Fri Jun 17 17:14:25 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.316959	84.514768	0.000000
0.443724	87.723235	0.005005
0.499312	100.288196	0.010010
0.485627	78.072858	0.015014
0.517705	81.491039	0.020019
0.412362	77.280715	0.025024
0.083988	63.090115	0.030029
-0.236559	63.101170	0.035034
-0.122321	50.116114	0.040038
-0.301323	42.234653	0.045043
-1.085716	29.890934	0.050048
-1.059547	24.354602	0.055053
-1.199023	18.622427	0.060058
-1.801230	15.154191	0.065062
-2.719828	10.148848	0.070067
-2.987119	11.017927	0.075072
-3.220202	11.057264	0.080077
-3.364658	22.945417	0.085082
-3.427219	14.990547	0.090086
-3.474971	6.342166	0.095091
-3.930171	15.492298	0.100096
-4.184728	11.618381	0.105101
-4.699135	18.866219	0.110106
-4.269223	18.409964	0.115110
-4.312488	6.481983	0.120115
-5.366313	21.248013	0.125120
-5.734023	6.720056	0.130125
-6.172261	14.161245	0.135130
-6.192674	5.339207	0.140134
-6.384496	4.741609	0.145139
-6.825479	11.705909	0.150144
-6.312245	12.738480	0.155149
-6.431819	13.789018	0.160154
-7.011974	16.586918	0.165158
-7.190889	11.143881	0.170163
-7.803470	14.952572	0.175168
-7.606773	10.998713	0.180173
-8.658932	19.913601	0.185178
-8.947746	5.764826	0.190182
-9.424198	5.887834	0.195187
-9.675453	17.487082	0.200192
-8.910964	14.800228	0.205197
-9.608240	13.290719	0.210202
-9.966479	16.723052	0.215206
-9.458315	19.985320	0.220211
-9.813632	16.751323	0.225216
-9.988685	11.056836	0.230221
-11.052805	20.052251	0.235226
-11.163207	23.038465	0.240230
-11.276128	14.333623	0.245235
-11.208153	22.511370	0.250240
-11.504599	6.183157	0.255245
-12.236386	21.328206	0.260250
-12.446026	18.161358	0.265254
-12.579568	11.285456	0.270259
-13.030969	21.589150	0.275264
-12.625961	12.632063	0.280269
-12.922955	27.033327	0.285274
-13.641853	20.900785	0.290278
-14.305882	18.924586	0.295283
-14.765443	20.018024	0.300288
-14.281190	9.128327	0.305293
-14.539701	17.344160	0.310298
-14.349296	8.842274	0.315302
-14.464468	12.505336	0.320307
-15.102275	16.687231	0.325312
-15.793540	10.104921	0.330317
-15.815143	16.517629	0.335322
-15.751446	12.310009	0.340326
-15.811165	20.200749	0.345331
-16.503831	20.541835	0.350336
-17.017205	10.775223	0.355341
-17.343237	11.314263	0.360346
-17.247815	10.834478	0.365350
-17.100973	15.895292	0.370355
-17.633231	20.035569	0.375360
-17.820330	14.060506	0.380365
-18.797606	20.400013	0.385370
-19.072989	24.455560	0.390374
-19.241714	21.657235	0.395379
-19.133059	19.030458	0.400384
-19.129287	17.370476	0.405389
-18.949034	14.652274	0.410394
-19.282535	26.831343	0.415398
-19.836405	18.646556	0.420403
-20.691315	18.007434	0.425408
-20.713872	13.396598	0.430413
-20.818326	17.451554	0.435418
-21.130652	14.179827	0.440422
-21.050089	14.469735	0.445427
-21.139982	18.843329	0.450432
-21.526857	5.431313	0.455437
-21.790807	13.592598	0.460442
-22.320412	9.259435	0.465446
-22.246426	11.839870	0.470451
-23.013838	20.602843	0.475456
-23.197253	7.137272	0.480461
-23.657109	20.542440	0.485466
-23.969611	17.545821	0.490470
-23.475964	14.445192	0.495475
-24.223149	23.584074	0.500480
-23.901479	13.447578	0.505485
-24.380070	21.671779	0.510490
-25.054827	17.311831	0.515494
-25.231233	23.282007	0.520499
-25.879752	21.375061	0.525504
-25.503568	15.281303	0.530509
-25.585024	27.975936	0.535514
-25.823850	15.343625	0.540518
-25.761706	9.647993	0.545523
-26.593176	24.693586	0.550528
-27.193222	19.369095	0.555533
-26.876131	23.515594	0.560538
-27.435567	14.848866	0.565542
-26.879021	14.904549	0.570547
-27.693460	16.942009	0.575552
-28.255869	12.465511	0.580557
-28.580665	21.394271	0.585562
-28.809383	18.391816	0.590566
-28.705420	11.995613	0.595571
-28.913123	20.951676	0.600576
-28.846305	14.246903	0.605581
-29.585378	22.639118	0.610586
-29.976300	20.824327	0.615590
-29.748868	8.626985	0.620595
-30.270817	15.751166	0.625600
-30.150703	9.819757	0.630605
-30.752236	10.922391	0.635610
-31.336253	17.780825	0.640614
-31.609256	18.580408	0.645619
-31.843433	10.107069	0.650624
-31.431010	13.026697	0.655629
-31.722212	16.462885	0.660634
-32.158968	20.478756	0.665638
-32.718234	12.541141	0.670643
-33.035353	19.443811	0.675648
-33.214714	17.436383	0.680653
-33.481326	15.909159	0.685658
-33.405187	14.899983	0.690662
-33.414701	15.148625	0.695667
-34.119962	15.181209	0.700672
-34.468705	9.578349	0.705677
-34.578855	11.085721	0.710682
-34.664788	16.823002	0.715686
-34.554143	12.766627	0.720691
-35.380413	19.039200	0.725696
-35.652664	6.880524	0.730701
-36.026619	21.258857	0.735706
-36.292282	27.253936	0.740710
-36.275022	16.666820	0.745715
-36.454971	17.793699	0.750720
-36.378139	12.535673	0.755725
-37.270688	23.336173	0.760730
-37.673864	18.375003	0.765734
-37.659306	16.996990	0.770739
-38.044086	22.529000	0.775744
-37.831686	18.386050	0.780749
-38.107473	15.747208	0.785754
-38.472087	26.531187	0.790758
-38.819777	17.108806	0.795763
-39.521129	24.679973	0.800768
-39.422346	9.498466	0.805773
-39.518797	20.625224	0.810778
-39.486164	18.075612	0.815782
-39.695305	11.329100	0.820787
-40.433254	23.205008	0.825792
-40.820086	11.074059	0.830797
-40.935935	19.945194	0.835802
-41.270685	23.852351	0.840806
-41.165543	12.141826	0.845811
-41.354530	24.731985	0.850816
-41.523001	18.066522	0.855821
-42.139924	21.450101	0.860826
-42.750162	31.971617	0.865830
-42.316237	11.542613	0.870835
-43.116682	30.213551	0.875840
-42.901265	18.293081	0.880845
-42.517205	16.193375	0.885850
-43.717883	25.887753	0.890854
-44.046474	15.995314	0.895859
-44.716130	22.568636	0.900864
-44.204359	18.769398	0.905869
-44.479302	9.752087	0.910874
-44.525061	24.318188	0.915878
-44.874933	12.787098	0.920883
-45.781055	24.079435	0.925888
-45.927873	22.656025	0.930893
-46.046383	17.342066	0.935898
-46.223247	17.964843	0.940902
-46.286725	16.222901	0.945907
-46.452977	15.472859	0.950912
-46.265649	21.490903	0.955917
-47.209873	16.679665	0.960922
-47.781450	17.241963	0.965926
-47.768195	12.083503	0.970931
-47.848179	23.201999	0.975936
-47.855987	23.743395	0.980941
-48.003972	17.696712	0.985946
-48.974164	20.919586	0.990950
-49.095102	17.369382	0.995955
-49.464241	20.339408	1.000960
-49.585295	18.884286	1.005965
-49.555896	18.034627	1.010970
-50.175423	19.334430	1.015974
-49.665676	10.265411	1.020979
-49.803054	23.314662	1.025984
-50.448911	25.509595	1.030989
-50.781834	17.405301	1.035994
-51.239878	20.505742	1.040998
-51.188304	10.352582	1.046003
-51.984202	16.122834	1.051008
-51.713306	19.224641	1.056013
-52.545126	14.214754	1.061018
-52.927138	23.275371	1.066022
-52.555864	7.267337	1.071027
-52.876877	22.362849	1.076032
-52.862723	12.324638	1.081037
-52.802941	19.464399	1.086042
-53.312012	17.412327	1.091046
-53.946921	2.720028	1.096051
-54.221048	11.990820	1.101056
-54.426353	11.606807	1.106061
-54.367692	11.491880	1.111066
-54.483515	23.533528	1.116070
-55.085493	10.738217	1.121075
-55.478284	24.630500	1.126080
-55.674536	17.884015	1.131085
-55.697684	21.210723	1.136090
-55.626326	24.873167	1.141094
-56.171080	23.835784	1.146099
-56.908630	20.830894	1.151104
-57.201254	20.096137	1.156109
-57.031765	15.724314	1.161114
-57.638329	27.471432	1.166118
-57.395713	20.665211	1.171123
-57.724915	20.051184	1.176128
-57.960014	23.259997	1.181133
-58.511892	18.962902	1.186138
-59.128612	29.166214	1.191142
-58.783661	22.973650	1.196147
-59.007848	22.119181	1.201152
-58.818118	15.525597	1.206157
-59.625293	17.979212	1.211162
-60.329184	13.224718	1.216166
-60.320118	17.608104	1.221171
-60.636587	20.086506	1.226176
-60.731942	9.112801	1.231181
-60.481587	12.309188	1.236186
-60.882325	20.682061	1.241190
-61.194395	18.095034	1.246195
-61.889963	18.959143	1.251200
-62.277780	30.454414	1.256205
-61.706742	18.926123	1.261210
-62.394378	16.086787	1.266214
-61.858362	10.953904	1.271219
-63.042769	16.659886	1.276224
-63.365043	7.164422	1.281229
-63.517448	17.105837	1.286234
-63.860139	26.719945	1.291238
-63.842839	22.143923	1.296243
-63.846558	15.851855	1.301248
-64.352170	25.231188	1.306253
-64.976873	24.226632	1.311258
-65.368520	24.593264	1.316262
-65.313331	16.948367	1.321267
-65.401310	21.973427	1.326272
-65.277989	23.931566	1.331277
-65.361931	11.653183	1.336282
-66.248072	29.596008	1.341286
-66.655719	12.976478	1.346291
-67.058486	19.650275	1.351296
-67.190611	14.211698	1.356301
-66.992477	13.729243	1.361306
-67.048411	21.345061	1.366310
-66.694434	12.322063	1.371315
-67.806327	20.721598	1.376320
-67.964970	15.827525	1.381325
-68.384730	12.133616	1.386330
-68.715622	20.506323	1.391334
-68.510705	3.990984	1.396339
-69.920376	25.369145	1.401344
-70.151155	10.233352	1.406349
-69.804450	17.970881	1.411354
-70.317955	11.848810	1.416358
-70.254434	6.280033	1.421363
-70.314021	15.276587	1.426368
-70.367147	9.370033	1.431373
-70.211385	6.278606	1.436378
-70.948560	14.306232	1.441382
-71.365659	17.139786	1.446387
-71.727485	17.732929	1.451392
-71.737533	15.596916	1.456397
-71.701873	16.443657	1.461402
-72.572067	19.543748	1.466406
-72.838472	10.447471	1.471411
-73.420766	17.470393	1.476416
-73.164176	22.378577	1.481421
-73.151895	25.085695	1.486426
-73.485270	20.293287	1.491430
-73.421819	18.985290	1.496435
-74.451576	19.667568	1.501440
-74.879122	23.959558	1.506445
-75.114231	28.498780	1.511450
-75.210250	23.978301	1.516454
-74.930115	16.540699	1.521459
-75.241416	29.128894	1.526464
-75.116078	15.555167	1.531469
-76.064522	15.785459	1.536474
-76.679280	16.398945	1.541478
-76.542528	19.090106	1.546483
-76.750817	19.754023	1.551488
-76.905705	13.657779	1.556493
-76.578864	18.551322	1.561498
-77.372761	16.675462	1.566502
-77.858361	23.601801	1.571507
-78.409602	22.913986	1.576512
-78.446327	19.968417	1.581517
-78.321603	18.187492	1.586522
-78.533639	14.942708	1.591526
-78.912546	9.159774	1.596531
-78.890052	26.116830	1.601536
-79.195051	15.423455	1.606541
-79.558305	28.114807	1.611546
-80.083006	14.709925	1.616550
-79.893523	18.043116	1.621555
-80.294636	16.186022	1.626560
-80.747721	32.668239	1.631565
-81.162876	27.798850	1.636570
-81.450903	29.111430	1.641574
-81.445942	20.855263	1.646579
-81.508075	22.208037	1.651584
-81.613092	18.223033	1.656589
-81.525113	11.387863	1.661594
-82.947492	24.698294	1.666598
-83.006549	17.556247	1.671603
-83.173091	19.858964	1.676608
-83.439639	20.594529	1.681613
-83.174682	11.203509	1.686618
-83.204453	10.826231	1.691622
-83.689752	11.888830	1.696627
-84.652999	24.073527	1.701632
-84.803572	20.400775	1.706637
-84.493523	17.155234	1.711642
-85.148733	19.339689	1.716646
-84.944658	17.814929	1.721651
-85.061283	18.637259	1.726656
-85.848986	17.664542	1.731661
-86.090734	19.501432	1.736666
-86.468643	22.459303	1.741670
-86.440478	17.078340	1.746675
-86.640439	17.926365	1.751680
-86.551858	15.928662	1.756685
-86.697261	16.569496	1.761690
-87.659690	23.385669	1.766694
-87.817052	22.332629	1.771699
-88.174259	20.137312	1.776704
-88.375845	20.573777	1.781709
-88.166366	12.452529	1.786714
-88.332771	13.915383	1.791718
-89.050216	14.539233	1.796723
-89.519272	20.738420	1.801728
-89.321809	17.079638	1.806733
-89.489972	15.135472	1.811738
-89.796072	17.007924	1.816742
-90.116324	13.795143	1.821747
-90.858446	14.108551	1.826752
-91.048828	34.646448	1.831757
-91.097886	11.400923	1.836762
-91.528411	16.434976	1.841766
-91.220717	16.098287	1.846771
-91.382585	16.765144	1.851776
-91.546154	17.132340	1.856781
-92.179242	16.520885	1.861786
-92.594096	22.744214	1.866790
-92.521970	18.507567	1.871795
-92.807884	18.885236	1.876800
-93.191467	21.193648	1.881805
-93.842924	10.393698	1.886810
-94.125029	17.467355	1.891814
-94.446138	18.761360	1.896819
-94.492664	14.371973	1.901824
-94.254334	18.455188	1.906829
-94.208829	7.573707	1.911834
-94.538764	29.592481	1.916838
-94.938873	20.513891	1.921843
-95.505071	14.129254	1.926848
-96.027495	14.927881	1.931853
-95.844509	12.099902	1.936858
-96.296593	22.653927	1.941862
-96.213577	20.451727	1.946867
-97.048549	25.983204	1.951872
-97.568207	14.928095	1.956877
-97.240330	23.943905	1.961882
-97.384352	15.156037	1.966886
-97.751470	17.460133	1.971891
-97.782335	7.559454	1.976896
-97.819123	12.705646	1.981901
-97.760090	9.769023	1.986906
-98.945295	17.704000	1.991910
-98.933809	7.871661	1.996915
-99.437231	14.427531	2.006912
-99.235868	12.471767	2.016909
-98.385426	12.626563	2.026906
-98.088902	8.244461	2.036902
-97.233331	8.957170	2.046899
-96.758581	15.490379	2.056896
-96.462814	9.058868	2.066893
-96.253251	14.843459	2.076890
-95.117084	18.578388	2.086886
-94.941860	19.434040	2.096883
-94.793630	18.950809	2.106880
-93.548978	23.768246	2.116877
-93.478809	24.122311	2.126874
-93.055046	13.525005	2.136870
-92.295767	23.532250	2.146867
-92.014052	24.963147	2.156864
-91.675192	22.052324	2.166861
-90.589568	15.052050	2.176858
-90.595301	15.849860	2.186854
-90.204982	19.456275	2.196851
-89.248492	27.644385	2.206848
-89.131070	21.365613	2.216845
-87.942376	22.547727	2.226842
-87.602564	21.087208	2.236838
-87.676404	15.953224	2.246835
-87.275855	24.550087	2.256832
-86.454392	25.500829	2.266829
-86.035881	24.167708	2.276826
-85.049267	19.390310	2.286822
-84.769228	18.578912	2.296819
-84.290169	15.117433	2.306816
-84.165660	18.908125	2.316813
-83.166542	17.601576	2.326810
-82.988241	23.094599	2.336806
-82.499864	17.363112	2.346803
-81.641483	14.575955	2.356800
-81.407814	11.706925	2.366797
-81.154081	21.639162	2.376794
-80.160246	19.725133	2.386790
-80.230410	17.657035	2.396787
-79.338972	14.404408	2.406784
-78.595272	22.188073	2.416781
-78.346082	13.407921	2.426778
-78.252315	19.940455	2.436774
-77.199822	18.142535	2.446771
-77.001982	23.803615	2.456768
-76.568959	20.999642	2.466765
-75.679282	17.564345	2.476762
-75.330930	14.082314	2.486758
-75.089383	18.490559	2.496755
-74.157737	17.083793	2.506752
-73.756529	12.889774	2.516749
-73.696756	11.404286	2.526746
-72.549353	10.824105	2.536742
-72.267939	15.321155	2.546739
-72.018008	20.473886	2.556736
-71.241144	17.741972	2.566733
-70.479523	14.428733	2.576730
-70.370841	13.411094	2.586726
-70.444647	13.973242	2.596723
-69.546720	15.689952	2.606720
-68.942191	18.373213	2.616717
-67.813006	14.719092	2.626714
-67.360731	25.026338	2.636710
-67.402815	18.170070	2.646707
-67.262037	20.692536	2.656704
-66.462455	20.697727	2.666701
-65.932961	23.788829	2.676698
-65.167861	24.521131	2.686694
-64.490435	29.115557	2.696691
-64.479395	25.941912	2.706688
-64.139530	15.829196	2.716685
-63.412938	16.667482	2.726682
-62.887715	13.762432	2.736678
-62.423787	14.435537	2.746675
-61.585082	19.209823	2.756672
-61.416990	15.241076	2.766669
-61.067526	14.917432	2.776666
-60.105641	20.940123	2.786662
-59.774969	20.928427	2.796659
-59.476153	24.695875	2.806656
-58.874986	18.443580	2.816653
-57.985225	22.381899	2.826650
-57.921052	20.320513	2.836646
-57.440098	23.381551	2.846643
-56.812984	24.877733	2.856640
-56.650117	22.750544	2.866637
-55.622980	30.447189	2.876634
-55.016458	27.944734	2.886630
-55.090908	24.033100	2.896627
-54.435485	26.178183	2.906624
-53.723844	27.328373	2.916621
-53.470741	28.357205	2.926618
-52.517529	19.740386	2.936614
-52.093324	22.388030	2.946611
-52.055914	20.228547	2.956608
-51.476841	16.284542	2.966605
-50.481619	16.530868	2.976602
-49.996603	21.631481	2.986598
-50.255520	21.782802	2.996595
-49.430694	20.950195	3.006592
-49.085840	23.006226	3.016589
-48.064984	21.563890	3.026586
-47.559430	17.642974	3.036582
-47.303382	11.823659	3.046579
-47.039535	16.912432	3.056576
-45.685892	20.205390	3.066573
-45.355827	19.234922	3.076570
-45.203468	18.162009	3.086566
-45.371598	19.663936	3.096563
-44.544588	13.636492	3.106560
-44.032204	13.786641	3.116557
-43.178932	18.552780	3.126554
-42.286985	9.219835	3.136550
-41.956534	12.956140	3.146547
-42.169339	11.082268	3.156544
-41.377353	16.691805	3.166541
-40.719192	21.330732	3.176538
-40.507133	18.316119	3.186534
-39.362995	18.538680	3.196531
-38.987123	18.764080	3.206528
-38.819494	19.850195	3.216525
-38.719413	21.331642	3.226522
-37.744387	18.039244	3.236518
-37.610773	15.606910	3.246515
-36.670200	17.790346	3.256512
-35.750366	18.912648	3.266509
-35.641471	12.804230	3.276506
-35.459284	15.205610	3.286502
-35.025360	21.757871	3.296499
-34.258229	22.983011	3.306496
-33.836962	20.066989	3.316493
-32.933184	16.090152	3.326490
-32.661906	25.640123	3.336486
-32.223292	25.737335	3.346483
-32.065289	18.531668	3.356480
-31.175589	19.572637	3.366477
-30.706768	13.763002	3.376474
-30.695574	19.320162	3.386470
-29.854993	13.324449	3.396467
-29.092685	18.210432	3.406464
-28.311528	9.749862	3.416461
-27.834957	10.454656	3.426458
-27.553754	12.341864	3.436454
-27.867090	14.223578	3.446451
-26.989081	12.203351	3.456448
-26.354038	18.341634	3.466445
-25.771413	11.226417	3.476442
-24.821557	10.967956	3.486438
-24.620478	8.933012	3.496435
-24.405149	12.678775	3.506432
-23.692562	18.026281	3.516429
-23.320062	20.531372	3.526426
-22.921471	15.198721	3.536422
-21.920527	17.751881	3.546419
-21.538274	18.931145	3.556416
-21.670798	15.108988	3.566413
-20.574847	18.583693	3.576410
-19.888515	16.835986	3.586406
-19.780668	22.093351	3.596403
-19.573494	24.117147	3.606400
-18.575170	26.187257	3.616397
-18.227282	17.818662	3.626394
-17.989699	16.190994	3.636390
-17.064594	12.520229	3.646387
-16.763568	19.775260	3.656384
-16.310828	20.781184	3.666381
-15.108525	18.438536	3.676378
-15.015049	16.020580	3.686374
-15.134668	24.172226	3.696371
-14.266266	17.599686	3.706368
-13.431395	21.497746	3.716365
-13.147802	17.879282	3.726362
-12.975785	13.955327	3.736358
-11.926579	18.066912	3.746355
-11.709591	7.157222	3.756352
-11.564641	9.830148	3.766349
-10.356315	11.218659	3.776346
-10.094113	11.845282	3.786342
-9.936011	17.164633	3.796339
-9.599902	15.784362	3.806336
-8.632646	17.631034	3.816333
-8.191634	19.310101	3.826330
-7.179330	17.907726	3.836326
-6.961286	15.171305	3.846323
-7.040809	14.268924	3.856320
-6.797723	13.770323	3.866317
-6.023769	17.817412	3.876314
-4.855485	14.621130	3.886310
-4.060274	17.848863	3.896307
-3.961933	15.751567	3.906304
-4.057828	20.924447	3.916301
-3.660543	23.239693	3.926298
-3.098917	31.089411	3.936294
-2.567915	40.518377	3.946291
-2.179567	52.378624	3.956288
-1.444787	67.625192	3.966285
-0.862734	77.833859	3.976282
-0.673666	90.997138	3.986278
-0.408378	108.581564	3.996275
0.000000	118.994025	4.001280
0.347704	135.189130	4.006285
0.833497	138.336942	4.011290
0.767017	151.027215	4.016294
0.969359	140.451081	4.021299
0.945249	152.738859	4.026304
0.951389	154.206589	4.031309
1.240716	150.774042	4.036314
0.688363	153.460982	4.041318
0.926714	156.276377	4.046323
1.321250	156.675912	4.051328
1.248114	156.588220	4.056333
0.983005	158.299950	4.061338
0.775988	153.535030	4.066342
1.194842	164.894341	4.071347
1.281560	175.698319	4.076352
1.433649	175.711126	4.081357
1.424844	153.138289	4.086362
1.028851	147.229468	4.091366
0.840936	143.099352	4.096371
0.994115	165.122289	4.101376
0.838334	172.580340	4.106381
1.215247	167.705724	4.111386
1.202223	180.302875	4.116390
1.518214	173.884779	4.121395
1.518068	180.560389	4.126400
1.558728	179.769233	4.131405
1.579322	175.804348	4.136410
1.086139	176.775709	4.141414
1.611887	173.428377	4.146419
1.384844	174.382336	4.151424
1.121937	176.912831	4.156429
1.094100	172.623689	4.161434
1.103177	181.953476	4.166438
1.278709	168.989705	4.171443
1.346436	177.232302	4.176448
1.142602	182.352054	4.181453
1.473498	179.090586	4.186458
1.544752	188.382612	4.191462
1.426658	173.913250	4.196467
1.375804	180.515199	4.201472
1.532614	183.289294	4.206477
1.416805	182.463960	4.211482
1.432363	183.893028	4.216486
1.578887	179.867152	4.221491
1.354543	193.838938	4.226496
1.464202	186.671917	4.231501
1.437506	178.734286	4.236506
1.336518	183.433595	4.241510
1.475533	201.497473	4.246515
1.836638	208.585464	4.251520
1.538128	197.428910	4.256525
1.550576	191.098954	4.261530
1.758131	212.435868	4.266534
1.811835	196.038198	4.271539
1.691190	189.909741	4.276544
1.632923	180.883341	4.281549
2.154659	181.538987	4.286554
1.602273	182.193602	4.291558
1.445079	179.001426	4.296563
1.715954	185.939828	4.301568
1.633640	199.918992	4.306573
1.743974	201.801173	4.311578
1.748387	207.485028	4.316582
1.937704	209.931282	4.321587
2.086864	218.060316	4.326592
1.496492	203.842885	4.331597
1.346604	202.531262	4.336602
1.370752	204.853615	4.341606
1.737859	208.922984	4.346611
1.699318	214.935439	4.351616
1.814014	214.686285	4.356621
1.765164	209.778037	4.361626
1.890864	209.005107	4.366630
2.002407	209.056424	4.371635
2.060436	210.727668	4.376640
1.713335	216.595657	4.381645
1.770677	207.317171	4.386650
1.814350	212.032698	4.391654
1.892006	209.707634	4.396659
1.896656	217.270267	4.401664
1.568195	217.120429	4.406669
2.013260	214.349689	4.411674
1.828725	226.201444	4.416678
2.226610	232.723496	4.421683
2.316917	233.613855	4.426688
2.110463	228.312859	4.431693
2.185364	216.731326	4.436698
2.093028	220.791819	4.441702
2.077410	216.854256	4.446707
2.082351	217.581203	4.451712
1.720137	211.333051	4.456717
2.024271	226.396879	4.461722
1.958943	235.103651	4.466726
2.433548	235.863630	4.471731
2.132516	239.559020	4.476736
2.205587	250.735913	4.481741
2.395656	243.408684	4.486746
2.141484	245.653380	4.491750
2.113194	237.094184	4.496755
1.893408	241.761161	4.501760
1.947160	248.153744	4.506765
2.392924	252.640634	4.511770
2.337967	245.952449	4.516774
2.711720	245.070402	4.521779
2.449164	248.187328	4.526784
2.159746	243.399372	4.531789
2.476506	243.171489	4.536794
2.018796	242.833369	4.541798
2.301391	243.526597	4.546803
2.640569	243.069040	4.551808
2.123707	254.171131	4.556813
2.488408	245.100040	4.561818
2.174666	243.430059	4.566822
2.159350	246.230409	4.571827
2.444798	243.241897	4.576832
2.275241	256.061476	4.581837
2.167023	243.894678	4.586842
2.033804	251.701850	4.591846
2.355469	245.641732	4.596851
2.324212	254.368110	4.601856
2.364122	257.911126	4.606861
2.597125	257.959817	4.611866
2.346240	256.504149	4.616870
2.330934	257.850147	4.621875
2.759259	269.734251	4.626880
2.554782	270.070361	4.631885
2.689269	267.495094	4.636890
2.671952	264.853498	4.641894
2.482454	251.287686	4.646899
2.889523	251.091165	4.651904
2.489596	257.213236	4.656909
2.873765	249.983192	4.661914
2.368144	258.281076	4.666918
2.446401	254.086559	4.671923
3.114129	263.621069	4.676928
2.724930	268.516310	4.681933
2.750999	256.416573	4.686938
2.295758	254.095426	4.691942
2.590971	257.256787	4.696947
2.652160	278.282259	4.701952
2.757003	291.525123	4.706957
2.987011	278.206081	4.711962
2.414571	282.861043	4.716966
3.108137	279.146575	4.721971
3.079200	286.755476	4.726976
2.678300	275.165765	4.731981
2.947258	270.942308	4.736986
2.873211	268.396573	4.741990
2.824491	263.130125	4.746995
2.632596	261.509547	4.752000
2.621515	283.314867	4.757005
3.140479	279.221729	4.762010
2.681564	289.339775	4.767014
2.952111	288.944142	4.772019
2.885106	282.603872	4.777024
2.958664	286.808095	4.782029
3.008375	293.089282	4.787034
2.717191	297.210870	4.792038
2.880117	286.242177	4.797043
3.031119	291.582410	4.802048
2.985992	297.660125	4.807053
3.282770	285.981077	4.812058
3.407330	294.451485	4.817062
2.860712	287.640174	4.822067
2.970121	281.492385	4.827072
2.832999	293.293883	4.832077
3.038994	292.694280	4.837082
2.919557	288.891961	4.842086
3.253276	294.628461	4.847091
3.014510	287.119904	4.852096
2.963698	300.053180	4.857101
2.939992	287.265299	4.862106
2.469854	292.164924	4.867110
2.495466	290.991067	4.872115
2.787883	296.790475	4.877120
2.558218	321.699553	4.882125
3.157278	313.603176	4.887130
2.946260	324.009193	4.892134
3.080759	323.975591	4.897139
3.486377	316.227103	4.902144
3.187871	325.685262	4.907149
3.531859	315.223993	4.912154
3.243428	327.164924	4.917158
3.237213	321.451926	4.922163
3.116431	321.605403	4.927168
3.211294	335.099197	4.932173
3.563591	324.839598	4.937178
3.335567	322.638342	4.942182
3.460785	313.963998	4.947187
3.628596	317.978710	4.952192
3.279853	326.489328	4.957197
3.351276	308.826438	4.962202
3.123348	315.914511	4.967206
3.244814	320.278513	4.972211
3.245831	315.599535	4.977216
3.429607	319.247313	4.982221
3.441376	319.062232	4.987226
3.132155	335.482183	4.992230
3.303863	315.845445	4.997235
3.463213	322.286219	5.002240
3.494529	327.979460	5.007245
3.691083	324.578479	5.012250
3.488990	320.660834	5.017254
3.482150	323.888598	5.022259
3.292741	317.062298	5.027264
3.526236	338.912291	5.032269
3.891859	348.273094	5.037274
3.643376	347.970641	5.042278
3.620731	322.224337	5.047283
3.442440	326.531015	5.052288
3.431575	347.049764	5.057293
3.626952	355.824171	5.062298
3.450445	355.830819	5.067302
3.661492	358.610336	5.072307
3.899804	354.614742	5.077312
4.001305	363.809098	5.082317
4.079893	343.764124	5.087322
3.826085	334.582471	5.092326
3.769663	326.915910	5.097331
3.814847	325.825624	5.102336
3.556308	330.368433	5.107341
3.733515	315.031307	5.112346
3.683642	317.747430	5.117350
3.725030	311.536145	5.122355
3.710814	321.943784	5.127360
3.777408	340.537276	5.132365
4.219240	343.312568	5.137370
3.560661	332.819613	5.142374
3.694276	344.039396	5.147379
3.978796	343.738923	5.152384
4.104315	348.839505	5.157389
3.713264	330.155490	5.162394
3.827020	343.484731	5.167398
3.990749	341.533697	5.172403
3.916163	343.002233	5.177408
3.843700	352.925251	5.182413
4.060061	351.650615	5.187418
3.818994	351.784422	5.192422
3.943739	346.703418	5.197427
3.957814	345.743412	5.202432
3.603556	365.485917	5.207437
3.898387	356.438610	5.212442
3.950602	358.446307	5.217446
4.160635	354.289060	5.222451
3.939431	357.742694	5.227456
3.599938	370.623372	5.232461
3.835420	349.012108	5.237466
3.985747	354.096136	5.242470
4.086972	355.234119	5.247475
4.272094	355.244790	5.252480
3.729778	354.382596	5.257485
3.995538	356.126282	5.262490
3.781549	360.160068	5.267494
3.650315	367.675899	5.272499
4.008566	370.299524	5.277504
3.744540	384.114091	5.282509
4.078529	378.731892	5.287514
4.376019	391.079278	5.292518
4.084498	395.547865	5.297523
4.289982	389.809322	5.302528
4.215446	398.077262	5.307533
4.382255	385.064045	5.312538
4.303534	398.392175	5.317542
4.254411	395.496149	5.322547
4.394652	395.237418	5.327552
4.352061	403.388754	5.332557
4.524817	381.366164	5.337562
4.257079	395.046775	5.342566
4.236416	394.277444	5.347571
4.340694	395.106487	5.352576
4.343664	393.862976	5.357581
4.438898	384.891454	5.362586
4.353867	394.191230	5.367590
4.608094	392.784001	5.372595
4.731239	388.850166	5.377600
4.499357	390.414316	5.382605
4.360107	374.419916	5.387610
4.460992	391.422374	5.392614
4.161040	383.244119	5.397619
4.479070	379.498316	5.402624
4.235975	390.057316	5.407629
4.229267	374.538764	5.412634
4.137505	384.442908	5.417638
4.661070	378.342469	5.422643
4.583091	382.232686	5.427648
4.245310	391.558883	5.432653
4.372176	382.945992	5.437658
4.704174	409.041177	5.442662
4.964518	409.240036	5.447667
4.683632	390.558159	5.452672
4.304000	391.986237	5.457677
4.813401	391.517353	5.462682
4.855079	399.736968	5.467686
4.444193	392.237631	5.472691
4.444978	390.467795	5.477696
4.435461	408.944962	5.482701
4.756304	415.007278	5.487706
4.588372	414.491138	5.492710
4.719029	418.520932	5.497715
4.743861	416.290656	5.502720
4.560002	420.718858	5.507725
4.992482	413.365069	5.512730
4.985767	418.802602	5.517734
5.101903	420.052370	5.522739
5.096596	416.800561	5.527744
4.563181	402.447578	5.532749
4.706600	403.770164	5.537754
4.704836	416.094693	5.542758
4.780618	418.049738	5.547763
4.790187	413.843310	5.552768
4.885535	418.290024	5.557773
4.824781	406.153492	5.562778
4.752504	421.869719	5.567782
4.473100	425.727320	5.572787
4.733996	414.696272	5.577792
4.700506	423.287547	5.582797
4.778359	418.106766	5.587802
4.700677	425.865129	5.592806
4.723575	416.492588	5.597811
4.664687	418.797005	5.602816
5.179424	438.384106	5.607821
5.101024	436.037588	5.612826
4.968082	446.138651	5.617830
4.951203	446.190201	5.622835
5.628259	437.608570	5.627840
5.087796	439.687757	5.632845
5.213463	426.337387	5.637850
4.786012	427.627782	5.642854
4.815508	424.405510	5.647859
5.170496	429.899945	5.652864
5.051903	448.798449	5.657869
5.202636	437.600200	5.662874
5.397053	442.076630	5.667878
4.976623	436.725288	5.672883
5.419669	436.868520	5.677888
4.915851	436.669089	5.682893
5.444498	432.623439	5.687898
5.343141	432.922085	5.692902
5.340614	425.616917	5.697907
5.234533	422.041453	5.702912
4.966588	416.849873	5.707917
5.296044	429.529618	5.712922
5.295641	440.752409	5.717926
5.426570	435.418152	5.722931
5.478908	427.806675	5.727936
4.996420	420.389478	5.732941
5.198834	428.419194	5.737946
5.401710	443.421131	5.742950
5.424072	441.416029	5.747955
5.520500	444.387481	5.752960
5.353831	447.071929	5.757965
5.425714	443.103582	5.762970
5.515061	451.366411	5.767974
5.212493	442.352444	5.772979
5.234702	438.979431	5.777984
5.491448	442.232276	5.782989
5.676583	450.220277	5.787994
5.366200	443.613143	5.792998
5.255629	449.079395	5.798003
5.293039	443.620966	5.803008
5.636664	441.709282	5.808013
5.658600	437.791665	5.813018
5.403737	451.469002	5.818022
5.222137	447.517528	5.823027
5.361338	445.797495	5.828032
5.464383	449.294736	5.833037
5.508548	441.596204	5.838042
5.483275	455.164931	5.843046
5.302763	439.171601	5.848051
5.627039	443.393392	5.853056
5.649174	448.127569	5.858061
5.384400	447.403745	5.863066
5.582619	448.997445	5.868070
5.292310	440.914449	5.873075
5.708245	432.890680	5.878080
5.630100	464.212706	5.883085
5.590802	460.018334	5.888090
5.754436	459.653297	5.893094
5.596513	475.786381	5.898099
5.586238	472.387778	5.903104
5.505276	481.437101	5.908109
5.856229	482.333089	5.913114
5.757255	478.701571	5.918118
5.838759	481.580789	5.923123
6.148442	489.366558	5.928128
5.724949	480.980072	5.933133
5.810109	479.917862	5.938138
5.678734	481.889588	5.943142
5.624926	484.970678	5.948147
5.789943	480.271099	5.953152
5.741457	482.164716	5.958157
5.815984	479.946102	5.963162
5.834903	477.721734	5.968166
5.801356	478.084492	5.973171
6.260256	476.113977	5.978176
5.917426	492.605592	5.983181
5.918648	474.664096	5.988186
5.825947	478.474889	5.993190
5.646385	481.986948	5.998195
5.577547	473.786016	6.003200
5.720498	478.856116	6.008205
5.853710	474.540317	6.013210
5.933534	494.355086	6.018214
5.875632	494.845229	6.023219
5.977704	496.139767	6.028224
6.031563	509.568107	6.033229
6.053548	497.740989	6.038234
6.140206	504.322783	6.043238
6.010980	491.685672	6.048243
5.922355	474.931491	6.053248
5.731787	492.880389	6.058253
6.008802	493.724139	6.063258
6.304072	497.927678	6.068262
5.903420	494.743146	6.073267
5.879209	480.162183	6.078272
5.917185	496.710288	6.083277
6.231703	498.769519	6.088282
6.053618	496.206703	6.093286
5.816879	479.545020	6.098291
6.002124	487.526313	6.103296
6.086735	492.254460	6.108301
6.254845	493.899938	6.113306
6.114098	479.852607	6.118310
6.199140	476.731995	6.123315
6.347031	472.879669	6.128320
5.951085	482.391021	6.133325
5.726407	480.232008	6.138330
5.966740	486.609266	6.143334
6.015535	483.727337	6.148339
6.082095	464.480659	6.153344
5.787367	481.479118	6.158349
5.996603	473.096788	6.163354
6.052582	474.838851	6.168358
5.979332	473.801394	6.173363
6.145507	475.821934	6.178368
6.017406	474.909628	6.183373
5.935225	481.968024	6.188378
6.052283	475.426581	6.193382
5.846928	470.213133	6.198387
6.106127	475.665490	6.203392
5.808844	478.788628	6.208397
6.143749	474.102449	6.213402
6.047760	483.374894	6.218406
5.941286	471.759776	6.223411
6.322467	473.544478	6.228416
6.028447	485.473633	6.233421
5.953093	482.188066	6.238426
5.828539	480.378470	6.243430
5.969868	481.991102	6.248435
5.903640	480.707384	6.253440
5.823540	478.376929	6.258445
5.795252	482.124327	6.263450
5.650087	481.325958	6.268454
5.639911	497.283741	6.273459
6.138101	498.617223	6.278464
6.011330	502.884403	6.283469
6.258777	502.481160	6.288474
6.161288	491.801491	6.293478
5.630804	480.838991	6.298483
5.986643	478.969672	6.303488
6.120100	485.313189	6.308493
6.015523	487.772621	6.313498
6.041401	476.282516	6.318502
5.799975	486.389008	6.323507
5.754404	475.072202	6.328512
6.075805	493.085187	6.333517
6.152488	505.506664	6.338522
6.164459	494.943185	6.343526
5.989636	493.032817	6.348531
6.391367	481.748414	6.353536
6.011148	487.577609	6.358541
6.009748	490.558226	6.363546
6.164664	479.258808	6.368550
5.918579	489.389362	6.373555
5.962816	477.264134	6.378560
5.873985	486.403569	6.383565
6.322203	475.035667	6.388570
6.318931	477.173964	6.393574
6.077992	481.745268	6.398579
6.617519	475.129655	6.403584
6.170922	484.479125	6.408589
6.108527	475.148748	6.413594
6.213504	476.839252	6.418598
5.945993	472.586116	6.423603
6.099678	472.425397	6.428608
5.929965	476.523881	6.433613
6.131755	473.346960	6.438618
6.414154	475.146898	6.443622
5.685117	461.394707	6.448627
6.063612	455.097731	6.453632
5.886894	451.262268	6.458637
5.654010	445.228735	6.463642
6.005012	460.761373	6.468646
6.079366	471.755083	6.473651
6.358042	476.797689	6.478656
6.090151	462.087341	6.483661
5.907991	448.910073	6.488666
5.753229	447.303234	6.493670
5.700161	463.014336	6.498675
6.137047	473.770777	6.503680
5.702176	485.342287	6.508685
5.893319	480.069639	6.513690
6.179563	484.198503	6.518694
6.066609	485.119703	6.523699
6.112270	480.749585	6.528704
5.905781	483.648651	6.533709
5.973293	485.663491	6.538714
6.160700	482.374702	6.543718
6.117547	479.386104	6.548723
6.153676	464.835580	6.553728
5.647238	466.684546	6.558733
6.017564	467.487130	6.563738
5.930101	475.193468	6.568742
5.704200	479.845154	6.573747
5.623398	477.939484	6.578752
5.905306	481.601577	6.583757
5.764547	475.726770	6.588762
5.953237	473.531608	6.593766
5.880190	476.504004	6.598771
6.248437	482.375338	6.603776
6.161568	482.146858	6.608781
5.985230	479.654599	6.613786
6.085146	476.542564	6.618790
5.784589	488.623179	6.623795
5.915995	479.368529	6.628800
5.870493	482.335953	6.633805
5.905583	488.706478	6.638810
5.760725	481.047042	6.643814
5.765685	481.905030	6.648819
5.689174	484.370847	6.653824
5.685504	485.193368	6.658829
5.924349	478.956102	6.663834
6.184798	482.354172	6.668838
5.856896	492.057477	6.673843
6.240087	477.206725	6.678848
5.975198	482.890847	6.683853
6.282415	481.304106	6.688858
6.590788	481.643183	6.693862
5.926401	486.332827	6.698867
6.235620	480.912875	6.703872
5.820243	483.251890	6.708877
5.752405	486.485485	6.713882
6.507347	479.174168	6.718886
5.938690	490.712666	6.723891
6.101933	474.150464	6.728896
6.123454	479.976026	6.733901
5.954427	476.158618	6.738906
6.124596	476.924616	6.743910
5.772686	486.389972	6.748915
6.265995	490.961383	6.753920
6.147406	486.509437	6.758925
6.099578	482.929801	6.763930
6.149731	481.346125	6.768934
5.955316	494.251730	6.773939
6.137022	484.731389	6.778944
6.264086	474.062557	6.783949
5.948140	464.370777	6.788954
