Fri Jun 17 17:08:12 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.353320	104.224415	0.000000
2.411295	106.660096	0.005005
2.356207	94.419970	0.010010
2.270713	90.731786	0.015014
2.156276	71.736579	0.020019
1.918361	73.247599	0.025024
1.532453	53.847814	0.030029
0.857483	44.187085	0.035034
1.017918	40.163617	0.040038
0.602100	28.889256	0.045043
-0.014948	24.784467	0.050048
0.019912	18.310096	0.055053
-0.489745	19.515620	0.060058
-1.072929	6.432920	0.065062
-0.904264	0.197781	0.070067
-1.720170	12.020535	0.075072
-1.271007	-6.214597	0.080077
-1.978215	2.845200	0.085082
-2.666676	2.744901	0.090086
-2.581829	-0.908428	0.095091
-2.894970	3.486069	0.100096
-2.524009	3.691958	0.105101
-3.497204	1.334151	0.110106
-3.957527	-1.811600	0.115110
-3.896487	-4.024593	0.120115
-4.256057	3.385745	0.125120
-4.104708	7.990352	0.130125
-4.218060	8.359620	0.135130
-4.490372	6.047325	0.140134
-5.134509	8.704278	0.145139
-5.673305	20.736918	0.150144
-5.571235	13.271033	0.155149
-5.863281	5.750880	0.160154
-5.798380	-1.830574	0.165158
-5.915626	0.752811	0.170163
-6.605363	7.578872	0.175168
-7.275375	-1.209457	0.180173
-7.621292	3.800637	0.185178
-7.708975	-1.691758	0.190182
-7.771957	3.805484	0.195187
-7.729517	-2.772552	0.200192
-7.540418	5.551796	0.205197
-7.978826	1.923873	0.210202
-8.357853	-5.261548	0.215206
-8.992460	-13.976229	0.220211
-9.055874	2.759119	0.225216
-9.015230	-8.954371	0.230221
-9.492983	-1.539784	0.235226
-9.773971	2.733732	0.240230
-9.893761	0.038720	0.245235
-10.699636	-4.875898	0.250240
-10.574063	5.587626	0.255245
-10.604651	0.642215	0.260250
-10.676565	-2.128045	0.265254
-10.755292	1.736724	0.270259
-11.677440	8.354357	0.275264
-12.320415	4.802074	0.280269
-12.406513	-0.523840	0.285274
-12.792008	1.945477	0.290278
-12.760717	11.455580	0.295283
-12.476844	7.633996	0.300288
-12.411445	5.545583	0.305293
-13.263139	-5.277028	0.310298
-13.936561	7.332678	0.315302
-13.817392	-6.169260	0.320307
-13.999457	2.453578	0.325312
-13.952047	1.007115	0.330317
-14.481751	9.084301	0.335322
-14.999780	4.442895	0.340326
-15.129816	2.047359	0.345331
-15.566385	-0.971113	0.350336
-15.329155	2.547904	0.355341
-15.576390	2.504309	0.360346
-15.909189	-1.756052	0.365350
-16.650648	0.935825	0.370355
-17.350508	1.202290	0.375360
-16.936760	1.618919	0.380365
-17.178453	1.357930	0.385370
-17.094372	2.702747	0.390374
-17.002822	1.546523	0.395379
-17.531451	16.344061	0.400384
-17.984056	4.127263	0.405389
-18.669152	0.627566	0.410394
-18.725251	0.832215	0.415398
-18.777815	-3.357905	0.420403
-18.978395	-3.546399	0.425408
-19.032926	-1.708894	0.430413
-19.481353	-2.938359	0.435418
-20.347255	0.766584	0.440422
-20.197818	2.475861	0.445427
-20.795332	8.000584	0.450432
-20.434045	0.201542	0.455437
-20.543281	7.657492	0.460442
-20.718190	6.890495	0.465446
-21.233891	0.834823	0.470451
-22.085741	6.345779	0.475456
-22.112240	4.344865	0.480461
-22.585486	5.305171	0.485466
-22.432406	17.843020	0.490470
-22.074861	2.723784	0.495475
-22.396544	7.770699	0.500480
-22.501248	6.597369	0.505485
-23.338838	2.855044	0.510490
-23.737501	11.205658	0.515494
-23.536393	-0.456563	0.520499
-24.759695	8.735989	0.525504
-24.417888	1.265782	0.530509
-24.933268	0.991481	0.535514
-25.120176	7.029687	0.540518
-25.303031	-5.576284	0.545523
-25.693363	3.784858	0.550528
-25.375147	-1.768494	0.555533
-25.501212	9.547694	0.560538
-25.578982	9.888552	0.565542
-26.153957	-3.158990	0.570547
-26.913530	6.525980	0.575552
-26.657204	5.773339	0.580557
-27.278196	-0.864323	0.585562
-27.317099	0.540796	0.590566
-27.236690	-6.025197	0.595571
-28.237216	4.542823	0.600576
-28.461115	4.917838	0.605581
-28.918248	5.536846	0.610586
-28.951133	-0.091936	0.615590
-28.875987	5.485156	0.620595
-28.781243	6.854445	0.625600
-28.820602	6.867465	0.630605
-28.843957	3.631126	0.635610
-29.342994	7.949571	0.640614
-29.823247	1.283186	0.645619
-30.409072	3.573871	0.650624
-31.498821	-3.889256	0.655629
-31.155150	-5.867439	0.660634
-30.637712	0.576615	0.665638
-30.891149	-2.058096	0.670643
-31.531258	-0.226261	0.675648
-31.418044	-7.608543	0.680653
-32.374058	-2.732060	0.685658
-32.661965	-1.705867	0.690662
-32.713329	-5.783509	0.695667
-33.129092	4.304291	0.700672
-33.343374	-7.478710	0.705677
-33.450456	-1.992886	0.710682
-33.159873	1.760372	0.715686
-33.566125	4.331019	0.720691
-34.541654	-8.012554	0.725696
-34.623253	-4.268471	0.730701
-34.941341	2.096810	0.735706
-34.898154	3.515516	0.740710
-34.972759	2.273051	0.745715
-35.152973	7.161081	0.750720
-35.060727	-0.512531	0.755725
-35.679195	5.260169	0.760730
-36.102065	3.845308	0.765734
-36.481607	-4.229199	0.770739
-36.562788	-1.117830	0.775744
-36.700094	2.558160	0.780749
-37.783641	-2.380545	0.785754
-38.168133	6.188327	0.790758
-37.671973	4.767121	0.795763
-37.823706	10.907816	0.800768
-37.884630	8.493688	0.805773
-37.993096	10.310560	0.810778
-38.284072	12.152639	0.815782
-38.842013	12.472675	0.820787
-39.890564	8.868822	0.825792
-39.180464	14.449496	0.830797
-39.553441	6.536494	0.835802
-39.967446	10.457785	0.840806
-39.521962	3.582071	0.845811
-40.496356	10.727180	0.850816
-40.813347	5.189233	0.855821
-41.285645	11.683553	0.860826
-41.430161	2.406113	0.865830
-41.037857	4.290900	0.870835
-41.346345	5.425101	0.875840
-41.501210	0.608487	0.880845
-42.410030	13.564574	0.885850
-42.715370	8.491379	0.890854
-42.504001	6.255961	0.895859
-42.757550	7.343142	0.900864
-42.780290	8.788594	0.905869
-43.053250	4.344636	0.910874
-43.949999	7.519549	0.915878
-44.114763	0.713702	0.920883
-44.326625	9.328866	0.925888
-44.492873	5.253151	0.930893
-44.525458	8.150232	0.935898
-44.992169	6.996823	0.940902
-44.785348	5.235757	0.945907
-45.751370	6.153266	0.950912
-46.301087	14.244043	0.955917
-46.495472	-3.938577	0.960922
-46.509422	7.911105	0.965926
-46.449785	1.870702	0.970931
-46.937601	2.729242	0.975936
-46.438185	6.595193	0.980941
-46.414252	5.123625	0.985946
-46.880669	7.699736	0.990950
-47.382054	1.869015	0.995955
-47.577555	6.056691	1.000960
-47.890603	6.746470	1.005965
-48.895288	1.675076	1.010970
-49.249616	-8.655172	1.015974
-49.300710	1.451730	1.020979
-49.611162	9.912591	1.025984
-49.237127	6.431018	1.030989
-49.717920	5.474519	1.035994
-49.615795	-5.318375	1.040998
-49.738336	-2.039701	1.046003
-50.076159	5.738796	1.051008
-50.723515	7.117187	1.056013
-50.974321	0.701363	1.061018
-51.411091	3.413834	1.066022
-50.947474	-5.656456	1.071027
-51.697805	4.933520	1.076032
-52.163816	-7.509739	1.081037
-52.649993	-1.096982	1.086042
-53.145495	1.814691	1.091046
-52.412334	-0.219359	1.096051
-52.813623	7.881868	1.101056
-53.165821	5.394801	1.106061
-52.966471	-3.812515	1.111066
-53.240581	-1.361315	1.116070
-53.674678	-8.620451	1.121075
-54.410360	5.756250	1.126080
-54.209588	0.963006	1.131085
-54.524413	-2.689596	1.136090
-55.069476	6.566240	1.141094
-55.614073	6.622595	1.146099
-55.869174	5.121832	1.151104
-56.155478	2.014649	1.156109
-55.800050	0.740167	1.161114
-56.253639	11.805329	1.166118
-55.808771	3.395462	1.171123
-55.988818	9.185666	1.176128
-56.566571	3.385993	1.181133
-56.948116	3.063599	1.186138
-57.534368	7.262161	1.191142
-57.712407	-3.771477	1.196147
-57.926566	-0.627347	1.201152
-58.421061	-3.544819	1.206157
-58.710697	-3.679830	1.211162
-59.051395	9.281863	1.216166
-58.907672	-3.481792	1.221171
-59.127398	13.870552	1.226176
-59.193638	5.098097	1.231181
-59.211347	-1.076065	1.236186
-59.885480	11.595530	1.241190
-60.468671	7.483947	1.246195
-60.590868	11.855784	1.251200
-60.761167	12.497958	1.256205
-60.580248	1.072538	1.261210
-61.019380	18.780247	1.266214
-61.632668	7.226168	1.271219
-62.089273	4.132495	1.276224
-62.414465	0.662175	1.281229
-62.427547	5.908403	1.286234
-62.751022	4.807159	1.291238
-62.653830	4.683028	1.296243
-62.530828	9.848621	1.301248
-62.799208	9.891818	1.306253
-63.086982	1.657612	1.311258
-63.576740	15.304952	1.316262
-63.708194	9.023600	1.321267
-64.235753	9.268733	1.326272
-64.339885	5.985045	1.331277
-65.103845	5.419568	1.336282
-65.722954	13.285478	1.341286
-65.125614	3.804604	1.346291
-65.482605	6.534008	1.351296
-65.725207	5.510290	1.356301
-65.787520	-4.559477	1.361306
-65.858844	6.876462	1.366310
-65.542370	-4.161037	1.371315
-66.700323	3.905144	1.376320
-67.569235	5.313460	1.381325
-67.378954	-3.960426	1.386330
-67.458500	4.067976	1.391334
-67.411978	-7.113098	1.396339
-67.901436	7.861042	1.401344
-68.602852	7.270962	1.406349
-68.719819	3.084445	1.411354
-68.768448	2.092418	1.416358
-68.803482	2.136293	1.421363
-68.761801	10.951831	1.426368
-69.120578	4.059048	1.431373
-70.014556	9.328773	1.436378
-70.342947	7.042580	1.441382
-70.299161	0.167733	1.446387
-70.562080	9.742917	1.451392
-70.516372	4.123173	1.456397
-70.316981	-0.848822	1.461402
-71.288709	10.531375	1.466406
-71.791399	0.215133	1.471411
-72.195287	6.551859	1.476416
-72.041266	2.047977	1.481421
-72.254489	3.160621	1.486426
-72.354901	4.986021	1.491430
-72.016590	4.915343	1.496435
-72.970983	0.141066	1.501440
-73.478692	1.604975	1.506445
-73.236850	6.508290	1.511450
-73.811550	8.190534	1.516454
-73.804506	0.251665	1.521459
-74.107883	4.308486	1.526464
-74.403563	5.998219	1.531469
-75.044243	-0.197688	1.536474
-75.314580	7.007591	1.541478
-75.332960	-0.552318	1.546483
-75.814855	11.489209	1.551488
-75.540151	4.097247	1.556493
-75.280379	0.739254	1.561498
-76.512421	-1.756455	1.566502
-76.545164	-0.053403	1.571507
-76.813358	0.702921	1.576512
-77.352032	-2.021711	1.581517
-77.184412	-4.700956	1.586522
-77.518712	0.864868	1.591526
-77.128013	-4.076571	1.596531
-78.155953	-10.193495	1.601536
-78.674805	6.094035	1.606541
-78.587923	2.346439	1.611546
-78.941339	10.919225	1.616550
-78.736060	-0.905497	1.621555
-78.902824	7.389398	1.626560
-79.130909	5.552432	1.631565
-79.860564	-12.437787	1.636570
-80.258159	2.339927	1.641574
-80.128448	-9.889977	1.646579
-80.363306	-1.623431	1.651584
-80.510300	2.519674	1.656589
-80.718243	7.665491	1.661594
-81.436333	7.419371	1.666598
-81.492127	-2.904458	1.671603
-82.015045	-0.953966	1.676608
-81.740882	3.354940	1.681613
-81.767831	1.569786	1.686618
-82.830611	1.971777	1.691622
-82.955113	1.524369	1.696627
-83.129545	4.777730	1.701632
-83.500283	11.406128	1.706637
-83.534989	6.149620	1.711642
-83.647668	7.501293	1.716646
-83.479019	1.812372	1.721651
-84.447764	12.308622	1.726656
-84.940692	3.286439	1.731661
-84.952065	-1.907839	1.736666
-85.429523	5.694961	1.741670
-85.221400	-4.360561	1.746675
-85.500730	2.551991	1.751680
-85.456218	3.704274	1.756685
-85.465119	-3.791299	1.761690
-85.988142	0.418657	1.766694
-86.393378	-4.131964	1.771699
-86.817351	7.689182	1.776704
-86.797765	-5.953270	1.781709
-86.901563	5.983565	1.786714
-88.172271	11.880092	1.791718
-88.156937	-0.927733	1.796723
-88.232921	3.959940	1.801728
-88.677892	0.971292	1.806733
-88.239027	7.301909	1.811738
-88.690586	1.635973	1.816742
-88.557929	-3.850223	1.821747
-88.879517	0.114313	1.826752
-89.576135	14.497949	1.831757
-89.903358	0.884137	1.836762
-90.334718	0.674614	1.841766
-90.341420	0.903415	1.846771
-90.221015	-7.814217	1.851776
-90.438541	6.100235	1.856781
-91.043963	6.024431	1.861786
-91.688827	4.019558	1.866790
-91.874220	0.177317	1.871795
-92.017028	-3.931098	1.876800
-91.956428	2.329397	1.881805
-91.940133	-6.327318	1.886810
-92.124997	-2.477468	1.891814
-92.887310	-9.359594	1.896819
-93.396846	-10.166861	1.901824
-93.802786	-4.331414	1.906829
-93.420705	-6.685983	1.911834
-93.451653	1.755838	1.916838
-93.456489	-8.694067	1.921843
-93.934531	-9.945632	1.926848
-94.763685	-5.435161	1.931853
-94.667178	1.219750	1.936858
-94.887773	7.454177	1.941862
-95.006665	-3.401428	1.946867
-95.547449	-3.003331	1.951872
-96.394230	-2.700981	1.956877
-96.241389	-8.973345	1.961882
-96.709226	6.851053	1.966886
-96.618897	-2.611047	1.971891
-96.939123	-3.250678	1.976896
-96.826073	-8.683885	1.981901
-96.721626	-3.323804	1.986906
-97.356754	-0.340964	1.991910
-97.682673	-1.324978	1.996915
-98.104473	-6.540378	2.006912
-97.915576	-1.042655	2.016909
-96.910191	-3.822514	2.026906
-96.566081	-2.778057	2.036902
-96.660028	-2.084794	2.046899
-95.770353	-0.086208	2.056896
-95.378654	-0.869215	2.066893
-94.600252	6.722116	2.076890
-93.874501	4.244219	2.086886
-93.951558	1.486830	2.096883
-93.712946	4.025965	2.106880
-92.718108	-0.705853	2.116877
-92.275245	-1.664324	2.126874
-91.156436	-5.532560	2.136870
-90.993352	2.023739	2.146867
-90.858306	6.974021	2.156864
-90.845746	-0.321759	2.166861
-89.547122	0.954447	2.176858
-89.280313	-2.156876	2.186854
-88.630093	4.906086	2.196851
-88.204931	3.025468	2.206848
-87.799952	1.722780	2.216845
-87.517600	3.465097	2.226842
-86.577858	1.719441	2.236838
-86.409157	6.065844	2.246835
-85.254533	-1.145740	2.256832
-85.123142	6.462460	2.266829
-84.574281	-5.046055	2.276826
-84.451136	-1.630211	2.286822
-83.250836	-0.046221	2.296819
-83.164760	4.500041	2.306816
-83.064847	-0.367526	2.316813
-82.301458	-7.008452	2.326810
-81.983323	-2.988801	2.336806
-81.236635	-0.043723	2.346803
-80.512008	-5.708462	2.356800
-80.034390	-2.796306	2.366797
-80.019162	-6.272237	2.376794
-79.045037	0.441492	2.386790
-78.746307	-7.687056	2.396787
-78.183319	-9.118555	2.406784
-77.436491	-6.680896	2.416781
-77.303790	-2.974216	2.426778
-76.841135	3.046255	2.436774
-75.991175	-3.305573	2.446771
-75.980284	-1.332597	2.456768
-74.888715	0.448877	2.466765
-74.349090	-1.668306	2.476762
-74.036294	-2.052511	2.486758
-73.999062	-5.490015	2.496755
-73.510806	-2.783730	2.506752
-72.683259	-0.503724	2.516749
-72.218291	-1.980772	2.526746
-71.375947	0.353876	2.536742
-70.853063	-3.501439	2.546739
-70.759683	0.578693	2.556736
-70.494180	4.784132	2.566733
-69.380603	0.071505	2.576730
-69.399809	1.110366	2.586726
-68.717110	0.476374	2.596723
-68.087784	4.011194	2.606720
-67.762378	0.264973	2.616717
-66.848233	-2.492401	2.626714
-66.420044	3.156021	2.636710
-66.093383	0.401860	2.646707
-66.090096	-0.064065	2.656704
-65.361578	0.506704	2.666701
-64.584502	-0.919679	2.676698
-64.101044	-5.184156	2.686694
-63.249446	-2.849661	2.696691
-63.225897	-3.524838	2.706688
-63.082485	-8.809028	2.716685
-62.169759	-2.157997	2.726682
-61.426033	-2.780200	2.736678
-61.127892	-3.069498	2.746675
-60.226191	-4.731765	2.756672
-59.851146	-4.392489	2.766669
-59.723568	-8.147512	2.776666
-59.684081	-10.504210	2.786662
-58.469108	-4.412397	2.796659
-58.341882	-1.535449	2.806656
-57.625436	-9.262788	2.816653
-56.931119	-9.776602	2.826650
-56.689461	-7.281441	2.836646
-56.453399	-2.085558	2.846643
-55.242553	-5.273587	2.856640
-55.157892	-9.635568	2.866637
-54.882617	-8.483047	2.876634
-53.980413	-4.439758	2.886630
-53.594891	-6.632881	2.896627
-53.359525	-9.842508	2.906624
-52.392184	-7.867886	2.916621
-52.216958	-12.233659	2.926618
-51.768714	-9.151831	2.936614
-50.950894	-9.468238	2.946611
-50.663852	-9.444890	2.956608
-50.209804	-9.693517	2.966605
-49.278771	-1.789284	2.976602
-49.031098	-7.429071	2.986598
-49.075890	-7.267380	2.996595
-47.752497	-3.402379	3.006592
-47.493222	0.985677	3.016589
-46.949605	-1.274032	3.026586
-46.884385	-11.159607	3.036582
-45.817137	-4.348133	3.046579
-45.182692	-6.196750	3.056576
-45.324115	-5.991335	3.066573
-44.903337	-6.365825	3.076570
-44.495572	-5.315742	3.086566
-43.158874	-6.472182	3.096563
-42.745541	-1.495841	3.106560
-42.384547	3.822132	3.116557
-42.207865	2.722578	3.126554
-42.034318	-7.589413	3.136550
-41.267850	2.560062	3.146547
-40.707067	4.012480	3.156544
-39.430050	5.215042	3.166541
-39.890948	1.236761	3.176538
-39.208402	-0.913462	3.186534
-38.513565	-4.992174	3.196531
-37.744053	-1.034507	3.206528
-37.508287	-0.004241	3.216525
-37.414874	2.929900	3.226522
-36.513785	1.257267	3.236518
-36.005070	0.732618	3.246515
-35.804525	-0.239311	3.256512
-34.827296	2.148403	3.266509
-34.102336	-2.443305	3.276506
-34.045643	3.485995	3.286502
-34.144548	-2.642900	3.296499
-33.112324	5.191371	3.306496
-32.683947	0.732342	3.316493
-31.818591	0.111463	3.326490
-31.628687	-6.079071	3.336486
-31.200123	-4.073765	3.346483
-30.695351	2.522193	3.356480
-29.935953	0.027650	3.366477
-29.617526	0.543695	3.376474
-29.061796	0.399090	3.386470
-28.282835	-0.105473	3.396467
-28.202979	3.314608	3.406464
-27.908765	-0.086580	3.416461
-27.112176	4.006283	3.426458
-26.375193	-0.777302	3.436454
-26.023422	-1.817243	3.446451
-25.301958	3.758135	3.456448
-25.182636	5.165780	3.466445
-24.885854	0.128759	3.476442
-23.733598	-3.999903	3.486438
-23.360150	-2.563566	3.496435
-23.184610	-2.384954	3.506432
-22.276925	5.321637	3.516429
-21.784951	-0.754126	3.526426
-21.505640	-1.461936	3.536422
-21.563828	-7.337577	3.546419
-20.217639	-6.555112	3.556416
-20.085209	-1.245973	3.566413
-19.775953	-5.105883	3.576410
-18.898280	-3.585411	3.586406
-18.538966	-2.388173	3.596403
-18.079355	0.618469	3.606400
-17.073925	-4.096123	3.616397
-16.713521	-4.705382	3.626394
-16.765680	-1.097782	3.636390
-16.487944	-2.457950	3.646387
-15.420933	-1.582448	3.656384
-15.225756	1.600529	3.666381
-14.414297	0.267036	3.676378
-13.569225	2.747261	3.686374
-13.552500	-4.432443	3.696371
-13.396522	3.729062	3.706368
-12.117036	-3.961653	3.716365
-11.882439	-6.403340	3.726362
-11.976240	-6.160990	3.736358
-10.983184	-1.864470	3.746355
-10.666306	-1.518879	3.756352
-9.963092	3.072208	3.766349
-8.859093	-0.988561	3.776346
-9.066297	-5.983105	3.786342
-8.805498	1.643307	3.796339
-8.281587	-1.555402	3.806336
-7.423836	0.379557	3.816333
-7.084512	1.400911	3.826330
-6.275311	3.064557	3.836326
-6.047185	-1.118157	3.846323
-5.993898	2.922409	3.856320
-5.103416	13.073815	3.866317
-4.696096	9.803002	3.876314
-4.096309	20.883760	3.886310
-3.670910	24.576380	3.896307
-3.359102	30.056857	3.906304
-2.802931	43.338072	3.916301
-1.957792	46.927143	3.926298
-1.856255	55.080141	3.936294
-1.482225	70.474400	3.946291
-0.967537	86.580510	3.956288
-0.341624	102.562639	3.966285
0.000000	103.531998	3.971290
0.157958	121.376199	3.976294
0.444327	122.302604	3.981299
0.348092	128.477140	3.986304
0.094361	128.622880	3.991309
0.720450	129.793357	3.996314
0.438975	129.167991	4.001318
0.702567	138.472025	4.006323
0.939378	153.882073	4.011328
1.059808	147.783949	4.016333
0.884352	128.252003	4.021338
0.283180	131.672815	4.026342
0.799568	138.570777	4.031347
0.855631	140.534957	4.036352
1.088594	148.147218	4.041357
1.272756	149.058250	4.046362
0.763838	131.180918	4.051366
0.772104	129.568283	4.056371
0.847571	135.159973	4.061376
0.947876	131.175682	4.066381
1.161611	126.397807	4.071386
0.678681	128.145904	4.076390
0.953694	131.047530	4.081395
1.361560	136.756244	4.086400
0.671120	136.585232	4.091405
0.837828	134.279076	4.096410
0.961453	153.000247	4.101414
1.105604	156.493726	4.106419
1.339848	149.180447	4.111424
1.255752	146.902164	4.116429
1.398204	138.219852	4.121434
0.988527	137.038988	4.126438
1.223584	138.594141	4.131443
1.242716	122.924235	4.136448
0.883563	143.954914	4.141453
1.214177	131.393327	4.146458
1.299412	138.058073	4.151462
1.161284	133.314211	4.156467
0.767350	134.415260	4.161472
0.901543	132.633496	4.166477
1.095551	124.556921	4.171482
1.088601	139.426916	4.176486
0.986087	139.241852	4.181491
0.909326	144.770246	4.186496
0.933233	156.495552	4.191501
1.387114	156.134140	4.196506
1.254315	164.159049	4.201510
1.173656	161.643787	4.206515
1.618810	156.709827	4.211520
1.190651	153.229939	4.216525
1.579446	146.307938	4.221530
1.541742	163.844704	4.226534
1.316384	152.904649	4.231539
1.497295	157.617855	4.236544
1.031709	152.965711	4.241549
1.381607	147.743299	4.246554
1.025468	156.669844	4.251558
1.454479	160.643253	4.256563
1.759222	153.292600	4.261568
1.196556	163.621197	4.266573
1.456953	156.763552	4.271578
1.404094	154.775682	4.276582
1.496706	155.712982	4.281587
1.596724	158.417160	4.286592
1.308165	160.344693	4.291597
1.654460	151.442998	4.296602
1.455439	164.569334	4.301606
1.357581	157.650862	4.306611
1.424706	156.962421	4.311616
1.402389	155.193448	4.316621
1.411930	154.855571	4.321626
1.457727	156.180914	4.326630
1.347495	159.192755	4.331635
1.684913	162.779222	4.336640
1.472201	162.337784	4.341645
1.810501	158.334451	4.346650
1.746618	165.032874	4.351654
1.550771	159.240099	4.356659
1.445184	148.480433	4.361664
1.351469	159.976060	4.366669
1.751676	154.842766	4.371674
1.862373	164.453825	4.376678
1.847430	160.811519	4.381683
1.655415	158.510916	4.386688
1.484238	162.477721	4.391693
1.781899	157.679966	4.396698
1.676898	162.225405	4.401702
1.462941	159.663627	4.406707
1.501656	156.968288	4.411712
1.676488	163.197437	4.416717
1.824402	155.538765	4.421722
1.378487	170.943513	4.426726
1.794343	168.235017	4.431731
2.100163	179.776731	4.436736
1.823374	187.598454	4.441741
2.092057	174.922016	4.446746
1.693247	168.176500	4.451750
1.571678	173.294794	4.456755
2.149884	181.929893	4.461760
1.955387	193.651470	4.466765
1.999363	185.069564	4.471770
1.920538	190.998906	4.476774
1.951365	195.927497	4.481779
2.130681	194.239854	4.486784
1.657671	199.391311	4.491789
1.789646	184.139091	4.496794
1.977936	185.529355	4.501798
1.904977	180.646182	4.506803
2.241097	181.390667	4.511808
1.810136	191.772576	4.516813
1.887434	191.062118	4.521818
2.245303	196.691548	4.526822
2.120279	197.584117	4.531827
2.389777	188.965514	4.536832
2.215306	201.928552	4.541837
2.196577	190.393105	4.546842
2.070966	192.496219	4.551846
2.234902	192.469134	4.556851
2.598271	180.786514	4.561856
1.897633	171.369732	4.566861
2.215846	169.584413	4.571866
1.876107	188.613920	4.576870
2.187021	203.017925	4.581875
2.357577	182.217753	4.586880
2.146382	197.114056	4.591885
2.622827	191.749431	4.596890
2.447170	194.324204	4.601894
2.088089	179.969388	4.606899
2.216214	190.751309	4.611904
2.063661	192.630783	4.616909
2.414383	193.538208	4.621914
2.298122	193.178024	4.626918
2.045149	194.094425	4.631923
2.385527	183.097217	4.636928
2.124533	191.517199	4.641933
2.421229	182.413373	4.646938
1.914527	182.977870	4.651942
2.135462	187.974909	4.656947
2.417993	183.979259	4.661952
2.052496	192.010300	4.666957
2.167356	179.442306	4.671962
2.349483	195.622602	4.676966
1.867488	199.957208	4.681971
2.707339	204.968794	4.686976
2.526063	216.378771	4.691981
2.460775	194.261306	4.696986
2.718475	194.538909	4.701990
2.215559	190.970600	4.706995
2.724148	200.553829	4.712000
2.582218	205.416418	4.717005
2.539225	205.634677	4.722010
2.452879	193.137411	4.727014
2.713683	204.103700	4.732019
2.761591	199.987796	4.737024
2.471393	208.564391	4.742029
2.472456	199.909886	4.747034
2.946449	219.425781	4.752038
2.650581	210.138834	4.757043
2.797584	195.845517	4.762048
2.608811	199.053546	4.767053
2.617339	195.280643	4.772058
2.278141	199.860480	4.777062
2.716235	207.711786	4.782067
3.061884	216.306033	4.787072
2.992693	212.769032	4.792077
2.868793	192.557892	4.797082
2.775559	197.550715	4.802086
2.563139	202.276426	4.807091
2.789717	195.038598	4.812096
2.594150	200.362981	4.817101
2.554321	198.672690	4.822106
2.835505	215.315670	4.827110
2.716946	216.513823	4.832115
3.170058	223.898115	4.837120
2.827340	224.030033	4.842125
2.961712	216.849354	4.847130
2.879799	216.233438	4.852134
2.761534	217.788126	4.857139
3.406480	222.468821	4.862144
2.873323	210.203083	4.867149
2.772893	204.454224	4.872154
2.656278	204.951122	4.877158
2.935456	225.436743	4.882163
3.176764	217.044021	4.887168
2.787709	226.136314	4.892173
3.104793	215.161702	4.897178
2.968661	218.935426	4.902182
2.630341	225.711261	4.907187
3.151610	226.346830	4.912192
2.970253	224.409909	4.917197
3.085355	221.896632	4.922202
2.914916	228.589508	4.927206
3.090931	231.424135	4.932211
3.089216	226.337889	4.937216
2.781807	231.650878	4.942221
2.923512	230.836373	4.947226
3.264824	220.190043	4.952230
3.067351	231.126949	4.957235
2.995480	224.114143	4.962240
2.889218	238.745784	4.967245
3.181316	227.471027	4.972250
3.202329	228.670847	4.977254
3.131151	222.851603	4.982259
3.038132	222.388889	4.987264
2.846707	220.154482	4.992269
2.811504	222.197581	4.997274
3.044078	227.358459	5.002278
3.157087	234.749952	5.007283
3.575839	246.097514	5.012288
3.243077	254.069471	5.017293
3.745038	252.377133	5.022298
3.489261	242.308963	5.027302
3.325190	231.014711	5.032307
2.913946	232.040302	5.037312
3.094568	242.806035	5.042317
3.369755	252.986352	5.047322
3.404258	257.315835	5.052326
3.248035	259.944221	5.057331
3.529547	260.060987	5.062336
3.441562	256.299375	5.067341
3.152445	256.822775	5.072346
3.563776	259.694664	5.077350
3.149392	257.940920	5.082355
3.601185	260.912645	5.087360
3.519762	256.989705	5.092365
3.578712	257.625948	5.097370
3.500959	262.249767	5.102374
3.512642	260.591756	5.107379
3.472403	255.673718	5.112384
3.149099	268.715225	5.117389
3.545607	261.659677	5.122394
3.381763	265.895244	5.127398
3.485722	252.367388	5.132403
3.592951	261.463448	5.137408
3.591480	264.183133	5.142413
3.652721	268.885085	5.147418
3.420782	263.902410	5.152422
3.279174	263.306478	5.157427
3.634287	252.433067	5.162432
3.619466	264.958179	5.167437
3.573520	259.388304	5.172442
3.656184	255.360341	5.177446
3.460020	255.977221	5.182451
3.866158	259.021260	5.187456
3.545046	268.260152	5.192461
3.951371	280.961946	5.197466
3.686473	263.227817	5.202470
3.681109	282.587849	5.207475
4.013008	285.405260	5.212480
3.398189	284.154485	5.217485
4.112115	280.201562	5.222490
3.808450	288.497066	5.227494
4.036329	279.289180	5.232499
4.027052	272.513012	5.237504
3.746974	265.271747	5.242509
3.719224	263.237064	5.247514
3.626043	261.575170	5.252518
3.873458	276.318361	5.257523
4.255052	278.553857	5.262528
3.831293	287.315102	5.267533
4.050681	277.825452	5.272538
4.043706	272.049194	5.277542
3.622441	272.864712	5.282547
4.294559	280.310903	5.287552
3.975980	284.268297	5.292557
4.189311	265.678558	5.297562
3.626735	266.878884	5.302566
3.671115	271.153646	5.307571
3.942254	282.818616	5.312576
4.164408	283.568235	5.317581
4.171661	285.575870	5.322586
4.190221	277.345447	5.327590
4.208364	289.307233	5.332595
4.491681	279.475827	5.337600
3.808691	269.922652	5.342605
3.998046	274.993048	5.347610
4.067795	276.584178	5.352614
3.931122	285.024790	5.357619
4.250612	277.301624	5.362624
4.020204	285.390772	5.367629
4.108893	279.608675	5.372634
3.600363	282.454478	5.377638
3.752346	281.940580	5.382643
3.965928	277.079409	5.387648
4.033693	283.440265	5.392653
4.132920	287.024714	5.397658
4.116259	288.389063	5.402662
4.141749	295.152016	5.407667
4.709760	294.877010	5.412672
4.236805	301.858975	5.417677
4.005007	290.569030	5.422682
4.229252	298.731407	5.427686
4.520066	309.928008	5.432691
4.433159	303.730885	5.437696
4.374856	295.718457	5.442701
4.376613	293.067324	5.447706
4.116001	294.650613	5.452710
4.167110	308.931941	5.457715
4.516555	305.848275	5.462720
4.498110	317.129830	5.467725
4.821692	311.546666	5.472730
4.488793	308.340005	5.477734
4.431836	294.760912	5.482739
4.475625	288.387953	5.487744
4.104222	292.375836	5.492749
4.420940	297.511504	5.497754
4.646139	308.399720	5.502758
4.410071	316.245129	5.507763
4.824734	312.789497	5.512768
4.127674	316.694761	5.517773
4.615598	313.828037	5.522778
4.264868	315.512740	5.527782
4.372002	322.347778	5.532787
4.631162	316.570288	5.537792
4.380051	320.593438	5.542797
4.630123	318.004036	5.547802
4.545268	317.515492	5.552806
4.465246	320.126290	5.557811
4.842767	316.990989	5.562816
4.738768	322.901872	5.567821
4.597206	307.483254	5.572826
4.751530	306.309865	5.577830
4.511334	320.570752	5.582835
4.777488	316.542271	5.587840
4.617222	314.714117	5.592845
4.765690	316.160543	5.597850
4.775918	318.630637	5.602854
4.376034	320.877234	5.607859
4.820706	315.403789	5.612864
4.757972	325.007661	5.617869
5.040590	312.068115	5.622874
4.624399	315.452497	5.627878
4.602038	317.437035	5.632883
4.579402	314.226164	5.637888
4.579868	323.149774	5.642893
4.522961	332.262895	5.647898
4.843468	342.402389	5.652902
4.493152	350.351856	5.657907
5.238516	341.742677	5.662912
4.961657	336.195171	5.667917
5.234604	339.992691	5.672922
5.158346	346.839870	5.677926
5.085116	346.054178	5.682931
5.361291	341.594029	5.687936
4.929752	333.278941	5.692941
4.933560	320.305216	5.697946
5.022154	316.271516	5.702950
5.042748	333.497847	5.707955
4.923364	316.222550	5.712960
4.789613	329.213066	5.717965
5.220136	335.237970	5.722970
5.370507	337.170121	5.727974
4.971602	331.516607	5.732979
5.117736	324.475413	5.737984
5.003262	327.017740	5.742989
5.142753	327.315389	5.747994
4.967609	338.088028	5.752998
4.956035	342.646604	5.758003
5.528735	338.158285	5.763008
5.034990	344.248608	5.768013
5.294891	342.642474	5.773018
4.931926	350.516688	5.778022
4.786113	351.640447	5.783027
5.006983	341.830827	5.788032
4.682038	347.575187	5.793037
4.922292	347.996986	5.798042
4.648813	343.262729	5.803046
5.155543	355.834231	5.808051
5.572793	354.875648	5.813056
4.937937	362.011042	5.818061
5.286449	363.869217	5.823066
5.752792	367.732478	5.828070
5.482998	365.908906	5.833075
5.443638	348.436552	5.838080
5.215454	354.435577	5.843085
5.123514	346.242033	5.848090
5.182453	359.082737	5.853094
5.251010	374.825067	5.858099
5.443952	379.114633	5.863104
5.403546	387.435501	5.868109
5.721834	382.982154	5.873114
5.671862	374.211120	5.878118
5.054070	370.723037	5.883123
5.131761	371.825040	5.888128
5.217107	378.645373	5.893133
5.049340	382.569042	5.898138
5.823060	377.817008	5.903142
5.773363	373.760300	5.908147
5.658247	374.387788	5.913152
5.621008	369.893685	5.918157
5.758036	369.434762	5.923162
5.809795	374.876755	5.928166
5.645870	380.995154	5.933171
5.958924	370.843799	5.938176
5.460782	379.106160	5.943181
5.760375	370.750436	5.948186
5.664684	370.645537	5.953190
5.459270	373.249361	5.958195
5.822033	368.588724	5.963200
5.935347	375.520835	5.968205
5.655884	358.847531	5.973210
5.578280	352.661866	5.978214
5.498170	366.146507	5.983219
5.692388	362.570425	5.988224
5.407198	383.914740	5.993229
5.412296	374.436574	5.998234
5.553598	383.694778	6.003238
5.559087	378.916313	6.008243
6.065965	375.716678	6.013248
5.514793	378.226417	6.018253
5.801055	378.847379	6.023258
5.729488	380.992646	6.028262
5.786436	381.937860	6.033267
5.890409	383.143045	6.038272
5.729659	372.265307	6.043277
5.629304	384.518003	6.048282
5.768186	370.989568	6.053286
5.708853	378.165078	6.058291
5.971857	375.226008	6.063296
5.564541	372.053015	6.068301
5.427715	340.319386	6.073306
5.711149	356.449071	6.078310
5.675683	372.517125	6.083315
5.959422	367.020682	6.088320
5.544979	360.216703	6.093325
5.823888	368.291096	6.098330
5.720395	363.652704	6.103334
5.245332	355.065213	6.108339
5.959963	355.668649	6.113344
5.649432	365.543828	6.118349
5.617544	369.296118	6.123354
5.747003	362.989797	6.128358
5.567385	377.975154	6.133363
5.856757	369.394391	6.138368
5.809836	365.621190	6.143373
5.493100	358.123319	6.148378
5.799724	357.713563	6.153382
5.450879	349.322758	6.158387
5.942924	367.154536	6.163392
5.854989	363.794468	6.168397
5.647062	354.332777	6.173402
5.606681	347.543986	6.178406
5.603363	355.307906	6.183411
5.846946	339.465299	6.188416
5.383623	340.505078	6.193421
5.513191	352.952981	6.198426
5.660899	364.370743	6.203430
5.968014	377.488516	6.208435
5.663019	351.078541	6.213440
5.340575	355.916715	6.218445
5.804797	370.208370	6.223450
5.817977	363.396066	6.228454
5.676529	374.900181	6.233459
6.020196	361.494796	6.238464
5.809428	362.107989	6.243469
5.469770	341.721169	6.248474
5.679842	343.784690	6.253478
5.385257	348.580146	6.258483
5.513126	352.859998	6.263488
5.689680	363.220571	6.268493
6.086533	367.194051	6.273498
5.942853	350.013134	6.278502
5.582283	354.737664	6.283507
5.633049	343.405056	6.288512
5.209461	349.817613	6.293517
5.790300	358.331409	6.298522
6.128667	370.113539	6.303526
5.698041	356.082439	6.308531
6.015211	350.598600	6.313536
5.767537	350.693013	6.318541
5.693584	343.144928	6.323546
5.954147	336.047019	6.328550
5.802650	344.819284	6.333555
5.571507	342.634283	6.338560
5.814929	340.985303	6.343565
5.510078	345.942306	6.348570
5.679699	340.833858	6.353574
5.263081	344.381909	6.358579
5.637960	341.403925	6.363584
5.613165	341.945161	6.368589
5.693658	329.824000	6.373594
6.104439	343.639461	6.378598
5.673833	340.962502	6.383603
5.855261	338.006017	6.388608
5.450990	342.886796	6.393613
5.502554	343.974590	6.398618
5.762568	340.433557	6.403622
5.173339	344.330377	6.408627
5.369756	338.062863	6.413632
5.399142	356.720615	6.418637
6.048555	363.626565	6.423642
5.880322	357.834059	6.428646
5.743813	356.243096	6.433651
5.885721	344.863961	6.438656
5.395785	336.683492	6.443661
5.452352	338.526843	6.448666
6.028194	342.749205	6.453670
5.781333	337.764053	6.458675
5.749786	342.282733	6.463680
5.374280	345.266278	6.468685
5.336863	349.219581	6.473690
5.451705	350.629962	6.478694
5.910110	372.133449	6.483699
6.112602	365.319871	6.488704
5.890439	357.063309	6.493709
5.378702	349.047286	6.498714
5.528379	342.892127	6.503718
5.126606	348.158482	6.508723
5.848803	356.696931	6.513728
6.121198	376.243967	6.518733
5.662665	359.443937	6.523738
5.586247	356.913335	6.528742
5.733369	358.636852	6.533747
5.729065	349.616505	6.538752
5.728247	347.819861	6.543757
5.287146	353.670160	6.548762
5.902559	363.510034	6.553766
5.580030	370.081037	6.558771
5.906436	368.880226	6.563776
5.492534	370.074791	6.568781
5.418596	365.229216	6.573786
6.014430	373.311518	6.578790
5.905046	371.506671	6.583795
5.844029	357.505502	6.588800
5.794521	355.727804	6.593805
5.758673	349.447780	6.598810
5.519932	340.336163	6.603814
5.599867	342.528271	6.608819
5.623544	345.464609	6.613824
5.746796	353.213214	6.618829
5.652078	348.747024	6.623834
5.662504	337.450134	6.628838
5.627437	341.369496	6.633843
5.502753	341.102865	6.638848
5.299844	343.277653	6.643853
5.600704	360.740017	6.648858
5.971416	377.705539	6.653862
5.635906	378.932266	6.658867
6.020847	367.765113	6.663872
5.675624	353.725542	6.668877
5.580301	343.282535	6.673882
5.783007	342.236870	6.678886
5.360824	349.085898	6.683891
5.770877	363.681963	6.688896
5.685368	364.985932	6.693901
5.616900	368.045928	6.698906
5.951813	357.643291	6.703910
5.517151	367.204815	6.708915
5.579428	355.907581	6.713920
5.713693	367.653383	6.718925
5.776552	370.705759	6.723930
5.850918	355.681989	6.728934
5.448555	359.116179	6.733939
5.637179	349.904711	6.738944
5.721130	363.008454	6.743949
5.713299	370.714129	6.748954
5.672491	364.253375	6.753958
5.548533	372.183976	6.758963
5.844939	362.405400	6.763968
5.686506	349.782248	6.768973
5.445141	351.220261	6.773978
5.846352	347.949788	6.778982
5.691051	377.076559	6.783987
5.670097	372.117784	6.788992
5.729394	374.796012	6.793997
5.827612	358.907295	6.799002
5.830019	354.468571	6.804006
5.502128	353.449922	6.809011
5.787771	354.687858	6.814016
5.478419	341.452994	6.819021
5.529152	352.777937	6.824026
5.836102	352.676760	6.829030
5.577936	359.529316	6.834035
5.585360	355.826809	6.839040
5.667667	355.386848	6.844045
5.930628	370.789806	6.849050
5.877693	359.293071	6.854054
5.481094	352.711093	6.859059
5.457531	348.018769	6.864064
5.602585	355.279883	6.869069
5.957880	369.631083	6.874074
5.683298	351.974239	6.879078
5.454998	353.499079	6.884083
5.736313	364.500751	6.889088
5.955602	383.383312	6.894093
5.608639	372.301300	6.899098
5.698770	356.480038	6.904102
5.506243	345.169120	6.909107
5.729231	351.551762	6.914112
5.767165	348.277930	6.919117
5.560361	357.957472	6.924122
6.033360	356.707234	6.929126
5.546536	343.491013	6.934131
5.621512	345.179751	6.939136
5.460710	346.246800	6.944141
5.640526	357.435836	6.949146
5.918820	364.196860	6.954150
5.611604	352.214914	6.959155
5.971381	348.552117	6.964160
5.664664	343.991515	6.969165
5.349899	349.218741	6.974170
5.842971	351.223780	6.979174
5.738168	353.060211	6.984179
5.626334	345.989858	6.989184
5.455030	346.614843	6.994189
5.509349	359.239640	6.999194
6.011185	366.084674	7.004198
5.598099	367.966031	7.009203
5.518093	365.581658	7.014208
5.659998	364.146096	7.019213
5.379078	371.004807	7.024218
5.887684	361.338173	7.029222
5.519483	375.860546	7.034227
6.097593	373.118535	7.039232
5.975136	372.041862	7.044237
5.557812	360.464596	7.049242
5.567284	339.388273	7.054246
5.425626	354.097539	7.059251
5.942040	359.857561	7.064256
5.682817	361.097260	7.069261
5.413031	363.429788	7.074266
5.764864	361.701809	7.079270
5.735249	371.469915	7.084275
6.041877	372.658978	7.089280
5.723966	355.237256	7.094285
5.354270	352.945633	7.099290
5.666282	348.862357	7.104294
5.827040	366.801295	7.109299
5.921880	355.228299	7.114304
5.766163	352.918475	7.119309
5.338898	357.527599	7.124314
5.500977	345.407469	7.129318
5.530869	356.723052	7.134323
5.852699	366.944828	7.139328
5.830119	365.412876	7.144333
5.755962	353.363775	7.149338
5.738475	345.878135	7.154342
5.405763	344.467983	7.159347
5.608276	350.930793	7.164352
5.742797	367.257711	7.169357
5.694295	370.849566	7.174362
5.653948	362.086609	7.179366
5.535931	373.362456	7.184371
5.750089	372.762247	7.189376
5.479239	377.830037	7.194381
5.585740	376.486989	7.199386
5.978024	376.160282	7.204390
5.704464	385.975259	7.209395
5.852471	368.721369	7.214400
5.777683	355.062897	7.219405
5.582935	355.294739	7.224410
5.667502	355.598952	7.229414
5.627386	358.671008	7.234419
5.836886	358.555244	7.239424
5.606086	349.436776	7.244429
5.568897	351.761624	7.249434
5.813878	355.606421	7.254438
5.705651	360.226652	7.259443
5.578468	351.399397	7.264448
5.823816	346.991929	7.269453
5.676370	344.657249	7.274458
5.577536	340.014340	7.279462
5.460309	347.047707	7.284467
5.944732	365.364815	7.289472
5.683843	365.760192	7.294477
5.538517	356.846556	7.299482
5.619080	356.643294	7.304486
5.694304	373.989845	7.309491
5.895821	369.455467	7.314496
5.555366	360.057043	7.319501
5.471605	360.795550	7.324506
5.716854	369.685802	7.329510
5.516942	374.694243	7.334515
5.693590	375.131943	7.339520
5.583585	375.069483	7.344525
5.509987	371.794056	7.349530
6.015129	373.950619	7.354534
5.872852	381.900453	7.359539
6.002686	373.743837	7.364544
5.617046	355.845753	7.369549
5.679056	354.895105	7.374554
5.491623	339.712792	7.379558
5.629898	369.753161	7.384563
5.985922	364.720680	7.389568
5.656225	341.907927	7.394573
5.473790	354.427226	7.399578
5.542277	351.037610	7.404582
5.337694	370.498946	7.409587
5.965250	372.522680	7.414592
5.925152	375.888570	7.419597
5.826141	364.619519	7.424602
5.658576	351.723192	7.429606
5.460623	357.611223	7.434611
5.856950	355.968795	7.439616
5.491585	355.612123	7.444621
5.716042	363.617815	7.449626
5.891656	362.736690	7.454630
5.485164	353.665972	7.459635
5.681114	348.267600	7.464640
5.494430	361.773108	7.469645
5.654288	371.455849	7.474650
5.923407	377.368278	7.479654
5.787808	377.445247	7.484659
5.582019	357.207641	7.489664
5.576675	359.222312	7.494669
5.622825	372.520999	7.499674
5.885172	366.246265	7.504678
5.712001	368.897417	7.509683
5.709603	354.263912	7.514688
5.618553	346.966522	7.519693
5.371241	355.652301	7.524698
5.584931	368.907943	7.529702
5.516386	377.697815	7.534707
5.857028	374.487527	7.539712
5.893414	377.888658	7.544717
5.572907	375.141690	7.549722
5.859372	374.653193	7.554726
5.848324	377.292397	7.559731
5.914883	359.348354	7.564736
5.527722	355.940736	7.569741
5.128664	350.199426	7.574746
5.844271	367.761386	7.579750
5.735182	377.854892	7.584755
5.770839	371.137715	7.589760
5.936280	365.467939	7.594765
5.461595	356.947676	7.599770
5.754997	344.505373	7.604774
5.481801	356.493928	7.609779
5.803774	368.584457	7.614784
5.790532	359.477183	7.619789
5.229757	347.679665	7.624794
5.779203	362.872393	7.629798
5.922617	377.912001	7.634803
5.717977	361.544561	7.639808
5.567986	362.423134	7.644813
5.761665	372.651020	7.649818
5.721951	362.767678	7.654822
5.215531	362.408007	7.659827
5.652037	368.990590	7.664832
5.747894	372.070437	7.669837
5.474078	377.143851	7.674842
5.873909	369.710198	7.679846
5.748421	377.554821	7.684851
5.542434	377.017340	7.689856
5.625280	375.440236	7.694861
5.371895	371.201695	7.699866
5.537295	374.572304	7.704870
5.509731	379.951114	7.709875
5.801784	375.484961	7.714880
5.684465	375.441674	7.719885
5.725800	380.001926	7.724890
5.752859	375.730190	7.729894
5.481916	385.588342	7.734899
5.146611	378.488616	7.739904
5.514739	383.816459	7.744909
5.074910	381.807431	7.749914
5.321633	378.844229	7.754918
5.671560	387.058383	7.759923
5.680542	395.103062	7.764928
5.688040	394.655801	7.769933
6.019169	412.753550	7.774938
5.989769	387.082909	7.779942
5.461682	384.758999	7.784947
5.555829	380.489726	7.789952
5.922659	385.380882	7.794957
5.620057	387.571655	7.799962
5.907867	382.800728	7.804966
5.776737	384.443215	7.809971
5.702737	386.745770	7.814976
5.556465	383.594507	7.819981
5.390455	391.589336	7.824986
5.758647	387.039484	7.829990
5.636108	383.683190	7.834995
5.688573	380.839696	7.840000
5.901521	376.460890	7.845005
5.779128	373.845178	7.850010
6.072463	376.094963	7.855014
6.084400	382.550389	7.860019
5.795458	375.106499	7.865024
6.154654	380.181261	7.870029
5.820215	376.415393	7.875034
6.036949	378.967601	7.880038
5.741600	379.949862	7.885043
5.798541	382.509094	7.890048
5.731796	360.832877	7.895053
5.514531	355.899633	7.900058
5.925092	356.259184	7.905062
5.750457	345.575781	7.910067
5.455583	348.724712	7.915072
5.808774	352.473772	7.920077
5.451833	353.624335	7.925082
5.778527	355.193289	7.930086
