Wed Jun 15 16:47:24 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.021087	119.620634	0.000000
0.888584	110.542258	0.005005
1.174786	109.449043	0.010010
1.124905	111.516352	0.015014
1.461578	91.742488	0.020019
0.390884	94.235271	0.025024
0.750683	84.757420	0.030029
0.543998	82.395889	0.035034
0.078587	65.604492	0.040038
0.158948	63.498962	0.045043
-0.474463	54.774775	0.050048
-0.826023	45.239116	0.055053
-1.082470	34.627403	0.060058
-1.466763	52.977964	0.065062
-1.610850	34.315065	0.070067
-2.022271	21.614209	0.075072
-1.814460	23.711819	0.080077
-2.205843	25.031297	0.085082
-2.791312	4.022393	0.090086
-2.854295	20.197460	0.095091
-3.124869	7.050249	0.100096
-3.594354	-8.340614	0.105101
-3.327333	9.719074	0.110106
-3.823452	3.074954	0.115110
-4.367718	2.019063	0.120115
-4.810884	-5.035587	0.125120
-5.255294	9.593006	0.130125
-5.084835	-8.027944	0.135130
-5.155737	-0.924884	0.140134
-5.425040	-4.178558	0.145139
-6.253724	-19.984729	0.150144
-6.563802	-11.580672	0.155149
-6.766273	-6.904346	0.160154
-6.966691	2.963249	0.165158
-6.699578	-3.069923	0.170163
-7.040595	-11.958695	0.175168
-7.215430	-1.583855	0.180173
-7.480281	-15.729197	0.185178
-8.165017	-0.599336	0.190182
-8.237425	7.829869	0.195187
-8.441624	-5.943155	0.200192
-8.561743	-21.322295	0.205197
-8.430164	-16.434342	0.210202
-9.453010	13.905299	0.215206
-9.640809	3.699140	0.220211
-9.979043	-9.077706	0.225216
-10.114925	-6.637230	0.230221
-9.962361	-1.939082	0.235226
-10.237230	-6.325961	0.240230
-10.273823	-7.147225	0.245235
-11.361445	-7.624433	0.250240
-11.434595	1.611415	0.255245
-11.648010	-8.728705	0.260250
-11.946125	0.720896	0.265254
-11.804584	0.727223	0.270259
-11.565359	-9.034471	0.275264
-12.193902	5.581243	0.280269
-12.821083	-3.571861	0.285274
-13.258693	-12.944011	0.290278
-13.484924	-5.457595	0.295283
-13.490715	1.965561	0.300288
-13.475003	9.051549	0.305293
-13.525278	-13.816755	0.310298
-14.572235	-6.919353	0.315302
-14.796779	5.995438	0.320307
-14.852104	10.891401	0.325312
-15.066712	-2.421401	0.330317
-14.801674	-13.630046	0.335322
-14.839312	-5.841180	0.340326
-15.623446	6.698807	0.345331
-16.205170	0.200530	0.350336
-16.237878	-13.207825	0.355341
-16.448683	-5.783147	0.360346
-16.414481	1.700084	0.365350
-16.534916	10.433360	0.370355
-17.418098	0.348045	0.375360
-17.687822	-0.642636	0.380365
-17.574455	0.543608	0.385370
-18.230980	-5.300025	0.390374
-17.967022	-15.198086	0.395379
-18.302127	-8.109667	0.400384
-19.215762	-3.006261	0.405389
-19.429279	4.382076	0.410394
-19.734592	14.861449	0.415398
-19.640380	-9.521862	0.420403
-19.750207	-10.791992	0.425408
-20.001929	1.809746	0.430413
-19.633005	7.810067	0.435418
-19.876065	7.288083	0.440422
-20.526985	-6.714841	0.445427
-21.026095	-3.960817	0.450432
-21.144522	10.354662	0.455437
-21.194912	-12.015365	0.460442
-22.016067	24.418708	0.465446
-22.636145	10.943653	0.470451
-22.721242	-1.616975	0.475456
-21.945374	-9.175136	0.480461
-22.352665	-5.389759	0.485466
-22.742283	-7.311565	0.490470
-22.973572	-12.254013	0.495475
-23.527921	3.018646	0.500480
-24.188506	-15.472908	0.505485
-24.297162	-29.687254	0.510490
-24.493151	-0.960716	0.515494
-24.326049	5.312567	0.520499
-24.691191	-0.806798	0.525504
-24.678077	-18.836261	0.530509
-24.757375	0.042482	0.535514
-25.654136	11.553374	0.540518
-25.939389	-0.364251	0.545523
-25.968151	-8.893374	0.550528
-26.232267	3.346413	0.555533
-26.296734	-3.118577	0.560538
-26.545659	-3.997279	0.565542
-27.453878	2.543877	0.570547
-27.512051	4.100178	0.575552
-27.992488	6.046270	0.580557
-27.978575	-0.423487	0.585562
-28.203659	-6.457189	0.590566
-28.006616	-12.036155	0.595571
-28.223717	-18.034970	0.600576
-28.153453	-5.500952	0.605581
-28.768762	3.522049	0.610586
-29.023964	-2.206105	0.615590
-28.918603	1.841880	0.620595
-29.367481	7.691283	0.625600
-30.348025	7.324423	0.630605
-30.442731	-9.503586	0.635610
-30.937657	1.639135	0.640614
-30.810967	-7.159827	0.645619
-30.820917	-12.589070	0.650624
-30.811618	7.722460	0.655629
-31.452149	-3.441884	0.660634
-32.129781	-11.059218	0.665638
-32.318044	-10.626691	0.670643
-32.458983	-4.009232	0.675648
-32.276568	0.757276	0.680653
-32.548627	4.617570	0.685658
-32.959158	-1.971734	0.690662
-32.870128	-10.531963	0.695667
-33.661677	5.070112	0.700672
-34.267817	0.228774	0.705677
-34.045761	-20.594029	0.710682
-34.291263	-6.213077	0.715686
-34.218772	-6.952737	0.720691
-34.316287	9.845343	0.725696
-35.291801	0.305115	0.730701
-35.310822	-13.085868	0.735706
-35.645926	2.673474	0.740710
-35.635797	0.019451	0.745715
-35.543174	-2.176286	0.750720
-36.680930	5.244054	0.755725
-37.096951	-8.333164	0.760730
-37.073925	-16.163554	0.765734
-36.896409	-5.897261	0.770739
-37.351158	13.667477	0.775744
-37.645011	-1.149491	0.780749
-37.649603	1.265047	0.785754
-37.738452	1.424865	0.790758
-37.617578	0.792229	0.795763
-38.362566	14.828121	0.800768
-38.972232	-5.392231	0.805773
-38.875365	-12.105339	0.810778
-39.434917	6.340317	0.815782
-39.336156	9.843096	0.820787
-40.112731	-0.708273	0.825792
-40.645786	4.409676	0.830797
-40.608985	0.605381	0.835802
-41.129593	21.338615	0.840806
-40.728757	-3.208325	0.845811
-40.888506	-6.702054	0.850816
-40.989305	3.905092	0.855821
-40.857626	-11.186881	0.860826
-41.544220	-8.998380	0.865830
-41.957945	-4.650352	0.870835
-41.985906	2.847886	0.875840
-42.276403	-5.230378	0.880845
-42.372531	-16.063172	0.885850
-43.690448	2.980224	0.890854
-44.015303	10.575573	0.895859
-44.216081	-0.970997	0.900864
-43.803051	-8.255231	0.905869
-43.997872	0.219451	0.910874
-44.346319	8.449337	0.915878
-44.205149	2.913435	0.920883
-44.074500	-3.600175	0.925888
-44.546453	5.992388	0.930893
-45.220876	-6.726130	0.935898
-45.669327	0.457081	0.940902
-45.843809	13.547870	0.945907
-45.743318	11.869903	0.950912
-46.761312	-1.191746	0.955917
-46.919666	-2.961485	0.960922
-47.372858	10.135511	0.965926
-47.404821	-10.453753	0.970931
-47.178027	0.458515	0.975936
-47.259051	11.113298	0.980941
-47.149821	-0.294121	0.985946
-47.618339	-8.023746	0.990950
-48.063611	-4.370293	0.995955
-48.635640	17.385210	1.000960
-48.960872	8.649782	1.005965
-48.590537	1.882300	1.010970
-49.310689	-11.106934	1.015974
-49.993913	-5.352865	1.020979
-50.101046	9.114137	1.025984
-50.762194	4.083909	1.030989
-50.393524	3.983252	1.035994
-50.492435	-0.390584	1.040998
-50.566434	-19.848232	1.046003
-50.265605	7.514114	1.051008
-51.627868	11.493723	1.056013
-51.802683	-1.714477	1.061018
-51.817423	-9.139016	1.066022
-51.812611	-6.291107	1.071027
-51.807946	2.844083	1.076032
-52.121489	11.516150	1.081037
-53.086092	-12.801852	1.086042
-53.744093	-9.495591	1.091046
-53.690366	-1.287689	1.096051
-53.617061	10.450853	1.101056
-53.981182	-3.181504	1.106061
-53.870601	-16.961946	1.111066
-53.891877	2.432589	1.116070
-53.815566	-2.830589	1.121075
-54.405253	-7.911685	1.126080
-54.753089	-6.639750	1.131085
-54.843258	2.237076	1.136090
-55.849504	4.971142	1.141094
-56.508743	-8.341852	1.146099
-56.437764	13.622448	1.151104
-56.575709	-3.416027	1.156109
-56.605308	1.141371	1.161114
-56.843839	-6.801161	1.166118
-56.873396	0.883383	1.171123
-56.838600	-7.867244	1.176128
-57.328046	2.111247	1.181133
-57.651856	2.737524	1.186138
-58.280319	-1.979872	1.191142
-58.542912	-3.461699	1.196147
-58.454743	1.391703	1.201152
-59.091330	13.138271	1.206157
-58.830512	-8.693779	1.211162
-59.878967	2.495835	1.216166
-60.248566	4.524722	1.221171
-60.063781	-14.133862	1.226176
-60.295346	-3.897818	1.231181
-60.095531	7.970050	1.236186
-60.344147	7.336924	1.241190
-60.283229	-12.907333	1.246195
-60.381228	-3.333176	1.251200
-61.455484	16.643004	1.256205
-61.365429	-7.854534	1.261210
-61.542044	-1.082619	1.266214
-61.955439	4.754112	1.271219
-62.688399	-9.485207	1.276224
-63.115162	-0.305746	1.281229
-63.314139	9.072921	1.286234
-63.824131	-1.173691	1.291238
-63.522624	0.866404	1.296243
-63.565753	-5.352043	1.301248
-63.938288	-0.457027	1.306253
-63.698687	3.781845	1.311258
-63.989772	11.014022	1.316262
-63.880321	15.853061	1.321267
-64.244384	-8.685035	1.326272
-64.884893	1.376424	1.331277
-64.957752	-21.391351	1.336282
-66.016146	-7.851953	1.341286
-66.472663	17.062510	1.346291
-66.737049	2.678562	1.351296
-66.599941	-11.731185	1.356301
-66.509289	-16.711150	1.361306
-66.868849	9.703354	1.366310
-66.733070	10.711390	1.371315
-66.725917	-6.264845	1.376320
-67.311196	-11.573847	1.381325
-67.522725	6.298669	1.386330
-67.808040	-1.584442	1.391334
-68.273219	-13.965638	1.396339
-69.356954	-9.868510	1.401344
-69.056638	-4.124091	1.406349
-69.207245	-8.024168	1.411354
-69.457719	-8.374367	1.416358
-69.863465	-11.862751	1.421363
-70.102441	0.047641	1.426368
-70.147564	14.405257	1.431373
-69.985852	-21.011809	1.436378
-70.006371	-15.846783	1.441382
-70.590739	-3.370005	1.446387
-71.314284	5.523411	1.451392
-71.685987	-6.136359	1.456397
-71.629133	-19.270472	1.461402
-71.638563	-6.015905	1.466406
-71.930105	1.291906	1.471411
-72.786479	15.178411	1.476416
-72.929496	14.783720	1.481421
-73.176457	-15.454801	1.486426
-72.940002	1.510611	1.491430
-73.566605	-16.468360	1.496435
-73.245126	-2.588914	1.501440
-73.796307	5.895935	1.506445
-73.754374	-5.056155	1.511450
-74.475586	-12.443734	1.516454
-74.815230	-6.285973	1.521459
-74.865477	8.815875	1.526464
-75.010499	7.311558	1.531469
-74.592137	-17.418079	1.536474
-75.849013	-8.465134	1.541478
-76.548740	12.881667	1.546483
-76.458190	1.028304	1.551488
-76.749747	-2.800241	1.556493
-76.681954	-3.150857	1.561498
-76.731464	-1.929410	1.566502
-76.855470	9.085819	1.571507
-76.785265	-3.536768	1.576512
-77.404823	4.214215	1.581517
-78.090093	-6.865779	1.586522
-78.340469	2.229585	1.591526
-78.334984	-0.730554	1.596531
-78.347410	2.065555	1.601536
-78.695128	15.998600	1.606541
-79.355756	-2.411761	1.611546
-79.558264	-7.760152	1.616550
-79.865012	-20.156081	1.621555
-79.662158	-5.588220	1.626560
-79.872322	0.982874	1.631565
-79.814470	-16.220522	1.636570
-80.434079	-8.695434	1.641574
-81.077075	10.971825	1.646579
-81.120599	-6.448221	1.651584
-81.262517	-5.945422	1.656589
-81.209426	-19.765186	1.661594
-82.090375	3.345043	1.666598
-82.421758	14.879984	1.671603
-82.297811	-10.242541	1.676608
-82.840474	-15.256530	1.681613
-82.829818	-10.415379	1.686618
-82.701162	12.533922	1.691622
-83.399139	10.210103	1.696627
-84.123100	-0.288398	1.701632
-84.605655	5.111914	1.706637
-84.192360	-11.019264	1.711642
-84.512410	-5.799305	1.716646
-84.848623	-14.065420	1.721651
-84.369705	-17.934789	1.726656
-84.496345	-19.515336	1.731661
-85.109013	-5.568806	1.736666
-85.702073	3.245237	1.741670
-86.029596	-7.015445	1.746675
-85.873384	-2.844277	1.751680
-86.498624	2.715254	1.756685
-86.434263	-17.652473	1.761690
-87.236008	-0.902464	1.766694
-87.793562	-6.305616	1.771699
-87.622692	-9.987747	1.776704
-87.922740	-4.110861	1.781709
-87.966827	-5.996452	1.786714
-87.946411	-7.008151	1.791718
-87.856167	-2.131814	1.796723
-87.989260	0.964193	1.801728
-88.972301	0.112717	1.806733
-89.642856	-8.938402	1.811738
-89.442701	13.209525	1.816742
-89.710103	20.683518	1.821747
-89.562730	5.693210	1.826752
-90.137607	-6.319765	1.831757
-90.748461	-4.664328	1.836762
-91.125994	13.000261	1.841766
-91.190678	3.074732	1.846771
-90.822522	-3.084140	1.851776
-91.065998	14.411213	1.856781
-91.054872	-4.753925	1.861786
-91.575352	-16.530551	1.866790
-92.377095	-14.107081	1.871795
-92.280590	-1.490796	1.876800
-92.734308	7.799069	1.881805
-92.468616	-19.578616	1.886810
-93.279882	-11.015575	1.891814
-94.021601	10.243461	1.896819
-93.894408	9.867935	1.901824
-94.303584	3.688382	1.906829
-94.290051	-4.765556	1.911834
-94.179233	10.096005	1.916838
-94.293267	3.786092	1.921843
-94.310127	-10.310358	1.926848
-95.133456	6.650183	1.931853
-95.372990	6.695323	1.936858
-95.548109	7.742411	1.941862
-95.636555	0.317426	1.946867
-95.963270	-2.521222	1.951872
-96.996222	-9.365035	1.956877
-97.351369	10.457561	1.961882
-97.123735	19.992509	1.966886
-97.140394	16.760806	1.971891
-97.393482	-3.816669	1.976896
-97.701336	-11.294659	1.981901
-97.741823	8.172693	1.986906
-97.701012	8.804505	1.991910
-98.708744	8.436527	1.996915
-98.992694	-6.110393	2.006912
-98.421080	5.313924	2.016909
-97.947123	-7.183496	2.026906
-97.019402	-0.788419	2.036902
-96.619346	4.119058	2.046899
-96.451638	8.341733	2.056896
-96.236618	0.305948	2.066893
-95.511639	-2.087542	2.076890
-94.935340	-10.523300	2.086886
-94.163923	6.193064	2.096883
-93.321724	3.533567	2.106880
-93.394165	4.829525	2.116877
-93.325391	12.941782	2.126874
-92.714941	-2.176488	2.136870
-92.145953	8.785226	2.146867
-90.967427	2.661042	2.156864
-90.554337	-4.489198	2.166861
-90.486714	-0.063997	2.176858
-90.309808	-6.893405	2.186854
-89.271984	-2.066545	2.196851
-88.919653	6.484899	2.206848
-88.373841	-6.847659	2.216845
-87.559617	-2.862712	2.226842
-87.539730	-2.471650	2.236838
-87.118987	7.870575	2.246835
-86.220832	-5.388160	2.256832
-86.068822	5.379539	2.266829
-85.048001	8.210373	2.276826
-84.775499	12.473609	2.286822
-84.506846	8.511386	2.296819
-83.859868	6.154690	2.306816
-82.992656	1.782016	2.316813
-82.833159	0.892050	2.326810
-82.846919	-10.044965	2.336806
-81.676578	3.041693	2.346803
-81.349250	-13.767264	2.356800
-81.074136	-3.546665	2.366797
-80.140775	2.753948	2.376794
-79.820642	-5.066402	2.386790
-79.571313	-4.981030	2.396787
-78.977991	2.091679	2.406784
-78.523002	-3.952330	2.416781
-77.413671	-10.538878	2.426778
-76.939479	2.898110	2.436774
-76.845442	-11.917702	2.446771
-76.767074	0.521329	2.456768
-75.654779	-9.580200	2.466765
-75.271149	0.481620	2.476762
-75.142696	-8.961375	2.486758
-74.057317	-3.509147	2.496755
-73.689976	-2.632759	2.506752
-73.431376	2.271924	2.516749
-72.821169	-16.205910	2.526746
-72.007949	3.795307	2.536742
-71.864103	-10.113325	2.546739
-71.627982	-3.419237	2.556736
-70.599434	-0.340578	2.566733
-70.289853	-3.968010	2.576730
-70.033096	-4.571414	2.586726
-69.008097	11.249568	2.596723
-69.036172	0.270363	2.606720
-68.263107	-7.376730	2.616717
-67.454478	9.069578	2.626714
-67.463632	-12.044145	2.636710
-67.226808	8.933186	2.646707
-66.166423	-3.908482	2.656704
-65.961767	10.206583	2.666701
-64.963796	-1.048377	2.676698
-64.443028	11.537415	2.686694
-64.409002	0.735414	2.696691
-64.197240	13.035762	2.706688
-62.966548	-5.362005	2.716685
-62.325592	-6.139431	2.726682
-62.260526	0.901369	2.736678
-62.305610	0.351999	2.746675
-61.311241	0.018813	2.756672
-60.839198	8.472744	2.766669
-60.328357	-6.063693	2.776666
-59.641738	17.622499	2.786662
-59.558434	-2.968904	2.796659
-58.572430	6.201615	2.806656
-57.953869	10.940336	2.816653
-57.887998	0.784570	2.826650
-57.559583	10.838042	2.836646
-56.859595	4.699215	2.846643
-56.567998	0.233910	2.856640
-55.548844	-2.126707	2.866637
-54.989568	-1.502004	2.876634
-54.888720	0.223121	2.886630
-54.538199	4.596138	2.896627
-53.439907	1.870913	2.906624
-53.235454	-1.896291	2.916621
-53.028777	2.790591	2.926618
-51.859784	-8.608981	2.936614
-51.743865	7.036102	2.946611
-51.496265	-7.454063	2.956608
-50.979968	3.981480	2.966605
-50.241852	12.340475	2.976602
-49.932774	11.127398	2.986598
-48.840284	-3.533616	2.996595
-48.448148	-12.017856	3.006592
-48.539557	6.482012	3.016589
-47.935319	-17.198521	3.026586
-46.946055	-1.677238	3.036582
-46.674677	-8.400179	3.046579
-46.645434	0.833345	3.056576
-45.550974	-5.914606	3.066573
-45.334200	-8.841917	3.076570
-44.626369	-3.137644	3.086566
-44.006248	10.182494	3.096563
-43.786303	-14.804297	3.106560
-43.298846	-5.978970	3.116557
-42.845431	7.446253	3.126554
-42.063001	3.689508	3.136550
-41.859463	-8.580100	3.146547
-41.273710	2.814926	3.156544
-40.544010	0.339372	3.166541
-40.464746	-9.325041	3.176538
-39.815240	-7.265677	3.186534
-38.931579	-1.699703	3.196531
-38.570562	-5.508585	3.206528
-38.519003	-4.836220	3.216525
-37.382128	-13.444923	3.226522
-37.270835	3.793714	3.236518
-37.039152	-0.292974	3.246515
-36.096043	-0.718135	3.256512
-35.501372	3.586976	3.266509
-35.293406	-2.275063	3.276506
-35.134764	1.394015	3.286502
-34.116699	-10.306656	3.296499
-33.786544	-10.168463	3.306496
-32.567272	-6.454510	3.316493
-32.578199	-1.876464	3.326490
-32.405681	-6.122272	3.336486
-32.104272	2.417345	3.346483
-31.184805	-12.007646	3.356480
-30.935213	0.893002	3.366477
-29.962395	-11.572781	3.376474
-29.239698	-10.394998	3.386470
-29.240316	-6.093637	3.396467
-29.215997	-1.220755	3.406464
-28.117632	-16.911039	3.416461
-27.578395	12.295162	3.426458
-27.263550	-9.736569	3.436454
-26.385682	6.944445	3.446451
-26.025348	-10.173602	3.456448
-25.884228	-5.193103	3.466445
-25.433523	-9.963729	3.476442
-24.758084	2.115682	3.486438
-24.583040	7.479344	3.496435
-23.435271	1.684618	3.506432
-22.901412	-4.407094	3.516429
-22.850471	-11.102296	3.526426
-22.255375	-6.730584	3.536422
-21.521337	-19.489365	3.546419
-21.427789	-4.115965	3.556416
-20.412354	-15.542303	3.566413
-19.637646	-8.720517	3.576410
-19.763771	-3.488727	3.586406
-19.626616	-5.598385	3.596403
-18.748179	-8.897381	3.606400
-18.147941	4.967511	3.616397
-17.835931	-13.704226	3.626394
-16.868716	-0.625267	3.636390
-16.412468	-18.553281	3.646387
-16.609260	1.367249	3.656384
-15.524821	-8.442939	3.666381
-14.779681	-6.013080	3.676378
-14.694445	-1.374081	3.686374
-14.833646	-0.948430	3.696371
-13.604119	-19.277638	3.706368
-13.258874	4.408371	3.716365
-12.088253	-7.443447	3.726362
-11.973463	-4.107093	3.736358
-11.494190	-7.673871	3.746355
-11.368889	-2.680483	3.756352
-10.936823	-5.683969	3.766349
-10.225842	-18.277646	3.776346
-9.830061	4.930355	3.786342
-8.535826	-7.494519	3.796339
-8.522987	-3.443099	3.806336
-8.186230	-15.788848	3.816333
-8.051157	3.491621	3.826330
-6.859517	-11.383315	3.836326
-6.616452	-2.922159	3.846323
-6.511749	-2.837279	3.856320
-5.982676	-7.991053	3.866317
-5.431531	-7.263464	3.876314
-4.484570	-3.028521	3.886310
-4.308527	5.009120	3.896307
-3.886376	16.097452	3.906304
-3.318511	24.747728	3.916301
-3.113748	30.191432	3.926298
-2.631719	48.060754	3.936294
-1.902014	53.503745	3.946291
-1.325033	82.878582	3.956288
-0.666990	71.273301	3.966285
-0.590867	92.288187	3.976282
0.117958	101.569084	3.986278
0.000000	109.005525	3.991283
0.213010	135.157052	3.996288
0.614300	125.070972	4.001293
0.408766	122.881481	4.006298
0.604554	128.833028	4.011302
1.084575	161.013626	4.016307
1.222564	174.720064	4.021312
1.205233	171.212028	4.026317
1.154444	163.800461	4.031322
1.568852	156.511975	4.036326
1.413340	148.770191	4.041331
1.014373	129.641169	4.046336
1.227807	139.188121	4.051341
0.911081	157.963560	4.056346
1.211409	149.834522	4.061350
1.267665	159.349261	4.066355
1.003340	165.458540	4.071360
1.344395	147.665489	4.076365
0.992327	166.669818	4.081370
1.473533	165.128578	4.086374
1.435845	173.627009	4.091379
1.311559	169.657918	4.096384
1.112442	162.215031	4.101389
1.148092	159.847374	4.106394
1.085885	152.814528	4.111398
1.129365	171.469295	4.116403
1.264784	164.485858	4.121408
1.245330	162.278335	4.126413
1.199186	181.033253	4.131418
1.527471	174.287539	4.136422
1.342723	169.975582	4.141427
1.254164	162.321668	4.146432
1.395348	164.483084	4.151437
1.354279	173.952459	4.156442
1.279869	163.378639	4.161446
1.730460	167.038560	4.166451
1.303731	183.905743	4.171456
1.429741	180.322523	4.176461
1.394196	179.826412	4.181466
1.331721	169.687126	4.186470
1.492735	174.050311	4.191475
1.593275	194.052754	4.196480
1.746747	191.644610	4.201485
1.628198	171.319764	4.206490
1.819325	179.866108	4.211494
1.689100	181.063917	4.216499
1.678245	178.917315	4.221504
1.787948	176.096863	4.226509
1.318817	187.286850	4.231514
1.686597	166.357728	4.236518
1.654060	167.369424	4.241523
1.443262	173.472622	4.246528
1.687050	164.807011	4.251533
1.537017	182.608815	4.256538
1.705691	198.991515	4.261542
1.878829	197.437655	4.266547
1.948235	172.660405	4.271552
2.060487	165.658304	4.276557
1.791612	168.761692	4.281562
1.732804	158.493764	4.286566
1.508720	176.427160	4.291571
1.657141	169.858255	4.296576
2.216117	175.645431	4.301581
1.809801	168.924546	4.306586
2.012322	173.935193	4.311590
1.821726	183.592348	4.316595
1.517347	175.357652	4.321600
1.739844	174.047777	4.326605
1.789651	190.139968	4.331610
1.893751	200.917591	4.336614
1.779642	202.281226	4.341619
1.922778	199.889191	4.346624
2.429509	185.540092	4.351629
2.094682	201.406727	4.356634
2.102897	193.675249	4.361638
2.056262	174.541707	4.366643
2.135457	162.070192	4.371648
2.044764	166.589501	4.376653
1.489552	184.323022	4.381658
1.963467	180.422176	4.386662
1.846250	202.779107	4.391667
1.981389	206.438295	4.396672
2.234699	194.840498	4.401677
1.908453	190.681047	4.406682
2.486453	188.080226	4.411686
2.185619	193.309604	4.416691
2.084547	201.421079	4.421696
2.485560	191.122911	4.426701
1.852330	178.280819	4.431706
1.947233	171.703691	4.436710
2.004985	185.975228	4.441715
2.072816	207.325477	4.446720
2.487954	212.663724	4.451725
1.880870	213.844654	4.456730
2.121894	189.571509	4.461734
2.154978	197.797733	4.466739
1.821587	201.591070	4.471744
2.071711	186.839382	4.476749
2.187149	191.293658	4.481754
2.375712	191.592100	4.486758
2.391420	219.439782	4.491763
2.138410	201.378544	4.496768
2.509561	182.048300	4.501773
2.367047	205.696457	4.506778
2.293031	222.622709	4.511782
2.558518	209.497489	4.516787
2.138250	193.901388	4.521792
2.332539	206.277574	4.526797
2.548480	193.830490	4.531802
2.420601	204.244763	4.536806
2.280594	211.003918	4.541811
2.342229	208.218038	4.546816
2.605944	216.614623	4.551821
2.333222	213.413921	4.556826
2.426212	195.366659	4.561830
2.246891	196.879867	4.566835
2.191459	215.021400	4.571840
2.018152	209.018511	4.576845
2.146506	220.083862	4.581850
2.502341	206.719292	4.586854
2.543360	225.271667	4.591859
2.420518	228.692745	4.596864
2.963881	230.681957	4.601869
2.641613	250.505561	4.606874
2.747847	241.448322	4.611878
2.919484	223.970145	4.616883
2.814904	202.275187	4.621888
2.487101	208.776440	4.626893
2.521433	225.647797	4.631898
2.502606	198.224262	4.636902
2.606688	203.919912	4.641907
2.885639	228.185650	4.646912
2.682674	218.906567	4.651917
2.358002	216.192789	4.656922
2.714209	210.247600	4.661926
2.702911	222.820665	4.666931
2.663119	239.614889	4.671936
2.911541	214.352016	4.676941
2.675968	228.616752	4.681946
2.538112	231.478320	4.686950
2.934529	217.929198	4.691955
2.724311	221.555497	4.696960
3.056606	225.660445	4.701965
2.487408	227.863508	4.706970
2.633765	238.152975	4.711974
2.767266	225.137275	4.716979
2.780646	213.728738	4.721984
3.011022	222.833003	4.726989
2.733932	233.272941	4.731994
2.855818	223.487874	4.736998
2.831558	228.880295	4.742003
2.605117	248.467387	4.747008
2.925461	223.106125	4.752013
2.462124	220.404336	4.757018
2.391709	237.619119	4.762022
3.082342	265.511578	4.767027
2.752615	263.750594	4.772032
3.199800	244.481396	4.777037
3.028421	266.206659	4.782042
3.127556	279.399348	4.787046
3.313330	273.389177	4.792051
2.979966	256.703890	4.797056
3.073664	246.526610	4.802061
2.703005	272.621137	4.807066
3.087298	289.574489	4.812070
2.957730	272.853432	4.817075
2.773677	267.486301	4.822080
3.217246	263.274385	4.827085
2.744191	281.042382	4.832090
2.860056	279.103883	4.837094
2.983799	255.968378	4.842099
2.708850	261.887287	4.847104
2.885397	270.814798	4.852109
2.596462	293.773478	4.857114
3.161244	293.961708	4.862118
3.394440	278.039814	4.867123
3.352784	298.296729	4.872128
3.555207	293.242749	4.877133
3.505572	302.599978	4.882138
3.466484	306.193478	4.887142
3.198425	282.195694	4.892147
3.430687	278.863902	4.897152
3.384741	262.197795	4.902157
3.219547	276.786222	4.907162
3.346993	281.246924	4.912166
3.402116	260.551840	4.917171
3.291335	266.131402	4.922176
3.528810	268.630175	4.927181
3.381992	289.859953	4.932186
3.434184	270.410860	4.937190
3.692569	249.850097	4.942195
3.263514	265.764135	4.947200
3.607589	274.370980	4.952205
3.329936	287.897619	4.957210
3.208055	256.655829	4.962214
3.486438	282.422637	4.967219
3.580693	299.178102	4.972224
3.714049	286.383245	4.977229
3.354740	272.610348	4.982234
3.427411	280.242432	4.987238
3.718581	302.598507	4.992243
3.323292	304.707931	4.997248
3.617201	300.564339	5.002253
3.360755	284.513238	5.007258
3.850425	292.509082	5.012262
3.784023	306.516948	5.017267
3.749449	298.802255	5.022272
3.745466	275.387250	5.027277
3.281379	284.673177	5.032282
3.650464	291.147784	5.037286
3.693470	279.231521	5.042291
3.272779	293.967641	5.047296
3.458335	304.250576	5.052301
3.516791	303.409740	5.057306
3.416916	287.036129	5.062310
3.349269	286.966937	5.067315
3.466879	297.390817	5.072320
3.439001	294.856073	5.077325
3.262865	302.396607	5.082330
3.612454	321.168077	5.087334
4.212177	327.808093	5.092339
3.939712	322.615461	5.097344
4.267198	303.999187	5.102349
3.782957	315.721797	5.107354
3.945973	307.157448	5.112358
4.154535	301.104140	5.117363
3.984119	291.994634	5.122368
3.937597	289.291720	5.127373
3.695987	302.802847	5.132378
3.597632	297.857564	5.137382
3.821889	284.943810	5.142387
3.626828	307.749188	5.147392
3.893373	306.434193	5.152397
3.842111	342.840146	5.157402
3.577111	334.960202	5.162406
4.129922	325.193625	5.167411
3.741283	313.393751	5.172416
3.972011	319.732412	5.177421
3.970912	350.376089	5.182426
4.015584	333.382611	5.187430
4.059804	341.338750	5.192435
3.568621	340.912901	5.197440
4.104544	318.739657	5.202445
3.828524	341.604039	5.207450
3.923807	338.283725	5.212454
3.881921	344.521056	5.217459
3.894280	326.358723	5.222464
4.221794	319.192638	5.227469
4.013250	340.713635	5.232474
4.038152	345.054183	5.237478
4.275701	338.822253	5.242483
4.359344	339.410700	5.247488
4.628922	341.483744	5.252493
4.319233	319.893566	5.257498
4.069695	322.109218	5.262502
4.267688	335.900981	5.267507
3.987905	344.351917	5.272512
3.886002	324.026682	5.277517
4.302913	341.373138	5.282522
4.468940	362.409953	5.287526
4.390664	343.004722	5.292531
4.240322	328.703311	5.297536
4.430248	312.252581	5.302541
4.313404	333.722802	5.307546
3.970144	356.613215	5.312550
4.421294	356.245504	5.317555
4.162321	349.128977	5.322560
4.683939	363.321160	5.327565
4.543784	356.892100	5.332570
4.602270	348.980787	5.337574
4.458029	345.550406	5.342579
4.131316	344.646163	5.347584
4.308339	340.402316	5.352589
4.624618	370.374965	5.357594
4.493963	381.800168	5.362598
4.667362	372.191655	5.367603
4.578101	365.918627	5.372608
4.412466	345.413801	5.377613
4.151593	354.905112	5.382618
4.419154	358.118661	5.387622
4.746675	363.075963	5.392627
4.537859	373.194762	5.397632
4.729271	363.753741	5.402637
4.413024	355.930790	5.407642
4.695446	355.146949	5.412646
4.809872	368.161694	5.417651
4.460367	365.711263	5.422656
4.487065	355.835796	5.427661
4.773529	377.024079	5.432666
4.549338	375.317655	5.437670
5.081440	350.317554	5.442675
4.904479	361.021191	5.447680
4.597616	356.541043	5.452685
4.510755	348.546717	5.457690
4.315496	343.234187	5.462694
4.624754	349.999654	5.467699
4.905990	370.808802	5.472704
4.917801	375.189106	5.477709
4.545462	374.128745	5.482714
4.565615	362.676089	5.487718
4.714998	364.552568	5.492723
4.314055	367.880049	5.497728
4.346765	379.546870	5.502733
4.767513	384.695242	5.507738
4.669878	355.987450	5.512742
4.599469	358.187118	5.517747
4.805406	373.033132	5.522752
4.862640	380.109471	5.527757
4.771298	383.374940	5.532762
4.831351	379.793597	5.537766
5.092622	397.328804	5.542771
4.973046	409.526879	5.547776
5.194633	393.319817	5.552781
5.188706	383.386688	5.557786
4.775413	385.948240	5.562790
5.020085	370.842342	5.567795
4.804315	378.725457	5.572800
5.005168	395.209985	5.577805
5.078084	396.086088	5.582810
4.800967	391.555044	5.587814
5.207738	410.858061	5.592819
4.811304	405.117083	5.597824
4.948976	396.001583	5.602829
4.701535	410.363817	5.607834
4.709172	401.271974	5.612838
4.883695	387.407693	5.617843
4.773367	408.582084	5.622848
4.846760	411.290101	5.627853
4.570851	392.477691	5.632858
5.146263	415.202955	5.637862
5.257126	424.038817	5.642867
5.399464	417.752352	5.647872
5.047689	425.124774	5.652877
5.388821	436.600984	5.657882
5.236068	430.101271	5.662886
5.170039	407.784900	5.667891
5.282752	417.008632	5.672896
5.541265	410.307689	5.677901
5.217951	412.231710	5.682906
5.201658	389.270472	5.687910
5.475237	396.777374	5.692915
5.299318	405.582293	5.697920
5.260193	395.502823	5.702925
5.598974	404.794247	5.707930
5.145578	404.899093	5.712934
5.096542	398.979764	5.717939
5.235515	429.401281	5.722944
5.524496	433.368234	5.727949
5.300750	447.268563	5.732954
5.617253	430.609159	5.737958
5.631587	423.821306	5.742963
5.231763	431.517642	5.747968
5.342806	433.055393	5.752973
5.442925	443.482066	5.757978
5.595892	425.881461	5.762982
5.596515	420.391718	5.767987
5.430940	446.728963	5.772992
5.568415	427.057528	5.777997
5.834116	432.772821	5.783002
5.539237	436.632950	5.788006
5.623396	408.662400	5.793011
5.383725	400.076257	5.798016
5.421699	420.369596	5.803021
5.582588	445.044134	5.808026
5.666727	423.169727	5.813030
5.886984	415.044115	5.818035
5.307109	423.192020	5.823040
5.634650	423.333537	5.828045
5.639092	443.028622	5.833050
5.549399	427.191403	5.838054
5.758994	424.684276	5.843059
5.485040	432.281780	5.848064
5.378025	414.272640	5.853069
5.315733	418.860625	5.858074
5.475528	431.780524	5.863078
5.648277	426.032483	5.868083
5.667457	427.229986	5.873088
5.597915	411.511875	5.878093
5.532582	429.327096	5.883098
5.582411	443.792547	5.888102
5.864814	439.527410	5.893107
5.566455	423.436922	5.898112
5.851484	418.706331	5.903117
5.848910	448.073449	5.908122
6.187614	446.309604	5.913126
5.848359	435.029835	5.918131
5.190735	439.650313	5.923136
5.583186	442.656994	5.928141
5.653598	440.942223	5.933146
5.739382	466.384458	5.938150
5.621759	465.085784	5.943155
5.986510	450.357318	5.948160
6.042345	445.824800	5.953165
5.732252	461.240936	5.958170
5.597301	476.620153	5.963174
6.011905	464.900104	5.968179
6.058984	454.797471	5.973184
6.129162	471.955150	5.978189
6.288571	466.944130	5.983194
5.962847	460.067151	5.988198
6.238162	457.602822	5.993203
5.978483	465.280059	5.998208
6.102088	458.642131	6.003213
6.317376	451.979782	6.008218
6.007321	470.532147	6.013222
6.456679	462.990232	6.018227
6.255968	467.210163	6.023232
6.382964	465.013020	6.028237
6.446322	471.112560	6.033242
6.049385	462.937297	6.038246
6.427149	440.626258	6.043251
5.911411	430.457927	6.048256
5.945127	435.811541	6.053261
5.963478	438.903029	6.058266
5.898545	456.430853	6.063270
6.366561	452.547783	6.068275
5.906052	432.136260	6.073280
5.563689	448.553767	6.078285
6.106682	459.421515	6.083290
5.691052	461.369281	6.088294
6.067299	461.789520	6.093299
6.055217	479.063100	6.098304
5.746388	450.737867	6.103309
6.153267	458.705950	6.108314
5.894126	455.990793	6.113318
6.218130	471.071805	6.118323
6.003605	471.638407	6.123328
5.977701	457.170805	6.128333
6.128349	466.711568	6.133338
6.124247	463.592321	6.138342
6.161567	465.082182	6.143347
6.174649	484.777373	6.148352
6.025628	483.158544	6.153357
6.234554	464.743378	6.158362
6.051293	459.766499	6.163366
5.824551	460.964397	6.168371
5.840310	469.259724	6.173376
6.076533	474.620430	6.178381
6.096736	480.652823	6.183386
6.047545	472.733197	6.188390
6.128016	458.013231	6.193395
5.942117	459.269685	6.198400
6.422315	461.833340	6.203405
6.184230	480.534324	6.208410
5.979845	475.635509	6.213414
6.113323	454.995675	6.218419
5.995935	456.215651	6.223424
5.945633	474.246157	6.228429
6.109633	486.224301	6.233434
6.200605	476.665943	6.238438
6.106493	471.674031	6.243443
5.934166	478.548440	6.248448
5.790396	462.907750	6.253453
6.108731	455.606688	6.258458
5.696347	469.558435	6.263462
5.959266	482.045136	6.268467
6.114584	481.953499	6.273472
5.983984	463.281336	6.278477
6.345845	462.190193	6.283482
6.107320	473.896584	6.288486
6.178699	466.247555	6.293491
6.200832	479.572704	6.298496
6.309878	473.920306	6.303501
6.164691	447.016195	6.308506
5.762143	446.705220	6.313510
6.140234	461.892308	6.318515
6.359564	466.666577	6.323520
5.813794	448.680186	6.328525
6.209496	452.510636	6.333530
5.765392	457.690189	6.338534
6.207199	443.707108	6.343539
5.867114	452.842527	6.348544
5.781994	474.775394	6.353549
6.136266	470.176483	6.358554
6.164411	479.821251	6.363558
6.228288	480.984540	6.368563
6.214800	463.031603	6.373568
6.176777	450.003514	6.378573
5.971950	448.648719	6.383578
5.993339	458.312052	6.388582
5.857056	440.586399	6.393587
5.901771	441.408372	6.398592
5.969462	453.714332	6.403597
6.358268	473.740037	6.408602
6.102885	458.625342	6.413606
6.295047	445.175870	6.418611
5.807244	457.178745	6.423616
5.713444	450.757275	6.428621
6.170717	451.017532	6.433626
6.240379	453.631274	6.438630
6.147423	458.383359	6.443635
6.018511	464.291233	6.448640
5.927364	446.506422	6.453645
6.106215	420.018176	6.458650
5.849746	428.900739	6.463654
6.157518	462.827016	6.468659
5.991901	464.323878	6.473664
6.066665	457.930975	6.478669
6.525559	456.374158	6.483674
5.937393	459.840225	6.488678
5.932457	451.918130	6.493683
5.820388	430.071995	6.498688
5.844199	424.890442	6.503693
6.328029	451.643802	6.508698
5.928890	473.305884	6.513702
5.901975	459.413764	6.518707
6.051293	460.431334	6.523712
5.924266	460.291359	6.528717
6.027875	466.069952	6.533722
5.962872	477.318252	6.538726
6.256740	465.900290	6.543731
5.878075	451.113858	6.548736
5.880365	453.316914	6.553741
6.100503	471.872418	6.558746
5.878962	478.919506	6.563750
6.244484	462.064140	6.568755
6.084064	464.307602	6.573760
5.914399	468.744262	6.578765
5.754645	493.286409	6.583770
6.204712	473.813231	6.588774
6.138189	451.922939	6.593779
6.180619	458.441735	6.598784
6.057947	474.053210	6.603789
6.157848	471.082997	6.608794
5.790186	476.342554	6.613798
6.092561	480.770362	6.618803
5.935876	474.161189	6.623808
6.134921	456.350408	6.628813
6.213502	467.800977	6.633818
5.909340	485.087319	6.638822
6.070776	481.792936	6.643827
6.095741	461.453063	6.648832
6.384247	458.798827	6.653837
6.363779	474.410774	6.658842
6.132641	478.755989	6.663846
6.026803	447.787964	6.668851
5.787242	434.563837	6.673856
5.884864	450.370903	6.678861
6.220594	462.053312	6.683866
6.270514	472.867603	6.688870
6.144024	435.515336	6.693875
6.123686	429.537391	6.698880
5.918713	436.704934	6.703885
6.100875	442.557741	6.708890
5.904883	441.864699	6.713894
5.980963	438.585713	6.718899
6.057123	437.422127	6.723904
5.694301	436.625748	6.728909
6.344210	446.101353	6.733914
5.864153	461.055099	6.738918
6.427788	444.478445	6.743923
6.180218	444.665779	6.748928
6.156895	437.144578	6.753933
6.062557	436.006998	6.758938
6.176039	448.857817	6.763942
6.193716	439.241061	6.768947
6.194298	437.964682	6.773952
6.081728	423.902080	6.778957
6.114273	428.155959	6.783962
5.960697	446.849644	6.788966
5.912388	422.587643	6.793971
6.274387	436.294487	6.798976
5.795859	430.093457	6.803981
6.034014	426.140756	6.808986
5.961581	440.026233	6.813990
6.007498	433.918959	6.818995
6.014788	431.418037	6.824000
5.794722	438.465554	6.829005
5.942455	436.138225	6.834010
5.874279	441.976666	6.839014
6.037355	439.072372	6.844019
6.041617	431.900763	6.849024
5.892443	422.532169	6.854029
6.164009	436.922398	6.859034
6.116062	460.643512	6.864038
6.241773	455.285200	6.869043
6.004106	423.225568	6.874048
5.995969	435.798755	6.879053
6.142872	448.139958	6.884058
5.950618	457.108007	6.889062
6.063892	433.235286	6.894067
5.941352	427.574023	6.899072
5.801700	435.388260	6.904077
6.054914	461.301089	6.909082
5.759280	459.919670	6.914086
6.290976	450.865784	6.919091
6.088495	451.064410	6.924096
6.068911	469.487387	6.929101
6.012798	478.121911	6.934106
5.792733	472.396055	6.939110
6.313639	456.063501	6.944115
6.327420	468.633389	6.949120
5.892273	455.772729	6.954125
6.268036	457.246019	6.959130
5.788133	439.718122	6.964134
6.114849	443.665327	6.969139
6.110537	460.658822	6.974144
6.002852	469.208445	6.979149
5.902704	455.482421	6.984154
5.981017	454.568354	6.989158
6.251960	460.963366	6.994163
6.187250	471.129047	6.999168
6.011077	440.087034	7.004173
5.844502	445.271326	7.009178
5.789956	460.471510	7.014182
6.020629	461.788449	7.019187
6.035136	479.005845	7.024192
6.097535	464.207968	7.029197
5.931255	444.039408	7.034202
5.705298	476.935250	7.039206
6.147788	474.369503	7.044211
6.045325	467.342573	7.049216
5.797089	455.767980	7.054221
6.101975	446.814221	7.059226
5.895245	470.053650	7.064230
5.881393	473.724305	7.069235
6.029038	460.674994	7.074240
6.098109	447.262730	7.079245
6.278516	467.268709	7.084250
5.910065	485.219221	7.089254
5.939311	467.651641	7.094259
5.952200	450.921743	7.099264
5.723513	465.922538	7.104269
6.178468	476.718333	7.109274
5.996499	478.085019	7.114278
6.379711	458.375104	7.119283
6.160902	464.154399	7.124288
6.013303	468.364863	7.129293
6.236336	456.353800	7.134298
6.079899	470.761030	7.139302
5.811692	471.883409	7.144307
5.859236	465.545313	7.149312
6.058451	468.868533	7.154317
6.160717	457.843688	7.159322
5.966482	476.200143	7.164326
6.283195	471.036362	7.169331
5.879580	464.039571	7.174336
5.997683	465.098800	7.179341
6.186847	473.114116	7.184346
6.206887	463.748114	7.189350
6.340164	459.697909	7.194355
6.559852	475.424751	7.199360
6.360078	477.267794	7.204365
6.208899	446.031445	7.209370
5.902874	443.151700	7.214374
6.160835	436.329795	7.219379
6.187698	428.439647	7.224384
5.807965	431.555193	7.229389
6.082933	438.556513	7.234394
5.621081	441.892102	7.239398
6.045726	446.249087	7.244403
5.945204	452.884333	7.249408
6.032543	475.651578	7.254413
6.320541	479.832871	7.259418
6.172818	466.988132	7.264422
6.057298	436.002791	7.269427
6.165304	443.421266	7.274432
5.867327	438.883494	7.279437
6.190059	435.137292	7.284442
6.011341	445.308282	7.289446
6.073349	438.127817	7.294451
5.899684	440.324929	7.299456
6.057233	445.473708	7.304461
6.376103	455.562474	7.309466
5.793800	448.548757	7.314470
6.032822	430.830344	7.319475
6.350871	439.289173	7.324480
5.783531	452.070106	7.329485
6.036690	444.859627	7.334490
5.976764	435.006316	7.339494
5.984760	446.124152	7.344499
6.139066	444.692645	7.349504
5.880304	450.662912	7.354509
6.043769	467.602645	7.359514
6.083692	473.450165	7.364518
6.376664	455.088696	7.369523
6.448144	431.961858	7.374528
6.086791	434.365975	7.379533
6.038865	446.561807	7.384538
5.881880	448.069868	7.389542
5.939633	435.841784	7.394547
5.689406	430.476949	7.399552
5.899733	451.126179	7.404557
6.137986	441.917183	7.409562
6.196062	459.851040	7.414566
6.118246	468.802058	7.419571
5.900938	447.085553	7.424576
5.862870	447.856493	7.429581
6.256886	456.474820	7.434586
6.130130	458.798048	7.439590
6.230673	428.672840	7.444595
5.829438	420.943411	7.449600
5.859220	440.559432	7.454605
6.171205	456.608280	7.459610
5.897371	451.571003	7.464614
5.841564	438.668285	7.469619
6.391998	458.378319	7.474624
5.933469	465.937190	7.479629
6.264393	445.947583	7.484634
6.148735	460.509945	7.489638
6.183543	433.237847	7.494643
5.953991	426.241409	7.499648
5.700467	429.702970	7.504653
6.165276	430.357954	7.509658
5.935044	462.386269	7.514662
6.302073	459.851442	7.519667
6.210297	436.632212	7.524672
5.812177	439.829322	7.529677
6.078367	435.544473	7.534682
5.977284	443.030944	7.539686
5.886698	436.209227	7.544691
5.737390	452.905971	7.549696
6.369915	449.768131	7.554701
6.486244	454.472705	7.559706
6.085218	456.004919	7.564710
5.991287	441.798746	7.569715
5.871285	436.442080	7.574720
5.581070	436.109187	7.579725
5.940082	453.702983	7.584730
6.111225	467.630307	7.589734
5.995047	475.636699	7.594739
6.348265	465.292582	7.599744
6.139915	469.912019	7.604749
6.147154	466.531946	7.609754
6.053370	451.783567	7.614758
5.824955	459.348305	7.619763
6.105951	459.131529	7.624768
6.048131	457.900509	7.629773
6.400211	450.876106	7.634778
6.010263	458.292437	7.639782
5.826196	442.085972	7.644787
6.124746	447.201881	7.649792
6.092544	450.898055	7.654797
5.922311	439.273195	7.659802
6.029195	444.558787	7.664806
6.196307	444.798435	7.669811
6.047084	445.721610	7.674816
5.641018	451.059913	7.679821
6.027107	445.187529	7.684826
6.122271	451.946990	7.689830
6.245795	462.673843	7.694835
6.116692	474.938455	7.699840
5.715473	451.540194	7.704845
6.053668	441.286175	7.709850
6.120570	455.745462	7.714854
6.199917	474.656977	7.719859
6.245894	469.736617	7.724864
5.907660	449.246661	7.729869
5.934522	458.279910	7.734874
5.911150	463.284283	7.739878
6.017999	449.147417	7.744883
6.242917	457.268486	7.749888
6.111474	469.885162	7.754893
6.426813	459.461879	7.759898
6.273085	445.817916	7.764902
6.285133	450.157164	7.769907
6.137494	434.312547	7.774912
6.101905	431.326456	7.779917
6.212703	433.555772	7.784922
6.077227	431.848885	7.789926
6.204309	423.134842	7.794931
6.035254	450.595087	7.799936
6.057410	454.306447	7.804941
6.292822	428.328124	7.809946
6.208765	415.126456	7.814950
5.976324	431.343773	7.819955
5.816438	439.483244	7.824960
6.180423	443.475883	7.829965
5.985435	440.940715	7.834970
5.873150	448.477772	7.839974
5.835515	429.755069	7.844979
5.727816	435.771391	7.849984
5.398645	453.913461	7.854989
5.742604	440.673196	7.859994
5.950154	443.819341	7.864998
5.900497	457.998693	7.870003
6.420054	475.000825	7.875008
6.081710	470.322235	7.880013
6.021758	456.675885	7.885018
5.906070	458.193794	7.890022
5.825792	462.574742	7.895027
5.996124	463.042722	7.900032
6.081636	467.824900	7.905037
6.164024	472.550182	7.910042
6.134094	465.460265	7.915046
5.695711	460.056868	7.920051
5.980555	478.274766	7.925056
5.684764	463.082104	7.930061
6.120972	452.155376	7.935066
5.775924	465.298025	7.940070
6.248568	479.624088	7.945075
6.163688	464.156756	7.950080
