Fri Jun 17 17:11:19 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.996882	84.254765	0.000000
1.002368	72.845248	0.005005
1.004170	76.297645	0.010010
1.228385	78.666029	0.015014
0.735576	80.668549	0.020019
0.478764	61.164648	0.025024
0.529262	52.607403	0.030029
0.383149	54.853028	0.035034
-0.272738	49.180779	0.040038
-0.108954	40.048431	0.045043
-0.247288	31.469502	0.050048
-0.429151	13.628157	0.055053
-1.029690	10.355746	0.060058
-1.558079	3.226341	0.065062
-1.636449	-1.629025	0.070067
-2.283837	-2.564345	0.075072
-2.487836	-4.784188	0.080077
-2.955798	-3.926383	0.085082
-3.717306	-4.131947	0.090086
-3.214123	-8.705096	0.095091
-3.553130	-1.918001	0.100096
-3.320682	-4.192628	0.105101
-3.623922	-11.110614	0.110106
-4.844875	-3.930659	0.115110
-4.853575	-2.647968	0.120115
-4.951919	2.599211	0.125120
-5.147176	-4.540964	0.130125
-5.181721	3.416219	0.135130
-5.597670	-9.391927	0.140134
-5.752767	-5.688117	0.145139
-6.379927	0.837656	0.150144
-6.432508	-5.804095	0.155149
-6.706919	-9.988308	0.160154
-7.185707	-10.631777	0.165158
-7.113281	0.872415	0.170163
-6.911427	-5.461955	0.175168
-7.133104	0.867958	0.180173
-8.010184	0.735476	0.185178
-8.193230	-4.897735	0.190182
-8.324655	-7.932186	0.195187
-8.520972	3.022512	0.200192
-8.622342	-4.746180	0.205197
-8.781288	-3.207639	0.210202
-9.692128	0.619026	0.215206
-9.812285	-6.685773	0.220211
-10.129300	-8.557681	0.225216
-10.221362	-2.742641	0.230221
-10.092020	-3.389117	0.235226
-10.492338	-4.817588	0.240230
-10.771189	-7.225674	0.245235
-10.967952	-2.791916	0.250240
-11.286820	-8.732487	0.255245
-11.446465	-2.290343	0.260250
-11.574014	-1.113795	0.265254
-12.158807	-7.062854	0.270259
-13.079250	-1.140513	0.275264
-13.003076	-10.360485	0.280269
-13.168222	-2.782180	0.285274
-13.153079	0.619044	0.290278
-12.796639	3.279195	0.295283
-13.359086	5.884487	0.300288
-13.624073	0.720927	0.305293
-14.016990	-4.069525	0.310298
-14.767266	-6.017021	0.315302
-14.639791	-7.359766	0.320307
-15.066915	-0.640705	0.325312
-14.811928	-2.844882	0.330317
-14.519287	-1.933534	0.335322
-15.733469	-1.214342	0.340326
-15.987786	-8.138684	0.345331
-16.314325	-3.242122	0.350336
-16.073308	-9.244972	0.355341
-16.514889	-7.497837	0.360346
-17.616651	-9.077691	0.365350
-17.662870	-6.311542	0.370355
-18.019256	-3.551261	0.375360
-17.271008	2.452662	0.380365
-17.539769	-3.224317	0.385370
-18.082681	-7.311805	0.390374
-18.083399	-1.480770	0.395379
-18.433558	3.525687	0.400384
-19.048514	-7.088402	0.405389
-19.520566	-2.684069	0.410394
-19.921511	-7.130815	0.415398
-19.562336	-2.555428	0.420403
-19.678480	6.151365	0.425408
-19.681925	0.753908	0.430413
-20.038447	-0.753868	0.435418
-20.917494	-1.485710	0.440422
-21.040593	0.320375	0.445427
-21.258028	-0.869926	0.450432
-21.212357	2.998438	0.455437
-21.384298	-0.237266	0.460442
-21.719579	3.839853	0.465446
-22.085326	3.834710	0.470451
-22.691210	3.816203	0.475456
-22.762190	-9.021455	0.480461
-22.963011	-0.179233	0.485466
-23.209003	-3.858660	0.490470
-23.111061	-2.705385	0.495475
-23.582736	7.383808	0.500480
-24.299543	0.231264	0.505485
-24.350781	1.325076	0.510490
-24.502518	7.803205	0.515494
-24.169889	5.542708	0.520499
-24.282815	4.739170	0.525504
-24.872304	-2.187871	0.530509
-25.788848	9.291470	0.535514
-26.337330	-2.478389	0.540518
-26.265507	-3.514505	0.545523
-26.450423	-2.444058	0.550528
-26.428053	-7.274331	0.555533
-26.169378	-0.690773	0.560538
-26.723784	0.358015	0.565542
-27.147457	1.732968	0.570547
-27.962711	4.563210	0.575552
-28.017064	4.778033	0.580557
-27.951342	-2.215885	0.585562
-28.282821	-0.201709	0.590566
-27.849190	-4.622604	0.595571
-28.050941	-1.562823	0.600576
-28.693926	4.583945	0.605581
-29.271287	2.664936	0.610586
-29.704202	5.893973	0.615590
-29.717118	-1.794505	0.620595
-29.859839	-0.968855	0.625600
-29.996141	1.010708	0.630605
-30.369218	-4.181451	0.635610
-31.041889	7.757390	0.640614
-30.833824	-6.909936	0.645619
-31.208979	4.329440	0.650624
-31.107550	11.392016	0.655629
-31.194727	-1.378231	0.660634
-32.179979	-1.585077	0.665638
-32.357336	6.602450	0.670643
-32.778018	14.507396	0.675648
-32.748703	3.314590	0.680653
-32.791395	-0.377714	0.685658
-33.086643	-7.163827	0.690662
-32.939632	0.752716	0.695667
-33.796003	-2.075788	0.700672
-34.079022	-2.589983	0.705677
-34.297000	4.429582	0.710682
-34.672984	6.535418	0.715686
-34.454185	-8.561111	0.720691
-34.539131	-4.709912	0.725696
-34.887401	0.846193	0.730701
-35.607809	1.622829	0.735706
-36.010977	5.562051	0.740710
-35.985317	-1.853614	0.745715
-35.950059	6.906550	0.750720
-36.275972	3.230737	0.755725
-36.405879	-5.911173	0.760730
-37.003914	3.054895	0.765734
-37.086858	-1.564686	0.770739
-37.341750	3.631358	0.775744
-37.291380	1.973662	0.780749
-37.987785	-3.842980	0.785754
-39.019558	4.579118	0.790758
-38.643166	-2.274437	0.795763
-38.971815	0.283707	0.800768
-39.280308	3.502916	0.805773
-39.079536	4.031317	0.810778
-39.270192	0.540813	0.815782
-39.203981	5.919689	0.820787
-39.740633	8.450052	0.825792
-40.358810	4.754742	0.830797
-40.292945	-6.142807	0.835802
-40.837345	4.293739	0.840806
-40.404384	-6.839863	0.845811
-41.162600	11.258887	0.850816
-41.944771	2.942300	0.855821
-41.826702	-6.418624	0.860826
-42.421020	0.303563	0.865830
-42.083316	-3.777764	0.870835
-42.626395	-0.934549	0.875840
-42.601379	-1.136659	0.880845
-42.363790	-1.201241	0.885850
-42.790258	4.468898	0.890854
-43.149417	-4.009760	0.895859
-43.483671	0.494806	0.900864
-43.787763	4.897272	0.905869
-44.647755	3.957438	0.910874
-45.216728	0.290655	0.915878
-44.599195	0.022021	0.920883
-45.225358	2.693950	0.925888
-45.599887	-1.846378	0.930893
-45.654147	-8.964597	0.935898
-45.701458	5.547683	0.940902
-45.693614	-4.474332	0.945907
-45.772078	3.962955	0.950912
-46.223697	6.636852	0.955917
-46.423568	-1.918209	0.960922
-47.240098	7.624081	0.965926
-47.044246	-0.564406	0.970931
-47.174235	5.629107	0.975936
-47.345325	-0.454821	0.980941
-47.847718	-4.837143	0.985946
-48.178876	0.589826	0.990950
-48.198013	-3.427252	0.995955
-48.660342	7.804121	1.000960
-49.402653	3.138449	1.005965
-49.887516	0.202611	1.010970
-49.671880	10.827765	1.015974
-49.491267	-1.153662	1.020979
-50.259249	3.166471	1.025984
-50.285521	6.919712	1.030989
-49.967987	-6.620893	1.035994
-49.938546	3.268969	1.040998
-50.844816	2.263226	1.046003
-51.577229	2.613059	1.051008
-51.460684	1.472619	1.056013
-51.755842	-6.841246	1.061018
-52.019844	8.671217	1.066022
-52.094375	0.275682	1.071027
-52.905833	2.334324	1.076032
-53.339002	3.799065	1.081037
-52.620092	3.305394	1.086042
-53.220573	0.863752	1.091046
-53.319406	-1.905573	1.096051
-53.626320	7.758611	1.101056
-53.763372	-1.574905	1.106061
-54.393386	4.742770	1.111066
-54.847291	5.155038	1.116070
-54.795289	6.296019	1.121075
-55.124291	-0.962814	1.126080
-55.537489	0.327126	1.131085
-55.049063	3.486286	1.136090
-55.616920	-0.378802	1.141094
-55.442430	-6.291661	1.146099
-56.398607	-0.266087	1.151104
-56.640196	0.655720	1.156109
-56.835035	3.213132	1.161114
-57.142796	10.490933	1.166118
-56.973764	1.648211	1.171123
-57.319560	0.484381	1.176128
-58.156629	3.631419	1.181133
-58.307321	-14.625707	1.186138
-58.699575	3.894084	1.191142
-58.655406	-2.774205	1.196147
-58.639688	-0.729928	1.201152
-58.673722	-4.091560	1.206157
-58.247153	-1.129120	1.211162
-59.480634	6.107795	1.216166
-59.787087	-3.148424	1.221171
-60.220839	-0.294176	1.226176
-60.032156	4.117741	1.231181
-60.185262	0.559429	1.236186
-60.868851	1.861561	1.241190
-60.839881	-2.416098	1.246195
-61.656666	5.697951	1.251200
-61.625359	-3.400901	1.256205
-61.796032	-11.854840	1.261210
-61.886312	5.697956	1.266214
-61.765679	0.112144	1.271219
-62.572643	-0.888200	1.276224
-63.043135	1.173359	1.281229
-62.999456	-10.033464	1.286234
-62.951978	-16.279614	1.291238
-62.931840	-12.294928	1.296243
-63.919388	-8.743803	1.301248
-64.961912	-3.951205	1.306253
-64.405100	-6.068016	1.311258
-64.485224	6.816801	1.316262
-64.879181	-3.735743	1.321267
-64.608119	-1.133828	1.326272
-65.045844	-5.198932	1.331277
-65.042202	-1.816321	1.336282
-65.937347	2.199750	1.341286
-66.018422	-15.627318	1.346291
-66.285401	0.909384	1.351296
-66.633622	-1.829930	1.356301
-66.323220	-5.408261	1.361306
-67.423287	2.131284	1.366310
-67.683360	-7.630113	1.371315
-67.936724	-6.279323	1.376320
-67.624911	1.436366	1.381325
-68.040183	-6.082412	1.386330
-68.037233	0.428606	1.391334
-68.108233	3.011016	1.396339
-68.116594	-2.454292	1.401344
-68.752021	0.946938	1.406349
-69.408389	1.849489	1.411354
-69.668234	1.186209	1.416358
-69.621184	-1.854622	1.421363
-69.965079	0.860174	1.426368
-70.450482	-5.487428	1.431373
-70.789978	-5.277299	1.436378
-71.538286	5.370151	1.441382
-71.489014	-1.677862	1.446387
-71.485718	2.390139	1.451392
-71.160929	-7.965361	1.456397
-71.412978	-5.879336	1.461402
-71.740146	1.728270	1.466406
-71.840201	-10.690742	1.471411
-72.604108	-4.233991	1.476416
-73.310652	-1.667885	1.481421
-73.163551	-7.378860	1.486426
-73.324790	-5.952809	1.491430
-72.696632	-4.558527	1.496435
-73.543744	-11.354520	1.501440
-74.046382	-6.928326	1.506445
-74.246923	-9.778223	1.511450
-74.472782	-2.578965	1.516454
-74.712558	-1.966084	1.521459
-74.943279	-7.714299	1.526464
-75.797320	-3.194564	1.531469
-75.873039	-7.534540	1.536474
-76.295733	-3.138210	1.541478
-76.128493	-6.414308	1.546483
-76.124002	2.881193	1.551488
-75.949761	-6.685214	1.556493
-76.060701	-1.327609	1.561498
-76.802057	-5.017430	1.566502
-77.103575	0.691927	1.571507
-77.416332	-5.679242	1.576512
-77.745742	-1.055109	1.581517
-78.264364	3.453467	1.586522
-79.078512	14.575598	1.591526
-78.942557	-6.724871	1.596531
-78.406731	-1.106759	1.601536
-79.377459	3.006930	1.606541
-79.275398	-5.807683	1.611546
-79.479032	0.357418	1.616550
-79.693194	-9.996299	1.621555
-79.529158	-4.264288	1.626560
-80.462525	-5.722735	1.631565
-80.590201	-4.275426	1.636570
-81.450261	-3.709404	1.641574
-81.041523	-1.648570	1.646579
-81.273482	-8.706265	1.651584
-81.618846	-0.052345	1.656589
-81.018472	0.205586	1.661594
-81.930731	-1.391740	1.666598
-82.377313	4.512228	1.671603
-82.722897	-3.451078	1.676608
-82.686197	-0.092118	1.681613
-82.402576	-10.004275	1.686618
-83.827206	-7.192110	1.691622
-84.264784	-12.044584	1.696627
-84.099492	-8.702069	1.701632
-84.371320	-4.930310	1.706637
-84.089450	-2.437148	1.711642
-84.727762	4.145544	1.716646
-84.483006	-7.346106	1.721651
-84.458542	-17.117892	1.726656
-85.210417	-6.094137	1.731661
-85.738102	-3.013325	1.736666
-85.954042	0.215758	1.741670
-86.084638	-14.218449	1.746675
-85.931142	-7.562363	1.751680
-86.265616	-7.875995	1.756685
-86.542253	-9.449336	1.761690
-87.484992	-6.885601	1.766694
-87.391609	-14.715267	1.771699
-87.804300	-3.839062	1.776704
-88.110782	1.104095	1.781709
-87.869294	-12.960601	1.786714
-87.742815	-2.958614	1.791718
-88.346549	-9.718300	1.796723
-88.632730	-7.221874	1.801728
-88.760967	-2.037217	1.806733
-88.762993	-5.740617	1.811738
-89.966534	-1.788911	1.816742
-90.451911	-3.609538	1.821747
-90.099876	-0.437972	1.826752
-90.487028	-1.696352	1.831757
-90.117059	3.890527	1.836762
-90.526052	2.776869	1.841766
-90.957212	-4.576269	1.846771
-91.526733	-3.976650	1.851776
-92.192335	-7.984331	1.856781
-91.873398	-11.291172	1.861786
-92.292827	-0.585522	1.866790
-92.453144	-8.847006	1.871795
-92.427122	0.131747	1.876800
-92.475339	-9.558501	1.881805
-92.326415	-10.537381	1.886810
-93.299033	-2.639355	1.891814
-93.265831	-2.300362	1.896819
-93.646950	-5.011116	1.901824
-94.543136	-1.588833	1.906829
-94.600834	-8.588867	1.911834
-95.220232	-1.175794	1.916838
-95.026529	-5.230225	1.921843
-95.015962	1.574141	1.926848
-95.307431	-0.054946	1.931853
-95.094378	-7.198064	1.936858
-95.188461	1.266283	1.941862
-95.802241	-0.309223	1.946867
-96.344995	-3.455651	1.951872
-97.032514	-2.696705	1.956877
-96.900809	-8.620408	1.961882
-97.204928	1.564853	1.966886
-97.105986	-3.819624	1.971891
-97.583207	-11.250939	1.976896
-98.612841	-2.005134	1.981901
-98.446537	-9.494886	1.986906
-98.607649	2.970443	1.991910
-98.617567	-8.607922	1.996915
-98.376192	1.061550	2.006912
-98.416524	-3.608811	2.016909
-98.258703	-7.923858	2.026906
-97.270227	2.643528	2.036902
-97.191768	-4.894949	2.046899
-96.638404	-3.335789	2.056896
-95.865903	-0.221124	2.066893
-95.735050	-2.746914	2.076890
-95.320765	0.075798	2.086886
-94.350916	3.178996	2.096883
-94.249500	-6.150641	2.106880
-92.967024	-7.806454	2.116877
-92.743566	-2.985467	2.126874
-92.550098	-0.127429	2.136870
-92.734295	0.822097	2.146867
-91.432259	-2.746814	2.156864
-91.191540	-8.860812	2.166861
-90.043399	-2.967337	2.176858
-89.794668	-1.039621	2.186854
-89.952136	-1.996086	2.196851
-89.229532	-0.425739	2.206848
-88.396093	-3.428125	2.216845
-88.363224	-7.227256	2.226842
-87.514312	-5.961835	2.236838
-87.127757	-2.732626	2.246835
-86.529485	-0.782007	2.256832
-85.442470	-1.199471	2.266829
-85.108736	-10.340900	2.276826
-85.352350	-6.180244	2.286822
-84.952273	-4.534152	2.296819
-84.167367	-4.760319	2.306816
-83.801458	-1.788093	2.316813
-82.632904	-8.010294	2.326810
-82.305040	-2.483307	2.336806
-82.363296	-10.272117	2.346803
-81.166913	-2.427417	2.356800
-80.684513	-7.301643	2.366797
-80.561012	-4.918425	2.376794
-80.034661	-6.233569	2.386790
-79.352322	-4.452817	2.396787
-79.161790	-10.896538	2.406784
-79.012940	0.967677	2.416781
-77.731292	-0.862065	2.426778
-77.405976	3.574685	2.436774
-77.316307	-4.119575	2.446771
-76.082180	-0.877540	2.456768
-75.932253	-7.136291	2.466765
-75.575714	2.050124	2.476762
-74.904433	-0.528160	2.486758
-74.652636	-2.251711	2.496755
-73.724131	-4.398158	2.506752
-73.469862	-3.457898	2.516749
-73.022170	-7.446315	2.526746
-72.647677	-0.627766	2.536742
-71.710891	1.353125	2.546739
-71.395671	-8.206871	2.556736
-71.282887	-2.388851	2.566733
-70.212083	-5.968317	2.576730
-70.080291	1.002015	2.586726
-69.794242	-6.638940	2.596723
-68.469166	-4.651860	2.606720
-67.975655	-2.281740	2.616717
-67.802236	-6.804868	2.626714
-68.105679	0.516605	2.636710
-67.339730	-2.904106	2.646707
-66.515332	-5.982043	2.656704
-65.524365	-4.836453	2.666701
-65.150869	-3.850019	2.676698
-64.647649	-3.362511	2.686694
-64.602778	0.607338	2.696691
-64.377712	0.165018	2.706688
-63.414468	-3.276436	2.716685
-63.130215	-6.258063	2.726682
-62.201480	-4.814643	2.736678
-61.752297	-3.168214	2.746675
-61.741176	-5.403015	2.756672
-61.147448	-6.044728	2.766669
-60.436568	-1.263269	2.776666
-60.109286	-3.920503	2.786662
-59.389847	-4.572245	2.796659
-58.837283	-1.936706	2.806656
-58.623772	-1.839083	2.816653
-57.821914	-3.380020	2.826650
-57.074104	-6.157541	2.836646
-57.068118	-0.130505	2.846643
-56.714938	1.390809	2.856640
-55.800241	0.769243	2.866637
-55.458600	-1.846712	2.876634
-54.762700	-7.009333	2.886630
-54.303514	-0.466460	2.896627
-53.929094	1.079182	2.906624
-53.493745	-8.478456	2.916621
-52.879552	2.845868	2.926618
-52.246981	-9.987499	2.936614
-52.104435	-8.077301	2.946611
-51.635322	-4.229344	2.956608
-50.843790	-0.328485	2.966605
-50.576846	-2.842517	2.976602
-49.555245	0.724317	2.986598
-49.141606	0.849530	2.996595
-49.050592	4.113843	3.006592
-48.877587	1.367853	3.016589
-47.908561	1.791567	3.026586
-47.372906	-1.455317	3.036582
-46.419145	-3.038890	3.046579
-46.472263	-9.501979	3.056576
-45.873226	-5.292108	3.066573
-45.605086	-7.685417	3.076570
-44.615388	-4.113477	3.086566
-44.556593	-5.213576	3.096563
-44.208395	2.454615	3.106560
-43.322714	2.484766	3.116557
-42.801801	-0.189045	3.126554
-42.468753	-4.324967	3.136550
-41.440798	-2.782250	3.146547
-41.168812	-3.784219	3.156544
-41.144060	-4.083581	3.166541
-40.853997	-1.715797	3.176538
-39.676798	-0.569937	3.186534
-39.414587	-2.135965	3.196531
-39.096742	-8.856918	3.206528
-38.515845	-8.201925	3.216525
-37.930496	-5.156708	3.226522
-36.883125	-3.995195	3.236518
-36.966465	-2.319915	3.246515
-36.608022	1.062953	3.256512
-35.936843	-11.545460	3.266509
-35.098447	-3.725802	3.276506
-35.107663	-2.219330	3.286502
-34.306743	-2.493790	3.296499
-33.643041	-1.517655	3.306496
-33.456084	1.853806	3.316493
-33.071871	-6.562979	3.326490
-32.284873	-9.599917	3.336486
-32.209467	-0.936794	3.346483
-31.131349	-0.491494	3.356480
-30.412536	-1.452939	3.366477
-30.423573	-3.116400	3.376474
-30.118700	-7.940761	3.386470
-29.230906	-10.841523	3.396467
-28.950906	-5.051888	3.406464
-28.482463	-6.501833	3.416461
-27.167287	-5.693458	3.426458
-27.321741	-7.140237	3.436454
-26.911396	-1.461772	3.446451
-26.770820	-4.704234	3.456448
-25.578678	-4.584734	3.466445
-25.190887	-9.265996	3.476442
-25.128369	-4.461719	3.486438
-24.515845	-7.916392	3.496435
-23.507863	-1.584273	3.506432
-23.122470	-5.347360	3.516429
-23.033340	-8.981575	3.526426
-22.109041	-5.134786	3.536422
-22.009735	-3.839787	3.546419
-21.679406	0.051398	3.556416
-20.639717	-3.340712	3.566413
-20.580907	-6.052901	3.576410
-19.684894	-8.674853	3.586406
-19.003182	-4.619398	3.596403
-19.029685	-1.436516	3.606400
-18.649115	-6.529134	3.616397
-17.454129	-3.423820	3.626394
-17.437194	-5.012303	3.636390
-16.973194	-5.771743	3.646387
-15.778035	-0.348203	3.656384
-15.650372	-7.404854	3.666381
-15.517416	-1.652025	3.676378
-15.263741	-2.886865	3.686374
-14.063645	-1.238987	3.696371
-14.092184	-11.794572	3.706368
-13.385064	-8.551459	3.716365
-12.369523	-6.362349	3.726362
-12.297228	-12.838974	3.736358
-12.266961	-10.274286	3.746355
-11.489350	-4.551157	3.756352
-10.864334	-3.147733	3.766349
-10.065909	-8.762864	3.776346
-9.643654	-7.127759	3.786342
-9.665855	1.232493	3.796339
-8.920379	0.063504	3.806336
-8.284490	-1.373569	3.816333
-7.890876	-2.801590	3.826330
-7.200378	-7.021029	3.836326
-6.522603	-4.615929	3.846323
-6.267781	-2.922171	3.856320
-6.128386	0.615858	3.866317
-5.465164	-0.559612	3.876314
-4.907669	6.402803	3.886310
-4.365819	20.570561	3.896307
-3.750686	11.992487	3.906304
-3.507989	19.565408	3.916301
-2.980411	29.086387	3.926298
-2.647166	36.304619	3.936294
-2.233638	51.991426	3.946291
-1.782090	67.436013	3.956288
-1.329822	81.473098	3.966285
-0.653036	93.902469	3.976282
-0.484641	114.077137	3.986278
0.000000	132.901401	3.991283
0.367526	144.248315	3.996288
0.532834	154.412486	4.001293
0.761022	155.238258	4.006298
0.627991	158.947911	4.011302
0.743071	153.517478	4.016307
0.686168	153.900460	4.021312
0.788586	158.214088	4.026317
0.565910	155.642916	4.031322
0.955070	175.661432	4.036326
0.937821	177.734498	4.041331
1.298772	171.521414	4.046336
0.811248	173.520305	4.051341
1.111275	179.121453	4.056346
1.259950	174.480881	4.061350
1.354268	183.705919	4.066355
1.159805	152.948255	4.071360
0.790871	155.459245	4.076365
0.663496	156.840411	4.081370
1.081582	176.239031	4.086374
0.920090	189.143451	4.091379
1.252181	179.769335	4.096384
1.405985	190.402136	4.101389
1.386708	189.626829	4.106394
1.400224	185.253808	4.111398
1.062986	180.067267	4.116403
1.353891	168.923407	4.121408
0.961939	166.783521	4.126413
1.333595	170.915650	4.131418
1.346837	167.278141	4.136422
0.749720	174.657591	4.141427
1.149377	181.811970	4.146432
1.060309	183.561704	4.151437
0.822163	181.545239	4.156442
0.879170	176.888329	4.161446
1.189939	191.178472	4.166451
1.661233	184.051344	4.171456
1.340474	186.063168	4.176461
1.127114	194.179227	4.181466
1.248329	193.056745	4.186470
0.691507	187.872758	4.191475
1.181381	183.158698	4.196480
1.503744	198.766492	4.201485
1.530761	212.024203	4.206490
1.454914	194.861222	4.211494
1.192891	202.616360	4.216499
1.938958	204.047318	4.221504
1.429016	197.762305	4.226509
1.064016	194.792092	4.231514
1.541559	195.479333	4.236518
1.724522	206.740543	4.241523
1.235595	206.222872	4.246528
1.816169	206.992444	4.251533
1.687258	207.178222	4.256538
1.509121	193.612083	4.261542
1.343785	187.055688	4.266547
1.637984	207.570932	4.271552
1.550017	213.252566	4.276557
1.683981	220.339631	4.281562
1.881506	213.537025	4.286566
1.643376	199.971774	4.291571
1.728890	202.212073	4.296576
1.507032	195.519635	4.301581
1.262544	197.829387	4.306586
1.768436	217.016130	4.311590
1.553186	225.115351	4.316595
1.985348	222.710804	4.321600
1.922015	220.354278	4.326605
1.627656	218.051544	4.331610
1.499641	206.957554	4.336614
1.375417	213.164006	4.341619
1.794537	220.276687	4.346624
1.916084	223.453469	4.351629
1.628142	222.949554	4.356634
2.153671	221.346254	4.361638
2.250075	223.891799	4.366643
2.029197	213.311903	4.371648
1.926878	199.771044	4.376653
1.646617	197.070513	4.381658
1.547658	190.761592	4.386662
1.817599	200.342843	4.391667
1.815287	208.269515	4.396672
2.256699	219.854424	4.401677
1.878797	220.107635	4.406682
2.370371	215.382430	4.411686
2.123722	207.042815	4.416691
1.819865	190.964594	4.421696
1.639825	191.803165	4.426701
1.610850	200.921032	4.431706
1.979651	218.503347	4.436710
1.918315	221.122273	4.441715
2.147066	221.098629	4.446720
2.138186	225.374337	4.451725
1.921607	234.366919	4.456730
1.984001	229.869531	4.461734
2.001743	226.775706	4.466739
2.157478	229.201475	4.471744
2.115593	228.273833	4.476749
1.846171	227.553916	4.481754
2.264302	214.082828	4.486758
2.161352	232.544155	4.491763
2.054366	221.274583	4.496768
1.995336	231.440375	4.501773
2.249271	237.268049	4.506778
2.084933	222.957219	4.511782
1.976174	238.699068	4.516787
2.026901	221.793064	4.521792
1.952550	228.609678	4.526797
1.912397	229.057761	4.531802
2.098082	230.913978	4.536806
1.884419	233.887575	4.541811
1.982472	221.930549	4.546816
2.320471	237.535586	4.551821
2.232965	243.957751	4.556826
2.590502	235.080799	4.561830
2.419338	233.672626	4.566835
2.314870	226.588687	4.571840
2.076753	226.126021	4.576845
1.986786	245.399209	4.581850
2.660597	254.214604	4.586854
2.489761	260.310618	4.591859
2.670927	245.489456	4.596864
2.737753	234.118169	4.601869
2.327733	240.304449	4.606874
2.539912	224.422215	4.611878
1.985480	236.094908	4.616883
2.288852	228.469775	4.621888
2.157005	239.344857	4.626893
2.469522	249.869030	4.631898
2.515810	256.973447	4.636902
2.282027	262.585799	4.641907
2.451509	260.826580	4.646912
2.487674	257.663778	4.651917
2.482534	263.474336	4.656922
2.797211	254.084718	4.661926
2.384950	265.106672	4.666931
2.585846	254.957676	4.671936
2.930062	257.943928	4.676941
2.575319	255.110133	4.681946
2.983723	256.700032	4.686950
2.954717	253.861824	4.691955
2.591344	241.540829	4.696960
2.460814	235.056576	4.701965
2.240979	257.623368	4.706970
2.614242	255.804428	4.711974
2.716167	268.227246	4.716979
2.837730	266.419751	4.721984
2.888405	268.157121	4.726989
2.645770	270.698050	4.731994
2.947851	260.868293	4.736998
3.044692	271.232967	4.742003
2.761920	254.892272	4.747008
2.764952	248.480140	4.752013
2.498546	252.630728	4.757018
2.667053	252.509747	4.762022
2.678436	268.491745	4.767027
2.594294	271.738048	4.772032
2.836564	263.874609	4.777037
2.616538	268.967068	4.782042
3.056667	262.175621	4.787046
2.764209	264.990836	4.792051
3.171734	262.152098	4.797056
2.928751	272.259888	4.802061
2.802109	273.006904	4.807066
3.129882	265.859589	4.812070
2.605884	270.145350	4.817075
2.832944	269.325149	4.822080
2.856954	269.854921	4.827085
2.785013	277.020833	4.832090
3.140632	266.890118	4.837094
2.849780	269.991203	4.842099
2.794230	268.324838	4.847104
3.041832	268.065995	4.852109
3.072795	272.784426	4.857114
2.946957	268.152552	4.862118
3.051844	267.766468	4.867123
2.802496	267.036503	4.872128
2.890278	272.402417	4.877133
2.722509	277.692408	4.882138
2.937925	283.150974	4.887142
3.152689	290.079007	4.892147
3.181136	299.251719	4.897152
3.385986	286.634171	4.902157
3.214031	294.104231	4.907162
3.525383	281.272637	4.912166
2.739896	292.234890	4.917171
3.134284	281.135318	4.922176
3.384526	285.358501	4.927181
3.113722	293.931717	4.932186
3.053268	287.051188	4.937190
3.279711	295.808356	4.942195
3.331653	292.105777	4.947200
3.155838	285.260408	4.952205
3.335839	292.690321	4.957210
3.146434	294.914168	4.962214
3.239366	294.397660	4.967219
3.392491	281.097053	4.972224
3.605334	283.094002	4.977229
3.515637	293.957578	4.982234
3.672509	282.339222	4.987238
3.667084	280.420223	4.992243
3.334611	268.967080	4.997248
3.348688	269.505804	5.002253
3.153299	269.434651	5.007258
3.425183	272.233621	5.012262
3.453362	287.892178	5.017267
3.244693	290.338268	5.022272
3.342206	281.760847	5.027277
3.207609	284.638826	5.032282
3.553194	285.711693	5.037286
2.801296	285.470386	5.042291
3.222621	288.607221	5.047296
3.702966	290.658375	5.052301
3.402472	286.123804	5.057306
3.814612	288.137158	5.062310
3.559615	288.441970	5.067315
3.596015	285.244194	5.072320
3.724799	280.497573	5.077325
3.690862	291.851729	5.082330
3.962217	283.290207	5.087334
3.467674	287.912071	5.092339
3.471125	289.828383	5.097344
3.270313	284.209266	5.102349
3.362789	286.144919	5.107354
3.551960	294.884009	5.112358
3.576219	292.958101	5.117363
3.526591	284.396847	5.122368
3.712744	293.068357	5.127373
3.501982	300.765295	5.132378
3.913574	300.248707	5.137382
3.631346	308.845930	5.142387
3.863806	311.366902	5.147392
3.926385	308.350660	5.152397
3.622356	301.490482	5.157402
3.889153	296.314801	5.162406
3.553510	305.668801	5.167411
3.761478	311.211496	5.172416
4.059187	306.890069	5.177421
3.782033	315.800413	5.182426
3.992035	307.380896	5.187430
4.126946	315.115897	5.192435
3.740704	309.753934	5.197440
3.626697	299.039196	5.202445
4.056260	312.741184	5.207450
4.138931	311.609904	5.212454
4.156840	311.303200	5.217459
3.865998	295.823790	5.222464
3.958076	291.000978	5.227469
3.794372	296.211760	5.232474
4.266192	310.543326	5.237478
4.213660	303.662066	5.242483
4.014720	289.285489	5.247488
3.999878	288.510625	5.252493
3.885518	291.931662	5.257498
3.712820	291.245986	5.262502
4.217911	303.655693	5.267507
4.539315	302.801063	5.272512
3.991310	287.122867	5.277517
3.738315	294.316907	5.282522
4.055696	298.756857	5.287526
3.957703	314.506467	5.292531
4.314870	317.396646	5.297536
4.091570	302.961748	5.302541
4.057034	316.503878	5.307546
4.137950	312.751289	5.312550
4.194145	323.248851	5.317555
4.032278	310.152524	5.322560
4.019283	320.022415	5.327565
3.930005	319.527311	5.332570
3.890863	311.403568	5.337574
3.731859	318.133256	5.342579
4.110969	313.701800	5.347584
4.577312	316.008467	5.352589
4.240547	320.978462	5.357594
4.254828	313.685501	5.362598
3.723597	320.763590	5.367603
4.130574	334.761803	5.372608
4.667026	333.102410	5.377613
4.419490	342.265567	5.382618
4.682464	337.763225	5.387622
4.641768	326.872099	5.392627
4.399358	321.547005	5.397632
4.458282	317.507987	5.402637
4.166614	316.401236	5.407642
4.287742	318.774162	5.412646
4.244311	322.429297	5.417651
4.287465	335.083150	5.422656
4.471044	341.092859	5.427661
4.432156	342.986220	5.432666
4.755284	345.602043	5.437670
4.595984	341.416951	5.442675
4.227700	340.371872	5.447680
4.538307	345.634668	5.452685
4.389140	354.744778	5.457690
4.971905	344.208227	5.462694
4.646381	349.909268	5.467699
4.496193	346.162128	5.472704
4.500396	344.538314	5.477709
4.447923	339.008384	5.482714
4.634531	334.347251	5.487718
4.647701	346.662338	5.492723
4.552006	342.766822	5.497728
4.756065	345.914128	5.502733
4.601500	354.239344	5.507738
4.541474	335.988032	5.512742
4.327519	347.721434	5.517747
4.570693	348.733972	5.522752
4.709143	350.466827	5.527757
4.618842	348.481217	5.532762
4.925776	346.028398	5.537766
4.424840	345.128899	5.542771
4.654961	348.154655	5.547776
4.582555	352.501935	5.552781
4.314910	345.563070	5.557786
4.614774	336.537580	5.562790
4.755144	338.402132	5.567795
4.894437	355.662613	5.572800
4.775767	342.728590	5.577805
4.681236	362.994887	5.582810
4.967430	362.039150	5.587814
4.999201	369.535770	5.592819
4.961223	367.008061	5.597824
5.057203	353.874760	5.602829
4.568305	352.178587	5.607834
5.122293	361.559594	5.612838
5.225287	373.966138	5.617843
4.919691	364.515957	5.622848
4.811578	349.028421	5.627853
5.001069	354.084415	5.632858
5.007068	355.500064	5.637862
4.748801	357.715435	5.642867
4.951637	365.755698	5.647872
5.165854	373.517408	5.652877
5.227411	371.410056	5.657882
4.909552	366.776719	5.662886
4.969531	363.220000	5.667891
5.105615	371.579797	5.672896
5.406116	368.951823	5.677901
5.446156	372.080614	5.682906
5.273356	355.704167	5.687910
4.832979	340.663183	5.692915
4.804969	344.477970	5.697920
5.284842	353.972129	5.702925
5.404438	367.949663	5.707930
5.375960	350.387911	5.712934
5.241178	353.223901	5.717939
5.007554	342.586635	5.722944
5.052974	341.725778	5.727949
4.984588	363.666664	5.732954
5.349586	363.017316	5.737958
5.522837	368.673350	5.742963
5.294149	363.039695	5.747968
5.470776	351.259149	5.752973
5.043322	353.765097	5.757978
5.095716	355.300514	5.762982
5.195827	366.313944	5.767987
5.236650	367.615666	5.772992
5.575773	363.603276	5.777997
5.567185	374.796594	5.783002
5.196772	373.453691	5.788006
5.340817	373.912998	5.793011
5.600362	367.565729	5.798016
5.609316	364.825188	5.803021
5.327888	377.806138	5.808026
5.628181	372.134484	5.813030
5.272655	364.878100	5.818035
5.570663	374.830326	5.823040
5.348534	367.259909	5.828045
5.362340	378.451876	5.833050
5.826247	368.129638	5.838054
5.405680	374.283190	5.843059
5.647188	377.021712	5.848064
5.364934	369.650927	5.853069
5.570628	379.123777	5.858074
5.345596	373.391238	5.863078
5.266248	377.693501	5.868083
5.684809	365.503121	5.873088
5.494498	372.777356	5.878093
5.398084	370.450380	5.883098
5.357871	367.308538	5.888102
5.231053	376.482238	5.893107
5.579432	372.687152	5.898112
5.338159	370.117850	5.903117
4.929622	380.930486	5.908122
5.441354	382.321477	5.913126
5.731770	403.297995	5.918131
5.811119	396.157575	5.923136
6.176313	395.853926	5.928141
5.615520	390.101411	5.933146
5.894214	388.830194	5.938150
6.052636	373.427587	5.943155
5.927288	386.132972	5.948160
6.104043	373.519628	5.953165
5.613361	372.282754	5.958170
5.549026	373.041521	5.963174
5.682620	369.811588	5.968179
5.383722	371.976092	5.973184
5.899336	375.650210	5.978189
6.014973	395.626857	5.983194
6.230388	397.892165	5.988198
5.783745	382.259975	5.993203
5.417715	384.518322	5.998208
6.306176	389.953860	6.003213
5.867160	387.410516	6.008218
6.261007	365.617122	6.013222
5.878472	370.476141	6.018227
5.778393	380.263455	6.023232
6.074886	373.467812	6.028237
5.746168	378.563770	6.033242
5.866210	376.182661	6.038246
5.982669	377.309602	6.043251
5.782221	383.938857	6.048256
5.818157	378.883217	6.053261
5.630227	377.268049	6.058266
5.731986	378.424271	6.063270
6.156172	378.516738	6.068275
5.960252	384.045090	6.073280
6.047663	381.975276	6.078285
5.838896	374.162674	6.083290
6.131639	370.649554	6.088294
5.695210	375.388277	6.093299
5.708775	376.703609	6.098304
5.881152	368.962242	6.103309
5.899512	381.414235	6.108314
6.247573	372.982194	6.113318
6.099029	370.423331	6.118323
5.682312	374.743582	6.123328
6.053089	376.221149	6.128333
6.115348	383.293961	6.133338
6.471608	369.321330	6.138342
6.182825	374.401373	6.143347
5.934469	375.200988	6.148352
6.060217	373.616762	6.153357
5.947493	373.116673	6.158362
6.062852	363.748869	6.163366
6.126502	372.074331	6.168371
5.637784	358.099481	6.173376
5.547300	361.671277	6.178381
5.974470	372.444855	6.183386
6.438218	370.688021	6.188390
5.798740	364.609175	6.193395
5.237396	361.775758	6.198400
5.848339	365.521448	6.203405
5.825796	373.374805	6.208410
5.709190	369.794943	6.213414
5.902660	375.063997	6.218419
6.009013	365.418261	6.223424
6.002300	367.530253	6.228429
5.986616	371.872057	6.233434
6.157767	379.111869	6.238438
5.971020	370.422396	6.243443
5.745600	374.240007	6.248448
5.829336	365.254173	6.253453
5.937226	368.322352	6.258458
6.088994	364.762611	6.263462
5.964830	361.751152	6.268467
5.335985	353.807691	6.273472
5.890858	362.972864	6.278477
5.731603	376.802772	6.283482
5.792820	375.692222	6.288486
5.881464	366.311689	6.293491
5.661260	374.707618	6.298496
5.865001	375.137663	6.303501
5.708461	370.290437	6.308506
5.790661	370.193668	6.313510
5.819133	381.889564	6.318515
6.055154	376.458291	6.323520
6.376796	373.648410	6.328525
6.137535	382.911844	6.333530
6.079806	375.743304	6.338534
5.941280	369.367675	6.343539
6.095719	371.522936	6.348544
5.833011	351.819352	6.353549
5.409179	354.597219	6.358554
5.913360	363.270965	6.363558
5.804461	373.460334	6.368563
5.674959	372.296037	6.373568
5.954369	372.500382	6.378573
6.007318	375.274586	6.383578
5.946300	370.528503	6.388582
5.800909	371.354220	6.393587
5.530198	374.018825	6.398592
6.029423	370.519339	6.403597
5.910765	371.969128	6.408602
5.995869	375.794525	6.413606
5.938000	370.437953	6.418611
5.980085	384.391088	6.423616
6.230658	376.437213	6.428621
5.685073	365.567225	6.433626
5.597477	363.642929	6.438630
5.856560	376.720128	6.443635
5.944749	374.751813	6.448640
5.862887	376.301851	6.453645
5.771435	380.860099	6.458650
5.995721	376.885539	6.463654
6.157654	369.766135	6.468659
5.939536	371.801179	6.473664
5.921899	366.619075	6.478669
5.585965	364.885637	6.483674
5.758532	368.059099	6.488678
5.628785	368.867416	6.493683
5.735421	368.073738	6.498688
6.476078	366.686666	6.503693
6.167539	375.454851	6.508698
5.877105	354.711174	6.513702
5.737961	341.110599	6.518707
5.783961	349.933705	6.523712
6.007559	358.044711	6.528717
5.827498	366.270767	6.533722
6.029724	368.355529	6.538726
6.073926	360.057474	6.543731
5.382851	347.821053	6.548736
5.582945	362.098177	6.553741
6.079311	365.809827	6.558746
6.015539	369.716603	6.563750
6.166320	373.253629	6.568755
5.709364	359.004530	6.573760
6.141817	358.733906	6.578765
5.708858	354.855766	6.583770
5.610113	352.859916	6.588774
5.928274	358.363395	6.593779
5.944570	374.422831	6.598784
6.186926	372.677338	6.603789
5.577220	355.738088	6.608794
5.602167	366.533720	6.613798
6.088236	375.285274	6.618803
5.806259	373.094123	6.623808
5.912668	374.245231	6.628813
5.906161	376.045794	6.633818
6.180827	363.913274	6.638822
5.396462	356.837299	6.643827
5.996972	370.149603	6.648832
6.285156	366.020764	6.653837
5.939067	359.029416	6.658842
6.033115	346.741236	6.663846
6.157892	336.066704	6.668851
5.484274	339.789292	6.673856
5.799987	337.478281	6.678861
5.943588	336.209393	6.683866
5.343898	343.143370	6.688870
5.796986	351.454216	6.693875
5.620652	367.157699	6.698880
6.103082	363.979112	6.703885
6.039353	372.461908	6.708890
6.083617	367.911647	6.713894
6.309275	356.897689	6.718899
5.739590	352.136503	6.723904
5.882780	335.966855	6.728909
5.832313	334.599193	6.733914
5.931735	339.614899	6.738918
5.834688	332.966382	6.743923
5.568145	341.158451	6.748928
5.739727	346.144800	6.753933
5.917639	365.544111	6.758938
5.995091	370.721150	6.763942
6.382766	353.317753	6.768947
5.873624	353.644482	6.773952
5.860380	332.526000	6.778957
5.477486	351.373811	6.783962
5.797301	340.446434	6.788966
5.826208	359.644555	6.793971
6.137461	370.172968	6.798976
6.006372	356.530981	6.803981
5.960705	349.490296	6.808986
5.717716	340.398150	6.813990
5.694939	352.767565	6.818995
5.734335	357.672089	6.824000
5.899077	361.179756	6.829005
6.076189	373.630221	6.834010
5.903096	363.457474	6.839014
5.994047	348.340601	6.844019
5.741337	345.816421	6.849024
5.692832	341.796239	6.854029
5.702195	356.838754	6.859034
5.942367	367.363192	6.864038
6.026924	372.496623	6.869043
5.777845	373.112835	6.874048
6.035361	374.642577	6.879053
6.123242	365.458521	6.884058
6.010834	357.918416	6.889062
6.070554	348.673337	6.894067
5.803339	345.560744	6.899072
5.979756	335.219810	6.904077
5.531806	339.652396	6.909082
5.768330	339.220949	6.914086
5.955203	349.203469	6.919091
5.719119	350.134639	6.924096
6.031014	341.126683	6.929101
5.667281	357.667224	6.934106
5.919405	362.405361	6.939110
6.156833	360.284172	6.944115
5.426217	354.988115	6.949120
6.136589	365.077221	6.954125
5.944388	367.852506	6.959130
5.717134	370.287884	6.964134
6.026096	361.242515	6.969139
6.240559	355.668409	6.974144
6.026693	341.819375	6.979149
5.303951	350.838730	6.984154
5.680494	351.581049	6.989158
6.084726	369.262828	6.994163
6.031258	365.879676	6.999168
5.992211	351.209470	7.004173
5.620962	347.451711	7.009178
5.744733	351.582269	7.014182
6.111475	360.775158	7.019187
5.949325	365.067697	7.024192
5.677392	344.299449	7.029197
5.568981	359.670175	7.034202
5.613947	364.779005	7.039206
5.837202	369.727961	7.044211
5.871847	376.390757	7.049216
6.264590	366.831212	7.054221
6.156955	363.102254	7.059226
5.992728	355.979249	7.064230
6.214769	349.006944	7.069235
5.830478	340.844450	7.074240
5.663200	336.264239	7.079245
5.830051	333.854636	7.084250
5.696180	340.591010	7.089254
6.067294	353.400530	7.094259
5.790034	351.426063	7.099264
5.736000	338.498468	7.104269
5.899875	343.959110	7.109274
5.843874	354.815352	7.114278
6.202756	341.830371	7.119283
6.032145	341.818641	7.124288
6.002557	338.261423	7.129293
5.699138	339.274233	7.134298
5.735298	335.799230	7.139302
5.916927	337.885439	7.144307
5.687924	336.888645	7.149312
5.797161	339.675983	7.154317
6.190557	352.652692	7.159322
6.192296	350.441620	7.164326
6.007615	340.702191	7.169331
5.750492	351.745781	7.174336
6.095065	337.714933	7.179341
6.107978	341.297166	7.184346
5.801955	336.172675	7.189350
6.097901	342.048266	7.194355
5.968095	342.945195	7.199360
5.689304	341.849918	7.204365
5.650939	342.788678	7.209370
5.851498	346.278548	7.214374
5.815115	340.694833	7.219379
5.636280	343.384024	7.224384
5.728198	336.723436	7.229389
5.789514	353.226082	7.234394
5.616711	343.255175	7.239398
5.834054	350.921041	7.244403
6.152570	369.008778	7.249408
6.050779	352.423985	7.254413
5.794306	350.960716	7.259418
5.913521	338.470037	7.264422
5.901640	344.571831	7.269427
5.502351	354.652966	7.274432
6.004121	357.058536	7.279437
6.191002	357.106973	7.284442
6.012687	355.007525	7.289446
5.886347	345.051390	7.294451
5.737495	341.039599	7.299456
5.891883	337.829108	7.304461
5.869888	336.690557	7.309466
5.773130	350.728899	7.314470
5.906442	346.805580	7.319475
5.723304	338.089477	7.324480
5.842894	339.433754	7.329485
5.771834	345.421260	7.334490
6.036381	351.661225	7.339494
5.848803	346.631300	7.344499
5.702076	346.761235	7.349504
6.093152	344.529655	7.354509
5.922344	346.098224	7.359514
6.005121	341.126375	7.364518
6.003013	338.661776	7.369523
5.848945	338.871865	7.374528
5.681141	334.608662	7.379533
5.768531	334.009798	7.384538
5.810727	339.794363	7.389542
5.936953	331.243913	7.394547
5.700469	348.303598	7.399552
6.513858	343.298127	7.404557
6.009398	347.092254	7.409562
5.996855	348.916313	7.414566
6.276241	341.795161	7.419571
5.920436	338.320975	7.424576
6.199790	335.409397	7.429581
6.040265	346.288366	7.434586
5.881423	346.049717	7.439590
5.875529	336.997889	7.444595
5.644340	343.475156	7.449600
5.840719	336.975992	7.454605
5.636066	345.174747	7.459610
5.620021	337.422484	7.464614
5.660309	330.254053	7.469619
5.362446	345.572781	7.474624
5.826180	335.192774	7.479629
5.706781	345.127530	7.484634
5.902803	349.089788	7.489638
6.149962	347.748039	7.494643
5.717519	350.930296	7.499648
5.947822	341.200233	7.504653
5.803638	340.517116	7.509658
5.751380	341.703277	7.514662
6.110793	358.478828	7.519667
5.556192	348.307144	7.524672
6.158832	351.830432	7.529677
5.898439	348.145022	7.534682
5.767084	352.029677	7.539686
5.969186	348.380074	7.544691
5.521414	353.504692	7.549696
5.621531	358.588369	7.554701
6.316751	368.110878	7.559706
6.278570	363.490454	7.564710
6.366108	355.944941	7.569715
5.768996	349.051956	7.574720
5.629896	341.626212	7.579725
5.745866	344.454662	7.584730
5.417385	348.072524	7.589734
5.985796	357.208408	7.594739
5.904693	355.527533	7.599744
6.250160	360.466435	7.604749
5.846001	353.122038	7.609754
5.675625	347.794434	7.614758
5.931531	337.520405	7.619763
5.349784	344.794962	7.624768
6.083008	355.626193	7.629773
6.243843	363.293564	7.634778
5.981417	353.725706	7.639782
5.868922	337.515476	7.644787
5.761467	348.397829	7.649792
5.856071	333.347458	7.654797
5.909776	337.215952	7.659802
5.587967	341.608432	7.664806
6.061518	350.761262	7.669811
5.634695	351.509631	7.674816
6.123650	358.128876	7.679821
6.223827	351.919203	7.684826
5.603329	352.933409	7.689830
5.500929	347.033481	7.694835
5.830041	360.108893	7.699840
5.886693	363.033046	7.704845
5.770732	380.081812	7.709850
5.824815	374.095677	7.714854
6.365052	374.070384	7.719859
6.130724	366.898641	7.724864
5.759085	354.609910	7.729869
5.684048	342.939478	7.734874
5.736121	353.442482	7.739878
5.990525	360.166820	7.744883
5.695247	381.011155	7.749888
6.129970	375.859831	7.754893
5.907734	364.929389	7.759898
6.143274	360.867910	7.764902
6.310932	344.913624	7.769907
5.797335	346.390772	7.774912
5.989629	337.597270	7.779917
5.917903	343.154102	7.784922
5.670172	353.890657	7.789926
6.156164	347.875960	7.794931
5.763275	345.058947	7.799936
5.871771	355.050947	7.804941
5.784877	351.261909	7.809946
5.546518	355.960798	7.814950
6.018370	340.482645	7.819955
5.465299	355.199500	7.824960
5.739054	339.644556	7.829965
5.752221	356.605726	7.834970
5.991225	369.699280	7.839974
6.259258	366.656968	7.844979
5.776049	363.539424	7.849984
5.609107	365.011446	7.854989
5.503573	362.101084	7.859994
5.599370	379.811249	7.864998
6.136180	367.533132	7.870003
5.904318	375.668740	7.875008
6.053461	376.245008	7.880013
5.962708	375.743044	7.885018
6.323625	377.757426	7.890022
5.799033	353.805304	7.895027
5.770478	362.285604	7.900032
5.786766	351.792882	7.905037
6.209183	359.044597	7.910042
