Wed Jun 15 16:52:51 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.637179	107.823046	0.000000
1.859773	90.219905	0.005005
1.301059	114.192609	0.010010
1.363274	91.471674	0.015014
1.065948	78.004873	0.020019
1.040974	73.072008	0.025024
0.796350	78.744461	0.030029
0.155011	55.477934	0.035034
0.407618	46.363088	0.040038
-0.192572	35.154659	0.045043
-0.444435	35.512970	0.050048
-0.630235	56.798109	0.055053
-1.128977	35.897939	0.060058
-1.468560	4.079853	0.065062
-1.852297	6.591981	0.070067
-1.674064	10.533141	0.075072
-2.038746	14.509867	0.080077
-2.523623	4.222102	0.085082
-2.313186	6.627060	0.090086
-3.497060	4.560212	0.095091
-3.808892	-8.628598	0.100096
-4.110378	-20.567593	0.105101
-4.635138	2.441479	0.110106
-4.438371	0.648671	0.115110
-4.954180	6.263814	0.120115
-4.540158	-15.290516	0.125120
-4.333801	-7.984384	0.130125
-4.524919	7.953608	0.135130
-5.089072	2.200162	0.140134
-5.615707	-5.473694	0.145139
-5.678395	-18.402209	0.150144
-6.188507	-9.916054	0.155149
-7.269696	10.009395	0.160154
-6.854999	-7.466857	0.165158
-7.574487	-9.987568	0.170163
-7.660865	-3.305916	0.175168
-7.274212	4.783461	0.180173
-7.593581	14.201280	0.185178
-7.475915	-12.072895	0.190182
-7.924818	-15.217370	0.195187
-8.470217	4.914082	0.200192
-8.678168	14.752362	0.205197
-9.336123	11.289969	0.210202
-9.113932	-14.982633	0.215206
-9.334183	-5.346332	0.220211
-9.671934	18.199365	0.225216
-9.726828	8.790494	0.230221
-10.650491	-1.102280	0.235226
-10.819973	-15.381358	0.240230
-11.147483	-3.197473	0.245235
-11.203626	9.402250	0.250240
-11.058334	1.614093	0.255245
-11.289922	-7.010535	0.260250
-11.388074	-19.525091	0.265254
-11.505527	9.017855	0.270259
-12.238465	9.983126	0.275264
-12.748433	2.954120	0.280269
-12.991946	14.316725	0.285274
-12.440433	-0.379725	0.290278
-13.160410	-7.870206	0.295283
-13.775827	-1.362140	0.300288
-14.458855	3.501437	0.305293
-14.412406	8.174325	0.310298
-14.132140	-6.160443	0.315302
-14.673886	2.717538	0.320307
-14.823818	0.013032	0.325312
-14.540137	-2.895515	0.330317
-14.541276	7.787315	0.335322
-15.065244	5.058110	0.340326
-15.614154	-2.662769	0.345331
-15.400042	-17.026348	0.350336
-15.699644	-9.117827	0.355341
-17.193216	-5.091168	0.360346
-17.437591	-5.821856	0.365350
-17.210842	-2.617806	0.370355
-17.574980	3.139278	0.375360
-17.259473	10.752218	0.380365
-17.539063	3.032698	0.385370
-17.462421	-8.349894	0.390374
-18.441537	10.925680	0.395379
-18.727717	25.643667	0.400384
-18.872965	4.992702	0.405389
-19.196227	-9.032800	0.410394
-19.083622	3.000919	0.415398
-19.262721	14.162000	0.420403
-19.517946	-14.824946	0.425408
-20.112437	-9.016481	0.430413
-20.722053	21.307381	0.435418
-20.815653	9.886325	0.440422
-20.793006	-10.041871	0.445427
-20.684737	2.173676	0.450432
-20.747131	5.411998	0.455437
-21.436666	13.472075	0.460442
-21.980943	3.871528	0.465446
-21.993708	9.499521	0.470451
-22.331555	-2.851042	0.475456
-22.296677	9.452991	0.480461
-22.622516	0.620406	0.485466
-22.728615	-11.975703	0.490470
-23.511713	6.317121	0.495475
-23.771411	12.213597	0.500480
-23.601075	17.868153	0.505485
-24.127083	8.374870	0.510490
-23.878398	-21.032905	0.515494
-24.385762	13.702919	0.520499
-25.267485	6.476701	0.525504
-25.182995	-6.583173	0.530509
-25.541891	-5.549011	0.535514
-25.590082	8.098685	0.540518
-25.868573	11.824418	0.545523
-25.863747	2.932943	0.550528
-25.520657	-11.794748	0.555533
-26.452154	-7.770421	0.560538
-26.732674	-3.204096	0.565542
-27.372553	17.136329	0.570547
-27.289733	5.967359	0.575552
-27.390187	-9.110419	0.580557
-27.732726	-7.310809	0.585562
-27.315893	-17.881140	0.590566
-28.666069	1.780287	0.595571
-29.046634	0.537547	0.600576
-28.943126	11.338326	0.605581
-28.957269	4.369626	0.610586
-28.723085	-14.569879	0.615590
-29.448824	4.335323	0.620595
-29.958039	-22.273411	0.625600
-30.160470	-13.415609	0.630605
-30.669043	7.534431	0.635610
-30.402183	5.489442	0.640614
-30.875946	-12.573201	0.645619
-30.566361	-1.772751	0.650624
-30.846145	8.394836	0.655629
-31.661575	11.240015	0.660634
-31.969376	-1.268611	0.665638
-32.383630	0.335400	0.670643
-32.237719	5.629591	0.675648
-31.975310	-3.403587	0.680653
-32.657902	-3.558268	0.685658
-33.224427	-5.892859	0.690662
-33.642859	4.919795	0.695667
-33.782416	-13.158720	0.700672
-33.533911	-9.749041	0.705677
-34.035684	0.913434	0.710682
-33.788400	15.432074	0.715686
-34.578826	21.279443	0.720691
-34.870264	-0.690902	0.725696
-35.354546	-15.565557	0.730701
-35.487153	2.118443	0.735706
-35.712652	11.456824	0.740710
-35.769772	15.970648	0.745715
-35.830345	-2.697218	0.750720
-35.915142	-9.243969	0.755725
-36.851922	8.937237	0.760730
-36.906912	7.033134	0.765734
-37.207983	2.856565	0.770739
-37.279483	-2.765909	0.775744
-37.107746	7.130259	0.780749
-37.767882	20.230504	0.785754
-38.176202	5.203593	0.790758
-38.729763	9.114664	0.795763
-38.782811	-4.671298	0.800768
-38.517261	-14.967155	0.805773
-38.930888	2.632189	0.810778
-38.703964	-5.007775	0.815782
-39.446189	-1.604032	0.820787
-40.099620	9.971815	0.825792
-40.153034	14.298981	0.830797
-40.452115	4.884010	0.835802
-40.244254	-6.439278	0.840806
-40.480100	-4.080521	0.845811
-41.190931	1.251285	0.850816
-41.475633	-14.305736	0.855821
-41.592203	7.500076	0.860826
-41.701044	11.210201	0.865830
-41.834088	10.408043	0.870835
-41.922617	17.500915	0.875840
-42.390113	5.955809	0.880845
-42.930117	-2.990628	0.885850
-43.016206	-0.551562	0.890854
-43.076953	8.503505	0.895859
-43.695568	10.764830	0.900864
-44.064362	3.231896	0.905869
-44.794205	-18.154689	0.910874
-44.181849	-17.928450	0.915878
-44.687821	17.339534	0.920883
-45.142474	21.143409	0.925888
-45.088434	-5.171252	0.930893
-45.263481	-2.024305	0.935898
-44.992768	7.935111	0.940902
-45.455252	-0.656980	0.945907
-46.266181	5.054583	0.950912
-46.129813	-0.111878	0.955917
-46.719758	4.058921	0.960922
-46.788304	-12.098964	0.965926
-46.719153	0.302084	0.970931
-47.716848	16.377424	0.975936
-47.933297	9.792842	0.980941
-48.222625	17.863823	0.985946
-48.179097	3.643046	0.990950
-48.570782	-1.433876	0.995955
-48.572940	-1.657802	1.000960
-48.425137	12.558846	1.005965
-48.363699	15.895571	1.010970
-49.059966	3.040879	1.015974
-49.650599	-5.777827	1.020979
-50.172467	11.462490	1.025984
-50.087593	0.356617	1.030989
-50.345347	6.242805	1.035994
-50.322024	-3.220904	1.040998
-51.036178	7.526984	1.046003
-51.549331	11.249476	1.051008
-51.690892	-20.049147	1.056013
-51.622804	-6.999042	1.061018
-51.617687	-13.458354	1.066022
-51.713162	-9.880261	1.071027
-52.001613	-14.620004	1.076032
-52.067170	-14.553695	1.081037
-52.841088	-10.604928	1.086042
-52.790753	-7.047677	1.091046
-52.948458	11.014443	1.096051
-53.967221	8.310590	1.101056
-54.302531	-15.764277	1.106061
-54.488869	-4.433531	1.111066
-54.461490	-8.552416	1.116070
-54.419971	-18.133847	1.121075
-54.468531	-5.511720	1.126080
-54.342645	7.429706	1.131085
-55.164205	8.882140	1.136090
-55.492328	-4.691745	1.141094
-55.820396	-7.492975	1.146099
-55.854888	2.327280	1.151104
-56.336590	1.513496	1.156109
-57.654558	-1.099376	1.161114
-57.047182	-10.956626	1.166118
-56.890964	-0.243683	1.171123
-57.733302	-18.364069	1.176128
-57.598667	-27.301046	1.181133
-57.840319	-0.147441	1.186138
-57.763236	0.866163	1.191142
-57.937921	5.398328	1.196147
-58.839995	9.166254	1.201152
-59.053669	14.040655	1.206157
-59.368124	-7.142231	1.211162
-60.028247	-12.124968	1.216166
-59.921176	-8.031289	1.221171
-60.294776	-12.057467	1.226176
-59.889527	3.742001	1.231181
-59.699968	0.642248	1.236186
-59.785548	10.942180	1.241190
-60.625809	7.891781	1.246195
-60.681668	-7.367965	1.251200
-60.880347	-10.525971	1.256205
-62.166352	-9.803599	1.261210
-62.553737	8.340963	1.266214
-62.727349	4.871925	1.271219
-62.331434	2.563926	1.276224
-62.603137	-5.818501	1.281229
-63.079385	-6.248666	1.286234
-63.094969	-7.197981	1.291238
-63.143578	0.074033	1.296243
-63.433080	13.553468	1.301248
-63.548860	-1.248333	1.306253
-64.284727	-16.249394	1.311258
-64.527962	-10.304649	1.316262
-64.150106	0.379161	1.321267
-64.573548	-1.850934	1.326272
-65.087290	6.657531	1.331277
-65.490459	14.572230	1.336282
-66.172024	4.448773	1.341286
-66.231479	-15.574249	1.346291
-66.442002	-12.267752	1.351296
-66.560806	-7.481936	1.356301
-66.721703	4.900510	1.361306
-66.265683	-12.838640	1.366310
-66.414900	-11.450370	1.371315
-67.291026	8.610952	1.376320
-67.502629	1.106299	1.381325
-67.456792	-6.402919	1.386330
-67.751041	-9.658572	1.391334
-68.496640	-3.183936	1.396339
-68.907741	2.717039	1.401344
-69.071080	-3.539044	1.406349
-69.422070	0.021995	1.411354
-69.010207	-26.473391	1.416358
-68.988087	-7.943055	1.421363
-69.974233	9.664302	1.426368
-70.243734	3.070145	1.431373
-70.772121	-10.573719	1.436378
-70.638507	1.491735	1.441382
-70.698663	2.323133	1.446387
-71.075574	7.499138	1.451392
-71.077262	-3.332790	1.456397
-71.657504	-10.540749	1.461402
-72.273427	-6.134138	1.466406
-72.514093	11.576110	1.471411
-72.580172	-2.555419	1.476416
-72.338202	-27.314582	1.481421
-72.542635	-13.115212	1.486426
-72.544453	11.360703	1.491430
-73.476239	1.215767	1.496435
-73.824381	-20.273050	1.501440
-73.671431	-20.910582	1.506445
-73.965845	-1.239179	1.511450
-74.525482	-3.582795	1.516454
-75.381113	-17.385445	1.521459
-75.145007	-6.774296	1.526464
-75.016499	-4.533265	1.531469
-75.641749	6.044168	1.536474
-75.609623	-7.506092	1.541478
-75.709911	-32.680500	1.546483
-76.261377	-1.117064	1.551488
-75.786171	-6.153280	1.556493
-76.578505	-8.925128	1.561498
-76.975259	-24.732321	1.566502
-77.275172	-24.487499	1.571507
-77.624736	-7.103744	1.576512
-77.229608	-12.420390	1.581517
-77.702372	-0.831796	1.586522
-78.251258	-18.808414	1.591526
-78.645967	-18.238869	1.596531
-78.625311	-3.878021	1.601536
-78.596192	-3.934783	1.606541
-78.952750	-14.888967	1.611546
-79.287656	-15.877049	1.616550
-79.783019	-7.062870	1.621555
-80.597653	-0.276447	1.626560
-80.452739	-13.962926	1.631565
-80.887038	-10.210659	1.636570
-80.810697	-12.877881	1.641574
-80.701832	-10.563864	1.646579
-81.099393	-5.663221	1.651584
-80.764227	0.385197	1.656589
-81.583896	5.551515	1.661594
-81.854696	-4.470644	1.666598
-82.245072	-24.176463	1.671603
-82.503797	-16.745341	1.676608
-82.480874	-4.224896	1.681613
-82.573989	0.910615	1.686618
-83.090163	-19.687776	1.691622
-83.621719	-20.169465	1.696627
-84.160775	-0.347739	1.701632
-83.903482	1.760932	1.706637
-84.102561	-0.110674	1.711642
-84.163623	-28.537789	1.716646
-84.317042	-10.864183	1.721651
-85.166804	-4.119503	1.726656
-85.558468	-0.477857	1.731661
-85.775490	5.689643	1.736666
-85.983951	-7.814244	1.741670
-86.018285	-10.352495	1.746675
-86.257659	-0.955012	1.751680
-86.115082	-1.214400	1.756685
-86.159275	2.888200	1.761690
-86.460337	-4.995356	1.766694
-86.688064	-15.478591	1.771699
-87.270681	-14.538157	1.776704
-87.743984	-6.557229	1.781709
-88.777039	7.926089	1.786714
-88.667723	-2.897944	1.791718
-88.457644	-17.986876	1.796723
-89.023312	-5.056449	1.801728
-88.908043	-17.560792	1.806733
-89.199864	-13.906156	1.811738
-88.926895	-5.560174	1.816742
-89.312075	1.355522	1.821747
-89.884868	-5.552898	1.826752
-90.192514	-24.514497	1.831757
-90.473015	-16.943547	1.836762
-90.744701	-1.665317	1.841766
-90.410222	1.565018	1.846771
-91.015270	-6.571532	1.851776
-91.340922	3.028329	1.856781
-92.110722	3.246051	1.861786
-92.090866	-16.929457	1.866790
-92.059727	-13.029697	1.871795
-92.643851	-12.009998	1.876800
-92.034579	-17.907740	1.881805
-92.844643	-15.721212	1.886810
-93.361879	-5.620142	1.891814
-93.429792	3.466682	1.896819
-93.710300	-9.050481	1.901824
-93.593560	-22.192706	1.906829
-94.217139	4.786878	1.911834
-94.845365	4.342079	1.916838
-95.106542	-14.482498	1.921843
-95.606816	-6.454498	1.926848
-95.492061	1.919904	1.931853
-95.675511	-12.439912	1.936858
-95.508886	-18.828747	1.941862
-95.632088	-14.690701	1.946867
-95.708415	0.763088	1.951872
-95.823274	-1.037503	1.956877
-96.821279	2.860216	1.961882
-96.868558	-4.633907	1.966886
-97.186395	4.951149	1.971891
-97.477480	8.468453	1.976896
-97.363835	-13.390159	1.981901
-98.101074	-23.212892	1.986906
-98.846799	-0.066109	1.991910
-98.691256	-15.200581	1.996915
-98.841665	-2.010833	2.006912
-97.924695	-6.747979	2.016909
-97.895152	-3.546960	2.026906
-97.291576	-16.590059	2.036902
-97.214079	-4.243711	2.046899
-96.428612	-19.662101	2.056896
-96.153927	1.958308	2.066893
-95.348081	-12.694421	2.076890
-94.555726	-8.819032	2.086886
-94.369883	-9.482898	2.096883
-94.112751	-11.750644	2.106880
-93.430478	-22.900355	2.116877
-93.046402	-17.464066	2.126874
-92.307716	-9.907383	2.136870
-91.550465	-15.455613	2.146867
-91.570884	-12.607644	2.156864
-91.335867	0.425114	2.166861
-90.509376	-17.353391	2.176858
-90.274347	-9.769075	2.186854
-88.866170	-1.650106	2.196851
-88.515705	-19.090758	2.206848
-88.554090	-7.876441	2.216845
-88.225202	-15.952354	2.226842
-87.288472	-19.543357	2.236838
-87.018473	5.686845	2.246835
-86.188099	-12.191276	2.256832
-85.394482	3.898100	2.266829
-85.207657	-8.145009	2.276826
-85.598043	-2.386136	2.286822
-84.311429	-23.493820	2.296819
-83.685858	-10.029587	2.306816
-83.725791	0.653405	2.316813
-82.403441	-16.097355	2.326810
-82.113189	-2.685357	2.336806
-82.090264	-14.700089	2.346803
-81.757263	-11.731457	2.356800
-80.640910	-12.268303	2.366797
-80.684226	8.012195	2.376794
-79.593278	-13.782815	2.386790
-79.347193	1.041313	2.396787
-79.159493	3.342561	2.406784
-78.072034	2.506669	2.416781
-77.467504	-16.029080	2.426778
-77.553455	8.768571	2.436774
-77.058519	-11.814782	2.446771
-76.088900	-2.505926	2.456768
-75.924405	-8.505263	2.466765
-75.611966	1.988325	2.476762
-74.717192	-6.000762	2.486758
-74.258093	-1.993742	2.496755
-74.332977	5.074557	2.506752
-73.128463	-9.119093	2.516749
-72.997497	-11.291810	2.526746
-71.845983	2.098848	2.536742
-71.486274	-2.450884	2.546739
-71.352920	-9.518721	2.556736
-71.291802	13.922502	2.566733
-70.526097	-0.136902	2.576730
-70.268709	4.294691	2.586726
-68.986699	8.556255	2.596723
-68.486689	-2.100702	2.606720
-68.518827	5.397499	2.616717
-68.148915	8.411002	2.626714
-67.061746	-9.135418	2.636710
-66.683444	13.130252	2.646707
-66.550627	-5.582382	2.656704
-65.585067	-6.329775	2.666701
-65.235226	-0.381713	2.676698
-65.217637	-10.062286	2.686694
-64.177158	7.046812	2.696691
-63.948396	17.790701	2.706688
-63.565061	3.039773	2.716685
-62.385745	-2.904061	2.726682
-62.229055	10.294851	2.736678
-61.967415	2.229546	2.746675
-61.348767	-0.215981	2.756672
-60.678514	9.281630	2.766669
-60.372470	-0.216188	2.776666
-60.081897	15.963260	2.786662
-59.226357	-0.532281	2.796659
-58.973555	-5.108198	2.806656
-57.860220	6.827749	2.816653
-57.563532	5.119722	2.826650
-57.338418	6.702446	2.836646
-57.337918	6.615024	2.846643
-56.424449	-6.218939	2.856640
-56.041217	9.573808	2.866637
-54.749003	-6.893443	2.876634
-54.257109	8.553819	2.886630
-54.241648	12.328268	2.896627
-54.278879	7.401144	2.906624
-53.283102	5.724749	2.916621
-52.725335	1.279379	2.926618
-52.572127	8.580719	2.936614
-51.517528	17.519872	2.946611
-51.173170	0.496426	2.956608
-51.002138	2.528116	2.966605
-50.313337	12.754663	2.976602
-49.563884	-0.830420	2.986598
-49.415632	8.231158	2.996595
-48.774090	2.170755	3.006592
-48.071413	15.678873	3.016589
-47.780157	-5.261770	3.026586
-47.540660	7.471675	3.036582
-46.431629	-5.281811	3.046579
-46.120960	13.411413	3.056576
-46.348907	7.209847	3.066573
-44.891272	10.315309	3.076570
-44.411469	2.254939	3.086566
-44.437690	-3.694806	3.096563
-44.140547	-3.178768	3.106560
-43.226784	5.702959	3.116557
-42.987344	7.985188	3.126554
-42.278720	2.610237	3.136550
-41.706696	-4.841923	3.146547
-41.205289	8.078772	3.156544
-40.418317	5.795168	3.166541
-40.239619	-2.174052	3.176538
-39.962612	-7.898436	3.186534
-39.313309	-0.410329	3.196531
-38.306916	6.575084	3.206528
-38.323384	-6.799952	3.216525
-38.184747	0.221998	3.226522
-37.130731	-6.759857	3.236518
-36.674404	-8.946047	3.246515
-36.437109	7.787323	3.256512
-35.635683	4.094328	3.266509
-35.134440	3.546052	3.276506
-34.921059	-9.973641	3.286502
-34.262035	-0.242456	3.296499
-33.742019	-2.057321	3.306496
-33.376534	7.461327	3.316493
-32.335409	5.672249	3.326490
-31.550134	-9.003360	3.336486
-31.772227	12.976928	3.346483
-31.538023	-4.274746	3.356480
-31.059501	0.530207	3.366477
-30.193622	1.835767	3.376474
-29.903207	-10.113347	3.386470
-28.881300	-7.688218	3.396467
-28.390371	-5.685592	3.406464
-28.187505	-17.326287	3.416461
-28.007729	-1.333787	3.426458
-27.291242	2.890670	3.436454
-26.814106	-9.366457	3.446451
-26.331786	1.853482	3.456448
-25.332376	-6.037332	3.466445
-25.415835	-10.622569	3.476442
-24.747269	-18.169300	3.486438
-23.872511	2.978703	3.496435
-23.800387	-20.912070	3.506432
-23.433826	4.271870	3.516429
-22.399581	-9.378742	3.526426
-21.660589	-1.492491	3.536422
-21.723648	-9.817039	3.546419
-21.639987	-0.037386	3.556416
-20.968504	-1.431426	3.566413
-20.237720	-4.436355	3.576410
-19.578296	2.217834	3.586406
-18.593614	5.834478	3.596403
-18.534019	-8.662237	3.606400
-18.285205	-8.381979	3.616397
-18.280967	5.369472	3.626394
-17.569321	-14.019005	3.636390
-16.880871	-6.249151	3.646387
-16.146914	-7.321346	3.656384
-15.638301	3.750538	3.666381
-15.221182	5.109916	3.676378
-14.304021	-8.500407	3.686374
-14.139521	0.607871	3.696371
-14.066776	-1.200834	3.706368
-13.040705	6.251882	3.716365
-12.700226	-0.623412	3.726362
-12.205697	4.628705	3.736358
-11.358894	7.488235	3.746355
-10.944839	-1.839768	3.756352
-11.054463	8.909573	3.766349
-10.259852	-12.089461	3.776346
-9.636522	4.234612	3.786342
-9.429751	-7.854569	3.796339
-8.505032	-9.530078	3.806336
-7.929448	4.652419	3.816333
-7.846951	-5.215593	3.826330
-7.266719	0.649461	3.836326
-6.216188	-3.637719	3.846323
-6.106928	-7.693883	3.856320
-5.972535	15.391327	3.866317
-5.241606	14.502854	3.876314
-4.379752	-2.190978	3.886310
-4.466052	-1.528800	3.896307
-3.687419	9.400288	3.906304
-3.355015	23.740233	3.916301
-2.989910	9.637187	3.926298
-2.377000	36.674326	3.936294
-1.919128	42.199792	3.946291
-1.422742	39.889834	3.956288
-1.117077	60.539835	3.966285
-0.717186	81.662821	3.976282
-0.045490	100.855057	3.986278
0.000000	101.991166	3.991283
0.687898	110.625258	3.996288
0.585713	110.916517	4.001293
0.845608	112.154227	4.006298
0.844440	112.982493	4.011302
0.749853	119.323055	4.016307
0.727414	144.396460	4.021312
1.019111	149.500589	4.026317
1.530940	134.647407	4.031322
1.160914	132.979029	4.036326
0.777856	138.605131	4.041331
1.039814	144.701524	4.046336
0.909811	148.821504	4.051341
1.285333	147.302081	4.056346
1.109857	171.144067	4.061350
1.044237	153.392374	4.066355
1.420986	156.401702	4.071360
1.624129	160.285614	4.076365
1.882323	141.751128	4.081370
1.201547	133.208346	4.086374
1.081692	131.530981	4.091379
1.387198	140.620403	4.096384
0.933851	125.653878	4.101389
1.305362	123.506250	4.106394
1.448342	150.210866	4.111398
1.225567	151.197288	4.116403
1.259621	147.196915	4.121408
1.354823	140.915500	4.126413
1.517407	148.454249	4.131418
1.503314	158.328750	4.136422
1.428185	157.858032	4.141427
1.546614	137.780144	4.146432
1.007237	122.877162	4.151437
1.496262	136.507419	4.156442
1.404865	156.216413	4.161446
1.517443	158.413542	4.166451
1.634594	140.910138	4.171456
1.438481	144.608972	4.176461
1.473735	148.050477	4.181466
1.695969	171.226771	4.186470
1.254091	151.334484	4.191475
1.566781	138.362742	4.196480
1.530360	163.865036	4.201485
1.860129	178.662989	4.206490
1.466188	156.709841	4.211494
1.502889	122.513303	4.216499
1.072837	140.584882	4.221504
1.348852	168.172032	4.226509
1.506279	175.223939	4.231514
1.196821	165.448940	4.236518
1.769147	146.429477	4.241523
1.566920	156.836487	4.246528
1.501488	175.203570	4.251533
1.720149	153.340168	4.256538
1.499775	149.731541	4.261542
1.750869	155.365307	4.266547
1.648284	165.840791	4.271552
1.517339	163.404198	4.276557
1.555798	151.770426	4.281562
1.471684	166.510597	4.286566
1.876137	170.973838	4.291571
2.007238	157.241043	4.296576
1.843111	176.020798	4.301581
2.034444	165.228066	4.306586
1.911875	156.806690	4.311590
1.893467	156.293848	4.316595
2.124524	165.784157	4.321600
1.671012	166.390450	4.326605
1.811763	151.768839	4.331610
2.099004	151.810582	4.336614
2.177467	160.035021	4.341619
1.871522	178.146309	4.346624
1.649910	153.420932	4.351629
2.130186	156.042833	4.356634
1.680314	170.613507	4.361638
1.996404	154.406473	4.366643
2.167610	149.522151	4.371648
2.029101	169.082790	4.376653
2.442941	168.905037	4.381658
2.222075	156.779454	4.386662
2.258470	150.827861	4.391667
2.136503	165.442198	4.396672
1.819864	170.697967	4.401677
2.147543	162.479574	4.406682
1.821327	159.573240	4.411686
1.888749	152.913564	4.416691
2.179129	176.619877	4.421696
1.773969	176.452782	4.426701
2.009255	158.140564	4.431706
1.818470	162.707597	4.436710
1.867898	162.873773	4.441715
1.832759	153.224007	4.446720
1.974851	157.963802	4.451725
2.365666	162.974907	4.456730
1.898477	159.077292	4.461734
2.053154	171.572962	4.466739
2.228538	195.165332	4.471744
2.228908	197.814956	4.476749
2.216750	183.361918	4.481754
2.368525	197.379910	4.486758
2.511182	186.896277	4.491763
2.447036	187.347075	4.496768
2.141433	185.460689	4.501773
2.370186	196.526488	4.506778
2.211237	202.030741	4.511782
2.166109	189.633517	4.516787
2.247517	172.002417	4.521792
2.139902	189.139164	4.526797
2.510973	196.285396	4.531802
2.331071	189.788602	4.536806
2.505089	189.585375	4.541811
2.304459	192.781474	4.546816
2.263283	196.749472	4.551821
2.655541	173.071158	4.556826
2.155710	180.310997	4.561830
2.202675	186.764129	4.566835
2.598150	187.269678	4.571840
2.350191	180.429008	4.576845
2.212510	171.911968	4.581850
2.159128	188.626916	4.586854
2.285942	188.733743	4.591859
2.210360	187.353578	4.596864
2.393410	192.625324	4.601869
2.552818	189.649976	4.606874
2.378446	196.809896	4.611878
2.762930	215.884277	4.616883
2.523213	201.026076	4.621888
2.700908	205.789596	4.626893
2.895298	198.989358	4.631898
2.375016	183.567830	4.636902
2.655806	210.628901	4.641907
2.858390	198.118697	4.646912
2.640868	195.295605	4.651917
2.732149	186.335478	4.656922
2.468471	195.008598	4.661926
2.705024	191.381665	4.666931
2.738664	210.361018	4.671936
2.734500	200.720580	4.676941
2.543194	213.738901	4.681946
2.646594	234.634585	4.686950
2.588233	228.554794	4.691955
2.292206	218.226696	4.696960
2.585315	217.362386	4.701965
2.801331	224.097447	4.706970
2.801222	223.959594	4.711974
2.960004	222.573544	4.716979
2.788687	211.052227	4.721984
2.831681	218.094556	4.726989
2.827555	203.924347	4.731994
2.589526	219.399595	4.736998
2.422154	223.936142	4.742003
2.668059	225.619394	4.747008
2.796443	218.877504	4.752013
2.796317	213.975902	4.757018
2.959105	233.981841	4.762022
2.883042	235.565696	4.767027
3.162382	244.707841	4.772032
2.946004	230.251022	4.777037
3.324796	235.599834	4.782042
2.980937	236.750099	4.787046
2.764003	232.076878	4.792051
3.086884	225.702462	4.797056
2.933270	222.483785	4.802061
3.383624	237.556723	4.807066
2.916326	244.996401	4.812070
2.897511	234.242789	4.817075
2.859121	238.140791	4.822080
3.140607	239.880805	4.827085
3.328482	237.843414	4.832090
2.831325	254.440397	4.837094
2.675214	247.980093	4.842099
3.064211	237.227644	4.847104
2.936160	239.344793	4.852109
3.099795	229.009285	4.857114
3.368795	239.768281	4.862118
3.090499	258.774558	4.867123
3.278728	259.712597	4.872128
2.815437	254.055337	4.877133
3.065780	239.436345	4.882138
2.969072	272.617993	4.887142
3.407122	263.862521	4.892147
3.056424	249.828783	4.897152
2.736455	263.320582	4.902157
3.307675	248.858770	4.907162
3.044008	282.740706	4.912166
3.150528	292.522362	4.917171
3.485483	272.644972	4.922176
3.609925	294.230552	4.927181
3.333600	278.316018	4.932186
3.336185	269.306084	4.937190
3.419369	260.799647	4.942195
3.520332	276.765313	4.947200
3.431456	299.677741	4.952205
3.504091	284.481394	4.957210
3.558064	272.333481	4.962214
3.477791	275.506255	4.967219
3.553768	286.221126	4.972224
3.428768	301.597355	4.977229
3.427525	275.077073	4.982234
3.380290	287.266662	4.987238
3.725859	276.853902	4.992243
3.570810	268.784477	4.997248
3.445487	286.566650	5.002253
3.417215	294.292283	5.007258
3.444842	298.752137	5.012262
3.468114	291.289704	5.017267
3.250815	270.245237	5.022272
3.217248	298.768057	5.027277
3.264325	296.429377	5.032282
3.696884	298.549675	5.037286
3.433041	278.732071	5.042291
3.683302	272.858630	5.047296
3.633627	292.258156	5.052301
3.436193	297.635531	5.057306
3.589842	281.992440	5.062310
3.655148	263.212880	5.067315
3.885357	291.873607	5.072320
3.583530	304.059905	5.077325
3.960441	304.596344	5.082330
3.805304	281.651111	5.087334
3.553882	285.484203	5.092339
3.493726	301.284652	5.097344
3.710238	321.640115	5.102349
4.364286	313.568750	5.107354
3.871268	315.587106	5.112358
3.770634	296.280727	5.117363
4.041422	289.643120	5.122368
3.614698	277.755364	5.127373
3.667347	288.371202	5.132378
3.946960	314.027298	5.137382
4.236315	310.872222	5.142387
3.976242	291.407924	5.147392
4.054606	288.606351	5.152397
3.734726	292.699645	5.157402
3.540596	305.844459	5.162406
3.526102	304.510614	5.167411
3.960862	292.119627	5.172416
3.918231	316.492704	5.177421
4.110919	323.769392	5.182426
3.862249	320.876254	5.187430
4.208044	315.231655	5.192435
4.407375	297.115406	5.197440
3.899275	317.515738	5.202445
4.014003	318.693902	5.207450
4.044849	309.973933	5.212454
3.924060	306.515131	5.217459
4.300638	312.029176	5.222464
3.991383	332.275628	5.227469
4.275725	320.750446	5.232474
4.332292	315.209873	5.237478
4.062208	311.552799	5.242483
4.330988	308.597531	5.247488
4.217784	318.873535	5.252493
4.279851	320.966478	5.257498
4.405891	315.225318	5.262502
4.344930	324.261671	5.267507
4.079209	308.245325	5.272512
3.827495	310.603003	5.277517
4.526179	295.894081	5.282522
4.258717	320.833958	5.287526
4.256079	336.981845	5.292531
4.491992	319.002859	5.297536
4.180940	307.482564	5.302541
4.568830	307.354378	5.307546
4.564722	322.536044	5.312550
3.938061	306.385999	5.317555
4.370350	300.615245	5.322560
3.955835	304.716685	5.327565
4.096761	305.796803	5.332570
4.148351	312.268856	5.337574
3.821470	315.473612	5.342579
4.108923	313.284805	5.347584
3.857082	320.624990	5.352589
4.111268	317.747892	5.357594
4.263665	341.364608	5.362598
4.507227	342.451838	5.367603
4.843972	336.469971	5.372608
4.106943	371.627418	5.377613
4.493198	353.857242	5.382618
4.259147	348.611699	5.387622
4.639716	342.969827	5.392627
4.721216	352.342915	5.397632
4.293419	351.019856	5.402637
4.673378	341.513465	5.407642
4.559602	344.991580	5.412646
4.699049	360.449745	5.417651
4.765589	349.059676	5.422656
4.427467	351.731923	5.427661
4.730520	364.866242	5.432666
4.196602	361.792557	5.437670
4.796511	343.467804	5.442675
4.765681	355.069558	5.447680
4.429063	357.058719	5.452685
4.335368	347.036247	5.457690
4.542705	346.807388	5.462694
4.828723	352.543081	5.467699
4.832280	351.958930	5.472704
4.598985	354.190458	5.477709
4.810045	343.210758	5.482714
4.606042	367.798805	5.487718
4.324824	367.917229	5.492723
4.554419	344.182373	5.497728
4.688134	348.845482	5.502733
4.770434	359.560543	5.507738
4.788101	365.380441	5.512742
4.898615	365.919081	5.517747
4.817383	341.164380	5.522752
4.840649	355.744935	5.527757
4.800650	377.727639	5.532762
4.790907	373.666081	5.537766
4.925620	371.069049	5.542771
5.097202	363.702816	5.547776
4.972727	387.862643	5.552781
4.852379	370.323845	5.557786
4.697032	363.341913	5.562790
4.840886	370.845987	5.567795
5.304154	373.065295	5.572800
5.133078	392.788945	5.577805
5.114529	383.228824	5.582810
4.994512	359.760656	5.587814
4.782193	364.695810	5.592819
5.164216	376.651763	5.597824
5.337843	381.516039	5.602829
5.237253	369.804559	5.607834
5.093648	346.629445	5.612838
4.932014	363.223480	5.617843
5.137885	354.359637	5.622848
5.035415	350.606984	5.627853
5.077520	363.785708	5.632858
4.948035	374.780623	5.637862
4.740699	382.703495	5.642867
5.129418	381.640582	5.647872
5.154205	396.151476	5.652877
5.061165	373.639955	5.657882
5.163075	382.105779	5.662886
4.991762	403.147121	5.667891
5.247733	392.779078	5.672896
4.886337	386.963468	5.677901
5.255900	364.470312	5.682906
5.282653	376.960853	5.687910
4.841400	399.535593	5.692915
5.395744	387.024147	5.697920
5.356119	387.682992	5.702925
5.180552	375.253706	5.707930
5.095080	393.006629	5.712934
5.280071	396.618670	5.717939
5.337413	386.712180	5.722944
5.215442	395.901698	5.727949
5.388387	381.680976	5.732954
5.509419	388.317671	5.737958
5.073935	392.251248	5.742963
5.234764	394.791821	5.747968
5.508242	408.991432	5.752973
5.241907	403.481600	5.757978
5.473756	400.282837	5.762982
5.776725	410.992542	5.767987
5.553808	414.101909	5.772992
5.514483	398.977911	5.777997
5.016838	383.733359	5.783002
5.278807	396.210003	5.788006
5.202443	420.600461	5.793011
5.289400	413.082757	5.798016
5.694846	423.399981	5.803021
5.259071	420.430712	5.808026
5.699221	408.502190	5.813030
5.402232	421.975138	5.818035
5.464282	416.750185	5.823040
5.574797	424.951812	5.828045
5.134491	415.115904	5.833050
5.666594	406.607014	5.838054
5.363603	406.500272	5.843059
5.199631	408.116133	5.848064
5.352793	443.669099	5.853069
5.237034	447.596710	5.858074
5.754866	432.928101	5.863078
5.224933	443.291405	5.868083
5.827926	453.509910	5.873088
5.801057	460.068287	5.878093
5.412546	442.325720	5.883098
5.952335	428.878106	5.888102
5.875623	447.409754	5.893107
5.954884	452.192282	5.898112
6.002687	457.377464	5.903117
5.840195	463.456332	5.908122
6.000705	449.236221	5.913126
5.835885	443.833106	5.918131
5.997275	430.836105	5.923136
5.906563	447.906030	5.928141
6.167118	461.888235	5.933146
5.741376	452.975119	5.938150
5.464522	465.319497	5.943155
5.870049	462.740929	5.948160
5.897452	457.641546	5.953165
5.829997	434.045804	5.958170
6.042610	449.455370	5.963174
5.976148	457.566305	5.968179
5.982608	460.567242	5.973184
5.656038	450.842435	5.978189
5.756249	439.849318	5.983194
6.198474	446.812755	5.988198
5.733279	456.163103	5.993203
5.839244	454.973192	5.998208
5.815411	451.184140	6.003213
5.702773	444.634985	6.008218
6.050267	471.868267	6.013222
6.101306	493.544783	6.018227
6.440990	465.553012	6.023232
6.023585	469.234829	6.028237
6.111100	452.570235	6.033242
6.029718	448.159246	6.038246
5.907323	464.376876	6.043251
6.029439	469.691046	6.048256
6.110497	457.062630	6.053261
5.947196	463.726814	6.058266
6.077638	462.813612	6.063270
5.942066	462.911223	6.068275
6.394681	449.662370	6.073280
6.312316	451.211775	6.078285
6.196660	447.637562	6.083290
6.424563	467.664615	6.088294
6.146232	459.571564	6.093299
6.239343	456.781038	6.098304
6.257515	460.559559	6.103309
6.163096	448.438496	6.108314
6.299267	450.021037	6.113318
6.135576	448.336379	6.118323
5.989037	448.764006	6.123328
5.870606	438.219175	6.128333
6.074519	459.146104	6.133338
6.234720	459.446982	6.138342
5.990991	430.860458	6.143347
5.931530	410.800265	6.148352
6.013251	425.586476	6.153357
5.939579	452.603837	6.158362
6.188822	449.237348	6.163366
6.018682	429.542367	6.168371
6.105468	419.091484	6.173376
5.688461	438.775930	6.178381
5.781064	449.210079	6.183386
6.037952	449.588595	6.188390
5.647280	439.589295	6.193395
6.117849	452.466452	6.198400
6.073197	477.346974	6.203405
6.048298	461.121093	6.208410
6.206284	433.163748	6.213414
6.178786	456.960712	6.218419
6.237203	473.207265	6.223424
6.323075	448.174997	6.228429
5.957458	430.870703	6.233434
5.941171	426.185671	6.238438
5.920573	436.974119	6.243443
6.006236	430.141042	6.248448
5.991583	429.686957	6.253453
5.808987	443.552975	6.258458
6.028073	449.155047	6.263462
6.035390	451.815800	6.268467
6.066981	451.548508	6.273472
5.983266	445.882408	6.278477
5.964978	456.363890	6.283482
6.078391	456.343803	6.288486
6.122736	468.045777	6.293491
6.437787	440.333154	6.298496
5.654040	425.556773	6.303501
5.744556	445.540110	6.308506
5.826717	459.659716	6.313510
5.916808	462.403467	6.318515
6.080247	439.594951	6.323520
6.120501	436.420149	6.328525
5.757915	452.843682	6.333530
6.004237	433.784616	6.338534
6.012812	441.565001	6.343539
6.008759	444.848820	6.348544
5.936845	458.344583	6.353549
5.811943	452.814615	6.358554
5.910112	440.124888	6.363558
5.714776	459.883116	6.368563
6.335617	446.253798	6.373568
5.738914	458.468726	6.378573
5.937443	451.470691	6.383578
6.356777	443.301814	6.388582
5.938245	467.851389	6.393587
5.814269	460.597483	6.398592
5.993332	440.941257	6.403597
5.884741	450.612860	6.408602
6.079973	463.297884	6.413606
5.514378	465.105208	6.418611
5.944301	433.865775	6.423616
5.818160	440.750502	6.428621
5.702708	465.607389	6.433626
6.265088	462.000731	6.438630
5.580660	456.726491	6.443635
6.180964	469.424484	6.448640
6.212032	478.889243	6.453645
6.475689	491.685405	6.458650
6.099636	472.948142	6.463654
5.884997	452.336939	6.468659
5.802399	449.450661	6.473664
5.970351	469.619517	6.478669
6.046803	466.843678	6.483674
5.934003	447.446883	6.488678
5.935338	461.727129	6.493683
6.128693	447.877541	6.498688
6.066303	470.894164	6.503693
6.064241	456.471753	6.508698
6.157310	448.317135	6.513702
5.821699	464.422718	6.518707
6.225405	463.647053	6.523712
6.005841	455.927641	6.528717
5.883492	468.881882	6.533722
5.919439	447.643894	6.538726
5.694418	454.898622	6.543731
6.230139	463.901559	6.548736
6.525206	453.375984	6.553741
6.165532	441.116262	6.558746
6.324203	446.608757	6.563750
5.963710	459.539704	6.568755
6.303632	452.263198	6.573760
6.234074	451.013215	6.578765
6.447903	458.832393	6.583770
6.087521	446.688992	6.588774
5.786327	441.623102	6.593779
6.412501	455.999353	6.598784
6.236064	469.155687	6.603789
5.870860	449.308345	6.608794
5.797131	445.756897	6.613798
5.676806	466.501945	6.618803
6.158764	449.029250	6.623808
5.964597	467.334205	6.628813
6.214610	460.247359	6.633818
6.640618	446.118228	6.638822
6.129213	469.280375	6.643827
6.177567	462.454732	6.648832
6.114582	438.790769	6.653837
5.779900	449.340020	6.658842
5.946382	446.509157	6.663846
5.899165	467.293127	6.668851
5.973611	456.059312	6.673856
6.017732	447.663795	6.678861
5.861897	454.512989	6.683866
5.753384	460.873455	6.688870
5.938977	476.668493	6.693875
6.128040	456.229496	6.698880
5.977742	458.521605	6.703885
5.788456	466.876380	6.708890
6.323252	470.575150	6.713894
6.026517	473.443498	6.718899
6.230305	466.140257	6.723904
6.254727	478.011853	6.728909
6.011317	475.446710	6.733914
6.413150	460.585348	6.738918
5.916173	461.247763	6.743923
6.044501	433.838871	6.748928
5.935081	424.010917	6.753933
5.724646	453.233766	6.758938
6.175782	453.401628	6.763942
5.898532	445.268750	6.768947
6.054274	452.644432	6.773952
6.118749	466.418541	6.778957
6.087830	458.994576	6.783962
6.056439	460.269504	6.788966
5.862724	467.672758	6.793971
6.381319	447.698896	6.798976
6.210558	441.397386	6.803981
6.086030	426.039242	6.808986
5.837470	426.807590	6.813990
5.830978	431.550913	6.818995
6.193158	439.087008	6.824000
5.765273	438.848494	6.829005
6.070467	428.944028	6.834010
6.293941	428.538092	6.839014
5.833362	435.684456	6.844019
6.048066	439.943464	6.849024
5.913597	420.167233	6.854029
5.712308	417.330664	6.859034
6.116560	441.912224	6.864038
5.940386	460.099074	6.869043
6.277717	454.192136	6.874048
6.287491	453.451090	6.879053
5.926309	449.224842	6.884058
6.045233	429.677907	6.889062
5.579845	428.144225	6.894067
5.915722	441.365125	6.899072
6.008963	446.999141	6.904077
5.715897	457.082313	6.909082
5.980161	460.016378	6.914086
5.764544	457.492616	6.919091
5.997440	451.432079	6.924096
5.873354	457.437319	6.929101
5.956334	455.307932	6.934106
6.258623	459.066135	6.939110
6.477215	456.477324	6.944115
6.131224	454.141823	6.949120
6.241685	468.173895	6.954125
6.142882	462.058078	6.959130
6.298636	445.145559	6.964134
5.953656	429.143861	6.969139
5.832787	425.805396	6.974144
5.930520	455.929178	6.979149
5.892380	444.758271	6.984154
5.929736	444.056960	6.989158
5.678501	464.207187	6.994163
5.955774	440.722563	6.999168
5.726113	460.118111	7.004173
5.600137	466.114099	7.009178
6.046815	447.488807	7.014182
5.666064	444.492782	7.019187
5.792860	456.128049	7.024192
5.815409	468.282376	7.029197
5.626081	463.291117	7.034202
5.854764	477.663628	7.039206
5.917741	508.396295	7.044211
6.075626	496.876688	7.049216
6.101467	495.102106	7.054221
5.770531	498.378400	7.059226
6.258984	489.905188	7.064230
6.291348	488.785641	7.069235
6.189837	489.965421	7.074240
6.115168	460.694397	7.079245
6.161721	460.747803	7.084250
6.161650	457.039561	7.089254
6.069861	460.414828	7.094259
5.911589	470.956545	7.099264
6.041358	459.885135	7.104269
5.526234	454.195722	7.109274
5.791838	469.149180	7.114278
6.202616	478.733886	7.119283
6.469564	480.794670	7.124288
5.976979	482.787326	7.129293
6.108626	471.425472	7.134298
6.137466	463.190013	7.139302
5.777482	459.066356	7.144307
5.761951	468.244739	7.149312
6.049724	468.449956	7.154317
5.591061	461.198187	7.159322
5.878527	464.740631	7.164326
5.973708	489.151878	7.169331
6.246799	508.409554	7.174336
6.486866	506.492535	7.179341
6.208216	479.723571	7.184346
6.253895	459.386592	7.189350
5.863916	465.901694	7.194355
5.779870	478.939384	7.199360
6.078099	458.512826	7.204365
5.795689	452.768678	7.209370
6.111702	453.614783	7.214374
5.733368	462.284706	7.219379
5.593733	484.825708	7.224384
6.010513	488.827699	7.229389
6.233892	498.463905	7.234394
6.294416	490.763000	7.239398
6.299131	479.803393	7.244403
6.080760	470.914298	7.249408
6.054392	481.503475	7.254413
5.853201	464.148690	7.259418
5.909294	446.554504	7.264422
5.958198	456.138822	7.269427
6.217766	481.834618	7.274432
5.918293	475.120410	7.279437
5.817295	473.926820	7.284442
6.238574	496.020994	7.289446
6.111025	498.971677	7.294451
6.186078	467.659520	7.299456
5.803166	454.205839	7.304461
5.946270	472.107426	7.309466
6.277285	483.433933	7.314470
5.903650	477.000502	7.319475
6.078701	451.607729	7.324480
5.791145	461.005570	7.329485
5.961521	496.982174	7.334490
6.338660	485.366264	7.339494
5.863770	485.455533	7.344499
5.938591	479.722479	7.349504
6.055974	474.006366	7.354509
6.303591	477.893072	7.359514
6.445514	472.995631	7.364518
6.017566	466.146597	7.369523
6.171662	462.604945	7.374528
6.117556	462.211734	7.379533
5.902252	467.197922	7.384538
6.219253	462.716160	7.389542
5.943914	473.721538	7.394547
5.809421	461.326432	7.399552
5.996723	445.472424	7.404557
5.814073	459.739964	7.409562
6.218662	475.828099	7.414566
5.670127	460.407506	7.419571
5.842315	475.115778	7.424576
5.813557	453.880386	7.429581
6.034864	468.252134	7.434586
6.212194	472.617061	7.439590
6.095618	476.185635	7.444595
5.919944	472.218455	7.449600
5.901226	458.124236	7.454605
5.894151	456.088156	7.459610
6.376286	466.767798	7.464614
6.052427	468.900173	7.469619
6.062003	467.180369	7.474624
5.866856	467.492225	7.479629
5.908893	477.262657	7.484634
6.039847	450.665079	7.489638
6.038360	475.925562	7.494643
6.001670	472.457461	7.499648
6.250805	458.077288	7.504653
5.775203	471.699951	7.509658
6.012931	454.805146	7.514662
5.905819	463.833227	7.519667
6.097381	475.373856	7.524672
6.398337	483.387290	7.529677
6.017608	466.305932	7.534682
6.136405	463.556933	7.539686
6.168994	471.355857	7.544691
6.030652	467.347587	7.549696
6.097657	458.447937	7.554701
6.000908	460.396779	7.559706
6.005858	469.837537	7.564710
5.761568	474.674034	7.569715
5.850938	464.778972	7.574720
6.059922	446.409792	7.579725
5.650825	456.024913	7.584730
5.945828	474.653595	7.589734
6.200364	475.083502	7.594739
6.442219	482.273221	7.599744
6.098381	457.195448	7.604749
5.994923	455.897895	7.609754
6.072163	460.550051	7.614758
5.953328	474.885583	7.619763
6.151789	472.778443	7.624768
6.215331	461.461687	7.629773
6.102593	462.088917	7.634778
6.353076	460.037697	7.639782
6.124178	467.418157	7.644787
5.927901	454.432992	7.649792
6.107927	456.628587	7.654797
5.715617	465.717118	7.659802
5.941618	462.758334	7.664806
5.741406	462.120944	7.669811
5.958907	468.529244	7.674816
5.764429	466.229470	7.679821
5.656329	460.787380	7.684826
6.109493	467.143712	7.689830
5.874700	486.969559	7.694835
6.226022	487.006930	7.699840
6.252530	471.449074	7.704845
5.928713	468.407825	7.709850
6.017546	474.655088	7.714854
5.715063	471.542937	7.719859
6.047018	482.722696	7.724864
6.336502	490.555037	7.729869
5.948196	483.996376	7.734874
6.266377	477.407677	7.739878
5.905534	474.582668	7.744883
6.179575	463.342104	7.749888
6.100415	457.161881	7.754893
5.876429	479.133210	7.759898
5.929671	482.464587	7.764902
6.055843	470.137969	7.769907
5.921234	450.893436	7.774912
6.065470	464.207189	7.779917
5.621334	472.306263	7.784922
6.227554	461.989003	7.789926
5.784003	477.184748	7.794931
6.245672	477.999878	7.799936
6.079701	469.870497	7.804941
5.935565	462.506377	7.809946
6.265817	451.358239	7.814950
6.105842	460.009537	7.819955
6.005031	463.960823	7.824960
6.127494	469.387493	7.829965
6.157042	463.913382	7.834970
6.173002	440.066203	7.839974
6.099668	458.588823	7.844979
5.995559	468.176240	7.849984
6.107338	472.865701	7.854989
6.067575	462.557039	7.859994
6.068972	457.582304	7.864998
5.973652	474.610207	7.870003
5.860983	460.762251	7.875008
6.268425	453.368835	7.880013
5.659469	452.536097	7.885018
5.966676	450.438511	7.890022
6.051234	470.186701	7.895027
6.107428	476.389640	7.900032
6.119571	463.436217	7.905037
5.932356	456.199669	7.910042
6.268092	453.349220	7.915046
6.292842	463.764701	7.920051
5.719510	461.327576	7.925056
6.074419	472.535595	7.930061
5.873524	470.697964	7.935066
5.726201	456.347699	7.940070
5.701288	466.648671	7.945075
