061	94020.199553	34.171917
932.300304	94170.622075	34.176935
933.476164	94343.961414	34.181952
934.196232	94528.022658	34.186970
935.316066	94671.089255	34.191988
936.257584	94843.401254	34.197005
937.065275	95017.439113	34.202023
938.231532	95184.399946	34.207040
938.937591	95341.184551	34.212058
940.146207	95514.799013	34.217076
941.165926	95678.894957	34.222093
942.102021	95830.486339	34.227111
943.022648	96004.721483	34.232128
943.865446	96179.135285	34.237146
945.046915	96302.624329	34.242164
946.053495	96468.417722	34.247181
947.044448	96642.677449	34.252199
947.856977	96794.580041	34.257216
948.568001	96957.051855	34.262234
949.964339	97122.411871	34.267252
950.427238	97295.636731	34.272269
951.333778	97452.686605	34.277287
952.311578	97609.440874	34.282304
953.092197	97755.904700	34.287322
953.705699	97895.225219	34.292340
954.484951	98057.230942	34.297357
955.161771	98236.972239	34.302375
956.000873	98398.191726	34.307392
956.753450	98569.390063	34.312410
957.550730	98736.632215	34.317428
958.498201	98927.709034	34.322445
959.291261	99097.834534	34.327463
960.255563	99290.987668	34.332480
961.293225	99484.997439	34.337498
962.449460	99646.932299	34.342516
963.604282	99832.493421	34.347533
964.622798	100024.624091	34.352551
965.738863	100196.349661	34.357568
967.976423	100341.682920	34.362586
969.206352	100501.800622	34.367604
970.181746	100667.032175	34.372621
971.016588	100832.598220	34.377639
971.896890	100991.143460	34.382656
972.868416	101154.732879	34.387674
973.820700	101328.898903	34.392692
974.300231	101487.551416	34.397709
975.014121	101660.151059	34.402727
976.077656	101829.705977	34.407744
976.869037	102011.019180	34.412762
977.991671	102190.240417	34.417780
978.888471	102373.533065	34.422797
979.832643	102549.956338	34.427815
980.829302	102750.063189	34.432832
981.480280	102928.297540	34.437850
982.406271	103098.643373	34.442868
983.321124	103291.803660	34.447885
983.874734	103496.275764	34.452903
984.906629	103674.287815	34.457920
985.869371	103885.457354	34.462938
986.718356	104073.486987	34.467956
988.034258	104284.031669	34.472973
988.707979	104484.591616	34.477991
989.986465	104681.982457	34.483008
990.919361	104890.670528	34.488026
992.064768	105077.062975	34.493044
993.053646	105275.151997	34.498061
994.019292	105499.156046	34.503079
995.050203	105698.805320	34.508096
995.957937	105910.412078	34.513114
996.778420	106091.559339	34.518132
998.793463	106271.358227	34.523149
1000.148173	106464.298681	34.528167
1001.457067	106669.621000	34.533184
1002.199284	106837.020434	34.538202
1002.779328	107022.241080	34.543220
1004.482783	107211.722776	34.548237
1005.170983	107397.042195	34.553255
1006.265327	107573.468651	34.558272
1007.744949	107756.760263	34.563290
1008.400122	107943.583419	34.568308
1009.671911	108130.230113	34.573325
1010.203528	108302.005034	34.578343
1011.215854	108488.481793	34.583360
1012.038189	108688.758218	34.588378
1013.153232	108866.279107	34.593396
1013.946218	109063.118271	34.598413
1014.798568	109259.936429	34.603431
1015.648577	109445.243503	34.608448
1016.744054	109647.964507	34.613466
1017.664875	109809.907110	34.618484
1019.090373	110002.051166	34.623501
1019.856333	110196.534676	34.628519
1020.835055	110379.293823	34.633536
1022.038706	110545.525940	34.638554
1022.939340	110740.510475	34.643572
1023.917081	110924.869432	34.648589
1024.820875	111116.208312	34.653607
1026.166446	111279.926292	34.658624
1027.044828	111446.154351	34.663642
1027.975209	111640.519844	34.668660
1028.877472	111840.629352	34.673677
1030.032712	112035.429228	34.678695
1031.554016	112204.583158	34.683712
1032.403340	112395.332088	34.688730
1032.909502	112588.583735	34.693748
1034.209882	112781.452298	34.698765
1034.865099	112990.528680	34.703783
1035.979259	113183.924856	34.708800
1036.563949	113374.838344	34.713818
1037.619669	113588.109408	34.718836
1038.709627	113801.857848	34.723853
1039.615691	114019.881968	34.728871
1040.338950	114213.273946	34.733888
1041.373900	114425.997576	34.738906
1042.235302	114654.168353	34.743924
1043.104372	114875.777716	34.748941
1044.417057	115105.613245	34.753959
1045.187017	115313.814274	34.758976
1046.584883	115535.493648	34.763994
1047.648419	115785.936648	34.769012
1048.990360	116005.336020	34.774029
1049.945426	116228.576245	34.779047
1051.295142	116443.442416	34.784064
1052.520788	116661.865329	34.789082
1053.375941	116900.494722	34.794100
1054.917412	117119.464511	34.799117
1055.424619	117325.620888	34.804135
1056.408272	117534.715399	34.809152
1058.043883	117757.956828	34.814170
1058.975833	117975.995031	34.819188
1060.500905	118195.533365	34.824205
1061.317553	118421.955935	34.829223
1062.465819	118643.840488	34.834240
1063.795294	118868.712283	34.839258
1064.514216	119068.473510	34.844276
1066.231689	119276.446171	34.849293
1066.767970	119511.412620	34.854311
1067.762547	119729.010508	34.859328
1068.963966	119922.388307	34.864346
1069.726385	120138.621236	34.869364
1071.279414	120368.003953	34.874381
1072.368194	120580.410532	34.879399
1073.354094	120797.587170	34.884416
1074.507023	121022.897854	34.889434
1075.284944	121230.444286	34.894452
1076.280381	121449.398182	34.899469
1077.078212	121688.203904	34.904487
1078.334715	121920.106114	34.909504
1079.521565	122128.959970	34.914522
1080.748360	122346.577310	34.919540
1081.893915	122584.598064	34.924557
1082.842795	122811.628969	34.929575
1083.992777	123017.631511	34.934592
1085.406025	123230.295396	34.939610
1086.405625	123445.538133	34.944628
1087.722865	123651.846995	34.949645
1088.507618	123865.354208	34.954663
1089.662969	124081.653016	34.959680
1090.629357	124297.312979	34.964698
1091.530608	124518.827197	34.969716
1092.832158	124721.559880	34.974733
1093.649277	124919.989248	34.979751
1094.614328	125138.037983	34.984768
1095.462040	125360.771225	34.989786
1096.233901	125573.114330	34.994804
1097.364329	125778.442371	34.999821
1098.133230	126019.100259	35.004839
1099.569385	126259.092321	35.009856
1100.669145	126468.751671	35.014874
1101.340202	126700.445941	35.019892
1102.698980	126934.398381	35.024909
1103.764114	127180.440863	35.029927
1104.885426	127406.730730	35.034944
1106.002414	127629.322311	35.039962
1107.406717	127858.116239	35.044980
1108.791441	128088.448656	35.049997
1109.555445	128342.243293	35.055015
1110.446168	128575.892799	35.060032
1111.700862	128800.485401	35.065050
1112.866029	129050.480853	35.070068
1113.774978	129289.988296	35.075085
1115.122931	129519.995389	35.080103
1116.275410	129770.493111	35.085120
1117.524506	130021.851472	35.090138
1119.087638	130254.198689	35.095156
1121.046158	130464.339529	35.100173
1122.493165	130693.933447	35.105191
1123.226347	130908.741136	35.110208
1124.477765	131126.519453	35.115226
1125.399728	131367.118249	35.120244
1126.518412	131603.668376	35.125261
1127.620708	131813.896320	35.130279
1128.753631	132025.451541	35.135296
1129.820113	132264.867262	35.140314
1130.545943	132517.663116	35.145332
1131.756803	132759.378414	35.150349
1132.896465	132985.237205	35.155367
1133.821592	133225.380741	35.160384
1135.207263	133471.673997	35.165402
1135.737677	133709.173698	35.170420
1137.193913	133953.887218	35.175437
1138.030396	134198.134494	35.180455
1138.961895	134425.470336	35.185472
1140.084338	134691.224046	35.190490
1141.182125	134950.557003	35.195508
1142.451696	135200.508304	35.200525
1143.511775	135462.463024	35.205543
1144.646850	135720.845291	35.210560
1145.703122	135946.244433	35.215578
1146.907417	136214.393183	35.220596
1147.945875	136489.429893	35.225613
1148.894362	136744.631136	35.230631
1150.389783	137000.124422	35.235648
1151.688720	137247.500520	35.240666
1152.781040	137515.019261	35.245684
1154.231750	137781.048451	35.250701
1155.805901	138022.578602	35.255719
1156.670834	138258.712720	35.260736
1158.206595	138521.310845	35.265754
1159.220343	138767.503046	35.270772
1160.562996	139006.682474	35.275789
1161.695959	139270.164446	35.280807
1163.077418	139511.306246	35.285824
1164.521977	139765.637654	35.290842
1165.037739	140009.410940	35.295860
1166.653317	140219.799110	35.300877
1168.093711	140446.002522	35.305895
1168.843147	140690.477568	35.310912
1170.547983	140914.979572	35.315930
1171.215585	141128.078383	35.320948
1172.337891	141343.905556	35.325965
1173.766109	141585.434952	35.330983
1174.555090	141814.645940	35.336000
1175.809414	142034.411652	35.341018
1177.217294	142258.274246	35.346036
1178.568246	142484.658248	35.351053
1179.690388	142711.170281	35.356071
1180.484026	142936.267203	35.361088
1181.605897	143176.451031	35.366106
1182.808116	143428.085846	35.371124
1183.839274	143664.141758	35.376141
1184.819806	143918.669739	35.381159
1185.542497	144152.307310	35.386176
1186.657885	144406.068499	35.391194
1187.891436	144677.932173	35.396212
1188.838301	144934.096257	35.401229
1189.939949	145196.602279	35.406247
1191.218143	145474.120301	35.411264
1192.277328	145713.381042	35.416282
1193.573879	145982.936613	35.421300
1194.500692	146269.864663	35.426317
1195.864109	146538.754055	35.431335
1196.753950	146821.228998	35.436352
1198.143889	147069.384516	35.441370
1199.033492	147356.416303	35.446388
1200.200426	147654.526184	35.451405
1201.797068	147921.967261	35.456423
1202.599097	148193.929319	35.461440
1204.277974	148480.357974	35.466458
1205.331603	148792.623414	35.471476
1206.297969	149076.802941	35.476493
1207.816470	149345.193301	35.481511
1209.034097	149637.464904	35.486528
1210.622440	149911.453406	35.491546
1211.582306	150197.836817	35.496564
1212.460306	150484.375496	35.501581
1214.008543	150787.495910	35.506599
1215.380345	151084.496910	35.511616
1216.948404	151352.576814	35.516634
1217.997842	151627.453448	35.521652
1219.283596	151914.861825	35.526669
1220.785049	152227.032004	35.531687
1221.267015	152516.683089	35.536704
1222.890778	152786.248101	35.541722
1224.087673	153078.601207	35.546740
1224.955091	153363.489757	35.551757
1226.677622	153657.853376	35.556775
1227.656017	153951.251339	35.561792
1229.031576	154231.052589	35.566810
1230.255610	154531.403199	35.571828
1232.057559	154814.436154	35.576845
1233.449438	155096.219773	35.581863
1234.456283	155361.275393	35.586880
1236.096367	155647.753255	35.591898
1237.297532	155940.876121	35.596916
1238.531997	156217.189034	35.601933
1239.785050	156471.455405	35.606951
1240.757254	156757.607816	35.611968
1242.289105	157054.413797	35.616986
1243.337262	157341.407845	35.622004
1244.261059	157603.752691	35.627021
1245.765776	157904.489218	35.632039
1246.562469	158194.347073	35.637056
1247.741356	158452.025497	35.642074
1248.879282	158745.053084	35.647092
1249.690082	159032.187477	35.652109
1250.627679	159301.784628	35.657127
1251.598500	159579.002039	35.662144
1252.952207	159883.127504	35.667162
1254.077097	160185.060392	35.672180
1255.593564	160481.082831	35.677197
1256.913680	160755.256929	35.682215
1257.977463	161034.245078	35.687232
1259.328948	161365.834312	35.692250
1260.300723	161662.170984	35.697268
1261.814503	161944.630535	35.702285
1263.186006	162251.726791	35.707303
1264.322576	162574.303382	35.712320
1265.662232	162861.783735	35.717338
1266.847792	163174.461554	35.722356
1267.864849	163495.149427	35.727373
1269.191938	163786.393531	35.732391
1270.352474	164094.971944	35.737408
1272.069460	164420.664217	35.742426
1273.632085	164722.989710	35.747444
1274.672381	165037.126448	35.752461
1276.446806	165354.379593	35.757479
1277.378280	165662.043121	35.762496
1279.118597	165957.332092	35.767514
1280.491350	166285.036762	35.772532
1281.551881	166578.792876	35.777549
1283.024859	166879.994008	35.782567
1284.380948	167203.546930	35.787584
1285.585815	167506.814056	35.792602
1286.540140	167818.409862	35.797620
1288.040364	168126.339796	35.802637
1289.389600	168453.608095	35.807655
1290.688550	168764.684346	35.812672
1291.651574	169065.083980	35.817690
1293.070572	169385.216930	35.822708
1294.107429	169726.478105	35.827725
1295.808826	170035.212999	35.832743
1296.679611	170350.583709	35.837760
1298.249533	170673.188033	35.842778
1299.480321	171015.734036	35.847796
1300.884953	171334.233851	35.852813
1302.423509	171647.993509	35.857831
1303.841086	171962.663550	35.862848
1305.134698	172287.900941	35.867866
1306.421305	172623.851558	35.872884
1307.434981	172940.904475	35.877901
1309.111467	173271.732448	35.882919
1309.832644	173607.732839	35.887936
1311.375436	173912.015582	35.892954
1312.863834	174251.206014	35.897972
1313.839833	174598.122755	35.902989
1315.302443	174921.828066	35.908007
1316.608527	175243.835608	35.913024
1317.766257	175562.519659	35.918042
1319.244502	175908.449502	35.923060
1320.217831	176273.538663	35.928077
1321.660097	176592.360338	35.933095
1322.595496	176924.453156	35.938112
1323.595260	177279.964361	35.943130
1325.056242	177624.285083	35.948148
1326.488952	177972.762785	35.953165
1328.235984	178316.952383	35.958183
1329.694486	178648.805722	35.963200
1330.990166	178987.998183	35.968218
1332.503391	179339.289737	35.973236
1333.999333	179662.348829	35.978253
1335.606992	180000.303788	35.983271
1336.701838	180308.114959	35.988288
1338.070049	180616.377874	35.993306
1339.062640	180947.688930	35.998324
1340.297174	181281.449779	36.003341
1341.514489	181590.961951	36.008359
1342.882526	181929.439015	36.013376
1344.316797	182262.107240	36.018394
1345.491179	182584.362405	36.023412
1346.762052	182908.532844	36.028429
1348.375669	183251.344133	36.033447
1349.404548	183597.427225	36.038464
1350.628831	183925.825499	36.043482
1351.857148	184266.358999	36.048500
1353.095836	184602.361816	36.053517
1354.920164	184940.465917	36.058535
1355.999996	185291.032189	36.063552
1357.657002	185648.105678	36.068570
1359.049533	185990.120880	36.073588
1360.437959	186308.339970	36.078605
1362.273187	186649.994369	36.083623
1363.682109	187009.174071	36.088640
1364.967644	187339.664887	36.093658
1366.804829	187679.408778	36.098676
1367.843582	188032.525523	36.103693
1369.434854	188377.442348	36.108711
1370.433907	188703.431744	36.113728
1371.891330	189051.027743	36.118746
1373.768827	189393.771129	36.123764
1374.687667	189729.452174	36.128781
1376.204698	190091.870851	36.133799
1377.524268	190431.463031	36.138816
1379.232932	190773.481003	36.143834
1381.061508	191111.533432	36.148852
1382.251595	191459.492941	36.153869
1383.474400	191832.443681	36.158887
1384.955946	192181.057585	36.163904
1385.953072	192523.165231	36.168922
1387.537144	192860.354186	36.173940
1388.581273	193230.969477	36.178957
1389.722734	193560.809279	36.183975
1390.732901	193945.474628	36.188992
1392.213250	194312.495571	36.194010
1393.447216	194671.092085	36.199028
1394.751289	195035.632965	36.204045
1396.503234	195400.051332	36.209063
1397.730935	195774.549237	36.214080
1398.990793	196160.596503	36.219098