6.119098	359.611294	7.915046
6.211671	345.078466	7.920051
5.844834	351.759832	7.925056
5.998444	348.127170	7.930061
6.192835	344.959954	7.935066
5.678543	357.092370	7.940070
6.235643	346.238426	7.945075
5.659469	344.909992	7.950080
6.021307	346.967828	7.955085
5.835533	336.164745	7.960090
5.566434	347.431537	7.965094
5.780949	347.218251	7.970099
5.913413	350.820280	7.975104
5.967146	339.284737	7.980109
6.168801	337.113059	7.985114
5.790169	344.861206	7.990118
6.013757	334.752823	7.995136
5.802817	344.476535	8.000154
5.834416	336.935135	8.005171
5.505563	347.812990	8.010189
5.710477	348.875457	8.015206
5.969873	332.996560	8.020224
5.835813	343.401525	8.025242
5.849574	339.102163	8.030259
6.006433	340.347601	8.035277
5.786428	339.542880	8.040294
5.902620	339.192665	8.045312
5.744389	345.355975	8.050330
5.786074	340.091429	8.055347
5.830860	344.016472	8.060365
6.023638	370.011575	8.065382
6.183115	364.417038	8.070400
5.852054	358.207641	8.075418
5.913788	351.457610	8.080435
6.147583	352.180465	8.085453
5.873448	356.132538	8.090470
6.042314	340.461182	8.095488
6.235637	354.937347	8.100506
6.033109	347.126223	8.105523
6.291928	333.878284	8.110541
5.957291	349.846398	8.115558
5.801568	342.472928	8.120576
5.915083	350.168685	8.125594
5.976795	343.133647	8.130611
6.032664	340.481859	8.135629
5.852845	340.245799	8.140646
5.686712	347.048160	8.145664
6.395609	363.632927	8.150682
5.804303	356.660757	8.155699
6.228195	361.151673	8.160717
5.995999	371.794995	8.165734
6.288445	367.297546	8.170752
6.328366	354.649702	8.175770
5.937527	358.080867	8.180787
5.941393	346.587934	8.185805
5.616505	356.245955	8.190822
5.893227	365.834498	8.195840
5.918716	378.084845	8.200858
6.088120	378.201137	8.205875
6.171422	377.400916	8.210893
5.929100	372.420158	8.215910
6.017419	372.320026	8.220928
6.385129	376.377214	8.225946
6.364006	378.642700	8.230963
6.599650	376.723950	8.235981
5.838864	374.331505	8.240998
5.927539	365.232120	8.246016
6.344215	378.581320	8.251034
6.297273	374.473912	8.256051
5.957900	374.631661	8.261069
5.900136	371.436207	8.266086
6.068420	374.844712	8.271104
6.330870	365.352501	8.276122
6.306349	372.127792	8.281139
6.462392	377.004343	8.286157
6.277926	377.741606	8.291174
6.419668	371.084361	8.296192
6.226942	349.858640	8.301210
6.118747	347.570507	8.306227
6.334225	351.145163	8.311245
5.932866	358.226959	8.316262
6.167229	364.632475	8.321280
6.301294	365.935243	8.326298
6.142732	376.589359	8.331315
6.423983	366.706261	8.336333
6.230833	371.981764	8.341350
6.242427	378.629807	8.346368
6.176633	371.798020	8.351386
6.279453	375.745509	8.356403
6.317094	368.308591	8.361421
6.432313	381.404383	8.366438
5.936716	372.442261	8.371456
6.310248	368.476168	8.376474
5.834429	375.041261	8.381491
6.268545	369.789424	8.386509
6.150250	372.748757	8.391526
6.574124	380.461834	8.396544
6.402965	377.797582	8.401562
6.413385	373.294847	8.406579
6.277902	366.539009	8.411597
6.035496	376.849810	8.416614
5.986861	375.625693	8.421632
6.092175	371.963999	8.426650
6.397898	370.973675	8.431667
6.147959	374.019842	8.436685
5.803588	371.217074	8.441702
6.279962	368.660924	8.446720
6.218387	363.736733	8.451738
6.027710	370.693170	8.456755
6.561971	368.544488	8.461773
6.039975	379.307236	8.466790
6.470336	390.440393	8.471808
6.395769	387.482747	8.476826
6.616862	392.128235	8.481843
6.735312	373.831403	8.486861
6.187551	380.533248	8.491878
6.642788	379.674554	8.496896
6.238852	367.674044	8.501914
6.380877	375.750670	8.506931
6.324121	367.038219	8.511949
6.245388	365.444140	8.516966
6.534113	368.818847	8.521984
6.613314	361.145125	8.527002
6.579903	377.558431	8.532019
6.643291	363.354455	8.537037
6.392487	372.499825	8.542054
6.367732	367.976956	8.547072
6.752654	365.591111	8.552090
6.805034	370.939968	8.557107
6.544279	369.941839	8.562125
6.347332	374.905405	8.567143
6.260104	374.370319	8.572160
6.514268	371.687141	8.577178
6.365214	373.841816	8.582195
6.502176	363.093412	8.587213
6.369246	375.455318	8.592231
6.064614	370.863819	8.597248
6.633436	380.199508	8.602266
6.670535	381.244796	8.607283
6.563676	378.529899	8.612301
6.362425	379.638423	8.617319
6.545044	386.707215	8.622336
6.922737	392.880671	8.627354
6.718766	377.678102	8.632371
6.563815	369.931887	8.637389
6.481536	370.997016	8.642407
6.586554	369.859161	8.647424
6.353026	363.045809	8.652442
6.468315	373.960284	8.657459
7.031938	370.105496	8.662477
6.871641	377.799930	8.667495
6.759490	375.600041	8.672512
6.579591	367.503675	8.677530
6.507417	369.060780	8.682547
7.050592	373.838933	8.687565
6.633347	377.212883	8.692583
6.425536	369.744130	8.697600
6.681356	372.534007	8.702618
6.206052	375.762896	8.707635
6.595550	377.297790	8.712653
6.583785	381.505052	8.717671
6.405297	376.219221	8.722688
6.879686	376.192899	8.727706
6.571701	382.586608	8.732723
6.467499	379.357536	8.737741
6.651828	376.173806	8.742759
6.651502	389.229169	8.747776
6.924879	393.191420	8.752794
6.742016	393.096798	8.757811
6.565446	382.669958	8.762829
6.638773	374.796632	8.767847
6.877171	397.917330	8.772864
6.831228	389.422342	8.777882
6.571934	383.017362	8.782899
6.805555	393.103789	8.787917
7.227283	393.695419	8.792935
6.830870	379.870385	8.797952
6.701542	373.526476	8.802970
6.542265	373.611776	8.807987
6.776296	367.273612	8.813005
6.654941	379.817241	8.818023
6.443186	378.324594	8.823040
6.653705	385.262184	8.828058
6.993899	395.895023	8.833075
7.038411	393.051037	8.838093
6.810882	393.270701	8.843111
6.679995	378.593141	8.848128
7.194683	378.806753	8.853146
6.835549	380.489699	8.858163
6.626086	372.171886	8.863181
6.768441	378.951724	8.868199
6.719606	376.115776	8.873216
7.177433	391.446946	8.878234
6.890366	385.779981	8.883251
6.655118	372.153737	8.888269
7.002396	372.373325	8.893287
6.808742	378.730708	8.898304
6.976309	374.925804	8.903322
6.441922	379.242371	8.908339
6.806688	394.944099	8.913357
7.064105	396.591886	8.918375
6.910317	401.288663	8.923392
7.191019	397.665719	8.928410
7.087336	386.306174	8.933427
7.066667	384.690237	8.938445
6.815616	374.577133	8.943463
6.566114	374.725850	8.948480
7.093531	378.957066	8.953498
7.029408	389.227416	8.958515
6.855271	384.211701	8.963533
6.907676	368.291982	8.968551
6.701322	384.474812	8.973568
6.969486	388.675703	8.978586
7.225073	396.447860	8.983603
6.971156	384.769615	8.988621
7.212555	384.508224	8.993639
6.930162	380.857431	8.998656
6.941014	371.229097	9.003674
6.522837	390.221499	9.008691
6.880753	396.828914	9.013709
6.742626	395.516333	9.018727
6.666170	402.604180	9.023744
7.233823	401.262864	9.028762
6.838716	404.615425	9.033779
7.043174	404.934140	9.038797
7.035489	402.641496	9.043815
7.080940	405.238805	9.048832
6.960705	401.400439	9.053850
7.167709	401.693535	9.058867
7.434823	399.502449	9.063885
7.230945	402.037073	9.068903
7.322968	406.381803	9.073920
7.174581	397.468836	9.078938
7.269410	400.435660	9.083955
7.437065	402.883928	9.088973
7.297917	393.061043	9.093991
6.792050	387.844581	9.099008
7.238366	390.766562	9.104026
6.995265	388.081592	9.109043
7.437647	399.839867	9.114061
7.477894	379.355236	9.119079
6.848925	383.789878	9.124096
7.143060	370.988359	9.129114
6.896415	373.672201	9.134131
7.241809	382.331902	9.139149
7.466266	389.064636	9.144167
7.011443	388.076717	9.149184
7.108016	382.494400	9.154202
6.936932	381.951797	9.159219
6.972770	395.124962	9.164237
7.317788	393.659642	9.169255
7.031779	405.704526	9.174272
7.332458	401.504492	9.179290
6.827168	408.342387	9.184307
6.982917	395.786074	9.189325
7.051936	403.060353	9.194343
6.973695	404.711770	9.199360
7.305724	406.167447	9.204378
7.546750	398.011534	9.209395
7.303805	409.134776	9.214413
7.474990	398.412743	9.219431
7.649458	406.979028	9.224448
7.694964	407.579652	9.229466
7.290301	406.891438	9.234483
7.180329	400.590754	9.239501
7.224748	400.761872	9.244519
7.078985	398.249484	9.249536
7.194714	397.642674	9.254554
7.111933	402.662070	9.259571
7.293966	400.085159	9.264589
7.054612	402.097971	9.269607
7.112244	396.775642	9.274624
7.127518	403.593738	9.279642
7.089676	412.513593	9.284659
7.040853	394.812994	9.289677
6.934321	401.179329	9.294695
6.697072	420.914462	9.299712
7.284547	428.167928	9.304730
7.367402	428.366513	9.309747
7.450272	434.767517	9.314765
7.540171	426.369605	9.319783
7.380324	440.246339	9.324800
7.656568	429.810537	9.329818
7.816733	437.222425	9.334835
7.719886	424.602767	9.339853
7.875306	424.997934	9.344871
7.555015	408.850381	9.349888
7.483640	403.769552	9.354906
7.715259	397.576252	9.359923
6.708588	400.270685	9.364941
7.233226	409.670620	9.369959
7.798450	417.279324	9.374976
7.616020	414.293148	9.379994
7.858409	404.232249	9.385011
7.446836	405.554261	9.390029
7.520439	389.441643	9.395047
7.198412	403.700978	9.400064
7.168795	393.135936	9.405082
7.196882	400.332969	9.410099
7.534823	422.042202	9.415117
7.686319	417.527028	9.420135
7.643081	423.768491	9.425152
7.899395	421.182577	9.430170
8.037685	402.357066	9.435187
7.211412	402.604208	9.440205
7.132260	393.823621	9.445223
7.476386	411.429613	9.450240
7.361837	410.148148	9.455258
7.885041	417.574483	9.460275
7.790674	429.929825	9.465293
7.846539	414.833822	9.470311
7.520515	405.618515	9.475328
7.520806	398.104334	9.480346
7.508209	387.291016	9.485363
7.269961	401.833838	9.490381
7.958096	412.531287	9.495399
7.697894	425.380488	9.500416
7.701569	411.781223	9.505434
7.685515	395.670116	9.510451
7.368333	403.705573	9.515469
8.200179	405.612184	9.520487
7.788880	403.644083	9.525504
7.322370	397.536310	9.530522
7.544501	406.355476	9.535539
7.725448	417.716116	9.540557
7.802855	417.549496	9.545575
7.808419	427.905525	9.550592
7.506693	403.583548	9.555610
7.845299	410.239844	9.560627
7.588539	415.796385	9.565645
7.489903	413.550744	9.570663
7.902512	427.640756	9.575680
8.170575	423.536483	9.580698
7.810871	408.202696	9.585715
7.886111	402.699107	9.590733
7.722802	391.332934	9.595751
7.805279	401.523025	9.600768
7.562299	386.521205	9.605786
7.978439	392.069034	9.610803
7.453979	394.748666	9.615821
7.995733	403.439319	9.620839
7.746764	402.460093	9.625856
7.423922	408.534854	9.630874
7.985535	417.465696	9.635891
7.620038	420.167726	9.640909
7.976920	423.076825	9.645927
8.008565	429.354462	9.650944
8.074003	434.073862	9.655962
8.006257	412.161198	9.660979
7.820066	403.220066	9.665997
7.732768	404.545458	9.671015
7.832316	402.279278	9.676032
7.699486	416.884114	9.681050
8.082999	410.090809	9.686067
7.971122	429.822043	9.691085
7.910837	410.652591	9.696103
7.786071	414.316292	9.701120
7.881793	424.549469	9.706138
8.079250	426.220412	9.711155
7.785563	425.472024	9.716173
7.747242	433.362138	9.721191
7.718965	419.170001	9.726208
7.751271	429.554457	9.731226
8.250951	415.956598	9.736243
7.885994	428.694484	9.741261
8.169364	416.880065	9.746279
7.982663	420.523749	9.751296
7.864999	426.036703	9.756314
7.941351	425.394709	9.761331
7.977558	434.656176	9.766349
8.101087	429.734659	9.771367
8.106107	429.422604	9.776384
8.134206	428.621715	9.781402
7.918263	426.607362	9.786419
7.966352	430.158092	9.791437
8.089511	421.168878	9.796455
7.907812	416.594134	9.801472
7.894319	419.429963	9.806490
8.206755	417.052419	9.811507
7.777068	428.419687	9.816525
8.039815	423.428579	9.821543
8.224781	425.668676	9.826560
7.724054	431.176803	9.831578
8.111169	432.335754	9.836595
8.127413	429.222860	9.841613
8.126853	438.802619	9.846631
8.023385	434.458941	9.851648
7.814475	431.367724	9.856666
8.032138	428.600453	9.861683
8.040539	430.987605	9.866701
8.102010	430.064250	9.871719
8.120804	432.666190	9.876736
8.213876	431.592320	9.881754
8.323469	421.608202	9.886771
8.077507	427.405056	9.891789
7.812491	422.805383	9.896807
8.170436	438.470892	9.901824
7.950141	451.350682	9.906842
8.475697	449.948058	9.911859
8.577761	445.625132	9.916877
8.238284	437.794799	9.921895
8.486943	434.516513	9.926912
8.378231	421.837024	9.931930
8.363042	420.377246	9.936947
8.335561	421.899766	9.941965
8.060471	420.750486	9.946983
8.049159	419.163697	9.952000
8.134607	424.373229	9.957018
8.036365	421.370697	9.962035
8.376228	437.934211	9.967053
8.470108	439.946951	9.972071
8.535908	437.253342	9.977088
8.249071	430.117746	9.982106
8.436488	418.585590	9.987123
8.375523	427.422888	9.992141
8.387282	417.060383	9.997159
8.657307	422.114837	10.002176
8.258083	428.986682	10.007194
8.210840	418.149182	10.012211
8.426796	426.590088	10.017229
8.394191	414.805160	10.022247
8.660340	418.070255	10.027264
8.380044	416.347875	10.032282
8.648226	415.414964	10.037299
8.348321	423.290289	10.042317
8.369054	410.982567	10.047335
8.499445	425.036224	10.052352
8.288158	425.864160	10.057370
8.260914	419.844377	10.062387
8.153447	430.020590	10.067405
8.276607	427.575300	10.072423
8.367731	424.184237	10.077440
8.631907	439.218340	10.082458
8.732862	424.284503	10.087475
8.779326	418.804391	10.092493
8.313831	424.562937	10.097511
8.716406	411.877404	10.102528
8.440173	420.918574	10.107546
8.692754	422.074887	10.112563
8.583513	418.177804	10.117581
8.530189	425.014003	10.122599
8.551392	417.262892	10.127616
8.486800	426.007493	10.132634
8.462751	424.565131	10.137651
8.451579	421.329445	10.142669
8.334264	423.599510	10.147687
8.529337	413.080171	10.152704
8.277808	433.378276	10.157722
8.593295	436.434798	10.162739
8.782687	443.141497	10.167757
8.606525	450.609687	10.172775
8.449906	431.819772	10.177792
8.354369	445.310657	10.182810
8.783796	446.532255	10.187827
8.572631	451.006518	10.192845
8.452154	456.311700	10.197863
8.661990	448.005249	10.202880
8.599448	449.334994	10.207898
8.673290	447.866517	10.212915
8.535183	461.844963	10.217933
8.644481	452.149433	10.222951
8.576885	449.642547	10.227968
8.766492	448.841582	10.232986
8.892346	450.295315	10.238003
8.884335	458.713037	10.243021
9.175586	455.393615	10.248039
9.180402	443.097961	10.253056
8.805236	438.099894	10.258074
8.848917	423.266319	10.263091
8.605430	425.313676	10.268109
8.603925	424.671631	10.273127
8.613270	434.725290	10.278144
8.856313	445.385137	10.283162
8.832498	447.418030	10.288179
8.743134	444.690963	10.293197
8.824703	451.149665	10.298215
9.647960	437.505091	10.303232
8.732981	437.259737	10.308250
8.673033	424.761690	10.313267
8.769304	425.226526	10.318285
8.402006	429.218706	10.323303
8.803529	433.451376	10.328320
8.810924	445.183569	10.333338
9.033872	444.787658	10.338355
8.858833	447.519842	10.343373
8.992405	453.403611	10.348391
9.036845	434.228730	10.353408
8.819499	440.404658	10.358426
8.681216	430.547554	10.363443
9.033870	442.259757	10.368461
8.910508	458.319824	10.373479
9.014244	449.548765	10.378496
8.782073	448.177998	10.383514
9.133733	455.649397	10.388531
9.177648	436.472436	10.393549
8.895020	443.548707	10.398567
9.158555	429.864900	10.403584
8.689818	422.337728	10.408602
8.722988	439.552562	10.413619
8.886383	453.884200	10.418637
8.983585	452.459671	10.423655
9.116765	458.297054	10.428672
9.159806	453.214906	10.433690
8.960436	460.088977	10.438707
9.160992	456.426589	10.443725
8.693026	456.670668	10.448743
9.314323	445.252581	10.453760
8.827166	456.854009	10.458778
8.816717	444.862046	10.463795
9.304332	449.867156	10.468813
9.121230	455.078818	10.473831
9.260607	449.613761	10.478848
8.858846	454.101201	10.483866
9.101881	451.524576	10.488883
9.364495	446.738583	10.493901
8.968525	453.147733	10.498919
9.321380	450.030457	10.503936
9.054919	450.808515	10.508954
8.815753	446.308072	10.513971
9.032746	450.624760	10.518989
8.926449	448.491795	10.524007
8.991844	444.177720	10.529024
9.030437	450.942359	10.534042
8.978645	452.584463	10.539059
9.156363	440.106149	10.544077
8.843423	448.894403	10.549095
9.120124	443.196502	10.554112
9.445214	450.701250	10.559130
9.222615	445.839423	10.564147
9.292100	446.822250	10.569165
9.117192	451.911104	10.574183
9.341192	448.964052	10.579200
8.961666	452.485672	10.584218
9.276544	457.264398	10.589235
9.463803	460.660715	10.594253
9.396216	462.131642	10.599271
9.155219	456.094425	10.604288
9.339287	461.609992	10.609306
9.687710	464.730527	10.614323
9.334270	455.864403	10.619341
9.248580	452.358639	10.624359
9.521451	444.324367	10.629376
9.068526	446.039836	10.634394
9.089852	445.124924	10.639411
9.375906	466.280490	10.644429
9.291472	483.699747	10.649447
9.753071	471.457665	10.654464
9.509924	470.911289	10.659482
9.262714	462.953805	10.664499
9.303868	458.016249	10.669517
9.422582	477.632846	10.674535
9.687176	464.738727	10.679552
9.636295	455.901442	10.684570
9.552249	448.149307	10.689587
9.308983	438.845821	10.694605
9.040761	452.827580	10.699623
9.640035	461.531341	10.704640
9.314554	480.699572	10.709658
9.602433	473.231051	10.714675
9.579231	475.453397	10.719693
9.669976	478.703174	10.724711
9.501842	461.874424	10.729728
9.632411	463.049248	10.734746
9.478348	464.489473	10.739763
9.720183	448.087831	10.744781
9.675524	445.148823	10.749799
9.523544	447.901975	10.754816
9.761659	448.949877	10.759834
9.778469	446.575800	10.764851
9.334991	441.799304	10.769869
9.420172	458.907689	10.774887
9.600904	450.164182	10.779904
9.517399	448.775200	10.784922
9.406078	456.170416	10.789939
9.388745	462.908729	10.794957
9.608078	465.116350	10.799975
9.773411	477.310859	10.804992
9.770724	470.317960	10.810010
9.775890	480.799868	10.815027
9.727000	476.766962	10.820045
9.912476	484.461060	10.825063
9.588490	461.137886	10.830080
9.662536	469.416001	10.835098
9.383516	472.462692	10.840115
9.885232	470.311926	10.845133
9.700059	479.938141	10.850151
10.011407	475.381422	10.855168
9.900038	466.246730	10.860186
9.531964	457.524561	10.865203
9.722889	457.121965	10.870221
9.560122	470.153416	10.875239
9.895592	470.551529	10.880256
10.087472	470.618224	10.885274
9.766145	475.988289	10.890291
9.909613	465.282824	10.895309
9.652151	456.097032	10.900327
10.104601	467.614337	10.905344
10.178548	452.738698	10.910362
9.654173	460.387790	10.915379
9.743253	454.507111	10.920397
9.541488	453.516493	10.925415
9.593838	467.052889	10.930432
10.169712	469.870486	10.935450
9.599886	482.693053	10.940467
10.283345	470.159196	10.945485
10.090129	468.505597	10.950503
9.826536	471.162353	10.955520
10.161791	467.577960	10.960538
9.626681	467.707619	10.965555
9.924765	469.680319	10.970573
9.672000	474.927778	10.975591
9.758455	476.695910	10.980608
9.639595	478.112964	10.985626
9.997608	478.675821	10.990643
10.052918	471.924837	10.995661
9.605750	477.526628	11.000679
9.871365	476.335107	11.005696
9.905448	471.736686	11.010714
9.985416	474.554234	11.015731
10.115919	473.115704	11.020749
10.093085	484.039830	11.025767
10.078702	482.317533	11.030784
10.029770	478.348014	11.035802
9.880844	468.492654	11.040819
10.071391	471.058181	11.045837
10.145270	469.533008	11.050855
10.259462	479.240360	11.055872
10.224403	469.257815	11.060890
10.101717	481.580901	11.065907
10.314318	471.004087	11.070925
10.100386	475.676043	11.075943
9.975315	475.969223	11.080960
10.437226	471.557151	11.085978
10.100503	478.065312	11.090995
10.312819	471.431920	11.096013
10.157184	472.698800	11.101031
10.002498	472.847308	11.106048
10.225389	468.389145	11.111066
10.101131	478.782926	11.116083
10.440256	471.090157	11.121101
10.127987	478.698690	11.126119
10.108401	480.389968	11.131136
10.403266	461.858806	11.136154
9.929422	480.901512	11.141171
10.132775	472.204032	11.146189
10.233728	472.598806	11.151207
10.016408	468.997210	11.156224
10.327156	477.481439	11.161242
10.197447	485.440505	11.166259
10.246227	499.277695	11.171277
10.511553	503.952674	11.176295
10.472045	493.367948	11.181312
10.608979	478.036971	11.186330
9.993830	479.075528	11.191347
10.257772	476.110612	11.196365
10.455645	489.126031	11.201383
10.627891	498.510780	11.206400
10.732264	477.761050	11.211418
10.381177	472.668622	11.216435
10.391183	469.910272	11.221453
10.228441	471.568851	11.226471
9.983446	478.612311	11.231488
10.582360	484.672270	11.236506
10.324954	494.236097	11.241523
10.674658	497.173567	11.246541
10.598645	492.893808	11.251559
10.072590	491.912603	11.256576
10.437963	491.541045	11.261594
10.609368	493.259827	11.266611
10.253064	494.636040	11.271629
10.433345	492.004883	11.276647
10.445777	495.946759	11.281664
10.502689	493.631555	11.286682
10.358696	505.193499	11.291699
10.528911	502.170148	11.296717
10.675586	498.099220	11.301735
10.202391	504.343287	11.306752
10.559453	497.888959	11.311770
10.601346	500.291419	11.316787
10.550242	505.361483	11.321805
10.701062	492.455743	11.326823
10.349135	500.130518	11.331840
10.739831	493.795985	11.336858
10.563134	499.517186	11.341875
10.486761	501.369270	11.346893
10.764683	496.379948	11.351911
10.525005	509.890516	11.356928
10.380828	496.350788	11.361946
10.510949	499.801489	11.366963
10.256223	504.187739	11.371981
10.638338	517.718972	11.376999
10.913762	520.186351	11.382016
11.249439	514.208958	11.387034
10.822648	504.575139	11.392051
10.965713	497.992416	11.397069
11.266081	479.586686	11.402087
11.197227	493.031842	11.407104
11.123916	488.487877	11.412122
11.063994	501.649689	11.417139
11.358107	493.200477	11.422157
11.383021	482.221422	11.427175
10.920871	468.055885	11.432192
10.925136	463.461241	11.437210
10.662126	457.570780	11.442227
10.544444	454.168750	11.447245
10.797819	450.934359	11.452263
10.500969	470.297211	11.457280
10.974210	474.900028	11.462298
11.038512	477.511143	11.467315
11.074733	489.145869	11.472333
10.898245	472.362784	11.477351
10.939186	477.007338	11.482368
10.928558	475.660567	11.487386
10.733474	474.922359	11.492403
11.034494	483.302509	11.497421
11.028525	483.676671	11.502439
11.148096	485.555433	11.507456
11.024281	475.163459	11.512474
11.085915	471.599939	11.517491
11.012782	466.307981	11.522509
10.758954	465.980095	11.527527
10.864147	475.914119	11.532544
10.798029	485.533934	11.537562
10.685387	487.426688	11.542579
10.686252	483.034555	11.547597
10.969495	481.635396	11.552615
10.673248	490.346298	11.557632
10.876137	476.128677	11.562650
10.923494	484.141771	11.567667
10.870051	487.805838	11.572685
10.885786	480.196931	11.577703
11.027303	509.003708	11.582720
11.269612	500.667030	11.587738
11.164869	515.173597	11.592755
11.182086	523.517678	11.597773
11.169375	515.908955	11.602791
11.093757	528.589974	11.607808
11.189648	516.221648	11.612826
11.349638	526.137738	11.617843
11.168333	521.920941	11.622861
11.655875	519.064510	11.627879
10.890373	499.842293	11.632896
10.838800	504.663637	11.637914
11.324015	509.642593	11.642931
11.098904	512.255758	11.647949
11.357981	515.706090	11.652967
11.464355	516.987687	11.657984
11.532332	513.710679	11.663002
11.637267	510.308247	11.668019
11.070106	503.123154	11.673037
11.346361	501.459429	11.678055
11.304899	512.351240	11.683072
11.464916	509.775609	11.688090
11.506678	512.057433	11.693107
11.417579	501.584283	11.698125
11.319344	495.694568	11.703143
11.138046	501.044123	11.708160
11.487519	505.930688	11.713178
11.834608	515.228123	11.718195
11.255758	500.372758	11.723213
11.554778	490.235074	11.728231
11.221934	491.819968	11.733248
11.227707	502.658847	11.738266
11.989283	504.905471	11.743283
11.328901	502.001080	11.748301
11.384171	488.127446	11.753319
11.273745	500.709118	11.758336
11.208564	505.397695	11.763354
11.303513	511.378056	11.768371
11.342868	518.903560	11.773389
11.550434	511.009035	11.778407
11.496405	518.754572	11.783424
11.333485	516.371186	11.788442
11.683903	517.590767	11.793459
11.082745	514.826518	11.798477
11.546345	518.713881	11.803495
11.609822	521.139133	11.808512
11.748114	523.385427	11.813530
11.631362	511.868918	11.818547
11.322003	521.451239	11.823565
11.451630	515.914360	11.828583
11.427980	520.888732	11.833600
11.501580	517.234440	11.838618
11.603720	512.638867	11.843635
11.640811	516.252856	11.848653
11.746600	513.951374	11.853671
11.493979	524.084654	11.858688
11.687040	536.251177	11.863706
11.881048	538.684458	11.868723
11.501156	546.903625	11.873741
12.004511	527.112828	11.878759
12.061466	540.697732	11.883776
11.961535	518.380850	11.888794
11.783170	510.664634	11.893811
11.644821	515.589570	11.898829
11.818858	511.406029	11.903847
11.756159	512.333475	11.908864
11.803404	515.567264	11.913882
11.883740	515.755049	11.918899
11.639144	517.240836	11.923917
12.088277	527.566313	11.928935
11.701538	532.270749	11.933952
11.718993	544.564490	11.938970
12.080178	535.539191	11.943987
12.013663	538.416725	11.949005
11.964064	519.175486	11.954023
12.484942	528.069467	11.959040
12.230053	508.594076	11.964058
12.341292	502.983689	11.969075
12.032150	510.478143	11.974093
12.245097	496.347014	11.979111
12.485974	504.869248	11.984128
12.287317	500.920672	11.989146
12.681123	501.055174	11.994163
12.442225	493.746043	11.999181
12.158609	481.880353	12.004199
12.217359	470.714398	12.009216
12.045453	474.283791	12.014234
12.113262	472.540157	12.019251
11.822957	475.917436	12.024269
11.903135	462.616015	12.029287
12.085347	473.023809	12.034304
11.837386	475.936018	12.039322
12.005745	467.267190	12.044339
12.372795	476.970502	12.049357
12.089099	468.738591	12.054375
11.882340	477.066532	12.059392
11.912127	482.327458	12.064410
12.305111	495.837379	12.069427
12.188477	497.073174	12.074445
12.398251	504.192227	12.079463
12.477944	493.860304	12.084480
12.179821	499.025947	12.089498
12.146898	470.640616	12.094515
12.109137	489.653564	12.099533
12.118155	487.434504	12.104551
11.822051	490.180321	12.109568
12.032127	500.192786	12.114586
12.357915	490.364407	12.119603
12.367027	499.176910	12.124621
12.539944	493.179534	12.129639
12.740993	494.523734	12.134656
12.543111	499.776054	12.139674
12.563525	496.891569	12.144691
12.330731	484.964481	12.149709
12.154666	476.796953	12.154727
12.289539	477.998620	12.159744
12.278044	497.600668	12.164762
12.715717	491.450044	12.169779
12.073265	492.981486	12.174797
12.424191	499.180692	12.179815
12.538855	493.169378	12.184832
12.107160	501.976810	12.189850
12.566060	488.406727	12.194867
11.967502	501.971230	12.199885
12.018537	497.228853	12.204903
12.264854	491.121058	12.209920
12.205400	502.615214	12.214938
12.393122	491.586259	12.219955
12.239926	503.840030	12.224973
12.344882	505.514744	12.229991
12.456090	517.989912	12.235008
12.110898	520.722242	12.240026
12.664726	525.667164	12.245043
12.662655	522.370499	12.250061
12.487328	528.088137	12.255079
12.828261	528.678045	12.260096
12.476363	528.640649	12.265114
12.868069	519.505373	12.270131
13.049976	534.049149	12.275149
12.684743	527.556803	12.280167
12.809073	529.569611	12.285184
12.738067	533.982218	12.290202
12.490290	528.634234	12.295219
12.362567	534.378999	12.300237
12.789411	529.151938	12.305255
12.824658	533.484488	12.310272
12.867193	535.235520	12.315290
12.701094	524.896796	12.320307
12.480846	534.185792	12.325325
12.723796	528.872180	12.330343
12.690273	523.105940	12.335360
12.842976	530.495493	12.340378
12.874506	524.018496	12.345395
12.827252	529.000534	12.350413
12.879885	521.356343	12.355431
13.169264	518.487183	12.360448
12.813091	527.002178	12.365466
12.811317	517.986629	12.370483
12.690532	519.285512	12.375501
12.890789	513.847516	12.380519
12.777409	509.033651	12.385536
12.498399	525.466481	12.390554
12.864187	519.045927	12.395571
12.703046	521.468555	12.400589
12.510053	524.742473	12.405607
13.020268	514.515934	12.410624
12.751860	526.217855	12.415642
12.953981	527.054834	12.420659
13.052010	537.947689	12.425677
13.190877	539.325455	12.430695
13.366733	525.522682	12.435712
12.967602	521.065143	12.440730
13.026836	512.519537	12.445747
13.146793	510.302308	12.450765
12.780846	516.544301	12.455783
13.216087	503.704457	12.460800
12.984547	517.333552	12.465818
13.128522	510.491048	12.470835
13.268913	518.977437	12.475853
13.431468	513.676405	12.480871
13.298035	512.747057	12.485888
13.147413	519.184346	12.490906
13.312948	526.289110	12.495923
13.066579	515.452751	12.500941
13.192422	521.557499	12.505959
13.345271	518.511048	12.510976
13.016151	525.463992	12.515994
13.336138	514.850207	12.521011
13.404281	507.812451	12.526029
12.940693	521.838357	12.531047
13.254662	514.277101	12.536064
13.216177	523.691773	12.541082
12.989452	525.074204	12.546099
13.238021	545.887712	12.551117
13.530563	551.156560	12.556135
13.790996	533.083756	12.561152
13.404605	530.392854	12.566170
13.453236	518.596116	12.571187
13.160156	526.176287	12.576205
12.922872	520.252592	12.581223
13.267201	538.844052	12.586240
13.545768	549.324261	12.591258
13.595472	554.579145	12.596275
13.586536	551.786923	12.601293
13.550348	555.645170	12.606311
13.728533	549.330583	12.611328
13.457531	529.843278	12.616346
13.504875	523.031001	12.621363
13.678483	515.029725	12.626381
13.567015	510.511385	12.631399
13.647288	513.029898	12.636416
13.533583	515.093685	12.641434
13.451479	517.007349	12.646451
13.361468	510.945998	12.651469
13.629918	522.389408	12.656487
13.416945	512.354916	12.661504
13.710893	529.701297	12.666522
13.700514	533.245824	12.671539
13.541439	529.663664	12.676557
13.599340	538.941075	12.681575
14.027261	534.001803	12.686592
13.400235	532.747243	12.691610
13.303375	531.476212	12.696627
13.725734	534.805519	12.701645
13.342480	548.910413	12.706663
14.249629	539.404436	12.711680
13.747049	545.620926	12.716698
13.691392	551.361986	12.721715
13.663141	542.078011	12.726733
13.559117	548.468987	12.731751
13.793978	551.421816	12.736768
13.649795	550.337572	12.741786
13.655567	544.096522	12.746803
14.028101	542.784281	12.751821
13.615029	553.699307	12.756839
14.062582	547.589339	12.761856
14.224375	550.626748	12.766874
13.760872	543.929289	12.771891
13.829650	549.816385	12.776909
13.584137	552.528413	12.781927
14.034188	547.102819	12.786944
13.774300	542.701848	12.791962
13.459348	551.494037	12.796979
14.016382	539.453148	12.801997
13.716887	546.853308	12.807015
13.843309	539.151571	12.812032
13.878259	545.850130	12.817050
13.827184	540.977479	12.822067
13.870500	543.460805	12.827085
13.760263	552.400844	12.832103
14.430397	558.961357	12.837120
14.309864	555.885344	12.842138
14.195016	548.027854	12.847155
13.795155	532.380759	12.852173
14.139128	538.105978	12.857191
14.428745	542.222447	12.862208
14.064392	544.129290	12.867226
14.003826	546.613152	12.872243
14.400275	538.278983	12.877261
13.950153	543.550802	12.882279
14.102223	542.164780	12.887296
13.966962	541.450481	12.892314
14.402955	553.017039	12.897331
14.528518	552.842020	12.902349
13.854139	545.430849	12.907367
14.506982	548.180161	12.912384
14.326979	540.228000	12.917402
14.300149	546.190036	12.922419
14.315327	537.192327	12.927437
14.316109	547.770079	12.932455
14.390553	543.637332	12.937472
14.063282	537.409320	12.942490
14.273397	550.240881	12.947507
14.393384	561.228324	12.952525
14.242133	581.070028	12.957543
14.692588	571.682653	12.962560
14.503878	557.767821	12.967578
14.144733	559.447047	12.972595
14.553616	554.781582	12.977613
14.352921	572.275180	12.982631
14.600847	572.674659	12.987648
14.825735	571.583594	12.992666
14.320781	554.576884	12.997683
14.490814	548.322506	13.002701
14.330840	554.560986	13.007719
14.280787	555.642817	13.012736
14.617854	559.539806	13.017754
14.411507	568.995397	13.022771
14.709983	555.859566	13.027789
14.699380	570.118665	13.032807
14.852861	562.604137	13.037824
14.720268	561.359120	13.042842
14.683824	546.767860	13.047859
14.717275	545.042132	13.052877
14.310108	536.313030	13.057895
14.774785	549.117830	13.062912
14.719066	559.580779	13.067930
14.530467	564.972511	13.072947
14.680775	565.458880	13.077965
14.908265	566.012531	13.082983
14.670777	561.512366	13.088000
14.510091	567.233490	13.093018
14.633378	567.794226	13.098035
14.865201	561.942533	13.103053
14.601431	568.211064	13.108071
14.904464	570.837236	13.113088
14.983273	561.526597	13.118106
15.064463	572.553762	13.123123
14.927423	557.772337	13.128141
14.889114	565.004301	13.133159
14.872874	557.475074	13.138176
15.145986	560.261521	13.143194
14.406139	550.513379	13.148211
14.870118	550.966705	13.153229
14.875177	554.267352	13.158247
14.844811	555.369333	13.163264
14.787344	562.575151	13.168282
14.649734	561.906711	13.173299
14.641602	566.357496	13.178317
14.816721	568.679166	13.183335
14.922573	569.478411	13.188352
14.943150	561.876336	13.193370
14.702940	569.162330	13.198387
14.790782	569.152624	13.203405
14.665338	575.432613	13.208423
15.177893	579.389016	13.213440
15.548982	581.706460	13.218458
14.935027	577.240321	13.223475
14.978840	563.168146	13.228493
15.122829	572.110426	13.233511
15.410511	574.531490	13.238528
15.301412	570.572144	13.243546
15.242782	567.088232	13.248563
15.248211	557.217592	13.253581
15.295838	561.310119	13.258599
15.145524	562.011598	13.263616
15.470764	558.130053	13.268634
15.253431	566.670217	13.273651
15.295362	565.027126	13.278669
15.096037	561.128052	13.283687
15.113290	557.286084	13.288704
15.300132	558.449791	13.293722
15.086488	559.005903	13.298739
15.329623	577.042028	13.303757
15.577318	588.170063	13.308775
15.046523	579.024117	13.313792
15.520138	578.287940	13.318810
15.599736	587.897182	13.323827
15.867223	579.093320	13.328845
15.037316	570.587207	13.333863
15.228583	563.289609	13.338880
15.763257	572.526179	13.343898
15.371472	579.917680	13.348915
15.877113	575.674872	13.353933
15.379560	571.395278	13.358951
15.295868	561.505396	13.363968
15.542448	570.810713	13.368986
15.376507	584.493525	13.374003
15.537929	583.145509	13.379021
15.683616	585.686427	13.384039
15.627938	589.222750	13.389056
15.837564	585.077955	13.394074
15.851696	574.950168	13.399091
15.566806	554.790781	13.404109
15.465357	564.302156	13.409127
15.709297	578.884283	13.414144
15.923070	584.420743	13.419162
15.512997	564.764790	13.424179
15.648689	562.654378	13.429197
15.841678	571.585956	13.434215
15.618471	575.296959	13.439232
16.007029	569.824299	13.444250
15.632990	575.068918	13.449267
15.917822	571.912929	13.454285
16.025868	564.758287	13.459303
15.666587	555.623411	13.464320
15.490642	560.199322	13.469338
15.585353	574.685195	13.474355
15.912403	580.195936	13.479373
16.312881	576.778223	13.484391
15.875426	569.874864	13.489408
16.055409	565.467896	13.494426
15.669913	572.587896	13.499443
15.857146	574.755794	13.504461
15.718991	576.189645	13.509479
15.625560	580.736495	13.514496
15.682433	572.577440	13.519514
15.694858	588.022795	13.524531
16.133434	585.465612	13.529549
15.802002	582.344337	13.534567
15.640552	588.104766	13.539584
15.849666	582.342660	13.544602
15.959735	587.925686	13.549619
15.904852	579.082696	13.554637
16.362575	586.786316	13.559655
16.166084	578.751252	13.564672
16.033163	578.320399	13.569690
15.471398	581.616058	13.574707
16.178049	590.644541	13.579725
16.487886	598.132804	13.584743
16.324303	595.150546	13.589760
16.347796	583.611067	13.594778
16.187065	583.331479	13.599795
16.481689	595.830355	13.604813
16.421060	578.453333	13.609831
16.123170	577.510177	13.614848
16.224438	575.995204	13.619866
16.183633	578.867095	13.624883
16.162827	582.564733	13.629901
16.625360	586.812699	13.634919
16.447780	585.402532	13.639936
16.582662	575.262155	13.644954
16.323115	580.395627	13.649971
16.215720	573.054365	13.654989
16.238650	579.608688	13.660007
16.033367	582.819311	13.665024
16.200207	592.260917	13.670042
16.449737	600.130633	13.675059
16.496445	602.903935	13.680077
16.755809	593.479021	13.685095
16.381679	603.329815	13.690112
16.798672	593.407280	13.695130
16.283552	606.960959	13.700147
16.401130	605.797183	13.705165
16.824499	596.431025	13.710183
16.437892	608.423893	13.715200
16.879456	606.610643	13.720218
16.835726	606.888533	13.725235
16.487070	598.255962	13.730253
16.721201	602.161017	13.735271
16.847600	600.403497	13.740288
16.903523	596.716104	13.745306
17.033302	596.063648	13.750323
16.577292	585.344951	13.755341
16.766945	575.547215	13.760359
16.234681	577.402647	13.765376
16.548261	588.316794	13.770394
16.651830	605.506727	13.775411
16.943011	603.587380	13.780429
16.991656	597.198838	13.785447
16.662118	607.967942	13.790464
17.060746	600.969498	13.795482
16.782176	594.857178	13.800499
16.988592	599.887621	13.805517
17.425035	603.599613	13.810535
16.833170	585.768990	13.815552
16.609449	574.452483	13.820570
16.688718	580.249862	13.825587
16.862027	588.830219	13.830605
17.073227	588.210291	13.835623
16.890484	600.369647	13.840640
16.700458	602.491993	13.845658
17.308225	603.952447	13.850675
16.990860	600.428074	13.855693
17.294504	595.271268	13.860711
16.973560	605.309468	13.865728
16.775627	602.811425	13.870746
16.809402	594.528845	13.875763
17.012788	607.663912	13.880781
16.880449	602.199871	13.885799
17.139873	600.028341	13.890816
17.112648	605.310595	13.895834
16.904976	605.117543	13.900851
17.068161	604.134165	13.905869
17.363981	606.840474	13.910887
17.228042	609.703184	13.915904
16.832309	599.286051	13.920922
17.159710	611.132493	13.925939
16.913352	606.497184	13.930957
17.243759	605.966489	13.935975
17.571230	623.773314	13.940992
17.577107	615.936665	13.946010
17.439449	609.751512	13.951027
17.236143	599.908649	13.956045
17.425683	595.868560	13.961063
17.049497	591.113901	13.966080
17.302154	595.363880	13.971098
17.412403	619.993305	13.976115
17.274617	623.739528	13.981133
17.829414	623.087487	13.986151
17.730549	622.138609	13.991168
17.617118	601.912673	13.996186
17.575491	593.099556	14.001203
17.485964	595.561272	14.006221
17.431914	581.784458	14.011239
17.539566	594.065019	14.016256
17.753340	586.831775	14.021274
17.384868	596.247208	14.026291
17.308087	599.990175	14.031309
17.405557	606.945278	14.036327
17.681145	616.362328	14.041344
17.701820	618.191210	14.046362
18.004765	615.213291	14.051379
17.727937	631.838966	14.056397
17.967140	618.163958	14.061415
17.833088	612.741141	14.066432
17.374416	612.438243	14.071450
17.669517	610.487143	14.076467
17.576549	620.877197	14.081485
17.763975	621.000141	14.086503
17.877899	629.205577	14.091520
18.065376	625.419152	14.096538
18.211346	616.998235	14.101555
17.857793	618.813732	14.106573
17.992299	603.656445	14.111591
17.933289	598.192422	14.116608
17.897516	608.444034	14.121626
18.280766	601.284772	14.126643
17.477127	595.424868	14.131661
17.870930	602.125220	14.136679
18.002174	618.409454	14.141696
17.922754	623.437023	14.146714
18.054219	619.112115	14.151731
17.935377	625.602429	14.156749
18.321310	628.425250	14.161767
17.866405	626.403938	14.166784
17.948734	621.021526	14.171802
18.142472	627.862417	14.176819
18.098097	635.025544	14.181837
18.351965	627.068740	14.186855
18.370188	627.982350	14.191872
18.156821	620.291383	14.196890
18.279370	611.597807	14.201907
18.040527	614.251655	14.206925
18.079484	617.434288	14.211943
18.165878	631.275580	14.216960
17.617766	628.720193	14.221978
18.105986	626.938553	14.226995
17.803462	620.559554	14.232013
17.870857	625.672360	14.237031
18.038595	622.261433	14.242048
17.876774	632.411185	14.247066
18.195874	638.000822	14.252083
17.924710	647.322166	14.257101
18.859350	645.844644	14.262119
18.707509	647.099491	14.267136
18.299365	647.179898	14.272154
18.551702	641.542073	14.277171
18.552877	650.089465	14.282189
18.378618	638.376332	14.287207
18.407720	645.477452	14.292224
18.305125	645.868269	14.297242
18.638409	641.780263	14.302259
18.408188	661.860180	14.307277
18.799693	643.311951	14.312295
18.543006	648.576063	14.317312
18.741249	640.451739	14.322330
18.775504	653.154359	14.327347
18.448888	657.575237	14.332365
18.552386	650.289234	14.337383
18.840644	642.427289	14.342400
18.772048	647.338115	14.347418
18.953179	644.706987	14.352435
19.046565	646.038389	14.357453
18.534673	646.869256	14.362471
18.861607	645.538800	14.367488
19.013377	636.630526	14.372506
19.080169	629.407913	14.377523
18.759827	625.599404	14.382541
18.701770	615.818209	14.387559
18.715824	624.325654	14.392576
18.834713	642.570486	14.397594
19.225988	628.201344	14.402611
19.054883	640.604449	14.407629
18.670355	633.955630	14.412647
19.241588	633.471514	14.417664
18.746532	631.299603	14.422682
19.259265	631.333047	14.427699
19.084477	638.461163	14.432717
19.186364	626.592897	14.437735
18.944234	619.058669	14.442752
18.978002	619.090034	14.447770
18.783106	609.591214	14.452787
19.024626	634.232896	14.457805
18.974803	627.299529	14.462823
19.151347	636.889145	14.467840
18.924894	648.224762	14.472858
19.022150	640.181588	14.477875
19.231215	645.992258	14.482893
18.815398	646.681771	14.487911
19.066570	642.490886	14.492928
18.868691	636.714521	14.497946
18.899622	634.657140	14.502963
18.909230	640.962737	14.507981
18.903097	644.938443	14.512999
19.203631	658.226882	14.518016
19.057781	668.760984	14.523034
19.514448	667.859129	14.528051
19.203270	667.245318	14.533069
19.798461	668.617128	14.538087
19.691864	657.191532	14.543104
19.794548	663.911756	14.548122
19.629438	643.763247	14.553139
19.371081	640.701070	14.558157
19.379265	634.317663	14.563175
19.671659	634.238922	14.568192
19.128774	638.924464	14.573210
19.418177	646.250608	14.578227
19.764878	658.553294	14.583245
19.929835	653.132730	14.588263
19.533702	645.068416	14.593280
19.392010	638.606777	14.598298
19.286380	639.924606	14.603315
19.705972	659.279434	14.608333
19.755168	665.625505	14.613351
19.987880	664.822680	14.618368
19.821989	668.525951	14.623386
19.775443	649.604294	14.628403
19.617376	654.064277	14.633421
19.752574	665.317948	14.638439
20.117142	655.659188	14.643456