5.847295	460.033585	7.950080
6.095164	450.126346	7.955085
5.916305	465.037438	7.960090
6.112123	453.203713	7.965094
6.157342	453.043471	7.970099
5.792100	476.045240	7.975104
6.105161	458.372864	7.980109
6.237279	468.971058	7.985114
6.207191	459.649750	7.990118
6.105420	440.943547	7.995136
6.223489	456.365062	8.000154
6.085292	461.602864	8.005171
5.857815	459.736418	8.010189
6.084393	439.431665	8.015206
5.989309	451.648693	8.020224
5.890488	452.647847	8.025242
6.305213	449.546959	8.030259
6.114460	480.584217	8.035277
6.322745	467.292242	8.040294
6.383403	447.071182	8.045312
6.050239	451.809661	8.050330
6.347339	469.898262	8.055347
6.003577	478.590215	8.060365
6.026326	470.259171	8.065382
6.136418	484.389984	8.070400
5.691159	484.421785	8.075418
6.226312	462.251864	8.080435
6.424079	456.933839	8.085453
6.063304	468.470885	8.090470
6.123338	465.438744	8.095488
6.050131	467.125198	8.100506
6.059858	457.819528	8.105523
6.008705	469.090705	8.110541
5.868619	478.146324	8.115558
6.400221	465.498455	8.120576
6.171422	450.343951	8.125594
6.197764	438.479400	8.130611
6.319041	463.693904	8.135629
6.209973	467.794741	8.140646
6.185159	455.722158	8.145664
6.176722	459.604354	8.150682
6.358108	468.276622	8.155699
5.857390	456.144339	8.160717
6.135804	440.114325	8.165734
6.028395	462.088931	8.170752
5.968861	464.718422	8.175770
5.897299	453.400889	8.180787
5.829673	446.630113	8.185805
6.197076	469.679767	8.190822
6.520610	498.044137	8.195840
6.129617	488.793650	8.200858
6.473160	457.536866	8.205875
6.236157	450.672461	8.210893
6.449792	452.208981	8.215910
6.249132	466.723811	8.220928
6.098845	461.611686	8.225946
6.342075	440.922202	8.230963
6.221727	457.655190	8.235981
6.360352	477.606072	8.240998
6.336594	472.533252	8.246016
6.536943	460.118425	8.251034
6.388351	452.120146	8.256051
5.960447	465.670753	8.261069
6.377403	461.098659	8.266086
6.377488	449.840429	8.271104
6.032867	474.485971	8.276122
6.135008	463.078325	8.281139
6.267841	460.907032	8.286157
6.336981	468.923833	8.291174
6.151671	480.248380	8.296192
6.103159	505.354043	8.301210
6.600458	485.118434	8.306227
6.749964	479.028877	8.311245
6.425260	478.592164	8.316262
6.637759	482.486660	8.321280
6.309266	474.094107	8.326298
6.141183	454.220493	8.331315
6.168272	468.299181	8.336333
6.522027	468.709519	8.341350
6.590680	467.590361	8.346368
6.295994	472.953999	8.351386
6.025018	457.682282	8.356403
6.095352	469.622257	8.361421
6.228986	506.690424	8.366438
6.313008	494.069267	8.371456
6.369553	498.872652	8.376474
6.469620	501.118495	8.381491
6.478714	487.039873	8.386509
6.969910	497.393433	8.391526
6.709326	508.737722	8.396544
6.481245	487.080793	8.401562
6.258965	460.457247	8.406579
6.301367	470.126514	8.411597
6.417987	506.216869	8.416614
6.670737	509.007593	8.421632
6.402461	496.014267	8.426650
6.401784	488.459500	8.431667
6.229855	494.160039	8.436685
6.428086	500.244064	8.441702
6.758670	503.911630	8.446720
6.685791	496.817876	8.451738
6.541784	488.561315	8.456755
6.753534	494.228951	8.461773
6.282660	479.239388	8.466790
6.713670	476.627000	8.471808
6.157328	461.179767	8.476826
6.579298	473.219856	8.481843
6.323179	476.526729	8.486861
6.334342	486.067644	8.491878
6.416970	500.085131	8.496896
6.052129	510.136692	8.501914
6.128347	484.814273	8.506931
6.765214	481.490698	8.511949
6.628665	496.651761	8.516966
6.795973	509.136900	8.521984
6.531785	503.964964	8.527002
6.833786	493.605945	8.532019
6.584590	482.282618	8.537037
6.498403	495.353772	8.542054
6.892289	498.983029	8.547072
6.741015	496.322025	8.552090
6.715319	481.443975	8.557107
6.710358	486.112090	8.562125
6.652754	514.482013	8.567143
6.996446	500.838789	8.572160
6.634627	494.842976	8.577178
7.124971	484.511188	8.582195
6.773259	491.231801	8.587213
6.655865	488.518756	8.592231
6.597671	462.361157	8.597248
6.380132	481.108767	8.602266
6.721599	485.805139	8.607283
6.835058	479.546196	8.612301
6.579525	496.615944	8.617319
7.001960	506.042757	8.622336
6.538714	486.502443	8.627354
6.691377	468.302079	8.632371
7.012488	475.811827	8.637389
6.588193	489.624676	8.642407
6.715742	466.158722	8.647424
6.230280	458.301027	8.652442
6.476118	478.889121	8.657459
6.677152	484.548193	8.662477
6.772129	501.195757	8.667495
7.037813	499.360570	8.672512
6.474891	504.073668	8.677530
6.764757	494.582055	8.682547
6.741097	514.522708	8.687565
6.365363	504.449551	8.692583
6.463877	479.107616	8.697600
6.336020	507.536563	8.702618
6.562930	482.907444	8.707635
6.880788	486.428235	8.712653
6.933666	503.795447	8.717671
6.964183	496.434874	8.722688
6.743519	502.716337	8.727706
6.914865	494.749883	8.732723
6.756700	491.382152	8.737741
6.802277	482.862539	8.742759
6.867397	497.925629	8.747776
7.035147	511.014853	8.752794
6.687421	501.822544	8.757811
7.033561	508.675898	8.762829
6.846175	513.270654	8.767847
6.962818	492.950543	8.772864
6.688588	482.606860	8.777882
6.786136	496.952492	8.782899
6.792839	513.888004	8.787917
6.508083	499.427248	8.792935
6.708090	488.487326	8.797952
6.873788	479.841301	8.802970
6.726672	493.176385	8.807987
6.879261	513.311075	8.813005
6.930493	520.112018	8.818023
7.145165	506.381578	8.823040
6.964620	513.032981	8.828058
6.848013	506.579928	8.833075
6.982142	502.129246	8.838093
6.819234	507.857326	8.843111
6.893317	492.777691	8.848128
6.934970	499.759290	8.853146
6.715560	516.245009	8.858163
7.086255	515.198831	8.863181
6.784558	534.050054	8.868199
7.223457	542.420531	8.873216
7.274860	526.667048	8.878234
7.075398	516.113306	8.883251
7.173799	501.772935	8.888269
6.839698	494.870339	8.893287
6.748857	486.643663	8.898304
6.975032	517.595467	8.903322
6.951633	533.956319	8.908339
7.154664	524.485237	8.913357
6.995823	519.912246	8.918375
6.884381	511.047019	8.923392
6.834533	530.214192	8.928410
7.267909	527.841888	8.933427
7.199647	509.295319	8.938445
7.111451	529.550015	8.943463
7.309172	525.258650	8.948480
7.341921	521.842830	8.953498
7.000788	514.445171	8.958515
7.056994	511.480958	8.963533
6.658225	500.314188	8.968551
6.905661	514.023529	8.973568
7.196757	518.914992	8.978586
6.950091	512.037397	8.983603
7.164664	518.843029	8.988621
7.230444	538.002813	8.993639
7.456361	518.701420	8.998656
7.088680	532.734119	9.003674
6.870932	553.073525	9.008691
7.538582	526.046866	9.013709
7.253869	514.384798	9.018727
7.267884	517.376938	9.023744
6.843119	529.670945	9.028762
6.857828	544.033263	9.033779
7.122865	518.013634	9.038797
7.092473	514.709698	9.043815
7.421444	531.653766	9.048832
7.413493	539.896275	9.053850
7.158289	526.206373	9.058867
7.646724	514.629271	9.063885
7.119285	537.243904	9.068903
7.288332	516.197785	9.073920
7.067501	508.716782	9.078938
7.201330	526.699105	9.083955
7.121280	530.151547	9.088973
6.822964	524.451735	9.093991
6.753991	523.224941	9.099008
7.021593	539.186922	9.104026
7.042836	532.818724	9.109043
7.238521	524.605782	9.114061
7.694989	535.981058	9.119079
7.149085	539.431476	9.124096
7.134594	533.057375	9.129114
7.101610	513.613689	9.134131
7.339068	504.537702	9.139149
7.324279	521.229896	9.144167
7.121380	523.210841	9.149184
7.403786	533.624808	9.154202
7.159139	525.280558	9.159219
7.408385	522.551786	9.164237
7.127871	524.277031	9.169255
7.236921	525.336299	9.174272
7.499763	518.569916	9.179290
7.425009	527.695158	9.184307
7.585170	526.802931	9.189325
7.281774	532.938478	9.194343
7.136102	521.788708	9.199360
7.453102	519.603404	9.204378
7.119019	532.419184	9.209395
7.460191	548.075892	9.214413
7.492677	553.339931	9.219431
7.500130	568.821560	9.224448
7.205025	564.306006	9.229466
7.323677	559.417143	9.234483
7.462171	532.744280	9.239501
7.531674	555.181670	9.244519
7.421451	570.270463	9.249536
7.709283	569.915933	9.254554
7.407422	559.073560	9.259571
7.620038	558.014439	9.264589
7.317818	555.042146	9.269607
7.424291	538.982488	9.274624
7.738472	555.402700	9.279642
7.369881	552.977444	9.284659
7.606449	547.161580	9.289677
7.414948	532.189361	9.294695
7.613065	549.914011	9.299712
7.435255	542.228595	9.304730
7.674368	538.608540	9.309747
7.791344	545.176645	9.314765
7.266688	527.899527	9.319783
7.392044	538.652354	9.324800
7.568283	534.420820	9.329818
7.605706	561.189849	9.334835
7.295802	572.727323	9.339853
7.750620	569.083815	9.344871
7.362997	550.901892	9.349888
7.938028	557.823416	9.354906
7.885370	573.603583	9.359923
7.939961	521.485274	9.364941
7.408272	530.791118	9.369959
7.221318	543.648716	9.374976
7.326711	535.277215	9.379994
7.515772	542.515890	9.385011
7.546010	542.267396	9.390029
7.764960	554.863689	9.395047
7.660928	554.837623	9.400064
8.034527	560.543479	9.405082
7.502645	563.450498	9.410099
7.726177	551.586825	9.415117
7.328911	569.674579	9.420135
7.357862	574.878696	9.425152
7.504654	566.212426	9.430170
7.460188	567.669303	9.435187
7.506930	577.133056	9.440205
7.421087	562.608373	9.445223
7.545757	570.259950	9.450240
7.748070	579.716297	9.455258
7.583348	566.851032	9.460275
7.285033	553.821195	9.465293
7.586590	560.382221	9.470311
7.669921	581.616721	9.475328
7.994847	585.261233	9.480346
7.665268	567.043426	9.485363
7.835454	559.562033	9.490381
7.900331	562.571458	9.495399
7.562660	569.356695	9.500416
7.925583	562.250716	9.505434
7.511563	579.285544	9.510451
7.728854	573.691593	9.515469
8.104738	581.987098	9.520487
7.597277	585.160481	9.525504
8.163384	598.915730	9.530522
7.848526	571.770827	9.535539
7.690240	567.629301	9.540557
7.723468	571.131517	9.545575
7.392592	566.983779	9.550592
7.803259	569.718406	9.555610
7.930324	593.170853	9.560627
8.120766	593.539503	9.565645
8.207463	587.059608	9.570663
7.780202	570.006928	9.575680
7.903558	576.145078	9.580698
7.695834	596.902059	9.585715
7.696853	577.220159	9.590733
8.027235	604.767289	9.595751
7.762209	579.203260	9.600768
7.387344	581.823089	9.605786
7.739014	593.998479	9.610803
7.847744	609.875205	9.615821
7.961043	587.295918	9.620839
7.768933	584.712789	9.625856
7.920935	577.071544	9.630874
7.852081	606.242482	9.635891
7.598513	606.636982	9.640909
7.962564	589.222671	9.645927
7.800353	589.116481	9.650944
8.111281	586.258837	9.655962
7.861703	604.176496	9.660979
7.576866	611.176679	9.665997
8.430202	615.282933	9.671015
8.279666	609.271837	9.676032
8.406435	596.225737	9.681050
8.195524	584.224149	9.686067
8.042675	592.865428	9.691085
8.165618	597.719172	9.696103
7.848855	596.714275	9.701120
8.088360	572.115108	9.706138
7.772870	580.011527	9.711155
7.942973	586.670547	9.716173
8.188751	610.856635	9.721191
7.842189	594.482624	9.726208
8.028879	578.558150	9.731226
7.993315	605.067246	9.736243
8.054353	612.300445	9.741261
8.311050	596.374125	9.746279
8.180567	594.061046	9.751296
8.208814	602.882087	9.756314
7.934304	601.241347	9.761331
8.169974	595.194971	9.766349
8.072773	607.115508	9.771367
7.941869	609.582654	9.776384
8.222913	598.173288	9.781402
8.103081	610.619569	9.786419
7.962906	626.177213	9.791437
8.290695	622.617069	9.796455
8.064049	635.093912	9.801472
8.274583	643.243692	9.806490
8.334915	634.983788	9.811507
8.359429	636.719250	9.816525
8.537018	631.719176	9.821543
8.545383	614.602525	9.826560
8.305374	608.147288	9.831578
8.199962	602.886991	9.836595
7.986909	589.352523	9.841613
8.175340	594.679757	9.846631
7.997322	617.886875	9.851648
8.485703	616.586072	9.856666
8.488205	611.858768	9.861683
8.180006	608.704826	9.866701
8.155350	621.873173	9.871719
8.416200	630.550310	9.876736
8.406222	603.960110	9.881754
8.367548	606.833157	9.886771
8.290234	611.555283	9.891789
8.663458	604.135267	9.896807
7.959311	601.763194	9.901824
8.004404	595.888725	9.906842
8.337948	616.417148	9.911859
8.106543	638.015265	9.916877
8.332709	627.894020	9.921895
8.199201	620.928206	9.926912
8.578812	618.163015	9.931930
8.502777	631.459218	9.936947
8.262748	620.892330	9.941965
8.565004	620.664612	9.946983
8.437885	638.417331	9.952000
8.326814	635.996638	9.957018
8.663400	616.561511	9.962035
8.612801	623.170036	9.967053
8.561644	618.519197	9.972071
8.349519	618.868178	9.977088
8.659476	619.712018	9.982106
8.577664	628.701320	9.987123
8.082361	632.244156	9.992141
8.821204	616.483539	9.997159
8.680510	618.174569	10.002176
8.607327	624.919861	10.007194
8.433422	613.544734	10.012211
8.360486	612.907301	10.017229
8.410416	618.816232	10.022247
8.210473	616.952400	10.027264
8.646744	632.177354	10.032282
8.656329	625.317383	10.037299
8.564050	620.541781	10.042317
8.524373	621.750893	10.047335
8.539280	626.575073	10.052352
8.800949	625.729827	10.057370
8.539096	617.971967	10.062387
8.601326	612.887153	10.067405
8.762737	622.206921	10.072423
8.580980	632.284097	10.077440
8.290221	630.100719	10.082458
8.141148	627.606013	10.087475
8.268375	630.109322	10.092493
8.517980	616.328437	10.097511
8.474861	638.040674	10.102528
8.359002	636.822209	10.107546
8.454415	641.980532	10.112563
8.411520	637.235533	10.117581
8.330790	620.376839	10.122599
8.652867	637.257614	10.127616
8.632399	645.354849	10.132634
8.614754	648.219114	10.137651
8.173688	646.666114	10.142669
8.654062	652.401198	10.147687
8.572815	674.867908	10.152704
8.720536	666.706406	10.157722
8.780510	663.448216	10.162739
8.698220	660.421354	10.167757
8.942293	643.554711	10.172775
8.809941	656.178444	10.177792
8.624039	654.380673	10.182810
8.975232	643.392138	10.187827
8.856821	647.951429	10.192845
8.709762	651.959901	10.197863
8.594414	663.981979	10.202880
8.497799	661.955338	10.207898
8.847813	654.346275	10.212915
8.784139	645.408131	10.217933
8.747222	653.582676	10.222951
8.732398	656.949979	10.227968
8.736667	650.818822	10.232986
8.883567	641.352712	10.238003
8.559128	643.056596	10.243021
8.687525	649.521116	10.248039
8.632698	670.181000	10.253056
8.650414	664.060900	10.258074
9.211675	669.873640	10.263091
9.254767	673.721792	10.268109
8.903137	672.028649	10.273127
8.760827	650.368335	10.278144
8.742725	654.242732	10.283162
9.120047	655.585635	10.288179
8.676815	641.385119	10.293197
9.063812	632.845408	10.298215
9.040327	655.387560	10.303232
8.903563	669.280185	10.308250
8.917995	656.032382	10.313267
8.954064	659.053180	10.318285
9.101482	661.543514	10.323303
9.179158	657.265653	10.328320
9.073448	654.365266	10.333338
9.028631	657.947114	10.338355
8.700894	650.631698	10.343373
8.902024	659.016343	10.348391
9.340909	680.475707	10.353408
9.161410	666.108981	10.358426
9.028130	645.418664	10.363443
8.935654	666.105232	10.368461
8.952153	664.695943	10.373479
8.831944	664.333864	10.378496
9.203243	670.660738	10.383514
9.681858	675.245847	10.388531
9.184438	683.582704	10.393549
8.803147	664.400366	10.398567
8.982303	659.574287	10.403584
8.750540	654.639394	10.408602
9.038099	682.095344	10.413619
9.068393	690.999147	10.418637
9.291444	694.837736	10.423655
9.277077	692.415911	10.428672
9.107870	707.685110	10.433690
9.390103	697.663874	10.438707
9.448962	694.184760	10.443725
9.300419	679.736648	10.448743
9.336906	663.650541	10.453760
8.970149	663.536826	10.458778
9.178119	652.638373	10.463795
9.136965	656.084219	10.468813
9.226386	657.899877	10.473831
9.326820	672.652467	10.478848
9.004420	675.405334	10.483866
9.532548	668.037325	10.488883
9.102209	673.797559	10.493901
9.242435	702.156883	10.498919
9.356607	698.641470	10.503936
9.369241	682.701668	10.508954
9.369822	679.929733	10.513971
9.362417	665.365816	10.518989
9.306976	645.865648	10.524007
9.333108	658.846158	10.529024
9.110676	681.817572	10.534042
9.402767	673.741037	10.539059
9.141008	663.607612	10.544077
9.083662	683.942036	10.549095
9.136705	683.542076	10.554112
9.277715	697.652627	10.559130
9.307450	678.736900	10.564147
9.484071	669.470531	10.569165
9.387684	689.713115	10.574183
9.658526	685.164315	10.579200
9.300353	694.977656	10.584218
9.653480	682.017072	10.589235
9.737444	674.263336	10.594253
9.879554	679.064446	10.599271
9.584164	658.411332	10.604288
9.156386	664.113774	10.609306
9.541146	682.536273	10.614323
9.353658	675.814624	10.619341
9.542048	687.256947	10.624359
9.812951	687.395039	10.629376
9.485810	664.841979	10.634394
9.305799	650.932017	10.639411
9.000608	666.471315	10.644429
9.286838	683.519046	10.649447
9.314983	671.152185	10.654464
9.641548	682.510466	10.659482
9.700421	702.581485	10.664499
9.149228	698.746914	10.669517
9.396842	697.221201	10.674535
9.481215	681.202831	10.679552
9.527465	703.199522	10.684570
9.441137	684.311627	10.689587
9.556557	687.186381	10.694605
9.371864	699.800988	10.699623
9.481622	694.373149	10.704640
9.363467	712.559099	10.709658
9.217096	695.777784	10.714675
9.338386	694.536852	10.719693
9.440925	696.225480	10.724711
9.515025	704.054332	10.729728
9.544281	729.183721	10.734746
9.729022	719.719084	10.739763
9.529964	704.726002	10.744781
9.799101	710.724890	10.749799
9.811832	701.009731	10.754816
9.395447	716.843168	10.759834
9.738923	720.096662	10.764851
9.896219	716.859867	10.769869
9.488575	713.396934	10.774887
10.086078	717.177682	10.779904
9.818841	715.342965	10.784922
9.808675	707.830494	10.789939
9.608300	720.634175	10.794957
9.411014	722.386523	10.799975
9.619791	719.504408	10.804992
9.446513	720.555735	10.810010
9.685935	701.500730	10.815027
9.750452	706.969118	10.820045
9.640104	708.547003	10.825063
9.462080	724.434831	10.830080
9.731964	756.694399	10.835098
9.965116	755.423266	10.840115
10.050151	737.128375	10.845133
9.852793	745.041173	10.850151
10.032696	760.426602	10.855168
9.840340	774.138205	10.860186
10.093052	751.830143	10.865203
10.099006	726.263396	10.870221
9.739098	726.281288	10.875239
10.078210	724.045759	10.880256
9.738980	726.814504	10.885274
9.993145	724.921467	10.890291
10.112212	737.241779	10.895309
9.466620	719.720623	10.900327
9.971306	721.115298	10.905344
9.847957	741.119067	10.910362
10.084277	750.972449	10.915379
10.233116	745.578870	10.920397
9.984546	739.031318	10.925415
10.288021	746.835767	10.930432
10.328975	747.870191	10.935450
10.038750	729.582712	10.940467
9.854323	721.406504	10.945485
9.907224	717.398987	10.950503
10.410367	720.178973	10.955520
9.895866	715.851261	10.960538
9.784270	721.233042	10.965555
9.547169	751.458948	10.970573
9.788894	749.938237	10.975591
9.928885	746.482407	10.980608
9.768951	753.115157	10.985626
9.899319	755.959804	10.990643
10.021558	759.333113	10.995661
9.985210	767.600905	11.000679
10.062243	762.387153	11.005696
10.036718	755.211358	11.010714
10.172504	756.534655	11.015731
10.172035	759.811935	11.020749
10.202482	754.150791	11.025767
10.238752	737.437253	11.030784
10.378897	751.585979	11.035802
10.169595	761.669563	11.040819
10.358063	749.425809	11.045837
10.286054	746.427832	11.050855
10.450683	748.960993	11.055872
10.309662	763.887198	11.060890
10.064999	753.969037	11.065907
10.140244	748.277565	11.070925
9.781228	742.803195	11.075943
10.314660	768.491183	11.080960
10.397798	798.301956	11.085978
10.399869	785.307198	11.090995
10.426105	762.456683	11.096013
10.364279	767.599018	11.101031
10.597738	746.114594	11.106048
10.403842	751.648630	11.111066
10.231908	746.840200	11.116083
10.451183	756.402683	11.121101
10.538999	761.924508	11.126119
10.803148	752.549357	11.131136
10.412955	749.079793	11.136154
10.259983	743.889495	11.141171
10.644820	747.865785	11.146189
10.238868	750.436758	11.151207
10.373295	738.211882	11.156224
10.192189	742.523266	11.161242
10.293491	762.330629	11.166259
10.687284	743.818215	11.171277
9.912633	739.321636	11.176295
10.398771	757.354640	11.181312
10.291705	758.101504	11.186330
10.654871	766.883136	11.191347
10.903699	776.261465	11.196365
10.426016	773.163836	11.201383
10.347794	743.266964	11.206400
10.441554	747.746056	11.211418
10.434175	773.915742	11.216435
10.806856	773.057456	11.221453
10.498075	771.417441	11.226471
10.563209	789.646204	11.231488
10.520135	788.993595	11.236506
10.387242	788.418608	11.241523
10.557034	787.908037	11.246541
10.445353	795.328582	11.251559
10.619753	771.273669	11.256576
10.538687	775.945888	11.261594
10.663946	784.619346	11.266611
10.630997	778.499701	11.271629
10.773934	785.871080	11.276647
10.687432	769.473976	11.281664
10.517461	769.654817	11.286682
10.499686	788.323051	11.291699
10.916615	784.447630	11.296717
10.276826	787.751259	11.301735
10.710300	768.361428	11.306752
10.924272	781.817849	11.311770
10.763412	800.682828	11.316787
10.948857	771.679478	11.321805
10.609979	763.720157	11.326823
10.820836	775.207146	11.331840
10.873896	788.797814	11.336858
10.553071	793.619375	11.341875
10.874509	770.703533	11.346893
10.768736	771.719895	11.351911
10.717697	764.979299	11.356928
10.630358	792.533317	11.361946
10.904293	784.894745	11.366963
11.146843	763.653021	11.371981
11.089635	769.761557	11.376999
10.882101	779.075579	11.382016
10.755496	782.669889	11.387034
10.627370	775.510155	11.392051
10.794025	774.019068	11.397069
10.866881	784.372193	11.402087
10.907478	778.621493	11.407104
10.614991	777.137698	11.412122
10.726488	792.648213	11.417139
10.863331	781.859527	11.422157
10.596296	782.583628	11.427175
10.751997	797.053164	11.432192
11.320486	817.728121	11.437210
10.933850	814.599398	11.442227
10.952734	794.288056	11.447245
10.912033	815.202425	11.452263
11.207745	816.932942	11.457280
10.919945	787.642513	11.462298
10.725711	814.391425	11.467315
11.314051	817.410727	11.472333
11.046297	814.127748	11.477351
10.977640	803.501319	11.482368
11.111921	814.114222	11.487386
11.216113	830.181543	11.492403
11.283908	818.897978	11.497421
11.060529	796.157936	11.502439
11.207471	790.771936	11.507456
11.080351	783.679534	11.512474
10.816604	799.489012	11.517491
11.186306	799.642659	11.522509
11.089441	797.673703	11.527527
11.308364	817.962551	11.532544
11.306458	825.646686	11.537562
11.202384	826.637483	11.542579
11.224377	801.613779	11.547597
10.921415	801.667424	11.552615
10.712296	823.575521	11.557632
11.226002	822.777960	11.562650
11.131156	819.341636	11.567667
11.367414	818.780819	11.572685
11.374612	812.353031	11.577703
11.063059	827.333358	11.582720
11.552567	818.287954	11.587738
11.046337	802.697285	11.592755
11.269828	812.242772	11.597773
11.263183	824.240518	11.602791
11.030064	809.570495	11.607808
11.136124	801.146784	11.612826
11.172831	807.980464	11.617843
11.286599	821.961711	11.622861
11.326703	819.824191	11.627879
11.180781	832.619851	11.632896
11.244287	814.774960	11.637914
11.198270	827.180682	11.642931
11.137221	810.122515	11.647949
11.083683	836.791636	11.652967
11.136949	849.113368	11.657984
11.699094	830.666703	11.663002
11.507830	835.713652	11.668019
11.807920	844.509294	11.673037
11.512645	843.743579	11.678055
11.705421	839.945727	11.683072
11.797073	826.915860	11.688090
11.513918	803.645967	11.693107
11.300166	799.128017	11.698125
11.629791	817.322452	11.703143
11.504719	810.630379	11.708160
11.454669	806.849344	11.713178
11.259760	831.754500	11.718195
11.307374	820.787178	11.723213
11.679322	822.635476	11.728231
11.883959	846.416937	11.733248
11.772125	840.689140	11.738266
11.606624	829.634523	11.743283
11.751105	817.785874	11.748301
11.982911	822.699534	11.753319
11.500759	826.685495	11.758336
11.453245	817.787680	11.763354
11.351801	826.579019	11.768371
11.883194	827.015115	11.773389
11.743064	825.937913	11.778407
11.639056	818.863913	11.783424
11.731019	820.014584	11.788442
11.247133	831.408805	11.793459
11.716373	827.590360	11.798477
11.924460	842.958620	11.803495
11.597317	851.616351	11.808512
11.899118	844.759551	11.813530
11.784644	832.839935	11.818547
11.870904	826.706081	11.823565
12.070476	841.916242	11.828583
11.638014	823.171968	11.833600
11.307141	826.970768	11.838618
11.774359	823.987181	11.843635
11.512544	835.592967	11.848653
11.808300	854.140982	11.853671
11.605132	841.229786	11.858688
11.899978	829.304028	11.863706
11.839132	841.561662	11.868723
11.889909	838.862582	11.873741
11.848298	834.399322	11.878759
11.844818	842.237917	11.883776
11.827504	831.540795	11.888794
11.705212	843.887698	11.893811
11.672170	849.057775	11.898829
11.768251	846.199279	11.903847
11.767252	840.086334	11.908864
11.521042	836.330328	11.913882
11.399393	865.222865	11.918899
11.741179	873.274721	11.923917
12.217088	873.688009	11.928935
11.902357	864.812679	11.933952
12.127104	884.562015	11.938970
11.865139	880.468238	11.943987
12.359592	875.081557	11.949005
12.312590	857.127648	11.954023
12.228772	857.685783	11.959040
12.533057	865.860928	11.964058
12.348541	862.275479	11.969075
11.815478	857.395527	11.974093
11.975335	870.984658	11.979111
12.098496	876.469294	11.984128
12.381225	853.279189	11.989146
12.234406	875.076007	11.994163
11.960959	899.847146	11.999181
12.324608	880.507285	12.004199
12.265730	868.761378	12.009216
12.463865	858.436990	12.014234
12.111235	862.389551	12.019251
12.258074	859.073472	12.024269
12.367641	839.286509	12.029287
12.067184	828.532665	12.034304
12.338681	847.844028	12.039322
11.966014	868.142049	12.044339
12.128382	867.097214	12.049357
12.490326	855.119709	12.054375
12.368334	871.153309	12.059392
12.718317	876.662158	12.064410
12.486171	857.010854	12.069427
12.334658	851.517306	12.074445
12.348375	839.671455	12.079463
12.260777	834.809406	12.084480
12.172419	823.453342	12.089498
11.735013	837.681651	12.094515
12.030640	870.122589	12.099533
12.483116	882.470281	12.104551
12.550759	877.786840	12.109568
12.496282	883.899398	12.114586
12.351008	887.746752	12.119603
12.021442	891.793220	12.124621
12.641282	866.523997	12.129639
12.387028	888.649432	12.134656
12.487254	892.572230	12.139674
12.484155	880.402932	12.144691
12.500287	867.126721	12.149709
12.349022	869.859409	12.154727
12.219676	894.487761	12.159744
12.564416	886.279513	12.164762
12.457487	867.067619	12.169779
12.386752	871.056745	12.174797
12.316364	872.927276	12.179815
12.348330	886.624639	12.184832
12.303230	882.032054	12.189850
12.540155	898.938999	12.194867
12.530492	914.234682	12.199885
12.876202	903.921595	12.204903
12.418786	898.456443	12.209920
12.622640	903.994469	12.214938
12.803626	906.276789	12.219955
12.802083	917.552004	12.224973
12.906327	908.059226	12.229991
12.699834	892.540356	12.235008
12.578110	875.677528	12.240026
12.575447	880.048807	12.245043
12.731509	905.122794	12.250061
12.935922	896.435500	12.255079
12.623246	894.319861	12.260096
12.921831	895.206727	12.265114
12.821117	888.238225	12.270131
12.328626	901.514530	12.275149
12.611919	893.398203	12.280167
12.773341	913.855498	12.285184
12.788824	907.296414	12.290202
12.880881	891.106618	12.295219
12.544794	907.261736	12.300237
12.753636	898.871072	12.305255
12.545390	911.489942	12.310272
12.671151	910.487561	12.315290
12.528649	904.720922	12.320307
12.457357	917.197609	12.325325
12.765597	922.885277	12.330343
12.949137	930.852713	12.335360
13.039116	917.173116	12.340378
13.426566	931.534715	12.345395
12.994860	934.254326	12.350413
13.030207	897.917506	12.355431
12.595553	913.706834	12.360448
12.963107	925.084795	12.365466
13.041803	909.070077	12.370483
12.744187	940.197757	12.375501
13.217815	941.841914	12.380519
13.318469	936.833987	12.385536
13.097464	920.048525	12.390554
12.860325	918.154099	12.395571
12.841690	950.229434	12.400589
13.154837	952.623744	12.405607
13.139627	931.092974	12.410624
13.015731	925.164829	12.415642
13.095188	932.842362	12.420659
12.812919	945.494353	12.425677
13.407198	934.749422	12.430695
13.364692	925.908576	12.435712
13.349222	930.889900	12.440730
13.426232	946.735910	12.445747
13.490112	950.941528	12.450765
13.329655	925.870922	12.455783
13.247600	904.009297	12.460800
12.983891	895.228739	12.465818
13.079430	922.816139	12.470835
13.353134	928.275128	12.475853
13.483176	918.237571	12.480871
13.404693	946.069758	12.485888
13.180849	924.029817	12.490906
13.256468	932.108766	12.495923
13.129626	938.607125	12.500941
13.385729	931.236812	12.505959
13.185421	934.057616	12.510976
13.056785	934.992060	12.515994
13.221380	930.574595	12.521011
13.235437	943.696280	12.526029
13.358293	940.406582	12.531047
13.339831	925.395049	12.536064
13.336964	916.060187	12.541082
13.641302	922.247188	12.546099
13.411946	950.286750	12.551117
13.644740	938.734749	12.556135
13.595780	934.575253	12.561152
13.617720	930.655846	12.566170
13.350921	924.008695	12.571187
13.118291	936.940885	12.576205
13.638760	929.409986	12.581223
13.473308	918.279135	12.586240
13.416627	929.960415	12.591258
13.599184	935.595943	12.596275
13.290546	929.908607	12.601293
13.471496	912.496635	12.606311
13.779633	926.307015	12.611328
13.555318	945.433971	12.616346
13.620048	937.201319	12.621363
13.379958	935.317218	12.626381
13.342317	931.527311	12.631399
13.641058	940.461681	12.636416
13.708884	951.746711	12.641434
13.795532	955.539028	12.646451
13.743651	975.554711	12.651469
13.798904	985.823403	12.656487
13.722699	968.474627	12.661504
13.772204	952.732631	12.666522
13.815578	956.790497	12.671539
13.940392	979.202346	12.676557
13.830922	959.380085	12.681575
13.863623	935.652681	12.686592
13.697575	928.291027	12.691610
14.055356	952.886794	12.696627
13.563578	946.603598	12.701645
13.942555	940.358841	12.706663
14.225074	946.797131	12.711680
13.662694	949.696665	12.716698
13.690923	931.151449	12.721715
13.632226	949.391027	12.726733
13.816923	972.489345	12.731751
14.118484	969.825059	12.736768
13.808620	958.986479	12.741786
14.032964	940.489530	12.746803
13.875833	965.804597	12.751821
13.920815	972.522150	12.756839
14.100417	951.739272	12.761856
13.675099	956.563884	12.766874
13.842941	962.836238	12.771891
13.608932	985.183704	12.776909
13.935947	981.539672	12.781927
13.887050	955.942934	12.786944
13.934845	952.984454	12.791962
14.012702	960.220252	12.796979
14.116974	982.221925	12.801997
13.962349	959.145362	12.807015
14.125491	930.492553	12.812032
13.774342	955.768818	12.817050
13.881061	980.433573	12.822067
14.277900	995.223688	12.827085
13.921085	995.957028	12.832103
14.479997	1005.357070	12.837120
14.011471	996.968379	12.842138
13.999666	986.841944	12.847155
13.933909	993.162164	12.852173
14.298183	990.083578	12.857191
14.356684	986.830581	12.862208
14.238712	984.985826	12.867226
14.544228	984.293904	12.872243
14.638529	1001.653557	12.877261
14.382555	997.077778	12.882279
14.673760	983.029421	12.887296
14.159247	970.736647	12.892314
14.481374	986.604183	12.897331
14.407133	989.215629	12.902349
14.271057	981.035128	12.907367
14.238786	963.056226	12.912384
14.377205	982.694004	12.917402
14.982819	975.804552	12.922419
14.533772	953.829041	12.927437
14.475319	938.251318	12.932455
14.397052	948.553170	12.937472
13.951932	962.356798	12.942490
14.514677	969.453627	12.947507
14.224704	977.530336	12.952525
14.402953	981.094092	12.957543
14.815467	969.907543	12.962560
14.514113	989.493233	12.967578
14.570880	978.673853	12.972595
14.653091	990.145463	12.977613
14.680419	986.343330	12.982631
14.829731	1001.262327	12.987648
14.954098	990.588913	12.992666
14.761951	977.219105	12.997683
14.839595	958.658408	13.002701
14.688992	947.961879	13.007719
14.390239	952.776890	13.012736
14.226736	969.271765	13.017754
14.567780	979.411552	13.022771
14.629792	973.388017	13.027789
14.652177	989.498250	13.032807
15.134340	988.730691	13.037824
14.845090	998.257019	13.042842
15.022949	975.338031	13.047859
14.810678	956.146976	13.052877
14.704040	954.010760	13.057895
15.142498	957.348387	13.062912
14.429925	961.329952	13.067930
14.951647	941.395731	13.072947
14.946826	947.443627	13.077965
14.767702	963.714955	13.082983
14.875215	958.828789	13.088000
14.950512	954.018010	13.093018
14.790861	946.518219	13.098035
14.949288	972.153788	13.103053
14.890503	994.348131	13.108071
15.117054	979.835090	13.113088
14.449861	962.839038	13.118106
14.572958	991.038680	13.123123
14.823099	971.362829	13.128141
14.447420	990.482579	13.133159
14.921811	993.844387	13.138176
14.775819	984.125168	13.143194
14.815256	967.073639	13.148211
14.846832	971.806810	13.153229
14.987863	1000.865195	13.158247
14.975194	1001.604540	13.163264
14.814442	987.490746	13.168282
15.386008	1004.798395	13.173299
15.200656	997.378987	13.178317
15.088718	999.131825	13.183335
15.396049	983.267879	13.188352
15.184378	996.613479	13.193370
15.169658	1007.147917	13.198387
14.959722	986.329293	13.203405
14.877830	977.916373	13.208423
15.352653	1009.292923	13.213440
15.158368	1034.838867	13.218458
15.280334	1003.912321	13.223475
15.364104	1009.516970	13.228493
15.258077	1026.204620	13.233511
15.211682	1030.580020	13.238528
15.395125	1025.320845	13.243546
15.184782	1016.903941	13.248563
15.148652	999.676526	13.253581
15.126820	1008.882952	13.258599
15.422628	1022.901703	13.263616
15.064576	1014.038857	13.268634
15.146552	1001.337622	13.273651
15.618995	1004.787329	13.278669
15.161017	1018.000074	13.283687
15.390804	1008.778047	13.288704
15.247001	1019.311685	13.293722
15.459308	1023.515919	13.298739
15.578192	1010.957062	13.303757
15.515058	1021.264728	13.308775
15.452359	1012.437501	13.313792
15.527402	1017.250096	13.318810
15.509801	1007.304775	13.323827
15.350729	1012.305232	13.328845
15.100484	1017.203759	13.333863
15.497191	1029.332399	13.338880
15.475654	1059.433818	13.343898
15.817583	1051.354557	13.348915
15.751656	1025.121431	13.353933
15.587710	1024.765685	13.358951
16.126553	1034.002274	13.363968
15.791352	1025.551485	13.368986
15.731909	1014.340857	13.374003
15.990567	1006.288861	13.379021
15.456871	1019.869935	13.384039
15.765025	1002.124124	13.389056
15.830147	1006.679267	13.394074
15.822906	1004.607404	13.399091
16.176486	999.581965	13.404109
15.702136	1014.344459	13.409127
15.885355	1016.753069	13.414144
16.132786	1007.236468	13.419162
16.070613	1014.813857	13.424179
15.652557	1020.732681	13.429197
15.766792	1004.707069	13.434215
15.723452	1000.949969	13.439232
15.625150	1011.346686	13.444250
15.693280	1024.722233	13.449267
15.834790	1006.550233	13.454285
15.801004	997.873807	13.459303
16.113635	1003.925746	13.464320
15.785921	1026.497071	13.469338
15.658767	1015.946287	13.474355
16.164026	1011.405196	13.479373
15.999018	1033.361898	13.484391
15.799509	1039.427514	13.489408
15.813860	1050.830187	13.494426
15.554633	1040.985587	13.499443
16.274451	1033.077612	13.504461
16.202099	1063.086182	13.509479
16.227044	1052.383890	13.514496
16.309548	1045.573574	13.519514
16.015136	1054.954862	13.524531
16.169879	1050.497958	13.529549
16.210182	1049.974043	13.534567
16.079949	1050.458084	13.539584
16.229422	1053.349518	13.544602
16.032103	1043.352989	13.549619
16.228886	1023.936539	13.554637
16.084694	1044.933440	13.559655
16.498803	1056.181199	13.564672
16.147242	1054.679882	13.569690
15.898747	1043.226822	13.574707
16.374145	1036.788283	13.579725
16.295354	1048.202410	13.584743
16.429499	1058.709331	13.589760
16.714127	1047.305927	13.594778
16.330620	1053.752483	13.599795
16.422664	1044.591475	13.604813
16.114037	1040.790334	13.609831
16.077273	1042.997270	13.614848
16.363976	1053.932996	13.619866
16.107270	1058.106113	13.624883
16.547784	1044.954940	13.629901
16.167374	1045.435749	13.634919
16.475839	1054.296943	13.639936
16.532599	1057.187070	13.644954
16.481308	1038.082076	13.649971
16.529586	1037.578590	13.654989
16.211377	1054.348371	13.660007
16.701341	1078.080482	13.665024
16.652475	1070.910758	13.670042
16.399064	1081.238691	13.675059
16.820503	1080.109405	13.680077
16.646725	1072.031224	13.685095
16.472404	1062.547879	13.690112
16.781047	1066.681592	13.695130
16.646518	1090.238155	13.700147
16.946604	1091.727687	13.705165
16.705380	1071.167302	13.710183
16.712524	1071.828788	13.715200
16.287160	1058.556982	13.720218
16.463936	1069.453321	13.725235
16.813485	1060.343525	13.730253
16.986501	1086.175152	13.735271
16.947981	1075.433050	13.740288
16.918709	1060.554929	13.745306
16.883389	1078.093236	13.750323
17.307490	1073.249082	13.755341
16.920863	1058.300720	13.760359
16.889470	1045.043918	13.765376
16.615643	1041.391317	13.770394
16.783574	1057.726129	13.775411
16.953799	1071.858864	13.780429
16.738461	1071.326715	13.785447
17.070582	1063.140631	13.790464
17.125827	1073.422668	13.795482
16.645604	1083.701886	13.800499
16.936685	1066.981500	13.805517
16.738456	1072.697817	13.810535
16.856146	1071.824582	13.815552
17.274838	1079.954762	13.820570
17.015740	1073.415497	13.825587
17.337628	1046.969930	13.830605
17.164435	1070.178118	13.835623
17.423705	1072.351192	13.840640
17.020810	1079.184627	13.845658
17.025044	1062.275587	13.850675
17.089031	1068.549797	13.855693
17.336017	1065.126497	13.860711
17.306332	1055.651332	13.865728
17.742317	1065.931748	13.870746
17.279611	1067.506202	13.875763
17.244489	1049.704396	13.880781
17.154558	1054.107072	13.885799
17.162697	1068.231953	13.890816
17.406219	1058.908339	13.895834
17.219505	1069.793112	13.900851
16.676510	1071.656455	13.905869
16.940422	1056.284330	13.910887
16.962742	1053.700813	13.915904
17.297258	1054.628000	13.920922
16.921574	1054.316593	13.925939
16.937717	1061.409723	13.930957
17.533291	1076.118466	13.935975
17.626484	1085.286347	13.940992
17.756099	1082.271713	13.946010
17.491222	1085.124371	13.951027
17.521398	1050.888897	13.956045
17.533196	1046.728579	13.961063
17.501215	1063.030603	13.966080
17.855824	1058.043548	13.971098
17.558878	1075.082112	13.976115
17.628793	1063.775777	13.981133
17.433925	1044.011308	13.986151
17.592588	1055.278156	13.991168
17.261895	1074.076777	13.996186
17.429590	1086.947169	14.001203
17.616684	1078.709078	14.006221
17.749579	1080.918684	14.011239
17.794363	1090.168860	14.016256
17.901580	1096.244450	14.021274
17.858408	1101.470702	14.026291
17.608415	1085.275824	14.031309
17.871140	1088.905645	14.036327
17.694475	1093.482763	14.041344
17.760606	1085.678630	14.046362
17.436388	1098.489709	14.051379
17.971770	1094.185781	14.056397
17.784372	1091.452511	14.061415
17.775221	1077.304430	14.066432
17.684177	1083.074182	14.071450
17.683720	1105.126008	14.076467
18.116171	1094.642592	14.081485
18.056129	1077.966050	14.086503
18.029692	1075.992602	14.091520
17.976846	1085.683607	14.096538
18.252190	1101.410999	14.101555
17.957971	1081.826736	14.106573
18.102709	1094.123513	14.111591
18.229347	1091.479355	14.116608
18.529773	1072.072358	14.121626
18.266316	1095.706423	14.126643
18.092635	1097.674149	14.131661
17.922346	1080.486427	14.136679
18.036646	1068.503925	14.141696
17.852503	1079.952607	14.146714
18.080758	1097.266124	14.151731
18.182499	1091.252902	14.156749
18.389731	1084.038784	14.161767
18.010995	1093.762690	14.166784
18.228673	1084.736763	14.171802
18.287511	1080.019193	14.176819
17.976316	1092.526713	14.181837
18.292675	1095.802679	14.186855
18.366883	1080.221782	14.191872
18.192799	1083.436507	14.196890
18.333751	1097.966723	14.201907
18.102285	1087.782843	14.206925
18.065206	1064.983865	14.211943
17.766789	1080.747505	14.216960
18.121633	1077.634741	14.221978
17.937298	1084.914026	14.226995
18.101221	1093.944665	14.232013
18.168263	1089.540225	14.237031
18.152946	1108.943202	14.242048
18.593330	1118.613334	14.247066
18.399475	1112.602507	14.252083
18.411130	1123.949395	14.257101
18.790516	1127.612984	14.262119
18.404563	1116.416190	14.267136
18.319342	1099.345753	14.272154
18.738188	1125.405358	14.277171
18.812545	1113.102337	14.282189
18.862211	1091.383793	14.287207
18.686490	1105.040888	14.292224
18.935853	1114.265537	14.297242
18.686499	1118.442080	14.302259
18.364188	1109.884612	14.307277
18.656790	1089.909341	14.312295
18.525692	1105.398469	14.317312
18.500541	1095.106492	14.322330
18.487942	1111.346324	14.327347
18.715251	1129.139934	14.332365
18.602075	1118.430705	14.337383
18.571568	1106.695965	14.342400
18.949396	1103.801882	14.347418
18.906844	1141.534208	14.352435
18.866821	1145.811860	14.357453
19.115499	1129.635389	14.362471
18.826306	1114.538619	14.367488
18.996305	1110.860184	14.372506
19.097121	1132.370345	14.377523
19.278554	1114.873341	14.382541
18.980670	1099.564000	14.387559
19.016602	1100.566511	14.392576
19.173782	1115.037087	14.397594
18.906575	1116.639165	14.402611
18.862521	1101.541356	14.407629
19.145644	1080.319056	14.412647
18.781450	1100.498691	14.417664
18.956015	1127.490672	14.422682
19.365507	1143.516037	14.427699
19.394529	1130.459459	14.432717
19.271787	1105.574404	14.437735
19.278379	1113.124832	14.442752
19.309350	1108.582879	14.447770
19.164628	1093.429292	14.452787
19.019293	1090.353033	14.457805
19.054907	1105.215644	14.462823
18.941071	1135.006193	14.467840
19.496910	1140.486826	14.472858
19.542309	1139.568560	14.477875
19.208171	1139.691121	14.482893
19.505710	1144.408832	14.487911
19.398617	1137.542918	14.492928
19.113040	1127.159246	14.497946
19.369674	1124.412912	14.502963
19.168703	1134.278782	14.507981
19.421170	1128.608657	14.512999
19.340548	1143.432458	14.518016
19.470025	1131.072983	14.523034
19.311194	1121.687016	14.528051
19.363616	1144.530652	14.533069
19.524515	1138.713391	14.538087
19.471902	1140.724486	14.543104
19.256688	1125.663599	14.548122
19.520463	1118.149247	14.553139
19.593804	1128.091898	14.558157
19.790235	1125.458637	14.563175
19.570908	1135.742696	14.568192
19.602056	1132.207644	14.573210
19.703890	1141.663234	14.578227
19.537352	1131.849505	14.583245
19.761935	1118.097791	14.588263
19.847032	1118.192006	14.593280
20.044110	1116.490693	14.598298
19.834304	1122.541832	14.603315
19.337218	1148.484795	14.608333
19.507851	1142.254510	14.613351
19.776393	1132.295475	14.618368
19.700794	1141.102009	14.623386
19.873513	1135.533129	14.628403
19.669993	1129.511593	14.633421
19.870500	1128.667572	14.638439
19.854685	1147.550238	14.643456
19.743578	1148.039190	14.648474
20.111090	1160.142648	14.653491
20.014695	1156.816222	14.658509
20.159464	1154.416536	14.663527
20.337853	1169.564005	14.668544