6.060085	361.659343	7.935091
5.646920	355.004143	7.940096
5.687975	341.709655	7.945101
5.818184	347.415264	7.950106
5.889757	338.708508	7.955110
5.588311	339.788080	7.960115
5.598283	340.242235	7.965120
5.494952	334.237273	7.970125
5.539848	340.455379	7.975142
5.890449	344.994885	7.980160
5.162507	342.714288	7.985178
5.488004	365.937995	7.990195
5.985280	373.574508	7.995213
5.622878	377.176131	8.000230
6.009466	366.691696	8.005248
5.837264	357.660065	8.010266
5.798124	351.243487	8.015283
5.679911	340.533357	8.020301
5.350709	347.566940	8.025318
5.771493	363.471329	8.030336
5.885403	361.688345	8.035354
5.752112	361.028833	8.040371
5.612016	349.410406	8.045389
5.479344	361.727193	8.050406
5.962895	370.969191	8.055424
5.797429	371.402135	8.060442
6.112053	360.725550	8.065459
5.485866	356.516397	8.070477
5.880605	360.068344	8.075494
5.782796	358.422706	8.080512
5.786955	368.123089	8.085530
5.728408	369.520459	8.090547
5.891014	380.632772	8.095565
5.671550	373.804267	8.100582
5.965963	370.082197	8.105600
5.651148	364.751894	8.110618
5.820638	369.272695	8.115635
5.873092	371.046266	8.120653
5.694020	383.778817	8.125670
6.158008	373.086846	8.130688
5.973802	374.245873	8.135706
5.732676	356.739242	8.140723
5.549666	362.964351	8.145741
5.563912	370.174106	8.150758
5.760815	373.141474	8.155776
5.845314	380.256887	8.160794
5.702975	385.310386	8.165811
5.834692	374.937988	8.170829
5.898303	382.195641	8.175846
6.115851	385.548522	8.180864
6.114141	388.306996	8.185882
5.883345	386.332703	8.190899
6.266948	380.051539	8.195917
5.955793	384.368991	8.200934
6.053307	383.438656	8.205952
5.972917	385.467949	8.210970
5.965202	376.214299	8.215987
6.134078	357.197915	8.221005
5.746626	360.212214	8.226022
5.751067	348.373916	8.231040
5.664265	379.788282	8.236058
5.778616	380.054846	8.241075
5.949825	377.334465	8.246093
5.845147	383.218639	8.251110
6.072894	380.231795	8.256128
5.790402	380.462557	8.261146
5.824790	378.743178	8.266163
5.818318	372.725260	8.271181
5.631645	387.059528	8.276198
5.888036	376.815802	8.281216
5.847959	377.575513	8.286234
5.908464	376.746990	8.291251
6.072096	374.311702	8.296269
5.850141	382.771049	8.301286
5.479467	379.076261	8.306304
5.998494	386.062175	8.311322
5.845993	396.117522	8.316339
6.040690	385.315000	8.321357
6.095647	394.811698	8.326374
5.955436	391.843102	8.331392
6.242607	397.175185	8.336410
6.107376	399.453732	8.341427
5.996729	400.148408	8.346445
5.819783	406.142232	8.351462
6.041940	395.793367	8.356480
6.080316	404.504509	8.361498
6.027011	403.556724	8.366515
6.299360	396.642527	8.371533
6.209909	403.443979	8.376550
6.294927	403.536104	8.381568
6.245558	397.104477	8.386586
5.930188	378.541357	8.391603
6.312455	391.396146	8.396621
6.022996	397.064405	8.401638
6.423504	392.996180	8.406656
6.394540	391.470778	8.411674
5.830168	385.876461	8.416691
6.169709	381.107017	8.421709
6.053734	385.876238	8.426726
6.316057	383.119060	8.431744
6.079420	379.918878	8.436762
5.879871	384.655537	8.441779
5.966845	393.458980	8.446797
6.133891	401.203540	8.451814
6.090437	404.200431	8.456832
6.158123	408.324028	8.461850
6.212252	410.438437	8.466867
5.993077	403.331745	8.471885
5.922121	403.699576	8.476902
6.177083	409.374980	8.481920
6.307073	400.021072	8.486938
6.217645	403.428916	8.491955
6.251471	396.484882	8.496973
6.068305	410.461730	8.501990
6.179165	409.461464	8.507008
6.236778	409.175499	8.512026
5.824875	411.015233	8.517043
6.143005	404.462683	8.522061
6.026264	411.511371	8.527078
6.013481	402.261697	8.532096
6.477862	405.208035	8.537114
6.141715	405.650848	8.542131
6.221427	404.346337	8.547149
6.040039	413.550862	8.552166
6.125494	424.015653	8.557184
6.789327	426.381057	8.562202
6.147551	430.114552	8.567219
6.086707	417.080462	8.572237
6.266294	425.973048	8.577255
6.381009	425.849429	8.582272
6.563145	429.601085	8.587290
6.335278	423.029051	8.592307
6.287015	405.006296	8.597325
5.989739	416.280892	8.602343
6.337195	433.743867	8.607360
6.476833	429.760327	8.612378
6.592881	442.329710	8.617395
6.578388	421.757047	8.622413
6.258523	415.762071	8.627431
6.217331	411.652896	8.632448
6.553437	422.964139	8.637466
6.618475	426.941540	8.642483
6.452939	415.965230	8.647501
6.132677	415.049415	8.652519
6.636871	419.244150	8.657536
6.655087	408.445160	8.662554
6.349806	412.496312	8.667571
6.447256	406.225892	8.672589
6.030153	395.952770	8.677607
5.960324	426.919174	8.682624
6.332325	420.304321	8.687642
6.495897	434.432989	8.692659
6.566092	435.874906	8.697677
6.798272	440.886644	8.702695
6.722028	430.075192	8.707712
6.772141	420.684159	8.712730
6.303448	409.733637	8.717747
6.088459	405.558477	8.722765
6.556673	418.849950	8.727783
6.635709	436.802583	8.732800
6.841117	428.163227	8.737818
6.454649	409.054257	8.742835
6.372950	406.988059	8.747853
6.367637	414.247145	8.752871
6.404350	431.556272	8.757888
6.752231	435.581734	8.762906
6.607046	440.787089	8.767923
6.351804	429.154083	8.772941
6.476329	427.440778	8.777959
6.592194	441.085887	8.782976
6.841432	439.444561	8.787994
6.834600	436.210107	8.793011
6.694116	415.423373	8.798029
6.478063	410.461645	8.803047
6.303480	414.472572	8.808064
6.371131	411.931588	8.813082
6.451405	417.932265	8.818099
6.623635	430.776529	8.823117
6.976576	441.210258	8.828135
6.470636	427.521459	8.833152
6.872845	429.994319	8.838170
6.493674	426.856200	8.843187
6.613100	429.828583	8.848205
6.479102	435.038179	8.853223
6.311951	431.147360	8.858240
6.324071	435.020969	8.863258
6.478649	440.066864	8.868275
6.774560	431.677795	8.873293
7.032454	436.911618	8.878311
6.875560	427.553806	8.883328
6.978666	430.946583	8.888346
6.545178	439.739126	8.893363
6.634317	440.145501	8.898381
6.686819	435.928825	8.903399
6.215263	436.353597	8.908416
6.240026	434.664746	8.913434
6.436855	443.183445	8.918451
6.625744	440.701433	8.923469
6.724149	443.059844	8.928487
6.772258	443.262229	8.933504
6.846029	436.726464	8.938522
6.888765	435.313539	8.943539
6.800015	434.335820	8.948557
7.044791	428.419218	8.953575
6.861930	438.415865	8.958592
6.857904	431.888899	8.963610
6.740399	438.976699	8.968627
6.996382	434.791158	8.973645
6.874791	431.916696	8.978663
6.696484	435.011985	8.983680
6.732678	433.755056	8.988698
6.692678	436.637807	8.993715
6.699737	433.466393	8.998733
6.710151	434.008677	9.003751
6.625401	438.324139	9.008768
7.101920	435.516588	9.013786
6.766377	436.001816	9.018803
6.866236	431.839470	9.023821
7.060680	439.812941	9.028839
6.919276	438.650485	9.033856
7.020086	429.529737	9.038874
6.674913	440.768418	9.043891
6.854749	434.092988	9.048909
7.272488	435.105910	9.053927
6.920179	435.725607	9.058944
6.861266	437.357669	9.063962
6.944477	435.549861	9.068979
6.650522	434.753874	9.073997
7.230151	428.926879	9.079015
6.994799	431.455911	9.084032
7.108085	434.137017	9.089050
6.917028	433.360736	9.094067
6.741539	445.141641	9.099085
6.807503	433.482800	9.104103
6.720317	441.009619	9.109120
6.650085	437.562099	9.114138
6.742758	432.932876	9.119155
6.685082	432.530652	9.124173
6.932425	434.238966	9.129191
6.895447	435.900253	9.134208
6.903301	432.325396	9.139226
6.712752	438.296101	9.144243
6.836391	454.397204	9.149261
7.231308	450.808594	9.154279
6.857045	457.824128	9.159296
7.358363	452.146744	9.164314
7.071403	453.864346	9.169331
6.693479	447.877039	9.174349
6.762740	446.736453	9.179367
6.633902	468.274953	9.184384
6.878957	464.175663	9.189402
7.405613	465.366137	9.194419
7.191775	467.761491	9.199437
7.398916	456.818476	9.204455
7.006521	459.481480	9.209472
7.558186	458.603991	9.214490
7.240944	459.665658	9.219507
7.234477	452.520045	9.224525
7.256842	440.711372	9.229543
7.376132	439.093415	9.234560
7.327330	436.280863	9.239578
7.357450	436.231141	9.244595
7.186158	437.172887	9.249613
7.233911	428.319204	9.254631
6.582102	434.617538	9.259648
6.902716	438.855979	9.264666
6.808258	428.614634	9.269683
7.021023	439.695033	9.274701
7.301724	443.798784	9.279719
7.354777	454.580964	9.284736
6.927923	450.921675	9.289754
7.434984	452.695672	9.294771
7.231464	458.009540	9.299789
7.282023	442.025067	9.304807
7.117100	441.153505	9.309824
6.920406	439.323524	9.314842
7.467334	462.414911	9.319859
7.225535	446.404034	9.324877
7.353409	440.734988	9.329895
7.196042	440.249933	9.334912
7.063933	434.440063	9.339930
7.357891	449.802873	9.344947
7.106486	460.179793	9.349965
7.535916	461.552162	9.354983
7.277455	449.997227	9.360000
6.945279	441.062209	9.365018
7.314789	449.420528	9.370035
7.183061	464.462998	9.375053
7.376297	467.550865	9.380071
7.461509	467.509899	9.385088
7.538732	464.700211	9.390106
7.709630	457.495788	9.395123
7.253356	451.712628	9.400141
7.277907	438.832028	9.405159
7.326134	437.894528	9.410176
6.886568	448.219455	9.415194
7.213974	451.284034	9.420211
7.245391	457.425316	9.425229
7.303384	465.680514	9.430247
7.382552	466.481033	9.435264
7.434674	468.439695	9.440282
7.625607	465.422146	9.445299
7.568038	472.853514	9.450317
7.487011	466.249773	9.455335
7.290599	468.470591	9.460352
7.336442	470.185434	9.465370
7.758380	461.639980	9.470387
7.203788	455.455084	9.475405
7.415622	456.910859	9.480423
7.440965	464.099524	9.485440
7.608588	469.693609	9.490458
7.489315	466.823479	9.495475
7.414281	474.009345	9.500493
7.427622	460.680627	9.505511
7.140859	469.777513	9.510528
7.282980	463.472876	9.515546
7.524013	468.507166	9.520563
7.559811	465.931904	9.525581
7.590443	465.107357	9.530599
7.513685	473.625291	9.535616
7.532779	463.735097	9.540634
7.651368	462.859320	9.545651
7.524403	466.687360	9.550669
7.663877	465.513451	9.555687
7.850800	463.134903	9.560704
7.408713	470.559714	9.565722
7.625760	458.680679	9.570739
7.528589	469.342181	9.575757
7.449682	466.083483	9.580775
7.395639	473.129651	9.585792
7.363048	465.584864	9.590810
7.658043	455.227987	9.595827
7.339756	463.949235	9.600845
7.709947	456.085361	9.605863
7.607270	458.615965	9.610880
7.610168	468.946884	9.615898
7.565167	457.815481	9.620915
7.629749	460.405679	9.625933
7.492933	461.086205	9.630951
7.411655	465.098171	9.635968
7.429831	462.516193	9.640986
7.487581	459.465866	9.646003
7.345695	464.310475	9.651021
7.555360	468.734872	9.656039
7.625242	460.895322	9.661056
7.551212	472.956998	9.666074
7.889793	466.287646	9.671091
7.417695	468.808400	9.676109
7.709682	479.000338	9.681127
7.874904	498.787387	9.686144
7.699778	486.186767	9.691162
7.980938	476.163250	9.696179
7.390999	473.635107	9.701197
7.664146	490.942598	9.706215
7.662401	494.395332	9.711232
7.907474	496.986636	9.716250
7.856557	490.180848	9.721267
7.720156	502.387549	9.726285
7.969797	487.663538	9.731303
8.107764	479.018041	9.736320
7.526633	474.019737	9.741338
7.833796	462.657370	9.746355
7.552872	472.021572	9.751373
7.912346	487.432778	9.756391
8.157643	481.529848	9.761408
7.700869	475.543432	9.766426
7.916488	467.907590	9.771443
7.591448	469.269938	9.776461
7.839433	489.678010	9.781479
8.122682	500.318623	9.786496
7.909033	485.314166	9.791514
8.168707	473.620932	9.796531
7.910555	470.550674	9.801549
7.722609	474.495339	9.806567
8.035585	462.804080	9.811584
7.692087	464.624380	9.816602
7.616780	454.951834	9.821619
7.710904	472.113484	9.826637
7.969039	486.259944	9.831655
7.862753	491.219894	9.836672
7.980322	487.892514	9.841690
8.122636	495.370388	9.846707
7.894565	498.059624	9.851725
8.040995	499.940808	9.856743
7.657805	488.333550	9.861760
7.704787	506.715771	9.866778
8.034412	499.704417	9.871795
7.854940	502.485175	9.876813
8.077024	496.248329	9.881831
8.068762	493.582953	9.886848
8.025199	491.307272	9.891866
8.190613	496.250408	9.896883
8.203204	508.685676	9.901901
8.111589	498.134781	9.906919
8.171872	503.240461	9.911936
7.812241	498.958028	9.916954
8.356514	502.728049	9.921971
8.394145	501.212825	9.926989
8.267440	487.054083	9.932007
8.176158	475.357571	9.937024
7.655844	476.884847	9.942042
7.993697	489.712261	9.947059
7.685723	499.438820	9.952077
8.023935	502.606527	9.957095
8.516178	491.332659	9.962112
8.064270	497.482250	9.967130
8.006588	497.568372	9.972147
7.859075	498.624269	9.977165
8.202873	501.165113	9.982183
8.401704	504.573095	9.987200
7.921863	501.551292	9.992218
8.231663	502.028463	9.997235
8.159628	492.835036	10.002253
8.249061	502.071365	10.007271
8.253410	503.966323	10.012288
7.985073	506.732524	10.017306
7.881762	501.108575	10.022323
8.206417	499.387783	10.027341
8.037383	501.066106	10.032359
8.384988	489.843049	10.037376
8.103506	497.971042	10.042394
8.109209	498.774129	10.047411
8.119536	493.691684	10.052429
8.115694	500.160471	10.057447
8.261713	495.148377	10.062464
8.095771	504.295274	10.067482
8.166062	492.478792	10.072499
8.468878	501.938295	10.077517
8.320191	500.934907	10.082535
8.439791	504.606039	10.087552
8.259123	504.399635	10.092570
8.607296	495.674509	10.097587
8.232754	492.873572	10.102605
8.427472	504.432963	10.107623
8.314495	498.420299	10.112640
8.507148	504.152547	10.117658
8.249463	497.656101	10.122675
8.041017	495.878654	10.127693
7.892696	497.838944	10.132711
8.481359	523.428797	10.137728
8.311845	523.434893	10.142746
8.656680	514.490840	10.147763
8.617566	510.270870	10.152781
8.649755	513.964012	10.157799
8.567736	504.385063	10.162816
8.491346	494.753221	10.167834
8.468741	498.946175	10.172851
8.642052	491.604535	10.177869
8.533195	492.463669	10.182887
8.356463	487.572736	10.187904
8.547662	495.348759	10.192922
8.440231	500.923617	10.197939
8.473328	491.086586	10.202957
8.056170	496.880626	10.207975
8.341386	490.786426	10.212992
8.295691	499.897588	10.218010
8.505164	508.453589	10.223027
8.663518	521.374245	10.228045
8.401646	523.139846	10.233063
8.653756	517.310961	10.238080
8.604005	516.573979	10.243098
8.616441	510.534757	10.248115
8.582364	498.524610	10.253133
8.364914	499.672441	10.258151
8.783446	513.084054	10.263168
8.740417	510.479371	10.268186
8.695067	508.992308	10.273203
8.516207	494.371595	10.278221
8.104804	494.964505	10.283239
8.821283	510.331552	10.288256
8.154908	519.020537	10.293274
8.681971	514.801728	10.298291
9.005272	524.892436	10.303309
8.549167	527.803620	10.308327
9.163037	526.081011	10.313344
8.885509	525.979085	10.318362
8.615368	503.169456	10.323379
8.370527	506.317744	10.328397
8.363432	509.878843	10.333415
8.687923	518.004544	10.338432
8.649918	522.501025	10.343450
8.287728	523.054853	10.348467
8.669806	517.973006	10.353485
8.512921	520.114433	10.358503
8.758249	521.362498	10.363520
8.628428	521.837943	10.368538
8.666220	527.276870	10.373555
8.931634	519.042615	10.378573
8.743131	522.871646	10.383591
8.855932	518.932501	10.388608
8.779105	522.916578	10.393626
8.878330	518.116569	10.398643
8.989487	520.348276	10.403661
8.789637	529.054206	10.408679
8.713656	525.839690	10.413696
9.047289	523.312742	10.418714
8.541273	529.560112	10.423731
8.863772	523.912423	10.428749
8.556430	536.837864	10.433767
8.961740	521.666325	10.438784
8.808475	533.194017	10.443802
8.847813	519.499144	10.448819
9.020651	517.032975	10.453837
8.705194	525.621712	10.458855
8.910331	522.834844	10.463872
8.667353	530.835991	10.468890
8.515671	524.295146	10.473907
8.591326	527.540550	10.478925
8.788415	553.419535	10.483943
8.964893	547.357953	10.488960
9.061518	563.129828	10.493978
9.137683	547.532299	10.498995
9.197338	543.354757	10.504013
8.985692	540.985558	10.509031
9.006058	518.293356	10.514048
8.882898	527.548896	10.519066
9.004954	533.735768	10.524083
9.008664	536.758702	10.529101
8.407035	552.577140	10.534119
9.147682	556.916851	10.539136
9.058821	553.385991	10.544154
8.892595	552.407363	10.549171
9.358204	547.747613	10.554189
9.027386	549.862643	10.559207
9.043439	542.340833	10.564224
8.967798	554.923470	10.569242
9.047551	543.804536	10.574259
9.446714	552.341039	10.579277
9.353808	546.782859	10.584295
9.301666	545.191023	10.589312
9.213459	536.191189	10.594330
9.225458	527.933700	10.599347
9.082489	516.985651	10.604365
9.121822	522.649106	10.609383
9.182811	523.167831	10.614400
9.248272	518.349616	10.619418
8.921559	515.683824	10.624435
9.333700	519.749411	10.629453
9.200070	535.912454	10.634471
9.515112	518.696042	10.639488
9.544901	516.429424	10.644506
9.255813	516.249898	10.649523
9.701928	513.619814	10.654541
9.418637	514.570928	10.659559
9.524024	510.990864	10.664576
9.435964	512.803159	10.669594
9.416783	515.486810	10.674611
9.347695	513.342130	10.679629
9.115366	517.842170	10.684647
9.070894	511.025854	10.689664
9.245056	510.873063	10.694682
9.106111	507.740861	10.699699
9.328438	504.497829	10.704717
9.431152	509.285853	10.709735
9.210994	503.182348	10.714752
8.965309	505.688702	10.719770
8.898122	510.899816	10.724787
9.509253	502.134326	10.729805
9.351984	511.732900	10.734823
9.246980	510.590174	10.739840
9.543939	509.417643	10.744858
9.087708	503.401404	10.749875
9.374785	499.288230	10.754893
9.353293	502.274011	10.759911
9.063462	509.298170	10.764928
9.447988	511.863543	10.769946
9.049491	526.964192	10.774963
9.519581	535.667033	10.779981
9.631234	553.138433	10.784999
9.742731	549.097340	10.790016
9.669144	530.260993	10.795034
9.227075	524.376633	10.800051
9.700494	527.876175	10.805069
9.679218	521.259133	10.810087
9.454659	524.541838	10.815104
9.556768	509.774812	10.820122
9.207468	520.701073	10.825139
9.357592	527.543462	10.830157
9.838386	539.700360	10.835175
9.622524	536.200651	10.840192
9.417396	528.273716	10.845210
9.382248	539.156041	10.850227
9.834874	537.057310	10.855245
9.865901	546.349433	10.860263
9.411383	526.063531	10.865280
9.577844	531.340927	10.870298
9.545574	534.184422	10.875315
9.469841	536.510379	10.880333
9.504008	541.684580	10.885351
9.697190	541.021383	10.890368
9.864761	541.578491	10.895386
9.801712	540.039646	10.900403
9.776639	536.615502	10.905421
9.647149	531.472824	10.910439
9.543166	541.577480	10.915456
9.736408	537.144093	10.920474
9.905852	536.142939	10.925491
9.410390	532.153525	10.930509
9.774457	526.697927	10.935527
9.774356	544.611087	10.940544
9.949663	540.804647	10.945562
9.827515	539.889555	10.950579
9.525194	518.337911	10.955597
9.844778	532.301378	10.960615
9.923083	524.975907	10.965632
9.759442	524.238171	10.970650
9.600773	529.720383	10.975667
10.122321	522.190149	10.980685
9.691952	518.568236	10.985703
9.779894	522.709164	10.990720
9.688471	539.691902	10.995738
9.584108	536.459860	11.000755
9.785374	539.060815	11.005773
9.562664	546.258269	11.010791
9.652306	542.064917	11.015808
10.112624	541.267562	11.020826
9.731908	540.459221	11.025843
9.806613	538.587071	11.030861
9.915127	541.465234	11.035879
9.429597	540.179076	11.040896
9.793849	529.004795	11.045914
9.608223	540.147547	11.050931
9.631659	538.071337	11.055949
10.148568	532.933219	11.060967
9.826016	531.476284	11.065984
10.011537	528.987338	11.071002
9.493739	541.087987	11.076019
9.900733	540.479600	11.081037
9.954274	558.519677	11.086055
10.008936	569.904576	11.091072
10.064993	559.185406	11.096090
9.898112	573.430538	11.101107
10.234189	565.764982	11.106125
10.029703	563.900654	11.111143
9.963126	569.626411	11.116160
10.103210	565.613434	11.121178
9.779408	568.131010	11.126195
10.158383	566.156516	11.131213
10.082728	561.967012	11.136231
10.112904	568.390020	11.141248
10.047818	570.578002	11.146266
10.260198	573.611334	11.151283
10.150687	565.703918	11.156301
10.077162	566.922903	11.161319
9.951955	564.405683	11.166336
10.480342	570.985235	11.171354
10.091206	567.739696	11.176371
10.196426	567.611945	11.181389
10.265542	566.372563	11.186407
10.151700	573.182474	11.191424
9.970515	563.042260	11.196442
9.995297	567.723973	11.201459
9.986126	568.993084	11.206477
10.186743	557.384204	11.211495
10.079885	567.207289	11.216512
9.897217	560.592647	11.221530
9.707191	568.964905	11.226547
10.171701	565.815455	11.231565
10.372652	571.932148	11.236583
10.149952	567.598395	11.241600
10.488821	578.094591	11.246618
10.337689	579.192628	11.251635
10.279468	569.057756	11.256653
10.654903	574.368145	11.261671
10.130461	569.024191	11.266688
10.590129	565.056120	11.271706
10.369516	562.996259	11.276723
10.425068	563.596788	11.281741
10.668009	561.589201	11.286759
10.314349	574.960921	11.291776
10.407451	560.407730	11.296794
10.455345	567.653516	11.301811
10.472477	566.653072	11.306829
10.580906	567.102304	11.311847
10.713454	563.472244	11.316864
10.567821	563.914297	11.321882
10.310178	568.863408	11.326899
10.368218	568.252788	11.331917
10.473838	563.521579	11.336935
10.109843	565.683854	11.341952
10.487917	564.916505	11.346970
10.503302	563.844310	11.351987
10.408630	571.995027	11.357005
10.634292	569.780287	11.362023
10.541484	576.546747	11.367040
10.268449	564.834514	11.372058
10.258547	567.851252	11.377075
10.311388	585.674171	11.382093
10.567676	596.387633	11.387111
10.889186	601.839662	11.392128
10.862416	582.115417	11.397146
10.726421	575.952032	11.402163
10.452995	566.431431	11.407181
10.641859	562.236345	11.412199
10.487429	559.694850	11.417216
10.773908	570.885720	11.422234
10.734728	567.725902	11.427251
10.533527	571.597603	11.432269
10.683761	561.801682	11.437287
10.471773	583.617136	11.442304
10.834377	589.818179	11.447322
10.942430	596.434342	11.452339
10.647878	589.014525	11.457357
10.739081	572.862347	11.462375
10.529076	575.361600	11.467392
10.490960	584.022963	11.472410
10.919422	596.791315	11.477427
10.603330	603.617928	11.482445
10.350945	593.882609	11.487463
10.680043	606.388764	11.492480
10.841342	603.338126	11.497498
11.035632	603.235922	11.502515
10.859407	604.290497	11.507533
10.927260	603.685921	11.512551
10.637716	597.315585	11.517568
11.084055	600.590331	11.522586
10.806101	600.807940	11.527603
10.527870	600.806320	11.532621
11.023766	601.281302	11.537639
10.949758	608.509970	11.542656
10.820550	595.261518	11.547674
10.811081	606.897244	11.552691
10.605220	605.196907	11.557709
10.941064	599.165506	11.562727
10.959595	611.559911	11.567744
10.903207	607.124297	11.572762
11.039335	608.304699	11.577779
10.765172	600.381131	11.582797
11.008527	591.509409	11.587815
10.631279	607.833089	11.592832
10.914011	596.712660	11.597850
11.023496	597.161520	11.602867
10.686576	601.639799	11.607885
10.994454	603.117810	11.612903
10.612507	603.691459	11.617920
10.747550	611.793781	11.622938
11.183605	622.334085	11.627955
10.971517	635.185314	11.632973
11.181895	626.382042	11.637991
11.167304	623.548416	11.643008
11.262804	628.552818	11.648026
11.395886	614.839327	11.653043
11.080201	626.164966	11.658061
11.514652	625.062874	11.663079
11.011518	610.780181	11.668096
10.853387	604.409652	11.673114
11.152095	616.423659	11.678131
11.318700	616.689023	11.683149
11.518151	618.523419	11.688167
11.063137	606.977612	11.693184
11.277616	611.632336	11.698202
11.023346	609.229270	11.703219
11.102633	614.170028	11.708237
11.239668	622.455082	11.713255
11.058543	617.499095	11.718272
11.251027	629.569347	11.723290
11.406537	620.096506	11.728307
11.059699	627.766172	11.733325
11.461134	618.315050	11.738343
11.195532	626.205054	11.743360
11.322900	620.189399	11.748378
11.404090	614.729413	11.753395
11.301071	624.972536	11.758413
11.680225	616.334313	11.763431
11.243267	616.772628	11.768448
11.665941	623.279819	11.773466
11.509969	615.077760	11.778483
11.145697	619.735577	11.783501
11.293159	620.696789	11.788519
11.255612	622.898900	11.793536
11.242611	613.019654	11.798554
11.420542	609.557027	11.803571
11.159893	617.779447	11.808589
11.882036	608.753142	11.813607
11.728136	623.638833	11.818624
11.575700	625.911021	11.823642
11.701846	615.669693	11.828659
11.371123	619.713317	11.833677
11.309868	615.295044	11.838695
11.567719	609.729128	11.843712
11.205147	621.887497	11.848730
11.199792	618.014813	11.853747
11.354761	624.714522	11.858765
11.731358	617.552798	11.863783
11.388274	614.734799	11.868800
11.472470	618.316771	11.873818
11.553422	620.415137	11.878835
11.001291	626.472782	11.883853
11.399805	607.373044	11.888871
11.370273	617.582100	11.893888
11.631959	629.075733	11.898906
11.835438	636.804318	11.903923
11.518876	641.141635	11.908941
11.628130	650.416291	11.913959
11.770008	649.283895	11.918976
11.563815	653.520594	11.923994
11.977337	656.624244	11.929011
11.717035	644.168155	11.934029
11.566703	648.210935	11.939047
11.866214	641.577724	11.944064
11.799399	651.501287	11.949082
11.825215	643.739830	11.954099
11.541577	660.084814	11.959117
12.032799	643.497400	11.964135
11.955056	639.912313	11.969152
11.555232	626.785776	11.974170
12.048623	640.658056	11.979187
11.592125	631.198354	11.984205
11.979602	639.698466	11.989223
11.740115	644.802446	11.994240
11.767455	650.566360	11.999258
11.991043	640.300356	12.004275
11.590943	649.983665	12.009293
11.773301	643.813005	12.014311
11.864548	650.143421	12.019328
11.908330	648.426978	12.024346
11.988496	647.878814	12.029363
11.796157	645.040281	12.034381
12.047226	648.791951	12.039399
11.935204	645.966445	12.044416
12.211468	651.847242	12.049434
12.300873	642.578274	12.054451
11.989094	653.260022	12.059469
12.316207	639.031813	12.064487
12.310078	643.369892	12.069504
11.663342	631.875813	12.074522
11.917004	634.737151	12.079539
11.670074	637.685236	12.084557
11.985892	640.570100	12.089575
11.879857	642.586171	12.094592
11.873034	645.575643	12.099610
12.143973	655.046050	12.104627
12.106570	646.314263	12.109645
12.186749	649.584529	12.114663
12.202827	651.941303	12.119680
12.041220	650.356628	12.124698
12.224631	644.990658	12.129715
11.717371	647.030310	12.134733
12.075445	648.103357	12.139751
12.388109	651.450329	12.144768
12.140488	653.844437	12.149786
12.393110	657.963148	12.154803
12.277122	651.551149	12.159821
12.240779	650.488726	12.164839
12.467806	649.726992	12.169856
11.918263	648.340252	12.174874
12.144586	654.243129	12.179891
12.165237	648.390860	12.184909
11.946489	649.739493	12.189927
11.913952	640.512447	12.194944
11.998925	656.029678	12.199962
12.691209	662.182647	12.204979
12.664955	671.583375	12.209997
12.636529	666.521879	12.215015
12.320402	649.246855	12.220032
12.632524	652.614979	12.225050
12.505944	648.337467	12.230067
12.349604	648.367354	12.235085
12.094301	639.851893	12.240103
12.200377	648.185411	12.245120
12.153545	646.062011	12.250138
12.271756	655.041501	12.255155
12.325486	671.677840	12.260173
12.458883	668.202131	12.265191
12.847753	675.074978	12.270208
12.670435	672.664426	12.275226
12.706949	665.167107	12.280243
12.525569	653.239390	12.285261
12.575222	639.428531	12.290279
12.473756	642.998260	12.295296
12.255732	642.131181	12.300314
12.476750	647.115908	12.305331
12.535130	672.380004	12.310349
12.515379	660.252004	12.315367
12.691192	671.996147	12.320384
12.655073	670.434311	12.325402
12.748770	668.896170	12.330419
12.474775	670.628765	12.335437
13.291801	666.584148	12.340455
12.909317	658.847636	12.345472
12.731910	642.978203	12.350490
12.628988	639.957892	12.355507
12.475302	649.401439	12.360525
12.768671	642.320659	12.365543
12.764259	635.579907	12.370560
12.602054	642.097317	12.375578
12.979784	647.296728	12.380595
12.733983	636.057244	12.385613
12.882024	632.944437	12.390631
12.704874	633.318901	12.395648
12.834645	638.217027	12.400666
12.722519	641.305097	12.405683
12.679152	651.525135	12.410701
12.609339	658.152974	12.415719
12.883661	654.824110	12.420736
12.504880	663.707876	12.425754
13.210227	667.824368	12.430771
13.162809	671.546920	12.435789
13.029958	672.131527	12.440807
12.599572	650.612400	12.445824
13.183399	666.123297	12.450842
13.087224	660.877014	12.455859
12.739634	646.651105	12.460877
12.840160	664.353205	12.465895
13.294478	655.707388	12.470912
12.726488	660.037291	12.475930
13.170648	657.345308	12.480947
12.895219	662.529476	12.485965
12.854660	659.537966	12.490983
13.138730	657.431411	12.496000
13.091465	663.642739	12.501018
13.400509	669.437588	12.506035
12.969705	651.908805	12.511053
12.792236	646.208946	12.516071
13.012251	656.231875	12.521088
12.784673	666.800038	12.526106
12.911301	663.505955	12.531123
13.051429	668.545469	12.536141
12.823489	671.985055	12.541159
12.817464	661.770980	12.546176
12.864508	671.745311	12.551194
12.742918	667.742535	12.556211
13.047488	668.481194	12.561229
13.116987	683.134942	12.566247
13.434821	688.727564	12.571264
13.085029	695.748979	12.576282
13.242705	687.954758	12.581299
13.682780	697.531716	12.586317
13.142621	693.756760	12.591335
13.340031	673.259361	12.596352
13.186983	673.097573	12.601370
12.843927	674.393056	12.606387
13.034202	687.893939	12.611405
13.255721	702.197657	12.616423
13.470246	691.112905	12.621440
13.382571	695.855865	12.626458
13.771630	692.530362	12.631475
13.687436	694.717994	12.636493
13.729463	697.581057	12.641511
13.308618	684.793178	12.646528
13.296615	678.997305	12.651546
13.581004	684.245508	12.656563
13.690763	667.169738	12.661581
13.371493	666.968259	12.666599
13.468953	660.848512	12.671616
13.057993	665.229280	12.676634
13.612657	683.987731	12.681651
13.352308	683.274328	12.686669
13.176220	697.871082	12.691687
13.206178	688.632832	12.696704
13.092915	697.282144	12.701722
13.059078	693.222653	12.706739
13.435416	690.777945	12.711757
13.420515	695.131669	12.716775
13.619233	688.485272	12.721792
13.376630	695.109566	12.726810
13.534085	708.920429	12.731827
14.149911	710.658861	12.736845
13.554546	714.400455	12.741863
13.457288	695.280263	12.746880
13.395795	701.777219	12.751898
13.920859	711.808139	12.756915
14.157685	710.436744	12.761933
13.721225	703.714626	12.766951
14.000620	694.459912	12.771968
13.952832	693.624374	12.776986
13.751937	690.471331	12.782003
14.089344	691.998181	12.787021
13.829974	691.079116	12.792039
13.980463	690.016344	12.797056
13.790350	682.361619	12.802074
13.872788	687.328056	12.807091
13.919168	687.273860	12.812109
13.937479	691.525416	12.817127
14.381593	687.148510	12.822144
14.190687	693.648667	12.827162
13.935743	696.259338	12.832179
13.989250	693.403161	12.837197
13.916656	698.646141	12.842215
13.891007	693.376315	12.847232
13.663573	689.809995	12.852250
13.750818	696.130663	12.857267
13.767565	688.517138	12.862285
13.835713	688.266423	12.867303
13.981391	697.211453	12.872320
14.031468	696.834026	12.877338
13.504683	697.743147	12.882355
13.852036	690.915953	12.887373
13.735659	693.407339	12.892391
14.060861	692.315331	12.897408
14.044233	687.610701	12.902426
14.111604	689.817233	12.907443
14.194432	692.594385	12.912461
14.056674	689.896171	12.917479
14.101315	686.559022	12.922496
13.894399	690.449220	12.927514
14.198722	707.718114	12.932531
14.394957	708.833025	12.937549
14.144873	706.479047	12.942567
14.393747	701.566909	12.947584
14.198985	693.758237	12.952602
14.066799	694.293722	12.957619
14.349499	686.589146	12.962637
14.170844	691.161019	12.967655
14.087513	694.121093	12.972672
14.368013	706.382275	12.977690
14.564706	715.282028	12.982707
14.523048	702.279938	12.987725
14.081935	696.208358	12.992743
14.257526	685.900305	12.997760
14.394829	696.501339	13.002778
14.412327	704.861813	13.007795
14.430162	690.802080	13.012813
14.390722	692.832677	13.017831
14.397258	698.771906	13.022848
14.341552	702.096854	13.027866
14.381948	714.308979	13.032883
14.737680	710.941770	13.037901
14.330078	721.427104	13.042919
14.601267	712.772523	13.047936
14.596177	707.058556	13.052954
14.407685	708.619867	13.057971
14.390436	696.540042	13.062989
14.508116	714.162187	13.068007
14.469060	726.645976	13.073024
14.588979	717.045338	13.078042
14.794433	717.947708	13.083059
14.801579	713.526305	13.088077
14.509759	703.397300	13.093095
14.324306	690.120912	13.098112
14.753041	703.288887	13.103130
14.757601	710.943098	13.108147
14.540036	704.897346	13.113165
14.198764	717.558318	13.118183
14.561200	713.789626	13.123200
14.633771	716.274019	13.128218
14.282864	730.098731	13.133235
14.946793	711.097656	13.138253
14.718532	722.697201	13.143271
14.615132	718.479591	13.148288
14.873829	717.557680	13.153306
14.671042	718.868629	13.158323
14.795180	727.665496	13.163341
14.502355	722.737685	13.168359
14.540219	721.033044	13.173376
14.726287	718.201480	13.178394
14.515461	728.493690	13.183411
14.684048	723.841133	13.188429
14.675832	734.378787	13.193447
14.902860	745.295432	13.198464
15.325940	752.321870	13.203482
14.851425	745.037001	13.208499
15.155829	714.526737	13.213517
14.644502	725.913508	13.218535
14.777197	738.859082	13.223552
15.081073	749.770043	13.228570
15.091482	754.479003	13.233587
14.991726	745.380776	13.238605
14.888272	747.641494	13.243623
14.903653	744.177707	13.248640
15.192020	746.761072	13.253658
15.099206	751.454119	13.258675
15.547790	741.909658	13.263693
14.901860	742.289013	13.268711
14.772758	741.669140	13.273728
14.941487	741.440681	13.278746
14.919590	752.395555	13.283763
15.289931	750.245910	13.288781
14.827974	748.085005	13.293799
14.702871	753.720761	13.298816
14.902296	751.602674	13.303834
15.202879	745.593611	13.308851
15.442710	742.390925	13.313869
15.406482	747.391081	13.318887
15.248137	749.495185	13.323904
15.275746	742.058361	13.328922
15.119893	748.862931	13.333939
15.383688	744.696874	13.338957
15.422094	755.444889	13.343975
15.260400	750.948002	13.348992
15.182273	745.383750	13.354010
15.106937	751.902121	13.359027
15.676354	744.798837	13.364045
15.651826	744.386371	13.369063
15.318805	753.500165	13.374080
15.613706	744.105255	13.379098
15.207655	748.877528	13.384115
15.295335	734.548092	13.389133
15.631294	748.189370	13.394151
15.545809	748.334638	13.399168
15.791760	741.136308	13.404186
15.449976	750.891281	13.409203
15.622134	746.907766	13.414221
15.706342	748.873925	13.419239
15.476634	745.711093	13.424256
15.719483	738.896327	13.429274
15.069441	755.421791	13.434291
15.440977	740.746764	13.439309
15.805464	745.709054	13.444327
15.375459	745.673018	13.449344
15.431307	748.545407	13.454362
15.323532	746.479561	13.459379
15.643704	758.131079	13.464397
15.792147	767.847099	13.469415
15.806553	764.101598	13.474432
16.042281	747.124873	13.479450
15.872044	750.933995	13.484467
15.406721	750.350320	13.489485
15.500651	753.259685	13.494503
15.643449	762.254244	13.499520
16.043572	764.082075	13.504538
15.700393	770.512304	13.509555
15.476000	762.654785	13.514573
15.787530	777.644946	13.519591
15.753758	775.885280	13.524608
16.262194	775.616893	13.529626
16.311118	775.547707	13.534643
15.966291	761.123214	13.539661
15.782872	752.117623	13.544679
15.893970	767.399340	13.549696
16.064031	769.152818	13.554714
15.573068	765.834206	13.559731
15.728842	764.763858	13.564749
15.650480	771.548472	13.569767
15.910968	773.674299	13.574784
15.925774	770.120450	13.579802
15.706882	778.237792	13.584819
15.714121	776.235104	13.589837
15.761247	771.532253	13.594855
15.814078	781.535809	13.599872
15.978774	770.626005	13.604890
16.198818	784.929455	13.609907
16.316532	787.949433	13.614925
16.332400	779.107935	13.619943
15.967453	771.659182	13.624960
16.166042	763.932920	13.629978
16.001567	781.081599	13.634995
16.040612	789.583214	13.640013
16.386222	789.084031	13.645031
16.542320	797.278811	13.650048
16.656115	783.685889	13.655066
16.542557	772.946733	13.660083
16.394136	770.249490	13.665101
16.207055	761.513777	13.670119
16.095227	767.186699	13.675136
16.034148	744.586044	13.680154
16.434670	758.606339	13.685171
16.480747	759.332064	13.690189
16.597412	749.226665	13.695207
16.385447	757.403470	13.700224
16.389220	752.175188	13.705242
16.184601	763.775362	13.710259
16.352016	757.222322	13.715277
16.490313	762.481252	13.720295
16.582438	775.643823	13.725312
16.584424	766.885737	13.730330
16.541827	762.663127	13.735347
16.462420	750.878612	13.740365
16.509625	761.090951	13.745383
16.371278	783.432994	13.750400
16.827324	781.299808	13.755418
16.596808	773.760210	13.760435
16.227876	773.788033	13.765453
16.349902	773.152007	13.770471
16.880233	782.414036	13.775488
16.935009	779.075969	13.780506
17.269893	785.713957	13.785523
16.880991	767.696611	13.790541
16.960484	764.173348	13.795559
16.404570	758.662915	13.800576
16.612524	750.983525	13.805594
16.470424	750.863418	13.810611
16.509230	750.930945	13.815629
16.910186	755.497832	13.820647
16.447412	773.919628	13.825664
16.791678	774.978052	13.830682
16.783457	793.680597	13.835699
16.535026	793.133308	13.840717
17.018246	785.334139	13.845735
16.711745	784.328420	13.850752
17.259645	777.848343	13.855770
17.261098	785.410594	13.860787
16.863365	782.692192	13.865805
17.174871	779.489790	13.870823
17.013485	772.605197	13.875840
16.985766	751.597311	13.880858
16.834522	769.489794	13.885875
16.795799	782.268632	13.890893
17.382860	773.230632	13.895911
16.808252	786.288294	13.900928
17.058488	787.634772	13.905946
17.347237	793.643856	13.910963
17.251587	787.438052	13.915981
17.105139	769.274507	13.920999
16.838904	768.355792	13.926016
17.056158	774.733422	13.931034
17.191487	785.449602	13.936051
16.948221	788.112675	13.941069
17.542954	789.363315	13.946087
17.098128	780.587758	13.951104
17.200307	769.240735	13.956122
17.172076	779.395944	13.961139
17.033991	776.870987	13.966157
17.235673	773.896669	13.971175
17.044304	786.211148	13.976192
17.171166	772.492843	13.981210
17.231562	780.311419	13.986227
17.236498	779.718082	13.991245
17.402592	773.568380	13.996263
17.202689	780.260214	14.001280
17.155931	773.386881	14.006298
17.335490	778.503141	14.011315
17.123821	784.469812	14.016333
17.312856	768.990890	14.021351
17.546923	778.364359	14.026368
17.238833	766.650516	14.031386
17.332776	779.457299	14.036403
17.302267	789.866027	14.041421
17.902893	791.465666	14.046439
17.733914	798.483057	14.051456
17.606095	787.280541	14.056474
17.574345	766.462271	14.061491
17.305188	773.007748	14.066509
17.922570	787.603799	14.071527
17.679945	784.974570	14.076544
17.379398	769.188068	14.081562
17.621434	778.482659	14.086579
17.499722	793.212188	14.091597
17.712430	791.606423	14.096615
17.982838	787.341624	14.101632
17.956860	789.125720	14.106650
17.705461	775.001414	14.111667
17.431568	781.684288	14.116685
17.881451	785.694661	14.121703
17.921701	794.609046	14.126720
17.867180	788.780634	14.131738
17.854443	801.529580	14.136755
17.788802	796.397460	14.141773
17.739106	793.973157	14.146791
17.361985	796.968302	14.151808
17.754395	791.457314	14.156826
17.692598	798.891903	14.161843
17.854655	796.140690	14.166861
17.986723	789.728936	14.171879
17.868435	799.749530	14.176896
17.642140	791.730904	14.181914
17.811101	791.154001	14.186931
17.921577	796.345524	14.191949
17.812966	789.944642	14.196967
17.745036	791.637292	14.201984
18.037137	797.688337	14.207002
18.519446	810.145967	14.212019
18.048550	808.240460	14.217037
18.102437	802.412134	14.222055
17.848679	801.937773	14.227072
18.192109	808.744418	14.232090
18.616096	802.413660	14.237107
18.422577	799.750283	14.242125
18.269561	791.377373	14.247143
18.092672	791.187068	14.252160
18.227486	796.928055	14.257178
18.080009	785.280410	14.262195
17.941303	796.009470	14.267213
18.305259	801.146660	14.272231
18.513296	813.814830	14.277248
18.262680	817.694805	14.282266
18.550007	819.144957	14.287283
18.403998	808.632023	14.292301
18.308215	793.670467	14.297319
18.215258	801.615323	14.302336
17.976064	817.939111	14.307354
18.434679	809.040148	14.312371
18.355578	820.782091	14.317389
18.217812	816.812278	14.322407
18.549236	820.540005	14.327424
18.455639	820.339005	14.332442
18.436833	820.052350	14.337459
18.214799	820.450222	14.342477
18.275697	819.033456	14.347495
18.546863	824.176628	14.352512
18.078481	824.858738	14.357530
18.473822	826.744455	14.362547
18.630943	835.152853	14.367565
19.024701	836.240061	14.372583
18.972450	825.692242	14.377600
19.095484	817.615148	14.382618
19.161369	808.160631	14.387635
18.992413	814.023370	14.392653
18.899657	809.667753	14.397671
18.975564	811.738837	14.402688
18.842789	811.721897	14.407706
18.904267	809.745620	14.412723
18.588259	810.824426	14.417741
18.670363	810.703665	14.422759
18.795742	807.868393	14.427776
18.896153	809.118523	14.432794
19.119099	802.238537	14.437811
18.786549	811.585738	14.442829
19.033900	805.793362	14.447847
18.946525	810.080035	14.452864
18.769687	815.088623	14.457882
19.141019	804.572771	14.462899
18.891615	810.294165	14.467917
18.904135	810.045214	14.472935
18.623831	813.965160	14.477952
18.508074	807.994959	14.482970
18.571511	808.328062	14.487987
18.756126	820.979659	14.493005
18.963966	834.588375	14.498023
19.123355	837.641591	14.503040
19.197239	837.660377	14.508058
19.153429	833.834383	14.513075
19.360249	836.193929	14.518093
19.377882	838.914428	14.523111
19.499752	832.760242	14.528128
19.055513	842.441755	14.533146
19.680789	836.450340	14.538163
19.352510	831.168172	14.543181
19.355153	829.730774	14.548199
19.850155	832.399881	14.553216
19.497270	817.378677	14.558234
19.197110	803.401024	14.563251
19.210749	808.334253	14.568269
19.200561	800.747786	14.573287
19.522324	809.039834	14.578304
19.407676	826.020054	14.583322
19.596938	831.472494	14.588339
19.685422	812.408089	14.593357
19.479143	795.650044	14.598375
19.676203	798.723761	14.603392
19.221381	798.368246	14.608410
19.278862	801.329738	14.613427
19.287406	810.782834	14.618445
19.799169	828.680142	14.623463
19.900063	824.561217	14.628480
19.644078	832.893795	14.633498
19.727693	824.727191	14.638515
19.697249	831.357026	14.643533
19.446482	815.952337	14.648551
19.843368	823.018592	14.653568
19.276282	830.103347	14.658586
19.495228	820.008065	14.663603
19.807016	832.380282	14.668621