5.987427	459.106408	6.793958
5.373873	472.160402	6.798963
5.733153	473.708782	6.803968
6.081444	481.357098	6.808973
6.001226	479.685571	6.813978
6.228824	480.895108	6.818982
5.961766	478.035490	6.823987
5.887965	473.515126	6.828992
5.879786	483.729270	6.833997
6.134527	486.502337	6.839002
6.216913	479.571191	6.844006
6.147509	482.620931	6.849011
6.246246	475.537290	6.854016
6.061908	470.297656	6.859021
6.075499	454.400511	6.864026
6.035923	455.264125	6.869030
5.889610	453.968068	6.874035
6.135115	446.591666	6.879040
5.959293	449.713356	6.884045
5.687655	453.792861	6.889050
5.790986	455.259265	6.894054
5.941350	468.283366	6.899059
5.908831	471.566539	6.904064
6.311215	484.714329	6.909069
6.170992	470.031494	6.914074
6.224235	457.531817	6.919078
5.868462	461.818502	6.924083
6.083055	449.954669	6.929088
5.576261	455.381801	6.934093
5.657779	473.429506	6.939098
5.906776	468.917452	6.944102
5.756781	486.148988	6.949107
6.214388	482.458500	6.954112
6.130909	487.326673	6.959117
5.962777	481.354983	6.964122
6.204343	478.189803	6.969126
6.127487	479.257741	6.974131
6.057676	466.614327	6.979136
5.975495	467.597308	6.984141
5.866946	454.649537	6.989146
6.073474	461.722885	6.994150
6.003049	479.268174	6.999155
5.703516	464.696681	7.004160
6.296995	475.463206	7.009165
5.763183	485.690918	7.014170
5.909431	479.051281	7.019174
6.187223	490.069009	7.024179
5.980365	476.578307	7.029184
6.052527	478.583296	7.034189
5.998788	483.158807	7.039194
5.907165	475.903946	7.044198
5.671945	482.523644	7.049203
5.821421	481.704715	7.054208
6.271660	479.584480	7.059213
6.116844	478.219187	7.064218
6.555161	480.094048	7.069222
5.920777	476.899431	7.074227
5.966825	455.314771	7.079232
5.981450	457.837660	7.084237
5.833848	461.050962	7.089242
5.873047	453.201694	7.094246
5.788698	461.946289	7.099251
6.093195	470.235132	7.104256
6.201593	474.896370	7.109261
6.186352	466.389343	7.114266
6.206302	467.399354	7.119270
5.784963	456.388338	7.124275
6.030682	454.445368	7.129280
5.647073	446.866089	7.134285
5.803027	457.336308	7.139290
5.710852	475.380129	7.144294
5.457912	492.381323	7.149299
5.879303	493.356181	7.154304
6.210357	496.103738	7.159309
5.874061	499.659416	7.164314
6.234708	492.742594	7.169318
5.838906	497.241370	7.174323
5.786779	496.496603	7.179328
6.204021	491.928554	7.184333
5.964296	498.659122	7.189338
6.135608	490.976530	7.194342
5.983903	492.413302	7.199347
6.290022	487.692437	7.204352
6.111678	485.521577	7.209357
6.117760	492.352972	7.214362
6.163091	490.721552	7.219366
6.097480	499.854965	7.224371
5.714259	486.411330	7.229376
5.842427	495.332756	7.234381
6.017637	502.530717	7.239386
6.084797	500.761478	7.244390
5.921029	504.646646	7.249395
6.033783	493.912492	7.254400
6.281804	496.796003	7.259405
6.081987	479.353635	7.264410
5.915951	473.244253	7.269414
5.863874	482.176688	7.274419
5.959323	489.988990	7.279424
6.234690	494.127952	7.284429
5.734161	486.384959	7.289434
6.152481	494.892489	7.294438
5.506710	495.523170	7.299443
5.640970	499.211191	7.304448
6.015604	498.762337	7.309453
6.231666	501.143609	7.314458
6.173067	493.896274	7.319462
5.952630	502.099720	7.324467
6.475575	495.025480	7.329472
6.504253	487.129202	7.334477
6.453086	472.138714	7.339482
6.136472	471.134408	7.344486
5.550150	477.142505	7.349491
5.650480	461.729803	7.354496
6.090900	469.369904	7.359501
5.833308	477.588984	7.364506
6.091738	456.545639	7.369510
5.827792	463.520179	7.374515
6.285208	459.638903	7.379520
6.063475	465.010170	7.384525
5.463556	463.480284	7.389530
5.778477	456.934179	7.394534
6.100254	482.209871	7.399539
6.104222	469.861247	7.404544
6.325987	460.883253	7.409549
5.619786	464.336816	7.414554
5.946394	458.948516	7.419558
5.946469	472.804117	7.424563
6.060769	474.757503	7.429568
6.096927	475.193924	7.434573
5.824870	472.712840	7.439578
5.983973	467.219967	7.444582
6.182627	482.385446	7.449587
5.860544	462.167352	7.454592
5.820979	468.132517	7.459597
5.962028	479.921663	7.464602
6.052851	488.186635	7.469606
6.062814	494.255072	7.474611
5.877176	486.028358	7.479616
6.120957	488.460275	7.484621
5.880851	493.529326	7.489626
6.055965	488.560871	7.494630
6.173498	496.008181	7.499635
5.864922	480.267571	7.504640
6.009725	466.224096	7.509645
5.589401	471.583185	7.514650
5.894530	488.986336	7.519654
6.156248	486.305819	7.524659
5.981306	491.772131	7.529664
6.020654	487.533303	7.534669
5.888273	491.828645	7.539674
6.171736	490.895288	7.544678
5.899004	490.716252	7.549683
6.029917	492.921049	7.554688
5.944223	496.349426	7.559693
5.568248	498.788456	7.564698
6.017359	496.296425	7.569702
5.888322	504.638405	7.574707
6.004944	498.757907	7.579712
5.945231	490.800739	7.584717
5.730146	490.896089	7.589722
5.993511	495.471780	7.594726
6.126789	494.253765	7.599731
6.044325	493.586464	7.604736
6.032637	493.446523	7.609741
5.924360	486.962659	7.614746
6.296884	489.391924	7.619750
5.895809	492.286632	7.624755
5.824439	503.910808	7.629760
6.288043	499.286505	7.634765
6.133767	505.417176	7.639770
6.248179	494.251170	7.644774
6.315385	498.008550	7.649779
5.909119	479.029299	7.654784
6.199269	475.479722	7.659789
5.902842	469.791030	7.664794
5.917819	466.024737	7.669798
5.901465	478.552235	7.674803
5.791092	482.916931	7.679808
6.160891	484.518030	7.684813
6.052928	492.907808	7.689818
5.986063	481.396411	7.694822
6.080763	478.671431	7.699827
5.838992	484.185356	7.704832
5.805391	489.266454	7.709837
6.142578	506.384472	7.714842
6.348240	487.428805	7.719846
5.976546	483.379269	7.724851
6.042975	465.451021	7.729856
5.850496	469.667940	7.734861
5.947242	466.720027	7.739866
6.108022	456.927500	7.744870
5.918623	459.675522	7.749875
5.796631	453.666573	7.754880
5.855577	473.616804	7.759885
5.960580	484.858810	7.764890
6.297132	492.226496	7.769894
5.958841	480.417046	7.774899
5.919393	483.806555	7.779904
6.002483	474.048836	7.784909
5.971017	485.010614	7.789914
6.272055	469.441207	7.794918
6.007095	473.154731	7.799923
5.807841	459.655874	7.804928
5.929757	462.061866	7.809933
5.872123	473.498240	7.814938
6.183009	476.264735	7.819942
5.687970	472.035803	7.824947
5.948323	480.534852	7.829952
6.037538	491.237008	7.834957
5.671624	499.857334	7.839962
5.978368	497.545851	7.844966
6.103549	500.760587	7.849971
6.000062	496.772239	7.854976
6.183246	490.607960	7.859981
5.895719	504.850815	7.864986
6.298738	498.329516	7.869990
5.874071	499.556701	7.874995
6.105971	493.767552	7.880000
5.985606	480.335682	7.885005
5.707850	479.455948	7.890010
6.239657	485.653527	7.895014
6.053996	483.536770	7.900019
6.178928	476.575860	7.905024
5.965863	476.009795	7.910029
5.927849	471.310024	7.915034
5.802475	475.701090	7.920038
5.699242	481.559032	7.925043
6.212982	488.590602	7.930048
6.381524	485.105440	7.935053
5.978295	475.915190	7.940058
5.788663	462.388090	7.945062
5.789123	472.621906	7.950067
5.544324	484.322453	7.955072
5.860588	489.011501	7.960077
5.714865	495.295063	7.965082
6.030529	494.017723	7.970086
5.924986	503.216582	7.975091
5.893624	495.633390	7.980096
5.834578	495.299643	7.985101
5.895088	500.408910	7.990106
6.211713	501.992603	7.995110
5.958956	513.279691	8.000115
5.956763	504.889713	8.005133
6.311876	498.293245	8.010150
6.230558	504.033647	8.015168
6.345571	490.435163	8.020186
6.326633	498.306351	8.025203
6.132589	491.443324	8.030221
6.171666	481.581959	8.035238
6.107262	468.871905	8.040256
6.213140	464.171248	8.045274
5.913037	465.860560	8.050291
5.876703	475.528568	8.055309
6.441273	464.949408	8.060326
5.763053	471.638155	8.065344
5.993207	462.996902	8.070362
6.104024	458.308810	8.075379
5.860231	466.699403	8.080397
6.033624	467.668727	8.085414
6.191097	494.674897	8.090432
6.410845	482.983258	8.095450
6.081925	478.894981	8.100467
6.068527	470.397938	8.105485
6.019313	460.669166	8.110502
5.752865	476.752630	8.115520
6.143463	478.746193	8.120538
6.004346	491.683382	8.125555
6.167973	489.270365	8.130573
6.263463	498.873566	8.135590
6.281124	493.871842	8.140608
6.170105	475.719401	8.145626
6.109843	478.422695	8.150643
5.854297	477.828615	8.155661
6.431620	479.664183	8.160678
6.148645	476.930554	8.165696
6.309287	472.660911	8.170714
6.238462	470.796667	8.175731
5.890436	475.404720	8.180749
6.059530	472.044028	8.185766
6.084953	486.699381	8.190784
6.008880	492.786121	8.195802
6.365500	500.491744	8.200819
6.273303	500.867082	8.205837
6.344252	488.965152	8.210854
6.036218	491.826946	8.215872
5.954326	500.192023	8.220890
5.861443	504.636425	8.225907
6.270182	498.601074	8.230925
6.464222	499.387062	8.235942
6.072191	505.441294	8.240960
6.368452	499.343543	8.245978
6.447386	504.049912	8.250995
6.050674	506.511326	8.256013
6.036709	491.377127	8.261030
5.928160	499.144717	8.266048
5.958597	500.142923	8.271066
6.387476	502.665318	8.276083
6.149279	519.002573	8.281101
6.015200	503.256687	8.286118
6.169382	500.640728	8.291136
6.373785	507.734702	8.296154
6.388463	501.830003	8.301171
5.824133	501.655525	8.306189
6.182211	498.540949	8.311206
5.933025	500.111968	8.316224
6.080165	515.023078	8.321242
6.131784	520.766977	8.326259
6.394355	531.746838	8.331277
6.468728	529.329164	8.336294
6.417019	541.400950	8.341312
6.366540	532.630730	8.346330
6.517470	528.882722	8.351347
6.397310	534.307964	8.356365
6.557198	522.729386	8.361382
6.080790	517.560784	8.366400
6.402751	527.863305	8.371418
6.772757	531.556813	8.376435
6.073320	519.993920	8.381453
6.311029	517.928397	8.386470
6.055867	529.350191	8.391488
5.992214	535.596484	8.396506
6.435852	537.605843	8.401523
6.320606	536.862269	8.406541
6.419703	539.085578	8.411558
6.511879	532.977253	8.416576
6.411715	530.592725	8.421594
6.690827	530.067042	8.426611
6.589925	535.498138	8.431629
6.775447	532.126829	8.436646
6.448637	537.917300	8.441664
6.366914	534.703198	8.446682
6.554786	533.831687	8.451699
6.370909	536.919878	8.456717
6.313200	533.362836	8.461734
6.477705	534.884187	8.466752
6.137339	534.581741	8.471770
6.554909	530.636471	8.476787
6.406627	539.598777	8.481805
6.520679	531.603309	8.486822
6.304998	544.923513	8.491840
6.476134	537.194121	8.496858
6.528323	537.609824	8.501875
6.430525	538.019358	8.506893
6.761283	534.515845	8.511910
6.571942	535.835995	8.516928
6.494850	536.129695	8.521946
6.387478	532.704520	8.526963
6.201006	539.407415	8.531981
6.277313	536.610315	8.536998
6.370990	540.507814	8.542016
6.417450	541.629334	8.547034
6.420192	531.801336	8.552051
6.042498	534.154287	8.557069
6.292493	549.835080	8.562087
6.663350	559.573044	8.567104
6.457359	571.129991	8.572122
6.789069	564.429126	8.577139
6.539177	562.124594	8.582157
6.653892	567.318892	8.587175
6.652464	567.318346	8.592192
6.530695	569.759066	8.597210
6.597853	561.527498	8.602227
6.619899	567.584180	8.607245
6.782579	576.334596	8.612263
6.862939	573.618109	8.617280
6.840520	567.465241	8.622298
7.060352	562.823559	8.627315
6.526729	542.115905	8.632333
6.536198	548.251042	8.637351
6.429637	537.696388	8.642368
6.740696	555.746567	8.647386
6.917994	556.224146	8.652403
6.687360	559.029192	8.657421
6.606545	545.029781	8.662439
6.658501	548.987560	8.667456
6.647285	560.466850	8.672474
6.733348	558.518845	8.677491
6.711209	571.398469	8.682509
6.687779	575.707734	8.687527
6.527969	565.615616	8.692544
6.728545	565.908435	8.697562
7.138464	563.031863	8.702579
6.643822	566.031964	8.707597
7.020067	554.052665	8.712615
6.568388	551.124445	8.717632
6.970620	557.821218	8.722650
6.844207	539.707282	8.727667
6.784299	547.456576	8.732685
6.652889	538.190790	8.737703
6.646100	539.454811	8.742720
6.504241	546.977982	8.747738
7.187737	556.039815	8.752755
6.756899	554.226741	8.757773
6.860799	556.830130	8.762791
6.633908	553.643697	8.767808
6.715343	567.319028	8.772826
6.806512	563.375253	8.777843
6.847731	570.044448	8.782861
6.966162	566.896668	8.787879
7.138817	571.857536	8.792896
6.805959	558.106488	8.797914
6.684995	549.120827	8.802931
6.769895	555.152490	8.807949
6.829134	561.153385	8.812967
6.923114	560.127021	8.817984
6.700375	569.148961	8.823002
7.004944	569.444570	8.828019
6.745578	570.010085	8.833037
6.792317	574.376972	8.838055
6.924942	569.020314	8.843072
6.923629	574.268741	8.848090
7.253456	565.637239	8.853107
6.979678	575.601057	8.858125
6.707072	563.534934	8.863143
6.795954	564.332696	8.868160
6.924768	569.534100	8.873178
6.832643	572.032881	8.878195
6.941646	577.428707	8.883213
6.874193	567.424771	8.888231
7.198948	567.276116	8.893248
6.710805	572.231477	8.898266
6.811572	577.188156	8.903283
6.732769	568.273226	8.908301
6.709907	578.101644	8.913319
6.957204	571.398864	8.918336
6.420865	572.986914	8.923354
6.898630	577.034539	8.928371
6.707767	564.233822	8.933389
6.745999	570.325803	8.938407
6.964044	584.659884	8.943424
6.915672	604.593542	8.948442
6.819259	603.062643	8.953459
6.987470	602.795334	8.958477
6.681933	612.716427	8.963495
7.483501	598.376021	8.968512
7.336308	606.324681	8.973530
7.338727	608.628632	8.978547
6.981170	604.229554	8.983565
7.191136	602.736305	8.988583
7.013640	597.910479	8.993600
7.037936	610.126956	8.998618
7.322543	596.332092	9.003635
7.415860	601.254587	9.008653
6.996000	581.052340	9.013671
7.202234	577.399057	9.018688
7.009113	569.135952	9.023706
7.051296	566.051432	9.028723
7.186474	582.982939	9.033741
6.685491	592.559370	9.038759
7.266413	588.467652	9.043776
6.787746	613.351991	9.048794
7.266288	591.185773	9.053811
7.337843	597.661960	9.058829
7.010984	602.250391	9.063847
7.122117	597.562992	9.068864
7.113798	601.782358	9.073882
7.026153	602.756501	9.078899
7.287868	600.999748	9.083917
7.205692	596.398808	9.088935
7.367818	599.450757	9.093952
7.058236	606.248745	9.098970
7.394217	601.212380	9.103987
7.471467	606.716636	9.109005
7.145193	603.721109	9.114023
7.606591	595.569060	9.119040
7.323899	609.469508	9.124058
7.303335	607.204600	9.129075
6.991727	581.828064	9.134093
7.129525	600.530275	9.139111
7.685355	593.948234	9.144128
7.345546	599.179909	9.149146
7.063176	592.657477	9.154163
7.390949	591.922932	9.159181
7.271755	601.625263	9.164199
7.307919	597.454420	9.169216
7.266079	598.242026	9.174234
7.192460	592.475779	9.179251
7.538685	605.091264	9.184269
7.315312	604.707563	9.189287
7.491577	606.750155	9.194304
7.165823	601.849766	9.199322
7.132628	608.674839	9.204339
7.207422	608.969473	9.209357
6.985875	606.617313	9.214375
7.319685	602.955612	9.219392
7.192689	605.342487	9.224410
7.203517	601.921466	9.229427
7.139490	604.268742	9.234445
6.887996	608.537782	9.239463
7.251105	607.689891	9.244480
7.077487	613.414772	9.249498
7.316361	618.517392	9.254515
7.729438	621.223916	9.259533
7.119920	621.412038	9.264551
7.725317	622.021397	9.269568
7.480243	617.199712	9.274586
7.411870	609.705553	9.279603
7.408204	604.165057	9.284621
7.134960	613.318242	9.289639
7.519114	623.006993	9.294656
7.378537	649.000260	9.299674
7.557660	638.261644	9.304691
7.749553	632.574074	9.309709
7.206979	636.589756	9.314727
7.415098	633.907530	9.319744
7.501728	640.507990	9.324762
7.457090	649.840702	9.329779
7.659173	637.006299	9.334797
7.466742	646.038009	9.339815
7.331690	639.418831	9.344832
7.631530	643.052380	9.349850
7.472539	645.751642	9.354867
7.611283	646.115759	9.359885
7.376895	639.616038	9.364903
7.589250	643.593632	9.369920
7.566675	652.668366	9.374938
7.533194	650.518189	9.379955
7.784252	641.306475	9.384973
7.692749	642.223392	9.389991
7.758314	634.651844	9.395008
7.841162	647.782565	9.400026
7.363355	634.680889	9.405043
7.491225	630.629430	9.410061
7.374345	630.765190	9.415079
7.430055	645.939440	9.420096
7.588922	642.288306	9.425114
7.432934	639.640816	9.430131
7.812667	637.529231	9.435149
7.445034	652.702798	9.440167
7.644013	647.123485	9.445184
7.756958	644.155131	9.450202
7.784805	646.047017	9.455219
7.888045	637.051989	9.460237
7.827112	644.757804	9.465255
7.659321	649.468025	9.470272
7.679152	645.963418	9.475290
7.768685	649.601220	9.480307
7.641918	646.376866	9.485325
7.369688	643.947501	9.490343
7.565878	641.159391	9.495360
7.565756	644.282606	9.500378
7.623103	647.727741	9.505395
7.742956	647.370642	9.510413
7.584969	641.690836	9.515431
7.921514	648.240901	9.520448
7.889967	651.293756	9.525466
7.906893	643.896024	9.530483
7.820034	638.256164	9.535501
7.925576	646.346482	9.540519
7.919304	640.447181	9.545536
7.767049	642.350501	9.550554
7.956244	654.944298	9.555571
7.873285	641.641955	9.560589
7.955081	647.115354	9.565607
7.558241	647.693093	9.570624
7.703474	652.897898	9.575642
7.658323	647.536710	9.580659
7.717027	643.662086	9.585677
7.745435	648.213130	9.590695
7.725184	637.977698	9.595712
8.103044	648.433201	9.600730
7.741720	643.680237	9.605747
7.827878	648.923794	9.610765
7.745689	651.677216	9.615783
7.792089	650.019432	9.620800
7.965793	640.952457	9.625818
7.864082	651.118216	9.630835
7.871084	642.171659	9.635853
7.967165	643.703804	9.640871
8.078199	641.876628	9.645888
7.919077	645.731534	9.650906
8.207490	644.192960	9.655923
8.323307	648.198019	9.660941
7.954219	648.827637	9.665959
7.774392	643.705946	9.670976
7.905052	640.689770	9.675994
8.146950	644.400465	9.681011
8.098605	643.241269	9.686029
7.974987	648.162832	9.691047
7.821192	646.019466	9.696064
8.146515	644.216115	9.701082
8.315253	644.747674	9.706099
7.983297	649.560178	9.711117
7.973792	646.326962	9.716135
8.266459	643.606273	9.721152
8.076120	644.523282	9.726170
7.742802	658.736103	9.731187
7.883864	646.818068	9.736205
7.559223	649.798194	9.741223
7.437118	656.097555	9.746240
7.782447	657.630591	9.751258
8.017086	669.468477	9.756275
8.263876	668.001184	9.761293
8.069516	673.415385	9.766311
8.220636	673.846535	9.771328
8.234074	672.691632	9.776346
8.183175	675.881164	9.781363
8.322595	676.018610	9.786381
8.106546	677.454817	9.791399
8.078353	675.107512	9.796416
8.150178	677.826874	9.801434
8.165208	676.652417	9.806451
8.472968	674.506928	9.811469
7.994815	659.854811	9.816487
7.996300	666.445028	9.821504
8.314382	671.465214	9.826522
7.913410	678.143000	9.831539
8.202518	666.938870	9.836557
8.185073	673.663724	9.841575
8.142064	666.971758	9.846592
8.535439	667.316974	9.851610
7.972863	680.423322	9.856627
8.057170	673.480877	9.861645
8.276962	681.182958	9.866663
7.862725	669.045026	9.871680
8.459767	666.848304	9.876698
8.289290	678.655707	9.881715
8.193191	669.632578	9.886733
8.207797	675.639361	9.891751
8.068210	676.368814	9.896768
8.090743	678.498185	9.901786
8.064904	679.760463	9.906803
8.499068	673.803293	9.911821
8.222078	680.656324	9.916839
8.052527	674.635539	9.921856
8.349444	678.075699	9.926874
8.027113	684.571137	9.931891
8.409889	679.765141	9.936909
8.480052	683.408533	9.941927
8.328745	685.628016	9.946944
8.492935	678.378611	9.951962
8.746122	685.239377	9.956979
8.280574	677.484062	9.961997
8.566379	681.492761	9.967015
8.317037	686.484641	9.972032
8.613488	677.553332	9.977050
8.160752	677.815190	9.982067
8.529984	672.957317	9.987085
8.407318	683.931443	9.992103
7.950769	684.549815	9.997120
8.095811	674.735079	10.002138
8.417764	699.887039	10.007155
8.706464	702.060353	10.012173
8.349453	694.438946	10.017191
8.521477	705.779823	10.022208
8.641152	696.922372	10.027226
8.370955	690.292567	10.032243
8.413149	690.223554	10.037261
8.473317	703.268727	10.042279
8.279588	716.179356	10.047296
8.571338	703.046943	10.052314
8.556878	711.149172	10.057331
8.523004	709.912767	10.062349
8.679644	710.434529	10.067367
8.633945	710.369889	10.072384
8.662078	712.944759	10.077402
8.327335	711.294618	10.082419
8.830498	707.009312	10.087437
8.677377	709.745403	10.092455
8.505759	697.446262	10.097472
8.637026	695.264955	10.102490
8.308953	708.388445	10.107507
8.393618	712.227056	10.112525
8.522024	712.148043	10.117543
8.426729	706.051324	10.122560
8.603542	705.512131	10.127578
8.897807	718.073555	10.132595
8.931759	711.514831	10.137613
8.755676	706.778297	10.142631
8.347671	719.325754	10.147648
8.738492	713.175197	10.152666
8.801248	710.019911	10.157683
8.764266	707.432347	10.162701
9.014133	702.898418	10.167719
8.763871	703.223268	10.172736
9.172250	688.970771	10.177754
8.559031	678.971661	10.182771
8.507786	674.869653	10.187789
8.847703	680.299962	10.192807
8.666426	684.389253	10.197824
8.436748	680.319856	10.202842
8.403802	704.471048	10.207859
8.378136	707.862283	10.212877
8.791003	711.208969	10.217895
8.486552	708.475719	10.222912
8.732816	699.831854	10.227930
8.485534	710.473982	10.232947
8.450030	709.315599	10.237965
8.725618	702.967877	10.242983
8.725583	705.801544	10.248000
8.616626	711.314939	10.253018
8.798663	715.618632	10.258035
8.776093	720.698410	10.263053
8.932789	732.139485	10.268071
8.791110	739.546782	10.273088
8.877670	738.600768	10.278106
9.165759	740.267137	10.283123
9.064106	729.769406	10.288141
8.992738	718.519457	10.293159
8.972288	716.719048	10.298176
9.018969	709.531284	10.303194
8.830586	707.643051	10.308211
8.579327	709.637830	10.313229
8.908320	702.914131	10.318247
8.670502	713.728298	10.323264
8.782685	730.415183	10.328282
9.107370	734.206424	10.333299
9.099393	741.097044	10.338317
9.443572	736.883036	10.343335
8.879595	721.327867	10.348352
8.949421	715.434588	10.353370
9.088211	712.859928	10.358387
8.946006	708.624223	10.363405
8.985641	713.867859	10.368423
9.040336	711.922096	10.373440
9.034716	713.169205	10.378458
9.178010	703.770264	10.383475
9.188527	707.838900	10.388493
9.184414	703.613114	10.393511
8.950341	710.189359	10.398528
8.932057	711.008288	10.403546
8.871707	707.623877	10.408563
8.536857	715.384903	10.413581
9.160825	720.079279	10.418599
8.880766	739.075901	10.423616
9.583663	729.121163	10.428634
9.377466	739.231125	10.433651
8.973942	731.909930	10.438669
9.291933	732.447390	10.443687
8.980269	728.520930	10.448704
9.146071	727.600719	10.453722
9.326990	740.775055	10.458739
9.305459	730.566544	10.463757
9.125555	726.035940	10.468775
8.756816	721.830012	10.473792
9.208525	722.145062	10.478810
9.650796	737.399625	10.483827
9.184044	729.550395	10.488845
9.552770	706.164952	10.493863
9.457174	718.865584	10.498880
9.333562	710.858941	10.503898
9.437043	702.137043	10.508915
9.363699	712.060545	10.513933
9.390019	705.422192	10.518951
9.345892	699.307327	10.523968
9.210748	709.410773	10.528986
8.866244	711.226774	10.534003
8.800954	706.077167	10.539021
9.110028	705.611061	10.544039
8.884054	714.747001	10.549056
9.345831	723.092690	10.554074
9.321499	732.278188	10.559091
9.072921	737.546513	10.564109
9.328775	736.540668	10.569127
9.116261	742.666326	10.574144
9.111524	732.688274	10.579162
9.133817	746.184827	10.584179
8.815557	740.771176	10.589197
9.311548	735.393232	10.594215
9.212322	733.338218	10.599232
8.958899	751.051381	10.604250
9.190317	759.160202	10.609267
9.415999	763.361778	10.614285
9.356800	768.760041	10.619303
9.497432	773.601502	10.624320
9.486447	776.757453	10.629338
9.717314	769.754189	10.634355
9.271459	785.583167	10.639373
9.466520	776.534018	10.644391
9.660980	781.792294	10.649408
9.441296	786.500750	10.654426
9.601097	776.013659	10.659443
9.559260	777.433121	10.664461
9.408734	779.585761	10.669479
9.425447	768.843343	10.674496
9.687597	775.522947	10.679514
9.766507	765.754971	10.684531
9.226068	765.889094	10.689549
9.548060	770.570103	10.694567
9.450113	764.824566	10.699584
9.203400	778.909133	10.704602
9.477168	771.971961	10.709619
9.401673	779.892257	10.714637
9.610056	773.464541	10.719655
9.776123	781.234457	10.724672
9.202528	770.842702	10.729690
9.353014	777.020626	10.734707
9.509644	776.442465	10.739725
9.461700	778.343423	10.744743
9.493454	775.592463	10.749760
9.244221	777.545775	10.754778
9.441251	776.677847	10.759795
9.600448	792.303511	10.764813
9.787687	799.093799	10.769831
9.998919	805.893486	10.774848
9.739570	798.772690	10.779866
9.954611	784.331392	10.784883
9.706483	785.407807	10.789901
9.616875	776.753984	10.794919
9.555343	771.492714	10.799936
9.708698	779.544251	10.804954
9.487643	775.485206	10.809971
9.536382	798.193337	10.814989
9.682650	798.642815	10.820007
9.792762	806.188792	10.825024
9.520061	808.773527	10.830042
9.708101	797.922696	10.835059
9.499023	804.743037	10.840077
9.765660	811.481553	10.845095
9.944965	802.702510	10.850112
9.852136	807.542239	10.855130
9.941447	797.803024	10.860147
10.006229	813.427672	10.865165
9.613986	805.917177	10.870183
9.951699	795.233582	10.875200
9.632482	807.214813	10.880218
9.948682	801.216774	10.885235
9.820980	811.846574	10.890253
10.015059	811.462568	10.895271
9.836581	800.624629	10.900288
9.229162	804.958986	10.905306
9.895419	796.298205	10.910323
9.998080	808.594327	10.915341
9.910358	798.837690	10.920359
9.891365	803.761202	10.925376
9.800719	807.684879	10.930394
10.221370	807.854907	10.935411
10.053689	812.554727	10.940429
9.895069	812.136833	10.945447
10.216955	806.774026	10.950464
10.144438	809.703809	10.955482
10.276785	807.962436	10.960499
10.108686	809.945964	10.965517
10.100972	811.494197	10.970535
10.367887	806.331067	10.975552
10.086699	799.765440	10.980570
9.983267	804.562052	10.985587
9.772362	806.174372	10.990605
9.898230	801.011462	10.995623
9.737565	810.871201	11.000640
9.581659	809.052551	11.005658
9.893352	813.392000	11.010675
10.168434	838.595280	11.015693
10.273210	844.658396	11.020711
10.342496	839.105690	11.025728
10.178321	847.103946	11.030746
10.461591	828.483806	11.035763
10.193545	819.867690	11.040781
9.868778	812.666822	11.045799
9.891722	821.510284	11.050816
9.999788	837.898579	11.055834
10.227336	843.260227	11.060851
9.945203	840.679140	11.065869
10.337975	844.176037	11.070887
10.248871	844.806758	11.075904
10.078736	846.206413	11.080922
10.273367	830.474450	11.085939
10.152935	835.351845	11.090957
10.210844	843.687570	11.095975
10.448704	844.749346	11.100992
10.054261	844.556858	11.106010
10.383633	836.783497	11.111027
10.109867	838.429103	11.116045
10.224473	843.950461	11.121063
10.384354	841.477780	11.126080
10.111282	837.127974	11.131098
10.453972	837.085778	11.136115
10.446749	840.123604	11.141133
10.644653	845.747252	11.146151
10.869922	842.442886	11.151168
10.339435	841.686828	11.156186
10.634499	832.470049	11.161203
10.390331	838.230163	11.166221
10.597065	840.362007	11.171239
10.606599	837.627327	11.176256
10.341863	845.525769	11.181274
10.515432	840.654898	11.186291
10.797393	837.255683	11.191309
10.598367	836.179585	11.196327
10.316518	815.143710	11.201344
10.059844	819.439847	11.206362
10.573149	836.795363	11.211379
10.251327	847.139757	11.216397
10.745907	851.241743	11.221415
10.511458	840.841399	11.226432
10.368082	843.641637	11.231450
10.494452	842.821668	11.236467
10.399412	838.410775	11.241485
10.032952	851.481321	11.246503
10.423970	846.153464	11.251520
10.224677	855.848796	11.256538
10.446436	849.887695	11.261555
10.514919	844.914612	11.266573
10.302444	849.543548	11.271591
10.538180	841.225153	11.276608
10.595041	847.001371	11.281626
10.478617	847.240988	11.286643
10.845417	843.204873	11.291661
10.370980	846.834109	11.296679
10.808855	848.500001	11.301696
10.810795	859.982247	11.306714
10.919459	859.516774	11.311731
10.584002	850.329204	11.316749
10.761184	854.497334	11.321767
10.937512	845.605383	11.326784
10.735705	853.526438	11.331802
10.636214	854.106133	11.336819
10.856652	846.001683	11.341837
10.469795	851.378852	11.346855
10.869506	850.902400	11.351872
10.438561	848.123226	11.356890
10.818994	848.947931	11.361907
10.728385	854.727800	11.366925
10.848426	875.938653	11.371943
10.658949	873.630331	11.376960
10.566276	886.684923	11.381978
10.511372	883.023994	11.386995
10.940633	877.008314	11.392013
10.620618	886.527286	11.397031
10.876725	867.758474	11.402048
10.797065	882.785978	11.407066
10.729736	878.014977	11.412083
10.682240	865.838763	11.417101
10.788498	882.414796	11.422119
10.924873	867.553058	11.427136
10.933796	878.343647	11.432154
10.782255	883.626598	11.437171
10.862044	875.396308	11.442189
11.046449	883.451989	11.447207
11.103884	874.166029	11.452224
10.756352	881.201139	11.457242
11.081424	874.362671	11.462259
11.003721	877.973209	11.467277
10.558845	879.714974	11.472295
10.720767	870.002618	11.477312
10.974064	881.168313	11.482330
10.743167	878.303522	11.487347
10.886177	875.716324	11.492365
10.863381	903.146651	11.497383
11.063191	908.914091	11.502400
11.030309	905.694746	11.507418
11.145650	904.203024	11.512435
11.255051	906.767568	11.517453
10.939175	912.726625	11.522471
11.176559	915.946630	11.527488
11.182272	910.069445	11.532506
11.432605	906.588863	11.537523
11.217539	887.072803	11.542541
11.361536	879.163708	11.547559
11.229158	879.812647	11.552576
10.762702	869.115828	11.557594
11.169775	888.904269	11.562611
11.106266	898.439664	11.567629
11.001751	910.298284	11.572647
11.443336	901.880290	11.577664
11.526947	902.851968	11.582682
11.260385	893.100197	11.587699
11.243033	871.135686	11.592717
11.158016	876.418600	11.597735
11.316313	880.971349	11.602752
10.970179	885.888244	11.607770
11.069262	900.735277	11.612787
11.353026	904.493994	11.617805
10.970645	913.135999	11.622823
11.610426	913.339680	11.627840
11.163923	914.674261	11.632858
11.298531	905.678981	11.637875
11.250894	911.580067	11.642893
11.132453	907.697816	11.647911
11.626531	916.073279	11.652928
11.404865	904.643267	11.657946
11.354469	906.269861	11.662963
12.041801	905.559784	11.667981
11.268994	908.646537	11.672999
11.494617	912.303116	11.678016
11.580204	910.760437	11.683034
11.394133	914.135862	11.688051
11.345940	907.162190	11.693069
11.480955	913.340379	11.698087
11.254274	910.785493	11.703104
11.568392	914.164780	11.708122
11.520838	912.444637	11.713139
11.412280	905.229439	11.718157
11.380904	913.126526	11.723175
11.669807	910.854029	11.728192
11.696310	906.330399	11.733210
11.261272	921.231983	11.738227
11.799072	915.354537	11.743245
11.355510	917.493702	11.748263
11.212806	920.232428	11.753280
11.437951	903.879999	11.758298
11.426861	919.475242	11.763315
11.662573	900.510185	11.768333
11.527688	909.581101	11.773351
11.433280	908.519103	11.778368
11.463518	909.978366	11.783386
11.738029	915.956213	11.788403
11.695579	906.182535	11.793421
11.640298	905.961622	11.798439
11.451943	901.155222	11.803456
11.789920	907.938217	11.808474
11.666484	914.973099	11.813491
11.551313	911.399341	11.818509
11.351842	910.837456	11.823527
11.530861	909.191851	11.828544
11.833537	921.774876	11.833562
11.701518	926.823901	11.838579
12.088168	929.077024	11.843597
11.721714	915.976678	11.848615
11.367093	906.159225	11.853632
12.046202	924.606112	11.858650
11.986518	931.376088	11.863667
11.788022	913.545334	11.868685
12.103185	911.038958	11.873703
11.872071	914.720278	11.878720
12.202977	903.351560	11.883738
11.736396	907.513330	11.888755
11.719949	899.647035	11.893773
12.009227	900.156206	11.898791
11.812683	902.971984	11.903808
11.627798	907.740043	11.908826
11.649536	902.144434	11.913843
11.818774	924.728987	11.918861
11.953315	932.900850	11.923879
11.837923	939.549388	11.928896
12.285490	932.117336	11.933914
12.394978	943.642001	11.938931
12.007220	923.107414	11.943949
11.751718	915.736333	11.948967
11.864405	925.603460	11.953984
11.867713	930.705579	11.959002
11.826333	935.738359	11.964019
11.901155	939.022395	11.969037
12.199660	942.935356	11.974055
12.027713	935.914136	11.979072
12.109710	938.375371	11.984090
11.962803	938.390542	11.989107
11.945173	933.591578	11.994125
11.913383	937.330318	11.999143
12.307170	932.438561	12.004160
11.835238	935.298546	12.009178
11.726690	942.582919	12.014195
11.974363	939.145289	12.019213
11.981449	936.929868	12.024231
11.773321	933.854207	12.029248
12.202917	943.442698	12.034266
12.017043	946.838175	12.039283
12.049774	964.138682	12.044301
12.421370	961.610713	12.049319
12.162742	977.793193	12.054336
12.713342	972.940316	12.059354
12.399500	959.226889	12.064371
12.350953	944.655643	12.069389
12.580819	938.855750	12.074407
12.185636	949.507272	12.079424
12.476328	937.827513	12.084442
12.050228	937.270228	12.089459
12.267361	937.045764	12.094477
12.569441	932.194052	12.099495
12.329596	936.185473	12.104512
12.222236	932.737964	12.109530
11.865713	944.460555	12.114547
12.130271	943.510137	12.119565
12.667877	954.356596	12.124583
12.520086	960.176321	12.129600
12.447045	940.613753	12.134618
12.247802	942.095416	12.139635
12.266824	946.994151	12.144653
12.921694	956.558197	12.149671
12.521005	942.059265	12.154688
12.730869	940.888817	12.159706
12.372727	940.709584	12.164723
12.372250	931.134021	12.169741
12.276966	939.213387	12.174759
12.147170	932.599706	12.179776
12.574691	949.799538	12.184794
12.689970	961.799999	12.189811
12.706927	965.999122	12.194829
12.846496	951.722567	12.199847
12.490218	940.905029	12.204864
12.600813	938.470444	12.209882
12.418096	937.242031	12.214899
12.331354	940.831253	12.219917
13.031900	955.828350	12.224935
12.622147	958.411876	12.229952
12.899617	950.338834	12.234970
12.765238	940.940238	12.239987
12.627021	947.722881	12.245005
12.649695	942.940442	12.250023
12.601900	946.687750	12.255040
12.710010	938.131083	12.260058
12.477536	945.148277	12.265075
12.635240	960.967853	12.270093
12.825757	973.163286	12.275111
12.846481	976.120119	12.280128
12.373286	969.886319	12.285146
12.741387	970.582379	12.290163
12.969476	968.272741	12.295181
12.767995	972.985708	12.300199
12.713086	982.089039	12.305216
12.905195	970.818929	12.310234
12.833090	978.546057	12.315251
13.040036	975.417141	12.320269
13.117779	968.535101	12.325287
12.853987	962.557820	12.330304
12.831814	959.699656	12.335322
12.887113	977.253893	12.340339
12.655491	977.237871	12.345357
13.099640	969.087512	12.350375
12.921905	971.152972	12.355392
12.957215	967.959679	12.360410
13.051437	970.716903	12.365427
13.117859	974.130682	12.370445
13.114303	963.478109	12.375463
12.825558	962.454314	12.380480
12.615717	954.635884	12.385498
12.678716	970.094066	12.390515
12.529548	972.576409	12.395533
12.642372	965.170064	12.400551
12.645241	976.521147	12.405568
13.029264	963.938107	12.410586
12.848165	964.722306	12.415603
12.789502	973.133380	12.420621
13.528678	971.868650	12.425639
13.395492	973.260206	12.430656
13.606439	963.751048	12.435674
13.620321	966.868458	12.440691
13.136426	958.504272	12.445709
12.963460	971.525040	12.450727
13.133954	969.243085	12.455744
13.545552	960.015128	12.460762
13.034681	960.626594	12.465779
13.327507	955.444935	12.470797
13.239194	962.210628	12.475815
13.275774	967.458401	12.480832
13.108779	971.273557	12.485850
13.460297	956.587772	12.490867
13.214460	963.276505	12.495885
13.319690	953.502265	12.500903
13.326219	967.760448	12.505920
13.194454	956.473320	12.510938
13.056487	957.773155	12.515955
12.860699	955.135965	12.520973
13.207143	951.167770	12.525991
13.232320	957.745315	12.531008
13.270068	954.684683	12.536026
13.009437	954.763636	12.541043
13.353973	968.995950	12.546061
13.696496	968.737259	12.551079