20.013852	1140.627123	14.673562
20.254806	1126.281306	14.678579
20.018658	1127.010945	14.683597
20.049630	1116.415067	14.688615
20.031364	1113.210941	14.693632
19.982943	1139.768158	14.698650
20.256295	1132.397555	14.703667
20.407250	1148.020090	14.708685
20.224148	1165.214406	14.713703
20.229819	1154.409742	14.718720
20.219903	1143.331646	14.723738
20.006804	1129.207184	14.728755
20.173438	1159.935441	14.733773
20.242371	1148.842540	14.738791
19.866684	1159.038309	14.743808
20.312091	1151.547947	14.748826
20.566925	1148.664637	14.753843
20.230425	1145.353980	14.758861
20.304150	1144.521856	14.763879
20.566881	1139.866810	14.768896
20.388036	1144.238448	14.773914
20.618159	1151.081942	14.778931
20.492260	1150.092204	14.783949
20.581598	1145.671665	14.788967
20.394156	1153.513662	14.793984
20.319704	1165.041305	14.799002
20.619177	1152.497851	14.804019
20.558289	1131.049329	14.809037
20.549336	1145.906652	14.814055
20.613015	1144.685930	14.819072
20.716173	1133.661086	14.824090
21.022848	1135.691232	14.829107
20.710658	1141.734796	14.834125
20.988720	1146.981090	14.839143
21.006293	1148.085924	14.844160
20.570346	1148.283858	14.849178
21.052050	1122.116697	14.854195
20.598848	1124.567126	14.859213
20.607414	1132.311480	14.864231
20.698118	1143.023031	14.869248
20.591863	1153.043397	14.874266
20.989407	1140.669725	14.879283
21.020797	1151.101587	14.884301
20.684046	1144.666046	14.889319
20.789274	1133.053111	14.894336
20.707732	1149.588756	14.899354
20.933283	1148.070188	14.904371
20.742825	1156.659550	14.909389
20.933840	1137.706763	14.914407
20.824050	1131.739503	14.919424
20.702285	1143.596916	14.924442
20.926455	1155.320615	14.929459
20.812171	1147.880435	14.934477
20.665081	1148.734793	14.939495
20.513742	1166.222311	14.944512
20.939593	1164.793348	14.949530
21.082340	1160.679551	14.954547
20.834598	1185.663386	14.959565
21.199347	1167.871721	14.964583
21.127174	1156.832244	14.969600
20.933838	1182.204131	14.974618
21.099474	1186.095827	14.979635
21.393477	1169.418242	14.984653
21.175868	1163.718037	14.989671
21.315017	1166.648395	14.994688
21.203482	1183.393708	14.999706
21.306293	1167.479826	15.004723
21.381474	1178.457092	15.009741
21.169976	1177.513380	15.014759
21.259159	1171.417282	15.019776
21.117026	1179.094854	15.024794
21.463475	1188.076197	15.029811
21.616381	1184.179166	15.034829
21.660728	1188.678755	15.039847
22.066905	1178.519232	15.044864
21.672803	1164.684821	15.049882
21.722065	1156.321864	15.054899
21.347974	1169.191035	15.059917
21.651877	1172.873801	15.064935
21.959567	1166.359207	15.069952
21.717569	1189.009498	15.074970
21.839203	1177.067913	15.079987
21.645697	1172.433344	15.085005
21.428900	1165.820135	15.090023
21.448283	1172.147024	15.095040
21.317364	1185.133267	15.100058
21.677663	1165.802064	15.105075
21.658368	1164.156970	15.110093
21.728680	1188.245639	15.115111
21.821066	1197.046782	15.120128
21.955326	1207.067782	15.125146
21.982219	1200.423537	15.130163
21.901934	1194.667466	15.135181
22.108600	1197.873414	15.140199
22.484129	1187.323966	15.145216
21.868510	1186.113654	15.150234
21.884191	1178.936263	15.155251
22.089993	1171.348021	15.160269
21.967574	1152.977887	15.165287
21.980183	1165.746644	15.170304
21.624428	1153.380055	15.175322
21.915069	1159.955840	15.180339
22.105617	1185.991185	15.185357
21.806970	1199.226364	15.190375
22.220282	1194.183611	15.195392
22.136334	1185.692982	15.200410
22.412055	1187.799886	15.205427
22.380093	1187.189606	15.210445
22.200655	1190.545263	15.215463
22.529263	1184.512816	15.220480
21.951916	1172.140126	15.225498
21.995474	1194.717650	15.230515
22.162926	1206.371548	15.235533
22.231312	1198.339284	15.240551
22.449454	1178.744125	15.245568
22.216454	1194.766396	15.250586
22.204133	1194.659342	15.255603
22.513238	1193.329571	15.260621
22.242981	1192.216773	15.265639
22.427893	1201.308164	15.270656
22.229171	1205.213730	15.275674
22.423698	1202.604091	15.280691
22.501068	1195.930843	15.285709
22.472363	1197.074128	15.290727
22.565809	1182.927100	15.295744
22.186223	1203.162648	15.300762
22.123945	1205.163246	15.305779
22.304664	1198.625931	15.310797
22.379486	1216.838154	15.315815
22.907397	1205.720728	15.320832
22.747471	1220.925535	15.325850
22.762682	1224.016509	15.330867
22.899898	1225.101183	15.335885
22.688882	1225.015845	15.340903
23.091271	1213.590594	15.345920
23.035568	1212.317959	15.350938
22.893887	1198.284460	15.355955
22.912226	1199.185874	15.360973
22.679211	1197.391493	15.365991
22.332169	1185.201743	15.371008
22.719660	1202.399716	15.376026
22.951496	1215.573223	15.381043
22.991327	1212.898027	15.386061
23.026855	1233.309248	15.391079
23.385970	1219.919371	15.396096
22.995433	1203.864101	15.401114
23.011265	1214.616316	15.406131
23.119528	1218.157745	15.411149
22.899805	1225.849835	15.416167
23.278183	1196.970551	15.421184
23.130612	1200.461559	15.426202
23.106487	1210.593164	15.431219
23.235181	1203.884665	15.436237
23.066353	1208.047629	15.441255
23.251481	1219.998151	15.446272
22.974517	1234.461962	15.451290
23.498119	1214.903758	15.456307
23.354757	1197.045472	15.461325
23.336816	1217.557809	15.466343
23.433024	1235.223245	15.471360
23.425958	1216.640219	15.476378
23.237848	1195.864146	15.481395
23.192187	1203.267681	15.486413
23.024918	1211.757693	15.491431
23.227899	1225.008892	15.496448
23.383491	1221.823836	15.501466
23.678483	1219.263619	15.506483
23.285725	1217.723140	15.511501
23.523608	1205.807488	15.516519
23.999548	1196.668262	15.521536
23.638388	1211.915564	15.526554
23.291509	1223.366449	15.531571
23.333968	1203.649343	15.536589
23.300006	1225.500237	15.541607
23.584792	1228.846986	15.546624
23.380875	1224.057269	15.551642
23.576333	1219.719542	15.556659
23.976191	1239.528174	15.561677
23.648503	1256.940535	15.566695
24.051987	1251.186662	15.571712
24.001032	1256.736027	15.576730
23.624930	1226.453484	15.581747
23.548413	1219.126980	15.586765
23.603732	1242.360938	15.591783
23.989827	1253.716696	15.596800
24.051480	1248.240620	15.601818
23.820953	1238.852948	15.606835
24.155212	1246.561152	15.611853
23.703608	1251.355365	15.616871
23.772996	1252.317522	15.621888
23.988760	1237.283015	15.626906
24.027331	1225.688504	15.631923
24.055476	1248.683320	15.636941
23.715457	1256.428860	15.641959
24.245648	1242.181165	15.646976
24.156846	1237.858723	15.651994
24.306387	1238.746624	15.657011
24.328427	1254.746098	15.662029
23.963640	1255.100639	15.667047
23.911906	1235.708925	15.672064
24.007599	1244.598307	15.677082
24.290686	1245.104974	15.682099
24.442876	1236.882603	15.687117
23.908393	1245.881144	15.692135
24.105506	1271.530897	15.697152
24.236569	1279.071563	15.702170
24.281818	1278.064358	15.707187
24.729456	1259.248203	15.712205
24.368296	1282.458057	15.717223
24.770236	1284.780380	15.722240
24.505911	1274.674820	15.727258
24.701063	1258.379430	15.732275
24.889288	1254.490223	15.737293
24.681721	1265.104531	15.742311
24.416588	1255.267361	15.747328
24.654709	1249.683695	15.752346
24.819852	1255.602469	15.757363
24.565790	1248.104650	15.762381
24.438293	1235.833411	15.767399
24.903132	1241.286315	15.772416
24.850363	1254.999094	15.777434
24.743287	1264.665323	15.782451
25.265696	1250.426779	15.787469
24.625848	1264.568887	15.792487
24.917877	1255.032660	15.797504
24.874052	1225.885672	15.802522
24.445798	1217.916675	15.807539
25.196589	1245.324640	15.812557
24.720887	1272.609824	15.817575
25.399201	1259.157028	15.822592
25.205152	1236.545802	15.827610
25.052742	1232.076331	15.832627
25.079777	1233.499512	15.837645
24.805794	1247.902425	15.842663
25.003862	1237.700894	15.847680
24.979939	1245.296873	15.852698
24.904958	1259.532691	15.857715
25.084132	1251.518991	15.862733
24.727503	1264.359673	15.867751
25.257266	1271.788888	15.872768
25.192882	1275.385528	15.877786
24.897460	1267.798395	15.882803
25.164938	1242.900389	15.887821
24.802724	1267.387552	15.892839
25.017376	1267.737360	15.897856
25.053490	1262.413791	15.902874
25.115415	1270.861433	15.907891
25.510032	1269.947246	15.912909
25.295826	1288.706806	15.917927
25.142851	1301.338609	15.922944
25.717892	1286.041089	15.927962
25.741629	1277.807942	15.932979
25.756727	1279.160873	15.937997
25.510930	1277.932143	15.943015
25.414559	1263.733555	15.948032
25.554385	1254.814465	15.953050
25.345135	1287.407916	15.958067
25.744393	1276.914315	15.963085
25.643809	1286.937964	15.968103
25.621708	1281.578251	15.973120
25.794164	1292.664691	15.978138
25.682492	1293.684620	15.983155
26.071837	1280.054317	15.988173
25.739096	1301.294023	15.993191
25.725491	1296.441936	15.998208
26.187762	1270.432027	16.003226
25.876444	1270.998842	16.008243
25.994216	1276.699914	16.013261
25.868857	1275.204687	16.018279
25.680579	1272.198858	16.023296
25.853418	1266.139673	16.028314
25.936366	1287.333199	16.033331
25.924830	1284.124776	16.038349
25.697779	1274.880568	16.043367
25.911003	1287.590098	16.048384
25.974655	1284.502684	16.053402
25.773295	1288.257659	16.058419
25.983533	1289.244366	16.063437
25.833946	1286.867326	16.068455
25.940197	1297.600622	16.073472
25.979698	1296.065160	16.078490
25.921842	1295.185695	16.083507
26.001386	1302.103932	16.088525
25.910845	1331.633593	16.093543
26.233651	1322.615542	16.098560
26.485291	1311.206766	16.103578
26.390672	1301.678513	16.108595
26.592556	1301.307865	16.113613
26.989956	1318.163073	16.118631
26.603934	1301.306649	16.123648
26.742319	1287.245875	16.128666
26.348975	1294.226216	16.133683
26.817208	1300.918251	16.138701
26.811771	1309.174142	16.143719
26.597594	1295.075485	16.148736
26.628672	1280.497930	16.153754
26.492934	1279.118859	16.158771
26.755895	1257.563209	16.163789
26.899852	1252.261773	16.168807
26.754479	1270.894019	16.173824
27.168622	1284.999338	16.178842
26.670570	1273.191474	16.183859
26.547389	1252.147963	16.188877
26.899796	1257.852862	16.193895
26.941736	1276.193986	16.198912
27.042072	1276.139557	16.203930
26.833471	1273.024908	16.208947
27.094966	1281.088184	16.213965
26.978775	1267.293954	16.218983
26.888119	1275.653455	16.224000
26.766227	1265.079980	16.229018
26.773091	1271.900693	16.234035
26.923011	1256.926150	16.239053
27.368016	1257.400844	16.244071
26.834459	1265.620787	16.249088
27.362655	1262.373459	16.254106
27.092567	1258.127316	16.259123
26.674647	1259.338271	16.264141
27.011590	1266.493712	16.269159
26.909526	1285.447580	16.274176
27.132982	1291.576561	16.279194
27.157099	1297.740356	16.284211
26.977675	1279.088220	16.289229
27.255984	1289.709732	16.294247
26.941919	1308.451968	16.299264
26.865423	1297.587570	16.304282
26.639765	1299.928589	16.309299
26.739061	1301.132206	16.314317
27.156415	1330.439580	16.319335
27.086854	1340.286426	16.324352
27.708583	1326.252508	16.329370
27.651841	1318.267821	16.334387
27.228184	1319.568684	16.339405
26.970414	1340.619817	16.344423
27.213327	1337.337747	16.349440
27.562243	1341.643186	16.354458
27.774182	1347.065891	16.359475
27.598151	1353.215747	16.364493
27.974386	1350.852960	16.369511
27.609128	1359.874870	16.374528
27.957825	1339.666138	16.379546
27.831835	1344.857253	16.384563
28.127609	1365.017128	16.389581
27.897223	1365.918129	16.394599
28.107893	1365.618059	16.399616
28.180262	1318.105438	16.404634
27.897602	1325.578702	16.409651
27.794863	1336.635767	16.414669
28.173478	1328.438710	16.419687
27.708107	1304.698280	16.424704
28.102545	1310.754831	16.429722
27.956015	1344.836311	16.434739
28.078468	1350.137026	16.439757
28.443533	1336.349798	16.444775
27.928793	1333.255912	16.449792
28.290613	1355.922190	16.454810
28.244073	1369.432021	16.459827
28.204287	1344.039773	16.464845
28.479446	1347.969206	16.469863
28.400240	1350.127996	16.474880
28.193009	1338.245159	16.479898
28.220935	1350.743392	16.484915
28.205259	1349.983302	16.489933
28.400378	1338.842054	16.494951
28.017040	1356.777877	16.499968
28.362561	1354.126729	16.504986
28.309299	1340.868265	16.510003
28.590862	1345.926790	16.515021
28.200327	1355.654090	16.520039
28.279716	1368.861974	16.525056
28.529128	1352.868076	16.530074
28.312527	1342.439303	16.535091
28.418646	1337.128247	16.540109
28.566483	1358.443303	16.545127
28.510868	1379.333158	16.550144
28.705635	1369.679401	16.555162
28.719335	1367.416965	16.560179
28.705775	1373.008705	16.565197
28.941196	1364.197152	16.570215
28.718587	1377.524915	16.575232
29.214922	1375.413376	16.580250
29.016640	1366.853963	16.585267
28.804690	1372.314155	16.590285
29.081153	1374.587657	16.595303
28.898648	1381.306476	16.600320
29.144946	1370.031186	16.605338
29.347318	1357.140015	16.610355
29.123135	1350.552350	16.615373
29.191720	1319.285027	16.620391
29.024546	1348.329175	16.625408
29.079931	1339.612333	16.630426
29.021579	1345.535111	16.635443
28.988915	1373.063033	16.640461
29.297964	1373.110991	16.645479
28.914538	1366.330689	16.650496
29.107382	1360.867039	16.655514
29.215815	1356.190979	16.660531
28.977365	1360.071464	16.665549
29.193350	1367.010578	16.670567
28.966367	1369.762559	16.675584
29.427401	1352.329781	16.680602
29.452009	1372.404292	16.685619
29.353571	1374.077203	16.690637
29.490302	1355.516002	16.695655
29.220827	1360.847441	16.700672
29.240121	1394.070028	16.705690
29.536022	1409.262671	16.710707
29.556023	1410.194918	16.715725
29.900292	1388.100866	16.720743
29.688850	1391.196168	16.725760
29.639385	1403.722683	16.730778
29.756010	1405.432187	16.735795
29.701871	1392.227552	16.740813
29.962925	1373.888051	16.745831
29.909333	1388.207639	16.750848
29.833874	1380.547789	16.755866
30.122086	1388.596177	16.760883
29.945611	1391.593202	16.765901
30.143054	1397.956984	16.770919
29.957601	1397.036606	16.775936
30.178728	1390.133559	16.780954
30.250150	1386.426280	16.785971
30.047696	1380.999214	16.790989
30.001284	1391.449411	16.796007
29.587706	1397.857191	16.801024
29.910262	1392.733822	16.806042
30.137426	1370.630808	16.811059
30.002680	1388.449718	16.816077
30.085854	1402.297116	16.821095
29.912786	1391.848814	16.826112
29.991436	1387.064602	16.831130
30.140523	1397.248199	16.836147
30.130287	1419.784564	16.841165
30.522388	1434.485951	16.846183
30.638428	1422.747120	16.851200
30.548136	1411.438073	16.856218
30.825045	1412.721575	16.861235
30.643691	1421.516226	16.866253
30.639148	1397.517649	16.871271
30.103315	1381.455107	16.876288
30.529663	1385.998985	16.881306
30.820706	1398.997746	16.886323
30.809498	1397.202014	16.891341
30.781555	1404.835146	16.896359
30.460247	1401.093967	16.901376
30.680146	1401.787715	16.906394
31.003892	1392.952299	16.911411
30.709149	1403.434489	16.916429
30.496012	1412.282506	16.921447
30.917816	1405.235586	16.926464
30.908724	1400.553055	16.931482
30.936971	1390.584951	16.936499
30.839509	1416.898646	16.941517
30.994283	1419.104981	16.946535
31.003091	1410.874427	16.951552
30.874661	1394.911535	16.956570
31.009287	1394.514803	16.961587
30.586782	1412.533327	16.966605
30.679051	1396.354278	16.971623
31.066704	1411.107350	16.976640
31.253084	1393.459146	16.981658
31.231359	1413.970010	16.986675
31.006959	1418.538679	16.991693
31.360070	1400.254391	16.996711
31.210595	1401.523530	17.001728
31.094643	1424.632462	17.006746
31.494792	1432.242195	17.011763
31.437692	1432.442766	17.016781
31.552207	1420.149000	17.021799
31.592310	1421.525167	17.026816
31.324028	1431.733380	17.031834
31.543154	1436.786705	17.036851
31.493353	1432.937772	17.041869
31.608543	1433.000349	17.046887
31.979705	1435.151936	17.051904
31.871191	1426.285102	17.056922
31.681927	1412.657998	17.061939
31.448074	1425.813291	17.066957
31.624495	1418.158736	17.071975
31.656014	1413.427571	17.076992
31.420908	1423.384288	17.082010
31.665595	1431.122444	17.087027
31.564139	1443.416693	17.092045
31.659661	1415.938159	17.097063
31.744607	1425.826440	17.102080
31.515875	1417.205805	17.107098
31.694177	1424.541735	17.112115
31.472851	1442.928139	17.117133
31.942355	1461.094028	17.122151
32.184600	1466.480475	17.127168
31.975003	1466.458173	17.132186
32.501440	1438.504049	17.137203
32.050635	1460.531226	17.142221
32.209948	1466.375176	17.147239
32.441388	1462.965871	17.152256
32.347501	1453.917019	17.157274
32.581855	1437.808913	17.162291
32.432694	1459.944768	17.167309
32.251983	1457.569597	17.172327
31.951984	1442.561867	17.177344
32.282269	1439.750759	17.182362
32.569073	1446.117014	17.187379
32.370124	1450.985553	17.192397
32.724913	1443.541515	17.197415
32.692712	1431.821959	17.202432
32.607422	1444.789566	17.207450
32.612986	1439.562499	17.212467
32.696432	1440.256066	17.217485
32.613279	1454.445789	17.222503
32.476013	1451.550563	17.227520
32.290367	1450.598822	17.232538
32.509861	1454.139145	17.237555
32.645732	1455.362905	17.242573
32.562849	1453.214821	17.247591
32.979672	1478.572766	17.252608
32.750200	1499.741854	17.257626
32.981334	1478.320161	17.262643
33.044482	1465.487036	17.267661
32.981793	1483.712953	17.272679
32.994907	1485.524002	17.277696
33.093937	1475.030185	17.282714
33.232721	1457.504117	17.287731
33.286978	1478.531330	17.292749
33.189453	1478.179947	17.297767
33.570516	1484.449852	17.302784
32.936354	1466.035296	17.307802
33.305718	1457.536716	17.312819
33.477183	1476.826734	17.317837
33.173305	1475.976303	17.322855
33.236939	1477.062233	17.327872
33.266150	1485.704138	17.332890
33.420340	1486.249335	17.337907
33.435118	1482.034776	17.342925
33.473193	1481.706250	17.347943
33.370766	1468.392921	17.352960
33.482851	1475.710100	17.357978
33.557798	1476.219977	17.362995
33.435011	1486.428291	17.368013
33.458396	1475.862840	17.373031
33.759541	1454.130858	17.378048
33.303417	1475.611618	17.383066
34.017742	1474.229029	17.388083
33.989150	1467.234961	17.393101
34.064636	1467.565360	17.398119
34.053937	1470.414265	17.403136
34.024236	1487.717027	17.408154
34.211928	1479.874695	17.413171
34.026443	1471.348238	17.418189
33.707356	1460.090249	17.423207
33.892886	1468.902037	17.428224
33.844015	1460.776045	17.433242
34.021601	1461.872369	17.438259
33.989765	1475.402989	17.443277
33.935370	1474.689931	17.448295
34.077343	1462.846511	17.453312
33.922153	1446.329943	17.458330
34.282585	1465.066100	17.463347
33.853497	1489.861354	17.468365
34.120192	1494.523164	17.473383
34.334347	1479.078245	17.478400
33.880425	1487.981054	17.483418
34.005885	1497.333965	17.488435
34.430681	1500.104414	17.493453
34.419982	1492.439612	17.498471
34.424594	1475.594210	17.503488
34.306256	1497.218151	17.508506
34.449913	1493.018603	17.513523
34.196590	1484.378377	17.518541
34.303848	1503.469440	17.523559
34.216518	1520.164182	17.528576
34.481807	1533.646835	17.533594
34.715135	1522.603251	17.538611
34.398156	1513.883784	17.543629
34.590068	1503.789271	17.548647
34.888430	1518.133182	17.553664
34.833055	1524.003579	17.558682
35.133882	1504.029952	17.563699
34.888024	1500.962152	17.568717
34.698512	1518.288406	17.573735
34.948262	1528.556615	17.578752
34.876137	1535.593801	17.583770
35.109423	1522.383475	17.588787
35.372381	1524.746417	17.593805
35.390492	1534.278867	17.598823
35.378982	1508.410222	17.603840
35.047995	1516.770799	17.608858
35.350211	1520.817333	17.613875
35.442178	1517.205229	17.618893
35.314724	1497.209296	17.623911
35.603807	1488.340979	17.628928
35.496608	1502.645424	17.633946
35.399905	1492.445104	17.638963
35.547169	1506.035308	17.643981
35.554193	1500.827560	17.648999
35.619355	1496.093958	17.654016
35.720152	1499.491148	17.659034
35.625650	1489.460114	17.664051
35.589707	1507.301212	17.669069
35.337087	1523.716156	17.674087
35.549155	1514.939864	17.679104
35.625381	1523.071475	17.684122
35.626033	1543.126748	17.689139
36.068438	1543.753424	17.694157
36.034228	1523.606251	17.699175
35.860183	1530.240094	17.704192
35.853833	1548.162256	17.709210
35.879929	1544.957400	17.714227
36.060449	1537.789305	17.719245
35.861073	1532.785992	17.724263
36.047201	1552.482844	17.729280
35.862205	1558.186232	17.734298
35.889157	1539.986378	17.739315
36.137354	1523.937495	17.744333
35.716306	1544.191070	17.749351
35.809023	1536.892832	17.754368
35.913617	1538.678634	17.759386
36.163114	1550.924420	17.764403
36.366053	1559.804923	17.769421
36.509516	1581.069251	17.774439
36.527985	1576.677520	17.779456
36.671374	1572.885780	17.784474
36.730510	1556.577126	17.789491
36.409713	1551.725241	17.794509
36.268520	1569.428917	17.799527
36.518727	1571.362374	17.804544
36.715337	1558.294171	17.809562
36.648258	1564.373953	17.814579
37.040867	1571.640392	17.819597
36.855476	1581.126006	17.824615
36.637866	1559.147193	17.829632
36.859768	1550.765922	17.834650
36.624834	1567.779237	17.839667
36.872339	1576.673640	17.844685
36.710202	1564.944457	17.849703
36.837074	1546.356412	17.854720
36.949736	1559.493624	17.859738
36.685940	1571.813031	17.864755
37.165224	1553.202757	17.869773
36.667759	1572.316493	17.874791
37.244730	1560.523429	17.879808
36.795627	1565.617948	17.884826
36.666668	1557.776833	17.889843
37.236003	1555.005415	17.894861
36.951705	1571.308249	17.899879
37.088009	1576.978229	17.904896
37.412951	1607.127113	17.909914
37.424172	1596.195853	17.914931
37.460722	1587.984335	17.919949
37.348348	1583.367329	17.924967
37.705817	1593.543289	17.929984
37.489697	1599.250949	17.935002
37.170436	1595.892175	17.940019
37.680451	1578.827344	17.945037
37.367117	1586.877530	17.950055
37.535335	1577.961630	17.955072
37.932554	1570.281927	17.960090
37.478411	1575.999687	17.965107
37.551949	1578.967143	17.970125
37.491932	1592.186154	17.975143
37.631416	1585.073529	17.980160
37.740882	1593.815200	17.985178
38.013803	1588.415779	17.990195
38.589475	1600.899668	17.995213
38.656223	1605.233607	18.000231
38.496237	1592.154141	18.005248
38.482530	1583.630133	18.010266
38.556369	1573.397935	18.015283
38.538501	1556.843892	18.020301
38.305022	1577.064842	18.025319
38.161252	1576.370879	18.030336
38.279413	1568.115183	18.035354
38.211459	1567.236682	18.040371
38.522081	1568.431672	18.045389
38.468520	1580.789459	18.050407
38.685010	1566.594092	18.055424
38.348364	1559.625992	18.060442
38.435413	1573.023888	18.065459
38.654153	1576.446182	18.070477
38.333760	1557.277551	18.075495
38.227319	1569.792756	18.080512
38.607699	1566.920603	18.085530
38.551866	1583.359083	18.090547
38.841922	1561.238315	18.095565
38.611779	1576.403809	18.100583
38.638607	1567.631234	18.105600
38.761044	1573.606194	18.110618
38.548837	1554.905902	18.115635
38.649971	1550.786676	18.120653
38.421300	1569.138429	18.125671
38.473870	1602.599717	18.130688
38.756641	1596.615030	18.135706
38.609882	1588.661708	18.140723
39.008196	1593.342930	18.145741
38.835526	1610.950303	18.150759
38.904604	1604.108007	18.155776
39.401279	1601.209938	18.160794
39.253710	1612.004393	18.165811
39.467102	1613.655813	18.170829
38.990763	1632.608587	18.175847
39.133672	1619.989958	18.180864
39.537432	1610.688044	18.185882
39.318410	1623.657237	18.190899
39.546183	1637.606516	18.195917
39.790942	1626.456955	18.200935
39.727387	1618.912218	18.205952
39.662645	1612.529538	18.210970
39.403385	1615.738866	18.215987
39.733938	1631.341665	18.221005
39.571914	1621.985044	18.226023
39.837595	1617.683622	18.231040
40.064028	1613.911212	18.236058
39.659545	1613.510966	18.241075
39.947360	1607.531641	18.246093
39.724554	1632.924398	18.251111
39.612005	1633.347574	18.256128
39.690505	1624.337933	18.261146
39.726579	1618.441141	18.266163
39.845725	1616.021707	18.271181
39.992318	1623.309440	18.276199
39.588306	1625.381522	18.281216
40.042338	1614.777774	18.286234
40.034378	1642.468008	18.291251
40.306510	1652.606055	18.296269
40.205208	1645.545295	18.301287
40.428970	1656.653338	18.306304
40.609026	1661.026726	18.311322
40.220906	1666.416844	18.316339
40.331199	1642.685755	18.321357
40.329000	1650.496508	18.326375
40.236118	1634.502102	18.331392
40.328184	1642.529901	18.336410
40.362491	1646.000795	18.341427
40.691767	1656.850803	18.346445
40.551237	1646.465143	18.351463
40.540323	1644.542195	18.356480
40.633441	1655.437132	18.361498
40.889685	1677.541929	18.366515
41.169293	1687.505670	18.371533
40.925824	1676.982505	18.376551
40.945954	1660.198792	18.381568
41.124490	1660.824305	18.386586
41.204307	1673.393836	18.391603
41.028952	1648.551918	18.396621
41.034268	1651.346645	18.401639
40.772306	1666.294305	18.406656
41.380175	1663.461001	18.411674
41.220579	1663.802601	18.416691
41.320458	1667.321706	18.421709
41.259180	1662.061622	18.426727
41.040819	1668.608773	18.431744
41.609570	1677.259440	18.436762
41.401026	1660.649116	18.441779
41.980005	1646.476236	18.446797
41.814740	1650.628005	18.451815
41.527490	1659.923851	18.456832
41.830544	1657.940652	18.461850
41.376430	1654.360009	18.466867
41.686294	1669.137700	18.471885
41.453789	1666.212117	18.476903
41.317165	1654.049606	18.481920
41.488696	1642.030826	18.486938
41.558720	1654.785189	18.491955
41.593670	1652.504144	18.496973
41.600511	1643.749196	18.501991
41.814664	1674.516001	18.507008
41.847097	1698.349979	18.512026
41.770660	1701.720411	18.517043
42.182050	1696.796588	18.522061
42.314829	1684.238623	18.527079
42.097237	1695.672430	18.532096
42.361543	1676.894228	18.537114
42.196232	1685.257433	18.542131
42.235989	1693.534305	18.547149
42.241747	1686.101873	18.552167
42.316400	1679.099602	18.557184
42.346038	1673.396626	18.562202
42.522886	1680.085516	18.567219
42.421198	1677.750291	18.572237
42.524356	1684.265966	18.577255
42.169391	1683.379879	18.582272
42.517675	1673.399050	18.587290
42.215968	1676.879621	18.592307
42.354138	1688.329913	18.597325
42.632475	1705.321540	18.602343
42.681282	1711.354676	18.607360
42.692853	1698.618837	18.612378
42.655620	1714.591292	18.617395
42.687551	1704.459318	18.622413
42.951388	1689.578005	18.627431
42.755704	1698.720779	18.632448
42.965639	1707.845535	18.637466
42.917532	1714.486494	18.642483
42.790838	1704.798265	18.647501
43.091896	1693.735985	18.652519
42.648810	1715.813422	18.657536
43.177482	1735.497793	18.662554
42.911705	1745.706292	18.667571
43.219852	1743.656014	18.672589
43.465519	1745.474816	18.677607
43.650339	1737.219625	18.682624
43.702828	1735.126969	18.687642
43.646469	1750.128904	18.692659
43.465718	1736.324648	18.697677
43.591006	1731.931654	18.702695
43.616590	1752.125374	18.707712
43.546087	1731.849405	18.712730
43.230619	1744.709073	18.717747
43.403005	1747.327815	18.722765
43.796171	1729.879452	18.727783
43.402510	1730.909993	18.732800
43.606973	1741.635933	18.737818
43.642031	1758.307168	18.742835
44.060304	1763.033265	18.747853
44.256818	1735.467404	18.752871
44.063908	1764.299413	18.757888
44.320317	1756.534543	18.762906
44.420085	1761.499061	18.767923
44.397973	1748.504923	18.772941
44.508203	1730.926973	18.777959
44.075685	1730.616182	18.782976
44.353151	1725.992080	18.787994
44.351495	1749.227958	18.793011
44.343056	1736.863625	18.798029
44.392223	1729.289283	18.803047
44.503940	1744.822575	18.808064
44.685032	1761.651041	18.813082
44.276160	1773.299746	18.818099
44.720546	1762.357699	18.823117
44.974173	1744.473122	18.828135
44.560821	1754.624830	18.833152
44.833806	1748.508560	18.838170
44.809343	1763.290518	18.843187
44.671009	1759.130411	18.848205
44.713705	1756.900619	18.853223
44.622122	1750.403444	18.858240
44.729073	1729.829703	18.863258
44.967422	1749.110784	18.868275
44.814585	1768.199794	18.873293
45.145283	1757.155401	18.878311
44.911950	1747.830562	18.883328
44.896042	1738.181964	18.888346
45.290360	1752.126558	18.893363
45.284471	1770.306528	18.898381
45.456096	1770.896680	18.903399
45.433017	1788.997443	18.908416
45.514700	1788.230296	18.913434
45.614806	1776.435276	18.918451
45.636220	1769.495195	18.923469
45.658011	1754.337248	18.928487
45.364100	1740.263361	18.933504
45.210108	1767.790985	18.938522
45.442514	1779.512032	18.943539
45.580702	1768.638293	18.948557
45.774363	1767.062941	18.953575
45.654058	1780.824450	18.958592
45.577201	1782.280693	18.963610
45.537187	1776.021588	18.968627
45.451015	1773.430096	18.973645
45.839448	1778.771930	18.978663
45.579061	1797.694142	18.983680
45.910226	1806.652792	18.988698
46.269065	1815.100184	18.993715
46.097817	1801.230236	18.998733
46.121315	1785.079855	19.003751
46.087952	1807.610968	19.008768
45.934074	1812.027381	19.013786
46.351097	1796.672511	19.018803
45.920468	1803.685911	19.023821
46.517047	1796.959468	19.028839
46.343929	1805.994169	19.033856
46.527508	1811.093052	19.038874
46.683230	1823.354553	19.043891
46.437374	1837.780629	19.048909
46.717339	1810.578720	19.053927
46.393289	1823.689330	19.058944
46.632339	1832.354322	19.063962
47.110963	1838.043996	19.068979
46.996642	1845.605319	19.073997
46.937346	1839.250675	19.079015
46.905228	1834.726214	19.084032
47.057392	1823.068295	19.089050
47.026945	1826.206987	19.094067
46.976606	1820.617646	19.099085
46.969565	1817.922340	19.104103
47.009198	1830.211690	19.109120
47.104282	1820.930252	19.114138
47.212593	1823.147768	19.119155
47.000670	1831.080064	19.124173
47.080857	1818.244615	19.129191
46.931992	1825.895774	19.134208
47.631802	1828.433670	19.139226
47.612038	1846.291580	19.144243
47.442766	1861.285123	19.149261
47.748094	1835.482540	19.154279
47.551658	1831.737643	19.159296
47.549981	1835.570951	19.164314
47.699799	1854.229618	19.169331
47.406480	1857.094497	19.174349
47.796670	1832.382696	19.179367
48.006959	1842.254076	19.184384
47.469776	1852.682953	19.189402
47.775084	1845.707240	19.194419
47.690123	1843.192982	19.199437
48.002113	1848.713680	19.204455
48.072821	1862.028818	19.209472
48.501626	1889.683339	19.214490
48.539118	1863.480372	19.219507
48.234243	1855.814699	19.224525
48.670209	1856.371012	19.229543
48.542948	1869.837648	19.234560
48.571062	1864.854199	19.239578
48.427511	1848.202917	19.244595
48.131113	1845.535447	19.249613
48.347377	1855.277331	19.254631
48.185628	1870.978752	19.259648
48.377845	1868.726695	19.264666
48.896687	1856.817544	19.269683
48.349718	1876.652591	19.274701
48.504910	1872.834422	19.279719
48.606774	1868.572695	19.284736
48.580009	1862.628331	19.289754
48.276866	1851.383654	19.294771
48.419422	1876.268593	19.299789
49.047689	1895.776016	19.304807
49.171310	1895.509019	19.309824
48.992086	1903.596055	19.314842
49.340899	1883.913651	19.319859
49.143836	1890.674066	19.324877
49.311197	1895.817874	19.329895
49.553217	1901.265033	19.334912
49.127937	1892.196880	19.339930
49.310516	1892.443561	19.344947
49.075340	1902.469976	19.349965
49.281648	1883.013543	19.354983
49.469591	1874.176283	19.360000
49.363416	1899.979257	19.365018
49.692570	1911.997153	19.370035
49.630775	1913.248498	19.375053
49.587207	1924.480425	19.380071
49.739031	1934.049382	19.385088
49.499834	1923.406073	19.390106
49.690040	1908.591922	19.395123
49.852485	1911.946739	19.400141
49.841830	1922.055529	19.405159
49.973128	1916.528639	19.410176
49.810667	1926.615184	19.415194
49.948638	1926.269944	19.420211
50.346771	1934.454857	19.425229
50.280961	1917.257882	19.430247
50.255547	1929.655975	19.435264
50.309402	1945.248629	19.440282
50.877082	1946.649451	19.445299
50.346772	1936.136310	19.450317
50.662761	1930.507746	19.455335
50.760233	1940.550265	19.460352
50.619811	1929.349788	19.465370
50.309728	1920.331269	19.470387
50.495009	1942.610941	19.475405
50.845080	1938.233390	19.480423
51.019854	1929.917268	19.485440
50.661540	1937.899789	19.490458
50.930640	1952.659889	19.495475
51.031197	1940.184485	19.500493
50.885339	1929.575246	19.505511
51.066293	1939.933629	19.510528
50.900196	1946.288832	19.515546
51.083918	1928.239643	19.520563
50.871975	1941.293941	19.525581
50.901199	1940.044506	19.530599
50.997494	1938.488475	19.535616
51.050596	1950.125132	19.540634
51.665151	1965.573388	19.545651
51.423300	1977.424622	19.550669
51.363403	1978.030113	19.555687
51.504022	1979.092040	19.560704
51.598486	1973.620026	19.565722
51.609962	1963.577957	19.570739
51.648619	1975.117827	19.575757
51.425270	1967.857641	19.580775
51.622955	1967.203376	19.585792
51.639897	1985.519467	19.590810
51.807731	1965.099788	19.595827
51.704800	1962.089953	19.600845
51.663301	1969.228948	19.605863
52.030101	1980.926465	19.610880
52.030231	1991.899300	19.615898
52.171902	1986.587558	19.620915
52.225506	1988.861669	19.625933
52.403092	2004.645019	19.630951
52.670204	1999.161883	19.635968
52.502480	1994.917610	19.640986
52.628610	1962.176061	19.646003
52.476493	1967.101283	19.651021
52.622778	1964.677605	19.656039
52.612881	1948.786064	19.661056
52.270960	1964.422687	19.666074
52.675319	1976.245170	19.671091
52.941990	1975.253485	19.676109
52.941985	1984.519279	19.681127
53.002487	1986.856609	19.686144
52.624171	2004.748762	19.691162
52.923559	1995.605472	19.696179
52.664896	1984.498496	19.701197
52.934005	1974.716544	19.706215
52.908085	1987.563009	19.711232
52.926918	1979.755609	19.716250
52.838461	1973.611200	19.721267
53.031563	1969.390756	19.726285
52.847820	1988.779284	19.731303
53.191507	2003.320946	19.736320
53.136615	2027.246622	19.741338
53.486156	2011.572044	19.746355
53.439692	2008.391481	19.751373
53.549473	2016.354159	19.756391
53.555826	2008.020658	19.761408
53.310186	2017.963264	19.766426
53.439044	2020.597315	19.771443
53.634452	2026.265174	19.776461
53.466103	2020.735508	19.781479
53.689045	2015.589624	19.786496
53.741303	2055.270371	19.791514
53.714645	2056.171103	19.796531
53.781138	2055.804509	19.801549
54.010412	2033.738472	19.806567
54.110610	2029.457689	19.811584
53.981149	2040.196902	19.816602
53.896414	2048.486666	19.821619
54.095196	2045.219317	19.826637
54.440713	2034.370862	19.831655
54.731023	2059.059764	19.836672
54.425529	2068.563754	19.841690
54.830213	2050.588517	19.846707
54.600637	2028.222890	19.851725
54.331001	2043.296865	19.856743
54.745518	2051.842550	19.861760
54.809951	2051.093100	19.866778
54.884077	2060.508275	19.871795
54.747995	2045.277034	19.876813
54.832829	2051.531277	19.881831
54.984042	2054.705536	19.886848
54.966437	2054.953613	19.891866
54.728662	2062.533673	19.896883
55.106922	2053.373280	19.901901
55.090664	2047.755196	19.906919
55.297480	2053.983378	19.911936
55.071451	2066.707101	19.916954
55.444876	2044.162587	19.921971
55.255270	2057.456062	19.926989
55.122867	2065.642807	19.932007
55.494965	2046.384616	19.937024
55.388207	2031.964925	19.942042
55.250555	2072.319007	19.947059
55.510076	2080.256285	19.952077
55.358955	2075.702215	19.957095
55.741359	2055.803351	19.962112
55.827159	2067.605233	19.967130
55.710984	2086.569803	19.972147
55.729633	2076.810577	19.977165
55.704995	2065.093026	19.982183
55.864437	2073.324641	19.987200
55.706945	2084.157772	19.992218
55.941133	2095.114341	19.997235
56.309501	2087.244993	20.002253
56.084079	2083.115229	20.007271
56.343037	2095.731179	20.012288
56.562279	2113.402589	20.017306
56.376399	2104.479753	20.022323
56.551104	2102.013667	20.027341
56.460760	2099.682506	20.032359
56.645503	2107.176726	20.037376
56.726125	2108.981220	20.042394
56.563931	2093.165278	20.047411
56.850489	2087.222780	20.052429
56.416806	2116.983167	20.057447
56.535521	2095.481078	20.062464
56.394559	2088.278368	20.067482
56.411889	2090.714956	20.072499
57.029769	2100.198637	20.077517
56.762522	2127.896874	20.082535
57.279212	2132.668820	20.087552
57.350402	2132.833045	20.092570
57.310192	2126.229010	20.097587
57.002911	2123.778014	20.102605
56.773089	2117.711622	20.107623
57.259212	2135.342103	20.112640
57.825112	2128.004557	20.117658
57.686727	2134.418928	20.122675
57.940366	2143.308515	20.127693
57.773577	2133.496348	20.132711
57.761587	2112.172893	20.137728
57.351690	2117.680722	20.142746
57.566947	2147.126979	20.147763
57.810883	2151.601054	20.152781
58.001116	2147.594087	20.157799
58.193431	2153.495927	20.162816
58.193972	2155.561253	20.167834
58.099809	2143.084206	20.172851
58.200607	2145.225663	20.177869
58.069192	2134.387361	20.182887
58.290332	2133.893555	20.187904
58.358351	2149.059939	20.192922
58.313307	2153.285070	20.197939
58.355335	2147.293505	20.202957
58.204221	2130.617383	20.207975
58.444537	2130.382664	20.212992
58.634323	2148.718509	20.218010
58.285613	2146.904950	20.223027
58.654020	2144.401239	20.228045
58.644134	2158.442030	20.233063
59.111319	2163.354820	20.238080
59.103129	2176.099613	20.243098
58.835857	2176.110260	20.248115
59.346501	2165.199885	20.253133
59.257485	2177.741342	20.258151
59.075513	2158.751113	20.263168
59.499547	2171.057122	20.268186
59.116780	2172.411618	20.273203
59.279493	2159.124530	20.278221
59.501291	2156.997933	20.283239
59.766303	2152.483913	20.288256
59.542259	2173.660709	20.293274
59.485085	2158.665385	20.298291
59.508091	2159.830506	20.303309
59.409082	2181.139181	20.308327
59.635925	2163.723028	20.313344
59.657685	2155.304632	20.318362
59.397744	2160.455865	20.323379
59.800916	2160.402366	20.328397
59.313996	2169.812110	20.333415
59.575482	2192.943573	20.338432
59.916872	2213.535635	20.343450
60.027723	2203.952593	20.348467
60.058371	2184.297977	20.353485
59.976441	2182.916327	20.358503
59.850614	2191.010337	20.363520
59.978037	2204.429471	20.368538
59.823778	2203.032020	20.373555
60.374219	2202.560947	20.378573
60.391826	2217.323105	20.383591
60.557316	2221.814593	20.388608
60.542503	2204.449054	20.393626
60.518357	2197.400482	20.398643
61.181042	2218.678599	20.403661
60.526991	2234.697333	20.408679
60.853076	2219.536960	20.413696
61.368962	2224.589729	20.418714
61.246400	2231.559991	20.423731
61.596559	2237.915322	20.428749
61.433580	2225.510298	20.433767
61.323368	2214.086647	20.438784
61.422137	2220.261603	20.443802
61.255074	2203.532240	20.448819
61.212658	2188.160400	20.453837
61.170470	2207.810506	20.458855
61.310809	2227.151882	20.463872
61.596061	2220.970712	20.468890
60.941644	2228.301451	20.473907
61.270973	2231.805208	20.478925
61.276271	2245.462238	20.483943
61.573578	2272.950239	20.488960
61.839207	2263.682076	20.493978
61.768866	2254.936286	20.498995
62.160144	2256.662990	20.504013
61.926208	2256.499947	20.509031
62.215397	2244.353102	20.514048
62.580942	2256.713424	20.519066
62.296196	2258.657630	20.524083
62.515334	2235.396136	20.529101
62.512389	2241.469426	20.534119
62.793280	2250.181866	20.539136
62.772114	2253.593277	20.544154
62.514947	2247.843503	20.549171
62.705718	2232.514764	20.554189
62.385669	2244.295872	20.559207
62.510312	2258.424642	20.564224
62.826779	2237.450898	20.569242
62.296867	2237.746635	20.574259
62.824343	2261.888691	20.579277
63.006656	2287.414172	20.584295
62.863649	2276.291710	20.589312
63.101693	2261.983201	20.594330
63.028545	2279.793459	20.599347
63.137341	2268.546729	20.604365
63.200204	2271.774209	20.609383
63.096404	2275.167199	20.614400
63.198353	2275.888451	20.619418
63.320970	2274.608795	20.624435
63.702891	2267.258385	20.629453
63.793036	2287.139143	20.634471
63.767000	2307.488655	20.639488
63.791628	2291.858135	20.644506
63.810307	2288.745574	20.649523
64.112236	2285.341170	20.654541
63.870984	2291.798683	20.659559
63.824397	2293.896417	20.664576
64.147946	2284.500482	20.669594
64.245588	2283.145438	20.674611
64.180646	2285.652041	20.679629
64.001755	2294.805089	20.684647
64.139371	2300.432411	20.689664
64.312160	2292.276729	20.694682
64.361673	2290.878860	20.699699
64.535005	2299.426161	20.704717
64.422722	2300.059806	20.709735
64.342544	2281.362885	20.714752
64.521889	2276.976155	20.719770
64.361245	2310.735595	20.724787
64.304368	2308.351537	20.729805
64.601488	2325.936516	20.734823
64.492710	2333.365492	20.739840
64.723641	2329.201877	20.744858
64.549898	2325.137019	20.749875
64.856593	2336.179007	20.754893
65.062337	2348.830924	20.759911
64.703436	2357.974982	20.764928
65.422702	2348.674613	20.769946
65.107767	2347.919149	20.774963
65.233207	2364.349078	20.779981
65.383201	2367.473611	20.784999
65.552471	2366.883171	20.790016
65.718567	2381.616718	20.795034
65.797613	2382.629705	20.800051
66.176609	2374.621765	20.805069
66.152505	2384.077382	20.810087
66.163542	2382.348910	20.815104
66.754219	2371.290147	20.820122
66.280231	2346.418702	20.825139
66.117353	2346.599959	20.830157
66.273667	2351.939809	20.835175
66.048883	2357.974619	20.840192
66.205513	2352.639023	20.845210
66.420524	2360.173535	20.850227
66.423998	2380.099242	20.855245
66.544838	2378.966697	20.860263
66.371856	2384.897501	20.865280
66.378031	2358.671111	20.870298
66.423496	2361.495450	20.875315
66.471579	2362.583029	20.880333
66.999921	2364.084078	20.885351
66.701468	2375.314465	20.890368
66.846470	2398.431832	20.895386
66.775257	2407.253030	20.900403
67.060808	2391.391330	20.905421
67.388131	2381.064746	20.910439
66.852541	2390.898149	20.915456
67.463428	2395.106770	20.920474
67.115594	2405.637384	20.925491
67.372836	2388.061550	20.930509
67.380547	2385.954555	20.935527
67.508141	2383.829915	20.940544
67.850839	2402.147093	20.945562
67.832744	2401.541951	20.950579
67.373315	2400.807015	20.955597
67.499774	2410.598931	20.960615
67.336416	2416.284101	20.965632
68.048675	2432.910786	20.970650
67.471865	2432.227130	20.975667
67.483231	2422.671906	20.980685
68.043430	2428.484915	20.985703
67.754634	2443.879425	20.990720
68.405079	2451.564433	20.995738
68.476923	2449.790280	21.000755
68.642664	2436.389281	21.005773
68.429102	2430.515715	21.010791
68.553693	2443.137623	21.015808
68.676101	2452.376190	21.020826
68.632002	2447.836208	21.025843
68.536904	2448.554603	21.030861
68.906490	2438.882309	21.035879
68.495495	2441.549845	21.040896
68.942694	2448.109765	21.045914
68.979113	2458.268502	21.050931
69.022546	2460.985731	21.055949
69.490487	2474.355918	21.060967
69.222458	2485.048764	21.065984
69.399743	2482.515371	21.071002