19.373683	820.575803	14.673639
19.418526	823.812613	14.678656
19.622028	828.482022	14.683674
19.798065	822.944785	14.688691
19.663556	829.712380	14.693709
19.495976	827.570641	14.698727
19.827724	822.653943	14.703744
19.918244	851.365936	14.708762
20.103213	846.370089	14.713779
19.752113	838.559967	14.718797
19.646248	857.585100	14.723815
20.250764	848.024893	14.728832
20.045975	849.480469	14.733850
20.348721	850.124171	14.738867
20.146839	843.815535	14.743885
20.188300	835.542553	14.748903
19.914893	823.730781	14.753920
19.960676	836.259806	14.758938
20.187944	849.381869	14.763955
20.358320	847.465436	14.768973
20.100535	836.453374	14.773991
20.291962	828.391676	14.779008
20.082440	836.218138	14.784026
20.396729	828.648588	14.789043
20.090939	843.669769	14.794061
20.314482	843.564474	14.799079
20.774691	832.259466	14.804096
20.333125	824.609654	14.809114
20.409575	819.462177	14.814131
20.471711	816.329166	14.819149
20.063388	821.488429	14.824167
20.275822	811.824524	14.829184
19.822126	819.197890	14.834202
20.456520	837.140963	14.839219
20.301177	841.086993	14.844237
20.351779	851.912178	14.849255
20.726740	843.419597	14.854272
20.198827	854.483450	14.859290
20.562226	850.234278	14.864307
21.062831	846.978781	14.869325
20.720786	844.637703	14.874343
20.578142	842.938249	14.879360
20.373093	839.987822	14.884378
20.732096	841.600856	14.889395
20.476564	843.168796	14.894413
20.617751	855.889055	14.899431
20.736160	850.181869	14.904448
20.398089	849.178636	14.909466
20.569700	850.349223	14.914483
20.267053	848.452359	14.919501
20.250097	853.040314	14.924519
20.828198	842.242446	14.929536
20.456777	851.304022	14.934554
20.593224	838.099391	14.939571
20.506183	851.313064	14.944589
20.775167	856.730216	14.949607
21.361456	864.557092	14.954624
20.904616	863.253932	14.959642
21.282953	857.486219	14.964659
20.720994	844.481123	14.969677
20.872388	852.932212	14.974695
20.985012	847.834221	14.979712
20.797003	856.011821	14.984730
20.989003	865.314387	14.989747
21.190445	863.512074	14.994765
21.105043	868.484617	14.999783
21.392742	866.818352	15.004800
20.997683	858.273835	15.009818
20.996023	851.681932	15.014835
21.210872	854.514922	15.019853
21.148740	859.736337	15.024871
21.308077	860.472375	15.029888
20.969520	873.477885	15.034906
21.235851	875.077981	15.039923
21.065365	873.819347	15.044941
20.927639	879.701328	15.049959
21.445612	865.965175	15.054976
21.433699	876.506297	15.059994
21.434917	875.149442	15.065011
21.463555	875.749733	15.070029
21.644416	877.141607	15.075047
21.799747	859.477373	15.080064
21.584149	853.476114	15.085082
21.055258	848.263107	15.090099
21.198460	840.657818	15.095117
21.406152	866.331642	15.100135
21.464064	864.481535	15.105152
21.480459	872.115750	15.110170
21.532467	870.574480	15.115187
21.744553	868.159013	15.120205
21.380507	877.079623	15.125223
21.946731	868.608385	15.130240
21.540755	874.364880	15.135258
20.945822	883.968714	15.140275
21.472258	869.566622	15.145293
21.358904	878.665632	15.150311
21.796249	875.778497	15.155328
21.579189	873.910315	15.160346
21.578588	884.106273	15.165363
21.740446	875.904198	15.170381
21.246430	879.586467	15.175399
21.590322	874.029581	15.180416
21.638567	894.503866	15.185434
21.922109	893.859493	15.190451
22.462905	902.646260	15.195469
22.103253	886.035255	15.200487
22.122908	872.256732	15.205504
21.646934	866.994375	15.210522
21.713402	874.412012	15.215539
22.117663	866.153512	15.220557
21.930490	865.545647	15.225575
21.892203	867.425493	15.230592
21.841803	875.983359	15.235610
21.883629	884.112144	15.240627
22.229373	896.702773	15.245645
21.929506	900.824800	15.250663
22.228246	895.067941	15.255680
21.935325	897.144042	15.260698
22.248760	893.271647	15.265715
22.444437	891.408481	15.270733
22.111233	901.259360	15.275751
22.382296	899.530506	15.280768
22.553017	890.377395	15.285786
22.205065	895.381774	15.290803
22.563694	887.811913	15.295821
22.124967	894.086822	15.300839
22.315689	894.132249	15.305856
22.184978	895.301910	15.310874
22.297007	897.504395	15.315891
22.647252	889.042274	15.320909
22.429896	895.778395	15.325927
22.517886	892.819408	15.330944
22.521208	895.311993	15.335962
22.330599	894.950747	15.340979
22.624870	894.686854	15.345997
22.660231	904.454431	15.351015
22.383543	896.327203	15.356032
22.490945	894.503904	15.361050
22.365906	898.916147	15.366067
22.671264	898.485853	15.371085
22.614942	897.143678	15.376103
22.840699	888.090864	15.381120
22.351415	889.397676	15.386138
22.239350	888.225782	15.391155
22.695242	891.306102	15.396173
22.376988	902.495368	15.401191
22.254252	903.096805	15.406208
22.514061	918.422061	15.411226
22.633495	918.680508	15.416243
23.399976	906.844646	15.421261
23.384690	904.743722	15.426279
23.503607	906.907271	15.431296
23.184512	876.504058	15.436314
22.995763	882.279566	15.441331
23.287050	868.944454	15.446349
23.061917	877.227048	15.451367
23.433449	879.698981	15.456384
23.124601	874.554111	15.461402
23.148505	875.131174	15.466419
23.245020	871.411761	15.471437
23.193030	874.859546	15.476455
23.259707	878.283279	15.481472
23.133037	875.729638	15.486490
22.934701	883.875506	15.491507
23.191012	873.153541	15.496525
22.849448	879.993759	15.501543
22.890166	882.923803	15.506560
23.130377	870.204626	15.511578
22.860142	875.171280	15.516595
23.051664	880.404476	15.521613
22.800801	889.446430	15.526631
23.274134	899.212859	15.531648
23.344446	896.648521	15.536666
23.065186	912.570428	15.541683
23.430777	905.808806	15.546701
23.345471	903.917541	15.551719
23.266591	900.926055	15.556736
23.471873	898.426680	15.561754
23.260807	902.988648	15.566771
23.434372	905.681667	15.571789
23.479457	911.111644	15.576807
23.646442	903.621263	15.581824
23.676585	895.385167	15.586842
23.604537	909.871920	15.591859
23.790824	899.527303	15.596877
23.700984	909.143654	15.601895
23.550258	909.928080	15.606912
23.518500	908.633394	15.611930
23.419433	904.879948	15.616947
23.586528	915.137420	15.621965
23.904314	904.677249	15.626983
23.618880	912.518728	15.632000
23.849467	916.941943	15.637018
23.974431	935.214671	15.642035
24.425727	924.793316	15.647053
24.011402	912.001800	15.652071
24.086140	910.249673	15.657088
24.248417	912.613485	15.662106
24.291142	905.305164	15.667123
24.053002	897.307348	15.672141
23.826698	904.164245	15.677159
24.144137	900.789188	15.682176
23.894992	899.548349	15.687194
24.159765	901.917170	15.692211
24.233642	890.913720	15.697229
23.973573	899.347401	15.702247
23.720328	900.321297	15.707264
23.861210	895.595346	15.712282
23.863990	912.504178	15.717299
24.283717	920.965033	15.722317
24.401265	935.599816	15.727335
24.246409	931.765877	15.732352
24.665560	929.747066	15.737370
24.303645	922.793378	15.742387
24.504005	922.954914	15.747405
24.437093	907.587288	15.752423
24.414138	904.469583	15.757440
24.387282	898.466462	15.762458
24.359595	908.596864	15.767475
24.356270	915.721807	15.772493
24.641349	929.069356	15.777511
24.321039	929.133583	15.782528
24.872781	941.980547	15.787546
24.516294	928.722341	15.792563
24.560255	928.818145	15.797581
24.587745	931.319317	15.802599
24.618092	934.608556	15.807616
24.648009	935.670817	15.812634
24.714322	934.209049	15.817651
24.644725	932.987182	15.822669
24.982533	929.939818	15.827687
24.854985	942.629227	15.832704
24.898647	927.664048	15.837722
24.491959	920.412700	15.842739
24.633150	928.334058	15.847757
24.602862	932.488449	15.852775
24.387768	944.910929	15.857792
24.907388	933.654632	15.862810
24.357302	936.069135	15.867827
24.489930	928.655708	15.872845
24.669287	932.809898	15.877863
24.351621	938.304507	15.882880
24.991525	948.244453	15.887898
25.184461	950.539398	15.892915
25.237620	955.892463	15.897933
25.368820	943.606678	15.902951
25.464035	952.734448	15.907968
25.343162	923.160358	15.912986
25.082050	928.053862	15.918003
25.252460	917.135525	15.923021
25.161459	919.552458	15.928039
24.954481	915.838991	15.933056
25.167425	920.127352	15.938074
25.069127	930.721055	15.943091
25.120321	943.210293	15.948109
25.056712	950.348027	15.953127
25.135568	949.875067	15.958144
25.612990	948.176867	15.963162
25.520333	942.387411	15.968179
25.467932	947.737152	15.973197
25.450868	946.889604	15.978215
25.310901	939.688006	15.983232
25.923808	941.916692	15.988250
25.547861	942.784613	15.993267
25.291729	935.333834	15.998285
25.754297	942.067591	16.003303
25.410537	941.831794	16.008320
25.363110	934.687255	16.013338
25.894893	937.954567	16.018355
25.888267	939.204782	16.023373
25.879644	930.686937	16.028391
25.773912	940.868912	16.033408
25.887109	926.750399	16.038426
25.464793	934.217023	16.043443
25.705200	940.399152	16.048461
25.929334	940.690195	16.053479
25.528210	941.159172	16.058496
25.685357	931.623667	16.063514
25.771431	949.484393	16.068531
25.825732	941.112375	16.073549
25.888796	945.052444	16.078567
25.799794	964.753612	16.083584
26.340537	962.764191	16.088602
26.349881	969.887447	16.093619
26.325138	955.563106	16.098637
26.237789	937.571421	16.103655
26.003205	933.298394	16.108672
26.136957	931.861242	16.113690
26.166076	933.972794	16.118707
25.843097	935.197246	16.123725
26.096957	947.068188	16.128743
26.328944	956.253145	16.133760
26.645956	958.329842	16.138778
26.268374	951.596450	16.143795
26.284678	940.817483	16.148813
26.482642	943.172219	16.153831
26.222633	935.996873	16.158848
26.407015	947.415607	16.163866
26.587905	958.686906	16.168883
26.420413	956.401046	16.173901
26.476418	948.007088	16.178919
26.610409	959.482629	16.183936
26.416582	945.916285	16.188954
26.533444	946.079495	16.193971
26.417466	965.067467	16.198989
26.734767	956.789516	16.204007
26.523686	967.605917	16.209024
26.547246	956.709203	16.214042
26.675638	957.635814	16.219059
26.533256	959.689264	16.224077
26.739892	965.380978	16.229095
26.545891	966.793040	16.234112
26.797847	962.676923	16.239130
26.599816	958.358839	16.244147
26.737618	963.101805	16.249165
26.578755	957.498141	16.254183
26.854137	960.912793	16.259200
26.786262	961.397639	16.264218
26.751962	958.675489	16.269235
26.425721	967.559159	16.274253
26.844351	964.897549	16.279271
26.775563	986.598435	16.284288
27.140701	976.057121	16.289306
27.493564	984.275988	16.294323
27.283247	981.139017	16.299341
27.376092	973.066465	16.304359
27.340746	960.731973	16.309376
27.209929	960.297405	16.314394
27.153501	958.792258	16.319411
27.099707	955.696203	16.324429
27.147050	953.709266	16.329447
27.287302	973.293212	16.334464
27.640960	981.587138	16.339482
27.335366	966.702409	16.344499
27.066299	965.250713	16.349517
27.198894	967.807647	16.354535
27.230899	978.342326	16.359552
27.467245	975.167730	16.364570
27.538033	980.841479	16.369587
27.547688	982.855490	16.374605
27.469483	981.237825	16.379623
27.452980	985.937943	16.384640
27.473785	976.016430	16.389658
27.610110	976.919677	16.394675
27.646112	981.878377	16.399693
27.782843	976.568868	16.404711
27.690085	986.124731	16.409728
27.658794	986.359808	16.414746
27.516084	983.151366	16.419763
27.223873	981.578718	16.424781
27.617090	975.358512	16.429799
27.647903	990.260112	16.434816
27.707054	1002.689811	16.439834
28.144757	997.364915	16.444851
27.921669	1002.380463	16.449869
28.444333	988.765859	16.454887
28.045389	979.686118	16.459904
27.967145	966.930819	16.464922
28.181448	966.286535	16.469939
28.088886	963.068582	16.474957
28.257065	958.095173	16.479975
28.201340	966.241003	16.484992
27.772617	971.891476	16.490010
28.180428	971.072517	16.495027
28.018390	979.234843	16.500045
28.273147	970.718079	16.505063
28.361014	980.425799	16.510080
28.558067	985.923847	16.515098
28.282038	966.868658	16.520115
28.061412	977.909869	16.525133
28.262256	959.110847	16.530151
28.708575	980.719419	16.535168
28.291275	975.777570	16.540186
28.549630	971.087186	16.545203
28.364930	970.400563	16.550221
28.259984	976.990089	16.555239
27.988897	979.076350	16.560256
28.617739	991.883379	16.565274
28.705583	994.908362	16.570291
28.497435	1002.877586	16.575309
28.959712	995.030615	16.580327
29.094422	990.865083	16.585344
28.740390	992.746245	16.590362
28.659159	985.317157	16.595379
28.408760	987.085822	16.600397
28.429151	983.069207	16.605415
28.572703	989.978050	16.610432
28.989334	998.830783	16.615450
28.591506	986.776585	16.620467
28.461307	992.762077	16.625485
28.906473	994.047044	16.630503
28.680055	990.989514	16.635520
28.765777	998.030407	16.640538
28.795351	988.736926	16.645555
28.856968	998.071873	16.650573
29.257798	1005.433213	16.655591
29.351247	1012.762184	16.660608
28.929164	1000.191165	16.665626
29.329213	996.421274	16.670643
29.047035	998.834955	16.675661
29.418990	992.687564	16.680679
29.182375	991.804460	16.685696
28.925996	997.035372	16.690714
29.323442	1001.527725	16.695731
29.297850	1021.598723	16.700749
29.516392	1017.252723	16.705767
29.499781	1011.720274	16.710784
29.324293	1009.069611	16.715802
29.821760	1010.606504	16.720819
29.214370	1017.609463	16.725837
29.658680	1008.676546	16.730855
29.362744	1021.379834	16.735872
29.162585	1009.725421	16.740890
29.603014	1003.954422	16.745907
29.533021	1014.045863	16.750925
29.779189	1014.226558	16.755943
29.724820	1019.358945	16.760960
29.594073	1023.452501	16.765978
29.842108	1006.730521	16.770995
29.687996	1019.835807	16.776013
29.836424	1013.760596	16.781031
29.534454	1014.811098	16.786048
29.546138	1020.309655	16.791066
29.876151	1017.571036	16.796083
29.737998	1025.370377	16.801101
29.770294	1007.635089	16.806119
29.776910	1015.851682	16.811136
29.511882	1014.513084	16.816154
29.885176	1016.574530	16.821171
29.923912	1039.945337	16.826189
29.809862	1041.293726	16.831207
30.129309	1038.730475	16.836224
29.761148	1043.462682	16.841242
30.061569	1042.216706	16.846259
29.917204	1039.913212	16.851277
30.027091	1047.609136	16.856295
30.194877	1043.073148	16.861312
30.220960	1044.668707	16.866330
30.532268	1028.686942	16.871347
30.360772	1048.137766	16.876365
30.655026	1039.762425	16.881383
30.705970	1043.516354	16.886400
30.307361	1035.518366	16.891418
30.743142	1032.315729	16.896435
30.541637	1039.972858	16.901453
30.426295	1034.641842	16.906471
30.283456	1041.062504	16.911488
29.951508	1041.308578	16.916506
30.551687	1028.618415	16.921523
30.197257	1041.815278	16.926541
30.368489	1049.971459	16.931559
30.666522	1060.502922	16.936576
30.815489	1069.766703	16.941594
30.811812	1065.430066	16.946611
30.550423	1067.051754	16.951629
30.734656	1067.346676	16.956647
31.000305	1061.847214	16.961664
31.068389	1068.101340	16.966682
30.955835	1069.101467	16.971699
31.227047	1068.929196	16.976717
31.326869	1065.324931	16.981735
31.327856	1055.679483	16.986752
31.059772	1049.370743	16.991770
31.142844	1030.356573	16.996787
31.249658	1033.271724	17.001805
31.187331	1029.827875	17.006823
31.042070	1025.041967	17.011840
31.083694	1031.080408	17.016858
31.180051	1025.368162	17.021875
31.184945	1035.875892	17.026893
31.235743	1051.367117	17.031911
31.460220	1050.028256	17.036928
31.244701	1055.884652	17.041946
31.645829	1055.127428	17.046963
31.316227	1048.456881	17.051981
31.505450	1049.828878	17.056999
31.740936	1035.970638	17.062016
31.509496	1039.397500	17.067034
31.711283	1023.654011	17.072051
31.268803	1030.301628	17.077069
31.482092	1037.277244	17.082087
31.836065	1029.753362	17.087104
31.686646	1051.418924	17.092122
31.792688	1049.107666	17.097139
32.112268	1042.189467	17.102157
31.493053	1032.068007	17.107175
31.709327	1024.444971	17.112192
31.742530	1048.522191	17.117210
31.937858	1046.884646	17.122227
31.692009	1050.869392	17.127245
31.794219	1043.807014	17.132263
31.690287	1044.858853	17.137280
31.484207	1056.246900	17.142298
31.837037	1048.374001	17.147315
31.488388	1041.771187	17.152333
31.477902	1047.270682	17.157351
31.724630	1055.724935	17.162368
31.824695	1075.104281	17.167386
32.780757	1061.756936	17.172403
33.055412	1058.290930	17.177421
32.588008	1050.073669	17.182439
32.816706	1034.663871	17.187456
32.543668	1036.177261	17.192474
32.622857	1022.248951	17.197491
32.480264	1032.292631	17.202509
32.669676	1030.822598	17.207527
32.886036	1023.231437	17.212544
32.584103	1015.581548	17.217562
32.305471	999.658494	17.222579
32.359213	1001.733287	17.227597
32.435856	1016.934369	17.232615
32.671617	1014.176773	17.237632
32.819930	1023.793769	17.242650
32.860410	1012.533590	17.247667
32.135440	998.374407	17.252685
32.145321	1004.204344	17.257703
32.745897	1017.475914	17.262720
32.588108	1025.271826	17.267738
32.705136	1014.632752	17.272755
32.866940	1021.563771	17.277773
32.528658	1021.323124	17.282791
32.580147	1018.652844	17.287808
32.695526	1037.543007	17.292826
32.678448	1031.437820	17.297843
32.539633	1024.561566	17.302861
32.832466	1041.536106	17.307879
33.319830	1049.280706	17.312896
33.195838	1063.609708	17.317914
33.426401	1053.374161	17.322931
33.126230	1047.530970	17.327949
32.641862	1038.784668	17.332967
33.138315	1052.110580	17.337984
33.080691	1056.253406	17.343002
33.243066	1058.321962	17.348019
33.016556	1058.754833	17.353037
33.074112	1061.447871	17.358055
33.618368	1059.128342	17.363072
33.082558	1058.265042	17.368090
33.236100	1058.841037	17.373107
33.333023	1050.352824	17.378125
33.071420	1059.170688	17.383143
33.130521	1057.604599	17.388160
33.056981	1076.106542	17.393178
33.323739	1074.689001	17.398195
33.531212	1079.446013	17.403213
33.374449	1083.286833	17.408231
33.673989	1075.227511	17.413248
33.659942	1074.446380	17.418266
33.310150	1068.289001	17.423283
33.867909	1079.580818	17.428301
33.518022	1086.683916	17.433319
33.962920	1092.873063	17.438336
33.842325	1095.497689	17.443354
33.849842	1101.870553	17.448371
34.515182	1099.238780	17.453389
33.938824	1099.825070	17.458407
34.412795	1090.277753	17.463424
34.042782	1081.006537	17.468442
34.224505	1066.557230	17.473459
34.207195	1058.722618	17.478477
33.941979	1066.614748	17.483495
34.131461	1073.678586	17.488512
34.120145	1090.993089	17.493530
34.330996	1089.351385	17.498547
34.303019	1093.201116	17.503565
34.079820	1095.334155	17.508583
34.451649	1086.834877	17.513600
34.419047	1096.411911	17.518618
34.250575	1094.000608	17.523635
34.537124	1094.749766	17.528653
34.131160	1097.403318	17.533671
34.475327	1094.347781	17.538688
34.283706	1087.021239	17.543706
34.461010	1096.382291	17.548723
34.675536	1089.174065	17.553741
34.364247	1096.654200	17.558759
34.762212	1085.184560	17.563776
34.562119	1093.254061	17.568794
34.596442	1096.601334	17.573811
34.404998	1101.482919	17.578829
34.582891	1124.667741	17.583847
34.787284	1115.217180	17.588864
34.740406	1126.431974	17.593882
34.528431	1124.832589	17.598899
35.064042	1122.343235	17.603917
34.908343	1121.371087	17.608935
35.287134	1114.482384	17.613952
35.574779	1126.529338	17.618970
35.253212	1124.307642	17.623987
35.641489	1114.404096	17.629005
35.531862	1115.442713	17.634023
35.520167	1118.615363	17.639040
35.396003	1108.891474	17.644058
35.074377	1099.401583	17.649075
35.564677	1099.027945	17.654093
35.317490	1104.553022	17.659111
35.386265	1099.366966	17.664128
35.496954	1121.207102	17.669146
35.130208	1107.623293	17.674163
35.542566	1109.377485	17.679181
35.700112	1120.524834	17.684199
35.362979	1115.015307	17.689216
35.681751	1111.412040	17.694234
35.567174	1118.192196	17.699251
35.774994	1112.508634	17.704269
35.150972	1122.606405	17.709287
35.530917	1107.411938	17.714304
35.113321	1118.569054	17.719322
35.088455	1120.423867	17.724339
35.605998	1126.918658	17.729357
35.511489	1143.279761	17.734375
35.769417	1132.853794	17.739392
35.687541	1142.552034	17.744410
35.558967	1143.666241	17.749427
36.117311	1144.806825	17.754445
35.953092	1152.742841	17.759463
36.254609	1142.335212	17.764480
36.164732	1142.561525	17.769498
36.225226	1145.924143	17.774515
36.135313	1138.686574	17.779533
35.973771	1138.888185	17.784551
36.372293	1154.571317	17.789568
36.464191	1156.259882	17.794586
36.427096	1167.845900	17.799603
36.613471	1149.229361	17.804621
36.192783	1147.313101	17.809639
36.682686	1154.743171	17.814656
36.493772	1160.906590	17.819674
36.695677	1161.467859	17.824691
36.674892	1139.544547	17.829709
36.373051	1140.383232	17.834727
36.543805	1156.312482	17.839744
36.503174	1168.136480	17.844762
36.683134	1161.959912	17.849779
37.195996	1163.237974	17.854797
36.637699	1163.477969	17.859815
36.988456	1162.920838	17.864832
37.079507	1158.534179	17.869850
37.243068	1165.049238	17.874867
37.099258	1140.942122	17.879885
36.895344	1143.920355	17.884903
36.730210	1131.647846	17.889920
36.949558	1133.932525	17.894938
36.690182	1152.324506	17.899955
37.537920	1148.309705	17.904973
37.193923	1155.433508	17.909991
37.258359	1149.785181	17.915008
37.186723	1155.643290	17.920026
37.139645	1164.119664	17.925043
37.364373	1158.414379	17.930061
37.555787	1152.799669	17.935079
37.278956	1153.649158	17.940096
37.301499	1154.531170	17.945114
36.972996	1147.298214	17.950131
37.132738	1153.840674	17.955149
37.183462	1154.892799	17.960167
37.271535	1150.378690	17.965184
37.785699	1151.285682	17.970202
37.249336	1155.399052	17.975219
37.350286	1151.049725	17.980237
37.499112	1163.576456	17.985255
37.440935	1173.513287	17.990272
37.479144	1183.450640	17.995290
37.398894	1181.725029	18.000307
37.783257	1180.957201	18.005325
37.786655	1188.773647	18.010343
37.681892	1193.318819	18.015360
37.818676	1187.779709	18.020378
38.023090	1191.900279	18.025395
37.930491	1181.374276	18.030413
37.939544	1186.060365	18.035431
38.029693	1189.279486	18.040448
38.203066	1200.282929	18.045466
38.163618	1208.556491	18.050483
38.541140	1207.279580	18.055501
38.286161	1202.370125	18.060519
37.924095	1195.441926	18.065536
38.627302	1198.002089	18.070554
38.412143	1205.858019	18.075571
38.545818	1202.791777	18.080589
38.502753	1212.866274	18.085607
38.782719	1206.326228	18.090624
38.720294	1185.110143	18.095642
38.151723	1179.794957	18.100659
38.467813	1188.740493	18.105677
38.579085	1191.947442	18.110695
38.581074	1202.218769	18.115712
38.507009	1197.039491	18.120730
38.474046	1209.561435	18.125747
38.821841	1205.821438	18.130765
38.646775	1202.836037	18.135783
38.899024	1205.981371	18.140800
38.532507	1203.555330	18.145818
38.453422	1209.341865	18.150835
38.635606	1222.352059	18.155853
38.930605	1228.064617	18.160871
38.901749	1235.804955	18.165888
39.040129	1226.409785	18.170906
38.915461	1237.599794	18.175923
39.357491	1234.719296	18.180941
39.198396	1228.808495	18.185959
38.914729	1236.654174	18.190976
39.400223	1227.262334	18.195994
39.165515	1235.945910	18.201011
39.465913	1230.921307	18.206029
39.560019	1232.464636	18.211047
39.508833	1235.648204	18.216064
39.449855	1227.283441	18.221082
39.109488	1245.537816	18.226099
39.377276	1232.017722	18.231117
39.641868	1231.018231	18.236135
39.410261	1234.682558	18.241152
39.451395	1227.711346	18.246170
39.321141	1247.204383	18.251187
39.861754	1255.553210	18.256205
39.902314	1266.087845	18.261223
39.754814	1270.120079	18.266240
40.239546	1256.929644	18.271258
39.671973	1257.932181	18.276275
39.821929	1256.272629	18.281293
40.185830	1251.645719	18.286311
40.265037	1257.848470	18.291328
39.909092	1246.918961	18.296346
40.008286	1258.668609	18.301363
39.942864	1261.027802	18.306381
40.231664	1249.743108	18.311399
40.046165	1253.927318	18.316416
40.363678	1251.444273	18.321434
40.116869	1251.907687	18.326451
40.163646	1239.906162	18.331469
40.313027	1256.073312	18.336487
40.193056	1250.066239	18.341504
40.432086	1245.731731	18.346522
40.456016	1252.351134	18.351539
40.231300	1253.569907	18.356557
40.668034	1262.237963	18.361575
40.671689	1284.220524	18.366592
40.807452	1271.115635	18.371610
40.989727	1279.833472	18.376627
40.922922	1267.171690	18.381645
40.936079	1267.241120	18.386663
40.942758	1252.011309	18.391680
41.059754	1244.786544	18.396698
40.614794	1247.637935	18.401715
40.745085	1262.658694	18.406733
41.079041	1263.576748	18.411751
40.882035	1279.114505	18.416768
40.995118	1275.580032	18.421786
41.165948	1272.207216	18.426803
41.081869	1277.080461	18.431821
40.917065	1275.498810	18.436839
40.807627	1286.964267	18.441856
40.963497	1264.348445	18.446874
40.983566	1271.059440	18.451891
41.003119	1277.432345	18.456909
41.401612	1288.059469	18.461927
41.358668	1301.788230	18.466944
41.701683	1302.098498	18.471962
41.474704	1309.304494	18.476979
41.724928	1306.245239	18.481997
42.059420	1302.836161	18.487015
41.965251	1296.443297	18.492032
41.877587	1277.476491	18.497050
41.691685	1275.388913	18.502067
41.506949	1277.293936	18.507085
41.779811	1279.605175	18.512103
41.545763	1307.917251	18.517120
41.877610	1295.718702	18.522138
41.879689	1308.731739	18.527155
42.155278	1288.837247	18.532173
42.045473	1295.737943	18.537191
42.001845	1297.706916	18.542208
41.963647	1283.930554	18.547226
42.242605	1296.360964	18.552243
42.203351	1291.701051	18.557261
42.511457	1289.721518	18.562279
42.725427	1284.969916	18.567296
42.496063	1291.628678	18.572314
42.471053	1293.860690	18.577331
42.215430	1284.159326	18.582349
42.473381	1279.952762	18.587367
42.060163	1293.728490	18.592384
42.480846	1288.493725	18.597402
42.207299	1302.110423	18.602419
42.556093	1287.909513	18.607437
42.682629	1288.467565	18.612455
42.625355	1285.997201	18.617472
42.581981	1288.700754	18.622490
42.469661	1291.734262	18.627507
42.418863	1287.930182	18.632525
42.499283	1289.578545	18.637543
42.600325	1299.970477	18.642560
43.060106	1312.917288	18.647578
43.267670	1318.512919	18.652595
43.011747	1326.861105	18.657613
43.478989	1315.869926	18.662631
43.177839	1316.121512	18.667648
43.101441	1302.637302	18.672666
43.124104	1304.299203	18.677683
43.179086	1313.776778	18.682701
43.562071	1313.997729	18.687719
43.275470	1317.959396	18.692736
43.504498	1315.988278	18.697754
43.374688	1310.170214	18.702771
43.216364	1316.521912	18.707789
43.578472	1307.744609	18.712807
43.499819	1312.874043	18.717824
43.561049	1319.924272	18.722842
43.584796	1311.465401	18.727859
43.594311	1317.530944	18.732877
43.592116	1306.468978	18.737895
43.333552	1317.538388	18.742912
43.570073	1305.653698	18.747930
43.520770	1314.780112	18.752947
43.476759	1311.568976	18.757965
44.024061	1320.360417	18.762983
44.186135	1333.138227	18.768000
44.037191	1329.116596	18.773018
44.373598	1327.450457	18.778035
44.227149	1327.807037	18.783053
44.524503	1311.731633	18.788071
44.023320	1313.055808	18.793088
44.262657	1306.024061	18.798106
44.265128	1294.609763	18.803123
44.292659	1304.251732	18.808141
44.866201	1301.762741	18.813159
44.578760	1302.995880	18.818176
44.135519	1299.708583	18.823194
44.244655	1312.875479	18.828211
43.994666	1323.426947	18.833229
44.412466	1323.207478	18.838247
44.044912	1339.610233	18.843264
43.993037	1328.799415	18.848282
44.809876	1324.146811	18.853299
44.311272	1340.758744	18.858317
44.583655	1347.162095	18.863335
44.741693	1366.694767	18.868352
44.659934	1361.651356	18.873370
45.148591	1358.530022	18.878387
44.823735	1362.224049	18.883405
45.083356	1356.932961	18.888423
45.209556	1361.040986	18.893440
44.854792	1366.380496	18.898458
45.109491	1365.346816	18.903475
44.883175	1368.342593	18.908493
45.143305	1353.321340	18.913511
45.235200	1356.939802	18.918528
44.948453	1352.321398	18.923546
45.295358	1359.226136	18.928563
44.937289	1378.690274	18.933581
45.325207	1376.401803	18.938599
45.372458	1381.758753	18.943616
45.631548	1386.710820	18.948634
45.666295	1383.499571	18.953651
45.726065	1384.766346	18.958669
45.931192	1386.541234	18.963687
45.866600	1380.600495	18.968704
45.772158	1385.815646	18.973722
46.057831	1374.165642	18.978739
46.132452	1375.964975	18.983757
45.843196	1378.664135	18.988775
46.025052	1381.626328	18.993792
45.835180	1378.189032	18.998810
46.068951	1380.073723	19.003827
45.989043	1380.703885	19.008845
46.063266	1375.426675	19.013863
46.348909	1379.658989	19.018880
46.219455	1389.134194	19.023898
46.132824	1374.676053	19.028915
46.116101	1374.748481	19.033933
46.024083	1371.812628	19.038951
46.451422	1380.501604	19.043968
46.616783	1373.585269	19.048986
46.381926	1370.162144	19.054003
46.326682	1379.491548	19.059021
46.584427	1379.285688	19.064039
46.839774	1397.109745	19.069056
46.591698	1403.157898	19.074074
46.991313	1403.306403	19.079091
46.969698	1406.791777	19.084109
46.707475	1397.162698	19.089127
47.040046	1403.556857	19.094144
46.991872	1400.253484	19.099162
47.186949	1391.343662	19.104179
46.561185	1406.097313	19.109197
46.896671	1391.757578	19.114215
47.142757	1404.418731	19.119232
47.023938	1399.379498	19.124250
47.132836	1403.630958	19.129267
46.922270	1400.674252	19.134285
47.368642	1395.885172	19.139303
47.027656	1394.099725	19.144320
47.147715	1384.000434	19.149338
47.408402	1395.174540	19.154355
47.224060	1402.232157	19.159373
47.585396	1414.153312	19.164391
47.920339	1416.635747	19.169408
47.677911	1414.923678	19.174426
47.885400	1414.401768	19.179443
47.718732	1415.794760	19.184461
47.774782	1421.099475	19.189479
47.785250	1420.923295	19.194496
47.815168	1412.873178	19.199514
47.939669	1410.121013	19.204531
47.877042	1412.560077	19.209549
48.035691	1414.375369	19.214567
47.896305	1415.862644	19.219584
47.676420	1416.786144	19.224602
47.963544	1408.221244	19.229619
47.823901	1403.698452	19.234637
47.809179	1405.217762	19.239655
48.041241	1420.253255	19.244672
47.899949	1429.908008	19.249690
48.410168	1442.758753	19.254707
48.476043	1442.614308	19.259725
48.431643	1435.512340	19.264743
48.438815	1433.132026	19.269760
48.349150	1436.546828	19.274778
48.753589	1437.551603	19.279795
48.407645	1439.753118	19.284813
48.431274	1431.634747	19.289831
48.553478	1442.281520	19.294848
48.492335	1449.509230	19.299866
48.909241	1438.984196	19.304883
48.994011	1464.758579	19.309901
49.366407	1462.646689	19.314919
49.375988	1451.177945	19.319936
48.973948	1438.714255	19.324954
48.917607	1424.749842	19.329971
49.209601	1433.284574	19.334989
49.226687	1436.038339	19.340007
49.112674	1434.911213	19.345024
49.081864	1453.928542	19.350042
49.576820	1455.518657	19.355059
49.441487	1453.581702	19.360077
49.705648	1456.938097	19.365095
49.557906	1458.607470	19.370112
49.463515	1454.143282	19.375130
49.906240	1458.730608	19.380147
49.773300	1460.685311	19.385165
49.691561	1452.090355	19.390183
49.682582	1454.826015	19.395200
49.282172	1455.088195	19.400218
49.642158	1456.584209	19.405235
49.758828	1453.702237	19.410253
49.549012	1455.201615	19.415271
49.834395	1444.480724	19.420288
49.919292	1451.827074	19.425306
49.792785	1451.394136	19.430323
49.912679	1460.583459	19.435341
50.181086	1474.624400	19.440359
50.594674	1477.450461	19.445376
50.117118	1494.618893	19.450394
50.370129	1480.638054	19.455411
50.154914	1484.238691	19.460429
50.545824	1492.792055	19.465447
50.720624	1475.578995	19.470464
50.462081	1488.040232	19.475482
50.558411	1471.986656	19.480499
50.882392	1477.329930	19.485517
50.757324	1475.194812	19.490535
50.853318	1470.207648	19.495552
50.442774	1471.424645	19.500570
50.893882	1473.390941	19.505587
50.628066	1477.674385	19.510605
50.829245	1478.082246	19.515623
50.927432	1475.850969	19.520640
50.746369	1477.775485	19.525658
51.009543	1485.190251	19.530675
51.113993	1496.985270	19.535693
51.640421	1495.689888	19.540711
51.622561	1492.524761	19.545728
51.222396	1496.249445	19.550746
51.207291	1487.950870	19.555763
51.184480	1498.526510	19.560781
51.119527	1492.489333	19.565799
51.413795	1499.822955	19.570816
51.439299	1499.901752	19.575834
51.637193	1491.690607	19.580851
51.524662	1491.514397	19.585869
51.464760	1490.142450	19.590887
51.845554	1486.032342	19.595904
51.254701	1496.976400	19.600922
51.623144	1500.060359	19.605939
51.350808	1506.223606	19.610957
51.457433	1521.282014	19.615975
51.818297	1523.534177	19.620992
51.876915	1524.149983	19.626010
52.113905	1522.288539	19.631027
52.033741	1524.102590	19.636045
52.029132	1526.615099	19.641063
52.182877	1519.710473	19.646080
52.113549	1522.382554	19.651098
52.433286	1531.920984	19.656115
52.512548	1538.209664	19.661133
52.695510	1533.108421	19.666151
53.038941	1531.224955	19.671168
52.552784	1526.541215	19.676186
52.666472	1510.265033	19.681203
52.791637	1513.870916	19.686221
52.716698	1511.925490	19.691239
52.683305	1513.259727	19.696256
52.739849	1522.776540	19.701274
52.754575	1532.145587	19.706291
52.738896	1538.954371	19.711309
52.734486	1543.564461	19.716327
53.049560	1536.334986	19.721344
53.089278	1537.272434	19.726362
53.050188	1535.719861	19.731379
53.066103	1543.127718	19.736397
52.953405	1547.204239	19.741415
53.245403	1537.665635	19.746432
53.264121	1545.947426	19.751450
53.147657	1538.132594	19.756467
53.352303	1552.326720	19.761485
53.422304	1568.649121	19.766503
54.002796	1570.234481	19.771520
53.814513	1568.054739	19.776538
53.782875	1567.848942	19.781555
54.075298	1560.227950	19.786573
54.241385	1557.662939	19.791591
54.175985	1533.905166	19.796608
53.838523	1528.998290	19.801626
53.701887	1523.751744	19.806643
54.106305	1532.166273	19.811661
53.887112	1547.065868	19.816679
54.429450	1553.032319	19.821696
54.650775	1552.677001	19.826714
54.383595	1531.024003	19.831731
54.421840	1518.355972	19.836749
54.227196	1517.975695	19.841767
54.098289	1515.735699	19.846784
54.559986	1537.507065	19.851802
54.374824	1542.914902	19.856819
54.758311	1547.692019	19.861837
54.565528	1553.290101	19.866855
54.714494	1549.790940	19.871872
54.650676	1556.269941	19.876890
54.686536	1545.617222	19.881907
54.672004	1546.367626	19.886925
54.756089	1543.271765	19.891943
54.718601	1542.330728	19.896960
54.694641	1541.527993	19.901978
54.874803	1546.912517	19.906995
54.935920	1558.459670	19.912013
54.849476	1549.629224	19.917031
55.006796	1558.908053	19.922048
55.010689	1573.493828	19.927066
55.178591	1570.098995	19.932083
55.086193	1568.850945	19.937101
55.059587	1572.857653	19.942119
55.367558	1569.358045	19.947136
55.072049	1573.829519	19.952154
55.131848	1573.136876	19.957171
55.048330	1585.468709	19.962189
55.657603	1598.323989	19.967207
55.559505	1591.473391	19.972224
55.523398	1600.278098	19.977242
55.990596	1594.204407	19.982259
56.330524	1597.796270	19.987277
56.158025	1603.372888	19.992295
56.011785	1584.840240	19.997312
56.346161	1584.047632	20.002330
56.423755	1588.068128	20.007347
56.423555	1589.819292	20.012365
56.356336	1587.852102	20.017383
56.116030	1581.146795	20.022400
56.368234	1586.478809	20.027418
56.452170	1583.930204	20.032435
56.290144	1581.316179	20.037453
56.111911	1591.101973	20.042471
56.616299	1576.671399	20.047488
56.598245	1591.236822	20.052506
56.178603	1584.940450	20.057523
56.696841	1595.279386	20.062541
56.839358	1614.831881	20.067559
56.741564	1609.119011	20.072576
56.991266	1600.966127	20.077594
56.920603	1596.698740	20.082611
57.232562	1608.598726	20.087629
56.973923	1611.111343	20.092647
57.085655	1611.079747	20.097664
57.154426	1605.271873	20.102682
57.316728	1606.526351	20.107699
57.210601	1599.361338	20.112717
57.138784	1599.242926	20.117735
57.235545	1601.418130	20.122752
57.369882	1590.812399	20.127770
57.187253	1600.376884	20.132787
57.817052	1617.978335	20.137805
57.475436	1630.872387	20.142823
58.015668	1635.567182	20.147840
57.879677	1626.298866	20.152858
57.971396	1639.953578	20.157875
58.085945	1617.897648	20.162893
58.186668	1624.629250	20.167911
58.246835	1618.101547	20.172928
58.205242	1605.621516	20.177946
57.687766	1597.178818	20.182963
58.009793	1606.142510	20.187981
58.146096	1618.315002	20.192999
58.206040	1617.884536	20.198016
58.611330	1626.433617	20.203034
58.415395	1626.081504	20.208051
58.643991	1630.713918	20.213069
58.338652	1636.953961	20.218087
58.245522	1633.611552	20.223104
58.421427	1632.493313	20.228122
58.037201	1634.919326	20.233139
58.328847	1632.166114	20.238157
58.405917	1640.501250	20.243175
58.710122	1648.634862	20.248192
59.029248	1653.199482	20.253210
59.047208	1652.711426	20.258227
59.074845	1646.359983	20.263245
58.919537	1654.520362	20.268263
58.691448	1653.775169	20.273280
58.874866	1655.831648	20.278298
58.513566	1665.112877	20.283315
58.798125	1672.779691	20.288333
58.878581	1672.304870	20.293351
59.117065	1682.273825	20.298368
59.557919	1680.294623	20.303386
59.519632	1685.361171	20.308403
59.972495	1680.705572	20.313421
59.731258	1677.483044	20.318439
59.800750	1672.504944	20.323456
59.763995	1674.451562	20.328474
59.813865	1675.046387	20.333491
60.369850	1682.440931	20.338509
59.860452	1678.705886	20.343527
59.895096	1681.734729	20.348544
60.452328	1681.320038	20.353562
60.050243	1706.638732	20.358579
60.488554	1687.719440	20.363597
60.312146	1697.613265	20.368615
60.372955	1696.352734	20.373632
60.949220	1699.737233	20.378650
60.348183	1677.751328	20.383667
60.697563	1676.634570	20.388685
60.331554	1671.769007	20.393703
60.439079	1689.472301	20.398720
60.610191	1691.459964	20.403738
60.513286	1701.834278	20.408755
60.572211	1692.551244	20.413773
60.566109	1696.845914	20.418791
60.233624	1695.416890	20.423808
60.551799	1712.784808	20.428826
60.647887	1718.062105	20.433843
60.878134	1718.278528	20.438861
61.622378	1711.277253	20.443879
61.891202	1707.276248	20.448896
62.118333	1712.377040	20.453914
62.060213	1698.539841	20.458931
62.076819	1691.945331	20.463949
61.735096	1681.633618	20.468967
61.370477	1674.816647	20.473984
61.633763	1671.848458	20.479002
61.356143	1679.915006	20.484019
61.659366	1672.107126	20.489037
61.513914	1696.526856	20.494055
61.984311	1708.346257	20.499072
62.017424	1701.376953	20.504090
61.877618	1706.523373	20.509107
61.885303	1708.005917	20.514125
62.033828	1712.541821	20.519143
61.887714	1712.847567	20.524160
62.017109	1701.895731	20.529178
61.988449	1706.614625	20.534195
61.987820	1696.057237	20.539213
62.235527	1706.776642	20.544231
61.935785	1722.923648	20.549248
62.135358	1724.504618	20.554266
61.691585	1724.194085	20.559283
62.176703	1739.146101	20.564301
61.988870	1756.908795	20.569319
62.020586	1759.575148	20.574336
62.969062	1760.213545	20.579354
62.759406	1771.845622	20.584371
63.230663	1771.968449	20.589389
63.381280	1768.218177	20.594407
63.169981	1758.663478	20.599424
63.131215	1751.976177	20.604442
63.298418	1755.252295	20.609459
63.418223	1757.552432	20.614477
63.302055	1755.517765	20.619495
63.169320	1761.786257	20.624512
63.535658	1755.461549	20.629530
63.575511	1773.476187	20.634547
63.738510	1769.842755	20.639565
63.541101	1769.957026	20.644583
63.373536	1777.965569	20.649600
63.804206	1771.754967	20.654618
63.714327	1762.683630	20.659635
63.818242	1760.424196	20.664653
63.925349	1765.966214	20.669671
63.935705	1770.281397	20.674688
64.101922	1757.134816	20.679706
64.272000	1764.053378	20.684723
64.069959	1761.266051	20.689741
63.981576	1754.727152	20.694759
64.179492	1779.778530	20.699776
64.438772	1788.005510	20.704794
64.531418	1777.225085	20.709811
64.983305	1779.986571	20.714829
65.080841	1787.874683	20.719847
64.857396	1767.120781	20.724864
65.016692	1751.982830	20.729882
64.873142	1741.360976	20.734899
64.871341	1756.256137	20.739917
65.022446	1742.169952	20.744935
64.993821	1753.714450	20.749952
64.930613	1768.702506	20.754970
64.892792	1786.341484	20.759987
65.472693	1774.481258	20.765005
65.450633	1779.597896	20.770023
65.186996	1791.585024	20.775040
65.451468	1783.789041	20.780058
64.953597	1783.202851	20.785075
64.847048	1783.229580	20.790093
65.128118	1780.360777	20.795111
65.408866	1800.056281	20.800128
65.793882	1801.275729	20.805146
65.771992	1806.774240	20.810163
65.780457	1808.355090	20.815181
66.243957	1811.604024	20.820199
65.690355	1812.745214	20.825216
66.008009	1802.122652	20.830234
65.790413	1802.422956	20.835251
65.931592	1798.417552	20.840269
66.302578	1800.576737	20.845287
65.765744	1813.267950	20.850304
66.377779	1822.796565	20.855322
66.428186	1835.700044	20.860339
66.405917	1831.534393	20.865357
66.417919	1829.196129	20.870375
66.230742	1838.598523	20.875392
66.565396	1829.896752	20.880410
66.602159	1833.236692	20.885427
66.962382	1828.669282	20.890445
67.146561	1827.985091	20.895463
66.657498	1835.964024	20.900480
67.054325	1840.728780	20.905498
66.892575	1850.320657	20.910515
67.430800	1860.500938	20.915533
67.138349	1853.748667	20.920551
67.270524	1863.227529	20.925568
67.322637	1846.669886	20.930586
67.731296	1859.427230	20.935603
67.448078	1854.362020	20.940621
67.554221	1843.131271	20.945639
67.405852	1857.564270	20.950656
67.817834	1845.129532	20.955674
67.515331	1852.006200	20.960691
67.616737	1853.712555	20.965709
67.650837	1843.488667	20.970727
67.384184	1856.840923	20.975744
67.688687	1870.947881	20.980762
68.011861	1876.123318	20.985779
67.862275	1886.001387	20.990797
68.187819	1884.066915	20.995815
68.043012	1881.425174	21.000832
68.047138	1876.941341	21.005850
68.146999	1888.827581	21.010867
68.396204	1902.250837	21.015885
68.345759	1909.257689	21.020903
68.340720	1910.181731	21.025920
68.581061	1913.678014	21.030938
68.575486	1917.173829	21.035955
68.587107	1915.733658	21.040973
69.123292	1908.216081	21.045991
68.815192	1910.290897	21.051008
68.917395	1901.990714	21.056026
68.982738	1924.741894	21.061043
68.974563	1930.096828	21.066061
69.657829	1920.188630	21.071079
69.525714	1917.192801	21.076096
69.939528	1906.788835	21.081114
70.168287	1907.997253	21.086131
69.774222	1906.253241	21.091149
69.793201	1883.105719	21.096167