1400.628087	196508.968544	36.224116
1401.816501	196890.830080	36.229133
1403.390257	197278.241611	36.234151
1404.372428	197663.798078	36.239168
1405.543262	198033.063042	36.244186
1407.473677	198401.417673	36.249204
1408.843673	198806.290202	36.254221
1409.861726	199184.308780	36.259239
1411.672236	199563.976163	36.264256
1413.384330	199930.534643	36.269274
1414.984304	200300.363782	36.274292
1416.593980	200699.914336	36.279309
1418.051396	201082.797285	36.284327
1419.466370	201461.029996	36.289344
1420.896557	201812.219728	36.294362
1422.380775	202174.854253	36.299380
1423.622324	202561.729678	36.304397
1424.979978	202925.176221	36.309415
1426.737153	203312.275474	36.314432
1427.759289	203702.608792	36.319450
1429.239252	204070.040488	36.324468
1430.267191	204430.159311	36.329485
1431.834798	204772.758486	36.334503
1433.176080	205141.653325	36.339520
1434.410065	205522.832792	36.344538
1436.164551	205875.462182	36.349556
1437.613062	206227.927926	36.354573
1438.537611	206598.790765	36.359591
1440.017987	206991.212080	36.364608
1441.476691	207362.092168	36.369626
1442.534761	207723.199955	36.374644
1443.716302	208114.063939	36.379661
1445.153707	208512.937754	36.384679
1446.615181	208905.384847	36.389696
1447.594117	209300.148302	36.394714
1448.882224	209692.120101	36.399732
1450.350542	210112.595382	36.404749
1451.773014	210530.553657	36.409767
1453.119627	210943.523784	36.414784
1454.354441	211353.238483	36.419802
1455.990700	211763.917532	36.424820
1457.283773	212196.393948	36.429837
1459.201090	212615.805087	36.434855
1460.697329	213038.119478	36.439872
1462.068731	213480.544860	36.444890
1464.105313	213886.571687	36.449908
1464.998112	214314.528410	36.454925
1466.608003	214756.438542	36.459943
1467.970047	215161.338286	36.464960
1469.735160	215597.030322	36.469978
1471.630591	216020.817313	36.474996
1473.051603	216454.284637	36.480013
1474.586425	216883.087615	36.485031
1476.653722	217308.934878	36.490048
1477.709521	217728.957281	36.495066
1479.732030	218186.765744	36.500084
1481.324618	218636.317014	36.505101
1482.495258	219059.323351	36.510119
1483.989967	219467.725193	36.515136
1485.491819	219873.410022	36.520154
1486.831898	220287.656943	36.525172
1488.519147	220742.028034	36.530189
1489.891238	221160.032246	36.535207
1491.804050	221576.526671	36.540224
1492.905406	222005.500316	36.545242
1494.331345	222443.921228	36.550260
1495.744883	222869.926135	36.555277
1497.030333	223300.144694	36.560295
1498.880957	223751.530529	36.565312
1500.173722	224193.866716	36.570330
1501.671841	224595.684825	36.575348
1503.256702	225037.620653	36.580365
1504.603986	225478.581478	36.585383
1506.353714	225913.407198	36.590400
1507.556984	226360.897452	36.595418
1509.255719	226816.003736	36.600436
1510.533406	227246.899271	36.605453
1512.098064	227657.505489	36.610471
1514.037647	228109.376665	36.615488
1515.050460	228569.860610	36.620506
1516.683970	229013.632293	36.625524
1518.002185	229442.293762	36.630541
1519.684535	229877.449837	36.635559
1521.281577	230352.804617	36.640576
1522.617923	230801.787834	36.645594
1524.357423	231221.521012	36.650612
1525.869562	231671.951397	36.655629
1527.512418	232130.032683	36.660647
1529.228830	232549.164179	36.665664
1530.346583	232991.561171	36.670682
1532.223729	233418.873174	36.675700
1533.531827	233850.242882	36.680717
1534.681134	234257.636179	36.685735
1535.912147	234685.668138	36.690752
1537.422137	235147.845145	36.695770
1538.939831	235579.642489	36.700788
1540.582978	236020.488572	36.705805
1541.901425	236483.717209	36.710823
1543.208282	236920.861879	36.715840
1544.377102	237364.609466	36.720858
1546.366473	237832.074860	36.725876
1547.417719	238289.637308	36.730893
1548.977481	238755.220184	36.735911
1550.362951	239225.964192	36.740928
1551.889255	239712.181277	36.745946
1553.444545	240183.941211	36.750964
1554.952348	240642.755189	36.755981
1556.537506	241139.406433	36.760999
1558.181574	241637.065291	36.766016
1559.625631	242115.986229	36.771034
1561.360876	242600.499508	36.776052
1563.002316	243086.832931	36.781069
1564.463753	243555.390153	36.786087
1566.386052	244058.470278	36.791104
1567.617415	244557.550327	36.796122
1569.887509	245035.376026	36.801140
1571.339649	245530.204874	36.806157
1572.986886	246012.936310	36.811175
1574.758123	246480.990907	36.816192
1576.731202	246987.752020	36.821210
1577.949263	247477.669666	36.826228
1579.162764	247961.162024	36.831245
1580.922055	248473.346440	36.836263
1582.523690	248955.099783	36.841280
1583.792219	249439.906356	36.846298
1585.619539	249948.855779	36.851316
1587.557932	250442.545891	36.856333
1589.174039	250934.714879	36.861351
1591.548685	251441.162844	36.866368
1592.913301	251930.326255	36.871386
1594.953914	252399.818378	36.876404
1596.443138	252891.832889	36.881421
1597.887838	253372.703325	36.886439
1599.865618	253856.382241	36.891456
1601.119137	254344.474246	36.896474
1602.486874	254851.193761	36.901492
1603.871483	255345.666603	36.906509
1605.982724	255838.648173	36.911527
1607.577166	256317.337153	36.916544
1608.692161	256823.947490	36.921562
1610.676204	257329.017578	36.926580
1612.147547	257800.564034	36.931597
1614.170373	258292.266126	36.936615
1615.754019	258796.158257	36.941632
1617.386100	259301.033316	36.946650
1619.070760	259777.524380	36.951668
1621.059334	260262.551734	36.956685
1622.097961	260750.098422	36.961703
1623.980295	261240.579771	36.966720
1625.869868	261722.346629	36.971738
1627.428875	262206.987804	36.976756
1629.220193	262701.421711	36.981773
1630.565521	263171.059319	36.986791
1632.361635	263662.697949	36.991808
1633.551969	264171.761467	36.996826
1635.098110	264673.145150	37.001844
1636.669931	265146.530015	37.006861
1637.942198	265611.885886	37.011879
1639.949884	266102.447267	37.016896
1641.371498	266580.174845	37.021914
1642.777253	267057.574537	37.026932
1644.264226	267541.997228	37.031949
1645.701947	268040.297862	37.036967
1647.514259	268506.629937	37.041984
1648.921047	269009.024830	37.047002
1650.595860	269506.497663	37.052020
1652.054229	270001.185999	37.057037
1653.481983	270517.522323	37.062055
1655.123659	271036.947364	37.067072
1656.444107	271538.998328	37.072090
1657.791129	272039.799565	37.077108
1659.564217	272576.424259	37.082125
1661.024578	273126.664952	37.087143
1662.698942	273637.698267	37.092160
1664.320776	274185.421198	37.097178
1665.841215	274722.948031	37.102196
1667.447264	275255.633308	37.107213
1668.879145	275824.342026	37.112231
1670.714721	276360.772470	37.117248
1672.477308	276911.693423	37.122266
1673.949413	277485.726702	37.127284
1676.072826	278022.563623	37.132301
1677.367023	278582.144385	37.137319
1679.027311	279162.849056	37.142336
1680.773784	279702.970578	37.147354
1682.427134	280284.537275	37.152372
1684.286540	280867.059138	37.157389
1685.895710	281443.879831	37.162407
1688.059005	281990.074246	37.167424
1689.791250	282577.819742	37.172442
1691.492177	283149.082821	37.177460
1693.296969	283715.729334	37.182477
1694.888144	284318.124231	37.187495
1696.345724	284871.234548	37.192512
1697.834754	285449.714139	37.197530
1699.820776	286041.343985	37.202548
1702.076950	286603.969589	37.207565
1703.437708	287212.463373	37.212583
1705.368326	287774.020997	37.217600
1707.134953	288353.384469	37.222618
1708.893968	288941.662785	37.227636
1710.514766	289528.970976	37.232653
1712.147642	290115.030199	37.237671
1713.942678	290692.424049	37.242688
1715.755730	291276.162732	37.247706
1717.730558	291852.302920	37.252724
1719.906239	292437.196079	37.257741
1721.236967	293010.694340	37.262759
1723.284615	293586.738842	37.267776
1725.236538	294191.066836	37.272794
1726.941404	294757.281980	37.277812
1728.970777	295309.852098	37.282829
1730.717242	295878.519012	37.287847
1732.749457	296455.822755	37.292864
1734.817554	297017.293887	37.297882
1736.237324	297573.814794	37.302900
1738.138786	298122.709959	37.307917
1739.701014	298692.739668	37.312935
1741.411374	299259.363949	37.317952
1743.367918	299820.560126	37.322970
1744.726854	300385.890360	37.327988
1746.811196	300944.570479	37.333005
1748.479409	301499.354107	37.338023
1750.208357	302047.064004	37.343040
1752.435843	302610.765741	37.348058
1754.163269	303155.828468	37.353076
1755.862727	303678.745859	37.358093
1757.613310	304201.601221	37.363111
1759.077657	304724.653357	37.368128
1761.319574	305273.911516	37.373146
1763.041382	305801.562967	37.378164
1764.798857	306302.005168	37.383181
1766.631791	306824.857778	37.388199
1768.532212	307364.001044	37.393216
1770.166094	307914.867537	37.398234
1771.644577	308432.893084	37.403252
1773.330223	308954.640069	37.408269
1775.144462	309511.790490	37.413287
1776.472176	310044.916655	37.418304
1778.633501	310598.701224	37.423322
1779.864809	311170.412586	37.428340
1781.823487	311706.166840	37.433357
1783.324981	312273.686496	37.438375
1784.861486	312842.694722	37.443392
1786.611196	313395.639454	37.448410
1788.234514	313972.751710	37.453428
1789.878344	314558.033423	37.458445
1791.165160	315145.350382	37.463463
1792.976020	315720.691862	37.468480
1795.158071	316309.604379	37.473498
1796.942640	316917.343933	37.478516
1798.388728	317520.918994	37.483533
1800.103297	318107.278809	37.488551
1802.027875	318697.306664	37.493568
1803.856737	319309.539001	37.498586
1805.786885	319935.004418	37.503604
1807.443534	320550.834805	37.508621
1809.379324	321154.476135	37.513639
1811.410250	321765.866482	37.518656
1813.288802	322366.459517	37.523674
1814.704991	322979.286107	37.528692
1817.003639	323593.307256	37.533709
1818.780351	324218.504771	37.538727
1820.608035	324852.473191	37.543744
1822.492001	325464.590091	37.548762
1824.005073	326074.578754	37.553780
1825.949743	326697.337839	37.558797
1827.713060	327344.622025	37.563815
1829.364193	327976.938058	37.568832
1831.539623	328602.915322	37.573850
1833.385272	329230.920937	37.578868
1835.349330	329853.975056	37.583885
1837.081427	330516.438809	37.588903
1838.719355	331152.862229	37.593920
1840.713552	331776.043571	37.598938
1842.616279	332410.073963	37.603956
1844.322657	333048.191806	37.608973
1846.478844	333703.694799	37.613991
1848.637492	334339.489522	37.619008
1851.006791	334948.408568	37.624026
1852.700991	335582.793378	37.629044
1854.539288	336209.099745	37.634061
1856.434473	336834.831094	37.639079
1857.932606	337448.867234	37.644096
1860.024314	338080.796632	37.649114
1861.739815	338710.699061	37.654132
1863.703851	339367.943061	37.659149
1865.541046	340009.182267	37.664167
1867.327374	340627.144836	37.669184
1869.333709	341252.729629	37.674202
1871.079076	341904.367848	37.679220
1873.205143	342532.963252	37.684237
1874.854675	343160.487223	37.689255
1876.654890	343759.626283	37.694272
1878.422739	344357.012108	37.699290
1880.167835	344998.076623	37.704308
1882.358072	345603.017595	37.709325
1883.826609	346206.597987	37.714343
1885.583086	346828.118398	37.719360
1887.222708	347453.888590	37.724378
1888.744446	348089.187588	37.729396
1890.849544	348703.722619	37.734413
1892.499093	349337.511679	37.739431
1894.551365	349989.016502	37.744448
1896.644288	350614.365261	37.749466
1897.893747	351247.483557	37.754484
1900.240942	351912.464567	37.759501
1901.807198	352567.337395	37.764519
1903.938583	353200.308305	37.769536
1906.008885	353838.584113	37.774554
1907.321843	354524.049314	37.779572
1909.444055	355169.326653	37.784589
1911.715148	355829.059529	37.789607
1913.262174	356499.635630	37.794624
1915.507357	357179.906293	37.799642
1917.303708	357837.732831	37.804660
1919.359881	358514.156424	37.809677
1921.399652	359186.943412	37.814695
1923.378808	359872.213331	37.819712
1925.695718	360534.935736	37.824730
1927.270299	361202.616123	37.829748
1929.357303	361890.498900	37.834765
1931.208715	362566.509557	37.839783
1933.115922	363233.569000	37.844800
1935.466608	363921.855817	37.849818
1937.493362	364611.782539	37.854836
1939.311337	365275.067764	37.859853
1941.302500	365963.987326	37.864871
1943.146257	366658.804725	37.869888
1944.935195	367348.798694	37.874906
1946.677381	368037.265955	37.879924
1948.467340	368730.228455	37.884941
1950.527093	369420.394189	37.889959
1952.253945	370146.369543	37.894976
1954.377001	370833.125216	37.899994
1956.112490	371518.080484	37.905012
1958.327305	372246.369706	37.910029
1960.220504	372971.501620	37.915047
1962.235462	373667.988025	37.920064
1964.401983	374359.261868	37.925082
1966.483616	375075.747801	37.930100
1968.314824	375791.575967	37.935117
1970.335886	376514.738957	37.940135
1972.035080	377222.215916	37.945152
1974.311186	377939.322330	37.950170
1976.287981	378659.303870	37.955188
1978.158326	379362.474170	37.960205
1980.523269	380081.119580	37.965223
1982.318530	380798.550626	37.970240
1984.193896	381502.158239	37.975258
1985.967646	382241.903588	37.980276
1988.200494	382957.594008	37.985293
1990.442762	383673.267636	37.990311
1992.105327	384415.265642	37.995328
1994.177023	385133.852033	38.000346
1995.721653	385859.152853	38.005364
1997.582102	386592.093461	38.010381
1999.680131	387329.440788	38.015399
2001.415540	388055.041650	38.020416
2003.413747	388788.062040	38.025434
2005.380371	389526.597751	38.030452
2007.340086	390239.917557	38.035469
2009.389663	390950.950204	38.040487
2011.329080	391663.582084	38.045504
2014.042744	392359.744449	38.050522
2016.246248	393069.638928	38.055540
2018.481590	393781.083547	38.060557
2020.500768	394458.630959	38.065575
2022.129576	395170.346260	38.070592
2024.293863	395892.399791	38.075610
2026.216953	396604.996201	38.080628
2028.230666	397309.450044	38.085645
2030.295000	398041.404368	38.090663
2032.050323	398757.880567	38.095680
2033.921457	399474.599172	38.100698
2035.644620	400199.384118	38.105716
2037.509432	400936.900775	38.110733
2039.794405	401683.655570	38.115751
2041.561045	402438.586054	38.120768
2043.570313	403169.281330	38.125786
2045.279827	403931.100312	38.130804
2047.422292	404705.598884	38.135821
2049.919700	405442.769275	38.140839
2051.869294	406187.840407	38.145856
2054.060280	406957.176320	38.150874
2056.265943	407745.162122	38.155892
2058.355048	408514.218571	38.160909
2060.341354	409254.869302	38.165927
2062.230003	410029.921190	38.170944
2064.450205	410807.480585	38.175962
2066.565602	411588.277790	38.180980
2068.618734	412356.067048	38.185997
2070.708580	413135.582505	38.191015
2072.424092	413929.347955	38.196032
2074.513497	414701.725112	38.201050
2076.930897	415487.982482	38.206068
2078.973871	416287.449343	38.211085
2081.490815	417089.422546	38.216103
2083.278435	417878.523724	38.221120
2085.787190	418647.195282	38.226138
2087.904112	419435.004472	38.231156
2090.029451	420234.488445	38.236173
2092.518588	421008.309768	38.241191
2094.860575	421791.602939	38.246208
2097.117302	422555.716530	38.251226
2099.342386	423352.984236	38.256244
2101.361925	424142.689460	38.261261