69.854540	2468.644400	21.076019
69.570135	2475.151436	21.081037
69.640952	2458.045827	21.086055
69.420507	2463.236000	21.091072
69.666332	2480.487955	21.096090
69.726621	2471.048219	21.101107
69.473458	2475.785215	21.106125
69.832153	2454.894242	21.111143
69.826185	2470.645914	21.116160
69.617084	2480.634248	21.121178
69.573039	2479.834406	21.126195
69.785633	2483.709129	21.131213
70.039420	2502.918147	21.136231
69.782511	2506.000124	21.141248
70.094370	2489.159719	21.146266
70.508491	2514.935711	21.151283
70.526851	2514.539468	21.156301
71.190748	2489.751565	21.161319
70.525961	2492.344334	21.166336
70.977692	2480.255667	21.171354
70.963760	2482.900307	21.176371
70.819012	2487.468823	21.181389
70.939828	2500.716108	21.186407
70.903477	2519.804220	21.191424
71.038296	2504.187948	21.196442
71.311653	2500.758892	21.201459
71.217311	2518.173188	21.206477
71.492870	2505.035237	21.211495
71.203662	2492.368125	21.216512
71.362977	2515.791916	21.221530
71.435896	2520.675206	21.226547
71.525205	2505.823224	21.231565
71.581540	2486.444150	21.236583
71.610664	2500.327945	21.241600
71.154550	2506.664187	21.246618
71.612115	2537.359240	21.251635
71.518024	2542.285290	21.256653
71.792188	2516.922868	21.261671
71.870055	2549.042091	21.266688
71.732684	2561.869172	21.271706
72.022742	2539.190489	21.276723
72.024548	2536.791777	21.281741
71.995085	2555.321992	21.286759
72.180179	2588.121502	21.291776
72.350308	2573.493859	21.296794
72.689318	2566.505463	21.301811
72.545074	2589.745903	21.306829
72.806872	2575.474511	21.311847
72.765012	2557.663111	21.316864
72.694277	2563.524929	21.321882
72.932966	2570.884201	21.326899
72.567903	2558.114429	21.331917
72.799784	2545.836485	21.336935
72.831371	2575.426398	21.341952
72.980291	2582.100814	21.346970
73.189838	2582.313430	21.351987
73.115368	2582.363365	21.357005
73.842497	2569.487106	21.362023
73.552479	2578.433326	21.367040
73.369776	2585.700059	21.372058
73.529757	2584.855869	21.377075
73.683685	2580.438220	21.382093
74.203088	2577.993925	21.387111
73.638070	2588.726078	21.392128
73.928292	2572.497333	21.397146
73.886697	2575.312873	21.402163
73.615658	2593.741540	21.407181
73.969930	2593.904063	21.412199
74.137359	2596.116057	21.417216
74.345518	2607.355993	21.422234
74.479209	2616.076335	21.427251
74.096865	2617.693653	21.432269
74.288247	2599.227808	21.437287
73.998753	2613.433410	21.442304
74.197640	2631.392597	21.447322
74.775702	2632.480990	21.452339
74.606337	2646.939370	21.457357
74.814928	2638.725038	21.462375
75.044743	2655.392914	21.467392
74.919419	2655.060956	21.472410
74.945967	2629.831575	21.477427
74.624188	2635.276705	21.482445
74.913374	2656.626403	21.487463
75.366186	2667.135897	21.492480
75.538382	2650.336896	21.497498
75.482584	2646.949211	21.502515
75.320636	2666.101166	21.507533
75.755962	2671.559172	21.512551
75.898176	2655.258552	21.517568
75.673857	2656.107743	21.522586
75.992986	2658.858965	21.527603
76.048199	2681.013194	21.532621
75.998138	2677.537165	21.537639
76.036279	2662.146126	21.542656
76.279012	2650.002506	21.547674
76.330449	2672.142978	21.552691
76.251409	2700.146330	21.557709
76.425262	2695.178189	21.562727
76.734539	2687.048754	21.567744
76.809079	2681.512074	21.572762
76.845578	2691.871907	21.577779
76.564379	2711.665386	21.582797
76.550818	2694.948600	21.587815
76.793941	2685.719627	21.592832
76.481107	2683.343362	21.597850
76.835998	2699.784546	21.602867
76.710619	2703.039680	21.607885
76.528674	2683.659778	21.612903
77.148688	2704.683457	21.617920
77.527520	2715.763989	21.622938
77.676019	2710.017467	21.627955
77.327005	2704.779083	21.632973
77.691007	2706.144947	21.637991
77.867849	2716.725272	21.643008
77.361081	2719.482883	21.648026
77.573427	2692.519789	21.653043
77.485008	2684.386792	21.658061
77.494374	2702.078604	21.663079
77.795824	2722.699896	21.668096
77.862173	2728.619231	21.673114
77.900453	2720.029317	21.678131
77.679947	2726.887462	21.683149
78.066713	2729.134677	21.688167
78.395864	2724.036942	21.693184
78.134293	2733.844963	21.698202
78.159122	2730.658276	21.703219
78.254856	2758.016797	21.708237
78.247179	2773.809411	21.713255
78.562199	2770.685180	21.718272
78.412769	2781.063201	21.723290
78.675784	2768.785249	21.728307
78.862992	2773.540300	21.733325
78.968565	2781.531233	21.738343
79.281412	2803.688137	21.743360
78.902431	2784.897284	21.748378
79.027455	2779.350258	21.753395
79.480984	2790.065202	21.758413
79.589541	2782.382411	21.763431
79.671552	2791.340692	21.768448
79.348526	2801.848580	21.773466
79.397796	2787.122612	21.778483
79.566597	2795.867566	21.783501
79.754226	2800.622950	21.788519
79.863255	2811.663500	21.793536
79.756848	2833.331930	21.798554
79.686359	2826.709470	21.803571
79.917637	2812.809388	21.808589
79.731425	2811.678740	21.813607
80.271294	2834.337471	21.818624
79.974816	2858.471662	21.823642
80.387383	2852.226000	21.828659
80.377059	2848.129077	21.833677
80.612956	2849.539546	21.838695
80.430673	2840.861618	21.843712
80.615158	2864.720895	21.848730
81.032236	2864.708303	21.853747
80.952848	2886.863616	21.858765
81.544218	2881.207410	21.863783
81.530200	2878.883101	21.868800
81.419318	2864.948383	21.873818
81.475491	2853.784912	21.878835
81.360179	2868.869128	21.883853
81.610201	2888.074920	21.888871
82.014557	2856.354645	21.893888
81.620495	2871.556963	21.898906
81.759535	2862.941265	21.903923
81.671994	2863.033316	21.908941
81.705727	2873.123686	21.913959
81.837248	2867.613739	21.918976
81.672351	2857.129428	21.923994
81.885811	2866.087288	21.929011
81.940534	2873.054524	21.934029
82.175649	2875.015642	21.939047
82.483386	2880.387733	21.944064
82.313909	2892.456322	21.949082
82.587425	2898.373374	21.954099
82.675539	2889.482648	21.959117
82.619812	2885.665821	21.964135
82.909067	2883.988746	21.969152
82.577060	2884.514450	21.974170
82.665471	2887.601635	21.979187
82.513767	2899.826917	21.984205
82.780324	2913.739361	21.989223
83.236132	2920.060101	21.994240
83.158407	2914.518974	21.999258
83.194765	2918.403051	22.004275
83.250317	2903.400773	22.009293
83.347976	2923.387791	22.014311
83.716115	2927.746111	22.019328
83.673400	2925.882974	22.024346
83.672642	2909.523045	22.029363
83.573660	2920.575609	22.034381
83.727700	2941.494353	22.039399
83.959801	2944.520606	22.044416
83.722880	2944.372612	22.049434
84.044434	2943.792219	22.054451
83.975269	2956.191283	22.059469
83.935462	2950.240583	22.064487
84.516994	2925.409498	22.069504
84.453671	2937.560764	22.074522
84.417948	2950.596145	22.079539
84.414985	2961.477183	22.084557
84.389865	2955.260898	22.089575
84.536204	2968.730717	22.094592
84.619542	2988.429278	22.099610
84.818401	2978.408332	22.104627
84.658953	2977.188219	22.109645
84.879087	2991.975423	22.114663
85.131821	2977.444757	22.119680
85.007011	2995.760774	22.124698
85.337506	2986.099716	22.129715
85.539949	2985.626788	22.134733
85.012231	2996.191267	22.139751
85.708314	3001.752741	22.144768
85.379999	3031.728357	22.149786
85.519196	3025.109740	22.154803
85.770690	3007.678622	22.159821
85.829768	3013.786056	22.164839
86.004195	3011.786843	22.169856
85.998592	3034.953278	22.174874
85.896880	3038.666917	22.179891
86.130813	3046.888715	22.184909
86.437153	3057.575419	22.189927
86.503800	3034.688665	22.194944
86.418546	3033.541316	22.199962
86.334663	3048.801004	22.204979
86.676669	3063.128623	22.209997
86.397214	3059.862441	22.215015
86.677583	3076.120499	22.220032
86.876405	3080.181880	22.225050
87.051735	3065.981208	22.230067
87.118749	3066.118381	22.235085
87.130882	3080.258429	22.240103
87.499036	3101.815553	22.245120
87.515696	3094.756185	22.250138
87.330465	3076.191393	22.255155
87.721084	3085.063223	22.260173
87.915914	3090.076335	22.265191
88.140834	3086.144980	22.270208
87.572582	3113.816783	22.275226
87.954498	3099.227653	22.280243
88.309751	3078.193116	22.285261
88.055276	3073.403101	22.290279
88.127386	3090.358699	22.295296
88.123014	3123.132398	22.300314
88.520315	3114.234147	22.305331
88.405083	3118.353339	22.310349
88.278752	3121.444564	22.315367
88.580186	3108.660052	22.320384
88.560722	3110.125733	22.325402
89.063279	3117.978218	22.330419
88.790973	3126.818295	22.335437
88.652593	3140.516395	22.340455
89.012431	3132.294916	22.345472
89.503650	3136.295792	22.350490
89.385241	3140.767443	22.355507
89.437459	3139.744007	22.360525
89.420140	3142.101753	22.365543
89.727768	3148.615559	22.370560
89.792137	3137.147611	22.375578
89.624578	3155.539968	22.380595
89.719132	3140.084412	22.385613
90.048370	3126.603835	22.390631
89.887674	3142.564418	22.395648
89.878702	3156.813130	22.400666
89.674499	3149.145425	22.405683
90.226187	3154.901860	22.410701
90.355389	3172.674595	22.415719
90.703077	3176.174849	22.420736
90.629031	3176.846693	22.425754
90.740067	3173.066797	22.430771
90.392600	3174.046194	22.435789
90.148810	3160.391213	22.440807
90.551044	3176.850672	22.445824
90.568245	3207.211413	22.450842
90.909162	3208.225666	22.455859
90.935850	3186.608929	22.460877
90.809871	3195.856314	22.465895
91.368354	3228.609464	22.470912
91.476748	3238.075597	22.475930
91.500924	3244.485512	22.480947
91.616419	3233.632795	22.485965
91.633736	3239.917674	22.490983
91.843341	3218.408840	22.496000
91.928305	3216.209447	22.501018
91.818646	3218.893847	22.506035
91.913640	3227.949242	22.511053
91.825574	3251.773063	22.516071
92.409012	3254.051632	22.521088
92.460572	3261.036494	22.526106
92.158847	3241.462909	22.531123
92.566176	3240.012322	22.536141
92.351693	3251.737878	22.541159
92.370704	3234.105970	22.546176
92.894648	3258.648267	22.551194
92.982243	3292.619401	22.556211
93.147512	3277.418923	22.561229
92.960863	3265.773287	22.566247
93.287173	3270.761977	22.571264
93.499492	3286.571513	22.576282
93.301873	3288.042046	22.581299
93.351666	3276.989351	22.586317
93.312787	3271.860333	22.591335
93.215460	3284.857953	22.596352
93.741285	3290.940333	22.601370
93.749357	3308.365562	22.606387
93.846447	3314.883524	22.611405
93.880705	3306.654737	22.616423
94.023633	3294.074986	22.621440
93.982598	3316.113172	22.626458
94.260180	3327.053806	22.631475
94.259384	3336.245160	22.636493
94.290663	3343.365090	22.641511
94.284544	3333.852934	22.646528
94.878719	3314.457362	22.651546
94.408665	3341.181157	22.656563
94.779407	3345.457285	22.661581
94.857598	3346.512797	22.666599
95.173314	3350.029987	22.671616
95.241171	3358.457133	22.676634
95.469316	3372.281664	22.681651
95.459020	3360.491866	22.686669
95.381764	3353.593947	22.691687
95.328077	3348.910220	22.696704
95.746546	3360.548784	22.701722
95.354409	3365.775503	22.706739
95.768064	3353.477313	22.711757
95.658226	3345.274678	22.716775
95.854150	3352.786064	22.721792
95.680379	3390.461060	22.726810
95.720309	3392.124216	22.731827
95.999319	3376.684198	22.736845
96.045334	3376.775834	22.741863
96.030049	3385.294088	22.746880
96.593063	3394.000616	22.751898
96.569885	3417.981277	22.756915
96.909387	3405.542756	22.761933
96.518081	3398.032800	22.766951
96.575330	3405.005765	22.771968
96.806005	3405.120819	22.776986
96.612114	3426.749424	22.782003
96.831028	3425.563003	22.787021
97.002357	3425.725852	22.792039
97.032346	3455.834993	22.797056
97.421551	3456.368101	22.802074
97.737253	3447.484718	22.807091
97.950901	3438.662885	22.812109
97.904981	3458.222200	22.817127
97.938117	3448.189756	22.822144
98.231728	3446.964615	22.827162
98.010114	3460.879686	22.832179
98.223875	3472.921813	22.837197
98.035805	3456.728070	22.842215
97.851380	3453.177030	22.847232
98.347658	3485.246779	22.852250
98.087802	3487.947975	22.857267
98.193397	3482.220264	22.862285
98.432672	3500.541670	22.867303
98.626200	3513.920319	22.872320
98.822913	3506.218467	22.877338
98.852973	3506.902451	22.882355
99.094522	3515.085842	22.887373
99.216026	3515.531901	22.892391
99.435987	3523.599978	22.897408
99.950111	3529.275369	22.902426
99.787983	3530.181448	22.907443
100.154766	3520.715422	22.912461
100.449305	3542.313081	22.917479
100.454488	3516.630703	22.922496
100.763489	3499.423759	22.927514
100.212797	3502.975895	22.932531
100.228299	3508.188446	22.937549
100.467340	3490.217552	22.942567
100.333758	3476.236037	22.947584
100.130696	3491.677455	22.952602
100.017731	3515.934499	22.957619
100.541065	3525.504866	22.962637
100.520793	3526.599099	22.967655
100.431083	3532.192988	22.972672
100.547636	3539.504411	22.977690
100.741859	3541.316678	22.982707
101.047567	3539.618116	22.987725
101.026434	3559.864150	22.992743
101.316613	3608.464808	22.997760
101.534445	3598.728491	23.002778
101.488569	3586.986916	23.007795
101.864373	3593.179436	23.012813
101.972267	3600.226987	23.017831
101.715108	3597.239854	23.022848
102.079818	3585.821344	23.027866
102.139359	3584.225064	23.032883
101.950958	3576.811796	23.037901
102.202574	3591.740425	23.042919
102.286050	3593.079505	23.047936
102.465394	3583.655830	23.052954
102.617312	3602.082730	23.057971
102.334419	3622.468154	23.062989
102.420018	3620.272142	23.068007
102.574262	3601.712033	23.073024
102.741397	3613.655094	23.078042
102.788851	3645.989288	23.083059
103.197552	3656.841174	23.088077
103.289903	3647.920377	23.093095
103.218915	3655.104000	23.098112
103.359906	3638.458085	23.103130
103.417883	3642.419475	23.108147
103.333154	3647.794490	23.113165
103.366322	3675.959205	23.118183
103.751794	3687.269442	23.123200
103.888756	3662.387225	23.128218
103.896232	3670.518047	23.133235
104.290743	3672.916082	23.138253
104.452317	3674.484764	23.143271
104.232951	3696.454740	23.148288
104.808206	3689.206741	23.153306
104.603074	3699.809526	23.158323
104.661446	3718.150849	23.163341
104.881505	3708.233991	23.168359
104.707169	3695.121937	23.173376
104.682859	3699.146146	23.178394
104.970803	3740.627678	23.183411
105.117537	3723.570125	23.188429
105.295628	3712.543553	23.193447
105.282727	3716.809957	23.198464
105.248645	3731.496976	23.203482
105.597361	3752.930281	23.208499
105.609043	3743.852891	23.213517
105.953237	3755.883331	23.218535
105.932857	3751.084537	23.223552
106.319615	3750.575423	23.228570
105.909300	3752.392932	23.233587
106.584623	3772.649939	23.238605
106.762261	3779.523658	23.243623
106.503709	3769.392561	23.248640
106.624737	3775.029465	23.253658
107.111175	3791.135733	23.258675
106.825592	3787.858202	23.263693
107.061370	3776.119544	23.268711
106.884856	3753.874223	23.273728
107.119518	3762.311424	23.278746
106.811356	3761.374070	23.283763
107.131321	3777.928864	23.288781
107.530536	3801.575974	23.293799
107.061298	3819.998892	23.298816
107.289003	3800.095005	23.303834
107.329917	3800.909285	23.308851
107.749383	3812.995634	23.313869
107.767264	3824.803690	23.318887
107.899920	3838.640482	23.323904
108.042239	3828.913349	23.328922
108.218376	3842.205398	23.333939
108.389663	3859.341896	23.338957
108.425453	3850.708657	23.343975
108.367146	3844.093982	23.348992
108.758395	3837.744371	23.354010
108.616887	3846.597494	23.359027
108.734861	3861.325844	23.364045
108.967420	3853.512787	23.369063
108.929316	3879.393351	23.374080
109.091107	3892.114230	23.379098
109.043656	3883.710068	23.384115
109.226399	3886.358666	23.389133
109.319897	3898.653267	23.394151
109.308500	3920.081943	23.399168
109.871391	3912.151678	23.404186
109.930573	3895.168241	23.409203
109.931392	3892.988956	23.414221
110.228513	3924.404582	23.419239
110.248639	3945.880248	23.424256
110.762683	3916.349971	23.429274
110.804951	3912.245257	23.434291
110.582830	3926.585408	23.439309
110.975463	3939.182360	23.444327
110.685944	3934.208507	23.449344
110.830990	3912.065128	23.454362
111.025830	3918.380197	23.459379
111.007508	3931.178899	23.464397
111.256427	3943.840151	23.469415
111.537202	3952.855825	23.474432
111.559498	3929.292243	23.479450
111.368245	3949.768263	23.484467
111.388463	3965.048659	23.489485
111.856257	3954.922804	23.494503
111.770268	3948.177234	23.499520
111.924876	3958.081028	23.504538
111.816371	3988.956171	23.509555
111.696250	3996.316564	23.514573
112.572455	3982.839542	23.519591
112.037646	3990.632214	23.524608
112.412542	4006.204415	23.529626
112.619971	4035.518480	23.534643
112.492752	4031.323244	23.539661
112.833492	4013.868767	23.544679
112.620768	4041.377575	23.549696
112.824511	4047.591625	23.554714
113.108134	4048.790789	23.559731
113.155665	4051.691470	23.564749
113.542787	4065.956273	23.569767
113.632053	4076.379179	23.574784
113.882231	4061.641042	23.579802
114.005284	4080.474048	23.584819
113.838676	4069.661259	23.589837
114.322458	4060.501539	23.594855
114.126174	4073.296696	23.599872
114.127965	4073.788142	23.604890
114.518713	4090.530187	23.609907
114.317042	4118.499879	23.614925
114.767357	4106.185196	23.619943
114.514277	4092.523837	23.624960
114.980100	4094.003511	23.629978
114.977768	4120.503731	23.634995
115.092710	4138.239384	23.640013
115.095450	4126.456494	23.645031
115.437361	4122.535663	23.650048
115.677376	4130.849157	23.655066
116.025571	4143.544167	23.660083
115.846833	4145.370105	23.665101
115.952878	4128.779437	23.670119
115.562318	4121.026693	23.675136
115.947044	4128.730083	23.680154
116.272232	4151.424065	23.685171
116.337915	4161.883601	23.690189
116.361930	4156.431510	23.695207
116.487509	4148.809596	23.700224
116.269717	4154.348893	23.705242
116.602491	4162.999421	23.710259
116.559437	4162.911302	23.715277
116.613347	4153.280854	23.720295
116.874178	4174.999726	23.725312
116.675507	4193.958076	23.730330
116.810514	4186.075542	23.735347
116.814985	4190.155751	23.740365
117.252541	4198.775994	23.745383
117.212798	4210.245063	23.750400
117.088216	4214.159210	23.755418
117.690271	4249.243641	23.760435
117.947703	4262.408844	23.765453
118.223956	4241.640893	23.770471
118.080008	4228.679854	23.775488
118.171079	4241.153269	23.780506
118.449679	4235.315791	23.785523
118.301118	4256.754410	23.790541
118.912925	4263.363697	23.795559
119.199835	4276.491760	23.800576
119.217865	4266.084526	23.805594
119.162511	4251.164815	23.810611
119.129756	4253.318991	23.815629
119.140106	4268.254481	23.820647
119.019714	4269.642858	23.825664
119.242136	4284.222861	23.830682
119.509094	4268.296765	23.835699
119.821684	4293.833864	23.840717
119.619358	4309.719460	23.845735
119.859289	4293.308059	23.850752
120.289046	4286.984186	23.855770
120.391499	4299.744339	23.860787
120.585422	4317.983269	23.865805
120.525836	4321.268223	23.870823
120.763855	4315.405532	23.875840
120.901475	4306.119804	23.880858
120.787465	4300.067660	23.885875
120.847677	4305.752010	23.890893
120.988870	4303.164251	23.895911
121.234629	4325.418088	23.900928
121.045165	4345.400258	23.905946
121.262498	4340.601567	23.910963
121.365798	4331.680931	23.915981
121.902193	4340.051860	23.920999
121.825790	4371.683850	23.926016
121.833501	4372.450302	23.931034
122.053795	4361.254884	23.936051
121.809909	4360.101169	23.941069
121.696825	4376.870087	23.946087
122.089676	4393.959345	23.951104
122.200381	4405.693060	23.956122
122.556516	4388.847016	23.961139
122.468226	4421.915276	23.966157
122.694846	4435.242406	23.971175
122.871074	4419.416183	23.976192
123.027605	4408.891089	23.981210
123.530028	4416.470455	23.986227
123.311573	4441.168018	23.991245
123.756663	4449.236386	23.996263
123.506588	4454.588610	24.001280
123.616051	4453.863100	24.006298
124.064960	4436.702864	24.011315
123.858821	4441.782871	24.016333
124.066889	4457.084679	24.021351
124.224243	4457.108319	24.026368
124.250243	4461.081501	24.031386
124.832758	4462.061630	24.036403
124.563459	4483.788615	24.041421
124.784447	4471.546970	24.046439
124.997641	4474.939240	24.051456
124.737204	4485.788700	24.056474
124.930793	4481.592297	24.061491
124.938414	4491.739219	24.066509
125.093545	4485.888586	24.071527
125.504855	4497.971112	24.076544
125.628658	4530.981331	24.081562
125.506065	4506.372729	24.086579
125.714639	4514.854220	24.091597
125.937892	4515.758681	24.096615
126.285238	4517.022942	24.101632
125.945473	4535.863688	24.106650
126.247240	4530.962800	24.111667
126.529613	4525.484030	24.116685
126.396783	4525.630028	24.121703
127.034361	4524.793234	24.126720
126.519755	4549.400145	24.131738
126.673188	4559.510418	24.136755
126.868434	4553.763758	24.141773
126.911925	4557.373454	24.146791
126.997802	4585.374424	24.151808
126.974067	4593.623878	24.156826
127.341748	4576.831234	24.161843
127.163699	4608.193893	24.166861
127.640953	4597.507804	24.171879
127.674592	4605.526922	24.176896
127.551631	4629.286975	24.181914
127.850942	4658.073266	24.186931
128.452094	4640.399470	24.191949
128.501780	4633.029225	24.196967
128.939518	4653.853019	24.201984
128.505985	4675.144818	24.207002
129.197692	4667.851144	24.212019
129.359834	4692.185434	24.217037
129.378377	4675.264157	24.222055
129.495220	4651.249611	24.227072
129.235688	4668.685157	24.232090
129.915103	4681.615244	24.237107
129.826757	4674.281567	24.242125
129.755349	4655.629534	24.247143
130.142769	4664.400840	24.252160
130.091096	4685.335073	24.257178
130.446463	4699.960429	24.262195
130.217776	4696.798692	24.267213
130.153345	4684.786322	24.272231
130.400963	4693.727201	24.277248
130.555947	4716.795407	24.282266
130.687251	4728.246438	24.287283
130.708154	4717.950630	24.292301
130.978008	4724.120565	24.297319
131.156560	4727.098935	24.302336
131.156545	4737.658297	24.307354
131.270160	4753.281119	24.312371
131.445465	4744.923145	24.317389
131.149140	4764.233362	24.322407
131.712692	4786.332988	24.327424
131.555241	4794.449920	24.332442
132.097729	4780.570669	24.337459
132.188844	4795.858672	24.342477
132.018861	4814.038240	24.347495
132.593170	4821.118923	24.352512
132.503650	4821.938078	24.357530
132.836333	4834.602361	24.362547
132.697231	4842.967860	24.367565
132.885337	4853.467476	24.372583
133.338830	4844.062698	24.377600
133.080509	4833.834999	24.382618
133.209895	4848.515159	24.387635
133.349886	4860.834533	24.392653
133.371501	4869.540811	24.397671
133.871395	4856.136640	24.402688
133.410930	4860.838730	24.407706
133.812123	4879.357063	24.412723
133.947020	4902.582014	24.417741
133.999851	4888.218223	24.422759
134.163080	4905.174336	24.427776
134.275075	4943.656277	24.432794
134.487916	4940.907754	24.437811
134.627556	4915.509504	24.442829
134.639516	4953.826109	24.447847
135.148308	4972.211420	24.452864
135.061330	4967.581718	24.457882
135.136427	4955.502383	24.462899
135.263426	4980.814588	24.467917
135.222439	4993.525784	24.472935
135.801743	4983.811157	24.477952
135.549044	4995.980564	24.482970
135.828625	5021.852272	24.487987
136.252751	5010.733732	24.493005
136.463906	5015.963084	24.498023
136.475096	5003.487969	24.503040
136.618611	5024.498674	24.508058
136.808828	5052.208833	24.513075
136.742491	5050.411942	24.518093
136.976216	5033.559051	24.523111
137.105615	5033.879047	24.528128
137.182917	5055.119633	24.533146
137.508836	5042.025943	24.538163
137.854980	5057.261827	24.543181
137.920245	5067.412985	24.548199
138.166023	5064.814905	24.553216
138.107450	5059.541894	24.558234
138.425382	5078.952972	24.563251
138.609482	5106.372897	24.568269
138.167286	5109.831082	24.573287
138.585709	5082.816788	24.578304
138.650858	5083.900166	24.583322
138.706741	5100.935649	24.588339
139.100626	5123.533483	24.593357
139.134052	5125.822909	24.598375
139.380714	5108.817797	24.603392
139.281038	5118.961597	24.608410
139.183138	5131.196083	24.613427
139.586334	5158.497219	24.618445
139.785939	5142.980578	24.623463
139.701391	5134.027528	24.628480
139.866787	5167.792474	24.633498
139.958478	5180.940569	24.638515
140.329775	5178.794179	24.643533
140.456351	5177.977619	24.648551
140.504292	5204.815088	24.653568
140.606583	5216.248044	24.658586
140.658979	5212.427145	24.663603
140.681242	5199.753584	24.668621
140.700644	5231.260860	24.673639
140.899163	5232.692690	24.678656
141.328455	5271.782476	24.683674
141.594778	5269.621923	24.688691
142.043587	5253.643512	24.693709
141.915523	5273.962798	24.698727
142.005465	5279.880394	24.703744
142.268312	5288.406885	24.708762
142.525067	5291.501186	24.713779
142.700530	5279.415252	24.718797
142.532279	5305.794118	24.723815
142.535542	5305.967636	24.728832
143.241562	5298.753986	24.733850
142.916510	5278.994269	24.738867
143.447352	5292.061627	24.743885
143.360986	5324.752345	24.748903
143.852572	5327.805094	24.753920
143.575375	5320.650352	24.758938
143.543430	5314.877172	24.763955
143.877484	5321.353675	24.768973
143.820203	5326.871589	24.773991
144.091405	5332.945873	24.779008
144.024215	5335.306287	24.784026
143.631855	5349.943207	24.789043
144.460422	5380.526902	24.794061
144.109781	5387.102002	24.799079
144.353052	5387.677608	24.804096
144.618672	5415.917705	24.809114
144.833310	5420.349742	24.814131
145.054428	5436.959851	24.819149
145.160095	5451.252360	24.824167
145.212372	5436.456251	24.829184
145.675037	5439.983503	24.834202
145.707801	5468.142481	24.839219
146.237050	5473.436755	24.844237
146.237353	5478.414872	24.849255
146.359040	5482.780787	24.854272
146.533759	5475.652486	24.859290
146.774648	5499.608085	24.864307
147.108282	5495.575286	24.869325
146.400382	5498.314438	24.874343
147.142203	5498.409624	24.879360
147.061725	5528.871368	24.884378
146.993756	5527.308558	24.889395
147.358551	5522.925314	24.894413
147.324473	5545.565736	24.899431
147.712542	5555.968611	24.904448
147.662532	5553.336645	24.909466
147.997512	5567.668933	24.914483
148.184076	5578.302371	24.919501
148.098918	5583.337952	24.924519
148.272185	5579.687157	24.929536
148.722099	5608.604662	24.934554
148.687984	5610.899414	24.939571
149.048161	5619.891917	24.944589
149.076905	5623.220819	24.949607
149.056468	5625.831832	24.954624
149.309946	5628.487352	24.959642
149.388463	5639.607603	24.964659
149.877327	5635.017993	24.969677
150.173033	5661.999570	24.974695
150.095339	5681.866556	24.979712
150.198490	5674.790542	24.984730
150.341705	5682.885815	24.989747
150.636271	5674.616699	24.994765
150.637414	5677.046193	24.999783
150.934754	5698.366658	25.004800
150.693507	5708.453914	25.009818
150.898634	5720.294286	25.014835
151.255214	5708.923014	25.019853
151.346816	5717.433547	25.024871
151.207533	5739.758939	25.029888
151.743296	5754.019244	25.034906
151.434772	5767.848170	25.039923
151.834884	5764.163394	25.044941
151.901893	5772.637861	25.049959
152.064103	5775.226199	25.054976
152.131295	5804.784111	25.059994
152.604753	5788.479804	25.065011
152.564750	5779.291058	25.070029
152.750945	5805.156663	25.075047
152.607925	5836.010070	25.080064
152.807519	5842.211354	25.085082
153.134311	5835.492432	25.090099
153.434061	5847.749575	25.095117
153.496355	5870.062713	25.100135
153.053213	5875.852071	25.105152
153.426786	5881.778938	25.110170
153.722895	5879.787014	25.115187
154.169343	5892.300678	25.120205
154.427405	5922.453692	25.125223
154.626471	5918.619017	25.130240
154.629924	5920.100468	25.135258
155.150338	5926.071598	25.140275
155.454374	5935.029069	25.145293
155.371576	5928.831359	25.150311
155.325085	5939.991773	25.155328
155.726383	5935.480723	25.160346
155.458162	5954.864542	25.165363
155.995522	5952.061042	25.170381
156.372818	5945.343572	25.175399
155.788251	5969.653231	25.180416
156.404597	5964.178624	25.185434
156.195737	5979.696501	25.190451
156.730308	5976.977715	25.195469
156.685393	5983.519870	25.200487
156.679736	5986.051724	25.205504
157.183257	5992.761155	25.210522
157.033019	6009.360395	25.215539
157.504822	6020.453339	25.220557
157.482003	6036.872095	25.225575
157.857867	6032.966838	25.230592
157.928239	6032.205587	25.235610
158.100213	6038.819416	25.240627
158.211419	6045.689370	25.245645
158.269777	6050.378923	25.250663
158.656307	6066.022540	25.255680
158.604262	6056.266287	25.260698
158.513462	6066.336001	25.265715
158.943314	6089.030879	25.270733
158.714715	6103.527654	25.275751
158.983540	6107.501688	25.280768
159.448218	6097.516318	25.285786
159.248063	6123.750643	25.290803
159.637218	6146.580292	25.295821
159.793949	6152.699011	25.300839
159.507864	6139.202732	25.305856
160.229876	6162.705809	25.310874
160.050424	6200.292083	25.315891
160.252534	6195.681183	25.320909
160.637661	6189.227298	25.325927
160.526231	6199.627305	25.330944
160.768264	6219.013761	25.335962
160.969030	6221.541468	25.340979
161.338184	6228.772064	25.345997
161.412346	6252.238609	25.351015
161.390884	6250.342030	25.356032
161.758015	6251.711054	25.361050
161.996981	6274.153465	25.366067
162.231708	6282.934384	25.371085
162.325044	6282.450847	25.376103
162.603159	6283.198307	25.381120
163.044558	6292.240777	25.386138
162.843699	6313.797173	25.391155
163.196869	6291.370334	25.396173
163.288379	6279.945588	25.401191
163.032530	6292.044075	25.406208
163.169361	6305.047065	25.411226
163.244539	6320.918384	25.416243
163.471525	6331.227124	25.421261
163.929737	6345.085788	25.426279
163.806193	6354.708695	25.431296
164.175708	6347.691525	25.436314
164.189765	6379.016550	25.441331
164.203598	6379.435994	25.446349
164.325611	6381.733804	25.451367
164.520035	6400.573183	25.456384
164.377535	6410.540232	25.461402
164.762834	6425.840287	25.466419
165.164413	6431.140631	25.471437
165.351296	6433.031235	25.476455
165.522950	6451.619688	25.481472
166.074010	6453.932451	25.486490
166.451638	6477.035774	25.491507
166.333961	6495.620113	25.496525
166.613090	6486.231748	25.501543
166.531164	6473.603505	25.506560
166.812743	6500.358923	25.511578
166.925445	6508.796316	25.516595
166.984787	6512.637727	25.521613
167.062650	6513.603345	25.526631
167.367600	6522.484619	25.531648
167.422399	6545.643354	25.536666
167.896570	6542.991546	25.541683
167.730453	6549.522071	25.546701
167.859619	6566.174564	25.551719
168.371653	6564.501640	25.556736
168.444972	6561.193545	25.561754
168.426471	6586.374900	25.566771
168.404926	6616.803432	25.571789
168.739021	6592.689760	25.576807
168.744753	6597.413767	25.581824
169.044052	6609.121918	25.586842
169.146257	6635.699309	25.591859
169.535518	6668.607194	25.596877
169.613688	6672.934959	25.601895
169.539358	6665.055842	25.606912
170.131548	6677.127900	25.611930
170.082759	6689.852397	25.616947
170.192305	6698.931037	25.621965
170.547768	6719.284918	25.626983
170.511499	6736.314574	25.632000
170.711043	6716.160412	25.637018
170.831039	6728.855870	25.642035
171.218500	6749.511231	25.647053
171.658543	6764.469857	25.652071
171.288027	6781.302004	25.657088
171.551075	6784.814907	25.662106
171.589443	6793.017855	25.667123
171.766442	6800.649017	25.672141
172.297630	6807.596780	25.677159
172.573610	6810.965802	25.682176
172.505782	6837.233400	25.687194
172.762202	6843.137863	25.692212
173.183076	6839.958133	25.697229
173.402366	6846.007725	25.702247
173.256783	6867.012373	25.707264
173.489384	6864.370897	25.712282
173.753431	6867.650947	25.717300
173.589433	6876.062989	25.722317
174.100047	6900.482140	25.727335
174.156402	6906.303134	25.732352
174.038427	6917.040961	25.737370
174.283779	6927.923513	25.742388
174.350086	6943.852841	25.747405
174.753766	6931.020354	25.752423
175.034683	6951.786119	25.757440
175.269903	6974.514444	25.762458
175.483160	6975.997947	25.767476
175.170021	6976.030037	25.772493
175.936578	6979.654697	25.777511
176.053357	6989.895456	25.782528
176.174685	7005.680699	25.787546
176.279652	7006.080377	25.792564
176.289153	6998.079746	25.797581
176.654035	7021.400575	25.802599
176.689229	7041.427821	25.807616
176.965636	7047.989779	25.812634
177.148520	7030.450922	25.817652
177.059897	7037.207853	25.822669
177.383794	7045.149553	25.827687
177.527145	7067.742779	25.832704
177.562030	7076.760342	25.837722
177.822933	7091.828814	25.842740
178.104886	7106.887521	25.847757
178.351052	7101.560711	25.852775
178.290722	7117.738731	25.857792
178.470454	7145.792183	25.862810
178.682429	7142.209445	25.867828
178.847627	7139.673955	25.872845
179.340800	7163.760526	25.877863
179.516889	7187.132091	25.882880
179.315465	7190.065830	25.887898
179.778710	7187.759080	25.892916
180.019702	7203.984659	25.897933
180.209578	7210.293621	25.902951
180.330522	7243.564418	25.907968
180.253596	7246.944596	25.912986
180.408291	7237.686204	25.918004
180.307178	7261.451371	25.923021
181.342758	7267.867114	25.928039
181.488189	7279.343279	25.933056
181.549084	7295.188413	25.938074
182.000538	7293.855397	25.943092
181.582632	7311.033392	25.948109
181.891229	7322.084143	25.953127
182.033995	7338.236314	25.958144
182.275004	7334.991309	25.963162
182.589760	7335.753637	25.968180
182.599646	7367.984617	25.973197
183.048692	7371.899272	25.978215
183.331914	7369.426147	25.983232
183.084447	7382.169069	25.988250
183.512162	7401.187281	25.993268
183.408749	7413.448086	25.998285
183.815255	7414.541771	26.003303
183.949719	7429.565306	26.008320
183.811849	7441.419949	26.013338
184.592146	7439.274984	26.018356
184.252268	7459.385605	26.023373
184.745187	7477.506378	26.028391
184.687726	7487.739633	26.033408
185.159930	7494.839206	26.038426
185.962053	7487.055056	26.043444
185.924720	7489.749892	26.048461
186.147075	7502.660205	26.053479
185.951914	7509.804689	26.058496
186.222783	7523.185822	26.063514
186.633367	7512.052400	26.068532
186.598044	7524.136659	26.073549
186.340496	7543.220229	26.078567
186.644262	7552.674822	26.083584
186.408035	7542.961070	26.088602
186.751190	7555.871156	26.093620
186.802241	7592.373681	26.098637
187.011895	7587.541407	26.103655
187.324786	7587.318062	26.108672
187.769765	7633.765179	26.113690
187.646202	7628.721762	26.118708
187.834658	7643.255395	26.123725
187.823127	7645.756985	26.128743
188.167670	7683.992642	26.133760
188.269003	7692.460115	26.138778
188.897354	7706.286365	26.143796
188.683123	7718.085316	26.148813
189.153551	7742.560856	26.153831
189.534259	7749.919802	26.158848
189.647764	7758.760958	26.163866
190.155956	7752.489291	26.168884
190.177341	7784.199444	26.173901
190.743688	7793.131969	26.178919
190.967467	7787.631823	26.183936
190.918512	7783.062732	26.188954
191.201636	7775.656376	26.193972
191.258741	7809.365768	26.198989
191.357535	7820.727965	26.204007
191.420162	7810.676425	26.209024
191.418007	7813.003232	26.214042
192.064886	7829.706591	26.219060
191.826063	7832.522983	26.224077
191.619037	7865.286976	26.229095
192.345899	7859.976174	26.234112
192.274227	7876.751055	26.239130
192.703994	7894.292082	26.244148
192.792600	7906.104141	26.249165
193.006476	7921.990784	26.254183
193.445226	7943.461845	26.259200
193.290641	7945.875287	26.264218
193.735933	7947.231947	26.269236
193.613643	7962.574846	26.274253
193.928537	7994.092803	26.279271
194.209125	7984.797421	26.284288
194.349785	8001.287695	26.289306
194.889108	8007.180902	26.294324
194.869658	8038.263543	26.299341
195.455610	8057.375327	26.304359
195.595655	8060.449696	26.309376
195.603232	8051.856996	26.314394
195.896935	8039.595829	26.319412
195.871940	8067.599303	26.324429
196.315249	8083.449775	26.329447
196.709457	8079.628014	26.334464
196.607468	8075.370024	26.339482
197.187042	8087.573633	26.344500
196.970617	8121.176101	26.349517
197.057291	8103.711013	26.354535
197.360281	8116.604571	26.359552
197.330800	8145.984009	26.364570
197.887190	8153.777206	26.369588
197.759914	8162.640259	26.374605
197.961934	8160.785279	26.379623
197.897427	8173.715977	26.384640
198.397515	8192.836601	26.389658
198.985490	8189.770364	26.394676
199.084615	8203.826259	26.399693
199.407304	8224.827016	26.404711
199.836136	8213.200219	26.409728
199.933198	8223.686431	26.414746
199.980249	8238.833868	26.419764
200.006817	8235.906848	26.424781
200.106204	8234.261772	26.429799
200.127215	8259.206945	26.434816
200.253923	8262.085878	26.439834
200.381923	8256.310782	26.444852
200.474267	8270.118985	26.449869
200.780804	8296.781198	26.454887
201.088433	8318.283101	26.459904
201.170350	8329.394855	26.464922
201.112385	8308.495994	26.469940
201.423125	8336.765015	26.474957
201.561797	8371.265457	26.479975
202.004331	8381.299330	26.484992
201.932925	8397.028032	26.490010
202.605084	8413.121403	26.495028
202.402088	8441.354995	26.500045
202.769776	8439.788430	26.505063
203.105909	8442.662721	26.510080
203.436325	8456.431751	26.515098
203.491047	8478.455294	26.520116
204.060097	8484.956509	26.525133
203.820633	8483.615483	26.530151
204.586880	8511.830821	26.535168
204.582220	8529.113552	26.540186
204.795775	8510.432287	26.545204
204.738202	8531.987734	26.550221
204.764125	8541.520334	26.555239
204.968326	8558.377946	26.560256
205.053423	8582.214361	26.565274
205.397242	8590.033448	26.570292
205.812529	8612.028319	26.575309
206.028336	8595.677052	26.580327
206.292210	8612.373646	26.585344
206.284217	8645.230811	26.590362
206.531947	8655.135590	26.595380
206.874903	8647.366102	26.600397
207.211266	8660.746835	26.605415
207.141704	8683.883586	26.610432
207.120388	8693.555612	26.615450
207.304456	8717.323896	26.620468
207.938907	8734.138961	26.625485
208.141604	8772.098262	26.630503
208.590642	8761.461672	26.635520
208.423200	8760.690753	26.640538
208.998235	8781.111843	26.645556
209.327997	8801.949168	26.650573
209.047875	8814.044933	26.655591
209.496083	8828.906914	26.660608
209.596741	8824.705025	26.665626
209.549294	8836.976590	26.670644
209.868815	8873.332971	26.675661
209.809267	8879.063975	26.680679
210.278764	8887.823318	26.685696
210.583746	8914.957819	26.690714
211.053739	8923.926602	26.695732
211.121383	8933.711667	26.700749
211.104874	8940.245238	26.705767
211.305872	8953.677727	26.710784
212.009722	8970.926576	26.715802
212.029929	8997.095410	26.720820
212.300898	8993.170140	26.725837
212.473778	8998.181505	26.730855
212.664661	9031.086947	26.735872
212.761072	9033.005420	26.740890
213.062348	9031.000048	26.745908
213.089407	9053.164431	26.750925
213.173539	9064.438585	26.755943
213.737047	9060.572866	26.760960
213.745650	9086.463376	26.765978
213.790267	9066.717740	26.770996
214.256944	9094.437806	26.776013
214.352990	9126.250947	26.781031
214.705046	9129.273957	26.786048
214.746549	9134.655985	26.791066
215.158562	9136.134031	26.796084
215.377135	9148.459549	26.801101
215.409895	9179.846916	26.806119
215.751770	9178.205784	26.811136
215.634339	9201.791479	26.816154
215.736450	9227.924321	26.821172
216.164799	9226.979328	26.826189
216.058671	9236.627892	26.831207
216.507713	9244.833969	26.836224
216.595421	9279.395222	26.841242
216.985024	9295.062035	26.846260
217.183351	9312.233321	26.851277
217.203441	9344.958915	26.856295
217.613644	9352.058553	26.861312
217.706875	9358.480437	26.866330
217.789635	9366.416294	26.871348
218.321645	9392.438209	26.876365
218.449915	9428.691207	26.881383
218.954443	9430.975493	26.886400
219.029399	9437.022367	26.891418
219.238051	9451.948934	26.896436
219.591586	9466.460124	26.901453
219.306734	9490.798529	26.906471
219.947039	9516.675947	26.911488
220.612884	9518.849316	26.916506
220.744923	9539.826613	26.921524
221.032534	9557.433152	26.926541
221.339196	9569.137965	26.931559
221.480697	9563.023057	26.936576
221.730531	9564.673654	26.941594
221.858313	9570.097496	26.946612
222.404248	9585.566277	26.951629
222.314953	9615.311186	26.956647
222.620777	9605.485334	26.961664
222.684014	9601.862034	26.966682
222.721971	9636.700870	26.971700
222.934006	9653.366172	26.976717
223.013121	9665.073996	26.981735
223.414151	9661.217653	26.986752
223.682251	9686.066753	26.991770
223.838277	9688.885181	26.996788
224.271248	9690.696142	27.001805
224.512633	9733.221248	27.006823
224.295908	9739.322731	27.011840
224.759556	9744.250061	27.016858
224.879743	9766.607205	27.021876
225.149626	9782.699133	27.026893
225.138098	9815.333253	27.031911
225.504005	9818.774713	27.036928
225.652900	9813.262612	27.041946
225.677990	9832.993795	27.046964
226.306794	9854.966147	27.051981
226.550902	9875.827704	27.056999
226.875267	9893.098519	27.062016
226.976103	9913.680552	27.067034
226.917617	9942.989351	27.072052
227.323095	9924.116395	27.077069
227.440674	9939.583833	27.082087
227.531931	9979.145259	27.087104
227.814031	10007.830794	27.092122
227.754944	10010.780915	27.097140
228.214263	10017.977497	27.102157
228.271724	10062.019393	27.107175
228.590381	10064.183254	27.112192
229.090509	10092.159469	27.117210
229.587624	10103.333046	27.122228
229.396354	10100.357394	27.127245
229.984729	10110.888133	27.132263
230.312713	10118.061564	27.137280
230.579305	10153.505702	27.142298
230.753122	10165.579478	27.147316
231.342906	10146.870360	27.152333
231.014671	10169.613288	27.157351
231.413096	10178.026707	27.162368
231.769704	10189.836364	27.167386
231.725598	10209.794479	27.172404
232.024907	10227.728288	27.177421
231.837981	10240.015318	27.182439
232.171143	10256.573023	27.187456
232.263086	10253.156715	27.192474
232.435857	10294.406822	27.197492
232.655172	10329.884370	27.202509
233.013666	10351.281387	27.207527
233.232878	10374.317754	27.212544
233.672272	10371.856963	27.217562
233.787160	10402.094988	27.222580
234.216033	10422.595125	27.227597
234.438731	10436.045766	27.232615
234.621665	10453.131036	27.237632
234.837622	10458.614656	27.242650
234.700988	10503.303444	27.247668
235.405984	10508.604671	27.252685
235.441237	10516.768715	27.257703
235.741308	10546.794463	27.262720
236.254076	10563.786760	27.267738
236.368052	10576.431566	27.272756
236.757050	10586.548159	27.277773
236.813521	10607.377876	27.282791
236.963665	10608.601589	27.287808
237.314958	10632.631835	27.292826
237.381338	10668.430001	27.297844
237.839638	10668.121948	27.302861
237.948028	10668.497921	27.307879
238.242271	10696.517883	27.312896
238.559264	10716.860443	27.317914
238.843119	10737.815027	27.322932
239.602665	10757.458304	27.327949