13.173580	972.127350	12.556096
13.211382	971.218165	12.561114
13.609216	970.405427	12.566131
13.533696	982.827362	12.571149
13.746898	980.428863	12.576167
13.340838	967.685037	12.581184
13.275050	963.925903	12.586202
13.304064	966.922300	12.591219
13.553640	972.726371	12.596237
13.729833	969.623826	12.601255
13.268540	978.687624	12.606272
13.684870	977.760793	12.611290
13.811811	978.152076	12.616307
13.413603	981.580492	12.621325
13.983362	976.411847	12.626343
13.457430	973.843703	12.631360
13.581261	969.538904	12.636378
13.858071	977.619037	12.641395
13.595132	976.727559	12.646413
13.723742	971.879473	12.651431
13.845614	970.383117	12.656448
13.820489	969.126144	12.661466
13.738439	957.311094	12.666483
13.475164	958.045963	12.671501
13.409445	959.284972	12.676519
13.640273	969.253744	12.681536
13.879039	971.661369	12.686554
13.700676	972.763994	12.691571
13.384184	974.866691	12.696589
13.542572	967.322069	12.701607
13.517719	973.628031	12.706624
13.700245	970.500813	12.711642
13.684353	968.012450	12.716659
13.637051	978.668368	12.721677
13.662123	972.485990	12.726695
13.768915	984.587481	12.731712
13.618584	981.972650	12.736730
13.532252	985.257894	12.741747
13.650692	1002.198940	12.746765
13.673452	1010.523669	12.751783
13.674724	1007.228944	12.756800
13.847668	1007.297243	12.761818
14.217405	1010.302758	12.766835
13.767203	1011.169876	12.771853
14.077970	1003.526290	12.776871
13.921105	1017.031403	12.781888
13.998161	1004.652103	12.786906
14.140925	998.613135	12.791923
13.847099	1008.634889	12.796941
13.713533	1001.352548	12.801959
13.912198	1005.031346	12.806976
13.850020	1005.530832	12.811994
14.200647	1010.059524	12.817011
14.111872	1012.581045	12.822029
13.911868	1008.515093	12.827047
13.836799	1008.929718	12.832064
13.989401	1012.067384	12.837082
14.236253	999.990556	12.842099
14.002599	1012.939561	12.847117
14.080590	1005.682286	12.852135
14.217858	1013.712407	12.857152
13.996144	1022.126202	12.862170
14.374966	1018.385273	12.867187
14.371155	1032.042116	12.872205
14.358123	1015.015022	12.877223
14.278321	1013.828547	12.882240
14.336383	1008.218594	12.887258
14.279744	1004.313056	12.892275
14.363999	1009.734011	12.897293
14.042542	994.634882	12.902311
13.974801	1012.654470	12.907328
14.015260	1026.219700	12.912346
14.154801	1030.168161	12.917363
14.326125	1028.862782	12.922381
14.564324	1033.726295	12.927399
14.381383	1034.428523	12.932416
14.389826	1034.622586	12.937434
14.525137	1035.251443	12.942451
14.466724	1040.571721	12.947469
14.780573	1030.014761	12.952487
14.816099	1031.917228	12.957504
14.409542	1045.440249	12.962522
14.734345	1037.423859	12.967539
14.483365	1020.642993	12.972557
14.560457	1011.398563	12.977575
14.504583	1010.320704	12.982592
14.576066	1001.601989	12.987610
14.418780	1004.420709	12.992627
14.514289	1011.927483	12.997645
14.282093	1036.701652	13.002663
14.716154	1033.474740	13.007680
14.470044	1036.267287	13.012698
14.826697	1031.190343	13.017715
14.502371	1033.197111	13.022733
14.783995	1033.347340	13.027751
15.001203	1023.285952	13.032768
14.808765	1017.803456	13.037786
14.563722	1013.397762	13.042803
14.758441	1019.389307	13.047821
14.788747	1022.500454	13.052839
14.884787	1007.355143	13.057856
14.663483	1004.460389	13.062874
14.621095	1001.290633	13.067891
14.722939	1011.958789	13.072909
14.826598	1024.023432	13.077927
14.845424	1019.490415	13.082944
14.552525	1034.326357	13.087962
14.944667	1028.745508	13.092979
14.799910	1027.889891	13.097997
14.785204	1029.825904	13.103015
14.918358	1027.504086	13.108032
14.835912	1024.103594	13.113050
15.162737	1032.482513	13.118067
15.186388	1037.703327	13.123085
14.846391	1025.495689	13.128103
14.980315	1027.429436	13.133120
14.396056	1031.575368	13.138138
15.091860	1034.631802	13.143155
14.446275	1032.654375	13.148173
14.216158	1032.747940	13.153191
14.755920	1029.650303	13.158208
14.874071	1035.547106	13.163226
14.924388	1027.956641	13.168243
15.021610	1034.305325	13.173261
14.793610	1032.306123	13.178279
14.955522	1044.624471	13.183296
15.134917	1059.478778	13.188314
15.561270	1055.653172	13.193331
15.239313	1036.366098	13.198349
14.784984	1036.147342	13.203367
15.134900	1031.069943	13.208384
14.755974	1050.095583	13.213402
15.606710	1052.694793	13.218419
15.426833	1053.537057	13.223437
15.112853	1049.277057	13.228455
15.236928	1028.654104	13.233472
15.165173	1042.228159	13.238490
15.157714	1037.010957	13.243507
15.109313	1046.460078	13.248525
15.150139	1059.789068	13.253543
15.680734	1062.132847	13.258560
15.279570	1056.956672	13.263578
15.432367	1055.494535	13.268595
15.356558	1046.343607	13.273613
14.986563	1041.150839	13.278631
15.423225	1056.791474	13.283648
15.090801	1061.656541	13.288666
15.363789	1059.742951	13.293683
15.418480	1061.154858	13.298701
15.474141	1065.244430	13.303719
15.855864	1062.215967	13.308736
15.428042	1060.906243	13.313754
15.465451	1054.532026	13.318771
15.577165	1058.858724	13.323789
15.200681	1066.208557	13.328807
15.572737	1059.165357	13.333824
15.391276	1066.395376	13.338842
15.610791	1066.236653	13.343859
15.639099	1060.095826	13.348877
15.451149	1067.588723	13.353895
15.429515	1058.170527	13.358912
15.388743	1060.844305	13.363930
15.547097	1059.416676	13.368947
15.680902	1068.070994	13.373965
15.422804	1060.956561	13.378983
15.480548	1056.944598	13.384000
15.572097	1063.276915	13.389018
15.576365	1060.865891	13.394035
15.771985	1058.952563	13.399053
15.646630	1057.887431	13.404071
15.795929	1069.380376	13.409088
15.357672	1062.032909	13.414106
15.448875	1066.018546	13.419123
15.674868	1055.884027	13.424141
15.626047	1083.513084	13.429159
16.229433	1084.021230	13.434176
16.062857	1070.930439	13.439194
15.800014	1058.564682	13.444211
15.787927	1062.113572	13.449229
15.669611	1060.111882	13.454247
15.824226	1059.404524	13.459264
16.058212	1073.683656	13.464282
15.957158	1068.971349	13.469299
16.166767	1063.248789	13.474317
15.796268	1064.716805	13.479335
16.193370	1056.091172	13.484352
15.858808	1053.030204	13.489370
16.210344	1063.364387	13.494387
15.894756	1051.808545	13.499405
15.836847	1060.032542	13.504423
16.110500	1054.880415	13.509440
15.830138	1055.661433	13.514458
15.966313	1046.849659	13.519475
15.944942	1056.810017	13.524493
16.208469	1071.306273	13.529511
16.000484	1073.429134	13.534528
16.003866	1068.053829	13.539546
16.119141	1076.075828	13.544563
16.083920	1079.908869	13.549581
15.955461	1092.316463	13.554599
16.561763	1087.451930	13.559616
16.272561	1085.040472	13.564634
16.139932	1084.148586	13.569651
16.386590	1086.087617	13.574669
16.337720	1091.461441	13.579687
16.210047	1088.643229	13.584704
16.103403	1086.021120	13.589722
16.420749	1085.480011	13.594739
16.425003	1077.986938	13.599757
16.201633	1086.831731	13.604775
16.274473	1097.109904	13.609792
16.362439	1091.645731	13.614810
16.374194	1090.490093	13.619827
16.417626	1088.866613	13.624845
16.047394	1088.813003	13.629863
16.327290	1084.090123	13.634880
16.526330	1086.407130	13.639898
16.279682	1090.491842	13.644915
16.572233	1078.556170	13.649933
16.282807	1094.505319	13.654951
16.370880	1083.138252	13.659968
16.365041	1091.734302	13.664986
16.449842	1082.453117	13.670003
16.627394	1084.632757	13.675021
16.157095	1087.553518	13.680039
16.360637	1084.644428	13.685056
16.270967	1088.199920	13.690074
16.226400	1084.343533	13.695091
16.390759	1090.085439	13.700109
16.475210	1114.189804	13.705127
16.817572	1120.563522	13.710144
17.031574	1118.233370	13.715162
16.700847	1105.690285	13.720179
16.657648	1096.730354	13.725197
16.719519	1106.881622	13.730215
17.056389	1094.145299	13.735232
16.837890	1085.242464	13.740250
16.728779	1087.633526	13.745267
16.571238	1079.671306	13.750285
16.636867	1087.955882	13.755303
16.813916	1098.075008	13.760320
17.098948	1107.901007	13.765338
16.556319	1099.357933	13.770355
16.934357	1101.438112	13.775373
16.841978	1102.878012	13.780391
16.880364	1108.262141	13.785408
17.033165	1109.189656	13.790426
16.847051	1110.069178	13.795443
17.167874	1102.826610	13.800461
16.925378	1087.220981	13.805479
16.777381	1082.980623	13.810496
17.101078	1088.766907	13.815514
16.872874	1092.337160	13.820531
17.080104	1095.962590	13.825549
16.916536	1101.915693	13.830567
16.915517	1094.756545	13.835584
16.976682	1103.744202	13.840602
17.097141	1104.073182	13.845619
17.188612	1114.670696	13.850637
16.971769	1114.901813	13.855655
16.969660	1107.160582	13.860672
17.183574	1110.546726	13.865690
16.879634	1103.987113	13.870707
16.849566	1107.189411	13.875725
17.288996	1118.324339	13.880743
17.216641	1104.577336	13.885760
17.098504	1105.810110	13.890778
17.034500	1111.148270	13.895795
17.239824	1105.858670	13.900813
16.919886	1112.215312	13.905831
17.388275	1109.776345	13.910848
17.263607	1106.392695	13.915866
17.268304	1109.551028	13.920883
17.160140	1106.358720	13.925901
17.095363	1103.776890	13.930919
17.152549	1111.139696	13.935936
17.384145	1116.124405	13.940954
17.136829	1117.549905	13.945971
17.617123	1127.536365	13.950989
17.439475	1138.874267	13.956007
17.678816	1134.516366	13.961024
17.585396	1112.334640	13.966042
17.198609	1120.455467	13.971059
17.580594	1134.260862	13.976077
17.608942	1130.930116	13.981095
17.606744	1131.617660	13.986112
17.697241	1115.142908	13.991130
17.429270	1118.038311	13.996147
17.294815	1119.435602	14.001165
17.145341	1124.927337	14.006183
17.478542	1138.483769	14.011200
17.719632	1127.967969	14.016218
17.797255	1138.814247	14.021235
17.921126	1128.710827	14.026253
17.660843	1136.864177	14.031271
17.690174	1129.812168	14.036288
17.778976	1132.493160	14.041306
17.533807	1136.566222	14.046323
17.554798	1128.753033	14.051341
17.824350	1136.356130	14.056359
17.492759	1142.025773	14.061376
17.796458	1132.660538	14.066394
17.597530	1135.092125	14.071411
17.984114	1130.287328	14.076429
17.783341	1127.380082	14.081447
17.844807	1139.103418	14.086464
17.876516	1127.968906	14.091482
17.510677	1142.147811	14.096499
18.086572	1139.662625	14.101517
17.986936	1137.903872	14.106535
17.748923	1137.353895	14.111552
18.332633	1134.670569	14.116570
17.891499	1139.647427	14.121587
18.038932	1138.181844	14.126605
18.033018	1132.218716	14.131623
17.900810	1137.226503	14.136640
17.849343	1126.758939	14.141658
17.562792	1137.391745	14.146675
18.009732	1154.056711	14.151693
18.280665	1160.367124	14.156711
18.224831	1158.907374	14.161728
18.332674	1141.988784	14.166746
18.454533	1135.891430	14.171763
18.321470	1137.249910	14.176781
17.889264	1132.845765	14.181799
17.920599	1135.197348	14.186816
17.959301	1141.060549	14.191834
18.002582	1145.247471	14.196851
18.264282	1163.632929	14.201869
18.642569	1155.930804	14.206887
18.437869	1163.119063	14.211904
18.541916	1143.179967	14.216922
18.243655	1136.146581	14.221939
18.327849	1131.296775	14.226957
18.615335	1131.186987	14.231975
18.271180	1134.041515	14.236992
18.612921	1120.946109	14.242010
18.248172	1125.177226	14.247027
18.358296	1127.609802	14.252045
18.456901	1125.166553	14.257063
18.186069	1136.543169	14.262080
18.751955	1145.557188	14.267098
18.903806	1146.650211	14.272115
18.788052	1133.904448	14.277133
18.924577	1119.779813	14.282151
18.131076	1128.021395	14.287168
18.548810	1123.070089	14.292186
18.225776	1129.488666	14.297203
18.688406	1121.904816	14.302221
18.621202	1124.594809	14.307239
18.688721	1129.219805	14.312256
18.582284	1127.556667	14.317274
18.497470	1142.414815	14.322291
18.906157	1151.014040	14.327309
19.014982	1156.530566	14.332327
18.847756	1134.850032	14.337344
18.939442	1124.709840	14.342362
18.816085	1127.789466	14.347379
18.790058	1133.002034	14.352397
19.074754	1120.693241	14.357415
18.549207	1125.495551	14.362432
18.968057	1119.013813	14.367450
18.783828	1124.532190	14.372467
18.661738	1129.998903	14.377485
18.829898	1133.015902	14.382503
18.598514	1132.947087	14.387520
18.831808	1148.918063	14.392538
18.701158	1160.018650	14.397555
19.016676	1164.485904	14.402573
18.985343	1152.539052	14.407591
18.839241	1162.170224	14.412608
19.094548	1159.303695	14.417626
18.922965	1162.247649	14.422643
18.956223	1162.482074	14.427661
19.232839	1160.024584	14.432679
18.911104	1156.179605	14.437696
18.991157	1160.792685	14.442714
18.918266	1157.107910	14.447731
18.854459	1154.330249	14.452749
18.944295	1152.096318	14.457767
18.619316	1166.086572	14.462784
18.968275	1163.426513	14.467802
19.224465	1182.827042	14.472819
19.006903	1188.449797	14.477837
19.463101	1186.945485	14.482855
19.404898	1189.872173	14.487872
19.568055	1187.711086	14.492890
19.632314	1194.564508	14.497907
19.458008	1182.335110	14.502925
19.056754	1160.215900	14.507943
18.844514	1163.517385	14.512960
19.234906	1170.809481	14.517978
19.599491	1183.073780	14.522995
19.713795	1174.708072	14.528013
19.683658	1177.056494	14.533031
19.454449	1192.031993	14.538048
19.635089	1176.777970	14.543066
19.298277	1169.619093	14.548083
19.153649	1176.220231	14.553101
19.481687	1182.932169	14.558119
19.498611	1188.618700	14.563136
19.854734	1186.272001	14.568154
19.463767	1186.524187	14.573171
19.263267	1184.157415	14.578189
19.616816	1183.636663	14.583207
19.610888	1187.901852	14.588224
19.714998	1184.136864	14.593242
19.754258	1181.817639	14.598259
19.677109	1184.901800	14.603277
19.817696	1180.733128	14.608295
19.826008	1188.782019	14.613312
19.613215	1184.146908	14.618330
19.543405	1180.576572	14.623347
19.574946	1186.604359	14.628365
19.672275	1181.948409	14.633383
19.702452	1184.141537	14.638400
19.743708	1188.526043	14.643418
19.641695	1192.281241	14.648435
19.882711	1187.464797	14.653453
19.827899	1186.050148	14.658471
19.649231	1184.257677	14.663488
20.010862	1196.214223	14.668506
20.096317	1208.273768	14.673523
19.738263	1199.644841	14.678541
20.076870	1211.718607	14.683559
20.108634	1208.156577	14.688576
20.154492	1213.225338	14.693594
20.214410	1202.732516	14.698611
19.715644	1204.750978	14.703629
20.175307	1207.570332	14.708647
20.154909	1220.362808	14.713664
19.952876	1203.252359	14.718682
20.080790	1217.328398	14.723699
20.178583	1214.839995	14.728717
20.586734	1216.761648	14.733735
20.253744	1218.003766	14.738752
20.055142	1210.846305	14.743770
20.087685	1209.134468	14.748787
19.902005	1212.224076	14.753805
20.496946	1207.686973	14.758823
20.282326	1221.130212	14.763840
20.199775	1217.406479	14.768858
20.303553	1212.071127	14.773875
20.431785	1216.894317	14.778893
20.381392	1211.815291	14.783911
20.098640	1217.323699	14.788928
20.357173	1207.018718	14.793946
20.326599	1214.336320	14.798963
20.370068	1211.382556	14.803981
20.722424	1209.003804	14.808999
20.228057	1206.907126	14.814016
20.457659	1210.293834	14.819034
20.546128	1206.462940	14.824051
20.517285	1221.364220	14.829069
20.712037	1210.568282	14.834087
20.719140	1213.749857	14.839104
20.615562	1202.809032	14.844122
20.667199	1209.170876	14.849139
20.317908	1213.421101	14.854157
20.759533	1205.294266	14.859175
20.556883	1211.925141	14.864192
20.417792	1209.495405	14.869210
20.533415	1226.406063	14.874227
20.207412	1239.710358	14.879245
20.952848	1239.053602	14.884263
20.855929	1244.658686	14.889280
20.596941	1243.506702	14.894298
21.017682	1235.602212	14.899315
20.737179	1248.547783	14.904333
20.906466	1234.707746	14.909351
20.817374	1246.158167	14.914368
20.604909	1246.765709	14.919386
20.782860	1235.269029	14.924403
20.806013	1244.595357	14.929421
20.932354	1240.960908	14.934439
20.902323	1240.276754	14.939456
20.812729	1242.120914	14.944474
21.115477	1236.915073	14.949491
21.023535	1242.634679	14.954509
21.175762	1235.664159	14.959527
20.802177	1239.879848	14.964544
20.923524	1244.289245	14.969562
21.187925	1262.575557	14.974579
21.407476	1263.330575	14.979597
21.229881	1250.977265	14.984615
21.162580	1251.899249	14.989632
21.243088	1245.298507	14.994650
21.308301	1264.742299	14.999667
21.191210	1267.736662	15.004685
21.198669	1268.463944	15.009703
21.632833	1273.240631	15.014720
21.317883	1253.686775	15.019738
21.478353	1243.158315	15.024755
21.383422	1237.297342	15.029773
21.280148	1232.594408	15.034791
21.318795	1238.222230	15.039808
21.628889	1254.265979	15.044826
21.543049	1252.494290	15.049843
21.109120	1252.761492	15.054861
21.715062	1245.597839	15.059879
21.759621	1254.548582	15.064896
21.660353	1249.038706	15.069914
21.452631	1231.136288	15.074931
21.645639	1239.889912	15.079949
21.716737	1237.339804	15.084967
21.440376	1234.278179	15.089984
21.550752	1246.060786	15.095002
21.762689	1260.584693	15.100019
21.620940	1263.457173	15.105037
21.443632	1264.385633	15.110055
21.653199	1266.870597	15.115072
21.437540	1268.170773	15.120090
21.561195	1259.992434	15.125107
21.713095	1267.712393	15.130125
21.880078	1269.964286	15.135143
22.146271	1267.037662	15.140160
21.981155	1268.950676	15.145178
21.820613	1254.045797	15.150195
21.938417	1259.995498	15.155213
21.866088	1264.228833	15.160231
21.973355	1257.755917	15.165248
21.781105	1268.244401	15.170266
21.863332	1261.271332	15.175283
21.827592	1262.540421	15.180301
21.981715	1258.280111	15.185319
21.804964	1254.375971	15.190336
22.033903	1262.758688	15.195354
22.397685	1260.298111	15.200371
21.823495	1265.259330	15.205389
21.816101	1253.085988	15.210407
22.295797	1255.224486	15.215424
21.874306	1261.047300	15.220442
22.207471	1264.942772	15.225459
22.333827	1257.937173	15.230477
22.178163	1272.004887	15.235495
22.121522	1255.657195	15.240512
22.119066	1267.260942	15.245530
22.351067	1251.705406	15.250547
22.139717	1264.976099	15.255565
22.125311	1269.008475	15.260583
22.593938	1280.583141	15.265600
22.398880	1285.278206	15.270618
22.685243	1271.727720	15.275635
22.273574	1279.413017	15.280653
22.056696	1269.479919	15.285671
22.417213	1280.580052	15.290688
22.270651	1286.598507	15.295706
22.693194	1282.191611	15.300723
22.461128	1294.153217	15.305741
22.449635	1294.090369	15.310759
22.791462	1291.722016	15.315776
22.199137	1295.450079	15.320794
22.248023	1286.841256	15.325811
22.291659	1286.185799	15.330829
22.230812	1286.419334	15.335847
22.653184	1295.508475	15.340864
22.465224	1298.219751	15.345882
22.609645	1289.203327	15.350899
22.632407	1294.017695	15.355917
22.758911	1316.773698	15.360935
22.965719	1318.177273	15.365952
22.785057	1305.205551	15.370970
22.880520	1305.452867	15.375987
22.987861	1317.210049	15.381005
22.506746	1308.422782	15.386023
23.164520	1308.380576	15.391040
22.888790	1323.499363	15.396058
23.189357	1313.469993	15.401075
23.397804	1298.514763	15.406093
23.089048	1293.016071	15.411111
23.160070	1280.534014	15.416128
23.210313	1281.192769	15.421146
22.899515	1287.401510	15.426163
22.849974	1286.293053	15.431181
22.936012	1283.914463	15.436199
23.207464	1285.143123	15.441216
22.643649	1293.680460	15.446234
23.143445	1304.444478	15.451251
23.549610	1317.520058	15.456269
23.556548	1305.480115	15.461287
23.344456	1293.556900	15.466304
22.731508	1291.207882	15.471322
23.400505	1304.785809	15.476339
23.187460	1312.806993	15.481357
23.482825	1316.402866	15.486375
23.519679	1309.436923	15.491392
23.575544	1305.565362	15.496410
23.528462	1291.320307	15.501427
23.398144	1284.368383	15.506445
23.367146	1270.315943	15.511463
23.617369	1270.057630	15.516480
23.438547	1273.755538	15.521498
23.143719	1275.862942	15.526515
23.382836	1288.763514	15.531533
23.483194	1302.967041	15.536551
23.433149	1300.548472	15.541568
23.417177	1309.505765	15.546586
23.177150	1308.167952	15.551603
23.639984	1306.195612	15.556621
23.106178	1306.424693	15.561639
23.104540	1304.828366	15.566656
23.427307	1309.967664	15.571674
23.673623	1310.047391	15.576691
23.910978	1304.564218	15.581709
23.988449	1309.585238	15.586727
23.846395	1305.261157	15.591744
23.595725	1311.595736	15.596762
23.640752	1304.687884	15.601779
24.021350	1326.197374	15.606797
23.694085	1324.338250	15.611815
23.752945	1331.239478	15.616832
24.068986	1326.636105	15.621850
24.267777	1327.908340	15.626867
24.214186	1326.397810	15.631885
23.887511	1320.612725	15.636903
24.104216	1303.355795	15.641920
24.187361	1314.771733	15.646938
24.124971	1309.047051	15.651955
24.329513	1301.924897	15.656973
24.008128	1299.449071	15.661991
23.997564	1296.065704	15.667008
24.307348	1298.709207	15.672026
24.263103	1301.379667	15.677043
24.449937	1304.977829	15.682061
24.147163	1303.969727	15.687079
24.270912	1300.278217	15.692096
24.076360	1301.331587	15.697114
24.035201	1299.486327	15.702131
24.251367	1309.042021	15.707149
24.570073	1321.455784	15.712167
24.940888	1327.487075	15.717184
24.390063	1316.014228	15.722202
24.164743	1306.267544	15.727219
24.690765	1295.645217	15.732237
24.103594	1305.589941	15.737255
24.561083	1319.376259	15.742272
24.460863	1322.163898	15.747290
24.532417	1328.973255	15.752307
24.737401	1329.634637	15.757325
24.438558	1322.988652	15.762343
25.224213	1331.280840	15.767360
24.698486	1310.806857	15.772378
24.603823	1305.813108	15.777395
24.560926	1307.238897	15.782413
24.411371	1303.594388	15.787431
24.672436	1324.711553	15.792448
24.524811	1329.466461	15.797466
24.565443	1328.737488	15.802483
24.751941	1331.570381	15.807501
24.772160	1324.928841	15.812519
24.859753	1334.230339	15.817536
24.717789	1323.709576	15.822554
24.716295	1324.924947	15.827571
24.780718	1328.023005	15.832589
24.323345	1337.802084	15.837607
24.949729	1329.667702	15.842624
24.666480	1331.930663	15.847642
24.576842	1341.334851	15.852659
24.685107	1354.085186	15.857677
24.645481	1372.405627	15.862695
24.644472	1363.634980	15.867712
25.373205	1375.713713	15.872730
25.049716	1364.940031	15.877747
25.155501	1366.456069	15.882765
25.119429	1373.010507	15.887783
25.134213	1366.150961	15.892800
25.170615	1361.623190	15.897818
24.921380	1366.578458	15.902835
25.276070	1362.910749	15.907853
24.927594	1363.519644	15.912871
25.401006	1365.782821	15.917888
25.530206	1372.973549	15.922906
25.170935	1378.134901	15.927923
25.533901	1373.093804	15.932941
25.387569	1367.753122	15.937959
25.662678	1365.041527	15.942976
25.545367	1351.936798	15.947994
25.275689	1359.316258	15.953011
25.669597	1357.315212	15.958029
25.776382	1360.984959	15.963047
25.200056	1359.596744	15.968064
25.602085	1363.473709	15.973082
25.858678	1374.623073	15.978099
25.773533	1375.622044	15.983117
25.805080	1367.766431	15.988135
25.577243	1357.044963	15.993152
25.673947	1351.426888	15.998170
25.692291	1372.986027	16.003187
26.057163	1371.756714	16.008205
25.484009	1372.898215	16.013223
25.858818	1373.040047	16.018240
26.310335	1370.840453	16.023258
25.909275	1370.891568	16.028275
25.610967	1359.923158	16.033293
25.864517	1359.892237	16.038311
25.643801	1370.600477	16.043328
26.153175	1376.117431	16.048346
25.616295	1381.310666	16.053363
26.165898	1368.299790	16.058381
26.083533	1374.339104	16.063399
26.120513	1373.083585	16.068416
26.317043	1383.367373	16.073434
25.966981	1382.230122	16.078451
26.486539	1371.200168	16.083469
26.191569	1382.924667	16.088487
26.291626	1368.878307	16.093504
26.566693	1368.305635	16.098522
26.155252	1373.239836	16.103539
26.421977	1374.939749	16.108557
26.485825	1374.445491	16.113575
26.445225	1373.824504	16.118592
26.147849	1354.264843	16.123610
25.514641	1375.261436	16.128627
26.176236	1357.644680	16.133645
26.388769	1376.536975	16.138663
26.335695	1370.413883	16.143680
26.580687	1365.327833	16.148698
26.485113	1373.516132	16.153715
26.665561	1365.421997	16.158733
26.836098	1369.633496	16.163751
26.694791	1362.899105	16.168768
26.709648	1369.165557	16.173786
26.280401	1365.987589	16.178803
26.566167	1368.504786	16.183821
26.463731	1369.384980	16.188839
26.756185	1366.074850	16.193856
26.671844	1360.432535	16.198874
26.515509	1367.856544	16.203891
26.410289	1364.341655	16.208909
26.825952	1381.378591	16.213927
26.476782	1400.260345	16.218944
26.594250	1396.836778	16.223962
26.707963	1400.379008	16.228979
26.752476	1400.469445	16.233997
26.760315	1409.235440	16.239015
26.660707	1398.814275	16.244032
26.717019	1394.904036	16.249050
26.706872	1402.531315	16.254067
26.795345	1393.594994	16.259085
26.855415	1403.130630	16.264103
26.916168	1409.559544	16.269120
27.094150	1422.746368	16.274138
27.167482	1427.501192	16.279155
27.434818	1415.676537	16.284173
27.573462	1430.730489	16.289191
27.321173	1417.498537	16.294208
27.111010	1403.920627	16.299226
27.203811	1417.297584	16.304243
27.100888	1423.380884	16.309261
27.352012	1425.912115	16.314279
27.293455	1431.604195	16.319296
27.416046	1429.351394	16.324314
27.595680	1434.613736	16.329331
27.469416	1425.501284	16.334349
27.487273	1421.321452	16.339367
27.378537	1436.054332	16.344384
27.312758	1433.548990	16.349402
27.262885	1445.542239	16.354419
27.203333	1430.572374	16.359437
27.109881	1440.647712	16.364455
27.066298	1424.290191	16.369472
27.664201	1434.600997	16.374490
27.387266	1453.928279	16.379507
27.605889	1458.492038	16.384525
28.003423	1459.458028	16.389543
28.083967	1463.813642	16.394560
27.925478	1450.891261	16.399578
28.023056	1445.387572	16.404595
28.071606	1429.632827	16.409613
28.071563	1419.717921	16.414631
27.766911	1418.993581	16.419648
27.674662	1411.138051	16.424666
27.658255	1427.611438	16.429683
27.968804	1443.141541	16.434701
27.926089	1443.491747	16.439719
27.827650	1452.031736	16.444736
27.960362	1452.946470	16.449754
28.207305	1459.742086	16.454771
28.336585	1455.170112	16.459789
28.221007	1447.251119	16.464807
28.158974	1455.498845	16.469824
28.545545	1444.846055	16.474842
28.320786	1450.190579	16.479859
28.502186	1453.736531	16.484877
28.910716	1438.842789	16.489895
28.281015	1430.266758	16.494912
28.671679	1416.284253	16.499930
28.481933	1411.804293	16.504947
28.294675	1399.087125	16.509965
28.541273	1406.245364	16.514983
28.370686	1410.856085	16.520000
28.113662	1394.909260	16.525018
28.547510	1408.483059	16.530035
28.160645	1409.988470	16.535053
28.636395	1420.045955	16.540071
28.650644	1437.443368	16.545088
28.887935	1433.343986	16.550106
28.268966	1413.930615	16.555123
28.173858	1428.587209	16.560141
28.593227	1443.525223	16.565159
28.364008	1440.157303	16.570176
28.604847	1438.496643	16.575194
28.368714	1442.412773	16.580211
28.589616	1439.857417	16.585229
28.527640	1439.724221	16.590247
27.974669	1441.534797	16.595264
28.249495	1456.324412	16.600282
28.426893	1472.791223	16.605299
28.505352	1477.593635	16.610317
28.760381	1466.396565	16.615335
28.540042	1477.485122	16.620352
28.915138	1485.497217	16.625370
28.907828	1507.485994	16.630387
28.839798	1510.782873	16.635405
29.158729	1503.410122	16.640423
29.050128	1514.426197	16.645440
29.306787	1504.747304	16.650458
29.508601	1498.737303	16.655475
29.494970	1502.392454	16.660493
29.492228	1497.203053	16.665511
29.383327	1507.080219	16.670528
29.550112	1501.987045	16.675546
29.536249	1496.901854	16.680563
29.572825	1493.549190	16.685581
29.369717	1474.859123	16.690599
29.202216	1473.996238	16.695616
29.408644	1490.661389	16.700634
29.310526	1497.438000	16.705651
29.671877	1508.892483	16.710669
29.479638	1501.807449	16.715687
29.577266	1506.116929	16.720704
29.562157	1505.151155	16.725722
29.385628	1495.476555	16.730739
29.443237	1509.701156	16.735757
29.663479	1494.430791	16.740775
29.384626	1506.449549	16.745792
29.454838	1509.712032	16.750810
29.569710	1493.637151	16.755827
29.584828	1506.208215	16.760845
29.854964	1493.018495	16.765863
30.027085	1511.740511	16.770880
29.792081	1500.706755	16.775898
30.038493	1511.339416	16.780915
29.969024	1510.116934	16.785933
30.232169	1498.268897	16.790951
29.909528	1510.281550	16.795968
29.981226	1497.574801	16.800986
29.768811	1502.078331	16.806003
29.786757	1514.831606	16.811021
30.024980	1522.720411	16.816039
30.095393	1538.598000	16.821056
30.438597	1533.687694	16.826074
30.298274	1528.806579	16.831091
30.202858	1537.550440	16.836109
30.723278	1527.626908	16.841127
30.337680	1529.117552	16.846144
30.452389	1525.889687	16.851162
30.687734	1512.940375	16.856179
30.014412	1508.878947	16.861197
30.285931	1509.065114	16.866215
30.045799	1529.724537	16.871232
30.130543	1535.214099	16.876250
30.249988	1532.466934	16.881267
29.907551	1536.830671	16.886285
30.499859	1527.241247	16.891303
30.122874	1533.548486	16.896320
30.167570	1533.522359	16.901338
30.627669	1540.028255	16.906355
30.343201	1567.093415	16.911373
30.372156	1555.350402	16.916391
30.328537	1571.743033	16.921408
30.230219	1562.073895	16.926426
30.811690	1563.484903	16.931443
30.288417	1570.528666	16.936461
30.578515	1566.811411	16.941479
30.517814	1580.853777	16.946496
30.716835	1588.488112	16.951514
31.414468	1590.307368	16.956531
31.127243	1592.039144	16.961549
31.277281	1587.759346	16.966567
31.283313	1598.465879	16.971584
31.271577	1582.022585	16.976602
31.222568	1567.505554	16.981619
30.844012	1569.649352	16.986637
30.993791	1572.461623	16.991655
31.178610	1578.805419	16.996672
31.155149	1595.121103	17.001690
31.324156	1592.245612	17.006707
31.308545	1588.532710	17.011725
31.448013	1576.343365	17.016743
31.401773	1594.793513	17.021760
31.375495	1586.188356	17.026778
31.743130	1590.201802	17.031795
31.287148	1597.047387	17.036813
31.510553	1586.877520	17.041831
31.559739	1590.896261	17.046848
31.553594	1595.809621	17.051866
31.698409	1591.309039	17.056883
31.419128	1588.660815	17.061901
31.594813	1582.048834	17.066919
31.672671	1587.285626	17.071936
31.567428	1584.758866	17.076954
31.793964	1587.869006	17.081971
31.483887	1593.121856	17.086989
31.391921	1595.201094	17.092007
31.469376	1586.213738	17.097024
31.445086	1590.387210	17.102042
31.544071	1584.668280	17.107059
31.500302	1595.385451	17.112077
31.674761	1608.017513	17.117095
31.783485	1619.761310	17.122112
31.822777	1618.514442	17.127130
32.029157	1615.638641	17.132147
32.090509	1620.523467	17.137165
31.960196	1615.148934	17.142183
32.371912	1620.163317	17.147200
32.023228	1624.893073	17.152218
32.337604	1613.583278	17.157235
31.955496	1618.234730	17.162253
32.202206	1616.300245	17.167271
32.241016	1627.586776	17.172288
32.276650	1621.035853	17.177306
32.412691	1617.389861	17.182323
31.838588	1624.243280	17.187341
32.201187	1629.667795	17.192359
32.167004	1629.370530	17.197376
32.226431	1638.928072	17.202394
32.248279	1649.276897	17.207411
32.610042	1657.723972	17.212429
32.736956	1657.698352	17.217447
32.605424	1654.489343	17.222464
32.253090	1649.915473	17.227482
32.542940	1657.423723	17.232499
32.475920	1648.821366	17.237517
32.425559	1654.374764	17.242535
32.734884	1648.325971	17.247552
32.581882	1654.678706	17.252570
33.121317	1649.290476	17.257587
32.732561	1652.368649	17.262605
32.417881	1642.102753	17.267623
32.550118	1651.079701	17.272640
32.104726	1671.225796	17.277658
32.779622	1670.657524	17.282675
32.939517	1683.346004	17.287693
32.952699	1682.581421	17.292711
32.767780	1680.988354	17.297728
32.679821	1692.307420	17.302746
33.272282	1681.385210	17.307763
33.132208	1687.608251	17.312781
33.224544	1682.713613	17.317799
33.255052	1681.058755	17.322816
32.996301	1672.341797	17.327834
33.252406	1671.805339	17.332851
33.055863	1676.816906	17.337869
33.064882	1682.040762	17.342887
33.468513	1697.714703	17.347904
33.698810	1708.369470	17.352922
33.541889	1706.462299	17.357939
33.458184	1698.894571	17.362957
33.390584	1701.218197	17.367975
33.428031	1707.073553	17.372992
33.496143	1706.023068	17.378010
33.996193	1702.096082	17.383027
33.713498	1702.381457	17.388045
33.367740	1702.195034	17.393063
33.478079	1703.041062	17.398080
33.548506	1713.157841	17.403098
33.598724	1709.711919	17.408115
33.748702	1699.943551	17.413133
33.694023	1701.990621	17.418151
33.636182	1696.865430	17.423168
33.386671	1703.814930	17.428186
33.886679	1702.821792	17.433203
33.999668	1714.803926	17.438221
33.617823	1732.769865	17.443239
34.156105	1730.409739	17.448256
34.354014	1741.329753	17.453274
34.354317	1731.209080	17.458291
34.449306	1732.503328	17.463309
34.145313	1707.475449	17.468327
34.738793	1701.237673	17.473344
34.049750	1703.746874	17.478362
34.312287	1691.872414	17.483379
34.299376	1696.986535	17.488397
34.206288	1692.947905	17.493415
34.596570	1685.306518	17.498432
34.284454	1701.297067	17.503450
34.218952	1703.632549	17.508467
34.564112	1726.075251	17.513485
34.375260	1729.161944	17.518503
34.598094	1728.796368	17.523520
34.579256	1732.045353	17.528538
34.656305	1719.847373	17.533555
34.715375	1732.817219	17.538573
34.772403	1716.820618	17.543591
35.038910	1720.146582	17.548608
34.538132	1725.468573	17.553626
34.888150	1715.191752	17.558643
35.018284	1717.787237	17.563661
34.825876	1716.211946	17.568679
35.049918	1719.120954	17.573696
34.836616	1722.246749	17.578714
34.872158	1717.750514	17.583731
35.011732	1725.660938	17.588749
34.943984	1720.552346	17.593767
35.064780	1715.125017	17.598784
35.108432	1720.352972	17.603802
34.966858	1723.741647	17.608819
35.186951	1722.744246	17.613837
34.785966	1724.405969	17.618855
35.198546	1726.365928	17.623872
34.701718	1722.033770	17.628890
34.779493	1724.526935	17.633907
35.259515	1714.105672	17.638925
34.971115	1727.816334	17.643943
35.209853	1734.776033	17.648960
35.108226	1736.975005	17.653978
35.607153	1744.007997	17.658995
35.626109	1740.556240	17.664013
35.818330	1751.005161	17.669031
35.731037	1743.608873	17.674048
35.405571	1747.443864	17.679066
35.650323	1748.482513	17.684083
35.656751	1742.480092	17.689101
35.429099	1742.783090	17.694119
35.861722	1743.088940	17.699136
35.980911	1745.839398	17.704154
35.987805	1744.713259	17.709171
36.011094	1736.133244	17.714189
36.012985	1738.440601	17.719207
36.086342	1737.899082	17.724224
36.159797	1745.980742	17.729242
35.828854	1750.298139	17.734259
36.004250	1736.473963	17.739277
35.621208	1741.571667	17.744295
36.170003	1737.010589	17.749312
35.550145	1741.872066	17.754330
35.863738	1735.585917	17.759347
36.076362	1743.353893	17.764365
35.651021	1740.285433	17.769383
36.183963	1758.467461	17.774400
36.147245	1753.078111	17.779418
36.500018	1769.894827	17.784435
36.477826	1774.237290	17.789453
36.160503	1775.303224	17.794471
36.695600	1769.007803	17.799488
36.745262	1764.651727	17.804506
36.692729	1770.623637	17.809523
37.003243	1765.178143	17.814541
36.189839	1747.782097	17.819559
36.489325	1751.388805	17.824576
36.651219	1765.520324	17.829594
36.587315	1761.603202	17.834611
36.571157	1763.822224	17.839629
36.386861	1764.629039	17.844647
36.586945	1765.079839	17.849664
36.409888	1769.751978	17.854682
36.939315	1767.264185	17.859699
36.672382	1765.193010	17.864717
36.604894	1763.676478	17.869735
36.891388	1768.146765	17.874752
36.630280	1786.281280	17.879770
36.826628	1795.423247	17.884787
37.552720	1791.484653	17.889805
37.198906	1790.892480	17.894823
37.390547	1775.585255	17.899840
37.209581	1781.871824	17.904858
37.153172	1786.377851	17.909875
37.301467	1782.036085	17.914893
