Wed Jun 15 16:55:34 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.994092	90.720307	0.000000
0.791175	104.951417	0.005005
0.931209	118.820556	0.010010
0.804061	93.295781	0.015014
0.509579	79.560264	0.020019
0.163156	73.630320	0.025024
0.036693	65.910991	0.030029
-0.369048	43.514039	0.035034
-0.693569	31.545836	0.040038
-0.992803	21.823276	0.045043
-1.122508	14.546245	0.050048
-1.704475	26.360957	0.055053
-1.808360	21.478423	0.060058
-2.125862	-4.632646	0.065062
-2.378794	9.059749	0.070067
-2.396161	-4.920060	0.075072
-3.119753	-21.215152	0.080077
-3.625858	-20.545533	0.085082
-3.559691	-14.515493	0.090086
-3.903840	-16.853110	0.095091
-4.339594	-32.398504	0.100096
-4.827462	-18.161653	0.105101
-5.060971	-10.579325	0.110106
-5.148370	-32.773280	0.115110
-5.551363	-25.782246	0.120115
-5.096771	-13.032060	0.125120
-5.274370	-18.629811	0.130125
-6.177928	-35.261121	0.135130
-6.441324	-17.840004	0.140134
-6.897796	-18.589709	0.145139
-6.715014	-28.945491	0.150144
-6.888922	-7.561278	0.155149
-6.763049	-17.591799	0.160154
-7.711440	-30.787283	0.165158
-8.406816	-22.099961	0.170163
-8.514302	-10.343366	0.175168
-8.549898	-13.307472	0.180173
-8.823243	-34.454351	0.185178
-8.668635	-23.519588	0.190182
-8.785214	-8.523850	0.195187
-8.456995	-11.877949	0.200192
-9.281027	-26.673696	0.205197
-9.814238	-22.587652	0.210202
-9.707045	-18.687932	0.215206
-10.121589	-20.364533	0.220211
-10.749640	-23.298696	0.225216
-11.363244	-8.523564	0.230221
-11.323710	-9.085639	0.235226
-11.168172	-21.917658	0.240230
-11.780346	-20.482088	0.245235
-11.476550	-22.924118	0.250240
-11.557669	-30.358998	0.255245
-12.186341	-26.278191	0.260250
-12.591971	-10.157677	0.265254
-12.883565	-10.348676	0.270259
-13.016294	-31.868789	0.275264
-13.166883	-33.035313	0.280269
-13.566137	-15.395932	0.285274
-14.053135	-5.949335	0.290278
-14.732303	-10.284203	0.295283
-14.196774	-11.632771	0.300288
-14.742310	-17.268560	0.305293
-14.856491	-31.445714	0.310298
-14.836574	-35.176683	0.315302
-15.286760	-13.166789	0.320307
-15.221082	0.941511	0.325312
-15.553252	-3.862646	0.330317
-16.459795	-21.314599	0.335322
-16.402044	-17.550239	0.340326
-16.741880	-24.146397	0.345331
-16.749224	-11.160561	0.350336
-16.718768	-10.423555	0.355341
-17.222157	-9.976927	0.360346
-17.661864	-10.219110	0.365350
-18.019822	-24.479882	0.370355
-17.986592	-23.157282	0.375360
-18.151633	-18.065822	0.380365
-18.136086	-14.537746	0.385370
-18.743071	-19.009523	0.390374
-19.651933	-3.865193	0.395379
-19.594325	-4.354891	0.400384
-19.787514	-19.197284	0.405389
-19.929291	-26.361225	0.410394
-19.572518	-17.451419	0.415398
-20.002855	-4.422506	0.420403
-20.330200	-22.590260	0.425408
-20.720448	-26.233028	0.430413
-21.224302	-9.098386	0.435418
-20.810911	-27.862932	0.440422
-21.729899	-18.432649	0.445427
-22.078257	-27.747641	0.450432
-22.506454	-13.480598	0.455437
-22.718259	-18.950473	0.460442
-22.964984	-4.079910	0.465446
-23.057488	-4.153573	0.470451
-23.132071	-13.818927	0.475456
-23.055368	-4.286741	0.480461
-23.123908	-24.385138	0.485466
-23.112223	-24.585121	0.490470
-24.198089	-14.539626	0.495475
-24.351048	-24.233256	0.500480
-24.547648	-19.529979	0.505485
-24.611425	-19.384365	0.510490
-24.810842	-25.738667	0.515494
-25.875027	-7.016650	0.520499
-26.026445	-31.494910	0.525504
-26.560238	-12.079380	0.530509
-26.667355	-7.889934	0.535514
-26.393427	-25.145243	0.540518
-26.599289	-27.158774	0.545523
-26.413368	-11.969281	0.550528
-26.350876	-12.517197	0.555533
-27.100967	-20.113591	0.560538
-27.354829	-15.493872	0.565542
-27.903262	-9.331387	0.570547
-27.773517	-5.454629	0.575552
-27.924066	-12.727114	0.580557
-29.017030	-31.471572	0.585562
-29.095309	-16.376032	0.590566
-29.477828	-18.926792	0.595571
-29.232384	-25.600041	0.600576
-29.256007	-6.467585	0.605581
-29.566473	-8.992769	0.610586
-30.145439	-15.944682	0.615590
-30.837585	-5.306481	0.620595
-31.161332	-18.356611	0.625600
-31.014068	-37.516037	0.630605
-31.248193	-12.663382	0.635610
-31.105792	-6.892356	0.640614
-31.696463	-1.850010	0.645619
-31.620245	-19.047694	0.650624
-31.374935	-31.589132	0.655629
-32.506247	-19.654570	0.660634
-32.618949	-22.323114	0.665638
-33.050435	-24.744052	0.670643
-33.223236	-19.048489	0.675648
-33.038990	-8.675076	0.680653
-33.674251	-26.417674	0.685658
-34.172822	-30.958559	0.690662
-34.664842	-15.409532	0.695667
-34.572439	-14.348652	0.700672
-34.362375	-14.679768	0.705677
-34.735035	-14.591519	0.710682
-34.413013	-24.914774	0.715686
-34.825602	-21.479302	0.720691
-35.414596	-10.973665	0.725696
-35.682639	-17.415668	0.730701
-35.784494	-33.961947	0.735706
-36.663995	-17.189016	0.740710
-37.356558	-6.835831	0.745715
-37.430455	-12.740540	0.750720
-37.071593	-20.783088	0.755725
-37.551320	-28.955855	0.760730
-37.238125	-18.568740	0.765734
-37.472721	-24.918805	0.770739
-37.521221	-18.857390	0.775744
-38.372600	-16.584344	0.780749
-39.056312	-1.752737	0.785754
-39.107796	-22.778654	0.790758
-39.039014	-25.203646	0.795763
-39.260017	-27.559933	0.800768
-39.185380	-27.361237	0.805773
-39.713511	-22.528497	0.810778
-40.354354	-11.979865	0.815782
-40.629119	-24.507075	0.820787
-40.841380	-18.395612	0.825792
-40.641693	-27.918659	0.830797
-40.943227	-17.765051	0.835802
-41.034519	-4.015832	0.840806
-41.905485	-4.923426	0.845811
-42.234073	-18.266717	0.850816
-42.202704	-20.517041	0.855821
-42.218561	-9.319424	0.860826
-42.009861	1.021741	0.865830
-43.256100	-15.219130	0.870835
-43.725869	-27.596821	0.875840
-43.923018	-14.686260	0.880845
-43.999004	-15.186235	0.885850
-43.774986	-8.581533	0.890854
-44.186290	-22.383760	0.895859
-44.299980	-25.138356	0.900864
-44.335992	-14.690767	0.905869
-44.261912	-5.032279	0.910874
-44.841788	-24.575331	0.915878
-45.453259	-21.466553	0.920883
-45.600594	-13.470151	0.925888
-45.869800	-19.402358	0.930893
-45.960639	-17.191176	0.935898
-46.395555	-13.723898	0.940902
-47.163242	-13.040147	0.945907
-47.351688	-27.994582	0.950912
-47.417157	-15.694006	0.955917
-47.566847	5.448874	0.960922
-47.455194	-15.963475	0.965926
-47.437588	-17.793762	0.970931
-47.526064	-36.720585	0.975936
-48.248629	-8.618722	0.980941
-48.847557	-14.598241	0.985946
-48.556956	-20.453786	0.990950
-48.867226	-25.456771	0.995955
-49.440389	-24.497986	1.000960
-49.825055	-6.487638	1.005965
-50.384364	-8.636104	1.010970
-50.269505	-33.951368	1.015974
-50.343348	-22.371103	1.020979
-50.560557	-17.044631	1.025984
-50.434409	-2.318061	1.030989
-51.508319	-21.932567	1.035994
-51.519922	-20.371926	1.040998
-52.129809	-4.622002	1.046003
-52.123341	1.163795	1.051008
-52.056385	-13.825069	1.056013
-52.002725	-31.017035	1.061018
-51.885528	-33.377522	1.066022
-53.060399	-15.893965	1.071027
-53.459073	-16.232693	1.076032
-53.481831	-15.329160	1.081037
-53.500991	-8.384782	1.086042
-53.385105	-25.999671	1.091046
-54.362629	-16.041132	1.096051
-55.116405	-24.248215	1.101056
-55.090427	-23.441516	1.106061
-54.949908	-28.579173	1.111066
-54.961903	-18.123521	1.116070
-55.457017	-7.054349	1.121075
-55.551992	-22.193413	1.126080
-55.342105	-33.149879	1.131085
-55.968461	-22.115256	1.136090
-56.471348	-6.606843	1.141094
-56.947561	-17.465913	1.146099
-57.048164	-41.951559	1.151104
-57.170293	-34.782134	1.156109
-57.150092	-16.283039	1.161114
-57.233027	-19.973043	1.166118
-58.193980	-19.765669	1.171123
-58.396645	-27.522561	1.176128
-58.562323	-15.978706	1.181133
-58.672717	-4.240671	1.186138
-58.819963	-20.625176	1.191142
-58.830139	-21.864621	1.196147
-59.619116	-23.314007	1.201152
-59.899672	-12.651105	1.206157
-60.501409	-11.119892	1.211162
-60.122758	-33.895326	1.216166
-60.305692	-23.338332	1.221171
-60.176837	-3.468155	1.226176
-60.549481	-11.936015	1.231181
-61.685440	-12.458499	1.236186
-61.283853	-21.784677	1.241190
-61.443350	-18.326122	1.246195
-61.823872	-19.002750	1.251200
-61.719316	-15.947988	1.256205
-62.683626	-24.022616	1.261210
-62.905627	-38.545740	1.266214
-63.562374	-23.879503	1.271219
-63.367068	-6.373397	1.276224
-63.502172	-16.886860	1.281229
-63.656534	-33.974995	1.286234
-63.398535	-27.182870	1.291238
-63.695691	-14.343774	1.296243
-64.359334	-20.189386	1.301248
-64.696031	-12.878546	1.306253
-65.173229	4.287214	1.311258
-65.016823	-22.061734	1.316262
-65.301497	-32.919301	1.321267
-65.997905	-26.458824	1.326272
-66.317098	-4.166549	1.331277
-67.044076	-12.352416	1.336282
-66.538031	-33.446383	1.341286
-66.615206	-15.210658	1.346291
-66.654772	-1.286410	1.351296
-66.705272	0.792138	1.356301
-67.124843	-9.972521	1.361306
-67.416542	-7.626538	1.366310
-67.877275	-6.778465	1.371315
-68.100562	-13.276397	1.376320
-68.043822	-15.988233	1.381325
-69.149145	-29.333156	1.386330
-69.545810	-26.274576	1.391334
-69.661228	-18.724102	1.396339
-69.982528	-21.958131	1.401344
-69.189305	-12.766324	1.406349
-69.733269	-17.636876	1.411354
-69.726703	-29.877544	1.416358
-70.138785	-8.245052	1.421363
-70.835681	-12.508620	1.426368
-71.191077	-19.621175	1.431373
-71.548274	-17.938510	1.436378
-71.453347	-27.435955	1.441382
-71.678768	-12.500370	1.446387
-71.486685	-23.004372	1.451392
-72.111998	-42.827533	1.456397
-73.099151	-28.649343	1.461402
-73.305291	-5.257611	1.466406
-73.137016	-15.762517	1.471411
-73.017619	-26.905564	1.476416
-73.242556	-23.233282	1.481421
-73.497517	-14.927500	1.486426
-73.286641	-13.051168	1.491430
-74.146041	-25.164506	1.496435
-74.716979	-36.703945	1.501440
-74.675781	-13.315814	1.506445
-74.996765	-2.011245	1.511450
-74.550325	-26.356389	1.516454
-75.449627	-30.989466	1.521459
-75.982591	-28.238032	1.526464
-76.190322	-7.537281	1.531469
-76.675919	-7.283087	1.536474
-76.175908	-13.211123	1.541478
-76.444539	-18.660553	1.546483
-76.625526	-23.478437	1.551488
-77.533268	-23.605582	1.556493
-78.031224	-12.281341	1.561498
-77.852916	-17.565914	1.566502
-78.151483	-3.829793	1.571507
-78.297822	-12.303287	1.576512
-77.765878	-30.233245	1.581517
-78.414965	-15.594309	1.586522
-78.991652	-27.337690	1.591526
-79.993171	-28.998855	1.596531
-79.828487	-28.326748	1.601536
-79.636950	-12.801813	1.606541
-79.880582	0.057744	1.611546
-79.908571	-20.155265	1.616550
-80.246682	-31.402329	1.621555
-80.740225	-10.792155	1.626560
-80.864545	-10.490835	1.631565
-81.286401	-14.228403	1.636570
-81.443427	-24.061528	1.641574
-81.653823	-20.380009	1.646579
-81.933899	-18.051040	1.651584
-82.396639	-17.931230	1.656589
-83.122058	-22.309144	1.661594
-83.518546	-23.937130	1.666598
-83.088906	-15.199181	1.671603
-82.719694	-2.042086	1.676608
-82.943044	-10.649341	1.681613
-83.630160	-5.390806	1.686618
-83.641023	-21.227083	1.691622
-84.597028	-7.540935	1.696627
-84.836635	-6.833477	1.701632
-84.843068	-14.698563	1.706637
-85.018776	-22.393818	1.711642
-84.712089	-17.604246	1.716646
-85.139265	-10.712491	1.721651
-85.495993	-25.017645	1.726656
-85.934171	-19.965684	1.731661
-86.448880	-11.946547	1.736666
-86.442297	-16.871488	1.741670
-86.382264	-13.727196	1.746675
-87.353886	-8.593482	1.751680
-87.596529	-10.620959	1.756685
-88.020082	-5.058651	1.761690
-87.941822	-20.277046	1.766694
-88.051798	-18.720271	1.771699
-87.979654	-12.542664	1.776704
-88.316488	-22.508246	1.781709
-88.195943	-21.361561	1.786714
-88.763821	-23.100804	1.791718
-89.310444	-2.144184	1.796723
-89.567358	-1.376060	1.801728
-89.589760	-17.920976	1.806733
-89.871152	-17.727855	1.811738
-90.354015	-28.579004	1.816742
-90.942124	-10.824568	1.821747
-91.271699	-11.353360	1.826752
-91.093207	-5.766556	1.831757
-91.296764	-15.302175	1.836762
-90.969093	-32.429527	1.841766
-91.324505	-12.322785	1.846771
-92.024256	-10.530236	1.851776
-92.142621	-24.983292	1.856781
-92.746065	-4.732759	1.861786
-92.523872	-11.102485	1.866790
-93.080627	-29.673538	1.871795
-93.072805	-18.600885	1.876800
-93.672986	-17.650947	1.881805
-94.414400	-1.869224	1.886810
-94.363174	-25.602849	1.891814
-94.434411	-19.219451	1.896819
-94.503974	-8.670829	1.901824
-94.491391	-19.814277	1.906829
-94.634511	-13.993309	1.911834
-94.836017	-27.267325	1.916838
-95.569154	-12.847200	1.921843
-96.080593	8.452724	1.926848
-96.190595	-18.986318	1.931853
-96.087167	-16.489309	1.936858
-96.172365	-23.423379	1.941862
-96.410736	-7.967369	1.946867
-97.243336	0.455786	1.951872
-97.488396	-9.378087	1.956877
-97.770142	3.180391	1.961882
-97.723243	-6.977055	1.966886
-97.741688	-17.386387	1.971891
-97.931684	-27.667235	1.976896
-98.611132	-5.528798	1.981901
-99.242631	10.348608	1.986906
-99.333236	-15.518573	1.991910
-99.238487	-11.364663	1.996915
-99.472612	-21.555853	2.006912
-99.397250	-16.020053	2.016909
-98.517656	-23.285416	2.026906
-98.029204	-14.408194	2.036902
-98.013378	-11.978797	2.046899
-97.304419	-20.827024	2.056896
-97.029867	-15.096278	2.066893
-96.307526	-5.864397	2.076890
-95.459388	-24.885695	2.086886
-95.036045	-2.033671	2.096883
-94.986552	-19.615443	2.106880
-94.176574	-8.931882	2.116877
-93.633563	-23.898648	2.126874
-93.512279	-3.248300	2.136870
-92.504915	-16.464343	2.146867
-92.104264	-17.382802	2.156864
-91.932250	-19.264228	2.166861
-90.987691	-0.585312	2.176858
-90.688730	-25.109685	2.186854
-90.679995	-8.099932	2.196851
-89.409314	-16.300111	2.206848
-89.185578	-7.699252	2.216845
-89.104170	-8.119786	2.226842
-88.302502	-12.285462	2.236838
-87.717891	-19.626527	2.246835
-87.092203	-25.601947	2.256832
-86.326971	-11.941324	2.266829
-86.140670	-11.171512	2.276826
-86.044843	-17.457217	2.286822
-85.249473	-4.389358	2.296819
-84.902716	-14.707800	2.306816
-84.317481	-22.975938	2.316813
-83.430822	-10.464835	2.326810
-82.933115	-20.018344	2.336806
-82.925996	-2.477122	2.346803
-81.895667	-28.978974	2.356800
-81.281827	-9.301844	2.366797
-81.456779	-24.629491	2.376794
-81.227788	-13.107938	2.386790
-80.095132	-28.123456	2.396787
-79.776196	-17.367435	2.406784
-78.738290	-9.298095	2.416781
-78.479198	-12.377691	2.426778
-78.106659	-26.900947	2.436774
-77.908960	-21.015960	2.446771
-77.520884	-17.210365	2.456768
-76.866491	-9.732203	2.466765
-75.866370	-34.197222	2.476762
-75.520401	-23.477180	2.486758
-74.909889	-16.938593	2.496755
-75.073543	-29.898966	2.506752
-74.114201	-21.965694	2.516749
-73.492193	-5.670364	2.526746
-73.254426	-33.957494	2.536742
-72.919977	-21.116305	2.546739
-72.095049	-13.744752	2.556736
-71.903485	-16.451682	2.566733
-70.798341	-19.731155	2.576730
-70.497778	-14.031669	2.586726
-70.495741	-26.183820	2.596723
-69.523842	-17.419976	2.606720
-68.716131	-17.816929	2.616717
-68.743030	-22.882571	2.626714
-68.733804	-11.727486	2.636710
-67.520102	-23.798289	2.646707
-67.286151	-13.050836	2.656704
-66.790483	-12.731288	2.666701
-65.899006	-19.525005	2.676698
-65.683509	-0.950100	2.686694
-64.978853	-19.055588	2.696691
-64.082635	-29.182243	2.706688
-63.819893	-23.693116	2.716685
-63.972632	-4.305212	2.726682
-63.702611	-13.679359	2.736678
-62.708127	-9.030907	2.746675
-62.273127	-17.135643	2.756672
-61.353730	-1.629253	2.766669
-61.032228	-25.711501	2.776666
-61.182808	0.950781	2.786662
-59.891351	-10.901263	2.796659
-59.591455	-19.822932	2.806656
-59.342414	-12.743782	2.816653
-58.340292	-8.759349	2.826650
-57.735057	-21.619725	2.836646
-57.661792	-11.916597	2.846643
-57.567807	-21.780396	2.856640
-56.640450	-9.345644	2.866637
-56.241840	-19.827528	2.876634
-55.355594	-17.653493	2.886630
-54.723962	-12.635523	2.896627
-54.595573	-14.530383	2.906624
-54.523623	-27.445940	2.916621
-53.481441	3.150250	2.926618
-52.982317	-14.810653	2.936614
-52.797387	-15.425491	2.946611
-52.029203	-4.398099	2.956608
-51.253010	-10.615595	2.966605
-50.949043	-16.732922	2.976602
-50.639499	-20.749505	2.986598
-50.505297	-25.374186	2.996595
-49.812629	-5.400617	3.006592
-49.050432	-8.298848	3.016589
-48.036325	-1.602243	3.026586
-48.081507	-17.972353	3.036582
-48.050634	-8.603273	3.046579
-47.076694	-17.439586	3.056576
-46.693985	-3.156977	3.066573
-46.342839	-11.057130	3.076570
-45.342540	-12.186199	3.086566
-44.884468	-11.066213	3.096563
-44.866111	-25.889876	3.106560
-43.940357	-9.959625	3.116557
-43.406570	-20.620402	3.126554
-43.398736	-29.088243	3.136550
-42.655371	-6.286529	3.146547
-41.799516	-16.456104	3.156544
-41.720496	-13.544180	3.166541
-41.238751	-11.834982	3.176538
-40.354927	-25.050453	3.186534
-40.008587	-10.625139	3.196531
-39.860893	-11.381783	3.206528
-38.854403	-25.988873	3.216525
-38.702368	-3.272451	3.226522
-38.424762	-22.162233	3.236518
-37.551078	-10.721632	3.246515
-37.124519	-25.121270	3.256512
-36.492649	-15.564880	3.266509
-35.995526	-19.550138	3.276506
-35.947467	-27.266260	3.286502
-34.759057	-13.768800	3.296499
-34.206015	-20.950958	3.306496
-34.181133	-14.010772	3.316493
-33.990957	-9.114225	3.326490
-32.715651	-26.552878	3.336486
-32.474326	-12.196634	3.346483
-32.535413	-20.140269	3.356480
-31.343059	-18.336345	3.366477
-31.068587	-19.032058	3.376474
-30.595880	-9.338538	3.386470
-29.572616	-30.094663	3.396467
-29.140740	-17.352431	3.406464
-29.314139	-21.054028	3.416461
-29.030454	-10.127614	3.426458
-27.895042	-8.011147	3.436454
-27.703133	-14.042100	3.446451
-26.967262	-21.019791	3.456448
-26.040111	-10.571788	3.466445
-26.118452	-12.839029	3.476442
-26.043247	-10.208664	3.486438
-25.033795	-13.513603	3.496435
-24.455163	-7.627851	3.506432
-24.032902	-15.147039	3.516429
-22.977548	-9.011554	3.526426
-22.874253	-23.363304	3.536422
-22.720724	-4.804821	3.546419
-22.392760	-19.708896	3.556416
-21.458727	-15.493734	3.566413
-21.252067	-4.859889	3.576410
-20.458677	-11.660608	3.586406
-19.678181	-25.137737	3.596403
-19.398571	-6.414796	3.606400
-19.174026	-20.956671	3.616397
-18.649580	-3.917352	3.626394
-17.980537	-25.640394	3.636390
-17.558326	-13.556355	3.646387
-16.890097	-21.887989	3.656384
-16.183308	-17.342810	3.666381
-16.144311	-9.083585	3.676378
-15.901659	-23.236919	3.686374
-14.803138	-15.927360	3.696371
-14.646626	-33.528990	3.706368
-14.007007	-27.912203	3.716365
-12.917560	-37.847658	3.726362
-12.671201	-13.808577	3.736358
-12.469855	-19.085189	3.746355
-12.613643	-21.635656	3.756352
-11.888429	-17.483471	3.766349
-11.193065	-13.820804	3.776346
-10.409744	-24.159732	3.786342
-9.744451	-20.647366	3.796339
-9.663719	-28.298169	3.806336
-9.022006	-20.070202	3.816333
-8.464464	-19.235804	3.826330
-8.185109	-33.668792	3.836326
-6.965923	-16.302292	3.846323
-6.787176	-36.569887	3.856320
-6.855772	-25.797129	3.866317
-6.306186	-24.408196	3.876314
-5.208164	-25.519628	3.886310
-5.103257	-26.630211	3.896307
-4.730059	-18.891829	3.906304
-3.968105	-23.350605	3.916301
-3.898091	-4.847160	3.926298
-3.266749	-0.376129	3.936294
-2.787931	7.853686	3.946291
-2.282356	33.418702	3.956288
-1.887538	48.378426	3.966285
-1.406232	46.769360	3.976282
-1.251474	80.444236	3.986278
-0.606394	94.173331	3.996275
-0.148407	120.227182	4.006272
0.000000	153.693994	4.011277
0.527690	153.115263	4.016282
0.412329	149.331534	4.021286
0.793460	165.152643	4.026291
0.491257	184.193570	4.031296
0.735633	201.239647	4.036301
1.187471	189.766446	4.041306
0.998909	199.491678	4.046310
1.315167	200.558295	4.051315
1.475380	197.265948	4.056320
1.331444	223.363710	4.061325
1.541216	198.633123	4.066330
1.427903	200.049406	4.071334
1.497140	203.027287	4.076339
1.487816	234.661967	4.081344
1.187672	226.630039	4.086349
1.558699	194.531899	4.091354
1.437307	209.465710	4.096358
1.475524	215.374488	4.101363
1.308664	218.083018	4.106368
1.262336	203.911891	4.111373
1.667044	196.148418	4.116378
1.519029	208.307847	4.121382
1.419051	202.932065	4.126387
1.666574	216.488180	4.131392
1.572352	223.787080	4.136397
1.662142	209.037381	4.141402
1.180850	216.479259	4.146406
1.406527	222.259499	4.151411
1.533900	212.839301	4.156416
1.556934	200.556358	4.161421
1.593738	215.631141	4.166426
1.475610	226.895850	4.171430
1.661982	213.030439	4.176435
1.970450	197.160583	4.181440
1.328461	213.996222	4.186445
1.820540	218.200351	4.191450
1.640682	211.542532	4.196454
1.875775	213.915232	4.201459
1.639809	224.885421	4.206464
1.685285	213.408749	4.211469
1.425935	214.143151	4.216474
1.210259	209.064178	4.221478
1.276267	215.977126	4.226483
1.379503	220.453955	4.231488
1.393633	215.912114	4.236493
1.732162	216.447686	4.241498
1.734560	230.960062	4.246502
1.893201	245.699858	4.251507
1.980559	246.451445	4.256512
1.912398	243.962034	4.261517
1.764382	223.548734	4.266522
1.569662	217.375161	4.271526
1.724229	224.872856	4.276531
1.788304	233.117767	4.281536
1.832919	240.829752	4.286541
1.896537	242.421887	4.291546
1.490886	247.347519	4.296550
1.915697	266.928257	4.301555
1.701287	256.096051	4.306560
1.529190	254.924872	4.311565
2.006201	226.711533	4.316570
1.986176	254.440616	4.321574
1.917127	254.575660	4.326579
2.260689	238.863124	4.331584
1.803424	250.136051	4.336589
2.003286	256.709352	4.341594
2.230479	254.764888	4.346598
2.194129	249.745936	4.351603
2.064724	235.942652	4.356608
1.647904	248.528692	4.361613
2.193350	260.334345	4.366618
2.044038	267.751178	4.371622
2.180751	238.432088	4.376627
2.002692	233.199412	4.381632
1.969126	254.938718	4.386637
1.927040	258.291517	4.391642
1.901149	261.375689	4.396646
2.073446	244.246860	4.401651
2.337357	245.748780	4.406656
1.918761	256.234825	4.411661
2.232369	275.051383	4.416666
2.305836	287.907914	4.421670
2.471562	272.112471	4.426675
2.241813	255.141319	4.431680
2.328448	253.156258	4.436685
2.541282	255.403810	4.441690
1.932059	272.091158	4.446694
1.900064	270.053291	4.451699
1.897857	265.675819	4.456704
2.036164	261.724662	4.461709
2.356511	279.910545	4.466714
2.266964	300.564971	4.471718
2.334515	297.475838	4.476723
2.385778	290.642967	4.481728
2.313776	281.838780	4.486733
2.334549	283.840087	4.491738
2.063612	285.202719	4.496742
2.386998	286.010498	4.501747
2.798469	279.181733	4.506752
2.503158	293.842409	4.511757
2.636222	304.543129	4.516762
2.048359	293.976418	4.521766
2.338710	277.134245	4.526771
2.286107	278.856766	4.531776
2.373144	285.523697	4.536781
2.477629	290.982769	4.541786
2.358314	284.245860	4.546790
2.755046	270.688631	4.551795
2.876214	289.193617	4.556800
2.425038	300.180582	4.561805
2.577101	278.260990	4.566810
2.554679	266.508633	4.571814
2.664719	275.688151	4.576819
2.545417	293.521535	4.581824
2.651312	271.935612	4.586829
2.523846	283.297199	4.591834
2.491987	303.088795	4.596838
2.952011	285.606860	4.601843
2.781126	273.017446	4.606848
2.667768	299.408298	4.611853
2.750220	290.030299	4.616858
2.408650	292.706256	4.621862
2.469077	292.428471	4.626867
2.719765	275.964262	4.631872
2.658658	285.460513	4.636877
2.665112	279.138055	4.641882
2.553994	299.261671	4.646886
2.934761	302.548744	4.651891
3.154312	286.636373	4.656896
2.856153	297.627348	4.661901
2.952794	303.476392	4.666906
2.674070	285.341170	4.671910
2.794499	285.484460	4.676915
2.489135	300.048747	4.681920
2.811818	310.225787	4.686925
3.054406	315.934116	4.691930
2.834176	313.919261	4.696934
2.943100	315.527198	4.701939
3.204225	305.925031	4.706944
3.104686	310.738836	4.711949
3.249972	319.528422	4.716954
2.626897	323.986708	4.721958
2.725814	309.781418	4.726963
2.925486	305.784892	4.731968
2.641284	311.278906	4.736973
3.084636	310.756132	4.741978
2.742333	315.499275	4.746982
2.458863	321.161957	4.751987
3.010046	337.693027	4.756992
2.844658	324.756310	4.761997
3.248402	297.383490	4.767002
3.156861	309.878637	4.772006
2.937510	318.985852	4.777011
2.844613	307.350465	4.782016
2.798226	311.470675	4.787021
3.064761	318.579986	4.792026
2.705619	329.995973	4.797030
3.179081	336.546390	4.802035
3.434638	338.254394	4.807040
3.388507	330.169484	4.812045
3.407993	338.591889	4.817050
3.209572	330.356849	4.822054
3.262826	317.315347	4.827059
3.377930	306.686714	4.832064
3.193305	297.348604	4.837069
3.010467	306.062192	4.842074
3.069850	319.500631	4.847078
3.296380	341.237127	4.852083
3.688986	326.269967	4.857088
3.196799	326.577334	4.862093
3.430898	339.720273	4.867098
3.275310	344.828443	4.872102
3.362970	344.805206	4.877107
3.606212	336.110673	4.882112
3.203383	324.299996	4.887117
3.290251	316.532758	4.892122
3.444028	340.879753	4.897126
3.483999	343.812188	4.902131
3.736929	317.883894	4.907136
2.930320	322.585194	4.912141
3.397826	335.285596	4.917146
3.310965	345.161988	4.922150
3.360124	342.156284	4.927155
3.896469	351.473841	4.932160
3.660411	364.496511	4.937165
3.655675	330.098455	4.942170
3.328690	348.038532	4.947174
3.662791	349.860912	4.952179
3.433942	338.866686	4.957184
3.577878	340.761035	4.962189
3.792471	351.204063	4.967194
3.802637	362.888134	4.972198
3.586951	341.531934	4.977203
3.359495	332.579491	4.982208
3.130911	335.875824	4.987213
3.393103	332.321160	4.992218
3.633395	348.217425	4.997222
3.602694	349.966620	5.002227
3.723072	369.989234	5.007232
3.452776	364.948533	5.012237
3.351256	339.871708	5.017242
3.692676	346.252376	5.022246
3.670007	351.480339	5.027251
3.853698	349.665178	5.032256
3.589817	347.679037	5.037261
3.750347	332.413636	5.042266
3.489683	352.699156	5.047270
3.400909	367.709510	5.052275
3.820464	362.368463	5.057280
3.877581	366.787158	5.062285
3.970194	372.032676	5.067290
3.312296	357.394062	5.072294
3.512942	364.379431	5.077299
3.991104	369.559261	5.082304
3.715826	375.261253	5.087309
4.017661	380.623031	5.092314
4.026597	397.045591	5.097318
3.742398	375.386571	5.102323
3.808137	372.488903	5.107328
3.747143	387.563147	5.112333
3.550975	375.275645	5.117338
3.571824	396.322726	5.122342
3.621344	390.533894	5.127347
3.945952	383.107623	5.132352
3.469688	379.408336	5.137357
3.753322	385.840495	5.142362
4.097403	410.227277	5.147366
4.015007	424.834445	5.152371
4.418474	415.768022	5.157376
4.208853	409.491280	5.162381
4.367595	394.701005	5.167386
4.093541	389.285068	5.172390
3.927399	404.315740	5.177395
4.296518	401.623825	5.182400
3.962883	389.718601	5.187405
4.082046	395.933987	5.192410
3.897854	401.906423	5.197414
4.422917	400.217638	5.202419
4.077322	409.626719	5.207424
4.304041	424.690940	5.212429
4.314230	420.373227	5.217434
4.075625	416.176436	5.222438
4.400800	394.799934	5.227443
4.418503	413.587335	5.232448
4.047753	423.745572	5.237453
4.437661	417.019649	5.242458
4.235120	408.957290	5.247462
4.302584	409.833904	5.252467
4.556734	424.534612	5.257472
4.098017	405.743387	5.262477
4.531230	389.930452	5.267482
4.237612	394.675635	5.272486
4.284403	418.252630	5.277491
4.576334	428.402573	5.282496
4.448692	400.749129	5.287501
4.388491	368.633398	5.292506
4.144348	391.669305	5.297510
3.977277	417.368638	5.302515
4.670151	405.089959	5.307520
4.125472	405.408073	5.312525
4.563392	406.733281	5.317530
4.407091	410.047476	5.322534
4.339131	414.597144	5.327539
4.832740	393.503551	5.332544
4.301805	403.653720	5.337549
4.368079	419.426405	5.342554
4.028289	423.872827	5.347558
4.090633	405.999042	5.352563
4.302326	418.282679	5.357568
4.424765	408.677718	5.362573
4.258275	402.199909	5.367578
4.742321	437.749516	5.372582
4.578236	438.804280	5.377587
4.674519	421.244588	5.382592
4.501711	417.952379	5.387597
4.569330	418.274762	5.392602
4.398850	439.238497	5.397606
4.311629	440.078330	5.402611
4.570131	432.857001	5.407616
4.629899	440.922307	5.412621
4.728265	439.688365	5.417626
4.867504	449.657183	5.422630
4.666423	441.937861	5.427635
4.953309	424.284421	5.432640
4.476886	435.512016	5.437645
4.430321	433.513430	5.442650
4.512977	427.979342	5.447654
4.777204	453.598978	5.452659
4.927690	459.940022	5.457664
4.808017	451.508515	5.462669
4.880704	430.738351	5.467674
4.568307	435.833893	5.472678
4.759290	453.628420	5.477683
4.709977	451.323194	5.482688
4.555671	448.419752	5.487693
4.800445	451.459035	5.492698
4.894413	478.604924	5.497702
5.101591	491.024417	5.502707
5.314558	468.485530	5.507712
5.056078	452.245552	5.512717
4.947216	434.777751	5.517722
4.835120	450.952836	5.522726
4.798918	442.513163	5.527731
5.045067	428.141280	5.532736
4.746470	439.471483	5.537741
4.981274	464.004257	5.542746
5.064861	486.440128	5.547750
4.966317	471.542646	5.552755
5.361061	459.409275	5.557760
4.614472	480.781677	5.562765
4.993508	465.301283	5.567770
4.901368	481.578854	5.572774
4.835147	504.891043	5.577779
5.216454	485.651834	5.582784
4.891364	467.822865	5.587789
5.224033	478.204740	5.592794
5.123870	499.292578	5.597798
5.367563	487.364673	5.602803
5.449490	468.883060	5.607808
5.260859	491.799358	5.612813
5.297540	478.001258	5.617818
5.286287	466.251735	5.622822
5.235400	467.607811	5.627827
4.844608	484.178103	5.632832
4.763709	494.918952	5.637837
5.299889	474.474819	5.642842
4.918201	473.418065	5.647846
4.543415	483.301483	5.652851
5.037517	476.151686	5.657856
5.076960	489.145310	5.662861
5.570304	500.392037	5.667866
5.286045	493.829083	5.672870
5.106090	496.893679	5.677875
5.314027	505.927336	5.682880
5.411716	518.492990	5.687885
5.584567	518.415031	5.692890
5.246757	518.898133	5.697894
5.353614	516.615426	5.702899
5.550550	517.408305	5.707904
5.541747	529.411709	5.712909
5.549813	509.468240	5.717914
5.426041	511.078645	5.722918
5.499162	522.865881	5.727923
5.750598	519.645694	5.732928
5.380329	515.656192	5.737933
5.610092	511.422026	5.742938
5.793245	519.048615	5.747942
5.489091	516.760435	5.752947
5.579951	515.082525	5.757952
5.522450	505.064109	5.762957
5.711431	495.555229	5.767962
5.462718	506.989007	5.772966
5.542876	512.585848	5.777971
5.834364	512.872225	5.782976
5.540379	526.473217	5.787981
5.582719	526.136170	5.792986
5.712215	524.042876	5.797990
5.632456	504.314480	5.802995
5.607750	528.597652	5.808000
5.637190	534.392584	5.813005
5.591324	514.409289	5.818010
5.452896	535.350002	5.823014
5.439936	514.051211	5.828019
5.776955	501.239665	5.833024
5.757457	510.285063	5.838029
5.654575	523.356098	5.843034
5.644634	506.745009	5.848038
5.823650	499.560361	5.853043
6.115635	509.952927	5.858048
5.680022	530.238885	5.863053
5.582218	532.742904	5.868058
5.497243	517.723474	5.873062
5.362755	526.308056	5.878067
5.855162	527.479159	5.883072
5.782818	546.335367	5.888077
5.998877	552.327148	5.893082
5.972687	556.502487	5.898086
5.973151	551.590109	5.903091
6.076350	541.756912	5.908096
5.673391	543.545548	5.913101
6.072855	541.828080	5.918106
6.401651	532.534705	5.923110
5.846318	530.462344	5.928115
6.061717	532.982673	5.933120
5.686794	521.994007	5.938125
6.092437	516.024149	5.943130
6.063360	545.012337	5.948134
6.292129	564.321818	5.953139
6.205192	529.280980	5.958144
5.770821	516.708074	5.963149
6.210574	515.264213	5.968154
6.276140	539.775061	5.973158
5.778158	547.893728	5.978163
6.099372	527.093708	5.983168
5.835317	538.779824	5.988173
5.984194	537.979967	5.993178
6.150443	545.668355	5.998182
6.229446	537.046624	6.003187
6.279020	546.506989	6.008192
5.834126	568.400736	6.013197
6.265827	551.692544	6.018202
6.374299	549.198358	6.023206
6.180926	554.068587	6.028211
6.026270	565.744635	6.033216
5.971773	570.334740	6.038221
6.107786	553.258124	6.043226
6.031697	536.591346	6.048230
5.785448	545.250045	6.053235
5.964310	544.048467	6.058240
5.945833	540.689689	6.063245
6.114465	551.794592	6.068250
6.089622	564.148609	6.073254
5.789802	547.948309	6.078259
6.096445	546.988514	6.083264
6.337269	571.026924	6.088269
6.272898	595.368053	6.093274
6.524339	587.990965	6.098278
6.083448	556.871073	6.103283
6.389697	547.249559	6.108288
6.297717	557.854076	6.113293
5.969434	560.506871	6.118298
6.014133	546.696237	6.123302
6.152418	555.557552	6.128307
6.357545	563.741746	6.133312
5.967649	566.815006	6.138317
6.253907	584.288620	6.143322
6.387870	579.259370	6.148326
6.424211	578.431743	6.153331
6.425047	566.568969	6.158336
6.286602	550.808313	6.163341
5.971440	557.534035	6.168346
5.929018	555.325908	6.173350
5.819142	562.067031	6.178355
6.134445	565.871841	6.183360
6.292183	590.928557	6.188365
6.565781	560.517857	6.193370
6.343647	572.238503	6.198374
6.071194	561.517775	6.203379
6.413551	540.938471	6.208384
6.177647	552.445534	6.213389
5.955722	551.076093	6.218394
5.954004	553.621157	6.223398
6.342534	554.100437	6.228403
6.328292	540.491322	6.233408
6.125537	561.174080	6.238413
6.256532	561.600033	6.243418
6.401300	540.838524	6.248422
6.447813	565.157533	6.253427
6.234804	561.454749	6.258432
6.175579	562.670550	6.263437
6.325687	547.551475	6.268442
6.067155	552.464235	6.273446
6.242549	569.610488	6.278451
5.906832	552.231339	6.283456
6.140345	548.065105	6.288461
6.084183	540.806644	6.293466
5.828542	546.769044	6.298470
6.007399	574.955930	6.303475
6.226383	574.280524	6.308480
6.316700	585.561360	6.313485
6.324337	577.446719	6.318490
6.394107	577.065283	6.323494
6.103552	569.182424	6.328499
6.151329	552.304174	6.333504
5.977820	566.037902	6.338509
6.123064	582.878406	6.343514
6.434692	577.881354	6.348518
5.879609	582.775358	6.353523
6.225473	585.305900	6.358528
6.034516	585.557572	6.363533
6.397212	573.123004	6.368538
6.231201	586.673897	6.373542
6.253999	600.617302	6.378547
6.614656	587.121689	6.383552
6.195439	562.764265	6.388557
6.174581	565.566515	6.393562
6.328532	559.634781	6.398566
5.871918	559.045865	6.403571
6.243105	560.892230	6.408576
6.474380	563.949157	6.413581
6.196847	552.940724	6.418586
6.235771	568.957604	6.423590
5.990741	554.053274	6.428595
6.112151	539.620317	6.433600
6.067406	566.161976	6.438605
5.806196	580.242360	6.443610
5.804656	573.577212	6.448614
5.968464	574.106453	6.453619
6.276932	582.519117	6.458624
6.221907	589.185487	6.463629
6.366561	600.853040	6.468634
6.646608	591.012191	6.473638
6.125871	589.214070	6.478643
6.217481	580.972991	6.483648
6.182451	600.458598	6.488653
6.623641	586.618708	6.493658
6.610704	546.123813	6.498662
6.233117	565.356029	6.503667
6.585452	572.133235	6.508672
6.220055	556.289529	6.513677
6.137557	549.653354	6.518682
6.384105	557.672467	6.523686
6.139259	568.036887	6.528691
6.134390	560.347229	6.533696
5.892029	566.628940	6.538701
6.175914	549.692241	6.543706
6.286987	554.756019	6.548710
6.205546	572.384989	6.553715
6.427224	562.837617	6.558720
6.145337	555.873137	6.563725
6.319477	560.868095	6.568730
6.189490	553.050255	6.573734
5.856532	557.358760	6.578739
6.351599	545.878668	6.583744
6.239625	543.663490	6.588749
6.126146	554.585656	6.593754
6.312527	554.447160	6.598758
6.540324	564.691249	6.603763
6.417475	567.455900	6.608768
5.904535	571.091769	6.613773
6.356840	565.319865	6.618778
6.592429	544.276991	6.623782
6.233274	548.675844	6.628787
6.650745	549.057611	6.633792
6.201574	576.151769	6.638797
6.105810	563.747887	6.643802
6.035135	555.485005	6.648806
5.663256	574.692712	6.653811
6.049160	553.921031	6.658816
6.070413	550.403569	6.663821
6.005455	547.212381	6.668826
6.233040	560.012006	6.673830
5.905644	564.514425	6.678835
6.287247	537.484485	6.683840
5.996787	554.048532	6.688845
5.968165	560.950541	6.693850
6.151811	570.065196	6.698854
5.712800	548.234807	6.703859
6.250982	557.335060	6.708864
6.313763	588.302538	6.713869
5.981346	557.299080	6.718874
6.179689	578.956522	6.723878
6.233838	585.636615	6.728883
6.346440	582.634092	6.733888
6.281677	578.507868	6.738893
5.877828	569.189346	6.743898
6.390207	583.533335	6.748902
6.229129	602.066204	6.753907
6.426788	585.159203	6.758912
6.048778	557.767234	6.763917
6.079480	561.969968	6.768922
6.069782	574.051093	6.773926
6.158349	593.732504	6.778931
6.251843	581.039167	6.783936
6.092335	573.880340	6.788941
6.279115	594.852921	6.793946
6.347927	609.655659	6.798950
6.508427	599.549957	6.803955
6.486173	557.203641	6.808960
6.309413	564.047266	6.813965
5.974070	565.581166	6.818970
6.197668	549.291310	6.823974
6.321554	568.154280	6.828979
6.208165	564.249967	6.833984
6.089843	562.711287	6.838989
6.085017	544.736671	6.843994
6.291998	550.751063	6.848998
5.859856	567.375235	6.854003
6.009118	555.771852	6.859008
5.992865	559.900961	6.864013
6.252576	579.594123	6.869018
6.156434	597.142291	6.874022
6.123889	589.549823	6.879027
6.802773	584.110207	6.884032
6.386993	561.889650	6.889037
6.578391	557.662699	6.894042
6.575152	553.570016	6.899046
6.102071	561.004981	6.904051
6.156207	548.542601	6.909056
5.985318	555.115052	6.914061
6.312574	546.876186	6.919066
6.315835	554.653267	6.924070
5.819931	574.313946	6.929075
6.234478	568.585175	6.934080
5.919415	555.360674	6.939085
5.979855	542.929318	6.944090
5.962457	549.431812	6.949094
5.644254	578.649948	6.954099
6.366280	579.376575	6.959104
6.322316	587.808518	6.964109
6.217896	581.492913	6.969114
6.462860	582.013084	6.974118
6.306135	564.567941	6.979123
5.777163	563.752745	6.984128
5.923174	578.793363	6.989133
6.063905	586.503745	6.994138
6.322567	569.461003	6.999142
6.292191	571.038223	7.004147
6.302770	588.483807	7.009152
6.268825	607.603353	7.014157
6.335263	597.261541	7.019162
6.467325	591.280734	7.024166
6.250206	579.435617	7.029171
6.418373	568.889088	7.034176
6.296696	563.491708	7.039181
6.054296	555.779354	7.044186
6.162015	565.284675	7.049190
6.107180	561.444870	7.054195
6.273676	556.304993	7.059200
6.004136	564.484171	7.064205
6.219060	558.782572	7.069210
6.395465	559.068041	7.074214
6.254668	557.411540	7.079219
6.055254	570.795600	7.084224
6.201782	565.570630	7.089229
6.153248	561.765297	7.094234
6.101883	561.609267	7.099238
6.098239	559.089709	7.104243
5.920487	545.082433	7.109248
6.311141	581.303920	7.114253
6.572460	595.047599	7.119258
6.009284	576.116870	7.124262
5.942132	565.709062	7.129267
6.286457	577.597621	7.134272
6.132890	594.330764	7.139277
6.186052	590.050984	7.144282
6.293987	564.739216	7.149286
6.055742	575.001533	7.154291
6.287267	594.287610	7.159296
6.326523	591.277871	7.164301
6.266680	571.712323	7.169306
5.880361	547.969100	7.174310
6.175289	591.905598	7.179315
6.321371	603.325799	7.184320
6.151730	598.105319	7.189325
6.209789	583.851974	7.194330
6.671736	571.776070	7.199334
6.173900	578.714586	7.204339
6.031716	566.064551	7.209344
6.024434	559.475822	7.214349
6.052539	574.320373	7.219354
6.351996	571.156757	7.224358
5.996748	570.275168	7.229363
6.393868	576.261700	7.234368
6.369455	556.985670	7.239373
6.223256	551.697112	7.244378
6.123073	567.065275	7.249382
6.129902	566.242132	7.254387
6.256374	556.914405	7.259392
5.887669	571.952278	7.264397
5.977761	581.659102	7.269402
6.283113	579.462950	7.274406
6.244445	581.785456	7.279411
6.365937	591.820929	7.284416
6.408880	593.763665	7.289421
6.401844	585.524086	7.294426
6.284871	561.822651	7.299430
6.065193	545.870431	7.304435
6.103346	566.247427	7.309440
5.979941	563.149154	7.314445
6.059843	565.300637	7.319450
6.374287	565.617650	7.324454
5.699669	589.710199	7.329459
6.324203	571.447371	7.334464
6.366818	571.971386	7.339469
6.297273	596.167468	7.344474
6.407101	598.965688	7.349478
6.088932	577.671671	7.354483
6.178677	559.800281	7.359488
6.450976	559.461929	7.364493
6.308166	579.057949	7.369498
6.183449	566.768549	7.374502
6.414293	558.981539	7.379507
6.261741	560.125064	7.384512
6.465300	559.508141	7.389517
6.149923	556.019869	7.394522
6.642375	551.057361	7.399526
6.261892	553.919434	7.404531
6.230362	542.233675	7.409536
6.384324	548.419401	7.414541
6.103758	560.210857	7.419546
6.227313	562.968230	7.424550
5.727987	570.568926	7.429555
5.724484	549.312521	7.434560
5.886985	552.460321	7.439565
5.799953	554.290665	7.444570
6.043935	579.290886	7.449574
5.768273	584.930278	7.454579
6.565813	592.919420	7.459584
6.253171	602.851243	7.464589
6.299620	607.147768	7.469594
6.403411	589.710743	7.474598
6.001710	579.052892	7.479603
6.360530	577.281766	7.484608
6.161282	567.740322	7.489613
6.182037	565.297820	7.494618
6.217676	558.187642	7.499622
5.976913	561.726937	7.504627
6.499829	591.085572	7.509632
6.201772	580.834783	7.514637
6.162473	561.440265	7.519642
6.334815	542.651916	7.524646
6.186787	561.213062	7.529651
6.380325	557.574988	7.534656
6.457390	564.025181	7.539661
6.066473	574.393915	7.544666
6.322380	569.829180	7.549670
6.258594	556.877350	7.554675
6.376024	556.140004	7.559680
6.211233	567.523952	7.564685
6.082074	566.756624	7.569690
6.137895	562.599921	7.574694
6.134039	561.359581	7.579699
6.012491	551.934143	7.584704
6.603202	575.657266	7.589709
6.121629	559.231981	7.594714
6.495566	555.315107	7.599718
6.307381	562.543575	7.604723
6.507182	564.746370	7.609728
6.495420	566.542080	7.614733
6.173279	564.680465	7.619738
6.199791	541.379243	7.624742
6.112740	554.096104	7.629747
6.553314	560.990419	7.634752
6.164912	574.253301	7.639757
6.176032	545.212050	7.644762
6.231169	542.092662	7.649766
6.091682	556.653456	7.654771
6.101629	551.105690	7.659776
5.940359	561.627056	7.664781
5.891197	568.992167	7.669786
6.126509	557.629078	7.674790
5.968843	552.788308	7.679795
6.029808	564.151519	7.684800
5.982324	555.880365	7.689805
5.939679	550.816680	7.694810
5.858244	557.259522	7.699814
5.957755	566.426552	7.704819
6.416182	566.389691	7.709824
6.002523	568.741215	7.714829
6.237479	586.339912	7.719834
6.217955	577.222946	7.724838
6.427540	574.181017	7.729843
6.289320	559.038353	7.734848
6.222465	557.443028	7.739853
6.057039	570.747583	7.744858
6.191798	550.779474	7.749862
6.302496	565.351709	7.754867
6.382287	562.243139	7.759872
6.421793	554.703793	7.764877
6.025122	558.460132	7.769882
6.505494	548.487556	7.774886
6.439382	567.162626	7.779891
6.180237	560.549720	7.784896
6.077718	551.674362	7.789901
5.850674	566.683592	7.794906
6.446095	574.966263	7.799910
6.045675	567.477019	7.804915
6.004279	539.762508	7.809920
5.882211	556.994108	7.814925
6.321417	578.413955	7.819930
6.144483	569.873468	7.824934
5.987900	548.062600	7.829939
6.149505	542.029874	7.834944
5.972237	569.764106	7.839949
6.087881	596.643426	7.844954
6.626019	588.566986	7.849958
6.338444	560.517859	7.854963
6.440662	565.904306	7.859968
6.133475	575.873881	7.864973