239.562823	10767.445004	27.332967
239.697563	10788.025718	27.337984
239.672626	10778.141154	27.343002
240.098956	10811.608459	27.348020
240.505758	10829.371586	27.353037
240.793754	10840.707843	27.358055
240.767687	10842.423066	27.363072
240.992367	10858.626741	27.368090
241.191223	10897.690601	27.373108
241.572515	10908.177316	27.378125
241.794534	10915.336321	27.383143
241.844592	10939.825618	27.388160
242.392809	10954.810925	27.393178
242.203768	10989.743791	27.398196
242.549709	10985.057330	27.403213
242.624766	10998.943235	27.408231
242.887508	11010.590203	27.413248
243.340327	11037.588905	27.418266
243.232657	11074.747177	27.423284
243.585031	11063.985605	27.428301
244.333502	11086.727604	27.433319
244.594242	11110.185113	27.438336
244.879852	11112.706687	27.443354
245.191413	11124.235393	27.448372
245.660247	11118.046115	27.453389
245.931773	11125.642880	27.458407
246.067738	11149.479471	27.463424
246.356675	11135.161569	27.468442
246.322440	11147.814774	27.473460
246.440722	11153.946519	27.478477
246.817599	11184.060820	27.483495
246.718999	11180.678946	27.488512
247.119866	11174.766337	27.493530
247.316985	11215.676089	27.498548
247.455405	11233.402875	27.503565
247.829658	11242.615661	27.508583
247.755213	11255.107023	27.513600
247.768914	11284.127509	27.518618
247.805481	11313.271880	27.523636
248.345785	11330.228939	27.528653
248.477545	11344.650093	27.533671
248.703369	11380.669283	27.538688
248.905760	11411.362672	27.543706
249.153468	11429.695498	27.548724
249.321064	11451.863636	27.553741
249.645096	11488.050382	27.558759
249.778007	11501.527000	27.563776
250.597574	11519.785140	27.568794
251.245008	11541.590541	27.573812
251.445850	11555.337989	27.578829
251.974468	11562.904302	27.583847
252.015132	11582.334951	27.588864
252.648035	11586.291191	27.593882
252.819397	11592.550613	27.598900
252.806895	11617.412855	27.603917
252.808070	11633.992185	27.608935
253.025549	11640.556738	27.613952
253.594520	11647.601246	27.618970
253.675147	11674.906719	27.623988
253.751426	11696.676721	27.629005
254.187292	11700.603313	27.634023
254.013449	11731.630461	27.639040
254.335756	11759.121442	27.644058
254.370426	11770.249713	27.649076
254.629079	11790.194443	27.654093
255.416802	11799.318758	27.659111
255.438239	11830.496590	27.664128
255.703052	11847.173590	27.669146
256.023688	11859.657654	27.674164
256.057091	11874.619389	27.679181
256.536068	11897.131361	27.684199
256.566987	11933.083953	27.689216
257.132242	11947.211883	27.694234
257.230979	11953.461389	27.699252
257.858913	11981.246505	27.704269
258.218468	12014.201147	27.709287
257.958365	12009.717715	27.714304
258.023250	12020.046323	27.719322
258.520129	12051.810112	27.724340
259.191341	12087.721860	27.729357
259.232344	12092.923786	27.734375
259.588152	12103.966145	27.739392
259.781704	12113.462162	27.744410
260.074726	12136.854401	27.749428
260.374991	12161.875358	27.754445
260.528024	12153.490375	27.759463
260.625669	12176.390301	27.764480
261.300463	12191.415732	27.769498
261.363630	12205.465353	27.774516
261.641907	12229.350941	27.779533
262.368390	12252.358202	27.784551
262.429119	12265.796184	27.789568
262.612310	12264.836389	27.794586
262.595314	12282.949237	27.799604
262.753974	12312.458899	27.804621
263.099967	12297.392395	27.809639
263.470168	12337.363394	27.814656
263.750183	12343.149828	27.819674
264.223927	12346.988395	27.824692
264.328280	12380.305790	27.829709
264.327230	12370.110640	27.834727
264.292943	12390.815089	27.839744
264.841044	12420.925489	27.844762
264.986097	12451.116716	27.849780
264.789252	12454.612343	27.854797
265.249149	12471.141959	27.859815
265.730921	12509.240524	27.864832
265.990697	12533.734637	27.869850
266.317087	12547.422018	27.874868
266.402591	12571.336026	27.879885
266.894945	12584.634426	27.884903
267.260597	12607.905063	27.889920
267.671455	12622.500261	27.894938
267.825116	12643.162955	27.899956
268.034128	12680.293898	27.904973
268.314900	12681.913719	27.909991
268.302793	12696.287383	27.915008
268.739478	12708.920737	27.920026
268.905864	12746.195163	27.925044
269.176469	12774.388111	27.930061
269.933440	12756.358140	27.935079
269.773594	12781.627821	27.940096
270.223731	12799.248119	27.945114
270.705097	12834.316881	27.950132
270.819755	12854.900421	27.955149
270.957668	12857.634173	27.960167
271.292511	12896.016330	27.965184
271.529386	12900.826921	27.970202
271.674771	12915.371711	27.975220
271.925845	12942.058755	27.980237
272.428882	12965.198497	27.985255
272.351022	12990.824439	27.990272
273.024505	13015.407709	27.995290
273.458100	13042.951834	28.000308
273.645390	13064.194065	28.005325
274.378488	13064.182488	28.010343
274.290640	13079.578189	28.015360
274.748206	13106.540212	28.020378
275.047876	13118.946004	28.025396
274.972864	13136.109059	28.030413
275.560612	13138.268280	28.035431
275.644954	13163.634508	28.040448
276.350737	13180.135262	28.045466
276.251320	13181.314535	28.050484
276.427099	13196.075933	28.055501
276.855147	13218.479219	28.060519
276.890615	13241.167984	28.065536
276.904409	13254.103255	28.070554
277.331154	13266.040687	28.075572
277.096906	13284.389874	28.080589
277.735439	13327.660929	28.085607
277.975172	13367.558359	28.090624
278.288734	13367.538104	28.095642
278.802574	13380.720959	28.100660
278.932578	13420.174196	28.105677
279.227495	13442.665178	28.110695
279.117069	13462.755688	28.115712
279.523754	13490.418473	28.120730
279.752751	13519.149809	28.125748
279.943849	13554.893636	28.130765
280.439304	13570.735464	28.135783
280.405201	13570.419699	28.140800
280.698607	13585.153354	28.145818
281.565737	13628.576531	28.150836
281.406450	13645.167114	28.155853
281.940358	13662.575198	28.160871
282.114723	13692.728460	28.165888
282.637057	13717.307052	28.170906
283.262281	13739.619400	28.175924
283.358691	13740.327533	28.180941
283.712210	13749.016553	28.185959
283.993319	13758.303695	28.190976
284.205663	13803.022799	28.195994
284.369161	13821.250158	28.201012
284.852971	13829.710493	28.206029
285.222336	13848.535721	28.211047
285.244095	13861.848329	28.216064
285.606725	13874.765857	28.221082
285.723471	13905.444288	28.226100
285.627139	13914.224264	28.231117
286.006516	13948.830143	28.236135
286.099477	13991.138186	28.241152
286.419055	14003.085994	28.246170
287.004047	14015.227892	28.251188
287.134489	14056.901208	28.256205
287.278293	14076.416313	28.261223
287.920265	14089.971722	28.266240
287.571248	14113.885749	28.271258
288.375649	14153.182087	28.276276
288.764693	14199.634751	28.281293
289.118477	14206.345653	28.286311
289.477300	14234.617975	28.291328
289.822784	14275.923849	28.296346
290.161663	14272.836190	28.301364
290.412248	14284.516701	28.306381
290.607883	14318.194107	28.311399
291.111325	14357.400424	28.316416
291.236557	14373.472812	28.321434
291.560929	14388.221782	28.326452
291.748281	14415.307851	28.331469
292.095085	14432.763439	28.336487
292.153986	14466.061928	28.341504
292.849115	14479.352037	28.346522
293.388074	14494.111348	28.351540
293.190343	14522.827516	28.356557
293.566935	14523.234911	28.361575
294.228248	14548.525325	28.366592
294.286206	14582.136208	28.371610
294.672354	14612.418500	28.376628
294.957150	14617.743269	28.381645
295.331513	14628.393513	28.386663
295.742794	14648.998094	28.391680
295.514891	14687.369547	28.396698
296.000043	14692.412268	28.401716
295.932794	14737.525242	28.406733
296.139033	14746.692170	28.411751
296.620590	14760.693806	28.416768
296.824425	14801.742360	28.421786
297.265049	14830.383549	28.426804
297.212139	14865.576516	28.431821
297.473333	14879.546902	28.436839
297.961140	14910.728492	28.441856
298.372265	14929.346380	28.446874
298.821321	14964.522815	28.451892
298.997252	14996.961582	28.456909
299.702941	15009.293873	28.461927
299.933716	15029.314198	28.466944
300.276588	15059.617083	28.471962
300.548180	15078.261346	28.476980
300.646112	15069.976930	28.481997
301.012150	15102.195403	28.487015
301.079254	15140.301725	28.492032
301.174416	15159.187965	28.497050
301.918118	15159.411815	28.502068
302.158476	15188.211212	28.507085
302.292880	15218.320341	28.512103
302.455339	15251.393748	28.517120
302.529530	15278.443225	28.522138
302.796641	15285.536066	28.527156
303.032466	15332.532589	28.532173
303.349781	15355.459041	28.537191
303.867592	15381.414256	28.542208
303.634950	15409.241105	28.547226
304.726826	15441.958067	28.552244
304.797095	15491.705464	28.557261
305.168982	15519.385351	28.562279
305.752473	15535.181473	28.567296
305.684348	15556.728404	28.572314
306.013606	15586.137859	28.577332
306.826890	15587.547876	28.582349
307.535631	15617.644803	28.587367
308.580114	15637.168996	28.592384
308.375278	15651.415600	28.597402
308.658454	15654.764844	28.602420
308.967979	15647.548283	28.607437
309.198574	15678.392485	28.612455
309.476429	15698.739941	28.617472
309.714396	15721.927432	28.622490
310.138238	15732.650600	28.627508
310.154032	15743.201656	28.632525
309.839188	15770.793714	28.637543
310.312224	15811.171570	28.642560
310.559386	15833.352288	28.647578
311.164341	15864.043593	28.652596
311.197703	15884.195291	28.657613
311.393501	15916.550665	28.662631
311.924633	15946.455345	28.667648
311.882314	15959.055348	28.672666
312.520281	15980.583893	28.677684
312.874496	16031.716945	28.682701
313.224986	16064.719967	28.687719
313.454182	16082.537159	28.692736
313.584036	16102.484077	28.697754
314.388331	16129.217360	28.702772
314.697238	16165.237449	28.707789
314.818619	16188.769503	28.712807
315.067325	16196.015496	28.717824
315.332702	16220.606464	28.722842
315.868291	16245.691793	28.727860
315.910672	16297.494957	28.732877
316.217117	16322.411814	28.737895
316.549441	16332.211244	28.742912
316.728391	16355.480304	28.747930
317.237528	16384.112916	28.752948
317.457420	16427.682844	28.757965
317.900314	16457.760635	28.762983
318.329782	16478.183303	28.768000
318.231876	16510.381929	28.773018
318.637857	16522.993406	28.778036
319.037989	16552.124986	28.783053
319.133726	16602.550800	28.788071
319.647505	16624.321350	28.793088
319.837266	16641.746950	28.798106
320.472283	16675.772706	28.803124
320.848918	16719.930569	28.808141
320.825068	16746.828475	28.813159
321.294712	16756.016062	28.818176
321.273353	16780.417272	28.823194
321.596323	16804.884559	28.828212
322.028402	16850.089519	28.833229
322.114482	16877.013605	28.838247
322.879475	16906.715935	28.843264
323.046761	16929.319520	28.848282
323.449722	16952.268744	28.853300
323.993865	16976.721813	28.858317
324.116282	17014.014891	28.863335
324.664521	17052.851530	28.868352
324.851200	17070.966810	28.873370
325.281001	17095.861316	28.878388
325.663654	17133.152649	28.883405
325.810554	17141.810650	28.888423
326.449674	17160.240557	28.893440
326.871808	17206.012356	28.898458
326.876890	17227.371306	28.903476
327.149974	17249.890088	28.908493
327.922316	17270.090045	28.913511
328.171619	17288.430047	28.918528
328.539330	17304.810421	28.923546
328.670451	17322.378821	28.928564
328.844271	17360.622420	28.933581
328.922243	17381.807199	28.938599
329.475937	17413.999243	28.943616
329.297614	17462.238163	28.948634
329.747509	17485.906936	28.953652
330.487506	17501.357604	28.958669
330.611045	17543.821128	28.963687
331.198418	17579.727408	28.968704
331.492278	17617.055000	28.973722
331.774210	17633.839161	28.978740
332.174452	17654.239760	28.983757
332.307375	17696.850278	28.988775
332.669278	17712.787571	28.993792
332.989746	17749.858900	28.998810
333.297029	17775.471304	29.003828
333.786597	17805.271204	29.008845
334.023171	17855.999127	29.013863
334.661933	17876.776684	29.018880
335.034774	17898.491837	29.023898
335.393211	17934.053727	29.028916
335.824235	17956.500105	29.033933
335.858534	17989.445772	29.038951
336.463366	17994.939434	29.043968
336.887600	18048.105108	29.048986
336.945399	18064.594181	29.054004
337.524011	18079.022377	29.059021
337.819416	18103.814533	29.064039
338.155089	18141.163204	29.069056
338.382632	18164.253435	29.074074
338.961684	18201.800028	29.079092
338.997180	18221.284403	29.084109
339.149734	18247.882959	29.089127
339.744511	18287.780292	29.094144
340.337437	18303.356889	29.099162
340.410761	18316.432925	29.104180
340.709457	18353.643184	29.109197
340.785277	18384.321042	29.114215
341.243748	18404.462351	29.119232
341.704582	18423.418043	29.124250
341.962085	18452.188840	29.129268
342.492686	18473.000783	29.134285
342.426338	18509.552983	29.139303
343.308374	18540.003373	29.144320
343.371895	18582.457428	29.149338
343.443630	18612.146565	29.154356
344.008451	18628.834573	29.159373
343.906347	18651.894835	29.164391
344.395515	18680.437044	29.169408
344.580320	18704.301106	29.174426
345.022541	18748.281794	29.179444
345.198997	18794.691246	29.184461
345.280351	18819.064329	29.189479
345.977557	18857.166626	29.194496
346.320545	18881.703057	29.199514
346.461979	18926.600809	29.204532
347.161679	18942.259674	29.209549
347.316206	18996.683475	29.214567
347.750486	19031.962529	29.219584
347.876793	19043.603936	29.224602
348.495014	19079.311376	29.229620
348.937066	19122.607445	29.234637
349.277793	19164.624729	29.239655
349.730938	19193.670282	29.244672
350.133675	19231.585662	29.249690
350.598639	19272.572346	29.254708
350.884898	19282.054881	29.259725
351.302379	19307.211701	29.264743
351.515713	19343.561921	29.269760
351.974449	19387.127038	29.274778
352.415189	19411.361236	29.279796
352.674981	19442.756224	29.284813
352.757568	19472.609043	29.289831
353.071742	19498.692708	29.294848
353.636989	19544.152616	29.299866
354.108207	19564.986786	29.304884
354.460328	19595.023853	29.309901
354.817248	19625.611868	29.314919
355.527417	19664.087460	29.319936
355.738579	19684.745644	29.324954
356.111432	19728.384171	29.329972
356.619976	19760.184748	29.334989
356.353606	19780.434877	29.340007
356.997702	19806.354185	29.345024
357.252773	19835.498218	29.350042
357.339577	19875.883686	29.355060
358.045455	19907.792235	29.360077
358.500181	19948.206946	29.365095
358.705546	19973.024669	29.370112
359.059010	20000.245438	29.375130
359.579577	20044.648537	29.380148
360.471308	20062.310157	29.385165
360.817524	20091.102256	29.390183
361.299672	20110.250253	29.395200
361.918700	20106.030749	29.400218
361.885668	20143.008229	29.405236
362.437651	20170.948377	29.410253
362.624214	20202.237105	29.415271
362.339830	20224.710184	29.420288
363.091201	20255.714973	29.425306
363.020254	20281.988024	29.430324
363.208723	20307.039179	29.435341
363.858809	20363.986524	29.440359
364.248223	20377.134925	29.445376
364.567361	20401.319730	29.450394
364.675826	20445.123621	29.455412
364.879704	20498.384030	29.460429
365.329947	20527.746097	29.465447
365.677773	20550.124631	29.470464
366.281055	20598.837861	29.475482
365.997909	20641.132201	29.480500
366.879438	20670.316080	29.485517
367.054063	20712.519214	29.490535
367.554930	20759.517425	29.495552
368.404119	20777.380732	29.500570
368.835807	20820.826404	29.505588
369.076109	20825.132769	29.510605
369.482519	20858.040017	29.515623
369.658250	20870.002428	29.520640
370.106849	20906.344007	29.525658
369.997486	20952.672730	29.530676
370.517147	20962.590585	29.535693
370.771420	20999.522506	29.540711
371.240614	21030.204912	29.545728
371.496285	21075.234638	29.550746
371.587856	21124.853665	29.555764
372.129011	21140.838752	29.560781
372.510624	21177.491503	29.565799
372.798605	21226.722121	29.570816
373.208282	21273.528765	29.575834
373.295950	21303.683552	29.580852
373.821069	21355.148552	29.585869
374.096959	21403.869357	29.590887
374.471638	21439.382505	29.595904
374.980299	21490.410821	29.600922
375.136846	21531.928543	29.605940
375.943080	21556.835387	29.610957
376.351901	21617.561444	29.615975
376.701656	21663.073792	29.620992
377.408776	21684.133346	29.626010
377.741075	21726.407586	29.631028
378.440917	21770.312747	29.636045
379.061829	21779.620044	29.641063
379.473072	21808.435905	29.646080
380.095556	21839.469676	29.651098
380.130068	21859.825538	29.656116
380.684667	21880.385577	29.661133
381.045291	21931.472804	29.666151
381.099680	21973.747863	29.671168
381.561066	21980.232946	29.676186
381.606201	22022.642081	29.681204
382.054966	22050.008111	29.686221
382.626443	22079.166865	29.691239
383.168030	22091.361364	29.696256
383.900168	22134.257930	29.701274
383.931953	22176.943970	29.706292
384.457342	22191.340420	29.711309
384.750628	22237.040228	29.716327
384.883957	22286.616394	29.721344
385.241319	22308.500697	29.726362
385.135827	22342.887491	29.731380
385.839229	22377.457607	29.736397
386.174151	22418.818791	29.741415
386.374555	22440.357139	29.746432
387.039787	22485.679302	29.751450
387.158455	22537.837817	29.756468
387.911098	22576.513357	29.761485
388.282088	22596.915428	29.766503
388.578571	22613.517784	29.771520
389.239881	22662.083995	29.776538
389.391350	22704.773678	29.781556
389.902766	22736.218446	29.786573
390.639785	22776.237090	29.791591
390.446077	22805.559779	29.796608
390.987767	22829.132749	29.801626
391.388171	22864.523283	29.806644
391.573103	22909.993731	29.811661
392.041416	22952.641163	29.816679
392.500051	22996.386015	29.821696
392.807813	23030.871490	29.826714
393.260577	23062.443225	29.831732
393.803995	23083.093305	29.836749
394.206064	23127.625095	29.841767
394.436209	23160.629063	29.846784
394.965558	23189.990633	29.851802
394.918196	23215.474528	29.856820
395.196906	23254.395468	29.861837
395.703362	23304.400169	29.866855
396.139253	23347.660950	29.871872
396.487840	23356.060278	29.876890
396.968408	23384.791725	29.881908
397.109850	23438.856964	29.886925
397.760846	23471.815669	29.891943
397.834606	23523.546365	29.896960
398.366425	23567.383095	29.901978
398.330790	23613.090534	29.906996
398.966359	23650.753630	29.912013
399.662419	23681.217385	29.917031
399.505640	23741.417074	29.922048
400.350193	23806.632405	29.927066
400.584997	23840.573462	29.932084
401.221071	23860.562769	29.937101
401.898095	23909.029086	29.942119
402.372769	23970.344031	29.947136
402.638366	24002.014670	29.952154
403.375939	24019.414291	29.957172
404.027276	24037.367395	29.962189
404.376439	24085.311322	29.967207
404.724096	24114.464870	29.972224
405.620466	24148.789182	29.977242
405.661630	24182.384514	29.982260
406.042103	24222.646824	29.987277
407.061660	24233.496281	29.992295
406.789012	24282.297141	29.997312
407.346064	24322.432765	30.002330
407.649941	24350.717314	30.007348
407.753247	24393.294678	30.012365
408.187494	24423.930741	30.017383
408.434008	24460.743857	30.022400
408.852744	24467.309487	30.027418
409.110908	24520.318286	30.032436
409.608984	24585.644323	30.037453
410.151937	24620.335439	30.042471
410.334060	24644.075996	30.047488
411.048104	24690.474520	30.052506
411.386229	24738.084706	30.057524
411.721721	24787.609613	30.062541
412.194645	24810.432010	30.067559
412.671844	24845.938586	30.072576
412.772901	24898.794776	30.077594
413.220568	24939.933825	30.082612
413.772905	24977.348742	30.087629
414.267546	25022.997625	30.092647
414.104133	25072.955822	30.097664
414.904855	25121.362615	30.102682
415.104993	25155.815029	30.107700
415.956507	25184.429928	30.112717
416.738878	25234.312780	30.117735
417.074758	25270.814885	30.122752
417.393623	25294.940576	30.127770
417.754986	25349.194770	30.132788
418.100878	25392.723216	30.137805
418.615472	25419.497293	30.142823
418.795539	25454.510236	30.147840
419.122176	25511.091727	30.152858
419.551781	25541.626513	30.157876
419.925627	25571.705408	30.162893
420.452178	25613.741303	30.167911
421.153367	25663.241473	30.172928
421.827555	25689.951770	30.177946
422.010710	25717.258844	30.182964
422.152338	25772.041079	30.187981
422.394563	25787.766198	30.192999
422.697104	25821.632237	30.198016
423.343460	25864.336459	30.203034
423.549843	25908.344978	30.208052
424.015472	25958.879907	30.213069
424.176988	25998.222312	30.218087
424.675811	26051.156720	30.223104
424.863679	26102.783412	30.228122
425.155329	26155.074319	30.233140
425.632914	26193.729489	30.238157
426.583611	26247.949121	30.243175
426.704154	26309.297918	30.248192
427.134990	26321.075420	30.253210
427.681625	26380.299418	30.258228
427.990916	26425.509625	30.263245
428.642766	26478.606157	30.268263
428.947189	26515.229668	30.273280
429.444332	26564.026605	30.278298
430.287937	26600.750461	30.283316
430.527252	26650.761874	30.288333
431.181481	26687.974504	30.293351
431.611278	26732.479664	30.298368
432.075854	26771.395333	30.303386
432.604870	26814.230131	30.308404
433.129687	26855.285383	30.313421
433.465369	26882.244282	30.318439
433.682541	26933.878110	30.323456
434.173403	26960.440920	30.328474
434.820708	27006.889919	30.333492
435.067514	27070.951853	30.338509
435.516130	27086.161534	30.343527
435.908410	27135.474167	30.348544
436.249508	27187.608683	30.353562
436.532057	27241.588612	30.358580
436.633378	27284.654514	30.363597
437.244311	27329.702170	30.368615
437.527214	27382.670071	30.373632
438.131909	27450.588355	30.378650
438.768734	27484.517595	30.383668
438.820553	27538.236946	30.388685
439.488700	27583.796227	30.393703
439.916412	27642.834508	30.398720
440.305251	27672.947753	30.403738
441.170896	27727.145138	30.408756
441.597751	27789.883721	30.413773
442.113932	27819.001596	30.418791
442.659155	27863.998433	30.423808
443.152508	27912.539639	30.428826
443.544175	27966.803462	30.433844
443.710697	28009.453541	30.438861
444.388272	28042.197538	30.443879
444.673794	28089.461484	30.448896
444.934454	28135.114776	30.453914
445.474090	28194.502342	30.458932
445.484990	28223.035701	30.463949
445.943265	28263.099165	30.468967
446.290014	28325.550145	30.473984
446.996381	28390.537796	30.479002
447.761905	28437.600399	30.484020
447.750222	28486.299198	30.489037
448.352567	28543.147983	30.494055
448.717483	28584.788928	30.499072
449.527332	28633.532225	30.504090
449.805500	28679.818060	30.509108
450.514355	28754.155680	30.514125
450.989975	28765.407032	30.519143
451.415928	28807.199297	30.524160
452.123004	28849.430976	30.529178
452.686108	28893.421362	30.534196
452.649763	28938.125958	30.539213
453.152009	28960.305609	30.544231
453.561648	29015.326789	30.549248
453.608993	29060.986231	30.554266
454.561174	29106.508945	30.559284
454.725894	29154.783056	30.564301
455.286655	29183.653003	30.569319
455.825999	29240.025584	30.574336
455.793630	29303.299763	30.579354
456.627396	29345.404484	30.584372
456.743366	29381.789245	30.589389
457.431868	29438.626755	30.594407
457.708329	29507.484288	30.599424
458.281553	29546.872496	30.604442
458.899940	29598.482752	30.609460
459.020098	29641.141374	30.614477
459.599426	29673.683905	30.619495
459.676443	29734.437025	30.624512
460.042129	29808.968361	30.629530
460.795923	29864.159358	30.634548
460.863697	29927.898746	30.639565
461.755848	29965.427749	30.644583
462.139833	30041.149432	30.649600
462.810906	30118.041640	30.654618
463.335826	30162.773401	30.659636
463.876855	30221.905900	30.664653
464.149448	30267.897237	30.669671
464.630159	30313.340137	30.674688
464.552325	30370.121181	30.679706
465.621037	30427.318683	30.684724
466.038425	30513.771688	30.689741
466.706305	30556.241143	30.694759
467.064526	30612.086608	30.699776
467.486617	30659.161529	30.704794
468.332868	30717.740574	30.709812
468.559411	30789.437927	30.714829
468.993037	30815.047695	30.719847
469.652025	30862.544604	30.724864
469.936984	30920.321148	30.729882
470.481100	30983.118212	30.734900
470.979397	31046.986178	30.739917
471.270976	31096.651700	30.744935
472.057215	31135.828523	30.749952
472.645314	31198.757904	30.754970
473.071712	31251.467911	30.759988
473.805290	31290.909310	30.765005
474.712389	31334.170829	30.770023
475.493580	31381.021191	30.775040
475.691591	31446.135846	30.780058
476.238175	31470.566998	30.785076
476.476112	31495.632787	30.790093
476.851528	31552.771857	30.795111
477.602540	31597.290150	30.800128
477.653590	31653.483085	30.805146
478.456829	31686.437226	30.810164
478.667203	31729.470950	30.815181
479.434822	31778.867345	30.820199
479.885858	31832.928428	30.825216
479.680332	31872.822816	30.830234
480.398377	31905.179419	30.835252
480.653494	31971.147852	30.840269
480.895830	32031.086679	30.845287
481.643816	32067.281176	30.850304
481.855291	32114.883817	30.855322
482.666919	32173.173775	30.860340
482.607452	32222.402028	30.865357
483.117564	32259.803502	30.870375
483.669284	32310.514773	30.875392
483.805219	32379.296467	30.880410
484.275376	32420.380293	30.885428
484.877132	32479.939492	30.890445
485.212498	32564.570613	30.895463
486.018213	32595.588963	30.900480
486.552638	32655.109402	30.905498
486.850654	32704.813139	30.910516
487.379385	32760.826613	30.915533
487.965285	32809.448279	30.920551
488.760547	32859.199671	30.925568
489.309777	32934.638458	30.930586
489.887239	32981.201809	30.935604
490.714282	33008.052816	30.940621
490.971770	33064.547451	30.945639
491.793860	33114.566465	30.950656
491.821429	33189.896909	30.955674
492.123838	33221.460135	30.960692
492.768923	33258.705785	30.965709
492.922939	33331.255310	30.970727
493.737977	33382.071319	30.975744
493.946351	33454.527188	30.980762
494.367319	33495.110540	30.985780
495.156581	33545.536897	30.990797
495.471878	33615.088882	30.995815
495.938090	33668.115100	31.000832
495.969811	33729.649977	31.005850
496.919501	33796.270920	31.010868
497.412592	33875.348240	31.015885
497.644909	33917.446635	31.020903
498.256482	33967.004339	31.025920
498.888868	34051.003544	31.030938
499.275838	34106.221227	31.035956
500.099149	34167.715223	31.040973
500.743285	34230.889193	31.045991
501.298516	34286.120663	31.051008
501.502859	34351.443829	31.056026
501.976483	34390.392458	31.061044
502.644405	34469.774861	31.066061
503.102705	34519.646563	31.071079
503.803757	34590.053692	31.076096
504.106914	34645.122831	31.081114
504.647824	34688.525700	31.086132
505.166713	34746.446593	31.091149
505.679136	34816.403023	31.096167
506.056482	34877.443066	31.101184
506.574592	34956.199251	31.106202
506.982820	34997.769469	31.111220
507.510020	35050.938068	31.116237
508.055202	35126.705594	31.121255
508.825409	35191.572372	31.126272
509.244312	35259.469773	31.131290
509.697187	35304.172930	31.136308
510.243209	35383.633209	31.141325
510.418653	35432.377242	31.146343
511.407560	35485.404618	31.151360
511.836363	35564.831428	31.156378
512.464566	35639.123313	31.161396
512.605969	35682.736603	31.166413
513.065458	35749.543701	31.171431
513.724566	35791.553970	31.176448
514.076495	35870.527836	31.181466
514.741969	35925.266578	31.186484
515.122297	35999.875441	31.191501
515.535965	36049.373847	31.196519
516.102229	36107.143050	31.201536
516.354567	36185.569924	31.206554
517.114565	36230.344593	31.211572
517.863037	36267.185069	31.216589
518.211474	36345.394820	31.221607
519.201553	36398.639310	31.226624
519.023885	36456.166477	31.231642
519.638756	36494.468438	31.236660
520.674761	36562.814804	31.241677
520.791017	36641.666923	31.246695
521.591720	36681.835118	31.251712
521.822420	36746.411699	31.256730
522.365543	36811.160959	31.261748
523.306781	36862.559385	31.266765
523.436438	36910.406196	31.271783
524.024054	36987.793495	31.276800
524.749938	37053.955593	31.281818
525.333576	37100.471963	31.286836
526.026873	37152.909379	31.291853
526.538364	37206.655043	31.296871
527.096451	37266.969705	31.301888
527.377883	37341.609980	31.306906
528.177955	37384.541134	31.311924
528.496662	37440.572548	31.316941
528.625978	37522.815677	31.321959
528.860994	37578.634129	31.326976
529.368708	37631.087822	31.331994
529.982815	37718.061196	31.337012
530.565482	37781.576673	31.342029
531.306712	37844.346656	31.347047
532.231985	37899.566099	31.352064
532.550498	37976.355172	31.357082
533.029213	38054.389925	31.362100
533.709729	38097.487707	31.367117
534.084177	38180.283506	31.372135
534.684754	38238.735602	31.377152
535.126169	38290.533124	31.382170
535.620424	38367.244344	31.387188
536.370359	38442.108467	31.392205
537.068046	38497.398900	31.397223
537.993820	38551.430477	31.402240
538.499075	38632.581437	31.407258
538.896168	38685.081728	31.412276
539.615723	38720.357208	31.417293
540.010852	38796.928834	31.422311
540.516075	38863.758943	31.427328
540.986281	38907.111170	31.432346
541.080983	38965.125284	31.437364
542.013055	39047.839280	31.442381
542.090975	39127.128398	31.447399
542.649293	39183.507547	31.452416
543.045857	39265.907018	31.457434
543.618901	39331.136993	31.462452
544.042884	39404.272605	31.467469
544.516256	39479.597012	31.472487
544.971909	39546.295809	31.477504
545.917489	39623.761577	31.482522
546.200076	39689.359590	31.487540
546.929379	39780.543669	31.492557
547.521463	39843.632467	31.497575
547.911783	39898.602379	31.502592
548.419743	39986.093440	31.507610
548.724584	40057.928924	31.512628
549.786519	40139.057826	31.517645
549.990675	40212.128855	31.522663
550.713337	40289.274479	31.527680
551.196017	40373.378610	31.532698
551.676790	40423.143109	31.537716
552.595228	40492.739010	31.542733
552.947904	40579.198065	31.547751
553.104751	40637.027357	31.552768
554.126395	40689.764878	31.557786
554.703430	40740.704283	31.562804
555.248464	40818.241315	31.567821
555.679761	40903.038155	31.572839
556.283419	40951.840054	31.577856
556.885560	41020.202419	31.582874
557.020561	41098.035628	31.587892
557.698594	41157.361843	31.592909
558.517427	41235.227884	31.597927
558.825633	41316.379220	31.602944
559.673719	41386.526756	31.607962
560.355668	41458.952557	31.612980
560.824586	41517.294947	31.617997
561.125180	41583.461827	31.623015
561.701723	41646.692024	31.628032
562.363921	41732.278426	31.633050
562.434670	41831.087729	31.638068
563.274256	41900.720976	31.643085
563.861595	41964.865886	31.648103
564.505884	42047.079217	31.653120
565.599382	42138.723166	31.658138
566.060526	42208.549513	31.663156
566.552390	42245.577179	31.668173
567.170372	42327.875032	31.673191
567.667176	42414.473648	31.678208
568.264334	42487.419431	31.683226
568.446591	42546.570044	31.688244
569.442254	42607.663579	31.693261
569.811984	42693.119694	31.698279
570.413955	42789.150624	31.703296
571.083943	42852.126486	31.708314
571.616860	42935.968958	31.713332
572.220667	42990.714054	31.718349
572.536221	43068.611048	31.723367
573.067764	43156.621643	31.728384
573.717279	43218.831897	31.733402
574.238607	43288.125231	31.738420
575.315749	43370.617089	31.743437
575.929015	43449.887078	31.748455
576.818974	43516.667555	31.753472
577.750867	43581.929230	31.758490
578.178856	43645.152973	31.763508
579.060355	43724.291449	31.768525
579.270264	43784.558998	31.773543
580.092286	43828.843452	31.778560
580.474869	43903.819121	31.783578
580.756625	43970.622776	31.788596
581.366602	44030.297850	31.793613
581.982853	44109.879560	31.798631
582.193919	44200.685115	31.803648
583.074267	44256.831017	31.808666
583.481828	44330.891938	31.813684
583.908427	44392.571563	31.818701
584.097461	44463.382711	31.823719
584.640282	44548.114831	31.828736
585.545676	44642.409997	31.833754
585.816919	44711.093321	31.838772
586.782183	44792.205143	31.843789
587.241388	44864.911618	31.848807
588.085825	44946.422917	31.853824
588.748633	45019.118468	31.858842
589.192523	45101.293289	31.863860
589.769412	45176.791352	31.868877
590.455513	45256.401180	31.873895
591.248643	45314.342148	31.878912
592.224002	45380.051306	31.883930
592.996229	45438.030842	31.888948
593.538048	45484.051454	31.893965
594.355072	45526.752758	31.898983
594.503538	45584.090684	31.904000
594.985056	45645.563347	31.909018
595.278527	45706.650524	31.914036
595.886715	45782.392138	31.919053
596.462031	45871.819684	31.924071
596.556716	45928.491908	31.929088
597.197620	45988.878554	31.934106
597.561214	46057.529499	31.939124
597.962122	46159.635152	31.944141
598.793547	46233.460001	31.949159
599.126569	46325.101942	31.954176
599.792303	46399.352632	31.959194
600.352754	46475.843755	31.964212
601.038784	46564.744851	31.969229
601.662991	46638.949678	31.974247
602.313725	46716.604564	31.979264
603.185391	46805.899232	31.984282
603.956868	46907.619400	31.989300
604.488671	46979.106541	31.994317
605.176680	47039.463545	31.999335
605.610867	47126.666016	32.004352
606.281019	47199.542517	32.009370
606.847101	47293.433532	32.014388
607.549188	47381.710680	32.019405
607.953925	47464.151809	32.024423
608.380437	47543.975299	32.029440
609.318114	47617.229185	32.034458
609.899880	47715.189744	32.039476
610.382730	47773.281161	32.044493
611.234572	47869.186569	32.049511
612.070802	47973.566792	32.054528
612.777795	48050.611657	32.059546
613.231527	48137.490360	32.064564
613.582285	48213.663237	32.069581
614.330211	48291.523305	32.074599
614.759252	48392.641814	32.079616
615.704026	48456.800652	32.084634
616.274284	48528.435745	32.089652
616.622531	48624.889192	32.094669
617.102270	48728.492533	32.099687
617.765134	48812.649451	32.104704
618.802056	48873.579944	32.109722
619.429567	48969.749042	32.114740
619.797244	49065.551036	32.119757
620.313805	49154.624993	32.124775
620.864229	49239.711818	32.129792
621.673912	49330.045508	32.134810
622.205413	49416.475157	32.139828
622.811066	49486.475448	32.144845
623.465261	49574.852875	32.149863
624.098521	49675.770833	32.154880
624.801018	49765.470626	32.159898
625.120038	49852.366823	32.164916
625.880415	49933.351579	32.169933
626.117904	50026.760983	32.174951
627.026892	50139.493814	32.179968
628.097321	50224.410750	32.184986
628.710853	50306.649788	32.190004
630.167919	50376.190631	32.195021
631.249544	50442.417858	32.200039
631.382782	50502.271230	32.205056
632.271553	50572.781413	32.210074
632.848331	50655.097504	32.215092
633.157336	50730.816847	32.220109
634.217850	50789.892688	32.225127
634.881089	50840.182328	32.230144
635.246329	50911.282358	32.235162
635.549968	50987.306778	32.240180
636.129130	51052.921181	32.245197
636.578085	51116.135061	32.250215
637.043271	51195.206448	32.255232
637.895841	51261.780690	32.260250
638.011203	51343.133776	32.265268
638.375139	51426.293665	32.270285
639.224687	51502.735276	32.275303
639.349559	51599.098582	32.280320
640.162394	51690.084058	32.285338
640.959557	51782.759033	32.290356
640.921068	51865.393549	32.295373
642.248193	51968.748245	32.300391
642.644942	52077.354564	32.305408
643.469675	52153.218594	32.310426
644.065647	52228.264813	32.315444
644.791832	52320.429834	32.320461
646.013611	52412.851386	32.325479
646.727152	52516.193510	32.330496
647.590039	52577.452012	32.335514
648.139577	52660.681346	32.340532
648.518682	52757.832800	32.345549
649.209681	52840.025713	32.350567
649.842248	52920.418871	32.355584
650.597831	53006.938293	32.360602
651.456285	53098.131358	32.365620
651.672584	53178.948084	32.370637
652.694992	53268.611466	32.375655
653.078315	53349.158121	32.380672
653.606285	53429.921265	32.385690
654.117632	53543.068273	32.390708
654.788085	53639.803346	32.395725
655.509665	53716.480195	32.400743
655.917265	53815.900079	32.405760
656.713607	53916.342811	32.410778
657.279579	54010.860742	32.415796
657.770979	54101.645376	32.420813
658.519431	54183.360727	32.425831
659.227720	54298.431629	32.430848
659.974685	54409.434829	32.435866
660.605302	54497.330288	32.440884
661.258885	54611.515025	32.445901
662.088456	54693.155952	32.450919
662.242146	54794.827536	32.455936
663.480821	54865.219860	32.460954
664.207552	54971.573686	32.465972
664.719119	55089.884702	32.470989
665.929116	55186.487836	32.476007
666.438593	55272.953778	32.481024
667.040403	55355.127864	32.486042
667.420793	55462.565013	32.491060
667.893277	55562.873891	32.496077
669.004137	55632.222419	32.501095
669.241385	55727.719037	32.506112
669.907981	55843.835735	32.511130
671.068758	55931.763825	32.516148
671.555495	56030.644938	32.521165
672.322463	56119.112742	32.526183
672.742062	56222.175663	32.531200
673.504124	56309.451065	32.536218
673.951894	56415.252304	32.541236
674.614037	56501.369932	32.546253
675.436676	56610.736808	32.551271
675.873057	56729.967308	32.556288
676.891135	56826.919825	32.561306
677.583067	56896.228296	32.566324
678.487549	56963.814981	32.571341
679.393891	57061.854867	32.576359
679.869317	57151.209463	32.581376
680.454636	57239.901862	32.586394
680.885725	57313.121600	32.591412
681.449974	57406.556873	32.596429
682.415326	57490.379472	32.601447
683.080506	57594.021895	32.606464
683.295018	57678.108294	32.611482
684.116046	57771.597664	32.616500
684.628082	57864.361348	32.621517
685.540084	57976.431632	32.626535
686.112293	58076.547316	32.631552
686.819901	58175.743924	32.636570
687.527596	58280.090592	32.641588
688.083840	58362.986136	32.646605
689.052107	58434.939752	32.651623
689.548048	58551.795646	32.656640
690.266167	58658.442552	32.661658
690.897179	58767.688747	32.666676
691.592512	58867.446886	32.671693
692.804162	58952.915780	32.676711
693.519991	59066.414745	32.681728
694.243467	59165.133457	32.686746
694.941121	59241.406189	32.691764
695.484925	59342.392310	32.696781
696.134959	59442.205046	32.701799
696.713498	59552.146655	32.706816
697.338719	59660.773140	32.711834
698.073749	59735.777806	32.716852
698.516383	59841.326498	32.721869
699.265114	59970.433108	32.726887
700.108582	60075.961077	32.731904
700.590764	60163.021663	32.736922
701.433942	60261.163634	32.741940
702.147351	60393.109778	32.746957
703.034836	60494.828548	32.751975
703.545667	60606.954629	32.756992
704.073383	60726.288841	32.762010
704.747876	60817.093120	32.767028
705.303560	60923.008004	32.772045
706.354072	61051.736825	32.777063
706.974301	61154.078140	32.782080
707.295956	61268.305603	32.787098
708.491182	61371.652652	32.792116
708.888996	61496.055834	32.797133
710.190506	61599.936303	32.802151
710.802708	61705.346730	32.807168
711.399682	61818.318487	32.812186
712.556521	61930.610690	32.817204
712.880425	62055.048487	32.822221
713.516251	62166.271540	32.827239
714.211398	62265.035480	32.832256
715.076242	62378.136766	32.837274
715.604222	62475.222996	32.842292
716.033156	62614.732317	32.847309
716.763033	62713.359994	32.852327
717.355366	62826.843746	32.857344
717.888023	62953.489848	32.862362
719.062333	63051.704499	32.867380
719.789201	63187.547197	32.872397
720.655043	63312.623706	32.877415
721.304015	63421.576250	32.882432
722.093863	63523.598187	32.887450
723.505336	63609.970337	32.892468
724.358404	63713.322664	32.897485
725.316815	63808.239559	32.902503
726.310206	63902.955193	32.907520
726.701454	63987.158929	32.912538
727.653055	64053.864320	32.917556
728.437739	64143.445522	32.922573
728.979496	64228.851547	32.927591
729.197446	64336.641374	32.932608
729.785392	64442.133233	32.937626
730.394520	64516.013503	32.942644
730.682880	64617.428482	32.947661
731.193941	64739.759722	32.952679
731.996170	64855.097309	32.957696
732.212397	64955.268080	32.962714
733.240793	65071.726207	32.967732
733.970018	65203.947580	32.972749
734.698177	65339.071187	32.977767
735.299109	65438.839469	32.982784
735.964018	65556.542353	32.987802
736.675349	65678.302528	32.992820
737.223451	65805.336688	32.997837
738.061736	65909.770775	33.002855
739.147269	66048.025751	33.007872
739.968604	66177.678198	33.012890
740.810328	66290.204487	33.017908
741.732725	66414.892391	33.022925
742.271567	66527.830293	33.027943
743.887510	66632.651628	33.032960
744.631188	66729.779330	33.037978
745.382750	66825.686200	33.042996
745.808097	66947.418918	33.048013
746.671891	67080.793211	33.053031
747.710732	67170.377242	33.058048
748.162106	67270.924992	33.063066
749.398165	67379.611952	33.068084
750.077134	67490.509138	33.073101
750.647360	67602.341478	33.078119
751.481873	67712.126880	33.083136
751.889898	67829.575378	33.088154
752.429854	67931.603563	33.093172
752.976350	68059.246042	33.098189
753.830292	68170.332891	33.103207
755.109510	68294.657096	33.108224
755.190593	68418.377049	33.113242
756.114784	68557.604691	33.118260
756.524537	68674.216876	33.123277
757.240495	68788.642389	33.128295
758.246894	68900.131504	33.133312
758.828857	69037.111399	33.138330
759.521243	69163.750329	33.143348
760.502492	69303.289606	33.148365
760.882362	69435.760020	33.153383
762.377996	69542.683178	33.158400
762.588459	69682.870667	33.163418
763.560006	69805.301151	33.168436
764.508211	69925.346448	33.173453
764.773621	70053.009566	33.178471
765.648722	70200.626745	33.183488
765.938182	70339.376746	33.188506
767.247153	70458.303371	33.193524
768.072248	70586.983695	33.198541
768.456517	70716.983100	33.203559
769.642779	70830.810993	33.208576
770.251164	70961.274359	33.213594
771.032050	71109.280152	33.218612
772.028488	71247.046865	33.223629
772.758581	71367.857150	33.228647
773.737931	71480.647877	33.233664
774.179181	71612.666594	33.238682
775.508823	71738.627752	33.243700
776.263776	71860.682299	33.248717
777.257083	71972.683003	33.253735
778.230687	72058.220536	33.258752
778.817506	72178.850445	33.263770
779.570309	72300.667607	33.268788
780.423326	72390.348864	33.273805
781.035128	72507.385134	33.278823
781.859581	72607.232884	33.283840
782.279825	72717.511141	33.288858
783.100630	72833.939301	33.293876
783.915840	72959.651195	33.298893
784.509684	73073.993611	33.303911
785.399265	73190.892910	33.308928
785.815649	73317.437858	33.313946
786.648787	73451.856613	33.318964
787.203334	73593.271406	33.323981
787.986346	73719.315559	33.328999
788.736365	73852.466934	33.334016
789.077097	74007.394657	33.339034
789.871462	74126.654406	33.344052
790.950158	74244.647450	33.349069
791.621105	74394.565896	33.354087
