Wed Jun 15 16:58:26 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.448324	89.235675	0.000000
0.961662	110.887436	0.005005
1.277314	120.450632	0.010010
1.216403	84.109512	0.015014
0.824891	86.417654	0.020019
0.572829	83.031109	0.025024
0.360205	64.583722	0.030029
-0.114559	50.973656	0.035034
0.222590	39.135158	0.040038
0.064862	60.100959	0.045043
-0.654664	59.477794	0.050048
-0.923328	46.770806	0.055053
-1.781684	18.672270	0.060058
-1.602264	9.896462	0.065062
-2.002936	22.583207	0.070067
-1.913571	23.837155	0.075072
-2.851842	2.225661	0.080077
-3.368034	-10.851131	0.085082
-3.493723	7.864237	0.090086
-3.578229	26.430674	0.095091
-3.189387	12.555701	0.100096
-3.411821	-9.535710	0.105101
-3.793720	-6.133024	0.110106
-4.120693	5.029295	0.115110
-4.514466	3.441212	0.120115
-4.670998	-17.303522	0.125120
-4.768981	-1.621150	0.130125
-5.671125	-5.481065	0.135130
-5.754273	-9.081844	0.140134
-6.275701	8.453035	0.145139
-6.116265	-8.675603	0.150144
-6.069288	3.488508	0.155149
-6.168505	2.846485	0.160154
-6.757637	13.152392	0.165158
-7.546263	10.011383	0.170163
-7.841874	6.546528	0.175168
-7.788825	15.256171	0.180173
-7.751762	9.242286	0.185178
-7.598930	-4.906077	0.190182
-8.286193	4.374347	0.195187
-8.541808	19.161542	0.200192
-8.819146	0.144105	0.205197
-9.390208	-6.061659	0.210202
-9.071135	10.417906	0.215206
-10.225087	26.763111	0.220211
-10.174384	17.318646	0.225216
-10.629903	-10.399740	0.230221
-11.072884	6.728085	0.235226
-10.187254	19.972177	0.240230
-10.762483	15.297577	0.245235
-11.071811	-7.276450	0.250240
-11.121039	-2.253548	0.255245
-11.156859	2.563536	0.260250
-12.171199	5.630193	0.265254
-12.563557	5.117209	0.270259
-12.604875	15.393151	0.275264
-12.596038	4.900009	0.280269
-12.656744	8.480348	0.285274
-12.496509	20.456677	0.290278
-13.519396	23.716122	0.295283
-13.820486	3.033035	0.300288
-13.848444	0.090073	0.305293
-14.103942	22.690746	0.310298
-14.006270	1.453367	0.315302
-14.965381	19.821245	0.320307
-15.765526	17.911262	0.325312
-15.442998	1.048243	0.330317
-15.448850	6.108271	0.335322
-15.456748	5.010804	0.340326
-15.700123	6.054285	0.345331
-15.716150	4.825680	0.350336
-16.077122	-11.308623	0.355341
-16.440992	11.744377	0.360346
-17.039761	12.445598	0.365350
-17.355591	13.787125	0.370355
-17.439693	1.745225	0.375360
-17.404101	6.893497	0.380365
-18.077422	3.409880	0.385370
-18.475396	10.470626	0.390374
-18.396670	29.747757	0.395379
-18.704116	20.303194	0.400384
-18.769779	6.500184	0.405389
-18.683839	-3.349999	0.410394
-19.352912	11.955931	0.415398
-19.879220	27.052039	0.420403
-20.086301	5.993752	0.425408
-20.186391	16.262342	0.430413
-20.574880	13.108574	0.435418
-20.146017	-13.261581	0.440422
-20.956667	0.144154	0.445427
-21.573123	11.709737	0.450432
-21.821106	3.150268	0.455437
-22.057326	8.689509	0.460442
-21.943588	-1.464756	0.465446
-21.934057	15.399388	0.470451
-22.331438	15.191654	0.475456
-22.287629	12.995215	0.480461
-23.035530	18.803588	0.485466
-23.151210	1.625313	0.490470
-23.673851	2.246875	0.495475
-23.827236	1.660760	0.500480
-23.906689	26.947752	0.505485
-23.909708	27.076626	0.510490
-24.215311	8.791856	0.515494
-24.925885	-6.833174	0.520499
-25.285298	7.898559	0.525504
-25.119490	20.350027	0.530509
-25.449264	18.901800	0.535514
-25.446647	15.918271	0.540518
-25.810162	26.971525	0.545523
-26.568328	7.818796	0.550528
-26.799945	3.200561	0.555533
-27.084736	21.059853	0.560538
-26.892318	-1.065006	0.565542
-27.017907	5.073568	0.570547
-27.198265	20.783087	0.575552
-27.016276	5.202894	0.580557
-28.046943	14.001178	0.585562
-28.068798	3.728354	0.590566
-28.631710	17.193188	0.595571
-28.461921	7.647371	0.600576
-28.782073	-9.965169	0.605581
-29.315721	2.252379	0.610586
-29.902147	-3.867093	0.615590
-30.141098	4.548797	0.620595
-30.037781	18.793998	0.625600
-30.133654	15.022096	0.630605
-30.321092	14.652117	0.635610
-30.320265	14.061823	0.640614
-31.182926	22.401364	0.645619
-31.608579	17.825353	0.650624
-31.679765	15.908934	0.655629
-32.079224	11.861478	0.660634
-32.019758	0.302792	0.665638
-31.875943	8.723393	0.670643
-31.728216	9.937606	0.675648
-32.381200	15.943859	0.680653
-33.335452	4.764396	0.685658
-33.150102	0.999289	0.690662
-33.210548	5.472718	0.695667
-33.395819	16.187549	0.700672
-34.060665	15.280824	0.705677
-34.624855	18.263228	0.710682
-34.443984	8.516118	0.715686
-34.923561	0.434885	0.720691
-34.729533	-4.990965	0.725696
-34.877932	16.566183	0.730701
-35.375177	32.384706	0.735706
-36.019341	9.090055	0.740710
-36.592956	5.297873	0.745715
-36.467477	7.660837	0.750720
-36.604164	25.837561	0.755725
-36.455336	19.953171	0.760730
-36.479191	-3.563733	0.765734
-36.667893	10.120487	0.770739
-37.320171	28.810150	0.775744
-37.866557	20.153403	0.780749
-38.334857	10.960344	0.785754
-38.009042	10.117274	0.790758
-38.174280	23.042201	0.795763
-38.839089	2.957441	0.800768
-39.109802	8.132166	0.805773
-39.702409	5.684502	0.810778
-39.435506	6.648189	0.815782
-39.806932	27.178914	0.820787
-39.803424	20.930666	0.825792
-39.910986	14.770420	0.830797
-40.693415	2.794906	0.835802
-41.184873	8.594828	0.840806
-41.417424	21.701338	0.845811
-41.844556	11.425057	0.850816
-41.363058	-6.366827	0.855821
-41.617593	-3.037076	0.860826
-41.489289	13.870271	0.865830
-41.626898	23.554573	0.870835
-41.971795	11.876662	0.875840
-42.289030	12.864779	0.880845
-42.824589	10.488279	0.885850
-43.564947	10.431435	0.890854
-44.196312	17.261948	0.895859
-44.489581	13.219828	0.900864
-43.667992	18.861839	0.905869
-43.951733	9.956806	0.910874
-44.267401	8.576190	0.915878
-44.705940	19.105995	0.920883
-44.560649	22.718385	0.925888
-45.140874	9.835647	0.930893
-45.980248	8.221381	0.935898
-45.975027	14.696323	0.940902
-46.249037	4.777781	0.945907
-46.227733	-6.413944	0.950912
-46.261362	0.201471	0.955917
-46.793033	2.804337	0.960922
-46.770321	10.862504	0.965926
-47.573850	13.034929	0.970931
-47.843333	12.538040	0.975936
-47.884698	11.405955	0.980941
-48.217468	20.309474	0.985946
-48.006021	3.787484	0.990950
-48.458313	-1.532144	0.995955
-48.411031	4.404046	1.000960
-49.300379	15.661582	1.005965
-49.873459	14.638877	1.010970
-49.999619	20.071941	1.015974
-50.059164	25.741499	1.020979
-49.742998	11.400210	1.025984
-49.674387	-6.362893	1.030989
-50.164351	19.551834	1.035994
-50.514463	11.973304	1.040998
-51.270442	6.912498	1.046003
-51.451836	15.612449	1.051008
-51.011994	12.064224	1.056013
-51.595359	25.996669	1.061018
-52.123824	0.470003	1.066022
-52.764460	10.865802	1.071027
-52.864976	15.744086	1.076032
-52.952552	7.398803	1.081037
-53.150815	6.235830	1.086042
-52.845116	1.681104	1.091046
-53.480189	-4.646949	1.096051
-53.377265	10.169855	1.101056
-53.573717	20.625027	1.106061
-54.199206	22.439540	1.111066
-54.315463	5.213126	1.116070
-54.590821	-7.428976	1.121075
-55.232255	4.188670	1.126080
-55.520623	17.324425	1.131085
-56.070609	19.639416	1.136090
-56.177145	-1.462103	1.141094
-56.378176	-2.254995	1.146099
-56.229943	22.094805	1.151104
-56.240822	2.859230	1.156109
-56.383271	6.812343	1.161114
-56.274352	14.456356	1.166118
-56.967124	8.449060	1.171123
-57.286987	0.695571	1.176128
-57.417822	-0.501037	1.181133
-58.128049	-1.435770	1.186138
-58.745431	0.566603	1.191142
-59.157532	10.348050	1.196147
-59.203344	12.767338	1.201152
-59.257641	-4.828077	1.206157
-59.561915	5.611365	1.211162
-59.181791	11.775068	1.216166
-59.296526	13.949566	1.221171
-59.556048	-0.973272	1.226176
-60.265624	-8.624962	1.231181
-60.912958	-6.224834	1.236186
-60.846677	3.151524	1.241190
-60.775721	-4.448251	1.246195
-60.874496	-3.157590	1.251200
-61.590750	16.869210	1.256205
-62.041195	28.911544	1.261210
-62.274493	2.663630	1.266214
-62.646297	4.695160	1.271219
-62.564626	1.601009	1.276224
-62.368993	5.184259	1.281229
-62.803420	17.213382	1.286234
-62.989884	23.081771	1.291238
-63.793071	16.556781	1.296243
-64.291215	8.334595	1.301248
-63.796811	-5.811419	1.306253
-64.459731	14.480106	1.311258
-64.026585	-5.140166	1.316262
-64.601385	9.603092	1.321267
-65.270580	3.665294	1.326272
-65.514139	7.651987	1.331277
-65.700627	15.476019	1.336282
-65.729515	15.231061	1.341286
-65.914151	12.590003	1.346291
-65.918700	1.317219	1.351296
-66.598665	-1.058197	1.356301
-67.239506	17.708870	1.361306
-67.149841	22.604554	1.366310
-67.341022	22.542673	1.371315
-67.249957	14.468337	1.376320
-67.202149	8.429794	1.381325
-68.201854	3.875669	1.386330
-68.694271	5.825232	1.391334
-68.832304	5.016602	1.396339
-69.107215	-6.989212	1.401344
-69.093561	9.681384	1.406349
-69.198402	17.298974	1.411354
-68.991725	20.091436	1.416358
-69.489995	1.553740	1.421363
-70.092083	1.827493	1.426368
-70.385200	14.857492	1.431373
-70.811035	21.238150	1.436378
-70.512995	5.901771	1.441382
-70.816668	3.016020	1.446387
-71.598203	4.586429	1.451392
-71.766213	10.909182	1.456397
-72.534814	19.693852	1.461402
-72.392566	-11.370115	1.466406
-72.435717	4.573675	1.471411
-72.627788	19.911947	1.476416
-72.240345	7.281134	1.481421
-72.697181	-0.626782	1.486426
-73.316639	5.241348	1.491430
-74.208480	13.134901	1.496435
-74.254211	10.969834	1.501440
-73.995215	15.214486	1.506445
-74.060667	24.422735	1.511450
-73.979147	2.722923	1.516454
-74.290688	0.918934	1.521459
-75.137417	10.349714	1.526464
-75.231467	18.215093	1.531469
-75.692062	12.825022	1.536474
-75.796098	10.930804	1.541478
-75.713676	17.859579	1.546483
-76.691506	10.870724	1.551488
-76.803224	1.153336	1.556493
-77.349556	-1.324659	1.561498
-77.365492	9.442178	1.566502
-77.418649	12.148554	1.571507
-77.424235	8.829214	1.576512
-77.070488	22.029799	1.581517
-78.066208	10.250824	1.586522
-78.522159	9.003977	1.591526
-78.854037	10.902249	1.596531
-79.042694	32.565499	1.601536
-78.944323	9.581885	1.606541
-79.323756	8.230158	1.611546
-79.022362	13.317137	1.616550
-80.095546	13.626925	1.621555
-80.226823	4.192329	1.626560
-80.642254	10.481989	1.631565
-80.768195	28.701027	1.636570
-80.816591	2.178216	1.641574
-80.836625	-2.862262	1.646579
-81.131430	5.093897	1.651584
-81.544900	11.926276	1.656589
-82.164779	3.803822	1.661594
-82.119479	17.514178	1.666598
-82.327833	14.781552	1.671603
-82.153263	5.570641	1.676608
-82.475726	7.894095	1.681613
-83.065670	19.193496	1.686618
-83.346815	16.988519	1.691622
-83.591195	3.432178	1.696627
-84.017808	18.700406	1.701632
-83.606057	5.256982	1.706637
-84.384179	8.447472	1.711642
-84.984709	8.037949	1.716646
-85.280080	-10.577553	1.721651
-85.555711	9.180798	1.726656
-85.440033	6.873541	1.731661
-85.712248	4.865072	1.736666
-85.415868	15.616694	1.741670
-85.438024	6.453488	1.746675
-86.146470	23.420311	1.751680
-86.646540	27.473472	1.756685
-87.080172	20.842129	1.761690
-86.967500	-2.119168	1.766694
-87.020969	9.042237	1.771699
-87.820799	10.368073	1.776704
-88.191847	10.062870	1.781709
-88.339704	5.976699	1.786714
-88.573684	6.666564	1.791718
-88.456021	10.283317	1.796723
-89.129153	1.524034	1.801728
-88.860942	12.510251	1.806733
-88.970197	7.688317	1.811738
-89.632192	-8.371264	1.816742
-89.868426	3.712391	1.821747
-90.428760	26.662825	1.826752
-90.110085	10.959525	1.831757
-90.295478	6.316885	1.836762
-90.798841	5.485379	1.841766
-91.354987	19.861166	1.846771
-91.890788	9.476294	1.851776
-91.670181	8.667577	1.856781
-91.970351	19.677306	1.861786
-92.211080	12.413927	1.866790
-92.178999	8.499154	1.871795
-92.225745	3.412977	1.876800
-92.820162	-7.174480	1.881805
-93.412108	0.192651	1.886810
-93.681978	10.285588	1.891814
-93.749478	13.991638	1.896819
-93.723322	1.186261	1.901824
-93.519050	-3.590717	1.906829
-94.266015	16.592970	1.911834
-94.705550	12.236973	1.916838
-94.977310	14.667069	1.921843
-95.307409	14.877228	1.926848
-95.450182	-10.622790	1.931853
-95.473081	2.081396	1.936858
-95.352839	21.884817	1.941862
-96.239884	9.287084	1.946867
-96.478015	-6.051022	1.951872
-96.707737	1.605249	1.956877
-97.098765	10.864535	1.961882
-96.778614	10.774174	1.966886
-97.028155	2.196034	1.971891
-97.710568	-6.488120	1.976896
-98.006415	3.411223	1.981901
-98.478146	10.522137	1.986906
-98.649310	12.411110	1.991910
-98.414321	1.603705	1.996915
-98.731400	5.991148	2.006912
-98.572515	-2.131632	2.016909
-98.616213	2.468637	2.026906
-97.648068	13.770939	2.036902
-97.231183	6.719952	2.046899
-96.281534	4.849189	2.056896
-95.727612	14.117305	2.066893
-95.932871	5.058100	2.076890
-95.624742	15.202546	2.086886
-94.668658	-0.238118	2.096883
-93.807787	23.166518	2.106880
-93.083472	4.612649	2.116877
-92.864625	3.723958	2.126874
-92.668706	11.058626	2.136870
-92.723370	7.671475	2.146867
-91.752247	8.764952	2.156864
-90.899038	28.786260	2.166861
-90.245761	15.653054	2.176858
-90.228707	0.401763	2.186854
-89.797263	24.992309	2.196851
-89.037139	20.257675	2.206848
-88.287017	10.236466	2.216845
-88.211286	11.828469	2.226842
-87.936040	8.561520	2.236838
-87.040533	14.043470	2.246835
-86.615511	7.164285	2.256832
-85.357880	25.958382	2.266829
-85.637960	5.964781	2.276826
-85.022671	23.582391	2.286822
-84.982910	24.406169	2.296819
-83.986127	10.330312	2.306816
-83.814245	11.927956	2.316813
-82.852764	9.178247	2.326810
-82.339210	11.945276	2.336806
-82.174844	13.432551	2.346803
-81.854031	10.149477	2.356800
-81.088595	17.547958	2.366797
-80.682651	14.676914	2.376794
-79.881657	-4.314335	2.386790
-79.076847	0.630963	2.396787
-78.816947	14.566429	2.406784
-78.865733	1.627691	2.416781
-78.374923	14.910933	2.426778
-77.738432	19.617175	2.436774
-76.861007	1.459166	2.446771
-75.897645	10.936274	2.456768
-75.914919	12.552340	2.466765
-75.883079	1.737299	2.476762
-75.578618	10.148516	2.486758
-74.665668	14.544160	2.496755
-73.596887	2.979531	2.506752
-73.361265	25.917208	2.516749
-72.972928	2.783613	2.526746
-72.591622	17.780666	2.536742
-72.394088	14.399243	2.546739
-71.604508	11.481290	2.556736
-71.077698	8.275981	2.566733
-69.963291	13.245282	2.576730
-69.906375	14.601566	2.586726
-69.744197	16.865944	2.596723
-69.226487	4.451393	2.606720
-68.384402	2.521369	2.616717
-68.046247	22.208614	2.626714
-67.877121	12.670808	2.636710
-67.116503	25.868875	2.646707
-66.486227	18.967812	2.656704
-65.579035	6.601291	2.666701
-65.147979	19.736282	2.676698
-65.179110	14.868208	2.686694
-64.803565	8.268525	2.696691
-63.690037	4.089257	2.706688
-63.227772	26.502043	2.716685
-63.378155	4.530534	2.726682
-62.673034	11.421125	2.736678
-61.826895	23.848665	2.746675
-61.580454	8.053542	2.756672
-60.868115	19.995308	2.766669
-60.128195	24.981567	2.776666
-59.958233	16.744245	2.786662
-59.854369	29.412399	2.796659
-59.145150	6.789157	2.806656
-58.441690	12.709593	2.816653
-58.264872	13.898793	2.826650
-57.346823	6.237835	2.836646
-57.046053	11.665184	2.846643
-56.702428	8.719695	2.856640
-55.869565	22.776691	2.866637
-55.351793	2.022842	2.876634
-55.171098	20.988411	2.886630
-54.165514	20.046936	2.896627
-53.818058	14.820077	2.906624
-53.873461	11.894113	2.916621
-53.021166	5.795625	2.926618
-52.539697	1.395762	2.936614
-52.218855	4.223977	2.946611
-51.007013	23.128177	2.956608
-50.832135	4.581055	2.966605
-50.671867	23.508126	2.976602
-49.902175	12.532905	2.986598
-49.040316	7.951549	2.996595
-49.086421	2.438505	3.006592
-48.862195	23.524918	3.016589
-47.688259	12.020934	3.026586
-47.445244	7.838168	3.036582
-47.008406	20.273892	3.046579
-46.353344	14.277731	3.056576
-45.942043	7.570997	3.066573
-45.801126	1.500395	3.076570
-45.022903	10.227713	3.086566
-44.359423	13.859605	3.096563
-43.913496	6.784261	3.106560
-43.095367	19.933711	3.116557
-42.948132	21.870465	3.126554
-42.640361	16.728984	3.136550
-42.062409	15.105051	3.146547
-41.245103	22.164974	3.156544
-40.976004	9.472176	3.166541
-40.497646	15.908466	3.176538
-39.353854	23.641886	3.186534
-39.216418	13.585825	3.196531
-39.111755	20.908916	3.206528
-39.067915	6.939783	3.216525
-37.968255	21.474501	3.226522
-37.541946	24.974421	3.236518
-36.466652	7.732898	3.246515
-36.304127	24.861364	3.256512
-35.918931	15.878302	3.266509
-35.807189	11.201741	3.276506
-34.936647	19.140427	3.286502
-34.348338	11.450402	3.296499
-33.935842	8.729893	3.306496
-33.161415	5.715678	3.316493
-33.161949	17.436476	3.326490
-32.792716	20.186175	3.336486
-31.811079	9.070244	3.346483
-31.551241	14.586046	3.356480
-30.622936	4.390199	3.366477
-30.065799	5.923090	3.376474
-29.859489	7.214287	3.386470
-29.927912	8.982817	3.396467
-28.969175	16.928164	3.406464
-28.261385	15.520715	3.416461
-28.101838	7.130935	3.426458
-27.071105	10.516345	3.436454
-26.875926	17.492999	3.446451
-26.730844	6.093667	3.456448
-25.869091	21.028815	3.466445
-25.318590	4.196021	3.476442
-24.991329	15.275646	3.486438
-24.118141	10.661799	3.496435
-23.533862	14.569713	3.506432
-23.351076	13.483711	3.516429
-23.430606	2.352726	3.526426
-22.374980	17.922343	3.536422
-21.548163	3.686520	3.546419
-21.321959	14.164437	3.556416
-20.975364	10.024506	3.566413
-20.181281	5.124754	3.576410
-19.861488	7.400420	3.586406
-19.737932	6.891649	3.596403
-18.857105	12.798387	3.606400
-18.267376	5.598728	3.616397
-18.044867	8.896758	3.626394
-17.387541	10.188584	3.636390
-16.710179	21.397529	3.646387
-16.820561	10.342949	3.656384
-15.697501	22.884943	3.666381
-15.363746	11.371161	3.676378
-15.123840	24.752684	3.686374
-14.013054	14.996729	3.696371
-13.810587	18.946311	3.706368
-13.446342	32.834733	3.716365
-12.603835	7.996722	3.726362
-11.935350	25.653568	3.736358
-12.097646	6.314105	3.746355
-11.869547	27.364039	3.756352
-10.912706	13.408368	3.766349
-10.375816	13.435475	3.776346
-9.676341	8.762234	3.786342
-8.918246	0.617363	3.796339
-8.756025	18.887876	3.806336
-8.861340	8.139344	3.816333
-8.033071	18.331188	3.826330
-7.908679	-1.010210	3.836326
-6.472124	18.320499	3.846323
-6.248752	5.630616	3.856320
-5.958177	14.499773	3.866317
-5.331595	-1.483412	3.876314
-4.472149	23.827885	3.886310
-4.237743	12.644811	3.896307
-4.185780	13.867191	3.906304
-3.843344	33.343375	3.916301
-3.223431	16.290094	3.926298
-2.350043	39.353243	3.936294
-2.114005	31.454840	3.946291
-1.488679	68.538699	3.956288
-1.243211	58.181375	3.966285
-0.831979	71.562877	3.976282
-0.249839	102.487618	3.986278
0.000000	100.812819	3.991283
-0.040446	99.547502	3.996288
0.437150	131.578975	4.001293
0.834719	133.546209	4.006298
0.513183	126.563450	4.011302
0.902890	135.334521	4.016307
0.789063	128.409570	4.021312
0.725766	137.824300	4.026317
0.910227	135.142343	4.031322
0.550000	132.511141	4.036326
0.919900	121.492145	4.041331
0.516799	135.614191	4.046336
0.624060	138.487920	4.051341
1.472577	147.400295	4.056346
1.026213	163.541802	4.061350
1.152522	147.770903	4.066355
0.909061	131.670195	4.071360
0.970070	139.178466	4.076365
1.153101	146.326049	4.081370
0.949323	147.994725	4.086374
1.355934	133.709889	4.091379
1.002571	139.511897	4.096384
0.665411	150.771791	4.101389
1.113749	162.651298	4.106394
1.303746	153.497719	4.111398
1.334499	148.426894	4.116403
1.136231	154.516577	4.121408
1.380444	161.224747	4.126413
1.565947	147.389273	4.131418
1.219685	139.876819	4.136422
1.063507	118.267405	4.141427
1.136195	137.450185	4.146432
1.041172	133.320519	4.151437
1.083915	129.237238	4.156442
0.816215	160.397587	4.161446
1.477566	144.510058	4.166451
1.786237	157.627964	4.171456
1.437205	140.584470	4.176461
1.430520	140.520604	4.181466
1.215360	139.003705	4.186470
1.490907	132.394192	4.191475
1.181861	127.873647	4.196480
0.946521	133.947352	4.201485
1.145761	142.393397	4.206490
1.464709	174.736267	4.211494
1.777496	170.126854	4.216499
1.460078	141.576366	4.221504
1.485582	137.755371	4.226509
1.299820	147.560860	4.231514
1.139519	155.503652	4.236518
1.624575	143.356332	4.241523
1.457945	165.995999	4.246528
1.353466	156.080409	4.251533
1.341187	155.554027	4.256538
1.480476	165.130121	4.261542
1.895645	155.119183	4.266547
1.718071	170.077207	4.271552
1.316626	174.346417	4.276557
1.627401	149.160014	4.281562
1.528629	176.568683	4.286566
1.629332	171.182065	4.291571
1.670876	159.018949	4.296576
1.371966	164.041738	4.301581
1.412904	173.546886	4.306586
1.296972	160.872467	4.311590
1.472934	170.750379	4.316595
1.428997	184.031342	4.321600
1.363605	185.127494	4.326605
1.471845	170.555154	4.331610
1.390030	180.252829	4.336614
1.764600	183.869097	4.341619
1.512043	186.976409	4.346624
1.310885	173.501146	4.351629
1.845492	185.881743	4.356634
1.704377	200.507844	4.361638
1.717221	186.178535	4.366643
1.931452	184.363883	4.371648
1.868358	189.320087	4.376653
1.684649	188.992200	4.381658
1.652835	191.247128	4.386662
2.166654	177.981605	4.391667
1.835170	167.230895	4.396672
1.454009	173.008705	4.401677
2.007918	204.669437	4.406682
2.137093	205.307185	4.411686
2.239770	169.475465	4.416691
1.867376	181.761701	4.421696
1.591186	184.601543	4.426701
1.795147	188.450993	4.431706
1.756273	191.187990	4.436710
2.106515	188.249077	4.441715
2.043368	199.031750	4.446720
2.107929	191.900219	4.451725
2.058888	183.864135	4.456730
1.955811	189.700955	4.461734
2.126790	207.129131	4.466739
2.065839	193.196339	4.471744
1.837490	168.880970	4.476749
2.288761	179.194488	4.481754
1.887558	205.759847	4.486758
2.249815	197.705995	4.491763
2.218667	190.013890	4.496768
1.991165	183.571339	4.501773
2.035443	194.082241	4.506778
2.313772	201.457560	4.511782
2.254147	189.984502	4.516787
1.832876	192.045733	4.521792
2.174142	180.041706	4.526797
2.450044	196.521407	4.531802
1.955607	189.726014	4.536806
2.728713	190.317223	4.541811
2.134930	206.028278	4.546816
1.950016	183.262351	4.551821
2.257230	171.135719	4.556826
2.275482	193.305404	4.561830
2.164248	200.328517	4.566835
2.409920	205.147877	4.571840
2.227739	198.673661	4.576845
2.334252	190.551002	4.581850
2.159230	208.665528	4.586854
2.417960	186.675529	4.591859
2.337274	203.281641	4.596864
2.130890	210.173106	4.601869
2.287869	200.927986	4.606874
2.252335	202.434211	4.611878
2.590750	203.690420	4.616883
2.614647	196.876936	4.621888
2.197512	208.313448	4.626893
2.330825	218.325693	4.631898
2.207729	217.143767	4.636902
2.375643	189.095296	4.641907
2.409711	206.775747	4.646912
2.298426	203.341742	4.651917
2.459364	188.416695	4.656922
2.128610	210.399339	4.661926
2.335520	220.954014	4.666931
2.045972	214.343350	4.671936
2.113516	206.522372	4.676941
2.520021	227.201217	4.681946
2.481420	233.992780	4.686950
2.947518	228.548222	4.691955
2.700409	217.652012	4.696960
2.449747	227.461964	4.701965
2.537374	229.119312	4.706970
2.302576	256.395629	4.711974
2.556798	232.937555	4.716979
3.058716	227.172271	4.721984
2.765626	226.244734	4.726989
2.963835	245.195728	4.731994
2.662550	225.080055	4.736998
2.557775	212.420717	4.742003
2.619281	228.114847	4.747008
2.903454	228.234167	4.752013
2.771484	218.468065	4.757018
2.608548	225.931905	4.762022
2.940942	235.672265	4.767027
2.634358	236.036567	4.772032
2.648800	230.459293	4.777037
2.650075	230.466222	4.782042
2.514395	251.543861	4.787046
3.035519	234.236111	4.792051
2.926220	245.031278	4.797056
2.715305	247.293814	4.802061
2.620574	241.123264	4.807066
2.673751	249.325878	4.812070
2.901719	236.595846	4.817075
2.903357	243.395042	4.822080
2.706967	235.144161	4.827085
3.027530	237.590538	4.832090
2.741718	231.701245	4.837094
2.769342	226.903249	4.842099
3.061970	221.554145	4.847104
2.578557	221.994921	4.852109
3.110081	234.582165	4.857114
3.126264	251.906649	4.862118
2.819802	243.146391	4.867123
3.090853	227.710836	4.872128
3.176195	244.323318	4.877133
3.167857	253.788421	4.882138
2.864459	249.324023	4.887142
3.126951	224.828777	4.892147
3.028063	238.046289	4.897152
2.918574	248.809627	4.902157
3.075159	246.227452	4.907162
2.761829	243.724416	4.912166
3.430886	239.794871	4.917171
3.026045	255.907713	4.922176
3.177157	269.598553	4.927181
3.745173	263.612634	4.932186
3.104168	246.472558	4.937190
3.259047	239.771864	4.942195
2.880546	243.429242	4.947200
2.544028	236.792593	4.952205
3.033859	254.448287	4.957210
2.963232	280.713810	4.962214
3.683509	249.940856	4.967219
3.703071	257.356697	4.972224
3.283508	275.341944	4.977229
3.376846	273.135112	4.982234
2.937000	264.709399	4.987238
3.319815	261.904477	4.992243
3.576072	275.909696	4.997248
3.590604	265.726368	5.002253
3.593104	249.512184	5.007258
3.404113	275.699895	5.012262
3.277734	283.640995	5.017267
3.098113	284.140375	5.022272
3.345850	273.063725	5.027277
3.773939	278.281682	5.032282
3.397007	285.945756	5.037286
3.825310	272.005431	5.042291
3.477681	274.538268	5.047296
3.441327	266.113939	5.052301
3.507585	260.562223	5.057306
3.340416	265.819064	5.062310
3.417037	262.762391	5.067315
3.374351	279.893718	5.072320
3.703940	291.972094	5.077325
3.498096	260.053086	5.082330
3.096386	268.547217	5.087334
3.390004	271.915173	5.092339
3.572989	260.300065	5.097344
3.250391	269.602655	5.102349
3.674671	272.929881	5.107354
3.385818	273.562138	5.112358
3.292180	255.839048	5.117363
3.158110	273.198942	5.122368
3.523538	297.058146	5.127373
4.066784	287.739866	5.132378
3.516119	274.186732	5.137382
3.711259	284.061252	5.142387
3.683855	287.296215	5.147392
3.701073	298.904277	5.152397
3.665199	304.756570	5.157402
3.879270	305.103291	5.162406
4.029115	310.819836	5.167411
3.795728	281.364809	5.172416
3.496321	271.170816	5.177421
3.979751	298.210927	5.182426
3.895061	307.472940	5.187430
3.840000	286.529512	5.192435
4.091914	279.979676	5.197440
3.961041	276.531727	5.202445
3.792480	285.810942	5.207450
3.491071	285.035903	5.212454
3.744173	283.709629	5.217459
3.861389	297.361014	5.222464
3.994180	295.715571	5.227469
4.152078	293.699899	5.232474
3.977462	307.046266	5.237478
3.774554	301.963299	5.242483
3.904738	310.652671	5.247488
3.679239	294.146637	5.252493
4.161114	303.750644	5.257498
3.681356	290.028238	5.262502
3.779551	289.722025	5.267507
3.996141	303.810277	5.272512
3.755197	319.006992	5.277517
3.947437	296.881923	5.282522
3.794284	284.413610	5.287526
4.100695	293.300341	5.292531
3.908512	308.042214	5.297536
3.894521	312.025277	5.302541
4.126674	295.192060	5.307546
3.949340	300.844097	5.312550
4.057869	304.673145	5.317555
4.031107	317.469789	5.322560
4.249389	337.295813	5.327565
4.303586	342.038939	5.332570
4.406999	340.849264	5.337574
4.460126	323.268260	5.342579
4.366307	316.673049	5.347584
3.627566	318.319568	5.352589
4.345729	329.063378	5.357594
4.420143	337.971015	5.362598
4.179950	304.780401	5.367603
4.004902	315.908468	5.372608
4.086187	347.926381	5.377613
4.535628	332.609236	5.382618
4.452440	341.511353	5.387622
4.374692	334.509418	5.392627
4.334127	345.873344	5.397632
4.269931	333.660780	5.402637
4.606745	325.217069	5.407642
4.169301	326.554156	5.412646
4.145171	335.683757	5.417651
4.341375	353.844829	5.422656
4.133228	340.418319	5.427661
4.272387	324.653795	5.432666
4.248743	320.276811	5.437670
4.505221	329.798227	5.442675
4.612718	351.153362	5.447680
4.530151	332.936003	5.452685
4.429057	321.081916	5.457690
4.476775	346.814239	5.462694
4.512995	346.550525	5.467699
4.561024	351.060090	5.472704
4.544062	336.878802	5.477709
4.484793	326.460222	5.482714
4.336720	330.556401	5.487718
4.368518	337.949346	5.492723
4.637188	339.214035	5.497728
4.337258	352.477669	5.502733
4.601528	335.188873	5.507738
4.255234	343.039486	5.512742
4.270571	339.618064	5.517747
4.728325	341.715361	5.522752
4.733079	378.272820	5.527757
5.083702	354.014774	5.532762
4.356231	357.097025	5.537766
4.590982	360.272108	5.542771
4.978969	352.828201	5.547776
4.968708	373.507659	5.552781
4.805785	364.028243	5.557786
4.741217	366.107493	5.562790
4.719743	359.080759	5.567795
4.768468	350.723510	5.572800
4.410842	358.503596	5.577805
4.802060	360.849731	5.582810
4.643231	372.304642	5.587814
4.781329	377.941472	5.592819
4.776675	363.946937	5.597824
4.905218	354.691528	5.602829
5.273884	365.031351	5.607834
4.523492	377.300209	5.612838
5.085480	385.881961	5.617843
5.302824	380.314013	5.622848
4.967586	376.198330	5.627853
4.812137	364.654067	5.632858
4.605616	364.085596	5.637862
4.853785	366.404667	5.642867
5.268456	374.719550	5.647872
4.652368	375.366628	5.652877
5.096243	356.353162	5.657882
4.972870	357.183584	5.662886
4.937350	373.993129	5.667891
4.911204	362.232571	5.672896
4.778074	364.438273	5.677901
5.074402	364.023455	5.682906
4.895289	373.327945	5.687910
4.744143	383.675754	5.692915
5.087243	369.540386	5.697920
4.573261	377.020586	5.702925
4.525249	377.320654	5.707930
4.559144	386.645095	5.712934
4.819840	392.650540	5.717939
5.042101	384.739780	5.722944
4.936723	382.249410	5.727949
5.282904	389.304839	5.732954
4.776150	411.054651	5.737958
4.707329	412.873785	5.742963
5.121821	400.709020	5.747968
4.940851	408.356949	5.752973
5.350523	413.391453	5.757978
5.337108	427.676259	5.762982
5.308779	412.199558	5.767987
5.448374	431.851277	5.772992
5.480268	438.461877	5.777997
5.688398	405.672635	5.783002
5.153911	401.120902	5.788006
5.227951	384.098172	5.793011
5.213682	397.121484	5.798016
5.246906	432.045790	5.803021
5.423214	434.381284	5.808026
5.541099	435.528748	5.813030
5.382260	416.029731	5.818035
5.622524	412.449588	5.823040
5.059397	410.428169	5.828045
5.395942	413.247486	5.833050
5.382607	422.941101	5.838054
5.266343	417.789422	5.843059
5.432046	420.550558	5.848064
5.405949	425.635280	5.853069
5.384737	408.634183	5.858074
5.176855	429.602366	5.863078
5.497029	434.561010	5.868083
5.722508	425.288355	5.873088
4.995936	439.455358	5.878093
5.460095	430.574051	5.883098
5.305977	427.226880	5.888102
5.380623	430.356127	5.893107
5.253642	413.347349	5.898112
5.242307	426.396047	5.903117
5.707924	443.080925	5.908122
5.556241	475.311719	5.913126
5.739673	451.210970	5.918131
6.223615	451.945866	5.923136
5.634585	450.219340	5.928141
6.100313	429.704791	5.933146
5.584898	428.817533	5.938150
5.628561	435.154807	5.943155
5.576435	422.850999	5.948160
5.297204	424.543025	5.953165
6.145453	439.644401	5.958170
5.787890	455.944963	5.963174
5.559136	459.053230	5.968179
5.753259	454.829328	5.973184
5.790676	452.751372	5.978189
6.205069	441.060300	5.983194
5.792114	458.600851	5.988198
5.677150	463.292066	5.993203
5.509190	453.461055	5.998208
5.859841	443.530632	6.003213
5.956133	445.788794	6.008218
5.491973	471.637290	6.013222
5.663822	471.152679	6.018227
5.722019	458.341315	6.023232
5.633298	460.940599	6.028237
5.857618	446.082462	6.033242
5.736043	465.895665	6.038246
5.898265	461.800343	6.043251
5.822395	445.568027	6.048256
5.667054	471.209031	6.053261
6.146466	457.417534	6.058266
5.858544	460.144538	6.063270
5.703532	473.155266	6.068275
5.922279	474.082751	6.073280
5.742984	447.906610	6.078285
5.835236	456.924123	6.083290
6.023656	471.557778	6.088294
5.981547	464.509843	6.093299
6.095277	468.759794	6.098304
5.806062	464.507450	6.103309
5.808911	444.890821	6.108314
5.857971	470.187105	6.113318
5.771372	482.340429	6.118323
6.032450	458.717218	6.123328
5.550156	456.811762	6.128333
5.733341	470.757519	6.133338
5.912478	476.469483	6.138342
5.773370	464.107806	6.143347
6.341441	450.388474	6.148352
5.937040	448.903212	6.153357
5.898064	459.454395	6.158362
5.893848	479.594081	6.163366
5.801733	464.348644	6.168371
5.745483	449.993711	6.173376
5.715912	461.939804	6.178381
6.083455	459.298069	6.183386
6.056510	468.861182	6.188390
5.552556	439.433695	6.193395
5.791088	438.477872	6.198400
6.037526	462.577478	6.203405
5.976867	457.138014	6.208410
5.610256	433.193893	6.213414
5.601160	432.632646	6.218419
5.906406	448.079167	6.223424
5.454375	465.765969	6.228429
5.964906	470.588797	6.233434
5.859626	463.479683	6.238438
6.078407	470.102916	6.243443
6.077627	455.665022	6.248448
5.615048	447.510497	6.253453
6.017015	453.689029	6.258458
5.834209	458.050525	6.263462
5.501670	427.498160	6.268467
5.679918	442.538516	6.273472
5.645134	465.894036	6.278477
5.933824	438.425226	6.283482
5.493603	449.711841	6.288486
5.966047	469.142478	6.293491
6.073542	472.304975	6.298496
5.678011	456.423688	6.303501
6.027022	446.423988	6.308506
6.186340	450.240437	6.313510
6.023261	478.347062	6.318515
6.015161	448.822816	6.323520
5.606746	430.114752	6.328525
5.563989	445.437465	6.333530
5.964792	469.021882	6.338534
5.997435	458.534258	6.343539
5.816462	460.119689	6.348544
6.087569	450.353438	6.353549
5.791888	423.653218	6.358554
5.502197	434.808111	6.363558
5.659789	439.963497	6.368563
6.107992	463.879422	6.373568
5.772473	464.977323	6.378573
6.141060	444.471706	6.383578
5.964550	445.999181	6.388582
5.695370	450.977394	6.393587
5.705825	430.691283	6.398592
5.876227	443.254010	6.403597
5.982593	435.995402	6.408602
5.723788	438.662348	6.413606
5.370551	452.559814	6.418611
5.943453	456.420079	6.423616
5.958572	462.907488	6.428621
6.033156	461.023250	6.433626
5.624565	443.221185	6.438630
5.676529	439.853962	6.443635
5.881451	468.752666	6.448640
6.083605	476.623591	6.453645
6.024883	442.389669	6.458650
5.853421	423.180386	6.463654
5.713075	439.829169	6.468659
6.114079	453.851275	6.473664
5.679093	439.326526	6.478669
5.720914	424.829830	6.483674
5.397415	431.341323	6.488678
5.462648	446.179586	6.493683
6.080019	450.025595	6.498688
5.830020	464.252068	6.503693
6.141293	463.543963	6.508698
6.156661	470.930612	6.513702
5.924335	436.988980	6.518707
5.881280	427.542294	6.523712
5.674423	446.957809	6.528717
5.603932	439.493447	6.533722
5.895052	446.973016	6.538726
5.758979	439.270306	6.543731
6.133715	443.288501	6.548736
5.859524	439.577923	6.553741
5.899130	423.009886	6.558746
5.642703	437.717221	6.563750
5.655834	447.216284	6.568755
5.984324	436.384136	6.573760
5.821802	432.042500	6.578765
5.975224	432.341735	6.583770
5.843539	447.999458	6.588774
5.739119	433.202370	6.593779
5.669568	420.482880	6.598784
5.783435	436.976894	6.603789
6.187465	452.160276	6.608794
6.071836	431.039919	6.613798
5.914315	437.955866	6.618803
6.028159	427.029277	6.623808
5.561579	429.088655	6.628813
5.918335	445.983791	6.633818
5.693160	437.920945	6.638822
5.831974	427.471237	6.643827
5.717052	436.247945	6.648832
5.757856	437.978038	6.653837
5.961055	425.430495	6.658842
5.777681	437.357891	6.663846
5.682833	453.071581	6.668851
6.033372	439.160233	6.673856
6.012106	441.395501	6.678861
5.974765	437.658605	6.683866
6.128505	432.686133	6.688870
5.931526	416.701146	6.693875
6.072915	437.467693	6.698880
5.774150	453.112981	6.703885
5.859608	431.560064	6.708890
5.993956	439.051233	6.713894
5.876290	436.341419	6.718899
6.165373	430.305449	6.723904
5.857793	446.535592	6.728909
5.963135	438.274788	6.733914
5.809201	432.094314	6.738918
5.988145	420.860139	6.743923
6.003241	429.616836	6.748928
5.599306	443.388807	6.753933
5.837292	432.725115	6.758938
6.003688	446.887987	6.763942
5.696954	447.470922	6.768947
6.166482	432.372711	6.773952
5.803397	443.950706	6.778957
6.023850	428.565064	6.783962
5.729113	430.763646	6.788966
5.458080	438.231742	6.793971
5.710687	427.762144	6.798976
5.483288	435.202805	6.803981
5.891025	434.552647	6.808986
5.794403	433.160549	6.813990
5.391993	445.899524	6.818995
5.757399	416.165050	6.824000
5.803472	434.814477	6.829005
5.701367	437.898160	6.834010
5.650529	438.009193	6.839014
5.748238	430.459823	6.844019
5.840877	436.656913	6.849024
5.587697	445.806775	6.854029
5.776496	444.859959	6.859034
5.716373	441.482158	6.864038
5.759123	411.531114	6.869043
5.729656	421.084256	6.874048
5.649486	449.036356	6.879053
5.816294	460.021419	6.884058
5.735238	455.476219	6.889062
6.190761	447.869582	6.894067
6.129242	444.372154	6.899072
5.876862	454.224559	6.904077
5.849798	441.938494	6.909082
5.901590	420.955126	6.914086
5.759429	437.800516	6.919091
5.918033	441.741575	6.924096
5.850173	448.169790	6.929101
6.013251	416.918397	6.934106
6.009662	420.783168	6.939110
6.171226	435.882209	6.944115
5.875319	434.426172	6.949120
5.581904	435.260925	6.954125
5.977967	436.016458	6.959130
5.965920	442.162093	6.964134
5.718857	436.935447	6.969139
6.089810	432.319599	6.974144
5.848863	451.027330	6.979149
5.936070	431.934606	6.984154
5.972623	432.763166	6.989158
5.443689	441.823546	6.994163
5.449975	422.426265	6.999168
5.291536	437.757533	7.004173
5.392604	439.164656	7.009178
6.023791	442.189502	7.014182
5.950093	445.969683	7.019187
5.911997	437.629990	7.024192
5.482893	444.203430	7.029197
5.828766	456.835424	7.034202
6.084742	459.778945	7.039206
5.589869	433.513421	7.044211
5.971145	426.026493	7.049216
5.509948	441.000185	7.054221
5.588932	454.477996	7.059226
5.699680	465.161684	7.064230
5.612898	448.861719	7.069235
5.831708	448.736023	7.074240
5.674756	453.512402	7.079245
5.839055	445.632005	7.084250
5.805200	467.579763	7.089254
5.900843	474.333143	7.094259
5.866482	458.419295	7.099264
5.754013	450.389902	7.104269
5.957453	470.360112	7.109274
5.805132	485.039830	7.114278
5.476253	463.946876	7.119283
5.789000	477.284961	7.124288
5.748805	477.233439	7.129293
5.720824	466.976308	7.134298
5.761870	468.021153	7.139302
5.544807	457.246002	7.144307
5.957699	453.574580	7.149312
5.628637	475.216791	7.154317
5.753266	487.216932	7.159322
5.803762	459.258199	7.164326
5.883375	470.505879	7.169331
5.879070	460.769451	7.174336
5.670519	455.295633	7.179341
5.863564	457.814022	7.184346
6.038111	482.292314	7.189350
5.737681	459.277137	7.194355
5.834451	468.472958	7.199360
5.815832	471.486226	7.204365
5.393889	455.718706	7.209370
5.822307	470.661814	7.214374
5.955448	483.492742	7.219379
6.069755	465.798475	7.224384
6.004644	458.803865	7.229389
6.042784	451.480763	7.234394
5.971566	475.128496	7.239398
5.819660	477.686730	7.244403
5.604093	466.881435	7.249408
5.754587	456.930614	7.254413
5.515967	465.728965	7.259418
5.954539	466.884202	7.264422
5.822524	474.104917	7.269427
5.965920	477.782049	7.274432
5.680153	482.033015	7.279437
5.948719	467.815468	7.284442
5.989836	473.541460	7.289446
5.657156	473.210070	7.294451
5.879310	469.615052	7.299456
5.773953	469.326690	7.304461
6.026064	460.885262	7.309466
6.067987	471.775554	7.314470
5.590913	474.409424	7.319475
6.032775	462.281618	7.324480
5.517440	479.788900	7.329485
5.887268	479.750805	7.334490
5.898961	465.569102	7.339494
6.012665	469.220952	7.344499
6.071519	470.100578	7.349504
5.738039	472.896670	7.354509
5.902799	478.364783	7.359514
5.792609	486.036764	7.364518
5.508367	474.889553	7.369523
5.757734	463.901772	7.374528
5.727071	478.778308	7.379533
6.184780	458.601437	7.384538
5.907226	469.564253	7.389542
5.907970	481.229630	7.394547
6.193526	470.322971	7.399552
5.743019	463.991239	7.404557
5.847301	464.039940	7.409562
5.990744	481.692670	7.414566
5.940748	471.590205	7.419571
6.132523	481.459983	7.424576
5.831014	472.530086	7.429581
5.857949	457.282738	7.434586
6.058196	455.592984	7.439590
5.846826	473.543465	7.444595
6.053752	473.228356	7.449600
5.788107	472.530261	7.454605
5.871866	458.661799	7.459610
6.170835	474.361529	7.464614
5.628464	477.600941	7.469619
5.912724	468.018753	7.474624
5.912394	461.838432	7.479629
5.692801	466.388608	7.484634
5.965296	466.332170	7.489638
5.865107	468.427975	7.494643
5.853149	451.771555	7.499648
5.803078	454.233051	7.504653
5.783665	473.134838	7.509658
6.212181	482.505101	7.514662
5.663766	438.396917	7.519667
5.587594	433.794489	7.524672
5.813716	456.111320	7.529677
5.923749	465.642916	7.534682
5.790193	471.367093	7.539686
5.678982	476.117374	7.544691
5.871783	461.764480	7.549696
5.590319	462.370170	7.554701
5.756524	467.244376	7.559706
5.615407	463.991230	7.564710
5.630557	460.535779	7.569715
6.023888	476.605138	7.574720
5.909336	479.393462	7.579725
5.942943	456.591508	7.584730
5.746510	457.976081	7.589734
5.717587	476.282325	7.594739
5.819550	477.291850	7.599744
5.742064	474.040813	7.604749
5.878686	452.545802	7.609754
5.923473	459.414711	7.614758
5.563152	488.194967	7.619763
5.688433	466.644101	7.624768
5.549856	461.777044	7.629773
5.610435	454.935089	7.634778
5.826361	475.779829	7.639782
5.702178	472.729565	7.644787
5.962820	459.982505	7.649792
5.803887	457.225250	7.654797
5.628677	451.675785	7.659802
5.928580	468.832487	7.664806
6.072540	475.487126	7.669811
5.746419	445.744159	7.674816
5.839130	462.048148	7.679821
5.838824	465.089463	7.684826
5.858694	468.529042	7.689830
5.649380	476.022076	7.694835
6.056452	455.628757	7.699840
5.671130	471.207970	7.704845
5.916236	491.259907	7.709850
5.929631	467.475682	7.714854
5.655295	462.389767	7.719859
5.863263	457.940039	7.724864
5.909322	465.115241	7.729869
5.999297	481.734096	7.734874
6.076444	475.967817	7.739878
5.644984	484.515223	7.744883
6.188401	473.031668	7.749888
5.773592	482.528080	7.754893
5.937444	465.427084	7.759898
5.884996	465.104824	7.764902
5.567605	461.403156	7.769907
6.012891	456.855908	7.774912
5.725314	476.300682	7.779917
5.747604	470.964798	7.784922
6.009577	468.013784	7.789926
5.992170	479.087507	7.794931
6.193236	464.345063	7.799936
5.918060	463.083683	7.804941
5.941579	462.270918	7.809946
6.124945	473.388798	7.814950
5.947472	471.586265	7.819955
6.163259	450.820895	7.824960
5.677954	456.350757	7.829965
5.653387	452.093548	7.834970
5.856178	437.610388	7.839974
5.706875	447.718417	7.844979
6.027407	460.116860	7.849984
5.795783	467.254595	7.854989
5.635543	435.829901	7.859994
5.707642	449.523702	7.864998
5.618816	472.395119	7.870003
5.994254	466.730184	7.875008
5.860011	456.892710	7.880013
5.979071	468.072609	7.885018
5.898220	473.432746	7.890022
5.623670	471.223844	7.895027
6.328739	472.128964	7.900032
5.925292	465.367141	7.905037
5.912567	451.788379	7.910042
5.672104	441.670453	7.915046
5.746575	422.398531	7.920051
5.773741	421.169068	7.925056
5.813508	452.244969	7.930061
5.936235	481.810825	7.935066
5.920872	456.586269	7.940070
5.673660	434.345602	7.945075
5.963101	437.983101	7.950080
5.627827	454.992218	7.955085
6.032705	448.777492	7.960090