69.650487	1871.849377	21.101184
69.782929	1879.967170	21.106202
69.971620	1874.053045	21.111219
70.048990	1880.342179	21.116237
70.373509	1878.207090	21.121255
70.025101	1885.676841	21.126272
70.116034	1882.615602	21.131290
70.102344	1883.367850	21.136307
69.944155	1893.798934	21.141325
70.330586	1900.568214	21.146343
70.129102	1903.965481	21.151360
70.255187	1911.155597	21.156378
70.501661	1905.203510	21.161395
70.235993	1917.217056	21.166413
70.279262	1906.381361	21.171431
70.142039	1920.722408	21.176448
70.706737	1926.644346	21.181466
70.752069	1924.842267	21.186483
70.637502	1934.612971	21.191501
70.913281	1934.335212	21.196519
70.757501	1946.234453	21.201536
70.902413	1946.498528	21.206554
71.311935	1962.440898	21.211571
71.343730	1971.229412	21.216589
71.752821	1973.266933	21.221607
71.395910	1968.178499	21.226624
71.358837	1971.563024	21.231642
71.559148	1978.121928	21.236659
71.534376	1976.147240	21.241677
71.840398	1971.006504	21.246695
71.510817	1978.743647	21.251712
71.499663	1967.974434	21.256730
71.320548	1966.753756	21.261747
71.436356	1968.878995	21.266765
71.956261	1987.001897	21.271783
72.238538	1994.319245	21.276800
72.240509	1994.062186	21.281818
72.894650	1992.945547	21.286835
72.276318	1987.819056	21.291853
72.358332	1993.311781	21.296871
72.396929	1984.115812	21.301888
72.810073	1992.976002	21.306906
72.716379	1985.677246	21.311923
72.433237	1992.804700	21.316941
72.837077	1994.643487	21.321959
72.490714	1989.406834	21.326976
72.533948	1985.504275	21.331994
72.807672	1991.384438	21.337011
72.509199	2011.981212	21.342029
72.840588	2013.363531	21.347047
72.995795	2021.229972	21.352064
73.274680	2017.531947	21.357082
73.377394	2020.940496	21.362099
73.053286	2019.420675	21.367117
73.231473	2022.707625	21.372135
73.231621	2039.929155	21.377152
73.585724	2046.096379	21.382170
73.683804	2046.127290	21.387187
73.650592	2049.100552	21.392205
73.888153	2049.939795	21.397223
73.998081	2047.058441	21.402240
74.064844	2040.944040	21.407258
74.119044	2036.425461	21.412275
74.117306	2039.067500	21.417293
74.104664	2040.471956	21.422311
74.169825	2057.422066	21.427328
74.515753	2070.378991	21.432346
74.517679	2075.148032	21.437363
74.483040	2080.122762	21.442381
74.617821	2080.383799	21.447399
74.749496	2079.750844	21.452416
74.704491	2075.473943	21.457434
74.714864	2082.803450	21.462451
74.625775	2077.005100	21.467469
74.710061	2080.019078	21.472487
74.790545	2078.232401	21.477504
74.873639	2084.012781	21.482522
75.142572	2087.238598	21.487539
75.251422	2093.669834	21.492557
75.527532	2082.663427	21.497575
75.749485	2088.116787	21.502592
75.698639	2094.130066	21.507610
76.080259	2090.928348	21.512627
75.857433	2091.134641	21.517645
75.716481	2086.160280	21.522663
76.135992	2078.186412	21.527680
76.049260	2087.534073	21.532698
76.263019	2086.524475	21.537715
75.679211	2085.066706	21.542733
75.911453	2082.131553	21.547751
76.235423	2079.565023	21.552768
76.281239	2077.672293	21.557786
76.639832	2070.165257	21.562803
76.369967	2077.643306	21.567821
76.182394	2073.551126	21.572839
76.043252	2082.793318	21.577856
76.193606	2104.417222	21.582874
76.446527	2102.949136	21.587891
76.253545	2114.572005	21.592909
76.703645	2115.929880	21.597927
76.340209	2121.351009	21.602944
76.585722	2135.106979	21.607962
76.758779	2141.852376	21.612979
76.938689	2138.853073	21.617997
77.419559	2137.110874	21.623015
77.089127	2139.241400	21.628032
77.145023	2147.352762	21.633050
77.614045	2150.923303	21.638067
77.771948	2156.951915	21.643085
77.648985	2164.876864	21.648103
77.845725	2159.899509	21.653120
78.006150	2170.905403	21.658138
78.362569	2160.618685	21.663155
78.534022	2147.237827	21.668173
78.361233	2124.901363	21.673191
78.513082	2119.624387	21.678208
78.042842	2115.674844	21.683226
77.937888	2112.952816	21.688243
78.204924	2125.139414	21.693261
78.563859	2120.320947	21.698279
78.515464	2114.137858	21.703296
78.112068	2136.581413	21.708314
78.567748	2144.051909	21.713331
78.555078	2139.579060	21.718349
78.660840	2145.573418	21.723367
78.758464	2138.459336	21.728384
78.575168	2147.722684	21.733402
78.382260	2151.709540	21.738419
78.824505	2162.096923	21.743437
78.865909	2168.648458	21.748455
78.847733	2173.637805	21.753472
78.997627	2173.884127	21.758490
79.024160	2181.688568	21.763507
78.809122	2205.766715	21.768525
79.197881	2207.598193	21.773543
79.000690	2201.435861	21.778560
79.319675	2229.469904	21.783578
79.924176	2225.849610	21.788595
79.758882	2242.074024	21.793613
79.952897	2244.428045	21.798631
79.865667	2237.089119	21.803648
79.674929	2237.784978	21.808666
80.035986	2243.355832	21.813683
80.148583	2266.994571	21.818701
80.444784	2261.238029	21.823719
80.829934	2262.463794	21.828736
80.889450	2276.772866	21.833754
81.016194	2265.858478	21.838771
80.711448	2265.379545	21.843789
80.964542	2255.018989	21.848807
81.381172	2254.630019	21.853824
81.146979	2260.686825	21.858842
81.056550	2265.233469	21.863859
81.139088	2251.221214	21.868877
81.230156	2252.123005	21.873895
81.507231	2255.027416	21.878912
81.220046	2254.977862	21.883930
80.942743	2245.717698	21.888947
81.141719	2256.556218	21.893965
81.460061	2258.852963	21.898983
81.248194	2269.641656	21.904000
81.362843	2282.013945	21.909018
81.429949	2278.904225	21.914035
81.880176	2274.970177	21.919053
81.824960	2274.000545	21.924071
81.858655	2279.914015	21.929088
81.738087	2302.926181	21.934106
82.259529	2301.649287	21.939123
82.505127	2308.249232	21.944141
82.653418	2298.769089	21.949159
82.961032	2308.205681	21.954176
82.442912	2297.743336	21.959194
82.810459	2298.288540	21.964211
82.736918	2306.045106	21.969229
82.621186	2304.128801	21.974247
82.727479	2307.403349	21.979264
82.437538	2304.967550	21.984282
82.847900	2311.840913	21.989299
83.011229	2323.094473	21.994317
82.722311	2331.748295	21.999335
83.301435	2337.476650	22.004352
82.993425	2334.096176	22.009370
83.522348	2324.850015	22.014387
83.388216	2326.012867	22.019405
83.126223	2333.387756	22.024423
83.470168	2337.856721	22.029440
83.550743	2360.259931	22.034458
83.798451	2348.305656	22.039475
83.778767	2352.219679	22.044493
83.833942	2358.067795	22.049511
83.958605	2351.429850	22.054528
83.630287	2359.617775	22.059546
84.257039	2376.226861	22.064563
84.685410	2377.099375	22.069581
84.566574	2383.244542	22.074599
84.493140	2370.838482	22.079616
84.524146	2382.747567	22.084634
84.719386	2367.254606	22.089651
84.580338	2372.983031	22.094669
84.591573	2381.089340	22.099687
85.239809	2387.390504	22.104704
84.875832	2404.804454	22.109722
85.156927	2412.988377	22.114739
85.466606	2405.701130	22.119757
85.180606	2413.606448	22.124775
85.667550	2407.336243	22.129792
85.397308	2409.124109	22.134810
85.365145	2411.305105	22.139827
85.407164	2400.927561	22.144845
85.345965	2409.502634	22.149863
85.880511	2425.028230	22.154880
86.006079	2428.381493	22.159898
85.907120	2430.007426	22.164915
86.382422	2428.739372	22.169933
86.102914	2436.566060	22.174951
86.370386	2425.871884	22.179968
86.201348	2433.839274	22.184986
86.171941	2427.684009	22.190003
86.447914	2428.590515	22.195021
86.333955	2435.505399	22.200039
86.856150	2449.108181	22.205056
86.692085	2461.539532	22.210074
86.824014	2460.216331	22.215091
87.465124	2453.007058	22.220109
87.103435	2462.308902	22.225127
87.223004	2448.031248	22.230144
87.263893	2446.087322	22.235162
87.363432	2454.000245	22.240179
87.257429	2448.218347	22.245197
87.454620	2451.853427	22.250215
87.752144	2449.710151	22.255232
87.424123	2452.957691	22.260250
87.620252	2457.082735	22.265267
87.758613	2459.294063	22.270285
87.730757	2468.869186	22.275303
88.065318	2465.488985	22.280320
88.039114	2468.561167	22.285338
88.102068	2464.065420	22.290355
88.379690	2465.037800	22.295373
88.165650	2460.866841	22.300391
88.409919	2461.334109	22.305408
88.306255	2466.087746	22.310426
88.124682	2470.323597	22.315443
88.717937	2487.150191	22.320461
88.509991	2492.624743	22.325479
88.458067	2486.666119	22.330496
88.536135	2489.990674	22.335514
89.078760	2484.169082	22.340531
88.974906	2487.770732	22.345549
89.025556	2497.278099	22.350567
89.377230	2507.653995	22.355584
89.060798	2509.498763	22.360602
89.158865	2516.761930	22.365619
89.344687	2506.745869	22.370637
89.316167	2517.806246	22.375655
89.475132	2507.842288	22.380672
89.597071	2521.497873	22.385690
89.538849	2533.080152	22.390707
90.067704	2544.447939	22.395725
90.138912	2538.166848	22.400743
90.145760	2533.880021	22.405760
90.171461	2539.749248	22.410778
90.178935	2537.712826	22.415795
90.702613	2546.527013	22.420813
90.707273	2561.236035	22.425831
90.702858	2562.493888	22.430848
90.952268	2569.416951	22.435866
90.850641	2564.841434	22.440883
91.078943	2563.906560	22.445901
90.753769	2559.151649	22.450919
91.298222	2555.531025	22.455936
91.287739	2557.342277	22.460954
91.227256	2548.508915	22.465971
91.518456	2546.677323	22.470989
91.388982	2557.573394	22.476007
91.838515	2552.650365	22.481024
91.608980	2544.269532	22.486042
91.363857	2546.706029	22.491059
91.541573	2563.376161	22.496077
91.619978	2578.832040	22.501095
91.920533	2582.987404	22.506112
91.805760	2588.570134	22.511130
91.899771	2585.662192	22.516147
92.235749	2594.708398	22.521165
92.135828	2604.507797	22.526183
92.574778	2599.621554	22.531200
92.716309	2611.757736	22.536218
92.746301	2610.325078	22.541235
92.521287	2609.172214	22.546253
92.731665	2610.277045	22.551271
93.074296	2609.405851	22.556288
92.691257	2608.156014	22.561306
93.149122	2625.015101	22.566323
93.442504	2627.243212	22.571341
93.362795	2630.577482	22.576359
93.681681	2630.644538	22.581376
93.803405	2632.950000	22.586394
93.542337	2635.381286	22.591411
93.997211	2625.733452	22.596429
93.968049	2629.284924	22.601447
93.829304	2636.944610	22.606464
93.737137	2625.074955	22.611482
93.894077	2626.664680	22.616499
93.930050	2628.330811	22.621517
94.126684	2644.983319	22.626535
93.888452	2646.413115	22.631552
94.144448	2641.765544	22.636570
93.910602	2653.031803	22.641587
94.238425	2656.520412	22.646605
94.221479	2682.844856	22.651623
94.598246	2682.738504	22.656640
94.965016	2685.141841	22.661658
94.666957	2686.014226	22.666675
95.101132	2680.852356	22.671693
94.701189	2685.206845	22.676711
95.129890	2696.979601	22.681728
95.490309	2703.725605	22.686746
95.126409	2712.190903	22.691763
95.584474	2699.955323	22.696781
95.713296	2707.829648	22.701799
95.611835	2707.159031	22.706816
95.678418	2704.208772	22.711834
95.789910	2720.580610	22.716851
95.735137	2719.413226	22.721869
95.715906	2731.119102	22.726887
96.107821	2736.069613	22.731904
96.408378	2733.513957	22.736922
95.951739	2738.161758	22.741939
96.687442	2729.449538	22.746957
96.678650	2742.300217	22.751975
96.712271	2750.250625	22.756992
97.113681	2748.979079	22.762010
96.926551	2768.021238	22.767027
97.073774	2751.536597	22.772045
96.946357	2761.550520	22.777063
97.193342	2756.482338	22.782080
97.419421	2750.287636	22.787098
97.286443	2759.925686	22.792115
97.549837	2748.235840	22.797133
97.404707	2746.205066	22.802151
97.447688	2742.533872	22.807168
97.861034	2763.022397	22.812186
97.829825	2778.475429	22.817203
97.980117	2781.023032	22.822221
98.270543	2775.581064	22.827239
97.889792	2782.527051	22.832256
98.296979	2780.986414	22.837274
97.856606	2787.702926	22.842291
98.134765	2784.845846	22.847309
98.357743	2805.113290	22.852327
98.738518	2808.230116	22.857344
98.904936	2799.947921	22.862362
98.712698	2805.285317	22.867379
98.891490	2802.255363	22.872397
99.065789	2801.872795	22.877415
99.174024	2806.221610	22.882432
99.482992	2815.891769	22.887450
99.386147	2829.985586	22.892467
99.875080	2828.762091	22.897485
99.757417	2826.394042	22.902503
100.030167	2837.017543	22.907520
99.998278	2829.658115	22.912538
99.953293	2830.140393	22.917555
99.942061	2825.726167	22.922573
99.879865	2816.282659	22.927591
99.459861	2818.692350	22.932608
100.224709	2819.449917	22.937626
100.040373	2826.734174	22.942643
100.377472	2833.627033	22.947661
100.516188	2839.317343	22.952679
100.371084	2843.322809	22.957696
100.950212	2841.135832	22.962714
100.701797	2843.580008	22.967731
100.776699	2850.270761	22.972749
100.857915	2862.434486	22.977767
100.905394	2871.631957	22.982784
101.223867	2878.266889	22.987802
100.792470	2885.613099	22.992819
101.275198	2873.155553	22.997837
101.614878	2880.463390	23.002855
101.175487	2876.558131	23.007872
101.533235	2888.970431	23.012890
101.305550	2901.128824	23.017907
101.638692	2901.059252	23.022925
101.486233	2897.966604	23.027943
101.650284	2916.956095	23.032960
102.137534	2925.493067	23.037978
102.411227	2936.934653	23.042995
102.762617	2925.861990	23.048013
102.643510	2927.278313	23.053031
102.544439	2926.820298	23.058048
103.100564	2922.214113	23.063066
102.862333	2929.864882	23.068083
102.659893	2914.491408	23.073101
102.735642	2931.259989	23.078119
103.121828	2941.395777	23.083136
103.511871	2945.206815	23.088154
103.484944	2946.649950	23.093171
103.596097	2953.941464	23.098189
104.092478	2954.893272	23.103207
103.571656	2947.146107	23.108224
103.594658	2941.105955	23.113242
103.589950	2955.449554	23.118259
103.801773	2937.264086	23.123277
103.743682	2953.280856	23.128295
103.698766	2966.779507	23.133312
103.973123	2968.257621	23.138330
104.204406	2969.552328	23.143347
104.426884	2976.348936	23.148365
104.805274	2992.060515	23.153383
104.484357	3004.017141	23.158400
105.196381	2982.432870	23.163418
104.995843	2994.895116	23.168435
105.259129	2991.068345	23.173453
105.316525	2996.922633	23.178471
105.018570	2989.129748	23.183488
105.084626	2983.303701	23.188506
105.096636	3006.559461	23.193523
105.643008	3016.263133	23.198541
105.624288	3025.112216	23.203559
105.436807	3029.792937	23.208576
105.818547	3019.629808	23.213594
105.882066	3024.368823	23.218611
105.968268	3024.341864	23.223629
106.149517	3048.965347	23.228647
105.827779	3055.922121	23.233664
106.140079	3056.241479	23.238682
106.372145	3049.474750	23.243699
106.581106	3065.873670	23.248717
106.830923	3077.496508	23.253735
106.815349	3080.299698	23.258752
107.060583	3070.865187	23.263770
107.042852	3083.337285	23.268787
106.981139	3075.877570	23.273805
107.611881	3074.571826	23.278823
107.302706	3073.369914	23.283840
107.551503	3072.459168	23.288858
107.795598	3069.070644	23.293875
107.904890	3062.865697	23.298893
107.586040	3063.680133	23.303911
107.717486	3082.794940	23.308928
108.112047	3084.258603	23.313946
108.255359	3080.913599	23.318963
108.130415	3089.408292	23.323981
108.393289	3088.134150	23.328999
108.119760	3089.248169	23.334016
108.247331	3087.990607	23.339034
108.258264	3103.277888	23.344051
108.938718	3107.148195	23.349069
109.089718	3105.278023	23.354087
109.035739	3118.104629	23.359104
109.048973	3105.902103	23.364122
109.334091	3117.492331	23.369139
109.202254	3118.667458	23.374157
109.473589	3106.175167	23.379175
109.433460	3122.179283	23.384192
109.742581	3113.403874	23.389210
109.464130	3122.452489	23.394227
109.601468	3131.681641	23.399245
109.737752	3131.147101	23.404263
109.901527	3142.727196	23.409280
109.868262	3136.328568	23.414298
110.122481	3144.970536	23.419315
110.227603	3171.329067	23.424333
110.295658	3166.316868	23.429351
110.109490	3179.082413	23.434368
110.315385	3170.370589	23.439386
110.534065	3184.372522	23.444403
110.737428	3194.699503	23.449421
111.028247	3197.175787	23.454439
111.033136	3194.097486	23.459456
111.159809	3200.926257	23.464474
111.470736	3207.342092	23.469491
111.401343	3221.757321	23.474509
112.159565	3213.111968	23.479527
111.979840	3216.112162	23.484544
112.142627	3212.709164	23.489562
112.266354	3213.440609	23.494579
112.110847	3217.190787	23.499597
112.435415	3206.142071	23.504615
112.331572	3215.466476	23.509632
112.322185	3213.534747	23.514650
112.445060	3209.156006	23.519667
112.582248	3210.936494	23.524685
112.824756	3210.923327	23.529703
112.843340	3219.580871	23.534720
112.923866	3237.920397	23.539738
112.963192	3237.553163	23.544755
112.567992	3240.580114	23.549773
113.068483	3234.383719	23.554791
112.757300	3254.931480	23.559808
112.894005	3260.964438	23.564826
113.004910	3270.241376	23.569843
113.323268	3286.366418	23.574861
113.912610	3279.172071	23.579879
113.683729	3281.435884	23.584896
114.226699	3273.612175	23.589914
114.753818	3265.484380	23.594931
114.844589	3267.662784	23.599949
114.948342	3262.335537	23.604967
115.253535	3268.327900	23.609984
115.351293	3262.482700	23.615002
115.272354	3268.796404	23.620019
115.513323	3267.120337	23.625037
115.649957	3255.021216	23.630055
115.207251	3257.684375	23.635072
115.487562	3265.212123	23.640090
115.425628	3259.203286	23.645107
115.292362	3270.696999	23.650125
115.713288	3266.325016	23.655143
115.469475	3270.086338	23.660160
115.273530	3269.171922	23.665178
115.536397	3276.404908	23.670195
115.257118	3299.016528	23.675213
115.772643	3287.174528	23.680231
115.670874	3305.836190	23.685248
115.792502	3324.474530	23.690266
116.243772	3329.498056	23.695283
115.853507	3337.996814	23.700301
116.184760	3346.274875	23.705319
116.449503	3353.868646	23.710336
116.683924	3358.917193	23.715354
116.896528	3368.056410	23.720371
117.047866	3380.086826	23.725389
117.548718	3377.844276	23.730407
117.132423	3375.849032	23.735424
117.394193	3381.387975	23.740442
117.607478	3382.296298	23.745459
117.300596	3389.915387	23.750477
117.302878	3405.510340	23.755495
117.783660	3412.072461	23.760512
117.794418	3405.062799	23.765530
118.168060	3418.734042	23.770547
117.974145	3438.582955	23.775565
118.476557	3441.821447	23.780583
118.355540	3427.873069	23.785600
118.786177	3434.082864	23.790618
118.902958	3435.584062	23.795635
118.969607	3453.672183	23.800653
119.608874	3455.519280	23.805671
119.534309	3457.283012	23.810688
119.078753	3466.118709	23.815706
119.199837	3460.299878	23.820723
119.341713	3454.504762	23.825741
119.507928	3459.841873	23.830759
119.533101	3471.479107	23.835776
119.387170	3489.996735	23.840794
119.616677	3487.133834	23.845811
119.844006	3497.171568	23.850829
119.965278	3512.514544	23.855847
119.936136	3524.511276	23.860864
119.962396	3527.139071	23.865882
120.420957	3539.057130	23.870899
120.443021	3547.884376	23.875917
120.308017	3556.084896	23.880935
120.499065	3571.007231	23.885952
120.784907	3582.809915	23.890970
121.274111	3582.869153	23.895987
121.279209	3597.237698	23.901005
121.492955	3590.893123	23.906023
121.268844	3602.558099	23.911040
121.728320	3607.813058	23.916058
121.900082	3614.671530	23.921075
121.931867	3617.091310	23.926093
122.383113	3608.412889	23.931111
122.391834	3613.452170	23.936128
122.195949	3607.312685	23.941146
122.892876	3612.073407	23.946163
122.472677	3632.938240	23.951181
122.648714	3641.161140	23.956199
122.816378	3645.108140	23.961216
123.027121	3643.635900	23.966234
123.198804	3638.934323	23.971251
123.153442	3641.259040	23.976269
123.299244	3634.961176	23.981287
122.902619	3644.909756	23.986304
123.136726	3662.771054	23.991322
123.931658	3654.114244	23.996339
123.947765	3663.486313	24.001357
123.723904	3658.442537	24.006375
123.882159	3673.926394	24.011392
124.285947	3676.189470	24.016410
124.538906	3691.895038	24.021427
124.243020	3697.077102	24.026445
124.273232	3690.518862	24.031463
124.670369	3702.060592	24.036480
124.325182	3696.802684	24.041498
124.726674	3685.582561	24.046515
124.702859	3709.990739	24.051533
125.090766	3718.075309	24.056551
125.179227	3724.082996	24.061568
124.925078	3730.521289	24.066586
125.465907	3730.155754	24.071603
125.510701	3751.436055	24.076621
125.662376	3746.483801	24.081639
125.380869	3744.922072	24.086656
125.814608	3754.461832	24.091674
126.135009	3750.724219	24.096691
126.126345	3787.066586	24.101709
126.428860	3778.742359	24.106727
126.599883	3780.646835	24.111744
126.358994	3776.912715	24.116762
126.448554	3769.733869	24.121779
126.653641	3799.084325	24.126797
126.761124	3792.115905	24.131815
127.493629	3796.932592	24.136832
126.917805	3799.754592	24.141850
127.541382	3809.895994	24.146867
127.535606	3817.216793	24.151885
127.980759	3820.032934	24.156903
128.560009	3805.959975	24.161920
128.638068	3801.325490	24.166938
129.030573	3795.735089	24.171955
128.696965	3778.360640	24.176973
128.758984	3770.822149	24.181991
128.971286	3764.598626	24.187008
128.528544	3768.384855	24.192026
129.143000	3769.469480	24.197043
129.265626	3769.966459	24.202061
129.164988	3773.459981	24.207079
129.086966	3785.257135	24.212096
128.929924	3799.633911	24.217114
128.804865	3799.318000	24.222131
129.088093	3810.461756	24.227149
129.295057	3823.850775	24.232167
129.527352	3833.427603	24.237184
129.309530	3842.428361	24.242202
129.689545	3841.360317	24.247219
129.711581	3860.634434	24.252237
130.021538	3863.131271	24.257255
130.363115	3863.649750	24.262272
130.205124	3884.582776	24.267290
130.373718	3888.252873	24.272307
130.470367	3885.220614	24.277325
130.710598	3891.416559	24.282343
131.272614	3901.229622	24.287360
131.202379	3909.549896	24.292378
131.547522	3910.270962	24.297395
131.652101	3913.468959	24.302413
131.778906	3908.437704	24.307431
132.118997	3904.972412	24.312448
132.010843	3906.248006	24.317466
132.174709	3907.159849	24.322483
132.231683	3903.106477	24.327501
132.153282	3902.192964	24.332519
132.690241	3906.925631	24.337536
132.720260	3920.987535	24.342554
132.810385	3921.759248	24.347571
132.910730	3934.894783	24.352589
132.860821	3934.982581	24.357607
132.926931	3929.410147	24.362624
132.667913	3934.085305	24.367642
132.774808	3933.455610	24.372659
133.082156	3951.435400	24.377677
132.957210	3957.187654	24.382695
133.507330	3959.587502	24.387712
132.945450	3968.621094	24.392730
133.412403	3972.997645	24.397747
133.490434	3982.492310	24.402765
133.599423	3998.695802	24.407783
133.917375	4010.535213	24.412800
133.928170	4024.756727	24.417818
134.069245	4032.516283	24.422835
133.968484	4062.438214	24.427853
134.604499	4057.455384	24.432871
134.765777	4057.971937	24.437888
134.487349	4081.649267	24.442906
135.169335	4076.155567	24.447923
135.344009	4076.061930	24.452941
135.114536	4095.984127	24.457959
135.502709	4101.620452	24.462976
135.745316	4099.427020	24.467994
135.888847	4102.348463	24.473011
135.915607	4110.464901	24.478029
136.056048	4126.389635	24.483047
136.273402	4124.850102	24.488064
136.229551	4131.122095	24.493082
136.363919	4138.963146	24.498099
136.709402	4145.427179	24.503117
136.806999	4159.689517	24.508135
136.874626	4158.222113	24.513152
137.073234	4161.879413	24.518170
137.504130	4173.852172	24.523187
137.642905	4194.384271	24.528205
137.510456	4193.253309	24.533223
137.729453	4189.226491	24.538240
137.703012	4201.608393	24.543258
137.787250	4189.858652	24.548275
138.153744	4208.504606	24.553293
138.167385	4224.817498	24.558311
138.436583	4221.391875	24.563328
138.432256	4213.711811	24.568346
138.724210	4218.702645	24.573363
138.992278	4237.796555	24.578381
138.757544	4248.237200	24.583399
139.155947	4242.867745	24.588416
139.015603	4261.539710	24.593434
139.392205	4255.752546	24.598451
139.613517	4266.307213	24.603469
139.705781	4281.450218	24.608487
140.205397	4270.778035	24.613504
140.220270	4265.536884	24.618522
139.839817	4266.768765	24.623539
140.360238	4270.828592	24.628557
140.398002	4263.554962	24.633575
140.732834	4276.566764	24.638592
140.743360	4292.477029	24.643610
140.707973	4289.603663	24.648627
141.152777	4287.881413	24.653645
140.712122	4306.062301	24.658663
140.813191	4291.220202	24.663680
140.950463	4313.874315	24.668698
141.282311	4320.684839	24.673715
141.429029	4326.146373	24.678733
141.534155	4342.929305	24.683751
141.955315	4338.940520	24.688768
141.892024	4350.178077	24.693786
142.169848	4344.895566	24.698803
142.444498	4345.064102	24.703821
142.346552	4341.745928	24.708839
142.627677	4354.509984	24.713856
142.689966	4366.255907	24.718874
143.122107	4368.202513	24.723891
143.217971	4369.890773	24.728909
143.357551	4372.726295	24.733927
143.404646	4360.277755	24.738944
143.309327	4367.223073	24.743962
143.419720	4367.225171	24.748979
143.837658	4375.007406	24.753997
143.982250	4393.457345	24.759015
144.269688	4377.454869	24.764032
144.193217	4391.374627	24.769050
144.563146	4389.792389	24.774067
144.360688	4390.212678	24.779085
144.307089	4393.165359	24.784103
144.844417	4406.201110	24.789120
145.102814	4408.113590	24.794138
145.072005	4413.827528	24.799155
145.658396	4408.229108	24.804173
145.482091	4414.635842	24.809191
145.665938	4401.139960	24.814208
145.782855	4405.824451	24.819226
146.032335	4420.768996	24.824243
146.455848	4418.034347	24.829261
146.331419	4424.587610	24.834279
147.117627	4412.026446	24.839296
146.605680	4421.842289	24.844314
146.815899	4419.288779	24.849331
146.846402	4410.693225	24.854349
146.772499	4421.040317	24.859367
146.848516	4414.870687	24.864384
146.964165	4427.239394	24.869402
146.940069	4429.024773	24.874419
146.851569	4449.003533	24.879437
147.123450	4452.577847	24.884455
147.449310	4463.198754	24.889472
147.164333	4475.161547	24.894490
147.497225	4484.889805	24.899507
147.606755	4494.046417	24.904525
147.467443	4512.105801	24.909543
147.691708	4527.965823	24.914560
147.985401	4541.228820	24.919578
148.028639	4559.755651	24.924595
148.539523	4574.141850	24.929613
148.743265	4584.605934	24.934631
148.886913	4579.842582	24.939648
148.897234	4600.867512	24.944666
149.359006	4601.477484	24.949683
149.562047	4619.087115	24.954701
149.063826	4638.347440	24.959719
149.687111	4641.692506	24.964736
150.088942	4648.934146	24.969754
150.294259	4664.217032	24.974771
150.728495	4653.254613	24.979789
150.464397	4662.865609	24.984807
150.609541	4659.039956	24.989824
150.395417	4668.641076	24.994842
150.892472	4691.186333	24.999859
151.352612	4681.473370	25.004877
151.360419	4688.700175	25.009895
151.643326	4686.622825	25.014912
151.561009	4684.106858	25.019930
151.530554	4696.646539	25.024947
152.086455	4700.943939	25.029965
152.099751	4702.574289	25.034983
152.144788	4700.930240	25.040000
152.535130	4705.581198	25.045018
152.387527	4704.985101	25.050035
152.760038	4699.998609	25.055053
152.983082	4702.192644	25.060071
152.888897	4726.941324	25.065088
153.306369	4728.102074	25.070106
153.336649	4718.246306	25.075123
153.704030	4716.073009	25.080141
153.494675	4725.967128	25.085159
153.628771	4723.677448	25.090176
153.781795	4720.562419	25.095194
153.959947	4740.517715	25.100211
154.142914	4746.774314	25.105229
154.577264	4745.577478	25.110247
154.508819	4744.128693	25.115264
155.134026	4748.433492	25.120282
154.556798	4747.961550	25.125299
154.925369	4747.351345	25.130317
154.760037	4777.614564	25.135335
154.978992	4775.124125	25.140352
155.205390	4788.408753	25.145370
155.276934	4794.143623	25.150387
155.472579	4805.523553	25.155405
155.136048	4809.303795	25.160423
155.620660	4820.631780	25.165440
155.899230	4832.501199	25.170458
155.740705	4834.521603	25.175475
156.149464	4851.457026	25.180493
156.112858	4871.875032	25.185511
156.608063	4869.878153	25.190528
156.961439	4893.737599	25.195546
157.158536	4905.482788	25.200563
157.243257	4905.018978	25.205581
157.427613	4898.773665	25.210599
157.677825	4907.993773	25.215616
157.603660	4918.571990	25.220634
157.528607	4930.174194	25.225651
158.019075	4920.795486	25.230669
158.008260	4933.028092	25.235687
158.194825	4946.326561	25.240704
158.506795	4940.409704	25.245722
158.456852	4945.979740	25.250739
158.877405	4973.706895	25.255757
158.973176	4973.149102	25.260775
159.021513	4986.997455	25.265792
158.893672	4976.457416	25.270810
159.200051	5002.704071	25.275827
160.029698	5006.369332	25.280845
159.690925	5013.373504	25.285863
159.930388	5009.592737	25.290880
160.198917	5021.959347	25.295898
159.906379	5036.863809	25.300915
160.280396	5032.021089	25.305933
160.394609	5047.380917	25.310951
160.694068	5047.940700	25.315968
160.874410	5059.788022	25.320986
161.392387	5059.324671	25.326003
161.667955	5051.106244	25.331021
161.822381	5055.479908	25.336039
161.563403	5048.984513	25.341056
162.187635	5059.928766	25.346074
162.356375	5072.388392	25.351091
162.400390	5072.137685	25.356109
162.408939	5071.678652	25.361127
162.336520	5069.843013	25.366144
162.583368	5068.645809	25.371162
162.655564	5075.317882	25.376179
162.733066	5086.435697	25.381197
162.632436	5101.894284	25.386215
162.751435	5114.006227	25.391232
163.071502	5121.285302	25.396250
163.348494	5137.323046	25.401267
163.313074	5138.975713	25.406285
163.619737	5144.635414	25.411303
163.607370	5147.694006	25.416320
163.863123	5160.698421	25.421338
163.878608	5177.744439	25.426355
164.176251	5168.578769	25.431373
164.640175	5195.764346	25.436391
164.265025	5206.487280	25.441408
164.486467	5204.729595	25.446426
164.560313	5223.149736	25.451443
164.857296	5227.313103	25.456461
164.958193	5237.400924	25.461479
165.328174	5252.617642	25.466496
165.745515	5255.944299	25.471514
165.810080	5264.096793	25.476531
165.915863	5275.588081	25.481549
166.438628	5281.180419	25.486567
166.329415	5279.864372	25.491584
166.648171	5279.054506	25.496602
166.632987	5306.872769	25.501619
166.567440	5319.113195	25.506637
167.001436	5316.739730	25.511655
166.854737	5338.445429	25.516672
167.196888	5339.488006	25.521690
167.240556	5351.290527	25.526707
167.860584	5359.671317	25.531725
168.764087	5365.954138	25.536743
168.743179	5354.900686	25.541760
168.934279	5353.662319	25.546778
169.242130	5354.495586	25.551795
169.279574	5346.755260	25.556813
169.300034	5346.498224	25.561831
169.212001	5354.709988	25.566848
169.381635	5338.773369	25.571866
169.544018	5349.192069	25.576883
169.673935	5351.333151	25.581901
169.788946	5347.245350	25.586919
169.690299	5372.658930	25.591936
170.025583	5376.751392	25.596954
169.948910	5385.358226	25.601971
169.824564	5379.914588	25.606989
170.091375	5396.029897	25.612007
170.191194	5417.041832	25.617024
170.412463	5425.162069	25.622042
170.425909	5446.579039	25.627059
170.685538	5461.890693	25.632077
171.092593	5472.819342	25.637095
170.867374	5484.465808	25.642112
171.378834	5498.565293	25.647130
171.516766	5513.377408	25.652147
171.513812	5524.425417	25.657165
171.707680	5529.082494	25.662183
172.165243	5543.848615	25.667200
172.661107	5561.894228	25.672218
173.018703	5565.486060	25.677236
173.434017	5563.268458	25.682253
173.149261	5563.307077	25.687271
173.288634	5569.054587	25.692288
173.437237	5569.462249	25.697306
173.601204	5595.255488	25.702324
173.698041	5579.807219	25.707341
174.001820	5578.659587	25.712359
174.061710	5599.183002	25.717376
174.617427	5609.634178	25.722394
174.201216	5619.786117	25.727412
174.617930	5610.809907	25.732429
174.918638	5601.030729	25.737447
174.779364	5616.598628	25.742464
175.314530	5620.572881	25.747482
175.195465	5631.934820	25.752500
175.374913	5642.918736	25.757517
175.637926	5642.390625	25.762535
175.590735	5661.233065	25.767552
175.908721	5660.495769	25.772570
176.027815	5671.198322	25.777588
176.220200	5680.352884	25.782605
176.596472	5684.633941	25.787623
176.325212	5703.275808	25.792640
176.772041	5696.543936	25.797658
176.377629	5712.240172	25.802676
176.490488	5729.829803	25.807693
176.718276	5753.538938	25.812711
176.929057	5762.836986	25.817728
177.308053	5772.598552	25.822746
177.668379	5810.490205	25.827764
177.878419	5804.102437	25.832781
177.944445	5821.253379	25.837799
178.334278	5818.601280	25.842816
178.469156	5815.957678	25.847834
179.071793	5826.579989	25.852852
179.423108	5837.946614	25.857869
179.755492	5825.330585	25.862887
179.857267	5838.265846	25.867904
180.181319	5829.951537	25.872922
180.138736	5834.287269	25.877940
180.240889	5843.767237	25.882957
180.401849	5827.062864	25.887975
180.486268	5843.883130	25.892992
180.361954	5848.785348	25.898010
180.157440	5865.382710	25.903028
180.455354	5868.495425	25.908045
180.919848	5885.123412	25.913063
180.960446	5902.542517	25.918080
181.279775	5897.225031	25.923098
181.706721	5924.160464	25.928116
181.506019	5930.816810	25.933133
182.038898	5925.800929	25.938151
182.030725	5952.440108	25.943168
181.918570	5959.729960	25.948186
181.908738	5965.189724	25.953204
182.280412	5977.898313	25.958221
182.579760	5980.765864	25.963239
182.395328	5994.146555	25.968256
183.014097	6011.084565	25.973274
183.147862	6024.700676	25.978292
183.343558	6044.060058	25.983309
183.739390	6041.140711	25.988327
183.695215	6056.371892	25.993344
184.337713	6069.222220	25.998362
184.308107	6071.024452	26.003380
184.475597	6082.531278	26.008397
185.022909	6084.477875	26.013415
184.720361	6105.359891	26.018432
184.665396	6108.603750	26.023450
184.893005	6108.587949	26.028468
184.804938	6133.008589	26.033485
185.601495	6133.850486	26.038503
185.542208	6147.003366	26.043520
185.768907	6166.620025	26.048538
185.953806	6164.239785	26.053556
186.250365	6177.906166	26.058573
186.378745	6187.999480	26.063591
186.626352	6197.711470	26.068608
186.769158	6196.674032	26.073626
186.781265	6202.352344	26.078644
186.894309	6223.835730	26.083661
187.237451	6222.476731	26.088679
187.253671	6237.293998	26.093696
187.571507	6257.148454	26.098714
188.003501	6266.695164	26.103732
187.970057	6274.469863	26.108749
188.151479	6283.606118	26.113767
188.364786	6285.256169	26.118784
188.569461	6291.660216	26.123802
189.649027	6282.859399	26.128820
191.599413	6244.393563	26.133837
191.770821	6223.240877	26.138855
191.659703	6201.253021	26.143872
191.658604	6182.754210	26.148890
192.088702	6159.326494	26.153908
191.486793	6160.197558	26.158925
191.543175	6127.931050	26.163943
191.562996	6110.875708	26.168960
191.266667	6102.628110	26.173978
191.469759	6100.707977	26.178996
191.585958	6100.606723	26.184013
191.812692	6099.369468	26.189031
191.415086	6107.046283	26.194048
191.456982	6127.307158	26.199066
191.831056	6128.726486	26.204084
191.879701	6137.160895	26.209101
192.124904	6148.606025	26.214119
192.202185	6166.165036	26.219136
191.937525	6186.458810	26.224154
192.199064	6195.086287	26.229172
192.188520	6217.473917	26.234189
192.396952	6229.399367	26.239207
192.494979	6256.831094	26.244224
192.690337	6277.519549	26.249242
192.771930	6293.028572	26.254260
192.850953	6317.554842	26.259277
193.247817	6340.164011	26.264295
193.478943	6360.934059	26.269312
193.775757	6366.709260	26.274330
194.647725	6388.800843	26.279348
194.506179	6394.501604	26.284365
195.005165	6412.400388	26.289383
195.137914	6437.657508	26.294400
195.306951	6435.631938	26.299418
195.407375	6454.952520	26.304436
195.733209	6471.357636	26.309453
196.203015	6462.389457	26.314471
195.735318	6482.748850	26.319488
195.973005	6503.830688	26.324506
196.283318	6510.774134	26.329524
196.326385	6528.622782	26.334541
196.770952	6536.603310	26.339559
197.123685	6562.210021	26.344576
197.082904	6568.613221	26.349594
198.038836	6586.472508	26.354612
197.843933	6587.036520	26.359629
197.908066	6593.942142	26.364647
198.139132	6607.447284	26.369664
198.020795	6616.724120	26.374682
198.562882	6626.011736	26.379700
198.626857	6634.757346	26.384717
199.317357	6638.845467	26.389735
199.359633	6645.406604	26.394752
199.589758	6647.372109	26.399770
199.813271	6644.948363	26.404788
199.973037	6675.227355	26.409805
200.652213	6676.788226	26.414823
200.856743	6682.953798	26.419840
200.561606	6682.481379	26.424858
201.061819	6678.215810	26.429876
200.585323	6680.025416	26.434893
200.822172	6667.003990	26.439911
201.191358	6683.385584	26.444928
200.921023	6693.203631	26.449946
201.143215	6702.550747	26.454964
200.894945	6722.807824	26.459981
201.143562	6739.986922	26.464999
201.345342	6764.890464	26.470016
201.881774	6784.844740	26.475034
202.208908	6790.014078	26.480052
202.320794	6814.870411	26.485069
202.555817	6822.391254	26.490087
202.526940	6848.380836	26.495104
202.916460	6865.821003	26.500122
203.529436	6869.874807	26.505140
203.815566	6888.022955	26.510157
204.232095	6888.081312	26.515175
204.314039	6901.146763	26.520192
204.012850	6920.241632	26.525210
204.591352	6917.294141	26.530228
204.914876	6941.551542	26.535245
205.071359	6943.350521	26.540263
205.183145	6955.072819	26.545280
205.538951	6952.033935	26.550298
205.943286	6964.489780	26.555316
205.559687	6979.393865	26.560333
206.368024	6983.828763	26.565351
206.334944	6997.453743	26.570368
206.284387	7017.223860	26.575386
206.386636	7014.097130	26.580404
206.500148	7034.732433	26.585421
206.741786	7058.977626	26.590439
206.925671	7068.575501	26.595456
206.935608	7084.910866	26.600474
207.285676	7094.734774	26.605492
206.809562	7120.756578	26.610509
207.077660	7144.139730	26.615527
208.015191	7169.152445	26.620544
208.385383	7185.635214	26.625562
208.755436	7186.318834	26.630580
208.650331	7213.642609	26.635597
209.184979	7215.520567	26.640615
209.575885	7231.526549	26.645632
210.295276	7223.930355	26.650650
210.918062	7211.401247	26.655668
211.469475	7211.105585	26.660685
211.515264	7196.817382	26.665703
211.586347	7202.807624	26.670720
211.440482	7205.583965	26.675738
211.531044	7201.915644	26.680756
211.749002	7203.287759	26.685773
212.030893	7193.935290	26.690791
212.107902	7198.792657	26.695808
212.138903	7196.503213	26.700826
212.486384	7192.810322	26.705844
212.472288	7200.565718	26.710861
212.456612	7199.989347	26.715879
212.534099	7207.004868	26.720896
212.246129	7229.907113	26.725914
212.468323	7240.874799	26.730932
212.740612	7258.401830	26.735949
212.742476	7269.996116	26.740967
213.163889	7294.070804	26.745984
213.180886	7320.686043	26.751002
213.514173	7320.408506	26.756020
213.355139	7347.299582	26.761037
214.077651	7354.213508	26.766055
214.322795	7369.319896	26.771072
214.246206	7386.419823	26.776090
214.787526	7404.153586	26.781108
214.678906	7422.709003	26.786125
215.185369	7434.815847	26.791143
215.481176	7445.858877	26.796160
215.724584	7450.790285	26.801178
216.406849	7468.741734	26.806196
216.738563	7479.024216	26.811213
216.295235	7482.872449	26.816231
216.727527	7496.082614	26.821248
216.768908	7509.451476	26.826266
217.147604	7515.801113	26.831284
217.322177	7531.679502	26.836301
217.592119	7541.886430	26.841319
217.809046	7549.957285	26.846336
217.942052	7574.856196	26.851354
218.259624	7574.064539	26.856372
218.434299	7590.272227	26.861389
218.281005	7607.177971	26.866407
218.603954	7624.181048	26.871424
218.643821	7634.239579	26.876442
219.246362	7655.472642	26.881460
219.092937	7661.046645	26.886477
219.540570	7683.048283	26.891495
220.024257	7699.582835	26.896512
220.040778	7723.559243	26.901530
220.619146	7726.341372	26.906548
220.704718	7723.194431	26.911565
220.917323	7752.390697	26.916583
221.039014	7761.132064	26.921600
220.981442	7781.598262	26.926618
221.444962	7789.463636	26.931636
221.523619	7800.798998	26.936653
221.505765	7824.817504	26.941671
222.093679	7836.842592	26.946688
222.042059	7857.577294	26.951706
222.705000	7852.966148	26.956724
223.270367	7877.863013	26.961741
223.439440	7884.471337	26.966759
224.182050	7872.849728	26.971776
224.316629	7888.167181	26.976794
224.424331	7902.574583	26.981812
224.753575	7900.129931	26.986829
225.208926	7886.922330	26.991847
225.389107	7883.428013	26.996864
225.435189	7894.001625	27.001882
225.379830	7884.370799	27.006900
225.806147	7890.656747	27.011917
225.650627	7912.047616	27.016935
225.714188	7916.473408	27.021952
226.284709	7915.001663	27.026970
226.670860	7924.499494	27.031988
227.020481	7945.313371	27.037005
227.347365	7937.324400	27.042023
227.388842	7932.776315	27.047040
227.665417	7935.521191	27.052058
227.562424	7931.446894	27.057076
227.759671	7943.734691	27.062093
227.743973	7960.962966	27.067111
228.161701	7967.939621	27.072128
227.962756	7972.494906	27.077146
228.176690	7987.521207	27.082164
228.411379	8003.129346	27.087181
228.424476	8024.928744	27.092199
228.757725	8031.640613	27.097216
228.700894	8049.219262	27.102234
229.008838	8060.645110	27.107252
229.326378	8083.633873	27.112269
229.426380	8098.023826	27.117287
229.982972	8109.667557	27.122304
229.740324	8128.873089	27.127322
229.708073	8137.232988	27.132340
230.392587	8158.108871	27.137357
230.354948	8175.111795	27.142375
230.921504	8186.718480	27.147392
231.091900	8217.915554	27.152410
231.566939	8229.508329	27.157428
231.839927	8242.982691	27.162445
232.109717	8250.092758	27.167463
232.177486	8277.612559	27.172480
232.402760	8296.285239	27.177498
232.915476	8311.489070	27.182516
232.946359	8328.119991	27.187533
232.889486	8348.644303	27.192551
233.201369	8363.401823	27.197568
233.683596	8380.606900	27.202586
234.270435	8392.564846	27.207604
234.594132	8399.193382	27.212621
234.549640	8418.253691	27.217639
234.811215	8416.199108	27.222656
235.037408	8431.721640	27.227674
234.658485	8446.649942	27.232692
235.539239	8465.041398	27.237709
235.977863	8490.992219	27.242727
236.166127	8486.158060	27.247744
236.469311	8500.012827	27.252762
236.467145	8503.624152	27.257780
236.879430	8514.557196	27.262797
236.805134	8542.420880	27.267815
237.274738	8543.377127	27.272832
237.292981	8564.428838	27.277850
237.632339	8575.363013	27.282868
237.813831	8608.657555	27.287885
237.859306	8617.273412	27.292903
238.403144	8625.544153	27.297920
238.623316	8640.589727	27.302938
238.455866	8646.089202	27.307956
238.555053	8668.769267	27.312973
238.778168	8703.216655	27.317991
239.191804	8712.113278	27.323008
