Wed Jun 15 16:50:07 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.735411	114.622551	0.000000
1.901363	106.502224	0.005005
1.813163	105.040099	0.010010
1.922656	98.796084	0.015014
1.561923	99.271129	0.020019
1.493307	88.894968	0.025024
1.456695	80.802013	0.030029
1.019830	83.902082	0.035034
0.864459	66.060537	0.040038
0.660168	40.588657	0.045043
0.028968	34.448330	0.050048
0.065236	43.666339	0.055053
-0.379424	36.869079	0.060058
-0.473033	19.334330	0.065062
-0.534441	-5.154702	0.070067
-1.517893	-4.796139	0.075072
-1.378826	2.266618	0.080077
-1.460792	-7.679150	0.085082
-1.940810	-22.210951	0.090086
-2.281324	-23.618444	0.095091
-2.629165	4.279182	0.100096
-2.766750	-23.901074	0.105101
-3.391952	-26.974990	0.110106
-3.393023	-18.982238	0.115110
-3.780629	-31.420361	0.120115
-4.162861	-13.042764	0.125120
-4.248493	-15.834646	0.130125
-4.558142	-9.714776	0.135130
-4.487160	-16.051617	0.140134
-4.859213	-20.758321	0.145139
-5.277339	-22.393782	0.150144
-5.208379	-40.677015	0.155149
-5.591578	-30.727230	0.160154
-6.411721	-17.510600	0.165158
-6.990068	-15.877208	0.170163
-7.195628	-25.998152	0.175168
-6.500889	-30.944380	0.180173
-6.993948	-11.643494	0.185178
-6.958991	-28.860783	0.190182
-7.035166	-19.157638	0.195187
-7.820534	-7.527241	0.200192
-8.095741	-13.028363	0.205197
-8.774930	-13.145440	0.210202
-8.895634	-30.171870	0.215206
-9.067751	-23.265940	0.220211
-9.408776	-21.322662	0.225216
-9.043816	-29.547420	0.230221
-9.091742	-4.527930	0.235226
-9.652428	-4.411071	0.240230
-10.007377	-38.207959	0.245235
-10.506733	-25.317398	0.250240
-10.452120	-19.310997	0.255245
-10.638101	-29.394730	0.260250
-10.798117	-38.266155	0.265254
-11.325051	-27.333290	0.270259
-12.001621	-12.239881	0.275264
-12.035573	-4.560608	0.280269
-12.672595	-21.603425	0.285274
-12.607038	-29.624325	0.290278
-12.409199	-19.662636	0.295283
-12.657524	-17.345224	0.300288
-12.533126	-17.129987	0.305293
-13.218181	-20.146957	0.310298
-13.597884	-21.534558	0.315302
-13.768031	-15.049771	0.320307
-14.141933	-16.923271	0.325312
-13.937108	-26.808404	0.330317
-14.189538	-18.587871	0.335322
-15.057018	-27.463721	0.340326
-15.470758	-32.194802	0.345331
-15.659583	-12.734772	0.350336
-15.576710	-19.852283	0.355341
-15.880305	-18.722898	0.360346
-15.700655	-11.540786	0.365350
-15.801587	-11.260493	0.370355
-16.719386	-15.085971	0.375360
-16.639904	-32.713183	0.380365
-17.126339	-8.718466	0.385370
-17.142351	-7.144661	0.390374
-17.197140	-11.956277	0.395379
-18.038585	-21.299079	0.400384
-18.418529	-23.582438	0.405389
-18.518770	-3.271916	0.410394
-18.758937	-4.042566	0.415398
-18.823469	-16.442152	0.420403
-18.960015	-11.688718	0.425408
-18.651066	-29.593169	0.430413
-19.988283	-7.140048	0.435418
-20.226312	-13.062511	0.440422
-20.216661	-10.139829	0.445427
-20.470411	-20.979926	0.450432
-20.203150	-16.274977	0.455437
-20.388973	-13.170938	0.460442
-21.282380	-10.812519	0.465446
-21.680721	-14.904362	0.470451
-21.944498	-20.446432	0.475456
-21.772650	-14.864245	0.480461
-21.861029	-10.288638	0.485466
-22.148441	-8.436981	0.490470
-22.250779	-17.513958	0.495475
-23.220067	-20.222544	0.500480
-23.340393	-29.502907	0.505485
-23.566767	-15.721308	0.510490
-23.815538	-3.444679	0.515494
-23.619090	-21.088471	0.520499
-24.056226	-28.973026	0.525504
-24.170201	-15.947179	0.530509
-24.312213	-14.399606	0.535514
-24.894040	-24.641650	0.540518
-25.325511	-27.055385	0.545523
-25.527898	-21.195814	0.550528
-25.459913	-15.023333	0.555533
-25.686457	-13.111402	0.560538
-25.520341	-21.839539	0.565542
-26.239732	-34.055424	0.570547
-26.894659	-18.458365	0.575552
-26.820879	1.602536	0.580557
-27.014254	-8.743962	0.585562
-27.286684	-30.536027	0.590566
-27.703965	-28.259945	0.595571
-28.416728	-7.080645	0.600576
-28.436527	-7.430885	0.605581
-28.556315	-6.346672	0.610586
-28.741261	-18.923646	0.615590
-28.623408	-20.941841	0.620595
-28.575258	-22.074125	0.625600
-28.670792	-28.043510	0.630605
-29.506975	-17.495149	0.635610
-30.054852	-29.021046	0.640614
-30.371730	-28.478575	0.645619
-30.414642	-29.886912	0.650624
-30.181654	-28.193862	0.655629
-30.385468	-22.718674	0.660634
-31.166846	-27.825800	0.665638
-31.139272	-26.518440	0.670643
-31.609065	-14.905775	0.675648
-31.708085	-24.849992	0.680653
-32.582591	-12.086625	0.685658
-32.947330	-28.736341	0.690662
-32.664501	-32.325499	0.695667
-32.995914	-17.734916	0.700672
-32.756530	-22.226999	0.705677
-32.923381	-19.751705	0.710682
-33.357408	-24.327520	0.715686
-34.100313	-35.027481	0.720691
-34.520859	-13.729872	0.725696
-34.502087	-2.917754	0.730701
-35.122427	-24.672256	0.735706
-34.636886	-22.200904	0.740710
-34.465183	-13.546089	0.745715
-34.982845	-9.208199	0.750720
-35.914281	-24.778601	0.755725
-36.226259	-31.644707	0.760730
-36.377407	-18.474321	0.765734
-36.446406	-6.215567	0.770739
-36.651463	-10.337774	0.775744
-36.600130	-17.893385	0.780749
-36.614921	-33.810582	0.785754
-37.308846	-27.708200	0.790758
-37.538367	-4.979337	0.795763
-37.882149	-6.114817	0.800768
-38.185478	-27.356663	0.805773
-38.135119	-25.453799	0.810778
-39.059988	-10.401625	0.815782
-39.277193	-17.504070	0.820787
-39.500655	-18.318614	0.825792
-39.651349	-27.542661	0.830797
-39.981578	-8.022170	0.835802
-40.349271	-4.207716	0.840806
-39.743202	-22.191165	0.845811
-40.196786	-6.049109	0.850816
-40.043444	-9.171391	0.855821
-40.327207	-18.229529	0.860826
-41.080578	-24.198214	0.865830
-41.094958	-16.153547	0.870835
-41.396672	-15.889592	0.875840
-41.865495	-6.022018	0.880845
-42.558174	-11.353723	0.885850
-43.061713	-19.117712	0.890854
-42.823182	-24.892239	0.895859
-43.059423	-29.324262	0.900864
-42.973620	-34.515904	0.905869
-42.815315	-30.475481	0.910874
-42.886968	-12.595486	0.915878
-43.497794	-28.604866	0.920883
-44.280619	-32.385956	0.925888
-44.224716	-16.218418	0.930893
-44.512482	-22.392389	0.935898
-45.530829	-31.026475	0.940902
-45.380649	-31.281992	0.945907
-45.769752	-19.912214	0.950912
-45.759637	-17.376103	0.955917
-46.323632	-8.550083	0.960922
-46.015655	-21.223410	0.965926
-46.269820	-34.565860	0.970931
-46.315734	-13.222937	0.975936
-46.415320	-20.380528	0.980941
-47.380597	-21.612756	0.985946
-47.442819	-36.854773	0.990950
-47.458440	-35.550535	0.995955
-47.563550	-16.458586	1.000960
-47.885939	-22.203153	1.005965
-48.623665	-18.622202	1.010970
-49.289021	-12.953840	1.015974
-49.455571	-34.853060	1.020979
-49.397465	-32.561532	1.025984
-49.261817	-29.639356	1.030989
-49.638606	-20.952003	1.035994
-49.347965	-9.603407	1.040998
-49.624180	-32.306321	1.046003
-50.442648	-11.409541	1.051008
-50.692324	-33.777499	1.056013
-50.891518	-23.133571	1.061018
-51.009238	-7.280321	1.066022
-50.959520	-24.205392	1.071027
-51.994899	-29.321437	1.076032
-52.444411	-23.448154	1.081037
-52.626326	-11.527151	1.086042
-52.964476	-14.125090	1.091046
-52.571617	-23.900431	1.096051
-52.749593	-15.074387	1.101056
-52.706384	-28.522017	1.106061
-52.828594	-31.402845	1.111066
-53.280782	-8.703383	1.116070
-54.053809	-3.955933	1.121075
-54.296185	-8.644707	1.126080
-54.730969	-20.610512	1.131085
-54.582221	-20.302824	1.136090
-54.734124	-11.711818	1.141094
-55.261809	0.244931	1.146099
-55.568956	-5.585022	1.151104
-55.745395	4.429357	1.156109
-55.974717	-1.519503	1.161114
-55.902719	-13.896273	1.166118
-55.900109	-23.612940	1.171123
-56.824998	-16.045182	1.176128
-57.254410	-3.578404	1.181133
-57.287727	-1.317830	1.186138
-57.815002	-21.574489	1.191142
-57.159920	-30.274425	1.196147
-57.387949	-12.322720	1.201152
-57.958933	-19.662433	1.206157
-58.800678	-20.260169	1.211162
-58.960399	-7.479290	1.216166
-58.758442	-7.033809	1.221171
-59.370040	-9.332939	1.226176
-58.941464	-4.612923	1.231181
-59.664110	3.324781	1.236186
-60.314562	-12.564521	1.241190
-60.395852	-22.849625	1.246195
-60.895264	-6.777435	1.251200
-60.698796	-12.064810	1.256205
-60.642401	1.749774	1.261210
-60.902077	-15.018228	1.266214
-61.006479	-18.056875	1.271219
-62.324614	-9.646700	1.276224
-62.198281	-27.740551	1.281229
-62.408407	-14.877759	1.286234
-62.845303	2.566623	1.291238
-62.701848	-7.313900	1.296243
-62.762449	-24.363872	1.301248
-62.607309	-33.752589	1.306253
-63.256411	-18.471568	1.311258
-64.075743	10.856207	1.316262
-64.131959	-5.175108	1.321267
-64.183483	-23.528009	1.326272
-64.364246	-15.567611	1.331277
-64.369899	-0.954698	1.336282
-64.799649	-4.226044	1.341286
-65.241260	-23.361150	1.346291
-65.993681	-25.811409	1.351296
-66.041547	-10.123398	1.356301
-66.322776	-5.075369	1.361306
-66.117541	-14.716820	1.366310
-65.934566	-27.341071	1.371315
-66.306890	-1.742003	1.376320
-66.948558	-5.044912	1.381325
-67.483377	4.691526	1.386330
-67.745579	-10.468339	1.391334
-67.352780	-12.223116	1.396339
-67.783916	-13.383220	1.401344
-67.866877	-13.470095	1.406349
-68.435512	-14.738476	1.411354
-69.042789	-5.657307	1.416358
-68.807629	-15.637322	1.421363
-69.123247	-15.297281	1.426368
-69.066987	-22.031098	1.431373
-69.808218	-9.487538	1.436378
-70.236177	3.700102	1.441382
-70.371421	3.031574	1.446387
-70.475843	0.350320	1.451392
-70.933949	-5.898587	1.456397
-71.075426	-2.230521	1.461402
-71.094907	-13.268941	1.466406
-70.722971	-29.071206	1.471411
-71.988765	-6.004182	1.476416
-71.929614	-24.461588	1.481421
-72.179370	-13.140483	1.486426
-72.607670	-14.429492	1.491430
-72.437468	-11.859072	1.496435
-72.934536	-5.990353	1.501440
-73.936782	-13.221110	1.506445
-73.726423	-29.044415	1.511450
-74.162076	-20.463341	1.516454
-74.193235	-6.784928	1.521459
-74.243934	-5.952827	1.526464
-74.329723	-6.857005	1.531469
-74.187134	-1.713393	1.536474
-74.509010	4.612403	1.541478
-74.966300	-17.539949	1.546483
-75.469246	-21.265194	1.551488
-75.955360	-5.167779	1.556493
-75.701777	-7.005395	1.561498
-75.917272	-11.838390	1.566502
-76.418569	-2.417737	1.571507
-77.254536	-0.136868	1.576512
-77.393290	-6.971040	1.581517
-77.308581	-12.764343	1.586522
-77.522664	-14.306563	1.591526
-77.665974	-26.365019	1.596531
-77.618764	-14.922142	1.601536
-77.908886	-18.715508	1.606541
-78.721742	-27.501430	1.611546
-79.486893	-12.486605	1.616550
-79.041221	-18.426467	1.621555
-79.353001	-2.168067	1.626560
-79.097174	-8.371607	1.631565
-79.327731	-13.358168	1.636570
-79.997446	-18.456516	1.641574
-80.595272	-21.716553	1.646579
-80.769012	7.867136	1.651584
-80.308196	-14.001434	1.656589
-80.541921	-9.397665	1.661594
-80.932984	-5.789561	1.666598
-81.440704	-14.384435	1.671603
-82.514807	-17.993879	1.676608
-82.291269	-19.009648	1.681613
-82.360468	-15.679553	1.686618
-82.893507	-13.035130	1.691622
-82.586250	-10.034579	1.696627
-82.747497	-10.869466	1.701632
-82.645895	-15.769563	1.706637
-83.295288	-14.294487	1.711642
-84.050990	-7.500345	1.716646
-83.730153	-1.778834	1.721651
-83.860955	-5.651308	1.726656
-84.119284	-14.509647	1.731661
-85.152232	-12.465328	1.736666
-85.561527	-13.453057	1.741670
-85.472076	-5.052669	1.746675
-85.866925	-11.011849	1.751680
-85.423554	-23.066550	1.756685
-85.424258	-14.037594	1.761690
-85.690131	-5.716388	1.766694
-86.421001	-20.572489	1.771699
-87.271718	-14.060457	1.776704
-87.370534	-24.260785	1.781709
-87.045250	-24.649018	1.786714
-87.563163	11.272500	1.791718
-87.559816	5.547781	1.796723
-87.937898	-9.211369	1.801728
-88.820228	-11.922085	1.806733
-88.791833	-3.255521	1.811738
-89.148117	-6.354145	1.816742
-89.104453	-23.376264	1.821747
-89.439993	-13.539602	1.826752
-89.382808	-9.236147	1.831757
-89.118560	-7.475662	1.836762
-89.658084	-17.954631	1.841766
-90.266592	-23.807568	1.846771
-90.630470	-8.374019	1.851776
-90.649829	-10.336591	1.856781
-90.594338	7.703814	1.861786
-91.211600	-4.669034	1.866790
-91.783730	-29.247606	1.871795
-92.474448	-17.767610	1.876800
-92.203130	-1.832662	1.881805
-92.276716	-10.679018	1.886810
-92.742578	-22.321251	1.891814
-92.169996	-16.975266	1.896819
-92.465096	-6.485346	1.901824
-93.131113	-4.979704	1.906829
-93.469542	-8.307570	1.911834
-93.786410	11.869581	1.916838
-93.794072	-3.347150	1.921843
-93.986375	-17.749712	1.926848
-94.554365	-18.585637	1.931853
-95.096169	-10.901258	1.936858
-95.340833	-2.138961	1.941862
-95.346243	-15.660140	1.946867
-95.379243	-28.869566	1.951872
-95.629151	-17.905933	1.956877
-95.532525	-2.193561	1.961882
-96.317185	-8.249798	1.966886
-96.489179	-37.142648	1.971891
-97.045173	-29.971256	1.976896
-97.074672	-16.569139	1.981901
-96.932073	-4.448546	1.986906
-97.712757	-13.328668	1.991910
-98.276163	-23.962799	1.996915
-97.969742	-16.139283	2.006912
-97.446560	-24.989983	2.016909
-97.168257	-7.298212	2.026906
-97.167484	-10.100623	2.036902
-96.200765	-2.314345	2.046899
-96.090837	-4.968367	2.056896
-95.308721	-5.080475	2.066893
-94.406544	-0.788836	2.076890
-94.659389	-0.247099	2.086886
-93.277751	-10.086454	2.096883
-92.998835	-13.444693	2.106880
-93.043603	-17.232824	2.116877
-92.669266	2.926503	2.126874
-91.567888	-14.315202	2.136870
-91.168242	-1.819307	2.146867
-90.723412	-19.751461	2.156864
-90.038371	-0.892259	2.166861
-89.610697	-7.209097	2.176858
-89.455671	-11.075981	2.186854
-88.462314	-4.275006	2.196851
-88.459656	-12.810139	2.206848
-87.867706	-2.771265	2.216845
-86.922095	-18.209134	2.226842
-86.713114	-12.742916	2.236838
-86.312002	-20.027174	2.246835
-85.192290	-18.645447	2.256832
-84.918850	-5.377143	2.266829
-84.899532	-8.155062	2.276826
-84.761559	-5.033996	2.286822
-84.030055	-19.143556	2.296819
-83.437014	0.131571	2.306816
-82.646714	-2.383818	2.316813
-82.296196	-6.821515	2.326810
-81.092295	-8.635828	2.336806
-81.231052	-18.312994	2.346803
-80.926867	-15.823585	2.356800
-80.401523	-14.447633	2.366797
-79.549050	-13.665433	2.376794
-78.984790	3.858495	2.386790
-79.064802	-23.877521	2.396787
-78.054595	-5.119174	2.406784
-77.584282	-14.630418	2.416781
-77.568856	-19.500268	2.426778
-76.284501	0.017174	2.436774
-76.103677	-18.951124	2.446771
-76.150162	-6.401055	2.456768
-74.871396	-22.183578	2.466765
-74.491512	-8.767721	2.476762
-74.600234	-9.946700	2.486758
-73.322085	-4.003902	2.496755
-72.927289	-4.226327	2.506752
-72.771268	-15.332944	2.516749
-72.403661	-21.022329	2.526746
-71.284573	-0.655990	2.536742
-70.971323	-17.626788	2.546739
-71.157852	-2.556032	2.556736
-70.281947	-11.318357	2.566733
-69.652812	-19.808966	2.576730
-69.104700	-32.100934	2.586726
-68.313520	-3.566519	2.596723
-68.127392	-18.092944	2.606720
-67.868452	-17.011059	2.616717
-67.290157	-23.248283	2.626714
-66.481668	-9.419179	2.636710
-66.230076	-7.108840	2.646707
-66.040271	-22.409547	2.656704
-65.022481	-22.370663	2.666701
-64.749682	-10.318132	2.676698
-63.754362	-4.030792	2.686694
-63.311351	-1.202225	2.696691
-63.324726	-21.243881	2.706688
-63.025126	-7.603380	2.716685
-61.970854	-8.478039	2.726682
-61.657008	-20.893088	2.736678
-61.319591	-15.323643	2.746675
-60.247476	-15.726948	2.756672
-60.081894	-14.133997	2.766669
-60.010420	-26.252476	2.776666
-59.009343	-19.375044	2.786662
-58.921350	-7.297696	2.796659
-58.411267	-3.151537	2.806656
-57.262452	-18.734007	2.816653
-57.038999	-7.649378	2.826650
-56.843796	-12.254504	2.836646
-55.766784	-19.076898	2.846643
-55.522371	-12.896093	2.856640
-55.489424	-1.798545	2.866637
-54.564678	-4.846603	2.876634
-53.987865	-13.885245	2.886630
-53.709400	-3.037175	2.896627
-53.048499	-11.297270	2.906624
-52.697680	0.522314	2.916621
-52.309873	-9.494542	2.926618
-51.405289	-9.779289	2.936614
-50.859206	-16.350473	2.946611
-50.688714	-11.953810	2.956608
-50.368639	-11.720401	2.966605
-49.339993	0.461762	2.976602
-49.096171	-18.979105	2.986598
-48.721614	-3.155292	2.996595
-47.485942	-19.500905	3.006592
-47.944481	-8.843255	3.016589
-47.305148	-12.841144	3.026586
-46.426688	-18.574262	3.036582
-45.660024	-13.143510	3.046579
-45.841166	-20.020511	3.056576
-45.589957	-19.320581	3.066573
-44.605656	4.153480	3.076570
-44.150191	-22.039137	3.086566
-43.059064	-6.331181	3.096563
-43.224240	4.793091	3.106560
-42.985427	-15.677440	3.116557
-42.204497	-7.223864	3.126554
-41.262292	-1.453206	3.136550
-40.852964	-15.907873	3.146547
-40.892577	-10.586357	3.156544
-40.075949	1.334434	3.166541
-39.576437	-14.857422	3.176538
-39.284425	2.033440	3.186534
-38.201985	-10.605041	3.196531
-38.055693	-4.045819	3.206528
-38.079164	-4.961142	3.216525
-36.866897	-10.981344	3.226522
-36.269009	1.847258	3.236518
-36.140720	-15.783592	3.246515
-35.818433	5.436471	3.256512
-34.989122	-17.485377	3.266509
-34.816086	-6.049674	3.276506
-33.607660	-12.927863	3.286502
-33.696808	-12.155288	3.296499
-33.276733	-26.564510	3.306496
-32.668347	-19.712649	3.316493
-31.681227	-3.589547	3.326490
-31.490968	-20.160837	3.336486
-31.477099	-22.987043	3.346483
-30.471624	-2.055311	3.356480
-30.297880	-5.750563	3.366477
-29.369393	-15.218507	3.376474
-28.697680	-16.698820	3.386470
-28.384443	-0.606479	3.396467
-28.586616	-19.125589	3.406464
-27.399988	-0.901788	3.416461
-26.944888	-16.244473	3.426458
-26.878538	-10.350997	3.436454
-25.942161	-12.562796	3.446451
-25.654253	-15.310036	3.456448
-25.341552	-8.628084	3.466445
-24.244038	-0.491923	3.476442
-24.044047	-18.369007	3.486438
-23.613332	-14.973926	3.496435
-22.459394	-17.821024	3.506432
-22.151221	-0.431763	3.516429
-21.944800	-6.628181	3.526426
-21.800144	-11.955667	3.536422
-21.526857	-7.566507	3.546419
-20.492758	0.459931	3.556416
-20.113808	-19.048411	3.566413
-18.935676	-15.994442	3.576410
-18.676070	-19.642741	3.586406
-18.531891	2.612056	3.596403
-18.455282	-4.794495	3.606400
-17.574252	-21.547700	3.616397
-16.975032	-11.592394	3.626394
-16.857875	-12.974838	3.636390
-15.593715	-7.549351	3.646387
-15.334259	-10.643024	3.656384
-15.238870	-9.414494	3.666381
-14.477953	-11.686486	3.676378
-13.726167	-21.220638	3.686374
-13.742804	-1.801969	3.696371
-13.235498	-22.015219	3.706368
-12.449998	-5.888424	3.716365
-12.221936	-11.925146	3.726362
-11.481700	1.811947	3.736358
-10.401365	-14.082787	3.746355
-10.429911	-3.477425	3.756352
-10.371631	-19.236932	3.766349
-9.555829	-8.715006	3.776346
-8.844671	-4.298644	3.786342
-8.664200	0.392396	3.796339
-8.156098	-1.820335	3.806336
-7.409138	-11.992748	3.816333
-7.335897	-1.819639	3.826330
-6.537061	-14.170048	3.836326
-6.048398	-8.021006	3.846323
-5.266602	4.176187	3.856320
-4.933746	5.959291	3.866317
-4.597013	-12.201257	3.876314
-4.449037	-3.032168	3.886310
-4.023448	14.920564	3.896307
-3.303500	23.641148	3.906304
-3.136006	25.300362	3.916301
-2.442752	59.124839	3.926298
-1.665573	66.513925	3.936294
-1.239136	69.124001	3.946291
-0.952505	88.197538	3.956288
-0.443012	104.056758	3.966285
0.000000	119.949255	3.971290
-0.028457	113.871068	3.976294
0.425105	125.352755	3.981299
0.418353	141.633809	3.986304
0.531174	153.976289	3.991309
0.670524	158.377787	3.996314
0.360391	159.790295	4.001318
0.724151	151.178450	4.006323
0.498551	144.261979	4.011328
0.603589	151.153260	4.016333
0.992515	160.936704	4.021338
0.698012	167.087189	4.026342
0.815592	145.715162	4.031347
0.712797	151.997614	4.036352
0.875366	163.372149	4.041357
0.962449	161.701515	4.046362
0.879039	153.942184	4.051366
0.615455	164.977958	4.056371
0.809504	167.614017	4.061376
0.976344	148.885564	4.066381
1.106137	140.624606	4.071386
0.971035	163.922604	4.076390
1.075179	164.823727	4.081395
0.999375	158.952514	4.086400
0.907440	152.611847	4.091405
1.527277	154.224812	4.096410
1.018681	167.653304	4.101414
1.108778	169.080365	4.106419
1.178873	155.468810	4.111424
0.919270	147.699436	4.116429
1.178411	166.993137	4.121434
0.670320	170.396593	4.126438
0.895851	155.669602	4.131443
0.919183	166.286855	4.136448
0.800887	169.870637	4.141453
0.791001	158.327006	4.146458
1.004453	183.617998	4.151462
0.952838	173.348566	4.156467
1.280983	159.624422	4.161472
1.253903	186.905806	4.166477
1.487227	187.516869	4.171482
1.065810	194.036190	4.176486
1.348881	155.677929	4.181491
1.248560	168.111774	4.186496
1.008994	167.984289	4.191501
1.487509	179.663528	4.196506
1.351834	162.954235	4.201510
1.229163	147.937360	4.206515
1.077210	157.169180	4.211520
1.227399	165.587453	4.216525
1.490598	173.944045	4.221530
1.532189	180.846021	4.226534
1.374224	151.285190	4.231539
1.314092	161.904494	4.236544
1.006101	154.321368	4.241549
1.320527	162.979238	4.246554
1.590382	201.487795	4.251558
1.524645	184.833778	4.256563
1.507051	158.144919	4.261568
1.143946	151.676434	4.266573
1.514896	162.511955	4.271578
1.430449	167.499407	4.276582
1.296266	169.606116	4.281587
1.430572	181.330697	4.286592
1.503559	193.993513	4.291597
1.686910	187.612542	4.296602
1.689808	177.137891	4.301606
1.353116	184.937427	4.306611
1.422558	202.332721	4.311616
1.236432	195.960547	4.316621
1.890414	176.817711	4.321626
1.653661	196.695930	4.326630
1.895942	188.207892	4.331635
1.687870	173.892179	4.336640
1.300059	179.628679	4.341645
1.577375	183.201540	4.346650
1.372499	195.978738	4.351654
1.684155	206.919283	4.356659
1.906403	189.504454	4.361664
1.566587	172.976066	4.366669
2.122409	179.615696	4.371674
1.582068	183.657401	4.376678
1.685765	180.766325	4.381683
1.798289	185.257988	4.386688
1.432122	199.394954	4.391693
1.650361	194.441676	4.396698
1.550444	183.589103	4.401702
1.550616	191.934028	4.406707
1.470807	192.449756	4.411712
1.196636	198.768169	4.416717
1.647050	200.973101	4.421722
1.551363	204.148999	4.426726
1.550672	187.616614	4.431731
1.728009	193.541387	4.436736
1.841542	220.774044	4.441741
1.903158	227.993434	4.446746
2.017267	225.931138	4.451750
1.910847	203.855800	4.456755
1.707923	209.840830	4.461760
2.027030	217.795690	4.466765
1.938890	213.689217	4.471770
1.940771	223.276333	4.476774
2.047637	221.013206	4.481779
2.195049	233.320045	4.486784
1.433118	218.955050	4.491789
2.317437	210.077313	4.496794
2.164115	215.634011	4.501798
1.932127	196.038505	4.506803
2.071513	224.656633	4.511808
2.300277	216.851403	4.516813
1.919695	188.640452	4.521818
1.918804	181.031815	4.526822
2.255860	198.197622	4.531827
2.079354	227.065744	4.536832
1.979858	223.558649	4.541837
2.348253	218.468190	4.546842
2.147789	237.970811	4.551846
2.156005	222.312335	4.556851
2.036300	199.287454	4.561856
2.055751	208.759891	4.566861
2.467872	235.457298	4.571866
2.047802	229.074447	4.576870
2.513681	214.236950	4.581875
2.107152	206.498238	4.586880
2.067263	205.287265	4.591885
2.109341	220.393046	4.596890
2.550358	215.762612	4.601894
2.284648	205.107810	4.606899
2.398878	210.209033	4.611904
2.283314	231.686436	4.616909
2.484737	215.169673	4.621914
1.994393	207.323870	4.626918
2.280369	201.290755	4.631923
2.341314	212.081263	4.636928
2.472110	223.377737	4.641933
2.533804	228.561929	4.646938
2.549415	216.069792	4.651942
2.232640	196.564354	4.656947
2.181293	200.259204	4.661952
2.383171	214.986995	4.666957
2.629482	222.747025	4.671962
2.293500	222.123693	4.676966
2.338894	232.844280	4.681971
2.734663	243.123532	4.686976
2.206068	222.978614	4.691981
2.190452	213.091185	4.696986
1.864004	230.915128	4.701990
2.380623	242.027606	4.706995
2.276658	223.257892	4.712000
2.078782	219.039436	4.717005
2.575848	222.414901	4.722010
2.354074	234.606469	4.727014
2.466871	231.978747	4.732019
2.667862	229.210084	4.737024
2.615795	232.079484	4.742029
2.734450	246.761969	4.747034
2.501667	254.876908	4.752038
2.810545	243.843613	4.757043
2.737512	215.886828	4.762048
2.588315	237.547460	4.767053
2.700851	243.299354	4.772058
2.460459	251.445734	4.777062
2.973369	247.423507	4.782067
3.072106	237.039613	4.787072
2.790522	233.190017	4.792077
2.884372	238.832441	4.797082
2.491203	230.010141	4.802086
2.525222	230.822138	4.807091
2.817135	241.980529	4.812096
2.851897	240.708584	4.817101
2.963525	211.432270	4.822106
2.891392	235.762669	4.827110
2.737046	246.063878	4.832115
2.950358	235.483881	4.837120
2.554056	235.559270	4.842125
2.993199	240.477582	4.847130
2.941505	238.629521	4.852134
2.796963	221.302225	4.857139
3.021041	231.454275	4.862144
2.939902	248.354218	4.867149
2.947914	252.484860	4.872154
2.736035	251.599135	4.877158
2.679870	228.742359	4.882163
2.912330	261.962447	4.887168
2.796288	272.985854	4.892173
2.954209	270.328867	4.897178
2.967146	241.769694	4.902182
2.801645	267.693136	4.907187
2.924447	265.875523	4.912192
2.826988	261.196746	4.917197
2.862291	257.189815	4.922202
2.731938	257.642379	4.927206
2.797673	242.972390	4.932211
2.913136	252.274211	4.937216
2.872082	274.542940	4.942221
3.142266	278.387986	4.947226
3.157497	286.269889	4.952230
3.519399	285.593175	4.957235
3.298141	265.385674	4.962240
2.787742	253.434999	4.967245
3.024112	245.921676	4.972250
3.050142	285.343050	4.977254
3.434666	286.794761	4.982259
3.234328	281.515151	4.987264
3.014090	298.402918	4.992269
3.328113	308.316621	4.997274
3.161923	293.451412	5.002278
3.293705	277.707154	5.007283
3.591146	281.131603	5.012288
3.541189	296.450752	5.017293
3.488473	287.209824	5.022298
3.056470	265.691500	5.027302
3.209098	298.837559	5.032307
3.306381	299.278845	5.037312
3.267314	297.780073	5.042317
3.637145	285.409078	5.047322
3.709125	309.818668	5.052326
3.090550	297.305196	5.057331
3.290968	281.993308	5.062336
3.109536	277.766988	5.067341
3.546941	281.169096	5.072346
3.315751	301.876822	5.077350
3.478451	292.298727	5.082355
3.392510	298.270970	5.087360
3.585610	302.669448	5.092365
3.690396	280.565705	5.097370
3.316877	281.247167	5.102374
3.521775	287.569286	5.107379
3.609949	297.980297	5.112384
3.216924	301.390711	5.117389
3.532650	302.339248	5.122394
3.508979	288.689207	5.127398
3.359542	295.063967	5.132403
3.549401	307.566375	5.137408
3.319878	299.881326	5.142413
3.385063	279.658628	5.147418
3.234035	289.720789	5.152422
3.562465	296.008983	5.157427
3.690539	309.835882	5.162432
3.581576	286.500722	5.167437
3.937640	302.973246	5.172442
3.539092	318.583226	5.177446
3.766310	326.855388	5.182451
3.609145	305.019520	5.187456
3.666102	315.147454	5.192461
4.048318	318.182449	5.197466
3.630790	330.935391	5.202470
3.383876	322.455344	5.207475
4.080147	309.188131	5.212480
3.431359	323.608349	5.217485
3.844292	330.558624	5.222490
3.649709	339.870698	5.227494
3.585646	330.578152	5.232499
3.893506	318.216090	5.237504
3.502286	328.152241	5.242509
3.827667	331.396688	5.247514
3.735288	331.155306	5.252518
3.783660	318.523116	5.257523
4.139639	323.630002	5.262528
3.671499	338.020085	5.267533
4.269950	325.109259	5.272538
3.909922	330.894889	5.277542
3.660677	328.820612	5.282547
4.027683	328.395295	5.287552
3.821101	313.095096	5.292557
3.910269	311.142069	5.297562
4.051168	330.446541	5.302566
3.773533	344.242165	5.307571
4.148218	332.502169	5.312576
3.935252	324.637892	5.317581
3.957394	321.731067	5.322586
3.922070	332.443854	5.327590
4.330146	342.922874	5.332595
4.221536	321.607118	5.337600
3.928514	325.824717	5.342605
4.074578	328.359729	5.347610
4.253046	332.256346	5.352614
4.059996	319.764376	5.357619
3.887958	336.749971	5.362624
3.951960	349.296394	5.367629
4.301477	363.235409	5.372634
4.464167	373.793672	5.377638
4.537166	346.203162	5.382643
4.546534	332.312644	5.387648
4.095464	344.149377	5.392653
4.145680	336.708007	5.397658
4.158755	330.931539	5.402662
3.964943	321.191371	5.407667
4.357635	343.163604	5.412672
4.213753	358.045939	5.417677
4.253147	357.740164	5.422682
4.340900	362.402589	5.427686
4.400346	353.750559	5.432691
4.745126	356.665380	5.437696
4.144682	365.854742	5.442701
4.363612	362.734469	5.447706
4.400627	367.949718	5.452710
4.253906	367.013660	5.457715
4.504645	368.390222	5.462720
4.459577	360.653155	5.467725
4.272542	359.166696	5.472730
4.402089	344.575439	5.477734
4.278783	365.325006	5.482739
4.177186	363.083681	5.487744
4.135279	358.860916	5.492749
4.139203	362.799999	5.497754
4.249529	351.464036	5.502758
4.076411	378.708339	5.507763
4.389338	365.376185	5.512768
4.602677	364.979715	5.517773
4.649434	381.939363	5.522778
4.651717	377.824215	5.527782
4.848692	398.708922	5.532787
4.628901	373.081706	5.537792
4.402680	377.955831	5.542797
4.822744	354.943714	5.547802
4.533669	361.483235	5.552806
4.449124	375.558509	5.557811
4.524217	358.526119	5.562816
4.448104	376.751791	5.567821
4.743746	382.904077	5.572826
4.799484	373.483096	5.577830
4.923635	375.689589	5.582835
4.818079	364.116827	5.587840
4.623570	370.440962	5.592845
4.946798	383.656516	5.597850
4.670440	384.338893	5.602854
4.838756	377.750923	5.607859
4.828818	373.950806	5.612864
4.771217	385.204054	5.617869
4.916775	362.640464	5.622874
4.860240	380.580279	5.627878
4.846650	388.062147	5.632883
5.049449	383.516408	5.637888
4.548035	374.229721	5.642893
4.814625	375.859852	5.647898
4.971379	371.461116	5.652902
4.699370	384.075821	5.657907
5.276322	366.061607	5.662912
4.639533	385.607519	5.667917
4.971020	386.629811	5.672922
5.241037	384.664644	5.677926
4.898093	377.655592	5.682931
5.161388	381.406016	5.687936
4.890656	382.185025	5.692941
5.009161	369.954143	5.697946
4.912610	382.100769	5.702950
5.156668	389.130572	5.707955
5.527514	383.210518	5.712960
4.453741	364.206404	5.717965
4.655846	355.601134	5.722970
4.857349	376.011749	5.727974
4.626415	394.412973	5.732979
4.981652	375.736565	5.737984
4.935434	394.012461	5.742989
5.088012	378.376827	5.747994
5.169129	377.128383	5.752998
4.836412	391.668178	5.758003
5.445032	376.448351	5.763008
4.972815	387.429684	5.768013
4.922289	383.812161	5.773018
4.948250	378.950380	5.778022
4.796703	403.529937	5.783027
5.293381	417.725140	5.788032
5.148064	409.871243	5.793037
5.276392	394.891959	5.798042
5.418398	408.688729	5.803046
5.151277	406.231287	5.808051
5.332117	407.812852	5.813056
5.322035	422.433225	5.818061
5.253549	422.075730	5.823066
5.311410	407.841825	5.828070
5.436385	404.968104	5.833075
5.523451	409.715395	5.838080
5.406098	431.025869	5.843085
5.170958	430.569052	5.848090
5.475190	424.028642	5.853094
5.199956	407.997365	5.858099
5.438340	419.152203	5.863104
5.370068	429.329713	5.868109
5.522715	423.808629	5.873114
5.379287	422.992769	5.878118
5.092970	425.669685	5.883123
5.281696	412.109225	5.888128
5.221778	401.963631	5.893133
5.173735	426.836271	5.898138
5.271186	418.722561	5.903142
5.315989	423.953410	5.908147
5.298568	426.380997	5.913152
5.721022	447.974587	5.918157
5.793636	445.237952	5.923162
5.578328	438.683954	5.928166
5.374697	417.312149	5.933171
5.637405	414.607240	5.938176
5.363357	422.965053	5.943181
5.923772	428.412560	5.948186
5.482080	435.295868	5.953190
5.848693	456.550272	5.958195
5.849456	442.284140	5.963200
5.576549	419.851373	5.968205
5.035274	416.030243	5.973210
5.482557	452.375440	5.978214
5.760110	465.180837	5.983219
5.815414	448.113934	5.988224
5.498328	463.558188	5.993229
5.874556	446.612564	5.998234
6.001362	452.462603	6.003238
5.979220	463.321374	6.008243
5.838425	435.521879	6.013248
5.717250	423.342993	6.018253
5.623168	428.554968	6.023258
5.857762	430.124792	6.028262
5.713975	418.036951	6.033267
5.821587	414.966039	6.038272
5.653909	440.671924	6.043277
5.072660	432.588883	6.048282
5.525737	431.414212	6.053286
5.525262	442.656188	6.058291
5.918714	445.599483	6.063296
5.726205	470.925880	6.068301
5.825697	446.944997	6.073306
5.880368	449.040363	6.078310
5.409049	437.583133	6.083315
6.014599	424.783609	6.088320
5.596909	438.411579	6.093325
5.375689	450.077826	6.098330
5.496460	433.774214	6.103334
5.406483	432.128175	6.108339
5.674289	443.734616	6.113344
5.762770	456.236536	6.118349
5.761261	443.178138	6.123354
6.061169	457.880394	6.128358
5.588611	461.392078	6.133363
5.952144	455.697235	6.138368
5.965759	461.877219	6.143373
5.714020	439.625397	6.148378
5.592460	414.937780	6.153382
5.391748	414.371003	6.158387
5.675080	427.680986	6.163392
5.712684	437.432699	6.168397
6.131428	442.933119	6.173402
5.606477	437.048917	6.178406
5.379219	424.969536	6.183411
5.700002	418.580876	6.188416
5.677642	431.046837	6.193421
5.708129	451.262672	6.198426
5.657417	459.741139	6.203430
5.511604	451.681226	6.208435
5.989899	437.207744	6.213440
5.443825	447.999590	6.218445
5.583584	471.268121	6.223450
5.722596	460.540635	6.228454
5.579161	443.128460	6.233459
5.913617	456.579768	6.238464
5.545569	466.527568	6.243469
5.710989	456.664617	6.248474
6.080846	443.304934	6.253478
5.762235	427.528018	6.258483
5.667426	411.806468	6.263488
5.381336	408.709073	6.268493
5.709293	429.452813	6.273498
5.778934	447.189159	6.278502
5.680330	472.984206	6.283507
5.972303	449.570505	6.288512
5.402466	430.901693	6.293517
5.851329	440.264247	6.298522
5.373446	444.819915	6.303526
5.512161	452.425604	6.308531
5.665340	435.240440	6.313536
5.315660	445.781521	6.318541
5.813792	453.944170	6.323546
5.848816	464.092499	6.328550
5.692800	439.235632	6.333555
5.870236	443.421390	6.338560
5.864306	447.599865	6.343565
5.674760	461.411422	6.348570
5.410192	458.598317	6.353574
5.356584	460.608095	6.358579
5.590709	461.929505	6.363584
5.667192	459.718714	6.368589
5.744717	458.163173	6.373594
5.888365	448.715188	6.378598
5.595303	455.223643	6.383603
5.590784	435.867342	6.388608
5.803415	443.251381	6.393613
5.753278	443.513226	6.398618
6.046256	459.453778	6.403622
5.682323	450.712835	6.408627
6.108036	432.559879	6.413632
5.635991	433.378966	6.418637
5.429854	434.965197	6.423642
5.779389	437.384231	6.428646
5.736952	454.084457	6.433651
5.887473	453.382789	6.438656
5.903717	439.612177	6.443661
5.879808	426.960768	6.448666
5.527041	415.033339	6.453670
5.136717	423.925311	6.458675
5.717406	427.714052	6.463680
5.682765	455.595072	6.468685
6.048459	436.726865	6.473690
5.674330	433.533232	6.478694
5.459759	434.485956	6.483699
5.967344	438.544943	6.488704
5.741130	437.338107	6.493709
5.652573	436.094811	6.498714
5.765040	426.945472	6.503718
5.422537	433.318259	6.508723
6.066671	431.355383	6.513728
5.688441	419.367051	6.518733
5.570627	423.811419	6.523738
5.540808	427.459262	6.528742
5.563679	418.337854	6.533747
5.922678	421.429878	6.538752
5.722830	419.553897	6.543757
5.570481	409.580324	6.548762
5.892074	416.015796	6.553766
5.758594	432.380152	6.558771
5.771240	412.245175	6.563776
5.544360	415.559794	6.568781
5.639301	412.207757	6.573786
5.750000	420.426029	6.578790
5.330872	419.309771	6.583795
5.578452	420.684689	6.588800
5.742712	459.522065	6.593805
5.933131	436.051772	6.598810
6.217364	413.828709	6.603814
5.527577	417.544970	6.608819
5.725253	415.652225	6.613824
5.386173	420.032734	6.618829
5.600654	427.167669	6.623834
5.953489	431.933393	6.628838
5.481941	418.268172	6.633843
5.753608	420.192033	6.638848
5.842389	422.339467	6.643853
5.751528	434.168928	6.648858
5.853924	424.629226	6.653862
5.986922	413.113778	6.658867
5.694008	429.937051	6.663872
5.626386	434.976461	6.668877
5.729055	433.327884	6.673882
5.741330	423.334398	6.678886
5.428089	419.542269	6.683891
5.659110	421.735449	6.688896
5.409880	426.979376	6.693901
5.812208	422.221903	6.698906
5.748102	416.504916	6.703910
5.820940	422.371556	6.708915
5.599608	425.584146	6.713920
5.663849	431.381775	6.718925
5.852470	426.284063	6.723930
5.802621	410.462256	6.728934
5.759305	413.484530	6.733939
5.879024	419.532925	6.738944
5.604698	432.143218	6.743949
5.469414	427.929848	6.748954
5.692942	414.969926	6.753958
5.718791	427.203985	6.758963
5.822866	432.366347	6.763968
5.671166	429.712754	6.768973
5.817638	431.951573	6.773978
5.695809	419.805648	6.778982
5.736815	445.798452	6.783987
5.930611	432.860692	6.788992
5.655013	424.723888	6.793997
5.751916	412.970251	6.799002
6.100791	425.332637	6.804006
5.720835	443.423734	6.809011
5.828648	418.651149	6.814016
5.715637	410.070499	6.819021
5.778586	425.171653	6.824026
6.014356	431.028338	6.829030
5.693890	446.484084	6.834035
5.994686	416.408533	6.839040
5.802289	392.066090	6.844045
5.118394	404.742959	6.849050
5.534098	424.745450	6.854054
5.658498	426.256341	6.859059
5.834195	412.957379	6.864064
5.662646	436.225216	6.869069
5.741138	425.861015	6.874074
5.668516	415.163897	6.879078
5.680525	421.542215	6.884083
6.035272	428.201274	6.889088
5.578822	435.729616	6.894093
5.673654	420.726544	6.899098
5.552855	410.532112	6.904102
5.553926	426.138410	6.909107
5.712403	425.835644	6.914112
5.588362	425.664403	6.919117
5.993075	422.721762	6.924122
5.860621	407.194659	6.929126
5.587746	417.606820	6.934131
5.742772	417.423200	6.939136
5.208322	404.537447	6.944141
5.637143	420.315034	6.949146
6.024622	423.686656	6.954150
5.770083	425.795927	6.959155
5.917918	416.709408	6.964160
5.381204	406.933714	6.969165
5.620565	413.416117	6.974170
5.858728	413.411122	6.979174
5.759382	415.101928	6.984179
5.837338	429.500499	6.989184
5.432260	423.383313	6.994189
5.767213	414.684536	6.999194
5.584864	403.540927	7.004198
5.595810	404.184507	7.009203
5.717718	407.555522	7.014208
5.844920	417.275646	7.019213
5.474575	431.982790	7.024218
5.874823	433.251293	7.029222
5.366151	431.763920	7.034227
5.691288	406.002697	7.039232
5.440664	418.788503	7.044237
5.274679	438.099138	7.049242
5.802148	434.703339	7.054246
5.405120	420.859380	7.059251
5.600038	414.523878	7.064256
5.656683	420.014779	7.069261
5.384921	434.809512	7.074266
5.705622	423.753220	7.079270
5.851112	416.303466	7.084275
5.931683	416.519837	7.089280
5.891348	423.327837	7.094285
5.608137	438.862749	7.099290
6.076411	421.689749	7.104294
5.657712	406.189727	7.109299
5.743678	420.267938	7.114304
5.859111	434.726021	7.119309
5.938657	414.462101	7.124314
5.883396	420.572460	7.129318
5.684831	428.568292	7.134323
5.708131	409.535531	7.139328
5.726014	418.829707	7.144333
5.717107	433.586129	7.149338
5.503841	416.912760	7.154342
5.489604	407.810118	7.159347
5.671934	421.505138	7.164352
5.689811	439.749584	7.169357
5.638950	430.252271	7.174362
5.967785	414.856486	7.179366
5.626874	421.691270	7.184371
5.972244	423.397369	7.189376
5.866546	431.837458	7.194381
5.421015	403.023571	7.199386
5.740469	406.630954	7.204390
5.784357	417.081327	7.209395
5.959306	418.646801	7.214400
5.378004	414.156151	7.219405
5.194283	398.704609	7.224410
5.559521	414.695322	7.229414
5.866863	435.057846	7.234419
6.053718	418.904915	7.239424
6.087457	413.116715	7.244429
5.469245	402.595197	7.249434
5.557198	387.795325	7.254438
5.376335	400.906373	7.259443
5.664849	409.557617	7.264448
5.679003	411.408910	7.269453
5.334847	404.957505	7.274458
5.682785	426.403569	7.279462
5.654103	443.018152	7.284467
5.756875	431.313348	7.289472
5.467918	429.366859	7.294477
5.749663	430.711273	7.299482
5.782517	417.641495	7.304486
5.805999	417.812650	7.309491
5.755224	420.958777	7.314496
5.931764	435.443262	7.319501
6.050604	433.244318	7.324506
5.907683	397.808386	7.329510
5.388973	388.218345	7.334515
5.631191	396.118925	7.339520
5.731763	409.782659	7.344525
5.640991	414.450927	7.349530
5.765619	411.146170	7.354534
5.788818	427.394760	7.359539
5.816953	407.742875	7.364544
5.482711	391.059833	7.369549
5.288144	383.099460	7.374554
5.784562	408.548857	7.379558
5.710301	426.522236	7.384563
5.951142	435.872208	7.389568
5.883938	417.924333	7.394573
5.566719	392.374247	7.399578
5.715164	390.985644	7.404582
5.490024	409.867429	7.409587
5.782900	420.532946	7.414592
5.565455	414.980789	7.419597
5.593206	433.594611	7.424602
6.052753	425.492777	7.429606
5.550356	404.597903	7.434611
5.805637	402.288126	7.439616
5.606726	409.530925	7.444621
5.712108	425.487251	7.449626
5.786766	399.215693	7.454630
5.687794	406.406857	7.459635
5.855084	410.954841	7.464640
5.518778	393.887903	7.469645
5.532740	381.657320	7.474650
5.469107	403.008497	7.479654
5.724253	432.838521	7.484659
6.031364	419.062279	7.489664
5.661980	401.015993	7.494669
5.307530	413.673644	7.499674
5.957523	417.843549	7.504678
5.531764	417.191738	7.509683
5.544790	433.207233	7.514688
5.671650	417.259246	7.519693
5.602552	407.928519	7.524698
5.792082	415.185259	7.529702
5.868686	436.103227	7.534707
5.675317	431.436991	7.539712
5.912229	421.191725	7.544717
5.402700	404.077441	7.549722
5.632568	412.808617	7.554726
5.430294	419.079897	7.559731
5.798405	408.683236	7.564736
5.807158	428.298116	7.569741
5.847654	426.004396	7.574746
5.798908	415.856256	7.579750
5.981840	404.687399	7.584755
5.402773	397.449825	7.589760
5.758082	406.449700	7.594765
5.527216	400.157142	7.599770
5.892479	390.243254	7.604774
5.568302	396.312318	7.609779
5.857436	419.035716	7.614784
5.766756	398.654541	7.619789
5.644580	390.227532	7.624794
5.743141	398.314820	7.629798
5.054227	395.603419	7.634803
5.148452	413.134026	7.639808
5.388519	415.353134	7.644813
5.450165	411.350984	7.649818
5.457878	422.002761	7.654822
5.721877	424.367466	7.659827
5.760336	416.536663	7.664832
5.824178	408.888508	7.669837
5.844645	414.267995	7.674842
5.885241	408.309185	7.679846
6.010162	415.098947	7.684851
5.878328	415.238158	7.689856
5.713555	435.584592	7.694861
5.706162	427.289625	7.699866
6.248558	402.876539	7.704870
6.061304	408.105582	7.709875
5.844957	400.251788	7.714880
5.711468	385.972085	7.719885
5.355827	379.677269	7.724890
5.619790	385.290057	7.729894
5.431273	392.433371	7.734899
5.799939	416.963581	7.739904
5.819190	424.822597	7.744909
5.508676	402.207258	7.749914
5.805288	390.606586	7.754918
5.775443	406.429869	7.759923
5.796185	379.775621	7.764928
5.348032	385.272491	7.769933
5.683836	407.859424	7.774938
5.633936	394.670069	7.779942
5.746481	405.839182	7.784947
5.798951	412.228567	7.789952
5.907671	406.520313	7.794957
5.441875	406.176094	7.799962
5.535339	406.975909	7.804966
5.562257	401.941723	7.809971
5.556018	401.479338	7.814976
5.811717	410.671369	7.819981
5.528987	432.182597	7.824986
5.510634	425.485275	7.829990
5.323432	420.097595	7.834995
5.380006	416.435040	7.840000
5.622429	411.571905	7.845005
5.289762	420.286251	7.850010
5.411834	417.341882	7.855014
5.468045	414.549268	7.860019
5.635657	410.624309	7.865024
5.462685	408.904980	7.870029