792.523046	74531.692795	33.359104
793.267282	74685.806272	33.364122
794.291618	74825.064821	33.369140
795.035451	74959.318033	33.374157
795.680668	75102.321306	33.379175
796.584645	75219.918530	33.384192
797.402368	75364.665679	33.389210
798.113049	75525.487496	33.394228
799.239345	75659.473210	33.399245
799.876351	75786.299754	33.404263
800.880019	75923.336465	33.409280
801.565010	76083.578538	33.414298
802.763829	76220.553279	33.419316
803.921965	76350.844807	33.424333
804.504546	76477.899387	33.429351
805.503745	76607.991033	33.434368
806.034980	76761.958382	33.439386
806.648534	76913.162212	33.444404
807.532201	77037.147379	33.449421
808.160523	77177.188386	33.454439
809.059122	77320.657688	33.459456
809.896872	77456.618360	33.464474
810.507041	77603.533304	33.469492
811.082691	77764.020786	33.474509
812.058280	77920.832136	33.479527
812.948887	78042.835969	33.484544
813.943865	78177.971936	33.489562
815.212031	78334.554514	33.494580
816.116833	78480.857458	33.499597
816.746847	78597.265840	33.504615
817.942695	78723.726195	33.509632
818.538042	78872.024513	33.514650
819.051921	79026.598801	33.519668
819.822033	79155.326624	33.524685
820.433156	79286.617713	33.529703
821.814948	79395.816013	33.534720
823.024476	79553.631298	33.539738
823.800084	79679.666846	33.544756
824.938771	79808.464104	33.549773
825.587420	79946.318249	33.554791
825.986525	80086.592683	33.559808
826.998060	80207.500585	33.564826
827.762339	80324.161526	33.569844
828.393606	80470.605008	33.574861
828.943148	80628.189020	33.579879
829.686263	80756.443538	33.584896
830.521268	80874.816155	33.589914
831.268352	81019.479356	33.594932
832.089737	81171.468666	33.599949
832.491522	81297.948293	33.604967
833.702413	81418.937374	33.609984
834.547500	81560.007682	33.615002
835.333430	81700.753393	33.620020
836.630086	81830.459768	33.625037
837.154776	81957.555378	33.630055
838.429505	82092.972585	33.635072
839.118181	82226.785773	33.640090
839.888408	82345.259086	33.645108
840.747798	82481.202664	33.650125
841.550516	82616.093689	33.655143
842.343497	82757.420493	33.660160
843.006287	82889.502286	33.665178
843.505642	83024.123221	33.670196
844.336556	83181.153631	33.675213
845.078515	83345.860594	33.680231
845.845700	83472.032726	33.685248
846.625846	83618.276025	33.690266
847.310124	83795.635265	33.695284
848.477580	83953.482132	33.700301
849.171213	84094.909598	33.705319
850.229188	84237.112847	33.710336
851.482233	84394.189492	33.715354
852.040262	84573.479853	33.720372
852.802935	84709.427456	33.725389
853.554487	84863.831846	33.730407
854.357898	85018.918300	33.735424
855.186798	85171.572220	33.740442
855.814144	85349.446411	33.745460
856.791790	85505.045144	33.750477
857.425330	85666.180617	33.755495
858.277890	85836.809036	33.760512
859.006546	86010.900922	33.765530
860.228111	86190.657450	33.770548
861.135879	86343.786976	33.775565
862.157103	86508.824927	33.780583
863.054576	86654.036979	33.785600
863.898432	86828.780345	33.790618
864.595687	87002.783672	33.795636
866.020265	87157.769325	33.800653
866.546926	87308.949852	33.805671
867.242446	87474.073780	33.810688
868.224562	87638.550479	33.815706
869.197507	87815.013615	33.820724
870.950189	87966.894453	33.825741
871.838582	88121.785264	33.830759
872.700106	88255.908868	33.835776
873.764858	88401.395299	33.840794
874.413339	88575.399475	33.845812
875.367425	88725.417657	33.850829
875.945444	88872.974221	33.855847
876.896410	89020.210706	33.860864
877.618095	89181.798986	33.865882
878.733898	89352.308549	33.870900
879.334467	89493.101050	33.875917
880.145124	89666.415821	33.880935
881.276213	89820.841197	33.885952
881.966614	89971.417112	33.890970
882.601294	90144.935315	33.895988
883.456428	90299.890315	33.901005
884.180152	90455.557776	33.906023
884.890932	90630.364209	33.911040
886.062177	90798.945062	33.916058
886.974753	90968.101385	33.921076
887.934835	91110.926119	33.926093
888.564077	91274.151347	33.931111
889.518941	91423.617060	33.936128
890.390279	91567.534989	33.941146
890.984016	91731.408373	33.946164
891.689260	91876.545312	33.951181
892.339788	92047.100520	33.956199
893.805742	92220.515644	33.961216
894.369123	92388.929699	33.966234
895.332631	92556.905493	33.971252
896.254016	92712.966458	33.976269
897.172692	92880.027958	33.981287
897.723509	93042.999784	33.986304
899.181707	93202.785137	33.991322
899.641965	93375.665880	33.996340
900.682610	93550.774690	34.001357
901.517837	93732.855060	34.006375
902.124848	93914.968159	34.011392
903.029704	94078.204986	34.016410
904.197708	94252.082717	34.021428
905.168931	94427.209357	34.026445
905.852877	94614.333913	34.031463
906.867672	94784.797778	34.036480
908.114852	94958.553592	34.041498
908.817287	95144.913367	34.046516
910.347400	95312.979382	34.051533
911.377392	95502.908132	34.056551
912.062935	95660.754992	34.061568
912.995459	95820.764709	34.066586
913.613895	96013.835128	34.071604
914.606000	96190.895171	34.076621
915.429715	96362.199145	34.081639
916.407223	96539.131199	34.086656
917.721530	96725.022247	34.091674
918.091946	96913.526448	34.096692
919.250458	97091.882090	34.101709
920.295568	97261.567043	34.106727
921.135249	97433.236652	34.111744
921.550286	97622.701043	34.116762
922.626487	97824.268029	34.121780
923.666450	97996.984571	34.126797
924.599974	98180.423848	34.131815
925.245763	98380.186436	34.136832
926.720462	98555.753234	34.141850
927.803767	98726.594015	34.146868
929.102239	98919.657226	34.151885
929.583284	99084.592600	34.156903
930.481819	99259.759421	34.161920
931.852936	99437.615776	34.166938
932.891823	99627.441923	34.171956
933.685826	99790.589457	34.176973
934.689369	99977.765348	34.181991
935.665635	100166.073965	34.187008
936.818511	100334.445397	34.192026
937.514996	100515.953233	34.197044
938.430418	100682.910182	34.202061
939.703653	100887.286539	34.207079
940.530828	101052.133415	34.212096
941.513694	101220.893374	34.217114
942.079582	101418.180129	34.222132
943.247139	101565.026416	34.227149
944.300232	101736.019332	34.232167
944.957526	101915.454532	34.237184
946.095687	102095.501682	34.242202
946.486453	102293.837125	34.247220
947.814344	102457.641848	34.252237
948.737021	102630.688261	34.257255
949.262713	102821.484223	34.262272
950.424046	102986.339161	34.267290
951.286173	103180.988595	34.272308
952.364101	103351.450127	34.277325
953.258321	103510.629098	34.282343
954.215968	103683.771848	34.287360
954.984642	103854.724654	34.292378
955.824560	104057.115035	34.297396
956.681580	104223.028552	34.302413
957.348730	104378.812412	34.307431
958.358130	104571.149747	34.312448
959.330188	104765.286527	34.317466
960.211465	104963.207090	34.322484
961.185140	105143.378823	34.327501
962.345335	105315.232768	34.332519
963.037491	105519.843474	34.337536
963.916638	105712.217138	34.342554
964.818105	105897.857751	34.347572
965.723534	106108.104915	34.352589
967.258973	106305.053910	34.357607
968.101404	106492.538455	34.362624
968.926611	106665.672388	34.367642
969.574649	106878.222474	34.372660
970.971895	107097.805945	34.377677
971.629994	107292.564334	34.382695
972.319797	107494.246434	34.387712
973.863886	107678.679125	34.392730
975.075603	107883.659502	34.397748
976.188595	108071.927549	34.402765
977.243832	108272.250804	34.407783
977.629894	108475.788986	34.412800
979.155401	108666.830133	34.417818
979.861852	108886.289272	34.422836
980.751923	109104.415384	34.427853
981.854891	109302.813431	34.432871
982.871217	109498.706830	34.437888
983.869266	109692.502201	34.442906
984.819717	109915.323928	34.447924
985.842121	110105.407231	34.452941
987.230573	110306.349437	34.457959
988.263427	110520.043171	34.462976
989.052781	110712.512470	34.467994
990.050031	110919.603578	34.473012
990.656407	111133.587934	34.478029
992.026923	111321.557785	34.483047
992.814146	111532.032201	34.488064
993.850715	111743.366417	34.493082
994.963230	111956.779746	34.498100
997.217098	112110.307974	34.503117
998.382896	112290.300333	34.508135
999.177343	112501.262438	34.513152
1000.369484	112692.805343	34.518170
1001.479503	112883.476459	34.523188
1001.861544	113057.333089	34.528205
1002.902228	113261.572172	34.533223
1003.598724	113480.766424	34.538240
1004.485606	113660.053847	34.543258
1005.448679	113851.148673	34.548276
1006.294236	114058.453462	34.553293
1007.274839	114251.853696	34.558311
1008.036895	114457.807170	34.563328
1009.007222	114666.476738	34.568346
1010.065660	114890.372955	34.573364
1010.752191	115088.666796	34.578381
1012.028904	115309.756061	34.583399
1013.067917	115528.023299	34.588416
1013.908653	115729.083295	34.593434
1015.351453	115932.553711	34.598452
1016.192750	116140.318222	34.603469
1017.403704	116329.058250	34.608487
1018.279101	116525.722253	34.613504
1019.351514	116724.546826	34.618522
1020.305871	116926.762242	34.623540
1020.999168	117119.533113	34.628557
1022.372341	117298.789147	34.633575
1023.104035	117504.719534	34.638592
1024.433136	117716.482032	34.643610
1025.448303	117903.706672	34.648628
1026.949491	118086.202624	34.653645
1028.220184	118284.739450	34.658663
1029.120874	118477.003937	34.663680
1030.340292	118657.092187	34.668698
1030.952339	118844.985093	34.673716
1031.869143	119038.986495	34.678733
1033.204789	119259.869126	34.683751
1034.046196	119451.605193	34.688768
1034.923790	119650.710608	34.693786
1035.721824	119862.019330	34.698804
1036.427470	120070.101257	34.703821
1037.438309	120258.406445	34.708839
1038.633282	120490.547822	34.713856
1039.512902	120704.421406	34.718874
1040.502441	120925.754160	34.723892
1041.168414	121141.972338	34.728909
1042.485371	121358.768894	34.733927
1043.317689	121589.851291	34.738944
1044.427880	121798.411107	34.743962
1045.654969	122027.189036	34.748980
1046.511508	122277.786583	34.753997
1047.419175	122487.474517	34.759015
1048.110859	122702.623019	34.764032
1049.281334	122955.113303	34.769050
1050.646099	123180.620960	34.774068
1051.829484	123405.488693	34.779085
1052.869593	123652.849093	34.784103
1054.282152	123903.698255	34.789120
1055.554952	124111.842247	34.794138
1056.495245	124317.394112	34.799156
1057.072349	124562.506906	34.804173
1058.688940	124816.080034	34.809191
1059.393325	125048.224636	34.814208
1060.510559	125255.046398	34.819226
1061.464945	125488.673881	34.824244
1062.627462	125739.769974	34.829261
1063.840065	125955.071635	34.834279
1064.950466	126203.962480	34.839296
1065.719823	126447.373549	34.844314
1066.996232	126671.769121	34.849332
1067.829922	126926.097750	34.854349
1069.168772	127144.973659	34.859367
1070.305174	127395.175441	34.864384
1071.538899	127625.389631	34.869402
1072.644106	127843.447371	34.874420
1073.485143	128087.823050	34.879437
1075.164701	128317.943554	34.884455
1076.196139	128536.309949	34.889472
1077.227972	128772.206087	34.894490
1078.320651	128993.924280	34.899508
1079.276942	129220.127937	34.904525
1080.452533	129464.231281	34.909543
1081.671394	129693.373560	34.914560
1082.543734	129916.541666	34.919578
1084.017667	130150.132031	34.924596
1084.944901	130384.828397	34.929613
1085.983447	130596.706144	34.934631
1086.942579	130822.616912	34.939648
1087.872107	131065.493384	34.944666
1089.195437	131291.334767	34.949684
1089.940255	131516.107172	34.954701
1090.703153	131748.686196	34.959719
1091.449129	131990.636861	34.964736
1092.372956	132206.283749	34.969754
1093.467227	132424.730636	34.974772
1094.442315	132667.434588	34.979789
1095.675647	132926.791772	34.984807
1096.443201	133157.580511	34.989824
1097.691973	133376.654969	34.994842
1098.853800	133617.801618	34.999860
1099.302004	133881.415962	35.004877
1100.276017	134143.132988	35.009895
1101.480004	134399.730980	35.014912
1102.420541	134664.969171	35.019930
1104.009727	134919.086546	35.024948
1104.992672	135164.115434	35.029965
1106.245051	135425.949136	35.034983
1107.342519	135698.814070	35.040000
1108.119438	135945.987290	35.045018
1109.949215	136182.770880	35.050036
1110.636857	136458.194592	35.055053
1111.745335	136737.924835	35.060071
1113.074085	136993.990475	35.065088
1114.048317	137246.389474	35.070106
1115.621066	137522.081764	35.075124
1116.588148	137795.366179	35.080141
1117.784581	138044.463816	35.085159
1118.706735	138298.844586	35.090176
1119.682722	138565.085033	35.095194
1121.193757	138835.993591	35.100212
1122.515615	139128.780141	35.105229
1123.579314	139375.551599	35.110247
1124.693018	139628.605121	35.115264
1125.628832	139907.427285	35.120282
1126.886889	140158.140837	35.125300
1128.148020	140440.539832	35.130317
1129.325325	140702.174481	35.135335
1130.470650	140967.531368	35.140352
1131.909246	141257.997090	35.145370
1133.181734	141522.056777	35.150388
1133.986972	141769.864838	35.155405
1134.796006	142032.458150	35.160423
1136.402222	142304.875231	35.165440
1137.335741	142590.351319	35.170458
1138.344024	142841.633224	35.175476
1139.798805	143094.149281	35.180493
1141.224358	143352.479372	35.185511
1142.376284	143631.727680	35.190528
1143.882299	143908.130205	35.195546
1145.162688	144141.700801	35.200564
1146.336105	144392.446910	35.205581
1147.510470	144668.479141	35.210599
1148.703554	144944.637281	35.215616
1149.203635	145188.500723	35.220634
1150.824775	145427.970871	35.225652
1151.728049	145701.684780	35.230669
1152.683195	145963.383597	35.235687
1154.182012	146228.887639	35.240704
1154.814399	146511.250188	35.245722
1155.720100	146780.127976	35.250740
1157.064124	147042.087641	35.255757
1157.993811	147306.489029	35.260775
1159.294612	147587.532432	35.265792
1160.293615	147871.493875	35.270810
1161.347352	148135.018602	35.275828
1162.555791	148416.895402	35.280845
1163.704142	148708.257584	35.285863
1164.876718	148966.138117	35.290880
1165.500391	149235.562867	35.295898
1166.929869	149507.519833	35.300916
1167.869039	149781.322590	35.305933
1169.060743	150049.822614	35.310951
1170.207943	150308.122725	35.315968
1171.443348	150595.947370	35.320986
1172.474211	150857.847006	35.326004
1173.692751	151118.715611	35.331021
1174.602727	151395.756662	35.336039
1175.964376	151693.943500	35.341056
1177.000017	151976.573954	35.346074
1178.396970	152247.136164	35.351092
1179.229688	152542.297137	35.356109
1180.303442	152823.532611	35.361127
1181.967890	153109.593800	35.366144
1182.964122	153406.040987	35.371162
1184.228994	153694.721955	35.376180
1185.483976	153971.852065	35.381197
1186.587103	154280.375911	35.386215
1188.141001	154544.650408	35.391232
1189.059442	154843.595061	35.396250
1190.296799	155137.872472	35.401268
1191.519713	155439.447854	35.406285
1193.088434	155729.400611	35.411303
1193.992524	156006.983998	35.416320
1194.898364	156322.038561	35.421338
1196.479683	156615.585584	35.426356
1197.669512	156903.034785	35.431373
1198.850040	157202.106752	35.436391
1200.421737	157498.668302	35.441408
1201.617258	157786.211886	35.446426
1202.770071	158089.861763	35.451444
1204.185116	158377.056328	35.456461
1205.125585	158688.293450	35.461479
1206.862677	158961.980246	35.466496
1208.073288	159263.092592	35.471514
1209.700450	159545.655890	35.476532
1211.113931	159814.949429	35.481549
1212.108861	160099.587258	35.486567
1213.327176	160391.826990	35.491584
1214.318454	160697.591253	35.496602
1215.704553	160967.683576	35.501620
1217.071455	161259.181992	35.506637
1218.193450	161565.920758	35.511655
1219.283252	161846.749470	35.516672
1220.321348	162141.746428	35.521690
1221.929390	162431.272463	35.526708
1222.856721	162703.075889	35.531725
1224.221878	163015.862176	35.536743
1225.434597	163318.273035	35.541760
1226.335834	163606.782223	35.546778
1227.476523	163906.342090	35.551796
1228.530447	164188.207648	35.556813
1229.815381	164492.239053	35.561831
1230.952720	164816.659658	35.566848
1232.329432	165102.436443	35.571866
1233.368967	165405.360447	35.576884
1234.317346	165718.984349	35.581901
1235.726867	166039.119201	35.586919
1236.982737	166319.164093	35.591936
1238.069233	166624.017539	35.596954
1239.390831	166951.760907	35.601972
1241.314904	167270.284857	35.606989
1242.173463	167566.732597	35.612007
1243.971098	167854.272717	35.617024
1245.161636	168165.768374	35.622042
1246.408093	168442.872339	35.627060
1247.924703	168731.111741	35.632077
1248.881581	169040.368345	35.637095
1250.377896	169313.173334	35.642112
1251.142770	169595.807374	35.647130
1252.180832	169871.178383	35.652148
1254.204507	170139.295517	35.657165
1255.605976	170431.815722	35.662183
1257.019164	170688.223804	35.667200
1258.267965	170969.885817	35.672218
1259.414489	171248.660728	35.677236
1260.394015	171535.370153	35.682253
1261.191178	171850.154285	35.687271
1262.270593	172121.497198	35.692288
1263.587448	172411.201885	35.697306
1264.430932	172703.270618	35.702324
1265.347171	173027.737860	35.707341
1266.289324	173356.695191	35.712359
1267.614781	173662.001728	35.717376
1268.842745	173970.892162	35.722394
1270.050063	174288.848523	35.727412
1271.234111	174632.127070	35.732429
1272.229863	174959.805255	35.737447
1273.511564	175280.852429	35.742464
1274.755011	175609.471393	35.747482
1275.893305	175956.561504	35.752500
1277.346643	176286.584516	35.757517
1278.388177	176613.517888	35.762535
1279.782346	176960.027398	35.767552
1281.348345	177319.125436	35.772570
1282.186968	177658.637665	35.777588
1283.879634	178006.793288	35.782605
1284.669042	178359.250382	35.787623
1286.299968	178698.410670	35.792640
1287.662212	179062.111251	35.797658
1289.128058	179424.832899	35.802676
1290.302198	179756.017035	35.807693
1291.653654	180114.853738	35.812711
1293.011183	180462.904377	35.817728
1294.625065	180809.417537	35.822746
1296.052129	181166.954777	35.827764
1297.311424	181513.632837	35.832781
1298.493017	181858.282727	35.837799
1299.842192	182226.805919	35.842816
1301.125626	182564.983653	35.847834
1301.929656	182932.231166	35.852852
1303.886491	183277.257628	35.857869
1305.308198	183639.052169	35.862887
1307.018005	183977.409914	35.867904
1308.583860	184319.791681	35.872922
1309.998853	184645.027789	35.877940
1311.627047	184996.415255	35.882957
1312.682524	185362.864086	35.887975
1314.089680	185680.289230	35.892992
1315.008317	186015.008188	35.898010
1316.528602	186352.790433	35.903028
1317.927701	186703.198807	35.908045
1319.829620	187042.090115	35.913063
1321.142013	187354.108164	35.918080
1322.823237	187683.964377	35.923098
1323.561435	188026.887165	35.928116
1325.210719	188350.824934	35.933133
1326.212649	188691.626622	35.938151
1327.282422	189028.573097	35.943168
1328.620668	189368.257162	35.948186
1329.855228	189705.193198	35.953204
1331.406011	190043.513432	35.958221
1332.449352	190394.397346	35.963239
1333.735333	190733.857048	35.968256
1335.242267	191083.437381	35.973274
1336.047933	191418.766040	35.978292
1337.457450	191729.294451	35.983309
1338.386420	192047.494884	35.988327
1339.996087	192394.552741	35.993344
1341.240021	192744.592682	35.998362
1342.310189	193068.043446	36.003380
1343.779769	193402.017153	36.008397
1344.867567	193769.213610	36.013415
1346.222011	194122.772484	36.018432
1347.085011	194463.694567	36.023450
1348.179516	194809.531280	36.028468
1349.722228	195164.982067	36.033485
1350.669131	195540.311764	36.038503
1352.380270	195920.405154	36.043520
1353.738693	196274.559810	36.048538
1355.080959	196638.278509	36.053556
1356.685675	196999.328124	36.058573
1357.697950	197382.986146	36.063591
1358.823243	197743.992196	36.068608
1360.004026	198130.724574	36.073626
1361.108338	198526.523737	36.078644
1362.757490	198920.750043	36.083661
1363.879863	199296.530160	36.088679
1365.203004	199688.745552	36.093696
1367.260944	200067.079868	36.098714
1368.627854	200453.668397	36.103732
1370.473679	200839.989702	36.108749
1371.586864	201242.405637	36.113767
1373.039409	201627.260175	36.118784
1374.528975	202003.997997	36.123802
1375.655044	202388.072786	36.128820
1377.280145	202774.035282	36.133837
1378.461684	203188.881032	36.138855
1380.033810	203581.585809	36.143872
1381.619727	203955.753715	36.148890
1382.822957	204339.001284	36.153908
1384.519984	204740.058905	36.158925
1386.187826	205148.259113	36.163943
1387.138191	205520.864180	36.168960
1388.994916	205910.094032	36.173978
1389.799724	206313.783522	36.178996
1391.291877	206682.153240	36.184013
1392.550027	207088.121085	36.189031
1394.058441	207489.415418	36.194048
1395.668652	207893.945561	36.199066
1396.651919	208287.344323	36.204084
1398.300479	208684.266738	36.209101
1399.598649	209113.411347	36.214119
1400.749085	209524.374658	36.219136
1401.862966	209916.833276	36.224154
1403.127123	210332.340450	36.229172
1404.987421	210735.777598	36.234189
1406.489686	211158.741374	36.239207
1407.875350	211559.886541	36.244224
1409.652239	211952.423526	36.249242
1411.055220	212382.012912	36.254260
1412.422369	212793.211182	36.259277
1413.999887	213199.335675	36.264295
1415.269999	213603.836727	36.269312
1416.406325	213999.523923	36.274330
1417.660792	214423.789692	36.279348
1419.725220	214808.965777	36.284365
1420.667975	215232.550465	36.289383
1421.890332	215667.570353	36.294400
1423.369232	216060.594561	36.299418
1424.809460	216476.204723	36.304436
1426.301950	216888.379586	36.309453
1427.942405	217314.500325	36.314471
1429.152397	217737.671812	36.319488
1430.875270	218180.545144	36.324506
1432.056991	218571.267265	36.329524
1433.576612	218942.302917	36.334541
1434.736272	219360.181944	36.339559
1436.199174	219767.142491	36.344576
1437.740499	220163.500885	36.349594
1438.854332	220555.816955	36.354612
1440.422139	220977.546861	36.359629
1441.555071	221393.153152	36.364647
1443.227458	221801.078038	36.369664
1444.693081	222198.879315	36.374682
1445.905283	222617.144354	36.379700
1447.303516	223043.812716	36.384717
1448.744905	223470.729677	36.389735
1450.037467	223888.961117	36.394752
1451.849311	224298.142676	36.399770
1452.886355	224738.694422	36.404788
1454.325292	225176.895693	36.409805
1455.587004	225615.077138	36.414823
1457.277790	226038.432482	36.419840
1459.004489	226478.166091	36.424858
1460.330017	226930.591135	36.429876
1461.922925	227351.452902	36.434893
1463.585503	227784.039328	36.439911
1464.924926	228220.185815	36.444928
1466.640982	228675.194626	36.449946
1467.948110	229110.816227	36.454964
1469.415942	229548.495637	36.459981
1470.733306	229991.840227	36.464999
1472.046532	230460.282466	36.470016
1473.802319	230904.345254	36.475034
1475.112299	231340.100970	36.480052
1476.802025	231795.506223	36.485069
1478.441722	232249.346425	36.490087
1479.481523	232715.250827	36.495104
1481.325915	233150.441515	36.500122
1482.504445	233593.465264	36.505140
1484.096461	234054.355174	36.510157
1485.546191	234531.120223	36.515175
1486.813659	234980.356724	36.520192
1488.452597	235440.608150	36.525210
1490.120366	235917.290773	36.530228
1491.630053	236361.715896	36.535245
1493.318288	236827.348323	36.540263
1494.390033	237284.802946	36.545280
1496.542938	237735.171217	36.550298
1497.941902	238200.652021	36.555316
1499.568342	238682.988632	36.560333
1501.241681	239138.951861	36.565351
1502.590985	239582.929285	36.570368
1504.173809	240043.939278	36.575386
1505.566001	240526.522664	36.580404
1507.009807	240974.780719	36.585421
1508.660927	241425.850619	36.590439
1510.148328	241900.597876	36.595456
1511.994455	242337.031449	36.600474
1513.632238	242802.534998	36.605492
1514.826627	243265.699514	36.610509
1516.554743	243708.429710	36.615527
1518.341739	244174.013162	36.620544
1519.874488	244632.603049	36.625562
1521.226495	245072.629072	36.630580
1522.565228	245536.892044	36.635597
1524.471133	246003.170700	36.640615
1525.561370	246458.763302	36.645632
1527.459546	246901.242638	36.650650
1529.173010	247352.517087	36.655668
1530.268782	247787.204619	36.660685
1531.807111	248225.579383	36.665703
1532.844736	248658.956857	36.670720
1534.772876	249082.890575	36.675738
1536.130395	249540.780989	36.680756
1537.235831	250007.477624	36.685773
1538.910850	250448.855826	36.690791
1539.848217	250888.578087	36.695808
1541.217949	251354.445384	36.700826
1542.630482	251815.047758	36.705844
1543.898000	252275.395153	36.710861
1545.481810	252764.802750	36.715879
1546.884752	253250.303251	36.720896
1548.305246	253724.674797	36.725914
1549.564469	254227.956757	36.730932
1551.069792	254710.749052	36.735949
1553.117220	255183.773700	36.740967
1554.270535	255694.288936	36.745984
1555.834378	256203.212637	36.751002
1557.760740	256695.895029	36.756020
1559.491135	257208.983464	36.761037
1561.208099	257702.209074	36.766055
1562.580583	258204.255903	36.771072
1564.304911	258685.261798	36.776090
1565.712265	259194.924277	36.781108
1566.772728	259724.153896	36.786125
1569.003541	260237.846961	36.791143
1570.045041	260746.757326	36.796160
1571.738240	261279.185309	36.801178
1573.396730	261789.441974	36.806196
1574.807297	262321.179947	36.811213
1576.680595	262840.165292	36.816231
1578.030364	263351.641370	36.821248
1579.558573	263869.210108	36.826266
1581.343328	264407.363859	36.831284
1582.747058	264944.132314	36.836301
1584.812208	265469.842614	36.841319
1586.255518	265990.981076	36.846336
1587.591113	266510.866879	36.851354
1589.471816	267063.076952	36.856372
1591.211986	267614.141281	36.861389
1592.681267	268121.785028	36.866407
1594.099133	268656.923095	36.871424
1596.161133	269194.520125	36.876442
1597.987455	269740.716378	36.881460
1599.471591	270259.558584	36.886477
1601.270265	270769.431867	36.891495
1602.904814	271305.979450	36.896512
1604.783935	271853.028263	36.901530
1606.553524	272361.329492	36.906548
1607.924859	272898.959951	36.911565
1609.825079	273430.583494	36.916583
1611.242661	273954.893642	36.921600
1613.056985	274462.905119	36.926618
1614.743620	274998.803718	36.931636
1616.102327	275550.581405	36.936653
1618.137003	276056.039061	36.941671
1619.567136	276573.687236	36.946688
1621.177774	277104.031366	36.951706
1622.374560	277641.580847	36.956724
1623.989150	278177.637742	36.961741
1625.467800	278701.268731	36.966759
1626.931315	279248.322080	36.971776
1628.581970	279793.869949	36.976794
1630.577128	280307.048008	36.981812
1632.126728	280840.543944	36.986829
1633.935358	281380.930606	36.991847
1635.010660	281901.521650	36.996864
1636.924334	282430.355705	37.001882
1638.807752	282957.542221	37.006900
1640.004731	283461.242231	37.011917
1641.996853	283965.749579	37.016935
1643.258546	284500.629520	37.021952
1644.780617	285011.790584	37.026970
1646.525485	285532.489806	37.031988
1647.694136	286068.066200	37.037005
1649.494866	286591.191525	37.042023
1650.724181	287119.007116	37.047040
1652.569103	287673.009712	37.052058
1654.512300	288215.208022	37.057076
1656.366514	288762.194521	37.062093
1657.924609	289287.459272	37.067111
1659.529123	289831.765182	37.072128
1660.820891	290374.393412	37.077146
1662.371230	290915.198882	37.082164
1663.922499	291487.016247	37.087181
1665.697888	292037.965870	37.092199
1667.220382	292603.814202	37.097216
1668.734346	293178.932635	37.102234
1670.717502	293741.906053	37.107252
1672.342749	294312.454464	37.112269
1673.976889	294883.887824	37.117287
1675.738558	295449.887348	37.122304
1677.470040	296012.384065	37.127322
1679.232107	296604.717591	37.132340
1680.702597	297179.900822	37.137357
1682.439665	297750.744731	37.142375
1684.389852	298345.222662	37.147392
1686.048393	298924.760119	37.152410
1688.061983	299500.324522	37.157428
1689.717193	300087.298259	37.162445
1691.308851	300648.093260	37.167463
1693.051487	301231.312651	37.172480
1694.868788	301818.834170	37.177498
1696.886744	302377.873211	37.182516
1698.476330	302980.867698	37.187533
1700.507110	303559.683119	37.192551
1702.363084	304144.314655	37.197568
1704.091771	304705.978815	37.202586
1705.923388	305283.826272	37.207604
1707.630906	305875.989338	37.212621
1709.374253	306450.872663	37.217639
1711.068372	307015.957270	37.222656
1712.717740	307599.255256	37.227674
1714.577152	308174.565631	37.232692
1716.233770	308777.892641	37.237709
1717.638082	309341.613456	37.242727
1719.467909	309923.723381	37.247744
1720.764782	310531.033858	37.252762
1723.152594	311114.313327	37.257780
1724.206895	311696.894452	37.262797
1726.106001	312277.173456	37.267815
1727.714553	312884.313614	37.272832
1729.704844	313481.583707	37.277850
1731.825742	314061.533853	37.282868
1733.343231	314650.822908	37.287885
1734.850835	315246.483122	37.292903
1736.781619	315838.970787	37.297920
1738.038689	316436.542198	37.302938
1739.612506	317030.552234	37.307956
1741.339046	317639.082880	37.312973
1743.688625	318235.875487	37.317991
1745.496125	318824.982278	37.323008
1747.225688	319410.669029	37.328026
1749.278932	320014.504202	37.333044
1750.718458	320615.109002	37.338061
1752.454055	321181.075346	37.343079
1753.972024	321738.566560	37.348096
1755.567935	322334.306059	37.353114
1757.547031	322888.233063	37.358132
1758.711907	323480.427890	37.363149
1760.705425	324066.209078	37.368167
1762.398537	324650.765044	37.373184
1763.628910	325259.691132	37.378202
1765.653881	325851.722588	37.383220
1767.405643	326433.942161	37.388237
1768.674710	327027.026813	37.393255
1770.536286	327636.156076	37.398272
1772.020904	328267.684423	37.403290
1773.545993	328880.513039	37.408308
1775.325479	329484.305779	37.413325
1776.896387	330117.704909	37.418343
1778.857644	330738.795644	37.423360
1780.471131	331392.485059	37.428378
1782.385549	332035.251482	37.433396
1783.959808	332682.179736	37.438413
1785.676169	333308.335736	37.443431
1787.546119	333948.752523	37.448448
1789.089705	334616.126008	37.453466
1791.250981	335259.297796	37.458484
1792.379603	335933.730698	37.463501
1794.344016	336601.137878	37.468519
1796.249854	337281.874036	37.473536
1797.648009	337945.093347	37.478554
1799.428041	338597.528986	37.483572
1801.217582	339294.378292	37.488589
1803.361357	340002.379838	37.493607
1804.840884	340672.913021	37.498624
1806.644056	341358.385898	37.503642
1808.630778	342053.998069	37.508660
1810.560267	342736.944058	37.513677
1812.321414	343430.137787	37.518695
1814.661543	344124.140167	37.523712
1816.283450	344839.039123	37.528730
1818.259461	345523.005289	37.533748
1820.684953	346190.770642	37.538765
1822.557360	346891.866953	37.543783
1824.554587	347568.592539	37.548800
1826.218498	348269.322335	37.553818
1828.488652	348946.338559	37.558836
1830.401653	349623.454674	37.563853
1832.306731	350318.200651	37.568871
1833.737103	350983.372224	37.573888
1835.605490	351667.546339	37.578906
1839.014799	352339.046178	37.583924
1841.066855	352995.076598	37.588941
1843.138710	353647.566714	37.593959
1845.193828	354313.220553	37.598976
1846.787211	354990.156873	37.603994
1848.833418	355638.485427	37.609012
1850.365743	356288.056362	37.614029
1852.367809	356936.981788	37.619047
1854.635082	357578.545694	37.624064
1856.102196	358229.798102	37.629082
1857.877820	358894.590100	37.634100
1859.669290	359563.454130	37.639117
1861.118536	360210.492143	37.644135
1862.993164	360857.424520	37.649152
1864.561207	361542.202270	37.654170
1866.328654	362184.361394	37.659188
1867.876172	362859.250687	37.664205
1869.556232	363549.760861	37.669223
1871.239284	364224.934715	37.674240
1873.114082	364902.171233	37.679258
1874.744496	365556.121533	37.684276
1876.795146	366226.329581	37.689293
1878.649169	366875.578364	37.694311
1880.352295	367527.504882	37.699328
1882.087696	368205.518921	37.704346
1883.696701	368873.115679	37.709364
1885.759672	369532.761996	37.714381
1887.420364	370200.580561	37.719399
1889.677018	370878.562356	37.724416
1891.385335	371542.569575	37.729434
1893.345952	372237.037969	37.734452
1895.380099	372920.853243	37.739469
1896.927616	373615.718872	37.744487
1898.640516	374287.488078	37.749504
1900.552007	374983.586453	37.754522
1902.124576	375689.948588	37.759540
1904.006395	376406.948767	37.764557
1905.658730	377112.889137	37.769575
1908.021211	377827.143660	37.774592
1909.517430	378544.214809	37.779610
1911.141796	379286.001912	37.784628
1913.041237	380014.287023	37.789645
1914.746674	380740.889668	37.794663
1917.027034	381464.643317	37.799680
1918.673786	382225.154190	37.804698
1920.895928	382966.813707	37.809716
1922.942924	383710.260754	37.814733
1924.329906	384458.922158	37.819751
1926.741881	385190.713355	37.824768
1928.636143	385956.930368	37.829786
1930.837855	386713.697477	37.834804
1933.213005	387439.638316	37.839821
1935.031322	388202.366910	37.844839
1937.280015	388969.874256	37.849856
1939.295883	389721.885885	37.854874
1941.451719	390463.715901	37.859892
1942.983899	391201.549832	37.864909
1944.503264	391969.637313	37.869927
1946.642404	392720.340310	37.874944
1948.578015	393484.139073	37.879962
1950.756381	394237.561951	37.884980
1952.705583	395007.074918	37.889997
1954.814301	395764.502102	37.895015
1956.657132	396536.402006	37.900032
1958.792911	397312.238578	37.905050
1961.072893	398065.904591	37.910068
1963.176989	398812.331923	37.915085
1964.705328	399596.066294	37.920103
1966.747099	400381.748019	37.925120
1968.709672	401147.248768	37.930138
1970.302370	401914.792493	37.935156
1972.552609	402671.234542	37.940173
1974.235526	403476.430348	37.945191
1976.308007	404236.154921	37.950208
1978.539256	405010.048606	37.955226
1980.559089	405770.501110	37.960244
1982.617295	406557.785317	37.965261
1984.444420	407360.642784	37.970279
1986.524735	408138.605398	37.975296
1988.532652	408903.408751	37.980314
1990.116705	409688.427791	37.985332
1992.339605	410486.771729	37.990349
1994.193091	411289.282701	37.995367
1996.161111	412068.317957	38.000384
1998.126835	412842.011347	38.005402
2000.029473	413644.596326	38.010420
2001.715516	414454.513586	38.015437
2003.585880	415235.879416	38.020455
2006.185120	415992.304492	38.025472
2007.775715	416773.721631	38.030490
2010.201996	417540.110167	38.035508
2012.695039	418286.076787	38.040525
2014.752824	419045.364814	38.045543
2016.789102	419792.401749	38.050560
2018.836427	420568.893410	38.055578
2020.589307	421335.558952	38.060596
2022.786565	422080.881752	38.065613
2024.500187	422848.394415	38.070631
2026.547897	423631.604157	38.075648
2028.343314	424417.008670	38.080666
2029.913501	425192.753266	38.085684
2031.892913	425959.670918	38.090701
2033.701536	426765.330586	38.095719
2036.076855	427572.237576	38.100736
2037.517891	428364.891977	38.105754
2039.241549	429172.359914	38.110772
2041.359434	429970.774305	38.115789
2043.141781	430817.163278	38.120807
2045.046404	431650.339179	38.125824
2047.084082	432481.489681	38.130842
2048.996859	433332.223060	38.135860
2050.948383	434171.377674	38.140877
2053.082636	435009.662305	38.145895
2054.978502	435853.574854	38.150912
2056.852147	436729.753702	38.155930
2059.289089	437584.953412	38.160948
2061.306149	438456.842166	38.165965
2063.154361	439321.083447	38.170983
2065.687029	440184.268186	38.176000
2067.796647	441063.835862	38.181018
2069.786820	441920.768700	38.186036
2072.082821	442807.221102	38.191053
2074.414372	443702.335866	38.196071
2076.232664	444568.658024	38.201088
2078.761237	445423.293120	38.206106
2080.715986	446329.545826	38.211124
2082.829796	447197.891563	38.216141
2084.739068	448072.762716	38.221159
2087.276607	448954.273935	38.226176
2089.444509	449839.705359	38.231194
2091.575393	450731.733044	38.236212
2093.918973	451593.389669	38.241229
2095.933552	452463.462080	38.246247
2098.069518	453354.266480	38.251264
2100.209149	454245.791361	38.256282
2102.385502	455127.258747	38.261300
2104.673982	456011.704831	38.266317
2106.622939	456902.793985	38.271335
2108.924358	457778.818744	38.276352
2111.319564	458636.385053	38.281370
2113.193886	459531.519406	38.286388
2115.684735	460413.569301	38.291405
2118.147701	461281.277426	38.296423
2120.493263	462146.692713	38.301440
2122.491671	463018.801333	38.306458
2124.182714	463887.181916	38.311476
2126.595474	464764.707010	38.316493
2128.286930	465654.999896	38.321511
2130.799300	466528.892299	38.326528
2133.442352	467379.474497	38.331546
2135.345519	468246.315079	38.336564
2137.622749	469120.434269	38.341581
2139.675603	470009.156336	38.346599
2141.742346	470873.578924	38.351616
2144.356173	471734.082707	38.356634
2146.119418	472589.887924	38.361652
2148.337678	473419.810787	38.366669
2150.068276	474281.255306	38.371687
2151.842320	475104.205502	38.376704
2154.092350	475935.326865	38.381722
2155.634257	476809.014561	38.386740
2158.116384	477669.119740	38.391757
2159.827362	478514.663450	38.396775
2161.727130	479392.818687	38.401792
2163.962078	480248.046880	38.406810
2165.809020	481121.885999	38.411828
2167.796561	482013.842030	38.416845
2170.118569	482917.567434	38.421863
2172.009131	483791.524508	38.426880
2173.786872	484687.323370	38.431898
2175.756534	485600.365845	38.436916
2177.757803	486515.477495	38.441933
2179.735695	487444.178433	38.446951
2181.690259	488379.448689	38.451968
2183.974815	489315.473583	38.456986
2185.868255	490278.621946	38.462004
2188.214737	491198.231467	38.467021
2190.297006	492165.233248	38.472039
2192.515417	493120.651255	38.477056
2194.764221	494091.708072	38.482074
2196.702417	495069.221541	38.487092
2199.294615	496039.103067	38.492109
2201.471137	497009.957173	38.497127
2203.184461	497995.364719	38.502144
2205.601866	498981.456942	38.507162
2207.997006	499984.800864	38.512180
2210.064677	500967.858341	38.517197
2212.685267	501943.149706	38.522215
2214.793552	502950.097143	38.527232
2217.441513	503946.756180	38.532250
2219.899073	504931.987829	38.537268
2222.320869	505922.210172	38.542285
2224.581185	506914.921194	38.547303
2226.201081	507916.351480	38.552320
2228.952547	508927.265935	38.557338
2231.038921	509921.184393	38.562356
2233.332916	510895.041501	38.567373
2235.550885	511912.260865	38.572391
2237.918041	512914.922631	38.577408
2240.219397	513917.179519	38.582426
2242.202509	514947.905658	38.587444
2244.457866	515940.818095	38.592461
2246.720235	516955.490331	38.597479
2249.031064	517972.508194	38.602496
2251.468022	519004.355799	38.607514
2253.462910	520022.804195	38.612532
2255.490214	521025.157374	38.617549
2258.124658	522037.069622	38.622567
2261.594326	523059.307249	38.627584
2265.072020	524046.009866	38.632602
2267.473946	525016.051594	38.637620
2269.499100	526011.127978	38.642637
2271.810978	527004.782272	38.647655
2274.064910	528003.719389	38.652672
2276.586580	528972.732431	38.657690
2278.851133	529946.912088	38.662708
2280.772103	530928.033773	38.667725
2282.970003	531906.275819	38.672743
2284.931631	532893.705907	38.677760
2287.487381	533878.756881	38.682778
2288.829935	534892.233516	38.687796
2291.369251	535861.749891	38.692813
2293.425033	536854.485645	38.697831
2295.722238	537838.054341	38.702848
2298.256369	538806.922322	38.707866
2300.470905	539769.688795	38.712884
2303.047099	540737.614878	38.717901
2305.554223	541710.619342	38.722919
2307.651849	542672.757282	38.727936
2309.977599	543605.662869	38.732954
2312.201756	544565.991501	38.737972
2314.255657	545537.500651	38.742989
2316.995457	546523.919712	38.748007
2319.052517	547486.893513	38.753024
2321.806637	548431.329076	38.758042
2324.187443	549419.866206	38.763060
2326.382587	550389.808014	38.768077
2329.074434	551366.036093	38.773095
2331.052427	552327.882664	38.778112
2333.389560	553314.489026	38.783130
2335.633014	554311.094076	38.788148
2337.506058	555279.989664	38.793165
2339.600487	556277.128881	38.798183
2341.624214	557278.377994	38.803200
2343.872870	558290.069719	38.808218
2345.978468	559318.895499	38.813236
2348.263802	560352.436584	38.818253
2350.367719	561376.983898	38.823271
2352.580191	562428.162859	38.828288
2354.898611	563471.202999	38.833306
2356.978013	564538.261966	38.838324
2359.021634	565609.710704	38.843341
2361.372340	566666.455936	38.848359
2363.381920	567745.218965	38.853376
2366.257554	568836.103128	38.858394
2368.185272	569932.223653	38.863412
2370.207901	571042.595079	38.868429
2372.720080	572128.591655	38.873447
2375.281794	573235.521728	38.878464
2377.575457	574346.867418	38.883482
2379.821964	575480.408543	38.888500
2382.378954	576584.387874	38.893517
2385.008492	577702.259494	38.898535
2387.082988	578831.162319	38.903552
2389.893788	579964.558320	38.908570
2392.335445	581098.464123	38.913588
2394.578327	582211.832473	38.918605
2397.395524	583336.944026	38.923623
2399.489750	584482.735952	38.928640
2402.272717	585596.161422	38.933658
2404.515893	586749.991938	38.938676
2406.742798	587880.099830	38.943693
2409.388692	589024.673365	38.948711
2411.344338	590188.051784	38.953728
2413.969324	591333.813903	38.958746
2416.546559	592480.677658	38.963764
2419.314770	593627.600627	38.968781
2422.513118	594756.652944	38.973799
2425.230941	595876.106795	38.978816
2428.014051	597012.328713	38.983834
2430.614281	598136.147417	38.988852
2432.878134	599250.947604	38.993869
2435.432991	600375.811837	38.998887
2437.832587	601505.451464	39.003904
2440.473097	602627.229690	39.008922
2442.655795	603738.609674	39.013940
2445.103131	604870.417505	39.018957
2447.283985	605977.776952	39.023975
2449.693928	607108.469557	39.028992
2451.872937	608248.698878	39.034010
2454.165178	609377.784715	39.039028
2456.512270	610499.242691	39.044045
2459.602438	611590.393510	39.049063
2461.661685	612690.364778	39.054080
2463.912230	613795.550096	39.059098
2466.005874	614898.551282	39.064116
2468.164117	616006.334844	39.069133
2470.783219	617104.979596	39.074151
2473.029951	618218.329807	39.079168
2475.329438	619333.059383	39.084186
2477.629887	620468.575850	39.089204
2479.975498	621599.018065	39.094221
2482.918187	622744.941696	39.099239