239.282457	8743.399463	27.328026
239.586885	8757.620552	27.333044
239.942292	8770.508970	27.338061
240.346859	8795.712854	27.343079
240.674105	8797.783022	27.348096
241.103153	8820.488847	27.353114
241.110515	8836.727964	27.358132
241.844173	8843.590283	27.363149
241.730046	8851.407215	27.368167
242.572832	8854.676567	27.373184
242.502101	8861.601643	27.378202
242.890316	8883.243780	27.383220
243.010643	8886.388968	27.388237
242.934780	8900.610347	27.393255
243.684540	8904.545856	27.398272
243.880481	8919.802900	27.403290
243.931242	8918.330773	27.408308
244.390824	8928.255789	27.413325
244.367412	8942.116361	27.418343
244.761402	8949.090305	27.423360
245.091606	8947.013225	27.428378
245.055823	8961.202003	27.433396
245.418562	8962.677838	27.438413
245.471381	8969.618670	27.443431
245.738216	8977.076957	27.448448
245.782364	8992.030792	27.453466
246.082858	8997.015432	27.458484
246.418902	9010.756472	27.463501
246.593501	9038.496162	27.468519
246.683123	9036.119515	27.473536
246.730176	9052.277418	27.478554
246.982600	9076.928016	27.483572
247.151769	9090.154078	27.488589
247.331941	9116.177216	27.493607
247.054339	9133.373853	27.498624
247.370773	9153.608719	27.503642
247.711803	9177.255308	27.508660
248.510201	9194.493815	27.513677
248.590938	9227.199797	27.518695
248.945188	9238.669216	27.523712
249.177462	9261.503682	27.528730
249.627498	9284.313818	27.533748
249.933910	9294.436246	27.538765
249.962531	9318.984963	27.543783
250.114204	9333.260304	27.548800
250.705825	9354.554960	27.553818
250.509014	9375.055781	27.558836
251.058692	9389.755047	27.563853
251.105525	9413.936926	27.568871
251.625892	9423.082486	27.573888
251.834686	9453.472836	27.578906
252.082014	9473.045243	27.583924
252.753808	9473.615818	27.588941
253.015896	9496.931732	27.593959
253.682313	9501.008861	27.598976
253.812309	9513.220019	27.603994
253.928127	9527.053238	27.609012
254.553888	9519.863855	27.614029
254.923749	9530.760531	27.619047
255.072776	9545.208239	27.624064
255.250925	9556.052490	27.629082
255.151144	9554.453273	27.634100
255.206217	9550.457865	27.639117
255.171189	9581.917823	27.644135
255.393423	9593.071467	27.649152
255.805038	9610.538548	27.654170
255.907696	9635.022664	27.659188
256.225191	9650.472914	27.664205
256.325323	9675.102465	27.669223
256.744638	9684.747885	27.674240
256.874695	9707.280911	27.679258
256.694272	9727.765278	27.684276
257.175659	9748.269703	27.689293
257.390538	9784.825788	27.694311
257.573416	9800.681420	27.699328
258.007852	9832.427835	27.704346
257.847580	9854.249859	27.709364
258.450028	9867.351005	27.714381
258.685824	9896.083312	27.719399
259.237921	9922.374481	27.724416
259.589538	9941.871047	27.729434
259.862700	9957.874911	27.734452
260.131477	9968.991935	27.739469
260.710799	9990.397412	27.744487
260.753318	9993.092512	27.749504
261.475981	9999.285160	27.754522
261.869985	10009.343069	27.759540
262.128431	10009.210285	27.764557
262.170566	10034.429066	27.769575
262.363656	10051.316862	27.774592
262.763317	10043.997010	27.779610
262.805401	10051.995766	27.784628
263.191273	10062.847603	27.789645
263.163327	10075.087004	27.794663
263.455755	10088.977237	27.799680
263.694006	10095.100718	27.804698
263.970118	10108.087688	27.809716
264.173412	10123.931581	27.814733
264.627583	10142.781886	27.819751
264.410440	10149.857891	27.824768
264.845867	10169.079253	27.829786
264.596303	10177.388083	27.834804
265.156677	10191.488354	27.839821
265.306241	10215.068231	27.844839
265.548592	10239.649808	27.849856
266.124119	10258.185440	27.854874
266.088823	10275.314675	27.859892
266.524460	10286.695693	27.864909
267.324035	10300.044912	27.869927
267.501134	10316.343985	27.874944
267.900398	10332.226430	27.879962
268.254032	10349.495963	27.884980
268.945108	10334.722749	27.889997
269.001104	10344.069679	27.895015
269.555141	10361.547794	27.900032
270.215004	10355.313534	27.905050
270.180600	10364.843304	27.910068
271.068527	10346.862415	27.915085
271.525317	10336.784201	27.920103
271.839982	10323.410481	27.925120
272.348581	10321.971670	27.930138
272.478590	10321.532488	27.935156
272.167936	10296.808436	27.940173
272.107674	10288.335086	27.945191
272.412415	10288.398658	27.950208
272.622359	10298.988388	27.955226
272.197589	10321.911466	27.960244
272.419336	10319.903443	27.965261
272.981091	10338.038088	27.970279
272.807075	10356.480134	27.975296
273.056997	10367.203501	27.980314
272.925013	10390.194632	27.985332
273.380358	10411.466068	27.990349
273.627593	10432.029179	27.995367
273.874927	10449.240849	28.000384
274.261231	10457.872763	28.005402
274.246100	10486.414615	28.010420
274.953063	10508.793831	28.015437
275.319358	10529.166326	28.020455
275.132421	10553.406089	28.025472
275.821117	10573.034140	28.030490
275.739145	10591.525765	28.035508
275.943323	10615.664401	28.040525
276.178021	10635.208022	28.045543
276.055952	10655.827259	28.050560
276.609256	10680.697412	28.055578
276.745874	10708.531382	28.060596
277.237134	10721.532739	28.065613
277.999286	10740.561845	28.070631
278.116942	10779.668491	28.075648
278.760926	10783.768595	28.080666
278.709878	10806.660995	28.085684
278.907578	10809.064156	28.090701
279.549815	10845.608377	28.095719
279.344310	10859.852236	28.100736
279.891324	10878.413020	28.105754
279.704561	10902.221531	28.110772
280.103554	10925.127571	28.115789
280.551419	10936.778044	28.120807
280.430367	10958.735283	28.125824
280.991132	10977.610616	28.130842
281.186274	11006.480081	28.135860
281.586585	11024.351603	28.140877
281.847205	11048.681627	28.145895
282.133403	11068.056492	28.150912
282.689632	11085.322309	28.155930
282.744254	11104.929506	28.160948
282.967403	11122.923538	28.165965
283.355184	11141.525262	28.170983
283.543853	11155.699167	28.176000
284.145884	11166.208571	28.181018
284.442008	11191.213632	28.186036
285.012456	11206.650932	28.191053
284.933582	11218.680632	28.196071
285.299455	11237.004047	28.201088
285.710930	11246.785652	28.206106
285.714859	11262.306093	28.211124
285.955444	11284.644903	28.216141
286.530257	11311.738995	28.221159
286.460001	11333.456666	28.226176
287.150594	11344.354868	28.231194
287.629391	11358.345236	28.236212
288.320051	11363.063314	28.241229
288.965615	11363.064758	28.246247
289.172718	11366.938201	28.251264
289.441357	11358.152799	28.256282
289.132699	11373.767823	28.261300
289.509856	11388.944319	28.266317
289.865700	11400.051021	28.271335
289.986628	11424.444214	28.276352
290.357969	11424.888309	28.281370
290.308843	11441.180406	28.286388
290.434455	11453.990981	28.291405
290.575197	11471.430240	28.296423
291.245224	11503.743546	28.301440
291.633065	11519.080694	28.306458
291.753268	11533.839889	28.311476
291.881140	11557.165328	28.316493
292.120267	11572.115954	28.321511
292.153148	11607.847609	28.326528
292.716809	11620.791969	28.331546
292.923793	11644.558217	28.336564
292.838568	11666.526220	28.341581
293.267952	11687.806807	28.346599
293.166833	11725.206108	28.351616
293.521311	11750.890963	28.356634
293.746208	11784.841972	28.361652
294.187244	11812.181317	28.366669
295.157830	11837.994023	28.371687
296.385998	11832.862407	28.376704
297.355983	11829.327430	28.381722
298.555789	11818.330659	28.386740
298.935325	11799.657339	28.391757
299.446885	11782.320447	28.396775
299.373809	11774.021784	28.401792
299.539128	11746.225569	28.406810
299.781147	11733.101492	28.411828
299.328714	11729.434106	28.416845
299.469422	11724.349243	28.421863
299.439220	11727.664971	28.426880
299.619695	11722.562471	28.431898
299.933561	11731.782272	28.436916
300.122026	11730.755025	28.441933
300.133668	11743.723434	28.446951
300.075452	11753.920600	28.451968
300.532191	11757.812547	28.456986
300.635064	11778.175231	28.462004
300.243655	11790.498375	28.467021
300.753475	11816.335594	28.472039
300.627037	11840.505775	28.477056
300.756863	11869.212718	28.482074
301.088629	11912.832744	28.487092
300.993519	11938.238030	28.492109
301.599884	11972.392374	28.497127
301.805873	12009.859498	28.502144
301.903801	12043.802205	28.507162
302.347567	12081.617646	28.512180
302.323191	12130.414140	28.517197
302.811253	12167.760704	28.522215
302.795317	12205.692199	28.527232
303.127024	12243.961567	28.532250
303.746152	12267.923426	28.537268
304.671678	12302.977256	28.542285
305.779017	12308.480508	28.547303
306.537260	12324.338376	28.552320
307.138892	12330.450407	28.557338
307.424877	12350.375243	28.562356
307.703284	12379.860515	28.567373
308.182840	12369.080739	28.572391
308.083753	12391.375076	28.577408
308.317097	12401.024663	28.582426
308.686280	12396.467368	28.587444
308.502835	12419.371432	28.592461
308.848672	12432.245475	28.597479
309.190202	12463.020500	28.602496
309.377350	12484.030356	28.607514
309.605917	12495.953196	28.612532
309.686759	12517.663108	28.617549
310.381255	12532.726502	28.622567
310.460517	12568.685796	28.627584
310.710503	12582.444189	28.632602
311.133293	12605.938038	28.637620
311.119350	12638.286869	28.642637
311.387951	12654.442301	28.647655
311.624921	12690.968198	28.652672
312.291671	12724.371852	28.657690
312.368409	12734.518846	28.662708
312.555556	12767.070910	28.667725
313.306270	12795.183087	28.672743
313.183292	12832.684696	28.677760
313.586127	12858.224593	28.682778
314.527247	12871.977154	28.687796
314.966166	12882.582545	28.692813
315.374120	12904.057401	28.697831
315.455734	12926.525743	28.702848
315.762755	12946.723600	28.707866
316.093750	12948.944198	28.712884
316.047797	12979.325980	28.717901
316.506200	13004.475504	28.722919
316.783481	13035.371024	28.727936
317.101386	13056.946141	28.732954
317.477506	13080.040264	28.737972
317.675704	13100.344642	28.742989
317.955385	13124.562727	28.748007
318.395294	13152.266984	28.753024
318.436071	13180.374844	28.758042
319.100135	13196.101078	28.763060
319.463749	13218.603347	28.768077
320.182105	13225.454357	28.773095
320.244515	13249.305281	28.778112
321.069139	13265.302762	28.783130
322.027043	13263.783557	28.788148
322.286402	13261.924950	28.793165
322.800034	13254.212024	28.798183
323.075040	13254.443671	28.803200
322.977319	13260.396448	28.808218
322.977160	13258.563618	28.813236
323.091600	13264.147052	28.818253
323.853799	13271.246103	28.823271
323.456372	13298.055891	28.828288
323.907450	13296.040931	28.833306
324.337647	13303.716788	28.838324
323.784398	13333.975480	28.843341
324.413351	13350.536647	28.848359
324.734497	13383.887179	28.853376
324.770479	13398.435122	28.858394
325.283251	13414.306474	28.863412
325.403571	13456.167598	28.868429
325.649364	13473.589980	28.873447
325.501044	13516.469831	28.878464
325.628095	13550.535341	28.883482
326.316916	13579.905753	28.888500
326.469823	13622.863496	28.893517
326.869060	13653.263981	28.898535
327.408136	13695.625082	28.903552
327.737813	13726.153882	28.908570
328.295068	13750.909902	28.913588
328.451513	13777.615855	28.918605
329.502931	13800.148083	28.923623
330.198553	13808.501893	28.928640
330.888117	13825.718547	28.933658
331.474909	13829.772213	28.938676
331.443769	13854.210072	28.943693
331.709455	13857.207584	28.948711
332.009806	13879.306787	28.953728
332.373455	13894.749493	28.958746
332.626170	13908.109826	28.963764
332.811878	13935.670100	28.968781
333.340466	13952.291107	28.973799
333.135371	13979.919528	28.978816
333.381276	13997.831015	28.983834
334.040585	14009.795307	28.988852
334.339972	14031.437832	28.993869
335.155190	14042.886108	28.998887
336.309868	14025.197306	29.003904
336.716153	14015.952635	29.008922
337.645449	14007.755816	29.013940
337.702840	14004.132445	29.018957
338.074228	14003.060491	29.023975
338.539299	13994.485328	29.028992
338.282693	14001.927310	29.034010
338.598014	13994.311600	29.039028
338.601613	14002.648086	29.044045
338.495792	14023.265736	29.049063
338.725630	14036.209179	29.054080
339.004452	14052.329630	29.059098
339.054599	14059.522102	29.064116
339.259434	14102.338518	29.069133
339.669628	14114.421497	29.074151
339.820266	14136.162945	29.079168
339.528297	14165.295457	29.084186
339.787234	14192.478360	29.089204
340.216652	14228.796064	29.094221
340.133204	14263.265244	29.099239
340.399682	14300.015215	29.104256
340.908201	14341.632872	29.109274
341.330460	14378.707024	29.114292
341.623958	14421.793235	29.119309
342.111252	14462.725990	29.124327
342.331178	14497.266621	29.129344
342.717631	14531.872649	29.134362
343.607236	14551.015892	29.139380
343.921203	14595.142515	29.144397
344.410408	14610.276620	29.149415
344.539133	14643.913860	29.154432
344.572907	14667.743238	29.159450
345.214313	14690.073729	29.164468
345.459044	14720.207139	29.169485
345.899671	14752.224585	29.174503
346.342468	14773.103508	29.179520
346.360493	14802.688424	29.184538
347.112117	14819.399353	29.189556
347.253340	14865.192959	29.194573
347.827060	14887.534963	29.199591
348.079075	14925.869567	29.204608
347.975517	14961.478346	29.209626
348.896476	14983.795898	29.214644
349.014674	15010.154013	29.219661
349.287978	15043.154945	29.224679
349.669837	15074.651631	29.229696
349.944458	15107.423936	29.234714
350.850467	15125.967781	29.239732
351.249824	15151.150913	29.244749
351.561629	15158.193224	29.249767
352.616988	15187.794074	29.254784
352.959622	15196.847150	29.259802
354.019499	15194.776546	29.264820
354.626519	15203.397979	29.269837
354.843826	15202.993032	29.274855
355.245656	15195.116525	29.279872
355.079081	15222.836779	29.284890
355.598926	15226.531532	29.289908
355.705815	15238.301640	29.294925
355.864348	15248.584764	29.299943
356.114621	15261.212131	29.304960
356.244828	15287.010743	29.309978
356.842990	15294.163159	29.314996
356.830350	15318.771924	29.320013
356.523638	15340.553113	29.325031
357.200853	15358.536295	29.330048
357.305965	15395.276120	29.335066
357.928469	15416.994471	29.340084
358.094801	15450.239380	29.345101
358.377984	15476.789923	29.350119
358.749643	15525.537057	29.355136
358.568330	15558.917166	29.360154
359.348076	15588.551917	29.365172
359.811216	15628.022603	29.370189
360.001545	15660.329281	29.375207
360.370978	15688.256022	29.380224
360.448516	15735.848437	29.385242
360.999278	15764.359896	29.390260
361.478826	15805.740194	29.395277
361.381994	15845.572372	29.400295
362.034300	15867.833307	29.405312
362.748194	15910.405946	29.410330
363.521305	15925.123702	29.415348
363.841038	15957.529257	29.420365
363.594203	15990.175577	29.425383
364.491470	16016.628134	29.430400
365.014589	16035.439947	29.435418
365.696778	16061.324616	29.440436
366.051755	16081.687033	29.445453
366.639522	16103.038499	29.450471
367.680510	16112.248761	29.455488
368.001782	16117.013856	29.460506
368.953032	16102.097691	29.465524
369.168382	16114.140433	29.470541
369.421269	16119.473293	29.475559
370.155611	16111.079288	29.480576
369.816658	16110.517681	29.485594
370.191270	16100.501613	29.490612
370.288233	16105.849336	29.495629
370.500532	16111.940791	29.500647
370.794890	16128.484706	29.505664
370.666760	16135.917337	29.510682
371.109615	16151.360050	29.515700
371.558661	16176.177122	29.520717
371.487835	16197.754753	29.525735
372.167382	16217.745027	29.530752
371.949153	16255.271848	29.535770
372.193035	16267.844305	29.540788
372.616670	16304.720817	29.545805
372.265469	16339.057548	29.550823
373.064747	16371.890234	29.555840
373.116885	16413.584221	29.560858
373.737965	16456.782122	29.565876
373.706204	16485.681626	29.570893
374.082803	16536.615614	29.575911
374.286958	16567.714357	29.580928
374.577376	16619.408487	29.585946
375.153564	16661.394351	29.590964
375.450314	16711.030683	29.595981
375.565071	16751.127809	29.600999
376.588855	16802.035500	29.606016
376.773190	16848.905627	29.611034
377.439514	16884.797347	29.616052
378.335157	16919.916501	29.621069
378.376578	16956.856379	29.626087
379.400607	16987.545448	29.631104
380.263391	16999.700398	29.636122
380.796491	17011.478213	29.641140
381.503406	17035.900652	29.646157
381.581098	17059.559100	29.651175
382.186047	17061.693783	29.656192
382.468645	17088.395188	29.661210
382.619719	17106.172913	29.666228
383.182522	17113.347768	29.671245
383.346239	17147.392564	29.676263
383.895563	17157.843685	29.681280
384.581690	17188.778415	29.686298
384.768597	17194.420509	29.691316
385.272200	17211.484041	29.696333
385.106969	17233.282044	29.701351
385.646155	17242.432860	29.706368
385.987818	17274.537854	29.711386
386.359130	17292.654362	29.716404
386.572791	17314.824603	29.721421
386.842606	17340.469243	29.726439
387.214344	17366.759055	29.731456
387.465707	17393.756187	29.736474
387.461990	17422.799263	29.741492
387.868566	17454.168705	29.746509
387.881751	17500.958760	29.751527
388.309611	17534.544318	29.756544
388.783056	17574.557056	29.761562
389.022984	17595.961929	29.766580
389.826945	17639.214511	29.771597
389.839355	17685.656838	29.776615
390.561905	17722.192075	29.781632
391.010020	17764.769504	29.786650
391.215343	17801.745514	29.791668
391.724054	17834.340895	29.796685
392.039786	17869.850023	29.801703
392.873119	17900.359654	29.806720
393.104637	17923.777816	29.811738
394.031610	17948.983198	29.816756
395.179065	17964.720433	29.821773
395.242687	17979.493251	29.826791
395.560884	17991.723632	29.831808
395.874639	17990.968410	29.836826
396.379073	18017.963930	29.841844
397.168704	18024.314885	29.846861
397.572009	18039.039215	29.851879
397.731841	18049.981227	29.856896
397.960984	18057.372712	29.861914
397.943779	18082.167624	29.866932
398.545648	18094.507026	29.871949
398.041012	18120.883698	29.876967
398.427037	18154.018723	29.881984
398.970130	18180.316042	29.887002
398.891576	18222.646349	29.892020
399.434940	18252.383480	29.897037
399.431238	18299.358294	29.902055
399.637086	18336.999081	29.907072
400.237956	18380.837503	29.912090
400.490347	18425.463814	29.917108
401.353370	18465.874307	29.922125
401.397156	18529.541121	29.927143
402.159177	18561.170477	29.932160
402.546236	18600.449643	29.937178
402.682531	18649.065344	29.942196
403.073400	18684.735563	29.947213
403.694555	18734.327205	29.952231
404.574993	18764.646154	29.957248
404.879516	18796.099714	29.962266
405.592929	18834.076656	29.967284
406.491298	18857.520943	29.972301
406.931515	18871.016534	29.977319
407.856454	18886.435328	29.982336
408.933106	18893.453095	29.987354
409.495219	18921.525120	29.992372
409.797889	18917.084307	29.997389
410.126295	18921.823810	30.002407
410.875672	18903.900817	30.007424
411.257127	18908.579481	30.012442
411.504216	18931.690637	30.017460
412.214277	18936.875956	30.022477
412.393893	18924.516405	30.027495
412.456795	18939.591302	30.032512
412.663715	18943.974210	30.037530
412.892462	18963.218186	30.042548
413.245717	18983.057910	30.047565
413.384967	19000.760800	30.052583
413.567373	19019.523825	30.057600
413.550756	19034.530037	30.062618
414.025529	19086.349405	30.067636
414.845396	19106.247351	30.072653
414.832868	19130.770308	30.077671
415.137925	19176.912783	30.082688
415.282844	19211.277068	30.087706
415.405337	19248.842319	30.092724
415.841774	19279.081458	30.097741
415.671005	19322.774635	30.102759
416.277982	19368.350389	30.107776
416.754970	19412.658258	30.112794
417.129168	19459.612975	30.117812
417.850551	19499.942300	30.122829
418.147234	19543.232065	30.127847
418.790354	19589.690012	30.132864
419.196012	19631.147299	30.137882
419.903772	19672.412620	30.142900
420.339472	19693.927984	30.147917
420.829965	19734.704553	30.152935
421.217580	19759.182461	30.157952
422.039811	19786.534815	30.162970
422.007064	19823.014082	30.167988
422.512543	19851.112844	30.173005
422.804966	19880.831496	30.178023
423.278628	19901.831589	30.183040
423.953428	19930.539297	30.188058
424.049963	19973.459812	30.193076
425.010936	19991.899114	30.198093
425.224250	20032.068163	30.203111
425.421408	20072.268370	30.208128
425.866197	20096.385694	30.213146
426.062362	20141.457906	30.218164
426.398799	20169.429196	30.223181
426.604278	20208.486887	30.228199
427.060848	20252.835053	30.233216
427.511127	20299.424747	30.238234
427.382033	20343.045858	30.243252
428.133282	20368.493788	30.248269
428.907990	20418.764938	30.253287
429.755008	20440.443131	30.258304
430.488348	20466.669885	30.263322
430.954302	20511.166954	30.268340
431.330351	20548.634662	30.273357
431.726363	20574.055193	30.278375
432.312822	20611.210605	30.283392
432.775779	20623.060976	30.288410
433.078995	20665.794418	30.293428
433.775330	20691.193624	30.298445
434.096432	20722.864048	30.303463
434.867501	20753.198471	30.308480
435.247258	20773.519949	30.313498
435.091069	20814.176357	30.318516
435.646354	20847.840437	30.323533
436.080380	20877.004419	30.328551
436.150564	20903.908027	30.333568
436.770865	20942.080230	30.338586
437.028356	20992.057447	30.343604
437.495572	21019.280003	30.348621
437.506395	21069.829761	30.353639
437.874059	21110.967481	30.358656
438.482747	21159.529333	30.363674
438.826158	21197.254599	30.368692
439.577301	21232.482534	30.373709
439.938589	21281.204080	30.378727
441.173383	21315.079457	30.383744
442.108800	21337.277057	30.388762
442.317593	21369.501854	30.393780
442.776208	21396.951920	30.398797
443.105553	21425.620230	30.403815
443.563237	21461.378284	30.408832
443.937580	21475.662667	30.413850
444.068588	21515.916723	30.418868
444.150421	21540.809083	30.423885
444.878675	21585.260693	30.428903
445.113910	21619.195483	30.433920
445.444253	21666.963050	30.438938
445.464640	21707.433025	30.443956
446.221430	21749.863673	30.448973
446.634098	21794.355634	30.453991
446.807484	21828.928664	30.459008
447.378930	21862.298809	30.464026
448.265944	21903.530375	30.469044
448.900044	21932.891584	30.474061
449.441381	21975.492608	30.479079
449.838190	22016.127856	30.484096
450.639101	22045.614503	30.489114
450.884191	22078.101097	30.494132
451.416959	22096.095082	30.499149
451.650518	22129.778889	30.504167
451.653852	22161.455909	30.509184
452.666151	22174.685703	30.514202
452.595550	22212.638099	30.519220
453.266828	22246.143793	30.524237
453.524719	22285.136088	30.529255
453.625932	22326.532312	30.534272
454.161171	22367.415044	30.539290
454.104544	22412.013378	30.544308
454.732070	22458.343071	30.549325
455.528711	22495.459840	30.554343
455.921305	22535.849474	30.559360
456.945091	22567.873388	30.564378
457.238173	22605.829332	30.569396
457.867966	22635.995083	30.574413
458.418471	22666.196132	30.579431
458.960045	22703.116041	30.584448
459.636023	22727.775857	30.589466
460.241421	22748.735548	30.594484
461.027938	22779.903627	30.599501
461.437828	22805.894455	30.604519
461.741183	22838.560472	30.609536
461.833125	22860.980592	30.614554
462.811327	22892.370915	30.619572
463.417283	22911.943084	30.624589
463.933768	22938.473042	30.629607
464.173018	22971.660865	30.634624
464.267993	22998.227808	30.639642
464.251107	23043.224873	30.644660
464.700251	23068.121544	30.649677
464.903532	23108.985508	30.654695
464.957232	23166.499444	30.659712
465.556245	23206.946273	30.664730
466.049244	23262.578888	30.669748
466.422857	23295.845948	30.674765
466.858710	23353.959341	30.679783
467.086690	23403.428190	30.684800
467.750846	23455.191676	30.689818
468.127865	23512.891194	30.694836
468.783213	23562.693215	30.699853
469.175906	23613.646003	30.704871
469.786714	23668.397800	30.709888
470.902562	23701.862495	30.714906
471.024491	23755.270223	30.719924
471.264264	23796.101386	30.724941
472.333612	23833.003903	30.729959
472.692005	23875.162262	30.734976
473.416034	23910.173194	30.739994
473.521619	23963.330397	30.745012
473.952626	23995.621041	30.750029
474.849014	24031.688542	30.755047
475.315317	24071.845651	30.760064
476.076615	24107.897903	30.765082
476.501188	24154.757938	30.770100
476.832162	24193.089597	30.775117
477.278196	24223.233491	30.780135
477.505734	24264.976146	30.785152
477.852548	24299.599509	30.790170
478.608166	24344.676709	30.795188
478.759993	24391.122209	30.800205
479.695901	24427.571925	30.805223
479.765780	24467.641256	30.810240
480.537806	24505.912983	30.815258
481.079287	24547.496950	30.820276
481.529632	24585.238787	30.825293
482.046011	24626.290931	30.830311
482.678572	24651.847033	30.835328
483.462574	24665.417916	30.840346
484.426434	24689.225335	30.845364
485.132317	24705.218911	30.850381
485.409820	24715.940694	30.855399
485.698888	24731.432637	30.860416
486.425347	24757.796510	30.865434
486.773456	24773.726561	30.870452
487.228752	24787.550839	30.875469
487.703120	24812.335478	30.880487
488.155755	24830.676851	30.885504
488.536550	24852.900217	30.890522
488.219473	24884.588192	30.895540
488.644392	24930.813171	30.900557
488.952910	24957.098521	30.905575
489.239772	24993.584696	30.910592
489.747654	25035.440374	30.915610
490.104395	25085.373702	30.920628
490.445752	25128.146722	30.925645
490.755203	25179.166885	30.930663
490.821814	25241.598205	30.935680
491.652727	25295.216284	30.940698
492.287184	25339.606544	30.945716
492.389386	25397.190884	30.950733
493.039631	25447.095444	30.955751
493.459224	25517.688934	30.960768
494.044745	25563.500977	30.965786
494.837152	25618.549005	30.970804
494.898532	25674.075042	30.975821
495.897151	25732.167706	30.980839
496.287158	25792.105937	30.985856
496.923355	25838.380279	30.990874
497.945249	25880.632097	30.995892
498.582668	25917.926280	31.000909
499.551135	25967.044556	31.005927
499.381420	26003.179717	31.010944
499.930464	26041.741094	31.015962
500.253682	26098.155527	31.020980
500.573981	26144.158261	31.025997
501.542362	26189.895771	31.031015
501.756705	26235.969970	31.036032
502.124482	26288.633444	31.041050
502.763666	26339.958724	31.046068
503.133729	26385.392363	31.051085
503.816897	26434.720226	31.056103
504.222000	26483.126019	31.061120
504.504014	26527.640962	31.066138
505.170517	26576.886831	31.071156
505.999696	26626.345558	31.076173
506.564241	26678.908146	31.081191
507.225676	26712.667130	31.086208
508.365900	26747.034328	31.091226
509.135474	26776.554871	31.096244
509.308176	26810.269034	31.101261
509.951565	26846.766166	31.106279
510.134541	26884.163146	31.111296
510.575420	26915.038142	31.116314
511.132159	26958.038597	31.121332
511.597405	27008.218139	31.126349
512.231365	27031.105722	31.131367
512.594336	27076.731624	31.136384
513.058101	27111.678754	31.141402
513.431681	27149.975227	31.146420
513.446336	27203.731649	31.151437
514.129196	27244.850717	31.156455
514.600502	27291.556962	31.161472
514.957115	27342.493669	31.166490
515.707840	27392.519660	31.171508
515.946472	27437.192409	31.176525
516.880812	27465.910750	31.181543
517.193246	27498.218200	31.186560
517.740865	27540.152222	31.191578
518.929015	27564.494213	31.196596
519.202785	27604.057472	31.201613
520.016107	27626.158960	31.206631
520.408685	27672.831988	31.211648
520.645142	27706.373267	31.216666
520.925845	27746.345796	31.221684
521.227141	27792.892348	31.226701
521.328145	27833.320791	31.231719
521.648918	27878.911646	31.236736
522.400395	27938.753119	31.241754
522.681504	27979.798691	31.246772
523.182787	28037.347619	31.251789
523.823488	28089.390786	31.256807
524.727990	28141.809870	31.261824
524.913758	28198.345450	31.266842
525.460797	28245.931304	31.271860
525.510576	28315.452464	31.276877
526.133896	28366.653887	31.281895
526.637153	28435.346241	31.286912
527.196786	28502.199757	31.291930
528.180817	28547.404600	31.296948
528.643380	28611.031579	31.301965
529.262798	28672.815597	31.306983
529.858398	28719.195869	31.312000
530.393068	28784.827408	31.317018
530.934247	28833.942757	31.322036
531.543947	28882.952221	31.327053
532.287238	28934.173245	31.332071
533.294810	28966.456317	31.337088
533.872647	29012.420728	31.342106
534.657296	29059.067063	31.347124
534.981704	29115.074659	31.352141
535.443111	29146.152122	31.357159
536.246614	29187.344089	31.362176
536.810388	29224.231714	31.367194
537.716945	29266.829600	31.372212
538.209241	29306.786341	31.377229
538.853830	29345.569506	31.382247
538.978683	29387.903138	31.387264
539.460860	29422.501661	31.392282
540.475541	29458.276940	31.397300
540.767501	29508.120187	31.402317
540.992797	29546.427625	31.407335
541.622014	29584.854212	31.412352
541.944154	29629.401976	31.417370
542.560808	29670.746000	31.422388
543.282428	29726.960917	31.427405
543.855486	29753.108655	31.432423
544.579801	29803.565570	31.437440
544.904586	29841.226138	31.442458
545.604424	29874.309725	31.447476
546.013767	29913.726352	31.452493
546.338973	29954.844962	31.457511
546.981575	30000.457321	31.462528
547.228665	30040.812973	31.467546
547.854105	30077.619594	31.472564
548.570783	30141.519132	31.477581
548.818383	30189.690051	31.482599
549.308344	30237.486420	31.487616
549.426251	30284.584335	31.492634
550.149404	30339.728243	31.497652
550.463871	30399.537136	31.502669
551.117254	30453.869515	31.507687
551.556445	30510.414645	31.512704
551.894331	30570.684030	31.517722
552.469742	30620.025871	31.522740
552.974952	30676.582658	31.527757
553.956387	30728.763251	31.532775
554.453301	30779.847590	31.537792
554.543440	30834.129538	31.542810
555.576504	30885.352322	31.547828
555.909798	30936.549475	31.552845
556.579720	30981.579293	31.557863
557.201040	31024.121544	31.562880
558.111784	31088.945164	31.567898
559.150881	31123.760614	31.572916
559.332614	31178.858232	31.577933
559.790926	31222.431389	31.582951
560.343795	31278.695069	31.587968
560.495006	31313.853960	31.592986
561.020382	31367.894892	31.598004
561.295290	31434.888902	31.603021
561.809059	31497.615437	31.608039
562.353083	31549.000242	31.613056
562.646686	31617.115118	31.618074
563.349724	31683.893834	31.623092
563.633102	31756.191722	31.628109
564.241003	31817.423915	31.633127
565.013572	31894.228982	31.638144
565.310998	31957.040400	31.643162
566.314556	32018.576764	31.648180
567.149434	32095.337648	31.653197
567.698506	32152.018091	31.658215
567.887423	32216.464006	31.663232
568.719135	32293.219961	31.668250
569.231484	32355.889819	31.673268
569.600895	32426.298674	31.678285
570.279154	32479.964204	31.683303
571.656555	32532.311571	31.688320
572.220718	32588.454476	31.693338
573.378470	32636.660790	31.698356
574.125858	32675.948566	31.703373
574.578054	32729.737589	31.708391
575.612142	32761.950672	31.713408
575.931085	32823.404720	31.718426
576.634775	32856.389139	31.723444
577.123442	32896.891061	31.728461
577.845017	32932.551689	31.733479
579.166676	32962.742027	31.738496
579.248207	33002.011717	31.743514
579.834430	33023.567661	31.748532
580.251591	33068.363921	31.753549
580.970739	33105.154986	31.758567
581.878519	33144.505524	31.763584
581.898481	33193.700645	31.768602
582.394539	33232.255117	31.773620
582.482207	33279.962423	31.778637
582.736165	33331.984344	31.783655
583.033108	33378.571637	31.788672
583.492826	33439.215533	31.793690
584.059099	33504.420757	31.798708
584.358537	33577.562783	31.803725
584.838542	33634.994689	31.808743
585.580491	33699.934782	31.813760
585.996099	33780.003961	31.818778
586.736459	33828.342778	31.823796
587.657414	33897.930594	31.828813
588.498027	33952.129010	31.833831
588.988788	34007.487029	31.838848
589.646967	34070.839277	31.843866
590.798323	34102.202211	31.848884
592.324713	34127.980384	31.853901
593.242541	34168.410780	31.858919
594.211716	34185.211954	31.863936
594.331812	34224.159196	31.868954
594.966091	34243.676336	31.873972
595.454496	34269.734368	31.878989
595.906190	34281.928941	31.884007
596.558561	34321.545397	31.889024
596.683232	34354.846489	31.894042
596.857786	34396.420139	31.899060
597.322406	34429.317785	31.904077
597.354987	34480.824391	31.909095
597.851495	34523.424159	31.914112
597.989305	34589.698569	31.919130
598.402709	34649.969253	31.924148
599.095175	34712.784748	31.929165
599.368234	34786.381068	31.934183
599.975906	34841.185758	31.939200
600.353639	34921.007548	31.944218
600.774620	34990.108263	31.949236
601.269240	35075.465696	31.954253
601.703618	35159.580637	31.959271
602.274766	35221.913110	31.964288
602.551475	35328.023460	31.969306
603.333806	35400.833955	31.974324
603.886563	35502.676821	31.979341
604.738383	35584.319575	31.984359
605.677131	35659.443735	31.989376
606.401603	35741.461821	31.994394
607.114368	35822.525945	31.999412
608.363995	35894.080485	32.004429
608.902249	35961.110866	32.009447
610.041734	36025.671457	32.014464
610.460942	36076.796509	32.019482
611.408122	36120.417234	32.024500
612.452856	36184.277695	32.029517
612.867288	36245.778118	32.034535
613.740782	36293.451317	32.039552
613.948324	36358.341429	32.044570
614.892107	36408.584975	32.049588
615.284560	36478.519885	32.054605
615.863407	36540.577898	32.059623
616.665550	36592.297309	32.064640
616.879026	36654.141792	32.069658
617.255815	36710.180385	32.074676
618.222353	36775.971730	32.079693
618.515493	36840.625267	32.084711
619.540591	36895.786672	32.089728
620.008021	36960.799913	32.094746
621.185341	37009.803831	32.099764
621.820702	37067.804811	32.104781
622.166854	37131.358519	32.109799
623.199641	37185.257026	32.114816
623.302869	37246.910366	32.119834
623.535572	37297.214482	32.124852
624.876814	37350.932858	32.129869
625.472897	37417.747562	32.134887
626.483851	37458.450812	32.139904
626.687360	37510.862476	32.144922
627.154526	37565.714552	32.149940
627.666255	37630.577646	32.154957
627.949885	37702.283960	32.159975
628.856191	37758.149491	32.164992
629.160991	37829.246768	32.170010
629.256900	37887.630323	32.175028
630.251949	37963.704781	32.180045
630.861960	38041.469045	32.185063
631.196876	38103.781230	32.190080
631.353985	38189.667071	32.195098
632.157976	38269.281340	32.200116
632.668931	38339.355246	32.205133
633.293439	38407.210498	32.210151
634.165207	38476.044496	32.215168
635.013327	38553.187454	32.220186
635.344093	38611.767912	32.225204
636.442027	38671.666871	32.230221
637.162158	38734.794765	32.235239
638.394364	38785.580970	32.240256
638.800613	38853.808715	32.245274
639.233599	38902.395245	32.250292
639.956563	38959.724830	32.255309
640.513611	39036.009062	32.260327
641.258691	39095.314583	32.265344
641.716756	39163.702181	32.270362
642.158380	39226.903270	32.275380
643.084453	39293.875238	32.280397
643.528897	39381.704491	32.285415
643.900282	39441.054239	32.290432
644.809648	39516.338132	32.295450
645.125993	39591.585058	32.300468
645.827666	39653.683793	32.305485
646.829319	39720.711064	32.310503
648.566264	39761.191598	32.315520
649.452553	39820.993726	32.320538
649.947611	39873.019671	32.325556
650.893017	39920.718856	32.330573
651.602782	39972.441112	32.335591
651.944470	40022.153790	32.340608
652.591830	40074.041375	32.345626
653.261724	40126.386255	32.350644
653.817515	40167.079584	32.355661
654.329081	40241.071924	32.360679
654.874080	40286.644565	32.365696
655.652827	40351.791813	32.370714
655.745472	40420.292114	32.375732
656.652057	40483.837032	32.380749
656.712105	40557.498376	32.385767
657.494962	40622.371252	32.390784
657.650776	40702.564614	32.395802
658.205619	40782.205910	32.400820
658.846697	40846.620111	32.405837
659.503855	40932.590445	32.410855
660.152100	41005.660281	32.415872
660.845986	41094.267620	32.420890
661.324470	41184.224443	32.425908
662.238865	41260.228110	32.430925
662.823277	41358.909857	32.435943
663.770968	41432.158965	32.440960
664.849441	41493.178476	32.445978
665.611214	41558.430669	32.450996
668.098430	41578.983498	32.456013
670.444016	41606.104394	32.461031
672.024699	41608.206542	32.466048
672.580616	41612.360420	32.471066
673.247018	41620.268613	32.476084
673.957339	41618.714196	32.481101
673.999371	41631.464766	32.486119
674.515469	41651.085282	32.491136
675.131943	41669.868322	32.496154
675.341387	41687.058353	32.501172
675.789571	41710.361853	32.506189
676.028289	41746.618831	32.511207
676.129249	41773.645402	32.516224
676.320539	41824.606532	32.521242
676.558948	41871.288452	32.526260
677.338894	41926.748837	32.531277
677.548438	41984.735054	32.536295
677.953633	42042.193302	32.541312
678.500768	42098.699971	32.546330
678.701288	42147.804071	32.551348
679.202259	42217.341909	32.556365
679.362913	42292.568861	32.561383
679.955928	42366.673000	32.566400
680.313021	42445.321892	32.571418
680.449444	42532.058585	32.576436
681.234282	42624.370997	32.581453
681.808671	42723.737310	32.586471
682.508655	42813.687360	32.591488
683.405896	42903.980808	32.596506
684.018913	42998.221108	32.601524
684.723996	43089.292471	32.606541
685.390593	43194.442758	32.611559
685.875311	43287.035603	32.616576
686.843463	43386.330599	32.621594
687.380469	43489.783315	32.626612
688.059715	43571.452412	32.631629
688.854654	43684.247073	32.636647
689.741920	43777.747990	32.641664
690.319296	43871.193470	32.646682
690.958768	43984.805106	32.651700
691.967706	44067.473058	32.656717
692.525933	44163.531227	32.661735
693.051017	44267.176504	32.666752
694.200166	44353.557742	32.671770
694.736118	44459.532509	32.676788
695.471886	44553.242423	32.681805
696.077792	44660.018192	32.686823
697.082959	44758.565975	32.691840
697.849309	44844.978292	32.696858
698.282707	44945.778607	32.701876
699.290975	45042.379125	32.706893
699.447162	45145.209509	32.711911
700.339801	45246.800381	32.716928
700.986620	45355.849964	32.721946
701.515260	45451.824890	32.726964
702.530548	45548.420520	32.731981
703.599526	45643.728858	32.736999
704.247226	45740.383338	32.742016
705.359617	45830.715148	32.747034
706.525959	45914.789228	32.752052
707.421404	45996.774002	32.757069
708.314782	46082.460401	32.762087
708.966003	46162.408616	32.767104
710.136138	46221.906296	32.772122
710.364258	46311.964063	32.777140
711.028922	46383.441696	32.782157
711.978913	46463.597366	32.787175
713.122778	46540.929639	32.792192
713.829195	46614.684348	32.797210
714.298924	46687.490218	32.802228
714.864596	46762.437285	32.807245
715.597628	46836.027382	32.812263
716.129859	46905.842645	32.817280
717.225817	46981.046753	32.822298
718.028048	47056.205184	32.827316
719.082586	47120.471277	32.832333
719.910377	47181.727790	32.837351
720.449246	47254.998052	32.842368
721.615464	47319.590499	32.847386
722.156993	47381.049919	32.852404
722.944741	47440.687544	32.857421
723.566774	47506.413112	32.862439
724.399996	47549.757614	32.867456
726.288096	47591.635457	32.872474
727.223460	47639.403408	32.877492
727.682878	47675.856242	32.882509
728.140615	47711.324112	32.887527
728.777434	47758.450310	32.892544
729.521136	47795.573059	32.897562
729.596704	47849.484609	32.902580
730.191070	47893.406422	32.907597
730.606435	47949.238805	32.912615
731.035400	48007.595578	32.917632
731.507674	48071.162546	32.922650
731.757696	48149.451914	32.927668
732.208926	48216.158880	32.932685
732.587705	48295.390703	32.937703
732.809198	48390.487173	32.942720
733.560603	48483.746510	32.947738
733.752963	48584.359809	32.952756
734.420288	48689.297341	32.957773
735.440874	48776.178031	32.962791
736.841196	48856.051093	32.967808
737.853249	48947.529224	32.972826
738.682973	49043.266991	32.977844
739.611277	49127.780096	32.982861
740.422213	49208.952623	32.987879
741.075505	49309.818509	32.992896
742.197294	49382.362171	32.997914
742.817289	49473.456251	33.002932
743.726877	49540.666549	33.007949
744.393351	49618.930675	33.012967
745.160431	49713.020874	33.017984
746.200218	49786.331370	33.023002
747.146818	49864.553150	33.028020
747.821812	49941.414838	33.033037
748.403807	50028.598248	33.038055
748.772504	50115.861680	33.043072
749.656072	50201.021774	33.048090
750.032310	50297.264292	33.053108
750.346887	50382.282754	33.058125
751.277721	50481.861092	33.063143
751.622803	50587.727895	33.068160
752.396916	50682.620758	33.073178
752.813115	50794.465484	33.078196
753.585015	50906.296028	33.083213
754.633666	51015.895525	33.088231
754.951679	51110.664048	33.093248
756.013110	51215.050836	33.098266
756.915306	51327.310703	33.103284
758.105892	51432.245777	33.108301
758.900016	51526.507714	33.113319
759.739980	51621.760646	33.118336
760.630030	51710.126057	33.123354
761.338305	51814.321994	33.128372
761.960012	51902.941302	33.133389
762.832649	52015.942879	33.138407
763.343204	52107.923539	33.143424
764.204255	52214.073646	33.148442
764.708565	52312.872983	33.153460
765.640890	52413.617100	33.158477
767.045477	52509.917824	33.163495
767.896605	52599.165567	33.168512
768.372249	52698.925590	33.173530
768.804831	52803.690628	33.178548
770.098417	52897.768881	33.183565
771.142371	52984.130724	33.188583
771.650238	53074.846496	33.193600
772.629877	53162.761363	33.198618
773.293056	53255.606590	33.203636
774.256893	53349.646985	33.208653
775.224360	53433.218336	33.213671
775.868438	53510.759488	33.218688
776.667166	53600.431163	33.223706
777.549277	53686.513385	33.228724
778.031136	53759.874621	33.233741
778.784839	53836.008881	33.238759
779.056911	53923.191665	33.243776
779.773072	54016.050647	33.248794
780.196199	54108.927118	33.253812
780.917630	54207.706277	33.258829
781.495212	54303.375954	33.263847
782.124333	54409.083620	33.268864
783.220353	54492.429630	33.273882
784.817797	54577.354484	33.278900
785.810889	54666.379554	33.283917
787.053569	54751.357730	33.288935
787.657866	54835.424973	33.293952
788.417318	54925.412485	33.298970
789.003635	54997.768990	33.303988
789.699468	55097.397209	33.309005
790.638066	55173.196334	33.314023
790.804914	55268.414425	33.319040
791.977791	55362.410774	33.324058