6.156607	565.678835	7.869978
6.250632	542.918791	7.874982
6.089802	551.175885	7.879987
6.013812	570.128020	7.884992
6.245642	564.997960	7.889997
6.267884	547.208767	7.895002
6.211537	537.995608	7.900006
6.176293	553.333790	7.905011
6.037833	554.523817	7.910016
6.335129	566.130210	7.915021
6.213628	572.921597	7.920026
6.232710	557.364361	7.925030
6.178203	551.432157	7.930035
6.260493	544.855662	7.935040
6.526423	552.890313	7.940045
6.319989	575.951635	7.945050
6.537758	552.207424	7.950054
6.466132	541.233436	7.955059
6.514738	541.303858	7.960064
6.422284	558.373714	7.965069
6.156293	565.647694	7.970074
6.320191	547.517441	7.975078
5.951076	543.375920	7.980083
6.124802	551.552473	7.985088
6.462995	568.898419	7.990093
6.215305	553.553271	7.995098
6.531251	543.928874	8.000102
6.407622	549.152971	8.005107
6.202271	560.355887	8.010112
6.062039	574.093336	8.015130
6.039361	554.246499	8.020147
6.334030	555.595962	8.025165
6.041844	564.070149	8.030182
6.158418	557.807987	8.035200
6.100504	553.760168	8.040218
6.392384	551.371579	8.045235
6.482322	558.392162	8.050253
6.479423	555.401683	8.055270
6.134817	541.364708	8.060288
6.520657	561.938357	8.065306
6.086932	546.912352	8.070323
6.351266	534.338189	8.075341
6.271457	533.838855	8.080358
6.263023	531.271813	8.085376
6.187457	529.440758	8.090394
6.173392	524.576087	8.095411
6.368419	535.146390	8.100429
6.370018	557.831967	8.105446
6.267488	540.154725	8.110464
6.241034	525.073048	8.115482
6.213084	533.600179	8.120499
6.233566	543.921754	8.125517
6.206802	552.881648	8.130534
6.260680	551.466084	8.135552
6.490471	555.871373	8.140570
6.181864	564.696601	8.145587
6.738169	547.423913	8.150605
6.459219	544.124037	8.155622
6.353897	546.285352	8.160640
6.385122	529.180536	8.165658
6.022877	520.528630	8.170675
6.232760	528.657896	8.175693
6.060083	558.332307	8.180710
6.310230	552.919383	8.185728
6.772704	541.477005	8.190746
6.263504	569.133818	8.195763
6.534972	556.262380	8.200781
6.449196	552.381521	8.205798
6.278269	553.921378	8.210816
6.327325	555.351870	8.215834
6.223817	549.030931	8.220851
6.602741	540.583998	8.225869
6.399544	548.014826	8.230886
6.167682	549.502269	8.235904
6.481619	545.230744	8.240922
6.045824	549.906312	8.245939
6.203428	542.000437	8.250957
6.434698	538.750558	8.255974
6.294181	536.262609	8.260992
6.666512	540.671103	8.266010
6.420398	543.366957	8.271027
6.155971	558.198929	8.276045
6.253482	566.486017	8.281062
6.299467	552.820189	8.286080
6.672682	551.748985	8.291098
6.557022	558.424910	8.296115
6.658674	537.185791	8.301133
6.767854	554.550855	8.306150
6.555548	564.314329	8.311168
6.553701	541.255325	8.316186
6.523563	551.504584	8.321203
6.561992	548.011648	8.326221
6.692218	550.053747	8.331238
6.686949	558.299564	8.336256
6.651876	558.187312	8.341274
6.518787	542.534036	8.346291
6.222168	530.647290	8.351309
6.769522	551.464926	8.356326
6.462053	569.714378	8.361344
6.802030	548.924894	8.366362
6.345552	549.577163	8.371379
6.616666	555.719029	8.376397
6.534124	569.236277	8.381414
6.488216	555.916248	8.386432
6.493917	549.769627	8.391450
6.329603	557.218534	8.396467
6.833845	539.192273	8.401485
6.810659	554.198684	8.406502
6.649985	560.590006	8.411520
6.697408	560.353719	8.416538
6.442177	570.810416	8.421555
6.670816	553.387892	8.426573
6.449582	550.877660	8.431590
6.408286	552.868402	8.436608
6.714018	556.887428	8.441626
6.400639	548.096464	8.446643
6.342260	534.877994	8.451661
6.211305	539.563204	8.456678
6.297238	555.517945	8.461696
6.496412	567.132960	8.466714
6.449822	574.596171	8.471731
6.694209	580.459175	8.476749
6.801196	582.034089	8.481766
6.898754	600.125530	8.486784
6.656776	580.624556	8.491802
6.783382	576.365483	8.496819
6.702543	580.930643	8.501837
6.842229	584.885410	8.506854
6.540076	591.258405	8.511872
6.984534	587.682815	8.516890
7.013750	589.867560	8.521907
7.008229	575.878427	8.526925
6.952047	571.754059	8.531942
6.670723	553.894989	8.536960
6.956715	547.049381	8.541978
6.482110	575.485207	8.546995
6.488494	570.535079	8.552013
6.906172	550.515602	8.557030
6.633001	554.706356	8.562048
7.097485	567.932375	8.567066
6.695291	560.238258	8.572083
6.651136	550.314624	8.577101
6.711789	566.029036	8.582119
6.775562	568.096386	8.587136
6.843240	545.134025	8.592154
6.645253	558.049553	8.597171
6.588832	577.860422	8.602189
6.942934	588.229424	8.607207
6.655657	581.937364	8.612224
7.068095	577.821355	8.617242
6.845672	593.992992	8.622259
6.955892	605.642317	8.627277
7.186352	587.054915	8.632295
6.485861	577.079832	8.637312
6.756543	575.911724	8.642330
6.685476	579.051161	8.647347
7.085321	575.221113	8.652365
6.892740	582.492272	8.657383
6.627664	605.634866	8.662400
6.923764	579.335331	8.667418
6.718999	573.213349	8.672435
6.661541	594.275831	8.677453
7.034311	599.932443	8.682471
6.489701	594.593968	8.687488
6.774638	576.606955	8.692506
6.683210	584.793028	8.697523
6.806852	594.262588	8.702541
6.909574	605.166805	8.707559
6.585837	590.406949	8.712576
6.662923	577.082124	8.717594
7.044309	586.248723	8.722611
6.916357	582.242482	8.727629
6.898866	595.309659	8.732647
6.431404	603.047298	8.737664
6.818144	609.198121	8.742682
7.038534	639.634769	8.747699
7.147792	631.080326	8.752717
7.406774	616.741917	8.757735
7.050625	626.881564	8.762752
7.216014	614.827878	8.767770
7.135018	618.356948	8.772787
6.933351	597.665664	8.777805
6.849386	577.661451	8.782823
6.775291	593.351125	8.787840
6.999796	601.944517	8.792858
7.234020	613.650598	8.797875
7.239707	615.808634	8.802893
7.070056	591.841520	8.807911
6.570702	611.905207	8.812928
7.023830	620.039389	8.817946
7.028801	607.673631	8.822963
6.974816	635.898073	8.827981
6.985821	612.158974	8.832999
7.160851	613.211765	8.838016
7.024921	626.707875	8.843034
7.201759	639.355584	8.848051
7.174084	616.566604	8.853069
7.453215	599.094947	8.858087
7.221694	616.629148	8.863104
7.367455	612.334821	8.868122
7.025571	606.912951	8.873139
6.650321	614.140418	8.878157
6.759224	623.642441	8.883175
6.868778	629.610207	8.888192
6.792543	638.986087	8.893210
7.123184	620.238330	8.898227
7.375117	615.944267	8.903245
7.447977	631.638525	8.908263
7.138216	621.823384	8.913280
7.167281	611.495890	8.918298
7.228561	614.155620	8.923315
7.315924	612.335809	8.928333
7.393058	616.456979	8.933351
7.168664	632.112296	8.938368
7.123475	639.681774	8.943386
7.473894	620.275122	8.948403
7.412921	610.985058	8.953421
7.167520	612.279425	8.958439
7.316338	632.022797	8.963456
7.385657	630.466720	8.968474
7.509064	618.312320	8.973491
7.372982	625.031205	8.978509
7.096718	621.482413	8.983527
7.315477	619.351105	8.988544
7.631064	623.094876	8.993562
7.385436	603.708225	8.998579
7.007831	604.308497	9.003597
7.271346	602.214566	9.008615
7.292916	617.577420	9.013632
7.071504	627.122323	9.018650
7.220939	612.164504	9.023667
7.252575	622.468347	9.028685
7.328520	622.022579	9.033703
7.311377	613.856158	9.038720
7.084451	618.375314	9.043738
7.573769	619.460692	9.048755
7.267084	624.097824	9.053773
7.562466	614.495593	9.058791
7.384954	604.987455	9.063808
7.682464	612.547518	9.068826
7.671030	623.444931	9.073843
7.095711	622.267158	9.078861
7.378683	615.858512	9.083879
7.335076	616.890068	9.088896
7.472464	626.237428	9.093914
7.514372	624.802286	9.098931
6.976076	629.963093	9.103949
7.336747	636.114004	9.108967
7.132577	631.320861	9.113984
7.251551	609.318556	9.119002
7.472792	614.575629	9.124019
7.190458	639.654742	9.129037
7.520254	620.913814	9.134055
7.011390	613.654997	9.139072
7.157950	637.138161	9.144090
7.619230	618.908038	9.149107
7.440417	629.845712	9.154125
7.352098	623.446857	9.159143
7.278089	617.662400	9.164160
7.295618	622.583656	9.169178
7.506606	621.078262	9.174195
7.057814	633.973310	9.179213
7.769759	651.969776	9.184231
7.768479	661.180668	9.189248
7.460917	640.068659	9.194266
7.605419	614.110466	9.199283
7.642694	634.665066	9.204301
7.688145	616.393949	9.209319
7.121817	636.951083	9.214336
7.383567	637.849427	9.219354
7.610510	636.379770	9.224371
7.633581	655.201693	9.229389
7.840253	649.406066	9.234407
7.504039	639.213994	9.239424
7.671586	643.321609	9.244442
7.782318	652.602741	9.249459
7.679580	656.263920	9.254477
7.719672	629.228671	9.259495
7.583003	620.908322	9.264512
7.619618	613.158096	9.269530
7.782751	631.599562	9.274547
7.447510	641.594366	9.279565
7.709178	609.809861	9.284583
7.553012	603.635554	9.289600
7.457065	610.067466	9.294618
7.670872	642.834283	9.299635
7.674918	654.805044	9.304653
7.686189	629.389565	9.309671
7.638159	632.982463	9.314688
7.747393	656.319406	9.319706
7.812481	649.387457	9.324723
7.463772	650.163319	9.329741
7.855773	636.559986	9.334759
7.944522	658.124824	9.339776
7.979212	661.253887	9.344794
7.784459	625.943796	9.349811
7.517689	620.751962	9.354829
7.410189	611.559423	9.359847
7.506716	642.044588	9.364864
7.898089	646.913322	9.369882
8.136244	639.286524	9.374899
7.831406	631.566737	9.379917
7.453943	631.631898	9.384935
7.600926	642.687839	9.389952
7.645957	642.891293	9.394970
7.831006	632.268200	9.399987
8.005636	646.031225	9.405005
7.994183	664.284613	9.410023
8.184434	640.684110	9.415040
7.886212	635.681472	9.420058
7.724933	619.733743	9.425075
7.743586	616.899881	9.430093
7.818244	622.862585	9.435111
8.186517	620.364834	9.440128
7.744444	616.706474	9.445146
7.557784	622.014622	9.450163
7.473374	637.405442	9.455181
7.602201	645.389350	9.460199
8.047872	654.315018	9.465216
7.950594	647.792375	9.470234
7.950838	629.209216	9.475251
7.816239	657.890401	9.480269
8.105821	672.048905	9.485287
8.102403	645.635216	9.490304
7.670759	636.369491	9.495322
7.898340	636.162568	9.500339
7.837693	639.121410	9.505357
8.035117	628.542815	9.510375
7.823770	638.124339	9.515392
7.495487	666.565575	9.520410
7.855523	652.975283	9.525427
7.765484	645.996156	9.530445
7.884089	650.037570	9.535463
8.032045	660.257471	9.540480
7.934189	659.705717	9.545498
8.331058	642.870476	9.550515
7.785002	638.123202	9.555533
7.993445	655.446394	9.560551
8.329565	642.734232	9.565568
7.718319	645.019412	9.570586
8.239717	640.824964	9.575603
7.786916	654.694142	9.580621
7.923901	642.992867	9.585639
7.946380	634.360957	9.590656
7.596544	666.150989	9.595674
8.052966	653.053979	9.600691
7.644430	639.357014	9.605709
7.937949	637.355435	9.610727
8.262301	674.010156	9.615744
7.946855	670.576951	9.620762
8.131013	661.622621	9.625779
8.461445	654.981866	9.630797
8.355403	657.276350	9.635815
8.261788	652.211163	9.640832
8.219076	647.745173	9.645850
8.047698	645.506628	9.650867
8.038801	660.205257	9.655885
7.818753	655.893535	9.660903
8.395472	652.932119	9.665920
8.232365	644.532097	9.670938
8.140592	644.003052	9.675955
7.851591	662.618064	9.680973
7.766600	674.747215	9.685991
8.406741	670.938144	9.691008
8.398608	683.523665	9.696026
8.040911	665.106377	9.701043
8.169741	672.769128	9.706061
8.296663	671.216811	9.711079
8.523023	681.462735	9.716096
7.995966	689.021539	9.721114
7.953725	659.314750	9.726131
8.062835	666.912763	9.731149
8.022685	690.419484	9.736167
8.286914	670.044802	9.741184
8.102187	695.358889	9.746202
8.312237	698.779071	9.751219
8.237196	690.736218	9.756237
8.172057	683.936571	9.761255
8.551636	677.688263	9.766272
8.314826	699.092845	9.771290
8.173183	688.434059	9.776307
8.298310	681.318894	9.781325
8.114749	675.559604	9.786343
8.333721	686.167874	9.791360
8.267595	708.258043	9.796378
7.903531	674.642001	9.801395
7.870909	675.594208	9.806413
8.217001	678.352906	9.811431
8.512603	684.667205	9.816448
8.062420	694.886592	9.821466
8.297785	672.057015	9.826483
8.133894	669.941802	9.831501
8.477459	695.961578	9.836519
8.271343	697.935789	9.841536
8.344052	708.127519	9.846554
8.419759	724.287023	9.851571
8.465697	722.161136	9.856589
8.466432	720.353365	9.861607
8.789192	713.869912	9.866624
8.211271	710.894232	9.871642
8.385347	702.562242	9.876659
8.602635	709.352457	9.881677
8.655805	701.682596	9.886695
8.369295	691.357408	9.891712
8.564716	700.697388	9.896730
8.541824	703.790122	9.901747
8.359613	683.242416	9.906765
8.472668	686.137925	9.911783
8.200935	700.887013	9.916800
8.242520	721.601504	9.921818
8.313407	728.182028	9.926835
8.656020	703.404003	9.931853
8.073992	704.420338	9.936871
8.661623	709.455129	9.941888
8.459348	708.158139	9.946906
8.552725	701.368794	9.951923
8.934880	717.340679	9.956941
8.610276	717.267809	9.961959
8.930263	690.776194	9.966976
8.914954	697.988694	9.971994
8.953706	716.943498	9.977011
8.783113	712.239735	9.982029
8.286218	697.034506	9.987047
8.899642	691.659603	9.992064
8.613416	693.006773	9.997082
8.363814	690.470900	10.002099
8.647743	701.728699	10.007117
8.806615	711.655866	10.012135
8.958278	709.889573	10.017152
8.590495	697.195488	10.022170
8.416639	692.020844	10.027187
8.854118	700.301121	10.032205
8.824711	700.523273	10.037223
8.636361	689.276108	10.042240
8.632793	686.025056	10.047258
8.469268	687.815307	10.052275
8.889718	705.969623	10.057293
8.690811	722.504830	10.062311
9.001792	717.304668	10.067328
9.057069	684.462876	10.072346
8.683356	675.019294	10.077363
8.568108	687.121968	10.082381
8.047585	700.390440	10.087399
8.365716	701.555379	10.092416
8.392768	699.374169	10.097434
8.812820	710.486974	10.102451
8.789699	723.802170	10.107469
8.776128	727.742941	10.112487
8.941114	722.036732	10.117504
9.125235	700.716650	10.122522
8.933526	716.219740	10.127539
9.087926	723.686513	10.132557
8.749060	720.375737	10.137575
8.953928	696.926922	10.142592
8.993888	713.734076	10.147610
8.874884	730.252446	10.152627
9.090606	727.946574	10.157645
8.871697	739.747019	10.162663
8.702164	738.852773	10.167680
8.845668	723.645991	10.172698
8.744581	708.239157	10.177715
9.035432	704.551463	10.182733
8.653601	721.104597	10.187751
8.919600	723.215596	10.192768
9.064166	712.770941	10.197786
9.142646	702.431086	10.202803
9.123787	707.377767	10.207821
8.748103	736.278909	10.212839
9.383478	714.849303	10.217856
9.043816	700.320356	10.222874
9.055523	709.284611	10.227891
9.008851	706.996422	10.232909
9.000895	718.676383	10.237927
8.994184	697.889672	10.242944
9.124752	699.416324	10.247962
8.681148	711.133537	10.252979
9.004087	719.987917	10.257997
8.943506	709.786066	10.263015
9.152326	694.046515	10.268032
8.829042	723.510569	10.273050
8.946096	727.673291	10.278067
9.155837	724.237612	10.283085
9.073976	711.556091	10.288103
8.945773	716.845952	10.293120
9.009283	726.958430	10.298138
8.892546	719.336711	10.303155
8.739612	705.079084	10.308173
9.050235	712.525544	10.313191
8.977951	723.877354	10.318208
8.878037	709.560384	10.323226
8.773411	713.851147	10.328243
8.940442	720.654396	10.333261
8.929059	725.104607	10.338279
8.932501	750.095052	10.343296
9.195898	745.955413	10.348314
8.924322	745.173968	10.353331
9.173685	760.704582	10.358349
9.016647	758.717323	10.363367
9.079824	744.488201	10.368384
9.187610	741.987721	10.373402
8.811909	746.068043	10.378419
9.155635	755.601207	10.383437
9.388825	754.544470	10.388455
9.077640	761.533625	10.393472
9.115398	762.244347	10.398490
9.190351	750.879236	10.403507
9.199998	729.517295	10.408525
9.175738	751.883013	10.413543
8.894102	763.159733	10.418560
9.356432	758.954745	10.423578
9.216654	751.839832	10.428595
9.344125	737.990438	10.433613
9.189733	746.327025	10.438631
9.093889	748.142210	10.443648
9.468884	759.036671	10.448666
9.133817	778.002453	10.453683
9.923981	770.515705	10.458701
9.645128	751.452578	10.463719
9.630530	754.402257	10.468736
9.930676	764.983195	10.473754
9.471053	769.750538	10.478771
9.614950	745.985926	10.483789
9.558973	748.556227	10.488807
9.449111	761.735142	10.493824
9.376687	759.283628	10.498842
9.414543	749.651939	10.503859
9.314925	754.955983	10.508877
9.452689	758.957557	10.513895
9.486370	769.032975	10.518912
9.335406	753.699380	10.523930
9.129978	743.799812	10.528947
9.441517	737.435692	10.533965
9.231979	751.283256	10.538983
9.228633	760.756388	10.544000
9.390736	746.039586	10.549018
9.458033	743.088342	10.554035
9.586160	764.559642	10.559053
9.388024	744.566404	10.564071
9.201089	739.775692	10.569088
9.349546	751.468304	10.574106
9.627820	776.712015	10.579123
9.689515	776.513808	10.584141
9.277230	750.969553	10.589159
9.590911	751.235769	10.594176
9.763951	768.368044	10.599194
9.413270	781.683597	10.604211
9.576234	765.024830	10.609229
9.667562	763.570291	10.614247
9.548734	786.191976	10.619264
9.829916	780.908945	10.624282
9.117243	760.386116	10.629299
9.487456	776.615282	10.634317
9.638273	790.466897	10.639335
9.595866	792.226813	10.644352
9.836795	773.074221	10.649370
9.726932	778.290128	10.654387
10.088492	789.475435	10.659405
9.836873	790.308763	10.664423
9.833099	770.806755	10.669440
9.518022	765.852713	10.674458
9.595240	777.813151	10.679475
9.959235	780.847969	10.684493
10.193688	793.169340	10.689511
10.031739	760.714075	10.694528
10.092302	742.800254	10.699546
9.635356	763.579966	10.704563
9.533659	750.688952	10.709581
9.701555	751.086318	10.714599
9.547862	746.260099	10.719616
9.633958	735.212166	10.724634
9.374146	759.292155	10.729651
9.630436	766.558007	10.734669
9.741370	773.941459	10.739687
9.827783	781.845857	10.744704
9.833159	786.068377	10.749722
9.879353	797.252375	10.754739
9.849014	783.276008	10.759757
9.745543	774.029767	10.764775
9.620997	776.008613	10.769792
9.630553	767.527543	10.774810
9.701065	769.578654	10.779827
9.667194	770.193467	10.784845
9.852921	790.719807	10.789863
10.077640	800.588428	10.794880
9.831939	772.705510	10.799898
9.710965	776.599296	10.804915
9.815978	780.212004	10.809933
10.088545	781.293657	10.814951
9.847573	792.436055	10.819968
9.787497	776.052261	10.824986
9.394218	771.723083	10.830003
9.926843	785.566603	10.835021
10.293125	819.221940	10.840039
10.090517	797.402690	10.845056
10.146773	769.449509	10.850074
9.763004	780.973079	10.855091
9.867413	796.650485	10.860109
10.509244	795.070431	10.865127
10.102686	783.782604	10.870144
10.316191	773.688721	10.875162
10.045587	775.574117	10.880179
9.770195	773.882817	10.885197
10.115016	777.301212	10.890215
10.066888	766.386136	10.895232
9.804497	772.711307	10.900250
9.822387	794.925082	10.905267
10.344672	796.722945	10.910285
10.481349	800.144746	10.915303
9.732080	797.158300	10.920320
10.136411	800.876626	10.925338
9.954539	800.199909	10.930355
10.258927	795.117512	10.935373
10.335857	797.639979	10.940391
10.420219	815.340751	10.945408
10.644091	806.742669	10.950426
10.321152	778.340855	10.955443
10.041908	764.964740	10.960461
10.063151	778.275112	10.965479
10.045685	787.800581	10.970496
10.295228	775.665655	10.975514
10.332516	772.310517	10.980531
10.094198	791.854953	10.985549
10.441949	813.132884	10.990567
10.278817	809.863403	10.995584
10.162905	785.382121	11.000602
10.524557	790.376057	11.005619
10.475162	795.715898	11.010637
10.587035	789.255259	11.015655
10.203432	771.855533	11.020672
10.304942	786.829266	11.025690
10.318476	773.593687	11.030707
10.326962	763.865885	11.035725
10.345969	769.733639	11.040743
10.050253	791.191379	11.045760
10.428658	786.729163	11.050778
10.185838	784.424275	11.055795
10.260061	798.693172	11.060813
10.232216	811.201664	11.065831
10.303856	806.765831	11.070848
10.428756	801.910186	11.075866
10.459910	808.805201	11.080883
10.474496	799.710847	11.085901
10.685589	805.696241	11.090919
10.602711	826.090194	11.095936
10.325904	810.295772	11.100954
10.377686	817.154911	11.105971
10.316075	812.015698	11.110989
10.550237	812.356064	11.116007
10.376459	819.484307	11.121024
10.752605	822.586988	11.126042
10.625277	808.710659	11.131059
10.734855	822.291238	11.136077
10.836231	810.710748	11.141095
10.551731	797.971229	11.146112
10.674353	776.179443	11.151130
10.856644	778.977429	11.156147
10.452552	773.827030	11.161165
10.442375	768.802134	11.166183
10.374691	790.704837	11.171200
10.469193	808.651004	11.176218
10.628827	803.729792	11.181235
10.617717	797.889805	11.186253
10.780749	807.251538	11.191271
10.484264	820.635116	11.196288
10.590160	806.026830	11.201306
10.828027	816.999982	11.206323
10.453954	818.927279	11.211341
10.484368	799.865824	11.216359
10.383402	816.129405	11.221376
10.681534	813.200122	11.226394
10.825444	821.590971	11.231411
10.728001	810.535332	11.236429
10.905580	787.981104	11.241447
10.575060	810.883117	11.246464
10.834939	824.501443	11.251482
11.018299	818.353597	11.256499
10.547220	823.590639	11.261517
11.060764	801.365711	11.266535
10.973208	821.521321	11.271552
10.949873	824.328696	11.276570
11.001974	805.219569	11.281587
10.640597	805.112038	11.286605
11.082120	821.289616	11.291623
10.888529	825.944626	11.296640
10.672907	797.082541	11.301658
11.056090	816.283421	11.306675
10.583115	815.473263	11.311693
10.936713	801.771532	11.316711
10.848263	808.629143	11.321728
10.986476	791.246777	11.326746
10.941128	814.347470	11.331763
10.887200	824.007792	11.336781
11.154694	811.752284	11.341799
11.121386	793.037795	11.346816
10.870997	776.714871	11.351834
11.088383	778.900527	11.356851
10.700893	797.014989	11.361869
11.062578	783.483644	11.366887
10.711792	803.643175	11.371904
11.017787	810.144735	11.376922
11.068737	798.514236	11.381939
10.760042	816.698060	11.386957
10.825520	816.503853	11.391975
10.620006	810.553210	11.396992
10.851995	790.931922	11.402010
10.911491	812.224032	11.407027
10.924659	815.152210	11.412045
10.987231	799.929206	11.417063
10.851618	804.339750	11.422080
11.037413	785.583158	11.427098
10.676528	804.798844	11.432115
10.461425	825.800712	11.437133
10.635312	818.077879	11.442151
11.042327	809.133080	11.447168
11.133072	819.394719	11.452186
11.230482	835.803247	11.457203
11.028945	834.975292	11.462221
11.276928	818.517518	11.467239
11.313819	829.780911	11.472256
11.192363	831.535296	11.477274
11.218610	831.850293	11.482291
11.142114	833.973627	11.487309
11.216854	823.248682	11.492327
10.965946	825.233262	11.497344
11.002380	845.472029	11.502362
10.881195	837.260393	11.507379
11.157605	833.476655	11.512397
11.120673	823.437705	11.517415
11.372046	830.513308	11.522432
11.265531	847.538367	11.527450
11.403920	829.891824	11.532467
11.454922	822.960550	11.537485
11.663965	825.046339	11.542503
11.481025	804.004823	11.547520
11.428282	819.832599	11.552538
11.465868	821.124203	11.557555
11.204717	846.910005	11.562573
11.466720	817.173591	11.567591
11.446265	828.996314	11.572608
11.231493	836.116382	11.577626
11.619967	817.039818	11.582643
11.440131	837.804145	11.587661
11.425223	831.666426	11.592679
11.389375	828.586678	11.597696
11.308153	824.171378	11.602714
11.692914	825.692838	11.607731
11.466318	823.014397	11.612749
11.500057	825.036562	11.617767
11.282305	833.167975	11.622784
11.216082	822.274644	11.627802
11.216826	818.861182	11.632819
11.341501	838.557052	11.637837
11.962282	828.741998	11.642855
11.797957	816.130499	11.647872
11.400152	822.793240	11.652890
11.426928	828.676657	11.657907
11.377223	840.220242	11.662925
11.393179	842.428961	11.667943
11.719950	824.778944	11.672960
11.631345	828.047282	11.677978
11.905235	805.465698	11.682995
11.332550	832.448225	11.688013
11.298583	826.835862	11.693031
11.315320	828.179226	11.698048
11.448413	835.758994	11.703066
11.469914	837.210893	11.708083
11.396442	854.820304	11.713101
11.759431	844.413657	11.718119
11.673063	859.583131	11.723136
11.676070	860.068756	11.728154
11.835986	858.224823	11.733171
11.796630	856.636695	11.738189
11.977248	854.008345	11.743207
12.003062	852.429128	11.748224
11.734349	869.603029	11.753242
11.873018	865.865563	11.758259
11.595395	849.712569	11.763277
11.876749	848.315080	11.768295
11.983979	856.217356	11.773312
11.753361	859.312075	11.778330
11.872213	852.789544	11.783347
11.925238	857.765919	11.788365
11.794718	859.556639	11.793383
11.940271	843.478663	11.798400
12.031947	853.284483	11.803418
11.891079	843.995475	11.808435
11.573232	829.534730	11.813453
11.822792	846.367416	11.818471
11.653404	851.618965	11.823488
11.811923	874.509630	11.828506
12.005090	845.541425	11.833523
11.857478	857.300264	11.838541
11.876228	855.912026	11.843559
11.960421	861.446883	11.848576
11.293281	854.107637	11.853594
11.798821	835.730610	11.858611
11.618982	850.446748	11.863629
11.600946	860.515914	11.868647
11.857480	856.587364	11.873664
11.900327	876.666197	11.878682
12.451010	864.117260	11.883699
11.985416	858.489623	11.888717
11.966742	861.243492	11.893735
12.181130	849.497583	11.898752
12.050354	868.558522	11.903770
12.344024	874.623876	11.908787
12.366528	850.027514	11.913805
12.177313	829.890995	11.918823
12.260560	836.859676	11.923840
11.706869	865.643174	11.928858
12.044795	854.984331	11.933875
11.957153	848.511473	11.938893
12.143787	859.066266	11.943911
12.158098	883.517773	11.948928
12.210292	885.611582	11.953946
12.531514	872.230607	11.958963
12.557996	853.393398	11.963981
12.293840	845.503830	11.968999
12.007571	853.278760	11.974016
12.038106	853.786010	11.979034
12.269119	837.238131	11.984051
12.203053	851.272552	11.989069
12.303483	871.389193	11.994087
12.309209	874.444170	11.999104
12.288836	873.083158	12.004122
12.451893	855.330764	12.009139
12.502311	852.471143	12.014157
12.276138	856.794332	12.019175
12.110649	851.997286	12.024192
12.340779	862.272425	12.029210
12.770033	875.704876	12.034227
12.328177	859.593969	12.039245
12.130821	845.739707	12.044263
12.604481	847.635844	12.049280
12.551706	862.875537	12.054298
12.502775	862.414680	12.059315
12.505837	871.737059	12.064333
12.070689	858.841231	12.069351
12.076006	835.120044	12.074368
12.189570	879.297488	12.079386
12.258744	877.007349	12.084403
12.162175	871.636161	12.089421
12.155498	874.051130	12.094439
12.388601	875.363270	12.099456
12.081025	884.203369	12.104474
11.843418	896.931881	12.109491
12.645020	891.884873	12.114509
12.924470	894.013649	12.119527
12.599262	885.287715	12.124544
12.712239	895.632421	12.129562
12.550018	867.406093	12.134579
12.719178	875.130865	12.139597
12.620585	868.684702	12.144615
12.971665	844.151738	12.149632
12.529484	860.069397	12.154650
12.897257	875.228585	12.159667
12.838402	872.602808	12.164685
12.848244	867.509234	12.169703
12.923844	858.351134	12.174720
12.931839	887.593382	12.179738
12.836701	872.406897	12.184755
12.748958	867.678669	12.189773
12.836886	873.607791	12.194791
12.954609	870.391760	12.199808
12.912179	887.158600	12.204826
12.929893	873.323680	12.209843
13.020285	848.123934	12.214861
12.702678	874.391331	12.219879
12.946204	886.987781	12.224896
12.740219	881.428622	12.229914
12.819603	862.395601	12.234931
12.576013	861.570757	12.239949
12.791471	878.149635	12.244967
13.009661	888.677979	12.249984
12.821093	863.419513	12.255002
12.981251	841.460055	12.260019
12.957978	859.463137	12.265037
12.562366	877.134862	12.270055
12.751995	866.906908	12.275072
12.966499	862.632933	12.280090
12.977467	862.523304	12.285107
12.881963	856.492176	12.290125
12.711019	860.916349	12.295143
13.052567	859.744972	12.300160
12.761922	877.334406	12.305178
12.695387	859.903733	12.310195
13.061174	868.198114	12.315213
13.048221	865.150392	12.320231
12.602039	869.290708	12.325248
12.703624	859.624606	12.330266
12.959938	869.410610	12.335283
13.312543	901.818618	12.340301
12.898603	882.273353	12.345319
12.974261	869.840992	12.350336
12.917910	894.001615	12.355354
13.236859	901.906614	12.360371
13.250532	898.335722	12.365389
12.904462	898.282930	12.370407
13.300823	889.241642	12.375424
13.205312	896.281612	12.380442
13.306605	899.483554	12.385459
13.415761	896.822628	12.390477
13.369598	903.317972	12.395495
13.560825	887.164998	12.400512
13.330731	872.262164	12.405530
13.221965	868.803517	12.410547
13.226328	857.677293	12.415565
12.994210	853.486475	12.420583
13.206211	847.589624	12.425600
13.054728	872.858463	12.430618
13.068689	895.610295	12.435635
12.952592	888.606335	12.440653
13.207835	885.044136	12.445671
13.489822	902.123724	12.450688
13.428147	908.230888	12.455706
13.144671	887.879319	12.460723
13.750841	876.001931	12.465741
13.404193	902.625166	12.470759
13.391720	907.769820	12.475776
13.544648	900.589641	12.480794
13.432600	885.220946	12.485811
13.447591	894.306389	12.490829
13.062337	915.077214	12.495847
13.241829	892.812598	12.500864
13.292933	887.958198	12.505882
13.492859	884.109942	12.510899
13.658058	889.237136	12.515917
13.455926	913.199202	12.520935
13.500730	896.227622	12.525952
13.874978	888.837493	12.530970
13.434748	894.787680	12.535987
13.460051	878.691851	12.541005
13.650383	902.441839	12.546023
13.587568	904.859498	12.551040
13.900318	876.923660	12.556058
13.598011	883.510819	12.561075
13.937846	888.759508	12.566093
13.445141	898.718410	12.571111
14.018266	897.090956	12.576128
13.689036	904.967869	12.581146
13.428899	906.275913	12.586163
13.867389	892.021039	12.591181
13.446183	898.135264	12.596199
13.417549	892.086676	12.601216
13.721239	903.679953	12.606234
13.342787	896.623011	12.611251
13.422589	883.327875	12.616269
13.067758	884.124341	12.621287
13.489726	900.316059	12.626304
13.345780	915.438621	12.631322
13.644113	909.663174	12.636339
13.487730	925.152667	12.641357
13.697816	941.591101	12.646375
13.694472	927.805761	12.651392
13.954216	923.796959	12.656410
14.173461	916.800645	12.661427
14.254574	915.536215	12.666445
13.919298	909.001326	12.671463
13.950536	918.318093	12.676480
14.040158	939.839397	12.681498
13.851560	928.959521	12.686515
14.501086	906.186711	12.691533
14.588332	915.063427	12.696551
14.340713	911.737234	12.701568
14.230117	905.955270	12.706586
14.094541	895.014701	12.711603
14.095609	901.305833	12.716621
13.601238	910.600918	12.721639
13.875863	902.840241	12.726656
13.890627	911.633287	12.731674
13.969514	916.927765	12.736691
14.155725	886.395978	12.741709
14.160617	884.980507	12.746727
13.954707	893.004020	12.751744
13.972366	890.083188	12.756762
13.823402	898.155053	12.761779
14.193850	908.946562	12.766797
14.054783	913.171437	12.771815
14.360175	913.586528	12.776832
14.266240	920.787526	12.781850
13.860976	908.480265	12.786867
14.337994	898.924197	12.791885
14.206269	913.687056	12.796903
14.379807	929.753564	12.801920
14.359151	923.085793	12.806938
14.205439	917.325611	12.811955
14.230787	898.614681	12.816973
13.888922	907.158472	12.821991
14.036106	923.972738	12.827008
14.371126	929.829069	12.832026
14.230101	914.084130	12.837043
14.350411	911.408861	12.842061
14.541371	929.748574	12.847079
14.491599	921.005837	12.852096
14.434217	927.933052	12.857114
14.220861	924.938804	12.862131
14.505709	915.067919	12.867149
14.397670	928.028524	12.872167
14.236858	929.202962	12.877184
14.371804	933.977782	12.882202
14.019458	919.856326	12.887219
14.235477	903.413583	12.892237
14.519930	922.493941	12.897255
14.452372	915.213611	12.902272
14.855556	924.829552	12.907290
14.203339	923.214086	12.912307
14.395760	922.137310	12.917325
14.511401	912.201500	12.922343
14.577802	909.972626	12.927360
14.359936	904.891085	12.932378
14.205711	920.933225	12.937395
14.310984	914.281449	12.942413
14.662269	919.388332	12.947431
14.294845	913.138603	12.952448
14.239098	910.581284	12.957466
14.831435	933.366301	12.962483
14.899088	936.249582	12.967501
14.903800	948.486832	12.972519
14.918751	939.795084	12.977536
14.728141	932.598254	12.982554
14.337606	919.315178	12.987571
14.438466	908.838253	12.992589
14.869236	937.820918	12.997607
14.620289	937.781792	13.002624
15.011313	942.247436	13.007642
14.852606	953.611828	13.012659
14.723016	944.751493	13.017677
14.698025	939.555117	13.022695
14.766854	941.612138	13.027712
15.088810	955.796946	13.032730
15.040236	971.677524	13.037747
15.185664	940.184308	13.042765
14.782875	911.380095	13.047783
14.525048	920.017654	13.052800
14.940445	940.436674	13.057818
14.407437	951.565849	13.062835
14.589877	936.305189	13.067853
14.854292	943.378690	13.072871
14.856959	942.786894	13.077888
15.115324	944.692054	13.082906
14.698371	956.462712	13.087923
15.106763	940.986013	13.092941
14.952555	948.718308	13.097959
14.990911	932.279408	13.102976
14.866266	932.172410	13.107994
14.629920	952.542102	13.113011
14.771582	940.770553	13.118029
14.960409	948.645124	13.123047
14.920881	982.358141	13.128064
15.265007	964.863420	13.133082
15.393802	963.986380	13.138099
15.376196	969.900408	13.143117
15.457685	947.679656	13.148135
15.092355	937.617164	13.153152
15.250016	933.780406	13.158170
15.344238	948.970605	13.163187
15.076045	952.923499	13.168205
15.159226	935.784157	13.173223
14.986951	926.929804	13.178240
15.289806	931.509891	13.183258
15.274498	949.869644	13.188275
15.197609	947.806631	13.193293
15.121140	932.684110	13.198311
15.174269	929.858958	13.203328
15.396053	958.202356	13.208346
15.097320	980.394234	13.213363
15.474757	960.533099	13.218381
15.730638	972.892403	13.223399
15.263380	958.940649	13.228416
15.571378	935.660008	13.233434
15.209917	938.531251	13.238451
15.533018	947.160303	13.243469
15.457361	962.981190	13.248487
15.509082	974.394660	13.253504
15.286834	972.128952	13.258522
15.524077	965.579821	13.263539
15.605528	960.618638	13.268557
15.583816	958.737795	13.273575
15.519522	959.890578	13.278592
15.900049	946.178856	13.283610
15.466147	946.036765	13.288627
15.454020	951.293848	13.293645
15.700610	942.689575	13.298663
15.504260	939.410992	13.303680
15.850822	910.901245	13.308698
15.368871	938.642484	13.313715
15.608913	940.914850	13.318733
15.703155	952.890915	13.323751
15.491981	977.805809	13.328768
15.575106	962.025845	13.333786
15.683802	973.125055	13.338803
15.676166	971.260483	13.343821
15.967811	962.882650	13.348839
15.803410	984.145579	13.353856
15.699943	968.834718	13.358874
15.958371	957.585847	13.363891
15.945911	962.390939	13.368909
15.860973	953.091441	13.373927
15.807452	943.974406	13.378944
15.758287	954.061669	13.383962
15.710721	961.088825	13.388979
15.843780	962.033941	13.393997
16.040358	963.583069	13.399015
15.673534	968.843374	13.404032
16.196202	979.645694	13.409050
15.992580	974.004340	13.414067
15.864649	962.310486	13.419085
16.253358	944.485767	13.424103
15.794088	940.409510	13.429120
16.006482	960.681933	13.434138
16.044497	961.961473	13.439155
15.965218	953.962873	13.444173
16.355443	964.424366	13.449191
15.935647	953.420221	13.454208
15.920315	944.100468	13.459226
15.784969	936.634137	13.464243
16.005241	950.703495	13.469261
16.004413	959.228644	13.474279
15.794628	978.535197	13.479296
15.954598	961.324589	13.484314
15.864643	965.041785	13.489331
15.932382	966.839508	13.494349
16.081157	954.486803	13.499367
15.939574	960.610637	13.504384
15.769701	957.033655	13.509402
16.125714	968.042300	13.514419
15.909903	967.170448	13.519437
16.036248	969.369111	13.524455
16.049376	988.287452	13.529472
16.267444	1011.113574	13.534490
16.570707	1002.335967	13.539507
16.308327	1006.398418	13.544525
16.772171	993.559965	13.549543
16.498777	998.062902	13.554560
16.479566	970.410630	13.559578
16.515570	961.675736	13.564595
16.371556	949.183671	13.569613
16.551770	934.112210	13.574631
16.382646	945.010721	13.579648
16.193621	955.480946	13.584666
16.581147	965.890243	13.589683
16.377369	963.032362	13.594701
16.364603	956.515792	13.599719
16.011039	962.391364	13.604736
16.445379	977.370110	13.609754
16.706131	970.565680	13.614771
16.460029	1000.935094	13.619789
16.600762	992.803191	13.624807
16.678348	985.733822	13.629824
16.455525	987.521803	13.634842
16.836578	995.634348	13.639859
16.536344	992.701283	13.644877
16.678011	986.658561	13.649895
16.832258	980.669064	13.654912
16.545027	988.616914	13.659930
16.878557	992.915643	13.664947
16.919396	984.183086	13.669965
16.869122	958.677255	13.674983
16.368500	943.983680	13.680000
16.364353	963.272369	13.685018
16.793797	981.528750	13.690035
16.581845	993.924250	13.695053
16.773844	986.164884	13.700071
16.722452	978.280431	13.705088
16.792189	993.298584	13.710106
16.757116	1007.837642	13.715123
16.656864	997.848696	13.720141
16.846924	970.728036	13.725159
16.844949	993.733076	13.730176
16.727812	999.452200	13.735194
17.045077	986.981687	13.740211
17.048279	979.526388	13.745229
16.976492	975.784904	13.750247
17.038339	999.889754	13.755264
16.890530	1006.208090	13.760282
17.248934	985.562667	13.765299
16.560731	982.389168	13.770317
16.832952	987.834648	13.775335
16.727747	1011.789411	13.780352
16.564484	996.605303	13.785370
16.940743	987.771854	13.790387
16.978614	1026.541143	13.795405
17.217959	1031.148188	13.800423
17.113292	1032.943906	13.805440
17.219185	1013.887547	13.810458
17.047499	1004.774455	13.815475
16.672737	1026.200002	13.820493
17.214744	1012.803109	13.825511
17.260110	1019.511837	13.830528
17.174346	1026.116015	13.835546
17.166404	1016.431407	13.840563
17.567342	1011.938466	13.845581
17.446402	1022.781222	13.850599
17.415770	1032.183657	13.855616
17.192255	1015.267208	13.860634
17.309240	1019.862982	13.865651
17.211760	1023.512458	13.870669
17.672871	1035.205576	13.875687
17.546398	1024.804514	13.880704
17.403075	999.793817	13.885722
17.672267	990.397793	13.890739
17.512947	994.403948	13.895757
17.468566	989.914419	13.900775
17.557944	978.360581	13.905792
17.484743	971.345165	13.910810
17.629705	978.150306	13.915827
17.413702	977.886402	13.920845
17.723141	982.691639	13.925863
17.325290	969.652284	13.930880
17.455264	978.777718	13.935898
17.177216	990.649628	13.940915
17.615642	1000.715484	13.945933
17.629924	973.605466	13.950951
17.911584	967.618043	13.955968
17.566523	981.632268	13.960986
17.595341	967.857616	13.966003
17.447656	973.986202	13.971021
17.701741	966.453141	13.976039
17.667326	982.224625	13.981056
17.575189	990.839567	13.986074
17.919778	1000.368019	13.991091
17.747581	1002.221633	13.996109
17.443712	1000.651715	14.001127
17.813749	992.646838	14.006144
17.891488	1016.566531	14.011162
18.274449	1011.280698	14.016179
17.513910	996.327246	14.021197
18.002434	990.380905	14.026215
18.029197	990.551270	14.031232
17.516749	1001.734550	14.036250
17.582694	995.420552	14.041267
17.940167	1008.045406	14.046285
17.811590	996.371214	14.051303
17.945763	1015.383214	14.056320
18.034208	1027.222830	14.061338
18.204625	1010.433488	14.066355
17.957279	1005.092974	14.071373
18.200378	1021.217333	14.076391
18.226190	1012.315263	14.081408
17.897266	997.099293	14.086426
18.109462	1003.658651	14.091443
17.936084	1023.229820	14.096461
17.963827	1019.685505	14.101479
17.719616	990.164486	14.106496
17.593671	1010.499874	14.111514
18.048549	1026.542501	14.116531
17.776828	1025.641607	14.121549
18.174674	1002.899445	14.126567
17.788733	1012.906607	14.131584
17.372312	1013.349569	14.136602
17.813470	1020.869542	14.141619
18.097965	1048.816916	14.146637
18.038253	1052.265226	14.151655
18.360986	1031.513460	14.156672
17.778864	1046.638402	14.161690
18.048101	1047.369533	14.166707
18.196611	1038.924193	14.171725
18.271023	1035.710266	14.176743
18.586593	1023.583618	14.181760
18.251175	1032.222550	14.186778
18.231652	1047.411471	14.191795
18.029938	1047.476715	14.196813
18.623460	1050.009699	14.201831
18.912003	1059.401226	14.206848
18.567050	1057.000309	14.211866
18.811943	1030.585264	14.216883
18.430651	1050.431342	14.221901
18.619795	1041.267555	14.226919
18.688539	1035.173495	14.231936
18.387352	1043.234675	14.236954
18.667825	1034.589524	14.241971
18.747384	1022.621632	14.246989
18.658107	1034.865626	14.252007
18.443625	1039.940879	14.257024
18.354770	1042.625986	14.262042
18.487617	1033.702649	14.267059
18.703710	1019.066601	14.272077
18.708229	1043.703008	14.277095
18.763036	1049.486233	14.282112
18.676642	1039.203999	14.287130
18.948530	1013.620657	14.292147
18.805986	1026.294576	14.297165
18.513457	1048.953915	14.302183
18.902971	1036.608987	14.307200
18.907271	1036.089340	14.312218
18.577224	1037.546413	14.317235
18.443263	1049.320758	14.322253
18.892358	1067.119284	14.327271
19.054330	1053.888157	14.332288
18.921976	1050.484436	14.337306
19.205511	1052.173102	14.342323
18.953505	1070.138659	14.347341
18.955570	1069.183761	14.352359
19.042699	1063.585543	14.357376
18.644832	1048.654272	14.362394
19.078719	1065.603850	14.367411
19.354872	1069.558233	14.372429
19.260842	1046.633749	14.377447
19.381395	1038.497776	14.382464
18.590644	1039.049535	14.387482
19.123066	1026.803802	14.392499
19.038490	1057.729561	14.397517
19.040548	1062.200675	14.402535
19.424821	1052.065204	14.407552
19.022382	1052.340740	14.412570
19.234459	1047.613980	14.417587
19.238562	1055.996770	14.422605
19.072431	1057.258787	14.427623
19.232900	1052.995264	14.432640
19.499798	1055.999049	14.437658
19.325844	1063.060718	14.442675
19.427389	1064.291982	14.447693
19.442111	1050.213657	14.452711
19.639776	1043.113004	14.457728
19.305111	1047.421014	14.462746
19.094628	1037.196876	14.467763
19.274219	1031.357857	14.472781
19.446547	1028.239829	14.477799
19.431393	1039.995813	14.482816
19.382564	1066.773708	14.487834
19.330399	1055.601086	14.492851
19.317269	1057.918554	14.497869
19.317709	1055.602453	14.502887
19.649515	1049.779798	14.507904
19.238975	1045.445127	14.512922
19.534787	1049.558421	14.517939
19.443413	1062.113435	14.522957
19.170474	1055.408281	14.527975
19.402040	1046.956887	14.532992
19.417601	1051.994916	14.538010
19.246566	1053.997421	14.543027
19.695211	1048.589602	14.548045
19.694188	1068.241104	14.553063
19.747097	1055.876804	14.558080
19.819305	1074.797593	14.563098
19.677070	1056.100979	14.568115
19.870574	1050.526417	14.573133
19.566133	1045.994435	14.578151
19.731678	1059.526814	14.583168
19.668435	1073.738881	14.588186
19.942278	1065.583762	14.593203
20.055758	1068.803800	14.598221
20.041099	1088.727397	14.603239
20.168390	1057.322841	14.608256
20.103635	1049.933645	14.613274