6.187367	460.606426	7.965094
5.790914	454.101911	7.970099
5.720451	430.633661	7.975104
5.577360	443.142150	7.980109
5.680322	433.698655	7.985114
5.868073	434.660064	7.990118
5.849822	455.390257	7.995136
6.036489	452.492269	8.000154
5.708216	459.191768	8.005171
5.923204	439.812308	8.010189
5.937709	431.234896	8.015206
5.901165	441.093703	8.020224
6.089592	438.712599	8.025242
5.691436	440.161201	8.030259
5.772226	419.357615	8.035277
5.778782	442.566804	8.040294
5.656225	476.391044	8.045312
5.844758	463.340966	8.050330
5.978425	455.404187	8.055347
5.960037	455.268033	8.060365
6.268874	466.604273	8.065382
5.972615	467.787095	8.070400
5.807329	438.658469	8.075418
5.800967	426.669364	8.080435
5.574615	441.027128	8.085453
5.995744	473.284779	8.090470
5.878448	462.836078	8.095488
6.041553	449.782341	8.100506
6.050065	462.385768	8.105523
6.101300	470.441730	8.110541
5.971113	466.786494	8.115558
6.022509	456.448167	8.120576
5.828554	434.774679	8.125594
5.600723	456.786371	8.130611
5.590698	475.185480	8.135629
5.947026	463.284889	8.140646
6.099246	467.998355	8.145664
6.209306	463.668956	8.150682
5.928888	457.088424	8.155699
6.145565	468.587097	8.160717
6.170523	464.551306	8.165734
6.112485	467.489809	8.170752
6.243331	464.145959	8.175770
6.038849	474.663657	8.180787
6.215447	455.495482	8.185805
5.992600	443.844119	8.190822
5.625346	443.371343	8.195840
5.931683	465.182305	8.200858
5.971427	469.630583	8.205875
6.076871	465.926667	8.210893
5.822131	474.892887	8.215910
5.910819	468.872332	8.220928
5.886187	451.447453	8.225946
6.030869	467.581775	8.230963
5.959071	472.263190	8.235981
6.017480	462.444414	8.240998
5.885405	471.520736	8.246016
6.142602	463.339884	8.251034
6.160815	474.619759	8.256051
6.080804	469.135598	8.261069
6.144613	456.230018	8.266086
6.090118	450.616585	8.271104
5.944279	470.039021	8.276122
6.118658	463.469226	8.281139
6.235895	463.867484	8.286157
6.230411	476.660879	8.291174
6.066901	480.187318	8.296192
6.448132	466.221691	8.301210
6.364281	465.601419	8.306227
5.970441	485.984770	8.311245
6.193555	462.891429	8.316262
6.243479	457.648321	8.321280
6.380762	474.167226	8.326298
6.018612	466.914765	8.331315
6.282549	475.589522	8.336333
6.342652	459.381277	8.341350
6.056777	460.115268	8.346368
6.239103	468.570013	8.351386
6.169292	474.062577	8.356403
6.057282	473.754251	8.361421
6.056033	470.578152	8.366438
6.322604	474.304893	8.371456
6.345214	460.453639	8.376474
6.172369	455.514985	8.381491
5.951887	466.073794	8.386509
6.493379	465.310820	8.391526
5.870112	477.935424	8.396544
6.121751	461.616610	8.401562
6.190514	454.579178	8.406579
5.888743	462.838312	8.411597
6.142650	480.978223	8.416614
6.196619	480.432587	8.421632
6.322175	508.668192	8.426650
6.442243	505.415065	8.431667
6.264830	488.292970	8.436685
6.399316	473.383949	8.441702
6.299915	477.217024	8.446720
6.214343	469.014097	8.451738
6.222096	476.079997	8.456755
6.208825	509.905734	8.461773
6.529988	503.841138	8.466790
6.371331	499.060414	8.471808
6.520359	496.827306	8.476826
6.224503	484.341569	8.481843
6.223009	466.569345	8.486861
6.429205	484.712816	8.491878
6.303374	504.072852	8.496896
6.343344	510.090142	8.501914
6.619767	502.712749	8.506931
6.299913	491.241409	8.511949
6.594685	470.392355	8.516966
6.158883	463.917297	8.521984
6.285556	478.360710	8.527002
6.106764	513.640758	8.532019
6.005121	508.134279	8.537037
6.507049	484.841329	8.542054
6.058945	501.146464	8.547072
6.481248	510.929093	8.552090
6.511568	510.869805	8.557107
6.549437	505.103725	8.562125
6.685551	499.512006	8.567143
6.609953	522.050542	8.572160
6.488298	516.294881	8.577178
6.437768	506.265996	8.582195
6.452150	498.511559	8.587213
6.713790	502.706507	8.592231
6.572217	513.436999	8.597248
6.352866	500.945296	8.602266
6.572985	506.909591	8.607283
6.606714	513.786131	8.612301
6.384743	512.587970	8.617319
6.654587	519.637637	8.622336
6.328678	507.148975	8.627354
6.883949	494.746622	8.632371
6.582975	498.293815	8.637389
6.414441	495.739772	8.642407
6.367913	501.300130	8.647424
6.384604	501.193010	8.652442
6.830818	494.171900	8.657459
6.335975	506.141628	8.662477
6.738116	513.993208	8.667495
6.470172	491.378302	8.672512
6.528854	501.205667	8.677530
6.661827	500.054725	8.682547
6.198352	513.854868	8.687565
6.863427	494.935646	8.692583
6.397074	500.994985	8.697600
6.265404	508.823000	8.702618
6.840793	519.434520	8.707635
6.728070	513.201339	8.712653
6.665281	502.639892	8.717671
6.508754	511.507348	8.722688
6.373625	508.971299	8.727706
6.911217	497.243129	8.732723
6.560951	502.871887	8.737741
6.693700	517.344540	8.742759
6.701424	512.991007	8.747776
6.440295	507.116018	8.752794
6.441857	486.943563	8.757811
6.460633	498.642238	8.762829
6.799905	503.034336	8.767847
6.398506	495.701463	8.772864
6.398570	498.177646	8.777882
6.838534	512.091009	8.782899
6.507159	517.437105	8.787917
6.846778	495.510144	8.792935
6.584338	504.997583	8.797952
6.574408	497.140896	8.802970
6.707145	499.529621	8.807987
6.197833	520.366916	8.813005
6.611767	503.025263	8.818023
6.560907	495.406573	8.823040
6.539809	524.850649	8.828058
6.816524	517.031989	8.833075
6.592270	525.661111	8.838093
6.589685	541.067406	8.843111
6.690822	543.570680	8.848128
6.657033	540.338053	8.853146
7.014762	534.280095	8.858163
7.040159	540.405385	8.863181
7.082535	520.806290	8.868199
6.763355	531.557782	8.873216
6.960712	535.072123	8.878234
6.624192	505.225425	8.883251
6.724469	520.177819	8.888269
7.163888	515.810801	8.893287
6.966179	516.381841	8.898304
6.723103	513.087180	8.903322
6.829213	498.822010	8.908339
6.653542	512.494692	8.913357
6.993173	512.203926	8.918375
7.014191	515.092080	8.923392
6.491463	513.266848	8.928410
6.863630	511.762292	8.933427
6.909511	518.694881	8.938445
7.152789	532.560967	8.943463
6.846525	511.960156	8.948480
6.892997	525.323480	8.953498
6.941147	515.762493	8.958515
6.788771	517.068053	8.963533
6.958150	520.302155	8.968551
6.986871	504.834271	8.973568
6.957679	509.603707	8.978586
6.953134	513.011981	8.983603
6.511182	502.797561	8.988621
7.104045	520.052509	8.993639
7.498577	532.430436	8.998656
7.126521	522.351458	9.003674
7.071213	505.549322	9.008691
6.844833	490.969823	9.013709
6.943333	507.657922	9.018727
6.775519	525.985164	9.023744
6.558911	516.979792	9.028762
7.095506	507.717508	9.033779
7.067552	524.941336	9.038797
6.903757	534.313012	9.043815
7.157566	522.350699	9.048832
6.983198	522.584710	9.053850
6.966041	518.990485	9.058867
7.518576	514.876546	9.063885
7.226719	505.244921	9.068903
7.144252	511.442636	9.073920
6.630160	504.491171	9.078938
7.053573	506.861675	9.083955
6.701924	483.378388	9.088973
6.777582	517.481487	9.093991
7.037868	536.147621	9.099008
7.157478	523.397971	9.104026
7.425080	516.968904	9.109043
7.013324	518.957697	9.114061
6.977575	510.416195	9.119079
6.895510	542.117274	9.124096
6.884754	527.550320	9.129114
7.248639	515.668415	9.134131
7.404497	533.340971	9.139149
7.315809	548.963119	9.144167
7.133626	525.055812	9.149184
7.123873	531.577839	9.154202
7.366741	532.373623	9.159219
6.820456	496.180856	9.164237
7.156038	520.813808	9.169255
7.017211	549.036306	9.174272
7.086307	539.583326	9.179290
7.255436	519.314947	9.184307
7.217079	525.870528	9.189325
7.114869	544.468071	9.194343
7.494607	543.913761	9.199360
7.097114	521.424325	9.204378
7.394008	532.390647	9.209395
7.008159	538.433450	9.214413
7.043158	531.284863	9.219431
7.649816	526.048812	9.224448
7.196216	527.749034	9.229466
7.313479	530.657497	9.234483
7.098288	526.191334	9.239501
6.970691	527.209122	9.244519
7.389979	525.321983	9.249536
7.280407	535.012557	9.254554
7.380779	517.022022	9.259571
7.128966	538.109715	9.264589
7.238190	547.785786	9.269607
7.386180	522.288136	9.274624
7.352584	534.685946	9.279642
7.751196	542.474559	9.284659
7.242272	526.735272	9.289677
6.999948	534.400437	9.294695
7.166510	533.307604	9.299712
6.981646	543.394768	9.304730
7.488628	527.415959	9.309747
7.643389	520.319416	9.314765
7.163644	541.890520	9.319783
7.476126	538.471866	9.324800
7.267381	538.887197	9.329818
7.255828	547.181660	9.334835
7.409737	521.634130	9.339853
6.977976	547.563777	9.344871
7.327313	531.931298	9.349888
7.203947	538.321064	9.354906
7.349138	532.030690	9.359923
7.425154	522.283846	9.364941
7.114060	513.141182	9.369959
7.314228	519.721300	9.374976
7.106783	537.910069	9.379994
7.392694	543.543814	9.385011
7.548373	523.911820	9.390029
7.458284	541.658092	9.395047
7.647464	533.043196	9.400064
7.301470	532.834642	9.405082
7.366750	536.487509	9.410099
7.845349	539.950159	9.415117
7.601633	535.395525	9.420135
7.652575	538.800933	9.425152
7.420938	534.731861	9.430170
7.255163	527.041030	9.435187
7.346921	544.074378	9.440205
7.257044	536.979192	9.445223
7.337962	516.620010	9.450240
7.329260	542.566816	9.455258
7.757004	571.496381	9.460275
7.579014	562.887635	9.465293
7.437121	556.587033	9.470311
7.734745	563.582635	9.475328
7.697286	557.949029	9.480346
7.477073	533.705768	9.485363
7.359155	540.119331	9.490381
7.651440	550.426282	9.495399
7.712858	547.511879	9.500416
7.739134	570.139132	9.505434
7.454098	554.631638	9.510451
7.412531	540.892955	9.515469
7.419480	552.998137	9.520487
7.644329	567.402187	9.525504
7.705237	583.411540	9.530522
7.825012	569.458622	9.535539
7.782619	549.011342	9.540557
7.670654	570.287718	9.545575
7.796895	558.638600	9.550592
7.474601	555.637454	9.555610
7.424839	548.901670	9.560627
7.502062	548.788974	9.565645
7.584107	573.851793	9.570663
7.555535	579.274211	9.575680
7.623763	562.219872	9.580698
7.587367	569.306395	9.585715
7.736326	575.142163	9.590733
7.501790	565.274812	9.595751
7.556852	555.114501	9.600768
7.807767	565.689740	9.605786
7.763633	568.578143	9.610803
7.874635	573.013003	9.615821
7.433982	574.838713	9.620839
7.719733	564.156650	9.625856
7.578055	551.162739	9.630874
7.725444	569.884175	9.635891
7.828112	573.890220	9.640909
7.848308	577.069483	9.645927
7.722374	566.014338	9.650944
7.598968	563.546598	9.655962
7.903659	578.303600	9.660979
7.950258	574.596984	9.665997
7.859160	570.307292	9.671015
7.946474	555.223361	9.676032
8.093539	570.934291	9.681050
7.791047	588.560743	9.686067
7.928114	573.246588	9.691085
7.565449	561.355718	9.696103
7.917651	564.947597	9.701120
8.090265	571.881208	9.706138
7.652520	572.802363	9.711155
8.126269	576.291504	9.716173
7.839607	578.213286	9.721191
8.014972	557.412676	9.726208
7.846371	573.428460	9.731226
7.638624	576.150552	9.736243
7.889310	550.135141	9.741261
7.668567	565.862275	9.746279
7.845953	564.291015	9.751296
7.849638	585.162385	9.756314
7.736677	568.143788	9.761331
7.923583	569.025474	9.766349
8.002162	602.524219	9.771367
8.274592	603.430838	9.776384
7.988934	590.773100	9.781402
8.053542	563.919370	9.786419
8.231078	557.345373	9.791437
7.764845	571.178298	9.796455
7.771198	567.628686	9.801472
7.958968	575.480005	9.806490
7.955639	607.298190	9.811507
8.153056	601.171844	9.816525
8.342652	594.794601	9.821543
8.107497	571.852496	9.826560
7.924385	572.597454	9.831578
7.678490	591.086159	9.836595
7.984004	583.579448	9.841613
7.935304	608.671408	9.846631
8.050335	596.810985	9.851648
8.003992	604.957925	9.856666
8.069121	604.699532	9.861683
8.300325	595.465329	9.866701
7.846318	613.701920	9.871719
8.560602	604.620489	9.876736
8.407854	592.794089	9.881754
8.210816	596.485991	9.886771
8.272814	596.832867	9.891789
8.185264	590.351666	9.896807
8.319746	569.400951	9.901824
8.183606	574.762623	9.906842
8.088456	564.511513	9.911859
7.910126	553.869646	9.916877
7.971278	580.974128	9.921895
8.369491	577.587348	9.926912
8.571631	574.812729	9.931930
8.070867	584.919064	9.936947
8.159012	577.493147	9.941965
7.860489	579.553366	9.946983
8.363132	588.939511	9.952000
8.446443	609.219967	9.957018
8.326999	603.296041	9.962035
8.185102	575.346322	9.967053
8.268232	591.759769	9.972071
8.543784	585.388201	9.977088
8.065551	585.239973	9.982106
8.113755	605.850248	9.987123
8.398848	592.027524	9.992141
8.610306	583.097392	9.997159
8.544309	584.719396	10.002176
8.065595	585.617507	10.007194
8.231359	574.588342	10.012211
8.162633	559.329169	10.017229
8.275284	575.914048	10.022247
8.312675	605.265665	10.027264
8.662803	608.499926	10.032282
8.316319	575.592409	10.037299
8.430571	579.880713	10.042317
8.314787	568.411899	10.047335
8.111631	576.597235	10.052352
8.464414	588.546010	10.057370
8.345638	601.353902	10.062387
8.483044	598.899436	10.067405
8.347073	612.284918	10.072423
8.217553	604.114469	10.077440
8.419759	597.101658	10.082458
8.273308	599.297727	10.087475
8.245651	604.288825	10.092493
8.186515	626.404144	10.097511
8.552485	616.143902	10.102528
8.381182	597.402331	10.107546
8.248298	598.468227	10.112563
8.287789	605.531697	10.117581
8.027784	611.643273	10.122599
8.227353	611.809093	10.127616
8.235182	598.380314	10.132634
8.380973	609.971003	10.137651
8.740878	624.504318	10.142669
8.387341	605.149333	10.147687
8.437807	614.690119	10.152704
8.648786	624.955552	10.157722
8.438526	613.014758	10.162739
8.747083	621.917000	10.167757
8.319875	620.562446	10.172775
8.435966	633.527954	10.177792
8.720420	628.317367	10.182810
8.587328	642.753680	10.187827
8.832409	631.919576	10.192845
8.709679	627.152552	10.197863
8.598091	610.599989	10.202880
8.354069	608.099631	10.207898
8.300546	627.441673	10.212915
8.471823	641.814698	10.217933
8.599916	629.272064	10.222951
8.814466	636.991367	10.227968
8.874154	626.509369	10.232986
8.515150	640.912465	10.238003
8.919834	651.924822	10.243021
8.877943	636.447515	10.248039
8.877502	655.610200	10.253056
8.871776	612.724052	10.258074
8.461656	601.401367	10.263091
8.595191	606.724486	10.268109
8.810653	615.291223	10.273127
8.797580	618.565535	10.278144
8.929584	621.750241	10.283162
8.651608	625.156693	10.288179
8.472986	614.957326	10.293197
8.800624	631.249820	10.298215
9.015756	635.859168	10.303232
9.061394	628.833449	10.308250
8.852270	612.304086	10.313267
8.968852	603.508879	10.318285
9.268367	598.089770	10.323303
8.822595	600.341799	10.328320
8.944787	605.974088	10.333338
8.596781	604.668240	10.338355
8.387829	584.695950	10.343373
8.474968	600.130969	10.348391
8.243508	631.775743	10.353408
8.450793	638.082962	10.358426
8.587442	639.961068	10.363443
8.836968	632.582744	10.368461
8.693649	632.899101	10.373479
8.828778	635.806894	10.378496
8.889913	639.372897	10.383514
8.779588	634.598410	10.388531
8.710961	646.893961	10.393549
8.811437	640.209273	10.398567
8.562249	618.785922	10.403584
8.824463	623.390045	10.408602
8.739335	649.222533	10.413619
8.674091	657.346548	10.418637
8.924605	658.341905	10.423655
9.017182	681.459410	10.428672
9.444095	676.306738	10.433690
9.064283	669.374826	10.438707
8.842037	635.151928	10.443725
9.030050	656.649247	10.448743
8.826751	676.514294	10.453760
9.299948	663.011404	10.458778
9.061817	666.231605	10.463795
9.101032	646.645663	10.468813
9.109890	642.484963	10.473831
8.836032	644.745585	10.478848
9.133402	648.945100	10.483866
9.077981	646.325894	10.488883
9.094639	660.279238	10.493901
8.633753	666.962861	10.498919
9.141051	674.076872	10.503936
9.580944	662.633052	10.508954
9.160789	657.277456	10.513971
9.012866	663.932873	10.518989
8.987433	657.274397	10.524007
9.048226	662.632877	10.529024
9.242756	665.340164	10.534042
9.261413	660.660660	10.539059
9.326136	665.160069	10.544077
9.162319	653.226132	10.549095
9.012806	658.787724	10.554112
9.011177	671.470636	10.559130
9.064570	662.883321	10.564147
8.963764	680.944039	10.569165
9.252840	666.503632	10.574183
9.191186	665.685447	10.579200
9.126381	667.730375	10.584218
9.330037	679.219650	10.589235
9.167256	658.391441	10.594253
9.324442	676.283273	10.599271
9.194940	673.816719	10.604288
9.167056	659.406462	10.609306
9.016102	678.935099	10.614323
9.101871	674.473275	10.619341
9.237034	666.820805	10.624359
8.879767	670.948344	10.629376
8.905213	668.084929	10.634394
8.999183	680.812761	10.639411
9.112487	681.123018	10.644429
9.339375	688.939298	10.649447
9.166150	700.493922	10.654464
9.393632	700.404018	10.659482
9.334555	704.915337	10.664499
9.249254	696.617584	10.669517
9.960180	684.990610	10.674535
9.588094	680.362981	10.679552
9.095801	678.584554	10.684570
9.330334	681.184473	10.689587
9.350716	693.636171	10.694605
9.549919	712.510886	10.699623
9.534893	702.184255	10.704640
9.852857	686.009317	10.709658
9.203563	693.150051	10.714675
9.711486	712.058271	10.719693
9.615504	680.775898	10.724711
9.380294	670.971072	10.729728
9.442302	679.901794	10.734746
9.383887	679.588543	10.739763
9.390325	668.903564	10.744781
9.639387	665.732894	10.749799
9.005917	674.055127	10.754816
9.552244	701.011551	10.759834
9.722640	705.256565	10.764851
9.352615	684.450763	10.769869
9.457052	683.547763	10.774887
9.311782	692.870719	10.779904
9.340605	697.309553	10.784922
9.245629	691.252352	10.789939
9.456933	695.293611	10.794957
9.608475	696.262721	10.799975
9.255632	713.429262	10.804992
9.428929	676.976832	10.810010
9.201822	685.147194	10.815027
9.333294	698.055011	10.820045
9.680796	706.863589	10.825063
9.660058	723.661663	10.830080
9.435753	733.954432	10.835098
9.271635	728.208562	10.840115
9.187420	726.545022	10.845133
9.759091	721.152035	10.850151
9.621036	730.051496	10.855168
9.852973	718.116261	10.860186
9.651931	709.402314	10.865203
9.865084	721.152872	10.870221
9.993624	727.358311	10.875239
9.732038	729.493428	10.880256
9.889316	716.675304	10.885274
10.030721	724.723877	10.890291
9.887987	737.846191	10.895309
9.824787	733.638728	10.900327
9.881393	727.507559	10.905344
10.032078	709.395424	10.910362
10.125644	721.779652	10.915379
9.769189	723.400276	10.920397
10.003603	694.020317	10.925415
9.651190	697.161308	10.930432
9.744786	694.214205	10.935450
9.675190	693.010035	10.940467
9.929421	719.583977	10.945485
10.212445	708.582568	10.950503
9.731742	702.934289	10.955520
9.664181	680.175980	10.960538
9.945097	694.341420	10.965555
10.017697	714.927836	10.970573
10.039855	710.359027	10.975591
9.747201	700.655284	10.980608
9.709012	702.815076	10.985626
9.957602	729.654953	10.990643
10.201322	728.529282	10.995661
10.298564	718.784906	11.000679
9.890003	718.787519	11.005696
10.171473	692.626561	11.010714
9.912696	672.991137	11.015731
9.605221	697.207955	11.020749
10.158520	718.061099	11.025767
9.811166	710.350591	11.030784
10.019406	702.476833	11.035802
10.080063	716.638744	11.040819
9.945908	736.505134	11.045837
10.252182	721.166509	11.050855
9.941410	717.896275	11.055872
9.998567	719.209732	11.060890
10.154440	737.181357	11.065907
9.630233	750.318507	11.070925
10.240074	721.167615	11.075943
10.251239	718.607256	11.080960
9.931686	730.551929	11.085978
10.245894	731.213527	11.090995
10.157101	727.569199	11.096013
10.272878	712.352393	11.101031
9.902664	721.445291	11.106048
9.856521	731.197830	11.111066
9.892806	724.968572	11.116083
9.976500	729.701315	11.121101
9.972047	719.595797	11.126119
9.929507	728.347717	11.131136
9.918518	734.515505	11.136154
10.162881	733.688071	11.141171
9.883922	735.077740	11.146189
10.028383	729.897930	11.151207
10.117976	736.838251	11.156224
10.384677	766.491657	11.161242
10.283270	763.808496	11.166259
10.531759	760.233485	11.171277
10.271550	739.582051	11.176295
10.121028	756.542811	11.181312
10.233908	752.401888	11.186330
10.380710	760.234489	11.191347
10.087903	768.275239	11.196365
10.503586	763.583522	11.201383
10.593263	763.391228	11.206400
10.105412	747.872579	11.211418
10.280702	759.990841	11.216435
10.432336	770.055902	11.221453
10.342549	762.821363	11.226471
10.828038	751.081734	11.231488
10.465697	746.969853	11.236506
10.389064	741.778164	11.241523
9.874647	735.304666	11.246541
10.257940	730.010112	11.251559
10.561380	755.587573	11.256576
10.330645	773.072984	11.261594
10.787186	769.529024	11.266611
10.510985	749.542343	11.271629
11.050642	757.632374	11.276647
10.373629	749.127146	11.281664
10.568117	737.251219	11.286682
10.353309	739.840882	11.291699
10.185043	741.969533	11.296717
10.551581	751.554405	11.301735
10.531376	750.667669	11.306752
10.569610	768.233689	11.311770
10.961708	775.077101	11.316787
10.744533	773.290096	11.321805
10.296339	735.897995	11.326823
10.659986	742.537883	11.331840
10.565781	751.233411	11.336858
10.406853	750.040851	11.341875
10.360197	745.921965	11.346893
10.198894	754.060333	11.351911
10.359676	773.193865	11.356928
10.565098	780.417935	11.361946
10.354255	777.317639	11.366963
10.023191	765.304686	11.371981
10.506130	763.159725	11.376999
10.226814	783.241255	11.382016
10.491478	780.633679	11.387034
11.123260	776.836802	11.392051
10.830746	802.266142	11.397069
10.925963	779.668037	11.402087
10.682650	763.031495	11.407104
10.444640	763.198095	11.412122
10.888607	785.074343	11.417139
10.513189	778.167337	11.422157
10.660822	784.422976	11.427175
10.696364	799.061526	11.432192
10.621549	785.065196	11.437210
10.821781	798.242270	11.442227
10.734641	802.601998	11.447245
11.124169	786.589490	11.452263
11.239296	801.018191	11.457280
10.932996	783.645386	11.462298
10.634412	779.101518	11.467315
10.713523	780.271135	11.472333
10.962414	788.188328	11.477351
11.407387	796.760044	11.482368
11.201474	774.724171	11.487386
10.936783	760.225726	11.492403
10.660977	775.624078	11.497421
10.855670	762.165652	11.502439
10.855857	752.672565	11.507456
10.518082	755.921453	11.512474
11.359260	780.053961	11.517491
10.790538	767.329402	11.522509
10.682721	758.752637	11.527527
11.125818	790.863667	11.532544
10.822644	795.186181	11.537562
11.342615	785.338546	11.542579
10.968044	783.832994	11.547597
11.053046	786.584872	11.552615
10.934626	778.470059	11.557632
11.149774	792.294389	11.562650
11.069265	780.237558	11.567667
11.131398	788.662062	11.572685
10.939060	796.372922	11.577703
11.157762	785.706213	11.582720
10.912610	797.649762	11.587738
11.180758	797.408196	11.592755
11.014880	783.816970	11.597773
10.768799	792.072194	11.602791
11.051338	793.271661	11.607808
10.890315	796.845485	11.612826
10.989146	794.884732	11.617843
10.960412	798.960078	11.622861
10.770233	781.745399	11.627879
11.136628	801.421505	11.632896
11.008705	799.106794	11.637914
10.939793	793.998041	11.642931
10.419547	806.225085	11.647949
11.030546	819.588163	11.652967
11.012043	827.586171	11.657984
11.274180	825.625683	11.663002
11.335666	825.476620	11.668019
10.981696	835.429761	11.673037
11.336211	835.527567	11.678055
11.699237	827.509791	11.683072
11.276945	826.339396	11.688090
11.447346	830.261598	11.693107
11.423808	839.520246	11.698125
11.339754	821.687750	11.703143
11.495727	835.689767	11.708160
11.467680	832.672704	11.713178
11.290563	805.856825	11.718195
11.559087	819.695089	11.723213
11.137933	851.829419	11.728231
11.343181	839.575062	11.733248
11.265674	829.657678	11.738266
11.299709	840.847634	11.743283
10.915782	829.953800	11.748301
11.299055	832.336303	11.753319
11.743911	844.269669	11.758336
11.326704	843.036834	11.763354
11.391850	835.432850	11.768371
11.311127	819.560209	11.773389
11.120316	831.963478	11.778407
11.720843	825.849243	11.783424
11.548963	832.815501	11.788442
11.599075	830.156094	11.793459
11.837801	829.593000	11.798477
11.384680	843.924657	11.803495
11.659975	829.989294	11.808512
11.332512	823.026225	11.813530
11.676986	815.730227	11.818547
11.628263	824.933103	11.823565
11.253588	831.863897	11.828583
11.670583	823.278396	11.833600
11.599377	820.371197	11.838618
11.704500	827.986077	11.843635
11.550304	847.964064	11.848653
11.544877	846.658160	11.853671
11.746201	816.784748	11.858688
11.658130	825.738094	11.863706
11.634358	834.394970	11.868723
11.941761	840.914997	11.873741
11.582113	833.993749	11.878759
11.885402	843.880195	11.883776
11.695000	837.193504	11.888794
11.839404	831.147069	11.893811
11.761345	821.427662	11.898829
11.707336	822.080843	11.903847
11.736495	823.782496	11.908864
11.934253	835.295789	11.913882
11.759803	835.647405	11.918899
11.630015	823.420483	11.923917
11.564233	843.821827	11.928935
12.175189	833.054543	11.933952
11.882145	812.470822	11.938970
11.767243	806.667490	11.943987
11.635744	839.704656	11.949005
11.799941	828.507305	11.954023
11.952095	829.508204	11.959040
11.981806	857.122567	11.964058
11.709964	846.450390	11.969075
11.713321	841.388619	11.974093
11.790917	841.669850	11.979111
11.897183	857.106198	11.984128
11.780373	878.076994	11.989146
11.677873	860.170652	11.994163
11.977316	849.134548	11.999181
11.864910	847.511176	12.004199
11.812525	862.262716	12.009216
11.794594	872.897358	12.014234
12.240363	861.158601	12.019251
12.208514	851.800338	12.024269
11.690197	856.641268	12.029287
11.697269	868.241891	12.034304
11.973021	869.218431	12.039322
12.030248	848.454662	12.044339
12.065259	854.663998	12.049357
12.196399	874.129043	12.054375
12.389437	860.951439	12.059392
11.788877	848.056038	12.064410
11.982307	850.205125	12.069427
12.226447	854.816241	12.074445
12.154492	837.122241	12.079463
12.038814	848.416253	12.084480
11.674803	878.994166	12.089498
12.127184	885.579305	12.094515
12.239177	877.689580	12.099533
12.358701	897.876169	12.104551
12.388819	893.348203	12.109568
12.230684	898.912291	12.114586
12.246639	889.731391	12.119603
12.213188	866.240292	12.124621
12.230157	881.635729	12.129639
12.425403	895.364058	12.134656
12.354558	883.949769	12.139674
12.123547	858.860755	12.144691
12.681793	877.643966	12.149709
12.142698	875.112820	12.154727
12.383299	866.934102	12.159744
12.666084	852.480294	12.164762
12.026650	837.023307	12.169779
12.142001	864.807144	12.174797
12.472743	896.152623	12.179815
12.634375	878.333874	12.184832
12.403706	857.820962	12.189850
12.328361	867.872824	12.194867
12.395459	870.367017	12.199885
12.327668	871.520279	12.204903
12.739606	893.210491	12.209920
12.523316	879.889350	12.214938
12.411647	877.785665	12.219955
12.417874	881.750066	12.224973
12.326772	882.876973	12.229991
12.540757	870.124723	12.235008
12.670896	883.463218	12.240026
12.921416	896.242208	12.245043
12.717746	884.816610	12.250061
12.203587	870.616305	12.255079
12.490591	861.552102	12.260096
12.416135	869.302262	12.265114
12.563981	875.874748	12.270131
12.854791	883.017353	12.275149
12.662399	904.500052	12.280167
12.713647	896.617895	12.285184
12.489863	870.130496	12.290202
12.616466	870.358069	12.295219
12.771453	891.904669	12.300237
12.741035	883.244983	12.305255
12.645394	866.409265	12.310272
12.707206	873.090628	12.315290
12.681977	880.133630	12.320307
12.882021	887.232099	12.325325
12.476362	899.706057	12.330343
12.574388	892.915195	12.335360
12.591902	884.555872	12.340378
13.023711	880.279750	12.345395
12.765162	898.185933	12.350413
12.451243	891.397713	12.355431
12.637391	866.367077	12.360448
12.588871	883.861566	12.365466
12.670202	902.048602	12.370483
12.503252	899.951097	12.375501
12.546159	889.102400	12.380519
12.714558	896.697805	12.385536
12.929355	893.223778	12.390554
12.598640	888.954310	12.395571
12.803379	889.894075	12.400589
12.818947	919.193813	12.405607
12.980737	911.963186	12.410624
13.307200	905.849144	12.415642
12.883527	909.949147	12.420659
12.768063	897.672863	12.425677
12.346630	908.570223	12.430695
12.728199	910.037314	12.435712
12.729463	920.885296	12.440730
12.974589	911.583166	12.445747
12.869191	905.709839	12.450765
12.591170	914.905596	12.455783
12.177918	918.504797	12.460800
12.922703	927.246274	12.465818
13.073031	946.937610	12.470835
13.159768	939.738365	12.475853
13.421003	934.372597	12.480871
13.407338	934.720767	12.485888
13.370235	907.848016	12.490906
13.069544	896.618514	12.495923
13.256483	903.828477	12.500941
13.259713	921.887930	12.505959
13.252202	905.270418	12.510976
13.334232	898.197331	12.515994
13.032101	918.447037	12.521011
13.245266	912.670629	12.526029
13.221454	908.967794	12.531047
13.034219	905.759857	12.536064
13.062788	905.808014	12.541082
13.238312	918.849449	12.546099
13.383147	907.056381	12.551117
13.465686	899.849583	12.556135
13.196410	896.750062	12.561152
13.403108	900.135222	12.566170
13.261382	904.083834	12.571187
13.475865	903.634362	12.576205
13.547972	920.831866	12.581223
13.617648	896.491907	12.586240
13.387759	906.003340	12.591258
13.530571	915.109084	12.596275
13.542174	908.381106	12.601293
13.503956	903.896607	12.606311
13.498931	894.975206	12.611328
13.792657	901.523695	12.616346
13.453599	925.814972	12.621363
13.342719	914.235471	12.626381
13.479357	911.995298	12.631399
13.112781	902.191665	12.636416
13.674789	899.677216	12.641434
13.388251	903.306148	12.646451
13.797788	884.691306	12.651469
13.320945	896.105850	12.656487
13.253750	891.899398	12.661504
13.419935	897.116954	12.666522
13.191971	918.041722	12.671539
13.438504	896.738075	12.676557
13.392998	904.251048	12.681575
13.617787	914.937808	12.686592
13.829929	938.736348	12.691610
13.459955	950.000530	12.696627
13.662664	932.680015	12.701645
13.818223	932.664579	12.706663
13.946506	934.805551	12.711680
13.705868	916.973335	12.716698
13.407422	911.577166	12.721715
13.860772	906.511069	12.726733
13.769188	926.518171	12.731751
13.662826	941.847359	12.736768
14.095612	936.730924	12.741786
13.692715	920.176080	12.746803
13.905967	915.543650	12.751821
13.626296	916.728585	12.756839
13.756727	905.105571	12.761856
13.886045	934.020394	12.766874
13.573184	952.374674	12.771891
13.878288	941.048274	12.776909
13.686368	926.148572	12.781927
13.533216	942.312641	12.786944
13.691137	940.627070	12.791962
13.264610	944.274226	12.796979
13.520773	956.464199	12.801997
13.802016	946.897878	12.807015
13.712087	927.774241	12.812032
13.792956	937.428579	12.817050
13.459608	962.940406	12.822067
13.574527	959.853543	12.827085
13.663142	960.954593	12.832103
14.054310	973.038628	12.837120
14.325306	973.584281	12.842138
14.010045	979.969928	12.847155
14.222664	964.833104	12.852173
14.244739	959.753342	12.857191
14.087513	972.854438	12.862208
14.309552	969.239175	12.867226
14.225112	958.040212	12.872243
13.986424	962.411549	12.877261
13.923020	965.515755	12.882279
13.935551	980.627944	12.887296
14.390800	973.005475	12.892314
14.030834	969.742233	12.897331
14.532870	969.887986	12.902349
14.604242	949.347472	12.907367
14.401852	968.143140	12.912384
14.341242	944.723025	12.917402
13.848638	939.891865	12.922419
14.253671	937.975054	12.927437
14.380961	970.281035	12.932455
14.309467	964.307225	12.937472
14.204090	956.488904	12.942490
14.126710	982.361508	12.947507
14.480143	974.237099	12.952525
14.600607	950.012252	12.957543
14.457562	961.052571	12.962560
14.144430	955.613746	12.967578
14.313936	964.081019	12.972595
14.375264	958.759005	12.977613
14.651881	960.024408	12.982631
14.413089	954.999763	12.987648
14.560011	958.197228	12.992666
14.375288	949.588982	12.997683
14.416729	938.413903	13.002701
14.488835	940.328001	13.007719
14.345281	960.737138	13.012736
14.560098	962.331668	13.017754
13.981044	952.505651	13.022771
14.291764	954.961565	13.027789
14.254124	967.752418	13.032807
14.273677	970.314902	13.037824
14.494709	954.214347	13.042842
14.277526	963.578675	13.047859
14.233507	963.105894	13.052877
14.496216	947.229797	13.057895
14.460474	973.385489	13.062912
14.894938	962.864253	13.067930
14.459228	965.451494	13.072947
14.704353	970.803925	13.077965
14.980882	965.516897	13.082983
14.465432	977.463336	13.088000
14.864349	971.759529	13.093018
14.466524	964.714543	13.098035
14.673819	964.012779	13.103053
14.265647	968.504327	13.108071
14.705829	997.086276	13.113088
14.949455	1001.845121	13.118106
14.739216	1003.554377	13.123123
15.126098	980.100699	13.128141
14.987802	987.128979	13.133159
14.600490	990.585362	13.138176
15.182637	986.225327	13.143194
15.176107	979.266419	13.148211
14.613324	968.349005	13.153229
14.662803	952.320787	13.158247
14.424293	979.350431	13.163264
14.873339	997.686700	13.168282
14.771993	993.631692	13.173299
14.830158	985.142006	13.178317
14.994448	983.044066	13.183335
14.897125	1012.064387	13.188352
15.100627	989.404389	13.193370
14.991155	986.198737	13.198387
15.083620	993.568905	13.203405
15.396719	1001.020991	13.208423
14.955176	989.517037	13.213440
15.049168	992.343924	13.218458
14.845430	995.030495	13.223475
14.874291	995.591564	13.228493
15.169470	983.383238	13.233511
14.934953	993.534204	13.238528
15.088857	996.344303	13.243546
15.221907	1005.913604	13.248563
14.872390	1000.826751	13.253581
14.911854	995.194834	13.258599
15.092091	988.361021	13.263616
15.385763	982.576399	13.268634
15.057009	1004.307404	13.273651
15.043143	1006.233652	13.278669
15.267282	993.069884	13.283687
14.990552	999.985452	13.288704
15.467949	1004.984335	13.293722
15.413200	999.432340	13.298739
15.094840	1000.002278	13.303757
15.191849	1000.487632	13.308775
15.218349	1001.760523	13.313792
15.312375	985.747147	13.318810
15.313235	1007.080072	13.323827
15.168246	999.091942	13.328845
15.470924	991.444296	13.333863
15.126433	1010.269305	13.338880
15.442098	1008.737927	13.343898
15.643099	1004.199794	13.348915
15.616573	1022.124554	13.353933
15.846234	1008.555141	13.358951
15.285475	1006.987937	13.363968
15.551541	986.346515	13.368986
15.389875	990.887270	13.374003
15.416458	994.582165	13.379021
15.521698	1002.021468	13.384039
15.327347	1006.725463	13.389056
15.501213	1016.550557	13.394074
15.516246	1022.141570	13.399091
15.593680	1010.251222	13.404109
15.765316	1024.409838	13.409127
15.546391	1041.508072	13.414144
15.773028	1042.710303	13.419162
15.678979	1022.504529	13.424179
15.360822	1009.071698	13.429197
15.894616	1026.068743	13.434215
15.518533	1030.979407	13.439232
15.706777	1015.516329	13.444250
15.931977	998.198420	13.449267
15.441274	1022.642634	13.454285
15.784863	1037.081526	13.459303
15.560196	1039.631737	13.464320
15.895038	1029.109011	13.469338
15.794256	1029.295149	13.474355
15.578067	1019.317511	13.479373
15.687860	1020.496442	13.484391
15.753716	1016.277021	13.489408
15.924584	1028.415908	13.494426
15.795082	1022.118675	13.499443
15.399392	1022.024695	13.504461
15.767614	1022.070251	13.509479
15.829301	1026.076988	13.514496
15.831378	1013.720768	13.519514
16.127058	1015.084968	13.524531
16.131076	1006.474330	13.529549
15.794178	1012.518674	13.534567
16.013001	1030.975981	13.539584
15.953276	1050.159387	13.544602
16.102547	1012.223597	13.549619
15.879021	1008.266611	13.554637
15.831812	1018.996130	13.559655
15.534712	1023.018961	13.564672
15.827885	1047.289097	13.569690
16.169886	1039.295448	13.574707
16.092373	1045.623038	13.579725
16.493019	1066.604199	13.584743
16.476481	1058.885190	13.589760
16.339545	1032.960889	13.594778
16.028094	1026.243640	13.599795
15.839456	1041.717004	13.604813
16.406831	1034.587460	13.609831
16.241124	1041.427430	13.614848
16.024274	1046.464009	13.619866
16.243922	1039.149960	13.624883
16.110136	1055.266052	13.629901
16.601111	1064.218605	13.634919
16.439690	1059.151520	13.639936
16.166189	1043.976011	13.644954
16.044558	1037.536267	13.649971
16.132402	1056.368187	13.654989
16.372259	1053.145530	13.660007
16.174002	1057.715082	13.665024
16.283457	1032.020764	13.670042
16.527617	1036.610481	13.675059
16.418585	1062.989186	13.680077
16.758653	1060.791536	13.685095
16.388275	1044.953761	13.690112
16.815157	1046.882551	13.695130
16.867861	1054.311251	13.700147
16.291032	1065.940327	13.705165
16.594682	1048.543000	13.710183
16.530187	1045.974721	13.715200
16.507879	1043.814326	13.720218
16.568474	1059.984991	13.725235
16.134642	1057.491521	13.730253
16.409750	1038.436842	13.735271
16.626380	1044.295259	13.740288
16.424935	1062.611554	13.745306
16.719317	1036.966371	13.750323
16.185065	1034.083108	13.755341
16.447459	1037.158875	13.760359
16.264081	1058.353438	13.765376
16.329170	1064.212995	13.770394
16.518546	1066.462365	13.775411
16.769773	1067.351360	13.780429
16.982263	1063.560828	13.785447
16.817580	1068.211722	13.790464
16.584631	1082.352628	13.795482
16.927529	1069.181765	13.800499
16.664241	1082.477210	13.805517
16.854651	1058.958168	13.810535
16.731245	1083.549110	13.815552
16.766186	1076.490611	13.820570
17.088581	1066.042634	13.825587
16.972203	1069.157682	13.830605
17.043800	1078.530642	13.835623
17.115735	1081.342790	13.840640
17.098671	1076.968593	13.845658
17.139845	1059.192664	13.850675
16.859478	1072.252695	13.855693
17.082261	1074.201639	13.860711
17.564027	1068.769269	13.865728
17.085522	1066.446034	13.870746
17.093895	1059.197985	13.875763
16.823953	1038.628271	13.880781
16.896431	1026.286384	13.885799
17.021333	1041.197038	13.890816
16.785779	1070.111285	13.895834
17.462205	1056.986667	13.900851
17.204009	1074.030418	13.905869
17.419743	1071.375578	13.910887
17.427938	1042.743304	13.915904
16.902431	1033.295197	13.920922
17.222205	1027.773303	13.925939
16.860192	1045.753434	13.930957
17.401289	1066.023959	13.935975
17.145886	1070.239073	13.940992
17.049216	1076.611564	13.946010
17.159377	1062.585887	13.951027
17.097715	1057.954271	13.956045
17.393455	1053.499851	13.961063
17.031194	1079.180191	13.966080
17.174495	1078.632171	13.971098
17.540187	1067.867076	13.976115
17.382432	1071.574839	13.981133
17.406917	1075.265376	13.986151
17.506721	1066.422690	13.991168
17.718425	1064.460273	13.996186
17.767393	1063.217882	14.001203
17.469426	1080.013257	14.006221
17.647110	1073.230209	14.011239
17.556644	1060.012594	14.016256
17.412989	1074.839348	14.021274
17.947220	1064.434987	14.026291
17.630831	1077.933938	14.031309
17.864859	1060.936367	14.036327
17.699263	1073.976941	14.041344
17.134350	1069.457712	14.046362
17.502662	1055.996019	14.051379
17.350274	1057.942410	14.056397
17.458590	1065.182466	14.061415
17.688216	1082.878399	14.066432
17.495976	1077.055470	14.071450
17.627423	1067.401358	14.076467
17.701328	1063.087408	14.081485
17.836562	1071.579790	14.086503
17.665767	1071.798163	14.091520
17.266099	1075.813357	14.096538
17.681568	1072.110311	14.101555
17.697137	1082.302762	14.106573
17.619410	1060.928980	14.111591
17.769707	1073.667019	14.116608
17.740225	1096.388496	14.121626
18.027228	1090.524838	14.126643
17.947994	1103.598692	14.131661
17.857931	1103.146308	14.136679
18.092396	1100.137077	14.141696
17.853168	1112.323827	14.146714
17.960743	1092.982449	14.151731
17.751661	1097.709078	14.156749
17.784864	1095.194903	14.161767
17.882964	1094.349408	14.166784
17.988537	1114.344444	14.171802
18.176952	1104.677352	14.176819
17.813125	1093.876341	14.181837
18.033528	1083.193105	14.186855
18.171290	1102.822267	14.191872
17.912643	1112.586747	14.196890
18.355623	1099.366354	14.201907
18.298249	1086.326371	14.206925
18.249173	1088.099432	14.211943
18.497695	1095.001648	14.216960
17.828284	1106.459093	14.221978
18.367764	1104.026367	14.226995
18.082162	1090.301344	14.232013
17.833105	1102.095616	14.237031
18.086330	1109.514452	14.242048
17.640217	1114.793811	14.247066
18.131351	1085.298156	14.252083
18.042063	1107.237112	14.257101
18.125565	1139.336862	14.262119
18.471275	1127.959628	14.267136
18.132290	1124.420610	14.272154
18.623157	1135.775581	14.277171
18.575771	1118.427897	14.282189
18.110411	1133.442681	14.287207
18.865778	1125.554943	14.292224
18.710550	1133.075829	14.297242
18.556385	1124.017958	14.302259
18.449752	1119.372401	14.307277
18.471502	1118.288797	14.312295
18.706042	1121.536269	14.317312
18.585880	1128.153844	14.322330
18.830219	1108.593240	14.327347
18.806288	1096.789933	14.332365
17.960617	1104.615606	14.337383
18.434351	1109.763616	14.342400
18.491398	1114.115742	14.347418
18.598312	1107.558101	14.352435
18.752109	1117.542345	14.357453
18.478725	1116.513320	14.362471
18.761355	1129.060483	14.367488
18.733575	1127.228164	14.372506
19.134050	1120.771376	14.377523
19.001163	1114.185858	14.382541
18.859760	1135.790442	14.387559
18.711443	1120.736727	14.392576
18.966186	1125.219728	14.397594
19.297551	1114.562414	14.402611
18.878652	1115.228085	14.407629
18.710818	1142.802793	14.412647
19.077176	1142.817269	14.417664
18.197427	1128.709317	14.422682
18.668377	1104.957570	14.427699
18.844132	1120.206072	14.432717
18.811872	1138.857327	14.437735
18.685005	1121.875639	14.442752
19.003844	1108.540452	14.447770
19.068956	1104.175595	14.452787
18.613655	1118.916035	14.457805
18.768011	1130.601152	14.462823
19.214939	1116.177928	14.467840
19.009818	1129.550394	14.472858
19.193927	1135.326447	14.477875
19.141165	1118.801593	14.482893
18.652309	1135.656323	14.487911
18.810138	1158.003419	14.492928
18.837505	1160.510622	14.497946
18.917393	1169.744013	14.502963
19.244867	1168.484618	14.507981
19.189294	1152.077585	14.512999
19.662817	1156.913616	14.518016
19.122594	1156.056902	14.523034
19.246980	1132.900639	14.528051
19.491847	1157.443238	14.533069
19.136623	1155.895286	14.538087
19.530168	1146.882386	14.543104
19.334338	1162.100922	14.548122
19.482167	1153.422156	14.553139
19.691451	1134.431347	14.558157
19.523060	1140.237906	14.563175
19.511961	1149.118695	14.568192
19.409911	1152.176583	14.573210
19.448813	1141.029328	14.578227
19.809577	1132.006209	14.583245
19.399523	1148.247389	14.588263
19.661728	1157.349390	14.593280
19.369379	1141.743319	14.598298
19.534329	1137.696123	14.603315
19.408157	1135.904170	14.608333
19.609355	1157.506485	14.613351
19.704711	1147.443625	14.618368
19.394106	1141.026603	14.623386
19.484235	1142.705128	14.628403
19.619256	1159.165419	14.633421
19.321476	1153.699779	14.638439
19.294812	1134.572611	14.643456
19.579361	1151.537088	14.648474
19.907205	1172.648531	14.653491
20.132062	1162.545072	14.658509
20.132682	1175.644561	14.663527
19.946494	1148.545200	14.668544
19.731049	1142.845637	14.673562
19.764494	1146.972104	14.678579