2103.804407	424905.612130	38.266279
2105.631694	425675.322599	38.271296
2107.891050	426452.862735	38.276314
2109.813484	427244.865260	38.281332
2111.920419	428029.469751	38.286349
2114.164128	428790.937768	38.291367
2115.859997	429593.078720	38.296384
2118.024150	430368.079524	38.301402
2120.231618	431170.741829	38.306420
2122.515546	431953.114037	38.311437
2124.928769	432716.758677	38.316455
2126.734349	433505.081813	38.321472
2129.048800	434309.037993	38.326490
2131.028049	435092.976536	38.331508
2133.362246	435859.468281	38.336525
2135.446401	436638.680749	38.341543
2137.065123	437444.921394	38.346560
2139.560178	438239.449630	38.351578
2141.893660	439021.476073	38.356596
2144.029677	439798.548608	38.361613
2146.185062	440594.771736	38.366631
2148.549054	441379.444951	38.371648
2151.171503	442120.731066	38.376666
2153.559901	442844.826434	38.381684
2155.820201	443577.774656	38.386701
2158.562854	444322.054659	38.391719
2160.339495	445052.453463	38.396736
2162.408629	445779.136992	38.401754
2164.531784	446534.322755	38.406772
2166.227679	447271.086711	38.411789
2168.504562	447998.471887	38.416807
2170.586704	448762.339543	38.421824
2172.295081	449520.778466	38.426842
2174.251710	450255.678120	38.431860
2176.239753	451033.391859	38.436877
2178.273231	451809.097136	38.441895
2180.064305	452564.430391	38.446912
2182.303247	453350.009817	38.451930
2184.424462	454132.241405	38.456948
2186.208749	454931.998199	38.461965
2188.342132	455730.301442	38.466983
2190.363908	456539.313478	38.472000
2192.151435	457343.022940	38.477018
2194.479263	458147.876245	38.482036
2196.403657	458990.637435	38.487053
2199.038083	459825.106368	38.492071
2201.455913	460636.824750	38.497088
2203.372622	461449.806758	38.502106
2205.815088	462297.502708	38.507124
2207.836907	463158.831427	38.512141
2210.129977	463983.681061	38.517159
2212.366804	464815.380714	38.522176
2214.276797	465677.579791	38.527194
2217.044611	466525.699899	38.532212
2219.008133	467380.335178	38.537229
2221.153470	468213.827650	38.542247
2223.235265	469087.675742	38.547264
2225.590089	469949.614046	38.552282
2228.236833	470793.172447	38.557300
2230.382706	471658.657066	38.562317
2233.173506	472523.137403	38.567335
2235.468804	473400.747088	38.572352
2237.652593	474245.493320	38.577370
2239.675322	475114.833300	38.582388
2241.749825	475987.055006	38.587405
2244.646879	476838.691265	38.592423
2246.980279	477707.860384	38.597440
2249.212629	478567.004012	38.602458
2251.569388	479434.522875	38.607476
2253.690904	480288.503491	38.612493
2256.077486	481175.280759	38.617511
2258.058547	482035.920914	38.622528
2260.456467	482891.351191	38.627546
2262.674920	483777.020137	38.632564
2265.012684	484659.091432	38.637581
2267.593013	485523.659092	38.642599
2269.289444	486417.010526	38.647616
2271.328166	487291.630392	38.652634
2273.497426	488157.199219	38.657652
2275.421155	489058.206674	38.662669
2277.968751	489948.868102	38.667687
2280.697460	490832.993356	38.672704
2282.822822	491725.653770	38.677722
2285.386393	492596.946708	38.682740
2287.325746	493498.178413	38.687757
2289.746707	494398.930692	38.692775
2291.819857	495268.151791	38.697792
2293.972231	496174.659432	38.702810
2296.348402	497056.759932	38.707828
2298.433073	497933.918043	38.712845
2300.924118	498803.092827	38.717863
2303.018178	499688.938268	38.722880
2305.153357	500558.283503	38.727898
2307.124323	501419.640103	38.732916
2309.056318	502307.039418	38.737933
2311.216668	503192.487598	38.742951
2313.213587	504091.383245	38.747968
2315.882403	504960.260314	38.752986
2318.817292	505844.531403	38.758004
2320.576347	506769.546837	38.763021
2322.539224	507675.162074	38.768039
2325.180271	508569.118051	38.773056
2326.944026	509468.817059	38.778074
2329.646974	510398.059715	38.783092
2331.933286	511333.065276	38.788109
2334.619511	512247.229968	38.793127
2336.508561	513149.627079	38.798144
2338.558846	514092.576623	38.803162
2341.117211	515046.929579	38.808180
2342.916777	516009.162685	38.813197
2345.287741	516940.801219	38.818215
2347.621962	517904.896842	38.823232
2349.788750	518874.957642	38.828250
2352.160752	519858.832202	38.833268
2354.132451	520834.043806	38.838285
2356.349068	521827.997421	38.843303
2358.515600	522822.550194	38.848320
2360.372810	523814.469928	38.853338
2362.588459	524805.712152	38.858356
2364.743664	525837.096204	38.863373
2367.723753	526865.755793	38.868391
2370.677501	527873.952120	38.873408
2372.843614	528875.210594	38.878426
2375.701988	529900.258382	38.883444
2377.847858	530945.998518	38.888461
2380.072779	531969.548199	38.893479
2382.418542	532993.712134	38.898496
2384.479107	534030.135896	38.903514
2386.949992	535071.553653	38.908532
2388.812579	536145.011625	38.913549
2391.449242	537191.989306	38.918567
2393.904023	538255.932755	38.923584
2396.172548	539319.677704	38.928602
2398.683411	540372.233419	38.933620
2400.891979	541437.844465	38.938637
2403.082551	542530.951213	38.943655
2405.632782	543622.355144	38.948672
2408.145374	544699.293660	38.953690
2410.935626	545752.009342	38.958708
2413.142591	546848.804166	38.963725
2415.373738	547922.373551	38.968743
2418.226520	549002.496879	38.973760
2420.270140	550116.563119	38.978778
2423.015227	551218.004219	38.983796
2425.093733	552305.640540	38.988813
2427.506570	553376.394071	38.993831
2430.297425	554474.348946	38.998848
2432.578170	555582.654457	39.003866
2435.320619	556666.365651	39.008884
2437.560796	557789.777230	39.013901
2440.016039	558898.686881	39.018919
2442.284572	559981.706944	39.023936
2444.420574	561086.819758	39.028954
2447.026023	562204.273753	39.033972
2449.265607	563322.799142	39.038989
2451.849606	564418.718621	39.044007
2454.018205	565544.300912	39.049024
2456.204589	566650.446973	39.054042
2459.070526	567726.706750	39.059060
2461.452102	568829.170489	39.064077
2463.984678	569893.705536	39.069095
2466.317775	570989.515744	39.074112
2468.457065	572106.701680	39.079130
2470.851309	573182.182896	39.084148
2472.978348	574273.077793	39.089165
2475.699323	575383.004439	39.094183
2477.979280	576505.001567	39.099200
2480.534616	577628.660168	39.104218
2482.641205	578728.006372	39.109236
2484.998103	579856.967650	39.114253
2487.394408	580992.492795	39.119271
2489.891548	582120.975023	39.124288
2491.728661	583283.672043	39.129306
2494.354199	584453.903580	39.134324
2496.722116	585612.030264	39.139341
2499.337731	586766.396194	39.144359
2502.058717	587927.103682	39.149376
2504.404061	589109.320570	39.154394
2507.053682	590287.211078	39.159412
2509.066243	591483.186985	39.164429
2511.912738	592677.302579	39.169447
2514.550680	593863.765995	39.174464
2516.762782	595066.968657	39.179482
2519.303901	596257.368660	39.184500
2521.636688	597479.246589	39.189517
2524.262059	598695.789875	39.194535
2527.356436	599915.085160	39.199552
2529.235033	601162.451146	39.204570
2531.933293	602379.400769	39.209588
2534.601758	603595.126115	39.214605
2536.736333	604843.406493	39.219623
2539.786543	606086.093995	39.224640
2542.237044	607325.542079	39.229658
2544.787199	608547.170827	39.234676
2547.212240	609805.774088	39.239693
2549.581217	611071.202744	39.244711
2552.276770	612328.780405	39.249728
2554.575948	613594.888130	39.254746
2557.389295	614858.116873	39.259764
2560.056645	616125.678521	39.264781
2562.641027	617392.259247	39.269799
2565.446144	618654.658287	39.274816
2567.720899	619922.250631	39.279834
2570.498081	621185.714439	39.284852
2572.865883	622480.743845	39.289869
2575.251263	623784.363980	39.294887
2578.069717	625053.921257	39.299904
2580.374298	626344.752664	39.304922
2582.901040	627647.085201	39.309940
2585.601846	628935.342367	39.314957
2587.866771	630256.386280	39.319975
2590.484849	631541.096054	39.324992
2593.177618	632862.545335	39.330010
2595.838665	634157.169291	39.335028
2598.505427	635482.589725	39.340045
2600.738089	636792.687976	39.345063
2603.912488	638103.615160	39.350080
2606.286898	639414.709052	39.355098
2609.092767	640726.065440	39.360116
2611.694881	642045.771936	39.365133
2614.344714	643369.891704	39.370151
2616.894563	644675.349894	39.375168
2619.495491	645988.065108	39.380186
2622.011939	647326.010267	39.385204
2624.575398	648663.771473	39.390221
2627.276646	649963.440182	39.395239
2629.804634	651243.676873	39.400256
2632.242240	652550.134130	39.405274
2634.471397	653852.218864	39.410292
2637.203021	655144.632300	39.415309
2639.642410	656427.259400	39.420327
2642.026079	657736.234078	39.425344
2644.550284	659045.410475	39.430362
2647.312975	660357.560909	39.435380
2650.118055	661684.169932	39.440397
2652.225202	663007.078757	39.445415
2655.323723	664310.227373	39.450432
2657.799786	665651.335372	39.455450
2660.524073	666989.279593	39.460468
2663.334230	668311.297465	39.465485
2665.927869	669665.263485	39.470503
2668.884961	671004.848050	39.475520
2671.468621	672355.498281	39.480538
2673.835882	673711.313790	39.485556
2677.021782	675074.508128	39.490573
2679.465125	676419.925800	39.495591
2682.404064	677774.266406	39.500608
2684.943387	679142.991749	39.505626
2687.568286	680518.609220	39.510644
2690.242423	681887.305887	39.515661
2692.974377	683258.125718	39.520679
2695.500275	684652.274055	39.525696
2698.180701	686058.255508	39.530714
2700.592439	687442.411395	39.535732
2703.392707	688833.145676	39.540749
2705.800719	690251.982003	39.545767
2708.990289	691661.233707	39.550784
2711.401647	693077.788724	39.555802
2713.804670	694504.791225	39.560820
2717.142963	695935.282203	39.565837
2719.588865	697364.301618	39.570855
2722.093695	698776.911231	39.575872
2724.672390	700227.321701	39.580890
2727.562252	701670.004484	39.585908
2730.523904	703092.706670	39.590925
2733.046796	704573.345204	39.595943
2735.868593	706013.142330	39.600960
2738.735718	707479.699628	39.605978
2741.493809	708938.099390	39.610996
2744.301141	710386.040073	39.616013
2746.940864	711860.410229	39.621031
2749.535652	713318.489824	39.626048
2752.314050	714782.379782	39.631066
2755.180214	716255.111543	39.636084
2757.904620	717739.736431	39.641101
2760.342022	719217.467048	39.646119
2763.236649	720686.154892	39.651136
2765.657585	722179.297939	39.656154
2768.432335	723681.463202	39.661172
2771.528222	725190.622701	39.666189
2774.212488	726689.192745	39.671207
2776.778668	728180.293306	39.676224
2779.447403	729675.357015	39.681242
2781.961602	731202.440233	39.686260
2785.211321	732697.399453	39.691277
2787.584903	734218.160616	39.696295
2790.223803	735731.925791	39.701312
2793.507672	737250.929895	39.706330
2796.287568	738778.517630	39.711348
2798.937857	740296.605917	39.716365
2801.323567	741822.838547	39.721383
2804.463775	743359.212705	39.726400
2807.136816	744893.590426	39.731418
2809.214181	746405.722716	39.736436
2812.571959	747900.391082	39.741453
2815.658766	749401.376375	39.746471
2818.571957	750868.041949	39.751488
2821.412498	752350.164410	39.756506
2823.900412	753849.849479	39.761524
2827.347316	755335.538636	39.766541
2829.837786	756830.752829	39.771559
2832.910373	758330.652328	39.776576
2835.606665	759805.752250	39.781594
2838.320131	761295.331664	39.786612
2841.387091	762807.199970	39.791629
2843.802306	764330.634098	39.796647
2846.720335	765825.833751	39.801664
2849.523420	767354.152133	39.806682
2852.161315	768882.678119	39.811700
2855.210972	770410.971214	39.816717
2857.718621	771947.052319	39.821735
2860.209223	773498.348108	39.826752
2862.907996	775054.639928	39.831770
2865.637182	776594.976771	39.836788
2868.518508	778169.246785	39.841805
2870.895597	779752.247118	39.846823
2873.896888	781329.646382	39.851840
2876.610733	782942.187375	39.856858
2878.901865	784554.782459	39.861876
2882.501398	786153.408387	39.866893
2885.154407	787755.415330	39.871911
2888.144901	789370.395663	39.876928
2891.425271	790981.089789	39.881946
2893.855545	792609.792861	39.886964
2897.036869	794252.012997	39.891981
2899.713558	795879.089715	39.896999
2902.366564	797529.011083	39.902016
2905.656317	799196.264078	39.907034
2908.324056	800838.057436	39.912052
2911.504662	802475.365466	39.917069
2914.376712	804143.998371	39.922087
2917.464641	805817.133961	39.927104
2920.546142	807468.490087	39.932122
2923.912022	809119.450757	39.937140
2926.711213	810792.496300	39.942157
2929.990773	812469.010626	39.947175
2932.553241	814117.035066	39.952192
2935.673033	815784.741542	39.957210
2938.344786	817475.698192	39.962228
2941.165392	819146.771568	39.967245
2944.165048	820835.019964	39.972263
2947.043588	822512.075550	39.977280
2949.961490	824206.899672	39.982298
2952.786983	825899.305158	39.987316
2955.865874	827589.137696	39.992333
2958.569793	829298.098112	39.997351
2961.433242	831010.972682	40.002368
2964.633752	832713.401855	40.007386
2967.620260	834430.229221	40.012404
2970.858157	836106.333508	40.017421
2973.766385	837822.516324	40.022439
2976.981754	839529.137047	40.027456
2979.975614	841219.281327	40.032474
2982.410767	842934.659551	40.037492
2985.332718	844664.815306	40.042509
2988.307203	846384.036438	40.047527
2991.058375	848104.090281	40.052544
2993.868098	849833.480771	40.057562
2996.691910	851559.671483	40.062580
2999.771498	853309.530468	40.067597
3002.813843	855047.736198	40.072615
3005.951102	856745.246924	40.077632
3009.279339	858439.251354	40.082650
3011.941758	860135.131398	40.087668
3015.308851	861804.818061	40.092685
3017.982192	863514.602695	40.097703
3020.588859	865204.335147	40.102720
3023.645595	866905.251230	40.107738
3026.293176	868603.722169	40.112756
3029.743317	870301.292272	40.117773
3032.327084	872021.961245	40.122791
3034.949242	873721.121623	40.127808
3038.241898	875460.821632	40.132826
3040.571474	877207.428458	40.137844
3043.703910	878955.710144	40.142861
3046.261456	880707.243899	40.147879
3049.056583	882474.071435	40.152896
3052.154532	884261.674626	40.157914
3055.086843	886044.797575	40.162932
3058.264060	887821.925946	40.167949
3061.507490	889616.844157	40.172967
3064.398693	891422.845995	40.177984
3067.561476	893226.982892	40.183002
3070.290909	895059.466032	40.188020
3073.338231	896886.392191	40.193037
3076.910733	898686.715368	40.198055
3080.086991	900523.827570	40.203072
3083.449617	902343.935776	40.208090
3086.364033	904218.424143	40.213108
3089.332201	906056.946566	40.218125
3092.674609	907894.322528	40.223143
3095.330888	909744.098480	40.228160
3099.024819	911588.279215	40.233178
3102.155765	913440.784006	40.238196
3105.279470	915310.256779	40.243213
3108.560260	917182.430935	40.248231
3111.272361	919034.753697	40.253248
3114.850913	920900.803424	40.258266
3118.059619	922778.943383	40.263284
3121.166018	924646.758674	40.268301
3124.065997	926519.908649	40.273319
3127.252182	928388.715955	40.278336
3130.646248	930258.083622	40.283354
3133.799357	932146.095356	40.288372
3137.016778	934028.829385	40.293389
3140.166764	935914.065743	40.298407