20.068956	1035.202835	14.618291
20.041264	1035.690193	14.623309
20.139654	1064.002125	14.628327
19.935186	1044.662625	14.633344
20.204660	1041.854148	14.638362
19.940475	1037.812243	14.643379
20.231188	1035.636319	14.648397
19.850816	1041.022773	14.653415
20.037604	1027.465405	14.658432
20.209236	1056.622878	14.663450
20.007934	1033.760814	14.668467
20.215846	1043.947547	14.673485
20.006681	1049.246671	14.678503
20.172764	1024.689869	14.683520
19.424933	1035.707004	14.688538
20.013985	1065.728155	14.693555
20.461561	1060.031113	14.698573
20.213508	1083.153606	14.703591
20.506473	1083.618973	14.708608
20.425198	1075.455423	14.713626
20.227373	1070.261389	14.718643
20.580946	1066.185975	14.723661
20.410918	1058.695106	14.728679
20.199469	1047.066452	14.733696
19.912181	1076.117070	14.738714
20.439134	1074.712137	14.743731
20.591679	1066.527665	14.748749
20.417335	1078.958642	14.753767
20.345405	1082.439383	14.758784
20.365799	1085.571388	14.763802
20.238665	1076.486807	14.768819
20.592912	1076.487041	14.773837
20.286633	1089.072965	14.778855
20.274402	1091.303008	14.783872
20.379381	1093.703793	14.788890
20.075246	1086.158811	14.793907
20.080971	1072.012777	14.798925
20.181338	1089.046524	14.803943
20.690446	1101.938550	14.808960
20.511267	1104.810402	14.813978
20.654231	1096.806981	14.818995
20.940203	1091.940469	14.824013
20.749447	1109.803651	14.829031
20.781039	1102.976712	14.834048
20.994516	1094.538908	14.839066
21.002682	1089.119142	14.844083
21.234910	1096.553162	14.849101
20.945215	1099.301874	14.854119
21.295337	1083.890750	14.859136
20.945446	1089.602614	14.864154
20.819866	1072.428539	14.869171
20.990442	1057.632399	14.874189
20.805231	1057.855112	14.879207
20.672970	1057.175499	14.884224
21.089333	1061.500117	14.889242
20.851427	1059.053760	14.894259
21.285690	1064.929167	14.899277
20.699874	1064.292623	14.904295
21.293417	1080.189416	14.909312
21.030930	1073.890594	14.914330
20.712156	1061.126309	14.919347
20.902654	1080.496733	14.924365
20.997926	1095.375268	14.929383
21.007804	1088.318124	14.934400
21.373383	1076.247819	14.939418
21.527749	1101.940491	14.944435
21.720154	1101.857162	14.949453
21.252966	1088.093125	14.954471
20.878339	1056.098846	14.959488
21.347399	1084.118221	14.964506
21.464885	1094.647606	14.969523
21.524557	1087.646883	14.974541
21.011096	1098.437288	14.979559
20.977886	1089.125912	14.984576
21.450067	1086.930325	14.989594
21.224211	1105.091847	14.994611
21.473282	1110.261640	14.999629
21.235900	1099.056912	15.004647
21.621800	1094.425890	15.009664
21.646718	1102.171859	15.014682
21.257071	1104.721197	15.019699
21.646214	1090.080494	15.024717
21.407838	1114.468151	15.029735
21.580579	1096.392205	15.034752
21.862604	1082.854572	15.039770
21.357446	1090.301022	15.044787
21.289482	1106.570085	15.049805
21.437375	1091.417415	15.054823
21.135634	1095.533724	15.059840
21.389337	1089.544379	15.064858
21.368094	1090.773304	15.069875
21.729857	1121.440932	15.074893
21.679752	1119.568501	15.079911
21.875633	1125.687606	15.084928
22.097423	1118.355821	15.089946
21.784711	1125.394988	15.094963
21.801655	1124.515364	15.099981
21.808795	1107.905591	15.104999
21.748310	1104.878173	15.110016
21.957201	1115.814608	15.115034
22.029963	1104.590408	15.120051
22.196214	1110.047539	15.125069
22.188042	1103.259053	15.130087
22.050597	1095.140888	15.135104
21.947813	1081.655137	15.140122
21.978122	1087.604196	15.145139
21.758750	1100.081992	15.150157
21.835406	1121.186015	15.155175
22.345585	1107.296266	15.160192
22.015689	1123.485434	15.165210
21.847000	1139.769799	15.170227
22.214288	1135.306270	15.175245
22.213305	1126.545905	15.180263
22.040263	1120.115284	15.185280
21.976802	1125.737811	15.190298
21.787062	1136.643703	15.195315
22.006930	1116.613471	15.200333
21.996118	1119.559545	15.205351
22.102155	1105.704209	15.210368
22.185717	1108.062188	15.215386
22.248181	1122.954339	15.220403
22.187545	1123.021461	15.225421
22.143972	1107.430550	15.230439
22.168189	1108.592727	15.235456
22.456523	1132.008452	15.240474
22.364547	1165.861709	15.245491
22.598593	1153.977410	15.250509
22.670958	1144.947988	15.255527
22.694839	1137.698592	15.260544
22.470784	1129.873590	15.265562
22.237539	1145.847645	15.270579
22.709687	1132.238108	15.275597
22.897528	1140.664579	15.280615
22.455836	1119.485116	15.285632
22.632480	1120.663926	15.290650
22.545369	1136.314388	15.295667
22.821690	1137.792300	15.300685
22.716557	1123.086627	15.305703
22.738007	1119.840008	15.310720
22.910188	1111.534776	15.315738
22.391995	1124.391715	15.320755
22.689172	1147.152421	15.325773
22.959681	1142.464292	15.330791
22.691032	1133.072828	15.335808
22.816745	1149.298221	15.340826
22.651507	1145.698682	15.345843
22.675467	1136.099944	15.350861
22.744553	1145.100139	15.355879
22.389648	1157.765004	15.360896
23.027216	1151.249223	15.365914
22.770140	1149.171481	15.370931
22.947949	1151.454360	15.375949
22.889777	1147.150976	15.380967
22.830016	1130.918581	15.385984
23.089640	1143.997112	15.391002
22.876321	1146.981083	15.396019
23.010366	1145.805108	15.401037
23.156824	1143.660584	15.406055
23.305603	1172.087981	15.411072
23.314689	1142.974774	15.416090
22.872444	1126.134199	15.421107
23.447920	1147.116171	15.426125
23.325397	1155.572683	15.431143
23.376110	1153.544350	15.436160
23.439825	1150.294479	15.441178
23.059726	1153.026258	15.446195
23.065544	1138.420219	15.451213
23.423435	1136.412565	15.456231
23.368864	1163.607226	15.461248
23.604566	1175.977803	15.466266
23.628824	1171.025019	15.471283
23.471914	1131.866702	15.476301
23.494115	1126.207948	15.481319
23.143699	1145.768998	15.486336
23.515413	1152.444938	15.491354
23.282609	1152.775591	15.496371
23.372171	1154.645303	15.501389
23.475895	1171.693446	15.506407
23.645477	1156.496684	15.511424
23.729671	1143.879663	15.516442
23.642384	1162.982688	15.521459
23.735434	1178.682831	15.526477
23.875625	1156.725139	15.531495
23.680768	1152.125914	15.536512
24.068484	1144.115183	15.541530
23.893815	1154.801622	15.546547
23.824130	1146.597447	15.551565
23.819098	1152.891364	15.556583
23.789857	1161.140188	15.561600
24.153631	1145.123645	15.566618
23.774572	1132.259741	15.571635
23.756690	1124.255038	15.576653
23.558598	1125.511223	15.581671
23.716685	1132.191263	15.586688
24.091724	1149.759763	15.591706
24.099165	1169.650490	15.596723
24.115855	1169.474869	15.601741
24.353167	1173.672649	15.606759
24.309110	1171.237734	15.611776
24.256617	1136.665466	15.616794
24.217091	1123.861575	15.621811
23.867673	1127.890126	15.626829
24.082226	1117.191661	15.631847
23.816353	1112.192868	15.636864
23.901351	1139.456328	15.641882
23.909902	1170.089729	15.646899
24.236866	1157.916615	15.651917
24.367939	1133.209654	15.656935
24.043800	1157.874776	15.661952
24.097589	1169.026106	15.666970
24.361421	1164.900650	15.671987
24.348261	1147.190617	15.677005
24.511182	1161.838899	15.682023
24.351469	1147.315606	15.687040
24.530978	1147.024617	15.692058
24.345056	1151.505370	15.697075
24.218335	1146.250457	15.702093
24.219540	1159.024250	15.707111
23.956845	1171.509952	15.712128
24.329699	1144.285468	15.717146
24.479657	1152.450948	15.722163
24.368319	1175.179721	15.727181
24.681100	1172.073780	15.732199
24.519357	1171.775615	15.737216
24.898611	1182.642519	15.742234
24.387351	1187.534734	15.747251
24.457300	1163.689097	15.752269
24.698058	1156.931776	15.757287
24.465229	1180.873553	15.762304
24.494487	1178.857420	15.767322
24.701226	1177.132158	15.772339
24.881283	1166.771858	15.777357
25.102604	1170.032251	15.782375
24.837968	1171.440445	15.787392
25.131188	1163.248813	15.792410
24.901333	1182.364203	15.797427
24.451041	1198.100526	15.802445
24.865379	1168.233163	15.807463
24.789926	1165.581443	15.812480
24.801594	1162.820665	15.817498
24.683652	1178.670313	15.822515
24.976999	1199.275852	15.827533
25.475875	1195.199026	15.832551
24.975644	1196.757152	15.837568
25.181986	1196.590437	15.842586
25.606831	1188.080162	15.847603
25.204690	1176.096400	15.852621
25.370889	1178.768804	15.857639
24.816922	1179.234204	15.862656
25.529726	1168.966924	15.867674
25.591228	1173.849701	15.872691
25.416058	1178.284109	15.877709
25.415010	1158.789815	15.882727
25.306096	1163.190736	15.887744
25.383405	1182.033669	15.892762
25.174752	1171.891992	15.897779
25.277157	1163.224141	15.902797
25.585771	1166.434388	15.907815
25.459286	1168.148413	15.912832
25.339612	1176.745968	15.917850
25.464507	1175.418488	15.922867
25.253416	1159.730334	15.927885
25.843416	1183.887632	15.932903
25.384261	1190.110089	15.937920
25.609583	1190.813551	15.942938
25.847978	1179.993218	15.947955
25.574583	1183.839084	15.952973
25.550841	1174.517726	15.957991
25.363065	1181.168054	15.963008
25.419837	1197.040412	15.968026
25.734936	1203.487205	15.973043
25.510101	1210.215994	15.978061
26.009719	1196.733915	15.983079
25.752367	1199.527780	15.988096
25.681508	1190.871030	15.993114
25.893900	1198.421539	15.998131
25.706322	1209.869121	16.003149
26.182825	1202.737273	16.008167
25.891355	1200.836821	16.013184
25.939776	1185.397222	16.018202
26.022432	1204.103996	16.023219
25.783891	1193.370931	16.028237
26.273172	1186.311567	16.033255
25.919938	1192.612758	16.038272
26.099933	1193.180733	16.043290
26.094227	1198.903460	16.048307
26.102611	1210.355856	16.053325
26.020218	1197.510180	16.058343
26.011401	1198.070389	16.063360
25.988638	1185.672043	16.068378
26.337056	1200.575368	16.073395
26.250387	1234.349967	16.078413
26.304334	1216.273141	16.083431
26.514314	1214.099906	16.088448
26.368834	1215.600984	16.093466
26.505968	1207.519255	16.098483
26.424470	1211.794429	16.103501
26.614941	1212.420207	16.108519
26.404366	1213.152406	16.113536
26.309244	1189.964858	16.118554
26.598518	1207.189318	16.123571
26.316022	1224.185032	16.128589
27.074225	1219.369743	16.133607
26.528064	1204.814314	16.138624
26.658978	1192.137774	16.143642
26.688166	1188.318050	16.148659
26.677494	1218.768058	16.153677
26.899139	1211.983858	16.158695
26.630977	1186.871835	16.163712
26.581053	1191.732096	16.168730
27.121912	1207.839354	16.173747
26.683364	1204.497808	16.178765
26.592018	1181.959887	16.183783
26.744569	1200.216925	16.188800
26.782797	1221.248616	16.193818
26.697167	1215.536997	16.198835
26.817102	1208.664218	16.203853
26.958228	1183.064193	16.208871
26.877165	1217.264202	16.213888
26.905709	1207.730295	16.218906
27.497943	1198.883471	16.223923
26.861105	1221.997506	16.228941
27.167945	1208.466683	16.233959
27.048694	1205.588981	16.238976
26.836219	1215.571251	16.243994
26.938850	1214.526317	16.249011
26.827107	1228.628854	16.254029
26.984433	1202.057454	16.259047
26.786316	1199.206169	16.264064
27.126089	1203.315882	16.269082
27.256983	1211.378467	16.274099
27.030745	1228.514854	16.279117
27.408242	1229.628008	16.284135
27.922510	1226.452254	16.289152
27.480138	1217.431884	16.294170
27.358428	1214.456874	16.299187
27.040270	1214.121481	16.304205
27.429866	1212.514190	16.309223
27.523638	1229.671497	16.314240
27.437496	1243.213651	16.319258
27.942027	1248.419603	16.324275
27.822853	1230.769109	16.329293
27.513530	1218.001950	16.334311
27.824765	1210.238019	16.339328
27.594849	1193.760611	16.344346
28.166221	1175.427109	16.349363
27.614716	1214.838949	16.354381
27.767700	1216.193780	16.359399
27.756928	1193.591259	16.364416
27.549218	1194.441361	16.369434
27.934180	1208.458355	16.374451
27.597457	1197.382444	16.379469
27.896647	1186.524113	16.384487
28.109337	1194.265767	16.389504
27.870330	1203.347512	16.394522
27.637264	1199.287628	16.399539
27.694544	1229.365392	16.404557
28.289009	1232.115326	16.409575
28.213603	1229.389196	16.414592
28.095729	1236.531223	16.419610
28.116243	1243.305584	16.424627
28.454570	1232.725135	16.429645
27.770183	1217.328273	16.434663
27.995043	1251.232684	16.439680
28.062688	1243.942156	16.444698
28.290367	1217.503655	16.449715
28.157951	1229.793803	16.454733
28.445772	1244.764455	16.459751
28.650379	1231.939909	16.464768
28.323322	1231.702616	16.469786
28.696104	1220.211776	16.474803
28.423578	1230.061198	16.479821
28.366602	1212.792183	16.484839
28.029652	1201.103756	16.489856
28.093382	1235.106887	16.494874
28.364352	1235.468143	16.499891
28.323911	1225.959008	16.504909
28.493837	1209.928968	16.509927
28.443911	1206.191195	16.514944
28.184718	1229.927613	16.519962
28.390541	1229.596357	16.524979
28.174263	1225.586928	16.529997
28.342226	1229.733797	16.535015
28.745327	1258.004001	16.540032
28.482933	1265.245300	16.545050
28.668118	1253.174950	16.550067
28.891536	1242.753115	16.555085
28.768150	1255.695967	16.560103
28.915485	1257.966186	16.565120
28.648986	1253.585708	16.570138
28.944745	1231.999153	16.575155
28.861375	1238.471956	16.580173
28.510571	1269.117608	16.585191
28.768458	1250.434045	16.590208
29.065909	1233.930061	16.595226
29.119732	1215.405430	16.600243
28.960003	1246.457447	16.605261
29.194786	1249.718192	16.610279
29.264781	1246.513807	16.615296
29.531466	1227.245098	16.620314
29.286384	1238.838491	16.625331
29.422113	1259.649055	16.630349
29.353273	1251.115824	16.635367
29.260636	1228.620655	16.640384
29.353088	1244.594326	16.645402
29.468446	1235.738116	16.650419
29.390620	1240.183221	16.655437
29.240060	1257.980696	16.660455
29.583485	1241.591519	16.665472
29.265735	1230.118349	16.670490
29.776282	1225.897788	16.675507
29.741125	1233.232985	16.680525
29.619934	1240.939110	16.685543
29.755165	1241.478469	16.690560
29.441348	1239.974722	16.695578
29.555576	1236.972330	16.700595
29.801739	1235.098552	16.705613
29.107145	1230.061537	16.710631
29.371620	1237.079273	16.715648
29.367889	1259.562294	16.720666
29.444638	1252.813927	16.725683
29.463217	1226.520470	16.730701
29.393784	1239.911666	16.735719
29.619125	1260.666389	16.740736
29.615961	1287.068314	16.745754
29.590287	1278.441833	16.750771
29.732569	1263.200768	16.755789
29.576445	1264.896282	16.760807
29.763090	1273.872599	16.765824
29.438258	1282.367829	16.770842
29.896617	1284.265470	16.775859
30.139968	1300.352222	16.780877
30.239846	1289.463680	16.785895
30.734978	1286.623282	16.790912
30.228452	1282.084377	16.795930
30.278159	1273.300988	16.800947
30.210487	1261.722999	16.805965
30.579960	1263.852498	16.810983
30.657799	1260.551955	16.816000
30.111188	1275.970298	16.821018
30.236336	1265.981321	16.826035
30.242211	1252.563762	16.831053
30.044490	1243.689812	16.836071
30.439345	1251.964743	16.841088
30.129402	1273.262457	16.846106
30.573824	1294.686762	16.851123
30.568469	1288.406763	16.856141
30.148258	1296.136940	16.861159
30.602376	1289.807974	16.866176
30.323640	1291.857336	16.871194
30.524306	1296.158624	16.876211
30.684621	1309.666899	16.881229
30.466839	1308.248334	16.886247
30.721697	1283.963583	16.891264
30.466338	1288.187802	16.896282
30.740372	1287.096729	16.901299
30.598224	1281.952167	16.906317
30.558361	1286.859701	16.911335
30.988511	1293.589517	16.916352
30.526746	1297.056104	16.921370
30.702135	1288.680282	16.926387
30.912607	1276.850461	16.931405
30.807113	1305.692677	16.936423
31.176202	1307.132545	16.941440
31.185485	1307.985368	16.946458
31.168612	1303.864933	16.951475
30.970954	1299.354885	16.956493
31.016030	1301.410664	16.961511
31.185362	1296.159914	16.966528
31.369724	1313.696250	16.971546
31.382530	1317.813875	16.976563
31.506964	1306.676831	16.981581
31.123360	1287.930075	16.986599
31.307912	1261.212275	16.991616
31.146358	1280.689642	16.996634
31.232396	1302.879611	17.001651
31.575564	1312.692188	17.006669
31.643112	1305.868959	17.011687
31.549261	1293.492998	17.016704
31.330217	1309.596835	17.021722
31.187807	1323.962735	17.026739
31.446632	1309.918127	17.031757
31.710551	1313.004425	17.036775
31.811634	1328.010347	17.041792
31.511698	1323.310450	17.046810
31.536758	1314.912911	17.051827
31.590651	1313.487730	17.056845
31.290631	1316.243106	17.061863
31.584739	1298.438923	17.066880
31.291791	1320.426350	17.071898
31.649676	1303.480024	17.076915
31.579620	1320.363985	17.081933
31.645146	1322.975314	17.086951
31.985508	1310.278431	17.091968
32.027894	1316.411465	17.096986
32.067699	1332.824930	17.102003
32.195798	1345.766645	17.107021
32.299738	1329.043808	17.112039
31.972951	1300.351958	17.117056
32.113021	1319.686935	17.122074
32.033853	1336.358395	17.127091
32.335865	1320.917196	17.132109
32.304998	1309.962666	17.137127
32.414917	1323.050838	17.142144
32.261008	1322.341431	17.147162
32.187389	1314.994506	17.152179
32.322461	1302.715126	17.157197
32.214992	1308.105284	17.162215
32.108115	1330.439843	17.167232
32.233407	1334.571357	17.172250
31.765396	1320.096976	17.177267
32.287820	1336.124857	17.182285
31.816208	1333.797175	17.187303
32.369382	1327.447494	17.192320
32.286801	1347.378127	17.197338
32.208490	1356.060658	17.202355
32.729424	1363.196665	17.207373
32.626471	1365.886815	17.212391
33.000888	1340.462887	17.217408
32.941637	1346.071515	17.222426
32.775547	1361.906972	17.227443
33.128139	1368.277774	17.232461
32.964169	1351.907183	17.237479
32.974653	1358.268683	17.242496
33.138449	1338.151288	17.247514
32.998825	1343.197247	17.252531
32.953745	1333.069269	17.257549
33.062440	1310.418002	17.262567
33.197165	1308.542655	17.267584
33.169400	1332.075180	17.272602
33.025292	1329.896973	17.277619
33.178942	1308.903937	17.282637
33.040459	1314.450959	17.287655
33.100146	1319.220231	17.292672
33.176885	1318.225031	17.297690
33.206993	1305.366282	17.302707
33.504299	1319.360077	17.307725
32.996209	1334.384211	17.312743
32.903387	1323.953767	17.317760
33.381028	1322.455509	17.322778
33.527600	1339.587586	17.327795
33.577944	1346.087440	17.332813
33.218692	1366.579643	17.337831
33.560723	1356.456267	17.342848
33.510761	1343.531700	17.347866
33.546151	1353.573667	17.352883
33.647274	1352.590179	17.357901
33.546308	1341.754863	17.362919
33.504106	1344.151866	17.367936
33.431336	1346.668068	17.372954
33.739009	1341.132297	17.377971
33.468815	1334.055194	17.382989
33.522430	1344.200417	17.388007
33.851528	1332.647043	17.393024
33.714357	1351.816113	17.398042
33.695804	1358.844168	17.403059
34.342174	1357.533231	17.408077
33.608071	1348.291368	17.413095
33.595812	1356.297095	17.418112
34.045149	1377.297376	17.423130
33.788387	1381.727023	17.428147
34.083324	1371.913122	17.433165
34.115961	1373.701933	17.438183
34.433794	1384.315019	17.443200
34.336493	1396.917536	17.448218
34.076493	1378.852839	17.453235
34.312068	1362.447013	17.458253
34.560443	1390.685467	17.463271
34.095410	1361.492942	17.468288
34.312225	1363.315378	17.473306
34.327110	1383.081166	17.478323
34.656137	1364.308363	17.483341
34.407196	1368.356584	17.488359
34.359852	1359.747710	17.493376
34.266071	1381.673285	17.498394
34.119198	1397.063380	17.503411
34.190620	1377.999643	17.508429
34.505995	1372.264700	17.513447
34.214273	1372.953242	17.518464
34.213924	1389.038145	17.523482
34.516833	1396.457582	17.528499
35.039924	1390.778445	17.533517
35.021377	1399.071290	17.538535
34.884994	1401.433187	17.543552
35.142613	1393.364907	17.548570
35.132627	1403.661789	17.553587
35.173909	1373.553577	17.558605
35.243497	1353.127099	17.563623
35.020061	1370.780780	17.568640
34.570040	1375.552428	17.573658
34.596617	1373.778587	17.578675
35.358466	1373.373059	17.583693
35.382223	1394.033746	17.588711
35.143326	1391.144980	17.593728
35.388154	1398.316299	17.598746
34.999733	1376.339468	17.603763
35.387345	1377.127414	17.608781
35.493872	1393.128337	17.613799
35.328405	1386.669094	17.618816
35.421123	1356.685750	17.623834
35.106579	1352.125825	17.628851
35.305583	1387.946087	17.633869
35.555923	1401.421165	17.638887
35.510428	1398.612028	17.643904
35.789547	1384.094616	17.648922
35.484087	1397.948282	17.653939
35.590335	1402.902166	17.658957
35.513375	1402.525925	17.663975
35.252858	1391.932639	17.668992
35.605154	1397.804108	17.674010
35.317119	1393.540508	17.679027
35.512356	1385.686333	17.684045
35.573266	1396.568899	17.689063
35.756065	1408.516517	17.694080
35.956194	1399.940528	17.699098
35.838131	1391.429523	17.704115
35.617882	1381.951971	17.709133
35.949475	1382.234726	17.714151
36.113779	1393.211891	17.719168
36.040959	1402.493011	17.724186
35.757024	1410.175633	17.729203
36.394705	1418.539239	17.734221
36.139955	1418.959331	17.739239
36.313217	1418.277037	17.744256
36.338962	1409.798347	17.749274
36.407069	1426.664318	17.754291
36.516109	1415.598424	17.759309
36.462681	1390.399607	17.764327
36.283866	1401.615129	17.769344
36.660513	1410.419906	17.774362
36.210195	1399.704076	17.779379
36.271834	1417.128558	17.784397
36.260721	1409.060986	17.789415
36.456692	1409.653391	17.794432
36.701893	1402.879975	17.799450
36.548938	1416.331771	17.804467
36.753620	1428.896319	17.809485
36.630038	1418.551289	17.814503
36.466855	1398.754618	17.819520
36.840563	1402.772675	17.824538
36.687502	1392.808433	17.829555
36.545018	1399.633515	17.834573
36.632094	1404.962923	17.839591
36.831660	1406.161289	17.844608
37.122804	1395.092575	17.849626
36.713483	1415.291415	17.854643
36.663622	1415.273212	17.859661
36.932963	1415.573635	17.864679
37.066343	1451.742413	17.869696
37.284545	1430.123523	17.874714
37.268180	1434.153304	17.879731
37.323585	1449.554898	17.884749
37.455349	1445.798063	17.889767
37.075175	1439.993528	17.894784
37.395293	1426.761137	17.899802
36.746730	1432.539605	17.904819
37.233684	1434.789350	17.909837
37.176653	1442.767193	17.914855
37.069298	1434.918715	17.919872
37.291951	1430.131245	17.924890
37.334986	1455.673755	17.929907
37.128629	1438.524819	17.934925
37.339096	1434.359892	17.939943
37.467900	1450.699637	17.944960
37.667558	1456.222420	17.949978
37.523673	1456.885354	17.954995
37.618863	1467.124554	17.960013
38.294438	1449.308034	17.965031
38.016516	1445.643795	17.970048
38.086643	1448.935925	17.975066
37.853143	1454.113746	17.980083
37.783589	1458.763505	17.985101
38.279338	1448.967639	17.990119
37.980911	1447.061120	17.995136
38.329493	1446.142321	18.000154
38.210417	1431.836597	18.005171
37.991282	1418.434426	18.010189
38.280816	1417.454831	18.015207
37.847711	1428.124830	18.020224
38.235932	1429.593333	18.025242
38.232733	1428.650304	18.030259
38.260074	1447.066486	18.035277
38.492240	1463.552218	18.040295
38.539513	1468.016668	18.045312
38.480025	1442.440308	18.050330
38.278307	1444.068096	18.055347
38.190395	1452.956259	18.060365
38.585499	1440.811120	18.065383
38.386721	1452.321646	18.070400
38.746981	1440.081894	18.075418
38.459725	1451.197191	18.080435
38.259890	1473.548993	18.085453
38.361536	1456.166404	18.090471
38.366697	1453.388148	18.095488
38.475677	1441.778469	18.100506
38.474982	1468.265123	18.105523
38.567113	1471.351206	18.110541
38.869772	1497.960087	18.115559
38.952784	1493.197937	18.120576
39.312655	1479.639120	18.125594
39.147085	1484.163939	18.130611
38.919436	1503.732907	18.135629
39.218031	1492.212892	18.140647
39.006344	1487.914706	18.145664
38.828108	1478.813630	18.150682
38.813349	1494.111436	18.155699
38.673986	1480.911236	18.160717
38.904430	1477.068220	18.165735
38.950296	1483.346973	18.170752
39.198246	1501.407938	18.175770
39.471328	1513.569902	18.180787
39.457382	1500.234911	18.185805
39.465824	1486.431570	18.190823
39.257187	1499.178133	18.195840
39.443461	1501.087110	18.200858
39.538706	1511.882311	18.205875
39.493714	1505.441978	18.210893
40.001037	1492.454223	18.215911
39.565896	1492.820188	18.220928
39.695940	1501.230727	18.225946
39.916976	1499.855548	18.230963
39.566396	1491.895002	18.235981
39.733612	1484.766704	18.240999
39.586584	1509.305802	18.246016
39.828781	1497.214326	18.251034
39.972081	1495.416459	18.256051
40.123994	1497.137062	18.261069
40.033549	1481.186076	18.266087
40.030449	1490.926196	18.271104
40.081597	1503.220769	18.276122
40.028495	1514.483400	18.281139
40.110038	1513.543090	18.286157
40.750804	1494.953995	18.291175
40.482350	1490.639603	18.296192
40.200586	1496.615593	18.301210
40.215988	1493.614526	18.306227
40.299788	1485.429283	18.311245
40.509796	1491.843675	18.316263
40.054288	1510.322996	18.321280
40.298891	1514.977538	18.326298
40.431761	1504.450830	18.331315
40.320241	1513.423128	18.336333
40.461524	1513.725919	18.341351
40.394025	1532.784019	18.346368
40.492793	1515.621672	18.351386
40.603173	1501.892791	18.356403
40.720088	1507.894125	18.361421
40.630126	1533.268134	18.366439
40.626107	1525.601013	18.371456
40.965157	1525.115482	18.376474
41.058377	1524.006250	18.381491
41.096054	1542.056057	18.386509
41.125482	1539.786656	18.391527
41.344527	1546.846583	18.396544
41.288055	1523.389699	18.401562
41.304972	1514.906998	18.406579
40.844011	1526.989037	18.411597
41.267225	1511.769789	18.416615
41.055378	1532.562292	18.421632
41.434030	1537.071193	18.426650
41.695526	1549.588961	18.431667
41.638603	1542.108684	18.436685
41.660389	1522.424267	18.441703
41.480804	1512.495622	18.446720
41.251107	1497.566328	18.451738
41.542179	1514.018666	18.456755
41.504450	1531.940007	18.461773
41.583328	1515.919871	18.466791
41.702053	1528.419786	18.471808
41.519704	1543.069006	18.476826
41.909881	1531.392324	18.481843
41.630518	1517.795338	18.486861
42.007356	1508.168362	18.491879
41.666803	1510.179651	18.496896
41.514064	1513.739872	18.501914
42.056010	1522.857777	18.506931
42.037586	1539.246252	18.511949
42.194169	1540.266437	18.516967
41.857134	1525.794915	18.521984
41.907042	1516.392788	18.527002
41.972336	1533.381559	18.532019
41.535582	1551.795933	18.537037
42.004323	1545.978804	18.542055
42.028851	1556.550537	18.547072
41.981881	1556.929999	18.552090
42.125866	1551.230004	18.557107
42.454929	1548.992369	18.562125
42.411106	1551.930991	18.567143
42.527775	1559.262216	18.572160
42.417993	1560.820407	18.577178
42.518764	1558.785125	18.582195
42.311790	1572.829422	18.587213
42.467281	1568.493956	18.592231
42.424469	1577.866070	18.597248
42.987870	1579.970359	18.602266
43.036736	1594.131616	18.607283
42.883338	1593.589595	18.612301
43.181102	1581.745999	18.617319
42.826596	1570.802844	18.622336
42.636377	1551.494393	18.627354
43.026156	1571.011900	18.632371
42.888141	1574.562813	18.637389
43.103727	1557.236659	18.642407
43.200429	1571.562196	18.647424
43.388580	1578.918913	18.652442
43.334247	1582.487292	18.657459
42.977488	1575.594620	18.662477
43.328578	1581.406432	18.667495
43.235500	1582.824001	18.672512
42.995760	1587.250008	18.677530
43.271937	1574.342203	18.682547
43.186526	1583.260041	18.687565
43.456284	1583.900385	18.692583
43.533598	1567.384202	18.697600
43.557751	1566.736973	18.702618
43.498474	1584.168342	18.707635
43.028566	1582.078279	18.712653
43.628930	1577.884801	18.717671
43.706549	1596.592003	18.722688
43.629769	1613.780189	18.727706
43.652788	1600.831536	18.732723
43.649635	1598.224868	18.737741
43.809506	1598.725137	18.742759
44.174559	1604.730278	18.747776
43.748238	1606.373452	18.752794
44.062453	1589.359928	18.757811
43.768985	1597.766209	18.762829
43.911592	1594.156235	18.767847
44.088868	1601.104906	18.772864
43.989582	1593.128464	18.777882
44.348513	1620.837472	18.782899
44.355771	1613.289578	18.787917
44.825014	1619.467133	18.792935
44.741661	1614.752315	18.797952
44.607736	1602.546175	18.802970
44.572693	1592.499813	18.807987
44.260003	1588.609248	18.813005
44.397431	1594.438660	18.818023
44.555688	1603.440430	18.823040
44.542702	1617.006644	18.828058
44.803997	1631.110001	18.833075
44.659709	1630.145303	18.838093
44.639570	1629.378252	18.843111
44.745621	1628.903668	18.848128
44.499326	1621.273975	18.853146
44.685500	1604.863556	18.858163
44.432626	1628.229842	18.863181
44.808221	1629.417047	18.868199
44.815670	1615.526470	18.873216
44.919565	1632.656185	18.878234
45.526296	1653.874489	18.883251
45.153475	1666.531908	18.888269
45.249544	1662.701211	18.893287
45.530070	1643.527605	18.898304
45.391498	1647.920281	18.903322
45.617915	1643.818692	18.908339
45.427460	1651.628083	18.913357
45.588906	1635.087789	18.918375
45.658665	1627.152573	18.923392
45.701859	1641.943221	18.928410
45.700737	1625.108709	18.933427
45.407350	1620.005655	18.938445
45.431986	1611.935020	18.943463
45.669398	1623.037642	18.948480
45.613752	1642.932719	18.953498
46.097403	1632.702410	18.958515
46.047176	1639.288384	18.963533
45.693685	1644.004505	18.968551
46.133895	1630.135295	18.973568
45.743996	1629.794328	18.978586
45.987189	1641.378681	18.983603
45.878086	1641.903718	18.988621
45.591555	1646.804797	18.993639
46.087064	1622.113284	18.998656
45.998321	1625.243655	19.003674
45.983084	1631.069279	19.008691
46.218591	1643.783602	19.013709
46.043482	1644.271132	19.018727
46.405583	1637.551509	19.023744
46.219265	1667.128673	19.028762
46.506989	1660.629161	19.033779
46.496243	1646.586772	19.038797
46.303997	1671.763687	19.043815
46.587398	1678.505034	19.048832
46.615524	1680.441152	19.053850
46.833132	1656.870577	19.058867
47.056913	1655.810908	19.063885
46.790369	1662.288672	19.068903
46.969935	1663.222212	19.073920
46.667869	1661.388496	19.078938
46.867983	1667.192324	19.083955
46.874630	1668.854587	19.088973
46.812617	1655.700989	19.093991
46.898655	1640.945120	19.099008
46.588267	1659.685519	19.104026
47.016120	1666.454653	19.109043
47.283959	1668.737691	19.114061
47.443622	1682.622408	19.119079
47.443478	1686.290103	19.124096
47.624663	1677.761666	19.129114
47.869508	1660.719869	19.134131
47.633688	1647.407145	19.139149
47.310527	1643.760764	19.144167
47.376544	1649.461476	19.149184
46.999682	1674.608482	19.154202
47.463385	1665.933388	19.159219
47.584014	1666.314678	19.164237
47.605393	1674.330166	19.169255
47.861028	1682.998734	19.174272
47.876689	1693.305940	19.179290
47.799031	1671.994405	19.184307
47.465760	1673.468697	19.189325
47.468070	1695.084218	19.194343
47.917473	1694.695187	19.199360
47.675987	1698.888787	19.204378
48.271620	1701.889157	19.209395
48.190253	1707.225742	19.214413
48.111136	1726.995109	19.219431
48.159736	1715.435055	19.224448
48.215187	1694.769759	19.229466
48.260281	1704.133524	19.234483
48.363005	1718.261985	19.239501
48.164722	1716.896544	19.244519
48.623401	1711.058481	19.249536
48.702338	1702.602132	19.254554
48.751610	1693.847308	19.259571
48.737577	1696.254668	19.264589
48.476604	1691.099393	19.269607
48.637090	1690.676823	19.274624
48.552277	1700.596095	19.279642
48.645578	1704.150145	19.284659
48.875304	1711.929199	19.289677
48.607671	1729.290755	19.294695
48.857080	1700.237835	19.299712
48.796612	1713.100317	19.304730
48.654676	1725.452955	19.309747
49.162047	1741.109911	19.314765
48.950067	1734.050653	19.319783
49.598814	1727.636111	19.324800
49.449802	1744.655610	19.329818
49.543694	1721.505495	19.334835
49.770234	1702.251287	19.339853
49.374951	1710.055684	19.344871
49.771422	1719.774991	19.349888
49.406871	1710.966518	19.354906
49.427372	1687.495383	19.359923
49.723296	1681.962220	19.364941
49.384861	1709.735260	19.369959
49.698996	1691.904088	19.374976
49.612387	1702.313714	19.379994
49.559827	1720.080279	19.385011
49.662614	1728.698260	19.390029
49.635170	1726.254114	19.395047
49.666074	1728.761118	19.400064
49.739676	1717.873858	19.405082
49.597564	1707.869026	19.410099
49.932487	1712.070311	19.415117
50.208449	1741.881204	19.420135
50.188345	1738.192495	19.425152
50.097216	1764.690768	19.430170
50.275334	1757.627457	19.435187
50.470557	1753.006495	19.440205
49.854521	1765.820403	19.445223
50.149317	1763.908513	19.450240
49.924104	1763.197090	19.455258
49.561682	1752.754518	19.460275
50.384121	1763.567989	19.465293
50.522347	1790.819585	19.470311
50.675317	1776.615207	19.475328
50.167695	1776.193808	19.480346
49.809870	1774.717056	19.485363
50.870122	1791.951066	19.490381
50.979995	1817.874199	19.495399
51.238896	1804.077207	19.500416
51.290942	1779.330304	19.505434
51.016273	1778.990366	19.510451
51.275477	1787.037662	19.515469
51.132902	1782.193335	19.520487
51.284649	1774.303833	19.525504
51.132854	1778.012551	19.530522
51.142482	1764.005557	19.535539
51.519049	1764.698226	19.540557
51.342514	1787.412013	19.545575
51.423670	1794.712317	19.550592
51.438734	1787.763321	19.555610
51.261349	1790.097808	19.560627
51.594876	1796.737439	19.565645
51.400343	1794.464073	19.570663
51.805816	1773.665256	19.575680
51.471429	1791.475719	19.580698
51.629925	1812.551428	19.585715
51.600307	1807.665203	19.590733
51.665156	1808.129814	19.595751
52.022328	1791.052385	19.600768
51.892186	1784.894652	19.605786
51.731725	1784.207856	19.610803
51.910633	1792.837601	19.615821
52.116423	1825.420426	19.620839
52.166110	1816.675796	19.625856
52.258833	1802.946119	19.630874
52.195096	1826.494598	19.635891
52.725812	1838.978448	19.640909
52.549602	1829.016467	19.645927
52.539846	1782.564614	19.650944
52.604634	1775.473674	19.655962
52.508726	1781.171572	19.660979
52.626015	1799.682939	19.665997
52.796673	1786.720753	19.671015
52.983328	1786.482401	19.676032
52.845317	1778.225016	19.681050
52.409789	1788.368212	19.686067
52.531066	1789.365416	19.691085
52.868311	1793.881729	19.696103
52.921011	1810.205012	19.701120
52.926560	1830.418008	19.706138
52.763506	1840.988068	19.711155
52.930285	1829.759608	19.716173
52.664408	1841.266260	19.721191
52.685533	1821.947538	19.726208
52.673675	1821.696526	19.731226
52.625706	1839.834541	19.736243
53.215491	1848.218110	19.741261
53.292873	1862.194229	19.746279
53.394134	1852.097620	19.751296
53.249714	1841.442816	19.756314
53.412781	1836.477999	19.761331
53.412320	1841.900553	19.766349
53.606050	1861.212882	19.771367
53.837046	1868.672972	19.776384
53.853744	1866.577345	19.781402
53.801246	1875.007134	19.786419
54.089397	1864.374614	19.791437
54.067559	1866.180555	19.796455
54.187473	1876.574181	19.801472
54.271025	1860.491015	19.806490
54.176685	1846.606716	19.811507
54.677922	1870.946276	19.816525
54.358759	1854.847692	19.821543
54.281368	1840.454988	19.826560
54.549981	1829.474117	19.831578
54.241775	1820.354558	19.836595
54.510014	1830.015515	19.841613
54.090320	1847.385505	19.846631
54.234043	1855.480458	19.851648
54.745366	1843.828197	19.856666
54.452915	1861.817897	19.861683
54.586477	1865.872318	19.866701
54.295886	1862.244710	19.871719
54.699269	1853.543756	19.876736
54.666524	1842.880535	19.881754
54.609752	1862.247152	19.886771
54.837508	1873.660743	19.891789
54.972702	1875.562267	19.896807
55.004962	1870.917618	19.901824
55.121543	1877.121868	19.906842
54.986819	1899.250580	19.911859
55.263352	1894.115940	19.916877
55.016148	1886.564695	19.921895
55.226908	1896.965463	19.926912
55.273285	1880.810876	19.931930
55.586934	1878.069541	19.936947
55.490099	1888.356107	19.941965
55.459380	1886.091870	19.946983
54.990515	1877.908589	19.952000
55.683283	1898.192035	19.957018
55.392783	1901.115100	19.962035
55.818913	1892.685608	19.967053
55.930304	1907.711357	19.972071
56.018925	1921.548594	19.977088
56.603482	1913.653137	19.982106
56.246553	1894.228325	19.987123
56.075402	1883.923413	19.992141
56.201384	1858.997267	19.997159
55.970597	1857.795716	20.002176
56.098742	1869.104233	20.007194
56.096852	1896.446973	20.012211
56.115476	1875.501945	20.017229
56.478869	1877.052731	20.022247
56.264185	1893.514067	20.027264
56.268067	1908.605703	20.032282
56.076989	1896.629694	20.037299
56.288863	1895.784731	20.042317
56.270405	1892.468967	20.047335
56.519289	1900.551782	20.052352
56.480197	1901.415683	20.057370
56.638902	1911.030631	20.062387
56.656799	1903.294849	20.067405
56.802849	1920.294716	20.072423
56.688687	1938.032842	20.077440
57.140352	1934.573352	20.082458
56.706401	1915.224122	20.087475
56.746013	1904.220815	20.092493
57.018024	1926.016264	20.097511
57.374465	1956.585684	20.102528
57.750372	1936.632809	20.107546
57.604945	1916.026290	20.112563
58.100401	1915.047572	20.117581
57.852626	1931.616071	20.122599
57.918135	1925.665570	20.127616
58.149926	1891.143418	20.132634
57.603911	1903.930912	20.137651
57.687421	1917.228543	20.142669
57.809657	1926.339389	20.147687
57.301575	1917.661384	20.152704
57.768066	1915.956097	20.157722
57.598981	1910.484243	20.162739
57.775597	1911.124938	20.167757
57.918468	1938.360186	20.172775
57.690137	1937.895483	20.177792
58.199170	1930.046842	20.182810
58.252764	1951.390423	20.187827
58.356547	1945.443332	20.192845
58.178951	1939.801548	20.197863
58.206245	1946.187872	20.202880
58.026042	1951.506728	20.207898
57.937536	1963.828488	20.212915
58.248744	1958.102579	20.217933
58.477254	1945.757745	20.222951
58.553672	1967.571404	20.227968
58.658045	1980.168038	20.232986
58.610470	1964.568254	20.238003
58.662872	1953.942155	20.243021
58.952174	1965.795264	20.248039
58.814382	1963.254770	20.253056
59.409730	1979.172972	20.258074
59.167973	1971.325269	20.263091
59.392863	1958.732546	20.268109
59.315358	1965.857121	20.273127
59.222607	1968.040077	20.278144
59.624982	1953.237834	20.283162
59.544378	1940.840954	20.288179
59.219042	1946.826778	20.293197
59.567326	1959.172599	20.298215
59.453937	1971.276374	20.303232
59.229070	1982.766710	20.308250
59.474369	2003.299895	20.313267
59.597642	1986.622545	20.318285
59.655051	1991.673158	20.323303
59.672045	1994.865447	20.328320
59.998339	1975.208265	20.333338
60.179994	1982.876920	20.338355
59.719714	2003.725973	20.343373
60.047302	1984.339479	20.348391
59.900711	1986.525430	20.353408
60.102582	1977.902383	20.358426
60.178798	2001.934110	20.363443
60.013973	2000.200977	20.368461
60.537394	2013.899138	20.373479
60.299211	2020.071733	20.378496
60.405650	2015.200550	20.383514
60.563927	2010.174767	20.388531
60.602837	2009.794617	20.393549
60.690601	2009.957865	20.398567
60.512492	2034.724159	20.403584
60.748119	2006.503098	20.408602
60.610503	1995.725333	20.413619
60.607305	2009.438084	20.418637
60.716777	2018.452688	20.423655
60.556112	2031.445752	20.428672
60.981018	2029.351435	20.433690
60.980215	2037.522325	20.438707
60.938373	2053.066656	20.443725
61.436646	2036.362318	20.448743
61.226354	2030.544835	20.453760
61.280652	2042.540066	20.458778
61.139480	2034.918872	20.463795
61.421273	2042.543161	20.468813
61.423648	2039.843788	20.473831
61.626805	2051.899353	20.478848
61.770737	2062.554933	20.483866
62.008878	2073.864123	20.488883
61.883906	2079.297790	20.493901
61.917332	2049.947086	20.498919
61.838567	2059.615538	20.503936
62.047148	2073.012202	20.508954
62.149203	2080.840588	20.513971
62.342802	2046.197060	20.518989
62.472161	2051.530828	20.524007
61.906797	2064.936204	20.529024
62.335356	2064.004058	20.534042
62.445377	2050.520664	20.539059
62.215321	2044.374908	20.544077
62.879220	2040.253275	20.549095
62.101664	2059.693882	20.554112
62.505648	2059.034153	20.559130
62.320139	2043.068275	20.564147
62.186577	2076.813512	20.569165
62.372977	2091.953795	20.574183
62.909779	2093.674142	20.579200
62.609949	2071.838234	20.584218
62.908158	2085.502232	20.589235
63.085808	2090.321432	20.594253
62.765571	2079.648673	20.599271
63.283028	2090.288113	20.604288
63.128310	2097.772788	20.609306
63.418977	2109.162579	20.614323
63.433958	2121.459394	20.619341
63.358650	2107.089024	20.624359
63.463714	2098.888034	20.629376
63.670121	2113.670373	20.634394
63.879670	2114.132240	20.639411
63.684149	2106.005321	20.644429
64.006212	2096.594178	20.649447
63.494213	2093.503305	20.654464
63.786432	2105.729300	20.659482
63.764986	2112.994259	20.664499
63.607095	2117.318227	20.669517
63.974965	2079.609857	20.674535
64.187589	2091.027292	20.679552
64.032853	2094.077637	20.684570
64.185275	2113.540982	20.689587
63.945671	2101.146039	20.694605
64.378646	2093.849648	20.699623
64.144497	2114.296097	20.704640
64.341345	2126.992610	20.709658
64.305616	2112.878934	20.714675
64.251044	2126.041325	20.719693
64.613232	2137.093885	20.724711
64.489286	2121.532147	20.729728
64.849699	2128.582761	20.734746
64.870177	2130.640355	20.739763
64.707558	2133.203908	20.744781
65.014465	2124.454682	20.749799
65.132210	2149.937785	20.754816
64.873879	2150.938009	20.759834
65.242531	2163.670028	20.764851
65.305489	2150.436014	20.769869
66.005411	2133.497596	20.774887
65.694387	2140.405177	20.779904
65.419742	2127.245865	20.784922
65.693364	2114.119564	20.789939
65.527424	2144.340031	20.794957
65.807940	2151.678415	20.799975
65.652276	2150.076995	20.804992
65.461968	2135.641562	20.810010
65.852991	2137.423693	20.815027
65.693085	2134.600851	20.820045
65.816483	2142.916403	20.825063
65.885140	2152.595094	20.830080
65.576675	2158.812324	20.835098
65.927199	2151.533172	20.840115
65.918439	2161.563579	20.845133
66.095572	2166.852885	20.850151
65.882955	2170.922374	20.855168
66.110079	2157.187196	20.860186
66.354679	2169.236301	20.865203
66.118974	2190.759886	20.870221
66.608700	2186.391356	20.875239
66.540577	2181.844879	20.880256
66.460712	2194.772278	20.885274
66.670618	2192.468530	20.890291
66.252616	2190.023209	20.895309
66.708094	2179.230365	20.900327
67.144725	2213.567190	20.905344
67.246734	2215.414901	20.910362
67.676384	2202.653522	20.915379
67.453096	2213.010010	20.920397
67.595462	2201.509967	20.925415
67.578104	2188.876491	20.930432
67.654711	2189.379617	20.935450
67.951917	2186.094487	20.940467
67.713550	2169.586422	20.945485
68.085433	2170.103539	20.950503
67.789975	2183.692625	20.955520
68.016903	2190.017721	20.960538
68.127511	2163.221804	20.965555
67.625312	2163.427533	20.970573
67.849784	2168.054605	20.975591
68.035544	2178.437948	20.980608
67.905275	2161.299343	20.985626
68.252117	2158.651079	20.990643
68.062845	2161.442525	20.995661
68.055573	2169.855360	21.000679
68.176667	2182.938878	21.005696
68.159332	2197.995238	21.010714