5.509261	408.575328	7.875034
5.935425	435.404827	7.880038
5.487265	438.677100	7.885043
6.117780	417.111612	7.890048
5.969820	406.554601	7.895053
5.579595	421.044740	7.900058
5.725153	426.264760	7.905062
5.636358	429.214450	7.910067
5.629867	401.349713	7.915072
5.939453	411.925948	7.920077
5.546292	435.974214	7.925082
5.603944	430.359129	7.930086
5.825072	421.356086	7.935091
5.737619	405.346458	7.940096
5.492612	410.898352	7.945101
5.429486	411.042781	7.950106
5.703110	412.235927	7.955110
5.640391	421.024337	7.960115
5.662751	424.811529	7.965120
5.771154	414.155523	7.970125
5.343439	417.027782	7.975142
5.855917	433.042775	7.980160
5.938632	437.028668	7.985178
5.806416	413.410671	7.990195
5.753465	405.071299	7.995213
5.603409	405.619206	8.000230
5.726548	412.698294	8.005248
5.800918	429.645375	8.010266
5.707954	423.321373	8.015283
5.672081	409.494552	8.020301
5.778970	415.393700	8.025318
5.368560	403.010464	8.030336
5.625630	412.300134	8.035354
6.031916	438.548211	8.040371
5.974493	433.162940	8.045389
5.605271	436.413123	8.050406
5.914287	417.008364	8.055424
5.652649	430.535705	8.060442
5.696729	416.609765	8.065459
5.932147	415.703824	8.070477
5.701824	420.646987	8.075494
6.086325	418.743464	8.080512
5.561455	438.353500	8.085530
5.719587	407.704123	8.090547
5.896339	409.363430	8.095565
5.839102	425.674474	8.100582
5.934731	412.640643	8.105600
6.061926	409.753859	8.110618
6.046271	415.619927	8.115635
5.638311	420.866185	8.120653
5.675048	404.049890	8.125670
5.806049	399.217673	8.130688
5.691284	413.503569	8.135706
5.859442	429.458368	8.140723
6.035840	409.994651	8.145741
5.677118	415.173437	8.150758
5.798161	425.430201	8.155776
5.588992	432.722437	8.160794
5.743073	433.056155	8.165811
6.151666	437.332386	8.170829
6.155311	449.951982	8.175846
5.965592	439.241103	8.180864
5.821914	421.842379	8.185882
5.836351	430.213282	8.190899
6.102179	448.213763	8.195917
5.808860	455.592434	8.200934
6.053957	437.153841	8.205952
5.800576	422.562988	8.210970
5.890389	427.579689	8.215987
6.186114	442.645071	8.221005
5.728766	452.006580	8.226022
6.050105	439.412552	8.231040
6.110283	443.460619	8.236058
5.760982	447.745007	8.241075
6.029509	463.885165	8.246093
5.984316	459.399868	8.251110
6.196688	424.928222	8.256128
5.971449	415.158784	8.261146
5.528565	422.354736	8.266163
6.147159	435.901433	8.271181
6.118975	460.753073	8.276198
6.280745	450.073542	8.281216
5.809265	448.673965	8.286234
6.031196	439.535331	8.291251
6.057330	428.592290	8.296269
5.921148	429.140561	8.301286
5.994950	426.561821	8.306304
5.863798	437.962902	8.311322
5.570861	458.141251	8.316339
6.055643	468.342066	8.321357
5.952523	447.783188	8.326374
6.222208	433.819852	8.331392
6.162394	445.116263	8.336410
6.007600	454.753370	8.341427
6.266967	458.014902	8.346445
5.986149	461.424053	8.351462
6.429814	447.919410	8.356480
6.358859	462.399728	8.361498
5.907477	466.225341	8.366515
6.219114	465.464039	8.371533
5.767384	445.608749	8.376550
6.102370	449.287285	8.381568
5.996790	470.042780	8.386586
6.071036	468.065361	8.391603
6.312896	454.533351	8.396621
6.208910	455.991393	8.401638
6.056773	460.327134	8.406656
6.090798	469.917304	8.411674
6.047772	462.149817	8.416691
6.454430	458.209945	8.421709
6.256710	453.888988	8.426726
6.450968	448.136624	8.431744
6.234648	449.699227	8.436762
5.984501	455.372239	8.441779
6.614161	454.703518	8.446797
6.079070	440.425661	8.451814
5.924812	409.432743	8.456832
6.046291	430.813854	8.461850
5.953102	448.402542	8.466867
6.135422	458.508790	8.471885
5.988527	459.361009	8.476902
6.108523	446.358643	8.481920
6.036902	465.033530	8.486938
5.906270	475.647378	8.491955
6.254383	444.147476	8.496973
6.309580	450.964071	8.501990
6.260016	464.250451	8.507008
6.105421	470.399761	8.512026
5.991649	469.165708	8.517043
6.350935	464.375643	8.522061
6.122703	457.867249	8.527078
6.001506	452.911286	8.532096
6.244352	445.849498	8.537114
6.454788	457.949241	8.542131
6.877154	448.050327	8.547149
6.271921	464.236876	8.552166
6.181360	455.545921	8.557184
6.259741	448.259316	8.562202
6.318387	453.991404	8.567219
6.306284	471.041082	8.572237
6.055071	463.039276	8.577255
6.516938	451.580638	8.582272
6.469081	453.998317	8.587290
6.282857	460.290408	8.592307
6.402068	442.423143	8.597325
6.256439	468.114536	8.602343
6.348810	449.825639	8.607360
6.561502	445.129962	8.612378
6.299779	450.184887	8.617395
6.422180	456.471729	8.622413
6.201101	444.222478	8.627431
6.342707	451.671260	8.632448
6.392075	464.453932	8.637466
6.198539	465.578055	8.642483
6.276930	445.854682	8.647501
6.135630	450.652177	8.652519
6.402675	470.313027	8.657536
6.504442	488.434145	8.662554
6.291721	490.276294	8.667571
6.483114	475.487318	8.672589
6.441961	484.310715	8.677607
6.267152	489.552414	8.682624
6.664996	486.227792	8.687642
6.407473	482.370714	8.692659
6.574435	472.107809	8.697677
6.331269	497.463108	8.702695
6.351539	496.040808	8.707712
6.794052	474.091507	8.712730
6.490496	492.200401	8.717747
6.622042	478.898744	8.722765
6.437338	476.833544	8.727783
6.412898	473.714203	8.732800
6.794718	461.541337	8.737818
6.278475	474.130267	8.742835
6.641027	487.646706	8.747853
6.544282	490.554418	8.752871
6.475190	478.641140	8.757888
6.663489	461.213585	8.762906
6.569752	471.350997	8.767923
6.563306	462.309424	8.772941
6.279624	454.446906	8.777959
6.571606	457.985743	8.782976
6.659024	469.815456	8.787994
6.447577	484.699807	8.793011
6.633575	468.846189	8.798029
6.457469	478.281773	8.803047
6.524385	485.500662	8.808064
6.666478	480.108084	8.813082
6.798374	479.973755	8.818099
6.587683	490.525865	8.823117
6.533532	481.456250	8.828135
6.697066	472.565072	8.833152
6.533909	473.529200	8.838170
6.424695	470.485170	8.843187
6.732535	480.257197	8.848205
6.485950	503.147440	8.853223
6.207882	503.343973	8.858240
6.557950	486.084287	8.863258
6.662749	484.640344	8.868275
6.485926	488.154327	8.873293
6.561092	481.598244	8.878311
6.612046	485.606224	8.883328
6.757499	490.094707	8.888346
6.665070	503.665193	8.893363
6.677681	485.179160	8.898381
6.442342	473.192994	8.903399
6.379356	498.852676	8.908416
6.680587	477.228797	8.913434
6.283141	489.158626	8.918451
6.504507	508.589445	8.923469
6.716223	528.943865	8.928487
7.000864	525.130804	8.933504
7.122414	521.878893	8.938522
6.748030	522.435045	8.943539
6.761257	497.601980	8.948557
6.724670	483.581664	8.953575
6.724109	478.682999	8.958592
6.864144	497.751368	8.963610
6.661889	507.943833	8.968627
6.689878	499.923419	8.973645
7.329623	520.610917	8.978663
6.620965	512.569457	8.983680
6.720765	481.111301	8.988698
6.684201	481.708251	8.993715
6.463636	502.762830	8.998733
6.968672	514.451635	9.003751
6.672014	523.701126	9.008768
6.553671	502.634697	9.013786
6.577735	504.065973	9.018803
6.639130	506.907212	9.023821
7.052036	518.668218	9.028839
7.070911	522.546213	9.033856
7.224814	512.001957	9.038874
6.911804	515.766635	9.043891
7.034079	506.636854	9.048909
7.372766	498.341932	9.053927
6.844453	515.518686	9.058944
7.067131	509.072133	9.063962
7.205352	494.576491	9.068979
6.917837	484.875452	9.073997
6.962282	490.465651	9.079015
6.698305	483.962758	9.084032
7.058297	466.957384	9.089050
6.858289	484.577049	9.094067
6.622948	477.371006	9.099085
6.740762	493.793804	9.104103
6.827034	508.316962	9.109120
6.977765	495.888641	9.114138
6.816461	520.483814	9.119155
6.833439	531.058252	9.124173
7.182010	503.963202	9.129191
6.992850	520.753990	9.134208
7.271376	505.182990	9.139226
6.924717	506.734470	9.144243
6.974787	499.979436	9.149261
7.101332	505.403851	9.154279
7.024557	509.908204	9.159296
6.978854	516.706768	9.164314
6.950438	519.929184	9.169331
6.937076	510.217853	9.174349
6.954924	501.635692	9.179367
7.058480	507.171456	9.184384
7.269021	494.906333	9.189402
7.184371	509.432252	9.194419
7.120910	523.388113	9.199437
7.233085	522.553896	9.204455
7.013345	522.288163	9.209472
6.915497	504.889446	9.214490
7.035960	509.654624	9.219507
7.280975	510.456545	9.224525
7.045137	514.513402	9.229543
7.063124	512.091664	9.234560
7.264635	493.759883	9.239578
6.889566	514.146901	9.244595
6.873358	521.170646	9.249613
6.826438	510.701101	9.254631
6.934723	498.559732	9.259648
7.304373	505.784393	9.264666
7.173454	521.290527	9.269683
6.970667	516.045259	9.274701
7.360369	501.486404	9.279719
7.170586	498.835594	9.284736
7.168991	512.704275	9.289754
6.909207	508.448366	9.294771
6.968387	513.372547	9.299789
7.459149	511.334065	9.304807
6.884786	520.242450	9.309824
7.032529	497.370057	9.314842
7.059376	503.184758	9.319859
7.444860	513.812822	9.324877
7.330062	514.449366	9.329895
7.118893	521.902559	9.334912
7.082327	503.709195	9.339930
7.128247	517.575735	9.344947
7.212957	545.931476	9.349965
7.475223	547.034203	9.354983
7.126724	537.994205	9.360000
7.595333	534.800457	9.365018
7.391696	529.885251	9.370035
6.789149	535.947242	9.375053
7.000502	532.644180	9.380071
7.166725	536.879019	9.385088
7.051001	540.831117	9.390106
7.100281	535.590729	9.395123
7.266627	553.656678	9.400141
7.383130	529.383104	9.405159
7.036943	531.173811	9.410176
7.470920	545.731841	9.415194
7.457943	548.177422	9.420211
7.368868	549.339981	9.425229
7.379702	555.525650	9.430247
7.143957	552.752738	9.435264
7.448415	540.894871	9.440282
7.388094	537.350761	9.445299
7.336131	549.493153	9.450317
7.542893	540.087358	9.455335
7.550904	541.950893	9.460352
7.182439	526.529987	9.465370
7.448258	535.309867	9.470387
7.463427	561.366662	9.475405
7.887455	547.042772	9.480423
7.595815	536.900774	9.485440
7.183936	547.760404	9.490458
7.563423	542.947593	9.495475
7.724639	541.710598	9.500493
7.712416	546.198783	9.505511
7.764641	551.150005	9.510528
7.770296	534.922593	9.515546
7.983383	526.764324	9.520563
7.505083	531.550330	9.525581
7.669177	534.552111	9.530599
7.132580	533.382023	9.535616
7.353501	529.279772	9.540634
7.481167	537.783751	9.545651
7.673147	531.663726	9.550669
7.807873	539.346299	9.555687
7.780619	548.134472	9.560704
7.369252	548.661313	9.565722
7.506730	531.469966	9.570739
7.459891	526.611109	9.575757
7.927356	530.247600	9.580775
7.832664	551.705439	9.585792
7.651268	544.308218	9.590810
7.499506	506.665096	9.595827
7.477288	507.186075	9.600845
7.684650	533.184198	9.605863
7.676485	540.762666	9.610880
7.430497	528.344087	9.615898
7.736059	517.043378	9.620915
7.653097	540.478818	9.625933
7.540720	556.878521	9.630951
7.687390	544.233373	9.635968
7.782787	541.426797	9.640986
7.654535	545.885352	9.646003
7.411280	542.067325	9.651021
7.717178	549.369452	9.656039
7.513051	540.419441	9.661056
7.510065	559.262577	9.666074
7.849729	544.391863	9.671091
7.465626	543.108115	9.676109
7.615262	537.118869	9.681127
7.508982	533.450010	9.686144
7.760625	533.447620	9.691162
7.676395	552.432779	9.696179
7.661490	552.704786	9.701197
7.945806	544.926554	9.706215
7.724622	558.952496	9.711232
7.632220	552.413546	9.716250
7.881250	528.656503	9.721267
7.667047	546.440055	9.726285
7.816750	540.987259	9.731303
7.942563	536.372625	9.736320
7.868507	537.074858	9.741338
7.842052	539.874239	9.746355
7.445614	556.962238	9.751373
7.628815	553.630664	9.756391
7.558458	537.898646	9.761408
7.292315	537.863254	9.766426
7.829346	550.769978	9.771443
7.466377	563.653739	9.776461
7.867935	569.995058	9.781479
7.938042	587.031868	9.786496
7.854594	573.934509	9.791514
8.001266	557.783151	9.796531
7.785880	581.499419	9.801549
8.009970	590.117377	9.806567
8.036381	582.258258	9.811584
7.943253	570.129652	9.816602
7.974425	582.450205	9.821619
7.818908	595.728429	9.826637
7.962533	575.274823	9.831655
7.861793	575.954113	9.836672
7.829866	582.902256	9.841690
7.945386	576.683759	9.846707
7.650351	578.693710	9.851725
8.127159	567.857342	9.856743
8.223802	592.787456	9.861760
7.958084	586.052883	9.866778
7.976536	569.547907	9.871795
8.165622	573.865273	9.876813
8.007262	583.168202	9.881831
8.294752	588.101613	9.886848
8.076266	570.644238	9.891866
7.961384	566.629843	9.896883
8.092175	584.416448	9.901901
8.420784	576.740891	9.906919
8.091378	563.296794	9.911936
7.894867	558.413660	9.916954
8.024080	550.240605	9.921971
8.001434	565.108200	9.926989
8.066183	566.053071	9.932007
8.288280	557.941216	9.937024
7.808522	563.023945	9.942042
8.119918	554.033306	9.947059
7.768517	564.041361	9.952077
7.983069	578.192402	9.957095
8.070962	587.391959	9.962112
7.856966	576.192615	9.967130
8.265955	578.922504	9.972147
8.240945	582.399415	9.977165
8.525726	559.265572	9.982183
8.105788	568.954341	9.987200
7.755246	593.587200	9.992218
8.347629	562.765680	9.997235
8.216404	568.223860	10.002253
8.197524	576.110723	10.007271
8.207628	597.736787	10.012288
8.033076	589.207133	10.017306
8.190268	568.265309	10.022323
7.869708	561.487071	10.027341
7.888852	565.913303	10.032359
8.034032	582.921566	10.037376
7.804688	580.322837	10.042394
8.009513	579.268050	10.047411
8.189255	593.920093	10.052429
8.461790	593.800700	10.057447
8.417299	583.154768	10.062464
8.180419	578.595534	10.067482
8.430282	588.937682	10.072499
8.022431	578.719417	10.077517
8.290425	604.272527	10.082535
8.416261	615.869886	10.087552
8.124808	613.726075	10.092570
8.542946	594.630231	10.097587
8.566338	603.450508	10.102605
8.765723	582.925882	10.107623
8.543960	592.094749	10.112640
8.420150	587.271913	10.117658
8.147043	558.924567	10.122675
8.068036	567.765091	10.127693
8.008485	585.989240	10.132711
8.280853	589.626893	10.137728
8.084603	587.851497	10.142746
8.692139	603.514639	10.147763
8.400128	620.053512	10.152781
8.446305	611.233800	10.157799
8.419378	631.630354	10.162816
8.300174	626.837246	10.167834
8.536026	601.070918	10.172851
8.494543	624.728209	10.177869
8.303436	640.325590	10.182887
8.786784	624.679883	10.187904
8.452492	606.533138	10.192922
8.188342	609.845991	10.197939
8.085736	615.263642	10.202957
8.419668	613.856997	10.207975
8.383725	613.194062	10.212992
8.463922	614.624141	10.218010
8.805975	619.390519	10.223027
8.557579	621.766877	10.228045
8.216956	616.079423	10.233063
8.763550	610.043638	10.238080
8.359633	618.709602	10.243098
8.549968	623.365067	10.248115
8.755520	620.573237	10.253133
8.420418	620.536252	10.258151
8.517802	628.734840	10.263168
8.479171	616.854993	10.268186
8.681137	616.629380	10.273203
8.618324	626.417096	10.278221
8.367605	616.067749	10.283239
8.748697	632.717488	10.288256
8.249030	637.383273	10.293274
8.688546	617.751730	10.298291
8.310478	620.063910	10.303309
8.040294	637.296739	10.308327
8.501166	647.741619	10.313344
8.750049	646.506955	10.318362
8.740868	634.282753	10.323379
8.694410	651.782183	10.328397
8.847862	665.176193	10.333415
8.990580	647.054184	10.338432
9.141677	647.454819	10.343450
9.419594	648.102139	10.348467
9.096880	636.300217	10.353485
8.689780	629.402821	10.358503
8.978099	604.095109	10.363520
8.646766	617.139782	10.368538
9.278421	623.338600	10.373555
9.004043	624.626150	10.378573
8.576951	614.572215	10.383591
8.864551	606.918473	10.388608
8.916199	610.195473	10.393626
9.101378	609.603250	10.398643
9.136356	617.750548	10.403661
8.823950	618.364551	10.408679
8.902618	613.192488	10.413696
8.922018	619.461290	10.418714
8.799772	609.720069	10.423731
8.800635	611.583712	10.428749
8.552829	629.949525	10.433767
8.940936	608.576680	10.438784
8.931449	622.935703	10.443802
8.589908	622.780229	10.448819
8.736953	616.576185	10.453837
8.778578	630.579817	10.458855
8.885082	624.006195	10.463872
8.664220	625.756719	10.468890
8.674442	623.950348	10.473907
8.599814	614.371779	10.478925
8.567824	623.326381	10.483943
8.831887	628.399368	10.488960
9.035305	624.381851	10.493978
8.690623	615.287649	10.498995
9.118146	625.295825	10.504013
8.728290	642.281581	10.509031
9.223968	648.091577	10.514048
8.995326	648.886173	10.519066
8.961744	638.275104	10.524083
8.743658	630.085501	10.529101
8.988475	652.214931	10.534119
8.983481	639.062141	10.539136
8.978476	656.186815	10.544154
9.119593	652.594433	10.549171
9.242745	650.420969	10.554189
9.071688	652.520844	10.559207
9.338031	647.769205	10.564224
8.812886	645.484924	10.569242
9.307884	649.140412	10.574259
9.228767	635.531203	10.579277
8.900340	654.366246	10.584295
9.103419	653.091625	10.589312
9.436980	657.028939	10.594330
8.986624	646.545088	10.599347
9.344473	649.675753	10.604365
9.286958	646.020752	10.609383
9.116966	635.359314	10.614400
9.048486	633.346028	10.619418
8.970422	645.535415	10.624435
9.501361	639.331486	10.629453
8.816280	660.855063	10.634471
9.461193	648.876990	10.639488
8.914750	640.636459	10.644506
9.130123	634.113917	10.649523
9.368543	641.726763	10.654541
8.887219	661.600876	10.659559
9.480512	646.608743	10.664576
9.102730	648.164790	10.669594
9.405230	654.249066	10.674611
9.537938	652.251040	10.679629
9.347682	644.577948	10.684647
9.325969	655.162999	10.689664
9.272668	656.590347	10.694682
9.107084	641.479699	10.699699
9.431254	642.124393	10.704717
9.030736	652.009949	10.709735
9.264616	637.196085	10.714752
9.476868	642.410673	10.719770
8.837652	655.919234	10.724787
9.289778	647.446081	10.729805
9.311239	650.590911	10.734823
9.334130	660.806392	10.739840
9.258798	647.832789	10.744858
9.025379	638.028152	10.749875
9.219287	648.738743	10.754893
9.140312	660.397632	10.759911
9.186050	648.419785	10.764928
9.725315	664.642152	10.769946
9.365021	662.316161	10.774963
9.795747	633.710571	10.779981
9.457343	648.866485	10.784999
9.507919	651.218925	10.790016
9.367008	654.787035	10.795034
9.182227	635.952049	10.800051
9.835152	647.513987	10.805069
9.196936	657.594985	10.810087
9.543859	648.613673	10.815104
9.751626	639.918182	10.820122
9.579733	645.832002	10.825139
9.527321	649.735684	10.830157
9.364730	663.216851	10.835175
9.068139	646.239391	10.840192
9.530730	670.009952	10.845210
9.364528	680.361390	10.850227
9.898586	669.115403	10.855245
9.802146	676.018065	10.860263
9.840602	665.518956	10.865280
9.762792	676.685772	10.870298
9.627592	683.386633	10.875315
9.655776	654.366260	10.880333
9.267798	649.709172	10.885351
9.550665	673.437707	10.890368
9.903601	675.095677	10.895386
9.679772	675.605601	10.900403
9.966746	675.909787	10.905421
9.735954	678.049647	10.910439
9.735174	645.133574	10.915456
9.709413	653.888992	10.920474
9.467100	643.542369	10.925491
9.707002	664.202069	10.930509
9.667479	692.216309	10.935527
9.880641	681.081791	10.940544
9.678577	678.875869	10.945562
9.679825	691.940723	10.950579
9.671422	674.078139	10.955597
10.064312	667.123011	10.960615
9.876110	688.827239	10.965632
9.927831	688.490960	10.970650
9.514991	665.758875	10.975667
9.606689	667.284276	10.980685
9.774407	676.904141	10.985703
9.803855	675.592481	10.990720
9.918374	688.092109	10.995738
9.849192	690.328262	11.000755
9.792611	666.144573	11.005773
9.803925	684.664722	11.010791
9.874100	696.502577	11.015808
9.796994	682.394410	11.020826
9.752319	676.167413	11.025843
9.714056	685.072315	11.030861
9.942932	697.909255	11.035879
9.994857	683.566240	11.040896
10.039360	670.273881	11.045914
9.925604	673.471663	11.050931
9.969012	691.782439	11.055949
9.998632	688.299000	11.060967
10.150941	675.077675	11.065984
10.154352	671.168572	11.071002
9.812726	690.250261	11.076019
10.052815	675.904300	11.081037
10.129518	685.179368	11.086055
10.068582	696.900345	11.091072
10.283269	670.077157	11.096090
10.163674	673.519045	11.101107
9.982598	678.694343	11.106125
10.161926	696.206596	11.111143
10.127128	675.332857	11.116160
10.138268	658.439039	11.121178
10.013928	671.938394	11.126195
9.993957	658.542361	11.131213
10.176579	675.205559	11.136231
9.940780	682.382760	11.141248
10.245165	670.641997	11.146266
10.026473	663.049657	11.151283
10.158105	677.653251	11.156301
10.037317	701.060453	11.161319
10.173962	695.008251	11.166336
10.179311	672.235780	11.171354
9.687122	681.173973	11.176371
9.942188	692.873623	11.181389
9.925569	699.882364	11.186407
9.721718	682.226727	11.191424
9.904302	667.410979	11.196442
9.535621	672.377775	11.201459
10.088268	697.311718	11.206477
10.376009	706.968445	11.211495
10.263479	705.121440	11.216512
10.692897	691.878119	11.221530
10.080531	703.561228	11.226547
10.300234	709.910518	11.231565
10.264505	701.915289	11.236583
10.056339	706.724012	11.241600
10.476319	714.788649	11.246618
10.341505	692.234338	11.251635
10.310364	693.531880	11.256653
10.339456	720.154895	11.261671
10.090804	729.287747	11.266688
10.303090	696.545647	11.271706
10.425983	701.774038	11.276723
10.398007	719.300305	11.281741
10.390467	719.561061	11.286759
10.032888	715.668405	11.291776
10.486842	703.473490	11.296794
10.167956	705.301524	11.301811
10.501826	705.905948	11.306829
10.619515	715.197779	11.311847
10.619345	723.085561	11.316864
10.771643	711.154703	11.321882
10.428102	714.661062	11.326899
10.291789	700.112392	11.331917
10.327867	711.372292	11.336935
10.006017	718.645893	11.341952
10.252771	714.907433	11.346970
10.098342	704.873125	11.351987
10.531297	693.277982	11.357005
10.328593	709.879535	11.362023
10.058728	724.394152	11.367040
10.404048	720.710642	11.372058
10.661922	747.906756	11.377075
10.668489	744.632177	11.382093
10.815216	741.779789	11.387111
10.463513	742.362506	11.392128
10.686963	731.886998	11.397146
10.667575	718.881064	11.402163
10.725585	723.031898	11.407181
10.900338	730.912720	11.412199
10.330488	714.170841	11.417216
10.536316	686.117336	11.422234
10.543173	707.887263	11.427251
10.625891	740.858482	11.432269
10.822190	734.251377	11.437287
10.837955	741.248684	11.442304
10.836129	718.517478	11.447322
10.509223	711.470609	11.452339
10.699638	708.362551	11.457357
11.015650	712.136683	11.462375
10.433945	727.691248	11.467392
11.103803	729.532516	11.472410
10.622452	723.000107	11.477427
10.638072	729.262200	11.482445
11.120885	712.206442	11.487463
10.381238	722.743692	11.492480
10.296892	726.613016	11.497498
10.732137	737.988616	11.502515
10.977272	739.571913	11.507533
11.108166	749.241893	11.512551
10.801885	738.976525	11.517568
11.338378	725.959411	11.522586
11.108986	734.895337	11.527603
10.396687	710.366518	11.532621
10.888626	717.707844	11.537639
10.940510	730.504001	11.542656
11.105269	747.157044	11.547674
11.024697	759.322632	11.552691
10.631636	716.493602	11.557709
10.918690	710.944642	11.562727
10.682951	746.063107	11.567744
11.164672	729.388412	11.572762
11.349258	740.847256	11.577779
10.861355	733.410264	11.582797
11.419234	727.808081	11.587815
10.724853	740.794579	11.592832
10.974797	736.683935	11.597850
10.932477	726.570178	11.602867
11.309982	721.587507	11.607885
10.859109	713.470868	11.612903
10.993948	730.224382	11.617920
11.062014	726.784273	11.622938
11.290413	722.826758	11.627955
10.866297	733.738528	11.632973
11.301389	756.497411	11.637991
11.059448	740.805347	11.643008
11.120326	724.047589	11.648026
11.170988	723.721816	11.653043
11.073469	737.674644	11.658061
11.108553	745.662784	11.663079
11.267825	742.598931	11.668096
11.067485	720.257615	11.673114
11.218307	741.782796	11.678131
11.162529	755.244818	11.683149
10.993616	744.218264	11.688167
10.814664	753.499608	11.693184
11.046640	734.884921	11.698202
11.099044	730.646435	11.703219
11.209096	742.589910	11.708237
11.346018	738.985803	11.713255
11.001803	737.777117	11.718272
11.152142	739.008364	11.723290
11.134447	754.974339	11.728307
10.946955	742.472711	11.733325
11.347895	726.192172	11.738343
10.953929	731.877736	11.743360
10.869103	750.488537	11.748378
11.431424	756.950080	11.753395
11.421521	760.153940	11.758413
11.583989	751.610715	11.763431
11.161026	748.031234	11.768448
11.568829	759.579253	11.773466
11.508862	751.036478	11.778483
11.506465	728.214136	11.783501
11.274606	746.940249	11.788519
11.008431	758.730023	11.793536
11.516270	750.265515	11.798554
11.666542	750.325830	11.803571
11.369765	762.291583	11.808589
11.635246	747.702544	11.813607
11.267667	744.942134	11.818624
11.397425	768.756240	11.823642
11.751576	762.210120	11.828659
11.195042	752.682171	11.833677
11.412345	749.291883	11.838695
11.343919	777.457866	11.843712
11.742549	776.145999	11.848730
11.986185	764.713550	11.853747
11.467941	772.664044	11.858765
11.609643	766.278882	11.863783
11.274946	759.248629	11.868800
11.468751	753.235173	11.873818
11.715473	767.069052	11.878835
11.673402	765.178712	11.883853
11.724414	758.271578	11.888871
11.579684	771.763566	11.893888
11.680905	784.665265	11.898906
11.827154	761.195838	11.903923
11.452654	758.408525	11.908941
11.806532	762.786287	11.913959
11.992476	774.100679	11.918976
11.581234	767.414872	11.923994
11.919372	768.247272	11.929011
11.654393	757.517709	11.934029
11.932296	756.917340	11.939047
11.653419	752.911400	11.944064
11.749596	761.031933	11.949082
12.029931	747.828158	11.954099
11.530013	737.887231	11.959117
11.770251	766.642761	11.964135
11.622749	755.985099	11.969152
11.724482	749.951929	11.974170
11.924734	764.433863	11.979187
11.963175	764.469658	11.984205
11.886557	765.548307	11.989223
12.102803	765.990035	11.994240
11.804603	764.502752	11.999258
11.924472	769.216548	12.004275
11.733415	774.539157	12.009293
11.696545	750.751675	12.014311
11.852580	747.815290	12.019328
11.808413	769.167866	12.024346
11.912421	758.415111	12.029363
11.905150	755.400227	12.034381
11.962262	754.221944	12.039399
11.728763	777.025319	12.044416
11.567452	765.627710	12.049434
11.689033	750.865750	12.054451
11.789662	751.284469	12.059469
11.980868	754.307594	12.064487
11.857770	760.508689	12.069504
11.788210	755.032815	12.074522
12.144193	764.824227	12.079539
11.981506	766.342182	12.084557
11.912311	758.402734	12.089575
12.373686	795.814323	12.094592
12.172936	778.234813	12.099610
12.558555	755.228754	12.104627
11.935289	762.709820	12.109645
12.060153	783.747652	12.114663
11.931708	778.936738	12.119680
11.843039	765.782808	12.124698
12.570755	770.753245	12.129715
11.985571	766.724809	12.134733
12.270336	749.676352	12.139751
11.966481	760.260869	12.144768
11.900071	789.512372	12.149786
12.335465	784.423389	12.154803
12.277549	784.558845	12.159821
12.514841	799.303714	12.164839
12.266750	796.432725	12.169856
12.228091	786.185878	12.174874
12.201817	788.072329	12.179891
12.316101	806.347029	12.184909
12.765523	778.730236	12.189927
12.690991	761.994616	12.194944
12.120916	754.821421	12.199962
12.319797	762.462411	12.204979
12.162164	751.225775	12.209997
12.285283	760.573217	12.215015
12.262820	786.629727	12.220032
12.262093	778.478909	12.225050
12.478933	764.324551	12.230067
12.185163	780.014313	12.235085
12.200246	789.319406	12.240103
12.285942	787.199245	12.245120
12.316496	773.063757	12.250138
12.837785	780.859491	12.255155
12.433994	797.602510	12.260173
12.372421	785.760861	12.265191
12.447888	793.405729	12.270208
12.451322	793.921002	12.275226
12.477838	766.153903	12.280243
12.516193	771.097254	12.285261
12.496328	780.156511	12.290279
12.604390	785.561450	12.295296
12.345308	787.874459	12.300314
12.454356	786.686705	12.305331
12.389837	798.101839	12.310349
12.470903	774.646705	12.315367
12.620245	790.770202	12.320384
12.619490	800.818765	12.325402
12.775050	781.082110	12.330419
12.465203	769.843948	12.335437
12.611406	787.219988	12.340455
12.781056	794.554883	12.345472
12.625625	785.397423	12.350490
12.705008	762.261792	12.355507
12.497047	783.638602	12.360525
12.631445	792.780318	12.365543
12.612509	789.602144	12.370560
12.649785	779.933835	12.375578
12.738359	787.151943	12.380595
12.697363	796.691937	12.385613
13.044150	802.260723	12.390631
13.023742	780.606717	12.395648
12.721785	784.171556	12.400666
12.838715	773.591313	12.405683
12.604510	783.764640	12.410701
12.484472	790.423978	12.415719
12.886306	811.019134	12.420736
12.890494	811.349096	12.425754
13.322687	814.936186	12.430771
13.274606	793.798606	12.435789
12.863034	772.955510	12.440807
13.193815	780.796207	12.445824
12.785961	799.871954	12.450842
13.030797	770.377290	12.455859
12.642256	778.029262	12.460877
12.779005	791.890783	12.465895
13.011750	776.574547	12.470912
12.714615	793.220429	12.475930
12.981408	799.901649	12.480947
13.220470	804.319849	12.485965
12.923491	783.778090	12.490983
13.485545	790.653656	12.496000
13.212893	810.659674	12.501018
12.854289	794.931041	12.506035
12.623201	795.284336	12.511053
13.366043	811.427757	12.516071
13.419027	795.481836	12.521088
13.148509	768.294386	12.526106
13.290236	775.569141	12.531123
13.042572	792.435920	12.536141
12.853015	789.430982	12.541159
12.803434	780.761212	12.546176
12.844834	809.442329	12.551194
13.158766	799.808681	12.556211
12.934945	811.450097	12.561229
12.999129	822.173587	12.566247
13.221436	828.407665	12.571264
12.922194	815.433924	12.576282
12.998961	811.553105	12.581299
13.319265	815.201094	12.586317
13.523357	804.118760	12.591335
13.521786	806.484172	12.596352
13.397070	821.824078	12.601370
13.408938	804.783068	12.606387
13.507385	798.952730	12.611405
13.322377	822.820709	12.616423
13.626117	798.687866	12.621440
13.366960	821.817411	12.626458
13.791395	820.278304	12.631475
13.568360	825.310526	12.636493
13.341408	807.290646	12.641511
13.499794	807.482853	12.646528
13.557032	810.893189	12.651546
13.865468	808.633684	12.656563
13.364521	805.340725	12.661581
13.177873	804.298856	12.666599
13.312401	809.103820	12.671616
13.191339	822.410592	12.676634
13.369715	808.879413	12.681651
13.324040	800.980828	12.686669
13.114576	795.009497	12.691687
13.358562	808.532826	12.696704
13.283850	829.657624	12.701722
13.701181	813.396719	12.706739
13.749474	825.262397	12.711757
13.359605	826.324330	12.716775
13.230344	806.183452	12.721792
13.424931	794.848431	12.726810
13.780523	820.845279	12.731827
13.779649	818.014120	12.736845
13.345241	805.327811	12.741863
13.891354	812.150623	12.746880
13.782361	825.008671	12.751898
14.032612	823.626366	12.756915
13.882134	811.740151	12.761933
13.522885	805.907809	12.766951
13.772024	800.474404	12.771968
13.795422	817.888189	12.776986
13.750363	816.700513	12.782003
14.009255	816.878571	12.787021
13.629653	796.648105	12.792039
13.744027	801.727191	12.797056
13.704787	822.622654	12.802074
13.792708	817.132836	12.807091
13.770712	805.211225	12.812109
13.616284	787.842593	12.817127
13.824676	822.168739	12.822144
14.230408	839.411815	12.827162
13.715255	818.777751	12.832179
14.070070	820.469178	12.837197
14.034655	818.367452	12.842215
13.856883	813.114504	12.847232
13.681326	811.832184	12.852250
13.869547	841.361406	12.857267
14.083076	841.464206	12.862285
14.072215	844.525858	12.867303
14.242233	837.606895	12.872320
13.964712	826.762555	12.877338
13.904888	825.010243	12.882355
14.180810	843.345654	12.887373
14.198875	825.198082	12.892391
14.298434	793.154341	12.897408
13.926644	811.418944	12.902426
13.932227	814.094805	12.907443
13.968385	804.209892	12.912461
13.949318	833.402488	12.917479
14.311603	843.845395	12.922496
14.422892	838.628505	12.927514
14.128696	832.978560	12.932531
14.612152	837.581520	12.937549
14.205079	828.072612	12.942567
13.898655	822.793984	12.947584
14.214849	818.337124	12.952602
13.983204	830.043315	12.957619
14.223703	834.199347	12.962637
14.047192	837.865779	12.967655
14.492384	842.148279	12.972672
14.329106	849.337681	12.977690
14.306301	830.040074	12.982707
14.558484	844.206595	12.987725
14.448899	831.841093	12.992743
14.781022	829.054779	12.997760
14.236547	825.768024	13.002778
14.217079	823.395820	13.007795
14.494157	799.205391	13.012813
14.465294	805.015244	13.017831
14.059878	808.924068	13.022848
14.307539	826.438856	13.027866
14.446091	830.242934	13.032883
14.511233	816.263458	13.037901
14.447344	841.375781	13.042919
14.433180	851.990913	13.047936
14.399116	835.737570	13.052954
14.052291	821.909217	13.057971
14.262663	835.715807	13.062989
14.065767	854.340236	13.068007
14.358390	837.815146	13.073024
14.352685	824.145914	13.078042
14.348406	829.020759	13.083059
14.476150	838.052902	13.088077
14.226994	846.984582	13.093095
14.551116	848.991633	13.098112
14.754142	858.639726	13.103130
14.454934	868.864983	13.108147
14.871560	857.499127	13.113165
14.600965	856.864430	13.118183
14.771194	852.174859	13.123200
14.820175	853.761950	13.128218
14.921932	868.403234	13.133235
14.909878	855.433856	13.138253
14.531856	835.992633	13.143271
14.605895	839.431391	13.148288
14.955664	855.142113	13.153306
14.947290	870.363852	13.158323
14.887220	838.721691	13.163341
14.580871	823.133272	13.168359
14.808180	848.549066	13.173376
14.845385	857.465803	13.178394
14.752400	866.457393	13.183411
15.250015	844.193320	13.188429
14.800317	843.838548	13.193447
14.999197	857.856648	13.198464
15.051887	861.468285	13.203482
14.919050	848.018512	13.208499
14.862242	818.441944	13.213517
14.646091	830.244663	13.218535
15.348279	856.711223	13.223552
15.218125	850.981224	13.228570
14.679342	825.054319	13.233587
15.219679	834.899344	13.238605
15.020515	844.854183	13.243623
14.959524	851.878493	13.248640
14.970645	838.518394	13.253658
14.975903	832.128594	13.258675
14.959464	854.791912	13.263693
15.192727	859.719220	13.268711
15.053717	846.383530	13.273728
15.030567	840.351478	13.278746
14.646838	837.838438	13.283763
15.194365	852.718558	13.288781
14.941583	864.912786	13.293799
15.132298	846.385568	13.298816
15.324989	834.104624	13.303834
15.220596	845.088802	13.308851
15.341360	851.636934	13.313869
15.116487	857.222474	13.318887
14.995974	842.619200	13.323904
15.269129	842.213952	13.328922
15.134798	856.192750	13.333939
15.142697	861.411073	13.338957
15.042782	860.833187	13.343975
15.097220	852.559858	13.348992
15.271457	852.628710	13.354010
15.389443	878.677222	13.359027
15.644174	879.747468	13.364045
15.424041	877.830648	13.369063
15.338647	853.658509	13.374080
15.721065	859.404845	13.379098
15.733514	863.145048	13.384115
15.614768	845.863638	13.389133
15.709559	844.938305	13.394151
15.600602	831.300889	13.399168
15.843467	844.299180	13.404186
15.609388	847.584285	13.409203
15.312052	839.044476	13.414221
15.423564	838.586335	13.419239
15.468369	859.243806	13.424256
15.273711	850.902418	13.429274
15.471338	844.840571	13.434291
15.716081	832.374105	13.439309
15.730866	851.689342	13.444327
15.749290	861.347771	13.449344
15.683014	848.346426	13.454362
15.523137	852.928571	13.459379
15.583836	844.725256	13.464397
15.682444	847.254289	13.469415
15.305444	851.427943	13.474432
15.802112	849.396117	13.479450
15.580926	867.551177	13.484467
15.753127	866.246512	13.489485
15.776922	869.361384	13.494503
15.953505	879.893354	13.499520
16.235149	858.027357	13.504538
15.662529	855.966284	13.509555
15.298180	848.935674	13.514573
15.787198	854.672362	13.519591
15.707663	860.485690	13.524608
16.002955	872.732427	13.529626
16.087005	875.975495	13.534643
16.064161	870.117252	13.539661
15.955276	871.342444	13.544679
16.035346	876.475636	13.549696
15.838704	853.938388	13.554714
16.042254	860.563961	13.559731
15.748527	880.320666	13.564749
15.427884	872.053320	13.569767
15.890160	858.420275	13.574784
16.125516	857.312109	13.579802
15.884988	885.659055	13.584819
16.133857	879.367229	13.589837
16.043022	863.119498	13.594855
16.038329	853.331438	13.599872
16.143882	862.220943	13.604890
16.000562	884.720774	13.609907
16.142876	867.538779	13.614925
16.179717	876.689385	13.619943
16.220973	870.548967	13.624960
16.140044	854.901223	13.629978
16.015473	881.168516	13.634995
16.337417	879.154244	13.640013
16.347760	875.255751	13.645031
16.330791	871.324970	13.650048
16.300426	854.881576	13.655066
16.079050	883.835823	13.660083
16.452181	875.304063	13.665101
16.452905	876.103571	13.670119
16.323534	876.512775	13.675136
16.578768	872.364419	13.680154
16.196363	882.493916	13.685171
16.627662	862.282566	13.690189
16.558196	860.166290	13.695207
16.441975	866.452982	13.700224
16.494114	847.646871	13.705242
16.458643	872.705547	13.710259
16.575816	877.689142	13.715277
16.587015	868.669799	13.720295
16.254696	850.693455	13.725312
16.478949	870.549442	13.730330
16.445542	862.538098	13.735347
16.255961	855.741035	13.740365
16.433426	855.063388	13.745383
16.364697	866.802708	13.750400
16.553287	866.788992	13.755418
16.361298	857.588231	13.760435
16.459019	858.275474	13.765453
16.532817	846.152715	13.770471
16.596107	869.384124	13.775488
16.614108	872.675694	13.780506
16.595515	873.118547	13.785523
16.545398	857.613504	13.790541
16.738251	868.024010	13.795559
16.856985	874.782374	13.800576
16.866602	854.462419	13.805594
16.578509	862.814575	13.810611
16.838821	878.368102	13.815629
16.806261	877.672419	13.820647
16.641780	875.531893	13.825664
17.039371	874.539398	13.830682
16.665767	863.368971	13.835699
16.641342	869.142593	13.840717
16.892347	899.434480	13.845735
16.495212	912.449835	13.850752
16.941875	890.622056	13.855770
16.856109	882.303394	13.860787
17.131237	886.877033	13.865805
17.346892	900.011527	13.870823
16.969293	891.707532	13.875840
17.361473	871.836898	13.880858
17.098974	858.610360	13.885875
17.078276	875.302850	13.890893
17.173157	866.914688	13.895911
17.134894	855.748088	13.900928
17.365576	842.290694	13.905946
17.022858	858.545762	13.910963
17.170018	851.543289	13.915981
17.234068	847.500333	13.920999
17.020938	868.101254	13.926016
17.108102	857.708008	13.931034
17.144721	840.754871	13.936051
17.263584	855.600545	13.941069
17.483656	870.963227	13.946087
17.120425	855.859738	13.951104
17.305377	836.831844	13.956122
17.357317	855.916695	13.961139
16.973851	861.280183	13.966157
17.115773	842.780122	13.971175
17.129460	859.299536	13.976192
17.096925	846.461174	13.981210
17.032477	846.935416	13.986227
17.152108	867.625009	13.991245
17.504785	868.108450	13.996263
17.254881	891.544955	14.001280
17.670096	875.638573	14.006298
17.588595	883.473753	14.011315
17.537968	868.739645	14.016333
17.539826	876.104375	14.021351
17.597511	892.218330	14.026368
17.509681	859.629779	14.031386
17.388853	849.006413	14.036403
17.312022	863.144962	14.041421
17.675147	867.548189	14.046439
17.362988	878.275659	14.051456
17.691765	883.751610	14.056474
17.807245	884.292257	14.061491
17.495180	862.703551	14.066509
17.507757	870.389945	14.071527
17.605474	868.218095	14.076544
17.643739	878.715753	14.081562
17.816306	897.566900	14.086579
17.604732	894.146692	14.091597
17.622919	869.124162	14.096615
17.813317	901.096006	14.101632
17.795367	882.723569	14.106650
17.607097	886.362042	14.111667
17.462827	890.230388	14.116685
17.599469	869.856851	14.121703
17.467490	878.039259	14.126720
17.459879	875.858245	14.131738
17.311176	880.073392	14.136755
17.292580	884.979550	14.141773
18.123006	889.185414	14.146791
17.873863	923.254413	14.151808
17.632168	909.404474	14.156826
17.929982	897.447653	14.161843
17.793617	898.257615	14.166861
18.253680	915.384544	14.171879
18.016243	924.708424	14.176896
18.081885	904.557150	14.181914
18.216139	907.234691	14.186931
17.921091	901.273230	14.191949
17.900676	884.087210	14.196967
17.731119	888.043275	14.201984
18.228381	909.332552	14.207002
18.256073	906.225171	14.212019
18.174226	902.797398	14.217037
18.342102	894.033277	14.222055
18.202546	907.005767	14.227072
18.105202	902.529153	14.232090
17.969454	881.699170	14.237107
17.774631	900.998826	14.242125
18.051168	913.316295	14.247143
18.153298	929.306046	14.252160
18.163138	914.382026	14.257178
18.209336	892.153811	14.262195
18.177948	913.255329	14.267213
17.882491	909.187832	14.272231
18.016448	915.500310	14.277248
17.945235	913.163703	14.282266
18.243205	900.970103	14.287283
18.256062	921.613750	14.292301
18.696084	913.359718	14.297319
18.654225	936.947790	14.302336
18.372957	909.787053	14.307354
18.451598	907.211172	14.312371
18.291518	906.363476	14.317389
18.445011	926.401067	14.322407
18.484205	928.482176	14.327424
18.646851	923.819814	14.332442
18.781319	921.076281	14.337459
18.384447	926.678068	14.342477
18.672281	933.666125	14.347495
18.981702	921.645965	14.352512
18.524792	894.931890	14.357530
18.832629	888.495114	14.362547
18.522581	901.436439	14.367565
18.774455	901.747218	14.372583
18.771956	904.880808	14.377600
18.445992	907.534231	14.382618
18.706063	901.476311	14.387635
18.435957	900.409556	14.392653
19.032642	914.413433	14.397671
19.154003	909.230672	14.402688
18.537529	904.791827	14.407706
18.655465	912.761738	14.412723
18.948573	918.767478	14.417741
19.188406	921.713327	14.422759
18.839411	909.245335	14.427776
18.652349	889.708920	14.432794
18.857385	896.954969	14.437811
18.870546	932.747309	14.442829
19.114314	919.217329	14.447847
18.949270	924.296875	14.452864
19.057231	917.755457	14.457882
18.930717	889.303074	14.462899
18.909685	910.324452	14.467917
19.289488	913.992154	14.472935
19.055849	913.737959	14.477952
18.927837	909.855334	14.482970
19.218635	903.115444	14.487987
19.148543	913.095737	14.493005
19.305101	912.879397	14.498023
19.090997	880.159248	14.503040
18.961134	885.133387	14.508058
19.193142	905.669555	14.513075
18.964685	931.649654	14.518093
19.100445	915.479451	14.523111
19.007482	927.938681	14.528128
19.113659	931.107847	14.533146
19.133508	920.451639	14.538163
19.129622	921.864843	14.543181
19.310319	907.374583	14.548199
19.292024	929.662727	14.553216
19.433134	931.828444	14.558234
19.262612	921.952714	14.563251
19.244601	920.556872	14.568269
19.137356	909.738257	14.573287
19.525303	928.145098	14.578304
19.205378	935.024194	14.583322
19.341676	911.989139	14.588339
19.140166	921.030478	14.593357
19.651095	920.026729	14.598375
19.677754	930.908033	14.603392
19.264852	925.116196	14.608410
19.407238	912.924977	14.613427
19.363247	928.911224	14.618445
19.895914	951.675923	14.623463
19.569379	945.314830	14.628480
19.516889	935.314495	14.633498
19.615146	931.052336	14.638515
20.041605	950.680378	14.643533
19.722662	935.364525	14.648551
19.742118	940.911589	14.653568