3143.436806	937794.111306	40.303424
3146.659417	939669.761954	40.308442
3149.587991	941570.613974	40.313460
3152.659530	943454.975960	40.318477
3155.724968	945358.154126	40.323495
3158.662435	947266.101081	40.328512
3162.544402	949163.638199	40.333530
3165.179721	951060.395322	40.338548
3168.835262	952945.881500	40.343565
3171.959354	954846.786827	40.348583
3175.414240	956766.042297	40.353600
3178.972671	958704.213685	40.358618
3182.279067	960655.270014	40.363636
3185.422663	962605.302197	40.368653
3188.900096	964531.069598	40.373671
3191.749609	966473.879603	40.378688
3195.150827	968411.352990	40.383706
3198.446685	970357.366774	40.388724
3201.528191	972277.969549	40.393741
3205.294485	974211.571622	40.398759
3207.845060	976147.062148	40.403776
3211.245532	978064.990784	40.408794
3214.309503	980003.966942	40.413812
3217.528825	981936.414601	40.418829
3220.417485	983832.229006	40.423847
3223.460824	985730.990374	40.428864
3226.827821	987596.948963	40.433882
3229.566195	989489.544628	40.438900
3232.548760	991381.568077	40.443917
3235.869129	993289.337935	40.448935
3238.481610	995235.753311	40.453952
3241.752496	997123.776130	40.458970
3244.660886	999035.998194	40.463988
3247.965486	1000968.579663	40.469005
3251.443988	1002911.829174	40.474023
3254.776570	1004864.817270	40.479040
3258.097625	1006805.492867	40.484058
3261.380558	1008754.622205	40.489076
3264.673446	1010702.494885	40.494093
3268.157648	1012650.631817	40.499111
3270.990245	1014639.465112	40.504128
3273.688559	1016603.410707	40.509146
3276.844817	1018590.309085	40.514164
3279.899009	1020580.004606	40.519181
3282.925253	1022596.565544	40.524199
3285.689882	1024647.058756	40.529216
3289.036608	1026674.378370	40.534234
3292.145082	1028711.630600	40.539252
3294.897420	1030773.020765	40.544269
3298.264195	1032830.652359	40.549287
3301.644916	1034916.476070	40.554304
3304.734368	1036997.804555	40.559322
3308.161017	1039087.943338	40.564340
3311.693427	1041157.998703	40.569357
3314.683595	1043255.125791	40.574375
3317.691522	1045373.998926	40.579392
3321.606449	1047507.994013	40.584410
3324.940373	1049621.626577	40.589428
3328.110458	1051737.846598	40.594445
3331.779995	1053856.444581	40.599463
3334.895405	1055993.646335	40.604480
3338.334333	1058130.543690	40.609498
3341.212576	1060289.089351	40.614516
3344.252341	1062447.914739	40.619533
3347.513668	1064601.056734	40.624551
3350.669105	1066767.286329	40.629568
3354.046379	1068950.561455	40.634586
3356.968111	1071156.628980	40.639604
3360.067421	1073340.310437	40.644621
3363.376948	1075538.797745	40.649639
3366.656901	1077760.442738	40.654656
3370.156700	1079956.929174	40.659674
3373.451956	1082162.899138	40.664692
3376.501430	1084399.771809	40.669709
3379.986946	1086645.788078	40.674727
3383.071371	1088878.232080	40.679744
3386.330765	1091106.959485	40.684762
3389.844074	1093368.724249	40.689780
3392.618291	1095626.708038	40.694797
3396.423462	1097896.460890	40.699815
3399.815431	1100164.757038	40.704832
3403.281747	1102424.176236	40.709850
3406.774988	1104688.267219	40.714868
3409.822826	1106964.434709	40.719885
3413.118497	1109251.310138	40.724903
3416.423067	1111547.680482	40.729920
3419.884458	1113815.456382	40.734938
3423.523998	1116104.115065	40.739956
3426.771330	1118391.956389	40.744973
3429.981648	1120686.522023	40.749991
3433.576775	1122978.520648	40.755008
3437.644052	1125257.157174	40.760013
3440.657669	1127457.638819	40.765018
3444.036815	1129601.334179	40.770023
3447.423103	1131672.305404	40.775028
3450.352617	1133705.014003	40.780032
3453.575423	1135637.830791	40.785037
3456.724087	1137503.112255	40.790042
3459.414501	1139299.947921	40.795047
3462.452203	1140993.165942	40.800052
3464.954188	1142615.357010	40.805056
3467.710778	1144156.403766	40.810061
3470.366527	1145650.374880	40.815066
3472.799212	1147037.051145	40.820071
3475.287312	1148353.899183	40.825076
3477.178820	1149608.183255	40.830080
3479.237339	1150778.417302	40.835085
3481.373423	1151890.333211	40.840090
3483.171530	1152936.651688	40.845095
3485.312872	1153909.348498	40.850100
3486.930132	1154828.481269	40.855104
3488.849579	1155704.161203	40.860109
3490.273074	1156531.337907	40.865114
3491.475342	1157287.853981	40.870119
3493.413996	1157987.485712	40.875124
3494.577256	1158638.448594	40.880128
3495.966989	1159226.033619	40.885133
3497.788116	1159803.175963	40.890138
3498.654135	1160315.652770	40.895143
3499.827718	1160809.217248	40.900148
3501.115458	1161210.556770	40.905152
3502.455300	1161578.398076	40.910157
3503.374231	1161957.813114	40.915162
3504.485455	1162263.550444	40.920167
3505.581106	1162549.427642	40.925172
3506.138566	1162807.218492	40.930176
3506.797456	1163013.955026	40.935181
3507.604692	1163219.808579	40.940186
3508.585974	1163365.249984	40.945191
3509.224644	1163507.531376	40.950196
3509.714035	1163633.488489	40.955200
3510.662632	1163719.308288	40.960205
3510.913486	1163773.308338	40.965210
3511.627292	1163817.122607	40.970215
3512.220975	1163847.824142	40.975220
3512.811433	1163857.269009	40.980224
3513.220571	1163855.784532	40.985229
3513.620269	1163811.409384	40.990234
3514.299329	1163753.288605	40.995239
3514.886161	1163697.638819	41.000244
3515.083031	1163613.803158	41.005248
3515.658259	1163512.330215	41.010253
3515.952818	1163386.052216	41.015258
3516.420617	1163251.900252	41.020263
3517.006170	1163127.268860	41.025268
3516.865927	1162973.083708	41.030272
3517.312921	1162804.434116	41.035277
3517.854433	1162645.213312	41.040282
3517.637817	1162464.566361	41.045287
3517.938898	1162259.445787	41.050292
3518.374018	1162050.609290	41.055296
3518.427490	1161846.741960	41.060301
3518.838102	1161647.911736	41.065306
3519.020099	1161409.791478	41.070311
3519.056879	1161179.246259	41.075316
3519.553740	1160938.311547	41.080320
3519.330734	1160683.020793	41.085325
3519.697812	1160409.280099	41.090330
3519.988252	1160162.104237	41.095335
3519.769300	1159903.938630	41.100340
3520.083724	1159616.172257	41.105344
3520.185418	1159319.631298	41.110349
3520.313217	1159058.057459	41.115354
3520.046276	1158797.103001	41.120359
3520.521643	1158488.065245	41.125364
3520.381351	1158209.753929	41.130368
3520.311259	1157904.176444	41.135373
3520.959535	1157590.706604	41.140378
3520.862154	1157293.138111	41.145383
3520.756812	1156994.229682	41.150388
3521.006897	1156695.434925	41.155392
3521.207764	1156361.720006	41.160397
3521.507919	1156038.375397	41.165402
3521.166636	1155718.144465	41.170407
3521.445934	1155407.443890	41.175412
3521.393625	1155057.601117	41.180416
3521.664047	1154718.187023	41.185421
3521.385949	1154403.544057	41.190426
3521.312143	1154060.453028	41.195431
3521.525250	1153717.671013	41.200436
3521.615643	1153396.091713	41.205440
3521.927828	1153047.001880	41.210445
3521.721902	1152703.086778	41.215450
3521.434660	1152355.564655	41.220455
3521.913436	1151993.311294	41.225460
3521.795853	1151662.948981	41.230464
3521.676278	1151319.592188	41.235469
3521.905027	1150964.222474	41.240474
3521.819352	1150614.279299	41.245479
3521.955103	1150254.046605	41.250484
3522.097680	1149897.198354	41.255488
3521.783131	1149517.191488	41.260493
3522.228187	1149171.707131	41.265498
3521.786072	1148821.893186	41.270503
3522.204474	1148437.045226	41.275508
3521.871140	1148075.698731	41.280512
3521.982717	1147722.025048	41.285517
3522.066920	1147361.129469	41.290522
3521.847029	1146998.837619	41.295527
3522.220658	1146622.015733	41.300532
3522.259272	1146238.681450	41.305536
3521.958176	1145884.383905	41.310541
3521.971096	1145522.331635	41.315546
3521.790056	1145163.604928	41.320551
3522.358169	1144778.086438	41.325556
3522.023417	1144409.093389	41.330560
3521.744147	1144056.376556	41.335565
3522.133501	1143676.971313	41.340570
3522.084499	1143301.215185	41.345575
3522.276045	1142911.354615	41.350580
3521.899477	1142553.431552	41.355584
3522.197370	1142182.850973	41.360589
3522.118896	1141788.019124	41.365594
3521.741838	1141411.234101	41.370599
3521.800177	1141036.912478	41.375604
3521.596817	1140680.637085	41.380608
3521.719346	1140295.339853	41.385613
3521.906025	1139936.387896	41.390618
3521.796262	1139561.515186	41.395623
3522.053586	1139172.982052	41.400628
3521.813823	1138802.253508	41.405632
3522.239427	1138427.402288	41.410637
3521.884715	1138056.640545	41.415642
3521.596237	1137670.175858	41.420647
3522.097248	1137286.306633	41.425652
3522.012591	1136904.120424	41.430656
3521.935564	1136513.643314	41.435661
3522.003067	1136130.996509	41.440666
3521.785124	1135772.969072	41.445671
3521.745688	1135374.233661	41.450676
3521.775575	1135003.480197	41.455680
3521.427787	1134631.718050	41.460685
3521.985705	1134256.075439	41.465690
3521.349019	1133847.823073	41.470695
3521.039870	1133473.408118	41.475700
3521.320068	1133106.757048	41.480704
3521.614827	1132740.268373	41.485709
3521.480710	1132366.031713	41.490714
3521.444199	1131982.152807	41.495719
3521.611530	1131598.592850	41.500724
3521.462399	1131232.073381	41.505728
3521.403665	1130834.806750	41.510733
3521.696232	1130440.590106	41.515738
3521.324197	1130068.322675	41.520743
3521.497047	1129689.473431	41.525748
3521.343416	1129330.430878	41.530752
3521.546669	1128919.569745	41.535757
3521.699961	1128528.848445	41.540762
3521.198308	1128182.054943	41.545767
3521.351172	1127806.689513	41.550772
3521.380671	1127417.904736	41.555776
3521.343452	1127023.013864	41.560781
3521.074975	1126665.427980	41.565786
3521.077450	1126293.405936	41.570791
3521.064030	1125909.846659	41.575796
3521.110312	1125536.813084	41.580800
3520.965849	1125149.509379	41.585805
3521.180315	1124763.165402	41.590810
3520.778643	1124392.029129	41.595815
3521.177791	1124016.070852	41.600820
3520.968874	1123647.992394	41.605824
3520.543032	1123252.696096	41.610829
3520.987949	1122880.268095	41.615834
3520.696288	1122514.029338	41.620839
3520.981700	1122144.051950	41.625844
3520.657532	1121770.530609	41.630848
3520.343501	1121391.457760	41.635853
3520.712139	1121018.912654	41.640858
3520.472261	1120644.155820	41.645863
3520.487189	1120271.902698	41.650868
3520.554387	1119914.571410	41.655872
3519.793143	1119550.016939	41.660877
3520.364137	1119165.972396	41.665882
3520.424988	1118819.239986	41.670887
3520.518439	1118445.989391	41.675892
3520.239230	1118085.734390	41.680896
3520.139249	1117710.463180	41.685901
3520.585234	1117329.547835	41.690906
3520.159797	1116962.093151	41.695911
3520.401474	1116597.267741	41.700916
3520.026026	1116245.579153	41.705920
3520.018149	1115881.413424	41.710925
3520.386365	1115501.334327	41.715930
3519.835264	1115137.684262	41.720935
3519.974825	1114762.548575	41.725940
3520.306936	1114403.184931	41.730944
3520.321751	1114030.784107	41.735949
3520.259599	1113663.234212	41.740954
3519.962870	1113299.799156	41.745959
3519.940832	1112926.373967	41.750964
3519.872751	1112567.811847	41.755968
3519.725878	1112196.932124	41.760973
3520.049809	1111833.295587	41.765978
3519.985462	1111447.180800	41.770983
3519.869511	1111081.085048	41.775988
3519.838543	1110720.866813	41.780992
3519.672827	1110352.725684	41.785997
3519.629455	1110000.191279	41.791002
3519.295128	1109670.206806	41.796007
3519.505882	1109285.895804	41.801012
3519.425657	1108921.556142	41.806016
3519.257757	1108565.225300	41.811021
3519.343674	1108210.261124	41.816026
3519.266337	1107847.757700	41.821031
3519.239158	1107507.946749	41.826036
3519.211117	1107150.162410	41.831040
3519.478909	1106780.082034	41.836045
3519.420579	1106426.360946	41.841050
3519.011856	1106086.236605	41.846055
3519.167139	1105713.427232	41.851060
3519.103143	1105364.699683	41.856064
3519.166592	1105019.272049	41.861069
3519.024264	1104658.188595	41.866074
3518.948998	1104316.082442	41.871079
3519.049582	1103954.911881	41.876084
3518.745787	1103605.154527	41.881088
3518.749931	1103259.719484	41.886093
3519.008048	1102884.690821	41.891098
3518.681697	1102540.028654	41.896103
3518.828045	1102197.751640	41.901108
3518.827519	1101839.132262	41.906112
3518.617521	1101499.546019	41.911117
3519.055697	1101162.795143	41.916122
3518.621562	1100800.736748	41.921127
3519.073112	1100433.918981	41.926132
3519.065942	1100101.382080	41.931136
3518.774961	1099756.727609	41.936141
3518.707721	1099403.120982	41.941146
3518.667476	1099058.285042	41.946151
3518.845646	1098698.184450	41.951156
3518.550850	1098339.381170	41.956160
3518.124707	1097990.714847	41.961165
3518.395029	1097659.608098	41.966170
3518.305284	1097322.130904	41.971175
3518.493099	1096966.696635	41.976180
3518.658886	1096613.921594	41.981184
3518.808937	1096263.422539	41.986189
3518.619340	1095915.157573	41.991194
3518.569207	1095569.622386	41.996199
3518.678486	1095224.038894	42.001204
3518.488833	1094880.109606	42.006208
3518.391280	1094525.710557	42.011213
3518.454568	1094168.773121	42.016218
3518.159733	1093826.708665	42.021223
3518.208577	1093465.515351	42.026228
3518.214061	1093135.707251	42.031232
3518.037854	1092794.611231	42.036237
3518.156805	1092443.199880	42.041242
3517.965923	1092123.033280	42.046247
3518.292655	1091772.789100	42.051252
3518.108878	1091430.746682	42.056256
3517.938486	1091075.942522	42.061261
3517.960457	1090744.358112	42.066266
3517.598123	1090402.950767	42.071271
3517.639643	1090062.988106	42.076276
3517.685494	1089724.632014	42.081280
3517.714906	1089393.538657	42.086285
3517.898749	1089066.998552	42.091290
3517.816158	1088730.134613	42.096295
3517.608062	1088387.042044	42.101300
3517.601920	1088051.656593	42.106304
3517.565649	1087718.459577	42.111309
3517.563394	1087384.373979	42.116314
3517.142894	1087056.279137	42.121319
3517.131622	1086708.735154	42.126324
3517.272949	1086386.162570	42.131328
3516.981604	1086075.433216	42.136333
3517.299542	1085761.709723	42.141338
3517.133463	1085430.119472	42.146343
3517.137450	1085084.290785	42.151348
3516.948434	1084760.333887	42.156352
3517.154359	1084450.005111	42.161357
3517.178855	1084114.275868	42.166362
3516.932598	1083783.269758	42.171367
3517.218528	1083463.473093	42.176372
3516.940588	1083129.171551	42.181376
3517.159686	1082793.328825	42.186381
3516.961987	1082472.402588	42.191386
3516.817075	1082167.565242	42.196391
3517.024484	1081837.997028	42.201396
3517.003162	1081515.162564	42.206400
3516.567080	1081179.328278	42.211405
3516.482799	1080874.120756	42.216410
3516.569379	1080560.327611	42.221415
3516.494980	1080243.088181	42.226420
3516.640367	1079919.268084	42.231424
3516.394563	1079600.004095	42.236429
3516.395270	1079280.392876	42.241434
3516.276570	1078967.213779	42.246439
3516.531930	1078644.067803	42.251444
3516.096802	1078331.960297	42.256448
3516.186379	1078028.004889	42.261453
3516.368750	1077726.897566	42.266458
3515.800105	1077417.448029	42.271463
3516.441963	1077102.404446	42.276468
3516.269009	1076788.437162	42.281472