68.335443	2189.858823	21.015731
67.990559	2205.999057	21.020749
68.019399	2191.562686	21.025767
68.143392	2198.341725	21.030784
67.806392	2215.920179	21.035802
68.640160	2230.417990	21.040819
68.666189	2232.351080	21.045837
69.040051	2230.192251	21.050855
68.764776	2223.714977	21.055872
68.677260	2230.067250	21.060890
69.155522	2256.783255	21.065907
69.001300	2282.945663	21.070925
69.408268	2258.668777	21.075943
69.359073	2249.024058	21.080960
69.299093	2259.223791	21.085978
69.589374	2250.820981	21.090995
69.192758	2259.301055	21.096013
69.769109	2260.083845	21.101031
69.887081	2268.659372	21.106048
69.802623	2264.641562	21.111066
69.962552	2246.610170	21.116083
69.590369	2264.592850	21.121101
69.411371	2265.199130	21.126119
69.928161	2246.606688	21.131136
69.509378	2259.034828	21.136154
70.109191	2267.611231	21.141171
69.646239	2273.349199	21.146189
70.273528	2275.030112	21.151207
70.211422	2295.781584	21.156224
70.454337	2290.634261	21.161242
70.861942	2314.472766	21.166259
71.059286	2320.694652	21.171277
71.276544	2300.568441	21.176295
71.136841	2278.281736	21.181312
71.229354	2283.048345	21.186330
71.412130	2258.445378	21.191347
71.279333	2266.483897	21.196365
71.230117	2267.702876	21.201383
71.287805	2256.721817	21.206400
70.767429	2274.256242	21.211418
71.263835	2283.368355	21.216435
70.987947	2269.210278	21.221453
71.172544	2255.230606	21.226471
71.274347	2271.734423	21.231488
71.007185	2307.133068	21.236506
71.419226	2296.846449	21.241523
71.379793	2283.880378	21.246541
71.379262	2284.311130	21.251559
71.543395	2303.569569	21.256576
71.692486	2322.037932	21.261594
71.963154	2309.897617	21.266611
72.132370	2308.070969	21.271629
72.132481	2314.220738	21.276647
72.384766	2323.242527	21.281664
72.248148	2315.717373	21.286682
72.487345	2322.582040	21.291699
72.625540	2326.011020	21.296717
72.316297	2305.983218	21.301735
72.377429	2319.739151	21.306752
72.071118	2316.618868	21.311770
72.602882	2312.636401	21.316787
72.373770	2312.686098	21.321805
72.532591	2322.786146	21.326823
72.752831	2345.945542	21.331840
73.044893	2351.106490	21.336858
73.347724	2331.663817	21.341875
73.317548	2343.869372	21.346893
73.273962	2358.227192	21.351911
73.240163	2345.010771	21.356928
72.838523	2347.066209	21.361946
73.245359	2347.222596	21.366963
73.339129	2342.121159	21.371981
73.227785	2348.244681	21.376999
73.682948	2345.607518	21.382016
73.353373	2330.888074	21.387034
73.566733	2338.659623	21.392051
73.699481	2350.980954	21.397069
73.830814	2354.613207	21.402087
74.366917	2348.206987	21.407104
74.033750	2366.971398	21.412122
74.116064	2370.941622	21.417139
73.885725	2355.320862	21.422157
74.006685	2356.504642	21.427175
74.258627	2363.500861	21.432192
74.027047	2366.968122	21.437210
74.190040	2355.453731	21.442227
74.375228	2368.945548	21.447245
74.281321	2362.989237	21.452263
74.696055	2360.745500	21.457280
74.792944	2390.115080	21.462298
75.006146	2392.713310	21.467315
75.114318	2380.131559	21.472333
75.054318	2369.326928	21.477351
74.892177	2386.129756	21.482368
75.131513	2390.557031	21.487386
75.085223	2386.705689	21.492403
75.467277	2384.902711	21.497421
75.102281	2386.561416	21.502439
75.486415	2394.035526	21.507456
75.438090	2398.046239	21.512474
75.406073	2382.765847	21.517491
75.645671	2395.083728	21.522509
75.687835	2408.580713	21.527527
75.862312	2404.207532	21.532544
75.168622	2414.715988	21.537562
75.277688	2421.176090	21.542579
75.592958	2433.243149	21.547597
75.972236	2434.374999	21.552615
76.385736	2414.566943	21.557632
76.415651	2436.426053	21.562650
76.625376	2451.624049	21.567667
76.596256	2442.152045	21.572685
76.584526	2425.450964	21.577703
76.887830	2416.137200	21.582720
76.918557	2441.546598	21.587738
76.999805	2432.475784	21.592755
77.130935	2434.823846	21.597773
76.735415	2439.385563	21.602791
77.017823	2418.072635	21.607808
77.031110	2426.565959	21.612826
77.177603	2427.945690	21.617843
77.295994	2420.279150	21.622861
77.452254	2403.354893	21.627879
77.495330	2405.273871	21.632896
77.447690	2405.696272	21.637914
77.717253	2421.694260	21.642931
77.873660	2427.493102	21.647949
77.331517	2428.900026	21.652967
77.850890	2401.013576	21.657984
77.786143	2410.784148	21.663002
77.638362	2412.199909	21.668019
77.638166	2403.835568	21.673037
77.688148	2403.258335	21.678055
77.764343	2385.591346	21.683072
77.933343	2415.012041	21.688090
78.075566	2447.401313	21.693107
78.165998	2450.228272	21.698125
77.802112	2427.887660	21.703143
78.196040	2428.818695	21.708160
78.211599	2437.375419	21.713178
78.285638	2434.765595	21.718195
78.686825	2457.204032	21.723213
79.007918	2473.845622	21.728231
78.878697	2456.697852	21.733248
78.537609	2469.285539	21.738266
78.814536	2494.523851	21.743283
78.741218	2467.886024	21.748301
78.585119	2470.429562	21.753319
79.071340	2488.955196	21.758336
78.973600	2502.186647	21.763354
78.851002	2496.675508	21.768371
79.080401	2499.278559	21.773389
78.751562	2507.327161	21.778407
78.981388	2534.777706	21.783424
79.560129	2544.101926	21.788442
79.954990	2528.647717	21.793459
80.134339	2543.666797	21.798477
80.178403	2540.585406	21.803495
80.156329	2528.083905	21.808512
80.209918	2522.998889	21.813530
80.296931	2543.118273	21.818547
80.503321	2524.178031	21.823565
80.659349	2517.489521	21.828583
80.869654	2503.135354	21.833600
80.693723	2518.515629	21.838618
80.853988	2536.638561	21.843635
80.895486	2511.949888	21.848653
80.683451	2507.779107	21.853671
80.670821	2510.926406	21.858688
80.227611	2519.851262	21.863706
80.473787	2523.169545	21.868723
80.533732	2527.575330	21.873741
80.128477	2555.797682	21.878759
80.676646	2545.161486	21.883776
81.154477	2549.957210	21.888794
81.094432	2564.712568	21.893811
81.523190	2576.618686	21.898829
81.046874	2570.051374	21.903847
81.370601	2556.576115	21.908864
81.436897	2573.985988	21.913882
81.353882	2592.631593	21.918899
81.929377	2606.887347	21.923917
82.140795	2597.859680	21.928935
82.225409	2573.174610	21.933952
82.384903	2592.150559	21.938970
82.297972	2600.155299	21.943987
82.579260	2588.521792	21.949005
82.008204	2591.327000	21.954023
82.468313	2581.550676	21.959040
82.349286	2587.515547	21.964058
82.123239	2593.100133	21.969075
82.668552	2599.867695	21.974093
82.790813	2622.991542	21.979111
82.862947	2606.698785	21.984128
83.244012	2611.201903	21.989146
82.903262	2618.484731	21.994163
83.212844	2607.960937	21.999181
83.352715	2604.084880	22.004199
83.388418	2615.584592	22.009216
83.552544	2628.499101	22.014234
82.967829	2628.093264	22.019251
83.180932	2612.690852	22.024269
82.967083	2613.176545	22.029287
83.243658	2627.169357	22.034304
83.374491	2647.185390	22.039322
83.193343	2657.082031	22.044339
83.613433	2639.108159	22.049357
83.658414	2655.033477	22.054375
84.016217	2651.443595	22.059392
84.199303	2669.412540	22.064410
83.952939	2686.017635	22.069427
84.240647	2688.881714	22.074445
84.376259	2691.777815	22.079463
84.318649	2677.665367	22.084480
84.433850	2652.529510	22.089498
84.125128	2658.128174	22.094515
84.455366	2674.314402	22.099533
84.388594	2692.567736	22.104551
84.801519	2693.102793	22.109568
85.024267	2684.124574	22.114586
84.972183	2684.265277	22.119603
85.118274	2680.209065	22.124621
85.150104	2683.554929	22.129639
85.235666	2719.581769	22.134656
85.481779	2720.138880	22.139674
85.405944	2714.198144	22.144691
85.532273	2708.533804	22.149709
85.609064	2725.980692	22.154727
85.889764	2727.675038	22.159744
85.987178	2715.149705	22.164762
85.687994	2714.897836	22.169779
86.095364	2703.775420	22.174797
85.950926	2709.994502	22.179815
86.175629	2713.035115	22.184832
86.421534	2737.810713	22.189850
86.440221	2739.399557	22.194867
86.776592	2729.728221	22.199885
87.209189	2730.103948	22.204903
86.972292	2715.467822	22.209920
86.932204	2716.555031	22.214938
86.928447	2714.541791	22.219955
86.877169	2703.581174	22.224973
86.943546	2711.312840	22.229991
87.163991	2707.420688	22.235008
87.322725	2723.092668	22.240026
87.160470	2729.216881	22.245043
87.169929	2717.378230	22.250061
86.867841	2733.315120	22.255079
86.964511	2740.719989	22.260096
87.481327	2742.566633	22.265114
87.456803	2761.820802	22.270131
87.515389	2774.981189	22.275149
87.764976	2770.279788	22.280167
87.864269	2771.481746	22.285184
87.592779	2771.331781	22.290202
87.827752	2749.254096	22.295219
88.095213	2767.508581	22.300237
88.133340	2794.776731	22.305255
88.078349	2799.639912	22.310272
88.302726	2783.101369	22.315290
88.119386	2794.398072	22.320307
88.342937	2786.440782	22.325325
88.505994	2806.081473	22.330343
88.350270	2815.693147	22.335360
88.741609	2818.353144	22.340378
88.711710	2812.287473	22.345395
88.984975	2820.793559	22.350413
89.194105	2829.906823	22.355431
89.025443	2823.744014	22.360448
89.234367	2800.980691	22.365466
89.471650	2821.937501	22.370483
89.518450	2823.318193	22.375501
89.523985	2821.887577	22.380519
89.712719	2833.540093	22.385536
89.939233	2830.976651	22.390554
89.748819	2837.054386	22.395571
89.953360	2825.714054	22.400589
90.100446	2829.398337	22.405607
89.989171	2853.250005	22.410624
90.137047	2834.703449	22.415642
90.070272	2825.230738	22.420659
90.264984	2831.652258	22.425677
90.253380	2843.440628	22.430695
90.199805	2851.576190	22.435712
90.234781	2845.056734	22.440730
90.096820	2853.886859	22.445747
90.563075	2854.908517	22.450765
90.889755	2860.889597	22.455783
90.814396	2869.202760	22.460800
90.939322	2876.507959	22.465818
91.108594	2902.033396	22.470835
91.435861	2877.805906	22.475853
91.921424	2874.120265	22.480871
91.712769	2889.666139	22.485888
92.019361	2878.280366	22.490906
91.766426	2876.777509	22.495923
91.619711	2885.802184	22.500941
91.884625	2896.132488	22.505959
92.011338	2895.311878	22.510976
92.074951	2868.669035	22.515994
92.027430	2879.741809	22.521011
92.087358	2879.399498	22.526029
92.262901	2878.534015	22.531047
92.309564	2874.068844	22.536064
92.263566	2886.657708	22.541082
92.314228	2890.792923	22.546099
92.274005	2915.029942	22.551117
92.436664	2911.376392	22.556135
92.370353	2906.935980	22.561152
92.932490	2905.156921	22.566170
92.645325	2906.754005	22.571187
93.043875	2930.692590	22.576205
93.003377	2920.924571	22.581223
93.381058	2910.193871	22.586240
93.569501	2917.513592	22.591258
93.577838	2939.247471	22.596275
93.155121	2940.654976	22.601293
93.314925	2925.712380	22.606311
93.479315	2943.979777	22.611328
93.883785	2942.379897	22.616346
93.898966	2944.819235	22.621363
93.677665	2949.563900	22.626381
93.668373	2969.642283	22.631399
93.634542	2971.444135	22.636416
94.411164	2974.561494	22.641434
94.200639	2997.080346	22.646451
94.253834	2981.762053	22.651469
94.495116	2971.173127	22.656487
94.387419	2972.706708	22.661504
94.397135	2997.769753	22.666522
94.617244	3003.325049	22.671539
95.335857	3000.959561	22.676557
95.435004	2998.882239	22.681575
94.852185	3006.695345	22.686592
95.601387	2997.504772	22.691610
95.339005	3005.208439	22.696627
95.068429	3010.348226	22.701645
95.422955	2998.372822	22.706663
95.458993	3004.269716	22.711680
95.488391	3006.205005	22.716698
95.766930	3008.011734	22.721715
95.557149	3019.201370	22.726733
95.713866	3016.907077	22.731751
95.704752	3020.142668	22.736768
96.088702	3030.199289	22.741786
96.361681	3037.244303	22.746803
96.458986	3020.749728	22.751821
96.702671	3014.493512	22.756839
96.038303	3034.626885	22.761856
96.748236	3034.265145	22.766874
96.906388	3041.272645	22.771891
97.150219	3047.863874	22.776909
97.328441	3051.553498	22.781927
97.160668	3056.779646	22.786944
97.370252	3039.086915	22.791962
97.344332	3045.794164	22.796979
97.630841	3055.927920	22.801997
97.385563	3035.161123	22.807015
97.018608	3040.989402	22.812032
97.550063	3034.407905	22.817050
97.690150	3056.676806	22.822067
97.893930	3048.415992	22.827085
98.026761	3040.245046	22.832103
97.893743	3036.793850	22.837120
97.818117	3062.081510	22.842138
98.102289	3076.394895	22.847155
98.128564	3070.949884	22.852173
98.422186	3044.811776	22.857191
97.937073	3064.884468	22.862208
98.460620	3070.926593	22.867226
98.619384	3085.296729	22.872243
98.603332	3085.657045	22.877261
98.969699	3086.349400	22.882279
98.876262	3103.882516	22.887296
99.010841	3097.845059	22.892314
98.848215	3091.127076	22.897331
99.009307	3103.881481	22.902349
99.672573	3099.666482	22.907367
99.190075	3099.836386	22.912384
99.331327	3104.087776	22.917402
99.690640	3104.315406	22.922419
99.568583	3104.015759	22.927437
99.591804	3123.277646	22.932455
99.920541	3149.116868	22.937472
100.334166	3152.793403	22.942490
100.583850	3150.523882	22.947507
100.182801	3149.990838	22.952525
100.341520	3134.151864	22.957543
100.573147	3124.818222	22.962560
100.501438	3120.584326	22.967578
100.716905	3129.361720	22.972595
100.785869	3147.843136	22.977613
100.850955	3136.821058	22.982631
100.953137	3132.382658	22.987648
101.109043	3135.787244	22.992666
101.337415	3137.442651	22.997683
101.252817	3159.111892	23.002701
101.525401	3163.262275	23.007719
101.259567	3157.378351	23.012736
101.577021	3149.958249	23.017754
101.689850	3153.930523	23.022771
101.858128	3142.733927	23.027789
102.041227	3142.866477	23.032807
101.930844	3157.705712	23.037824
102.019201	3148.080018	23.042842
102.064673	3153.389650	23.047859
102.029685	3153.119114	23.052877
101.955664	3182.984145	23.057895
102.163677	3191.903145	23.062912
102.243653	3183.819195	23.067930
102.222592	3166.590760	23.072947
102.562492	3174.887040	23.077965
102.818674	3198.155747	23.082983
102.506697	3199.391055	23.088000
102.946849	3202.406991	23.093018
102.757272	3213.250553	23.098035
102.588709	3208.191193	23.103053
103.482159	3211.892776	23.108071
103.282458	3225.007457	23.113088
103.384275	3241.522351	23.118106
103.738824	3246.749845	23.123123
103.453241	3241.778701	23.128141
103.646692	3241.528677	23.133159
103.502731	3262.619549	23.138176
104.065260	3283.889742	23.143194
104.290230	3272.857288	23.148211
104.184480	3254.856611	23.153229
104.424528	3260.184123	23.158247
104.544663	3279.862233	23.163264
104.333582	3290.774749	23.168282
104.774055	3279.286253	23.173299
104.764544	3290.772682	23.178317
105.147321	3277.460053	23.183335
105.214651	3303.519285	23.188352
105.243431	3300.655404	23.193370
105.357462	3292.291782	23.198387
105.395227	3286.650919	23.203405
105.376670	3295.906205	23.208423
105.597535	3293.965014	23.213440
105.708634	3289.407391	23.218458
106.035260	3300.932960	23.223475
105.761294	3311.821635	23.228493
105.913294	3303.939675	23.233511
105.834412	3314.393598	23.238528
105.957777	3321.211915	23.243546
106.044441	3320.210126	23.248563
106.221410	3331.230776	23.253581
106.469179	3332.513746	23.258599
106.422299	3331.453912	23.263616
106.301925	3346.765208	23.268634
106.347903	3350.035658	23.273651
107.037408	3353.280671	23.278669
107.117834	3370.018704	23.283687
107.272220	3375.097051	23.288704
106.919743	3364.693558	23.293722
107.378145	3363.344148	23.298739
107.473495	3374.999318	23.303757
107.375754	3379.922890	23.308775
107.125095	3373.024073	23.313792
107.406431	3386.559356	23.318810
107.714145	3385.947570	23.323827
107.930120	3395.882596	23.328845
108.090244	3393.543989	23.333863
108.338207	3408.560253	23.338880
108.257651	3418.044143	23.343898
108.585867	3408.044433	23.348915
108.340443	3406.598544	23.353933
108.868147	3406.391308	23.358951
109.120072	3420.507607	23.363968
109.019107	3415.015198	23.368986
109.041975	3403.578293	23.374003
109.075811	3417.597568	23.379021
109.366737	3400.032898	23.384039
109.582564	3415.613678	23.389056
109.238859	3410.080287	23.394074
109.633432	3398.671130	23.399091
109.598337	3392.504524	23.404109
109.588240	3400.097219	23.409127
109.707404	3415.834508	23.414144
109.605280	3422.296270	23.419162
110.166598	3429.176902	23.424179
109.859281	3442.775253	23.429197
110.035264	3438.721581	23.434215
110.217401	3413.232511	23.439232
110.367374	3414.803866	23.444250
110.407217	3441.077892	23.449267
110.491551	3456.357833	23.454285
110.514096	3449.874031	23.459303
110.499986	3459.721932	23.464320
110.821789	3469.326359	23.469338
111.097161	3501.470279	23.474355
110.986145	3505.785510	23.479373
111.442108	3490.616675	23.484391
111.345138	3480.981637	23.489408
111.165739	3501.570076	23.494426
111.342069	3505.599855	23.499443
111.522307	3511.039691	23.504461
111.648157	3520.793841	23.509479
111.814825	3524.801799	23.514496
111.779511	3511.632456	23.519514
112.117020	3531.869798	23.524531
112.207660	3558.315732	23.529549
112.387569	3543.537510	23.534567
112.545205	3536.049349	23.539584
112.516799	3553.533059	23.544602
113.030418	3556.837296	23.549619
112.544623	3552.701032	23.554637
112.825998	3555.036250	23.559655
113.029966	3581.579039	23.564672
112.931189	3571.810789	23.569690
113.142523	3563.608094	23.574707
113.413644	3590.086263	23.579725
113.486721	3604.576545	23.584743
113.964538	3607.943593	23.589760
113.719382	3607.035588	23.594778
113.978856	3594.424894	23.599795
113.900022	3603.207097	23.604813
114.150580	3601.556213	23.609831
114.600336	3617.160938	23.614848
114.521382	3626.125640	23.619866
114.901325	3608.851709	23.624883
115.034856	3619.722276	23.629901
115.081889	3610.560959	23.634919
115.206231	3601.566188	23.639936
114.909656	3625.968326	23.644954
115.513697	3606.713827	23.649971
115.464299	3608.508483	23.654989
115.572562	3617.819772	23.660007
115.716429	3609.204614	23.665024
115.801156	3602.538440	23.670042
115.970068	3598.369959	23.675059
115.971483	3599.676337	23.680077
115.962466	3609.458537	23.685095
116.252078	3589.121463	23.690112
116.155001	3588.249025	23.695130
116.281574	3587.668344	23.700147
116.115075	3593.805016	23.705165
116.223390	3606.225280	23.710183
116.345712	3603.797817	23.715200
116.367041	3614.776481	23.720218
116.737580	3620.682507	23.725235
116.837751	3633.330302	23.730253
116.548641	3627.292772	23.735271
117.030753	3622.253309	23.740288
116.886128	3638.277897	23.745306
117.000424	3652.156738	23.750323
116.941386	3653.255410	23.755341
116.895549	3671.011207	23.760359
116.925664	3685.890524	23.765376
117.362301	3683.451660	23.770394
117.850972	3675.171979	23.775411
118.141325	3696.111369	23.780429
117.916966	3696.515765	23.785447
118.580339	3677.907228	23.790464
118.352816	3698.405463	23.795482
118.284586	3698.450228	23.800499
118.312307	3708.031749	23.805517
118.043524	3713.904879	23.810535
118.719726	3717.936757	23.815552
118.638862	3735.848011	23.820570
118.863169	3733.180858	23.825587
118.924158	3748.777520	23.830605
119.163858	3771.239443	23.835623
119.607481	3762.050691	23.840640
119.671148	3746.813761	23.845658
119.821045	3737.036204	23.850675
119.963184	3753.039903	23.855693
119.846545	3764.908533	23.860711
120.302697	3757.140445	23.865728
120.239939	3756.861691	23.870746
120.637013	3758.278874	23.875763
120.786617	3774.766563	23.880781
120.515268	3785.159109	23.885799
120.990097	3771.088774	23.890816
120.995872	3788.741302	23.895834
121.189125	3773.520923	23.900851
121.129819	3767.055828	23.905869
121.146305	3763.696290	23.910887
121.436631	3771.935342	23.915904
121.406396	3756.487754	23.920922
121.517638	3759.697905	23.925939
121.556848	3784.704603	23.930957
121.639916	3803.189198	23.935975
121.823307	3793.349185	23.940992
122.146985	3790.266222	23.946010
122.236982	3775.618571	23.951027
122.236502	3777.883870	23.956045
122.399995	3808.076586	23.961063
122.717474	3826.817534	23.966080
122.611823	3824.587143	23.971098
122.657885	3811.161399	23.976115
122.540588	3818.606276	23.981133
122.389426	3846.442171	23.986151
122.928185	3833.697346	23.991168
123.092602	3852.607701	23.996186
122.984409	3857.096173	24.001203
123.204485	3844.273101	24.006221
123.102162	3864.412898	24.011239
123.653882	3881.761558	24.016256
123.886326	3868.368742	24.021274
123.864346	3877.708795	24.026291
124.115115	3891.698954	24.031309
124.106004	3904.172914	24.036327
124.418624	3887.248359	24.041344
124.473895	3894.935213	24.046362
124.392786	3902.058029	24.051379
124.636146	3908.468222	24.056397
124.755765	3907.914267	24.061415
124.938567	3882.713863	24.066432
124.687046	3901.307992	24.071450
124.958791	3927.827186	24.076467
125.208636	3917.081879	24.081485
125.208500	3933.489171	24.086503
125.277016	3928.120731	24.091520
125.320439	3932.721566	24.096538
125.565277	3936.894264	24.101555
125.512418	3949.985294	24.106573
125.791770	3960.200353	24.111591
125.649161	3949.889533	24.116608
126.089585	3978.406804	24.121626
126.503189	3976.474821	24.126643
126.751174	3979.707696	24.131661
126.245053	3993.556689	24.136679
126.654812	4002.232599	24.141696
126.391082	4010.313146	24.146714
126.913377	4010.737868	24.151731
127.000146	4006.723000	24.156749
126.872865	4008.890394	24.161767
127.346725	4013.848452	24.166784
127.452202	4034.087394	24.171802
127.522724	4051.183097	24.176819
127.760825	4043.892211	24.181837
127.671330	4041.085529	24.186855
128.082997	4058.670510	24.191872
128.181632	4091.190709	24.196890
128.156144	4086.079861	24.201907
128.560548	4063.029638	24.206925
128.265609	4053.042723	24.211943
128.500359	4070.275475	24.216960
128.695044	4103.265629	24.221978
128.713025	4097.961383	24.226995
129.370552	4091.144057	24.232013
128.888396	4105.647029	24.237031
129.062652	4108.386234	24.242048
129.397162	4125.570676	24.247066
129.284028	4105.024685	24.252083
129.793080	4111.820566	24.257101
129.634386	4111.529903	24.262119
129.983663	4132.801471	24.267136
130.072808	4152.286611	24.272154
130.104780	4127.696333	24.277171
130.403242	4140.527910	24.282189
130.161178	4158.806823	24.287207
130.559566	4173.570248	24.292224
130.853400	4156.117033	24.297242
130.549373	4179.337864	24.302259
130.917842	4159.738553	24.307277
131.286060	4179.732313	24.312295
131.631158	4197.457580	24.317312
131.648220	4211.080167	24.322330
131.795920	4197.315458	24.327347
132.078742	4182.842245	24.332365
132.087346	4193.340373	24.337383
132.141254	4199.590268	24.342400
132.079145	4186.846412	24.347418
132.220155	4178.118029	24.352435
132.255936	4178.040888	24.357453
132.541877	4189.129380	24.362471
132.916872	4197.902086	24.367488
132.699640	4215.849419	24.372506
132.585069	4213.415730	24.377523
133.133789	4218.462662	24.382541
133.006414	4221.084018	24.387559
133.168192	4212.448636	24.392576
133.226286	4214.269694	24.397594
133.462994	4242.255390	24.402611
133.329489	4250.338165	24.407629
133.525208	4241.603068	24.412647
133.552491	4227.624774	24.417664
133.829667	4245.301874	24.422682
133.856143	4281.321257	24.427699
134.125983	4279.192530	24.432717
134.086628	4266.079902	24.437735
134.502164	4284.524310	24.442752
134.423370	4300.565082	24.447770
134.284423	4316.253618	24.452787
134.748078	4300.682740	24.457805
134.825081	4295.213168	24.462823
134.867319	4329.986408	24.467840
134.809401	4341.493229	24.472858
134.702370	4338.153583	24.477875
135.541120	4335.734789	24.482893
135.583377	4346.249506	24.487911
135.747605	4349.527794	24.492928
136.216385	4362.540067	24.497946
135.825918	4377.404900	24.502963
136.397200	4366.454601	24.507981
136.593987	4380.335819	24.512999
136.356193	4401.057931	24.518016
136.733352	4393.495487	24.523034
136.812807	4409.177950	24.528051
137.335958	4408.675014	24.533069
137.429425	4398.664640	24.538087
137.138620	4398.328874	24.543104
137.513870	4405.776109	24.548122
137.646681	4410.113504	24.553139
137.607161	4384.179951	24.558157
137.735070	4409.017101	24.563175
138.183690	4419.428504	24.568192
138.362618	4420.841837	24.573210
137.874752	4430.887530	24.578227
138.386583	4434.150919	24.583245
138.742612	4430.875680	24.588263
138.919794	4428.558706	24.593280
139.235007	4444.088867	24.598298
138.650131	4476.146058	24.603315
138.887782	4467.648388	24.608333
138.882880	4449.833586	24.613351
139.265307	4466.497119	24.618368
139.475522	4486.817770	24.623386
139.457167	4483.647687	24.628403
139.644411	4474.375292	24.633421
139.718837	4487.798491	24.638439
140.201697	4505.317496	24.643456
140.409143	4520.908453	24.648474
140.055275	4521.429934	24.653491
140.398620	4492.426317	24.658509
140.653070	4509.167734	24.663527
140.587507	4530.343438	24.668544
140.642227	4540.788119	24.673562
140.626273	4532.068151	24.678579
141.221251	4514.887996	24.683597
141.147871	4544.718738	24.688615
141.142933	4570.954445	24.693632
141.685758	4557.559160	24.698650
141.390037	4548.081883	24.703667
141.722884	4570.375250	24.708685
141.631124	4604.144100	24.713703
141.930148	4587.782830	24.718720
142.033792	4596.151003	24.723738
141.906088	4603.721595	24.728755
142.328170	4618.972861	24.733773
142.552075	4634.815539	24.738791
142.571345	4628.198323	24.743808
143.008224	4615.930711	24.748826
142.838735	4643.136232	24.753843
142.835778	4646.922515	24.758861
143.229506	4661.780483	24.763879
143.521860	4666.050251	24.768896
143.450305	4693.433769	24.773914
143.460992	4689.937196	24.778931
143.808660	4674.160310	24.783949
144.161252	4692.050258	24.788967
144.041528	4695.499159	24.793984
144.639236	4709.270333	24.799002
144.454729	4718.737745	24.804019
144.872142	4702.178843	24.809037
144.666442	4715.064280	24.814055
144.779138	4718.646040	24.819072
145.261206	4731.330054	24.824090
145.213723	4743.919690	24.829107
145.509338	4731.458796	24.834125
145.704944	4728.972986	24.839143
145.711745	4746.668562	24.844160
146.016578	4751.166211	24.849178
145.748745	4748.201074	24.854195
146.015868	4748.623102	24.859213
146.221706	4763.154343	24.864231
146.187770	4782.955098	24.869248
146.450974	4777.519157	24.874266
146.202336	4796.798717	24.879283
146.605520	4787.138884	24.884301
146.883652	4811.053831	24.889319
147.046243	4813.960837	24.894336
147.495973	4812.845222	24.899354
147.660933	4809.294785	24.904371
147.640896	4810.904415	24.909389
147.961322	4835.459652	24.914407
147.739021	4851.813286	24.919424
148.370294	4831.964589	24.924442
148.010889	4840.212554	24.929459
148.367260	4852.071377	24.934477
148.455017	4863.474594	24.939495
148.585783	4868.056157	24.944512
148.658450	4853.543817	24.949530
149.095612	4865.738907	24.954547
149.087038	4868.472237	24.959565
149.241845	4868.828970	24.964583
149.338769	4896.630677	24.969600
149.338041	4908.198153	24.974618
149.665638	4899.257040	24.979635
149.561923	4901.399403	24.984653
149.826331	4915.508904	24.989671
149.774465	4929.954536	24.994688
150.080670	4925.051991	24.999706
150.299835	4950.326505	25.004723
150.546897	4959.793228	25.009741
151.125904	4952.837717	25.014759
151.208867	4956.202397	25.019776
151.498363	4964.506201	25.024794
151.412324	4954.529460	25.029811
151.641754	4949.587231	25.034829
151.687838	4958.137945	25.039847
151.577436	4950.004610	25.044864
151.748655	4966.944921	25.049882
151.596984	4988.502013	25.054899
151.927992	4985.876861	25.059917
152.185238	4974.179597	25.064935
151.950387	4990.411434	25.069952
152.354031	5018.652840	25.074970
152.065321	5023.391555	25.079987
151.843089	5018.590076	25.085005
152.811959	5029.256878	25.090023
152.589005	5048.504946	25.095040
152.956325	5055.904987	25.100058
152.937952	5075.715748	25.105075
152.966623	5079.405177	25.110093
153.576516	5096.444013	25.115111
153.537297	5107.349092	25.120128
154.021996	5109.391503	25.125146
153.849625	5092.804833	25.130163
153.709678	5118.913770	25.135181
154.143898	5119.964116	25.140199
154.312883	5131.367888	25.145216
154.684522	5131.274226	25.150234
155.011580	5142.932995	25.155251
155.195715	5147.642832	25.160269
155.247613	5133.675798	25.165287
155.008154	5143.810826	25.170304
155.890722	5163.472442	25.175322
156.063201	5180.106079	25.180339
156.040584	5171.275433	25.185357
156.198438	5172.126561	25.190375
156.334045	5190.107663	25.195392
156.407985	5180.366553	25.200410
156.602036	5179.301035	25.205427
156.718394	5171.607290	25.210445
156.920862	5197.323556	25.215463
157.010612	5211.772034	25.220480
157.293513	5192.141469	25.225498
157.267365	5203.328712	25.230515
157.583526	5214.926736	25.235533
157.962796	5223.686722	25.240551
157.853657	5228.936391	25.245568
157.979516	5234.588187	25.250586
157.949000	5225.609994	25.255603
158.024913	5240.937970	25.260621
158.266272	5255.557112	25.265639
158.019004	5252.328631	25.270656
158.442483	5263.932975	25.275674
158.721733	5280.764831	25.280691
158.688143	5284.096083	25.285709
158.874558	5307.995453	25.290727
158.974988	5333.046894	25.295744
159.350605	5323.114113	25.300762
159.440726	5326.800534	25.305779
159.574839	5326.642967	25.310797
160.162304	5345.817340	25.315815
159.880280	5358.898602	25.320832
160.183414	5361.227354	25.325850
160.207756	5384.868968	25.330867
160.284581	5389.571018	25.335885
160.570331	5385.718988	25.340903
160.984193	5406.802495	25.345920
161.377176	5403.087078	25.350938
161.381704	5404.141118	25.355955
161.876100	5401.410158	25.360973
162.280296	5390.913145	25.365991
161.935378	5380.672990	25.371008
162.322788	5401.347069	25.376026
162.800387	5420.881038	25.381043
162.475470	5420.827662	25.386061
162.980928	5408.675268	25.391079
162.960733	5407.970736	25.396096
162.992312	5417.778865	25.401114
163.117879	5409.211012	25.406131
163.328727	5401.199956	25.411149
163.472234	5410.726980	25.416167
163.179384	5405.129541	25.421184
163.497980	5397.752281	25.426202
163.444642	5427.495969	25.431219
163.644175	5445.238449	25.436237
163.718378	5424.261318	25.441255
163.685668	5438.056202	25.446272
163.626937	5474.056600	25.451290
164.169078	5485.402914	25.456307
163.986830	5478.344205	25.461325
164.457579	5498.699514	25.466343
164.408557	5510.743546	25.471360
164.816976	5548.379989	25.476378
164.756323	5543.611494	25.481395
164.819760	5544.687700	25.486413
165.029777	5561.214356	25.491431
165.465770	5569.190330	25.496448
165.553945	5576.785963	25.501466
166.115093	5601.112865	25.506483
166.167344	5596.818633	25.511501
166.623852	5605.281809	25.516519
166.647307	5622.297645	25.521536
166.928394	5607.353298	25.526554
167.610461	5619.701440	25.531571
167.144466	5641.438542	25.536589
167.420088	5618.513604	25.541607
167.646558	5620.640488	25.546624
167.945323	5643.321754	25.551642
168.348817	5620.517425	25.556659
168.232719	5639.809199	25.561677
168.349993	5640.305229	25.566695
168.665735	5646.512838	25.571712
168.612087	5641.012017	25.576730
168.381445	5631.063065	25.581747
168.728705	5648.504190	25.586765
168.921294	5671.038859	25.591783
169.038102	5671.604657	25.596800
169.401294	5664.270693	25.601818
169.403891	5685.151258	25.606835
169.439767	5685.580027	25.611853
169.602075	5696.602621	25.616871
169.428346	5718.396268	25.621888
169.525597	5723.724212	25.626906
169.839887	5729.264735	25.631923
170.013643	5753.233420	25.636941
170.267792	5754.560429	25.641959
170.668987	5772.554230	25.646976
170.755997	5780.643490	25.651994
171.461470	5788.162824	25.657011
171.747642	5791.990594	25.662029
171.972212	5803.700655	25.667047
172.060248	5800.352872	25.672064
171.804254	5800.110536	25.677082
172.610852	5796.630642	25.682100
172.644004	5810.753575	25.687117
172.563155	5788.432202	25.692135
172.274472	5802.644133	25.697152
172.502493	5837.186097	25.702170
172.787058	5824.319046	25.707188
173.071383	5831.268578	25.712205
173.141573	5852.409869	25.717223
173.052768	5867.969628	25.722240
173.124870	5855.922351	25.727258
173.391949	5892.509685	25.732276
173.659451	5900.397520	25.737293
174.228656	5907.137801	25.742311
174.092109	5908.302985	25.747328
174.151998	5910.296004	25.752346
174.604773	5926.999095	25.757364
174.424386	5944.525372	25.762381
174.600309	5951.826749	25.767399
174.990898	5955.613291	25.772416
174.711607	5941.558120	25.777434
175.301571	5972.016687	25.782452
174.942612	5979.499769	25.787469
175.114943	5992.244658	25.792487
175.613807	6007.996453	25.797504
175.889844	6007.740622	25.802522
176.282590	6024.207655	25.807540
175.836120	6056.822031	25.812557
176.501550	6044.371828	25.817575
176.980748	6038.907639	25.822592
177.178680	6073.133419	25.827610
177.210516	6087.976954	25.832628
177.430573	6075.606220	25.837645
177.554812	6059.499866	25.842663
177.781145	6086.726763	25.847680
177.842526	6098.260449	25.852698
178.085316	6104.379894	25.857716
178.348307	6112.097703	25.862733
178.494007	6108.119806	25.867751
178.687522	6119.384413	25.872768
178.723495	6146.136920	25.877786
178.845063	6123.556014	25.882804
178.952798	6142.663382	25.887821
179.227383	6150.355671	25.892839
179.579885	6171.050321	25.897856
179.776652	6176.114319	25.902874
180.144780	6185.253888	25.907892
180.124819	6193.119284	25.912909
180.229301	6185.587647	25.917927
180.682797	6196.441213	25.922944
180.579470	6221.562790	25.927962
180.761212	6216.868221	25.932980
180.876843	6210.300559	25.937997
180.768487	6214.661378	25.943015
181.237010	6239.740866	25.948032
181.320852	6255.509906	25.953050
181.657111	6267.021137	25.958068
181.817107	6264.664210	25.963085
182.073166	6255.471131	25.968103
182.211696	6278.304611	25.973120
182.577544	6310.677809	25.978138
182.864829	6308.703425	25.983156
182.553255	6302.085827	25.988173
182.773194	6312.543379	25.993191
182.914897	6341.732518	25.998208
182.788959	6336.696981	26.003226
183.336540	6331.925395	26.008244
183.427229	6351.032684	26.013261
183.691698	6391.284559	26.018279
183.968587	6374.769945	26.023296
184.148646	6376.457709	26.028314
184.608652	6379.378868	26.033332
184.863823	6411.079945	26.038349
185.032520	6422.967435	26.043367
185.347771	6417.531385	26.048384
185.203886	6424.378689	26.053402
185.455486	6422.588157	26.058420
185.616578	6431.012792	26.063437
185.759661	6441.212630	26.068455
185.935640	6440.475245	26.073472
185.779664	6457.350360	26.078490
186.128003	6450.254730	26.083508
186.333083	6451.027253	26.088525
186.386734	6484.800562	26.093543
186.723653	6506.807815	26.098560
186.701918	6506.838209	26.103578
186.771662	6488.166137	26.108596
187.016870	6529.228325	26.113613
186.822825	6547.338696	26.118631
187.672246	6532.340514	26.123648
187.675991	6560.093253	26.128666
188.168109	6545.945517	26.133684
188.335432	6574.591036	26.138701
188.392803	6594.438459	26.143719
188.774848	6589.535468	26.148736
188.181934	6589.190893	26.153754
188.948691	6588.476375	26.158772
189.234955	6622.824213	26.163789
189.271667	6640.170893	26.168807
189.679768	6628.320684	26.173824
189.464604	6643.665057	26.178842
189.655726	6655.068257	26.183860
190.132546	6675.588295	26.188877
190.293902	6677.879644	26.193895
190.708028	6665.196428	26.198912
190.780512	6686.064026	26.203930
190.848542	6716.550831	26.208948
190.994877	6711.626110	26.213965
191.101604	6713.457933	26.218983
191.551463	6734.333331	26.224000
191.481225	6747.898141	26.229018
191.638955	6754.090958	26.234036
191.778045	6761.420064	26.239053
191.928424	6768.229135	26.244071
192.275665	6786.094423	26.249088
192.190124	6794.145781	26.254106
192.480789	6818.326733	26.259124
192.833774	6851.409956	26.264141
192.969605	6840.399556	26.269159
193.618438	6838.210626	26.274176
193.387204	6863.545335	26.279194
193.440371	6862.339971	26.284212
193.752702	6892.924173	26.289229
193.999495	6890.781975	26.294247
194.339236	6901.203590	26.299264
194.303243	6918.370834	26.304282
194.793103	6915.645095	26.309300
195.261652	6940.746181	26.314317
195.488511	6938.515527	26.319335
195.891311	6938.864412	26.324352
195.716568	6940.471865	26.329370
195.800977	6949.333915	26.334388
195.998709	6963.809487	26.339405
196.033360	6963.871516	26.344423
196.561171	6994.223043	26.349440
196.633832	6996.968130	26.354458
196.621340	6990.965085	26.359476
196.837699	7011.022625	26.364493
197.053555	7039.816510	26.369511
197.152094	7043.854358	26.374528
197.314428	7030.324927	26.379546
197.731061	7055.645828	26.384564
197.817262	7064.345813	26.389581
197.836079	7062.568471	26.394599
198.283929	7090.342879	26.399616
198.347798	7113.427348	26.404634
198.629351	7118.265410	26.409652
198.947040	7113.958801	26.414669
199.025296	7120.028654	26.419687
199.360267	7130.676833	26.424704
199.547930	7158.819989	26.429722
199.912552	7160.901423	26.434740
199.895006	7144.375585	26.439757
200.228919	7162.052926	26.444775
200.497467	7169.379340	26.449792
200.486947	7188.132665	26.454810
200.735606	7179.350960	26.459828
201.030699	7167.826150	26.464845
200.600811	7205.836233	26.469863
201.303443	7221.362648	26.474880
201.454545	7209.548559	26.479898
201.580538	7219.193772	26.484916
202.066112	7235.752275	26.489933
202.357148	7256.529397	26.494951
202.157557	7248.573797	26.499968
202.019936	7238.891956	26.504986
202.598992	7260.197959	26.510004
202.776825	7280.598482	26.515021
202.775687	7305.865566	26.520039
203.252571	7298.600656	26.525056
203.137501	7312.475377	26.530074
203.414664	7335.459173	26.535092
203.536902	7345.694152	26.540109
203.558284	7361.398629	26.545127
204.052715	7364.863983	26.550144
204.493289	7383.598137	26.555162
204.729932	7412.805480	26.560180
205.283078	7401.944670	26.565197
205.278187	7408.660758	26.570215
205.512608	7414.446614	26.575232
205.549712	7439.817062	26.580250
205.838626	7435.754529	26.585268
205.797362	7445.596835	26.590285
205.965879	7468.635791	26.595303
206.185367	7466.431482	26.600320
206.740262	7478.122874	26.605338
206.508182	7495.464902	26.610356
207.224260	7497.991940	26.615373
207.120954	7518.596728	26.620391
207.311413	7528.803230	26.625408
207.512832	7527.826513	26.630426
207.655298	7546.647131	26.635444
208.386866	7559.359965	26.640461
208.362522	7551.218536	26.645479
208.665139	7552.553840	26.650496
208.837981	7581.642884	26.655514
209.087791	7587.560930	26.660532
209.211183	7588.239905	26.665549
209.175196	7610.178016	26.670567
209.571484	7614.226670	26.675584
209.528578	7633.571018	26.680602
209.713304	7646.249842	26.685620
210.025114	7631.746212	26.690637
210.459394	7669.608728	26.695655
210.752827	7676.253589	26.700672
210.769700	7678.220472	26.705690
211.130222	7687.508269	26.710708
211.136665	7701.131717	26.715725
210.927268	7703.392727	26.720743
211.269462	7724.344726	26.725760
211.275495	7742.256455	26.730778
211.475784	7741.565004	26.735796
211.808729	7771.109923	26.740813
211.704435	7792.090104	26.745831
212.254266	7783.574897	26.750848
212.377097	7823.380929	26.755866
212.512116	7851.098509	26.760884
213.002978	7857.940792	26.765901
212.981427	7856.251148	26.770919
213.357010	7873.026174	26.775936
214.075889	7892.405638	26.780954
214.354239	7922.392227	26.785972
214.634042	7910.309058	26.790989
215.034578	7899.647959	26.796007
215.253775	7916.879662	26.801024
215.297385	7915.334393	26.806042
215.292478	7920.321235	26.811060
215.661520	7927.879087	26.816077
215.815494	7948.570301	26.821095
215.689073	7940.399858	26.826112
215.779713	7945.578835	26.831130
215.686027	7982.059757	26.836148
216.285377	7985.448850	26.841165
216.204211	7992.913368	26.846183
216.178697	7995.314149	26.851200
216.639336	8032.495885	26.856218
216.735520	8059.416150	26.861236
217.098159	8058.660059	26.866253
217.496220	8058.136747	26.871271
217.766810	8082.347380	26.876288
218.295144	8104.519780	26.881306
218.274559	8108.223181	26.886324
218.879269	8101.593615	26.891341
219.029232	8124.219977	26.896359
219.428447	8116.374492	26.901376
219.582326	8127.646700	26.906394
219.832467	8156.052242	26.911412
220.006307	8164.511932	26.916429
219.951055	8163.329502	26.921447
220.378756	8172.448975	26.926464
220.714268	8172.935416	26.931482
220.729490	8195.586505	26.936500
221.096981	8188.926790	26.941517
221.261757	8209.366116	26.946535
221.389932	8202.812091	26.951552
221.474070	8209.556340	26.956570
221.428897	8249.875562	26.961588
221.746222	8251.766098	26.966605
221.688315	8255.084277	26.971623
222.040040	8263.065715	26.976640
222.135424	8300.772312	26.981658
222.545748	8324.588496	26.986676
222.859712	8326.631598	26.991693
222.992648	8331.205946	26.996711
223.163570	8344.091596	27.001728
223.580802	8375.305984	27.006746
223.758086	8388.282765	27.011764
224.121106	8392.552915	27.016781
224.221624	8392.979742	27.021799
224.797568	8433.475615	27.026816
225.085384	8445.798605	27.031834
225.033090	8439.174276	27.036852
225.340916	8439.680265	27.041869
225.446133	8471.583547	27.046887
225.927241	8492.625456	27.051904
226.091138	8486.336339	27.056922
226.134146	8506.440182	27.061940
226.261203	8509.878283	27.066957
226.745992	8510.833100	27.071975
226.868873	8530.807214	27.076992
227.287697	8561.219160	27.082010
227.112772	8569.909960	27.087028
227.528913	8571.054904	27.092045
227.707295	8595.771440	27.097063
228.018326	8591.109544	27.102080
228.454679	8589.863186	27.107098
228.348674	8623.789543	27.112116
228.938292	8603.239274	27.117133
228.971672	8622.781730	27.122151
229.008077	8657.676206	27.127168
229.741683	8644.959098	27.132186
229.600508	8642.698441	27.137204
229.743703	8662.040081	27.142221
230.370439	8664.364704	27.147239
229.687941	8668.746237	27.152256
230.466120	8685.786404	27.157274
230.389029	8711.306931	27.162292
230.659874	8716.505220	27.167309
230.871445	8736.713034	27.172327
230.858959	8739.466193	27.177344
231.348029	8749.106702	27.182362
231.558854	8771.722363	27.187380
231.887996	8805.340149	27.192397
232.034778	8814.623761	27.197415
232.182409	8811.458457	27.202432
232.705568	8818.896765	27.207450
232.579155	8860.455684	27.212468
232.782152	8872.604785	27.217485
233.354013	8876.431011	27.222503
233.403480	8880.532572	27.227520
233.967876	8908.591411	27.232538
233.952623	8925.744025	27.237556
234.325828	8937.265689	27.242573
234.858612	8948.790924	27.247591
234.592648	8973.396378	27.252608
235.056074	8971.349249	27.257626
235.089357	8977.803726	27.262644
235.476383	8995.980001	27.267661
235.831887	9026.031553	27.272679
235.944014	9041.417119	27.277696