6.125189	452.809021	7.955085
6.241439	453.802757	7.960090
6.030914	469.061576	7.965094
5.675497	471.733831	7.970099
5.988419	452.837649	7.975104
5.988466	456.203646	7.980109
6.215284	460.170126	7.985114
5.728758	474.069219	7.990118
6.118907	476.168854	7.995136
6.160025	472.712098	8.000154
6.377529	467.292403	8.005171
6.365982	482.803242	8.010189
6.230607	474.784852	8.015206
6.010736	467.401806	8.020224
6.138568	454.535317	8.025242
6.140798	477.834921	8.030259
6.284520	474.333461	8.035277
6.171245	468.818276	8.040294
6.333626	466.662557	8.045312
6.108254	443.728347	8.050330
5.789606	447.472479	8.055347
6.037366	465.000577	8.060365
5.844666	461.352609	8.065382
6.181548	462.001287	8.070400
6.237292	463.773770	8.075418
6.210981	467.895948	8.080435
6.109740	463.891725	8.085453
6.017437	474.689220	8.090470
6.145310	472.271662	8.095488
6.335435	463.430614	8.100506
6.172645	462.554753	8.105523
6.584543	468.016014	8.110541
6.290614	450.546861	8.115558
6.221482	432.606945	8.120576
5.972226	451.593140	8.125594
6.100472	448.291824	8.130611
6.635096	436.275475	8.135629
6.348772	428.621819	8.140646
6.102543	437.288465	8.145664
6.365923	438.793826	8.150682
6.294330	443.372071	8.155699
6.295816	445.505385	8.160717
6.518277	437.672197	8.165734
6.383684	431.333920	8.170752
6.403933	438.797321	8.175770
5.985450	428.517851	8.180787
5.976988	428.208147	8.185805
6.343054	452.154957	8.190822
5.962343	446.110718	8.195840
6.189205	435.110403	8.200858
6.151804	449.348885	8.205875
5.910361	443.121639	8.210893
6.038545	440.231042	8.215910
6.029468	467.604837	8.220928
6.197103	474.686817	8.225946
5.887017	465.457014	8.230963
6.217066	457.668616	8.235981
6.421688	481.959089	8.240998
6.323214	475.991684	8.246016
6.393142	457.865517	8.251034
5.996835	463.349250	8.256051
6.222514	463.377119	8.261069
6.499438	461.877571	8.266086
5.925032	489.754063	8.271104
6.564208	462.320922	8.276122
6.347497	451.422632	8.281139
6.138951	473.376952	8.286157
6.096023	485.797910	8.291174
6.248103	473.454412	8.296192
6.374662	459.333275	8.301210
6.181994	458.503286	8.306227
6.091176	464.184887	8.311245
6.354941	455.553165	8.316262
6.398191	467.337803	8.321280
6.218164	482.069139	8.326298
6.151486	489.392447	8.331315
6.431388	487.838286	8.336333
6.508847	481.231645	8.341350
6.539352	493.537158	8.346368
6.635620	490.279787	8.351386
6.259607	468.198150	8.356403
6.329741	470.460732	8.361421
6.514702	482.501311	8.366438
6.167725	477.255584	8.371456
6.313783	489.642362	8.376474
6.589753	493.408676	8.381491
6.819360	497.041159	8.386509
6.537888	490.953247	8.391526
6.243226	479.372251	8.396544
6.956882	464.252379	8.401562
6.558727	473.171351	8.406579
6.349390	482.947352	8.411597
6.498239	482.188051	8.416614
6.400098	463.932020	8.421632
6.646618	462.320503	8.426650
6.267006	481.999048	8.431667
6.205282	471.942892	8.436685
6.558873	475.619231	8.441702
6.455855	502.651828	8.446720
6.560545	492.365065	8.451738
6.909993	501.047053	8.456755
6.625802	495.573782	8.461773
6.699858	475.651857	8.466790
6.066275	485.228363	8.471808
6.451313	476.288679	8.476826
6.611398	474.429020	8.481843
6.436931	497.614589	8.486861
6.659467	508.137996	8.491878
6.386147	513.584498	8.496896
6.633003	492.036421	8.501914
6.464821	506.655718	8.506931
6.603217	501.350826	8.511949
6.795022	492.831242	8.516966
7.055615	514.802847	8.521984
6.892015	505.918489	8.527002
6.687700	481.332987	8.532019
6.731446	468.480973	8.537037
6.451080	477.277263	8.542054
6.524633	489.646701	8.547072
6.516490	475.477162	8.552090
6.145379	475.906522	8.557107
6.279449	501.679028	8.562125
6.705036	494.041902	8.567143
6.668077	510.476487	8.572160
6.897054	516.656282	8.577178
6.885259	512.796864	8.582195
6.711142	502.967371	8.587213
6.838366	513.953452	8.592231
6.668736	515.798609	8.597248
6.854704	508.160929	8.602266
6.589901	492.421752	8.607283
6.497354	488.939262	8.612301
6.896177	500.516486	8.617319
6.544949	502.029060	8.622336
6.645105	487.465539	8.627354
6.578570	506.354893	8.632371
6.576823	521.030138	8.637389
6.817879	509.226964	8.642407
6.434704	494.493679	8.647424
6.314344	510.222273	8.652442
6.728758	518.877300	8.657459
6.659517	517.026015	8.662477
6.989675	483.595834	8.667495
6.553373	506.682111	8.672512
6.701509	519.423192	8.677530
6.545883	506.737816	8.682547
6.366847	510.730269	8.687565
6.625173	497.918928	8.692583
6.692947	500.254521	8.697600
6.651178	494.995839	8.702618
6.709108	521.799960	8.707635
6.727791	547.239940	8.712653
7.012322	525.299579	8.717671
6.580646	526.726265	8.722688
6.918940	547.212170	8.727706
6.813749	558.746390	8.732723
6.926458	542.043554	8.737741
7.282301	520.972757	8.742759
6.922620	517.456672	8.747776
6.787097	523.355367	8.752794
6.485695	518.483285	8.757811
6.832632	518.866697	8.762829
6.741883	519.665847	8.767847
6.978815	541.499611	8.772864
6.862471	547.639761	8.777882
6.816636	545.674892	8.782899
6.827033	549.911956	8.787917
7.072811	544.011909	8.792935
6.873729	531.242381	8.797952
6.871005	522.557642	8.802970
6.784777	532.430225	8.807987
6.683045	544.774754	8.813005
6.622438	540.987747	8.818023
6.393674	540.389933	8.823040
6.433600	526.957663	8.828058
6.782474	546.062094	8.833075
6.371609	559.906817	8.838093
6.896320	561.002177	8.843111
7.030878	548.774178	8.848128
7.161220	568.413232	8.853146
7.374321	587.501188	8.858163
7.009322	581.532918	8.863181
7.170954	549.939775	8.868199
6.899147	538.123725	8.873216
7.082983	547.094057	8.878234
7.069129	566.418255	8.883251
6.833561	546.829807	8.888269
7.209098	539.549551	8.893287
6.957346	548.303467	8.898304
6.921727	572.898278	8.903322
7.333810	571.710933	8.908339
6.836770	559.752415	8.913357
6.927555	556.203500	8.918375
7.389670	563.925439	8.923392
7.412157	567.042323	8.928410
7.448049	558.447316	8.933427
6.789968	568.194213	8.938445
6.841611	556.115601	8.943463
7.069283	547.711776	8.948480
6.879505	543.776774	8.953498
7.068283	546.213504	8.958515
7.302800	554.829403	8.963533
7.129160	569.434999	8.968551
6.768593	568.536223	8.973568
7.279181	563.006069	8.978586
7.691587	559.419647	8.983603
7.019600	553.292732	8.988621
6.935149	527.987742	8.993639
7.117829	553.996820	8.998656
7.262819	573.734120	9.003674
7.350356	552.812708	9.008691
7.370696	535.615839	9.013709
6.920486	539.327322	9.018727
7.348503	556.992716	9.023744
7.206263	537.717995	9.028762
7.442373	522.263224	9.033779
6.996800	534.234769	9.038797
7.108582	542.821548	9.043815
7.278477	539.793368	9.048832
7.076208	532.490625	9.053850
7.280030	520.094653	9.058867
7.093415	541.621748	9.063885
7.340070	556.686268	9.068903
7.320175	557.775790	9.073920
7.221078	539.375970	9.078938
7.428051	533.672247	9.083955
7.475607	537.659536	9.088973
7.466458	536.161206	9.093991
7.489862	539.799733	9.099008
7.363681	537.595262	9.104026
7.453013	533.063605	9.109043
7.136167	537.894454	9.114061
7.218434	542.792971	9.119079
7.235473	516.584768	9.124096
7.015345	528.696855	9.129114
7.365468	545.274536	9.134131
7.001536	552.657723	9.139149
7.670405	546.483483	9.144167
7.426047	525.242950	9.149184
7.234136	535.684418	9.154202
7.499923	529.406177	9.159219
7.445325	528.296943	9.164237
7.493356	548.444610	9.169255
7.194640	542.048395	9.174272
7.066155	536.645904	9.179290
7.244757	546.220866	9.184307
7.153726	546.173651	9.189325
7.373721	551.314295	9.194343
7.410250	560.543362	9.199360
7.618610	575.987254	9.204378
7.660531	572.908681	9.209395
7.371001	572.337636	9.214413
7.079164	568.895737	9.219431
7.319102	562.926490	9.224448
7.316761	562.578676	9.229466
7.709528	556.264680	9.234483
7.461159	575.178067	9.239501
7.477407	575.963769	9.244519
7.559236	566.239533	9.249536
7.278896	566.396881	9.254554
7.454203	575.231671	9.259571
7.420260	589.324870	9.264589
7.532137	566.877601	9.269607
7.834837	562.949961	9.274624
7.145204	580.054724	9.279642
7.413345	591.228636	9.284659
7.430103	589.011851	9.289677
7.547647	573.900744	9.294695
7.600597	560.161457	9.299712
7.567174	569.645130	9.304730
7.335798	576.506663	9.309747
7.288170	575.347075	9.314765
7.393457	575.621844	9.319783
7.244333	567.732906	9.324800
7.071131	578.492185	9.329818
7.379820	570.586330	9.334835
7.211310	584.744074	9.339853
7.181361	600.749176	9.344871
7.507707	596.344918	9.349888
7.610798	614.278875	9.354906
7.523601	610.651812	9.359923
7.722253	603.543434	9.364941
7.432569	610.212903	9.369959
7.511387	605.687881	9.374976
7.531313	606.316131	9.379994
7.511905	614.628750	9.385011
7.675641	615.200369	9.390029
7.410840	588.945142	9.395047
7.902607	604.608981	9.400064
7.416314	621.906305	9.405082
7.368390	595.398357	9.410099
7.802558	606.931937	9.415117
7.693024	614.217911	9.420135
8.072773	608.202911	9.425152
7.660110	611.710131	9.430170
7.967492	608.014712	9.435187
7.740822	614.750814	9.440205
7.709310	616.562729	9.445223
7.933363	606.956065	9.450240
7.658722	610.897041	9.455258
7.768027	619.734204	9.460275
7.814389	605.785393	9.465293
7.953853	590.266923	9.470311
7.894416	612.094268	9.475328
7.829824	620.077346	9.480346
7.685980	611.512995	9.485363
7.818950	599.462336	9.490381
7.988916	605.245535	9.495399
7.866073	624.415917	9.500416
7.671954	612.087602	9.505434
7.877316	605.323097	9.510451
7.973911	597.430141	9.515469
7.871158	597.945040	9.520487
8.061196	617.264240	9.525504
7.723821	614.663382	9.530522
8.030278	592.305343	9.535539
8.098373	595.428766	9.540557
7.887513	620.567626	9.545575
8.120141	610.709023	9.550592
7.861281	602.521559	9.555610
7.999053	590.521573	9.560627
8.093994	594.370374	9.565645
7.777579	602.686709	9.570663
7.724308	568.994798	9.575680
7.745253	595.466870	9.580698
7.972362	592.377565	9.585715
7.946218	589.239785	9.590733
7.993063	617.234546	9.595751
8.068646	626.210220	9.600768
7.975789	610.776959	9.605786
7.818641	603.260781	9.610803
7.986394	608.892716	9.615821
7.490960	601.821016	9.620839
8.109172	603.293827	9.625856
7.968000	603.737637	9.630874
7.852905	622.633880	9.635891
7.986410	615.188624	9.640909
7.949675	615.995383	9.645927
7.803041	595.415580	9.650944
7.932146	612.152559	9.655962
7.933796	618.814623	9.660979
8.169798	608.938342	9.665997
8.234823	587.732594	9.671015
8.423170	592.099174	9.676032
8.218540	612.893430	9.681050
8.359771	594.697461	9.686067
8.279074	600.328832	9.691085
7.615335	609.725410	9.696103
7.860236	585.728508	9.701120
7.992487	588.463383	9.706138
8.180548	608.867632	9.711155
8.165786	612.370890	9.716173
7.738613	613.021860	9.721191
8.039816	596.076949	9.726208
8.349870	602.984412	9.731226
7.941380	624.691458	9.736243
8.086772	611.973369	9.741261
7.784184	596.473828	9.746279
7.807624	599.420727	9.751296
7.965016	626.165003	9.756314
7.760623	612.205573	9.761331
8.024319	603.682509	9.766349
7.985496	594.277128	9.771367
8.299777	613.569788	9.776384
8.432495	637.891088	9.781402
8.464590	618.488170	9.786419
8.086217	597.428105	9.791437
7.944393	605.866824	9.796455
7.791897	622.513385	9.801472
8.229518	641.554562	9.806490
8.421495	638.191112	9.811507
8.569487	620.898762	9.816525
8.369594	620.183803	9.821543
8.393652	620.283369	9.826560
8.071287	615.957184	9.831578
7.992276	601.201181	9.836595
8.199942	624.066972	9.841613
8.259528	622.248208	9.846631
8.436640	639.815733	9.851648
8.326610	653.585142	9.856666
8.270010	642.770166	9.861683
8.375964	627.704316	9.866701
7.898130	642.055613	9.871719
8.364366	643.537998	9.876736
8.102332	653.216645	9.881754
8.027076	638.821793	9.886771
8.170032	630.113902	9.891789
8.214047	643.607324	9.896807
7.992685	639.752004	9.901824
8.432514	641.117331	9.906842
8.164142	643.201495	9.911859
8.641396	627.991728	9.916877
8.195326	642.941348	9.921895
8.445931	638.965720	9.926912
8.423355	641.251126	9.931930
8.261215	629.513803	9.936947
8.011392	637.571091	9.941965
8.142269	667.228658	9.946983
8.653880	665.569572	9.952000
8.653993	681.248126	9.957018
8.311097	660.894807	9.962035
8.449280	647.953728	9.967053
8.519210	670.271054	9.972071
8.602859	672.122195	9.977088
8.541243	659.671381	9.982106
8.242975	640.171991	9.987123
8.817312	641.883588	9.992141
8.345534	657.883738	9.997159
8.491340	674.158508	10.002176
8.574750	667.134876	10.007194
8.319114	679.541354	10.012211
8.734684	675.306530	10.017229
8.541019	690.314653	10.022247
8.695756	669.807942	10.027264
8.718885	649.977843	10.032282
8.588956	646.125319	10.037299
8.401305	649.155820	10.042317
8.396287	660.188264	10.047335
8.651107	649.508477	10.052352
8.818990	661.633200	10.057370
8.306859	670.938737	10.062387
8.744682	675.982418	10.067405
8.168866	674.135817	10.072423
8.813363	675.278399	10.077440
8.646798	666.105344	10.082458
8.488257	675.667028	10.087475
8.643352	682.326687	10.092493
8.683398	668.392935	10.097511
8.783926	655.180001	10.102528
8.630739	679.877264	10.107546
8.687731	682.627151	10.112563
8.688978	661.237110	10.117581
8.764890	665.256252	10.122599
8.640996	671.049764	10.127616
8.664183	666.735536	10.132634
8.447218	669.276631	10.137651
8.581186	685.652260	10.142669
8.672659	676.285121	10.147687
8.610074	666.894641	10.152704
8.797818	678.864364	10.157722
8.531280	692.181164	10.162739
8.592405	684.845643	10.167757
8.427447	679.927344	10.172775
8.370064	685.267079	10.177792
8.635934	667.718154	10.182810
8.408369	680.905407	10.187827
8.851967	701.721265	10.192845
8.888132	707.362784	10.197863
8.783115	708.122285	10.202880
9.018048	716.747062	10.207898
8.901796	712.872975	10.212915
9.286939	697.733267	10.217933
8.605528	695.045097	10.222951
8.695304	695.574922	10.227968
8.932265	692.847452	10.232986
8.568123	696.084441	10.238003
8.913758	708.638754	10.243021
8.565241	723.553045	10.248039
8.534549	714.566996	10.253056
8.656117	695.588938	10.258074
8.876215	701.531364	10.263091
8.414326	720.383983	10.268109
8.456753	720.677408	10.273127
8.584263	705.435722	10.278144
8.821321	716.892345	10.283162
8.705295	742.930739	10.288179
8.807451	752.729037	10.293197
8.845776	746.180409	10.298215
9.134878	725.598578	10.303232
8.927944	743.513765	10.308250
9.221435	766.920259	10.313267
8.943444	743.130455	10.318285
8.855586	743.688456	10.323303
9.339970	747.933441	10.328320
9.468733	737.482737	10.333338
9.175747	733.545750	10.338355
9.305031	735.680420	10.343373
9.092672	723.915506	10.348391
9.083250	705.314793	10.353408
9.030620	708.229906	10.358426
8.970024	726.080841	10.363443
8.929335	728.738740	10.368461
9.540819	716.209804	10.373479
9.176864	714.384962	10.378496
9.295828	709.225396	10.383514
9.295824	715.845955	10.388531
9.053284	699.490159	10.393549
9.125458	721.276231	10.398567
8.800411	709.227279	10.403584
9.369156	689.158578	10.408602
9.128990	695.320234	10.413619
9.385324	698.910367	10.418637
9.093534	690.931882	10.423655
9.155014	698.982429	10.428672
9.448130	721.047157	10.433690
9.188841	714.463301	10.438707
9.047154	706.450654	10.443725
8.836439	698.883453	10.448743
8.776971	701.011624	10.453760
9.059602	735.776992	10.458778
9.400080	746.910921	10.463795
9.398185	734.740748	10.468813
9.387597	732.237005	10.473831
9.349591	733.378043	10.478848
9.655893	724.635231	10.483866
9.015531	713.891881	10.488883
9.098200	706.717115	10.493901
9.128454	722.588904	10.498919
9.085282	738.882281	10.503936
9.369350	736.756794	10.508954
9.432872	735.026613	10.513971
9.686296	736.975065	10.518989
9.448434	739.963107	10.524007
9.000694	733.872759	10.529024
9.256611	730.130713	10.534042
9.051394	736.208088	10.539059
9.225732	752.565211	10.544077
9.445877	762.579090	10.549095
9.322091	747.187899	10.554112
9.714712	732.186254	10.559130
9.686654	737.679877	10.564147
9.815951	746.484191	10.569165
9.421722	731.609333	10.574183
9.425045	714.716961	10.579200
9.495267	717.803651	10.584218
9.310163	704.234347	10.589235
9.319788	709.960545	10.594253
9.501818	729.632394	10.599271
9.300557	750.735154	10.604288
9.521920	745.844994	10.609306
9.494370	745.155372	10.614323
9.503887	744.356109	10.619341
9.872351	749.394550	10.624359
9.507438	739.465959	10.629376
9.684634	709.455212	10.634394
9.537215	712.355094	10.639411
9.540106	715.227381	10.644429
9.563886	692.498505	10.649447
9.316710	713.740754	10.654464
9.531741	734.049401	10.659482
9.569623	740.275331	10.664499
9.473525	738.029846	10.669517
9.517524	747.407652	10.674535
9.545809	738.555012	10.679552
9.636624	746.428539	10.684570
9.816489	743.585136	10.689587
9.596844	758.781625	10.694605
9.951421	747.918894	10.699623
9.715576	742.436363	10.704640
9.687623	726.434734	10.709658
9.299037	721.799669	10.714675
9.547410	734.267348	10.719693
9.858919	737.701167	10.724711
9.488192	758.875043	10.729728
9.561323	749.591774	10.734746
9.670331	747.734127	10.739763
9.439365	753.013521	10.744781
9.606700	750.682778	10.749799
9.423509	760.330751	10.754816
9.646057	730.713738	10.759834
9.490690	738.332060	10.764851
9.183297	747.943283	10.769869
9.540205	743.418117	10.774887
9.259548	749.464079	10.779904
10.070036	773.641409	10.784922
9.882544	776.747380	10.789939
9.621183	771.707717	10.794957
9.995029	758.720515	10.799975
10.010201	778.653699	10.804992
9.959962	769.027617	10.810010
9.809198	758.843800	10.815027
9.704715	751.785647	10.820045
9.850918	735.930966	10.825063
9.568980	764.299339	10.830080
9.772355	783.160566	10.835098
9.958740	769.801294	10.840115
9.852820	760.461903	10.845133
9.823822	773.114194	10.850151
9.998700	796.617086	10.855168
10.223666	784.039108	10.860186
9.897984	776.453280	10.865203
9.926892	776.529610	10.870221
9.985689	770.812403	10.875239
9.794361	779.730336	10.880256
9.804252	785.370419	10.885274
9.989862	775.415966	10.890291
9.729773	773.226801	10.895309
10.219690	788.200574	10.900327
9.887290	777.417699	10.905344
10.045468	774.630223	10.910362
9.898863	781.393018	10.915379
9.712001	787.683266	10.920397
9.698916	778.772300	10.925415
9.553170	783.277983	10.930432
9.875299	786.545142	10.935450
10.047080	767.924149	10.940467
9.837595	775.688502	10.945485
10.007553	789.448959	10.950503
9.588387	797.069775	10.955520
10.066766	803.091572	10.960538
10.059690	789.852517	10.965555
10.156200	808.843217	10.970573
10.270213	826.792938	10.975591
10.107870	827.781054	10.980608
9.705633	826.949663	10.985626
9.765415	831.204523	10.990643
9.843238	834.558117	10.995661
10.307163	810.250625	11.000679
10.091600	807.477381	11.005696
10.601244	810.718181	11.010714
10.511676	827.560514	11.015731
10.286898	817.411128	11.020749
10.497343	791.484778	11.025767
10.457398	810.848725	11.030784
10.029147	829.048551	11.035802
10.492112	812.883835	11.040819
10.173284	801.918236	11.045837
10.346058	805.680232	11.050855
10.207511	818.703916	11.055872
10.574015	827.989508	11.060890
10.284095	810.485530	11.065907
10.173500	795.491512	11.070925
10.579718	811.483792	11.075943
10.326410	807.935990	11.080960
10.003122	789.716384	11.085978
10.628530	783.485470	11.090995
10.234101	790.248093	11.096013
10.310182	792.738616	11.101031
10.394698	804.424396	11.106048
10.254630	808.924031	11.111066
10.287098	822.397380	11.116083
10.265845	817.899855	11.121101
10.380435	820.963292	11.126119
10.053867	817.584442	11.131136
10.199869	810.633744	11.136154
10.331464	823.919007	11.141171
10.292146	808.256187	11.146189
10.329639	803.606771	11.151207
10.255779	814.802433	11.156224
10.239302	805.615315	11.161242
10.437003	819.700063	11.166259
10.201728	829.914018	11.171277
10.104950	809.270682	11.176295
10.228180	818.350868	11.181312
10.252798	838.941744	11.186330
10.496674	832.108291	11.191347
10.567132	846.303339	11.196365
10.788739	856.969720	11.201383
10.662623	846.064541	11.206400
10.481060	837.636578	11.211418
10.890319	842.972656	11.216435
10.644246	841.839447	11.221453
10.815972	829.672289	11.226471
10.843280	842.364039	11.231488
10.666845	823.618978	11.236506
10.675950	808.476066	11.241523
10.563927	816.982694	11.246541
10.657357	823.442622	11.251559
10.631597	823.863232	11.256576
10.458387	799.914131	11.261594
10.547063	792.875992	11.266611
10.639011	820.371088	11.271629
10.345149	828.268671	11.276647
10.682903	840.348241	11.281664
10.610477	830.899166	11.286682
10.745915	832.629691	11.291699
10.651181	856.979578	11.296717
10.858864	855.940037	11.301735
10.766745	838.109420	11.306752
10.588892	838.075667	11.311770
10.596582	846.095820	11.316787
10.661505	861.670665	11.321805
10.721515	845.197901	11.326823
11.061346	838.844617	11.331840
10.931659	836.533132	11.336858
10.819797	845.751273	11.341875
10.880352	856.478709	11.346893
10.830883	829.761905	11.351911
11.014681	836.567636	11.356928
10.599195	848.800130	11.361946
11.036066	853.702235	11.366963
10.484880	847.648026	11.371981
10.861802	829.682539	11.376999
10.851972	836.540834	11.382016
10.639655	861.653369	11.387034
10.899035	849.166180	11.392051
10.791079	841.000585	11.397069
10.882012	849.014560	11.402087
10.935230	852.705207	11.407104
10.727087	850.153898	11.412122
11.171046	839.858263	11.417139
10.803797	855.439087	11.422157
11.039739	848.208814	11.427175
11.180635	828.930723	11.432192
10.747646	844.751177	11.437210
10.849133	854.291451	11.442227
10.509699	846.520410	11.447245
10.596916	833.092750	11.452263
10.943690	853.163207	11.457280
10.821109	886.266024	11.462298
11.046522	859.317570	11.467315
10.825612	876.747850	11.472333
10.808067	866.314546	11.477351
10.882195	886.732190	11.482368
10.748628	895.714247	11.487386
11.388549	878.008016	11.492403
11.242714	860.990271	11.497421
11.112611	883.195136	11.502439
11.138237	873.593646	11.507456
10.672836	875.464601	11.512474
11.264565	861.665820	11.517491
10.944691	871.073430	11.522509
10.780111	884.687046	11.527527
11.212197	891.425300	11.532544
11.018108	880.001153	11.537562
11.141268	894.284165	11.542579
11.462483	914.865192	11.547597
11.358833	896.032934	11.552615
11.302958	890.487940	11.557632
11.413278	905.754422	11.562650
11.181974	877.465345	11.567667
11.225654	872.994956	11.572685
11.075364	870.051604	11.577703
11.355548	876.364286	11.582720
11.403614	891.046709	11.587738
11.383082	879.086336	11.592755
11.347977	878.696796	11.597773
11.380369	885.597335	11.602791
11.255659	893.261736	11.607808
11.131854	882.357625	11.612826
11.493229	892.409455	11.617843
11.417397	910.414067	11.622861
11.376912	921.361540	11.627879
11.586889	902.833159	11.632896
11.778700	882.530021	11.637914
11.484986	873.319699	11.642931
11.247686	890.740601	11.647949
11.569940	879.172774	11.652967
11.469646	872.773246	11.657984
11.099432	885.839110	11.663002
11.423770	877.801215	11.668019
11.338666	898.070235	11.673037
11.516681	901.536682	11.678055
11.757270	889.813587	11.683072
11.465804	891.529258	11.688090
11.631308	898.663151	11.693107
11.582237	887.587082	11.698125
11.335788	884.791867	11.703143
11.450159	896.148164	11.708160
11.129228	902.698939	11.713178
11.359223	887.599936	11.718195
11.361288	909.876674	11.723213
11.601939	919.716544	11.728231
11.795771	908.453407	11.733248
11.616188	911.674504	11.738266
11.778018	912.591144	11.743283
11.730797	911.769859	11.748301
11.529125	916.292498	11.753319
11.890546	920.862892	11.758336
11.619718	916.467787	11.763354
11.534814	896.941862	11.768371
11.755277	906.796081	11.773389
11.476792	904.767081	11.778407
11.905330	900.641539	11.783424
11.875427	925.492991	11.788442
11.724317	913.600616	11.793459
11.810279	904.623910	11.798477
11.517408	916.429214	11.803495
11.884403	903.636181	11.808512
11.829891	907.491260	11.813530
11.990094	911.511887	11.818547
12.107175	915.896340	11.823565
11.818684	911.192720	11.828583
12.005449	895.032234	11.833600
11.991183	915.618127	11.838618
11.597001	907.351509	11.843635
11.879695	902.855979	11.848653
11.383841	891.307526	11.853671
11.832689	892.716354	11.858688
11.646079	900.215641	11.863706
11.663845	906.664493	11.868723
11.572983	911.452110	11.873741
11.173518	929.026987	11.878759
12.071879	911.164455	11.883776
11.375523	915.498049	11.888794
11.477527	921.387656	11.893811
12.140467	917.537169	11.898829
11.919014	948.527584	11.903847
12.141596	944.661403	11.908864
11.912416	938.949707	11.913882
12.050528	949.688401	11.918899
12.161901	946.160594	11.923917
12.142745	957.276964	11.928935
12.254653	937.333227	11.933952
11.959676	950.099581	11.938970
12.229269	945.071499	11.943987
12.234206	932.741419	11.949005
12.069784	944.839511	11.954023
11.991550	950.876699	11.959040
12.163359	957.695387	11.964058
12.166645	935.445104	11.969075
12.181832	924.463381	11.974093
12.168434	944.052380	11.979111
12.202453	942.437358	11.984128
12.296756	938.657616	11.989146
12.378233	940.935022	11.994163
12.079516	918.920942	11.999181
11.973982	914.727595	12.004199
12.234022	934.046845	12.009216
12.082990	950.381199	12.014234
12.250333	951.545094	12.019251
12.451427	943.930479	12.024269
12.130258	947.972020	12.029287
12.465707	953.358121	12.034304
12.274630	931.317378	12.039322
11.957535	932.689446	12.044339
12.501892	954.046333	12.049357
12.230948	967.980280	12.054375
12.347006	951.940249	12.059392
12.163981	944.133765	12.064410
11.944182	956.056125	12.069427
11.972136	955.986981	12.074445
11.796427	959.071066	12.079463
12.000114	950.073600	12.084480
12.210885	958.052379	12.089498
12.195849	938.720707	12.094515
12.374763	945.284344	12.099533
12.438445	959.238062	12.104551
12.478222	974.057726	12.109568
12.549622	961.667045	12.114586
12.551388	947.452529	12.119603
12.645803	943.185295	12.124621
12.320652	951.029565	12.129639
12.395610	956.497386	12.134656
12.424454	950.939255	12.139674
12.341413	946.742674	12.144691
12.649567	950.171586	12.149709
12.238837	975.574510	12.154727
12.588044	967.123312	12.159744
12.539180	973.885684	12.164762
12.552964	978.087080	12.169779
12.855129	958.424393	12.174797
12.685074	967.273187	12.179815
12.683586	977.415740	12.184832
12.315035	977.766166	12.189850
12.411489	973.594625	12.194867
12.478324	962.068847	12.199885
12.352258	962.868051	12.204903
12.518600	956.951158	12.209920
12.638219	958.765984	12.214938
12.775145	967.161002	12.219955
12.624644	974.090427	12.224973
12.214228	994.559558	12.229991
12.524613	974.861248	12.235008
12.448609	974.653615	12.240026
12.303054	980.778299	12.245043
12.776718	978.031539	12.250061
12.592390	999.906448	12.255079
12.886377	991.360156	12.260096
13.001675	988.893624	12.265114
12.732371	1001.297208	12.270131
12.891982	989.017683	12.275149
12.763256	995.757249	12.280167
12.875809	1015.603800	12.285184
12.820209	1010.915487	12.290202
13.022859	1009.861417	12.295219
13.117136	1006.440430	12.300237
12.801938	995.381694	12.305255
12.808329	970.974211	12.310272
13.182975	974.619936	12.315290
12.793953	983.373366	12.320307
12.886485	993.742948	12.325325
12.665907	991.239524	12.330343
12.928432	995.648180	12.335360
13.125170	987.310137	12.340378
12.707748	1003.740624	12.345395
13.006226	1007.499706	12.350413
13.020096	1004.883932	12.355431
13.006972	993.483127	12.360448
12.930552	999.638410	12.365466
13.109146	1016.242884	12.370483
13.249378	1003.069337	12.375501
12.956637	1001.298323	12.380519
12.973526	981.686686	12.385536
13.004597	1003.965655	12.390554
12.887949	1019.158960	12.395571
13.013482	989.719053	12.400589
12.772666	989.214429	12.405607
12.769984	1003.077998	12.410624
13.301786	998.873373	12.415642
12.831893	992.571972	12.420659
12.870352	1001.109331	12.425677
12.856662	1000.122010	12.430695
12.911955	1011.179376	12.435712
13.256824	1030.004830	12.440730
13.148212	1046.397785	12.445747
13.356101	1026.259893	12.450765
12.978673	1032.096325	12.455783
12.994452	1030.727259	12.460800
12.982580	1022.526106	12.465818
13.154626	1036.948477	12.470835
13.218998	1031.383854	12.475853
13.283447	1033.664974	12.480871
13.501573	1028.910855	12.485888
13.416836	1019.639834	12.490906
13.067263	1026.903483	12.495923
13.643815	1012.544620	12.500941
13.490422	1031.816008	12.505959
13.518177	1021.857076	12.510976
13.867985	1021.735727	12.515994
13.358988	1045.697478	12.521011
13.476794	1022.233094	12.526029
13.073098	1030.605411	12.531047
13.084526	1031.369990	12.536064
13.234967	1016.423538	12.541082
13.278123	1027.398592	12.546099
13.368776	1039.024399	12.551117
13.537112	1031.679950	12.556135
13.628366	1028.698913	12.561152
13.755658	1031.946664	12.566170
13.151743	1050.672581	12.571187
13.361122	1046.431092	12.576205
13.390256	1042.662587	12.581223
13.281522	1019.112055	12.586240
13.210771	1051.711784	12.591258
13.367276	1072.802505	12.596275
13.675489	1067.863547	12.601293
13.667367	1056.209668	12.606311
13.893317	1060.620550	12.611328
14.066813	1072.530648	12.616346
13.787247	1077.866401	12.621363
13.897433	1061.807251	12.626381
13.717313	1039.085702	12.631399
13.595277	1035.690025	12.636416
13.562543	1032.343749	12.641434
13.698689	1057.529177	12.646451
13.908809	1065.223349	12.651469
13.919744	1054.951506	12.656487
13.637387	1035.535107	12.661504
13.925435	1033.442083	12.666522
13.721580	1046.364356	12.671539
13.641949	1028.082674	12.676557
13.900102	1027.972536	12.681575
13.680629	1055.957868	12.686592
13.823518	1073.474671	12.691610
13.678972	1071.061793	12.696627
13.788558	1046.357383	12.701645
13.913251	1060.550260	12.706663
13.822920	1056.888972	12.711680
14.279038	1049.521851	12.716698
14.102767	1077.340009	12.721715
13.933877	1060.852394	12.726733
14.247152	1071.178956	12.731751
13.809385	1042.949474	12.736768
14.093069	1044.602979	12.741786
13.907128	1043.440924	12.746803
14.243649	1037.017873	12.751821
14.012339	1048.860214	12.756839
13.289511	1042.012944	12.761856
13.966507	1033.437798	12.766874
13.816932	1046.605564	12.771891
14.055759	1057.940626	12.776909
14.039587	1072.816372	12.781927
14.050076	1062.901005	12.786944
14.275035	1048.431947	12.791962
14.115470	1050.937641	12.796979
14.209417	1067.764276	12.801997
14.101477	1060.208841	12.807015
13.836214	1069.670031	12.812032
14.229600	1059.894389	12.817050
13.934784	1066.997472	12.822067
14.051597	1060.326711	12.827085
13.810842	1054.312926	12.832103
13.975761	1058.515936	12.837120
13.992064	1052.531601	12.842138
13.800052	1055.789222	12.847155
13.898434	1062.393180	12.852173
14.381034	1092.932974	12.857191
14.108765	1104.728720	12.862208
14.360012	1092.469098	12.867226
14.416509	1094.378996	12.872243
14.464285	1099.310550	12.877261
14.346462	1082.522320	12.882279
14.352741	1079.304887	12.887296
14.482896	1078.853099	12.892314
13.990573	1092.198307	12.897331
14.287861	1089.484021	12.902349
14.483008	1074.003485	12.907367
14.367820	1088.575710	12.912384
14.588903	1070.425020	12.917402
14.369711	1081.103887	12.922419
14.405856	1078.498688	12.927437
14.649734	1076.767396	12.932455
14.646670	1091.209704	12.937472
14.633081	1097.393314	12.942490
14.354340	1091.286801	12.947507
14.106453	1079.198827	12.952525
14.427541	1078.642275	12.957543
14.450785	1090.168067	12.962560
14.570718	1088.961266	12.967578
14.656272	1104.491522	12.972595
14.348835	1091.860465	12.977613
14.805275	1075.089517	12.982631
14.517357	1086.708648	12.987648
14.727853	1073.452286	12.992666
14.633262	1074.652589	12.997683
14.217983	1079.231240	13.002701
14.377318	1076.289423	13.007719
14.691704	1084.614638	13.012736
14.682280	1073.976947	13.017754
14.510584	1079.258269	13.022771
14.532370	1077.705771	13.027789
14.681916	1103.927015	13.032807
14.891142	1118.075176	13.037824
14.912953	1103.107880	13.042842
14.775360	1094.616224	13.047859
14.760317	1102.684451	13.052877
14.971447	1092.289265	13.057895
14.572052	1097.643155	13.062912
14.955004	1100.494034	13.067930
15.072072	1112.864952	13.072947
14.767204	1092.200321	13.077965
14.777403	1077.311427	13.082983
14.348399	1104.915560	13.088000
14.803639	1100.791752	13.093018
14.870463	1119.859675	13.098035
14.835172	1129.942577	13.103053
15.184934	1106.962708	13.108071
14.728882	1112.168032	13.113088
14.947051	1115.949466	13.118106
15.026280	1137.240499	13.123123
14.999507	1125.819219	13.128141
15.141094	1121.741336	13.133159
15.256355	1129.843541	13.138176
15.018291	1115.928577	13.143194
15.224178	1121.440256	13.148211
15.141456	1135.549104	13.153229
15.249989	1129.959239	13.158247
15.101594	1133.375080	13.163264
14.984467	1117.442490	13.168282
15.131852	1114.135113	13.173299
15.216545	1136.066127	13.178317
15.273330	1124.162946	13.183335
14.803904	1120.330392	13.188352
14.931122	1108.404957	13.193370
14.647633	1128.600695	13.198387
14.939399	1142.852926	13.203405
15.112785	1133.910150	13.208423
15.069615	1122.489319	13.213440
15.132445	1129.135983	13.218458
15.211456	1123.368564	13.223475
15.238693	1122.156513	13.228493
15.284519	1127.494598	13.233511
15.147019	1145.296737	13.238528
15.386839	1144.302346	13.243546
15.811755	1146.635598	13.248563
15.382385	1133.068395	13.253581
15.426631	1135.386621	13.258599
15.210771	1129.550045	13.263616
15.510830	1113.084752	13.268634
15.329451	1114.881442	13.273651
15.103073	1124.663718	13.278669
15.680251	1137.394535	13.283687
15.480152	1154.494901	13.288704
15.610284	1144.525367	13.293722
15.393450	1150.674395	13.298739
15.333174	1149.566251	13.303757
15.716378	1128.150321	13.308775
15.447009	1152.748480	13.313792
15.163115	1164.002133	13.318810
15.477444	1152.668522	13.323827
15.414238	1147.400071	13.328845
15.541812	1132.068995	13.333863
15.640803	1154.313539	13.338880
15.744841	1148.526722	13.343898
15.360570	1144.020114	13.348915
15.420509	1139.441770	13.353933
15.768798	1145.767023	13.358951
15.748404	1154.935990	13.363968
15.544238	1137.114686	13.368986
15.826517	1151.730215	13.374003
15.786587	1154.509391	13.379021
15.697094	1137.473860	13.384039
15.522974	1142.922393	13.389056
15.680935	1157.987895	13.394074
16.001282	1148.366753	13.399091
15.669436	1149.465852	13.404109
16.128749	1135.354540	13.409127
15.997836	1154.322834	13.414144
15.718033	1154.599851	13.419162
15.736710	1146.929574	13.424179
15.649644	1134.814782	13.429197
16.031463	1140.979806	13.434215
15.602070	1146.555250	13.439232
15.399041	1151.215255	13.444250
15.679604	1149.321829	13.449267
15.752904	1163.355521	13.454285
15.975776	1165.108830	13.459303
16.004900	1183.969828	13.464320
15.879997	1184.595664	13.469338
16.020931	1192.337348	13.474355
16.183220	1186.196092	13.479373
16.239765	1183.574810	13.484391
16.217653	1201.398979	13.489408
16.079831	1194.208467	13.494426
15.800749	1164.408324	13.499443
15.901570	1159.674534	13.504461
15.975066	1175.640606	13.509479
16.282158	1186.422882	13.514496
16.034594	1188.171970	13.519514
16.354142	1182.947411	13.524531
15.992002	1204.146951	13.529549
16.008174	1185.940245	13.534567
16.257826	1171.643031	13.539584
16.124830	1170.199744	13.544602
16.170279	1184.071660	13.549619
16.397333	1189.045154	13.554637
16.199562	1176.501095	13.559655
16.781344	1179.394900	13.564672
16.111514	1181.726539	13.569690
16.374772	1169.108264	13.574707
16.274391	1180.035316	13.579725
16.466116	1188.215642	13.584743
16.531136	1171.797591	13.589760
16.157770	1171.149551	13.594778
16.285444	1176.369329	13.599795
16.490183	1193.497007	13.604813
16.623373	1172.842630	13.609831
16.671335	1193.418415	13.614848
16.509780	1204.032147	13.619866
16.708732	1188.204101	13.624883
16.368736	1188.591435	13.629901
16.468200	1189.098224	13.634919
16.187848	1196.575853	13.639936
16.307129	1192.217159	13.644954
16.723318	1183.572041	13.649971
16.471100	1182.181223	13.654989
16.190351	1196.946815	13.660007
16.168363	1207.894191	13.665024
16.517307	1201.445476	13.670042
16.377762	1181.260368	13.675059
16.416047	1196.113655	13.680077
16.353621	1203.357781	13.685095
16.578885	1201.807659	13.690112
16.639884	1210.910368	13.695130
16.768346	1216.847966	13.700147
16.692279	1238.072503	13.705165
16.771130	1242.102824	13.710183
16.844518	1217.784148	13.715200
16.539963	1203.647077	13.720218
16.857979	1213.484192	13.725235
16.577591	1224.517776	13.730253
16.564139	1219.664794	13.735271
16.860876	1222.251862	13.740288
16.806603	1227.971003	13.745306
16.959366	1233.397824	13.750323
16.727825	1231.570223	13.755341
17.067159	1211.338704	13.760359
17.039109	1202.487432	13.765376
16.860048	1217.967854	13.770394
16.838126	1227.223218	13.775411
17.009289	1233.753820	13.780429
16.930690	1211.994506	13.785447
16.983564	1213.661966	13.790464
16.810232	1238.934678	13.795482
16.883901	1225.018480	13.800499
16.814636	1204.725096	13.805517
16.805123	1226.389592	13.810535
17.083294	1233.220249	13.815552
17.052157	1230.957362	13.820570
16.904306	1202.015759	13.825587
16.849091	1215.214251	13.830605
16.987906	1224.893729	13.835623
17.124855	1230.075289	13.840640
16.673789	1227.399927	13.845658
17.100549	1219.300057	13.850675
17.102694	1230.308701	13.855693
17.217912	1234.337832	13.860711
17.259833	1249.097973	13.865728
16.834842	1257.234520	13.870746
17.216933	1264.264993	13.875763
17.292548	1257.274458	13.880781
17.264116	1241.358176	13.885799
17.509931	1235.106467	13.890816
17.228382	1247.579186	13.895834
17.339612	1258.287213	13.900851
17.443142	1245.309833	13.905869
17.202372	1245.681361	13.910887
17.639453	1251.884334	13.915904
17.111677	1256.826427	13.920922
17.243469	1246.891977	13.925939
17.433722	1254.118971	13.930957
17.335609	1243.772821	13.935975
17.531174	1259.195212	13.940992
17.397011	1266.523450	13.946010
17.616860	1249.293400	13.951027
17.432514	1239.338087	13.956045
17.284669	1250.835103	13.961063
17.783267	1259.698733	13.966080
17.505465	1252.160745	13.971098
17.662234	1233.684153	13.976115
17.584953	1250.057904	13.981133
17.483809	1250.673519	13.986151
17.831769	1239.031603	13.991168
17.386520	1254.292926	13.996186
17.365306	1246.231156	14.001203
17.630346	1231.552693	14.006221
17.668088	1238.949731	14.011239
17.629653	1259.209646	14.016256
17.511551	1258.765914	14.021274
17.947978	1259.910556	14.026291
18.029323	1285.004774	14.031309
18.206569	1274.995487	14.036327
18.298940	1255.677055	14.041344
18.268060	1242.195244	14.046362
17.825191	1247.478927	14.051379
17.890050	1230.031361	14.056397
17.622929	1244.848278	14.061415
17.618564	1255.528468	14.066432
17.508644	1262.433408	14.071450
17.938899	1255.411918	14.076467
17.446275	1244.037326	14.081485
17.833926	1254.430049	14.086503
18.119323	1272.928015	14.091520
17.824059	1269.869699	14.096538
18.545500	1255.450847	14.101555
18.055186	1265.736170	14.106573
18.048592	1269.283689	14.111591
18.246780	1247.608079	14.116608
17.891964	1237.321477	14.121626
17.840041	1241.391811	14.126643
18.030260	1278.291090	14.131661
18.120689	1275.290757	14.136679
18.005332	1268.776947	14.141696
18.309776	1278.161927	14.146714
18.279701	1278.748676	14.151731
18.179582	1274.625775	14.156749
18.332150	1277.801701	14.161767
18.082133	1257.146282	14.166784
18.435000	1273.743982	14.171802
18.121545	1289.011702	14.176819
18.388617	1286.544936	14.181837
18.211854	1274.971995	14.186855
18.340827	1266.761409	14.191872
18.140460	1293.819261	14.196890
18.026821	1290.115913	14.201907
17.978237	1271.607873	14.206925
18.095285	1278.916743	14.211943
18.213548	1280.881009	14.216960
18.108975	1288.285156	14.221978
18.173105	1275.127495	14.226995
18.198562	1267.057706	14.232013
18.260440	1291.392537	14.237031
18.683615	1287.138382	14.242048
18.372106	1312.196999	14.247066
18.232663	1329.753766	14.252083
18.730438	1314.070749	14.257101
18.443984	1307.217960	14.262119
18.711248	1300.321000	14.267136
18.424079	1330.223797	14.272154
18.504168	1315.180143	14.277171
18.625627	1309.436833	14.282189
18.547820	1316.415704	14.287207
18.643682	1307.095475	14.292224
18.891601	1309.124222	14.297242
18.676502	1314.550363	14.302259
18.922555	1314.629483	14.307277
18.697239	1296.996188	14.312295
18.770843	1310.571707	14.317312
18.766426	1321.967237	14.322330
18.897866	1304.604427	14.327347
18.598514	1314.428010	14.332365
18.192410	1313.690810	14.337383
18.764807	1289.410589	14.342400
18.421915	1309.147003	14.347418
18.514063	1324.245489	14.352435
18.637841	1308.617395	14.357453
19.206421	1335.031437	14.362471
18.958441	1320.206327	14.367488
18.754806	1306.669956	14.372506
18.756334	1330.079018	14.377523
18.934306	1317.696515	14.382541
18.720490	1345.384683	14.387559
19.212156	1320.486110	14.392576
19.017051	1343.391592	14.397594
18.638221	1347.509877	14.402611
19.281420	1335.711544	14.407629
19.244622	1320.049457	14.412647
19.161269	1330.972129	14.417664
19.033620	1324.606748	14.422682
18.951743	1325.967334	14.427699
19.346270	1325.948116	14.432717
19.336340	1322.127841	14.437735
19.468222	1331.486463	14.442752
19.254626	1337.818157	14.447770
19.201589	1339.435039	14.452787
19.422780	1312.530079	14.457805
19.468912	1331.102884	14.462823
19.435238	1331.727918	14.467840
19.460526	1327.418569	14.472858
19.434076	1337.481843	14.477875
19.657154	1324.916035	14.482893
19.308439	1306.336714	14.487911
19.189145	1306.741306	14.492928
19.194688	1318.972000	14.497946
19.242757	1318.365502	14.502963
19.356934	1333.847176	14.507981
19.415228	1331.443343	14.512999
19.462786	1317.916719	14.518016
19.558795	1333.216890	14.523034
19.456790	1342.779978	14.528051
19.390238	1319.009441	14.533069
19.154856	1341.150693	14.538087
19.343743	1323.061410	14.543104
19.376842	1319.975781	14.548122
19.269446	1333.883719	14.553139
19.488474	1334.780600	14.558157
19.386224	1330.063785	14.563175
19.712680	1330.625073	14.568192
19.724266	1339.114417	14.573210
19.809668	1344.368594	14.578227
19.691476	1343.421448	14.583245
19.444543	1336.563887	14.588263
19.553668	1339.636303	14.593280
19.837793	1341.273334	14.598298
19.775455	1367.173631	14.603315
20.036508	1363.638804	14.608333
19.797061	1363.273671	14.613351
20.153607	1359.651230	14.618368
20.142594	1365.753340	14.623386
19.705683	1357.543134	14.628403
20.110110	1334.562648	14.633421
19.455243	1323.120343	14.638439
19.925795	1347.414590	14.643456
20.005404	1353.803323	14.648474
19.976760	1344.257543	14.653491