19.826009	1143.280794	14.683597
20.014953	1170.713247	14.688615
20.158494	1162.799564	14.693632
19.969177	1145.219658	14.698650
19.765984	1123.822144	14.703667
20.037617	1127.238149	14.708685
20.017942	1164.399327	14.713703
20.302702	1161.621282	14.718720
20.233795	1140.894787	14.723738
19.875418	1152.401727	14.728755
20.178757	1134.848167	14.733773
19.896723	1140.234638	14.738791
20.188436	1130.106276	14.743808
20.383411	1135.661494	14.748826
20.116111	1142.607744	14.753843
20.143609	1146.509265	14.758861
19.795183	1156.633505	14.763879
20.160332	1143.833119	14.768896
20.079323	1146.538402	14.773914
20.370523	1164.894857	14.778931
20.451214	1172.911093	14.783949
20.423854	1174.901880	14.788967
20.352079	1156.292645	14.793984
20.263357	1160.812245	14.799002
20.061750	1171.405418	14.804019
20.183869	1180.664113	14.809037
20.186899	1156.354336	14.814055
20.597168	1151.622265	14.819072
20.297732	1153.439463	14.824090
20.370886	1165.870622	14.829107
20.541607	1161.679293	14.834125
20.352062	1161.959314	14.839143
20.652208	1154.976606	14.844160
20.556354	1180.493435	14.849178
20.313054	1158.718636	14.854195
20.770819	1155.270131	14.859213
20.712378	1161.997373	14.864231
20.657388	1159.992523	14.869248
20.498808	1166.538431	14.874266
20.500706	1156.999546	14.879283
20.632444	1163.787365	14.884301
20.770405	1160.507920	14.889319
20.970769	1149.301997	14.894336
20.533167	1151.546554	14.899354
20.924572	1150.240776	14.904371
21.032473	1149.832626	14.909389
20.877382	1176.886913	14.914407
21.088787	1155.321946	14.919424
20.641085	1141.660664	14.924442
20.400792	1150.042455	14.929459
20.740889	1153.546044	14.934477
20.738972	1167.304151	14.939495
21.203044	1159.079393	14.944512
20.725447	1160.777940	14.949530
20.629390	1156.983860	14.954547
21.012081	1151.682964	14.959565
20.803952	1142.539928	14.964583
20.815694	1150.889318	14.969600
20.862860	1161.932001	14.974618
20.876059	1162.659108	14.979635
21.241004	1159.088967	14.984653
20.948334	1190.460435	14.989671
21.493084	1181.332293	14.994688
20.993157	1174.188855	14.999706
20.804947	1164.164678	15.004723
21.176502	1183.380596	15.009741
21.000075	1191.489025	15.014759
21.313096	1191.433988	15.019776
21.421378	1181.531724	15.024794
21.266111	1175.413840	15.029811
21.458394	1197.152690	15.034829
21.674310	1202.191604	15.039847
21.220675	1162.804761	15.044864
21.480665	1170.809176	15.049882
21.468988	1154.768909	15.054899
21.526177	1142.983255	15.059917
21.012535	1155.028328	15.064935
21.005563	1180.903999	15.069952
21.670640	1193.598297	15.074970
21.479286	1190.565642	15.079987
21.634953	1171.287263	15.085005
21.614691	1176.853760	15.090023
21.677578	1174.269623	15.095040
21.546483	1185.983850	15.100058
21.273383	1202.353304	15.105075
21.822476	1192.378285	15.110093
21.406530	1183.145779	15.115111
21.581356	1179.424715	15.120128
21.755275	1174.530957	15.125146
21.591099	1178.407482	15.130163
21.803003	1177.743029	15.135181
21.407957	1177.288890	15.140199
21.572415	1166.347093	15.145216
21.808130	1185.335621	15.150234
21.430043	1194.854897	15.155251
21.848083	1180.902022	15.160269
21.458288	1188.096138	15.165287
21.464445	1193.760120	15.170304
21.698634	1178.438659	15.175322
21.245472	1187.378454	15.180339
21.944003	1185.374242	15.185357
21.795992	1202.336162	15.190375
21.920587	1213.259419	15.195392
22.042937	1208.795233	15.200410
21.873701	1195.815365	15.205427
22.112491	1212.376056	15.210445
22.106588	1208.287998	15.215463
22.124013	1188.599279	15.220480
22.286646	1197.939261	15.225498
21.990048	1205.005314	15.230515
22.252079	1191.766823	15.235533
21.898509	1190.250378	15.240551
22.005552	1200.698297	15.245568
22.446385	1200.938006	15.250586
22.240937	1206.201634	15.255603
22.427918	1187.886624	15.260621
22.074766	1190.514379	15.265639
22.399123	1202.267103	15.270656
22.348799	1179.816248	15.275674
22.352903	1199.100684	15.280691
22.405177	1196.035343	15.285709
22.359605	1180.715438	15.290727
22.058484	1195.908997	15.295744
22.249943	1208.387946	15.300762
22.259865	1202.297365	15.305779
22.547179	1182.916231	15.310797
22.236954	1205.851154	15.315815
22.429869	1215.169414	15.320832
22.508114	1198.550302	15.325850
22.327430	1191.769253	15.330867
22.458218	1206.049426	15.335885
22.357961	1214.668086	15.340903
22.437849	1192.695082	15.345920
22.739578	1200.198542	15.350938
22.507956	1215.501865	15.355955
22.478156	1194.755551	15.360973
22.346158	1192.869991	15.365991
22.295355	1211.590230	15.371008
22.569953	1221.665675	15.376026
22.788843	1226.022871	15.381043
22.822097	1235.535302	15.386061
23.029168	1245.699462	15.391079
23.084771	1231.858392	15.396096
22.851827	1201.074638	15.401114
22.716920	1185.126045	15.406131
22.822817	1196.991030	15.411149
22.983979	1224.804360	15.416167
23.066230	1229.504336	15.421184
23.090286	1213.144596	15.426202
22.938018	1193.881160	15.431219
22.918460	1190.418441	15.436237
22.911403	1211.327472	15.441255
23.007318	1206.472179	15.446272
23.221439	1200.221605	15.451290
22.715649	1218.194111	15.456307
22.970615	1220.120535	15.461325
22.960276	1225.619185	15.466343
22.930267	1233.852322	15.471360
23.117069	1222.815376	15.476378
23.376309	1226.228433	15.481395
23.106112	1235.963805	15.486413
23.006138	1231.415713	15.491431
22.890377	1224.035676	15.496448
22.941215	1213.275181	15.501466
22.933387	1221.339823	15.506483
22.900923	1225.329797	15.511501
23.347824	1254.913831	15.516519
23.286960	1251.616154	15.521536
23.787449	1240.772967	15.526554
23.330619	1249.847624	15.531571
23.671704	1250.271987	15.536589
23.417993	1219.742650	15.541607
23.613641	1223.966023	15.546624
23.535199	1218.958678	15.551642
23.371807	1230.560883	15.556659
23.596672	1236.695309	15.561677
23.526709	1231.578219	15.566695
23.507755	1229.748857	15.571712
24.039584	1227.153046	15.576730
23.586427	1226.203119	15.581747
23.732339	1235.084875	15.586765
23.405773	1226.725646	15.591783
23.491128	1238.188447	15.596800
23.837663	1238.316999	15.601818
23.797968	1254.856352	15.606835
23.761794	1248.543602	15.611853
24.024932	1262.930961	15.616871
23.597320	1245.250983	15.621888
23.667915	1245.639062	15.626906
23.840421	1268.683727	15.631923
24.256607	1257.867252	15.636941
24.221265	1237.873978	15.641959
23.967610	1240.380500	15.646976
23.833840	1248.501590	15.651994
23.734850	1246.920337	15.657011
24.148497	1241.223640	15.662029
24.193935	1253.613596	15.667047
23.822325	1262.864880	15.672064
24.171922	1250.392587	15.677082
24.175407	1273.163984	15.682099
23.822389	1266.984080	15.687117
24.434361	1252.196428	15.692135
24.028285	1264.940863	15.697152
24.352939	1258.415268	15.702170
24.037455	1260.333138	15.707187
23.820851	1255.426449	15.712205
24.437706	1268.910483	15.717223
24.561666	1265.829937	15.722240
24.475162	1257.431314	15.727258
24.096190	1267.326577	15.732275
24.299602	1262.336109	15.737293
24.267253	1262.967131	15.742311
24.050851	1251.703855	15.747328
24.154255	1253.654739	15.752346
24.371315	1272.251671	15.757363
24.052198	1257.062209	15.762381
24.171419	1237.278376	15.767399
23.852674	1264.838096	15.772416
24.196071	1292.013801	15.777434
24.289926	1288.687694	15.782451
24.386570	1279.225672	15.787469
24.356665	1278.383116	15.792487
24.114055	1288.674656	15.797504
24.703254	1300.431906	15.802522
24.600156	1297.430796	15.807539
24.820712	1308.503873	15.812557
24.821630	1293.125692	15.817575
24.680752	1281.760958	15.822592
25.085171	1286.864690	15.827610
25.124989	1288.024800	15.832627
24.855278	1273.135942	15.837645
25.331140	1270.313111	15.842663
25.171124	1287.626239	15.847680
25.145085	1263.728184	15.852698
25.172796	1271.449067	15.857715
24.973318	1289.954560	15.862733
25.678409	1269.116810	15.867751
25.033016	1281.082400	15.872768
25.207407	1283.759374	15.877786
24.961911	1280.905294	15.882803
25.218277	1262.881412	15.887821
25.779192	1269.409127	15.892839
25.132028	1260.808245	15.897856
25.018192	1239.681265	15.902874
24.790658	1238.913192	15.907891
25.039749	1243.376497	15.912909
25.124953	1260.163754	15.917927
25.079743	1277.734113	15.922944
25.092036	1274.419421	15.927962
25.311404	1279.968790	15.932979
25.603788	1283.805612	15.937997
25.219341	1278.105981	15.943015
25.394371	1258.795067	15.948032
25.418767	1265.169769	15.953050
25.365197	1279.482642	15.958067
25.453543	1282.912244	15.963085
25.743977	1270.276623	15.968103
25.423956	1274.287563	15.973120
25.526939	1263.501194	15.978138
25.513862	1270.283078	15.983155
25.358786	1267.054498	15.988173
25.359912	1281.296636	15.993191
25.217993	1292.528005	15.998208
25.590971	1263.425068	16.003226
25.385284	1251.210247	16.008243
25.106577	1278.931840	16.013261
25.782283	1262.170824	16.018279
25.424196	1279.907922	16.023296
25.594256	1303.479002	16.028314
25.572306	1291.537947	16.033331
25.538496	1280.369937	16.038349
25.939099	1286.163998	16.043367
25.661390	1296.447666	16.048384
25.809794	1300.600343	16.053402
25.960045	1302.273969	16.058419
25.771625	1290.330314	16.063437
25.876518	1279.516460	16.068455
25.660804	1284.085618	16.073472
25.862123	1298.510484	16.078490
25.728372	1300.551538	16.083507
25.400354	1305.851102	16.088525
26.089347	1305.265441	16.093543
26.009906	1325.018065	16.098560
26.225312	1336.572119	16.103578
26.336462	1328.381485	16.108595
25.996401	1323.263439	16.113613
26.279638	1314.846488	16.118631
26.279172	1313.029215	16.123648
26.648630	1312.511710	16.128666
26.769920	1326.219093	16.133683
26.452000	1332.138997	16.138701
26.523961	1306.254866	16.143719
26.230440	1316.927683	16.148736
26.210048	1316.956970	16.153754
26.802078	1326.028970	16.158771
26.536138	1311.153917	16.163789
26.714397	1300.965274	16.168807
26.145455	1312.058810	16.173824
26.366798	1329.586064	16.178842
26.558124	1321.891810	16.183859
26.199300	1308.577514	16.188877
26.298222	1310.632764	16.193895
26.412387	1334.817023	16.198912
26.636329	1331.208151	16.203930
26.749240	1312.069208	16.208947
26.513483	1316.750324	16.213965
26.762884	1315.013679	16.218983
26.991464	1325.716632	16.224000
26.579188	1311.222272	16.229018
26.857470	1299.486063	16.234035
26.553255	1317.763188	16.239053
26.985692	1303.352319	16.244071
26.951693	1305.527838	16.249088
26.688166	1314.067656	16.254106
26.673841	1322.420562	16.259123
26.830230	1320.528263	16.264141
26.463684	1327.511564	16.269159
26.602448	1337.991137	16.274176
27.022230	1324.921889	16.279194
27.431249	1333.893656	16.284211
27.029892	1354.127369	16.289229
27.447488	1333.224766	16.294247
27.400440	1347.846199	16.299264
27.347020	1341.228851	16.304282
27.491688	1311.872478	16.309299
27.254469	1326.092643	16.314317
27.392020	1331.404036	16.319335
27.073360	1322.838869	16.324352
27.347351	1335.439784	16.329370
27.035738	1343.585886	16.334387
27.324627	1328.199835	16.339405
27.584540	1336.017288	16.344423
27.500208	1338.337219	16.349440
27.822856	1324.670781	16.354458
27.753596	1322.944285	16.359475
27.333779	1317.006841	16.364493
27.578732	1301.947884	16.369511
27.210687	1308.334714	16.374528
27.308178	1324.024796	16.379546
27.518288	1318.126329	16.384563
27.317208	1330.457503	16.389581
27.347478	1336.849567	16.394599
27.850959	1343.465036	16.399616
27.416601	1335.354510	16.404634
27.568993	1339.836776	16.409651
27.588764	1342.708762	16.414669
27.359698	1325.785065	16.419687
27.477669	1327.005671	16.424704
27.573604	1347.919419	16.429722
27.794460	1375.104896	16.434739
27.656513	1371.715920	16.439757
27.907487	1351.993316	16.444775
28.056523	1362.835592	16.449792
27.895959	1381.612260	16.454810
28.355250	1367.922710	16.459827
28.163652	1359.834342	16.464845
28.276853	1364.459970	16.469863
28.195182	1362.430080	16.474880
28.347169	1377.400746	16.479898
28.582365	1354.197102	16.484915
28.211360	1355.191698	16.489933
28.450563	1359.676156	16.494951
28.109971	1359.814644	16.499968
28.286004	1357.777691	16.504986
28.488905	1349.747728	16.510003
28.250879	1359.455525	16.515021
28.476264	1369.588106	16.520039
27.992313	1346.486097	16.525056
28.223455	1352.992084	16.530074
28.427960	1339.027810	16.535091
28.081561	1355.927038	16.540109
28.370376	1360.082407	16.545127
28.262038	1364.062127	16.550144
28.028312	1365.025083	16.555162
28.468494	1339.204228	16.560179
28.565388	1345.290768	16.565197
28.290934	1344.903781	16.570215
28.603083	1357.017910	16.575232
28.403908	1367.415979	16.580250
28.269888	1380.051097	16.585267
28.706718	1372.369384	16.590285
29.214190	1382.816691	16.595303
29.154427	1381.350961	16.600320
28.769930	1366.797344	16.605338
28.993329	1357.966734	16.610355
28.610229	1381.106929	16.615373
28.853011	1372.525509	16.620391
29.348222	1379.576119	16.625408
28.889018	1375.663888	16.630426
28.867647	1360.617101	16.635443
28.705967	1390.318698	16.640461
28.766495	1382.713335	16.645479
29.163368	1371.877438	16.650496
28.848383	1380.669244	16.655514
29.098643	1390.057347	16.660531
28.788367	1388.848123	16.665549
28.905460	1380.253521	16.670567
29.358727	1379.516602	16.675584
28.731862	1378.993704	16.680602
28.919495	1372.759737	16.685619
28.726192	1394.641213	16.690637
29.403199	1396.632431	16.695655
29.670242	1416.901209	16.700672
29.563742	1413.316323	16.705690
29.733388	1404.717451	16.710707
29.561828	1393.336744	16.715725
29.386984	1389.478380	16.720743
29.491410	1387.019891	16.725760
29.677280	1389.828028	16.730778
30.035526	1379.555762	16.735795
29.413313	1380.897905	16.740813
29.469349	1372.774807	16.745831
29.633340	1368.602738	16.750848
29.809166	1381.851854	16.755866
29.708908	1379.637871	16.760883
29.392224	1381.448007	16.765901
29.989705	1401.067806	16.770919
29.926013	1394.407852	16.775936
29.862834	1393.658958	16.780954
30.106363	1382.355495	16.785971
30.101496	1382.429942	16.790989
29.970512	1377.405644	16.796007
29.893546	1371.430708	16.801024
29.787165	1383.271582	16.806042
29.740832	1369.738110	16.811059
30.153527	1401.813925	16.816077
29.831353	1404.934415	16.821095
30.115021	1383.770967	16.826112
29.967996	1385.534862	16.831130
29.918782	1403.119212	16.836147
30.097822	1413.089441	16.841165
30.038126	1404.834896	16.846183
30.433737	1401.009984	16.851200
30.123753	1410.820825	16.856218
30.599736	1396.053344	16.861235
30.531493	1383.549132	16.866253
30.505650	1388.015700	16.871271
30.617294	1402.329725	16.876288
30.347014	1408.669837	16.881306
30.364935	1402.562208	16.886323
30.519095	1400.230901	16.891341
30.163172	1393.016721	16.896359
30.402176	1394.621963	16.901376
30.208541	1392.482451	16.906394
30.425145	1388.533420	16.911411
30.543986	1412.006660	16.916429
30.397189	1415.973167	16.921447
30.449861	1390.016606	16.926464
30.349643	1393.473458	16.931482
30.794400	1411.049791	16.936499
30.751510	1394.847145	16.941517
30.303421	1415.173190	16.946535
30.994335	1412.345299	16.951552
30.865536	1421.844971	16.956570
31.190179	1408.349743	16.961587
31.218422	1394.564118	16.966605
30.922106	1397.358064	16.971623
30.950725	1396.059771	16.976640
30.813368	1395.913846	16.981658
30.699484	1412.434338	16.986675
31.129468	1413.541100	16.991693
30.857010	1433.053382	16.996711
31.438056	1436.499606	17.001728
31.017152	1427.735479	17.006746
31.121867	1425.476399	17.011763
31.133877	1412.082034	17.016781
31.054807	1422.352148	17.021799
31.628358	1418.363704	17.026816
31.104977	1425.689725	17.031834
31.725313	1407.505844	17.036851
31.239941	1419.665026	17.041869
31.123514	1419.972131	17.046887
31.337268	1413.975115	17.051904
31.433432	1425.947374	17.056922
31.272592	1423.799191	17.061939
31.403096	1415.589568	17.066957
31.253681	1412.374388	17.071975
31.486954	1423.619620	17.076992
31.218184	1437.543694	17.082010
31.722411	1436.040059	17.087027
31.986444	1429.980999	17.092045
31.642419	1438.495515	17.097063
31.995964	1442.997806	17.102080
31.775913	1433.743304	17.107098
31.712420	1407.671491	17.112115
31.847659	1438.786281	17.117133
31.610099	1442.048271	17.122151
31.788786	1454.787447	17.127168
31.924398	1449.666029	17.132186
32.049004	1445.297639	17.137203
32.042820	1459.470399	17.142221
31.849382	1473.271452	17.147239
32.118197	1448.820360	17.152256
32.280075	1454.223817	17.157274
32.133226	1462.088185	17.162291
31.975667	1448.280965	17.167309
31.849221	1438.607538	17.172327
32.019805	1445.470640	17.177344
32.000754	1459.073707	17.182362
31.971315	1463.255719	17.187379
32.133699	1447.191006	17.192397
32.357281	1453.057977	17.197415
32.054817	1444.462020	17.202432
32.291435	1440.449052	17.207450
32.616969	1457.773747	17.212467
32.633889	1468.470744	17.217485
32.373001	1465.990643	17.222503
32.619602	1439.209807	17.227520
32.377351	1445.119020	17.232538
32.873101	1451.368771	17.237555
32.470138	1449.813326	17.242573
32.536103	1454.354387	17.247591
32.733681	1458.854610	17.252608
32.504959	1468.788249	17.257626
32.592356	1463.469820	17.262643
32.830569	1473.922523	17.267661
32.715543	1480.387072	17.272679
32.989995	1460.454589	17.277696
32.929815	1459.937132	17.282714
32.800701	1478.510635	17.287731
32.784624	1479.008986	17.292749
32.692283	1477.854664	17.297767
32.906842	1464.589736	17.302784
33.210127	1469.128484	17.307802
32.925179	1479.534211	17.312819
33.223989	1457.412173	17.317837
33.376316	1471.236381	17.322855
33.363397	1466.632011	17.327872
33.223165	1453.639258	17.332890
33.227023	1452.597554	17.337907
33.421862	1454.242082	17.342925
32.955551	1486.560066	17.347943
33.222963	1455.001633	17.352960
33.198780	1460.138663	17.357978
33.330471	1474.974227	17.362995
33.295931	1476.374050	17.368013
32.965421	1464.406702	17.373031
33.140011	1448.322258	17.378048
33.267108	1479.991108	17.383066
33.269992	1500.169920	17.388083
33.425905	1508.244162	17.393101
33.361089	1494.368042	17.398119
33.262785	1479.953496	17.403136
33.460801	1503.220234	17.408154
33.312160	1504.879904	17.413171
33.793575	1500.050360	17.418189
33.847829	1504.819994	17.423207
33.826800	1508.043263	17.428224
33.788817	1508.290469	17.433242
34.384299	1505.483253	17.438259
34.179745	1504.273965	17.443277
34.025020	1497.316186	17.448295
33.793022	1499.153079	17.453312
34.025616	1495.508593	17.458330
33.897279	1490.927815	17.463347
34.198000	1483.429232	17.468365
34.075800	1488.978050	17.473383
34.159210	1509.130184	17.478400
34.036152	1507.060471	17.483418
34.243243	1514.667601	17.488435
34.568543	1507.193383	17.493453
34.259957	1521.242787	17.498471
34.386497	1505.666112	17.503488
34.393441	1518.419553	17.508506
34.389895	1518.721094	17.513523
34.477951	1521.324406	17.518541
34.566722	1527.938524	17.523559
34.673057	1519.407616	17.528576
34.925188	1497.628692	17.533594
34.119118	1501.702791	17.538611
34.909249	1521.511136	17.543629
34.603381	1497.362764	17.548647
34.533312	1473.609421	17.553664
34.991010	1498.986594	17.558682
34.685584	1509.520107	17.563699
34.619625	1484.316686	17.568717
34.362462	1476.825377	17.573735
34.725859	1484.881063	17.578752
34.880869	1511.842286	17.583770
34.955914	1519.827164	17.588787
35.248766	1504.188861	17.593805
34.928948	1508.502024	17.598823
34.726738	1519.028228	17.603840
34.678826	1511.706510	17.608858
34.757643	1500.917473	17.613875
35.032654	1511.673402	17.618893
34.712427	1513.740774	17.623911
34.830911	1519.286927	17.628928
34.648852	1519.347064	17.633946
34.578304	1524.346238	17.638963
34.966650	1530.590056	17.643981
34.945720	1554.047547	17.648999
35.084197	1559.557740	17.654016
35.019500	1540.085639	17.659034
35.057797	1534.318216	17.664051
35.712170	1556.629203	17.669069
35.807016	1576.653481	17.674087
35.786569	1549.373886	17.679104
35.524032	1537.601798	17.684122
35.462879	1529.320167	17.689139
35.552085	1539.098973	17.694157
35.525174	1550.597584	17.699175
35.620657	1547.680807	17.704192
36.040638	1536.572333	17.709210
35.861925	1548.120630	17.714227
35.975118	1553.404637	17.719245
35.992104	1549.670501	17.724263
35.469081	1536.686813	17.729280
35.697397	1531.247162	17.734298
35.784102	1555.324620	17.739315
35.989680	1544.206996	17.744333
36.104923	1558.807518	17.749351
36.032010	1556.559961	17.754368
36.199126	1557.855616	17.759386
36.370199	1555.066373	17.764403
36.121917	1569.149055	17.769421
36.207747	1568.437128	17.774439
36.157900	1553.535869	17.779456
36.362138	1536.805333	17.784474
36.366132	1562.309447	17.789491
36.562213	1569.085534	17.794509
36.587514	1560.077847	17.799527
36.507220	1541.304331	17.804544
36.439703	1550.626767	17.809562
36.322829	1564.665096	17.814579
36.769549	1543.622384	17.819597
36.686412	1558.457022	17.824615
36.342373	1556.468692	17.829632
36.625010	1552.170297	17.834650
36.526220	1559.511236	17.839667
36.718162	1532.746944	17.844685
36.654231	1537.592504	17.849703
36.424118	1543.892675	17.854720
37.030260	1531.637348	17.859738
36.667479	1537.978433	17.864755
37.159260	1533.380578	17.869773
36.902941	1550.722121	17.874791
36.608829	1564.811880	17.879808
36.857450	1554.725786	17.884826
36.651231	1548.390335	17.889843
37.042375	1542.758453	17.894861
36.981192	1556.180717	17.899879
36.445865	1561.197767	17.904896
37.108911	1555.724840	17.909914
37.078599	1568.235321	17.914931
36.960030	1581.019987	17.919949
36.794600	1587.410940	17.924967
37.131511	1586.556853	17.929984
37.386323	1567.727434	17.935002
37.226221	1568.912732	17.940019
37.320334	1572.212635	17.945037
37.189725	1584.128912	17.950055
37.337289	1570.460585	17.955072
37.430773	1557.198069	17.960090
37.186432	1564.032274	17.965107
37.574002	1597.579065	17.970125
37.945291	1598.464785	17.975143
37.941904	1583.874746	17.980160
37.601469	1581.518180	17.985178
37.515159	1584.599137	17.990195
37.737845	1590.241457	17.995213
37.863175	1587.966253	18.000231
37.739949	1593.792187	18.005248
37.862224	1606.974478	18.010266
37.755741	1608.771060	18.015283
37.932311	1609.122643	18.020301
37.983855	1590.927248	18.025319
38.040557	1598.360300	18.030336
38.120979	1589.281098	18.035354
37.783629	1600.084261	18.040371
38.096195	1581.976127	18.045389
38.518113	1580.680821	18.050407
37.908520	1604.259383	18.055424
38.355138	1591.656534	18.060442
38.118636	1596.805080	18.065459
38.159355	1594.693726	18.070477
38.074594	1580.457812	18.075495
38.257700	1590.334396	18.080512
38.350738	1609.277852	18.085530
38.091596	1613.694477	18.090547
38.400865	1623.195486	18.095565
38.954181	1619.645577	18.100583
38.557015	1609.603384	18.105600
38.599740	1610.185013	18.110618
38.619668	1610.273372	18.115635
38.611639	1611.635368	18.120653
38.551317	1618.973817	18.125671
38.616093	1626.594779	18.130688
39.063455	1625.608780	18.135706
38.811569	1615.843396	18.140723
38.811620	1599.548318	18.145741
38.966957	1604.998963	18.150759
38.870273	1619.656805	18.155776
39.349410	1605.880120	18.160794
38.982451	1613.767065	18.165811
39.278891	1614.043045	18.170829
39.476579	1611.701363	18.175847
39.144329	1620.825222	18.180864
39.260434	1609.597264	18.185882
38.931234	1623.018021	18.190899
39.448619	1620.086221	18.195917
39.203025	1614.164543	18.200935
39.241044	1626.336291	18.205952
39.485481	1602.530381	18.210970
39.060465	1600.921194	18.215987
39.020402	1601.451361	18.221005
39.327178	1608.042477	18.226023
39.360889	1616.550169	18.231040
39.984566	1628.384145	18.236058
39.552293	1635.221393	18.241075
39.590956	1628.580635	18.246093
39.580217	1623.537663	18.251111
39.771541	1640.075272	18.256128
39.864383	1621.735152	18.261146
39.866747	1612.126728	18.266163
39.783802	1617.432935	18.271181
39.792865	1610.096735	18.276199
40.098585	1609.371790	18.281216
40.234837	1621.446118	18.286234
40.111668	1638.649443	18.291251
39.764685	1617.858829	18.296269
39.980820	1618.781309	18.301287
39.916020	1631.311121	18.306304
40.315077	1613.065160	18.311322
40.228020	1627.785184	18.316339
39.980172	1623.048169	18.321357
40.217998	1615.949202	18.326375
39.752088	1609.093277	18.331392
40.014479	1633.887729	18.336410
40.142414	1654.742388	18.341427
40.337198	1663.808206	18.346445
40.475453	1647.368906	18.351463
40.549486	1643.512745	18.356480
41.022280	1654.642894	18.361498
40.812501	1659.108744	18.366515
40.590504	1649.598973	18.371533
40.910084	1639.342962	18.376551
40.997954	1641.276488	18.381568
40.787470	1636.301159	18.386586
40.674292	1650.148445	18.391603
41.043854	1668.314052	18.396621
40.862493	1637.047569	18.401639
40.695706	1636.571143	18.406656
41.006892	1630.115024	18.411674
40.888115	1643.847408	18.416691
40.957735	1657.189594	18.421709
40.887434	1652.255745	18.426727
40.736142	1635.626266	18.431744
41.188453	1640.526872	18.436762
41.131055	1652.352183	18.441779
41.025684	1681.125648	18.446797
41.434128	1663.311056	18.451815
41.464390	1662.394573	18.456832
41.535810	1673.328030	18.461850
41.387918	1685.626590	18.466867
41.118868	1681.797299	18.471885
41.284230	1673.335866	18.476903
41.612417	1668.515355	18.481920
41.353136	1672.179225	18.486938
41.807191	1672.528351	18.491955
41.669822	1679.393443	18.496973
41.959293	1681.636893	18.501991
41.582329	1674.415527	18.507008
41.858363	1671.536591	18.512026
41.571148	1667.837149	18.517043
41.614142	1679.798319	18.522061
41.765061	1662.326714	18.527079
41.591552	1676.174055	18.532096
41.963247	1674.865589	18.537114
42.191822	1694.845487	18.542131
42.187545	1719.188186	18.547149
42.249497	1704.972882	18.552167
41.914676	1690.590728	18.557184
41.753237	1701.439385	18.562202
42.223988	1714.714348	18.567219
42.275350	1703.803551	18.572237
42.622487	1691.613631	18.577255
42.227508	1696.079197	18.582272
42.205519	1688.970878	18.587290
42.294504	1696.222498	18.592307
42.512965	1692.670145	18.597325
42.732148	1681.335652	18.602343
42.302442	1700.197138	18.607360
42.456228	1687.937521	18.612378
42.810527	1672.857867	18.617395
42.657262	1690.748559	18.622413
42.675314	1704.828092	18.627431
42.625086	1701.329291	18.632448
42.588694	1681.964217	18.637466
42.858945	1681.797376	18.642483
42.725699	1699.932947	18.647501
43.246679	1720.237413	18.652519
43.323057	1727.799728	18.657536
42.717683	1694.636087	18.662554
43.067415	1695.076650	18.667571
42.886735	1715.647424	18.672589
43.296686	1714.666028	18.677607
43.079136	1716.569343	18.682624
43.312173	1733.294706	18.687642
43.612629	1711.571258	18.692659
43.186749	1727.498802	18.697677
43.403842	1714.554826	18.702695
43.123570	1714.346311	18.707712
43.434433	1706.475549	18.712730
43.294910	1710.233689	18.717747
43.311962	1732.516326	18.722765
43.452871	1720.976082	18.727783
43.512812	1722.867000	18.732800
43.473200	1718.572019	18.737818
43.445076	1726.811604	18.742835
43.546718	1766.485560	18.747853
43.690285	1750.600768	18.752871
43.918329	1745.589836	18.757888
43.608658	1746.924444	18.762906
43.799802	1753.231547	18.767923
43.818360	1761.130827	18.772941
43.974568	1758.898320	18.777959
43.676851	1770.151061	18.782976
43.708228	1760.218425	18.787994
43.952299	1770.737082	18.793011
44.298589	1790.093543	18.798029
44.603837	1776.083194	18.803047
44.577085	1769.502584	18.808064
44.595198	1785.400312	18.813082
44.608091	1763.980459	18.818099
44.392225	1738.802867	18.823117
44.227991	1737.957785	18.828135
44.239708	1758.768616	18.833152
44.146618	1777.213719	18.838170
44.754933	1770.307931	18.843187
44.465922	1759.449013	18.848205
44.652886	1772.727133	18.853223
44.435943	1789.315052	18.858240
44.399639	1776.821181	18.863258
44.676761	1759.879382	18.868275
44.577367	1778.319624	18.873293
44.958584	1775.335609	18.878311
45.204027	1798.111100	18.883328
45.154098	1800.528938	18.888346
45.115038	1796.034377	18.893363
45.168723	1786.701261	18.898381
45.098386	1774.175721	18.903399
44.960833	1765.071228	18.908416
45.260858	1785.094150	18.913434
45.614929	1799.035187	18.918451
45.309037	1802.603269	18.923469
45.427060	1796.437709	18.928487
45.453183	1782.364840	18.933504
45.611698	1783.964630	18.938522
45.326772	1775.832323	18.943539
45.137706	1776.298456	18.948557
45.429069	1777.275824	18.953575
45.480223	1783.882099	18.958592
45.449107	1795.060395	18.963610
45.891352	1808.862092	18.968627
45.551142	1806.138303	18.973645
45.908719	1792.473452	18.978663
45.580174	1792.777830	18.983680
45.823562	1794.144939	18.988698
46.054332	1794.880601	18.993715
45.944350	1794.645518	18.998733
45.965967	1784.213007	19.003751
45.875312	1789.412204	19.008768
45.716515	1794.021408	19.013786
46.073931	1794.932853	19.018803
46.018467	1801.277284	19.023821
46.312618	1808.862991	19.028839
46.469055	1825.398890	19.033856
45.964658	1813.445734	19.038874
46.467864	1823.112024	19.043891
46.311062	1834.572975	19.048909
46.119144	1826.617260	19.053927
46.332302	1799.573658	19.058944
46.071650	1826.007394	19.063962
46.472646	1810.259687	19.068979
46.518467	1800.102341	19.073997
46.538144	1821.913805	19.079015
46.466405	1830.620403	19.084032
46.725295	1845.766441	19.089050
47.024660	1847.365595	19.094067
46.966512	1842.804897	19.099085
47.021374	1850.800959	19.104103
46.817851	1856.287773	19.109120
46.983602	1843.104880	19.114138
47.654099	1820.673014	19.119155
47.289718	1833.863595	19.124173
47.211797	1843.655453	19.129191
47.560192	1841.996269	19.134208
47.167888	1831.242835	19.139226
47.432673	1823.126529	19.144243
47.232402	1840.247270	19.149261
47.296342	1848.502999	19.154279
47.206047	1841.371456	19.159296
47.352722	1833.521561	19.164314
47.313298	1849.643289	19.169331
47.368191	1845.806872	19.174349
47.751107	1833.887643	19.179367
47.579125	1837.450529	19.184384
47.408282	1842.790233	19.189402
47.815750	1854.507685	19.194419
47.541369	1860.332523	19.199437
47.698198	1853.023254	19.204455
48.124163	1851.686322	19.209472
47.878537	1868.409059	19.214490
48.487917	1870.102133	19.219507
48.389642	1861.044822	19.224525
48.163156	1849.721561	19.229543
48.262269	1861.063485	19.234560
48.165189	1845.098504	19.239578
48.145905	1859.053469	19.244595
48.215594	1863.695099	19.249613
48.441647	1857.888654	19.254631
48.606957	1839.960819	19.259648
48.565267	1854.420071	19.264666
48.668013	1863.760517	19.269683
48.566294	1843.996372	19.274701
48.470692	1861.464923	19.279719
48.926215	1864.715892	19.284736
48.215150	1845.458955	19.289754
48.544868	1848.849289	19.294771
48.247445	1869.835249	19.299789
48.551824	1867.663558	19.304807
48.549247	1853.755768	19.309824
48.448309	1852.236670	19.314842
48.665482	1856.380989	19.319859
48.779365	1880.699399	19.324877
48.722337	1897.057308	19.329895
48.841422	1893.745696	19.334912
48.771961	1872.882599	19.339930
48.937632	1874.157167	19.344947
49.100526	1894.927258	19.349965
49.060337	1916.030977	19.354983
49.259147	1901.495591	19.360000
49.334527	1901.656267	19.365018
49.929727	1904.775621	19.370035
50.051393	1908.385451	19.375053
49.618918	1909.118933	19.380071
49.650401	1898.071547	19.385088
49.513488	1917.933626	19.390106
49.864701	1895.766182	19.395123
50.102037	1906.948908	19.400141
49.996656	1909.930543	19.405159
49.996455	1896.563554	19.410176
49.652645	1905.014820	19.415194
50.028213	1911.244670	19.420211
49.920743	1888.406233	19.425229
50.024484	1894.648326	19.430247
49.850873	1900.993822	19.435264
49.684296	1891.266713	19.440282
49.879757	1901.236319	19.445299
49.704469	1916.492358	19.450317
50.027057	1908.394403	19.455335
50.276328	1902.129666	19.460352
50.090112	1931.076672	19.465370
50.381148	1948.171352	19.470387
50.208004	1931.511901	19.475405
50.391555	1917.801597	19.480423
50.614297	1916.059057	19.485440
50.624601	1944.427558	19.490458
50.593208	1938.506374	19.495475
50.521952	1921.317106	19.500493
50.537764	1917.132277	19.505511
50.764362	1945.223253	19.510528
50.802836	1947.473189	19.515546
50.920307	1952.981289	19.520563
51.122144	1940.868912	19.525581
51.235019	1964.487955	19.530599
51.417044	1946.403129	19.535616
51.565355	1958.694881	19.540634
51.742971	1936.460415	19.545651
51.510426	1906.917253	19.550669
51.366907	1908.438155	19.555687
51.360935	1908.274055	19.560704
51.446263	1915.660511	19.565722
51.483067	1910.566879	19.570739
51.222636	1902.891192	19.575757
51.430348	1907.996939	19.580775
51.817172	1922.978241	19.585792
51.555609	1935.490826	19.590810
51.837771	1915.388008	19.595827
52.015786	1944.787447	19.600845
51.659858	1943.563382	19.605863
51.744757	1924.207185	19.610880
51.825325	1927.657603	19.615898
51.635163	1949.840377	19.620915
52.220819	1959.469807	19.625933
51.968595	1949.869390	19.630951
52.032735	1935.527649	19.635968
51.871443	1934.353983	19.640986
51.985500	1934.204194	19.646003
52.061604	1937.730633	19.651021
51.933844	1936.076321	19.656039
51.800023	1935.642558	19.661056
51.889306	1954.554884	19.666074
52.012300	1953.606232	19.671091
52.410528	1953.858707	19.676109
52.300692	1978.559846	19.681127
52.610474	1976.175083	19.686144
52.114965	1971.749601	19.691162
52.479462	1966.731893	19.696179
52.613538	1978.615265	19.701197
52.630901	2002.341175	19.706215
52.797287	1996.168331	19.711232
52.842278	1993.322793	19.716250
52.905335	1991.453512	19.721267
53.113369	1984.926710	19.726285
53.370210	1983.126077	19.731303
53.469034	1993.318170	19.736320
53.050329	1994.515334	19.741338
53.128194	1992.188477	19.746355
52.930022	1999.430815	19.751373
52.914859	1976.242706	19.756391
53.539093	1993.681413	19.761408
53.483518	2032.362647	19.766426
53.535454	2022.179738	19.771443
53.703658	2004.015254	19.776461
53.545404	2001.420682	19.781479
53.886293	2002.554318	19.786496
53.550305	2026.852832	19.791514
53.713125	2022.899538	19.796531
53.693533	2020.119874	19.801549
53.731471	2021.272282	19.806567
54.249396	2009.309744	19.811584
54.197655	1992.490428	19.816602
53.938530	2000.028808	19.821619
54.111976	2019.153838	19.826637
54.126486	2010.573375	19.831655
54.049834	1995.822840	19.836672
53.843606	2004.120051	19.841690
53.727890	2019.254263	19.846707
54.161456	2023.624039	19.851725
54.384279	2028.455924	19.856743
54.321943	2017.177545	19.861760
54.099188	2035.864424	19.866778
54.216011	2049.683902	19.871795
54.607513	2034.971495	19.876813
54.658918	2025.275097	19.881831
54.963268	2038.453258	19.886848
54.972800	2044.103713	19.891866
54.991183	2047.809467	19.896883
54.990343	2022.351039	19.901901
54.667006	2023.658111	19.906919
54.899861	2043.550470	19.911936
54.946986	2069.326005	19.916954
54.954833	2058.735376	19.921971
55.176548	2045.181023	19.926989
55.049823	2062.340930	19.932007
55.167395	2070.567152	19.937024
55.400696	2068.125736	19.942042
55.033835	2057.335660	19.947059
55.338359	2050.503569	19.952077
55.198899	2068.802481	19.957095
55.517188	2048.120496	19.962112
55.409984	2052.903599	19.967130
55.593801	2075.430681	19.972147
55.678385	2074.390848	19.977165
55.899022	2081.902045	19.982183
55.830800	2074.763694	19.987200
55.979519	2090.266111	19.992218
55.997137	2091.309402	19.997235
56.003020	2091.977537	20.002253
55.602328	2085.939501	20.007271
55.971518	2070.954715	20.012288
56.242586	2071.813531	20.017306
56.218114	2076.745932	20.022323
56.329878	2075.934241	20.027341
56.216573	2074.033772	20.032359
55.989216	2064.970018	20.037376
56.291435	2068.320466	20.042394
56.473715	2075.339862	20.047411
56.413959	2088.182147	20.052429
56.501936	2115.767406	20.057447
56.548033	2100.736395	20.062464
56.681098	2110.653468	20.067482
56.959562	2116.552958	20.072499
56.878858	2089.146361	20.077517
56.755801	2114.124556	20.082535
56.904090	2109.894853	20.087552
57.070495	2095.098251	20.092570
56.934050	2083.662514	20.097587
56.833495	2090.156517	20.102605
56.864146	2113.181221	20.107623
56.958087	2102.425083	20.112640
56.965704	2096.005847	20.117658
57.129837	2103.763750	20.122675
57.432401	2121.884778	20.127693
57.194165	2136.308874	20.132711
57.400879	2133.065196	20.137728
57.755650	2123.688517	20.142746
57.773031	2130.825329	20.147763
57.939691	2138.895570	20.152781
57.810731	2139.053902	20.157799
57.723250	2122.869368	20.162816
57.892587	2127.203031	20.167834
57.640322	2139.310578	20.172851
57.998411	2126.501195	20.177869
57.698452	2126.778614	20.182887
58.113583	2146.673166	20.187904
58.269020	2145.310357	20.192922
58.190943	2157.243786	20.197939
58.678223	2159.880627	20.202957
58.362175	2169.881304	20.207975
58.574678	2153.726875	20.212992
58.701384	2147.161485	20.218010
58.418316	2152.424387	20.223027
58.756607	2150.181415	20.228045
58.721140	2150.112918	20.233063
58.654178	2141.381604	20.238080
59.296961	2144.445812	20.243098
58.602777	2135.855348	20.248115
58.625195	2126.759237	20.253133
58.503282	2141.403344	20.258151
58.678363	2121.426692	20.263168
58.958879	2132.505123	20.268186
58.874860	2160.766701	20.273203
58.893966	2144.903741	20.278221
59.001108	2126.888744	20.283239
59.030082	2152.136903	20.288256
59.079383	2153.913020	20.293274
59.109460	2176.533065	20.298291
59.433742	2154.109707	20.303309
59.443605	2175.504080	20.308327
59.538443	2178.999236	20.313344
59.504619	2168.158672	20.318362
59.253533	2169.238500	20.323379
59.302195	2160.833380	20.328397
59.480605	2171.809246	20.333415
59.350743	2187.346479	20.338432
59.995441	2200.892774	20.343450
59.675369	2190.228608	20.348467
59.934061	2174.172805	20.353485
59.850158	2191.426648	20.358503
60.021504	2202.913357	20.363520
60.521912	2197.134663	20.368538
60.069238	2189.251370	20.373555
59.997474	2193.846902	20.378573
60.366672	2202.756288	20.383591
60.308660	2205.308868	20.388608
60.660771	2186.911943	20.393626
60.484888	2183.622443	20.398643
60.511785	2198.639679	20.403661
60.662320	2227.006687	20.408679
60.609921	2226.789341	20.413696
61.319442	2204.877343	20.418714
60.894450	2216.526278	20.423731
61.066094	2217.687998	20.428749
60.956412	2214.115847	20.433767
61.126942	2214.418158	20.438784
61.085368	2211.814109	20.443802
60.942382	2233.855464	20.448819
61.503651	2219.326503	20.453837
60.976917	2210.248760	20.458855
61.085382	2215.078740	20.463872
61.204026	2210.856959	20.468890
61.205942	2214.668213	20.473907
61.198148	2220.768564	20.478925
61.446717	2240.121670	20.483943
61.418858	2244.450852	20.488960
61.612085	2245.721193	20.493978
61.584916	2253.146083	20.498995
61.777440	2235.733278	20.504013
61.910998	2239.813974	20.509031
61.842418	2254.555557	20.514048
61.893757	2253.563718	20.519066
62.039301	2245.853540	20.524083
62.434690	2246.940401	20.529101
62.205946	2236.459206	20.534119
62.018234	2223.696637	20.539136
62.450645	2227.618908	20.544154
62.447129	2257.499260	20.549171
62.651054	2233.644352	20.554189
62.463578	2217.654951	20.559207
62.437815	2229.321176	20.564224
62.687373	2246.540740	20.569242
62.786603	2245.295853	20.574259
63.129215	2257.862278	20.579277
63.117399	2243.298885	20.584295
63.069509	2245.805417	20.589312
63.127840	2248.235253	20.594330
62.666370	2241.245162	20.599347
62.990933	2239.428388	20.604365
63.078841	2246.738311	20.609383
63.118705	2272.051589	20.614400
63.441508	2264.302761	20.619418
63.222039	2248.686858	20.624435
63.422613	2246.793543	20.629453
63.707708	2256.041507	20.634471
63.316735	2272.519556	20.639488
63.844020	2255.658391	20.644506
63.383501	2255.824081	20.649523
63.557094	2257.223039	20.654541
63.426486	2260.825043	20.659559
63.386504	2251.031812	20.664576
63.480746	2257.981701	20.669594
63.549890	2249.443643	20.674611
63.723700	2266.759886	20.679629
63.692196	2276.610381	20.684647
63.746128	2271.690443	20.689664
64.188070	2267.868785	20.694682
64.020951	2288.247762	20.699699
64.094944	2272.999607	20.704717
64.140790	2289.251087	20.709735
64.237947	2315.357390	20.714752
64.754364	2303.817539	20.719770
64.259148	2299.849117	20.724787
64.621339	2307.603326	20.729805
64.557231	2330.540194	20.734823
64.637126	2306.986920	20.739840
64.932363	2291.953324	20.744858
64.660756	2304.682498	20.749875
64.571395	2314.595030	20.754893
65.130161	2316.935980	20.759911
64.875243	2308.836611	20.764928
64.732257	2314.947039	20.769946
65.033356	2329.576727	20.774963
65.364213	2319.506066	20.779981
65.303786	2341.324618	20.784999
65.181100	2326.870004	20.790016
65.637106	2326.910218	20.795034
65.429139	2349.290276	20.800051
65.621868	2334.440085	20.805069
65.713630	2319.347189	20.810087
65.613987	2334.007678	20.815104
65.862052	2326.421144	20.820122
65.868585	2337.571767	20.825139
65.716495	2348.554941	20.830157
65.999545	2342.751099	20.835175
65.976008	2337.982008	20.840192
65.950521	2361.333729	20.845210
66.327025	2351.229721	20.850227
66.262951	2336.524901	20.855245
66.367478	2353.379050	20.860263
66.174334	2361.261664	20.865280
66.219499	2335.858488	20.870298
66.439929	2357.720597	20.875315
66.445403	2351.682156	20.880333
66.507932	2358.584289	20.885351
66.473159	2372.113414	20.890368
66.670181	2371.467216	20.895386
66.639530	2368.875506	20.900403
66.872460	2377.533445	20.905421
67.140664	2391.677568	20.910439
66.922057	2382.392629	20.915456
67.254770	2372.382837	20.920474
67.120321	2367.147697	20.925491
67.107786	2382.023917	20.930509
67.089712	2385.861151	20.935527
67.209820	2383.567306	20.940544
67.626701	2378.867920	20.945562
67.439801	2393.534618	20.950579
67.258202	2408.451397	20.955597
67.671611	2404.234585	20.960615
67.577794	2404.012172	20.965632
67.684520	2396.192703	20.970650
67.889437	2389.000804	20.975667
67.815480	2371.749971	20.980685
68.040276	2391.459008	20.985703
67.740401	2398.271859	20.990720
68.136074	2385.250769	20.995738
67.987621	2378.616202	21.000755
67.715547	2404.467977	21.005773
68.101064	2415.754028	21.010791
68.234078	2420.029220	21.015808
68.436910	2426.509248	21.020826
68.631935	2417.423411	21.025843
68.696903	2433.691959	21.030861
68.829862	2430.725227	21.035879
68.812424	2426.908293	21.040896
69.373928	2399.638086	21.045914
68.888666	2412.422140	21.050931
68.707116	2427.582591	21.055949
68.864491	2417.245896	21.060967
68.620044	2401.556419	21.065984
68.877696	2412.897451	21.071002