19.479771	646.898604	14.648474
19.761935	656.574017	14.653491
19.449687	665.244372	14.658509
19.427364	659.107741	14.663527
19.736093	670.358556	14.668544
19.508396	680.385637	14.673562
19.637755	661.535312	14.678579
19.577715	660.025884	14.683597
19.915778	662.110264	14.688615
19.734062	665.525043	14.693632
20.032890	682.677688	14.698650
19.964566	681.747744	14.703667
20.075129	685.947355	14.708685
20.341690	691.169786	14.713703
20.354414	675.992121	14.718720
19.930677	669.361023	14.723738
20.172558	661.371354	14.728755
20.076152	668.028024	14.733773
19.813194	656.930167	14.738791
20.344259	667.025404	14.743808
20.191830	688.005944	14.748826
20.372934	681.109166	14.753843
20.469275	667.907434	14.758861
20.163755	673.883755	14.763879
20.289862	662.196266	14.768896
19.871047	663.114805	14.773914
20.422091	672.631962	14.778931
20.327653	679.019824	14.783949
20.376693	684.007166	14.788967
20.467212	686.331302	14.793984
20.196857	694.581944	14.799002
20.303150	681.466729	14.804019
20.076562	688.694809	14.809037
19.998214	691.458993	14.814055
20.516027	681.565311	14.819072
20.084650	692.895457	14.824090
20.551779	693.227406	14.829107
20.579196	688.353866	14.834125
20.407908	693.368776	14.839143
20.415702	685.660702	14.844160
20.208542	697.295882	14.849178
20.155016	691.343744	14.854195
20.338184	694.570135	14.859213
20.503616	715.888012	14.864231
20.705300	721.072421	14.869248
20.463145	711.338299	14.874266
21.035843	709.601463	14.879283
21.293364	707.768204	14.884301
20.926306	701.940412	14.889319
21.118043	681.008971	14.894336
21.023851	682.236326	14.899354
20.801306	679.665595	14.904371
21.068200	673.687960	14.909389
20.943949	682.305426	14.914407
21.132772	682.551161	14.919424
20.882863	678.658299	14.924442
20.905385	679.446599	14.929459
20.648009	684.153199	14.934477
20.698660	676.323841	14.939495
20.725142	678.454106	14.944512
20.570733	679.286183	14.949530
20.518786	677.487632	14.954547
21.274833	696.791901	14.959565
20.972436	699.630920	14.964583
21.198113	695.760772	14.969600
20.885524	708.934837	14.974618
20.958331	708.721541	14.979635
21.002037	707.583618	14.984653
20.963129	715.400554	14.989671
21.204215	707.499570	14.994688
21.505988	707.104527	14.999706
21.427297	706.235552	15.004723
21.248629	705.669002	15.009741
21.185761	713.712345	15.014759
21.766699	701.408715	15.019776
21.150249	692.069864	15.024794
21.140608	703.435032	15.029811
21.214153	701.466024	15.034829
21.410182	710.749516	15.039847
21.597439	711.612596	15.044864
21.327789	703.147530	15.049882
21.405037	710.892602	15.054899
21.316724	712.949832	15.059917
21.441649	712.311957	15.064935
21.542358	711.649369	15.069952
21.295242	715.657273	15.074970
21.462514	706.891648	15.079987
21.263153	702.716578	15.085005
21.333425	710.176214	15.090023
21.474687	708.093990	15.095040
21.331342	705.092205	15.100058
21.020662	710.903071	15.105075
21.504527	697.854015	15.110093
21.383999	708.012898	15.115111
21.903013	706.363917	15.120128
21.834618	706.815188	15.125146
21.547967	713.413740	15.130163
21.793605	698.776436	15.135181
21.358507	713.983722	15.140199
21.789165	719.294235	15.145216
22.185335	720.187352	15.150234
22.057725	713.298763	15.155251
21.906080	699.245958	15.160269
21.703893	701.907506	15.165287
22.119641	689.738814	15.170304
21.955503	701.479635	15.175322
21.784303	690.714314	15.180339
21.823178	698.972220	15.185357
21.700240	706.077576	15.190375
21.983276	707.412105	15.195392
22.196401	721.445196	15.200410
22.245499	707.827492	15.205427
22.033827	687.343774	15.210445
21.948568	688.284232	15.215463
21.957123	692.354943	15.220480
22.045925	698.718263	15.225498
22.574922	707.327555	15.230515
22.474035	691.876651	15.235533
22.452516	697.133187	15.240551
22.301998	686.320930	15.245568
22.462231	692.053914	15.250586
22.220522	689.143673	15.255603
22.313093	685.645429	15.260621
22.384549	690.833167	15.265639
21.754831	690.419926	15.270656
22.108748	689.242845	15.275674
21.903628	688.205921	15.280691
22.433994	694.421050	15.285709
22.666577	715.051630	15.290727
22.475506	707.891917	15.295744
22.346178	692.751034	15.300762
21.997757	702.105131	15.305779
22.313393	709.760781	15.310797
22.329192	721.852000	15.315815
22.493574	721.296734	15.320832
22.494680	719.731864	15.325850
22.318644	727.308623	15.330867
22.606079	718.149226	15.335885
22.309862	729.979733	15.340903
22.509473	709.571713	15.345920
22.379867	712.732188	15.350938
22.369018	720.500175	15.355955
22.911792	713.824747	15.360973
22.681626	716.731483	15.365991
22.750274	715.956515	15.371008
22.551763	712.088760	15.376026
22.504987	722.568245	15.381043
22.964394	740.995164	15.386061
22.965736	750.405913	15.391079
22.755633	747.978565	15.396096
23.057767	747.518702	15.401114
22.921309	754.993037	15.406131
23.333000	740.036381	15.411149
23.015728	717.835840	15.416167
23.004481	715.191600	15.421184
22.722236	709.843375	15.426202
22.675253	722.711710	15.431219
23.045568	727.662398	15.436237
23.032848	739.541653	15.441255
23.185574	750.422419	15.446272
23.426651	743.497142	15.451290
23.370368	735.016476	15.456307
23.040284	720.892923	15.461325
22.982823	716.273426	15.466343
23.425358	730.572706	15.471360
23.034225	720.188187	15.476378
23.034617	733.273248	15.481395
23.397639	734.108297	15.486413
23.404262	738.391533	15.491431
23.094679	745.408842	15.496448
23.619209	732.854737	15.501466
23.586828	736.049842	15.506483
23.274084	720.876429	15.511501
22.837494	721.417439	15.516519
22.925494	732.508936	15.521536
23.570114	727.812703	15.526554
23.349446	737.399508	15.531571
23.763341	733.951581	15.536589
23.267641	743.432537	15.541607
23.285639	739.261878	15.546624
23.813844	742.212246	15.551642
23.455702	747.931808	15.556659
23.421262	732.855818	15.561677
23.503463	738.365189	15.566695
23.237692	735.673098	15.571712
23.474898	744.031913	15.576730
23.547971	744.375820	15.581747
23.613211	741.581470	15.586765
23.453866	742.065968	15.591783
23.617456	750.057322	15.596800
23.879024	746.407559	15.601818
23.934741	771.771637	15.606835
24.307869	753.627093	15.611853
23.730864	749.323057	15.616871
23.760295	739.483151	15.621888
23.697039	731.349489	15.626906
23.545616	748.567005	15.631923
24.163026	762.271931	15.636941
24.245667	764.402716	15.641959
23.797756	764.052950	15.646976
23.771029	754.851068	15.651994
24.055821	770.133627	15.657011
24.184959	763.754079	15.662029
24.209796	765.344900	15.667047
24.467959	767.654373	15.672064
24.035577	758.621874	15.677082
24.202120	765.810828	15.682099
24.192289	756.072707	15.687117
24.343869	757.197609	15.692135
23.863417	758.101202	15.697152
24.021934	749.192923	15.702170
23.975289	761.548866	15.707187
24.163731	763.814025	15.712205
23.838252	753.087884	15.717223
24.219521	769.222461	15.722240
24.521115	755.695810	15.727258
24.295083	761.117453	15.732275
24.341156	758.627841	15.737293
24.464917	761.035631	15.742311
24.195192	759.701980	15.747328
24.511514	760.258591	15.752346
24.133011	760.905884	15.757363
24.238466	756.087655	15.762381
24.702796	766.423366	15.767399
24.723279	782.113230	15.772416
24.792114	760.143908	15.777434
24.563189	757.175628	15.782451
24.890997	751.824018	15.787469
24.853797	754.179825	15.792487
24.645952	762.535657	15.797504
25.010952	750.001951	15.802522
24.752316	752.140641	15.807539
24.829639	752.111425	15.812557
24.719956	749.348116	15.817575
24.658199	747.244121	15.822592
24.621937	741.314485	15.827610
24.674679	753.145668	15.832627
24.747705	760.266704	15.837645
24.988014	783.563638	15.842663
24.797961	780.924304	15.847680
24.963183	777.983810	15.852698
24.753556	779.620295	15.857715
24.880797	783.140038	15.862733
25.069437	781.914048	15.867751
25.101760	787.008525	15.872768
24.985482	786.415067	15.877786
25.068909	787.195022	15.882803
25.002916	778.259479	15.887821
25.138684	787.857344	15.892839
25.071427	784.030350	15.897856
25.400806	775.501113	15.902874
25.228328	776.884982	15.907891
25.822775	773.187366	15.912909
25.821372	775.104183	15.917927
25.295937	762.580283	15.922944
25.611839	744.300389	15.927962
25.235565	752.102751	15.932979
24.707109	739.849433	15.937997
25.514392	762.168693	15.943015
25.646853	777.736798	15.948032
25.729172	769.340354	15.953050
25.339257	763.168721	15.958067
25.297022	753.677310	15.963085
25.519352	769.413529	15.968103
25.101542	781.560723	15.973120
25.838874	787.425369	15.978138
25.809909	778.579728	15.983155
25.319825	783.533881	15.988173
25.578712	769.424196	15.993191
25.592752	780.989015	15.998208
25.956319	776.695954	16.003226
25.747824	778.210998	16.008243
25.723584	780.246565	16.013261
26.017806	772.305813	16.018279
25.840707	770.951647	16.023296
26.162444	780.708744	16.028314
26.071013	774.875268	16.033331
25.800404	762.264529	16.038349
25.799219	746.609609	16.043367
25.737249	761.750202	16.048384
25.715908	762.107439	16.053402
25.850607	772.368422	16.058419
25.931141	777.693451	16.063437
25.873578	783.123319	16.068455
25.929237	775.688722	16.073472
26.241140	770.652722	16.078490
25.926154	775.631703	16.083507
25.871011	780.747802	16.088525
25.912888	771.527028	16.093543
25.686873	779.473317	16.098560
25.625416	772.923880	16.103578
25.752979	781.225156	16.108595
25.881481	799.599277	16.113613
26.496991	786.660542	16.118631
26.454244	793.268979	16.123648
26.806653	801.734458	16.128666
26.611609	792.926648	16.133683
26.268023	804.678870	16.138701
26.589488	793.298751	16.143719
26.600642	795.187107	16.148736
26.371174	794.794734	16.153754
26.586877	793.114273	16.158771
26.385684	793.303778	16.163789
26.664262	796.934583	16.168807
26.416374	810.722352	16.173824
26.719291	803.018707	16.178842
26.956535	808.134247	16.183859
26.546319	792.008322	16.188877
26.505146	780.587311	16.193895
26.447732	776.532713	16.198912
26.531583	802.214191	16.203930
26.207760	803.979101	16.208947
26.242678	805.461564	16.213965
26.363744	804.450728	16.218983
26.164559	803.034880	16.224000
26.490777	803.130427	16.229018
26.563683	820.171770	16.234035
26.865564	835.271643	16.239053
27.046392	828.962212	16.244071
26.908803	823.778082	16.249088
27.058262	825.246234	16.254106
27.185620	833.860940	16.259123
27.183909	829.378985	16.264141
27.236600	830.594339	16.269159
27.175242	840.176185	16.274176
27.087924	834.176264	16.279194
27.067755	826.211759	16.284211
26.894263	839.665947	16.289229
27.252181	822.384036	16.294247
27.191567	823.335956	16.299264
27.051513	824.760500	16.304282
27.135767	826.204846	16.309299
27.042375	827.651948	16.314317
27.494183	825.202758	16.319335
27.154329	827.786033	16.324352
27.129925	823.523586	16.329370
27.162236	828.797990	16.334387
27.203507	822.729460	16.339405
27.430622	827.867554	16.344423
27.283431	833.719793	16.349440
27.189979	822.484201	16.354458
27.447640	822.688381	16.359475
27.578516	844.969406	16.364493
27.824626	843.199639	16.369511
27.654978	839.812459	16.374528
27.539940	833.505747	16.379546
27.464363	826.637000	16.384563
27.689394	843.553877	16.389581
27.800090	848.678259	16.394599
27.489087	846.340102	16.399616
27.630238	848.264729	16.404634
27.853360	849.395856	16.409651
27.577757	852.968792	16.414669
27.837195	850.321663	16.419687
27.977615	846.009376	16.424704
27.982287	841.754689	16.429722
28.333135	842.852383	16.434739
28.118805	841.231580	16.439757
28.306344	840.880520	16.444775
28.280045	845.556045	16.449792
27.928826	828.958098	16.454810
28.092727	829.938053	16.459827
28.353968	830.467209	16.464845
28.296116	823.562843	16.469863
27.854179	824.043921	16.474880
28.238574	829.708598	16.479898
28.397778	818.807371	16.484915
28.183904	822.881426	16.489933
28.213181	811.680165	16.494951
27.950104	824.690597	16.499968
28.044650	838.160467	16.504986
28.570505	844.214606	16.510003
28.328184	846.049827	16.515021
28.473913	848.542164	16.520039
27.940528	855.235324	16.525056
27.912619	843.513260	16.530074
28.385589	842.528180	16.535091
28.054664	854.569262	16.540109
27.891229	843.844864	16.545127
28.207043	855.557996	16.550144
28.393616	866.568250	16.555162
28.692981	866.486382	16.560179
28.391693	880.558269	16.565197
28.974894	865.179702	16.570215
28.720774	875.792369	16.575232
28.882282	870.023110	16.580250
28.927298	875.045432	16.585267
28.915161	881.889750	16.590285
29.103504	873.936231	16.595303
28.828618	854.070244	16.600320
28.448558	851.634121	16.605338
28.859563	861.683108	16.610355
28.813675	873.849262	16.615373
29.238259	872.105337	16.620391
29.083181	869.309396	16.625408
28.812829	877.376483	16.630426
29.259976	867.948537	16.635443
29.170535	874.102985	16.640461
29.085716	874.052296	16.645479
29.075661	867.684422	16.650496
28.866733	875.917273	16.655514
29.175501	865.263188	16.660531
28.976615	874.724220	16.665549
29.308396	870.069115	16.670567
29.242811	871.049814	16.675584
29.287535	876.353665	16.680602
29.409182	868.399030	16.685619
28.705996	865.276890	16.690637
29.046930	872.615639	16.695655
29.070264	870.099476	16.700672
29.000395	868.629847	16.705690
29.442573	879.342918	16.710707
29.575428	886.017085	16.715725
29.714785	890.341487	16.720743
29.687136	882.853759	16.725760
29.303952	893.131217	16.730778
29.663047	887.005113	16.735795
29.614805	894.595160	16.740813
29.839908	890.174697	16.745831
29.733232	891.948798	16.750848
29.581810	889.360501	16.755866
29.747362	894.387597	16.760883
29.900148	892.255798	16.765901
30.026303	891.041759	16.770919
29.975790	895.526059	16.775936
29.602476	898.511342	16.780954
29.956138	893.434506	16.785971
29.699601	892.380524	16.790989
29.973220	889.005482	16.796007
29.709154	888.982222	16.801024
29.971648	898.153211	16.806042
29.923774	894.968208	16.811059
29.968699	900.926328	16.816077
29.840828	889.634994	16.821095
29.776987	892.761742	16.826112
29.548699	888.019807	16.831130
30.066465	891.489627	16.836147
30.316600	912.681303	16.841165
30.356448	907.973532	16.846183
30.713366	919.995613	16.851200
30.486192	896.641908	16.856218
30.318153	888.418105	16.861235
30.237012	886.306289	16.866253
30.123605	882.315297	16.871271
30.354725	891.288359	16.876288
30.284688	911.944305	16.881306
30.419349	905.186635	16.886323
30.445545	910.306973	16.891341
30.577748	902.006097	16.896359
30.785558	914.049412	16.901376
30.929140	909.100790	16.906394
30.992090	898.445807	16.911411
30.757473	883.335031	16.916429
30.765252	880.120310	16.921447
30.560615	879.613183	16.926464
30.153887	880.700581	16.931482
30.853651	892.750298	16.936499
30.724477	906.102302	16.941517
30.969193	912.515776	16.946535
30.916983	911.110921	16.951552
30.802634	914.293703	16.956570
30.801805	910.071800	16.961587
30.861962	912.587818	16.966605
30.856049	911.439426	16.971623
31.184389	909.769364	16.976640
30.868390	916.589797	16.981658
30.977935	906.219175	16.986675
30.823386	909.484617	16.991693
30.732799	909.711643	16.996711
30.919773	904.792815	17.001728
30.666409	914.573933	17.006746
30.962148	914.724545	17.011763
31.407541	933.984688	17.016781
31.649880	937.295977	17.021799
31.575334	929.022757	17.026816
31.255529	914.947314	17.031834
31.397168	905.439421	17.036851
31.456303	909.346083	17.041869
31.399148	909.045533	17.046887
31.534869	915.211390	17.051904
31.869066	929.414696	17.056922
31.866305	912.633946	17.061939
31.398920	912.387406	17.066957
31.647794	897.654893	17.071975
31.215956	891.763782	17.076992
31.387967	905.684984	17.082010
31.768766	921.279278	17.087027
31.316501	925.741782	17.092045
31.603613	928.588566	17.097063
31.366225	921.666360	17.102080
31.495584	930.606360	17.107098
31.991391	926.805819	17.112115
32.047610	934.171842	17.117133
31.627448	925.911974	17.122151
31.709747	920.744412	17.127168
31.742791	938.957014	17.132186
31.925768	926.845525	17.137203
31.926016	937.754916	17.142221
32.322479	947.657565	17.147239
32.295460	944.643486	17.152256
32.029553	936.070194	17.157274
32.164832	946.098138	17.162291
32.104552	944.306846	17.167309
32.164573	946.232372	17.172327
32.481000	945.693361	17.177344
32.422057	960.555313	17.182362
32.260948	951.087869	17.187379
32.539469	945.399915	17.192397
32.456612	941.576656	17.197415
32.529924	933.580811	17.202432
32.234677	938.648684	17.207450
32.439684	936.423164	17.212467
32.651942	943.646728	17.217485
32.038641	952.627502	17.222503
32.496194	952.349666	17.227520
32.504870	949.532792	17.232538
32.307037	946.216411	17.237555
32.729505	950.087498	17.242573
32.167745	951.698279	17.247591
32.717545	955.336797	17.252608
32.481893	957.915766	17.257626
32.720955	945.760690	17.262643
32.901130	942.207083	17.267661
32.586862	956.457170	17.272679
32.918540	942.550180	17.277696
32.838712	948.823919	17.282714
32.668766	944.923013	17.287731
33.126950	947.522480	17.292749
33.133110	958.097062	17.297767
33.492277	949.478137	17.302784
33.202519	948.621789	17.307802
33.095592	945.824523	17.312819
33.186382	947.748478	17.317837
33.062895	953.758231	17.322855
32.835024	946.622237	17.327872
33.074619	960.480684	17.332890
33.227439	962.931705	17.337907
33.482880	966.193187	17.342925
33.055558	968.459150	17.347943
33.214533	965.734610	17.352960
33.181141	966.308410	17.357978
33.380719	961.614230	17.362995
33.529384	961.898731	17.368013
33.287451	964.733850	17.373031
33.559960	960.814122	17.378048
33.433564	972.188264	17.383066
33.528814	968.312562	17.388083
33.683179	961.557498	17.393101
33.072252	962.147371	17.398119
33.413464	962.851814	17.403136
33.555952	974.891468	17.408154
33.729487	990.179353	17.413171
34.294975	994.161713	17.418189
34.149470	985.157379	17.423207
34.395581	955.938990	17.428224
34.151907	952.310165	17.433242
34.015247	947.624632	17.438259
33.962361	956.820910	17.443277
34.109394	949.681656	17.448295
34.124993	945.314894	17.453312
34.346286	956.254879	17.458330
34.160454	946.565967	17.463347
34.314134	940.531067	17.468365
33.741347	951.977812	17.473383
33.882606	940.336214	17.478400
34.259391	944.938476	17.483418
33.991419	943.000610	17.488435
34.168498	942.861512	17.493453
33.983184	966.714477	17.498471
34.497636	971.712742	17.503488
34.706777	978.554577	17.508506
34.809900	973.606359	17.513523
34.617839	959.945841	17.518541
34.362315	944.096392	17.523559
34.345858	945.033894	17.528576
34.400145	961.554105	17.533594
34.423095	976.064683	17.538611
34.601787	965.978183	17.543629
34.502819	977.783181	17.548647
34.539810	975.010019	17.553664
34.908743	987.201013	17.558682
34.483774	978.391549	17.563699
34.736246	970.828089	17.568717
34.736458	974.129238	17.573735
34.682074	968.512354	17.578752
34.625276	971.662355	17.583770
34.402012	976.382073	17.588787
34.696042	969.392386	17.593805
34.658623	992.031500	17.598823
34.961162	998.492484	17.603840
35.243635	994.327797	17.608858
35.257329	1003.703185	17.613875
35.433487	996.181529	17.618893
35.105289	998.801869	17.623911
35.309082	996.664727	17.628928
35.301416	996.415789	17.633946
35.280791	999.038550	17.638963
35.358112	991.836852	17.643981
35.307275	998.886070	17.648999
35.288628	986.697420	17.654016
35.502158	994.872718	17.659034
35.285210	989.541100	17.664051
35.512423	988.959045	17.669069
35.377213	993.889318	17.674087
35.665651	995.534772	17.679104
35.624027	990.541319	17.684122
35.433877	1002.240631	17.689139
35.663343	995.212059	17.694157
35.776785	1006.241261	17.699175
36.030135	989.206847	17.704192
35.747561	998.213777	17.709210
35.754531	1003.409779	17.714227
35.712261	993.328098	17.719245
35.555084	990.191949	17.724263
35.526082	991.776782	17.729280
35.370104	994.328736	17.734298
35.512561	1011.685092	17.739315
36.046092	1017.957699	17.744333
36.051926	1026.150999	17.749351
36.126430	1020.503619	17.754368
36.309725	1017.175057	17.759386
35.922904	1022.724690	17.764403
36.493329	1016.524044	17.769421
36.234478	1021.356771	17.774439
36.273229	1018.631732	17.779456
36.339866	1020.911662	17.784474
36.110227	1025.867483	17.789491
36.275629	1016.601624	17.794509
36.156947	1027.622573	17.799527
36.290649	1020.567782	17.804544
36.313598	1020.391311	17.809562
36.529787	1022.304276	17.814579
36.651632	1017.090347	17.819597
36.340409	1022.087677	17.824615
36.461063	1018.038851	17.829632
36.683471	1020.428318	17.834650
36.687100	1035.475603	17.839667
36.847158	1043.568479	17.844685
37.030971	1038.658403	17.849703
36.889660	1035.589289	17.854720
37.008017	1021.929877	17.859738
36.609365	1015.387957	17.864755
37.091586	1013.673412	17.869773
36.746825	1032.444564	17.874791
37.174902	1026.715190	17.879808
36.859877	1027.731846	17.884826
36.677109	1033.353862	17.889843
37.237412	1033.073908	17.894861
37.401995	1036.069024	17.899879
37.156194	1039.167779	17.904896
37.092326	1030.995086	17.909914
37.225958	1042.408342	17.914931
37.383369	1034.076828	17.919949
37.375106	1031.219844	17.924967
37.274644	1039.697734	17.929984
37.699785	1031.713832	17.935002
37.565008	1032.792259	17.940019
37.421767	1025.620904	17.945037
37.321783	1034.971506	17.950055
37.245174	1039.718440	17.955072
37.636505	1018.620698	17.960090
37.319036	1026.850804	17.965107
37.387111	1030.626096	17.970125
37.553852	1029.231688	17.975143
37.503301	1028.982004	17.980160
37.770153	1029.332291	17.985178
37.480602	1036.612925	17.990195
37.389691	1026.787720	17.995213
37.765817	1030.963366	18.000231
37.636314	1039.697253	18.005248
37.726526	1056.070262	18.010266
38.055289	1060.645109	18.015283
38.314968	1053.663062	18.020301
38.285763	1048.052594	18.025319
38.737621	1054.191947	18.030336
38.489164	1030.180977	18.035354
38.247655	1022.463777	18.040371
38.387101	1014.850187	18.045389
38.379075	1012.752579	18.050407
37.950164	1018.843038	18.055424
38.231521	1007.595802	18.060442
38.276164	1017.496344	18.065459
38.167520	1009.952334	18.070477
38.472214	1022.417801	18.075495
38.239706	1025.329313	18.080512
38.449743	1027.627141	18.085530
38.147261	1042.685153	18.090547
38.563242	1040.758791	18.095565
38.783323	1044.762354	18.100583
38.429967	1040.629320	18.105600
38.669515	1047.227166	18.110618
38.329403	1058.151480	18.115635
38.424087	1042.364978	18.120653
38.756873	1044.038498	18.125671
38.391459	1041.091665	18.130688
38.795910	1045.619678	18.135706
38.630233	1060.787642	18.140723
38.751538	1071.560870	18.145741
39.154805	1068.624064	18.150759
39.503504	1065.029035	18.155776
39.636083	1062.552948	18.160794
39.500259	1052.284424	18.165811
39.142070	1035.833467	18.170829
39.475036	1024.305213	18.175847
39.259167	1035.052569	18.180864
39.581015	1032.705653	18.185882
39.323277	1038.079908	18.190899
39.527106	1023.603569	18.195917
39.190889	1033.413492	18.200935
38.805142	1028.542966	18.205952
39.514524	1028.787028	18.210970
39.237597	1032.901931	18.215987
39.297598	1050.507851	18.221005
39.459148	1052.990112	18.226023
39.442866	1056.855018	18.231040
39.760365	1050.401921	18.236058
39.455186	1057.567057	18.241075
40.067654	1052.503452	18.246093
40.027452	1051.259573	18.251111
39.661862	1057.516287	18.256128
40.027661	1046.692763	18.261146
40.031463	1053.814812	18.266163
40.033489	1048.141281	18.271181
40.223079	1052.684928	18.276199
40.060327	1051.283866	18.281216
40.167537	1051.004418	18.286234
39.856690	1042.809385	18.291251
40.142113	1051.108585	18.296269
40.102601	1051.055482	18.301287
39.645583	1055.343229	18.306304
40.044921	1051.816555	18.311322
40.120185	1050.288536	18.316339
39.927292	1050.650278	18.321357
40.134587	1051.039204	18.326375
39.874091	1058.516190	18.331392
40.263677	1058.590580	18.336410
40.269839	1073.631969	18.341427
40.314391	1084.948649	18.346445
40.176936	1083.696522	18.351463
40.487729	1083.733223	18.356480
41.128046	1089.803868	18.361498
40.832314	1088.241054	18.366515
40.701195	1074.672663	18.371533
40.595904	1078.809443	18.376551
40.657420	1078.793877	18.381568
40.673079	1071.942533	18.386586
40.786258	1080.980581	18.391603
40.814140	1072.053280	18.396621
40.655020	1075.685249	18.401639
40.733047	1076.677130	18.406656
41.101297	1071.561988	18.411674
40.947749	1086.549622	18.416691
41.201070	1091.123632	18.421709
41.665397	1097.223531	18.426727
41.534728	1085.367188	18.431744
41.356457	1079.378744	18.436762
41.489311	1075.691246	18.441779
41.406726	1066.977574	18.446797
41.641819	1063.408513	18.451815
41.166708	1069.558243	18.456832
41.748169	1067.896488	18.461850
41.606823	1081.638051	18.466867
41.615992	1075.360593	18.471885
41.566820	1065.993365	18.476903
41.571046	1074.868031	18.481920
41.401708	1060.293450	18.486938
41.424600	1073.776223	18.491955
41.555593	1074.343178	18.496973
41.900656	1065.567093	18.501991
41.778264	1068.791005	18.507008
41.760197	1076.158420	18.512026
41.829102	1088.098192	18.517043
41.644751	1094.993668	18.522061
41.960838	1092.600065	18.527079
42.305243	1093.124465	18.532096
42.405244	1098.182207	18.537114
42.283316	1102.618203	18.542131
42.143245	1095.587227	18.547149
42.489281	1093.639808	18.552167
41.697178	1090.089501	18.557184
42.044995	1088.477206	18.562202
42.340277	1093.339899	18.567219
41.995780	1096.368852	18.572237
42.337539	1093.396990	18.577255
42.156496	1097.514477	18.582272
42.103143	1089.853370	18.587290
42.457101	1095.061808	18.592307
42.448825	1098.291562	18.597325
42.273966	1089.366452	18.602343
42.090595	1110.423373	18.607360
42.410931	1117.240097	18.612378
42.702790	1121.223877	18.617395
42.909060	1122.690490	18.622413
43.165418	1115.005847	18.627431
43.182368	1123.759926	18.632448
43.015535	1112.093030	18.637466
42.966459	1105.135112	18.642483
43.037808	1112.414063	18.647501
43.111054	1106.600333	18.652519
42.978694	1102.255362	18.657536
43.073244	1113.656663	18.662554
43.054789	1110.913950	18.667571
42.919756	1112.215644	18.672589
43.631963	1110.280590	18.677607
43.311782	1111.907137	18.682624
43.149651	1116.267145	18.687642
43.040200	1115.848122	18.692659
43.178308	1112.342805	18.697677
43.286899	1114.605147	18.702695
43.036445	1114.043030	18.707712
42.876458	1112.440724	18.712730
43.568071	1116.002565	18.717747
43.324914	1129.931164	18.722765
43.621306	1136.627471	18.727783
43.471074	1136.210107	18.732800
43.548961	1139.330672	18.737818
43.879274	1135.026900	18.742835
43.853248	1140.402834	18.747853
44.032389	1132.206234	18.752871
43.804866	1143.199687	18.757888
43.857255	1135.938682	18.762906
43.886101	1132.736548	18.767923
43.790346	1140.144857	18.772941
43.961588	1126.352552	18.777959
43.902007	1138.503868	18.782976
44.029274	1124.444475	18.787994
44.166066	1140.497641	18.793011
44.061286	1161.099460	18.798029
44.689828	1152.460850	18.803047
44.381401	1170.442301	18.808064
44.327100	1169.484997	18.813082
44.480457	1169.380154	18.818099
44.200940	1175.811185	18.823117
44.604811	1156.172141	18.828135
44.718029	1170.584044	18.833152
44.819683	1168.030801	18.838170
44.676864	1156.060285	18.843187
44.649900	1164.135099	18.848205
44.847709	1164.694495	18.853223
44.449281	1172.633027	18.858240
44.729293	1173.496467	18.863258
44.754982	1162.625063	18.868275
44.452500	1170.959836	18.873293
44.892888	1170.075032	18.878311
45.057102	1169.807367	18.883328
44.757840	1168.952584	18.888346
44.815583	1161.083220	18.893363
44.704130	1186.049008	18.898381
45.311760	1180.199582	18.903399
45.107690	1186.311790	18.908416
45.253534	1189.289973	18.913434
45.594919	1180.190036	18.918451
45.442607	1185.794842	18.923469
45.636535	1185.689555	18.928487
45.698836	1191.191766	18.933504
45.589539	1178.562536	18.938522
45.804448	1164.072021	18.943539
45.538016	1162.808254	18.948557
45.581545	1152.846849	18.953575
45.576901	1149.295173	18.958592
45.537397	1172.697861	18.963610
45.754801	1180.930880	18.968627
45.643419	1176.408786	18.973645
45.240094	1179.311316	18.978663
45.487114	1179.233818	18.983680
45.559157	1180.352681	18.988698
45.613141	1177.701851	18.993715
45.541667	1180.888584	18.998733
45.678022	1199.203217	19.003751
46.340625	1203.308859	19.008768
46.117977	1206.912048	19.013786
46.407752	1199.215117	19.018803
46.515058	1201.829248	19.023821
46.589221	1202.612339	19.028839
46.456566	1201.103508	19.033856
46.549166	1196.941586	19.038874
46.402883	1199.477789	19.043891
46.622092	1194.919248	19.048909
46.434892	1201.812882	19.053927
46.850351	1195.437929	19.058944
46.779764	1200.314222	19.063962
46.860282	1192.107211	19.068979
46.992022	1193.466144	19.073997
46.636560	1190.741635	19.079015
46.679214	1181.307109	19.084032
46.535765	1195.036918	19.089050
46.801393	1193.430004	19.094067
46.667885	1200.399750	19.099085
46.814561	1196.689848	19.104103
47.214147	1195.527977	19.109120
46.897436	1200.827445	19.114138
47.004494	1182.583714	19.119155
46.835324	1195.209177	19.124173
46.868837	1198.985924	19.129191
47.226489	1206.117339	19.134208
47.194005	1223.672295	19.139226
47.357667	1221.369358	19.144243
46.932826	1225.572279	19.149261
47.365040	1222.712914	19.154279
47.471334	1213.450463	19.159296
47.448896	1220.894261	19.164314
47.674560	1216.934620	19.169331
47.527068	1218.267132	19.174349
47.746146	1221.892181	19.179367
47.653481	1219.186192	19.184384
47.620544	1215.713217	19.189402
47.661240	1213.077974	19.194419
47.733455	1226.073960	19.199437
47.662213	1248.866310	19.204455
47.916282	1242.264233	19.209472
47.868197	1249.129255	19.214490
48.255365	1249.701277	19.219507
48.095370	1256.725843	19.224525
48.320410	1251.158081	19.229543
48.293270	1244.490539	19.234560
48.459831	1239.074229	19.239578
48.770640	1232.882003	19.244595
48.687307	1249.246661	19.249613
48.156748	1248.690149	19.254631
48.381771	1239.157170	19.259648
48.135070	1236.891332	19.264666
48.596436	1234.890478	19.269683
48.354188	1246.952163	19.274701
48.292564	1243.037901	19.279719
48.499506	1234.875602	19.284736
48.373363	1239.623743	19.289754
48.394632	1241.197885	19.294771
48.648547	1246.805274	19.299789
48.810293	1251.878001	19.304807
49.277107	1253.761939	19.309824
48.682418	1253.772760	19.314842
49.349940	1261.779050	19.319859
49.262812	1256.590323	19.324877
49.096581	1258.372789	19.329895
49.268487	1250.926124	19.334912
49.139259	1257.634956	19.339930
49.116520	1255.953920	19.344947
49.357094	1257.028244	19.349965
49.157582	1256.546628	19.354983
49.723597	1250.067894	19.360000
49.263600	1259.948923	19.365018
49.394685	1249.689054	19.370035
49.121783	1255.345422	19.375053
49.069989	1250.587031	19.380071
49.393329	1255.426610	19.385088
49.038416	1262.081224	19.390106
49.520310	1262.991429	19.395123
49.558704	1278.533156	19.400141
49.606890	1273.491221	19.405159
49.662665	1271.320771	19.410176
49.702816	1281.807251	19.415194
49.972157	1278.574565	19.420211
50.100823	1275.333371	19.425229
50.031649	1281.260209	19.430247
50.106893	1277.213352	19.435264
50.231419	1281.363169	19.440282
50.034807	1278.561851	19.445299
50.109401	1296.255781	19.450317
50.256346	1299.009793	19.455335
50.662882	1287.807689	19.460352
50.597840	1297.532946	19.465370
50.930049	1298.359372	19.470387
51.190250	1288.061878	19.475405
51.037420	1277.678317	19.480423
50.944079	1260.666581	19.485440
50.899538	1255.455030	19.490458
50.920280	1252.558538	19.495475
50.832393	1269.115307	19.500493
50.808529	1261.953527	19.505511
51.131513	1249.136649	19.510528
50.852774	1258.683626	19.515546
51.279184	1251.379301	19.520563
51.307731	1258.370957	19.525581
51.230079	1257.823421	19.530599
51.151067	1248.000427	19.535616
50.785523	1261.657367	19.540634
50.837803	1248.975635	19.545651
51.096514	1254.825529	19.550669
51.367976	1276.962952	19.555687
51.427128	1285.484132	19.560704
51.200949	1297.460511	19.565722
51.113478	1285.605889	19.570739
51.138531	1287.193185	19.575757
51.277853	1299.422590	19.580775
50.939068	1291.215532	19.585792
50.803418	1306.533859	19.590810
51.602331	1312.664455	19.595827
51.777002	1322.107374	19.600845
51.580825	1323.913327	19.605863
52.110745	1320.564491	19.610880
52.160931	1320.796471	19.615898
51.933181	1318.227873	19.620915
52.051026	1314.459744	19.625933
52.191580	1325.781905	19.630951
52.629033	1312.289669	19.635968
52.327952	1319.918403	19.640986
52.383283	1305.170035	19.646003
52.565108	1304.574254	19.651021
52.367926	1307.581518	19.656039
52.873952	1308.664876	19.661056
52.617038	1304.458655	19.666074
52.453936	1315.865132	19.671091
52.688560	1310.792987	19.676109
52.557802	1306.085104	19.681127
53.097098	1301.147359	19.686144
53.109136	1309.363006	19.691162
52.844093	1303.423147	19.696179
52.474232	1300.782110	19.701197
52.355747	1312.126447	19.706215
52.806639	1303.978290	19.711232
52.546229	1306.027587	19.716250
52.979762	1302.308959	19.721267
52.805297	1302.190491	19.726285
52.860189	1311.577723	19.731303
52.618110	1306.610002	19.736320
52.576153	1328.138584	19.741338
52.731048	1342.002004	19.746355
53.010650	1331.851252	19.751373
52.948836	1341.951974	19.756391
53.326326	1349.062837	19.761408
53.623343	1355.957163	19.766426
53.669134	1361.570051	19.771443
53.390356	1353.606129	19.776461
53.686091	1356.535417	19.781479
53.703503	1352.457208	19.786496
53.932513	1349.508763	19.791514
53.986121	1356.689994	19.796531
53.995278	1347.077868	19.801549
53.729821	1343.199032	19.806567
54.023297	1350.988015	19.811584
53.797560	1352.871717	19.816602
53.659481	1352.068479	19.821619
53.956281	1351.628386	19.826637
54.350194	1374.573135	19.831655
54.798466	1366.253338	19.836672
54.585118	1361.976870	19.841690
54.240743	1339.396676	19.846707
54.881746	1342.268973	19.851725
54.282110	1336.335498	19.856743
54.664493	1331.885622	19.861760
54.795112	1336.228531	19.866778
54.493567	1338.168924	19.871795
54.501837	1340.756232	19.876813
54.196271	1360.764539	19.881831
54.842492	1365.152470	19.886848
54.772431	1375.134508	19.891866
54.660098	1371.247144	19.896883
54.912698	1363.852760	19.901901
54.574894	1373.148999	19.906919
54.942838	1366.944863	19.911936
54.879887	1379.088660	19.916954
55.042371	1390.237542	19.921971
55.647384	1393.996518	19.926989
55.515760	1396.344493	19.932007
55.694267	1388.167942	19.937024
55.584718	1376.228733	19.942042
55.480999	1365.357041	19.947059
55.607621	1355.159653	19.952077
55.584900	1360.315436	19.957095
55.486800	1360.889376	19.962112
55.489285	1362.981205	19.967130
55.665329	1367.797664	19.972147
55.880293	1374.318244	19.977165
55.542987	1386.049781	19.982183
55.707536	1387.684374	19.987200
55.465524	1385.961816	19.992218
55.556308	1388.869663	19.997235
56.364123	1381.703459	20.002253
55.561070	1389.378254	20.007271
55.530494	1388.713049	20.012288
55.584351	1395.837958	20.017306
56.054610	1402.908233	20.022323
56.427615	1410.915519	20.027341
56.178640	1413.194027	20.032359
56.623126	1412.693561	20.037376
56.460380	1405.671330	20.042394
56.507289	1404.482234	20.047411
56.482415	1403.320817	20.052429
56.698694	1409.446713	20.057447
56.970008	1401.485041	20.062464
57.043225	1394.286593	20.067482
56.828647	1409.115002	20.072499
56.916999	1394.951597	20.077517
56.612942	1403.885167	20.082535
56.873499	1409.506866	20.087552
56.919098	1408.706168	20.092570
57.260731	1418.424540	20.097587
57.594306	1412.251688	20.102605
57.267057	1410.657070	20.107623
57.503776	1394.916286	20.112640
57.637041	1390.144812	20.117658
57.227069	1392.857151	20.122675
57.381700	1396.267368	20.127693
57.425994	1418.681326	20.132711
57.555322	1421.950482	20.137728
57.510918	1420.041931	20.142746
57.282670	1417.259230	20.147763
57.904789	1417.786700	20.152781
57.847479	1428.885527	20.157799
57.901831	1417.058413	20.162816
57.687014	1421.389467	20.167834
57.869465	1424.484838	20.172851
58.001321	1417.695522	20.177869
58.044579	1425.712740	20.182887
58.352742	1415.891432	20.187904
58.193965	1418.021093	20.192922
57.626568	1425.815004	20.197939
58.254775	1423.983638	20.202957
58.266913	1442.906595	20.207975
58.216135	1443.150238	20.212992
58.294928	1450.337563	20.218010
58.048445	1448.836996	20.223027
58.250730	1441.839512	20.228045
58.412116	1454.338990	20.233063
58.441384	1463.114048	20.238080
59.117576	1461.235728	20.243098
59.018984	1477.878355	20.248115
59.118242	1466.992541	20.253133
59.309560	1471.984050	20.258151
59.143439	1444.044255	20.263168
59.233990	1436.291737	20.268186
58.874285	1440.116573	20.273203
59.467856	1453.569004	20.278221
59.198607	1441.052754	20.283239
59.182582	1454.265561	20.288256
59.636657	1456.650060	20.293274
59.142374	1459.999245	20.298291
59.401118	1457.836374	20.303309
59.418849	1474.192740	20.308327
59.282731	1462.268903	20.313344
59.639812	1452.739042	20.318362
59.762855	1459.945001	20.323379
59.797754	1452.365501	20.328397
59.952260	1464.592514	20.333415
59.875506	1456.770156	20.338432
60.084034	1458.199813	20.343450
59.731659	1456.825110	20.348467
59.862592	1456.067706	20.353485
59.989279	1462.862833	20.358503
60.120206	1463.711305	20.363520
59.981814	1456.669255	20.368538
59.864357	1462.136086	20.373555
60.145957	1472.128244	20.378573
60.359883	1487.895336	20.383591
60.465871	1480.385502	20.388608
60.552587	1484.989682	20.393626
60.240995	1489.842342	20.398643
60.284732	1481.006263	20.403661
60.414016	1486.262019	20.408679
60.636936	1496.863935	20.413696
60.589774	1508.234356	20.418714
60.547672	1513.374513	20.423731
61.085876	1505.339691	20.428749
61.010886	1506.659390	20.433767
61.198488	1518.241584	20.438784
61.489827	1505.018345	20.443802
61.326417	1510.012128	20.448819
60.943476	1507.362205	20.453837
61.398597	1500.825029	20.458855
61.571982	1500.098363	20.463872
61.521758	1501.258042	20.468890
61.608566	1498.218637	20.473907
61.709861	1500.536185	20.478925
61.523207	1495.560373	20.483943
61.561024	1510.863457	20.488960
61.647036	1497.215301	20.493978
61.528654	1503.124812	20.498995
61.940177	1503.567210	20.504013
61.770961	1520.870429	20.509031
61.645441	1534.082998	20.514048
62.181865	1533.699925	20.519066
61.933869	1535.600340	20.524083
61.852682	1532.417592	20.529101
62.342647	1529.933216	20.534119
62.163526	1536.696523	20.539136
62.403560	1530.472636	20.544154
62.104865	1534.621602	20.549171
62.337993	1533.113756	20.554189
62.367770	1551.179201	20.559207
62.938718	1551.343533	20.564224
63.234621	1553.084658	20.569242
62.884232	1546.933695	20.574259
62.744734	1522.401886	20.579277
62.864897	1536.529123	20.584295
62.806652	1544.092805	20.589312
63.396296	1549.944111	20.594330
63.072060	1557.818932	20.599347
63.207750	1554.008804	20.604365
63.105997	1549.092485	20.609383
63.122122	1551.276953	20.614400
63.612419	1548.455516	20.619418
63.625432	1561.262807	20.624435
63.457627	1554.232293	20.629453
63.840608	1549.703911	20.634471
63.676933	1539.768032	20.639488
63.569388	1520.633597	20.644506
63.493894	1532.934322	20.649523
63.885930	1534.007903	20.654541
63.713115	1546.063399	20.659559
63.322517	1555.327182	20.664576
63.609726	1548.205696	20.669594
63.271593	1558.293821	20.674611
63.492925	1550.231720	20.679629
63.611731	1547.414544	20.684647
63.967948	1564.117500	20.689664
64.258951	1562.427201	20.694682
64.019730	1570.667816	20.699699
64.121154	1570.875142	20.704717
64.045925	1559.301342	20.709735
64.185041	1572.977044	20.714752
64.967908	1579.560806	20.719770
65.049465	1584.481618	20.724787
64.876923	1564.824472	20.729805
64.926872	1556.160150	20.734823
64.684709	1557.998181	20.739840
64.759157	1546.544789	20.744858
64.794574	1562.771146	20.749875
64.806578	1575.831369	20.754893
65.270279	1572.596242	20.759911
64.612806	1572.004115	20.764928
64.704530	1576.369698	20.769946
64.886103	1576.653860	20.774963
64.856259	1587.970675	20.779981
65.130091	1596.811068	20.784999
65.077336	1612.183636	20.790016
65.419683	1605.036031	20.795034
65.479224	1616.169508	20.800051
65.313403	1609.322891	20.805069
65.621446	1605.929377	20.810087
65.428437	1616.324520	20.815104
66.134718	1626.381630	20.820122
66.167918	1629.361691	20.825139
66.321435	1631.599320	20.830157
66.431336	1619.123849	20.835175
66.045130	1603.040323	20.840192
66.554240	1593.125272	20.845210
66.469387	1599.804042	20.850227
66.314963	1596.445659	20.855245
66.514628	1584.970640	20.860263
66.192808	1600.512716	20.865280
66.747509	1612.538297	20.870298
66.736472	1628.731893	20.875315
66.492293	1630.268695	20.880333
66.557205	1626.397872	20.885351
66.650055	1638.958889	20.890368
66.667087	1627.154352	20.895386
66.511040	1624.976931	20.900403
67.024131	1625.638278	20.905421
67.108235	1627.020915	20.910439
66.636542	1639.384027	20.915456
66.874869	1629.048999	20.920474
66.803555	1655.774606	20.925491
66.954016	1654.977727	20.930509
67.282505	1657.017385	20.935527
67.374502	1657.777851	20.940544
67.392664	1644.422336	20.945562
67.697922	1647.649309	20.950579
67.295262	1646.431762	20.955597
67.677927	1648.144700	20.960615
67.841967	1657.752583	20.965632
67.947951	1649.297399	20.970650
67.852245	1660.603952	20.975667
68.012699	1668.461661	20.980685
68.076544	1666.048084	20.985703
68.176409	1673.411538	20.990720
68.282450	1671.576771	20.995738
68.111322	1669.731375	21.000755
68.376684	1666.024472	21.005773
68.414386	1670.008117	21.010791
68.216000	1674.972333	21.015808
68.384176	1668.734350	21.020826
68.550031	1678.628557	21.025843
68.696118	1675.041080	21.030861
68.603422	1663.582703	21.035879
68.537254	1674.683965	21.040896
68.726108	1665.540594	21.045914
69.107887	1647.041998	21.050931
68.953443	1661.595300	21.055949
69.158091	1650.398537	21.060967
69.291747	1659.578403	21.065984
69.376118	1651.934285	21.071002
69.417523	1655.737391	21.076019
69.180337	1655.296274	21.081037
69.531058	1648.887411	21.086055
69.588440	1653.233526	21.091072
69.576527	1647.600281	21.096090
69.230622	1645.494174	21.101107