37.217792	1782.714365	17.919911
37.203692	1775.434636	17.924928
37.350881	1782.338313	17.929946
37.226466	1783.971002	17.934963
37.564852	1779.045279	17.939981
37.268888	1786.506080	17.944999
37.321018	1777.930697	17.950016
37.332859	1775.530114	17.955034
37.538353	1779.749301	17.960051
37.715640	1773.749177	17.965069
37.798596	1785.941083	17.970087
37.596164	1780.568637	17.975104
37.703581	1776.592721	17.980122
37.616399	1780.031816	17.985139
37.795678	1774.841990	17.990157
37.575908	1783.457052	17.995175
37.840405	1774.522357	18.000192
37.794192	1790.537699	18.005210
37.754611	1803.201953	18.010227
37.960546	1806.753358	18.015245
38.172579	1811.274616	18.020263
37.845077	1808.617833	18.025280
37.630326	1809.308058	18.030298
37.622522	1814.341841	18.035315
38.366761	1804.445500	18.040333
37.927587	1812.118306	18.045351
38.079168	1809.178349	18.050368
38.284924	1807.417577	18.055386
38.192931	1810.011021	18.060403
38.565425	1812.267813	18.065421
38.662701	1824.297132	18.070439
38.558547	1817.401250	18.075456
38.515066	1805.189772	18.080474
38.598141	1797.902149	18.085491
38.776819	1799.845878	18.090509
38.635525	1798.020744	18.095527
38.344175	1803.431574	18.100544
38.149817	1818.364481	18.105562
38.434331	1820.574086	18.110579
38.517803	1822.413564	18.115597
39.026735	1818.290192	18.120615
38.944947	1826.316595	18.125632
38.967576	1826.870121	18.130650
38.867509	1831.009402	18.135667
38.908775	1825.338954	18.140685
38.885846	1823.778789	18.145703
39.199338	1821.323730	18.150720
39.083312	1818.539275	18.155738
38.902821	1822.348219	18.160755
39.151946	1819.959371	18.165773
39.211963	1816.024394	18.170791
38.871703	1820.094146	18.175808
38.964340	1813.790360	18.180826
39.045386	1832.863729	18.185843
39.364328	1845.121182	18.190861
39.544272	1860.460814	18.195879
39.730158	1846.539520	18.200896
39.921302	1837.093359	18.205914
39.640767	1830.422851	18.210931
39.828919	1813.068921	18.215949
39.608248	1818.738088	18.220967
39.507418	1820.522372	18.225984
39.819822	1816.208437	18.231002
39.315106	1818.544104	18.236019
39.830462	1811.228718	18.241037
39.468364	1805.317054	18.246055
39.382254	1818.455984	18.251072
39.898898	1836.944357	18.256090
39.825676	1844.912259	18.261107
39.816576	1846.166337	18.266125
39.938851	1846.000150	18.271143
39.872569	1854.298794	18.276160
39.853986	1844.559927	18.281178
39.825478	1841.882575	18.286195
39.764311	1840.517742	18.291213
39.991012	1836.375921	18.296231
39.697487	1851.778493	18.301248
40.001403	1843.257681	18.306266
40.304218	1846.135904	18.311283
40.091951	1857.733233	18.316301
40.745624	1864.007486	18.321319
40.396983	1869.284160	18.326336
40.547379	1853.946705	18.331354
40.268118	1852.522057	18.336371
40.625051	1856.190502	18.341389
40.478313	1868.354115	18.346407
40.263368	1869.493589	18.351424
40.237175	1869.530032	18.356442
40.655836	1871.548450	18.361459
40.669068	1865.764536	18.366477
41.041068	1874.360030	18.371495
40.767626	1868.741874	18.376512
41.133047	1860.826974	18.381530
41.275309	1866.429142	18.386547
41.528063	1859.503446	18.391565
41.456695	1845.678849	18.396583
41.129220	1840.259449	18.401600
41.124660	1839.100167	18.406618
40.835613	1831.766111	18.411635
41.099671	1825.098001	18.416653
41.260133	1824.338458	18.421671
41.062975	1826.600565	18.426688
41.296698	1821.870572	18.431706
41.286038	1826.445779	18.436723
41.047330	1835.354569	18.441741
41.519706	1848.666053	18.446759
41.139460	1853.017656	18.451776
41.506644	1854.715493	18.456794
41.596551	1853.985787	18.461811
41.513815	1850.206025	18.466829
41.418791	1858.346456	18.471847
41.461797	1854.665873	18.476864
41.448449	1848.957249	18.481882
41.638162	1856.677517	18.486899
41.591601	1861.413820	18.491917
41.447775	1849.384734	18.496935
41.689820	1851.347465	18.501952
41.684510	1856.111556	18.506970
41.436925	1863.315926	18.511987
41.618196	1877.765194	18.517005
41.806149	1878.899121	18.522023
41.543470	1896.212367	18.527040
42.038288	1879.829839	18.532058
42.160381	1891.585793	18.537075
42.174628	1883.785550	18.542093
42.209909	1887.661797	18.547111
42.109959	1888.749088	18.552128
42.093816	1883.766905	18.557146
41.960384	1894.431074	18.562163
41.863335	1893.994253	18.567181
42.252872	1894.207268	18.572199
42.168003	1908.973243	18.577216
42.145091	1913.289486	18.582234
42.483768	1921.494873	18.587251
42.728902	1919.896049	18.592269
42.646573	1913.585870	18.597287
42.654727	1909.274842	18.602304
43.317070	1909.126370	18.607322
42.988152	1897.432738	18.612339
42.792477	1882.450022	18.617357
42.724493	1872.111078	18.622375
42.572763	1884.977899	18.627392
42.686545	1883.805244	18.632410
42.881948	1905.554985	18.637427
42.601298	1914.363704	18.642445
42.813410	1899.792330	18.647463
42.647269	1916.627346	18.652480
42.892936	1908.161063	18.657498
42.698549	1903.508502	18.662515
42.838215	1901.401222	18.667533
42.951472	1915.220093	18.672551
42.859210	1936.082644	18.677568
43.094618	1926.890097	18.682586
43.290750	1943.709811	18.687603
43.387717	1932.443402	18.692621
43.786121	1934.857718	18.697639
43.665154	1943.223373	18.702656
43.827019	1926.942987	18.707674
44.135166	1923.826197	18.712691
44.083469	1912.097107	18.717709
43.882512	1902.883007	18.722727
43.736253	1903.470513	18.727744
44.156865	1891.539706	18.732762
44.144522	1884.467115	18.737779
43.779038	1888.775330	18.742797
44.135112	1885.461604	18.747815
43.746640	1891.421681	18.752832
43.951071	1891.839086	18.757850
43.869555	1894.824505	18.762867
43.882128	1887.326903	18.767885
43.946687	1881.776973	18.772903
43.551166	1896.981581	18.777920
44.095246	1906.939445	18.782938
44.178361	1921.925939	18.787955
43.902264	1924.152755	18.792973
44.545383	1922.192110	18.797991
44.307540	1932.973267	18.803008
44.191483	1924.487570	18.808026
44.316849	1924.907487	18.813043
44.257269	1937.245251	18.818061
44.366206	1927.144583	18.823079
44.510314	1930.590938	18.828096
44.351857	1929.082423	18.833114
44.658515	1923.119007	18.838131
44.324520	1931.077934	18.843149
44.646491	1920.257210	18.848167
44.142543	1928.904232	18.853184
44.607513	1944.196966	18.858202
44.525023	1951.688900	18.863219
44.193236	1959.971493	18.868237
44.386755	1948.529968	18.873255
44.696159	1966.321046	18.878272
44.753849	1977.400361	18.883290
45.301451	1983.941903	18.888307
45.089242	1991.295178	18.893325
45.142479	1978.174171	18.898343
45.196955	1987.264241	18.903360
45.173377	1986.847489	18.908378
45.431898	1979.487311	18.913395
45.220371	1986.923543	18.918413
45.184632	1979.567786	18.923431
45.110882	1989.766978	18.928448
45.246574	1990.334789	18.933466
45.391441	1987.686863	18.938483
45.018762	1989.493909	18.943501
45.537878	1991.023594	18.948519
45.509627	2008.055084	18.953536
45.454176	2017.007929	18.958554
45.731613	2016.559254	18.963571
45.555027	2023.055430	18.968589
45.770406	2009.760200	18.973607
45.710388	2022.761500	18.978624
45.684841	2022.775001	18.983642
45.823677	2015.387062	18.988659
45.950204	2011.177592	18.993677
46.325818	2013.198066	18.998695
45.887739	2006.101692	19.003712
45.956689	2016.550415	19.008730
46.232512	2005.627853	19.013747
46.209487	2005.489358	19.018765
46.240466	1998.975664	19.023783
46.451397	2012.519723	19.028800
46.574092	2009.171532	19.033818
46.359727	2013.568050	19.038835
46.055606	2010.554190	19.043853
46.272181	2017.141711	19.048871
46.308770	2036.583749	19.053888
46.332662	2047.031320	19.058906
46.641117	2038.988002	19.063923
46.340278	2039.933493	19.068941
46.947327	2041.593452	19.073959
46.517561	2041.359567	19.078976
46.352203	2045.836927	19.083994
46.810742	2040.735244	19.089011
46.684756	2045.056451	19.094029
46.875861	2062.162173	19.099047
47.143469	2062.412780	19.104064
47.204254	2068.325024	19.109082
47.484459	2058.900934	19.114099
47.198564	2061.129004	19.119117
47.497064	2056.847237	19.124135
47.032831	2032.424608	19.129152
47.176632	2038.891950	19.134170
47.577395	2044.287040	19.139187
47.259446	2065.411689	19.144205
47.472374	2065.085155	19.149223
47.723163	2058.916797	19.154240
47.527498	2062.095240	19.159258
47.641785	2056.972423	19.164275
47.702469	2050.435659	19.169293
47.573997	2049.271760	19.174311
47.949331	2055.391171	19.179328
47.769864	2049.020310	19.184346
48.081529	2054.302652	19.189363
47.847826	2057.050401	19.194381
47.821575	2049.676105	19.199399
47.948994	2062.939596	19.204416
47.599181	2053.700541	19.209434
48.270376	2058.672335	19.214451
48.194924	2054.539339	19.219469
47.905029	2056.605866	19.224487
47.826063	2045.994217	19.229504
47.726911	2057.353205	19.234522
47.879999	2055.652342	19.239539
47.856445	2061.099460	19.244557
48.060443	2077.175479	19.249575
48.348087	2085.036279	19.254592
48.141624	2090.696883	19.259610
48.548636	2080.404050	19.264627
48.217196	2086.555512	19.269645
48.576455	2079.385635	19.274663
48.480960	2091.425549	19.279680
48.294688	2083.400655	19.284698
48.316479	2090.491852	19.289715
48.479222	2106.864134	19.294733
48.831143	2106.347564	19.299751
49.493249	2098.776154	19.304768
49.062481	2105.315400	19.309786
49.443116	2095.111588	19.314803
48.998025	2080.600459	19.319821
48.992358	2077.610603	19.324839
49.481309	2091.364431	19.329856
49.497389	2086.848489	19.334874
49.316521	2074.463962	19.339891
48.932627	2070.918063	19.344909
49.149023	2084.640020	19.349927
49.236562	2090.694286	19.354944
49.272164	2093.927999	19.359962
49.479172	2093.959542	19.364979
49.262560	2096.172557	19.369997
48.985461	2102.455941	19.375015
49.367184	2096.985898	19.380032
49.155478	2102.133588	19.385050
49.102533	2105.693445	19.390067
49.541792	2127.581316	19.395085
49.333272	2129.496528	19.400103
49.770716	2130.526406	19.405120
49.623046	2132.765371	19.410138
49.818190	2132.748490	19.415155
49.898590	2127.766325	19.420173
49.982403	2128.777812	19.425191
50.289841	2123.402393	19.430208
50.494720	2136.712522	19.435226
50.605152	2124.512220	19.440243
50.524205	2113.390214	19.445261
50.411916	2117.213878	19.450279
50.711511	2116.065442	19.455296
50.273446	2120.414917	19.460314
50.496550	2108.504174	19.465331
50.225342	2121.173328	19.470349
50.487104	2121.675701	19.475367
50.963231	2114.347798	19.480384
50.335820	2123.076471	19.485402
50.503983	2109.863808	19.490419
50.616600	2126.894849	19.495437
50.790720	2137.358064	19.500455
50.943174	2131.038696	19.505472
50.725442	2141.485151	19.510490
51.260155	2133.447880	19.515507
50.840342	2136.940765	19.520525
50.724253	2133.121595	19.525543
50.897811	2131.994106	19.530560
50.914493	2125.929594	19.535578
51.318787	2127.263413	19.540595
51.110136	2130.649545	19.545613
51.067662	2141.951535	19.550631
51.482969	2131.863594	19.555648
51.016198	2141.578985	19.560666
51.133089	2157.240028	19.565683
51.182061	2170.045378	19.570701
51.319941	2170.015968	19.575719
51.792713	2169.529705	19.580736
51.542101	2165.507291	19.585754
51.938740	2158.342582	19.590771
51.780802	2163.532932	19.595789
51.888750	2163.073053	19.600807
51.860264	2157.010132	19.605824
51.616602	2165.108103	19.610842
51.732630	2164.689009	19.615859
51.591340	2160.448814	19.620877
51.744769	2181.845675	19.625895
52.023690	2181.556202	19.630912
51.939655	2185.002344	19.635930
52.040740	2184.094382	19.640947
52.196015	2185.147541	19.645965
52.357741	2182.488118	19.650983
52.059799	2191.311678	19.656000
52.380279	2186.759680	19.661018
52.719109	2179.928988	19.666035
52.849986	2179.346004	19.671053
52.830877	2186.351914	19.676071
53.088521	2179.540228	19.681088
52.751122	2170.458492	19.686106
52.785663	2172.748674	19.691123
53.087745	2172.464014	19.696141
52.638911	2176.850729	19.701159
53.225938	2159.747447	19.706176
53.183279	2171.966834	19.711194
53.196615	2175.597188	19.716211
53.351704	2177.253935	19.721229
52.921969	2174.554234	19.726247
53.135317	2172.005921	19.731264
53.210220	2176.311492	19.736282
53.168769	2178.087915	19.741299
53.569329	2178.865260	19.746317
53.379828	2191.837433	19.751335
53.672437	2180.225327	19.756352
53.298267	2170.225665	19.761370
53.350902	2174.132564	19.766387
53.258582	2174.657569	19.771405
53.118244	2169.610501	19.776423
53.524154	2168.982986	19.781440
53.185781	2183.389378	19.786458
53.621537	2188.109396	19.791475
53.709960	2204.153181	19.796493
53.650663	2200.265892	19.801511
53.868588	2198.920389	19.806528
53.604211	2204.261911	19.811546
53.967735	2198.145629	19.816563
54.043309	2194.416638	19.821581
54.051836	2205.174357	19.826599
54.030289	2203.271790	19.831616
54.073252	2221.833450	19.836634
54.193339	2230.422587	19.841651
54.246948	2227.909083	19.846669
53.932804	2241.655185	19.851687
54.225425	2233.216750	19.856704
54.061372	2230.442171	19.861722
54.446440	2241.295603	19.866739
54.547168	2247.471363	19.871757
54.673497	2261.117499	19.876775
55.150616	2247.678954	19.881792
55.413889	2240.000927	19.886810
55.352951	2228.868032	19.891827
55.583092	2209.494422	19.896845
55.384429	2209.226058	19.901863
55.664852	2205.553177	19.906880
55.403596	2206.801949	19.911898
54.884779	2211.129437	19.916915
55.203106	2205.859269	19.921933
55.289596	2197.714963	19.926951
55.388400	2198.351120	19.931968
55.332427	2206.336025	19.936986
55.291933	2206.980374	19.942003
55.486114	2206.357339	19.947021
55.187483	2213.186879	19.952039
55.645194	2212.725561	19.957056
55.739977	2207.330732	19.962074
55.602376	2205.312016	19.967091
55.610052	2202.682526	19.972109
55.240137	2207.925052	19.977127
55.400489	2205.277666	19.982144
55.496743	2213.288062	19.987162
55.495909	2227.540360	19.992179
55.733911	2242.519531	19.997197
55.485898	2242.524337	20.002215
55.467491	2238.736938	20.007232
55.623391	2252.088380	20.012250
55.930965	2266.142991	20.017267
56.003848	2263.300678	20.022285
55.909734	2272.763654	20.027303
56.112252	2265.891406	20.032320
56.595050	2268.579948	20.037338
56.334614	2266.987952	20.042355
56.728466	2266.454566	20.047373
56.374769	2276.951664	20.052391
56.817904	2292.837369	20.057408
56.838688	2296.349187	20.062426
56.749535	2304.834555	20.067443
56.923724	2307.227929	20.072461
56.845779	2294.742651	20.077479
56.974530	2302.967778	20.082496
57.251669	2298.851313	20.087514
57.317726	2296.462899	20.092531
57.412636	2302.840442	20.097549
57.293354	2302.895901	20.102567
56.948308	2297.572570	20.107584
57.175260	2298.507126	20.112602
56.850531	2307.386780	20.117619
57.126765	2301.450326	20.122637
57.306047	2301.072292	20.127655
57.281149	2310.469060	20.132672
57.482681	2298.074341	20.137690
56.977658	2303.827166	20.142707
57.554257	2306.215075	20.147725
57.681641	2332.465450	20.152743
57.710901	2327.602354	20.157760
57.689907	2331.082933	20.162778
57.519046	2334.630155	20.167795
57.438164	2331.859451	20.172813
57.543034	2336.387258	20.177831
57.584968	2356.191418	20.182848
57.719433	2359.428834	20.187866
57.744171	2364.448726	20.192883
58.037075	2360.218202	20.197901
57.945881	2364.455365	20.202919
58.442464	2374.980897	20.207936
58.695021	2374.772972	20.212954
58.826689	2380.655444	20.217971
58.877400	2371.367738	20.222989
58.793055	2357.091283	20.228007
58.681023	2346.958169	20.233024
59.080833	2339.480242	20.238042
58.970498	2343.366632	20.243059
59.321659	2350.095318	20.248077
59.068617	2343.356235	20.253095
58.913472	2345.582298	20.258112
59.408422	2335.773913	20.263130
58.891614	2341.346813	20.268147
59.276253	2339.786969	20.273165
59.052135	2335.804595	20.278183
59.080591	2341.254190	20.283200
59.241511	2343.175350	20.288218
59.029995	2344.826510	20.293235
59.346771	2345.107929	20.298253
59.607183	2355.493955	20.303271
59.354710	2367.034169	20.308288
59.524696	2365.589923	20.313306
59.157981	2378.573988	20.318323
59.633540	2375.492674	20.323341
59.651879	2380.636867	20.328359
59.540247	2385.211696	20.333376
59.608342	2373.354863	20.338394
59.514885	2378.946786	20.343411
59.594370	2388.437280	20.348429
59.834091	2396.991664	20.353447
59.854481	2402.218598	20.358464
60.275670	2397.289945	20.363482
60.384332	2399.585165	20.368499
60.369817	2400.427968	20.373517
60.631248	2399.539408	20.378535
60.305281	2398.319327	20.383552
60.369069	2392.669733	20.388570
60.425292	2402.789717	20.393587
60.448222	2394.278693	20.398605
60.858947	2393.719664	20.403623
60.500866	2402.709249	20.408640
60.753453	2392.409200	20.413658
60.441733	2391.618659	20.418675
60.825618	2399.501421	20.423693
61.265977	2410.995808	20.428711
61.064978	2424.625230	20.433728
61.408287	2417.254692	20.438746
61.099945	2421.233856	20.443763
61.445037	2421.054253	20.448781
61.241250	2416.094819	20.453799
60.904845	2430.050306	20.458816
61.283012	2413.575580	20.463834
61.229256	2431.121241	20.468851
61.083641	2420.658608	20.473869
61.161340	2415.947676	20.478887
61.449668	2418.977635	20.483904
61.581028	2417.033485	20.488922
61.621612	2440.161337	20.493939
61.744999	2447.904735	20.498957
61.649935	2448.591630	20.503975
61.621687	2452.374241	20.508992
61.708815	2441.673296	20.514010
61.416080	2446.890080	20.519027
61.820195	2452.680838	20.524045
62.242371	2454.877106	20.529063
62.332086	2468.972837	20.534080
62.791606	2463.404695	20.539098
62.937279	2460.835693	20.544115
62.651849	2439.188728	20.549133
62.824113	2437.646455	20.554151
62.406473	2423.924960	20.559168
62.759241	2420.412453	20.564186
62.678111	2433.009714	20.569203
62.745649	2427.740995	20.574221
62.878457	2426.795856	20.579239
62.545681	2438.917210	20.584256
62.840294	2439.926754	20.589274
62.988884	2462.767780	20.594291
63.239396	2455.618169	20.599309
63.159965	2461.971602	20.604327
62.928549	2462.178382	20.609344
63.157368	2455.991079	20.614362
63.248713	2460.756613	20.619379
63.093748	2461.267235	20.624397
63.501165	2453.286394	20.629415
63.240831	2467.796224	20.634432
63.556313	2448.673105	20.639450
63.000472	2451.629588	20.644467
62.997520	2459.041614	20.649485
63.479524	2480.193323	20.654503
63.178826	2489.175782	20.659520
63.394170	2490.163858	20.664538
63.560836	2493.436110	20.669555
63.129390	2487.706581	20.674573
63.437507	2507.819858	20.679591
63.458496	2511.662020	20.684608
63.685592	2513.189901	20.689626
64.130704	2530.096040	20.694643
64.320100	2537.536766	20.699661
64.644055	2530.945020	20.704679
64.847234	2522.767764	20.709696
64.954625	2513.911125	20.714714
65.060877	2502.792767	20.719731
64.752269	2489.138136	20.724749
65.293020	2484.620312	20.729767
64.869982	2491.830508	20.734784
64.880651	2478.763400	20.739802
64.845177	2480.253419	20.744819
64.546927	2484.885674	20.749837
64.624949	2470.753000	20.754855
64.663496	2496.171137	20.759872
64.914639	2509.126638	20.764890
65.182533	2516.643288	20.769907
65.150304	2525.021673	20.774925
65.460373	2518.411766	20.779943
65.326364	2521.149719	20.784960
65.288627	2520.962875	20.789978
65.750364	2514.281697	20.794995
65.326115	2524.761157	20.800013
65.622039	2513.899863	20.805031
65.183651	2518.681016	20.810048
65.313598	2519.998656	20.815066
65.303301	2539.975518	20.820083
65.518095	2555.361624	20.825101
65.716552	2546.681966	20.830119
65.697773	2555.739267	20.835136
66.162318	2562.195646	20.840154
66.106949	2573.887514	20.845171
66.223038	2579.930138	20.850189
66.739170	2573.954497	20.855207
66.531663	2581.960843	20.860224
66.285429	2564.251482	20.865242
66.537824	2572.123902	20.870259
66.114743	2574.607138	20.875277
66.695611	2568.500261	20.880295
66.412766	2572.281514	20.885312
66.423140	2580.401654	20.890330
66.632991	2577.594003	20.895347
66.590067	2577.128085	20.900365
66.809560	2583.961439	20.905383
66.935099	2597.543432	20.910400
66.880090	2603.424336	20.915418
67.125695	2600.047323	20.920435
67.161791	2601.262059	20.925453
67.245150	2602.336256	20.930471
67.123802	2598.491859	20.935488
67.113666	2603.228239	20.940506
67.043512	2606.850127	20.945523
67.253337	2626.896033	20.950541
67.529240	2625.474319	20.955559
67.371492	2630.516752	20.960576
67.206466	2633.025221	20.965594
67.873226	2631.431846	20.970611
67.545433	2632.479493	20.975629
67.901926	2625.254707	20.980647
67.587994	2638.801505	20.985664
67.735519	2645.875207	20.990682
68.044211	2653.005988	20.995699
68.151903	2660.447360	21.000717
68.457465	2655.250822	21.005735
68.497523	2663.225119	21.010752
68.283693	2665.493265	21.015770
68.288717	2649.174410	21.020787
68.624357	2659.348126	21.025805
68.596026	2644.749087	21.030823
68.751211	2650.428529	21.035840
68.775131	2647.436795	21.040858
68.932436	2650.542517	21.045875
68.904265	2651.175780	21.050893
68.983115	2640.577260	21.055911
68.877499	2644.164499	21.060928
69.743506	2614.138072	21.065946
70.888198	2583.688594	21.070963
70.586045	2592.941447	21.075981
70.611657	2581.323811	21.080999
70.825056	2562.937240	21.086016
70.593185	2547.705552	21.091034
70.550473	2523.148305	21.096051
70.498770	2525.453268	21.101069
70.714377	2497.339578	21.106087
70.168114	2499.309394	21.111104
69.763456	2499.553629	21.116122
70.293681	2483.886665	21.121139
70.189306	2495.642528	21.126157
70.194211	2490.670825	21.131175
70.056376	2487.713487	21.136192
70.101525	2491.324059	21.141210
70.341786	2484.724588	21.146227
70.189938	2488.480899	21.151245
70.134526	2481.091164	21.156263
70.014559	2488.232876	21.161280
70.090086	2491.125770	21.166298
70.277282	2489.306195	21.171315
70.264594	2500.622001	21.176333
70.484977	2506.590568	21.181351
70.305787	2521.781088	21.186368
70.280711	2514.693790	21.191386
70.408678	2527.632377	21.196403
70.369623	2538.852982	21.201421
70.283530	2554.338311	21.206439
70.479647	2551.925486	21.211456
70.603645	2576.781494	21.216474
70.847896	2582.005535	21.221491
70.792201	2594.348293	21.226509
70.890690	2594.039195	21.231527
70.515039	2600.423807	21.236544
70.935814	2621.367371	21.241562
71.305816	2621.125751	21.246579
71.049057	2634.349246	21.251597
71.452901	2644.254517	21.256615
71.650652	2655.959498	21.261632
71.155831	2666.133835	21.266650
71.606304	2648.464890	21.271667
71.430076	2674.958835	21.276685
71.667857	2687.276513	21.281703
71.762661	2696.221311	21.286720
71.857913	2695.074119	21.291738
71.971605	2689.759056	21.296755
72.078630	2708.744139	21.301773
72.394408	2720.466563	21.306791
72.782741	2722.768108	21.311808
72.442507	2715.528757	21.316826
72.539893	2717.051444	21.321843
72.604842	2716.669961	21.326861
72.706447	2715.628804	21.331879
72.958272	2710.020288	21.336896
72.807422	2710.824346	21.341914
72.983563	2705.977667	21.346931
72.575640	2721.527675	21.351949
72.778709	2726.453080	21.356967
73.075477	2744.005799	21.361984
73.240469	2757.806980	21.367002
73.247064	2743.573326	21.372019
73.002535	2755.014862	21.377037
73.310518	2745.524322	21.382055
73.374804	2749.975132	21.387072
73.138440	2753.512074	21.392090
73.635417	2762.549920	21.397107
73.809327	2775.921262	21.402125
73.876176	2766.597960	21.407143
74.101834	2769.688802	21.412160
73.779821	2777.753652	21.417178
74.106842	2761.278793	21.422195
74.163824	2767.862450	21.427213
74.156075	2763.397520	21.432231
74.096444	2768.460700	21.437248
74.222351	2784.046069	21.442266
74.410458	2788.990517	21.447283
74.308207	2799.439479	21.452301
74.450401	2792.103374	21.457319
74.791206	2786.652494	21.462336
74.741172	2785.631023	21.467354
75.237448	2780.421646	21.472371
75.389508	2786.378446	21.477389
75.391934	2777.504455	21.482407
75.627763	2775.078302	21.487424
75.429889	2783.470970	21.492442
75.754294	2780.217051	21.497459
75.678133	2777.617147	21.502477
75.308278	2772.651731	21.507495
76.252113	2765.311152	21.512512
75.728448	2764.763702	21.517530
76.122037	2748.743569	21.522547
75.866819	2749.889010	21.527565
75.726215	2735.643211	21.532583
76.202374	2736.190688	21.537600
75.518660	2741.860370	21.542618
75.666716	2734.578439	21.547635
75.794277	2762.338263	21.552653
75.610436	2767.337435	21.557671
75.840684	2765.549653	21.562688
75.751647	2767.623046	21.567706
75.833091	2781.816504	21.572723
76.334502	2795.954743	21.577741
76.250936	2795.321940	21.582759
76.708162	2800.146462	21.587776
76.434506	2805.296016	21.592794
76.353420	2794.044796	21.597811
76.629127	2797.410021	21.602829
76.695703	2818.815108	21.607847
77.112188	2828.892817	21.612864
76.756283	2842.034141	21.617882
77.185346	2828.586550	21.622899
77.320518	2837.956246	21.627917
77.391737	2836.212998	21.632935
77.342700	2832.722690	21.637952
77.244203	2846.255123	21.642970
77.412423	2833.951742	21.647987
77.177619	2830.648225	21.653005
77.069475	2835.185596	21.658023
77.231720	2845.815054	21.663040
77.651952	2854.046363	21.668058
77.648089	2840.502594	21.673075
78.364352	2843.898946	21.678093
78.340803	2843.748325	21.683111
78.496377	2838.959357	21.688128
78.237690	2844.718682	21.693146
78.294715	2838.794835	21.698163
78.523383	2839.406286	21.703181
78.214870	2831.952144	21.708199
78.474464	2831.654852	21.713216
78.470007	2834.326836	21.718234
78.421364	2826.249940	21.723251
78.762129	2838.262414	21.728269
78.383166	2845.810351	21.733287
78.678403	2853.731704	21.738304
78.535162	2869.803261	21.743322
78.708815	2865.543601	21.748339
78.981032	2866.065525	21.753357
78.757191	2878.376607	21.758375
78.928749	2876.652901	21.763392
79.361485	2906.469887	21.768410
79.561025	2897.609921	21.773427
79.824133	2893.108599	21.778445
79.247032	2900.596179	21.783463
79.733008	2894.101771	21.788480
79.550687	2896.630874	21.793498
79.580502	2896.356808	21.798515
79.587830	2896.329410	21.803533
79.435995	2905.637785	21.808551
80.086969	2908.731201	21.813568
80.043115	2917.966120	21.818586
80.217490	2918.357447	21.823603
80.321208	2913.963718	21.828621
80.355634	2927.922586	21.833639
80.521701	2923.194059	21.838656
80.920479	2920.545512	21.843674
80.442551	2930.930613	21.848691
80.923029	2916.657807	21.853709
80.278190	2919.078338	21.858727
80.635816	2920.547163	21.863744
80.854854	2937.988997	21.868762
80.772806	2946.221152	21.873779
80.813623	2944.433728	21.878797
80.853090	2946.129069	21.883815
81.134957	2941.607684	21.888832
81.437516	2948.175014	21.893850
81.327093	2942.919556	21.898867
81.697228	2950.008372	21.903885
81.492758	2965.671669	21.908903
82.078754	2964.318476	21.913920
81.977816	2980.748104	21.918938
82.030658	2976.059246	21.923955
81.985352	2966.273721	21.928973
82.094587	2969.158739	21.933991
82.234035	2968.385313	21.939008
82.182924	2970.905219	21.944026
82.057968	2963.097648	21.949043
82.109719	2960.859159	21.954061
81.893653	2976.541718	21.959079
82.024164	2966.813592	21.964096
82.552415	2976.850380	21.969114
82.529599	2990.426268	21.974131
82.508256	3000.175645	21.979149
82.449307	2991.915716	21.984167
82.552035	2994.607711	21.989184
82.617617	3000.611253	21.994202
82.557333	3010.967155	21.999219
82.956522	3024.776503	22.004237
82.685597	3035.823780	22.009255
83.065153	3029.919491	22.014272
82.852894	3031.216485	22.019290
82.791651	3035.206706	22.024307
83.453830	3043.678242	22.029325
83.145144	3053.064352	22.034343
83.085292	3060.372332	22.039360
83.439641	3055.167948	22.044378
83.461039	3073.710190	22.049395
83.855321	3083.469682	22.054413
83.744354	3083.184756	22.059431
83.726200	3081.400425	22.064448
84.240427	3084.772925	22.069466
84.050857	3085.673601	22.074483
84.531558	3063.578328	22.079501
84.628900	3078.421435	22.084519
84.604794	3076.721565	22.089536
84.933556	3084.761097	22.094554
85.169097	3091.566810	22.099571
84.806796	3068.741880	22.104589
84.423064	3080.782820	22.109607
84.641352	3078.308351	22.114624
85.255625	3089.651496	22.119642
85.035542	3095.936036	22.124659
85.337762	3097.126268	22.129677
85.286904	3099.420544	22.134695
85.184561	3101.702509	22.139712
85.560610	3101.121269	22.144730
85.294168	3100.424351	22.149747
85.615078	3105.046016	22.154765
85.719158	3114.467112	22.159783
85.776202	3126.388763	22.164800
86.095913	3121.820483	22.169818
85.917494	3128.159534	22.174835
86.178940	3121.405475	22.179853
86.087734	3125.480233	22.184871
86.043539	3121.667375	22.189888
86.382860	3112.915563	22.194906
85.823151	3123.375411	22.199923
86.203333	3128.501055	22.204941
85.935434	3137.507963	22.209959
85.994833	3142.032539	22.214976
86.860216	3146.427887	22.219994
86.558074	3155.622008	22.225011
87.254532	3171.851194	22.230029
86.821016	3184.005220	22.235047
87.049711	3181.721937	22.240064
87.384688	3169.344117	22.245082
87.033861	3177.470657	22.250099
87.314952	3171.109804	22.255117
87.210125	3168.058259	22.260135
87.326437	3166.129118	22.265152
87.443408	3162.561535	22.270170
87.579254	3184.484792	22.275187
88.091341	3187.288723	22.280205
87.977640	3193.533572	22.285223
88.170458	3197.746200	22.290240
88.207841	3194.941905	22.295258
87.948003	3199.390015	22.300275
88.173902	3190.973968	22.305293
87.976856	3197.930370	22.310311
88.304575	3198.626565	22.315328
88.105460	3186.698947	22.320346
87.926941	3207.227503	22.325363
88.478967	3221.956199	22.330381
88.598956	3232.804381	22.335399
88.729342	3233.325480	22.340416
89.272666	3231.565936	22.345434
88.662988	3224.382151	22.350451
88.854375	3225.816424	22.355469
88.867968	3224.116572	22.360487
89.161228	3231.711252	22.365504
89.032715	3242.527900	22.370522
89.034421	3240.170118	22.375539
89.447438	3238.316865	22.380557
89.717864	3235.674637	22.385575
89.661456	3234.410472	22.390592
89.882344	3230.239723	22.395610
89.772651	3245.248512	22.400627
90.050720	3244.589842	22.405645
90.100230	3262.663027	22.410663
89.895640	3263.814657	22.415680
90.006683	3267.158135	22.420698
90.328782	3266.801625	22.425715
90.471595	3257.589826	22.430733
90.565022	3269.595312	22.435751
90.404912	3269.247283	22.440768
90.570769	3261.979080	22.445786
90.792897	3272.684318	22.450803
90.967746	3276.682611	22.455821
91.221529	3288.411831	22.460839
91.158741	3287.717674	22.465856
91.223210	3291.264586	22.470874
91.342724	3287.040190	22.475891
91.616900	3294.677053	22.480909
91.752825	3275.319750	22.485927
91.626970	3285.298112	22.490944
92.026378	3281.575677	22.495962
91.988236	3279.120959	22.500979
91.829984	3277.871355	22.505997
92.010193	3275.984736	22.511015
92.095610	3284.649516	22.516032
92.067646	3279.539311	22.521050
91.786923	3276.371294	22.526067
92.073779	3272.774665	22.531085
92.392832	3277.197853	22.536103
92.085884	3278.661012	22.541120
92.153908	3292.778418	22.546138
92.077826	3305.525164	22.551155
91.946317	3307.315108	22.556173
92.459695	3314.564554	22.561191
92.636510	3330.266038	22.566208
92.865636	3333.085918	22.571226
93.201689	3335.049757	22.576243
93.057726	3334.646282	22.581261
93.180969	3334.507090	22.586279
92.909141	3337.644504	22.591296
93.521946	3349.342844	22.596314
93.483744	3361.337990	22.601331
93.654107	3367.191962	22.606349
94.067315	3362.512002	22.611367
93.738604	3363.756715	22.616384
93.968985	3353.347905	22.621402
94.105714	3364.688328	22.626419
93.769731	3364.665620	22.631437
94.251697	3353.937409	22.636455
94.111401	3362.815354	22.641472
94.319273	3366.726677	22.646490
94.117413	3387.828305	22.651507
94.128830	3389.424802	22.656525
94.397815	3392.488094	22.661543
94.430763	3392.576135	22.666560
94.917113	3388.293108	22.671578
95.119155	3412.527180	22.676595
95.021190	3409.602413	22.681613
95.325686	3412.157393	22.686631
95.300536	3415.546375	22.691648
95.671780	3412.384555	22.696666
95.953454	3413.139205	22.701683
95.689245	3397.226555	22.706701
95.341917	3374.497123	22.711719
95.507284	3394.306107	22.716736
95.627222	3401.889515	22.721754
95.345226	3403.672981	22.726771
95.670924	3412.876304	22.731789
96.066321	3398.492781	22.736807
95.956794	3410.532499	22.741824
96.050998	3420.885440	22.746842
95.988272	3430.786860	22.751859
96.127749	3438.763930	22.756877
96.252827	3426.751930	22.761895
96.406893	3436.877193	22.766912
96.702107	3437.064574	22.771930
97.244352	3441.125878	22.776947
97.370274	3443.473904	22.781965
97.431726	3431.968983	22.786983
97.409675	3435.288943	22.792000
97.499372	3410.509059	22.797018
97.281375	3416.162606	22.802035
97.502232	3428.807735	22.807053
97.297144	3429.902367	22.812071
97.476239	3438.806415	22.817088
97.679141	3441.638156	22.822106
97.889017	3437.094733	22.827123
97.750810	3449.824754	22.832141
97.912096	3445.980816	22.837159
97.624824	3447.295428	22.842176
98.088261	3463.701459	22.847194
97.984382	3478.031874	22.852211
98.001746	3474.129556	22.857229
98.193630	3481.368333	22.862247
98.144725	3488.518377	22.867264
98.533527	3498.336135	22.872282
98.422992	3503.921454	22.877299
98.400096	3509.959191	22.882317
98.847204	3502.440961	22.887335
98.611175	3514.511234	22.892352
99.135790	3518.966083	22.897370
99.017891	3529.009427	22.902387
99.138079	3528.079314	22.907405
99.370034	3524.711462	22.912423
99.336295	3543.345718	22.917440
99.310677	3556.220123	22.922458
99.714699	3570.106722	22.927475
99.449529	3563.618756	22.932493
99.740625	3561.436478	22.937511
99.636817	3574.063627	22.942528
99.952407	3588.702424	22.947546
100.050061	3583.779533	22.952563
100.032415	3594.306708	22.957581
100.621224	3579.375067	22.962599
100.651839	3595.924832	22.967616
100.355534	3590.972521	22.972634
100.580639	3610.751376	22.977651
100.190768	3619.115761	22.982669
101.191538	3600.075795	22.987687
101.459337	3615.962468	22.992704
101.428709	3611.056164	22.997722
101.235315	3606.073356	23.002739
101.664167	3607.717442	23.007757
101.569953	3605.326722	23.012775
101.552151	3617.686827	23.017792
101.605977	3603.057487	23.022810
101.933941	3599.752412	23.027827
101.881123	3607.722153	23.032845
101.945366	3609.064983	23.037863
101.791917	3623.660885	23.042880
101.990865	3621.958928	23.047898
102.219208	3634.920734	23.052915
102.001358	3620.237699	23.057933
101.846032	3615.019795	23.062951
101.763520	3638.938870	23.067968
101.891131	3649.903018	23.072986
102.674736	3652.905642	23.078003
102.596345	3659.093226	23.083021
103.185013	3672.150709	23.088039
103.181925	3679.291257	23.093056
103.072919	3684.310963	23.098074
103.121672	3679.604069	23.103091
102.804415	3683.892152	23.108109
103.283169	3685.408647	23.113127
103.460375	3692.717293	23.118144
103.421203	3710.648234	23.123162
103.482345	3708.712053	23.128179
103.401881	3718.676452	23.133197
103.837566	3709.497221	23.138215
104.030729	3726.617426	23.143232
103.963995	3739.235397	23.148250
104.155002	3743.985943	23.153267
104.277045	3750.622596	23.158285
104.471799	3745.226767	23.163303
104.390690	3747.552547	23.168320
104.447925	3756.641223	23.173338
104.571032	3765.975288	23.178355
104.681685	3779.977375	23.183373
105.120227	3761.368099	23.188391
105.477542	3752.536161	23.193408
105.560112	3759.941285	23.198426
105.454076	3759.183813	23.203443
105.682081	3761.015646	23.208461
105.522201	3749.127538	23.213479
105.818690	3754.587420	23.218496
105.794698	3753.506826	23.223514
106.028152	3774.689402	23.228531
105.760740	3788.178271	23.233549
106.359194	3775.415986	23.238567
106.277215	3781.611696	23.243584
106.128408	3774.168752	23.248602
106.549849	3776.848865	23.253619
106.756955	3784.017528	23.258637