236.456452	9029.710520	27.282714
236.660564	9047.514606	27.287732
236.683912	9082.738247	27.292749
236.941650	9099.518301	27.297767
236.966844	9091.593150	27.302784
237.536865	9103.333665	27.307802
237.612339	9117.634517	27.312820
237.937491	9149.023173	27.317837
238.047504	9165.541799	27.322855
238.468243	9167.418513	27.327872
238.646657	9178.229027	27.332890
239.056426	9204.544953	27.337908
239.550537	9221.257728	27.342925
239.876222	9197.776250	27.347943
239.834113	9195.170709	27.352960
240.509451	9219.613149	27.357978
240.671640	9231.562913	27.362996
240.700587	9230.871355	27.368013
240.843077	9251.137711	27.373031
240.885821	9253.307660	27.378048
241.143601	9245.629122	27.383066
241.309059	9280.061795	27.388084
241.976659	9296.938168	27.393101
242.113118	9294.125105	27.398119
242.152187	9295.960927	27.403136
242.790205	9303.113486	27.408154
242.739590	9329.982984	27.413172
242.853297	9332.135706	27.418189
243.087408	9332.571993	27.423207
243.183755	9334.073856	27.428224
243.464232	9361.714136	27.433242
243.769491	9390.245114	27.438260
243.939974	9404.308418	27.443277
243.896468	9403.658753	27.448295
243.827860	9433.226660	27.453312
244.051988	9442.091447	27.458330
244.615258	9475.103307	27.463348
244.817779	9492.942814	27.468365
245.125882	9511.268982	27.473383
245.062319	9538.136246	27.478400
245.577950	9556.087134	27.483418
245.804045	9551.129451	27.488436
245.555691	9565.136074	27.493453
246.353491	9582.869456	27.498471
246.258887	9619.763877	27.503488
246.452253	9629.305707	27.508506
247.041345	9648.886790	27.513524
247.338169	9671.068928	27.518541
247.606448	9701.251959	27.523559
247.762370	9722.390981	27.528576
248.338664	9712.562101	27.533594
248.287871	9732.042644	27.538612
248.611481	9752.723161	27.543629
248.827015	9774.140681	27.548647
248.890015	9799.216060	27.553664
249.408487	9789.433706	27.558682
249.360908	9817.124255	27.563700
249.760341	9834.259749	27.568717
250.176123	9849.594356	27.573735
250.604341	9863.634389	27.578752
250.774008	9857.891195	27.583770
251.214415	9888.876328	27.588788
251.462721	9909.774281	27.593805
251.709321	9920.815058	27.598823
252.059743	9925.924199	27.603840
252.623309	9922.960908	27.608858
252.944910	9937.447105	27.613876
252.989227	9938.832385	27.618893
253.409947	9954.355315	27.623911
253.168643	9979.835700	27.628928
253.306353	9983.914304	27.633946
253.865569	9979.094428	27.638964
253.594642	10004.315882	27.643981
254.154509	10032.646058	27.648999
254.080713	10060.339786	27.654016
254.220999	10054.773873	27.659034
254.583943	10072.023563	27.664052
254.567371	10117.971440	27.669069
255.143938	10138.869022	27.674087
255.268865	10135.200739	27.679104
255.689383	10147.210123	27.684122
255.679137	10187.402479	27.689140
256.079102	10213.646087	27.694157
256.792794	10222.190977	27.699175
256.588916	10244.873319	27.704192
257.441088	10251.290693	27.709210
257.433382	10248.554055	27.714228
257.585997	10273.920206	27.719245
258.176647	10300.774406	27.724263
258.142727	10313.029921	27.729280
258.470403	10329.973012	27.734298
258.443260	10331.962463	27.739316
258.450749	10362.351310	27.744333
259.054585	10394.433654	27.749351
259.395912	10400.108428	27.754368
259.501121	10406.541364	27.759386
259.830636	10431.071170	27.764404
259.994076	10461.415536	27.769421
260.527736	10476.048357	27.774439
260.622264	10476.970896	27.779456
261.145569	10506.340609	27.784474
261.401847	10507.846093	27.789492
261.645004	10537.845033	27.794509
262.031508	10547.179852	27.799527
262.289816	10561.881875	27.804544
262.554611	10571.861452	27.809562
262.936048	10583.293161	27.814580
262.809562	10584.735861	27.819597
263.288826	10599.169833	27.824615
263.262745	10622.678766	27.829632
263.722883	10624.459354	27.834650
264.148355	10629.633518	27.839668
264.097268	10652.904806	27.844685
264.568841	10676.604927	27.849703
264.502392	10681.038819	27.854720
264.591271	10682.228543	27.859738
264.715974	10715.281574	27.864756
265.177917	10748.311252	27.869773
265.225081	10747.941937	27.874791
265.748666	10770.209453	27.879808
266.007244	10775.260001	27.884826
266.444584	10802.501144	27.889844
266.502722	10835.275549	27.894861
266.884653	10836.082884	27.899879
266.808700	10863.688568	27.904896
267.464735	10883.411358	27.909914
267.714631	10900.822412	27.914932
267.892559	10927.254334	27.919949
268.241034	10942.226173	27.924967
268.586486	10943.275065	27.929984
268.609319	10988.384763	27.935002
269.268061	11009.440849	27.940020
269.297361	11017.634495	27.945037
269.549318	11027.780323	27.950055
270.061547	11055.629453	27.955072
270.141253	11052.059018	27.960090
270.794705	11086.882882	27.965108
270.860183	11094.660193	27.970125
271.402034	11093.746756	27.975143
271.738716	11135.213054	27.980160
271.756990	11145.596068	27.985178
272.158823	11149.768398	27.990196
272.103521	11168.734702	27.995213
272.599712	11170.166742	28.000231
272.929983	11205.716969	28.005248
273.183574	11218.340018	28.010266
273.540182	11231.854296	28.015284
273.564011	11237.968596	28.020301
274.162352	11253.258647	28.025319
274.147793	11268.721653	28.030336
274.445862	11276.811950	28.035354
274.841325	11277.564297	28.040372
274.881206	11330.826630	28.045389
275.145725	11346.998244	28.050407
275.474750	11358.760563	28.055424
275.815699	11367.132916	28.060442
276.299255	11380.388455	28.065460
276.248839	11398.969027	28.070477
276.678899	11410.004951	28.075495
276.898088	11439.184797	28.080512
277.256275	11464.837912	28.085530
277.551342	11461.052991	28.090548
277.895153	11476.104088	28.095565
278.015742	11487.329834	28.100583
278.434262	11512.666631	28.105600
278.677198	11537.618128	28.110618
278.872909	11544.944041	28.115636
279.518367	11554.443847	28.120653
279.892882	11557.279287	28.125671
280.045706	11595.606528	28.130688
280.010044	11595.979533	28.135706
280.091891	11613.102460	28.140724
280.314701	11624.839199	28.145741
280.475017	11645.751606	28.150759
280.974647	11656.210611	28.155776
281.196872	11656.552040	28.160794
281.926111	11668.190176	28.165812
282.048034	11695.905611	28.170829
281.986036	11719.589093	28.175847
282.283234	11733.489366	28.180864
282.499266	11735.557765	28.185882
282.983415	11753.209124	28.190900
282.909179	11793.679203	28.195917
283.304953	11803.882904	28.200935
283.836238	11818.562258	28.205952
283.720948	11833.647790	28.210970
284.100682	11840.238402	28.215988
284.221849	11864.794597	28.221005
284.548321	11890.503264	28.226023
284.820649	11908.907430	28.231040
284.863864	11959.838774	28.236058
285.351156	11960.613798	28.241076
285.298334	11978.050045	28.246093
285.650371	12015.603314	28.251111
286.221961	12043.093811	28.256128
286.405929	12066.310992	28.261146
286.899686	12089.526655	28.266164
287.487339	12116.777509	28.271181
287.631633	12138.046124	28.276199
288.195504	12142.303810	28.281216
288.444814	12165.917613	28.286234
288.893748	12185.419424	28.291252
289.122406	12209.373867	28.296269
289.392025	12230.298915	28.301287
289.523796	12239.115137	28.306304
289.724282	12262.519725	28.311322
289.884603	12271.156364	28.316340
290.108898	12309.222994	28.321357
290.446883	12322.612080	28.326375
290.828896	12343.323340	28.331392
291.214652	12359.479888	28.336410
291.757841	12370.841259	28.341428
291.797894	12409.178048	28.346445
291.648217	12440.460213	28.351463
292.133225	12459.404953	28.356480
292.445017	12467.972558	28.361498
292.967675	12483.962451	28.366516
293.015381	12525.701463	28.371533
293.434044	12554.870871	28.376551
293.948541	12570.466732	28.381568
294.135778	12597.520650	28.386586
294.335400	12597.832750	28.391604
294.649946	12636.857374	28.396621
294.827860	12644.372649	28.401639
295.663752	12672.727308	28.406656
295.752938	12711.612092	28.411674
296.109489	12701.675109	28.416692
296.362090	12721.917446	28.421709
296.702418	12741.829410	28.426727
296.901014	12775.610287	28.431744
297.167605	12791.730238	28.436762
297.825425	12797.927100	28.441780
298.079000	12802.496990	28.446797
298.303512	12831.158548	28.451815
298.653996	12868.078319	28.456832
298.625109	12876.528323	28.461850
299.170746	12866.667141	28.466868
299.479856	12888.255365	28.471885
299.463177	12926.234857	28.476903
300.324162	12930.008018	28.481920
299.722630	12940.355150	28.486938
300.225265	12950.339466	28.491956
300.260396	12992.788426	28.496973
300.243432	13016.041752	28.501991
300.991629	13024.136565	28.507008
301.167722	13051.972230	28.512026
301.818254	13080.085652	28.517044
302.104502	13096.272777	28.522061
302.480654	13123.991220	28.527079
302.873651	13133.369028	28.532096
303.103254	13158.477300	28.537114
303.574341	13168.730094	28.542132
304.020200	13205.720756	28.547149
304.113569	13199.821170	28.552167
304.618441	13216.808957	28.557184
304.402344	13241.486789	28.562202
304.887318	13250.969220	28.567220
305.334584	13282.482134	28.572237
305.536461	13313.224194	28.577255
305.895870	13312.871777	28.582272
305.816584	13346.304275	28.587290
306.453125	13348.253783	28.592308
306.721592	13366.820977	28.597325
307.038635	13399.230117	28.602343
307.275761	13419.490070	28.607360
307.653392	13437.168763	28.612378
308.080264	13459.064460	28.617396
308.324218	13468.663257	28.622413
308.852809	13486.592806	28.627431
309.413051	13489.278951	28.632448
309.458891	13527.155780	28.637466
309.936257	13538.773085	28.642484
310.357523	13537.577707	28.647501
310.745030	13539.027141	28.652519
311.144676	13569.636176	28.657536
311.139687	13599.478589	28.662554
311.209836	13614.405162	28.667572
311.606607	13622.885290	28.672589
312.058697	13636.905801	28.677607
312.413748	13671.420611	28.682624
312.267426	13699.669127	28.687642
312.603673	13703.953812	28.692660
312.969858	13728.781211	28.697677
312.996044	13754.312423	28.702695
313.461589	13783.537770	28.707712
314.145495	13792.116303	28.712730
314.045455	13803.852826	28.717748
314.667978	13832.197516	28.722765
314.858196	13871.848378	28.727783
315.148917	13877.622573	28.732800
315.243584	13894.339284	28.737818
315.579650	13922.046028	28.742836
315.822286	13946.265468	28.747853
316.261835	14000.529494	28.752871
317.034272	13991.954546	28.757888
316.966260	14001.755680	28.762906
317.366740	14029.529177	28.767924
317.905482	14053.187754	28.772941
318.218404	14064.745943	28.777959
318.549218	14086.218738	28.782976
318.616554	14132.382492	28.787994
319.171559	14149.915275	28.793012
319.219115	14166.208303	28.798029
319.577982	14192.094935	28.803047
319.915708	14197.193371	28.808064
319.785698	14243.164714	28.813082
320.147722	14271.130917	28.818100
320.778528	14283.930425	28.823117
320.761978	14310.225928	28.828135
321.617114	14342.021771	28.833152
321.486521	14352.331391	28.838170
322.162858	14370.674786	28.843188
322.693526	14384.727877	28.848205
322.666205	14412.662525	28.853223
323.115245	14434.543280	28.858240
323.616290	14445.292243	28.863258
323.799085	14453.281072	28.868276
324.087597	14460.990866	28.873293
324.646767	14503.998558	28.878311
324.902840	14496.230349	28.883328
325.097021	14515.693563	28.888346
325.331977	14536.571400	28.893364
325.961352	14547.579716	28.898381
325.874365	14591.710756	28.903399
326.268586	14604.267542	28.908416
326.712933	14627.529706	28.913434
327.096350	14635.873121	28.918452
327.408989	14667.198255	28.923469
327.734453	14684.038383	28.928487
328.206776	14695.877967	28.933504
328.451552	14734.280220	28.938522
328.607878	14748.230014	28.943540
329.066822	14754.332860	28.948557
329.345391	14800.900116	28.953575
329.302785	14836.193788	28.958592
329.688078	14850.321727	28.963610
330.064388	14872.156786	28.968628
330.380660	14889.208227	28.973645
330.728297	14938.851449	28.978663
331.153264	14953.833311	28.983680
331.687183	14969.389689	28.988698
332.059180	14978.616042	28.993716
332.742193	15014.519825	28.998733
332.892255	15045.946612	29.003751
333.139232	15044.479733	29.008768
333.221991	15056.276784	29.013786
333.830490	15074.064896	29.018804
334.541226	15097.817929	29.023821
334.660231	15127.789226	29.028839
334.715520	15143.864496	29.033856
335.105215	15165.546462	29.038874
335.176036	15190.963834	29.043892
335.600254	15221.143316	29.048909
335.869019	15236.940735	29.053927
336.395962	15253.513373	29.058944
336.699261	15278.591493	29.063962
336.850446	15308.163848	29.068980
337.493557	15345.666551	29.073997
337.589501	15347.543312	29.079015
338.189104	15362.558160	29.084032
338.322729	15403.418185	29.089050
338.484813	15436.588202	29.094068
339.073238	15448.913430	29.099085
339.358340	15481.142920	29.104103
339.624347	15512.299319	29.109120
340.442077	15520.008864	29.114138
340.374151	15543.711541	29.119156
340.628495	15576.743685	29.124173
340.936462	15619.178101	29.129191
341.531374	15625.200510	29.134208
341.662347	15649.496101	29.139226
342.038778	15679.967987	29.144244
342.766135	15700.458683	29.149261
342.848490	15721.014988	29.154279
343.306664	15732.493644	29.159296
343.591880	15746.527012	29.164314
343.553868	15773.901604	29.169332
344.250601	15806.008580	29.174349
344.412963	15835.256992	29.179367
344.772037	15844.796425	29.184384
345.238265	15861.797327	29.189402
345.316763	15892.827843	29.194420
345.612570	15916.994170	29.199437
345.869333	15930.892143	29.204455
346.084121	15964.021435	29.209472
346.804990	15982.080373	29.214490
347.015015	16001.679856	29.219508
347.368841	16025.723295	29.224525
347.740735	16063.091232	29.229543
347.746742	16089.204658	29.234560
348.262687	16105.423830	29.239578
348.415715	16146.586665	29.244596
349.230099	16170.445496	29.249613
349.555154	16181.590304	29.254631
349.908435	16200.085280	29.259648
350.265295	16248.590013	29.264666
350.223746	16266.956451	29.269684
350.876450	16282.187163	29.274701
351.327923	16328.911464	29.279719
351.403038	16362.520085	29.284736
351.664350	16378.318269	29.289754
351.953654	16421.931934	29.294772
352.512251	16435.156403	29.299789
352.836881	16481.429312	29.304807
353.076806	16521.018548	29.309824
353.870295	16540.021138	29.314842
353.972403	16551.727824	29.319860
354.508400	16588.510392	29.324877
354.355863	16628.358565	29.329895
355.084327	16644.064075	29.334912
355.503584	16675.618165	29.339930
355.825851	16704.572230	29.344948
356.164230	16728.269392	29.349965
356.638029	16775.188279	29.354983
356.803401	16784.254376	29.360000
357.515810	16820.631666	29.365018
357.625906	16853.915594	29.370036
358.057811	16866.794139	29.375053
358.523539	16902.966511	29.380071
358.675143	16934.812748	29.385088
359.069374	16966.310072	29.390106
359.420959	16988.205644	29.395124
360.035420	17002.697904	29.400141
360.174468	17033.139041	29.405159
360.479176	17077.380735	29.410176
361.097698	17106.795622	29.415194
361.287409	17146.509717	29.420212
362.118073	17154.580396	29.425229
362.103897	17171.373618	29.430247
362.601548	17211.390027	29.435264
363.081099	17225.362622	29.440282
363.459105	17252.090989	29.445300
363.782052	17264.398416	29.450317
364.130758	17295.139523	29.455335
364.047067	17323.723612	29.460352
364.613533	17344.720500	29.465370
364.714350	17374.514534	29.470388
365.300184	17420.920316	29.475405
365.396549	17448.201438	29.480423
365.750095	17469.381808	29.485440
366.189358	17508.496060	29.490458
366.737887	17542.635675	29.495476
367.245964	17572.624416	29.500493
367.866047	17594.287318	29.505511
367.948522	17605.107531	29.510528
368.238193	17621.715479	29.515546
368.678337	17656.632897	29.520564
369.117350	17687.678186	29.525581
369.440881	17696.884149	29.530599
369.417387	17727.476360	29.535616
370.096895	17739.244542	29.540634
370.278752	17772.838424	29.545652
370.179547	17810.237746	29.550669
370.644502	17841.252248	29.555687
371.070349	17879.165476	29.560704
371.531467	17901.630479	29.565722
371.759161	17932.660707	29.570740
372.289729	17967.385751	29.575757
372.690057	17981.717246	29.580775
372.850094	18039.437391	29.585792
373.465286	18071.417298	29.590810
373.363342	18099.556563	29.595828
373.700819	18141.757814	29.600845
374.219988	18181.473576	29.605863
374.430764	18228.884542	29.610880
375.381388	18263.296523	29.615898
375.717164	18293.556192	29.620916
376.211883	18304.400179	29.625933
376.945522	18345.138487	29.630951
377.073351	18399.307896	29.635968
377.722581	18422.042002	29.640986
377.805034	18430.508016	29.646004
378.257725	18451.564524	29.651021
378.775673	18499.379453	29.656039
378.863751	18529.653681	29.661056
379.433527	18544.917549	29.666074
379.719589	18584.267723	29.671092
380.099708	18602.108457	29.676109
380.557787	18632.250825	29.681127
381.116875	18668.348624	29.686144
381.909269	18699.756708	29.691162
382.168219	18731.821971	29.696180
382.559418	18751.402698	29.701197
382.975444	18753.003162	29.706215
383.247693	18810.099072	29.711232
383.385387	18814.529040	29.716250
383.454898	18855.699863	29.721268
384.478560	18863.818325	29.726285
384.698708	18880.768453	29.731303
384.898960	18921.638859	29.736320
385.615385	18940.948575	29.741338
385.878945	18967.953984	29.746356
386.321328	19005.461999	29.751373
386.949711	19022.322768	29.756391
386.781683	19048.250562	29.761408
387.347723	19066.503998	29.766426
387.333053	19108.310379	29.771444
387.860280	19152.966968	29.776461
388.342596	19173.400059	29.781479
388.487140	19188.213047	29.786496
388.982556	19221.846356	29.791514
389.141520	19273.081739	29.796532
390.079853	19316.509188	29.801549
390.525157	19329.333869	29.806567
391.010112	19332.371553	29.811584
391.860267	19356.000580	29.816602
392.248289	19407.729730	29.821620
392.650292	19417.683440	29.826637
392.809357	19422.633350	29.831655
392.776811	19444.269376	29.836672
393.335365	19482.837428	29.841690
393.765142	19512.497449	29.846708
393.759787	19538.274615	29.851725
394.312539	19548.920691	29.856743
394.455882	19579.449371	29.861760
394.970047	19596.359547	29.866778
394.597085	19626.896369	29.871796
395.574886	19670.441179	29.876813
396.152105	19686.491430	29.881831
396.442729	19717.219863	29.886848
396.827278	19749.324676	29.891866
397.076815	19780.843417	29.896884
397.450700	19822.242213	29.901901
397.898339	19845.608996	29.906919
397.892540	19880.042070	29.911936
398.336019	19912.908263	29.916954
398.650350	19962.803926	29.921972
399.341652	19967.744893	29.926989
399.912764	20011.748703	29.932007
399.795453	20069.696730	29.937024
400.632002	20109.062061	29.942042
400.961196	20121.277598	29.947060
401.342041	20155.978396	29.952077
402.009950	20208.195026	29.957095
402.153137	20241.847613	29.962112
402.885405	20270.476984	29.967130
402.950174	20316.455244	29.972148
403.259713	20345.047387	29.977165
403.660242	20360.468582	29.982183
403.479359	20422.454260	29.987200
404.420541	20478.778641	29.992218
404.653702	20503.515359	29.997236
404.911282	20539.791586	30.002253
405.390543	20576.269301	30.007271
405.872957	20629.045972	30.012288
406.492923	20668.196195	30.017306
407.188538	20717.586612	30.022324
407.641167	20742.534919	30.027341
408.208046	20765.697294	30.032359
408.458546	20813.028712	30.037376
408.643956	20840.672750	30.042394
409.482729	20866.522192	30.047412
409.797088	20904.596354	30.052429
410.627660	20934.418136	30.057447
410.978295	20956.809396	30.062464
411.478332	20992.171672	30.067482
411.657511	21023.036009	30.072500
411.889530	21048.722709	30.077517
412.601390	21072.098021	30.082535
412.457109	21108.949471	30.087552
412.844124	21167.874194	30.092570
413.415600	21196.072996	30.097588
413.671220	21224.325598	30.102605
414.108285	21242.068347	30.107623
414.429592	21298.211000	30.112640
415.128861	21347.386718	30.117658
415.473671	21388.039119	30.122676
415.151050	21415.042881	30.127693
416.114266	21457.566975	30.132711
416.549113	21497.682975	30.137728
417.025268	21534.448639	30.142746
417.443090	21584.237486	30.147764
417.758770	21612.510778	30.152781
418.248407	21649.454182	30.157799
418.513060	21695.486781	30.162816
418.705551	21731.741676	30.167834
419.349977	21786.760612	30.172852
419.860535	21821.872256	30.177869
420.288191	21855.334501	30.182887
420.714553	21890.280481	30.187904
421.095450	21930.724880	30.192922
421.250288	21968.627611	30.197940
421.534714	22003.871581	30.202957
422.546011	22039.391249	30.207975
422.808568	22084.301237	30.212992
423.673580	22104.357855	30.218010
424.054149	22106.189953	30.223028
424.659864	22159.217529	30.228045
425.072160	22181.322788	30.233063
425.268478	22212.910105	30.238080
425.762419	22240.494463	30.243098
426.206689	22263.817911	30.248116
426.920224	22299.283273	30.253133
427.671466	22327.760138	30.258151
427.728045	22355.989205	30.263168
428.228564	22358.447885	30.268186
428.822121	22391.759258	30.273204
428.712770	22437.464706	30.278221
429.243066	22457.245973	30.283239
429.503887	22499.854072	30.288256
429.683008	22505.131084	30.293274
430.556400	22548.475251	30.298292
430.678084	22596.067906	30.303309
431.127173	22618.178702	30.308327
431.584793	22646.368812	30.313344
431.643419	22692.896961	30.318362
432.004715	22742.003341	30.323380
432.233641	22796.375331	30.328397
432.987869	22814.139885	30.333415
433.443388	22863.406053	30.338432
434.008978	22918.522141	30.343450
434.401031	22956.165628	30.348468
434.558590	22985.496858	30.353485
435.175577	23016.079719	30.358503
435.696899	23060.030438	30.363520
436.213311	23123.560042	30.368538
437.023302	23129.042050	30.373556
437.244041	23190.881781	30.378573
437.736756	23203.132482	30.383591
438.240157	23241.672637	30.388608
438.569133	23295.056959	30.393626
439.420206	23314.005838	30.398644
439.684475	23356.207203	30.403661
440.403353	23381.911662	30.408679
440.628325	23410.996009	30.413696
440.561414	23461.857467	30.418714
441.387490	23505.281298	30.423732
441.763818	23520.627435	30.428749
442.121296	23548.247526	30.433767
442.727267	23596.843003	30.438784
442.839356	23666.017966	30.443802
443.380150	23694.079428	30.448820
443.980995	23723.620939	30.453837
444.546100	23765.795710	30.458855
444.837533	23793.841771	30.463872
445.232948	23826.433514	30.468890
446.043683	23870.940827	30.473908
445.660748	23912.107422	30.478925
446.222796	23935.448430	30.483943
446.660457	23982.448867	30.488960
446.822171	24046.707475	30.493978
447.787581	24081.887467	30.498996
447.883107	24139.913752	30.504013
448.549751	24169.120382	30.509031
449.289481	24207.529113	30.514048
449.435401	24247.333630	30.519066
450.140234	24293.108288	30.524084
450.372347	24334.391898	30.529101
451.077435	24368.928054	30.534119
451.619683	24383.489181	30.539136
451.919243	24419.205576	30.544154
452.198098	24465.052641	30.549172
452.660836	24501.234187	30.554189
453.107095	24532.519689	30.559207
453.496993	24589.951776	30.564224
453.947333	24613.460387	30.569242
454.726347	24642.534176	30.574260
454.938995	24678.506714	30.579277
455.927200	24704.777327	30.584295
456.271200	24729.069955	30.589312
456.416734	24769.949521	30.594330
456.939660	24810.620210	30.599348
457.101128	24849.878027	30.604365
457.765653	24897.206188	30.609383
457.592230	24935.040534	30.614400
457.719193	24977.227638	30.619418
458.533447	25016.661829	30.624436
459.116092	25067.956922	30.629453
459.429326	25117.475508	30.634471
460.346673	25151.807916	30.639488
460.655670	25227.872454	30.644506
461.350251	25267.216623	30.649524
461.348921	25303.993727	30.654541
461.995318	25321.159076	30.659559
462.624018	25374.565113	30.664576
462.582834	25438.026819	30.669594
463.379091	25480.489359	30.674612
463.755725	25542.726646	30.679629
464.108461	25595.177690	30.684647
464.958877	25631.937802	30.689664
465.216943	25656.933448	30.694682
465.571211	25711.699365	30.699700
466.016157	25773.300215	30.704717
466.663100	25811.390478	30.709735
467.481257	25855.681041	30.714752
467.495425	25911.301658	30.719770
468.285296	25943.352966	30.724788
468.921543	25989.517256	30.729805
469.269583	26059.962343	30.734823
470.457488	26092.373936	30.739840
470.726315	26111.461570	30.744858
471.376996	26151.103607	30.749876
471.677340	26189.524768	30.754893
471.915530	26221.014906	30.759911
472.189368	26273.722337	30.764928
472.888898	26304.368488	30.769946
473.288454	26335.426926	30.774964
473.477359	26397.351437	30.779981
473.833032	26452.893759	30.784999
474.567739	26504.045076	30.790016
474.926742	26532.343122	30.795034
475.539468	26557.962730	30.800052
475.819181	26616.154707	30.805069
476.107536	26680.741404	30.810087
476.668914	26715.484277	30.815104
477.140712	26756.256380	30.820122
477.651732	26803.093252	30.825140
477.999900	26860.757525	30.830157
478.370441	26911.998605	30.835175
479.072708	26960.581522	30.840192
479.542946	26994.625666	30.845210
480.059135	27046.421829	30.850228
480.297993	27120.366493	30.855245
480.995343	27146.223743	30.860263
481.787243	27172.907509	30.865280
482.501107	27226.784688	30.870298
483.345273	27277.956519	30.875316
483.991013	27297.369580	30.880333
484.380470	27326.681058	30.885351
485.037877	27356.538115	30.890368
485.072754	27384.463753	30.895386
485.442275	27420.663763	30.900404
485.546598	27444.802742	30.905421
486.071165	27467.481440	30.910439
486.478586	27506.482401	30.915456
487.048128	27558.782248	30.920474
487.775615	27583.748915	30.925492
488.119809	27631.815708	30.930509
488.257587	27697.276388	30.935527
488.532270	27724.311387	30.940544
489.151808	27770.838087	30.945562
489.383364	27806.670603	30.950580
489.669130	27863.241498	30.955597
490.220100	27935.072230	30.960615
490.878308	27986.116039	30.965632
491.036094	28040.756294	30.970650
491.497496	28092.075790	30.975668
492.102378	28144.693303	30.980685
492.186573	28195.501369	30.985703
492.716473	28257.259582	30.990720
493.336776	28334.761090	30.995738
494.001761	28393.289733	31.000756
494.564431	28440.868508	31.005773
495.225386	28487.778272	31.010791
496.030933	28551.081704	31.015808
496.461039	28616.936029	31.020826
497.360791	28660.040732	31.025844
497.994155	28686.790900	31.030861
497.829424	28750.539211	31.035879
498.465943	28802.065312	31.040896
498.645073	28873.103438	31.045914
499.373603	28904.238369	31.050932
500.088061	28952.386484	31.055949
500.467261	29019.985590	31.060967
501.368947	29077.767759	31.065984
501.903127	29116.155284	31.071002
502.597667	29142.101181	31.076020
503.206879	29200.525075	31.081037
503.422172	29256.399322	31.086055
504.073564	29296.928581	31.091072
504.519128	29347.383850	31.096090
504.710895	29396.092687	31.101108
505.487815	29449.326102	31.106125
506.171299	29491.247885	31.111143
506.585359	29526.981287	31.116160
506.578994	29595.198342	31.121178
507.037936	29649.040061	31.126196
507.690196	29710.963074	31.131213
507.867843	29760.302990	31.136231
508.421186	29808.991120	31.141248
508.783718	29872.322111	31.146266
509.392471	29921.414632	31.151284
510.495261	29965.817077	31.156301
510.912331	30035.350718	31.161319
511.398878	30094.356231	31.166336
511.712374	30125.593468	31.171354
512.152274	30169.008178	31.176372
513.176863	30245.334813	31.181389
513.386760	30296.787584	31.186407
514.130436	30336.550118	31.191424
514.528976	30390.079206	31.196442
515.264551	30430.783337	31.201460
515.873202	30465.208961	31.206477
516.505103	30519.851303	31.211495
517.091364	30549.706733	31.216512
517.353986	30593.495633	31.221530
517.670531	30634.830963	31.226548
518.399576	30659.246644	31.231565
518.539384	30705.387324	31.236583
519.148996	30748.283342	31.241600
519.523068	30802.158437	31.246618
520.178905	30861.138598	31.251636
520.540234	30894.700559	31.256653
520.603951	30957.715781	31.261671
521.703559	31003.383259	31.266688
522.025581	31034.835239	31.271706
522.340861	31094.238377	31.276724
522.773340	31158.530980	31.281741
523.148053	31206.814045	31.286759
523.806769	31261.296559	31.291776
524.459335	31323.023381	31.296794
524.845448	31380.564005	31.301812
525.378023	31422.944427	31.306829
525.811760	31482.947644	31.311847
526.529637	31545.112432	31.316864
527.399910	31618.924745	31.321882
527.684830	31670.659421	31.326900
528.342519	31703.558820	31.331917
528.841826	31766.325198	31.336935
529.652555	31809.739543	31.341952
530.276478	31837.729660	31.346970
530.664772	31891.668872	31.351988
531.106802	31953.189782	31.357005
531.161882	32010.446444	31.362023
532.127825	32078.354900	31.367040
532.263952	32151.823815	31.372058
532.830226	32206.778847	31.377076
533.481095	32246.848172	31.382093
533.821612	32306.879082	31.387111
534.705105	32381.336025	31.392128
535.163164	32449.907151	31.397146
535.499185	32490.871391	31.402164
536.487700	32529.573165	31.407181
536.953352	32592.559446	31.412199
537.707311	32647.112584	31.417216
538.400529	32699.107822	31.422234
538.718358	32767.646565	31.427252
538.979092	32821.227965	31.432269
539.387116	32866.878898	31.437287
540.214001	32923.288580	31.442304
540.744048	33002.018411	31.447322
540.974425	33070.121619	31.452340
541.858597	33111.012546	31.457357
542.147217	33168.530985	31.462375
542.809181	33214.860221	31.467392
543.318851	33278.775579	31.472410
543.810685	33349.584710	31.477428
544.652886	33410.470426	31.482445
545.152277	33463.604210	31.487463
545.612346	33519.271857	31.492480
546.348196	33580.393427	31.497498
546.795286	33622.973139	31.502516
547.267011	33697.901224	31.507533
547.464326	33752.515034	31.512551
548.397624	33833.286440	31.517568
548.954157	33862.821163	31.522586
549.280505	33915.931258	31.527604
550.347023	33970.490523	31.532621
550.580257	34028.216538	31.537639
551.264760	34095.422055	31.542656
551.607995	34138.774254	31.547674
552.248548	34193.155306	31.552692
553.104462	34251.230397	31.557709
553.455890	34319.567703	31.562727
553.833429	34369.121097	31.567744
554.532136	34410.033061	31.572762
554.680172	34483.396161	31.577780
555.403950	34509.979442	31.582797
555.785672	34565.505572	31.587815
556.079644	34629.180637	31.592832
556.526172	34688.956057	31.597850
557.094923	34748.922896	31.602868
557.980587	34799.677774	31.607885
558.251878	34880.465502	31.612903
558.722521	34951.495970	31.617920
559.176176	35011.511107	31.622938
560.133522	35062.826016	31.627956
560.936414	35103.977963	31.632973
561.425508	35167.360842	31.637991
561.748767	35248.526619	31.643008
562.743249	35307.203904	31.648026
562.910708	35366.014823	31.653044
563.811360	35426.392982	31.658061
564.182144	35482.545408	31.663079
564.768105	35534.699258	31.668096
565.841262	35604.771399	31.673114
565.998853	35685.253406	31.678132
566.587137	35726.066746	31.683149
567.087123	35776.171836	31.688167
567.285590	35853.855266	31.693184
568.347382	35911.766120	31.698202
568.818828	35992.816157	31.703220
569.489735	36037.434729	31.708237
569.944782	36103.862180	31.713255
570.441391	36172.684378	31.718272
571.155718	36239.268308	31.723290
571.471978	36307.098415	31.728308
572.416349	36347.500947	31.733325
572.912786	36419.473385	31.738343
573.435753	36494.884485	31.743360
574.292714	36568.331598	31.748378
575.655976	36602.190218	31.753396
576.999747	36625.960453	31.758413
577.386022	36677.869788	31.763431
577.786457	36718.716433	31.768448
578.614732	36756.387357	31.773466
579.069329	36820.501314	31.778484
579.447330	36853.948815	31.783501
580.004814	36902.027957	31.788519
580.553734	36949.660537	31.793536
581.012534	36975.928385	31.798554
581.105524	37025.176441	31.803572
581.887237	37082.597744	31.808589
581.641536	37138.667870	31.813607
582.305705	37192.618727	31.818624
582.914705	37270.707568	31.823642
582.845763	37336.109020	31.828660
583.735087	37396.722950	31.833677
584.112681	37475.718736	31.838695
584.826648	37561.804006	31.843712
585.588392	37614.985789	31.848730
585.532973	37675.400093	31.853748
586.542587	37736.474988	31.858765
587.299805	37831.210808	31.863783
587.611780	37911.342826	31.868800
588.610585	37956.846173	31.873818
589.165731	38022.585714	31.878836
589.502654	38096.730922	31.883853
589.763706	38185.775306	31.888871
590.085835	38259.002105	31.893888
591.200008	38317.063600	31.898906
591.433430	38380.683161	31.903924
592.575191	38438.838328	31.908941
593.306668	38520.194553	31.913959
594.015639	38568.840155	31.918976
595.020198	38600.252830	31.923994
595.396429	38681.677926	31.929012
595.915181	38717.879766	31.934029
596.404590	38787.192913	31.939047
597.020831	38848.642695	31.944064
597.733089	38895.530742	31.949082
597.805578	38964.831373	31.954100
598.549503	39019.052280	31.959117
599.279202	39106.663562	31.964135
599.312147	39173.699167	31.969152
600.000872	39236.757362	31.974170
600.236640	39300.521806	31.979188
601.118193	39389.687424	31.984205
601.277570	39465.773873	31.989223
602.263951	39549.576506	31.994240
602.626989	39616.331992	31.999258
602.622201	39701.858166	32.004276
603.708280	39789.035157	32.009293
604.551533	39858.571717	32.014311
604.794218	39929.132499	32.019328
605.856624	40009.998915	32.024346
606.689222	40094.258715	32.029364
607.077920	40157.802077	32.034381
608.043430	40240.992737	32.039399
608.687653	40322.781804	32.044416
609.643897	40397.007763	32.049434
610.245359	40458.392862	32.054452
610.852075	40513.897116	32.059469
611.393730	40584.376350	32.064487
611.837622	40678.610724	32.069504
612.480643	40754.414382	32.074522
612.847470	40822.502499	32.079540
613.298355	40883.607738	32.084557
613.958929	40959.841774	32.089575
614.896547	41055.944044	32.094592
615.848560	41115.537451	32.099610
616.296496	41179.686944	32.104628
616.835972	41250.459507	32.109645
617.399279	41332.768352	32.114663
617.544016	41427.232767	32.119680
618.723260	41483.399815	32.124698
619.270377	41558.916483	32.129716
619.804945	41638.261205	32.134733
620.472980	41732.170454	32.139751
620.999068	41795.273868	32.144768
621.749308	41859.123300	32.149786
622.045034	41940.172271	32.154804
622.899776	42039.298440	32.159821
623.865108	42111.399208	32.164839
623.786625	42190.926491	32.169856
624.840289	42264.294848	32.174874
625.280327	42338.055252	32.179892
625.924342	42408.442554	32.184909
626.264159	42489.688698	32.189927
626.941006	42590.596011	32.194944
627.729416	42662.365152	32.199962
628.606755	42738.495050	32.204980
629.454883	42789.982624	32.209997
630.119498	42881.145694	32.215015
630.317706	42980.154942	32.220032
630.866448	43052.634418	32.225050
631.559595	43120.882384	32.230068
632.055491	43202.131156	32.235085
633.017216	43256.442364	32.240103
633.898971	43329.764458	32.245120
634.780949	43396.040838	32.250138
635.315060	43454.738595	32.255156
635.622242	43523.591613	32.260173
636.302280	43589.829436	32.265191
636.641375	43657.819028	32.270208
637.249996	43727.705822	32.275226
637.923372	43794.295890	32.280244
638.792387	43884.884036	32.285261
639.205967	43941.396591	32.290279
639.788476	44012.488394	32.295296
640.616658	44083.097929	32.300314
640.949565	44173.428771	32.305332
641.636974	44253.959181	32.310349
642.335469	44316.736557	32.315367
642.835305	44409.339244	32.320384
643.998372	44491.907304	32.325402
644.375541	44554.520723	32.330420
644.963079	44626.179157	32.335437
645.743158	44708.634644	32.340455
646.265217	44787.410968	32.345472
646.952593	44866.589683	32.350490
647.478942	44954.063671	32.355508
647.988784	45049.761826	32.360525
649.078823	45108.881314	32.365543
649.667619	45175.622922	32.370560
650.128548	45250.783803	32.375578
650.955450	45348.202273	32.380596
651.429857	45429.650651	32.385613
652.290336	45513.782352	32.390631
652.755729	45591.305426	32.395648
653.583667	45662.391440	32.400666
654.006805	45743.979106	32.405684
654.153327	45845.885263	32.410701
655.278915	45923.644824	32.415719
656.036259	46019.521784	32.420736
656.815439	46105.664964	32.425754
657.574015	46163.226035	32.430772
658.247593	46253.794883	32.435789
659.418085	46344.957768	32.440807
660.033239	46422.516396	32.445824
660.576237	46472.362830	32.450842
661.177371	46553.261603	32.455860
661.636975	46653.671247	32.460877
662.049427	46722.382975	32.465895
662.595958	46803.187653	32.470912
663.347413	46887.255151	32.475930
664.078733	46988.401591	32.480948
664.478574	47081.188792	32.485965
665.060980	47140.114400	32.490983
665.763598	47237.907421	32.496000
666.592404	47329.693561	32.501018
667.530337	47398.630419	32.506036
668.128251	47497.562988	32.511053
668.958612	47597.888042	32.516071
669.752196	47671.743880	32.521088
670.277252	47740.993310	32.526106
670.760189	47833.281087	32.531124
671.510421	47928.379611	32.536141
672.524150	48001.660446	32.541159
672.953116	48095.612992	32.546176
673.256802	48167.647656	32.551194
674.108387	48247.053557	32.556212
674.555992	48342.838833	32.561229
675.435886	48435.177677	32.566247
676.131511	48527.487410	32.571264
676.757117	48602.590342	32.576282
677.474841	48687.015648	32.581300
678.483831	48751.063941	32.586317
679.000969	48821.960656	32.591335
679.758263	48917.135629	32.596352
680.149560	48990.150489	32.601370
681.082393	49054.146075	32.606388
681.510685	49126.129081	32.611405
682.288758	49212.071966	32.616423
682.745791	49301.128161	32.621440
683.495216	49361.874132	32.626458
684.406687	49452.188581	32.631476
684.815170	49540.445517	32.636493
685.203171	49601.362468	32.641511
685.905582	49709.690275	32.646528
686.678142	49792.665157	32.651546
687.146604	49889.695862	32.656564
687.461404	50000.757758	32.661581
688.357499	50094.892560	32.666599
688.738746	50177.892695	32.671616
689.587558	50270.109831	32.676634
690.473257	50385.453457	32.681652
690.815195	50495.234777	32.686669
691.837566	50581.206675	32.691687
692.345268	50682.305608	32.696704
693.315830	50770.819651	32.701722
694.376040	50868.900830	32.706740
694.605699	50966.639647	32.711757
695.185455	51069.743580	32.716775
696.261533	51186.188046	32.721792
697.003318	51275.086443	32.726810
697.970081	51342.368580	32.731828
698.535522	51452.146912	32.736845
699.348911	51547.095237	32.741863
700.458105	51656.115411	32.746880
700.872445	51745.006902	32.751898
701.683815	51825.119735	32.756916
701.866673	51925.009281	32.761933
702.768643	52029.249504	32.766951
703.188592	52130.446375	32.771968
704.213801	52221.522616	32.776986
704.951106	52307.511454	32.782004
705.284278	52427.430777	32.787021
706.158527	52530.516040	32.792039
707.034867	52626.760541	32.797056
707.431091	52711.938970	32.802074
708.586693	52819.037803	32.807092
709.057788	52930.264588	32.812109
710.310198	53017.071673	32.817127
711.481188	53081.692075	32.822144
711.838362	53170.710139	32.827162
712.815213	53272.917022	32.832180
713.119629	53375.652410	32.837197
714.095204	53461.250143	32.842215
714.520270	53550.748310	32.847232
715.045322	53628.562856	32.852250
716.356947	53730.341012	32.857268
716.598066	53825.492996	32.862285
717.391864	53932.038680	32.867303
718.135613	54012.522377	32.872320
718.811177	54109.139073	32.877338
719.468465	54208.336687	32.882356
719.805414	54299.394259	32.887373
720.992391	54390.930976	32.892391
721.572078	54493.181462	32.897408
722.168524	54610.515497	32.902426
722.699424	54693.589370	32.907444
722.985011	54778.656180	32.912461
723.954038	54893.788803	32.917479
724.943932	55000.352187	32.922496
725.478253	55090.894425	32.927514
726.137666	55162.122744	32.932532
726.597318	55261.503668	32.937549
727.399681	55378.189204	32.942567
728.229373	55477.472214	32.947584
728.803742	55563.347636	32.952602
729.888772	55637.318754	32.957620
730.425872	55748.636071	32.962637
731.313414	55846.041364	32.967655
731.989182	55959.560824	32.972672
732.311216	56049.586599	32.977690
733.140333	56152.341603	32.982708
733.601970	56258.828509	32.987725
734.527641	56355.446624	32.992743
735.249479	56467.817881	32.997760
735.684046	56589.733127	33.002778
736.312615	56691.923868	33.007796
736.978231	56802.461468	33.012813
737.667940	56934.736213	33.017831
738.484983	57039.671275	33.022848
739.171560	57158.623144	33.027866
740.338772	57273.459038	33.032884
741.115793	57393.458845	33.037901
741.852365	57509.795150	33.042919
743.198288	57631.635850	33.047936
743.655342	57744.797364	33.052954
744.509522	57819.434030	33.057972
745.227043	57936.502608	33.062989
745.950833	58058.158031	33.068007
746.838481	58174.264793	33.073024
747.141048	58278.160393	33.078042
748.190730	58374.047621	33.083060
748.989024	58495.320633	33.088077
749.584379	58608.723310	33.093095
750.458757	58730.408542	33.098112
751.282028	58836.735905	33.103130
751.984789	58929.978714	33.108148
752.784085	59060.164405	33.113165
753.561934	59179.012247	33.118183
754.202897	59280.462386	33.123200
755.251768	59400.214619	33.128218
755.788100	59505.803085	33.133236
756.567565	59627.667454	33.138253
757.080781	59750.846649	33.143271
758.095166	59864.477959	33.148288
758.707171	59980.874598	33.153306
759.667400	60066.971283	33.158324
760.468202	60199.420076	33.163341
760.983961	60327.088978	33.168359
761.867608	60422.034027	33.173376
762.594167	60544.740539	33.178394
763.606378	60647.962578	33.183412
763.854814	60769.769937	33.188429
764.397792	60889.981158	33.193447
765.575417	61002.138526	33.198464
766.469300	61131.860782	33.203482
767.433501	61258.899135	33.208500
768.296706	61363.432309	33.213517
769.065757	61474.933046	33.218535
769.994018	61568.441622	33.223552
770.565557	61692.299304	33.228570
771.517407	61800.807773	33.233588
772.269635	61911.580629	33.238605
773.058000	62012.413573	33.243623
774.023696	62131.810364	33.248640
774.651901	62240.728549	33.253658
774.986040	62332.891553	33.258676
775.675822	62430.930559	33.263693
776.499264	62564.257004	33.268711
777.745893	62673.625227	33.273728
778.070876	62779.992589	33.278746
779.165676	62862.097469	33.283764
780.419928	62958.187752	33.288781
780.999656	63078.665064	33.293799
782.032056	63168.447678	33.298816
782.458720	63267.039784	33.303834
782.960239	63371.440830	33.308852
783.340391	63473.454477	33.313869