69.477927	1671.383790	21.106125
69.895069	1674.039421	21.111143
69.750543	1686.658432	21.116160
69.814843	1680.364086	21.121178
69.874919	1673.920839	21.126195
69.771526	1685.375144	21.131213
70.304885	1676.101283	21.136231
69.620482	1686.423023	21.141248
69.862973	1677.770334	21.146266
70.013435	1691.348192	21.151283
69.857845	1711.628480	21.156301
70.111530	1705.975482	21.161319
70.117853	1720.935584	21.166336
70.117873	1707.123583	21.171354
70.484081	1719.728605	21.176371
70.657674	1741.374693	21.181389
70.933637	1719.374309	21.186407
70.906077	1730.263290	21.191424
70.889656	1728.585877	21.196442
70.854411	1730.360011	21.201459
71.298735	1737.506799	21.206477
71.299487	1726.257255	21.211495
71.385164	1731.805774	21.216512
71.330404	1729.774497	21.221530
71.320814	1731.639643	21.226547
71.206787	1724.393422	21.231565
71.580955	1715.199932	21.236583
71.114084	1725.348930	21.241600
71.489763	1731.430354	21.246618
71.739351	1744.124856	21.251635
71.896514	1755.537485	21.256653
72.063733	1747.561835	21.261671
71.996048	1762.237426	21.266688
71.966255	1750.161444	21.271706
72.339202	1753.040576	21.276723
72.034187	1747.256794	21.281741
72.550575	1751.889251	21.286759
72.195792	1751.410589	21.291776
72.364073	1751.725311	21.296794
72.475824	1749.547460	21.301811
72.396409	1752.454134	21.306829
72.492578	1744.821001	21.311847
72.253677	1737.071118	21.316864
72.184400	1746.175707	21.321882
72.306469	1749.281966	21.326899
72.652917	1775.065909	21.331917
72.949716	1766.213200	21.336935
72.800125	1776.442178	21.341952
72.636256	1771.575875	21.346970
72.743075	1772.079159	21.351987
72.838458	1779.530416	21.357005
73.234444	1771.777757	21.362023
73.077226	1782.704465	21.367040
73.329714	1797.396170	21.372058
73.462632	1791.570298	21.377075
73.176135	1800.522830	21.382093
73.560669	1790.479932	21.387111
73.604949	1801.905057	21.392128
73.859197	1791.894441	21.397146
74.135518	1792.514044	21.402163
74.157008	1791.522451	21.407181
74.332725	1776.261893	21.412199
74.512495	1782.488889	21.417216
74.483252	1786.025027	21.422234
74.936112	1781.210556	21.427251
74.406492	1786.775527	21.432269
74.430669	1785.702779	21.437287
74.647174	1783.537435	21.442304
74.336175	1784.259764	21.447322
75.132855	1775.254288	21.452339
74.557146	1786.135588	21.457357
75.110370	1784.311923	21.462375
75.103797	1783.042710	21.467392
74.793084	1792.272490	21.472410
74.809238	1782.119167	21.477427
74.515564	1785.813426	21.482445
74.620492	1778.484727	21.487463
74.957488	1789.213949	21.492480
74.865206	1810.177941	21.497498
75.164841	1815.077938	21.502515
75.102300	1824.195627	21.507533
75.015931	1814.002234	21.512551
75.403213	1815.932536	21.517568
75.220562	1827.702482	21.522586
75.448044	1839.886955	21.527603
75.722439	1841.032867	21.532621
75.921653	1837.761328	21.537639
75.750749	1847.063575	21.542656
75.516784	1841.728976	21.547674
75.823860	1831.843414	21.552691
76.186098	1848.725995	21.557709
76.704985	1859.810867	21.562727
76.915451	1849.872451	21.567744
76.575445	1845.992884	21.572762
76.963876	1823.350036	21.577779
76.649127	1825.276933	21.582797
76.561871	1821.536075	21.587815
76.662023	1813.302638	21.592832
76.849099	1829.380841	21.597850
77.126821	1827.406500	21.602867
77.158173	1830.634939	21.607885
76.744578	1821.679788	21.612903
76.810206	1849.945183	21.617920
76.827950	1852.392419	21.622938
77.170969	1846.498538	21.627955
77.045935	1860.714066	21.632973
77.169052	1853.615381	21.637991
77.326581	1844.518843	21.643008
77.095725	1851.555847	21.648026
77.240371	1873.955755	21.653043
76.889071	1879.521438	21.658061
77.461566	1879.491424	21.663079
77.879542	1882.350894	21.668096
77.842955	1878.490971	21.673114
78.316457	1879.621513	21.678131
78.250952	1874.862059	21.683149
77.950028	1869.091723	21.688167
78.370215	1873.234297	21.693184
78.007321	1874.646363	21.698202
78.324320	1875.442675	21.703219
78.319387	1893.725707	21.708237
78.644283	1891.980528	21.713255
79.031127	1896.501881	21.718272
78.840087	1891.275879	21.723290
79.222980	1884.058023	21.728307
79.112469	1881.537168	21.733325
79.002215	1885.812783	21.738343
79.106878	1883.680186	21.743360
78.917799	1891.452003	21.748378
79.168262	1882.397085	21.753395
79.019275	1883.239345	21.758413
78.949034	1888.370523	21.763431
79.260928	1879.019174	21.768448
78.635713	1890.472951	21.773466
78.931303	1896.241765	21.778483
79.156746	1913.120379	21.783501
79.272080	1914.461631	21.788519
79.679150	1920.757208	21.793536
79.486876	1942.152173	21.798554
79.650235	1936.521584	21.803571
80.175994	1944.237620	21.808589
80.301612	1932.714021	21.813607
80.213501	1935.695797	21.818624
79.996230	1935.878140	21.823642
80.348227	1932.040240	21.828659
80.439104	1938.180496	21.833677
80.468645	1930.899294	21.838695
80.801668	1933.774073	21.843712
80.703090	1942.714353	21.848730
81.176267	1952.175767	21.853747
80.749521	1943.487300	21.858765
81.394103	1947.635910	21.863783
81.246330	1933.540390	21.868800
80.895662	1937.019350	21.873818
81.288808	1934.395491	21.878835
81.408192	1949.883094	21.883853
81.439898	1950.180754	21.888871
81.583860	1953.183809	21.893888
81.562056	1955.189596	21.898906
81.665335	1958.509259	21.903923
81.548215	1962.965173	21.908941
81.212690	1957.391895	21.913959
81.875101	1952.734675	21.918976
81.545693	1959.610151	21.923994
81.610162	1954.822379	21.929011
81.919084	1966.588688	21.934029
81.978606	1973.448746	21.939047
82.281109	1972.745877	21.944064
81.994468	1982.212717	21.949082
82.328332	1964.333922	21.954099
82.386922	1962.865279	21.959117
82.749969	1961.135800	21.964135
82.729971	1962.321593	21.969152
82.747442	1963.586592	21.974170
82.714286	1962.671394	21.979187
82.605138	1971.655574	21.984205
82.349321	1973.064419	21.989223
83.010196	1984.634453	21.994240
82.974283	1997.637639	21.999258
83.336364	1983.639234	22.004275
83.891634	1989.298389	22.009293
83.564900	1985.250436	22.014311
83.844526	1967.471991	22.019328
83.649543	1986.416647	22.024346
84.142733	1978.981989	22.029363
84.158690	1963.697403	22.034381
83.985466	1951.269899	22.039399
84.161814	1945.289900	22.044416
83.794163	1946.543310	22.049434
84.026844	1941.924046	22.054451
83.789850	1948.506989	22.059469
83.907258	1967.950107	22.064487
83.972145	1968.119811	22.069504
83.725073	1977.195420	22.074522
83.891677	1983.264054	22.079539
84.032480	1981.633713	22.084557
84.103108	2009.674155	22.089575
84.272895	2006.926378	22.094592
84.135364	2007.332088	22.099610
84.470983	2027.364616	22.104627
84.924922	2031.654383	22.109645
84.862420	2044.380133	22.114663
85.391168	2033.379238	22.119680
85.173228	2045.583173	22.124698
85.290866	2041.523560	22.129715
85.289466	2038.963285	22.134733
85.259649	2041.610978	22.139751
85.231292	2037.256332	22.144768
85.471580	2059.122494	22.149786
85.470024	2061.110363	22.154803
85.662879	2056.951236	22.159821
85.885226	2065.438244	22.164839
85.900865	2056.224609	22.169856
85.903070	2064.013148	22.174874
85.842108	2060.190696	22.179891
86.256474	2070.467485	22.184909
85.904068	2080.077205	22.189927
86.289947	2091.515066	22.194944
86.285430	2084.574892	22.199962
86.380586	2093.660231	22.204979
86.076222	2084.456453	22.209997
86.286704	2104.373260	22.215015
86.983877	2099.298007	22.220032
87.140532	2106.230172	22.225050
87.009258	2109.290023	22.230067
87.081250	2103.806057	22.235085
86.924235	2103.545306	22.240103
86.991209	2108.378943	22.245120
87.195277	2112.624431	22.250138
87.140992	2105.394087	22.255155
87.311813	2117.373230	22.260173
87.331283	2129.825185	22.265191
88.135501	2137.278107	22.270208
87.968143	2126.495985	22.275226
87.761643	2127.111589	22.280243
87.883601	2131.361672	22.285261
87.665927	2129.265288	22.290279
88.206398	2125.906267	22.295296
88.137865	2137.867723	22.300314
87.918123	2131.236532	22.305331
88.593869	2138.834037	22.310349
88.138381	2152.585052	22.315367
88.349468	2158.814476	22.320384
88.394625	2160.294188	22.325402
88.459626	2153.266050	22.330419
88.625967	2152.552731	22.335437
88.523897	2155.119536	22.340455
88.837019	2175.074496	22.345472
88.979663	2181.521215	22.350490
88.779167	2188.687973	22.355507
88.965759	2194.343120	22.360525
89.135752	2186.818371	22.365543
89.135399	2179.158940	22.370560
89.423185	2182.726342	22.375578
89.534281	2201.199908	22.380595
90.172584	2203.253510	22.385613
90.197466	2214.852639	22.390631
90.015114	2200.275602	22.395648
90.342461	2209.222418	22.400666
90.254428	2197.227028	22.405683
90.420986	2183.571970	22.410701
90.109214	2177.276141	22.415719
90.230889	2184.032654	22.420736
90.330782	2196.963436	22.425754
90.190068	2202.345018	22.430771
90.616525	2191.922446	22.435789
90.489727	2198.256072	22.440807
90.738553	2195.219922	22.445824
90.468300	2195.007911	22.450842
90.789086	2218.209383	22.455859
90.997884	2214.975939	22.460877
91.018818	2232.875139	22.465895
91.037476	2227.551966	22.470912
91.350463	2231.590009	22.475930
91.199613	2238.112694	22.480947
91.245580	2227.027718	22.485965
91.019946	2237.304283	22.490983
91.856369	2233.198397	22.496000
91.590315	2243.868309	22.501018
91.781853	2232.611495	22.506035
91.891277	2232.380875	22.511053
91.869030	2239.368029	22.516071
91.822706	2237.638047	22.521088
91.840353	2258.282790	22.526106
92.041842	2261.173586	22.531123
92.558652	2256.476694	22.536141
92.490714	2279.669629	22.541159
92.406232	2267.562174	22.546176
92.601998	2271.939405	22.551194
92.623834	2276.813667	22.556211
92.642748	2280.047811	22.561229
92.693176	2295.740532	22.566247
92.811114	2289.317731	22.571264
93.117486	2302.424530	22.576282
93.197362	2293.304020	22.581299
93.527316	2293.519050	22.586317
93.237616	2287.950241	22.591335
93.778281	2297.419945	22.596352
93.728206	2321.177316	22.601370
93.754436	2325.622895	22.606387
94.020052	2320.791346	22.611405
94.227425	2318.125461	22.616423
93.749642	2318.362912	22.621440
94.408628	2318.648463	22.626458
94.026326	2313.639936	22.631475
94.555719	2313.841507	22.636493
94.251807	2316.866306	22.641511
94.606904	2313.007720	22.646528
94.662370	2305.896450	22.651546
94.274590	2306.631954	22.656563
94.961688	2313.674885	22.661581
94.715712	2312.603294	22.666599
94.551114	2316.634899	22.671616
95.173065	2315.544271	22.676634
94.592849	2341.139051	22.681651
94.802758	2335.589562	22.686669
94.717747	2333.225031	22.691687
94.826677	2343.647254	22.696704
95.522399	2354.557422	22.701722
95.118288	2366.937041	22.706739
95.754244	2364.913730	22.711757
95.312751	2374.362051	22.716775
95.594912	2368.899760	22.721792
95.830980	2374.824714	22.726810
96.008698	2384.673699	22.731827
96.142012	2386.578564	22.736845
96.347193	2391.869262	22.741863
96.600068	2383.510533	22.746880
96.456893	2391.654118	22.751898
96.521892	2398.367779	22.756915
96.940878	2385.074154	22.761933
96.693344	2386.997821	22.766951
96.878842	2382.184686	22.771968
96.954293	2388.235554	22.776986
96.750199	2390.618557	22.782003
97.027884	2386.833056	22.787021
96.934177	2395.884602	22.792039
96.872764	2411.905095	22.797056
97.422717	2416.264058	22.802074
97.539696	2413.056857	22.807091
97.355423	2417.349643	22.812109
97.123872	2421.565243	22.817127
97.391338	2429.750453	22.822144
97.755476	2440.789806	22.827162
97.617737	2448.042321	22.832179
97.769751	2445.731693	22.837197
98.225778	2451.863440	22.842215
98.353068	2458.108487	22.847232
98.747690	2458.738776	22.852250
98.835075	2472.101807	22.857267
98.800681	2461.556815	22.862285
98.900669	2453.908921	22.867303
98.765811	2454.238996	22.872320
99.221269	2450.056991	22.877338
98.877538	2455.266484	22.882355
99.157761	2456.583532	22.887373
99.095102	2465.706340	22.892391
99.121781	2455.738237	22.897408
99.242601	2465.397902	22.902426
99.136041	2460.224599	22.907443
99.455608	2458.467647	22.912461
99.251666	2476.268665	22.917479
99.302201	2479.664532	22.922496
99.644239	2491.456054	22.927514
99.569305	2484.041161	22.932531
99.830353	2501.794856	22.937549
100.035077	2507.625854	22.942567
99.886156	2523.512178	22.947584
100.296280	2520.624366	22.952602
99.879953	2525.943590	22.957619
100.209082	2538.447565	22.962637
100.672262	2538.064052	22.967655
100.527335	2540.870730	22.972672
100.628836	2542.591521	22.977690
100.852451	2537.527897	22.982707
101.012389	2540.944575	22.987725
101.311527	2548.425336	22.992743
101.251817	2564.099621	22.997760
101.867278	2567.928030	23.002778
101.911524	2571.432054	23.007795
101.876824	2556.238775	23.012813
101.710381	2542.932852	23.017831
101.521873	2542.294630	23.022848
101.725768	2555.773811	23.027866
101.662449	2560.464272	23.032883
101.744642	2566.844816	23.037901
102.131188	2568.542257	23.042919
101.794133	2572.891973	23.047936
102.178689	2570.737967	23.052954
102.237698	2597.073042	23.057971
102.410127	2584.759644	23.062989
102.995982	2569.088007	23.068007
103.216170	2574.812124	23.073024
103.719537	2561.463774	23.078042
103.688778	2573.200377	23.083059
103.480274	2561.172362	23.088077
103.217940	2547.332736	23.093095
102.959870	2546.200143	23.098112
103.383664	2552.956611	23.103130
103.403562	2558.693928	23.108147
103.329377	2564.674452	23.113165
103.760932	2562.228764	23.118183
103.788650	2567.777373	23.123200
103.670395	2569.937465	23.128218
103.319117	2570.277129	23.133235
103.666443	2588.283135	23.138253
103.968400	2599.964072	23.143271
103.691005	2606.228002	23.148288
104.103596	2600.734506	23.153306
103.982298	2624.433699	23.158323
104.283659	2631.109755	23.163341
104.251136	2631.144859	23.168359
104.042627	2653.940034	23.173376
104.698243	2655.399057	23.178394
105.372211	2640.076901	23.183411
105.319886	2641.525219	23.188429
105.502497	2642.217917	23.193447
105.505907	2644.028647	23.198464
105.702361	2629.658348	23.203482
105.478462	2649.575204	23.208499
105.653647	2644.111697	23.213517
106.023732	2647.765537	23.218535
106.026160	2666.396700	23.223552
106.241032	2662.933008	23.228570
106.200567	2667.972480	23.233587
106.452283	2671.612137	23.238605
106.438565	2661.202559	23.243623
106.198572	2668.448545	23.248640
106.467346	2667.804407	23.253658
106.444385	2657.185332	23.258675
106.526263	2663.406510	23.263693
106.856553	2661.075279	23.268711
106.915612	2684.941060	23.273728
107.292444	2676.300143	23.278746
107.229294	2685.683806	23.283763
107.433842	2683.010849	23.288781
107.715890	2683.181089	23.293799
107.483034	2682.805757	23.298816
107.857368	2678.748992	23.303834
107.653066	2680.789533	23.308851
107.540472	2681.076540	23.313869
107.900148	2676.389890	23.318887
107.997330	2679.390231	23.323904
107.897591	2699.011303	23.328922
107.953203	2703.663145	23.333939
108.111102	2711.776156	23.338957
107.911829	2706.834726	23.343975
108.308188	2712.373702	23.348992
108.439345	2714.527407	23.354010
108.560840	2736.431983	23.359027
108.920053	2738.200525	23.364045
108.991021	2731.405009	23.369063
108.550232	2741.812548	23.374080
108.978635	2735.537194	23.379098
108.774730	2751.987254	23.384115
108.825749	2758.329354	23.389133
109.418697	2762.768286	23.394151
109.407218	2767.492718	23.399168
109.380464	2765.173954	23.404186
109.673057	2783.552692	23.409203
109.812851	2793.862994	23.414221
109.997513	2792.575699	23.419239
110.236835	2791.682497	23.424256
110.167283	2785.050870	23.429274
110.438703	2786.476898	23.434291
110.088414	2787.692049	23.439309
110.618520	2795.993660	23.444327
110.650775	2802.495993	23.449344
110.773090	2805.910320	23.454362
110.651706	2812.643321	23.459379
110.781328	2815.050068	23.464397
111.255313	2809.837262	23.469415
111.700223	2826.957978	23.474432
111.727678	2812.461254	23.479450
111.771072	2808.954762	23.484467
111.924150	2808.245982	23.489485
111.782204	2799.014785	23.494503
111.766113	2817.115705	23.499520
111.976476	2817.938061	23.504538
112.155825	2809.370443	23.509555
112.256405	2820.641676	23.514573
112.472319	2821.998973	23.519591
112.138379	2826.388400	23.524608
112.381315	2820.345030	23.529626
112.504609	2817.486327	23.534643
112.324561	2845.220697	23.539661
112.829071	2839.605143	23.544679
112.624915	2853.235864	23.549696
112.739922	2850.793916	23.554714
113.115287	2860.047326	23.559731
113.175246	2882.393860	23.564749
113.648177	2880.705084	23.569767
113.563372	2886.799316	23.574784
113.849276	2883.538354	23.579802
113.841178	2883.140234	23.584819
113.645941	2870.156555	23.589837
113.871105	2873.951865	23.594855
113.815518	2881.298023	23.599872
114.079206	2887.260714	23.604890
114.453504	2899.731882	23.609907
114.322420	2905.347162	23.614925
114.504242	2901.180590	23.619943
114.557408	2907.146775	23.624960
114.831450	2907.804606	23.629978
114.753896	2914.411461	23.634995
114.726178	2940.226843	23.640013
114.763600	2921.650099	23.645031
115.068707	2931.304233	23.650048
115.042054	2931.546645	23.655066
115.471137	2947.905500	23.660083
115.181995	2966.030314	23.665101
115.197928	2967.076342	23.670119
115.615578	2960.346746	23.675136
115.503351	2964.861978	23.680154
116.147437	2980.822511	23.685171
116.104761	2994.639135	23.690189
116.534941	2975.158408	23.695207
116.580154	3000.843258	23.700224
116.380331	2990.650228	23.705242
116.756863	2982.973836	23.710259
116.471118	2987.961646	23.715277
116.693897	2981.961331	23.720295
116.667280	2987.259649	23.725312
116.651085	2979.003197	23.730330
116.930574	2996.489805	23.735347
117.219710	2996.965983	23.740365
117.652000	2993.459001	23.745383
117.510735	2991.495481	23.750400
117.508888	2986.577063	23.755418
117.465000	2995.680918	23.760435
117.592682	3013.013231	23.765453
117.810076	3014.854198	23.770471
117.813244	3019.587296	23.775488
117.951527	3019.420379	23.780506
118.155521	3032.301089	23.785523
117.853998	3045.219751	23.790541
118.394865	3049.231560	23.795559
118.686845	3058.979696	23.800576
118.476229	3051.559125	23.805594
118.902314	3067.361471	23.810611
119.030319	3077.339246	23.815629
119.264854	3073.176469	23.820647
119.389883	3082.231435	23.825664
119.296175	3070.982835	23.830682
119.482855	3072.403286	23.835699
119.268309	3075.247615	23.840717
119.444518	3086.462767	23.845735
119.633586	3103.112087	23.850752
119.972090	3092.687786	23.855770
120.530437	3096.899871	23.860787
120.873290	3097.139941	23.865805
120.699856	3092.639014	23.870823
120.692020	3080.341008	23.875840
120.632831	3079.563545	23.880858
121.111263	3081.232389	23.885875
120.797769	3085.125928	23.890893
121.412286	3087.137544	23.895911
121.213725	3094.192573	23.900928
121.280811	3108.461570	23.905946
121.016850	3113.017022	23.910963
121.129506	3113.188250	23.915981
121.139175	3109.508540	23.920999
121.590389	3122.230121	23.926016
121.845678	3138.381030	23.931034
121.978039	3138.566309	23.936051
121.843850	3145.840999	23.941069
122.025687	3142.783122	23.946087
122.029936	3139.968949	23.951104
122.088058	3166.062592	23.956122
122.271183	3161.053533	23.961139
122.348948	3175.116073	23.966157
123.074060	3165.307855	23.971175
122.766496	3167.239227	23.976192
123.013341	3181.652056	23.981210
123.474501	3186.338232	23.986227
123.204400	3196.199547	23.991245
123.504907	3195.116219	23.996263
123.705261	3194.513749	24.001280
123.478175	3200.376212	24.006298
123.538641	3200.877798	24.011315
123.550878	3209.759833	24.016333
123.730140	3218.433784	24.021351
124.107228	3230.385022	24.026368
124.003140	3216.328720	24.031386
124.507231	3222.581937	24.036403
124.466809	3232.502360	24.041421
124.700962	3237.555834	24.046439
124.637291	3245.324412	24.051456
124.731546	3245.426253	24.056474
124.972191	3243.198821	24.061491
124.897601	3242.273501	24.066509
125.134875	3244.036775	24.071527
125.413391	3240.338344	24.076544
124.915872	3243.030889	24.081562
125.089557	3256.962198	24.086579
125.479997	3273.127799	24.091597
125.726343	3269.612677	24.096615
125.925854	3280.194114	24.101632
125.809969	3299.505600	24.106650
126.351119	3289.231764	24.111667
126.598366	3290.742180	24.116685
126.933146	3279.111563	24.121703
127.351327	3277.691321	24.126720
127.347893	3277.891687	24.131738
127.579256	3260.184367	24.136755
127.449215	3270.432730	24.141773
127.611550	3275.526107	24.146791
127.542800	3267.188069	24.151808
127.624231	3267.234162	24.156826
127.659619	3264.042708	24.161843
127.756872	3267.909771	24.166861
127.617309	3266.708604	24.171879
127.974646	3261.795378	24.176896
127.881617	3271.553686	24.181914
128.298064	3262.382192	24.186931
128.221335	3287.377473	24.191949
128.180659	3297.840553	24.196967
128.669778	3297.406257	24.201984
128.220014	3298.173362	24.207002
128.670849	3290.091916	24.212019
128.715585	3316.983783	24.217037
128.789350	3331.041617	24.222055
129.090303	3327.220527	24.227072
129.071935	3329.603124	24.232090
129.291954	3335.154698	24.237107
129.150736	3355.148485	24.242125
129.480581	3353.718897	24.247143
129.566606	3354.631638	24.252160
129.378934	3358.431493	24.257178
129.679489	3378.537742	24.262195
129.626884	3390.622327	24.267213
129.799240	3398.587216	24.272231
130.446077	3409.822829	24.277248
130.230942	3417.852514	24.282266
130.801842	3410.125897	24.287283
131.183233	3413.026389	24.292301
131.288345	3434.222388	24.297319
131.722598	3421.085605	24.302336
131.327881	3420.064244	24.307354
131.850947	3414.372957	24.312371
131.919596	3428.677424	24.317389
131.465529	3423.012276	24.322407
131.658299	3426.087043	24.327424
131.496520	3428.828956	24.332442
131.989843	3418.044031	24.337459
131.853185	3440.071638	24.342477
131.755999	3457.882806	24.347495
131.996610	3460.355077	24.352512
132.062579	3468.016780	24.357530
132.474422	3482.129998	24.362547
132.363440	3484.102764	24.367565
132.594798	3489.094968	24.372583
133.218313	3495.428461	24.377600
133.138712	3508.639402	24.382618
133.532304	3509.193920	24.387635
133.754492	3517.699864	24.392653
133.666118	3511.136024	24.397671
134.010941	3510.825714	24.402688
133.798055	3506.815135	24.407706
134.087256	3506.436894	24.412723
134.255734	3506.066902	24.417741
134.036389	3508.168321	24.422759
134.411173	3511.664485	24.427776
134.104822	3523.548398	24.432794
134.723569	3524.017465	24.437811
134.550213	3518.896646	24.442829
134.453138	3534.300524	24.447847
135.102997	3542.902754	24.452864
135.152215	3560.930683	24.457882
135.458756	3555.370220	24.462899
135.265570	3556.491595	24.467917
135.405556	3557.281195	24.472935
135.737104	3572.617427	24.477952
135.479023	3581.968659	24.482970
136.150784	3574.803616	24.487987
136.451277	3563.553334	24.493005
136.542266	3561.105031	24.498023
136.874508	3564.370060	24.503040
136.497741	3565.047084	24.508058
136.545979	3571.301777	24.513075
137.039088	3582.268934	24.518093
137.341155	3595.793340	24.523111
137.343194	3584.026036	24.528128
137.331934	3595.286490	24.533146
137.339909	3580.276088	24.538163
137.567428	3578.156316	24.543181
137.379919	3593.995409	24.548199
137.425442	3601.169965	24.553216
137.729493	3616.960077	24.558234
138.141169	3620.802933	24.563251
138.249480	3614.155178	24.568269
138.144442	3621.974129	24.573287
138.642147	3630.776517	24.578304
138.864512	3646.532196	24.583322
138.865121	3645.399843	24.588339
139.053087	3644.742717	24.593357
139.179921	3644.217812	24.598375
139.298550	3637.432883	24.603392
139.367854	3650.590455	24.608410
139.390342	3659.758479	24.613427
139.451145	3664.070333	24.618445
139.388428	3664.953867	24.623463
139.889374	3665.816970	24.628480
139.594016	3678.603221	24.633498
139.844644	3695.469745	24.638515
140.085557	3695.423974	24.643533
139.783809	3709.264986	24.648551
140.292415	3721.529042	24.653568
140.296092	3733.799445	24.658586
140.624694	3746.744302	24.663603
140.844985	3752.706271	24.668621
140.952800	3761.190010	24.673639
141.127041	3759.767345	24.678656
141.323616	3770.831949	24.683674
141.372757	3769.330846	24.688691
141.561476	3776.324974	24.693709
141.534966	3782.414198	24.698727
141.698169	3790.047300	24.703744
142.055404	3802.268061	24.708762
142.015036	3805.710429	24.713779
142.396187	3809.012665	24.718797
142.477932	3808.114882	24.723815
142.404017	3804.876120	24.728832
142.447257	3826.694430	24.733850
142.780360	3833.625609	24.738867
143.248834	3827.630213	24.743885
143.287892	3831.503149	24.748903
143.270499	3823.459076	24.753920
143.631701	3842.613201	24.758938
143.685399	3857.532832	24.763955
144.203267	3853.383799	24.768973
144.244705	3853.971257	24.773991
144.613466	3852.090612	24.779008
144.023422	3857.341495	24.784026
144.059304	3856.120577	24.789043
144.558929	3854.534764	24.794061
144.238974	3867.673334	24.799079
145.048622	3876.732729	24.804096
145.037752	3877.017420	24.809114
145.130922	3881.176298	24.814131
145.248899	3884.971163	24.819149
144.980916	3883.903508	24.824167
145.116819	3895.203904	24.829184
145.561634	3908.291812	24.834202
145.817253	3899.716832	24.839219
146.191832	3909.474614	24.844237
146.292394	3927.516091	24.849255
146.359472	3920.406882	24.854272
146.748205	3931.565671	24.859290
146.395270	3943.707283	24.864307
146.894352	3932.568639	24.869325
146.691801	3940.032247	24.874343
147.119545	3944.324547	24.879360
147.191151	3958.473474	24.884378
147.075060	3967.532797	24.889395
147.099464	3956.387178	24.894413
146.966185	3970.561892	24.899431
147.258398	3969.807498	24.904448
147.911039	3980.020764	24.909466
147.756194	3980.380177	24.914483
148.197241	4003.023307	24.919501
148.113915	4009.247668	24.924519
148.839752	3999.143893	24.929536
148.982943	4000.525195	24.934554
149.253532	4011.452456	24.939571
149.128016	4003.158897	24.944589
149.284935	4010.419870	24.949607
149.725417	4022.261563	24.954624
149.533272	4026.733678	24.959642
149.622541	4024.506093	24.964659
150.100565	4024.039370	24.969677
150.000006	4026.018740	24.974695
150.353600	4017.421903	24.979712
150.268181	4018.189132	24.984730
149.850079	4019.143553	24.989747
150.203594	4034.629369	24.994765
150.340903	4054.989241	24.999783
150.595773	4056.826863	25.004800
150.321706	4058.732693	25.009818
150.448421	4079.168383	25.014835
150.575660	4088.107802	25.019853
150.566038	4098.001604	25.024871
151.072242	4108.203457	25.029888
151.499344	4121.633909	25.034906
151.321625	4144.984488	25.039923
151.757436	4142.822942	25.044941
151.562602	4159.834473	25.049959
151.859298	4156.134384	25.054976
152.612810	4158.761734	25.059994
152.788563	4157.300981	25.065011
153.027871	4155.083884	25.070029
153.009113	4173.389210	25.075047
153.526562	4153.302669	25.080064
153.877313	4156.214302	25.085082
153.586504	4148.331656	25.090099
153.536580	4149.954542	25.095117
153.688102	4159.327829	25.100135
153.752666	4153.155692	25.105152
154.054024	4159.651674	25.110170
153.754882	4173.502111	25.115187
154.175352	4169.671985	25.120205
154.060192	4181.148187	25.125223
154.211827	4179.647339	25.130240
154.463666	4197.747860	25.135258
154.387536	4204.727127	25.140275
154.827438	4200.373998	25.145293
154.717489	4224.883697	25.150311
154.974580	4221.447696	25.155328
155.032999	4227.143785	25.160346
154.959566	4251.604144	25.165363
155.485241	4261.240567	25.170381
155.715042	4258.254833	25.175399
155.987017	4277.482990	25.180416
156.034696	4285.393054	25.185434
156.284731	4294.408264	25.190451
156.397464	4285.230733	25.195469
156.293292	4310.092418	25.200487
156.666464	4308.278322	25.205504
156.897913	4313.822048	25.210522
156.890946	4331.356968	25.215539
157.581354	4336.009342	25.220557
157.860157	4338.665204	25.225575
157.744269	4337.660839	25.230592
157.850740	4336.056440	25.235610
158.159634	4346.482607	25.240627
158.250884	4337.584252	25.245645
158.402792	4359.002111	25.250663
158.320026	4363.730995	25.255680
158.897309	4363.409215	25.260698
158.772917	4368.898686	25.265715
158.908973	4358.098068	25.270733
159.198154	4367.719517	25.275751
159.081504	4385.922439	25.280768
159.223913	4389.142011	25.285786
159.489015	4393.867438	25.290803
159.572763	4395.858755	25.295821
159.594072	4401.546111	25.300839
159.958223	4421.399394	25.305856
159.939739	4428.106144	25.310874
160.138406	4428.046525	25.315891
160.460654	4450.997889	25.320909
160.612366	4452.106116	25.325927
160.405555	4455.615267	25.330944
160.810109	4465.219967	25.335962
160.619584	4481.597949	25.340979
160.797049	4488.261925	25.345997
161.134576	4508.036263	25.351015
161.097417	4510.125652	25.356032
161.252799	4511.744387	25.361050
161.265067	4545.829674	25.366067
161.992396	4539.941025	25.371085
162.229360	4552.798612	25.376103
162.739395	4568.590897	25.381120
162.886148	4564.753396	25.386138
162.999500	4560.076412	25.391155
163.331928	4556.109617	25.396173
163.517023	4555.210370	25.401191
163.574491	4546.854614	25.406208
163.733409	4545.195801	25.411226
163.615207	4552.485417	25.416243
163.936892	4551.216954	25.421261
163.655199	4551.064684	25.426279
163.589073	4570.201325	25.431296
164.140448	4576.888262	25.436314
163.965091	4592.807851	25.441331
164.382556	4583.981944	25.446349
164.232948	4597.634645	25.451367
164.440650	4602.906780	25.456384
165.008781	4609.613785	25.461402
164.689986	4634.837690	25.466419
165.238755	4630.460055	25.471437
165.423131	4633.690031	25.476455
165.074786	4645.048596	25.481472
165.619368	4651.970596	25.486490
165.943909	4656.125492	25.491507
166.070817	4670.378097	25.496525
166.244750	4680.962372	25.501543
166.238917	4690.389689	25.506560
166.337530	4689.034638	25.511578
166.405081	4705.505427	25.516595
166.869096	4715.313039	25.521613
167.241300	4714.680386	25.526631
167.372914	4719.565915	25.531648
167.524112	4730.408380	25.536666
167.978810	4747.307889	25.541683
167.893999	4747.938805	25.546701
167.939784	4745.782136	25.551719
168.264484	4749.543255	25.556736
168.760479	4758.995907	25.561754
168.806963	4777.830569	25.566771
168.834556	4776.394381	25.571789
168.929217	4780.551282	25.576807
168.589910	4782.680676	25.581824
169.206350	4785.875115	25.586842
169.092403	4810.839235	25.591859
169.460835	4803.305857	25.596877
169.132195	4819.309425	25.601895
169.457187	4839.728910	25.606912
169.433943	4838.946173	25.611930
169.518280	4865.775443	25.616947
169.760718	4869.077725	25.621965
170.060481	4884.105111	25.626983
170.359813	4894.514331	25.632000
170.987435	4898.192073	25.637018
171.220872	4914.494543	25.642035
171.335802	4924.851731	25.647053
171.707098	4925.131218	25.652071
171.582397	4931.233658	25.657088
172.179980	4915.243119	25.662106
172.228150	4915.226621	25.667123
172.459869	4914.962257	25.672141
173.086350	4926.612676	25.677159
173.202494	4926.024139	25.682176
173.387027	4906.180978	25.687194
173.187371	4907.133406	25.692212
173.013513	4902.553663	25.697229
173.403045	4918.986924	25.702247
173.476768	4928.508272	25.707264
173.665759	4915.331855	25.712282
173.669417	4928.752246	25.717300
173.653057	4919.935236	25.722317
173.589076	4947.160232	25.727335
173.886071	4957.125698	25.732352
173.962747	4954.343268	25.737370
174.274896	4980.975005	25.742388
174.103555	4998.782128	25.747405
174.554353	4986.306397	25.752423
174.588613	5011.040652	25.757440
175.040991	5011.511435	25.762458
175.190925	5021.244632	25.767476
175.107441	5018.580161	25.772493
175.677244	5034.313370	25.777511
175.916154	5034.184059	25.782528
176.037562	5012.680823	25.787546
176.488987	5021.311735	25.792564
176.851683	5034.798568	25.797581
177.505719	5028.050872	25.802599
176.882901	5034.533035	25.807616
177.452810	5036.531858	25.812634
177.455525	5041.156170	25.817652
177.544486	5046.605699	25.822669
177.642706	5039.624303	25.827687
177.547728	5045.745476	25.832704
177.601210	5028.735552	25.837722
177.670042	5055.256634	25.842740
177.604439	5060.651519	25.847757
178.205866	5076.256655	25.852775
177.849379	5098.796442	25.857792
178.228477	5092.388169	25.862810
178.547770	5121.309998	25.867828
178.489086	5132.519184	25.872845
178.890882	5139.977838	25.877863
178.713111	5153.938915	25.882880
179.575119	5161.253377	25.887898
180.209954	5169.395527	25.892916
180.787290	5167.827789	25.897933
181.387726	5165.617491	25.902951
181.532923	5151.858261	25.907968
181.481120	5123.718430	25.912986
181.203904	5132.238144	25.918004
181.353908	5129.249757	25.923021
181.538432	5124.611972	25.928039
181.256556	5128.048687	25.933056
181.415457	5134.909767	25.938074
181.599548	5156.973902	25.943092
181.583538	5159.288258	25.948109
181.855868	5164.463212	25.953127
181.705831	5188.489626	25.958144
182.154241	5190.047928	25.963162
182.367291	5213.135902	25.968180
182.455478	5217.205787	25.973197
182.535023	5231.494336	25.978215
182.596703	5249.360681	25.983232
182.595477	5258.997068	25.988250
182.826345	5272.027951	25.993268
183.026426	5292.875960	25.998285
183.301001	5297.848176	26.003303
183.524287	5319.170426	26.008320
183.549707	5329.341134	26.013338
183.946202	5342.133481	26.018356
183.999780	5356.937600	26.023373
184.537438	5372.844247	26.028391
184.854704	5385.201659	26.033408
184.916998	5387.120272	26.038426
185.111377	5399.673746	26.043444
185.340847	5407.637652	26.048461
186.086740	5402.859253	26.053479
185.528136	5415.223611	26.058496
185.827866	5426.349823	26.063514
186.218358	5435.302973	26.068532
186.311589	5439.085395	26.073549
186.955214	5442.414861	26.078567
187.155481	5454.521627	26.083584
187.457387	5443.658842	26.088602
187.669879	5450.026789	26.093620
187.490131	5448.914037	26.098637
187.562459	5440.904239	26.103655
187.608057	5450.862174	26.108672
187.727534	5448.754597	26.113690
187.732450	5452.120887	26.118708
187.875773	5472.527278	26.123725
188.122118	5488.005168	26.128743
187.814222	5492.978934	26.133760
188.008593	5508.906531	26.138778
188.604872	5527.575126	26.143796
188.853090	5549.165263	26.148813
189.065132	5552.861813	26.153831
188.974621	5565.148508	26.158848
188.982332	5578.820809	26.163866
189.269876	5590.683987	26.168884
189.228583	5620.279397	26.173901
189.688374	5624.758623	26.178919
189.963552	5646.569666	26.183936
190.333599	5647.525136	26.188954
191.256403	5647.186886	26.193972
191.571072	5664.777748	26.198989
191.811028	5648.077990	26.204007
191.756116	5656.441331	26.209024
191.904735	5653.968165	26.214042
192.180447	5669.702837	26.219060
192.056531	5689.295431	26.224077
192.533586	5678.974393	26.229095
192.774182	5690.388640	26.234112
192.632468	5681.019448	26.239130
192.785340	5694.953628	26.244148
192.757638	5709.550268	26.249165
192.991257	5713.320455	26.254183
192.730432	5730.694338	26.259200
193.065594	5747.441516	26.264218
192.958741	5768.026114	26.269236
193.147871	5787.110791	26.274253
194.268728	5799.123926	26.279271
194.368088	5809.606363	26.284288
194.565063	5808.815339	26.289306
194.895704	5806.211091	26.294324
195.246460	5817.235376	26.299341
195.748534	5819.675610	26.304359
195.701100	5824.377794	26.309376
195.629793	5825.939821	26.314394
196.011113	5817.343706	26.319412
195.817130	5834.271050	26.324429
196.138826	5846.340613	26.329447
196.438033	5852.217025	26.334464
196.480327	5847.529416	26.339482
196.634328	5872.064763	26.344500
196.787501	5889.225109	26.349517
196.642908	5888.046625	26.354535
196.643138	5901.230555	26.359552
197.215904	5908.270514	26.364570
197.311698	5924.637071	26.369588
197.506584	5939.322167	26.374605
197.576277	5953.049077	26.379623
198.229423	5967.906942	26.384640
198.143838	5977.197845	26.389658
198.784398	5990.194327	26.394676
198.670491	6002.126097	26.399693
199.193378	6005.009480	26.404711
199.123657	6009.759528	26.409728
199.301746	6018.734916	26.414746
200.031773	6021.469680	26.419764
200.165333	6023.126855	26.424781
199.933895	6024.884059	26.429799
200.089195	6028.758700	26.434816
199.916394	6047.143779	26.439834
200.490426	6043.174280	26.444852
200.429407	6071.653033	26.449869
200.772221	6079.387365	26.454887
200.823611	6092.721265	26.459904
201.018960	6098.721355	26.464922
201.878209	6100.639954	26.469940
201.563060	6101.063457	26.474957
201.958756	6112.735783	26.479975
201.965027	6128.272309	26.484992
202.077893	6140.990354	26.490010
202.548643	6142.820712	26.495028
202.768305	6161.046198	26.500045
202.778414	6158.462860	26.505063
203.468981	6182.654345	26.510080
203.733390	6179.748356	26.515098
203.769804	6182.215614	26.520116
203.906677	6190.363067	26.525133
204.319451	6194.705348	26.530151
204.350157	6209.336851	26.535168
204.611210	6219.507573	26.540186
204.729543	6216.434456	26.545204
204.653830	6227.862269	26.550221
205.182441	6231.528433	26.555239
204.887793	6241.952180	26.560256
205.140788	6268.168242	26.565274
205.301313	6267.969248	26.570292
205.234059	6289.912904	26.575309
205.824824	6304.565643	26.580327
206.340345	6307.135256	26.585344
206.912245	6328.322183	26.590362
207.200420	6318.979636	26.595380
207.169456	6329.566774	26.600397
207.851735	6319.517612	26.605415
208.120756	6335.363542	26.610432
207.784444	6331.557047	26.615450
208.050316	6336.671239	26.620468
208.291400	6346.422404	26.625485
208.418393	6351.966882	26.630503
208.716098	6351.361518	26.635520
208.418995	6358.143736	26.640538
208.877901	6375.708276	26.645556
208.572889	6378.812782	26.650573
209.026671	6403.182573	26.655591
209.359838	6403.665339	26.660608
209.409140	6430.236082	26.665626
209.647992	6438.418703	26.670644
209.638254	6448.166710	26.675661
209.759159	6471.087529	26.680679
210.151060	6473.675348	26.685696
210.329936	6491.066794	26.690714
210.915664	6491.642285	26.695732
211.117821	6499.011102	26.700749
211.623232	6513.888518	26.705767
212.027165	6513.435628	26.710784
212.223306	6519.053741	26.715802
212.671997	6515.193958	26.720820
212.832106	6507.643983	26.725837
213.121087	6495.976874	26.730855
213.245966	6498.816214	26.735872
213.289479	6505.553714	26.740890
213.575606	6503.804252	26.745908
213.872380	6527.637161	26.750925
213.785678	6530.618781	26.755943
214.212408	6523.281270	26.760960
213.903110	6529.507150	26.765978
213.954018	6519.765981	26.770996
214.219418	6536.638223	26.776013
214.322766	6547.170109	26.781031
214.819843	6552.792580	26.786048
214.372631	6567.246263	26.791066
214.728729	6577.749563	26.796084
214.555151	6594.573508	26.801101
214.961830	6615.062853	26.806119
215.205387	6626.196885	26.811136
215.598508	6652.205993	26.816154
215.587745	6656.317108	26.821172
215.921213	6670.426930	26.826189
216.448131	6683.583861	26.831207
216.692896	6686.178047	26.836224
216.816703	6709.185370	26.841242
217.132494	6708.528942	26.846260
217.660433	6731.972458	26.851277
217.811195	6731.719947	26.856295
218.249104	6727.757146	26.861312
218.438210	6734.135801	26.866330
218.386589	6751.565044	26.871348
218.739599	6763.883733	26.876365
219.209366	6766.314523	26.881383
219.350080	6756.515754	26.886400
219.311643	6772.030409	26.891418
219.533049	6780.136553	26.896436
219.874845	6777.164826	26.901453
220.057448	6788.925046	26.906471
220.552524	6797.125930	26.911488
220.324441	6808.622012	26.916506
220.744199	6808.195629	26.921524
220.611319	6819.286011	26.926541
220.630212	6836.479149	26.931559
221.154459	6842.678501	26.936576
221.208542	6863.130659	26.941594
221.462383	6871.802513	26.946612
221.296685	6892.180166	26.951629
221.240526	6911.210861	26.956647
221.668173	6918.175358	26.961664
221.726183	6950.258363	26.966682
222.517832	6966.218156	26.971700
222.738255	6993.081201	26.976717
223.209563	7003.742867	26.981735
223.348567	6999.735933	26.986752
223.314596	7018.711085	26.991770
224.016512	7022.480972	26.996788
224.120751	7049.412252	27.001805
224.309751	7068.109389	27.006823
224.346368	7059.728203	27.011840
224.400171	7086.040942	27.016858
224.990957	7089.736365	27.021876
225.482762	7111.866315	27.026893
225.737230	7121.035222	27.031911
225.632380	7122.735277	27.036928
225.627889	7142.913965	27.041946
225.777158	7153.565439	27.046964
226.237804	7172.402668	27.051981
226.257472	7181.550759	27.056999
226.765793	7195.763540	27.062016
227.064649	7222.073596	27.067034
227.291925	7220.981306	27.072052
227.478665	7228.563334	27.077069
227.763340	7243.116573	27.082087
227.961648	7243.721023	27.087104
228.177130	7265.615899	27.092122
228.555023	7252.571570	27.097140
229.168493	7241.578603	27.102157
229.406891	7234.988846	27.107175
229.754879	7226.661386	27.112192
229.997124	7237.738567	27.117210
229.874239	7243.584022	27.122228
230.251196	7251.143121	27.127245
230.561688	7267.024054	27.132263
230.760215	7262.188768	27.137280
230.566025	7270.739938	27.142298
231.088783	7262.140029	27.147316
231.213597	7267.494573	27.152333
231.268501	7280.157000	27.157351
231.680757	7286.344417	27.162368
231.326428	7299.374958	27.167386
231.255585	7305.645800	27.172404
231.528401	7321.073830	27.177421
231.654161	7351.210270	27.182439
231.770395	7364.451759	27.187456
232.130964	7389.176474	27.192474
232.283886	7411.723121	27.197492
232.502851	7427.710006	27.202509
232.812238	7447.989741	27.207527
233.164141	7460.274499	27.212544
233.184915	7483.250438	27.217562
233.645091	7494.839821	27.222580
234.354568	7507.199111	27.227597
234.724411	7511.645780	27.232615
235.034080	7531.983866	27.237632
235.106687	7551.391716	27.242650
235.279410	7556.249242	27.247668
235.614115	7566.308558	27.252685
236.083298	7585.199999	27.257703
236.434714	7584.806224	27.262720
236.225045	7608.968301	27.267738
236.243795	7612.316997	27.272756
236.604778	7629.235963	27.277773
237.011715	7645.100462	27.282791
237.735714	7635.477572	27.287808
237.788065	7661.282653	27.292826
237.963592	7663.973578	27.297844
238.230528	7664.672195	27.302861
237.970773	7673.769320	27.307879
239.151126	7670.898354	27.312896
239.232028	7674.063443	27.317914
239.313445	7677.888538	27.322932