106.635197	3782.186153	23.263655
106.586928	3779.911408	23.268672
106.596127	3789.178580	23.273690
107.102899	3794.057790	23.278707
106.980854	3817.394655	23.283725
107.173146	3813.819920	23.288743
107.058658	3813.420196	23.293760
107.123088	3812.726529	23.298778
107.322461	3802.730501	23.303795
107.236257	3844.048808	23.308813
107.551560	3838.719932	23.313831
108.028942	3844.092294	23.318848
107.633977	3844.191604	23.323866
107.928393	3836.520223	23.328883
107.860356	3847.919835	23.333901
107.931022	3862.512576	23.338919
108.133323	3863.241854	23.343936
107.915609	3873.712296	23.348954
108.472870	3865.609766	23.353971
108.450567	3870.266651	23.358989
108.285228	3892.179137	23.364007
108.707396	3886.584026	23.369024
108.536002	3903.946140	23.374042
109.247820	3889.062671	23.379059
109.034151	3891.648723	23.384077
108.722176	3890.310427	23.389095
109.287005	3903.776452	23.394112
109.511181	3912.693754	23.399130
109.535461	3908.686228	23.404147
109.567549	3915.189062	23.409165
109.811630	3920.436817	23.414183
109.978601	3911.028862	23.419200
109.802567	3917.068186	23.424218
110.116223	3927.007381	23.429235
109.915489	3942.386347	23.434253
110.443111	3944.094382	23.439271
110.561917	3939.047769	23.444288
110.537947	3941.442832	23.449306
110.336840	3935.524064	23.454323
110.704192	3952.671875	23.459341
110.969761	3965.898279	23.464359
111.128552	3975.588007	23.469376
110.860514	3975.332317	23.474394
111.148585	3968.986915	23.479411
111.465022	3977.747563	23.484429
111.437146	3972.337468	23.489447
111.699373	3967.331587	23.494464
111.696840	3970.757487	23.499482
112.171032	3980.980316	23.504499
112.513641	3978.813439	23.509517
112.231551	3978.462433	23.514535
112.619412	3977.787852	23.519552
112.576239	3990.129236	23.524570
112.883805	3980.579747	23.529587
112.530940	3963.311377	23.534605
112.503479	3980.730374	23.539623
112.986673	3969.816478	23.544640
112.856092	3975.762826	23.549658
112.888437	3976.609738	23.554675
112.785705	3972.753243	23.559693
112.966893	3968.299094	23.564711
112.753202	3974.581346	23.569728
112.891555	4004.230036	23.574746
113.072938	4009.214186	23.579763
112.880699	4005.971462	23.584781
113.179535	4023.374080	23.589799
113.395831	4023.174530	23.594816
113.256891	4044.974559	23.599834
113.755463	4052.893840	23.604851
114.027578	4060.038832	23.609869
113.866987	4058.152452	23.614887
114.026127	4076.893103	23.619904
114.410111	4083.695057	23.624922
114.815803	4082.979708	23.629939
114.412679	4085.203125	23.634957
114.425153	4097.010858	23.639975
115.007573	4100.608509	23.644992
115.113128	4118.037841	23.650010
115.355516	4119.639734	23.655027
115.422661	4113.560158	23.660045
115.129629	4115.099042	23.665063
116.267381	4086.045275	23.670080
116.380391	4090.424976	23.675098
116.741745	4077.582937	23.680115
116.546529	4082.515508	23.685133
116.404671	4081.605289	23.690151
116.852835	4070.323862	23.695168
117.167558	4056.963923	23.700186
116.852148	4039.742399	23.705203
117.197598	4033.286240	23.710221
116.927199	4029.890729	23.715239
117.050958	4028.038209	23.720256
117.065133	4027.213495	23.725274
117.249565	4032.054606	23.730291
117.371166	4026.130211	23.735309
117.074664	4036.432727	23.740327
117.287066	4019.798801	23.745344
117.372854	4020.263552	23.750362
117.314971	4022.177186	23.755379
117.197673	4022.831616	23.760397
117.119486	4053.114898	23.765415
117.626828	4049.837408	23.770432
117.693717	4065.691385	23.775450
117.647748	4075.086416	23.780467
117.620465	4082.340240	23.785485
118.003286	4088.362749	23.790503
118.298793	4089.120256	23.795520
118.135839	4096.234404	23.800538
118.295287	4122.333230	23.805555
118.445556	4132.179219	23.810573
118.495512	4125.655184	23.815591
118.918299	4138.150777	23.820608
119.103156	4147.457089	23.825626
118.968103	4155.063553	23.830643
119.653836	4149.606465	23.835661
119.358578	4155.466059	23.840679
119.358520	4162.003476	23.845696
119.515333	4177.735913	23.850714
119.934126	4180.327548	23.855731
120.189993	4183.540840	23.860749
119.900689	4182.450363	23.865767
120.145545	4182.398058	23.870784
120.151477	4193.265863	23.875802
120.042730	4212.240595	23.880819
120.838207	4207.438583	23.885837
120.700790	4206.018090	23.890855
121.222912	4204.141479	23.895872
120.961805	4213.787341	23.900890
121.155950	4211.576987	23.905907
121.324189	4206.647684	23.910925
121.128515	4206.999349	23.915943
121.532320	4212.518342	23.920960
120.996428	4234.594479	23.925978
121.527658	4237.750207	23.930995
121.629615	4227.921698	23.936013
121.418470	4241.500832	23.941031
121.801033	4254.629285	23.946048
122.200632	4257.107570	23.951066
122.150096	4271.186105	23.956083
122.246747	4267.004230	23.961101
122.197180	4287.115855	23.966119
122.354459	4288.739786	23.971136
122.433889	4295.649938	23.976154
122.962035	4304.602395	23.981171
122.896333	4305.592411	23.986189
122.847768	4327.536499	23.991207
123.051041	4321.394056	23.996224
123.411932	4326.350050	24.001242
123.210443	4331.041183	24.006259
123.432987	4337.512540	24.011277
122.850244	4359.387942	24.016295
123.513693	4358.355685	24.021312
123.831255	4361.298876	24.026330
123.614622	4379.517597	24.031347
124.376274	4383.539148	24.036365
124.495779	4390.055216	24.041383
124.824669	4381.901779	24.046400
124.836777	4375.751708	24.051418
124.962027	4378.191341	24.056435
125.013709	4370.013102	24.061453
124.892527	4371.117871	24.066471
125.105389	4371.675707	24.071488
125.077717	4370.581112	24.076506
125.307139	4393.126444	24.081523
125.717596	4394.168064	24.086541
125.501064	4407.442673	24.091559
125.839078	4406.534588	24.096576
125.779126	4402.322000	24.101594
125.690491	4397.362874	24.106611
126.173070	4396.852882	24.111629
125.913116	4400.592174	24.116647
126.293347	4407.534288	24.121664
126.686451	4418.593066	24.126682
126.380293	4414.935651	24.131699
126.649994	4418.747581	24.136717
126.650720	4422.660915	24.141735
126.402521	4438.430996	24.146752
126.537401	4446.231363	24.151770
126.761015	4451.885917	24.156787
127.356160	4462.122039	24.161805
127.245865	4478.489819	24.166823
127.433675	4479.505443	24.171840
127.456178	4481.703856	24.176858
127.721668	4488.865897	24.181875
128.057773	4492.611682	24.186893
128.149370	4508.220620	24.191911
128.052757	4506.409788	24.196928
128.117829	4510.501459	24.201946
128.266835	4520.998409	24.206963
128.794979	4523.916874	24.211981
128.586904	4523.734292	24.216999
128.774262	4533.735028	24.222016
128.988035	4522.547361	24.227034
128.789438	4531.942042	24.232051
128.993847	4545.952465	24.237069
128.935170	4564.703516	24.242087
129.348851	4560.554718	24.247104
129.604444	4568.831236	24.252122
129.723189	4587.676473	24.257139
129.620431	4587.992228	24.262157
129.818661	4592.694976	24.267175
129.802101	4594.870757	24.272192
130.391524	4604.377872	24.277210
130.329034	4622.201899	24.282227
130.511401	4616.149446	24.287245
130.859768	4616.645395	24.292263
130.747106	4609.623680	24.297280
130.936424	4620.489656	24.302298
130.906762	4640.603151	24.307315
131.468346	4642.821467	24.312333
131.293002	4654.325339	24.317351
131.336620	4655.972923	24.322368
131.386851	4649.515566	24.327386
131.519566	4667.304842	24.332403
131.734179	4667.136280	24.337421
131.609153	4685.230662	24.342439
131.838703	4682.541831	24.347456
132.055436	4696.876385	24.352474
132.203770	4695.948617	24.357491
132.535063	4698.700579	24.362509
132.985385	4696.183757	24.367527
132.745958	4702.958854	24.372544
133.135217	4703.428321	24.377562
132.923909	4727.286978	24.382579
133.156246	4720.537075	24.387597
133.179570	4728.674292	24.392615
132.981742	4725.086218	24.397632
133.464302	4725.116479	24.402650
133.307184	4724.962441	24.407667
133.784708	4735.816041	24.412685
133.820303	4745.949240	24.417703
133.580545	4748.436203	24.422720
134.034973	4751.671744	24.427738
134.586477	4777.318242	24.432755
134.759976	4769.386531	24.437773
134.789352	4780.804495	24.442791
134.809440	4781.076999	24.447808
134.993234	4769.997309	24.452826
135.061212	4777.189156	24.457843
135.224082	4767.807755	24.462861
134.920499	4782.568292	24.467879
135.211175	4800.106227	24.472896
135.488254	4792.599895	24.477914
135.317974	4807.917153	24.482931
135.350148	4813.657995	24.487949
135.594189	4823.972393	24.492967
135.616389	4832.536704	24.497984
135.929210	4839.984799	24.503002
136.082639	4859.272716	24.508019
136.384830	4857.451484	24.513037
136.686095	4857.353577	24.518055
136.702663	4861.684154	24.523072
136.732269	4874.029888	24.528090
136.919637	4884.828642	24.533107
137.278714	4884.121009	24.538125
137.288209	4890.708333	24.543143
137.070917	4891.387290	24.548160
137.935701	4904.907900	24.553178
137.731827	4921.804392	24.558195
137.654884	4906.300904	24.563213
137.949615	4910.839649	24.568231
137.552331	4919.135070	24.573248
138.153927	4934.178478	24.578266
138.328370	4945.092042	24.583283
138.350633	4938.879421	24.588301
138.264205	4958.494779	24.593319
138.452331	4971.339549	24.598336
138.787030	4971.343981	24.603354
138.844128	4986.565346	24.608371
139.047003	4992.545656	24.613389
139.217584	4995.585851	24.618407
139.338018	5010.285585	24.623424
139.803866	5010.127249	24.628442
140.056283	5025.157105	24.633459
140.251543	5015.385055	24.638477
140.646157	5014.631346	24.643495
141.005660	5011.694046	24.648512
140.637314	5013.319560	24.653530
140.580690	5014.430971	24.658547
141.113884	5018.376462	24.663565
141.138725	5013.364418	24.668583
140.925649	5017.543399	24.673600
141.007229	5006.685295	24.678618
141.104147	5036.429060	24.683635
141.329865	5043.554650	24.688653
140.970135	5045.372476	24.693671
141.213323	5048.692015	24.698688
141.970656	5057.622571	24.703706
141.798790	5070.864325	24.708723
141.929278	5064.587990	24.713741
142.713541	5060.493252	24.718759
142.799942	5063.558476	24.723776
143.042035	5053.857376	24.728794
142.969200	5055.587360	24.733811
142.834007	5067.049419	24.738829
143.041076	5049.605283	24.743847
142.964807	5065.796329	24.748864
142.925397	5081.842655	24.753882
142.948494	5096.233381	24.758899
143.152891	5089.540732	24.763917
143.294774	5096.804713	24.768935
143.365118	5120.688040	24.773952
143.674183	5119.964294	24.778970
143.572979	5127.649083	24.783987
143.791747	5134.934958	24.789005
143.879709	5146.967994	24.794023
143.843490	5157.381955	24.799040
144.227857	5163.866929	24.804058
144.197317	5189.137498	24.809075
144.345224	5189.671507	24.814093
144.888252	5206.026767	24.819111
144.807669	5222.369117	24.824128
145.101588	5212.674272	24.829146
145.633072	5238.065739	24.834163
145.451436	5239.130997	24.839181
146.117411	5234.884182	24.844199
146.394821	5234.405115	24.849216
146.481782	5229.442534	24.854234
146.441049	5237.278780	24.859251
146.475848	5226.756717	24.864269
146.718252	5226.487450	24.869287
146.616687	5242.377302	24.874304
146.830565	5246.066401	24.879322
147.090679	5251.684464	24.884339
147.240739	5255.184126	24.889357
147.445589	5255.315675	24.894375
147.229057	5256.897869	24.899392
147.868202	5276.393046	24.904410
147.861470	5273.891446	24.909427
147.652307	5282.822083	24.914445
147.789180	5274.859977	24.919463
147.686877	5285.482686	24.924480
148.224780	5297.171713	24.929498
148.471581	5298.543813	24.934515
148.639366	5314.772527	24.939533
148.637796	5304.290323	24.944551
148.798536	5323.532703	24.949568
148.819756	5335.500580	24.954586
149.104156	5342.952063	24.959603
148.954864	5347.038622	24.964621
149.372478	5356.796848	24.969639
149.339093	5368.182351	24.974656
149.558202	5369.537007	24.979674
149.705384	5375.963038	24.984691
149.714752	5394.078428	24.989709
149.840395	5397.705830	24.994727
149.944860	5411.715521	24.999744
149.896723	5427.255657	25.004762
150.705139	5433.708080	25.009779
150.392064	5438.228273	25.014797
150.607420	5454.209800	25.019815
150.873990	5468.888828	25.024832
151.042994	5467.314124	25.029850
151.542555	5491.941049	25.034867
151.524398	5493.821086	25.039885
151.978506	5497.137173	25.044903
151.843245	5495.283030	25.049920
151.675991	5490.029464	25.054938
151.809263	5509.394774	25.059955
151.996533	5520.049852	25.064973
152.485166	5519.898755	25.069991
152.478115	5537.831954	25.075008
152.955199	5547.200011	25.080026
153.149991	5545.821849	25.085043
152.965782	5546.303162	25.090061
153.200081	5549.549464	25.095079
153.306226	5550.321190	25.100096
153.509263	5543.793182	25.105114
153.797513	5551.330759	25.110131
153.969897	5577.040781	25.115149
153.965332	5580.512656	25.120167
154.200300	5568.860774	25.125184
153.675298	5578.750581	25.130202
154.235551	5582.143558	25.135219
153.978488	5605.059733	25.140237
154.664504	5600.186506	25.145255
154.933068	5597.490252	25.150272
155.276430	5606.125265	25.155290
155.918247	5606.456709	25.160307
155.527982	5602.296328	25.165325
156.209954	5595.420927	25.170343
156.268206	5607.308035	25.175360
156.488750	5601.871848	25.180378
156.535991	5597.082722	25.185395
156.198306	5606.471225	25.190413
156.531233	5601.551926	25.195431
156.615077	5605.150093	25.200448
156.325103	5595.403191	25.205466
156.659354	5619.283584	25.210483
156.806153	5640.348009	25.215501
157.017178	5634.012385	25.220519
157.192737	5637.838685	25.225536
157.292580	5646.566958	25.230554
157.296791	5654.937807	25.235571
157.440436	5667.692088	25.240589
157.800912	5669.878608	25.245607
157.735237	5683.737243	25.250624
157.964086	5688.706954	25.255642
158.023346	5691.724830	25.260659
158.347562	5705.276112	25.265677
158.165082	5714.462464	25.270695
158.660631	5722.376802	25.275712
158.718390	5741.875449	25.280730
159.103577	5751.638523	25.285747
159.070297	5745.144190	25.290765
159.167902	5756.149059	25.295783
159.814146	5764.799198	25.300800
160.036265	5755.866537	25.305818
160.523612	5750.037843	25.310835
160.657216	5764.601414	25.315853
160.690962	5759.349798	25.320871
160.696530	5756.885458	25.325888
160.731187	5755.522075	25.330906
160.546332	5771.974471	25.335923
160.670475	5780.122255	25.340941
160.898161	5786.541378	25.345959
160.997607	5791.883897	25.350976
161.395042	5812.786399	25.355994
161.460985	5820.366562	25.361011
160.998488	5833.048433	25.366029
161.385141	5843.313025	25.371047
161.951312	5853.899063	25.376064
161.865285	5863.474303	25.381082
162.390214	5862.805230	25.386099
162.683098	5878.987746	25.391117
162.535911	5877.790827	25.396135
162.799889	5880.625862	25.401152
162.835253	5895.109791	25.406170
163.085040	5900.770760	25.411187
163.161715	5911.884755	25.416205
163.165834	5904.112942	25.421223
163.530232	5906.282305	25.426240
163.649824	5928.032916	25.431258
163.627628	5932.518300	25.436275
163.785507	5938.081140	25.441293
164.327174	5943.347860	25.446311
164.378068	5957.289752	25.451328
164.375183	5980.882532	25.456346
164.814820	5969.301885	25.461363
164.729776	5976.907214	25.466381
164.680544	5996.656301	25.471399
165.092008	5997.114249	25.476416
164.870280	6002.864637	25.481434
165.317173	6024.988665	25.486451
165.461327	6043.367517	25.491469
165.556394	6032.522220	25.496487
165.744857	6051.448987	25.501504
165.768459	6066.038992	25.506522
166.017227	6064.788074	25.511539
166.302999	6089.362462	25.516557
166.359905	6091.323035	25.521575
166.801703	6094.515279	25.526592
167.105279	6110.630884	25.531610
167.407837	6104.666583	25.536627
167.676681	6108.918562	25.541645
167.666309	6113.845462	25.546663
167.933096	6119.460366	25.551680
167.798479	6134.329552	25.556698
167.954576	6138.448265	25.561715
168.481239	6138.851633	25.566733
168.154195	6151.877490	25.571751
168.835256	6159.388678	25.576768
168.512649	6161.378459	25.581786
168.637977	6162.473103	25.586803
168.434849	6179.781164	25.591821
168.762083	6203.955816	25.596839
168.892735	6199.377908	25.601856
168.785758	6221.854169	25.606874
169.054939	6232.623713	25.611891
169.336567	6254.384864	25.616909
169.815395	6268.208661	25.621927
170.297908	6282.038945	25.626944
170.392773	6288.265323	25.631962
170.298411	6295.777051	25.636979
170.542610	6317.263326	25.641997
170.908167	6321.371696	25.647015
171.105277	6319.544136	25.652032
171.199030	6337.034596	25.657050
171.811289	6348.081950	25.662067
171.911555	6338.941586	25.667085
171.712434	6353.845325	25.672103
171.957437	6360.867493	25.677120
172.058210	6373.149014	25.682138
172.060508	6380.589585	25.687156
172.457675	6385.817458	25.692173
172.492181	6415.813633	25.697191
172.693797	6407.321150	25.702208
172.949906	6426.571868	25.707226
172.915761	6428.568093	25.712244
173.360276	6442.355212	25.717261
173.277056	6446.392479	25.722279
173.766623	6452.902254	25.727296
173.826878	6468.468720	25.732314
174.325455	6459.733103	25.737332
174.883874	6444.777834	25.742349
174.940430	6452.700119	25.747367
175.227519	6442.098305	25.752384
175.180152	6445.768090	25.757402
175.532183	6451.868308	25.762420
175.699235	6448.178246	25.767437
175.478582	6453.395388	25.772455
175.636246	6447.807110	25.777472
175.821218	6441.551895	25.782490
175.751508	6441.239173	25.787508
176.019530	6457.932077	25.792525
176.028383	6469.489359	25.797543
176.525770	6470.706505	25.802560
176.100066	6477.067508	25.807578
176.401563	6498.755596	25.812596
176.260472	6504.269075	25.817613
176.177799	6520.245286	25.822631
176.180198	6525.137110	25.827648
176.878182	6556.864798	25.832666
176.947449	6558.141280	25.837684
177.708701	6572.075152	25.842701
177.584857	6597.112218	25.847719
177.958202	6591.838549	25.852736
177.772462	6603.060436	25.857754
178.104513	6611.663227	25.862772
178.594788	6610.257140	25.867789
178.942010	6617.429416	25.872807
179.342393	6632.495293	25.877824
179.413230	6646.878710	25.882842
179.527064	6639.697941	25.887860
180.113518	6635.133170	25.892877
179.928530	6645.689402	25.897895
180.223396	6636.088051	25.902912
180.033867	6648.097456	25.907930
180.166399	6653.454459	25.912948
180.286480	6660.436083	25.917965
180.420417	6663.985999	25.922983
180.823908	6678.020374	25.928000
180.973234	6693.692770	25.933018
180.975055	6696.269061	25.938036
180.990152	6704.751290	25.943053
181.223818	6723.223966	25.948071
181.704262	6727.945835	25.953088
181.589250	6737.043589	25.958106
181.841517	6744.097014	25.963124
182.460955	6746.081551	25.968141
181.996174	6753.036744	25.973159
182.651929	6765.610720	25.978176
182.847125	6781.231472	25.983194
182.788643	6772.843453	25.988212
183.150121	6779.980354	25.993229
183.250185	6810.428733	25.998247
183.627381	6806.843083	26.003264
183.782363	6814.908299	26.008282
183.701343	6835.719955	26.013300
183.794978	6837.435072	26.018317
183.518450	6849.229090	26.023335
184.534988	6862.276433	26.028352
184.633367	6867.820346	26.033370
184.516488	6870.165128	26.038388
185.029246	6887.084831	26.043405
185.318700	6900.225461	26.048423
185.444210	6898.667297	26.053440
185.434628	6912.453884	26.058458
185.544399	6932.028846	26.063476
186.360153	6925.708006	26.068493
186.073913	6923.154923	26.073511
186.171610	6937.716089	26.078528
186.182995	6945.756399	26.083546
186.441562	6958.920326	26.088564
186.952394	6963.602560	26.093581
186.739238	6980.746175	26.098599
186.834888	6983.723593	26.103616
187.185554	6982.190233	26.108634
187.269720	7001.608064	26.113652
187.757515	7018.688015	26.118669
187.968216	7017.691465	26.123687
187.934870	7016.714203	26.128704
188.158777	7040.410289	26.133722
188.588627	7044.071014	26.138740
188.697175	7042.035180	26.143757
188.784930	7044.043520	26.148775
189.143540	7064.326364	26.153792
189.431441	7068.973209	26.158810
188.945174	7072.055219	26.163828
189.482825	7077.144193	26.168845
189.786879	7092.120968	26.173863
189.960154	7082.697088	26.178880
189.965830	7098.589884	26.183898
190.245967	7115.960438	26.188916
190.492460	7125.875805	26.193933
190.244600	7136.524727	26.198951
190.201636	7151.237853	26.203968
190.811149	7158.090320	26.208986
190.506644	7180.644870	26.214004
191.220823	7194.472118	26.219021
191.249775	7210.540748	26.224039
191.151929	7216.130780	26.229056
191.722413	7235.502743	26.234074
191.971665	7247.946949	26.239092
192.764490	7249.431712	26.244109
192.781673	7271.997526	26.249127
193.056792	7278.459787	26.254144
193.602694	7265.798757	26.259162
193.400805	7279.748373	26.264180
194.161555	7279.391370	26.269197
194.054213	7297.929258	26.274215
194.305617	7293.546007	26.279232
194.732535	7289.380922	26.284250
194.548341	7296.795412	26.289268
194.594849	7285.785615	26.294285
194.542281	7294.294369	26.299303
194.952519	7302.469440	26.304320
195.466405	7308.311520	26.309338
195.269139	7320.521998	26.314356
195.392770	7317.991325	26.319373
195.629715	7333.285099	26.324391
195.803217	7347.473289	26.329408
196.320329	7345.715317	26.334426
196.106709	7355.563139	26.339444
195.900012	7369.769628	26.344461
195.943339	7385.135010	26.349479
196.227948	7405.803948	26.354496
196.652556	7408.019446	26.359514
196.738409	7428.721442	26.364532
196.903322	7435.330473	26.369549
197.210192	7457.876769	26.374567
197.667276	7475.072593	26.379584
197.826241	7474.408352	26.384602
197.779743	7501.978214	26.389620
198.046157	7505.197532	26.394637
198.180960	7521.025970	26.399655
198.260289	7529.262447	26.404672
198.667186	7536.926198	26.409690
198.762764	7570.037591	26.414708
199.008086	7571.209282	26.419725
199.460443	7577.531938	26.424743
199.493792	7593.649061	26.429760
199.357025	7593.858670	26.434778
200.084874	7629.342414	26.439796
200.388623	7624.056343	26.444813
200.342446	7622.239131	26.449831
200.507215	7636.894557	26.454848
201.177735	7643.333800	26.459866
201.197040	7641.771158	26.464884
201.509945	7655.187361	26.469901
201.664340	7642.294130	26.474919
201.424072	7661.852538	26.479936
201.919980	7658.240673	26.484954
202.176877	7667.426820	26.489972
202.122568	7672.821518	26.494989
202.248118	7699.962196	26.500007
202.498516	7708.617752	26.505024
202.862047	7711.910773	26.510042
202.819995	7734.658803	26.515060
202.925636	7748.057537	26.520077
203.339193	7759.696595	26.525095
203.466142	7776.575810	26.530112
203.715112	7775.902115	26.535130
204.039346	7802.177354	26.540148
204.357705	7808.454627	26.545165
204.195332	7814.885041	26.550183
204.392548	7829.720363	26.555200
204.550228	7829.735322	26.560218
204.967891	7865.976132	26.565236
205.243036	7866.840412	26.570253
205.418359	7879.882663	26.575271
205.554917	7898.012074	26.580288
206.209215	7898.404532	26.585306
205.878512	7906.485629	26.590324
206.203898	7924.794799	26.595341
206.031120	7934.692906	26.600359
206.267630	7964.559973	26.605376
206.757849	7976.774085	26.610394
207.035625	7992.977817	26.615412
207.771743	7985.327543	26.620429
208.588634	7981.438561	26.625447
208.143033	7980.781021	26.630464
208.459636	7991.327264	26.635482
208.442383	8007.156246	26.640500
208.624473	7997.017483	26.645517
208.901192	8009.875998	26.650535
208.776073	8021.485814	26.655552
209.281640	8034.726961	26.660570
209.290784	8044.249887	26.665588
209.261516	8056.886735	26.670605
209.713261	8067.054526	26.675623
209.461588	8079.925277	26.680640
209.811878	8096.916597	26.685658
210.092572	8116.050276	26.690676
210.113354	8128.059718	26.695693
210.522345	8148.082718	26.700711
210.306850	8153.877741	26.705728
211.022098	8167.812010	26.710746
211.211406	8184.422922	26.715764
211.051658	8202.672022	26.720781
211.340914	8217.620023	26.725799
212.094161	8230.509814	26.730816
211.916081	8249.868765	26.735834
212.133696	8261.115380	26.740852
212.318299	8276.234432	26.745869
212.514104	8284.282584	26.750887
212.941259	8296.751617	26.755904
213.268019	8310.925440	26.760922
213.607871	8323.145111	26.765940
213.364274	8324.250008	26.770957
214.120998	8342.106725	26.775975
214.474858	8336.619102	26.780992
214.665350	8342.500339	26.786010
215.108043	8351.077029	26.791028
214.926133	8343.660267	26.796045
215.344353	8340.297481	26.801063
215.300033	8370.788591	26.806080
215.790457	8368.203107	26.811098
215.655631	8364.494234	26.816116
215.665321	8364.088718	26.821133
216.033008	8388.753100	26.826151
216.057306	8403.260059	26.831168
216.343097	8400.796011	26.836186
216.745204	8423.928104	26.841204
216.748626	8431.103981	26.846221
216.957109	8434.799454	26.851239
216.908444	8458.141989	26.856256
217.236600	8462.706936	26.861274
217.507956	8480.361663	26.866292
217.483599	8493.699912	26.871309
217.821426	8504.850315	26.876327
218.105027	8524.711082	26.881344
218.316436	8544.733540	26.886362
218.548444	8550.633163	26.891380
218.713769	8573.895408	26.896397
219.298379	8568.337855	26.901415
219.352814	8593.071145	26.906432
219.898985	8612.385026	26.911450
220.224868	8619.286051	26.916468
219.965320	8617.397834	26.921485
220.690882	8625.988328	26.926503
220.991087	8626.128491	26.931520
221.208598	8628.767722	26.936538
221.688778	8639.175357	26.941556
221.647153	8661.590632	26.946573
222.250052	8655.483316	26.951591
222.188473	8663.740642	26.956608
222.065203	8659.440547	26.961626
222.463614	8672.384147	26.966644
222.382687	8696.064818	26.971661
222.175376	8697.581216	26.976679
222.803286	8708.832445	26.981696
223.052586	8715.526455	26.986714
223.557702	8737.023067	26.991732
223.181110	8755.178849	26.996749
223.786263	8759.078685	27.001767
223.908213	8780.843839	27.006784
224.012167	8772.228474	27.011802
224.585768	8783.378495	27.016820
224.783415	8806.381265	27.021837
225.142346	8803.783690	27.026855
225.224141	8816.288459	27.031872
225.332971	8828.231806	27.036890
225.867137	8839.096950	27.041908
225.666191	8841.662378	27.046925
225.879408	8860.718360	27.051943
226.131305	8872.107808	27.056960
226.377185	8879.839142	27.061978
227.035396	8895.983731	27.066996
226.576728	8900.358928	27.072013
227.315878	8921.939004	27.077031
227.540582	8936.846414	27.082048
227.901349	8941.855104	27.087066
227.931444	8946.305076	27.092084
227.968980	8961.995919	27.097101
228.197058	8958.380220	27.102119
228.456970	8979.827310	27.107136
228.739015	8979.398582	27.112154
228.443400	8989.182254	27.117172
228.366740	9007.511420	27.122189
228.883500	9017.617814	27.127207
229.429265	9047.016433	27.132224
229.742619	9058.555719	27.137242
229.979107	9067.911499	27.142260
229.875925	9085.383346	27.147277
230.135604	9085.791000	27.152295
230.778534	9104.510393	27.157312
230.699472	9114.022617	27.162330
231.251052	9128.072370	27.167348
231.177262	9153.068889	27.172365
231.487568	9158.054521	27.177383
231.645212	9178.762613	27.182400
231.839599	9182.286507	27.187418
232.031983	9197.468160	27.192436
232.191770	9207.106183	27.197453
232.808457	9225.677253	27.202471
233.182771	9239.242144	27.207488
233.176505	9242.094334	27.212506
233.993041	9257.613489	27.217524
233.741509	9257.761833	27.222541
234.254935	9263.522791	27.227559
234.537620	9285.454928	27.232576
234.300752	9296.598966	27.237594
234.807460	9295.454626	27.242612
235.024145	9313.905559	27.247629
235.365011	9310.764977	27.252647
235.723233	9326.681765	27.257664
235.674912	9338.797344	27.262682
236.046775	9350.974673	27.267700
235.941874	9356.355498	27.272717
236.208412	9374.171146	27.277735
236.331721	9387.981117	27.282752
236.485072	9417.278611	27.287770
236.639291	9427.534525	27.292788
236.782740	9440.055535	27.297805
237.454784	9460.855771	27.302823
237.387200	9470.218982	27.307840
237.590535	9488.140580	27.312858
238.096318	9498.474412	27.317876
237.854705	9533.887938	27.322893
238.613297	9549.723456	27.327911
238.695160	9567.724411	27.332928
239.156846	9576.526280	27.337946
239.562666	9586.772791	27.342964
239.500108	9602.732197	27.347981
239.310235	9615.003852	27.352999
240.018502	9641.781580	27.358016
240.187029	9667.414562	27.363034
240.263247	9663.788488	27.368052
240.142934	9687.086419	27.373069
240.706164	9710.043135	27.378087
241.374589	9728.046859	27.383104
241.473613	9740.330479	27.388122
241.835683	9759.540840	27.393140
242.215976	9767.750522	27.398157
242.551804	9783.763659	27.403175
242.587908	9799.075839	27.408192
242.762129	9804.107132	27.413210
243.316350	9811.182654	27.418228
243.500537	9824.113154	27.423245
243.748594	9826.191323	27.428263
244.200264	9844.439173	27.433280
244.248009	9850.579451	27.438298
244.570945	9850.997099	27.443316
244.769482	9873.489182	27.448333
245.010780	9881.178433	27.453351
245.254532	9874.769524	27.458368
245.195269	9887.011807	27.463386
245.344513	9906.894252	27.468404
245.667805	9920.990515	27.473421
245.669350	9927.659239	27.478439
246.029776	9941.708384	27.483456
245.816247	9954.197723	27.488474
246.723219	9959.434255	27.493492
246.332525	9989.458950	27.498509
246.990887	10002.301353	27.503527
247.173490	10011.568162	27.508544
247.536846	10035.877351	27.513562
247.725665	10049.142082	27.518580
247.673387	10052.396756	27.523597
247.986990	10071.917276	27.528615
248.301025	10088.228981	27.533632
248.476680	10114.733603	27.538650
249.039314	10128.575207	27.543668
249.204292	10141.713198	27.548685
249.702314	10162.741006	27.553703
250.132503	10171.559468	27.558720
249.842427	10178.962152	27.563738
250.653602	10192.349698	27.568756
250.394540	10213.289866	27.573773
250.864695	10225.919496	27.578791
251.326109	10236.622001	27.583808
251.967585	10242.019340	27.588826
252.177950	10251.076054	27.593844
252.102887	10245.729171	27.598861
252.373789	10267.354207	27.603879
253.165838	10273.323708	27.608896
253.009908	10287.328172	27.613914
253.332904	10286.084303	27.618932
253.357732	10312.096711	27.623949
253.367191	10311.725849	27.628967
253.878470	10329.457776	27.633984
253.719265	10341.714646	27.639002
254.049826	10349.453894	27.644020
254.055349	10372.296239	27.649037
254.784724	10389.389306	27.654055
255.017187	10405.056261	27.659072
255.137519	10416.374131	27.664090
255.493590	10420.442612	27.669108
255.683284	10437.348084	27.674125
256.089754	10455.455241	27.679143
256.276491	10459.911119	27.684160
256.417499	10491.330315	27.689178
256.877548	10491.188687	27.694196
257.206942	10510.926135	27.699213
257.578470	10530.873263	27.704231
257.657177	10530.354595	27.709248
257.692938	10546.670458	27.714266
257.873190	10559.519481	27.719284
258.436077	10578.776241	27.724301
258.979487	10587.936164	27.729319
259.391923	10588.870756	27.734336
259.417085	10611.664482	27.739354
259.841315	10605.591644	27.744372
260.144655	10603.482819	27.749389
260.375718	10613.937865	27.754407
260.607862	10623.871976	27.759424
260.698790	10629.754843	27.764442
261.094973	10627.848821	27.769460
261.057797	10646.548305	27.774477
261.207801	10657.955167	27.779495
261.716864	10662.629353	27.784512
261.733071	10695.798211	27.789530
262.052539	10705.514600	27.794548
262.236742	10710.786388	27.799565
261.957929	10728.724878	27.804583
262.686901	10735.141502	27.809600
262.726884	10758.639672	27.814618
263.221480	10765.755467	27.819636
263.552358	10780.709192	27.824653
263.805404	10787.091463	27.829671
264.071791	10797.539972	27.834688
264.034641	10824.344262	27.839706
264.689299	10820.543824	27.844724
264.803304	10832.353868	27.849741
264.989729	10845.604686	27.854759
265.323533	10859.804813	27.859776
265.436839	10890.242999	27.864794
265.484170	10897.978361	27.869812
265.754495	10907.094814	27.874829
266.004379	10932.808474	27.879847
266.260879	10939.554221	27.884864
266.428131	10967.640507	27.889882
266.819181	10983.915902	27.894900
267.173184	11007.129053	27.899917
267.357166	11030.472908	27.904935
267.862820	11035.229709	27.909952
268.167343	11068.726450	27.914970
268.049119	11074.937315	27.919988
268.634687	11102.049866	27.925005
268.630745	11121.504666	27.930023
269.094459	11128.797509	27.935040
269.345395	11159.793204	27.940058
269.734072	11173.284865	27.945076
270.211851	11194.890956	27.950093
269.934589	11211.419437	27.955111
271.099886	11218.543755	27.960128
271.289904	11218.854319	27.965146
271.572385	11249.179983	27.970164
271.875692	11258.015400	27.975181
271.665998	11267.043208	27.980199
272.322835	11271.168299	27.985216
272.291772	11288.428067	27.990234
272.526053	11306.652246	27.995252
272.704912	11322.912816	28.000269
273.025339	11336.321408	28.005287
273.936873	11342.856069	28.010304
273.850831	11364.510369	28.015322
274.126337	11376.979431	28.020340
274.094376	11384.739230	28.025357
274.530183	11404.308822	28.030375
275.129272	11420.075791	28.035392
275.263013	11432.662995	28.040410
275.557411	11442.387147	28.045428
276.173432	11455.666363	28.050445
276.099795	11463.636398	28.055463
276.828559	11467.585712	28.060480
277.376837	11484.317674	28.065498
277.301652	11489.201056	28.070516
277.646362	11480.365397	28.075533
277.269346	11494.353274	28.080551
277.904826	11510.903744	28.085568
277.787562	11525.712012	28.090586
278.024868	11548.308721	28.095604
278.186998	11548.075557	28.100621
278.454356	11580.249584	28.105639
279.013949	11591.825422	28.110656
278.942364	11616.331386	28.115674
279.216215	11638.829178	28.120692
279.239184	11656.006299	28.125709
279.336482	11676.054772	28.130727
279.865013	11702.752349	28.135744
280.340680	11717.859377	28.140762
280.978438	11743.115936	28.145780
280.972956	11747.174707	28.150797
281.214688	11767.226085	28.155815
281.470517	11780.295953	28.160832
281.992375	11805.292951	28.165850
281.894834	11831.267467	28.170868
282.388830	11838.420084	28.175885
282.569171	11859.800721	28.180903
282.501904	11878.241104	28.185920
283.122110	11893.844297	28.190938
283.595857	11903.568870	28.195956
283.972202	11915.350301	28.200973
284.095496	11937.068286	28.205991
284.681332	11940.220470	28.211008
285.090876	11950.743643	28.216026
285.179364	11970.727761	28.221044
285.705793	11988.018563	28.226061
286.009427	12011.574024	28.231079
285.898246	12010.607811	28.236096
286.290365	12021.819406	28.241114
286.335899	12043.468510	28.246132
286.582152	12061.953137	28.251149
286.846432	12093.221022	28.256167
287.361089	12103.756772	28.261184
287.535733	12116.845129	28.266202
287.920625	12141.247679	28.271220
288.598125	12156.655660	28.276237
288.590492	12168.445918	28.281255
288.970100	12189.516536	28.286272
289.101899	12201.869863	28.291290
289.426144	12228.231928	28.296308
289.803297	12232.258764	28.301325
289.933181	12252.305688	28.306343
290.071446	12264.446825	28.311360
290.729651	12278.430418	28.316378
291.088226	12299.588193	28.321396
291.379573	12316.056418	28.326413
291.253090	12329.004299	28.331431
292.032795	12343.413726	28.336448
292.087237	12365.466772	28.341466
292.461254	12388.312986	28.346484
292.547749	12392.791572	28.351501
292.760491	12412.224527	28.356519
292.617660	12430.292006	28.361536
293.136560	12455.032060	28.366554
293.193593	12485.780432	28.371572
293.730413	12509.731237	28.376589
293.933293	12538.677902	28.381607
294.343598	12550.161043	28.386624
294.644926	12579.950274	28.391642
295.198026	12601.607193	28.396660
295.698796	12610.377453	28.401677
295.863761	12629.040123	28.406695
296.171496	12656.155744	28.411712
296.425679	12666.801325	28.416730
296.351863	12687.011850	28.421748