20.287020	1354.073398	14.658509
19.926908	1370.913803	14.663527
20.132291	1367.962451	14.668544
20.331252	1347.031284	14.673562
19.947123	1358.218395	14.678579
20.207548	1348.946222	14.683597
20.179571	1351.449998	14.688615
20.362394	1360.704277	14.693632
20.246523	1341.269694	14.698650
20.029496	1316.808150	14.703667
20.193332	1317.565957	14.708685
20.081420	1337.997727	14.713703
20.232400	1341.353612	14.718720
20.211914	1344.928143	14.723738
20.350486	1355.935193	14.728755
20.603600	1360.609131	14.733773
20.317798	1358.178221	14.738791
20.389830	1328.907786	14.743808
20.233100	1313.415195	14.748826
19.984684	1339.697689	14.753843
20.277591	1341.726485	14.758861
20.469180	1349.163884	14.763879
20.412726	1353.408578	14.768896
20.524239	1360.825168	14.773914
20.638327	1357.970481	14.778931
20.623239	1353.685706	14.783949
20.804309	1368.463017	14.788967
20.365124	1354.776204	14.793984
20.552721	1342.146380	14.799002
20.588693	1348.722103	14.804019
20.436857	1369.766377	14.809037
20.226343	1359.959961	14.814055
20.266677	1340.179659	14.819072
20.348292	1357.224446	14.824090
20.678881	1361.719772	14.829107
20.548535	1341.284270	14.834125
20.435149	1359.490550	14.839143
20.352927	1359.462836	14.844160
20.543787	1354.946139	14.849178
20.265912	1370.443930	14.854195
20.742542	1369.927200	14.859213
20.902932	1371.447314	14.864231
20.870921	1373.054919	14.869248
21.080801	1387.179605	14.874266
20.665812	1394.161883	14.879283
20.925244	1376.203267	14.884301
20.803068	1376.833679	14.889319
20.913018	1391.714771	14.894336
20.997158	1374.039596	14.899354
21.067128	1379.744166	14.904371
21.203222	1390.368470	14.909389
21.064067	1389.650128	14.914407
20.984499	1368.719301	14.919424
21.228741	1370.910045	14.924442
21.202081	1375.240745	14.929459
21.074935	1358.874423	14.934477
20.580205	1365.009730	14.939495
20.403022	1376.045358	14.944512
20.889260	1365.748685	14.949530
20.884891	1382.806628	14.954547
21.033468	1381.840191	14.959565
21.001061	1372.901568	14.964583
20.986691	1372.305092	14.969600
21.415055	1375.488795	14.974618
21.070256	1381.863051	14.979635
21.257320	1375.774994	14.984653
21.432353	1386.642016	14.989671
21.488679	1397.413040	14.994688
21.323150	1380.599598	14.999706
21.423638	1380.196001	15.004723
21.467517	1376.066693	15.009741
21.709039	1364.224902	15.014759
21.392882	1361.282690	15.019776
21.558463	1378.507773	15.024794
21.094050	1392.532232	15.029811
21.305897	1376.922381	15.034829
20.933415	1371.415265	15.039847
21.294036	1388.375700	15.044864
21.597785	1390.861661	15.049882
21.767108	1406.558162	15.054899
22.112296	1401.039989	15.059917
21.843158	1393.422564	15.064935
21.923289	1399.977531	15.069952
21.847069	1372.380939	15.074970
21.619971	1381.011104	15.079987
21.635096	1382.226265	15.085005
21.731568	1374.849837	15.090023
21.621127	1367.571962	15.095040
22.260246	1385.223700	15.100058
22.006323	1375.892451	15.105075
21.884228	1365.886323	15.110093
22.151247	1366.057528	15.115111
21.897399	1360.752610	15.120128
21.917117	1372.845701	15.125146
21.636049	1387.127388	15.130163
21.739831	1371.860818	15.135181
22.157355	1363.123078	15.140199
21.816388	1385.347969	15.145216
21.696718	1368.802587	15.150234
21.582408	1369.934732	15.155251
21.840758	1387.378889	15.160269
22.182828	1402.511823	15.165287
22.091573	1391.961926	15.170304
22.352541	1395.249067	15.175322
21.830293	1397.527023	15.180339
22.077259	1398.459833	15.185357
22.012071	1391.731132	15.190375
22.394885	1394.179722	15.195392
22.095652	1395.213521	15.200410
22.302578	1416.045653	15.205427
22.166943	1395.659858	15.210445
22.213468	1384.016576	15.215463
22.173162	1385.133836	15.220480
21.980155	1402.945152	15.225498
21.890863	1418.085818	15.230515
22.274676	1404.688348	15.235533
22.272612	1390.543625	15.240551
22.077549	1414.654442	15.245568
22.285672	1417.109765	15.250586
21.849328	1406.438777	15.255603
22.187973	1391.725463	15.260621
22.418956	1410.505558	15.265639
22.170398	1391.451811	15.270656
22.613460	1404.857131	15.275674
22.332651	1433.395019	15.280691
22.510947	1429.446292	15.285709
22.838069	1412.126596	15.290727
22.634303	1423.306580	15.295744
22.650099	1422.230913	15.300762
22.587232	1430.140620	15.305779
22.643520	1420.586463	15.310797
22.683090	1407.696171	15.315815
22.460135	1427.247010	15.320832
22.468483	1434.591434	15.325850
22.769543	1432.873385	15.330867
22.725405	1413.997100	15.335885
22.862236	1428.920331	15.340903
22.817503	1420.501317	15.345920
22.878025	1408.035221	15.350938
22.950498	1417.911865	15.355955
22.981649	1437.844939	15.360973
23.083630	1411.611721	15.365991
22.798449	1422.566926	15.371008
22.842522	1427.697578	15.376026
22.692327	1406.758788	15.381043
22.740089	1412.352303	15.386061
23.031134	1425.489226	15.391079
22.658541	1430.337734	15.396096
22.817448	1407.990688	15.401114
22.710303	1411.004195	15.406131
22.785771	1430.995473	15.411149
22.819271	1423.799075	15.416167
22.928396	1430.058876	15.421184
22.972561	1432.821449	15.426202
23.524231	1452.072594	15.431219
23.256082	1464.293429	15.436237
23.373215	1436.761498	15.441255
23.264476	1439.006058	15.446272
23.177435	1440.544436	15.451290
23.281057	1439.216217	15.456307
23.251112	1448.841363	15.461325
23.434377	1463.482017	15.466343
23.334220	1457.500730	15.471360
23.526204	1428.672874	15.476378
23.356496	1433.158007	15.481395
23.460619	1457.189731	15.486413
23.621979	1451.829253	15.491431
23.176057	1452.161673	15.496448
23.412863	1434.729150	15.501466
23.522327	1457.993532	15.506483
23.456525	1455.698161	15.511501
23.530632	1448.448889	15.516519
23.484769	1454.162395	15.521536
23.613045	1452.109692	15.526554
23.403127	1459.549240	15.531571
23.426054	1458.500142	15.536589
23.689254	1435.794362	15.541607
23.661332	1444.584813	15.546624
23.519623	1451.873451	15.551642
23.622394	1455.975646	15.556659
23.723179	1455.125740	15.561677
23.290569	1461.086978	15.566695
23.193012	1455.944640	15.571712
23.513807	1464.458331	15.576730
23.717322	1478.357728	15.581747
23.704108	1466.772276	15.586765
23.986439	1472.095112	15.591783
24.070310	1491.138539	15.596800
23.843781	1488.392074	15.601818
23.957707	1479.096702	15.606835
24.183934	1486.613169	15.611853
24.052623	1471.458956	15.616871
24.066210	1457.806552	15.621888
24.175362	1463.708667	15.626906
24.245737	1473.579495	15.631923
23.959578	1464.990853	15.636941
24.154003	1469.095027	15.641959
24.268912	1482.835487	15.646976
24.119792	1478.101475	15.651994
24.393429	1458.696152	15.657011
24.052375	1462.890587	15.662029
24.352431	1474.164966	15.667047
24.531499	1497.076840	15.672064
24.016122	1471.734441	15.677082
24.715053	1454.195907	15.682099
24.466184	1465.229473	15.687117
24.574769	1475.813610	15.692135
24.586424	1475.598077	15.697152
24.521373	1463.246270	15.702170
24.592270	1461.815607	15.707187
24.122776	1463.778723	15.712205
24.288408	1465.962201	15.717223
24.210503	1455.249460	15.722240
24.336322	1454.370816	15.727258
24.548139	1463.974618	15.732275
24.335480	1474.609972	15.737293
24.461037	1462.027006	15.742311
24.566958	1454.987583	15.747328
24.300755	1460.434619	15.752346
24.416635	1461.556972	15.757363
24.433163	1465.107604	15.762381
24.543919	1476.540994	15.767399
24.790204	1474.372155	15.772416
24.650617	1482.267211	15.777434
24.889738	1501.462810	15.782451
24.921149	1495.520480	15.787469
25.038154	1472.643967	15.792487
24.939637	1471.501676	15.797504
24.923503	1479.312071	15.802522
24.842244	1461.575860	15.807539
24.688788	1459.270865	15.812557
25.084751	1481.938947	15.817575
25.025802	1488.688059	15.822592
25.019623	1491.606469	15.827610
25.295842	1489.629782	15.832627
25.107604	1486.194858	15.837645
25.286425	1454.063273	15.842663
25.213170	1453.503880	15.847680
24.975968	1458.963246	15.852698
25.090273	1459.605356	15.857715
24.970741	1457.817373	15.862733
25.007040	1469.313052	15.867751
25.198992	1479.713866	15.872768
25.226384	1476.357261	15.877786
25.539330	1484.667090	15.882803
25.245961	1499.421084	15.887821
25.117295	1481.530615	15.892839
25.401071	1495.497552	15.897856
25.281025	1493.212910	15.902874
25.525402	1500.942282	15.907891
25.700288	1498.023892	15.912909
25.388749	1469.280843	15.917927
25.590950	1475.619158	15.922944
25.608084	1484.621133	15.927962
25.470797	1477.244417	15.932979
24.990909	1488.264417	15.937997
25.351282	1486.503497	15.943015
25.603715	1474.384289	15.948032
25.306669	1487.702488	15.953050
25.482722	1496.393134	15.958067
25.185508	1496.589194	15.963085
25.574347	1469.535611	15.968103
25.469084	1487.531988	15.973120
25.206831	1500.052401	15.978138
25.891587	1491.257929	15.983155
25.796457	1520.019273	15.988173
26.094343	1516.749425	15.993191
25.930419	1486.984433	15.998208
25.669149	1487.820668	16.003226
25.707161	1500.862397	16.008243
25.732721	1514.934510	16.013261
25.737630	1508.060739	16.018279
26.026337	1504.682690	16.023296
25.756354	1511.394853	16.028314
26.230318	1490.415386	16.033331
26.228989	1498.725005	16.038349
26.046293	1514.285050	16.043367
26.094282	1516.669333	16.048384
25.950354	1508.843897	16.053402
26.426847	1498.046987	16.058419
26.397620	1506.901750	16.063437
26.791096	1502.448552	16.068455
26.276247	1499.227505	16.073472
26.151126	1490.935786	16.078490
26.094394	1461.836539	16.083507
26.029860	1474.499021	16.088525
26.027487	1506.687548	16.093543
26.316316	1512.680829	16.098560
26.208972	1499.431162	16.103578
26.260444	1482.842122	16.108595
26.298033	1504.806443	16.113613
26.455907	1519.702374	16.118631
26.497545	1500.496227	16.123648
26.158991	1497.393159	16.128666
26.297474	1495.803621	16.133683
26.375546	1497.517724	16.138701
26.319349	1495.318671	16.143719
26.604954	1496.961872	16.148736
26.495190	1503.622559	16.153754
26.558670	1504.195037	16.158771
26.456108	1502.172307	16.163789
26.804982	1527.077075	16.168807
26.937141	1537.937317	16.173824
26.772477	1535.409506	16.178842
26.869438	1540.356002	16.183859
27.004922	1525.156564	16.188877
26.768937	1511.568480	16.193895
26.868211	1488.483995	16.198912
26.477285	1504.851989	16.203930
26.793220	1528.065334	16.208947
26.771329	1540.456019	16.213965
26.849786	1539.357688	16.218983
26.928551	1526.326794	16.224000
26.561112	1532.270696	16.229018
26.998182	1535.342881	16.234035
27.253824	1525.372039	16.239053
27.131236	1517.380510	16.244071
27.102038	1516.636118	16.249088
26.911367	1537.588538	16.254106
27.209945	1530.087613	16.259123
27.039283	1517.856341	16.264141
27.021242	1531.102000	16.269159
27.422851	1525.795572	16.274176
27.090849	1540.792455	16.279194
26.855304	1529.402717	16.284211
26.859972	1520.027071	16.289229
26.952404	1534.384739	16.294247
27.187899	1555.574760	16.299264
27.483917	1562.146470	16.304282
27.883060	1559.940550	16.309299
27.463354	1555.251723	16.314317
27.488062	1550.867029	16.319335
27.835548	1537.427525	16.324352
27.569073	1543.596918	16.329370
27.573546	1529.738619	16.334387
27.579466	1533.117239	16.339405
27.478724	1536.618877	16.344423
27.531594	1538.616124	16.349440
27.460635	1558.463594	16.354458
27.760990	1563.241476	16.359475
27.671979	1558.205345	16.364493
27.483202	1558.768736	16.369511
27.907629	1549.467372	16.374528
27.538814	1554.625954	16.379546
27.577846	1566.441952	16.384563
27.807252	1554.817323	16.389581
27.571880	1564.822773	16.394599
27.370456	1554.927347	16.399616
27.618297	1536.390665	16.404634
27.908550	1545.645409	16.409651
28.216451	1579.124351	16.414669
27.965719	1573.226649	16.419687
28.325633	1572.489786	16.424704
28.314055	1572.758105	16.429722
28.033254	1569.100519	16.434739
28.090325	1550.080596	16.439757
28.224301	1536.211321	16.444775
28.363094	1539.250731	16.449792
28.158456	1543.778078	16.454810
27.991402	1551.242273	16.459827
28.158763	1556.862817	16.464845
28.099494	1565.687153	16.469863
28.492374	1574.565093	16.474880
28.575461	1590.342849	16.479898
28.256836	1566.593017	16.484915
28.462419	1553.797975	16.489933
28.334314	1566.906377	16.494951
28.463184	1582.113000	16.499968
28.535900	1580.478724	16.504986
28.465206	1566.480977	16.510003
28.448451	1569.497979	16.515021
28.288928	1591.030236	16.520039
28.800962	1575.765076	16.525056
28.497999	1564.914784	16.530074
28.644003	1562.442692	16.535091
28.817459	1570.296295	16.540109
28.762762	1588.755986	16.545127
28.842894	1582.892363	16.550144
28.753193	1578.263732	16.555162
29.131958	1572.855771	16.560179
28.822682	1568.385351	16.565197
28.781145	1579.009719	16.570215
28.812394	1555.477714	16.575232
28.952526	1561.585234	16.580250
29.005740	1577.076343	16.585267
29.041389	1580.322627	16.590285
29.095181	1576.464107	16.595303
29.045104	1547.472924	16.600320
28.805781	1552.951567	16.605338
28.724141	1564.775598	16.610355
29.180249	1558.122452	16.615373
28.664656	1561.113743	16.620391
29.133956	1566.004916	16.625408
28.995827	1589.521884	16.630426
29.069046	1586.170376	16.635443
29.242916	1579.699758	16.640461
29.186805	1574.185059	16.645479
29.179336	1569.819947	16.650496
29.216183	1590.362283	16.655514
29.094677	1580.729558	16.660531
29.035103	1571.860254	16.665549
28.883948	1564.151018	16.670567
29.564701	1593.935212	16.675584
29.471031	1606.466820	16.680602
29.278588	1606.210620	16.685619
29.522678	1591.451436	16.690637
29.568400	1600.776932	16.695655
29.717432	1609.326175	16.700672
29.307401	1600.164550	16.705690
29.520417	1583.115728	16.710707
29.555309	1597.064846	16.715725
29.412051	1615.612515	16.720743
29.710471	1587.015734	16.725760
29.513944	1595.176895	16.730778
29.532982	1604.798473	16.735795
29.643864	1582.285033	16.740813
29.709401	1596.306235	16.745831
29.909578	1584.377721	16.750848
29.802478	1592.414578	16.755866
29.513143	1598.816166	16.760883
30.013070	1602.537187	16.765901
29.837325	1617.113721	16.770919
30.091631	1630.195292	16.775936
30.129818	1630.551923	16.780954
30.265014	1615.790636	16.785971
30.314223	1617.284964	16.790989
30.028551	1640.432088	16.796007
30.419166	1634.592711	16.801024
30.297138	1604.090210	16.806042
30.211801	1601.129586	16.811059
30.327271	1598.421052	16.816077
30.310785	1594.658572	16.821095
30.263722	1576.070893	16.826112
30.358128	1580.431633	16.831130
30.454088	1597.090838	16.836147
30.448528	1594.293765	16.841165
30.272576	1583.383699	16.846183
30.542771	1588.955084	16.851200
30.485978	1602.308860	16.856218
30.536896	1623.509601	16.861235
30.768030	1608.952300	16.866253
30.283632	1590.789261	16.871271
30.484780	1599.687781	16.876288
30.799154	1619.862907	16.881306
30.451929	1631.160037	16.886323
30.770720	1615.975482	16.891341
30.671701	1627.373982	16.896359
30.719737	1616.311351	16.901376
30.639552	1607.137231	16.906394
30.460996	1616.416255	16.911411
30.952553	1606.704637	16.916429
30.332797	1608.569204	16.921447
30.836215	1607.640156	16.926464
30.833983	1613.497069	16.931482
30.528888	1617.337548	16.936499
30.726429	1606.857862	16.941517
30.798919	1615.440422	16.946535
30.936311	1611.049587	16.951552
30.895493	1618.354892	16.956570
30.728574	1635.483276	16.961587
31.210938	1627.597185	16.966605
31.079339	1650.455434	16.971623
31.211962	1652.972474	16.976640
31.397779	1653.887263	16.981658
31.093421	1660.431486	16.986675
31.631835	1634.513772	16.991693
31.246918	1634.751780	16.996711
31.414226	1638.546474	17.001728
31.379420	1647.891703	17.006746
31.394556	1642.403387	17.011763
31.634111	1634.200112	17.016781
31.612629	1646.289698	17.021799
31.696206	1639.029915	17.026816
31.617660	1645.208539	17.031834
31.308211	1646.088564	17.036851
31.505190	1638.053607	17.041869
31.567070	1636.912350	17.046887
31.552841	1644.064584	17.051904
31.561549	1643.856031	17.056922
31.635121	1656.852457	17.061939
32.006790	1631.309375	17.066957
31.653653	1626.714226	17.071975
31.609842	1629.316608	17.076992
31.745583	1649.089200	17.082010
31.535918	1645.937839	17.087027
31.568906	1634.424136	17.092045
31.561394	1647.324234	17.097063
31.671796	1643.694578	17.102080
31.939780	1639.879665	17.107098
31.969818	1653.538163	17.112115
32.286764	1659.946452	17.117133
32.454041	1676.850302	17.122151
31.789780	1647.714120	17.127168
32.143153	1664.227239	17.132186
32.110585	1679.416356	17.137203
32.441343	1657.571637	17.142221
32.710404	1659.451398	17.147239
32.208617	1652.974813	17.152256
32.381903	1627.328723	17.157274
32.247877	1646.535885	17.162291
32.454108	1653.470529	17.167309
32.168970	1635.668814	17.172327
32.183115	1632.955762	17.177344
32.575785	1656.500544	17.182362
32.312969	1685.464971	17.187379
32.511687	1672.248908	17.192397
32.540966	1659.664371	17.197415
32.502071	1662.782175	17.202432
32.489647	1679.938906	17.207450
32.867320	1677.154750	17.212467
33.027642	1653.633738	17.217485
32.768847	1671.725078	17.222503
32.423173	1671.428564	17.227520
32.615368	1665.228052	17.232538
32.590884	1653.836702	17.237555
32.702234	1650.682772	17.242573
32.704787	1666.171519	17.247591
32.377980	1669.458630	17.252608
32.655766	1668.948282	17.257626
32.404991	1664.060674	17.262643
32.829374	1661.853225	17.267661
32.891041	1683.013205	17.272679
32.987557	1680.994160	17.277696
33.360176	1671.217430	17.282714
33.011161	1688.402437	17.287731
32.971319	1684.672135	17.292749
32.945041	1691.605563	17.297767
32.795949	1673.120928	17.302784
33.323248	1687.622087	17.307802
33.095990	1705.071381	17.312819
33.193241	1672.954883	17.317837
33.367001	1681.309470	17.322855
32.890033	1680.544303	17.327872
33.418055	1690.447001	17.332890
33.159305	1706.240234	17.337907
33.380835	1693.181472	17.342925
33.397190	1700.179792	17.347943
33.669483	1716.596154	17.352960
34.000512	1717.915993	17.357978
33.964620	1713.297028	17.362995
34.158537	1682.195030	17.368013
33.963148	1683.526580	17.373031
33.754146	1696.568065	17.378048
33.932562	1689.587602	17.383066
33.680049	1675.863746	17.388083
33.712998	1666.638914	17.393101
33.916078	1676.438051	17.398119
33.772155	1675.283862	17.403136
34.115647	1675.240213	17.408154
34.007908	1677.869108	17.413171
33.890362	1671.787089	17.418189
33.792824	1664.376161	17.423207
33.498158	1679.481748	17.428224
33.749284	1686.561515	17.433242
34.159633	1691.607027	17.438259
34.169683	1719.306504	17.443277
33.905139	1717.121380	17.448295
33.830535	1694.390940	17.453312
34.110118	1697.214932	17.458330
34.036906	1700.723964	17.463347
33.961734	1705.612462	17.468365
34.005468	1702.979530	17.473383
34.180941	1710.333861	17.478400
34.501557	1715.647307	17.483418
34.403666	1720.874338	17.488435
34.726996	1734.818427	17.493453
34.242598	1715.363774	17.498471
34.419841	1731.184666	17.503488
34.296890	1728.195202	17.508506
34.633101	1730.266786	17.513523
34.845422	1743.904000	17.518541
34.581760	1731.143353	17.523559
34.533448	1725.592968	17.528576
34.776509	1742.982491	17.533594
34.842981	1739.663554	17.538611
34.753885	1718.186692	17.543629
34.966711	1721.822341	17.548647
34.982316	1737.284107	17.553664
35.104337	1735.484022	17.558682
34.634171	1742.241666	17.563699
34.638264	1726.411710	17.568717
34.800182	1724.043535	17.573735
35.070541	1747.852321	17.578752
34.983032	1732.889388	17.583770
34.999051	1731.479086	17.588787
35.021733	1726.661893	17.593805
35.044047	1723.676370	17.598823
34.753517	1710.214913	17.603840
35.398615	1732.582508	17.608858
35.193551	1740.291018	17.613875
35.254330	1727.440742	17.618893
35.034024	1743.273025	17.623911
35.296401	1757.516616	17.628928
35.754140	1755.426944	17.633946
35.476550	1778.419034	17.638963
35.680325	1758.820391	17.643981
35.743705	1736.614317	17.648999
35.603168	1754.853402	17.654016
35.471393	1749.624513	17.659034
35.658401	1748.104375	17.664051
35.689601	1739.300764	17.669069
35.768990	1740.618598	17.674087
35.726492	1749.193666	17.679104
35.896939	1766.076917	17.684122
35.697903	1746.175148	17.689139
35.803379	1735.043109	17.694157
35.789100	1753.419366	17.699175
35.855357	1760.300729	17.704192
36.150300	1742.723238	17.709210
35.939794	1757.720525	17.714227
35.676699	1756.838629	17.719245
35.886700	1739.274096	17.724263
35.404183	1749.134817	17.729280
36.108830	1764.416123	17.734298
36.252386	1765.026745	17.739315
36.162738	1747.570567	17.744333
35.963554	1737.449796	17.749351
35.803894	1746.758447	17.754368
36.310096	1745.140393	17.759386
36.450754	1767.661957	17.764403
36.184063	1777.323776	17.769421
36.271592	1769.813329	17.774439
36.206077	1753.696779	17.779456
36.417903	1766.176262	17.784474
36.389069	1771.567157	17.789491
36.460991	1786.110599	17.794509
36.465790	1763.157726	17.799527
36.467103	1755.042271	17.804544
36.617837	1753.379142	17.809562
36.770743	1771.994963	17.814579
36.266055	1761.613407	17.819597
36.854275	1746.576876	17.824615
36.759419	1770.137944	17.829632
36.547747	1765.241282	17.834650
36.582903	1774.332360	17.839667
37.008089	1777.932536	17.844685
37.159367	1792.326480	17.849703
37.319725	1795.511757	17.854720
37.274716	1784.318740	17.859738
37.014293	1768.236943	17.864755
37.077442	1755.939190	17.869773
36.827240	1761.638753	17.874791
36.621373	1792.220802	17.879808
36.913394	1802.325435	17.884826
37.162283	1785.726076	17.889843
37.021514	1785.522837	17.894861
37.273395	1787.324368	17.899879
37.145438	1801.790643	17.904896
37.367640	1791.862647	17.909914
37.480012	1780.157012	17.914931
37.357985	1791.691201	17.919949
37.346763	1798.745884	17.924967
37.328510	1798.297444	17.929984
37.537989	1782.164450	17.935002
37.414540	1785.340042	17.940019
36.959393	1792.904707	17.945037
37.779227	1815.872062	17.950055
37.935388	1822.869968	17.955072
37.819998	1826.577102	17.960090
37.999751	1812.798811	17.965107
37.848960	1800.704256	17.970125
37.845324	1776.515311	17.975143
38.019762	1786.718679	17.980160
37.977914	1801.632932	17.985178
37.949193	1785.192617	17.990195
38.001083	1782.945547	17.995213
38.023389	1776.787925	18.000231
37.604909	1782.624830	18.005248
37.844632	1784.374149	18.010266
38.316141	1818.449287	18.015283
38.167174	1821.109031	18.020301
38.518529	1795.468561	18.025319
38.470763	1812.023332	18.030336
38.563209	1822.866723	18.035354
38.659339	1807.740325	18.040371
38.366287	1778.659945	18.045389
38.253946	1774.242729	18.050407
38.548091	1798.016567	18.055424
38.653986	1815.556177	18.060442
38.803423	1792.925843	18.065459
38.274381	1781.211364	18.070477
38.580872	1773.536312	18.075495
38.733007	1795.871708	18.080512
38.851854	1784.869089	18.085530
38.696990	1790.092765	18.090547
38.515265	1805.754105	18.095565
38.547821	1801.265505	18.100583
38.538887	1783.830586	18.105600
38.836060	1791.231466	18.110618
38.540813	1799.877458	18.115635
38.478833	1807.709078	18.120653
38.877523	1791.575311	18.125671
38.619817	1795.581393	18.130688
38.511394	1825.364001	18.135706
39.107656	1838.926830	18.140723
39.045283	1828.560404	18.145741
39.419636	1830.828907	18.150759
39.608654	1835.506695	18.155776
39.346216	1831.073035	18.160794
39.331048	1827.223880	18.165811
39.626335	1838.757730	18.170829
39.524550	1822.805239	18.175847
39.219210	1824.762329	18.180864
39.286359	1815.005188	18.185882
39.181623	1821.361700	18.190899
39.233416	1814.803108	18.195917
39.408050	1828.534305	18.200935
39.582855	1833.724280	18.205952
39.419282	1819.968573	18.210970
39.497662	1807.848540	18.215987
39.258750	1824.786219	18.221005
39.550251	1822.307657	18.226023
39.590604	1821.296690	18.231040
39.548816	1845.357565	18.236058
39.935744	1862.977731	18.241075
40.101286	1862.453944	18.246093
40.008357	1844.229748	18.251111
39.878924	1842.455853	18.256128
39.929989	1861.208766	18.261146
40.248020	1858.351281	18.266163
39.866581	1858.387970	18.271181
40.123901	1842.398354	18.276199
40.213447	1852.221484	18.281216
40.027031	1873.394383	18.286234
40.363752	1854.324819	18.291251
40.236838	1842.043349	18.296269
40.313723	1846.202475	18.301287
40.690573	1857.115010	18.306304
40.582960	1851.266073	18.311322
40.646366	1830.935468	18.316339
40.467958	1837.426086	18.321357
40.573323	1849.401090	18.326375
40.889260	1853.222447	18.331392
40.622332	1838.067549	18.336410
40.619498	1802.152137	18.341427
40.288396	1829.124884	18.346445
40.489393	1820.752720	18.351463
40.796161	1838.783761	18.356480
40.632390	1843.484229	18.361498
40.891682	1820.687009	18.366515
40.876517	1820.655789	18.371533
40.997594	1839.086340	18.376551
40.867123	1856.402512	18.381568
40.782342	1837.938442	18.386586
40.818878	1817.227825	18.391603
40.724759	1827.882507	18.396621
40.877774	1824.361493	18.401639
40.864623	1841.027678	18.406656
40.922591	1837.855076	18.411674
41.283958	1843.879406	18.416691
41.166626	1863.904390	18.421709
41.419709	1869.946723	18.426727
41.533351	1861.099306	18.431744
41.301304	1860.943624	18.436762
41.634127	1849.374798	18.441779
41.200858	1866.776643	18.446797
41.467796	1866.160328	18.451815
41.723703	1848.175862	18.456832
41.632641	1871.081767	18.461850
41.506949	1873.191620	18.466867
41.458810	1859.413750	18.471885
41.366451	1844.148715	18.476903
41.567809	1853.386454	18.481920
41.137632	1874.703948	18.486938
41.898143	1870.363087	18.491955
41.552543	1870.561339	18.496973
41.938801	1874.550277	18.501991
42.211079	1885.914575	18.507008
41.846810	1895.922548	18.512026
42.061118	1881.400048	18.517043
41.930283	1885.888139	18.522061
41.965619	1899.487626	18.527079
42.094019	1892.170425	18.532096
42.061653	1889.213784	18.537114
42.174685	1881.929141	18.542131
42.226780	1881.922822	18.547149
42.372642	1867.579034	18.552167
42.385558	1874.694121	18.557184
42.133800	1898.029396	18.562202
42.488725	1903.943812	18.567219
42.889947	1907.879017	18.572237
42.575044	1890.234059	18.577255
42.915163	1876.852453	18.582272
42.299789	1882.202940	18.587290
42.585034	1876.150124	18.592307
42.448062	1903.633628	18.597325
42.844367	1911.515824	18.602343
42.702744	1903.678389	18.607360
42.621827	1922.043030	18.612378
42.835918	1916.768835	18.617395
42.841097	1899.611122	18.622413
42.763311	1903.037704	18.627431
43.022426	1905.677457	18.632448
42.991222	1919.118208	18.637466
43.167474	1901.096165	18.642483
43.197122	1901.016110	18.647501
42.908125	1901.774583	18.652519
42.835148	1910.020099	18.657536
43.024895	1923.475315	18.662554
43.236487	1909.884256	18.667571
43.011333	1908.198992	18.672589
43.123814	1922.773551	18.677607
43.277625	1928.879154	18.682624
43.186465	1937.598169	18.687642
43.580427	1935.653633	18.692659
43.450155	1925.588758	18.697677
43.589892	1922.121677	18.702695
43.794149	1916.459813	18.707712
43.772596	1937.892804	18.712730
43.815859	1934.385178	18.717747
43.895548	1936.847442	18.722765
43.421227	1927.248791	18.727783
44.090552	1917.418839	18.732800
43.903533	1922.299123	18.737818
44.001767	1917.687255	18.742835
44.046350	1919.187889	18.747853
43.988992	1937.533107	18.752871
44.268688	1927.787809	18.757888
44.096790	1909.119292	18.762906
44.123876	1920.883513	18.767923
44.409882	1904.126740	18.772941
44.000292	1911.123710	18.777959
44.574826	1911.449380	18.782976
44.145864	1921.995419	18.787994
44.467618	1895.989174	18.793011
44.458557	1905.185551	18.798029
44.172802	1917.911625	18.803047
44.581574	1896.716831	18.808064
44.383318	1924.035829	18.813082
44.377664	1918.832094	18.818099
44.701864	1934.991244	18.823117
44.459716	1952.361996	18.828135
45.121443	1941.309997	18.833152
45.070545	1930.752960	18.838170
44.898977	1932.607264	18.843187
44.783325	1932.563128	18.848205
44.715352	1928.765677	18.853223
44.791170	1930.085495	18.858240
44.912683	1945.311901	18.863258
44.795112	1945.946199	18.868275
45.168692	1936.025175	18.873293
44.879330	1950.392499	18.878311
44.772901	1949.116268	18.883328
45.255092	1945.693358	18.888346
45.356191	1927.186654	18.893363
45.180394	1937.040304	18.898381
44.923784	1951.794956	18.903399
45.623716	1965.681351	18.908416
45.548139	1971.174413	18.913434
45.618305	1951.751608	18.918451
45.577334	1934.437144	18.923469
45.454788	1956.305864	18.928487
46.046440	1950.133795	18.933504
45.400983	1930.011029	18.938522
45.543680	1933.847061	18.943539
45.717429	1934.594701	18.948557
45.790942	1951.512480	18.953575
46.005140	1951.179628	18.958592
45.449715	1952.327340	18.963610
45.621455	1962.170022	18.968627
45.771483	1970.826270	18.973645
45.553001	1975.272582	18.978663
45.956719	1952.821701	18.983680
45.916217	1957.730529	18.988698
45.725813	1960.727986	18.993715
46.199521	1957.422103	18.998733
46.113908	1977.484112	19.003751
46.422460	1995.059224	19.008768
46.383674	2002.147095	19.013786
45.988898	1998.158304	19.018803
46.369200	2001.949873	19.023821
46.523159	1979.167364	19.028839
46.406897	1982.593040	19.033856
46.168100	1997.432768	19.038874
46.370821	2008.119116	19.043891
46.952471	1990.348222	19.048909
46.743218	1982.720900	19.053927
46.700357	1995.027050	19.058944
46.695563	1996.482809	19.063962
46.820154	1981.563603	19.068979
47.248064	1989.677283	19.073997
46.796847	1995.069763	19.079015
46.680474	1984.329255	19.084032
46.820456	1989.731593	19.089050
46.767528	1984.161211	19.094067
47.124422	1998.574807	19.099085
46.829583	2020.597853	19.104103
47.113978	2026.038041	19.109120
47.506269	2014.534250	19.114138
47.228176	2006.086166	19.119155
47.625144	2019.352331	19.124173
47.377037	2021.217523	19.129191
47.517455	2007.166083	19.134208
47.415619	2017.085599	19.139226
47.477712	2020.408398	19.144243
47.733513	1993.995643	19.149261
47.603786	1999.984578	19.154279
47.712569	2015.070468	19.159296
48.024309	2007.751059	19.164314
47.991331	1985.968835	19.169331
48.285885	1990.355661	19.174349
47.842736	1999.127466	19.179367
48.000461	1992.621456	19.184384
48.019087	1998.730336	19.189402
47.814668	1982.182550	19.194419
47.954007	1993.657955	19.199437
47.790862	2020.017172	19.204455
48.100122	1994.156401	19.209472
48.154274	2000.273975	19.214490
48.195106	1997.584495	19.219507
48.467276	1978.546108	19.224525
48.411802	1997.539094	19.229543
47.851633	2005.543678	19.234560
48.165797	2001.241509	19.239578
48.708452	2011.344521	19.244595
48.702294	2006.266406	19.249613
48.667268	1999.693052	19.254631
48.533292	1984.721412	19.259648
48.248868	2006.889049	19.264666
48.278481	2014.189103	19.269683
48.808310	2020.155060	19.274701
48.960563	2039.460359	19.279719
48.999491	2024.366227	19.284736
49.060295	2005.750360	19.289754
48.751523	2024.987562	19.294771
49.046506	2035.734457	19.299789
48.986964	2030.309219	19.304807
49.248517	2016.846988	19.309824
49.323775	2017.107559	19.314842
49.079793	2029.283420	19.319859
49.240485	2019.556744	19.324877
49.152122	2031.359810	19.329895
49.048763	2021.604145	19.334912
49.019268	2009.836952	19.339930
49.171408	2006.376954	19.344947
49.450229	2011.349347	19.349965
49.558575	2020.092123	19.354983
49.299756	2012.698918	19.360000
49.546453	2012.189270	19.365018
49.505744	2040.983930	19.370035
49.811308	2055.132391	19.375053
49.662910	2055.004116	19.380071
49.815475	2038.478658	19.385088
50.000409	2050.636993	19.390106
49.621074	2040.761401	19.395123
49.843459	2048.100763	19.400141
50.014890	2043.766472	19.405159
49.632868	2038.917258	19.410176
50.271916	2051.745293	19.415194
49.841944	2055.835017	19.420211
50.251588	2035.250700	19.425229
50.165153	2047.317682	19.430247
49.894249	2038.483129	19.435264
50.018667	2044.216245	19.440282
50.323603	2072.697496	19.445299
50.536915	2074.353299	19.450317
50.813002	2064.040210	19.455335
50.897982	2080.789338	19.460352
51.144476	2070.716623	19.465370
50.732725	2071.406920	19.470387
51.004688	2055.236645	19.475405
50.695425	2070.433397	19.480423
50.783478	2078.704647	19.485440
51.289499	2062.777425	19.490458
50.895560	2067.059880	19.495475
51.109847	2048.125346	19.500493
50.936401	2053.772281	19.505511
50.934438	2056.034810	19.510528
51.311570	2055.407364	19.515546
51.443159	2060.790745	19.520563
51.389025	2041.436784	19.525581
50.916213	2048.949581	19.530599
51.346975	2037.785414	19.535616
51.539600	2038.612011	19.540634
51.324214	2045.683523	19.545651
51.590185	2047.513461	19.550669
51.267929	2048.308926	19.555687
51.157140	2061.278595	19.560704
51.457944	2061.617719	19.565722
50.958242	2050.622557	19.570739
51.147231	2043.577010	19.575757
51.392896	2062.156502	19.580775
51.411024	2070.614664	19.585792
51.745777	2071.760823	19.590810
51.618672	2089.381468	19.595827
51.617736	2085.310055	19.600845
51.529229	2082.994132	19.605863
51.742729	2081.817749	19.610880
52.085580	2094.270436	19.615898
51.896596	2109.759006	19.620915
52.380803	2099.491309	19.625933
52.186900	2098.222239	19.630951
52.209400	2103.876962	19.635968
52.173538	2110.356735	19.640986
52.450507	2112.408247	19.646003
52.405856	2087.604539	19.651021
52.410975	2078.819411	19.656039
52.500130	2098.483080	19.661056
52.713116	2100.318927	19.666074
52.552460	2106.014545	19.671091
52.620853	2087.053097	19.676109
52.660656	2086.562088	19.681127
52.552548	2112.032215	19.686144
52.851841	2133.779913	19.691162
53.093841	2128.289162	19.696179
53.274169	2120.672871	19.701197
53.211156	2122.735202	19.706215
52.741682	2131.554338	19.711232
53.404779	2127.076482	19.716250
53.301443	2121.741602	19.721267
53.126455	2120.483280	19.726285
53.266352	2106.270841	19.731303
53.228070	2114.505026	19.736320
53.326346	2127.040471	19.741338
53.428772	2130.101657	19.746355
53.298200	2119.205653	19.751373
53.383361	2125.807729	19.756391
53.681413	2106.432094	19.761408
53.673296	2116.744872	19.766426
53.597544	2118.675671	19.771443
53.474582	2113.768665	19.776461
53.674928	2138.580198	19.781479
53.652747	2153.319724	19.786496
54.228207	2139.550145	19.791514
53.852922	2147.733857	19.796531
53.963546	2142.516243	19.801549
53.981397	2129.093990	19.806567
54.029637	2145.446676	19.811584
54.227316	2147.540523	19.816602
53.862825	2142.237181	19.821619
53.965898	2125.522698	19.826637
54.431632	2140.704521	19.831655
54.139019	2177.175516	19.836672
54.681938	2177.672039	19.841690
54.817975	2176.957484	19.846707
54.822941	2169.677179	19.851725
54.678760	2154.869530	19.856743
54.610111	2155.911622	19.861760
54.792257	2167.844371	19.866778
54.936933	2169.330948	19.871795
54.803232	2170.181760	19.876813
54.995042	2154.409990	19.881831
55.001378	2167.672838	19.886848
55.189180	2169.442887	19.891866
55.003353	2161.347120	19.896883
54.883238	2157.223643	19.901901
55.122964	2159.962002	19.906919
55.341495	2159.453068	19.911936
55.331356	2173.467328	19.916954
55.326672	2159.146866	19.921971
55.061455	2144.231496	19.926989
55.477675	2165.310033	19.932007
55.299039	2166.707150	19.937024
55.401582	2153.027617	19.942042
55.342339	2160.207606	19.947059
55.608023	2182.550586	19.952077
55.696668	2171.452403	19.957095
55.532883	2200.681111	19.962112
55.926400	2183.527398	19.967130
55.832558	2192.476685	19.972147
55.371985	2190.665754	19.977165
55.549347	2186.591322	19.982183
55.871128	2173.319262	19.987200
56.069381	2168.812521	19.992218
56.011608	2169.941580	19.997235
56.147500	2191.110761	20.002253
56.505242	2210.003349	20.007271
56.247378	2208.156065	20.012288
56.779854	2215.245284	20.017306
56.069057	2208.681955	20.022323
56.721456	2198.770977	20.027341
56.828874	2192.678833	20.032359
56.581776	2208.285748	20.037376
56.764915	2199.601424	20.042394
57.040204	2216.953688	20.047411
56.598262	2220.359136	20.052429
56.951301	2200.824912	20.057447
56.932145	2195.369126	20.062464
56.837941	2213.786304	20.067482
57.046347	2220.339320	20.072499
56.962025	2207.537025	20.077517
57.258167	2211.452083	20.082535
56.822285	2205.037682	20.087552
56.838901	2201.769494	20.092570
57.372500	2203.019690	20.097587
57.188415	2206.934689	20.102605
57.343335	2190.036304	20.107623
57.254260	2205.780067	20.112640
57.351859	2217.433472	20.117658
57.357469	2210.771043	20.122675
56.920299	2217.138665	20.127693
57.750284	2229.973973	20.132711
57.864648	2247.446155	20.137728
57.905130	2239.237667	20.142746
57.935811	2240.144965	20.147763
57.888268	2240.746446	20.152781
58.148801	2236.176155	20.157799
58.023626	2226.016358	20.162816
57.976957	2230.072210	20.167834
58.043356	2234.523183	20.172851
57.670829	2235.010681	20.177869
58.131826	2226.484917	20.182887
58.278692	2246.958093	20.187904
58.523297	2267.796969	20.192922
58.237878	2259.271426	20.197939
58.406634	2259.638969	20.202957
58.509391	2241.178651	20.207975
58.661548	2251.724931	20.212992
58.518373	2265.969885	20.218010
58.627567	2258.463393	20.223027
58.551319	2254.451813	20.228045
58.576730	2254.741487	20.233063
58.693224	2256.245426	20.238080
58.405200	2261.860100	20.243098
58.657807	2255.920582	20.248115
59.077956	2259.273029	20.253133
59.178770	2274.657881	20.258151
59.077515	2279.227601	20.263168
59.271311	2289.125205	20.268186
59.308019	2272.617855	20.273203
59.534607	2270.423721	20.278221
59.657183	2263.986485	20.283239
59.572822	2276.408558	20.288256
59.379515	2264.346641	20.293274
59.676244	2261.963094	20.298291
59.600132	2272.081637	20.303309
59.893863	2250.029928	20.308327
59.627345	2261.285743	20.313344
59.698412	2261.850402	20.318362
59.717762	2270.368305	20.323379
59.706600	2255.031086	20.328397
59.905261	2240.036505	20.333415
59.780482	2260.495052	20.338432
59.800269	2273.131073	20.343450
59.962330	2278.866520	20.348467
60.503916	2276.312904	20.353485
60.510531	2281.828020	20.358503
60.169109	2291.247633	20.363520
60.343621	2294.685357	20.368538
60.475388	2289.615453	20.373555
60.321280	2283.787811	20.378573
60.573263	2288.992152	20.383591
60.665233	2293.248497	20.388608
60.763139	2278.636018	20.393626
60.831529	2272.105978	20.398643
60.722512	2274.097894	20.403661
60.941305	2282.123574	20.408679
60.989007	2279.225464	20.413696
60.918709	2268.426757	20.418714
61.051025	2265.073404	20.423731
60.986132	2283.677817	20.428749
60.922600	2290.981389	20.433767
60.928455	2295.735742	20.438784
61.075414	2320.533069	20.443802
61.529137	2312.209903	20.448819
61.155460	2306.782845	20.453837
61.584501	2308.777764	20.458855
61.725337	2326.604854	20.463872
61.590394	2314.357003	20.468890
61.481809	2294.984559	20.473907
61.537439	2316.710294	20.478925
61.608263	2310.636451	20.483943
61.698777	2326.974866	20.488960
61.952412	2329.044239	20.493978
62.166122	2338.720905	20.498995
62.004064	2335.377607	20.504013
62.441913	2336.456464	20.509031
62.073062	2343.466085	20.514048
62.189559	2330.312838	20.519066
62.545190	2317.699319	20.524083
62.015593	2329.965128	20.529101
62.545805	2340.195887	20.534119
62.532306	2339.548647	20.539136
62.319434	2332.595257	20.544154
62.469878	2310.698712	20.549171
62.268298	2337.928263	20.554189
62.431033	2333.725916	20.559207
62.667666	2337.663141	20.564224
62.599545	2341.723945	20.569242
62.914853	2358.349995	20.574259
63.000768	2367.959820	20.579277
63.257886	2359.019422	20.584295
63.226652	2355.933588	20.589312
62.979514	2378.277261	20.594330
62.890109	2364.250877	20.599347
63.083155	2349.805255	20.604365
63.289223	2359.593809	20.609383
63.314813	2362.163786	20.614400
63.404235	2334.601067	20.619418
63.548311	2331.593140	20.624435
63.297509	2356.939640	20.629453
63.476139	2360.833513	20.634471
63.751451	2375.618269	20.639488
63.770140	2379.086880	20.644506
64.186422	2370.796243	20.649523
64.320056	2366.724462	20.654541
64.142225	2353.825311	20.659559
64.261488	2335.528758	20.664576
64.253761	2343.021526	20.669594
64.243676	2342.616594	20.674611
63.976338	2333.442065	20.679629
64.175183	2327.414569	20.684647
64.404503	2343.073678	20.689664
64.095372	2358.670429	20.694682
64.530466	2344.498147	20.699699
64.436846	2363.298710	20.704717
64.362818	2378.220318	20.709735
64.633184	2361.634699	20.714752
64.467059	2368.910585	20.719770
65.005446	2353.067168	20.724787
64.584833	2361.717757	20.729805
64.749988	2366.913446	20.734823
65.075386	2353.922279	20.739840
64.771719	2359.964208	20.744858
65.116770	2379.001107	20.749875
64.831773	2387.658429	20.754893
65.092542	2389.438293	20.759911
65.494199	2388.975357	20.764928
65.598077	2388.574619	20.769946
65.698312	2374.896155	20.774963
65.609564	2382.173235	20.779981
65.467053	2400.181463	20.784999
65.768813	2395.609135	20.790016
65.299670	2381.890525	20.795034
65.385750	2388.384903	20.800051
65.752431	2380.066244	20.805069
65.632358	2395.937252	20.810087
65.570140	2390.096944	20.815104
65.934501	2401.860810	20.820122
65.716336	2409.930423	20.825139
65.933876	2415.085390	20.830157
65.785265	2400.921142	20.835175
65.987872	2401.623001	20.840192
66.047667	2417.995719	20.845210
66.513917	2433.403990	20.850227
66.394510	2425.645870	20.855245
66.525214	2430.157228	20.860263
66.674872	2442.271318	20.865280
66.524666	2454.416666	20.870298
66.889931	2434.865955	20.875315
66.742950	2432.885081	20.880333
66.783924	2434.447375	20.885351
66.922262	2421.022769	20.890368
67.119395	2428.426419	20.895386
67.228647	2425.620259	20.900403
67.268816	2438.277355	20.905421
67.113150	2430.340214	20.910439
67.207164	2414.301707	20.915456
67.376955	2415.982257	20.920474
67.035470	2422.610287	20.925491
67.483524	2433.096576	20.930509
67.138971	2445.327765	20.935527
67.477483	2442.420932	20.940544
67.613715	2458.629904	20.945562
67.666977	2458.141482	20.950579
67.609044	2444.532394	20.955597
67.400881	2455.921105	20.960615
67.691884	2461.598115	20.965632
68.003460	2477.203420	20.970650
67.828373	2468.743174	20.975667
67.978373	2473.012220	20.980685
68.241648	2487.569977	20.985703
68.422718	2474.393143	20.990720
68.726118	2464.157642	20.995738
68.723291	2471.870494	21.000755
68.722292	2480.320529	21.005773
68.642861	2491.000307	21.010791
68.762828	2463.039655	21.015808
68.883857	2450.672833	21.020826
69.035687	2453.764200	21.025843
69.067238	2462.913065	21.030861
68.514153	2442.238517	21.035879
69.017980	2454.246854	21.040896
68.899292	2461.007151	21.045914
68.959744	2458.864851	21.050931
69.371589	2459.226673	21.055949