792.097340	55463.501309	33.329076
792.476225	55566.425952	33.334093
793.531406	55672.474039	33.339111
794.135126	55785.251254	33.344128
795.001278	55874.132222	33.349146
796.168037	55992.068038	33.354164
796.936366	56103.694990	33.359181
797.858240	56205.622899	33.364199
799.186307	56297.222023	33.369216
800.100859	56396.845733	33.374234
801.006724	56481.843007	33.379252
801.910515	56577.943435	33.384269
802.717614	56666.060510	33.389287
803.254066	56772.838788	33.394304
803.890546	56872.353055	33.399322
804.636664	56971.938086	33.404340
805.354860	57076.236006	33.409357
806.305288	57171.971361	33.414375
806.376628	57286.677996	33.419392
807.378304	57388.251144	33.424410
808.421073	57505.464503	33.429428
809.188374	57606.812254	33.434445
810.624337	57693.192772	33.439463
811.487800	57804.484833	33.444480
812.391340	57898.727436	33.449498
813.270943	57993.814940	33.454516
813.987623	58090.307579	33.459533
814.609355	58189.015623	33.464551
815.189419	58295.984362	33.469568
815.634991	58397.029292	33.474586
816.447125	58505.749058	33.479604
817.109187	58614.393207	33.484621
818.947297	58712.093002	33.489639
819.503727	58816.812314	33.494656
820.140982	58921.000535	33.499674
821.040452	59030.043578	33.504692
821.531868	59140.880242	33.509709
822.627924	59236.234714	33.514727
823.205922	59355.179146	33.519744
824.151020	59452.247095	33.524762
824.645421	59555.842951	33.529780
825.293815	59668.659863	33.534797
826.497307	59778.206312	33.539815
826.950470	59892.270310	33.544832
828.145269	60002.552537	33.549850
829.060576	60099.925577	33.554868
830.168714	60202.405332	33.559885
830.885956	60303.269326	33.564903
832.108738	60403.620139	33.569920
833.025863	60481.440081	33.574938
833.960131	60566.759588	33.579956
834.810698	60653.433240	33.584973
835.870306	60744.446202	33.589991
836.176031	60829.264388	33.595008
837.342005	60913.617805	33.600026
838.108326	60989.789833	33.605044
839.021785	61076.789828	33.610061
840.740516	61149.302878	33.615079
841.136354	61239.916273	33.620096
841.705378	61317.000812	33.625114
842.676267	61411.962809	33.630132
842.899568	61510.108464	33.635149
843.969728	61592.849900	33.640167
844.376514	61693.487877	33.645184
845.293989	61786.753924	33.650202
845.973457	61891.316955	33.655220
846.456656	61995.363198	33.660237
847.282638	62097.128186	33.665255
848.390215	62208.606156	33.670272
849.343729	62293.512515	33.675290
850.507518	62391.967705	33.680308
851.501981	62505.981741	33.685325
852.523433	62598.519969	33.690343
853.386866	62701.773460	33.695360
853.757072	62810.501079	33.700378
854.371457	62909.056255	33.705396
855.409280	63021.220232	33.710413
855.809821	63122.409846	33.715431
856.647571	63244.393180	33.720448
857.325563	63357.257134	33.725466
857.969182	63482.384071	33.730484
859.008391	63601.485248	33.735501
860.204953	63703.999459	33.740519
861.340368	63813.540889	33.745536
862.590642	63925.194101	33.750554
863.587603	64027.945327	33.755572
864.293495	64142.022619	33.760589
865.325591	64240.660205	33.765607
866.023232	64356.522669	33.770624
866.252135	64467.981685	33.775642
867.131128	64577.152496	33.780660
867.345851	64702.585554	33.785677
868.745314	64829.384153	33.790695
868.894509	64966.018796	33.795712
870.094509	65084.735150	33.800730
871.170589	65206.285884	33.805748
871.520948	65346.524581	33.810765
872.451526	65470.212446	33.815783
873.399188	65611.106070	33.820800
874.537155	65739.673129	33.825818
876.320906	65846.298135	33.830836
876.886615	65960.231635	33.835853
877.805649	66078.633604	33.840871
879.295346	66194.242058	33.845888
880.359294	66300.672750	33.850906
881.805305	66400.320272	33.855924
882.930572	66494.850074	33.860941
884.090308	66584.791081	33.865959
885.446516	66658.508989	33.870976
886.360088	66748.244992	33.875994
887.185572	66815.881152	33.881012
888.056529	66911.403358	33.886029
888.405524	66996.985629	33.891047
889.632795	67084.211670	33.896064
890.724860	67151.962724	33.901082
892.436480	67205.247007	33.906100
892.872378	67274.523542	33.911117
894.091477	67334.111013	33.916135
894.698987	67402.815772	33.921152
894.867536	67463.760237	33.926170
895.569307	67542.862689	33.931188
896.159811	67622.793168	33.936205
896.776652	67715.313809	33.941223
897.204202	67799.590205	33.946240
897.629236	67894.109737	33.951258
898.617093	67989.566848	33.956276
899.078905	68112.854914	33.961293
899.499611	68206.946628	33.966311
900.409639	68314.234973	33.971328
900.862760	68448.047213	33.976346
902.127286	68570.332195	33.981364
902.438023	68713.128947	33.986381
903.167830	68827.139216	33.991399
904.121270	68956.951528	33.996416
904.634772	69100.867975	34.001434
905.839610	69234.130451	34.006452
906.339649	69380.447382	34.011469
907.261155	69529.534371	34.016487
908.450345	69667.968002	34.021504
909.220508	69826.712092	34.026522
910.431441	69956.342323	34.031540
911.510250	70092.628210	34.036557
913.159685	70226.879057	34.041575
914.702601	70348.413523	34.046592
915.560634	70471.428157	34.051610
916.832187	70584.251334	34.056628
917.894196	70711.489046	34.061645
918.830802	70831.893833	34.066663
919.446844	70941.362490	34.071680
919.789547	71074.741567	34.076698
921.079728	71191.833140	34.081716
921.758456	71318.733353	34.086733
923.057024	71437.652354	34.091751
924.459842	71569.157534	34.096768
924.930399	71685.755460	34.101786
925.867476	71798.678456	34.106804
926.659499	71935.776131	34.111821
927.958031	72059.795432	34.116839
928.560485	72182.754750	34.121856
929.253148	72313.958628	34.126874
930.166916	72451.665417	34.131892
930.744752	72582.510547	34.136909
931.546457	72712.535152	34.141927
932.394735	72852.203105	34.146944
933.323279	72996.576309	34.151962
934.419278	73132.669859	34.156980
934.850146	73285.171699	34.161997
936.058997	73428.710745	34.167015
937.183465	73579.309820	34.172032
937.948964	73718.092711	34.177050
939.701312	73837.784360	34.182068
940.628761	73972.627310	34.187085
941.275040	74106.935918	34.192103
942.550827	74229.238513	34.197120
943.474675	74365.905887	34.202138
944.788503	74492.251228	34.207156
945.756030	74623.145111	34.212173
946.738150	74745.126179	34.217191
947.415922	74874.899622	34.222208
948.138833	75011.749828	34.227226
948.782216	75151.542363	34.232244
949.741934	75285.382418	34.237261
950.476644	75427.248672	34.242279
951.340061	75567.140146	34.247296
951.697128	75707.869180	34.252314
952.325067	75846.119117	34.257332
952.996822	75997.271611	34.262349
953.880932	76140.249794	34.267367
954.832410	76290.725386	34.272384
955.714271	76446.052141	34.277402
956.826497	76593.106610	34.282420
957.841676	76747.129375	34.287437
958.321827	76903.196445	34.292455
959.364582	77065.312947	34.297472
960.453130	77221.382488	34.302490
961.833410	77377.177004	34.307508
962.866175	77537.255554	34.312525
963.664809	77687.917771	34.317543
965.026690	77837.494456	34.322560
966.026549	78003.635168	34.327578
966.974606	78151.410310	34.332596
968.967141	78279.372500	34.337613
970.067319	78423.151795	34.342631
971.296730	78555.904107	34.347648
972.082228	78707.517873	34.352666
972.965299	78840.297712	34.357684
973.757799	78987.870130	34.362701
974.465377	79133.110768	34.367719
975.261742	79284.530523	34.372736
975.894747	79448.313711	34.377754
976.672189	79603.325475	34.382772
977.278712	79764.015684	34.387789
978.042361	79934.106605	34.392807
979.517414	80095.812693	34.397824
980.103284	80266.017846	34.402842
981.275733	80417.762345	34.407860
982.436667	80598.388500	34.412877
982.938188	80768.212870	34.417895
984.016324	80945.546937	34.422912
985.211694	81127.835380	34.427930
986.034271	81300.394002	34.432948
986.850009	81491.807640	34.437965
987.798089	81667.859350	34.442983
989.076621	81839.890887	34.448000
989.644210	82018.836369	34.453018
991.438281	82186.615793	34.458036
993.107314	82344.003601	34.463053
994.480289	82501.055693	34.468071
996.018206	82655.304072	34.473088
996.657760	82809.708886	34.478106
997.968689	82958.182698	34.483124
999.156910	83115.035555	34.488141
1000.117692	83268.460101	34.493159
1001.450251	83401.419728	34.498176
1002.381839	83536.439641	34.503194
1003.877022	83679.984159	34.508212
1004.712043	83811.244501	34.513229
1006.009554	83950.710947	34.518247
1007.147199	84078.790704	34.523264
1007.886529	84216.105257	34.528282
1009.259354	84336.497931	34.533300
1010.955007	84461.760213	34.538317
1011.894063	84584.225541	34.543335
1013.204424	84690.052508	34.548352
1014.263210	84815.643833	34.553370
1015.026012	84942.303646	34.558388
1015.524020	85060.377581	34.563405
1016.206528	85184.964012	34.568423
1017.252672	85298.791112	34.573440
1017.823814	85441.253357	34.578458
1018.646394	85571.690486	34.583476
1019.734637	85705.798517	34.588493
1020.723399	85828.249481	34.593511
1021.558408	85952.669168	34.598528
1022.309357	86080.533036	34.603546
1023.329422	86213.984564	34.608564
1024.449056	86345.692870	34.613581
1025.000641	86476.762154	34.618599
1025.975256	86609.495783	34.623616
1026.784401	86746.117578	34.628634
1027.712539	86891.104812	34.633652
1028.523754	87034.055777	34.638669
1029.536551	87188.358090	34.643687
1030.526752	87343.880130	34.648704
1032.047890	87475.616731	34.653722
1032.928309	87631.810667	34.658740
1034.160988	87781.707698	34.663757
1035.641649	87916.636499	34.668775
1036.944157	88056.322761	34.673792
1037.951755	88197.083947	34.678810
1039.462939	88323.030298	34.683828
1040.578755	88454.643429	34.688845
1041.424609	88595.319904	34.693863
1042.585410	88723.262975	34.698880
1043.405078	88872.273518	34.703898
1044.223179	89006.729913	34.708916
1045.532085	89147.731510	34.713933
1046.250330	89294.793374	34.718951
1047.135895	89434.145557	34.723968
1047.914566	89593.153807	34.728986
1048.765627	89738.474993	34.734004
1050.629614	89880.230517	34.739021
1051.366248	90044.204059	34.744039
1052.626854	90191.213083	34.749056
1053.316830	90346.038772	34.754074
1054.296540	90498.823812	34.759092
1055.431858	90649.027153	34.764109
1055.743450	90818.493983	34.769127
1056.886288	90985.722878	34.774144
1057.867145	91153.422835	34.779162
1058.398950	91332.457784	34.784180
1059.377432	91501.337745	34.789197
1060.518412	91687.115960	34.794215
1061.317993	91876.490242	34.799232
1062.097086	92062.837710	34.804250
1063.237511	92246.291147	34.809268
1064.275561	92424.319752	34.814285
1065.288341	92631.918259	34.819303
1066.433763	92815.944800	34.824320
1067.579516	93001.333506	34.829338
1068.885371	93199.906725	34.834356
1070.022539	93383.685731	34.839373
1070.615911	93590.880921	34.844391
1071.506312	93774.665821	34.849408
1072.852681	93963.187017	34.854426
1074.208718	94153.815861	34.859444
1077.424131	94300.784937	34.864461
1079.184978	94457.813788	34.869479
1080.799531	94602.429725	34.874496
1082.173057	94738.053734	34.879514
1083.115709	94874.845054	34.884532
1084.525440	95004.451083	34.889549
1085.171992	95144.382045	34.894567
1086.056992	95292.864101	34.899584
1087.460453	95427.986856	34.904602
1087.740531	95577.039401	34.909620
1088.734040	95718.049127	34.914637
1089.311354	95882.214899	34.919655
1090.672399	96026.501407	34.924672
1091.758004	96178.778934	34.929690
1092.764533	96301.045891	34.934708
1093.817205	96438.011151	34.939725
1094.717827	96589.619210	34.944743
1095.317416	96727.256281	34.949760
1096.304693	96888.024532	34.954778
1096.936115	97040.173758	34.959796
1097.883229	97195.816626	34.964813
1098.261663	97366.222725	34.969831
1098.966394	97544.495438	34.974848
1099.878616	97722.481763	34.979866
1100.594375	97913.897708	34.984884
1101.284373	98115.518224	34.989901
1102.007328	98317.533721	34.994919
1103.506883	98524.309412	34.999936
1104.789284	98733.699501	35.004954
1105.489902	98935.559033	35.009972
1106.628139	99151.060540	35.014989
1107.866217	99369.332979	35.020007
1109.381186	99582.926974	35.025024
1110.602485	99790.436576	35.030042
1111.057016	100015.878482	35.035060
1112.567429	100220.045042	35.040077
1113.447637	100443.166158	35.045095
1114.626237	100662.200288	35.050112
1115.991722	100882.566544	35.055130
1116.576019	101105.609553	35.060148
1118.054961	101306.712879	35.065165
1119.713844	101524.332389	35.070183
1121.434932	101733.174079	35.075200
1123.218138	101923.088036	35.080218
1126.543865	102068.210038	35.085236
1129.433913	102198.392520	35.090253
1130.997503	102354.939722	35.095271
1132.489232	102475.041075	35.100288
1134.010199	102602.571741	35.105306
1134.796186	102722.879970	35.110324
1135.920634	102843.588505	35.115341
1136.785196	102964.593994	35.120359
1137.836144	103089.691244	35.125376
1138.446699	103207.681654	35.130394
1139.523921	103355.988987	35.135412
1140.563650	103482.445043	35.140429
1141.010770	103616.281947	35.145447
1141.864141	103761.703285	35.150464
1142.803061	103918.939755	35.155482
1142.956634	104085.856444	35.160500
1143.962537	104241.893280	35.165517
1144.732618	104416.802427	35.170535
1145.378398	104602.587000	35.175552
1146.740732	104790.166395	35.180570
1147.236422	104979.676644	35.185588
1148.350246	105172.935859	35.190605
1149.375613	105358.206845	35.195623
1150.147058	105566.014562	35.200640
1151.287120	105765.049063	35.205658
1152.172648	105978.185822	35.210676
1153.397315	106181.021679	35.215693
1154.810657	106383.359160	35.220711
1156.005224	106599.185387	35.225728
1156.803596	106809.202178	35.230746
1157.889716	107010.167470	35.235764
1159.204980	107215.415345	35.240781
1160.702368	107426.549621	35.245799
1162.198144	107634.202640	35.250816
1163.787468	107825.261650	35.255834
1164.248055	108039.941963	35.260852
1165.657404	108240.064870	35.265869
1166.271323	108442.841853	35.270887
1167.515126	108648.125190	35.275904
1168.610710	108826.986596	35.280922
1169.601387	109029.464811	35.285940
1170.764355	109231.421949	35.290957
1171.987574	109439.653418	35.295975
1172.498621	109636.008900	35.300992
1175.064543	109812.010807	35.306010
1176.386713	110012.794630	35.311028
1177.951915	110206.509241	35.316045
1179.180019	110393.732087	35.321063
1180.179432	110581.044820	35.326080
1181.012347	110779.609950	35.331098
1181.970674	110973.823361	35.336116
1183.350791	111175.682858	35.341133
1184.142533	111381.023763	35.346151
1185.102719	111580.181621	35.351168
1186.426671	111781.016099	35.356186
1187.555248	111997.288932	35.361204
1189.083976	112196.141562	35.366221
1189.879784	112414.309750	35.371239
1190.677592	112633.632150	35.376256
1191.927357	112853.413389	35.381274
1193.007933	113076.138220	35.386292
1194.229774	113305.327802	35.391309
1195.369057	113531.416421	35.396327
1197.081109	113749.202369	35.401344
1198.364414	113955.418270	35.406362
1200.030935	114182.425545	35.411380
1201.663569	114383.240263	35.416397
1203.275888	114591.293978	35.421415
1204.390074	114790.512581	35.426432
1206.088146	114987.279208	35.431450
1207.306956	115192.311273	35.436468
1208.343914	115389.342400	35.441485
1209.816516	115583.591300	35.446503
1210.731725	115780.303257	35.451520
1212.008451	115984.723295	35.456538
1212.932359	116193.777217	35.461556
1214.859696	116393.188959	35.466573
1216.277503	116566.788669	35.471591
1218.325972	116741.323790	35.476608
1219.970808	116912.353886	35.481626
1221.398462	117088.932676	35.486644
1222.555229	117264.581857	35.491661
1223.546043	117449.483845	35.496679
1224.529000	117624.492516	35.501696
1225.295102	117800.374492	35.506714
1226.137258	117995.137160	35.511732
1227.581096	118180.627584	35.516749
1228.892208	118363.315578	35.521767
1229.699035	118551.359549	35.526784
1231.130440	118739.187101	35.531802
1232.022424	118942.614969	35.536820
1233.229067	119120.700056	35.541837
1235.144305	119311.251423	35.546855
1235.826530	119509.852224	35.551872
1237.467316	119692.544587	35.556890
1238.482899	119886.898362	35.561908
1239.764817	120061.251236	35.566925
1241.115251	120257.186586	35.571943
1242.086443	120457.215821	35.576960
1243.041451	120646.452553	35.581978
1244.360231	120847.187109	35.586996
1245.465189	121038.910566	35.592013
1246.724997	121247.818513	35.597031
1247.412577	121462.880235	35.602048
1248.837115	121657.507359	35.607066
1249.578341	121860.460894	35.612084
1250.451739	122068.538973	35.617101
1251.417516	122269.215003	35.622119
1252.472997	122476.150534	35.627136
1253.932375	122680.777412	35.632154
1254.840467	122904.341829	35.637172
1255.928278	123111.732629	35.642189
1257.393450	123331.697402	35.647207
1258.288764	123547.145247	35.652224
1259.697924	123780.797030	35.657242
1261.209363	123990.937121	35.662260
1262.666759	124208.260851	35.667277
1264.367925	124416.838946	35.672295
1265.335324	124631.610884	35.677312
1266.526247	124848.045556	35.682330
1267.781100	125089.083845	35.687348
1268.919985	125320.726509	35.692365
1269.962472	125553.261434	35.697383
1271.049618	125790.974462	35.702400
1272.293627	126017.966234	35.707418
1273.567339	126261.342721	35.712436
1274.925767	126504.301504	35.717453
1276.730607	126740.711463	35.722471
1277.778825	126973.028067	35.727488
1279.181624	127207.974659	35.732506
1280.477403	127452.130061	35.737524
1281.259163	127700.821552	35.742541
1283.187841	127927.980014	35.747559
1283.894458	128192.633130	35.752576
1285.313357	128437.840577	35.757594
1286.162163	128698.177487	35.762612
1287.471716	128941.721203	35.767629
1289.557384	129185.594411	35.772647
1291.046869	129416.981465	35.777664
1292.568275	129644.967828	35.782682
1293.630708	129910.210230	35.787700
1294.926839	130148.606452	35.792717
1296.358628	130385.866479	35.797735
1297.737572	130634.621636	35.802752
1299.455177	130863.205381	35.807770
1301.092683	131102.984579	35.812788
1302.333452	131344.073672	35.817805
1303.590583	131579.888439	35.822823
1304.359727	131824.951072	35.827840
1306.166690	132043.906906	35.832858
1307.668779	132289.586781	35.837876
1308.339335	132533.023185	35.842893
1309.783457	132779.312226	35.847911
1310.613922	133035.250772	35.852928
1312.059376	133276.231677	35.857946
1313.235390	133534.284657	35.862964
1314.446094	133797.392212	35.867981
1315.661113	134050.169022	35.872999
1316.946881	134307.322503	35.878016
1318.216998	134562.819826	35.883034
1319.149048	134822.837791	35.888052
1320.481760	135078.924610	35.893069
1321.851398	135346.556948	35.898087
1323.223681	135624.485635	35.903104
1324.186430	135886.256480	35.908122
1325.202185	136167.038057	35.913140
1326.753236	136444.246670	35.918157
1327.591155	136714.539285	35.923175
1328.258032	137011.538276	35.928192
1329.869028	137290.899353	35.933210
1331.013849	137592.591440	35.938228
1332.264776	137882.756146	35.943245
1333.700074	138176.950077	35.948263
1336.157332	138452.744440	35.953280
1338.856702	138682.082116	35.958298
1340.521850	138918.579183	35.963316
1342.129726	139144.107009	35.968333
1344.547960	139360.334658	35.973351
1345.753661	139587.935486	35.978368
1346.999017	139805.362155	35.983386
1347.709101	140019.556880	35.988404
1348.742982	140258.501005	35.993421
1350.394022	140485.463353	35.998439
1351.325038	140737.297991	36.003456
1352.441866	140973.570521	36.008474
1353.642270	141216.310386	36.013492
1354.699834	141454.662903	36.018509
1356.246791	141699.085877	36.023527
1357.659469	141952.675450	36.028544
1359.775434	142177.023020	36.033562
1361.038905	142412.887929	36.038580
1362.024949	142652.553927	36.043597
1363.585124	142900.761981	36.048615
1364.767183	143150.112369	36.053632
1366.123886	143406.410103	36.058650
1367.151919	143653.329482	36.063668
1368.171616	143912.768277	36.068685
1369.430963	144166.399256	36.073703
1370.837604	144445.129382	36.078720
1372.115786	144706.534763	36.083738
1373.889160	144971.918035	36.088756
1374.791135	145237.156103	36.093773
1376.536793	145497.944435	36.098791
1378.097788	145774.769748	36.103808
1379.279938	146038.673721	36.108826
1380.626130	146306.103384	36.113844
1381.815923	146578.494298	36.118861
1383.351946	146857.323131	36.123879
1384.588419	147132.145437	36.128896
1386.015033	147406.836825	36.133914
1387.408199	147679.620766	36.138932
1388.333236	147975.477902	36.143949
1389.803258	148251.132295	36.148967
1390.722427	148540.869209	36.153984
1392.105358	148840.639753	36.159002
1393.619830	149139.427003	36.164020
1395.095054	149433.809447	36.169037
1396.788485	149716.844627	36.174055
1398.753033	150006.381572	36.179072
1400.454834	150298.285386	36.184090
1401.965989	150570.944192	36.189108
1403.110524	150851.986190	36.194125
1404.609472	151121.048865	36.199143
1406.297318	151416.337509	36.204160
1407.498972	151692.772073	36.209178
1409.387121	151966.076033	36.214196
1410.814523	152229.780435	36.219213
1412.166324	152505.967684	36.224231
1413.820453	152785.988162	36.229248
1415.185655	153060.540916	36.234266
1416.925642	153324.505432	36.239284
1417.672232	153608.119842	36.244301
1419.306622	153877.661449	36.249319
1420.222099	154159.019395	36.254336
1421.843597	154434.871282	36.259354
1422.814217	154713.991570	36.264372
1424.192322	155005.452150	36.269389
1425.704684	155297.780583	36.274407
1427.321032	155588.381452	36.279424
1428.513694	155890.725119	36.284442
1430.287553	156153.485337	36.289460
1431.458568	156431.848807	36.294477
1432.948279	156703.691781	36.299495
1434.193793	156969.779793	36.304512
1435.375453	157250.532092	36.309530
1436.402169	157531.984391	36.314548
1437.745547	157810.772869	36.319565
1439.799158	158085.703161	36.324583
1440.806227	158359.146984	36.329600
1441.992132	158655.689745	36.334618
1443.634201	158937.595286	36.339636
1444.672055	159235.169019	36.344653
1446.079123	159523.955472	36.349671
1447.986334	159816.822186	36.354688
1449.053668	160114.219789	36.359706
1450.459491	160410.523102	36.364724
1451.738773	160730.408779	36.369741
1453.169679	161025.887688	36.374759
1454.634397	161335.128391	36.379776
1455.705348	161650.031643	36.384794
1457.163862	161961.574347	36.389812
1458.573471	162283.759342	36.394829
1460.470438	162596.908753	36.399847
1461.787796	162908.646780	36.404864
1463.869323	163224.980135	36.409882
1465.688531	163534.812538	36.414900
1466.949744	163856.513864	36.419917
1469.439617	164139.747586	36.424935
1471.504090	164440.575620	36.429952
1473.115421	164731.596981	36.434970
1474.643437	165016.099782	36.439988
1476.446216	165302.500167	36.445005
1478.535643	165574.415760	36.450023
1480.151270	165845.003205	36.455040
1481.259137	166130.889821	36.460058
1482.839917	166403.338980	36.465076
1484.206209	166686.902440	36.470093
1485.724939	166963.463724	36.475111
1487.005432	167246.740463	36.480128
1488.172670	167538.754944	36.485146
1489.425389	167826.392204	36.490164
1490.994705	168118.318424	36.495181
1491.767117	168417.459117	36.500199
1493.176515	168716.191643	36.505216
1494.194189	169030.383035	36.510234
1495.709227	169339.240788	36.515252
1496.986004	169658.177397	36.520269
1498.300664	169980.764502	36.525287
1499.542596	170309.571100	36.530304
1500.526015	170641.125789	36.535322
1502.143467	170976.727262	36.540340
1503.183205	171321.893524	36.545357
1504.587962	171656.596117	36.550375
1506.283838	172006.125485	36.555392
1507.437536	172364.769981	36.560410
1508.610858	172717.538399	36.565428
1509.918904	173081.784483	36.570445
1511.726822	173436.737276	36.575463
1513.317077	173792.439457	36.580480
1514.547953	174171.770205	36.585498
1516.945531	174509.412094	36.590516
1519.295636	174848.231759	36.595533
1521.978454	175175.970308	36.600551
1524.008947	175495.290925	36.605568
1525.770969	175816.637927	36.610586
1527.522976	176125.995637	36.615604
1528.948136	176435.231796	36.620621
1530.449846	176742.363144	36.625639
1532.149883	177051.062611	36.630656
1533.559706	177359.799409	36.635674
1534.564381	177645.646444	36.640692
1536.185418	177946.533904	36.645709
1537.657707	178234.362781	36.650727
1539.102659	178524.253876	36.655744
1539.983949	178813.034354	36.660762
1541.659088	179103.944000	36.665780
1543.391868	179425.369731	36.670797
1544.901352	179711.588903	36.675815
1546.712337	180012.469744	36.680832
1548.651915	180311.427199	36.685850
1550.354748	180590.625825	36.690868
1552.738041	180871.629666	36.695885
1553.918361	181169.423300	36.700903
1555.548891	181457.053536	36.705920
1556.768160	181763.017963	36.710938
1557.932281	182047.555617	36.715956
1559.157082	182350.819005	36.720973
1560.803384	182649.508341	36.725991
1562.259118	182966.102313	36.731008
1563.170600	183287.814726	36.736026
1564.721424	183602.099265	36.741044
1566.063429	183932.070669	36.746061
1567.442443	184263.535713	36.751079
1569.004586	184594.236202	36.756096
1570.412938	184930.688806	36.761114
1571.903104	185260.884802	36.766132
1573.757583	185603.233373	36.771149
1575.148420	185946.359043	36.776167
1576.953914	186295.752135	36.781184
1578.384967	186652.736765	36.786202
1580.207312	186998.856468	36.791220
1581.424214	187348.607503	36.796237
1582.556554	187706.308335	36.801255
1584.297464	188054.732818	36.806272
1585.709658	188418.611691	36.811290
1587.062938	188781.449005	36.816308
1588.899886	189156.788289	36.821325
1590.602194	189520.549776	36.826343
1592.044187	189874.975574	36.831360
1593.474467	190258.069329	36.836378
1595.134644	190628.191784	36.841396
1597.208425	191003.922420	36.846413
1599.711628	191354.778945	36.851431
1601.542329	191698.652655	36.856448
1602.931576	192057.682853	36.861466
1605.575608	192383.729115	36.866484
1607.865315	192723.393987	36.871501
1609.488283	193065.773714	36.876519
1611.361588	193395.494970	36.881536
1612.957099	193719.792429	36.886554
1614.535038	194040.463659	36.891572
1615.981798	194372.368148	36.896589
1617.022692	194715.576985	36.901607
1618.523289	195049.431157	36.906624
1619.725443	195395.879620	36.911642
1621.239936	195736.336679	36.916660
1622.817071	196098.976990	36.921677
1623.962148	196442.825221	36.926695
1625.748556	196786.365818	36.931712
1627.217371	197147.442921	36.936730
1628.603840	197504.041313	36.941748
1630.748352	197852.847633	36.946765
1632.517236	198206.593284	36.951783
1633.863263	198554.862715	36.956800
1635.538155	198914.861403	36.961818
1637.030557	199270.067693	36.966836
1638.568450	199622.424324	36.971853
1640.096702	199985.538115	36.976871
1641.608660	200328.710516	36.981888
1642.970986	200661.219015	36.986906
1645.043861	201009.304162	36.991924
1646.854857	201354.095239	36.996941
1647.662262	201689.912778	37.001959
1649.575486	202045.164948	37.006976
1650.716181	202407.136523	37.011994
1652.345739	202763.442284	37.017012
1654.123345	203132.637948	37.022029
1655.206791	203501.137924	37.027047
1657.076778	203857.447230	37.032064
1658.399616	204235.154573	37.037082
1659.990012	204618.545868	37.042100
1661.626491	204999.899923	37.047117
1663.137677	205384.565244	37.052135
1664.762196	205771.981723	37.057152
1666.509821	206178.438492	37.062170
1668.465512	206560.661592	37.067188
1670.007265	206964.947229	37.072205
1671.246879	207360.879228	37.077223
1672.950814	207760.240783	37.082240
1674.589915	208176.858533	37.087258
1676.193786	208581.142053	37.092276
1677.621006	208999.500642	37.097293
1679.203602	209418.787949	37.102311
1681.138896	209841.548949	37.107328
1682.865975	210255.699253	37.112346
1684.476363	210682.238854	37.117364
1686.828444	211099.667384	37.122381
1688.334961	211522.596731	37.127399
1690.126055	211935.119198	37.132416
1692.215257	212362.222668	37.137434
1693.424631	212789.905775	37.142452
1694.888245	213212.926567	37.147469
1696.578882	213646.603862	37.152487
1698.219826	214081.129572	37.157504
1699.423370	214528.555446	37.162522
1700.819676	214977.322994	37.167540
1702.702555	215424.132638	37.172557
1704.877177	215866.045102	37.177575
1707.239034	216287.178644	37.182592
1709.357371	216729.409191	37.187610
1711.184198	217158.559323	37.192628
1713.895735	217571.005170	37.197645
1716.084744	217987.653833	37.202663
1718.003478	218456.136093	37.207680
1719.977475	218858.778744	37.212698
1721.742346	219265.749977	37.217716
1723.796970	219664.826629	37.222733
1725.410515	220074.696143	37.227751
1726.911074	220458.171252	37.232768
1728.576668	220858.713817	37.237786
1730.212094	221267.669921	37.242804
1732.448229	221648.512854	37.247821
1734.049085	222044.066889	37.252839
1735.869195	222439.433595	37.257856
1737.316217	222836.082686	37.262874
1739.250096	223228.486972	37.267892
1741.162337	223605.072303	37.272909
1742.933727	223996.261545	37.277927
1744.935707	224382.714937	37.282944
1746.473317	224772.421508	37.287962
1748.308779	225156.238022	37.292980
1750.296838	225531.089695	37.297997
1752.049177	225918.910157	37.303015
1753.683745	226300.325131	37.308032
1754.910069	226696.871187	37.313050
1756.282965	227078.458865	37.318068
1758.200155	227450.229163	37.323085
1759.656216	227830.382850	37.328103
1761.489321	228188.046578	37.333120
1762.816501	228572.414809	37.338138
1764.011395	228953.757985	37.343156
1765.605479	229345.247117	37.348173
1767.368666	229742.373681	37.353191
1768.732601	230149.042015	37.358208
1770.071120	230561.430905	37.363226
1771.453136	230971.857886	37.368244
1773.508846	231392.741177	37.373261
1775.124123	231827.847030	37.378279
1777.630659	232217.922634	37.383296
1779.783728	232632.773160	37.388314
1781.422455	233042.477359	37.393332
1783.604598	233451.101908	37.398349
1785.500233	233867.878010	37.403367
1787.785111	234283.625409	37.408384
1789.071026	234695.500542	37.413402
1790.605457	235124.862575	37.418420
1792.223865	235534.830304	37.423437
1793.756952	235966.201353	37.428455
1795.479992	236403.994005	37.433472
1797.548123	236838.580691	37.438490
1799.177454	237274.231775	37.443508
1801.115402	237712.322100	37.448525
1802.587073	238154.453388	37.453543
1804.318031	238600.378401	37.458560
1806.472992	239036.886156	37.463578
1807.861346	239496.383800	37.468596
1809.675943	239942.831274	37.473613
1811.236202	240406.239713	37.478631
1813.256340	240856.820946	37.483648
1815.653939	241311.481102	37.488666
1816.700795	241782.191665	37.493684
1818.307069	242241.480947	37.498701
1819.708363	242722.625798	37.503719
1821.325539	243202.313236	37.508736
1823.735542	243675.087676	37.513754
1825.695749	244153.932494	37.518772
1828.399876	244609.385997	37.523789
1831.824579	245042.595045	37.528807
1834.014710	245483.350688	37.533824
1836.242170	245926.691858	37.538842
1837.769464	246364.992885	37.543860
1840.027350	246797.813428	37.548877
1842.179221	247213.530534	37.553895
1844.583380	247632.203867	37.558912
1846.686667	248034.314000	37.563930
1848.357030	248449.248582	37.568948
1850.204286	248848.124991	37.573965
1852.215407	249262.902326	37.578983
1853.431841	249677.887943	37.584000
1855.216871	250088.918459	37.589018
1856.494288	250524.420406	37.594036
1858.090363	250951.182066	37.599053
1859.250814	251386.145253	37.604071
1860.804274	251834.913779	37.609088
1862.219555	252278.878933	37.614106
1863.652016	252750.607235	37.619124
1865.560688	253197.996893	37.624141
1866.899517	253676.854213	37.629159
1868.522070	254144.868428	37.634176
1870.443034	254613.519329	37.639194
1871.732470	255097.263008	37.644212
1873.552122	255584.119852	37.649229
1875.355825	256068.007333	37.654247
1877.131383	256552.687128	37.659264
1879.260428	257034.641131	37.664282
1880.712286	257515.996136	37.669300
1882.950620	257987.872485	37.674317
1884.507635	258458.515381	37.679335
1886.368541	258932.613593	37.684352
1888.730628	259406.679559	37.689370
1890.835834	259881.829580	37.694388
1893.090095	260346.793524	37.699405
1894.625527	260814.162773	37.704423
1896.680113	261295.214466	37.709440
1898.913369	261762.137596	37.714458
1901.233489	262239.842553	37.719476
1903.381468	262692.680650	37.724493
1905.241486	263177.396508	37.729511
1907.496545	263635.017630	37.734528
1909.729847	264092.819924	37.739546
1911.768686	264559.799307	37.744564
1913.696985	265018.388240	37.749581
1915.708401	265479.605004	37.754599
1917.640855	265941.037720	37.759616
1919.343056	266398.392900	37.764634
1921.269346	266868.996373	37.769652
1922.937409	267345.383276	37.774669
1924.601953	267825.758555	37.779687
1926.003065	268303.204810	37.784704
1928.351847	268786.107579	37.789722
1930.140925	269283.277344	37.794740
1932.150237	269759.604994	37.799757
1934.144733	270252.598770	37.804775
1935.434839	270742.990452	37.809792
1937.528789	271246.025858	37.814810
1939.416550	271748.611992	37.819828
1941.386055	272253.419214	37.824845
1943.602867	272749.217471	37.829863
1945.478280	273271.769609	37.834880
1947.273688	273766.238765	37.839898
1949.124331	274283.356930	37.844916
1951.049561	274799.471020	37.849933
1952.965572	275310.987744	37.854951
1955.375059	275824.504644	37.859968
1958.133064	276304.838066	37.864986
1960.410875	276819.771732	37.870004
1962.463227	277307.103962	37.875021
1964.473936	277807.574922	37.880039
1965.828597	278320.676624	37.885056
1968.189459	278826.472398	37.890074
1969.907795	279338.317413	37.895092
1971.790456	279851.073749	37.900109
1973.076022	280364.765897	37.905127
1975.146128	280886.328231	37.910144
1976.870005	281396.871305	37.915162
1978.603343	281934.057654	37.920180
1979.979850	282464.290649	37.925197
1982.284961	282987.433576	37.930215
1984.124525	283535.646947	37.935232
1986.612008	284073.717647	37.940250
1988.406998	284612.358484	37.945268
1990.685344	285141.950813	37.950285
1992.729965	285669.344752	37.955303
1995.007527	286204.597955	37.960320
1997.374821	286732.620521	37.965338
1999.247167	287260.926368	37.970356
2001.197552	287793.230637	37.975373
2003.778347	288315.319033	37.980391
2005.400377	288835.862440	37.985408
2008.001361	289354.666857	37.990426
2009.677771	289881.267888	37.995444
2011.192878	290398.012856	38.000461
2013.176126	290909.267989	38.005479
2014.555055	291409.191181	38.010496
2016.422133	291922.366433	38.015514
2018.175956	292441.908238	38.020532
2019.772252	292963.505875	38.025549
2021.678638	293494.930278	38.030567
2023.256575	294037.125227	38.035584
2024.920221	294575.264947	38.040602
2026.541552	295137.081149	38.045620
2028.404676	295683.208676	38.050637
2030.391906	296254.534054	38.055655
2032.467933	296835.925030	38.060672
2034.275459	297401.660969	38.065690
2036.407249	297988.014531	38.070708
2038.499282	298567.310628	38.075725
2040.642884	299137.324560	38.080743
2043.106031	299717.492360	38.085760
2045.916762	300292.392631	38.090778
2048.079479	300869.555678	38.095796
2050.652062	301429.656394	38.100813
2053.318601	301988.646169	38.105831
2055.644021	302548.882805	38.110848
2058.366645	303106.256588	38.115866
2060.132522	303662.591802	38.120884
2062.155300	304208.595332	38.125901
2064.626305	304761.226019	38.130919
2066.356590	305317.531461	38.135936
2068.453531	305870.801262	38.140954
2070.304388	306432.489029	38.145972
2072.379232	306995.202639	38.150989
2074.507629	307552.443519	38.156007
2076.005742	308126.825585	38.161024
2078.393834	308682.542916	38.166042
2080.420674	309271.863539	38.171060
2081.999549	309845.432875	38.176077
2084.516624	310411.859077	38.181095
2086.671601	310986.111990	38.186112
2088.822913	311561.757986	38.191130
2090.963985	312150.377923	38.196148
2092.955620	312735.183546	38.201165
2095.266688	313306.498302	38.206183
2097.104417	313889.441271	38.211200
2099.426460	314464.960673	38.216218
2101.728612	315044.440214	38.221236
2103.820835	315615.062262	38.226253
2106.747130	316178.126866	38.231271
2109.047585	316757.440479	38.236288
2111.986165	317300.103677	38.241306
2114.247577	317859.659176	38.246324
2116.073453	318424.665412	38.251341
2118.530140	318972.219774	38.256359
2120.536494	319528.198184	38.261376
2123.137470	320063.277807	38.266394
2125.490900	320606.620922	38.271412
2127.242043	321149.348354	38.276429
2129.297894	321686.079329	38.281447
2131.245397	322245.446940	38.286464
2133.111424	322796.774379	38.291482
2135.617164	323331.030381	38.296500
2138.112005	323872.469055	38.301517
2141.151296	324405.967409	38.306535
2143.159988	324927.140155	38.311552
2145.003021	325457.983906	38.316570
2147.301020	325987.198954	38.321588
2148.975180	326519.330873	38.326605
2150.870235	327050.202839	38.331623
2152.683499	327581.109016	38.336640
2154.680576	328119.647255	38.341658
2156.978915	328639.673542	38.346676
2158.487130	329156.754112	38.351693
2160.933358	329663.900487	38.356711
2162.308586	330199.145879	38.361728
2164.498166	330711.276015	38.366746
2166.514057	331236.631481	38.371764
2168.556730	331783.505501	38.376781
2170.645034	332310.539805	38.381799
2172.206992	332874.745466	38.386816
2174.037947	333421.562212	38.391834
2175.826388	333991.354536	38.396852
2177.568579	334564.017072	38.401869
2179.833092	335151.411909	38.406887
2181.359882	335752.706401	38.411904
2183.192962	336335.057248	38.416922
2185.671124	336931.865368	38.421940
2188.028160	337555.086015	38.426957
2190.041525	338166.781123	38.431975
2192.195991	338787.862786	38.436992
2194.375236	339395.758978	38.442010
2196.587431	340023.948568	38.447028
2198.593415	340662.088948	38.452045
2200.954668	341284.603102	38.457063
2202.769811	341936.668036	38.462080
2204.490549	342583.206777	38.467098
2206.361940	343244.280692	38.472116
2208.204285	343913.751363	38.477133
2210.936695	344588.369763	38.482151
2212.788597	345262.743678	38.487168
2214.741459	345946.253252	38.492186
2217.475763	346632.135968	38.497204
2219.457181	347314.783195	38.502221
2221.837408	348004.231816	38.507239
2224.511574	348697.326545	38.512256
2226.730312	349389.445591	38.517274
2229.243130	350075.440103	38.522292
2231.186774	350774.257519	38.527309
2233.927751	351462.349866	38.532327
2236.335220	352162.286547	38.537344
2238.899941	352847.544170	38.542362
2241.270158	353542.135882	38.547380
2243.466841	354232.913487	38.552397
2245.862535	354913.015043	38.557415
2248.217839	355620.820839	38.562432
2250.595562	356305.419501	38.567450
2252.843853	356991.829862	38.572468
2255.382163	357679.474843	38.577485
2257.921942	358354.751740	38.582503
2260.361988	359033.687554	38.587520
2262.785285	359719.262125	38.592538
2265.067637	360400.408432	38.597556
2267.203467	361088.163786	38.602573
2269.707069	361763.947715	38.607591
2271.781332	362445.879924	38.612608
2274.003063	363133.991358	38.617626
2276.410018	363801.891701	38.622644
2278.579646	364481.514686	38.627661
2281.128208	365158.881279	38.632679
2283.902841	365839.293284	38.637696
2286.248361	366498.227473	38.642714
2289.087289	367168.280537	38.647732
2291.756217	367825.539842	38.652749
2294.124969	368472.335831	38.657767
2296.037720	369132.335282	38.662784
2298.614118	369795.409008	38.667802
2300.957180	370449.200625	38.672820
2303.071307	371104.540246	38.677837
2305.409550	371739.641547	38.682855
2307.533191	372364.292225	38.687872
2310.251750	372976.557990	38.692890
2312.992537	373575.976267	38.697908
2314.861154	374197.035584	38.702925
2317.207818	374803.295237	38.707943
2319.357760	375411.073264	38.712960
2321.132775	376034.296554	38.717978
2323.121401	376662.139513	38.722996
2324.772680	377296.797883	38.728013
2326.942537	377935.238589	38.733031
2328.922753	378589.902858	38.738048
2331.148485	379236.551418	38.743066
2333.135419	379902.701733	38.748084
2335.266011	380577.968937	38.753101
2337.350990	381255.740326	38.758119
2339.691854	381944.840357	38.763136
2342.029128	382629.869715	38.768154
2344.221745	383327.180512	38.773172
2346.565152	384023.310496	38.778189
2349.124528	384715.536005	38.783207
2351.956411	385415.206124	38.788224
2354.146220	386108.578389	38.793242
2356.845334	386814.755538	38.798260
2359.052762	387521.454699	38.803277
2361.883775	388230.367096	38.808295
2364.084082	388934.678053	38.813312
2366.262756	389644.731127	38.818330
2368.662406	390366.037173	38.823348
2370.546635	391088.070760	38.828365
2372.971929	391806.651843	38.833383
2375.729164	392541.636949	38.838400
2377.838331	393271.312658	38.843418
2380.133740	394002.916916	38.848436
2382.325631	394742.174879	38.853453
2384.699807	395480.446604	38.858471
2386.966949	396239.322690	38.863488
2388.986003	396987.373233	38.868506
2391.720200	397731.307476	38.873524
2393.955332	398500.090300	38.878541
2396.114822	399271.754266	38.883559
2398.645895	400034.542760	38.888576
2401.313410	400812.467321	38.893594
2404.034071	401565.275589	38.898612
2406.160497	402351.103040	38.903629
2408.736035	403114.789957	38.908647
2411.380970	403875.302775	38.913664
2413.733737	404662.041682	38.918682
2415.877012	405421.607242	38.923700
2418.420663	406217.011459	38.928717
2420.722477	406992.544910	38.933735
2423.404928	407766.346667	38.938752
2425.769941	408550.109654	38.943770
2428.304358	409324.575516	38.948788
2430.998451	410106.440261	38.953805
2433.490836	410873.496862	38.958823
2435.954027	411660.673917	38.963840
2438.251984	412446.892439	38.968858
2441.322327	413206.060377	38.973876
2444.872749	413959.326737	38.978893
2448.159552	414693.416781	38.983911
2451.546642	415420.276691	38.988928
2454.522698	416129.582597	38.993946
2457.957733	416818.912562	38.998964
2460.674073	417523.942981	39.003981
2463.355531	418208.700490	39.008999
2466.024202	418880.121589	39.014016
2467.952074	419563.473186	39.019034
2470.268505	420236.157353	39.024052
2472.161861	420900.967947	39.029069
2473.920067	421550.160387	39.034087
2476.272146	422204.048401	39.039104
2478.038740	422875.840880	39.044122
2480.138336	423539.356730	39.049140
2482.113077	424221.813159	39.054157
2484.227777	424907.670546	39.059175