296.849116	12703.033377	28.426765
297.299094	12728.702464	28.431783
297.530331	12749.675542	28.436800
298.041390	12769.067240	28.441818
298.340528	12786.530611	28.446836
298.524729	12797.618123	28.451853
298.981211	12820.148673	28.456871
298.800337	12829.071698	28.461888
299.789867	12847.526710	28.466906
299.803337	12873.991885	28.471924
300.287693	12869.790637	28.476941
300.424909	12898.551865	28.481959
301.007028	12904.706956	28.486976
301.577606	12908.063587	28.491994
301.135485	12926.037932	28.497012
301.638935	12922.307846	28.502029
301.668130	12937.089912	28.507047
301.796304	12957.985828	28.512064
302.535803	12968.366596	28.517082
302.464592	12992.453803	28.522100
303.119855	13005.059593	28.527117
303.281894	13034.396873	28.532135
303.440506	13049.595645	28.537152
304.376538	13048.182751	28.542170
304.549515	13071.332809	28.547188
304.786124	13076.196383	28.552205
305.203527	13083.994226	28.557223
304.872708	13107.295801	28.562240
305.801340	13118.702688	28.567258
305.822406	13137.654604	28.572276
306.166128	13152.290055	28.577293
306.302181	13174.355853	28.582311
306.399730	13194.529082	28.587328
306.716798	13218.397673	28.592346
306.773699	13243.125858	28.597364
307.122092	13262.669671	28.602381
307.302630	13281.559014	28.607399
307.662495	13319.030457	28.612416
308.125677	13342.473090	28.617434
308.265237	13369.611537	28.622452
308.506201	13388.653287	28.627469
308.896204	13429.194654	28.632487
309.165794	13453.593118	28.637504
309.483599	13474.596875	28.642522
309.826720	13500.860159	28.647540
310.105747	13527.097887	28.652557
310.541100	13550.698312	28.657575
310.556831	13580.130222	28.662592
311.214586	13603.068114	28.667610
311.571063	13630.030694	28.672628
311.764457	13657.567276	28.677645
311.747806	13684.300381	28.682663
312.275179	13713.390644	28.687680
313.060890	13740.420781	28.692698
312.969204	13766.287087	28.697716
313.271518	13792.560773	28.702733
314.026545	13817.998084	28.707751
314.132868	13848.211302	28.712768
314.478777	13863.556227	28.717786
314.687731	13892.127624	28.722804
315.121283	13916.717028	28.727821
315.478773	13940.720225	28.732839
316.317879	13955.732714	28.737856
317.618784	13947.056799	28.742874
317.778982	13974.095109	28.747892
318.154796	13967.306482	28.752909
318.956680	13950.062782	28.757927
319.658591	13936.985322	28.762944
320.511766	13928.634385	28.767962
320.380548	13922.043484	28.772980
320.396854	13900.118818	28.777997
320.502656	13896.777660	28.783015
320.769800	13898.388276	28.788032
320.861432	13885.520989	28.793050
320.905409	13906.830837	28.798068
320.681429	13899.705332	28.803085
321.303191	13914.446574	28.808103
321.464847	13923.622184	28.813120
321.461906	13931.658903	28.818138
321.358413	13959.431288	28.823156
321.236194	13965.407514	28.828173
321.732617	13989.671384	28.833191
321.711138	14021.961270	28.838208
322.182754	14031.726883	28.843226
322.248226	14059.773960	28.848244
322.409347	14095.327524	28.853261
322.559692	14132.187901	28.858279
322.556128	14173.762604	28.863296
323.073552	14192.737300	28.868314
323.182070	14235.294315	28.873332
323.576094	14270.916737	28.878349
324.061783	14302.029149	28.883367
324.246722	14355.661206	28.888384
324.506244	14385.927192	28.893402
325.680753	14422.017599	28.898420
326.227716	14451.214672	28.903437
326.454184	14471.010294	28.908455
326.795391	14501.028089	28.913472
327.290984	14516.350338	28.918490
327.451151	14555.433852	28.923508
327.740009	14576.251557	28.928525
328.280166	14599.795110	28.933543
328.430402	14629.639979	28.938560
328.925535	14647.744189	28.943578
329.424262	14675.264857	28.948596
330.021778	14691.799674	28.953613
330.621618	14712.327901	28.958631
330.849187	14727.907646	28.963648
331.429229	14730.501848	28.968666
331.621431	14751.893765	28.973684
332.396357	14765.365230	28.978701
333.090082	14759.023082	28.983719
332.906612	14764.314722	28.988736
333.569887	14782.700061	28.993754
333.830968	14783.623026	28.998772
334.065217	14798.196187	29.003789
335.152823	14777.507697	29.008807
335.463655	14776.077185	29.013824
335.650147	14785.835457	29.018842
335.692461	14805.357893	29.023860
335.869864	14807.155304	29.028877
336.028220	14813.364193	29.033895
335.658905	14829.709881	29.038912
336.278944	14837.720777	29.043930
336.243040	14863.582699	29.048948
336.289658	14877.224110	29.053965
337.114931	14903.288191	29.058983
336.911465	14936.632997	29.064000
337.221289	14953.193810	29.069018
337.370889	14982.899155	29.074036
337.899626	15006.535031	29.079053
338.022337	15027.924669	29.084071
338.410792	15064.530081	29.089088
338.714153	15086.253865	29.094106
338.770158	15121.946903	29.099124
339.075123	15156.902013	29.104141
340.082848	15176.437879	29.109159
341.348331	15178.724422	29.114176
341.768303	15193.156752	29.119194
342.615494	15212.899011	29.124212
342.535931	15229.007823	29.129229
343.040689	15227.478860	29.134247
342.637749	15238.019361	29.139264
342.870599	15252.495439	29.144282
343.549372	15275.263550	29.149300
343.658469	15289.323631	29.154317
343.475954	15300.661327	29.159335
343.630682	15332.353957	29.164352
343.914896	15351.143355	29.169370
344.203299	15372.535862	29.174388
344.503243	15403.608723	29.179405
344.807621	15440.268345	29.184423
345.103976	15470.068401	29.189440
345.273235	15486.936812	29.194458
345.928118	15512.521074	29.199476
345.991722	15540.700236	29.204493
346.614850	15578.925925	29.209511
347.089140	15610.635353	29.214528
347.230342	15632.623223	29.219546
347.687584	15656.927599	29.224564
347.958816	15691.084028	29.229581
348.649296	15715.962874	29.234599
349.010596	15737.662133	29.239616
349.379639	15762.811962	29.244634
350.422485	15770.619104	29.249652
350.970927	15782.362143	29.254669
351.379768	15793.880921	29.259687
351.562060	15810.189530	29.264704
351.957168	15833.410620	29.269722
352.525974	15826.611240	29.274740
352.434999	15845.301186	29.279757
352.947966	15855.830203	29.284775
353.076539	15872.191931	29.289792
353.204913	15895.406982	29.294810
353.464818	15903.112557	29.299828
353.766458	15941.230150	29.304845
354.066869	15953.884575	29.309863
354.452907	15989.099092	29.314880
354.439900	16004.396894	29.319898
354.950266	16028.144476	29.324916
355.280692	16066.599613	29.329933
355.684640	16071.645921	29.334951
355.764397	16108.438918	29.339968
356.102777	16141.555860	29.344986
356.996704	16153.564895	29.350004
357.528971	16177.542335	29.355021
357.897803	16198.087160	29.360039
358.419581	16219.583859	29.365056
358.487215	16234.633621	29.370074
359.141789	16258.527812	29.375092
359.284775	16284.223536	29.380109
359.519811	16304.852193	29.385127
359.930158	16325.309892	29.390144
360.236946	16357.564014	29.395162
360.848340	16371.141211	29.400180
360.579169	16404.436846	29.405197
361.139038	16421.130987	29.410215
361.615423	16441.261035	29.415232
362.264668	16475.485544	29.420250
363.010506	16489.617412	29.425268
363.046108	16519.803154	29.430285
363.467326	16530.194951	29.435303
363.622829	16546.839753	29.440320
363.841486	16565.125993	29.445338
364.339863	16600.212815	29.450356
364.480577	16618.489995	29.455373
364.741782	16643.110545	29.460391
365.038693	16670.527797	29.465408
365.189210	16701.602708	29.470426
365.930572	16730.525645	29.475444
365.624249	16767.998991	29.480461
365.815091	16798.388011	29.485479
366.606679	16820.258386	29.490496
366.709046	16861.001030	29.495514
368.101595	16888.266582	29.500532
368.215059	16903.727055	29.505549
368.669286	16929.652657	29.510567
369.010484	16961.260691	29.515584
368.751710	16983.417687	29.520602
369.299378	16994.668344	29.525620
369.728889	17026.561327	29.530637
370.044723	17054.568760	29.535655
370.620712	17074.858005	29.540672
370.672795	17105.647376	29.545690
371.391575	17126.311769	29.550708
371.540698	17155.511957	29.555725
372.167997	17173.344791	29.560743
372.287130	17201.315790	29.565760
372.568015	17222.510178	29.570778
373.251801	17250.177809	29.575796
373.545096	17277.503664	29.580813
374.128216	17300.273133	29.585831
374.820589	17324.049095	29.590848
374.760723	17352.168308	29.595866
375.584847	17366.682009	29.600884
375.881433	17404.851106	29.605901
375.749077	17409.504561	29.610919
376.550471	17438.967333	29.615936
376.523236	17474.862134	29.620954
376.859230	17493.443600	29.625972
377.185566	17534.489606	29.630989
377.355210	17563.453804	29.636007
378.059159	17591.610478	29.641024
378.277002	17629.700167	29.646042
379.064230	17639.409204	29.651060
379.258638	17665.218331	29.656077
379.815122	17700.405025	29.661095
380.357971	17727.803665	29.666112
380.682548	17753.145194	29.671130
381.183182	17769.547880	29.676148
381.201680	17789.214941	29.681165
381.828197	17819.796713	29.686183
382.137900	17843.223981	29.691200
382.281991	17871.434724	29.696218
382.868201	17900.278290	29.701236
383.866473	17909.608779	29.706253
384.291468	17934.178817	29.711271
385.142626	17943.287847	29.716288
385.221393	17963.706497	29.721306
385.414069	17978.087599	29.726324
385.613954	17998.008525	29.731341
385.874037	18016.231160	29.736359
386.342525	18040.764179	29.741376
386.596820	18055.770399	29.746394
387.069312	18076.478472	29.751412
387.403322	18097.617862	29.756429
387.481203	18128.332327	29.761447
387.836000	18151.544454	29.766464
387.945746	18186.566777	29.771482
388.529152	18206.261873	29.776500
388.834888	18235.560904	29.781517
388.912704	18278.362014	29.786535
389.420885	18297.754432	29.791552
389.801435	18335.661068	29.796570
390.090968	18369.692292	29.801588
391.158071	18393.084376	29.806605
391.340340	18429.157672	29.811623
392.080278	18449.391418	29.816640
392.075194	18472.663775	29.821658
392.513472	18494.084295	29.826676
393.000542	18527.416195	29.831693
393.074807	18566.012691	29.836711
393.831073	18585.654301	29.841728
393.527243	18609.687452	29.846746
393.958638	18629.554912	29.851764
394.485618	18666.042818	29.856781
394.968769	18708.359938	29.861799
395.570011	18723.447856	29.866816
395.455509	18757.293178	29.871834
396.012105	18783.444295	29.876852
396.376511	18807.311550	29.881869
396.632747	18842.419690	29.886887
397.006177	18863.326493	29.891904
397.055163	18904.740396	29.896922
397.655790	18943.950285	29.901940
398.090477	18979.628133	29.906957
398.446284	19016.372252	29.911975
398.981748	19051.218469	29.916992
399.557299	19106.054343	29.922010
400.123372	19121.383363	29.927028
400.557407	19158.378075	29.932045
400.952764	19197.550138	29.937063
401.425372	19224.059576	29.942080
401.373156	19265.513254	29.947098
401.900208	19298.253591	29.952116
402.451553	19326.159514	29.957133
402.718105	19363.076874	29.962151
403.452558	19384.826128	29.967168
403.716645	19433.312565	29.972186
403.935768	19467.282048	29.977204
404.315567	19498.068694	29.982221
404.873863	19534.958465	29.987239
405.501424	19551.947218	29.992256
406.007950	19590.710755	29.997274
406.518876	19625.048293	30.002292
406.965143	19655.844684	30.007309
406.823112	19681.674979	30.012327
407.642433	19722.573535	30.017344
407.886919	19752.173910	30.022362
408.533462	19787.419422	30.027380
408.866472	19813.339702	30.032397
409.226597	19852.531763	30.037415
409.508253	19887.043507	30.042432
409.765553	19917.055105	30.047450
410.217279	19952.544586	30.052468
410.681237	19986.127605	30.057485
410.915555	20026.504484	30.062503
411.423706	20066.509621	30.067520
411.874012	20107.353747	30.072538
412.119472	20141.883064	30.077556
412.544918	20188.104541	30.082573
412.764415	20231.438915	30.087591
413.333216	20255.334195	30.092608
413.071768	20306.543376	30.097626
413.694509	20362.537482	30.102644
414.749027	20391.804202	30.107661
415.029158	20451.342988	30.112679
415.750570	20476.308984	30.117696
416.148258	20509.929285	30.122714
416.906856	20521.565110	30.127732
418.337760	20534.369491	30.132749
418.775974	20567.827090	30.137767
419.444088	20565.978863	30.142784
419.362960	20576.415653	30.147802
419.519401	20587.727434	30.152820
420.378589	20609.407113	30.157837
420.314269	20633.223633	30.162855
421.114281	20652.324359	30.167872
420.862426	20683.225987	30.172890
421.401130	20707.842708	30.177908
421.884367	20730.649229	30.182925
421.673956	20759.827144	30.187943
422.433022	20759.601929	30.192960
423.115628	20786.339106	30.197978
423.654878	20806.941727	30.202996
423.756910	20827.954402	30.208013
424.264578	20852.125567	30.213031
424.770129	20871.193469	30.218048
425.169550	20889.590021	30.223066
425.137677	20920.040880	30.228084
425.570011	20946.127728	30.233101
425.450318	20978.699707	30.238119
426.030219	21007.906019	30.243136
426.583782	21035.934250	30.248154
426.319878	21071.332114	30.253172
427.070384	21114.325136	30.258189
427.211182	21146.311790	30.263207
427.707725	21179.682084	30.268224
428.449500	21226.000502	30.273242
429.164828	21262.672478	30.278260
429.746056	21294.367094	30.283277
429.731502	21332.470697	30.288295
430.639301	21366.594511	30.293312
431.213104	21395.796203	30.298330
431.678858	21429.949424	30.303348
432.078675	21460.882978	30.308365
432.479031	21495.159141	30.313383
432.935368	21525.678208	30.318400
433.473618	21549.444808	30.323418
433.761678	21589.829122	30.328436
434.286240	21605.399097	30.333453
434.452396	21657.813767	30.338471
434.845481	21688.086627	30.343488
435.214965	21724.221048	30.348506
435.693821	21752.289685	30.353524
436.051454	21795.190451	30.358541
436.570118	21828.342340	30.363559
437.151649	21862.336874	30.368576
437.679651	21905.168625	30.373594
437.793858	21950.439088	30.378612
438.687043	21976.555048	30.383629
439.008135	22005.281016	30.388647
439.269560	22033.592793	30.393664
439.901856	22075.267648	30.398682
440.309589	22101.114392	30.403700
442.345949	22100.421576	30.408717
442.598723	22103.315744	30.413735
443.226067	22128.687711	30.418752
443.585391	22147.628402	30.423770
443.748280	22157.680319	30.428788
444.488913	22165.867131	30.433805
444.670325	22198.862901	30.438823
445.046940	22212.234747	30.443840
445.564923	22223.757205	30.448858
445.309131	22222.997307	30.453876
445.996186	22253.851491	30.458893
446.032186	22285.394131	30.463911
446.676696	22313.398344	30.468928
447.268234	22333.084339	30.473946
447.490531	22357.703995	30.478964
447.810674	22389.972265	30.483981
448.223772	22429.147329	30.488999
448.324964	22455.455502	30.494016
448.771295	22489.210428	30.499034
448.905119	22526.199340	30.504052
449.665034	22559.892860	30.509069
450.015961	22598.291810	30.514087
450.199512	22627.737058	30.519104
450.910649	22667.227414	30.524122
451.102385	22702.821060	30.529140
451.584053	22727.980022	30.534157
451.823864	22771.003747	30.539175
451.958709	22807.889031	30.544192
452.740344	22855.227089	30.549210
452.912058	22878.305863	30.554228
453.265703	22923.632185	30.559245
453.745356	22974.720027	30.564263
453.905167	23025.750767	30.569280
454.496654	23066.342075	30.574298
454.907917	23119.196760	30.579316
455.725246	23145.735540	30.584333
456.399998	23192.100438	30.589351
456.667963	23236.293859	30.594368
457.772090	23265.491117	30.599386
457.879574	23306.262733	30.604404
458.095892	23338.685661	30.609421
458.477591	23379.582211	30.614439
458.757183	23429.031562	30.619456
459.833580	23462.686926	30.624474
460.129373	23508.060682	30.629492
460.901734	23542.485771	30.634509
460.959171	23587.770023	30.639527
461.875798	23622.535580	30.644544
462.289771	23664.278986	30.649562
462.574138	23706.345215	30.654580
462.994439	23737.224328	30.659597
463.757316	23779.003103	30.664615
464.141564	23818.138850	30.669632
464.493120	23849.398588	30.674650
465.182674	23897.699427	30.679668
465.546370	23924.961319	30.684685
466.114538	23971.046422	30.689703
466.387910	24014.430410	30.694720
466.890053	24048.775250	30.699738
467.391500	24092.332866	30.704756
468.130761	24101.321949	30.709773
468.575998	24150.572413	30.714791
468.860492	24182.228678	30.719808
470.655420	24188.210236	30.724826
471.471535	24215.268137	30.729844
471.759139	24232.144621	30.734861
472.283138	24252.589972	30.739879
472.602482	24266.316733	30.744896
473.341477	24276.381452	30.749914
473.900710	24301.182926	30.754932
474.183114	24303.394453	30.759949
474.441423	24326.602734	30.764967
474.820067	24351.238730	30.769984
475.228130	24369.524089	30.775002
475.396258	24407.668891	30.780020
475.599222	24414.624592	30.785037
476.165782	24453.122799	30.790055
476.090244	24491.033861	30.795072
476.459168	24507.852955	30.800090
477.284959	24531.329969	30.805108
478.410780	24550.256422	30.810125
478.801060	24581.265057	30.815143
478.984308	24609.781769	30.820160
479.827697	24640.197996	30.825178
479.940630	24677.538830	30.830196
480.340967	24705.789402	30.835213
480.466101	24728.162451	30.840231
481.359601	24764.389771	30.845248
481.855592	24787.335264	30.850266
482.372204	24816.143897	30.855284
482.815912	24838.984597	30.860301
483.301465	24871.513959	30.865319
483.585310	24910.911750	30.870336
484.004417	24921.452630	30.875354
484.104704	24949.649355	30.880372
484.297346	24980.896555	30.885389
485.034649	25014.235977	30.890407
485.572129	25046.466871	30.895424
486.103080	25082.035947	30.900442
486.431176	25119.007672	30.905460
486.733603	25155.848112	30.910477
487.346642	25193.876612	30.915495
487.504602	25235.453474	30.920512
487.886315	25272.120134	30.925530
488.093115	25325.744210	30.930548
489.137241	25365.723298	30.935565
488.973801	25407.902780	30.940583
489.647719	25470.139435	30.945600
490.726423	25499.007259	30.950618
491.575845	25534.609543	30.955636
492.143408	25567.356860	30.960653
492.252732	25607.781959	30.965671
493.007153	25650.907251	30.970688
493.639370	25681.026057	30.975706
493.746149	25725.788894	30.980724
494.354825	25765.670911	30.985741
494.799744	25802.400753	30.990759
494.922120	25860.800254	30.995776
495.619703	25885.618899	31.000794
495.824987	25953.713719	31.005812
496.316849	25990.660118	31.010829
496.829710	26036.898754	31.015847
497.619851	26079.038208	31.020864
498.310931	26113.567147	31.025882
498.534597	26168.213033	31.030900
499.129193	26199.225354	31.035917
499.783351	26248.920290	31.040935
499.973595	26297.266664	31.045952
500.462018	26340.882624	31.050970
500.793798	26395.990733	31.055988
501.516467	26450.018396	31.061005
502.045784	26492.943455	31.066023
502.021622	26546.890425	31.071040
502.737115	26594.364957	31.076058
503.511083	26643.457570	31.081076
503.899753	26687.876416	31.086093
505.065049	26733.484931	31.091111
505.579335	26782.567445	31.096128
506.091000	26815.468369	31.101146
506.755218	26845.325237	31.106164
507.604163	26870.902463	31.111181
508.400539	26908.793900	31.116199
508.824043	26936.123195	31.121216
509.751252	26960.381619	31.126234
510.140122	26987.085858	31.131252
510.572650	27016.744920	31.136269
511.406260	27040.312405	31.141287
511.531458	27072.385293	31.146304
512.045394	27086.037831	31.151322
512.328199	27124.371491	31.156340
512.448305	27160.161356	31.161357
513.164072	27185.855804	31.166375
513.274058	27234.101411	31.171392
513.875983	27264.489842	31.176410
514.055899	27308.676820	31.181428
514.831624	27349.272912	31.186445
515.118042	27389.338386	31.191463
515.605862	27428.181247	31.196480
515.724042	27479.530230	31.201498
516.466624	27530.523300	31.206516
516.701579	27560.108851	31.211533
517.417652	27600.724903	31.216551
517.428187	27657.130121	31.221568
517.990980	27695.964284	31.226586
518.384237	27743.564890	31.231604
519.093869	27792.993221	31.236621
519.540439	27839.165667	31.241639
520.066465	27891.646882	31.246656
520.812863	27938.328162	31.251674
521.523503	27974.087876	31.256692
522.226682	28007.397753	31.261709
523.011903	28046.943410	31.266727
523.342514	28104.858468	31.271744
523.649543	28142.354371	31.276762
524.245586	28179.953778	31.281780
525.068187	28232.626523	31.286797
525.181502	28264.164135	31.291815
525.508775	28318.506206	31.296832
525.831564	28361.085322	31.301850
526.650154	28417.447134	31.306868
527.144677	28466.345258	31.311885
528.361725	28506.583687	31.316903
528.680902	28560.722801	31.321920
529.029710	28603.244558	31.326938
529.969727	28646.346502	31.331956
530.114439	28689.672124	31.336973
530.520080	28731.515946	31.341991
531.144537	28788.813463	31.347008
531.605333	28834.121779	31.352026
531.774326	28884.015263	31.357044
532.321686	28936.070186	31.362061
533.097952	28976.300881	31.367079
533.752000	29042.853683	31.372096
534.048418	29085.420017	31.377114
535.033780	29134.254272	31.382132
535.411773	29185.211789	31.387149
536.365015	29205.452924	31.392167
537.165966	29265.426402	31.397184
537.570485	29308.997503	31.402202
538.292679	29342.720068	31.407220
538.341859	29386.337755	31.412237
539.423604	29417.804955	31.417255
539.704602	29463.274113	31.422272
540.368413	29502.597160	31.427290
541.285018	29538.076646	31.432308
541.417106	29588.066605	31.437325
541.798063	29626.717584	31.442343
542.381372	29657.955658	31.447360
542.632724	29713.633438	31.452378
543.170004	29758.461362	31.457396
543.567855	29813.758622	31.462413
544.167651	29854.585387	31.467431
544.582649	29909.504659	31.472448
544.990677	29962.188377	31.477466
545.918606	30013.508138	31.482484
546.161737	30059.571960	31.487501
546.983231	30108.972505	31.492519
547.614897	30156.568493	31.497536
547.852360	30205.624599	31.502554
548.425892	30258.430006	31.507572
548.796303	30304.605845	31.512589
549.612066	30354.071133	31.517607
550.190705	30404.109147	31.522624
550.616690	30454.406130	31.527642
551.998751	30476.890201	31.532660
552.751390	30510.502690	31.537677
553.458715	30551.177551	31.542695
553.844533	30590.669101	31.547712
554.346847	30624.692527	31.552730
555.325412	30631.051819	31.557748
555.382060	30676.485655	31.562765
556.143673	30692.204362	31.567783
556.639683	30717.230625	31.572800
557.180623	30753.863482	31.577818
557.597725	30771.889080	31.582836
557.835893	30817.501374	31.587853
558.439602	30841.759006	31.592871
558.918356	30875.979295	31.597888
559.038034	30923.839077	31.602906
559.618415	30955.288191	31.607924
559.730762	31017.615876	31.612941
560.481922	31064.724360	31.617959
560.900965	31121.423116	31.622976
560.834774	31181.133820	31.627994
561.533298	31232.798144	31.633012
561.975235	31295.135177	31.638029
562.375987	31367.393022	31.643047
562.926987	31426.737020	31.648064
563.353316	31503.127702	31.653082
563.983839	31561.995125	31.658100
564.903710	31628.731297	31.663117
565.296524	31690.787597	31.668135
565.840621	31750.525085	31.673152
566.681143	31822.453023	31.678170
567.435178	31870.377253	31.683188
568.923090	31910.950870	31.688205
569.792648	31966.113446	31.693223
570.339182	32002.340929	31.698240
570.652295	32059.404218	31.703258
571.624091	32097.448181	31.708276
571.662165	32148.634809	31.713293
572.451388	32199.605338	31.718311
573.095300	32228.960464	31.723328
573.209469	32290.626541	31.728346
574.088142	32331.053023	31.733364
574.820877	32378.177538	31.738381
575.341242	32429.117646	31.743399
575.884511	32474.961225	31.748416
576.278878	32529.586005	31.753434
577.145572	32566.105419	31.758452
577.886264	32627.599204	31.763469
578.027397	32663.939540	31.768487
578.757615	32717.786525	31.773504
578.914876	32776.578804	31.778522
579.733137	32817.212069	31.783540
580.016380	32886.917584	31.788557
580.490322	32936.210215	31.793575
580.884001	32988.536149	31.798592
581.371789	33054.620522	31.803610
582.070893	33101.222413	31.808628
582.613134	33168.342652	31.813645
582.729826	33238.042488	31.818663
583.886099	33288.901550	31.823680
584.103355	33356.341532	31.828698
584.453376	33418.019683	31.833716
585.057041	33487.144196	31.838733
585.610450	33561.203254	31.843751
586.549049	33624.239121	31.848768
586.744343	33699.516342	31.853786
588.062499	33757.516346	31.858804
588.593024	33820.175724	31.863821
589.367456	33883.280793	31.868839
590.277980	33936.236865	31.873856
590.886575	33992.165414	31.878874
591.631673	34036.360625	31.883892
591.920065	34087.738464	31.888909
592.276469	34139.931958	31.893927
592.984534	34179.112909	31.898944
593.594110	34223.807605	31.903962
594.606839	34271.102076	31.908980
594.552824	34320.675550	31.913997
594.939050	34378.908072	31.919015
595.449661	34430.325732	31.924032
595.950459	34499.654279	31.929050
596.867025	34542.392695	31.934068
597.491137	34609.899231	31.939085
597.706450	34672.153188	31.944103
598.253621	34729.807855	31.949120
598.648491	34787.440659	31.954138
599.378724	34842.209251	31.959156
600.098217	34915.817142	31.964173
600.650184	34964.297669	31.969191
602.031352	35015.342067	31.974208
602.894927	35061.918610	31.979226
604.317644	35097.094843	31.984244
604.874525	35144.072834	31.989261
605.808317	35182.072906	31.994279
606.540132	35218.168864	31.999296
606.647626	35249.824037	32.004314
607.768984	35277.179797	32.009332
607.746375	35318.700039	32.014349
608.497901	35362.556619	32.019367
608.855454	35398.503641	32.024384
609.137830	35456.166741	32.029402
609.745129	35500.883938	32.034420
610.222774	35551.426616	32.039437
610.589399	35602.284534	32.044455
611.048478	35661.913534	32.049472
611.303361	35726.026608	32.054490
611.999831	35791.704556	32.059508
612.628224	35855.377344	32.064525
612.966487	35926.969703	32.069543
613.526925	35986.851210	32.074560
613.990335	36047.935707	32.079578
614.879363	36122.950085	32.084596
615.213695	36191.861482	32.089613
615.945135	36275.970109	32.094631
616.450802	36334.021854	32.099648
616.901836	36421.075030	32.104666
617.803091	36473.907580	32.109684
618.738908	36550.090047	32.114701
618.922250	36608.335067	32.119719
620.085471	36677.713503	32.124736
620.487162	36750.867210	32.129754
621.248133	36814.600270	32.134772
621.837955	36881.227812	32.139789
622.114174	36952.260102	32.144807
622.952130	37009.646531	32.149824
624.062020	37082.560887	32.154842
624.718565	37138.548071	32.159860
625.214013	37206.846358	32.164877
625.387274	37275.895939	32.169895
626.246973	37343.424093	32.174912
627.004930	37400.559917	32.179930
628.454133	37441.865886	32.184948
629.924069	37483.632486	32.189965
630.182242	37533.207128	32.194983
631.429254	37571.958786	32.200000
631.826484	37615.901769	32.205018
632.477113	37660.891721	32.210036
633.006591	37698.156215	32.215053
633.363786	37744.656489	32.220071
633.935951	37766.552045	32.225088
634.515524	37828.933152	32.230106
634.813526	37854.349506	32.235124
635.486863	37896.489219	32.240141
635.688197	37952.958521	32.245159
636.132832	37999.530150	32.250176
636.587655	38055.638882	32.255194
636.811152	38104.463300	32.260212
637.462592	38166.025585	32.265229
637.413038	38239.247588	32.270247
638.376548	38299.742131	32.275264
638.951596	38377.968122	32.280282
639.801920	38451.167812	32.285300
640.029404	38518.132979	32.290317
640.480670	38594.537059	32.295335
641.266194	38670.200993	32.300352
641.362513	38752.125448	32.305370
642.192355	38832.526964	32.310388
643.142979	38911.469386	32.315405
643.670708	38998.664211	32.320423
644.708805	39066.914091	32.325440
645.521147	39152.884986	32.330458
645.901676	39217.706064	32.335476
646.961607	39278.030010	32.340493
647.828902	39351.997551	32.345511
648.698476	39406.030787	32.350528
649.458743	39478.400408	32.355546
650.414341	39541.548816	32.360564
651.189222	39595.472068	32.365581
651.478104	39669.177071	32.370599
652.394273	39734.289840	32.375616
652.668587	39794.850107	32.380634
653.264234	39856.515737	32.385652
654.091539	39923.086553	32.390669
654.739404	39993.377642	32.395687
655.402781	40053.457470	32.400704
655.910323	40126.796541	32.405722
656.752240	40181.335425	32.410740
658.510455	40226.823346	32.415757
659.583447	40285.415367	32.420775
660.177819	40319.113569	32.425792
660.996764	40351.174042	32.430810
661.373725	40402.087850	32.435828
662.129533	40443.522088	32.440845
662.682625	40485.665640	32.445863
663.285954	40530.146478	32.450880
664.209031	40575.928620	32.455898
664.307075	40631.896133	32.460916
665.506509	40672.363838	32.465933
665.516274	40725.356743	32.470951
666.349249	40768.701437	32.475968
666.978424	40834.885433	32.480986
667.590806	40880.404231	32.486004
668.156168	40944.332562	32.491021
668.647760	40995.311055	32.496039
669.166316	41051.708812	32.501056
669.498042	41103.462339	32.506074
670.045523	41175.921328	32.511092
670.716442	41236.360500	32.516109
671.071387	41305.136223	32.521127
671.754420	41379.249853	32.526144
672.311601	41443.749527	32.531162
672.508387	41522.882006	32.536180
673.558439	41590.113250	32.541197
674.170055	41672.539717	32.546215
675.031587	41738.653641	32.551232
675.708116	41816.403859	32.556250
676.604899	41889.966286	32.561268
677.267692	41953.632519	32.566285
677.811837	42034.711098	32.571303
678.725309	42087.649407	32.576320
679.574339	42142.000327	32.581338
680.089999	42205.884439	32.586356
681.201772	42254.613428	32.591373
681.725175	42309.656645	32.596391
682.176246	42370.694836	32.601408
682.764399	42430.277116	32.606426
683.207192	42496.175966	32.611444
684.001643	42563.443709	32.616461
684.750461	42630.523527	32.621479
685.419154	42686.263577	32.626496
685.977167	42759.184797	32.631514
686.487276	42829.910510	32.636532
687.076195	42897.324089	32.641549
687.355411	42968.170750	32.646567
688.109852	43049.493517	32.651584
688.881235	43138.299738	32.656602
689.193868	43225.774396	32.661620
689.808370	43309.047479	32.666637
690.026737	43392.831887	32.671655
690.445598	43492.622668	32.676672
691.466780	43584.723690	32.681690
692.229351	43684.505789	32.686708
692.765866	43778.349013	32.691725
693.568160	43861.511284	32.696743
694.621920	43963.532485	32.701760
695.345050	44052.638386	32.706778
696.237370	44145.625544	32.711796
697.541086	44227.506359	32.716813
698.509224	44300.438120	32.721831
699.347892	44362.804602	32.726848
700.695873	44438.509260	32.731866
700.708598	44523.062245	32.736884
701.675955	44584.397694	32.741901
702.636582	44654.335588	32.746919
703.162554	44728.337051	32.751936
704.012265	44805.878360	32.756954
704.115554	44878.608627	32.761972
704.711125	44944.534941	32.766989
706.066046	45000.505818	32.772007
706.545541	45086.490009	32.777024
707.615330	45154.109744	32.782042
707.879384	45227.010437	32.787060
709.020173	45287.801536	32.792077
709.879974	45363.875167	32.797095
710.390147	45429.501592	32.802112
711.467815	45484.582117	32.807130
711.755051	45569.934164	32.812148
712.602794	45628.586739	32.817165
712.719158	45704.902010	32.822183
713.558216	45775.761048	32.827200
714.457441	45848.353433	32.832218
715.025220	45931.143818	32.837236
715.685247	45992.844342	32.842253
716.595993	46069.461810	32.847271
717.428148	46153.693429	32.852288
718.271351	46219.270465	32.857306
718.865412	46302.781248	32.862324
719.499889	46361.897813	32.867341
719.991583	46436.031660	32.872359
720.700765	46524.829471	32.877376
721.649442	46597.514415	32.882394
722.174718	46677.956198	32.887412
723.202932	46732.969630	32.892429
724.305313	46810.477225	32.897447
725.262382	46865.834434	32.902464
726.396380	46919.804528	32.907482
727.028792	46971.524345	32.912500
727.878412	47016.725008	32.917517
728.442175	47067.875426	32.922535
728.940468	47132.856036	32.927552
729.328698	47180.085302	32.932570
729.500129	47244.586864	32.937588
730.410096	47312.894559	32.942605
730.352496	47382.288427	32.947623
730.881217	47463.162449	32.952640
731.553282	47540.842365	32.957658
732.209618	47624.579155	32.962676
732.642099	47710.327255	32.967693
733.040158	47804.826125	32.972711
733.581312	47895.868877	32.977728
734.467429	47987.214813	32.982746
735.036741	48094.546438	32.987764
735.299052	48190.348784	32.992781
736.181319	48293.792448	32.997799
737.373279	48386.602268	33.002816
738.557041	48482.875258	33.007834
739.056243	48599.228464	33.012852
739.720019	48693.046493	33.017869
740.790454	48790.142027	33.022887
741.517670	48894.691633	33.027904
742.193290	48976.987825	33.032922
743.474947	49068.677514	33.037940
744.183994	49149.516093	33.042957
745.377257	49246.211393	33.047975
746.270543	49329.682590	33.052992
746.845851	49415.022977	33.058010
747.493311	49511.829177	33.063028
748.084228	49592.749240	33.068045
749.126992	49677.874220	33.073063
749.678916	49770.468524	33.078080
750.501745	49855.804514	33.083098
751.203965	49943.994002	33.088116
751.936608	50025.659850	33.093133
753.095666	50117.561243	33.098151
753.693130	50206.056738	33.103168
755.060759	50278.322906	33.108186
755.498322	50363.522961	33.113204
756.197234	50450.511931	33.118221
756.771515	50550.762462	33.123239
757.096612	50639.128279	33.128256
757.916793	50736.066713	33.133274
758.581625	50833.536792	33.138292
759.435752	50921.828707	33.143309
760.363813	51010.405658	33.148327
761.128223	51098.795397	33.153344
762.159444	51182.637061	33.158362
763.065854	51270.561804	33.163380
763.328241	51369.377472	33.168397
763.888124	51445.187119	33.173415
764.676676	51555.660277	33.178432
765.891966	51639.883986	33.183450
766.392220	51735.724446	33.188468
767.039572	51819.525191	33.193485
768.254661	51915.456341	33.198503
768.346285	52020.210495	33.203520
769.311555	52109.847623	33.208538
770.231614	52208.236174	33.213556
770.565393	52299.836373	33.218573
771.449739	52399.798581	33.223591
772.076762	52503.537755	33.228608
772.740315	52603.202823	33.233626
773.161862	52702.497921	33.238644
773.645977	52815.941229	33.243661
774.585258	52931.868338	33.248679
775.134313	53045.378008	33.253696
776.285249	53143.600265	33.258714
777.288847	53239.326635	33.263732
777.851600	53340.989693	33.268749
778.415150	53438.243209	33.273767
779.130340	53544.949021	33.278784
779.951617	53650.822776	33.283802
780.727865	53748.503734	33.288820
781.650291	53847.418212	33.293837
782.883968	53940.355120	33.298855
783.951018	54043.833534	33.303872
784.651734	54137.902347	33.308890
785.345063	54235.637400	33.313908
786.123666	54329.953247	33.318925
787.120284	54435.391431	33.323943
787.431502	54531.434901	33.328960
788.618913	54620.515897	33.333978
789.428681	54715.384428	33.338996
790.014645	54824.089954	33.344013
791.414528	54918.305479	33.349031
792.216763	55021.245370	33.354048
793.136532	55114.675903	33.359066
793.781952	55196.450515	33.364084
794.377793	55295.824539	33.369101
795.654690	55383.516679	33.374119
796.466432	55475.772638	33.379136
797.039286	55567.689564	33.384154
798.037727	55656.212648	33.389172
798.831676	55751.568991	33.394189
799.907881	55840.863510	33.399207
800.086182	55946.211796	33.404224
801.089757	56028.587536	33.409242
802.076517	56137.252687	33.414260
802.350683	56243.016311	33.419277
803.393778	56339.408321	33.424295
804.250551	56435.926513	33.429312
805.748331	56524.623333	33.434330
806.471958	56616.501123	33.439348
807.547536	56705.382576	33.444365
808.331702	56787.273404	33.449383
808.625901	56876.165266	33.454400
809.547145	56963.342068	33.459418
810.351144	57065.357031	33.464436