19.668123	929.408801	14.658586
19.586159	926.157866	14.663603
19.644511	947.315843	14.668621
19.812216	940.086862	14.673639
19.941006	953.912946	14.678656
19.796442	945.162149	14.683674
19.751171	949.710035	14.688691
19.777068	962.382268	14.693709
20.046593	963.984978	14.698727
19.929647	960.536621	14.703744
19.995342	968.019848	14.708762
20.000554	951.825326	14.713779
19.955553	935.893384	14.718797
19.916737	932.890764	14.723815
20.225330	945.700865	14.728832
19.951096	959.805312	14.733850
20.289331	931.525984	14.738867
20.083927	913.336713	14.743885
19.669454	922.029191	14.748903
20.041939	951.440109	14.753920
19.823042	951.464999	14.758938
20.029765	935.133973	14.763955
20.169818	962.793232	14.768973
20.142008	945.662780	14.773991
20.230449	926.009550	14.779008
19.946597	947.996714	14.784026
20.203123	958.782586	14.789043
19.922332	950.327260	14.794061
20.151644	939.589881	14.799079
19.864623	932.292779	14.804096
20.002795	943.688893	14.809114
20.422811	956.832862	14.814131
19.982559	945.967506	14.819149
20.286631	950.338007	14.824167
20.464841	961.916643	14.829184
20.630735	978.458658	14.834202
20.729015	962.693513	14.839219
20.487742	966.356803	14.844237
20.196933	953.647526	14.849255
20.290465	941.890429	14.854272
20.498741	947.098792	14.859290
20.647226	961.346716	14.864307
20.714761	967.317624	14.869325
20.657397	952.595962	14.874343
20.635285	937.026580	14.879360
20.564956	933.666169	14.884378
20.582741	941.108593	14.889395
20.374897	957.835445	14.894413
20.298232	973.950631	14.899431
20.811295	962.391740	14.904448
20.807740	969.994357	14.909466
20.879705	984.225328	14.914483
21.039326	976.822710	14.919501
20.875636	960.733728	14.924519
20.910179	919.531257	14.929536
20.474732	938.654541	14.934554
20.794662	965.191053	14.939571
20.799825	970.414097	14.944589
20.659075	959.069230	14.949607
20.956104	954.999258	14.954624
20.686437	973.649142	14.959642
20.707922	970.389663	14.964659
20.728504	955.436571	14.969677
20.901904	959.331847	14.974695
21.083959	969.546324	14.979712
20.780616	974.233394	14.984730
21.130229	972.678987	14.989747
20.941657	948.418263	14.994765
20.957678	968.726988	14.999783
20.966328	973.127127	15.004800
20.717204	976.581141	15.009818
20.930689	956.694171	15.014835
21.129202	961.404477	15.019853
21.053371	990.272095	15.024871
21.346333	988.542351	15.029888
20.925090	979.771526	15.034906
21.268922	987.614503	15.039923
21.397941	993.767240	15.044941
21.524042	1007.845623	15.049959
21.900557	997.390100	15.054976
21.383962	968.392540	15.059994
21.340007	964.255029	15.065011
21.412485	970.701279	15.070029
21.242208	959.177578	15.075047
21.504644	945.082430	15.080064
21.344277	969.195222	15.085082
21.526142	968.229023	15.090099
21.456789	957.019368	15.095117
21.370234	957.536824	15.100135
21.192837	953.933146	15.105152
21.346397	974.190713	15.110170
21.757795	999.762314	15.115187
21.451321	994.218445	15.120205
21.407032	980.074961	15.125223
21.833578	993.207354	15.130240
21.976831	1003.596728	15.135258
22.003268	981.047223	15.140275
21.794109	958.986569	15.145293
21.561627	956.973380	15.150311
21.730253	954.404859	15.155328
21.556221	980.107021	15.160346
21.604506	960.452707	15.165363
21.503633	966.098877	15.170381
21.648904	982.670184	15.175399
21.963974	999.689313	15.180416
21.796419	995.189441	15.185434
21.701669	987.097740	15.190451
21.893973	987.838042	15.195469
21.855868	1004.780928	15.200487
21.934053	999.394105	15.205504
21.933879	1000.917404	15.210522
21.827527	973.770846	15.215539
22.170291	999.481807	15.220557
21.904026	1014.885445	15.225575
22.056738	998.201754	15.230592
21.548579	987.003977	15.235610
21.810236	988.108215	15.240627
22.146752	1000.985089	15.245645
21.967858	996.782194	15.250663
22.385443	982.397856	15.255680
22.094573	982.518871	15.260698
22.181600	998.460317	15.265715
22.031603	999.213693	15.270733
22.088603	988.016592	15.275751
22.223836	977.109446	15.280768
22.362297	989.345490	15.285786
22.362776	1010.266724	15.290803
22.191492	990.390749	15.295821
22.112171	988.548849	15.300839
22.310904	987.511768	15.305856
22.059810	996.814726	15.310874
22.203772	995.937347	15.315891
22.760086	999.133493	15.320909
22.400950	999.153416	15.325927
22.459424	1003.880875	15.330944
22.847687	1016.405474	15.335962
22.427605	1016.063810	15.340979
22.580930	987.302689	15.345997
22.331978	979.659299	15.351015
22.332449	993.584753	15.356032
22.780361	1013.850704	15.361050
22.621052	1007.048669	15.366067
22.660204	994.860668	15.371085
22.777876	1021.394073	15.376103
22.631406	1025.085006	15.381120
22.706247	1028.589209	15.386138
22.853353	1004.152802	15.391155
23.118686	1012.433067	15.396173
22.945264	1016.183139	15.401191
22.892544	984.230508	15.406208
22.717279	977.394321	15.411226
22.307152	992.552586	15.416243
22.668173	998.566224	15.421261
22.416643	1019.996986	15.426279
22.853673	997.815838	15.431296
22.984588	1008.105311	15.436314
22.833643	1013.160810	15.441331
22.986774	992.976068	15.446349
22.921546	1006.416257	15.451367
23.109992	994.207227	15.456384
23.016001	1003.443096	15.461402
23.100562	1008.465678	15.466419
23.208555	1021.312412	15.471437
22.929917	1011.817416	15.476455
23.265877	1000.055833	15.481472
22.999767	1015.222007	15.486490
22.814681	1007.975328	15.491507
22.850896	998.326244	15.496525
22.926180	1012.307741	15.501543
23.167781	1002.707370	15.506560
22.915563	995.870607	15.511578
23.347295	1025.043662	15.516595
23.233945	1032.709128	15.521613
23.582695	1026.098352	15.526631
23.365724	1046.136509	15.531648
23.336726	1055.334117	15.536666
23.372244	1049.925003	15.541683
23.910473	1028.921253	15.546701
23.275297	1025.713894	15.551719
23.194450	1050.713251	15.556736
23.426911	1045.723154	15.561754
23.184181	1036.616081	15.566771
23.744843	1019.213738	15.571789
23.534186	1043.699532	15.576807
23.366042	1054.744185	15.581824
23.388617	1036.771261	15.586842
23.573552	1027.015910	15.591859
23.556203	1033.218533	15.596877
23.629214	1058.289992	15.601895
23.479682	1044.958425	15.606912
23.550916	1023.981767	15.611930
23.621597	1032.196105	15.616947
23.861137	1040.054868	15.621965
23.505455	1043.120505	15.626983
23.679490	1032.040611	15.632000
23.855550	1018.211968	15.637018
23.594613	1027.450938	15.642035
23.868493	1049.861503	15.647053
24.102496	1059.102638	15.652071
24.237669	1058.163830	15.657088
24.025799	1040.207208	15.662106
23.776823	1025.269762	15.667123
24.038871	1031.521366	15.672141
23.852038	1024.370417	15.677159
23.811011	1051.475263	15.682176
24.339483	1062.459613	15.687194
24.229394	1059.448574	15.692211
24.203490	1046.117830	15.697229
24.268137	1062.838144	15.702247
24.156429	1047.307071	15.707264
24.190821	1033.412773	15.712282
24.148980	1044.546952	15.717299
24.284783	1045.840061	15.722317
24.161584	1062.374837	15.727335
24.316771	1056.916917	15.732352
24.476972	1041.631690	15.737370
24.225221	1064.985027	15.742387
24.518128	1056.337913	15.747405
24.266975	1063.813326	15.752423
24.494364	1061.413280	15.757440
24.611973	1059.690562	15.762458
24.084380	1052.759945	15.767475
24.524273	1050.457723	15.772493
24.617756	1057.255372	15.777511
24.586482	1045.053779	15.782528
24.924313	1044.478626	15.787546
24.357645	1059.478030	15.792563
24.433463	1045.573726	15.797581
24.487167	1048.610383	15.802599
24.542505	1059.046696	15.807616
24.693522	1047.802034	15.812634
24.537195	1065.788186	15.817651
24.581573	1060.336572	15.822669
24.608579	1051.260192	15.827687
24.675258	1055.982966	15.832704
24.617026	1069.015758	15.837722
24.507784	1071.411402	15.842739
24.588219	1044.777318	15.847757
24.739473	1040.818301	15.852775
24.628132	1064.234240	15.857792
25.021172	1039.264517	15.862810
24.703250	1054.243375	15.867827
24.743600	1074.009182	15.872845
24.529941	1069.274546	15.877863
24.522787	1068.948874	15.882880
25.313942	1072.500422	15.887898
25.296648	1093.910413	15.892915
25.612478	1099.275028	15.897933
25.245504	1087.586835	15.902951
25.316833	1086.537247	15.907968
25.199316	1058.781903	15.912986
24.858624	1053.784674	15.918003
25.056890	1073.849304	15.923021
25.233214	1090.523936	15.928039
25.510622	1084.655944	15.933056
25.271171	1071.212473	15.938074
25.182269	1061.584911	15.943091
25.258781	1071.795939	15.948109
25.432770	1088.504312	15.953127
25.409465	1080.474260	15.958144
25.297386	1064.231597	15.963162
25.437440	1074.375447	15.968179
25.313060	1076.132414	15.973197
25.369036	1087.514076	15.978215
25.215126	1078.900344	15.983232
25.705943	1069.532302	15.988250
25.221888	1087.103167	15.993267
25.580984	1092.857776	15.998285
25.469088	1076.336103	16.003303
25.210285	1085.843094	16.008320
25.761127	1069.630802	16.013338
25.610062	1073.590255	16.018355
25.667342	1096.057051	16.023373
25.693703	1093.693566	16.028391
25.289616	1081.212101	16.033408
25.933909	1084.922336	16.038426
25.665010	1104.309963	16.043443
26.011874	1118.087071	16.048461
25.749813	1094.936906	16.053479
25.674944	1094.947934	16.058496
25.837993	1094.783064	16.063514
25.884791	1112.424856	16.068531
25.933548	1097.153464	16.073549
26.096288	1120.394208	16.078567
26.335963	1112.444174	16.083584
26.389086	1096.929502	16.088602
26.098514	1087.986565	16.093619
25.785169	1085.514791	16.098637
25.997601	1102.594982	16.103655
25.931499	1103.339517	16.108672
25.993182	1084.412375	16.113690
26.064437	1099.403521	16.118707
26.324211	1080.752036	16.123725
26.377169	1091.610609	16.128743
26.446455	1104.489419	16.133760
26.724559	1095.338751	16.138778
26.443435	1081.000018	16.143795
26.441576	1085.713562	16.148813
26.295040	1091.092982	16.153831
26.167650	1106.329409	16.158848
26.213152	1100.767877	16.163866
26.380437	1094.186076	16.168883
26.408221	1084.249918	16.173901
26.347834	1079.203702	16.178919
26.204720	1095.326553	16.183936
26.334313	1090.738975	16.188954
26.301681	1091.425630	16.193971
26.215367	1076.282262	16.198989
26.403444	1089.805634	16.204007
26.503104	1105.724146	16.209024
26.614229	1089.616674	16.214042
26.346775	1091.202453	16.219059
26.553558	1098.363782	16.224077
26.972541	1124.249616	16.229095
26.669463	1107.812934	16.234112
26.964055	1118.919616	16.239130
26.828988	1132.406389	16.244147
27.213400	1116.375449	16.249165
27.353451	1101.996814	16.254183
26.920482	1102.687240	16.259200
27.284353	1087.514632	16.264218
27.070397	1087.366308	16.269235
26.949844	1083.640634	16.274253
27.111897	1083.074946	16.279271
26.909963	1071.401804	16.284288
27.286018	1067.394905	16.289306
27.225094	1083.869426	16.294323
27.033122	1087.685089	16.299341
27.175002	1074.677098	16.304359
26.846221	1079.341835	16.309376
27.046117	1074.960012	16.314394
26.927283	1081.053963	16.319411
27.164550	1105.745886	16.324429
27.286433	1099.142753	16.329447
27.281742	1109.421149	16.334464
27.743162	1106.691844	16.339482
27.566665	1104.580527	16.344499
26.947722	1095.234679	16.349517
27.362973	1099.378241	16.354535
27.081362	1108.713567	16.359552
27.585452	1110.463115	16.364570
27.843472	1113.587645	16.369587
27.605224	1124.439260	16.374605
27.614862	1116.510805	16.379623
27.407306	1108.576229	16.384640
27.574315	1099.228222	16.389658
27.661621	1118.255405	16.394675
27.853497	1124.750969	16.399693
27.689393	1117.241976	16.404711
27.412804	1109.729730	16.409728
27.464785	1110.279992	16.414746
27.478451	1126.196204	16.419763
27.489486	1124.115691	16.424781
27.207183	1104.552427	16.429799
26.854165	1118.863200	16.434816
27.453056	1130.525656	16.439834
27.487505	1130.243194	16.444851
27.787934	1150.667328	16.449869
28.007093	1148.000682	16.454887
27.615797	1136.838784	16.459904
28.232564	1136.712590	16.464922
27.940168	1140.405427	16.469939
27.843135	1141.820071	16.474957
28.042929	1143.328346	16.479975
28.162174	1154.741620	16.484992
27.943686	1135.652201	16.490010
28.272382	1145.107113	16.495027
28.368841	1168.106385	16.500045
28.539627	1159.408053	16.505063
28.227579	1143.495719	16.510080
28.173507	1141.303551	16.515098
28.459917	1127.218246	16.520115
28.342909	1127.359731	16.525133
28.632171	1149.413263	16.530151
28.529170	1135.340641	16.535168
28.687421	1130.662609	16.540186
28.561917	1152.595461	16.545203
28.587092	1135.781453	16.550221
28.700977	1121.228427	16.555239
28.296687	1146.635437	16.560256
28.531959	1150.140906	16.565274
28.408608	1128.352667	16.570291
28.137605	1133.081772	16.575309
28.190955	1140.160530	16.580327
28.200731	1145.085208	16.585344
28.642853	1155.033265	16.590362
28.786397	1157.026804	16.595379
28.262684	1157.895180	16.600397
28.568335	1160.852537	16.605415
28.699670	1165.097057	16.610432
28.500706	1159.752927	16.615450
28.971535	1154.559959	16.620467
28.343831	1167.717938	16.625485
28.795418	1169.696982	16.630503
28.729892	1167.019321	16.635520
28.958658	1163.816864	16.640538
29.317472	1175.745450	16.645555
29.325682	1191.325410	16.650573
29.628555	1169.185644	16.655591
29.186398	1163.398057	16.660608
28.877212	1161.625807	16.665626
29.144839	1136.816379	16.670643
28.961013	1151.223897	16.675661
29.029152	1159.152277	16.680679
29.205965	1168.402044	16.685696
29.201344	1152.770117	16.690714
29.578091	1159.510374	16.695731
29.358836	1193.509401	16.700749
29.537704	1170.337426	16.705767
29.606920	1162.935783	16.710784
29.401352	1157.400566	16.715802
29.316366	1148.207334	16.720819
29.138107	1153.223801	16.725837
29.885311	1182.941658	16.730855
29.846525	1183.074251	16.735872
29.519084	1157.986051	16.740890
29.520552	1137.906870	16.745907
29.568146	1151.795456	16.750925
29.878659	1168.096509	16.755943
29.606053	1153.268820	16.760960
29.879119	1158.131100	16.765978
29.644489	1159.356331	16.770995
29.449124	1188.060557	16.776013
29.916808	1170.433308	16.781031
29.465717	1183.278423	16.786048
29.603025	1183.891242	16.791066
29.667959	1170.233840	16.796083
29.775837	1187.083038	16.801101
29.887050	1169.889902	16.806119
29.807358	1172.427690	16.811136
29.657928	1165.301883	16.816154
30.036997	1164.703381	16.821171
29.608911	1181.877994	16.826189
29.668438	1170.678177	16.831207
29.829592	1178.806695	16.836224
30.038068	1200.294854	16.841242
30.093798	1209.184922	16.846259
29.955830	1208.905367	16.851277
30.125044	1191.759202	16.856295
30.120188	1208.021588	16.861312
30.233751	1199.374805	16.866330
30.608522	1201.466425	16.871347
30.280179	1203.865234	16.876365
30.411724	1182.946092	16.881383
30.473190	1198.755588	16.886400
30.589595	1213.517292	16.891418
30.650516	1184.915105	16.896435
30.518128	1191.790681	16.901453
30.678943	1206.486589	16.906471
30.688827	1195.955428	16.911488
30.649371	1177.670619	16.916506
30.979998	1193.125960	16.921523
30.855878	1207.226000	16.926541
30.558787	1183.937428	16.931559
30.795030	1197.762310	16.936576
30.498250	1207.135627	16.941594
30.768960	1201.551997	16.946611
30.601717	1201.345275	16.951629
30.850060	1191.739637	16.956647
30.880078	1202.313862	16.961664
30.706056	1197.403975	16.966682
31.007894	1194.037997	16.971699
30.793831	1210.930385	16.976717
30.893487	1210.928612	16.981735
31.132834	1195.203680	16.986752
30.979263	1180.970221	16.991770
31.038627	1190.407282	16.996787
30.692959	1198.985225	17.001805
30.884511	1192.595977	17.006823
31.017592	1191.969538	17.011840
30.840628	1210.949682	17.016858
30.942633	1228.416678	17.021875
31.021561	1227.645483	17.026893
31.185118	1233.409039	17.031911
31.558009	1221.785638	17.036928
31.257766	1217.605784	17.041946
31.729964	1215.447771	17.046963
31.309330	1218.140113	17.051981
31.448658	1219.834822	17.056999
31.293940	1210.206824	17.062016
31.332647	1227.049293	17.067034
31.329701	1210.152863	17.072051
31.390005	1215.616917	17.077069
31.704350	1216.559747	17.082087
31.846638	1202.303059	17.087104
31.389338	1214.353452	17.092122
31.821795	1224.302661	17.097139
31.658071	1220.355599	17.102157
31.576339	1227.574901	17.107175
31.870030	1222.537334	17.112192
31.859198	1213.766744	17.117210
31.750321	1198.399085	17.122227
31.548380	1217.630747	17.127245
31.708521	1211.366929	17.132263
31.985145	1227.091108	17.137280
31.954819	1247.219620	17.142298
32.593771	1231.664485	17.147315
32.040588	1237.979945	17.152333
32.093958	1224.641062	17.157351
32.619350	1207.200448	17.162368
31.984018	1209.594981	17.167386
32.250843	1217.228908	17.172403
32.151322	1220.817074	17.177421
31.864013	1205.323419	17.182439
32.061788	1217.861976	17.187456
32.292545	1240.321473	17.192474
32.064291	1225.190097	17.197491
32.151785	1235.016144	17.202509
32.129267	1233.756419	17.207527
32.562932	1235.824339	17.212544
32.326163	1257.488297	17.217562
32.181698	1251.439229	17.222579
32.350216	1245.864401	17.227597
32.276395	1230.902039	17.232615
32.286677	1238.564890	17.237632
32.237025	1253.249080	17.242650
32.201680	1243.389180	17.247667
32.447236	1258.082451	17.252685
32.581679	1274.508754	17.257703
33.074808	1268.359138	17.262720
32.880664	1272.907120	17.267738
33.424258	1272.810435	17.272755
33.017916	1259.257598	17.277773
32.807851	1243.643783	17.282791
33.082445	1233.456359	17.287808
32.858376	1244.158703	17.292826
32.779451	1246.806390	17.297843
32.844632	1246.794176	17.302861
32.739179	1229.741378	17.307879
33.012167	1240.145981	17.312896
32.978369	1277.641075	17.317914
33.191335	1269.714168	17.322931
33.255301	1251.472796	17.327949
33.261766	1255.360506	17.332967
33.470901	1265.025954	17.337984
33.167898	1277.767659	17.343002
33.357676	1267.699420	17.348019
33.366083	1253.035285	17.353037
33.383651	1261.764998	17.358055
33.541243	1257.453878	17.363072
33.518200	1273.556090	17.368090
33.449129	1279.113774	17.373107
33.434041	1267.233957	17.378125
33.064344	1240.529856	17.383143
33.632048	1247.230822	17.388160
33.253786	1247.521164	17.393178
33.701658	1251.644322	17.398195
33.416777	1261.139889	17.403213
33.402832	1252.306322	17.408231
33.492240	1249.994486	17.413248
33.312286	1262.670088	17.418266
33.517417	1247.180821	17.423283
33.186203	1258.381770	17.428301
33.551798	1283.626260	17.433319
33.486218	1288.035017	17.438336
33.534778	1277.206434	17.443354
34.064308	1268.793656	17.448371
33.759174	1282.531251	17.453389
33.477104	1292.545738	17.458407
34.445096	1287.239377	17.463424
34.310758	1289.737408	17.468442
34.578556	1273.284832	17.473459
34.126679	1281.567354	17.478477
34.194719	1272.445686	17.483495
34.225973	1270.315955	17.488512
34.112750	1287.654057	17.493530
34.554835	1277.611130	17.498547
34.279328	1266.846635	17.503565
34.395039	1284.578002	17.508583
34.276303	1281.276683	17.513600
34.413898	1278.593678	17.518618
34.255294	1276.441298	17.523635
34.576023	1273.454178	17.528653
34.367108	1267.565128	17.533671
34.728829	1259.814779	17.538688
34.288695	1281.209298	17.543706
34.661324	1288.790549	17.548723
35.059355	1279.231265	17.553741
34.756059	1287.631724	17.558759
35.012556	1265.364081	17.563776
34.672664	1269.956319	17.568794
34.782157	1257.602388	17.573811
34.836939	1259.967119	17.578829
34.679815	1264.493236	17.583847
34.832050	1280.724919	17.588864
34.354423	1270.995653	17.593882
34.867520	1269.006916	17.598899
35.318063	1288.523664	17.603917
34.997714	1317.665718	17.608935
35.110993	1294.796647	17.613952
35.212048	1304.786405	17.618970
35.122738	1301.821478	17.623987
35.119019	1281.954529	17.629005
34.901497	1279.866302	17.634023
35.306059	1293.226551	17.639040
35.264116	1294.318892	17.644058
35.295740	1301.823953	17.649075
35.817204	1292.259516	17.654093
35.026250	1288.935355	17.659111
35.346569	1291.987339	17.664128
35.320006	1282.201437	17.669146
35.468742	1282.391014	17.674163
35.709388	1292.742547	17.679181
35.546146	1305.580935	17.684199
35.615275	1291.941920	17.689216
35.662287	1301.619815	17.694234
35.757155	1290.079600	17.699251
35.964074	1287.179084	17.704269
35.546046	1280.488757	17.709287
35.730542	1295.950737	17.714304
35.708864	1282.266809	17.719322
36.081183	1286.818408	17.724339
35.809189	1297.808958	17.729357
35.818571	1304.287130	17.734375
36.013780	1292.365752	17.739392
35.776952	1302.960526	17.744410
35.727756	1279.359351	17.749427
35.973608	1280.867409	17.754445
35.572168	1292.374309	17.759463
35.675641	1295.513690	17.764480
35.818716	1301.733307	17.769498
35.854422	1312.292695	17.774515
36.148056	1312.450555	17.779533
35.864348	1331.631025	17.784551
36.424425	1316.452239	17.789568
36.402543	1313.590510	17.794586
36.083629	1307.420677	17.799603
36.252991	1315.227711	17.804621
35.902957	1315.750243	17.809639
36.427015	1323.604056	17.814656
36.210927	1343.235169	17.819674
36.395810	1354.287531	17.824691
36.648955	1341.880272	17.829709
36.586886	1356.899116	17.834727
36.779193	1351.606571	17.839744
36.636203	1347.139732	17.844762
36.708609	1340.005623	17.849779
36.937811	1338.387732	17.854797
36.768033	1349.021250	17.859815
36.695411	1349.444016	17.864832
36.846215	1338.855717	17.869850
36.642126	1351.775089	17.874867
36.802278	1359.839121	17.879885
36.761572	1353.001882	17.884903
37.118154	1344.125139	17.889920
37.133988	1350.386368	17.894938
37.196353	1335.845982	17.899955
37.430579	1322.157811	17.904973
37.090424	1343.389473	17.909991
37.215577	1341.400971	17.915008
37.390523	1335.333036	17.920026
36.840531	1338.383410	17.925043
37.099728	1340.383741	17.930061
36.926517	1328.500978	17.935079
37.204275	1333.918808	17.940096
37.078987	1343.728427	17.945114
37.288165	1368.629897	17.950131
37.876778	1375.214401	17.955149
37.507470	1370.206444	17.960167
37.713247	1366.488670	17.965184
37.934073	1371.193941	17.970202
37.554553	1348.206665	17.975219
37.687448	1354.239742	17.980237
37.644472	1359.444010	17.985255
37.973802	1362.870220	17.990272
38.013500	1364.513315	17.995290
37.761649	1348.165129	18.000307
37.870906	1323.429000	18.005325
37.532928	1338.494010	18.010343
37.670154	1367.276554	18.015360
37.942543	1368.088465	18.020378
37.649252	1376.615931	18.025395
37.853321	1366.883968	18.030413
37.906192	1353.985013	18.035431
38.218737	1347.479076	18.040448
38.111659	1360.600780	18.045466
37.883895	1371.157892	18.050483
38.393634	1365.670596	18.055501
37.804585	1358.758652	18.060519
38.009141	1361.352626	18.065536
38.120309	1382.784599	18.070554
38.055888	1401.046836	18.075571
38.139848	1381.187017	18.080589
38.357224	1383.472056	18.085607
38.506369	1384.639789	18.090624
38.556297	1388.307211	18.095642
38.343112	1383.145625	18.100659
38.510410	1373.693097	18.105677
38.647547	1381.267454	18.110695
38.677859	1379.291373	18.115712
38.646376	1383.329940	18.120730
38.208618	1403.338431	18.125747
38.758560	1394.606240	18.130765
39.159713	1401.996066	18.135783
39.301468	1415.316406	18.140800
39.092304	1397.371119	18.145818
39.103214	1387.834509	18.150835
38.911091	1390.902410	18.155853
39.117459	1379.601814	18.160871
39.056395	1369.201817	18.165888
38.830968	1381.632136	18.170906
39.201572	1405.996577	18.175923
39.412282	1400.543825	18.180941
39.202323	1422.989235	18.185959
39.285877	1416.169516	18.190976
39.658137	1395.334785	18.195994
39.516538	1396.721589	18.201011
39.264640	1392.867086	18.206029
39.127726	1386.837283	18.211047
39.253181	1386.941261	18.216064
39.612701	1400.064910	18.221082
39.474837	1412.040727	18.226099
39.559645	1416.702953	18.231117
39.571313	1404.425980	18.236135
39.400483	1395.622093	18.241152
39.417967	1412.445345	18.246170
39.305995	1418.325747	18.251187
39.372932	1411.833112	18.256205
39.785251	1389.562762	18.261223
39.541225	1401.179427	18.266240
39.644836	1417.814378	18.271258
39.557250	1417.011944	18.276275
39.927214	1423.234265	18.281293
39.839152	1439.401715	18.286311
40.298589	1427.621468	18.291328
40.531869	1416.966545	18.296346
40.075422	1443.619002	18.301363
40.205485	1422.726051	18.306381
40.282192	1429.467891	18.311399
40.345147	1438.566302	18.316416
40.512356	1425.111112	18.321434
40.373805	1414.869230	18.326451
40.341996	1409.525728	18.331469
40.244842	1420.352170	18.336487
40.439551	1437.870803	18.341504
40.568839	1425.478926	18.346522
40.281483	1412.581629	18.351539
40.437946	1419.867541	18.356557
40.553229	1433.155567	18.361575
40.680232	1429.641501	18.366592
40.686075	1420.773864	18.371610
40.561368	1435.752557	18.376627
40.560586	1433.418991	18.381645
40.610739	1433.559817	18.386663
40.491814	1421.300377	18.391680
40.708072	1417.637539	18.396698
40.543965	1431.779818	18.401715
40.824053	1442.279822	18.406733
40.680610	1446.458534	18.411751
40.623402	1438.498350	18.416768
41.108336	1453.721810	18.421786
40.785444	1462.486053	18.426803
40.788189	1452.896335	18.431821
41.321884	1446.172258	18.436839
41.055897	1447.729883	18.441856
41.079065	1445.109153	18.446874
41.176766	1454.133441	18.451891
41.493635	1471.033437	18.456909
41.564661	1484.472589	18.461927
41.417609	1471.816663	18.466944
41.729300	1458.648523	18.471962
41.807883	1468.920681	18.476979
41.794544	1473.505759	18.481997
41.421401	1472.702095	18.487015
41.565280	1454.770824	18.492032
41.695591	1457.397846	18.497050
41.387303	1477.167764	18.502067
41.580786	1474.244044	18.507085
41.440326	1462.751050	18.512103
41.926713	1477.688630	18.517120
42.156122	1458.245522	18.522138
41.781703	1458.737352	18.527155
41.982199	1469.719713	18.532173
41.651364	1471.719654	18.537191
41.988628	1468.552048	18.542208
42.270525	1441.904743	18.547226
41.899809	1457.494553	18.552243
42.047476	1456.764141	18.557261
42.212607	1463.345354	18.562279
42.134916	1469.851859	18.567296
42.638885	1470.259447	18.572314
42.462596	1471.315057	18.577331
42.309711	1483.107036	18.582349
42.539751	1459.522909	18.587367
42.471315	1463.793637	18.592384
42.536322	1475.839007	18.597402
42.428880	1466.569882	18.602419
42.847107	1474.546752	18.607437
42.823343	1471.031612	18.612455
42.501230	1471.282861	18.617472
42.833607	1471.061274	18.622490
42.536670	1480.639659	18.627507
42.692960	1494.882462	18.632525
42.978561	1494.803023	18.637543
42.843383	1500.156797	18.642560
43.428102	1499.608534	18.647578
43.081554	1506.932738	18.652595
43.101025	1498.444611	18.657613
43.168236	1477.839469	18.662631
42.783366	1499.259601	18.667648
43.182245	1495.453599	18.672666
42.970708	1490.971967	18.677683
42.685344	1498.626336	18.682701
42.913273	1492.578613	18.687719
42.759223	1487.019412	18.692736
43.262067	1494.551007	18.697754
43.123005	1511.842266	18.702771
42.954150	1511.828479	18.707789
43.287705	1500.584613	18.712807
43.305224	1517.356116	18.717824
43.166272	1523.965759	18.722842
43.265051	1502.684844	18.727859
43.328805	1500.698399	18.732877
43.666989	1531.826163	18.737895
43.582467	1536.255145	18.742912
43.751517	1531.166339	18.747930
43.862352	1542.595168	18.752947
43.797769	1541.346699	18.757965
44.169004	1516.344771	18.762983
43.929191	1523.161197	18.768000
44.104795	1527.895048	18.773018
44.000956	1521.130259	18.778035
44.147951	1524.287884	18.783053
44.265186	1537.170747	18.788071
44.135721	1529.407553	18.793088
44.460535	1534.278329	18.798106
44.403346	1537.756052	18.803123
44.248215	1521.724696	18.808141
44.705049	1529.519662	18.813159
44.440824	1521.071022	18.818176
44.563694	1519.045383	18.823194
44.679742	1535.639046	18.828211
44.504116	1538.872817	18.833229
44.947787	1525.830415	18.838247
44.609217	1537.309297	18.843264
44.699033	1521.962895	18.848282
44.843633	1530.662618	18.853299
44.482230	1531.814851	18.858317
44.913771	1514.848352	18.863335
44.606436	1533.484378	18.868352
44.544393	1530.936068	18.873370
44.741201	1540.501880	18.878387
44.740825	1531.180779	18.883405
45.095371	1531.467719	18.888423
44.566385	1535.468290	18.893440
44.917153	1540.524205	18.898458
45.004771	1555.270235	18.903475
45.011154	1570.116888	18.908493
45.015053	1563.876089	18.913511
45.209091	1556.613241	18.918528
45.280581	1542.587868	18.923546
45.237357	1552.944863	18.928563
45.097681	1572.758088	18.933581
45.291563	1559.358203	18.938599
45.134134	1558.915356	18.943616
45.528473	1564.545844	18.948634
45.786332	1581.019292	18.953651
45.752791	1584.669950	18.958669
45.985929	1584.754660	18.963687
45.882994	1575.661556	18.968704
45.869591	1570.465023	18.973722
45.639975	1550.995114	18.978739
45.877918	1562.597794	18.983757
45.991787	1562.103030	18.988775
45.765425	1570.202508	18.993792
45.711385	1582.926843	18.998810
45.814213	1576.221854	19.003827
45.639001	1564.807050	19.008845
46.138461	1578.436158	19.013863
46.077129	1563.020913	19.018880
46.224214	1567.637665	19.023898
46.409309	1584.758733	19.028915
46.494407	1595.041807	19.033933
46.626601	1569.650350	19.038951
46.501098	1567.349674	19.043968
46.516504	1565.976296	19.048986
46.374669	1578.544405	19.054003
46.112774	1579.625190	19.059021
46.445117	1587.750337	19.064039
46.443510	1604.189243	19.069056
46.713519	1585.369347	19.074074
46.725569	1578.886401	19.079091
46.654392	1593.999186	19.084109
46.716542	1599.861314	19.089127
47.035075	1605.973240	19.094144
46.946247	1591.116133	19.099162
47.001035	1577.546738	19.104179
46.816022	1601.690480	19.109197
47.269576	1607.773796	19.114215
46.883795	1591.690342	19.119232
46.937791	1590.153532	19.124250
47.206622	1592.555664	19.129267
47.044923	1604.313964	19.134285
47.063625	1596.354044	19.139303
47.336495	1621.948303	19.144320
47.079255	1627.762061	19.149338
47.448911	1615.040608	19.154355
47.463730	1615.831134	19.159373
47.481417	1635.535973	19.164391
47.593718	1632.002739	19.169408
47.486356	1614.641329	19.174426
47.589440	1615.195958	19.179443
47.604805	1629.497206	19.184461
47.860086	1611.966742	19.189479
47.803373	1617.908644	19.194496
47.678135	1634.322747	19.199514
47.842340	1610.134634	19.204531
47.727253	1623.913258	19.209549
47.541261	1627.234568	19.214567
47.986099	1651.625905	19.219584
48.010113	1636.254542	19.224602
48.352493	1640.330392	19.229619
48.044290	1651.988653	19.234637
48.317314	1635.294522	19.239655
48.532326	1635.766398	19.244672
48.406346	1630.364086	19.249690
48.504636	1640.414055	19.254707
48.364579	1632.124226	19.259725
48.480302	1626.274875	19.264743
48.795005	1637.238092	19.269760
48.734270	1637.803064	19.274778
48.905103	1619.824143	19.279795
48.691287	1615.279578	19.284813
48.758210	1630.161059	19.289831
48.939336	1637.688224	19.294848
48.669527	1632.273466	19.299866
48.603415	1633.020390	19.304883
48.501960	1630.922085	19.309901
48.635271	1623.594748	19.314919
48.866568	1633.803896	19.319936
48.715264	1645.422940	19.324954
49.211608	1641.482712	19.329971
49.142049	1659.241193	19.334989
49.305118	1667.682287	19.340007
49.406003	1672.845766	19.345024
49.025808	1680.471220	19.350042
49.535120	1655.928726	19.355059
49.335733	1652.461262	19.360077
49.543545	1657.790099	19.365095
49.732391	1657.126578	19.370112
49.698008	1663.963439	19.375130
49.956681	1666.788334	19.380147
49.524993	1664.174341	19.385165
49.854205	1642.962118	19.390183
49.907930	1648.846913	19.395200
49.845022	1675.325708	19.400218
50.015752	1668.337566	19.405235
49.736240	1651.175687	19.410253
50.173737	1644.003247	19.415271
49.720238	1653.088232	19.420288
49.733576	1651.343809	19.425306
50.316677	1656.789431	19.430323
49.904865	1649.867352	19.435341
50.165675	1634.159974	19.440359
49.990337	1658.295515	19.445376
49.813053	1654.474275	19.450394
50.173935	1651.549724	19.455411
49.971195	1664.950728	19.460429
50.194094	1665.582587	19.465447
50.323236	1675.407744	19.470464
50.172596	1675.504210	19.475482
50.367520	1675.828355	19.480499
50.363907	1678.101346	19.485517
50.403908	1663.041323	19.490535
50.851561	1699.428285	19.495552
50.792203	1710.332821	19.500570
50.915343	1693.247733	19.505587
51.057734	1686.503587	19.510605
50.975326	1698.557846	19.515623
51.358241	1692.204472	19.520640
51.264526	1700.998780	19.525658
51.705266	1699.433083	19.530675
51.657914	1678.126378	19.535693
51.317011	1650.425766	19.540711
51.722073	1668.188389	19.545728
51.352919	1678.194688	19.550746
51.287668	1655.330963	19.555763
51.163070	1651.654824	19.560781
51.364400	1662.666709	19.565799
51.451161	1658.643797	19.570816
51.235191	1648.117271	19.575834
51.445117	1670.638412	19.580851
51.740713	1697.179630	19.585869
51.435264	1696.371360	19.590887
51.572273	1702.880666	19.595904
51.670302	1704.088558	19.600922
51.709460	1686.164087	19.605939
51.641288	1686.526199	19.610957
51.552702	1695.832542	19.615975
51.713237	1687.087878	19.620992
51.795413	1704.350963	19.626010
51.894034	1713.583674	19.631027
51.937002	1711.553205	19.636045
52.006590	1718.576016	19.641063
52.115985	1730.920587	19.646080
51.932284	1738.729697	19.651098
52.214899	1727.268933	19.656115
52.117303	1719.639718	19.661133
52.152431	1726.301078	19.666151
52.212395	1719.230057	19.671168
52.268828	1747.777310	19.676186
52.454021	1753.290294	19.681203
52.383757	1752.040975	19.686221
52.890104	1732.961909	19.691239
52.632463	1750.523276	19.696256
52.625161	1771.130464	19.701274
52.932034	1764.018621	19.706291
52.709357	1751.863346	19.711309
52.902977	1742.060150	19.716327
53.089051	1756.115931	19.721344
52.918257	1792.798973	19.726362
53.163356	1772.546147	19.731379
53.198300	1769.290769	19.736397
53.142652	1775.528658	19.741415
53.529933	1775.313051	19.746432
53.587459	1783.725104	19.751450
53.852089	1755.866771	19.756467
54.201255	1758.599777	19.761485
53.890360	1753.928032	19.766503
54.037805	1732.839207	19.771520
53.556961	1740.962326	19.776538
53.752193	1743.375858	19.781555
53.767971	1733.155100	19.786573
53.473906	1734.848862	19.791591
53.893901	1712.468235	19.796608
53.869727	1723.909571	19.801626
54.017614	1738.474692	19.806643
53.743302	1763.448337	19.811661
53.706484	1755.492688	19.816679
54.437711	1759.564735	19.821696
54.082950	1776.748757	19.826714
53.944860	1751.771273	19.831731
54.299240	1751.384269	19.836749
53.986846	1775.430067	19.841767
54.380605	1753.931096	19.846784
54.214706	1768.858075	19.851802
54.293322	1768.894123	19.856819
54.375694	1764.194880	19.861837
54.115937	1773.169787	19.866855
54.248390	1787.222746	19.871872
54.299908	1806.968073	19.876890
54.323139	1803.616709	19.881907
54.533536	1788.470150	19.886925
54.833919	1814.456955	19.891943
55.121239	1818.816405	19.896960
54.988660	1833.598992	19.901978
55.130664	1823.304767	19.906995
55.198567	1833.202140	19.912013
54.977438	1824.749064	19.917031
55.490196	1802.659018	19.922048
55.472850	1816.499602	19.927066
55.135779	1820.578647	19.932083
55.339947	1817.101435	19.937101
55.228824	1814.033538	19.942119
55.727600	1804.206840	19.947136
55.344658	1817.247282	19.952154
55.570946	1801.923020	19.957171
55.286563	1808.058787	19.962189
55.381795	1797.896496	19.967207
55.510853	1800.207609	19.972224
55.312763	1820.253596	19.977242
55.659871	1822.924073	19.982259
55.794587	1835.461749	19.987277
55.673349	1830.511741	19.992295
55.707283	1848.861683	19.997312
55.832468	1849.394266	20.002330
56.163710	1839.781611	20.007347
55.921351	1854.571140	20.012365
55.911378	1855.966051	20.017383
56.361027	1832.955275	20.022400
56.502146	1849.812110	20.027418
56.489925	1859.711030	20.032435
56.225674	1842.988650	20.037453
56.417849	1857.367073	20.042471
56.806279	1856.377511	20.047488
56.637800	1860.870647	20.052506
56.768484	1854.666839	20.057523
56.871283	1864.902886	20.062541
57.000821	1862.982969	20.067559
57.481016	1841.488881	20.072576
57.145058	1848.336886	20.077594
56.908057	1861.380409	20.082611
56.814762	1843.724640	20.087629
56.280034	1858.600471	20.092647
56.852479	1866.842361	20.097664
56.990534	1872.093152	20.102682
56.947366	1866.746940	20.107699
57.250676	1854.849576	20.112717
57.207970	1875.569625	20.117735
57.299007	1887.377107	20.122752
57.208654	1892.984485	20.127770
57.151643	1894.912955	20.132787
57.549775	1886.872374	20.137805
57.604302	1899.513001	20.142823
57.503519	1886.509388	20.147840
57.511815	1882.847446	20.152858
57.805809	1888.252755	20.157875
57.823186	1893.454119	20.162893
57.911031	1921.250095	20.167911
57.983319	1919.087711	20.172928
58.007342	1918.361375	20.177946
58.236754	1916.789050	20.182963
58.575353	1916.428761	20.187981
58.564632	1910.034853	20.192999
58.917796	1900.033868	20.198016
58.557777	1883.110480	20.203034
58.605806	1877.237778	20.208051
58.908261	1876.836916	20.213069
58.797759	1875.054479	20.218087
58.859864	1860.918971	20.223104
59.196122	1867.930160	20.228122
58.762466	1866.668454	20.233139
58.901972	1862.074580	20.238157
58.513139	1875.108270	20.243175
58.531903	1861.639342	20.248192
58.668969	1862.017532	20.253210
58.520486	1867.755251	20.258227
58.924103	1873.715555	20.263245
58.750835	1909.358741	20.268263
59.081374	1918.662876	20.273280
59.122992	1909.440589	20.278298
58.894899	1892.412926	20.283315
58.930117	1902.445641	20.288333
58.810543	1911.222693	20.293351
58.969013	1917.087133	20.298368
59.266867	1928.756456	20.303386
59.241057	1928.656739	20.308403
59.325344	1936.992028	20.313421
59.226749	1941.701746	20.318439
59.395348	1929.034907	20.323456
59.456910	1937.707647	20.328474
59.588280	1961.374853	20.333491
60.167080	1951.403268	20.338509
59.671145	1951.457798	20.343527
59.813602	1965.654910	20.348544
59.890639	1971.592265	20.353562
59.651649	1967.568781	20.358579
60.049833	1956.592099	20.363597
60.389827	1963.045635	20.368615
60.360885	1980.116409	20.373632
60.494443	1989.635485	20.378650
60.883430	1975.389665	20.383667
61.114685	1966.889506	20.388685
60.836860	1963.393405	20.393703
60.901514	1955.592898	20.398720
60.850807	1940.319683	20.403738
60.843873	1952.403690	20.408755
61.208286	1940.342354	20.413773
60.733489	1954.886881	20.418791
60.589288	1947.761812	20.423808
60.627663	1954.605476	20.428826
60.890349	1976.546508	20.433843
61.268467	1963.794831	20.438861
61.145746	1967.458251	20.443879
60.956548	1977.846936	20.448896
61.266339	1976.851665	20.453914
61.145582	1981.045765	20.458931
61.649805	1981.474191	20.463949
61.418157	1978.113244	20.468967
61.386441	1970.072404	20.473984
61.234005	1980.521835	20.479002
61.332341	2007.402528	20.484019
61.428329	1994.823604	20.489037
61.684607	2002.579331	20.494055
61.279474	2012.896952	20.499072
61.798338	1996.241613	20.504090
61.707327	2004.435072	20.509107
62.082779	2033.324948	20.514125
62.072107	2040.558180	20.519143
62.244204	2022.276569	20.524160
62.107109	2034.334815	20.529178
62.602575	2044.532272	20.534195
62.445275	2030.485217	20.539213
62.663569	2029.197933	20.544231
62.598396	2030.745164	20.549248
62.721741	2042.994490	20.554266
62.476605	2034.257916	20.559283
62.687844	2026.135568	20.564301
62.648023	2033.560292	20.569319
62.338840	2037.741359	20.574336
62.637044	2047.297623	20.579354
62.710977	2053.159946	20.584371
62.771349	2025.082856	20.589389
62.572879	2020.201050	20.594407
62.832093	2053.463200	20.599424
63.231216	2073.577729	20.604442
63.190846	2073.231053	20.609459
63.418279	2040.254584	20.614477
63.120645	2054.338315	20.619495
63.328257	2061.590693	20.624512
63.588385	2062.879485	20.629530
63.066828	2050.438480	20.634547
63.420601	2051.956830	20.639565
63.586584	2052.180472	20.644583
63.119621	2053.251482	20.649600
63.682706	2069.976539	20.654618
63.746796	2087.886333	20.659635
64.086098	2069.908372	20.664653
63.767749	2066.625402	20.669671
63.683938	2079.202537	20.674688
64.073591	2072.881648	20.679706
63.949297	2076.057254	20.684723
63.926320	2079.628739	20.689741
64.200960	2062.118082	20.694759
64.414682	2081.464587	20.699776
64.522447	2093.743000	20.704794
64.590518	2110.082859	20.709811
64.614739	2095.993053	20.714829
64.859280	2086.170301	20.719847
64.961967	2099.770676	20.724864
65.151473	2072.959525	20.729882
64.732398	2072.206223	20.734899
65.028454	2088.527084	20.739917
64.659377	2077.023481	20.744935
64.609066	2077.717530	20.749952
65.056936	2095.992773	20.754970
64.958121	2112.821940	20.759987
65.026860	2098.834008	20.765005
65.207500	2089.280428	20.770023
64.888101	2087.586117	20.775040
64.893829	2107.888707	20.780058
64.965246	2131.904999	20.785075
65.193751	2129.491320	20.790093
65.499729	2126.956395	20.795111
65.346899	2130.668521	20.800128
65.617814	2112.113532	20.805146
65.464186	2128.187837	20.810163
65.578395	2154.284415	20.815181
65.952097	2159.709812	20.820199
66.023027	2141.765880	20.825216
66.053823	2160.094178	20.830234
66.352898	2158.143553	20.835251
66.229357	2150.299157	20.840269
66.378503	2128.559329	20.845287
66.272991	2148.523922	20.850304
66.414133	2153.251756	20.855322
66.293421	2151.316080	20.860339
66.264475	2142.263553	20.865357
66.476596	2138.227870	20.870375
66.349511	2156.464951	20.875392
66.846266	2162.178228	20.880410
66.853806	2161.573874	20.885427
67.122778	2172.414052	20.890445
67.472570	2162.450554	20.895463
67.032496	2158.134617	20.900480
67.217550	2123.096934	20.905498
66.942183	2135.617203	20.910515
66.944260	2162.407893	20.915533
67.395427	2156.897230	20.920551
67.433381	2173.941321	20.925568
67.579833	2153.417338	20.930586
67.618879	2154.466342	20.935603
67.452161	2170.296539	20.940621
67.705170	2154.659198	20.945639
67.624285	2149.736369	20.950656
67.539648	2159.102762	20.955674
67.647945	2172.172250	20.960691
67.595351	2173.774984	20.965709
67.667950	2156.807654	20.970727
67.580276	2138.591563	20.975744
68.075836	2145.802106	20.980762
67.966181	2170.767410	20.985779
68.157105	2149.461711	20.990797
67.978837	2157.936060	20.995815
68.331380	2192.879346	21.000832
68.439606	2179.609097	21.005850
68.129425	2183.375678	21.010867
68.303735	2202.856384	21.015885
68.650333	2195.504355	21.020903
68.092968	2193.319625	21.025920
68.391196	2186.920900	21.030938
68.520453	2190.539486	21.035955
68.650171	2225.325901	21.040973
68.837323	2209.735995	21.045991
68.729074	2214.407634	21.051008
69.401966	2217.742038	21.056026
69.043974	2218.743683	21.061043
68.858492	2217.752496	21.066061
69.417387	2201.979241	21.071079
69.166353	2200.888572	21.076096
69.490306	2215.422691	21.081114
69.297436	2224.350789	21.086131