2484.532497	623903.109989	39.104256
2487.113707	625043.553078	39.109274
2489.264777	626190.193692	39.114292
2491.412463	627366.144159	39.119309
2494.430087	628521.338186	39.124327
2497.356955	629717.687106	39.129344
2499.579683	630903.678274	39.134362
2502.143488	632070.202121	39.139380
2504.615286	633273.918227	39.144397
2507.349928	634444.647080	39.149415
2509.445401	635637.769353	39.154432
2511.844928	636818.175275	39.159450
2514.527247	638039.633362	39.164468
2516.858859	639237.797334	39.169485
2519.332116	640446.280114	39.174503
2522.313506	641690.166737	39.179520
2524.862682	642888.221954	39.184538
2527.232243	644121.338424	39.189556
2529.678398	645357.636057	39.194573
2532.270405	646582.039174	39.199591
2534.880762	647805.444221	39.204608
2537.352891	649030.170588	39.209626
2540.136215	650296.228931	39.214644
2542.469084	651531.045180	39.219661
2545.360141	652776.384188	39.224679
2547.591923	654015.895498	39.229696
2550.054566	655269.516765	39.234714
2552.707226	656534.707646	39.239732
2555.220824	657795.176318	39.244749
2558.218991	659040.161019	39.249767
2560.858885	660301.832312	39.254784
2563.820941	661540.379477	39.259802
2566.506314	662811.231636	39.264820
2569.033704	664066.658855	39.269837
2571.737237	665319.256092	39.274855
2574.099127	666585.136907	39.279872
2576.311673	667848.387547	39.284890
2579.260389	669099.009554	39.289908
2581.917886	670366.831095	39.294925
2584.441041	671625.004100	39.299943
2586.587836	672905.605929	39.304960
2589.235767	674173.617524	39.309978
2591.911709	675447.222712	39.314996
2594.562733	676743.780416	39.320013
2597.008470	678028.509499	39.325031
2599.703105	679301.289644	39.330048
2602.271046	680551.998136	39.335066
2604.983569	681853.749860	39.340084
2607.032417	683169.688161	39.345101
2609.884893	684436.618835	39.350119
2612.555473	685728.341125	39.355136
2615.154678	687033.054654	39.360154
2618.228906	688328.465198	39.365172
2620.333847	689623.155786	39.370189
2623.051471	690903.758914	39.375207
2626.115938	692195.490552	39.380224
2628.507470	693452.455213	39.385242
2631.278465	694716.972327	39.390260
2633.556381	695997.368793	39.395277
2636.540655	697245.614951	39.400295
2638.928659	698497.256269	39.405312
2641.560728	699760.087705	39.410330
2644.288324	700992.175595	39.415348
2646.463705	702262.112680	39.420365
2649.024925	703513.310748	39.425383
2651.990366	704787.461099	39.430400
2654.557922	706054.205310	39.435418
2656.871559	707333.244669	39.440436
2659.586997	708614.456700	39.445453
2662.000413	709892.209257	39.450471
2664.245406	711203.877531	39.455488
2667.020523	712524.419770	39.460506
2669.752535	713820.601245	39.465524
2671.991368	715122.409855	39.470541
2674.905813	716438.114413	39.475559
2677.562466	717767.416112	39.480576
2680.217240	719085.077595	39.485594
2682.869034	720438.305461	39.490612
2685.559198	721792.001151	39.495629
2687.782286	723129.034370	39.500647
2690.906923	724494.634693	39.505664
2693.421955	725844.288295	39.510682
2696.441959	727181.130859	39.515700
2698.770355	728555.239197	39.520717
2701.540355	729925.041953	39.525735
2704.444650	731289.059309	39.530752
2706.886962	732670.759891	39.535770
2709.627234	734043.285522	39.540788
2712.470620	735435.069966	39.545805
2715.207058	736827.718749	39.550823
2718.098687	738231.407047	39.555840
2721.022021	739633.857507	39.560858
2723.873827	741008.140132	39.565876
2726.327536	742420.098874	39.570893
2729.447207	743802.293007	39.575911
2732.611880	745210.135367	39.580928
2735.193869	746603.125928	39.585946
2738.066177	747994.885272	39.590964
2741.031044	749409.455260	39.595981
2744.017350	750789.064329	39.600999
2746.936239	752177.064889	39.606016
2749.667909	753565.587454	39.611034
2752.927811	754960.030735	39.616052
2755.449800	756355.969174	39.621069
2758.467782	757729.509648	39.626087
2761.074285	759112.719726	39.631104
2763.774711	760502.900881	39.636122
2766.714273	761902.682434	39.641140
2769.368373	763298.562193	39.646157
2772.013044	764692.611690	39.651175
2774.842999	766104.574804	39.656192
2777.360874	767490.502552	39.661210
2780.172666	768871.650787	39.666228
2782.761674	770296.436764	39.671245
2785.583676	771716.979398	39.676263
2788.444041	773129.134727	39.681280
2790.898299	774535.387631	39.686298
2793.888519	775930.869012	39.691316
2796.592126	777347.794476	39.696333
2799.153832	778755.187830	39.701351
2801.900763	780185.013075	39.706368
2804.467225	781611.347527	39.711386
2807.121548	783023.546620	39.716404
2809.852148	784486.050043	39.721421
2812.950241	785911.891295	39.726439
2815.649465	787298.225278	39.731456
2818.094696	788697.378364	39.736474
2820.881248	790097.427211	39.741492
2823.343913	791484.949633	39.746509
2825.962396	792903.004820	39.751527
2828.775317	794324.566334	39.756544
2831.393676	795737.495806	39.761562
2833.934831	797173.078725	39.766580
2836.509454	798599.743082	39.771597
2838.783687	800040.512279	39.776615
2841.876708	801494.898466	39.781632
2844.416565	802970.312688	39.786650
2847.449352	804420.473784	39.791668
2849.943645	805906.719351	39.796685
2852.630549	807386.302739	39.801703
2855.513437	808879.764969	39.806720
2857.924415	810364.031955	39.811738
2860.600636	811889.479635	39.816756
2864.157223	813409.455248	39.821773
2866.759813	814930.028634	39.826791
2869.869781	816446.414771	39.831808
2872.689644	817977.157556	39.836826
2875.745564	819496.819604	39.841844
2878.772254	821045.965695	39.846861
2881.526934	822594.357214	39.851879
2884.566435	824139.754922	39.856896
2887.631280	825670.251579	39.861914
2890.530264	827204.516980	39.866932
2894.094708	828782.975137	39.871949
2896.606099	830343.678798	39.876967
2899.724297	831896.745967	39.881984
2902.456994	833463.683952	39.887002
2905.084355	835028.994548	39.892020
2908.132095	836593.905802	39.897037
2910.591012	838176.693825	39.902055
2913.395325	839753.729731	39.907072
2916.569124	841340.000022	39.912090
2919.568750	842925.710217	39.917108
2922.024606	844504.792004	39.922125
2925.205301	846111.514892	39.927143
2928.171502	847709.600573	39.932160
2930.942470	849306.535411	39.937178
2934.276691	850920.171254	39.942196
2936.891314	852534.578189	39.947213
2939.463482	854139.056045	39.952231
2942.818868	855778.820404	39.957248
2945.219560	857408.406547	39.962266
2948.092282	859024.771603	39.967284
2951.626697	860663.209307	39.972301
2954.475499	862298.703365	39.977319
2957.742802	863918.369588	39.982336
2960.373315	865573.094867	39.987354
2963.500659	867202.767171	39.992372
2966.646220	868832.578989	39.997389
2969.538684	870488.436426	40.002407
2972.817607	872103.682813	40.007424
2975.659421	873747.222403	40.012442
2979.022099	875396.127838	40.017460
2982.096476	877015.596198	40.022477
2984.612395	878652.610108	40.027495
2988.104343	880290.073837	40.032512
2990.643553	881919.795298	40.037530
2993.822140	883559.881050	40.042548
2996.849298	885207.358981	40.047565
2999.951514	886855.422057	40.052583
3002.858324	888493.200230	40.057600
3005.870896	890135.228963	40.062618
3008.427324	891747.332482	40.067636
3011.539274	893373.849115	40.072653
3014.060228	894988.426997	40.077671
3017.166117	896578.730196	40.082688
3020.354934	898175.421390	40.087706
3023.086322	899791.015749	40.092724
3026.087425	901395.410131	40.097741
3028.863174	902996.978019	40.102759
3031.969460	904640.118282	40.107776
3035.226807	906247.999547	40.112794
3037.924998	907865.905196	40.117812
3041.120399	909482.778759	40.122829
3044.214277	911137.288549	40.127847
3047.124392	912760.853138	40.132864
3049.892188	914407.804129	40.137882
3052.718197	916075.202864	40.142900
3055.509012	917751.035608	40.147917
3058.494764	919416.623031	40.152935
3061.565914	921097.721730	40.157952
3064.625492	922791.452024	40.162970
3067.706457	924475.821984	40.167988
3070.588804	926183.391972	40.173005
3073.510808	927884.948154	40.178023
3076.529208	929602.916161	40.183040
3079.405726	931337.892422	40.188058
3082.275638	933053.912019	40.193076
3085.503596	934789.046342	40.198093
3088.049366	936547.083797	40.203111
3091.158825	938297.073741	40.208128
3094.416672	940069.896338	40.213146
3097.585389	941820.424204	40.218164
3100.906310	943585.255045	40.223181
3103.896312	945353.460755	40.228199
3107.607675	947134.416424	40.233216
3110.994672	948908.986228	40.238234
3113.897011	950667.080573	40.243252
3117.342279	952429.733170	40.248269
3120.164107	954220.027359	40.253287
3123.534185	956018.879797	40.258304
3126.617229	957858.092084	40.263322
3129.444252	959710.159461	40.268340
3132.217763	961541.012014	40.273357
3135.395040	963374.735260	40.278375
3138.572633	965242.267449	40.283392
3141.429383	967111.590744	40.288410
3144.443184	968958.017983	40.293428
3148.307420	970809.568500	40.298445
3151.194853	972674.441514	40.303463
3154.317058	974566.470778	40.308480
3157.367385	976435.848730	40.313498
3160.056138	978323.782846	40.318516
3163.369035	980221.613428	40.323533
3166.815856	982108.562846	40.328551
3170.217802	983982.041107	40.333568
3173.200856	985871.134229	40.338586
3176.315126	987744.008173	40.343604
3180.070928	989632.116392	40.348621
3182.539331	991548.793236	40.353639
3185.601172	993449.170326	40.358656
3188.602794	995359.612926	40.363674
3191.623034	997262.802636	40.368692
3194.644952	999173.997786	40.373709
3197.650187	1001077.754471	40.378727
3201.092983	1003015.450010	40.383744
3204.217233	1004935.651272	40.388762
3207.225557	1006868.992567	40.393780
3210.671300	1008792.291465	40.398797
3213.350564	1010749.858387	40.403815
3216.803511	1012636.853181	40.408832
3220.223611	1014518.474697	40.413850
3223.029537	1016423.775874	40.418868
3226.207285	1018317.625434	40.423885
3229.216286	1020200.510225	40.428903
3232.330579	1022094.160411	40.433920
3235.502397	1024015.978204	40.438938
3238.383547	1025911.761056	40.443956
3241.967099	1027829.881643	40.448973
3244.958551	1029752.754761	40.453991
3247.936590	1031669.077600	40.459008
3251.223460	1033621.664265	40.464026
3254.130609	1035531.459002	40.469044
3257.210481	1037497.293439	40.474061
3260.351649	1039456.637528	40.479079
3263.768282	1041392.206505	40.484096
3267.284232	1043367.847326	40.489114
3270.046624	1045365.546737	40.494132
3273.416947	1047339.219126	40.499149
3276.819190	1049317.092488	40.504167
3279.867687	1051301.245706	40.509184
3283.148513	1053318.893218	40.514202
3286.257227	1055342.947835	40.519220
3289.184846	1057351.198964	40.524237
3292.910954	1059394.139181	40.529255
3296.128662	1061390.877364	40.534272
3299.476812	1063428.732638	40.539290
3302.554696	1065481.713826	40.544308
3306.133830	1067531.254698	40.549325
3309.208256	1069594.019869	40.554343
3312.897301	1071657.729258	40.559360
3316.255473	1073723.878065	40.564378
3319.563057	1075772.106855	40.569396
3322.752906	1077856.935305	40.574413
3326.056090	1079919.314891	40.579431
3329.207942	1081976.729328	40.584448
3332.632957	1084068.427273	40.589466
3336.207870	1086158.818838	40.594484
3339.349168	1088262.337576	40.599501
3342.450426	1090352.436858	40.604519
3346.392366	1092470.435895	40.609536
3349.725498	1094550.474843	40.614554
3352.527162	1096653.756291	40.619572
3356.125905	1098753.704192	40.624589
3359.123257	1100881.542908	40.629607
3362.467567	1102996.094517	40.634624
3365.878749	1105129.339396	40.639642
3368.829284	1107259.529925	40.644660
3372.261736	1109380.420075	40.649677
3375.447080	1111525.449141	40.654695
3378.760654	1113675.023290	40.659712
3382.066704	1115819.553714	40.664730
3385.285591	1117978.734827	40.669748
3388.513229	1120153.482054	40.674765
3391.811708	1122311.282416	40.679783
3394.913435	1124494.067717	40.684800
3398.373811	1126671.726025	40.689818
3401.587786	1128842.749236	40.694836
3404.715684	1131029.685771	40.699853
3408.381166	1133242.079960	40.704871
3411.416454	1135437.077019	40.709888
3415.317534	1137636.896102	40.714906
3418.550500	1139850.680914	40.719924
3421.869745	1142040.437931	40.724941
3425.237949	1144236.658959	40.729959
3428.552324	1146463.461195	40.734976
3432.235636	1148681.419848	40.739994
3435.484137	1150890.110143	40.745012
3438.916468	1153067.738757	40.750016
3442.158126	1155213.899229	40.755021
3445.620272	1157284.229099	40.760026
3449.025399	1159274.512716	40.765031
3452.477863	1161219.702300	40.770036
3456.195440	1163081.259218	40.775040
3458.826254	1164845.608919	40.780045
3461.795684	1166556.051225	40.785050
3465.310851	1168169.653013	40.790055
3467.839841	1169699.495673	40.795060
3470.318318	1171153.706326	40.800064
3473.133679	1172536.716983	40.805069
3475.773324	1173821.416726	40.810074
3478.283623	1175051.236579	40.815079
3481.006478	1176194.678335	40.820084
3483.168779	1177240.240945	40.825088
3485.307528	1178245.084420	40.830093
3487.506563	1179180.864522	40.835098
3489.157142	1180040.560730	40.840103
3490.501126	1180865.511158	40.845108
3492.489499	1181614.430066	40.850112
3494.370150	1182290.015978	40.855117
3495.404828	1182924.894496	40.860122
3497.048308	1183509.899530	40.865127
3498.641255	1184052.873579	40.870132
3500.093660	1184550.645193	40.875136
3501.602891	1184978.354109	40.880141
3502.418707	1185392.311189	40.885146
3503.869461	1185750.811856	40.890151
3504.414112	1186077.263671	40.895156
3505.723655	1186371.961934	40.900160
3506.908037	1186616.433929	40.905165
3507.636588	1186809.048138	40.910170
3508.836841	1186982.107593	40.915175
3509.642020	1187155.696588	40.920180
3510.208475	1187281.164561	40.925184
3511.373799	1187371.544170	40.930189
3511.841125	1187437.396270	40.935194
3512.497296	1187466.161319	40.940199
3513.264331	1187473.370838	40.945204
3513.288435	1187467.253735	40.950208
3514.090915	1187448.217765	40.955213
3514.564275	1187412.118889	40.960218
3515.399463	1187359.219162	40.965223
3515.569781	1187292.038458	40.970228
3516.279748	1187182.443888	40.975232
3516.841475	1187067.698335	40.980237
3516.991231	1186931.008435	40.985242
3517.639562	1186777.866173	40.990247
3517.792592	1186640.791833	40.995252
3518.478977	1186458.756205	41.000256
3518.949506	1186271.387718	41.005261
3518.980730	1186055.768477	41.010266
3519.368655	1185847.137390	41.015271
3519.510540	1185642.301705	41.020276
3519.940645	1185407.020698	41.025280
3520.364296	1185157.334213	41.030285
3520.364509	1184912.222011	41.035290
3520.588515	1184653.228695	41.040295
3520.806621	1184386.506831	41.045300
3521.165110	1184114.948539	41.050304
3521.438534	1183828.143453	41.055309
3521.387417	1183546.740800	41.060314
3521.774151	1183248.402352	41.065319
3522.004115	1182933.317260	41.070324
3521.911232	1182624.008550	41.075328
3521.894595	1182328.601890	41.080333
3521.926940	1181987.414492	41.085338
3522.395157	1181666.281899	41.090343
3522.060907	1181336.693049	41.095348
3522.486083	1181017.693120	41.100352
3522.782049	1180682.026478	41.105357
3522.413573	1180335.334557	41.110362
3522.833532	1179970.312003	41.115367
3522.636063	1179641.346508	41.120372
3522.819771	1179286.204840	41.125376
3522.968406	1178955.443380	41.130381
3523.159060	1178608.732574	41.135386
3523.137806	1178222.274335	41.140391
3523.157518	1177853.494619	41.145396
3523.093365	1177499.025490	41.150400
3523.163532	1177124.720480	41.155405
3523.462167	1176762.131303	41.160410
3523.683314	1176368.238694	41.165415
3523.395778	1176011.348758	41.170420
3523.581003	1175621.552858	41.175424
3523.907407	1175254.800794	41.180429
3523.766183	1174869.055958	41.185434
3524.025240	1174474.919614	41.190439
3523.705700	1174100.178467	41.195444
3523.433534	1173703.336802	41.200448
3524.140273	1173296.967447	41.205453
3523.602910	1172916.613024	41.210458
3523.711833	1172516.600248	41.215463
3523.456947	1172128.879205	41.220468
3523.752453	1171714.813827	41.225472
3523.936541	1171319.224897	41.230477
3523.700855	1170926.599919	41.235482
3523.575223	1170518.547285	41.240487
3523.582146	1170126.010838	41.245492
3523.958835	1169734.705166	41.250496
3523.940676	1169355.987354	41.255501
3523.881995	1168939.967038	41.260506
3524.149202	1168524.331881	41.265511
3523.992291	1168116.285469	41.270516
3524.180835	1167695.971826	41.275520
3523.999672	1167280.878074	41.280525
3523.913268	1166890.851920	41.285530
3524.157103	1166466.181352	41.290535
3523.960554	1166061.002776	41.295540
3523.906591	1165663.985931	41.300544
3523.780849	1165249.571817	41.305549
3523.856530	1164834.241588	41.310554
3524.034577	1164414.799509	41.315559
3523.735230	1164014.391633	41.320564
3523.769319	1163585.931898	41.325568
3523.858960	1163181.806023	41.330573
3523.743281	1162782.218582	41.335578
3523.767984	1162360.463852	41.340583
3523.869281	1161932.141324	41.345588
3523.729946	1161519.702535	41.350592
3524.087732	1161105.069865	41.355597
3523.796390	1160677.182118	41.360602
3523.806514	1160277.193941	41.365607
3523.835618	1159876.226666	41.370612
3524.044821	1159454.680582	41.375616
3523.930889	1159034.477749	41.380621
3523.932450	1158629.164405	41.385626
3523.998178	1158185.126783	41.390631
3523.759293	1157749.992903	41.395636
3523.878416	1157320.155873	41.400640
3523.918100	1156910.352290	41.405645
3523.701743	1156490.435777	41.410650
3523.701597	1156076.600172	41.415655
3523.607070	1155653.474396	41.420660
3523.579822	1155214.689257	41.425664
3523.553235	1154815.426674	41.430669
3523.120351	1154402.666275	41.435674
3523.429197	1153956.622361	41.440679
3523.678565	1153551.349836	41.445684
3523.534159	1153124.715713	41.450688
3523.552517	1152718.470431	41.455693
3523.283782	1152291.978665	41.460698
3523.317735	1151880.079763	41.465703
3523.341360	1151460.953213	41.470708
3523.293964	1151020.022395	41.475712
3523.586050	1150600.025512	41.480717
3523.246413	1150198.285878	41.485722
3523.502418	1149775.766512	41.490727
3523.072413	1149367.157897	41.495732
3523.142950	1148935.128033	41.500736
3523.104950	1148509.050073	41.505741
3523.152199	1148090.409707	41.510746
3523.190474	1147665.103894	41.515751
3522.712844	1147269.513328	41.520756
3522.654210	1146848.232978	41.525760
3522.879575	1146438.152221	41.530765
3522.706432	1146008.671863	41.535770
3523.006317	1145586.663079	41.540775
3522.838022	1145173.041193	41.545780
3522.646546	1144765.459210	41.550784
3522.887969	1144362.421019	41.555789
3522.799166	1143941.103506	41.560794
3522.976091	1143500.171201	41.565799
3522.593956	1143098.467185	41.570804
3522.597064	1142678.741282	41.575808
3522.753151	1142268.727929	41.580813
3522.619894	1141865.750973	41.585818
3522.877425	1141456.606738	41.590823
3522.696729	1141023.876355	41.595828
3522.602963	1140604.855963	41.600832
3522.682533	1140196.402850	41.605837
3522.426015	1139760.260177	41.610842
3522.739806	1139353.127138	41.615847
3522.555635	1138944.620989	41.620852
3522.158571	1138523.397632	41.625856
3522.171438	1138126.472545	41.630861
3521.887076	1137710.957335	41.635866
3522.386760	1137291.767173	41.640871
3522.482215	1136877.548448	41.645876
3522.579167	1136452.565726	41.650880
3522.053697	1136049.116036	41.655885
3522.178229	1135638.879820	41.660890
3522.251739	1135227.195464	41.665895
3522.268339	1134825.273333	41.670900
3522.013443	1134405.314577	41.675904
3522.339477	1133985.511988	41.680909
3522.421164	1133574.838409	41.685914
3522.344761	1133167.104987	41.690919
3522.526635	1132764.429619	41.695924
3522.002493	1132337.414298	41.700928
3521.979847	1131915.224670	41.705933
3521.706434	1131505.685417	41.710938
3522.047588	1131088.788542	41.715943
3522.169583	1130685.015001	41.720948
3521.844653	1130296.021627	41.725952
3522.231884	1129878.261750	41.730957
3522.015122	1129465.893811	41.735962
3521.987972	1129048.897882	41.740967
3521.818905	1128630.275848	41.745972
3521.902218	1128207.013803	41.750976
3521.954653	1127788.384273	41.755981
3521.443798	1127393.216743	41.760986
3521.983567	1126976.345802	41.765991
3521.703775	1126577.464524	41.770996
3521.321144	1126176.572157	41.776000
3521.373654	1125770.249078	41.781005
3521.336440	1125375.044305	41.786010
3521.393635	1124966.851130	41.791015
3521.149691	1124548.301619	41.796020
3521.337951	1124149.352091	41.801024
3521.239359	1123748.135320	41.806029
3521.263378	1123343.155321	41.811034
3521.108530	1122951.693844	41.816039
3521.090244	1122576.177535	41.821044
3520.897041	1122170.287472	41.826048
3521.091523	1121756.684281	41.831053
3520.726606	1121358.379306	41.836058
3520.873998	1120957.960139	41.841063
3520.744297	1120563.367010	41.846068
3520.585530	1120185.038830	41.851072
3520.816846	1119782.612698	41.856077
3520.494775	1119392.918754	41.861082
3520.807484	1119006.045561	41.866087
3520.601105	1118615.227870	41.871092
3520.564771	1118224.258352	41.876096
3520.631409	1117814.183180	41.881101
3520.605529	1117413.908595	41.886106
3520.817374	1117012.230542	41.891111
3520.812174	1116637.153000	41.896116
3520.622475	1116251.784104	41.901120
3520.737087	1115844.505494	41.906125
3520.267338	1115439.389740	41.911130
3520.232486	1115059.248839	41.916135
3520.081048	1114679.958407	41.921140
3520.277446	1114297.436879	41.926144
3520.376414	1113885.434641	41.931149
3520.262938	1113507.771775	41.936154
3520.679547	1113131.425799	41.941159
3520.533804	1112758.866310	41.946164
3520.227323	1112345.572592	41.951168
3520.318158	1111959.944552	41.956173
3519.892570	1111564.069397	41.961178
3519.983683	1111170.179186	41.966183
3519.995288	1110802.324439	41.971188
3519.553007	1110418.677522	41.976192
3520.044158	1110031.986312	41.981197
3519.747314	1109660.954771	41.986202
3519.988273	1109268.427677	41.991207
3519.894746	1108879.172662	41.996212
3519.472357	1108487.938846	42.001216
3519.634709	1108120.735027	42.006221
3519.688811	1107742.734778	42.011226
3519.633220	1107360.047210	42.016231
3519.919444	1106976.703185	42.021236
3519.319734	1106587.843271	42.026240
3519.709019	1106221.523055	42.031245
3519.386538	1105862.554166	42.036250
3519.223077	1105465.231697	42.041255
3519.303584	1105091.339404	42.046260
3519.119034	1104705.714201	42.051264
3519.362564	1104325.627795	42.056269
3518.984248	1103956.509378	42.061274
3519.300613	1103586.964619	42.066279
3519.376296	1103229.856979	42.071284
3519.169424	1102848.976216	42.076288
3519.279549	1102482.161186	42.081293
3519.338927	1102110.550605	42.086298
3519.232886	1101727.853673	42.091303
3519.278077	1101363.362972	42.096308
3518.979770	1100977.585550	42.101312
3519.426399	1100586.781944	42.106317
3519.216876	1100235.737607	42.111322
3518.964089	1099864.310688	42.116327
3519.172759	1099481.498358	42.121332
3518.990055	1099122.822822	42.126336
3519.271156	1098742.337032	42.131341
3518.958564	1098352.070706	42.136346
3519.100652	1097969.831827	42.141351
3519.148397	1097621.731869	42.146356
3518.806257	1097250.427025	42.151360
3519.082027	1096873.445936	42.156365
3518.793402	1096504.377213	42.161370
3518.751645	1096129.501536	42.166375
3519.076554	1095776.740024	42.171380
3518.721076	1095408.660207	42.176384
3518.789526	1095029.192379	42.181389
3518.403559	1094660.588206	42.186394
3518.550223	1094268.803155	42.191399
3518.595161	1093906.011203	42.196404
3518.609761	1093560.431539	42.201408
3518.677086	1093183.323614	42.206413
3518.276131	1092807.702743	42.211418
3518.086428	1092461.607954	42.216423
3518.230203	1092107.201098	42.221428
3518.006560	1091745.553626	42.226432
3518.535081	1091393.047773	42.231437
3517.945792	1091049.897550	42.236442
3518.300649	1090671.035172	42.241447
3518.206597	1090297.967599	42.246452
3518.024138	1089954.297933	42.251456
3517.961488	1089597.366286	42.256461
3517.832179	1089242.434104	42.261466
3517.552649	1088895.551778	42.266471
3517.925968	1088547.198305	42.271476
3517.500037	1088181.993005	42.276480
3517.957199	1087831.088353	42.281485
3517.629945	1087485.944690	42.286490
3517.818432	1087134.368452	42.291495
3517.732770	1086786.169398	42.296500
3517.343767	1086447.679501	42.301504
3517.650546	1086088.731095	42.306509
3517.472655	1085726.387547	42.311514
3517.487660	1085373.671503	42.316519
3517.758206	1085033.355085	42.321524
3517.401693	1084705.106558	42.326528
3517.317150	1084346.395332	42.331533
3517.469380	1084016.103598	42.336538
3517.594950	1083641.583849	42.341543
3517.473888	1083298.346303	42.346548
3517.454515	1082963.415223	42.351552
3517.732904	1082606.639811	42.356557
3517.497132	1082254.242585	42.361562
3517.618271	1081906.368728	42.366567
3517.266941	1081557.207290	42.371572
3516.909122	1081222.128976	42.376576
3517.215628	1080899.202780	42.381581
3517.314176	1080546.352205	42.386586
3517.067087	1080187.585807	42.391591
3516.793796	1079862.966354	42.396596
3516.575936	1079514.803799	42.401600
3516.884602	1079174.882954	42.406605
3516.799568	1078866.586516	42.411610
3516.938265	1078533.277005	42.416615
3516.834708	1078182.802749	42.421620
3516.789925	1077830.184139	42.426624
3516.842579	1077493.945118	42.431629
3516.647463	1077165.887884	42.436634
3516.752159	1076839.009900	42.441639
3517.075654	1076510.923951	42.446644
3516.685492	1076156.909771	42.451648
3516.914566	1075816.696976	42.456653
3516.730316	1075491.130569	42.461658
3516.670645	1075146.697475	42.466663
3516.880010	1074806.617188	42.471668
3516.689927	1074478.782056	42.476672
3516.614304	1074139.571835	42.481677
3516.507021	1073820.234072	42.486682
3516.657770	1073470.952946	42.491687
3516.399825	1073148.910449	42.496692
3516.186075	1072829.820690	42.501696
3516.085240	1072496.470700	42.506701
3516.172388	1072165.472139	42.511706
3516.051245	1071837.082936	42.516711
3515.864871	1071524.544401	42.521716
3515.882428	1071200.323398	42.526720
3516.027100	1070889.328215	42.531725
3515.749778	1070561.368900	42.536730
3515.962816	1070232.059353	42.541735
3515.936505	1069913.537922	42.546740
3515.757709	1069617.618910	42.551744
3515.638321	1069284.941892	42.556749
3515.601914	1068964.732311	42.561754
3515.680944	1068638.522523	42.566759
3515.889539	1068335.546320	42.571764
3515.918094	1068011.327221	42.576768
3515.612327	1067696.089321	42.581773
3515.664318	1067379.812471	42.586778
3516.020325	1067072.702227	42.591783
3515.886583	1066751.321322	42.596788
3515.215508	1066442.036096	42.601792
3515.674035	1066100.796917	42.606797
3515.559461	1065793.500205	42.611802
3515.391122	1065493.508219	42.616807
3515.489873	1065183.159267	42.621812
3515.496212	1064860.586103	42.626816
3515.577123	1064553.091572	42.631821
3515.327668	1064244.671784	42.636826
3515.470603	1063917.689694	42.641831
3515.391384	1063604.200821	42.646836
3515.271887	1063282.807131	42.651840
3515.544567	1062982.701701	42.656845
3515.019565	1062667.403738	42.661850
3514.649478	1062376.131997	42.666855
3515.138419	1062063.617077	42.671860
3515.040965	1061751.951314	42.676864
3514.932927	1061452.402853	42.681869
3514.924622	1061173.911424	42.686874
3514.836917	1060855.644887	42.691879
3515.019691	1060551.280513	42.696884
3514.771165	1060242.443484	42.701888
3514.848998	1059929.489864	42.706893
3514.719582	1059634.565779	42.711898
3514.895872	1059343.621504	42.716903
3515.025449	1059047.660024	42.721908
3514.745492	1058749.534223	42.726912
3514.546108	1058457.063531	42.731917
3514.133314	1058152.761068	42.736922
3514.498455	1057860.551159	42.741927
3514.569187	1057559.990658	42.746932
3514.251458	1057249.840892	42.751936
3514.380512	1056948.466507	42.756941
3514.456037	1056678.214877	42.761946
3514.223329	1056405.205656	42.766951
3514.207601	1056100.724532	42.771956
3514.084731	1055811.570893	42.776960
3514.584782	1055510.635232	42.781965
3514.406475	1055221.845425	42.786970
3514.242867	1054939.208270	42.791975
3513.898058	1054657.357798	42.796980
3513.601703	1054368.735626	42.801985
3513.793809	1054091.395944	42.806989
3513.866361	1053808.662020	42.811994
3514.195420	1053517.867373	42.816999
3514.183095	1053235.021640	42.822004
3513.914136	1052942.462867	42.827009
3513.999926	1052682.140505	42.832013
3513.847163	1052374.582998	42.837018
3513.828875	1052092.933691	42.842023
3514.180189	1051817.093442	42.847028
3513.780106	1051517.728391	42.852033
3513.906334	1051231.091472	42.857037
3513.731092	1050954.330178	42.862042
3513.822699	1050681.273936	42.867047
3513.873757	1050406.281134	42.872052
3513.899178	1050126.357745	42.877057
3513.843453	1049815.843634	42.882061
3513.792081	1049548.062433	42.887066
3513.826900	1049260.759473	42.892071
3513.953755	1048985.587087	42.897076
3513.813203	1048713.437117	42.902081
3513.477304	1048414.183076	42.907085
3513.479808	1048147.097419	42.912090
3513.329572	1047865.447658	42.917095
3513.639527	1047603.594442	42.922100
3513.309701	1047314.416350	42.927105
3513.548380	1047043.280352	42.932109
3513.679334	1046778.231576	42.937114
3513.465274	1046483.197950	42.942119
3513.371761	1046203.482047	42.947124
3513.327029	1045954.065724	42.952129
3513.476074	1045683.167664	42.957133
3513.239973	1045398.992414	42.962138
3513.248429	1045110.802524	42.967143
3513.234238	1044849.741837	42.972148
3512.938065	1044585.044903	42.977153
3513.126875	1044312.044947	42.982157
3513.251630	1044034.501953	42.987162
3513.075128	1043777.957727	42.992167
3513.240569	1043495.937333	42.997172
3512.960580	1043243.636226	43.002177
3513.015390	1042980.930444	43.007181
3513.133901	1042692.596832	43.012186
3513.004857	1042438.301813	43.017191
3513.153619	1042191.679899	43.022196
3513.153085	1041912.215449	43.027201
3513.218653	1041616.876912	43.032205
3513.004804	1041368.248699	43.037210
3512.858357	1041102.104600	43.042215
3512.940660	1040822.571697	43.047220
3512.981493	1040543.804845	43.052225
3513.234314	1040279.005471	43.057229
3512.996451	1040019.397764	43.062234
3513.001301	1039750.070595	43.067239
3512.901003	1039495.346117	43.072244
3512.512012	1039233.116273	43.077249
3512.487090	1038949.446176	43.082253
3512.570397	1038713.799777	43.087258
3512.398428	1038450.723765	43.092263
3512.534586	1038191.839400	43.097268
3512.610221	1037937.111287	43.102273
3512.759013	1037663.984606	43.107277
3512.463612	1037427.862577	43.112282
3512.410566	1037168.188051	43.117287
3512.652103	1036900.231427	43.122292
3512.452600	1036655.355738	43.127297
3512.772789	1036382.234681	43.132301
3512.363944	1036118.410312	43.137306
3512.371898	1035866.597453	43.142311
3512.285907	1035621.560870	43.147316
3512.454761	1035368.344557	43.152321
3512.342437	1035113.227965	43.157325
3512.129147	1034855.600596	43.162330
3512.447528	1034606.775956	43.167335
3512.583612	1034334.939558	43.172340
3512.282494	1034083.967959	43.177345
3512.399484	1033813.947976	43.182349
3512.313459	1033580.725201	43.187354
3512.207724	1033333.268519	43.192359
3512.246069	1033074.936700	43.197364
3511.962449	1032815.097239	43.202369
3512.007525	1032578.907155	43.207373
3512.039927	1032331.867288	43.212378
3511.491809	1032071.649548	43.217383
3512.055035	1031830.114850	43.222388
3511.908251	1031576.584707	43.227393
3511.836483	1031333.196784	43.232397
3511.775370	1031110.904101	43.237402
3511.770662	1030849.862122	43.242407
3511.964534	1030598.264835	43.247412
3511.764164	1030369.090439	43.252417
3511.813941	1030110.425838	43.257421
3512.033650	1029884.358119	43.262426
3511.804464	1029634.820861	43.267431
3511.754714	1029376.041802	43.272436
3511.808229	1029145.032000	43.277441
3511.856256	1028900.452889	43.282445
3511.729259	1028670.518688	43.287450
3511.495373	1028424.512191	43.292455
3511.793583	1028177.825982	43.297460
3511.538883	1027948.658116	43.302465
3511.634606	1027699.755962	43.307469
3511.516940	1027444.580210	43.312474
3511.358395	1027200.057620	43.317479
3511.549942	1026966.028301	43.322484
3511.193195	1026738.281068	43.327489
3511.515287	1026504.404739	43.332493
3511.583490	1026280.541926	43.337498
3511.626834	1026035.547556	43.342503
3511.943274	1025786.717762	43.347508
3511.389902	1025553.430468	43.352513
3511.278808	1025309.205100	43.357517
3511.352660	1025098.669614	43.362522
3511.000698	1024842.444487	43.367527
3511.582651	1024611.063436	43.372532
3511.265330	1024369.642203	43.377537
3511.305213	1024157.331996	43.382541
3511.127681	1023927.211121	43.387546
3511.182909	1023685.117332	43.392551
3511.056022	1023458.943924	43.397556
3510.986679	1023219.080510	43.402561
3511.004216	1022986.076997	43.407565
3511.174119	1022763.608254	43.412570
3511.131424	1022533.020036	43.417575
3511.147494	1022306.485655	43.422580
3511.111329	1022092.461142	43.427585
3510.992583	1021855.262937	43.432589
3510.963312	1021613.481519	43.437594
3510.843529	1021396.146602	43.442599
3510.977788	1021166.927936	43.447604
3510.997387	1020955.954732	43.452609
3511.188823	1020718.172351	43.457613
3510.992336	1020476.272452	43.462618
3510.755071	1020257.942706	43.467623
3511.074950	1020034.273869	43.472628
3510.304916	1019810.484574	43.477633
3510.614818	1019576.126988	43.482637
3510.640783	1019359.756433	43.487642
3510.758631	1019144.623808	43.492647
3510.839415	1018925.219524	43.497652
3510.595716	1018702.269689	43.502657
3511.001722	1018494.439619	43.507661
3510.974545	1018247.854810	43.512666
3510.700733	1018013.042906	43.517671
3510.790794	1017793.301727	43.522676
3510.698264	1017566.690908	43.527681
3510.705297	1017355.487389	43.532685
3510.593035	1017143.421992	43.537690
3510.433182	1016929.317979	43.542695
3510.239380	1016691.525585	43.547700
3510.212379	1016495.632904	43.552705
3510.403213	1016272.806300	43.557709
3510.243596	1016044.300611	43.562714
3510.146731	1015844.513373	43.567719
3510.439959	1015619.410995	43.572724
3510.415375	1015395.031625	43.577729
3510.559034	1015184.889198	43.582733
3510.415047	1014986.924142	43.587738
3510.364637	1014760.193239	43.592743
3510.544137	1014545.068576	43.597748
3510.440635	1014343.578243	43.602753
3510.409845	1014117.498007	43.607757
3510.332047	1013903.847976	43.612762
3510.018746	1013696.541745	43.617767
3509.970794	1013474.906266	43.622772
3509.991488	1013277.630975	43.627777
3510.042824	1013058.099642	43.632781
3510.111612	1012861.773220	43.637786
3509.889539	1012650.819293	43.642791
3509.688786	1012442.185467	43.647796
3509.693909	1012232.247052	43.652801
3509.868294	1012024.216010	43.657805
3509.705415	1011818.953241	43.662810
3509.497371	1011624.961076	43.667815
3509.674313	1011443.432964	43.672820
3509.774123	1011243.547135	43.677825
3509.835631	1011029.182078	43.682829
3510.125328	1010809.426680	43.687834
3509.523493	1010603.900418	43.692839
3509.966469	1010395.570665	43.697844
3509.365711	1010203.440696	43.702849
3509.859344	1009995.768128	43.707853
3510.175942	1009794.045803	43.712858
3509.761460	1009598.948783	43.717863
3509.763129	1009406.984033	43.722868
3509.726678	1009193.731709	43.727873
3509.592991	1008983.111906	43.732877
3509.537861	1008782.483901	43.737882
3509.626771	1008601.073197	43.742887
3509.592463	1008393.720255	43.747892
3509.778060	1008200.712002	43.752897
3509.924289	1007977.856100	43.757901
3509.598945	1007784.237194	43.762906
3509.182108	1007603.169391	43.767911
3509.521136	1007388.036839	43.772916
3509.562437	1007203.963763	43.777921
3509.548267	1007015.420781	43.782925
3509.719196	1006806.419883	43.787930
3509.432338	1006590.095853	43.792935
3509.415128	1006420.204968	43.797940
3509.163594	1006242.470048	43.802945
3509.225399	1006027.331328	43.807949
3509.563120	1005827.895197	43.812954
3509.277377	1005644.505982	43.817959
3509.356811	1005451.323975	43.822964
3509.164029	1005256.429332	43.827969
3509.138760	1005054.983035	43.832973
3509.162644	1004874.436040	43.837978
3508.945488	1004696.549538	43.842983
3509.328589	1004517.196610	43.847988
3509.062674	1004321.406219	43.852993
3509.275907	1004117.552357	43.857997
3509.336632	1003922.667258	43.863002
3508.726258	1003736.642668	43.868007
3508.923201	1003541.138205	43.873012
3509.155858	1003374.811999	43.878017
3508.860685	1003195.918098	43.883021
3508.793284	1002987.107115	43.888026
3508.685080	1002812.354589	43.893031
3508.889502	1002625.769997	43.898036
3508.734322	1002444.785652	43.903041
3508.840568	1002243.314837	43.908045
3509.066507	1002073.447886	43.913050
3508.555587	1001896.786907	43.918055
3508.781314	1001702.090115	43.923060
3508.634767	1001528.277561	43.928065
3508.630361	1001344.215815	43.933069
3508.830874	1001173.352670	43.938074
3508.515641	1000980.764323	43.943079
3508.751279	1000809.592386	43.948084
3508.672363	1000636.520089	43.953089
3508.539887	1000445.635736	43.958093
3508.661440	1000268.332985	43.963098
3508.615133	1000100.398808	43.968103
3508.578004	999894.389502	43.973108
3508.386221	999730.654912	43.978113
3508.499593	999557.907448	43.983117
3508.606411	999383.987342	43.988122
3508.095374	999216.006118	43.993127
3508.408744	999055.090030	43.998132
3508.294566	998869.797423	44.003137
3508.123146	998693.175298	44.008141
3508.209698	998525.464708	44.013146
3508.120580	998349.889577	44.018151
3508.313174	998184.488774	44.023156
3508.027104	998031.336320	44.028161
3508.230694	997842.743781	44.033165
3508.386266	997673.340857	44.038170
3508.016742	997517.948062	44.043175
3508.263299	997342.968290	44.048180
3508.256346	997189.552314	44.053185
3507.959364	996997.409979	44.058189
3508.132597	996824.764197	44.063194
3508.119148	996656.040640	44.068199
3508.261849	996502.873701	44.073204
3507.927612	996323.087091	44.078209
3508.188080	996160.343960	44.083213
3508.252747	996001.623021	44.088218
3507.921187	995831.173601	44.093223
3507.914969	995653.455259	44.098228
3508.153415	995502.194255	44.103233
3508.092898	995360.040431	44.108237
3508.302885	995171.552937	44.113242
3507.944451	994999.036632	44.118247
3508.138092	994836.948702	44.123252
3508.107529	994687.951654	44.128257
3508.345967	994505.674299	44.133261
3508.320321	994337.468559	44.138266
3507.924701	994172.632443	44.143271
3508.063347	993994.253545	44.148276
3507.889983	993823.522853	44.153281
3508.055871	993665.597144	44.158285
3507.788295	993505.009217	44.163290
3507.673010	993343.611865	44.168295
3507.877678	993169.387625	44.173300
3507.762777	993024.064986	44.178305
3507.749601	992855.910806	44.183309
3507.939977	992685.378454	44.188314
3507.791839	992526.400462	44.193319
3507.848297	992374.891188	44.198324
3507.858955	992225.822776	44.203329
3507.829739	992052.577774	44.208333
3507.727752	991881.484482	44.213338
3507.572125	991728.627916	44.218343
3507.687077	991574.065084	44.223348
3507.311392	991429.329657	44.228353
3507.510771	991274.549765	44.233357
3507.658609	991113.923359	44.238362
3507.738981	990962.762577	44.243367
3507.649985	990802.361414	44.248372
3507.755284	990644.459281	44.253377
3507.655223	990480.247527	44.258381
3507.482902	990322.967342	44.263386
3507.157828	990167.853618	44.268391
3507.112589	990007.130238	44.273396
3507.050729	989866.692300	44.278401
3507.454158	989717.590994	44.283405
3507.297898	989569.943525	44.288410
3507.142264	989436.045565	44.293415
3507.466423	989269.875714	44.298420
3507.466508	989128.336364	44.303425
3507.283112	988979.019733	44.308429
3507.433653	988836.180192	44.313434
3507.424251	988676.681526	44.318439
3507.721751	988515.957152	44.323444
3506.798207	988388.404722	44.328449
3507.176653	988216.731845	44.333453
3507.327972	988062.262770	44.338458
3507.356255	987936.787456	44.343463
3507.219200	987791.725035	44.348468
3506.874209	987634.789288	44.353473
3506.710127	987498.017527	44.358477
3506.871950	987333.183973	44.363482
3506.753021	987198.544302	44.368487
3506.854477	987061.815915	44.373492
3506.866675	986929.685444	44.378497
3507.218996	986773.099035	44.383501
3507.025862	986633.969215	44.388506
3507.025521	986493.730727	44.393511
3506.793307	986363.188859	44.398516
3506.760834	986217.093176	44.403521
3506.944027	986070.177431	44.408525
3507.137109	985928.526788	44.413530
3506.910059	985781.671179	44.418535
3506.994826	985626.463818	44.423540
3507.108815	985508.631897	44.428545
3506.763606	985350.071506	44.433549
3507.121638	985207.692512	44.438554
3506.733647	985068.556578	44.443559
3506.958315	984913.013911	44.448564
3506.926281	984804.465338	44.453569
3506.890771	984648.274958	44.458573
3507.124865	984509.803925	44.463578
3506.864947	984373.558730	44.468583
3507.106872	984217.017966	44.473588
3506.613097	984088.907888	44.478593
3506.390698	983962.117135	44.483597
3506.744706	983813.748246	44.488602
3506.781244	983688.178057	44.493607
3506.708066	983548.562629	44.498612
3506.526522	983419.312015	44.503617
3506.634269	983273.703715	44.508621
3506.442412	983148.647513	44.513626
3506.353573	983009.900335	44.518631
3506.920507	982864.205964	44.523636
3506.787433	982734.345932	44.528641
3506.478327	982586.737981	44.533645
3506.745651	982457.684642	44.538650
3506.396110	982321.698201	44.543655
3506.566029	982176.930671	44.548660
3506.493407	982064.234680	44.553665
3506.585424	981921.231529	44.558669
3506.664317	981789.947719	44.563674
3506.376929	981669.856176	44.568679
3506.668534	981506.297993	44.573684
3506.477503	981403.180873	44.578689
3506.184721	981288.649931	44.583693
3506.328470	981157.731639	44.588698
3506.030069	981012.523322	44.593703
3505.982799	980891.789753	44.598708
3506.416457	980770.681352	44.603713
3506.350896	980642.716448	44.608717
3506.671916	980497.295327	44.613722
3505.992241	980375.873460	44.618727
3505.977318	980244.667299	44.623732
3506.122315	980127.207689	44.628737
3506.080102	979994.241652	44.633741
3506.350862	979861.611799	44.638746
3505.707453	979749.257275	44.643751
3506.313018	979636.792537	44.648756
3506.157612	979526.405159	44.653761
3506.153587	979382.279473	44.658765
3506.291516	979259.526648	44.663770
3506.231914	979135.924259	44.668775
3506.361995	978998.607092	44.673780
3506.413994	978884.557501	44.678785
3506.222357	978772.891151	44.683789