69.207494	2433.113711	21.076019
68.904434	2453.986653	21.081037
69.025526	2438.417806	21.086055
69.066886	2428.337836	21.091072
69.275055	2439.475681	21.096090
69.236370	2456.383723	21.101107
69.176904	2446.164325	21.106125
69.598238	2439.820946	21.111143
69.433426	2462.430416	21.116160
69.913299	2473.791455	21.121178
70.156776	2486.544896	21.126195
69.954411	2480.358494	21.131213
70.329096	2475.572169	21.136231
69.951172	2468.752487	21.141248
70.027554	2445.428482	21.146266
70.262476	2460.631740	21.151283
70.281673	2471.390862	21.156301
70.539864	2474.912036	21.161319
70.385192	2470.687523	21.166336
70.436969	2447.054245	21.171354
70.511817	2462.052498	21.176371
70.660373	2502.353084	21.181389
70.588951	2487.310607	21.186407
70.353142	2483.057576	21.191424
70.754694	2484.711260	21.196442
70.952818	2490.047195	21.201459
70.828118	2505.078662	21.206477
71.004838	2493.786310	21.211495
71.063408	2495.858624	21.216512
71.182719	2492.548126	21.221530
71.163405	2504.953732	21.226547
71.469842	2505.459933	21.231565
71.877668	2513.220680	21.236583
71.382706	2533.683188	21.241600
71.844911	2523.720197	21.246618
71.887284	2515.292697	21.251635
71.904022	2507.158370	21.256653
72.085861	2520.606366	21.261671
72.051997	2523.518829	21.266688
72.117522	2509.002041	21.271706
72.226724	2496.160656	21.276723
72.039332	2512.520983	21.281741
72.429397	2508.966952	21.286759
72.155407	2517.642607	21.291776
72.276583	2506.091750	21.296794
72.419772	2496.228927	21.301811
72.207843	2509.626844	21.306829
72.322292	2512.729133	21.311847
72.384408	2511.658639	21.316864
72.448967	2515.488745	21.321882
72.637872	2504.532311	21.326899
72.493878	2492.090983	21.331917
72.638539	2503.572191	21.336935
72.330157	2517.846548	21.341952
72.631751	2539.073554	21.346970
72.647226	2530.942965	21.351987
72.470120	2539.044245	21.357005
72.860341	2545.131996	21.362023
73.193720	2569.171859	21.367040
73.106871	2573.042942	21.372058
73.475333	2568.775648	21.377075
73.513260	2568.357670	21.382093
73.448416	2562.142999	21.387111
73.631549	2566.304848	21.392128
73.556276	2566.970374	21.397146
73.721987	2568.541405	21.402163
73.545846	2580.275849	21.407181
73.845077	2565.266126	21.412199
73.930687	2578.615919	21.417216
74.143412	2584.452154	21.422234
74.227292	2580.353126	21.427251
74.389258	2578.041117	21.432269
74.600002	2562.351834	21.437287
74.078688	2583.227361	21.442304
74.002634	2605.464948	21.447322
74.228055	2583.464131	21.452339
74.231710	2601.525198	21.457357
74.641751	2616.454040	21.462375
74.689632	2614.653914	21.467392
74.683271	2598.830811	21.472410
75.019513	2606.752625	21.477427
74.927880	2624.878474	21.482445
75.163816	2605.106854	21.487463
75.158152	2597.147612	21.492480
74.868112	2600.190598	21.497498
75.483701	2614.607197	21.502515
75.464585	2628.941517	21.507533
75.350381	2607.676804	21.512551
75.595849	2604.045284	21.517568
75.810617	2632.276069	21.522586
75.897724	2632.845877	21.527603
75.555529	2630.169011	21.532621
76.000626	2611.102079	21.537639
76.128967	2617.688185	21.542656
75.888865	2642.227200	21.547674
76.440006	2638.021221	21.552691
76.177754	2623.167603	21.557709
76.527423	2610.112004	21.562727
76.519750	2630.365593	21.567744
76.204477	2631.176671	21.572762
76.246415	2625.320060	21.577779
76.307174	2622.486857	21.582797
76.465300	2625.358363	21.587815
76.431291	2614.472540	21.592832
76.278197	2621.228561	21.597850
76.691736	2620.989815	21.602867
76.562235	2636.599282	21.607885
76.586869	2656.323038	21.612903
76.837284	2656.668449	21.617920
76.884898	2643.168517	21.622938
76.984870	2642.087035	21.627955
76.861301	2665.910871	21.632973
76.931292	2670.751977	21.637991
76.883562	2667.911894	21.643008
77.088010	2671.004854	21.648026
77.470664	2668.184976	21.653043
77.221115	2690.469660	21.658061
77.350191	2698.173430	21.663079
77.726496	2698.285471	21.668096
77.819849	2702.453336	21.673114
78.039006	2718.305424	21.678131
78.058711	2713.004540	21.683149
78.081444	2700.247934	21.688167
78.105120	2702.948590	21.693184
78.058729	2710.504222	21.698202
78.277832	2688.845588	21.703219
78.129720	2703.979134	21.708237
78.327657	2708.019104	21.713255
78.395678	2707.244822	21.718272
78.255042	2721.246801	21.723290
78.914103	2722.381256	21.728307
78.692772	2726.438356	21.733325
78.869094	2726.911154	21.738343
79.331763	2721.692951	21.743360
78.934522	2719.896694	21.748378
78.997160	2741.296518	21.753395
78.888923	2736.789493	21.758413
79.128225	2725.943259	21.763431
78.968520	2737.297010	21.768448
79.074612	2747.652455	21.773466
79.509593	2732.456775	21.778483
79.422147	2741.050162	21.783501
79.606168	2749.292635	21.788519
79.581072	2768.228211	21.793536
79.872857	2761.011746	21.798554
79.971725	2748.224608	21.803571
79.811513	2767.991452	21.808589
79.778999	2774.271969	21.813607
80.242154	2761.629515	21.818624
80.072455	2771.239519	21.823642
80.188476	2770.374440	21.828659
79.989355	2769.767904	21.833677
80.225060	2772.975979	21.838695
80.539774	2759.374532	21.843712
80.343316	2794.236230	21.848730
80.622159	2793.250752	21.853747
80.632313	2792.226615	21.858765
80.884366	2799.338737	21.863783
81.066591	2810.623246	21.868800
80.868598	2806.394973	21.873818
81.390263	2786.343063	21.878835
81.194661	2796.013654	21.883853
81.181698	2795.290344	21.888871
81.351628	2784.426205	21.893888
81.590082	2793.029537	21.898906
81.378368	2787.289179	21.903923
81.567289	2808.500142	21.908941
81.644935	2829.779712	21.913959
81.663541	2821.366798	21.918976
81.859553	2817.178911	21.923994
81.870630	2807.429637	21.929011
81.998565	2814.957891	21.934029
82.180987	2826.583080	21.939047
82.180452	2830.605296	21.944064
82.191190	2819.138981	21.949082
82.170686	2815.824160	21.954099
82.408198	2813.749992	21.959117
82.193968	2832.526770	21.964135
82.595054	2834.293745	21.969152
82.507819	2849.254010	21.974170
82.502228	2848.830029	21.979187
82.770932	2852.700097	21.984205
82.726995	2857.809858	21.989223
82.769422	2861.408700	21.994240
82.561521	2863.268833	21.999258
82.705913	2862.110319	22.004275
83.144127	2874.208168	22.009293
82.805378	2875.207561	22.014311
83.249484	2869.776264	22.019328
83.221050	2873.378355	22.024346
83.587125	2879.134448	22.029363
83.736776	2867.458946	22.034381
83.913877	2868.991124	22.039399
83.903410	2860.662707	22.044416
83.516357	2875.272201	22.049434
84.259435	2880.397568	22.054451
84.295281	2883.138365	22.059469
83.909394	2873.997881	22.064487
84.558010	2868.372968	22.069504
84.421690	2896.216842	22.074522
84.372212	2909.083996	22.079539
84.661058	2906.652363	22.084557
84.586205	2895.523124	22.089575
84.727658	2896.908459	22.094592
84.576063	2916.356789	22.099610
85.113288	2895.366855	22.104627
84.730902	2879.643981	22.109645
84.895015	2878.235783	22.114663
85.111830	2888.092578	22.119680
84.937095	2900.228555	22.124698
84.848486	2884.455555	22.129715
84.774013	2880.078915	22.134733
84.638483	2902.902274	22.139751
85.298526	2916.606000	22.144768
85.202801	2903.968590	22.149786
85.347924	2928.784123	22.154803
85.406028	2965.341515	22.159821
85.497958	2957.973952	22.164839
85.538675	2951.740302	22.169856
85.709229	2962.239354	22.174874
85.826269	2949.959611	22.179891
86.173155	2950.709703	22.184909
86.014288	2956.642127	22.189927
86.763881	2973.576361	22.194944
86.620736	2984.360701	22.199962
86.484812	2962.539905	22.204979
86.757313	2964.487965	22.209997
86.635938	2974.145615	22.215015
87.141076	2959.410107	22.220032
87.047492	2956.269516	22.225050
86.852622	2957.174281	22.230067
86.630803	2962.273910	22.235085
86.564658	2986.695171	22.240103
87.056594	2992.598205	22.245120
87.177611	3000.736672	22.250138
87.122125	2983.201427	22.255155
87.131047	2986.275587	22.260173
87.156296	2996.152298	22.265191
87.191023	3000.587576	22.270208
87.762234	3012.225226	22.275226
87.744361	3005.877432	22.280243
87.920223	3023.311006	22.285261
87.962275	3021.428539	22.290279
88.206428	3002.932256	22.295296
88.338231	3015.121199	22.300314
88.328688	3024.507873	22.305331
88.543465	3008.785584	22.310349
88.705183	3005.595906	22.315367
88.642161	2985.778527	22.320384
88.624168	3010.834899	22.325402
88.548375	3018.968698	22.330419
88.553778	3015.267513	22.335437
88.618940	3013.416067	22.340455
89.052143	3030.581365	22.345472
88.988707	3041.656472	22.350490
88.681368	3051.118550	22.355507
88.988226	3040.204639	22.360525
88.973935	3036.076639	22.365543
89.044637	3036.981810	22.370560
89.044246	3057.988799	22.375578
89.194078	3059.109805	22.380595
89.383645	3069.479228	22.385613
89.674206	3075.932635	22.390631
89.363534	3077.062620	22.395648
89.180596	3075.176779	22.400666
89.716368	3085.721654	22.405683
89.835065	3082.086762	22.410701
90.218868	3097.641988	22.415719
90.452446	3105.687706	22.420736
90.539906	3087.573866	22.425754
90.240177	3088.051137	22.430771
90.391443	3094.647240	22.435789
90.520636	3100.596874	22.440807
90.926545	3107.830154	22.445824
90.596565	3105.078358	22.450842
90.802651	3121.644356	22.455859
91.222784	3125.168642	22.460877
90.863188	3115.037761	22.465895
91.127312	3093.688601	22.470912
91.219896	3099.352980	22.475930
91.382691	3115.562388	22.480947
91.292473	3126.117438	22.485965
91.417193	3131.199223	22.490983
91.575878	3124.007340	22.496000
91.812168	3134.318699	22.501018
91.866176	3138.217232	22.506035
92.123722	3134.164350	22.511053
91.763755	3140.202704	22.516071
92.172894	3128.209945	22.521088
92.169368	3138.357612	22.526106
91.960948	3141.622425	22.531123
92.107536	3139.697081	22.536141
91.969048	3163.172026	22.541159
92.368625	3155.154191	22.546176
92.482448	3162.091905	22.551194
92.079141	3173.263422	22.556211
92.590301	3166.631314	22.561229
92.943682	3178.907380	22.566247
92.936293	3201.598207	22.571264
93.078583	3203.955962	22.576282
93.281424	3190.079743	22.581299
93.378538	3181.236187	22.586317
93.371834	3187.913546	22.591335
93.494253	3166.854404	22.596352
93.739037	3179.912698	22.601370
93.526317	3173.122284	22.606387
93.987008	3182.749424	22.611405
93.521614	3201.964370	22.616423
94.121256	3216.753817	22.621440
94.258272	3201.616362	22.626458
94.092528	3203.938807	22.631475
94.429416	3210.941640	22.636493
94.209796	3217.473507	22.641511
94.173495	3199.539023	22.646528
94.573566	3195.558626	22.651546
94.666668	3205.220738	22.656563
94.668219	3188.558216	22.661581
94.563012	3215.449009	22.666599
94.927944	3236.673796	22.671616
94.989417	3231.493771	22.676634
95.073091	3232.181479	22.681651
95.286843	3242.877105	22.686669
94.991286	3231.923448	22.691687
94.972047	3221.909266	22.696704
95.284916	3227.073956	22.701722
95.100995	3211.694282	22.706739
95.324652	3220.444181	22.711757
95.486939	3247.626224	22.716775
95.457938	3257.820104	22.721792
95.731791	3247.547260	22.726810
95.708287	3254.510267	22.731827
95.928601	3255.901893	22.736845
95.629093	3257.622108	22.741863
96.035997	3274.518236	22.746880
96.293428	3291.678033	22.751898
96.118365	3294.098281	22.756915
96.093303	3274.746452	22.761933
96.130531	3312.355052	22.766951
96.476148	3299.766618	22.771968
96.686070	3305.435303	22.776986
96.675143	3317.555167	22.782003
97.236427	3322.617036	22.787021
97.308390	3340.733226	22.792039
97.259361	3336.348708	22.797056
97.680998	3327.741176	22.802074
97.376709	3344.029583	22.807091
97.802464	3334.599995	22.812109
97.934774	3335.518623	22.817127
98.055973	3334.155465	22.822144
97.841610	3327.616802	22.827162
98.033511	3325.863457	22.832179
97.656685	3331.937935	22.837197
97.777168	3336.119598	22.842215
97.707023	3340.150497	22.847232
98.369782	3334.206186	22.852250
98.209693	3352.487494	22.857267
98.355534	3359.348951	22.862285
98.679613	3367.293443	22.867303
98.282762	3357.190406	22.872320
98.768788	3361.587627	22.877338
98.493144	3373.979405	22.882355
98.777459	3387.370483	22.887373
98.874658	3385.730015	22.892391
99.122331	3393.786349	22.897408
99.274540	3395.779341	22.902426
99.408985	3388.367544	22.907443
99.553474	3387.402067	22.912461
99.847243	3423.112235	22.917479
99.803441	3414.630380	22.922496
99.990534	3407.101224	22.927514
99.792243	3418.264824	22.932531
100.155312	3399.954892	22.937549
100.315470	3415.076380	22.942567
100.138335	3413.620401	22.947584
100.590276	3398.617703	22.952602
100.205569	3391.135998	22.957619
100.391233	3411.582463	22.962637
100.164531	3433.929792	22.967655
100.584419	3428.302520	22.972672
100.881923	3426.496481	22.977690
100.733309	3446.823443	22.982707
100.936908	3429.262397	22.987725
101.393443	3442.669942	22.992743
100.929527	3454.196524	22.997760
101.228662	3434.944057	23.002778
101.354604	3450.612127	23.007795
101.518292	3453.696038	23.012813
101.574898	3471.187027	23.017831
101.709056	3467.079456	23.022848
101.896232	3457.835660	23.027866
101.909246	3471.916462	23.032883
102.132518	3455.457149	23.037901
102.175737	3459.776798	23.042919
102.024495	3466.558665	23.047936
102.270614	3443.202150	23.052954
102.007548	3462.654431	23.057971
102.031646	3479.057991	23.062989
102.582964	3481.087987	23.068007
102.358665	3479.079415	23.073024
102.775036	3494.084437	23.078042
102.263334	3509.185948	23.083059
102.741337	3491.664125	23.088077
103.099878	3497.748833	23.093095
103.089725	3507.422489	23.098112
103.373779	3518.672189	23.103130
103.075785	3519.035219	23.108147
103.405016	3504.849671	23.113165
103.210996	3526.741381	23.118183
103.459434	3542.568617	23.123200
103.313814	3532.547560	23.128218
103.538620	3554.549022	23.133235
103.731915	3567.263232	23.138253
103.825238	3563.534200	23.143271
103.923584	3551.559010	23.148288
104.489882	3568.497424	23.153306
104.029624	3582.116029	23.158323
104.755648	3579.446515	23.163341
104.770603	3585.807896	23.168359
105.016025	3600.154912	23.173376
105.152507	3583.926912	23.178394
105.122491	3591.515305	23.183411
105.312410	3592.777942	23.188429
105.584532	3590.567649	23.193447
105.540594	3593.440053	23.198464
105.493343	3587.950738	23.203482
105.443974	3583.757724	23.208499
105.917705	3585.786580	23.213517
105.877933	3589.993415	23.218535
105.711758	3584.348177	23.223552
105.935865	3577.464537	23.228570
105.754015	3569.122524	23.233587
105.975925	3598.066633	23.238605
106.181422	3616.193363	23.243623
105.945137	3602.707420	23.248640
106.428772	3611.398836	23.253658
106.434067	3614.552060	23.258675
106.437413	3615.879975	23.263693
106.714938	3631.615495	23.268711
106.541229	3644.713026	23.273728
107.036686	3635.175683	23.278746
106.722627	3640.432889	23.283763
106.733271	3653.963705	23.288781
107.056035	3657.553021	23.293799
107.336267	3663.771591	23.298816
107.239275	3674.062013	23.303834
107.389839	3681.745995	23.308851
107.549258	3697.679037	23.313869
108.005425	3704.344498	23.318887
108.229699	3696.573839	23.323904
108.285761	3683.348352	23.328922
108.352462	3700.204912	23.333939
108.241869	3693.185204	23.338957
108.313782	3691.310909	23.343975
108.316647	3693.368970	23.348992
108.580806	3711.197557	23.354010
108.372419	3708.646604	23.359027
108.606153	3709.486098	23.364045
108.998667	3701.395534	23.369063
108.635557	3721.382740	23.374080
108.816825	3720.782790	23.379098
109.212085	3717.773847	23.384115
108.920008	3722.856596	23.389133
109.369530	3727.486711	23.394151
109.083983	3750.713641	23.399168
109.744345	3751.975910	23.404186
109.389369	3769.513202	23.409203
109.467529	3757.857306	23.414221
109.579758	3747.473447	23.419239
109.696788	3781.116368	23.424256
109.571808	3787.290538	23.429274
110.101469	3791.581469	23.434291
110.673658	3793.892882	23.439309
110.723208	3801.687505	23.444327
110.719496	3807.973722	23.449344
110.878676	3794.960807	23.454362
110.730019	3801.320181	23.459379
110.926006	3814.429003	23.464397
111.106380	3806.584448	23.469415
110.913013	3797.840307	23.474432
111.158088	3806.674396	23.479450
111.357629	3831.285750	23.484467
111.566178	3820.902067	23.489485
111.808214	3826.056619	23.494503
111.727995	3829.729099	23.499520
111.814110	3821.953258	23.504538
111.967018	3828.640540	23.509555
111.804930	3835.592853	23.514573
112.260798	3852.925195	23.519591
112.087896	3862.561207	23.524608
112.696679	3839.389229	23.529626
112.653981	3848.663977	23.534643
112.601797	3861.478438	23.539661
112.911702	3832.948555	23.544679
112.971238	3838.678506	23.549696
112.979292	3854.222578	23.554714
113.213084	3887.484060	23.559731
113.316433	3892.789496	23.564749
113.640821	3874.182858	23.569767
113.083814	3896.381708	23.574784
113.265825	3880.005135	23.579802
113.592556	3879.833868	23.584819
113.791940	3895.767794	23.589837
113.939644	3910.024954	23.594855
114.010838	3920.395812	23.599872
113.983475	3903.568214	23.604890
114.300439	3895.574870	23.609907
114.401305	3918.344919	23.614925
114.417249	3916.835531	23.619943
114.582207	3922.476049	23.624960
114.777884	3905.152962	23.629978
114.839857	3908.785628	23.634995
114.721857	3933.056137	23.640013
115.088780	3941.456023	23.645031
114.578837	3936.630404	23.650048
115.096460	3938.155041	23.655066
115.205793	3945.229865	23.660083
115.182108	3965.527022	23.665101
115.347324	3954.209524	23.670119
115.482362	3974.275360	23.675136
115.582740	3978.030231	23.680154
115.647599	3974.104439	23.685171
116.080144	3965.609117	23.690189
116.271867	3974.673758	23.695207
116.541958	3975.250780	23.700224
116.591830	3971.089291	23.705242
116.785808	3966.540234	23.710259
116.362702	3987.227416	23.715277
116.764414	3977.656540	23.720295
116.784352	3971.688691	23.725312
116.903251	3999.323295	23.730330
116.792549	3997.875571	23.735347
117.156219	3990.500211	23.740365
117.272633	3980.794203	23.745383
117.121381	3983.428916	23.750400
117.478374	4011.026166	23.755418
117.647578	4020.434692	23.760435
117.688686	4021.266864	23.765453
117.780179	4020.642764	23.770471
117.739569	4039.817685	23.775488
117.689593	4030.802882	23.780506
117.949447	4043.707263	23.785523
118.129929	4063.752321	23.790541
118.497203	4048.370490	23.795559
118.084392	4057.277215	23.800576
118.538940	4075.998334	23.805594
118.502580	4084.272428	23.810611
118.576267	4080.036112	23.815629
118.977512	4092.529003	23.820647
119.520267	4115.265691	23.825664
119.325281	4125.848575	23.830682
119.578540	4115.608874	23.835699
119.796713	4102.130269	23.840717
119.987230	4105.060871	23.845735
120.202551	4109.286518	23.850752
120.256950	4111.014089	23.855770
120.328147	4106.408512	23.860787
120.112471	4106.594180	23.865805
120.372192	4100.586659	23.870823
120.438249	4106.956148	23.875840
120.259765	4134.596828	23.880858
120.644587	4142.026200	23.885875
120.532292	4143.944696	23.890893
120.569918	4123.606101	23.895911
120.518771	4158.746258	23.900928
120.911834	4152.415912	23.905946
121.039251	4143.885877	23.910963
120.805920	4162.854620	23.915981
121.366273	4193.351122	23.920999
121.343899	4187.444905	23.926016
121.698823	4192.379755	23.931034
121.906476	4186.876451	23.936051
122.165287	4199.140614	23.941069
121.983167	4185.763513	23.946087
122.127087	4199.073776	23.951104
122.644977	4221.898191	23.956122
123.117916	4219.785528	23.961139
122.817275	4204.028893	23.966157
123.134785	4201.923806	23.971175
122.938439	4212.010934	23.976192
122.900638	4217.687033	23.981210
123.269077	4212.985066	23.986227
123.107481	4214.076717	23.991245
123.573639	4223.513854	23.996263
123.454868	4234.604274	24.001280
123.367958	4248.406639	24.006298
123.659842	4227.772362	24.011315
123.176265	4242.546132	24.016333
123.464838	4250.190270	24.021351
123.701812	4275.787835	24.026368
124.135596	4276.920473	24.031386
124.155183	4265.750428	24.036403
123.886942	4264.632636	24.041421
124.317642	4285.733439	24.046439
124.647863	4293.053013	24.051456
124.520238	4302.900507	24.056474
124.898153	4307.744985	24.061491
124.789026	4311.551485	24.066509
125.026507	4321.405981	24.071527
125.021187	4325.030377	24.076544
125.279465	4332.374456	24.081562
125.409978	4311.830116	24.086579
125.203287	4321.017485	24.091597
125.667997	4338.073924	24.096615
125.860683	4352.706525	24.101632
125.824431	4354.442410	24.106650
126.168742	4343.924530	24.111667
126.145341	4353.274932	24.116685
126.550779	4377.288587	24.121703
126.737377	4382.983964	24.126720
126.611245	4368.258131	24.131738
126.840557	4375.836930	24.136755
126.418580	4397.324836	24.141773
126.651573	4381.480630	24.146791
126.844598	4381.579870	24.151808
127.211502	4398.654899	24.156826
127.366569	4413.883911	24.161843
127.545312	4425.745357	24.166861
127.442292	4414.878527	24.171879
127.780276	4415.545132	24.176896
127.945002	4443.228071	24.181914
128.044705	4445.787143	24.186931
128.194641	4438.200047	24.191949
128.225630	4451.818943	24.196967
128.335862	4464.236604	24.201984
128.392044	4469.321299	24.207002
128.165923	4456.317759	24.212019
128.489870	4476.980178	24.217037
128.702727	4475.077775	24.222055
129.193780	4477.412741	24.227072
128.951430	4505.566982	24.232090
129.395112	4492.360610	24.237107
129.502706	4514.832401	24.242125
129.734385	4522.972283	24.247143
129.722878	4505.697131	24.252160
129.871689	4506.509170	24.257178
129.811252	4506.327073	24.262195
130.032881	4536.706608	24.267213
130.408532	4545.319549	24.272231
130.580414	4527.428652	24.277248
130.382903	4536.080787	24.282266
130.777272	4550.751902	24.287283
130.583587	4556.156252	24.292301
130.866295	4535.103015	24.297319
131.062230	4539.405211	24.302336
131.330413	4563.941430	24.307354
130.933092	4554.748683	24.312371
131.105072	4558.697765	24.317389
131.074051	4584.373193	24.322407
131.864632	4577.761247	24.327424
131.776786	4591.701077	24.332442
132.100553	4589.703170	24.337459
132.134802	4584.681125	24.342477
132.438806	4573.429217	24.347495
132.679367	4605.404934	24.352512
132.625668	4624.968560	24.357530
132.983342	4598.366347	24.362547
132.960263	4608.502266	24.367565
132.860120	4615.260443	24.372583
133.151000	4604.776020	24.377600
132.934073	4612.886142	24.382618
132.992200	4603.235439	24.387635
133.343073	4600.961798	24.392653
133.291114	4635.097283	24.397671
133.589276	4639.392458	24.402688
133.510250	4633.912745	24.407706
134.075665	4638.961381	24.412723
133.793674	4652.278240	24.417741
133.600834	4668.188995	24.422759
134.102028	4671.114038	24.427776
134.261383	4656.275798	24.432794
134.521397	4661.329237	24.437811
134.663309	4695.864310	24.442829
134.840914	4690.661458	24.447847
134.707595	4680.122671	24.452864
134.991810	4687.070908	24.457882
135.311010	4689.451627	24.462899
135.377884	4696.823570	24.467917
135.725828	4710.787559	24.472935
135.559435	4719.447252	24.477952
135.742587	4724.642938	24.482970
135.909154	4709.076694	24.487987
135.785620	4714.623049	24.493005
135.825417	4746.449950	24.498023
136.613656	4753.618471	24.503040
136.616428	4758.047527	24.508058
136.548843	4739.373917	24.513075
136.691296	4747.279058	24.518093
136.542057	4770.419635	24.523111
137.098670	4769.063145	24.528128
136.856773	4764.645721	24.533146
137.370991	4750.084578	24.538163
137.197692	4782.271956	24.543181
137.626735	4782.993218	24.548199
137.854420	4791.466182	24.553216
137.781405	4805.556900	24.558234
138.004550	4812.623158	24.563251
138.026425	4821.890770	24.568269
138.161679	4834.967975	24.573287
138.475331	4824.412713	24.578304
138.496743	4827.688323	24.583322
138.567312	4813.529560	24.588339
138.979464	4855.782480	24.593357
138.773831	4864.934563	24.598375
139.066745	4858.394892	24.603392
139.144150	4851.406978	24.608410
139.340016	4848.498682	24.613427
139.485842	4863.087935	24.618445
139.404590	4871.812384	24.623463
139.862662	4883.691411	24.628480
139.954107	4888.256638	24.633498
139.688160	4882.349065	24.638515
140.117382	4888.226191	24.643533
140.166141	4907.432299	24.648551
140.636822	4923.476195	24.653568
140.725272	4930.986416	24.658586
140.911293	4924.194696	24.663603
141.035799	4921.372194	24.668621
141.166215	4938.916817	24.673639
141.290076	4954.601518	24.678656
141.146493	4951.001261	24.683674
141.078231	4943.228714	24.688691
141.329212	4964.855023	24.693709
141.543160	4966.105143	24.698727
142.275452	4949.406989	24.703744
141.784517	4979.073636	24.708762
141.844906	4992.450352	24.713779
142.246433	5002.373846	24.718797
142.093541	5009.053114	24.723815
142.282181	5004.987317	24.728832
142.364116	5005.161612	24.733850
142.672249	5009.671779	24.738867
143.196862	5026.872625	24.743885
143.224745	5028.949563	24.748903
143.331248	5014.527591	24.753920
143.164290	5037.417949	24.758938
143.455329	5041.697090	24.763955
143.714763	5029.169139	24.768973
143.668949	5052.078871	24.773991
143.692046	5066.825603	24.779008
144.058732	5070.902487	24.784026
144.195746	5072.079896	24.789043
144.235208	5072.867120	24.794061
144.653221	5101.163717	24.799079
144.942117	5097.859291	24.804096
144.572483	5094.151863	24.809114
144.329432	5091.785738	24.814131
144.993508	5115.041652	24.819149
145.122989	5127.953127	24.824167
145.587235	5131.459175	24.829184
145.697334	5128.480353	24.834202
145.537306	5139.911704	24.839219
145.818103	5152.705281	24.844237
146.082116	5154.278252	24.849255
146.480943	5137.074361	24.854272
146.174374	5157.959985	24.859290
146.355464	5171.715737	24.864307
146.601885	5178.591305	24.869325
146.694010	5175.438275	24.874343
146.715957	5187.785276	24.879360
147.203812	5184.848750	24.884378
147.289714	5189.850422	24.889395
147.405627	5205.792994	24.894413
147.451398	5216.462823	24.899431
147.675512	5205.827215	24.904448
147.757649	5198.368671	24.909466
147.895194	5224.561407	24.914483
148.489956	5247.049825	24.919501
148.176135	5239.397234	24.924519
148.570802	5219.898619	24.929536
148.488459	5232.182571	24.934554
148.470177	5254.170316	24.939571
149.080065	5253.106960	24.944589
148.819751	5245.971519	24.949607
148.936427	5255.023328	24.954624
148.957743	5268.007123	24.959642
148.835677	5291.713288	24.964659
149.200182	5287.640012	24.969677
149.537421	5312.450263	24.974695
149.960757	5306.886910	24.979712
150.304659	5308.217557	24.984730
150.601382	5302.310946	24.989747
150.659926	5300.004405	24.994765
150.447524	5314.293030	24.999783
150.895261	5330.404920	25.004800
151.035212	5356.780951	25.009818
150.890899	5343.119824	25.014835
151.341643	5330.137175	25.019853
150.944484	5344.527223	25.024871
151.303100	5357.032120	25.029888
151.506686	5366.989736	25.034906
151.547861	5359.766630	25.039923
151.764308	5362.987291	25.044941
151.809372	5388.753840	25.049959
152.085854	5394.078035	25.054976
152.426420	5392.501675	25.059994
152.229659	5380.538995	25.065011
152.815509	5398.706542	25.070029
152.945427	5410.327196	25.075047
152.984325	5386.155520	25.080064
152.975292	5398.273154	25.085082
153.025466	5436.059772	25.090099
153.268118	5425.076059	25.095117
153.358124	5417.489728	25.100135
153.551195	5421.711539	25.105152
153.895590	5455.133705	25.110170
153.878897	5460.053201	25.115187
154.105361	5451.926572	25.120205
153.969048	5458.648963	25.125223
154.282066	5470.132711	25.130240
154.413514	5478.800306	25.135258
154.031939	5484.866754	25.140275
154.505613	5495.479455	25.145293
154.825103	5520.426834	25.150311
155.240836	5503.773704	25.155328
155.184730	5504.347207	25.160346
155.428776	5518.029080	25.165363
155.492319	5539.065877	25.170381
155.513442	5533.222435	25.175399
155.846259	5544.991954	25.180416
156.163464	5577.547582	25.185434
155.993009	5575.122534	25.190451
156.231232	5559.062086	25.195469
156.483938	5573.330002	25.200487
156.542500	5600.959710	25.205504
156.837550	5591.868091	25.210522
156.535399	5594.557930	25.215539
157.213127	5606.129552	25.220557
157.581328	5631.225760	25.225575
157.734382	5632.020229	25.230592
157.626016	5626.674154	25.235610
157.737214	5642.122654	25.240627
158.107472	5640.518134	25.245645
158.456127	5627.022951	25.250663
158.592442	5649.994416	25.255680
158.855824	5659.886039	25.260698
158.868425	5632.212652	25.265715
158.714270	5622.616080	25.270733
158.690435	5667.041372	25.275751
158.838303	5684.620176	25.280768
159.176023	5680.046870	25.285786
159.351842	5683.325101	25.290803
159.755699	5684.365154	25.295821
159.833056	5701.368591	25.300839
159.822062	5686.176792	25.305856
160.155206	5702.246190	25.310874
160.198109	5730.974045	25.315891
160.371626	5735.190905	25.320909
160.538873	5744.766559	25.325927
160.668752	5729.681762	25.330944
161.007254	5740.823293	25.335962
161.074552	5761.912529	25.340979
161.476458	5770.695055	25.345997
161.278603	5768.340255	25.351015
161.166206	5772.284666	25.356032
161.530939	5771.731497	25.361050
161.769204	5786.218936	25.366067
161.887814	5803.508992	25.371085
162.398565	5804.516429	25.376103
162.616937	5793.366381	25.381120
162.512035	5803.803227	25.386138
162.943916	5814.666375	25.391155
162.906964	5811.394774	25.396173
163.077231	5825.960025	25.401191
163.320429	5838.393431	25.406208
163.587425	5846.645110	25.411226
162.997420	5846.875716	25.416243
163.204694	5840.112372	25.421261
163.265366	5848.612724	25.426279
163.750437	5870.684713	25.431296
164.080915	5891.442825	25.436314
164.004056	5884.249609	25.441331
164.349934	5878.169296	25.446349
164.199470	5915.245301	25.451367
164.286364	5931.826127	25.456384
164.555768	5917.945732	25.461402
164.296949	5934.643531	25.466419
164.535994	5950.504705	25.471437
165.158616	5960.517880	25.476455
165.059605	5962.663946	25.481472
165.441956	5970.490698	25.486490
165.585186	5989.052173	25.491507
165.809678	5994.135543	25.496525
166.380742	6011.193183	25.501543
166.364674	6016.758465	25.506560
166.906095	6010.840686	25.511578
167.110716	6030.415759	25.516595
167.004960	6033.853984	25.521613
167.257751	6037.819621	25.526631
167.125252	6032.690795	25.531648
167.660131	6053.262976	25.536666
167.517132	6060.855297	25.541683
167.883432	6052.531222	25.546701
168.417391	6072.269662	25.551719
168.215626	6089.214124	25.556736
168.469296	6096.631856	25.561754
168.680058	6082.681077	25.566771
168.810628	6061.139860	25.571789
168.853300	6080.979569	25.576807
168.714913	6094.014064	25.581824
169.140870	6100.490270	25.586842
168.946716	6108.769858	25.591859
169.347750	6112.847251	25.596877
169.370688	6126.886298	25.601895
169.502544	6130.174250	25.606912
169.785997	6132.948928	25.611930
169.981564	6141.068067	25.616947
170.163900	6161.583674	25.621965
170.413173	6169.611664	25.626983
170.288202	6207.898026	25.632000
170.818045	6187.347048	25.637018
170.913953	6181.989078	25.642035
171.222702	6204.773407	25.647053
171.514727	6223.892119	25.652071
171.718777	6227.767426	25.657088
171.724013	6209.658808	25.662106
171.445764	6223.268141	25.667123
171.723151	6261.377512	25.672141
171.951590	6266.550091	25.677159
171.976552	6255.529319	25.682176
172.561670	6258.020296	25.687194
172.636146	6273.979863	25.692212
172.544672	6288.923863	25.697229
172.896901	6309.905337	25.702247
172.872774	6327.042377	25.707264
173.188481	6320.164444	25.712282
173.643722	6327.871056	25.717300
173.899837	6329.684059	25.722317
173.960740	6341.347523	25.727335
174.117759	6353.690846	25.732352
174.369042	6345.612807	25.737370
174.162876	6356.145895	25.742388
174.491783	6354.772568	25.747405
174.808154	6361.874921	25.752423
174.970800	6387.050016	25.757440
175.184153	6376.836297	25.762458
175.268430	6377.629571	25.767476
175.396128	6397.104812	25.772493
175.775511	6402.135161	25.777511
175.369051	6409.491629	25.782528
175.924359	6417.003387	25.787546
175.808449	6418.286870	25.792564
175.657919	6426.122761	25.797581
176.196181	6437.150675	25.802599
175.982160	6454.800774	25.807616
176.424740	6482.977310	25.812634
176.406457	6492.215146	25.817652
176.733994	6498.343571	25.822669
177.080821	6510.310740	25.827687
177.117818	6533.651526	25.832704
177.604191	6547.758486	25.837722
177.611323	6548.772411	25.842740
177.862196	6559.174993	25.847757
178.249549	6562.337347	25.852775
178.343357	6561.761590	25.857792
178.789179	6563.042435	25.862810
178.868319	6574.808582	25.867828
179.357649	6586.356552	25.872845
179.530249	6590.082012	25.877863
179.466020	6603.905944	25.882880
179.575427	6610.297646	25.887898
179.573202	6619.113960	25.892916
180.130383	6611.058872	25.897933
180.461113	6627.343033	25.902951
180.161002	6637.395321	25.907968
180.208242	6629.279584	25.912986
180.323662	6643.138441	25.918004
180.555325	6640.894448	25.923021
180.846502	6664.829328	25.928039
180.776728	6672.072800	25.933056
180.897310	6677.473596	25.938074
180.964229	6684.807099	25.943092
181.280264	6715.069762	25.948109
181.781786	6740.032721	25.953127
182.192087	6751.156420	25.958144
182.162474	6740.583352	25.963162
182.026655	6762.460736	25.968180
182.568429	6771.705815	25.973197
182.833341	6767.862421	25.978215
183.198946	6772.117517	25.983232
183.421544	6758.431537	25.988250
183.572623	6796.364634	25.993268
183.882573	6814.497526	25.998285
184.163671	6798.247207	26.003303
183.976146	6810.800988	26.008320
184.301816	6802.567888	26.013338
184.302478	6808.283855	26.018356
184.500263	6820.400313	26.023373
184.482989	6836.077152	26.028391
184.402397	6828.788044	26.033408
184.880925	6840.150563	26.038426
185.063868	6860.410657	26.043444
185.481184	6873.030712	26.048461
185.828822	6877.740043	26.053479
185.392463	6905.178601	26.058496
185.621335	6906.536667	26.063514
186.160597	6901.752522	26.068532
186.455955	6908.849540	26.073549
186.372968	6915.069587	26.078567
186.398488	6929.345178	26.083584
186.914059	6949.622483	26.088602
187.193716	6957.557659	26.093620
186.827623	6970.974252	26.098637
187.206991	6962.041162	26.103655
187.290349	6971.567643	26.108672
187.645995	6988.058328	26.113690
187.506536	7006.200729	26.118708
187.690960	7009.876692	26.123725
187.992269	7021.350132	26.128743
188.553396	7027.441746	26.133760
188.840616	7048.151451	26.138778
188.874048	7053.628597	26.143796
188.673049	7036.222482	26.148813
189.311928	7047.882717	26.153831
189.148951	7065.634532	26.158848
189.502771	7070.869744	26.163866
189.583029	7085.415604	26.168884
189.709305	7102.601092	26.173901
190.046224	7102.842745	26.178919
190.190176	7124.807497	26.183936
190.473559	7144.639494	26.188954
190.461087	7152.085166	26.193972
190.783644	7157.832732	26.198989
190.908982	7154.125709	26.204007
191.269363	7158.671186	26.209024
191.126195	7175.098009	26.214042
191.795255	7192.370314	26.219060
191.527858	7208.296364	26.224077
192.207958	7227.653014	26.229095
192.341466	7223.044493	26.234112
192.462761	7213.351816	26.239130
192.807415	7225.791615	26.244148
192.920146	7246.607590	26.249165
193.230809	7248.704646	26.254183
193.280433	7256.110182	26.259200
193.775638	7289.426306	26.264218
193.672784	7276.646927	26.269236
193.903173	7275.404780	26.274253
194.177338	7278.291453	26.279271
194.039613	7304.000796	26.284288
194.368214	7317.178471	26.289306
194.441242	7321.641141	26.294324
194.605641	7323.788362	26.299341
194.882407	7335.486989	26.304359
194.944585	7378.068390	26.309376
195.530385	7371.998263	26.314394
195.556117	7359.496830	26.319412
195.689692	7398.466719	26.324429
196.241843	7389.507989	26.329447
196.096224	7409.641556	26.334464
195.887199	7427.334841	26.339482
196.429870	7442.623263	26.344500
196.655511	7444.116972	26.349517
196.922287	7445.453467	26.354535
197.256869	7466.793798	26.359552
197.183981	7479.700885	26.364570
197.617818	7481.364168	26.369588
197.585803	7499.610272	26.374605
197.898752	7514.835917	26.379623
198.096278	7519.718302	26.384640
198.341926	7511.944979	26.389658
198.605668	7517.562215	26.394676
198.507895	7550.001119	26.399693
198.781446	7557.017770	26.404711
199.063320	7564.813495	26.409728
199.052353	7575.078491	26.414746
199.253322	7579.210593	26.419764
199.484159	7614.921882	26.424781
199.746505	7614.368248	26.429799
199.869860	7612.082949	26.434816
200.024607	7641.615260	26.439834
200.635782	7654.512632	26.444852
200.363281	7656.471413	26.449869
200.849155	7656.137583	26.454887
201.089069	7655.782176	26.459904
201.104620	7670.182944	26.464922
201.271064	7679.445296	26.469940
201.513168	7684.062842	26.474957
201.921095	7695.351021	26.479975
201.804860	7722.285272	26.484992
202.079494	7740.102967	26.490010
202.551002	7731.255812	26.495028
202.295882	7762.348464	26.500045
202.694025	7777.626442	26.505063
203.246399	7778.565320	26.510080
203.109003	7778.580972	26.515098
203.485381	7780.927920	26.520116
203.488886	7798.596744	26.525133
203.685697	7813.819818	26.530151
203.819255	7826.048078	26.535168
204.177314	7835.111114	26.540186
204.772366	7851.737988	26.545204
204.707274	7861.117459	26.550221
205.023803	7879.867149	26.555239
205.242916	7884.574395	26.560256
205.177327	7878.448682	26.565274
205.809568	7906.960687	26.570292
205.387496	7931.164985	26.575309
206.010609	7929.193993	26.580327
206.009783	7948.323034	26.585344
206.001936	7954.179828	26.590362
206.495699	7950.846474	26.595380
206.455818	7983.240476	26.600397
206.711670	7991.268317	26.605415
207.219881	8005.899075	26.610432
207.263970	8006.713249	26.615450
207.753947	8025.699861	26.620468
207.838621	8032.611686	26.625485
208.494754	8021.751582	26.630503
208.516097	8035.030246	26.635520
208.788750	8041.200639	26.640538
209.197068	8049.693967	26.645556
209.291831	8070.971574	26.650573
209.218458	8075.042816	26.655591
209.374193	8080.776546	26.660608
209.299942	8075.973711	26.665626
209.651066	8102.897547	26.670644
209.933839	8137.735125	26.675661
210.263979	8122.805925	26.680679
210.748175	8135.260801	26.685696
210.573002	8146.273133	26.690714
210.567664	8154.704917	26.695732
210.547843	8170.414616	26.700749
211.146877	8181.042306	26.705767
211.602814	8177.653726	26.710784
211.660682	8219.445039	26.715802
211.978491	8232.131463	26.720820
212.057561	8227.769489	26.725837
212.456135	8218.837243	26.730855
212.884266	8242.918081	26.735872
212.826944	8255.824807	26.740890
213.162492	8257.259483	26.745908
213.164479	8254.272732	26.750925
213.142697	8266.257652	26.755943
213.542022	8292.857247	26.760960
213.350608	8306.153965	26.765978
213.926363	8291.810143	26.770996
213.671577	8300.372217	26.776013
213.978893	8317.484229	26.781031
214.638350	8333.188965	26.786048
214.533145	8357.428981	26.791066
214.826612	8349.614269	26.796084
215.057503	8362.642002	26.801101
215.341483	8398.535306	26.806119
215.837405	8398.029689	26.811136
215.748710	8389.920540	26.816154
216.060709	8414.609936	26.821172
216.164420	8445.930537	26.826189
216.328995	8438.600173	26.831207
216.599823	8448.192265	26.836224
216.689019	8462.290185	26.841242
216.974177	8461.969029	26.846260
217.034064	8467.864439	26.851277
217.275146	8497.660532	26.856295
217.241537	8505.882954	26.861312
217.730474	8524.896332	26.866330
218.062174	8541.424111	26.871348
217.988612	8568.730796	26.876365
218.282503	8571.124574	26.881383
218.828600	8579.421369	26.886400
218.753310	8624.333326	26.891418
219.313521	8623.046033	26.896436
219.525090	8625.822012	26.901453
219.624247	8627.380053	26.906471
219.780068	8647.985202	26.911488
220.148455	8666.643778	26.916506
220.583772	8676.041863	26.921524
220.588827	8702.842759	26.926541
220.952535	8699.259022	26.931559
221.517064	8712.167337	26.936576
220.991609	8728.746364	26.941594
221.364312	8713.129884	26.946612
221.674538	8747.537399	26.951629
222.022341	8766.142788	26.956647
222.146212	8775.853085	26.961664
222.311696	8795.532195	26.966682
222.763754	8808.908889	26.971700
222.807587	8817.450255	26.976717
222.974120	8832.351677	26.981735
223.540313	8846.574328	26.986752
223.510590	8864.850773	26.991770
223.871879	8857.607428	26.996788
223.654326	8886.896424	27.001805
223.921220	8907.889174	27.006823
224.457839	8906.345062	27.011840
224.612404	8934.917379	27.016858
225.137990	8924.264894	27.021876
225.074021	8929.381525	27.026893
225.270345	8978.224638	27.031911
225.948911	8971.743203	27.036928
225.806508	8975.170795	27.041946
226.032607	8977.627031	27.046964
225.953222	9007.694414	27.051981
226.466840	9031.124373	27.056999
226.792041	9029.465535	27.062016
226.800628	9025.408766	27.067034
227.236283	9046.756594	27.072052
227.250809	9072.920953	27.077069
227.626098	9082.741908	27.082087
227.992806	9085.159965	27.087104
228.171900	9104.632432	27.092122
228.786042	9098.846812	27.097140
229.039656	9093.100284	27.102157
228.990840	9104.909944	27.107175
229.189402	9106.368121	27.112192
229.118952	9121.621653	27.117210
229.359309	9134.687055	27.122228
229.450823	9141.775449	27.127245
229.391606	9162.011178	27.132263
230.094942	9162.665294	27.137280
230.098263	9179.022741	27.142298
230.514297	9205.561257	27.147316
230.589793	9208.859958	27.152333
230.429482	9238.775752	27.157351
230.750332	9246.591866	27.162368
230.713540	9268.561511	27.167386
231.052096	9270.597527	27.172404
231.589413	9298.959190	27.177421
231.529911	9337.482173	27.182439
231.889404	9342.871587	27.187456
232.105725	9353.779116	27.192474
232.333436	9368.474030	27.197492
232.908869	9377.038921	27.202509
233.188087	9388.629979	27.207527
233.347713	9424.535923	27.212544
233.731741	9449.836474	27.217562
234.311452	9454.157748	27.222580
234.348793	9451.813936	27.227597
234.482004	9477.044917	27.232615
234.864629	9482.473088	27.237632
234.929402	9490.541931	27.242650
235.201822	9496.813752	27.247668
235.265759	9502.323728	27.252685
235.314878	9527.735661	27.257703
235.735587	9551.674801	27.262720
235.826614	9566.842221	27.267738
236.095412	9592.953612	27.272756
236.856642	9605.106325	27.277773
236.734002	9606.316743	27.282791
236.977227	9612.503644	27.287808
237.360899	9648.243905	27.292826
237.658013	9643.254788	27.297844
238.005918	9672.919665	27.302861
237.955034	9670.959012	27.307879
238.100056	9680.530110	27.312896
238.474077	9715.270238	27.317914
238.680312	9715.643412	27.322932
239.011356	9744.073035	27.327949