69.159646	2199.534111	21.091149
69.639694	2204.444893	21.096167
69.672410	2224.644967	21.101184
69.951875	2239.351392	21.106202
69.734921	2235.695687	21.111219
69.620427	2229.116369	21.116237
69.888101	2231.414580	21.121255
69.693960	2234.938415	21.126272
69.797933	2233.211424	21.131290
70.081724	2239.450782	21.136307
70.243520	2249.216393	21.141325
70.692822	2265.345121	21.146343
70.630906	2257.809429	21.151360
70.654297	2248.484161	21.156378
70.680462	2247.382421	21.161395
70.480535	2231.629723	21.166413
70.648058	2248.651208	21.171431
70.522251	2272.594915	21.176448
70.762733	2245.990553	21.181466
70.722068	2242.264581	21.186483
70.745530	2255.774562	21.191501
71.124281	2270.137895	21.196519
70.907886	2250.656349	21.201536
71.010861	2239.607697	21.206554
71.016867	2253.436352	21.211571
71.257961	2265.100846	21.216589
71.017392	2277.467473	21.221607
70.745078	2298.099381	21.226624
71.098443	2279.228058	21.231642
71.314652	2273.151460	21.236659
71.208910	2286.767056	21.241677
71.663221	2310.925144	21.246695
71.699029	2321.343700	21.251712
71.872972	2311.752020	21.256730
71.884671	2299.747016	21.261747
71.813692	2301.799183	21.266765
72.213280	2313.275149	21.271783
71.822334	2307.157551	21.276800
72.269607	2310.434491	21.281818
72.316265	2312.699859	21.286835
71.974005	2303.876441	21.291853
72.683952	2307.808283	21.296871
72.593174	2324.882081	21.301888
72.729589	2325.626177	21.306906
72.890223	2289.995005	21.311923
72.832849	2295.651598	21.316941
72.699516	2300.722027	21.321959
72.845992	2317.452726	21.326976
72.984674	2317.312145	21.331994
73.104058	2320.598592	21.337011
72.933012	2328.000858	21.342029
73.328936	2316.034104	21.347047
72.923855	2324.956094	21.352064
73.121361	2313.760983	21.357082
73.164775	2319.347593	21.362099
73.314270	2337.558276	21.367117
73.439098	2326.224797	21.372135
73.201780	2320.912181	21.377152
73.478810	2336.767533	21.382170
73.876653	2352.487406	21.387187
73.732017	2354.608041	21.392205
73.969994	2344.552488	21.397223
74.008662	2337.572876	21.402240
73.978476	2337.724920	21.407258
74.333929	2351.073056	21.412275
74.357539	2366.909302	21.417293
74.402521	2348.132940	21.422311
74.443738	2333.149114	21.427328
74.156859	2348.117114	21.432346
74.745449	2358.121766	21.437363
74.399084	2349.456061	21.442381
74.703394	2340.232914	21.447399
74.367476	2346.013100	21.452416
74.272855	2339.908521	21.457434
74.655430	2349.128447	21.462451
74.472441	2381.315259	21.467469
75.129940	2372.955431	21.472487
75.027885	2360.587939	21.477504
74.870101	2367.012799	21.482522
75.253694	2382.339453	21.487539
74.954010	2387.390556	21.492557
75.104553	2380.753796	21.497575
75.509169	2386.216384	21.502592
75.432094	2406.744337	21.507610
75.545673	2425.521796	21.512627
75.242292	2416.097101	21.517645
75.511411	2394.232562	21.522663
75.598310	2408.819617	21.527680
75.441106	2407.036470	21.532698
75.537716	2429.536414	21.537715
75.629436	2424.073934	21.542733
76.346811	2420.281210	21.547751
76.269588	2423.186454	21.552768
76.112036	2427.028840	21.557786
76.122913	2413.718973	21.562803
75.844893	2416.216325	21.567821
76.434043	2440.041363	21.572839
76.497741	2461.741213	21.577856
76.747668	2473.418380	21.582874
76.579271	2444.935581	21.587891
76.900346	2447.601221	21.592909
77.138919	2455.450150	21.597927
76.915964	2453.543238	21.602944
76.948897	2446.013430	21.607962
77.223077	2460.461140	21.612979
77.165161	2445.904543	21.617997
77.134041	2431.537596	21.623015
77.190779	2449.123094	21.628032
77.093965	2485.854611	21.633050
77.382030	2464.925080	21.638067
77.161249	2460.998047	21.643085
77.583733	2472.219798	21.648103
77.543256	2486.688430	21.653120
77.408874	2481.553010	21.658138
77.801683	2466.037014	21.663155
77.851765	2459.929142	21.668173
77.993727	2495.296041	21.673191
78.461358	2503.763538	21.678208
78.416148	2505.327297	21.683226
78.394119	2473.041711	21.688243
78.207433	2483.101337	21.693261
78.215684	2489.067777	21.698279
78.536320	2510.568373	21.703296
78.497854	2502.550413	21.708314
78.833365	2489.404913	21.713331
79.048457	2492.045365	21.718349
79.122481	2494.595562	21.723367
78.978524	2494.087577	21.728384
79.010205	2499.926152	21.733402
79.081502	2490.037789	21.738419
79.220605	2510.299289	21.743437
79.124604	2507.556163	21.748455
79.055785	2487.530325	21.753472
78.848553	2488.884278	21.758490
79.399475	2495.438304	21.763507
79.479362	2514.918772	21.768525
79.248829	2513.335102	21.773543
79.537704	2518.588356	21.778560
79.390872	2531.677182	21.783578
79.283787	2502.070536	21.788595
79.543850	2522.615560	21.793613
79.711214	2550.091019	21.798631
80.047850	2554.364493	21.803648
79.807831	2543.889644	21.808666
80.384759	2543.551467	21.813683
80.080989	2566.569475	21.818701
80.086715	2558.197976	21.823719
80.077131	2555.177019	21.828736
80.269341	2587.072178	21.833754
80.517116	2583.854578	21.838771
80.532045	2566.319346	21.843789
80.787339	2578.160248	21.848807
80.794672	2576.276281	21.853824
80.518196	2591.718908	21.858842
81.182450	2586.544973	21.863859
81.134298	2590.652745	21.868877
81.260100	2609.082200	21.873895
81.437565	2592.573270	21.878912
81.485546	2608.452975	21.883930
81.799717	2598.968438	21.888947
81.700696	2608.766059	21.893965
81.639868	2599.893013	21.898983
81.777911	2600.731721	21.904000
81.511702	2608.582263	21.909018
82.036433	2586.636832	21.914035
81.710648	2599.985961	21.919053
81.935621	2606.782254	21.924071
81.898371	2588.635041	21.929088
81.807503	2584.486341	21.934106
82.141756	2609.267800	21.939123
82.277433	2616.559293	21.944141
82.229673	2603.501631	21.949159
82.689407	2594.632909	21.954176
82.736543	2610.837314	21.959194
82.890262	2609.915819	21.964211
82.797066	2603.556803	21.969229
82.617850	2578.388438	21.974247
82.877469	2596.748530	21.979264
82.401825	2605.153876	21.984282
82.920560	2607.912455	21.989299
83.327673	2635.752918	21.994317
83.118013	2635.679345	21.999335
83.196006	2619.151789	22.004352
83.270980	2634.287995	22.009370
83.442491	2625.210818	22.014387
83.258228	2629.359002	22.019405
83.375036	2614.890088	22.024423
83.527750	2611.029823	22.029440
83.426636	2635.788595	22.034458
83.816235	2662.443789	22.039475
83.686281	2652.184305	22.044493
83.801653	2655.188457	22.049511
83.975457	2656.660143	22.054528
83.772642	2650.674879	22.059546
84.107134	2669.681645	22.064563
84.287477	2678.773794	22.069581
84.116613	2680.465996	22.074599
84.591099	2691.319131	22.079616
84.420060	2679.572143	22.084634
84.546088	2678.860308	22.089651
84.744136	2692.678784	22.094669
84.835876	2684.323510	22.099687
84.738362	2685.143282	22.104704
84.736577	2706.317170	22.109722
85.185841	2701.213167	22.114739
85.125707	2716.780974	22.119757
85.300443	2718.755001	22.124775
85.845230	2711.373324	22.129792
85.404373	2714.862849	22.134810
85.616326	2719.085920	22.139827
85.288325	2712.198022	22.144845
85.391677	2743.295705	22.149863
85.649858	2728.148101	22.154880
85.640969	2723.753763	22.159898
85.902583	2735.273512	22.164915
86.087814	2737.919729	22.169933
86.104537	2757.501481	22.174951
86.158858	2752.304083	22.179968
86.310927	2773.964774	22.184986
86.200184	2765.825174	22.190003
86.622916	2781.805906	22.195021
86.501870	2770.793989	22.200039
86.882425	2757.622514	22.205056
86.970122	2779.616640	22.210074
86.748138	2768.888691	22.215091
86.795408	2761.626992	22.220109
86.828554	2774.809889	22.225127
87.211186	2779.845406	22.230144
87.195895	2782.601919	22.235162
87.598997	2797.415992	22.240179
87.715097	2787.529089	22.245197
87.270952	2794.079978	22.250215
87.317912	2799.399481	22.255232
87.669460	2796.079858	22.260250
87.576906	2779.820830	22.265267
88.070960	2791.317958	22.270285
87.836698	2800.784161	22.275303
88.169570	2797.719755	22.280320
88.037125	2792.822264	22.285338
88.046869	2789.835266	22.290355
88.134553	2817.268078	22.295373
88.034727	2825.730520	22.300391
88.575821	2818.222059	22.305408
88.195969	2822.325459	22.310426
88.227978	2797.076760	22.315443
88.088529	2811.395932	22.320461
88.395099	2835.117513	22.325479
88.667135	2838.502058	22.330496
88.772172	2850.477237	22.335514
88.640774	2839.214063	22.340531
88.872870	2832.682909	22.345549
89.032885	2854.098141	22.350567
89.403124	2864.533447	22.355584
89.538286	2869.747269	22.360602
89.695299	2868.304810	22.365619
89.963365	2867.190413	22.370637
89.923647	2874.769048	22.375655
90.144320	2863.239636	22.380672
89.941646	2874.557112	22.385690
90.156949	2875.626936	22.390707
90.415599	2861.690185	22.395725
90.130698	2837.926866	22.400743
90.181726	2858.118743	22.405760
90.275787	2877.483761	22.410778
90.454834	2856.044027	22.415795
90.615934	2847.135347	22.420813
90.716551	2863.579769	22.425831
90.724093	2873.808710	22.430848
90.129329	2858.062057	22.435866
90.331875	2839.260438	22.440883
90.537168	2870.156519	22.445901
90.669102	2893.648025	22.450919
90.684456	2888.853623	22.455936
90.844259	2894.021852	22.460954
91.102870	2915.202992	22.465971
91.437264	2918.129080	22.470989
91.350803	2925.140932	22.476007
91.704998	2910.177061	22.481024
91.599429	2916.501407	22.486042
91.597610	2917.967498	22.491059
91.692708	2902.300088	22.496077
91.635140	2915.889974	22.501095
92.045125	2936.864855	22.506112
92.066077	2941.434863	22.511130
92.126253	2921.951640	22.516147
92.234852	2938.733363	22.521165
92.287155	2937.233801	22.526183
92.482878	2939.928115	22.531200
92.609277	2947.587001	22.536218
92.381430	2939.356437	22.541235
92.325759	2963.457520	22.546253
92.340673	2974.308460	22.551271
92.845200	2965.815542	22.556288
92.757635	2977.688214	22.561306
92.905514	2990.089440	22.566323
93.176106	2986.749498	22.571341
93.223705	2984.729119	22.576359
93.346016	2987.428881	22.581376
93.382377	3013.908437	22.586394
93.577245	3018.538499	22.591411
93.686523	2993.816605	22.596429
93.371891	2988.958013	22.601447
93.289056	3017.884336	22.606464
93.937898	3027.851916	22.611482
93.684944	3021.007968	22.616499
93.927291	3011.702940	22.621517
93.885431	3039.737208	22.626535
94.495193	3048.684218	22.631552
94.691820	3054.793744	22.636570
94.566748	3056.883095	22.641587
95.048971	3036.619639	22.646605
94.777557	3060.931897	22.651623
95.339863	3060.198342	22.656640
95.189142	3042.188818	22.661658
95.323669	3023.514146	22.666675
95.300095	3014.916166	22.671693
94.997504	3031.965715	22.676711
95.416872	3020.889515	22.681728
95.579720	3031.648145	22.686746
95.481089	3044.349763	22.691763
95.631002	3044.749383	22.696781
95.510245	3049.543996	22.701799
95.286137	3043.608940	22.706816
95.443741	3043.191639	22.711834
95.647901	3043.306738	22.716851
95.853417	3047.742946	22.721869
95.962499	3065.707263	22.726887
96.077078	3077.893813	22.731904
96.149393	3076.672393	22.736922
96.022905	3067.201731	22.741939
96.402839	3063.607708	22.746957
96.536939	3099.441808	22.751975
96.323166	3102.704940	22.756992
96.646364	3088.507939	22.762010
96.457424	3096.853183	22.767027
96.803661	3107.028478	22.772045
96.860446	3121.368655	22.777063
96.956828	3118.739086	22.782080
97.488080	3123.955253	22.787098
97.233292	3127.213949	22.792115
97.592647	3116.559754	22.797133
97.222822	3127.749542	22.802151
97.210986	3116.983672	22.807168
97.428702	3140.863697	22.812186
97.243646	3156.388030	22.817203
97.969407	3155.647932	22.822221
97.962166	3150.030701	22.827239
97.823483	3156.804267	22.832256
98.081950	3182.045972	22.837274
98.082289	3194.265268	22.842291
98.621383	3180.912726	22.847309
98.696680	3168.481424	22.852327
98.716675	3176.416048	22.857344
98.795795	3173.170690	22.862362
98.617778	3170.379193	22.867379
99.255483	3180.998643	22.872397
98.893502	3196.552449	22.877415
99.051683	3212.157704	22.882432
99.260800	3205.087730	22.887450
99.428951	3212.917782	22.892467
99.598522	3214.772661	22.897485
99.820803	3218.355060	22.902503
99.434421	3216.378019	22.907520
99.614600	3199.610539	22.912538
99.520946	3225.484059	22.917555
99.834235	3232.365435	22.922573
99.923797	3223.178824	22.927591
100.235677	3224.866504	22.932608
100.225701	3232.635655	22.937626
100.168615	3239.436715	22.942643
100.339497	3213.489656	22.947661
100.534886	3247.620259	22.952679
100.350575	3276.354408	22.957696
100.519060	3259.458298	22.962714
100.928410	3254.336894	22.967731
100.822574	3233.329891	22.972749
101.054998	3244.176178	22.977767
101.038817	3260.072668	22.982784
101.503522	3265.422702	22.987802
101.305859	3264.346065	22.992819
101.697019	3267.028811	22.997837
102.006054	3294.385547	23.002855
101.603684	3282.841463	23.007872
102.016915	3270.887647	23.012890
101.996000	3276.746822	23.017907
102.151636	3281.870599	23.022925
102.249743	3264.520216	23.027943
102.009870	3279.909062	23.032960
102.246508	3276.084562	23.037978
101.952438	3271.600592	23.042995
102.527874	3273.638780	23.048013
102.359222	3276.413244	23.053031
102.112591	3275.586405	23.058048
102.463508	3278.690326	23.063066
102.746657	3286.306946	23.068083
102.700778	3301.622817	23.073101
102.768412	3316.740437	23.078119
102.726578	3309.353848	23.083136
103.294125	3308.051365	23.088154
103.200846	3320.286822	23.093171
103.394887	3325.867606	23.098189
103.365004	3334.795887	23.103207
103.382605	3340.940817	23.108224
103.612875	3324.138944	23.113242
103.852645	3344.896667	23.118259
103.986559	3358.393892	23.123277
104.190379	3359.039706	23.128295
104.338676	3337.996274	23.133312
104.441234	3341.313868	23.138330
104.111871	3362.887830	23.143347
104.518457	3366.430755	23.148365
104.616197	3366.212689	23.153383
104.793174	3360.678315	23.158400
105.131401	3367.718607	23.163418
104.995548	3387.087418	23.168435
105.184397	3387.151709	23.173453
105.392793	3368.117597	23.178471
105.186935	3367.977254	23.183488
105.464934	3376.073855	23.188506
105.030343	3392.620074	23.193523
105.135741	3384.623154	23.198541
105.374669	3376.380967	23.203559
105.365389	3405.724954	23.208576
105.771380	3408.261391	23.213594
105.611021	3404.839632	23.218611
105.772525	3421.475947	23.223629
106.034216	3434.523229	23.228647
105.927574	3426.205059	23.233664
106.358067	3428.592386	23.238682
106.252411	3445.554145	23.243699
106.201472	3448.775090	23.248717
106.647741	3463.595074	23.253735
106.698510	3462.195902	23.258752
107.016462	3458.526213	23.263770
106.495533	3463.091043	23.268787
106.932601	3484.203127	23.273805
106.958579	3469.687404	23.278823
107.168989	3483.304172	23.283840
107.644169	3489.382409	23.288858
107.274614	3490.249339	23.293875
107.390652	3512.668727	23.298893
107.901669	3516.402876	23.303911
108.107850	3509.336201	23.308928
108.374605	3513.758488	23.313946
108.462609	3513.633753	23.318963
108.439451	3510.458961	23.323981
108.517665	3489.788288	23.328999
108.472007	3501.581019	23.334016
108.568954	3517.547853	23.339034
108.342266	3522.189265	23.344051
108.739274	3506.155438	23.349069
108.832180	3503.065986	23.354087
108.849664	3518.632602	23.359104
109.077522	3514.420554	23.364122
108.766022	3539.194674	23.369139
108.799328	3534.295539	23.374157
109.130332	3523.605597	23.379175
109.036941	3538.555571	23.384192
109.500371	3557.345887	23.389210
109.488841	3576.076530	23.394227
109.642839	3559.787553	23.399245
109.797005	3541.651088	23.404263
109.270229	3578.328903	23.409280
109.794435	3597.787711	23.414298
109.522299	3603.077941	23.419315
109.739840	3598.563270	23.424333
109.911213	3611.728372	23.429351
110.003621	3624.055423	23.434368
110.507480	3623.029954	23.439386
110.949375	3644.494778	23.444403
111.010426	3659.392579	23.449421
111.416796	3633.008299	23.454439
111.444837	3631.304625	23.459456
111.922771	3641.518154	23.464474
111.822127	3657.573486	23.469491
111.783409	3654.387456	23.474509
112.184939	3634.384172	23.479527
111.965156	3636.842765	23.484544
111.898646	3650.584566	23.489562
111.953814	3643.796700	23.494579
112.011298	3617.883251	23.499597
111.872727	3613.314041	23.504615
112.051179	3641.573606	23.509632
112.674881	3661.058571	23.514650
112.521977	3661.948170	23.519667
112.433024	3662.522503	23.524685
112.473848	3654.519777	23.529703
112.683276	3671.864922	23.534720
112.817488	3668.029694	23.539738
112.952950	3673.774604	23.544755
113.139850	3679.673207	23.549773
113.672436	3699.522855	23.554791
113.403389	3701.398306	23.559808
113.785037	3679.649958	23.564826
113.727968	3671.755124	23.569843
114.090437	3676.197663	23.574861
114.073908	3689.433248	23.579879
113.975986	3698.177524	23.584896
113.831053	3689.219329	23.589914
113.963349	3698.168852	23.594931
114.289779	3718.968070	23.599949
114.082982	3732.027470	23.604967
114.105842	3713.951474	23.609984
114.475278	3716.445385	23.615002
114.785182	3742.523343	23.620019
114.856562	3760.260662	23.625037
114.943679	3742.997969	23.630055
114.867617	3748.261755	23.635072
114.882399	3767.923647	23.640090
115.079827	3762.656991	23.645107
115.068958	3777.197329	23.650125
115.475055	3766.859352	23.655143
115.431111	3771.270853	23.660160
115.837288	3801.931291	23.665178
116.124030	3787.565869	23.670195
115.689940	3793.428358	23.675213
116.218184	3788.313118	23.680231
116.156997	3806.419417	23.685248
116.294632	3798.038440	23.690266
116.380473	3787.810844	23.695283
116.211329	3820.951844	23.700301
116.456566	3834.410816	23.705319
116.365202	3823.333798	23.710336
115.932906	3818.509343	23.715354
116.756014	3855.907216	23.720371
116.933272	3859.848559	23.725389
117.514960	3835.919838	23.730407
117.377117	3829.921999	23.735424
117.385293	3840.150097	23.740442
117.851439	3884.504585	23.745459
117.688733	3873.784769	23.750477
118.218729	3856.779850	23.755495
118.202987	3871.054367	23.760512
118.234452	3867.989168	23.765530
118.351822	3870.871780	23.770547
118.137473	3894.091933	23.775565
118.446587	3868.465795	23.780583
118.400268	3864.362141	23.785600
118.694091	3894.417748	23.790618
118.848470	3902.107916	23.795635
118.686657	3900.550142	23.800653
118.961185	3905.016335	23.805671
118.884913	3892.108544	23.810688
118.971057	3901.185488	23.815706
119.309565	3929.837216	23.820723
119.429002	3942.340359	23.825741
119.628664	3933.057973	23.830759
119.731811	3925.298533	23.835776
119.662020	3937.951436	23.840794
120.130473	3937.383936	23.845811
120.465976	3957.206840	23.850829
120.038649	3959.817487	23.855847
120.144651	3948.688870	23.860864
120.190393	3947.899503	23.865882
120.473094	3987.480760	23.870899
120.821322	3990.573068	23.875917
120.911477	3966.798590	23.880935
120.757762	3971.456816	23.885952
120.882039	3981.727434	23.890970
121.467977	3995.048365	23.895987
121.385670	4014.552214	23.901005
121.797077	4000.336655	23.906023
121.763463	3994.831933	23.911040
121.994976	3999.133223	23.916058
122.083993	3990.472201	23.921075
121.973893	4010.647133	23.926093
122.443852	4006.851221	23.931111
122.198561	4001.080310	23.936128
121.934612	3986.286240	23.941146
122.242872	4015.834412	23.946163
122.344494	4020.587855	23.951181
122.894184	4036.241845	23.956199
122.959966	4034.097663	23.961216
122.705063	4028.227154	23.966234
123.107045	4043.596521	23.971251
122.966164	4063.230969	23.976269
123.194423	4060.354462	23.981287
123.015289	4058.577893	23.986304
123.120588	4081.668348	23.991322
123.415302	4076.597902	23.996339
123.285626	4084.993330	24.001357
123.625764	4086.645732	24.006375
124.002856	4104.985653	24.011392
123.975917	4114.229825	24.016410
124.609550	4125.430497	24.021427
124.331864	4126.662575	24.026445
124.545377	4120.310321	24.031463
124.417887	4116.467441	24.036480
124.453219	4137.508621	24.041498
124.784957	4135.317330	24.046515
124.729454	4152.139102	24.051533
125.070168	4153.879207	24.056551
124.920219	4136.569032	24.061568
124.806623	4143.231605	24.066586
125.712146	4174.088408	24.071603
125.454886	4172.419612	24.076621
125.908575	4172.251377	24.081639
125.764646	4182.157804	24.086656
125.483371	4177.986399	24.091674
126.262412	4175.758197	24.096691
126.364047	4200.258818	24.101709
126.373032	4216.595222	24.106727
126.600081	4194.519747	24.111744
126.159622	4193.733543	24.116762
126.757179	4195.217444	24.121779
126.912198	4232.869728	24.126797
127.113779	4237.907889	24.131815
127.355183	4219.584964	24.136832
127.006470	4224.508547	24.141850
127.344677	4225.591229	24.146867
127.498716	4244.329574	24.151885
127.792370	4236.095606	24.156903
128.056481	4235.010310	24.161920
128.056512	4246.742912	24.166938
128.130116	4254.107641	24.171955
128.300715	4263.055886	24.176973
128.459338	4256.361086	24.181991
128.378188	4269.005506	24.187008
128.554351	4256.774175	24.192026
128.621296	4247.769820	24.197043
128.560158	4266.433909	24.202061
128.801299	4284.852017	24.207079
128.847500	4272.533097	24.212096
128.680895	4283.003155	24.217114
129.270902	4297.214585	24.222131
128.901936	4307.954703	24.227149
129.150317	4324.011515	24.232167
129.754823	4313.707319	24.237184
129.741074	4323.685235	24.242202
129.557482	4332.158995	24.247219
130.025377	4352.881363	24.252237
130.087638	4349.700748	24.257255
130.481118	4348.651941	24.262272
130.478456	4349.801192	24.267290
130.723512	4358.467514	24.272307
130.729370	4380.178438	24.277325
130.793550	4382.059929	24.282343
130.961697	4376.876051	24.287360
130.997026	4376.249402	24.292378
131.248212	4384.554895	24.297395
131.449489	4386.236181	24.302413
131.647703	4406.583511	24.307431
131.837287	4392.510937	24.312448
132.004584	4411.250443	24.317466
132.431842	4406.209562	24.322483
132.349936	4419.041626	24.327501
132.091156	4423.485464	24.332519
132.356590	4415.623769	24.337536
132.217974	4412.052331	24.342554
132.879272	4405.293698	24.347571
132.964118	4429.417546	24.352589
132.672248	4457.856312	24.357607
132.844497	4435.623412	24.362624
132.984229	4428.866307	24.367642
133.128820	4433.875762	24.372659
133.126177	4452.529622	24.377677
133.101652	4473.096515	24.382695
133.312999	4463.987075	24.387712
133.124987	4455.881003	24.392730
133.366892	4474.746049	24.397747
133.332499	4503.252587	24.402765
133.675872	4503.223048	24.407783
134.162582	4505.337092	24.412800
134.121019	4529.723709	24.417818
134.326111	4516.704735	24.422835
134.433566	4531.758302	24.427853
134.851272	4550.125899	24.432871
134.784059	4561.733632	24.437888
134.745784	4558.823518	24.442906
135.204320	4546.249245	24.447923
135.562642	4583.188881	24.452941
135.514409	4592.497485	24.457959
135.807072	4591.842479	24.462976
135.694322	4600.718844	24.467994
135.716541	4578.196363	24.473011
136.175437	4579.108739	24.478029
136.024319	4599.893565	24.483047
136.390413	4594.774543	24.488064
136.359216	4616.524990	24.493082
136.678831	4601.178009	24.498099
136.621521	4601.286329	24.503117
136.659532	4643.777750	24.508135
137.031847	4643.261941	24.513152
137.305559	4633.389353	24.518170
137.082819	4624.657445	24.523187
136.937368	4650.883040	24.528205
137.349240	4677.780752	24.533223
137.966260	4665.456176	24.538240
137.726559	4648.630331	24.543258
137.719945	4675.849940	24.548275
138.195602	4688.672773	24.553293
138.180842	4694.444853	24.558311
138.519392	4707.157681	24.563328
138.266614	4701.216879	24.568346
138.755845	4691.562971	24.573363
138.684569	4709.643448	24.578381
138.780949	4743.395685	24.583399
139.149398	4727.384612	24.588416
139.090449	4713.079984	24.593434
139.051528	4741.113697	24.598451
139.257671	4746.913862	24.603469
139.126579	4749.785528	24.608487
139.667081	4750.118689	24.613504
139.804848	4779.503578	24.618522
139.878613	4787.907108	24.623539
140.011863	4786.518205	24.628557
140.214640	4806.026335	24.633575
140.715444	4823.477775	24.638592
140.659809	4821.364571	24.643610
140.648924	4798.311417	24.648627
140.755583	4818.722841	24.653645
140.781976	4827.175952	24.658663
141.258027	4827.938266	24.663680
141.242439	4839.427047	24.668698
141.509809	4839.812428	24.673715
142.019769	4837.658127	24.678733
141.933958	4841.098311	24.683751
142.222647	4863.378134	24.688768
142.224849	4866.402600	24.693786
142.284577	4852.083352	24.698803
142.598471	4857.534653	24.703821
142.436914	4881.058186	24.708839
142.865581	4867.865756	24.713856
142.800944	4852.612335	24.718874
142.771154	4841.626382	24.723891
143.122542	4865.186395	24.728909
142.922814	4872.902880	24.733927
143.139898	4883.491832	24.738944
143.102943	4885.592851	24.743962
142.980234	4887.554103	24.748979
143.445630	4918.179214	24.753997
143.341225	4937.675668	24.759015
143.616785	4917.367534	24.764032
143.570062	4932.674919	24.769050
143.661119	4963.338743	24.774067
144.169099	4957.818205	24.779085
144.311028	4986.960672	24.784103
144.588112	4995.270089	24.789120
145.024571	4976.336876	24.794138
144.855894	4974.939183	24.799155
145.039124	5001.120507	24.804173
144.931412	5027.857827	24.809191
145.600484	5007.802667	24.814208
145.344187	5004.946998	24.819226
145.574175	5041.897120	24.824243
145.710521	5057.502334	24.829261
145.968287	5055.234163	24.834279
146.046019	5034.996753	24.839296
146.187441	5060.447284	24.844314
146.263358	5069.420696	24.849331
146.560204	5072.340610	24.854349
146.408911	5074.568816	24.859367
147.077668	5103.777211	24.864384
146.729879	5100.222852	24.869402
146.734968	5100.785831	24.874419
147.163536	5129.204816	24.879437
146.989604	5133.852948	24.884455
147.388219	5144.214443	24.889472
147.587460	5160.168823	24.894490
147.850294	5152.778062	24.899507
148.557614	5155.446307	24.904525
148.419820	5167.187023	24.909543
148.565585	5174.582391	24.914560
148.593960	5164.092515	24.919578
149.001153	5166.883189	24.924595
148.909996	5179.054404	24.929613
149.086361	5191.096384	24.934631
149.369734	5182.876215	24.939648
149.569161	5182.611796	24.944666
149.044151	5199.851655	24.949683
149.557242	5215.624310	24.954701
149.670000	5222.340890	24.959719
149.773041	5215.406432	24.964736
149.580047	5217.052561	24.969754
149.767120	5250.172002	24.974771
149.941238	5242.346241	24.979789
149.969779	5268.270104	24.984807
150.186834	5282.105080	24.989824
150.653297	5276.075530	24.994842
150.504766	5285.590496	24.999859
151.118918	5301.596546	25.004877
151.070202	5321.196486	25.009895
151.127238	5311.596287	25.014912
151.674177	5312.439043	25.019930
151.597933	5335.489311	25.024947
151.985040	5332.378840	25.029965
152.239740	5329.669785	25.034983
152.288951	5360.939749	25.040000
152.549955	5356.013834	25.045018
152.450314	5369.877988	25.050035
153.018756	5368.115542	25.055053
152.947765	5363.439369	25.060071
153.014744	5346.108931	25.065088
152.997019	5364.978981	25.070106
152.745932	5375.890516	25.075123
153.248236	5380.925820	25.080141
153.178913	5386.793002	25.085159
153.307921	5398.224050	25.090176
153.599412	5392.380066	25.095194
153.703699	5423.731215	25.100211
154.053310	5415.272020	25.105229
153.904796	5425.393387	25.110247
154.014402	5436.253634	25.115264
154.561651	5443.654843	25.120282
154.949082	5431.773916	25.125299
154.764457	5439.859850	25.130317
155.264688	5472.911880	25.135335
155.238078	5467.942899	25.140352
155.556480	5478.078886	25.145370
155.334169	5480.456291	25.150387
155.372513	5489.295990	25.155405
155.454188	5495.929238	25.160423
155.967920	5493.863602	25.165440
156.014188	5500.899962	25.170458
156.018739	5521.726833	25.175475
156.373209	5508.781173	25.180493
156.194570	5531.068696	25.185511
156.277292	5535.478470	25.190528
156.752321	5547.740286	25.195546
157.023005	5568.010626	25.200563
157.130755	5563.194619	25.205581
157.266726	5580.339855	25.210599
157.352272	5595.456344	25.215616
157.843947	5599.081208	25.220634
157.521542	5600.073532	25.225651
158.090812	5621.315124	25.230669
158.341209	5622.588805	25.235687
158.898804	5621.032071	25.240704
158.717050	5635.600612	25.245722
158.362361	5614.726779	25.250739
158.930956	5622.647406	25.255757
159.317171	5654.071733	25.260775
159.052946	5650.442412	25.265792
159.030730	5639.769620	25.270810
159.132769	5648.709127	25.275827
159.559951	5663.657417	25.280845
159.650761	5693.436849	25.285863
159.653497	5680.030241	25.290880
160.080813	5678.515895	25.295898
159.813423	5700.083642	25.300915
160.436530	5712.140403	25.305933
160.333528	5727.903561	25.310951
160.401477	5731.742965	25.315968
160.407740	5738.818328	25.320986
160.216014	5772.000680	25.326003
160.705002	5776.840666	25.331021
161.092583	5776.551449	25.336039
161.452283	5793.319383	25.341056
161.810717	5797.978968	25.346074
161.996183	5802.311207	25.351091
162.138115	5816.808322	25.356109
162.324254	5813.426221	25.361127
162.383209	5820.692138	25.366144
162.906321	5826.765158	25.371162
162.614451	5837.593590	25.376179
162.864086	5820.902169	25.381197
163.515140	5849.616832	25.386215
163.847037	5853.998518	25.391232
163.791613	5834.017914	25.396250
163.676887	5830.237463	25.401267
164.415859	5817.572919	25.406285
164.116692	5834.350938	25.411303
164.356077	5857.426995	25.416320
164.325110	5841.520151	25.421338
164.452537	5850.578027	25.426355
164.121118	5849.904036	25.431373
164.481708	5839.189512	25.436391
164.440741	5833.332575	25.441408
164.723827	5860.339448	25.446426
164.504290	5891.015077	25.451443
164.768297	5888.582360	25.456461
164.637615	5888.251601	25.461479
164.903604	5918.206861	25.466496
165.476490	5946.762167	25.471514
165.241568	5940.804945	25.476531
165.512206	5947.137854	25.481549
165.905799	5967.090354	25.486567
166.199305	6000.950550	25.491584
166.380445	5999.729230	25.496602
166.360358	6019.626519	25.501619
166.874000	6023.488030	25.506637
166.870722	6030.991510	25.511655
166.992015	6044.881967	25.516672
167.350835	6049.930175	25.521690
167.125989	6066.007134	25.526707
167.450071	6086.066948	25.531725
167.629871	6088.790239	25.536743
167.891891	6091.925961	25.541760
168.106979	6100.170619	25.546778
168.153860	6126.690168	25.551795
168.305404	6120.574526	25.556813
168.608161	6124.483113	25.561831
168.367766	6143.711787	25.566848
168.659878	6136.009796	25.571866
168.955961	6158.958024	25.576883
169.159081	6190.758595	25.581901
169.601977	6194.371975	25.586919
169.663896	6212.775522	25.591936
169.748419	6202.350086	25.596954
170.102154	6216.070782	25.601971
170.176654	6231.992142	25.606989
170.366805	6238.486119	25.612007
170.511943	6252.919718	25.617024
171.040201	6240.396354	25.622042
170.699349	6255.588660	25.627059
170.627644	6276.214552	25.632077
171.064210	6274.120619	25.637095
171.509253	6293.300796	25.642112
171.567558	6302.832208	25.647130
171.676197	6320.277683	25.652147
171.764677	6326.816844	25.657165
172.097743	6314.466237	25.662183
172.371816	6342.714916	25.667200
172.596242	6346.065582	25.672218
173.070127	6341.640851	25.677236
173.122935	6336.544681	25.682253
173.437771	6359.471600	25.687271
173.536807	6366.279138	25.692288
173.877180	6360.719265	25.697306
173.713773	6355.435959	25.702324
174.116621	6353.105833	25.707341
174.194410	6385.092091	25.712359
174.132290	6408.731428	25.717376
174.371165	6387.961654	25.722394
174.425620	6369.211149	25.727412
174.439936	6386.404540	25.732429
174.971652	6376.313013	25.737447
174.889290	6398.733910	25.742464
175.066206	6409.028542	25.747482
175.498238	6415.416085	25.752500
175.228450	6419.218540	25.757517
175.685617	6433.119601	25.762535
175.602834	6447.570565	25.767552
175.763258	6429.604527	25.772570
175.953051	6440.159282	25.777588
175.659834	6453.312606	25.782605
176.073778	6465.106453	25.787623
176.551621	6493.282362	25.792640
176.394401	6490.419888	25.797658
176.769738	6495.982889	25.802676
176.802213	6525.522339	25.807693
176.949214	6523.113190	25.812711
177.126816	6529.501476	25.817728
177.370163	6566.692006	25.822746
177.566258	6566.106824	25.827764
177.787759	6570.393162	25.832781
178.144262	6576.438883	25.837799
178.375708	6609.343225	25.842816
178.559338	6629.559243	25.847834
179.042301	6628.624658	25.852852
178.648690	6608.938732	25.857869
179.145595	6642.363911	25.862887
179.008699	6666.417218	25.867904
179.403030	6649.908512	25.872922
179.525646	6674.244185	25.877940
179.487418	6680.493765	25.882957
179.918227	6697.681288	25.887975
179.698198	6707.710168	25.892992
180.095201	6710.750477	25.898010
180.613302	6732.793867	25.903028
180.459104	6763.291883	25.908045
180.826418	6764.125033	25.913063
180.847088	6780.940597	25.918080
181.146260	6784.577864	25.923098
181.340265	6784.932897	25.928116
181.781743	6806.370472	25.933133
181.773773	6817.794087	25.938151
181.770864	6848.652752	25.943168
182.286769	6839.273473	25.948186
182.374243	6834.589576	25.953204
182.567376	6860.504635	25.958221
182.767587	6869.636521	25.963239
182.610902	6884.447386	25.968256
183.118425	6873.104655	25.973274
183.652567	6900.512452	25.978292
183.516494	6908.009943	25.983309
183.830186	6902.407433	25.988327
183.864702	6933.641233	25.993344
184.287466	6938.162957	25.998362
184.435589	6919.713288	26.003380
184.390534	6935.029840	26.008397
184.975667	6957.251865	26.013415
184.922009	6977.313025	26.018432
184.904114	6970.929340	26.023450
185.171888	6957.735360	26.028468
184.859214	6981.531540	26.033485
185.195759	7009.866784	26.038503
185.638518	7011.840001	26.043520
185.581347	7012.031788	26.048538
185.764634	7034.056504	26.053556
185.709598	7058.116572	26.058573
186.016087	7073.639384	26.063591
185.780860	7077.028749	26.068608
186.298933	7106.475672	26.073626
186.843226	7086.951151	26.078644
186.570693	7116.248761	26.083661
187.346451	7143.987982	26.088679
186.992430	7148.471160	26.093696
187.345151	7145.288449	26.098714
187.484213	7147.907618	26.103732
188.039218	7192.516538	26.108749
188.227501	7203.148447	26.113767
188.398606	7203.775424	26.118784
188.669787	7189.892396	26.123802
189.350709	7195.196466	26.128820
189.221628	7220.472737	26.133837
189.556128	7200.579924	26.138855
189.597547	7203.818473	26.143872
189.793183	7222.765370	26.148890
190.153847	7229.242218	26.153908
190.168704	7244.345204	26.158925
190.350539	7241.153302	26.163943
190.662543	7241.638085	26.168960
190.378924	7247.863072	26.173978
190.952889	7260.890720	26.178996
190.981503	7267.267306	26.184013
191.274718	7272.942595	26.189031
191.060319	7298.653625	26.194048
191.332106	7296.933692	26.199066
191.652938	7309.874839	26.204084
191.186038	7337.727189	26.209101
191.883966	7350.444622	26.214119
192.144203	7356.660120	26.219136
192.152600	7385.377478	26.224154
192.744491	7397.403695	26.229172
192.494073	7414.228108	26.234189
193.108753	7407.353839	26.239207
193.322403	7429.945051	26.244224
193.585320	7434.974119	26.249242
193.761749	7446.994204	26.254260
193.890156	7465.446120	26.259277
194.441116	7450.525135	26.264295
194.327205	7460.784246	26.269312
194.324766	7484.236571	26.274330
195.043679	7485.907882	26.279348
194.723416	7511.607612	26.284365
194.849551	7521.064768	26.289383
195.413046	7526.382054	26.294400
195.165653	7508.639671	26.299418
195.620535	7529.597990	26.304436
195.512251	7574.700726	26.309453
195.862501	7562.851900	26.314471
196.135459	7561.920856	26.319488
196.085006	7588.283339	26.324506
196.401578	7612.476197	26.329524
196.687314	7620.568229	26.334541
196.923686	7628.512487	26.339559
197.248165	7634.031535	26.344576
197.351836	7634.157771	26.349594
197.741752	7636.519789	26.354612
197.404721	7659.874089	26.359629
197.759155	7671.351459	26.364647
197.870210	7687.716369	26.369664
198.296479	7723.337411	26.374682
198.692861	7712.718083	26.379700
198.667596	7710.481730	26.384717
199.036457	7722.426917	26.389735
199.435391	7745.892858	26.394752
199.128580	7762.041796	26.399770
199.709309	7761.360732	26.404788
199.517025	7757.376840	26.409805
199.728930	7777.523513	26.414823
200.009248	7803.400916	26.419840
200.029477	7812.280360	26.424858
200.609561	7815.450512	26.429876
200.224467	7806.378614	26.434893
200.683967	7835.030923	26.439911
200.726102	7851.539699	26.444928
200.775341	7863.983556	26.449946
201.434878	7879.760311	26.454964
201.456327	7898.272147	26.459981
201.996183	7888.096015	26.464999
202.194628	7910.464403	26.470016
202.157655	7943.825814	26.475034
202.555523	7931.287611	26.480052
202.499488	7937.402023	26.485069
202.677544	7956.859107	26.490087
203.049193	7966.507508	26.495104
203.146835	7989.169095	26.500122
203.589490	7975.108985	26.505140
203.476358	7992.151536	26.510157
203.547128	8027.144467	26.515175
204.001164	8023.269511	26.520192
203.937139	8044.041759	26.525210
204.803135	8062.430787	26.530228
204.656906	8081.142231	26.535245
204.826046	8095.296733	26.540263
205.088988	8088.196765	26.545280
205.452207	8076.821101	26.550298
205.909152	8106.177618	26.555316
205.806462	8140.564685	26.560333
205.958222	8131.620478	26.565351
206.380896	8133.814135	26.570368
206.465974	8139.796626	26.575386
206.549891	8156.468145	26.580404
206.956968	8178.147976	26.585421
206.970238	8182.264789	26.590439
207.423873	8180.287898	26.595456
207.273319	8207.463398	26.600474
207.480633	8217.999130	26.605492
207.609727	8233.513416	26.610509
207.953923	8237.573992	26.615527
207.858350	8259.262165	26.620544
207.967121	8267.937432	26.625562
208.599479	8276.781368	26.630580
208.995389	8314.751791	26.635597
208.991717	8318.387082	26.640615
209.687181	8320.921606	26.645632
209.968222	8322.448776	26.650650
210.240273	8332.495832	26.655668
209.945257	8358.490472	26.660685
210.122685	8358.819537	26.665703
210.504212	8366.922117	26.670720
210.440578	8380.719185	26.675738
210.911290	8376.482255	26.680756
210.960454	8400.844158	26.685773
211.135022	8441.867093	26.690791
211.294982	8436.771048	26.695808
211.200114	8439.210137	26.700826
211.922120	8446.193271	26.705844
212.004724	8463.583604	26.710861
211.982532	8500.700511	26.715879
212.383823	8499.914392	26.720896
212.187909	8507.149237	26.725914
212.699035	8536.090425	26.730932
213.049623	8551.691291	26.735949
213.060487	8565.035951	26.740967
213.505998	8574.754432	26.745984
213.417486	8587.494913	26.751002
213.989835	8603.572697	26.756020
213.949191	8596.090277	26.761037
214.168921	8613.979502	26.766055
214.420701	8633.700897	26.771072
214.791570	8626.711234	26.776090
215.235535	8648.188721	26.781108
215.232211	8671.707542	26.786125
215.560387	8646.166140	26.791143
215.722898	8662.885853	26.796160
216.042522	8677.093987	26.801178
216.176302	8692.056636	26.806196
216.474654	8692.090072	26.811213
216.410716	8729.627899	26.816231
216.945349	8723.931144	26.821248
216.849744	8715.200748	26.826266
217.284200	8743.440638	26.831284
217.172305	8761.943227	26.836301
217.790057	8775.909232	26.841319
218.180564	8780.798726	26.846336
218.069511	8799.142913	26.851354
217.761714	8809.397916	26.856372
218.181466	8804.903085	26.861389
218.388415	8826.538115	26.866407
218.342987	8838.261190	26.871424
218.418715	8867.032342	26.876442
218.761867	8887.699831	26.881460
219.374291	8888.536713	26.886477
219.754158	8922.311757	26.891495
220.056894	8944.896726	26.896512
220.123106	8949.653191	26.901530
220.703866	8941.860797	26.906548
221.176177	8961.717077	26.911565
220.892915	8986.141894	26.916583
221.224867	8996.516573	26.921600
221.577265	9004.141493	26.926618
221.587331	9014.868657	26.931636
221.690721	9013.530001	26.936653
221.494877	9040.895565	26.941671
222.033285	9066.820615	26.946688
222.351475	9088.642403	26.951706
222.475217	9084.535075	26.956724
222.802017	9098.576217	26.961741
222.810792	9126.569716	26.966759
223.263532	9130.797681	26.971776
223.571458	9154.299661	26.976794
223.568871	9170.643930	26.981812
223.939285	9174.262505	26.986829
223.990642	9195.948164	26.991847
224.810101	9200.965398	26.996864
224.800554	9218.285936	27.001882
224.998305	9220.220767	27.006900
225.284852	9226.841435	27.011917
225.334361	9247.660303	27.016935
225.731884	9242.105736	27.021952
226.120814	9277.960934	27.026970
226.387946	9288.485137	27.031988
226.579808	9285.630634	27.037005
226.471945	9310.137238	27.042023
227.047893	9304.565772	27.047040
227.292587	9313.684642	27.052058
226.922765	9334.802892	27.057076
227.050533	9354.585058	27.062093
227.401811	9361.532979	27.067111
227.769017	9360.456306	27.072128
227.779828	9399.560985	27.077146
227.858230	9407.064393	27.082164
228.361341	9424.144505	27.087181
228.631876	9455.831847	27.092199
229.163880	9432.488435	27.097216
229.318560	9465.401586	27.102234
229.392675	9490.245437	27.107252
229.850893	9488.275510	27.112269
229.919558	9485.812301	27.117287
230.336029	9498.933208	27.122304
230.562128	9514.544569	27.127322
230.623029	9509.970208	27.132340
231.014159	9513.644511	27.137357
230.866117	9537.782404	27.142375
231.209864	9558.387663	27.147392
231.156310	9580.504690	27.152410
231.214273	9578.470134	27.157428
231.717621	9591.379855	27.162445
231.586389	9623.539546	27.167463
232.583326	9640.083047	27.172480
232.421613	9646.815760	27.177498
232.336174	9656.480071	27.182516
232.686943	9685.908269	27.187533
232.923055	9720.801229	27.192551
233.361612	9735.238773	27.197568
233.384328	9739.719111	27.202586
233.342997	9756.394894	27.207604
234.190524	9780.836529	27.212621
234.313134	9818.172044	27.217639
234.480213	9819.070746	27.222656
234.927215	9845.757291	27.227674
235.041530	9853.876433	27.232692
235.245819	9866.816886	27.237709
235.245192	9895.980594	27.242727
236.036341	9909.528283	27.247744
236.295173	9919.095704	27.252762
236.446617	9950.704468	27.257780
236.857899	9939.815754	27.262797
237.010349	9952.834156	27.267815
237.268151	9974.332391	27.272832
237.491826	10005.273212	27.277850
237.685496	10004.643416	27.282868
237.794194	10009.632628	27.287885
238.239732	10027.229368	27.292903
238.224355	10029.778442	27.297920
238.464710	10063.041000	27.302938
238.258208	10097.754290	27.307956
239.121669	10100.326734	27.312973
239.145748	10111.198042	27.317991
239.581230	10124.258041	27.323008
239.455875	10134.108824	27.328026
239.439311	10160.306946	27.333044
240.067539	10173.521029	27.338061
240.015283	10186.012626	27.343079
240.591547	10224.852627	27.348096
240.761177	10242.469198	27.353114