3516.305632	1076473.553034	42.286477
3516.563931	1076151.507510	42.291482
3516.168034	1075850.872216	42.296487
3516.484961	1075537.040479	42.301492
3516.218175	1075230.298764	42.306496
3515.871926	1074907.703214	42.311501
3515.885672	1074595.788569	42.316506
3516.086781	1074300.925703	42.321511
3515.974734	1073989.765777	42.326516
3515.661294	1073673.336887	42.331520
3515.593346	1073364.632240	42.336525
3515.827866	1073076.327817	42.341530
3515.741254	1072781.526554	42.346535
3515.973053	1072455.520001	42.351540
3515.605134	1072154.004129	42.356544
3515.627345	1071844.622267	42.361549
3515.928208	1071539.117881	42.366554
3515.663502	1071252.433654	42.371559
3515.635392	1070956.563270	42.376564
3515.401783	1070649.559250	42.381568
3515.475780	1070324.124765	42.386573
3515.867250	1070036.211294	42.391578
3515.528967	1069745.999155	42.396583
3515.697406	1069439.534185	42.401588
3515.606895	1069136.268026	42.406592
3515.341295	1068833.302427	42.411597
3515.771135	1068534.629413	42.416602
3515.484942	1068254.042962	42.421607
3515.666810	1067922.004359	42.426612
3515.505525	1067621.743923	42.431616
3515.659025	1067331.707757	42.436621
3515.658281	1067037.833789	42.441626
3515.302641	1066726.878518	42.446631
3515.465029	1066417.167224	42.451636
3515.284741	1066122.504164	42.456640
3515.103982	1065842.931612	42.461645
3515.204008	1065536.548556	42.466650
3515.076797	1065239.231330	42.471655
3515.029423	1064952.951736	42.476660
3514.930052	1064658.870458	42.481664
3514.931978	1064354.747386	42.486669
3515.010883	1064062.722217	42.491674
3514.797477	1063772.173491	42.496679
3514.583941	1063494.893202	42.501684
3514.402900	1063221.636660	42.506688
3514.479714	1062929.840452	42.511693
3514.824456	1062621.232920	42.516698
3514.487491	1062358.453068	42.521703
3514.856803	1062079.272387	42.526708
3514.943814	1061781.829144	42.531712
3514.799704	1061502.607482	42.536717
3514.882223	1061221.119452	42.541722
3514.676144	1060935.812406	42.546727
3514.760510	1060635.514839	42.551732
3514.749499	1060344.462778	42.556736
3514.234454	1060050.588764	42.561741
3514.766100	1059761.342901	42.566746
3514.280892	1059505.579229	42.571751
3514.364400	1059234.681985	42.576756
3514.488437	1058940.932506	42.581760
3514.408623	1058659.051231	42.586765
3514.642101	1058370.359532	42.591770
3514.278278	1058073.464657	42.596775
3514.608821	1057808.912357	42.601780
3514.553966	1057524.174537	42.606784
3514.163132	1057238.802766	42.611789
3514.627897	1056965.611106	42.616794
3514.250340	1056693.122916	42.621799
3514.241496	1056409.572883	42.626804
3514.494201	1056124.422994	42.631808
3514.209096	1055843.202665	42.636813
3514.219508	1055568.377981	42.641818
3513.880951	1055305.743787	42.646823
3514.205180	1055020.043051	42.651828
3513.867995	1054735.400589	42.656832
3513.858642	1054460.138335	42.661837
3514.188735	1054197.244862	42.666842
3513.908831	1053923.832447	42.671847
3513.743079	1053635.922996	42.676852
3514.023022	1053357.858081	42.681856
3513.680212	1053089.911612	42.686861
3513.879334	1052813.086329	42.691866
3513.631127	1052540.661134	42.696871
3513.771288	1052270.184106	42.701876
3513.448859	1051998.805433	42.706880
3513.306697	1051740.502934	42.711885
3513.873004	1051473.871813	42.716890
3513.594937	1051222.513278	42.721895
3513.343659	1050942.002488	42.726900
3513.743989	1050682.789413	42.731904
3513.474718	1050420.393903	42.736909
3513.509741	1050151.084884	42.741914
3513.341102	1049887.489617	42.746919
3513.433987	1049614.478073	42.751924
3513.399295	1049361.933386	42.756928
3513.098816	1049092.917647	42.761933
3513.278103	1048820.335262	42.766938
3513.075111	1048575.793205	42.771943
3512.942273	1048324.279062	42.776948
3512.958913	1048061.917677	42.781952
3513.041977	1047792.679062	42.786957
3513.133495	1047537.423969	42.791962
3512.647558	1047303.394933	42.796967
3512.960235	1047040.743347	42.801972
3512.771041	1046794.575624	42.806977
3512.534061	1046558.736214	42.811981
3512.792492	1046288.430077	42.816986
3512.784566	1046032.252998	42.821991
3512.730761	1045780.900059	42.826996
3512.633074	1045544.415141	42.832001
3512.543972	1045291.983555	42.837005
3512.865384	1045022.957441	42.842010
3512.358550	1044778.780724	42.847015
3512.501677	1044534.196437	42.852020
3512.670972	1044281.000155	42.857025
3512.546485	1044044.938690	42.862029
3512.765010	1043807.651455	42.867034
3512.740930	1043556.675841	42.872039
3512.422163	1043291.535507	42.877044
3512.544104	1043034.618921	42.882049
3512.430870	1042807.971369	42.887053
3512.544404	1042568.039701	42.892058
3512.221282	1042333.677405	42.897063
3512.056957	1042083.817845	42.902068
3512.265277	1041835.528499	42.907073
3512.029556	1041587.011268	42.912077
3512.198647	1041343.925049	42.917082
3512.000214	1041107.847512	42.922087
3512.093365	1040883.117061	42.927092
3512.215535	1040645.130646	42.932097
3511.920928	1040402.852898	42.937101
3512.054708	1040164.264013	42.942106
3511.845838	1039936.161705	42.947111
3512.159825	1039687.855682	42.952116
3512.019867	1039454.985236	42.957121
3511.889520	1039206.247501	42.962125
3511.912278	1038982.321955	42.967130
3511.407037	1038742.617080	42.972135
3511.735792	1038523.553903	42.977140
3511.759883	1038294.669031	42.982145
3511.696184	1038048.189301	42.987149
3512.047365	1037824.549882	42.992154
3511.769034	1037608.258457	42.997159
3511.741148	1037353.908522	43.002164
3511.686724	1037116.573923	43.007169
3511.385433	1036898.807921	43.012173
3511.625561	1036674.850445	43.017178
3511.291271	1036452.526261	43.022183
3511.527188	1036214.041338	43.027188
3511.604925	1035981.957023	43.032193
3511.209072	1035770.256997	43.037197
3511.565516	1035539.946474	43.042202
3511.326218	1035331.493367	43.047207
3511.521211	1035097.514648	43.052212
3511.741456	1034862.844641	43.057217
3511.682162	1034635.177677	43.062221
3511.592794	1034400.152136	43.067226
3511.342854	1034184.303626	43.072231
3511.454768	1033952.709790	43.077236
3511.466527	1033732.058740	43.082241
3511.151631	1033511.065632	43.087245
3511.306348	1033269.177491	43.092250
3511.274788	1033041.634457	43.097255
3511.030452	1032831.346452	43.102260
3511.125176	1032620.897878	43.107265
3510.710853	1032394.069048	43.112269
3510.676818	1032182.366725	43.117274
3510.849596	1031976.818045	43.122279
3511.001616	1031745.222760	43.127284
3511.108899	1031532.407575	43.132289
3511.109802	1031329.186942	43.137293
3511.431029	1031110.414443	43.142298
3510.807792	1030880.944277	43.147303
3510.917705	1030646.502359	43.152308
3511.046211	1030438.774057	43.157313
3510.878549	1030237.768668	43.162317
3510.945270	1030009.311101	43.167322
3510.770285	1029813.521137	43.172327
3511.070731	1029588.010070	43.177332
3510.755724	1029354.455556	43.182337
3510.469163	1029147.716145	43.187341
3510.672480	1028949.799602	43.192346
3510.596948	1028734.002068	43.197351
3510.822907	1028507.006686	43.202356
3510.762534	1028297.970612	43.207361
3510.395080	1028103.702385	43.212365
3510.700971	1027890.521984	43.217370
3510.766000	1027686.189460	43.222375
3510.954055	1027478.728849	43.227380
3510.626021	1027256.424483	43.232385
3510.565344	1027059.937878	43.237389
3510.659236	1026828.535908	43.242394
3510.632905	1026629.993697	43.247399
3510.851957	1026400.394527	43.252404
3510.569299	1026180.559454	43.257409
3510.471104	1025992.569507	43.262413
3510.458620	1025791.669382	43.267418
3510.327603	1025581.865015	43.272423
3510.476794	1025360.763582	43.277428
3510.270467	1025159.872706	43.282433
3510.059092	1024957.812293	43.287437
3510.827550	1024755.292410	43.292442
3510.372704	1024555.583984	43.297447
3510.267874	1024354.453620	43.302452
3510.498453	1024135.810869	43.307457
3510.280362	1023925.958791	43.312461
3510.483903	1023721.167830	43.317466
3510.219042	1023522.069911	43.322471
3509.871473	1023320.554581	43.327476
3510.440724	1023127.801476	43.332481
3510.133077	1022922.968577	43.337485
3510.390446	1022718.616943	43.342490
3510.201065	1022507.737327	43.347495
3510.227964	1022302.050855	43.352500
3510.065295	1022095.127327	43.357505
3509.861176	1021899.065077	43.362509
3510.146426	1021706.697835	43.367514
3510.293224	1021517.644442	43.372519
3510.166827	1021320.773257	43.377524
3509.795072	1021127.815420	43.382529
3509.869302	1020926.532522	43.387533
3510.278872	1020719.269979	43.392538
3509.974204	1020518.422858	43.397543
3509.810309	1020317.933401	43.402548
3510.098989	1020120.369663	43.407553
3509.782073	1019926.973428	43.412557
3510.167521	1019736.656517	43.417562
3509.814175	1019537.043545	43.422567
3509.847019	1019335.419323	43.427572
3509.757216	1019146.810155	43.432577
3509.602937	1018947.434518	43.437581
3509.462079	1018748.631814	43.442586
3509.339373	1018568.062713	43.447591
3509.236228	1018397.383018	43.452596
3509.084378	1018203.803175	43.457601
3508.760680	1018007.624609	43.462605
3508.928605	1017835.233333	43.467610
3509.013852	1017671.488371	43.472615
3509.087170	1017486.290575	43.477620
3508.981468	1017306.745774	43.482625
3509.227172	1017128.884534	43.487629
3509.331987	1016937.451285	43.492634
3509.231380	1016760.314901	43.497639
3509.058329	1016593.960150	43.502644
3509.276819	1016413.556824	43.507649
3509.160018	1016241.357712	43.512653
3509.159471	1016035.446069	43.517658
3509.111275	1015857.301756	43.522663
3509.223892	1015688.348888	43.527668
3509.463624	1015498.300770	43.532673
3509.396997	1015336.648864	43.537677
3509.367305	1015135.369684	43.542682
3509.433838	1014966.985339	43.547687
3509.201610	1014768.445260	43.552692
3509.073793	1014587.457763	43.557697
3509.070380	1014417.903194	43.562701
3509.576861	1014236.605723	43.567706
3509.273884	1014049.220154	43.572711
3509.206324	1013860.235624	43.577716
3509.150033	1013690.764979	43.582721
3508.840158	1013497.826076	43.587725
3509.231810	1013312.146991	43.592730
3508.840609	1013148.348780	43.597735
3508.990956	1012976.782793	43.602740
3509.194187	1012806.757110	43.607745
3508.757113	1012617.403153	43.612749
3509.236215	1012438.383737	43.617754
3508.979998	1012268.028877	43.622759
3509.049692	1012084.402481	43.627764
3508.951564	1011918.868638	43.632769
3508.867660	1011732.438565	43.637773
3508.913902	1011552.004907	43.642778
3508.962750	1011381.670156	43.647783
3508.898573	1011192.789866	43.652788
3508.888577	1011032.559690	43.657793
3508.938492	1010842.968692	43.662797
3508.717861	1010664.105339	43.667802
3508.837390	1010501.992387	43.672807
3508.930472	1010337.158022	43.677812
3508.794521	1010149.226407	43.682817
3508.599762	1009974.613083	43.687821
3508.979475	1009812.243073	43.692826
3508.837666	1009639.068510	43.697831
3508.621702	1009480.577645	43.702836
3508.762865	1009303.652681	43.707841
3508.480481	1009138.650722	43.712845
3508.928849	1008965.358271	43.717850
3508.596153	1008805.701192	43.722855
3508.719864	1008628.757939	43.727860
3508.940219	1008443.238297	43.732865
3508.426657	1008281.262998	43.737869
3508.580487	1008093.312361	43.742874
3508.159329	1007923.631097	43.747879
3508.293005	1007772.423672	43.752884
3508.817256	1007615.800258	43.757889
3508.368078	1007437.941731	43.762893
3508.661176	1007266.664590	43.767898
3508.380822	1007114.924335	43.772903
3508.188492	1006921.935334	43.777908
3508.472580	1006762.021595	43.782913
3508.515258	1006626.843730	43.787917
3508.660771	1006441.367878	43.792922
3508.301783	1006265.694298	43.797927
3508.316169	1006107.070724	43.802932
3508.392843	1005959.908878	43.807937
3508.023546	1005790.057669	43.812941
3508.056148	1005611.673206	43.817946
3507.964576	1005454.507717	43.822951
3508.202024	1005310.706814	43.827956
3508.240905	1005157.110524	43.832961
3508.008338	1004993.730049	43.837965
3508.013404	1004815.908650	43.842970
3508.089049	1004660.833654	43.847975
3507.960975	1004518.142874	43.852980
3508.189399	1004359.921415	43.857985
3508.037457	1004185.121881	43.862989
3508.520810	1004039.496954	43.867994
3508.335160	1003871.017168	43.872999
3507.974450	1003711.026002	43.878004
3508.320626	1003554.708555	43.883009
3508.135436	1003399.252723	43.888013
3508.570545	1003221.213042	43.893018
3508.201980	1003061.691321	43.898023
3508.388576	1002912.291257	43.903028
3508.177824	1002742.322322	43.908033
3508.079521	1002581.964051	43.913037
3508.201933	1002417.769450	43.918042
3508.082652	1002265.677765	43.923047
3507.814797	1002100.565022	43.928052
3508.184655	1001939.722148	43.933057
3507.776071	1001779.100245	43.938061
3508.362442	1001624.052531	43.943066
3507.852208	1001484.170777	43.948071
3507.876214	1001315.872353	43.953076
3508.064278	1001145.303070	43.958081
3507.720017	1001011.028041	43.963085
3507.945078	1000848.425845	43.968090
3507.930785	1000700.265978	43.973095
3507.430133	1000533.782988	43.978100
3507.885502	1000390.697282	43.983105
3507.519036	1000259.036621	43.988109
3507.482244	1000106.094472	43.993114
3508.010904	999957.144233	43.998119
3507.957427	999783.750257	44.003124
3507.956560	999629.620960	44.008129
3507.431191	999491.445047	44.013133
3507.842089	999341.913823	44.018138
3507.693852	999191.886501	44.023143
3507.718403	999044.650675	44.028148
3507.842962	998887.656612	44.033153
3507.881093	998722.784472	44.038157
3507.749874	998571.471952	44.043162
3507.654534	998435.049756	44.048167
3507.445951	998276.827609	44.053172
3507.539284	998109.980755	44.058177
3507.462192	997978.901181	44.063181
3507.585258	997826.455546	44.068186
3507.478593	997691.186088	44.073191
3507.383364	997541.203740	44.078196
3507.556336	997406.563255	44.083201
3507.440636	997252.972672	44.088205
3507.656353	997103.219753	44.093210
3507.539361	996954.199568	44.098215
3507.691697	996810.976024	44.103220
3507.647814	996664.858652	44.108225
3507.596317	996527.993682	44.113229
3507.303875	996386.099128	44.118234
3507.314055	996223.399639	44.123239
3507.393519	996067.114323	44.128244
3507.365510	995935.492299	44.133249
3506.590670	995805.549145	44.138253
3506.925822	995657.102448	44.143258
3507.246898	995514.305564	44.148263
3507.210776	995378.969347	44.153268
3507.386353	995228.296611	44.158273
3506.836367	995098.689998	44.163277
3507.082476	994971.482922	44.168282
3507.087115	994836.127052	44.173287
3507.212486	994685.740536	44.178292
3507.296821	994539.060058	44.183297
3506.923357	994424.221982	44.188301
3507.061501	994279.962353	44.193306
3506.953961	994142.756720	44.198311
3506.984185	994013.711995	44.203316
3507.246334	993857.628162	44.208321
3506.984006	993724.336549	44.213325
3507.098936	993578.990796	44.218330
3506.974964	993474.521769	44.223335
3506.812972	993324.438962	44.228340
3507.128964	993178.562479	44.233345
3506.897144	993053.925601	44.238349
3507.105224	992919.660313	44.243354
3506.721515	992777.885547	44.248359
3506.872531	992651.032121	44.253364
3507.190804	992513.132082	44.258369
3506.881430	992366.850325	44.263373
3506.789359	992235.933034	44.268378