69.348582	2479.675485	21.060967
69.360287	2474.610205	21.065984
69.438280	2450.351006	21.071002
69.499885	2438.178630	21.076019
69.324861	2460.524087	21.081037
69.298715	2467.250003	21.086055
69.246891	2449.481506	21.091072
69.267885	2459.334561	21.096090
69.271844	2464.413242	21.101107
69.241238	2491.278448	21.106125
69.190817	2494.641791	21.111143
69.448429	2494.843303	21.116160
69.386707	2519.470942	21.121178
69.566634	2516.312786	21.126195
69.753623	2511.692077	21.131213
69.966838	2531.055037	21.136231
70.242519	2523.315818	21.141248
70.422257	2551.347757	21.146266
70.220957	2546.599303	21.151283
70.546797	2540.917610	21.156301
71.022795	2546.673317	21.161319
71.203050	2536.329004	21.166336
71.181595	2548.691697	21.171354
71.140520	2534.070056	21.176371
71.516257	2503.447588	21.181389
71.168838	2508.220233	21.186407
71.244014	2511.806487	21.191424
71.301159	2500.339217	21.196442
71.031958	2489.189030	21.201459
71.053766	2497.172584	21.206477
71.020802	2506.900157	21.211495
71.718834	2534.347874	21.216512
71.342627	2529.534051	21.221530
71.319374	2522.955673	21.226547
71.541919	2517.671905	21.231565
71.276570	2535.731492	21.236583
71.202691	2522.385363	21.241600
71.245219	2521.276761	21.246618
71.838247	2531.637406	21.251635
71.875822	2538.352035	21.256653
71.727657	2547.715856	21.261671
72.349238	2546.358242	21.266688
72.147832	2564.387023	21.271706
72.261426	2564.244282	21.276723
72.668069	2534.906014	21.281741
72.420027	2546.812131	21.286759
72.534192	2542.300873	21.291776
72.109699	2536.410351	21.296794
72.621014	2551.108057	21.301811
72.588459	2546.835381	21.306829
72.256025	2545.786181	21.311847
72.462135	2537.369581	21.316864
72.748455	2547.607324	21.321882
72.919586	2583.586573	21.326899
73.116366	2577.518383	21.331917
72.896233	2566.253355	21.336935
73.509968	2565.002138	21.341952
73.246953	2583.981334	21.346970
72.946960	2580.292721	21.351987
73.463937	2580.999717	21.357005
73.388673	2573.893773	21.362023
73.542626	2566.127805	21.367040
73.467951	2562.907790	21.372058
73.443902	2567.411302	21.377075
73.788626	2568.174120	21.382093
73.325726	2574.592393	21.387111
73.747697	2580.338342	21.392128
73.939359	2585.849165	21.397146
74.205435	2599.681872	21.402163
74.341831	2612.465512	21.407181
74.253003	2616.352670	21.412199
73.925971	2594.688734	21.417216
74.246040	2585.336288	21.422234
74.140678	2598.025438	21.427251
74.495386	2603.736062	21.432269
74.293907	2592.240407	21.437287
74.370843	2589.656651	21.442304
74.294565	2608.618994	21.447322
74.484949	2631.679200	21.452339
75.035615	2614.166018	21.457357
74.878226	2622.209165	21.462375
74.758850	2626.818787	21.467392
74.887353	2616.197582	21.472410
74.833699	2630.192584	21.477427
75.196761	2616.873563	21.482445
74.975426	2624.312016	21.487463
75.392399	2634.769530	21.492480
75.598669	2649.692123	21.497498
75.959239	2654.171663	21.502515
75.907059	2643.310061	21.507533
75.710051	2644.793020	21.512551
75.844866	2642.450638	21.517568
75.712497	2634.567407	21.522586
75.513668	2641.357953	21.527603
75.714790	2635.086689	21.532621
75.677015	2653.697304	21.537639
75.702306	2645.890164	21.542656
76.278970	2652.393534	21.547674
76.190431	2668.267289	21.552691
76.053105	2651.006711	21.557709
75.955074	2664.375509	21.562727
76.437411	2653.859759	21.567744
76.676716	2668.752703	21.572762
76.272960	2679.217741	21.577779
76.794327	2664.685487	21.582797
76.810599	2659.392653	21.587815
76.762001	2669.231165	21.592832
76.987599	2701.070598	21.597850
77.102098	2693.508695	21.602867
77.249874	2681.406717	21.607885
77.197918	2694.738995	21.612903
77.300753	2689.556632	21.617920
77.401019	2694.957812	21.622938
77.505688	2677.439924	21.627955
77.883107	2672.007497	21.632973
77.478490	2689.507292	21.637991
77.589515	2696.130927	21.643008
77.810812	2679.688095	21.648026
77.485536	2675.105144	21.653043
77.604435	2683.498476	21.658061
77.336835	2678.510382	21.663079
77.570988	2667.120217	21.668096
77.610531	2694.751238	21.673114
77.704669	2726.643349	21.678131
77.901201	2715.861249	21.683149
78.448008	2694.015375	21.688167
78.342073	2703.745684	21.693184
78.210021	2718.319781	21.698202
78.489282	2721.424983	21.703219
78.769402	2740.434682	21.708237
78.489484	2735.627319	21.713255
78.657353	2733.229075	21.718272
78.727051	2749.580631	21.723290
79.033651	2742.488660	21.728307
78.825147	2722.193935	21.733325
78.819042	2727.227916	21.738343
79.047662	2745.890473	21.743360
79.371531	2746.089702	21.748378
79.258510	2738.835611	21.753395
79.320761	2730.786331	21.758413
79.494848	2745.413394	21.763431
79.552442	2755.253504	21.768448
79.894333	2751.405833	21.773466
79.754949	2756.695674	21.778483
79.882250	2765.742098	21.783501
79.987288	2739.701057	21.788519
80.053400	2737.591439	21.793536
79.962267	2737.319164	21.798554
79.895074	2761.947899	21.803571
80.081215	2747.159392	21.808589
79.997253	2737.935029	21.813607
80.406517	2747.984110	21.818624
80.360390	2751.208433	21.823642
80.155982	2778.551814	21.828659
80.643479	2764.695639	21.833677
80.590440	2769.153810	21.838695
80.599595	2781.972001	21.843712
80.714394	2794.351740	21.848730
80.779483	2783.914300	21.853747
80.782429	2754.205771	21.858765
80.644751	2782.399822	21.863783
80.740946	2800.025813	21.868800
81.048058	2793.438193	21.873818
81.328991	2819.189054	21.878835
81.360001	2791.565493	21.883853
81.436397	2787.893557	21.888871
81.511375	2795.609460	21.893888
81.701511	2784.967522	21.898906
81.379052	2793.629293	21.903923
81.746399	2797.418678	21.908941
81.914448	2806.540861	21.913959
81.933964	2825.008769	21.918976
82.367949	2832.339819	21.923994
82.362029	2829.446530	21.929011
82.214177	2802.637045	21.934029
82.344728	2816.321500	21.939047
82.228925	2835.265854	21.944064
82.309801	2816.522377	21.949082
82.490619	2801.200716	21.954099
82.876153	2810.891408	21.959117
82.351950	2817.756072	21.964135
82.544347	2827.904026	21.969152
83.040978	2819.017865	21.974170
82.894007	2833.249898	21.979187
83.046631	2843.122977	21.984205
82.851813	2852.744068	21.989223
83.091030	2841.978445	21.994240
83.286428	2831.648752	21.999258
83.224510	2847.965477	22.004275
83.266311	2835.855696	22.009293
83.147942	2827.778739	22.014311
83.195128	2839.690816	22.019328
83.654624	2869.229457	22.024346
83.616683	2866.740809	22.029363
83.624828	2876.311843	22.034381
83.792115	2884.680558	22.039399
83.799005	2869.068322	22.044416
84.120303	2859.475776	22.049434
83.895595	2866.589552	22.054451
84.135254	2874.272180	22.059469
84.018804	2889.734491	22.064487
83.945717	2883.783010	22.069504
84.695009	2861.049616	22.074522
84.490690	2890.160858	22.079539
84.711126	2898.932359	22.084557
85.081771	2886.264721	22.089575
84.794360	2874.951142	22.094592
85.116046	2871.464214	22.099610
84.997507	2888.815399	22.104627
85.087341	2885.814557	22.109645
85.266609	2870.932985	22.114663
85.327348	2872.825085	22.119680
85.384529	2889.985838	22.124698
85.578779	2903.703737	22.129715
85.780723	2902.897659	22.134733
85.730573	2899.470595	22.139751
85.853359	2911.862100	22.144768
86.119162	2900.328953	22.149786
86.146464	2909.550233	22.154803
86.134604	2885.387666	22.159821
85.893142	2879.328988	22.164839
85.768114	2904.917777	22.169856
86.135754	2901.585235	22.174874
86.145244	2903.701921	22.179891
86.227374	2901.540625	22.184909
86.209259	2890.360661	22.189927
86.243991	2906.805159	22.194944
86.572735	2919.392133	22.199962
86.559228	2933.093609	22.204979
86.519300	2925.966703	22.209997
86.823574	2921.783322	22.215015
86.441005	2922.732870	22.220032
86.769005	2934.855276	22.225050
87.032043	2947.270084	22.230067
87.184271	2946.277953	22.235085
87.608703	2931.142846	22.240103
87.466166	2932.915807	22.245120
87.654036	2935.276017	22.250138
87.394279	2951.198236	22.255155
87.716553	2948.419962	22.260173
87.971366	2936.337099	22.265191
87.615754	2937.541609	22.270208
87.801133	2949.411843	22.275226
88.144560	2969.071318	22.280243
87.976325	2969.950416	22.285261
88.342180	2964.870148	22.290279
88.409134	2964.675079	22.295296
88.755271	2949.643432	22.300314
88.472907	2964.447496	22.305331
88.768162	2966.924200	22.310349
88.628840	2974.021161	22.315367
88.273820	2968.909836	22.320384
88.521826	2958.856368	22.325402
88.556445	2951.893684	22.330419
88.623423	2962.497043	22.335437
88.677635	2984.158020	22.340455
88.949553	3004.788490	22.345472
89.175924	2990.238151	22.350490
89.260864	3006.764211	22.355507
88.983786	3015.787656	22.360525
89.304784	2982.130548	22.365543
89.531810	2997.176608	22.370560
89.776875	3015.480127	22.375578
89.635447	3028.953054	22.380595
89.598204	3009.154978	22.385613
89.732144	3016.757128	22.390631
90.233726	3012.510413	22.395648
90.235343	2994.691712	22.400666
90.192033	3007.983271	22.405683
89.819339	3032.194474	22.410701
90.317254	3018.210383	22.415719
90.226394	3018.152008	22.420736
90.351981	3027.260083	22.425754
90.476281	3050.109030	22.430771
90.412168	3057.958075	22.435789
90.581592	3039.838003	22.440807
90.580885	3038.287155	22.445824
90.844501	3056.525066	22.450842
91.003731	3063.729604	22.455859
91.044430	3057.114448	22.460877
91.605406	3052.101897	22.465895
91.346504	3073.409868	22.470912
91.474341	3060.630260	22.475930
91.431768	3054.003869	22.480947
91.392426	3060.646408	22.485965
91.797359	3082.718213	22.490983
91.584877	3090.410711	22.496000
91.791228	3098.869337	22.501018
91.690076	3088.914422	22.506035
91.957698	3096.306747	22.511053
92.166934	3085.100686	22.516071
92.084144	3084.605005	22.521088
92.309043	3113.076714	22.526106
92.687419	3104.652203	22.531123
92.663125	3108.248343	22.536141
92.997759	3097.274671	22.541159
92.993014	3086.865098	22.546176
93.039260	3089.054073	22.551194
93.331706	3089.745057	22.556211
93.194368	3092.555637	22.561229
93.489411	3098.552259	22.566247
93.292299	3087.415115	22.571264
93.445968	3093.490207	22.576282
93.405950	3106.572473	22.581299
93.147543	3097.174578	22.586317
93.476874	3079.580530	22.591335
93.581666	3090.565872	22.596352
93.263957	3111.753117	22.601370
93.842393	3126.179883	22.606387
93.951451	3134.526471	22.611405
94.067763	3125.189459	22.616423
94.313978	3134.751428	22.621440
94.134714	3117.920042	22.626458
94.038840	3108.887559	22.631475
94.032320	3136.854900	22.636493
94.786560	3162.453331	22.641511
94.587735	3151.997645	22.646528
94.342820	3145.734140	22.651546
94.614090	3158.122171	22.656563
94.774707	3169.284543	22.661581
94.631969	3157.651213	22.666599
94.639313	3161.425383	22.671616
94.876889	3167.191201	22.676634
95.189465	3168.614015	22.681651
94.965258	3178.452543	22.686669
95.071410	3180.049807	22.691687
95.164844	3186.896616	22.696704
95.507830	3192.273216	22.701722
95.851338	3204.187981	22.706739
95.849591	3214.090744	22.711757
96.119970	3190.867958	22.716775
96.353471	3209.820200	22.721792
96.332404	3200.242685	22.726810
96.309669	3194.465813	22.731827
96.340143	3203.345839	22.736845
96.651503	3193.231952	22.741863
96.593691	3207.782828	22.746880
96.401796	3208.171612	22.751898
96.523015	3183.119360	22.756915
96.725151	3177.261837	22.761933
96.940233	3180.150796	22.766951
96.897205	3195.242857	22.771968
96.884304	3212.485031	22.776986
97.052180	3214.564762	22.782003
96.623635	3217.266613	22.787021
97.309623	3209.597818	22.792039
97.328693	3224.285005	22.797056
97.139216	3239.172200	22.802074
97.962297	3242.380735	22.807091
97.548263	3247.629326	22.812109
97.835078	3252.404666	22.817127
97.983205	3249.356526	22.822144
97.873175	3246.792533	22.827162
97.989533	3239.621352	22.832179
98.199349	3246.029710	22.837197
98.379292	3256.913194	22.842215
98.194075	3265.663364	22.847232
98.488537	3258.533208	22.852250
98.910080	3272.673671	22.857267
98.888701	3272.489652	22.862285
98.845304	3274.119708	22.867303
98.845111	3265.097305	22.872320
99.007788	3269.959691	22.877338
99.167639	3274.323780	22.882355
98.718269	3287.857660	22.887373
99.144480	3272.620559	22.892391
99.515566	3283.229983	22.897408
99.595515	3301.909516	22.902426
99.751262	3298.154079	22.907443
99.292419	3287.164360	22.912461
99.568012	3274.530810	22.917479
99.802962	3316.787570	22.922496
99.691051	3331.730730	22.927514
99.984921	3314.668599	22.932531
100.181412	3309.085553	22.937549
100.129009	3312.571042	22.942567
100.467211	3318.837755	22.947584
100.618215	3343.937808	22.952602
100.900679	3330.138826	22.957619
100.326003	3345.837140	22.962637
101.009672	3328.638147	22.967655
101.197730	3324.682306	22.972672
101.004917	3341.113299	22.977690
101.155134	3332.353570	22.982707
101.168809	3334.184023	22.987725
101.581883	3331.850473	22.992743
101.705697	3333.779446	22.997760
101.593867	3325.653711	23.002778
101.769770	3320.995227	23.007795
102.067215	3350.144883	23.012813
101.708227	3326.783004	23.017831
102.088878	3303.154071	23.022848
101.964112	3308.572577	23.027866
101.854989	3317.057472	23.032883
101.604454	3352.114994	23.037901
101.990763	3352.415322	23.042919
102.240520	3334.640846	23.047936
102.294189	3350.759493	23.052954
102.557504	3368.527597	23.057971
102.394129	3376.043242	23.062989
102.371945	3367.518457	23.068007
102.808501	3375.815586	23.073024
102.684809	3391.078829	23.078042
102.825117	3401.476691	23.083059
103.076340	3403.153147	23.088077
103.339983	3399.076736	23.093095
103.636568	3407.863502	23.098112
103.375619	3422.049564	23.103130
103.998815	3403.128760	23.108147
103.849389	3413.725280	23.113165
103.957923	3412.360653	23.118183
104.071933	3402.379232	23.123200
103.911418	3403.965078	23.128218
103.985021	3406.134028	23.133235
104.251324	3413.324186	23.138253
104.292596	3423.372126	23.143271
104.679218	3428.943548	23.148288
104.369315	3426.162774	23.153306
104.664495	3425.610135	23.158323
104.571734	3431.289905	23.163341
104.539869	3426.597618	23.168359
104.802796	3430.619554	23.173376
104.989230	3444.427211	23.178394
105.132459	3450.403590	23.183411
105.005038	3474.819027	23.188429
105.117097	3463.972025	23.193447
105.612973	3454.100090	23.198464
105.352300	3462.446344	23.203482
105.783615	3477.102655	23.208499
105.957150	3470.303182	23.213517
106.043469	3468.502499	23.218535
106.141387	3468.883946	23.223552
106.264772	3473.699351	23.228570
106.252034	3470.619488	23.233587
106.516110	3466.531375	23.238605
106.493791	3460.758862	23.243623
106.642928	3466.072325	23.248640
106.611525	3477.888246	23.253658
106.664438	3482.726323	23.258675
106.984364	3478.783688	23.263693
106.758651	3480.362995	23.268711
107.025449	3479.162743	23.273728
107.203566	3482.950305	23.278746
107.212280	3477.958017	23.283763
107.340206	3498.520040	23.288781
107.646405	3519.519911	23.293799
107.883341	3512.898312	23.298816
107.698667	3507.745469	23.303834
107.614093	3512.170880	23.308851
107.953564	3533.746126	23.313869
107.955249	3523.152929	23.318887
108.138875	3513.495336	23.323904
107.967006	3518.894338	23.328922
108.333286	3553.388229	23.333939
108.428960	3568.644333	23.338957
108.461359	3552.303827	23.343975
108.529829	3524.012388	23.348992
108.499664	3549.566690	23.354010
108.900759	3546.608176	23.359027
109.007930	3548.906429	23.364045
108.740659	3545.891050	23.369063
109.250231	3560.853969	23.374080
109.299011	3574.186501	23.379098
109.639903	3563.340589	23.384115
109.634472	3557.156624	23.389133
109.596077	3550.566727	23.394151
109.938512	3560.645889	23.399168
109.569102	3574.719513	23.404186
109.827004	3565.972171	23.409203
109.771784	3587.424342	23.414221
110.030914	3599.123850	23.419239
109.953590	3592.881283	23.424256
109.732996	3611.556135	23.429274
110.205575	3616.926233	23.434291
110.353782	3606.444780	23.439309
110.088238	3633.313597	23.444327
110.956473	3641.819043	23.449344
110.576254	3649.958399	23.454362
110.666636	3634.357770	23.459379
111.215353	3643.874204	23.464397
111.067890	3649.574705	23.469415
111.293968	3661.006319	23.474432
111.718794	3675.320809	23.479450
111.870026	3689.576003	23.484467
112.076366	3685.025561	23.489485
112.073870	3664.513280	23.494503
112.200743	3661.183950	23.499520
112.150697	3677.663553	23.504538
112.317551	3673.666248	23.509555
112.517754	3664.711867	23.514573
112.258061	3654.986310	23.519591
112.492061	3670.351537	23.524608
112.115461	3681.286542	23.529626
112.739065	3696.213429	23.534643
113.071317	3684.766545	23.539661
112.820509	3696.949965	23.544679
113.251202	3708.117308	23.549696
113.094710	3714.429711	23.554714
113.054632	3689.355854	23.559731
113.279729	3707.694203	23.564749
113.445126	3727.576966	23.569767
113.823877	3725.348629	23.574784
114.047834	3741.274598	23.579802
113.934709	3735.735475	23.584819
114.055907	3713.917158	23.589837
113.979970	3735.844969	23.594855
114.306780	3734.239143	23.599872
114.438634	3739.299277	23.604890
114.236264	3745.330319	23.609907
114.601055	3764.256629	23.614925
114.607050	3767.527665	23.619943
114.557221	3746.711309	23.624960
114.844743	3745.679451	23.629978
114.836113	3750.713200	23.634995
115.186342	3762.386362	23.640013
115.158006	3782.619098	23.645031
115.413180	3791.402691	23.650048
115.196817	3782.941848	23.655066
115.310301	3780.462280	23.660083
115.837554	3797.347957	23.665101
115.588147	3801.985124	23.670119
115.926713	3797.233088	23.675136
115.816446	3811.580421	23.680154
116.098987	3802.484214	23.685171
116.142696	3799.283745	23.690189
116.237416	3837.344937	23.695207
116.812353	3816.405172	23.700224
116.835723	3812.153412	23.705242
116.867087	3817.778169	23.710259
117.405704	3828.607711	23.715277
117.514872	3812.911285	23.720295
117.682196	3802.792655	23.725312
117.424085	3802.767621	23.730330
117.340081	3820.025963	23.735347
117.450863	3822.598051	23.740365
117.244171	3821.787804	23.745383
117.464515	3801.446378	23.750400
117.639321	3802.299936	23.755418
117.253759	3815.643430	23.760435
117.972300	3832.395969	23.765453
117.969752	3837.137817	23.770471
118.156996	3832.213939	23.775488
118.091729	3832.235380	23.780506
118.072340	3834.132178	23.785523
118.244500	3845.050237	23.790541
118.457361	3879.708782	23.795559
118.494909	3869.591476	23.800576
118.415496	3859.497047	23.805594
118.472236	3883.400841	23.810611
118.862746	3902.572268	23.815629
118.870520	3906.653419	23.820647
119.030970	3911.415203	23.825664
119.276256	3914.155029	23.830682
119.408028	3925.081392	23.835699
119.821849	3913.397254	23.840717
119.870369	3951.351014	23.845735
120.085030	3943.768800	23.850752
120.093363	3946.684983	23.855770
120.192001	3950.450756	23.860787
120.864023	3955.163451	23.865805
120.317038	3959.397306	23.870823
120.315763	3953.925049	23.875840
120.968201	3942.420737	23.880858
120.777608	3976.170637	23.885875
121.329223	3960.314342	23.890893
121.142218	3957.394666	23.895911
121.177856	3981.084592	23.900928
121.480833	3973.225187	23.905946
121.615070	3967.353392	23.910963
121.939337	3958.150795	23.915981
121.869633	3977.322972	23.920999
122.049103	3989.919745	23.926016
122.215604	3993.484169	23.931034
122.062032	3998.227401	23.936051
122.287198	3981.105815	23.941069
122.034470	3992.992164	23.946087
122.024259	3997.873114	23.951104
122.348188	3989.501608	23.956122
122.485045	4011.530860	23.961139
122.698067	4019.821578	23.966157
122.647057	4027.559901	23.971175
122.740354	4023.166812	23.976192
123.140650	4034.536649	23.981210
123.003288	4057.105344	23.986227
123.471676	4061.873767	23.991245
123.264813	4060.991885	23.996263
123.479434	4057.938899	24.001280
123.954601	4061.679881	24.006298
123.772685	4076.221768	24.011315
124.164578	4078.975389	24.016333
124.151405	4073.045632	24.021351
124.329656	4077.931684	24.026368
124.238339	4060.691450	24.031386
124.306955	4082.540357	24.036403
124.386897	4097.427950	24.041421
124.541171	4087.014457	24.046439
124.719120	4095.864525	24.051456
125.004207	4111.614642	24.056474
124.725593	4114.910932	24.061491
125.120437	4131.362186	24.066509
125.251947	4135.362719	24.071527
125.434450	4113.093181	24.076544
125.838740	4113.961393	24.081562
125.495729	4134.194620	24.086579
126.043602	4144.747280	24.091597
126.167967	4144.275598	24.096615
126.101912	4143.256670	24.101632
126.546517	4149.333316	24.106650
126.369535	4159.263673	24.111667
126.633912	4137.557314	24.116685
126.666529	4153.080701	24.121703
126.476100	4154.701880	24.126720
126.749247	4156.040561	24.131738
127.185988	4177.859875	24.136755
127.457437	4164.881027	24.141773
127.222649	4164.552939	24.146791
127.125723	4158.676358	24.151808
127.540871	4152.021890	24.156826
127.697094	4160.650400	24.161843
127.981478	4183.210610	24.166861
128.205939	4199.041303	24.171879
128.293142	4195.279457	24.176896
128.566733	4190.532922	24.181914
128.305886	4198.451273	24.186931
128.388994	4197.708860	24.191949
128.697240	4208.975145	24.196967
128.645225	4200.385739	24.201984
128.644497	4172.093920	24.207002
128.791952	4207.076591	24.212019
128.811789	4219.972751	24.217037
128.979627	4225.345588	24.222055
129.051779	4223.674318	24.227072
129.674721	4229.820736	24.232090
129.537572	4260.664916	24.237107
129.928948	4264.223346	24.242125
129.928413	4258.903608	24.247143
129.766022	4244.809425	24.252160
129.781524	4243.238455	24.257178
129.570138	4273.101663	24.262195
130.108537	4274.445341	24.267213
130.470215	4263.721880	24.272231
130.604579	4271.052937	24.277248
130.807380	4299.308450	24.282266
130.303255	4328.111519	24.287283
130.637879	4306.429142	24.292301
130.694385	4294.680932	24.297319
130.844172	4318.164724	24.302336
131.388708	4346.549674	24.307354
131.294332	4343.499662	24.312371
131.500045	4336.110067	24.317389
131.747883	4342.981480	24.322407
131.609921	4350.831966	24.327424
131.932947	4348.638144	24.332442
131.907437	4364.268588	24.337459
132.420048	4379.199521	24.342477
132.812367	4387.075390	24.347495
132.537213	4372.998148	24.352512
132.612811	4364.514331	24.357530
132.760780	4382.468800	24.362547
133.072116	4390.978503	24.367565
133.038687	4383.867370	24.372583
132.945192	4380.117622	24.377600
133.693987	4401.174296	24.382618
133.458952	4424.153745	24.387635
134.207572	4410.101390	24.392653
133.968256	4391.758901	24.397671
133.859245	4403.868264	24.402688
133.884263	4402.540973	24.407706
134.236773	4390.741022	24.412723
134.233280	4412.213741	24.417741
134.496769	4401.751677	24.422759
134.448800	4419.539360	24.427776
134.898501	4407.729635	24.432794
134.801237	4421.801180	24.437811
134.979348	4446.039911	24.442829
134.723569	4426.186762	24.447847
134.591466	4423.244145	24.452864
135.264980	4440.128407	24.457882
135.124086	4464.528537	24.462899
135.307728	4449.472291	24.467917
135.526560	4473.846852	24.472935
135.583441	4487.668189	24.477952
135.526867	4483.751296	24.482970
135.885347	4489.046268	24.487987
136.203491	4521.673163	24.493005
136.286672	4517.637896	24.498023
135.988086	4507.182026	24.503040
136.796042	4522.446568	24.508058
136.736800	4542.331870	24.513075
137.147146	4531.834428	24.518093
137.189721	4541.197660	24.523111
137.216953	4534.922476	24.528128
137.334986	4537.365536	24.533146
137.789385	4555.103433	24.538163
137.813154	4566.505960	24.543181
138.219512	4564.604631	24.548199
137.986687	4559.684976	24.553216
138.286704	4571.654838	24.558234
138.038475	4545.452401	24.563251
138.190090	4553.748436	24.568269
138.655216	4583.284317	24.573287
138.400203	4595.727004	24.578304
138.778729	4591.694882	24.583322
139.027387	4579.172596	24.588339
138.924696	4589.669678	24.593357
139.260629	4603.639099	24.598375
139.282821	4623.487820	24.603392
139.623078	4617.838425	24.608410
139.777322	4610.040677	24.613427
139.779724	4630.551326	24.618445
140.085297	4624.865141	24.623463
139.742310	4622.708105	24.628480
140.365843	4624.196802	24.633498
140.666375	4651.329349	24.638515
140.500397	4637.234613	24.643533
140.804999	4646.407763	24.648551
140.604605	4653.860852	24.653568
140.964719	4631.197056	24.658586
141.057213	4646.841357	24.663603
141.181719	4672.629036	24.668621
141.440818	4666.284777	24.673639
141.437584	4670.153779	24.678656
141.392535	4664.708977	24.683674
141.523481	4667.989280	24.688691
141.463504	4700.781787	24.693709
141.899810	4691.446074	24.698727
141.679718	4684.119981	24.703744
142.057785	4676.330885	24.708762
142.210431	4717.174782	24.713779
141.992844	4732.824738	24.718797
142.446512	4714.080355	24.723815
142.536674	4723.057885	24.728832
142.736964	4739.844295	24.733850
143.047425	4758.314469	24.738867
142.959924	4758.223837	24.743885
143.548850	4743.956628	24.748903
143.430474	4766.421644	24.753920
143.733830	4779.084808	24.758938
143.708040	4793.225587	24.763955
143.844582	4768.905634	24.768973
144.094036	4764.113702	24.773991
144.215029	4785.347078	24.779008
144.483486	4783.955119	24.784026
144.496049	4790.982931	24.789043
144.557280	4802.362118	24.794061
144.672868	4792.580919	24.799079
144.483707	4801.811341	24.804096
144.850660	4813.421907	24.809114
145.197102	4817.544187	24.814131
145.379369	4826.580180	24.819149
145.448842	4831.528934	24.824167
145.462721	4831.780603	24.829184
145.848013	4839.833849	24.834202
146.100889	4859.503810	24.839219
145.998916	4849.463644	24.844237
146.328212	4843.868340	24.849255
146.260161	4873.910592	24.854272
146.274280	4892.923987	24.859290
146.514727	4883.615405	24.864307
146.665750	4881.663710	24.869325
147.060537	4894.777215	24.874343
146.892162	4915.539687	24.879360
146.866033	4917.762928	24.884378
147.406664	4915.809449	24.889395
147.255272	4924.228192	24.894413
147.552722	4940.433016	24.899431
147.698116	4939.997994	24.904448
147.989913	4955.844714	24.909466
148.364117	4962.219144	24.914483
148.541324	4951.515062	24.919501
148.707694	4956.593121	24.924519
148.592860	4948.187696	24.929536
148.793727	4960.922275	24.934554
149.519271	4985.444229	24.939571
149.412843	4983.425219	24.944589
149.747038	4979.342056	24.949607
149.694333	4975.294478	24.954624
149.817354	4984.217911	24.959642
149.682239	4994.108417	24.964659
149.692743	4973.656626	24.969677
149.842519	4997.504050	24.974695
149.895540	5007.620171	24.979712
150.277816	5001.133376	24.984730
150.369983	5004.850082	24.989747
150.550766	5015.506518	24.994765
150.338696	5025.649918	24.999783
150.515952	5023.800565	25.004800
150.588657	5034.692590	25.009818
150.901027	5065.912914	25.014835
151.271028	5073.247149	25.019853
151.452212	5057.477722	25.024871
151.540769	5059.333998	25.029888
151.509454	5087.581994	25.034906
151.950793	5098.711187	25.039923
151.944843	5108.927671	25.044941
152.511761	5100.641012	25.049959
152.641988	5091.317054	25.054976
152.546510	5106.494054	25.059994
152.884655	5120.660823	25.065011
152.866424	5127.490328	25.070029
153.262105	5113.453536	25.075047
153.112053	5108.996019	25.080064
152.862228	5126.932433	25.085082
153.296146	5113.930674	25.090099
153.110329	5130.829733	25.095117
153.687238	5139.604633	25.100135
153.790166	5147.420441	25.105152
153.515120	5138.224840	25.110170
154.192337	5151.529693	25.115187
154.176039	5180.294282	25.120205
154.264078	5191.861847	25.125223
154.059999	5180.966276	25.130240
154.154232	5180.599545	25.135258
154.380992	5193.639491	25.140275
154.856231	5228.325416	25.145293
154.989029	5220.211217	25.150311
155.073515	5211.343179	25.155328
155.358438	5238.899420	25.160346
156.044246	5248.443806	25.165363
155.953703	5265.702473	25.170381
156.182824	5253.811627	25.175399
156.184602	5261.563496	25.180416
156.003849	5280.030023	25.185434
156.566920	5272.492746	25.190451
156.511245	5286.327487	25.195469
156.774417	5289.786867	25.200487
157.012782	5294.174384	25.205504
157.213101	5298.192983	25.210522
157.597095	5316.222922	25.215539
157.524364	5308.404061	25.220557
157.591748	5285.924695	25.225575
157.786162	5308.136047	25.230592
157.712476	5340.016396	25.235610
158.019782	5340.041237	25.240627
158.038250	5324.098422	25.245645
158.467488	5351.678263	25.250663
158.473061	5368.980218	25.255680
158.696258	5366.389355	25.260698
158.846692	5369.490204	25.265715
158.823465	5387.076868	25.270733
159.399501	5380.310255	25.275751
159.518873	5392.542498	25.280768
159.073413	5404.372396	25.285786
159.885830	5403.486978	25.290803
159.594586	5410.212109	25.295821
160.202249	5421.196332	25.300839
160.293993	5415.043208	25.305856
160.282291	5428.554657	25.310874
160.398472	5448.492054	25.315891
160.547035	5445.186320	25.320909
160.608384	5434.402230	25.325927
160.780004	5447.801906	25.330944
160.835270	5477.473753	25.335962
161.288439	5465.618563	25.340979
161.288051	5489.401786	25.345997
161.043399	5499.483552	25.351015
161.667930	5504.363247	25.356032
161.906382	5505.123115	25.361050
162.190532	5499.124788	25.366067
161.894157	5532.743571	25.371085
162.411749	5529.750873	25.376103
162.672895	5537.886811	25.381120
162.500961	5530.230299	25.386138
162.912812	5563.132494	25.391155
163.086766	5565.031416	25.396173
163.221028	5561.720934	25.401191
163.680478	5562.671463	25.406208
163.529388	5566.465902	25.411226
163.659540	5573.526608	25.416243
163.291890	5573.279890	25.421261
163.830768	5575.338997	25.426279
164.483323	5594.836365	25.431296
164.031770	5589.737159	25.436314
164.576209	5606.646389	25.441331
164.450000	5618.326842	25.446349
164.232835	5622.137724	25.451367
164.772187	5638.784826	25.456384
164.900696	5655.031305	25.461402
165.330149	5657.128977	25.466419
165.318445	5655.661577	25.471437
165.299348	5663.484027	25.476455
165.264296	5684.321954	25.481472
165.285714	5692.281432	25.486490
165.279697	5719.494058	25.491507
165.449634	5715.369340	25.496525
166.340047	5719.724832	25.501543
166.844336	5729.895998	25.506560
166.737001	5749.636843	25.511578
167.035949	5751.831294	25.516595
167.259148	5745.749631	25.521613
167.526639	5757.352930	25.526631
168.029035	5757.328214	25.531648
167.846765	5750.022927	25.536666
168.045405	5769.038007	25.541683
168.114239	5761.262066	25.546701
168.127225	5766.376759	25.551719
168.583255	5769.979980	25.556736
168.497802	5790.674794	25.561754
168.759221	5777.691539	25.566771
169.010670	5786.827296	25.571789
168.961613	5789.674957	25.576807
169.397207	5783.759377	25.581824
169.619306	5793.693340	25.586842
169.638911	5807.270027	25.591859
170.166349	5810.116534	25.596877
170.037094	5793.251925	25.601895
170.023784	5793.580547	25.606912
170.051558	5828.251586	25.611930
170.692867	5824.657649	25.616947
170.865903	5831.147574	25.621965
170.425038	5814.292302	25.626983
170.682003	5828.145554	25.632000
170.632452	5863.618863	25.637018
170.985544	5873.687147	25.642035
171.135159	5867.844775	25.647053
171.367271	5868.668313	25.652071
171.881129	5888.593323	25.657088
171.406805	5919.240974	25.662106
171.714475	5926.405193	25.667123
171.964621	5908.830484	25.672141
171.731917	5939.359505	25.677159
172.438998	5965.232999	25.682176
172.422495	5983.468480	25.687194
172.756062	5988.377509	25.692212
172.802375	5984.441268	25.697229
173.011659	5989.570059	25.702247
173.457091	6006.383085	25.707264
173.383657	6018.108269	25.712282
173.608781	6017.091108	25.717300
174.151208	6022.113679	25.722317
174.055802	6041.944661	25.727335
174.426441	6047.115318	25.732352
174.315616	6030.056843	25.737370
174.578277	6028.912998	25.742388
174.831299	6066.284943	25.747405
174.607522	6063.198094	25.752423
175.141244	6056.548429	25.757440
174.897099	6066.468259	25.762458
175.187844	6091.315400	25.767476
175.520030	6089.399376	25.772493
175.502235	6094.927561	25.777511
175.826685	6125.455836	25.782528
175.816658	6124.633440	25.787546
176.320346	6108.982119	25.792564
176.442995	6135.715515	25.797581
176.395202	6170.436810	25.802599
176.704532	6157.883942	25.807616
176.812155	6161.478677	25.812634
177.122990	6185.858833	25.817652
177.181296	6193.083278	25.822669
177.169413	6197.943539	25.827687
177.608077	6211.956495	25.832704
177.844013	6231.547520	25.837722
177.898345	6219.607651	25.842740
178.261365	6226.772314	25.847757
178.015206	6241.968226	25.852775
178.485783	6264.698745	25.857792
178.665250	6282.816754	25.862810
178.839657	6256.318746	25.867828
179.402157	6273.353683	25.872845
179.339801	6306.867740	25.877863
179.778971	6296.850227	25.882880
179.675655	6298.694257	25.887898
180.081539	6306.274746	25.892916
180.281883	6327.513651	25.897933
180.273802	6334.901114	25.902951
180.481922	6324.594172	25.907968
180.653063	6319.942670	25.912986
180.680051	6356.448246	25.918004
181.139991	6370.439718	25.923021
180.844147	6360.804660	25.928039
181.205345	6359.580331	25.933056
181.303289	6382.626159	25.938074
181.535297	6396.381669	25.943092
182.034295	6413.046506	25.948109
181.952705	6427.879154	25.953127
182.115545	6429.432742	25.958144
182.263655	6435.130897	25.963162
182.525963	6444.424318	25.968180
182.749340	6456.594537	25.973197
182.551092	6465.501818	25.978215
183.340779	6456.829182	25.983232
183.484267	6473.039389	25.988250
183.441225	6495.459008	25.993268
183.546742	6496.511787	25.998285
183.750075	6496.333320	26.003303
183.976460	6510.643064	26.008320
184.218665	6546.892635	26.013338
184.091894	6550.794328	26.018356
184.551319	6528.279109	26.023373
184.421133	6566.049460	26.028391
184.768359	6573.892555	26.033408
184.954495	6577.134220	26.038426
185.030545	6587.447976	26.043444
185.677787	6599.183271	26.048461
185.685207	6624.849418	26.053479
185.893075	6621.309992	26.058496
185.902057	6625.480643	26.063514
186.127082	6641.218447	26.068532
186.723747	6638.408564	26.073549
186.823998	6650.632747	26.078567
187.219895	6642.764922	26.083584
187.144434	6641.930867	26.088602
187.208018	6660.931156	26.093620
187.701938	6663.317957	26.098637
187.784743	6671.049656	26.103655
187.942104	6667.202782	26.108672
187.990433	6675.840281	26.113690
188.182864	6685.172953	26.118708
188.588793	6677.413702	26.123725
188.130723	6700.262072	26.128743
188.914167	6707.464983	26.133760
189.136743	6701.414161	26.138778
189.294924	6709.398415	26.143796
189.391713	6712.522179	26.148813
189.228708	6735.929004	26.153831
189.353657	6734.645641	26.158848
189.692180	6745.169705	26.163866
189.628762	6762.114875	26.168884
189.891427	6753.668938	26.173901
190.006325	6792.164783	26.178919
190.371012	6801.626956	26.183936
190.738147	6806.742535	26.188954
190.770625	6811.979955	26.193972
190.912711	6817.889901	26.198989
191.007673	6843.232455	26.204007
191.642368	6860.304931	26.209024
191.615884	6849.663528	26.214042
191.664391	6854.845157	26.219060
192.277374	6877.079752	26.224077
192.328565	6896.369418	26.229095
192.400774	6906.767495	26.234112
192.575291	6910.729745	26.239130
193.056777	6918.589812	26.244148
193.381568	6938.453693	26.249165
193.409160	6944.717294	26.254183
193.402667	6933.438984	26.259200
193.526589	6950.932218	26.264218
193.794846	6965.588656	26.269236
194.031081	6949.373132	26.274253
193.815324	6960.557110	26.279271
194.017697	7000.111199	26.284288
194.452220	7012.816331	26.289306
194.302372	7021.701361	26.294324
194.968455	7026.307714	26.299341
195.104387	7054.302465	26.304359
195.389402	7069.714997	26.309376
195.616676	7071.544658	26.314394
195.615106	7092.022578	26.319412
196.389977	7088.674835	26.324429
196.346649	7086.018265	26.329447
196.485675	7094.660697	26.334464
197.168614	7118.058649	26.339482
197.023905	7125.851003	26.344500
197.324804	7129.956230	26.349517
197.239423	7133.304300	26.354535
197.551853	7117.069713	26.359552
197.470873	7135.112435	26.364570
197.617690	7155.864782	26.369588
197.602324	7154.202937	26.374605
197.468404	7179.123943	26.379623
197.862699	7182.330554	26.384640
198.166801	7209.962709	26.389658
198.374759	7216.513593	26.394676
198.731195	7235.953664	26.399693
199.017527	7266.599931	26.404711
199.506223	7271.853870	26.409728
199.767480	7267.797529	26.414746
199.693487	7278.122356	26.419764
200.302264	7284.138466	26.424781
200.207194	7289.729848	26.429799
200.028161	7298.189082	26.434816
200.459746	7314.094251	26.439834
200.700112	7312.359027	26.444852
200.898697	7314.941603	26.449869
201.085087	7344.928843	26.454887
200.986201	7348.330773	26.459904
201.418985	7361.466858	26.464922
201.188869	7370.162166	26.469940
201.883362	7379.273299	26.474957
202.024223	7408.418443	26.479975
202.095523	7414.143035	26.484992
202.537331	7412.973825	26.490010
202.515799	7418.103424	26.495028
202.588442	7434.866576	26.500045
202.597302	7454.210780	26.505063
202.863661	7451.994791	26.510080
203.448955	7455.347488	26.515098
203.385901	7489.908451	26.520116
204.293740	7505.797339	26.525133
204.347856	7495.471763	26.530151
204.130520	7501.058220	26.535168
204.759537	7510.549602	26.540186
204.836199	7516.441877	26.545204
205.207648	7527.188626	26.550221
205.339808	7564.738475	26.555239
205.449010	7563.099712	26.560256
205.871291	7542.106762	26.565274
205.442758	7560.307414	26.570292
206.041049	7584.793855	26.575309
206.383520	7588.115037	26.580327
206.616858	7592.576490	26.585344
206.765710	7605.794346	26.590362
206.568412	7607.480012	26.595380
206.909733	7623.385447	26.600397
207.317179	7654.210132	26.605415
207.408114	7643.262519	26.610432
207.633493	7650.220226	26.615450
207.409453	7665.956867	26.620468
207.484756	7702.289451	26.625485
208.035697	7715.627611	26.630503
208.213887	7718.832632	26.635520
208.415792	7742.226339	26.640538
208.707402	7767.133883	26.645556
208.968868	7757.999294	26.650573
208.992669	7776.388496	26.655591
209.360826	7796.919652	26.660608
209.785588	7800.243821	26.665626
210.044906	7834.860958	26.670644
209.945940	7835.188418	26.675661
210.220506	7837.456108	26.680679
210.363449	7851.979328	26.685696
210.707735	7856.708406	26.690714
210.741730	7892.496970	26.695732
210.742579	7888.585878	26.700749
211.107103	7884.334330	26.705767
211.511656	7916.053090	26.710784
211.627865	7933.775902	26.715802
211.804698	7948.610996	26.720820
212.116686	7941.057237	26.725837
212.479452	7953.824214	26.730855
212.491315	7983.924990	26.735872
213.090620	7995.118760	26.740890
213.190054	8005.735944	26.745908
213.265852	7991.578935	26.750925
213.515382	8024.774206	26.755943
213.543992	8044.170213	26.760960
213.818734	8032.469769	26.765978
213.740184	8050.009101	26.770996
214.256011	8064.605579	26.776013
214.478490	8065.448550	26.781031
214.171606	8082.013630	26.786048
214.747248	8092.716004	26.791066
215.183271	8100.045489	26.796084
214.985306	8137.801674	26.801101
215.373052	8150.676517	26.806119
215.733524	8151.944030	26.811136
216.117545	8156.114551	26.816154
216.192872	8171.692761	26.821172
216.210061	8183.839717	26.826189
216.794567	8189.734181	26.831207
216.740722	8210.655355	26.836224
216.518308	8241.130834	26.841242
216.995365	8246.880046	26.846260
217.211075	8257.347452	26.851277
217.634928	8272.283800	26.856295
217.860909	8311.832169	26.861312
218.458195	8309.213279	26.866330
218.658866	8320.148667	26.871348
218.665346	8330.026934	26.876365
219.037700	8321.592753	26.881383
218.940962	8330.971428	26.886400
219.403245	8342.854373	26.891418
219.945295	8360.157623	26.896436
220.019656	8374.649340	26.901453
220.470187	8380.426612	26.906471
220.454425	8376.810334	26.911488
220.640327	8389.398180	26.916506
220.478524	8403.606826	26.921524
220.804253	8407.785471	26.926541
221.135690	8407.780353	26.931559
220.922360	8440.746610	26.936576
221.335271	8449.634757	26.941594
221.576611	8461.775608	26.946612
221.581437	8464.593584	26.951629
222.317210	8495.479083	26.956647
222.082000	8515.675337	26.961664
222.630238	8504.483027	26.966682
222.693749	8523.937651	26.971700
222.645639	8545.097746	26.976717
223.129587	8559.247092	26.981735
222.906816	8584.511060	26.986752
223.511988	8603.136743	26.991770
223.839485	8615.806124	26.996788
223.819116	8629.693109	27.001805
224.226116	8637.664013	27.006823
224.666406	8671.411155	27.011840
225.079908	8671.765009	27.016858
225.566092	8675.204446	27.021876
225.757420	8682.769169	27.026893
225.783406	8700.724338	27.031911
225.578538	8707.785106	27.036928
225.816732	8720.876512	27.041946
226.413163	8727.887592	27.046964
226.523330	8732.142107	27.051981
226.656230	8754.889504	27.056999
226.728256	8757.299482	27.062016
227.275081	8779.524083	27.067034
227.497830	8802.945062	27.072052
227.972215	8789.512228	27.077069
228.179430	8791.506865	27.082087
227.833253	8809.210972	27.087104
228.410214	8831.064434	27.092122
228.381246	8849.050116	27.097140
228.655985	8843.130051	27.102157
228.910550	8855.660457	27.107175
228.946861	8887.310487	27.112192
229.336353	8901.737231	27.117210
229.426762	8899.895085	27.122228
229.645492	8899.114689	27.127245
229.870245	8909.937031	27.132263
229.697041	8946.508866	27.137280
229.986743	8937.057043	27.142298
230.245466	8972.628989	27.147316
230.536879	8977.486859	27.152333
231.163311	8986.904746	27.157351
231.186087	9025.350388	27.162368
231.138527	9025.583529	27.167386
231.702993	9046.932922	27.172404
232.192684	9074.110411	27.177421
232.197490	9065.478228	27.182439
232.426983	9101.334895	27.187456
232.973078	9128.203077	27.192474
232.957599	9117.138920	27.197492
233.057123	9112.651230	27.202509
233.361933	9139.315137	27.207527
233.464364	9173.475177	27.212544
233.772884	9174.426863	27.217562
233.780985	9196.522104	27.222580
233.922707	9219.943699	27.227597
234.602025	9217.498565	27.232615
235.125047	9237.560222	27.237632
235.069821	9265.670037	27.242650
235.631797	9264.024814	27.247668
235.447603	9270.041970	27.252685
236.305954	9295.167826	27.257703
236.401876	9314.956745	27.262720
236.623632	9293.978854	27.267738
236.781311	9322.886897	27.272756
236.400566	9346.696663	27.277773
237.010391	9363.771648	27.282791
237.362887	9375.599478	27.287808
237.590400	9365.674861	27.292826
237.565422	9413.331942	27.297844
237.798289	9431.651511	27.302861
238.121444	9425.112032	27.307879
238.144200	9430.105795	27.312896
238.479137	9467.266721	27.317914
238.746619	9480.979297	27.322932
238.729648	9502.473420	27.327949