810.421663	57154.394685	33.469453
811.564140	57258.458722	33.474471
812.396315	57364.912917	33.479488
812.983785	57460.096858	33.484506
814.318349	57548.945395	33.489524
814.951821	57649.279121	33.494541
815.870867	57740.485070	33.499559
816.589538	57847.636840	33.504576
817.676064	57939.586855	33.509594
819.184427	58018.051148	33.514612
820.581334	58089.121549	33.519629
821.810388	58153.628870	33.524647
822.308305	58228.299417	33.529664
823.047664	58297.741851	33.534682
824.136938	58382.710394	33.539700
824.755244	58457.526117	33.544717
825.748848	58526.560604	33.549735
826.250969	58597.446400	33.554752
827.118878	58671.033399	33.559770
828.034645	58745.358442	33.564788
828.413546	58820.727145	33.569805
829.086244	58900.502743	33.574823
829.696420	58983.979750	33.579840
830.162531	59087.489334	33.584858
831.051611	59164.291374	33.589876
831.193720	59247.297344	33.594893
832.065159	59347.151330	33.599911
832.863562	59437.310627	33.604928
833.174429	59526.028160	33.609946
834.212163	59618.354178	33.614964
834.997250	59722.294375	33.619981
835.732602	59828.992553	33.624999
836.425053	59931.780005	33.630016
836.898876	60030.850162	33.635034
837.858115	60134.118919	33.640052
838.695926	60239.784717	33.645069
839.498084	60344.982973	33.650087
839.776215	60466.814980	33.655104
840.558178	60586.592176	33.660122
841.605502	60701.168703	33.665140
841.970558	60833.954117	33.670157
843.015313	60945.865283	33.675175
844.012981	61074.154625	33.680192
844.841030	61193.061846	33.685210
845.954358	61316.188703	33.690228
847.339119	61433.348959	33.695245
848.339194	61532.067283	33.700263
849.038535	61648.868509	33.705280
849.756994	61764.036518	33.710298
850.865821	61872.958817	33.715316
851.885149	61987.743151	33.720333
852.851419	62094.768815	33.725351
853.845360	62220.708355	33.730368
854.315615	62322.065681	33.735386
855.461970	62422.186185	33.740404
856.254991	62544.248494	33.745421
856.925552	62655.422057	33.750439
857.877209	62778.464441	33.755456
858.778131	62892.628756	33.760474
859.426491	63010.527068	33.765492
860.164403	63116.976505	33.770509
861.619886	63230.488075	33.775527
862.510566	63341.609840	33.780544
863.055260	63449.407845	33.785562
864.944336	63557.552168	33.790580
865.758426	63658.909568	33.795597
866.564588	63761.305456	33.800615
867.678100	63869.162944	33.805632
867.942653	63972.547389	33.810650
869.050725	64086.178220	33.815668
869.470599	64197.098270	33.820685
870.312993	64308.909628	33.825703
870.763951	64424.358149	33.830720
871.426072	64548.337800	33.835738
872.798220	64656.017382	33.840756
873.703295	64775.646825	33.845773
874.515337	64896.531419	33.850791
875.671382	65021.152563	33.855808
876.224328	65130.791190	33.860826
877.263667	65249.579262	33.865844
878.124067	65357.423276	33.870861
878.791082	65481.654216	33.875879
879.921806	65597.154451	33.880896
880.877196	65714.441883	33.885914
881.642979	65831.887881	33.890932
882.205891	65956.119954	33.895949
882.899292	66072.384484	33.900967
884.117082	66198.861045	33.905984
884.821423	66321.409142	33.911002
886.424798	66430.835983	33.916020
887.023731	66552.385082	33.921037
887.937567	66660.713740	33.926055
888.555773	66778.802777	33.931072
889.645818	66889.031607	33.936090
890.277410	66999.033644	33.941108
891.115598	67112.586656	33.946125
892.068127	67217.801236	33.951143
893.169908	67324.875606	33.956160
893.455711	67440.873954	33.961178
894.944716	67542.947443	33.966196
896.149010	67651.536463	33.971213
896.945281	67757.860798	33.976231
897.757595	67873.154537	33.981248
898.600755	67983.645032	33.986266
899.792378	68079.087627	33.991284
900.527498	68192.233624	33.996301
901.024107	68290.207731	34.001319
902.341288	68402.037988	34.006336
902.754693	68517.458347	34.011354
903.931827	68636.906562	34.016372
904.869026	68759.777917	34.021389
905.699113	68863.598400	34.026407
906.498947	68983.281899	34.031424
907.588532	69096.563568	34.036442
908.750088	69200.065122	34.041460
909.427648	69322.881657	34.046477
910.420337	69439.576612	34.051495
911.234190	69549.201234	34.056512
911.946211	69669.529133	34.061530
913.030844	69795.745814	34.066548
913.517643	69917.067260	34.071565
914.799492	70029.835104	34.076583
916.427068	70146.592952	34.081600
917.735313	70248.266838	34.086618
919.513078	70334.188154	34.091636
920.829920	70437.145116	34.096653
921.607137	70523.865573	34.101671
922.678166	70612.263864	34.106688
923.300554	70709.083700	34.111706
924.306688	70805.783373	34.116724
924.772825	70899.215416	34.121741
925.291255	71003.863148	34.126759
926.230365	71100.783944	34.131776
927.039261	71205.858705	34.136794
927.819023	71310.900873	34.141812
928.510808	71430.578050	34.146829
928.886182	71561.001481	34.151847
929.739145	71661.872332	34.156864
930.712630	71799.925325	34.161882
931.523471	71917.726306	34.166900
932.273449	72033.773729	34.171917
933.142008	72179.921881	34.176935
933.978863	72296.576017	34.181952
934.429228	72441.056307	34.186970
935.402407	72577.855880	34.191988
936.129330	72720.205269	34.197005
936.677899	72871.223644	34.202023
937.871240	73020.074452	34.207040
938.303282	73176.540235	34.212058
939.355533	73330.855220	34.217076
939.994155	73485.138760	34.222093
940.767075	73638.180545	34.227111
941.823691	73803.710835	34.232128
942.818754	73968.373527	34.237146
944.245911	74114.587421	34.242164
945.183372	74261.098592	34.247181
946.168061	74424.912659	34.252199
947.362068	74576.398576	34.257216
947.428924	74733.859467	34.262234
949.123831	74884.967135	34.267252
950.320977	75034.299040	34.272269
950.724122	75190.904177	34.277287
952.217212	75323.302318	34.282304
952.764498	75471.391571	34.287322
953.813851	75613.333110	34.292340
954.756907	75754.907395	34.297357
955.517773	75900.832647	34.302375
956.917100	76040.555778	34.307392
957.664457	76182.184252	34.312410
958.673841	76326.192583	34.317428
960.088455	76455.789636	34.322445
961.502977	76591.478415	34.327463
962.594935	76722.692847	34.332480
963.477088	76859.667045	34.337498
964.413059	76994.425699	34.342516
965.507172	77120.480849	34.347533
965.844605	77267.889545	34.352551
967.396045	77389.815893	34.357568
968.422129	77530.995574	34.362586
969.290104	77668.812036	34.367604
970.586811	77785.836457	34.372621
971.481176	77916.489813	34.377639
973.119317	78040.916501	34.382656
973.841880	78172.675181	34.387674
974.885521	78297.347441	34.392692
976.042047	78427.043082	34.397709
977.063866	78559.456506	34.402727
978.638479	78655.501854	34.407744
979.557951	78769.602037	34.412762
980.817686	78886.948309	34.417780
981.390749	79007.299975	34.422797
982.398830	79126.732450	34.427815
983.795837	79235.448496	34.432832
984.665883	79352.052173	34.437850
985.568994	79462.280898	34.442868
986.583523	79575.275033	34.447885
987.264272	79713.938509	34.452903
988.323533	79821.739252	34.457920
989.192979	79954.451860	34.462938
989.818584	80068.398634	34.467956
990.785925	80200.552408	34.472973
991.369971	80334.725304	34.477991
992.206541	80471.476081	34.483008
993.106774	80611.240997	34.488026
994.106837	80760.346581	34.493044
995.088102	80889.174503	34.498061
995.796740	81036.900544	34.503079
996.851797	81181.963634	34.508096
997.745594	81331.925667	34.513114
998.788261	81484.230037	34.518132
999.867496	81624.218198	34.523149
1000.472900	81771.409408	34.528167
1001.718197	81914.901942	34.533184
1002.786744	82078.656895	34.538202
1003.401498	82224.856207	34.543220
1004.998396	82386.127918	34.548237
1005.517816	82544.985641	34.553255
1006.603955	82684.934859	34.558272
1007.558312	82844.469026	34.563290
1008.611411	83012.200064	34.568308
1009.801882	83150.458208	34.573325
1010.613068	83308.500917	34.578343
1011.634513	83467.427217	34.583360
1012.156479	83626.557708	34.588378
1013.451156	83780.657658	34.593396
1015.010524	83932.044707	34.598413
1015.082929	84096.687948	34.603431
1016.386376	84246.765532	34.608448
1018.474249	84393.284605	34.613466
1019.876863	84535.634812	34.618484
1020.910759	84665.924113	34.623501
1021.958689	84801.836751	34.628519
1022.688720	84921.282367	34.633536
1023.607404	85050.783050	34.638554
1024.732409	85182.426830	34.643572
1025.853109	85310.174391	34.648589
1026.541383	85442.613435	34.653607
1027.504580	85577.475323	34.658624
1028.392600	85713.926015	34.663642
1028.967757	85856.586120	34.668660
1030.076244	86006.656785	34.673677
1030.698946	86162.978459	34.678695
1031.565041	86314.787124	34.683712
1032.648029	86472.793576	34.688730
1032.765702	86639.725215	34.693748
1034.221545	86802.721567	34.698765
1035.340982	86963.382945	34.703783
1036.699012	87133.883663	34.708800
1037.985815	87293.412140	34.713818
1038.872528	87461.386326	34.718836
1040.113797	87623.335547	34.723853
1040.990071	87790.617723	34.728871
1042.114768	87950.367376	34.733888
1042.961109	88125.548036	34.738906
1043.682809	88297.896652	34.743924
1044.975960	88453.995687	34.748941
1045.796634	88630.861317	34.753959
1047.043358	88796.348831	34.758976
1048.753846	88975.499455	34.763994
1050.635284	89118.095398	34.769012
1052.364935	89262.812101	34.774029
1053.469972	89406.418254	34.779047
1054.731194	89546.100979	34.784064
1056.667685	89666.136189	34.789082
1057.813885	89801.023453	34.794100
1058.829806	89915.447311	34.799117
1059.942972	90035.570361	34.804135
1060.936736	90163.282944	34.809152
1061.858013	90294.666240	34.814170
1062.724432	90436.710669	34.819188
1063.597210	90557.331889	34.824205
1064.670881	90685.989640	34.829223
1065.491648	90828.936325	34.834240
1066.229564	90965.169977	34.839258
1066.976601	91117.522704	34.844276
1067.936921	91259.062742	34.849293
1068.759179	91413.341522	34.854311
1069.599906	91562.194214	34.859328
1070.877986	91703.019574	34.864346
1071.958814	91874.119111	34.869364
1073.686808	91993.054959	34.874381
1074.774144	92152.478056	34.879399
1075.874771	92289.127337	34.884416
1076.852741	92433.386555	34.889434
1077.606915	92589.374029	34.894452
1079.117152	92717.470122	34.899469
1080.149651	92873.122081	34.904487
1081.396145	93008.244798	34.909504
1082.668942	93143.256297	34.914522
1083.877625	93294.527033	34.919540
1084.985451	93425.022873	34.924557
1086.211313	93564.658727	34.929575
1087.218675	93698.274188	34.934592
1088.804487	93819.793385	34.939610
1089.387504	93961.430726	34.944628
1090.782125	94089.420272	34.949645
1091.628377	94226.559344	34.954663
1092.684975	94344.060936	34.959680
1093.880601	94468.680051	34.964698
1094.545037	94601.604074	34.969716
1095.265558	94723.720730	34.974733
1096.199750	94850.942425	34.979751
1097.130306	94985.368858	34.984768
1098.214230	95127.664063	34.989786
1098.886744	95265.154233	34.994804
1100.031948	95412.384652	34.999821
1101.189746	95558.126284	35.004839
1101.782030	95718.870062	35.009856
1102.800182	95863.826401	35.014874
1103.590227	96023.140366	35.019892
1104.528344	96184.709673	35.024909
1105.904526	96349.353502	35.029927
1106.649993	96521.091756	35.034944
1107.875447	96689.542050	35.039962
1108.993009	96865.595229	35.044980
1109.766434	97027.748063	35.049997
1111.023640	97217.884831	35.055015
1111.839116	97399.182901	35.060032
1113.178244	97568.937007	35.065050
1114.215327	97751.232738	35.070068
1115.421471	97922.385045	35.075085
1116.537130	98113.128164	35.080103
1117.367532	98289.599818	35.085120
1118.718891	98481.034653	35.090138
1119.695254	98688.360355	35.095156
1120.855228	98864.268539	35.100173
1121.868575	99057.485826	35.105191
1122.755331	99255.790406	35.110208
1123.949292	99448.398247	35.115226
1124.684987	99647.851546	35.120244
1125.834284	99851.960839	35.125261
1126.896712	100056.605338	35.130279
1127.936397	100264.572838	35.135296
1129.128896	100466.444935	35.140314
1130.333169	100668.797854	35.145332
1131.930363	100884.452822	35.150349
1132.823414	101086.081902	35.155367
1133.842353	101291.186680	35.160384
1135.278220	101501.086573	35.165402
1136.493568	101709.777430	35.170420
1138.012632	101918.907125	35.175437
1138.935116	102116.062880	35.180455
1139.884609	102328.424590	35.185472
1141.498283	102520.871881	35.190490
1142.791580	102727.633140	35.195508
1144.390430	102925.005760	35.200525
1145.586161	103113.512342	35.205543
1146.645134	103307.475851	35.210560
1147.863686	103500.857105	35.215578
1148.896813	103695.144386	35.220596
1150.423464	103887.590893	35.225613
1151.468842	104065.833207	35.230631
1152.999248	104269.249275	35.235648
1154.656462	104433.195677	35.240666
1156.289178	104593.094477	35.245684
1157.683568	104769.168670	35.250701
1158.755963	104929.035825	35.255719
1159.972744	105100.037773	35.260736
1161.389520	105266.093638	35.265754
1162.951443	105415.725216	35.270772
1164.396223	105543.808375	35.275789
1165.624919	105709.188982	35.280807
1166.391318	105868.960610	35.285824
1167.698766	106026.984280	35.290842
1168.632873	106176.141707	35.295860
1169.401125	106330.077044	35.300877
1170.648962	106481.375267	35.305895
1170.986650	106639.018838	35.310912
1171.827502	106799.011683	35.315930
1172.095562	106968.764511	35.320948
1173.496519	107133.986077	35.325965
1174.795652	107299.884187	35.330983
1175.313087	107489.231176	35.336000
1176.567947	107670.920819	35.341018
1177.122194	107864.089516	35.346036
1178.263511	108046.623841	35.351053
1179.394427	108247.502066	35.356071
1180.566822	108439.432367	35.361088
1181.591137	108641.078532	35.366106
1183.039936	108855.613795	35.371124
1183.897953	109054.997966	35.376141
1185.209412	109252.471684	35.381159
1186.064746	109457.787355	35.386176
1187.477668	109667.559551	35.391194
1188.121471	109893.117569	35.396212
1189.641025	110098.125207	35.401229
1191.235860	110313.255784	35.406247
1192.538365	110525.358359	35.411264
1194.337076	110727.828925	35.416282
1195.425010	110941.414420	35.421300
1196.506061	111152.431166	35.426317
1197.845864	111353.551025	35.431335
1198.891888	111567.870407	35.436352
1200.016855	111765.557899	35.441370
1202.305834	111961.761563	35.446388
1203.398368	112157.062965	35.451405
1205.075939	112358.780201	35.456423
1206.253559	112550.333114	35.461440
1207.748737	112730.382371	35.466458
1208.804893	112932.270207	35.471476
1210.000334	113124.495557	35.476493
1211.380910	113328.118725	35.481511
1212.047985	113516.823838	35.486528
1213.408241	113704.275033	35.491546
1214.685497	113902.319869	35.496564
1215.867430	114101.268754	35.501581
1216.822535	114310.404694	35.506599
1218.057757	114523.663916	35.511616
1218.868964	114715.254449	35.516634
1220.519268	114916.373886	35.521652
1221.720336	115131.949221	35.526669
1222.993275	115338.088059	35.531687
1223.931734	115544.321893	35.536704
1224.868985	115755.207256	35.541722
1225.710875	115969.530884	35.546740
1226.855206	116195.867825	35.551757
1228.156106	116403.732888	35.556775
1229.181333	116635.439869	35.561792
1229.947313	116871.474304	35.566810
1231.366423	117105.603142	35.571828
1232.393445	117337.036756	35.576845
1233.614112	117569.821213	35.581863
1234.528790	117820.308658	35.586880
1235.623562	118058.059538	35.591898
1237.000138	118302.975407	35.596916
1237.915596	118550.630765	35.601933
1239.702072	118790.135575	35.606951
1241.927536	118994.622185	35.611968
1243.521267	119212.595978	35.616986
1245.090106	119438.102377	35.622004
1246.188719	119654.007458	35.627021
1248.361772	119871.763374	35.632039
1249.428602	120083.077093	35.637056
1250.610232	120288.176773	35.642074
1252.014466	120478.022002	35.647092
1252.849106	120675.540789	35.652109
1254.340815	120859.139353	35.657127
1255.288471	121049.786317	35.662144
1256.746282	121246.457910	35.667162
1257.769055	121436.119148	35.672180
1258.286891	121633.671557	35.677197
1260.065919	121829.951596	35.682215
1260.814119	122051.609671	35.687232
1262.112824	122261.329138	35.692250
1263.076921	122467.557213	35.697268
1264.019177	122692.064585	35.702285
1265.399334	122915.449155	35.707303
1266.146511	123148.305766	35.712320
1267.511274	123382.189656	35.717338
1268.506586	123614.780614	35.722356
1269.071992	123863.020218	35.727373
1270.257483	124106.786673	35.732391
1271.739862	124366.981473	35.737408
1272.858521	124617.708247	35.742426
1274.549132	124865.693411	35.747444
1275.408956	125130.725351	35.752461
1276.661803	125383.286579	35.757479
1278.236460	125649.611281	35.762496
1279.283284	125916.127251	35.767514
1280.507922	126171.665445	35.772532
1281.930358	126428.744589	35.777549
1283.833353	126676.126219	35.782567
1285.371769	126938.133450	35.787584
1286.935253	127193.484519	35.792602
1288.450792	127437.045385	35.797620
1289.513557	127689.568394	35.802637
1290.990108	127937.677290	35.807655
1292.369118	128190.633574	35.812672
1293.430774	128443.074166	35.817690
1295.053010	128695.487198	35.822708
1296.127825	128947.308594	35.827725
1297.902373	129203.173534	35.832743
1298.957951	129445.520817	35.837760
1300.077619	129704.008236	35.842778
1301.358194	129953.141663	35.847796
1302.565835	130210.008808	35.852813
1305.063393	130432.312006	35.857831
1307.067120	130667.919881	35.862848
1308.394139	130895.440228	35.867866
1309.857834	131127.591743	35.872884
1311.096691	131351.935546	35.877901
1312.095418	131583.318180	35.882919
1313.880335	131809.133838	35.887936
1314.875162	132040.989464	35.892954
1316.444258	132268.340002	35.897972
1317.201309	132514.918189	35.902989
1318.503861	132730.742228	35.908007
1320.030061	132963.708007	35.913024
1321.675411	133194.120279	35.918042
1322.892344	133416.872142	35.923060
1324.005581	133664.452232	35.928077
1325.446680	133886.384144	35.933095
1326.862742	134105.519998	35.938112
1328.170839	134339.837612	35.943130
1329.588300	134555.768831	35.948148
1330.154858	134803.321458	35.953165
1331.308621	135024.712905	35.958183
1332.181305	135273.701613	35.963200
1333.462156	135528.354979	35.968218
1334.869410	135765.658341	35.973236
1335.859266	136019.780564	35.978253
1337.835866	136254.710928	35.983271
1339.311642	136491.107964	35.988288
1340.146109	136731.239093	35.993306
1341.942352	136941.848845	35.998324
1343.303658	137180.843514	36.003341
1344.463321	137412.025183	36.008359
1345.787979	137640.302986	36.013376
1347.499472	137861.772997	36.018394
1348.591485	138083.359886	36.023412
1349.982127	138323.422863	36.028429
1351.244976	138551.970682	36.033447
1353.031504	138788.471853	36.038464
1354.404365	139020.326559	36.043482
1355.497039	139238.459442	36.048500
1356.530234	139481.886561	36.053517
1357.606420	139714.213622	36.058535
1359.040256	139952.391690	36.063552
1360.245892	140219.227567	36.068570
1361.656251	140466.365043	36.073588
1362.699381	140717.762275	36.078605
1364.234024	140966.366289	36.083623
1365.588534	141227.593379	36.088640
1366.609742	141484.553745	36.093658
1367.989083	141755.747390	36.098676
1369.152692	142031.784826	36.103693
1370.588567	142299.651052	36.108711
1371.796597	142562.205879	36.113728
1373.135342	142854.261807	36.118746
1374.588334	143114.624417	36.123764
1375.754260	143393.144967	36.128781
1377.502231	143671.228801	36.133799
1378.997191	143947.150263	36.138816
1380.497732	144223.884548	36.143834
1381.409841	144498.727601	36.148852
1383.144993	144778.787856	36.153869
1384.501634	145061.703022	36.158887
1385.962469	145344.248060	36.163904
1386.945310	145618.923133	36.168922
1388.284678	145908.163352	36.173940
1389.425145	146203.843263	36.178957
1391.227739	146491.806551	36.183975
1393.089748	146775.260110	36.188992
1394.670009	147064.875453	36.194010
1396.346016	147339.879830	36.199028
1397.528964	147625.735444	36.204045
1398.825386	147907.985310	36.209063
1400.303219	148186.148815	36.214080
1401.831409	148465.878732	36.219098
1403.488030	148734.073457	36.224116
1405.308647	149014.532689	36.229133
1406.246240	149298.907336	36.234151
1408.127127	149569.163612	36.239168
1409.351457	149853.469578	36.244186
1410.868256	150122.255569	36.249204
1412.157935	150394.721287	36.254221
1413.997213	150661.022452	36.259239
1415.902812	150917.066174	36.264256
1416.930242	151201.351577	36.269274
1418.703175	151448.834061	36.274292
1420.109161	151717.776647	36.279309
1421.588330	151974.862209	36.284327
1423.116849	152231.713010	36.289344
1424.724209	152497.012758	36.294362
1426.150413	152747.313625	36.299380
1427.385126	153011.258097	36.304397
1428.735514	153272.635642	36.309415
1430.211903	153520.231446	36.314432
1431.678394	153769.213090	36.319450
1433.323180	154019.130797	36.324468
1435.152539	154257.019799	36.329485
1436.582479	154489.065392	36.334503
1438.804455	154705.759237	36.339520
1440.163803	154919.616378	36.344538
1442.221484	155122.652781	36.349556
1444.222882	155326.105490	36.354573
1445.394095	155538.969716	36.359591
1446.775032	155736.654236	36.364608
1447.967418	155947.030861	36.369626
1449.302186	156151.156518	36.374644
1450.150163	156375.051619	36.379661
1450.876624	156599.906851	36.384679
1453.000784	156813.241490	36.389696
1454.119980	157044.693994	36.394714
1455.113490	157279.441574	36.399732
1455.981818	157535.624787	36.404749
1456.818803	157786.613647	36.409767
1458.077136	158038.637873	36.414784
1459.410935	158307.460063	36.419802
1460.518612	158573.619401	36.424820
1461.765176	158846.722140	36.429837
1462.459068	159140.609586	36.434855
1464.079894	159426.137394	36.439872
1464.896406	159721.036263	36.444890
1466.067047	160031.965009	36.449908
1467.548037	160351.052868	36.454925
1468.956780	160653.725894	36.459943
1471.404114	160962.331259	36.464960
1472.519596	161276.424809	36.469978
1474.010830	161584.901518	36.474996
1475.736466	161894.876766	36.480013
1476.813016	162216.824426	36.485031
1478.422757	162522.712869	36.490048
1479.599124	162849.660265	36.495066
1481.253934	163177.482405	36.500084
1483.248115	163501.634844	36.505101
1484.267654	163832.472797	36.510119
1486.332685	164140.378136	36.515136
1488.432048	164443.217541	36.520154
1490.247963	164741.360789	36.525172
1492.261600	165054.965361	36.530189
1493.685764	165353.533036	36.535207
1495.393547	165642.856798	36.540224
1496.972410	165955.271117	36.545242
1498.565822	166239.149136	36.550260
1500.089686	166534.726566	36.555277
1501.418821	166842.937963	36.560295
1502.759056	167139.780668	36.565312
1504.022641	167447.791425	36.570330
1505.576377	167747.825710	36.575348
1507.314827	168048.351624	36.580365
1508.363088	168361.860583	36.585383
1510.206263	168657.843248	36.590400
1511.741672	168975.729552	36.595418
1513.197054	169276.843521	36.600436
1514.702299	169571.517742	36.605453
1516.357297	169893.210099	36.610471
1517.398301	170187.622644	36.615488
1518.943175	170513.195199	36.620506
1520.027903	170822.489395	36.625524
1522.266552	171127.191002	36.630541
1523.641316	171447.747818	36.635559
1525.547188	171744.514062	36.640576
1527.450799	172045.026102	36.645594
1528.862495	172352.436182	36.650612
1530.255352	172660.143261	36.655629
1531.589440	172960.070291	36.660647
1532.884800	173255.462510	36.665664
1534.283349	173555.331843	36.670682
1535.864676	173855.286965	36.675700
1537.890268	174131.083683	36.680717
1538.979201	174417.875046	36.685735
1540.785851	174696.541301	36.690752
1542.569303	174988.474837	36.695770
1543.896028	175270.764677	36.700788
1545.794885	175562.720593	36.705805
1547.081002	175846.657615	36.710823
1548.415094	176136.400822	36.715840
1549.740822	176427.708125	36.720858
1551.176544	176726.156740	36.725876
1552.874349	177036.671174	36.730893
1554.019152	177355.642828	36.735911
1555.072423	177667.664088	36.740928
1556.535600	177981.243840	36.745946
1558.037630	178302.307139	36.750964
1559.500976	178623.163127	36.755981
1560.961625	178957.487541	36.760999
1562.506028	179287.853094	36.766016
1564.014852	179620.231997	36.771034
1566.089054	179949.523999	36.776052
1568.080620	180280.760994	36.781069
1569.564579	180597.310579	36.786087
1571.403907	180909.919343	36.791104
1573.387627	181231.809504	36.796122
1574.664234	181563.020850	36.801140
1576.305613	181888.081411	36.806157
1577.802693	182212.380948	36.811175
1579.369859	182545.847611	36.816192
1581.453799	182854.594138	36.821210
1584.047418	183164.793772	36.826228
1586.449515	183448.232347	36.831245
1588.487997	183749.566228	36.836263
1590.515162	184027.167784	36.841280
1592.784940	184304.717841	36.846298
1594.587968	184593.948184	36.851316
1596.129112	184856.187008	36.856333
1597.575054	185131.377263	36.861351
1599.554845	185397.341213	36.866368
1600.891923	185662.587917	36.871386
1601.987923	185929.589458	36.876404
1603.678096	186200.682618	36.881421
1605.529018	186472.207406	36.886439
1607.613246	186706.756469	36.891456
1609.767502	186959.192935	36.896474
1612.568577	187186.288225	36.901492
1614.294004	187426.078774	36.906509
1615.510924	187664.850265	36.911527
1616.812635	187900.041722	36.916544
1617.918289	188140.826571	36.921562
1618.927443	188394.106585	36.926580
1620.513943	188644.410456	36.931597
1621.793997	188910.468773	36.936615
1622.632737	189180.231982	36.941632
1624.404789	189441.742821	36.946650
1625.365932	189721.262749	36.951668
1627.102666	189993.495839	36.956685
1628.613008	190276.494449	36.961703
1629.639344	190560.501331	36.966720
1631.152777	190853.835431	36.971738
1633.053434	191140.327884	36.976756
1634.238810	191436.093086	36.981773
1635.500689	191730.717222	36.986791
1636.702801	192045.689662	36.991808
1638.352388	192357.517405	36.996826
1639.510536	192678.035317	37.001844
1640.914624	192989.627668	37.006861
1642.047012	193303.767537	37.011879
1643.248565	193615.256951	37.016896
1644.727122	193936.248730	37.021914
1646.367996	194267.117490	37.026932
1647.533892	194591.312837	37.031949
1648.813786	194925.774151	37.036967
1650.467257	195270.648988	37.041984
1652.174840	195617.852670	37.047002
1652.995587	195980.934985	37.052020
1655.217454	196327.917571	37.057037
1656.853405	196698.244894	37.062055
1658.377809	197055.109915	37.067072
1660.072040	197426.180713	37.072090
1661.502128	197787.534232	37.077108
1663.005270	198154.933560	37.082125
1664.647074	198533.636756	37.087143
1666.101046	198920.041643	37.092160
1667.854677	199312.201194	37.097178
1669.525233	199701.748634	37.102196
1671.671667	200079.564179	37.107213
1673.426552	200470.714393	37.112231
1675.083961	200860.727571	37.117248
1678.167488	201234.737448	37.122266
1680.145858	201593.912431	37.127284
1682.514459	201956.300273	37.132301
1684.292345	202321.720797	37.137319
1686.041372	202684.278481	37.142336
1688.152918	203037.559983	37.147354
1689.451796	203394.761565	37.152372
1691.678318	203738.796740	37.157389
1692.707546	204113.707950	37.162407
1694.473794	204479.090343	37.167424
1696.186190	204843.442272	37.172442
1697.649678	205221.156574	37.177460
1699.190111	205572.119559	37.182477
1701.428337	205947.652079	37.187495
1704.391167	206265.902724	37.192512
1707.016841	206589.518082	37.197530
1709.074645	206929.024569	37.202548
1710.548343	207250.357582	37.207565
1712.374606	207581.677251	37.212583
1714.064788	207906.887893	37.217600
1715.401002	208241.605602	37.222618
1716.842976	208589.309657	37.227636
1718.220590	208915.566587	37.232653
1720.094278	209261.309978	37.237671
1720.963148	209615.157550	37.242688
1722.691061	209957.283711	37.247706
1724.187396	210319.893446	37.252724
1725.809552	210673.773016	37.257741
1727.563705	211039.746186	37.262759
1729.205655	211393.930219	37.267776
1730.852705	211761.244825	37.272794
1732.275635	212132.890146	37.277812
1733.786024	212495.455940	37.282829
1735.620437	212859.112374	37.287847
1737.229872	213233.855221	37.292864
1738.986384	213606.924452	37.297882
1740.683983	213983.103431	37.302900
1742.708053	214363.141019	37.307917
1744.665359	214754.645421	37.312935
1746.096217	215129.120881	37.317952
1747.486097	215503.655425	37.322970
1749.392195	215880.594863	37.327988
1751.331551	216239.294737	37.333005
1753.568921	216625.046000	37.338023
1755.068969	217009.066953	37.343040
1757.074613	217367.582232	37.348058
1758.477076	217741.996387	37.353076
1760.202340	218075.645182	37.358093
1762.122109	218451.042980	37.363111
1763.575559	218846.609553	37.368128
1766.008886	219185.249723	37.373146
1767.259801	219552.279335	37.378164
1768.757638	219900.804521	37.383181
1770.851341	220271.582967	37.388199
1772.005472	220636.194126	37.393216
1774.326516	220992.891873	37.398234
1776.061261	221350.627727	37.403252
1777.854851	221709.167769	37.408269
1779.876002	222081.335995	37.413287
1781.591860	222451.828913	37.418304
1783.183794	222823.918346	37.423322
1784.677832	223205.880178	37.428340
1786.294135	223580.355576	37.433357
1787.803923	223963.815872	37.438375
1789.784011	224353.676385	37.443392
1791.674820	224728.389346	37.448410
1793.515330	225120.586868	37.453428
1795.149276	225503.066339	37.458445
1796.875565	225901.686065	37.463463
1798.731058	226306.229265	37.468480
1800.404381	226693.912878	37.473498
1802.145283	227101.728823	37.478516
1804.074652	227503.799762	37.483533
1806.171004	227896.649339	37.488551
1807.288412	228314.580129	37.493568
1809.608643	228720.273048	37.498586
1811.194016	229138.459040	37.503604
1812.890766	229539.406198	37.508621
1814.968486	229964.955478	37.513639
1816.094176	230387.463300	37.518656
1818.157851	230805.219361	37.523674
1819.669295	231245.674977	37.528692
1821.329377	231672.263706	37.533709
1823.508344	232113.347884	37.538727
1825.039705	232548.469769	37.543744
1827.159798	232987.813516	37.548762
1829.282603	233414.025554	37.553780
1830.968801	233850.243008	37.558797
1832.647393	234282.373249	37.563815
1834.328113	234731.751880	37.568832
1836.677047	235158.718383	37.573850
1838.910696	235596.729353	37.578868
1840.548677	236019.700707	37.583885
1842.897109	236453.909912	37.588903
1844.879230	236878.172532	37.593920
1846.883215	237302.813520	37.598938
1849.299504	237706.735365	37.603956
1851.457141	238124.494186	37.608973
1853.578740	238540.938955	37.613991
1855.234431	238956.648918	37.619008
1856.993001	239352.960842	37.624026
1859.060116	239775.107207	37.629044
1860.096527	240188.991651	37.634061
1862.315217	240590.056031	37.639079
1864.067416	241024.500871	37.644096
1865.801919	241441.879068	37.649114
1867.409348	241860.854008	37.654132
1868.912834	242283.428644	37.659149
1870.792227	242699.768901	37.664167
1872.808973	243129.702842	37.669184
1874.771273	243555.836124	37.674202
1877.272099	243970.246445	37.679220
1879.377056	244388.126939	37.684237
1881.517125	244776.890740	37.689255
1883.320271	245189.030591	37.694272
1885.366579	245562.823348	37.699290
1887.253680	245933.086545	37.704308
1889.138516	246317.144279	37.709325
1891.006790	246690.358189	37.714343
1892.795868	247080.961200	37.719360
1894.649343	247470.055204	37.724378
1895.978268	247872.547678	37.729396
1897.063282	248274.141087	37.734413
1898.974251	248680.627843	37.739431
1900.384290	249100.077333	37.744448
1902.203343	249523.650967	37.749466
1903.855901	249948.776775	37.754484
1905.091218	250384.946237	37.759501
1906.951000	250809.098562	37.764519
1908.457430	251275.707598	37.769536
1910.247674	251726.113605	37.774554
1912.050789	252183.351278	37.779572
1914.070271	252658.107035	37.784589
1916.051532	253132.412202	37.789607
1917.795446	253600.888860	37.794624
1919.665323	254071.275568	37.799642
1921.930178	254539.031358	37.804660
1924.029932	255013.190944	37.809677
1926.461912	255479.141241	37.814695
1927.651269	255958.888348	37.819712
1929.676785	256446.829347	37.824730
1931.588844	256941.851391	37.829748
1932.996506	257432.105084	37.834765
1935.428563	257932.502863	37.839783
1936.685648	258429.615114	37.844800
1938.984789	258926.681747	37.849818
1941.246814	259430.460988	37.854836
1942.928701	259943.583102	37.859853
1945.089906	260442.476092	37.864871
1947.087173	260961.947393	37.869888
1949.294058	261450.264806	37.874906
1951.779287	261938.180299	37.879924
1953.717310	262442.139510	37.884941
1956.043074	262928.175770	37.889959
1957.793393	263432.343417	37.894976
1960.250096	263926.867535	37.899994
1962.233503	264414.128232	37.905012
1964.644019	264907.008149	37.910029
1967.022643	265379.799084	37.915047
1968.853855	265879.150416	37.920064
1971.137856	266358.103805	37.925082
1973.237547	266823.064794	37.930100
1975.114856	267305.920554	37.935117
1977.287501	267786.491427	37.940135
1979.313626	268256.848647	37.945152
1980.994166	268742.021739	37.950170
1982.941804	269211.450978	37.955188
1984.442448	269707.855399	37.960205
1986.888965	270181.824122	37.965223
1988.525750	270673.632152	37.970240
1990.408158	271160.216607	37.975258
1992.693387	271637.715621	37.980276
1994.391321	272127.860162	37.985293
1996.336410	272622.179817	37.990311
1998.390871	273106.522681	37.995328
1999.895812	273611.938310	38.000346
2001.918494	274101.085805	38.005364
2003.531193	274610.698537	38.010381
2005.223661	275115.064136	38.015399
2007.257054	275623.055584	38.020416
2009.054935	276137.689593	38.025434
2010.992190	276645.085130	38.030452
2012.500802	277154.684336	38.035469
2014.477845	277652.240342	38.040487
2016.138772	278144.309905	38.045504
2018.135607	278650.624032	38.050522
2021.115698	279131.702248	38.055540
2023.417087	279629.225187	38.060557
2025.220133	280120.453545	38.065575
2027.778251	280607.465863	38.070592
2030.137387	281098.142323	38.075610
2032.432099	281569.268849	38.080628
2034.547309	282056.020454	38.085645
2037.195242	282534.833383	38.090663
2039.699361	283010.163398	38.095680
2041.143587	283497.352284	38.100698
2043.668260	283960.940739	38.105716
2046.051217	284430.368226	38.110733
2048.299256	284904.287280	38.115751
2050.287312	285373.726568	38.120768
2051.884825	285845.540603	38.125786
2054.110623	286312.524511	38.130804
2056.040983	286796.193440	38.135821
2058.045724	287274.107868	38.140839
2059.757886	287751.357945	38.145856
2062.342110	288229.528772	38.150874
2064.690275	288701.107519	38.155892
2066.452782	289192.314561	38.160909
2068.107190	289675.511210	38.165927
2070.313739	290162.272261	38.170944
2071.860741	290662.120203	38.175962
2073.967367	291159.460489	38.180980
2076.005453	291681.397287	38.185997
2078.076304	292170.128902	38.191015
2080.207117	292677.314219	38.196032
2082.012530	293191.840983	38.201050
2084.229918	293700.302992	38.206068
2086.169954	294222.194200	38.211085
2088.079895	294739.414561	38.216103
2090.548770	295261.569010	38.221120
2092.005562	295787.088938	38.226138
2094.424590	296294.743939	38.231156
2096.004428	296837.738284	38.236173
2098.376530	297358.044644	38.241191
2100.251993	297903.372056	38.246208
2102.212495	298445.482332	38.251226
2103.898924	298990.022582	38.256244
2106.233013	299550.682025	38.261261
2108.090567	300100.292946	38.266279
2110.894504	300644.994657	38.271296
2112.937160	301200.816613	38.276314
2115.446710	301734.614548	38.281332
2117.501593	302292.205955	38.286349
2119.400604	302841.108609	38.291367
2121.389349	303385.269284	38.296384