239.230820	9752.145595	27.332967
239.440081	9752.398548	27.337984
239.755725	9775.463774	27.343002
239.889561	9805.175294	27.348020
240.066661	9818.125688	27.353037
240.024566	9822.935749	27.358055
240.653081	9818.398280	27.363072
240.782501	9857.991655	27.368090
241.087607	9881.083192	27.373108
241.575496	9885.531605	27.378125
241.243646	9909.706684	27.383143
241.597597	9927.672065	27.388160
241.785006	9954.342554	27.393178
242.160388	9962.480828	27.398196
242.605480	9986.495363	27.403213
243.070507	9986.686370	27.408231
243.142141	9983.090744	27.413248
243.373584	10003.316541	27.418266
243.210387	10030.255390	27.423284
244.058851	10036.886730	27.428301
243.885541	10067.347352	27.433319
244.374464	10071.835817	27.438336
244.807196	10070.261505	27.443354
244.656481	10105.072645	27.448372
245.073077	10091.912151	27.453389
244.954857	10105.232152	27.458407
245.479864	10129.676365	27.463424
245.545733	10145.021780	27.468442
245.731404	10158.387710	27.473460
246.224495	10146.685100	27.478477
246.166235	10184.278128	27.483495
246.621233	10206.375759	27.488512
247.164416	10221.146944	27.493530
247.090793	10239.922154	27.498548
247.747574	10217.473089	27.503565
247.595285	10250.838653	27.508583
247.841997	10276.323109	27.513600
247.895175	10275.180905	27.518618
248.301957	10292.210885	27.523636
248.633125	10307.407864	27.528653
248.921107	10334.145080	27.533671
249.490581	10328.226983	27.538688
249.230806	10336.612960	27.543706
249.433985	10363.322490	27.548724
249.790193	10375.664020	27.553741
250.080468	10404.988486	27.558759
250.313144	10409.331131	27.563776
250.400570	10406.367667	27.568794
250.583956	10444.572004	27.573812
251.201443	10467.329220	27.578829
251.478139	10485.022858	27.583847
251.748217	10475.432390	27.588864
252.160463	10501.738189	27.593882
252.161707	10523.477220	27.598900
252.519628	10528.767266	27.603917
252.346331	10534.001723	27.608935
253.059933	10555.607349	27.613952
253.309303	10580.905174	27.618970
253.491952	10603.966009	27.623988
254.137315	10593.753422	27.629005
254.167196	10597.935067	27.634023
254.436218	10637.150497	27.639040
254.841676	10643.772582	27.644058
254.874603	10660.242453	27.649076
255.237680	10651.351736	27.654093
255.376815	10675.926711	27.659111
255.686767	10684.702381	27.664128
255.745016	10705.540578	27.669146
255.941579	10711.671817	27.674164
256.217324	10716.785670	27.679181
256.367770	10747.185436	27.684199
256.582179	10787.191649	27.689216
256.809448	10785.388914	27.694234
256.731074	10801.151854	27.699252
257.194345	10823.198565	27.704269
257.503496	10858.069279	27.709287
257.719331	10855.732791	27.714304
257.951720	10894.650856	27.719322
258.272510	10920.182395	27.724340
258.800285	10931.249081	27.729357
258.814625	10962.488592	27.734375
259.138573	10979.409326	27.739392
259.500001	10978.772262	27.744410
259.548631	11005.257126	27.749428
260.207531	11018.581040	27.754445
260.379400	11038.533636	27.759463
260.786844	11058.117286	27.764480
260.978662	11064.110021	27.769498
261.077867	11083.494138	27.774516
261.569486	11110.130483	27.779533
261.444725	11123.457140	27.784551
261.983998	11120.946656	27.789568
262.416209	11132.031635	27.794586
262.666848	11159.894171	27.799604
263.320994	11162.579361	27.804621
263.429214	11165.595788	27.809639
263.430976	11174.751125	27.814656
263.862824	11200.744483	27.819674
263.704885	11218.093257	27.824692
264.039678	11212.060009	27.829709
264.378089	11232.120031	27.834727
264.202603	11255.801047	27.839744
264.725157	11261.732911	27.844762
264.791822	11293.427602	27.849780
264.709139	11294.982079	27.854797
265.309421	11316.302617	27.859815
265.496807	11340.980139	27.864832
265.999264	11365.726952	27.869850
265.944962	11399.389878	27.874868
266.141808	11395.860685	27.879885
266.347933	11413.835629	27.884903
266.376904	11468.037492	27.889920
266.856787	11480.107375	27.894938
266.933893	11511.452597	27.899956
267.784883	11541.714503	27.904973
267.941614	11548.576571	27.909991
268.298706	11568.411789	27.915008
268.934289	11603.562624	27.920026
268.942510	11613.139370	27.925044
269.406310	11610.357698	27.930061
269.575652	11633.200080	27.935079
269.857950	11670.202317	27.940096
270.363495	11681.201517	27.945114
270.329353	11686.231391	27.950132
271.007752	11695.751815	27.955149
271.017498	11738.900283	27.960167
271.446365	11750.783441	27.965184
271.866249	11760.809020	27.970202
271.837795	11778.430836	27.975220
272.184907	11784.217004	27.980237
272.557843	11812.274739	27.985255
272.687140	11827.060660	27.990272
273.357988	11836.397297	27.995290
273.378407	11852.848407	28.000308
273.879261	11863.954066	28.005325
274.193073	11873.633302	28.010343
274.267953	11888.103718	28.015360
274.817438	11890.597575	28.020378
275.198167	11907.016783	28.025396
275.368201	11906.333320	28.030413
275.667887	11913.339718	28.035431
275.715535	11932.709751	28.040448
276.056351	11955.224130	28.045466
275.935540	11966.059963	28.050484
276.421863	11986.595144	28.055501
276.566064	11994.433926	28.060519
276.862883	12008.977281	28.065536
277.343789	12010.454468	28.070554
277.257791	12035.999858	28.075572
277.415321	12063.037242	28.080589
277.710799	12089.501238	28.085607
277.999376	12088.785578	28.090624
278.533599	12098.475014	28.095642
278.335715	12134.382323	28.100660
278.933443	12166.986734	28.105677
279.075059	12171.887677	28.110695
279.234217	12192.474025	28.115712
279.836884	12208.029723	28.120730
280.076195	12231.887069	28.125748
280.090905	12236.258350	28.130765
280.119163	12272.251497	28.135783
280.318810	12302.461756	28.140800
280.700714	12322.384406	28.145818
280.704318	12349.960542	28.150836
281.099309	12366.321934	28.155853
281.595173	12384.547879	28.160871
281.704393	12417.803858	28.165888
282.108002	12416.008836	28.170906
282.709227	12460.240034	28.175924
282.760316	12476.953773	28.180941
283.452481	12480.210354	28.185959
283.479570	12495.488809	28.190976
283.974871	12524.944791	28.195994
283.822684	12564.490569	28.201012
284.270342	12577.141690	28.206029
284.984744	12596.474055	28.211047
284.819288	12609.713347	28.216064
285.223300	12615.452605	28.221082
285.309788	12643.763160	28.226100
285.761243	12672.676783	28.231117
286.384111	12699.129448	28.236135
286.377487	12708.074344	28.241152
286.880394	12708.156729	28.246170
286.866738	12748.010942	28.251188
287.173044	12774.523910	28.256205
287.529408	12791.381338	28.261223
287.504668	12807.679391	28.266240
288.512813	12819.451097	28.271258
288.622940	12862.826280	28.276276
289.038464	12878.091342	28.281293
289.377663	12882.684918	28.286311
289.201650	12882.247659	28.291328
289.726671	12914.547335	28.296346
290.270946	12949.097792	28.301364
290.489797	12965.224197	28.306381
290.787709	12959.170394	28.311399
290.895111	12979.243990	28.316416
291.448383	13006.708383	28.321434
291.498260	13034.512814	28.326452
291.709360	13046.276143	28.331469
292.449173	13057.622828	28.336487
292.495707	13093.523409	28.341504
292.790393	13115.330922	28.346522
292.991923	13127.401562	28.351540
293.072284	13136.773497	28.356557
293.323101	13150.406116	28.361575
293.062777	13204.657700	28.366592
293.330155	13225.416568	28.371610
293.575050	13244.833590	28.376628
294.162257	13285.172845	28.381645
294.530483	13300.030156	28.386663
294.866181	13333.710697	28.391680
295.360140	13371.156158	28.396698
295.839909	13378.106661	28.401716
296.061457	13409.776793	28.406733
296.648301	13432.496036	28.411751
296.539834	13452.199369	28.416768
297.119066	13472.738440	28.421786
297.782465	13495.586933	28.426804
297.678082	13524.413510	28.431821
297.914574	13525.949346	28.436839
298.103708	13539.267900	28.441856
298.713203	13570.902616	28.446874
298.890363	13602.683666	28.451892
298.941002	13613.868078	28.456909
299.498244	13619.888062	28.461927
299.485504	13651.657252	28.466944
300.087995	13686.417118	28.471962
300.473537	13694.518600	28.476980
300.338698	13702.019065	28.481997
300.709437	13725.692257	28.487015
300.881101	13762.933465	28.492032
300.921636	13761.514208	28.497050
301.635590	13797.428994	28.502068
301.576438	13820.565135	28.507085
302.278647	13828.343349	28.512103
302.428156	13850.984959	28.517120
302.854732	13880.343696	28.522138
303.186347	13907.797403	28.527156
303.347377	13915.855728	28.532173
303.847786	13945.162992	28.537191
303.850040	13979.575948	28.542208
304.345130	13999.559189	28.547226
304.709313	14020.739559	28.552244
304.539889	14023.532952	28.557261
305.301095	14057.423607	28.562279
305.409343	14110.685309	28.567296
305.873483	14118.233550	28.572314
306.246057	14131.170114	28.577332
306.543847	14140.658768	28.582349
307.351725	14180.413096	28.587367
307.076732	14212.198352	28.592384
307.415459	14231.761785	28.597402
307.416914	14228.306015	28.602420
308.006456	14261.834681	28.607437
308.810474	14299.952759	28.612455
308.899743	14322.956372	28.617472
309.412156	14331.870779	28.622490
309.553722	14345.023739	28.627508
310.099560	14366.623638	28.632525
310.260723	14388.526630	28.637543
310.265775	14419.659366	28.642560
310.389048	14432.456149	28.647578
310.995040	14462.452844	28.652596
311.137880	14479.579742	28.657613
311.818409	14493.311898	28.662631
311.952932	14523.838840	28.667648
312.063038	14573.657160	28.672666
312.683336	14583.582854	28.677684
312.863046	14616.152570	28.682701
313.398281	14613.156897	28.687719
313.469080	14633.363871	28.692736
313.740110	14654.863011	28.697754
314.054739	14698.039156	28.702772
314.137795	14721.687277	28.707789
314.637013	14733.391632	28.712807
314.625251	14776.760578	28.717824
315.288141	14797.300125	28.722842
315.786803	14809.373360	28.727860
315.944276	14843.258257	28.732877
316.117860	14850.341140	28.737895
316.233673	14861.207580	28.742912
316.986322	14908.628004	28.747930
317.427236	14942.326035	28.752948
317.845022	14964.327656	28.757965
318.106838	14965.343375	28.762983
318.417393	14991.574856	28.768000
318.459491	15017.146348	28.773018
319.090180	15060.977204	28.778036
319.374277	15069.712280	28.783053
319.582621	15074.381684	28.788071
320.039482	15109.769847	28.793088
320.206847	15149.731657	28.798106
320.584102	15165.996401	28.803124
320.999125	15174.490866	28.808141
321.278167	15193.920349	28.813159
321.536187	15221.274986	28.818176
321.465370	15219.165666	28.823194
322.111945	15256.492585	28.828212
322.164302	15277.847459	28.833229
322.599508	15271.401373	28.838247
322.964472	15308.369949	28.843264
322.902911	15350.142882	28.848282
323.179442	15386.146075	28.853300
323.531813	15389.075688	28.858317
323.614769	15420.701742	28.863335
324.015971	15448.712295	28.868352
324.343214	15487.963031	28.873370
325.032181	15503.352448	28.878388
325.123783	15556.815480	28.883405
325.572369	15564.247206	28.888423
325.928939	15591.133914	28.893440
326.211332	15618.422160	28.898458
326.663082	15643.876532	28.903476
326.951652	15671.538901	28.908493
327.462868	15705.964410	28.913511
327.483029	15729.681121	28.918528
327.695075	15760.027386	28.923546
328.148567	15791.941214	28.928564
328.622806	15825.285729	28.933581
328.999173	15836.864624	28.938599
329.241094	15867.414171	28.943616
329.526154	15911.728338	28.948634
329.893882	15922.679943	28.953652
330.230991	15950.831174	28.958669
330.735788	15968.995092	28.963687
331.150242	16007.903312	28.968704
331.461862	16044.048724	28.973722
331.971765	16056.395242	28.978740
332.163736	16083.026295	28.983757
332.309225	16114.996369	28.988775
332.696321	16140.323521	28.993792
332.929918	16178.708884	28.998810
333.848106	16196.549463	29.003828
333.788169	16212.885909	29.008845
334.029760	16230.865095	29.013863
334.434697	16276.389668	29.018880
334.269215	16316.875806	29.023898
335.016089	16330.103726	29.028916
335.467589	16345.287332	29.033933
335.818339	16385.652108	29.038951
335.890551	16426.389221	29.043968
336.448233	16440.231584	29.048986
337.125216	16448.491177	29.054004
337.334109	16483.314984	29.059021
337.851518	16517.024131	29.064039
338.095760	16542.641845	29.069056
338.216957	16560.214202	29.074074
338.828668	16581.549293	29.079092
338.875584	16626.634414	29.084109
339.220492	16649.539199	29.089127
339.325308	16663.533792	29.094144
339.732691	16670.276260	29.099162
340.200372	16711.377411	29.104180
340.353952	16762.050998	29.109197
340.793835	16778.584383	29.114215
341.158417	16798.329453	29.119232
341.478247	16823.980824	29.124250
341.985430	16848.794381	29.129268
342.069527	16897.535107	29.134285
342.610002	16926.792288	29.139303
342.982541	16926.830067	29.144320
343.172389	16964.676062	29.149338
343.694075	16984.913905	29.154356
343.535379	17029.785098	29.159373
344.410929	17039.090172	29.164391
344.753884	17052.049725	29.169408
344.814801	17096.506579	29.174426
345.357022	17106.221360	29.179444
345.558397	17122.299632	29.184461
345.925751	17150.944380	29.189479
346.215848	17186.080927	29.194496
346.408944	17220.927828	29.199514
346.674601	17237.573990	29.204532
347.237954	17270.482792	29.209549
347.626112	17291.225337	29.214567
348.003936	17323.001790	29.219584
347.919276	17369.768673	29.224602
348.153018	17391.537635	29.229620
348.470194	17409.264499	29.234637
349.155828	17450.763336	29.239655
349.669570	17486.577526	29.244672
350.285006	17519.884843	29.249690
350.702702	17530.348583	29.254708
350.807881	17576.834102	29.259725
351.386946	17601.276013	29.264743
351.738862	17600.841236	29.269760
351.930606	17636.310207	29.274778
352.308286	17680.765173	29.279796
352.633767	17700.442144	29.284813
353.074664	17719.001554	29.289831
353.675895	17754.546554	29.294848
353.691045	17770.547479	29.299866
354.367131	17783.307580	29.304884
354.520592	17830.356378	29.309901
354.801234	17870.749011	29.314919
355.439707	17877.321414	29.319936
355.181541	17890.038931	29.324954
355.844607	17932.906028	29.329972
356.228763	17988.944980	29.334989
356.531261	17991.122058	29.340007
356.828530	18014.944454	29.345024
356.863379	18061.252257	29.350042
357.939028	18106.070625	29.355060
358.153683	18121.200447	29.360077
358.126900	18149.837979	29.365095
358.617955	18188.317915	29.370112
359.159756	18214.376104	29.375130
359.519166	18223.195001	29.380148
359.975564	18246.859052	29.385165
360.127199	18284.397607	29.390183
360.498248	18319.783268	29.395200
360.940939	18362.144131	29.400218
361.299046	18375.975404	29.405236
361.651189	18411.608687	29.410253
362.125512	18438.280461	29.415271
362.623245	18449.109839	29.420288
362.423750	18484.290645	29.425306
362.985980	18511.168674	29.430324
363.228539	18560.301107	29.435341
363.655893	18580.116765	29.440359
364.221576	18607.514509	29.445376
364.476075	18636.005544	29.450394
365.177339	18677.703500	29.455412
365.225620	18700.314980	29.460429
365.377804	18725.382320	29.465447
365.850062	18756.476081	29.470464
366.214870	18805.486598	29.475482
366.718152	18824.044835	29.480500
366.769860	18859.815409	29.485517
367.541176	18895.916391	29.490535
367.750333	18902.003744	29.495552
367.801690	18934.954759	29.500570
368.384767	18960.115195	29.505588
368.664342	18980.940864	29.510605
368.432495	19015.822367	29.515623
369.270068	19057.821886	29.520640
369.643668	19098.791672	29.525658
370.004970	19128.396046	29.530676
370.611020	19148.121396	29.535693
370.412968	19190.995326	29.540711
370.917152	19229.908985	29.545728
371.241240	19270.425548	29.550746
371.911653	19285.988690	29.555764
372.249654	19336.064427	29.560781
372.642922	19380.117897	29.565799
373.108136	19402.289472	29.570816
373.084652	19411.246346	29.575834
373.875194	19446.350760	29.580852
374.212482	19495.919555	29.585869
374.675118	19518.493651	29.590887
375.295894	19531.573198	29.595904
375.490243	19568.250145	29.600922
375.940199	19618.818946	29.605940
376.474867	19652.422926	29.610957
376.956150	19685.372192	29.615975
377.545982	19686.464859	29.620992
377.871981	19718.522466	29.626010
378.264274	19752.104458	29.631028
378.366376	19790.679189	29.636045
378.585571	19809.345366	29.641063
379.064592	19824.188759	29.646080
379.543330	19877.124297	29.651098
379.865081	19890.568783	29.656116
380.305879	19904.127596	29.661133
380.564675	19951.682061	29.666151
381.245140	19986.862557	29.671168
381.376552	19995.713768	29.676186
381.604694	20029.075964	29.681204
381.931766	20073.244675	29.686221
382.294665	20096.802304	29.691239
382.931828	20138.397897	29.696256
383.010821	20169.223537	29.701274
383.167497	20210.332796	29.706292
383.736944	20251.761739	29.711309
383.883172	20279.181114	29.716327
384.473505	20308.278450	29.721344
384.820026	20356.659758	29.726362
384.995382	20387.025361	29.731380
385.519702	20436.354846	29.736397
385.707772	20468.044185	29.741415
386.273207	20519.875060	29.746432
386.725871	20546.441902	29.751450
387.280808	20561.041695	29.756468
388.076852	20609.461399	29.761485
388.416494	20652.160427	29.766503
388.817721	20685.014564	29.771520
389.314031	20701.477950	29.776538
389.633679	20736.971862	29.781556
390.164430	20781.529696	29.786573
390.336046	20795.866716	29.791591
390.718645	20821.204980	29.796608
390.823791	20868.587256	29.801626
391.308982	20889.619392	29.806644
391.659362	20908.079124	29.811661
392.009591	20963.796427	29.816679
392.536678	20990.936520	29.821696
392.730448	21021.503594	29.826714
393.180033	21067.765482	29.831732
393.546789	21102.117396	29.836749
393.782300	21128.970112	29.841767
394.477099	21151.298425	29.846784
394.636368	21187.860211	29.851802
394.758127	21207.524575	29.856820
395.355118	21241.277546	29.861837
395.705279	21278.917782	29.866855
396.131039	21302.398953	29.871872
396.297622	21333.149224	29.876890
396.717471	21375.166885	29.881908
397.504313	21411.108425	29.886925
397.744805	21475.750738	29.891943
398.238324	21490.260607	29.896960
398.491170	21516.715403	29.901978
398.810834	21557.960286	29.906996
399.497096	21616.237978	29.912013
399.644674	21648.817481	29.917031
400.074521	21667.400502	29.922048
400.440421	21692.061830	29.927066
401.144620	21745.357033	29.932084
401.768400	21798.410306	29.937101
401.592705	21815.499734	29.942119
402.223683	21827.165338	29.947136
402.334611	21878.411842	29.952154
402.866878	21900.947729	29.957172
403.901326	21942.909432	29.962189
403.843560	21986.886681	29.967207
404.188162	22035.372501	29.972224
404.604452	22067.173793	29.977242
405.458690	22092.833353	29.982260
406.000938	22116.542360	29.987277
406.087470	22160.546675	29.992295
406.718700	22199.627607	29.997312
406.988189	22227.222158	30.002330
407.436624	22264.277693	30.007348
407.977968	22283.620196	30.012365
408.344598	22313.429586	30.017383
408.760321	22355.682142	30.022400
408.833546	22368.934793	30.027418
409.142292	22394.035409	30.032436
409.794173	22447.495995	30.037453
410.027609	22489.821569	30.042471
410.313625	22511.856639	30.047488
410.911979	22559.436552	30.052506
411.051251	22597.436209	30.057524
411.878576	22635.196168	30.062541
412.408249	22688.685594	30.067559
412.852345	22723.240901	30.072576
412.998695	22744.772787	30.077594
413.477321	22777.930418	30.082612
413.866446	22814.375810	30.087629
414.254358	22875.486633	30.092647
414.638285	22905.286337	30.097664
414.956047	22933.503124	30.102682
415.090942	22962.978307	30.107700
415.884107	23011.345557	30.112717
416.101042	23055.543515	30.117735
416.648766	23086.654991	30.122752
417.040470	23132.293646	30.127770
417.505412	23155.556538	30.132788
417.905641	23197.541029	30.137805
417.842308	23251.704087	30.142823
418.132155	23285.195035	30.147840
418.996292	23321.665539	30.152858
419.561142	23381.911804	30.157876
419.876309	23419.025016	30.162893
420.163750	23476.599381	30.167911
420.570875	23505.112959	30.172928
421.264762	23541.449674	30.177946
421.381123	23570.123334	30.182964
422.098840	23618.727101	30.187981
422.374411	23650.395406	30.192999
422.698331	23674.095389	30.198016
423.018067	23701.263105	30.203034
423.473057	23756.551440	30.208052
424.019672	23799.757218	30.213069
424.609001	23829.007493	30.218087
425.051173	23850.250701	30.223104
425.488571	23894.849599	30.228122
425.637548	23955.360544	30.233140
426.205866	23966.172418	30.238157
426.449125	24017.439852	30.243175
427.129845	24041.682120	30.248192
427.795350	24089.300999	30.253210
427.787629	24133.428532	30.258228
428.616489	24169.952431	30.263245
428.132793	24212.616811	30.268263
428.948447	24239.304575	30.273280
429.612470	24278.165775	30.278298
429.671694	24339.465498	30.283316
430.142779	24379.017859	30.288333
430.425764	24430.286292	30.293351
431.162986	24466.319851	30.298368
431.569647	24493.185949	30.303386
431.861604	24547.944080	30.308404
432.774063	24576.762289	30.313421
433.323813	24638.574910	30.318439
433.814171	24684.381220	30.323456
434.175586	24710.690672	30.328474
434.681173	24760.725025	30.333492
435.100258	24808.210046	30.338509
435.391396	24836.123804	30.343527
435.634483	24868.998082	30.348544
436.247074	24913.515546	30.353562
436.560785	24963.422943	30.358580
437.261580	24998.820345	30.363597
437.606725	25053.306431	30.368615
437.567248	25097.339234	30.373632
438.142083	25122.608099	30.378650
438.686033	25166.259310	30.383668
439.328664	25218.758940	30.388685
439.650113	25278.183383	30.393703
440.061139	25316.030747	30.398720
440.460711	25354.471383	30.403738
440.838309	25415.192607	30.408756
441.600006	25438.802254	30.413773
441.949374	25468.545974	30.418791
442.120018	25513.976877	30.423808
443.032324	25564.827851	30.428826
443.317168	25601.982406	30.433844
443.724812	25654.227340	30.438861
444.419529	25700.319579	30.443879
444.719831	25742.471973	30.448896
445.551869	25758.992104	30.453914
445.867859	25804.199517	30.458932
446.345678	25855.176747	30.463949
446.392801	25885.975569	30.468967
447.041270	25923.293093	30.473984
447.596728	25971.745947	30.479002
447.780898	26030.858256	30.484020
448.458959	26048.891072	30.489037
448.849875	26081.642362	30.494055
448.958182	26127.982432	30.499072
449.617057	26169.663517	30.504090
450.163820	26222.844372	30.509108
450.900931	26248.490213	30.514125
451.317941	26272.206844	30.519143
452.013099	26304.271251	30.524160
452.596370	26347.810203	30.529178
452.490933	26374.437465	30.534196
452.505398	26391.979475	30.539213
453.398440	26433.315034	30.544231
453.553548	26464.467631	30.549248
454.221597	26496.270385	30.554266
454.342075	26551.637294	30.559284
454.629662	26600.473643	30.564301
455.224008	26642.893499	30.569319
455.361484	26692.303669	30.574336
455.797143	26746.056429	30.579354
456.035409	26785.807401	30.584372
456.742154	26814.556177	30.589389
457.148941	26860.492549	30.594407
457.389920	26919.604863	30.599424
457.623145	26974.820480	30.604442
457.999233	27032.467971	30.609460
458.768079	27095.822396	30.614477
459.142463	27145.040201	30.619495
459.374066	27203.516380	30.624512
460.027299	27266.587762	30.629530
460.462248	27313.613533	30.634548
461.205687	27369.820058	30.639565
462.162962	27414.176748	30.644583
462.372954	27463.731713	30.649600
462.821564	27512.263366	30.654618
463.358357	27587.807033	30.659636
463.426234	27631.238849	30.664653
464.130600	27665.718676	30.669671
464.537903	27725.911776	30.674688
465.401133	27768.294742	30.679706
465.735357	27819.470301	30.684724
466.508666	27881.230964	30.689741
467.342707	27907.022571	30.694759
467.549591	27954.753280	30.699776
467.878337	28003.697227	30.704794
468.115136	28065.499866	30.709812
468.737225	28116.098876	30.714829
469.295903	28158.835908	30.719847
469.833731	28193.088827	30.724864
470.391964	28247.682392	30.729882
470.510766	28298.267297	30.734900
470.723334	28341.065110	30.739917
471.630792	28390.416071	30.744935
471.823409	28441.250996	30.749952
473.149237	28485.984857	30.754970
473.433177	28533.698137	30.759988
474.034753	28561.121979	30.765005
474.610441	28604.620619	30.770023
474.888114	28635.167090	30.775040
475.511627	28669.599211	30.780058
476.124434	28725.844379	30.785076
476.333851	28772.312109	30.790093
476.819377	28793.554340	30.795111
476.981773	28840.689250	30.800128
477.650672	28889.081166	30.805146
478.072268	28931.505264	30.810164
478.342152	28982.805313	30.815181
478.869078	29035.700110	30.820199
479.244808	29077.845108	30.825216
479.964439	29112.457803	30.830234
479.887406	29175.227849	30.835252
480.180548	29235.205366	30.840269
480.752145	29274.877076	30.845287
481.275311	29315.279213	30.850304
481.998348	29357.518931	30.855322
482.952987	29427.778135	30.860340
482.995196	29463.651607	30.865357
483.025247	29490.799129	30.870375
483.779069	29533.674523	30.875392
484.433237	29586.225093	30.880410
484.803340	29652.727156	30.885428
485.196588	29685.278341	30.890445
485.963507	29722.057808	30.895463
486.357393	29778.399351	30.900480
486.782150	29815.273389	30.905498
487.137264	29866.808028	30.910516
487.387063	29903.055038	30.915533
487.928732	29962.722749	30.920551
488.216137	30028.542790	30.925568
489.000301	30058.380386	30.930586
489.758240	30125.082019	30.935604
490.175102	30170.740096	30.940621
490.772598	30207.476031	30.945639
491.158266	30281.558108	30.950656
491.784826	30316.103422	30.955674
492.678395	30366.720978	30.960692
493.023786	30401.549494	30.965709
493.488654	30446.026895	30.970727
493.660196	30514.946718	30.975744
494.345996	30550.135699	30.980762
495.027704	30604.463964	30.985780
495.358652	30639.147080	30.990797
495.730004	30695.971665	30.995815
496.244601	30754.223872	31.000832
496.974926	30782.333449	31.005850
497.146102	30827.541727	31.010868
497.907654	30892.343508	31.015885
498.378644	30945.294394	31.020903
498.936378	31000.802115	31.025920
499.837852	31025.931108	31.030938
499.831553	31068.875928	31.035956
500.648375	31117.350596	31.040973
501.116709	31156.611497	31.045991
501.715662	31228.413129	31.051008
502.287412	31254.719973	31.056026
502.834795	31297.346764	31.061044
502.641227	31360.364788	31.066061
503.571202	31414.048882	31.071079
503.866991	31458.430616	31.076096
504.558302	31514.403734	31.081114
504.830194	31556.508820	31.086132
504.893217	31603.819083	31.091149
505.577334	31666.068602	31.096167
505.700170	31740.774469	31.101184
506.298389	31787.526770	31.106202
506.808961	31835.801647	31.111220
506.754094	31909.215745	31.116237
507.330851	31978.430913	31.121255
507.820256	32061.497713	31.126272
508.766875	32109.335364	31.131290
509.736889	32171.883338	31.136308
510.048784	32234.524468	31.141325
510.835760	32297.797188	31.146343
511.164733	32344.787901	31.151360
511.888116	32380.646362	31.156378
512.470695	32445.221629	31.161396
513.123665	32520.537331	31.166413
513.651542	32556.362194	31.171431
513.930830	32616.833208	31.176448
514.662778	32665.606989	31.181466
515.009586	32729.190594	31.186484
515.198533	32795.898643	31.191501
516.308896	32817.872348	31.196519
516.652533	32855.917780	31.201536
517.007192	32921.507326	31.206554
517.366756	32972.160722	31.211572
518.197569	33008.040586	31.216589
518.758193	33044.268030	31.221607
519.124495	33100.530226	31.226624
519.471870	33158.477340	31.231642
520.075062	33206.560866	31.236660
520.132293	33265.534309	31.241677
520.364517	33330.252737	31.246695
520.994130	33375.524391	31.251712
521.382437	33430.077135	31.256730
522.076643	33501.910228	31.261748
522.027828	33580.687602	31.266765
522.876908	33636.685621	31.271783
523.534196	33703.291360	31.276800
524.136961	33751.247089	31.281818
524.703350	33819.502623	31.286836
525.205955	33890.005941	31.291853
525.825113	33957.537081	31.296871
526.441978	34025.832405	31.301888
527.126279	34070.380596	31.306906
527.927692	34126.766668	31.311924
528.469648	34193.727759	31.316941
529.103114	34257.490403	31.321959
529.291722	34306.055589	31.326976
529.835296	34349.170028	31.331994
530.592921	34421.128914	31.337012
530.868624	34468.235070	31.342029
531.396723	34516.435547	31.347047
532.183006	34599.134007	31.352064
532.547880	34662.402930	31.357082
533.282538	34715.510973	31.362100
533.923051	34775.175625	31.367117
534.557897	34818.512781	31.372135
534.913739	34867.042419	31.377152
535.512312	34943.301979	31.382170
536.003749	34995.160513	31.387188
536.396940	35055.154096	31.392205
536.847323	35119.543293	31.397223
537.538919	35183.457443	31.402240
537.957713	35229.743686	31.407258
538.743989	35297.807691	31.412276
539.028415	35377.087059	31.417293
539.705147	35429.673553	31.422311
539.935302	35484.157792	31.427328
539.940408	35556.794635	31.432346
541.210321	35618.749978	31.437364
541.461144	35678.024500	31.442381
542.202501	35747.085302	31.447399
542.662739	35818.773977	31.452416
543.254757	35881.530101	31.457434
544.138265	35930.909516	31.462452
544.299162	35996.252179	31.467469
545.089507	36056.126745	31.472487
545.929879	36121.357636	31.477504
546.190956	36189.710607	31.482522
547.061370	36227.483806	31.487540
547.588460	36316.436880	31.492557
548.072472	36357.401334	31.497575
548.655923	36413.840160	31.502592
549.140755	36469.702204	31.507610
549.609785	36542.320083	31.512628
549.925714	36604.733066	31.517645
550.043557	36668.545367	31.522663
550.556261	36731.068293	31.527680
551.111128	36801.596645	31.532698
552.088418	36845.377624	31.537716
552.531984	36908.666792	31.542733
553.405882	36994.252519	31.547751
553.795287	37042.160883	31.552768
554.609289	37084.956447	31.557786
554.987834	37148.364497	31.562804
555.191989	37193.397461	31.567821
555.672303	37251.982922	31.572839
556.459038	37324.923882	31.577856
556.951233	37403.537331	31.582874
557.680464	37446.193132	31.587892
558.057714	37518.924811	31.592909
558.428870	37561.592694	31.597927
558.973304	37624.807775	31.602944
559.619251	37698.452006	31.607962
560.184976	37772.390657	31.612980
560.333116	37830.733074	31.617997
561.365568	37867.867601	31.623015
561.722255	37961.704360	31.628032
562.120788	38047.897512	31.633050
562.938670	38099.098923	31.638068
563.297395	38159.660917	31.643085
564.102144	38236.840962	31.648103
564.791365	38309.814661	31.653120
565.410206	38363.056858	31.658138
565.970711	38428.323460	31.663156
566.107621	38505.128951	31.668173
567.158452	38562.564064	31.673191
567.874164	38630.570379	31.678208
568.537603	38717.231094	31.683226
569.177610	38767.823128	31.688244
569.478377	38831.546632	31.693261
569.644035	38896.435153	31.698279
570.410977	38979.185517	31.703296
571.026879	39043.624634	31.708314
571.937616	39098.641828	31.713332
572.268872	39168.263290	31.718349
572.990702	39245.249899	31.723367
573.736226	39322.930418	31.728384
574.565521	39375.626407	31.733402
575.174010	39422.883183	31.738420
575.530378	39502.080555	31.743437
575.894248	39577.742171	31.748455
576.866406	39625.059342	31.753472
577.339407	39673.102937	31.758490
578.002774	39749.391218	31.763508
578.333162	39836.806673	31.768525
578.985399	39884.268893	31.773543
579.604654	39936.013325	31.778560
580.267139	40010.778414	31.783578
580.642205	40062.462540	31.788596
581.693863	40133.332214	31.793613
581.928531	40200.578027	31.798631
582.619987	40240.731174	31.803648
582.655002	40311.371773	31.808666
583.525562	40401.481393	31.813684
584.056555	40460.116261	31.818701
584.524573	40522.773367	31.823719
585.232233	40598.470836	31.828736
585.162594	40690.107014	31.833754
586.069929	40762.388609	31.838772
586.705758	40825.653466	31.843789
587.174201	40892.793788	31.848807
587.720145	40974.333543	31.853824
587.901088	41059.721611	31.858842
588.744385	41119.121369	31.863860
589.127577	41203.747580	31.868877
589.571528	41276.050936	31.873895
590.582095	41375.078092	31.878912
591.003533	41440.113380	31.883930
592.097595	41489.347035	31.888948
592.503943	41553.763398	31.893965
593.435302	41625.504697	31.898983
594.099805	41693.310012	31.904000
594.869817	41756.417054	31.909018
595.461751	41804.112050	31.914036
595.759396	41872.969770	31.919053
596.051304	41949.562218	31.924071
597.232029	42010.399038	31.929088
597.544988	42069.643277	31.934106
598.196162	42129.387402	31.939124
598.502643	42210.593443	31.944141
599.119315	42294.494851	31.949159
599.548669	42340.062141	31.954176
599.946800	42406.253721	31.959194
600.715727	42494.859514	31.964212
601.202608	42589.901379	31.969229
601.578840	42656.201647	31.974247
602.785286	42716.323163	31.979264
603.113504	42808.235692	31.984282
603.713689	42874.001001	31.989300
604.593867	42938.697528	31.994317
604.857317	43020.242555	31.999335
605.920017	43104.837930	32.004352
606.546508	43197.400780	32.009370
606.850136	43260.264887	32.014388
607.325903	43336.062504	32.019405
607.449945	43416.937823	32.024423
608.245364	43496.146305	32.029440
609.052225	43580.877671	32.034458
609.786542	43657.113743	32.039476
610.411486	43743.896279	32.044493
611.187741	43835.544212	32.049511
611.824211	43900.877866	32.054528
612.136997	43978.330832	32.059546
612.865768	44057.716893	32.064564
614.244620	44127.635677	32.069581
614.959038	44196.821567	32.074599
615.809150	44275.686574	32.079616
616.267896	44345.833919	32.084634
616.861636	44407.539616	32.089652
617.556148	44494.759322	32.094669
618.371770	44546.954757	32.099687
618.625731	44603.284056	32.104704
618.932401	44682.035347	32.109722
619.565019	44761.244576	32.114740
620.322914	44851.217887	32.119757
620.963453	44917.315307	32.124775
621.682065	44983.551607	32.129792
622.141457	45053.546829	32.134810
622.686520	45115.524963	32.139828
623.802223	45198.312174	32.144845
623.857794	45287.544867	32.149863
624.952516	45358.983294	32.154880
625.191287	45417.249732	32.159898
625.772653	45491.845346	32.164916
626.363930	45569.167407	32.169933
626.903006	45648.389558	32.174951
627.507120	45719.373680	32.179968
627.999656	45808.704033	32.184986
628.722828	45882.466393	32.190004
629.575652	45948.229328	32.195021
630.215843	46036.011446	32.200039
630.851021	46113.492694	32.205056
631.491049	46184.908360	32.210074
632.117713	46258.836540	32.215092
632.730240	46324.937277	32.220109
633.209394	46393.652416	32.225127
633.754304	46454.324755	32.230144
634.482512	46532.007073	32.235162
635.279635	46618.758828	32.240180
636.184013	46670.399353	32.245197
636.348487	46748.403005	32.250215
637.265430	46817.615724	32.255232
637.667890	46870.372158	32.260250
638.543368	46950.156807	32.265268
639.238001	47041.663540	32.270285
639.503874	47106.056144	32.275303
640.307981	47162.447560	32.280320
640.835418	47243.557069	32.285338
641.570906	47313.458340	32.290356
642.137057	47370.603267	32.295373
642.615842	47455.428590	32.300391
643.246598	47550.080571	32.305408
643.760472	47635.453472	32.310426
644.526614	47696.333268	32.315444
645.115039	47776.172000	32.320461
645.548948	47867.946850	32.325479
646.436483	47943.758385	32.330496
646.675046	48037.242987	32.335514
647.188913	48127.120823	32.340532
648.004422	48207.378573	32.345549
648.170350	48308.139002	32.350567
649.097897	48405.512344	32.355584
649.779172	48519.570856	32.360602
650.479510	48590.685746	32.365620
651.388713	48670.317406	32.370637
651.867000	48776.245233	32.375655
652.706204	48858.844855	32.380672
653.587606	48944.652433	32.385690
653.901565	49037.096957	32.390708
654.853387	49124.118924	32.395725
655.368384	49219.363643	32.400743
656.212716	49296.621381	32.405760
657.306287	49385.818960	32.410778
657.670080	49466.232451	32.415796
658.198353	49550.967446	32.420813
658.594993	49654.352673	32.425831
659.489446	49748.094245	32.430848
660.095861	49830.660765	32.435866
660.482784	49910.889163	32.440884
661.369341	49984.959584	32.445901
661.979910	50100.248770	32.450919
662.883643	50209.215416	32.455936
663.284916	50298.727415	32.460954
664.022955	50379.316651	32.465972
665.005172	50477.455846	32.470989
665.328742	50576.320135	32.476007
665.849335	50653.551596	32.481024
666.677646	50754.212463	32.486042
666.968054	50854.410040	32.491060
668.044861	50937.153159	32.496077
668.652838	51027.477643	32.501095
669.357758	51120.720406	32.506112
669.973060	51227.292990	32.511130
670.406655	51315.023248	32.516148
671.589950	51403.362780	32.521165
671.572791	51523.548809	32.526183
672.475682	51620.772170	32.531200
673.408758	51701.524267	32.536218
673.872161	51790.470839	32.541236
674.726673	51891.790274	32.546253
675.197451	52006.340288	32.551271
675.980601	52095.570239	32.556288
676.928984	52170.589567	32.561306
677.200602	52277.707965	32.566324
678.126414	52342.492559	32.571341
678.842223	52428.257903	32.576359
679.594555	52520.403715	32.581376
680.328171	52620.448893	32.586394
681.167851	52695.374522	32.591412
682.021332	52746.518899	32.596429
682.451356	52841.795718	32.601447
683.559995	52932.911883	32.606464
683.823159	53012.570469	32.611482
684.323906	53089.274934	32.616500
684.884788	53164.242115	32.621517
685.632868	53263.517588	32.626535
686.610848	53359.015992	32.631552
687.341653	53434.114081	32.636570
687.742991	53513.720330	32.641588
688.850227	53610.060895	32.646605
689.173888	53699.601575	32.651623
689.716617	53788.190517	32.656640
690.795202	53883.513814	32.661658
691.183754	53961.882712	32.666676
692.449959	54055.634497	32.671693
692.579898	54155.859973	32.676711
693.352828	54238.007346	32.681728
693.839542	54330.587853	32.686746
694.193557	54424.681587	32.691764
695.148209	54524.911747	32.696781
695.530934	54654.498732	32.701799
696.020881	54759.140533	32.706816
696.917101	54840.632040	32.711834
697.240886	54949.522325	32.716852
698.457782	55052.346261	32.721869
699.050061	55158.653754	32.726887
699.695235	55273.886079	32.731904
700.307402	55366.059105	32.736922
701.516372	55480.927888	32.741940
702.383426	55569.243951	32.746957
703.216019	55677.479366	32.751975
704.140022	55766.191245	32.756992
704.931034	55862.607839	32.762010
705.433131	55964.720694	32.767028
706.584053	56055.190653	32.772045
707.103371	56147.370062	32.777063
707.656305	56235.311399	32.782080
708.044399	56324.998815	32.787098
708.746823	56423.429248	32.792116
709.805856	56515.161134	32.797133
710.394155	56636.046472	32.802151
711.202732	56723.650835	32.807168
711.760813	56805.737094	32.812186
712.289183	56926.286622	32.817204
712.930385	57023.959372	32.822221
713.524176	57104.082370	32.827239
714.001981	57222.418084	32.832256
715.263684	57311.447638	32.837274
715.614424	57437.134724	32.842292
716.690585	57540.569930	32.847309
717.191518	57652.826242	32.852327
718.092498	57738.650740	32.857344
719.345732	57818.655103	32.862362
719.690120	57932.714314	32.867380
720.553001	58039.504511	32.872397
721.405215	58126.324422	32.877415
721.957118	58213.352271	32.882432
722.692273	58302.751271	32.887450
723.239185	58419.578940	32.892468
723.795903	58499.321973	32.897485
724.644116	58598.788074	32.902503
725.207241	58718.249681	32.907520
725.912909	58817.007455	32.912538
726.476647	58908.838590	32.917556
727.359048	58983.556972	32.922573
727.912127	59111.698209	32.927591
728.398996	59218.455753	32.932608
729.415924	59290.871989	32.937626
729.971139	59379.964342	32.942644
730.556628	59498.359057	32.947661
731.299527	59617.031789	32.952679
732.066637	59719.019183	32.957696
732.694367	59802.212184	32.962714
733.242572	59909.942745	32.967732
733.912562	60022.355147	32.972749
734.870893	60134.189762	32.977767
735.338710	60246.181837	32.982784
736.484187	60342.688128	32.987802
737.017858	60472.143054	32.992820
738.228103	60566.017262	32.997837
738.572311	60682.183918	33.002855
739.328108	60797.531280	33.007872
740.286916	60897.502451	33.012890
740.546488	61023.397865	33.017908
741.371085	61128.883882	33.022925
742.443758	61235.485941	33.027943
742.890423	61362.452163	33.032960
744.449849	61460.266802	33.037978
744.981756	61570.688449	33.042996
745.808553	61695.110417	33.048013
746.236282	61801.360653	33.053031
746.796627	61907.412599	33.058048
747.773555	62015.829383	33.063066
748.358967	62154.766114	33.068084
749.084521	62257.152456	33.073101
750.213566	62355.042517	33.078119
750.799059	62469.719768	33.083136
751.717037	62583.521182	33.088154
752.336705	62704.488695	33.093172
753.026350	62820.686469	33.098189
754.023945	62936.720295	33.103207
754.661520	63051.847279	33.108224
755.574657	63158.302562	33.113242
756.114291	63275.956044	33.118260
756.879081	63399.570807	33.123277
757.914609	63513.996363	33.128295
758.644806	63618.537665	33.133312
759.740260	63709.367541	33.138330
760.192432	63839.912989	33.143348
761.037497	63940.467863	33.148365
761.751052	64066.888702	33.153383
762.484597	64185.103206	33.158400
763.306570	64272.997553	33.163418
763.972284	64401.539372	33.168436
764.459984	64519.707926	33.173453
765.511050	64624.106589	33.178471
766.097324	64739.776184	33.183488
767.359000	64859.417980	33.188506
767.584842	64981.639678	33.193524
768.471973	65082.028889	33.198541
769.414410	65203.090667	33.203559
770.188288	65322.961099	33.208576
771.126611	65409.159807	33.213594
771.944115	65520.213092	33.218612
772.582104	65639.633756	33.223629
773.845683	65761.751937	33.228647
774.372321	65867.849030	33.233664
775.464451	65959.568053	33.238682
775.737630	66076.959280	33.243700
776.309862	66189.333509	33.248717
777.091737	66284.025498	33.253735
777.349791	66384.986388	33.258752
778.419152	66494.119670	33.263770
778.952823	66619.182661	33.268788
779.703112	66728.957735	33.273805
780.033975	66831.754555	33.278823
780.835252	66954.992816	33.283840
781.787187	67064.982902	33.288858
782.280227	67179.796626	33.293876
783.128303	67311.177397	33.298893
783.952553	67450.989299	33.303911
784.429092	67573.696977	33.308928
785.681127	67668.184911	33.313946
786.205943	67809.907172	33.318964
787.071344	67948.830623	33.323981
787.823230	68077.848920	33.328999
788.801641	68204.908848	33.334016
789.938721	68296.517016	33.339034
790.498583	68438.920503	33.344052
791.533407	68576.846628	33.349069