238.989648	9513.489623	27.332967
239.037984	9535.856723	27.337984
239.468935	9565.957430	27.343002
239.976084	9578.518352	27.348020
240.253831	9595.817797	27.353037
240.649129	9619.985723	27.358055
241.156533	9635.036369	27.363072
241.033042	9628.483175	27.368090
241.638382	9645.361510	27.373108
241.707138	9671.234357	27.378125
241.796964	9680.490851	27.383143
242.103124	9707.687151	27.388160
242.384350	9705.048585	27.393178
242.808504	9709.105773	27.398196
242.822169	9719.900535	27.403213
243.157744	9737.612757	27.408231
243.375417	9780.241919	27.413248
243.486585	9769.921184	27.418266
243.885331	9775.163267	27.423284
243.722142	9791.438589	27.428301
243.985232	9817.240971	27.433319
244.366755	9842.841093	27.438336
244.307179	9859.838179	27.443354
244.779154	9856.667916	27.448372
245.005401	9872.275638	27.453389
245.716335	9896.309134	27.458407
245.993599	9905.744306	27.463424
246.241453	9924.178541	27.468442
246.637064	9907.230676	27.473460
246.681282	9922.604660	27.478477
247.024463	9932.792980	27.483495
246.980879	9943.099557	27.488512
247.149556	9934.950225	27.493530
247.502881	9960.388214	27.498548
247.618692	9967.754152	27.503565
247.658819	9981.193602	27.508583
247.997479	10011.471086	27.513600
248.156798	10009.048739	27.518618
248.504999	10017.695628	27.523636
248.451559	10045.008632	27.528653
248.617942	10073.028125	27.533671
249.022695	10083.381230	27.538688
249.304798	10092.509314	27.543706
249.701495	10113.475924	27.548724
249.948974	10153.378217	27.553741
250.534994	10164.178750	27.558759
250.568548	10164.455217	27.563776
250.329110	10183.823305	27.568794
250.674494	10211.256588	27.573812
250.948003	10242.341607	27.578829
251.570060	10240.167291	27.583847
251.747649	10264.291041	27.588864
251.978873	10289.277917	27.593882
252.337937	10293.756388	27.598900
252.985163	10312.780432	27.603917
253.420217	10336.245006	27.608935
253.429900	10342.072999	27.613952
253.337604	10338.950974	27.618970
253.510263	10358.427626	27.623988
253.650345	10382.130833	27.629005
254.087611	10394.591314	27.634023
254.483906	10424.318142	27.639040
254.389143	10442.476399	27.644058
254.903334	10454.486269	27.649076
254.988906	10483.117685	27.654093
255.327410	10478.411323	27.659111
255.743504	10493.135233	27.664128
255.452619	10545.151403	27.669146
256.420976	10539.479234	27.674164
256.288591	10572.058453	27.679181
256.444698	10578.981640	27.684199
257.054069	10606.905253	27.689216
256.970738	10615.236226	27.694234
257.496712	10624.874131	27.699252
257.596678	10661.203918	27.704269
258.146874	10657.429809	27.709287
258.451269	10672.516561	27.714304
258.520888	10715.434993	27.719322
259.068478	10711.626644	27.724340
259.058060	10733.078812	27.729357
259.278686	10738.097009	27.734375
259.591729	10764.007679	27.739392
259.652572	10779.715302	27.744410
260.317398	10791.415395	27.749428
260.339519	10795.781112	27.754445
260.514549	10821.564229	27.759463
260.812985	10852.065789	27.764480
260.722015	10863.834881	27.769498
260.986324	10861.200498	27.774516
261.465288	10896.315013	27.779533
261.325579	10935.998092	27.784551
261.709929	10954.666974	27.789568
262.159715	10964.299556	27.794586
262.327973	10968.449764	27.799604
262.459596	10992.064691	27.804621
262.837615	11005.657133	27.809639
263.115300	11028.533532	27.814656
263.193854	11036.388198	27.819674
263.741975	11055.881653	27.824692
264.053124	11099.825407	27.829709
264.167903	11103.511072	27.834727
264.589104	11126.481270	27.839744
264.445422	11145.388069	27.844762
265.243330	11152.124334	27.849780
265.025518	11177.130865	27.854797
265.566883	11211.813551	27.859815
266.252640	11224.212361	27.864832
266.435409	11243.065340	27.869850
267.016873	11243.315894	27.874868
266.804743	11267.045525	27.879885
267.297862	11263.356329	27.884903
267.791106	11284.838668	27.889920
267.777838	11310.129852	27.894938
268.216656	11323.488021	27.899956
268.130366	11335.974301	27.904973
268.380224	11343.451067	27.909991
268.923123	11360.677119	27.915008
268.766604	11389.777106	27.920026
269.405541	11401.525253	27.925044
269.279945	11409.290159	27.930061
269.510405	11423.194858	27.935079
270.061189	11470.744064	27.940096
270.487261	11498.159934	27.945114
271.039516	11490.215840	27.950132
270.785321	11488.836013	27.955149
271.135315	11523.228812	27.960167
271.481562	11544.162320	27.965184
271.582713	11564.197370	27.970202
272.140908	11559.858504	27.975220
272.381071	11583.469765	27.980237
272.210062	11605.971328	27.985255
272.838653	11625.759403	27.990272
273.196032	11655.509927	27.995290
273.508380	11656.836102	28.000308
273.927759	11678.138967	28.005325
273.887524	11696.600797	28.010343
273.933593	11723.380323	28.015360
274.248812	11734.712708	28.020378
274.963538	11746.498217	28.025396
274.756179	11778.934734	28.030413
275.073160	11798.605931	28.035431
275.585661	11832.736225	28.040448
275.591672	11844.926426	28.045466
275.988002	11842.625347	28.050484
276.510459	11866.937170	28.055501
276.368844	11904.069874	28.060519
276.903499	11911.976442	28.065536
277.131509	11919.561072	28.070554
277.518895	11934.325722	28.075572
277.719653	11967.092218	28.080589
277.808564	11991.165485	28.085607
278.372041	12006.449385	28.090624
278.248864	12018.674455	28.095642
279.113864	12042.686536	28.100660
279.475782	12069.090689	28.105677
279.308760	12092.399728	28.110695
279.862670	12102.248976	28.115712
279.883577	12139.560979	28.120730
280.292518	12139.699835	28.125748
280.520015	12145.039537	28.130765
280.348071	12170.700971	28.135783
280.673268	12199.313204	28.140800
281.394809	12216.289305	28.145818
281.221054	12225.552226	28.150836
281.845117	12235.985517	28.155853
281.988547	12266.141987	28.160871
282.335909	12264.686337	28.165888
282.668546	12306.117667	28.170906
282.919538	12337.112804	28.175924
283.156646	12343.686210	28.180941
283.364196	12344.321552	28.185959
284.099827	12364.211814	28.190976
284.154015	12401.663090	28.195994
284.178841	12414.377637	28.201012
284.634831	12424.753741	28.206029
284.961738	12444.409124	28.211047
285.481601	12465.519189	28.216064
285.360593	12483.063328	28.221082
285.446250	12511.436032	28.226100
286.011480	12537.502497	28.231117
286.066600	12558.071058	28.236135
286.699171	12567.924142	28.241152
286.671863	12589.766026	28.246170
286.756802	12626.245347	28.251188
287.202249	12643.197406	28.256205
287.539534	12679.995175	28.261223
288.076865	12712.294787	28.266240
288.301594	12720.728789	28.271258
288.608966	12730.275681	28.276276
288.710707	12747.202705	28.281293
289.068204	12800.596971	28.286311
289.786561	12795.335597	28.291328
289.783853	12814.039878	28.296346
289.970410	12844.103651	28.301364
290.681307	12876.630952	28.306381
290.674571	12896.813116	28.311399
291.189052	12909.516483	28.316416
291.136109	12933.509822	28.321434
291.367003	12945.528991	28.326452
291.997515	12973.687234	28.331469
292.145562	13014.568703	28.336487
292.415324	13033.419661	28.341504
292.772648	13045.456619	28.346522
293.028944	13056.476676	28.351540
293.499644	13086.874469	28.356557
293.864747	13122.062316	28.361575
294.044919	13120.813046	28.366592
294.277126	13133.400938	28.371610
294.466667	13165.173579	28.376628
294.633045	13204.605292	28.381645
294.960140	13225.762387	28.386663
295.056277	13222.474737	28.391680
295.490263	13256.346088	28.396698
295.944824	13298.926591	28.401716
296.597439	13323.931312	28.406733
296.396875	13340.610321	28.411751
296.896940	13353.170676	28.416768
297.234859	13375.481913	28.421786
297.467765	13387.656282	28.426804
297.893763	13415.458328	28.431821
298.034870	13442.457427	28.436839
298.287721	13471.631419	28.441856
298.853327	13484.277951	28.446874
298.734639	13510.576376	28.451892
299.222095	13525.661576	28.456909
299.490551	13533.269439	28.461927
299.684758	13560.534915	28.466944
300.128418	13606.568734	28.471962
300.554126	13624.609938	28.476980
300.798007	13619.525171	28.481997
300.889111	13639.659799	28.487015
301.079248	13678.996571	28.492032
301.917693	13692.704314	28.497050
301.599203	13705.397029	28.502068
302.261291	13706.353616	28.507085
302.362865	13746.199158	28.512103
302.799487	13779.299880	28.517120
303.056730	13780.614858	28.522138
303.471409	13797.670913	28.527156
303.696047	13810.741957	28.532173
303.822209	13859.597435	28.537191
304.252701	13885.400786	28.542208
304.434992	13897.867528	28.547226
304.604887	13928.319759	28.552244
305.330061	13945.696538	28.557261
305.099068	13977.357476	28.562279
305.558998	14013.759076	28.567296
306.300387	14019.496670	28.572314
306.411709	14041.386948	28.577332
306.708165	14065.772534	28.582349
307.032218	14084.558240	28.587367
307.160460	14124.683150	28.592384
307.727606	14134.404623	28.597402
307.887972	14162.071424	28.602420
308.220268	14177.463349	28.607437
308.524055	14210.369451	28.612455
308.988785	14235.365662	28.617472
309.120391	14271.833118	28.622490
309.258897	14285.082653	28.627508
310.140476	14292.205890	28.632525
310.045235	14325.723355	28.637543
310.819318	14359.965499	28.642560
311.232074	14379.965971	28.647578
311.604608	14384.337014	28.652596
312.094756	14392.372714	28.657613
312.058578	14428.129219	28.662631
312.357411	14446.854907	28.667648
312.784475	14463.211565	28.672666
312.964440	14486.077524	28.677684
313.497683	14495.669303	28.682701
313.390450	14527.889170	28.687719
313.807532	14536.879317	28.692736
313.859249	14575.544655	28.697754
314.002439	14609.781257	28.702772
314.670381	14598.913193	28.707789
314.875952	14641.056192	28.712807
315.080931	14693.191368	28.717824
315.574223	14700.787063	28.722842
315.799296	14737.155033	28.727860
316.190737	14748.949690	28.732877
316.673860	14774.191093	28.737895
316.886554	14781.615727	28.742912
317.209658	14798.839245	28.747930
317.361160	14848.248197	28.752948
317.522226	14839.611513	28.757965
317.465116	14890.172289	28.762983
318.001642	14919.858285	28.768000
318.302533	14944.099491	28.773018
318.467713	14998.790288	28.778036
318.949622	15007.056149	28.783053
319.278363	15041.113305	28.788071
319.651903	15079.246055	28.793088
319.975828	15092.681504	28.798106
320.426896	15131.570565	28.803124
320.415588	15162.349731	28.808141
321.004541	15189.356549	28.813159
321.170655	15221.258439	28.818176
321.469443	15242.791599	28.823194
321.639742	15258.302715	28.828212
322.157603	15285.978559	28.833229
322.548475	15328.333832	28.838247
322.399952	15355.781083	28.843264
323.360798	15382.512468	28.848282
323.431340	15408.297351	28.853300
323.839953	15420.905947	28.858317
324.168772	15454.221736	28.863335
324.273656	15476.953367	28.868352
324.883667	15497.762561	28.873370
325.091168	15529.346200	28.878388
325.899281	15556.174020	28.883405
326.076549	15569.589970	28.888423
326.620213	15607.492570	28.893440
327.129589	15644.698087	28.898458
327.086807	15645.307162	28.903476
327.706828	15655.592859	28.908493
327.868082	15692.317052	28.913511
328.268832	15707.443835	28.918528
328.782312	15735.887044	28.923546
328.769098	15762.534144	28.928564
329.245987	15769.040973	28.933581
329.451138	15808.022710	28.938599
329.595999	15829.222776	28.943616
330.048603	15842.850334	28.948634
330.112087	15879.654137	28.953652
330.546841	15898.630101	28.958669
331.041320	15925.879106	28.963687
331.199169	15958.674188	28.968704
331.571029	15978.655026	28.973722
331.922582	15996.856902	28.978740
332.688537	16032.407198	28.983757
333.140499	16060.104705	28.988775
332.996069	16070.168686	28.993792
333.387691	16078.722645	28.998810
333.465603	16130.842451	29.003828
334.154288	16170.038291	29.008845
334.508272	16182.968537	29.013863
334.731759	16203.754243	29.018880
334.923052	16228.644265	29.023898
335.368538	16278.768587	29.028916
335.838651	16295.250786	29.033933
335.986374	16304.146161	29.038951
336.263007	16336.314070	29.043968
336.770496	16365.738025	29.048986
336.941338	16404.704794	29.054004
336.830386	16426.584579	29.059021
337.323903	16453.566717	29.064039
337.863576	16491.193094	29.069056
337.930270	16507.980124	29.074074
338.435934	16557.089905	29.079092
339.049381	16577.721835	29.084109
339.317565	16603.074087	29.089127
339.758871	16646.149397	29.094144
340.188932	16659.511876	29.099162
340.151978	16683.357613	29.104180
340.626409	16721.561070	29.109197
340.999359	16741.200680	29.114215
341.147682	16784.138792	29.119232
341.524380	16810.705852	29.124250
341.953078	16833.800361	29.129268
342.387356	16875.408625	29.134285
342.656930	16891.484859	29.139303
342.983610	16907.200230	29.144320
343.774363	16936.214365	29.149338
343.876823	16991.681840	29.154356
344.249278	16997.722587	29.159373
344.753013	17002.554924	29.164391
344.780429	17033.543983	29.169408
345.335056	17055.573115	29.174426
345.126603	17102.947560	29.179444
345.610296	17112.303225	29.184461
346.376965	17127.246373	29.189479
346.598531	17154.957011	29.194496
346.911320	17184.072614	29.199514
347.059912	17207.305336	29.204532
347.386451	17238.726051	29.209549
347.708653	17269.539198	29.214567
348.012010	17282.790735	29.219584
348.331257	17311.380681	29.224602
348.862541	17344.543955	29.229620
349.241439	17363.497759	29.234637
349.641521	17391.685212	29.239655
349.995159	17436.947287	29.244672
350.224644	17463.360061	29.249690
350.531376	17504.217160	29.254708
350.793869	17517.957907	29.259725
351.322153	17571.475198	29.264743
351.162671	17595.704996	29.269760
351.817339	17608.528386	29.274778
352.010525	17639.199634	29.279796
352.543845	17672.169380	29.284813
353.139469	17700.737989	29.289831
353.258511	17729.497282	29.294848
353.577832	17774.108738	29.299866
354.038935	17828.580456	29.304884
354.199064	17856.204713	29.309901
354.666502	17884.325148	29.314919
354.996154	17916.320341	29.319936
355.585850	17947.503506	29.324954
355.904840	17985.444019	29.329972
355.886016	18011.496793	29.334989
356.843061	18031.846842	29.340007
356.653882	18079.042819	29.345024
357.824297	18093.190420	29.350042
358.001917	18141.394576	29.355060
358.168957	18153.288670	29.360077
358.668638	18192.894125	29.365095
359.050472	18222.914310	29.370112
359.684807	18241.062516	29.375130
359.799387	18277.707232	29.380148
360.342401	18298.581511	29.385165
360.993951	18313.313077	29.390183
361.192427	18346.041610	29.395200
361.448409	18373.663510	29.400218
361.802066	18380.640946	29.405236
362.054939	18426.220284	29.410253
362.190768	18449.663346	29.415271
362.329257	18479.927523	29.420288
362.454441	18511.041918	29.425306
362.924325	18552.089025	29.430324
363.194032	18593.550733	29.435341
363.616711	18618.674106	29.440359
364.112390	18638.836337	29.445376
364.676136	18674.919126	29.450394
364.885643	18716.315433	29.455412
365.202752	18750.432681	29.460429
365.722959	18779.559405	29.465447
366.104992	18818.880027	29.470464
366.639014	18833.623597	29.475482
366.846701	18857.194071	29.480500
367.162093	18896.631492	29.485517
367.907478	18932.968553	29.490535
368.055220	18954.169035	29.495552
368.057926	18965.474578	29.500570
368.871895	19002.591706	29.505588
368.985799	19044.422319	29.510605
369.532720	19059.264838	29.515623
369.248823	19095.154427	29.520640
369.879896	19108.250848	29.525658
370.116781	19145.840346	29.530676
370.415936	19189.622008	29.535693
370.861023	19200.771090	29.540711
371.007506	19256.281487	29.545728
371.564072	19302.801362	29.550746
371.958828	19335.475789	29.555764
372.328726	19358.895661	29.560781
372.877442	19390.346834	29.565799
373.001579	19434.392916	29.570816
373.344316	19478.540133	29.575834
374.054580	19503.180730	29.580852
374.173689	19548.302937	29.585869
374.628823	19560.844000	29.590887
374.667193	19591.686321	29.595904
375.188690	19648.272552	29.600922
375.834970	19690.391998	29.605940
376.229706	19727.742371	29.610957
376.621713	19745.128382	29.615975
377.120120	19792.660168	29.620992
377.481855	19845.544030	29.626010
377.908922	19864.076626	29.631028
378.343755	19882.814452	29.636045
378.629186	19912.943488	29.641063
378.949979	19972.164835	29.646080
379.570019	19994.855451	29.651098
379.807568	20019.332164	29.656116
380.411703	20044.739838	29.661133
380.530186	20079.486905	29.666151
381.199726	20135.396184	29.671168
381.473002	20165.754675	29.676186
381.647022	20175.888350	29.681204
382.214128	20215.594713	29.686221
382.745053	20255.062821	29.691239
383.020861	20289.090762	29.696256
383.388844	20301.725602	29.701274
384.071328	20334.050242	29.706292
383.777712	20395.641341	29.711309
384.323030	20434.057668	29.716327
384.914299	20461.588263	29.721344
385.233185	20472.967131	29.726362
385.762828	20518.861190	29.731380
385.980041	20565.546291	29.736397
385.953561	20586.440309	29.741415
386.930165	20649.729879	29.746432
386.935944	20674.575303	29.751450
387.687701	20691.026431	29.756468
387.822924	20740.321812	29.761485
388.284458	20776.104500	29.766503
388.364026	20812.366525	29.771520
388.990825	20848.494089	29.776538
389.809007	20888.330832	29.781556
389.819857	20929.116025	29.786573
390.474717	20957.530741	29.791591
390.630161	20982.738112	29.796608
390.879062	21024.516739	29.801626
391.382165	21062.928885	29.806644
391.431611	21092.799535	29.811661
391.972572	21118.227174	29.816679
392.771694	21165.897655	29.821696
393.169914	21214.474721	29.826714
393.821650	21227.372366	29.831732
393.865596	21243.712395	29.836749
394.246821	21265.529893	29.841767
394.791201	21316.756691	29.846784
394.907456	21348.035528	29.851802
395.219635	21358.913238	29.856820
395.323666	21393.231924	29.861837
395.806412	21434.897282	29.866855
396.178018	21489.014350	29.871872
396.293866	21522.667676	29.876890
397.289727	21540.278984	29.881908
397.276889	21597.485079	29.886925
397.990602	21629.033054	29.891943
398.571042	21646.233865	29.896960
399.027288	21692.311966	29.901978
399.398604	21723.096932	29.906996
399.728323	21765.991225	29.912013
399.938104	21790.609132	29.917031
400.296585	21820.732712	29.922048
400.446489	21855.785705	29.927066
401.136663	21874.177767	29.932084
401.404615	21923.352249	29.937101
401.812265	21970.764954	29.942119
402.364703	22010.142239	29.947136
402.502128	22048.623372	29.952154
403.037913	22088.653101	29.957172
403.390689	22136.530943	29.962189
403.733733	22174.893269	29.967207
404.088930	22218.465557	29.972224
404.551264	22254.386868	29.977242
405.316243	22297.380883	29.982260
405.733591	22346.237124	29.987277
405.795334	22376.002411	29.992295
406.594127	22415.500758	29.997312
406.723681	22452.664581	30.002330
407.236801	22481.086396	30.007348
407.289476	22521.398763	30.012365
407.955263	22567.687446	30.017383
408.525366	22621.996106	30.022400
408.614906	22658.333010	30.027418
409.372667	22695.212292	30.032436
409.552483	22743.222916	30.037453
410.040173	22770.282562	30.042471
410.512322	22821.849099	30.047488
410.703744	22883.723960	30.052506
411.422892	22903.617983	30.057524
411.657474	22941.126569	30.062541
412.175269	22984.519487	30.067559
412.411400	23028.461972	30.072576
412.747701	23078.508279	30.077594
413.250173	23100.106344	30.082612
413.536244	23159.535507	30.087629
414.193387	23194.696696	30.092647
414.582186	23229.539674	30.097664
415.015987	23277.133063	30.102682
415.728411	23318.099849	30.107700
416.065285	23362.181071	30.112717
416.605361	23405.680182	30.117735
417.097600	23430.190774	30.122752
417.302213	23477.839935	30.127770
417.959182	23500.679013	30.132788
418.182037	23543.359017	30.137805
418.620571	23589.703829	30.142823
418.951697	23635.959301	30.147840
419.167541	23663.881988	30.152858
419.656875	23695.042087	30.157876
419.706542	23748.382444	30.162893
420.440488	23805.463241	30.167911
421.097855	23824.206581	30.172928
421.202186	23853.472383	30.177946
421.750775	23896.072669	30.182964
421.923810	23950.709789	30.187981
422.624002	23989.506027	30.192999
422.924714	24009.538285	30.198016
423.156302	24042.192132	30.203034
423.635143	24087.672375	30.208052
424.179596	24131.284583	30.213069
424.440888	24185.187343	30.218087
425.215790	24202.916808	30.223104
425.832293	24253.112675	30.228122
425.976092	24299.372533	30.233140
425.942192	24342.360280	30.238157
426.331172	24372.503902	30.243175
426.788888	24423.984709	30.248192
426.911230	24464.602406	30.253210
427.236999	24521.396721	30.258228
427.921484	24567.104442	30.263245
428.208462	24632.547499	30.268263
428.690567	24678.853419	30.273280
429.376851	24739.885482	30.278298
429.763370	24778.401086	30.283316
430.203243	24810.156385	30.288333
430.307394	24861.257021	30.293351
431.507385	24915.065382	30.298368
431.893614	24951.634150	30.303386
432.470645	24996.380046	30.308404
433.323381	25033.538894	30.313421
433.350532	25087.319225	30.318439
433.889827	25129.539430	30.323456
434.175095	25169.813399	30.328474
434.377346	25221.558005	30.333492
434.528664	25253.726038	30.338509
435.260410	25298.921786	30.343527
435.646319	25349.878013	30.348544
436.279628	25415.866064	30.353562
436.849948	25439.832149	30.358580
437.162927	25464.310663	30.363597
437.346279	25519.632319	30.368615
438.313863	25571.374556	30.373632
438.946265	25603.309255	30.378650
439.426129	25645.239392	30.383668
439.838930	25686.920537	30.388685
439.611488	25735.129934	30.393703
440.576600	25770.362308	30.398720
441.143520	25806.688624	30.403738
441.300633	25866.328366	30.408756
441.978387	25912.271050	30.413773
441.719741	25948.201072	30.418791
442.319655	25983.718128	30.423808
442.184592	26036.925906	30.428826
443.300869	26102.595586	30.433844
443.651709	26149.081738	30.438861
443.702255	26183.546739	30.443879
444.561371	26238.595110	30.448896
444.930146	26293.835040	30.453914
445.395659	26328.799461	30.458932
446.201861	26381.646257	30.463949
446.406710	26436.188362	30.468967
446.809664	26484.516508	30.473984
447.121433	26557.481499	30.479002
447.387753	26598.720737	30.484020
447.960315	26629.730572	30.489037
448.625030	26687.967894	30.494055
449.265888	26722.801659	30.499072
449.758084	26780.265147	30.504090
450.335361	26815.639449	30.509108
450.780686	26848.961968	30.514125
451.360270	26900.326077	30.519143
451.955523	26917.255455	30.524160
451.748053	26942.366110	30.529178
452.233744	26985.747789	30.534196
452.777663	27033.675740	30.539213
453.070200	27079.756171	30.544231
453.682585	27097.562834	30.549248
454.025532	27170.096364	30.554266
454.209922	27221.484143	30.559284
454.839243	27251.957454	30.564301
455.147030	27297.452477	30.569319
455.924648	27355.523615	30.574336
456.195733	27393.559581	30.579354
456.700199	27436.937727	30.584372
456.956955	27476.247288	30.589389
457.363143	27536.963494	30.594407
458.372897	27558.373070	30.599424
458.820563	27601.117604	30.604442
458.875127	27669.105528	30.609460
459.136437	27719.564282	30.614477
459.937601	27754.286938	30.619495
460.718683	27791.018939	30.624512
460.736618	27851.115970	30.629530
461.309100	27895.253626	30.634548
461.849210	27938.463145	30.639565
461.936428	28009.992175	30.644583
462.877292	28049.596920	30.649600
463.272834	28084.790971	30.654618
463.963960	28115.567866	30.659636
464.544007	28176.207151	30.664653
464.966158	28246.461207	30.669671
465.458904	28281.772078	30.674688
465.706060	28319.681579	30.679706
465.895240	28358.408196	30.684724
466.502250	28422.756303	30.689741
466.837983	28481.995584	30.694759
467.600955	28514.281627	30.699776
467.706634	28553.536603	30.704794
468.634887	28614.056832	30.709812
468.866159	28653.206127	30.714829
469.081510	28708.176390	30.719847
469.894659	28766.016183	30.724864
469.845141	28811.107418	30.729882
470.967382	28852.071908	30.734900
471.264910	28914.119931	30.739917
471.771416	28965.980168	30.744935
472.233916	29010.422739	30.749952
472.430621	29066.185785	30.754970
473.286177	29101.797995	30.759988
473.873950	29150.465870	30.765005
474.121773	29219.005225	30.770023
475.069373	29262.727996	30.775040
475.363388	29311.107340	30.780058
475.822999	29339.663041	30.785076
476.486918	29368.948384	30.790093
476.968595	29428.911230	30.795111
477.527232	29477.190550	30.800128
477.820358	29512.234105	30.805146
478.222124	29561.211446	30.810164
478.572720	29597.173058	30.815181
478.796920	29659.677482	30.820199
479.433936	29704.673418	30.825216
479.583624	29752.957973	30.830234
480.172389	29810.699544	30.835252
480.645356	29840.279044	30.840269
481.027669	29898.780522	30.845287
481.093967	29960.668617	30.850304
481.975831	30030.592187	30.855322
482.236955	30069.739763	30.860340
483.010571	30098.150218	30.865357
483.027831	30165.031162	30.870375
483.665040	30217.905076	30.875392
484.062612	30280.127590	30.880410
484.165364	30313.936116	30.885428
485.102794	30363.098529	30.890445
485.498601	30436.466714	30.895463
485.910022	30484.741618	30.900480
486.338617	30556.824163	30.905498
486.649089	30623.264123	30.910516
487.411273	30671.585707	30.915533
487.567263	30723.591134	30.920551
488.182320	30782.268503	30.925568
488.655191	30845.250318	30.930586
489.379285	30914.086792	30.935604
489.812798	30958.450828	30.940621
490.637794	31032.365781	30.945639
490.988057	31079.097216	30.950656
491.591077	31121.376855	30.955674
492.106950	31187.737724	30.960692
492.807192	31250.254418	30.965709
493.047970	31302.850109	30.970727
493.631222	31344.108290	30.975744
494.193581	31402.973121	30.980762
494.418484	31469.562943	30.985780
495.283494	31533.996729	30.990797
495.422996	31580.332129	30.995815
496.184181	31633.426477	31.000832
496.398686	31706.672229	31.005850
496.935091	31770.378794	31.010868
497.605256	31807.267014	31.015885
498.310128	31872.709632	31.020903
498.797559	31936.200905	31.025920
499.339553	31975.959416	31.030938
499.623763	32039.588740	31.035956
500.227724	32114.674212	31.040973
500.537385	32160.509823	31.045991
500.828627	32202.947696	31.051008
501.485267	32276.166970	31.056026
501.586334	32357.109903	31.061044
502.319533	32417.994280	31.066061
502.903260	32471.685211	31.071079
503.471882	32531.174321	31.076096
504.373191	32583.652141	31.081114
504.789635	32640.049725	31.086132
505.346136	32694.275860	31.091149
505.659095	32765.317117	31.096167
506.114253	32813.215808	31.101184
506.904537	32861.753361	31.106202
507.052365	32919.931433	31.111220
508.222186	32981.212582	31.116237
508.770890	33049.827744	31.121255
509.151221	33092.436045	31.126272
509.590858	33153.324145	31.131290
509.802661	33215.202900	31.136308
510.592769	33254.453238	31.141325
511.298628	33298.046267	31.146343
511.349154	33371.562690	31.151360
511.757671	33426.263547	31.156378
512.596121	33482.688783	31.161396
512.820658	33553.394467	31.166413
512.961151	33615.349510	31.171431
513.802788	33672.866487	31.176448
514.252925	33734.799200	31.181466
514.698073	33799.979563	31.186484
515.259490	33864.383733	31.191501
515.542857	33929.979379	31.196519
516.078648	33979.865131	31.201536
516.391021	34039.691950	31.206554
517.341197	34098.590124	31.211572
517.783919	34145.576347	31.216589
518.080921	34204.737369	31.221607
518.635743	34278.994625	31.226624
519.301343	34326.616573	31.231642
519.666529	34388.060780	31.236660
520.488397	34438.367548	31.241677
520.793685	34504.630617	31.246695
520.993787	34573.403953	31.251712
521.917703	34631.399534	31.256730
522.204420	34697.212034	31.261748
522.823957	34742.766546	31.266765
523.514071	34828.192383	31.271783
523.843260	34898.826217	31.276800
524.581463	34936.637441	31.281818
524.764303	34994.832350	31.286836
525.605039	35064.675558	31.291853
526.099848	35143.004117	31.296871
526.843091	35196.358323	31.301888
527.593437	35250.935799	31.306906
527.810852	35319.690241	31.311924
528.038731	35360.770444	31.316941
528.741111	35439.949538	31.321959
529.139131	35512.224723	31.326976
529.870037	35573.909245	31.331994
530.469557	35637.060874	31.337012
531.196121	35694.470917	31.342029
531.683083	35767.783214	31.347047
531.718597	35824.446380	31.352064
532.419988	35881.346842	31.357082
532.601125	35965.622124	31.362100
533.302074	36027.193261	31.367117
534.130916	36084.297363	31.372135
534.574002	36152.853665	31.377152
535.070992	36225.367842	31.382170
535.689828	36319.190594	31.387188
535.990419	36376.326086	31.392205
536.693970	36450.911827	31.397223
537.307851	36512.634715	31.402240
538.078220	36583.921849	31.407258
538.583377	36663.729066	31.412276
538.963196	36714.897904	31.417293
539.573685	36782.412864	31.422311
539.779762	36845.690569	31.427328
540.295643	36927.630414	31.432346
540.639677	37011.457714	31.437364
541.584497	37079.338279	31.442381
542.257391	37161.114409	31.447399
542.575407	37209.921782	31.452416
543.248289	37260.728206	31.457434
543.419351	37354.062324	31.462452
543.859383	37410.354443	31.467469
544.510218	37495.692277	31.472487
544.957236	37575.434270	31.477504
545.960685	37652.140356	31.482522
546.363851	37728.194838	31.487540
546.818684	37799.939728	31.492557
547.721857	37868.830562	31.497575
548.010509	37937.384502	31.502592
548.884222	37996.601725	31.507610
549.804024	38075.305315	31.512628
550.296677	38116.603751	31.517645
551.049632	38185.457497	31.522663
551.177618	38239.427377	31.527680
551.930450	38316.941429	31.532698
552.538444	38378.251987	31.537716
553.019129	38419.802415	31.542733
553.767548	38467.749983	31.547751
554.090383	38534.697339	31.552768
554.486603	38583.126284	31.557786
555.211013	38644.932944	31.562804
555.625856	38694.227003	31.567821
556.111043	38762.524396	31.572839
556.292544	38838.951569	31.577856
556.611268	38889.448695	31.582874
557.212837	38959.883167	31.587892
557.867722	39039.174412	31.592909
558.392308	39097.158953	31.597927
558.673730	39174.782965	31.602944
559.608295	39245.428660	31.607962
559.839425	39304.986722	31.612980
560.552673	39393.971687	31.617997
561.374018	39470.807138	31.623015
561.356154	39540.301513	31.628032
562.118500	39617.699655	31.633050
562.651788	39697.992279	31.638068
563.022938	39785.558595	31.643085
563.830909	39854.557970	31.648103
564.221748	39936.424863	31.653120
565.256989	40011.810153	31.658138
565.632958	40071.952806	31.663156
566.192444	40156.671307	31.668173
566.808950	40240.326600	31.673191
567.267098	40330.153674	31.678208
568.015526	40388.578821	31.683226
568.547863	40468.748765	31.688244
569.566121	40534.117830	31.693261
570.308437	40604.696429	31.698279
570.493275	40670.667619	31.703296
571.157003	40756.782578	31.708314
572.046033	40823.193525	31.713332
572.356032	40900.065836	31.718349
573.109861	40977.670040	31.723367
573.530092	41048.439284	31.728384
574.355409	41113.611887	31.733402
574.858034	41192.814603	31.738420
575.181049	41253.171922	31.743437
575.904451	41332.316684	31.748455
576.349361	41406.293335	31.753472
576.785549	41470.316254	31.758490
577.163065	41561.557877	31.763508
577.807694	41644.217533	31.768525
578.287107	41703.638283	31.773543
578.928408	41782.719647	31.778560
579.954635	41870.636025	31.783578
580.621545	41952.314872	31.788596
581.061877	42018.867419	31.793613
582.178927	42070.668295	31.798631
582.899615	42148.702778	31.803648
583.533302	42193.326872	31.808666
583.958949	42279.106393	31.813684
584.177812	42339.096239	31.818701
584.952344	42394.212226	31.823719
585.298797	42486.688360	31.828736
585.809438	42562.432860	31.833754
586.172742	42626.503429	31.838772
586.840741	42683.882267	31.843789
587.384680	42774.543717	31.848807
588.073914	42862.239573	31.853824
588.760362	42921.402799	31.858842
589.272808	43000.343396	31.863860
589.527963	43083.664184	31.868877
590.359120	43151.627330	31.873895
590.662310	43230.249920	31.878912
591.055827	43316.162706	31.883930
591.912214	43370.362111	31.888948
592.135908	43434.878409	31.893965
592.920908	43519.581568	31.898983
593.223065	43605.210893	31.904000
594.242047	43666.215688	31.909018
594.694402	43760.161288	31.914036
595.296671	43839.358979	31.919053
595.986162	43909.463422	31.924071
596.665493	43978.026091	31.929088
597.457224	44062.313922	31.934106
597.852057	44136.193040	31.939124
598.376947	44193.770697	31.944141
599.096726	44265.790902	31.949159
599.901034	44347.823905	31.954176
600.709565	44441.524726	31.959194
601.021070	44504.227627	31.964212
601.286710	44561.148398	31.969229
602.346528	44634.998601	31.974247
602.850080	44729.404751	31.979264
603.221608	44805.374021	31.984282
604.283763	44862.277815	31.989300
604.819040	44929.882809	31.994317
605.577579	45027.768476	31.999335
605.986700	45122.226949	32.004352
606.346232	45188.415967	32.009370
607.086820	45254.217103	32.014388
607.251564	45343.040583	32.019405
608.021561	45437.169541	32.024423
608.638957	45514.787017	32.029440
608.928951	45573.029714	32.034458
609.933464	45659.471265	32.039476
610.378861	45768.671044	32.044493
611.165542	45850.653618	32.049511
611.909455	45926.796444	32.054528
612.677471	46004.305839	32.059546
613.284738	46107.368464	32.064564
613.671763	46190.267841	32.069581
614.564348	46239.522240	32.074599
614.991187	46316.925106	32.079616
615.786831	46411.575705	32.084634
616.616449	46498.552047	32.089652
617.077220	46588.327121	32.094669
618.111210	46646.491336	32.099687
618.625185	46719.596966	32.104704
618.971772	46804.488566	32.109722
620.094495	46873.042364	32.114740
620.527354	46960.209522	32.119757
621.402256	47022.250048	32.124775
621.664661	47095.799687	32.129792
622.438145	47191.152524	32.134810
623.031433	47266.706831	32.139828
623.253152	47329.658247	32.144845
623.936353	47405.491907	32.149863
624.411556	47492.136718	32.154880
624.965464	47576.220829	32.159898
625.891789	47657.730427	32.164916
626.124460	47738.142454	32.169933
627.002118	47802.449053	32.174951
627.255154	47914.187572	32.179968
627.636596	48001.608030	32.184986
628.412888	48077.410081	32.190004
628.979707	48180.958112	32.195021
629.676880	48266.193114	32.200039
630.390162	48349.562841	32.205056
631.335965	48427.507597	32.210074
632.051814	48523.786112	32.215092
632.526620	48609.315162	32.220109
633.335728	48675.716973	32.225127
634.097051	48741.154340	32.230144
634.076246	48815.281649	32.235162
634.732439	48898.862167	32.240180
635.370828	48984.005916	32.245197
636.033019	49065.221036	32.250215
636.559584	49158.351038	32.255232
636.982881	49232.747672	32.260250
637.942892	49313.526264	32.265268
638.446558	49403.156106	32.270285
639.147863	49506.335514	32.275303
639.487547	49578.906307	32.280320
640.047931	49659.818692	32.285338
640.648287	49748.591051	32.290356
641.090761	49852.939290	32.295373
641.929548	49951.336331	32.300391
642.260217	50056.278888	32.305408
643.157597	50162.464232	32.310426
643.570606	50247.044552	32.315444
643.683797	50346.274010	32.320461
644.068881	50437.996781	32.325479
645.520104	50560.315402	32.330496
646.127585	50686.446933	32.335514
647.181387	50775.480786	32.340532
647.563994	50868.573465	32.345549
648.360095	50960.401402	32.350567
649.025395	51069.608183	32.355584
649.622463	51186.441034	32.360602
650.539367	51271.106894	32.365620
651.248883	51355.700004	32.370637
651.932508	51471.534965	32.375655
652.743245	51569.998680	32.380672
653.452210	51658.960961	32.385690
654.126625	51746.719774	32.390708
654.785855	51844.379318	32.395725
655.709559	51949.006938	32.400743
656.580621	52044.191206	32.405760
657.029183	52125.164095	32.410778
658.059764	52216.242407	32.415796
658.574930	52305.182844	32.420813
659.216135	52382.382435	32.425831
660.101111	52475.062013	32.430848
660.426728	52556.552879	32.435866
661.543092	52636.002700	32.440884
662.277095	52727.700919	32.445901
662.805967	52816.843592	32.450919
663.290643	52911.716966	32.455936
664.072117	52994.656738	32.460954
664.763824	53077.712763	32.465972
665.676055	53155.208642	32.470989
666.111211	53246.623894	32.476007
666.773788	53327.143260	32.481024
667.238016	53404.894164	32.486042
668.121986	53496.612332	32.491060
668.591326	53600.998648	32.496077
669.316442	53670.561775	32.501095
670.005280	53759.600260	32.506112
670.109185	53852.159611	32.511130
671.312938	53936.496091	32.516148
671.981516	54032.582746	32.521165
672.442950	54128.982042	32.526183
673.269252	54236.970469	32.531200
673.655462	54313.521845	32.536218
674.402784	54384.972720	32.541236
675.100324	54486.445452	32.546253
675.628273	54596.405605	32.551271
676.413793	54681.787266	32.556288
676.574278	54768.896092	32.561306
677.765674	54852.524734	32.566324
678.328778	54958.962340	32.571341
679.145908	55049.078468	32.576359
679.728449	55117.280488	32.581376
680.593356	55185.227635	32.586394
681.521151	55285.017635	32.591412
681.827063	55376.931761	32.596429
682.394185	55446.445215	32.601447
683.233222	55542.738613	32.606464
683.625228	55626.060364	32.611482
684.268600	55707.016053	32.616500
685.153178	55806.120912	32.621517
685.394409	55913.539265	32.626535
686.300009	55995.994373	32.631552
687.129886	56076.617538	32.636570
688.161072	56164.372199	32.641588
688.593187	56275.532753	32.646605
689.067244	56364.081600	32.651623
689.632800	56446.563175	32.656640
690.379267	56541.657419	32.661658
691.118860	56662.044127	32.666676
691.433949	56769.031662	32.671693
691.991192	56859.325413	32.676711
693.294416	56965.594841	32.681728
693.624196	57060.886776	32.686746
694.147069	57162.970875	32.691764
695.181337	57279.711357	32.696781
695.919283	57395.913874	32.701799
696.814014	57469.986379	32.706816
697.285537	57563.696731	32.711834
698.295417	57683.678589	32.716852
698.703530	57794.472588	32.721869
699.420462	57885.452323	32.726887
700.253716	58002.489334	32.731904
701.008601	58112.577050	32.736922
701.551549	58199.157732	32.741940
702.372386	58297.445316	32.746957
703.049486	58384.674416	32.751975
703.662032	58484.798111	32.756992
703.983644	58620.171294	32.762010
704.636463	58735.245753	32.767028
705.608548	58846.521176	32.772045
706.187024	58939.430541	32.777063
707.052029	59051.919035	32.782080
708.029214	59190.675788	32.787098
708.572013	59283.441002	32.792116
709.359718	59385.448593	32.797133
710.281812	59485.513573	32.802151
711.137442	59594.809331	32.807168
711.369669	59715.469017	32.812186
712.709433	59806.771753	32.817204
713.186167	59881.472054	32.822221
714.083338	60009.739217	32.827239
714.759319	60119.857401	32.832256
715.509069	60215.449000	32.837274
716.380622	60303.545394	32.842292
717.261848	60399.703841	32.847309
717.708216	60503.321714	32.852327
718.673647	60604.497327	32.857344
719.304914	60703.226207	32.862362
720.465800	60780.489933	32.867380
721.056001	60872.837627	32.872397
721.736571	60961.657264	32.877415
722.759180	61045.971967	32.882432
723.219942	61168.435287	32.887450
724.232136	61260.708756	32.892468
724.750621	61331.546392	32.897485
725.111114	61406.650746	32.902503
725.887883	61493.213428	32.907520
726.479397	61603.277874	32.912538
727.198877	61700.038025	32.917556
727.721819	61791.491027	32.922573
727.924155	61898.948162	32.927591
729.054264	61981.195152	32.932608
729.275261	62073.817879	32.937626
729.883288	62168.481584	32.942644
730.544451	62292.365856	32.947661
731.099422	62417.842054	32.952679
732.229657	62526.647085	32.957696
732.698308	62633.526959	32.962714
733.184935	62735.885695	32.967732
734.057312	62844.482223	32.972749
734.361144	62973.163305	32.977767
735.243857	63071.710579	32.982784
735.921835	63195.749279	32.987802
736.292817	63335.943020	32.992820
737.805281	63459.112389	32.997837
738.080147	63571.711001	33.002855
738.828437	63671.136606	33.007872
739.513755	63815.592115	33.012890
740.287337	63933.172880	33.017908
741.423361	64066.583741	33.022925
742.147580	64206.984276	33.027943
743.223356	64303.893946	33.032960
743.828900	64426.883960	33.037978
744.776342	64551.094988	33.042996
745.572681	64650.713367	33.048013
746.156997	64767.331553	33.053031
747.006891	64897.154464	33.058048
747.616291	65033.363811	33.063066
748.423586	65150.320270	33.068084
749.109854	65254.535917	33.073101
749.978258	65374.896735	33.078119
750.597739	65501.929842	33.083136
751.545262	65620.325917	33.088154
752.381712	65729.613737	33.093172
752.986057	65843.763286	33.098189
753.766757	65978.503132	33.103207
754.681329	66112.140870	33.108224
755.342820	66225.467695	33.113242
755.709127	66342.756598	33.118260
757.120677	66461.226263	33.123277
757.267642	66598.584272	33.128295
758.793350	66711.126296	33.133312
759.151196	66855.486605	33.138330
759.742850	66982.350111	33.143348
760.882362	67080.950120	33.148365
761.263086	67214.973925	33.153383
762.375086	67323.118451	33.158400
763.032748	67459.259992	33.163418
763.589083	67581.587939	33.168436
764.856843	67690.056333	33.173453
765.612168	67813.907859	33.178471
766.187424	67932.701048	33.183488
767.211654	68042.058577	33.188506
768.019497	68170.828031	33.193524
768.861508	68288.953366	33.198541
769.543898	68395.992278	33.203559
770.512895	68506.676269	33.208576
771.308487	68615.638369	33.213594
772.093424	68737.391686	33.218612
772.753066	68837.482698	33.223629
773.357072	68956.118923	33.228647
774.442762	69070.345811	33.233664
774.911184	69182.589035	33.238682
775.779513	69311.456682	33.243700
776.822610	69419.686687	33.248717
777.096680	69533.462187	33.253735
777.915342	69623.364943	33.258752
778.878551	69736.180590	33.263770
779.313796	69834.397839	33.268788
780.305472	69938.175625	33.273805
780.778644	70063.092279	33.278823
781.498785	70175.419361	33.283840
781.727913	70296.824637	33.288858
782.542845	70424.898685	33.293876
783.335996	70547.900308	33.298893
784.069267	70667.713438	33.303911
785.077435	70790.712581	33.308928
786.151226	70925.018702	33.313946
786.404756	71069.147116	33.318964
787.411982	71166.877800	33.323981
788.376015	71290.380291	33.328999
788.889258	71427.911813	33.334016
789.753906	71579.125200	33.339034
790.373717	71707.207619	33.344052
791.619982	71820.265856	33.349069
791.947706	71937.282645	33.354087
792.598339	72081.725398	33.359104