240.727272	10245.818489	27.358132
241.168066	10263.596652	27.363149
241.556903	10290.242357	27.368167
241.513093	10306.046386	27.373184
241.871624	10328.687911	27.378202
241.999317	10359.130141	27.383220
242.592800	10371.412010	27.388237
243.092785	10392.980285	27.393255
243.204734	10404.053886	27.398272
243.613086	10396.673661	27.403290
243.526308	10436.748529	27.408308
244.308723	10428.022571	27.413325
244.128692	10450.371226	27.418343
244.291160	10478.685931	27.423360
244.933594	10474.073503	27.428378
244.821257	10479.345138	27.433396
245.099042	10490.044821	27.438413
245.469166	10500.396853	27.443431
245.837065	10507.264553	27.448448
246.010073	10514.349561	27.453466
245.869873	10549.715323	27.458484
246.203660	10564.407239	27.463501
246.229637	10564.109962	27.468519
246.572853	10581.263427	27.473536
246.772207	10607.445516	27.478554
246.791455	10644.937894	27.483572
247.352927	10647.531182	27.488589
247.565570	10646.562671	27.493607
247.426832	10676.999903	27.498624
247.896306	10684.210086	27.503642
247.877780	10703.172910	27.508660
248.618782	10728.355137	27.513677
249.137060	10759.398414	27.518695
249.257742	10761.554121	27.523712
249.777602	10771.063964	27.528730
249.550584	10799.519996	27.533748
250.068654	10802.492274	27.538765
250.215943	10828.454896	27.543783
250.215707	10840.918719	27.548800
250.750102	10847.870125	27.553818
250.613539	10865.757743	27.558836
250.966105	10899.861317	27.563853
251.113238	10922.394466	27.568871
251.519452	10930.403703	27.573888
251.966897	10969.095087	27.578906
252.138553	10990.360802	27.583924
252.043111	10990.443559	27.588941
252.455865	11002.424941	27.593959
252.676183	11044.547474	27.598976
252.986031	11063.471440	27.603994
253.547477	11079.215623	27.609012
253.695776	11094.082826	27.614029
253.727312	11102.113092	27.619047
254.154113	11125.039077	27.624064
254.626085	11148.271142	27.629082
254.524135	11170.335355	27.634100
255.004425	11197.874919	27.639117
255.333797	11214.339740	27.644135
255.601403	11209.385721	27.649152
255.615284	11228.216205	27.654170
255.621532	11261.163108	27.659188
256.045214	11286.428579	27.664205
256.534143	11292.112374	27.669223
256.794378	11302.954931	27.674240
257.212400	11338.237300	27.679258
257.447394	11345.373880	27.684276
257.952029	11370.176320	27.689293
258.084787	11395.516812	27.694311
257.912373	11394.819835	27.699328
258.385682	11395.466378	27.704346
258.752416	11432.855933	27.709364
258.908998	11436.776613	27.714381
259.162477	11463.444283	27.719399
259.145384	11478.320264	27.724416
259.461203	11478.805351	27.729434
259.927455	11500.041978	27.734452
260.005791	11534.627832	27.739469
260.067531	11555.117637	27.744487
260.476936	11567.259909	27.749504
261.328618	11574.935922	27.754522
261.230116	11593.205630	27.759540
261.305323	11635.244200	27.764557
261.683390	11644.785873	27.769575
262.127524	11639.886057	27.774592
262.379533	11662.090191	27.779610
262.656641	11684.548588	27.784628
262.823416	11680.528013	27.789645
263.166689	11702.434326	27.794663
263.018547	11715.200551	27.799680
263.575847	11725.635106	27.804698
263.400178	11742.781022	27.809716
263.975640	11762.229110	27.814733
264.316034	11780.685688	27.819751
264.851199	11799.461443	27.824768
265.186953	11795.599617	27.829786
265.161535	11832.182861	27.834804
265.359917	11829.407970	27.839821
266.100794	11855.062288	27.844839
266.024672	11875.788760	27.849856
266.294283	11872.448306	27.854874
266.497227	11903.281226	27.859892
266.812044	11919.980779	27.864909
266.993790	11935.077202	27.869927
267.368304	11958.795263	27.874944
267.856248	11955.336006	27.879962
267.814441	11975.435400	27.884980
267.873803	11995.226635	27.889997
268.456407	12016.799218	27.895015
268.540073	12040.604053	27.900032
269.193340	12040.459133	27.905050
268.858601	12047.684641	27.910068
269.090351	12082.893083	27.915085
269.711096	12115.755978	27.920103
269.730761	12135.078136	27.925120
270.245538	12140.583872	27.930138
270.648859	12166.449649	27.935156
270.727212	12193.522446	27.940173
271.086720	12199.949544	27.945191
271.372376	12240.907206	27.950208
271.785085	12249.522618	27.955226
271.831892	12265.208051	27.960244
271.915148	12269.059911	27.965261
272.433286	12301.069654	27.970279
272.451981	12313.087981	27.975296
272.931331	12320.918830	27.980314
273.203465	12349.507058	27.985332
273.569533	12369.452904	27.990349
273.754412	12380.452019	27.995367
273.522716	12422.171527	28.000384
274.146402	12438.161224	28.005402
274.110123	12454.987091	28.010420
274.769486	12476.587791	28.015437
275.210569	12504.919928	28.020455
275.345208	12525.360328	28.025472
275.592684	12555.582129	28.030490
275.827284	12584.732364	28.035508
276.076672	12585.417533	28.040525
276.604871	12598.056176	28.045543
276.560186	12636.870717	28.050560
277.310811	12656.767568	28.055578
277.494846	12667.777260	28.060596
277.735807	12678.840578	28.065613
278.245874	12700.774272	28.070631
278.265634	12733.355647	28.075648
278.538342	12751.355792	28.080666
278.822011	12748.603680	28.085684
279.225362	12783.390625	28.090701
279.673690	12802.200025	28.095719
279.472917	12828.003601	28.100736
280.141733	12808.513360	28.105754
280.399401	12817.082217	28.110772
280.338470	12840.309463	28.115789
280.698848	12853.268307	28.120807
280.972360	12866.707101	28.125824
281.157744	12878.071224	28.130842
281.331598	12915.998724	28.135860
281.472547	12921.304155	28.140877
281.621055	12953.923003	28.145895
281.783126	12999.654257	28.150912
281.950749	12995.493773	28.155930
282.697637	13040.235154	28.160948
282.746379	13056.984579	28.165965
282.927791	13096.226106	28.170983
283.233195	13126.121923	28.176000
283.564205	13131.738721	28.181018
283.796621	13143.318212	28.186036
284.172470	13179.113441	28.191053
284.589396	13215.849706	28.196071
284.829011	13236.626609	28.201088
285.139638	13265.314887	28.206106
285.613829	13267.935643	28.211124
286.222485	13298.793239	28.216141
286.731759	13337.126402	28.221159
286.646125	13341.461783	28.226176
287.232032	13333.244945	28.231194
287.431946	13371.106186	28.236212
287.487371	13400.385192	28.241229
287.917180	13393.684676	28.246247
287.891068	13410.098617	28.251264
288.065786	13440.189142	28.256282
288.842621	13474.540086	28.261300
288.696276	13488.218937	28.266317
289.141139	13514.551146	28.271335
289.012522	13539.978386	28.276352
289.451450	13539.407994	28.281370
290.067509	13583.002571	28.286388
289.969329	13623.735672	28.291405
290.787161	13625.499274	28.296423
290.681077	13670.069768	28.301440
291.255528	13679.392708	28.306458
291.220464	13688.629634	28.311476
291.560088	13732.434155	28.316493
291.903281	13757.589193	28.321511
292.503101	13790.702420	28.326528
292.437580	13803.169086	28.331546
293.031495	13826.247809	28.336564
293.065446	13863.018883	28.341581
293.789415	13873.164958	28.346599
293.908563	13894.287992	28.351616
294.279586	13897.865013	28.356634
294.738018	13926.638774	28.361652
294.657120	13963.997880	28.366669
295.025175	13971.437458	28.371687
295.251332	13984.388663	28.376704
295.810053	14007.837449	28.381722
296.365001	14039.078781	28.386740
296.771919	14060.713869	28.391757
297.799795	14047.903723	28.396775
297.493678	14051.242840	28.401792
297.987057	14077.497836	28.406810
298.176093	14108.089107	28.411828
298.575662	14096.510939	28.416845
299.073254	14114.631453	28.421863
299.429928	14125.927191	28.426880
299.460457	14106.460482	28.431898
299.825722	14100.432929	28.436916
299.388035	14127.450053	28.441933
300.444070	14157.198563	28.446951
300.044823	14155.487140	28.451968
300.421792	14160.287574	28.456986
300.462142	14162.477499	28.462004
300.518541	14210.075602	28.467021
301.158458	14213.917114	28.472039
301.009829	14249.071020	28.477056
301.299834	14256.879740	28.482074
301.498407	14279.090018	28.487092
301.458193	14312.562174	28.492109
301.645477	14360.175338	28.497127
301.798197	14383.252113	28.502144
302.192794	14409.216699	28.507162
302.700192	14454.460906	28.512180
302.623962	14512.825286	28.517197
303.098288	14520.584774	28.522215
303.465557	14545.198941	28.527232
303.998484	14585.116380	28.532250
304.385677	14621.350211	28.537268
304.408205	14654.533797	28.542285
305.122592	14677.199894	28.547303
305.511271	14721.717545	28.552320
305.826791	14734.118825	28.557338
306.279593	14738.604356	28.562356
306.283330	14776.008080	28.567373
306.985859	14816.652870	28.572391
307.131160	14865.021375	28.577408
307.398400	14878.300579	28.582426
308.084190	14879.693772	28.587444
308.110746	14905.978389	28.592461
308.731987	14955.874272	28.597479
309.127561	14975.438707	28.602496
308.908023	14983.670757	28.607514
309.461879	15003.073557	28.612532
309.896817	15038.630717	28.617549
310.080965	15070.428531	28.622567
310.194189	15076.293939	28.627584
310.630732	15094.742378	28.632602
310.870817	15139.919204	28.637620
310.868287	15179.798928	28.642637
312.034953	15183.731722	28.647655
312.096243	15213.556698	28.652672
312.400186	15240.807710	28.657690
312.876328	15254.476608	28.662708
313.043669	15296.586718	28.667725
313.548933	15311.768381	28.672743
313.838168	15313.438291	28.677760
313.701747	15346.036550	28.682778
314.430524	15389.885273	28.687796
314.550676	15415.416181	28.692813
314.986037	15414.291625	28.697831
314.975271	15447.822716	28.702848
314.983158	15471.120371	28.707866
315.792775	15502.595081	28.712884
315.786957	15547.936583	28.717901
316.425791	15560.371755	28.722919
316.650016	15582.042212	28.727936
316.893685	15604.889808	28.732954
317.270437	15629.707343	28.737972
317.123013	15660.940199	28.742989
317.877624	15689.288381	28.748007
318.370378	15715.470497	28.753024
318.479239	15735.455123	28.758042
318.854235	15779.851867	28.763060
318.968044	15807.660009	28.768077
319.265214	15831.310664	28.773095
319.830899	15851.196323	28.778112
320.125733	15880.304731	28.783130
320.682015	15906.304889	28.788148
320.745277	15925.329683	28.793165
320.859241	15950.350287	28.798183
321.497655	15977.336107	28.803200
321.965826	15993.867204	28.808218
322.387628	16007.413340	28.813236
322.390508	16051.544514	28.818253
322.738102	16064.389072	28.823271
323.083965	16078.262994	28.828288
323.191623	16114.596768	28.833306
323.980657	16132.321545	28.838324
324.077483	16153.473272	28.843341
324.287607	16176.579359	28.848359
324.491457	16199.138094	28.853376
324.463517	16218.955226	28.858394
324.968488	16249.157939	28.863412
325.141916	16286.217188	28.868429
325.593705	16304.926090	28.873447
326.050288	16340.788254	28.878464
326.111636	16393.196956	28.883482
326.704576	16411.239678	28.888500
327.035513	16437.210147	28.893517
327.558776	16470.190212	28.898535
327.860795	16501.998141	28.903552
327.896356	16532.200130	28.908570
328.370958	16549.387902	28.913588
328.884698	16587.548364	28.918605
329.385138	16633.573587	28.923623
330.032978	16645.212246	28.928640
329.967180	16657.600770	28.933658
330.345724	16692.516839	28.938676
330.530883	16717.236879	28.943693
330.681679	16741.838131	28.948711
331.077968	16764.072726	28.953728
331.395178	16795.216807	28.958746
331.547278	16826.941394	28.963764
332.094287	16870.244175	28.968781
332.359128	16893.444676	28.973799
332.722106	16909.825452	28.978816
333.037807	16946.930463	28.983834
333.652133	16983.198227	28.988852
333.837145	17021.552698	28.993869
334.182842	17029.331493	28.998887
334.785466	17054.131220	29.003904
334.766050	17112.898982	29.008922
335.091578	17119.800164	29.013940
335.566009	17146.855991	29.018957
335.822899	17178.444171	29.023975
336.549323	17199.682362	29.028992
336.713318	17230.148104	29.034010
337.249964	17249.283782	29.039028
336.975282	17280.047458	29.044045
337.440896	17310.417817	29.049063
338.224777	17318.182674	29.054080
338.525933	17362.980475	29.059098
338.901065	17395.436846	29.064116
339.335915	17416.252254	29.069133
339.591977	17432.824582	29.074151
340.319546	17448.843069	29.079168
340.316330	17484.821531	29.084186
340.587224	17493.287452	29.089204
340.688319	17536.394584	29.094221
340.950056	17560.650922	29.099239
341.294367	17594.012703	29.104256
341.682038	17620.888217	29.109274
342.105277	17633.133647	29.114292
342.346726	17667.224949	29.119309
342.820960	17715.998318	29.124327
342.896822	17729.513202	29.129344
342.791410	17749.568786	29.134362
343.432167	17771.064589	29.139380
343.694065	17821.097957	29.144397
344.023365	17857.422627	29.149415
344.378985	17880.842790	29.154432
344.165902	17903.162266	29.159450
345.093495	17934.220287	29.164468
345.287727	17972.353231	29.169485
345.588653	18011.775219	29.174503
346.140492	18031.875450	29.179520
346.259860	18074.435645	29.184538
346.603687	18104.718845	29.189556
347.180464	18132.843753	29.194573
347.541724	18194.969498	29.199591
347.845542	18210.067362	29.204608
348.303939	18241.844956	29.209626
348.423929	18262.398232	29.214644
348.793071	18314.661355	29.219661
349.329543	18342.421316	29.224679
350.258337	18362.927789	29.229696
350.370659	18390.633388	29.234714
350.661649	18426.451825	29.239732
351.288997	18460.971201	29.244749
351.526677	18484.517311	29.249767
352.091459	18488.868757	29.254784
352.296700	18519.750907	29.259802
352.563539	18545.724278	29.264820
352.832651	18575.595128	29.269837
352.852955	18624.936367	29.274855
353.504238	18658.635757	29.279872
353.799492	18683.055288	29.284890
353.976228	18694.566764	29.289908
355.082282	18727.124107	29.294925
355.082791	18776.773270	29.299943
355.543400	18785.440216	29.304960
355.799184	18800.718361	29.309978
356.335632	18818.177286	29.314996
356.711654	18872.015637	29.320013
356.777088	18905.013192	29.325031
357.370810	18915.820737	29.330048
357.676016	18936.185062	29.335066
357.979756	18960.688716	29.340084
358.453722	19001.321795	29.345101
358.481633	19044.088747	29.350119
358.930771	19054.190491	29.355136
359.315135	19073.851535	29.360154
359.693484	19110.610628	29.365172
359.892996	19156.572851	29.370189
359.877531	19189.406228	29.375207
360.356671	19207.046839	29.380224
360.673863	19253.472211	29.385242
360.814642	19288.510315	29.390260
361.435108	19320.748694	29.395277
361.546529	19359.729197	29.400295
362.202398	19397.707213	29.405312
362.533297	19430.394004	29.410330
362.893374	19466.756545	29.415348
363.490041	19507.452564	29.420365
363.829825	19540.089241	29.425383
364.115375	19572.060310	29.430400
364.468176	19597.904494	29.435418
364.679684	19640.387305	29.440436
365.732176	19677.756639	29.445453
366.049969	19697.431001	29.450471
366.537740	19728.519364	29.455488
366.660734	19747.097365	29.460506
366.885513	19769.317076	29.465524
367.252585	19798.928062	29.470541
367.600475	19851.697664	29.475559
367.741896	19858.479095	29.480576
368.171726	19885.743835	29.485594
368.183550	19931.978811	29.490612
368.702200	19950.609899	29.495629
368.912328	19991.520712	29.500647
369.497966	20039.544855	29.505664
369.639074	20054.625578	29.510682
370.172773	20073.446626	29.515700
370.550477	20126.864764	29.520717
370.467160	20172.797716	29.525735
371.393784	20203.163462	29.530752
371.774572	20242.656402	29.535770
371.685380	20275.302341	29.540788
372.375875	20290.730736	29.545805
372.133747	20336.096105	29.550823
372.677483	20386.970275	29.555840
373.297704	20427.313147	29.560858
373.548336	20475.343451	29.565876
374.270301	20496.257196	29.570893
374.521268	20541.229554	29.575911
374.857499	20597.643214	29.580928
375.423015	20621.757714	29.585946
375.899961	20658.119327	29.590964
376.660669	20694.733651	29.595981
376.728256	20718.259022	29.600999
377.330173	20758.583654	29.606016
377.372019	20811.214548	29.611034
378.083804	20826.029875	29.616052
378.652505	20834.481426	29.621069
379.004341	20875.407263	29.626087
379.241284	20905.722713	29.631104
379.652796	20949.296635	29.636122
379.734493	20976.986399	29.641140
380.432993	20992.310086	29.646157
381.013510	21032.356747	29.651175
381.280281	21077.026854	29.656192
381.368413	21094.648949	29.661210
381.397569	21140.329534	29.666228
382.100039	21175.510563	29.671245
382.321459	21222.010864	29.676263
382.883297	21242.799094	29.681280
383.337452	21298.880372	29.686298
383.789937	21329.558241	29.691316
384.088865	21329.343370	29.696333
384.189821	21388.677104	29.701351
385.011764	21438.729786	29.706368
385.147220	21467.663162	29.711386
385.466460	21487.601096	29.716404
386.015401	21523.476628	29.721421
386.423367	21576.921224	29.726439
386.753425	21594.199631	29.731456
387.515483	21625.656112	29.736474
387.429908	21655.206456	29.741492
388.055084	21700.742822	29.746509
388.620852	21744.980673	29.751527
389.112949	21773.612892	29.756544
389.464925	21804.784329	29.761562
389.638362	21832.050479	29.766580
390.001956	21844.663598	29.771597
390.318921	21905.579355	29.776615
390.617496	21942.953803	29.781632
391.398640	21961.963131	29.786650
391.380747	22011.886694	29.791668
391.864807	22037.224285	29.796685
392.127524	22054.221068	29.801703
392.716121	22096.778708	29.806720
393.113092	22142.964078	29.811738
393.285280	22163.348033	29.816756
393.631385	22177.728385	29.821773
393.947452	22217.824733	29.826791
394.338904	22243.959877	29.831808
395.422178	22278.571123	29.836826
395.359790	22313.056396	29.841844
395.698518	22334.948564	29.846861
396.044501	22372.030792	29.851879
396.322202	22401.457806	29.856896
397.077066	22438.296067	29.861914
397.348434	22473.968831	29.866932
398.000876	22514.174281	29.871949
398.284707	22526.336018	29.876967
398.541208	22569.372229	29.881984
399.083307	22611.694500	29.887002
399.138378	22651.965855	29.892020
399.526090	22665.906206	29.897037
399.640992	22704.449379	29.902055
399.933037	22761.486198	29.907072
400.307048	22796.507344	29.912090
400.567574	22838.239774	29.917108
401.183826	22869.598141	29.922125
401.522509	22927.498077	29.927143
402.288997	22972.147455	29.932160
403.306713	23005.270149	29.937178
403.007618	23053.868498	29.942196
403.317594	23086.621105	29.947213
403.932062	23131.395344	29.952231
404.440688	23175.767816	29.957248
404.688901	23204.236240	29.962266
404.547020	23252.512793	29.967284
405.429207	23301.654565	29.972301
405.728908	23348.704380	29.977319
406.273185	23379.303056	29.982336
406.600862	23418.772870	29.987354
406.569900	23478.282417	29.992372
407.502935	23531.824671	29.997389
407.923900	23573.645941	30.002407
408.135451	23604.345712	30.007424
408.670007	23658.945893	30.012442
408.955651	23698.885260	30.017460
409.947617	23738.518847	30.022477
410.490689	23797.469589	30.027495
410.670620	23826.749705	30.032512
411.250564	23871.348728	30.037530
411.701352	23899.452192	30.042548
411.776847	23932.737096	30.047565
412.553641	23962.325628	30.052583
412.673275	24006.490210	30.057600
413.026388	24041.131121	30.062618
413.546732	24083.282530	30.067636
413.964847	24127.850628	30.072653
414.397047	24177.903355	30.077671
414.701788	24205.530073	30.082688
415.215180	24243.853276	30.087706
415.479906	24296.984904	30.092724
416.136464	24330.430030	30.097741
416.156581	24371.144860	30.102759
416.623338	24424.732293	30.107776
417.159470	24469.805264	30.112794
417.623517	24512.492088	30.117812
418.288547	24548.604040	30.122829
418.619821	24591.604688	30.127847
419.003630	24618.397551	30.132864
419.200912	24662.439075	30.137882
419.724931	24717.096454	30.142900
420.013090	24735.534456	30.147917
420.611799	24785.287127	30.152935
421.141620	24834.034327	30.157952
421.412698	24836.364150	30.162970
421.486998	24897.974140	30.167988
422.015751	24946.748646	30.173005
422.798123	24965.887329	30.178023
423.270301	24986.860582	30.183040
423.602122	25040.226282	30.188058
423.719020	25089.669979	30.193076
424.390917	25105.675121	30.198093
424.803559	25148.042498	30.203111
425.043499	25190.053777	30.208128
426.005003	25206.058479	30.213146
425.946675	25259.129812	30.218164
426.438144	25310.607817	30.223181
426.703977	25329.679291	30.228199
427.142051	25367.214900	30.233216
427.853648	25427.359195	30.238234
427.855039	25477.450666	30.243252
428.315203	25497.010571	30.248269
428.787977	25569.000328	30.253287
429.239955	25608.472071	30.258304
429.584012	25631.184434	30.263322
430.051466	25692.240398	30.268340
430.390869	25742.445533	30.273357
430.961308	25795.012586	30.278375
430.885194	25825.212016	30.283392
431.530853	25863.613227	30.288410
431.789314	25942.250058	30.293428
432.484224	25993.381159	30.298445
433.318990	26024.870139	30.303463
433.331033	26083.415126	30.308480
434.487201	26119.286884	30.313498
434.687373	26160.099258	30.318516
435.113197	26223.095661	30.323533
435.633677	26263.238815	30.328551
436.099046	26285.485760	30.333568
436.953527	26328.651955	30.338586
437.199885	26378.376044	30.343604
437.683593	26413.563180	30.348621
438.077262	26453.593697	30.353639
438.375637	26496.047964	30.358656
439.037555	26516.886117	30.363674
439.320110	26567.982986	30.368692
439.685709	26618.132763	30.373709
439.972828	26670.459171	30.378727
439.982677	26701.032295	30.383744
440.521804	26732.110965	30.388762
440.947670	26786.765990	30.393780
441.743768	26849.604198	30.398797
442.616134	26874.022341	30.403815
442.638857	26922.936570	30.408832
443.211695	26956.927407	30.413850
443.379308	27017.706496	30.418868
443.971528	27076.949101	30.423885
444.572092	27105.348532	30.428903
444.687762	27135.282058	30.433920
445.174029	27176.849120	30.438938
445.688719	27246.257563	30.443956
446.303209	27289.976773	30.448973
446.395792	27313.691717	30.453991
446.829748	27355.794563	30.459008
447.447815	27415.500855	30.464026
447.951976	27477.717806	30.469044
448.136502	27513.519615	30.474061
448.630705	27553.458831	30.479079
448.817244	27617.034502	30.484096
449.360958	27665.163028	30.489114
449.867741	27709.844150	30.494132
450.298548	27751.623626	30.499149
450.749244	27804.631405	30.504167
451.438426	27829.115871	30.509184
451.684137	27873.790081	30.514202
451.974496	27945.998200	30.519220
452.591786	27988.069162	30.524237
453.069511	28016.585022	30.529255
453.280739	28071.828413	30.534272
453.863962	28124.799520	30.539290
454.397899	28170.839923	30.544308
454.182198	28213.531611	30.549325
454.941287	28269.943628	30.554343
455.666603	28322.115961	30.559360
456.117880	28372.352925	30.564378
456.579511	28417.443923	30.569396
456.835632	28469.836144	30.574413
457.391377	28526.131193	30.579431
457.995909	28568.240380	30.584448
458.188099	28621.517328	30.589466
458.768527	28699.512772	30.594484
459.048725	28749.447906	30.599501
459.649033	28777.525273	30.604519
460.056686	28838.936696	30.609536
460.957547	28899.071416	30.614554
461.338345	28967.638369	30.619572
461.490147	29001.142933	30.624589
462.422336	29038.259599	30.629607
462.713397	29090.272580	30.634624
463.116647	29153.417541	30.639642
463.709424	29212.572798	30.644660
464.179559	29255.835103	30.649677
464.835958	29284.720994	30.654695
465.355234	29358.944367	30.659712
465.570184	29410.813170	30.664730
466.568689	29441.718359	30.669748
466.749598	29478.086323	30.674765
467.398082	29540.223811	30.679783
467.672074	29608.691088	30.684800
468.288514	29645.596255	30.689818
468.769642	29666.474421	30.694836
469.094802	29721.145956	30.699853
469.225406	29784.865043	30.704871
469.987326	29855.627956	30.709888
470.263326	29896.463499	30.714906
470.964082	29925.743749	30.719924
471.142847	29993.638402	30.724941
471.837738	30032.288453	30.729959
472.028585	30080.122414	30.734976
472.231260	30129.042839	30.739994
472.942998	30197.758738	30.745012
473.221335	30270.041659	30.750029
474.219760	30311.525389	30.755047
474.500295	30368.821407	30.760064
474.974487	30421.959533	30.765082
475.383150	30480.468167	30.770100
475.376280	30529.354934	30.775117
476.256236	30577.694726	30.780135
476.664049	30650.913671	30.785152
477.095102	30706.491949	30.790170
478.014668	30754.090679	30.795188
477.804451	30811.910861	30.800205
478.981047	30875.625213	30.805223
479.271077	30931.328452	30.810240
479.918258	30964.534165	30.815258
480.376105	31008.600995	30.820276
480.482309	31083.590844	30.825293
481.091285	31143.223215	30.830311
481.775752	31193.423548	30.835328
482.062780	31242.181751	30.840346
482.599974	31295.738021	30.845364
483.170701	31349.124874	30.850381
483.961168	31371.790021	30.855399
483.908761	31433.289788	30.860416
484.626485	31472.573370	30.865434
485.218591	31524.247384	30.870452
485.036996	31562.809020	30.875469
486.028406	31616.313332	30.880487
486.385398	31671.853297	30.885504
486.594749	31732.093152	30.890522
487.164366	31788.942289	30.895540
487.533395	31833.435994	30.900557
488.214852	31908.526811	30.905575
488.462750	31956.690912	30.910592
488.921206	32004.347148	30.915610
489.665301	32072.077659	30.920628
490.368137	32123.416523	30.925645
491.008326	32171.440703	30.930663
491.207438	32237.141833	30.935680
491.573571	32294.824400	30.940698
492.482236	32351.720320	30.945716
492.627224	32386.655377	30.950733
493.389761	32457.460325	30.955751
493.493967	32525.433947	30.960768
493.902789	32579.946053	30.965786
494.795883	32630.264342	30.970804
495.343002	32694.729771	30.975821
495.851603	32747.430770	30.980839
496.629377	32794.216134	30.985856
497.061366	32876.580267	30.990874
497.650063	32905.537005	30.995892
498.110543	32945.216594	31.000909
498.628681	33005.047005	31.005927
499.099587	33063.919997	31.010944
499.494905	33114.473338	31.015962
500.185325	33150.506101	31.020980
500.666715	33220.338351	31.025997
500.989252	33278.454127	31.031015
501.558272	33322.710352	31.036032
501.969190	33379.032426	31.041050
502.729215	33457.230929	31.046068
503.706218	33497.908633	31.051085
503.764919	33528.925857	31.056103
504.038739	33585.782359	31.061120
504.187892	33663.628349	31.066138
505.210551	33709.908754	31.071156
505.252590	33765.854438	31.076173
505.716079	33820.339278	31.081191
506.013996	33887.658303	31.086208
506.533710	33946.261156	31.091226
507.070589	34017.201167	31.096244
507.456877	34088.021200	31.101261
508.131004	34150.710408	31.106279
508.517834	34196.589134	31.111296
509.016383	34280.403383	31.116314
509.623360	34349.310668	31.121332
510.108415	34404.052477	31.126349
510.596111	34455.433699	31.131367
511.359639	34528.868825	31.136384
511.581109	34613.623356	31.141402
512.335859	34663.781006	31.146420
512.689460	34715.929777	31.151437
513.277958	34787.135709	31.156455
513.984422	34849.118426	31.161472
514.318043	34906.461530	31.166490
514.964423	34980.246034	31.171508
515.285237	35046.612783	31.176525
515.792035	35086.971098	31.181543
516.336207	35152.184357	31.186560
516.561974	35230.280174	31.191578
517.294076	35281.399393	31.196596
517.683331	35332.588012	31.201613
518.200179	35375.942943	31.206631
518.752328	35452.250360	31.211648
519.172733	35521.271910	31.216666
519.630934	35573.611031	31.221684
520.053070	35623.558129	31.226701
520.577806	35708.816847	31.231719
521.098880	35790.520366	31.236736
521.125116	35856.522276	31.241754
522.359627	35897.693105	31.246772
522.589616	35958.224834	31.251789
523.196883	36043.392637	31.256807
523.847139	36113.599706	31.261824
524.475385	36185.363211	31.266842
525.254493	36229.068194	31.271860
525.716552	36304.668375	31.276877
526.158586	36388.404096	31.281895
526.913825	36440.166568	31.286912
527.021312	36494.746835	31.291930
527.800291	36567.108633	31.296948
528.360523	36640.810127	31.301965
529.005962	36721.383441	31.306983
529.616793	36764.284446	31.312000
530.023217	36815.231509	31.317018
530.755787	36904.885845	31.322036
531.128327	36971.705644	31.327053
531.290034	37039.049648	31.332071
531.983848	37107.385267	31.337088
532.259247	37164.808378	31.342106
532.772035	37232.126677	31.347124
533.634065	37315.153604	31.352141
533.841458	37405.155962	31.357159
534.448655	37458.864539	31.362176
534.745494	37525.193985	31.367194
535.231399	37596.986674	31.372212
536.202191	37691.326661	31.377229
537.047516	37749.679992	31.382247
537.880378	37822.770123	31.387264
538.347953	37896.305899	31.392282
538.988543	37936.995715	31.397300
539.310330	38006.286160	31.402317
539.850799	38092.901210	31.407335
540.653299	38136.755326	31.412352
541.112656	38198.787355	31.417370
541.775414	38256.241502	31.422388
542.636889	38336.350885	31.427405
543.097207	38382.395520	31.432423
543.800000	38442.482003	31.437440
543.704838	38512.187262	31.442458
544.204129	38571.572453	31.447476
544.715516	38642.355204	31.452493
544.720610	38702.374747	31.457511
545.635352	38790.168480	31.462528
545.742352	38861.971997	31.467546
546.272886	38928.520502	31.472564
546.985176	38999.328281	31.477581
547.230563	39086.448160	31.482599
547.877768	39170.065140	31.487616
548.210560	39237.414368	31.492634
549.414528	39306.330555	31.497652
549.887746	39397.261573	31.502669
550.374312	39468.929063	31.507687
551.109997	39541.392065	31.512704
551.584341	39611.768127	31.517722
552.270819	39658.921190	31.522740
552.990327	39722.670311	31.527757
553.306918	39789.973775	31.532775
554.425204	39859.171344	31.537792
554.907074	39896.107540	31.542810
555.324058	39939.471077	31.547828
555.980717	40013.770150	31.552845
556.525994	40088.081612	31.557863
557.189029	40130.994659	31.562880
557.968248	40177.818134	31.567898
558.360302	40241.228637	31.572916
558.664395	40303.195696	31.577933
559.118688	40355.568349	31.582951
559.502464	40409.470969	31.587968
559.903039	40493.216859	31.592986
560.438906	40562.150337	31.598004
561.001925	40621.749520	31.603021
561.497420	40715.580970	31.608039
562.295676	40781.697527	31.613056
562.708740	40834.867456	31.618074
563.217437	40901.991808	31.623092
563.679095	40977.425446	31.628109
564.500492	41047.651909	31.633127
564.681719	41130.073398	31.638144
565.371793	41190.085886	31.643162
565.743565	41275.626663	31.648180
566.617604	41357.363438	31.653197
566.863579	41432.941904	31.658215
567.884128	41514.689906	31.663232
568.321207	41595.423562	31.668250
568.912877	41659.762450	31.673268
569.574865	41745.257495	31.678285
569.689726	41804.385334	31.683303
570.519783	41879.919684	31.688320
571.014327	41965.973713	31.693338
571.633365	42025.779725	31.698356
572.334182	42113.034592	31.703373
572.641597	42196.226033	31.708391
573.642969	42271.768429	31.713408
574.132336	42353.696303	31.718426
574.860396	42429.578056	31.723444
575.637046	42515.111422	31.728461
575.696547	42585.567493	31.733479
576.629998	42640.825351	31.738496
577.451687	42720.465059	31.743514
577.577222	42813.298268	31.748532
578.567858	42883.579596	31.753549
578.804309	42963.392778	31.758567
579.558763	43032.242652	31.763584
580.285256	43102.227516	31.768602
580.735437	43187.622218	31.773620
581.468660	43250.775314	31.778637
581.579660	43315.609784	31.783655
582.290652	43397.748783	31.788672
582.968954	43476.837757	31.793690
583.396361	43546.883181	31.798708
584.581018	43609.991362	31.803725
584.538161	43686.419177	31.808743
585.681881	43768.412594	31.813760
585.794397	43851.735264	31.818778
586.515071	43924.028730	31.823796
587.318406	43985.846876	31.828813
587.586468	44065.899534	31.833831
587.973287	44151.429127	31.838848
588.660214	44225.481439	31.843866
589.376079	44296.612249	31.848884
589.893408	44360.069986	31.853901
590.291594	44468.824925	31.858919
591.499407	44520.586227	31.863936
592.435730	44576.114613	31.868954
592.638284	44639.710537	31.873972
593.357138	44703.783355	31.878989
593.635569	44771.979604	31.884007
594.171930	44836.193517	31.889024
594.586369	44925.617911	31.894042
595.421123	45001.435805	31.899060
596.080945	45051.710569	31.904077
596.449039	45112.098440	31.909095
597.020918	45188.209925	31.914112
597.718823	45254.643304	31.919130
598.207862	45339.908929	31.924148
598.747863	45417.974566	31.929165
599.121601	45496.516307	31.934183
599.513636	45550.214801	31.939200
600.400510	45656.120840	31.944218
601.329127	45743.547840	31.949236
601.923061	45810.249795	31.954253
601.848624	45877.618047	31.959271
602.561867	45955.054296	31.964288
603.037283	46057.630239	31.969306
603.613457	46145.815087	31.974324
604.322460	46241.517992	31.979341
604.916288	46331.737248	31.984359
605.568429	46416.412548	31.989376
606.162267	46491.278595	31.994394
606.320399	46590.402083	31.999412
607.374930	46675.896155	32.004429
608.062494	46759.029528	32.009447
608.692574	46849.655753	32.014464
609.381452	46940.080105	32.019482
609.569022	47024.661229	32.024500
610.431851	47132.562467	32.029517
611.096304	47224.678293	32.034535
611.760505	47302.311355	32.039552
612.265931	47398.631615	32.044570
612.755778	47490.101881	32.049588
613.770789	47576.073899	32.054605
614.198565	47676.873119	32.059623
614.677440	47770.430525	32.064640
615.429040	47846.914691	32.069658
616.002583	47949.554250	32.074676
616.627697	48022.498288	32.079693
617.214303	48123.737833	32.084711
617.889691	48234.022446	32.089728
618.369064	48311.816507	32.094746
618.963599	48411.284858	32.099764
620.120482	48501.863623	32.104781
620.599490	48591.733784	32.109799
621.134677	48667.628649	32.114816
621.808738	48763.324919	32.119834
622.638651	48869.091158	32.124852
623.414785	48935.322580	32.129869
624.027856	49023.843251	32.134887
624.605687	49125.313815	32.139904
625.448539	49208.460785	32.144922
626.107495	49272.237045	32.149940
626.814166	49340.622339	32.154957
627.454927	49436.611716	32.159975
628.299485	49529.507986	32.164992
628.870567	49594.386137	32.170010
629.190173	49662.498629	32.175028
629.803512	49751.928961	32.180045
630.352012	49831.685206	32.185063
631.013891	49924.480949	32.190080
631.770092	50011.226804	32.195098
632.217637	50107.576749	32.200116
632.993575	50159.630251	32.205133
633.373616	50242.990824	32.210151
633.794448	50331.059862	32.215168
634.581127	50391.313452	32.220186
635.027510	50491.357202	32.225204
635.801149	50571.218316	32.230221
636.190815	50661.750955	32.235239
636.876014	50716.694762	32.240256
637.479683	50793.325797	32.245274
638.056363	50902.379016	32.250292
638.820558	51004.567818	32.255309
639.310271	51082.150464	32.260327
639.443203	51168.521335	32.265344
640.364879	51276.265945	32.270362
640.436490	51370.489462	32.275380
641.383576	51456.051330	32.280397
641.695185	51584.132690	32.285415
642.344757	51669.750964	32.290432
642.971724	51759.403214	32.295450
643.628793	51878.760237	32.300468
644.369434	51978.627364	32.305485
645.211068	52093.050503	32.310503
646.084729	52173.186032	32.315520
646.907113	52266.102447	32.320538
647.870705	52387.319610	32.325556
648.440270	52470.440663	32.330573
649.128808	52576.373993	32.335591
649.924137	52664.578255	32.340608
651.186524	52763.876911	32.345626
651.278491	52857.172639	32.350644
651.886855	52933.495614	32.355661
652.529534	53023.710201	32.360679
653.014220	53115.375749	32.365696
653.931561	53211.587912	32.370714
654.220187	53328.326944	32.375732
655.135070	53409.086185	32.380749
655.716182	53508.014783	32.385767
656.055435	53616.971010	32.390784
656.934207	53698.252258	32.395802
657.475474	53807.833168	32.400820
658.086704	53904.478357	32.405837
658.899781	54003.762840	32.410855
659.514918	54103.933337	32.415872
660.261283	54205.643027	32.420890
660.850987	54291.586059	32.425908
661.543469	54383.160120	32.430925
662.078260	54498.741075	32.435943
662.619010	54599.861376	32.440960
663.748365	54708.510044	32.445978
664.375376	54817.905608	32.450996
665.369938	54909.962924	32.456013
666.131893	54992.734532	32.461031
666.528322	55089.143121	32.466048
667.467569	55193.068829	32.471066
667.832456	55285.301402	32.476084
668.374365	55372.223684	32.481101
669.164544	55489.177158	32.486119
669.698239	55580.397700	32.491136
670.791836	55655.668855	32.496154
671.409713	55754.482777	32.501172
671.904788	55868.088334	32.506189
672.777407	55951.957656	32.511207
673.199755	56026.873583	32.516224
673.919355	56134.220588	32.521242
674.217051	56243.842788	32.526260
675.271737	56352.051737	32.531277
675.999922	56426.735465	32.536295
676.488200	56509.722961	32.541312
677.176413	56605.477995	32.546330
677.625890	56720.713423	32.551348
678.420542	56808.895534	32.556365
679.024221	56886.090879	32.561383
679.664848	56974.798298	32.566400
679.844407	57072.800398	32.571418
680.953147	57171.938436	32.576436
681.796136	57259.198452	32.581453
682.716469	57356.744765	32.586471
683.234828	57452.885794	32.591488
684.051589	57539.601697	32.596506
684.471601	57637.301525	32.601524
685.356147	57738.235927	32.606541
686.170238	57831.252932	32.611559
686.608519	57939.667186	32.616576
687.451887	58027.840390	32.621594
687.866812	58113.911194	32.626612
688.766357	58203.826118	32.631629
689.349343	58311.479249	32.636647
690.012911	58419.075427	32.641664
690.860051	58514.838760	32.646682
691.740281	58604.935615	32.651700
692.417335	58697.233726	32.656717
693.145818	58794.945193	32.661735
693.776718	58900.243062	32.666752
694.527139	58977.839381	32.671770
695.009995	59093.929841	32.676788
695.521740	59192.961768	32.681805
696.357364	59293.905856	32.686823
696.913783	59422.345717	32.691840
697.618857	59520.209948	32.696858
698.212838	59617.176760	32.701876
698.620914	59726.629423	32.706893
699.573025	59838.084432	32.711911
700.203393	59962.787350	32.716928
700.816997	60057.869989	32.721946
701.647196	60156.683496	32.726964
702.243208	60267.232884	32.731981
703.201546	60388.964858	32.736999
703.420478	60508.620593	32.742016
704.104276	60621.015287	32.747034
705.029216	60743.462686	32.752052
705.814425	60846.015405	32.757069
706.570653	60955.695345	32.762087
707.588083	61058.318229	32.767104
708.500404	61186.641128	32.772122
709.194311	61292.712170	32.777140
709.941458	61377.787953	32.782157
710.716492	61473.722738	32.787175
711.127271	61603.609890	32.792192
712.141450	61712.644684	32.797210
712.731999	61803.865495	32.802228
713.209291	61913.287059	32.807245
713.893730	62031.819599	32.812263
714.662994	62158.124733	32.817280
715.310893	62255.247062	32.822298
715.891429	62370.297599	32.827316
716.304687	62488.296178	32.832333
717.260356	62599.974479	32.837351
717.926254	62708.876253	32.842368
718.557303	62826.114045	32.847386
719.238976	62955.914590	32.852404
719.904846	63057.834667	32.857421
721.166540	63161.951037	32.862439
721.779800	63277.848208	32.867456
722.611619	63407.020116	32.872474
723.195129	63508.172359	32.877492
723.683607	63612.538811	32.882509
724.712222	63728.787093	32.887527
725.356130	63840.985084	32.892544
725.801826	63926.197206	32.897562
727.009030	64043.359514	32.902580
726.913124	64151.061231	32.907597
727.394665	64266.277899	32.912615
728.313748	64387.585374	32.917632
729.287137	64505.648526	32.922650
730.123396	64624.961182	32.927668
730.952867	64721.287887	32.932685
731.536250	64830.524341	32.937703
732.467212	64962.508694	32.942720
733.461146	65081.001575	32.947738
734.344400	65158.422758	32.952756
734.718995	65262.133809	32.957773
735.576112	65373.407460	32.962791
735.838956	65514.936227	32.967808
737.032136	65606.434848	32.972826
737.790843	65724.926045	32.977844
738.221150	65846.152205	32.982861
739.305623	65970.235559	32.987879
740.160125	66087.271855	32.992896
740.817284	66175.979176	32.997914
741.528005	66288.489257	33.002932
742.134653	66424.777950	33.007949
742.846595	66536.568582	33.012967
743.322056	66655.642873	33.017984
744.093630	66779.808052	33.023002
744.700973	66901.301945	33.028020
745.378886	67013.954138	33.033037
746.373806	67141.485424	33.038055
747.039525	67275.184564	33.043072
748.124579	67400.085536	33.048090
749.180042	67520.074110	33.053108
749.533434	67635.014714	33.058125
750.680724	67765.167026	33.063143
751.248783	67884.144578	33.068160
751.860678	67991.749462	33.073178
752.798287	68119.460578	33.078196
753.498776	68235.725283	33.083213
754.161979	68367.206655	33.088231
754.796417	68502.916488	33.093248
755.501813	68615.920513	33.098266
756.505366	68727.756964	33.103284
756.649614	68875.599422	33.108301
758.109243	69006.061924	33.113319
758.897888	69120.003201	33.118336
759.632400	69228.605708	33.123354
760.156130	69369.200984	33.128372
760.846160	69510.168024	33.133389
761.555378	69611.986883	33.138407
761.947831	69771.003601	33.143424
763.133592	69883.498915	33.148442
763.586775	70024.274598	33.153460
764.254718	70160.489075	33.158477
765.228482	70268.267175	33.163495
765.429665	70417.394486	33.168512
766.418821	70566.190416	33.173530
767.328268	70702.311611	33.178548
768.006393	70838.168408	33.183565
769.229466	70974.694781	33.188583
769.962393	71108.502122	33.193600
770.669076	71250.394805	33.198618
771.326959	71366.538447	33.203636
772.141041	71491.818346	33.208653
772.792837	71632.717361	33.213671
773.802476	71785.280438	33.218688
774.649309	71905.764792	33.223706
775.514513	72009.624325	33.228724
776.165783	72167.187376	33.233741
776.594791	72284.651032	33.238759
777.314035	72395.561199	33.243776
777.952705	72526.939774	33.248794
779.054879	72649.295682	33.253812
779.798959	72760.361718	33.258829
780.508562	72897.105370	33.263847
781.107656	73047.823089	33.268864
781.358202	73176.614072	33.273882
782.520261	73291.489892	33.278900
783.166761	73444.649620	33.283917
784.622715	73574.034338	33.288935
785.517641	73711.207856	33.293952
785.994528	73842.754010	33.298970
786.947517	73980.147296	33.303988
787.703259	74125.617339	33.309005
788.486979	74249.350232	33.314023
789.539000	74376.435214	33.319040
790.056165	74496.267720	33.324058
791.440200	74627.333729	33.329076
792.062450	74771.685623	33.334093
793.185768	74893.532308	33.339111
793.627088	75021.872829	33.344128
794.720447	75167.363708	33.349146
795.249283	75298.669864	33.354164
795.639748	75431.251765	33.359181
796.652733	75549.060521	33.364199
797.583077	75704.225681	33.369216
797.955272	75829.129591	33.374234
798.741966	75974.689175	33.379252
799.178777	76129.894603	33.384269