792.526057	68709.887606	33.354087
792.982344	68825.727954	33.359104
793.947649	68922.140173	33.364122
794.495568	69075.783811	33.369140
795.270960	69209.085106	33.374157
795.955698	69336.232019	33.379175
796.917336	69452.788947	33.384192
797.655846	69587.432671	33.389210
798.506014	69733.862072	33.394228
799.216211	69845.177472	33.399245
800.386479	69965.179937	33.404263
800.742375	70117.649063	33.409280
802.068802	70252.427559	33.414298
802.651716	70393.259958	33.419316
803.209687	70507.569129	33.424333
804.261488	70633.190179	33.429351
805.074458	70773.639399	33.434368
805.670544	70912.614314	33.439386
806.712639	71036.488061	33.444404
807.287937	71174.810598	33.449421
808.332689	71318.677235	33.454439
809.037931	71445.416199	33.459456
809.675260	71564.491507	33.464474
811.062275	71712.078883	33.469492
811.593277	71856.419684	33.474509
812.910493	71971.218359	33.479527
813.549227	72098.591829	33.484544
813.837733	72242.975296	33.489562
815.088978	72372.152420	33.494580
815.817805	72503.850899	33.499597
816.561396	72634.947077	33.504615
817.261286	72765.216648	33.509632
818.151840	72894.317391	33.514650
819.212792	73053.602207	33.519668
819.614549	73181.312131	33.524685
820.396805	73322.504087	33.529703
821.107917	73467.003085	33.534720
821.761394	73588.578349	33.539738
822.650952	73727.232300	33.544756
823.641778	73874.242437	33.549773
824.709941	74012.742273	33.554791
825.075813	74167.325449	33.559808
825.983889	74308.838252	33.564826
827.395818	74427.232493	33.569844
827.877831	74597.247737	33.574861
828.949256	74727.493160	33.579879
829.971136	74842.400270	33.584896
830.407454	74973.485584	33.589914
831.095045	75110.170883	33.594932
832.016417	75237.996915	33.599949
832.744712	75352.550500	33.604967
833.548762	75498.280895	33.609984
834.384319	75631.966569	33.615002
835.366526	75771.674431	33.620020
836.220370	75893.672264	33.625037
837.071283	75995.953354	33.630055
837.979896	76140.127761	33.635072
838.902050	76274.037074	33.640090
839.833334	76405.485662	33.645108
840.214574	76550.293734	33.650125
841.359901	76663.286567	33.655143
842.108295	76811.476050	33.660160
843.083527	76956.549210	33.665178
844.166100	77084.953957	33.670196
844.675124	77217.021041	33.675213
845.561877	77352.138098	33.680231
845.974247	77492.539243	33.685248
846.979028	77631.452104	33.690266
847.933062	77763.240294	33.695284
848.612995	77915.660610	33.700301
849.465622	78070.191147	33.705319
850.280131	78204.699259	33.710336
851.060098	78339.694565	33.715354
852.204930	78485.413913	33.720372
852.750163	78654.855834	33.725389
854.039048	78793.286396	33.730407
855.302273	78941.961824	33.735424
855.983247	79082.297131	33.740442
856.684197	79216.058539	33.745460
857.608581	79358.455247	33.750477
858.627362	79513.891890	33.755495
859.225210	79658.874410	33.760512
859.860226	79792.523686	33.765530
860.988916	79923.751992	33.770548
861.618084	80087.561744	33.775565
862.992101	80241.338256	33.780583
863.608772	80385.360990	33.785600
864.306740	80538.264459	33.790618
865.253021	80676.851908	33.795636
866.033207	80818.522753	33.800653
866.979670	80962.292348	33.805671
867.881037	81131.820868	33.810688
868.661289	81271.173162	33.815706
870.029685	81418.038721	33.820724
870.696215	81573.484642	33.825741
871.504674	81723.746569	33.830759
872.395136	81857.498866	33.835776
873.432825	82007.497122	33.840794
874.542153	82162.937265	33.845812
875.103490	82310.840173	33.850829
876.215966	82450.163907	33.855847
876.963110	82587.885147	33.860864
877.496497	82731.569813	33.865882
878.550335	82889.971965	33.870900
879.223316	83044.832350	33.875917
879.934679	83173.238687	33.880935
881.182876	83335.578235	33.885952
881.693492	83509.307399	33.890970
883.044235	83637.800577	33.895988
883.534459	83807.859948	33.901005
884.425894	83950.816334	33.906023
885.390235	84092.496342	33.911040
885.941269	84250.155965	33.916058
886.660315	84419.321755	33.921076
887.603844	84579.430384	33.926093
888.408224	84710.727511	33.931111
889.766835	84849.164962	33.936128
890.331079	85010.370444	33.941146
891.381072	85148.968220	33.946164
891.803554	85311.091262	33.951181
892.669213	85468.846529	33.956199
893.758471	85616.658476	33.961216
894.534769	85761.739321	33.966234
895.418939	85931.977214	33.971252
896.286553	86087.123477	33.976269
897.594491	86227.842601	33.981287
898.320942	86395.168008	33.986304
898.921039	86566.147120	33.991322
900.072570	86697.486872	33.996340
900.783176	86860.180639	34.001357
901.730548	87027.898060	34.006375
902.735457	87205.471070	34.011392
903.383706	87358.599481	34.016410
904.715488	87505.073782	34.021428
905.906040	87676.305268	34.026445
906.235962	87844.896139	34.031463
907.227024	88020.282124	34.036480
908.065018	88171.264925	34.041498
909.171187	88337.339467	34.046516
909.765390	88519.565015	34.051533
910.472311	88672.388669	34.056551
911.901179	88843.184429	34.061568
912.783325	89009.129897	34.066586
913.797190	89163.646156	34.071604
914.856135	89344.978814	34.076621
915.573202	89512.891362	34.081639
916.494463	89701.589618	34.086656
917.584946	89853.421139	34.091674
919.101353	89991.281119	34.096692
920.066134	90165.953498	34.101709
920.980806	90337.617036	34.106727
921.950726	90485.466979	34.111744
923.164962	90647.610387	34.116762
923.933159	90791.281116	34.121780
924.878267	90965.386807	34.126797
925.951497	91114.951193	34.131815
926.837828	91281.095495	34.136832
927.254588	91459.114253	34.141850
928.534000	91607.603550	34.146868
929.134703	91769.704060	34.151885
930.232173	91916.219260	34.156903
930.930221	92091.772561	34.161920
931.697981	92268.676253	34.166938
932.265273	92433.862405	34.171956
933.085408	92613.411627	34.176973
934.237033	92776.883572	34.181991
935.206401	92946.525462	34.187008
936.155880	93129.177193	34.192026
937.524574	93301.046628	34.197044
938.337215	93477.103795	34.202061
939.080547	93634.073443	34.207079
940.031138	93799.066479	34.212096
940.860275	93976.896647	34.217114
941.765091	94172.347985	34.222132
942.674666	94356.756073	34.227149
943.438109	94507.152290	34.232167
944.316241	94685.087175	34.237184
944.920210	94876.619233	34.242202
946.190747	95082.352961	34.247220
946.824385	95264.338818	34.252237
947.813976	95442.868460	34.257255
948.798708	95629.571335	34.262272
949.361436	95816.199742	34.267290
950.590352	95998.092798	34.272308
951.657699	96163.911800	34.277325
952.350163	96337.686682	34.282343
953.431286	96522.532264	34.287360
954.089396	96704.328604	34.292378
954.858432	96873.733570	34.297396
955.855448	97078.738084	34.302413
956.468618	97269.705064	34.307431
957.838960	97448.021902	34.312448
958.634336	97627.840180	34.317466
959.630493	97833.547401	34.322484
960.597529	98032.614731	34.327501
961.304287	98216.034656	34.332519
962.825626	98416.456789	34.337536
963.306891	98615.450759	34.342554
964.518057	98809.685840	34.347572
965.772093	98978.544082	34.352589
966.870718	99187.322080	34.357607
968.115768	99395.773801	34.362624
968.848181	99584.428390	34.367642
969.894240	99761.568344	34.372660
970.928302	99956.417671	34.377677
971.795154	100162.121200	34.382695
972.924113	100351.279513	34.387712
973.787031	100546.946672	34.392730
974.578923	100720.653569	34.397748
975.600992	100924.596807	34.402765
976.620088	101141.064314	34.407783
978.166039	101323.982335	34.412800
979.263370	101519.972877	34.417818
980.361160	101701.024069	34.422836
981.656390	101898.339671	34.427853
982.414158	102087.135468	34.432871
983.381678	102274.017737	34.437888
984.306705	102442.478768	34.442906
985.427853	102650.832294	34.447924
986.359051	102847.126429	34.452941
987.104678	103023.921039	34.457959
988.414509	103211.703354	34.462976
989.159232	103411.350176	34.467994
990.396261	103602.616920	34.473012
991.243259	103784.446113	34.478029
992.351323	103972.178684	34.483047
993.476999	104148.779029	34.488064
994.080108	104369.356817	34.493082
995.146044	104566.325688	34.498100
996.484481	104752.689967	34.503117
997.107604	104931.430090	34.508135
998.133540	105115.347583	34.513152
999.564854	105314.344966	34.518170
1000.847752	105514.109202	34.523188
1001.888216	105687.270661	34.528205
1003.261687	105859.415851	34.533223
1003.994291	106054.158949	34.538240
1004.922077	106251.809311	34.543258
1006.133507	106426.796404	34.548276
1006.801669	106622.757472	34.553293
1007.855054	106803.161762	34.558311
1008.698262	106973.432578	34.563328
1009.848586	107173.123784	34.568346
1010.868189	107367.417701	34.573364
1011.797832	107559.359635	34.578381
1012.420293	107739.854182	34.583399
1013.657984	107935.230782	34.588416
1014.470426	108131.502253	34.593434
1015.178887	108337.126408	34.598452
1016.466889	108526.647884	34.603469
1016.962197	108717.821405	34.608487
1018.479373	108895.478471	34.613504
1019.055005	109100.991174	34.618522
1020.307344	109274.742933	34.623540
1021.450292	109438.647492	34.628557
1022.349140	109638.981482	34.633575
1023.576499	109825.469852	34.638592
1024.281179	110023.115671	34.643610
1025.556920	110205.862320	34.648628
1026.144569	110388.888475	34.653645
1027.210737	110587.960702	34.658663
1028.287353	110791.883799	34.663680
1028.924557	110988.293939	34.668698
1030.068502	111169.700970	34.673716
1031.049153	111367.475800	34.678733
1031.952067	111597.640423	34.683751
1033.303328	111792.013231	34.688768
1034.374275	111990.335049	34.693786
1035.474757	112175.809355	34.698804
1036.704246	112385.039300	34.703821
1037.703656	112604.138396	34.708839
1038.499454	112802.131569	34.713856
1039.471108	113007.380754	34.718874
1040.541675	113220.291500	34.723892
1041.532440	113420.803095	34.728909
1042.156023	113628.977236	34.733927
1043.464956	113842.600858	34.738944
1044.862711	114074.060171	34.743962
1045.955001	114272.230396	34.748980
1047.214082	114499.421830	34.753997
1047.998110	114725.110076	34.759015
1049.209979	114914.410300	34.764032
1050.265482	115122.055725	34.769050
1050.982147	115352.080044	34.774068
1052.178489	115585.776906	34.779085
1053.257088	115788.432196	34.784103
1054.456969	115992.918545	34.789120
1055.535718	116210.918463	34.794138
1056.313873	116446.541219	34.799156
1058.032687	116647.209431	34.804173
1058.942151	116870.449332	34.809191
1060.080964	117065.287249	34.814208
1061.024007	117295.847679	34.819226
1061.914349	117524.530992	34.824244
1062.984079	117725.833526	34.829261
1064.306482	117933.443150	34.834279
1064.905601	118155.452220	34.839296
1066.061663	118394.107621	34.844314
1066.861028	118633.432068	34.849332
1068.227679	118829.030092	34.854349
1069.004135	119056.604329	34.859367
1070.094638	119272.674872	34.864384
1071.409608	119510.401190	34.869402
1072.697675	119729.926863	34.874420
1073.921612	119939.087847	34.879437
1074.519349	120191.471062	34.884455
1076.127982	120410.024096	34.889472
1076.982522	120628.272487	34.894490
1077.760806	120843.139382	34.899508
1079.373957	121061.874020	34.904525
1080.229375	121312.564666	34.909543
1081.043067	121540.570626	34.914560
1082.418199	121742.839426	34.919578
1083.126266	121962.439881	34.924596
1084.688193	122205.102140	34.929613
1085.419744	122441.314389	34.934631
1086.610878	122660.194127	34.939648
1087.439799	122879.933614	34.944666
1088.684326	123108.907148	34.949684
1089.685282	123317.026943	34.954701
1090.538222	123533.903558	34.959719
1091.535672	123749.440036	34.964736
1092.777001	123992.372815	34.969754
1093.635946	124203.867759	34.974772
1094.863091	124408.447758	34.979789
1095.591646	124647.605555	34.984807
1096.572108	124888.295081	34.989824
1097.785238	125128.656682	34.994842
1098.557072	125349.475838	34.999860
1100.036946	125567.556493	35.004877
1100.902374	125832.781719	35.009895
1102.049622	126075.075437	35.014912
1102.861212	126305.108333	35.019930
1104.090322	126567.352564	35.024948
1105.353665	126800.749110	35.029965
1106.706626	127038.973892	35.034983
1107.564577	127279.766273	35.040000
1108.724887	127517.342273	35.045018
1109.799819	127772.233769	35.050036
1111.186801	128027.912365	35.055053
1112.339154	128272.060609	35.060071
1113.352788	128527.044608	35.065088
1114.587586	128779.611506	35.070106
1115.404866	129022.946571	35.075124
1116.748279	129262.800013	35.080141
1117.691134	129532.328809	35.085159
1118.526163	129788.480830	35.090176
1119.800921	130034.283298	35.095194
1121.104785	130276.166442	35.100212
1122.514908	130543.130038	35.105229
1123.441622	130822.508429	35.110247
1124.585657	131069.316679	35.115264
1125.906762	131312.802129	35.120282
1126.868797	131572.851893	35.125300
1128.317118	131837.906358	35.130317
1129.577619	132101.358945	35.135335
1130.883164	132344.842342	35.140352
1132.433112	132586.816911	35.145370
1133.156076	132830.121378	35.150388
1134.118489	133069.395312	35.155405
1135.681075	133335.888609	35.160423
1136.502854	133578.941696	35.165440
1137.686835	133827.045336	35.170458
1138.939727	134105.042776	35.175476
1139.951279	134339.437841	35.180493
1140.963072	134594.725347	35.185511
1141.990612	134866.973505	35.190528
1143.143822	135115.751439	35.195546
1144.010507	135371.094447	35.200564
1145.180315	135641.893227	35.205581
1146.474135	135908.097434	35.210599
1147.746952	136170.301354	35.215616
1148.934214	136425.688537	35.220634
1149.964218	136696.785462	35.225652
1151.562961	136959.601187	35.230669
1152.868924	137208.217897	35.235687
1153.634351	137456.076337	35.240704
1155.259393	137720.161610	35.245722
1155.853817	137998.618238	35.250740
1157.186158	138245.577694	35.255757
1158.280725	138492.235950	35.260775
1159.675478	138769.755606	35.265792
1160.759346	139031.772802	35.270810
1161.622782	139280.668424	35.275828
1163.252725	139522.073262	35.280845
1164.159957	139797.894362	35.285863
1164.847465	140062.077063	35.290880
1166.545741	140303.045215	35.295898
1167.546257	140549.024279	35.300916
1168.961280	140788.356410	35.305933
1170.204358	141032.105540	35.310951
1170.899443	141280.929746	35.315968
1172.329797	141522.343930	35.320986
1173.132676	141760.465391	35.326004
1174.377057	142023.950307	35.331021
1175.286596	142300.564999	35.336039
1176.286972	142565.298934	35.341056
1177.613240	142805.801151	35.346074
1178.637390	143065.336412	35.351092
1179.758446	143334.113885	35.356109
1181.001479	143619.382539	35.361127
1182.052897	143894.579237	35.366144
1183.551126	144160.840995	35.371162
1184.249419	144442.047309	35.376180
1185.533858	144704.341603	35.381197
1186.612112	144971.414377	35.386215
1187.774360	145258.802151	35.391232
1188.893876	145544.386023	35.396250
1189.848993	145838.153052	35.401268
1191.088923	146125.699978	35.406285
1192.334877	146405.741169	35.411303
1193.618614	146709.073358	35.416320
1195.016852	147008.407382	35.421338
1196.122550	147291.281274	35.426356
1197.206498	147564.053999	35.431373
1198.827984	147859.401779	35.436391
1199.938507	148170.383903	35.441408
1201.456154	148436.953853	35.446426
1202.843803	148722.214741	35.451444
1204.199110	149006.532095	35.456461
1205.536089	149298.666785	35.461479
1206.933557	149567.991567	35.466496
1208.505431	149859.191588	35.471514
1209.603177	150118.589102	35.476532
1210.603016	150385.094035	35.481549
1212.131272	150686.136663	35.486567
1212.894143	150974.422671	35.491584
1214.258548	151230.347100	35.496602
1215.562755	151506.512143	35.501620
1216.596392	151786.769727	35.506637
1218.326100	152074.904761	35.511655
1219.363231	152367.227596	35.516672
1220.610076	152647.355032	35.521690
1221.364409	152941.276392	35.526708
1222.589943	153215.780281	35.531725
1223.965865	153484.883609	35.536743
1224.911847	153781.735155	35.541760
1226.045011	154069.337191	35.546778
1227.268116	154386.733194	35.551796
1228.332950	154666.309601	35.556813
1229.469727	154949.605249	35.561831
1230.696196	155274.948220	35.566848
1232.069587	155569.028842	35.571866
1233.265731	155860.134834	35.576884
1234.676264	156143.305354	35.581901
1236.147150	156449.934050	35.586919
1237.130907	156759.322009	35.591936
1238.208669	157033.712921	35.596954
1239.653697	157331.042408	35.601972
1241.094125	157614.586614	35.606989
1242.500592	157926.983798	35.612007
1243.454041	158233.991042	35.617024
1244.720585	158504.910831	35.622042
1246.126769	158812.900723	35.627060
1247.255029	159103.154212	35.632077
1248.561099	159371.523695	35.637095
1249.520701	159656.519300	35.642112
1250.918314	159933.605019	35.647130
1252.316515	160225.788397	35.652148
1253.241740	160510.681602	35.657165
1254.274453	160787.896891	35.662183
1255.588342	161078.057980	35.667200
1256.883320	161362.071597	35.672218
1257.946558	161678.449453	35.677236
1259.374084	161972.365943	35.682253
1260.581082	162265.851564	35.687271
1261.525179	162563.163205	35.692288
1262.801765	162846.403654	35.697306
1264.075680	163158.825413	35.702324
1265.539095	163455.994361	35.707341
1266.720206	163749.469471	35.712359
1268.162555	164058.939607	35.717376
1269.620111	164356.065222	35.722394
1270.886011	164667.167542	35.727412
1272.086896	164963.172637	35.732429
1273.551895	165257.588394	35.737447
1274.475329	165584.346513	35.742464
1276.124196	165868.231160	35.747482
1277.585234	166184.120961	35.752500
1279.102942	166481.657633	35.757517
1280.192123	166812.851153	35.762535
1281.353161	167129.634847	35.767552
1282.566144	167423.180984	35.772570
1283.645216	167721.826367	35.777588
1284.741008	168041.215850	35.782605
1286.419049	168342.634128	35.787623
1287.202145	168690.209386	35.792640
1288.742530	168994.801551	35.797658
1289.997374	169299.176507	35.802676
1291.007941	169634.782000	35.807693
1292.391200	169941.081522	35.812711
1293.851340	170275.856367	35.817728
1295.237308	170606.826678	35.822746
1296.400039	170950.702721	35.827764
1297.332081	171274.545663	35.832781
1299.057304	171581.916628	35.837799
1300.104994	171925.349622	35.842816
1301.284249	172263.840110	35.847834
1302.805905	172615.270404	35.852852
1303.761149	172939.667057	35.857869
1304.909754	173264.452845	35.862887
1306.088313	173615.541378	35.867904
1307.766710	173944.508203	35.872922
1308.908902	174292.308575	35.877940
1310.225497	174663.216297	35.882957
1311.708266	174994.100927	35.887975
1312.743681	175350.352901	35.892992
1314.451755	175685.849759	35.898010
1316.006533	176032.833539	35.903028
1317.595604	176360.233097	35.908045
1319.053107	176678.392657	35.913063
1320.232916	177026.016626	35.918080
1321.714634	177377.362373	35.923098
1323.016955	177711.417574	35.928116
1324.165172	178021.718111	35.933133
1325.796631	178355.114268	35.938151
1326.675507	178707.026014	35.943168
1328.167277	179030.969742	35.948186
1329.772737	179386.332602	35.953204
1330.832392	179740.760118	35.958221
1332.320426	180063.772091	35.963239
1333.557228	180381.662255	35.968256
1334.848935	180716.082278	35.973274
1336.023007	181052.148454	35.978292
1337.560844	181384.641266	35.983309
1339.284510	181672.659431	35.988327
1340.264938	181993.356161	35.993344
1341.630486	182309.841125	35.998362
1343.035878	182639.673332	36.003380
1344.322269	182957.000324	36.008397
1346.071345	183281.626981	36.013415
1346.755687	183610.112112	36.018432
1348.254699	183945.978645	36.023450
1349.301100	184258.504772	36.028468
1350.399187	184588.831607	36.033485
1351.535360	184934.283615	36.038503
1352.661439	185292.076678	36.043520
1353.974032	185628.454313	36.048538
1355.473577	185974.957363	36.053556
1356.623139	186335.279377	36.058573
1358.099941	186696.374824	36.063591
1359.439072	187057.901573	36.068608
1360.604393	187411.259710	36.073626
1362.264554	187767.191320	36.078644
1363.459357	188120.079511	36.083661
1365.175184	188464.544487	36.088679
1366.594973	188827.300803	36.093696
1367.985808	189192.437928	36.098714
1369.331469	189568.552085	36.103732
1370.577431	189923.677295	36.108749
1372.282041	190296.436721	36.113767
1373.418973	190654.123228	36.118784
1375.048719	190999.125655	36.123802
1376.631743	191371.988316	36.128820
1377.325203	191764.980556	36.133837
1378.886536	192139.997023	36.138855
1380.306591	192504.985431	36.143872
1381.696009	192868.876763	36.148890
1383.379640	193246.736315	36.153908
1384.518902	193636.697021	36.158925
1386.244844	194000.450885	36.163943
1387.108215	194381.017271	36.168960
1388.630374	194758.227501	36.173978
1390.400188	195117.423475	36.178996
1391.877233	195491.332370	36.184013
1393.238563	195879.658627	36.189031
1394.642346	196282.465266	36.194048
1396.149439	196643.605047	36.199066
1397.757600	196997.557502	36.204084
1399.038579	197374.569609	36.209101
1400.617683	197753.566006	36.214119
1401.769812	198113.909515	36.219136
1403.289708	198480.186589	36.224154
1404.548146	198875.213368	36.229172
1405.556160	199270.855186	36.234189
1407.336257	199633.198309	36.239207
1408.845140	200001.402825	36.244224
1410.099260	200403.536455	36.249242
1411.762447	200774.043136	36.254260
1412.865689	201160.260260	36.259277
1414.667168	201519.347311	36.264295
1416.172202	201906.441908	36.269312
1417.576743	202297.554575	36.274330
1419.724276	202660.272422	36.279348
1421.269922	203009.773129	36.284365
1422.760010	203379.865517	36.289383
1424.076620	203755.155933	36.294400
1425.392221	204113.841547	36.299418
1426.656057	204462.062892	36.304436
1427.656143	204848.304973	36.309453
1429.066900	205216.693345	36.314471
1430.632782	205580.601453	36.319488
1432.083870	205928.976772	36.324506
1433.528670	206268.428913	36.329524
1434.506249	206634.635924	36.334541
1435.925875	206996.365953	36.339559
1437.064379	207373.659907	36.344576
1438.321570	207739.191364	36.349594
1439.734553	208089.843215	36.354612
1441.208582	208489.243918	36.359629
1442.214329	208845.883361	36.364647
1443.472979	209223.179383	36.369664
1444.641693	209618.750950	36.374682
1446.060219	210031.640737	36.379700
1447.152747	210425.476697	36.384717
1448.669089	210809.340548	36.389735
1450.400976	211217.956503	36.394752
1451.352880	211628.734885	36.399770
1452.913231	212053.242829	36.404788
1454.056007	212458.686217	36.409805
1455.797052	212857.150597	36.414823
1457.147278	213281.724932	36.419840
1458.380892	213703.527088	36.424858
1459.948500	214141.834560	36.429876
1461.474242	214573.827498	36.434893
1462.685962	215004.122066	36.439911
1464.545113	215435.073817	36.444928
1465.795105	215862.140924	36.449946
1467.133931	216287.722412	36.454964
1468.545413	216751.719541	36.459981
1470.493726	217191.604810	36.464999
1471.903931	217648.393956	36.470016
1473.309965	218136.958135	36.475034
1475.265849	218573.191525	36.480052
1476.610169	219002.975278	36.485069
1478.112797	219436.544504	36.490087
1479.595606	219894.704045	36.495104
1480.624469	220349.257954	36.500122
1482.373590	220785.357715	36.505140
1483.542033	221238.749772	36.510157
1485.339558	221694.579894	36.515175
1486.815696	222156.027347	36.520192
1488.266449	222615.423783	36.525210
1490.360700	223036.008570	36.530228
1491.954414	223495.664671	36.535245
1493.465839	223945.430796	36.540263
1495.341020	224389.881197	36.545280
1496.925486	224823.180412	36.550298
1498.855108	225259.472273	36.555316
1500.268538	225699.965699	36.560333
1501.868881	226131.921226	36.565351
1503.543235	226563.637581	36.570368
1504.509215	227006.216440	36.575386
1506.494112	227440.577157	36.580404
1507.767959	227856.692815	36.585421
1509.195482	228298.768547	36.590439
1511.123894	228738.731243	36.595456
1512.456251	229173.358274	36.600474
1513.971784	229610.395000	36.605492
1515.489615	230054.265499	36.610509
1516.775465	230466.679519	36.615527
1518.764550	230903.210709	36.620544
1520.103551	231363.015789	36.625562
1521.450085	231800.621178	36.630580
1522.860605	232227.422177	36.635597
1524.386970	232650.725496	36.640615
1526.291448	233092.002221	36.645632
1527.470212	233538.835845	36.650650
1529.093938	233962.762039	36.655668
1529.957015	234386.510166	36.660685
1531.658901	234811.060929	36.665703
1533.146592	235213.142863	36.670720
1534.079332	235639.702542	36.675738
1536.124236	236087.747125	36.680756
1537.684158	236538.336933	36.685773
1539.153287	236958.639142	36.690791
1540.647355	237380.208388	36.695808
1541.765921	237820.917192	36.700826
1543.587228	238249.445437	36.705844
1545.057822	238695.204122	36.710861
1546.368994	239132.734690	36.715879
1548.168071	239588.932316	36.720896
1549.847205	240021.425571	36.725914
1551.465671	240466.325956	36.730932
1552.813509	240925.979759	36.735949
1554.255348	241382.469289	36.740967
1556.094191	241825.609084	36.745984
1557.455093	242277.363817	36.751002
1559.057534	242724.862917	36.756020
1560.525864	243207.567160	36.761037
1562.233440	243655.533487	36.766055
1563.815925	244098.186864	36.771072
1565.753415	244560.494759	36.776090
1567.026841	245034.522044	36.781108
1568.390523	245513.158614	36.786125
1570.099671	245972.890432	36.791143
1571.835689	246432.948874	36.796160
1573.326412	246892.845373	36.801178
1574.895055	247373.763188	36.806196
1576.511603	247855.817043	36.811213
1577.731532	248310.807021	36.816231
1579.628260	248782.121608	36.821248
1580.848723	249279.408557	36.826266
1582.742431	249758.904801	36.831284
1584.200698	250246.323069	36.836301
1585.829097	250725.356384	36.841319
1587.790817	251183.047656	36.846336
1589.230640	251678.498215	36.851354
1590.660666	252175.068739	36.856372
1592.539269	252649.846233	36.861389
1594.062471	253115.664792	36.866407
1596.051705	253612.627325	36.871424
1597.052541	254116.536079	36.876442
1599.031069	254616.803769	36.881460
1600.343497	255079.026259	36.886477
1602.070075	255561.884367	36.891495
1603.758937	256065.173236	36.896512
1605.099761	256565.268282	36.901530
1607.012584	257046.013624	36.906548
1608.297750	257553.129764	36.911565
1609.851520	258046.788937	36.916583
1611.550095	258551.322453	36.921600
1613.550000	259053.393149	36.926618
1615.044608	259547.037292	36.931636
1616.555583	260050.814793	36.936653
1618.278170	260536.394132	36.941671
1619.933143	261033.289179	36.946688
1621.336688	261529.666892	36.951706
1623.017290	262030.901754	36.956724
1624.745127	262519.274742	36.961741
1626.379088	263019.704351	36.966759
1627.998163	263530.373879	36.971776
1629.273904	264045.596336	36.976794
1631.197198	264538.001274	36.981812
1633.271142	265044.175181	36.986829
1634.430403	265546.867142	36.991847
1636.268839	266032.629863	36.996864
1637.584721	266518.656389	37.001882
1639.292017	266997.428954	37.006900
1640.916304	267472.099610	37.011917
1642.350320	267943.143293	37.016935
1644.289119	268438.210980	37.021952
1645.590197	268940.242346	37.026970
1647.267585	269425.800768	37.031988
1648.926516	269909.431165	37.037005
1650.244722	270399.061644	37.042023
1651.957883	270897.720757	37.047040
1653.593203	271396.265152	37.052058
1655.403807	271897.803007	37.057076
1657.463136	272396.352466	37.062093
1658.426037	272917.690799	37.067111
1660.260145	273416.403097	37.072128
1661.736042	273928.307075	37.077146
1663.086986	274432.864082	37.082164
1664.831585	274952.495417	37.087181
1666.494182	275478.667925	37.092199
1668.233548	276018.366483	37.097216
1669.811724	276527.302625	37.102234
1671.458215	277052.636649	37.107252
1673.352598	277591.163479	37.112269
1674.836041	278127.394565	37.117287
1676.764097	278655.447777	37.122304
1678.415982	279197.084882	37.127322
1679.788675	279732.009791	37.132340
1681.788670	280266.093292	37.137357
1683.127786	280822.562276	37.142375
1684.734421	281360.416733	37.147392
1686.502762	281894.153401	37.152410
1688.383115	282450.477977	37.157428
1690.179798	282988.017375	37.162445
1691.662372	283547.681320	37.167463
1693.611128	284110.518123	37.172480
1695.477973	284646.390112	37.177498
1697.386652	285191.398187	37.182516
1698.951039	285760.008605	37.187533
1700.548370	286320.457833	37.192551
1702.145283	286864.673777	37.197568
1703.656998	287439.231107	37.202586
1705.308299	288007.184436	37.207604
1706.979247	288564.133788	37.212621
1708.388732	289152.951715	37.217639
1710.380547	289702.985678	37.222656
1711.626022	290293.248595	37.227674
1713.332352	290883.433061	37.232692
1715.068001	291448.184223	37.237709
1716.836651	292021.436801	37.242727
1718.864886	292612.602203	37.247744
1720.383593	293213.526542	37.252762
1722.462312	293786.288560	37.257780
1724.311092	294348.087736	37.262797
1726.085972	294948.377483	37.267815
1727.998984	295523.622727	37.272832
1729.867206	296091.862328	37.277850
1731.429957	296672.341411	37.282868
1733.384418	297252.194217	37.287885
1735.227988	297823.579043	37.292903
1737.074645	298387.188342	37.297920
1738.693727	298966.046379	37.302938
1740.457042	299549.601780	37.307956
1742.075260	300117.481540	37.312973
1744.069961	300691.087063	37.317991
1745.748753	301269.465701	37.323008
1747.535069	301849.474272	37.328026
1749.028819	302428.029326	37.333044
1750.957929	302980.780996	37.338061
1752.578010	303543.130198	37.343079
1754.596720	304098.299035	37.348096
1756.014713	304663.697447	37.353114
1757.641128	305227.610475	37.358132
1759.669349	305767.453365	37.363149
1760.956108	306328.266536	37.368167
1762.419865	306893.389979	37.373184
1764.144686	307457.273185	37.378202
1765.694538	308023.543604	37.383220
1767.661965	308599.239822	37.388237
1769.055159	309190.645749	37.393255
1770.876245	309764.885401	37.398272
1772.837080	310340.952046	37.403290
1774.439519	310922.280029	37.408308
1776.446632	311507.219570	37.413325
1778.332808	312108.275644	37.418343
1779.692262	312695.218202	37.423360
1781.662230	313312.250542	37.428378
1783.217230	313910.935241	37.433396
1785.271668	314501.660623	37.438413
1787.212357	315113.858645	37.443431
1788.968844	315716.051419	37.448448
1790.884237	316319.686060	37.453466
1792.884666	316932.570593	37.458484
1794.612674	317525.662529	37.463501
1796.440106	318126.859191	37.468519
1798.361610	318718.716025	37.473536
1800.368018	319345.875734	37.478554
1801.679097	319978.197791	37.483572
1803.565443	320570.629043	37.488589
1805.284546	321191.116048	37.493607
1807.058001	321806.890947	37.498624
1809.086073	322444.226813	37.503642
1810.819339	323080.411880	37.508660
1812.609692	323682.226839	37.513677
1814.396211	324304.908532	37.518695
1815.897778	324940.631483	37.523712
1818.287813	325567.619568	37.528730
1819.792302	326197.540557	37.533748
1821.535688	326830.665836	37.538765
1823.779202	327458.675028	37.543783
1825.925336	328110.687214	37.548800
1827.507088	328745.673134	37.553818
1829.358755	329367.481729	37.558836
1831.444254	329982.999690	37.563853
1832.808076	330627.243381	37.568871
1834.437113	331294.844400	37.573888
1836.452516	331922.717945	37.578906
1838.278103	332561.151977	37.583924
1840.330756	333195.733369	37.588941
1842.148802	333849.336078	37.593959
1843.617906	334504.689743	37.598976
1845.517449	335152.628027	37.603994
1847.229061	335803.356890	37.609012
1849.332392	336464.421744	37.614029
1851.213955	337122.849696	37.619047
1853.038630	337764.905442	37.624064
1854.834002	338401.881335	37.629082
1856.500937	339070.119517	37.634100
1858.568345	339735.516286	37.639117
1859.941291	340405.537547	37.644135
1861.804711	341067.701813	37.649152
1863.884943	341716.241630	37.654170
1865.671334	342395.154596	37.659188
1867.420292	343052.946121	37.664205
1869.189580	343724.381478	37.669223
1870.978066	344416.414940	37.674240
1873.032066	345064.230574	37.679258
1874.760895	345695.364891	37.684276
1877.113959	346345.753879	37.689293
1878.987026	346987.939142	37.694311
1880.783747	347638.833899	37.699328
1882.796637	348276.105728	37.704346
1884.398209	348917.878267	37.709364
1886.571659	349554.700216	37.714381
1888.044776	350218.175487	37.719399
1889.319612	350881.115604	37.724416
1891.577550	351527.210400	37.729434
1893.215207	352202.151585	37.734452
1894.966892	352873.181106	37.739469
1896.907530	353539.804535	37.744487
1898.720712	354197.810878	37.749504
1900.783347	354877.818410	37.754522
1902.573373	355574.380170	37.759540
1904.597029	356261.249507	37.764557
1906.359279	356927.926979	37.769575
1908.246901	357617.537645	37.774592
1910.372027	358320.774784	37.779610
1911.699319	359037.605416	37.784628
1913.886696	359711.121508	37.789645
1916.035714	360412.898739	37.794663
1918.009278	361107.284175	37.799680
1919.931789	361822.801410	37.804698
1921.717059	362535.893037	37.809716
1923.554205	363231.913981	37.814733
1925.833377	363931.731727	37.819751
1927.471857	364669.495667	37.824768
1929.456436	365385.091514	37.829786
1931.354554	366106.980270	37.834804
1933.175941	366810.120599	37.839821
1935.073628	367554.332787	37.844839
1937.499771	368287.661997	37.849856
1939.162014	369004.081475	37.854874
1940.839412	369753.107133	37.859892
1942.943002	370481.170889	37.864909
1945.064275	371203.916072	37.869927
1946.913107	371941.759385	37.874944
1949.188886	372687.811979	37.879962
1950.994353	373443.235829	37.884980
1952.985395	374142.051447	37.889997
1955.105520	374889.048592	37.895015
1957.030150	375648.972315	37.900032
1959.002518	376385.462400	37.905050
1960.787469	377135.283217	37.910068
1962.463033	377882.570019	37.915085
1964.443676	378640.518279	37.920103
1966.398472	379394.954598	37.925120
1968.391543	380128.649191	37.930138
1970.352319	380903.669127	37.935156
1972.294992	381659.934408	37.940173
1974.102339	382425.308760	37.945191
1976.183853	383173.250613	37.950208
1978.495696	383922.025306	37.955226
1980.139176	384702.233976	37.960244
1982.074583	385475.276504	37.965261
1984.570008	386256.702522	37.970279
1986.197531	387015.307094	37.975296
1988.286273	387786.799172	37.980314
1990.245184	388562.528272	37.985332
1992.831285	389318.081122	37.990349
1994.680478	390088.948962	37.995367
1996.423250	390867.750681	38.000384
1998.851774	391610.244237	38.005402
2000.647935	392374.042775	38.010420
2002.766953	393120.201977	38.015437
2004.617312	393888.694770	38.020455
2006.676950	394629.580058	38.025472
2008.943152	395371.655412	38.030490
2010.471317	396095.102770	38.035508
2012.649832	396841.769893	38.040525
2014.553806	397587.728761	38.045543
2016.407935	398338.214111	38.050560
2018.649147	399053.108680	38.055578
2020.192382	399813.796658	38.060596
2022.065167	400573.447607	38.065613
2024.521724	401321.324885	38.070631
2026.210857	402074.301960	38.075648
2028.479596	402840.341485	38.080666
2030.423991	403614.193793	38.085684
2032.486185	404359.295389	38.090701
2034.576918	405106.653374	38.095719
2036.704667	405882.745142	38.100736
2038.618779	406663.006255	38.105754
2040.683754	407440.357672	38.110772
2042.591074	408200.965880	38.115789
2044.962800	408986.888684	38.120807
2046.698932	409783.357418	38.125824
2048.841189	410573.605125	38.130842
2051.135643	411341.891125	38.135860
2052.823064	412128.824683	38.140877
2054.848733	412921.581990	38.145895
2056.952523	413709.515373	38.150912
2058.888826	414506.344298	38.155930
2060.725089	415320.694275	38.160948
2062.519659	416125.502261	38.165965
2064.907468	416935.000227	38.170983
2066.831001	417767.268700	38.176000
2068.926468	418581.246854	38.181018
2070.679633	419412.604272	38.186036
2072.682818	420249.819756	38.191053
2075.071521	421052.984210	38.196071
2077.002943	421901.148273	38.201088
2079.181192	422743.697578	38.206106
2080.980176	423591.269717	38.211124
2083.018313	424423.960953	38.216141
2085.239890	425250.567943	38.221159
2087.215976	426118.534472	38.226176
2089.291745	426986.428748	38.231194
2091.270942	427834.661845	38.236212
2093.721782	428688.053604	38.241229
2095.971117	429538.056319	38.246247
2097.803825	430406.020847	38.251264
2100.330373	431258.144958	38.256282
2102.416309	432103.324979	38.261300
2104.237101	432975.704053	38.266317
2106.669376	433843.141033	38.271335
2108.404297	434704.687859	38.276352
2110.545510	435556.265369	38.281370
2112.786512	436434.672956	38.286388
2114.722777	437323.068723	38.291405
2116.881237	438193.071757	38.296423
2118.833155	439067.985202	38.301440
2121.555163	439929.579781	38.306458
2123.945396	440829.455544	38.311476
2125.615451	441688.980700	38.316493
2127.878098	442542.049921	38.321511
2130.052551	443426.119898	38.326528
2131.949497	444305.899659	38.331546
2134.491512	445182.198751	38.336564
2136.271080	446056.817976	38.341581
2138.850967	446937.291039	38.346599
2140.414406	447821.336495	38.351616
2142.877715	448701.909363	38.356634
2145.232849	449565.264629	38.361652
2147.289619	450400.610312	38.366669
2149.415535	451237.379004	38.371687
2151.178883	452102.550817	38.376704
2153.449415	452950.508039	38.381722
2155.905759	453787.071367	38.386740
2157.814672	454625.563052	38.391757
2160.465638	455486.454495	38.396775
2162.148034	456355.966113	38.401792
2163.972479	457179.400212	38.406810
2166.220391	458038.027469	38.411828
2168.199717	458924.676131	38.416845
2170.503024	459775.131373	38.421863
2172.351429	460647.468359	38.426880
2174.377923	461527.878448	38.431898
2176.703072	462426.148402	38.436916
2178.506912	463305.860488	38.441933
2181.351858	464192.490097	38.446951
2183.015964	465088.020097	38.451968
2185.213503	465975.485920	38.456986
2187.804706	466885.288907	38.462004
2189.842354	467786.751127	38.467021
2191.821717	468672.109785	38.472039
2193.934462	469605.063422	38.477056
2196.577481	470525.857448	38.482074
2198.658107	471432.601716	38.487092
2201.018176	472337.387602	38.492109
2202.989222	473255.180692	38.497127
2204.933102	474192.386537	38.502144
2207.139442	475117.528913	38.507162
2209.410443	476051.507045	38.512180
2211.462080	476992.598112	38.517197
2213.967793	477943.973300	38.522215
2215.978559	478877.752577	38.527232
2218.315883	479825.523530	38.532250
2220.301094	480768.101692	38.537268
2222.258456	481710.535218	38.542285
2224.811250	482669.740542	38.547303
2226.744247	483636.370680	38.552320
2228.863623	484608.877371	38.557338
2231.390436	485593.534796	38.562356
2233.404626	486578.727847	38.567373
2236.143454	487545.066363	38.572391
2238.168046	488505.664422	38.577408
2240.502304	489481.456034	38.582426
2242.619982	490463.792057	38.587444
2244.959987	491432.710486	38.592461
2247.477421	492425.319926	38.597479
2249.348527	493421.714472	38.602496
2252.093926	494386.970057	38.607514
2254.502553	495351.874086	38.612532
2256.893252	496347.005287	38.617549
2259.002727	497318.812295	38.622567
2261.443607	498320.279552	38.627584
2263.943951	499282.373687	38.632602
2266.093268	500266.871796	38.637620
2268.105250	501252.646788	38.642637
2270.133206	502229.381905	38.647655
2272.721194	503221.655491	38.652672
2274.727964	504225.365278	38.657690
2277.236712	505201.493794	38.662708
2279.944105	506195.738592	38.667725
2282.051533	507190.929978	38.672743
2284.583526	508180.141259	38.677760
2286.516033	509143.119994	38.682778
2288.868409	510114.191216	38.687796
2291.093151	511123.442729	38.692813
2293.575786	512101.532426	38.697831
2295.852233	513088.166663	38.702848
2297.971556	514050.518893	38.707866
2300.716915	514989.573096	38.712884
2302.740766	515934.638279	38.717901
2304.925091	516892.825425	38.722919
2307.502340	517856.634756	38.727936
2309.566851	518804.191965	38.732954
2311.727006	519765.583917	38.737972
2313.785120	520728.041813	38.742989
2316.173099	521671.541512	38.748007
2318.256454	522650.502680	38.753024
2320.154371	523651.749850	38.758042
2322.577567	524632.594059	38.763060
2324.769753	525619.206086	38.768077
2327.619952	526593.959981	38.773095
2329.385914	527611.539883	38.778112
2331.628679	528628.065987	38.783130
2334.159108	529620.303657	38.788148
2336.021148	530641.338638	38.793165
2338.524786	531653.789110	38.798183
2340.865901	532663.730233	38.803200
2342.893518	533680.400287	38.808218
2345.092923	534711.872922	38.813236
2347.545838	535763.165040	38.818253
2350.235504	536806.993671	38.823271
2352.438488	537847.807823	38.828288
2354.794772	538893.554668	38.833306
2357.074395	539928.066614	38.838324
2359.281606	540997.437972	38.843341
2361.592849	542058.460536	38.848359
2363.950791	543149.432836	38.853376
2366.399476	544204.839084	38.858394
2368.908325	545258.647575	38.863412
2371.157446	546359.451299	38.868429
2373.686557	547438.494971	38.873447
2376.283360	548507.938871	38.878464
2379.009250	549583.816962	38.883482
2381.781994	550663.978712	38.888500
2383.643838	551729.322987	38.893517
2386.383072	552778.451991	38.898535
2388.925167	553875.594663	38.903552
2391.604760	554962.723502	38.908570
2394.644180	556024.674013	38.913588
2397.086460	557087.293177	38.918605
2399.598638	558152.179319	38.923623
2401.948965	559213.841894	38.928640
2404.670291	560293.248051	38.933658
2406.986702	561350.425217	38.938676
2409.508095	562422.858477	38.943693
2411.850087	563482.825903	38.948711
2414.261482	564535.061332	38.953728
2416.764986	565620.449235	38.958746
2419.624879	566686.753628	38.963764
2422.114085	567738.668826	38.968781
2424.738763	568785.053205	38.973799
2427.019350	569832.112835	38.978816
2429.120304	570910.999852	38.983834
2431.560240	571965.341099	38.988852
2433.872842	573035.831428	38.993869
2436.376873	574098.018523	38.998887
2438.932026	575150.923412	39.003904
2441.199855	576225.268723	39.008922
2443.770905	577290.640421	39.013940
2446.177388	578346.967016	39.018957
2448.808970	579399.805859	39.023975
2451.361511	580467.269197	39.028992
2453.681565	581530.314931	39.034010
2456.129769	582597.261533	39.039028
2458.719500	583658.525274	39.044045
2461.498855	584682.251689	39.049063
2464.216283	585683.185202	39.054080
2466.076990	586702.581604	39.059098
2468.836175	587709.159284	39.064116
2471.068110	588730.079874	39.069133
2473.622348	589750.410200	39.074151
2475.944228	590794.303342	39.079168
2478.035951	591820.550323	39.084186
2480.817958	592841.583793	39.089204
2483.272788	593889.245694	39.094221