3506.558034	992125.899750	44.273383
3506.874152	991986.037373	44.278388
3506.561914	991844.422541	44.283393
3506.604746	991716.201073	44.288397
3506.678393	991575.588518	44.293402
3506.461524	991459.007106	44.298407
3506.610637	991351.041320	44.303412
3507.030111	991212.020471	44.308417
3506.581149	991070.798933	44.313421
3506.689988	990948.400101	44.318426
3506.434312	990823.328173	44.323431
3506.331068	990689.744137	44.328436
3506.526181	990575.124676	44.333441
3506.187224	990457.665144	44.338445
3506.282641	990328.818597	44.343450
3506.242793	990215.791018	44.348455
3506.247964	990088.124225	44.353460
3506.920770	989947.762878	44.358465
3506.586281	989821.901648	44.363469
3506.391247	989709.474784	44.368474
3506.499365	989577.390415	44.373479
3506.134139	989445.185858	44.378484
3506.288267	989326.353716	44.383489
3506.033327	989229.241546	44.388493
3506.320677	989094.092543	44.393498
3506.094985	988985.655876	44.398503
3506.053385	988856.993680	44.403508
3506.452624	988730.987475	44.408513
3506.229394	988607.715015	44.413517
3506.162412	988505.096403	44.418522
3506.274183	988384.788227	44.423527
3506.395454	988275.890658	44.428532
3506.299411	988150.343433	44.433537
3506.167302	988033.385167	44.438541
3506.405887	987908.753161	44.443546
3506.087265	987793.479341	44.448551
3506.157829	987667.991613	44.453556
3506.328139	987529.214601	44.458561
3506.193865	987421.416106	44.463565
3506.232626	987324.515800	44.468570
3506.185582	987198.549216	44.473575
3506.009146	987076.894771	44.478580
3505.907413	986961.275639	44.483585
3505.838770	986834.719065	44.488589
3506.160189	986727.320316	44.493594
3506.022345	986602.721749	44.498599
3505.679212	986504.992095	44.503604
3506.479621	986372.816987	44.508609
3506.038172	986258.117889	44.513613
3505.971555	986143.842736	44.518618
3506.256744	986046.587324	44.523623
3505.916070	985914.101528	44.528628
3506.321906	985780.708868	44.533633
3505.991941	985668.907675	44.538637
3506.161782	985569.711008	44.543642
3506.256964	985447.098568	44.548647
3505.816890	985350.243566	44.553652
3506.166196	985222.801479	44.558657
3505.952730	985102.379966	44.563661
3506.077509	984974.774088	44.568666
3505.916987	984875.717383	44.573671
3506.127165	984763.418992	44.578676
3506.054161	984647.064841	44.583681
3505.389708	984528.267461	44.588685
3505.895404	984428.116999	44.593690
3505.946389	984334.580821	44.598695
3505.531298	984220.129254	44.603700
3506.119295	984085.104862	44.608705
3505.736379	983981.675761	44.613709
3505.396596	983864.177960	44.618714
3505.761683	983754.958599	44.623719
3505.985784	983662.066360	44.628724
3505.841048	983548.240268	44.633729
3505.614658	983431.398377	44.638733
3505.686548	983311.087339	44.643738
3505.220154	983231.581731	44.648743
3505.257748	983112.932178	44.653748
3505.602714	983016.884739	44.658753
3505.875714	982939.401615	44.663757
3505.778952	982822.135291	44.668762
3505.471431	982691.033976	44.673767
3505.649686	982599.010911	44.678772
3505.624978	982508.777676	44.683777
3505.461781	982404.307188	44.688781
3505.281169	982282.453472	44.693786
3505.223873	982175.617418	44.698791
3505.390436	982078.118593	44.703796
3505.225094	981986.044578	44.708801
3505.623915	981883.523050	44.713805
3505.678827	981768.358865	44.718810
3505.836154	981675.054618	44.723815
3505.580318	981547.630166	44.728820
3505.626992	981460.298911	44.733825
3505.324464	981375.856545	44.738829
3505.605019	981255.565519	44.743834
3505.410475	981154.496189	44.748839
3505.295356	981051.653656	44.753844
3505.543418	980959.690379	44.758849
3505.308307	980850.514349	44.763853
3505.551221	980749.365802	44.768858
3505.549297	980646.497336	44.773863
3505.204872	980543.878815	44.778868
3505.396165	980459.536957	44.783873
3505.100321	980347.332762	44.788877
3505.066696	980249.054128	44.793882
3505.259370	980163.926092	44.798887
3505.153587	980055.104365	44.803892
3505.360103	979935.286268	44.808897
3505.025558	979852.976155	44.813901
3505.028993	979784.776692	44.818906
3505.097171	979681.195361	44.823911
3504.586397	979574.873909	44.828916
3505.251073	979481.743434	44.833921
3504.921253	979398.155736	44.838925
3504.987139	979300.332973	44.843930
3505.106417	979218.622983	44.848935
3504.886164	979145.078326	44.853940
3505.152447	979032.364861	44.858945
3504.942283	978945.819251	44.863949
3505.075965	978839.671143	44.868954
3505.106080	978736.274416	44.873959
3505.026204	978636.216636	44.878964
3504.910675	978539.876645	44.883969
3504.653163	978472.486337	44.888973
3504.742760	978378.259882	44.893978
3504.881019	978284.121594	44.898983
3504.788726	978207.123161	44.903988
3504.764710	978102.453357	44.908993
3504.597371	978013.736405	44.913997
3504.982231	977930.400486	44.919002
3504.878714	977843.625155	44.924007
3504.669009	977752.467631	44.929012
3504.942900	977667.093586	44.934017
3504.800328	977585.598892	44.939021
3505.050171	977480.481632	44.944026
3504.703742	977405.078201	44.949031
3504.486380	977321.930363	44.954036
3504.993445	977237.977750	44.959041
3504.772972	977149.744906	44.964045
3504.831298	977067.623238	44.969050
3504.696329	976977.223080	44.974055
3504.655791	976885.828379	44.979060
3504.676433	976789.925278	44.984065
3504.449430	976714.199798	44.989069
3504.639369	976623.740545	44.994074
3504.809952	976521.453800	44.999079
3504.571358	976449.246173	45.004084
3504.741937	976371.788697	45.009089
3504.223463	976288.577675	45.014093
3504.403231	976213.854011	45.019098
3504.902384	976138.294617	45.024103
3504.240899	976049.335292	45.029108
3505.090299	975951.326240	45.034113
3505.002196	975879.086637	45.039117
3504.857732	975788.375952	45.044122
3504.949977	975701.242577	45.049127
3504.914280	975623.417853	45.054132
3504.910979	975508.919425	45.059137
3504.665603	975421.837407	45.064141
3504.899992	975332.621608	45.069146
3504.900349	975257.328326	45.074151
3504.381703	975165.887138	45.079156
3504.421990	975074.841366	45.084161
3504.112051	975004.583014	45.089165
3504.388397	974931.489127	45.094170
3504.484046	974835.932116	45.099175
3504.426205	974766.509444	45.104180
3504.293524	974691.915191	45.109185
3504.495093	974625.968666	45.114189
3504.452903	974538.057387	45.119194
3504.537668	974458.338867	45.124199
3504.421555	974372.686575	45.129204
3504.625200	974275.831052	45.134209
3504.358157	974212.108567	45.139213
3503.945861	974141.465278	45.144218
3504.189681	974068.659161	45.149223
3504.489875	973974.129945	45.154228
3504.378046	973896.685533	45.159233
3504.377579	973841.913291	45.164237
3504.476559	973745.555093	45.169242
3504.762663	973656.695940	45.174247
3504.542389	973575.352590	45.179252
3504.442456	973508.953816	45.184257
3504.380694	973413.790285	45.189261
3504.133906	973352.695926	45.194266
3504.298935	973263.068084	45.199271
3504.281024	973202.716975	45.204276
3504.260085	973133.561906	45.209281
3504.174699	973058.840789	45.214285
3504.287193	972971.075649	45.219290
3504.408817	972892.014046	45.224295
3504.307719	972819.542361	45.229300
3504.532448	972726.668060	45.234305
3504.176219	972655.018935	45.239309
3504.269847	972582.120865	45.244314
3504.032673	972512.993928	45.249319
3504.113825	972445.281210	45.254324
3504.617152	972378.085160	45.259329
3504.104848	972295.989090	45.264333
3504.226054	972202.536350	45.269338
3504.458838	972138.610651	45.274343
3503.875464	972086.461420	45.279348
3504.315651	972002.247503	45.284353
3503.952129	971938.711310	45.289357
3503.931821	971865.333697	45.294362
3504.180640	971770.580960	45.299367
3503.901218	971702.429648	45.304372
3504.192676	971624.398901	45.309377
3503.895257	971559.673468	45.314381
3503.884064	971477.385294	45.319386
3504.057352	971416.396811	45.324391
3504.098028	971353.178956	45.329396
3504.393032	971283.166742	45.334401
3504.380419	971225.240255	45.339405
3504.451362	971134.126869	45.344410
3504.065194	971051.992212	45.349415
3504.159103	970989.446576	45.354420
3503.949981	970907.867836	45.359425
3503.925872	970841.229974	45.364429
3504.261501	970775.314973	45.369434
3504.142855	970707.223219	45.374439
3504.001868	970631.501028	45.379444
3503.744561	970544.542594	45.384449
3503.812414	970490.118556	45.389453
3504.001018	970404.944007	45.394458
3504.270744	970339.915669	45.399463
3504.195552	970283.066530	45.404468
3504.329797	970211.991183	45.409473
3504.112195	970139.015478	45.414477
3504.048573	970042.426135	45.419482
3504.158939	969979.768921	45.424487
3503.630112	969906.058522	45.429492
3504.228898	969841.851229	45.434497
3504.319685	969772.930889	45.439501
3504.026465	969709.358422	45.444506
3504.253291	969642.371683	45.449511
3503.789403	969568.254730	45.454516
3504.235146	969476.270264	45.459521
3504.112288	969412.274917	45.464525
3503.820039	969345.272325	45.469530
3504.220477	969267.387389	45.474535
3503.658334	969205.615587	45.479540
3504.032397	969148.093897	45.484545
3503.958634	969087.121376	45.489549
3504.146188	969025.419937	45.494554
3504.104850	968963.657643	45.499559
3503.861746	968876.084251	45.504564
3504.221565	968789.193376	45.509569
3504.018473	968730.489942	45.514573
3503.840581	968667.572212	45.519578
3504.066225	968593.231206	45.524583
3503.630520	968546.311915	45.529588
3503.809137	968457.977402	45.534593
3503.587004	968387.623486	45.539597
3503.698327	968320.248762	45.544602
3503.830934	968261.778955	45.549607
3503.575595	968217.568563	45.554612
3504.102121	968145.913533	45.559617
3503.533069	968083.837078	45.564621
3503.764764	968030.048100	45.569626
3503.898629	967982.736670	45.574631
3503.806889	967910.788911	45.579636
3503.849110	967825.306514	45.584641
3503.855453	967774.587498	45.589645
3503.906643	967687.926642	45.594650
3503.806675	967628.117915	45.599655
3503.537881	967569.021778	45.604660
3503.956204	967490.816096	45.609665
3503.536933	967441.535072	45.614669
3503.777425	967381.276033	45.619674
3503.705761	967308.632002	45.624679
3503.611275	967255.868706	45.629684
3503.510389	967207.904125	45.634689
3503.682687	967135.021877	45.639693
3503.385001	967060.257639	45.644698
3503.659800	967011.054453	45.649703
3503.438208	966964.380742	45.654708
3503.597339	966900.996459	45.659713
3503.412588	966845.208538	45.664717
3503.471578	966779.391222	45.669722
3503.723948	966704.727622	45.674727
3503.999959	966664.139095	45.679732
3503.660886	966594.272139	45.684737
3503.692287	966541.187755	45.689741
3503.578528	966475.493348	45.694746
3503.732513	966420.233116	45.699751
3503.538602	966363.952361	45.704756
3503.717519	966270.589484	45.709761
3504.079720	966213.725980	45.714765
3503.604386	966172.963925	45.719770
3503.888323	966096.524337	45.724775
3503.665800	966020.558916	45.729780
3503.697785	965959.731689	45.734785
3504.077709	965906.388162	45.739789
3503.686298	965834.169946	45.744794
3503.994431	965776.919257	45.749799
3503.602528	965716.551057	45.754804
3503.773871	965658.831989	45.759809
3503.634979	965579.614697	45.764813
3503.501672	965505.978562	45.769818
3503.602164	965397.530082	45.774823
3503.664548	965219.440149	45.779828
3503.857006	964944.539794	45.784833
3503.357027	964656.319211	45.789837
3503.320215	964256.517388	45.794842
3503.412773	963840.989950	45.799847
3503.114970	963364.353454	45.804852
3503.283232	962810.282333	45.809857
3503.218299	962182.005680	45.814861
3503.037183	961499.181702	45.819866
3503.002856	960727.534830	45.824871
3502.859560	959898.250184	45.829876
3502.929076	958998.992362	45.834881
3502.939788	958033.696579	45.839885
3502.268494	956977.908697	45.844890
3502.532775	955858.026132	45.849895
3502.051957	954690.347202	45.854900
3502.163066	953464.521568	45.859905
3501.806331	952149.679179	45.864909
3501.577665	950748.908466	45.869914
3501.866847	949257.863220	45.874919
3501.220138	947710.609454	45.879924
3501.145051	946069.007536	45.884929
3500.633506	944359.777679	45.889933
3500.363922	942561.556524	45.894938
3500.457848	940691.017129	45.899943
3499.815345	938740.686609	45.904948
3499.746305	936671.968952	45.909953
3499.100856	934557.312577	45.914957
3498.786172	932357.903158	45.919962
3498.754523	930075.184999	45.924967
3498.259018	927710.236363	45.929972
3497.690565	925247.500045	45.934977
3497.456221	922701.791897	45.939981
3497.206974	920082.686011	45.944986
3496.783483	917372.001226	45.949991
3495.980656	914586.603704	45.954996
3495.519103	911713.252668	45.960001
3495.154044	908795.947447	45.965005
3495.099852	905771.757183	45.970010
3494.395620	902631.116085	45.975015
3493.845680	899437.001686	45.980020
3493.649958	896166.968278	45.985025
3492.629741	892820.221726	45.990029
3492.367717	889370.922120	45.995034
3491.981963	885837.159064	46.000039
3491.093755	882251.422073	46.005044
3490.769724	878561.572769	46.010049
3490.233814	874796.771573	46.015053
3489.696366	870930.545558	46.020058
3489.101094	866965.254769	46.025063
3487.977066	862965.074608	46.030068
3487.547727	858874.882489	46.035073
3486.643651	854688.873870	46.040077
3485.725110	850401.153405	46.045082
3485.376661	846068.186403	46.050087
3484.623789	841630.847246	46.055092
3484.015433	837132.646009	46.060097
3483.412421	832544.833701	46.065101
3482.331359	827877.110170	46.070106
3481.487508	823097.862639	46.075111
3480.534882	818255.704947	46.080116
3479.845151	813326.422109	46.085121
3479.040388	808315.319176	46.090125
3478.323377	803236.011992	46.095130
3477.611034	798078.930804	46.100135
3476.564503	792814.718085	46.105140
3475.704385	787452.291939	46.110145
3474.678018	782042.622128	46.115149
3473.706272	776544.150174	46.120154
3472.790746	770944.013502	46.125159
3471.633779	765272.224022	46.130164
3470.651622	759494.352314	46.135169
3469.813589	753672.218719	46.140173
3468.775586	747761.646406	46.145178
3467.848095	741746.468275	46.150183
3466.540183	735654.271876	46.155188
3465.677208	729471.239845	46.160193
3464.639554	723196.745782	46.165197
3463.042141	716857.964709	46.170202
3462.165135	710450.446470	46.175207
3460.803170	703933.214231	46.180212
3460.090408	697330.437200	46.185217
3458.517443	690659.977861	46.190221
3456.961966	683875.205960	46.195226
3456.070140	677019.817919	46.200231
3454.706415	670139.134269	46.205236
3453.390770	663123.886062	46.210241
3452.242654	656039.702210	46.215245
3450.797229	648877.164969	46.220250
3449.451326	641599.677079	46.225255
3447.946942	634290.900287	46.230260
3446.464190	626886.375974	46.235265
3445.050816	619401.502400	46.240269
3443.755650	611831.759415	46.245274
3442.161003	604172.746953	46.250279
3440.522554	596473.796709	46.255284
3439.118240	588651.320037	46.260289
3437.464986	580777.865439	46.265293
3435.955185	572841.325017	46.270298
3434.390175	564769.985598	46.275303
3432.272824	556665.307163	46.280308
3430.754398	548485.988854	46.285313
3429.081587	540214.914212	46.290317
3427.455998	531871.373476	46.295322
3425.682066	523459.570343	46.300327