800.620547	76270.124418	33.389287
801.185005	76406.553816	33.394304
801.842625	76545.719650	33.399322
802.969338	76697.748031	33.404340
804.008583	76850.272551	33.409357
804.499924	76986.426736	33.414375
805.276926	77136.163317	33.419392
806.093096	77277.938517	33.424410
807.169277	77406.384317	33.429428
807.709222	77544.462861	33.434445
808.609142	77689.174041	33.439463
809.783117	77839.140798	33.444480
810.868806	77966.987492	33.449498
811.983918	78110.129066	33.454516
812.152350	78243.707053	33.459533
813.217608	78365.721878	33.464551
814.228994	78515.429165	33.469568
814.650842	78649.688775	33.474586
815.631883	78781.042370	33.479604
816.154196	78931.320240	33.484621
817.071829	79066.563076	33.489639
817.866575	79198.803763	33.494656
818.798284	79358.674946	33.499674
819.730472	79506.624739	33.504692
820.187220	79641.017425	33.509709
820.641173	79772.122391	33.514727
821.824442	79914.397879	33.519744
822.377898	80073.552368	33.524762
823.324187	80206.096616	33.529780
823.383493	80372.343062	33.534797
824.464544	80544.829469	33.539815
825.438373	80682.729458	33.544832
826.128763	80823.485529	33.549850
827.011343	80989.524727	33.554868
828.043317	81124.995243	33.559885
828.768780	81280.182904	33.564903
830.115378	81439.386952	33.569920
830.447878	81573.350037	33.574938
831.483909	81703.832568	33.579956
832.186067	81834.807452	33.584973
832.909658	81975.255326	33.589991
833.909361	82130.068324	33.595008
834.371179	82267.740007	33.600026
835.344035	82425.146678	33.605044
836.068551	82572.221173	33.610061
836.843437	82719.187097	33.615079
837.853111	82873.984583	33.620096
838.488087	83036.999097	33.625114
839.701917	83180.738916	33.630132
840.178258	83324.291449	33.635149
841.081715	83481.887743	33.640167
842.075518	83645.087774	33.645184
842.665769	83791.047341	33.650202
843.596908	83947.870514	33.655220
844.477962	84101.660134	33.660237
845.047865	84261.815768	33.665255
845.744511	84439.348919	33.670272
846.911302	84608.183010	33.675290
848.257240	84756.314123	33.680308
848.580994	84903.602752	33.685325
849.317610	85085.284463	33.690343
850.242305	85233.526184	33.695360
851.066692	85406.155354	33.700378
851.844482	85567.740922	33.705396
852.862988	85734.614927	33.710413
853.696762	85898.009328	33.715431
854.719422	86067.415745	33.720448
855.550430	86241.581172	33.725466
856.909553	86381.223723	33.730484
857.357752	86540.934538	33.735501
858.745078	86701.914949	33.740519
860.978890	86849.096795	33.745536
861.727394	86988.211149	33.750554
862.871748	87119.023174	33.755572
863.726754	87264.746014	33.760589
864.176019	87413.270081	33.765607
864.735676	87534.797883	33.770624
865.172987	87695.353644	33.775642
866.064848	87845.623300	33.780660
866.741239	87993.164486	33.785677
867.431648	88156.459313	33.790695
868.816254	88314.819210	33.795712
869.299174	88477.226749	33.800730
870.228109	88633.651935	33.805748
870.891210	88788.230142	33.810765
871.596902	88948.737565	33.815783
872.423149	89123.545495	33.820800
872.797666	89298.581179	33.825818
873.652532	89456.460465	33.830836
874.603621	89631.403431	33.835853
875.385236	89819.739926	33.840871
876.573647	89970.594393	33.845888
877.286147	90135.563582	33.850906
878.257205	90326.726714	33.855924
879.494948	90495.269224	33.860941
880.058825	90674.871637	33.865959
880.921883	90821.526524	33.870976
881.529835	91002.256863	33.875994
882.451889	91166.027949	33.881012
883.523912	91337.502105	33.886029
884.117161	91527.876687	33.891047
885.445370	91689.938988	33.896064
886.048987	91874.707789	33.901082
886.945139	92032.610118	33.906100
887.954174	92194.519719	33.911117
888.770819	92365.290367	33.916135
889.628272	92536.371923	33.921152
890.434758	92697.407074	33.926170
891.538275	92855.046446	33.931188
892.194348	93031.803557	33.936205
892.624877	93207.586623	33.941223
893.715479	93363.199966	33.946240
894.502407	93543.495973	33.951258
895.484355	93710.495958	33.956276
896.264744	93897.991550	33.961293
897.249765	94079.252490	33.966311
897.893673	94237.008456	33.971328
898.970025	94420.199862	33.976346
899.934086	94610.025039	33.981364
901.008845	94783.643627	33.986381
901.768048	94961.967471	33.991399
902.806694	95124.657729	33.996416
903.521230	95331.276747	34.001434
904.247433	95530.313117	34.006452
905.322386	95708.811830	34.011469
906.212414	95883.709325	34.016487
907.742829	96078.769135	34.021504
908.258227	96257.857947	34.026522
909.151503	96447.082526	34.031540
910.093871	96649.541913	34.036557
910.838012	96843.718582	34.041575
911.970780	97010.615065	34.046592
913.041797	97204.936840	34.051610
914.185353	97385.145471	34.056628
915.069454	97551.168866	34.061645
915.973968	97742.813222	34.066663
917.472115	97906.515849	34.071680
918.355762	98081.107228	34.076698
919.558483	98265.116810	34.081716
920.408899	98454.199312	34.086733
921.104811	98616.621167	34.091751
922.063574	98800.130614	34.096768
923.203520	98963.013153	34.101786
924.048141	99139.125002	34.106804
925.205879	99313.356958	34.111821
926.013521	99503.068534	34.116839
926.940370	99672.833951	34.121856
927.626589	99859.763944	34.126874
928.579351	100023.602224	34.131892
929.565148	100189.936658	34.136909
930.324939	100391.159008	34.141927
931.146952	100585.415400	34.146944
931.851531	100757.054398	34.151962
932.899890	100919.781219	34.156980
933.784609	101114.202269	34.161997
934.646732	101316.117830	34.167015
936.491580	101480.394419	34.172032
936.852859	101675.792529	34.177050
937.846550	101860.692409	34.182068
938.905715	102013.839533	34.187085
939.819066	102207.871750	34.192103
941.166367	102403.777428	34.197120
941.819154	102577.235345	34.202138
942.951410	102735.186366	34.207156
943.892081	102928.554806	34.212173
944.787743	103125.407975	34.217191
945.849668	103299.923883	34.222208
947.045266	103458.071524	34.227226
947.976925	103622.841969	34.232244
948.854254	103806.179693	34.237261
949.417708	104001.942144	34.242279
950.192530	104153.648518	34.247296
950.910432	104315.185337	34.252314
951.627397	104509.387752	34.257332
952.723633	104698.001530	34.262349
953.259784	104871.076349	34.267367
954.132682	105026.254068	34.272384
954.998347	105221.076786	34.277402
955.791037	105418.173460	34.282420
957.125179	105607.812005	34.287437
957.549070	105791.593284	34.292455
958.060424	105996.180733	34.297472
959.252080	106209.484224	34.302490
959.821319	106400.077990	34.307508
960.746133	106587.448416	34.312525
961.476072	106829.846693	34.317543
962.108347	107052.000402	34.322560
963.192510	107257.111046	34.327578
964.232324	107455.569076	34.332596
965.079637	107679.098355	34.337613
965.740264	107927.217299	34.342631
967.199118	108154.119789	34.347648
968.388552	108366.263367	34.352666
969.267788	108595.621030	34.357684
970.288270	108805.174353	34.362701
971.023397	109038.194546	34.367719
972.141363	109244.910892	34.372736
973.563918	109461.698281	34.377754
974.577900	109713.195300	34.382772
975.775486	109921.094321	34.387789
976.807853	110140.434130	34.392807
978.129165	110376.573703	34.397824
979.616426	110579.376319	34.402842
980.612719	110802.299324	34.407860
981.906578	110987.632386	34.412877
983.036869	111175.324330	34.417895
983.958057	111374.755847	34.422912
985.013394	111586.465850	34.427930
985.792964	111790.572424	34.432948
987.020623	111982.535217	34.437965
987.795442	112184.884882	34.442983
988.592669	112400.241231	34.448000
989.687076	112610.977449	34.453018
990.588732	112820.201741	34.458036
991.457121	113032.245244	34.463053
992.657519	113242.031480	34.468071
993.314532	113464.437058	34.473088
994.571386	113683.097185	34.478106
995.082860	113885.654968	34.483124
996.415933	114084.366984	34.488141
997.743194	114309.531656	34.493159
998.744252	114530.406953	34.498176
999.953885	114730.942859	34.503194
1000.949905	114931.110112	34.508212
1001.926379	115136.704004	34.513229
1002.937735	115340.900161	34.518247
1004.137367	115538.694576	34.523264
1005.162693	115752.519383	34.528282
1005.764818	115982.542726	34.533300
1006.659815	116176.857462	34.538317
1007.439124	116389.245552	34.543335
1008.848098	116578.106702	34.548352
1009.774947	116809.932904	34.553370
1010.586271	117033.621264	34.558388
1011.878911	117225.863279	34.563405
1013.020318	117427.050677	34.568423
1013.777766	117648.257004	34.573440
1014.843754	117880.398479	34.578458
1015.533926	118080.144716	34.583476
1016.727556	118301.942974	34.588493
1017.642098	118488.390022	34.593511
1018.699324	118688.814802	34.598528
1019.828969	118897.971227	34.603546
1020.365518	119107.252447	34.608564
1021.416681	119305.516024	34.613581
1022.006494	119529.311395	34.618599
1022.860699	119734.946472	34.623616
1023.884928	119949.525532	34.628634
1024.794586	120185.119969	34.633652
1025.889719	120405.291059	34.638669
1026.864332	120635.214756	34.643687
1027.500127	120873.128090	34.648704
1028.729054	121089.050313	34.653722
1029.630278	121320.562778	34.658740
1030.641703	121549.892163	34.663757
1031.355161	121794.389188	34.668775
1032.561423	122048.791841	34.673792
1033.870359	122278.762122	34.678810
1035.152227	122525.718403	34.683828
1036.197820	122736.361165	34.688845
1036.938703	122994.815100	34.693863
1037.866379	123248.450561	34.698880
1039.465831	123487.315986	34.703898
1040.311077	123717.995069	34.708916
1041.594694	123946.043840	34.713933
1042.796209	124201.923296	34.718951
1043.555404	124452.568316	34.723968
1044.830796	124674.528720	34.728986
1045.880046	124900.101754	34.734004
1046.919285	125149.591267	34.739021
1048.062896	125395.010392	34.744039
1049.055779	125629.557845	34.749056
1050.630796	125874.377445	34.754074
1051.694212	126121.437917	34.759092
1052.858586	126334.013013	34.764109
1053.708345	126575.460317	34.769127
1054.801486	126825.132354	34.774144
1055.834067	127059.646436	34.779162
1056.526359	127303.723621	34.784180
1057.810912	127541.963877	34.789197
1058.930160	127774.175286	34.794215
1059.928889	128020.108714	34.799232
1060.954808	128277.040569	34.804250
1061.954095	128514.296301	34.809268
1063.435075	128754.237308	34.814285
1064.854928	128994.633891	34.819303
1065.907117	129224.966316	34.824320
1067.060071	129455.106398	34.829338
1068.079216	129700.099418	34.834356
1069.044490	129925.559107	34.839373
1070.250134	130168.737959	34.844391
1071.745298	130397.903352	34.849408
1073.044284	130624.669260	34.854426
1073.646681	130872.097907	34.859444
1074.487181	131086.572138	34.864461
1075.666439	131339.739798	34.869479
1076.614864	131582.313099	34.874496
1077.603491	131801.102730	34.879514
1078.466436	132055.203013	34.884532
1079.207255	132306.676333	34.889549
1080.448123	132549.614475	34.894567
1081.193871	132801.331778	34.899584
1082.206157	133026.337158	34.904602
1083.489314	133285.815949	34.909620
1084.587711	133536.390773	34.914637
1085.933704	133788.245022	34.919655
1086.849483	134040.869484	34.924672
1088.011477	134276.823972	34.929690
1088.879942	134514.248423	34.934708
1089.916013	134767.682757	34.939725
1091.139389	134997.585745	34.944743
1092.066235	135239.189220	34.949760
1093.124639	135473.014597	34.954778
1093.779292	135710.533915	34.959796
1094.953216	135954.079567	34.964813
1095.829868	136220.380783	34.969831
1096.687795	136476.177893	34.974848
1097.898062	136733.972577	34.979866
1099.130336	136990.992353	34.984884
1100.054842	137257.636469	34.989901
1101.293772	137531.381023	34.994919
1102.401954	137779.299627	34.999936
1103.237116	138010.961545	35.004954
1104.061380	138303.886428	35.009972
1104.607511	138593.183209	35.014989
1106.261234	138856.094030	35.020007
1107.271498	139130.155885	35.025024
1108.631740	139405.024360	35.030042
1109.980522	139683.003216	35.035060
1110.733706	139959.244326	35.040077
1112.197176	140245.348558	35.045095
1112.632975	140525.703909	35.050112
1114.331274	140798.841793	35.055130
1115.090634	141089.101334	35.060148
1116.275914	141396.955007	35.065165
1117.729747	141666.159057	35.070183
1118.625216	141954.869393	35.075200
1120.023553	142236.424078	35.080218
1121.168357	142530.372772	35.085236
1122.126822	142825.115538	35.090253
1123.789969	143094.993731	35.095271
1124.714581	143374.176144	35.100288
1126.007463	143640.544048	35.105306
1127.340413	143917.431806	35.110324
1128.783915	144193.885095	35.115341
1129.787020	144488.761562	35.120359
1130.709988	144797.526042	35.125376
1131.909953	145056.958700	35.130394
1133.006302	145330.168760	35.135412
1133.846177	145632.220999	35.140429
1135.334386	145934.714094	35.145447
1136.124148	146217.923395	35.150464
1137.408935	146490.705611	35.155482
1138.868203	146783.053348	35.160500
1139.756655	147080.215117	35.165517
1141.141017	147363.386178	35.170535
1141.858241	147647.481228	35.175552
1143.317072	147935.831228	35.180570
1144.328234	148234.072983	35.185588
1145.241463	148531.851485	35.190605
1146.856355	148801.477241	35.195623
1147.850093	149094.960681	35.200640
1149.365001	149378.088086	35.205658
1150.769566	149654.057873	35.210676
1152.057411	149951.532612	35.215693
1153.650970	150244.457117	35.220711
1154.595128	150507.104224	35.225728
1156.102970	150755.088039	35.230746
1156.998905	151045.267889	35.235764
1157.989215	151338.047077	35.240781
1159.252083	151608.740994	35.245799
1159.991688	151874.247212	35.250816
1160.917612	152153.041650	35.255834
1162.110836	152459.113299	35.260852
1163.659411	152738.874730	35.265869
1164.778857	152999.468653	35.270887
1165.667210	153262.005034	35.275904
1166.528395	153554.404457	35.280922
1167.927194	153827.184826	35.285940
1168.419417	154102.526696	35.290957
1169.870640	154359.599985	35.295975
1170.879878	154657.944849	35.300992
1172.178904	154945.513669	35.306010
1173.343252	155220.727345	35.311028
1174.174040	155496.771792	35.316045
1175.614421	155778.387419	35.321063
1176.175680	156084.592761	35.326080
1177.288811	156370.477915	35.331098
1178.702339	156663.228619	35.336116
1179.838523	156970.132521	35.341133
1181.260369	157274.708462	35.346151
1182.237069	157586.628619	35.351168
1183.317946	157881.270010	35.356186
1184.501120	158165.977121	35.361204
1185.590624	158480.067582	35.366221
1186.684992	158784.316089	35.371239
1188.033905	159116.952513	35.376256
1188.861391	159412.027737	35.381274
1189.868703	159731.329997	35.386292
1190.987058	160067.805378	35.391309
1191.953467	160384.925017	35.396327
1193.181227	160730.724533	35.401344
1194.441916	161061.869428	35.406362
1195.764517	161373.280171	35.411380
1196.995619	161701.073407	35.416397
1198.308408	162044.079185	35.421415
1199.469642	162379.323499	35.426432
1200.346810	162698.810244	35.431450
1202.109605	163021.248787	35.436468
1203.155724	163368.407386	35.441485
1204.542607	163729.785157	35.446503
1205.901340	164054.886538	35.451520
1207.150795	164356.702720	35.456538
1208.469918	164700.617610	35.461556
1209.363492	165056.886649	35.466573
1210.561579	165364.529247	35.471591
1212.349531	165719.983848	35.476608
1213.588952	166033.486013	35.481626
1215.192242	166343.733190	35.486644
1216.370909	166697.571042	35.491661
1217.772370	167018.298301	35.496679
1218.915268	167333.285018	35.501696
1220.187370	167665.571624	35.506714
1221.488571	167980.828758	35.511732
1222.455138	168298.947472	35.516749
1223.729428	168636.557441	35.521767
1224.653815	168975.039818	35.526784
1225.619676	169312.883545	35.531802
1227.125066	169644.892956	35.536820
1228.142511	169985.258316	35.541837
1229.621282	170304.677369	35.546855
1230.630013	170647.041351	35.551872
1231.985805	170981.661255	35.556890
1233.307611	171333.609619	35.561908
1234.315329	171672.098790	35.566925
1236.024736	171983.484981	35.571943
1237.096348	172336.827502	35.576960
1238.403441	172686.669724	35.581978
1239.638882	172996.466094	35.586996
1240.923898	173329.960283	35.592013
1242.303928	173664.291406	35.597031
1243.452153	174009.259065	35.602048
1244.454125	174333.784879	35.607066
1245.869563	174664.043961	35.612084
1246.926513	175003.133280	35.617101
1248.327179	175326.039319	35.622119
1249.628822	175651.324274	35.627136
1250.337971	175974.716902	35.632154
1251.773442	176299.920773	35.637172
1252.635820	176634.358509	35.642189
1254.238237	176941.899611	35.647207
1255.039725	177279.689487	35.652224
1256.199995	177633.793408	35.657242
1257.610281	177966.512883	35.662260
1258.800174	178306.187496	35.667277
1259.925445	178662.563654	35.672295
1260.993483	179012.885563	35.677312
1262.051111	179354.835580	35.682330
1263.474166	179684.036500	35.687348
1264.878763	180038.980479	35.692365
1266.453379	180392.236363	35.697383
1267.973820	180746.772825	35.702400
1269.072598	181111.788423	35.707418
1270.269645	181436.050411	35.712436
1271.067674	181795.942414	35.717453
1272.696695	182163.847924	35.722471
1274.160082	182531.009215	35.727488
1275.382562	182882.309874	35.732506
1276.710736	183239.332281	35.737524
1277.844786	183588.190074	35.742541
1278.989852	183954.969786	35.747559
1280.212060	184328.669335	35.752576
1281.409102	184686.332510	35.757594
1283.048273	185064.017327	35.762612
1284.137102	185464.058436	35.767629
1285.681800	185825.022743	35.772647
1286.802666	186189.803793	35.777664
1287.716534	186554.583397	35.782682
1289.112814	186937.779424	35.787700
1290.474448	187341.381540	35.792717
1291.605069	187705.498432	35.797735
1292.754570	188079.883407	35.802752
1293.666443	188478.262347	35.807770
1295.037465	188870.285144	35.812788
1296.264854	189269.772764	35.817805
1297.852391	189668.492946	35.822823
1299.327717	190057.739624	35.827840
1300.559272	190443.271862	35.832858
1301.819915	190825.856940	35.837876
1303.477450	191225.325408	35.842893
1304.961091	191638.522147	35.847911
1306.655220	192013.757208	35.852928
1307.851835	192388.746744	35.857946
1309.635996	192770.864723	35.862964
1311.019518	193162.673586	35.867981
1312.659680	193542.230672	35.872999
1313.967287	193928.750852	35.878016
1315.383860	194300.022070	35.883034
1316.774353	194659.684290	35.888052
1317.826813	195049.122740	35.893069
1319.391340	195423.524701	35.898087
1320.682983	195787.043705	35.903104
1322.129088	196164.668824	35.908122
1323.365516	196532.073273	35.913140
1324.182210	196907.839051	35.918157
1325.700964	197277.994202	35.923175
1327.303988	197664.793773	35.928192
1328.256245	198041.737275	35.933210
1329.783355	198415.363497	35.938228
1331.059369	198781.923872	35.943245
1332.359936	199150.170778	35.948263
1333.522266	199514.278425	35.953280
1334.513339	199897.371012	35.958298
1335.998476	200266.926789	35.963316
1337.286760	200634.587353	35.968333
1338.456881	200991.617593	35.973351
1339.778997	201354.071218	35.978368
1341.095124	201736.942994	35.983386
1342.358975	202111.585789	35.988404
1343.628572	202473.927104	35.993421
1344.597865	202851.758514	35.998439
1346.006537	203235.512132	36.003456
1347.388828	203617.659782	36.008474
1348.772502	204002.551720	36.013492
1350.319240	204382.784621	36.018509
1351.245122	204765.915271	36.023527
1353.015234	205170.365990	36.028544
1354.075299	205572.612665	36.033562
1355.672699	205947.982660	36.038580
1357.133530	206342.765227	36.043597
1358.215468	206742.284914	36.048615
1359.753763	207143.432842	36.053632
1360.558929	207535.689003	36.058650
1361.857507	207943.711802	36.063668
1363.502134	208359.958266	36.068685
1364.500565	208755.007630	36.073703
1366.216881	209188.146831	36.078720
1367.225743	209599.476786	36.083738
1369.082946	210000.333162	36.088756
1370.371571	210402.847213	36.093773
1371.640157	210823.613066	36.098791
1372.901193	211256.242003	36.103808
1374.129038	211677.488868	36.108826
1375.661556	212088.884933	36.113844
1376.910810	212502.958268	36.118861
1378.303223	212941.529753	36.123879
1379.785646	213375.885652	36.128896
1381.003102	213793.297516	36.133914
1382.468595	214236.244520	36.138932
1383.972115	214675.581251	36.143949
1385.089357	215100.380972	36.148967
1386.475464	215536.033543	36.153984
1387.882327	215983.240369	36.159002
1389.354958	216420.635392	36.164020
1390.866468	216857.391204	36.169037
1392.273942	217274.102561	36.174055
1393.942038	217765.440713	36.179072
1395.282121	218235.146235	36.184090
1396.658984	218679.755308	36.189108
1398.338420	219095.033083	36.194125
1399.870936	219524.788220	36.199143
1401.069445	219967.756477	36.204160
1402.094203	220419.644708	36.209178
1403.682403	220864.965520	36.214196
1405.406042	221294.392106	36.219213
1407.083307	221739.321140	36.224231
1408.592005	222150.449264	36.229248
1409.860208	222598.827532	36.234266
1411.182577	223027.464071	36.239284
1412.530880	223470.981728	36.244301
1413.600966	223915.969482	36.249319
1415.441967	224341.528672	36.254336
1416.585549	224793.391017	36.259354
1418.223765	225253.758498	36.264372
1419.558554	225681.108146	36.269389
1421.044659	226118.136988	36.274407
1423.172761	226543.352422	36.279424
1424.161771	226988.188032	36.284442
1425.648653	227432.638378	36.289460
1427.383892	227847.865139	36.294477
1428.736673	228251.396348	36.299495
1430.047777	228678.202065	36.304512
1431.385082	229099.239146	36.309530
1432.903678	229504.525103	36.314548
1434.491614	229920.291175	36.319565
1435.580009	230339.646265	36.324583
1437.222915	230746.185659	36.329600
1438.835211	231159.437064	36.334618
1439.956085	231565.480919	36.339636
1441.596698	231982.489461	36.344653
1443.025411	232422.445593	36.349671
1444.588811	232840.536304	36.354688
1445.789795	233255.030355	36.359706
1447.016059	233676.684474	36.364724
1448.350633	234111.657425	36.369741
1449.690601	234557.324588	36.374759
1451.340038	234974.010206	36.379776
1452.969982	235413.027777	36.384794
1454.060579	235860.924415	36.389812
1455.363463	236285.037111	36.394829
1456.491292	236746.799207	36.399847
1457.939293	237213.767875	36.404864
1458.740752	237667.991399	36.409882
1460.098498	238128.931965	36.414900
1461.866423	238584.827363	36.419917
1462.850762	239068.185469	36.424935
1464.315458	239551.287800	36.429952
1465.461976	240029.312745	36.434970
1467.024003	240527.109221	36.439988
1468.610887	241011.947896	36.445005
1469.964460	241492.761949	36.450023
1471.469294	241967.303287	36.455040
1473.067004	242480.797272	36.460058
1474.866797	242981.761283	36.465076
1476.535291	243455.593114	36.470093
1477.766294	243967.398393	36.475111
1479.514843	244441.650933	36.480128
1480.823127	244957.306813	36.485146
1482.154707	245442.349976	36.490164
1483.881548	245938.734593	36.495181
1485.364005	246436.303615	36.500199
1486.923388	246935.994700	36.505216
1488.334301	247439.928040	36.510234
1489.489082	247960.695731	36.515252
1491.314924	248454.706131	36.520269
1492.662426	248955.273978	36.525287
1494.252218	249461.848510	36.530304
1495.972818	249991.696668	36.535322
1497.378840	250485.677845	36.540340
1498.969654	250986.132364	36.545357
1500.957192	251477.580242	36.550375
1502.917838	251972.716610	36.555392
1504.227212	252492.297145	36.560410
1506.043671	252976.281147	36.565428
1508.008232	253455.109799	36.570445
1509.414091	253939.975445	36.575463
1511.355944	254435.879678	36.580480
1512.526564	254916.593516	36.585498
1514.123491	255392.842656	36.590516
1515.388659	255905.016213	36.595533
1516.884568	256386.719029	36.600551
1518.453993	256865.082205	36.605568
1519.899527	257366.202010	36.610586
1521.243955	257858.320620	36.615604
1522.616280	258341.162673	36.620621
1524.036503	258836.444632	36.625639
1525.231883	259324.904989	36.630656
1526.934921	259827.151928	36.635674
1528.235198	260335.511438	36.640692
1529.821860	260789.384510	36.645709
1531.194926	261281.423247	36.650727
1532.655636	261778.756851	36.655744
1534.274812	262250.635603	36.660762
1535.716514	262724.194835	36.665780
1537.645576	263214.998658	36.670797
1539.223647	263725.370052	36.675815
1540.731445	264185.759247	36.680832
1542.304474	264669.330759	36.685850
1543.590168	265180.054818	36.690868
1545.229483	265654.241232	36.695885
1546.925097	266156.387132	36.700903
1548.710291	266647.569192	36.705920
1549.978629	267145.771335	36.710938
1550.967776	267655.298249	36.715956
1552.667151	268143.419739	36.720973
1554.417529	268658.967869	36.725991
1555.418528	269176.010978	36.731008
1557.048760	269677.987349	36.736026
1558.400172	270215.167130	36.741044
1560.144647	270726.954611	36.746061
1561.168216	271260.427654	36.751079
1562.686241	271793.996281	36.756096
1564.303329	272316.878627	36.761114
1565.596405	272867.655354	36.766132
1567.279779	273420.780144	36.771149
1568.915383	273966.011665	36.776167
1570.319511	274494.184408	36.781184
1571.913114	275060.607005	36.786202
1573.167295	275620.937113	36.791220
1574.768066	276178.287674	36.796237
1576.690845	276724.914916	36.801255
1578.319443	277285.256198	36.806272
1580.027305	277843.373201	36.811290
1581.718345	278410.966883	36.816308
1583.298926	278964.047314	36.821325
1584.937134	279533.450665	36.826343
1586.820947	280089.882335	36.831360
1588.417720	280640.288856	36.836378
1589.567225	281203.214839	36.841396
1591.681362	281774.439060	36.846413
1593.373140	282339.228466	36.851431
1594.913144	282888.698548	36.856448
1596.788466	283457.137751	36.861466
1598.080597	284028.135445	36.866484
1599.770877	284589.717854	36.871501
1601.370150	285150.856298	36.876519
1603.088140	285725.309175	36.881536
1604.597996	286282.673884	36.886554
1605.856424	286843.507409	36.891572
1608.085959	287401.384647	36.896589
1609.780197	287987.289579	36.901607
1611.597132	288537.331122	36.906624
1613.393742	289094.232319	36.911642
1614.880939	289670.436394	36.916660
1616.577528	290226.613226	36.921677
1618.202591	290786.482818	36.926695
1619.613036	291348.366852	36.931712
1621.655346	291909.941155	36.936730
1623.253988	292465.591847	36.941748
1624.765277	293009.341901	36.946765
1626.371315	293588.608940	36.951783
1627.827469	294161.344886	36.956800
1630.107747	294695.258129	36.961818
1631.555720	295258.871833	36.966836
1633.477864	295815.140387	36.971853
1635.325423	296339.440558	36.976871
1636.331683	296897.556959	36.981888
1637.980892	297416.576560	36.986906
1639.367677	297953.670598	36.991924
1641.189092	298498.462521	36.996941
1642.759926	299029.323666	37.001959
1644.164798	299567.524513	37.006976
1645.993774	300096.178977	37.011994
1647.260918	300657.002009	37.017012
1648.928773	301203.558182	37.022029
1650.552455	301745.775646	37.027047
1651.901851	302299.464703	37.032064
1653.581488	302863.915833	37.037082
1654.970882	303427.954490	37.042100
1656.780375	303973.151625	37.047117
1658.626694	304568.703178	37.052135
1660.287271	305131.569695	37.057152
1661.822485	305692.548741	37.062170
1663.605546	306259.248686	37.067188
1665.213681	306816.424716	37.072205
1666.790587	307404.129533	37.077223
1668.835024	307990.940673	37.082240
1670.624324	308545.587205	37.087258
1672.318441	309130.239052	37.092276
1673.974300	309715.223409	37.097293
1675.952827	310268.202315	37.102311
1677.014559	310859.143297	37.107328
1679.047035	311453.221378	37.112346
1680.707621	312041.287008	37.117364
1682.313801	312609.091907	37.122381
1683.755535	313201.477028	37.127399
1685.444341	313795.823179	37.132416
1687.197130	314387.640206	37.137434
1688.764982	314997.792713	37.142452
1690.229584	315579.718897	37.147469
1692.154637	316173.296766	37.152487
1693.826711	316779.608664	37.157504
1695.755000	317385.009964	37.162522
1697.247355	317993.855543	37.167540
1699.041114	318613.413070	37.172557
1700.659529	319219.231137	37.177575
1702.200082	319821.730429	37.182592
1704.016536	320444.950252	37.187610
1705.667000	321057.577853	37.192628
1707.111738	321660.229427	37.197645
1709.178880	322290.754966	37.202663
1710.829746	322919.769011	37.207680
1712.915482	323523.009201	37.212698
1714.466698	324134.228765	37.217716
1716.110462	324774.830178	37.222733
1718.007615	325415.891283	37.227751
1719.524098	326023.087057	37.232768
1721.140908	326631.428441	37.237786
1722.911783	327276.681038	37.242804
1724.763221	327913.966681	37.247821
1726.437629	328533.553087	37.252839
1728.287141	329143.100972	37.257856
1730.406779	329760.087928	37.262874
1731.990093	330400.108444	37.267892
1733.797838	331043.436337	37.272909
1735.674617	331642.697335	37.277927
1737.314193	332255.929300	37.282944
1739.222357	332892.035521	37.287962
1740.814216	333539.179611	37.292980
1742.701301	334149.989515	37.297997
1744.554399	334788.140006	37.303015
1745.940663	335424.202384	37.308032
1748.183654	336019.625114	37.313050
1750.328899	336615.616019	37.318068
1752.151600	337221.147871	37.323085
1754.167986	337806.180374	37.328103
1755.889546	338383.766535	37.333120
1757.844351	338977.528881	37.338138
1759.062083	339560.770028	37.343156
1761.161198	340118.728861	37.348173
1763.315797	340699.340495	37.353191
1765.033835	341294.664039	37.358208
1767.059802	341862.896539	37.363226
1768.795931	342420.458832	37.368244
1770.532036	343000.554981	37.373261
1771.785588	343598.085718	37.378279
1773.480589	344183.200704	37.383296
1775.446216	344771.157685	37.388314
1777.230081	345371.143147	37.393332
1778.811785	345948.945916	37.398349
1780.573784	346530.366935	37.403367
1782.251616	347153.368452	37.408384
1783.858668	347758.378838	37.413402
1785.803525	348337.818817	37.418420
1786.892643	348943.102544	37.423437
1788.860173	349555.441306	37.428455
1790.410461	350188.778579	37.433472
1792.220660	350792.472688	37.438490
1794.240713	351430.740372	37.443508
1796.032106	352051.424471	37.448525
1797.588761	352687.289256	37.453543
1799.620500	353332.684674	37.458560
1801.053419	353969.947400	37.463578
1802.565284	354599.879475	37.468596
1804.253950	355229.773365	37.473613
1806.235428	355871.967912	37.478631
1807.609040	356537.649410	37.483648
1809.794958	357210.012520	37.488666
1811.366421	357865.643011	37.493684
1813.238100	358516.392746	37.498701
1815.241781	359183.958932	37.503719
1816.595452	359863.344250	37.508736
1818.620706	360522.639096	37.513754
1820.861728	361182.826619	37.518772
1822.053631	361855.101538	37.523789
1824.067439	362538.038194	37.528807
1826.036945	363245.428652	37.533824
1827.450736	363903.171287	37.538842
1829.825308	364565.057601	37.543860
1831.589483	365272.648998	37.548877
1833.858615	365951.552820	37.553895
1835.394208	366616.841129	37.558912
1837.546664	367289.221041	37.563930
1839.634471	367975.628606	37.568948
1841.389512	368670.932178	37.573965
1843.610260	369325.710609	37.578983
1845.010203	370014.554136	37.584000
1846.873226	370676.445556	37.589018
1848.904700	371384.083210	37.594036
1850.527881	372069.909642	37.599053
1852.703832	372741.478448	37.604071
1854.025874	373447.494171	37.609088
1855.521946	374120.950720	37.614106
1857.511527	374798.422283	37.619124
1859.118859	375499.582661	37.624141
1861.024883	376209.278005	37.629159
1862.920781	376926.544166	37.634176
1864.565606	377627.605753	37.639194
1866.534269	378318.100437	37.644212
1868.141875	379031.972839	37.649229
1870.135578	379755.479819	37.654247
1871.540015	380464.334925	37.659264
1873.023907	381137.456715	37.664282
1874.837996	381836.680824	37.669300
1876.661288	382544.206446	37.674317
1878.529990	383249.326136	37.679335
1880.552140	383945.150396	37.684352
1882.124092	384658.073924	37.689370
1883.890281	385364.053282	37.694388
1885.520927	386087.458998	37.699405
1887.637640	386794.440092	37.704423
1889.376059	387540.184139	37.709440
1891.009466	388269.803428	37.714458
1892.957617	388989.441224	37.719476
1894.572328	389747.628258	37.724493
1896.472710	390487.217896	37.729511
1898.282315	391230.100884	37.734528
1900.371477	391968.788056	37.739546
1902.591766	392722.671545	37.744564
1904.014468	393491.421686	37.749581
1906.020272	394255.189561	37.754599
1908.261507	395024.856441	37.759616
1910.232780	395792.926214	37.764634
1911.855738	396539.920046	37.769652
1913.566227	397322.213664	37.774669
1915.641260	398091.703285	37.779687
1917.817578	398878.416268	37.784704
1919.631689	399654.118042	37.789722
1922.240190	400413.879336	37.794740
1923.999244	401198.850578	37.799757
1925.866527	401994.350572	37.804775
1927.785389	402768.710735	37.809792
1930.069338	403547.804666	37.814810
1932.110361	404317.617656	37.819828
1933.614874	405117.601692	37.824845
1935.954984	405907.720606	37.829863
1937.979354	406685.504491	37.834880
1939.680610	407457.872576	37.839898
1941.880913	408248.176687	37.844916
1943.686131	409059.577615	37.849933
1945.818021	409858.663927	37.854951
1948.015774	410630.506911	37.859968
1949.851819	411415.586618	37.864986
1952.072560	412203.189486	37.870004
1953.828105	413003.410920	37.875021
1956.391390	413792.532099	37.880039
1958.369121	414585.424847	37.885056
1960.013996	415354.690630	37.890074
1962.345072	416141.450043	37.895092
1964.409716	416943.857562	37.900109
1966.521033	417717.055255	37.905127
1968.322183	418512.264967	37.910144
1970.359365	419293.051404	37.915162
1972.548270	420051.680066	37.920180
1974.479734	420860.648890	37.925197
1976.085265	421654.071666	37.930215
1978.177679	422459.291200	37.935232
1980.263728	423223.438728	37.940250
1982.375882	423998.497625	37.945268
1983.895215	424812.117762	37.950285
1986.069804	425612.411601	37.955303
1988.272237	426392.596984	37.960320
1990.047368	427169.030413	37.965338
1992.256231	427964.507742	37.970356
1993.849736	428775.453148	37.975373
1995.961244	429566.337238	37.980391
1997.776206	430353.143349	37.985408
1999.909670	431150.351257	37.990426
2001.976540	431957.567669	37.995444
2003.863523	432766.355783	38.000461
2005.663298	433515.901644	38.005479
2007.801382	434279.946935	38.010496
2009.645690	435065.529297	38.015514
2011.606136	435847.219157	38.020532
2013.402708	436628.099951	38.025549
2015.281862	437416.887350	38.030567
2017.341403	438205.972338	38.035584
2019.008999	438985.883617	38.040602
2021.416739	439792.823561	38.045620
2022.782786	440582.042179	38.050637
2024.795386	441372.746086	38.055655
2026.631989	442188.449772	38.060672
2028.579163	443013.315221	38.065690
2030.249514	443836.829683	38.070708
2032.028053	444672.186488	38.075725
2034.001117	445500.851558	38.080743
2035.736432	446354.872630	38.085760
2037.428738	447206.692082	38.090778
2039.657961	448063.195888	38.095796
2041.269011	448927.760911	38.100813
2043.761126	449800.391715	38.105831
2045.749615	450668.972863	38.110848
2047.587530	451558.130730	38.115866
2049.552651	452437.367386	38.120884
2051.637201	453319.683793	38.125901
2053.668527	454188.771754	38.130919
2055.912503	455092.229681	38.135936
2057.867713	456011.879223	38.140954
2060.156660	456895.781557	38.145972
2062.809086	457770.838091	38.150989
2065.359022	458666.859040	38.156007
2067.947155	459584.981238	38.161024
2069.695088	460485.858414	38.166042
2071.777289	461351.300119	38.171060
2074.059354	462250.190834	38.176077
2076.155733	463138.657950	38.181095
2078.701139	464027.365566	38.186112
2080.967023	464896.820318	38.191130
2083.472051	465785.759528	38.196148
2085.691669	466663.383786	38.201165
2087.585056	467528.083786	38.206183
2089.883218	468412.490945	38.211200
2092.095591	469311.124085	38.216218
2094.375584	470175.491640	38.221236
2095.926521	471056.970797	38.226253
2098.399651	471930.223107	38.231271
2100.693141	472796.846022	38.236288
2102.091115	473682.272347	38.241306
2104.386819	474586.658309	38.246324
2106.159261	475475.981326	38.251341
2107.961764	476365.409084	38.256359
2110.696483	477243.577750	38.261376
2112.260711	478141.043456	38.266394
2114.777213	479021.589285	38.271412
2116.992002	479917.043626	38.276429
2118.806230	480816.662303	38.281447
2120.968201	481740.674724	38.286464
2123.111177	482634.190613	38.291482
2125.238693	483506.707727	38.296500
2126.938985	484435.457472	38.301517
2129.172929	485359.729014	38.306535
2131.363663	486244.576091	38.311552
2133.659381	487166.371503	38.316570
2135.968405	488065.246383	38.321588
2138.086481	488975.113102	38.326605
2140.358327	489872.640583	38.331623
2142.710960	490786.868425	38.336640
2144.507636	491678.274285	38.341658
2147.022544	492546.197079	38.346676
2149.403965	493437.114016	38.351693
2151.390529	494307.357896	38.356711
2153.570336	495165.060821	38.361728
2155.702780	496024.898891	38.366746
2157.194306	496908.113070	38.371764
2158.964358	497776.501633	38.376781
2161.207190	498649.965077	38.381799
2163.850983	499551.672734	38.386816
2165.767359	500457.337051	38.391834
2167.754815	501336.354513	38.396852
2169.453731	502230.406488	38.401869
2171.029568	503153.990786	38.406887
2173.601241	504067.019388	38.411904
2175.563250	505004.106644	38.416922
2177.385752	505938.440314	38.421940
2179.424781	506846.561498	38.426957
2181.867351	507774.888838	38.431975
2184.077804	508734.264284	38.436992
2185.796001	509690.840645	38.442010
2188.009449	510628.673811	38.447028
2190.170922	511574.326183	38.452045
2191.913143	512563.550062	38.457063
2194.511738	513532.760055	38.462080
2196.417730	514509.082501	38.467098
2198.514207	515502.249626	38.472116
2200.823101	516490.430423	38.477133
2202.800429	517493.169135	38.482151
2205.612311	518469.802945	38.487168
2207.587963	519473.675049	38.492186
2209.606391	520462.711418	38.497204
2212.046400	521473.835322	38.502221
2214.227531	522479.746335	38.507239
2216.692980	523471.539297	38.512256
2218.717380	524489.183608	38.517274
2221.385963	525514.663072	38.522292
2223.428075	526530.808006	38.527309
2225.719319	527547.951711	38.532327
2228.071718	528547.641735	38.537344
2230.385787	529577.285459	38.542362
2232.680159	530585.863355	38.547380
2235.356057	531604.783305	38.552397
2237.491444	532625.182536	38.557415
2239.632847	533639.519293	38.562432
2242.134921	534665.758366	38.567450
2244.429320	535693.319015	38.572468
2246.674434	536705.614507	38.577485
2248.738380	537732.616462	38.582503
2250.981933	538755.892494	38.587520
2253.023704	539786.476586	38.592538
2255.136032	540815.666907	38.597556
2257.651238	541850.000143	38.602573
2259.592134	542902.465786	38.607591
2262.249790	543929.278913	38.612608
2264.665453	544976.079122	38.617626
2266.691512	546009.686847	38.622644
2269.074068	547037.375521	38.627661
2271.492628	548063.926665	38.632679
2273.790881	549112.499738	38.637696
2275.926603	550153.477474	38.642714
2278.079204	551199.251635	38.647732
2280.574244	552253.990604	38.652749
2282.622605	553286.098325	38.657767
2285.194392	554332.118002	38.662784
2287.377338	555375.105500	38.667802
2289.491145	556422.045459	38.672820
2292.194583	557468.304641	38.677837
2294.175752	558501.836687	38.682855
2296.484769	559501.264623	38.687872
2299.390745	560525.493088	38.692890
2301.287650	561543.176986	38.697908
2303.792460	562548.072301	38.702925
2306.150281	563550.152581	38.707943
2308.220494	564537.988188	38.712960
2310.845553	565567.449069	38.717978
2313.086842	566576.149248	38.722996
2315.473047	567574.150876	38.728013
2317.326986	568599.883960	38.733031
2319.885132	569605.736045	38.738048
2322.047046	570627.290880	38.743066
2323.773163	571666.910660	38.748084
2326.191175	572705.830170	38.753101
2328.167629	573760.700937	38.758119
2330.381048	574828.244658	38.763136
2332.874838	575861.222627	38.768154
2335.349889	576919.763966	38.773172
2337.837562	577985.942218	38.778189
2339.500130	579064.760350	38.783207
2341.968339	580125.641931	38.788224
2344.584203	581200.756991	38.793242
2346.122697	582291.306739	38.798260
2349.003562	583395.132294	38.803277
2350.918757	584480.711901	38.808295
2353.187913	585575.114218	38.813312
2355.429656	586684.115989	38.818330
2357.629196	587801.497826	38.823348
2359.959700	588914.995216	38.828365
2362.243771	590041.181576	38.833383
2364.910322	591164.743641	38.838400
2367.046762	592319.313904	38.843418
2368.984145	593473.104161	38.848436
2371.295877	594604.170582	38.853453
2373.601835	595747.457001	38.858471
2376.027208	596914.412412	38.863488
2378.676615	598072.047688	38.868506
2381.113502	599233.210840	38.873524
2383.722799	600402.545214	38.878541
2386.346382	601565.449738	38.883559
2388.573804	602727.351918	38.888576
2391.423613	603897.146932	38.893594
2393.910724	605082.604629	38.898612
2396.334739	606222.443611	38.903629
2398.139787	607391.855572	38.908647
2401.137370	608566.457115	38.913664
2403.677253	609746.868516	38.918682
2405.633466	610933.908972	38.923700
2408.565687	612099.848552	38.928717
2410.654610	613265.856518	38.933735
2413.006468	614446.257786	38.938752
2415.499180	615641.767760	38.943770
2417.629135	616822.504646	38.948788
2420.136760	618012.405727	38.953805
2422.638418	619195.579168	38.958823
2424.701899	620392.147829	38.963840
2427.454120	621596.621719	38.968858
2429.605756	622800.212286	38.973876
2432.451383	623978.713970	38.978893
2434.463145	625183.713601	38.983911
2437.046443	626394.331721	38.988928
2439.642592	627612.756608	38.993946
2441.789355	628816.179217	38.998964
2444.460228	629993.403489	39.003981
2446.837112	631218.398369	39.008999
2448.992496	632435.197821	39.014016
2451.718189	633644.522580	39.019034
2454.120992	634829.195295	39.024052
2456.932569	636006.328055	39.029069
2459.519711	637190.554441	39.034087
2461.906661	638353.215913	39.039104
2464.901137	639490.941905	39.044122
2467.156866	640662.101319	39.049140
2470.024874	641811.021784	39.054157
2472.273378	642956.224310	39.059175
2474.827003	644138.515411	39.064192
2477.135031	645315.073951	39.069210
2479.700310	646474.696095	39.074228
2482.249870	647627.306595	39.079245
2484.523680	648822.765539	39.084263
2487.048007	649974.764119	39.089280
2489.493415	651147.682305	39.094298
2491.880268	652362.943416	39.099316
2494.430231	653549.520861	39.104333
2497.120646	654723.624709	39.109351
2499.544218	655902.118685	39.114368
2502.040217	657096.902558	39.119386
2504.201731	658304.001781	39.124404
2506.811571	659511.825648	39.129421