239.731752	7685.007742	27.327949
239.985442	7704.660600	27.332967
240.285464	7697.591733	27.337984
240.399011	7703.724180	27.343002
240.227411	7692.257967	27.348020
240.869651	7705.990518	27.353037
240.716530	7724.069424	27.358055
241.062570	7735.353416	27.363072
241.180224	7731.746847	27.368090
241.155431	7744.325209	27.373108
241.707175	7752.117814	27.378125
241.822957	7767.013100	27.383143
241.843441	7784.997853	27.388160
242.275762	7791.994258	27.393178
242.556999	7810.515466	27.398196
242.649185	7810.493230	27.403213
242.798438	7832.861487	27.408231
243.242796	7850.234733	27.413248
243.166111	7856.238154	27.418266
243.377206	7874.261444	27.423284
243.755802	7884.978497	27.428301
243.928962	7920.997049	27.433319
244.246236	7918.809810	27.438336
244.707280	7946.074030	27.443354
245.172270	7945.941016	27.448372
245.762828	7924.515794	27.453389
245.935564	7926.654256	27.458407
246.682132	7923.014834	27.463424
246.676636	7930.170691	27.468442
246.487621	7943.962788	27.473460
247.125158	7943.437183	27.478477
247.172188	7957.328711	27.483495
247.138071	7953.341638	27.488512
246.970245	7957.886431	27.493530
247.372811	7966.824842	27.498548
247.579206	7970.397656	27.503565
247.475557	7995.993671	27.508583
247.558604	8020.531528	27.513600
248.184665	8016.300054	27.518618
247.851554	8033.737295	27.523636
248.539409	8053.531133	27.528653
248.420519	8074.723319	27.533671
248.789421	8089.276732	27.538688
249.070638	8119.994554	27.543706
249.110662	8132.192224	27.548724
249.441108	8149.066404	27.553741
249.713758	8174.222866	27.558759
250.146595	8195.334574	27.563776
250.644969	8213.699653	27.568794
250.415975	8231.789376	27.573812
251.441101	8231.493978	27.578829
252.131001	8254.926232	27.583847
252.334131	8257.380294	27.588864
252.516399	8251.639162	27.593882
252.751325	8272.416774	27.598900
253.030298	8275.374987	27.603917
253.170399	8276.936000	27.608935
253.461006	8277.132870	27.613952
253.342605	8292.944298	27.618970
253.516516	8307.860366	27.623988
254.019923	8321.970997	27.629005
254.155441	8337.830871	27.634023
254.718411	8347.702303	27.639040
254.787333	8360.717739	27.644058
254.667474	8372.821634	27.649076
255.165859	8385.596374	27.654093
254.892202	8402.451456	27.659111
255.439347	8422.235260	27.664128
255.429487	8440.640929	27.669146
255.754073	8460.976149	27.674164
256.341093	8471.023267	27.679181
257.386527	8469.107269	27.684199
258.330718	8468.730789	27.689216
258.406274	8462.106929	27.694234
258.349639	8470.012785	27.699252
258.894433	8467.798701	27.704269
258.798554	8472.660960	27.709287
259.293058	8466.236111	27.714304
259.063079	8461.822988	27.719322
259.051034	8490.731977	27.724340
259.417872	8487.186246	27.729357
259.346262	8500.996340	27.734375
259.431253	8519.563582	27.739392
259.509027	8530.041164	27.744410
259.544960	8550.520561	27.749428
260.133303	8576.007261	27.754445
259.756372	8595.858947	27.759463
260.286467	8618.001968	27.764480
260.544385	8620.426503	27.769498
261.102985	8649.421364	27.774516
261.468074	8658.123767	27.779533
261.838814	8678.407483	27.784551
261.990995	8680.540797	27.789568
262.239801	8694.059136	27.794586
262.001416	8719.002017	27.799604
262.337434	8728.112616	27.804621
262.619934	8748.289768	27.809639
262.954752	8766.413250	27.814656
263.878324	8777.981727	27.819674
263.140496	8797.416243	27.824692
264.077196	8802.683683	27.829709
264.455883	8829.321081	27.834727
264.447463	8843.466008	27.839744
264.875856	8854.741840	27.844762
265.193969	8882.517457	27.849780
265.515718	8884.320128	27.854797
265.435416	8903.782600	27.859815
265.746511	8922.208760	27.864832
266.133812	8932.763585	27.869850
266.097756	8957.447134	27.874868
266.715350	8967.586383	27.879885
266.953218	8983.299125	27.884903
267.075285	9005.967378	27.889920
267.680067	9022.896164	27.894938
267.564217	9043.940240	27.899956
267.774015	9047.509582	27.904973
268.178313	9072.605411	27.909991
268.307389	9095.367159	27.915008
268.610554	9112.706949	27.920026
268.741150	9122.454546	27.925044
269.389858	9138.544272	27.930061
269.328973	9161.038320	27.935079
270.052298	9178.223297	27.940096
270.344533	9183.352154	27.945114
270.816079	9204.409139	27.950132
271.118741	9213.406604	27.955149
271.177728	9232.213749	27.960167
271.214236	9247.031418	27.965184
271.698658	9263.930827	27.970202
271.705881	9279.953174	27.975220
272.022867	9300.343508	27.980237
272.206015	9322.397835	27.985255
272.240157	9342.558703	27.990272
272.943366	9360.985610	27.995290
272.877310	9385.878050	28.000308
273.414443	9416.286424	28.005325
273.816758	9413.071770	28.010343
275.643276	9406.629288	28.015360
276.604384	9387.331385	28.020378
276.622851	9386.799097	28.025396
277.213261	9359.044526	28.030413
277.140693	9363.585706	28.035431
277.048648	9363.581473	28.040448
277.473009	9358.473280	28.045466
276.951513	9343.739574	28.050484
277.025355	9351.873913	28.055501
276.974843	9359.768160	28.060519
276.916891	9366.463857	28.065536
277.170417	9374.783420	28.070554
277.083683	9403.984552	28.075572
277.762940	9417.004222	28.080589
277.880212	9432.560978	28.085607
277.787317	9461.343348	28.090624
277.911789	9483.738517	28.095642
278.116137	9504.858409	28.100660
278.486313	9529.572246	28.105677
278.684378	9564.529211	28.110695
278.925738	9594.484453	28.115712
279.564819	9607.154084	28.120730
279.443361	9633.006978	28.125748
280.074394	9657.873047	28.130765
280.102912	9673.449508	28.135783
280.289699	9699.596353	28.140800
280.350324	9721.204420	28.145818
281.105198	9744.542203	28.150836
281.241327	9773.899992	28.155853
281.613097	9798.289404	28.160871
281.799334	9816.479727	28.165888
282.384596	9828.529808	28.170906
282.081120	9852.127873	28.175924
282.638322	9875.358459	28.180941
283.104864	9901.812092	28.185959
283.011769	9927.696985	28.190976
283.680153	9941.239632	28.195994
284.124070	9981.033199	28.201012
284.194291	9997.378252	28.206029
284.642593	10018.058080	28.211047
284.747306	10043.538449	28.216064
284.896988	10061.800511	28.221082
284.948435	10090.602567	28.226100
285.661354	10127.176116	28.231117
285.809740	10135.412701	28.236135
286.530913	10153.089898	28.241152
287.052673	10162.888951	28.246170
287.596454	10180.098535	28.251188
288.101013	10201.736700	28.256205
288.353760	10205.346436	28.261223
288.592532	10221.016123	28.266240
288.955968	10223.841710	28.271258
289.083434	10236.277770	28.276276
289.420684	10242.644252	28.281293
289.819232	10249.192783	28.286311
290.011960	10270.354216	28.291328
290.426610	10276.012991	28.296346
290.466456	10278.106097	28.301364
290.481493	10302.757225	28.306381
291.024764	10311.003928	28.311399
290.884384	10331.778023	28.316416
291.565427	10347.454716	28.321434
291.627977	10369.350892	28.326452
291.663083	10387.419644	28.331469
292.197031	10406.439966	28.336487
292.345985	10429.012797	28.341504
292.692184	10439.259527	28.346522
292.947385	10460.906379	28.351540
293.314497	10480.401996	28.356557
293.810244	10500.066922	28.361575
293.744493	10517.452190	28.366592
294.197749	10540.100675	28.371610
294.375159	10566.571137	28.376628
294.693852	10581.244674	28.381645
295.175120	10601.428166	28.386663
295.155063	10625.849265	28.391680
295.519245	10630.763373	28.396698
296.071145	10662.097373	28.401716
296.080852	10673.080064	28.406733
296.119931	10690.727787	28.411751
296.748943	10723.711452	28.416768
297.224421	10734.448206	28.421786
297.626263	10758.901048	28.426804
297.704725	10766.765102	28.431821
298.126527	10802.391135	28.436839
298.642687	10811.137373	28.441856
299.365087	10811.529632	28.446874
301.186668	10799.395223	28.451892
301.113067	10793.492433	28.456909
301.707349	10777.588012	28.461927
301.704173	10771.314270	28.466944
302.175198	10753.961797	28.471962
302.399022	10755.054558	28.476980
302.148784	10747.666883	28.481997
302.367520	10745.435767	28.487015
302.230710	10741.760503	28.492032
302.589127	10741.839790	28.497050
302.496844	10746.973156	28.502068
302.537222	10744.106727	28.507085
302.554365	10755.657066	28.512103
302.405964	10778.658743	28.517120
302.819447	10793.006314	28.522138
302.876635	10821.596004	28.527156
303.009874	10850.247168	28.532173
303.608057	10862.660661	28.537191
303.795758	10900.738216	28.542208
304.040102	10926.709679	28.547226
304.263643	10949.823137	28.552244
304.268385	10981.442473	28.557261
304.598804	11008.439743	28.562279
304.889688	11056.162859	28.567296
305.318558	11084.784234	28.572314
305.778156	11108.586690	28.577332
305.991691	11145.743453	28.582349
306.559048	11163.945255	28.587367
306.668779	11191.600335	28.592384
307.287050	11213.734664	28.597402
308.238656	11227.334564	28.602420
308.458272	11245.847924	28.607437
308.988060	11265.657042	28.612455
308.929350	11293.794095	28.617472
309.299870	11306.420663	28.622490
309.462389	11329.893043	28.627508
309.621253	11346.112858	28.632525
310.176614	11367.317123	28.637543
310.616352	11393.085118	28.642560
311.000643	11405.161110	28.647578
311.220772	11432.979476	28.652596
311.476252	11442.254701	28.657613
312.038204	11460.678345	28.662631
311.964059	11482.617648	28.667648
312.352321	11506.591695	28.672666
312.835838	11518.968019	28.677684
312.928852	11543.815300	28.682701
313.452627	11563.800694	28.687719
313.555210	11590.780060	28.692736
313.685435	11612.658799	28.697754
314.021024	11634.730364	28.702772
314.209934	11666.359836	28.707789
314.778486	11693.666940	28.712807
314.805736	11719.491374	28.717824
314.984192	11747.771032	28.722842
315.461711	11767.808485	28.727860
315.826147	11792.715060	28.732877
316.232367	11816.519548	28.737895
316.309027	11854.154506	28.742912
317.080368	11874.701116	28.747930
317.530338	11892.671114	28.752948
318.063409	11906.111054	28.757965
318.485945	11917.037038	28.762983
319.018250	11938.997548	28.768000
319.109735	11944.737392	28.773018
319.649009	11960.940326	28.778036
320.391462	11966.428636	28.783053
320.314687	11974.596411	28.788071
320.144974	11998.362901	28.793088
320.379997	12004.112013	28.798106
320.919243	12027.559065	28.803124
320.922623	12045.734217	28.808141
321.083358	12062.973998	28.813159
321.297021	12090.854449	28.818176
321.454302	12101.654435	28.823194
321.893809	12125.420756	28.828212
322.163655	12149.098686	28.833229
322.642525	12171.277974	28.838247
322.670027	12195.924400	28.843264
322.953557	12214.382551	28.848282
323.347253	12235.441472	28.853300
323.385626	12270.801936	28.858317
323.892854	12289.683158	28.863335
324.158926	12326.120041	28.868352
324.743759	12344.484162	28.873370
325.179933	12368.996774	28.878388
325.404560	12394.507414	28.883405
325.973737	12409.572789	28.888423
326.328070	12445.664347	28.893440
326.750964	12459.438224	28.898458
327.164833	12475.533287	28.903476
327.394970	12497.817377	28.908493
327.917126	12515.848567	28.913511
327.885161	12541.677842	28.918528
328.178290	12565.757511	28.923546
328.866690	12578.995711	28.928564
328.615269	12609.962661	28.933581
329.132088	12628.888386	28.938599
329.799008	12668.441150	28.943616
329.776714	12680.417020	28.948634
330.432900	12705.371085	28.953652
330.243692	12727.154681	28.958669
330.605594	12734.679491	28.963687
331.056331	12770.736846	28.968704
331.549044	12806.527284	28.973722
332.011575	12819.599912	28.978740
332.144090	12846.029554	28.983757
333.171130	12858.783082	28.988775
333.567431	12874.492211	28.993792
333.492788	12900.532437	28.998810
334.335900	12904.737322	29.003828
334.505802	12927.460656	29.008845
334.754737	12948.787241	29.013863
334.868290	12967.485658	29.018880
334.853207	12992.524886	29.023898
335.502190	13005.232597	29.028916
335.812988	13035.828021	29.033933
335.963625	13056.075812	29.038951
336.311911	13083.771707	29.043968
336.169633	13117.126349	29.048986
336.989109	13138.131469	29.054004
337.017584	13157.629051	29.059021
337.444909	13190.161138	29.064039
337.883043	13208.077829	29.069056
338.105351	13238.409393	29.074074
338.613409	13258.180436	29.079092
338.754160	13286.374478	29.084109
339.130581	13307.436084	29.089127
339.737773	13334.706440	29.094144
340.299687	13359.573159	29.099162
340.488464	13373.698743	29.104180
340.751163	13406.014337	29.109197
341.070119	13424.904519	29.114215
341.612322	13460.128709	29.119232
342.021264	13478.789674	29.124250
342.145915	13499.552945	29.129268
342.461566	13519.457130	29.134285
343.199572	13540.313982	29.139303
343.586938	13559.842255	29.144320
343.610248	13576.772363	29.149338
344.382952	13585.211158	29.154356
344.535575	13601.502029	29.159373
344.865154	13609.746533	29.164391
345.485363	13632.682872	29.169408
345.601661	13646.433043	29.174426
346.062108	13655.686521	29.179444
345.981394	13673.165114	29.184461
346.363125	13679.968424	29.189479
346.657749	13705.031367	29.194496
346.523885	13733.783995	29.199514
347.191763	13748.801125	29.204532
347.242522	13774.686377	29.209549
347.482893	13808.539916	29.214567
347.994219	13826.761906	29.219584
347.959108	13859.594364	29.224602
348.679361	13877.318360	29.229620
348.843813	13911.521989	29.234637
349.827943	13939.383209	29.239655
349.814202	13959.189777	29.244672
350.073602	13999.246874	29.249690
350.506778	14008.410523	29.254708
350.861852	14052.420260	29.259725
351.259669	14071.017559	29.264743
351.442808	14105.382394	29.269760
351.498442	14137.319338	29.274778
352.559654	14165.656709	29.279796
352.646880	14190.036179	29.284813
352.654466	14227.593528	29.289831
352.961701	14258.521227	29.294848
353.335407	14298.460777	29.299866
353.881509	14320.004566	29.304884
354.317966	14347.566603	29.309901
354.236811	14373.704816	29.314919
354.742591	14418.916669	29.319936
355.456381	14439.439846	29.324954
356.903979	14441.904057	29.329972
357.572881	14459.432332	29.334989
357.643354	14472.089145	29.340007
358.328305	14474.423153	29.345024
358.451682	14494.899480	29.350042
359.084181	14502.170546	29.355060
359.081557	14510.893076	29.360077
359.449428	14527.383947	29.365095
359.818440	14537.989619	29.370112
359.632762	14565.256626	29.375130
360.062119	14581.045444	29.380148
360.332441	14602.179933	29.385165
360.378221	14619.299667	29.390183
360.718767	14639.128583	29.395200
360.917199	14680.732571	29.400218
361.053019	14702.192139	29.405236
361.340094	14742.095152	29.410253
361.539804	14770.245706	29.415271
361.858663	14807.101750	29.420288
362.274050	14849.664639	29.425306
362.387842	14870.270690	29.430324
363.025398	14908.454682	29.435341
363.416587	14955.053528	29.440359
364.044085	14995.526321	29.445376
364.962028	15008.796152	29.450394
365.816760	15014.831114	29.455412
366.503224	15030.440536	29.460429
367.541603	15032.413305	29.465447
368.462739	15025.197907	29.470464
368.769076	15030.017374	29.475482
369.347470	15015.347167	29.480500
369.748804	14999.248483	29.485517
369.590667	14988.450210	29.490535
369.794883	14972.677452	29.495552
369.872343	14981.314428	29.500570
369.882254	14977.443609	29.505588
370.250849	14981.677442	29.510605
370.097387	14995.308066	29.515623
370.450096	15004.255532	29.520640
370.541896	15022.359415	29.525658
370.626366	15041.652924	29.530676
370.717734	15061.050910	29.535693
370.734016	15094.236655	29.540711
371.409673	15116.012154	29.545728
371.610250	15164.785209	29.550746
371.692651	15183.694654	29.555764
371.778009	15221.958495	29.560781
372.244174	15259.930630	29.565799
372.792313	15301.197548	29.570816
372.954408	15338.052455	29.575834
373.505504	15363.485131	29.580852
373.793452	15414.737872	29.585869
374.167531	15437.870521	29.590887
374.749930	15466.910696	29.595904
375.328799	15502.903935	29.600922
375.773807	15542.872500	29.605940
376.311481	15579.537890	29.610957
376.278599	15600.511249	29.615975
376.829981	15638.005132	29.620992
377.267277	15688.225166	29.626010
377.899261	15712.543201	29.631028
378.487035	15730.420468	29.636045
378.790985	15764.961002	29.641063
379.343350	15779.382909	29.646080
380.063983	15792.257435	29.651098
380.604632	15820.436693	29.656116
380.897984	15835.046682	29.661133
381.267157	15862.278835	29.666151
381.630400	15864.740573	29.671168
381.866152	15893.195997	29.676186
382.175919	15919.891173	29.681204
382.640422	15934.991391	29.686221
382.744345	15968.175371	29.691239
383.182435	15986.821748	29.696256
383.484123	16018.883823	29.701274
383.805746	16045.859375	29.706292
383.874872	16080.571979	29.711309
383.948843	16127.783243	29.716327
384.579306	16148.844137	29.721344
384.837541	16189.155810	29.726362
385.354090	16225.238217	29.731380
385.528497	16261.538310	29.736397
386.029059	16289.370377	29.741415
386.477909	16333.321784	29.746432
386.834472	16361.281924	29.751450
387.475568	16396.647319	29.756468
387.792097	16433.433309	29.761485
387.973861	16466.750374	29.766503
388.611378	16498.265806	29.771520
389.590688	16526.751708	29.776538
389.614284	16548.541269	29.781556
390.059432	16581.959832	29.786573
390.858461	16585.555132	29.791591
391.975817	16598.964952	29.796608
392.257495	16623.774419	29.801626
392.689415	16623.170067	29.806644
393.101158	16635.699349	29.811661
393.188315	16655.260688	29.816679
393.486192	16664.648491	29.821696
394.221216	16676.290259	29.826714
394.401295	16682.412695	29.831732
395.002696	16698.931586	29.836749
395.043544	16709.783905	29.841767
395.576521	16710.784749	29.846784
395.939830	16735.114248	29.851802
396.026787	16756.899864	29.856820
396.430543	16764.583521	29.861837
397.044043	16768.542276	29.866855
397.443198	16781.441033	29.871872
397.808240	16794.990165	29.876890
397.683889	16820.315035	29.881908
398.063981	16830.581453	29.886925
398.299372	16866.180756	29.891943
398.511699	16883.926183	29.896960
398.813527	16914.861352	29.901978
399.001598	16948.881368	29.906996
399.462361	16975.959855	29.912013
399.544548	17014.735944	29.917031
400.497647	17042.073242	29.922048
400.928415	17065.964845	29.927066
401.212799	17101.737791	29.932084
402.072909	17121.664676	29.937101
402.566068	17161.108981	29.942119
402.830171	17173.696299	29.947136
403.084190	17210.681983	29.952154
403.389488	17242.931839	29.957172
403.890375	17273.874022	29.962189
404.033328	17309.864798	29.967207
404.488513	17330.855435	29.972224
404.492495	17370.209670	29.977242
404.579964	17408.508172	29.982260
405.594907	17445.066906	29.987277
405.537477	17497.149573	29.992295
406.317186	17515.249116	29.997312
406.532431	17551.950376	30.002330
406.878386	17590.931484	30.007348
407.459239	17632.252394	30.012365
407.969619	17662.271555	30.017383
408.482343	17703.462085	30.022400
409.301091	17734.114299	30.027418
409.917909	17763.037727	30.032436
410.436165	17794.094648	30.037453
410.352636	17825.877406	30.042471
411.274954	17837.865645	30.047488
411.884053	17865.694951	30.052506
411.835363	17879.733011	30.057524
412.674691	17908.189381	30.062541
413.332479	17930.419269	30.067559
413.841257	17947.853338	30.072576
414.084350	17974.058459	30.077594
414.451120	18001.207832	30.082612
414.488821	18008.196204	30.087629
415.044341	18039.458632	30.092647
415.144767	18064.376029	30.097664
415.287355	18094.695100	30.102682
415.772231	18124.832835	30.107700
416.352565	18152.907015	30.112717
416.907118	18182.284487	30.117735
416.990539	18212.008257	30.122752
417.630478	18239.866173	30.127770
417.996263	18269.959319	30.132788
418.459296	18297.520397	30.137805
418.757756	18333.776044	30.142823
419.379963	18350.907940	30.147840
419.747249	18372.652264	30.152858
420.806825	18397.253203	30.157876
421.748710	18395.362853	30.162893
422.073436	18408.313077	30.167911
422.415137	18425.788012	30.172928
422.933013	18440.359860	30.177946
422.828935	18458.785371	30.182964
423.309136	18470.756075	30.187981
423.410149	18482.151312	30.192999
423.637568	18509.725078	30.198016
423.843753	18531.548392	30.203034
423.780011	18563.427009	30.208052
424.310923	18581.137099	30.213069
424.321810	18616.433775	30.218087
424.660791	18665.720682	30.223104
425.107881	18699.704410	30.228122
425.105853	18742.568933	30.233140
425.557154	18774.654051	30.238157
425.904352	18830.376797	30.243175
426.074963	18869.620189	30.248192
426.981968	18928.784742	30.253210
427.227514	18975.948797	30.258228
427.784351	19021.604603	30.263245
428.012122	19078.580829	30.268263
428.773219	19121.360558	30.273280
429.154382	19164.518804	30.278298
429.493925	19217.929804	30.283316
430.181621	19252.875777	30.288333
430.903252	19305.860997	30.293351
431.282709	19336.409411	30.298368
432.068225	19363.497757	30.303386
432.876087	19394.980943	30.308404
433.657583	19434.891965	30.313421
433.672975	19463.847300	30.318439
434.285687	19488.889836	30.323456
434.752295	19523.587745	30.328474
434.814289	19560.987331	30.333492
435.280285	19589.573228	30.338509
435.756238	19621.479304	30.343527
436.023241	19655.357727	30.348544
436.701854	19702.987928	30.353562
437.007043	19738.703169	30.358580
437.577050	19761.255939	30.363597
438.031191	19803.656421	30.368615
438.426350	19832.524091	30.373632
439.082892	19853.437172	30.378650
439.192002	19905.710941	30.383668
439.428777	19926.186176	30.388685
440.463549	19961.515850	30.393703
440.559866	19997.487056	30.398720
440.886629	20027.572508	30.403738
441.188575	20077.654861	30.408756
441.790596	20104.055962	30.413773
442.576486	20149.219589	30.418791
442.316835	20184.414722	30.423808
442.984402	20212.813696	30.428826
443.571645	20264.816823	30.433844
444.306722	20281.676551	30.438861
444.343487	20325.943433	30.443879
445.333011	20339.774853	30.448896
446.437278	20366.851302	30.453914
446.724930	20393.637741	30.458932
447.342733	20412.161494	30.463949
447.780239	20440.116619	30.468967
447.881511	20446.502640	30.473984
448.724512	20476.397520	30.479002
449.325191	20497.511458	30.484020
450.208550	20509.959030	30.489037
450.299640	20523.611887	30.494055
450.707302	20536.302458	30.499072
450.821193	20561.180341	30.504090
450.924596	20590.588108	30.509108
451.483158	20607.188959	30.514125
451.955844	20637.074683	30.519143
452.136318	20659.819494	30.524160
452.518058	20680.582171	30.529178
452.294088	20709.229392	30.534196
452.931065	20733.943396	30.539213
453.951117	20750.092497	30.544231
454.302269	20781.676223	30.549248
455.111997	20799.295062	30.554266
455.577978	20831.993428	30.559284
455.585283	20856.082200	30.564301
456.123922	20883.687015	30.569319
456.245449	20915.728524	30.574336
456.662732	20943.952728	30.579354
456.832499	20972.845604	30.584372
457.119956	21013.559828	30.589389
457.366455	21059.994847	30.594407
457.966668	21108.111909	30.599424
458.361525	21146.153475	30.604442
458.532616	21190.490190	30.609460
458.824049	21241.189509	30.614477
459.198156	21282.184832	30.619495
459.557455	21347.859765	30.624512
460.082994	21397.254573	30.629530
460.634769	21453.316263	30.634548
461.213736	21499.071313	30.639565
462.126561	21545.237749	30.644583
462.410555	21593.295188	30.649600
462.895701	21632.521170	30.654618
463.218024	21681.086509	30.659636
464.390143	21725.420773	30.664653
465.020675	21765.893774	30.669671
465.156674	21809.952550	30.674688
465.949103	21852.262590	30.679706
466.140077	21894.016697	30.684724
466.662596	21929.132855	30.689741
467.680970	21953.715930	30.694759
467.893896	21999.186240	30.699776
468.335125	22041.274418	30.704794
468.836316	22076.864304	30.709812
469.601461	22090.754945	30.714829
470.611749	22121.853280	30.719847
470.703167	22155.835272	30.724864
471.349118	22181.948520	30.729882
471.544011	22225.617012	30.734900
471.942626	22250.494245	30.739917
472.584736	22290.917700	30.744935
473.093955	22319.486867	30.749952
473.364748	22347.559569	30.754970
473.635543	22387.636533	30.759988
474.197076	22419.861677	30.765005
474.787904	22461.005196	30.770023
474.481656	22492.783298	30.775040
475.200786	22538.976736	30.780058
475.312691	22579.058465	30.785076
475.911097	22618.490254	30.790093
476.405171	22675.945301	30.795111
476.676675	22720.559479	30.800128
477.413586	22768.478801	30.805146
477.685396	22809.428584	30.810164
477.940919	22856.809983	30.815181
479.215480	22897.197650	30.820199
479.655980	22939.316560	30.825216
480.898870	22968.804122	30.830234
481.089749	23005.287961	30.835252
481.922962	23043.068610	30.840269
482.078025	23071.393528	30.845287
481.977429	23103.381450	30.850304
482.890793	23133.222056	30.855322
483.165628	23179.528872	30.860340
483.844154	23201.981502	30.865357
484.540186	23234.412928	30.870375
484.485769	23258.860700	30.875392
484.660769	23282.273812	30.880410
484.992136	23326.491723	30.885428
485.320371	23361.207892	30.890445
485.880517	23410.643820	30.895463
486.108892	23458.200129	30.900480
486.620318	23491.973113	30.905498
487.266614	23554.157068	30.910516
487.485443	23592.487242	30.915533
488.102553	23634.545427	30.920551
489.265499	23673.199945	30.925568
489.755009	23707.699229	30.930586
490.744435	23750.905372	30.935604
491.109968	23788.360079	30.940621
491.895528	23810.533968	30.945639
492.045046	23852.878505	30.950656
492.404160	23873.328741	30.955674
492.704038	23929.102978	30.960692
493.164821	23967.601968	30.965709
493.916030	24002.779054	30.970727
494.010471	24059.098766	30.975744
494.555335	24091.553778	30.980762
494.957738	24141.514766	30.985780
495.017659	24183.543838	30.990797
495.553098	24232.205649	30.995815
495.898215	24291.644755	31.000832
496.666976	24348.272906	31.005850
496.823979	24404.898763	31.010868
496.973428	24446.875764	31.015885
497.623288	24509.327541	31.020903
498.100923	24562.018089	31.025920
498.653134	24618.743026	31.030938
499.426368	24679.500147	31.035956
499.628993	24734.085161	31.040973
500.555624	24785.118498	31.045991
500.989854	24849.957097	31.051008
501.689164	24895.303888	31.056026
502.313895	24951.033809	31.061044
502.850910	25003.428831	31.066061
503.975641	25037.867886	31.071079
504.404973	25085.647671	31.076096
505.261721	25122.853398	31.081114
505.889795	25162.652022	31.086132
506.165780	25195.273639	31.091149
506.611260	25233.484684	31.096167
507.054542	25282.713604	31.101184
507.676055	25311.811654	31.106202
508.065421	25348.117704	31.111220
508.448840	25398.236906	31.116237
508.782077	25444.343015	31.121255
509.097607	25488.140172	31.126272
509.964994	25526.234488	31.131290
510.597052	25571.871806	31.136308
511.446462	25607.597332	31.141325
512.201105	25638.500112	31.146343
512.844788	25664.295775	31.151360
513.117892	25701.300036	31.156378
513.489586	25731.099518	31.161396
513.706800	25766.012485	31.166413
514.093541	25801.834178	31.171431
514.497855	25845.614346	31.176448
514.759544	25889.352073	31.181466
515.393049	25931.066210	31.186484
515.379914	25983.574511	31.191501
516.557084	26030.592410	31.196519
516.788642	26068.433935	31.201536
517.207279	26115.981787	31.206554
517.972668	26146.013110	31.211572
518.208104	26201.518387	31.216589
518.968764	26236.319975	31.221607
519.589820	26266.981108	31.226624
519.858699	26318.251257	31.231642
520.435183	26354.326478	31.236660
520.583347	26406.452836	31.241677
521.304495	26450.383802	31.246695
521.871301	26500.330654	31.251712
522.059300	26547.662494	31.256730
522.814691	26597.521530	31.261748
522.995125	26659.040206	31.266765
523.649886	26699.979847	31.271783
523.805151	26767.130544	31.276800
524.258791	26809.867164	31.281818
524.800401	26869.345629	31.286836
525.371596	26930.913937	31.291853
526.249942	26970.949617	31.296871
526.577124	27039.738372	31.301888
527.156986	27091.388174	31.306906
527.966593	27155.368715	31.311924
527.996866	27206.797836	31.316941
528.648678	27256.079773	31.321959
529.672160	27322.343974	31.326976
530.090977	27366.469430	31.331994
531.204212	27421.173547	31.337012
531.364843	27470.761636	31.342029
532.071960	27519.372683	31.347047
532.649664	27572.081052	31.352064
532.906714	27621.293938	31.357082
534.009320	27656.584191	31.362100
534.860605	27706.307469	31.367117
535.330919	27752.330725	31.372135
536.057276	27791.992913	31.377152
536.146265	27832.123817	31.382170
536.859756	27873.031244	31.387188
537.194925	27923.828250	31.392205
538.068716	27956.611330	31.397223
538.711143	28000.480440	31.402240
538.913627	28034.545520	31.407258
539.803032	28074.430495	31.412276
539.826153	28120.049480	31.417293
540.707605	28165.746874	31.422311
540.977105	28204.444832	31.427328
541.306152	28255.243822	31.432346
541.835738	28303.886549	31.437364
542.000140	28357.227470	31.442381
542.405235	28420.592125	31.447399
543.191516	28465.908617	31.452416
543.568536	28521.533455	31.457434
544.417130	28568.685387	31.462452
545.467613	28614.690293	31.467469
546.462992	28661.243936	31.472487
546.914723	28705.370479	31.477504
547.226244	28744.150991	31.482522
548.210733	28783.201562	31.487540
548.247578	28835.574527	31.492557
548.977713	28866.878348	31.497575
549.398541	28911.717219	31.502592
549.332354	28952.214034	31.507610
550.246964	29003.479520	31.512628
550.628790	29050.568303	31.517645
551.107880	29100.821137	31.522663
551.785985	29154.126509	31.527680
552.029639	29211.517168	31.532698
552.848834	29256.038381	31.537716
552.612809	29302.921267	31.542733
553.521458	29361.965565	31.547751
553.934780	29392.893876	31.552768
554.622968	29457.846362	31.557786
554.641530	29504.614947	31.562804
554.891505	29561.403114	31.567821
555.501390	29627.776328	31.572839
556.213111	29684.466132	31.577856
556.772000	29751.564455	31.582874
557.493368	29802.776037	31.587892
557.980584	29876.622592	31.592909
558.644710	29924.089612	31.597927
559.160050	29981.914079	31.602944
559.762967	30052.464119	31.607962
560.652447	30102.657988	31.612980
560.831832	30170.007078	31.617997
561.693697	30230.661674	31.623015
562.037633	30289.559937	31.628032
562.473600	30354.917304	31.633050
563.322724	30406.863496	31.638068
563.528010	30481.097000	31.643085
564.660550	30528.522577	31.648103
565.874065	30565.538772	31.653120
566.575463	30614.399180	31.658138
567.160070	30646.910367	31.663156
567.649244	30707.748395	31.668173
568.323285	30762.034265	31.673191
569.013772	30799.254548	31.678208
569.296770	30851.851371	31.683226
570.043872	30895.388539	31.688244
570.311258	30956.267409	31.693261
570.782942	31006.782500	31.698279
571.254811	31052.053781	31.703296
571.362978	31121.144220	31.708314
572.229711	31181.397423	31.713332
573.285414	31214.481405	31.718349
574.252676	31253.606614	31.723367
575.249656	31298.485274	31.728384
575.507229	31359.029554	31.733402
575.859393	31387.731312	31.738420
576.630236	31429.779737	31.743437
578.005933	31457.125270	31.748455
578.737529	31487.218760	31.753472
578.989143	31515.959511	31.758490
580.323386	31531.183185	31.763508
580.900164	31562.498362	31.768525
581.142304	31590.543491	31.773543
581.741823	31621.362771	31.778560
581.992104	31655.493208	31.783578
582.556417	31687.283970	31.788596
583.003990	31719.447569	31.793613
583.434023	31764.254330	31.798631
583.746412	31798.627155	31.803648
583.655076	31850.787417	31.808666
584.432701	31894.309365	31.813684
584.693504	31946.780610	31.818701
585.018204	31998.704990	31.823719
585.487892	32058.077356	31.828736
585.952561	32131.463796	31.833754
586.374726	32187.083271	31.838772
588.370265	32220.435908	31.843789
589.819089	32243.807349	31.848807
590.783978	32272.579194	31.853824
591.440640	32298.884250	31.858842
592.328621	32308.364131	31.863860
592.823520	32333.575928	31.868877
593.403220	32361.812351	31.873895
593.705535	32381.045116	31.878912
594.150321	32404.823306	31.883930
594.438530	32429.252304	31.888948
594.471876	32449.473281	31.893965
594.802061	32486.870552	31.898983
595.253108	32517.025008	31.904000
594.941269	32572.177505	31.909018
595.481348	32611.121071	31.914036
595.805033	32667.499942	31.919053
596.074386	32733.799399	31.924071
596.651883	32795.825878	31.929088
596.555580	32870.242550	31.934106
597.433250	32943.443860	31.939124
597.500284	33009.695895	31.944141
598.451329	33096.034776	31.949159
599.076281	33168.029375	31.954176
599.329042	33250.666722	31.959194
599.997616	33333.784479	31.964212
600.453581	33417.382868	31.969229
601.208381	33495.128837	31.974247
601.655338	33573.478497	31.979264
602.630850	33664.274983	31.984282
603.379045	33734.585221	31.989300
604.077902	33805.806451	31.994317
605.194570	33891.004572	31.999335
605.852008	33952.106649	32.004352
606.634753	34021.512905	32.009370
607.556592	34081.381817	32.014388
608.373024	34155.349335	32.019405
608.855793	34212.631305	32.024423
609.592499	34275.403340	32.029440
610.014056	34340.853527	32.034458
610.613429	34392.401609	32.039476
611.360217	34461.376889	32.044493
611.794604	34533.026782	32.049511
612.615096	34581.812078	32.054528
613.054351	34665.314932	32.059546
613.748601	34719.552748	32.064564
614.350434	34789.503267	32.069581
614.623551	34856.400116	32.074599
615.882860	34912.545508	32.079616
616.280924	34982.057232	32.084634
617.163383	35030.066580	32.089652
617.638656	35096.025014	32.094669
618.040341	35167.266288	32.099687
619.002117	35225.680675	32.104704
619.299118	35294.692816	32.109722
619.926907	35367.964483	32.114740
620.422387	35432.958232	32.119757
621.010327	35505.735278	32.124775
621.861640	35547.786389	32.129792
622.470226	35617.006820	32.134810
623.309627	35675.995290	32.139828
624.271512	35736.696269	32.144845
624.571067	35808.263171	32.149863
625.484251	35865.703026	32.154880
625.703854	35929.923805	32.159898
626.260624	35985.873601	32.164916
626.789031	36053.237477	32.169933
627.531121	36120.316794	32.174951
628.677669	36183.002197	32.179968
628.825632	36247.469551	32.184986
629.651397	36301.055923	32.190004
630.517898	36359.256258	32.195021
630.936517	36415.627998	32.200039
631.977917	36461.184554	32.205056
632.660485	36532.125779	32.210074
633.065414	36580.568889	32.215092
633.703891	36627.477325	32.220109
634.267090	36696.961929	32.225127
634.900097	36749.921997	32.230144
634.918845	36808.782156	32.235162
635.331932	36855.608671	32.240180
636.186961	36917.458134	32.245197
636.393416	36976.470732	32.250215
637.086392	37036.318050	32.255232
637.431983	37112.518990	32.260250
638.139259	37184.834798	32.265268
638.782170	37259.345728	32.270285
638.956304	37333.846422	32.275303
639.755385	37411.920756	32.280320
640.216890	37501.089136	32.285338
640.614671	37575.935603	32.290356
641.668400	37654.341146	32.295373
642.038732	37740.820847	32.300391
643.161138	37810.201082	32.305408
643.663346	37892.354309	32.310426
644.316999	37969.050588	32.315444
645.531186	38054.498407	32.320461
646.286808	38115.468878	32.325479
647.524809	38178.957212	32.330496
648.050113	38239.918995	32.335514
648.942168	38295.286811	32.340532
649.800202	38355.900186	32.345549
650.257615	38420.712115	32.350567
650.985240	38473.342695	32.355584
651.465458	38553.280382	32.360602
651.837616	38611.232274	32.365620
652.419095	38695.102570	32.370637
652.813528	38754.080246	32.375655
653.815704	38822.426861	32.380672
654.283664	38890.827708	32.385690
654.969142	38958.469839	32.390708
656.401599	39008.494398	32.395725
656.864717	39078.793859	32.400743
657.611079	39143.942327	32.405760
657.876110	39214.082643	32.410778
658.899678	39281.313137	32.415796
659.450576	39334.322769	32.420813
661.538622	39359.942801	32.425831
662.510516	39402.462651	32.430848
663.331828	39442.226585	32.435866
663.494443	39490.162097	32.440884
664.107160	39519.878440	32.445901
664.383365	39583.682876	32.450919
664.832701	39630.510504	32.455936
665.417989	39677.435634	32.460954
665.668523	39743.441949	32.465972
666.673016	39799.906822	32.470989
666.905179	39870.673823	32.476007
667.103279	39925.426279	32.481024
667.747035	40001.242525	32.486042
667.923953	40083.282821	32.491060
668.440308	40140.600038	32.496077
668.782842	40241.096489	32.501095
669.490651	40312.821647	32.506112
670.218643	40405.893324	32.511130
670.638910	40487.497256	32.516148
671.867130	40567.212196	32.521165
672.204428	40659.308257	32.526183
673.046062	40731.498984	32.531200
673.840423	40827.885967	32.536218
674.251816	40901.155840	32.541236
675.397406	40968.605864	32.546253
675.909957	41060.251801	32.551271
676.582220	41135.881722	32.556288
677.022484	41209.492131	32.561306
677.914215	41289.474419	32.566324
678.413846	41356.638487	32.571341
679.279138	41430.696956	32.576359
680.265648	41488.094995	32.581376
681.219791	41545.182885	32.586394
681.845762	41621.431782	32.591412
682.877257	41690.668168	32.596429
683.317247	41749.976214	32.601447
683.954170	41813.649544	32.606464
684.511125	41883.738919	32.611482
685.507636	41937.733366	32.616500
687.059345	41981.536251	32.621517
687.965279	42045.535096	32.626535
688.668678	42081.759943	32.631552
689.343996	42131.047359	32.636570
689.215104	42203.032423	32.641588
690.114891	42257.290117	32.646605
690.501439	42317.944322	32.651623
691.113511	42377.323675	32.656640
691.742635	42451.580137	32.661658
691.802433	42519.755962	32.666676
692.938091	42586.736802	32.671693
693.324123	42669.341075	32.676711
694.716848	42719.331822	32.681728
695.650847	42779.820870	32.686746
695.924832	42857.819242	32.691764
696.671599	42918.466115	32.696781
696.927657	42998.466592	32.701799
697.727803	43073.691680	32.706816
698.369962	43153.003577	32.711834
698.514532	43228.341284	32.716852
699.041140	43321.890427	32.721869
699.625988	43404.537565	32.726887
700.386945	43506.223063	32.731904
701.064443	43589.149268	32.736922
701.473253	43686.723332	32.741940
701.981050	43770.161592	32.746957
702.954501	43858.056957	32.751975
703.636571	43961.965058	32.756992
704.854852	44055.440925	32.762010
705.109612	44141.919264	32.767028
706.472486	44218.299572	32.772045
707.046156	44311.915312	32.777063
707.875149	44402.180067	32.782080
708.982491	44480.741498	32.787098
709.462812	44574.509817	32.792116
710.522933	44664.364874	32.797133
710.826860	44736.152045	32.802151
711.467345	44824.094586	32.807168
712.123483	44905.075619	32.812186
712.639143	45007.994075	32.817204
713.403000	45087.031869	32.822221
713.961231	45185.886692	32.827239
714.727829	45274.647172	32.832256
715.880963	45355.714988	32.837274
716.364842	45428.659045	32.842292
717.969679	45498.051195	32.847309
719.198017	45572.931030	32.852327
720.102558	45642.045259	32.857344
720.843832	45704.457745	32.862362
721.561115	45765.955520	32.867380
722.339132	45830.657993	32.872397
722.814261	45899.977081	32.877415
723.348524	45978.131504	32.882432
724.083139	46040.476735	32.887450
724.542649	46112.069633	32.892468
724.855375	46195.017359	32.897485
725.522677	46271.433062	32.902503
726.133927	46343.247953	32.907520
726.550140	46415.044969	32.912538
727.016268	46493.935976	32.917556
727.726942	46571.501463	32.922573
728.119927	46652.849460	32.927591
728.673010	46748.527005	32.932608
729.553817	46841.981142	32.937626
729.965782	46921.271339	32.942644
731.038870	47021.187126	32.947661
731.471800	47107.674720	32.952679
732.225780	47209.915043	32.957696
732.962647	47300.575263	32.962714
733.554149	47403.639411	32.967732
734.471457	47494.576926	32.972749
735.250762	47585.642000	32.977767
735.984528	47691.444207	32.982784
737.028053	47777.618729	32.987802
737.394701	47866.925132	32.992820
738.530888	47952.036577	32.997837
739.594414	48051.460378	33.002855
740.481847	48132.003083	33.007872
741.516921	48223.973022	33.012890
741.878064	48315.625773	33.017908
742.881793	48395.540759	33.022925
743.739169	48486.221345	33.027943
744.162287	48576.491247	33.032960
745.282062	48659.928411	33.037978
745.830729	48751.331041	33.042996
746.750532	48841.965049	33.048013
747.661416	48925.198020	33.053031
748.080222	49010.553281	33.058048
748.820280	49104.591399	33.063066
749.083008	49204.214130	33.068084
749.918359	49289.277240	33.073101
750.465118	49393.297546	33.078119
750.866004	49501.167387	33.083136
751.713556	49602.953316	33.088154
752.519203	49710.918216	33.093172
753.560741	49810.452696	33.098189
754.900520	49901.290444	33.103207
755.802728	49989.323933	33.108224
756.804921	50078.917289	33.113242
757.606584	50157.603459	33.118260
758.820840	50242.901619	33.123277
759.513479	50311.938446	33.128295
760.290095	50408.314135	33.133312
760.917151	50474.349225	33.138330
762.249832	50560.721975	33.143348
762.941946	50638.433356	33.148365
763.833984	50705.467565	33.153383
763.978194	50791.248997	33.158400
764.795145	50873.204652	33.163418
765.279488	50957.951202	33.168436
765.967714	51037.806352	33.173453
766.243876	51120.813039	33.178471
767.214807	51231.336422	33.183488
767.910966	51327.887973	33.188506
768.534495	51420.080474	33.193524
769.125465	51514.224562	33.198541
769.962608	51598.340461	33.203559
770.989124	51689.140693	33.208576
771.866464	51778.032977	33.213594
772.752512	51874.985309	33.218612
773.797418	51959.839015	33.223629
774.363300	52051.936683	33.228647
774.748389	52146.402292	33.233664
775.916523	52226.252152	33.238682
776.689133	52309.579505	33.243700
777.033587	52404.444801	33.248717
778.101865	52475.739224	33.253735
778.734271	52561.681170	33.258752
779.580915	52632.362235	33.263770
780.270925	52727.411809	33.268788
780.728356	52810.193432	33.273805
781.489234	52891.288723	33.278823
781.849978	52988.270607	33.283840
783.020801	53071.503518	33.288858
783.468676	53164.687417	33.293876
784.509148	53260.698584	33.298893
785.397420	53359.281618	33.303911
786.179173	53459.057974	33.308928
786.729002	53556.946343	33.313946
787.149696	53672.648250	33.318964
788.293562	53762.225572	33.323981
789.091443	53858.115661	33.328999
789.613006	53959.397231	33.334016
790.434552	54074.289419	33.339034