3506.492080	978628.115031	44.688794
3506.129757	978517.058161	44.693799
3506.238049	978377.481912	44.698804
3506.154056	978253.278082	44.703809
3506.225390	978118.099593	44.708813
3506.420782	978006.256798	44.713818
3506.272088	977887.333506	44.718823
3506.030755	977749.070132	44.723828
3506.154923	977635.081492	44.728833
3506.142356	977507.819657	44.733837
3506.413936	977379.823956	44.738842
3505.945679	977270.226547	44.743847
3505.844844	977131.045349	44.748852
3505.763706	977014.927622	44.753857
3505.953555	976892.213221	44.758861
3505.960191	976754.471515	44.763866
3505.930153	976655.641387	44.768871
3506.312725	976529.954665	44.773876
3506.076461	976408.179943	44.778881
3505.803651	976280.053796	44.783885
3505.889415	976174.939207	44.788890
3505.882955	976052.141374	44.793895
3506.163710	975918.734109	44.798900
3505.896134	975798.027072	44.803905
3505.988793	975702.386868	44.808909
3506.219719	975573.281950	44.813914
3506.095289	975437.192397	44.818919
3506.313670	975322.848876	44.823924
3505.809909	975224.267640	44.828929
3505.773495	975081.212393	44.833933
3506.007308	974978.105000	44.838938
3505.868402	974859.703937	44.843943
3505.869554	974723.087782	44.848948
3505.876993	974613.850124	44.853953
3505.629463	974510.129026	44.858957
3505.777559	974378.174712	44.863962
3505.959254	974256.383198	44.868967
3505.787920	974141.395688	44.873972
3505.667951	974020.431275	44.878977
3505.496185	973920.794864	44.883981
3505.586270	973799.986816	44.888986
3505.367044	973704.658074	44.893991
3505.506990	973580.805057	44.898996
3505.494740	973490.622755	44.904001
3505.344739	973378.257417	44.909005
3505.103286	973256.514361	44.914010
3504.910366	973181.420998	44.919015
3505.327652	973060.934771	44.924020
3505.619484	972945.357877	44.929025
3505.409350	972835.926533	44.934029
3505.320615	972714.342465	44.939034
3505.214495	972625.629441	44.944039
3505.334002	972527.192619	44.949044
3505.396889	972415.262505	44.954049
3505.180319	972307.093958	44.959053
3505.371901	972193.181619	44.964058
3504.982065	972090.516380	44.969063
3505.034855	971986.700156	44.974068
3504.937105	971895.430615	44.979073
3505.114865	971770.456028	44.984077
3505.072045	971656.375956	44.989082
3504.974267	971578.212706	44.994087
3505.315232	971471.795679	44.999092
3505.204150	971362.515610	45.004097
3504.911216	971277.628695	45.009101
3505.323573	971162.974585	45.014106
3505.025690	971085.913987	45.019111
3505.105741	970984.227967	45.024116
3505.127163	970887.442754	45.029121
3505.128554	970782.145328	45.034125
3504.823040	970671.905526	45.039130
3504.935005	970577.057421	45.044135
3504.769337	970474.717799	45.049140
3504.862317	970384.469343	45.054145
3504.890889	970268.686186	45.059149
3505.067613	970172.059076	45.064154
3504.873164	970088.508547	45.069159
3505.203831	969998.019126	45.074164
3504.864421	969891.782765	45.079169
3504.933747	969783.813193	45.084173
3505.091444	969689.236532	45.089178
3504.917898	969587.078147	45.094183
3505.355225	969486.187692	45.099188
3505.090316	969406.847812	45.104193
3504.780815	969301.672332	45.109197
3505.133403	969196.581652	45.114202
3505.120524	969093.311258	45.119207
3505.026024	969013.448428	45.124212
3505.195433	968916.801417	45.129217
3504.965150	968796.430272	45.134221
3504.842817	968703.547721	45.139226
3504.541349	968608.735216	45.144231
3504.964174	968500.095916	45.149236
3504.473191	968417.451014	45.154241
3504.569379	968321.687167	45.159245
3504.746024	968242.160569	45.164250
3504.508980	968162.407292	45.169255
3504.623774	968066.538226	45.174260
3504.990280	967960.933136	45.179265
3504.738728	967876.380745	45.184269
3505.144687	967776.640389	45.189274
3504.960217	967680.912097	45.194279
3504.818624	967586.839708	45.199284
3504.624765	967509.909804	45.204289
3504.538675	967393.793855	45.209293
3504.543371	967310.268033	45.214298
3504.434064	967246.637773	45.219303
3504.658799	967132.130002	45.224308
3504.655009	967059.177601	45.229313
3504.467765	966959.814562	45.234317
3504.782421	966863.207039	45.239322
3504.648040	966776.170977	45.244327
3504.811550	966695.645872	45.249332
3504.616333	966588.443294	45.254337
3504.390214	966512.386745	45.259341
3504.786424	966421.536451	45.264346
3504.521220	966325.015401	45.269351
3504.653219	966252.715964	45.274356
3504.740487	966164.263005	45.279361
3504.358753	966071.870353	45.284365
3504.654322	965988.179486	45.289370
3504.543360	965899.950998	45.294375
3504.677407	965805.608184	45.299380
3504.549805	965713.853543	45.304385
3504.218650	965628.105830	45.309389
3504.587295	965525.785952	45.314394
3504.497963	965462.916270	45.319399
3504.414382	965360.961802	45.324404
3504.369476	965280.745088	45.329409
3504.329012	965200.330614	45.334413
3504.346167	965103.154820	45.339418
3503.993356	965034.544361	45.344423
3504.528962	964958.145884	45.349428
3504.500787	964863.030662	45.354433
3504.327498	964793.799994	45.359437
3504.624069	964701.077679	45.364442
3504.368523	964623.237641	45.369447
3504.701051	964540.695241	45.374452
3504.414034	964458.939481	45.379457
3504.503130	964375.553093	45.384461
3504.632796	964272.172641	45.389466
3504.361884	964182.670540	45.394471
3504.459476	964101.434194	45.399476
3504.587204	964025.482436	45.404481
3504.406012	963929.691170	45.409485
3504.359763	963835.835665	45.414490
3504.303231	963765.397650	45.419495
3504.382418	963682.002855	45.424500
3504.442982	963588.615638	45.429505
3504.208594	963507.131641	45.434509
3504.588317	963431.130544	45.439514
3504.013515	963367.730024	45.444519
3504.400377	963273.402072	45.449524
3504.518932	963170.199653	45.454529
3504.352018	963095.558041	45.459533
3504.011019	963007.421098	45.464538
3504.102477	962934.498719	45.469543
3504.146923	962852.469562	45.474548
3504.142674	962779.560987	45.479553
3504.134933	962704.104110	45.484557
3504.167417	962622.563643	45.489562
3504.179165	962546.317492	45.494567
3504.114994	962464.594708	45.499572
3504.007537	962391.306211	45.504577
3504.113339	962301.222802	45.509581
3504.337115	962221.801272	45.514586
3503.976742	962156.489965	45.519591
3504.227788	962074.611726	45.524596
3504.143078	961993.963751	45.529601
3503.722762	961926.405469	45.534605
3503.978726	961838.054299	45.539610
3503.790095	961764.967232	45.544615
3503.842183	961685.076518	45.549620
3504.068184	961606.528289	45.554625
3503.923828	961544.409022	45.559629
3504.157409	961489.970337	45.564634
3503.951496	961411.392572	45.569639
3504.073491	961336.288503	45.574644
3503.756926	961275.468981	45.579649
3503.918545	961191.926558	45.584653
3504.074217	961101.718174	45.589658
3503.966770	961036.254483	45.594663
3504.147058	960952.509466	45.599668
3504.482892	960876.383910	45.604673
3503.694495	960813.970731	45.609677
3503.549288	960740.079274	45.614682
3503.587415	960664.686180	45.619687
3503.751251	960599.663016	45.624692
3503.460111	960531.674965	45.629697
3503.605865	960462.045571	45.634701
3504.027000	960382.076025	45.639706
3503.777180	960321.039362	45.644711
3503.609518	960242.635445	45.649716
3504.018958	960192.469321	45.654721
3503.621053	960128.513781	45.659725
3503.804947	960047.794344	45.664730
3503.714911	959968.687613	45.669735
3503.846271	959896.700695	45.674740
3504.310766	959846.718594	45.679745
3503.834884	959764.731212	45.684749
3503.750867	959680.422979	45.689754
3504.043705	959606.739005	45.694759
3503.922853	959519.787116	45.699764
3503.983375	959463.690935	45.704769
3503.968886	959404.664933	45.709773
3504.281672	959319.697749	45.714778
3503.802727	959250.843028	45.719783
3503.827040	959190.827878	45.724788
3503.873606	959084.034100	45.729793
3503.598241	959008.474883	45.734797
3503.816602	958945.091140	45.739802
3503.746284	958890.972187	45.744807
3503.799331	958835.753704	45.749812
3503.966472	958746.781454	45.754817
3503.576612	958661.822256	45.759821
3503.609414	958516.774003	45.764826
3503.567588	958347.314442	45.769831
3503.568804	958099.578279	45.774836
3503.700760	957795.805584	45.779841
3503.488006	957416.055888	45.784845
3503.886762	956980.070133	45.789850
3503.833658	956485.460063	45.794855
3503.290614	955883.469036	45.799860
3503.486591	955270.758663	45.804865
3503.270325	954598.838733	45.809869
3503.417304	953852.348479	45.814874
3502.985709	953025.670044	45.819879
3502.917448	952121.671671	45.824884
3502.913059	951162.375163	45.829889
3502.588937	950120.626236	45.834893
3502.444371	949010.272298	45.839898
3502.394243	947822.472613	45.844903
3502.565258	946559.548371	45.849908
3502.240070	945227.504305	45.854913
3501.896280	943797.935025	45.859917
3501.697715	942290.388276	45.864922
3501.423881	940720.562051	45.869927
3501.402791	939051.893533	45.874932
3501.118336	937305.199559	45.879937
3500.552578	935471.095672	45.884941
3500.713200	933543.469201	45.889946
3500.307805	931539.245960	45.894951
3499.805358	929462.013320	45.899956
3499.942095	927291.762458	45.904961
3499.270371	925048.533343	45.909965
3499.218865	922713.913107	45.914970
3498.370480	920292.065207	45.919975
3498.393389	917751.686747	45.924980
3498.149261	915176.447021	45.929985
3497.650673	912500.938327	45.934989
3497.351753	909699.579603	45.939994
3496.805223	906858.441108	45.944999
3496.467163	903927.090879	45.950004
3495.799153	900911.282109	45.955009
3495.455881	897817.161268	45.960013
3495.035878	894617.984864	45.965018
3494.741342	891344.327633	45.970023
3494.161128	888000.790727	45.975028
3493.786619	884541.845415	45.980033
3492.822834	881026.759819	45.985037
3492.499240	877405.582970	45.990042
3491.867028	873708.188042	45.995047
3491.395300	869920.485823	46.000052
3490.991131	866059.541680	46.005057
3490.436851	862113.699698	46.010061
3490.088535	858075.557389	46.015066
3488.923285	853968.884209	46.020071
3488.552405	849763.681184	46.025076
3488.079544	845465.968970	46.030081
3487.232397	841104.805597	46.035085
3486.913128	836631.022777	46.040090
3485.994778	832083.197547	46.045095
3485.191736	827465.879945	46.050100
3484.797831	822745.444265	46.055105
3483.391541	817957.778324	46.060109
3483.221922	813074.624025	46.065114
3481.995565	808132.425323	46.070119
3481.011206	803077.299840	46.075124
3480.675165	797929.009445	46.080129
3479.762272	792702.877491	46.085133
3478.977155	787399.792935	46.090138
3478.266451	782028.155859	46.095143
3477.162727	776572.723041	46.100148
3476.499556	770994.581743	46.105153
3475.380872	765347.421048	46.110157
3474.650057	759620.489935	46.115162
3473.428981	753798.598092	46.120167
3472.542370	747891.047089	46.125172
3471.955067	741899.197501	46.130177
3470.694328	735829.621021	46.135181
3469.669279	729657.633837	46.140186
3468.935366	723424.817991	46.145191
3467.929170	717095.127677	46.150196
3467.016102	710664.338580	46.155201
3465.953629	704145.960070	46.160205
3464.714149	697534.859532	46.165210
3463.464784	690859.705690	46.170215
3462.554723	684111.072562	46.175220
3461.302504	677262.283374	46.180225
3460.440182	670307.054736	46.185229
3458.849825	663287.416660	46.190234
3457.829034	656195.072540	46.195239
3456.080767	648995.488519	46.200244
3455.122437	641724.559976	46.205249
3453.735849	634383.296867	46.210253
3452.423135	626933.006195	46.215258
3450.982843	619419.329609	46.220263
3449.767018	611827.398694	46.225268
3448.408327	604151.564222	46.230273
3446.733643	596398.843873	46.235277
3445.434956	588559.046539	46.240282
3443.579987	580629.873407	46.245287
3442.255478	572648.906511	46.250292
3440.743249	564556.878643	46.255297
3439.117196	556387.929413	46.260301
3438.007994	548159.356169	46.265306
3435.889915	539845.318707	46.270311
3434.217914	531455.675935	46.275316
3432.925940	522972.433624	46.280321
3430.762313	514434.310504	46.285325
3429.189677	505821.975363	46.290330
3427.062742	497123.220503	46.295335
3425.507512	488348.779537	46.300340
3423.569766	479511.277434	46.305345
3421.470522	470589.434242	46.310349
3419.816046	461598.723429	46.315354
3418.184349	452542.653476	46.320359
3415.729004	443414.060805	46.325364
3414.010142	434230.958792	46.330369
3411.912557	424968.987388	46.335373
3410.034327	415634.861739	46.340378
3407.458724	406215.216922	46.345383
3405.452474	396719.341571	46.350388
3403.078677	387178.820366	46.355393
3400.769518	377601.207366	46.360397
3398.600097	367936.878938	46.365402
3396.083429	358218.276538	46.370407
3393.584726	348432.347130	46.375412
3391.233198	338601.066738	46.380417
3388.603857	328721.327148	46.385421
3386.175608	318763.246058	46.390426
3383.505336	308788.032362	46.395431
3380.248220	298756.281297	46.400436
3377.941854	288637.613701	46.405441
3374.688052	278488.628934	46.410445
3372.165439	268325.116761	46.415450
3369.046735	258100.536834	46.420455
3365.767879	247832.039293	46.425460
3362.762834	237510.499371	46.430465
3359.457591	227190.578555	46.435469
3356.256732	216736.562297	46.440474
3353.152353	206333.106363	46.445479
3349.111569	195898.660125	46.450484
3345.603709	185460.289999	46.455489
3341.337457	175012.396200	46.460493
3337.643607	164511.456504	46.465498
3333.430460	154009.385043	46.470503
3329.148594	143536.574051	46.475508
3324.724281	133068.411748	46.480513
3319.800459	122586.803964	46.485517
3314.706563	112115.732245	46.490522
3309.290992	101670.882223	46.495527
3303.442420	91277.232043	46.500532
3296.903126	80923.671462	46.505537
3287.699592	70682.740096	46.510541
3269.764989	60785.285906	46.515546
3245.214428	51228.554109	46.520551
3220.106107	42007.237052	46.525556
3194.955824	33204.724509	46.530561
3166.159215	24961.266944	46.535565
3128.834581	17508.212055	46.540570
3082.916814	10964.839066	46.545575
3035.992716	5305.773479	46.550580
2973.296924	1070.192920	46.555585
2822.831057	376.866736	46.560589
2720.404812	351.520482	46.565594
2699.835026	367.889436	46.570599
2736.487716	359.930034	46.575604
2796.550255	357.947697	46.580609
2852.010605	339.286231	46.585613
2889.312784	327.798368	46.590618
2906.014582	336.062697	46.595623
2905.990252	345.028272	46.600628
2898.653332	329.867611	46.605633
2888.334171	329.398462	46.610637
2880.045433	325.282905	46.615642
2875.151850	335.095380	46.620647
2871.947277	315.742161	46.625652
2870.381117	319.909018	46.630657
2868.487026	333.933436	46.635661
2866.598860	326.679430	46.640666
2864.668380	321.107883	46.645671
2862.265232	309.321742	46.650676
2859.569276	314.088098	46.655681
2856.152304	314.402252	46.660685
2853.051002	319.615141	46.665690
2850.058091	315.755132	46.670695
2847.022029	312.947540	46.675700
2844.193846	288.852544	46.680705
2841.050230	302.994639	46.685709
2837.813954	315.514622	46.690714
2834.522212	305.588843	46.695719
2831.395609	307.495102	46.700724
2828.607736	308.479466	46.705729
2824.943426	293.491714	46.710733
2821.776504	288.117423	46.715738
2818.541992	301.946792	46.720743
2815.043429	313.869090	46.725748
2812.196065	303.175861	46.730753
2808.573093	309.883887	46.735757
2805.417763	300.493604	46.740762
2802.441221	287.562792	46.745767
2798.560504	280.851300	46.750772
2795.411136	282.466161	46.755777
2792.156201	279.426650	46.760781
2788.945969	280.902488	46.765786
2785.755356	294.331007	46.770791
2781.601627	295.822117	46.775796
2778.386128	281.224365	46.780801
2775.448916	312.961253	46.785805
2771.862033	302.691539	46.790810
2768.907157	278.727389	46.795815
2764.925152	285.940120	46.800820
2761.781532	273.526389	46.805825
2758.661733	276.902226	46.810829
2754.997613	277.046848	46.815834
2751.583417	286.371590	46.820839
2747.967867	277.660177	46.825844
2745.268106	279.207935	46.830849
2741.280103	296.986509	46.835853
2737.699723	286.678267	46.840858
2734.481864	265.759739	46.845863
2731.066728	287.602844	46.850868
2728.124445	283.297135	46.855873
2724.271901	266.513704	46.860877
2720.382777	261.829035	46.865882
2717.371278	267.653674	46.870887
2714.036713	283.948834	46.875892
2710.352946	283.393834	46.880897
2706.707610	269.944361	46.885901
2704.058370	258.400939	46.890906
2701.008434	255.911288	46.895911
2696.683944	263.162157	46.900916
2693.176298	272.217417	46.905921
2689.929548	260.645355	46.910925
2686.479595	264.001565	46.915930
2682.884326	271.256905	46.920935
2679.610142	261.972132	46.925940
2675.423675	254.752381	46.930945
2672.210297	261.551142	46.935949
2669.317739	277.691352	46.940954
2666.339488	268.316947	46.945959
2662.079264	263.500143	46.950964
2658.540810	263.564013	46.955969
2654.987381	269.970290	46.960973
2651.673796	266.505371	46.965978
2648.526812	261.794461	46.970983
2645.452588	268.452206	46.975988
2641.791888	270.860137	46.980993
2637.981550	267.978568	46.985997
2634.411010	252.363788	46.991002
2631.121662	243.672169	46.996007
2627.094452	255.700394	47.001012
2624.118827	249.999902	47.006017
2620.805558	267.858313	47.011021
2617.386617	255.055125	47.016026
2613.705824	247.008513	47.021031
2609.812778	255.028678	47.026036
2606.978726	240.908966	47.031041
2603.156193	236.833009	47.036045
2599.816014	247.579449	47.041050
2596.450468	261.534227	47.046055
2592.532391	252.290075	47.051060
2589.271948	235.251400	47.056065
2585.770113	255.279821	47.061069
2582.033191	252.703140	47.066074
2578.732702	254.336688	47.071079
2575.600244	246.790792	47.076084
2572.351575	252.691179	47.081089
2568.538004	256.021371	47.086093
2565.107284	255.373912	47.091098
2561.659503	252.326062	47.096103
2557.800113	234.056470	47.101108
2554.777795	246.096979	47.106113
2550.788736	245.621599	47.111117
2547.623502	249.084216	47.116122
2544.107472	241.256017	47.121127
2540.647779	234.166101	47.126132
2537.503732	241.657235	47.131137
2533.750183	254.144271	47.136141
2530.180099	251.361353	47.141146
2526.866024	236.250789	47.146151
2523.346189	238.742576	47.151156
2519.794225	239.329509	47.156161
2516.051343	257.563703	47.161165
2512.692263	248.030124	47.166170
2509.513493	231.273784	47.171175
2505.411163	249.075478	47.176180
2502.479150	242.710647	47.181185
2498.855122	238.199818	47.186189
2494.996330	252.392610	47.191194
2491.860485	248.447533	47.196199
2488.306852	248.901480	47.201204
2484.999110	224.912723	47.206209
2481.469720	231.330281	47.211213
2477.720574	251.221641	47.216218
2474.550214	236.466518	47.221223
2470.756696	239.853719	47.226228
2467.695346	246.527445	47.231233
2463.928047	252.247536	47.236237
2460.301995	237.280495	47.241242
2456.947541	230.263438	47.246247
2453.188715	241.117233	47.251252
2450.022456	240.122080	47.256257
2446.398273	251.139244	47.261261
2442.856805	240.049301	47.266266
2440.050524	220.450561	47.271271
2436.156410	228.316575	47.276276
2432.626346	244.996580	47.281281
2428.763211	237.234664	47.286285
2425.171554	222.657378	47.291290
2422.505219	221.252280	47.296295
2418.438217	241.322825	47.301300
2415.062991	229.527277	47.306305
2411.387078	247.118497	47.311309
2407.886724	228.144639	47.316314
2404.674197	228.498277	47.321319
2401.030518	241.090543	47.326324
2397.543475	236.712846	47.331329
2393.724112	234.122931	47.336333
2390.472192	219.605457	47.341338
2387.493478	219.002018	47.346343
2383.869986	225.867116	47.351348
2380.036678	231.156370	47.356353
2376.408786	221.848336	47.361357
2372.814812	225.818638	47.366362
2369.832269	235.528252	47.371367
2366.241380	231.617145	47.376372
2362.835457	230.628212	47.381377
2359.218945	233.708476	47.386381
2355.451940	224.285285	47.391386
2352.359705	208.527136	47.396391
2348.149914	226.527501	47.401396
2345.504490	235.791267	47.406401
2342.098802	233.320985	47.411405
2338.359676	232.656624	47.416410
2334.962734	217.699646	47.421415
2331.004447	230.700334	47.426420
2327.644268	219.816940	47.431425
2323.981701	227.222990	47.436429
2320.876285	233.522451	47.441434
2317.233715	234.730227	47.446439
2313.284623	226.805387	47.451444
2310.025338	207.175898	47.456449
2306.632160	218.194052	47.461453
2302.922703	227.920875	47.466458
2299.785364	217.651341	47.471463
2296.334958	221.607565	47.476468
2292.989115	214.615717	47.481473
2289.503762	216.721031	47.486477
2285.639623	225.885518	47.491482
2282.376187	218.698864	47.496487
2278.694664	232.397444	47.501492
2275.281947	218.249367	47.506497
2271.708037	221.492318	47.511501
2268.226346	227.709133	47.516506
2264.615966	211.742121	47.521511
2260.947684	223.252648	47.526516
2257.732866	226.864813	47.531521
2254.372792	217.747072	47.536525
2250.826090	220.638102	47.541530
2247.435130	222.164579	47.546535
2243.529231	216.369013	47.551540
2240.368939	219.517122	47.556545
2236.841817	218.733798	47.561549
2233.543846	226.890449	47.566554
2230.300136	220.628460	47.571559
2225.825639	199.886347	47.576564
2222.563915	213.403133	47.581569
2219.396446	215.475580	47.586573
2215.846219	229.246044	47.591578
2212.395076	206.362059	47.596583
2208.810600	199.353983	47.601588
2205.032531	207.066883	47.606593
2201.748539	225.695803	47.611597
2198.333955	221.856230	47.616602
2194.825167	203.314246	47.621607
2191.165102	205.469136	47.626612
2187.735963	211.128723	47.631617
2184.051248	210.837141	47.636621
2180.577245	215.972908	47.641626
2177.169194	190.299763	47.646631
2174.004527	218.840683	47.651636
2170.243881	211.451103	47.656641
2166.985035	210.446093	47.661645
2163.041713	219.914014	47.666650
2159.475438	200.555155	47.671655
2156.065517	225.420929	47.676660
2152.595387	221.764953	47.681665
2149.396239	217.424444	47.686669
2146.071671	216.556061	47.691674
2142.532700	214.564115	47.696679
2138.822600	211.856289	47.701684
2135.282587	196.019135	47.706689
2131.774902	203.093598	47.711693
2128.143448	193.236149	47.716698
2124.884349	194.384312	47.721703
2121.204467	206.560207	47.726708
2117.837561	213.184900	47.731713
2113.996503	198.034786	47.736717
2110.680859	194.404654	47.741722
2107.483668	207.387096	47.746727
2103.832724	213.443669	47.751732
2100.382624	199.749748	47.756737
2096.691854	196.321286	47.761741
2093.234170	206.073826	47.766746
2089.757903	199.186569	47.771751
2086.432602	205.295380	47.776756
2083.073428	198.679234	47.781761
2079.578488	217.041105	47.786765
2075.565537	215.422832	47.791770
2072.269112	189.413703	47.796775
2068.249161	197.571511	47.801780
2065.393218	209.434142	47.806785
2062.093361	221.310130	47.811789
2058.186554	196.303733	47.816794
2054.840795	185.750885	47.821799
2051.190669	210.115486	47.826804
2047.852833	196.552337	47.831809
2044.067216	198.122500	47.836813
2040.570277	191.980720	47.841818
2037.492056	204.511375	47.846823
2033.620752	220.780856	47.851828
2030.397669	207.053468	47.856833
2027.048432	208.258469	47.861837
2023.193188	217.907146	47.866842
2019.624931	198.894478	47.871847
2015.912643	196.150779	47.876852
2012.814551	195.313758	47.881857
2009.118592	194.835010	47.886861
2005.576365	174.980165	47.891866
2002.623254	193.829939	47.896871
1999.101602	211.511610	47.901876
1995.241966	201.591650	47.906881
1992.025132	192.216048	47.911885
1988.312970	197.240738	47.916890
1984.766116	204.149777	47.921895
1981.057700	207.569825	47.926900
1977.815524	200.850384	47.931905
1974.643393	180.328993	47.936909
1970.848279	187.887254	47.941914
1967.315466	199.866697	47.946919
1963.549374	208.610579	47.951924
1960.208573	201.729059	47.956929
1956.588439	192.815987	47.961933
1953.062278	191.562977	47.966938
1949.899489	189.456789	47.971943
1946.443356	201.401986	47.976948
1942.863160	203.067146	47.981953
1939.380287	184.174136	47.986957
1935.613973	177.949307	47.991962
1932.058742	186.490305	47.996967
1928.721071	194.062693	48.001972
1925.473147	198.433729	48.006977
1921.604456	181.268392	48.011981
1917.994594	179.528075	48.016986
1914.626904	192.708169	48.021991
1911.352874	208.705424	48.026996
1907.934064	197.730352	48.032001
1904.315948	184.208511	48.037005
1900.538716	197.082893	48.042010
1897.247221	191.947152	48.047015
1893.611041	205.570889	48.052020
1889.938692	188.026227	48.057025
1886.683255	177.728087	48.062029
1883.172519	206.658758	48.067034
1879.927003	184.053937	48.072039
1876.262404	189.012033	48.077044
1872.819535	177.892599	48.082049
1869.615588	189.708410	48.087053
1865.778191	189.310287	48.092058
1862.395109	180.620079	48.097063
1858.413853	197.608836	48.102068
1854.954254	195.944083	48.107073
1851.589394	186.896033	48.112077
1848.205780	184.917279	48.117082
1845.444945	188.438719	48.122087
1841.152369	188.242274	48.127092
1837.820985	197.731192	48.132097
1834.258734	193.816441	48.137101
1830.458318	188.284679	48.142106
1827.484025	170.602022	48.147111
1823.256433	177.086884	48.152116
1820.045791	177.814635	48.157121
1816.567113	169.035074	48.162125
1813.004100	191.668256	48.167130
1809.916610	173.401047	48.172135
1806.285001	185.852199	48.177140
1802.732608	200.138079	48.182145
1799.382408	187.175432	48.187149
1795.855081	182.274870	48.192154
1792.117750	181.753144	48.197159
1788.532853	167.172840	48.202164
1785.043690	178.135365	48.207169
1781.694334	179.206825	48.212173
1778.086694	168.692524	48.217178
1774.861412	188.452095	48.222183
1770.916021	188.902363	48.227188
1767.526892	168.942034	48.232193
1764.024981	178.116696	48.237197
1760.393631	180.753881	48.242202
1757.428371	193.781309	48.247207
1753.733700	183.903745	48.252212
1750.544105	181.448023	48.257217
1746.750537	188.909453	48.262221
1743.129457	183.562813	48.267226
1739.909670	167.752818	48.272231
1735.660156	186.623492	48.277236
1732.751079	189.792101	48.282241
1729.635845	174.352641	48.287245
1725.756982	175.781795	48.292250
1722.353581	187.029694	48.297255
1718.484100	186.006975	48.302260
1714.876186	186.758301	48.307265
1711.561968	175.282727	48.312269
1707.813151	182.072785	48.317274
1705.212646	185.146687	48.322279
1701.379381	168.416835	48.327284
1697.474137	161.641043	48.332289
1693.972771	172.394899	48.337293
1690.439330	182.358259	48.342298
1687.099810	175.761387	48.347303
1683.523964	190.731250	48.352308
1680.167708	179.138627	48.357313
1676.663574	170.813874	48.362317
1672.847212	187.179149	48.367322
1669.391471	165.790801	48.372327
1665.890792	172.455091	48.377332
1662.522857	174.097393	48.382337
1659.173950	169.809965	48.387341
1655.501529	181.034208	48.392346
1652.178312	183.270891	48.397351
1648.536098	178.919801	48.402356
1645.194462	168.279217	48.407361
1642.213859	176.088927	48.412365
1638.144038	170.438774	48.417370
1634.802561	157.350814	48.422375
1631.105061	177.185074	48.427380
1627.400577	188.215651	48.432385
1624.062059	182.869702	48.437389
1620.083881	176.485389	48.442394
1616.674924	172.239360	48.447399
1613.257394	184.947551	48.452404
1609.984675	186.614413	48.457409
1606.800132	169.178484	48.462413
1603.093886	178.476106	48.467418
1599.535087	188.412320	48.472423
1595.727289	187.571854	48.477428
1592.475517	178.888345	48.482433
1589.177989	178.072980	48.487437
1585.885218	191.007020	48.492442
1582.280032	188.242333	48.497447
1578.227458	183.719482	48.502452
1574.926232	177.784002	48.507457
1571.667825	174.768746	48.512461
1567.891385	163.755752	48.517466
1564.533184	170.530733	48.522471
1560.975878	173.394719	48.527476
1557.306542	173.577787	48.532481
1553.683215	169.967838	48.537485
1550.342520	156.497737	48.542490
1547.234108	173.509156	48.547495
1543.472144	177.784153	48.552500
1539.945614	175.641312	48.557505
1536.970782	167.548911	48.562509
1533.058058	175.637966	48.567514
1529.765262	168.615105	48.572519
1525.925297	178.558975	48.577524
1522.399539	182.612404	48.582529
1519.005080	159.277399	48.587533
1515.452888	165.015660	48.592538
1511.818948	173.367187	48.597543
1508.107129	171.311469	48.602548
1504.839510	157.270888	48.607553
1501.230490	154.197229	48.612557
1497.845469	175.789064	48.617562
1494.660059	183.291896	48.622567
1491.066265	167.442274	48.627572
1487.447049	162.120141	48.632577
1484.306802	160.891381	48.637581
1480.304017	174.566570	48.642586
1477.085723	173.429413	48.647591
1473.395484	157.877863	48.652596
1470.101596	169.220620	48.657601
1466.881488	172.556767	48.662605
1462.853215	192.188710	48.667610
1459.306317	162.200422	48.672615
1455.765939	158.182248	48.677620
1452.517060	166.218694	48.682625
1448.967156	182.793989	48.687629
1445.320842	173.288539	48.692634
1442.018991	158.194363	48.697639
1438.797104	162.171532	48.702644
1434.863659	164.723880	48.707649
1431.136338	159.832070	48.712653
1427.712916	178.336368	48.717658
1424.323104	165.734260	48.722663
1421.047618	174.621907	48.727668
1417.754426	161.251176	48.732673
1414.194713	144.232355	48.737677
1410.335541	159.249045	48.742682
1406.613550	158.079443	48.747687
1403.165905	171.581159	48.752692
1399.777090	166.543528	48.757697
1396.536134	160.005329	48.762701
1392.929998	172.278505	48.767706
1389.347760	178.630345	48.772711
1385.772601	166.961975	48.777716
1382.220870	152.975569	48.782721
1378.792612	153.022857	48.787725
1375.411945	158.305623	48.792730
1372.009900	150.857269	48.797735
1368.199054	171.510443	48.802740
1365.092080	177.423389	48.807745
1361.658273	165.293609	48.812749
1357.904766	157.331705	48.817754
1354.329494	156.845614	48.822759
1350.599564	157.160325	48.827764
1347.319129	142.441598	48.832769
1343.838552	156.561459	48.837773
1339.846010	176.272761	48.842778
1336.725144	151.930926	48.847783
1333.509347	165.720819	48.852788
1329.654901	162.370116	48.857793
1326.343011	166.853850	48.862797
1322.578557	175.477371	48.867802
1319.164744	156.577670	48.872807
1315.982954	154.067998	48.877812
1312.541147	164.181014	48.882817
1309.123129	170.203621	48.887821
1305.057989	174.402311	48.892826
1301.893103	157.198821	48.897831
1298.411137	166.798993	48.902836
1294.619169	157.762888	48.907841
1291.558630	150.750659	48.912845
1287.712659	149.686819	48.917850
1284.138823	159.609741	48.922855
1280.176536	179.087606	48.927860
1277.032944	164.711606	48.932865
1274.008127	137.971541	48.937869
1270.304878	159.271066	48.942874
1267.008740	152.092059	48.947879
1263.314687	157.023824	48.952884
1259.568965	165.172543	48.957889
1256.338735	159.108526	48.962893
1252.448937	157.334080	48.967898
1249.044099	156.387438	48.972903
1245.402478	168.153953	48.977908
1242.022516	163.893574	48.982913
1239.525818	162.655567	48.987917
1235.428907	160.151292	48.992922
1232.199522	169.874146	48.997927
1227.853487	159.739162	49.002932
1224.256370	155.864151	49.007937
1221.277651	169.662002	49.012941
1217.639941	155.620645	49.017946
1214.342531	143.810471	49.022951
1210.846879	144.020194	49.027956
1207.145805	156.051435	49.032961
1203.935138	166.084709	49.037965
1200.132319	174.774596	49.042970
1196.815654	157.746074	49.047975
1193.335998	155.784002	49.052980
1189.520824	166.979706	49.057985
1186.240244	169.687606	49.062989
1182.645993	158.729434	49.067994
1178.949614	138.010777	49.072999
1175.674637	159.612520	49.078004
1172.063377	167.838816	49.083009
1168.734642	149.239574	49.088013
1165.106709	153.687061	49.093018
1161.582803	154.697165	49.098023
1158.113383	180.063571	49.103028
1154.722338	161.843256	49.108033
1151.176326	143.057158	49.113037
1147.657810	163.400521	49.118042
1144.517132	164.889142	49.123047
1140.617400	159.218240	49.128052
1136.829809	149.622187	49.133057
1133.895217	140.964824	49.138061
1130.283858	153.040077	49.143066
1126.669108	168.597473	49.148071
1123.099887	166.625658	49.153076
1119.643310	159.368847	49.158081
1116.091315	158.268410	49.163085
1112.516413	156.712058	49.168090
1109.010935	145.043034	49.173095
1105.452472	150.611257	49.178100
1101.645573	170.370021	49.183105
1098.637236	152.940074	49.188109
1095.379634	147.563900	49.193114
1091.799411	155.026403	49.198119
1088.384117	154.512462	49.203124
1084.692699	149.435000	49.208129
1081.093685	149.706739	49.213133
1077.199304	162.550747	49.218138
1073.760237	155.750081	49.223143
1070.421572	174.931612	49.228148
1066.950829	167.166073	49.233153
1063.698857	142.097261	49.238157
1060.054358	148.963508	49.243162
1056.663463	145.664584	49.248167
1052.979690	142.699897	49.253172
1049.527040	146.112887	49.258177
1046.110655	151.061653	49.263181
1042.355065	167.614404	49.268186
1039.016408	160.212888	49.273191
1035.788419	163.760936	49.278196
1032.163214	155.436143	49.283201
1028.866683	142.482713	49.288205
1025.172765	141.636494	49.293210
1021.650629	150.935720	49.298215
1018.122310	166.817836	49.303220
1014.223945	165.958814	49.308225
1011.457829	146.106699	49.313229
1007.341463	161.008377	49.318234
1004.284756	141.906620	49.323239
1000.525205	150.391754	49.328244
996.753892	151.125540	49.333249
993.330707	154.919996	49.338253
989.610968	159.641184	49.343258
986.547028	164.011621	49.348263
983.145182	152.956017	49.353268
979.565134	139.676544	49.358273
976.488670	135.990941	49.363277
972.331874	146.270864	49.368282
968.704730	148.487602	49.373287
965.561652	154.984632	49.378292
961.787864	150.972229	49.383297
958.536043	141.476649	49.388301
954.837074	134.466142	49.393306
951.812986	141.503250	49.398311
948.175816	154.576711	49.403316
944.354528	136.248372	49.408321
941.059413	141.470241	49.413325
937.590396	147.482384	49.418330
934.114602	132.882799	49.423335
930.323399	135.895008	49.428340
926.621967	151.658346	49.433345
923.506103	144.546937	49.438349
919.919174	138.724308	49.443354
916.468220	138.868008	49.448359
912.901953	143.851248	49.453364
909.248499	152.320584	49.458369
906.012978	134.373007	49.463373
902.583520	127.239216	49.468378
898.846133	138.337249	49.473383
895.411814	148.251002	49.478388
891.709527	149.571448	49.483393
888.562926	128.667249	49.488397
885.054449	129.117786	49.493402
881.387666	140.366642	49.498407
878.126956	152.219749	49.503412
874.354850	136.155585	49.508417
871.132906	120.441646	49.513421
867.146458	146.141539	49.518426
863.965920	153.260846	49.523431
860.646877	144.714065	49.528436
856.939838	133.328173	49.533441
853.578915	140.141964	49.538445
849.899683	157.771529	49.543450
846.282223	157.174099	49.548455
842.591283	147.208535	49.553460
839.009885	153.490734	49.558465
835.955927	137.735349	49.563469
832.462990	136.614857	49.568474
828.894483	147.262731	49.573479
825.488956	148.355361	49.578484
821.775105	150.189043	49.583489
818.601516	138.402075	49.588493
814.691729	156.755914	49.593498
810.979470	146.259125	49.598503
808.015861	133.915845	49.603508
804.340226	142.732967	49.608513
800.827444	140.077466	49.613517
797.134157	146.836474	49.618522
793.627542	121.422269	49.623527
790.518591	128.284635	49.628532
786.614425	148.053822	49.633537
783.097662	143.951241	49.638541
779.900560	126.838678	49.643546
776.318592	124.062925	49.648551
772.772134	137.041854	49.653556
769.290177	132.588074	49.658561
766.065269	126.397190	49.663565
762.333527	148.594126	49.668570
759.087115	165.879398	49.673575
755.436791	140.313233	49.678580
751.572556	145.028805	49.683585
748.573285	133.572862	49.688589
744.576539	146.867266	49.693594
740.739109	140.999698	49.698599
737.473817	141.639210	49.703604
734.126708	141.909090	49.708609
730.994277	124.543309	49.713613
727.401200	139.323852	49.718618
723.656701	133.360258	49.723623
720.195285	127.012052	49.728628
716.882916	148.419127	49.733633
713.433651	138.615179	49.738637
709.744800	140.176966	49.743642
706.302116	129.113897	49.748647
702.804628	138.346047	49.753652
699.157287	143.404532	49.758657
695.682219	133.793079	49.763661
692.005196	125.057729	49.768666
689.006207	128.041526	49.773671
685.270284	139.353772	49.778676
681.505862	159.983812	49.783681
678.184022	126.967711	49.788685
674.510809	123.120490	49.793690
671.153998	128.869276	49.798695
667.951754	137.583317	49.803700
664.692624	146.666623	49.808705
661.160641	128.333151	49.813709
657.209476	116.636742	49.818714
653.606465	134.512613	49.823719
650.281704	127.411201	49.828724
646.377310	122.314837	49.833729
642.982004	132.243053	49.838733
639.397759	132.228585	49.843738
636.193620	128.676107	49.848743
632.580343	123.824454	49.853748
629.325366	144.288868	49.858753
625.880210	152.215109	49.863757
622.008572	148.316243	49.868762
618.658435	124.660656	49.873767
615.227316	132.791239	49.878772
611.530491	139.504061	49.883777
608.405078	131.856092	49.888781
604.733922	149.086362	49.893786
600.962184	140.663633	49.898791
597.700415	128.096278	49.903796
593.817232	147.453674	49.908801
590.747621	135.207537	49.913805
586.980998	134.718049	49.918810
583.531016	144.984612	49.923815
580.203975	136.171694	49.928820
576.567024	117.700069	49.933825
573.337088	124.241974	49.938829
569.649478	146.222055	49.943834
565.943623	140.700328	49.948839
562.458781	121.443411	49.953844
559.083945	127.198184	49.958849
555.950696	130.299309	49.963853
552.195456	125.246632	49.968858
548.390000	131.372129	49.973863
545.166328	150.042344	49.978868
541.707551	145.267121	49.983873
538.249975	126.445184	49.988877
534.729031	122.377772	49.993882
531.177698	143.965329	49.998887
527.655151	145.749125	50.003892
523.714179	135.253521	50.008897
520.588071	119.859063	50.013901
516.939985	132.340656	50.018906
513.642211	129.657497	50.023911
510.215604	139.071568	50.028916
506.416556	129.045576	50.033921
503.081015	119.355447	50.038925
499.561314	135.153258	50.043930
495.765415	127.437235	50.048935
492.600648	125.274774	50.053940
488.976495	138.417408	50.058945
485.529586	135.783658	50.063949
481.842618	138.813221	50.068954
478.468730	118.620602	50.073959
475.142664	129.020324	50.078964
471.202886	130.067224	50.083969
468.363569	115.939823	50.088973
464.637250	126.317770	50.093978
461.374542	127.095096	50.098983
457.802783	131.005988	50.103988
454.307858	120.107974	50.108993
450.672343	124.791939	50.113997
447.085414	150.744139	50.119002
442.930965	145.709034	50.124007
439.590747	126.246974	50.129012
435.970695	130.063360	50.134017
433.286183	123.967273	50.139021
429.614575	119.186048	50.144026
426.078289	139.656340	50.149031
422.435114	128.361412	50.154036
418.956120	132.832702	50.159041
415.527696	116.325039	50.164045
411.835073	117.714091	50.169050
408.031155	135.491942	50.174055
405.052960	137.164372	50.179060
401.431144	143.637232	50.184065
397.953672	121.800692	50.189069
394.468444	132.948145	50.194074
390.829373	137.899669	50.199079
387.194689	127.997537	50.204084
383.704458	120.174103	50.209089
380.277790	114.559525	50.214093
376.980672	136.621440	50.219098
373.651778	147.239395	50.224103
370.371117	128.716056	50.229108
366.467317	125.777375	50.234113
362.828921	113.166258	50.239117
359.324587	126.023955	50.244122
355.729621	123.517136	50.249127
352.336190	128.390413	50.254132
348.732335	129.335230	50.259137
345.550623	126.560286	50.264141
341.963841	137.849428	50.269146
337.978363	108.628739	50.274151
334.855902	123.886065	50.279156
331.114911	133.847846	50.284161
327.949663	132.540321	50.289165
324.335122	148.215354	50.294170
320.846896	163.292477	50.299175
317.701119	128.291804	50.304180
313.809495	127.281559	50.309185
310.345497	130.128773	50.314189
307.056998	135.566161	50.319194
303.198890	139.962334	50.324199
299.801940	116.719192	50.329204
296.185155	120.222499	50.334209
293.073189	118.813561	50.339213
289.370478	135.973291	50.344218
285.666999	140.823251	50.349223
282.514344	140.423287	50.354228
278.799254	141.340650	50.359233
275.157069	122.913419	50.364237
271.644268	116.138453	50.369242
268.666454	126.429522	50.374247
265.017451	124.418307	50.379252
261.260753	116.360301	50.384257
257.721652	122.685103	50.389261
254.266678	133.731831	50.394266
250.811306	138.451837	50.399271
247.704570	121.259999	50.404276
243.604160	126.430756	50.409281
239.871548	115.852019	50.414285
236.724590	132.727287	50.419290
233.253480	128.737345	50.424295
229.951610	110.002191	50.429300
226.082918	135.157036	50.434305
222.987142	127.304533	50.439309
219.722958	124.191903	50.444314
215.864784	131.044726	50.449319
212.622214	130.240210	50.454324
208.473102	138.226714	50.459329
205.060020	117.205561	50.464333
201.529405	123.151272	50.469338
198.474910	132.235868	50.474343
194.962513	104.071492	50.479348
190.824771	122.658921	50.484353
187.585318	140.232721	50.489357
184.309240	137.951098	50.494362
180.866000	110.938238	50.499367
177.360960	109.901196	50.504372
173.513002	115.516999	50.509377
169.971399	106.180972	50.514381
166.507684	109.674738	50.519386
163.281973	119.913777	50.524391
159.811610	129.212606	50.529396
155.990513	120.939508	50.534401
152.743931	106.533745	50.539405
149.296759	115.857445	50.544410
145.918054	127.654641	50.549415
142.504904	116.319837	50.554420
138.713430	123.517493	50.559425
135.248741	115.712687	50.564429
131.612424	120.393693	50.569434
128.044636	132.247495	50.574439
124.591372	121.204514	50.579444
121.290527	103.012128	50.584449
117.917412	113.256007	50.589453
114.087571	129.251276	50.594458
110.408280	132.311929	50.599463
107.186959	113.230421	50.604468
103.587473	130.117372	50.609473
100.274823	129.477198	50.614477
96.373654	113.888352	50.619482
93.100141	118.060486	50.624487
89.564134	105.674235	50.629492
86.006215	118.931236	50.634497
82.899600	119.084767	50.639501
79.209824	117.975123	50.644506
75.495716	133.089317	50.649511
72.520974	117.731623	50.654516
68.526968	110.569413	50.659521
65.005646	110.892201	50.664525
61.704914	110.270500	50.669530
58.036367	120.181270	50.674535
54.394142	126.106138	50.679540
50.882256	125.356075	50.684545
47.801899	97.561984	50.689549
44.143209	106.410481	50.694554
40.311741	124.842014	50.699559
37.181595	135.731085	50.704564
33.884249	118.984615	50.709569
30.119987	103.328719	50.714573
26.870625	121.079677	50.719578
23.211839	117.985708	50.724583
19.730314	112.136856	50.729588
16.290213	126.345593	50.734593
12.775567	116.608848	50.739597
8.808858	110.787209	50.744602
5.053444	116.105881	50.749607
2.343058	99.973793	50.754612