2509.065560	660737.290335	39.134439
2511.317827	661932.572963	39.139456
2513.948934	663157.323369	39.144474
2516.097791	664416.351759	39.149492
2518.504770	665635.847684	39.154509
2521.272794	666881.211629	39.159527
2524.131719	668128.838038	39.164544
2527.053985	669366.737619	39.169562
2529.332764	670593.338441	39.174580
2532.208396	671821.623165	39.179597
2534.447308	673073.332021	39.184615
2537.252945	674335.972309	39.189632
2539.748949	675585.963096	39.194650
2542.167314	676840.325171	39.199668
2544.397847	678106.183611	39.204685
2547.171457	679367.854022	39.209703
2549.407392	680635.406214	39.214720
2551.773664	681905.546646	39.219738
2554.362154	683169.115938	39.224756
2557.376824	684439.695148	39.229773
2559.772860	685725.897543	39.234791
2562.489995	687020.756687	39.239808
2565.275861	688284.134918	39.244826
2567.816102	689583.873099	39.249844
2570.400395	690855.665546	39.254861
2572.575948	692160.058335	39.259879
2575.077964	693456.267269	39.264896
2577.769581	694745.012515	39.269914
2580.223528	696039.565285	39.274932
2582.867619	697354.834132	39.279949
2585.284549	698673.417856	39.284967
2587.574028	699989.197659	39.289984
2590.865185	701302.880582	39.295002
2593.457000	702615.292571	39.300020
2596.035413	703909.713528	39.305037
2598.931508	705218.264380	39.310055
2601.383883	706528.079332	39.315072
2604.105528	707815.552580	39.320090
2606.445729	709143.225347	39.325108
2609.230812	710478.793717	39.330125
2611.755979	711792.405072	39.335143
2614.205845	713099.340204	39.340160
2617.274262	714409.488717	39.345178
2619.333223	715728.710810	39.350196
2622.451034	717037.950718	39.355213
2624.826811	718376.012114	39.360231
2627.563615	719681.737323	39.365248
2630.170061	720968.282908	39.370266
2632.571497	722254.120452	39.375284
2634.862634	723525.682234	39.380301
2637.437509	724829.542015	39.385319
2639.952697	726144.529237	39.390336
2642.525630	727416.189763	39.395354
2644.538235	728716.167649	39.400372
2647.278685	730005.935839	39.405389
2650.214293	731331.342186	39.410407
2652.849520	732654.507865	39.415424
2655.275472	733985.001131	39.420442
2657.723968	735308.160575	39.425460
2660.366729	736647.416289	39.430477
2663.203862	737974.420094	39.435495
2665.467947	739320.550980	39.440512
2668.514057	740654.777605	39.445530
2670.772832	742024.687536	39.450548
2673.351450	743379.112722	39.455565
2676.491500	744727.738478	39.460583
2679.340703	746084.566783	39.465600
2682.227104	747455.653389	39.470618
2684.997380	748848.164411	39.475636
2687.312122	750213.242455	39.480653
2690.143234	751587.854064	39.485671
2691.985805	752976.035770	39.490688
2695.157738	754363.700674	39.495706
2697.704937	755777.475164	39.500724
2700.111580	757193.081958	39.505741
2702.689879	758598.501864	39.510759
2704.994587	760015.377057	39.515776
2707.997117	761439.799175	39.520794
2710.575178	762861.760543	39.525812
2712.805938	764312.641907	39.530829
2716.138052	765757.307233	39.535847
2718.717237	767199.753594	39.540864
2721.717827	768646.328348	39.545882
2724.434916	770092.915877	39.550900
2727.081222	771554.276627	39.555917
2729.923415	773032.519452	39.560935
2732.452547	774504.130839	39.565952
2735.261178	775971.177729	39.570970
2737.977791	777430.039131	39.575988
2740.550359	778894.674377	39.581005
2743.391758	780386.663488	39.586023
2745.862158	781860.196219	39.591040
2749.030897	783337.241076	39.596058
2752.144706	784833.915287	39.601076
2754.524000	786332.607523	39.606093
2757.269956	787807.923257	39.611111
2759.734566	789309.707253	39.616128
2762.661939	790814.923272	39.621146
2765.270723	792334.431488	39.626164
2767.883681	793827.443898	39.631181
2770.727021	795335.438865	39.636199
2773.456698	796852.926933	39.641216
2776.282566	798367.671423	39.646234
2778.865511	799883.058415	39.651252
2781.781808	801401.634894	39.656269
2784.893415	802921.560475	39.661287
2787.507979	804444.513006	39.666304
2790.187580	805972.353587	39.671322
2792.893498	807514.279331	39.676340
2795.242846	809034.010239	39.681357
2798.495884	810551.445586	39.686375
2801.299821	812110.163149	39.691392
2804.958259	813635.592760	39.696410
2807.668219	815140.168933	39.701428
2810.647472	816660.581729	39.706445
2813.548745	818144.819649	39.711463
2816.396385	819606.767374	39.716480
2819.327413	821079.413194	39.721498
2821.985076	822566.760645	39.726516
2824.925573	824020.257927	39.731533
2828.030521	825485.604028	39.736551
2830.499647	826964.287382	39.741568
2833.469465	828409.400287	39.746586
2836.401076	829892.077910	39.751604
2839.044291	831379.243002	39.756621
2842.095424	832852.894504	39.761639
2844.994272	834348.888928	39.766656
2847.579453	835831.001454	39.771674
2850.415292	837300.170050	39.776692
2852.902702	838795.932411	39.781709
2855.737829	840294.793035	39.786727
2858.528511	841828.489163	39.791744
2861.134954	843330.178399	39.796762
2863.760051	844835.351943	39.801780
2866.402863	846382.758479	39.806797
2869.009213	847914.917131	39.811815
2871.600809	849461.576624	39.816832
2874.596773	851032.373193	39.821850
2877.654095	852597.324921	39.826868
2880.260527	854150.400398	39.831885
2882.930440	855719.390196	39.836903
2885.727955	857302.425868	39.841920
2888.199100	858896.852605	39.846938
2891.393652	860481.723877	39.851956
2893.870889	862094.239828	39.856973
2896.822362	863712.458808	39.861991
2899.682345	865335.013693	39.867008
2902.761242	866950.993077	39.872026
2905.793199	868581.083315	39.877044
2908.455842	870199.266615	39.882061
2911.532637	871847.548938	39.887079
2914.611364	873490.440126	39.892096
2917.489347	875141.817357	39.897114
2920.745030	876784.739885	39.902132
2923.394955	878424.889058	39.907149
2926.541153	880074.366148	39.912167
2929.756575	881728.204512	39.917184
2932.739418	883356.098813	39.922202
2936.089055	884994.399288	39.927220
2938.702418	886664.722640	39.932237
2942.200494	888300.040772	39.937255
2944.972174	889957.898874	39.942272
2947.617077	891621.865681	39.947290
2950.867655	893267.883959	39.952308
2953.530077	894945.649331	39.957325
2956.527277	896617.274645	39.962343
2959.580336	898268.541370	39.967360
2961.936665	899923.876762	39.972378
2965.584184	901588.054622	39.977396
2968.127299	903265.601728	39.982413
2971.266476	904931.766145	39.987431
2974.261081	906625.953686	39.992448
2976.999367	908306.486250	39.997466
2979.853078	909961.672259	40.002484
2982.578141	911636.968290	40.007501
2985.868701	913340.797052	40.012519
2988.719680	915038.501427	40.017536
2991.691807	916730.473292	40.022554
2994.675214	918417.502610	40.027572
2997.473032	920118.638125	40.032589
3000.394955	921808.758225	40.037607
3003.054447	923525.266611	40.042624
3006.200106	925223.306122	40.047642
3008.995004	926887.109328	40.052660
3012.111877	928570.383216	40.057677
3014.839245	930217.824583	40.062695
3017.606867	931873.758288	40.067712
3020.567546	933550.697762	40.072730
3023.644250	935249.208472	40.077748
3026.532720	936935.239019	40.082765
3029.392089	938606.667910	40.087783
3032.488857	940292.067552	40.092800
3035.197434	941981.962076	40.097818
3038.443636	943664.624584	40.102836
3041.540535	945386.621833	40.107853
3044.482273	947119.442574	40.112871
3047.607018	948819.179525	40.117888
3050.670342	950546.627536	40.122906
3053.830498	952263.838871	40.127924
3056.213737	953992.338262	40.132941
3059.035370	955739.733250	40.137959
3061.986115	957558.474424	40.142976
3065.156807	959354.829993	40.147994
3068.451017	961158.721434	40.153012
3071.426761	962989.078532	40.158029
3074.168072	964805.994632	40.163047
3077.168500	966620.340993	40.168064
3079.755533	968456.545431	40.173082
3082.801002	970310.830823	40.178100
3086.024125	972188.006973	40.183117
3089.028428	974067.239017	40.188135
3092.000244	975937.960923	40.193152
3095.007531	977806.116152	40.198170
3097.962576	979698.620022	40.203188
3100.695919	981614.403847	40.208205
3103.872328	983506.000050	40.213223
3106.990027	985424.922147	40.218240
3110.120538	987351.566793	40.223258
3113.616825	989256.094381	40.228276
3116.281797	991192.899761	40.233293
3119.861488	993113.143541	40.238311
3123.552099	995054.103688	40.243328
3126.576555	996970.510241	40.248346
3129.450092	998883.865909	40.253364
3132.308233	1000851.244926	40.258381
3135.502240	1002797.016100	40.263399
3138.532662	1004754.370963	40.268416
3141.584134	1006713.469468	40.273434
3144.983504	1008661.067946	40.278452
3148.096971	1010608.816608	40.283469
3151.215778	1012563.255547	40.288487
3154.726263	1014534.871430	40.293504
3157.943197	1016497.711047	40.298522
3161.083073	1018467.524818	40.303540
3164.267772	1020447.961408	40.308557
3167.144338	1022398.731444	40.313575
3170.151198	1024368.526765	40.318592
3173.368468	1026337.787955	40.323610
3176.613733	1028311.955752	40.328628
3179.568467	1030304.889110	40.333645
3182.698133	1032305.193294	40.338663
3185.726552	1034293.793546	40.343680
3188.982114	1036289.076565	40.348698
3192.232309	1038289.722168	40.353716
3195.632047	1040275.739514	40.358733
3198.853189	1042252.402133	40.363751
3202.343847	1044236.988306	40.368768
3205.275981	1046250.043762	40.373786
3208.889774	1048245.888313	40.378804
3211.648191	1050227.006337	40.383821
3214.590583	1052205.749140	40.388839
3217.712173	1054173.751716	40.393856
3221.036015	1056108.138747	40.398874
3224.090268	1058056.116169	40.403892
3226.913393	1060029.671796	40.408909
3230.048682	1061967.413905	40.413927
3233.251815	1063929.424229	40.418944
3236.026715	1065906.160383	40.423962
3239.370666	1067870.866607	40.428980
3242.428044	1069862.153032	40.433997
3245.227928	1071856.113894	40.439015
3248.794666	1073841.076629	40.444032
3251.792556	1075851.661637	40.449050
3255.104117	1077863.945260	40.454068
3258.399594	1079881.233637	40.459085
3261.242840	1081905.888679	40.464103
3264.496989	1083942.159273	40.469120
3267.483961	1085993.776559	40.474138
3271.111031	1088040.500094	40.479156
3274.222058	1090085.773319	40.484173
3277.433013	1092153.946531	40.489191
3280.654494	1094204.048273	40.494208
3283.793132	1096284.119389	40.499226
3287.105935	1098378.149817	40.504244
3290.375332	1100486.348755	40.509261
3293.571750	1102573.432116	40.514279
3296.876679	1104669.791265	40.519296
3299.823001	1106798.828278	40.524314
3302.842790	1108907.206669	40.529332
3305.759778	1111037.999300	40.534349
3309.138201	1113174.055309	40.539367
3312.289384	1115326.702624	40.544384
3315.723688	1117484.903676	40.549402
3319.152569	1119635.869510	40.554420
3322.459978	1121809.547744	40.559437
3325.780108	1123978.447255	40.564455
3329.284870	1126136.754736	40.569472
3332.766506	1128320.187692	40.574490
3335.992778	1130490.155439	40.579508
3339.787787	1132660.282596	40.584525
3342.991481	1134853.405102	40.589543
3346.453824	1137050.504894	40.594560
3349.982507	1139217.618364	40.599578
3353.294114	1141400.821892	40.604596
3356.926959	1143576.261319	40.609613
3359.950128	1145764.617709	40.614631
3363.898417	1147965.715538	40.619648
3367.004052	1150159.420568	40.624666
3370.289854	1152334.050420	40.629684
3373.446161	1154536.313503	40.634701
3376.587308	1156743.790950	40.639719
3380.290096	1158934.402406	40.644736
3383.160959	1161145.827901	40.649754
3386.707396	1163342.073048	40.654772
3389.911047	1165561.381917	40.659789
3392.868543	1167785.345866	40.664807
3396.611905	1170013.128724	40.669824
3399.800463	1172228.762303	40.674842
3403.063717	1174445.417354	40.679860
3406.774977	1176685.590637	40.684877
3409.426380	1178947.619311	40.689895
3412.893654	1181171.711812	40.694912
3416.248285	1183408.295446	40.699930
3419.738796	1185663.036012	40.704948
3423.005707	1187935.123275	40.709965
3426.323984	1190175.826527	40.714983
3429.927118	1192426.664203	40.720000
3432.929653	1194705.847094	40.725018
3436.321955	1196937.587549	40.730023
3439.699731	1199125.389323	40.735028
3442.580657	1201289.831589	40.740032
3445.779982	1203361.145634	40.745037
3449.126466	1205360.933520	40.750042
3452.738838	1207278.577766	40.755047
3455.576557	1209143.748161	40.760052
3458.184125	1210928.044519	40.765056
3461.705825	1212608.058309	40.770061
3464.197422	1214218.642122	40.775066
3466.684788	1215753.051427	40.780071
3469.692910	1217217.813332	40.785076
3471.678274	1218609.408830	40.790080
3474.332962	1219897.432558	40.795085
3476.565402	1221151.750877	40.800090
3479.004095	1222330.903698	40.805095
3481.003095	1223437.384191	40.810100
3482.889089	1224472.306320	40.815104
3484.712157	1225454.563033	40.820109
3486.255771	1226384.407088	40.825114
3488.075601	1227239.938478	40.830119
3490.207010	1228015.963648	40.835124
3492.055885	1228756.651647	40.840128
3493.608234	1229450.826533	40.845133
3495.119905	1230089.977775	40.850138
3496.484844	1230693.261555	40.855143
3498.133585	1231230.687210	40.860148
3498.993160	1231713.268138	40.865152
3500.592068	1232137.971384	40.870157
3501.456827	1232561.734397	40.875162
3502.772285	1232946.889418	40.880167
3504.042205	1233273.579967	40.885172
3504.724751	1233573.037149	40.890176
3505.913795	1233825.513651	40.895181
3506.634956	1234053.730465	40.900186
3507.505814	1234265.976481	40.905191
3508.407227	1234434.875823	40.910196
3508.783018	1234585.591599	40.915200
3509.582761	1234694.766238	40.920205
3510.316537	1234797.985710	40.925210
3511.194609	1234863.347905	40.930215
3511.972674	1234876.265146	40.935220
3512.584648	1234900.577734	40.940224
3513.232701	1234913.702650	40.945229
3513.516308	1234899.119844	40.950234
3513.993018	1234856.084990	40.955239
3514.670548	1234790.559774	40.960244
3515.016796	1234717.354017	40.965248
3515.358801	1234629.983734	40.970253
3515.963266	1234533.622757	40.975258
3516.342177	1234408.315236	40.980263
3516.691553	1234277.417964	40.985268
3516.924251	1234119.976066	40.990272
3517.486394	1233951.757264	40.995277
3517.845893	1233780.024604	41.000282
3517.903730	1233575.993816	41.005287
3518.344948	1233399.108502	41.010292
3518.294725	1233196.664749	41.015296
3518.665055	1232972.237931	41.020301
3518.900816	1232753.602967	41.025306
3519.005441	1232523.793259	41.030311
3519.785529	1232284.259339	41.035316
3519.615280	1232036.479616	41.040320
3519.672365	1231781.284534	41.045325
3519.912904	1231530.894989	41.050330
3520.207481	1231246.355603	41.055335
3520.436293	1230966.007446	41.060340
3520.215997	1230688.142444	41.065344
3520.542813	1230398.887241	41.070349
3520.708837	1230121.487116	41.075354
3520.895333	1229837.259459	41.080359
3521.020508	1229529.239779	41.085364
3520.936824	1229219.276791	41.090368
3521.561779	1228897.703368	41.095373
3521.125659	1228574.511659	41.100378
3521.468473	1228258.728591	41.105383
3521.534583	1227940.172178	41.110388
3521.724837	1227619.522396	41.115392
3521.870025	1227276.276186	41.120397
3521.906231	1226930.131563	41.125402
3521.866139	1226600.215907	41.130407
3521.887743	1226276.522373	41.135412
3521.615098	1225922.706086	41.140416
3522.189100	1225568.819060	41.145421
3521.889272	1225223.173492	41.150426
3522.226661	1224854.805096	41.155431
3522.288871	1224509.798285	41.160436
3522.455437	1224170.446917	41.165440
3522.310132	1223792.369687	41.170445
3522.018154	1223432.219677	41.175450
3521.989095	1223073.495217	41.180455
3522.411786	1222703.369077	41.185460
3522.404155	1222325.253468	41.190464
3522.227377	1221960.870142	41.195469
3522.705323	1221609.338975	41.200474
3522.406859	1221226.985509	41.205479
3522.720769	1220847.118753	41.210484
3522.546276	1220496.272236	41.215488
3522.405352	1220109.603840	41.220493
3522.579994	1219723.041029	41.225498
3522.761998	1219324.670859	41.230503
3523.053250	1218950.367830	41.235508
3522.804664	1218579.398033	41.240512
3522.907913	1218175.809583	41.245517
3522.857051	1217789.978645	41.250522
3522.824300	1217407.107589	41.255527
3523.247587	1217013.192110	41.260532
3522.890605	1216631.251294	41.265536
3522.954705	1216207.875074	41.270541
3522.986816	1215834.601784	41.275546
3522.596978	1215451.455673	41.280551
3523.079643	1215052.234444	41.285556
3522.916062	1214666.559980	41.290560
3522.820719	1214250.718949	41.295565
3522.823177	1213855.038491	41.300570
3522.806824	1213458.114015	41.305575
3522.855905	1213080.706459	41.310580
3522.532815	1212677.501907	41.315584
3522.792999	1212266.588196	41.320589
3522.709634	1211885.557547	41.325594
3522.574688	1211505.536709	41.330599
3522.447957	1211088.881858	41.335604
3522.570564	1210699.771423	41.340608
3522.529200	1210298.579857	41.345613
3522.149455	1209894.603377	41.350618
3522.271302	1209515.797031	41.355623
3522.566848	1209124.852739	41.360628
3522.377485	1208728.245148	41.365632
3522.538244	1208308.787753	41.370637
3522.520623	1207919.676422	41.375642
3522.481025	1207540.656898	41.380647
3522.567896	1207124.955747	41.385652
3522.154310	1206742.191147	41.390656
3522.524849	1206343.526486	41.395661
3522.720182	1205931.177746	41.400666
3522.558482	1205533.193738	41.405671
3522.462459	1205133.762132	41.410676
3522.413552	1204748.258009	41.415680
3522.516568	1204321.172591	41.420685
3522.475377	1203911.231480	41.425690
3522.435296	1203521.508808	41.430695
3522.705215	1203132.455610	41.435700
3522.462946	1202719.920898	41.440704
3522.553086	1202319.864578	41.445709
3522.357072	1201915.697681	41.450714
3522.113435	1201498.375828	41.455719
3522.182365	1201089.598263	41.460724
3521.861685	1200704.679522	41.465728
3522.053533	1200310.359908	41.470733
3522.014565	1199898.691000	41.475738
3521.873307	1199501.455748	41.480743
3521.772562	1199106.904416	41.485748
3521.842374	1198712.482431	41.490752
3522.061630	1198299.516930	41.495757
3522.242530	1197915.902373	41.500762
3521.750407	1197518.477990	41.505767
3522.146362	1197106.795729	41.510772
3521.682098	1196713.904449	41.515776
3521.857302	1196315.714076	41.520781
3521.696660	1195918.111619	41.525786
3521.481179	1195536.920342	41.530791
3521.785541	1195133.922324	41.535796
3521.618980	1194736.793183	41.540800
3521.725322	1194326.251363	41.545805
3521.819819	1193923.850833	41.550810
3521.239211	1193532.708759	41.555815
3521.630735	1193132.640007	41.560820
3521.454068	1192753.115489	41.565824
3521.531682	1192338.380299	41.570829
3521.616186	1191955.371572	41.575834
3521.337933	1191567.319595	41.580839
3521.716500	1191157.138688	41.585844
3521.268169	1190758.434047	41.590848
3521.442833	1190362.697899	41.595853
3521.512075	1189975.033076	41.600858
3521.172965	1189585.714255	41.605863
3521.424917	1189184.986715	41.610868
3521.341454	1188779.958239	41.615872
3521.631288	1188401.259494	41.620877
3521.454503	1187984.336115	41.625882
3521.189816	1187572.472135	41.630887
3521.468928	1187185.504139	41.635892
3520.938663	1186801.462337	41.640896
3521.092999	1186412.669982	41.645901
3521.228840	1186009.081741	41.650906
3521.144204	1185638.521150	41.655911
3521.239264	1185219.260516	41.660916
3520.931794	1184807.183615	41.665920
3520.989478	1184425.597609	41.670925
3520.927410	1184044.379682	41.675930
3520.952645	1183644.954628	41.680935
3521.038250	1183256.689749	41.685940
3520.492497	1182867.370202	41.690944
3520.740729	1182488.622512	41.695949
3520.822753	1182077.676614	41.700954
3520.916019	1181683.361520	41.705959
3520.794323	1181297.055527	41.710964
3520.688293	1180918.063267	41.715968
3520.793667	1180518.478511	41.720973
3520.889796	1180122.443450	41.725978
3520.834264	1179729.040468	41.730983
3520.616915	1179341.568697	41.735988
3520.405861	1178950.769893	41.740992
3520.509552	1178576.941869	41.745997
3520.940740	1178184.095473	41.751002
3520.414474	1177775.076311	41.756007
3520.689102	1177388.037482	41.761012
3520.863601	1177013.802753	41.766016
3520.342112	1176605.067748	41.771021
3520.313801	1176224.683709	41.776026
3520.279644	1175855.772454	41.781031
3520.563871	1175461.707876	41.786036
3520.264909	1175084.490153	41.791040
3520.097378	1174673.188320	41.796045
3520.213913	1174279.250462	41.801050
3520.169521	1173925.195842	41.806055
3520.368004	1173546.653305	41.811060
3519.996733	1173151.861855	41.816064
3520.274545	1172750.520170	41.821069
3520.266967	1172371.737634	41.826074
3519.814682	1171980.077742	41.831079
3520.112825	1171598.264481	41.836084
3520.008264	1171240.924384	41.841088
3519.807863	1170844.137563	41.846093
3519.950767	1170461.889333	41.851098
3519.804748	1170068.337061	41.856103
3519.884730	1169703.312195	41.861108
3519.676415	1169334.534216	41.866112
3519.428523	1168938.459762	41.871117
3519.653614	1168565.686373	41.876122
3519.955501	1168174.277383	41.881127
3519.668633	1167798.040830	41.886132
3519.503599	1167423.173299	41.891136
3519.575608	1167031.338945	41.896141
3519.673240	1166665.721284	41.901146
3519.394558	1166292.774356	41.906151
3519.500204	1165910.765856	41.911156
3519.348688	1165545.488686	41.916160
3519.280798	1165155.803566	41.921165
3519.356924	1164776.361788	41.926170
3519.307675	1164408.438015	41.931175
3519.733141	1164035.686577	41.936180
3519.322102	1163662.290545	41.941184
3518.981967	1163284.415357	41.946189
3519.275104	1162905.936148	41.951194
3519.247422	1162541.940903	41.956199
3519.130180	1162153.174451	41.961204
3519.155628	1161793.654806	41.966208
3519.149394	1161428.539066	41.971213
3519.283309	1161055.340086	41.976218
3518.733226	1160684.117860	41.981223
3519.088217	1160305.062569	41.986228
3518.806356	1159947.735944	41.991232
3518.860717	1159558.465218	41.996237
3518.917199	1159194.412836	42.001242
3518.757723	1158842.191571	42.006247
3518.878775	1158481.294360	42.011252
3518.750807	1158113.036171	42.016256
3518.830507	1157748.123055	42.021261
3519.067075	1157362.537543	42.026266
3518.671716	1157002.664309	42.031271
3519.039467	1156629.112090	42.036276
3518.954265	1156268.286033	42.041280
3518.581402	1155889.694161	42.046285
3518.750353	1155528.775493	42.051290
3518.658665	1155157.843938	42.056295
3518.506556	1154801.659879	42.061300
3518.354053	1154449.994744	42.066304
3518.262816	1154072.172092	42.071309
3518.198004	1153701.701351	42.076314
3518.182247	1153368.021187	42.081319
3518.258238	1153004.483381	42.086324
3518.396505	1152636.460361	42.091328
3518.485131	1152266.526110	42.096333
3518.204328	1151914.807408	42.101338
3518.176064	1151585.372127	42.106343
3518.356527	1151207.015029	42.111348
3518.227712	1150847.244918	42.116352
3518.134772	1150482.140211	42.121357
3518.271951	1150143.873642	42.126362
3518.097072	1149772.197395	42.131367
3518.218468	1149395.425143	42.136372
3518.080609	1149052.302313	42.141376
3518.159383	1148698.604395	42.146381
3518.290906	1148337.862205	42.151386
3518.084042	1147984.258207	42.156391
3518.246209	1147606.498652	42.161396
3517.893127	1147255.807752	42.166400
3518.007143	1146901.983639	42.171405
3518.062902	1146544.922650	42.176410
3517.652842	1146189.715323	42.181415
3517.773550	1145821.503866	42.186420
3517.863206	1145469.294213	42.191424
3517.456141	1145130.795943	42.196429
3517.714393	1144769.220223	42.201434
3517.792060	1144421.778528	42.206439
3517.855985	1144075.549079	42.211444
3517.703666	1143731.798362	42.216448
3517.829995	1143379.253761	42.221453
3517.585446	1143005.310509	42.226458
3516.727254	1142661.132206	42.231463
3517.243629	1142323.819858	42.236468
3517.706891	1141995.412458	42.241472
3517.436928	1141632.855537	42.246477
3517.637082	1141275.319982	42.251482
3517.300691	1140944.132631	42.256487
3517.523670	1140593.189413	42.261492
3517.311393	1140239.637424	42.266496
3517.520155	1139878.210144	42.271501
3517.169488	1139553.296939	42.276506
3516.824558	1139220.674463	42.281511
3516.953840	1138858.431388	42.286516
3517.025875	1138505.476283	42.291520
3517.163925	1138184.195926	42.296525
3517.312411	1137848.083276	42.301530
3517.131993	1137500.514635	42.306535
3517.279510	1137131.883979	42.311540
3516.973997	1136813.727228	42.316544
3516.921950	1136465.120006	42.321549
3516.699374	1136115.093361	42.326554
3516.652620	1135783.630816	42.331559
3516.574648	1135456.332106	42.336564
3516.410148	1135124.847833	42.341568
3516.420221	1134761.204756	42.346573
3516.761233	1134454.294919	42.351578
3516.458119	1134129.896678	42.356583
3516.858567	1133777.048069	42.361588
3516.576674	1133447.948922	42.366592
3516.403344	1133117.101017	42.371597
3516.842072	1132793.829447	42.376602
3516.087320	1132463.891952	42.381607
3516.262567	1132125.796997	42.386612
3516.093537	1131795.626530	42.391616
3516.093521	1131453.810732	42.396621
3516.137594	1131142.576113	42.401626
3516.088516	1130816.602979	42.406631
3515.884665	1130488.543727	42.411636
3515.941688	1130164.224517	42.416640
3515.767159	1129844.678003	42.421645
3516.149119	1129535.195493	42.426650
3516.024450	1129214.937344	42.431655
3515.747072	1128869.863094	42.436660
3515.766319	1128555.723347	42.441664
3515.775409	1128256.975339	42.446669
3515.847336	1127928.047139	42.451674
3515.969303	1127592.907188	42.456679
3516.054626	1127274.400354	42.461684
3515.737650	1126963.837183	42.466688
3515.514296	1126633.640967	42.471693
3515.789447	1126309.526918	42.476698
3515.818971	1125997.137700	42.481703
3515.929554	1125674.344343	42.486708
3515.693717	1125353.587010	42.491712
3515.458099	1125040.995153	42.496717
3515.485914	1124721.393638	42.501722
3515.244639	1124404.958358	42.506727
3515.610709	1124076.410479	42.511732
3515.288014	1123789.555881	42.516736
3515.405800	1123474.148641	42.521741
3515.732509	1123159.164402	42.526746
3515.189211	1122861.157221	42.531751
3515.295936	1122531.795383	42.536756
3515.550359	1122214.577396	42.541760
3515.290988	1121918.375318	42.546765
3515.415829	1121599.142378	42.551770
3515.506886	1121286.657907	42.556775
3515.339810	1120964.006531	42.561780
3515.410227	1120643.582583	42.566784
3515.007127	1120339.029899	42.571789
3515.705802	1120026.752786	42.576794
3515.420572	1119711.570963	42.581799
3515.352282	1119377.470858	42.586804
3515.084886	1119078.730999	42.591808
3514.949414	1118777.475368	42.596813
3515.073689	1118465.964089	42.601818
3515.060905	1118157.887868	42.606823
3514.923105	1117844.477713	42.611828
3514.800649	1117522.850396	42.616832
3514.868335	1117236.628234	42.621837
3515.256790	1116939.185972	42.626842
3514.875037	1116641.186805	42.631847
3514.752502	1116335.692876	42.636852
3514.555339	1116046.876966	42.641856
3514.804696	1115721.648355	42.646861
3514.917092	1115408.531210	42.651866
3514.259533	1115117.357465	42.656871
3514.648472	1114805.780514	42.661876
3514.490414	1114516.208241	42.666880
3514.462315	1114212.389615	42.671885
3514.525420	1113924.942397	42.676890
3514.450006	1113628.441974	42.681895
3514.231898	1113317.450844	42.686900
3514.557535	1113026.955505	42.691904
3514.081793	1112751.457396	42.696909
3514.378738	1112432.221954	42.701914
3514.349630	1112128.953349	42.706919
3514.443059	1111841.962027	42.711924
3514.397375	1111551.066398	42.716928
3514.118245	1111255.422608	42.721933
3514.357724	1110968.360575	42.726938
3514.033574	1110683.093733	42.731943
3514.310034	1110366.792633	42.736948
3514.156555	1110074.212458	42.741952
3513.931649	1109801.957522	42.746957
3514.112938	1109510.914093	42.751962
3513.742281	1109217.368579	42.756967
3514.105815	1108911.276494	42.761972
3514.036261	1108637.600607	42.766976
3513.821809	1108359.638578	42.771981
3514.052908	1108062.398596	42.776986
3513.955218	1107788.875128	42.781991
3513.971201	1107494.408095	42.786996
3514.012497	1107203.740353	42.792001
3513.601987	1106912.749354	42.797005
3513.862338	1106607.784704	42.802010
3513.893180	1106321.846066	42.807015
3514.150727	1106051.518500	42.812020
3513.887334	1105767.986662	42.817025
3513.517178	1105475.001036	42.822029
3513.839884	1105206.912843	42.827034
3513.783420	1104913.080809	42.832039
3513.476534	1104615.070461	42.837044
3513.616745	1104338.562059	42.842049
3513.752443	1104063.664485	42.847053
3513.896317	1103758.080036	42.852058
3513.754769	1103478.803005	42.857063
3513.520865	1103195.035397	42.862068
3513.693457	1102899.526949	42.867073
3513.589961	1102630.234075	42.872077
3513.581994	1102364.543872	42.877082
3513.574154	1102075.136788	42.882087
3513.794460	1101774.971072	42.887092
3513.519227	1101503.834157	42.892097
3513.141371	1101240.826083	42.897101
3513.645778	1100954.907186	42.902106
3513.106288	1100689.126463	42.907111
3513.250277	1100409.834782	42.912116
3513.226188	1100107.800072	42.917121
3513.155406	1099827.175038	42.922125
3513.572450	1099560.894402	42.927130
3513.264939	1099307.629908	42.932135
3513.021518	1099011.499036	42.937140
3513.010905	1098737.406261	42.942145
3513.177301	1098473.504326	42.947149
3513.486488	1098207.270435	42.952154
3512.979211	1097923.079438	42.957159
3512.820855	1097655.556241	42.962164
3513.036489	1097380.113855	42.967169
3512.574817	1097101.324950	42.972173
3512.727567	1096842.416083	42.977178
3512.606816	1096579.999820	42.982183
3512.638546	1096310.369577	42.987188
3512.381997	1096046.227522	42.992193
3512.286061	1095778.888309	42.997197
3512.496106	1095519.428270	43.002202
3512.395043	1095263.452259	43.007207
3512.682543	1095008.835727	43.012212
3512.493469	1094754.859976	43.017217
3512.616685	1094482.539490	43.022221
3512.512203	1094211.487166	43.027226
3512.260457	1093966.865249	43.032231
3512.604899	1093693.607171	43.037236
3512.647453	1093421.629569	43.042241
3512.507362	1093172.836900	43.047245
3512.683110	1092924.172279	43.052250
3512.387275	1092661.403469	43.057255
3512.382669	1092394.552412	43.062260
3512.619217	1092122.381934	43.067265
3512.476534	1091865.103154	43.072269
3512.168044	1091611.382781	43.077274
3511.981289	1091346.712762	43.082279
3512.157918	1091087.237567	43.087284
3511.998855	1090847.918763	43.092289
3512.168080	1090595.413096	43.097293
3512.320118	1090328.434608	43.102298
3512.141682	1090090.043453	43.107303
3512.210745	1089842.596233	43.112308
3511.924153	1089582.167423	43.117313
3511.795746	1089329.077076	43.122317
3512.015627	1089071.701943	43.127322
3511.635105	1088823.228411	43.132327
3512.256476	1088555.127304	43.137332
3511.691390	1088315.763741	43.142337
3511.653210	1088083.777374	43.147341
3511.877474	1087815.513533	43.152346
3511.572208	1087566.395126	43.157351
3511.390748	1087334.879570	43.162356
3511.588675	1087096.390862	43.167361
3511.803797	1086856.355283	43.172365
3511.995120	1086605.002357	43.177370
3511.806348	1086354.179705	43.182375
3511.776915	1086082.804711	43.187380
3511.641737	1085858.600076	43.192385
3511.679659	1085619.785376	43.197389
3511.446306	1085363.651499	43.202394
3511.697115	1085099.276046	43.207399
3511.505656	1084860.369915	43.212404
3511.352201	1084622.693581	43.217409
3511.446634	1084390.719582	43.222413
3511.780851	1084166.272017	43.227418
3511.441627	1083927.445168	43.232423
3511.422483	1083671.196357	43.237428
3511.790962	1083419.667119	43.242433
3511.379159	1083190.506737	43.247437
3511.282388	1082955.817527	43.252442
3511.357981	1082704.687186	43.257447
3511.053929	1082453.415944	43.262452
3511.524044	1082223.014418	43.267457
3510.910708	1081991.438513	43.272461
3510.859674	1081750.837855	43.277466
3511.253505	1081535.386258	43.282471
3511.052259	1081284.523896	43.287476
3511.012738	1081042.163020	43.292481
3510.702489	1080821.521856	43.297485
3510.916287	1080599.825864	43.302490
3510.971391	1080364.712175	43.307495
3511.140278	1080110.759993	43.312500
3511.060012	1079889.947294	43.317505
3510.880952	1079665.590837	43.322509
3510.777950	1079424.992084	43.327514
3510.736147	1079195.890701	43.332519
3510.768781	1078968.687194	43.337524
3510.789617	1078751.843267	43.342529
3510.693975	1078529.826160	43.347533
3510.773660	1078274.459280	43.352538
3510.848868	1078050.378540	43.357543
3510.906063	1077836.276373	43.362548
3510.761892	1077605.781007	43.367553
3510.200321	1077379.761376	43.372557
3510.937249	1077170.802033	43.377562
3510.525075	1076943.203421	43.382567
3510.395273	1076698.455929	43.387572
3510.731600	1076483.870672	43.392577
3510.337091	1076283.418473	43.397581
3510.455849	1076046.283620	43.402586
3510.652158	1075837.362348	43.407591
3510.549377	1075612.442578	43.412596
3510.553847	1075385.766978	43.417601
3510.530616	1075156.300956	43.422605
3510.414344	1074927.320922	43.427610
3510.543827	1074716.734842	43.432615
3510.286072	1074487.471505	43.437620
3510.647777	1074281.153400	43.442625
3510.248148	1074065.921971	43.447629
3510.375342	1073833.973847	43.452634
3510.144698	1073615.910619	43.457639
3510.166095	1073384.825618	43.462644
3510.341945	1073169.656317	43.467649
3510.126655	1072953.485952	43.472653
3510.200816	1072736.874988	43.477658
3510.198185	1072534.683231	43.482663
3510.054560	1072325.587716	43.487668
3510.211474	1072098.270259	43.492673
3510.051279	1071899.252564	43.497677
3509.945679	1071669.461634	43.502682
3510.236595	1071440.364717	43.507687
3509.927185	1071242.981786	43.512692
3510.300877	1071043.652826	43.517697
3510.366797	1070812.740314	43.522701
3510.085660	1070589.181486	43.527706
3510.108666	1070394.212731	43.532711
3509.791930	1070180.160759	43.537716
3510.168536	1069957.140813	43.542721
3510.029604	1069726.889310	43.547725
3510.061401	1069519.580784	43.552730
3509.917305	1069321.332165	43.557735
3509.700443	1069110.491309	43.562740
3509.826770	1068887.372916	43.567745
3509.949202	1068700.213042	43.572749
3509.848740	1068475.384219	43.577754
3509.584856	1068277.309926	43.582759
3509.685080	1068065.318734	43.587764
3509.817051	1067866.972072	43.592769
3509.624891	1067670.980091	43.597773
3509.539708	1067442.932297	43.602778
3509.621739	1067245.437108	43.607783
3509.547773	1067028.817276	43.612788
3509.534653	1066843.828943	43.617793
3509.463557	1066621.228117	43.622797
3509.631889	1066427.248844	43.627802
3509.445277	1066239.190060	43.632807
3509.230605	1066027.653084	43.637812
3509.150900	1065825.611358	43.642817
3509.147617	1065635.192452	43.647821
3509.494301	1065440.186728	43.652826
3509.118654	1065237.979676	43.657831
3509.240802	1065048.963223	43.662836
3509.178629	1064832.447263	43.667841
3509.279355	1064649.098493	43.672845
3509.268024	1064441.797703	43.677850
3509.346995	1064266.909112	43.682855
3509.318727	1064070.569107	43.687860
3509.300670	1063856.798668	43.692865
3508.975822	1063661.262911	43.697869
3509.009316	1063469.030269	43.702874
3509.355294	1063290.119984	43.707879
3509.138046	1063090.984499	43.712884
3509.097291	1062881.223050	43.717889
3508.842382	1062700.274605	43.722893
3508.969605	1062496.054639	43.727898
3509.197938	1062316.361850	43.732903
3509.034034	1062123.633296	43.737908
3509.052876	1061929.423593	43.742913
3509.150561	1061725.853914	43.747917
3508.884823	1061542.365617	43.752922
3508.724361	1061369.253882	43.757927
3508.665010	1061180.808418	43.762932
3509.081924	1060972.824825	43.767937
3508.877306	1060790.168112	43.772941
3509.163753	1060581.228154	43.777946
3509.252467	1060400.725344	43.782951
3508.877412	1060219.522467	43.787956
3508.954044	1060015.507743	43.792961
3508.687343	1059832.829492	43.797965
3508.862013	1059652.769628	43.802970
3508.959256	1059465.877229	43.807975
3508.741065	1059258.704152	43.812980
3508.861051	1059077.863841	43.817985
3508.576551	1058894.386703	43.822989
3508.765703	1058706.104641	43.827994
3508.596399	1058538.878630	43.832999
3508.431719	1058341.778568	43.838004
3508.581817	1058144.715967	43.843009
3508.462759	1057976.501088	43.848013
3508.658292	1057778.550716	43.853018
3508.930171	1057598.215000	43.858023
3508.347450	1057420.326910	43.863028
3508.806843	1057259.704123	43.868033
3508.644971	1057069.785733	43.873037
3508.961754	1056871.397349	43.878042
3509.009317	1056681.045581	43.883047
3508.563509	1056491.732319	43.888052
3508.805988	1056304.323282	43.893057
3508.556084	1056125.278355	43.898061
3508.623978	1055950.512878	43.903066
3508.530650	1055753.115743	43.908071
3508.478345	1055569.682485	43.913076
3508.602490	1055385.153658	43.918081
3508.526936	1055198.723469	43.923085
3508.259965	1055028.225724	43.928090
3508.401528	1054842.133362	43.933095
3508.349942	1054675.252839	43.938100
3508.365368	1054499.293095	43.943105
3508.308618	1054324.882343	43.948109
3508.223809	1054135.814458	43.953114
3508.287220	1053981.236126	43.958119
3508.154516	1053789.271499	43.963124
3508.344721	1053605.925910	43.968129
3508.042541	1053448.596355	43.973133
3508.558812	1053264.510693	43.978138
3508.396471	1053066.160907	43.983143
3508.340514	1052906.557208	43.988148
3508.591972	1052746.705375	43.993153
3508.056639	1052564.987896	43.998157
3508.388312	1052367.881987	44.003162
3508.350933	1052195.812167	44.008167
3508.279587	1052029.144323	44.013172
3508.386662	1051844.017706	44.018177
3507.522425	1051683.354248	44.023181
3507.636430	1051504.388911	44.028186
3508.223317	1051334.504718	44.033191
3508.052594	1051162.907071	44.038196
3508.315304	1050976.857521	44.043201
3507.816403	1050800.382297	44.048205
3508.012384	1050643.566196	44.053210
3507.868663	1050487.573491	44.058215
3507.878466	1050322.095153	44.063220
3507.995434	1050132.760585	44.068225
3507.782520	1049957.465765	44.073229
3508.031963	1049793.476084	44.078234
3508.013278	1049632.613751	44.083239
3507.660067	1049468.327687	44.088244
3507.759899	1049311.489677	44.093249
3507.674797	1049132.673427	44.098253
3507.798829	1048952.562285	44.103258
3508.027154	1048794.433796	44.108263
3507.936657	1048616.277369	44.113268
3508.136746	1048460.750019	44.118273
3507.519942	1048304.484122	44.123277
3507.751226	1048132.726280	44.128282
3507.568373	1047968.078043	44.133287
3507.376795	1047808.156476	44.138292
3507.787912	1047637.029381	44.143297
3507.737379	1047480.646966	44.148301
3507.526767	1047313.956540	44.153306
3507.503943	1047165.573629	44.158311
3507.571697	1046990.042068	44.163316
3507.720689	1046817.194980	44.168321
3507.725069	1046688.684175	44.173325
3507.700767	1046514.118230	44.178330
3507.627909	1046356.935333	44.183335
3507.341431	1046198.045059	44.188340
3507.559161	1046014.153622	44.193345
3507.201615	1045868.205215	44.198349
3507.410907	1045702.652531	44.203354
3507.448074	1045533.936354	44.208359
3507.468295	1045389.265139	44.213364
3507.469699	1045231.941540	44.218369
3507.112140	1045071.968336	44.223373
3507.237176	1044890.662596	44.228378
3507.365326	1044745.473894	44.233383
3507.123544	1044611.643225	44.238388
3507.521856	1044445.538951	44.243393
3507.383477	1044294.200463	44.248397
3507.339016	1044121.108010	44.253402
3507.479134	1043963.339199	44.258407
3507.271449	1043803.980938	44.263412
3507.476229	1043651.795589	44.268417
3507.269873	1043502.185594	44.273421
3507.319374	1043344.510728	44.278426
3507.159424	1043201.357907	44.283431
3507.106604	1043044.850742	44.288436
3507.164706	1042872.185527	44.293441
3506.902028	1042734.738116	44.298445
3507.247065	1042588.587678	44.303450
3507.408072	1042438.695267	44.308455
3507.018579	1042279.419803	44.313460
3507.192920	1042113.572544	44.318465
3507.256465	1041972.187234	44.323469
3506.811086	1041812.327765	44.328474
3506.876513	1041671.031118	44.333479
3506.730356	1041514.496193	44.338484
3507.031324	1041371.413565	44.343489
3507.002445	1041242.008890	44.348493
3506.997545	1041082.152506	44.353498
3506.825244	1040925.701949	44.358503
3506.844004	1040772.791779	44.363508
3506.999395	1040646.435867	44.368513
3507.129121	1040512.251843	44.373517
3506.877997	1040353.381651	44.378522
3506.937255	1040187.785861	44.383527
3506.899197	1040042.888228	44.388532
3506.840915	1039909.687309	44.393537
3506.547068	1039758.057430	44.398541
3506.585246	1039623.093639	44.403546
3506.883647	1039476.385667	44.408551
3506.307194	1039325.660642	44.413556
3506.391289	1039186.134685	44.418561
3506.575610	1039056.450649	44.423565
3506.244217	1038909.444710	44.428570
3506.499612	1038770.073482	44.433575
3506.473143	1038659.559589	44.438580
3506.585038	1038505.024634	44.443585
3506.317462	1038380.234015	44.448589
3506.381523	1038233.821969	44.453594
3506.565565	1038092.801637	44.458599
3506.562367	1037940.494113	44.463604
3506.676743	1037813.887196	44.468609
3506.265327	1037678.370028	44.473613
3506.495166	1037546.032144	44.478618
3506.370743	1037394.793481	44.483623
3506.179098	1037264.065742	44.488628
3506.650172	1037115.429478	44.493633
3506.119346	1036983.783826	44.498637
3506.060505	1036864.824846	44.503642
3506.461625	1036727.119494	44.508647
3506.183992	1036585.556665	44.513652
3506.232412	1036452.061923	44.518657
3506.258401	1036337.527319	44.523661
3506.166847	1036207.048471	44.528666
3506.356243	1036072.941015	44.533671
3506.314359	1035945.930412	44.538676
3506.621706	1035786.644309	44.543681
3505.903142	1035652.966510	44.548685
3505.692634	1035531.875654	44.553690
3505.669479	1035407.848844	44.558695
3505.747177	1035294.348513	44.563700
3505.601037	1035155.436692	44.568705
3505.875681	1035041.124742	44.573709
3505.862462	1034923.277842	44.578714
3506.079803	1034781.781154	44.583719
3506.007068	1034665.583523	44.588724
3506.439130	1034546.977999	44.593729
3506.213175	1034410.092786	44.598733
3506.303610	1034263.572006	44.603738
3506.300527	1034139.513666	44.608743
3506.018565	1033997.982552	44.613748
3506.321166	1033875.609914	44.618753
3506.043834	1033753.523663	44.623757
3506.170258	1033613.560747	44.628762
3506.177311	1033485.905335	44.633767
3505.760326	1033355.897228	44.638772
3506.005357	1033237.778596	44.643777
3506.029250	1033112.047583	44.648781
3506.123270	1032963.362700	44.653786
3506.278049	1032840.217369	44.658791
3506.111012	1032711.411384	44.663796
3506.134785	1032578.021494	44.668801
3506.030001	1032475.431994	44.673805
3505.826954	1032324.746223	44.678810
3505.947061	1032192.396075	44.683815
3506.296865	1032091.273516	44.688820