2485.453546	594901.331763	39.099239
2488.010845	595945.488510	39.104256
2489.853727	596999.140422	39.109274
2492.419666	598077.277516	39.114292
2494.670734	599135.681013	39.119309
2497.142217	600196.907936	39.124327
2499.756403	601259.467455	39.129344
2501.841865	602340.697011	39.134362
2504.152222	603422.339661	39.139380
2506.685615	604531.984006	39.144397
2508.985678	605630.345383	39.149415
2512.057971	606727.723595	39.154432
2513.748598	607858.962085	39.159450
2516.302963	608966.121890	39.164468
2518.672648	610084.064372	39.169485
2521.106165	611221.402095	39.174503
2523.981070	612360.203747	39.179520
2525.836555	613514.167553	39.184538
2528.790292	614662.528920	39.189556
2531.218996	615809.108144	39.194573
2533.651533	616951.417457	39.199591
2536.029142	618122.974263	39.204608
2538.605790	619297.474494	39.209626
2541.417117	620452.011105	39.214644
2543.327087	621619.873425	39.219661
2546.105220	622820.510665	39.224679
2548.670880	624009.904508	39.229696
2551.111801	625196.739854	39.234714
2553.593625	626402.777685	39.239732
2556.069917	627622.622346	39.244749
2558.768012	628820.359223	39.249767
2561.582721	630003.056278	39.254784
2563.794203	631238.318929	39.259802
2566.370530	632428.678180	39.264820
2569.372246	633652.891663	39.269837
2571.726271	634884.010670	39.274855
2574.146682	636123.412378	39.279872
2576.786684	637341.664749	39.284890
2579.768469	638562.813529	39.289908
2582.191562	639797.286861	39.294925
2584.645852	641026.667833	39.299943
2587.791616	642265.518652	39.304960
2590.059533	643482.313345	39.309978
2592.862043	644701.170499	39.314996
2595.582909	645940.047196	39.320013
2597.972902	647168.204957	39.325031
2600.711130	648399.747361	39.330048
2603.433046	649646.549782	39.335066
2606.035512	650891.622521	39.340084
2608.746785	652110.701545	39.345101
2611.508721	653358.532710	39.350119
2614.427964	654581.712372	39.355136
2616.589348	655804.816822	39.360154
2619.176709	657053.808145	39.365172
2622.011265	658296.124635	39.370189
2624.140310	659534.615097	39.375207
2626.804253	660753.188114	39.380224
2629.660172	661996.626699	39.385242
2632.128293	663217.663537	39.390260
2634.592875	664419.529126	39.395277
2636.747323	665642.104954	39.400295
2639.728911	666852.294594	39.405312
2642.113031	668053.074190	39.410330
2644.277075	669269.763009	39.415348
2647.011704	670506.353829	39.420365
2649.339810	671746.731601	39.425383
2652.042786	672959.875630	39.430400
2654.464193	674215.036813	39.435418
2657.047124	675454.588425	39.440436
2659.536700	676693.942342	39.445453
2661.829938	677970.551105	39.450471
2664.689335	679246.345332	39.455488
2667.270774	680524.644776	39.460506
2669.660428	681802.998533	39.465524
2671.921374	683106.835999	39.470541
2674.695828	684400.915292	39.475559
2677.240724	685701.407112	39.480576
2679.789602	687024.957740	39.485594
2681.969056	688338.544603	39.490612
2685.089363	689669.065754	39.495629
2687.796025	690991.019980	39.500647
2690.335108	692346.313923	39.505664
2692.621920	693687.300652	39.510682
2695.307715	695038.888544	39.515700
2698.007884	696420.485408	39.520717
2700.892520	697805.756506	39.525735
2703.859884	699159.450559	39.530752
2706.740418	700550.840170	39.535770
2709.182754	701942.726879	39.540788
2711.767186	703322.768636	39.545805
2714.360087	704713.892987	39.550823
2717.533989	706104.897869	39.555840
2720.214649	707499.874199	39.560858
2723.067834	708887.165622	39.565876
2725.618581	710308.216460	39.570893
2728.451149	711728.094462	39.575911
2731.588333	713112.775113	39.580928
2734.278488	714509.286813	39.585946
2737.471031	715918.110029	39.590964
2740.226484	717334.541992	39.595981
2743.123076	718750.366807	39.600999
2745.830022	720144.560269	39.606016
2748.271932	721553.209152	39.611034
2751.302999	722954.598858	39.616052
2754.413283	724385.857424	39.621069
2756.845470	725798.191671	39.626087
2759.912614	727196.980470	39.631104
2762.303992	728612.498616	39.636122
2765.262536	730036.328052	39.641140
2768.019948	731453.618399	39.646157
2770.555288	732889.917030	39.651175
2773.592931	734306.417904	39.656192
2776.283083	735729.642506	39.661210
2778.814894	737145.976578	39.666228
2782.270340	738571.782942	39.671245
2784.765795	740007.908961	39.676263
2787.338063	741428.909886	39.681280
2790.339581	742876.033875	39.686298
2793.242348	744301.204048	39.691316
2796.416256	745709.500073	39.696333
2799.150562	747151.644521	39.701351
2801.941354	748573.003847	39.706368
2804.977406	749977.156010	39.711386
2807.584538	751404.439734	39.716404
2810.419346	752826.890557	39.721421
2813.225046	754229.180219	39.726439
2816.216050	755623.401754	39.731456
2818.809901	757011.871003	39.736474
2821.275453	758381.742611	39.741492
2824.283686	759759.108103	39.746509
2826.710178	761137.108552	39.751527
2829.447108	762533.461531	39.756544
2832.201798	763939.986575	39.761562
2834.745452	765324.981747	39.766580
2837.577571	766714.298702	39.771597
2840.129541	768146.732784	39.776615
2842.950872	769554.066364	39.781632
2845.954295	770990.208240	39.786650
2848.280575	772436.457228	39.791668
2851.594012	773869.582779	39.796685
2854.129512	775295.041297	39.801703
2856.726256	776733.231630	39.806720
2859.398823	778200.350398	39.811738
2861.831696	779658.474158	39.816756
2864.959181	781140.689832	39.821773
2867.507300	782650.038369	39.826791
2870.563233	784119.730178	39.831808
2873.238788	785598.262349	39.836826
2875.740158	787115.320678	39.841844
2879.116655	788619.604321	39.846861
2881.889939	790125.436054	39.851879
2884.768809	791663.973034	39.856896
2887.560158	793196.358838	39.861914
2890.551974	794714.071687	39.866932
2893.451473	796231.277281	39.871949
2896.165652	797773.361507	39.876967
2898.975988	799328.703822	39.881984
2902.144110	800865.820208	39.887002
2904.788142	802432.100515	39.892020
2908.042151	804002.086189	39.897037
2910.744158	805576.649764	39.902055
2913.140391	807137.550539	39.907072
2916.332275	808719.286713	39.912090
2919.144672	810281.407886	39.917108
2922.247475	811897.281822	39.922125
2924.906814	813491.293932	39.927143
2927.712197	815069.907912	39.932160
2930.989913	816660.676819	39.937178
2933.539014	818275.020139	39.942196
2936.810003	819859.855802	39.947213
2939.680663	821485.137595	39.952231
2942.836547	823108.316474	39.957248
2945.731126	824705.235951	39.962266
2948.656044	826332.589921	39.967284
2951.707066	827937.968389	39.972301
2954.458087	829589.316218	39.977319
2957.275133	831207.777230	39.982336
2960.555207	832828.293999	39.987354
2963.425905	834464.403367	39.992372
2966.603602	836082.370371	39.997389
2969.587494	837717.345602	40.002407
2972.335853	839360.462415	40.007424
2975.029272	840982.874302	40.012442
2977.945374	842634.563521	40.017460
2980.976520	844285.610733	40.022477
2984.173845	845935.179769	40.027495
2987.136674	847571.814827	40.032512
2990.504582	849219.719443	40.037530
2993.092668	850863.141537	40.042548
2996.850760	852495.544248	40.047565
2999.813319	854156.011210	40.052583
3002.558283	855787.135033	40.057600
3005.879886	857432.683714	40.062618
3008.772879	859068.062644	40.067636
3011.965162	860662.208421	40.072653
3014.622682	862247.201221	40.077671
3017.822975	863834.990746	40.082688
3020.859010	865440.716501	40.087706
3023.197004	867033.726906	40.092724
3026.596403	868626.337113	40.097741
3029.449656	870239.637670	40.102759
3031.983353	871835.901086	40.107776
3034.903291	873457.526227	40.112794
3037.451509	875088.838849	40.117812
3040.384118	876698.643460	40.122829
3043.320469	878353.574633	40.127847
3045.998468	880002.476303	40.132864
3049.240099	881646.956771	40.137882
3051.537296	883322.449452	40.142900
3055.008187	884993.404495	40.147917
3058.075863	886665.686556	40.152935
3061.312512	888347.986674	40.157952
3064.489074	890048.538378	40.162970
3067.672517	891745.789668	40.167988
3070.607323	893449.046531	40.173005
3073.486999	895151.324893	40.178023
3076.444677	896855.591174	40.183040
3079.735753	898568.354915	40.188058
3082.473090	900307.003204	40.193076
3085.574397	902054.788375	40.198093
3088.403504	903788.015631	40.203111
3091.259647	905542.464203	40.208128
3094.561184	907281.178751	40.213146
3097.175483	909046.984842	40.218164
3100.244470	910806.384531	40.223181
3103.438090	912600.496625	40.228199
3106.455993	914391.267726	40.233216
3109.566229	916177.789848	40.238234
3112.797178	917987.919422	40.243252
3115.816325	919766.657940	40.248269
3119.126944	921555.328477	40.253287
3122.008260	923385.228281	40.258304
3125.407556	925198.114746	40.263322
3128.155072	927021.049041	40.268340
3131.267092	928834.293067	40.273357
3134.584606	930655.994401	40.278375
3137.524397	932500.513446	40.283392
3140.724153	934327.685291	40.288410
3143.902252	936181.804428	40.293428
3146.829281	938009.664351	40.298445
3150.282735	939854.502599	40.303463
3153.523112	941696.622895	40.308480
3156.773246	943559.221399	40.313498
3159.703874	945416.810016	40.318516
3162.606785	947264.184429	40.323533
3166.302840	949118.695065	40.328551
3169.319254	950956.611213	40.333568
3172.781614	952819.945392	40.338586
3175.642478	954703.306523	40.343604
3179.002960	956560.049549	40.348621
3182.431442	958469.663041	40.353639
3185.453540	960385.850463	40.358656
3188.939404	962297.610267	40.363674
3191.933856	964197.774068	40.368692
3194.894810	966102.005628	40.373709
3198.423096	968029.635366	40.378727
3201.569300	969951.019309	40.383744
3205.162716	971860.951501	40.388762
3207.992645	973772.422534	40.393780
3211.003008	975683.811791	40.398797
3214.183167	977595.315296	40.403815
3217.534874	979506.249598	40.408832
3220.329821	981400.365978	40.413850
3223.465602	983282.305185	40.418868
3226.648773	985145.603175	40.423885
3229.668068	987016.008938	40.428903
3232.708599	988897.960245	40.433920
3236.309823	990769.372726	40.438938
3239.066334	992670.161107	40.443956
3242.003128	994565.618243	40.448973
3245.364650	996458.817976	40.453991
3248.429722	998344.634877	40.459008
3251.914519	1000255.003701	40.464026
3255.061023	1002185.266917	40.469044
3258.289950	1004095.546563	40.474061
3261.413844	1006038.569523	40.479079
3264.579944	1007982.856701	40.484096
3267.944963	1009911.221203	40.489114
3270.510225	1011877.337274	40.494132
3273.607087	1013839.773375	40.499149
3277.135364	1015804.940463	40.504167
3280.302611	1017781.097131	40.509184
3283.532857	1019757.612795	40.514202
3286.671264	1021757.922621	40.519220
3289.678793	1023763.729555	40.524237
3293.243813	1025760.606242	40.529255
3295.974010	1027796.431785	40.534272
3299.854304	1029818.382354	40.539290
3303.082120	1031836.618411	40.544308
3305.781458	1033859.424306	40.549325
3309.413944	1035914.054427	40.554343
3312.423213	1037970.344332	40.559360
3315.841510	1040025.710668	40.564378
3319.423447	1042099.856812	40.569396
3322.994918	1044159.451850	40.574413
3325.979126	1046197.382256	40.579431
3329.418966	1048273.193123	40.584448
3332.796317	1050335.147019	40.589466
3335.890004	1052431.591263	40.594484
3339.036881	1054522.134535	40.599501
3342.997740	1056600.504487	40.604519
3346.077295	1058697.360080	40.609536
3349.387057	1060792.899631	40.614554
3353.076724	1062904.479398	40.619572
3356.324253	1065007.738175	40.624589
3359.726861	1067099.515655	40.629607
3363.005308	1069212.576852	40.634624
3366.302221	1071314.753556	40.639642
3369.544301	1073446.130778	40.644660
3372.460940	1075574.911227	40.649677
3376.420880	1077685.548787	40.654695
3379.778211	1079798.437428	40.659712
3383.049867	1081926.693865	40.664730
3386.082829	1084084.002707	40.669748
3389.145846	1086214.157362	40.674765
3392.461381	1088355.861482	40.679783
3395.571305	1090512.615108	40.684800
3399.048528	1092668.546795	40.689818
3402.240507	1094842.952138	40.694836
3405.537651	1096996.904872	40.699853
3408.685972	1099186.653847	40.704871
3411.971047	1101364.432702	40.709888
3415.644852	1103532.119326	40.714906
3419.053031	1105709.363282	40.719924
3422.058702	1107887.603233	40.724941
3425.704525	1110082.277113	40.729959
3428.500391	1112292.752397	40.734976
3432.261899	1114482.850211	40.739994
3435.636513	1116674.684871	40.745012
3439.299218	1118861.258139	40.750016
3442.752214	1120995.171880	40.755021
3445.804286	1123051.562974	40.760026
3449.337693	1125052.549768	40.765031
3452.801928	1126977.258572	40.770036
3455.930542	1128797.948992	40.775040
3459.340104	1130580.131647	40.780045
3462.421772	1132288.683713	40.785050
3465.244890	1133892.974423	40.790055
3467.638821	1135434.635285	40.795060
3470.359995	1136872.192793	40.800064
3473.288006	1138243.725786	40.805069
3475.587916	1139564.893493	40.810074
3478.045650	1140777.340841	40.815079
3480.564903	1141933.242381	40.820084
3482.377044	1143029.062331	40.825088
3484.408350	1144014.992853	40.830093
3486.114745	1144970.925967	40.835098
3488.413147	1145856.721222	40.840103
3490.015854	1146705.895527	40.845108
3491.865059	1147461.259138	40.850112
3493.694438	1148163.074078	40.855117
3494.985309	1148833.428429	40.860122
3496.541226	1149438.381154	40.865127
3498.204509	1149997.967916	40.870132
3499.400379	1150505.572894	40.875136
3500.864081	1150965.446619	40.880141
3501.927209	1151393.905533	40.885146
3503.085021	1151755.365438	40.890151
3504.321838	1152101.353351	40.895156
3505.210328	1152403.064514	40.900160
3506.596109	1152663.207621	40.905165
3507.575332	1152884.967254	40.910170
3508.742284	1153096.083550	40.915175
3509.238204	1153226.172026	40.920180
3509.867661	1153351.596673	40.925184
3510.953917	1153452.709187	40.930189
3511.456497	1153533.184837	40.935194
3512.501651	1153582.237004	40.940199
3513.176339	1153621.505000	40.945204
3513.577413	1153617.936530	40.950208
3514.307064	1153580.141208	40.955213
3514.855197	1153538.683681	40.960218
3515.469811	1153487.653896	40.965223
3516.168653	1153410.293033	40.970228
3516.324796	1153300.171190	40.975232
3517.083544	1153161.452465	40.980237
3517.360341	1153044.299883	40.985242
3517.657229	1152876.774922	40.990247
3518.385243	1152724.511328	40.995252
3518.508995	1152550.093072	41.000256
3518.908746	1152354.793227	41.005261
3518.979756	1152147.893755	41.010266
3519.212562	1151942.853332	41.015271
3519.516480	1151731.353976	41.020276
3519.783533	1151495.988094	41.025280
3520.124795	1151252.739102	41.030285
3520.044804	1151010.305927	41.035290
3520.415206	1150736.627035	41.040295
3520.812934	1150467.286448	41.045300
3521.136709	1150193.681780	41.050304
3521.494525	1149911.626570	41.055309
3521.282026	1149621.976862	41.060314
3521.806132	1149321.579272	41.065319
3521.819955	1149015.090292	41.070324
3522.042762	1148699.737414	41.075328
3522.249675	1148369.586519	41.080333
3522.154149	1148058.227458	41.085338
3522.554813	1147722.034222	41.090343
3522.690913	1147409.651096	41.095348
3522.702783	1147059.074257	41.100352
3523.023520	1146709.371129	41.105357
3522.703557	1146357.759754	41.110362
3522.874392	1145997.322751	41.115367
3522.990422	1145653.271302	41.120372
3522.892792	1145301.647828	41.125376
3523.587328	1144929.579711	41.130381
3523.372394	1144570.436378	41.135386
3523.385673	1144199.756640	41.140391
3523.661491	1143817.153086	41.145396
3523.846445	1143449.047900	41.150400
3523.671475	1143072.155318	41.155405
3523.553633	1142681.567053	41.160410
3524.034388	1142294.266486	41.165415
3523.943532	1141924.867474	41.170420
3523.859132	1141535.232693	41.175424
3524.192408	1141118.173571	41.180429
3524.001952	1140721.949337	41.185434
3523.849675	1140344.004736	41.190439
3524.014589	1139949.087659	41.195444
3523.876148	1139562.923130	41.200448
3524.242563	1139147.601711	41.205453
3524.184502	1138753.676425	41.210458
3524.150423	1138351.838342	41.215463
3524.436175	1137959.411328	41.220468
3524.472949	1137536.802480	41.225472
3524.410990	1137121.013127	41.230477
3524.499403	1136712.953493	41.235482
3524.647751	1136291.841520	41.240487
3524.431157	1135874.460438	41.245492
3524.298462	1135463.586795	41.250496
3524.232864	1135033.386534	41.255501
3524.112164	1134630.805972	41.260506
3524.373617	1134204.949831	41.265511
3524.485086	1133779.274305	41.270516
3524.362713	1133374.983602	41.275520
3524.095713	1132947.403320	41.280525
3524.080959	1132538.184657	41.285530
3524.068830	1132117.148350	41.290535
3524.135853	1131692.168477	41.295540
3524.247999	1131285.399001	41.300544
3524.215643	1130855.805770	41.305549
3523.951389	1130428.973278	41.310554
3523.692761	1130017.794479	41.315559
3523.678792	1129591.709397	41.320564
3523.667465	1129195.926284	41.325568
3524.015623	1128779.511733	41.330573
3524.149497	1128361.387901	41.335578
3524.002480	1127921.589942	41.340583
3523.795873	1127492.039435	41.345588
3523.670817	1127098.687773	41.350592
3524.074732	1126666.401539	41.355597
3524.068905	1126251.179816	41.360602
3524.263324	1125808.296794	41.365607
3523.972579	1125392.864883	41.370612
3523.598545	1124966.088664	41.375616
3523.904384	1124538.975984	41.380621
3523.538003	1124105.181424	41.385626
3523.738458	1123685.823382	41.390631
3523.679779	1123262.476523	41.395636
3523.711937	1122839.366793	41.400640
3523.672846	1122415.092665	41.405645
3523.540761	1122010.512109	41.410650
3523.197849	1121582.984265	41.415655
3523.442170	1121169.040317	41.420660
3523.385097	1120739.016883	41.425664
3523.251071	1120306.018589	41.430669
3523.140649	1119895.082709	41.435674
3523.151362	1119492.383939	41.440679
3522.952918	1119059.962325	41.445684
3523.095853	1118644.124717	41.450688
3523.610301	1118212.279532	41.455693
3523.256311	1117801.223030	41.460698
3523.555043	1117373.443721	41.465703
3523.231144	1116959.267764	41.470708
3523.380919	1116533.066288	41.475712
3523.338720	1116119.064978	41.480717
3523.274050	1115689.781175	41.485722
3523.088076	1115263.629422	41.490727
3522.998259	1114833.899863	41.495732
3522.882495	1114426.168702	41.500736
3523.377812	1114007.624605	41.505741
3522.961757	1113600.452377	41.510746
3522.859565	1113174.120847	41.515751
3523.246473	1112738.517336	41.520756
3523.012097	1112332.459099	41.525760
3523.152019	1111905.509986	41.530765
3522.839717	1111486.520769	41.535770
3522.800073	1111071.270814	41.540775
3522.843284	1110645.477987	41.545780
3522.572651	1110233.923099	41.550784
3522.878829	1109818.710303	41.555789
3522.366419	1109386.037318	41.560794
3522.525592	1108957.037255	41.565799
3522.545558	1108556.665705	41.570804
3522.386128	1108142.259389	41.575808
3522.606860	1107718.974345	41.580813
3522.438340	1107307.560640	41.585818
3522.587548	1106880.592928	41.590823
3522.830899	1106450.806277	41.595828
3522.170655	1106044.820751	41.600832
3522.757141	1105625.990968	41.605837
3522.302762	1105231.181293	41.610842
3522.566324	1104796.578654	41.615847
3522.504843	1104367.058140	41.620852
3522.183305	1103947.387633	41.625856
3522.254688	1103542.621839	41.630861
3522.119795	1103123.716488	41.635866
3522.138144	1102706.855896	41.640871
3522.170090	1102294.548547	41.645876
3522.126705	1101868.649163	41.650880
3522.247529	1101454.638093	41.655885
3521.746781	1101053.985881	41.660890
3521.800570	1100642.887174	41.665895
3521.789675	1100230.811701	41.670900
3521.912396	1099828.627318	41.675904
3522.097273	1099404.790918	41.680909
3521.509545	1098996.445799	41.685914
3521.483365	1098593.811513	41.690919
3521.887390	1098184.859183	41.695924
3521.580400	1097777.140919	41.700928
3521.797987	1097377.245612	41.705933
3521.811402	1096971.135775	41.710938
3521.362836	1096536.846443	41.715943
3521.558100	1096138.107067	41.720948
3521.310540	1095739.985411	41.725952
3521.524677	1095321.470066	41.730957
3521.436219	1094925.654834	41.735962
3521.176541	1094511.270321	41.740967
3521.200871	1094126.193807	41.745972
3521.107095	1093740.726468	41.750976
3521.038391	1093319.231185	41.755981
3521.321932	1092917.080879	41.760986
3520.986470	1092529.652370	41.765991
3521.089312	1092130.154448	41.770996
3520.988835	1091721.850344	41.776000
3520.787859	1091330.579238	41.781005
3520.726829	1090939.927305	41.786010
3520.522469	1090530.592884	41.791015
3520.921440	1090115.572292	41.796020
3521.115040	1089736.670018	41.801024
3520.894404	1089340.564545	41.806029
3520.786810	1088936.842358	41.811034
3520.902030	1088536.886260	41.816039
3521.038624	1088134.597358	41.821044
3520.900300	1087733.665632	41.826048
3520.802317	1087332.697685	41.831053
3520.716645	1086931.698133	41.836058
3520.580038	1086527.514173	41.841063
3520.268917	1086141.446868	41.846068
3520.231009	1085777.836289	41.851072
3520.414853	1085370.925155	41.856077
3520.345046	1084980.517186	41.861082
3520.146482	1084579.075127	41.866087
3520.579735	1084178.746057	41.871092
3520.473159	1083782.312615	41.876096
3520.492276	1083392.735166	41.881101
3519.991221	1083039.663981	41.886106
3520.200929	1082638.970804	41.891111
3520.199532	1082252.384740	41.896116
3520.021136	1081867.431337	41.901120
3519.991320	1081458.248310	41.906125
3519.924614	1081075.235399	41.911130
3519.918154	1080686.524136	41.916135
3519.838026	1080301.635897	41.921140
3519.733730	1079934.095316	41.926144
3519.997082	1079545.546223	41.931149
3519.681698	1079159.752364	41.936154
3519.556308	1078762.764883	41.941159
3519.685565	1078396.426152	41.946164
3519.660218	1078028.168210	41.951168
3519.593408	1077642.706209	41.956173
3519.673897	1077241.157646	41.961178
3519.633634	1076862.837635	41.966183
3519.356918	1076494.901813	41.971188
3519.125351	1076100.042997	41.976192
3519.441078	1075733.398912	41.981197
3519.236642	1075360.476502	41.986202
3519.238041	1074977.504682	41.991207
3519.359515	1074607.935374	41.996212
3519.350093	1074235.480512	42.001216
3519.073702	1073856.607030	42.006221
3519.242837	1073502.039412	42.011226
3519.254343	1073111.921154	42.016231
3519.125329	1072734.483163	42.021236
3518.864795	1072377.318811	42.026240
3519.060762	1071991.895559	42.031245
3519.031118	1071615.132924	42.036250
3518.806810	1071244.239999	42.041255
3519.025844	1070869.595982	42.046260
3518.712926	1070509.819063	42.051264
3518.810621	1070136.106256	42.056269
3518.565323	1069774.154746	42.061274
3518.457837	1069395.136977	42.066279
3518.826265	1069043.036380	42.071284
3518.544701	1068690.635561	42.076288
3518.715197	1068319.960547	42.081293
3518.519998	1067947.108538	42.086298
3518.331263	1067569.035952	42.091303
3518.704839	1067218.933590	42.096308
3518.444167	1066866.893149	42.101312
3518.392613	1066494.592199	42.106317
3518.405613	1066126.392563	42.111322
3518.222668	1065763.396399	42.116327
3518.587165	1065399.612495	42.121332
3518.193811	1065049.690600	42.126336
3518.090086	1064679.681025	42.131341
3518.086533	1064328.397883	42.136346
3517.874902	1063968.367680	42.141351
3518.248329	1063623.715022	42.146356
3517.961097	1063259.993093	42.151360
3518.215573	1062892.403341	42.156365
3518.142958	1062546.793959	42.161370
3517.763119	1062165.299995	42.166375
3518.157541	1061806.472674	42.171380
3517.842451	1061476.145954	42.176384
3518.005461	1061126.941952	42.181389
3517.779650	1060769.786325	42.186394
3517.742951	1060402.752369	42.191399
3517.970158	1060050.676433	42.196404
3517.766977	1059688.630944	42.201408
3517.706134	1059332.703504	42.206413
3517.681184	1059003.721965	42.211418
3517.669325	1058647.067798	42.216423
3517.906891	1058294.974309	42.221428
3517.550838	1057941.799820	42.226432
3517.573091	1057571.676825	42.231437
3517.587357	1057220.515131	42.236442
3517.249608	1056876.520850	42.241447
3517.335986	1056549.687526	42.246452
3517.192386	1056195.691529	42.251456
3517.514546	1055847.379722	42.256461
3517.069850	1055512.571766	42.261466
3517.020301	1055161.096690	42.266471
3517.555103	1054796.969467	42.271476
3517.020908	1054471.368620	42.276480
3517.208957	1054121.138057	42.281485
3517.106980	1053788.676106	42.286490
3516.905785	1053454.667520	42.291495
3517.025121	1053112.195563	42.296500
3516.733076	1052773.435131	42.301504
3516.613503	1052435.300695	42.306509
3516.298654	1052108.559881	42.311514
3516.242907	1051758.316157	42.316519
3516.692997	1051435.654045	42.321524
3516.591252	1051131.587392	42.326528
3516.558209	1050790.057901	42.331533
3516.535146	1050453.330065	42.336538
3516.527042	1050114.842387	42.341543
3516.831927	1049774.738464	42.346548
3516.225861	1049456.477356	42.351552
3516.849632	1049131.625683	42.356557
3516.329421	1048805.109561	42.361562
3516.043651	1048456.528484	42.366567
3516.368302	1048130.895199	42.371572
3516.209452	1047805.901610	42.376576
3516.373947	1047464.906663	42.381581
3516.567730	1047156.614800	42.386586
3516.129027	1046823.210224	42.391591
3516.356662	1046501.841973	42.396596
3516.463874	1046190.807066	42.401600
3516.313166	1045836.824549	42.406605
3515.956189	1045510.570150	42.411610
3515.859975	1045175.271704	42.416615
3516.120780	1044844.143946	42.421620
3515.843521	1044524.482791	42.426624
3516.090464	1044211.092245	42.431629
3515.975116	1043889.435907	42.436634
3515.577124	1043578.627518	42.441639
3515.739794	1043252.154690	42.446644
3515.574258	1042949.388273	42.451648
3515.762515	1042610.602963	42.456653
3515.685697	1042277.928344	42.461658
3515.737895	1041991.790829	42.466663
3515.782226	1041657.802862	42.471668
3515.526543	1041349.552178	42.476672
3515.414920	1041050.345904	42.481677
3515.583517	1040722.080307	42.486682
3515.204914	1040398.235276	42.491687
3515.577469	1040083.624481	42.496692
3515.547257	1039789.750356	42.501696
3515.571309	1039468.201663	42.506701
3515.069976	1039165.380987	42.511706
3515.302351	1038859.038844	42.516711
3515.507825	1038529.767545	42.521716
3515.200266	1038219.127812	42.526720
3515.185727	1037897.591387	42.531725
3515.348269	1037615.078649	42.536730
3514.843754	1037299.777894	42.541735
3515.048332	1036971.865324	42.546740
3514.737649	1036689.480278	42.551744
3515.000602	1036368.486921	42.556749
3514.893039	1036058.564252	42.561754
3514.670385	1035783.567602	42.566759
3514.487460	1035486.589058	42.571764
3514.336098	1035180.978439	42.576768
3514.533581	1034868.714008	42.581773
3514.807711	1034592.512403	42.586778
3514.492481	1034297.427547	42.591783
3514.632940	1034001.671371	42.596788
3514.725368	1033717.617668	42.601792
3514.620716	1033411.128088	42.606797
3514.763611	1033108.742837	42.611802
3514.511020	1032795.178148	42.616807
3514.848230	1032505.698697	42.621812
3514.547054	1032222.311274	42.626816
3514.569312	1031914.266479	42.631821
3514.549283	1031624.896993	42.636826
3514.545845	1031319.534432	42.641831
3514.271212	1031034.145890	42.646836
3514.246796	1030750.444492	42.651840
3514.455644	1030439.576345	42.656845
3514.120322	1030155.024385	42.661850
3514.099773	1029862.852125	42.666855
3514.408180	1029545.816568	42.671860
3514.027420	1029260.548566	42.676864
3514.239254	1028972.262562	42.681869
3514.217914	1028695.333416	42.686874
3513.853836	1028405.369442	42.691879
3514.159329	1028095.033037	42.696884
3513.797188	1027824.995117	42.701888
3514.118648	1027542.720843	42.706893
3514.032172	1027248.872615	42.711898
3513.706236	1026979.175448	42.716903
3514.071809	1026673.498161	42.721908
3513.889051	1026406.656836	42.726912
3514.041858	1026104.278289	42.731917
3514.120465	1025824.186264	42.736922
3514.060605	1025523.652775	42.741927
3514.040986	1025245.098687	42.746932
3513.518873	1024952.267774	42.751936
3513.450346	1024662.254906	42.756941
3513.653444	1024412.024787	42.761946
3513.828803	1024118.259861	42.766951
3513.844157	1023837.012451	42.771956
3513.536794	1023536.897842	42.776960
3513.908954	1023268.264235	42.781965
3513.671251	1022994.869975	42.786970
3513.375715	1022720.599177	42.791975
3513.278865	1022432.027024	42.796980
3513.329082	1022159.029440	42.801985
3513.691937	1021894.695606	42.806989
3513.281612	1021611.466945	42.811994
3513.190960	1021341.265418	42.816999
3513.191641	1021053.188197	42.822004
3513.304894	1020790.492409	42.827009
3513.001904	1020511.846660	42.832013
3513.366888	1020255.389846	42.837018
3512.795236	1019999.754699	42.842023
3513.023288	1019706.817100	42.847028
3513.179656	1019457.828856	42.852033
3513.115220	1019170.441910	42.857037
3513.139751	1018895.543189	42.862042
3513.043930	1018635.789085	42.867047
3513.281907	1018353.938859	42.872052
3512.837378	1018078.786278	42.877057
3513.064616	1017814.185538	42.882061
3512.646865	1017568.022637	42.887066
3512.741180	1017296.140010	42.892071
3513.075843	1017015.080267	42.897076
3512.786992	1016760.415834	42.902081
3512.838570	1016485.685946	42.907085
3512.879579	1016222.400019	42.912090
3512.688932	1015973.411566	42.917095
3512.960792	1015719.578488	42.922100
3512.593787	1015452.051716	42.927105
3512.845244	1015179.166974	42.932109
3512.670634	1014913.719097	42.937114
3512.420354	1014656.136964	42.942119
3512.612371	1014380.892688	42.947124
3512.477694	1014123.849827	42.952129
3512.669666	1013867.615525	42.957133
3512.416719	1013620.281363	42.962138
3512.303978	1013357.760811	42.967143
3512.428382	1013080.132921	42.972148
3512.588001	1012834.056166	42.977153
3512.417041	1012563.736969	42.982157
3512.353205	1012321.171820	42.987162
3512.123481	1012070.656983	42.992167
3512.286377	1011819.289077	42.997172
3512.340599	1011568.316506	43.002177
3512.492946	1011320.523081	43.007181
3512.438725	1011043.795909	43.012186
3512.326772	1010788.248930	43.017191
3512.471656	1010531.190366	43.022196
3512.154789	1010275.556713	43.027201
3512.193937	1010018.686566	43.032205
3512.349996	1009783.556668	43.037210
3512.080798	1009541.586036	43.042215
3511.896443	1009277.526368	43.047220
3512.058154	1009022.729102	43.052225
3511.941618	1008777.395540	43.057229
3511.926009	1008527.076757	43.062234
3511.991172	1008280.427873	43.067239
3511.777668	1008032.452988	43.072244
3511.752256	1007796.006243	43.077249
3511.981945	1007547.937076	43.082253
3511.546314	1007300.161062	43.087258
3511.318633	1007038.726337	43.092263
3511.823478	1006795.343545	43.097268
3511.840213	1006561.658244	43.102273
3511.600065	1006320.419905	43.107277
3512.078093	1006063.783683	43.112282
3511.487848	1005833.766738	43.117287
3511.822063	1005592.889033	43.122292
3511.563521	1005348.499738	43.127297
3511.393386	1005104.377129	43.132301
3511.513005	1004860.779915	43.137306
3511.321053	1004635.998852	43.142311
3511.456489	1004397.826837	43.147316
3511.248973	1004146.664463	43.152321
3511.193203	1003931.075459	43.157325
3511.306015	1003704.650471	43.162330
3511.216117	1003461.416663	43.167335
3511.148110	1003209.508572	43.172340
3511.307858	1002981.198083	43.177345
3511.160429	1002742.516396	43.182349
3511.121278	1002513.830552	43.187354
3510.726353	1002301.057492	43.192359
3511.192403	1002068.766879	43.197364
3511.074705	1001830.431122	43.202369
3511.004785	1001608.526831	43.207373
3510.950577	1001369.674548	43.212378
3511.087008	1001130.975473	43.217383
3511.313440	1000908.410882	43.222388
3511.273881	1000704.182990	43.227393
3510.815680	1000456.013196	43.232397
3510.862758	1000224.689480	43.237402
3510.663100	999992.325983	43.242407
3510.985868	999780.216197	43.247412
3510.807864	999548.025639	43.252417
3510.566766	999323.917896	43.257421
3510.814359	999120.559339	43.262426
3510.813371	998880.424794	43.267431
3510.929906	998656.523896	43.272436
3510.655199	998435.989785	43.277441
3510.493158	998196.924078	43.282445
3510.444754	997973.120747	43.287450
3510.377062	997759.928321	43.292455
3510.598731	997548.823091	43.297460
3510.065258	997330.139239	43.302465
3510.494341	997120.542420	43.307469
3510.500006	996903.311879	43.312474
3510.338827	996658.044050	43.317479
3510.677753	996427.978588	43.322484
3510.232854	996226.286480	43.327489
3510.427711	996005.190784	43.332493
3510.223397	995787.075226	43.337498
3509.888991	995582.224150	43.342503
3510.304075	995370.323959	43.347508
3510.417854	995145.700283	43.352513
3510.294684	994943.422362	43.357517
3510.344236	994741.985849	43.362522
3510.452688	994511.393427	43.367527
3510.290989	994301.205089	43.372532
3510.119190	994092.277649	43.377537
3510.257552	993867.306976	43.382541
3510.480150	993666.875966	43.387546
3510.341259	993451.194108	43.392551
3510.413797	993241.707776	43.397556
3510.325961	993033.897308	43.402561
3510.389919	992800.513316	43.407565
3509.929543	992576.565006	43.412570
3509.998684	992369.289314	43.417575
3509.824378	992156.001431	43.422580
3509.683746	991949.817449	43.427585
3509.825723	991753.329713	43.432589
3509.739869	991539.906646	43.437594
3509.890094	991344.963546	43.442599
3509.709064	991137.294112	43.447604
3509.707705	990933.975754	43.452609
3509.864457	990733.062092	43.457613
3509.805980	990519.303662	43.462618
3509.487217	990325.378107	43.467623
3509.390136	990107.416893	43.472628
3509.472210	989917.117574	43.477633
3509.457198	989737.752057	43.482637
3509.261564	989533.927983	43.487642
3508.974925	989319.089099	43.492647
3509.448649	989128.698918	43.497652
3509.505870	988953.198688	43.502657
3509.222822	988753.165529	43.507661
3509.573337	988547.655327	43.512666
3509.199188	988346.549755	43.517671
3509.320459	988154.331402	43.522676
3509.050510	987960.902622	43.527681
3508.843130	987781.409590	43.532685
3509.540663	987584.979147	43.537690
3509.579864	987388.455216	43.542695
3509.576999	987176.318490	43.547700
3509.243031	986989.112440	43.552705
3509.136447	986780.003155	43.557709
3508.761871	986614.163166	43.562714
3509.029544	986427.717895	43.567719
3508.967609	986234.879408	43.572724
3508.724292	986028.204989	43.577729
3508.614619	985850.879865	43.582733
3509.079995	985690.438065	43.587738
3508.920415	985505.789940	43.592743
3509.292388	985300.744788	43.597748
3509.236191	985117.824112	43.602753
3509.075866	984931.693279	43.607757
3509.120221	984728.341049	43.612762
3508.704990	984541.165603	43.617767
3508.922348	984349.974647	43.622772
3508.911800	984176.583946	43.627777
3508.796788	983984.166259	43.632781
3508.579256	983804.061464	43.637786
3508.538714	983629.096849	43.642791
3508.651922	983456.933244	43.647796
3508.684393	983283.996564	43.652801
3508.467054	983095.764626	43.657805
3508.641193	982918.789864	43.662810
3508.501485	982724.283039	43.667815
3508.896640	982547.455685	43.672820
3508.672607	982366.427658	43.677825
3508.417290	982188.719702	43.682829
3508.522199	982001.375272	43.687834
3508.328648	981816.613349	43.692839
3508.498829	981641.064744	43.697844
3508.184016	981461.097404	43.702849
3508.438699	981289.431230	43.707853
3508.704472	981121.860831	43.712858
3508.242555	980957.433687	43.717863
3508.416516	980776.485091	43.722868
3508.181169	980598.235911	43.727873
3508.134449	980426.104986	43.732877
3508.693505	980254.650699	43.737882
3508.324501	980078.752119	43.742887
3508.189936	979903.884270	43.747892
3508.012434	979736.932521	43.752897
3507.936191	979556.963622	43.757901
3508.346420	979387.657513	43.762906
3508.163198	979236.228632	43.767911
3508.211433	979055.734876	43.772916
3508.334670	978871.314150	43.777921
3508.091888	978721.640470	43.782925
3508.523082	978524.160311	43.787930
3508.246362	978347.215967	43.792935
3508.419560	978196.482712	43.797940
3508.134165	978036.926932	43.802945
3508.212114	977863.330013	43.807949
3508.201227	977691.110866	43.812954
3507.744678	977521.501340	43.817959
3508.275780	977343.415440	43.822964
3508.049507	977172.975664	43.827969
3507.640720	977011.652079	43.832973
3508.008551	976853.031002	43.837978
3507.800471	976675.925913	43.842983
3507.910154	976504.531056	43.847988
3507.924813	976348.789327	43.852993
3507.724802	976204.517659	43.857997
3508.043469	976014.595425	43.863002
3507.395820	975856.993971	43.868007
3507.593216	975702.573416	43.873012
3507.429508	975536.279027	43.878017
3507.709011	975370.102377	43.883021
3507.676360	975231.841176	43.888026
3507.664837	975058.956255	43.893031
3507.705941	974899.063654	43.898036
3507.635891	974729.307737	43.903041
3507.679838	974581.434429	43.908045
3507.617888	974422.914667	43.913050
3507.346793	974282.518257	43.918055
3507.366774	974127.204268	43.923060
3507.141165	973970.459421	43.928065
3507.051461	973805.667526	43.933069
3507.371509	973654.790555	43.938074
3507.110869	973503.124927	43.943079
3507.516502	973346.650316	43.948084
3507.234430	973202.316561	43.953089
3507.145746	973051.980156	43.958093
3507.214240	972894.668345	43.963098
3507.081743	972766.635752	43.968103
3507.492142	972599.672461	43.973108
3507.595842	972445.179602	43.978113
3507.072209	972277.969462	43.983117
3507.262743	972143.412602	43.988122
3507.078341	971991.498764	43.993127
3507.355938	971839.309123	43.998132
3507.094196	971695.521157	44.003137
3507.145086	971538.762148	44.008141
3507.302746	971378.262938	44.013146
3507.648786	971230.449178	44.018151
3507.340873	971094.579884	44.023156
3507.651758	970935.706616	44.028161
3507.262170	970771.757683	44.033165
3507.458367	970626.008132	44.038170
3507.272103	970484.428259	44.043175
3506.931601	970322.513597	44.048180
3507.006288	970165.615310	44.053185
3507.201140	970025.820916	44.058189
3507.188552	969881.652851	44.063194
3506.892983	969730.676250	44.068199
3507.142926	969581.857106	44.073204
3507.028904	969448.363951	44.078209
3507.016201	969312.208082	44.083213
3506.806916	969163.062185	44.088218
3506.899370	969026.588561	44.093223
3507.107428	968880.499103	44.098228
3506.881427	968731.540545	44.103233
3506.729853	968594.215784	44.108237
3507.002142	968444.188723	44.113242
3506.942602	968313.695161	44.118247
3506.774545	968169.020215	44.123252
3506.674612	968008.958819	44.128257
3506.744972	967875.594574	44.133261
3506.965072	967717.136823	44.138266
3506.580884	967588.442708	44.143271
3506.382669	967449.629550	44.148276
3506.318643	967330.179108	44.153281
3506.411038	967189.549247	44.158285
3506.542074	967023.351187	44.163290
3506.231543	966905.499326	44.168295
3506.737444	966785.160279	44.173300
3506.865431	966649.701605	44.178305
3506.760551	966506.933058	44.183309
3506.676943	966348.585567	44.188314
3506.915154	966217.211893	44.193319
3507.002373	966065.488313	44.198324
3506.975048	965953.446781	44.203329
3506.538862	965814.731300	44.208333
3506.587984	965670.447446	44.213338
3506.355879	965533.356684	44.218343
3506.532205	965385.714425	44.223348
3506.759201	965249.128995	44.228353
3506.418955	965122.429509	44.233357
3506.581665	965010.436277	44.238362
3506.404938	964863.230607	44.243367
3506.641577	964717.912376	44.248372
3506.401447	964592.654203	44.253377
3506.107162	964452.804882	44.258381
3506.474346	964309.512191	44.263386
3506.574137	964185.756719	44.268391
3506.602164	964049.273578	44.273396
3506.799115	963920.009752	44.278401
3506.528200	963797.972631	44.283405
3506.563933	963635.121731	44.288410
3506.465072	963502.173906	44.293415
3506.560281	963388.298537	44.298420
3506.427786	963239.378290	44.303425
3506.440419	963102.385305	44.308429
3506.700703	962968.582079	44.313434
3506.512213	962857.486783	44.318439
3506.493168	962728.329797	44.323444
3506.297364	962586.850969	44.328449
3506.348779	962448.562047	44.333453
3506.457804	962310.162313	44.338458
3506.051716	962200.952297	44.343463
3506.220119	962062.046790	44.348468
3506.679182	961946.710878	44.353473
3506.197743	961810.944711	44.358477
3506.393202	961667.614626	44.363482
3506.419152	961542.442322	44.368487
3506.307811	961392.490681	44.373492
3506.221198	961275.270804	44.378497
3506.442192	961154.959107	44.383501
3506.505501	961025.750412	44.388506
3505.667468	960887.962664	44.393511
3505.943067	960749.890163	44.398516
3505.958381	960630.385658	44.403521
3505.858989	960491.388397	44.408525
3505.990102	960372.741808	44.413530
3505.947462	960265.297975	44.418535
3506.050656	960133.121515	44.423540
3506.095344	959993.598320	44.428545
3505.826459	959891.675292	44.433549
3506.217250	959776.601393	44.438554
3505.829876	959645.573098	44.443559
3506.123368	959526.097955	44.448564
3506.121316	959393.725793	44.453569
3505.987259	959268.726615	44.458573
3505.979422	959154.588491	44.463578
3505.990041	959031.423464	44.468583
3505.934541	958909.835709	44.473588
3505.893797	958799.520444	44.478593
3505.684794	958673.147802	44.483597
3505.858914	958541.903895	44.488602
3505.543938	958428.194274	44.493607
3505.627726	958314.318660	44.498612
3505.753701	958189.743654	44.503617
3505.677649	958072.849271	44.508621
3506.063676	957960.093821	44.513626
3505.980553	957848.688499	44.518631
3506.140890	957721.351463	44.523636
3506.132411	957601.003487	44.528641
3505.652033	957473.766523	44.533645
3506.072821	957345.887877	44.538650
3505.651949	957242.766021	44.543655
3505.375634	957127.945417	44.548660
3505.448654	957001.980215	44.553665
3505.693383	956888.148076	44.558669
3505.767115	956764.041421	44.563674
3505.740660	956638.280876	44.568679
3505.447800	956545.916662	44.573684
3505.838899	956442.450571	44.578689
3505.350315	956309.695429	44.583693
3505.818552	956201.993719	44.588698
3505.336388	956094.446544	44.593703
3505.315670	955973.379906	44.598708
3505.459038	955873.056868	44.603713
3505.620740	955762.586649	44.608717
3505.537458	955633.794293	44.613722
3505.282368	955542.321783	44.618727
3505.414593	955429.171617	44.623732
3505.221820	955326.209407	44.628737
3505.277116	955233.628280	44.633741
3505.718572	955109.039713	44.638746
3505.584052	955000.418824	44.643751
3505.445769	954873.337768	44.648756
3505.262702	954789.299775	44.653761
3505.204784	954695.866752	44.658765
3505.468279	954578.085189	44.663770
3505.117435	954474.653576	44.668775
3505.332858	954374.856919	44.673780
3505.230682	954273.388900	44.678785
3505.004760	954159.599984	44.683789
3505.633569	954038.780553	44.688794