784.057403	63576.544323	33.318887
785.101155	63674.606733	33.323904
785.306037	63801.818046	33.328922
786.109793	63937.368844	33.333940
786.901835	64056.268415	33.338957
787.510227	64166.963576	33.343975
788.499855	64278.892064	33.348992
788.944745	64423.195891	33.354010
790.046341	64552.577089	33.359028
790.753668	64656.148026	33.364045
791.577104	64783.693106	33.369063
792.381664	64924.641751	33.374080
793.138123	65065.978546	33.379098
793.848460	65176.055550	33.384116
794.654222	65301.438781	33.389133
795.569787	65444.673407	33.394151
796.425946	65564.291716	33.399168
796.988152	65698.294899	33.404186
797.696783	65822.028646	33.409204
798.749248	65953.607494	33.414221
799.108864	66099.289858	33.419239
800.439653	66242.758558	33.424256
801.858110	66354.886723	33.429274
802.723783	66465.747747	33.434292
803.885686	66605.384688	33.439309
804.593005	66714.831985	33.444327
805.295891	66829.881156	33.449344
806.021958	66967.272637	33.454362
807.076852	67072.852739	33.459380
808.050817	67175.899267	33.464397
808.495388	67315.185351	33.469415
809.394195	67446.008910	33.474432
810.004510	67553.776210	33.479450
810.623680	67665.259607	33.484468
811.444497	67798.064227	33.489485
812.335416	67931.585093	33.494503
813.058403	68069.856745	33.499520
813.910140	68205.775386	33.504538
814.462424	68335.871561	33.509556
815.390623	68462.075540	33.514573
815.881109	68585.292851	33.519591
816.770553	68724.451682	33.524608
817.647486	68862.564087	33.529626
818.457052	68992.470143	33.534644
819.700341	69100.703561	33.539661
820.648194	69227.111213	33.544679
821.696877	69353.945515	33.549696
822.429286	69499.944163	33.554714
823.228005	69609.347322	33.559732
824.063319	69747.029887	33.564749
824.592189	69882.570187	33.569767
825.929562	69992.556539	33.574784
826.754026	70108.444556	33.579802
827.517068	70217.673428	33.584820
828.768893	70338.537262	33.589837
829.310253	70450.699533	33.594855
830.197336	70559.941309	33.599872
830.928680	70690.332305	33.604890
831.850277	70800.442110	33.609908
832.838856	70915.049308	33.614925
833.243537	71016.609183	33.619943
833.906005	71134.679214	33.624960
834.502425	71261.738777	33.629978
835.036413	71372.136849	33.634996
836.072730	71484.722356	33.640013
836.475953	71598.753393	33.645031
837.636509	71741.314250	33.650048
838.165910	71884.454484	33.655066
838.868789	72000.562624	33.660084
839.744865	72124.489356	33.665101
840.296792	72272.414817	33.670119
841.230334	72417.666952	33.675136
841.895287	72542.914518	33.680154
842.834421	72686.593161	33.685172
843.805330	72821.200373	33.690189
844.779620	72959.019968	33.695207
845.494157	73080.089306	33.700224
846.411200	73228.776777	33.705242
846.922497	73393.637323	33.710260
848.087379	73536.494005	33.715277
848.897158	73674.661530	33.720295
849.967050	73809.049942	33.725312
850.534516	73968.556144	33.730330
851.319914	74120.471128	33.735348
852.488178	74257.135155	33.740365
853.105263	74393.992235	33.745383
854.105739	74557.073599	33.750400
855.050003	74689.578561	33.755418
855.545445	74848.091400	33.760436
856.646802	74990.917639	33.765453
857.416993	75147.193011	33.770471
858.571925	75304.291303	33.775488
859.413058	75445.158894	33.780506
860.013965	75593.605022	33.785524
861.272672	75727.512569	33.790541
862.092736	75889.438561	33.795559
863.273224	76043.097797	33.800576
864.521252	76177.376670	33.805594
865.307022	76291.698279	33.810612
866.372467	76431.245134	33.815629
867.045761	76590.468594	33.820647
867.841932	76710.349550	33.825664
869.013388	76854.865014	33.830682
869.269462	77007.380910	33.835700
870.342657	77143.395811	33.840717
870.980367	77278.585416	33.845735
871.701276	77419.820815	33.850752
872.877577	77583.142501	33.855770
873.480132	77725.980505	33.860788
874.586427	77866.332974	33.865805
875.232340	78023.870103	33.870823
876.287704	78173.517301	33.875840
877.457673	78295.248894	33.880858
878.413027	78455.217250	33.885876
879.239960	78603.684439	33.890893
880.198993	78737.438537	33.895911
881.108498	78876.748419	33.900928
882.330654	79017.146016	33.905946
882.619639	79157.793457	33.910964
883.652539	79299.122218	33.915981
884.783677	79433.497248	33.920999
885.400629	79565.168697	33.926016
886.347729	79710.018260	33.931034
887.146909	79865.696323	33.936052
888.246712	79989.137613	33.941069
888.941813	80127.813982	33.946087
889.905713	80264.701096	33.951104
890.636381	80410.033716	33.956122
891.295233	80547.921714	33.961140
892.299046	80677.043736	33.966157
892.882370	80815.837721	33.971175
893.757857	80937.948720	33.976192
894.435767	81085.577893	33.981210
894.911773	81242.697862	33.986228
896.177391	81370.907760	33.991245
896.852078	81542.336817	33.996263
897.420474	81693.688493	34.001280
898.711577	81850.741396	34.006298
899.377387	82012.737745	34.011316
900.411717	82164.091566	34.016333
901.240723	82303.847327	34.021351
902.541205	82441.134976	34.026368
903.610342	82598.242400	34.031386
904.460765	82756.664850	34.036404
905.759417	82907.176640	34.041421
906.617634	83049.165230	34.046439
907.638973	83184.245140	34.051456
908.593999	83327.237971	34.056474
909.453446	83507.590099	34.061492
910.816734	83633.108184	34.066509
911.553996	83763.329412	34.071527
912.184358	83921.790022	34.076544
913.048002	84082.041492	34.081562
913.860719	84229.289408	34.086580
914.943456	84361.753450	34.091597
915.431153	84530.262683	34.096615
916.564015	84708.042329	34.101632
917.747340	84843.813913	34.106650
918.355973	85007.372096	34.111668
919.169205	85158.371186	34.116685
920.042844	85317.959075	34.121703
921.174893	85469.476967	34.126720
922.064085	85636.112324	34.131738
922.372490	85791.368186	34.136756
923.451696	85963.073845	34.141773
924.527775	86131.200349	34.146791
925.900758	86290.453153	34.151808
927.243041	86446.903002	34.156826
927.895654	86606.359177	34.161844
929.078442	86752.853588	34.166861
930.083962	86914.702150	34.171879
931.009253	87079.747588	34.176896
932.158504	87211.097208	34.181914
932.899851	87369.575953	34.186932
934.050923	87516.289230	34.191949
935.009219	87667.888218	34.196967
935.775750	87818.988370	34.201984
936.958814	87970.286478	34.207002
937.509186	88129.339755	34.212020
937.976247	88286.794395	34.217037
938.970452	88435.285722	34.222055
939.842566	88602.976628	34.227072
940.917748	88754.386222	34.232090
941.496488	88935.681431	34.237108
942.344821	89103.544369	34.242125
943.519501	89259.135988	34.247143
944.103322	89426.823447	34.252160
945.314943	89586.859491	34.257178
945.814413	89773.109874	34.262196
946.663658	89948.280939	34.267213
947.824069	90118.497845	34.272231
948.704134	90299.696879	34.277248
949.545156	90474.379635	34.282266
950.404801	90641.998566	34.287284
951.477873	90797.205809	34.292301
952.298442	90980.634699	34.297319
953.049728	91147.287919	34.302336
954.534235	91304.904859	34.307354
955.292607	91462.762970	34.312372
956.162059	91611.731580	34.317389
957.179084	91789.761604	34.322407
958.119728	91981.639338	34.327424
959.031529	92127.990579	34.332442
959.995984	92294.863453	34.337460
961.122873	92468.450504	34.342477
962.852382	92629.554404	34.347495
963.721028	92790.067406	34.352512
964.544348	92935.552204	34.357530
965.321395	93105.410803	34.362548
966.202245	93292.638390	34.367565
967.481749	93466.099888	34.372583
968.000762	93626.074976	34.377600
969.412029	93768.151465	34.382618
969.871670	93955.770196	34.387636
970.691175	94130.881989	34.392653
971.905448	94309.347516	34.397671
972.941630	94473.584510	34.402688
974.062651	94641.795913	34.407706
975.055087	94825.871442	34.412724
975.786966	94991.674844	34.417741
977.055621	95193.239286	34.422759
978.069404	95360.384757	34.427776
979.611560	95508.424662	34.432794
980.512834	95680.065704	34.437812
982.313524	95851.591110	34.442829
983.337836	96005.403304	34.447847
984.118719	96151.022050	34.452864
985.480876	96289.222490	34.457882
986.668445	96468.594412	34.462900
987.403410	96638.465732	34.467917
988.115736	96789.125272	34.472935
988.795407	96933.182978	34.477952
989.808338	97100.302516	34.482970
990.642590	97291.866473	34.487988
991.327575	97461.061791	34.493005
992.264486	97617.278522	34.498023
993.439634	97794.725251	34.503040
994.024379	97974.163372	34.508058
995.074328	98168.420387	34.513076
996.057888	98322.741220	34.518093
997.137075	98484.098893	34.523111
997.682630	98668.296046	34.528128
998.841743	98852.798397	34.533146
999.952647	99033.758846	34.538164
1001.089367	99227.376808	34.543181
1002.250147	99410.357434	34.548199
1002.970643	99568.464298	34.553216
1003.993887	99770.752429	34.558234
1004.714038	99944.782614	34.563252
1006.298893	100127.584536	34.568269
1007.264870	100322.283700	34.573287
1008.226462	100485.978049	34.578304
1009.318338	100662.863903	34.583322
1010.030923	100858.976470	34.588340
1011.121794	101043.658191	34.593357
1012.232335	101223.710251	34.598375
1013.175221	101391.756466	34.603392
1014.224565	101565.990427	34.608410
1015.323985	101761.166160	34.613428
1015.830079	101949.496335	34.618445
1017.244423	102124.781795	34.623463
1017.698600	102306.361726	34.628480
1018.963632	102482.244096	34.633498
1019.997223	102677.526382	34.638516
1020.815434	102835.814876	34.643533
1021.946973	103000.193868	34.648551
1022.582360	103189.803441	34.653568
1023.590730	103379.264207	34.658586
1024.884144	103559.182343	34.663604
1025.818418	103743.130798	34.668621
1026.655646	103939.012304	34.673639
1027.350715	104113.721062	34.678656
1028.910005	104294.436216	34.683674
1030.031560	104499.924262	34.688692
1030.878596	104683.229037	34.693709
1032.506467	104843.757949	34.698727
1033.168172	105039.651481	34.703744
1034.544660	105231.996698	34.708762
1035.402619	105430.368154	34.713780
1036.537605	105606.768296	34.718797
1037.886946	105779.062865	34.723815
1038.721285	105976.467289	34.728832
1039.550353	106183.068084	34.733850
1040.502448	106377.271132	34.738868
1041.188981	106553.720072	34.743885
1042.301783	106755.947443	34.748903
1043.076426	106957.282383	34.753920
1044.001137	107167.927753	34.758938
1045.150099	107361.808001	34.763956
1045.977125	107580.299464	34.768973
1047.191787	107795.524581	34.773991
1048.478201	107999.353959	34.779008
1049.599775	108189.660696	34.784026
1050.778102	108398.830260	34.789044
1051.831294	108633.061026	34.794061
1053.285367	108816.009624	34.799079
1054.487701	108999.431664	34.804096
1055.213195	109207.770476	34.809114
1056.377775	109426.297469	34.814132
1057.239366	109639.252759	34.819149
1059.107107	109827.864880	34.824167
1059.783962	110021.285270	34.829184
1060.721319	110237.867904	34.834202
1062.046261	110412.603324	34.839220
1062.999178	110630.402496	34.844237
1064.345046	110811.216765	34.849255
1064.856590	111018.439735	34.854272
1066.550616	111231.523596	34.859290
1067.612873	111414.364690	34.864308
1068.745945	111608.962517	34.869325
1069.889154	111790.538814	34.874343
1071.046141	112003.438768	34.879360
1071.874171	112220.410075	34.884378
1072.720302	112412.287022	34.889396
1073.659330	112602.743957	34.894413
1074.908620	112801.777277	34.899431
1076.033281	113015.779876	34.904448
1076.494686	113236.594631	34.909466
1077.868876	113442.427001	34.914484
1078.800390	113638.149366	34.919501
1079.770331	113858.391161	34.924519
1080.644335	114083.388265	34.929536
1082.068799	114277.564371	34.934554
1083.413534	114473.832536	34.939572
1084.042544	114693.516583	34.944589
1085.178437	114924.684625	34.949607
1086.166361	115145.326461	34.954624
1087.464947	115341.988467	34.959642
1088.944461	115534.872178	34.964660
1090.003238	115757.635475	34.969677
1091.168921	115955.527274	34.974695
1091.940119	116137.333135	34.979712
1093.023854	116319.189939	34.984730
1094.247687	116525.222150	34.989748
1094.953720	116730.745923	34.994765
1096.219649	116914.071453	34.999783
1097.323966	117112.577029	35.004800
1098.127746	117323.562043	35.009818
1099.246049	117528.960267	35.014836
1099.526190	117763.739160	35.019853
1100.804696	117962.145967	35.024871
1101.927234	118186.096325	35.029888
1103.157611	118408.789033	35.034906
1104.369898	118615.611324	35.039924
1105.249224	118834.311021	35.044941
1106.711799	119063.077392	35.049959
1107.763099	119294.890952	35.054976
1108.794565	119492.703089	35.059994
1110.429140	119693.685950	35.065012
1111.184394	119928.201599	35.070029
1112.941203	120159.715667	35.075047
1113.600418	120380.440141	35.080064
1114.728388	120586.213657	35.085082
1116.163880	120796.904789	35.090100
1116.953253	121034.781580	35.095117
1117.915801	121259.656757	35.100135
1118.924063	121487.288414	35.105152
1119.919090	121734.741629	35.110170
1120.862726	121956.710995	35.115188
1121.837562	122196.530756	35.120205
1123.215569	122433.967077	35.125223
1124.807912	122654.922349	35.130240
1125.963920	122881.298735	35.135258
1127.333236	123112.317518	35.140276
1128.308566	123356.670531	35.145293
1129.887871	123578.458605	35.150311
1130.905646	123786.756680	35.155328
1131.643942	124033.511442	35.160346
1133.083747	124266.795979	35.165364
1134.326470	124485.148923	35.170381
1135.612250	124709.414374	35.175399
1136.748365	124946.822243	35.180416
1137.463204	125162.124545	35.185434
1138.685322	125404.540217	35.190452
1139.570292	125656.328011	35.195469
1140.931079	125895.898761	35.200487
1142.052021	126129.174532	35.205504
1142.921506	126352.570610	35.210522
1144.125127	126582.744036	35.215540
1144.967706	126817.173677	35.220557
1146.293988	127081.916061	35.225575
1147.478419	127336.076471	35.230592
1148.336511	127573.741177	35.235610
1149.816735	127806.514398	35.240628
1150.461171	128058.501426	35.245645
1152.029015	128325.534124	35.250663
1153.105866	128581.801259	35.255680
1153.952862	128820.935067	35.260698
1155.334400	129075.875973	35.265716
1156.067257	129319.937446	35.270733
1157.379646	129572.447758	35.275751
1158.869133	129826.540577	35.280768
1159.703121	130086.802172	35.285786
1161.564438	130309.898841	35.290804
1162.703183	130556.881685	35.295821
1164.368118	130808.317268	35.300839
1165.391865	131056.159623	35.305856
1166.267640	131298.248520	35.310874
1167.249561	131505.933909	35.315892
1167.977653	131759.002149	35.320909
1169.392276	132005.976319	35.325927
1170.670503	132235.837662	35.330944
1171.854322	132461.647406	35.335962
1173.015638	132693.090496	35.340980
1173.680468	132941.070416	35.345997
1174.590283	133165.599483	35.351015
1175.793372	133410.794283	35.356032
1177.033535	133688.790572	35.361050
1178.481632	133929.626400	35.366068
1179.862789	134164.174991	35.371085
1181.199070	134399.835564	35.376103
1182.492761	134656.966178	35.381120
1183.460067	134902.693111	35.386138
1184.881998	135138.028078	35.391156
1186.156747	135385.165779	35.396173
1187.174230	135635.048019	35.401191
1188.501229	135859.768057	35.406208
1189.389465	136118.346413	35.411226
1190.524595	136366.985228	35.416244
1192.533834	136603.374899	35.421261
1194.127182	136854.616719	35.426279
1195.511573	137087.702853	35.431296
1196.632576	137330.304241	35.436314
1197.765437	137574.287336	35.441332
1198.781090	137806.133670	35.446349
1199.601397	138022.445555	35.451367
1201.161232	138281.500727	35.456384
1201.988661	138548.501156	35.461402
1203.071223	138797.839080	35.466420
1204.589726	139038.143452	35.471437
1205.428599	139307.011813	35.476455
1206.698968	139544.622305	35.481472
1207.659118	139815.414555	35.486490
1208.658636	140067.007137	35.491508
1209.741366	140322.911308	35.496525
1210.885544	140608.564378	35.501543
1212.440591	140873.219225	35.506560
1213.724706	141142.092261	35.511578
1215.167049	141401.520770	35.516596
1216.538957	141666.833358	35.521613
1217.524902	141927.697912	35.526631
1219.131815	142178.470630	35.531648
1220.212117	142440.667565	35.536666
1221.359060	142695.945155	35.541684
1222.796805	142969.600204	35.546701
1223.847666	143245.958692	35.551719
1225.267684	143484.726084	35.556736
1225.831526	143736.886998	35.561754
1227.386914	144017.403517	35.566772
1228.453167	144291.117730	35.571789
1229.288104	144559.204216	35.576807
1230.909708	144833.820112	35.581824
1231.897313	145099.793315	35.586842
1232.891142	145379.779524	35.591860
1234.377698	145650.518541	35.596877
1235.805296	145939.593065	35.601895
1236.747082	146228.420453	35.606912
1238.130115	146497.585307	35.611930
1239.254344	146759.262391	35.616948
1240.693404	147013.952865	35.621965
1242.005268	147305.543195	35.626983
1243.701324	147584.099494	35.632000
1244.545032	147853.249535	35.637018
1245.977447	148114.238983	35.642036
1246.985308	148401.373832	35.647053
1248.002309	148678.605041	35.652071
1249.103614	148945.044923	35.657088
1250.607648	149186.272074	35.662106
1251.568737	149433.817311	35.667124
1253.164896	149717.682371	35.672141
1254.165663	149989.244743	35.677159
1255.653700	150247.729381	35.682176
1256.676168	150527.852725	35.687194
1257.835647	150786.433455	35.692212
1259.025671	151047.306511	35.697229
1260.461392	151309.371083	35.702247
1261.945966	151603.783129	35.707264
1262.822786	151891.246172	35.712282
1263.899525	152152.551599	35.717300
1265.390592	152408.768004	35.722317
1266.729105	152694.131783	35.727335
1268.311304	152983.275173	35.732352
1269.009645	153270.258320	35.737370
1270.469082	153538.765153	35.742388
1271.653486	153809.361343	35.747405
1273.412971	154105.929338	35.752423
1274.290913	154400.159157	35.757440
1275.421420	154691.305465	35.762458
1276.946646	154960.889674	35.767476
1278.116273	155253.238796	35.772493
1278.933300	155559.144211	35.777511
1280.434330	155849.794266	35.782528
1281.567401	156149.576508	35.787546
1282.964490	156430.874435	35.792564
1284.713439	156740.009472	35.797581
1285.616661	157054.652136	35.802599
1287.148047	157330.644969	35.807616
1288.553739	157611.835883	35.812634
1289.382952	157929.161624	35.817652
1291.192508	158237.461347	35.822669
1292.141585	158522.755294	35.827687
1293.735941	158824.904839	35.832704
1294.815295	159135.044599	35.837722
1295.881758	159464.889253	35.842740
1297.245920	159773.096874	35.847757
1298.650181	160061.269790	35.852775
1300.362133	160349.368628	35.857792
1301.219466	160676.872909	35.862810
1302.571951	160999.160369	35.867828
1304.544721	161288.986221	35.872845
1305.679578	161614.955369	35.877863
1307.359522	161899.416983	35.882880
1308.448155	162196.550207	35.887898
1309.345191	162514.560807	35.892916
1310.922709	162811.211843	35.897933
1311.858441	163128.104406	35.902951
1313.377047	163434.576318	35.907968
1314.387984	163766.089000	35.912986
1315.739229	164058.663166	35.918004
1317.255233	164358.304155	35.923021
1318.469316	164691.097420	35.928039
1319.520227	165017.665531	35.933056
1320.913571	165345.448377	35.938074
1322.359226	165643.613066	35.943092
1323.784519	165958.200647	35.948109
1324.904058	166296.553862	35.953127
1326.376230	166596.598608	35.958144
1327.754959	166923.025787	35.963162
1328.959872	167250.029709	35.968180
1330.202949	167554.153662	35.973197
1331.241002	167898.661178	35.978215
1332.691323	168206.625330	35.983232
1333.836236	168526.162868	35.988250
1335.131698	168860.992559	35.993268
1336.397748	169177.292059	35.998285
1337.827144	169482.274213	36.003303
1338.914471	169782.252231	36.008320
1340.188824	170109.875166	36.013338
1341.191650	170444.765177	36.018356
1342.909625	170767.333096	36.023373
1343.752789	171093.625974	36.028391
1345.449383	171411.697522	36.033408
1346.668223	171746.434721	36.038426
1347.846024	172073.986440	36.043444
1349.255149	172406.654165	36.048461
1350.511511	172739.844414	36.053479
1351.946538	173064.708741	36.058496
1353.346050	173417.307759	36.063514
1354.643283	173738.100879	36.068532
1356.612230	174065.180960	36.073549
1357.713688	174405.743453	36.078567
1359.096285	174756.515440	36.083584
1360.743585	175106.916432	36.088602
1361.723171	175430.362374	36.093620
1362.887339	175762.472809	36.098637
1364.213045	176121.462182	36.103655
1365.470699	176476.442665	36.108672
1367.255081	176820.450487	36.113690
1368.687767	177159.252264	36.118708
1370.337475	177494.454555	36.123725
1371.375455	177866.156999	36.128743
1372.740131	178221.488031	36.133760
1374.521358	178549.937108	36.138778
1375.510646	178903.342589	36.143796
1377.165019	179269.915684	36.148813
1378.067906	179630.409555	36.153831
1379.464405	179972.891874	36.158848
1380.715426	180322.964582	36.163866
1382.075056	180685.687843	36.168884
1383.939145	181064.600979	36.173901
1385.052251	181411.886524	36.178919
1386.541024	181776.043154	36.183936
1387.663356	182173.807233	36.188954
1388.926674	182531.152896	36.193972
1390.911342	182883.508288	36.198989
1392.623619	183253.806823	36.204007
1393.916765	183628.124428	36.209024
1395.740116	183991.809979	36.214042
1397.343026	184338.970968	36.219060
1399.029347	184685.739712	36.224077
1400.191745	185055.900590	36.229095
1401.499111	185403.726588	36.234112
1403.188883	185743.977700	36.239130
1404.638121	186090.096631	36.244148
1406.033869	186446.990119	36.249165
1407.367065	186817.223830	36.254183
1408.661880	187156.457442	36.259200
1410.329418	187513.579637	36.264218
1411.975806	187855.780515	36.269236
1413.902961	188175.825602	36.274253
1415.347975	188533.498863	36.279271
1416.687466	188886.139875	36.284288
1418.003758	189215.545228	36.289306
1419.339114	189563.646933	36.294324
1420.733842	189899.060077	36.299341
1422.202415	190243.285128	36.304359
1423.828043	190602.693465	36.309376
1424.950933	190947.487559	36.314394
1426.311813	191285.224712	36.319412
1427.629372	191625.789053	36.324429
1428.830194	191959.456393	36.329447
1430.297394	192309.431726	36.334464
1431.752464	192652.378558	36.339482
1432.586047	193003.909727	36.344500
1433.796661	193329.560441	36.349517
1435.174218	193662.776653	36.354535
1436.414353	194003.392902	36.359552
1437.888371	194355.740350	36.364570
1438.680329	194725.327486	36.369588
1440.319352	195069.806566	36.374605
1441.409932	195446.660957	36.379623
1443.009170	195798.437515	36.384640
1445.058395	196138.360915	36.389658
1446.606040	196487.052337	36.394676
1447.987727	196858.928928	36.399693
1449.703369	197245.910637	36.404711
1450.739685	197585.171169	36.409728
1452.132087	197934.530993	36.414746
1453.806175	198311.065127	36.419764
1455.578781	198687.750254	36.424781
1456.712558	199051.466609	36.429799
1458.212841	199402.086148	36.434816
1459.935872	199760.630990	36.439834
1461.072365	200159.507356	36.444852
1462.688006	200544.240100	36.449869
1464.208789	200910.391256	36.454887
1465.374526	201272.210206	36.459904
1467.142081	201650.347740	36.464922
1468.443145	202029.300738	36.469940
1470.182586	202418.391214	36.474957
1471.315214	202795.255990	36.479975
1472.667203	203168.239644	36.484992
1474.178490	203560.484798	36.490010
1475.481883	203979.416293	36.495028
1476.983008	204353.752869	36.500045
1478.025543	204733.677413	36.505063
1479.868330	205139.093763	36.510080
1481.658553	205535.658760	36.515098
1482.983756	205913.905015	36.520116
1484.769579	206315.109319	36.525133
1485.997404	206727.695463	36.530151
1487.375710	207135.345336	36.535168
1489.150389	207513.335170	36.540186
1490.315840	207924.198730	36.545204
1491.951006	208325.019709	36.550221
1493.234486	208732.401830	36.555239
1495.466034	209141.750121	36.560256
1497.423734	209518.183320	36.565274
1498.622036	209931.959905	36.570292
1500.293903	210305.701407	36.575309
1501.816624	210701.639269	36.580327
1502.875362	211120.028919	36.585344
1504.630689	211506.624998	36.590362
1506.118710	211905.736245	36.595380
1507.640185	212291.003281	36.600397
1509.035710	212698.958647	36.605415
1510.178602	213110.398852	36.610432
1511.720113	213506.982107	36.615450
1513.114267	213925.483033	36.620468
1514.508828	214352.112762	36.625485
1515.744878	214760.917086	36.630503
1517.564838	215159.214409	36.635520
1519.329213	215571.465478	36.640538
1520.576162	216003.943494	36.645556
1521.988670	216413.513693	36.650573
1523.601678	216835.395619	36.655591
1524.476281	217245.769471	36.660608
1526.573970	217657.390984	36.665626
1527.613866	218173.114881	36.670644
1529.325577	218598.391852	36.675661
1530.712149	218991.850402	36.680679
1532.001401	219417.048369	36.685696
1533.646072	219808.994624	36.690714
1535.115208	220224.642284	36.695732
1536.393991	220640.043738	36.700749
1538.270096	221061.240739	36.705767
1539.454499	221483.163207	36.710784
1541.125335	221896.752709	36.715802
1542.479652	222319.615749	36.720820
1543.787303	222737.865686	36.725837
1545.440246	223173.483800	36.730855
1546.852451	223622.122203	36.735872
1548.332476	224032.957789	36.740890
1549.637411	224501.047695	36.745908
1551.226308	224930.028975	36.750925
1552.929781	225374.003923	36.755943
1554.105077	225836.355260	36.760960
1555.938469	226288.592541	36.765978
1557.268718	226746.273914	36.770996
1558.972969	227196.427902	36.776013
1560.847424	227644.371155	36.781031
1562.762592	228097.694122	36.786048
1565.126501	228521.201515	36.791066
1566.294571	228969.063036	36.796084
1568.499858	229410.557420	36.801101
1570.177080	229849.930676	36.806119
1571.715616	230298.091403	36.811136
1573.589087	230714.981453	36.816154
1575.159323	231167.889798	36.821172
1576.778845	231592.876443	36.826189
1578.395490	232021.852787	36.831207
1579.935124	232487.115273	36.836224
1581.334518	232932.742307	36.841242
1582.958659	233363.474206	36.846260
1584.293771	233794.432895	36.851277
1586.025153	234246.715065	36.856295
1587.514174	234704.957046	36.861312
1589.483700	235134.367105	36.866330
1591.115281	235572.318121	36.871348
1592.910767	236016.847647	36.876365
1594.675533	236464.685664	36.881383
1595.943480	236900.109426	36.886400
1597.272441	237349.723686	36.891418
1598.901539	237789.332246	36.896436
1600.122857	238248.898660	36.901453
1602.010417	238708.026146	36.906471
1603.392948	239161.471969	36.911488
1605.128133	239629.288954	36.916506
1606.539074	240082.376763	36.921524
1608.165349	240536.674830	36.926541
1609.863941	240990.149181	36.931559
1611.058649	241473.910716	36.936576
1612.621121	241943.539991	36.941594
1614.162460	242405.197559	36.946612
1615.370250	242871.254951	36.951629
1617.343756	243344.731480	36.956647
1618.562851	243836.343728	36.961664
1620.599461	244299.574744	36.966682
1622.422479	244774.781053	36.971700
1623.956376	245243.609190	36.976717
1625.849407	245730.744974	36.981735
1627.553262	246225.609882	36.986752
1628.959589	246681.582640	36.991770
1630.691151	247154.522276	36.996788
1632.158775	247644.830893	37.001805
1634.048256	248096.331595	37.006823
1635.598610	248586.094687	37.011840
1637.056080	249054.281505	37.016858
1638.971327	249510.758984	37.021876
1640.318273	249972.436835	37.026893
1641.868385	250413.302212	37.031911
1643.156855	250884.517002	37.036928
1644.536927	251353.862859	37.041946
1646.576643	251814.819073	37.046964
1647.882024	252293.374248	37.051981
1649.870241	252754.670240	37.056999
1650.854989	253225.607615	37.062016
1652.922832	253703.759065	37.067034
1654.782035	254185.273204	37.072052
1656.025627	254675.221581	37.077069
1657.801358	255138.536274	37.082087
1659.149108	255620.567871	37.087104
1661.264763	256114.463443	37.092122
1663.057834	256581.205730	37.097140
1664.538457	257072.488569	37.102157
1666.544435	257576.234223	37.107175
1668.242383	258088.693477	37.112192
1669.801944	258555.322895	37.117210
1671.653326	259027.340646	37.122228
1673.120345	259533.132135	37.127245
1675.118645	260017.243314	37.132263
1676.868268	260516.663013	37.137280
1678.349090	261009.903332	37.142298
1679.987199	261518.944015	37.147316
1681.552580	262012.322878	37.152333
1683.764078	262488.879757	37.157351
1685.236556	263007.372368	37.162368
1687.031649	263512.652770	37.167386
1689.090002	263989.412543	37.172404
1691.352582	264474.191347	37.177421
1693.794541	264959.397666	37.182439
1695.154577	265444.528273	37.187456
1696.643397	265909.492644	37.192474
1698.574437	266415.638713	37.197492
1699.425424	266913.071556	37.202509
1701.515778	267387.309714	37.207527
1703.071630	267899.588126	37.212544
1704.591611	268399.399110	37.217562
1706.165665	268891.402005	37.222580
1707.309547	269404.433039	37.227597
1708.883249	269925.699493	37.232615
1710.284195	270438.407671	37.237632
1712.020561	270975.319876	37.242650
1713.682292	271488.872974	37.247668
1715.058284	272007.476980	37.252685
1716.945621	272546.953397	37.257703
1718.377422	273080.128075	37.262720
1719.773704	273598.218522	37.267738
1721.759299	274147.685096	37.272756
1723.577751	274699.489993	37.277773
1725.665335	275243.069848	37.282791
1727.505467	275762.252154	37.287808
1729.028714	276309.784389	37.292826
1731.234697	276850.166406	37.297844
1732.771529	277401.377627	37.302861
1735.013374	277936.366195	37.307879
1736.355505	278460.426599	37.312896
1738.257281	279014.800230	37.317914
1739.877292	279537.923377	37.322932
1741.290576	280074.974492	37.327949
1743.032791	280620.276583	37.332967
1745.002215	281177.351826	37.337984
1747.076468	281718.481203	37.343002
1749.083425	282246.563622	37.348020
1750.349351	282784.013211	37.353037
1752.513357	283316.029573	37.358055
1754.084902	283846.668883	37.363072
1755.401319	284378.110821	37.368090
1757.067926	284885.666673	37.373108
1758.647662	285412.311999	37.378125
1760.021326	285934.366648	37.383143
1761.989154	286482.485144	37.388160
1763.453552	287024.969580	37.393178
1765.265131	287549.080623	37.398196
1766.605716	288085.485604	37.403213
1769.065269	288624.168049	37.408231
1770.938468	289188.168509	37.413248
1772.344413	289725.852394	37.418266
1774.438296	290251.228435	37.423284
1775.669047	290819.900751	37.428301
1777.426055	291362.372140	37.433319
1779.481601	291920.159462	37.438336
1781.257427	292496.659931	37.443354
1783.448783	293049.009889	37.448372
1785.239221	293600.102847	37.453389
1786.978323	294169.439165	37.458407
1788.461189	294744.326981	37.463424
1790.092941	295320.508368	37.468442
1791.685955	295872.030305	37.473460
1793.454767	296444.068984	37.478477
1795.055219	297031.270751	37.483495
1796.848995	297627.352827	37.488512
1798.549300	298209.934836	37.493530
1800.806641	298783.633856	37.498548
1802.488567	299388.817912	37.503565
1804.353062	299987.339402	37.508583
1806.497299	300567.371981	37.513600
1808.325344	301134.068513	37.518618
1810.652945	301731.056008	37.523636
1812.504272	302327.991602	37.528653
1814.373827	302891.420597	37.533671
1816.646786	303476.241111	37.538688
1817.959845	304069.775538	37.543706
1820.253126	304648.287020	37.548724
1821.973086	305233.137348	37.553741
1824.144803	305822.760409	37.558759
1825.949356	306386.103455	37.563776
1827.884987	306970.780288	37.568794
1829.849515	307556.083501	37.573812
1831.312970	308159.522558	37.578829
1833.276491	308733.262703	37.583847
1834.996611	309300.207613	37.588864
1836.415212	309901.051590	37.593882
1838.353629	310502.897600	37.598900
1840.428851	311086.025436	37.603917
1842.311692	311680.710512	37.608935
1844.213912	312281.584558	37.613952
1845.858552	312870.611672	37.618970
1848.016944	313439.411439	37.623988
1849.755190	314049.111352	37.629005
1851.925372	314625.925371	37.634023
1853.827068	315218.727105	37.639040
1855.333248	315833.149220	37.644058
1857.410409	316407.628882	37.649076
1859.062027	316991.646243	37.654093
1860.756090	317601.045661	37.659111
1862.264316	318200.414860	37.664128
1863.777986	318812.957295	37.669146
1865.687734	319417.100254	37.674164
1866.968697	320036.399717	37.679181
1868.945808	320655.350354	37.684199
1870.808379	321272.816220	37.689216
1872.256909	321907.611471	37.694234
1874.058714	322512.710206	37.699252
1876.038101	323146.898428	37.704269
1877.937213	323754.509056	37.709287
1879.901437	324352.835568	37.714304
1881.297809	324960.416399	37.719322
1883.443799	325567.664749	37.724340
1885.048754	326183.654735	37.729357
1887.098406	326792.049889	37.734375
1888.974958	327421.947612	37.739392
1890.932780	328025.902674	37.744410
1893.129669	328630.117063	37.749428
1894.652540	329274.907038	37.754445
1896.120410	329929.220063	37.759463
1898.203395	330552.501125	37.764480
1899.860984	331177.572226	37.769498
1902.113916	331821.808064	37.774516
1903.946399	332474.331792	37.779533
1905.662937	333138.113953	37.784551
1907.435865	333779.259095	37.789568
1909.104780	334424.780706	37.794586
1911.029667	335086.652465	37.799604
1912.807638	335757.857384	37.804621
1914.802282	336432.166275	37.809639
1917.029308	337099.955169	37.814656
1918.948072	337788.983496	37.819674
1921.057738	338446.265542	37.824692
1922.704956	339122.146636	37.829709
1924.906228	339796.100014	37.834727
1927.044569	340458.048412	37.839744
1929.107593	341147.796032	37.844762
1931.030174	341812.504119	37.849780
1933.562899	342469.919487	37.854797
1935.768807	343152.407640	37.859815
1938.456796	343796.682577	37.864832
1940.135061	344467.640023	37.869850
1942.089896	345146.131882	37.874868
1943.978610	345802.797240	37.879885
1946.186671	346450.492296	37.884903
1948.573476	347117.007048	37.889920
1950.476877	347773.617761	37.894938
1952.403508	348421.560975	37.899956
1954.202052	349110.073103	37.904973
1955.380791	349780.759550	37.909991
1957.604241	350441.036285	37.915008
1959.058416	351105.643273	37.920026
1961.045728	351785.937891	37.925044
1962.980171	352463.820133	37.930061
1964.603302	353160.624302	37.935079
1966.377618	353851.860479	37.940096
1968.054354	354545.284360	37.945114
1970.124970	355230.207446	37.950132
1971.790306	355959.289774	37.955149
1973.665461	356670.257971	37.960167
1975.714810	357386.539796	37.965184
1977.441970	358097.305721	37.970202
1979.115840	358793.097792	37.975220
1981.668098	359518.192311	37.980237
1983.333860	360259.380199	37.985255
1985.640342	360964.394449	37.990272
1987.173758	361724.226849	37.995290
1989.345963	362439.741991	38.000308
1991.368079	363157.324337	38.005325
1993.236384	363903.410828	38.010343
1995.500610	364629.299300	38.015360
1997.453737	365369.306146	38.020378
1999.646489	366079.044448	38.025396
2001.688998	366805.665081	38.030413
2003.672208	367542.302489	38.035431
2005.976705	368259.440862	38.040448
2007.608495	368967.823447	38.045466
2009.917010	369674.508465	38.050484
2012.258987	370367.172328	38.055501
2013.993343	371052.034725	38.060519
2016.243315	371762.139909	38.065536
2018.135633	372467.268151	38.070554
2020.533317	373152.261357	38.075572
2022.286473	373840.315666	38.080589
2024.082845	374543.187676	38.085607
2026.614669	375247.776245	38.090624
2028.495660	375962.121568	38.095642
2030.821204	376647.009698	38.100660
2032.613601	377331.693553	38.105677
2034.415820	378053.567583	38.110695
2036.869188	378772.428222	38.115712
2038.810741	379474.874243	38.120730
2040.039725	380179.959509	38.125748
2042.444389	380904.413771	38.130765
2044.188271	381648.792162	38.135783
2046.489442	382374.677690	38.140800
2048.720587	383092.774383	38.145818
2050.939597	383813.342708	38.150836
2053.063006	384547.882675	38.155853
2054.671219	385288.982464	38.160871
2056.524381	386032.763579	38.165888
2058.683902	386770.747110	38.170906
2060.636882	387503.322185	38.175924
2062.883712	388264.076168	38.180941
2064.752568	389018.764429	38.185959
2067.133817	389753.955781	38.190976
2069.045441	390508.652451	38.195994
2071.029414	391277.870779	38.201012
2073.475435	392052.190955	38.206029
2075.227386	392803.436535	38.211047
2077.502844	393562.207769	38.216064
2079.355979	394343.565023	38.221082
2081.325283	395101.056041	38.226100
2083.689604	395868.830224	38.231117
2085.751958	396641.906914	38.236135
2088.904798	397387.258026	38.241152
2091.470660	398146.678150	38.246170
2093.751235	398899.232179	38.251188
2096.284534	399641.841182	38.256205
2098.309845	400380.815100	38.261223
2100.876261	401111.394019	38.266240
2103.034950	401861.890283	38.271258
2104.680341	402600.161083	38.276276
2106.964938	403347.709120	38.281293
2108.412961	404105.866574	38.286311
2110.734890	404855.066923	38.291328
2112.452872	405605.386018	38.296346
2114.546136	406360.006844	38.301364
2116.503465	407127.425352	38.306381
2118.053370	407896.055494	38.311399
2120.147689	408646.965925	38.316416
2122.413126	409426.000908	38.321434
2124.047348	410209.703543	38.326452
2125.858783	410993.557200	38.331469
2127.933477	411789.504899	38.336487
2129.807454	412560.053690	38.341504
2132.039985	413372.673588	38.346522
2133.570814	414187.081748	38.351540
2135.791762	414979.744451	38.356557
2138.089303	415785.491550	38.361575
2140.109232	416593.944666	38.366592
2142.115474	417411.645181	38.371610
2144.258676	418242.746236	38.376628
2146.000264	419044.837531	38.381645
2147.880901	419840.853488	38.386663
2150.147652	420628.373259	38.391680
2152.098882	421446.132394	38.396698
2154.374747	422261.456638	38.401716
2156.434747	423049.340696	38.406733
2158.568076	423858.736708	38.411751
2160.784145	424670.143901	38.416768
2162.806168	425486.671304	38.421786
2164.814471	426321.859587	38.426804
2166.994532	427127.849942	38.431821
2169.214344	427946.415357	38.436839
2171.303132	428780.367415	38.441856
2173.486225	429630.224181	38.446874
2175.385238	430456.150107	38.451892
2178.011151	431274.586759	38.456909
2180.014148	432136.940355	38.461927
2182.334590	432985.643072	38.466944
2184.968867	433813.508416	38.471962
2186.945559	434675.925795	38.476980
2189.504265	435532.039997	38.481997
2191.757212	436388.881842	38.487015
2194.099288	437211.765261	38.492032
2196.251616	438060.007922	38.497050
2198.257099	438948.378303	38.502068
2200.622458	439803.202055	38.507085
2203.214294	440640.800410	38.512103
2205.995608	441484.864679	38.517120
2208.654851	442331.700681	38.522138
2210.697929	443171.825676	38.527156
2213.076694	444008.473521	38.532173
2215.342918	444868.636509	38.537191
2217.208418	445735.055439	38.542208
2219.802437	446572.127388	38.547226
2221.447601	447403.556316	38.552244
2223.850399	448272.923033	38.557261
2225.701497	449141.182384	38.562279
2228.409623	449991.003954	38.567296
2230.980112	450842.433329	38.572314
2233.228589	451699.142474	38.577332
2235.765715	452564.519928	38.582349
2237.431569	453431.270191	38.587367
2239.967056	454280.847987	38.592384
2241.976225	455136.496515	38.597402
2243.872390	456019.791431	38.602420
2246.080571	456896.726816	38.607437
2248.106897	457762.327988	38.612455
2250.220066	458639.306300	38.617472
2252.434239	459542.725592	38.622490
2254.610511	460456.375069	38.627508
2256.678863	461332.284623	38.632525
2258.245823	462224.214815	38.637543
2260.491585	463126.458355	38.642560
2262.521845	464047.401061	38.647578
2264.586956	464988.869209	38.652596
2266.862748	465891.286256	38.657613
2269.219388	466816.292905	38.662631
2271.420239	467756.040193	38.667648
2273.860923	468694.995354	38.672666
2276.280600	469620.364767	38.677684
2278.715928	470546.091817	38.682701
2281.007481	471473.920645	38.687719
2283.420904	472415.125718	38.692736
2285.630105	473344.242121	38.697754
2287.460682	474279.944005	38.702772
2290.028931	475219.317909	38.707789
2292.450942	476157.810415	38.712807
2294.216201	477113.136305	38.717824
2296.684282	478029.552491	38.722842
2298.589712	478959.755894	38.727860
2301.067138	479881.787296	38.732877
2302.845786	480815.504705	38.737895
2305.579016	481734.269903	38.742912
2307.712738	482642.785378	38.747930
2309.923387	483585.279984	38.752948
2312.226589	484527.659970	38.757965
2314.322648	485490.273418	38.762983
2316.489835	486419.044561	38.768000
2318.508888	487358.798750	38.773018
2321.675730	488291.195631	38.778036
2324.378625	489250.982498	38.783053
2326.262760	490208.580690	38.788071
2328.708139	491154.575719	38.793088
2331.334359	492095.795714	38.798106
2333.059769	493047.460564	38.803124
2335.219722	494004.856330	38.808141
2338.038653	494986.113130	38.813159
2340.417996	495965.115718	38.818176
2342.979041	496903.461297	38.823194
2345.401857	497861.608641	38.828212
2348.139416	498818.742024	38.833229
2350.750250	499802.986209	38.838247
2352.796025	500782.221211	38.843264
2355.405491	501734.417825	38.848282
2357.575570	502710.240850	38.853300
2359.703156	503695.295089	38.858317
2362.369606	504687.818336	38.863335
2364.663359	505656.739674	38.868352
2366.973272	506643.202369	38.873370
2369.218818	507633.398612	38.878388
2371.556804	508604.710559	38.883405
2373.938990	509605.253296	38.888423
2376.278201	510621.422073	38.893440
2378.336417	511621.641418	38.898458
2380.156593	512637.667765	38.903476
2382.595763	513650.704590	38.908493
2384.845326	514677.570366	38.913511
2387.069145	515727.660696	38.918528
2389.633197	516741.235778	38.923546
2391.906331	517768.904894	38.928564
2394.497340	518820.391508	38.933581
2397.301129	519874.795660	38.938599
2399.954748	520897.660897	38.943616
2402.802113	521917.202014	38.948634
2404.925941	522951.606940	38.953652
2407.689958	523990.219468	38.958669
2410.120623	525037.631835	38.963687
2411.970860	526076.605613	38.968704
2415.193384	527100.322975	38.973722
2417.480526	528123.621508	38.978740
2420.018827	529152.298290	38.983757
2422.475125	530189.327536	38.988775
2425.048912	531230.394306	38.993792
2427.485900	532257.614899	38.998810
2429.751634	533288.971180	39.003828
2432.007067	534326.298142	39.008845
2434.740156	535370.822596	39.013863
2437.147015	536414.722219	39.018880
2440.060046	537432.593021	39.023898
2441.864017	538483.389336	39.028916
2444.447744	539506.805426	39.033933
2446.839314	540543.112981	39.038951
2449.551610	541583.418827	39.043968
2451.438522	542621.470568	39.048986
2454.097336	543674.211140	39.054004
2456.820525	544711.368585	39.059021
2459.624789	545736.766277	39.064039
2461.918834	546726.511302	39.069056