3506.299205	1031964.552132	44.693825
3505.853888	1031836.643058	44.698829
3505.819674	1031703.241808	44.703834
3505.827778	1031573.993463	44.708839
3505.670096	1031450.288033	44.713844
3505.928056	1031341.324795	44.718849
3505.977451	1031222.033894	44.723853
3505.970570	1031075.639050	44.728858
3505.934255	1030958.486762	44.733863
3505.715770	1030836.423785	44.738868
3505.692686	1030709.678100	44.743873
3505.726151	1030587.084023	44.748877
3505.742897	1030460.422953	44.753882
3506.085253	1030339.225084	44.758887
3505.789029	1030228.782029	44.763892
3505.673030	1030105.620969	44.768897
3505.993252	1029966.018860	44.773901
3505.861954	1029846.437805	44.778906
3505.921563	1029740.090827	44.783911
3505.627322	1029609.006699	44.788916
3505.791297	1029475.519584	44.793921
3505.449393	1029381.047803	44.798925
3505.124915	1029270.299883	44.803930
3505.262459	1029142.233054	44.808935
3505.144094	1029025.925459	44.813940
3505.394885	1028906.261349	44.818945
3505.254644	1028801.866662	44.823949
3505.106891	1028693.499785	44.828954
3505.158430	1028578.801612	44.833959
3504.851127	1028479.271777	44.838964
3505.054994	1028357.860015	44.843969
3505.074227	1028255.850641	44.848973
3505.132058	1028151.217433	44.853978
3505.300400	1028044.432782	44.858983
3505.059094	1027926.572532	44.863988
3505.295959	1027802.527557	44.868993
3505.077993	1027719.536063	44.873997
3504.845519	1027597.113947	44.879002
3505.003485	1027480.244255	44.884007
3505.060803	1027392.067581	44.889012
3505.061619	1027287.912050	44.894017
3505.141522	1027189.361257	44.899021
3505.062120	1027078.045064	44.904026
3505.149602	1026940.246707	44.909031
3504.633544	1026847.020402	44.914036
3504.827910	1026752.415848	44.919041
3504.763224	1026650.487912	44.924045
3504.724743	1026526.169285	44.929050
3505.038884	1026439.873363	44.934055
3504.884088	1026351.327604	44.939060
3504.996422	1026245.777621	44.944065
3504.953799	1026134.921142	44.949069
3504.871822	1026035.019944	44.954074
3505.063810	1025912.006475	44.959079
3504.993416	1025838.654101	44.964084
3504.783810	1025725.684892	44.969089
3504.897029	1025604.422138	44.974093
3504.719134	1025513.637793	44.979098
3504.715655	1025432.321594	44.984103
3504.684399	1025338.214909	44.989108
3504.968391	1025208.095407	44.994113
3504.923354	1025122.129112	44.999117
3505.091495	1025021.199353	45.004122
3504.917747	1024909.758631	45.009127
3504.905509	1024817.869478	45.014132
3504.727441	1024701.869503	45.019137
3504.944354	1024594.332473	45.024141
3504.822715	1024502.262286	45.029146
3505.239048	1024412.040772	45.034151
3504.799703	1024301.891908	45.039156
3504.853180	1024193.404686	45.044161
3504.667744	1024104.246760	45.049165
3504.545064	1023998.402282	45.054170
3504.965499	1023893.144993	45.059175
3504.641479	1023808.173960	45.064180
3504.888795	1023702.262950	45.069185
3504.868417	1023588.734690	45.074189
3504.222765	1023508.950632	45.079194
3504.821663	1023415.192621	45.084199
3504.229729	1023324.247049	45.089204
3504.637049	1023226.445186	45.094209
3504.748978	1023125.102687	45.099213
3504.491179	1023024.401030	45.104218
3504.580528	1022928.197751	45.109223
3504.505576	1022843.461954	45.114228
3504.737992	1022726.480758	45.119233
3504.595726	1022644.759070	45.124237
3504.651269	1022535.754564	45.129242
3504.738872	1022435.664243	45.134247
3504.491771	1022349.785650	45.139252
3504.476987	1022266.000964	45.144257
3504.654820	1022161.817875	45.149261
3504.357098	1022066.730327	45.154266
3504.582607	1021981.447112	45.159271
3504.452250	1021874.496979	45.164276
3504.465804	1021784.687462	45.169281
3504.449993	1021679.266498	45.174285
3504.184914	1021602.011221	45.179290
3504.705957	1021499.796059	45.184295
3504.443917	1021403.236530	45.189300
3504.378441	1021314.596399	45.194305
3504.396489	1021241.169240	45.199309
3504.237494	1021154.093883	45.204314
3504.449804	1021051.242431	45.209319
3504.589922	1020966.636838	45.214324
3504.336620	1020879.378750	45.219329
3504.477353	1020780.123138	45.224333
3504.406834	1020703.696459	45.229338
3504.366128	1020594.185049	45.234343
3504.213718	1020497.785882	45.239348
3504.297578	1020411.532063	45.244353
3504.596582	1020339.016911	45.249357
3504.478600	1020257.741476	45.254362
3504.827368	1020146.410978	45.259367
3504.587728	1020060.011012	45.264372
3504.579742	1019954.168282	45.269377
3504.677280	1019861.888735	45.274381
3504.471499	1019772.859279	45.279386
3504.570478	1019679.703322	45.284391
3504.696410	1019596.340688	45.289396
3504.602723	1019483.808629	45.294401
3504.534373	1019387.764646	45.299405
3504.631269	1019291.885860	45.304410
3504.292371	1019195.495034	45.309415
3504.153083	1019108.287647	45.314420
3504.395825	1019019.754559	45.319425
3504.134526	1018942.656087	45.324429
3503.787581	1018848.007229	45.329434
3504.391006	1018760.769155	45.334439
3504.266261	1018674.717083	45.339444
3503.898423	1018592.779415	45.344449
3503.996102	1018519.885775	45.349453
3503.871912	1018429.074818	45.354458
3504.129317	1018329.756666	45.359463
3504.144325	1018265.510308	45.364468
3504.325639	1018165.522466	45.369473
3504.313086	1018090.118171	45.374477
3504.076554	1018007.179841	45.379482
3503.991650	1017929.359047	45.384487
3503.990685	1017855.017254	45.389492
3504.193664	1017740.169171	45.394497
3504.335486	1017653.960499	45.399501
3504.013904	1017584.908976	45.404506
3504.057615	1017500.364085	45.409511
3503.693500	1017411.808551	45.414516
3503.860018	1017316.272816	45.419521
3503.702022	1017247.287260	45.424525
3503.871046	1017182.906092	45.429530
3503.796438	1017095.365596	45.434535
3503.554503	1017029.109031	45.439540
3504.027193	1016951.474058	45.444545
3504.148365	1016861.276822	45.449549
3503.688318	1016773.697727	45.454554
3504.089090	1016690.052554	45.459559
3503.794097	1016634.283942	45.464564
3503.945987	1016542.620426	45.469569
3504.162935	1016455.604399	45.474573
3503.816242	1016386.056885	45.479578
3504.025882	1016295.738928	45.484583
3503.983877	1016214.004118	45.489588
3503.963811	1016130.711185	45.494593
3503.994335	1016058.961676	45.499597
3503.757435	1015979.197228	45.504602
3503.956487	1015898.388980	45.509607
3503.676960	1015835.522562	45.514612
3503.762485	1015773.857471	45.519617
3504.073293	1015690.309342	45.524621
3503.700844	1015606.872505	45.529626
3504.188270	1015518.341057	45.534631
3504.074924	1015443.112031	45.539636
3503.953514	1015360.504042	45.544641
3503.849865	1015273.522532	45.549645
3503.598092	1015210.741651	45.554650
3503.863288	1015103.208937	45.559655
3503.710165	1015034.680919	45.564660
3503.584198	1014982.169519	45.569665
3503.600122	1014911.961422	45.574669
3503.370694	1014835.578142	45.579674
3503.870817	1014727.805353	45.584679
3503.407965	1014689.232964	45.589684
3503.799594	1014613.229915	45.594689
3503.934985	1014527.945463	45.599693
3503.628006	1014437.100094	45.604698
3503.821244	1014373.265450	45.609703
3503.796197	1014308.300666	45.614708
3504.017525	1014218.238777	45.619713
3503.928153	1014133.470945	45.624717
3503.552807	1014067.492786	45.629722
3503.474433	1013993.501148	45.634727
3503.600226	1013917.532493	45.639732
3503.520762	1013859.564186	45.644737
3503.829868	1013769.772031	45.649741
3503.507531	1013687.172559	45.654746
3503.531754	1013607.331455	45.659751
3503.493444	1013548.090520	45.664756
3503.682812	1013492.405207	45.669761
3503.885021	1013416.611465	45.674765
3503.596582	1013348.959362	45.679770
3503.518247	1013254.657666	45.684775
3503.503876	1013166.657553	45.689780
3503.637097	1013102.624123	45.694785
3503.625414	1013046.481840	45.699789
3503.585027	1012962.951076	45.704794
3503.722239	1012880.458348	45.709799
3503.527799	1012833.377933	45.714804
3503.457545	1012744.797595	45.719809
3503.959924	1012661.367246	45.724813
3503.426154	1012608.415142	45.729818
3503.336827	1012528.480298	45.734823
3503.515770	1012432.082410	45.739828
3503.524019	1012294.131442	45.744833
3503.954193	1012108.114707	45.749837
3503.623264	1011868.684396	45.754842
3503.551441	1011561.674425	45.759847
3503.450059	1011163.898118	45.764852
3503.399780	1010708.946026	45.769857
3503.588249	1010220.194942	45.774861
3503.337978	1009644.290956	45.779866
3503.356026	1008988.478555	45.784871
3502.811033	1008310.711536	45.789876
3503.268691	1007521.563924	45.794881
3503.339731	1006678.982112	45.799885
3503.022510	1005747.247580	45.804890
3503.093968	1004743.990366	45.809895
3502.576113	1003692.295733	45.814900
3502.524840	1002541.844894	45.819905
3502.483211	1001332.366930	45.824909
3502.028271	1000037.412039	45.829914
3501.958999	998648.707333	45.834919
3501.868328	997186.609740	45.839924
3501.900033	995628.921311	45.844929
3501.701572	994001.254761	45.849933
3501.149241	992296.063786	45.854938
3501.400970	990501.385558	45.859943
3501.060350	988632.877447	45.864948
3500.598098	986647.548194	45.869953
3500.674516	984580.605663	45.874957
3499.996000	982431.784571	45.879962
3500.188966	980199.064599	45.884967
3499.759065	977883.279059	45.889972
3499.311780	975485.108562	45.894977
3499.145882	972990.804498	45.899981
3498.667385	970407.778813	45.904986
3498.819271	967733.799920	45.909991
3498.321537	964997.753864	45.914996
3498.104386	962143.928934	45.920001
3497.841513	959190.248991	45.925005
3497.523733	956179.046156	45.930010
3496.959207	953142.680434	45.935015
3496.665587	950022.785891	45.940020
3495.838081	946813.822348	45.945025
3495.493976	943529.846749	45.950029
3494.914025	940167.972240	45.955034
3494.653941	936719.238343	45.960039
3494.218736	933178.001864	45.965044
3493.334044	929562.591896	45.970049
3493.141859	925851.145758	45.975053
3492.637846	922058.759343	45.980058
3491.776812	918190.587833	45.985063
3491.443976	914226.492952	45.990068
3490.839702	910178.092858	45.995073
3490.249530	906064.001807	46.000077
3489.324362	901867.255397	46.005082
3489.138439	897543.731246	46.010087
3488.519362	893172.011106	46.015092
3487.651305	888715.003352	46.020097
3486.892708	884149.715635	46.025101
3486.011630	879515.140482	46.030106
3485.626176	874792.125762	46.035111
3484.648503	870008.357239	46.040116
3483.889298	865113.733261	46.045121
3483.238290	860137.228507	46.050125
3482.241849	855091.418372	46.055130
3481.635949	849927.339116	46.060135
3480.773315	844714.968280	46.065140
3479.939485	839402.949770	46.070145
3479.057357	834000.721301	46.075149
3477.888837	828534.155173	46.080154
3477.679727	822953.626914	46.085159
3476.600730	817318.112795	46.090164
3475.635602	811587.923032	46.095169
3474.853634	805775.229211	46.100173
3473.615863	799843.274000	46.105178
3472.661792	793830.218057	46.110183
3471.760807	787764.975737	46.115188
3470.636936	781610.769298	46.120193
3470.273751	775364.132983	46.125197
3468.879047	769033.930945	46.130202
3467.953779	762591.807225	46.135207
3466.922068	756059.581832	46.140212
3465.839083	749455.489950	46.145217
3464.834449	742762.599116	46.150221
3463.428117	736011.651525	46.155226
3462.402521	729153.263531	46.160231
3461.390579	722207.211043	46.165236
3460.034038	715174.081022	46.170241
3458.838540	708050.548883	46.175245
3457.483615	700849.130295	46.180250
3456.537693	693550.246286	46.185255
3455.303962	686190.539559	46.190260
3453.969426	678717.669884	46.195265
3452.995149	671173.856293	46.200269
3451.141775	663565.897988	46.205274
3450.062740	655858.479127	46.210279
3448.806721	648061.054481	46.215284
3447.337546	640184.764338	46.220289
3445.914435	632201.183442	46.225293
3444.374390	624155.086667	46.230298
3443.019804	616024.015486	46.235303
3441.357092	607846.855672	46.240308
3439.482246	599562.678129	46.245313
3438.442595	591205.612108	46.250317
3436.425218	582781.445242	46.255322
3434.669826	574246.065805	46.260327
3433.050710	565648.081932	46.265332
3431.488870	556980.348296	46.270337
3429.855258	548238.538769	46.275341
3428.231885	539396.542649	46.280346
3426.365509	530508.163862	46.285351
3424.545478	521529.156084	46.290356
3422.391799	512481.446518	46.295361
3420.663667	503347.184863	46.300365
3419.112656	494148.729348	46.305370
3416.775365	484875.806771	46.310375
3415.051063	475526.604167	46.315380
3412.859225	466119.738846	46.320385
3410.679302	456652.827417	46.325389
3408.521073	447086.133444	46.330394
3406.168267	437458.142933	46.335399
3404.235613	427789.461358	46.340404
3401.658614	418048.728088	46.345409
3399.661568	408229.946269	46.350413
3397.190304	398361.976745	46.355418
3394.905403	388410.661780	46.360423
3392.268901	378430.386540	46.365428
3389.771072	368379.098354	46.370433
3387.594812	358253.780165	46.375437
3385.034659	348104.697363	46.380442
3382.408837	337880.044487	46.385447
3379.602300	327624.857799	46.390452
3376.467736	317298.905636	46.395457
3373.925970	306929.594441	46.400461
3371.027590	296526.020681	46.405466
3368.045508	286071.061944	46.410471
3365.055649	275569.863382	46.415476
3362.001100	265035.241032	46.420481
3358.701155	254453.195065	46.425485
3355.349584	243841.607191	46.430490
3351.772082	233207.243875	46.435495
3348.519809	222471.451898	46.440500
3344.412647	211738.494339	46.445505
3340.914142	201031.979452	46.450509
3336.966219	190318.544592	46.455514
3333.498405	179566.634693	46.460519
3329.329720	168815.914912	46.465524
3325.336118	158060.747118	46.470529
3321.491322	147285.909960	46.475533
3316.502749	136525.649269	46.480538
3311.708739	125763.904178	46.485543
3306.756098	115016.513968	46.490548
3301.417108	104297.362585	46.495553
3295.885201	93618.615242	46.500557
3289.580899	82971.108587	46.505562
3282.732301	72377.989619	46.510567
3270.010565	62036.805968	46.515572
3244.438969	52113.901231	46.520577
3218.318093	42490.262514	46.525581
3189.637393	33376.922071	46.530586
3150.723022	25022.608468	46.535591
3104.088177	17538.135457	46.540596
3056.863140	10881.511950	46.545601
3013.840309	5094.505201	46.550605
2950.338244	880.706159	46.555610
2796.692661	346.919104	46.560615
2699.301382	353.511630	46.565620
2682.784355	375.726114	46.570625
2722.560292	359.715055	46.575629
2783.925869	331.900310	46.580634
2840.250355	320.116300	46.585639
2876.963122	329.407830	46.590644
2891.841333	333.805097	46.595649
2891.566703	320.708156	46.600653
2882.813554	329.177146	46.605658
2873.299055	335.968026	46.610663
2866.020043	320.234926	46.615668
2860.354379	320.088342	46.620673
2857.364234	321.187025	46.625677
2854.941012	326.286450	46.630682
2853.482095	324.580614	46.635687
2852.062201	315.840278	46.640692
2849.948620	321.369973	46.645697
2848.180091	302.804896	46.650701
2844.751093	295.901883	46.655706
2841.874443	321.532625	46.660711
2838.678400	315.306911	46.665716
2835.479055	306.056628	46.670721
2832.879072	302.823083	46.675725
2829.361411	302.854333	46.680730
2826.045260	309.261194	46.685735
2823.298667	296.571117	46.690740
2819.752841	295.425084	46.695745
2816.857283	297.881402	46.700749
2813.834438	305.927130	46.705754
2810.623881	291.831526	46.710759
2807.529899	291.520861	46.715764
2803.802661	295.238316	46.720769
2801.129523	293.297426	46.725773
2797.692677	292.754935	46.730778
2793.972019	298.470855	46.735783
2790.665103	294.331263	46.740788
2787.532043	276.687873	46.745793
2784.534376	271.370919	46.750797
2780.569426	296.280764	46.755802
2777.151739	307.000802	46.760807
2774.601992	290.967000	46.765812
2771.055734	264.766955	46.770817
2767.776028	269.786020	46.775821
2764.294188	293.330113	46.780826
2760.761468	272.531305	46.785831
2757.616774	267.587037	46.790836
2754.101256	285.121676	46.795841
2750.757059	255.745943	46.800845
2747.162173	272.284168	46.805850
2743.838142	257.126630	46.810855
2740.597842	277.729188	46.815860
2736.667617	286.506762	46.820865
2733.853162	256.352854	46.825869
2730.209540	260.236980	46.830874
2727.225031	288.069672	46.835879
2723.771944	290.326627	46.840884
2719.898376	280.739409	46.845889
2717.049714	274.016420	46.850893
2713.196372	280.762152	46.855898
2709.752688	273.533430	46.860903
2706.683875	269.749821	46.865908
2702.590590	269.395805	46.870913
2699.334285	267.571821	46.875917
2696.220848	257.416566	46.880922
2692.760897	265.739077	46.885927
2689.192274	273.805756	46.890932
2685.324927	263.562311	46.895937
2682.288581	247.897283	46.900941
2679.043608	259.256311	46.905946
2675.726190	264.091329	46.910951
2672.212676	262.482699	46.915956
2668.673364	254.032507	46.920961
2665.053463	252.636453	46.925965
2661.525366	259.161657	46.930970
2658.076746	246.331358	46.935975
2654.814239	252.390353	46.940980
2650.732270	268.593497	46.945985
2647.617368	248.579133	46.950989
2644.366298	252.490906	46.955994
2640.591082	259.205036	46.960999
2637.184279	258.054321	46.966004
2633.260813	263.558985	46.971009
2629.986425	254.399146	46.976013
2627.203606	240.461740	46.981018
2623.438251	248.632292	46.986023
2620.373356	253.750249	46.991028
2617.117328	263.046477	46.996033
2613.276955	259.535342	47.001037
2610.014912	250.504586	47.006042
2606.426862	231.713907	47.011047
2602.871068	249.616838	47.016052
2598.891299	244.865389	47.021057
2596.075395	234.770051	47.026061
2592.531470	245.677050	47.031066
2588.538861	249.694639	47.036071
2585.697407	238.531193	47.041076
2581.568111	247.534888	47.046081
2577.889619	234.898613	47.051085
2574.608864	234.897724	47.056090
2571.448078	241.120402	47.061095
2568.435129	237.571908	47.066100
2564.272300	241.827994	47.071105
2561.486143	249.806924	47.076109
2557.453286	240.319689	47.081114
2554.033895	240.509571	47.086119
2550.360930	252.302137	47.091124
2546.894108	248.346585	47.096129
2543.827753	239.740154	47.101133
2540.133224	247.012001	47.106138
2536.929619	236.062387	47.111143
2533.442177	220.967174	47.116148
2529.795982	231.512925	47.121153
2526.521726	245.848541	47.126157
2522.458147	233.518084	47.131162
2518.916963	214.266461	47.136167
2515.902162	222.084610	47.141172
2512.282054	219.527267	47.146177
2508.797271	217.938644	47.151181
2505.195163	236.733816	47.156186
2501.809815	246.936382	47.161191
2498.494965	220.125301	47.166196
2494.598039	211.641074	47.171201
2491.221041	213.610142	47.176205
2487.615309	224.236931	47.181210
2484.498244	228.030775	47.186215
2480.878669	207.125428	47.191220
2477.512837	224.931439	47.196225
2473.969816	226.424089	47.201229
2470.767762	221.553646	47.206234
2466.999043	215.504864	47.211239
2463.689154	226.957801	47.216244
2459.656237	217.421623	47.221249
2456.813741	216.943064	47.226253
2452.888426	239.672326	47.231258
2449.452015	224.251882	47.236263
2445.997528	227.818159	47.241268
2442.528091	223.049633	47.246273
2439.061893	223.346822	47.251277
2435.281135	238.366759	47.256282
2432.165262	224.592411	47.261287
2428.848462	222.192946	47.266292
2425.134719	221.529769	47.271297
2421.819856	202.626132	47.276301
2418.121587	212.800008	47.281306
2414.530167	229.033576	47.286311
2411.011272	217.217809	47.291316
2407.728957	210.395343	47.296321
2404.150494	206.164112	47.301325
2400.643704	226.394613	47.306330
2396.931592	222.730460	47.311335
2393.473956	192.155012	47.316340
2390.118382	204.473541	47.321345
2386.972419	220.196333	47.326349
2383.196135	219.263820	47.331354
2380.093867	214.916384	47.336359
2376.711061	206.150048	47.341364
2372.551699	218.864937	47.346369
2369.283318	218.491766	47.351373
2365.556145	219.011964	47.356378
2361.701575	224.730988	47.361383
2358.497471	215.357790	47.366388
2355.320303	214.119816	47.371393
2351.629606	206.959379	47.376397
2348.172583	196.672786	47.381402
2344.605401	201.871391	47.386407
2341.204012	212.852808	47.391412
2337.562120	220.787650	47.396417
2334.275802	207.911176	47.401421
2330.858806	193.601883	47.406426
2327.077278	211.391533	47.411431
2324.009808	222.545377	47.416436
2320.197767	216.689776	47.421441
2316.737532	189.423425	47.426445
2313.654019	204.153472	47.431450
2309.891401	226.008226	47.436455
2306.677387	210.474261	47.441460
2302.999453	195.949359	47.446465
2299.060824	194.546769	47.451469
2295.614110	202.750998	47.456474
2292.054589	220.345823	47.461479
2288.847274	210.696581	47.466484
2285.207875	212.680306	47.471489
2281.771201	213.055562	47.476493
2278.150092	206.458421	47.481498
2274.916744	204.028301	47.486503
2271.498488	209.576059	47.491508
2267.897913	200.148352	47.496513
2264.419398	205.455482	47.501517
2261.074697	215.557785	47.506522
2257.095462	212.375572	47.511527
2253.951006	199.082146	47.516532
2250.111791	215.791956	47.521537
2246.530766	213.392060	47.526541
2243.069128	196.883494	47.531546
2239.968455	207.276324	47.536551
2236.452435	207.984410	47.541556
2232.672209	204.138133	47.546561
2229.471315	186.961045	47.551565
2225.956252	200.224054	47.556570
2222.403460	225.237593	47.561575
2219.006969	206.341332	47.566580
2215.285877	198.480254	47.571585
2211.857833	182.441868	47.576589
2208.531430	191.632403	47.581594
2205.027486	204.450851	47.586599
2201.345659	206.311691	47.591604
2197.701994	215.371281	47.596609
2194.598288	207.010922	47.601613
2191.045940	195.075734	47.606618
2187.293653	187.519914	47.611623
2184.095374	195.253786	47.616628
2180.231298	206.712182	47.621633
2177.037317	195.871595	47.626637
2173.406675	207.179327	47.631642
2169.725997	213.463028	47.636647
2166.421178	207.256517	47.641652
2163.176869	208.943601	47.646657
2159.372450	188.334857	47.651661
2155.690293	192.918190	47.656666
2151.949596	210.991682	47.661671
2148.869172	212.519946	47.666676
2145.535006	213.281140	47.671681
2141.950452	183.872061	47.676685
2138.333262	187.876466	47.681690
2134.644491	214.426798	47.686695
2131.533289	197.169165	47.691700
2127.818018	190.686691	47.696705
2124.302635	186.883505	47.701709
2120.845055	194.983442	47.706714
2117.409804	202.718844	47.711719
2114.205659	177.535130	47.716724
2110.601008	172.209039	47.721729
2107.055189	189.669335	47.726733
2103.651086	206.848208	47.731738
2099.753842	189.703984	47.736743
2096.485810	187.055243	47.741748
2092.807680	199.368568	47.746753
2089.351506	208.773222	47.751757
2085.675612	200.887203	47.756762
2082.045755	184.752957	47.761767
2079.162878	190.205469	47.766772
2075.299417	189.121866	47.771777
2071.941394	207.785707	47.776781
2068.615974	190.894325	47.781786
2064.919881	192.208699	47.786791
2061.334293	189.949341	47.791796
2057.895511	188.170852	47.796801
2054.131551	204.660253	47.801805
2051.032711	199.163838	47.806810
2047.325483	195.631461	47.811815
2044.028861	169.280264	47.816820
2040.332706	197.116902	47.821825
2037.116347	210.163990	47.826829
2033.186831	193.817877	47.831834
2029.829117	183.299152	47.836839
2026.838104	174.395101	47.841844
2022.956819	184.948222	47.846849
2019.161596	194.647850	47.851853
2015.963529	181.890695	47.856858
2012.012428	200.812091	47.861863
2008.987017	188.294383	47.866868
2005.392318	178.172273	47.871873
2001.954966	184.006207	47.876877
1998.236608	198.905179	47.881882
1994.769101	191.192498	47.886887
1991.885076	167.204283	47.891892
1987.991643	187.902291	47.896897
1984.447224	189.835072	47.901901
1980.866152	189.910127	47.906906
1977.010727	197.736795	47.911911
1974.039682	190.196937	47.916916
1970.302837	187.719213	47.921921
1967.113380	199.415417	47.926925
1963.570470	188.328381	47.931930
1959.651378	195.734858	47.936935
1956.176044	181.929956	47.941940
1952.746779	186.034841	47.946945
1949.343321	175.694672	47.951949
1945.988357	173.546290	47.956954
1942.559678	194.426898	47.961959
1938.730883	182.822675	47.966964
1935.252937	176.769747	47.971969
1931.964354	183.220776	47.976973
1928.393963	193.815580	47.981978
1924.793208	201.690424	47.986983
1921.631862	175.600506	47.991988
1918.033395	171.069103	47.996993
1914.296400	184.005788	48.001997
1911.171140	191.407000	48.007002
1907.414118	181.179143	48.012007
1903.854864	173.906440	48.017012
1900.206801	179.995063	48.022017
1896.674155	193.378567	48.027021
1893.201025	178.867807	48.032026
1889.646664	177.020574	48.037031
1886.415223	179.400433	48.042036
1882.941387	187.458550	48.047041
1879.416543	174.071659	48.052045
1875.955971	184.424327	48.057050
1871.946020	190.189125	48.062055
1869.141456	170.485213	48.067060
1865.423467	180.450441	48.072065
1861.908550	184.250466	48.077069
1858.548856	192.007432	48.082074
1854.553557	181.193783	48.087079
1851.496611	159.848588	48.092084
1847.695100	172.558288	48.097089
1844.065090	182.092122	48.102093
1840.679902	174.355005	48.107098
1837.318225	186.876637	48.112103
1834.386147	182.372551	48.117108
1830.352984	181.750147	48.122113
1826.548030	185.257209	48.127117
1823.626183	174.043829	48.132122
1819.465273	173.033512	48.137127
1816.448139	167.138026	48.142132
1812.949707	173.437176	48.147137
1809.313566	177.455310	48.152141
1805.950584	166.652698	48.157146
1802.069794	182.508286	48.162151
1798.871094	183.458886	48.167156
1795.323681	173.440479	48.172161
1791.668109	167.164794	48.177165
1788.447521	182.361591	48.182170
1784.862017	178.364077	48.187175
1781.366447	177.533144	48.192180
1777.468066	180.509132	48.197185
1774.534266	181.867944	48.202189
1771.024590	179.847274	48.207194
1767.224357	159.223275	48.212199
1764.052199	164.595076	48.217204
1760.023889	181.154114	48.222209
1756.657452	175.777963	48.227213
1753.371951	160.233886	48.232218
1749.703482	170.219790	48.237223
1745.894765	185.262187	48.242228
1742.923802	193.163008	48.247233
1739.318913	182.603751	48.252237
1736.024620	162.595216	48.257242
1732.186221	175.593382	48.262247
1728.832148	193.062996	48.267252
1725.355500	190.671009	48.272257
1721.758314	176.346857	48.277261
1718.425713	159.153675	48.282266
1714.548333	181.147521	48.287271
1711.007586	174.104487	48.292276
1707.472919	171.539489	48.297281
1704.109994	167.880949	48.302285
1701.119237	170.245734	48.307290
1697.807087	170.688512	48.312295
1693.896878	173.056155	48.317300
1690.112887	178.278477	48.322305
1686.651385	178.645974	48.327309
1683.221174	157.296489	48.332314
1679.381688	166.374564	48.337319
1676.337048	166.445007	48.342324
1672.829890	156.834169	48.347329
1669.235734	173.635296	48.352333
1665.717894	155.552329	48.357338
1662.227967	173.257930	48.362343
1658.870955	160.057761	48.367348
1655.541764	162.464006	48.372353
1651.843642	167.177945	48.377357
1648.136324	157.408772	48.382362
1644.525019	176.836884	48.387367
1641.000391	153.367770	48.392372
1637.779482	174.695250	48.397377
1634.117887	184.327111	48.402381
1630.584042	174.366148	48.407386
1626.885980	167.792352	48.412391
1623.876795	156.817434	48.417396
1620.508094	180.417607	48.422401
1616.885292	167.173422	48.427405
1613.477838	154.163715	48.432410
1609.528064	163.981137	48.437415
1605.809702	148.413104	48.442420
1602.503805	149.391738	48.447425
1598.964806	169.891770	48.452429
1595.641567	171.798196	48.457434
1591.902994	160.457320	48.462439
1588.552303	173.619412	48.467444
1585.132726	166.697624	48.472449
1581.876399	181.963117	48.477453
1578.595433	159.244103	48.482458
1574.841138	174.436199	48.487463
1571.132504	158.544290	48.492468
1567.631776	157.107137	48.497473
1563.823893	162.529175	48.502477
1560.891328	175.084840	48.507482
1557.309510	167.286913	48.512487
1553.717120	144.443147	48.517492
1550.321513	154.037640	48.522497
1546.287550	165.597696	48.527501
1543.277972	165.915739	48.532506
1539.518767	161.144822	48.537511
1535.740512	143.557139	48.542516
1532.493811	154.120649	48.547521
1529.548475	162.634242	48.552525
1526.177036	162.069723	48.557530
1522.016620	178.800498	48.562535
1518.613836	180.681909	48.567540
1515.248218	157.837720	48.572545
1511.353429	155.401215	48.577549
1507.827613	156.209813	48.582554
1504.235293	158.113828	48.587559
1501.164011	159.256215	48.592564
1497.908197	158.481941	48.597569
1493.949782	175.716724	48.602573
1490.776856	152.939013	48.607578
1487.042316	164.312755	48.612583
1483.606733	167.293406	48.617588
1480.230067	178.368187	48.622593
1476.760238	166.123705	48.627597
1473.128439	146.339069	48.632602
1469.355321	179.362292	48.637607
1466.134568	162.566418	48.642612
1462.587960	140.669295	48.647617
1458.876194	166.887891	48.652621
1456.106324	168.015277	48.657626
1452.126145	171.395380	48.662631
1448.646852	159.905563	48.667636
1444.798388	149.278497	48.672641
1441.077880	153.798142	48.677645
1437.817642	145.114931	48.682650
1434.595067	159.950986	48.687655
1431.139866	153.686247	48.692660
1427.677956	163.805889	48.697665
1424.101187	167.916996	48.702669
1420.934090	158.791071	48.707674
1417.048905	147.397374	48.712679
1413.683677	146.012811	48.717684
1410.080823	162.463471	48.722689
1406.086031	164.419953	48.727693
1402.966661	149.135460	48.732698
1399.343303	145.793519	48.737703
1396.159030	145.248581	48.742708
1392.643752	150.577421	48.747713
1388.431722	159.971128	48.752717
1385.561719	148.687592	48.757722
1382.067439	156.877413	48.762727
1378.282754	150.924657	48.767732
1375.229477	162.411511	48.772737
1371.619001	157.138887	48.777741
1368.197195	153.534733	48.782746
1364.612843	165.219831	48.787751
1361.197427	170.564171	48.792756
1357.642103	149.663713	48.797761
1353.875574	156.329487	48.802765
1350.395367	152.258216	48.807770
1346.903486	177.563684	48.812775
1343.219397	155.484428	48.817780
1339.994070	160.488433	48.822785
1336.733893	154.182876	48.827789
1333.094396	145.791383	48.832794
1329.281941	152.111587	48.837799
1326.007503	171.813177	48.842804
1322.631445	166.746730	48.847809
1319.027949	151.382188	48.852813
1315.549005	145.382066	48.857818
1311.741970	176.716140	48.862823
1308.361426	162.123609	48.867828
1304.839771	144.816515	48.872833
1301.116964	147.811510	48.877837
1297.915598	166.647735	48.882842
1294.289506	174.053208	48.887847
1290.753238	159.443187	48.892852
1287.895800	148.877561	48.897857
1283.696640	158.351567	48.902861
1280.283275	174.269183	48.907866
1276.892446	157.187612	48.912871
1273.249395	140.269132	48.917876
1269.876290	142.938590	48.922881
1266.279723	154.081889	48.927885
1262.892833	153.954199	48.932890
1259.758020	166.029667	48.937895
1255.877025	146.368499	48.942900
1252.873378	153.770179	48.947905
1249.005233	162.953796	48.952909
1245.466164	145.752901	48.957914
1241.758118	158.172966	48.962919
1238.259068	150.749953	48.967924
1234.921977	146.895528	48.972929
1231.084154	153.179324	48.977933
1228.017231	153.288562	48.982938
1224.188459	151.553269	48.987943
1220.669073	147.649433	48.992948
1217.429401	151.454422	48.997953
1213.749200	156.577661	49.002957
1210.527993	169.739120	49.007962
1207.038223	158.754288	49.012967
1203.383363	145.825048	49.017972
1200.064535	146.239961	49.022977
1196.208038	156.957918	49.027981
1192.723726	152.763017	49.032986
1189.030999	153.924668	49.037991
1185.843908	152.968340	49.042996
1182.662765	140.594926	49.048001
1178.941749	154.955188	49.053005
1175.642049	147.256928	49.058010
1171.908161	141.958631	49.063015
1168.295918	157.825839	49.068020
1164.592773	165.256120	49.073025
1160.566721	158.365838	49.078029
1158.044464	143.917419	49.083034
1154.120900	152.671735	49.088039
1150.782455	150.371673	49.093044
1147.920676	139.673966	49.098049
1143.812782	166.228822	49.103053
1140.491074	148.428442	49.108058
1136.986599	137.386219	49.113063
1133.078648	140.388187	49.118068
1129.446053	158.073589	49.123073
1125.814573	156.746244	49.128077
1122.966320	136.533230	49.133082
1119.286004	148.573701	49.138087
1115.532808	150.868181	49.143092
1112.123292	143.659920	49.148097
1108.616639	146.735140	49.153101
1105.411606	158.282446	49.158106
1101.767415	152.777214	49.163111
1098.339153	160.876056	49.168116
1094.924577	155.731062	49.173121
1091.620031	162.651952	49.178125
1088.136481	138.969044	49.183130
1084.148193	146.991259	49.188135
1080.308994	156.604814	49.193140
1077.110265	141.943866	49.198145
1073.516140	132.480052	49.203149
1070.187209	152.533284	49.208154
1066.857542	157.728839	49.213159
1063.166944	144.861922	49.218164
1059.810937	132.976465	49.223169
1056.132173	151.079880	49.228173
1052.663591	131.970407	49.233178
1049.073691	135.333441	49.238183
1045.669121	142.978947	49.243188
1042.530043	138.165930	49.248193
1038.661627	135.428029	49.253197
1035.292085	124.679867	49.258202
1031.903226	133.658664	49.263207
1028.448748	138.076285	49.268212
1024.545441	135.588207	49.273217
1020.916115	129.044188	49.278221
1017.803633	143.709078	49.283226
1014.015918	145.117734	49.288231
1010.742846	145.669111	49.293236
1007.279119	151.237812	49.298241
1003.446932	155.006068	49.303245
1000.160964	135.405991	49.308250
996.603103	127.658626	49.313255
993.113982	141.931534	49.318260
989.770664	140.307012	49.323265
986.024687	133.988741	49.328269
982.845702	145.005100	49.333274
979.208993	131.681791	49.338279
975.457673	143.756335	49.343284
972.330438	141.042195	49.348289
968.377565	148.983156	49.353293
964.992661	128.871191	49.358298
961.757665	126.741679	49.363303
958.029132	136.002394	49.368308
954.597475	152.189857	49.373313
951.108423	146.906214	49.378317
947.835109	127.121598	49.383322
944.049240	142.626008	49.388327
940.436472	146.586237	49.393332
937.216229	148.315360	49.398337
933.524528	135.465886	49.403341
930.249864	129.785124	49.408346
926.456728	144.511428	49.413351
923.028897	138.818075	49.418356
919.920447	140.679973	49.423361
916.125626	155.888955	49.428365
912.633897	139.127458	49.433370
909.063305	123.824187	49.438375
905.377240	141.057102	49.443380
902.204339	144.258134	49.448385
898.449991	144.468499	49.453389
895.345300	121.712939	49.458394
891.619601	129.134231	49.463399
887.848839	143.965664	49.468404
884.581337	136.269658	49.473409
880.835867	127.612542	49.478413
877.530656	120.438306	49.483418
873.984781	133.606303	49.488423
870.609841	154.285313	49.493428
867.065283	143.522932	49.498433
863.178579	121.073795	49.503437
859.960462	135.852744	49.508442
856.495234	159.750542	49.513447
852.838152	151.910236	49.518452
849.825809	130.706558	49.523457
846.302751	135.183431	49.528461
842.660809	139.064576	49.533466
838.906079	153.020164	49.538471
835.050758	144.299034	49.543476
831.734839	133.322943	49.548481
828.193392	137.654496	49.553485
825.154370	122.706827	49.558490
822.132364	122.165750	49.563495
818.426163	136.415869	49.568500
814.838401	142.989439	49.573505
810.847572	136.490641	49.578509
807.455906	114.088055	49.583514
803.818024	126.678101	49.588519
800.200344	131.714463	49.593524
797.077689	123.915282	49.598529
793.406756	136.702667	49.603533
790.198788	131.148284	49.608538
786.446904	133.193242	49.613543
782.643575	134.071513	49.618548
779.436134	128.339781	49.623553
775.887294	129.601298	49.628557
772.679836	134.189152	49.633562
769.036884	144.011630	49.638567
765.561972	128.687523	49.643572
762.290895	140.944857	49.648577
758.774364	134.999999	49.653581
754.900246	112.702578	49.658586
751.503529	146.758102	49.663591
747.533614	130.976644	49.668596
744.302745	138.791871	49.673601
740.797364	150.338293	49.678605
737.391425	129.987194	49.683610
733.595710	129.449734	49.688615
730.027634	140.106253	49.693620
727.077789	124.287264	49.698625
723.206196	139.964442	49.703629
720.034875	146.264887	49.708634
716.465300	143.580026	49.713639
713.007710	130.702306	49.718644
709.670677	129.269057	49.723649
705.866771	143.341028	49.728653
702.416009	146.092138	49.733658
698.803888	130.822795	49.738663
695.347866	127.807373	49.743668
691.749177	142.588764	49.748673
688.280824	136.507651	49.753677
685.294020	128.549467	49.758682
681.251895	135.345810	49.763687
677.746112	134.196238	49.768692
674.281477	131.401246	49.773697
670.886101	146.559442	49.778701
667.446622	140.639200	49.783706
663.736425	115.268949	49.788711
660.141154	118.168533	49.793716
656.881874	134.783852	49.798721
653.166519	141.453838	49.803725
649.876423	125.140935	49.808730
646.533072	130.630824	49.813735
642.717497	137.550863	49.818740
639.171114	127.297568	49.823745
635.827601	146.488386	49.828749
632.247420	131.247553	49.833754
628.989082	122.227035	49.838759
625.137978	120.263967	49.843764
621.687248	130.364308	49.848769
618.064183	142.885805	49.853773
614.615064	128.004810	49.858778
611.431409	123.628401	49.863783
607.658823	127.472841	49.868788
604.442521	144.074282	49.873793
600.752101	135.657338	49.878797
597.353592	126.974277	49.883802
593.929487	131.541565	49.888807
590.673813	130.795629	49.893812
586.897405	139.033366	49.898817
582.867515	129.644801	49.903821
580.044088	114.818335	49.908826
576.351045	127.345772	49.913831
572.752568	135.608481	49.918836
569.479339	137.554572	49.923841
565.447658	122.044092	49.928845
562.349680	128.917458	49.933850
558.641118	133.972698	49.938855
555.283417	124.468002	49.943860
552.041782	120.854963	49.948865
547.825069	143.800211	49.953869
544.734910	133.218589	49.958874
541.538615	112.625083	49.963879
537.558422	113.633819	49.968884
534.045728	133.133442	49.973889
530.805365	147.257223	49.978893
527.341987	130.040016	49.983898
523.875882	105.690307	49.988903
520.263420	125.907217	49.993908
516.737935	132.648793	49.998913
512.886912	125.225081	50.003917
509.573765	112.664677	50.008922
506.151814	112.439090	50.013927
502.545886	126.679967	50.018932
499.425527	136.505218	50.023937
495.673591	131.983222	50.028941
492.427345	130.011374	50.033946
489.130837	121.660251	50.038951
485.072655	133.304391	50.043956
481.822948	125.829809	50.048961
477.915199	126.602292	50.053965
474.400858	134.742340	50.058970
470.979567	141.621606	50.063975
467.416762	140.789543	50.068980
464.500046	116.324649	50.073985
460.618423	114.612058	50.078989
456.988483	128.734625	50.083994
453.732546	131.664777	50.088999
449.940952	118.783204	50.094004
446.742535	130.818056	50.099009
443.232529	142.317416	50.104013
439.583570	136.346485	50.109018
436.110874	135.237845	50.114023
432.639048	115.149893	50.119028
429.218262	125.882944	50.124033
425.250367	144.687085	50.129037
422.082154	145.105518	50.134042
418.663169	136.782058	50.139047
414.985781	132.101801	50.144052
411.955043	116.897607	50.149057
407.994347	135.320394	50.154061
404.522433	131.755535	50.159066
401.000692	123.129626	50.164071
397.416450	125.452513	50.169076
394.136292	128.222867	50.174081
390.373109	127.586200	50.179085
387.306548	135.473593	50.184090
384.078362	121.403026	50.189095
380.170416	134.165937	50.194100
376.644436	141.204197	50.199105
372.637638	134.699753	50.204109
369.392246	136.398868	50.209114
366.147260	131.014662	50.214119
362.596481	119.260779	50.219124
359.343928	125.858198	50.224129
355.801905	124.091344	50.229133
351.711506	143.557275	50.234138
348.354715	131.927477	50.239143
344.440827	110.449032	50.244148
341.439640	121.644281	50.249153
338.151737	125.134655	50.254157
334.824261	137.486592	50.259162
331.359934	124.515250	50.264167
327.402986	118.637894	50.269172
324.187026	133.833641	50.274177
320.126255	131.944757	50.279181
317.092718	122.574084	50.284186
313.459426	138.370885	50.289191
309.964399	128.104982	50.294196
306.690337	115.379329	50.299201
302.842667	134.341505	50.304205
299.377188	143.454507	50.309210
295.811100	122.294569	50.314215
292.415516	119.928350	50.319220
288.935764	120.439946	50.324225
285.493110	138.899993	50.329229
281.796665	135.927876	50.334234
279.007481	124.559013	50.339239
274.944957	119.440070	50.344244
271.788672	137.186252	50.349249
267.947941	131.789968	50.354253
264.343747	116.593235	50.359258
261.237531	127.057041	50.364263
257.032052	138.491645	50.369268
253.922719	120.299430	50.374273
250.149132	120.915428	50.379277
246.969414	123.533693	50.384282
243.796843	133.639239	50.389287
240.000750	134.958069	50.394292
236.351967	122.343494	50.399297
232.593699	125.600600	50.404301
229.421524	127.998335	50.409306
226.167242	130.181272	50.414311
222.620890	132.289652	50.419316
219.145421	134.705345	50.424321
215.676354	126.730525	50.429325
211.886074	111.079142	50.434330
208.282937	119.583874	50.439335
204.528370	132.561211	50.444340
201.294018	130.207860	50.449345
197.755106	126.463607	50.454349
194.492057	120.469718	50.459354
191.079411	116.807102	50.464359
187.134378	109.484976	50.469364
183.928982	122.902097	50.474369
180.586161	126.930958	50.479373
176.766592	121.042448	50.484378
173.273518	114.792515	50.489383
169.878390	122.313722	50.494388
166.566564	122.632504	50.499393
163.134908	125.609584	50.504397
159.203434	120.143435	50.509402
155.955683	114.149806	50.514407
152.132516	122.225805	50.519412
148.858518	136.389299	50.524417
145.027796	131.223558	50.529421
141.937415	123.707166	50.534426
138.341871	108.891852	50.539431
134.754207	128.273383	50.544436
131.777422	136.841180	50.549441
127.868911	121.016138	50.554445
124.090157	120.278846	50.559450
121.190366	123.362890	50.564455
117.377294	128.194240	50.569460
113.739908	121.006484	50.574465
110.494765	108.228047	50.579469
106.643459	102.974693	50.584474
103.320800	120.940069	50.589479
99.760159	126.698621	50.594484
96.269649	119.609422	50.599489
92.708188	131.308995	50.604493
89.102309	120.958869	50.609498
85.740960	106.689969	50.614503
82.194198	118.497987	50.619508
78.512216	119.963880	50.624513
75.179452	116.375631	50.629517
71.474022	124.850280	50.634522
68.481490	122.861196	50.639527
64.900624	116.289059	50.644532
61.557631	106.245025	50.649537
58.076495	133.107779	50.654541
54.393954	131.107639	50.659546
50.952252	122.082555	50.664551
46.762599	103.207053	50.669556
43.720377	116.480458	50.674561
40.655971	127.995420	50.679565
37.013779	119.095022	50.684570
33.273599	112.816268	50.689575
29.587152	119.469945	50.694580
26.044238	121.480596	50.699585
22.702722	123.780738	50.704589
18.938795	119.791058	50.709594
15.730202	107.414744	50.714599
12.162439	121.329403	50.719604
8.902045	122.487435	50.724609
5.559455	126.930263	50.729613
1.575779	100.412373	50.734618