793.499733	72238.103091	33.364122
794.362897	72370.006221	33.369140
795.403591	72485.757533	33.374157
795.908800	72629.741154	33.379175
796.963480	72778.883062	33.384192
797.679647	72888.234413	33.389210
798.482657	73042.509725	33.394228
799.170803	73190.968918	33.399245
799.702018	73317.494870	33.404263
800.754989	73438.864244	33.409280
801.530900	73592.300689	33.414298
802.115325	73747.034500	33.419316
803.304799	73885.639990	33.424333
804.014689	74020.873037	33.429351
805.006601	74157.830903	33.434368
805.709378	74317.456203	33.439386
806.194432	74472.034582	33.444404
807.262268	74590.796423	33.449421
807.938865	74734.576157	33.454439
808.601879	74882.298677	33.459456
809.666866	75032.289243	33.464474
810.108488	75184.843689	33.469492
811.033803	75309.627850	33.474509
812.114123	75461.218753	33.479527
812.716673	75616.886243	33.484544
813.953557	75766.208482	33.489562
814.780272	75903.754866	33.494580
816.088710	76036.068589	33.499597
816.606035	76202.783251	33.504615
817.468091	76324.415390	33.509632
818.237754	76458.173983	33.514650
818.945505	76618.207499	33.519668
820.018343	76750.336802	33.524685
820.900595	76878.368704	33.529703
821.445747	77020.876179	33.534720
822.553644	77166.011080	33.539738
822.974450	77301.679122	33.544756
823.964830	77445.317454	33.549773
824.835133	77604.774809	33.554791
825.639147	77751.045232	33.559808
826.662920	77868.282772	33.564826
827.102864	78009.384723	33.569844
828.110811	78161.341534	33.574861
829.024933	78294.296924	33.579879
829.722533	78435.865030	33.584896
830.748502	78563.743897	33.589914
831.364227	78708.698307	33.594932
832.254446	78824.925750	33.599949
833.058263	78967.396810	33.604967
833.697008	79113.981865	33.609984
834.698307	79229.984379	33.615002
835.357066	79353.779371	33.620020
836.274551	79493.553309	33.625037
836.812871	79647.628191	33.630055
837.153763	79794.007605	33.635072
838.056063	79927.038018	33.640090
838.656903	80077.949373	33.645108
839.532315	80233.326219	33.650125
840.646131	80386.349776	33.655143
841.373005	80527.028236	33.660160
842.624214	80666.539388	33.665178
843.276190	80842.925552	33.670196
844.013816	80999.506993	33.675213
845.033086	81133.208430	33.680231
846.069368	81260.032141	33.685248
846.732552	81417.539659	33.690266
847.490486	81599.404780	33.695284
848.693964	81752.087633	33.700301
849.448977	81901.258971	33.705319
850.158108	82053.683922	33.710336
851.017988	82202.928504	33.715354
851.750786	82351.682677	33.720372
852.619310	82488.004295	33.725389
853.640153	82659.112429	33.730407
854.848021	82832.594800	33.735424
855.963350	82966.057227	33.740442
856.737411	83119.883011	33.745460
857.685103	83265.963489	33.750477
858.993142	83401.218543	33.755495
859.257517	83566.619552	33.760512
860.568387	83720.019167	33.765530
861.127244	83861.695140	33.770548
862.046342	84021.848209	33.775565
863.021682	84170.915905	33.780583
863.989723	84334.732303	33.785600
864.759731	84456.987122	33.790618
865.502195	84604.331070	33.795636
866.468123	84757.927495	33.800653
867.208523	84921.380806	33.805671
867.786681	85076.118892	33.810688
869.201613	85210.924202	33.815706
870.307981	85366.133763	33.820724
871.204721	85512.224411	33.825741
871.976260	85644.544610	33.830759
872.573610	85806.256400	33.835776
873.386134	85962.942020	33.840794
873.822789	86098.540427	33.845812
874.698436	86265.739077	33.850829
876.376913	86418.545676	33.855847
876.890802	86580.105858	33.860864
877.898240	86744.571987	33.865882
878.328085	86896.436424	33.870900
879.119128	87053.537927	33.875917
880.067781	87219.200290	33.880935
880.804158	87373.010262	33.885952
881.681386	87517.066853	33.890970
882.319999	87673.482761	33.895988
883.336695	87844.794859	33.901005
884.011615	88020.340655	33.906023
884.922672	88189.382260	33.911040
885.905155	88336.988835	33.916058
886.875273	88518.551257	33.921076
887.853946	88668.109401	33.926093
888.655087	88820.722358	33.931111
889.541027	88985.275026	33.936128
890.718821	89145.541181	33.941146
891.202031	89287.224996	33.946164
891.745718	89436.549820	33.951181
892.913589	89603.711569	33.956199
893.628571	89758.179891	33.961216
894.647316	89902.012684	33.966234
895.507176	90084.522972	33.971252
896.202732	90246.027928	33.976269
897.078385	90399.822158	33.981287
897.684756	90572.215439	33.986304
899.031977	90745.038189	33.991322
899.924574	90922.183395	33.996340
901.093760	91079.287451	34.001357
901.920700	91228.633804	34.006375
901.980235	91411.046009	34.011392
903.234615	91587.370738	34.016410
904.243947	91760.300979	34.021428
905.087404	91940.695652	34.026445
906.290224	92106.951719	34.031463
906.912678	92287.227296	34.036480
907.923574	92462.953212	34.041498
908.912421	92650.638628	34.046516
909.748224	92821.535789	34.051533
911.069005	92986.550760	34.056551
911.904647	93167.158497	34.061568
912.728038	93344.719183	34.066586
913.848255	93528.617877	34.071604
914.932300	93694.632447	34.076621
915.555766	93864.629101	34.081639
916.592437	94030.381667	34.086656
917.481847	94215.728730	34.091674
918.527934	94409.032188	34.096692
919.336540	94582.629835	34.101709
920.206883	94748.851496	34.106727
921.103642	94934.791457	34.111744
921.991303	95107.620318	34.116762
923.025083	95289.034007	34.121780
924.235121	95472.287079	34.126797
925.224875	95647.083977	34.131815
926.068694	95815.114835	34.136832
927.377643	95970.575840	34.141850
928.023936	96165.009961	34.146868
928.731655	96337.326596	34.151885
930.334275	96500.780931	34.156903
931.584517	96669.016398	34.161920
932.438202	96850.984128	34.166938
933.241930	97030.334646	34.171956
934.123350	97187.912125	34.176973
934.810006	97337.737190	34.181991
935.660440	97529.945673	34.187008
937.148323	97689.420113	34.192026
937.717501	97851.978002	34.197044
938.561130	98033.063618	34.202061
939.872757	98208.021845	34.207079
940.756931	98363.890961	34.212096
941.407034	98526.224699	34.217114
942.526111	98712.194578	34.222132
943.455953	98882.181849	34.227149
944.536886	99055.335746	34.232167
945.086486	99234.953111	34.237184
946.031653	99415.702880	34.242202
946.813329	99577.173498	34.247220
948.105938	99751.588668	34.252237
949.341436	99915.809886	34.257255
949.785596	100099.527654	34.262272
950.600984	100273.379551	34.267290
951.603443	100438.497289	34.272308
952.507071	100597.839960	34.277325
953.691761	100754.206166	34.282343
954.417051	100932.458283	34.287360
955.220879	101104.646549	34.292378
956.655851	101256.011286	34.297396
957.004487	101411.987832	34.302413
958.159068	101578.468042	34.307431
959.035014	101771.167127	34.312448
959.534652	101940.720700	34.317466
960.552742	102116.210539	34.322484
961.622493	102303.620657	34.327501
962.651811	102477.338461	34.332519
963.133670	102658.954067	34.337536
963.961849	102841.419140	34.342554
965.222580	103035.374831	34.347572
966.200093	103228.194818	34.352589
967.477287	103399.959627	34.357607
968.210191	103599.147736	34.362624
968.981657	103801.908250	34.367642
970.046726	103978.409837	34.372660
971.068448	104160.206561	34.377677
972.319936	104357.048274	34.382695
973.130501	104535.526817	34.387712
974.255403	104745.251774	34.392730
975.884824	104931.328747	34.397748
976.557742	105098.120370	34.402765
977.684763	105288.816353	34.407783
978.460578	105501.891257	34.412800
979.729574	105676.148341	34.417818
980.590991	105845.091800	34.422836
981.381538	106044.042328	34.427853
982.685528	106233.405331	34.432871
983.200446	106431.213916	34.437888
984.145713	106622.297956	34.442906
985.357862	106802.017535	34.447924
986.089982	107007.830063	34.452941
987.216488	107213.680409	34.457959
988.106740	107396.522001	34.462976
989.179861	107575.459314	34.467994
989.972681	107785.143279	34.473012
991.591071	107991.805043	34.478029
993.183350	108159.629603	34.483047
993.839829	108350.178657	34.488064
995.118625	108540.714996	34.493082
996.168757	108711.304896	34.498100
996.674215	108915.839923	34.503117
997.996461	109103.067516	34.508135
998.912478	109282.865585	34.513152
999.782012	109480.226903	34.518170
1000.761466	109677.204234	34.523188
1001.788818	109861.864083	34.528205
1002.851909	110048.786481	34.533223
1003.711898	110236.453006	34.538240
1004.582566	110430.540713	34.543258
1005.830331	110629.785973	34.548276
1006.221538	110840.687639	34.553293
1007.377776	111026.892183	34.558311
1008.367250	111213.416874	34.563328
1009.335745	111424.367137	34.568346
1010.066935	111627.783661	34.573364
1011.030415	111834.976013	34.578381
1012.123814	112034.890488	34.583399
1013.214771	112255.023038	34.588416
1013.945733	112455.773132	34.593434
1015.537527	112635.279408	34.598452
1016.403717	112854.693912	34.603469
1017.407451	113048.715137	34.608487
1018.796783	113252.047852	34.613504
1019.423310	113428.881258	34.618522
1020.233986	113618.352830	34.623540
1021.123553	113804.316456	34.628557
1022.380507	113995.629755	34.633575
1023.283249	114208.284594	34.638592
1024.057404	114407.775134	34.643610
1025.137880	114588.645439	34.648628
1025.762172	114797.917812	34.653645
1026.954007	115003.665028	34.658663
1028.106110	115205.847915	34.663680
1028.771064	115423.884682	34.668698
1029.887915	115642.963373	34.673716
1030.793380	115866.474647	34.678733
1031.621335	116059.836690	34.683751
1032.653547	116279.947860	34.688768
1033.496596	116516.485361	34.693786
1034.453659	116738.778915	34.698804
1035.318848	116957.174697	34.703821
1036.470280	117174.904142	34.708839
1037.702528	117412.031080	34.713856
1038.785721	117642.153186	34.718874
1040.365974	117865.201625	34.723892
1041.642720	118109.485287	34.728909
1042.269825	118332.086642	34.733927
1043.542247	118540.317165	34.738944
1044.425129	118765.008202	34.743962
1045.507580	118991.847288	34.748980
1046.434178	119224.047973	34.753997
1047.598330	119457.744413	34.759015
1048.706802	119691.033846	34.764032
1049.635299	119912.216771	34.769050
1050.917625	120141.604078	34.774068
1051.867610	120370.642634	34.779085
1053.104247	120604.374492	34.784103
1054.047964	120823.699363	34.789120
1055.110720	121074.885938	34.794138
1056.503205	121286.664484	34.799156
1057.614317	121524.719963	34.804173
1058.658028	121765.132680	34.809191
1059.920744	121980.599677	34.814208
1060.772774	122198.505603	34.819226
1061.598936	122414.820840	34.824244
1062.797558	122669.736869	34.829261
1063.922464	122887.932365	34.834279
1065.467182	123112.028543	34.839296
1066.093469	123354.563435	34.844314
1067.451738	123584.687766	34.849332
1068.324217	123828.427775	34.854349
1069.494210	124041.454247	34.859367
1071.094112	124249.114320	34.864384
1071.864931	124482.054493	34.869402
1073.347090	124713.624504	34.874420
1073.916822	124950.137149	34.879437
1074.684761	125167.267953	34.884455
1075.907989	125378.102911	34.889472
1076.790829	125621.779950	34.894490
1077.793501	125870.736451	34.899508
1078.885768	126106.829855	34.904525
1079.755703	126357.104961	34.909543
1080.980901	126573.118644	34.914560
1081.517385	126830.245557	34.919578
1082.849556	127066.877210	34.924596
1084.018925	127303.157395	34.929613
1085.020584	127541.228741	34.934631
1086.198814	127798.017163	34.939648
1087.247597	128049.278018	34.944666
1088.435779	128271.380706	34.949684
1089.290447	128481.639230	34.954701
1090.357008	128722.915644	34.959719
1091.645681	128960.811321	34.964736
1092.416488	129181.772828	34.969754
1094.023210	129402.496538	34.974772
1095.245176	129652.297132	34.979789
1096.105407	129874.554335	34.984807
1097.646981	130104.989868	34.989824
1098.377319	130329.122288	34.994842
1099.319135	130547.720557	34.999860
1100.448882	130800.879157	35.004877
1101.357514	131034.987762	35.009895
1102.726665	131256.600512	35.014912
1103.624853	131504.872466	35.019930
1104.857143	131751.266001	35.024948
1106.239964	132001.920916	35.029965
1107.130308	132233.975456	35.034983
1108.144823	132471.588474	35.040000
1109.143575	132712.412840	35.045018
1110.123262	132972.674178	35.050036
1111.242544	133228.997769	35.055053
1112.393017	133477.281710	35.060071
1113.367319	133727.219221	35.065088
1114.378658	133979.015988	35.070106
1115.711021	134228.822283	35.075124
1116.797323	134499.029451	35.080141
1117.691144	134771.463717	35.085159
1119.024103	135006.786760	35.090176
1120.147030	135267.081273	35.095194
1121.392660	135526.039252	35.100212
1122.290012	135782.027029	35.105229
1123.408118	136040.528475	35.110247
1124.598536	136303.089405	35.115264
1125.668314	136574.711235	35.120282
1127.154632	136815.435342	35.125300
1127.890491	137099.768645	35.130317
1129.080140	137382.318051	35.135335
1130.552077	137628.210296	35.140352
1131.514541	137876.964914	35.145370
1132.816083	138145.658372	35.150388
1134.178408	138432.765031	35.155405
1135.103657	138689.835996	35.160423
1136.402745	138942.815604	35.165440
1137.263393	139211.514463	35.170458
1138.338633	139487.444765	35.175476
1139.428530	139771.730036	35.180493
1140.492065	140036.395685	35.185511
1141.851273	140275.340367	35.190528
1143.051885	140553.895960	35.195546
1144.151767	140840.191917	35.200564
1145.257687	141115.027538	35.205581
1146.141956	141370.401601	35.210599
1147.389236	141635.721522	35.215616
1148.619800	141931.438467	35.220634
1150.018391	142208.986075	35.225652
1151.399564	142470.765568	35.230669
1152.404148	142738.289683	35.235687
1153.441265	143016.436084	35.240704
1154.849226	143299.988511	35.245722
1155.995628	143561.739037	35.250740
1157.329171	143825.045662	35.255757
1158.433446	144100.615727	35.260775
1159.732505	144363.919479	35.265792
1160.507283	144629.759068	35.270810
1161.917525	144900.263612	35.275828
1162.790577	145166.788509	35.280845
1163.881606	145452.072047	35.285863
1165.257175	145701.462727	35.290880
1166.040952	145981.868533	35.295898
1167.362913	146230.232003	35.300916
1168.548327	146474.980342	35.305933
1169.583692	146736.646268	35.310951
1170.887531	146994.313307	35.315968
1171.701300	147273.519728	35.320986
1173.378107	147532.980574	35.326004
1174.232209	147807.162732	35.331021
1174.880079	148070.931483	35.336039
1176.039958	148334.097717	35.341056
1177.186299	148614.502533	35.346074
1178.446785	148893.292792	35.351092
1179.728494	149175.074631	35.356109
1180.535568	149462.187361	35.361127
1181.948180	149750.026749	35.366144
1183.262586	150038.544105	35.371162
1184.248796	150321.043107	35.376180
1185.268917	150608.801891	35.381197
1186.318719	150895.074188	35.386215
1187.630400	151175.433455	35.391232
1188.587303	151491.238121	35.396250
1189.563088	151802.349739	35.401268
1191.107992	152095.233480	35.406285
1192.172308	152407.553128	35.411303
1193.399653	152694.900814	35.416320
1194.535120	153009.737708	35.421338
1195.437630	153328.065570	35.426356
1197.008581	153606.612057	35.431373
1197.800578	153924.519298	35.436391
1199.193589	154234.072971	35.441408
1200.587854	154537.413945	35.446426
1201.377298	154861.633297	35.451444
1202.906212	155185.124522	35.456461
1203.802032	155522.104667	35.461479
1205.360213	155809.155076	35.466496
1206.568516	156122.572517	35.471514
1207.792702	156451.972179	35.476532
1209.222018	156771.814756	35.481549
1210.205754	157082.511844	35.486567
1211.866361	157407.255782	35.491584
1213.247595	157712.894531	35.496602
1214.498991	158023.542257	35.501620
1215.884612	158332.521243	35.506637
1216.707531	158661.688699	35.511655
1218.158837	158981.571104	35.516672
1219.552135	159270.792668	35.521690
1220.720229	159599.200573	35.526708
1221.907085	159905.535355	35.531725
1223.015494	160232.626354	35.536743
1224.132754	160548.808877	35.541760
1225.597896	160860.686729	35.546778
1226.917232	161187.154451	35.551796
1228.287400	161513.083607	35.556813
1229.849413	161809.996024	35.561831
1230.965711	162108.709498	35.566848
1232.568279	162429.748837	35.571866
1233.699946	162741.556628	35.576884
1234.964719	163038.971060	35.581901
1236.140065	163336.541951	35.586919
1237.759429	163635.754393	35.591936
1239.018485	163946.383093	35.596954
1240.279817	164235.687185	35.601972
1241.989737	164542.274937	35.606989
1242.826723	164852.079277	35.612007
1244.209938	165136.421549	35.617024
1245.283256	165422.288605	35.622042
1246.190423	165726.733808	35.627060
1247.859586	166017.594136	35.632077
1248.813635	166319.320759	35.637095
1250.206486	166584.982561	35.642112
1251.642683	166867.640256	35.647130
1252.697073	167152.024923	35.652148
1254.145403	167422.757840	35.657165
1255.532442	167699.554681	35.662183
1256.325501	167976.387894	35.667200
1257.597794	168268.991111	35.672218
1258.800228	168563.219215	35.677236
1260.345570	168845.389675	35.682253
1261.164780	169137.857802	35.687271
1262.442898	169418.896051	35.692288
1263.575258	169720.896075	35.697306
1264.749423	170024.654968	35.702324
1265.644693	170307.373500	35.707341
1267.084426	170636.520725	35.712359
1268.295060	170948.870160	35.717376
1269.786327	171247.890199	35.722394
1270.520326	171548.699471	35.727412
1272.103420	171862.871748	35.732429
1273.175546	172200.808481	35.737447
1274.342270	172515.409300	35.742464
1275.983738	172825.391156	35.747482
1276.688202	173139.869544	35.752500
1278.014939	173447.306227	35.757517
1279.121735	173781.746615	35.762535
1280.501491	174111.779122	35.767552
1281.815663	174442.725773	35.772570
1282.860559	174784.886289	35.777588
1284.398085	175093.758419	35.782605
1285.385169	175426.428398	35.787623
1286.862497	175771.976421	35.792640
1288.383000	176117.786336	35.797658
1289.604820	176456.186167	35.802676
1291.125399	176772.952735	35.807693
1292.447268	177108.130003	35.812711
1293.875842	177464.497933	35.817728
1295.377805	177782.492521	35.822746
1296.580272	178121.097627	35.827764
1298.119211	178442.351956	35.832781
1299.024641	178784.843326	35.837799
1300.453561	179141.997632	35.842816
1301.982752	179468.857029	35.847834
1302.934670	179786.549309	35.852852
1304.558506	180128.423785	35.857869
1305.570921	180471.277223	35.862887
1307.115261	180816.532736	35.867904
1308.477729	181144.864771	35.872922
1309.352708	181494.436298	35.877940
1310.616095	181839.351737	35.882957
1312.407538	182197.140661	35.887975
1313.539581	182533.274375	35.892992
1314.625508	182866.003766	35.898010
1316.087485	183203.673896	35.903028
1317.604400	183552.214298	35.908045
1318.797879	183905.874602	35.913063
1320.214021	184251.326720	35.918080
1321.502073	184601.498427	35.923098
1322.523550	184941.587881	35.928116
1324.120934	185291.065787	35.933133
1325.235245	185653.419872	35.938151
1326.656376	185991.178093	35.943168
1328.162917	186334.344157	35.948186
1329.855727	186668.355498	35.953204
1331.068931	186995.835036	35.958221
1332.099563	187368.013390	35.963239
1333.643315	187725.944085	35.968256
1335.154090	188042.261620	35.973274
1336.378035	188359.884939	35.978292
1337.555724	188690.845698	35.983309
1339.012124	189025.303883	35.988327
1340.256786	189363.378572	35.993344
1341.697586	189679.285375	35.998362
1342.627020	190003.478419	36.003380
1343.981041	190338.900628	36.008397
1345.237896	190694.143128	36.013415
1345.930912	191031.087501	36.018432
1347.191232	191375.086895	36.023450
1348.574319	191745.953967	36.028468
1349.801562	192103.253763	36.033485
1351.266069	192459.919959	36.038503
1352.498582	192795.224134	36.043520
1354.152129	193157.067989	36.048538
1355.174169	193547.212513	36.053556
1356.749534	193916.995194	36.058573
1358.350464	194260.917147	36.063591
1359.768834	194640.416123	36.068608
1361.150723	195001.897022	36.073626
1362.493611	195383.787003	36.078644
1363.767751	195731.985876	36.083661
1364.595862	196098.007828	36.088679
1365.880228	196487.759767	36.093696
1367.172967	196866.772721	36.098714
1368.474674	197241.051192	36.103732
1370.142537	197647.276137	36.108749
1371.602234	198013.420845	36.113767
1372.650353	198397.040951	36.118784
1374.105467	198784.227079	36.123802
1375.195337	199193.921519	36.128820
1376.658591	199573.315953	36.133837
1378.274327	199978.129587	36.138855
1379.261236	200375.635157	36.143872
1380.947589	200781.038755	36.148890
1382.076188	201170.616177	36.153908
1383.591891	201577.957151	36.158925
1384.909852	201979.023264	36.163943
1386.361652	202371.118867	36.168960
1387.917081	202770.550722	36.173978
1389.189100	203196.478045	36.178996
1390.758652	203603.796776	36.184013
1392.223495	204003.377630	36.189031
1393.963670	204415.434077	36.194048
1395.590354	204811.374281	36.199066
1396.860405	205208.111940	36.204084
1398.649827	205586.444697	36.209101
1399.875852	206004.232471	36.214119
1401.177110	206417.045743	36.219136
1403.143506	206796.968071	36.224154
1404.126409	207195.630369	36.229172
1405.542564	207592.902802	36.234189
1407.774608	207999.197324	36.239207
1409.154210	208391.185287	36.244224
1410.505613	208764.311781	36.249242
1411.988466	209181.122605	36.254260
1413.432678	209563.646375	36.259277
1414.925645	209933.453821	36.264295
1416.024302	210316.089086	36.269312
1417.649790	210722.447223	36.274330
1418.863781	211111.276403	36.279348
1420.082431	211496.437058	36.284365
1421.809240	211876.842907	36.289383
1423.068891	212281.059860	36.294400
1424.404423	212678.295136	36.299418
1425.652939	213068.816762	36.304436
1427.282895	213447.379233	36.309453
1428.912296	213847.377828	36.314471
1430.251977	214236.810488	36.319488
1431.745477	214601.280311	36.324506
1432.930143	214979.313558	36.329524
1434.060596	215352.659029	36.334541
1435.490556	215729.512197	36.339559
1436.680250	216113.238359	36.344576
1438.071695	216504.424963	36.349594
1439.325107	216883.877233	36.354612
1440.820019	217286.656586	36.359629
1442.211829	217753.404979	36.364647
1443.229791	218164.470196	36.369664
1445.003540	218569.139323	36.374682
1446.025866	218954.708226	36.379700
1447.450426	219361.800342	36.384717
1449.014877	219779.360389	36.389735
1450.216112	220203.484037	36.394752
1451.723812	220601.906958	36.399770
1453.054960	221012.348528	36.404788
1454.789405	221444.669292	36.409805
1456.340183	221880.831968	36.414823
1457.464784	222296.671895	36.419840
1458.732083	222702.381334	36.424858
1460.604873	223146.979338	36.429876
1461.570532	223588.554073	36.434893
1463.291232	224020.379875	36.439911
1465.232275	224451.739264	36.444928
1466.778294	224868.103914	36.449946
1467.836881	225316.731288	36.454964
1469.509999	225762.515936	36.459981
1471.148892	226180.876699	36.464999
1472.334979	226618.998278	36.470016
1473.896901	227050.049225	36.475034
1475.557483	227497.468236	36.480052
1476.927458	227947.705461	36.485069
1478.887470	228394.062431	36.490087
1480.271133	228833.861369	36.495104
1481.862272	229260.851437	36.500122
1483.320056	229690.176376	36.505140
1484.955705	230151.325234	36.510157
1486.769260	230595.504413	36.515175
1488.179508	231012.954293	36.520192
1490.019879	231427.057860	36.525210
1491.130536	231894.954389	36.530228
1492.426813	232333.865219	36.535245
1494.348369	232753.242750	36.540263
1495.670235	233208.687953	36.545280
1497.066975	233636.587762	36.550298
1498.655351	234067.556124	36.555316
1499.724987	234511.769059	36.560333
1501.821616	234959.573202	36.565351
1503.132335	235413.985644	36.570368
1504.579869	235860.375471	36.575386
1506.222580	236294.719560	36.580404
1507.714352	236744.305143	36.585421
1509.094945	237197.314106	36.590439
1510.538236	237638.984905	36.595456
1512.153621	238078.113712	36.600474
1513.696463	238507.577603	36.605492
1515.207080	238958.969510	36.610509
1517.083467	239418.989599	36.615527
1518.533866	239850.148499	36.620544
1519.883144	240285.592601	36.625562
1521.734676	240733.655786	36.630580
1522.849074	241185.321718	36.635597
1524.848163	241614.260297	36.640615
1526.146026	242063.840383	36.645632
1527.890986	242511.366310	36.650650
1529.760911	242926.103740	36.655668
1530.927120	243353.964038	36.660685
1532.811456	243784.754943	36.665703
1533.932501	244210.947789	36.670720
1535.247513	244608.963577	36.675738
1536.949822	245041.183997	36.680756
1537.798719	245483.478376	36.685773
1539.542609	245890.494184	36.690791
1540.818709	246310.212899	36.695808
1542.391264	246750.611886	36.700826
1543.473624	247210.550899	36.705844
1545.151305	247650.705365	36.710861
1546.892729	248079.291754	36.715879
1548.211468	248540.768868	36.720896
1549.467492	248993.975717	36.725914
1551.130569	249438.606102	36.730932
1552.651176	249907.012274	36.735949
1554.077973	250379.854674	36.740967
1555.814827	250852.773558	36.745984
1556.980097	251300.486015	36.751002
1559.165852	251783.467776	36.756020
1560.195144	252253.609191	36.761037
1562.115485	252704.297784	36.766055
1563.453005	253186.150961	36.771072
1564.947589	253671.255717	36.776090
1566.750275	254144.802496	36.781108
1568.242651	254608.265049	36.786125
1569.870489	255082.451173	36.791143
1571.263073	255596.534087	36.796160
1572.629815	256075.336624	36.801178
1574.428366	256556.075093	36.806196
1576.057008	257054.293923	36.811213
1577.678576	257549.592842	36.816231
1579.247920	258041.623620	36.821248
1580.723013	258523.254836	36.826266
1582.514558	259017.916721	36.831284
1584.211647	259523.644796	36.836301
1585.714553	260015.738088	36.841319
1587.087562	260513.314636	36.846336
1588.903728	261029.997643	36.851354
1590.856949	261522.702774	36.856372
1592.285514	262008.610201	36.861389
1593.905366	262506.705051	36.866407
1595.941433	263001.835213	36.871424
1597.531397	263505.472813	36.876442
1599.167999	264004.911075	36.881460
1600.575853	264493.590556	36.886477
1602.377164	264978.902539	36.891495
1603.860594	265489.416033	36.896512
1605.549200	265991.258338	36.901530
1607.261245	266480.623532	36.906548
1608.646916	266983.429810	36.911565
1610.533848	267485.289360	36.916583
1612.342404	267976.161915	36.921600
1613.578998	268486.028446	36.926618
1615.296045	268982.859679	36.931636
1617.034734	269477.781679	36.936653
1618.663434	269990.300323	36.941671
1619.941851	270475.466320	36.946688
1621.476466	270968.794738	36.951706
1623.482631	271487.320824	36.956724
1624.903829	272016.815276	36.961741
1626.678336	272499.737925	36.966759
1628.516092	272996.748158	36.971776
1629.970584	273514.498910	36.976794
1631.697401	273993.845662	36.981812
1632.932503	274521.360395	36.986829
1634.628559	275024.208331	36.991847
1636.154570	275543.315858	36.996864
1637.583136	276024.766377	37.001882
1639.212281	276518.655702	37.006900
1640.791590	277017.531286	37.011917
1642.180212	277479.578308	37.016935
1644.215399	277996.895304	37.021952
1645.820136	278487.508082	37.026970
1647.463637	278977.707050	37.031988
1648.742735	279494.866225	37.037005
1650.464014	279973.416016	37.042023
1652.061079	280488.767730	37.047040
1653.865250	280988.461728	37.052058
1655.693488	281476.567223	37.057076
1657.566527	281995.070449	37.062093
1659.078782	282483.632127	37.067111
1660.759850	283001.834203	37.072128
1662.466331	283520.386326	37.077146
1664.292143	284007.927157	37.082164
1665.575764	284540.872827	37.087181
1667.228159	285060.166202	37.092199
1668.727138	285577.349630	37.097216
1670.166208	286103.177899	37.102234
1672.074459	286633.143757	37.107252
1673.555140	287174.278840	37.112269
1674.877979	287715.107937	37.117287
1676.895674	288240.656058	37.122304
1678.382652	288772.843435	37.127322
1680.268170	289314.767973	37.132340
1681.972446	289877.701572	37.137357
1683.486749	290403.121987	37.142375
1685.340037	290946.315835	37.147392
1686.915813	291507.536988	37.152410
1688.411555	292066.102013	37.157428
1690.018667	292627.084798	37.162445
1692.016131	293167.731399	37.167463
1693.704567	293709.239554	37.172480
1695.380355	294284.351787	37.177498
1697.335950	294829.773509	37.182516
1698.908987	295394.051820	37.187533
1700.466435	295978.700657	37.192551
1702.171355	296524.537153	37.197568
1703.727320	297089.445299	37.202586
1705.804718	297661.097092	37.207604
1707.614866	298226.770504	37.212621
1709.390580	298789.703652	37.217639
1711.293278	299362.416984	37.222656
1712.991706	299931.960759	37.227674
1714.852670	300483.035257	37.232692
1716.301290	301052.792052	37.237709
1717.919892	301605.449962	37.242727
1719.764170	302181.916650	37.247744
1721.135409	302758.534298	37.252762
1723.213329	303341.152947	37.257780
1724.973100	303908.759730	37.262797
1726.418866	304467.754395	37.267815
1728.617222	305055.397045	37.272832
1729.857750	305656.045133	37.277850
1731.648037	306214.667877	37.282868
1733.675977	306783.178277	37.287885
1735.334184	307373.841416	37.292903
1736.980755	307955.334377	37.297920
1738.456818	308529.080311	37.302938
1740.334579	309098.083282	37.307956
1742.150640	309683.371667	37.312973
1743.647511	310266.804001	37.317991
1745.523031	310868.200901	37.323008
1747.392826	311447.271607	37.328026
1749.213787	312016.746801	37.333044
1751.044436	312598.253803	37.338061
1752.223091	313171.179031	37.343079
1754.320919	313736.203038	37.348096
1756.058756	314306.031205	37.353114
1758.062717	314848.766059	37.358132
1759.198884	315418.786887	37.363149
1760.773704	315999.371270	37.368167
1763.016726	316565.645696	37.373184
1764.300095	317125.878048	37.378202
1766.010643	317684.715216	37.383220
1768.219008	318273.836549	37.388237
1769.589297	318865.224380	37.393255
1771.454465	319449.415648	37.398272
1772.701466	320022.759783	37.403290
1774.468214	320610.614245	37.408308
1776.374047	321212.203466	37.413325
1778.018350	321817.233123	37.418343
1779.558259	322422.553943	37.423360
1781.523795	323037.422571	37.428378
1783.406029	323630.919666	37.433396
1784.757897	324268.679675	37.438413
1786.566846	324872.511888	37.443431
1788.731503	325495.348250	37.448448
1790.038695	326137.235940	37.453466
1791.932044	326755.889947	37.458484
1793.708969	327372.297371	37.463501
1795.496475	328010.303621	37.468519
1797.430950	328652.671413	37.473536
1799.307022	329308.295251	37.478554
1801.042962	329930.040897	37.483572
1802.795552	330554.443165	37.488589
1804.664240	331216.115266	37.493607
1806.482528	331875.833365	37.498624
1808.094074	332526.946254	37.503642
1809.824222	333170.415985	37.508660
1811.820074	333817.465031	37.513677
1813.351318	334487.177722	37.518695
1815.747354	335155.165808	37.523712
1817.474139	335810.563119	37.528730
1819.008867	336446.183226	37.533748
1821.398962	337117.245654	37.538765
1822.961381	337778.485233	37.543783
1825.066737	338434.829335	37.548800
1826.647626	339122.881317	37.553818
1828.612609	339766.006645	37.558836
1830.480415	340434.625796	37.563853
1831.891517	341096.483435	37.568871
1833.943223	341765.385043	37.573888
1836.108624	342430.883179	37.578906
1837.645130	343106.781738	37.583924
1839.407689	343803.422159	37.588941
1841.110680	344478.868600	37.593959
1843.012190	345148.968270	37.598976
1844.869185	345845.716608	37.603994
1846.938714	346516.201272	37.609012
1848.984294	347187.797311	37.614029
1850.353279	347856.348367	37.619047
1852.464463	348546.112140	37.624064
1854.540039	349245.109855	37.629082
1856.366881	349912.870930	37.634100
1858.376045	350583.688530	37.639117
1859.969200	351263.726603	37.644135
1862.206262	351930.959272	37.649152
1864.158850	352630.560268	37.654170
1865.964516	353298.097658	37.659188
1867.756543	353984.507768	37.664205
1869.409990	354665.118866	37.669223
1871.413147	355328.583575	37.674240
1873.487905	355997.482183	37.679258
1875.095969	356680.302410	37.684276
1876.781672	357347.671000	37.689293
1878.483164	357997.924080	37.694311
1880.351327	358644.181324	37.699328
1882.257860	359318.866377	37.704346
1883.687335	359974.741430	37.709364
1885.698794	360654.589116	37.714381
1887.497785	361324.616090	37.719399
1889.161175	362015.002954	37.724416
1890.839303	362697.459702	37.729434
1892.714524	363372.235662	37.734452
1894.683736	364087.654273	37.739469
1896.512255	364783.319718	37.744487
1897.918579	365467.372405	37.749504
1899.600598	366158.471192	37.754522
1901.301121	366886.847221	37.759540
1903.801848	367622.941845	37.764557
1905.490821	368338.709631	37.769575
1907.577558	369031.440728	37.774592
1909.510808	369787.171142	37.779610
1911.282182	370496.466836	37.784628
1913.576088	371225.118772	37.789645
1915.067141	371957.744466	37.794663
1917.125929	372689.323505	37.799680
1919.312306	373416.783234	37.804698
1921.149646	374137.640641	37.809716
1923.457485	374878.747754	37.814733
1925.396312	375624.770211	37.819751
1927.435808	376359.144466	37.824768
1929.335779	377107.272805	37.829786
1931.091604	377858.553913	37.834804
1933.234216	378598.596330	37.839821
1935.043126	379329.548338	37.844839
1937.011180	380091.144147	37.849856
1938.952949	380843.445946	37.854874
1940.590453	381586.119709	37.859892
1942.776926	382328.483844	37.864909
1944.684749	383101.890030	37.869927
1946.669523	383877.294278	37.874944
1948.735490	384629.491314	37.879962
1950.297297	385388.600535	37.884980
1952.484139	386148.527327	37.889997
1954.493062	386912.776135	37.895015
1956.576101	387689.012622	37.900032
1958.311984	388460.698761	37.905050
1960.278205	389215.950421	37.910068
1962.264559	389997.826166	37.915085
1964.189905	390784.915166	37.920103
1966.323114	391546.751341	37.925120
1968.210169	392309.116628	37.930138
1970.175275	393086.584234	37.935156
1972.584750	393888.927949	37.940173
1974.146781	394670.858287	37.945191
1976.091500	395433.086324	37.950208
1977.812241	396213.734297	37.955226
1979.875811	397023.479453	37.960244
1981.792872	397815.865088	37.965261
1983.733850	398607.338712	37.970279
1985.322614	399385.695570	37.975296
1987.806764	400184.539488	37.980314
1989.353708	400997.277591	37.985332
1991.495224	401803.660799	37.990349
1993.419869	402594.041429	37.995367
1995.489866	403398.542098	38.000384
1997.377623	404213.465157	38.005402
1999.320619	405025.745878	38.010420
2001.580656	405810.686456	38.015437
2003.597101	406604.285704	38.020455
2005.858773	407383.481081	38.025472
2007.804113	408177.706242	38.030490
2009.652683	408949.806309	38.035508
2011.742082	409709.937478	38.040525
2013.616284	410486.322606	38.045543
2015.764322	411290.989133	38.050560
2017.945519	412058.538673	38.055578
2019.685393	412827.329842	38.060596
2021.870526	413599.065417	38.065613
2023.678228	414399.186328	38.070631
2025.593382	415191.970386	38.075648
2027.932930	415971.033489	38.080666
2029.535140	416769.292989	38.085684
2031.589066	417582.853040	38.090701
2033.715052	418381.052932	38.095719
2035.959193	419176.980060	38.100736
2038.012275	419969.925736	38.105754
2039.501910	420798.495792	38.110772
2042.060648	421616.479850	38.115789
2043.695334	422424.486052	38.120807
2045.919998	423233.711211	38.125824
2048.051270	424057.890722	38.130842
2049.887375	424877.761936	38.135860
2052.113850	425711.644890	38.140877
2053.872429	426538.436993	38.145895
2055.945037	427365.402744	38.150912
2058.100511	428218.859368	38.155930
2060.076315	429073.935997	38.160948
2062.132091	429902.489361	38.165965
2064.441433	430753.603680	38.170983
2066.559044	431597.783512	38.176000
2068.501200	432423.585382	38.181018
2070.286831	433295.300120	38.186036
2072.833315	434141.546327	38.191053
2074.983713	435008.531016	38.196071
2076.895111	435846.215098	38.201088
2078.996170	436715.371765	38.206106
2080.775526	437594.874235	38.211124
2083.289856	438439.704245	38.216141
2085.563091	439290.110083	38.221159
2087.554558	440172.363607	38.226176
2090.111917	441047.303399	38.231194
2092.033956	441912.901617	38.236212
2094.073544	442756.991536	38.241229
2096.130425	443641.831135	38.246247
2098.111464	444516.680126	38.251264
2100.468863	445390.015820	38.256282
2102.269669	446248.230266	38.261300
2104.182125	447122.127163	38.266317
2106.587298	448014.575889	38.271335
2108.359486	448889.993373	38.276352
2110.555815	449771.831197	38.281370
2112.492458	450673.049661	38.286388
2115.066998	451556.825826	38.291405
2116.767462	452423.613332	38.296423
2118.791181	453302.096916	38.301440
2121.455928	454216.954300	38.306458
2123.222444	455122.310959	38.311476
2125.448062	455991.191600	38.316493
2128.079573	456874.381451	38.321511
2129.732927	457765.229563	38.326528
2131.769528	458680.399099	38.331546
2133.711424	459586.239885	38.336564
2136.192806	460464.952078	38.341581
2138.453460	461350.943190	38.346599
2140.310137	462263.706545	38.351616
2142.773325	463170.514855	38.356634
2144.725356	464043.850591	38.361652
2146.863833	464895.077734	38.366669
2149.423335	465772.888160	38.371687
2151.284699	466638.947215	38.376704
2154.210838	467498.222061	38.381722
2156.013586	468354.965896	38.386740
2158.324312	469199.812919	38.391757
2160.287316	470077.832578	38.396775
2162.331074	470953.676738	38.401792
2164.836861	471802.522014	38.406810
2166.705953	472648.049321	38.411828
2169.028940	473516.454442	38.416845
2171.202779	474386.865618	38.421863
2173.146968	475264.903710	38.426880
2175.199894	476143.994557	38.431898
2177.549655	477019.560191	38.436916
2179.447157	477902.938937	38.441933
2181.745695	478796.009342	38.446951
2183.526900	479686.546111	38.451968
2185.577491	480568.409206	38.456986
2187.944532	481494.976718	38.462004
2189.817772	482409.811619	38.467021
2192.192376	483304.620734	38.472039
2194.120857	484209.508613	38.477056
2196.328292	485153.035605	38.482074
2198.287124	486089.889187	38.487092
2200.569136	487004.121883	38.492109
2202.933688	487961.007030	38.497127
2204.602246	488898.619753	38.502144
2207.420305	489817.617752	38.507162
2209.564882	490772.216837	38.512180
2211.732164	491721.712682	38.517197
2213.826783	492667.736798	38.522215
2215.930166	493637.934537	38.527232
2218.042225	494584.305875	38.532250
2220.024398	495547.754835	38.537268
2221.988438	496510.547344	38.542285
2224.746651	497498.788682	38.547303
2226.656468	498483.933912	38.552320
2229.024348	499454.920214	38.557338
2231.264390	500430.917068	38.562356
2233.496571	501442.878988	38.567373
2235.592594	502433.917934	38.572391
2237.829015	503422.302409	38.577408
2240.071533	504392.468953	38.582426
2242.234633	505409.447369	38.587444
2244.400707	506394.438285	38.592461
2246.810695	507392.895738	38.597479
2248.805507	508405.429954	38.602496
2251.563291	509430.734459	38.607514
2253.503946	510430.696760	38.612532
2255.750817	511431.252550	38.617549
2258.040473	512452.358683	38.622567
2260.010305	513484.391767	38.627584
2262.478025	514496.616832	38.632602
2264.853248	515510.355223	38.637620
2267.153508	516526.258711	38.642637
2269.635968	517565.501941	38.647655
2271.525482	518605.630832	38.652672
2274.266765	519607.302715	38.657690
2276.311416	520620.060082	38.662708
2278.048418	521661.017717	38.667725
2280.826974	522698.962433	38.672743
2283.226606	523729.947326	38.677760
2285.611086	524747.767789	38.682778
2288.071582	525773.466493	38.687796
2290.613227	526803.716410	38.692813
2293.424645	527817.281652	38.697831
2295.551943	528835.121847	38.702848
2298.022414	529836.570783	38.707866
2300.570363	530804.504312	38.712884
2302.525353	531773.882524	38.717901
2305.368155	532741.288826	38.722919
2307.168642	533707.142269	38.727936
2309.581510	534673.485837	38.732954
2311.535643	535662.342572	38.737972
2313.513543	536669.148329	38.742989
2315.722567	537647.711175	38.748007
2318.003548	538657.449751	38.753024
2320.195393	539658.376034	38.758042
2322.306981	540651.899115	38.763060
2324.663452	541649.539655	38.768077
2326.986618	542666.436524	38.773095
2329.161978	543704.566299	38.778112
2331.589940	544709.275550	38.783130
2333.726963	545754.304206	38.788148
2336.073344	546794.341735	38.793165
2338.576829	547818.533755	38.798183
2340.714174	548854.630156	38.803200
2343.045610	549884.633143	38.808218
2345.492454	550956.075230	38.813236
2347.926856	551994.955230	38.818253
2350.039466	553048.188874	38.823271
2352.313146	554138.265259	38.828288
2354.478507	555190.923016	38.833306
2356.887772	556247.731566	38.838324
2359.320479	557340.239342	38.843341
2361.652029	558406.139920	38.848359
2363.822396	559488.113618	38.853376
2366.027997	560573.762730	38.858394
2368.380926	561684.773050	38.863412
2370.531032	562782.611279	38.868429
2373.336826	563884.470178	38.873447
2375.351400	564999.427676	38.878464
2377.810204	566100.706146	38.883482
2380.191566	567203.863405	38.888500
2382.104897	568339.496063	38.893517
2385.185202	569461.178703	38.898535
2387.504843	570594.538198	38.903552
2389.932985	571723.512643	38.908570
2392.198818	572844.432554	38.913588
2394.432828	573983.480884	38.918605
2397.103088	575109.556407	38.923623
2399.356704	576256.328242	38.928640
2401.886603	577398.584553	38.933658
2404.256474	578529.071993	38.938676
2406.935873	579685.396717	38.943693
2409.685919	580813.056353	38.948711
2411.921885	581949.276796	38.953728
2414.292022	583096.506621	38.958746
2417.106523	584227.055448	38.963764
2419.243204	585378.475012	38.968781
2421.676089	586524.522423	38.973799
2424.199102	587686.141776	38.978816
2426.926643	588820.542668	38.983834
2429.325618	589964.516961	38.988852
2431.730073	591117.254565	38.993869
2434.152051	592241.659867	38.998887
2436.236526	593383.155702	39.003904
2438.976434	594545.682357	39.008922
2441.231396	595697.953369	39.013940
2443.348914	596866.518844	39.018957
2445.862516	598025.184409	39.023975
2448.244102	599194.678036	39.028992
2450.906347	600343.222141	39.034010
2453.273495	601493.905681	39.039028
2455.370121	602654.285405	39.044045
2458.088066	603797.321541	39.049063
2460.476983	604922.374352	39.054080
2462.642708	606052.861088	39.059098
2465.422106	607183.786099	39.064116
2467.333496	608314.692333	39.069133
2469.864080	609454.192895	39.074151
2472.426627	610577.710001	39.079168
2474.919074	611736.654664	39.084186
2477.114864	612892.577178	39.089204
2479.137384	614056.564015	39.094221
2481.584706	615195.598384	39.099239
2484.401729	616361.965513	39.104256
2486.799693	617542.783090	39.109274
2489.102479	618715.289335	39.114292