2486.442384	425605.998454	39.064192
2488.393666	426315.539428	39.069210
2490.524741	427034.041961	39.074228
2492.698777	427763.806087	39.079245
2494.433879	428494.531928	39.084263
2497.076359	429231.059002	39.089280
2499.309528	429990.715414	39.094298
2501.596837	430752.008994	39.099316
2503.833867	431521.031207	39.104333
2506.216028	432299.621732	39.109351
2508.931530	433081.066891	39.114368
2511.189645	433879.213896	39.119386
2513.652051	434669.555659	39.124404
2515.967599	435478.874011	39.129421
2518.331198	436282.183834	39.134439
2521.098523	437091.016045	39.139456
2523.208138	437923.207215	39.144474
2526.126108	438736.459668	39.149492
2528.596384	439571.313530	39.154509
2531.071869	440389.740734	39.159527
2533.785231	441228.439256	39.164544
2536.155683	442074.296970	39.169562
2538.742458	442914.470414	39.174580
2541.124812	443772.960235	39.179597
2543.713579	444611.398711	39.184615
2546.988812	445457.583170	39.189632
2549.784211	446318.787762	39.194650
2552.768006	447151.548520	39.199668
2555.681843	447995.720330	39.204685
2557.994059	448843.195537	39.209703
2560.646068	449673.839042	39.214720
2563.699465	450518.595706	39.219738
2566.575549	451356.166183	39.224756
2569.373661	452198.925154	39.229773
2571.435985	453030.545115	39.234791
2574.519143	453863.378819	39.239808
2576.358539	454721.364938	39.244826
2578.757282	455564.660111	39.249844
2581.373995	456419.514002	39.254861
2583.903176	457274.852220	39.259879
2587.125301	458112.293755	39.264896
2589.787539	458974.110958	39.269914
2592.855877	459815.400203	39.274932
2595.365639	460653.865159	39.279949
2597.929906	461486.978180	39.284967
2601.040665	462331.844668	39.289984
2603.949144	463171.552952	39.295002
2606.556193	463997.274813	39.300020
2609.115031	464833.735316	39.305037
2611.403756	465660.551769	39.310055
2614.590721	466502.345681	39.315072
2616.937558	467323.623838	39.320090
2619.736710	468142.164561	39.325108
2622.983879	468971.662590	39.330125
2625.911921	469791.526603	39.335143
2628.743055	470596.163025	39.340160
2631.185726	471417.704811	39.345178
2633.999499	472218.587108	39.350196
2636.394895	473034.559608	39.355213
2638.850105	473840.888451	39.360231
2641.268943	474650.724708	39.365248
2643.414781	475438.951276	39.370266
2645.878098	476223.606627	39.375284
2648.195482	477025.021926	39.380301
2650.841761	477816.802203	39.385319
2653.394583	478607.099214	39.390336
2655.275269	479415.654274	39.395354
2658.023056	480213.424983	39.400372
2660.278207	481024.624199	39.405389
2662.456946	481860.492168	39.410407
2665.101612	482671.553053	39.415424
2667.570899	483512.446629	39.420442
2670.234971	484356.499776	39.425460
2673.222256	485189.049602	39.430477
2676.060474	486040.011735	39.435495
2678.454168	486889.290152	39.440512
2681.193791	487747.102359	39.445530
2683.517916	488593.685157	39.450548
2687.068510	489463.040280	39.455565
2689.117964	490334.720234	39.460583
2692.407840	491180.613860	39.465600
2694.938889	492053.843640	39.470618
2697.671482	492931.588059	39.475636
2700.439537	493805.749441	39.480653
2702.811042	494693.051048	39.485671
2706.628120	495547.876212	39.490688
2709.585481	496428.733741	39.495706
2712.133902	497316.121219	39.500724
2714.735613	498184.938593	39.505741
2716.977077	499066.129796	39.510759
2719.873370	499956.296407	39.515776
2722.695389	500854.397294	39.520794
2725.244644	501742.205425	39.525812
2727.713909	502642.033036	39.530829
2730.749431	503530.017539	39.535847
2734.037047	504426.333962	39.540864
2736.707277	505327.897297	39.545882
2739.881777	506219.242513	39.550900
2742.984374	507104.853053	39.555917
2745.812976	508002.157419	39.560935
2748.964983	508882.368251	39.565952
2751.614530	509777.989776	39.570970
2754.483050	510659.309296	39.575988
2757.445669	511536.683117	39.581005
2760.012404	512409.083883	39.586023
2763.285132	513303.949983	39.591040
2766.017277	514178.594416	39.596058
2768.702422	515058.187072	39.601076
2771.630135	515952.808020	39.606093
2774.019690	516840.059297	39.611111
2776.857099	517721.088936	39.616128
2779.556826	518611.764973	39.621146
2781.493183	519502.213557	39.626164
2784.412382	520406.251642	39.631181
2786.947599	521314.178766	39.636199
2790.093492	522215.150541	39.641216
2792.666488	523132.030050	39.646234
2794.972929	524035.198488	39.651252
2798.100926	524944.371661	39.656269
2801.064106	525858.754593	39.661287
2804.062946	526765.069016	39.666304
2806.856986	527680.879236	39.671322
2809.362037	528587.013481	39.676340
2812.753782	529496.872805	39.681357
2815.284826	530422.022612	39.686375
2818.323985	531337.012230	39.691392
2820.542021	532261.594590	39.696410
2822.959697	533182.410974	39.701428
2825.592189	534098.603722	39.706445
2828.630990	535003.750034	39.711463
2831.257545	535886.160581	39.716480
2834.671339	536766.021720	39.721498
2836.870481	537664.346301	39.726516
2839.314832	538552.359712	39.731533
2841.605205	539461.273750	39.736551
2844.797255	540366.106685	39.741568
2847.468659	541282.236752	39.746586
2850.298751	542206.933405	39.751604
2853.137744	543117.584361	39.756621
2855.705574	544054.878536	39.761639
2858.577340	544976.569173	39.766656
2861.096186	545919.580351	39.771674
2864.026087	546860.749770	39.776692
2867.239561	547803.869918	39.781709
2870.317374	548747.953628	39.786727
2873.383340	549696.097147	39.791744
2876.484066	550650.905894	39.796762
2879.084866	551596.531243	39.801780
2882.279477	552555.413699	39.806797
2884.773729	553519.119133	39.811815
2887.794649	554492.067149	39.816832
2890.581162	555466.491310	39.821850
2893.520673	556450.367214	39.826868
2896.320568	557433.339632	39.831885
2898.846885	558434.473162	39.836903
2901.431084	559417.636146	39.841920
2904.307761	560417.657682	39.846938
2907.336970	561423.304705	39.851956
2910.430743	562426.603816	39.856973
2913.304525	563443.674324	39.861991
2916.407654	564458.719257	39.867008
2919.394175	565478.022935	39.872026
2922.119243	566499.348441	39.877044
2924.965638	567525.091950	39.882061
2927.271500	568564.850338	39.887079
2930.408859	569600.471253	39.892096
2933.145961	570656.655166	39.897114
2935.565277	571718.776980	39.902132
2938.660999	572778.389371	39.907149
2941.544922	573854.609147	39.912167
2944.415524	574921.154842	39.917184
2947.325435	575996.936095	39.922202
2950.216805	577075.838863	39.927220
2953.252165	578134.306813	39.932237
2956.180068	579240.106008	39.937255
2959.515786	580320.058009	39.942272
2962.451807	581408.557813	39.947290
2965.225411	582509.776105	39.952308
2968.058598	583607.425515	39.957325
2971.043588	584716.132315	39.962343
2974.156773	585817.296721	39.967360
2977.563126	586907.484216	39.972378
2980.587388	588014.980182	39.977396
2983.973481	589101.263121	39.982413
2986.260542	590212.186830	39.987431
2989.617824	591306.192814	39.992448
2993.116423	592404.083478	39.997466
2995.965563	593513.653966	40.002484
2999.001003	594605.504815	40.007501
3002.026775	595714.388173	40.012519
3005.005636	596810.101190	40.017536
3008.090142	597908.699133	40.022554
3011.605166	598994.802646	40.027572
3015.152360	600072.687052	40.032589
3018.595588	601161.653982	40.037607
3021.754022	602224.931459	40.042624
3025.258005	603271.282895	40.047642
3027.934181	604314.321855	40.052660
3031.149670	605332.200294	40.057677
3033.826679	606329.857420	40.062695
3036.870183	607340.427608	40.067712
3039.821717	608351.673329	40.072730
3042.447824	609385.347678	40.077748
3045.541989	610395.685786	40.082765
3048.559762	611431.958633	40.087783
3051.111856	612462.059845	40.092800
3054.065017	613483.696824	40.097818
3057.205489	614532.114974	40.102836
3059.278457	615586.311099	40.107853
3062.054581	616646.440485	40.112871
3064.701481	617726.187849	40.117888
3067.867238	618820.090766	40.122906
3070.388198	619923.688250	40.127924
3073.359506	621022.101294	40.132941
3076.304982	622121.956762	40.137959
3079.237040	623257.232417	40.142976
3082.327340	624380.620355	40.147994
3085.165727	625514.324430	40.153012
3087.963977	626665.599473	40.158029
3090.687613	627822.157352	40.163047
3093.463750	628994.413330	40.168064
3096.410210	630176.898914	40.173082
3098.963790	631365.558850	40.178100
3101.967545	632566.691877	40.183117
3105.127507	633780.241967	40.188135
3108.041491	634998.983037	40.193152
3111.211226	636219.136447	40.198170
3114.409306	637473.376199	40.203188
3117.997343	638703.348509	40.208205
3120.574159	639947.760183	40.213223
3123.469604	641205.886751	40.218240
3126.969208	642457.124803	40.223258
3130.369099	643723.986037	40.228276
3133.658885	644971.358945	40.233293
3136.980857	646238.218387	40.238311
3140.196412	647504.437882	40.243328
3143.534228	648760.258735	40.248346
3146.501335	650046.537088	40.253364
3149.877630	651298.743341	40.258381
3153.295815	652567.478169	40.263399
3156.522432	653835.484482	40.268416
3159.772673	655110.198974	40.273434
3163.061748	656382.600197	40.278452
3166.227154	657653.412575	40.283469
3169.789390	658932.758617	40.288487
3172.737140	660202.677553	40.293504
3176.554038	661461.931526	40.298522
3179.845786	662729.620540	40.303540
3183.663125	663967.640939	40.308557
3187.278914	665228.178426	40.313575
3190.139811	666493.352161	40.318592
3194.079003	667733.701923	40.323610
3196.727626	668973.456643	40.328628
3200.293198	670222.248704	40.333645
3203.405791	671461.302524	40.338663
3206.489934	672710.640569	40.343680
3210.189624	673951.308042	40.348698
3213.338077	675181.064740	40.353716
3216.334019	676409.491580	40.358733
3219.746461	677652.696606	40.363751
3222.658782	678889.009582	40.368768
3225.838579	680129.137487	40.373786
3228.591624	681375.428552	40.378804
3231.502760	682623.958229	40.383821
3234.954139	683855.739034	40.388839
3237.939037	685074.270764	40.393856
3241.293520	686270.134905	40.398874
3244.393834	687483.954517	40.403892
3247.428021	688679.999840	40.408909
3250.493502	689886.800420	40.413927
3253.277120	691102.269232	40.418944
3256.939431	692312.813082	40.423962
3260.321907	693546.259266	40.428980
3263.247303	694763.190345	40.433997
3266.495493	695990.912034	40.439015
3268.850968	697230.562446	40.444032
3272.240240	698486.478580	40.449050
3275.277303	699744.405161	40.454068
3278.548626	701012.571695	40.459085
3281.433857	702283.492420	40.464103
3284.719705	703570.019227	40.469120
3288.537595	704854.136569	40.474138
3291.885984	706161.672848	40.479156
3294.690704	707448.345808	40.484173
3298.113008	708750.176135	40.489191
3301.054058	710061.841256	40.494208
3304.534048	711373.760235	40.499226
3307.900266	712707.772142	40.504244
3310.927778	714036.927947	40.509261
3314.610488	715372.001770	40.514279
3317.557961	716705.847341	40.519296
3321.770434	718052.728201	40.524314
3324.964026	719401.934789	40.529332
3327.837220	720745.239064	40.534349
3331.242284	722102.578177	40.539367
3334.521270	723469.949678	40.544384
3337.647293	724840.431842	40.549402
3341.208844	726218.570850	40.554420
3344.600403	727587.117446	40.559437
3347.986395	728971.739949	40.564455
3351.419717	730348.758893	40.569472
3354.963570	731720.340029	40.574490
3358.862368	733095.778009	40.579508
3362.478384	734485.296887	40.584525
3365.842348	735859.610389	40.589543
3369.198441	737234.232333	40.594560
3372.977067	738600.109360	40.599578
3376.180665	739999.101455	40.604596
3379.561559	741379.318695	40.609613
3383.526212	742738.335424	40.614631
3387.083983	744110.055767	40.619648
3390.574969	745486.478067	40.624666
3394.027212	746875.383131	40.629684
3397.182905	748247.529590	40.634701
3400.520249	749625.021761	40.639719
3403.627818	750999.153964	40.644736
3407.751745	752376.519233	40.649754
3411.014087	753754.765670	40.654772
3414.446311	755127.812396	40.659789
3418.057597	756489.604012	40.664807
3421.360618	757863.756089	40.669824
3424.896942	759246.677262	40.674842
3428.303577	760622.478603	40.679860
3431.535663	761999.681953	40.684877
3435.421002	763380.952728	40.689895
3438.296346	764762.726562	40.694912
3442.058258	766135.690607	40.699930
3445.798602	767523.203559	40.704948
3449.047896	768885.126660	40.709965
3452.213821	770270.943336	40.714983
3455.451149	771656.144572	40.720000
3458.573979	773040.220181	40.725018
3461.817231	774422.833033	40.730023
3465.360433	775748.758711	40.735028
3468.811631	777024.299204	40.740032
3471.403056	778246.949459	40.745037
3474.440880	779404.709745	40.750042
3477.236303	780499.544838	40.755047
3480.257706	781518.319868	40.760052
3483.041439	782480.080491	40.765056
3485.753651	783386.543148	40.770061
3488.319788	784204.596507	40.775066
3490.612645	784973.038029	40.780071
3492.976478	785659.869042	40.785076
3495.320001	786288.774681	40.790080
3497.501172	786851.928452	40.795085
3499.703184	787369.468734	40.800090
3501.510922	787813.998766	40.805095
3503.282487	788222.973058	40.810100
3504.796929	788563.015284	40.815104
3506.324515	788869.080949	40.820109
3507.802559	789118.235623	40.825114
3508.657555	789337.656405	40.830119
3510.042696	789501.603208	40.835124
3511.264977	789640.463563	40.840128
3512.341315	789735.809616	40.845133
3512.626534	789803.178780	40.850138
3513.753768	789847.952722	40.855143
3514.316405	789851.692381	40.860148
3515.462711	789841.380766	40.865152
3515.756613	789790.131477	40.870157
3516.655319	789721.632881	40.875162
3517.171119	789627.989024	40.880167
3517.459904	789523.570879	40.885172
3518.111479	789388.968558	40.890176
3518.280016	789246.630105	40.895181
3518.956280	789079.535639	40.900186
3519.613760	788907.820884	40.905191
3519.845023	788719.905587	40.910196
3520.159428	788495.112110	40.915200
3520.460104	788290.464295	40.920205
3521.139656	788049.279396	40.925210
3521.212111	787798.995427	40.930215
3521.406545	787552.565554	40.935220
3521.770030	787264.219631	40.940224
3521.952439	786998.995513	40.945229
3521.697353	786709.107177	40.950234
3522.233898	786434.020995	40.955239
3522.149238	786128.300417	40.960244
3522.210719	785832.080510	40.965248
3522.219338	785527.842914	40.970253
3522.177369	785210.177680	40.975258
3522.313127	784902.303150	40.980263
3521.987299	784576.789367	40.985268
3522.368175	784259.798865	40.990272
3522.106204	783931.540582	40.995277
3522.388066	783611.931407	41.000282
3522.232429	783276.838808	41.005287
3522.331772	782948.475875	41.010292
3522.617380	782599.605564	41.015296
3522.144690	782259.796040	41.020301
3522.004956	781925.178921	41.025306
3522.056903	781585.103303	41.030311
3522.194716	781257.739181	41.035316
3522.237531	780902.677377	41.040320
3522.334870	780562.939689	41.045325
3522.139655	780207.243442	41.050330
3522.389434	779862.871807	41.055335
3522.128539	779515.960176	41.060340
3521.991559	779163.745986	41.065344
3521.950750	778828.280210	41.070349
3521.884805	778465.390510	41.075354
3522.100543	778112.328788	41.080359
3521.426753	777779.822986	41.085364
3521.447113	777423.413178	41.090368
3521.194296	777097.353118	41.095373
3520.929191	776735.542171	41.100378
3521.174875	776397.701756	41.105383
3521.092110	776049.167607	41.110388
3520.697631	775705.197805	41.115392
3520.495921	775374.424352	41.120397
3520.533745	775038.721807	41.125402
3520.263597	774707.486367	41.130407
3520.628404	774384.699188	41.135412
3520.535672	774029.324256	41.140416
3519.982702	773705.723196	41.145421
3520.353851	773374.961798	41.150426
3520.013771	773044.549296	41.155431
3519.860619	772712.268672	41.160436
3520.012809	772369.677387	41.165440
3519.752461	772046.201189	41.170445
3519.627740	771712.442264	41.175450
3519.694249	771376.518348	41.180455
3519.521369	771066.925990	41.185460
3519.220352	770725.811156	41.190464
3519.327147	770407.129108	41.195469
3519.152792	770092.569282	41.200474
3519.175354	769773.775334	41.205479
3518.621951	769455.112113	41.210484
3518.401273	769134.754053	41.215488
3518.187583	768817.239209	41.220493
3518.258231	768525.487299	41.225498
3518.398365	768215.576157	41.230503
3518.312193	767897.113806	41.235508
3518.136556	767595.311822	41.240512
3517.833424	767285.583042	41.245517
3517.969070	766982.472539	41.250522
3517.830195	766659.036778	41.255527
3517.687221	766369.651059	41.260532
3517.555136	766068.026510	41.265536
3517.376979	765775.616422	41.270541
3517.390263	765480.057263	41.275546
3517.625991	765185.139916	41.280551
3517.176203	764893.578387	41.285556
3516.943449	764600.046653	41.290560
3516.490167	764299.044847	41.295565
3516.429170	764019.416518	41.300570
3516.410148	763737.107932	41.305575
3516.079923	763462.878475	41.310580
3516.179449	763181.417082	41.315584
3516.221120	762916.870942	41.320589
3516.029921	762630.801055	41.325594
3516.085686	762355.382384	41.330599
3515.865526	762072.255387	41.335604
3515.795671	761799.500648	41.340608
3515.733310	761536.353664	41.345613
3515.628833	761248.589177	41.350618
3515.518889	760986.466804	41.355623
3515.408533	760723.003422	41.360628
3515.609495	760453.904620	41.365632
3515.115505	760192.656873	41.370637
3514.876581	759926.177478	41.375642
3515.267067	759668.613854	41.380647
3514.879653	759408.012183	41.385652
3514.851249	759144.184277	41.390656
3514.790486	758892.047240	41.395661
3514.565728	758642.100167	41.400666
3514.678092	758394.901993	41.405671
3514.492224	758126.968897	41.410676
3514.555598	757877.689322	41.415680
3514.171827	757628.278060	41.420685
3514.115521	757386.750582	41.425690
3514.042701	757138.801895	41.430695
3513.754335	756890.584616	41.435700
3514.307153	756649.722859	41.440704
3513.514533	756412.580446	41.445709
3513.906506	756159.636423	41.450714
3513.593283	755920.918652	41.455719
3513.409869	755685.627556	41.460724
3513.481760	755449.645263	41.465728
3513.424196	755220.835512	41.470733
3513.523020	754988.586558	41.475738
3512.920598	754756.397072	41.480743
3512.995389	754531.741440	41.485748
3512.953828	754297.026090	41.490752
3513.021575	754086.973401	41.495757
3512.933966	753848.993163	41.500762
3512.798328	753633.678317	41.505767
3512.555679	753404.301803	41.510772
3512.667187	753181.328908	41.515776
3512.462740	752966.451184	41.520781
3512.269046	752740.849282	41.525786
3512.364930	752532.379164	41.530791
3512.066233	752320.462130	41.535796
3512.424321	752091.342326	41.540800
3511.896174	751894.663156	41.545805
3511.744748	751685.914684	41.550810
3512.093043	751466.063464	41.555815
3511.681622	751260.211214	41.560820
3511.876506	751064.181710	41.565824
3511.534116	750861.814493	41.570829
3511.303701	750655.175274	41.575834
3511.399168	750449.958656	41.580839
3511.302938	750258.452157	41.585844
3511.334800	750053.976563	41.590848
3511.116617	749867.124287	41.595853
3510.892743	749668.263285	41.600858
3511.060594	749467.998510	41.605863
3510.810279	749288.894238	41.610868
3510.892880	749093.673348	41.615872
3510.712577	748906.742279	41.620877
3510.696005	748719.977296	41.625882
3510.644692	748526.246582	41.630887
3510.461529	748346.269493	41.635892
3510.574816	748160.556692	41.640896
3510.352675	747977.415043	41.645901
3510.267428	747802.350670	41.650906
3510.424342	747620.620471	41.655911
3510.200089	747438.059495	41.660916
3510.268297	747257.768624	41.665920
3509.809480	747090.014620	41.670925
3509.966989	746916.224588	41.675930
3509.815373	746732.992630	41.680935
3509.722315	746559.285483	41.685940
3509.638032	746386.363822	41.690944
3509.592808	746231.225191	41.695949
3509.527064	746059.034613	41.700954
3509.594353	745894.875020	41.705959
3509.247820	745728.605491	41.710964
3509.217911	745562.378968	41.715968
3509.595926	745398.355339	41.720973
3509.101615	745235.263342	41.725978
3509.356578	745071.994700	41.730983
3508.971735	744923.164278	41.735988
3509.109299	744752.740449	41.740992
3508.964349	744599.365642	41.745997
3508.903324	744444.589732	41.751002
3509.112950	744290.408741	41.756007
3508.865671	744135.212570	41.761012
3509.313677	743971.246434	41.766016
3508.805462	743832.501484	41.771021
3508.552674	743660.437475	41.776026
3508.876473	743509.782135	41.781031
3508.728759	743359.943489	41.786036
3508.470950	743203.346238	41.791040
3508.232151	743068.053869	41.796045
3508.203458	742912.105205	41.801050
3508.222199	742764.848406	41.806055
3507.910983	742626.296873	41.811060
3508.422948	742472.178658	41.816064
3508.308849	742332.649854	41.821069
3508.024869	742200.317079	41.826074
3508.122668	742060.995713	41.831079
3508.115503	741920.897988	41.836084
3508.312541	741768.103853	41.841088
3507.956798	741631.520370	41.846093
3507.713528	741497.438173	41.851098
3508.142445	741360.423609	41.856103
3507.708155	741223.648232	41.861108
3507.738794	741076.704194	41.866112
3507.501589	740951.118539	41.871117
3507.795891	740810.110518	41.876122
3507.809363	740679.681527	41.881127
3507.184735	740568.002794	41.886132
3507.370012	740421.565123	41.891136
3507.796184	740298.530464	41.896141
3507.708731	740164.152624	41.901146
3507.828076	740026.572590	41.906151
3507.210378	739894.899441	41.911156
3507.313858	739778.736295	41.916160
3507.388870	739655.601303	41.921165
3507.154512	739513.915599	41.926170
3507.202658	739388.258037	41.931175
3507.310329	739269.019686	41.936180
3507.091864	739138.949986	41.941184
3507.095701	739022.792258	41.946189
3507.006646	738899.029534	41.951194
3507.136428	738779.038108	41.956199
3507.035614	738646.566234	41.961204
3506.800853	738533.656559	41.966208
3506.877877	738417.626327	41.971213
3506.698001	738293.275497	41.976218
3506.937074	738190.425134	41.981223
3506.498269	738067.053607	41.986228
3506.867242	737946.515347	41.991232
3506.710011	737836.650599	41.996237
3506.672126	737719.194317	42.001242
3506.821280	737598.340770	42.006247
3506.340278	737499.608359	42.011252
3506.338692	737374.966343	42.016256
3506.316766	737277.540798	42.021261
3506.275977	737162.847792	42.026266
3506.180120	737062.165988	42.031271
3505.983604	736949.277043	42.036276
3506.113042	736846.180063	42.041280
3506.187023	736734.431013	42.046285
3505.918646	736635.454839	42.051290
3506.439582	736532.239633	42.056295
3506.039953	736433.678544	42.061300
3506.024310	736321.493154	42.066304
3506.117696	736212.109016	42.071309
3506.027352	736108.642946	42.076314
3506.085939	736007.773883	42.081319
3506.358242	735902.711046	42.086324
3505.833272	735799.213821	42.091328
3505.768593	735690.591048	42.096333
3506.002186	735604.881916	42.101338
3505.788941	735494.746783	42.106343
3505.535886	735401.048552	42.111348
3505.270504	735291.315187	42.116352
3505.937482	735205.876637	42.121357
3505.600562	735105.309053	42.126362
3505.830630	735012.169884	42.131367
3505.497161	734922.092543	42.136372
3505.494682	734827.950242	42.141376
3505.480509	734740.391941	42.146381
3505.576863	734643.211796	42.151386
3505.641591	734548.758130	42.156391
3505.267577	734451.999892	42.161396
3505.397035	734361.641770	42.166400
3505.526064	734272.916218	42.171405
3505.394480	734183.143734	42.176410
3505.657276	734097.067188	42.181415
3505.497326	733995.911958	42.186420
3505.593932	733905.554146	42.191424
3505.373852	733808.069686	42.196429
3505.492691	733722.012922	42.201434
3505.506280	733613.349135	42.206439
3505.271740	733537.447694	42.211444
3505.633148	733434.912135	42.216448
3505.495909	733361.567246	42.221453
3505.522438	733261.461108	42.226458
3505.758290	733159.883428	42.231463
3505.293899	733078.569852	42.236468
3505.376472	732977.708316	42.241472
3505.131788	732895.564454	42.246477
3505.286302	732798.352441	42.251482
3504.924778	732711.819675	42.256487
3505.016342	732620.260056	42.261492
3505.178524	732538.936520	42.266496
3504.970191	732466.882531	42.271501
3505.141774	732375.901058	42.276506
3505.117219	732289.011004	42.281511
3504.929202	732209.425450	42.286516
3505.198246	732123.376334	42.291520
3504.819206	732041.444039	42.296525
3505.255688	731956.801391	42.301530
3504.965565	731868.514780	42.306535
3505.131550	731790.599635	42.311540
3505.139250	731693.151017	42.316544
3505.003609	731610.183808	42.321549
3505.059593	731538.474001	42.326554
3505.059493	731449.243580	42.331559
3504.955040	731373.052709	42.336564
3504.827813	731291.417833	42.341568
3504.894003	731203.263159	42.346573
3504.498215	731130.336895	42.351578
3504.751783	731051.360254	42.356583
3504.741955	730969.009448	42.361588
3504.671927	730877.011127	42.366592
3504.634887	730812.639403	42.371597
3504.382547	730732.604264	42.376602
3504.366616	730660.155740	42.381607
3504.153985	730591.998047	42.386612
3504.452608	730507.957332	42.391616
3504.303267	730441.818381	42.396621
3504.251858	730371.056950	42.401626
3504.360950	730303.041763	42.406631
3504.408098	730235.878169	42.411636
3504.291181	730152.051017	42.416640
3504.146746	730084.373048	42.421645
3504.186372	730029.590491	42.426650
3504.473588	729945.149631	42.431655
3504.329470	729883.215051	42.436660
3504.204200	729819.246250	42.441664
3504.016886	729747.115069	42.446669
3504.017769	729680.301228	42.451674
3504.033221	729609.423059	42.456679
3504.143611	729533.872823	42.461684
3504.022667	729464.006515	42.466688
3504.080092	729397.973488	42.471693
3503.906615	729337.624570	42.476698
3504.267583	729265.547107	42.481703
3504.096511	729217.926366	42.486708
3504.098261	729139.319481	42.491712
3504.131715	729085.373627	42.496717
3504.174417	729018.398846	42.501722
3503.883615	728944.246815	42.506727
3503.974283	728876.965747	42.511732
3504.178819	728811.696192	42.516736
3504.125695	728750.084688	42.521741
3503.726029	728678.127727	42.526746
3503.842542	728620.152766	42.531751
3503.836554	728553.925238	42.536756
3503.980117	728488.365960	42.541760
3503.652689	728436.308269	42.546765
3503.690767	728379.285743	42.551770
3504.249732	728317.322139	42.556775
3503.859014	728261.608069	42.561780
3503.706617	728184.057727	42.566784
3503.712763	728132.190659	42.571789
3503.638814	728071.023307	42.576794
3503.994129	727999.975904	42.581799
3503.415888	727945.132818	42.586804
3503.608487	727885.505278	42.591808
3503.671195	727827.186802	42.596813
3504.023286	727766.590785	42.601818
3503.804126	727700.143858	42.606823
3503.409719	727638.233572	42.611828
3503.823589	727588.822264	42.616832
3503.478875	727530.866248	42.621837
3503.632631	727488.829465	42.626842
3503.460196	727423.957908	42.631847
3503.577571	727365.329851	42.636852
3503.838582	727306.182209	42.641856
3503.845426	727253.913109	42.646861
3503.479170	727194.868319	42.651866
3503.562905	727128.267602	42.656871
3503.357335	727076.924264	42.661876
3503.588577	727018.671262	42.666880
3503.417418	726963.655222	42.671885
3503.484362	726906.122200	42.676890
3503.722869	726855.199541	42.681895
3503.467855	726804.110390	42.686900
3503.775778	726738.064005	42.691904
3503.319472	726695.281674	42.696909
3503.565586	726631.523788	42.701914
3503.430208	726573.377752	42.706919
3503.649161	726525.230925	42.711924
3503.366920	726467.257048	42.716928
3503.246300	726408.364183	42.721933
3503.237231	726369.073720	42.726938
3503.514877	726304.366656	42.731943
3503.046564	726258.165145	42.736948
3503.069615	726203.607399	42.741952
3503.193088	726153.095787	42.746957
3503.225035	726106.017951	42.751962
3503.005570	726060.666106	42.756967
3502.734253	726011.358520	42.761972
3503.147888	725967.536714	42.766976
3503.027092	725921.028119	42.771981
3502.751906	725881.184680	42.776986
3503.140032	725824.928887	42.781991
3503.031207	725792.044334	42.786996
3503.108423	725738.267377	42.792001
3503.072120	725682.278955	42.797005
3502.979464	725636.358729	42.802010
3503.297410	725581.649012	42.807015
3503.055371	725538.081929	42.812020
3503.067520	725491.202054	42.817025
3503.138898	725449.217984	42.822029
3502.940395	725410.747104	42.827034
3502.780352	725346.749033	42.832039
3502.878880	725321.261537	42.837044
3503.126188	725261.258986	42.842049
3502.889834	725223.487258	42.847053
3502.977204	725185.760971	42.852058
3503.317948	725117.466123	42.857063
3503.032574	725086.837946	42.862068
3502.906493	725029.670562	42.867073
3503.172001	724997.761660	42.872077
3503.196859	724951.273061	42.877082
3502.993041	724897.933506	42.882087
3502.936475	724848.087873	42.887092
3503.032757	724814.868167	42.892097
3503.158239	724772.772589	42.897101
3503.238752	724725.133677	42.902106
3503.263020	724667.096435	42.907111
3502.981546	724629.577227	42.912116
3502.722631	724584.075071	42.917121
3502.796136	724535.593712	42.922125
3502.985182	724488.877131	42.927130
3503.197225	724449.887873	42.932135
3502.837872	724401.675497	42.937140
3503.012290	724350.599230	42.942145
3503.016303	724305.894619	42.947149
3502.934237	724259.320662	42.952154
3503.046774	724211.623928	42.957159
3502.847366	724182.712832	42.962164
3502.673084	724137.342906	42.967169
3502.937725	724091.355011	42.972173
3502.869532	724045.372300	42.977178
3502.934202	724005.364479	42.982183
3502.812374	723970.244463	42.987188
3502.788104	723913.052502	42.992193
3502.927551	723867.480556	42.997197
3502.761303	723834.498538	43.002202
3502.968870	723779.695970	43.007207
3502.921883	723748.081695	43.012212
3503.018159	723700.136869	43.017217
3502.852805	723651.392396	43.022221
3502.628898	723607.861659	43.027226
3502.776221	723564.765001	43.032231
3502.728608	723535.083066	43.037236
3502.801359	723490.362677	43.042241
3502.546301	723445.894480	43.047245
3502.422149	723409.384606	43.052250
3502.305353	723373.517721	43.057255
3502.337648	723342.285323	43.062260
3502.391451	723308.917872	43.067265
3502.601716	723282.116866	43.072269
3502.398149	723238.878224	43.077274
3502.503852	723201.536368	43.082279
3502.387042	723184.355646	43.087284
3502.381016	723145.693671	43.092289
3502.521689	723110.377912	43.097293
3502.264999	723070.022119	43.102298
3502.342563	723041.259524	43.107303
3502.087945	723015.773693	43.112308
3502.159064	722976.800768	43.117313
3502.366637	722939.341756	43.122317
3502.200903	722916.715945	43.127322
3502.364161	722880.255376	43.132327
3502.194570	722859.216271	43.137332
3502.333926	722820.330472	43.142337
3502.202247	722779.506472	43.147341
3502.296307	722744.742126	43.152346
3502.371248	722722.571716	43.157351
3502.259268	722696.763906	43.162356
3502.282153	722656.211179	43.167361
3502.301025	722628.943978	43.172365
3502.071745	722593.885433	43.177370
3502.005562	722557.957073	43.182375
3501.856745	722529.676253	43.187380
3502.388358	722512.733982	43.192385
3502.318970	722472.493035	43.197389
3502.238008	722442.911832	43.202394
3502.213451	722420.211760	43.207399
3502.023787	722387.673984	43.212404
3502.403359	722348.300119	43.217409
3502.059154	722322.331225	43.222413
3502.079078	722300.020056	43.227418
3502.255587	722263.455435	43.232423
3501.997492	722246.841417	43.237428
3502.305494	722217.343852	43.242433
3502.266390	722171.494624	43.247437
3502.146997	722145.785468	43.252442
3502.201454	722104.877806	43.257447
3501.980705	722096.189184	43.262452
3501.953952	722056.187039	43.267457
3501.850052	722024.030255	43.272461
3501.740525	722002.037124	43.277466
3501.978914	721971.261242	43.282471
3501.818466	721956.018603	43.287476
3502.040217	721935.061202	43.292481
3501.746396	721896.936704	43.297485
3501.788488	721881.313429	43.302490
3502.274647	721855.305001	43.307495
3502.084669	721833.721323	43.312500
3502.034916	721797.786949	43.317505
3502.041247	721771.510518	43.322509
3502.345837	721755.694900	43.327514
3501.980215	721726.158178	43.332519
3501.842195	721687.412052	43.337524
3501.870770	721660.834134	43.342529
3501.916737	721640.648692	43.347533
3501.504058	721629.363715	43.352538
3501.766968	721607.605453	43.357543
3501.506279	721584.446340	43.362548
3501.710364	721561.111202	43.367553
3501.669707	721547.087451	43.372557
3501.565013	721521.373928	43.377562
3501.784265	721506.166870	43.382567
3501.641916	721479.219994	43.387572
3501.952005	721458.345948	43.392577
3502.235661	721440.847536	43.397581
3501.845996	721412.701858	43.402586
3501.581863	721392.467900	43.407591
3501.560104	721366.839349	43.412596
3501.889446	721353.795279	43.417601
3501.890017	721318.891667	43.422605
3502.052891	721294.471855	43.427610
3501.931256	721275.106486	43.432615
3501.729756	721261.158410	43.437620
3501.910834	721242.883264	43.442625
3502.196937	721205.304283	43.447629
3501.567592	721182.403286	43.452634
3501.635385	721149.123982	43.457639
3501.588726	721142.884585	43.462644
3501.656681	721120.165665	43.467649
3501.731351	721087.926162	43.472653
3501.569576	721074.367850	43.477658
3502.021637	721062.691296	43.482663
3501.841379	721038.823240	43.487668
3501.555354	721023.599637	43.492673
3501.989499	720979.797585	43.497677
3501.654419	720971.771226	43.502682
3501.920221	720942.028203	43.507687
3501.782254	720928.416136	43.512692
3501.632846	720902.013945	43.517697
3502.110386	720876.945931	43.522701
3501.707945	720865.211983	43.527706
3502.009932	720826.488287	43.532711
3501.884927	720812.229324	43.537716
3501.587485	720795.965968	43.542721
3501.426767	720772.292245	43.547725
3501.407836	720771.849100	43.552730
3501.612991	720736.413411	43.557735
3501.526930	720719.470403	43.562740
3501.481412	720700.041530	43.567745
3501.219216	720669.343549	43.572749
3501.381850	720664.606273	43.577754
3501.852001	720654.661559	43.582759
3501.242481	720636.763644	43.587764
3501.172392	720611.339081	43.592769
3501.668157	720595.985500	43.597773
3501.465378	720591.506900	43.602778
3501.817758	720566.805719	43.607783
3501.287373	720551.472879	43.612788
3501.539573	720540.374042	43.617793
3501.577133	720522.121030	43.622797
3501.471356	720500.668719	43.627802
3502.067486	720489.116308	43.632807
3501.557243	720460.293147	43.637812
3501.602069	720448.385528	43.642817
3501.439857	720435.817926	43.647821
3501.391770	720410.785787	43.652826
3501.509126	720377.396036	43.657831
3501.730872	720373.144671	43.662836
3501.391897	720367.746351	43.667841
3501.361350	720342.661523	43.672845
3501.191426	720339.813654	43.677850
3501.309566	720331.761363	43.682855
3501.626783	720315.147567	43.687860
3501.326134	720284.752028	43.692865
3501.004356	720287.681104	43.697869
3501.094864	720268.774180	43.702874
3501.060992	720264.118736	43.707879
3501.178230	720246.298219	43.712884
3501.457039	720227.955110	43.717889
3501.344834	720216.568962	43.722893
3501.294286	720211.965830	43.727898
3501.993552	720194.445705	43.732903
3501.630400	720168.374018	43.737908
3501.630824	720152.357692	43.742913
3501.801266	720131.205883	43.747917
3501.508543	720119.254401	43.752922
3501.431873	720093.978102	43.757927
3501.531092	720071.697429	43.762932
3501.781442	720053.904090	43.767937
3501.581000	720043.920709	43.772941
3501.353278	720016.983195	43.777946
3501.461691	719988.304095	43.782951
3501.609409	719996.015196	43.787956
3501.610610	719973.254589	43.792961
3501.701321	719949.784909	43.797965
3501.578762	719938.697614	43.802970
3501.569346	719916.632827	43.807975
3501.389902	719904.959841	43.812980
3501.574413	719903.094584	43.817985
3501.685655	719873.075761	43.822989
3501.666431	719858.996031	43.827994
3501.433263	719837.364710	43.832999
3501.429750	719818.472303	43.838004
3501.336834	719802.421140	43.843009
3501.540808	719793.659914	43.848013
3501.436171	719768.188896	43.853018
3501.495858	719751.120653	43.858023
3501.220306	719746.554445	43.863028
3501.433900	719732.386440	43.868033
3501.827984	719712.932205	43.873037
3501.463808	719711.008812	43.878042
3501.508682	719684.620238	43.883047
3501.523250	719655.360437	43.888052
3501.087637	719638.225046	43.893057
3501.190519	719640.191568	43.898061
3501.133559	719636.134654	43.903066
3501.533252	719623.572146	43.908071
3501.463698	719601.268516	43.913076
3501.437857	719582.478441	43.918081
3501.763751	719579.895500	43.923085
3501.236544	719558.113686	43.928090
3501.690477	719528.532887	43.933095
3501.604473	719537.374007	43.938100
3501.462679	719508.932963	43.943105
3501.598420	719484.363558	43.948109
3501.266972	719481.641265	43.953114
3501.518084	719449.267078	43.958119
3501.554019	719443.954968	43.963124
3501.598144	719426.888634	43.968129
3501.589503	719407.252289	43.973133
3501.328889	719397.079712	43.978138
3501.503839	719379.247806	43.983143
3501.477833	719374.788926	43.988148
3501.657829	719346.690876	43.993153
3501.551057	719337.881343	43.998157
3501.261505	719322.109703	44.003162
3501.612300	719295.223025	44.008167
3501.633845	719290.756242	44.013172
3501.403276	719282.215062	44.018177
3501.640470	719249.644038	44.023181
3501.359523	719231.639198	44.028186
3501.391671	719221.913941	44.033191
3501.346343	719215.623286	44.038196
3501.590461	719185.332073	44.043201
3501.601158	719175.362348	44.048205
3501.350098	719178.875220	44.053210
3501.546213	719148.294255	44.058215
3501.281968	719124.632952	44.063220
3501.619003	719123.833342	44.068225
3501.762050	719087.210698	44.073229
3501.082707	719085.388831	44.078234
3501.560865	719071.820685	44.083239
3501.457299	719073.871050	44.088244
3501.709433	719038.965897	44.093249
3501.767631	719033.649847	44.098253
3501.127188	719013.819428	44.103258
3501.502471	718980.282273	44.108263
3501.266146	718976.205085	44.113268
3501.002445	718979.224200	44.118273
3501.638864	718960.323284	44.123277
3501.369401	718944.894761	44.128282
3501.302473	718920.902713	44.133287
3501.222650	718921.362209	44.138292
3501.067050	718912.857854	44.143297
3501.044042	718877.005628	44.148301
3500.939197	718872.807474	44.153306
3501.129769	718859.137729	44.158311
3500.927644	718866.114193	44.163316
3500.989606	718855.094150	44.168321
3501.354851	718858.703683	44.173325
3501.006847	718852.909115	44.178330
3501.123618	718822.042506	44.183335
3501.151496	718814.202043	44.188340
3501.268562	718806.793179	44.193345
3501.476588	718811.866936	44.198349
3500.823285	718797.443853	44.203354
3501.356575	718793.338582	44.208359
3501.330335	718769.587346	44.213364
3501.346616	718746.572928	44.218369
3501.268830	718751.148417	44.223373
3501.217930	718752.644620	44.228378
3501.420336	718732.178304	44.233383
3501.274724	718720.002121	44.238388
3501.268503	718709.141936	44.243393
3501.370446	718702.380207	44.248397
3501.037249	718687.904035	44.253402
3501.063864	718661.019296	44.258407
3500.896102	718654.897235	44.263412
3500.862832	718645.727660	44.268417
3501.363295	718644.206673	44.273421
3501.090557	718652.732423	44.278426
3501.505443	718628.610320	44.283431
3501.175670	718612.546413	44.288436
3501.042752	718602.748522	44.293441
3501.375799	718584.740010	44.298445
3501.243424	718598.350924	44.303450
3501.367336	718569.763579	44.308455
3501.043372	718547.846341	44.313460
3500.851311	718544.158389	44.318465
3501.245508	718529.115378	44.323469
3501.173743	718538.649539	44.328474
3500.852756	718531.213630	44.333479
3500.975851	718535.954422	44.338484
3501.051938	718514.665324	44.343489
3501.299538	718497.761849	44.348493
3501.237300	718494.498783	44.353498
3501.316101	718479.904570	44.358503
3501.476448	718474.372900	44.363508
3501.303011	718454.910336	44.368513
3501.318657	718431.547984	44.373517
3500.962853	718427.093501	44.378522
3501.256705	718430.814213	44.383527
3501.188776	718430.279847	44.388532
3500.890335	718398.835541	44.393537
3501.159643	718390.954785	44.398541
3500.953283	718382.408680	44.403546
3501.101887	718381.243372	44.408551
3501.003172	718373.324223	44.413556
3500.801021	718380.995445	44.418561
3501.117329	718369.684749	44.423565
3500.752654	718380.309020	44.428570
3500.935252	718354.488639	44.433575
3500.968330	718339.752948	44.438580
3500.744929	718337.706772	44.443585
3501.059966	718325.701873	44.448589
3500.422639	718333.246666	44.453594
3500.798936	718325.348168	44.458599
3501.114498	718319.096392	44.463604
3500.933306	718327.756134	44.468609
3501.133475	718317.555688	44.473613
3500.975133	718317.135450	44.478618
3500.978765	718313.613443	44.483623
3501.007844	718312.467878	44.488628
3500.835441	718286.854744	44.493633
3501.185981	718261.006322	44.498637
3501.062518	718268.317463	44.503642
3500.983958	718265.552975	44.508647
3501.159488	718263.540051	44.513652
3501.041643	718264.303447	44.518657
3501.153078	718260.515619	44.523661
3501.074798	718251.105063	44.528666
3501.206644	718232.434683	44.533671
3500.841993	718234.181216	44.538676
3500.868588	718225.993233	44.543681
3500.864374	718224.208392	44.548685
3500.676708	718217.791714	44.553690
3500.795256	718220.251958	44.558695
3501.161338	718221.282570	44.563700
3500.854475	718224.209892	44.568705
3500.968745	718216.453787	44.573709
3501.069676	718224.323054	44.578714
3501.129126	718197.133813	44.583719
3501.138862	718192.222017	44.588724
3500.795829	718179.879280	44.593729
3501.046869	718167.587146	44.598733
3501.207831	718162.104767	44.603738
3501.185077	718166.473090	44.608743
3501.282927	718165.911311	44.613748
3501.100057	718137.819566	44.618753
3501.369981	718128.351330	44.623757
3500.964706	718121.573756	44.628762
3501.239582	718115.080563	44.633767
3501.275852	718111.553078	44.638772
3501.052219	718096.760185	44.643777
3501.067224	718074.041716	44.648781
3500.940425	718065.779728	44.653786
3500.742019	718067.449224	44.658791
3500.881487	718071.939583	44.663796
3500.854899	718069.017647	44.668801
3500.977649	718053.324265	44.673805
3500.957804	718069.000574	44.678810
3501.005732	718062.544844	44.683815
3501.265645	718040.083401	44.688820
3500.820004	718030.286918	44.693825
3501.146862	718013.468566	44.698829
3500.898248	718023.429327	44.703834