791.104359	54176.691088	33.344052
792.026409	54281.970447	33.349069
792.854494	54378.635201	33.354087
793.709708	54487.446030	33.359104
794.912129	54594.386461	33.364122
795.512027	54691.198037	33.369140
796.031459	54811.780660	33.374157
797.407460	54893.590862	33.379175
798.045879	55005.587116	33.384192
799.302991	55109.823272	33.389210
800.527613	55197.062184	33.394228
801.417646	55288.868476	33.399245
802.451817	55383.621008	33.404263
802.982364	55468.234057	33.409280
804.164687	55544.626135	33.414298
805.010730	55621.156470	33.419316
805.851259	55711.582830	33.424333
806.650304	55784.595764	33.429351
807.354349	55886.956374	33.434368
808.294296	55956.363817	33.439386
809.852076	56031.002017	33.444404
810.671815	56101.320872	33.449421
811.730415	56189.785973	33.454439
812.232460	56263.500809	33.459456
813.447566	56323.846832	33.464474
814.066969	56394.825550	33.469492
814.939671	56470.741801	33.474509
815.801481	56527.159834	33.479527
816.559195	56600.075203	33.484544
817.587745	56662.431063	33.489562
817.906156	56739.325003	33.494580
818.739810	56804.582496	33.499597
819.464967	56889.314628	33.504615
819.992407	56972.790841	33.509632
820.465545	57051.126329	33.514650
821.609916	57140.061669	33.519668
821.982733	57229.814263	33.524685
822.852414	57301.070621	33.529703
823.185991	57406.331529	33.534720
823.862047	57497.640075	33.539738
824.589544	57588.327528	33.544756
825.251909	57691.728042	33.549773
825.855491	57786.670908	33.554791
826.485723	57906.602984	33.559808
827.031512	57994.718844	33.564826
827.995729	58110.059355	33.569844
828.861382	58228.134270	33.574861
830.811239	58309.357712	33.579879
832.119653	58392.962990	33.584896
832.959264	58472.248008	33.589914
834.088701	58549.058508	33.594932
834.369842	58628.898170	33.599949
835.267372	58699.289086	33.604967
835.634771	58780.941409	33.609984
836.345392	58875.707338	33.615002
836.673683	58965.525630	33.620020
837.206557	59070.939119	33.625037
838.293985	59167.571402	33.630055
838.632516	59278.617565	33.635072
839.486177	59369.475378	33.640090
839.969711	59480.119387	33.645108
840.646695	59590.428536	33.650125
841.509419	59710.724586	33.655143
842.314297	59826.910315	33.660160
843.257129	59951.858655	33.665178
844.094223	60066.011676	33.670196
844.587921	60191.118198	33.675213
845.600710	60305.546768	33.680231
846.560027	60435.627305	33.685248
847.434918	60550.535196	33.690266
849.145606	60659.983358	33.695284
850.143868	60776.812368	33.700301
851.257596	60890.525925	33.705319
852.025440	60991.031095	33.710336
853.198505	61107.991000	33.715354
854.436031	61203.584163	33.720372
854.994290	61310.983354	33.725389
855.938754	61408.067181	33.730407
856.515771	61509.194381	33.735424
857.017883	61624.505182	33.740442
857.953468	61733.537872	33.745460
858.393660	61843.525611	33.750477
859.757948	61953.682916	33.755495
860.161959	62080.313894	33.760512
861.492787	62191.855943	33.765530
862.523264	62294.251747	33.770548
863.606164	62401.942504	33.775565
864.746566	62491.673152	33.780583
865.396868	62604.714655	33.785600
866.187235	62712.676823	33.790618
867.529826	62813.854051	33.795636
868.208801	62911.949842	33.800653
869.244782	63009.923637	33.805671
869.958654	63116.769165	33.810688
870.755741	63216.831601	33.815706
871.520723	63328.960456	33.820724
872.336250	63426.688372	33.825741
873.589204	63520.633645	33.830759
874.322532	63632.048791	33.835776
875.041204	63735.748784	33.840794
876.159649	63844.351433	33.845812
876.784213	63954.104917	33.850829
877.647933	64070.235407	33.855847
878.314984	64174.913326	33.860864
878.967120	64288.475766	33.865882
879.958117	64386.842836	33.870900
880.666028	64509.455792	33.875917
881.928876	64613.543966	33.880935
882.584663	64727.133484	33.885952
883.401217	64848.105780	33.890970
884.504113	64951.476253	33.895988
885.614703	65057.159668	33.901005
886.418464	65164.323233	33.906023
887.106236	65273.529532	33.911040
888.154226	65389.042569	33.916058
889.114029	65495.126212	33.921076
889.597652	65614.874901	33.926093
890.540234	65718.661413	33.931111
891.529344	65806.920628	33.936128
892.759815	65885.657380	33.941146
895.297519	65949.390615	33.946164
895.998045	66042.060810	33.951181
896.820708	66110.637266	33.956199
897.698144	66198.695404	33.961216
898.121980	66286.468842	33.966234
899.169622	66358.650228	33.971252
899.602449	66448.294160	33.976269
900.254931	66533.950741	33.981287
900.993827	66634.475492	33.986304
901.557936	66741.623690	33.991322
902.305258	66835.971307	33.996340
902.694433	66965.049568	34.001357
903.584252	67064.324823	34.006375
904.465504	67182.126124	34.011392
904.874330	67307.517354	34.016410
905.704179	67424.576190	34.021428
906.592318	67557.318075	34.026445
906.742868	67697.226352	34.031463
907.871405	67824.024899	34.036480
908.230274	67979.466302	34.041498
909.224731	68115.001221	34.046516
910.107256	68274.416938	34.051533
910.865353	68426.090334	34.056551
911.761988	68575.617409	34.061568
912.819909	68730.505712	34.066586
913.787902	68879.062029	34.071604
914.867330	69023.693405	34.076621
916.138103	69172.606181	34.081639
917.090494	69309.926100	34.086656
917.890204	69447.556774	34.091674
919.044649	69593.406214	34.096692
920.106543	69747.567789	34.101709
920.928029	69882.162608	34.106727
922.068125	70035.263655	34.111744
922.963160	70181.299266	34.116762
924.554397	70307.251756	34.121780
925.775475	70436.484931	34.126797
927.144604	70552.074050	34.131815
928.949908	70663.443339	34.136832
929.865180	70782.169485	34.141850
930.733594	70898.950150	34.146868
931.258400	71013.094715	34.151885
931.962298	71133.894009	34.156903
933.036883	71254.758931	34.161920
933.462985	71381.631962	34.166938
934.747423	71493.863463	34.171956
935.707366	71615.103549	34.176973
936.565557	71740.199621	34.181991
937.803760	71851.011524	34.187008
938.599449	71985.914683	34.192026
939.126053	72106.046914	34.197044
940.058296	72227.402536	34.202061
940.973860	72361.598855	34.207079
941.944485	72478.592437	34.212096
942.685701	72621.742191	34.217114
943.424873	72751.461293	34.222132
944.022108	72894.225683	34.227149
945.028132	73036.752423	34.232167
945.985647	73168.271728	34.237184
946.680876	73311.383060	34.242202
947.770593	73436.045749	34.247220
948.680846	73585.504197	34.252237
949.404909	73733.989024	34.257255
950.793955	73866.269392	34.262272
951.844424	74012.880576	34.267290
952.501842	74128.322313	34.272308
953.074447	74269.132933	34.277325
954.204046	74396.286267	34.282343
954.884890	74541.748052	34.287360
955.612916	74677.773229	34.292378
956.610182	74813.058874	34.297396
957.408354	74951.818931	34.302413
958.149484	75099.956004	34.307431
959.246488	75240.192508	34.312448
960.471346	75379.687679	34.317466
961.759471	75518.458546	34.322484
963.082762	75658.388200	34.327501
963.873919	75798.116109	34.332519
965.379874	75921.066760	34.337536
966.636106	76053.717558	34.342554
968.254314	76167.492595	34.347572
969.393472	76286.913627	34.352589
970.736139	76385.220530	34.357607
972.046797	76498.807962	34.362624
972.849777	76615.636396	34.367642
973.739202	76726.885075	34.372660
974.619063	76848.135818	34.377677
974.962167	76964.890601	34.382695
975.870315	77083.272666	34.387712
976.421555	77203.934719	34.392730
977.455990	77334.808340	34.397748
978.473629	77479.822427	34.402765
979.346250	77617.625400	34.407783
980.218042	77749.546816	34.412800
980.571397	77890.771085	34.417818
981.952189	78015.670691	34.422836
982.866685	78153.318209	34.427853
983.773823	78305.895910	34.432871
984.845452	78444.796891	34.437888
985.386418	78598.740403	34.442906
986.276364	78745.036341	34.447924
987.164426	78907.040112	34.452941
988.993616	79033.838262	34.457959
991.702518	79136.396516	34.462976
992.666530	79260.847189	34.467994
993.692880	79385.914457	34.473012
994.822143	79497.889890	34.478029
996.056084	79604.541130	34.483047
996.926097	79723.487499	34.488064
997.634769	79846.358025	34.493082
998.377390	79955.369778	34.498100
999.142620	80073.968475	34.503117
999.712347	80212.678979	34.508135
1000.904831	80346.795499	34.513152
1000.984124	80477.978774	34.518170
1001.659357	80619.027558	34.523188
1002.863008	80772.218008	34.528205
1003.574125	80919.449692	34.533223
1004.584395	81070.517006	34.538240
1005.503719	81240.560311	34.543258
1006.310353	81383.439308	34.548276
1007.170986	81540.373773	34.553293
1007.963181	81710.764324	34.558311
1008.949677	81864.415695	34.563328
1009.587640	82035.093639	34.568346
1010.931067	82195.881258	34.573364
1011.792563	82362.311060	34.578381
1012.814522	82518.959750	34.583399
1014.265179	82677.107393	34.588416
1015.243016	82852.214317	34.593434
1016.478357	83004.769146	34.598452
1017.856861	83159.154991	34.603469
1018.936413	83301.994333	34.608487
1019.834202	83462.890073	34.613504
1020.642832	83603.504877	34.618522
1021.171145	83747.362177	34.623540
1022.401600	83872.945312	34.628557
1023.466832	84036.006407	34.633575
1024.874567	84178.157678	34.638592
1025.289931	84335.944352	34.643610
1026.267461	84493.961505	34.648628
1027.570692	84644.889809	34.653645
1028.891808	84802.542017	34.658663
1029.569020	84954.683480	34.663680
1030.580832	85110.990764	34.668698
1031.374712	85270.188913	34.673716
1032.739843	85434.038946	34.678733
1033.258381	85594.303711	34.683751
1034.422376	85756.968178	34.688768
1035.821933	85906.604182	34.693786
1037.464628	86057.276495	34.698804
1038.981071	86202.434031	34.703821
1040.176734	86346.013149	34.708839
1041.019236	86483.501192	34.713856
1041.996356	86638.198211	34.718874
1043.413252	86787.767358	34.723892
1044.002069	86929.305604	34.728909
1045.084648	87087.759478	34.733927
1046.095413	87230.792511	34.738944
1047.165188	87389.877004	34.743962
1047.791082	87544.650906	34.748980
1048.843474	87700.696602	34.753997
1049.434417	87867.400470	34.759015
1051.013861	88032.207584	34.764032
1051.188080	88203.798676	34.769050
1052.495305	88371.887022	34.774068
1053.422474	88543.032893	34.779085
1054.410202	88720.093258	34.784103
1055.511163	88885.346398	34.789120
1056.039994	89085.242441	34.794138
1056.626176	89269.246175	34.799156
1057.832760	89460.584398	34.804173
1058.867198	89644.345774	34.809191
1059.859534	89842.753642	34.814208
1060.670419	90044.060148	34.819226
1061.645627	90240.569217	34.824244
1063.214382	90436.063738	34.829261
1063.805260	90636.373787	34.834279
1065.020860	90838.398237	34.839296
1066.523351	91039.408452	34.844314
1067.943258	91236.491084	34.849332
1069.897961	91407.645137	34.854349
1071.753253	91565.760015	34.859367
1072.978119	91730.227363	34.864384
1074.192547	91887.551939	34.869402
1075.194107	92056.881371	34.874420
1076.278488	92214.716993	34.879437
1077.326658	92386.382807	34.884455
1078.286126	92544.494465	34.889472
1079.056420	92709.866677	34.894490
1079.762168	92883.314393	34.899508
1081.005363	93044.129182	34.904525
1081.987878	93225.837660	34.909543
1083.368140	93390.347405	34.914560
1084.630797	93552.725707	34.919578
1086.094704	93697.215813	34.924596
1088.151149	93841.564154	34.929613
1089.147887	93996.811680	34.934631
1090.662040	94150.227333	34.939648
1091.926107	94281.638812	34.944666
1092.602880	94416.661477	34.949684
1093.917069	94551.363912	34.954701
1094.580882	94680.009685	34.959719
1095.255875	94816.946460	34.964736
1096.226455	94947.872141	34.969754
1096.957407	95094.669559	34.974772
1097.655602	95234.548239	34.979789
1098.499673	95393.532945	34.984807
1099.375913	95558.172444	34.989824
1100.571100	95709.460487	34.994842
1100.760858	95878.286281	34.999860
1102.293414	96037.895187	35.004877
1103.633850	96205.582761	35.009895
1104.705189	96369.992696	35.014912
1105.936639	96536.136989	35.019930
1107.312646	96693.079336	35.024948
1108.733621	96845.697854	35.029965
1109.813201	97008.040572	35.034983
1110.893791	97182.804642	35.040000
1112.126826	97336.900694	35.045018
1113.184463	97508.182704	35.050036
1114.762733	97663.350330	35.055053
1115.802416	97809.599720	35.060071
1117.467205	97958.614065	35.065088
1118.319892	98125.325523	35.070106
1119.304380	98280.677766	35.075124
1120.353824	98437.172401	35.080141
1120.946153	98606.095370	35.085159
1121.948803	98768.063358	35.090176
1123.260459	98935.748616	35.095194
1124.205978	99113.796260	35.100212
1125.776941	99278.237279	35.105229
1126.439841	99450.307019	35.110247
1127.100005	99632.957690	35.115264
1128.318838	99814.757244	35.120282
1129.209356	100001.785168	35.125300
1130.315528	100174.843573	35.130317
1132.114594	100344.711184	35.135335
1133.011801	100522.200533	35.140352
1134.108036	100712.327211	35.145370
1135.595329	100892.684324	35.150388
1136.674574	101073.344664	35.155405
1137.153602	101262.450805	35.160423
1138.625614	101437.280518	35.165440
1140.295032	101599.060869	35.170458
1141.220687	101789.534059	35.175476
1142.652364	101970.851371	35.180493
1143.378489	102155.490870	35.185511
1144.590576	102341.406069	35.190528
1145.786251	102527.249343	35.195546
1146.596203	102723.725856	35.200564
1147.586748	102910.486035	35.205581
1148.443329	103108.211439	35.210599
1149.358908	103316.161118	35.215616
1150.657732	103507.186545	35.220634
1151.146588	103713.544842	35.225652
1152.335141	103922.397548	35.230669
1153.582850	104148.719063	35.235687
1154.263998	104356.950195	35.240704
1155.656563	104566.217442	35.245722
1156.518382	104783.565871	35.250740
1157.712751	105006.940067	35.255757
1159.278052	105210.421258	35.260775
1160.949747	105406.186005	35.265792
1162.879787	105608.406575	35.270810
1163.890944	105805.297068	35.275828
1165.277958	105998.757687	35.280845
1167.298693	106172.546483	35.285863
1168.457125	106359.119655	35.290880
1169.675741	106524.481924	35.295898
1169.936846	106704.468272	35.300916
1171.881203	106855.108665	35.305933
1173.217010	107023.025735	35.310951
1174.166231	107191.134649	35.315968
1175.453178	107350.689712	35.320986
1176.377290	107538.057289	35.326004
1177.365341	107703.224444	35.331021
1178.036715	107879.705437	35.336039
1178.849043	108066.955917	35.341056
1180.173530	108251.234796	35.346074
1181.025473	108451.743122	35.351092
1181.877814	108647.236895	35.356109
1182.668664	108852.875640	35.361127
1183.404238	109063.059830	35.366144
1185.460311	109260.106366	35.371162
1186.732106	109452.572319	35.376180
1189.020820	109636.244671	35.381197
1190.741549	109824.281317	35.386215
1191.843027	110000.122098	35.391232
1193.426709	110184.485133	35.396250
1194.243609	110370.686709	35.401268
1195.437299	110548.086481	35.406285
1196.379514	110733.459019	35.411303
1197.253643	110923.328456	35.416320
1198.441458	111127.955774	35.421338
1199.243048	111333.459425	35.426356
1199.840702	111532.930493	35.431373
1201.287500	111747.286439	35.436391
1202.258150	111959.531446	35.441408
1203.690253	112163.631872	35.446426
1205.156689	112381.169203	35.451444
1206.592464	112571.868939	35.456461
1208.044006	112779.859884	35.461479
1208.823488	112992.334536	35.466496
1210.572687	113194.008243	35.471514
1211.542893	113408.468753	35.476532
1212.590387	113607.652076	35.481549
1213.831983	113827.733780	35.486567
1214.901763	114041.131098	35.491584
1216.071193	114246.417905	35.496602
1217.077072	114466.417028	35.501620
1218.329592	114686.807718	35.506637
1219.916257	114896.819086	35.511655
1221.313656	115101.820928	35.516672
1222.878124	115308.608306	35.521690
1224.984778	115499.318048	35.526708
1226.526177	115683.787925	35.531725
1228.100436	115874.373117	35.536743
1229.413097	116050.533855	35.541760
1231.858991	116213.482892	35.546778
1232.677292	116399.382377	35.551796
1233.694021	116570.793440	35.556813
1235.108234	116747.815892	35.561831
1235.620614	116918.134359	35.566848
1236.756856	117101.426259	35.571866
1237.539064	117292.646456	35.576884
1238.598886	117473.672715	35.581901
1239.950254	117660.594311	35.586919
1240.785752	117850.339578	35.591936
1242.200900	118044.158662	35.596954
1243.337832	118246.945546	35.601972
1244.517706	118440.806318	35.606989
1245.850195	118631.285227	35.612007
1246.760412	118824.344329	35.617024
1248.048477	119026.921540	35.622042
1249.139062	119224.857179	35.627060
1250.115700	119421.039058	35.632077
1250.740466	119608.119092	35.637095
1251.768490	119818.170465	35.642112
1252.921516	120027.645058	35.647130
1253.817407	120232.145760	35.652148
1254.704790	120447.255685	35.657165
1255.968050	120662.634313	35.662183
1256.998936	120894.944968	35.667200
1257.999548	121117.327470	35.672218
1259.358869	121344.214177	35.677236
1260.447075	121582.755508	35.682253
1262.310977	121799.550825	35.687271
1263.434873	122041.587536	35.692288
1264.507656	122263.535808	35.697306
1265.593021	122511.386824	35.702324
1266.948433	122746.877055	35.707341
1268.287658	122982.866075	35.712359
1269.465075	123228.566038	35.717376
1270.521822	123473.071401	35.722394
1271.603033	123716.510140	35.727412
1272.963810	123962.654607	35.732429
1274.479120	124213.654756	35.737447
1275.758546	124463.187954	35.742464
1277.112426	124718.274625	35.747482
1278.065647	124972.707487	35.752500
1279.691752	125233.697366	35.757517
1281.008969	125486.603980	35.762535
1282.166418	125750.654419	35.767552
1284.031531	125992.523888	35.772570
1285.714214	126247.353369	35.777588
1287.272656	126485.602034	35.782605
1288.845967	126720.085740	35.787623
1289.973704	126963.859604	35.792640
1291.038120	127204.819428	35.797658
1292.394061	127457.964012	35.802676
1293.638880	127710.786872	35.807693
1294.750321	127950.274403	35.812711
1295.839195	128206.473378	35.817728
1297.358452	128461.183451	35.822746
1298.909423	128711.339888	35.827764
1300.084684	128953.853959	35.832781
1302.118020	129194.351611	35.837799
1302.737548	129454.403298	35.842816
1304.004804	129705.742861	35.847834
1305.074623	129967.917016	35.852852
1306.295695	130234.124574	35.857869
1307.801305	130490.894205	35.862887
1308.572373	130753.390613	35.867904
1309.787749	131021.215600	35.872922
1311.487518	131279.201680	35.877940
1312.918276	131535.941460	35.882957
1314.638020	131796.235529	35.887975
1315.344851	132073.001948	35.892992
1317.192274	132327.904236	35.898010
1318.542351	132582.383953	35.903028
1319.967268	132847.616051	35.908045
1321.775210	133080.409463	35.913063
1323.106675	133342.035466	35.918080
1324.872182	133583.650195	35.923098
1325.991862	133829.024920	35.928116
1327.541003	134075.052888	35.933133
1328.873867	134309.277716	35.938151
1329.916392	134561.503965	35.943168
1330.681185	134812.966839	35.948186
1332.100603	135069.977406	35.953204
1333.137180	135323.148658	35.958221
1334.562040	135581.886524	35.963239
1335.680036	135849.057583	35.968256
1337.069102	136090.905366	35.973274
1339.305229	136314.382958	35.978292
1341.319492	136521.061888	35.983309
1343.505219	136732.125791	35.988327
1345.046907	136942.372304	35.993344
1346.334545	137150.519578	35.998362
1347.818967	137352.955433	36.003380
1348.697387	137567.258964	36.008397
1349.787339	137779.348009	36.013415
1351.132409	137986.895043	36.018432
1351.885730	138207.119126	36.023450
1352.932216	138434.472429	36.028468
1354.046735	138669.030467	36.033485
1355.614595	138892.610725	36.038503
1356.947771	139119.325153	36.043520
1358.048374	139350.010306	36.048538
1359.485367	139587.209260	36.053556
1360.608678	139833.185499	36.058573
1362.185038	140071.772149	36.063591
1363.221913	140313.138055	36.068608
1364.394685	140565.489313	36.073626
1365.641803	140812.314274	36.078644
1366.519087	141083.991991	36.083661
1368.120004	141348.856675	36.088679
1369.259399	141600.181247	36.093696
1370.589177	141852.351014	36.098714
1372.252979	142115.068124	36.103732
1373.475085	142385.912649	36.108749
1374.399738	142654.196371	36.113767
1375.827529	142935.016114	36.118784
1376.960255	143211.829140	36.123802
1378.012698	143512.218978	36.128820
1379.092428	143803.628608	36.133837
1380.786132	144094.139904	36.138855
1382.614585	144370.542280	36.143872
1383.940989	144665.012319	36.148890
1385.570347	144956.327576	36.153908
1386.964579	145238.426604	36.158925
1388.551042	145521.409059	36.163943
1390.237201	145805.429802	36.168960
1391.420077	146093.531051	36.173978
1393.253534	146373.334120	36.178996
1394.545597	146665.036193	36.184013
1395.615550	146938.096515	36.189031
1397.249594	147228.224529	36.194048
1398.677283	147510.107444	36.199066
1400.735535	147781.310745	36.204084
1401.725029	148063.105705	36.209101
1403.590093	148336.602650	36.214119
1404.904417	148612.044639	36.219136
1406.751644	148888.300801	36.224154
1408.395156	149155.055192	36.229172
1409.758089	149437.382123	36.234189
1411.200367	149700.546434	36.239207
1412.641856	149965.894253	36.244224
1413.810064	150234.713776	36.249242
1415.374425	150499.829386	36.254260
1416.641234	150769.105670	36.259277
1417.871685	151040.241717	36.264295
1419.083139	151313.171262	36.269312
1420.557372	151598.755697	36.274330
1422.471757	151867.894368	36.279348
1423.594426	152148.683291	36.284365
1424.778547	152422.931782	36.289383
1426.152020	152690.796064	36.294400
1427.404551	152970.542060	36.299418
1429.115872	153255.084810	36.304436
1430.497910	153523.194467	36.309453
1432.580533	153783.059026	36.314471
1433.547554	154049.592153	36.319488
1435.304015	154295.028384	36.324506
1436.639229	154553.931144	36.329524
1437.940482	154813.450124	36.334541
1438.969626	155076.339401	36.339559
1440.271970	155331.079396	36.344576
1441.239013	155604.764785	36.349594
1442.475018	155878.204510	36.354612
1443.800414	156174.426794	36.359629
1445.136927	156450.441602	36.364647
1446.258930	156738.545104	36.369664
1447.537985	157033.512913	36.374682
1449.102449	157314.075389	36.379700
1450.963492	157611.094826	36.384717
1452.371563	157911.401084	36.389735
1453.802361	158200.250393	36.394752
1455.143092	158497.210389	36.399770
1456.904949	158797.286948	36.404788
1457.986440	159105.572342	36.409805
1459.839149	159392.165437	36.414823
1462.348086	159669.187670	36.419840
1464.035882	159959.529190	36.424858
1466.092141	160227.305667	36.429876
1467.690871	160495.108995	36.434893
1469.391786	160763.671002	36.439911
1470.844546	161048.350097	36.444928
1472.178033	161317.890053	36.449946
1473.849066	161582.440540	36.454964
1475.072030	161864.651270	36.459981
1476.560110	162140.641291	36.464999
1477.724487	162406.524311	36.470016
1478.886740	162706.081506	36.475034
1480.555326	162983.087456	36.480052
1481.354396	163280.437870	36.485069
1482.583699	163564.358994	36.490087
1484.004408	163859.199723	36.495104
1485.582461	164166.348889	36.500122
1487.191325	164460.452029	36.505140
1488.427144	164768.791444	36.510157
1490.158052	165062.903818	36.515175
1491.943573	165364.292102	36.520192
1493.262915	165672.015041	36.525210
1495.371132	165955.057518	36.530228
1497.422960	166237.108790	36.535245
1499.472835	166521.636440	36.540263
1501.430731	166786.260194	36.545280
1503.055449	167068.793626	36.550298
1504.590095	167341.129401	36.555316
1506.411732	167610.576976	36.560333
1507.730837	167878.701034	36.565351
1509.330339	168139.382574	36.570368
1510.478595	168410.393135	36.575386
1511.948836	168672.596492	36.580404
1513.294025	168953.576636	36.585421
1514.937255	169213.203925	36.590439
1516.230505	169497.393721	36.595456
1517.375157	169788.436799	36.600474
1518.616974	170056.243938	36.605492
1520.298577	170328.256090	36.610509
1521.189310	170617.722257	36.615527
1522.659632	170913.946568	36.620544
1523.682016	171221.249052	36.625562
1524.923101	171528.136608	36.630580
1526.263064	171835.999600	36.635597
1527.215240	172154.956520	36.640615
1528.338493	172471.323837	36.645632
1529.831727	172813.215343	36.650650
1531.312709	173122.725765	36.655668
1532.518397	173440.799065	36.660685
1533.726768	173757.008542	36.665703
1535.271506	174083.570565	36.670720
1536.693963	174410.916512	36.675738
1538.160631	174724.665612	36.680756
1539.373929	175071.023282	36.685773
1540.635564	175403.478896	36.690791
1542.310133	175754.054450	36.695808
1543.953171	176094.434131	36.700826
1545.638612	176423.843992	36.705844
1547.028713	176780.959172	36.710861
1548.273409	177139.167090	36.715879
1549.765043	177489.607571	36.720896
1551.040769	177856.445627	36.725914
1552.453884	178223.910845	36.730932
1553.874353	178597.456823	36.735949
1555.323969	178988.350366	36.740967
1557.058603	179358.879959	36.745984
1558.499221	179730.730163	36.751002
1560.728414	180098.340090	36.756020
1562.322326	180487.456893	36.761037
1563.892341	180868.355992	36.766055
1566.115666	181232.091067	36.771072
1568.224759	181590.212164	36.776090
1570.950279	181936.239090	36.781108
1572.802666	182272.398577	36.786125
1574.372906	182630.006775	36.791143
1576.169367	182972.450109	36.796160
1577.118877	183329.924705	36.801178
1579.200911	183672.820163	36.806196
1581.137565	184013.101745	36.811213
1582.508532	184374.105456	36.816231
1583.998921	184719.529943	36.821248
1585.594450	185072.148919	36.826266
1587.191244	185397.860124	36.831284
1589.056593	185748.014245	36.836301
1590.427228	186095.942360	36.841319
1592.428698	186428.193085	36.846336
1594.134265	186771.182841	36.851354
1595.502057	187113.139007	36.856372
1597.580363	187455.994946	36.861389
1599.377588	187792.057555	36.866407
1601.003303	188132.301469	36.871424
1602.846413	188461.378722	36.876442
1604.967015	188763.855879	36.881460
1607.172185	189080.563391	36.886477
1608.804304	189395.298457	36.891495
1610.919831	189688.565256	36.896512
1612.631512	189991.852799	36.901530
1614.514466	190296.560661	36.906548
1615.947766	190597.383951	36.911565
1616.943818	190902.927423	36.916583
1619.395941	191175.999567	36.921600
1621.360565	191462.571977	36.926618
1623.853141	191729.381466	36.931636
1626.168463	191981.597172	36.936653
1627.919089	192246.208776	36.941671
1629.407645	192507.272322	36.946688
1630.591240	192781.260152	36.951706
1631.765222	193048.268563	36.956724
1632.984205	193320.513702	36.961741
1633.948863	193603.021713	36.966759
1635.145380	193881.468211	36.971776
1636.087889	194183.634559	36.976794
1637.260348	194492.556191	36.981812
1638.520233	194800.957020	36.986829
1639.558892	195130.978140	36.991847
1640.928263	195449.926499	36.996864
1642.038468	195770.595199	37.001882
1643.044455	196100.347390	37.006900
1644.017653	196422.159222	37.011917
1645.091899	196781.916002	37.016935
1646.513680	197119.640775	37.021952
1647.048205	197482.728249	37.026970
1648.788772	197866.870727	37.031988
1649.684972	198249.873070	37.037005
1650.964934	198646.931979	37.042023
1652.584180	199053.103570	37.047040
1653.927782	199466.153817	37.052058
1655.294557	199886.071384	37.057076
1656.897325	200316.363386	37.062093
1658.352060	200747.837949	37.067111
1660.315835	201175.472613	37.072128
1662.276002	201612.848736	37.077146
1664.205877	202045.090406	37.082164
1666.042414	202469.008383	37.087181
1667.908426	202910.217012	37.092199
1669.735182	203338.788705	37.097216
1671.884689	203765.608001	37.102234
1673.434125	204202.305929	37.107252
1675.504069	204629.270326	37.112269
1677.305531	205072.089631	37.117287
1679.026073	205493.999847	37.122304
1681.182468	205925.147281	37.127322
1683.219242	206338.845332	37.132340
1686.119168	206743.158767	37.137357
1687.713405	207150.154016	37.142375
1689.690604	207566.369820	37.147392
1691.213582	207968.594078	37.152410
1692.894263	208387.580591	37.157428
1694.533640	208799.998661	37.162445
1695.781707	209208.420355	37.167463
1697.582575	209627.621860	37.172480
1699.352867	210038.716539	37.177498
1700.780327	210458.428530	37.182516
1703.194686	210866.474557	37.187533
1705.095445	211278.366315	37.192551
1706.793730	211687.830147	37.197568
1708.464968	212100.728928	37.202586
1710.019209	212517.712514	37.207604
1711.811500	212932.042742	37.212621
1713.614716	213337.636547	37.217639
1715.860778	213743.107990	37.222656
1717.870559	214152.810933	37.227674
1719.601551	214541.380609	37.232692
1721.472253	214941.484558	37.237709
1723.367813	215342.068656	37.242727
1725.478538	215737.615477	37.247744
1727.081042	216132.410050	37.252762
1728.616263	216526.430069	37.257780
1730.389016	216926.888784	37.262797
1731.767610	217327.135086	37.267815
1733.544250	217721.602473	37.272832
1734.934791	218118.192663	37.277850
1736.880156	218541.741642	37.282868
1738.740898	218986.641066	37.287885
1740.189624	219390.769900	37.292903
1741.980311	219802.387017	37.297920
1743.792869	220188.806615	37.302938
1745.542960	220593.525102	37.307956
1747.694385	220986.901501	37.312973
1749.189766	221394.890870	37.317991
1750.788126	221788.031635	37.323008
1753.067313	222180.324391	37.328026
1755.354923	222550.468988	37.333044
1758.423140	222900.038978	37.338061
1760.135488	223268.401703	37.343079
1761.876288	223607.195897	37.348096
1763.409190	223950.013260	37.353114
1764.664176	224300.929362	37.358132
1766.219513	224653.803301	37.363149
1767.990103	225006.058413	37.368167
1769.666751	225353.986742	37.373184
1771.118633	225707.719090	37.378202
1772.785819	226072.135566	37.383220
1774.407725	226430.083590	37.388237
1775.922304	226805.144707	37.393255
1777.194424	227178.596088	37.398272
1778.846775	227567.454310	37.403290
1780.125761	227948.857049	37.408308
1781.996647	228346.419076	37.413325
1783.378146	228748.457666	37.418343
1784.854576	229149.643489	37.423360
1786.521510	229574.269121	37.428378
1788.050824	229992.314651	37.433396
1789.705918	230421.466123	37.438413
1791.335496	230841.910592	37.443431
1794.001987	231259.009315	37.448448
1796.753202	231668.551062	37.453466
1798.428876	232082.488734	37.458484
1800.195538	232494.227945	37.463501
1802.239616	232909.630852	37.468519
1804.276614	233323.257931	37.473536
1806.180981	233730.075085	37.478554
1808.301765	234129.922799	37.483572
1810.810980	234514.821838	37.488589
1812.868365	234921.260932	37.493607
1814.569458	235323.441756	37.498624
1816.297168	235718.608237	37.503642
1817.637493	236121.866730	37.508660
1819.471470	236518.033432	37.513677
1821.078318	236937.811518	37.518695
1822.118384	237357.100219	37.523712
1823.885584	237774.846838	37.528730
1825.397186	238213.694959	37.533748
1826.998083	238639.370985	37.538765
1828.822063	239069.634119	37.543783
1831.384060	239489.564183	37.548800
1833.526091	239915.762805	37.553818
1835.046028	240355.782562	37.558836
1837.327876	240781.578659	37.563853
1838.768982	241218.031438	37.568871
1840.566089	241663.012051	37.573888
1842.027269	242098.802663	37.578906
1843.848094	242544.390619	37.583924
1845.863533	242965.916316	37.588941
1847.841454	243403.249315	37.593959
1849.695494	243857.623308	37.598976
1851.298326	244304.037839	37.603994
1853.100650	244752.579245	37.609012
1855.026584	245202.650423	37.614029
1856.247894	245670.392338	37.619047
1857.857255	246121.076172	37.624064
1860.238955	246585.731236	37.629082
1861.499309	247055.653317	37.634100
1863.121630	247511.010988	37.639117
1864.947134	247995.777569	37.644135
1866.600325	248476.102394	37.649152
1868.322361	248950.624502	37.654170
1870.308429	249435.264612	37.659188
1872.438978	249924.631687	37.664205
1873.841076	250424.636851	37.669223
1875.715646	250896.468396	37.674240
1878.039622	251375.338781	37.679258
1880.041751	251836.582309	37.684276
1882.608707	252271.033876	37.689293
1885.632887	252689.355170	37.694311
1887.656033	253123.109906	37.699328
1889.912395	253538.815378	37.704346
1891.944545	253973.305800	37.709364
1894.037396	254373.187170	37.714381
1896.088680	254794.033278	37.719399
1897.911669	255213.672620	37.724416
1900.068570	255614.407563	37.729434
1901.666796	256038.657010	37.734452
1903.431993	256443.597819	37.739469
1905.149998	256882.612345	37.744487
1906.620794	257307.391265	37.749504
1908.247383	257731.331527	37.754522
1909.529677	258177.836196	37.759540
1911.038003	258625.675217	37.764557
1913.247367	259073.982369	37.769575
1914.849148	259536.438189	37.774592
1917.148402	259990.420724	37.779610
1918.685895	260454.106440	37.784628
1920.550012	260928.229504	37.789645
1922.184488	261386.818284	37.794663
1924.069518	261873.334409	37.799680
1925.898527	262344.643081	37.804698
1927.401492	262835.362844	37.809716
1929.242731	263319.700913	37.814733
1930.875510	263830.924451	37.819751
1932.427559	264336.267492	37.824768
1934.666291	264834.256508	37.829786
1936.365182	265355.476866	37.834804
1937.972072	265879.734996	37.839821
1939.743720	266419.181809	37.844839
1941.676220	266951.158318	37.849856
1943.296420	267474.650567	37.854874
1945.477058	268019.337113	37.859892
1947.660049	268552.921484	37.864909
1950.189468	269091.604575	37.869927
1952.254299	269605.900879	37.874944
1954.969515	270117.675453	37.879962
1958.166424	270623.399822	37.884980
1961.188049	271115.282547	37.889997
1964.274267	271593.868183	37.895015
1966.094242	272068.522223	37.900032
1968.434446	272534.071383	37.905050
1970.545020	273013.299077	37.910068
1972.410956	273477.401132	37.915085
1974.280034	273947.522296	37.920103
1975.735115	274412.833934	37.925120
1977.519973	274884.059689	37.930138
1978.913466	275371.175112	37.935156
1980.205813	275863.183578	37.940173
1982.279231	276350.031972	37.945191
1983.973473	276858.686499	37.950208
1985.616746	277358.330534	37.955226
1987.328708	277862.255012	37.960244
1988.960442	278376.860466	37.965261
1990.886076	278886.360953	37.970279
1992.406433	279406.773931	37.975296
1994.899183	279922.731530	37.980314
1996.496495	280447.142478	37.985332
1998.115703	280987.119606	37.990349
2000.155652	281517.169593	37.995367
2002.000403	282060.840201	38.000384
2003.933610	282590.168008	38.005402
2005.610154	283148.113309	38.010420
2007.387117	283696.692414	38.015437
2009.381919	284235.657313	38.020455
2011.401809	284790.136358	38.025472
2013.179124	285314.629536	38.030490
2015.109981	285842.753230	38.035508
2016.828816	286393.796411	38.040525
2018.611168	286933.955462	38.045543
2020.675349	287489.001432	38.050560
2022.199346	288042.483670	38.055578
2023.524633	288615.174009	38.060596
2025.597544	289178.924162	38.065613
2027.860000	289754.324680	38.070631
2029.298776	290349.798261	38.075648
2031.430598	290936.899272	38.080666
2033.825793	291522.379138	38.085684
2036.081749	292109.047703	38.090701
2038.432562	292695.392943	38.095719
2040.684952	293295.416592	38.100736
2043.585022	293867.669912	38.105754
2045.732832	294441.467379	38.110772
2047.797986	295025.562326	38.115789
2050.137629	295617.736468	38.120807
2051.841136	296197.465743	38.125824
2054.805862	296760.829394	38.130842
2057.728830	297319.345859	38.135860
2059.830642	297881.627376	38.140877
2062.660667	298439.772293	38.145895
2064.743787	299004.870020	38.150912
2066.479528	299548.484543	38.155930
2068.741326	300105.444497	38.160948
2070.822702	300664.920175	38.165965
2073.502172	301206.134233	38.170983
2076.059602	301748.381355	38.176000
2078.624693	302272.541169	38.181018
2080.676835	302819.792912	38.186036
2082.306626	303358.476363	38.191053
2084.546348	303885.093655	38.196071
2086.400026	304428.787668	38.201088
2088.273494	304963.713252	38.206106
2090.328471	305514.325950	38.211124
2092.199415	306067.708453	38.216141
2094.046526	306608.418670	38.221159
2096.063015	307163.725491	38.226176
2098.070161	307719.411136	38.231194
2099.915972	308280.402087	38.236212
2102.394975	308828.789768	38.241229
2104.665469	309376.446429	38.246247
2106.989964	309945.650886	38.251264
2108.861935	310501.949407	38.256282
2110.913156	311068.905508	38.261300
2112.230152	311629.300315	38.266317
2114.523659	312204.664373	38.271335
2116.236495	312783.396115	38.276352
2118.087831	313375.686268	38.281370
2119.977586	313962.353329	38.286388
2121.603826	314550.811532	38.291405
2123.822658	315152.650735	38.296423
2125.574805	315771.854966	38.301440
2127.536399	316378.144924	38.306458
2129.323190	317007.108946	38.311476
2130.878127	317626.735886	38.316493
2133.255084	318250.537825	38.321511
2135.330736	318887.206960	38.326528
2137.655368	319529.846733	38.331546
2139.644591	320168.854126	38.336564
2142.005821	320795.047324	38.341581
2145.197778	321402.967756	38.346599
2147.682745	322031.515379	38.351616
2149.926020	322646.208252	38.356634
2152.498898	323244.540024	38.361652
2154.384354	323836.683232	38.366669
2156.969274	324405.168603	38.371687
2158.929648	324991.524938	38.376704
2160.901552	325570.967865	38.381722
2163.070166	326152.987793	38.386740
2165.469333	326708.153257	38.391757
2168.457769	327277.002040	38.396775
2171.229732	327828.210887	38.401792
2173.298530	328384.760999	38.406810
2175.970205	328934.808216	38.411828
2178.398888	329481.564673	38.416845
2180.603848	330025.179557	38.421863
2182.827535	330583.739246	38.426880
2184.534014	331140.043486	38.431898
2185.902127	331690.635480	38.436916
2187.980397	332273.040614	38.441933
2190.688843	332838.478839	38.446951
2193.023083	333388.386254	38.451968
2195.293983	333954.977011	38.456986
2197.252357	334533.468583	38.462004
2199.229398	335112.839320	38.467021
2201.776524	335684.087746	38.472039
2203.979440	336252.873938	38.477056
2206.431922	336828.847175	38.482074
2209.150487	337382.228974	38.487092
2211.359382	337947.467327	38.492109
2213.621970	338506.877761	38.497127
2215.896325	339084.835236	38.502144
2217.571043	339662.961572	38.507162
2219.849227	340250.423669	38.512180
2221.547599	340842.619838	38.517197
2223.544649	341425.291996	38.522215
2225.169611	342033.654394	38.527232
2226.864350	342646.185599	38.532250
2229.274511	343262.702340	38.537268
2231.037797	343882.287857	38.542285
2233.506603	344503.905859	38.547303
2236.042717	345105.479711	38.552320
2238.527304	345728.398781	38.557338
2240.948253	346349.264372	38.562356
2243.705817	346958.873769	38.567373
2246.497386	347573.189928	38.572391
2248.438244	348196.571911	38.577408
2250.135017	348817.803268	38.582426
2252.321457	349438.285190	38.587444
2254.207243	350079.541595	38.592461
2256.139993	350714.411389	38.597479
2258.526065	351362.697362	38.602496
2260.441632	352014.959621	38.607514
2263.010151	352664.464934	38.612532
2264.797420	353314.267507	38.617549
2267.030512	353968.325591	38.622567
2269.189050	354633.119499	38.627584
2271.004131	355311.636595	38.632602
2273.509195	355984.598526	38.637620
2275.128450	356666.653135	38.642637
2277.653941	357345.197269	38.647655
2279.326463	358030.950439	38.652672
2280.981177	358735.952566	38.657690
2283.373332	359430.722442	38.662708
2285.241321	360141.551077	38.667725
2287.673847	360850.370844	38.672743
2289.779362	361578.539004	38.677760
2291.982032	362293.739038	38.682778
2294.684165	363004.251495	38.687796
2296.824193	363729.507357	38.692813
2298.913620	364463.662372	38.697831
2301.253667	365193.195653	38.702848
2303.048848	365902.561944	38.707866
2305.426907	366607.962688	38.712884
2307.535776	367318.214465	38.717901
2309.686484	368031.337594	38.722919
2312.022981	368736.755891	38.727936
2314.421258	369463.406482	38.732954
2316.926884	370183.531591	38.737972
2318.813199	370905.063969	38.742989
2321.264476	371637.724538	38.748007
2323.785214	372362.343976	38.753024
2326.550843	373090.940855	38.758042
2329.401582	373810.632000	38.763060
2331.810000	374548.616669	38.768077
2334.353229	375264.550165	38.773095
2337.160565	375971.396917	38.778112
2339.897608	376701.774956	38.783130
2341.966776	377426.871899	38.788148
2344.184806	378151.370960	38.793165
2346.802792	378875.661604	38.798183
2349.026514	379607.203640	38.803200
2350.785661	380337.538825	38.808218
2353.194837	381067.674377	38.813236
2355.392859	381824.072436	38.818253
2357.596165	382556.491320	38.823271
2359.946364	383315.289431	38.828288
2362.524753	384072.029128	38.833306
2365.552029	384806.492293	38.838324
2368.089162	385554.000716	38.843341
2370.533134	386298.769049	38.848359
2373.638391	387026.272528	38.853376
2376.231032	387762.134088	38.858394
2379.183874	388491.276903	38.863412
2381.108519	389240.168709	38.868429
2383.225463	389973.876937	38.873447
2385.772932	390707.521860	38.878464
2387.648232	391461.691419	38.883482
2390.065327	392199.783594	38.888500
2392.279677	392951.654965	38.893517
2394.375180	393707.760214	38.898535
2396.506573	394480.644870	38.903552
2398.516667	395239.767180	38.908570
2400.980053	396013.469615	38.913588
2403.559845	396793.899380	38.918605
2406.331667	397554.762347	38.923623
2409.188844	398320.178408	38.928640
2411.175008	399105.814669	38.933658
2413.387238	399870.840435	38.938676
2416.672106	400642.408892	38.943693
2419.343208	401399.310328	38.948711
2422.217892	402154.485545	38.953728
2424.317250	402922.818309	38.958746
2427.143135	403683.079100	38.963764
2429.479290	404442.994928	38.968781
2431.650825	405204.209440	38.973799
2434.073958	405964.981363	38.978816
2436.539727	406743.358435	38.983834
2438.776248	407502.522603	38.988852
2441.093640	408272.064385	38.993869
2443.417557	409042.799248	38.998887
2445.997099	409821.120115	39.003904
2448.360369	410586.636515	39.008922
2450.923715	411345.410554	39.013940
2453.902831	412122.078415	39.018957
2456.360506	412883.789534	39.023975
2459.118110	413638.007701	39.028992
2461.624484	414405.796101	39.034010
2464.459309	415143.798874	39.039028
2466.736398	415896.334302	39.044045
2469.322882	416624.787901	39.049063
2471.581354	417348.134179	39.054080
2473.644769	418078.962913	39.059098
2475.983996	418796.252930	39.064116
2478.171858	419524.664374	39.069133
2480.358113	420265.614753	39.074151