3423.845283	514981.706600	46.305332
3421.762862	506425.274858	46.310337
3420.185868	497777.290353	46.315341
3417.995315	489058.310571	46.320346
3416.040574	480288.262376	46.325351
3414.196764	471443.809990	46.330356
3412.076295	462531.730076	46.335361
3410.026716	453564.224265	46.340365
3407.733801	444519.084958	46.345370
3405.991667	435382.316089	46.350375
3403.794224	426213.411919	46.355380
3401.362235	416967.497229	46.360385
3399.002028	407669.910881	46.365389
3396.679903	398282.920093	46.370394
3394.658806	388831.357741	46.375399
3391.931884	379337.787771	46.380404
3389.633037	369781.676466	46.385409
3387.052773	360175.263306	46.390413
3384.129136	350522.252222	46.395418
3381.867353	340791.875585	46.400423
3379.025178	331028.603687	46.405428
3376.482571	321206.867418	46.410433
3373.581041	311349.182376	46.415437
3370.791066	301443.494763	46.420442
3368.479212	291470.103555	46.425447
3365.095685	281479.456009	46.430452
3362.029319	271435.119312	46.435457
3359.043197	261342.697217	46.440461
3355.758582	251201.661206	46.445466
3353.004135	241052.700413	46.450471
3349.379768	230852.323286	46.455476
3345.870795	220581.132195	46.460481
3342.821726	210291.535101	46.465485
3338.960313	200016.879135	46.470490
3335.266986	189723.919996	46.475495
3331.402704	179424.747125	46.480500
3327.226782	169087.001631	46.485505
3323.365857	158747.097955	46.490509
3318.728325	148410.766830	46.495514
3314.407380	138067.777718	46.500519
3309.520767	127747.056483	46.505524
3304.828071	117423.808896	46.510529
3299.279805	107135.864824	46.515533
3293.895226	96877.780787	46.520538
3288.333957	86649.124773	46.525543
3281.363466	76472.865511	46.530548
3273.903884	66361.253115	46.535553
3264.826183	56390.433055	46.540557
3249.663398	46657.819581	46.545562
3206.047505	37892.134946	46.550567
3153.610789	29857.562325	46.555572
3104.918384	22478.963660	46.560577
3060.652563	15887.683691	46.565581
3019.990239	10159.268284	46.570586
2983.678754	5307.493793	46.575591
2947.017846	1458.920162	46.580596
2846.362313	352.177905	46.585601
2757.312403	346.060430	46.590605
2731.583195	341.072506	46.595610
2753.260521	344.338219	46.600615
2797.640359	313.002319	46.605620
2841.276989	290.012425	46.610625
2872.099508	304.277244	46.615629
2887.243636	315.511855	46.620634
2889.759511	302.086720	46.625639
2884.940804	318.216949	46.630644
2877.736499	303.168502	46.635649
2870.722115	293.647132	46.640653
2865.434065	286.785606	46.645658
2862.385848	294.819028	46.650663
2859.818197	301.501628	46.655668
2858.077912	302.807323	46.660673
2856.747280	275.806103	46.665677
2854.157261	294.105612	46.670682
2851.575212	303.950363	46.675687
2848.330025	289.038987	46.680692
2845.860950	273.031824	46.685697
2842.672480	272.431502	46.690701
2839.911376	299.104451	46.695706
2836.808019	276.278070	46.700711
2833.595138	280.449153	46.705716
2830.423295	284.491344	46.710721
2827.438226	288.857197	46.715725
2824.066694	281.885045	46.720730
2821.304475	262.798127	46.725735
2817.853519	266.350168	46.730740
2814.489322	265.877775	46.735745
2811.645240	284.419324	46.740749
2808.107530	290.079234	46.745754
2805.064497	275.907692	46.750759
2801.558966	261.867656	46.755764
2798.377339	264.429642	46.760769
2794.998065	272.073627	46.765773
2791.786233	282.937483	46.770778
2788.461158	254.619058	46.775783
2784.954704	267.985794	46.780788
2781.989195	250.037904	46.785793
2778.526317	248.646790	46.790797
2775.017198	267.218847	46.795802
2771.575409	267.960232	46.800807
2768.206277	255.930324	46.805812
2764.699481	251.486528	46.810817
2761.830840	242.843646	46.815821
2758.160373	264.160804	46.820826
2754.827198	267.656951	46.825831
2751.380341	254.172250	46.830836
2747.955435	243.357457	46.835841
2744.953938	247.652443	46.840845
2741.243939	271.551590	46.845850
2738.177706	263.428615	46.850855
2734.401858	245.829709	46.855860
2730.806340	247.694924	46.860865
2727.303895	245.972777	46.865869
2723.880554	251.280414	46.870874
2721.056452	243.371365	46.875879
2717.213252	266.001240	46.880884
2714.022198	254.661459	46.885889
2711.055597	255.205948	46.890893
2707.275273	254.529837	46.895898
2703.639644	250.020302	46.900903
2699.823199	236.939291	46.905908
2696.123293	239.416492	46.910913
2693.383465	259.988422	46.915917
2689.869852	264.559048	46.920922
2686.561750	250.846022	46.925927
2683.290242	247.665457	46.930932
2679.805852	239.122360	46.935937
2676.197850	249.149786	46.940941
2671.967993	267.371916	46.945946
2668.883090	244.659351	46.950951
2665.590716	236.034689	46.955956
2662.273911	244.903011	46.960961
2659.036609	255.523870	46.965965
2654.733527	258.691949	46.970970
2651.508264	227.766372	46.975975
2648.011530	235.977660	46.980980
2645.231576	251.297373	46.985985
2641.653278	234.491869	46.990989
2637.926340	253.473642	46.995994
2634.711798	241.095155	47.000999
2631.256617	238.996014	47.006004
2627.553396	257.758828	47.011009
2623.886866	237.081564	47.016013
2620.594086	229.287430	47.021018
2617.759961	217.428480	47.026023
2613.512579	235.251485	47.031028
2610.028518	237.717897	47.036033
2606.936992	238.484959	47.041037
2602.939949	226.706577	47.046042
2599.743972	228.500742	47.051047
2596.617945	239.995647	47.056052
2592.754421	236.952595	47.061057
2589.716345	220.675416	47.066061
2586.138029	232.466363	47.071066
2582.446395	236.547284	47.076071
2579.023783	235.635474	47.081076
2575.499223	218.208358	47.086081
2572.015685	220.294205	47.091085
2568.570179	227.789456	47.096090
2565.171157	225.212700	47.101095
2561.515446	225.054546	47.106100
2557.945283	232.753649	47.111105
2554.903757	213.401463	47.116109
2551.038230	231.777194	47.121114
2547.729230	232.827553	47.126119
2543.933122	232.417028	47.131124
2540.556560	225.151704	47.136129
2537.376456	218.748152	47.141133
2533.632010	233.267342	47.146138
2530.514808	220.816648	47.151143
2526.907501	228.266284	47.156148
2523.002426	209.280943	47.161153
2519.760125	210.837732	47.166157
2516.004991	229.770397	47.171162
2512.846799	215.332273	47.176167
2509.464410	210.128723	47.181172
2506.043247	206.923996	47.186177
2503.001180	219.624871	47.191181
2498.884656	238.783171	47.196186
2495.330346	217.697063	47.201191
2491.972077	207.436614	47.206196
2488.205170	206.748439	47.211201
2484.512705	220.899782	47.216205
2481.334070	215.406847	47.221210
2478.038013	215.136845	47.226215
2474.203633	228.857616	47.231220
2470.565312	223.726274	47.236225
2467.901441	211.694903	47.241229
2464.413830	208.716802	47.246234
2461.016801	194.634579	47.251239
2456.996823	212.263559	47.256244
2453.533114	223.890534	47.261249
2450.340768	220.051562	47.266253
2446.693141	212.640698	47.271258
2443.293187	213.515607	47.276263
2439.864516	202.708347	47.281268
2435.575117	200.321496	47.286273
2432.376166	199.749912	47.291277
2429.042967	216.345252	47.296282
2425.659935	199.024837	47.301287
2422.136604	207.246202	47.306292
2418.690326	213.263071	47.311297
2415.366275	205.195232	47.316301
2411.677371	216.925249	47.321306
2408.250306	209.013495	47.326311
2404.458228	204.333520	47.331316
2401.207922	206.872449	47.336321
2397.752089	203.184882	47.341325
2394.041965	223.960912	47.346330
2390.774614	204.286600	47.351335
2386.983196	202.947486	47.356340
2383.449003	199.917721	47.361345
2380.392283	191.777903	47.366349
2376.684016	211.149146	47.371354
2373.416913	205.235516	47.376359
2369.767837	211.757096	47.381364
2366.336506	211.148494	47.386369
2363.234410	190.867989	47.391373
2359.263525	201.119203	47.396378
2355.603539	207.112049	47.401383
2352.266717	207.634371	47.406388
2348.570318	204.039378	47.411393
2345.313615	202.651857	47.416397
2341.436412	212.303531	47.421402
2338.535048	185.132927	47.426407
2334.941051	189.361798	47.431412
2331.292391	207.634820	47.436417
2327.574854	202.841479	47.441421
2324.073137	188.831953	47.446426
2320.651694	197.768622	47.451431
2317.180514	204.383997	47.456436
2313.820478	193.068699	47.461441
2310.645983	191.921561	47.466445
2306.479704	204.515682	47.471450
2303.608607	199.732606	47.476455
2299.827278	203.376918	47.481460
2296.540199	195.473714	47.486465
2292.837093	177.629887	47.491469
2289.154746	193.794116	47.496474
2286.075124	204.821724	47.501479
2282.151561	199.149489	47.506484
2278.365984	181.178498	47.511489
2275.107282	183.905996	47.516493
2271.518631	202.951716	47.521498
2268.169520	207.993252	47.526503
2265.333930	200.486452	47.531508
2261.593291	186.999258	47.536513
2258.113029	177.660932	47.541517
2254.077243	190.610087	47.546522
2250.814611	175.838679	47.551527
2247.506221	180.391795	47.556532
2243.760322	185.849672	47.561537
2240.608606	177.022330	47.566541
2236.945863	196.214633	47.571546
2233.590908	199.328651	47.576551
2229.854748	189.120429	47.581556
2226.357037	198.469439	47.586561
2223.087428	196.786675	47.591565
2219.425445	200.148341	47.596570
2215.812873	182.032156	47.601575
2212.068908	187.707940	47.606580
2208.873341	196.781313	47.611585
2205.359641	189.401285	47.616589
2201.765322	195.944971	47.621594
2198.555433	179.411699	47.626599
2194.983997	202.613843	47.631604
2191.300075	196.401490	47.636609
2187.880093	173.792951	47.641613
2184.240618	188.115757	47.646618
2180.810042	180.220998	47.651623
2177.493693	172.328220	47.656628
2173.986701	181.549836	47.661633
2170.964436	182.470885	47.666637
2166.904768	193.810513	47.671642
2163.326844	189.206531	47.676647
2159.978660	174.821492	47.681652
2156.567853	178.912596	47.686657
2152.971256	183.549789	47.691661
2149.140205	189.782831	47.696666
2145.695124	180.604988	47.701671
2142.283006	175.606107	47.706676
2138.770085	186.009742	47.711681
2135.535915	173.175223	47.716685
2131.834353	181.663136	47.721690
2128.420157	176.038678	47.726695
2124.890106	177.905496	47.731700
2121.246574	183.195016	47.736705
2117.719337	187.449667	47.741709
2114.276540	187.818418	47.746714
2111.238139	186.846907	47.751719
2107.551547	191.609452	47.756724
2103.787425	179.969301	47.761729
2100.018889	192.444129	47.766733
2096.672499	189.764219	47.771738
2093.505605	179.851258	47.776743
2089.949492	183.395281	47.781748
2086.159644	195.564269	47.786753
2082.944648	191.247216	47.791757
2079.184115	173.454743	47.796762
2076.306527	167.153261	47.801767
2072.073110	188.557332	47.806772
2068.596811	199.937997	47.811777
2065.560718	175.583462	47.816781
2062.071529	174.992243	47.821786
2058.482473	176.073123	47.826791
2055.004258	185.674277	47.831796
2051.142440	180.831797	47.836801
2047.752717	171.747280	47.841805
2044.211681	184.715820	47.846810
2041.068289	171.960985	47.851815
2037.656978	173.775505	47.856820
2033.635178	193.668112	47.861825
2030.574829	174.270275	47.866829
2026.649287	162.368070	47.871834
2023.429741	165.952090	47.876839
2020.181080	187.547782	47.881844
2016.344130	184.937688	47.886849
2013.105095	180.225997	47.891853
2009.159953	166.382466	47.896858
2005.442348	191.411063	47.901863
2002.409808	182.205001	47.906868
1998.682368	182.176644	47.911873
1995.387845	178.239433	47.916877
1992.031362	178.173265	47.921882
1988.199139	179.575244	47.926887
1985.229578	177.763781	47.931892
1981.727381	168.564386	47.936897
1978.236668	171.477266	47.941901
1974.075449	160.185349	47.946906
1970.575618	166.031278	47.951911
1967.078421	188.746805	47.956916
1963.740460	177.374709	47.961921
1960.750861	163.359769	47.966925
1957.147625	165.228872	47.971930
1953.344056	177.934048	47.976935
1949.816670	184.991111	47.981940
1945.962978	182.755823	47.986945
1942.939102	174.781773	47.991949
1939.344789	153.837401	47.996954
1935.827165	155.953808	48.001959
1932.695402	176.493126	48.006964
1928.813344	165.781601	48.011969
1925.465027	153.237730	48.016973
1922.045347	156.117210	48.021978
1918.374700	172.395419	48.026983
1914.796890	163.719047	48.031988
1911.273459	167.795094	48.036993
1907.767080	152.613402	48.041997
1904.470682	165.248233	48.047002
1901.105097	177.415748	48.052007
1897.494534	165.456235	48.057012
1893.575297	147.577154	48.062017
1890.184077	156.244299	48.067021
1886.783398	176.090494	48.072026
1883.460111	170.184324	48.077031
1880.094073	176.913323	48.082036
1876.395980	162.044616	48.087041
1873.095205	160.627790	48.092045
1869.222183	168.811352	48.097050
1866.035298	171.446967	48.102055
1862.360972	157.150265	48.107060
1858.534227	167.355297	48.112065
1855.469253	163.700798	48.117069
1851.761430	166.227533	48.122074
1848.470275	178.467822	48.127079
1845.110604	181.484327	48.132084
1841.210042	164.717998	48.137089
1837.594130	151.422137	48.142093
1834.080138	175.103848	48.147098
1830.762910	154.693793	48.152103
1827.232924	158.715516	48.157108
1823.745036	177.169684	48.162113
1820.462124	162.753084	48.167117
1816.581461	160.099316	48.172122
1813.432862	155.607891	48.177127
1809.942542	167.536366	48.182132
1806.287720	175.394325	48.187137
1803.024807	155.615753	48.192141
1799.293946	170.965492	48.197146
1795.668052	173.810888	48.202151
1792.510593	161.551768	48.207156
1788.874309	165.887782	48.212161
1785.534855	156.386428	48.217165
1781.682009	166.449601	48.222170
1778.354992	155.988421	48.227175
1774.876968	164.113854	48.232180
1771.340420	176.771492	48.237185
1767.836869	160.546306	48.242189
1764.393375	151.739453	48.247194
1760.930304	155.817935	48.252199
1757.325353	172.140404	48.257204
1753.814825	166.250696	48.262209
1750.371971	164.658593	48.267213
1746.296512	168.317263	48.272218
1743.075400	156.066705	48.277223
1739.708792	162.270544	48.282228
1736.158527	170.819378	48.287233
1732.880366	168.795848	48.292237
1729.261446	141.185196	48.297242
1725.721374	143.588919	48.302247
1722.180514	160.755303	48.307252
1718.787065	162.093308	48.312257
1715.292365	145.161574	48.317261
1711.515682	141.567464	48.322266
1708.204855	144.441309	48.327271
1704.932453	143.566493	48.332276
1701.322873	154.653180	48.337281
1698.076479	157.490553	48.342285
1694.239324	162.903947	48.347290
1690.819788	153.770208	48.352295
1687.314011	145.774113	48.357300
1683.403067	166.194826	48.362305
1680.543698	162.613417	48.367309
1676.541151	168.322732	48.372314
1673.176507	150.806771	48.377319
1669.501776	144.519336	48.382324
1666.051166	162.176715	48.387329
1662.841071	164.047674	48.392333
1659.501186	163.044623	48.397338
1655.936301	145.216255	48.402343
1652.467691	144.836600	48.407348
1648.675636	160.589691	48.412353
1645.288141	154.181572	48.417357
1641.685685	145.952074	48.422362
1638.175345	137.404532	48.427367
1634.243002	163.801247	48.432372
1631.045009	174.341908	48.437377
1627.803770	154.993931	48.442381
1624.095129	141.685108	48.447386
1620.463525	147.716185	48.452391
1617.000101	160.532460	48.457396
1613.520992	158.092411	48.462401
1610.166766	154.370045	48.467405
1606.484782	157.987928	48.472410
1603.244313	137.740288	48.477415
1599.714394	152.495021	48.482420
1596.103555	177.156664	48.487425
1593.083826	160.377749	48.492429
1589.125298	151.383423	48.497434