2491.299549	619899.489011	39.119309
2494.153063	621093.302378	39.124327
2496.340296	622284.146112	39.129344
2498.500996	623501.506786	39.134362
2501.326763	624706.726460	39.139380
2503.222059	625919.661669	39.144397
2505.966027	627125.675022	39.149415
2508.360155	628358.990817	39.154432
2510.580790	629574.608457	39.159450
2513.402568	630820.809009	39.164468
2515.758620	632077.429157	39.169485
2518.078050	633322.770000	39.174503
2520.807149	634569.993905	39.179520
2522.968338	635835.287665	39.184538
2525.587580	637110.587439	39.189556
2528.419374	638395.280521	39.194573
2530.744417	639644.512816	39.199591
2533.262731	640917.616552	39.204608
2535.828849	642201.583097	39.209626
2538.404935	643490.127744	39.214644
2540.907984	644786.953323	39.219661
2543.480588	646088.241801	39.224679
2546.178566	647361.065987	39.229696
2548.583845	648665.294216	39.234714
2551.245271	649962.281992	39.239732
2553.713532	651271.149381	39.244749
2556.759617	652577.258706	39.249767
2559.268695	653897.490517	39.254784
2561.828024	655203.685637	39.259802
2564.833184	656500.567114	39.264820
2567.237384	657807.391671	39.269837
2570.045925	659112.731163	39.274855
2572.752763	660420.553873	39.279872
2575.351582	661737.831255	39.284890
2577.994687	663045.910921	39.289908
2580.761305	664333.082913	39.294925
2583.616049	665636.297826	39.299943
2586.434055	666941.035228	39.304960
2588.984121	668246.684997	39.309978
2591.498343	669545.196498	39.314996
2594.155991	670856.443767	39.320013
2596.724802	672166.032724	39.325031
2599.790427	673464.366610	39.330048
2602.478615	674769.646470	39.335066
2605.429977	676030.147713	39.340084
2607.795624	677322.098317	39.345101
2610.336508	678626.220062	39.350119
2613.064322	679933.558316	39.355136
2615.569241	681230.163683	39.360154
2618.071074	682534.936211	39.365172
2620.824434	683820.056288	39.370189
2622.942245	685101.077726	39.375207
2625.907524	686409.496631	39.380224
2628.255878	687691.408978	39.385242
2630.908093	688953.277896	39.390260
2633.650317	690211.530738	39.395277
2636.486725	691463.089874	39.400295
2638.750324	692732.835691	39.405312
2641.251783	694002.214075	39.410330
2643.532572	695281.224458	39.415348
2645.770446	696565.069812	39.420365
2648.150743	697835.213334	39.425383
2650.649956	699118.051491	39.430400
2652.728484	700431.818056	39.435418
2655.394348	701743.407763	39.440436
2657.545038	703042.442459	39.445453
2660.417685	704388.108793	39.450471
2662.808454	705727.947293	39.455488
2665.045106	707077.466258	39.460506
2667.730829	708425.858790	39.465524
2669.847202	709786.519575	39.470541
2672.547804	711154.843632	39.475559
2675.160052	712547.280155	39.480576
2677.510075	713944.187576	39.485594
2680.427709	715353.743353	39.490612
2682.631066	716752.837500	39.495629
2685.633120	718166.762386	39.500647
2688.095787	719595.433279	39.505664
2690.678845	721034.626737	39.510682
2693.440848	722488.976518	39.515700
2696.130310	723929.533541	39.520717
2698.729735	725372.427071	39.525735
2701.323403	726819.766983	39.530752
2703.775544	728292.185035	39.535770
2706.415690	729761.837432	39.540788
2709.099843	731274.801226	39.545805
2712.103793	732735.261626	39.550823
2714.626156	734217.075465	39.555840
2717.591418	735720.176492	39.560858
2720.213741	737226.115721	39.565876
2722.992838	738723.651160	39.570893
2725.947450	740235.784212	39.575911
2728.836748	741726.076537	39.580928
2731.738030	743232.370031	39.585946
2734.388657	744738.270920	39.590964
2737.312141	746256.219531	39.595981
2740.256645	747773.724295	39.600999
2743.228311	749282.944407	39.606016
2745.996561	750785.991830	39.611034
2749.007967	752283.386861	39.616052
2751.874367	753791.800668	39.621069
2754.870550	755296.943345	39.626087
2757.780244	756811.657327	39.631104
2760.370508	758310.465856	39.636122
2763.374848	759808.469779	39.641140
2766.262910	761327.611631	39.646157
2769.512117	762818.042798	39.651175
2772.437060	764313.007253	39.656192
2775.144387	765797.626644	39.661210
2777.775365	767279.014718	39.666228
2780.694747	768786.962115	39.671245
2783.531560	770284.244972	39.676263
2786.249950	771767.777690	39.681280
2789.412874	773269.665604	39.686298
2792.085435	774749.562111	39.691316
2794.875835	776239.458908	39.696333
2797.744409	777743.677631	39.701351
2800.648897	779220.032870	39.706368
2803.131775	780723.407717	39.711386
2805.907415	782208.212752	39.716404
2808.952650	783687.516412	39.721421
2811.173322	785187.064846	39.726439
2813.868105	786640.944284	39.731456
2816.590974	788099.086109	39.736474
2819.313634	789565.757517	39.741492
2821.843425	791037.993371	39.746509
2824.338366	792513.655458	39.751527
2827.174546	793973.272310	39.756544
2829.745445	795432.827365	39.761562
2832.216356	796904.636765	39.766580
2835.165985	798407.451788	39.771597
2838.009649	799932.729960	39.776615
2840.491715	801425.571592	39.781632
2843.175747	802950.410808	39.786650
2845.855933	804457.984510	39.791668
2848.980376	805989.323169	39.796685
2851.521324	807546.339841	39.801703
2854.132760	809069.984403	39.806720
2856.674614	810618.038505	39.811738
2859.797965	812180.063919	39.816756
2862.881456	813742.909396	39.821773
2865.491264	815297.362174	39.826791
2868.450070	816877.383932	39.831808
2871.294527	818484.594261	39.836826
2874.219238	820057.134211	39.841844
2877.439516	821630.133667	39.846861
2879.834606	823244.033039	39.851879
2882.986753	824825.265684	39.856896
2885.788360	826426.760138	39.861914
2888.844058	828051.667642	39.866932
2891.910357	829666.811360	39.871949
2894.459837	831289.439425	39.876967
2897.787914	832898.818179	39.881984
2900.428892	834519.846168	39.887002
2903.452589	836127.986658	39.892020
2906.727473	837780.234920	39.897037
2909.099476	839415.414336	39.902055
2912.045401	841047.308250	39.907072
2915.038483	842685.783220	39.912090
2917.913831	844335.918174	39.917108
2920.550504	845969.616776	39.922125
2923.112880	847648.796163	39.927143
2925.899941	849318.451464	39.932160
2928.478577	850992.361475	39.937178
2931.741870	852650.847257	39.942196
2934.619848	854347.707029	39.947213
2937.466077	856059.352573	39.952231
2940.325041	857740.625902	39.957248
2943.203441	859431.045094	39.962266
2946.301165	861118.829134	39.967284
2949.187441	862824.028982	39.972301
2952.154467	864558.312395	39.977319
2955.132766	866263.795251	39.982336
2957.856849	867977.271149	39.987354
2961.028387	869684.084153	39.992372
2964.341723	871408.210552	39.997389
2967.211528	873151.472816	40.002407
2970.139901	874858.403303	40.007424
2973.479209	876573.970018	40.012442
2976.314888	878286.028446	40.017460
2979.235588	879985.488733	40.022477
2982.228229	881709.875098	40.027495
2985.316056	883432.096752	40.032512
2988.126245	885166.225866	40.037530
2991.508590	886893.273531	40.042548
2994.406596	888625.006322	40.047565
2997.416861	890347.225122	40.052583
3001.149613	892058.774329	40.057600
3004.287222	893773.964954	40.062618
3006.968148	895475.407524	40.067636
3010.121533	897153.316901	40.072653
3013.008814	898814.870643	40.077671
3016.496733	900452.325409	40.082688
3019.077339	902137.819145	40.087706
3021.754543	903798.715661	40.092724
3024.975054	905450.463024	40.097741
3027.494766	907126.384247	40.102759
3030.236078	908802.728648	40.107776
3032.845461	910483.015340	40.112794
3035.667812	912177.472044	40.117812
3038.603580	913890.426455	40.122829
3041.139132	915595.514446	40.127847
3044.116294	917332.090727	40.132864
3046.576042	919088.083418	40.137882
3049.290247	920833.099716	40.142900
3052.819224	922575.022490	40.147917
3055.565861	924341.174682	40.152935
3058.389079	926117.000727	40.157952
3061.144821	927886.978346	40.162970
3063.608622	929703.295163	40.167988
3066.684477	931501.262439	40.173005
3069.325910	933326.666341	40.178023
3072.046585	935162.921015	40.183040
3075.733941	937008.717783	40.188058
3078.743094	938870.439293	40.193076
3081.888152	940717.799642	40.198093
3084.744469	942582.246374	40.203111
3088.030867	944448.441377	40.208128
3091.289779	946324.099928	40.213146
3094.150796	948198.571767	40.218164
3097.612657	950070.927143	40.223181
3100.589033	951982.484068	40.228199
3103.648780	953867.647505	40.233216
3106.665865	955756.318777	40.238234
3109.796453	957717.109162	40.243252
3113.501008	959648.201868	40.248269
3116.420570	961606.250535	40.253287
3119.518208	963556.958953	40.258304
3123.038959	965517.879697	40.263322
3126.039392	967493.942611	40.268340
3129.174783	969470.475846	40.273357
3132.091480	971429.675303	40.278375
3135.025252	973396.301361	40.283392
3138.494735	975369.382292	40.288410
3141.692338	977349.141039	40.293428
3145.144789	979326.906017	40.298445
3148.115718	981316.830057	40.303463
3151.411595	983280.488975	40.308480
3154.652577	985271.230666	40.313498
3157.490995	987258.813189	40.318516
3160.952739	989252.897078	40.323533
3163.892209	991244.715018	40.328551
3166.998200	993238.335978	40.333568
3170.247127	995221.708824	40.338586
3172.971223	997228.085368	40.343604
3176.277884	999235.501668	40.348621
3178.934143	1001247.362761	40.353639
3182.348288	1003264.595795	40.358656
3185.332527	1005296.897856	40.363674
3188.053595	1007341.702685	40.368692
3191.202290	1009371.638384	40.373709
3194.251788	1011421.600167	40.378727
3197.248512	1013454.742429	40.383744
3200.405884	1015489.545126	40.388762
3203.304865	1017563.734308	40.393780
3206.494153	1019610.980468	40.398797
3209.472066	1021674.831384	40.403815
3212.685237	1023719.703437	40.408832
3216.063006	1025766.798772	40.413850
3218.656010	1027805.640508	40.418868
3222.379066	1029824.039617	40.423885
3224.767099	1031837.004506	40.428903
3228.233209	1033864.414153	40.433920
3231.684771	1035889.641557	40.438938
3234.552801	1037937.668442	40.443956
3238.078895	1039985.315393	40.448973
3240.866869	1042037.149175	40.453991
3244.351370	1044085.027025	40.459008
3247.650350	1046166.564764	40.464026
3250.521129	1048230.349796	40.469044
3254.292860	1050290.618792	40.474061
3257.740456	1052366.144609	40.479079
3261.128193	1054438.496593	40.484096
3264.359683	1056500.771309	40.489114
3267.499356	1058586.795856	40.494132
3271.020676	1060668.125412	40.499149
3274.331835	1062757.921404	40.504167
3276.955350	1064865.274935	40.509184
3280.015460	1066972.228191	40.514202
3283.008826	1069104.952737	40.519220
3286.336958	1071225.958348	40.524237
3289.365594	1073378.778421	40.529255
3292.330067	1075510.164294	40.534272
3295.530333	1077654.183576	40.539290
3299.074755	1079830.905388	40.544308
3301.928523	1082007.446629	40.549325
3304.956986	1084196.768209	40.554343
3308.203991	1086401.140914	40.559360
3311.692695	1088597.221119	40.564378
3314.580647	1090792.225971	40.569396
3318.217987	1092998.156865	40.574413
3320.998133	1095236.359852	40.579431
3324.281978	1097476.894598	40.584448
3328.170371	1099714.494279	40.589466
3331.096470	1101962.194572	40.594484
3334.476218	1104194.684690	40.599501
3337.685443	1106453.904015	40.604519
3340.848097	1108715.801832	40.609536
3344.275688	1110992.885719	40.614554
3347.004514	1113258.940105	40.619572
3350.625539	1115505.727241	40.624589
3354.173862	1117793.506136	40.629607
3357.283108	1120081.805604	40.634624
3361.297766	1122370.022203	40.639642
3364.182753	1124667.603467	40.644660
3367.855546	1126962.927610	40.649677
3371.078442	1129237.987519	40.654695
3374.476473	1131528.260349	40.659712
3377.951734	1133830.992613	40.664730
3381.076160	1136154.478763	40.669748
3384.594389	1138435.787450	40.674765
3388.231137	1140744.206438	40.679783
3391.309435	1143056.347309	40.684800
3395.333912	1145346.706374	40.689818
3398.535255	1147667.874840	40.694836
3401.620951	1149974.530573	40.699853
3405.299933	1152296.135099	40.704871
3408.413824	1154583.863185	40.709888
3411.892277	1156879.689608	40.714906
3415.223434	1159211.887914	40.719924
3418.600785	1161536.820247	40.724941
3422.278779	1163847.196556	40.729959
3425.254216	1166166.371414	40.734976
3429.290765	1168461.652756	40.739994
3432.239976	1170778.221056	40.745012
3435.569726	1173083.987619	40.750016
3438.936213	1175341.948838	40.755021
3441.900531	1177535.204465	40.760026
3445.236787	1179631.870881	40.765031
3448.606189	1181683.057017	40.770036
3451.810969	1183659.765692	40.775040
3455.451094	1185567.344950	40.780045
3458.311914	1187391.868523	40.785050
3461.408818	1189125.076610	40.790055
3463.830496	1190768.056199	40.795060
3466.643641	1192328.327937	40.800064
3469.144306	1193821.111500	40.805069
3471.436728	1195260.627877	40.810074
3474.315374	1196592.244679	40.815079
3476.337953	1197869.970719	40.820084
3478.366853	1199074.467175	40.825088
3480.903155	1200203.263431	40.830093
3482.605572	1201293.492435	40.835098
3484.616952	1202283.565374	40.840103
3486.413484	1203219.851179	40.845108
3488.181728	1204083.692950	40.850112
3489.840057	1204913.476813	40.855117
3491.185344	1205706.534889	40.860122
3493.293907	1206413.325242	40.865127
3494.476605	1207068.827720	40.870132
3495.886833	1207699.852053	40.875136
3497.331337	1208256.419477	40.880141
3498.367090	1208778.433085	40.885146
3499.906064	1209253.016612	40.890151
3501.005420	1209693.074064	40.895156
3502.018007	1210082.263482	40.900160
3503.450298	1210453.845405	40.905165
3504.292163	1210790.295153	40.910170
3505.312284	1211057.322315	40.915175
3506.280309	1211325.841926	40.920180
3507.050179	1211534.469946	40.925184
3507.917829	1211711.621537	40.930189
3508.531878	1211883.473338	40.935194
3509.446095	1212049.560286	40.940199
3510.227313	1212158.662464	40.945204
3510.815899	1212229.887243	40.950208
3511.695740	1212280.097501	40.955213
3512.254209	1212321.468609	40.960218
3513.151949	1212340.320676	40.965223
3513.439100	1212347.012272	40.970228
3514.040235	1212322.110508	40.975232
3514.698832	1212266.686737	40.980237
3514.874296	1212198.799828	40.985242
3515.412297	1212111.383651	40.990247
3515.771828	1212028.675427	40.995252
3516.434855	1211924.387256	41.000256
3516.864437	1211784.565445	41.005261
3517.102701	1211648.328427	41.010266
3517.425797	1211499.904434	41.015271
3517.626706	1211332.024632	41.020276
3518.139757	1211154.632607	41.025280
3518.534159	1210961.900230	41.030285
3518.766405	1210768.438309	41.035290
3519.134939	1210553.131349	41.040295
3519.237463	1210336.267400	41.045300
3519.355045	1210112.275444	41.050304
3519.788839	1209863.781465	41.055309
3519.954534	1209611.011902	41.060314
3520.317921	1209364.940091	41.065319
3520.256770	1209118.270795	41.070324
3520.326731	1208838.319050	41.075328
3520.690879	1208547.625790	41.080333
3520.843054	1208266.317941	41.085338
3521.302236	1207975.763930	41.090343
3521.269007	1207691.363771	41.095348
3521.387455	1207372.914880	41.100352
3521.569988	1207067.833588	41.105357
3521.566544	1206764.451322	41.110362
3522.163068	1206449.801646	41.115367
3521.963396	1206134.888961	41.120372
3521.901281	1205792.288413	41.125376
3522.288069	1205464.024114	41.130381
3522.183542	1205148.754047	41.135386
3522.610464	1204802.820174	41.140391
3522.462358	1204463.050751	41.145396
3522.526939	1204123.598787	41.150400
3522.702656	1203763.480654	41.155405
3522.298870	1203412.714805	41.160410
3522.679462	1203065.077581	41.165415
3522.848805	1202698.603580	41.170420
3522.778244	1202356.056343	41.175424
3523.116193	1201978.906344	41.180429
3522.957213	1201616.723348	41.185434
3523.212270	1201238.688570	41.190439
3523.273569	1200879.700305	41.195444
3523.247491	1200508.974944	41.200448
3523.261007	1200145.909429	41.205453
3523.051104	1199776.568820	41.210458
3523.249296	1199380.110913	41.215463
3523.055390	1198993.070961	41.220468
3523.311383	1198621.787789	41.225472
3523.388667	1198237.274030	41.230477
3523.267772	1197865.435269	41.235482
3523.502817	1197471.640101	41.240487
3523.343828	1197094.119908	41.245492
3523.153979	1196699.303062	41.250496
3523.380968	1196308.236723	41.255501
3523.254927	1195928.184581	41.260506
3523.675540	1195514.021780	41.265511
3523.610401	1195117.842511	41.270516
3523.185431	1194738.409255	41.275520
3523.721659	1194358.883701	41.280525
3523.403628	1193948.473772	41.285530
3523.844025	1193537.342656	41.290535
3523.621159	1193152.686789	41.295540
3523.722983	1192748.970335	41.300544
3523.523091	1192347.808928	41.305549
3523.553710	1191958.512243	41.310554
3523.875340	1191542.355534	41.315559
3523.313466	1191143.885489	41.320564
3523.507451	1190752.497391	41.325568
3523.570714	1190323.220534	41.330573
3523.591630	1189928.038633	41.335578
3523.737131	1189531.677872	41.340583
3523.659858	1189133.631087	41.345588
3523.676157	1188710.151212	41.350592
3524.021227	1188293.447004	41.355597
3523.350827	1187883.929588	41.360602
3523.701007	1187470.919964	41.365607
3524.023602	1187063.431260	41.370612
3523.666260	1186649.532076	41.375616
3523.402296	1186245.461897	41.380621
3523.586323	1185842.039037	41.385626
3523.746218	1185431.061876	41.390631
3523.709345	1184995.337918	41.395636
3523.459180	1184591.606936	41.400640
3523.587045	1184183.735581	41.405645
3523.421333	1183772.962898	41.410650
3523.411098	1183346.884049	41.415655
3523.361925	1182934.049130	41.420660
3523.333461	1182519.577591	41.425664
3523.718316	1182116.773144	41.430669
3523.564107	1181701.974583	41.435674
3523.793715	1181272.955483	41.440679
3523.565358	1180872.792032	41.445684
3523.647088	1180428.943074	41.450688
3523.878986	1180015.735578	41.455693
3523.555333	1179597.217795	41.460698
3523.372498	1179184.295061	41.465703
3523.693705	1178775.966841	41.470708
3523.282584	1178340.310821	41.475712
3523.540984	1177919.300920	41.480717
3523.284770	1177502.205116	41.485722
3523.271573	1177092.386340	41.490727
3523.091202	1176686.521084	41.495732
3523.092404	1176262.403641	41.500736
3523.198511	1175830.316535	41.505741
3523.096300	1175418.118342	41.510746
3523.188557	1175005.384118	41.515751
3523.383264	1174602.122826	41.520756
3523.125215	1174186.835823	41.525760
3523.258452	1173765.604844	41.530765
3522.818171	1173351.601446	41.535770
3523.135479	1172920.747087	41.540775
3523.159228	1172510.184323	41.545780
3523.017594	1172066.224453	41.550784
3523.267774	1171656.689153	41.555789
3522.833733	1171261.668835	41.560794
3523.135599	1170838.852860	41.565799
3522.720587	1170412.063314	41.570804
3522.880264	1170001.752551	41.575808
3522.951344	1169595.293423	41.580813
3523.066440	1169172.467640	41.585818
3522.866109	1168741.636597	41.590823
3522.786558	1168341.523109	41.595828
3522.696673	1167924.388194	41.600832
3522.679460	1167487.665023	41.605837
3522.664718	1167074.320740	41.610842
3522.756432	1166664.703278	41.615847
3522.743849	1166265.080807	41.620852
3522.664343	1165851.178359	41.625856
3522.776157	1165428.428007	41.630861
3522.231040	1165014.158238	41.635866
3522.434238	1164594.442503	41.640871
3522.444516	1164192.863217	41.645876
3522.504047	1163780.380101	41.650880
3522.664289	1163365.296817	41.655885
3522.125299	1162954.170003	41.660890
3522.487142	1162526.419532	41.665895
3522.170660	1162116.702364	41.670900
3521.828143	1161720.945663	41.675904
3522.201853	1161327.498696	41.680909
3522.318573	1160910.715826	41.685914
3522.145655	1160503.401228	41.690919
3522.498828	1160081.597634	41.695924
3522.041113	1159652.234974	41.700928
3522.385293	1159249.938273	41.705933
3521.731039	1158853.354609	41.710938
3521.833513	1158431.365126	41.715943
3521.910842	1158022.965622	41.720948
3521.987080	1157618.507275	41.725952
3521.917878	1157213.190380	41.730957
3521.921191	1156815.966155	41.735962
3522.031281	1156405.638083	41.740967
3521.719732	1155990.427290	41.745972
3521.761332	1155584.209579	41.750976
3521.846395	1155164.420847	41.755981
3521.476503	1154775.526236	41.760986
3521.411432	1154362.323009	41.765991
3521.740550	1153954.417732	41.770996
3521.578834	1153568.049914	41.776000
3521.711705	1153161.440778	41.781005
3521.260977	1152761.713041	41.786010
3521.523829	1152354.546814	41.791015
3521.438101	1151956.307449	41.796020
3521.181200	1151544.903167	41.801024
3521.423964	1151124.387451	41.806029
3521.113179	1150726.660444	41.811034
3521.184776	1150327.609089	41.816039
3521.169871	1149931.857223	41.821044
3521.133804	1149524.711044	41.826048
3521.439754	1149138.509697	41.831053
3521.308374	1148765.332588	41.836058
3521.339954	1148350.125791	41.841063
3521.330297	1147934.987884	41.846068
3520.918652	1147533.246121	41.851072
3520.844396	1147139.853381	41.856077
3520.915084	1146757.212843	41.861082
3521.129823	1146344.851256	41.866087
3520.984676	1145938.299476	41.871092
3520.632700	1145554.314239	41.876096
3521.016152	1145149.036764	41.881101
3520.643984	1144766.893895	41.886106
3520.821360	1144381.408788	41.891111
3520.701636	1143987.314661	41.896116
3520.400899	1143588.763463	41.901120
3520.857594	1143183.607825	41.906125
3520.575650	1142801.023480	41.911130
3520.809169	1142409.219840	41.916135
3520.850949	1142019.411030	41.921140
3520.551197	1141618.719028	41.926144
3520.626921	1141218.978575	41.931149
3520.727259	1140815.598063	41.936154
3520.220077	1140433.164340	41.941159
3520.444014	1140043.464774	41.946164
3520.184552	1139661.788708	41.951168
3520.351055	1139264.353509	41.956173
3520.142367	1138875.018960	41.961178
3520.300125	1138500.309935	41.966183
3520.409561	1138111.246644	41.971188
3520.104073	1137732.002566	41.976192
3520.316513	1137345.999395	41.981197
3519.992530	1136954.263963	41.986202
3520.063462	1136568.322494	41.991207
3520.266311	1136188.029641	41.996212
3519.881278	1135791.754712	42.001216
3520.265673	1135400.072854	42.006221
3520.009419	1135016.162172	42.011226
3520.144413	1134626.934238	42.016231
3520.027747	1134260.901185	42.021236
3520.092805	1133869.159066	42.026240
3519.954424	1133487.018770	42.031245
3519.726987	1133094.412532	42.036250
3519.919409	1132715.868442	42.041255
3520.133095	1132343.661729	42.046260
3519.919730	1131948.687578	42.051264
3519.999305	1131560.765060	42.056269
3519.792423	1131170.674993	42.061274
3519.759099	1130784.235472	42.066279
3520.008412	1130392.682277	42.071284
3519.544910	1130017.952421	42.076288
3519.921403	1129629.745192	42.081293
3519.604474	1129246.949332	42.086298
3519.863605	1128869.927540	42.091303
3519.683814	1128499.894446	42.096308
3519.546351	1128124.216763	42.101312
3519.930032	1127742.433949	42.106317
3519.684846	1127370.525856	42.111322
3519.680428	1126975.909404	42.116327
3519.398015	1126605.190851	42.121332
3519.784366	1126224.916420	42.126336
3519.577120	1125815.784537	42.131341
3519.417797	1125451.341143	42.136346
3519.346031	1125083.622607	42.141351
3519.574488	1124693.938274	42.146356
3519.212363	1124325.073165	42.151360
3519.300278	1123947.065231	42.156365
3519.035893	1123563.091053	42.161370
3519.160036	1123178.549253	42.166375
3519.118842	1122801.433573	42.171380
3518.915820	1122441.457322	42.176384
3519.330404	1122051.073440	42.181389
3519.103412	1121686.574693	42.186394
3519.168595	1121315.241027	42.191399
3519.284815	1120939.110904	42.196404
3518.675293	1120579.171446	42.201408
3519.006922	1120201.429949	42.206413
3518.849268	1119821.074945	42.211418
3519.053538	1119438.632584	42.216423
3518.571308	1119073.045035	42.221428
3518.659444	1118685.232371	42.226432
3518.773650	1118330.453709	42.231437
3518.554515	1117983.139699	42.236442
3518.382770	1117609.110110	42.241447
3518.681316	1117234.119149	42.246452
3518.655838	1116879.267386	42.251456
3518.624468	1116503.612426	42.256461
3518.538751	1116131.562669	42.261466
3518.424903	1115776.652464	42.266471
3518.384176	1115430.859702	42.271476
3518.240998	1115067.135765	42.276480
3518.456933	1114681.396009	42.281485
3518.094838	1114348.459541	42.286490
3518.153648	1113978.620684	42.291495
3518.131796	1113619.260957	42.296500
3518.126956	1113254.056065	42.301504
3518.306069	1112874.773890	42.306509
3518.103808	1112540.458876	42.311514
3518.188021	1112196.821988	42.316519
3518.130384	1111831.242826	42.321524
3517.916563	1111459.558016	42.326528
3518.264350	1111088.041261	42.331533
3517.898759	1110747.343785	42.336538
3517.800634	1110393.124633	42.341543
3517.723153	1110041.932794	42.346548
3517.370856	1109699.067020	42.351552
3517.829805	1109332.278340	42.356557
3517.510885	1108973.802174	42.361562
3517.740144	1108635.832119	42.366567
3517.729391	1108302.462933	42.371572
3517.693825	1107954.087440	42.376576
3517.934355	1107571.270161	42.381581
3517.347941	1107242.704292	42.386586
3517.279667	1106890.636787	42.391591
3517.715861	1106549.827825	42.396596
3517.240659	1106191.287545	42.401600
3517.915803	1105839.315412	42.406605
3517.604571	1105498.276495	42.411610
3517.578691	1105159.079509	42.416615
3517.450554	1104809.178448	42.421620
3517.213583	1104449.718775	42.426624
3517.477763	1104098.369432	42.431629
3517.199489	1103764.572306	42.436634
3516.936837	1103421.482967	42.441639
3517.136440	1103069.312777	42.446644
3517.165917	1102728.902599	42.451648
3517.244107	1102388.845224	42.456653
3517.103286	1102040.200211	42.461658
3517.168990	1101686.719303	42.466663
3517.089935	1101355.894711	42.471668
3517.217675	1101002.836783	42.476672
3517.269935	1100670.705798	42.481677
3516.879605	1100362.625623	42.486682
3516.625133	1100004.211168	42.491687
3517.148431	1099656.545892	42.496692
3516.903351	1099317.878332	42.501696
3516.812452	1098976.582003	42.506701
3516.746291	1098639.946471	42.511706
3517.036095	1098302.370528	42.516711
3516.734931	1097972.236133	42.521716
3516.740070	1097637.343851	42.526720
3516.911817	1097295.037199	42.531725
3516.656834	1096961.580900	42.536730
3516.516425	1096611.341721	42.541735
3516.460573	1096277.714805	42.546740
3516.481983	1095961.948385	42.551744
3516.855193	1095631.942861	42.556749
3516.797640	1095287.824532	42.561754
3516.724562	1094967.230644	42.566759
3516.665663	1094626.133088	42.571764
3516.425467	1094276.812145	42.576768
3516.545087	1093926.260722	42.581773
3516.477849	1093611.520557	42.586778
3516.606039	1093299.601996	42.591783
3516.621986	1092957.812680	42.596788
3516.470177	1092625.508453	42.601792
3516.600794	1092266.134838	42.606797
3516.797917	1091961.500990	42.611802
3516.326223	1091620.569533	42.616807
3516.469351	1091300.393469	42.621812
3516.123220	1090968.498572	42.626816
3516.244933	1090622.617827	42.631821
3516.094440	1090296.492357	42.636826
3516.263583	1089981.981544	42.641831
3516.173846	1089647.760385	42.646836
3516.031310	1089316.114108	42.651840
3515.910830	1088996.132962	42.656845
3516.072320	1088672.637107	42.661850
3515.994038	1088322.043528	42.666855
3516.037225	1088015.105434	42.671860
3515.509774	1087714.569043	42.676864
3515.721733	1087389.742662	42.681869
3515.380162	1087044.093668	42.686874
3515.758770	1086735.302837	42.691879
3515.960657	1086433.904554	42.696884
3515.714170	1086121.251690	42.701888
3515.857121	1085775.538123	42.706893
3515.504160	1085470.343101	42.711898
3515.701618	1085142.988078	42.716903
3515.423502	1084815.212268	42.721908
3515.218674	1084523.075970	42.726912
3515.627373	1084203.972140	42.731917
3515.701387	1083886.918671	42.736922
3515.440190	1083566.832921	42.741927
3515.250376	1083253.910055	42.746932
3515.014225	1082973.301181	42.751936
3515.383166	1082653.345715	42.756941
3515.294804	1082345.150098	42.761946
3515.238209	1082031.943241	42.766951
3515.248295	1081706.235222	42.771956
3514.802842	1081419.344685	42.776960
3515.011815	1081123.215998	42.781965
3515.062355	1080788.810981	42.786970
3515.148174	1080490.461232	42.791975
3515.177661	1080175.214297	42.796980
3514.864310	1079895.611263	42.801985
3514.844374	1079575.539221	42.806989
3514.889162	1079269.451254	42.811994
3515.122764	1078966.386644	42.816999
3515.237051	1078649.405790	42.822004
3514.891478	1078354.274067	42.827009
3515.002940	1078048.106633	42.832013
3514.789291	1077753.016682	42.837018
3514.706571	1077446.079402	42.842023
3515.103274	1077126.851325	42.847028
3514.657771	1076833.190167	42.852033
3514.781185	1076520.021261	42.857037
3514.871601	1076227.775794	42.862042
3514.842150	1075925.065920	42.867047
3514.950483	1075626.254511	42.872052
3514.889204	1075323.420516	42.877057
3515.075436	1075014.381301	42.882061
3514.570741	1074719.271476	42.887066
3514.464394	1074423.311569	42.892071
3514.669153	1074116.908496	42.897076
3514.536636	1073813.234018	42.902081
3514.479585	1073516.736553	42.907085
3514.447597	1073216.567508	42.912090
3514.034433	1072932.396432	42.917095
3514.491083	1072624.907397	42.922100
3514.240053	1072329.626864	42.927105
3514.613568	1072034.419762	42.932109
3513.857897	1071756.010615	42.937114
3514.121927	1071483.282659	42.942119
3514.108886	1071185.113742	42.947124
3514.046834	1070889.339921	42.952129
3514.283126	1070586.771527	42.957133
3514.109045	1070298.386674	42.962138
3514.069284	1070003.138192	42.967143
3514.178456	1069724.291029	42.972148
3513.838262	1069462.523163	42.977153
3514.250036	1069154.750611	42.982157
3514.104441	1068869.266853	42.987162
3513.799845	1068579.370578	42.992167
3514.165637	1068287.040350	42.997172
3513.871667	1068014.039333	43.002177
3513.980228	1067709.986705	43.007181
3514.223311	1067418.688476	43.012186
3514.052165	1067122.921801	43.017191
3514.256790	1066842.854278	43.022196
3514.198670	1066552.233088	43.027201
3514.149201	1066259.286023	43.032205
3513.998751	1065984.428598	43.037210
3513.962209	1065683.655195	43.042215
3514.665220	1065385.726541	43.047220
3513.933359	1065094.465583	43.052225
3514.012276	1064810.177150	43.057229
3513.808261	1064537.758306	43.062234
3513.506902	1064250.808807	43.067239
3513.742190	1063950.088224	43.072244
3513.685012	1063678.950150	43.077249
3513.726363	1063391.803108	43.082253
3513.576148	1063119.208834	43.087258
3513.661679	1062843.192735	43.092263
3513.831541	1062537.399584	43.097268
3513.464030	1062280.781394	43.102273
3513.648135	1061998.159561	43.107277
3513.589849	1061722.496066	43.112282
3513.354107	1061440.011008	43.117287
3513.858948	1061157.485776	43.122292
3513.512533	1060886.546588	43.127297
3513.470779	1060599.556404	43.132301
3513.559118	1060333.333895	43.137306
3513.097539	1060057.557124	43.142311
3513.439012	1059769.401041	43.147316
3513.183093	1059503.773082	43.152321
3513.300043	1059215.432347	43.157325
3513.222387	1058951.482417	43.162330
3512.962330	1058681.672915	43.167335
3512.732785	1058418.878613	43.172340
3512.924094	1058138.080779	43.177345
3513.050590	1057850.630600	43.182349
3512.930848	1057598.185775	43.187354
3512.785690	1057324.147293	43.192359
3513.139023	1057043.170654	43.197364
3512.747255	1056791.311925	43.202369
3512.858539	1056522.010191	43.207373
3512.774008	1056258.028804	43.212378
3512.789653	1056007.223805	43.217383
3512.799307	1055738.382516	43.222388
3512.373430	1055456.875060	43.227393
3512.757786	1055185.727936	43.232397
3512.901242	1054951.628341	43.237402
3512.654189	1054689.237631	43.242407
3512.564106	1054406.560751	43.247412
3512.319455	1054139.226159	43.252417
3512.468032	1053887.242288	43.257421
3512.540384	1053607.679874	43.262426
3512.352791	1053366.913787	43.267431
3512.550763	1053130.895743	43.272436
3512.321988	1052876.420461	43.277441
3512.422635	1052585.999824	43.282445
3512.365001	1052333.207445	43.287450
3511.940589	1052095.222133	43.292455
3511.888449	1051842.599328	43.297460
3511.950031	1051580.010076	43.302465
3512.463938	1051350.037901	43.307469
3512.383467	1051091.018287	43.312474
3512.665273	1050840.996068	43.317479
3512.305706	1050578.911056	43.322484
3512.226151	1050314.258769	43.327489
3512.493464	1050053.203484	43.332493
3512.334378	1049806.487946	43.337498
3511.851736	1049540.128043	43.342503
3512.195809	1049289.832479	43.347508
3512.182407	1049055.605467	43.352513
3512.491214	1048804.521684	43.357517
3512.352037	1048542.014341	43.362522
3512.182582	1048279.982167	43.367527
3512.280934	1048024.071397	43.372532
3512.042321	1047763.281053	43.377537
3512.243383	1047514.087208	43.382541
3511.966532	1047289.675831	43.387546
3511.855914	1047043.022242	43.392551
3512.180728	1046782.382567	43.397556
3511.904285	1046544.616832	43.402561
3511.965585	1046279.845039	43.407565
3511.704059	1046015.886290	43.412570
3511.660746	1045784.519387	43.417575
3512.337475	1045556.404287	43.422580
3511.844659	1045306.452893	43.427585
3512.194767	1045033.944445	43.432589
3512.163570	1044783.893469	43.437594
3511.837837	1044539.481983	43.442599
3511.746320	1044290.674385	43.447604
3511.613964	1044051.812060	43.452609
3511.314266	1043797.027473	43.457613
3511.487229	1043550.558214	43.462618
3511.552861	1043302.743124	43.467623
3511.673841	1043079.834815	43.472628
3511.540874	1042840.920476	43.477633
3511.438765	1042599.671793	43.482637
3511.645230	1042353.723638	43.487642
3511.433082	1042118.173241	43.492647
3511.668340	1041881.186251	43.497652
3511.552652	1041646.469694	43.502657
3511.268900	1041403.459431	43.507661
3511.618220	1041165.456679	43.512666
3511.186710	1040922.256406	43.517671
3511.537585	1040685.489342	43.522676
3511.344021	1040460.981224	43.527681
3511.312138	1040195.644476	43.532685
3511.269967	1039969.738257	43.537690
3510.986647	1039745.022663	43.542695
3511.306833	1039515.558051	43.547700
3511.116107	1039281.527390	43.552705
3511.383186	1039035.519085	43.557709
3511.570821	1038801.115838	43.562714
3511.243301	1038572.492529	43.567719
3511.743919	1038331.926227	43.572724
3511.437029	1038101.442892	43.577729
3511.161976	1037839.708485	43.582733
3511.253206	1037600.145054	43.587738
3511.071458	1037375.703847	43.592743
3511.341918	1037137.638437	43.597748
3510.840489	1036897.175174	43.602753
3510.999200	1036671.972456	43.607757
3511.073837	1036451.997964	43.612762
3510.821717	1036226.071032	43.617767
3510.848497	1036007.731371	43.622772
3510.740774	1035781.859376	43.627777
3510.815486	1035539.888202	43.632781
3511.030329	1035322.071179	43.637786
3510.529528	1035111.039571	43.642791
3510.833564	1034876.645422	43.647796
3510.733002	1034644.823884	43.652801
3510.924608	1034427.266009	43.657805
3510.942810	1034195.793302	43.662810
3510.375087	1033972.826847	43.667815
3510.747943	1033742.922087	43.672820
3510.383177	1033526.001352	43.677825
3510.740483	1033288.628218	43.682829
3510.850445	1033080.129117	43.687834
3510.438608	1032881.290690	43.692839
3510.771468	1032633.924032	43.697844
3510.448383	1032403.497914	43.702849
3510.424265	1032180.951073	43.707853
3510.303817	1031986.776221	43.712858
3510.430223	1031768.060467	43.717863
3510.364237	1031529.907741	43.722868
3510.280762	1031325.441228	43.727873
3510.258885	1031123.668141	43.732877
3510.211849	1030912.983807	43.737882
3509.759273	1030696.838953	43.742887
3510.097055	1030475.326476	43.747892
3510.057988	1030264.325852	43.752897
3510.198868	1030043.603396	43.757901
3510.258583	1029850.486672	43.762906
3510.294646	1029637.028839	43.767911
3510.249355	1029412.922403	43.772916
3510.089384	1029206.453838	43.777921
3510.252179	1028997.599832	43.782925
3510.389500	1028786.514346	43.787930
3510.000475	1028573.376489	43.792935
3510.197234	1028355.193572	43.797940
3509.970925	1028153.540610	43.802945
3510.335269	1027937.832560	43.807949
3510.033643	1027735.983184	43.812954
3509.907434	1027529.640880	43.817959
3510.072063	1027303.962024	43.822964
3509.870563	1027095.096952	43.827969
3509.908380	1026902.172650	43.832973
3509.996603	1026688.399835	43.837978
3509.948339	1026476.967033	43.842983
3509.826473	1026270.577565	43.847988
3509.587251	1026067.591706	43.852993
3509.935356	1025852.968885	43.857997
3509.920094	1025661.755028	43.863002
3509.429510	1025464.022257	43.868007
3509.880344	1025256.725703	43.873012
3509.434619	1025044.916558	43.878017
3509.792585	1024846.052909	43.883021
3509.626902	1024653.472336	43.888026
3509.665823	1024444.177903	43.893031
3509.915912	1024234.356157	43.898036
3510.159478	1024028.211597	43.903041
3509.873426	1023831.841681	43.908045
3509.786225	1023631.069228	43.913050
3509.689129	1023429.612512	43.918055
3509.924849	1023217.718970	43.923060
3509.998310	1023012.922525	43.928065
3509.700979	1022802.943415	43.933069
3509.716360	1022599.595949	43.938074
3509.450420	1022407.051626	43.943079
3509.619879	1022199.203429	43.948084
3509.463740	1022015.355594	43.953089
3509.345801	1021805.309560	43.958093
3509.656876	1021595.184998	43.963098
3509.263804	1021398.650445	43.968103
3509.502405	1021194.148331	43.973108
3509.335380	1021000.666455	43.978113
3509.481065	1020817.408626	43.983117
3509.713902	1020635.682542	43.988122
3509.364709	1020426.884040	43.993127
3509.629401	1020203.424778	43.998132
3509.473507	1020013.981571	44.003137
3509.471024	1019834.111593	44.008141
3509.528819	1019630.843538	44.013146
3509.220908	1019431.024267	44.018151
3509.297319	1019244.621661	44.023156
3509.470366	1019042.768770	44.028161
3509.169219	1018819.638722	44.033165
3509.469871	1018650.451943	44.038170
3509.130702	1018463.703704	44.043175
3509.443433	1018260.538140	44.048180
3509.260089	1018086.561782	44.053185
3509.302000	1017894.297083	44.058189
3509.209214	1017683.704399	44.063194
3508.852327	1017500.615184	44.068199
3509.075677	1017310.727116	44.073204
3509.134644	1017126.586594	44.078209
3508.976789	1016939.466611	44.083213
3509.111442	1016739.284520	44.088218
3508.939900	1016568.656748	44.093223
3509.226592	1016376.202719	44.098228
3509.088067	1016174.492251	44.103233
3509.017253	1015999.850249	44.108237
3509.036780	1015801.983795	44.113242
3509.057780	1015600.906096	44.118247
3509.041461	1015405.750185	44.123252
3509.088880	1015248.251251	44.128257
3508.859369	1015043.310946	44.133261
3509.254639	1014872.829659	44.138266
3509.004801	1014695.749027	44.143271
3508.965917	1014475.996256	44.148276
3508.818541	1014282.473859	44.153281
3508.473334	1014103.253754	44.158285
3508.930492	1013925.546845	44.163290
3508.530867	1013754.968379	44.168295
3508.987474	1013573.851122	44.173300
3508.926120	1013392.716221	44.178305
3508.969158	1013201.359284	44.183309
3508.982117	1013015.731870	44.188314
3508.448347	1012827.954165	44.193319
3508.526439	1012630.840801	44.198324
3508.491602	1012472.889167	44.203329
3508.714306	1012278.751194	44.208333
3508.827473	1012114.061805	44.213338
3508.162057	1011938.614448	44.218343
3508.378857	1011762.239050	44.223348
3508.650477	1011569.428799	44.228353
3508.807565	1011392.080036	44.233357
3508.934355	1011224.058788	44.238362
3508.877109	1011051.398654	44.243367
3508.456263	1010847.988995	44.248372
3508.687593	1010671.479899	44.253377
3508.547357	1010477.922729	44.258381
3508.893199	1010291.859191	44.263386
3507.895727	1010114.951955	44.268391
3508.450038	1009941.573979	44.273396
3508.596146	1009768.452295	44.278401
3508.244999	1009596.281959	44.283405
3508.106155	1009440.789548	44.288410
3508.415155	1009271.027711	44.293415
3508.469417	1009084.875181	44.298420
3508.552904	1008925.638177	44.303425
3508.260930	1008724.560843	44.308429
3508.399230	1008545.959124	44.313434
3507.992685	1008394.370508	44.318439
3508.248963	1008200.961522	44.323444
3508.255466	1008042.101144	44.328449
3508.378193	1007892.647992	44.333453
3508.802332	1007717.278626	44.338458
3508.403896	1007520.745643	44.343463
3508.508143	1007330.054343	44.348468
3508.324149	1007172.756631	44.353473
3508.293562	1006998.898413	44.358477
3508.616393	1006830.713995	44.363482
3508.439415	1006664.746308	44.368487
3508.292690	1006482.333641	44.373492
3508.078518	1006300.217947	44.378497
3508.147343	1006133.805161	44.383501
3508.378057	1005952.674797	44.388506
3508.282989	1005812.831054	44.393511
3508.471763	1005614.578819	44.398516
3508.570134	1005448.140973	44.403521
3508.116506	1005260.778777	44.408525
3508.213695	1005089.272493	44.413530
3508.239948	1004945.885469	44.418535
3508.086441	1004784.527904	44.423540
3507.953009	1004609.737581	44.428545
3507.899988	1004425.783848	44.433549
3507.874870	1004270.422112	44.438554
3507.535004	1004087.380198	44.443559
3507.868928	1003928.836641	44.448564
3507.881947	1003772.190120	44.453569
3507.948052	1003598.795116	44.458573
3507.963354	1003459.264150	44.463578
3507.604692	1003305.682267	44.468583
3507.605426	1003123.234168	44.473588
3507.794483	1002964.395523	44.478593
3507.631783	1002806.194232	44.483597
3507.868524	1002641.402595	44.488602
3507.837512	1002491.053349	44.493607
3507.684509	1002310.648046	44.498612
3507.919111	1002152.363036	44.503617
3507.400814	1001996.046811	44.508621
3507.770246	1001839.872040	44.513626
3507.594532	1001697.798531	44.518631
3507.705588	1001516.059095	44.523636
3507.584839	1001351.775467	44.528641
3507.481182	1001201.111904	44.533645
3507.857546	1001029.533869	44.538650
3507.771822	1000882.071188	44.543655
3507.724213	1000724.863555	44.548660
3507.565122	1000553.359289	44.553665
3507.332959	1000397.535884	44.558669
3507.410865	1000240.878267	44.563674
3507.256171	1000082.307440	44.568679
3507.343674	999930.702355	44.573684
3507.454215	999792.525727	44.578689
3507.453976	999648.132497	44.583693
3507.422102	999479.495766	44.588698
3507.379147	999325.364356	44.593703
3507.567736	999166.906112	44.598708
3507.442669	999026.802116	44.603713
3507.510816	998870.887251	44.608717
3507.533705	998705.821547	44.613722
3507.747568	998552.503270	44.618727
3507.377807	998380.480986	44.623732
3507.297966	998247.946601	44.628737
3507.189895	998100.707366	44.633741
3507.360418	997924.881314	44.638746
3507.688487	997779.120241	44.643751
3507.801721	997620.533793	44.648756
3507.522462	997484.800156	44.653761
3507.217468	997321.111800	44.658765
3507.463933	997152.359992	44.663770
3507.167233	997013.987892	44.668775
3507.340196	996856.344363	44.673780
3507.176906	996710.149682	44.678785