2482.927105	421002.656401	39.079168
2484.795048	421745.033684	39.084186
2487.657193	422487.097651	39.089204
2490.125854	423236.344446	39.094221
2492.222882	423993.022881	39.099239
2495.096759	424734.561483	39.104256
2497.822128	425490.836422	39.109274
2500.056857	426234.359212	39.114292
2502.477447	427017.724916	39.119309
2504.390643	427802.667967	39.124327
2506.951763	428580.694086	39.129344
2508.660107	429367.847242	39.134362
2511.484083	430165.420568	39.139380
2513.859489	430970.887572	39.144397
2516.251094	431779.108404	39.149415
2518.606588	432579.866433	39.154432
2520.993308	433414.909690	39.159450
2523.535693	434231.372178	39.164468
2526.906117	435044.378893	39.169485
2529.624380	435867.991840	39.174503
2531.929785	436683.242318	39.179520
2533.968421	437527.151474	39.184538
2536.749485	438346.615701	39.189556
2539.732217	439185.802749	39.194573
2542.239639	440031.463468	39.199591
2544.814569	440871.211409	39.204608
2547.032748	441709.114533	39.209626
2549.563912	442555.333030	39.214644
2552.072852	443413.412243	39.219661
2554.135575	444277.906275	39.224679
2556.756116	445130.941574	39.229696
2558.890484	446002.437801	39.234714
2561.662862	446881.735252	39.239732
2564.250881	447752.984423	39.244749
2567.057918	448636.200309	39.249767
2570.425130	449500.926452	39.254784
2572.631578	450379.819383	39.259802
2575.271878	451247.578455	39.264820
2578.151140	452123.707864	39.269837
2580.989070	452988.125432	39.274855
2583.984739	453846.817233	39.279872
2586.596989	454719.796779	39.284890
2590.308834	455574.859679	39.289908
2593.283486	456419.643568	39.294925
2596.154762	457255.258145	39.299943
2599.072795	458088.555523	39.304960
2601.797678	458929.332961	39.309978
2604.473002	459753.653352	39.314996
2607.367300	460578.257546	39.320013
2609.798777	461408.111018	39.325031
2612.707990	462230.723564	39.330048
2615.136181	463047.214969	39.335066
2618.415539	463845.538088	39.340084
2621.346488	464658.846904	39.345101
2623.638929	465472.834106	39.350119
2626.045574	466282.371680	39.355136
2628.516866	467092.319669	39.360154
2631.124789	467895.641805	39.365172
2633.519930	468706.595947	39.370189
2635.715966	469516.285573	39.375207
2638.191617	470338.071723	39.380224
2640.579926	471150.489770	39.385242
2643.000459	471957.461778	39.390260
2645.797437	472752.161567	39.395277
2648.331642	473542.779306	39.400295
2650.904439	474322.041660	39.405312
2653.690598	475104.014521	39.410330
2656.285018	475889.926237	39.415348
2659.273376	476682.053249	39.420365
2661.315060	477484.050996	39.425383
2663.917606	478281.072477	39.430400
2666.016618	479101.778292	39.435418
2668.172308	479920.215841	39.440436
2670.568079	480746.000228	39.445453
2672.880178	481596.251706	39.450471
2675.547245	482446.101485	39.455488
2677.782278	483311.685558	39.460506
2680.103977	484177.768892	39.465524
2682.333267	485056.396734	39.470541
2684.452526	485958.525051	39.475559
2687.353557	486829.229917	39.480576
2690.656368	487730.264288	39.485594
2692.831368	488635.123855	39.490612
2695.758273	489551.925979	39.495629
2698.008633	490470.608788	39.500647
2701.407943	491386.478987	39.505664
2704.172686	492322.238739	39.510682
2706.428717	493264.036914	39.515700
2709.628603	494185.241231	39.520717
2711.767089	495130.992941	39.525735
2714.244509	496077.392813	39.530752
2717.081126	497039.370918	39.535770
2719.680082	497993.614783	39.540788
2722.885853	498943.062997	39.545805
2725.640384	499907.160526	39.550823
2728.869667	500863.557665	39.555840
2732.036483	501823.339749	39.560858
2735.172451	502769.756474	39.565876
2738.037965	503718.332075	39.570893
2740.763872	504672.876895	39.575911
2743.598553	505618.523407	39.580928
2746.429095	506578.486106	39.585946
2749.390430	507520.874597	39.590964
2752.254266	508464.182088	39.595981
2755.840824	509400.155855	39.600999
2759.149657	510337.431515	39.606016
2761.728308	511281.174693	39.611034
2764.450300	512212.035215	39.616052
2767.089675	513138.772078	39.621069
2769.678677	514096.458215	39.626087
2772.548531	515022.541994	39.631104
2775.380753	515965.962764	39.636122
2777.772662	516915.194107	39.641140
2780.894960	517846.107313	39.646157
2783.210842	518805.967814	39.651175
2785.809843	519743.151156	39.656192
2788.546667	520705.392885	39.661210
2791.023221	521663.788672	39.666228
2793.783140	522631.798926	39.671245
2796.710957	523593.121455	39.676263
2799.482950	524554.710821	39.681280
2802.556264	525518.555938	39.686298
2804.879724	526490.923374	39.691316
2807.327248	527463.257397	39.696333
2810.436285	528432.850569	39.701351
2812.683160	529422.259553	39.706368
2815.585623	530405.100048	39.711386
2817.721217	531404.765544	39.716404
2820.419443	532395.662026	39.721421
2823.349662	533388.516661	39.726439
2826.597031	534344.458896	39.731456
2829.947439	535285.524605	39.736474
2832.946010	536223.366436	39.741492
2836.135535	537158.800807	39.746509
2838.871467	538088.915486	39.751527
2842.082573	539023.369105	39.756544
2844.526443	539973.082495	39.761562
2847.318072	540918.147101	39.766580
2850.211695	541863.232330	39.771597
2852.490038	542818.064198	39.776615
2854.997980	543779.181077	39.781632
2857.897672	544746.353430	39.786650
2860.638272	545716.049904	39.791668
2864.094804	546668.311657	39.796685
2867.041517	547655.992325	39.801703
2869.659433	548634.958190	39.806720
2872.328375	549613.695125	39.811738
2875.085933	550615.825156	39.816756
2878.204881	551598.618900	39.821773
2880.817276	552591.981320	39.826791
2883.464121	553605.520970	39.831808
2886.505982	554602.736049	39.836826
2889.026636	555613.833793	39.841844
2892.160652	556637.819129	39.846861
2894.551718	557667.526830	39.851879
2897.137677	558713.150251	39.856896
2900.216522	559743.035653	39.861914
2903.004413	560803.934298	39.866932
2905.289714	561855.939756	39.871949
2907.954835	562942.655629	39.876967
2910.861733	564014.425503	39.881984
2913.455710	565095.047677	39.887002
2915.965823	566188.749952	39.892020
2919.471473	567288.923241	39.897037
2922.601860	568377.366681	39.902055
2926.037528	569463.257651	39.907072
2929.855352	570547.637872	39.912090
2932.583913	571638.631043	39.917108
2936.309192	572707.332740	39.922125
2939.564153	573796.145906	39.927143
2942.243888	574877.734195	39.932160
2945.203416	575956.573913	39.937178
2948.139473	577046.211707	39.942196
2951.326075	578132.100796	39.947213
2954.056047	579232.216676	39.952231
2957.001851	580311.132628	39.957248
2960.206910	581404.004545	39.962266
2962.490005	582502.247576	39.967284
2965.523056	583594.902587	39.972301
2968.517032	584691.928695	39.977319
2971.396003	585803.364068	39.982336
2974.313101	586906.870699	39.987354
2976.603103	588035.694053	39.992372
2979.795075	589152.383435	39.997389
2982.497248	590276.216498	40.002407
2985.462047	591399.198781	40.007424
2988.420856	592525.834126	40.012442
2991.018832	593675.820083	40.017460
2994.261512	594814.415628	40.022477
2997.472394	595958.065847	40.027495
3000.174795	597105.545394	40.032512
3003.480606	598251.910960	40.037530
3005.638786	599410.272046	40.042548
3008.797948	600551.427173	40.047565
3011.459181	601717.435908	40.052583
3014.211705	602891.221470	40.057600
3016.912423	604070.752311	40.062618
3019.912579	605235.046037	40.067636
3022.588228	606385.110898	40.072653
3025.496077	607531.417761	40.077671
3028.575472	608680.031924	40.082688
3031.924244	609800.466214	40.087706
3035.199066	610955.670188	40.092724
3038.422918	612084.801719	40.097741
3042.205061	613204.023235	40.102759
3045.450775	614357.529195	40.107776
3049.250256	615475.168388	40.112794
3051.934194	616600.929220	40.117812
3055.247896	617724.970828	40.122829
3058.369906	618843.579774	40.127847
3061.426927	619982.379566	40.132864
3064.245019	621113.452640	40.137882
3066.765650	622273.743090	40.142900
3069.603987	623418.565519	40.147917
3072.609938	624578.877862	40.152935
3075.336964	625754.948339	40.157952
3078.925517	626912.713621	40.162970
3082.056473	628077.521709	40.167988
3085.177146	629262.580882	40.173005
3088.181893	630440.235773	40.178023
3091.314585	631614.792190	40.183040
3094.570700	632794.089953	40.188058
3098.182255	633962.363459	40.193076
3101.377753	635140.708054	40.198093
3105.285304	636320.199119	40.203111
3108.424657	637501.878982	40.208128
3112.039953	638653.006866	40.213146
3115.275359	639829.963557	40.218164
3118.840724	640990.966551	40.223181
3121.978079	642151.759094	40.228199
3125.004132	643297.126154	40.233216
3128.323890	644463.261339	40.238234
3131.467838	645638.167447	40.243252
3134.864103	646783.329036	40.248269
3137.869955	647953.900031	40.253287
3141.062767	649127.693345	40.258304
3144.011531	650278.562016	40.263322
3146.919338	651461.648142	40.268340
3150.131033	652632.883188	40.273357
3153.368621	653812.196547	40.278375
3156.227821	654998.954251	40.283392
3159.515597	656189.034788	40.288410
3162.303954	657391.554897	40.293428
3165.259057	658570.344478	40.298445
3168.475622	659768.417704	40.303463
3170.935082	660970.252330	40.308480
3174.334147	662178.801754	40.313498
3177.072039	663408.812038	40.318516
3179.850027	664630.247697	40.323533
3183.163312	665863.979464	40.328551
3185.253206	667116.114173	40.333568
3188.367636	668356.423029	40.338586
3191.498733	669626.611691	40.343604
3194.450319	670891.536850	40.348621
3198.540907	672144.865364	40.353639
3202.143179	673414.515968	40.358656
3205.629266	674659.802196	40.363674
3209.429506	675896.767873	40.368692
3212.326628	677162.794500	40.373709
3215.783062	678413.696940	40.378727
3218.600551	679680.784133	40.383744
3221.832133	680927.159679	40.388762
3224.649304	682201.451602	40.393780
3227.848015	683473.119078	40.398797
3231.205461	684735.594417	40.403815
3233.954590	685979.473925	40.408832
3237.439845	687223.408679	40.413850
3240.542993	688450.506343	40.418868
3243.343062	689682.648979	40.423885
3246.709710	690900.533960	40.428903
3249.409904	692137.665951	40.433920
3252.681236	693372.547518	40.438938
3255.767652	694623.608945	40.443956
3258.656987	695880.280066	40.448973
3262.650416	697119.976439	40.453991
3265.885099	698389.722417	40.459008
3269.378662	699628.552863	40.464026
3272.652565	700892.872893	40.469044
3275.960262	702148.132169	40.474061
3279.374823	703414.888198	40.479079
3282.526914	704686.308942	40.484096
3285.918024	705956.611438	40.489114
3289.316242	707241.685175	40.494132
3292.629494	708530.542941	40.499149
3296.176099	709790.743404	40.504167
3298.953874	711100.249417	40.509184
3302.291415	712394.708795	40.514202
3304.885359	713709.635081	40.519220
3307.989300	715024.025120	40.524237
3311.248132	716355.354865	40.529255
3314.446084	717694.350050	40.534272
3317.281475	719037.741895	40.539290
3320.513701	720387.924413	40.544308
3323.349315	721764.755276	40.549325
3326.907967	723131.151792	40.554343
3330.009675	724521.768611	40.559360
3333.194132	725906.057572	40.564378
3336.299089	727303.073369	40.569396
3339.568044	728701.651528	40.574413
3343.150483	730109.274453	40.579431
3346.566797	731531.201906	40.584448
3349.982927	732948.336424	40.589466
3353.024311	734368.345120	40.594484
3356.214090	735811.625621	40.599501
3359.907922	737236.942722	40.604519
3363.383451	738686.517710	40.609536
3367.475297	740113.968616	40.614554
3371.864030	741535.341945	40.619572
3375.170040	742946.971728	40.624589
3379.209777	744356.797256	40.629607
3383.309856	745776.417419	40.634624
3387.091804	747168.474422	40.639642
3391.247556	748555.933359	40.644660
3395.254123	749921.241228	40.649677
3399.051353	751296.196707	40.654695
3402.761595	752663.927014	40.659712
3405.517951	754023.888948	40.664730
3408.960645	755389.799477	40.669748
3411.772540	756748.628586	40.674765
3415.231595	758121.629807	40.679783
3418.497058	759494.365876	40.684800
3421.428636	760873.994204	40.689818
3425.084811	762238.885305	40.694836
3427.966922	763637.301720	40.699853
3431.042118	765018.114780	40.704871
3434.473149	766401.121962	40.709888
3437.740797	767802.285896	40.714906
3441.297610	769193.553522	40.719924
3444.484814	770598.184373	40.724941
3448.347284	771989.956906	40.729959
3451.576971	773389.185186	40.734976
3455.165165	774784.354933	40.739994
3458.779140	776183.330199	40.745012
3461.983757	777573.237580	40.750016
3465.018644	778905.322485	40.755021
3467.874377	780209.491030	40.760026
3471.294994	781443.524052	40.765031
3473.954359	782616.480400	40.770036
3477.183163	783716.661608	40.775040
3480.543118	784751.647206	40.780045
3483.290111	785731.961915	40.785050
3485.984485	786622.386590	40.790055
3488.778125	787454.043759	40.795060
3491.012044	788214.038434	40.800064
3493.950723	788899.334200	40.805069
3495.601395	789532.099636	40.810074
3497.876928	790119.992561	40.815079
3499.960630	790640.853400	40.820084
3501.356472	791090.848632	40.825088
3503.103221	791504.600995	40.830093
3504.373100	791871.790464	40.835098
3505.395435	792201.375475	40.840103
3506.814098	792463.832872	40.845108
3508.007617	792708.046178	40.850112
3509.204717	792895.178220	40.855117
3510.062840	793052.745260	40.860122
3510.941935	793191.298359	40.865127
3512.174598	793279.449664	40.870132
3512.786100	793343.391833	40.875136
3513.588144	793379.602658	40.880141
3514.283860	793387.247603	40.885146
3515.016941	793369.347985	40.890151
3515.584270	793331.486903	40.895156
3516.045317	793271.198556	40.900160
3516.726351	793182.387475	40.905165
3517.282524	793078.370464	40.910170
3517.784621	792965.372781	40.915175
3518.446613	792823.663082	40.920180
3518.679886	792673.867922	40.925184
3519.043027	792497.033025	40.930189
3519.262137	792318.007102	40.935194
3519.610846	792126.085518	40.940199
3520.213827	791908.965997	40.945204
3520.013038	791691.481369	40.950208
3520.001895	791459.073632	40.955213
3520.440907	791231.054440	40.960218
3520.460214	790985.214317	40.965223
3520.261281	790733.849931	40.970228
3520.157983	790482.460801	40.975232
3520.897609	790222.472359	40.980237
3520.982693	789964.941061	40.985242
3520.743379	789680.575547	40.990247
3521.109109	789406.614592	40.995252
3521.020720	789131.980965	41.000256
3521.372177	788845.960954	41.005261
3521.314380	788553.755529	41.010266
3521.203196	788254.469606	41.015271
3521.041631	787951.394854	41.020276
3520.737447	787654.130696	41.025280
3521.034300	787349.135909	41.030285
3520.834151	787057.433213	41.035290
3520.836879	786749.069562	41.040295
3520.963955	786447.210362	41.045300
3520.724978	786139.450221	41.050304
3520.682894	785833.905848	41.055309
3520.558944	785520.937760	41.060314
3520.663773	785222.373813	41.065319
3520.542254	784911.935452	41.070324
3520.241199	784603.726084	41.075328
3520.061906	784291.549318	41.080333
3520.225207	783983.531597	41.085338
3519.757526	783675.654097	41.090343
3520.076648	783369.944908	41.095348
3519.714973	783068.565000	41.100352
3519.880730	782752.575521	41.105357
3519.928668	782455.184635	41.110362
3519.968222	782149.568149	41.115367
3520.084654	781831.136077	41.120372
3519.522629	781531.151466	41.125376
3519.547334	781210.099841	41.130381
3519.336726	780903.192765	41.135386
3519.244773	780601.271484	41.140391
3519.477368	780295.200158	41.145396
3519.220854	779998.004320	41.150400
3519.052409	779690.005484	41.155405
3519.112205	779383.481305	41.160410
3518.727814	779070.423316	41.165415
3518.708817	778774.712793	41.170420
3518.331818	778486.431600	41.175424
3518.793736	778177.575364	41.180429
3518.479048	777884.485950	41.185434
3518.161443	777592.221957	41.190439
3518.158948	777291.132490	41.195444
3517.848711	777016.810498	41.200448
3517.872527	776714.117642	41.205453
3517.871163	776424.068176	41.210458
3517.585714	776134.103353	41.215463
3517.630136	775849.241928	41.220468
3517.415103	775559.193410	41.225472
3517.455914	775278.495273	41.230477
3517.483715	775002.466155	41.235482
3517.445383	774715.456995	41.240487
3517.254074	774424.128557	41.245492
3517.095731	774154.795189	41.250496
3517.207379	773869.451657	41.255501
3516.723906	773599.609924	41.260506
3516.689964	773319.686327	41.265511
3516.612912	773040.005448	41.270516
3516.419051	772767.918242	41.275520
3515.876555	772513.610401	41.280525
3515.965890	772245.397475	41.285530
3515.919425	771975.620949	41.290535
3515.713481	771715.959276	41.295540
3515.808909	771464.022059	41.300544
3515.976639	771189.846337	41.305549
3515.775721	770934.343752	41.310554
3515.823393	770677.263966	41.315559
3515.741418	770410.934091	41.320564
3515.617869	770165.738641	41.325568
3515.383588	769901.928413	41.330573
3515.249211	769647.306540	41.335578
3515.046010	769391.997427	41.340583
3515.111855	769136.487230	41.345588
3514.582844	768907.874369	41.350592
3514.831863	768656.703214	41.355597
3514.698102	768408.346630	41.360602
3514.258658	768166.981296	41.365607
3514.736469	767918.063714	41.370612
3514.156536	767686.168812	41.375616
3514.253507	767439.417500	41.380621
3514.352403	767212.965309	41.385626
3513.926921	766968.108455	41.390631
3513.895676	766734.466611	41.395636
3513.819679	766504.867030	41.400640
3514.080107	766275.648461	41.405645
3513.621887	766049.006508	41.410650
3513.614385	765811.437309	41.415655
3513.640127	765583.665976	41.420660
3513.190461	765363.361639	41.425664
3513.242545	765141.784606	41.430669
3513.556528	764918.727881	41.435674
3513.285905	764698.226462	41.440679
3512.966312	764478.022495	41.445684
3513.128628	764260.444459	41.450688
3512.792621	764039.934479	41.455693
3512.674501	763827.074777	41.460698
3512.451426	763610.725090	41.465703
3512.555184	763398.161765	41.470708
3512.176999	763195.782003	41.475712
3512.546826	762971.819803	41.480717
3512.518074	762770.702450	41.485722
3512.307217	762571.484007	41.490727
3512.431086	762362.784448	41.495732
3512.197016	762153.940964	41.500736
3512.023249	761952.480459	41.505741
3511.892318	761748.245225	41.510746
3511.453716	761544.548579	41.515751
3511.407745	761355.136236	41.520756
3511.041597	761168.534531	41.525760
3511.275629	760974.725338	41.530765
3511.026697	760782.520294	41.535770
3510.942294	760585.941801	41.540775
3510.991806	760406.850001	41.545780
3510.844384	760233.164143	41.550784
3510.826500	760036.511048	41.555789
3510.936820	759871.556352	41.560794
3510.682128	759689.389529	41.565799
3510.667017	759503.576856	41.570804
3510.387181	759342.178310	41.575808
3510.599578	759144.526525	41.580813
3510.615766	758973.745357	41.585818
3510.214549	758800.068599	41.590823
3510.249781	758631.497130	41.595828
3510.114090	758475.681838	41.600832
3510.235940	758306.990164	41.605837
3510.060943	758129.312799	41.610842
3509.855960	757959.137575	41.615847
3510.150373	757785.668141	41.620852
3509.818887	757623.402629	41.625856
3509.828196	757456.832889	41.630861
3509.814475	757301.615003	41.635866
3509.585227	757136.163487	41.640871
3510.042746	756967.337312	41.645876
3509.648518	756815.775495	41.650880
3509.609526	756654.378824	41.655885
3510.071771	756492.451669	41.660890
3509.593663	756324.111403	41.665895
3509.800171	756147.805644	41.670900
3509.397754	755998.845176	41.675904
3509.532902	755845.646351	41.680909
3509.452984	755696.231777	41.685914
3509.055141	755536.746686	41.690919
3508.937470	755381.753787	41.695924
3508.888830	755227.783081	41.700928
3508.596660	755076.910433	41.705933
3508.638137	754934.520766	41.710938
3508.658577	754795.884150	41.715943
3508.821144	754651.494363	41.720948
3508.431928	754507.390533	41.725952
3508.702029	754366.828725	41.730957
3508.568687	754233.292881	41.735962
3508.296777	754089.655567	41.740967
3508.542389	753933.882101	41.745972
3508.477358	753806.055252	41.750976
3508.743576	753659.605198	41.755981
3508.296867	753525.121252	41.760986
3507.914070	753389.933064	41.765991
3508.280327	753250.816364	41.770996
3508.384785	753112.728055	41.776000
3507.887969	752976.020586	41.781005
3508.042018	752844.536592	41.786010
3507.935370	752725.488983	41.791015
3507.624410	752581.187938	41.796020
3507.835917	752458.774801	41.801024
3507.792814	752318.326090	41.806029
3507.940990	752196.067409	41.811034
3507.547807	752077.600409	41.816039
3507.788617	751943.814832	41.821044
3507.562089	751836.379855	41.826048
3507.476020	751696.618389	41.831053
3507.677827	751575.822758	41.836058
3507.274787	751455.619116	41.841063
3507.400353	751328.707517	41.846068
3507.097979	751217.176790	41.851072
3507.258381	751090.453100	41.856077
3507.663131	750981.617644	41.861082
3507.223338	750862.497554	41.866087
3507.391305	750729.542736	41.871092
3506.987088	750614.068347	41.876096
3507.083850	750491.889997	41.881101
3506.948555	750382.246176	41.886106
3506.905736	750271.449315	41.891111
3507.071230	750151.724257	41.896116
3506.848822	750037.396847	41.901120
3506.799317	749937.711716	41.906125
3507.011075	749809.031875	41.911130
3506.845932	749709.955764	41.916135
3506.531859	749600.132805	41.921140
3506.482065	749494.019419	41.926144
3506.579926	749383.581865	41.931149
3506.736026	749268.933549	41.936154
3506.405588	749177.041915	41.941159
3506.422921	749057.176230	41.946164
3505.953813	748966.787263	41.951168
3505.995642	748862.774681	41.956173
3506.040873	748762.762349	41.961178
3505.990280	748673.881932	41.966183
3506.108701	748573.163320	41.971188
3505.890695	748478.329585	41.976192
3505.960454	748374.503504	41.981197
3505.758365	748293.154448	41.986202
3505.654710	748207.835202	41.991207
3505.925841	748097.746057	41.996212
3505.590547	748012.561777	42.001216
3505.768081	747915.135666	42.006221
3506.108720	747835.421677	42.011226
3505.910377	747739.241460	42.016231
3505.944147	747643.515869	42.021236
3505.556508	747552.306325	42.026240
3505.650217	747459.928970	42.031245
3505.747717	747365.078957	42.036250
3505.675925	747283.796665	42.041255
3505.532116	747198.176482	42.046260
3505.703741	747107.412933	42.051264
3505.650483	747012.435284	42.056269
3505.363997	746924.908260	42.061274
3505.476132	746847.445911	42.066279
3505.341985	746753.071539	42.071284
3505.282858	746666.986731	42.076288
3504.986885	746586.969808	42.081293
3505.418621	746500.011267	42.086298
3505.055463	746428.603641	42.091303
3505.260757	746338.814093	42.096308
3505.047424	746271.235441	42.101312
3505.032355	746186.077144	42.106317
3504.982714	746102.950130	42.111322
3505.091100	746025.282547	42.116327
3505.209290	745948.452846	42.121332
3505.034231	745862.773763	42.126336
3505.327190	745786.309016	42.131341
3505.241976	745704.765372	42.136346
3504.885993	745628.702900	42.141351
3504.817617	745548.786030	42.146356
3504.657409	745473.628874	42.151360
3504.612257	745402.011030	42.156365
3504.621793	745322.078973	42.161370
3504.680266	745254.644351	42.166375
3505.031999	745185.578847	42.171380
3504.828160	745115.714749	42.176384
3504.721546	745037.825741	42.181389
3504.836169	744959.207323	42.186394
3504.638053	744893.097278	42.191399
3504.759655	744819.271440	42.196404
3504.735726	744755.059407	42.201408
3504.792889	744674.569093	42.206413
3504.876063	744599.462209	42.211418
3504.596794	744522.585341	42.216423
3504.702154	744453.751860	42.221428
3504.789146	744377.109666	42.226432
3504.716235	744297.526860	42.231437
3504.993517	744224.213524	42.236442
3504.424248	744167.898103	42.241447
3504.789549	744088.735157	42.246452
3504.499624	744021.792473	42.251456
3504.586801	743953.699216	42.256461
3504.348309	743873.892280	42.261466
3503.930870	743815.423284	42.266471
3504.352584	743744.949201	42.271476
3504.347656	743688.240432	42.276480
3504.196719	743625.523414	42.281485
3504.318581	743554.899412	42.286490
3504.213380	743489.256623	42.291495
3504.342910	743429.903281	42.296500
3504.345403	743365.873306	42.301504
3504.334813	743292.895528	42.306509
3504.090981	743231.970725	42.311514
3504.080715	743187.274319	42.316519
3504.401823	743111.965576	42.321524
3504.078736	743060.941660	42.326528
3504.126041	742995.714568	42.331533
3504.062474	742934.015976	42.336538
3503.843700	742873.380938	42.341543
3504.133391	742813.304226	42.346548
3504.667330	742755.560192	42.351552
3503.990557	742694.406087	42.356557
3503.950932	742619.646737	42.361562
3503.548334	742566.160320	42.366567
3504.215281	742509.925430	42.371572
3504.089741	742455.156241	42.376576
3503.867969	742390.562006	42.381581
3503.674345	742331.055993	42.386586
3503.680930	742293.522054	42.391591
3503.703847	742229.281669	42.396596
3503.563918	742165.908347	42.401600
3503.808461	742122.251731	42.406605
3503.582446	742062.452334	42.411610
3503.562184	742017.206974	42.416615
3503.648783	741960.124480	42.421620
3503.817207	741914.748447	42.426624
3503.553474	741844.420113	42.431629
3503.520358	741801.648319	42.436634
3503.483648	741755.167831	42.441639
3503.548667	741703.972090	42.446644
3503.399354	741656.124903	42.451648
3503.209510	741610.509600	42.456653
3503.398674	741565.424865	42.461658
3503.402617	741526.008415	42.466663
3503.595196	741464.305462	42.471668
3503.391701	741432.835771	42.476672
3503.272480	741374.052093	42.481677
3503.203602	741320.403170	42.486682
3503.387639	741281.450309	42.491687
3503.468758	741234.304346	42.496692
3502.960425	741184.090219	42.501696
3503.385479	741139.607028	42.506701
3503.739801	741089.497037	42.511706
3503.215781	741040.817798	42.516711
3503.219939	740992.248812	42.521716
3503.525954	740949.614205	42.526720
3503.442579	740902.889125	42.531725
3503.608027	740846.329619	42.536730
3502.958584	740806.226200	42.541735
3503.454947	740765.191327	42.546740
3502.995812	740718.576714	42.551744
3502.977993	740677.477974	42.556749
3503.145384	740628.434636	42.561754
3502.688025	740596.459495	42.566759
3503.158099	740550.135490	42.571764
3502.955081	740509.115943	42.576768
3503.018937	740473.740228	42.581773
3503.375155	740422.389155	42.586778
3503.087355	740393.105605	42.591783
3503.096293	740341.217844	42.596788
3502.821493	740297.142359	42.601792
3502.809847	740240.805651	42.606797
3503.088901	740212.862205	42.611802
3502.950012	740177.667065	42.616807
3503.059954	740134.912090	42.621812
3502.778467	740099.987490	42.626816
3502.779930	740066.945099	42.631821
3502.872812	740026.170943	42.636826
3502.808362	739993.930579	42.641831
3502.698781	739953.238971	42.646836
3502.594330	739923.082474	42.651840
3502.484983	739881.054887	42.656845
3502.910683	739852.591283	42.661850
3502.592429	739822.370803	42.666855
3502.758109	739786.381603	42.671860
3502.873309	739749.064983	42.676864
3502.560806	739720.920764	42.681869
3502.872417	739667.840846	42.686874
3502.776507	739650.246544	42.691879
3502.593394	739595.417607	42.696884
3502.713782	739575.412951	42.701888
3502.544160	739533.492420	42.706893
3502.773792	739503.922207	42.711898
3502.515016	739477.746972	42.716903
3502.584404	739432.026815	42.721908
3502.697027	739401.881935	42.726912
3502.885240	739367.717462	42.731917
3502.698047	739334.109570	42.736922
3502.496219	739301.097588	42.741927
3502.848842	739262.057487	42.746932
3502.577054	739230.095633	42.751936
3502.327623	739196.299564	42.756941
3502.485528	739165.552665	42.761946
3502.022839	739132.830441	42.766951
3502.643041	739109.476968	42.771956
3502.437397	739085.517836	42.776960
3502.586528	739058.581222	42.781965
3502.899221	739020.535954	42.786970
3502.616821	738989.613781	42.791975
3502.502113	738953.419789	42.796980
3502.438276	738922.213878	42.801985
3502.308241	738894.531292	42.806989
3502.661753	738862.316211	42.811994
3502.495787	738840.031836	42.816999
3502.512108	738802.133445	42.822004
3502.461161	738777.554151	42.827009
3502.150151	738747.476798	42.832013
3502.229034	738721.045379	42.837018
3502.031530	738685.408054	42.842023
3502.473062	738664.012260	42.847028
3502.243520	738628.528394	42.852033
3502.325866	738606.004434	42.857037
3502.359343	738570.229476	42.862042
3502.650349	738560.138334	42.867047
3502.440568	738514.656936	42.872052
3502.132806	738488.486536	42.877057
3502.282220	738461.448906	42.882061
3502.396591	738439.117081	42.887066
3502.253244	738412.968738	42.892071
3502.245247	738393.279177	42.897076
3502.334200	738387.228686	42.902081
3502.120099	738344.369208	42.907085
3502.242679	738322.678880	42.912090
3501.973804	738282.054515	42.917095
3502.054770	738266.852233	42.922100
3501.814444	738236.266507	42.927105
3501.859742	738220.179462	42.932109
3502.265373	738200.866358	42.937114
3501.718879	738177.752437	42.942119
3501.994021	738154.750055	42.947124
3501.786521	738136.873984	42.952129
3501.501986	738113.766064	42.957133
3502.050533	738100.564222	42.962138
3502.198574	738089.011806	42.967143
3502.042038	738056.036647	42.972148
3501.934932	738034.482446	42.977153
3501.962503	738020.080154	42.982157
3502.028122	737998.052015	42.987162
3502.056322	737977.464850	42.992167
3502.133567	737952.861827	42.997172
3502.185120	737922.721441	43.002177
3501.873233	737903.130366	43.007181
3502.175413	737891.799583	43.012186
3502.045295	737871.436220	43.017191
3502.082915	737845.404542	43.022196
3501.955004	737820.389707	43.027201
3501.597879	737803.626143	43.032205
3502.406572	737771.925187	43.037210
3501.756668	737766.540591	43.042215
3502.003531	737741.265659	43.047220
3501.875025	737707.344323	43.052225
3501.717195	737698.563249	43.057229
3502.071040	737672.379793	43.062234
3501.948998	737658.743765	43.067239
3501.810835	737635.857668	43.072244
3501.969621	737617.177705	43.077249
3501.711180	737601.288045	43.082253
3502.104761	737585.191645	43.087258
3501.555571	737565.836874	43.092263
3501.770421	737562.585325	43.097268
3501.878497	737533.770096	43.102273
3501.625373	737518.324714	43.107277
3502.072108	737492.966489	43.112282
3501.843887	737477.714836	43.117287
3501.703252	737453.344202	43.122292
3501.842107	737445.899286	43.127297
3501.595147	737417.191788	43.132301
3502.160134	737395.425833	43.137306
3501.878435	737384.042375	43.142311
3502.274932	737356.663285	43.147316
3502.019931	737350.272996	43.152321
3501.821743	737329.078310	43.157325
3502.384435	737306.867159	43.162330
3502.321905	737285.452012	43.167335
3502.349572	737258.479910	43.172340
3502.026326	737220.135293	43.177345
3501.724620	737203.757166	43.182349
3501.909203	737191.108800	43.187354
3501.657198	737176.256360	43.192359
3501.922183	737150.333293	43.197364
3501.841129	737132.137175	43.202369
3501.716587	737114.443033	43.207373
3502.063264	737096.176150	43.212378
3501.633445	737077.740644	43.217383
3501.810266	737056.582230	43.222388
3501.888511	737047.464526	43.227393
3501.509789	737024.517462	43.232397
3502.046920	736996.569582	43.237402
3501.883039	736993.034003	43.242407
3501.700707	736967.431681	43.247412
3501.906967	736942.210419	43.252417
3501.543297	736943.210881	43.257421
3501.896884	736913.165227	43.262426
3501.778735	736900.170554	43.267431
3501.674123	736887.915889	43.272436
3501.878371	736865.416359	43.277441
3501.900587	736849.973666	43.282445
3501.917377	736828.692641	43.287450
3501.847115	736812.127008	43.292455
3502.084935	736796.302190	43.297460
3501.474161	736781.656757	43.302465
3501.630417	736771.387692	43.307469
3501.933383	736752.978795	43.312474
3501.802523	736734.394121	43.317479
3502.025823	736714.414770	43.322484
3501.862988	736700.140534	43.327489
3501.874185	736675.890892	43.332493
3501.689404	736663.154274	43.337498
3501.648900	736659.697130	43.342503
3501.822211	736631.758614	43.347508
3501.903096	736608.833375	43.352513
3501.797006	736605.683963	43.357517
3501.868477	736578.059006	43.362522
3501.773318	736569.464277	43.367527
3501.596100	736551.480674	43.372532
3501.803186	736528.930243	43.377537
3501.653697	736522.224932	43.382541
3501.710518	736503.064351	43.387546
3501.908972	736480.515210	43.392551
3501.990575	736465.655806	43.397556
3501.651191	736443.591335	43.402561
3501.605503	736431.969566	43.407565
3501.695653	736418.543791	43.412570
3501.543963	736415.500813	43.417575
3501.319095	736383.074395	43.422580
3501.375277	736375.345223	43.427585
3501.599376	736367.885221	43.432589
3501.794442	736365.180823	43.437594
3501.597975	736341.706800	43.442599
3501.521733	736329.298126	43.447604
3501.730796	736319.118731	43.452609
3501.449192	736308.575015	43.457613
3501.784670	736275.560684	43.462618
3501.828193	736271.644093	43.467623
3501.682174	736260.335584	43.472628
3501.802594	736232.107486	43.477633
3501.807915	736221.664705	43.482637
3501.826580	736215.525211	43.487642
3501.335985	736196.652312	43.492647
3501.549892	736164.746366	43.497652
3501.729299	736166.152064	43.502657
3501.479498	736156.790624	43.507661
3501.756673	736129.723995	43.512666
3501.813896	736113.878185	43.517671
3501.709306	736103.552391	43.522676
3501.910165	736077.685940	43.527681
3501.754311	736067.220103	43.532685
3501.954935	736051.845368	43.537690
3501.572440	736034.290440	43.542695
3501.655838	736024.230417	43.547700
3501.603331	736016.073452	43.552705
3501.287221	735989.153880	43.557709
3501.482945	735982.836478	43.562714
3501.500678	735981.052076	43.567719
3501.512906	735972.240999	43.572724
3501.769837	735959.826185	43.577729
3501.512723	735935.717621	43.582733
3501.379108	735921.635127	43.587738
3500.974831	735914.525996	43.592743
3501.400768	735917.078769	43.597748
3501.512613	735908.053198	43.602753
3501.332076	735880.714933	43.607757
3501.646619	735876.802853	43.612762
3501.202291	735876.431032	43.617767
3501.471481	735869.309550	43.622772
3501.615464	735852.459073	43.627777
3501.410164	735830.271769	43.632781
3501.660309	735819.639534	43.637786
3501.483591	735815.610642	43.642791
3501.699900	735793.798986	43.647796
3501.802677	735776.608720	43.652801
3501.709612	735769.744979	43.657805
3501.846829	735756.607265	43.662810
3501.668986	735738.918886	43.667815
3501.547041	735729.387342	43.672820
3501.481068	735719.401112	43.677825
3501.597768	735690.924265	43.682829
3501.974731	735674.826783	43.687834
3501.640577	735677.208289	43.692839
3501.568494	735651.633028	43.697844
3501.706931	735645.473305	43.702849
3501.247538	735636.541826	43.707853
3501.307361	735626.237740	43.712858
3501.382652	735620.286401	43.717863
3501.654725	735601.929463	43.722868
3501.696597	735591.034390	43.727873
3501.287156	735588.479120	43.732877
3501.418640	735577.816682	43.737882
3501.421069	735553.119659	43.742887
3501.315195	735535.913865	43.747892
3501.500599	735517.769028	43.752897
3501.178186	735523.613138	43.757901
3501.647824	735522.397363	43.762906
3501.428945	735504.764741	43.767911
3501.248436	735490.788224	43.772916
3501.763051	735474.717087	43.777921
3501.266673	735472.126653	43.782925
3501.818115	735470.550901	43.787930
3501.632046	735444.399897	43.792935
3501.424505	735434.436706	43.797940
3501.397546	735432.362608	43.802945
3501.527141	735423.581026	43.807949
3501.420052	735398.406689	43.812954
3501.777160	735393.101522	43.817959
3501.536280	735382.648840	43.822964
3501.773321	735376.175654	43.827969
3501.166956	735352.568491	43.832973
3501.529548	735330.780898	43.837978
3501.208883	735338.555119	43.842983
3501.535360	735332.908516	43.847988
3501.498733	735314.750418	43.852993
3501.593752	735293.947330	43.857997
3501.131207	735283.580643	43.863002
3501.152826	735285.062068	43.868007
3501.136971	735282.837612	43.873012
3501.476588	735270.358577	43.878017
3501.338332	735269.193727	43.883021
3501.618251	735245.489283	43.888026
3501.430674	735233.394277	43.893031
3501.457240	735228.688065	43.898036
3501.624661	735222.424240	43.903041
3501.291064	735214.807856	43.908045
3501.340070	735191.141410	43.913050
3501.556282	735183.533130	43.918055
3501.398475	735185.836142	43.923060
3501.599341	735182.189988	43.928065
3501.463704	735151.228684	43.933069
3501.637362	735143.033456	43.938074
3501.421743	735152.176362	43.943079
3501.287314	735128.540045	43.948084
3501.875978	735104.239716	43.953089
3501.838023	735096.920832	43.958093
3501.673912	735087.197510	43.963098
3501.440970	735063.082324	43.968103
3501.453049	735043.381197	43.973108
3501.431086	735028.833221	43.978113
3501.359451	735043.446497	43.983117
3501.782426	735025.310786	43.988122
3501.594921	735012.126524	43.993127
3501.821549	734989.717028	43.998132
3501.795577	734986.801217	44.003137
3501.822855	734969.572204	44.008141
3501.808574	734951.558081	44.013146
3501.871312	734937.490905	44.018151
3501.912103	734921.694954	44.023156
3501.609824	734900.956502	44.028161
3501.691040	734882.431476	44.033165
3501.638911	734869.125614	44.038170
3501.430214	734861.240769	44.043175
3501.470401	734854.205732	44.048180
3501.261375	734841.915692	44.053185
3501.454578	734817.184878	44.058189
3501.507515	734807.177862	44.063194
3501.669693	734804.280390	44.068199
3501.422729	734811.547966	44.073204
3501.584086	734764.449481	44.078209
3501.332673	734770.282401	44.083213
3501.676942	734761.217134	44.088218
3501.200636	734758.623146	44.093223
3501.345927	734752.214119	44.098228
3501.807065	734730.854096	44.103233
3501.636304	734721.725401	44.108237
3501.965858	734710.435109	44.113242
3501.640155	734689.551488	44.118247
3501.843449	734664.571049	44.123252
3501.632740	734659.408733	44.128257
3501.429677	734644.296009	44.133261
3501.818045	734628.244050	44.138266
3501.756178	734613.998906	44.143271
3501.779907	734598.551628	44.148276
3501.933606	734575.806542	44.153281
3501.439368	734571.285007	44.158285
3501.590584	734552.302164	44.163290
3501.632449	734540.762183	44.168295
3501.631323	734527.991816	44.173300
3501.653181	734523.879957	44.178305
3501.261415	734500.432813	44.183309
3501.518856	734475.145842	44.188314
3501.894094	734474.737507	44.193319
3501.639404	734476.710235	44.198324
3501.756996	734449.169327	44.203329
3501.610649	734444.243733	44.208333
3501.862540	734433.906378	44.213338
3501.464849	734410.608449	44.218343
3501.338859	734390.532541	44.223348
3501.651740	734384.887525	44.228353
3501.776876	734378.283533	44.233357
3501.601819	734355.394152	44.238362
3501.704895	734345.922777	44.243367
3501.566396	734340.550322	44.248372
3501.764660	734324.826175	44.253377
3501.343671	734305.442306	44.258381
3501.457877	734281.069403	44.263386
3501.607274	734273.669308	44.268391
3501.474288	734280.869025	44.273396
3501.399201	734258.210349	44.278401
3501.493824	734238.988617	44.283405
3501.579198	734230.510047	44.288410
3501.831277	734230.023051	44.293415
3501.405535	734213.263287	44.298420
3501.690392	734190.247933	44.303425
3501.404897	734199.007458	44.308429
3501.738658	734177.419514	44.313434
3501.782048	734154.740968	44.318439
3501.560792	734150.520591	44.323444
3501.636010	734140.756570	44.328449
3501.578619	734118.094575	44.333453
3501.564676	734105.127649	44.338458
3501.698685	734096.195386	44.343463
3501.463915	734085.640997	44.348468
3501.852003	734057.262021	44.353473
3501.493157	734046.381572	44.358477
3501.727898	734043.719347	44.363482
3501.739788	734021.689157	44.368487
3501.376967	734009.967779	44.373492
3501.322054	734000.225093	44.378497
3501.570039	734000.382290	44.383501
3501.676778	733990.266363	44.388506
3501.525321	733979.351551	44.393511
3501.440402	733960.802355	44.398516
3501.728782	733963.180488	44.403521
3501.242748	733935.440558	44.408525
3501.529985	733911.433963	44.413530
3501.433017	733901.005068	44.418535
3501.081942	733904.181929	44.423540
3501.414688	733898.186772	44.428545
3501.360695	733895.225692	44.433549
3501.712091	733871.109369	44.438554
3501.629634	733860.925539	44.443559
3501.257537	733855.739871	44.448564
3501.466571	733855.408477	44.453569
3501.169096	733834.913992	44.458573
3501.039091	733825.827045	44.463578
3501.240668	733806.388594	44.468583
3501.164641	733813.925839	44.473588
3501.561489	733806.929955	44.478593
3501.631148	733811.472923	44.483597
3501.368438	733792.903217	44.488602
3501.282035	733775.294405	44.493607
3501.151967	733758.781851	44.498612
3501.494578	733757.784832	44.503617
3501.225841	733757.829409	44.508621
3501.325762	733756.080436	44.513626
3501.515215	733750.108850	44.518631
3501.642388	733735.187361	44.523636
3501.589601	733709.800745	44.528641
3501.401711	733708.643866	44.533645
3501.843621	733697.779129	44.538650
3501.527691	733677.782334	44.543655
3501.545491	733680.799315	44.548660
3501.928361	733667.518589	44.553665
3501.754393	733632.844951	44.558669
3501.498340	733630.016173	44.563674
3501.535732	733630.158676	44.568679
3501.434231	733618.096515	44.573684
3501.675657	733588.304494	44.578689
3501.635258	733583.707396	44.583693
3501.587305	733575.844227	44.588698
3501.763667	733556.359835	44.593703
3501.701767	733538.894972	44.598708
3501.714637	733527.803876	44.603713
3501.696799	733521.717861	44.608717
3501.962363	733493.604677	44.613722
3501.437055	733481.562841	44.618727
3501.379288	733478.107177	44.623732
3501.421068	733447.407025	44.628737
3501.393688	733440.084885	44.633741
3501.592651	733437.032329	44.638746
3501.669936	733428.059195	44.643751
3501.323856	733412.225201	44.648756
3501.565397	733395.006917	44.653761
3501.610937	733394.900547	44.658765
3501.342228	733385.093435	44.663770
3501.628569	733375.194588	44.668775
3501.276489	733352.430617	44.673780
3501.313987	733340.642108	44.678785
3501.294117	733338.615803	44.683789
3501.428730	733333.346060	44.688794
3501.637953	733316.380479	44.693799
3501.214207	733309.024708	44.698804
3501.539140	733289.366601	44.703809
3501.188681	733295.860535	44.708813
3501.342007	733286.429119	44.713818
3501.099967	733291.469449	44.718823