1585.817871	165.099290	48.502439
1582.053045	135.864431	48.507444
1578.504129	163.351280	48.512449
1575.329606	164.473980	48.517453
1571.299240	165.298535	48.522458
1568.088336	141.979356	48.527463
1564.479162	148.837572	48.532468
1561.228874	168.860464	48.537473
1557.942242	168.395776	48.542477
1553.999166	148.999920	48.547482
1550.594543	138.286130	48.552487
1547.046110	161.341533	48.557492
1543.236303	165.323048	48.562497
1540.488531	142.191146	48.567501
1536.822519	156.381209	48.572506
1533.212178	161.483699	48.577511
1529.723723	161.996592	48.582516
1525.990261	155.685486	48.587521
1522.637729	140.543777	48.592525
1519.110666	149.688146	48.597530
1515.254363	147.897848	48.602535
1512.202775	141.297844	48.607540
1508.498449	156.707020	48.612545
1505.093863	151.106276	48.617549
1501.495814	161.378281	48.622554
1498.382592	145.921958	48.627559
1494.630946	141.331440	48.632564
1490.972763	159.765353	48.637569
1487.466964	143.346111	48.642573
1483.892894	137.868944	48.647578
1480.907882	150.540210	48.652583
1477.602866	149.630733	48.657588
1473.436947	151.529894	48.662593
1470.098944	143.318610	48.667597
1466.152679	156.557126	48.672602
1462.913859	160.832527	48.677607
1459.824603	140.674063	48.682612
1456.029545	145.592904	48.687617
1452.728929	142.172516	48.692621
1448.800253	147.049588	48.697626
1444.980774	161.868447	48.702631
1442.224832	152.714807	48.707636
1438.366664	153.188142	48.712641
1435.173297	129.041486	48.717645
1431.636907	146.862428	48.722650
1428.060014	157.006277	48.727655
1424.833126	142.311681	48.732660
1421.230561	155.976964	48.737665
1417.400458	139.966628	48.742669
1413.655739	137.424229	48.747674
1410.371625	143.505772	48.752679
1407.171787	145.457617	48.757684
1403.662797	153.662784	48.762689
1400.098911	144.217937	48.767693
1396.420691	127.022857	48.772698
1393.250820	127.248159	48.777703
1389.584613	143.011532	48.782708
1385.729866	148.626553	48.787713
1382.025018	132.951302	48.792717
1378.862071	154.537874	48.797722
1375.552402	130.852101	48.802727
1372.247023	135.767301	48.807732
1368.540647	152.122993	48.812737
1364.985302	156.388134	48.817741
1361.600153	146.548022	48.822746
1357.633251	135.920348	48.827751
1354.450302	130.446671	48.832756
1350.601628	161.560405	48.837761
1347.640899	155.753705	48.842765
1344.094533	138.996289	48.847770
1340.721823	138.828836	48.852775
1337.120471	138.409592	48.857780
1333.170326	136.204291	48.862785
1329.990030	123.187678	48.867789
1326.032760	146.337428	48.872794
1322.981457	140.406899	48.877799
1319.744117	138.712733	48.882804
1315.939529	142.529838	48.887809
1312.678366	154.761784	48.892813
1308.562343	145.750139	48.897818
1305.293377	133.406150	48.902823
1301.868917	134.970437	48.907828
1298.179575	151.049002	48.912833
1295.283836	141.240807	48.917837
1291.729806	138.398778	48.922842
1287.855054	130.462546	48.927847
1284.377016	145.585158	48.932852
1280.391343	148.465523	48.937857
1277.340255	147.092510	48.942861
1273.821106	118.323756	48.947866
1270.469427	147.336915	48.952871
1267.282762	154.514294	48.957876
1263.428214	141.061308	48.962881
1260.238915	135.371207	48.967885
1256.709537	142.479873	48.972890
1252.393498	151.221492	48.977895
1249.347602	137.642041	48.982900
1245.600598	155.879880	48.987905
1242.314374	150.849755	48.992909
1238.849974	149.626467	48.997914
1235.367387	148.639485	49.002919
1231.781886	137.235223	49.007924
1228.475605	152.208172	49.012929
1225.111927	144.884951	49.017933
1221.318081	142.477335	49.022938
1217.668397	142.959387	49.027943
1214.376068	124.887488	49.032948
1210.604020	127.590868	49.037953
1207.541822	137.224956	49.042957
1203.588740	153.549125	49.047962
1200.007485	143.116549	49.052967
1197.200685	125.184892	49.057972
1193.129262	143.331473	49.062977
1189.619375	134.017041	49.067981
1186.261640	148.548759	49.072986
1183.131847	141.213392	49.077991
1179.697141	116.279027	49.082996
1175.654940	145.740012	49.088001
1172.188366	141.739692	49.093005
1168.739956	137.973032	49.098010
1165.574629	144.755588	49.103015
1162.332980	124.348950	49.108020
1158.224841	130.931617	49.113025
1154.954055	132.852669	49.118029
1151.161988	154.135437	49.123034
1147.376018	131.177758	49.128039
1144.098225	120.068430	49.133044
1140.619120	141.054775	49.138049
1137.588613	151.433189	49.143053
1133.780659	133.294440	49.148058
1130.182572	130.010040	49.153063
1127.049127	122.557925	49.158068
1123.083241	138.410223	49.163073
1119.693602	148.459750	49.168077
1116.374419	140.007920	49.173082
1112.707268	128.760260	49.178087
1109.788170	134.662595	49.183092
1105.452670	148.723623	49.188097
1102.116027	138.446842	49.193101
1098.708009	125.765876	49.198106
1094.992797	118.875737	49.203111
1092.027941	126.254490	49.208116
1088.038387	150.389420	49.213121
1084.894731	130.938921	49.218125
1081.399729	122.168415	49.223130
1077.539749	125.001798	49.228135
1074.394724	131.688995	49.233140
1070.476249	122.961674	49.238145
1067.262854	121.601252	49.243149
1063.377871	145.594820	49.248154
1059.904020	128.881280	49.253159
1056.980383	111.490464	49.258164
1053.257916	123.348012	49.263169
1049.934692	135.764688	49.268173
1046.465785	146.503459	49.273178
1042.507388	135.905970	49.278183
1039.035296	116.349343	49.283188
1035.404111	136.337747	49.288193
1032.149936	146.006851	49.293197
1028.572894	127.225257	49.298202
1025.347687	139.456483	49.303207
1021.773680	143.111670	49.308212
1018.011616	138.664320	49.313217
1014.688401	127.335773	49.318221
1011.093037	122.476777	49.323226
1007.685837	141.261711	49.328231
1004.323760	152.168420	49.333236
1000.444021	135.774760	49.338241
997.220215	115.985499	49.343245
993.717743	126.469884	49.348250
989.998135	136.175398	49.353255
987.017817	133.837309	49.358260
982.845331	138.890909	49.363265
979.748910	137.282451	49.368269
976.134420	129.484175	49.373274
972.385701	129.581805	49.378279
969.420367	137.108065	49.383284
965.672218	120.982547	49.388289
962.103860	128.349520	49.393293
958.426245	124.736043	49.398298
954.783843	130.188367	49.403303
951.588254	121.906527	49.408308
948.211724	132.568026	49.413313
944.683041	120.016685	49.418317
941.532699	135.456509	49.423322
937.479749	140.368667	49.428327
934.138717	117.403515	49.433332
930.178485	130.759668	49.438337
927.088901	141.711177	49.443341
923.661608	143.145408	49.448346
919.854279	125.699923	49.453351
916.764963	107.622940	49.458356
912.922872	130.231249	49.463361
909.530188	136.796045	49.468365
906.013060	127.662427	49.473370
902.401626	122.510206	49.478375
899.015457	113.732796	49.483380
895.371420	134.282300	49.488385
892.064877	136.042861	49.493389
888.688222	132.896048	49.498394
885.322335	129.903323	49.503399
882.139289	122.994595	49.508404
878.057656	121.922346	49.513409
874.106975	119.190241	49.518413
870.877005	129.279484	49.523418
867.297798	138.989196	49.528423
864.062381	127.349908	49.533428
860.602099	124.624038	49.538433
856.991534	127.440328	49.543437
853.102792	115.350296	49.548442
849.881320	123.741902	49.553447
846.957825	127.332470	49.558452
842.968823	136.549937	49.563457
839.680463	128.145666	49.568461
835.872939	139.120561	49.573466
832.339108	140.851010	49.578471
829.407675	123.218345	49.583476
825.456940	129.452720	49.588481
822.201963	127.125044	49.593485
818.818743	142.225055	49.598490
814.535462	136.698281	49.603495
811.316924	121.824163	49.608500
807.726242	121.082541	49.613505
804.429013	120.705596	49.618509
801.016685	114.974745	49.623514
797.342413	134.682980	49.628519
794.042071	127.607323	49.633524
790.473849	124.815466	49.638529
786.849309	124.690664	49.643533
783.514957	128.060660	49.648538
779.656514	140.079588	49.653543
776.815043	131.370227	49.658548
773.304382	108.626075	49.663553
769.318008	111.112937	49.668557
765.849758	124.428655	49.673562
762.116398	124.912141	49.678567
759.094388	122.169294	49.683572
755.547479	132.115698	49.688577
751.896601	124.398939	49.693581
748.275463	115.843511	49.698586
744.497091	128.003803	49.703591
741.301603	122.508059	49.708596
737.546348	125.851206	49.713601
734.742035	118.495490	49.718605
731.210487	110.408158	49.723610
727.616180	124.714310	49.728615
723.972062	114.058847	49.733620
720.187206	123.050983	49.738625
716.873490	123.062318	49.743629
713.286778	104.500888	49.748634
709.480791	105.935123	49.753639
706.455709	124.625752	49.758644
702.653446	137.639760	49.763649
699.454996	107.333311	49.768653
696.069096	99.790753	49.773658
692.166015	125.934744	49.778663
688.852134	105.843240	49.783668
684.936280	115.834318	49.788673
681.572252	115.660829	49.793677
678.419179	122.522042	49.798682
674.644527	126.049246	49.803687
672.002707	127.001809	49.808692
667.897909	110.445443	49.813697
664.249498	111.081274	49.818701
661.047725	132.094054	49.823706
657.307716	130.189958	49.828711
653.886604	119.860037	49.833716
650.174040	112.511627	49.838721
646.714399	119.740632	49.843725
643.288736	129.927092	49.848730
639.568263	132.823201	49.853735
636.069141	109.473530	49.858740
632.705576	112.918753	49.863745
629.256615	114.910710	49.868749
625.931204	133.027720	49.873754
622.261139	120.210316	49.878759
619.221029	111.557334	49.883764
615.379632	119.767215	49.888769
611.814848	109.471415	49.893773
608.102551	124.079526	49.898778
604.558236	136.678680	49.903783
601.372197	122.375330	49.908788
597.831080	113.353007	49.913793
594.444358	105.578821	49.918797
590.888299	117.648593	49.923802
587.191514	125.134904	49.928807
583.741856	121.221795	49.933812
580.119564	111.084273	49.938817
576.667654	117.208470	49.943821
573.248674	127.856112	49.948826
569.685076	124.450922	49.953831
566.536797	104.698432	49.958836
562.766162	105.349474	49.963841
559.512609	106.235715	49.968845
555.608504	111.017250	49.973850
551.900385	117.432958	49.978855
548.575694	126.131952	49.983860
544.685001	124.420807	49.988865
541.806550	106.616530	49.993869
538.359625	97.375954	49.998874
534.877117	113.320107	50.003879
531.208724	107.792701	50.008884
527.666548	98.231775	50.013889
524.213834	119.813906	50.018893
520.525007	130.534751	50.023898
517.219456	122.360204	50.028903
513.625757	114.421673	50.033908
510.543802	116.174321	50.038913
506.782571	121.727577	50.043917
503.112182	123.974379	50.048922
499.390699	130.085632	50.053927
496.413478	114.627236	50.058932
492.546425	116.836095	50.063937
489.253433	101.175145	50.068941
485.942807	93.912374	50.073946
482.036877	105.580675	50.078951
478.890887	111.054931	50.083956
475.069938	118.145512	50.088961
471.414629	111.857782	50.093965
468.146523	115.148521	50.098970
464.477568	108.304093	50.103975
461.184506	116.462168	50.108980
457.751556	107.867140	50.113985
454.244342	101.102865	50.118989
450.726885	118.292814	50.123994
446.741282	114.518997	50.128999
443.559626	103.604840	50.134004
440.217341	104.180362	50.139009
436.777966	102.755487	50.144013
433.101636	105.219145	50.149018
429.498228	103.450755	50.154023
426.115532	116.843712	50.159028
422.332991	119.860205	50.164033
418.988345	109.590389	50.169037
415.858952	115.835593	50.174042
411.890092	113.210955	50.179047
408.417476	101.545059	50.184052
405.145207	120.158710	50.189057
401.828327	104.502872	50.194061
398.383012	103.798330	50.199066
394.362879	118.653486	50.204071
390.718293	115.207920	50.209076
387.665026	122.283301	50.214081
384.118990	136.500857	50.219085
381.016039	118.846976	50.224090
377.169495	112.478637	50.229095
373.600584	110.152749	50.234100
369.739872	111.580039	50.239105
366.171704	97.961958	50.244109
363.187794	109.108768	50.249114
359.630216	131.178141	50.254119
355.808543	118.097406	50.259124
352.220600	108.639365	50.264129
349.103121	112.277469	50.269133
345.969614	100.283823	50.274138
341.727674	127.460902	50.279143
338.450450	109.586004	50.284148
334.635722	103.020573	50.289153
331.302447	125.319015	50.294157
327.886007	124.771520	50.299162
324.710589	119.913794	50.304167
321.325450	101.577520	50.309172
317.723374	116.071453	50.314177
313.861700	117.186718	50.319181
310.461913	110.812485	50.324186
306.537177	99.584568	50.329191
303.437823	108.535462	50.334196
299.948228	113.456408	50.339201
296.787092	130.456728	50.344205
293.403743	118.087791	50.349210
289.255442	132.518300	50.354215
285.962238	121.349898	50.359220
282.487473	107.861150	50.364225
278.882807	103.364886	50.369229
275.138270	117.061437	50.374234
271.875901	122.123014	50.379239
268.454248	117.201140	50.384244
264.940290	127.652807	50.389249
261.047126	108.558749	50.394253
257.955078	99.853398	50.399258
254.850147	112.510198	50.404263
251.080374	116.465640	50.409268
247.333795	111.470309	50.414273
244.040200	116.515057	50.419277
240.848909	104.972956	50.424282
236.891362	124.142116	50.429287
233.196253	107.354764	50.434292
229.793175	106.487573	50.439297
226.242969	107.667634	50.444301
222.778935	113.667040	50.449306
219.619949	124.133074	50.454311
216.017723	112.039574	50.459316
212.217597	117.878677	50.464321
208.518924	118.816637	50.469325
205.146323	101.457049	50.474330
201.720806	112.576359	50.479335
198.548807	106.580453	50.484340
195.116737	104.328340	50.489345
191.718917	111.674885	50.494349
187.888858	109.017890	50.499354
184.121418	103.689566	50.504359
181.006533	115.240930	50.509364
177.338533	113.892838	50.514369
173.817525	109.577542	50.519373
170.565918	115.656896	50.524378
166.587078	103.544676	50.529383
163.749011	95.751228	50.534388
159.719732	125.141185	50.539393
156.152515	112.118709	50.544397
152.750756	111.589008	50.549402
149.097937	109.580946	50.554407
145.992532	101.665952	50.559412
142.329837	120.914471	50.564417
138.955855	115.475289	50.569421
135.432622	95.921693	50.574426
131.582591	103.076045	50.579431
128.432412	115.866044	50.584436
124.828487	111.202051	50.589441
121.007894	114.385866	50.594445
117.723360	111.165766	50.599450
113.807217	109.803670	50.604455
110.732878	93.828205	50.609460
107.355206	113.789011	50.614465
104.109581	106.342695	50.619469
100.772668	108.206022	50.624474
96.551768	112.878379	50.629479
93.266450	106.131915	50.634484
89.499426	110.391019	50.639489
86.127341	103.353981	50.644493
83.169845	89.721713	50.649498
79.197141	103.378899	50.654503
76.060575	96.057818	50.659508
72.068604	117.751462	50.664513
68.428400	107.892766	50.669517
65.292368	96.551273	50.674522
61.566149	107.976710	50.679527
58.430107	119.525798	50.684532
54.573529	104.747172	50.689537
51.406608	94.275823	50.694541
47.870680	99.922197	50.699546
44.074681	109.364943	50.704551
40.752003	98.481347	50.709556
37.298472	102.924142	50.714561
33.548913	110.079110	50.719565
30.533480	98.746316	50.724570
26.717860	115.508413	50.729575
23.287461	99.709722	50.734580
19.490714	105.051287	50.739585
16.144393	108.368482	50.744589
12.766659	79.533702	50.749594
8.889250	119.621331	50.754599
5.887774	106.972467	50.759604
2.595947	89.769756	50.764609