3500.918293	718015.341417	44.708839
3500.947070	718015.634219	44.713844
3500.930385	718007.205181	44.718849
3501.544470	717999.217484	44.723853
3500.710115	717980.458216	44.728858
3501.188782	717961.531524	44.733863
3501.363467	717959.816260	44.738868
3500.752613	717962.942704	44.743873
3501.240819	717954.777371	44.748877
3501.026367	717959.475074	44.753882
3501.132769	717949.884863	44.758887
3501.412443	717929.899807	44.763892
3501.230447	717912.272558	44.768897
3501.233975	717909.891180	44.773901
3500.968079	717903.139994	44.778906
3501.217534	717891.938901	44.783911
3501.339740	717875.104492	44.788916
3501.142313	717858.918063	44.793921
3501.340027	717857.347771	44.798925
3501.441906	717855.594919	44.803930
3501.301493	717833.248676	44.808935
3501.342458	717823.917133	44.813940
3501.439645	717812.245100	44.818945
3501.442748	717812.145354	44.823949
3501.144623	717785.460264	44.828954
3501.239200	717752.857381	44.833959
3501.212640	717757.424947	44.838964
3501.191088	717752.766064	44.843969
3501.570831	717741.940042	44.848973
3501.394408	717719.797848	44.853978
3501.345804	717703.735326	44.858983
3501.368864	717707.451512	44.863988
3501.245790	717691.252471	44.868993
3501.606922	717662.126821	44.873997
3501.285590	717664.709521	44.879002
3501.341711	717656.317699	44.884007
3501.373066	717634.041741	44.889012
3501.118723	717622.229131	44.894017
3501.262289	717614.616431	44.899021
3501.332434	717608.553488	44.904026
3501.210847	717596.322095	44.909031
3501.119041	717577.935221	44.914036
3500.964902	717559.360203	44.919041
3501.116222	717547.530051	44.924045
3501.231733	717556.885578	44.929050
3501.193238	717556.941506	44.934055
3501.107853	717555.021132	44.939060
3500.843697	717526.643159	44.944065
3501.014318	717504.889459	44.949069
3500.850601	717513.596754	44.954074
3501.124479	717502.391106	44.959079
3501.226941	717500.737287	44.964084
3501.231157	717503.861458	44.969089
3501.474790	717493.950439	44.974093
3501.207020	717479.560559	44.979098
3501.450639	717460.175564	44.984103
3502.228067	717438.172609	44.989108
3502.619224	717405.469763	44.994113
3501.659683	717395.955865	44.999117
3501.934955	717363.321607	45.004122
3501.949977	717356.622760	45.009127
3501.585864	717325.135665	45.014132
3502.038098	717304.674181	45.019137
3501.657653	717290.401801	45.024141
3501.504267	717275.595845	45.029146
3501.675085	717253.543843	45.034151
3501.756093	717223.818124	45.039156
3501.606788	717209.705823	45.044161
3501.569424	717195.277379	45.049165
3501.171996	717180.213962	45.054170
3501.701719	717155.969443	45.059175
3501.346816	717171.107556	45.064180
3501.504435	717136.309301	45.069185
3501.571527	717126.030192	45.074189
3501.593020	717118.040385	45.079194
3501.643389	717093.478069	45.084199
3501.551936	717067.351784	45.089204
3501.443647	717064.442998	45.094209
3501.629614	717032.863901	45.099213
3501.354562	717024.923010	45.104218
3501.631507	717015.948408	45.109223
3501.576439	716991.998472	45.114228
3501.047715	716972.194332	45.119233
3501.375695	716955.968935	45.124237
3501.335590	716969.269616	45.129242
3501.076807	716949.123184	45.134247
3501.268899	716926.273129	45.139252
3501.207753	716909.566292	45.144257
3501.318801	716908.655015	45.149261
3501.417694	716912.408627	45.154266
3501.134073	716884.378929	45.159271
3501.543668	716866.304478	45.164276
3501.421343	716861.413725	45.169281
3501.604640	716853.198505	45.174285
3500.999195	716835.688570	45.179290
3501.233938	716815.013809	45.184295
3501.060480	716810.974773	45.189300
3501.351586	716812.960466	45.194305
3501.412162	716804.368634	45.199309
3501.188165	716792.748259	45.204314
3501.325737	716768.021763	45.209319
3501.347302	716758.940271	45.214324
3501.258860	716763.617816	45.219329
3501.294008	716738.213674	45.224333
3501.024636	716732.801478	45.229338
3501.297002	716726.506057	45.234343
3501.012028	716715.590138	45.239348
3501.428737	716710.312583	45.244353
3501.113622	716701.187453	45.249357
3500.970082	716691.438683	45.254362
3500.736733	716674.015738	45.259367
3501.233249	716668.973001	45.264372
3500.716764	716666.974843	45.269377
3500.861792	716668.935105	45.274381
3500.798493	716662.695105	45.279386
3500.810176	716664.330157	45.284391
3500.729449	716665.831660	45.289396
3500.975139	716666.882370	45.294401
3500.885687	716657.372655	45.299405
3500.792444	716654.262813	45.304410
3500.720324	716661.715688	45.309415
3501.095873	716650.690531	45.314420
3500.847696	716640.016467	45.319425
3500.916366	716623.089180	45.324429
3501.149336	716624.092390	45.329434
3501.154967	716617.543325	45.334439
3501.272650	716621.641211	45.339444
3500.827563	716621.813942	45.344449
3500.991775	716620.248960	45.349453
3500.989551	716600.059291	45.354458
3500.751492	716580.603045	45.359463
3501.293398	716573.915718	45.364468
3501.018145	716570.538280	45.369473
3501.022970	716569.793342	45.374477
3500.862572	716571.506456	45.379482
3500.895495	716565.845769	45.384487
3501.372049	716564.526804	45.389492
3500.816854	716544.229952	45.394497
3500.999023	716524.952169	45.399501
3501.040376	716524.201191	45.404506
3500.819066	716515.060356	45.409511
3501.293313	716506.102214	45.414516
3501.094660	716517.643940	45.419521
3501.064712	716511.299101	45.424525
3501.185722	716513.957873	45.429530
3501.121420	716489.263917	45.434535
3501.103614	716472.052971	45.439540
3501.104817	716465.008441	45.444545
3500.961730	716467.016362	45.449549
3501.065823	716472.059114	45.454554
3501.025696	716455.595938	45.459559
3501.309656	716453.018981	45.464564
3500.897565	716432.995858	45.469569
3501.090117	716424.183395	45.474573
3501.080211	716418.579294	45.479578
3501.110115	716418.475103	45.484583
3501.182021	716402.538997	45.489588
3501.011938	716421.219699	45.494593
3501.507556	716388.396418	45.499597
3501.313033	716364.864604	45.504602
3501.265329	716368.394644	45.509607
3501.393798	716352.548314	45.514612
3501.189648	716340.328731	45.519617
3501.246634	716322.112948	45.524621
3501.245682	716323.898980	45.529626
3501.239346	716321.072304	45.534631
3501.097451	716309.487300	45.539636
3501.101699	716306.013957	45.544641
3501.190418	716274.100819	45.549645
3501.206055	716260.902231	45.554650
3501.236280	716261.294074	45.559655
3501.411777	716254.419002	45.564660
3501.341666	716245.401714	45.569665
3501.404580	716229.665203	45.574669
3501.306089	716217.477589	45.579674
3501.301063	716207.754976	45.584679
3501.297131	716212.418861	45.589684
3500.921601	716172.694185	45.594689
3501.219019	716161.185207	45.599693
3501.061419	716169.793662	45.604698
3501.244251	716163.264570	45.609703
3501.384491	716160.364008	45.614708
3500.935809	716151.905274	45.619713
3501.302181	716118.110106	45.624717
3500.941999	716122.584864	45.629722
3500.948272	716117.027498	45.634727
3501.004151	716114.240081	45.639732
3500.781342	716111.300277	45.644737
3500.904323	716103.441563	45.649741
3500.721133	716111.855867	45.654746
3500.439168	716108.826619	45.659751
3500.668777	716103.133117	45.664756
3500.591077	716107.908471	45.669761
3500.603414	716098.728570	45.674765
3501.115099	716105.738193	45.679770
3501.072072	716094.979922	45.684775
3501.255381	716073.319639	45.689780
3500.778778	716064.270110	45.694785
3501.162017	716057.310937	45.699789
3501.120156	716061.485072	45.704794
3500.869308	716057.805732	45.709799
3500.960078	716054.218767	45.714804
3500.952478	716051.342598	45.719809
3500.880560	716046.046158	45.724813
3500.750685	716048.994588	45.729818
3500.771765	716021.655807	45.734823
3500.977298	716005.944919	45.739828
3500.201158	715949.417817	45.744833
3500.722702	715827.536233	45.749837
3500.729489	715668.280639	45.754842
3500.392278	715437.883373	45.759847
3500.517616	715152.379973	45.764852
3500.143514	714815.793985	45.769857
3500.042115	714414.098155	45.774861
3499.790167	713959.560296	45.779866
3499.373697	713432.423252	45.784871
3499.737991	712853.957021	45.789876
3498.813279	712230.151329	45.794881
3498.950624	711538.767573	45.799885
3498.448148	710790.942031	45.804890
3497.725106	709990.611943	45.809895
3497.550845	709126.315176	45.814900
3496.881611	708212.059068	45.819905
3496.796725	707219.888585	45.824909
3496.236216	706170.713376	45.829914
3495.470442	705063.872143	45.834919
3495.293940	703889.325294	45.839924
3494.613533	702671.176042	45.844929
3493.836106	701383.945070	45.849933
3493.022514	700033.656078	45.854938
3492.468540	698630.869817	45.859943
3491.519106	697152.153031	45.864948
3490.752437	695628.353297	45.869953
3490.443716	694024.935348	45.874957
3489.260932	692382.222492	45.879962
3488.317114	690662.643957	45.884967
3487.963184	688894.017350	45.889972
3486.634153	687067.017164	45.894977
3485.554378	685166.222662	45.899981
3484.776250	683212.097039	45.904986
3483.543106	681197.710436	45.909991
3482.929161	679116.022787	45.914996
3481.722505	676984.980877	45.920001
3480.530273	674782.373127	45.925005
3479.306181	672556.069206	45.930010
3478.129890	670240.368931	45.935015
3476.942103	667881.906223	45.940020
3475.389613	665466.542348	45.945025
3474.595303	662982.425000	45.950029
3473.268489	660457.672299	45.955034
3471.614119	657863.962682	45.960039
3470.721186	655225.988076	45.965044
3469.065323	652528.633247	45.970049
3467.803681	649765.967211	45.975053
3466.362496	646961.829554	45.980058
3464.598283	644114.665590	45.985063
3463.522423	641188.568816	45.990068
3461.678921	638227.693890	45.995073
3460.242533	635212.057178	46.000077
3458.733441	632131.236158	46.005082
3456.560463	629012.017778	46.010087
3455.183073	625836.905434	46.015092
3453.466807	622620.926134	46.020097
3451.777232	619349.558476	46.025101
3450.468101	616030.073253	46.030106
3448.303100	612655.219643	46.035111
3446.623169	609213.800584	46.040116
3444.820764	605754.188275	46.045121
3443.081332	602220.883028	46.050125
3440.815697	598637.775622	46.055130
3438.923028	595008.701822	46.060135
3437.217758	591347.127228	46.065140
3435.063580	587631.580639	46.070145
3433.345026	583858.863368	46.075149
3431.052317	580048.564903	46.080154
3428.854003	576185.061529	46.085159
3426.991039	572281.161089	46.090164
3424.803482	568348.679160	46.095169
3422.668259	564347.213564	46.100173
3420.645155	560305.919507	46.105178
3418.470268	556216.357704	46.110183
3416.270662	552081.000833	46.115188
3413.932678	547914.715933	46.120193
3411.803359	543693.837136	46.125197
3409.151579	539420.776041	46.130202
3406.966452	535119.965565	46.135207
3404.761259	530770.587025	46.140212
3402.406262	526393.238946	46.145217
3399.853757	521955.554998	46.150221
3397.204421	517483.605411	46.155226
3394.712111	512974.461550	46.160231
3392.488834	508421.930271	46.165236
3389.876788	503830.051532	46.170241
3387.292716	499202.237909	46.175245
3384.783639	494530.686782	46.180250
3381.920581	489828.969969	46.185255
3379.622493	485084.132093	46.190260
3376.496373	480308.648476	46.195265
3374.219242	475482.495058	46.200269
3371.148073	470631.817470	46.205274
3368.503375	465737.879704	46.210279
3365.717911	460819.119113	46.215284
3362.854106	455859.771697	46.220289
3360.120824	450862.491610	46.225293
3357.221245	445844.779106	46.230298
3354.027590	440786.127763	46.235303
3351.298298	435706.814324	46.240308
3347.613169	430582.376832	46.245313
3345.479024	425446.618838	46.250317
3342.548591	420265.277407	46.255322
3339.452170	415068.673926	46.260327
3336.430252	409830.432704	46.265332
3332.738539	404568.926487	46.270337
3330.225358	399268.146090	46.275341
3327.017255	393966.177363	46.280346
3323.732135	388620.765039	46.285351
3321.007613	383255.103491	46.290356
3317.505294	377859.043946	46.295361
3314.315258	372433.981497	46.300365
3311.187676	366989.138940	46.305370
3307.291519	361521.988737	46.310375
3304.162655	356031.112224	46.315380
3300.602096	350524.829516	46.320385
3297.632414	344994.737202	46.325389
3294.184592	339449.722851	46.330394
3290.640460	333880.139901	46.335399
3287.082206	328289.216502	46.340404
3283.615366	322687.586713	46.345409
3280.267720	317061.895490	46.350413
3276.566752	311443.039138	46.355418
3273.113589	305794.731924	46.360423
3269.520621	300126.064383	46.365428
3265.656606	294461.493803	46.370433
3261.868997	288765.203526	46.375437
3258.343749	283066.362652	46.380442
3254.289033	277369.985868	46.385447
3250.971809	271652.988127	46.390452
3247.070876	265931.524308	46.395457
3243.432681	260199.056549	46.400461
3239.811958	254470.570149	46.405466
3235.975213	248715.511670	46.410471
3232.123605	242965.449468	46.415476
3227.768590	237206.045366	46.420481
3223.615842	231441.050003	46.425485
3219.893695	225686.210369	46.430490
3215.775767	219919.656941	46.435495
3211.945729	214161.033076	46.440500
3207.815223	208372.023389	46.445505
3203.927084	202560.000169	46.450509
3199.733257	196801.603969	46.455514
3195.088159	191047.854997	46.460519
3191.116262	185293.637001	46.465524
3186.943694	179558.011797	46.470529
3182.731664	173825.865546	46.475533
3178.508477	168101.640353	46.480538
3173.645540	162383.855370	46.485543
3169.848160	156683.464029	46.490548
3165.219423	151000.526088	46.495553
3160.986195	145317.623259	46.500557
3156.563169	139650.648124	46.505562
3151.826092	134002.899742	46.510567
3147.354605	128375.791388	46.515572
3142.330552	122764.917849	46.520577
3137.938533	117171.452142	46.525581
3133.388242	111598.086077	46.530586
3128.448639	106058.590352	46.535591
3123.673418	100524.692744	46.540596
3118.560725	95033.932705	46.545601
3113.527207	89573.825336	46.550605
3108.700395	84138.331098	46.555610
3103.322222	78736.471230	46.560615
3098.171444	73375.177183	46.565620
3092.759826	68057.144653	46.570625
3087.237260	62770.206709	46.575629
3081.641692	57535.798074	46.580634
3075.643606	52359.536971	46.585639
3069.790126	47248.183972	46.590644
3061.980838	42215.771919	46.595649
3047.756620	37439.600394	46.600653
3032.616310	32822.544299	46.605658
3017.412388	28400.213990	46.610663
3003.313939	24182.031728	46.615668
2989.237393	20204.462926	46.620673
2976.235047	16459.826618	46.625677
2963.422615	12945.718728	46.630682
2951.047231	9686.860407	46.635687
2939.081504	6654.834764	46.640692
2926.475111	3870.663185	46.645697
2912.111869	1393.571566	46.650701
2858.486992	247.479078	46.655706
2783.637239	266.513598	46.660711
2746.229793	250.003904	46.665716
2741.601020	249.960354	46.670721
2757.262273	251.455151	46.675725
2780.286828	248.669910	46.680730
2799.699199	251.843607	46.685735
2812.027895	238.180072	46.690740
2816.294800	239.468947	46.695745
2814.300841	235.845009	46.700749
2810.136184	243.654119	46.705754
2804.789683	252.488859	46.710759
2800.038695	235.639999	46.715764
2796.740500	236.693020	46.720769
2794.432502	242.679859	46.725773
2791.942363	233.157843	46.730778
2789.291924	240.478157	46.735783
2786.546544	240.655653	46.740788
2783.861645	236.167478	46.745793
2781.028978	239.155742	46.750797
2778.422954	226.277013	46.755802
2774.876731	241.219481	46.760807
2771.970191	229.547306	46.765812
2768.192961	235.973891	46.770817
2764.899577	231.684524	46.775821
2762.301049	221.931826	46.780826
2758.971410	232.526561	46.785831
2756.036719	224.481446	46.790836
2752.598088	226.083065	46.795841
2749.195190	224.572239	46.800845
2746.248764	228.019027	46.805850
2742.658422	232.575681	46.810855
2739.701481	221.511006	46.815860
2736.125879	216.770886	46.820865
2732.551891	220.423584	46.825869
2729.442328	217.910671	46.830874
2725.983927	221.371964	46.835879
2722.708654	220.003432	46.840884
2719.586587	208.849488	46.845889
2716.228196	224.565445	46.850893
2713.145851	221.717887	46.855898
2709.263154	222.886474	46.860903
2705.930537	198.841022	46.865908
2702.391262	215.485805	46.870913
2699.288351	213.704933	46.875917
2695.800933	209.551549	46.880922
2692.262307	221.745625	46.885927
2689.214054	208.324283	46.890932
2686.136010	219.127833	46.895937
2682.118963	211.720769	46.900941
2678.683976	208.949968	46.905946
2674.792331	217.066243	46.910951
2671.609670	213.477736	46.915956
2668.347525	211.163196	46.920961
2665.335651	217.851130	46.925965
2662.206489	202.568281	46.930970
2657.866842	212.821526	46.935975
2654.201250	209.249239	46.940980
2651.246653	212.111536	46.945985
2647.797214	206.524744	46.950989
2644.326600	198.306184	46.955994
2640.865747	208.083811	46.960999
2637.358846	207.053057	46.966004
2634.036471	207.246840	46.971009
2631.163730	207.385331	46.976013
2627.258748	211.443383	46.981018
2623.613023	213.443282	46.986023
2620.211711	197.147986	46.991028
2616.905443	205.417027	46.996033
2613.324794	205.707459	47.001037
2609.690175	209.324310	47.006042
2606.352131	201.774919	47.011047
2602.889497	199.332004	47.016052
2599.189894	199.747323	47.021057
2595.943329	196.148739	47.026061
2592.663865	196.298153	47.031066
2588.856844	199.110590	47.036071
2586.166296	197.698248	47.041076
2582.195925	196.667705	47.046081
2578.554400	201.708938	47.051085
2575.261707	204.135686	47.056090
2571.613532	198.149297	47.061095
2568.087837	197.726955	47.066100
2564.961922	194.688007	47.071105
2560.991868	196.596215	47.076109
2558.025208	198.736134	47.081114
2554.322925	205.641059	47.086119
2551.378036	200.797472	47.091124
2547.537163	201.663071	47.096129
2543.774888	202.553155	47.101133
2540.620085	190.555446	47.106138
2536.661208	200.177214	47.111143
2533.297098	194.681184	47.116148
2530.114507	196.272157	47.121153
2526.579406	200.837785	47.126157
2523.199029	190.995488	47.131162
2519.491638	198.188412	47.136167
2516.244520	193.701956	47.141172
2512.145266	195.391044	47.146177
2509.094595	201.609708	47.151181
2505.661367	190.714491	47.156186
2502.304016	195.781942	47.161191
2498.560207	193.910596	47.166196
2495.106748	189.409976	47.171201
2491.499089	191.112012	47.176205
2488.337083	181.403109	47.181210
2484.249402	181.561321	47.186215
2481.288861	186.443098	47.191220
2477.781703	183.003206	47.196225
2474.329804	178.487943	47.201229
2471.140834	189.420481	47.206234
2467.589130	188.916292	47.211239
2463.931443	178.794169	47.216244
2460.354584	182.479521	47.221249
2456.307408	185.370122	47.226253
2453.482011	186.155666	47.231258
2449.875031	183.776252	47.236263
2446.634171	183.434919	47.241268
2443.113464	181.489777	47.246273
2439.221042	184.414759	47.251277
2435.972884	184.679290	47.256282
2432.391879	184.542496	47.261287
2429.091626	184.463605	47.266292
2425.628949	184.921342	47.271297
2421.373966	189.893389	47.276301
2418.314969	170.923137	47.281306
2415.016547	183.867351	47.286311
2411.388100	178.872441	47.291316
2407.987342	179.077606	47.296321
2404.262122	178.116949	47.301325
2400.784020	179.064293	47.306330
2397.669223	184.056525	47.311335
2394.052839	183.044108	47.316340
2390.799620	185.789473	47.321345
2386.983822	178.817291	47.326349
2383.534001	170.682566	47.331354
2379.959083	181.798266	47.336359
2376.570364	181.166718	47.341364
2373.003399	181.238604	47.346369
2369.825302	178.870328	47.351373
2366.262304	171.009522	47.356378
2362.538008	171.166478	47.361383
2359.019937	173.070070	47.366388
2355.528475	173.569336	47.371393
2351.772896	178.077677	47.376397
2348.497411	168.541620	47.381402
2345.044515	177.965279	47.386407
2341.731797	173.699607	47.391412
2338.202461	174.896241	47.396417
2334.316120	177.977390	47.401421
2331.014269	170.354772	47.406426
2327.626429	183.171373	47.411431
2324.218552	186.815825	47.416436
2320.512478	181.053970	47.421441
2316.856881	171.337378	47.426445
2313.764827	172.172309	47.431450
2309.846334	173.732586	47.436455
2306.571713	178.906458	47.441460
2303.412553	186.035982	47.446465
2299.684400	177.965584	47.451469
2296.161489	174.813418	47.456474
2292.103287	177.862685	47.461479
2289.308602	179.099102	47.466484
2285.704485	175.080659	47.471489
2281.955710	182.379094	47.476493
2278.793551	178.592737	47.481498
2275.252013	184.925808	47.486503
2271.441251	172.168116	47.491508
2268.572939	172.269810	47.496513
2264.796322	171.612616	47.501517
2261.630998	169.153903	47.506522
2257.844456	182.279514	47.511527
2254.214834	172.672544	47.516532
2250.540538	173.884973	47.521537
2246.487222	181.052131	47.526541
2243.398274	171.753254	47.531546
2240.028158	176.601595	47.536551
2236.970149	165.054452	47.541556
2233.457956	173.212612	47.546561
2229.610060	170.100326	47.551565
2226.108566	161.439325	47.556570
2222.682291	170.852343	47.561575
2219.255892	174.379171	47.566580
2215.512452	166.793493	47.571585
2212.162008	173.736305	47.576589
2209.172601	156.453035	47.581594
2205.222156	167.300123	47.586599
2201.855220	170.293969	47.591604
2198.440751	166.693927	47.596609
2194.446989	176.976120	47.601613
2191.081497	169.954999	47.606618
2187.056424	171.441479	47.611623
2184.135484	161.354678	47.616628
2180.853874	166.893687	47.621633
2177.251971	167.961971	47.626637
2173.867313	167.073574	47.631642
2169.977692	174.316493	47.636647
2166.351925	173.398580	47.641652
2163.114686	175.932683	47.646657
2159.446764	170.942376	47.651661
2156.656031	164.899791	47.656666
2153.034189	171.235600	47.661671
2149.809746	166.078693	47.666676
2145.927861	169.803187	47.671681
2142.128041	173.245118	47.676685
2138.540837	166.124216	47.681690
2135.033319	171.226679	47.686695
2131.500761	159.049606	47.691700
2128.417378	167.816239	47.696705
2124.696012	163.382831	47.701709
2121.800812	162.456605	47.706714
2117.638973	168.832963	47.711719
2113.886078	167.235015	47.716724
2110.470255	171.310750	47.721729
2107.151514	162.764033	47.726733
2103.572602	169.702149	47.731738
2100.245486	166.972782	47.736743
2096.816599	164.045181	47.741748
2093.427531	168.106036	47.746753
2089.377500	175.816259	47.751757
2086.632532	168.965342	47.756762
2082.557318	170.208623	47.761767
2078.957200	163.918739	47.766772
2075.420417	166.124829	47.771777
2072.101399	168.167560	47.776781
2069.152356	157.111845	47.781786
2065.468693	173.601744	47.786791
2061.727400	171.060223	47.791796
2058.246582	167.681854	47.796801
2054.073009	161.020698	47.801805
2051.023348	165.825162	47.806810
2047.271236	161.702994	47.811815
2043.957953	159.772576	47.816820
2040.818026	161.095566	47.821825
2037.523398	165.928788	47.826829
2034.087012	159.699043	47.831834
2030.174626	172.184393	47.836839
2026.885393	163.853088	47.841844
2023.303811	164.796576	47.846849
2019.154496	160.073444	47.851853
2016.483592	159.671753	47.856858
2012.306598	160.475524	47.861863
2009.267230	153.858753	47.866868
2005.699670	153.675896	47.871873
2001.801655	161.399088	47.876877
1998.656592	158.347187	47.881882
1994.816118	163.722593	47.886887
1991.509655	160.704151	47.891892
1988.584805	157.522032	47.896897
1984.868071	158.965112	47.901901
1981.493161	150.588653	47.906906
1977.787435	157.932095	47.911911
1974.226299	164.066174	47.916916
1970.488956	160.935623	47.921921
1967.422753	156.366964	47.926925
1963.747089	159.176335	47.931930
1960.073157	161.414720	47.936935
1956.732349	149.037922	47.941940
1953.187198	157.724102	47.946945
1949.493212	173.235617	47.951949
1946.392162	144.353614	47.956954
1942.568952	155.721522	47.961959
1938.859186	141.490527	47.966964
1935.688294	156.630791	47.971969
1932.459297	155.855529	47.976973
1929.005739	145.959036	47.981978
1924.876366	158.385303	47.986983
1921.746574	157.300365	47.991988
1918.284701	150.982203	47.996993
1914.464450	152.971365	48.001997
1911.168400	146.266775	48.007002
1907.482909	152.332117	48.012007
1904.320025	154.999924	48.017012
1900.544845	158.470148	48.022017
1896.848169	155.306881	48.027021
1893.701757	153.132652	48.032026
1890.156325	154.957298	48.037031
1886.794923	150.385135	48.042036
1883.119204	150.787459	48.047041
1879.558031	161.454466	48.052045
1876.217972	155.852815	48.057050
1872.443222	152.394663	48.062055
1869.408259	152.470577	48.067060
1865.519669	159.796071	48.072065
1861.722042	150.908620	48.077069
1858.648994	153.229058	48.082074
1854.983627	159.186917	48.087079
1851.374470	148.439514	48.092084
1848.049581	140.693675	48.097089
1844.719085	158.379264	48.102093
1841.418577	155.739245	48.107098
1837.352511	153.286892	48.112103
1834.080870	155.207698	48.117108
1830.701236	154.022551	48.122113
1827.180046	158.969850	48.127117
1824.033020	155.274502	48.132122
1820.254804	160.836686	48.137127
1816.930008	152.730317	48.142132
1813.190255	155.212598	48.147137
1809.354675	152.878758	48.152141
1805.986028	142.357355	48.157146
1802.565118	148.122589	48.162151
1798.802337	149.005727	48.167156
1795.468471	140.885890	48.172161
1792.181572	148.243140	48.177165
1788.567823	151.299727	48.182170
1785.124444	150.217144	48.187175
1781.238127	148.390809	48.192180
1778.192600	147.186440	48.197185
1774.415404	158.911935	48.202189
1771.466208	155.532534	48.207194
1767.669500	157.034846	48.212199
1763.951701	147.811225	48.217204
1760.485156	159.926288	48.222209
1756.716289	159.163692	48.227213
1753.750302	152.505760	48.232218
1749.894420	151.931055	48.237223
1746.618125	143.536891	48.242228
1742.987205	139.212002	48.247233
1739.306268	149.262548	48.252237
1736.136171	143.981941	48.257242
1732.556421	152.356904	48.262247
1728.797402	158.566211	48.267252
1725.845265	146.970601	48.272257
1722.178109	164.004429	48.277261
1718.674465	146.574992	48.282266
1715.230549	155.531108	48.287271
1711.449270	151.077050	48.292276
1707.670552	156.051743	48.297281
1704.357339	160.041127	48.302285
1701.145037	148.391377	48.307290
1697.670700	146.551491	48.312295
1694.141332	155.361551	48.317300
1690.466707	148.315963	48.322305
1686.923804	153.886021	48.327309
1683.479909	144.838292	48.332314
1679.593192	152.310060	48.337319
1676.506732	151.623264	48.342324
1673.110442	147.765514	48.347329
1669.631050	155.264686	48.352333
1666.295389	147.924940	48.357338
1662.452704	150.790677	48.362343
1658.581907	153.166947	48.367348
1655.338943	152.275032	48.372353
1651.463950	150.026025	48.377357
1648.484656	139.643679	48.382362
1645.027199	144.695012	48.387367
1641.484682	149.364001	48.392372
1638.167897	141.407633	48.397377
1634.272257	155.329700	48.402381
1630.712357	146.240473	48.407386
1627.492193	152.384999	48.412391
1623.976853	145.744449	48.417396
1620.560380	141.761431	48.422401
1617.171279	148.046059	48.427405
1613.935510	144.418288	48.432410
1610.049319	151.177051	48.437415
1606.716901	156.915535	48.442420
1602.811534	148.391360	48.447425
1599.287917	148.162108	48.452429
1595.758960	144.841868	48.457434
1591.915233	141.496070	48.462439
1588.575933	149.337741	48.467444
1585.687855	140.809698	48.472449
1582.246720	153.055059	48.477453
1578.770558	147.747579	48.482458
1574.954291	155.324584	48.487463
1571.265086	152.051261	48.492468
1567.913348	149.941925	48.497473
1564.439138	153.362153	48.502477
1561.133593	144.929197	48.507482
1557.435924	146.241823	48.512487
1553.708551	141.486927	48.517492
1550.561239	145.915622	48.522497
1546.491679	142.269079	48.527501
1543.266002	137.581971	48.532506
1539.924948	146.934384	48.537511
1535.972148	141.210663	48.542516
1532.858078	140.719185	48.547521
1529.240708	143.988338	48.552525
1526.172139	131.361991	48.557530
1522.608695	143.507097	48.562535
1518.876745	140.804705	48.567540
1515.517305	142.459117	48.572545
1512.140334	140.572861	48.577549
1508.690683	143.564195	48.582554
1504.669437	145.588249	48.587559
1501.298962	142.322725	48.592564
1497.904187	138.177758	48.597569
1494.063378	153.318280	48.602573
1490.567207	137.943120	48.607578
1487.312239	137.196798	48.612583
1483.610253	145.496321	48.617588
1480.411886	142.712786	48.622593
1477.049073	140.387113	48.627597
1473.640660	134.017289	48.632602
1469.401807	143.079163	48.637607
1466.048273	140.979095	48.642612
1462.786911	137.399112	48.647617
1459.016400	141.118785	48.652621
1456.075437	136.976745	48.657626
1452.444100	136.195382	48.662631
1448.687546	140.138107	48.667636
1445.275586	134.114829	48.672641
1441.542095	150.043516	48.677645
1438.305241	140.611219	48.682650
1434.566848	142.178961	48.687655
1430.995133	137.354170	48.692660
1427.666439	145.477576	48.697665
1424.268979	139.909336	48.702669
1421.195694	133.248166	48.707674
1417.429065	135.135160	48.712679
1413.764378	143.814743	48.717684
1410.559174	140.812962	48.722689
1406.509321	142.199329	48.727693
1403.437672	138.636479	48.732698
1400.028354	144.943770	48.737703
1396.044276	141.303142	48.742708
1392.870129	135.540422	48.747713
1389.231597	140.389728	48.752717
1385.682640	143.167145	48.757722
1382.094282	137.787883	48.762727
1378.440358	142.750063	48.767732
1375.233000	132.632916	48.772737
1371.786490	143.651883	48.777741
1368.561747	125.556951	48.782746
1364.611240	137.853395	48.787751
1361.115614	143.481196	48.792756
1357.696845	142.106597	48.797761
1353.879388	147.907172	48.802765
1350.778236	129.631911	48.807770
1347.279893	139.550067	48.812775
1343.746742	142.338319	48.817780
1340.282008	134.346580	48.822785
1336.385485	151.154488	48.827789
1333.358209	139.832367	48.832794
1329.819313	131.073660	48.837799
1326.015761	133.983145	48.842804
1322.897112	132.412572	48.847809
1318.961789	131.872972	48.852813
1315.586514	139.856974	48.857818
1312.780006	143.571002	48.862823
1308.768245	145.313065	48.867828
1305.434518	137.635100	48.872833
1301.505559	139.121500	48.877837
1298.327431	133.471216	48.882842
1294.205620	135.356066	48.887847
1291.209788	136.299929	48.892852
1288.022515	128.432522	48.897857
1283.767525	142.690352	48.902861
1280.830027	143.644083	48.907866
1277.164351	143.806912	48.912871
1273.415152	149.139800	48.917876
1270.186139	139.869950	48.922881
1266.612804	147.086845	48.927885
1263.485925	140.624534	48.932890
1259.491720	137.153663	48.937895
1256.055696	145.663627	48.942900
1252.450393	143.281285	48.947905
1249.156522	138.334801	48.952909
1245.583275	138.449767	48.957914
1242.356621	144.793779	48.962919
1238.278428	147.492370	48.967924
1235.147017	139.103650	48.972929
1231.509690	147.900802	48.977933
1228.277866	140.275071	48.982938
1224.537060	153.543473	48.987943
1220.974572	143.016306	48.992948
1217.698240	137.710354	48.997953
1213.934987	152.111053	49.002957
1210.643394	144.230820	49.007962
1207.201246	148.759991	49.012967
1203.606917	145.423333	49.017972
1200.253826	133.290463	49.022977
1196.415374	143.189780	49.027981
1192.902813	137.146523	49.032986
1189.887155	136.001004	49.037991
1185.983110	139.000702	49.042996
1182.630446	137.119780	49.048001
1178.950586	142.447759	49.053005
1175.702980	137.706591	49.058010
1171.946514	137.750984	49.063015
1168.096591	139.595593	49.068020
1164.883623	137.937391	49.073025
1161.512765	140.950874	49.078029
1158.266176	138.466089	49.083034
1154.614503	136.952512	49.088039
1150.918099	139.636787	49.093044
1147.476684	136.464455	49.098049
1144.110832	141.899025	49.103053
1140.330211	137.732953	49.108058
1137.074349	135.185986	49.113063
1133.199563	142.855966	49.118068
1130.054516	136.914991	49.123073
1126.327875	141.937014	49.128077
1122.863350	132.129173	49.133082
1119.184772	145.481459	49.138087
1116.168820	139.081187	49.143092
1113.028392	130.922000	49.148097
1109.494331	136.368522	49.153101
1105.616294	136.500244	49.158106
1101.902878	142.990445	49.163111
1098.658432	134.488192	49.168116
1094.992780	137.141171	49.173121
1091.386978	139.680424	49.178125
1087.941013	132.560607	49.183130
1084.561905	138.388148	49.188135
1080.727141	131.927621	49.193140
1077.420459	130.487511	49.198145
1074.037409	131.894999	49.203149
1070.091935	132.822751	49.208154
1066.901892	136.504285	49.213159
1062.783202	129.147823	49.218164
1059.700837	141.967084	49.223169
1056.526559	144.698406	49.228173
1053.493651	141.852847	49.233178
1049.810455	136.335922	49.238183
1045.766349	143.260719	49.243188
1042.739522	136.310959	49.248193
1038.689381	139.070810	49.253197
1035.248401	125.548059	49.258202
1031.748658	134.596640	49.263207
1028.280697	134.014315	49.268212
1025.074136	135.813081	49.273217
1021.407185	139.531364	49.278221
1018.021508	131.763230	49.283226
1014.253675	127.020131	49.288231
1010.985981	127.855596	49.293236
1007.712395	134.078513	49.298241
1003.960263	131.143964	49.303245
1000.092667	131.638538	49.308250
996.945870	135.904365	49.313255
993.361715	131.318669	49.318260
990.073221	131.591053	49.323265
986.048338	132.299015	49.328269
982.804799	136.923482	49.333274
979.489218	135.763570	49.338279
975.575426	134.173881	49.343284
972.332147	138.202952	49.348289
968.608934	135.280017	49.353293
965.362287	139.846801	49.358298
962.233288	140.906749	49.363303
958.505117	140.167966	49.368308
955.094077	136.500391	49.373313
951.201210	132.131337	49.378317
947.969825	131.454568	49.383322
944.365205	129.846556	49.388327
940.479399	133.382585	49.393332
937.537821	137.376018	49.398337
933.661221	142.737656	49.403341
930.268254	131.535600	49.408346
927.170843	136.582034	49.413351
923.153902	128.078903	49.418356
920.020904	129.331357	49.423361
915.817011	133.702638	49.428365
912.864341	135.043176	49.433370
909.593096	134.599004	49.438375
905.690441	134.577342	49.443380
902.574556	128.811700	49.448385
898.735501	129.261381	49.453389
895.209491	121.463382	49.458394
891.841299	125.745314	49.463399
887.968615	123.675092	49.468404
884.522347	130.482856	49.473409
881.171733	130.586266	49.478413
878.044598	127.482987	49.483418
874.363975	128.666137	49.488423
870.354887	130.463453	49.493428
867.258379	133.119065	49.498433
863.638097	141.849955	49.503437
860.685880	132.880082	49.508442
856.937527	136.408179	49.513447
853.031752	130.552674	49.518452
849.599977	131.714275	49.523457
845.939076	132.086486	49.528461
842.796233	129.100101	49.533466
839.348423	135.843435	49.538471
835.931658	133.666013	49.543476
832.442669	134.297416	49.548481
828.304248	131.590755	49.553485
825.040599	127.593757	49.558490
821.589915	123.178675	49.563495
817.930743	126.383173	49.568500
815.074648	126.490394	49.573505
811.585747	131.144082	49.578509
807.993080	128.111430	49.583514
804.316156	131.493135	49.588519
800.520130	141.100018	49.593524
797.179518	127.648666	49.598529
793.270060	134.773751	49.603533
790.251180	130.077644	49.608538
786.834541	132.179656	49.613543
782.997581	126.182762	49.618548
779.961888	121.456700	49.623553
776.086445	129.220648	49.628557
772.490845	115.039490	49.633562
768.879600	130.792697	49.638567
765.510581	130.036120	49.643572
762.528276	126.423847	49.648577
758.829469	129.185253	49.653581
755.340119	122.805475	49.658586
751.771019	118.374205	49.663591
747.799641	120.341606	49.668596
744.718899	122.705007	49.673601
740.663385	130.991234	49.678605
737.784296	123.117172	49.683610
734.535389	131.394804	49.688615
730.690109	127.701258	49.693620
726.812413	120.926586	49.698625
723.258601	127.676955	49.703629
720.117123	123.375805	49.708634
716.891314	125.551177	49.713639
713.291491	121.581677	49.718644
710.051379	123.239058	49.723649
706.113948	134.005554	49.728653
702.609173	127.037171	49.733658
698.801748	136.724179	49.738663
695.041986	128.882108	49.743668
692.303202	120.393971	49.748673
688.644926	130.249609	49.753677
685.192564	123.334309	49.758682
681.482383	126.508922	49.763687
677.921842	129.201667	49.768692
674.640865	121.079439	49.773697
670.846880	127.716993	49.778701
667.250224	125.662541	49.783706
664.312947	125.906885	49.788711
660.658491	128.746861	49.793716
657.378052	124.635388	49.798721
653.362710	135.068547	49.803725
649.853903	127.166111	49.808730
646.589984	125.759930	49.813735
642.809076	124.346846	49.818740
639.851906	120.502975	49.823745
636.340267	124.616143	49.828749
632.487447	123.073324	49.833754
629.106628	120.586823	49.838759
625.115114	135.055886	49.843764
621.687262	118.687406	49.848769
618.468644	121.584107	49.853773
614.919115	117.616617	49.858778
611.815855	127.152041	49.863783
608.207052	125.913668	49.868788
604.932535	123.940960	49.873793
600.950977	118.029252	49.878797
597.248340	131.082051	49.883802
594.041361	121.514173	49.888807
590.300191	128.256302	49.893812
587.218743	119.787659	49.898817
583.395518	125.520042	49.903821
579.621863	118.201175	49.908826
576.336429	118.845777	49.913831
573.051495	127.592460	49.918836
569.571022	119.608049	49.923841
565.787282	126.886520	49.928845
562.008415	124.974317	49.933850
559.276241	120.664342	49.938855
555.471951	123.784451	49.943860
552.237728	116.830890	49.948865
548.595772	128.732466	49.953869
544.682099	126.972908	49.958874
541.218650	120.330336	49.963879
537.689851	128.857458	49.968884
534.610718	123.327182	49.973889
530.939782	127.981546	49.978893
527.672383	119.706639	49.983898
524.063737	124.110311	49.988903
520.227579	133.238465	49.993908
516.726556	121.938747	49.998913
513.370396	117.658042	50.003917
509.913377	120.206860	50.008922
506.583981	118.580796	50.013927
502.856387	120.878753	50.018932
499.237104	117.321182	50.023937
495.605840	127.926908	50.028941
492.484844	121.011625	50.033946
489.282465	123.256112	50.038951
485.510313	120.224185	50.043956
481.848735	117.780504	50.048961
478.375734	113.883516	50.053965
474.785203	111.647874	50.058970
471.219002	115.741832	50.063975
467.405208	120.603501	50.068980
464.346723	115.696593	50.073985
460.808420	123.813520	50.078989
457.645036	112.606979	50.083994
453.971285	114.611287	50.088999
450.140959	124.025258	50.094004
446.711527	117.261494	50.099009
443.349998	123.523734	50.104013
439.798680	120.491090	50.109018
436.765355	119.009301	50.114023
432.518782	125.844992	50.119028
429.016648	110.979730	50.124033
425.653261	120.887250	50.129037
422.354883	116.365757	50.134042
418.745030	114.830560	50.139047
415.226137	125.047884	50.144052
412.060106	105.670225	50.149057
408.669407	117.432298	50.154061
405.058434	114.239892	50.159066
401.549718	114.752816	50.164071
397.501009	120.835801	50.169076
394.208531	121.027468	50.174081
390.390378	128.574668	50.179085
387.324949	119.575875	50.184090
383.877676	112.846317	50.189095
380.231875	123.584992	50.194100
376.690052	116.039185	50.199105
373.058488	127.442689	50.204109
369.407470	120.877228	50.209114
366.320141	111.391524	50.214119
362.720846	122.422238	50.219124
359.610482	115.081045	50.224129
355.923174	127.131409	50.229133
352.434327	124.239631	50.234138
348.677886	125.757733	50.239143
345.049871	127.675221	50.244148
341.920697	125.368592	50.249153
338.163088	120.642658	50.254157
334.525513	119.381706	50.259162
331.467501	118.286144	50.264167
327.465104	120.642750	50.269172
324.275425	115.874581	50.274177
320.580271	119.647923	50.279181
317.090093	118.065712	50.284186
313.925675	114.178399	50.289191
310.137453	119.799259	50.294196
306.933483	112.104455	50.299201
302.977245	125.991531	50.304205
299.851544	120.518928	50.309210
296.469509	115.664341	50.314215
292.532189	116.820840	50.319220
289.246542	109.387672	50.324225
285.565496	109.196832	50.329229
282.001855	110.934569	50.334234
278.600012	116.539219	50.339239
274.861391	112.389572	50.344244
271.629168	114.434957	50.349249
268.403174	115.322934	50.354253
264.251158	120.298417	50.359258
261.290448	117.655832	50.364263
257.789685	116.391171	50.369268
254.220336	116.711842	50.374273
250.749891	118.694606	50.379277
247.228413	116.220189	50.384282
243.603134	119.083533	50.389287
240.008961	123.094341	50.394292
236.672496	120.777647	50.399297
233.124369	113.995930	50.404301
229.513730	116.952365	50.409306
226.203467	112.321144	50.414311
222.274484	126.987772	50.419316
219.117054	123.926801	50.424321
215.714560	121.605903	50.429325
211.805945	122.139274	50.434330
209.017754	121.896456	50.439335
205.283084	122.673450	50.444340
201.758351	117.363538	50.449345
198.095958	123.469168	50.454349
194.744818	124.210072	50.459354
191.251527	112.029907	50.464359
187.463251	118.524095	50.469364
184.066649	118.318060	50.474369
180.453954	123.831934	50.479373
176.710078	112.035402	50.484378
173.493767	109.880153	50.489383
170.041107	124.567331	50.494388
166.513116	107.295441	50.499393
163.067034	120.086534	50.504397
159.659620	122.375825	50.509402
156.615574	112.592650	50.514407
152.355362	119.742297	50.519412
148.958967	110.466221	50.524417
145.510598	122.431475	50.529421
141.774196	122.749230	50.534426
138.453689	116.094362	50.539431
135.432285	120.221824	50.544436
131.716625	118.159853	50.549441
127.885896	113.912399	50.554445
124.517859	113.089544	50.559450
120.846161	109.106145	50.564455
117.302967	125.361621	50.569460
113.899003	110.296875	50.574465
110.558529	116.571877	50.579469
107.064939	115.737934	50.584474
104.006150	116.690619	50.589479
100.267952	120.431858	50.594484
96.446735	110.357378	50.599489
92.770389	104.687781	50.604493
89.707582	111.304610	50.609498
86.361779	110.793829	50.614503
82.299641	121.983792	50.619508
78.762655	114.616671	50.624513
75.003221	110.130888	50.629517
71.497252	106.998922	50.634522
68.313738	112.619760	50.639527
64.690199	116.693033	50.644532
61.428022	115.144019	50.649537
58.366106	116.912642	50.654541
54.517899	119.135970	50.659546
51.021411	113.327790	50.664551
47.331836	114.560787	50.669556
43.739292	112.103908	50.674561
40.517026	125.087008	50.679565
36.635479	124.058711	50.684570
33.675995	114.489121	50.689575
29.880214	128.546326	50.694580
26.087049	113.748429	50.699585
22.703098	117.087309	50.704589
19.312936	122.238547	50.709594
15.810982	114.241701	50.714599
12.452655	120.265983	50.719604
9.343157	121.357217	50.724609
5.775600	119.588072	50.729613
1.981503	123.676336	50.734618