2464.684963	547722.496164	39.074074
2467.095122	548734.662687	39.079092
2469.515662	549739.914679	39.084109
2472.009139	550719.838862	39.089127
2474.176441	551723.027459	39.094144
2476.413190	552721.053489	39.099162
2478.457988	553733.768748	39.104180
2480.959914	554750.857907	39.109197
2483.203235	555793.499188	39.114215
2485.318741	556808.336638	39.119232
2487.922220	557823.570303	39.124250
2490.128731	558861.508003	39.129268
2492.398414	559908.500648	39.134285
2494.865648	560968.895119	39.139303
2496.688951	562029.663022	39.144320
2499.528697	563111.630500	39.149338
2501.498437	564210.230217	39.154356
2503.907739	565301.734065	39.159373
2506.399052	566392.380195	39.164391
2508.470227	567489.131645	39.169408
2511.357629	568577.822216	39.174426
2513.995798	569715.520942	39.179444
2516.726774	570810.778079	39.184461
2519.308074	571925.897956	39.189479
2521.683215	573073.936387	39.194496
2523.974850	574180.724937	39.199514
2527.119895	575317.943472	39.204532
2529.768600	576438.279028	39.209549
2532.432833	577560.269026	39.214567
2534.917888	578713.449300	39.219584
2537.227921	579843.271967	39.224602
2539.982304	580988.220608	39.229620
2542.424963	582119.119477	39.234637
2545.510141	583253.721674	39.239655
2547.939542	584423.987738	39.244672
2550.771169	585549.091582	39.249690
2553.212374	586685.940657	39.254708
2555.634606	587845.952294	39.259725
2558.226970	589005.524433	39.264743
2560.320989	590161.909485	39.269760
2563.023247	591335.176560	39.274778
2565.249429	592509.059214	39.279796
2567.388476	593674.822588	39.284813
2569.997681	594850.416910	39.289831
2572.529120	596042.893919	39.294848
2575.236497	597214.028966	39.299866
2577.780641	598404.111350	39.304884
2580.338741	599615.560139	39.309901
2583.409009	600800.804490	39.314919
2585.882053	602000.600459	39.319936
2588.131685	603177.875416	39.324954
2590.762796	604388.365033	39.329972
2593.326255	605589.226360	39.334989
2595.841293	606801.033519	39.340007
2597.980770	608030.543822	39.345024
2600.727238	609238.750751	39.350042
2603.516415	610476.598439	39.355060
2605.483756	611709.492434	39.360077
2608.641143	612938.653277	39.365095
2610.648652	614189.381053	39.370112
2613.534885	615398.456036	39.375130
2616.157106	616642.755190	39.380148
2618.267400	617895.401215	39.385165
2621.188908	619146.071612	39.390183
2623.895431	620378.885733	39.395200
2626.586589	621611.914007	39.400218
2629.313657	622851.695859	39.405236
2631.683223	624065.504645	39.410253
2634.664181	625268.731794	39.415271
2637.443078	626480.653532	39.420288
2640.016018	627700.517597	39.425306
2642.564391	628899.863466	39.430324
2644.789651	630092.834005	39.435341
2647.600951	631306.902933	39.440359
2650.104605	632550.450449	39.445376
2652.702941	633774.560591	39.450394
2655.384185	634988.329102	39.455412
2657.801303	636224.417887	39.460429
2660.490387	637442.045408	39.465447
2663.172240	638688.382616	39.470464
2665.886231	639935.862938	39.475482
2669.064804	641175.082431	39.480500
2671.833052	642415.418486	39.485517
2674.943178	643653.104217	39.490535
2677.582336	644911.170786	39.495552
2680.212902	646151.726507	39.500570
2683.109790	647397.024649	39.505588
2685.630904	648642.381621	39.510605
2688.675298	649878.773673	39.515623
2691.096172	651143.483515	39.520640
2693.734171	652430.130506	39.525658
2696.363088	653690.447347	39.530676
2698.718114	654953.739881	39.535693
2701.687247	656227.384082	39.540711
2704.290869	657496.490678	39.545728
2706.852637	658781.132823	39.550746
2709.862101	660065.782494	39.555764
2712.087825	661366.279839	39.560781
2714.631220	662654.401655	39.565799
2717.276807	663967.678654	39.570816
2719.539117	665286.565943	39.575834
2722.211309	666602.667199	39.580852
2724.549837	667948.056613	39.585869
2727.483800	669276.986892	39.590887
2730.103487	670602.749242	39.595904
2732.964827	671950.673585	39.600922
2735.996413	673289.574451	39.605940
2738.859253	674643.880075	39.610957
2742.018220	675986.803661	39.615975
2744.858033	677320.787544	39.620992
2748.078042	678654.468889	39.626010
2750.991500	680006.947465	39.631028
2753.448456	681345.041246	39.636045
2756.722059	682670.831706	39.641063
2759.242809	684021.894095	39.646080
2761.801570	685377.222505	39.651098
2764.753953	686718.279063	39.656116
2767.592146	688069.039992	39.661133
2770.876269	689398.622641	39.666151
2773.947660	690740.010129	39.671168
2776.716562	692072.065061	39.676186
2779.688821	693393.963042	39.681204
2782.234687	694743.278079	39.686221
2785.207914	696065.873270	39.691239
2788.168784	697406.332066	39.696256
2790.795089	698734.441559	39.701274
2793.491251	700049.396045	39.706292
2796.172270	701405.066427	39.711309
2799.241486	702734.880763	39.716327
2801.661012	704088.196551	39.721344
2804.401516	705435.450687	39.726362
2807.227588	706762.461263	39.731380
2809.724399	708115.881300	39.736397
2812.856279	709435.148096	39.741415
2815.599727	710775.923061	39.746432
2818.344920	712081.721129	39.751450
2821.106713	713387.119137	39.756468
2823.712951	714709.028162	39.761485
2826.124061	716007.645834	39.766503
2828.703264	717323.013812	39.771520
2831.232249	718641.896833	39.776538
2834.162954	719964.514950	39.781556
2836.496046	721310.324480	39.786573
2838.958103	722668.113876	39.791591
2841.816154	724020.176733	39.796608
2843.994682	725365.060507	39.801626
2847.027447	726728.372308	39.806644
2849.916351	728115.110946	39.811661
2852.380891	729498.967488	39.816679
2855.371710	730900.540159	39.821696
2858.214210	732300.809935	39.826714
2861.247313	733678.133944	39.831732
2864.283654	735098.044279	39.836749
2867.346851	736502.047299	39.841767
2870.344509	737911.050043	39.846784
2873.539129	739337.149123	39.851802
2876.337255	740743.367114	39.856820
2878.856619	742183.629221	39.861837
2881.522402	743598.790033	39.866855
2884.468036	745026.181414	39.871872
2886.867769	746480.382318	39.876890
2890.398750	747931.564145	39.881908
2892.680122	749386.972620	39.886925
2895.780053	750823.786820	39.891943
2898.439013	752307.522628	39.896960
2901.170139	753791.554379	39.901978
2903.562763	755273.337578	39.906996
2906.492186	756780.064075	39.912013
2909.595428	758270.708490	39.917031
2912.595261	759778.754979	39.922048
2915.190916	761302.568093	39.927066
2918.302269	762825.597255	39.932084
2920.599928	764331.281990	39.937101
2923.508288	765854.226969	39.942119
2926.524513	767391.257201	39.947136
2929.537030	768935.005050	39.952154
2932.651701	770477.483084	39.957172
2935.976760	772010.857514	39.962189
2938.844189	773540.599582	39.967207
2941.877089	775095.203721	39.972224
2944.911339	776651.297292	39.977242
2947.782731	778208.021144	39.982260
2950.723383	779773.879261	39.987277
2954.083426	781299.862004	39.992295
2957.418782	782845.701031	39.997312
2960.576403	784407.727324	40.002330
2963.728366	785932.032239	40.007348
2966.566288	787475.440739	40.012365
2969.278597	789030.699466	40.017383
2971.989183	790591.111127	40.022400
2974.401977	792144.171227	40.027418
2977.609394	793726.801935	40.032436
2980.611072	795290.885613	40.037453
2983.356717	796847.659317	40.042471
2986.072823	798431.273599	40.047488
2989.038143	800028.883624	40.052506
2992.406478	801608.830046	40.057524
2994.816085	803185.149282	40.062541
2997.922420	804769.361914	40.067559
3001.112861	806360.730431	40.072576
3003.878621	807938.986951	40.077594
3007.354764	809529.378119	40.082612
3010.466127	811102.447180	40.087629
3012.984411	812664.644871	40.092647
3016.138754	814205.318420	40.097664
3019.218369	815762.067127	40.102682
3022.025472	817287.487794	40.107700
3024.948100	818820.209088	40.112717
3028.244349	820374.583382	40.117735
3031.668157	821907.343859	40.122752
3034.780038	823481.961074	40.127770
3037.728848	825042.766940	40.132788
3040.513229	826573.773040	40.137805
3043.486762	828154.371220	40.142823
3046.539522	829728.433364	40.147840
3049.125932	831293.664617	40.152858
3052.091620	832871.077330	40.157876
3054.830564	834470.357524	40.162893
3057.452544	836044.716793	40.167911
3060.425943	837657.585284	40.172928
3063.882615	839283.696506	40.177946
3067.168440	840876.234365	40.182964
3069.704218	842489.224621	40.187981
3072.479052	844129.540141	40.192999
3075.440391	845775.771082	40.198016
3078.053909	847441.562592	40.203034
3081.535465	849092.870897	40.208052
3084.406479	850761.628961	40.213069
3087.289028	852433.826266	40.218087
3090.502204	854095.905490	40.223104
3093.387829	855799.443671	40.228122
3096.240568	857500.771525	40.233140
3099.158973	859208.024617	40.238157
3102.232383	860928.845875	40.243175
3105.508819	862654.194074	40.248192
3108.546514	864379.191201	40.253210
3111.779197	866101.728637	40.258228
3114.637372	867835.564355	40.263245
3117.430183	869575.598157	40.268263
3121.174380	871329.790752	40.273280
3124.130012	873080.018013	40.278298
3127.063531	874828.284766	40.283316
3130.406773	876587.970087	40.288333
3133.563453	878369.123907	40.293351
3136.434465	880129.770096	40.298368
3139.486322	881900.978793	40.303386
3143.004621	883676.892364	40.308404
3146.317478	885471.335107	40.313421
3149.540318	887236.843079	40.318439
3153.256831	889013.320754	40.323456
3155.986168	890794.049611	40.328474
3158.968696	892566.467232	40.333492
3162.075617	894351.148843	40.338509
3164.603848	896174.235746	40.343527
3167.985726	897984.452337	40.348544
3171.244968	899784.571583	40.353562
3174.092303	901595.363561	40.358580
3177.093815	903417.204169	40.363597
3179.960435	905228.944989	40.368615
3183.128709	907039.665891	40.373632
3186.225351	908895.325799	40.378650
3189.227512	910725.180724	40.383668
3192.625185	912566.963988	40.388685
3195.608125	914427.523620	40.393703
3198.992840	916272.013477	40.398720
3201.839759	918122.024023	40.403738
3205.437332	919978.967545	40.408756
3208.437113	921850.352264	40.413773
3212.473278	923669.196522	40.418791
3216.326277	925489.953643	40.423808
3219.190626	927325.986213	40.428826
3222.315160	929114.661101	40.433844
3225.785552	930905.748140	40.438861
3228.600031	932720.484284	40.443879
3231.565847	934508.047689	40.448896
3234.290918	936292.271252	40.453914
3237.351996	938101.007191	40.458932
3240.175769	939908.012410	40.463949
3242.733033	941712.621698	40.468967
3246.486421	943543.754189	40.473984
3249.353934	945399.715241	40.479002
3252.024142	947259.344184	40.484020
3255.353491	949096.420999	40.489037
3258.128518	950978.377379	40.494055
3261.771213	952822.186346	40.499072
3265.496759	954708.533056	40.504090
3268.445218	956617.716432	40.509108
3271.611972	958553.552180	40.514125
3274.878784	960504.857065	40.519143
3278.287297	962450.199868	40.524160
3281.696018	964413.941326	40.529178
3285.353232	966372.966978	40.534196
3289.001385	968326.053703	40.539213
3292.336697	970279.504454	40.544231
3295.449221	972247.843658	40.549248
3298.824525	974238.974534	40.554266
3301.766733	976223.536459	40.559284
3305.159069	978206.751655	40.564301
3307.707389	980206.472402	40.569319
3311.200294	982194.817074	40.574336
3314.130748	984210.121490	40.579354
3317.079431	986229.189174	40.584372
3320.759455	988263.575367	40.589389
3324.044339	990303.136635	40.594407
3327.864940	992319.220761	40.599424
3331.945163	994355.544280	40.604442
3335.308393	996385.328045	40.609460
3338.519620	998417.713463	40.614477
3341.722383	1000465.685196	40.619495
3344.911797	1002519.713403	40.624512
3348.374770	1004560.821602	40.629530
3351.102754	1006594.814854	40.634548
3354.492729	1008674.897106	40.639565
3357.430256	1010740.038551	40.644583
3360.723750	1012821.417811	40.649600
3364.121024	1014918.282490	40.654618
3367.227945	1017013.735641	40.659636
3370.606312	1019095.296936	40.664653
3373.792384	1021196.822259	40.669671
3377.146168	1023294.147675	40.674688
3381.060281	1025384.408540	40.679706
3383.969736	1027507.298232	40.684724
3387.269084	1029623.135355	40.689741
3390.664752	1031758.627239	40.694759
3393.850419	1033877.698987	40.699776
3397.104372	1036016.892900	40.704794
3400.286392	1038144.088366	40.709812
3403.830588	1040296.540249	40.714829
3407.151100	1042431.136185	40.719847
3410.556846	1044577.133197	40.724864
3414.043405	1046744.822332	40.729882
3417.021153	1048905.489985	40.734900
3420.677927	1051051.441643	40.739917
3423.818900	1053215.595652	40.744935
3427.271358	1055375.389115	40.749952
3430.816282	1057544.126213	40.754970
3435.081910	1059695.077573	40.759988
3439.200339	1061828.885849	40.765005
3442.948961	1063950.903765	40.770010
3446.393411	1066004.534179	40.775015
3449.977323	1068024.383988	40.780020
3452.644049	1069978.647057	40.785024
3455.736617	1071839.491049	40.790029
3458.871160	1073619.564140	40.795034
3461.500793	1075341.318493	40.800039
3464.513677	1076978.352164	40.805044
3467.179607	1078547.660124	40.810048
3469.737160	1080040.527866	40.815053
3471.968907	1081453.503600	40.820058
3474.477575	1082777.245539	40.825063
3476.806645	1084048.143273	40.830068
3478.724435	1085260.806733	40.835072
3481.044728	1086375.264116	40.840077
3483.386623	1087462.942373	40.845082
3485.207820	1088457.543431	40.850087
3487.571327	1089374.080370	40.855092
3488.920713	1090258.061442	40.860096
3490.859224	1091051.199233	40.865101
3492.065352	1091820.688667	40.870106
3493.683300	1092529.488206	40.875111
3495.182567	1093187.474144	40.880116
3496.468717	1093794.297603	40.885120
3497.893707	1094350.874953	40.890125
3499.218699	1094876.019653	40.895130
3500.339833	1095340.856887	40.900135
3501.318996	1095756.492245	40.905140
3502.320231	1096165.489814	40.910144
3503.350246	1096510.634598	40.915149
3504.445298	1096845.796714	40.920154
3505.571381	1097139.509165	40.925159
3505.965905	1097393.817551	40.930164
3506.848908	1097605.274104	40.935168
3508.202516	1097793.783209	40.940173
3509.077958	1097960.842654	40.945178
3509.639594	1098073.714906	40.950183
3510.704013	1098197.884184	40.955188
3511.027411	1098270.810307	40.960192
3511.934323	1098323.553652	40.965197
3512.545179	1098377.875565	40.970202
3513.311836	1098376.505941	40.975207
3513.750531	1098358.069774	40.980212
3514.222701	1098325.185461	40.985216
3514.733549	1098262.452671	40.990221
3515.020431	1098203.486332	40.995226
3515.338875	1098118.593080	41.000231
3516.127653	1098006.934218	41.005236
3516.553254	1097909.011357	41.010240
3517.258303	1097781.100488	41.015245
3517.598611	1097625.505729	41.020250
3517.984817	1097463.106976	41.025255
3518.404594	1097299.836843	41.030260
3518.333299	1097128.415268	41.035264
3519.234178	1096919.133855	41.040269
3519.166801	1096718.901575	41.045274
3519.252550	1096483.044253	41.050279
3520.037072	1096237.014846	41.055284
3520.053443	1095995.502402	41.060288
3520.309658	1095756.236285	41.065293
3520.487484	1095507.977084	41.070298
3520.530398	1095249.775866	41.075303
3520.791269	1094988.750991	41.080308
3520.850231	1094714.730236	41.085312
3521.155669	1094417.874826	41.090317
3521.428064	1094124.358818	41.095322
3521.514523	1093836.122448	41.100327
3521.978501	1093540.533038	41.105332
3521.402468	1093221.547676	41.110336
3522.031253	1092901.387690	41.115341
3521.779816	1092603.279970	41.120346
3522.114440	1092256.321021	41.125351
3522.323628	1091936.364691	41.130356
3522.165286	1091626.601080	41.135360
3522.209770	1091286.618713	41.140365
3522.477643	1090941.789421	41.145370
3522.595779	1090589.874952	41.150375
3522.640656	1090252.892818	41.155380
3522.497162	1089908.544585	41.160384
3522.569541	1089568.450002	41.165389
3522.304226	1089210.665423	41.170394
3522.887911	1088860.478340	41.175399
3523.031003	1088508.329046	41.180404
3522.929812	1088166.546343	41.185408
3523.105236	1087793.838693	41.190413
3523.152438	1087430.135446	41.195418
3522.806466	1087066.472619	41.200423
3523.071811	1086676.133859	41.205428
3522.994439	1086306.433136	41.210432
3522.969500	1085939.958054	41.215437
3522.970275	1085593.011773	41.220442
3522.995852	1085202.606766	41.225447
3523.127017	1084829.319711	41.230452
3522.781318	1084465.578799	41.235456
3523.026615	1084067.384903	41.240461
3522.885107	1083691.283681	41.245466
3522.848123	1083317.249311	41.250471
3522.820393	1082943.571402	41.255476
3522.904485	1082575.604897	41.260480
3523.094077	1082199.729851	41.265485
3522.744683	1081816.434528	41.270490
3522.966340	1081423.999427	41.275495
3523.209794	1081052.449844	41.280500
3522.695707	1080672.651401	41.285504
3522.844915	1080270.069624	41.290509
3522.901693	1079882.061059	41.295514
3522.865639	1079513.811702	41.300519
3522.966145	1079139.276004	41.305524
3523.030372	1078749.457955	41.310528
3523.192331	1078340.300275	41.315533
3523.060254	1077949.593457	41.320538
3522.802593	1077551.486404	41.325543
3523.007039	1077169.117423	41.330548
3522.586693	1076791.721904	41.335552
3522.905963	1076406.591924	41.340557
3522.642723	1076014.327781	41.345562
3522.677487	1075619.489194	41.350567
3522.513236	1075246.170793	41.355572
3522.810818	1074856.324621	41.360576
3522.754279	1074451.810754	41.365581
3522.751541	1074059.555583	41.370586
3522.749268	1073674.766507	41.375591
3522.748686	1073284.473109	41.380596
3522.537779	1072889.381797	41.385600
3522.552612	1072474.427866	41.390605
3522.457420	1072102.997814	41.395610
3522.694837	1071721.972418	41.400615
3522.885094	1071316.993953	41.405620
3522.799192	1070937.697455	41.410624
3522.845175	1070545.470826	41.415629
3522.633138	1070134.126238	41.420634
3522.531323	1069743.981731	41.425639
3522.791603	1069344.326480	41.430644
3522.312963	1068952.360723	41.435648
3522.283509	1068556.157635	41.440653
3522.334710	1068156.354079	41.445658
3522.266096	1067754.136510	41.450663
3522.436308	1067377.244639	41.455668
3522.221767	1066988.654122	41.460672
3522.029477	1066592.817066	41.465677
3522.164123	1066194.011269	41.470682
3521.964854	1065816.592046	41.475687
3522.098162	1065423.407402	41.480692
3521.749498	1065032.198641	41.485696
3522.149447	1064649.307756	41.490701
3522.280147	1064267.589494	41.495706
3522.143894	1063852.200291	41.500711
3522.282235	1063455.312650	41.505716
3522.126914	1063075.676452	41.510720
3522.127007	1062673.267950	41.515725
3521.971537	1062279.809712	41.520730
3521.643268	1061912.927014	41.525735
3521.920690	1061526.179947	41.530740
3521.347131	1061132.997433	41.535744
3521.783717	1060732.493710	41.540749
3521.583238	1060351.039700	41.545754
3521.532484	1059954.123254	41.550759
3521.548108	1059566.414753	41.555764
3521.692789	1059172.010616	41.560768
3521.735352	1058794.454830	41.565773
3521.661456	1058420.842622	41.570778
3521.239514	1058018.163301	41.575783
3521.339526	1057616.621298	41.580788
3521.426229	1057247.335753	41.585792
3521.592583	1056881.192731	41.590797
3521.264972	1056492.746283	41.595802
3520.967368	1056105.231417	41.600807
3521.201460	1055716.830602	41.605812
3521.375238	1055327.351969	41.610816
3521.197970	1054936.553952	41.615821
3521.277184	1054559.666268	41.620826
3521.047175	1054160.241016	41.625831
3521.092672	1053787.066627	41.630836
3521.012317	1053430.763913	41.635840
3521.114798	1053029.080531	41.640845
3520.979364	1052633.386974	41.645850
3520.922475	1052262.441248	41.650855
3521.127890	1051871.749167	41.655860
3520.935868	1051511.482608	41.660864
3520.896142	1051116.822352	41.665869
3520.715455	1050738.076705	41.670874
3520.879042	1050351.625816	41.675879
3521.103035	1049963.497567	41.680884
3520.642613	1049601.510377	41.685888
3520.732821	1049204.376249	41.690893
3520.735795	1048838.788538	41.695898
3520.835917	1048469.106783	41.700903
3520.952887	1048074.879407	41.705908
3520.638749	1047696.430210	41.710912
3520.770615	1047304.462394	41.715917
3520.663937	1046928.919394	41.720922
3520.231308	1046563.060113	41.725927
3520.710260	1046171.534335	41.730932
3520.414514	1045809.658365	41.735936
3520.464262	1045430.704783	41.740941
3520.583398	1045042.345505	41.745946
3520.477402	1044668.387714	41.750951
3520.366781	1044282.814148	41.755956
3520.156786	1043923.988623	41.760960
3520.195621	1043531.189756	41.765965
3520.111120	1043185.434425	41.770970
3520.098994	1042799.934838	41.775975
3519.949691	1042419.069174	41.780980
3519.916133	1042068.984343	41.785984
3520.201128	1041698.530732	41.790989
3520.383290	1041320.530976	41.795994
3519.917127	1040940.485928	41.800999
3520.150113	1040579.244915	41.806004
3519.938547	1040219.213629	41.811008
3519.760009	1039842.139382	41.816013
3519.677422	1039450.038602	41.821018
3519.416859	1039088.782035	41.826023
3519.445455	1038730.451802	41.831028
3519.372473	1038381.301455	41.836032
3519.880876	1038009.501553	41.841037
3519.629964	1037639.832791	41.846042
3519.088732	1037283.050559	41.851047
3519.598539	1036923.170675	41.856052
3519.440226	1036567.730368	41.861056
3519.485889	1036195.305161	41.866061
3519.358345	1035828.204363	41.871066
3519.246312	1035459.819096	41.876071
3519.520361	1035099.086221	41.881076
3519.235009	1034766.579339	41.886080
3519.312661	1034400.898867	41.891085
3519.116813	1034017.723584	41.896090
3519.018089	1033668.378711	41.901095
3518.966710	1033321.133426	41.906100
3518.918285	1032969.413645	41.911104
3519.038729	1032595.090080	41.916109
3519.158373	1032247.459401	41.921114
3518.909360	1031903.352932	41.926119
3518.815520	1031541.385594	41.931124
3518.583748	1031195.005844	41.936128
3518.930016	1030846.379185	41.941133
3518.899676	1030483.267678	41.946138
3518.914646	1030115.864116	41.951143
3518.687889	1029763.196920	41.956148
3518.329428	1029423.216853	41.961152
3518.363047	1029071.334770	41.966157
3518.377598	1028725.148692	41.971162
3518.226480	1028385.943146	41.976167
3518.509617	1028037.248470	41.981172
3518.105227	1027682.251029	41.986176
3518.254828	1027330.724693	41.991181
3518.273442	1027013.014074	41.996186
3517.856506	1026655.143558	42.001191
3517.950291	1026305.209283	42.006196
3518.110821	1025980.245550	42.011200
3517.690757	1025627.446158	42.016205
3517.878694	1025290.032278	42.021210
3517.761603	1024969.514105	42.026215
3518.104427	1024628.060709	42.031220
3517.680536	1024286.615837	42.036224
3517.840873	1023923.725436	42.041229
3517.953270	1023609.296279	42.046234
3517.716447	1023289.865138	42.051239
3517.403090	1022934.163610	42.056244
3517.665501	1022605.108639	42.061248
3517.301613	1022262.269872	42.066253
3517.448014	1021929.315280	42.071258
3517.720959	1021593.119472	42.076263
3517.519273	1021269.784875	42.081268
3517.424434	1020951.167005	42.086272
3517.570370	1020599.315653	42.091277
3517.532061	1020269.203102	42.096282
3517.154094	1019953.582550	42.101287
3517.219556	1019637.095036	42.106292
3517.257348	1019285.761275	42.111296
3517.355335	1018966.707884	42.116301
3517.349302	1018639.308131	42.121306
3516.995551	1018313.790413	42.126311
3517.417340	1017987.931992	42.131316
3517.256206	1017651.183335	42.136320
3517.203568	1017307.505209	42.141325
3517.459167	1016991.710857	42.146330
3516.938011	1016674.182307	42.151335
3517.375866	1016331.819834	42.156340
3516.682020	1016010.690312	42.161344
3516.666115	1015682.246104	42.166349
3516.877641	1015367.241580	42.171354
3516.968784	1015057.579805	42.176359
3516.946179	1014723.934385	42.181364
3516.839651	1014387.758074	42.186368
3516.881679	1014062.025990	42.191373
3516.671496	1013746.028973	42.196378
3516.488518	1013430.301120	42.201383
3516.799544	1013095.532916	42.206388
3516.710765	1012785.387205	42.211392
3516.473548	1012480.300430	42.216397
3516.556251	1012157.948716	42.221402
3516.648174	1011835.674196	42.226407
3516.684206	1011507.269224	42.231412
3516.588977	1011197.425786	42.236416
3516.246432	1010878.471774	42.241421
3516.477079	1010580.881745	42.246426
3516.557250	1010270.861303	42.251431
3516.514144	1009934.311466	42.256436
3516.280898	1009617.989429	42.261440
3516.563014	1009304.480777	42.266445
3516.437458	1008997.145803	42.271450
3516.147897	1008687.099189	42.276455
3516.123142	1008367.173068	42.281460
3516.012989	1008058.715052	42.286464
3515.816312	1007744.809708	42.291469
3515.990768	1007446.771897	42.296474
3516.350658	1007138.575114	42.301479
3516.403793	1006821.173952	42.306484
3516.251548	1006509.526438	42.311488
3516.086275	1006190.180815	42.316493
3516.320643	1005870.945835	42.321498
3515.804289	1005561.542946	42.326503
3515.773325	1005252.334973	42.331508
3515.928950	1004934.810936	42.336512
3515.881970	1004643.665522	42.341517
3515.840380	1004345.986088	42.346522
3515.656001	1004031.094001	42.351527
3515.738476	1003705.826984	42.356532
3515.721294	1003428.332893	42.361536
3515.661375	1003120.861827	42.366541
3515.498645	1002819.229699	42.371546
3515.295496	1002521.675463	42.376551
3515.418359	1002222.105438	42.381556
3515.251942	1001922.469874	42.386560
3515.250298	1001620.455326	42.391565
3515.103019	1001338.208179	42.396570
3514.927708	1001053.031307	42.401575
3515.067646	1000741.309645	42.406580
3515.057309	1000443.322337	42.411584
3514.881672	1000140.673394	42.416589
3515.078260	999847.975373	42.421594
3515.171299	999565.502924	42.426599
3515.169270	999274.852737	42.431604
3514.675823	998988.261070	42.436608
3515.066005	998679.890367	42.441613
3515.057378	998397.279053	42.446618
3514.605759	998118.524930	42.451623
3514.874433	997826.684578	42.456628
3515.096027	997529.090200	42.461632
3514.935829	997243.232035	42.466637
3514.911205	996959.382799	42.471642
3514.543961	996664.177929	42.476647
3514.683315	996382.416007	42.481652
3514.410623	996117.075736	42.486656
3514.400166	995829.075677	42.491661
3514.549922	995548.537261	42.496666
3514.518987	995274.251007	42.501671
3514.416300	994968.877873	42.506676
3514.311200	994690.677768	42.511680
3514.504128	994419.529257	42.516685
3514.375115	994141.306179	42.521690
3514.241951	993869.697825	42.526695
3514.307351	993580.109213	42.531700
3514.478610	993298.676352	42.536704
3514.346324	993011.040808	42.541709
3514.430785	992744.509283	42.546714
3514.170934	992466.908152	42.551719
3514.392342	992167.960360	42.556724
3514.262522	991903.374589	42.561728
3514.167562	991608.836980	42.566733
3514.365012	991332.470200	42.571738
3514.080697	991068.748623	42.576743
3514.197633	990804.948729	42.581748
3513.786403	990526.107549	42.586752
3514.013810	990241.588428	42.591757
3514.134892	989971.507427	42.596762
3513.675083	989696.047202	42.601767
3514.146122	989423.249044	42.606772
3513.802447	989173.690495	42.611776
3513.782735	988890.900397	42.616781
3513.871191	988611.785560	42.621786
3513.683221	988352.019535	42.626791
3514.213063	988075.049589	42.631796
3514.035092	987807.647017	42.636800
3513.912894	987527.928350	42.641805
3513.555733	987253.406340	42.646810
3513.760190	986988.634553	42.651815
3513.589397	986723.424332	42.656820
3513.435230	986464.054588	42.661824
3513.502575	986194.388862	42.666829
3513.512972	985918.570844	42.671834
3513.145416	985670.912375	42.676839
3513.823920	985422.485197	42.681844
3513.436557	985146.695358	42.686848
3513.605499	984888.372101	42.691853
3513.650739	984613.656673	42.696858
3513.000265	984338.359200	42.701863
3513.686757	984070.638925	42.706868
3513.478988	983829.122703	42.711872
3513.168169	983560.175819	42.716877
3513.444945	983295.904177	42.721882
3512.987434	983048.341941	42.726887
3513.173618	982778.592818	42.731892
3513.085198	982517.274957	42.736896
3512.990212	982265.907997	42.741901
3513.106875	982019.183210	42.746906
3513.004826	981765.451343	42.751911
3512.934633	981492.851209	42.756916
3512.999955	981232.132975	42.761920
3513.033624	980997.490304	42.766925
3513.148075	980737.132142	42.771930
3512.894022	980492.258602	42.776935
3513.226313	980224.221010	42.781940
3512.686851	979970.188368	42.786945
3512.703236	979721.231405	42.791949
3513.013786	979470.456336	42.796954
3512.758707	979209.503197	42.801959
3512.893073	978963.718477	42.806964
3512.913661	978721.460038	42.811969
3512.671620	978455.779562	42.816973
3512.883156	978189.425638	42.821978
3512.120933	977955.766561	42.826983
3512.725890	977708.677568	42.831988
3512.507962	977442.066370	42.836993
3512.479173	977209.624479	42.841997
3512.584717	976983.993854	42.847002
3512.366725	976730.546388	42.852007
3512.371028	976469.523310	42.857012
3512.439740	976224.902707	42.862017
3512.530507	975990.631825	42.867021
3512.548334	975733.288288	42.872026
3512.194353	975503.959551	42.877031
3512.348071	975253.025531	42.882036
3512.407976	975007.376551	42.887041
3512.179652	974769.587913	42.892045
3512.561245	974530.710989	42.897050
3512.532808	974274.874320	42.902055
3512.415539	974022.659657	42.907060
3512.043369	973795.417244	42.912065
3511.926010	973545.626834	42.917069
3512.154676	973310.147717	42.922074
3511.568274	973083.499271	42.927079
3511.815247	972838.900414	42.932084
3511.668371	972621.748205	42.937089
3511.624504	972398.113842	42.942093
3511.806431	972153.105134	42.947098
3511.611347	971915.583992	42.952103
3512.049755	971695.462936	42.957108
3511.962883	971474.930716	42.962113
3511.602262	971230.852636	42.967117
3511.986462	970982.140080	42.972122
3511.774497	970754.848660	42.977127
3511.851987	970526.326189	42.982132
3511.709018	970293.133237	42.987137
3511.463850	970066.505117	42.992141
3511.581284	969836.578406	42.997146
3511.371053	969607.968906	43.002151
3511.832894	969367.689252	43.007156
3511.667036	969161.665968	43.012161
3511.542517	968928.610355	43.017165
3511.547779	968681.818461	43.022170
3511.400080	968455.796014	43.027175
3511.397462	968242.174566	43.032180
3511.076169	968027.031149	43.037185
3510.967119	967798.626715	43.042189
3511.411749	967578.542712	43.047194
3510.993416	967363.782115	43.052199
3511.426922	967117.440043	43.057204
3510.945672	966903.945629	43.062209
3511.031269	966692.210597	43.067213
3511.399647	966458.973678	43.072218
3511.047035	966253.072766	43.077223
3511.031410	966047.402803	43.082228
3511.107863	965825.353558	43.087233
3510.871378	965605.502157	43.092237
3511.155902	965381.736402	43.097242
3510.747268	965186.581301	43.102247
3511.233094	964957.966091	43.107252
3511.273850	964726.966025	43.112257
3510.902117	964514.442485	43.117261
3511.045419	964301.826270	43.122266
3510.777931	964082.901527	43.127271
3511.174748	963869.933692	43.132276
3510.653875	963671.414450	43.137281
3510.555314	963437.250189	43.142285
3510.993431	963212.982932	43.147290
3510.745394	963011.946289	43.152295
3511.095262	962792.380852	43.157300
3510.994868	962573.077213	43.162305
3510.637158	962381.444643	43.167309
3510.836175	962169.328577	43.172314
3510.559170	961962.869714	43.177319
3510.585213	961757.431696	43.182324
3510.589901	961533.072462	43.187329
3510.496652	961325.482310	43.192333
3510.395779	961109.847891	43.197338
3510.314936	960902.730602	43.202343
3510.577051	960678.295717	43.207348
3510.560085	960496.543653	43.212353
3510.540177	960299.002119	43.217357
3510.660558	960085.841989	43.222362
3510.586338	959874.568912	43.227367
3510.592169	959663.176865	43.232372
3510.267413	959452.321789	43.237377
3510.200537	959246.907712	43.242381
3510.248335	959035.289642	43.247386
3509.914940	958844.712232	43.252391
3510.220402	958644.412755	43.257396
3510.266447	958468.764661	43.262401
3510.339790	958256.329275	43.267405
3510.389705	958041.830315	43.272410
3510.191571	957843.253313	43.277415
3509.976590	957635.256193	43.282420
3510.214743	957449.737053	43.287425
3509.919912	957254.294516	43.292429
3510.323651	957050.098043	43.297434
3510.067629	956860.521429	43.302439
3509.954928	956669.345381	43.307444
3509.915604	956465.299323	43.312449
3509.943192	956270.260913	43.317453
3509.787670	956078.974280	43.322458
3509.671406	955876.542918	43.327463
3509.769646	955671.130096	43.332468
3509.635732	955497.400014	43.337473
3509.600378	955305.956051	43.342477
3509.916834	955113.490599	43.347482
3509.338407	954936.563013	43.352487
3509.641270	954754.893340	43.357492
3509.393200	954585.933038	43.362497
3509.556303	954395.569918	43.367501
3509.480925	954197.491180	43.372506
3509.205547	954021.247120	43.377511
3509.718902	953846.588917	43.382516
3509.612951	953671.644101	43.387521
3509.484396	953478.042307	43.392525
3509.581412	953279.708242	43.397530
3509.348277	953101.512102	43.402535
3509.307779	952927.009375	43.407540
3509.646612	952759.422774	43.412545
3509.496091	952580.812171	43.417549
3509.554225	952401.873912	43.422554
3509.200889	952210.174853	43.427559
3509.456240	952029.947159	43.432564
3509.496079	951857.499978	43.437569
3509.326058	951671.205206	43.442573
3509.739701	951469.303689	43.447578
3509.308243	951300.934933	43.452583
3509.228683	951133.364072	43.457588
3509.296040	950979.641804	43.462593
3508.955341	950774.678708	43.467597
3509.297407	950593.046238	43.472602
3509.143612	950423.645778	43.477607
3509.440724	950243.827099	43.482612
3509.365718	950066.743838	43.487617
3509.070438	949911.517681	43.492621
3509.240148	949726.819584	43.497626
3508.875341	949551.202336	43.502631
3508.999244	949354.914055	43.507636
3509.023343	949206.315976	43.512641
3509.014766	949021.334706	43.517645
3509.099349	948843.800095	43.522650
3508.678362	948704.644521	43.527655
3508.681321	948511.982718	43.532660
3508.834663	948337.387843	43.537665
3508.827461	948188.861357	43.542669
3508.796718	948010.359418	43.547674
3508.625206	947828.618293	43.552679
3508.829310	947666.921401	43.557684
3508.593487	947509.793407	43.562689
3508.650093	947345.907906	43.567693
3508.836313	947189.754245	43.572698
3508.814791	947013.610915	43.577703
3509.205698	946838.638915	43.582708
3508.677329	946669.176770	43.587713
3508.231500	946512.148841	43.592717
3508.469949	946338.909372	43.597722
3508.120321	946166.431580	43.602727
3508.575118	946007.323978	43.607732
3508.893462	945846.605247	43.612737
3508.532599	945683.310717	43.617741
3508.471023	945526.381237	43.622746
3508.116618	945383.676004	43.627751
3508.728051	945219.440202	43.632756
3508.511228	945056.389668	43.637761
3508.260476	944885.961079	43.642765
3508.343177	944717.484366	43.647770
3508.105554	944569.946117	43.652775
3508.359468	944423.568556	43.657780
3508.444893	944247.696979	43.662785
3507.981909	944072.580662	43.667789
3508.469984	943923.466941	43.672794
3508.396069	943785.559581	43.677799
3507.914949	943626.820765	43.682804
3508.261607	943450.304124	43.687809
3507.965166	943316.446748	43.692813
3507.948781	943159.630075	43.697818
3507.929228	942992.264626	43.702823
3507.551106	942845.659223	43.707828
3508.007933	942697.186600	43.712833
3507.731446	942537.997435	43.717837
3507.949470	942399.621836	43.722842
3507.871381	942257.264660	43.727847
3507.496440	942097.023648	43.732852
3507.819283	941945.483674	43.737857
3507.581186	941810.427477	43.742861
3507.573604	941662.481337	43.747866
3507.424621	941531.526277	43.752871
3507.789580	941374.305489	43.757876
3507.837614	941207.734705	43.762881
3507.445293	941077.096019	43.767885
3507.880948	940939.796667	43.772890
3507.680135	940790.706922	43.777895
3507.507543	940634.127839	43.782900
3507.616525	940497.350208	43.787905
3507.130357	940339.087646	43.792909
3507.267123	940210.833815	43.797914
3506.872676	940091.584266	43.802919
3507.526060	939935.615568	43.807924
3507.724654	939785.855943	43.812929
3507.538096	939656.970389	43.817933
3507.376522	939515.703419	43.822938
3507.037749	939392.112224	43.827943
3507.360318	939232.819725	43.832948
3507.475585	939107.420327	43.837953
3507.488258	938964.383060	43.842957
3507.287791	938818.690787	43.847962
3507.255053	938697.431242	43.852967
3507.521377	938558.370566	43.857972
3507.407168	938412.940661	43.862977
3507.428949	938293.006022	43.867981
3507.369707	938156.386990	43.872986
3507.385801	938002.288902	43.877991
3507.516132	937848.839166	43.882996
3507.541457	937705.573669	43.888001
3507.414376	937571.157624	43.893005
3507.469576	937441.410240	43.898010
3507.119130	937311.342617	43.903015
3507.376729	937152.189757	43.908020
3507.278007	937013.340338	43.913025
3507.418204	936895.561664	43.918029
3507.421404	936745.651686	43.923034
3507.103433	936618.632792	43.928039
3507.168077	936478.494692	43.933044
3507.071727	936341.930705	43.938049
3506.689139	936225.950859	43.943053
3506.915242	936079.248681	43.948058
3507.152224	935957.209735	43.953063
3506.917116	935824.494759	43.958068
3506.979918	935704.782454	43.963073
3506.939452	935572.701048	43.968077
3507.095396	935427.144277	43.973082
3506.878536	935310.541047	43.978087
3506.834881	935178.066310	43.983092
3507.184787	935040.051146	43.988097
3506.800682	934913.962206	43.993101
3506.675150	934791.572049	43.998106
3506.494537	934663.811468	44.003111
3506.824154	934542.492733	44.008116
3507.169582	934408.974530	44.013121
3506.719839	934256.284084	44.018125
3507.043287	934134.188869	44.023130
3506.952573	934011.294846	44.028135
3506.833305	933882.353037	44.033140
3506.865376	933767.403300	44.038145
3506.374770	933638.420693	44.043149
3506.438681	933502.333214	44.048154
3506.514350	933383.046485	44.053159
3506.487366	933266.463028	44.058164
3506.678817	933136.011351	44.063169
3506.652204	933030.947404	44.068173
3506.609020	932916.375804	44.073178
3506.537358	932794.987180	44.078183
3506.436522	932669.470525	44.083188
3506.458251	932550.270036	44.088193
3506.479893	932417.811651	44.093197
3506.520748	932287.267903	44.098202
3506.843196	932177.134735	44.103207
3506.310370	932044.854447	44.108212
3506.561549	931922.528206	44.113217
3506.510404	931819.365597	44.118221
3506.695753	931696.852891	44.123226
3506.595567	931588.314210	44.128231
3506.437196	931466.044944	44.133236
3506.521697	931335.662822	44.138241
3506.231805	931205.627398	44.143245
3506.238326	931095.427838	44.148250
3506.400066	930961.661173	44.153255
3506.371480	930848.483849	44.158260
3506.189646	930750.990856	44.163265
3506.021299	930624.572383	44.168269
3506.270404	930510.285216	44.173274
3506.413390	930412.444279	44.178279
3506.459766	930286.270697	44.183284
3506.479273	930167.497736	44.188289
3506.193443	930048.291950	44.193293
3506.201570	929922.596556	44.198298
3505.982884	929801.260053	44.203303
3506.021916	929706.786808	44.208308
3506.081445	929600.199514	44.213313
3505.765430	929489.827739	44.218317
3506.319252	929383.443031	44.223322
3506.369703	929284.731734	44.228327
3506.113344	929159.734739	44.233332
3506.182274	929057.844544	44.238337
3506.019354	928935.614202	44.243341
3505.910431	928801.453600	44.248346
3505.997928	928699.841889	44.253351
3506.012662	928588.628098	44.258356
3506.395800	928485.810179	44.263361
3505.846065	928354.017937	44.268365
3506.066857	928248.338434	44.273370
3505.999186	928150.298585	44.278375
3505.902758	928029.863088	44.283380
3506.232914	927928.292923	44.288385
3505.982996	927819.990780	44.293389
3506.181481	927710.555087	44.298394
3506.226208	927592.105399	44.303399
3506.191075	927483.953378	44.308404
3506.299221	927356.931479	44.313409
3505.824206	927275.863985	44.318413
3506.092774	927154.291135	44.323418
3505.821038	927039.534977	44.328423
3505.879379	926940.298487	44.333428
3505.816717	926827.810996	44.338433
3505.690044	926724.466414	44.343437
3506.180686	926623.999027	44.348442
3505.779529	926520.503422	44.353447
3505.476220	926387.949204	44.358452
3505.673692	926283.965806	44.363457
3505.320145	926205.650875	44.368461
3505.600359	926109.535933	44.373466
3505.566067	926005.008327	44.378471
3505.258071	925893.599559	44.383476
3505.327602	925788.185118	44.388481
3505.484049	925700.642533	44.393485
3505.544076	925605.708950	44.398490
3505.466337	925517.047858	44.403495
3505.569374	925408.542829	44.408500
3505.412129	925301.232650	44.413505
3505.202513	925213.838635	44.418509
3505.538187	925102.596044	44.423514
3505.680306	925009.658310	44.428519
3505.364536	924913.620217	44.433524
3505.766938	924810.344144	44.438529
3505.606650	924710.910219	44.443533
3505.700936	924603.256158	44.448538
3505.446746	924504.699635	44.453543
3505.436524	924415.624546	44.458548
3505.753631	924318.798260	44.463553
3505.078305	924225.789280	44.468557
3505.344501	924109.439111	44.473562
3505.276192	924004.204933	44.478567
3505.153022	923909.271693	44.483572
3505.301876	923837.477758	44.488577
3505.373164	923737.891577	44.493581
3505.522027	923625.591067	44.498586
3505.237365	923530.100511	44.503591
3505.250940	923441.871367	44.508596
3505.594348	923339.154201	44.513601
3505.503513	923249.111025	44.518605
3505.575745	923161.156298	44.523610
3505.475728	923063.798953	44.528615
3504.897555	922951.604212	44.533620
3505.131847	922871.508293	44.538625
3504.951526	922781.856981	44.543629
3505.263155	922688.755222	44.548634
3505.145945	922586.099652	44.553639
3505.127237	922497.475531	44.558644
3505.230628	922400.842614	44.563649
3505.162959	922318.478699	44.568653
3505.469215	922217.189898	44.573658
3505.339429	922136.854394	44.578663
3505.145336	922035.740854	44.583668
3505.193295	921942.765965	44.588673
3505.263263	921842.567733	44.593677
3505.385723	921742.840225	44.598682
3505.146884	921665.114274	44.603687
3504.907615	921569.100459	44.608692
3505.365046	921464.404089	44.613697
3505.138248	921400.435878	44.618701
3505.267144	921317.735656	44.623706
3505.013850	921216.520360	44.628711
3505.145463	921106.191839	44.633716
3505.223626	921018.393915	44.638721
3504.975470	920926.701746	44.643725
3505.383119	920838.654138	44.648730
3505.428242	920760.098395	44.653735
3505.121172	920665.908748	44.658740
3505.109618	920564.160180	44.663745
3505.327026	920470.458351	44.668749
3505.393406	920390.064712	44.673754
3505.111889	920296.345797	44.678759
3505.059653	920210.192889	44.683764
3505.096113	920112.760154	44.688769
3505.040532	920026.123524	44.693773
3505.026830	919916.853848	44.698778