3505.416422	953934.550722	44.693799
3505.192111	953824.197732	44.698804
3505.354890	953747.355731	44.703809
3504.872677	953650.338326	44.708813
3505.285031	953538.822015	44.713818
3505.066644	953422.432473	44.718823
3504.911170	953308.995664	44.723828
3505.397233	953218.029061	44.728833
3505.116175	953121.829524	44.733837
3505.319611	953006.891806	44.738842
3505.277629	952909.883503	44.743847
3505.180530	952813.456510	44.748852
3505.289017	952697.092296	44.753857
3504.942728	952610.270575	44.758861
3504.838726	952508.959181	44.763866
3504.404791	952416.503236	44.768871
3504.868739	952324.758920	44.773876
3505.258795	952227.762217	44.778881
3504.861075	952121.898446	44.783885
3504.917706	952025.335595	44.788890
3504.586801	951926.633769	44.793895
3505.072476	951837.556620	44.798900
3505.117354	951755.536507	44.803905
3504.646820	951652.258875	44.808909
3504.851202	951542.743056	44.813914
3504.870160	951455.267379	44.818919
3504.719927	951365.234028	44.823924
3504.892139	951266.915159	44.828929
3504.650605	951174.500813	44.833933
3504.993346	951063.324922	44.838938
3504.819045	950967.641597	44.843943
3504.759911	950876.053251	44.848948
3505.116344	950793.105008	44.853953
3504.772834	950696.200183	44.858957
3505.019999	950591.730087	44.863962
3505.022225	950505.772509	44.868967
3504.828697	950420.611520	44.873972
3504.967884	950327.927783	44.878977
3504.570146	950223.077792	44.883981
3504.639958	950107.522745	44.888986
3504.702358	950042.703574	44.893991
3504.569175	949943.165187	44.898996
3504.814882	949852.657179	44.904001
3504.736664	949783.454150	44.909005
3504.737575	949662.922245	44.914010
3504.356018	949568.491589	44.919015
3504.479622	949482.113955	44.924020
3504.549530	949403.307346	44.929025
3504.454830	949324.143670	44.934029
3504.770086	949219.347269	44.939034
3504.399166	949142.428442	44.944039
3504.762217	949031.492542	44.949044
3504.599381	948943.908328	44.954049
3504.675677	948875.337899	44.959053
3504.549178	948769.264584	44.964058
3504.358381	948682.255051	44.969063
3504.555716	948592.881950	44.974068
3504.418043	948523.001479	44.979073
3504.399896	948430.692548	44.984077
3504.577589	948328.965039	44.989082
3504.059200	948238.458778	44.994087
3504.388251	948163.038023	44.999092
3504.341044	948072.642777	45.004097
3503.863944	948016.218680	45.009101
3503.873172	947909.530723	45.014106
3503.885045	947828.219589	45.019111
3504.256321	947764.565924	45.024116
3504.272948	947682.581309	45.029121
3503.828741	947593.296574	45.034125
3504.248025	947514.690898	45.039130
3504.048058	947453.330363	45.044135
3504.365279	947350.123923	45.049140
3504.163074	947275.831309	45.054145
3503.919371	947212.176356	45.059149
3504.308402	947104.642967	45.064154
3504.300206	947032.517950	45.069159
3504.291679	946943.916522	45.074164
3504.551128	946849.234708	45.079169
3504.195848	946784.539185	45.084173
3504.190146	946708.960782	45.089178
3504.566836	946640.694384	45.094183
3504.487788	946548.266066	45.099188
3504.417287	946465.414354	45.104193
3504.107904	946355.010739	45.109197
3504.495470	946284.630290	45.114202
3504.341378	946207.632014	45.119207
3504.302153	946123.428462	45.124212
3504.353885	946048.980604	45.129217
3504.141249	945983.964164	45.134221
3504.377858	945875.568122	45.139226
3504.363076	945782.732330	45.144231
3504.455715	945714.213094	45.149236
3504.373361	945624.834781	45.154241
3504.053170	945543.542450	45.159245
3504.278794	945479.214003	45.164250
3503.904574	945405.018688	45.169255
3504.033857	945304.485311	45.174260
3504.457831	945221.053177	45.179265
3504.141877	945147.706960	45.184269
3504.152240	945062.807275	45.189274
3504.249420	944991.978017	45.194279
3504.277113	944916.080507	45.199284
3504.191402	944839.625607	45.204289
3504.163630	944757.985324	45.209293
3504.144491	944686.116946	45.214298
3503.871422	944599.052288	45.219303
3503.882128	944500.247836	45.224308
3503.941270	944439.383918	45.229313
3503.638372	944368.132883	45.234317
3503.913502	944300.619128	45.239322
3503.993687	944217.994216	45.244327
3503.964423	944144.490771	45.249332
3504.183382	944093.851294	45.254337
3503.700614	943997.706261	45.259341
3503.871977	943919.278639	45.264346
3503.392536	943856.292206	45.269351
3503.234191	943761.910426	45.274356
3503.800869	943713.318597	45.279361
3503.446559	943659.893900	45.284365
3503.621131	943591.620727	45.289370
3503.561454	943511.308023	45.294375
3503.416203	943433.979603	45.299380
3503.692953	943379.681268	45.304385
3503.516939	943325.456942	45.309389
3504.010413	943243.802897	45.314394
3503.600914	943191.724467	45.319399
3503.496233	943116.589362	45.324404
3503.926881	943043.282195	45.329409
3503.407371	942973.102188	45.334413
3503.540425	942897.541325	45.339418
3503.529063	942837.724783	45.344423
3503.787038	942755.718436	45.349428
3504.010721	942670.169388	45.354433
3503.499142	942628.455713	45.359437
3503.886053	942560.038193	45.364442
3503.621566	942497.191644	45.369447
3503.622208	942434.204797	45.374452
3503.420165	942357.061496	45.379457
3503.377693	942279.411403	45.384461
3503.445591	942222.259214	45.389466
3503.439598	942151.695940	45.394471
3503.384808	942088.138791	45.399476
3503.713575	942005.629618	45.404481
3503.240667	941941.564280	45.409485
3503.545605	941898.751477	45.414490
3503.488146	941826.178787	45.419495
3503.102808	941747.618439	45.424500
3503.851341	941688.910058	45.429505
3503.417546	941627.615076	45.434509
3503.488242	941562.304919	45.439514
3503.610815	941501.971580	45.444519
3503.477439	941453.665823	45.449524
3503.670291	941379.895042	45.454529
3503.318317	941324.240542	45.459533
3503.601745	941267.330085	45.464538
3503.661804	941196.263571	45.469543
3503.466209	941127.635571	45.474548
3503.790177	941055.660626	45.479553
3503.451341	940973.245128	45.484557
3503.730379	940908.947375	45.489562
3503.317728	940853.489654	45.494567
3503.426526	940792.479104	45.499572
3503.092914	940722.717713	45.504577
3503.201116	940674.364968	45.509581
3503.420101	940585.809588	45.514586
3503.676260	940535.609003	45.519591
3503.312833	940494.045669	45.524596
3503.336075	940409.547620	45.529601
3503.018880	940351.479337	45.534605
3503.142169	940287.775069	45.539610
3503.132597	940238.958154	45.544615
3503.288016	940184.358885	45.549620
3503.636060	940124.548011	45.554625
3503.353525	940068.485059	45.559629
3503.200180	939986.119382	45.564634
3503.392674	939924.317615	45.569639
3503.118953	939889.832550	45.574644
3503.287721	939815.660038	45.579649
3503.136193	939752.090447	45.584653
3503.170372	939706.522648	45.589658
3503.166329	939636.596585	45.594663
3503.074620	939571.192428	45.599668
3503.518523	939525.459649	45.604673
3503.043807	939487.647696	45.609677
3503.046773	939393.064489	45.614682
3503.232150	939336.820716	45.619687
3503.196897	939280.228966	45.624692
3503.285299	939220.738348	45.629697
3503.044642	939166.193724	45.634701
3503.292449	939106.771491	45.639706
3502.826437	939054.469255	45.644711
3503.094469	939005.211406	45.649716
3503.767514	938964.232687	45.654721
3503.163150	938907.059112	45.659725
3503.380952	938843.801429	45.664730
3503.477587	938766.939763	45.669735
3503.193055	938702.803742	45.674740
3503.220125	938627.198699	45.679745
3503.069507	938586.736470	45.684749
3503.416250	938516.162065	45.689754
3503.197888	938469.953537	45.694759
3503.099887	938424.204498	45.699764
3503.115244	938366.347294	45.704769
3503.014101	938322.420849	45.709773
3503.073991	938241.815659	45.714778
3502.929466	938189.835647	45.719783
3502.818781	938149.267524	45.724788
3503.151952	938080.320649	45.729793
3502.821042	938035.853951	45.734797
3503.096744	937976.606261	45.739802
3502.859010	937916.003170	45.744807
3503.026338	937870.781338	45.749812
3503.327002	937815.173986	45.754817
3502.774168	937732.167072	45.759821
3502.669209	937619.913644	45.764826
3502.712643	937485.562310	45.769831
3502.924367	937251.952304	45.774836
3502.989855	936950.984746	45.779841
3502.993862	936606.052683	45.784845
3503.020973	936180.083446	45.789850
3502.699758	935705.660611	45.794855
3502.591624	935159.445850	45.799860
3502.502997	934568.332975	45.804865
3502.422023	933913.391849	45.809869
3502.360026	933182.688185	45.814874
3502.103776	932392.747239	45.819879
3501.862840	931500.277023	45.824884
3502.410957	930563.712023	45.829889
3501.771241	929569.323769	45.834893
3501.978525	928460.993210	45.839898
3501.839260	927290.765581	45.844903
3501.249013	926062.464882	45.849908
3501.353763	924754.316575	45.854913
3501.026632	923361.445911	45.859917
3500.768503	921890.154096	45.864922
3500.709991	920330.248758	45.869927
3500.212217	918704.005223	45.874932
3500.100531	916982.138769	45.879937
3499.824451	915183.249294	45.884941
3499.456097	913294.045636	45.889946
3499.179548	911348.349464	45.894951
3498.785888	909321.251303	45.899956
3498.701495	907176.504424	45.904961
3498.556246	904947.053736	45.909965
3497.859399	902644.279190	45.914970
3497.249062	900280.647031	45.919975
3497.080260	897807.214613	45.924980
3496.727175	895237.969250	45.929985
3496.266336	892609.732815	45.934989
3495.771176	889896.768861	45.939994
3495.413731	887082.570992	45.944999
3494.924547	884216.360379	45.950004
3494.581708	881262.932426	45.955009
3494.193233	878203.090230	45.960013
3493.926170	875065.083348	45.965018
3493.129384	871852.401683	45.970023
3492.910055	868537.068570	45.975028
3492.411744	865162.418982	45.980033
3491.547797	861696.580298	45.985037
3491.401615	858127.945609	45.990042
3490.525050	854479.666715	45.995047
3490.152523	850774.993325	46.000052
3489.670309	846971.246625	46.005057
3488.520030	843085.867141	46.010061
3488.160683	839103.941784	46.015066
3487.528567	835054.347746	46.020071
3486.543574	830910.656075	46.025076
3486.386953	826696.524339	46.030081
3485.441213	822404.134096	46.035085
3484.603179	818017.838978	46.040090
3484.213294	813558.591052	46.045095
3483.258492	809025.069980	46.050100
3482.248828	804382.930757	46.055105
3481.966581	799644.719826	46.060109
3480.999608	794852.313920	46.065114
3480.056388	789985.219429	46.070119
3479.147775	785009.376357	46.075124
3478.216089	779972.702684	46.080129
3477.266808	774849.940310	46.085133
3476.493019	769630.420809	46.090138
3475.453005	764357.666760	46.095143
3474.631477	758962.817308	46.100148
3473.765092	753508.197565	46.105153
3472.962489	747992.972700	46.110157
3471.967696	742340.776796	46.115162
3470.600385	736620.661152	46.120167
3469.392936	730840.872919	46.125172
3468.709777	724981.900397	46.130177
3467.505783	719015.232708	46.135181
3466.893880	712961.869108	46.140186
3465.445896	706845.029502	46.145191
3464.197375	700640.811580	46.150196
3463.839074	694335.504582	46.155201
3462.399498	687938.803079	46.160205
3461.148674	681483.015670	46.165210
3459.661327	674940.346787	46.170215
3458.345849	668312.974034	46.175220
3457.183303	661628.268942	46.180225
3455.853800	654844.584396	46.185229
3455.008384	647954.749707	46.190234
3453.662342	641012.385464	46.195239
3452.231603	633985.371338	46.200244
3450.973371	626882.460225	46.205249
3449.594729	619695.228491	46.210253
3448.115001	612423.761120	46.215258
3446.748798	605062.745080	46.220263
3445.017590	597641.177910	46.225268
3443.841223	590131.363664	46.230273
3442.082843	582553.405089	46.235277
3440.809531	574878.788155	46.240282
3439.448603	567136.756858	46.245287
3437.549574	559334.493342	46.250292
3436.120381	551414.939805	46.255297
3434.331430	543428.701463	46.260301
3432.484873	535385.086796	46.265306
3430.824113	527270.565402	46.270311
3429.013102	519065.665996	46.275316
3427.629318	510787.581410	46.280321
3425.718028	502445.201928	46.285325
3423.975790	494025.512893	46.290330
3422.028269	485538.133594	46.295335
3420.305667	476973.684133	46.300340
3418.230342	468341.130406	46.305345
3416.243921	459627.444797	46.310349
3414.375086	450840.799750	46.315354
3412.321843	442012.780680	46.320359
3410.177974	433082.288494	46.325364
3408.263654	424081.876337	46.330369
3406.024236	415049.072296	46.335373
3403.921821	405937.869563	46.340378
3401.875754	396756.778208	46.345383
3399.215433	387516.228908	46.350388
3396.893371	378184.553035	46.355393
3394.440750	368854.858811	46.360397
3392.268482	359444.046663	46.365402
3389.681252	349954.695147	46.370407
3387.319772	340417.626355	46.375412
3385.266884	330829.881629	46.380417
3382.283588	321220.673058	46.385421
3379.669190	311519.774482	46.390426
3377.100206	301752.483250	46.395431
3373.985067	291960.994307	46.400436
3371.044270	282117.500734	46.405441
3368.334810	272263.551331	46.410445
3365.396757	262333.109729	46.415450
3362.282943	252360.275864	46.420455
3358.957846	242349.119379	46.425460
3356.292601	232315.356406	46.430465
3352.891747	222221.603739	46.435469
3349.427844	212062.581616	46.440474
3346.287588	201915.130787	46.445479
3342.364420	191769.376489	46.450484
3338.835376	181609.449687	46.455489
3335.205513	171399.734027	46.460493
3331.207087	161197.482459	46.465498
3326.750550	150966.041894	46.470503
3322.458071	140770.997943	46.475508
3318.154690	130543.482347	46.480513
3313.420603	120327.076671	46.485517
3308.244473	110132.729318	46.490522
3302.914343	99953.119095	46.495527
3296.771144	89847.163929	46.500532
3290.630671	79744.370165	46.505537
3282.726516	69736.005814	46.510541
3274.027838	59836.714188	46.515546
3255.061964	50280.438358	46.520551
3230.231563	41080.312901	46.525556
3205.677116	32233.107903	46.530561
3177.365452	23875.214595	46.535565
3138.315372	16319.140815	46.540570
3089.890810	9705.389271	46.545575
3038.063198	4023.397827	46.550580
2943.016897	527.954610	46.555585
2778.806385	384.530804	46.560589
2695.721130	374.567637	46.565594
2695.229427	353.420143	46.570599
2745.271317	347.421944	46.575604
2810.809908	339.066810	46.580609
2865.567520	343.710225	46.585613
2898.180643	346.987189	46.590618
2910.049284	347.614127	46.595623
2906.874707	339.334114	46.600628
2897.931662	311.430414	46.605633
2887.747311	332.235223	46.610637
2879.690096	353.633389	46.615642
2875.095219	338.673015	46.620647
2872.079413	345.366859	46.625652
2870.641953	340.795740	46.630657
2869.166686	323.618985	46.635661
2867.130646	322.102217	46.640666
2865.228807	321.647889	46.645671
2862.290390	346.425717	46.650676
2859.547271	334.789044	46.655681
2856.600935	325.961512	46.660685
2853.563395	306.343456	46.665690
2850.557561	327.472542	46.670695
2847.056105	335.995328	46.675700
2844.019811	329.641098	46.680705
2840.883549	307.544553	46.685709
2837.941511	317.616649	46.690714
2835.116447	311.882745	46.695719
2831.828330	317.547576	46.700724
2828.286470	304.456621	46.705729
2824.786870	302.597833	46.710733
2821.820568	305.864791	46.715738
2818.711587	293.096101	46.720743
2815.288429	308.647726	46.725748
2811.902709	315.725049	46.730753
2808.567266	314.007599	46.735757
2805.326080	302.441450	46.740762
2802.155034	295.833348	46.745767
2799.300812	310.114384	46.750772
2796.328069	319.283873	46.755777
2792.365360	311.638562	46.760781
2788.644524	284.600293	46.765786
2785.018465	297.032016	46.770791
2781.461683	310.224266	46.775796
2778.798741	291.388469	46.780801
2775.564012	295.289822	46.785805
2772.424493	291.517564	46.790810
2768.743774	283.077432	46.795815
2765.011537	294.039219	46.800820
2761.449746	282.884658	46.805825
2758.273717	288.099925	46.810829
2755.215879	286.873489	46.815834
2751.730247	274.318378	46.820839
2747.972423	296.349668	46.825844
2744.891143	296.852886	46.830849
2741.114411	284.278191	46.835853
2737.865305	293.347934	46.840858
2734.409482	290.896089	46.845863
2731.101457	302.130565	46.850868
2727.950303	290.360116	46.855873
2724.111772	278.821290	46.860877
2720.667211	283.996398	46.865882
2717.297524	296.236123	46.870887
2713.968028	296.291564	46.875892
2711.074344	270.427570	46.880897
2707.415117	271.826142	46.885901
2703.769451	279.280869	46.890906
2700.061896	282.327765	46.895911
2696.410187	291.293532	46.900916
2693.277603	270.411503	46.905921
2689.393172	277.143630	46.910925
2686.281830	292.959740	46.915930
2682.629589	301.918305	46.920935
2678.943760	282.395240	46.925940
2675.875106	269.276795	46.930945
2672.412563	278.720507	46.935949
2669.178393	292.462040	46.940954
2666.011693	267.573957	46.945959
2662.305117	260.940099	46.950964
2658.274484	270.215366	46.955969
2654.871986	288.403972	46.960973
2651.349685	281.638906	46.965978
2648.117780	265.436570	46.970983
2644.545581	270.554126	46.975988
2641.960267	269.872701	46.980993
2638.049996	273.530248	46.985997
2634.332787	276.550846	46.991002
2631.429881	259.792941	46.996007
2627.148529	271.854393	47.001012
2623.820309	260.150805	47.006017
2620.510101	260.284394	47.011021
2617.291299	272.088178	47.016026
2613.940207	268.171045	47.021031
2609.903930	270.633029	47.026036
2606.268678	247.499227	47.031041
2602.912510	260.720958	47.036045
2599.620017	269.068766	47.041050
2596.635365	265.468357	47.046055
2592.847246	258.365193	47.051060
2589.566710	246.351115	47.056065
2585.855055	270.663863	47.061069
2582.003841	258.915826	47.066074
2578.600282	257.548186	47.071079
2575.235858	262.161243	47.076084
2571.750855	253.447769	47.081089
2568.366294	270.943561	47.086093
2564.865779	283.335310	47.091098
2561.680034	262.034297	47.096103
2557.753062	269.471044	47.101108
2554.768451	259.124389	47.106113
2551.222264	273.817863	47.111117
2547.745878	261.223279	47.116122
2544.245329	241.375633	47.121127
2540.307171	264.613656	47.126132
2537.053129	263.959279	47.131137
2533.501943	264.145270	47.136141
2529.899328	267.149779	47.141146
2526.997168	257.457302	47.146151
2523.053182	253.479849	47.151156
2519.406378	232.753804	47.156161
2516.195665	254.908551	47.161165
2512.611737	269.361435	47.166170
2509.160644	254.416128	47.171175
2505.484094	248.816486	47.176180
2502.224086	225.900487	47.181185
2499.095825	244.982113	47.186189
2494.981294	255.131499	47.191194
2491.705243	238.996150	47.196199
2488.154703	234.564866	47.201204
2484.958016	238.784204	47.206209
2480.817229	241.919700	47.211213
2477.250193	255.268473	47.216218
2474.230258	243.897004	47.221223
2470.755200	235.906043	47.226228
2467.567274	240.003886	47.231233
2463.986789	245.706978	47.236237
2460.170892	248.330682	47.241242
2457.112270	252.376627	47.246247
2453.255296	247.372327	47.251252
2449.965358	220.613385	47.256257
2446.631632	235.769999	47.261261
2442.604774	261.687683	47.266266
2439.664128	234.679939	47.271271
2435.878805	236.312511	47.276276
2432.212667	244.303018	47.281281
2428.412217	238.096347	47.286285
2425.172114	236.983961	47.291290
2422.018318	231.644720	47.296295
2418.551740	242.940616	47.301300
2414.968593	226.344670	47.306305
2411.488663	235.334767	47.311309
2408.046080	237.184385	47.316314
2404.666068	238.332252	47.321319
2400.647267	230.348039	47.326324
2397.230758	225.596188	47.331329
2393.978350	244.310519	47.336333
2390.221468	241.099079	47.341338
2387.101806	225.018612	47.346343
2383.740176	229.142073	47.351348
2380.399516	235.354727	47.356353
2376.688738	248.404157	47.361357
2372.870019	246.878285	47.366362
2369.486715	246.334479	47.371367
2365.747959	243.218219	47.376372
2362.075149	234.283598	47.381377
2358.873329	239.550400	47.386381
2355.284627	241.482639	47.391386
2352.303722	250.110596	47.396391
2348.654609	244.371960	47.401396
2345.338733	218.795447	47.406401
2341.409863	216.803691	47.411405
2337.739630	227.294869	47.416410
2334.838887	231.623291	47.421415
2330.842599	231.678286	47.426420
2327.618528	227.561305	47.431425
2324.121097	229.626083	47.436429
2320.533875	227.014999	47.441434
2317.395157	216.756058	47.446439
2313.286369	216.530118	47.451444
2310.105920	224.163060	47.456449
2306.837247	247.174294	47.461453
2302.899457	232.518347	47.466458
2299.581098	214.855926	47.471463
2296.031542	212.811204	47.476468
2292.477719	226.998228	47.481473
2289.319394	218.826893	47.486477
2285.409773	235.221087	47.491482
2282.184967	220.557171	47.496487
2278.283826	231.040291	47.501492
2275.017236	218.392166	47.506497
2271.603285	220.613170	47.511501
2267.932814	236.619105	47.516506
2264.612385	217.544880	47.521511
2261.041638	220.488606	47.526516
2257.798314	235.171347	47.531521
2254.012633	234.209001	47.536525
2250.604633	227.796343	47.541530
2247.115544	220.103084	47.546535
2243.691983	239.763701	47.551540
2240.286548	224.903791	47.556545
2236.627964	223.631252	47.561549
2232.820540	223.331381	47.566554
2229.454412	217.391663	47.571559
2225.860133	235.234318	47.576564
2222.662630	228.901980	47.581569
2219.221253	217.319815	47.586573
2215.675939	220.391064	47.591578
2212.272023	241.145033	47.596583
2208.533633	240.488713	47.601588
2205.220789	216.912605	47.606593
2201.587536	220.451657	47.611597
2198.127238	234.941928	47.616602
2195.080605	237.170449	47.621607
2190.745523	238.425235	47.626612
2187.435352	216.334455	47.631617
2184.103950	223.109035	47.636621
2180.787192	227.541741	47.641626
2177.355046	226.183347	47.646631
2173.569432	235.002187	47.651636
2170.131285	219.588282	47.656641
2166.792847	231.597462	47.661645
2163.003046	228.100167	47.666650
2159.717924	236.192182	47.671655
2156.024056	240.277612	47.676660
2152.775777	220.528041	47.681665
2149.285731	223.463834	47.686669
2145.610824	214.202579	47.691674
2142.260776	225.951174	47.696679
2138.466472	233.755574	47.701684
2135.234599	226.251475	47.706689
2131.619902	231.222744	47.711693
2127.818626	215.146066	47.716698
2124.542433	203.023943	47.721703
2120.863670	214.146180	47.726708
2117.683330	223.436274	47.731713
2114.324539	209.254768	47.736717
2110.310137	213.683705	47.741722
2107.136579	227.026270	47.746727
2103.447617	223.575313	47.751732
2100.142667	218.104905	47.756737
2096.572586	208.611336	47.761741
2092.950255	209.496656	47.766746
2090.090783	201.107052	47.771751
2086.365334	208.453324	47.776756
2082.731195	217.014888	47.781761
2078.940389	196.055390	47.786765
2075.221529	208.830406	47.791770
2072.405990	225.989834	47.796775
2068.527612	227.576971	47.801780
2065.137812	219.769476	47.806785
2062.142692	198.466339	47.811789
2058.206604	214.147386	47.816794
2054.772022	220.097658	47.821799
2050.817559	223.071139	47.826804
2047.493849	220.609881	47.831809
2044.071655	216.428059	47.836813
2040.507900	212.523811	47.841818
2037.479625	205.571077	47.846823
2033.459246	206.001026	47.851828
2030.044024	216.468793	47.856833
2026.537146	225.849681	47.861837
2023.225733	219.520356	47.866842
2019.848184	195.351257	47.871847
2016.023623	210.632739	47.876852
2012.547435	224.672092	47.881857
2009.359278	217.524275	47.886861
2005.493466	205.662652	47.891866
2002.527412	201.621944	47.896871
1998.734931	220.509285	47.901876
1995.162825	215.638199	47.906881
1991.411600	213.422795	47.911885
1988.036599	216.371838	47.916890
1984.612249	207.503207	47.921895
1981.037740	206.365397	47.926900
1977.418807	194.321809	47.931905
1974.132026	221.073658	47.936909
1970.296862	223.341297	47.941914
1967.223446	213.510464	47.946919
1963.508359	200.884438	47.951924
1960.067475	210.941543	47.956929
1956.773813	207.890683	47.961933
1952.834802	191.748879	47.966938
1949.842106	203.496571	47.971943
1945.887738	219.947575	47.976948
1942.717858	217.096384	47.981953
1939.378457	206.415496	47.986957
1935.678309	199.235984	47.991962
1932.088120	205.470432	47.996967
1928.511503	217.613577	48.001972
1925.078683	219.905322	48.006977
1921.556079	202.543796	48.011981
1918.147919	212.390527	48.016986
1914.691198	215.191695	48.021991
1910.852190	227.397577	48.026996
1907.311564	201.428972	48.032001
1904.203144	215.109068	48.037005
1900.579449	215.237479	48.042010
1897.389817	209.661342	48.047015
1893.525477	210.497409	48.052020
1889.956762	206.544539	48.057025
1886.900207	228.929533	48.062029
1883.339669	215.264531	48.067034
1879.797724	207.615717	48.072039
1875.961123	208.208586	48.077044
1872.614029	192.562158	48.082049
1868.871273	192.762019	48.087053
1865.240969	210.601720	48.092058
1861.999265	190.402148	48.097063
1858.599581	220.102008	48.102068
1854.682156	202.334227	48.107073
1851.616362	189.441149	48.112077
1847.899665	201.723927	48.117082
1844.678074	211.728321	48.122087
1841.118882	207.478157	48.127092
1837.712883	192.811777	48.132097
1834.180785	187.981045	48.137101
1830.543910	206.072896	48.142106
1827.400603	191.762116	48.147111
1823.639556	194.751443	48.152116
1819.918205	207.146575	48.157121
1816.385644	205.898544	48.162125
1812.565302	214.198445	48.167130
1809.601796	196.501388	48.172135
1805.949178	197.075972	48.177140
1802.620876	190.712175	48.182145
1799.293426	207.582618	48.187149
1795.689122	197.153776	48.192154
1792.076911	197.441538	48.197159
1788.323994	199.134978	48.202164
1785.078286	199.059225	48.207169
1781.560210	198.578181	48.212173
1777.954214	195.155546	48.217178
1774.581425	209.527217	48.222183
1771.152983	201.088212	48.227188
1767.375704	187.462327	48.232193
1764.095244	190.986176	48.237197
1760.276324	201.736088	48.242202
1756.983205	207.222178	48.247207
1753.602637	208.856960	48.252212
1749.897470	195.268900	48.257217
1746.357167	197.596313	48.262221
1742.929514	201.950616	48.267226
1739.654591	186.872718	48.272231
1735.749118	196.620742	48.277236
1732.777110	206.165423	48.282241
1729.116563	200.579280	48.287245
1725.466370	191.870198	48.292250
1722.315199	185.827814	48.297255
1718.450449	210.485359	48.302260
1714.818569	198.331413	48.307265
1711.508217	182.739506	48.312269
1707.896270	191.128760	48.317274
1704.634900	188.794904	48.322279
1700.904793	208.470492	48.327284
1697.645575	191.421594	48.332289
1693.798206	180.262392	48.337293
1690.438992	195.328293	48.342298
1687.145748	204.049899	48.347303
1683.474613	184.396998	48.352308
1679.705718	173.692454	48.357313
1676.706536	188.088311	48.362317
1672.661152	207.690649	48.367322
1669.498272	191.614032	48.372327
1665.773775	183.175514	48.377332
1662.067569	197.095078	48.382337
1658.932148	198.192065	48.387341
1655.278025	202.055810	48.392346
1652.003577	175.129943	48.397351
1648.449818	183.682546	48.402356
1644.760986	199.046716	48.407361
1641.403546	210.018745	48.412365
1637.631734	189.758138	48.417370
1634.588293	176.640041	48.422375
1630.847013	195.971422	48.427380
1627.246547	200.398683	48.432385
1623.900568	187.248629	48.437389
1620.491806	202.618286	48.442394
1617.240905	191.724708	48.447399
1613.570635	199.300213	48.452404
1610.084998	196.683198	48.457409
1606.517796	191.932862	48.462413
1602.908201	199.729590	48.467418
1599.340858	203.867194	48.472423
1595.687390	200.871548	48.477428
1592.258824	176.740707	48.482433
1588.812675	176.692399	48.487437
1585.048124	198.244162	48.492442
1581.772893	182.339055	48.497447
1578.532886	180.079372	48.502452
1574.670087	176.137333	48.507457
1571.449771	182.007053	48.512461
1567.859478	176.842977	48.517466
1564.369846	183.631266	48.522471
1560.957878	196.459598	48.527476
1557.218528	207.443581	48.532481
1554.231481	199.277916	48.537485
1550.309417	204.593147	48.542490
1546.798043	187.827652	48.547495
1543.285792	175.234937	48.552500
1539.835296	188.506442	48.557505
1536.578505	190.196164	48.562509
1532.608394	199.166748	48.567514
1529.583698	193.029995	48.572519
1525.897328	198.958799	48.577524
1522.260168	174.883055	48.582529
1518.872671	169.957513	48.587533
1514.943640	189.894237	48.592538
1511.825267	188.477880	48.597543
1508.316678	181.518668	48.602548
1504.531471	187.078666	48.607553
1501.420336	190.587506	48.612557
1497.617999	182.313857	48.617562
1494.671787	163.286572	48.622567
1490.989638	182.338913	48.627572
1487.228920	179.843323	48.632577
1483.708419	178.781398	48.637581
1480.020641	199.538344	48.642586
1477.055121	190.968758	48.647591
1473.328363	186.559420	48.652596
1469.828946	190.990100	48.657601
1466.235356	201.464712	48.662605
1462.715677	184.489738	48.667610
1459.185489	172.115586	48.672615
1455.540254	193.317317	48.677620
1452.244829	186.888996	48.682625
1448.864928	185.093322	48.687629
1445.340978	194.985568	48.692634
1441.989421	182.953938	48.697639
1438.501580	175.680998	48.702644
1434.585918	179.468745	48.707649
1431.357745	189.697791	48.712653
1427.877007	184.609919	48.717658
1424.143989	166.211200	48.722663
1420.765396	167.261219	48.727668
1417.179605	190.582461	48.732673
1413.708896	186.005515	48.737677
1409.998209	176.786055	48.742682
1406.516245	165.899288	48.747687
1402.858292	172.750047	48.752692
1399.551048	169.448189	48.757697
1396.569545	169.901559	48.762701
1393.033952	182.662250	48.767706
1389.425780	174.600879	48.772711
1385.842164	164.683053	48.777716
1382.227646	166.055446	48.782721
1378.777428	171.845597	48.787725
1375.013512	193.695919	48.792730
1371.662484	180.289587	48.797735
1368.114294	159.226808	48.802740
1364.508473	170.811176	48.807745
1360.975751	183.800960	48.812749
1357.455249	185.136935	48.817754
1354.331417	172.742635	48.822759
1350.986316	155.450017	48.827764
1347.176392	160.787371	48.832769
1343.627686	181.543181	48.837773
1339.786437	187.849211	48.842778
1336.786810	180.278521	48.847783
1333.518857	172.141990	48.852788
1329.963325	173.570372	48.857793
1326.272971	168.997379	48.862797
1322.340523	171.946290	48.867802
1318.956854	162.535600	48.872807
1315.510961	174.562464	48.877812
1312.069128	165.661324	48.882817
1308.865945	165.419258	48.887821
1304.987746	181.000347	48.892826
1301.467920	181.861347	48.897831
1298.017604	174.968009	48.902836
1294.569379	182.375004	48.907841
1291.204961	165.823883	48.912845
1287.464048	174.749535	48.917850
1284.225606	176.499869	48.922855
1280.642338	189.204060	48.927860
1277.270295	188.786766	48.932865
1273.640017	170.018626	48.937869
1270.147125	173.381145	48.942874
1266.903996	179.978234	48.947879
1263.050122	170.214887	48.952884
1259.392135	161.633961	48.957889
1256.227676	183.503336	48.962893
1252.302773	184.681990	48.967898
1249.118527	163.729581	48.972903
1245.283738	165.185755	48.977908
1242.023041	166.128700	48.982913
1238.699090	152.476518	48.987917
1234.977051	179.329670	48.992922
1231.515179	158.225420	48.997927
1228.099571	158.997437	49.002932
1224.839930	170.636482	49.007937
1221.257359	186.024387	49.012941
1217.164123	178.672663	49.017946
1213.926507	157.323260	49.022951
1210.841288	161.783535	49.027956
1206.832534	164.546822	49.032961
1203.669299	165.159700	49.037965
1199.718089	178.705055	49.042970
1196.415694	180.851107	49.047975
1193.023158	182.326933	49.052980
1189.215010	164.783146	49.057985
1186.279223	149.121097	49.062989
1182.353522	172.737707	49.067994
1178.995802	182.780276	49.072999
1175.411139	164.248839	49.078004
1172.095298	161.098069	49.083009
1168.827984	150.805199	49.088013
1165.043719	170.742687	49.093018
1161.711473	176.834360	49.098023
1158.037850	160.407378	49.103028
1154.094334	150.417920	49.108033
1150.981898	166.600361	49.113037
1147.293023	187.281220	49.118042
1144.052257	170.398250	49.123047
1140.877539	156.047233	49.128052
1137.179748	166.292737	49.133057
1133.420590	177.249666	49.138061
1129.708998	178.274894	49.143066
1126.476820	171.204282	49.148071
1123.006259	155.084339	49.153076
1119.362759	161.877793	49.158081
1116.072688	170.194716	49.163085
1112.833968	169.237890	49.168090
1109.079780	160.114004	49.173095
1105.315300	161.726643	49.178100
1101.620217	158.715071	49.183105
1098.270986	171.226691	49.188109
1094.849636	163.151927	49.193114
1091.850107	160.192241	49.198119
1087.996339	173.319169	49.203124
1084.119089	184.082443	49.208129
1080.786616	173.232552	49.213133
1077.167917	171.875326	49.218138
1074.087509	161.816023	49.223143
1070.667055	182.487999	49.228148
1066.975081	180.202961	49.233153
1063.731598	164.059073	49.238157
1059.970186	163.131453	49.243162
1056.379654	154.917144	49.248167
1052.649795	157.973719	49.253172
1049.063013	159.720509	49.258177
1046.026621	178.788501	49.263181
1042.393578	170.057196	49.268186
1039.147048	166.284422	49.273191
1035.538950	157.066821	49.278196
1031.621524	165.257012	49.283201
1028.273839	173.905765	49.288205
1024.806196	168.025500	49.293210
1021.408683	166.784000	49.298215
1017.745304	160.151418	49.303220
1014.274168	168.388283	49.308225
1011.154816	171.962800	49.313229
1007.477882	178.806815	49.318234
1004.278156	150.854363	49.323239
1000.366189	161.940938	49.328244
996.999828	171.210220	49.333249
993.289393	154.448318	49.338253
989.822168	176.435010	49.343258
986.212497	169.694534	49.348263
982.610918	163.968399	49.353268
979.179353	150.704080	49.358273
975.896619	162.141537	49.363277
972.244742	172.589555	49.368282
968.561207	163.380404	49.373287
965.520097	147.872901	49.378292
961.543771	173.189842	49.383297
958.404818	170.804085	49.388301
955.098699	169.145737	49.393306
951.574246	151.056639	49.398311
948.138641	162.010328	49.403316
944.258493	185.200754	49.408321
940.694044	160.155227	49.413325
937.159904	149.642573	49.418330
933.495830	155.397497	49.423335
930.431930	172.135662	49.428340
926.594584	175.199695	49.433345
923.498086	148.754860	49.438349
919.608697	161.576500	49.443354
916.489034	167.050068	49.448359
912.943319	168.878239	49.453364
909.343246	158.983165	49.458369
905.986297	153.907711	49.463373
902.395382	170.630016	49.468378
898.770456	166.789681	49.473383
895.158180	156.732681	49.478388
891.341594	163.370056	49.483393
888.262542	157.169324	49.488397
884.490754	174.936291	49.493402
881.207136	164.564891	49.498407
878.185187	155.222291	49.503412
874.117310	149.618703	49.508417
870.825491	172.025006	49.513421
866.888784	185.958267	49.518426
863.390792	166.734937	49.523431
860.339495	146.340817	49.528436
856.880239	156.376881	49.533441
853.506860	159.275653	49.538445
849.823138	164.409723	49.543450
846.340212	158.330455	49.548455
842.766512	168.304836	49.553460
839.238517	162.555490	49.558465
835.536142	138.022447	49.563469
832.073901	157.172427	49.568474
828.610188	165.185202	49.573479
825.220558	157.929265	49.578484
821.485779	154.557345	49.583489
818.317551	148.376905	49.588493
814.765666	171.554775	49.593498
811.408459	174.439455	49.598503
807.743319	162.387810	49.603508
803.871705	147.363807	49.608513
800.391652	156.766957	49.613517
797.021995	158.889676	49.618522
793.607978	160.652557	49.623527
790.506452	151.513637	49.628532
786.599133	163.109649	49.633537
783.374030	160.363349	49.638541
779.514986	166.402986	49.643546
776.057932	151.155466	49.648551
772.616044	136.765266	49.653556
768.844289	159.383219	49.658561
765.632957	160.960626	49.663565
762.147775	155.403329	49.668570
758.541153	150.374912	49.673575
755.105154	150.674560	49.678580
751.579217	145.304035	49.683585
748.130802	142.180220	49.688589
744.755182	160.482261	49.693594
741.206185	166.001746	49.698599
737.787372	149.117104	49.703604
733.834819	146.401694	49.708609
730.478763	146.221947	49.713613
726.855013	166.058790	49.718618
723.573797	164.255186	49.723623
720.100050	142.651777	49.728628
716.414953	155.746753	49.733633
713.198690	167.227095	49.738637
709.652102	160.615565	49.743642
706.133352	156.173131	49.748647
702.536073	145.967197	49.753652
698.948264	150.214446	49.758657
695.794734	135.090587	49.763661
692.075107	147.594949	49.768666
688.483117	164.115866	49.773671
685.171601	150.826981	49.778676
681.563294	149.336864	49.783681
678.119509	155.250062	49.788685
674.571189	155.076842	49.793690
671.006096	149.340043	49.798695
667.663883	150.540085	49.803700
663.905845	155.818016	49.808705
660.527568	155.785604	49.813709
656.835850	149.421714	49.818714
653.583113	142.209173	49.823719
649.949178	151.386940	49.828724
646.444094	149.066845	49.833729
643.012572	152.999373	49.838733
639.560661	151.398316	49.843738
636.526152	137.503112	49.848743
632.843702	131.813742	49.853748
629.046401	145.338241	49.858753
625.642966	160.586169	49.863757
621.693981	163.072189	49.868762
618.491776	143.896988	49.873767
615.044104	131.169069	49.878772
611.294894	141.944433	49.883777
607.836210	154.447958	49.888781
604.243192	140.729165	49.893786
600.980314	130.521248	49.898791
597.519608	140.956873	49.903796
593.866213	162.503073	49.908801
590.393288	141.051447	49.913805
586.900134	137.704969	49.918810
583.637469	150.255634	49.923815
580.464729	161.827873	49.928820
576.434643	158.710654	49.933825
573.035834	150.579612	49.938829
569.385609	157.214429	49.943834
565.650887	152.662246	49.948839
562.466841	128.536053	49.953844
558.850382	145.043900	49.958849
555.576716	139.515322	49.963853
551.922811	153.566428	49.968858
548.187162	161.561995	49.973863
545.359389	134.714970	49.978868
541.046016	152.783120	49.983873
537.834466	154.530245	49.988877
534.064380	136.547618	49.993882
530.725543	150.259748	49.998887
527.829393	163.086189	50.003892
523.972158	152.914430	50.008897
520.738986	137.310380	50.013901
516.797328	142.581524	50.018906
513.177706	147.880590	50.023911
510.163379	141.849184	50.028916
506.427104	142.078706	50.033921
503.060166	121.855971	50.038925
499.451735	144.576042	50.043930
495.783544	163.025065	50.048935
492.277597	153.156052	50.053940
488.659030	137.628509	50.058945
485.423908	139.916189	50.063949
481.867313	146.601967	50.068954
478.256328	140.249323	50.073959
475.135062	141.753985	50.078964
471.435668	149.202419	50.083969
467.987952	156.857997	50.088973
464.098821	155.600143	50.093978
460.703652	153.163742	50.098983
457.198794	148.976210	50.103988
453.575456	133.799903	50.108993
450.619100	140.586003	50.113997
447.233526	146.903709	50.119002
443.414851	154.511448	50.124007
439.453869	139.898754	50.129012
436.143529	146.338689	50.134017
432.973747	142.661584	50.139021
429.271499	134.688488	50.144026
426.014161	141.608760	50.149031
422.506107	145.739689	50.154036
419.069629	128.577564	50.159041
415.440400	141.633438	50.164045
411.326383	158.747437	50.169050
408.386853	148.824271	50.174055
404.937465	141.733439	50.179060
401.171375	155.411513	50.184065
397.788368	140.119777	50.189069
394.247623	138.023331	50.194074
390.566108	146.943222	50.199079
387.428653	160.837269	50.204084
383.538233	154.544553	50.209089
380.304613	131.325674	50.214093
376.483465	140.461983	50.219098
372.821540	139.474824	50.224103
369.626110	132.286722	50.229108
365.782898	143.381956	50.234113
362.690413	142.933251	50.239117
359.399329	163.874158	50.244122
355.879217	137.958858	50.249127
352.456510	125.798948	50.254132
348.520048	153.208965	50.259137
345.436051	152.529808	50.264141
341.919396	155.722591	50.269146
337.803039	137.793400	50.274151
334.857902	142.924081	50.279156
330.971113	159.175399	50.284161
327.715830	154.942689	50.289165
323.947787	145.527955	50.294170
320.112988	155.346723	50.299175
317.531640	136.669731	50.304180
314.050377	144.999221	50.309185
310.642510	139.933114	50.314189
306.944468	146.559580	50.319194
302.949276	155.643108	50.324199
299.465532	142.597197	50.329204
296.073518	141.617970	50.334209
292.856682	138.503305	50.339213
289.221281	146.578314	50.344218
285.586767	152.945610	50.349223
282.139907	130.920048	50.354228
278.405335	144.589113	50.359233
275.212484	143.371609	50.364237
271.610207	158.103350	50.369242
268.137026	147.293905	50.374247
265.059676	136.990332	50.379252
260.913789	147.441944	50.384257
257.506949	154.424481	50.389261
254.386223	150.027629	50.394266
250.811349	159.872936	50.399271
247.170778	142.132637	50.404276
243.454101	148.389825	50.409281
240.149232	152.294224	50.414285
236.715993	134.688668	50.419290
233.271950	133.559941	50.424295
229.544553	148.208982	50.429300
225.815651	155.672181	50.434305
222.621222	146.834425	50.439309
219.119178	147.713865	50.444314
215.595036	135.836551	50.449319
212.370686	139.704278	50.454324
208.397475	140.421962	50.459329
205.247747	149.054022	50.464333
201.619583	152.034468	50.469338
197.974003	154.354003	50.474343
194.497292	152.137789	50.479348
190.865506	148.171072	50.484353
187.470396	124.806402	50.489357
184.053473	141.944790	50.494362
180.272766	133.222781	50.499367
177.386525	132.339191	50.504372
173.777124	154.131375	50.509377
169.995603	145.392040	50.514381
166.672169	134.534844	50.519386
162.917310	139.961069	50.524391
159.698587	135.541698	50.529396
155.845250	143.748172	50.534401
152.811339	128.553809	50.539405
149.011899	146.717617	50.544410
145.247405	149.442339	50.549415
142.111914	129.973650	50.554420
138.635492	138.961768	50.559425
135.047785	138.397219	50.564429
131.307313	142.256653	50.569434
127.990154	129.114589	50.574439
124.615172	111.038049	50.579444
121.031129	132.846254	50.584449
118.005543	145.920985	50.589453
114.151230	132.125376	50.594458
110.325505	131.051699	50.599463
107.211620	148.510760	50.604468
103.143433	156.959730	50.609473
99.779932	134.059744	50.614477
96.366492	151.790956	50.619482
93.054237	147.593837	50.624487
89.293476	119.402046	50.629492
85.908684	133.972226	50.634497
82.568464	131.256078	50.639501
78.953130	147.845384	50.644506
75.445307	136.115905	50.649511
72.191138	146.092659	50.654516
68.155216	141.423165	50.659521
64.977536	121.309363	50.664525
61.519116	125.862857	50.669530
57.598255	143.964000	50.674535
54.724847	156.511011	50.679540
51.003336	145.512507	50.684545
47.579578	150.031976	50.689549
43.972259	146.031713	50.694554
40.318530	131.681569	50.699559
36.933088	135.631141	50.704564
33.425904	136.713066	50.709569
29.794073	122.738515	50.714573
26.373623	136.947059	50.719578
22.847059	132.926266	50.724583
19.274427	141.666264	50.729588
15.875675	151.417659	50.734593
12.744557	144.304854	50.739597
9.135699	127.487677	50.744602
5.786506	124.073360	50.749607
1.887609	148.208240	50.754612