3500.938105	733274.416583	44.723828
3501.272293	733276.044753	44.728833
3500.982015	733257.725900	44.733837
3501.499118	733238.530980	44.738842
3501.098510	733235.676443	44.743847
3501.199063	733241.798849	44.748852
3501.354170	733237.515794	44.753857
3501.634559	733242.519329	44.758861
3501.719498	733220.969947	44.763866
3501.723366	733199.978483	44.768871
3501.245161	733199.612112	44.773876
3501.832262	733192.386231	44.778881
3501.200877	733164.519138	44.783885
3501.416233	733141.858832	44.788890
3501.382183	733148.894686	44.793895
3501.152839	733145.813785	44.798900
3501.746551	733137.398584	44.803905
3501.461448	733128.237464	44.808909
3501.620745	733099.298840	44.813914
3501.454483	733102.643501	44.818919
3501.264512	733094.506285	44.823924
3501.470566	733083.976748	44.828929
3501.310405	733065.982511	44.833933
3501.228748	733041.836260	44.838938
3501.196465	733054.367301	44.843943
3501.407595	733046.609325	44.848948
3501.934470	733045.631281	44.853953
3501.348131	733018.498859	44.858957
3501.561260	733005.096572	44.863962
3501.623744	733007.759864	44.868967
3500.997549	733002.764155	44.873972
3501.128136	732987.246620	44.878977
3501.143638	732967.589357	44.883981
3501.560455	732957.470403	44.888986
3501.301832	732948.403720	44.893991
3501.390677	732951.013166	44.898996
3501.690997	732953.934224	44.904001
3501.250656	732934.451226	44.909005
3501.528315	732915.146583	44.914010
3501.692400	732907.396248	44.919015
3501.574604	732913.158915	44.924020
3501.407256	732876.302536	44.929025
3501.127285	732861.001132	44.934029
3501.491134	732857.574547	44.939034
3501.451810	732857.234649	44.944039
3501.418903	732860.903937	44.949044
3501.596586	732842.358279	44.954049
3501.242434	732833.851856	44.959053
3501.363784	732828.732504	44.964058
3501.451543	732811.736428	44.969063
3501.306796	732813.542858	44.974068
3501.411541	732803.178226	44.979073
3501.379573	732782.538165	44.984077
3501.602736	732757.201967	44.989082
3501.578495	732764.088006	44.994087
3501.126018	732764.955104	44.999092
3501.400075	732767.781551	45.004097
3501.203039	732733.404913	45.009101
3501.573039	732721.313003	45.014106
3501.509218	732723.106080	45.019111
3501.169756	732720.785862	45.024116
3501.560631	732712.700804	45.029121
3501.636294	732699.320727	45.034125
3501.626068	732671.893891	45.039130
3501.499553	732672.558601	45.044135
3501.431234	732675.936763	45.049140
3501.651678	732636.737731	45.054145
3501.619028	732626.940194	45.059149
3501.557292	732623.286776	45.064154
3501.516691	732618.342587	45.069159
3501.044422	732588.714329	45.074164
3501.513953	732577.843529	45.079169
3501.725003	732582.957957	45.084173
3501.420448	732577.116654	45.089178
3501.491446	732560.667440	45.094183
3501.541912	732547.538831	45.099188
3501.643983	732521.281193	45.104193
3501.560698	732531.642977	45.109197
3501.316507	732521.632714	45.114202
3501.677022	732501.026098	45.119207
3501.339309	732488.209097	45.124212
3501.682983	732481.022815	45.129217
3501.519854	732483.872098	45.134221
3501.624686	732461.277660	45.139226
3501.608606	732450.239380	45.144231
3501.526982	732441.737016	45.149236
3502.002927	732423.438181	45.154241
3501.910661	732408.500993	45.159245
3501.617291	732392.903842	45.164250
3501.766683	732367.529103	45.169255
3501.482560	732351.979856	45.174260
3501.577609	732347.805281	45.179265
3501.568576	732345.380837	45.184269
3501.860167	732312.159468	45.189274
3502.186302	732305.718619	45.194279
3501.662532	732291.347647	45.199284
3501.802365	732250.377607	45.204289
3501.514126	732263.298762	45.209293
3501.806038	732232.206065	45.214298
3501.939553	732210.943041	45.219303
3501.942716	732209.655344	45.224308
3502.018943	732180.380565	45.229313
3501.751526	732176.463854	45.234317
3501.417118	732170.082539	45.239322
3501.945216	732152.863771	45.244327
3501.418090	732128.540836	45.249332
3501.362236	732112.705837	45.254337
3501.374072	732116.912721	45.259341
3501.082932	732096.957416	45.264346
3501.571228	732072.367482	45.269351
3501.412210	732066.699813	45.274356
3501.699589	732054.571049	45.279361
3501.516867	732053.759672	45.284365
3501.349179	732050.767188	45.289370
3501.707448	732021.791826	45.294375
3501.424741	732014.560100	45.299380
3501.590675	731999.430945	45.304385
3501.507648	731999.593377	45.309389
3501.640162	731974.616311	45.314394
3501.537253	731968.939300	45.319399
3501.330549	731962.289144	45.324404
3501.738032	731948.654933	45.329409
3501.400540	731925.042768	45.334413
3501.455317	731917.804700	45.339418
3501.677492	731907.370001	45.344423
3501.248230	731902.489600	45.349428
3501.722813	731879.386800	45.354433
3501.545087	731880.159066	45.359437
3501.487200	731863.482157	45.364442
3501.473301	731862.543831	45.369447
3501.116151	731837.003559	45.374452
3501.466147	731828.082615	45.379457
3501.097687	731814.774468	45.384461
3501.327100	731825.085481	45.389466
3501.403125	731820.963295	45.394471
3501.363259	731821.118598	45.399476
3501.097976	731795.662045	45.404481
3501.385905	731785.315354	45.409485
3501.196080	731781.534174	45.414490
3501.492250	731775.048342	45.419495
3501.233782	731775.883476	45.424500
3501.489231	731770.939360	45.429505
3501.404268	731746.245107	45.434509
3501.557999	731730.968920	45.439514
3501.525689	731720.328454	45.444519
3501.822058	731721.715616	45.449524
3501.586334	731700.512269	45.454529
3501.077260	731678.264676	45.459533
3501.541680	731680.366821	45.464538
3501.861059	731672.391578	45.469543
3501.471621	731664.384912	45.474548
3501.863182	731626.489656	45.479553
3501.658259	731629.890827	45.484557
3501.498268	731626.352228	45.489562
3501.396569	731594.975513	45.494567
3501.045466	731582.505903	45.499572
3501.679264	731582.005198	45.504577
3501.422543	731586.405288	45.509581
3501.642637	731572.256726	45.514586
3501.542300	731547.316821	45.519591
3501.281236	731550.776820	45.524596
3501.836165	731532.462926	45.529601
3501.489597	731537.967270	45.534605
3501.363180	731508.079823	45.539610
3501.665587	731496.393400	45.544615
3501.607963	731485.855844	45.549620
3501.506186	731478.791808	45.554625
3501.659843	731456.434086	45.559629
3501.819571	731439.918414	45.564634
3501.948743	731435.044480	45.569639
3501.460133	731420.369035	45.574644
3501.986633	731394.780376	45.579649
3501.792812	731388.226654	45.584653
3501.522873	731360.343106	45.589658
3501.637846	731350.172999	45.594663
3501.613587	731342.699886	45.599668
3501.790979	731326.230582	45.604673
3501.807538	731313.798837	45.609677
3501.521837	731302.605471	45.614682
3501.421961	731288.410252	45.619687
3501.236927	731271.158908	45.624692
3501.848408	731249.220148	45.629697
3501.744926	731253.892208	45.634701
3501.499657	731234.075748	45.639706
3501.216256	731215.800639	45.644711
3501.585119	731212.620137	45.649716
3501.614118	731203.900113	45.654721
3501.656008	731202.457298	45.659725
3501.631967	731174.383916	45.664730
3501.763754	731165.547826	45.669735
3501.322559	731164.036276	45.674740
3501.488996	731144.547718	45.679745
3501.526271	731122.307347	45.684749
3501.720194	731107.270943	45.689754
3501.747146	731096.421784	45.694759
3501.578770	731084.664008	45.699764
3501.582924	731070.104575	45.704769
3501.522203	731069.817656	45.709773
3501.606695	731054.502117	45.714778
3501.595675	731030.239144	45.719783
3501.650324	731029.735077	45.724788
3501.651078	731017.057886	45.729793
3501.535961	731012.224068	45.734797
3501.536928	730984.839185	45.739802
3501.730391	730959.056587	45.744807
3501.536065	730972.558525	45.749812
3501.566942	730938.433717	45.754817
3501.603137	730908.021973	45.759821
3501.531148	730835.881398	45.764826
3501.413124	730710.560950	45.769831
3501.126587	730545.994482	45.774836
3501.414544	730300.208422	45.779841
3501.225297	730013.733492	45.784845
3500.849037	729662.099795	45.789850
3500.944885	729249.350593	45.794855
3500.304730	728793.756207	45.799860
3500.109189	728259.199910	45.804865
3499.956868	727691.855112	45.809869
3499.239108	727057.332679	45.814874
3499.286375	726373.284269	45.819879
3498.764467	725614.645956	45.824884
3498.613981	724812.413840	45.829889
3498.204851	723942.740399	45.834893
3497.533988	723020.773068	45.839898
3497.334557	722024.312622	45.844903
3496.627851	720998.117222	45.849908
3495.857663	719883.738374	45.854913
3495.470873	718733.439121	45.859917
3494.917413	717502.555335	45.864922
3494.621782	716219.060788	45.869927
3493.483989	714875.175032	45.874932
3493.006298	713476.576621	45.879937
3492.408275	712008.924741	45.884941
3491.121941	710490.050529	45.889946
3490.700426	708900.803094	45.894951
3489.846952	707267.480810	45.899956
3489.126361	705554.451386	45.904961
3488.383163	703794.633457	45.909965
3487.330806	701971.748497	45.914970
3486.274901	700089.883138	45.919975
3485.291865	698148.640618	45.924980
3484.183714	696160.348241	45.929985
3482.991338	694096.072884	45.934989
3482.001511	691985.466223	45.939994
3480.719862	689817.284274	45.944999
3479.597344	687617.892730	45.950004
3478.442365	685327.511889	45.955009
3477.304112	683004.979153	45.960013
3476.320887	680607.762305	45.965018
3475.098261	678161.830410	45.970023
3473.552842	675672.296068	45.975028
3472.279548	673111.413009	45.980033
3470.905887	670497.090655	45.985037
3469.823591	667833.564458	45.990042
3468.786297	665107.467923	45.995047
3466.751581	662335.095720	46.000052
3465.613954	659501.024387	46.005057
3463.997033	656609.229258	46.010061
3462.691598	653688.057770	46.015066
3461.357366	650689.029755	46.020071
3459.469175	647661.151563	46.025076
3457.776416	644554.584034	46.030081
3456.358579	641412.261004	46.035085
3454.649385	638219.043404	46.040090
3452.778887	634975.922522	46.045095
3451.206357	631683.035681	46.050100
3449.664493	628332.678748	46.055105
3447.444282	624940.152731	46.060109
3445.712937	621493.861158	46.065114
3443.824957	618001.088599	46.070119
3441.911240	614467.396336	46.075124
3440.196168	610867.441927	46.080129
3438.324017	607236.403459	46.085133
3436.339519	603560.103835	46.090138
3434.560384	599809.643315	46.095143
3432.552536	596021.345446	46.100148
3430.778547	592184.310978	46.105153
3428.677846	588304.731560	46.110157
3426.353012	584385.983149	46.115162
3424.050981	580405.425032	46.120167
3422.102348	576387.406467	46.125172
3419.709869	572320.819650	46.130177
3417.480423	568227.229641	46.135181
3415.204802	564087.178014	46.140186
3413.192524	559895.501192	46.145191
3410.490801	555666.232787	46.150196
3408.325129	551399.356301	46.155201
3406.105261	547070.100332	46.160205
3403.841756	542720.283028	46.165210
3401.555591	538313.229561	46.170215
3398.983837	533874.385420	46.175220
3396.689028	529382.552131	46.180225
3394.217633	524853.483120	46.185229
3391.224783	520291.519156	46.190234
3388.958801	515684.829045	46.195239
3386.127763	511036.240145	46.200244
3383.704912	506354.225177	46.205249
3381.143191	501647.114626	46.210253
3378.279464	496897.642343	46.215258
3376.263898	492092.556360	46.220263
3373.209889	487277.344609	46.225268
3370.522668	482398.337278	46.230273
3367.555217	477500.533796	46.235277
3364.476085	472563.306819	46.240282
3362.158716	467584.029076	46.245287
3359.047713	462579.781128	46.250292
3356.325112	457554.334145	46.255297
3353.436927	452487.262178	46.260301
3350.335821	447394.499581	46.265306
3347.553990	442253.045397	46.270311
3344.548891	437098.657727	46.275316
3341.480583	431903.931502	46.280321
3338.720897	426679.879084	46.285325
3335.303141	421439.572759	46.290330
3332.798961	416148.805686	46.295335
3329.171816	410854.089984	46.300340
3326.013483	405505.970425	46.305345
3323.179136	400153.485365	46.310349
3319.851719	394770.836424	46.315354
3316.882419	389357.218925	46.320359
3313.174120	383916.141838	46.325364
3310.136607	378464.965565	46.330369
3307.222716	372978.846207	46.335373
3303.699555	367479.571375	46.340378
3300.349665	361939.653513	46.345383
3296.516108	356399.291225	46.350388
3293.666748	350831.468090	46.355393
3290.064155	345241.719562	46.360397
3286.648888	339623.614034	46.365402
3283.324995	333988.781218	46.370407
3279.576972	328349.206094	46.375412
3275.982902	322684.216833	46.380417
3272.868184	317014.086912	46.385421
3268.931412	311331.691708	46.390426
3265.825250	305622.287092	46.395431
3261.917449	299909.888945	46.400436
3258.600389	294170.248338	46.405441
3254.327893	288417.185010	46.410445
3250.431624	282673.647000	46.415450
3247.267985	276914.384806	46.420455
3243.474015	271146.137943	46.425460
3239.751241	265354.243489	46.430465
3235.828821	259565.025061	46.435469
3231.877026	253782.627820	46.440474
3228.087113	247974.799471	46.445479
3223.846250	242175.918315	46.450484
3220.085726	236377.600804	46.455489
3216.348209	230561.813031	46.460493
3212.458523	224759.624520	46.465498
3208.719085	218936.222775	46.470503
3204.350136	213119.007150	46.475508
3200.908248	207264.128657	46.480513
3196.732537	201392.501841	46.485517
3192.552210	195583.596797	46.490522
3188.567364	189755.159189	46.495527
3184.043922	183943.797620	46.500532
3180.041314	178137.864600	46.505537
3175.937190	172337.153156	46.510541
3171.588267	166549.124098	46.515546
3167.296172	160759.881102	46.520551
3162.782615	154994.762736	46.525556
3158.417518	149225.122171	46.530561
3154.079082	143486.283757	46.535565
3149.464030	137742.636176	46.540570
3145.103692	132016.839650	46.545575
3140.452729	126322.643544	46.550580
3135.779509	120643.821315	46.555585
3131.399336	114964.454816	46.560589
3126.303588	109330.932178	46.565594
3122.025319	103699.961854	46.570599
3116.722583	98112.220562	46.575604
3112.030558	92539.031659	46.580609
3107.438425	87003.231731	46.585613
3102.454820	81495.049872	46.590618
3097.305906	75999.582436	46.595623
3091.876653	70557.181509	46.600628
3086.598052	65155.887225	46.605633
3081.332895	59779.098308	46.610637
3075.819534	54457.848276	46.615642
3070.357892	49170.512154	46.620647
3064.135177	43963.471033	46.625652
3057.996640	38784.531269	46.630657
3051.281297	33687.269973	46.635661
3041.609173	28741.798104	46.640666
3025.971532	24051.225015	46.645671
3009.357896	19552.043983	46.650676
2992.714717	15283.595730	46.655681
2974.964434	11293.928521	46.660685
2949.978235	7822.491180	46.665690
2920.129985	4850.411112	46.670695
2891.235883	2321.206303	46.675700
2856.812680	464.341038	46.680705
2786.066140	255.566980	46.685709
2741.675703	256.969626	46.690714
2732.307375	242.855230	46.695719
2746.038277	253.982770	46.700724
2769.529658	252.745261	46.705729
2791.503878	248.439132	46.710733
2805.681938	242.012431	46.715738
2811.681193	226.737540	46.720743
2810.796628	228.799893	46.725748
2806.516919	240.285949	46.730753
2801.721574	242.121368	46.735757
2796.853907	242.404642	46.740762
2793.997243	227.232482	46.745767
2790.993320	225.791765	46.750772
2788.079462	225.588070	46.755777
2785.760446	228.909285	46.760781
2782.663740	236.303268	46.765786
2780.553426	224.915125	46.770791
2777.572431	231.783582	46.775796
2774.748383	223.356267	46.780801
2771.974795	215.712336	46.785805
2768.102750	228.709860	46.790810
2765.117718	222.812856	46.795815
2761.818213	221.813792	46.800820
2758.835725	220.495454	46.805825
2755.963680	211.610777	46.810829
2752.700228	218.769711	46.815834
2749.344507	213.590828	46.820839
2745.856473	214.192231	46.825844
2742.407253	213.261380	46.830849
2739.649878	215.873118	46.835853
2736.249894	219.135096	46.840858
2732.722599	214.276690	46.845863
2729.682561	217.177753	46.850868
2726.354594	218.474152	46.855873
2722.941067	220.193210	46.860877
2719.355590	213.221660	46.865882
2716.204331	204.823699	46.870887
2712.917563	212.267529	46.875892
2709.783534	210.407157	46.880897
2706.574548	210.449316	46.885901
2702.414034	210.002307	46.890906
2699.117963	206.235428	46.895911
2695.834857	204.835866	46.900916
2692.177291	211.545219	46.905921
2689.331046	204.862586	46.910925
2685.403578	218.263821	46.915930
2681.886862	197.973514	46.920935
2679.191195	203.075169	46.925940
2675.738843	198.302095	46.930945
2672.698226	192.071990	46.935949
2668.742491	202.370201	46.940954
2665.051982	197.089932	46.945959
2661.868480	204.465587	46.950964
2657.978404	202.327052	46.955969
2654.886964	198.996201	46.960973
2651.112732	197.079053	46.965978
2648.279990	194.727009	46.970983
2644.761032	199.811446	46.975988
2640.858192	198.702193	46.980993
2637.255910	195.803441	46.985997
2633.446666	200.373724	46.991002
2630.359147	197.056846	46.996007
2627.151186	205.017147	47.001012
2623.749839	199.710750	47.006017
2620.625890	192.082715	47.011021
2617.589088	206.394279	47.016026
2614.206933	191.259573	47.021031
2610.582443	194.843176	47.026036
2606.404106	193.861265	47.031041
2603.113408	186.554495	47.036045
2599.858478	203.385103	47.041050
2596.277859	192.689468	47.046055
2592.955313	197.215714	47.051060
2589.047923	189.335759	47.056065
2585.773162	190.311066	47.061069
2582.153442	196.570023	47.066074
2578.855648	186.850000	47.071079
2575.609676	187.481717	47.076084
2571.527272	192.596741	47.081089
2568.693665	177.103877	47.086093
2564.359401	189.455200	47.091098
2561.543021	181.779847	47.096103
2558.075822	180.146638	47.101108
2554.629513	185.095183	47.106113
2551.244823	178.894124	47.111117
2547.837836	188.554742	47.116122
2544.429480	186.098566	47.121127
2540.677616	183.925617	47.126132
2537.217450	179.673359	47.131137
2533.749986	181.380180	47.136141
2530.284611	194.621333	47.141146
2526.778440	184.415278	47.146151
2523.112856	187.532931	47.151156
2519.505621	185.750861	47.156161
2516.035332	182.650784	47.161165
2512.757941	180.575720	47.166170
2509.367629	175.579793	47.171175
2505.923520	185.986409	47.176180
2502.590293	185.215142	47.181185
2499.358081	178.151769	47.186189
2495.288866	188.131848	47.191194
2492.003047	180.708924	47.196199
2488.240822	179.081408	47.201204
2484.582489	179.793907	47.206209
2481.905915	176.867124	47.211213
2477.914085	178.367374	47.216218
2474.487676	176.601184	47.221223
2470.826363	174.764964	47.226228
2467.436932	179.294480	47.231233
2464.416642	177.120442	47.236237
2460.449423	178.545590	47.241242
2457.055733	169.043444	47.246247
2453.270629	167.602683	47.251252
2449.867902	176.690177	47.256257
2446.664638	167.994803	47.261261
2443.225918	171.132969	47.266266
2439.621921	167.785933	47.271271
2436.179811	172.118566	47.276276
2432.635347	168.624922	47.281281
2429.344753	168.289088	47.286285
2425.863142	169.580570	47.291290
2422.377166	176.366494	47.296295
2418.949898	166.466386	47.301300
2415.130888	174.971820	47.306305
2411.725756	171.219102	47.311309
2408.085880	185.675630	47.316314
2404.747864	169.939452	47.321319
2401.250814	171.385265	47.326324
2397.684246	175.125408	47.331329
2394.109610	172.541591	47.336333
2390.558609	180.058003	47.341338
2387.383300	169.516680	47.346343
2383.866015	181.026584	47.351348
2380.323134	174.016341	47.356353
2376.665291	166.176785	47.361357
2373.047706	172.841470	47.366362
2369.720045	162.617263	47.371367
2366.326468	177.285221	47.376372
2362.627709	172.185002	47.381377
2359.252190	172.896947	47.386381
2355.376144	170.413404	47.391386
2352.297277	165.979561	47.396391
2348.915981	171.994566	47.401396
2345.346638	168.941829	47.406401
2341.852854	163.122722	47.411405
2338.506061	164.316761	47.416410
2334.862347	166.441885	47.421415
2331.458740	171.068966	47.426420
2327.551149	166.260304	47.431425
2324.310476	163.795488	47.436429
2320.614949	164.440681	47.441434
2316.993672	165.510684	47.446439
2313.793110	167.785027	47.451444
2310.090689	178.213839	47.456449
2307.014409	166.275211	47.461453
2303.503709	166.328378	47.466458
2300.302730	166.501145	47.471463
2296.556030	154.708900	47.476468
2292.866744	165.518576	47.481473
2289.803660	160.588626	47.486477
2285.669167	170.666515	47.491482
2282.563442	163.751501	47.496487
2278.730761	165.191830	47.501492
2275.264502	168.794291	47.506497
2271.971239	157.833931	47.511501
2268.497160	161.966163	47.516506
2264.791176	161.468378	47.521511
2261.513746	157.340023	47.526516
2257.882308	168.549030	47.531521
2254.340162	153.056006	47.536525
2251.141258	158.878655	47.541530
2246.872715	164.399348	47.546535
2243.721381	159.421693	47.551540
2240.638164	161.576404	47.556545
2237.204845	157.075662	47.561549
2233.563621	165.266440	47.566554
2229.956953	154.093997	47.571559
2226.411173	151.625731	47.576564
2222.644740	154.780859	47.581569
2219.414654	158.762795	47.586573
2215.655767	156.689586	47.591578
2212.250345	157.184400	47.596583
2209.386966	155.320038	47.601588
2205.414296	165.378490	47.606593
2201.861673	153.160900	47.611597
2198.326594	160.064249	47.616602
2194.608960	158.001591	47.621607
2191.663944	157.452013	47.626612
2187.812041	159.142676	47.631617
2184.648292	148.959575	47.636621
2180.943786	168.395137	47.641626
2177.623476	150.050219	47.646631
2174.468526	149.552204	47.651636
2170.360051	161.034281	47.656641
2167.131093	151.299692	47.661645
2163.176234	161.792923	47.666650
2160.037079	160.484597	47.671655
2156.721973	158.946910	47.676660
2152.669754	156.306462	47.681665
2149.132632	153.774076	47.686669
2145.978149	152.481326	47.691674
2142.335670	156.654381	47.696679
2138.614230	151.264105	47.701684
2135.057205	162.121845	47.706689
2131.932964	150.586990	47.711693
2128.882807	160.797954	47.716698
2125.230045	156.924891	47.721703
2121.627027	153.652575	47.726708
2117.702972	156.888769	47.731713
2114.290783	152.023112	47.736717
2110.956640	158.692744	47.741722
2107.283875	154.325522	47.746727
2104.136445	153.610625	47.751732
2100.371535	163.016288	47.756737
2096.902737	146.284232	47.761741
2093.365598	150.548410	47.766746
2089.728019	162.035225	47.771751
2086.335686	154.404558	47.776756
2082.823447	163.252728	47.781761
2080.007738	148.400662	47.786765
2076.029707	153.714331	47.791770
2072.624430	149.477864	47.796775
2068.948405	151.269146	47.801780
2065.053684	150.657966	47.806785
2061.969922	149.327318	47.811789
2058.509181	146.232575	47.816794
2054.618310	156.465660	47.821799
2051.395228	147.564152	47.826804
2047.687010	159.673658	47.831809
2044.324464	150.795657	47.836813
2040.813712	153.239408	47.841818
2037.518228	152.675785	47.846823
2034.264136	158.026425	47.851828
2030.421157	154.963662	47.856833
2026.960721	153.505417	47.861837
2023.216138	154.280758	47.866842
2020.315771	150.434681	47.871847
2016.788036	150.080846	47.876852
2013.053485	158.863683	47.881857
2009.502777	141.902963	47.886861
2005.761876	151.544680	47.891866
2002.106966	151.407295	47.896871
1998.714106	149.085181	47.901876
1995.342262	147.943614	47.906881
1992.103689	147.477751	47.911885
1988.378995	152.062391	47.916890
1984.901322	141.291523	47.921895
1981.447333	151.929632	47.926900
1977.682218	152.067070	47.931905
1974.363467	146.818416	47.936909
1970.790346	144.991322	47.941914
1967.600054	144.053933	47.946919
1964.045073	149.480728	47.951924
1960.659513	152.071141	47.956929
1957.353094	148.213069	47.961933
1953.683516	144.675468	47.966938
1950.081428	144.305992	47.971943
1946.401357	143.982988	47.976948
1942.553153	141.869386	47.981953
1939.313485	141.173257	47.986957
1935.707775	139.636157	47.991962
1931.991280	147.373133	47.996967
1928.625978	134.627891	48.001972
1925.374915	141.373279	48.006977
1921.983220	137.863858	48.011981
1918.472192	152.576418	48.016986
1914.976585	147.178138	48.021991
1911.750354	143.145198	48.026996
1907.761396	149.324575	48.032001
1904.426479	143.890994	48.037005
1900.634801	156.102455	48.042010
1897.348503	143.548387	48.047015
1894.050090	143.615464	48.052020
1890.314811	145.894673	48.057025
1886.967358	135.551265	48.062029
1883.558505	141.350750	48.067034
1879.799191	143.576527	48.072039
1876.244473	146.893813	48.077044
1872.650675	146.299645	48.082049
1869.568435	137.125528	48.087053
1865.993655	144.657915	48.092058
1862.389354	150.049947	48.097063
1858.860963	140.340008	48.102068
1855.643890	144.401159	48.107073
1852.090615	136.085988	48.112077
1848.328362	139.322054	48.117082
1844.517578	140.255348	48.122087
1841.063877	133.534747	48.127092
1837.747086	142.468312	48.132097
1834.123715	140.075024	48.137101
1830.976173	135.751063	48.142106
1827.425870	133.228059	48.147111
1823.834647	140.429902	48.152116
1820.118491	145.700200	48.157121
1816.932677	133.402084	48.162125
1813.326627	137.065574	48.167130
1809.929837	141.505438	48.172135
1806.721037	132.496805	48.177140
1802.793919	138.468884	48.182145
1799.369723	142.213148	48.187149
1795.551125	140.545696	48.192154
1791.785580	134.262031	48.197159
1788.435784	130.609424	48.202164
1785.126564	135.879591	48.207169
1781.908813	129.972827	48.212173
1778.602591	130.553973	48.217178
1774.921616	143.692420	48.222183
1771.536186	126.976305	48.227188
1767.700797	146.145513	48.232193
1764.461507	137.050997	48.237197
1760.884389	145.210006	48.242202
1757.103703	146.492218	48.247207
1753.655847	135.206126	48.252212
1750.660850	144.148969	48.257217
1747.393498	136.211174	48.262221
1743.640080	138.813601	48.267226
1739.555682	135.312406	48.272231
1736.341441	142.195292	48.277236
1732.707916	150.114637	48.282241
1728.884285	133.758125	48.287245
1725.536765	139.916586	48.292250
1722.485543	141.426602	48.297255
1718.913649	127.044570	48.302260
1714.860845	139.475084	48.307265
1711.622419	129.325909	48.312269
1708.222905	133.327426	48.317274
1704.887836	134.212182	48.322279
1701.488636	135.099482	48.327284
1697.644112	131.995866	48.332289
1694.008488	130.918213	48.337293
1690.891744	135.987228	48.342298
1687.208945	135.144734	48.347303
1683.828549	125.459972	48.352308
1680.056317	135.991011	48.357313
1676.725629	131.756742	48.362317
1673.212591	133.109707	48.367322
1669.619202	143.579931	48.372327
1666.322166	129.045823	48.377332
1662.955250	135.983276	48.382337
1659.420006	134.855071	48.387341
1655.749988	143.230059	48.392346
1651.953592	131.076343	48.397351
1649.020154	129.889620	48.402356
1644.587718	136.913357	48.407361
1641.926409	126.950759	48.412365
1638.442534	116.374665	48.417370
1634.674963	126.285325	48.422375
1631.408106	123.249794	48.427380
1627.577043	133.741688	48.432385
1623.969902	131.905946	48.437389
1620.553621	133.360133	48.442394
1616.961158	137.016802	48.447399
1613.919550	133.101508	48.452404
1610.237386	131.156460	48.457409
1607.010930	129.198614	48.462413
1603.359439	128.331471	48.467418
1599.421387	131.734054	48.472423
1596.148934	126.178704	48.477428
1592.219742	130.396995	48.482433
1588.962388	124.883351	48.487437
1585.441460	128.251715	48.492442
1582.377056	132.174880	48.497447
1579.067154	121.096191	48.502452
1575.202407	124.403366	48.507457
1571.476952	131.475914	48.512461
1568.000137	130.866176	48.517466
1564.441928	141.959757	48.522471
1560.959578	120.294355	48.527476
1558.020880	132.296760	48.532481
1554.866080	125.416754	48.537485
1550.916715	121.404373	48.542490
1546.999510	133.765974	48.547495
1543.663911	123.063754	48.552500
1539.754661	133.524681	48.557505
1536.398683	128.367249	48.562509
1533.260328	126.692439	48.567514
1529.672609	128.865609	48.572519
1526.137514	119.232701	48.577524
1522.164515	126.013431	48.582529
1519.031123	126.258089	48.587533
1515.693025	128.458355	48.592538
1511.880988	130.540666	48.597543
1508.984155	123.490445	48.602548
1504.928996	129.236763	48.607553
1501.384270	123.282245	48.612557
1497.940013	123.338113	48.617562
1494.151999	122.161001	48.622567
1490.883083	125.825692	48.627572
1487.784513	129.881281	48.632577
1484.569889	117.760933	48.637581
1480.477408	130.346622	48.642586
1476.617841	127.800236	48.647591
1473.339881	123.619368	48.652596
1469.840073	131.556608	48.657601
1466.475718	128.551197	48.662605
1463.152367	122.970069	48.667610
1459.384309	121.893678	48.672615
1456.383510	126.908507	48.677620
1452.710267	130.958781	48.682625
1449.729713	117.707788	48.687629
1445.767652	128.983274	48.692634
1441.778949	132.616806	48.697639
1438.198647	121.482451	48.702644
1434.971569	131.291609	48.707649
1431.317594	130.009842	48.712653
1428.081465	123.673085	48.717658
1424.453574	127.642059	48.722663
1421.053436	120.235715	48.727668
1417.468756	129.559741	48.732673
1414.017783	124.225180	48.737677
1410.538973	121.788975	48.742682
1407.207204	130.487542	48.747687
1403.782992	127.463698	48.752692
1399.764907	124.163216	48.757697
1396.335179	119.829589	48.762701
1392.981397	132.054068	48.767706
1389.028562	125.528762	48.772711
1386.167080	123.861630	48.777716
1382.292761	132.500620	48.782721
1379.177385	124.064549	48.787725
1375.473953	117.810477	48.792730
1371.545427	124.057872	48.797735
1368.568702	130.023680	48.802740
1365.023231	126.898029	48.807745
1361.673378	123.520697	48.812749
1357.992523	128.872563	48.817754
1354.593827	135.517152	48.822759
1351.068433	117.503135	48.827764
1347.491821	131.119513	48.832769
1344.043740	128.353061	48.837773
1340.598593	131.722089	48.842778
1337.059100	124.398138	48.847783
1333.147536	126.397667	48.852788
1329.400164	127.034792	48.857793
1326.322588	118.407992	48.862797
1322.969693	129.870657	48.867802
1319.744431	122.828494	48.872807
1316.111674	123.980809	48.877812
1312.426994	125.241985	48.882817
1308.883750	127.135847	48.887821
1305.824190	124.827136	48.892826
1301.866023	127.364075	48.897831
1298.530092	125.373339	48.902836
1295.061531	120.914031	48.907841
1291.336524	124.967311	48.912845
1287.773792	119.292453	48.917850
1284.075570	127.437000	48.922855
1280.995580	114.607983	48.927860
1277.143512	122.384763	48.932865
1273.876361	115.515750	48.937869
1270.505879	121.244425	48.942874
1266.419586	129.940188	48.947879
1263.324304	120.510855	48.952884
1259.895886	127.972286	48.957889
1256.811344	129.151918	48.962893
1253.422288	116.041092	48.967898
1249.369320	122.371404	48.972903
1245.615257	120.140457	48.977908
1241.947746	123.868112	48.982913
1238.697865	119.875984	48.987917
1235.237625	123.160381	48.992922
1231.810409	114.499512	48.997927
1228.580415	123.314923	49.002932
1225.319230	125.818010	49.007937
1221.498171	123.773238	49.012941
1218.047533	125.294442	49.017946
1214.066725	116.342794	49.022951
1210.344483	114.903445	49.027956
1207.257082	115.090400	49.032961
1204.010206	115.105690	49.037965
1200.722210	114.676102	49.042970
1196.768783	120.603371	49.047975
1193.069448	113.755614	49.052980
1189.522633	121.941622	49.057985
1186.119600	123.589342	49.062989
1182.851838	124.853892	49.067994
1179.200641	126.776829	49.072999
1175.847528	119.371994	49.078004
1172.027184	122.021369	49.083009
1168.510042	119.139452	49.088013
1165.008866	112.869602	49.093018
1161.706820	116.765602	49.098023
1158.260648	115.788443	49.103028
1155.226506	123.491199	49.108033
1151.640893	125.388282	49.113037
1147.981473	121.400047	49.118042
1144.137073	120.119164	49.123047
1141.178717	107.656682	49.128052
1137.069837	115.384630	49.133057
1133.438812	116.574909	49.138061
1130.392750	116.960295	49.143066
1126.369645	125.227552	49.148071
1123.164044	107.589942	49.153076
1119.692513	117.570118	49.158081
1116.188999	113.947561	49.163085
1112.597357	110.697597	49.168090
1109.317320	122.478072	49.173095
1105.757908	116.576696	49.178100
1101.990541	124.261436	49.183105
1098.561526	116.493542	49.188109
1095.508463	120.653562	49.193114
1091.723541	119.836270	49.198119
1088.000327	118.469623	49.203124
1084.504654	124.432539	49.208129
1081.236415	118.629492	49.213133
1077.729011	117.691376	49.218138
1074.544735	123.160204	49.223143
1070.943227	125.655950	49.228148
1067.066908	120.575619	49.233153
1063.703621	122.098447	49.238157
1059.978275	116.711673	49.243162
1056.724969	124.136511	49.248167
1053.487752	110.732517	49.253172
1049.571557	114.082864	49.258177
1046.250813	120.381656	49.263181
1042.887908	117.007566	49.268186
1038.707284	118.204674	49.273191
1035.754291	116.672971	49.278196
1032.022857	122.197896	49.283201
1028.601004	119.531180	49.288205
1025.350720	115.913850	49.293210
1021.447884	116.130497	49.298215
1018.396075	116.916133	49.303220
1014.634318	124.348417	49.308225
1010.824562	114.657220	49.313229
1007.635147	116.272405	49.318234
1004.012183	125.390391	49.323239
1000.588103	117.495084	49.328244
997.244555	120.050307	49.333249
993.826479	119.026797	49.338253
990.123725	102.937045	49.343258
986.462169	109.189036	49.348263
983.293142	114.929301	49.353268
979.342560	114.854360	49.358273
975.575107	107.057114	49.363277
972.298967	112.458184	49.368282
968.842272	116.122681	49.373287
965.723179	106.131817	49.378292
962.245349	111.199127	49.383297
958.960732	114.930584	49.388301
955.464526	116.182323	49.393306
951.497707	112.842634	49.398311
948.222912	112.207224	49.403316
944.343192	117.919245	49.408321
940.892545	113.240626	49.413325
937.614866	105.847382	49.418330
934.046564	107.572869	49.423335
931.172764	113.029347	49.428340
927.045192	108.904726	49.433345
923.191550	116.099553	49.438349
919.963062	111.079990	49.443354
916.091793	109.823729	49.448359
912.916746	109.202776	49.453364
909.438477	118.744773	49.458369
906.416975	111.898672	49.463373
902.804954	112.127161	49.468378
899.015190	117.827451	49.473383
895.649253	108.289458	49.478388
891.985475	113.282710	49.483393
888.193249	119.362105	49.488397
885.006833	103.748779	49.493402
881.397138	113.013450	49.498407
878.401573	106.510577	49.503412
874.793327	116.274272	49.508417
870.863202	109.270979	49.513421
867.388722	113.269445	49.518426
863.793846	109.466932	49.523431
860.486744	118.333299	49.528436
857.061600	114.463348	49.533441
853.668290	109.172241	49.538445
850.411530	107.977439	49.543450
846.440055	113.469164	49.548455
842.667578	102.994472	49.553460
839.261015	103.569970	49.558465
836.056907	111.272347	49.563469
832.792048	110.056210	49.568474
828.794123	105.895578	49.573479
825.228972	102.131584	49.578484
821.864510	113.702892	49.583489
818.111090	113.329776	49.588493
815.038132	104.969073	49.593498
811.408458	109.999557	49.598503
808.354173	98.441312	49.603508
804.475144	115.438515	49.608513
800.952375	111.055572	49.613517
797.771215	104.727435	49.618522
793.749325	110.425506	49.623527
790.311355	99.649466	49.628532
786.954965	108.590370	49.633537
783.045762	111.253489	49.638541
779.975356	104.048380	49.643546
776.264601	108.284862	49.648551
773.200131	100.381593	49.653556
769.403528	110.743386	49.658561
765.753232	116.289024	49.663565
762.578402	106.310955	49.668570
758.931555	117.692786	49.673575
755.725420	119.652933	49.678580
751.928492	111.307095	49.683585
748.479401	119.657412	49.688589
745.179011	115.258915	49.693594
741.122707	113.598429	49.698599
737.730462	102.747953	49.703604
733.907960	112.845309	49.708609
730.690813	109.118548	49.713613
727.502902	106.338483	49.718618
723.533813	108.769671	49.723623
720.321359	101.512028	49.728628
717.332475	108.939198	49.733633
713.423806	112.962128	49.738637
709.693055	111.690247	49.743642
706.193733	112.399467	49.748647
703.084319	102.617402	49.753652
699.039472	108.921248	49.758657
695.551607	105.606310	49.763661
692.104656	111.736501	49.768666
688.456215	112.709861	49.773671
685.354126	110.939156	49.778676
681.916182	117.700516	49.783681
678.090443	108.584809	49.788685
675.025942	105.881586	49.793690
671.420725	112.903579	49.798695
667.927588	109.888504	49.803700
664.229414	110.513168	49.808705
660.925958	118.448455	49.813709
657.529981	108.282439	49.818714
653.982905	113.043408	49.823719
650.101108	105.861841	49.828724
646.296474	103.884588	49.833729
643.022061	112.171844	49.838733
639.966393	103.916568	49.843738
636.348379	116.474955	49.848743
632.854873	113.790311	49.853748
629.174462	106.603546	49.858753
625.719835	112.356778	49.863757
622.403837	96.224151	49.868762
619.069825	112.941565	49.873767
615.334828	107.480291	49.878772
611.586407	115.413135	49.883777
608.150645	111.090327	49.888781
604.424998	113.651710	49.893786
600.988417	112.549144	49.898791
598.038709	112.814956	49.903796
594.217281	109.568923	49.908801
590.552819	122.154206	49.913805
587.512032	108.469023	49.918810
584.005696	116.901401	49.923815
580.305326	116.618971	49.928820
576.698148	102.575174	49.933825
572.681569	111.383555	49.938829
569.700744	106.214451	49.943834
565.954626	111.809136	49.948839
562.897622	103.919022	49.953844
559.520219	107.977212	49.958849
555.780875	105.243485	49.963853
552.471925	107.247513	49.968858
548.278556	103.836758	49.973863
544.930835	103.479816	49.978868
541.821901	106.445396	49.983873
538.151785	109.025641	49.988877
534.983745	102.689645	49.993882
530.791531	102.978532	49.998887
527.373704	106.142436	50.003892
524.026523	108.140998	50.008897
520.781569	103.649047	50.013901
517.464626	98.381891	50.018906
513.879965	107.233838	50.023911
510.352654	105.698675	50.028916
506.530705	111.112425	50.033921
503.162573	113.521387	50.038925
499.461455	107.329406	50.043930
495.846614	109.509198	50.048935
492.404907	106.239280	50.053940
488.880384	107.552978	50.058945
485.305036	109.439100	50.063949
482.134048	109.021485	50.068954
478.539865	102.747239	50.073959
475.051218	99.709899	50.078964
471.669900	113.066788	50.083969
468.206389	107.132167	50.088973
464.696589	105.329514	50.093978
461.156438	112.717399	50.098983
457.998532	100.201862	50.103988
454.354094	102.959073	50.108993
450.597770	117.164841	50.113997
447.144881	106.998427	50.119002
443.174450	107.494676	50.124007
440.140249	109.056920	50.129012
436.869377	107.053189	50.134017
433.124764	113.228108	50.139021
429.500390	105.139509	50.144026
425.893207	105.447569	50.149031
422.669581	102.845582	50.154036
418.730536	105.395031	50.159041
415.385389	104.895500	50.164045
412.262742	100.687227	50.169050
408.464397	106.789396	50.174055
404.920381	101.228740	50.179060
401.763339	105.470686	50.184065
397.780313	100.152471	50.189069
394.773058	101.859064	50.194074
391.105949	110.493934	50.199079
387.477757	108.395090	50.204084
383.765213	100.622911	50.209089
380.724514	102.531023	50.214093
376.967328	96.705861	50.219098
373.255950	107.392276	50.224103
369.707300	110.261331	50.229108
366.777961	94.874012	50.234113
363.361158	107.761300	50.239117
359.911287	95.808615	50.244122
356.077830	112.261678	50.249127
352.403885	111.961864	50.254132
349.155257	104.727940	50.259137
345.298192	101.670824	50.264141
342.180940	93.920570	50.269146
338.555590	105.416196	50.274151
334.861247	90.249731	50.279156
331.358393	100.272241	50.284161
327.506596	97.207560	50.289165
324.548258	92.370402	50.294170
320.636875	103.023981	50.299175
317.699190	102.662863	50.304180
314.172328	91.390994	50.309185
310.627731	89.784699	50.314189
306.937202	97.956638	50.319194
303.249136	111.332450	50.324199
299.686552	93.876376	50.329204
296.073243	104.980304	50.334209
292.677941	97.491777	50.339213
289.715839	102.945020	50.344218
285.744361	97.326251	50.349223
282.596663	98.060522	50.354228
278.909669	104.182596	50.359233
275.153969	100.727663	50.364237
271.675959	100.894827	50.369242
268.107952	102.099331	50.374247
264.854565	99.341801	50.379252
261.902772	100.152666	50.384257
258.147566	95.226551	50.389261
254.771905	102.694631	50.394266
250.597373	96.821138	50.399271
247.334298	94.018072	50.404276
243.987467	96.583561	50.409281
240.207303	105.544990	50.414285
237.155288	98.442691	50.419290
233.206448	93.521544	50.424295
229.887045	98.045952	50.429300
226.159980	101.687545	50.434305
222.750248	106.285973	50.439309
219.647604	93.525879	50.444314
215.846618	94.625682	50.449319
212.501941	93.568989	50.454324
208.925941	97.197337	50.459329
204.967019	95.712479	50.464333
201.996520	102.383544	50.469338
198.304887	101.312685	50.474343
194.555978	104.478617	50.479348
191.403227	100.163852	50.484353
187.773533	95.779751	50.489357
184.445709	94.040273	50.494362
180.775088	99.025841	50.499367
177.460802	88.513459	50.504372
173.734532	93.304828	50.509377
170.039522	105.954337	50.514381
166.840521	98.554083	50.519386
163.625790	96.177785	50.524391
160.049264	93.326838	50.529396
156.523210	98.202566	50.534401
152.576699	102.958727	50.539405
149.649125	101.211180	50.544410
145.925536	97.565556	50.549415
142.318681	93.658607	50.554420
138.648096	96.904916	50.559425
135.073997	94.045500	50.564429
131.734973	91.601679	50.569434
128.177088	93.698946	50.574439
124.441026	93.961623	50.579444
121.151220	93.800074	50.584449
117.480137	93.840419	50.589453
114.580990	94.442359	50.594458
110.993160	98.734028	50.599463
107.361571	84.896506	50.604468
103.689791	92.844499	50.609473
100.355789	97.324084	50.614477
96.687827	93.306767	50.619482
93.185373	103.936410	50.624487
89.574875	97.140574	50.629492
86.509848	99.709886	50.634497
82.552354	96.481883	50.639501
78.839894	90.982118	50.644506
75.237220	100.324060	50.649511
72.031986	96.237364	50.654516
68.939264	91.457095	50.659521
65.474231	93.787037	50.664525
61.997445	86.818645	50.669530
58.134054	93.616898	50.674535
54.973172	95.806711	50.679540
51.156314	89.002198	50.684545
47.414242	96.266922	50.689549
44.165428	89.371558	50.694554
40.753446	92.748633	50.699559
37.241806	88.771900	50.704564
34.006170	87.489852	50.709569
29.695328	97.958102	50.714573
26.535455	98.452092	50.719578
23.415434	96.588438	50.724583
19.814724	99.433911	50.729588
16.470274	89.562117	50.734593
12.786730	94.271159	50.739597
9.167559	95.179930	50.744602
5.402571	96.626401	50.749607
1.784675	92.959613	50.754612