3504.940412	919840.039463	44.703783
3504.637126	919766.244349	44.708788
3504.932449	919669.435003	44.713793
3504.858421	919569.603752	44.718797
3504.992963	919494.673747	44.723802
3504.693190	919414.903730	44.728807
3504.812949	919332.656293	44.733812
3505.194518	919252.771685	44.738817
3504.834949	919174.452314	44.743821
3504.684840	919067.113857	44.748826
3505.062672	918978.848551	44.753831
3504.969610	918893.163021	44.758836
3504.930760	918809.585714	44.763841
3504.540322	918724.813179	44.768845
3504.813247	918645.611667	44.773850
3504.756274	918573.493213	44.778855
3504.333668	918483.907257	44.783860
3504.744788	918388.308044	44.788865
3504.988970	918317.388545	44.793869
3504.663867	918236.160912	44.798874
3504.755385	918148.699805	44.803879
3504.738548	918068.670901	44.808884
3504.868251	917999.114450	44.813889
3504.718951	917908.510949	44.818893
3504.790731	917821.240482	44.823898
3504.707240	917736.402055	44.828903
3504.439824	917653.326290	44.833908
3504.811358	917576.886222	44.838913
3504.504108	917499.304749	44.843917
3504.586367	917404.320430	44.848922
3504.708068	917331.867217	44.853927
3504.528222	917259.462713	44.858932
3504.598424	917178.828527	44.863937
3504.548636	917109.868289	44.868941
3504.662595	917029.224695	44.873946
3504.587584	916936.762669	44.878951
3504.403900	916858.092147	44.883956
3504.205105	916759.867739	44.888961
3504.193231	916690.606987	44.893965
3504.598775	916615.207572	44.898970
3504.814668	916546.003815	44.903975
3504.649799	916482.256735	44.908980
3504.803725	916409.304343	44.913985
3504.812834	916323.272734	44.918989
3504.625734	916225.614867	44.923994
3504.677181	916157.396705	44.928999
3504.617269	916076.671407	44.934004
3504.855273	915979.517206	44.939009
3504.769544	915906.886648	44.944013
3504.791537	915816.027647	44.949018
3504.653729	915729.240145	44.954023
3504.329330	915664.257296	44.959028
3504.634065	915574.407587	44.964033
3504.466176	915515.563740	44.969037
3504.400342	915438.587816	44.974042
3504.268503	915366.921261	44.979047
3504.404061	915314.288406	44.984052
3504.777278	915195.128682	44.989057
3504.599648	915116.432202	44.994061
3504.570120	915037.999288	44.999066
3504.703356	914964.067506	45.004071
3504.508410	914884.503293	45.009076
3504.744295	914811.130737	45.014081
3504.418198	914743.824509	45.019085
3504.408010	914647.844067	45.024090
3504.902955	914562.379458	45.029095
3504.606162	914499.980287	45.034100
3504.652330	914406.781122	45.039105
3504.664775	914340.185179	45.044109
3504.547320	914264.357818	45.049114
3504.620716	914191.292897	45.054119
3504.392457	914117.794804	45.059124
3504.729051	914052.491284	45.064129
3504.667314	913958.531280	45.069133
3504.704714	913865.228023	45.074138
3504.547085	913789.207978	45.079143
3504.030974	913707.751992	45.084148
3504.226697	913630.900486	45.089153
3504.198580	913567.964572	45.094157
3504.190721	913490.662708	45.099162
3504.326333	913435.987743	45.104167
3504.177521	913359.671156	45.109172
3504.381791	913293.705718	45.114177
3504.164161	913227.616197	45.119181
3504.247817	913151.740413	45.124186
3504.465989	913063.406342	45.129191
3504.302553	912985.737449	45.134196
3504.481144	912922.760134	45.139201
3504.179010	912847.232906	45.144205
3504.453131	912766.211260	45.149210
3504.247066	912690.762471	45.154215
3504.340437	912636.086549	45.159220
3504.355337	912571.975356	45.164225
3504.157190	912494.980114	45.169229
3504.068617	912411.313636	45.174234
3504.147098	912344.586332	45.179239
3504.004496	912263.433140	45.184244
3503.963059	912197.495094	45.189249
3503.725757	912143.254409	45.194253
3504.026478	912084.296743	45.199258
3504.147049	912004.735436	45.204263
3504.040877	911933.694932	45.209268
3503.926572	911870.078965	45.214273
3503.780250	911807.624558	45.219277
3504.172831	911744.020074	45.224282
3504.007982	911688.413128	45.229287
3504.125714	911619.356534	45.234292
3504.124020	911538.265922	45.239297
3503.936826	911475.043113	45.244301
3503.801042	911403.807840	45.249306
3504.008798	911348.232533	45.254311
3503.907301	911294.925426	45.259316
3504.045612	911212.649866	45.264321
3503.867778	911149.614658	45.269325
3503.911457	911080.756410	45.274330
3504.033176	911021.334770	45.279335
3503.888768	910980.471384	45.284340
3504.191981	910889.002775	45.289345
3503.826391	910811.336655	45.294349
3503.940120	910748.345298	45.299354
3503.916048	910703.120405	45.304359
3503.219940	910634.474902	45.309364
3503.683372	910553.968354	45.314369
3503.627868	910518.487549	45.319373
3503.699393	910473.727243	45.324378
3503.841432	910403.108443	45.329383
3503.783888	910335.125597	45.334388
3503.927829	910264.890501	45.339393
3503.763934	910221.227830	45.344397
3503.993942	910140.753744	45.349402
3503.881694	910080.878340	45.354407
3503.775316	910021.580018	45.359412
3503.998436	909952.195971	45.364417
3503.869588	909889.717082	45.369421
3503.699442	909829.076888	45.374426
3503.915920	909759.305719	45.379431
3503.885217	909697.676588	45.384436
3503.552847	909646.417220	45.389441
3503.820560	909568.243572	45.394445
3503.925527	909517.875555	45.399450
3503.972045	909476.390902	45.404455
3503.580309	909413.853504	45.409460
3503.995873	909338.931911	45.414465
3503.852110	909284.358465	45.419469
3503.689806	909218.694302	45.424474
3503.757612	909142.669790	45.429479
3503.735550	909084.601623	45.434484
3503.866192	909026.025367	45.439489
3504.125961	908965.112010	45.444493
3504.031045	908908.693954	45.449498
3503.947042	908840.311315	45.454503
3503.884461	908761.023102	45.459508
3504.217347	908696.428868	45.464513
3503.855666	908655.294747	45.469517
3503.902408	908578.204799	45.474522
3503.920847	908515.589744	45.479527
3503.600532	908468.273011	45.484532
3503.575085	908390.517024	45.489537
3503.783776	908321.115030	45.494541
3503.742028	908272.303571	45.499546
3503.851332	908219.607595	45.504551
3503.607730	908157.610560	45.509556
3504.261457	908104.534383	45.514561
3503.777850	908046.338451	45.519565
3503.725476	907956.809876	45.524570
3503.958824	907897.722424	45.529575
3503.533498	907837.102559	45.534580
3503.725778	907770.687516	45.539585
3503.701855	907719.359592	45.544589
3503.551422	907660.525820	45.549594
3503.973916	907591.754972	45.554599
3503.571795	907551.487779	45.559604
3503.846135	907504.740363	45.564609
3503.617455	907436.460827	45.569613
3503.836620	907381.230001	45.574618
3503.872546	907320.528550	45.579623
3503.731449	907253.100809	45.584628
3503.666196	907193.862101	45.589633
3503.622905	907125.837725	45.594637
3503.751367	907059.135238	45.599642
3503.692110	907008.771607	45.604647
3503.276735	906951.035510	45.609652
3503.514117	906885.181527	45.614657
3503.361698	906846.991194	45.619661
3503.593115	906779.399877	45.624666
3503.902400	906732.929771	45.629671
3503.192160	906680.161244	45.634676
3503.465487	906622.211807	45.639681
3503.186242	906561.650533	45.644685
3503.403717	906505.060208	45.649690
3503.808405	906467.837135	45.654695
3503.392813	906415.982686	45.659700
3503.542975	906352.646101	45.664705
3503.441490	906310.100644	45.669709
3503.057299	906240.384406	45.674714
3503.589456	906168.393023	45.679719
3503.475885	906135.017213	45.684724
3503.626989	906090.498157	45.689729
3503.673515	906028.429698	45.694733
3503.413013	905964.287697	45.699738
3503.429617	905910.330468	45.704743
3503.253710	905856.790511	45.709748
3503.606641	905790.228973	45.714753
3503.458676	905748.555604	45.719757
3503.348666	905693.458865	45.724762
3503.547444	905648.542351	45.729767
3503.324968	905611.030791	45.734772
3503.726452	905539.149380	45.739777
3503.322392	905491.048992	45.744781
3503.434250	905426.646448	45.749786
3503.445972	905377.800905	45.754791
3503.327592	905323.956794	45.759796
3503.447761	905265.246311	45.764801
3503.255648	905229.078631	45.769805
3503.456953	905180.007076	45.774810
3503.751265	905098.098253	45.779815
3503.661027	904974.837659	45.784820
3503.523449	904792.693418	45.789825
3503.278232	904556.496904	45.794829
3503.305056	904285.584974	45.799834
3503.431363	903943.290634	45.804839
3503.120347	903524.668099	45.809844
3503.219505	903048.488381	45.814849
3503.149852	902520.820162	45.819853
3502.824108	901904.766544	45.824858
3502.939708	901234.863430	45.829863
3502.847138	900518.251511	45.834868
3502.679079	899720.105966	45.839873
3502.547383	898853.807214	45.844877
3502.454852	897924.253330	45.849882
3502.495045	896902.009315	45.854887
3501.930840	895808.129436	45.859892
3501.981508	894653.784166	45.864897
3501.849106	893417.981204	45.869901
3501.666871	892101.614178	45.874906
3501.498932	890736.167770	45.879911
3500.976051	889287.497741	45.884916
3501.005840	887717.823746	45.889921
3500.839077	886103.785565	45.894925
3500.851921	884393.937645	45.899930
3500.387751	882615.732297	45.904935
3499.697721	880748.128009	45.909940
3499.786980	878795.531210	45.914945
3499.607936	876762.010307	45.919949
3499.338015	874644.835580	45.924954
3499.097439	872435.552493	45.929959
3498.233010	870163.985241	45.934964
3498.319550	867781.036266	45.939969
3497.624270	865356.746766	45.944973
3497.384792	862816.484441	45.949978
3497.252216	860196.548944	45.954983
3496.430410	857515.174158	45.959988
3496.202943	854730.891091	45.964993
3495.887212	851872.416213	45.969997
3495.287272	848918.345779	45.975002
3494.756423	845906.325254	45.980007
3493.958204	842794.440272	45.985012
3493.637119	839607.025940	45.990017
3493.195212	836337.976252	45.995021
3492.834624	832995.058891	46.000026
3492.404261	829554.542448	46.005031
3491.759365	826055.576957	46.010036
3491.145651	822437.619251	46.015041
3490.522445	818736.184418	46.020045
3490.104107	814976.732625	46.025050
3489.276467	811127.234113	46.030055
3488.552149	807195.365189	46.035060
3487.966121	803197.337306	46.040065
3487.362966	799121.545319	46.045069
3486.392511	794944.353573	46.050074
3486.457092	790678.842095	46.055079
3485.330402	786329.277054	46.060084
3484.727338	781895.987565	46.065089
3484.090636	777400.508652	46.070093
3482.948015	772826.079617	46.075098
3482.452065	768140.395586	46.080103
3481.496510	763376.764270	46.085108
3480.687502	758546.228286	46.090113
3479.705560	753633.879879	46.095117
3478.950747	748654.907157	46.100122
3478.370674	743554.227802	46.105127
3477.355230	738391.191150	46.110132
3476.618338	733138.757982	46.115137
3475.549849	727791.101190	46.120141
3474.396345	722371.745546	46.125146
3473.435614	716877.129634	46.130151
3472.604206	711313.324562	46.135156
3471.789973	705639.471037	46.140161
3470.968746	699895.785678	46.145165
3469.858223	694047.705274	46.150170
3468.897835	688124.037288	46.155175
3467.824729	682109.692728	46.160180
3466.530710	675988.871952	46.165185
3465.488889	669824.110286	46.170189
3464.235612	663575.433543	46.175194
3463.075984	657238.253746	46.180199
3461.882825	650827.488572	46.185204
3460.696079	644349.167274	46.190209
3459.338104	637769.437179	46.195213
3458.292346	631117.752123	46.200218
3457.329856	624378.613835	46.205223
3456.045801	617539.526277	46.210228
3454.669595	610614.954255	46.215233
3453.398964	603642.550991	46.220237
3451.875581	596585.060382	46.225242
3450.366091	589420.065487	46.230247
3448.680070	582185.978848	46.235252
3447.531894	574877.833243	46.240257
3445.943631	567507.649443	46.245261
3444.335079	560053.747937	46.250266
3443.097162	552508.120442	46.255271
3441.460964	544900.460499	46.260276
3440.046143	537184.308446	46.265281
3438.146155	529398.956520	46.270285
3436.496534	521565.211502	46.275290
3435.149313	513634.195059	46.280295
3433.280836	505623.875562	46.285300
3431.726955	497553.557987	46.290305
3430.013938	489415.373973	46.295309
3428.097772	481183.146076	46.300314
3426.401139	472888.582267	46.305319
3424.493540	464524.570389	46.310324
3422.779606	456063.421932	46.315329
3420.776291	447544.457237	46.320333
3418.964454	438952.209101	46.325338
3416.893361	430297.944181	46.330343
3414.563561	421552.535279	46.335348
3412.844836	412762.539709	46.340353
3410.551950	403918.827622	46.345357
3408.459232	394982.333564	46.350362
3406.239940	385964.746008	46.355367
3403.735800	376899.513357	46.360372
3401.391548	367784.140455	46.365377
3398.972853	358631.586706	46.370381
3396.583357	349397.878801	46.375386
3394.605009	340100.097176	46.380391
3391.676869	330746.950941	46.385396
3389.718044	321327.503111	46.390401
3386.825360	311875.265164	46.395405
3384.082884	302358.271357	46.400410
3381.565714	292798.192581	46.405415
3378.591130	283191.218689	46.410420
3375.974302	273527.898526	46.415425
3372.937297	263832.667162	46.420429
3370.084393	254097.852901	46.425434
3367.116695	244308.247026	46.430439
3363.724342	234473.811852	46.435444
3361.014600	224593.306003	46.440449
3357.928753	214619.843233	46.445453
3354.120595	204689.876945	46.450458
3350.586817	194740.835938	46.455463
3346.705202	184769.840817	46.460468
3342.868704	174778.036161	46.465473
3339.262849	164750.220589	46.470477
3335.118917	154712.658796	46.475482
3331.074552	144679.385421	46.480487
3326.571060	134675.547170	46.485492
3321.851044	124644.751252	46.490497
3316.767455	114624.562679	46.495501
3311.215387	104644.534334	46.500506
3305.443934	94683.616867	46.505511
3298.388673	84808.111953	46.510516
3288.453703	75029.025463	46.515521
3265.902457	65687.403778	46.520525
3230.622782	56942.238141	46.525530
3190.150763	48810.422421	46.530535
3147.027342	41326.468871	46.535540
3105.427932	34587.254764	46.540545
3067.509088	28644.648169	46.545549
3033.714226	23480.251063	46.550554
3004.679276	19055.421393	46.555559
2979.519076	15330.004899	46.560564
2958.299391	12250.236968	46.565569
2940.510141	9759.103440	46.570573
2925.855122	7774.058919	46.575578
2914.133359	6218.227155	46.580583
2904.540411	5027.799624	46.585588
2897.408469	4124.839224	46.590593
2891.755471	3444.576876	46.595597
2887.480563	2951.849311	46.600602
2884.125764	2605.196159	46.605607
2881.832758	2398.199117	46.610612
2880.535972	2231.703498	46.615617
2879.194272	2113.318350	46.620621
2877.925946	2046.356845	46.625626
2877.369110	1978.761950	46.630631
2876.489051	1942.858043	46.635636
2876.342858	1864.129940	46.640641
2875.644948	1814.127516	46.645645
2874.719096	1726.580656	46.650650
2874.056406	1606.025289	46.655655
2872.693261	1503.335535	46.660660
2871.461479	1359.820980	46.665665
2869.770365	1228.889176	46.670669
2868.132367	1036.485816	46.675674
2866.420601	835.166573	46.680679
2863.945604	633.494861	46.685684
2861.604603	407.477716	46.690689
2858.601400	198.440193	46.695693
2845.988659	242.389690	46.700698
2836.583508	266.404630	46.705703
2831.461960	273.591696	46.710708
2828.672970	280.907508	46.715713
2827.035990	266.627174	46.720717
2825.181351	250.760633	46.725722
2823.457749	250.981377	46.730727
2820.885762	260.094525	46.735732
2817.966081	266.637547	46.740737
2814.722481	262.511185	46.745741
2810.973209	243.169723	46.750746
2808.123418	249.637491	46.755751
2804.487563	274.526776	46.760756
2801.169241	265.725370	46.765761
2797.972202	255.142972	46.770765
2794.462727	261.563144	46.775770
2791.473404	266.224953	46.780775
2788.021264	268.585397	46.785780
2785.263608	254.198138	46.790785
2781.946222	236.136813	46.795789
2778.106540	241.889502	46.800794
2775.018595	249.605204	46.805799
2771.717335	252.461947	46.810804
2768.352723	263.989436	46.815809
2764.783572	265.656531	46.820813
2761.731222	256.899790	46.825818
2758.445000	242.752901	46.830823
2754.901782	252.675201	46.835828
2751.284682	239.086577	46.840833
2747.976649	253.396532	46.845837
2744.393937	248.867785	46.850842
2741.078938	247.890304	46.855847
2737.668751	243.438576	46.860852
2734.215162	224.828073	46.865857
2731.022233	221.640939	46.870861
2727.608098	238.684604	46.875866
2723.978004	236.248652	46.880871
2721.181003	238.709456	46.885876
2717.729724	232.780229	46.890881
2714.196518	229.490474	46.895885
2709.925323	236.191037	46.900890
2706.886031	235.897138	46.905895
2703.429474	226.686017	46.910900
2699.826539	227.082968	46.915905
2697.454624	220.878826	46.920909
2693.948820	248.939254	46.925914
2689.907393	224.683776	46.930919
2686.001304	218.458240	46.935924
2683.419025	220.849026	46.940929
2679.766974	230.919598	46.945933
2676.132406	232.272859	46.950938
2672.569520	211.511418	46.955943
2668.998512	229.170681	46.960948
2665.571605	235.645150	46.965953
2662.192553	230.887250	46.970957
2658.825370	217.151449	46.975962
2654.890452	220.732920	46.980967
2651.585347	230.793354	46.985972
2648.237133	236.168425	46.990977
2644.876708	219.700689	46.995981
2641.255070	220.625864	47.000986
2638.436090	216.182368	47.005991
2634.713528	218.859632	47.010996
2631.215589	227.514046	47.016001
2627.952343	221.120892	47.021005
2624.035033	212.120253	47.026010
2620.908171	219.396804	47.031015
2617.425633	241.155794	47.036020
2613.656650	219.275640	47.041025
2610.488230	205.362978	47.046029
2606.746483	229.758390	47.051034
2603.195253	215.760176	47.056039
2599.467013	220.474325	47.061044
2596.514826	222.686412	47.066049
2593.373371	225.544098	47.071053
2589.504036	206.261009	47.076058
2586.275107	215.143546	47.081063
2582.438203	237.502259	47.086068
2579.188178	218.671850	47.091073
2575.930555	198.153838	47.096077
2572.292923	206.523609	47.101082
2568.642153	210.685776	47.106087
2565.413162	218.824415	47.111092
2561.370061	219.422747	47.116097
2558.195125	227.324204	47.121101
2554.520435	221.816637	47.126106
2551.075644	210.500458	47.131111
2547.600214	220.274016	47.136116
2544.086906	218.455978	47.141121
2541.026323	220.765569	47.146125
2537.141207	212.609343	47.151130
2533.878258	213.089602	47.156135
2530.153103	219.170753	47.161140
2526.976012	222.063738	47.166145
2523.350910	212.308248	47.171149
2519.828815	202.787537	47.176154
2516.455366	204.665835	47.181159
2512.823166	217.875966	47.186164
2509.566720	205.416876	47.191169
2506.013884	205.781486	47.196173
2502.658920	231.036800	47.201178
2499.214522	212.955682	47.206183
2495.430099	203.811086	47.211188
2491.723064	220.102255	47.216193
2488.533792	225.836597	47.221197
2485.000375	203.451200	47.226202
2481.382647	195.245696	47.231207
2477.817737	199.895275	47.236212
2474.409451	199.111263	47.241217
2471.529021	198.539312	47.246221
2467.538115	205.758527	47.251226
2464.382157	197.821763	47.256231
2460.510054	193.720899	47.261236
2457.130995	208.463148	47.266241
2453.752991	216.761348	47.271245
2449.814222	210.554657	47.276250
2446.693993	184.550686	47.281255
2443.284178	200.132280	47.286260
2439.341944	215.210778	47.291265
2436.251778	201.145034	47.296269
2432.381013	193.466839	47.301274
2429.391918	186.367046	47.306279
2426.016308	204.498815	47.311284
2422.333960	204.232453	47.316289
2418.911914	191.264774	47.321293
2415.124512	214.582591	47.326298
2411.832830	212.358824	47.331303
2408.225838	203.055887	47.336308
2404.571366	193.694002	47.341313
2401.142359	202.610279	47.346317
2397.461795	210.090376	47.351322
2394.217392	200.872471	47.356327
2390.737786	179.686463	47.361332
2387.364155	179.363684	47.366337
2384.280535	193.904310	47.371341
2380.749616	209.721352	47.376346
2377.152392	188.711688	47.381351
2373.572915	193.996348	47.386356
2369.820135	203.861472	47.391361
2366.169164	200.527886	47.396365
2362.172018	194.542582	47.401370
2358.955411	181.031348	47.406375
2355.921841	194.875945	47.411380
2352.594317	193.279709	47.416385
2348.842810	179.809246	47.421389
2345.173508	192.209796	47.426394
2341.999255	188.262239	47.431399
2338.369454	180.937879	47.436404
2334.497711	188.692691	47.441409
2331.033808	181.926951	47.446413
2327.730865	195.569062	47.451418
2324.620693	206.972314	47.456423
2321.098378	190.788197	47.461428
2317.485504	183.467073	47.466433
2314.247960	181.250310	47.471437
2310.771024	189.058991	47.476442
2307.409437	188.446896	47.481447
2303.615385	178.052357	47.486452
2299.626407	181.821460	47.491457
2296.291854	188.110353	47.496461
2292.774578	203.721650	47.501466
2289.357576	182.831887	47.506471
2285.712900	177.155775	47.511476
2282.500547	181.076274	47.516481
2279.367262	193.418041	47.521485
2275.215632	205.527649	47.526490
2271.824850	186.480382	47.531495
2268.237425	189.234960	47.536500
2265.077490	202.693897	47.541505
2261.346671	199.848531	47.546509
2257.683677	178.163610	47.551514
2254.428295	174.307310	47.556519
2250.999502	203.766792	47.561524
2247.575291	186.757818	47.566529
2244.291709	171.763366	47.571533
2240.621514	199.905541	47.576538
2236.599511	190.748402	47.581543
2233.068055	183.868670	47.586548
2229.433648	175.624441	47.591553
2226.676971	180.546954	47.596557
2223.358669	190.262434	47.601562
2219.859822	177.972348	47.606567
2216.200361	172.347744	47.611572
2211.926957	164.224117	47.616577
2208.943097	180.211286	47.621581
2205.124295	194.195103	47.626586
2202.012322	184.420888	47.631591
2198.339918	163.252334	47.636596
2195.035130	182.599647	47.641601
2191.453652	172.806011	47.646605
2188.071959	188.545700	47.651610
2184.486435	177.974095	47.656615
2181.504548	176.199888	47.661620
2177.771961	180.072170	47.666625
2174.012781	156.497307	47.671629
2170.133441	177.903387	47.676634
2166.893370	181.826135	47.681639
2163.670051	191.203486	47.686644
2159.767291	180.816310	47.691649
2156.641431	178.448318	47.696653
2152.944732	185.918538	47.701658
2149.662817	184.479421	47.706663
2145.800558	174.510558	47.711668
2142.145880	164.824226	47.716673
2138.937667	175.035627	47.721677
2135.507632	174.821605	47.726682
2132.356722	180.282393	47.731687
2128.495040	185.259257	47.736692
2125.194832	169.508813	47.741697
2121.617418	176.897909	47.746701
2117.750789	197.163920	47.751706
2114.281394	175.896419	47.756711
2110.897404	168.418694	47.761716
2107.503471	188.724218	47.766721
2104.517945	181.253665	47.771725
2100.446328	187.357511	47.776730
2096.677063	168.484285	47.781735
2093.362110	165.798396	47.786740
2089.879777	177.898482	47.791745
2086.603568	183.464301	47.796749
2083.053233	180.762984	47.801754
2079.479708	159.581368	47.806759
2076.196860	162.802806	47.811764
2072.277804	184.855213	47.816769
2068.946425	168.683487	47.821773
2065.257577	168.991525	47.826778
2061.971879	168.290375	47.831783
2058.612064	179.878301	47.836788
2055.153375	174.247893	47.841793
2051.673356	172.482616	47.846797
2048.137685	191.349957	47.851802
2044.454634	182.394310	47.856807
2040.944810	168.749334	47.861812
2037.419275	164.674018	47.866817
2034.322669	175.431115	47.871821
2030.181962	185.811376	47.876826
2026.741562	178.839200	47.881831
2023.511083	171.679496	47.886836
2019.695337	162.994064	47.891841
2016.482990	164.970197	47.896845
2012.486354	178.628271	47.901850
2009.511275	152.898044	47.906855
2006.151673	155.402566	47.911860
2002.429615	161.531848	47.916865
1999.156297	157.559566	47.921869
1995.533740	165.693652	47.926874
1991.978555	185.676781	47.931879
1988.479012	178.179903	47.936884
1984.905039	160.021126	47.941889
1981.559029	146.972841	47.946893
1978.136691	176.769610	47.951898
1974.606533	178.646961	47.956903
1971.327547	179.621477	47.961908
1966.936451	175.586882	47.966913
1963.886725	166.857387	47.971917
1960.487946	170.369382	47.976922
1956.770812	168.867102	47.981927
1953.518728	167.960989	47.986932
1949.987577	188.709430	47.991937
1946.853512	164.446516	47.996941
1943.162543	166.618339	48.001946
1939.178071	154.848432	48.006951
1936.271489	168.402067	48.011956
1932.190611	182.985391	48.016961
1929.033230	180.039194	48.021965
1925.662276	176.103766	48.026970
1921.978627	169.445039	48.031975
1918.748678	169.803714	48.036980
1914.654569	157.503027	48.041985
1911.197729	169.067443	48.046989
1907.850094	184.774954	48.051994
1904.403554	171.835219	48.056999
1900.962876	152.000870	48.062004
1897.010277	164.917177	48.067009
1893.949179	158.416788	48.072013
1890.382286	162.269460	48.077018
1887.365288	164.371256	48.082023
1883.977497	170.049767	48.087028
1879.958989	168.653084	48.092033
1876.689480	170.068024	48.097037
1872.825084	168.269180	48.102042
1869.154255	152.522448	48.107047
1865.854937	154.148090	48.112052
1862.281607	185.889505	48.117057
1858.750262	175.303240	48.122061
1855.337764	171.013945	48.127066
1851.951061	178.826260	48.132071
1848.308177	162.521896	48.137076
1845.130072	156.359570	48.142081
1841.417681	144.202440	48.147085
1837.766824	153.771852	48.152090
1834.188374	166.627147	48.157095
1831.240132	150.322338	48.162100
1827.463769	146.700773	48.167105
1824.285155	155.574147	48.172109
1820.318979	184.266442	48.177114
1816.694181	167.311581	48.182119
1813.387467	147.515470	48.187124
1809.760171	160.650604	48.192129
1806.651655	164.125033	48.197133
1802.861825	176.980794	48.202138
1799.175343	159.964019	48.207143
1795.695558	138.159002	48.212148
1792.112987	155.925303	48.217153
1789.007740	158.007762	48.222157
1785.630200	152.144823	48.227162
1782.057978	160.698330	48.232167
1778.474023	151.065962	48.237172
1775.138461	153.209610	48.242177
1771.346388	155.111229	48.247181
1767.735351	159.492596	48.252186
1764.345113	165.058506	48.257191
1760.673029	160.837842	48.262196
1757.157509	167.320550	48.267201
1754.010548	163.956324	48.272205
1750.396768	166.340522	48.277210
1746.881891	158.198694	48.282215
1743.405625	139.759707	48.287220
1739.911537	157.615401	48.292225
1736.527502	164.002139	48.297229
1732.713314	157.311008	48.302234
1728.947178	137.479497	48.307239
1725.946372	151.542058	48.312244
1722.455876	159.382587	48.317249
1719.145942	164.765197	48.322253
1715.246684	152.477783	48.327258
1711.659446	151.730663	48.332263
1708.197332	164.508603	48.337268
1704.681191	166.574946	48.342273
1701.325339	167.448622	48.347277
1697.839543	168.763391	48.352282
1694.207639	166.440539	48.357287
1690.971631	166.779105	48.362292
1687.079428	162.536501	48.367297
1684.139179	136.148122	48.372301
1680.297142	142.408910	48.377306
1676.723978	159.026319	48.382311
1673.229818	155.593944	48.387316
1669.717425	158.770563	48.392321
1666.380789	141.221972	48.397325
1662.949596	150.366927	48.402330
1659.261865	169.332344	48.407335
1656.204560	145.693279	48.412340
1651.992240	163.622439	48.417345
1648.650404	147.962149	48.422349
1645.150791	150.789822	48.427354
1641.595274	157.794217	48.432359
1638.592490	151.325176	48.437364
1634.802429	161.607494	48.442369
1631.097452	142.536104	48.447373
1627.989472	134.189995	48.452378
1624.297981	137.768583	48.457383
1620.941494	137.145512	48.462388
1616.847547	136.266413	48.467393
1613.849692	143.662068	48.472397
1610.464591	159.170143	48.477402
1607.161570	169.177177	48.482407
1603.618325	163.672048	48.487412
1599.883309	156.479032	48.492417
1596.027090	154.099437	48.497421
1592.494127	144.745049	48.502426
1588.924201	130.311757	48.507431
1585.654964	142.738865	48.512436
1582.115642	143.367939	48.517441
1578.715850	126.526103	48.522445
1575.201344	147.846468	48.527450
1571.606228	156.147153	48.532455
1568.725363	145.273315	48.537460
1564.706708	158.258264	48.542465
1561.338298	151.356554	48.547469
1557.687789	158.820677	48.552474
1554.330837	127.428286	48.557479
1550.374610	140.431532	48.562484
1546.896871	159.715380	48.567489
1543.811752	148.731825	48.572493
1540.277379	138.071308	48.577498
1536.821231	128.601990	48.582503
1533.385686	141.253362	48.587508
1529.427302	156.649004	48.592513
1526.302735	146.451489	48.597517
1522.581802	137.180057	48.602522
1518.754695	148.924574	48.607527
1515.723982	145.792835	48.612532
1512.030934	140.264940	48.617537
1508.738457	143.503592	48.622541
1505.037809	170.323873	48.627546
1502.050369	146.428341	48.632551
1498.873466	128.957488	48.637556
1494.396771	154.724509	48.642561
1490.962774	150.793600	48.647565
1487.627922	141.920538	48.652570
1484.411531	139.496184	48.657575
1481.017007	146.098422	48.662580
1476.951704	152.684406	48.667585
1473.688571	154.061083	48.672589
1469.995574	159.505630	48.677594
1466.617255	159.517584	48.682599
1463.288471	133.521591	48.687604
1459.521997	129.938362	48.692609
1456.042090	151.332564	48.697613
1452.586125	152.734663	48.702618
1449.135408	142.581846	48.707623
1445.800669	131.657116	48.712628
1441.804295	138.456062	48.717633
1438.510242	149.813240	48.722637
1435.295157	138.852880	48.727642
1431.670694	128.912836	48.732647
1428.495941	122.875468	48.737652
1424.356574	151.315534	48.742657
1420.910505	160.942769	48.747661
1417.670370	149.540952	48.752666
1414.190325	132.204230	48.757671
1410.818507	134.179415	48.762676
1406.983906	157.737424	48.767681
1403.444477	146.426644	48.772685
1400.023689	143.871027	48.777690
1396.238571	160.246310	48.782695
1393.440053	136.467955	48.787700
1389.858365	140.018373	48.792705
1386.285728	143.643357	48.797709
1382.540577	144.644864	48.802714
1378.818847	133.857931	48.807719
1375.463831	131.822199	48.812724
1371.884454	153.900098	48.817729
1368.823569	150.914374	48.822733
1365.037380	141.664562	48.827738
1361.549615	135.890585	48.832743
1357.994636	134.777964	48.837748
1354.328442	151.336051	48.842753
1351.457243	130.942403	48.847757
1347.513324	141.585331	48.852762
1344.158707	138.627979	48.857767
1340.578830	134.974659	48.862772
1336.944319	146.867494	48.867777
1333.539849	135.512887	48.872781
1329.773869	129.842560	48.877786
1326.399140	126.005741	48.882791
1323.384270	128.573519	48.887796
1319.483670	155.687056	48.892801
1316.024111	150.838495	48.897805
1312.320717	135.687947	48.902810
1309.162725	147.203631	48.907815
1305.810089	145.876816	48.912820
1301.719619	139.018087	48.917825
1298.460069	131.755467	48.922829
1294.862697	145.058177	48.927834
1291.302375	147.859733	48.932839
1288.187894	130.125877	48.937844
1284.522324	137.927901	48.942849
1281.360884	149.943126	48.947853
1277.652213	139.056438	48.952858
1273.906650	121.049641	48.957863
1270.443302	132.289897	48.962868
1266.614516	147.398980	48.967873
1263.449065	136.376766	48.972877
1260.259381	126.932387	48.977882
1256.453141	126.628675	48.982887
1252.999931	144.009967	48.987892
1249.186813	141.253925	48.992897
1245.898878	129.727039	48.997901
1242.581882	144.150292	49.002906
1239.061312	144.992381	49.007911
1235.436869	148.618986	49.012916
1231.674482	144.104864	49.017921
1228.673295	143.562131	49.022925
1224.930890	146.135813	49.027930
1221.113275	140.571929	49.032935
1218.006104	151.016229	49.037940
1214.382982	143.723206	49.042945
1211.021892	129.366770	49.047949
1207.093718	130.096523	49.052954
1203.750951	143.580576	49.057959
1200.749729	132.068041	49.062964
1197.099845	134.505521	49.067969
1193.312535	122.278338	49.072973
1189.665309	128.556423	49.077978
1186.236464	126.252322	49.082983
1183.170645	126.973598	49.087988
1179.490485	140.381953	49.092993
1176.013140	146.429977	49.097997
1172.326087	133.050124	49.103002
1168.997201	119.578211	49.108007
1165.188158	131.546278	49.113012
1161.915025	138.852187	49.118017
1158.561364	137.254434	49.123021
1154.896939	126.228543	49.128026
1151.286358	128.088288	49.133031
1147.964742	133.053208	49.138036
1144.317379	134.440292	49.143041
1140.561193	121.369208	49.148045
1137.369843	124.308009	49.153050
1133.631053	146.420369	49.158055
1130.421961	126.927270	49.163060
1126.895015	141.441940	49.168065
1123.242048	140.727385	49.173069
1120.069001	138.183695	49.178074
1115.969526	141.005191	49.183079
1112.618919	132.562294	49.188084
1109.360934	150.046259	49.193089
1106.255943	147.691099	49.198093
1102.383250	129.823092	49.203098
1098.929482	123.490639	49.208103
1095.289318	128.113875	49.213108
1091.385503	150.373651	49.218113
1088.003649	130.690395	49.223117
1084.698936	132.570212	49.228122
1081.120571	128.679246	49.233127
1077.826209	127.925145	49.238132
1074.403514	115.728905	49.243137
1071.184733	110.864814	49.248141
1067.450863	126.428242	49.253146
1063.730593	141.105460	49.258151
1060.251736	128.145883	49.263156
1056.683205	123.921459	49.268161
1053.419849	127.162603	49.273165
1050.012113	142.820970	49.278170
1046.472042	134.022396	49.283175
1042.610678	111.904135	49.288180
1038.915137	127.493997	49.293185
1035.797534	124.680570	49.298189
1032.286240	133.433449	49.303194
1028.483450	125.358540	49.308199
1025.379845	117.036409	49.313204
1021.627906	141.283625	49.318209
1018.147220	127.538158	49.323213
1014.607883	122.292475	49.328218
1010.761373	146.989761	49.333223
1008.395889	121.431516	49.338228
1004.434810	130.247322	49.343233
1000.733169	127.541584	49.348237
997.574396	128.388281	49.353242
993.441208	136.089878	49.358247
990.354980	124.056242	49.363252
986.745326	147.028939	49.368257
983.138435	129.312757	49.373261
979.509894	104.366271	49.378266
975.957491	117.206101	49.383271
972.703272	127.655019	49.388276
968.988429	123.162313	49.393281
965.736615	123.257008	49.398285
962.644899	123.648835	49.403290
959.055237	126.661963	49.408295
955.631236	116.897574	49.413300
951.370933	143.841918	49.418305
947.784141	131.776716	49.423309
944.840630	122.590479	49.428314
941.271711	115.918747	49.433319
937.905816	126.365894	49.438324
933.985414	144.503219	49.443329
930.673564	132.514559	49.448333
926.939790	121.128470	49.453338
923.569756	141.473206	49.458343
920.376146	123.842628	49.463348
916.593463	106.150911	49.468353
913.132236	128.362595	49.473357
909.869502	125.542119	49.478362
905.917331	126.306093	49.483367
902.573282	126.829579	49.488372
898.936983	126.283055	49.493377
895.790723	129.562940	49.498381
892.187790	118.159416	49.503386
888.439995	141.299461	49.508391
885.195968	114.041469	49.513396
881.607028	108.890375	49.518401
878.054415	109.635937	49.523405
874.753166	136.954433	49.528410
870.818070	131.181209	49.533415
867.386833	117.983860	49.538420
863.895464	130.843064	49.543425
860.528117	129.529066	49.548429
857.481833	138.674109	49.553434
853.982087	129.702778	49.558439
850.438939	116.474991	49.563444
846.360408	109.506988	49.568449
843.352073	130.844374	49.573453
839.780459	116.308202	49.578458
835.787027	108.017008	49.583463
832.328088	101.574496	49.588468
828.670161	131.677310	49.593473
825.391926	129.059100	49.598477
822.143247	118.652353	49.603482
818.692853	120.049007	49.608487
815.177678	116.381950	49.613492
811.413767	119.103520	49.618497
808.387650	125.455994	49.623501
804.660158	121.025157	49.628506
801.145619	107.679539	49.633511
797.535470	112.414068	49.638516
793.754965	135.400220	49.643521
790.646035	126.529726	49.648525
787.131121	110.170013	49.653530
783.226210	124.533243	49.658535
779.854777	107.226112	49.663540
776.427645	120.355285	49.668545
773.171256	106.976033	49.673549
769.835581	103.470345	49.678554
766.148629	110.397079	49.683559
762.787632	129.903531	49.688564
758.669252	130.126239	49.693569
755.391133	106.550769	49.698573
752.105044	109.260245	49.703578
748.413955	109.231281	49.708583
745.139363	112.039778	49.713588
741.603120	125.703405	49.718593
737.899832	130.061424	49.723597
734.722832	114.872123	49.728602
730.904242	104.772635	49.733607
727.395972	115.456249	49.738612
723.893543	123.329339	49.743617
720.080331	123.241147	49.748621
716.956540	105.853805	49.753626
713.336620	130.438960	49.758631
710.181309	112.091262	49.763636
706.441446	107.462970	49.768641
702.818449	111.870680	49.773645
699.773073	116.108718	49.778650
696.015294	115.077791	49.783655
692.677369	108.566444	49.788660
688.713902	117.220816	49.793665
685.247188	110.474062	49.798669
682.022792	107.160753	49.803674
678.245005	120.677059	49.808679
674.991350	109.633476	49.813684
671.386595	92.523497	49.818689
667.708393	122.853212	49.823693
664.482939	128.850488	49.828698
660.767327	115.419000	49.833703
657.450361	99.016538	49.838708
653.894023	111.042317	49.843713
650.525709	105.162029	49.848717
647.033153	104.107255	49.853722
643.090771	121.019058	49.858727
640.446476	118.560325	49.863732
636.647707	131.580082	49.868737
632.704874	117.958560	49.873741
629.303486	106.241183	49.878746
625.640054	116.819957	49.883751
622.345491	125.027208	49.888756
618.635063	122.098724	49.893761
615.179419	104.872206	49.898765
611.881652	112.626505	49.903770
608.118213	114.884860	49.908775
604.635561	122.233288	49.913780
601.341402	105.115551	49.918785
597.842805	99.015918	49.923789
594.593281	114.769419	49.928794
590.997634	127.260338	49.933799
587.520855	109.247952	49.938804
583.786184	101.245652	49.943809
580.372150	123.928854	49.948813
577.023809	130.169407	49.953818
573.253902	128.797655	49.958823
569.920768	122.298209	49.963828
566.515662	118.409211	49.968833
562.679143	115.304985	49.973837
559.448931	111.127566	49.978842
555.376884	113.976718	49.983847
552.238063	113.143527	49.988852
548.612554	133.126500	49.993857
545.693605	107.211935	49.998861
541.858851	105.338544	50.003866
538.691118	125.776520	50.008871
535.023111	99.739452	50.013876
531.319356	97.553227	50.018881
527.942321	104.822607	50.023885
524.363698	132.215686	50.028890
520.247622	123.591015	50.033895
517.249845	102.051837	50.038900
513.650741	99.632103	50.043905
510.086762	112.012088	50.048909
506.356714	118.924861	50.053914
502.981020	121.539956	50.058919
500.239407	106.598687	50.063924
496.301649	116.598422	50.068929
492.588245	123.246251	50.073933
489.240741	117.344758	50.078938
485.551765	97.619860	50.083943
482.500764	110.244478	50.088948
478.676330	129.770868	50.093953
475.321046	115.893099	50.098957
471.885623	99.288450	50.103962
467.580502	108.571911	50.108967
464.512909	85.336283	50.113972
460.983483	98.294533	50.118977
457.810182	119.808025	50.123981
454.765364	108.278157	50.128986
450.686686	106.670719	50.133991
447.076964	91.072206	50.138996
443.342581	101.017326	50.144001
439.959956	115.686347	50.149005
437.309925	109.507794	50.154010
433.466308	99.588932	50.159015
430.095470	112.379451	50.164020
426.319358	118.238632	50.169025
422.080140	110.068921	50.174029
419.258012	112.797896	50.179034
415.527210	112.790970	50.184039
412.605497	85.059727	50.189044
409.011069	106.086487	50.194049
404.504611	105.104337	50.199053
401.408656	120.474846	50.204058
397.945312	123.454077	50.209063
394.683066	119.525299	50.214068
391.410603	111.006210	50.219073
388.019761	91.979616	50.224077
384.111375	103.294906	50.229082
380.468820	128.848583	50.234087
377.194575	117.679623	50.239092
373.601933	100.313839	50.244097
370.224225	95.528668	50.249101
366.459392	111.736111	50.254106
362.682326	126.923119	50.259111
359.179223	114.202412	50.264116
356.276967	112.219575	50.269121
352.966303	105.252715	50.274125
349.549527	114.838430	50.279130
345.430719	117.027101	50.284135
342.388976	88.830097	50.289140
339.008790	90.653287	50.294145
334.779055	100.349727	50.299149
331.335493	104.194993	50.304154
327.910768	95.602164	50.309159
324.779729	108.629709	50.314164
321.192051	109.090945	50.319169
317.603625	95.923009	50.324173
314.490485	95.074548	50.329178
310.522453	114.359914	50.334183
307.077768	113.287256	50.339188
303.374913	100.552644	50.344193
299.875042	94.698935	50.349197
296.857079	95.848033	50.354202
292.536140	106.796694	50.359207
289.406210	99.931313	50.364212
286.141969	113.359487	50.369217
282.613007	108.935341	50.374221
279.298812	114.122754	50.379226
275.284525	110.527422	50.384231
271.806952	99.590538	50.389236
268.335993	92.974073	50.394241
265.103109	104.918752	50.399245
261.647256	110.324402	50.404250
257.675000	103.163665	50.409255
254.406611	106.364770	50.414260
251.143882	110.999854	50.419265
247.515000	94.684529	50.424269
244.175888	106.037823	50.429274
240.296005	116.557732	50.434279
236.894414	117.418567	50.439284
233.556000	105.642609	50.444289
229.756086	96.892933	50.449293
226.209089	88.309818	50.454298
223.119261	114.143770	50.459303
219.941044	111.066634	50.464308
216.345699	121.211350	50.469313
212.427710	124.079645	50.474317
208.947101	93.471228	50.479322
205.534807	120.931489	50.484327
202.072686	110.805431	50.489332
198.465225	105.508165	50.494337
194.839848	121.397989	50.499341
191.640452	112.207792	50.504346
187.847530	107.232675	50.509351
184.266203	98.282370	50.514356
180.775991	118.909354	50.519361
177.198313	121.600797	50.524365
173.897637	108.450019	50.529370
170.159672	101.363879	50.534375
166.995559	88.967892	50.539380
163.484875	102.791357	50.544385
160.003115	100.069325	50.549389
156.548401	95.792699	50.554394
152.950580	121.145963	50.559399
149.624437	100.314465	50.564404
146.027846	99.095155	50.569409
142.474664	97.422004	50.574413
139.065658	109.766450	50.579418
135.127493	106.434549	50.584423
131.857942	109.051327	50.589428
128.440985	120.023744	50.594433
124.837947	107.841062	50.599437
121.447321	100.863090	50.604442
117.948135	111.791286	50.609447
114.543436	111.645519	50.614452
110.928551	101.885494	50.619457
107.375321	94.690252	50.624461
104.181273	97.156855	50.629466
100.368144	102.119410	50.634471
96.840799	107.163675	50.639476
93.149103	99.969223	50.644481
89.476344	92.321821	50.649485
86.366041	98.773516	50.654490
82.704682	106.664372	50.659495
79.412884	107.460586	50.664500
76.023390	95.356008	50.669505
71.907874	107.376474	50.674509
68.749659	116.946122	50.679514
65.573406	118.472468	50.684519
61.833612	101.809920	50.689524
58.549264	92.253967	50.694529
54.972516	110.221674	50.699533
51.327454	120.963598	50.704538
47.364324	117.344575	50.709543
44.097651	97.406440	50.714548
40.910840	99.024014	50.719553
37.273221	121.625643	50.724557
34.108254	115.893520	50.729562
30.149387	103.872795	50.734567
26.915534	94.761104	50.739572
23.347441	105.099575	50.744577
19.747243	122.355702	50.749581
16.230943	105.549122	50.754586
12.622757	95.536611	50.759591
9.361262	100.713267	50.764596
5.988377	101.665758	50.769601
2.617794	105.939682	50.774605