3507.480072	996569.135077	44.683789
3507.512157	996401.565290	44.688794
3507.042488	996259.111508	44.693799
3507.402474	996086.217443	44.698804
3507.141007	995957.166847	44.703809
3506.867693	995817.982275	44.708813
3507.098276	995666.434460	44.713818
3507.083876	995538.600311	44.718823
3507.165760	995390.285053	44.723828
3507.289741	995228.804225	44.728833
3507.149522	995094.354681	44.733837
3507.148308	994938.050793	44.738842
3506.851834	994785.299450	44.743847
3506.551833	994639.853550	44.748852
3506.702135	994505.439661	44.753857
3506.657829	994364.135157	44.758861
3506.877344	994214.986874	44.763866
3506.729592	994085.095299	44.768871
3506.994151	993932.033671	44.773876
3507.019513	993793.919855	44.778881
3506.802993	993654.575414	44.783885
3506.877307	993501.728471	44.788890
3506.856170	993373.651750	44.793895
3507.086718	993224.768085	44.798900
3506.615134	993078.043240	44.803905
3506.570460	992941.869842	44.808909
3506.819646	992795.116459	44.813914
3506.409356	992675.374277	44.818919
3506.653544	992541.093433	44.823924
3506.662963	992418.644511	44.828929
3506.827481	992256.487571	44.833933
3506.963705	992123.482069	44.838938
3506.677374	991977.575757	44.843943
3506.840438	991844.071806	44.848948
3506.430187	991711.536679	44.853953
3506.504865	991574.140822	44.858957
3506.572652	991438.692938	44.863962
3506.482560	991307.655788	44.868967
3506.942455	991159.070302	44.873972
3506.761800	991024.823635	44.878977
3506.438825	990893.620273	44.883981
3506.962202	990750.084545	44.888986
3506.277911	990610.840035	44.893991
3506.607965	990469.572080	44.898996
3506.418928	990346.721136	44.904001
3506.584742	990194.355367	44.909005
3506.798587	990078.942025	44.914010
3506.281668	989947.358653	44.919015
3506.321545	989797.051192	44.924020
3506.277286	989681.477230	44.929025
3506.251192	989555.363608	44.934029
3506.435994	989427.456697	44.939034
3506.259090	989305.166520	44.944039
3506.538640	989164.654861	44.949044
3506.465554	989028.099785	44.954049
3506.464154	988895.919440	44.959053
3506.699391	988754.624555	44.964058
3506.335736	988616.156380	44.969063
3506.555195	988489.295809	44.974068
3506.274344	988375.587913	44.979073
3505.917237	988255.939005	44.984077
3506.237104	988112.467880	44.989082
3506.161199	987995.206298	44.994087
3506.436856	987873.981643	44.999092
3506.210334	987744.250870	45.004097
3506.097032	987609.522251	45.009101
3506.361215	987483.802808	45.014106
3506.257903	987359.409632	45.019111
3506.371499	987215.949913	45.024116
3506.192718	987105.322406	45.029121
3506.034468	986981.222768	45.034125
3506.119677	986861.178951	45.039130
3506.210478	986735.276384	45.044135
3506.222977	986595.428469	45.049140
3506.271230	986486.313003	45.054145
3506.117095	986349.121492	45.059149
3506.336205	986224.748039	45.064154
3506.130727	986103.955378	45.069159
3505.970615	985961.777967	45.074164
3506.371637	985838.049331	45.079169
3505.826563	985727.260195	45.084173
3506.068009	985610.190080	45.089178
3506.005993	985481.356765	45.094183
3506.235042	985343.882732	45.099188
3505.986941	985232.156547	45.104193
3505.779355	985097.579303	45.109197
3506.089196	984977.458830	45.114202
3505.765066	984889.166835	45.119207
3505.966534	984733.720536	45.124212
3505.856637	984624.204997	45.129217
3505.936918	984511.629614	45.134221
3505.967865	984401.305589	45.139226
3505.806569	984275.292605	45.144231
3505.707708	984143.506226	45.149236
3506.098712	984020.911437	45.154241
3505.973277	983898.691988	45.159245
3505.998851	983772.344209	45.164250
3505.852805	983666.331246	45.169255
3505.758700	983536.482883	45.174260
3505.668433	983425.964682	45.179265
3505.591538	983318.371544	45.184269
3506.026707	983200.048321	45.189274
3505.969785	983097.134870	45.194279
3505.571980	982978.748955	45.199284
3505.722641	982847.379813	45.204289
3505.788381	982728.424084	45.209293
3505.771181	982620.514992	45.214298
3505.463282	982519.390322	45.219303
3505.334107	982391.084250	45.224308
3505.572516	982264.570385	45.229313
3505.770704	982159.156388	45.234317
3505.608166	982030.457044	45.239322
3505.651656	981935.417291	45.244327
3505.788396	981819.263378	45.249332
3505.750293	981708.410321	45.254337
3505.509893	981606.574644	45.259341
3505.303315	981482.558660	45.264346
3505.516063	981377.616239	45.269351
3505.434666	981257.579633	45.274356
3505.419828	981157.847811	45.279361
3505.687291	981043.805649	45.284365
3505.976421	980931.222960	45.289370
3505.674845	980810.724795	45.294375
3505.591659	980709.726444	45.299380
3505.652961	980587.698435	45.304385
3505.468218	980467.173781	45.309389
3505.686909	980363.677204	45.314394
3505.997084	980262.313067	45.319399
3505.749159	980149.021841	45.324404
3505.651570	980016.944604	45.329409
3505.491750	979919.071409	45.334413
3505.632221	979789.099208	45.339418
3505.398868	979671.692417	45.344423
3505.452752	979564.495571	45.349428
3505.588520	979454.058705	45.354433
3505.554023	979354.396368	45.359437
3505.473006	979238.030442	45.364442
3505.522013	979136.591658	45.369447
3505.573536	979017.951902	45.374452
3505.469494	978896.305913	45.379457
3505.315992	978791.474076	45.384461
3505.166762	978688.007779	45.389466
3505.208640	978572.878516	45.394471
3505.327836	978471.220918	45.399476
3505.348542	978364.007041	45.404481
3505.479111	978269.282918	45.409485
3505.293889	978164.835755	45.414490
3505.207582	978060.077182	45.419495
3505.302256	977944.633374	45.424500
3505.384978	977821.174466	45.429505
3504.938399	977722.822207	45.434509
3505.106888	977612.442149	45.439514
3505.082701	977516.753618	45.444519
3504.870520	977424.417870	45.449524
3504.950588	977323.919310	45.454529
3505.398773	977211.334968	45.459533
3505.357542	977101.957125	45.464538
3505.012278	977017.945745	45.469543
3505.168067	976898.071812	45.474548
3505.343501	976798.721407	45.479553
3505.025462	976713.625735	45.484557
3505.092264	976599.919077	45.489562
3504.857602	976499.848939	45.494567
3505.017749	976410.270643	45.499572
3504.947897	976310.952178	45.504577
3504.975259	976196.266336	45.509581
3504.981197	976098.691541	45.514586
3504.907739	976007.776645	45.519591
3505.038306	975908.809283	45.524596
3505.067227	975812.985758	45.529601
3504.871690	975707.517696	45.534605
3505.212622	975599.710421	45.539610
3505.274570	975505.440772	45.544615
3504.907387	975408.600141	45.549620
3505.145385	975324.174487	45.554625
3505.174776	975219.149303	45.559629
3504.846506	975089.147573	45.564634
3504.742886	975002.133180	45.569639
3504.768741	974892.995465	45.574644
3505.116712	974806.197091	45.579649
3504.840344	974725.563445	45.584653
3504.983723	974620.899699	45.589658
3504.981035	974541.294133	45.594663
3504.740696	974449.501823	45.599668
3504.975047	974333.375425	45.604673
3504.916321	974235.486150	45.609677
3505.248616	974137.824211	45.614682
3504.974198	974039.869318	45.619687
3504.697650	973944.162662	45.624692
3504.720473	973850.067845	45.629697
3504.487297	973755.915839	45.634701
3504.746068	973652.095694	45.639706
3504.571430	973552.844487	45.644711
3504.584782	973487.795866	45.649716
3504.803103	973388.770541	45.654721
3504.652146	973300.662132	45.659725
3504.721006	973217.798412	45.664730
3504.624672	973109.625066	45.669735
3504.748288	973033.597148	45.674740
3505.037667	972944.139044	45.679745
3504.887497	972839.491135	45.684749
3504.625607	972729.087886	45.689754
3504.714906	972670.767599	45.694759
3504.648159	972570.992483	45.699764
3504.888855	972461.577441	45.704769
3504.710568	972363.284568	45.709773
3504.799878	972264.456757	45.714778
3504.502569	972188.780481	45.719783
3504.596637	972106.581419	45.724788
3504.849583	971999.503671	45.729793
3504.899461	971910.460265	45.734797
3504.804251	971812.339953	45.739802
3504.574445	971724.513848	45.744807
3504.685135	971641.620476	45.749812
3504.859921	971550.104751	45.754817
3504.295604	971444.031880	45.759821
3504.755555	971267.237036	45.764826
3504.368453	971061.806639	45.769831
3504.510611	970782.984387	45.774836
3504.665092	970481.245967	45.779841
3504.569298	970075.103443	45.784845
3504.443336	969608.544978	45.789850
3504.327458	969082.626018	45.794855
3504.298464	968476.660733	45.799860
3504.866692	967825.592107	45.804865
3504.319791	967095.903348	45.809869
3504.051980	966292.427602	45.814874
3503.900804	965416.728016	45.819879
3503.950021	964460.430583	45.824884
3503.813823	963432.083584	45.829889
3503.590949	962348.293039	45.834893
3503.709546	961183.373003	45.839898
3503.580579	959924.331458	45.844903
3503.225791	958578.066245	45.849908
3503.277271	957165.796650	45.854913
3502.823810	955675.183352	45.859917
3502.737526	954136.651616	45.864922
3502.375618	952530.531947	45.869927
3502.214923	950820.694830	45.874932
3502.455242	949011.984601	45.879937
3502.143395	947135.777867	45.884941
3501.986136	945174.256307	45.889946
3501.238968	943127.352852	45.894951
3501.186783	940995.237866	45.899956
3501.040082	938772.568517	45.904961
3500.425207	936464.574440	45.909965
3500.442160	934068.758524	45.914970
3500.194819	931606.193510	45.919975
3499.621549	929039.029995	45.924980
3499.721820	926390.037858	45.929985
3499.116335	923656.925343	45.934989
3498.967133	920833.894202	45.939994
3498.441143	917910.548496	45.944999
3497.945156	914919.915270	45.950004
3497.858981	911826.832606	45.955009
3497.272355	908672.290833	45.960013
3496.908001	905405.303874	45.965018
3496.359772	902054.924064	45.970023
3496.060519	898611.377416	45.975028
3495.515252	895112.982966	45.980033
3494.878300	891513.957267	45.985037
3494.765927	887808.314187	45.990042
3494.215277	884046.990874	45.995047
3493.500924	880189.715239	46.000052
3493.057708	876243.233000	46.005057
3492.399485	872217.176817	46.010061
3492.382497	868107.479479	46.015066
3491.706485	863895.057339	46.020071
3490.566482	859599.440115	46.025076
3490.332549	855211.882757	46.030081
3489.205182	850747.519612	46.035085
3488.760281	846195.427868	46.040090
3488.079745	841584.969320	46.045095
3487.534790	836869.709921	46.050100
3487.061153	832057.917669	46.055105
3486.082459	827159.338323	46.060109
3485.551327	822170.529039	46.065114
3485.034976	817124.843297	46.070119
3484.076299	811962.978055	46.075124
3483.397672	806708.820695	46.080129
3482.423141	801402.546641	46.085133
3481.770011	796004.298391	46.090138
3481.050896	790494.710765	46.095143
3479.890742	784899.418017	46.100148
3479.358931	779222.826955	46.105153
3478.359754	773454.443588	46.110157
3477.735390	767602.209878	46.115162
3476.824082	761685.693056	46.120167
3476.052084	755664.636636	46.125172
3475.030150	749537.296639	46.130177
3473.624236	743340.416622	46.135181
3472.728128	737052.523251	46.140186
3471.789508	730673.620258	46.145191
3470.742523	724229.118717	46.150196
3469.814006	717697.325651	46.155201
3468.822199	711051.883172	46.160205
3467.844736	704337.627115	46.165210
3467.092603	697510.190028	46.170215
3465.895833	690598.284078	46.175220
3464.586335	683604.646844	46.180225
3463.563018	676560.581506	46.185229
3462.446278	669407.172736	46.190234
3461.401661	662156.484434	46.195239
3459.731404	654828.308561	46.200244
3458.554693	647405.552088	46.205249
3457.326697	639905.875794	46.210253
3456.103743	632320.910764	46.215258
3454.912529	624664.672010	46.220263
3453.678811	616924.760931	46.225268
3452.190233	609091.331067	46.230273
3450.561669	601182.428792	46.235277
3449.554782	593164.346105	46.240282
3448.059421	585084.951912	46.245287
3446.735633	576924.940110	46.250292
3445.328936	568672.461016	46.255297
3443.535716	560333.432412	46.260301
3442.243513	551924.838959	46.265306
3440.355782	543451.733896	46.270311
3439.116131	534871.361633	46.275316
3437.347759	526231.916673	46.280321
3435.580686	517501.294904	46.285325
3434.076792	508682.961783	46.290330
3432.464785	499793.856759	46.295335
3430.432072	490840.932742	46.300340
3429.079818	481804.702356	46.305345
3426.939199	472688.360096	46.310349
3425.290089	463485.741643	46.315354
3423.151907	454231.464647	46.320359
3420.848204	444886.852641	46.325364
3419.187107	435475.104911	46.330369
3417.009213	426019.614263	46.335373
3414.803697	416491.182881	46.340378
3412.839951	406868.690837	46.345383
3410.487932	397169.466648	46.350388
3408.434345	387430.253021	46.355393
3406.045541	377648.499265	46.360397
3403.934257	367790.829799	46.365402
3401.500809	357844.036754	46.370407
3398.879160	347846.570292	46.375412
3396.182948	337807.379083	46.380417
3393.450079	327698.197221	46.385421
3391.227207	317541.224184	46.390426
3388.471131	307362.532790	46.395431
3385.549961	297118.004617	46.400436
3382.475670	286817.710847	46.405441
3379.376239	276451.417784	46.410445
3376.834262	266081.561564	46.415450
3373.506580	255671.910673	46.420455
3370.314958	245219.354745	46.425460
3367.001222	234704.228263	46.430465
3363.243765	224155.704069	46.435469
3360.129507	213562.466496	46.440474
3356.491833	202988.122950	46.445479
3352.806158	192378.674148	46.450484
3349.052848	181757.706467	46.455489
3344.819028	171132.674954	46.460493
3340.174852	160497.634254	46.465498
3336.038125	149856.170469	46.470503
3331.233398	139239.019640	46.475508
3326.803284	128632.345489	46.480513
3321.505602	118044.285556	46.485517
3315.950128	107467.714696	46.490522
3309.708912	96936.175424	46.495527
3302.567537	86468.354957	46.500532
3294.577324	76063.366337	46.505537
3284.970899	65801.743322	46.510541
3270.721709	55771.841112	46.515546
3246.489916	46178.760068	46.520551
3219.808718	36947.242741	46.525556
3191.636619	28159.111596	46.530561
3155.893866	20097.059825	46.535565
3109.970443	12980.374336	46.540570
3059.696562	6756.321342	46.545575
3003.072178	1677.982285	46.550580
2851.282838	385.207344	46.555585
2723.807127	408.416099	46.560589
2686.299843	381.637411	46.565594
2717.033316	352.588534	46.570599
2779.640952	344.969012	46.575604
2842.395259	346.002714	46.580609
2886.213431	363.079958	46.585613
2908.095463	345.472367	46.590618
2911.365887	325.663736	46.595623
2904.746071	330.315246	46.600628
2894.301867	334.870660	46.605633
2884.749831	325.275463	46.610637
2877.792421	314.796093	46.615642
2874.547776	334.534325	46.620647
2872.102035	331.000006	46.625652
2871.329773	321.047629	46.630657
2870.038798	302.172510	46.635661
2868.245438	301.557935	46.640666
2865.702476	313.410667	46.645671
2862.628037	311.748014	46.650676
2860.040663	302.764030	46.655681
2856.600314	313.400271	46.660685
2853.336313	329.274004	46.665690
2850.439346	307.991794	46.670695
2846.951593	293.882407	46.675700
2844.285888	299.533101	46.680705
2840.998805	325.638806	46.685709
2838.162411	314.070295	46.690714
2835.112160	305.057863	46.695719
2831.763480	297.334672	46.700724
2828.613110	300.861326	46.705729
2825.513224	315.875881	46.710733
2821.598097	311.838624	46.715738
2818.629990	286.289332	46.720743
2815.122377	303.399048	46.725748
2812.142881	311.880073	46.730753
2808.268342	314.223152	46.735757
2805.785207	293.311857	46.740762
2802.473043	286.745654	46.745767
2799.120312	297.138786	46.750772
2795.671387	298.109222	46.755777
2791.931741	299.019764	46.760781
2789.036329	289.449716	46.765786
2785.568125	293.801709	46.770791
2782.203249	289.159105	46.775796
2778.616304	268.264109	46.780801
2775.638087	278.752247	46.785805
2771.793294	300.869207	46.790810
2768.517616	288.557139	46.795815
2765.116675	277.894349	46.800820
2762.003553	275.211272	46.805825
2758.363815	293.867709	46.810829
2755.218346	292.455646	46.815834
2751.781824	277.459701	46.820839
2747.985039	287.871699	46.825844
2744.685884	286.384159	46.830849
2741.589199	285.968712	46.835853
2737.749472	275.512940	46.840858
2734.678792	279.959124	46.845863
2731.316243	281.019026	46.850868
2727.692531	259.991141	46.855873
2724.216366	288.313169	46.860877
2721.144028	289.281625	46.865882
2717.821468	275.256177	46.870887
2713.888903	275.879528	46.875892
2710.613289	275.360418	46.880897
2706.703170	285.557907	46.885901
2703.729343	275.864504	46.890906
2700.833450	259.341154	46.895911
2697.045798	267.504308	46.900916
2693.208821	269.403830	46.905921
2689.816809	274.001855	46.910925
2686.522657	255.365990	46.915930
2683.018852	271.847173	46.920935
2679.779890	253.471529	46.925940
2676.145185	262.347077	46.930945
2671.986220	281.354402	46.935949
2668.789005	265.639561	46.940954
2666.201105	258.863756	46.945959
2661.940475	277.330865	46.950964
2658.275052	270.074037	46.955969
2654.780678	287.395074	46.960973
2651.151946	277.900139	46.965978
2648.692643	259.980751	46.970983
2645.034279	263.318754	46.975988
2642.063334	274.464806	46.980993
2638.461787	276.483375	46.985997
2634.451350	258.096453	46.991002
2631.037549	236.629888	46.996007
2627.674362	254.322483	47.001012
2624.312652	256.017695	47.006017
2620.203091	256.487677	47.011021
2617.183222	270.019062	47.016026
2614.035553	275.654283	47.021031
2609.941893	264.519040	47.026036
2606.684983	236.686200	47.031041
2603.355898	253.175372	47.036045
2599.604975	261.449209	47.041050
2596.600408	243.384496	47.046055
2593.006549	243.571764	47.051060
2589.271856	257.208584	47.056065
2585.887823	260.637120	47.061069
2582.112606	259.921859	47.066074
2579.019846	252.651252	47.071079
2575.726387	250.072871	47.076084
2571.993419	237.561027	47.081089
2568.237399	245.352030	47.086093
2564.915336	245.100487	47.091098
2561.494404	247.607413	47.096103
2558.160641	252.469730	47.101108
2554.654594	232.624647	47.106113
2551.390966	255.697177	47.111117
2547.750569	262.277935	47.116122
2544.504342	242.810053	47.121127
2540.397444	239.530755	47.126132
2537.099000	242.130249	47.131137
2533.758268	258.206445	47.136141
2530.077332	242.201834	47.141146
2526.993718	232.246582	47.146151
2523.138171	228.898325	47.151156
2519.832544	240.086158	47.156161
2516.027675	254.975981	47.161165
2512.785574	249.922425	47.166170
2509.394186	228.529401	47.171175
2505.414012	252.167666	47.176180
2502.460303	242.628706	47.181185
2498.882678	238.345995	47.186189
2495.127955	242.493290	47.191194
2491.882598	228.835976	47.196199
2488.243544	231.402280	47.201204
2484.982417	226.522842	47.206209
2481.320850	224.065388	47.211213
2477.802379	231.697390	47.216218
2474.579152	235.309176	47.221223
2470.702535	258.797404	47.226228
2467.576840	241.562656	47.231233
2463.788845	234.103713	47.236237
2460.473951	248.367805	47.241242
2456.806333	222.459711	47.246247
2453.338227	244.550463	47.251252
2449.991383	240.494987	47.256257
2446.440139	248.254047	47.261261
2443.042632	241.516854	47.266266
2439.875096	240.229318	47.271271
2436.337583	246.086916	47.276276
2432.823234	229.896084	47.281281
2428.834368	231.447093	47.286285
2425.368802	240.679860	47.291290
2421.945418	219.677707	47.296295
2418.331734	226.803772	47.301300
2415.287456	236.336801	47.306305
2411.239528	236.187964	47.311309
2407.952271	216.294294	47.316314
2404.764453	232.477667	47.321319
2401.131290	240.492336	47.326324
2397.586198	225.407037	47.331329
2393.941307	224.299756	47.336333
2390.504468	214.486395	47.341338
2387.001603	227.548967	47.346343
2383.383013	238.720386	47.351348
2380.590297	224.516650	47.356353
2376.777198	209.994279	47.361357
2372.945825	217.454277	47.366362
2370.009950	218.769113	47.371367
2365.820659	233.964154	47.376372
2362.807831	212.669127	47.381377
2359.055761	223.276876	47.386381
2355.501375	230.805445	47.391386
2352.244869	236.585853	47.396391
2348.944549	243.763559	47.401396
2345.314017	213.319665	47.406401
2341.573839	231.757133	47.411405
2338.391910	230.657376	47.416410
2334.684589	220.064240	47.421415
2331.031221	232.731310	47.426420
2327.606936	219.928219	47.431425
2324.284682	219.795983	47.436429
2320.819290	225.147097	47.441434
2317.253366	218.871519	47.446439
2313.504041	218.740471	47.451444
2310.228026	215.239241	47.456449
2306.516455	230.494705	47.461453
2302.670117	229.900127	47.466458
2299.602843	210.415065	47.471463
2296.135808	226.915695	47.476468
2293.137035	228.289075	47.481473
2289.751691	211.678438	47.486477
2286.044048	208.095504	47.491482
2282.572572	214.484339	47.496487
2278.452962	220.862584	47.501492
2275.212929	229.269499	47.506497
2271.506688	231.156141	47.511501
2268.195562	223.641849	47.516506
2265.092447	214.293696	47.521511
2261.157938	207.755868	47.526516
2257.781879	206.500734	47.531521
2254.039009	210.449864	47.536525
2250.612706	205.969501	47.541530
2247.456347	202.841783	47.546535
2243.388572	213.951187	47.551540
2240.520577	214.939199	47.556545
2236.932656	222.340658	47.561549
2232.841636	210.049398	47.566554
2229.965837	205.567819	47.571559
2226.292723	211.896710	47.576564
2222.865401	213.294238	47.581569
2219.437422	217.356685	47.586573
2215.878382	205.782969	47.591578
2212.124870	204.746275	47.596583
2208.422891	221.561007	47.601588
2205.303986	224.842972	47.606593
2201.986615	213.914318	47.611597
2198.280819	212.410450	47.616602
2194.744865	213.469095	47.621607
2190.618493	231.667948	47.626612
2187.354877	220.020650	47.631617
2184.419439	205.712037	47.636621
2181.034423	203.092523	47.641626
2177.655056	212.896528	47.646631
2173.868823	214.469290	47.651636
2170.439335	216.958849	47.656641
2166.730647	214.268529	47.661645
2163.351480	213.134303	47.666650
2160.081768	206.564418	47.671655
2156.034555	209.032564	47.676660
2152.957071	215.894494	47.681665
2149.150568	201.071794	47.686669
2145.480699	215.412257	47.691674
2142.367162	215.701236	47.696679
2138.807628	212.093061	47.701684
2135.469878	227.104911	47.706689
2131.922914	211.074848	47.711693
2128.355618	220.581274	47.716698
2125.091194	206.251198	47.721703
2121.340416	207.739809	47.726708
2117.375832	208.502614	47.731713
2114.157085	220.077239	47.736717
2110.641935	215.112435	47.741722
2107.562654	206.008933	47.746727
2103.722022	219.822288	47.751732
2100.191798	212.696309	47.756737
2096.685652	201.055247	47.761741
2093.166945	190.090730	47.766746
2090.031559	205.314926	47.771751
2086.239846	218.273217	47.776756
2083.257404	202.994015	47.781761
2079.448988	208.031776	47.786765
2075.551015	214.146467	47.791770
2072.327519	218.633567	47.796775
2068.531654	210.671083	47.801780
2065.026025	201.765982	47.806785
2061.530146	192.987524	47.811789
2058.302843	199.800110	47.816794
2054.914477	208.170989	47.821799
2051.296114	207.152037	47.826804
2048.044560	213.216829	47.831809
2044.535049	217.962625	47.836813
2040.817051	215.051651	47.841818
2037.524455	194.849474	47.846823
2033.603222	199.637441	47.851828
2030.236608	193.452167	47.856833
2026.871773	200.047637	47.861837
2023.329207	212.693463	47.866842
2019.905690	203.559985	47.871847
2016.277778	194.104011	47.876852
2012.749557	188.361311	47.881857
2009.231699	199.062932	47.886861
2005.403695	218.699550	47.891866
2002.088414	208.477093	47.896871
1998.692784	199.031145	47.901876
1995.421727	193.618526	47.906881
1992.022125	190.442964	47.911885
1988.094622	186.095439	47.916890
1984.932120	179.856299	47.921895
1981.581344	203.910188	47.926900
1977.878228	202.712594	47.931905
1974.526126	203.915817	47.936909
1970.757799	208.421217	47.941914
1967.051761	206.422688	47.946919
1963.183570	196.998295	47.951924
1960.524719	197.989493	47.956929
1956.879492	200.950565	47.961933
1953.345956	195.135870	47.966938
1949.943702	187.565574	47.971943
1946.229452	207.715540	47.976948
1942.744956	187.208210	47.981953
1939.176844	186.660657	47.986957
1935.645759	189.481569	47.991962
1932.362030	201.606073	47.996967
1928.687065	202.113443	48.001972
1925.143357	201.468251	48.006977
1921.919020	189.456652	48.011981
1918.401030	191.058581	48.016986
1915.083209	195.932908	48.021991
1911.309244	192.983891	48.026996
1907.750333	179.310330	48.032001
1904.203487	195.212293	48.037005
1900.519198	203.520873	48.042010
1897.368802	187.449042	48.047015
1893.546830	186.450939	48.052020
1890.199165	184.660962	48.057025
1886.810098	197.648670	48.062029
1883.355399	201.981324	48.067034
1879.745593	200.695782	48.072039
1876.332403	183.605273	48.077044
1872.755658	182.416975	48.082049
1869.212877	205.225167	48.087053
1865.560493	191.813566	48.092058
1862.723863	183.649555	48.097063
1858.744617	193.459608	48.102068
1855.237545	201.857937	48.107073
1851.530786	185.570836	48.112077
1848.178325	182.998994	48.117082
1844.916965	189.074449	48.122087
1840.687960	188.076549	48.127092
1837.444085	182.643647	48.132097
1834.222537	199.587457	48.137101
1831.009329	191.841118	48.142106
1827.552993	194.021455	48.147111
1823.631630	196.978036	48.152116
1820.167766	193.435141	48.157121
1816.545153	182.499580	48.162125
1813.027833	178.356161	48.167130
1809.841429	182.947327	48.172135
1806.573046	198.080385	48.177140
1802.818175	188.329520	48.182145
1799.262986	170.212985	48.187149
1795.481618	172.976705	48.192154
1792.484014	182.658847	48.197159
1788.625325	201.588334	48.202164
1785.287533	184.147079	48.207169
1781.847381	165.217955	48.212173
1778.206922	163.630534	48.217178
1774.643005	193.658937	48.222183
1771.073384	197.600124	48.227188
1767.583138	184.347596	48.232193
1764.176504	176.901934	48.237197
1760.335574	195.992742	48.242202
1756.945895	170.561567	48.247207
1753.318356	190.103595	48.252212
1750.360326	199.649903	48.257217
1747.076980	182.209557	48.262221
1743.215374	172.628862	48.267226
1739.900764	188.568116	48.272231
1736.098231	200.197150	48.277236
1732.158875	190.875209	48.282241
1728.843262	177.622702	48.287245
1725.625677	181.610583	48.292250
1721.922105	176.271451	48.297255
1718.738621	169.081193	48.302260
1715.433463	187.574772	48.307265
1711.723254	195.832264	48.312269
1707.884362	186.831044	48.317274
1704.810799	170.638947	48.322279
1701.210922	173.698798	48.327284
1697.901008	184.648445	48.332289
1694.471786	190.278737	48.337293
1690.267471	176.535927	48.342298
1687.307712	166.923652	48.347303
1683.807316	185.840889	48.352308
1680.050381	188.267106	48.357313
1676.691002	175.179495	48.362317
1672.922126	186.049218	48.367322
1669.671585	192.112106	48.372327
1666.166756	183.006170	48.377332
1662.705531	172.199454	48.382337
1659.205753	165.395347	48.387341
1655.472288	178.681043	48.392346
1652.142375	184.854694	48.397351
1648.380989	196.711655	48.402356
1644.932408	182.290845	48.407361
1641.556548	191.700450	48.412365
1637.876238	190.585590	48.417370
1634.957877	177.720185	48.422375
1630.825020	195.700190	48.427380
1627.516103	176.549246	48.432385
1624.038424	166.297011	48.437389
1620.565592	169.911252	48.442394
1617.079602	179.384114	48.447399
1613.460191	195.307221	48.452404
1609.971398	181.481212	48.457409
1606.868599	184.080666	48.462413
1602.893745	183.670443	48.467418
1599.566409	180.519262	48.472423
1595.759887	176.710357	48.477428
1592.666635	199.850265	48.482433
1589.160914	172.088855	48.487437
1585.450034	169.010350	48.492442
1582.257821	169.101642	48.497447
1578.746999	184.656728	48.502452
1575.142405	189.279909	48.507457
1571.717796	171.712761	48.512461
1567.849785	172.479851	48.517466
1564.511477	178.997625	48.522471
1560.845706	194.677044	48.527476
1557.516295	172.207752	48.532481
1554.229211	180.488797	48.537485
1550.288924	181.405932	48.542490
1547.051570	165.112824	48.547495
1543.632549	178.706341	48.552500
1539.966509	187.541893	48.557505
1536.773795	188.124457	48.562509
1532.636456	190.725888	48.567514
1529.376321	177.061665	48.572519
1526.049404	167.158978	48.577524
1522.565130	153.967796	48.582529
1519.161619	170.046064	48.587533
1515.306213	189.095535	48.592538
1511.990308	180.293029	48.597543
1508.423698	167.953644	48.602548
1505.255352	159.193193	48.607553
1501.786373	169.331825	48.612557
1497.913171	172.995624	48.617562
1494.353880	177.926445	48.622567
1490.796244	167.817899	48.627572
1487.357963	167.207321	48.632577
1484.003286	184.606443	48.637581
1480.449550	180.491309	48.642586
1477.018845	148.658678	48.647591
1473.382137	167.029746	48.652596
1470.063329	180.947776	48.657601
1466.683899	174.438501	48.662605
1462.788641	167.268092	48.667610
1459.586343	168.510748	48.672615
1455.720146	165.917847	48.677620
1452.410721	158.868477	48.682625
1448.832786	150.112626	48.687629
1445.194796	178.210906	48.692634
1442.092321	184.499221	48.697639
1438.772457	173.287540	48.702644
1434.896614	159.670459	48.707649
1431.348887	171.588408	48.712653
1427.579783	166.137746	48.717658
1424.430039	156.950182	48.722663
1420.909969	167.192668	48.727668
1417.459111	183.080316	48.732673
1414.043970	173.439365	48.737677
1410.726413	158.554668	48.742682
1407.140288	166.690881	48.747687
1403.129289	186.859383	48.752692
1399.403890	186.415995	48.757697
1396.019434	165.082377	48.762701
1392.692194	156.849049	48.767706
1389.648179	159.537733	48.772711
1386.305538	183.105715	48.777716
1382.442339	168.631889	48.782721
1378.740704	146.914340	48.787725
1375.240540	170.351850	48.792730
1371.864096	161.872240	48.797735
1368.101686	173.682905	48.802740
1364.946657	167.254634	48.807745
1361.534948	156.027986	48.812749
1358.080861	161.887138	48.817754
1354.627124	173.270617	48.822759
1350.678806	172.564950	48.827764
1347.231199	163.453126	48.832769
1344.020021	160.931516	48.837773
1340.281909	161.589888	48.842778
1336.672714	156.142583	48.847783
1333.401921	168.384784	48.852788
1329.502754	172.664672	48.857793
1326.422148	175.398882	48.862797
1322.587420	154.500015	48.867802
1319.710111	163.062518	48.872807
1315.785859	173.953492	48.877812
1311.997904	163.202900	48.882817
1308.828791	167.071773	48.887821
1305.290871	177.404068	48.892826
1301.959048	168.305217	48.897831
1298.392944	168.549505	48.902836
1294.747538	170.520694	48.907841
1291.331067	179.001848	48.912845
1287.636469	165.099154	48.917850
1284.022650	162.726407	48.922855
1280.925786	171.825806	48.927860
1277.396597	152.478386	48.932865
1274.169455	161.739860	48.937869
1270.162401	170.393378	48.942874
1266.776938	175.060433	48.947879
1263.577190	163.770342	48.952884
1259.503298	164.063845	48.957889
1256.014843	169.432322	48.962893
1252.742291	175.644016	48.967898
1249.802129	170.437306	48.972903
1245.755469	163.393538	48.977908
1242.110305	169.124377	48.982913
1238.813149	162.356415	48.987917
1234.948847	160.679670	48.992922
1231.754112	162.117586	48.997927
1228.209501	173.570370	49.002932
1225.114554	172.714139	49.007937
1221.510494	160.456002	49.012941
1217.867706	158.598182	49.017946
1214.274551	161.228236	49.022951
1210.614068	169.364972	49.027956
1207.001452	176.064406	49.032961
1203.832630	169.305756	49.037965
1200.208177	178.716804	49.042970
1196.738881	154.809917	49.047975
1193.383005	135.653459	49.052980
1189.684507	154.383129	49.057985
1186.421908	171.636219	49.062989
1182.196723	176.647713	49.067994
1178.891328	153.431249	49.072999
1175.648754	151.975073	49.078004
1172.317980	155.184200	49.083009
1168.903703	174.188867	49.088013
1164.923079	169.374637	49.093018
1161.683270	141.536289	49.098023
1158.434731	155.381046	49.103028
1154.584670	164.512691	49.108033
1151.434583	147.663282	49.113037
1147.489880	157.718897	49.118042
1144.155885	158.414930	49.123047
1140.852911	166.439011	49.128052
1137.117473	172.972209	49.133057
1133.762272	153.146927	49.138061
1130.211739	150.745767	49.143066
1126.489870	158.190595	49.148071
1122.596133	178.070619	49.153076
1119.310949	172.280807	49.158081
1116.608086	154.327797	49.163085
1112.882191	150.954621	49.168090
1109.727274	147.774740	49.173095
1105.798358	145.521689	49.178100
1101.779946	159.469006	49.183105
1098.299827	157.387199	49.188109
1094.752821	167.752246	49.193114
1091.885496	140.103221	49.198119
1088.063414	136.425931	49.203124
1084.400174	161.123616	49.208129
1081.243565	146.983205	49.213133
1077.531267	146.467694	49.218138
1073.963835	156.285267	49.223143
1070.865115	154.471371	49.228148
1066.990843	140.287087	49.233153
1064.013436	143.745996	49.238157
1060.035002	143.935471	49.243162
1056.630703	146.921415	49.248167
1053.019591	150.800725	49.253172
1049.489005	150.995973	49.258177
1046.132469	144.560211	49.263181
1042.484168	165.121134	49.268186
1039.439814	146.495457	49.273191
1035.843276	136.696685	49.278196
1032.009020	163.585663	49.283201
1028.305345	160.571000	49.288205
1024.616844	157.646169	49.293210
1021.434069	137.566813	49.298215
1017.976475	139.892843	49.303220
1014.552626	160.725182	49.308225
1011.242965	160.230137	49.313229
1007.898909	147.875264	49.318234
1004.214823	140.676414	49.323239
1000.527278	146.865767	49.328244
997.001577	152.492056	49.333249
993.545623	150.974526	49.338253
989.644785	166.299332	49.343258
986.465483	170.177521	49.348263
983.248896	170.910574	49.353268
979.480193	177.588830	49.358273
976.313334	155.668359	49.363277
972.480652	172.978647	49.368282
968.905794	157.774881	49.373287
965.229397	145.786833	49.378292
961.666070	156.679722	49.383297
958.555638	154.739868	49.388301
954.964656	170.658685	49.393306
951.815789	156.342363	49.398311
948.213258	147.269194	49.403316
944.068715	156.473726	49.408321
941.285198	148.765064	49.413325
937.249703	156.715050	49.418330
933.842983	161.191325	49.423335
930.374661	151.888154	49.428340
926.770038	145.851020	49.433345
923.433948	145.375477	49.438349
920.088752	146.276286	49.443354
916.537894	137.899348	49.448359
913.074546	154.960929	49.453364
909.234974	168.590462	49.458369
906.082649	148.565924	49.463373
901.973434	144.747247	49.468378
898.971177	130.875940	49.473383
895.595936	154.418697	49.478388
891.877388	152.144354	49.483393
888.671191	150.995913	49.488397
884.689566	151.526943	49.493402
881.553994	146.585398	49.498407
878.014351	148.235206	49.503412
874.766465	148.221983	49.508417
871.136847	133.497209	49.513421
867.063956	154.185994	49.518426
863.626099	152.715658	49.523431
860.322482	148.021067	49.528436
856.636487	153.394620	49.533441
853.428803	154.997418	49.538445
849.905685	151.083174	49.543450
846.553149	137.480248	49.548455
842.591480	153.345179	49.553460
839.298050	150.985278	49.558465
836.036187	141.636241	49.563469
832.327520	143.798637	49.568474
829.145939	149.998829	49.573479
824.978945	147.281669	49.578484
821.877162	138.805772	49.583489
818.760968	149.201681	49.588493
815.096202	142.987020	49.593498
811.664727	127.783786	49.598503
807.973406	139.094030	49.603508
804.047052	151.532161	49.608513
800.550522	138.516614	49.613517
797.174317	139.123703	49.618522
793.801892	135.705270	49.623527
790.496147	146.504587	49.628532
786.796950	140.596306	49.633537
783.543695	126.913605	49.638541
779.818720	118.752650	49.643546
776.335257	124.362686	49.648551
772.599571	136.995136	49.653556
769.110874	138.085444	49.658561
766.114247	137.438208	49.663565
762.344326	152.883824	49.668570
758.876504	148.313672	49.673575
755.363597	136.795858	49.678580
751.649634	136.595884	49.683585
747.918458	125.718935	49.688589
744.388495	142.144633	49.693594
741.333224	142.654654	49.698599
737.818433	146.714817	49.703604
734.554765	126.954248	49.708609
730.785507	138.903804	49.713613
727.105955	155.015670	49.718618
723.739351	153.012586	49.723623
720.397149	132.733084	49.728628
716.802242	128.331823	49.733633
713.525611	138.591986	49.738637
710.008318	143.930349	49.743642
706.383132	141.972251	49.748647
702.616376	139.834323	49.753652
698.985377	142.590050	49.758657
696.139163	146.852724	49.763661
692.539950	149.097344	49.768666
688.864705	131.538116	49.773671
685.079155	126.236147	49.778676
681.531700	148.816878	49.783681
678.578101	141.200266	49.788685
674.376966	143.430369	49.793690
671.151706	139.250311	49.798695
667.527714	134.952133	49.803700
664.157525	124.589747	49.808705
660.971859	125.289435	49.813709
657.177426	144.789476	49.818714
653.947845	149.724037	49.823719
650.560273	138.537464	49.828724
646.677991	131.402850	49.833729
643.121721	129.428771	49.838733
639.299126	138.028152	49.843738
635.965088	135.734847	49.848743
632.675205	144.349534	49.853748
629.098675	160.209450	49.858753
626.178172	135.368963	49.863757
622.308934	128.045671	49.868762
618.701260	137.103687	49.873767
615.081599	152.741370	49.878772
611.409086	143.474398	49.883777
608.264673	118.707434	49.888781
604.505492	130.917579	49.893786
601.423982	142.879771	49.898791
597.987478	158.855267	49.903796
594.161075	149.424318	49.908801
590.614346	146.163518	49.913805
586.749896	131.032641	49.918810
583.549023	123.455846	49.923815
580.368430	128.009851	49.928820
576.730613	138.413673	49.933825
573.464418	141.514944	49.938829
569.641313	148.733985	49.943834
566.132590	135.262101	49.948839
562.574974	128.869406	49.953844
558.958760	136.577990	49.958849
555.616099	128.401674	49.963853
551.952480	136.086425	49.968858
548.738168	149.852829	49.973863
545.401852	137.807028	49.978868
541.438803	124.032176	49.983873
538.366192	136.864878	49.988877
534.593259	149.793812	49.993882
530.872315	128.432883	49.998887
527.591708	127.463431	50.003892
524.034634	142.274819	50.008897
520.733140	115.504880	50.013901
516.769350	126.933840	50.018906
513.390663	134.073501	50.023911
509.951673	129.246571	50.028916
506.163106	134.622564	50.033921
503.060150	131.140717	50.038925
499.730360	141.133164	50.043930
496.385576	131.353014	50.048935
492.884228	129.306518	50.053940
489.201846	131.578891	50.058945
485.582166	134.865552	50.063949
481.799007	134.300331	50.068954
478.554853	115.056999	50.073959
475.260969	128.994093	50.078964
471.391645	132.863766	50.083969
467.876202	121.890511	50.088973
464.642571	133.044800	50.093978
460.777396	123.308248	50.098983
457.439740	132.691852	50.103988
453.672957	145.227804	50.108993
450.630248	121.847675	50.113997
447.184781	139.943516	50.119002
443.494962	132.882007	50.124007
439.818185	127.785956	50.129012
436.136489	134.265031	50.134017
433.391618	142.140079	50.139021
429.614082	143.760957	50.144026
425.930236	127.102618	50.149031
422.301016	126.538341	50.154036
418.766578	137.071250	50.159041
415.939783	131.871100	50.164045
411.972708	130.810615	50.169050
408.387755	123.952088	50.174055
405.042951	127.625453	50.179060
401.179561	149.865157	50.184065
397.864868	151.972595	50.189069
394.620522	133.834939	50.194074
391.055922	117.970278	50.199079
387.562083	126.844651	50.204084
384.162469	154.981914	50.209089
380.452572	139.760125	50.214093
376.907106	127.350461	50.219098
373.191242	126.370921	50.224103
369.928217	132.607343	50.229108
366.086438	154.976276	50.234113
362.893737	125.415143	50.239117
359.484201	132.049546	50.244122
356.129165	130.598259	50.249127
352.375950	132.186160	50.254132
348.623655	139.542371	50.259137
345.326942	131.626119	50.264141
341.947012	152.477726	50.269146
338.734338	123.635796	50.274151
335.370404	126.047607	50.279156
331.629939	129.001642	50.284161
327.624654	110.265932	50.289165
323.703943	124.750839	50.294170
320.180064	132.762809	50.299175
317.398193	135.059626	50.304180
313.969494	147.153956	50.309185
310.621100	135.074397	50.314189
306.808049	127.285401	50.319194
303.353910	120.834442	50.324199
299.697838	134.193692	50.329204
295.927038	149.592192	50.334209
293.011954	137.324059	50.339213
289.350288	130.869708	50.344218
285.853146	131.106794	50.349223
282.736902	137.500318	50.354228
279.068814	135.356210	50.359233
275.742043	116.021218	50.364237
271.813646	129.566041	50.369242
268.084360	138.159364	50.374247
264.773874	127.411916	50.379252
261.263978	157.811220	50.384257
258.107760	131.123729	50.389261
254.423959	141.600697	50.394266
250.622385	145.668138	50.399271
247.030977	128.788487	50.404276
243.562700	144.160006	50.409281
240.331190	127.340458	50.414285
236.912150	128.104361	50.419290
233.275730	130.630791	50.424295
229.705031	141.436812	50.429300
226.286268	135.071692	50.434305
222.985093	122.642786	50.439309
219.331891	140.177106	50.444314
215.849488	146.156178	50.449319
212.663190	131.644902	50.454324
208.565217	133.248417	50.459329
205.235802	123.852930	50.464333
201.860808	120.644583	50.469338
198.130509	129.098420	50.474343
194.997411	130.698477	50.479348
191.065206	154.112478	50.484353
187.827368	134.975415	50.489357
184.072015	117.292311	50.494362
180.713421	130.465930	50.499367
177.184441	133.746940	50.504372
173.693690	144.415484	50.509377
170.423284	132.942830	50.514381
166.719096	128.768200	50.519386
163.345914	139.955237	50.524391
159.633673	144.700564	50.529396
156.089342	148.257474	50.534401
152.690273	124.208850	50.539405
149.351709	129.062992	50.544410
145.987456	129.801121	50.549415
142.500156	132.378523	50.554420
138.611715	131.263786	50.559425
134.827078	146.508679	50.564429
131.305495	146.740417	50.569434
128.211004	138.683945	50.574439
124.991737	127.744443	50.579444
121.203708	134.850092	50.584449
117.728386	117.497399	50.589453
114.416769	136.560556	50.594458
110.652230	137.507589	50.599463
107.275460	130.261005	50.604468
103.513743	139.632367	50.609473
99.918473	132.062031	50.614477
96.664450	142.016550	50.619482
93.674311	143.566202	50.624487
89.771787	137.699856	50.629492
85.659216	134.618978	50.634497
82.548965	114.017936	50.639501
79.167891	129.798581	50.644506
75.538673	140.272531	50.649511
72.360317	125.406592	50.654516
68.611061	119.629371	50.659521
65.447157	133.207965	50.664525
61.967843	133.548173	50.669530
58.036218	133.282372	50.674535
54.794966	135.326620	50.679540
50.827054	157.398773	50.684545
47.398697	133.363839	50.689549
43.830932	122.657769	50.694554
40.584863	124.112817	50.699559
37.381778	132.386489	50.704564
33.561112	132.520330	50.709569
30.069111	131.045885	50.714573
26.568970	136.587029	50.719578
23.166456	124.599771	50.724583
19.860178	120.492948	50.729588
16.060909	145.964394	50.734593
12.810712	144.586326	50.739597
8.895089	129.155490	50.744602
5.335995	121.237039	50.749607
2.083763	120.063021	50.754612