2123.207901	303952.286756	38.301402
2126.055360	304494.419184	38.306420
2127.966109	305046.963699	38.311437
2130.329268	305603.848801	38.316455
2132.260876	306146.529099	38.321472
2135.159884	306688.944162	38.326490
2137.347566	307228.984776	38.331508
2139.624221	307777.743349	38.336525
2141.515093	308324.581338	38.341543
2143.797517	308869.547763	38.346560
2146.409547	309394.799981	38.351578
2149.646541	309912.936203	38.356596
2151.720429	310434.664624	38.361613
2154.247848	310951.387886	38.366631
2156.009109	311461.581228	38.371648
2157.861900	311956.417781	38.376666
2159.779445	312449.081899	38.381684
2161.928800	312927.229760	38.386701
2163.820123	313434.823562	38.391719
2165.721651	313923.036738	38.396736
2167.357259	314438.893626	38.401754
2169.997242	314935.205323	38.406772
2171.608206	315456.645655	38.411789
2173.136907	315960.549197	38.416807
2174.978689	316496.900266	38.421824
2176.367295	317044.495113	38.426842
2178.892058	317587.403033	38.431860
2180.753865	318136.358299	38.436877
2183.064310	318692.522413	38.441895
2185.119424	319252.507661	38.446912
2186.768405	319817.151414	38.451930
2188.960577	320387.337342	38.456948
2191.107587	320976.061446	38.461965
2193.151656	321564.441836	38.466983
2195.098105	322150.954144	38.472000
2196.894021	322764.044546	38.477018
2199.461280	323362.808129	38.482036
2201.100984	323967.483188	38.487053
2203.365460	324593.655658	38.492071
2205.381259	325206.888922	38.497088
2207.256078	325836.337774	38.502106
2209.284163	326474.285438	38.507124
2211.383251	327118.333274	38.512141
2213.222999	327784.403518	38.517159
2215.707706	328435.812017	38.522176
2217.961536	329087.378438	38.527194
2221.135337	329722.435562	38.532212
2223.927490	330366.916792	38.537229
2226.389288	331022.285701	38.542247
2228.646479	331667.653116	38.547264
2230.727926	332309.386536	38.552282
2233.107137	332954.845755	38.557300
2235.511139	333595.622288	38.562317
2237.359400	334258.365663	38.567335
2240.133211	334909.143497	38.572352
2242.615527	335550.036180	38.577370
2244.836114	336196.549084	38.582388
2247.175333	336841.942878	38.587405
2249.014333	337497.869735	38.592423
2251.380100	338138.800833	38.597440
2253.734966	338806.657475	38.602458
2255.905958	339458.747570	38.607476
2257.986524	340123.078676	38.612493
2259.717019	340781.468707	38.617511
2261.930340	341449.288318	38.622528
2264.246057	342125.813216	38.627546
2266.356541	342806.702941	38.632564
2268.786411	343490.677454	38.637581
2270.454502	344168.169432	38.642599
2273.329318	344844.309861	38.647616
2276.048368	345524.501820	38.652634
2278.608361	346183.721421	38.657652
2281.085840	346853.300050	38.662669
2283.472100	347521.843560	38.667687
2285.614415	348194.427514	38.672704
2287.633486	348878.416675	38.677722
2289.811088	349551.329969	38.682740
2292.034566	350235.569207	38.687757
2294.718950	350902.135450	38.692775
2297.444231	351557.595347	38.697792
2299.677201	352228.048122	38.702810
2302.174130	352897.609478	38.707828
2305.075812	353533.953281	38.712845
2307.449256	354176.135240	38.717863
2310.179103	354789.549876	38.722880
2312.197907	355400.434454	38.727898
2314.151105	356028.118527	38.732916
2316.154477	356641.854852	38.737933
2318.440162	357279.893542	38.742951
2320.746426	357904.116232	38.747968
2323.060749	358529.774323	38.752986
2324.553296	359160.278066	38.758004
2326.965583	359805.994861	38.763021
2329.007693	360462.266235	38.768039
2331.112392	361114.584034	38.773056
2333.325233	361772.708392	38.778074
2335.319090	362439.153985	38.783092
2337.527522	363121.941369	38.788109
2339.885039	363804.971178	38.793127
2342.313517	364483.918240	38.798144
2344.741806	365172.518587	38.803162
2347.107815	365852.821650	38.808180
2349.839205	366539.901166	38.813197
2352.196606	367228.526735	38.818215
2354.832903	367903.877699	38.823232
2357.113603	368609.917116	38.828250
2359.298891	369291.024836	38.833268
2362.307746	369983.093378	38.838285
2364.455448	370687.948187	38.843303
2366.784610	371381.320216	38.848320
2368.930695	372087.441633	38.853338
2371.258919	372799.504632	38.858356
2373.604327	373499.833193	38.863373
2375.712538	374208.658036	38.868391
2378.018806	374928.442629	38.873408
2380.084421	375655.961941	38.878426
2382.416410	376375.889962	38.883444
2385.154869	377098.956383	38.888461
2387.525304	377827.596820	38.893479
2389.953587	378561.537447	38.898496
2392.598747	379299.813247	38.903514
2394.966290	380027.696921	38.908532
2397.637517	380766.595509	38.913549
2400.058589	381501.867813	38.918567
2402.574646	382232.467959	38.923584
2404.960065	382965.254078	38.928602
2407.499302	383695.665699	38.933620
2410.242567	384421.438054	38.938637
2412.987788	385144.328853	38.943655
2415.766857	385874.119166	38.948672
2418.212565	386587.773177	38.953690
2420.467423	387316.324298	38.958708
2423.139499	388036.727867	38.963725
2425.449570	388769.799490	38.968743
2428.148107	389489.430130	38.973760
2431.014370	390203.464806	38.978778
2433.310119	390921.861402	38.983796
2435.900615	391638.215254	38.988813
2438.653911	392348.188446	38.993831
2441.470752	393054.231088	38.998848
2443.650508	393765.888261	39.003866
2445.633337	394470.515039	39.008884
2448.264484	395177.755208	39.013901
2450.624652	395889.002562	39.018919
2453.526575	396605.237326	39.023936
2455.742788	397305.018883	39.028954
2457.559564	398017.394598	39.033972
2459.858718	398746.703071	39.038989
2462.099170	399463.509508	39.044007
2464.255326	400182.466085	39.049024
2466.930507	400894.122082	39.054042
2469.341924	401591.360359	39.059060
2472.001112	402276.884520	39.064077
2474.572642	402975.329224	39.069095
2477.111716	403657.773763	39.074112
2479.760742	404336.737609	39.079130
2482.153849	405035.667233	39.084148
2484.391359	405724.951991	39.089165
2486.662378	406427.641752	39.094183
2488.685336	407131.722687	39.099200
2491.507389	407822.834189	39.104218
2493.584471	408532.620861	39.109236
2496.243481	409254.097678	39.114253
2498.037010	409970.505378	39.119271
2500.670932	410696.608759	39.124288
2503.110123	411428.297382	39.129306
2505.474100	412166.488117	39.134324
2508.151494	412900.300393	39.139341
2510.668613	413650.151718	39.144359
2513.053802	414390.252197	39.149376
2515.538984	415138.267823	39.154394
2517.827093	415899.109642	39.159412
2520.478153	416660.881983	39.164429
2522.654198	417441.678670	39.169447
2524.837152	418201.861887	39.174464
2527.480295	418992.359517	39.179482
2530.278746	419780.198528	39.184500
2532.799725	420566.134365	39.189517
2535.597904	421343.213308	39.194535
2537.730851	422131.063235	39.199552
2540.676148	422921.867971	39.204570
2543.104103	423721.088111	39.209588
2545.788726	424518.771349	39.214605
2548.283212	425318.890449	39.219623
2550.473749	426124.603069	39.224640
2553.641644	426925.367866	39.229658
2556.078636	427745.921553	39.234676
2558.312417	428557.266703	39.239693
2561.028092	429369.922013	39.244711
2563.522124	430191.900902	39.249728
2566.392650	431010.498479	39.254746
2568.662439	431839.645296	39.259764
2571.582088	432652.508014	39.264781
2574.109675	433486.969792	39.269799
2576.602073	434305.969937	39.274816
2579.400229	435127.876547	39.279834
2582.742450	435950.827733	39.284852
2586.217578	436723.523056	39.289869
2589.491653	437532.662713	39.294887
2592.396697	438332.674921	39.299904
2594.890534	439111.928633	39.304922
2597.189471	439923.421017	39.309940
2599.901962	440695.094348	39.314957
2602.257012	441495.590563	39.319975
2604.890961	442292.925293	39.324992
2607.411739	443075.628029	39.330010
2609.956367	443879.143197	39.335028
2612.933551	444661.258390	39.340045
2615.266210	445466.217294	39.345063
2617.833207	446250.164338	39.350080
2620.559990	447040.025539	39.355098
2622.830861	447844.652984	39.360116
2625.985011	448639.746358	39.365133
2629.291958	449417.840492	39.370151
2631.850435	450200.025595	39.375168
2634.862853	450964.152059	39.380186
2637.520344	451743.633513	39.385204
2640.210260	452509.881180	39.390221
2643.828233	453237.159424	39.395239
2647.404498	453943.483558	39.400256
2650.387100	454636.582633	39.405274
2653.011572	455335.734980	39.410292
2655.497881	456018.352021	39.415309
2657.882107	456711.126199	39.420327
2660.076659	457419.683098	39.425344
2662.154443	458113.623175	39.430362
2664.056525	458813.180381	39.435380
2666.501679	459551.652043	39.440397
2668.842972	460279.295382	39.445415
2670.972959	461014.631077	39.450432
2673.422999	461756.913109	39.455450
2675.165896	462523.648393	39.460468
2677.687134	463296.290683	39.465485
2679.864960	464082.404145	39.470503
2682.080473	464878.588244	39.475520
2684.788279	465676.124152	39.480538
2687.381810	466483.955978	39.485556
2689.748692	467289.467091	39.490573
2691.940285	468130.094188	39.495591
2694.520366	468968.245382	39.500608
2697.346440	469817.839793	39.505626
2699.724532	470674.897935	39.510644
2702.437992	471549.040168	39.515661
2705.025444	472409.572592	39.520679
2707.978315	473285.464251	39.525696
2710.436592	474168.065172	39.530714
2712.969122	475058.542981	39.535732
2715.337974	475947.388937	39.540749
2718.150501	476836.826049	39.545767
2720.675365	477762.986739	39.550784
2723.393443	478675.382072	39.555802
2725.859439	479606.408981	39.560820
2728.424113	480523.888663	39.565837
2731.391777	481457.616363	39.570855
2733.930940	482383.590620	39.575872
2737.223934	483335.900720	39.580890
2739.609110	484288.916314	39.585908
2742.561955	485230.882062	39.590925
2745.433341	486173.114274	39.595943
2748.544247	487132.521194	39.600960
2752.135567	488056.663531	39.605978
2755.310886	488993.798260	39.610996
2757.947165	489918.656532	39.616013
2761.555940	490854.509148	39.621031
2764.594537	491769.461544	39.626048
2768.078813	492682.374038	39.631066
2771.124155	493595.108822	39.636084
2773.902891	494502.490356	39.641101
2776.769464	495400.474571	39.646119
2779.284528	496317.742961	39.651136
2782.556508	497203.304262	39.656154
2784.989167	498118.419981	39.661172
2787.779280	499024.901316	39.666189
2790.818356	499923.473622	39.671207
2793.274110	500838.386262	39.676224
2796.000933	501732.171075	39.681242
2798.567191	502643.334219	39.686260
2800.813078	503550.364515	39.691277
2803.395802	504483.613088	39.696295
2805.636059	505412.124936	39.701312
2808.365178	506341.763540	39.706330
2811.391094	507263.585372	39.711348
2814.270562	508200.050405	39.716365
2817.266982	509139.668133	39.721383
2820.097986	510075.930950	39.726400
2823.036273	511005.013447	39.731418
2825.566033	511915.660640	39.736436
2828.133022	512819.142489	39.741453
2831.252831	513721.725171	39.746471
2833.408196	514618.317514	39.751488
2836.362280	515522.940742	39.756506
2839.114115	516435.355708	39.761524
2841.566699	517345.599953	39.766541
2844.551783	518265.679010	39.771559
2847.158459	519198.361492	39.776576
2849.749580	520123.533839	39.781594
2852.286650	521055.057103	39.786612
2854.555230	522000.722887	39.791629
2857.464304	522957.053540	39.796647
2859.929403	523927.097116	39.801664
2862.454579	524902.104816	39.806682
2865.149796	525885.884627	39.811700
2867.892984	526884.547967	39.816717
2870.840863	527871.478934	39.821735
2873.486019	528886.741695	39.826752
2876.878239	529881.672554	39.831770
2879.678974	530910.062185	39.836788
2882.642616	531929.996498	39.841805
2885.635021	532938.428640	39.846823
2888.376079	533979.448307	39.851840
2891.381509	534994.480424	39.856858
2894.838074	536022.954652	39.861876
2897.586153	537060.128078	39.866893
2900.760882	538088.601879	39.871911
2903.708971	539122.271951	39.876928
2906.814705	540171.739268	39.881946
2909.856554	541200.412896	39.886964
2913.024777	542233.669023	39.891981
2916.373813	543259.173824	39.896999
2919.428120	544299.338957	39.902016
2922.543579	545327.648093	39.907034
2925.687624	546352.859224	39.912052
2928.365339	547398.437221	39.917069
2931.922073	548406.632771	39.922087
2934.941054	549451.345056	39.927104
2938.849595	550448.623449	39.932122
2942.618993	551448.717479	39.937140
2946.067084	552444.267203	39.942157
2949.626243	553419.268484	39.947175
2952.310032	554406.205453	39.952192
2955.510617	555370.671144	39.957210
2958.913988	556358.954011	39.962228
2962.011126	557322.542596	39.967245
2965.116911	558273.297953	39.972263
2968.566053	559229.455047	39.977280
2971.661111	560179.472702	39.982298
2974.600786	561117.190607	39.987316
2977.450144	562065.656177	39.992333
2980.671360	563007.060374	39.997351
2983.334734	563966.117366	40.002368
2986.174372	564908.803537	40.007386
2989.029086	565863.822101	40.012404
2991.419013	566818.395186	40.017421
2994.068915	567787.314667	40.022439
2996.488248	568748.969849	40.027456
2999.388169	569725.985446	40.032474
3002.148581	570705.258466	40.037492
3005.223451	571672.257475	40.042509
3008.240411	572637.435769	40.047527
3011.765040	573628.201539	40.052544
3015.131976	574606.721466	40.057562
3018.456977	575572.226347	40.062580
3020.942774	576546.124423	40.067597
3024.043063	577511.968286	40.072615
3026.805593	578486.371414	40.077632
3029.440385	579437.193221	40.082650
3032.229772	580372.216883	40.087668
3034.840537	581320.941462	40.092685
3038.454940	582238.784903	40.097703
3041.602578	583194.748259	40.102720
3044.397876	584132.894406	40.107738
3046.927604	585082.092899	40.112756
3049.475400	586044.449816	40.117773
3052.362143	587019.457538	40.122791
3055.157118	587998.411787	40.127808
3057.596578	588996.792730	40.132826
3060.459809	589995.672003	40.137844
3063.137093	591011.838041	40.142861
3065.961616	592025.187116	40.147879
3068.673184	593069.533810	40.152896
3071.359111	594107.479855	40.157914
3074.078928	595151.691234	40.162932
3076.932132	596233.106410	40.167949
3080.237579	597301.073823	40.172967
3083.315194	598389.164590	40.177984
3086.392145	599481.460434	40.183002
3089.623269	600565.365795	40.188020
3092.534047	601667.497517	40.193037
3095.670662	602773.091026	40.198055
3099.358139	603871.779047	40.203072
3102.754622	604975.264895	40.208090
3106.215518	606081.085681	40.213108
3108.618540	607194.680588	40.218125
3111.739284	608310.599316	40.223143
3115.130585	609441.273203	40.228160
3118.057619	610576.863066	40.233178
3121.459221	611702.254523	40.238196
3124.309344	612846.330938	40.243213
3127.866155	613979.669941	40.248231
3130.295381	615129.632518	40.253248
3133.730527	616270.358472	40.258266
3136.971382	617421.098098	40.263284
3140.092893	618591.184162	40.268301
3143.251638	619750.491498	40.273319
3146.056124	620913.732709	40.278336
3149.000259	622088.870755	40.283354
3152.534369	623257.936998	40.288372
3155.059337	624463.568660	40.293389
3158.043790	625649.154819	40.298407
3160.968900	626840.863948	40.303424
3163.771753	628053.039392	40.308442
3166.942318	629260.371146	40.313460
3169.923922	630497.209777	40.318477
3173.132307	631714.792044	40.323495
3176.245250	632952.219700	40.328512
3179.370731	634186.703725	40.333530
3182.637725	635409.188791	40.338548
3185.810914	636650.660788	40.343565
3189.867385	637885.849888	40.348583
3193.574946	639120.998962	40.353600
3197.009743	640340.229706	40.358618
3200.334883	641560.181809	40.363636
3203.426941	642791.548948	40.368653
3206.963483	644010.225702	40.373671
3210.462740	645222.429349	40.378688
3213.695829	646439.567795	40.383706
3217.429779	647634.440802	40.388724
3220.550365	648844.028490	40.393741
3223.970189	650043.751216	40.398759
3227.752079	651230.511736	40.403776
3230.983114	652433.516556	40.408794
3234.831441	653601.246542	40.413812
3238.049782	654774.622167	40.418829
3241.157234	655912.459239	40.423847
3244.654219	657038.046731	40.428864
3247.263949	658172.466507	40.433882
3250.192127	659288.127937	40.438900
3252.968524	660425.295663	40.443917
3256.422066	661558.285256	40.448935
3259.672352	662699.687935	40.453952
3262.291141	663850.467002	40.458970
3265.455072	664998.629456	40.463988
3268.447357	666164.546881	40.469005
3271.574187	667330.100811	40.474023
3274.681185	668517.354999	40.479040
3277.104108	669698.206847	40.484058
3280.504859	670905.308765	40.489076
3283.194667	672112.522977	40.494093
3286.178332	673331.516948	40.499111
3289.942565	674555.841367	40.504128
3292.899112	675794.355933	40.509146
3296.416404	677033.806011	40.514164
3299.711749	678271.189125	40.519181
3302.931853	679522.779621	40.524199
3306.394073	680779.029209	40.529216
3309.267001	682047.176532	40.534234
3312.655596	683309.450462	40.539252
3315.880751	684600.430852	40.544269
3318.987429	685889.410470	40.549287
3322.475906	687166.426816	40.554304
3325.459919	688475.166234	40.559322
3328.440707	689783.368681	40.564340
3331.896635	691092.840463	40.569357
3335.009049	692428.426094	40.574375
3338.437603	693755.226249	40.579392
3341.639887	695095.209370	40.584410
3345.240306	696421.681619	40.589428
3348.477433	697776.528555	40.594445
3351.841464	699121.874111	40.599463
3355.442485	700485.960969	40.604480
3358.573903	701858.437907	40.609498
3362.062665	703194.610422	40.614516
3364.829747	704569.742612	40.619533
3368.049679	705958.255177	40.624551
3372.037815	707339.878491	40.629568
3374.871693	708722.262753	40.634586
3378.194616	710115.336141	40.639604
3382.654458	711492.299200	40.644621
3386.625786	712866.842785	40.649639
3390.528641	714236.868601	40.654656
3394.699143	715607.320665	40.659674
3398.468774	716953.865966	40.664692
3402.574368	718297.319686	40.669709
3406.329606	719627.903390	40.674727
3410.328519	720950.964413	40.679744
3413.843347	722269.296045	40.684762
3417.727512	723575.688982	40.689780
3421.442633	724879.431432	40.694797
3424.983037	726187.147701	40.699815
3428.449931	727480.979352	40.704832
3431.334987	728780.285480	40.709850
3434.851385	730077.551104	40.714868
3437.766265	731373.918682	40.719885
3440.820684	732678.204106	40.724903
3443.848130	733997.738052	40.729920
3446.805816	735316.227914	40.734938
3450.185365	736640.354567	40.739956
3453.570616	737966.728609	40.744973
3456.380504	739295.789623	40.749991
3460.038276	740634.996657	40.755008
3463.022970	741967.308002	40.760013
3466.201738	743239.750847	40.765018
3469.635402	744471.703996	40.770023
3472.618000	745646.694091	40.775028
3475.967878	746749.092212	40.780032
3478.313537	747811.028808	40.785037
3481.046249	748795.875081	40.790042
3483.752374	749717.857921	40.795047
3486.577933	750587.349050	40.800052
3489.355362	751372.386650	40.805056
3491.481968	752109.940056	40.810061
3493.514954	752771.485218	40.815066
3495.818263	753373.721563	40.820071
3497.963008	753934.312096	40.825076
3499.949087	754427.591478	40.830080
3501.812623	754868.081811	40.835085
3503.701298	755248.954892	40.840090
3504.890761	755588.555554	40.845095
3506.012843	755886.834244	40.850100
3507.388662	756129.032569	40.855104
3508.695659	756345.813403	40.860109
3509.766111	756513.908505	40.865114
3510.681313	756648.016845	40.870119
3511.527792	756769.942555	40.875124
3512.757196	756835.435928	40.880128
3513.686179	756878.767252	40.885133
3514.717466	756883.088616	40.890138
3515.141925	756872.061163	40.895143
3515.888065	756826.824550	40.900148
3516.704816	756761.190806	40.905152
3516.970008	756680.099445	40.910157
3517.505806	756580.106983	40.915162
3518.242364	756452.684795	40.920167
3518.479721	756315.421270	40.925172
3518.619111	756143.617528	40.930176
3518.761645	755984.693398	40.935181
3519.362567	755802.044375	40.940186
3519.658230	755609.765646	40.945191
3519.648346	755409.929971	40.950196
3519.827821	755186.212570	40.955200
3520.654823	754968.157979	40.960205
3520.735622	754738.420617	40.965210
3520.742923	754484.446131	40.970215
3520.652019	754237.786995	40.975220
3521.164934	753975.120820	40.980224
3520.811660	753718.217961	40.985229
3521.192186	753446.371189	40.990234
3521.236555	753166.619858	40.995239
3521.051520	752886.797501	41.000244
3521.408935	752606.183935	41.005248
3521.094231	752323.843888	41.010253
3520.997327	752029.752246	41.015258
3521.235957	751738.952548	41.020263
3521.030173	751440.905168	41.025268
3521.137438	751140.028436	41.030272
3520.948714	750849.463467	41.035277
3520.741368	750547.578346	41.040282
3520.812895	750247.265591	41.045287
3520.658070	749939.321193	41.050292
3521.033436	749631.178137	41.055296
3520.708901	749332.377541	41.060301
3520.375324	749019.831377	41.065306
3520.598521	748730.848231	41.070311
3520.263993	748422.033372	41.075316
3520.485647	748109.902412	41.080320
3520.589206	747806.475723	41.085325
3520.599688	747503.250275	41.090330
3520.586801	747182.176230	41.095335
3520.421439	746879.746329	41.100340
3520.193559	746562.586675	41.105344
3520.059087	746246.683790	41.110349
3519.903910	745940.261757	41.115354
3519.805593	745641.133962	41.120359
3519.346394	745339.236766	41.125364
3519.397045	745024.489766	41.130368
3519.439011	744729.110384	41.135373
3519.343379	744435.720127	41.140378
3519.291943	744123.722380	41.145383
3518.714437	743826.285516	41.150388
3519.201638	743516.300634	41.155392
3519.193928	743228.882897	41.160397
3518.929940	742926.910169	41.165402
3519.063514	742625.057967	41.170407
3518.790594	742330.085598	41.175412
3518.430107	742030.567034	41.180416
3518.318647	741739.601035	41.185421
3518.085518	741443.154784	41.190426
3517.967668	741152.069307	41.195431
3517.973458	740870.993055	41.200436
3517.962424	740586.002139	41.205440
3517.623196	740291.855009	41.210445
3517.630345	740008.719951	41.215450
3517.674063	739719.187503	41.220455
3517.151434	739447.101644	41.225460
3517.450553	739160.375813	41.230464
3517.174092	738891.693199	41.235469
3517.113494	738611.883681	41.240474
3516.947712	738341.482089	41.245479
3516.504250	738063.151358	41.250484
3516.601776	737799.911569	41.255488
3516.510977	737529.272123	41.260493
3516.619838	737260.619282	41.265498
3516.328955	736991.578114	41.270503
3515.960818	736734.714118	41.275508
3515.994812	736467.432589	41.280512
3515.867012	736207.443737	41.285517
3515.670738	735944.042919	41.290522
3515.679789	735694.952206	41.295527
3515.451271	735442.180999	41.300532
3515.415894	735177.095108	41.305536
3515.509191	734938.558959	41.310541
3515.564172	734690.122426	41.315546
3515.638239	734435.636091	41.320551
3515.143423	734186.779865	41.325556
3515.209751	733930.298772	41.330560
3515.144732	733684.969712	41.335565
3514.776092	733434.435731	41.340570
3514.971245	733184.345374	41.345575
3514.574998	732955.386293	41.350580
3514.622524	732715.306581	41.355584
3514.492429	732470.892046	41.360589
3514.271732	732241.240049	41.365594
3514.281002	732006.195940	41.370599
3514.156713	731765.076590	41.375604
3514.164508	731534.227890	41.380608
3513.821509	731311.502171	41.385613
3513.740231	731080.358143	41.390618
3513.787673	730851.513775	41.395623
3513.535817	730626.278078	41.400628
3513.609323	730398.456613	41.405632
3513.321531	730183.565185	41.410637
3513.413616	729958.303647	41.415642
3513.341709	729746.287084	41.420647
3512.910585	729524.121219	41.425652
3513.242898	729307.321082	41.430656
3513.080561	729096.738943	41.435661
3512.381641	728880.444589	41.440666
3513.069807	728666.144340	41.445671
3512.706988	728456.470419	41.450676
3512.477750	728247.611171	41.455680
3512.724845	728055.709209	41.460685
3512.457559	727829.358352	41.465690
3512.479324	727633.867290	41.470695
3512.136460	727430.554552	41.475700
3512.113225	727227.778462	41.480704
3512.036037	727035.856610	41.485709
3511.897223	726833.089843	41.490714
3512.013289	726635.527955	41.495719
3511.587323	726442.807540	41.500724
3511.512143	726237.389444	41.505728
3511.401676	726057.342107	41.510733
3511.557089	725865.503064	41.515738
3511.657887	725674.411863	41.520743
3511.375068	725496.759266	41.525748
3511.261222	725307.132067	41.530752
3510.979672	725110.243398	41.535757
3510.841665	724940.236103	41.540762
3510.848665	724751.765510	41.545767
3510.541575	724579.201645	41.550772
3510.717069	724398.426438	41.555776
3510.785814	724229.113705	41.560781
3510.568799	724048.792191	41.565786
3510.738288	723868.948063	41.570791
3510.369368	723704.801986	41.575796
3510.417102	723526.160070	41.580800
3510.467640	723363.524002	41.585805
3510.464387	723188.303331	41.590810
3510.393525	723024.044896	41.595815
3510.090243	722854.864597	41.600820
3510.453063	722673.177966	41.605824
3510.278262	722509.917921	41.610829
3510.184121	722345.649861	41.615834
3510.211084	722184.432126	41.620839
3509.900608	722027.133875	41.625844
3509.748238	721844.919316	41.630848
3509.874803	721680.452866	41.635853
3509.686490	721536.362197	41.640858
3509.697147	721375.676788	41.645863
3509.330336	721212.918711	41.650868
3509.204990	721068.164967	41.655872
3509.359373	720906.306365	41.660877
3509.027073	720754.639910	41.665882
3509.117540	720610.239185	41.670887
3508.759392	720470.620606	41.675892
3508.772493	720316.360272	41.680896
3509.027309	720175.147878	41.685901
3508.674387	720025.653324	41.690906
3509.128987	719882.617823	41.695911
3508.662574	719742.062744	41.700916
3508.793194	719592.034199	41.705920
3508.571229	719448.954298	41.710925
3508.532373	719311.346312	41.715930
3508.318464	719176.641325	41.720935
3508.223607	719047.766444	41.725940
3508.729377	718907.234999	41.730944
3508.212024	718770.689048	41.735949
3508.098800	718629.461714	41.740954
3508.324239	718495.516252	41.745959
3507.899364	718375.662429	41.750964
3507.890358	718247.058589	41.755968
3508.245420	718115.664696	41.760973
3507.924109	717984.926110	41.765978
3507.827385	717840.260380	41.770983
3507.920390	717731.868535	41.775988
3507.889219	717594.379812	41.780992
3507.530431	717488.737962	41.785997
3507.383932	717355.133332	41.791002
3507.791167	717227.337894	41.796007
3507.359367	717108.508743	41.801012
3507.233846	716985.262048	41.806016
3507.534794	716868.887870	41.811021
3507.142369	716762.597551	41.816026
3507.649238	716625.946556	41.821031
3507.417846	716516.104394	41.826036
3507.612092	716403.610813	41.831040
3507.424058	716276.097708	41.836045
3506.970685	716149.122618	41.841050
3507.114213	716046.505021	41.846055
3507.061264	715933.847564	41.851060
3507.211536	715814.804686	41.856064
3507.060336	715708.907677	41.861069
3506.881587	715603.261954	41.866074
3506.906775	715489.494145	41.871079
3506.693458	715373.829246	41.876084
3506.765230	715264.615239	41.881088
3506.857346	715158.224556	41.886093
3506.827353	715062.073694	41.891098
3506.932184	714948.831204	41.896103
3506.530986	714849.960712	41.901108
3506.698922	714731.594258	41.906112
3506.826226	714631.343786	41.911117
3506.448046	714531.572616	41.916122
3506.657512	714424.111272	41.921127
3506.513448	714325.043273	41.926132
3506.638899	714224.986765	41.931136
3506.518767	714125.267390	41.936141
3506.348473	714013.347988	41.941146
3506.491035	713904.352792	41.946151
3506.292799	713810.597393	41.951156
3506.348458	713704.889154	41.956160
3506.509394	713608.888689	41.961165
3505.943067	713503.776977	41.966170
3506.278201	713396.033672	41.971175
3506.102083	713308.621201	41.976180
3506.085042	713224.208796	41.981184
3505.693808	713120.701084	41.986189
3505.579029	713029.206110	41.991194
3506.220253	712944.433991	41.996199
3505.826519	712866.929054	42.001204
3505.900120	712769.643148	42.006208
3506.266013	712681.936117	42.011213
3505.579320	712586.064141	42.016218
3505.826704	712490.731553	42.021223
3505.584318	712402.129525	42.026228
3505.705110	712310.438969	42.031232
3505.613912	712219.477318	42.036237
3505.578691	712140.070062	42.041242
3505.680039	712051.705371	42.046247
3505.358103	711970.606721	42.051252
3505.839077	711880.688478	42.056256
3505.321461	711790.636501	42.061261
3505.289601	711712.018857	42.066266
3505.232251	711629.880507	42.071271
3505.141144	711549.236052	42.076276
3505.255395	711470.393479	42.081280
3504.906182	711387.506823	42.086285
3505.037798	711314.368294	42.091290
3505.156726	711237.260130	42.096295
3505.141205	711168.512878	42.101300
3504.997397	711090.950417	42.106304
3505.413414	711024.314828	42.111309
3504.952852	710932.755130	42.116314
3505.089154	710860.356536	42.121319
3504.685364	710782.089612	42.126324
3504.844668	710709.139876	42.131328
3504.603137	710635.908262	42.136333
3504.798763	710570.645892	42.141338
3504.902854	710487.923774	42.146343
3504.609983	710426.166406	42.151348
3504.654766	710356.211187	42.156352
3504.714641	710294.096704	42.161357
3504.798864	710227.757947	42.166362
3504.846991	710142.609139	42.171367
3505.098038	710075.695535	42.176372
3504.846136	710005.438953	42.181376
3504.739460	709932.377594	42.186381
3504.555156	709864.888881	42.191386
3504.645474	709780.821722	42.196391
3504.336414	709732.814294	42.201396
3504.276091	709670.864082	42.206400
3504.869859	709600.811949	42.211405
3504.372081	709534.613639	42.216410
3504.557364	709461.500002	42.221415
3504.479495	709403.919878	42.226420
3504.540946	709337.131123	42.231424
3504.309093	709261.651871	42.236429
3504.276791	709196.118766	42.241434
3504.190776	709138.140992	42.246439
3503.993174	709082.961742	42.251444
3503.998117	709020.449867	42.256448
3504.352491	708960.312738	42.261453
3503.898400	708911.877795	42.266458
3504.187117	708840.479589	42.271463
3503.989284	708793.491208	42.276468
3503.863542	708730.700896	42.281472
3503.961437	708684.805073	42.286477
3503.660520	708621.198796	42.291482
3503.725393	708562.943919	42.296487
3503.799364	708516.058059	42.301492
3503.912085	708461.419372	42.306496
3503.919546	708414.692914	42.311501
3503.838077	708362.568449	42.316506
3503.653727	708302.664704	42.321511
3503.711427	708253.644895	42.326516
3503.639241	708196.601928	42.331520
3503.579384	708152.566615	42.336525
3503.216256	708105.800404	42.341530
3503.933445	708058.458143	42.346535
3503.772687	708009.522700	42.351540
3503.484075	707961.899211	42.356544
3503.736076	707899.090036	42.361549
3503.615984	707866.285952	42.366554
3503.742561	707799.474447	42.371559
3503.889868	707751.231501	42.376564
3503.640296	707698.683850	42.381568
3503.587556	707654.644806	42.386573
3503.433296	707605.010747	42.391578
3503.622776	707553.631147	42.396583
3503.406169	707497.848905	42.401588
3503.513772	707451.944883	42.406592
3503.682382	707406.378161	42.411597
3503.371235	707363.174904	42.416602
3503.925738	707308.505530	42.421607
3503.780314	707264.430140	42.426612
3503.854516	707212.620597	42.431616
3503.835903	707154.767258	42.436621
3503.280234	707108.673042	42.441626
3503.861691	707053.997598	42.446631
3503.475120	707005.838698	42.451636
3503.198260	706973.404755	42.456640
3503.401318	706916.804433	42.461645
3503.070388	706882.342862	42.466650
3503.576182	706824.052985	42.471655
3503.358912	706788.876954	42.476660
3503.451930	706735.670819	42.481664
3503.449679	706678.506882	42.486669
3503.079604	706650.110007	42.491674
3503.350582	706599.704550	42.496679
3502.961643	706566.244612	42.501684
3503.057719	706530.618413	42.506688
3503.387780	706484.771799	42.511693
3503.056726	706451.152849	42.516698
3503.026398	706402.882030	42.521703
3503.004667	706370.006311	42.526708
3502.974437	706334.002837	42.531712
3502.909951	706291.101097	42.536717
3502.763732	706265.546669	42.541722
3503.324077	706228.153794	42.546727
3502.782053	706186.870157	42.551732
3503.038048	706148.384868	42.556736
3503.033884	706102.939138	42.561741
3502.844024	706074.907928	42.566746
3502.996463	706013.988861	42.571751
3502.864671	705985.848427	42.576756
3502.887725	705953.063055	42.581760
3502.828887	705915.324129	42.586765
3502.771673	705881.657698	42.591770
3502.984567	705848.045836	42.596775
3502.576375	705814.685497	42.601780
3502.665747	705782.683241	42.606784
3502.863673	705748.229067	42.611789
3502.921008	705719.361119	42.616794
3502.854851	705685.198691	42.621799
3502.488333	705646.516017	42.626804
3502.629898	705611.871929	42.631808
3502.804352	705581.295336	42.636813
3502.713134	705559.951808	42.641818
3502.765599	705521.149658	42.646823
3502.920406	705485.062388	42.651828
3502.921683	705452.278712	42.656832
3502.541526	705414.988078	42.661837
3502.494297	705387.427786	42.666842
3503.005826	705347.555537	42.671847
3502.663924	705321.881631	42.676852
3502.724929	705280.593336	42.681856
3503.155916	705251.364033	42.686861
3502.864523	705208.941470	42.691866
3502.650080	705169.486419	42.696871
3502.830212	705141.738747	42.701876
3502.727769	705112.249411	42.706880
3502.637024	705076.797108	42.711885
3502.187503	705054.120659	42.716890
3502.671247	705018.126101	42.721895
3502.722919	704994.571870	42.726900
3502.751913	704959.645721	42.731904
3502.903285	704933.988492	42.736909
3502.471199	704896.654524	42.741914
3502.714673	704860.152587	42.746919
3502.876520	704831.363752	42.751924
3502.598383	704784.863492	42.756928
3502.725200	704762.438761	42.761933
3502.507119	704741.561262	42.766938
3502.778268	704693.181382	42.771943
3502.583456	704672.001810	42.776948
3502.258214	704642.647046	42.781952
3502.430538	704615.296392	42.786957
3502.628417	704585.159501	42.791962
3502.563743	704547.117497	42.796967
3502.449303	704542.665631	42.801972
3502.352697	704499.760296	42.806977
3502.514977	704473.255376	42.811981
3502.035154	704450.433312	42.816986
3502.777921	704420.503867	42.821991
3502.742104	704397.210859	42.826996
3502.657198	704352.911868	42.832001
3502.894023	704331.709807	42.837005
3502.725402	704304.166123	42.842010
3502.584744	704259.081003	42.847015
3502.530029	704236.982987	42.852020
3502.485119	704213.094836	42.857025
3502.531194	704183.975225	42.862029
3502.457150	704154.577290	42.867034
3502.552864	704127.337117	42.872039
3502.631673	704103.825657	42.877044
3502.354277	704073.517131	42.882049
3502.365272	704033.522836	42.887053
3502.629455	704017.581613	42.892058
3502.254753	703983.463451	42.897063
3502.153231	703961.074382	42.902068
3502.341342	703931.036192	42.907073
3502.482926	703900.608139	42.912077
3502.283330	703891.251567	42.917082
3502.783942	703859.422640	42.922087
3502.691273	703834.398664	42.927092
3502.515015	703799.153984	42.932097
3502.728633	703762.155540	42.937101
3502.608754	703738.179104	42.942106
3502.668526	703708.558812	42.947111
3502.238081	703681.155780	42.952116
3502.402874	703653.455560	42.957121
3502.603647	703613.378281	42.962125
3502.351844	703591.658970	42.967130
3502.358012	703562.245769	42.972135
3502.872722	703536.822457	42.977140
3503.191175	703505.618539	42.982145
3503.105812	703459.725186	42.987149
3502.693196	703427.846868	42.992154
3502.696900	703390.732481	42.997159
3502.795683	703367.662882	43.002164
3502.515268	703343.562833	43.007169
3502.626833	703319.745728	43.012173
3502.626164	703278.805874	43.017178
3502.378050	703255.743623	43.022183
3502.536937	703225.558768	43.027188
3502.082351	703190.307925	43.032193
3502.698930	703162.432105	43.037197
3502.427848	703137.584659	43.042202
3502.488245	703109.303730	43.047207
3502.413380	703085.069620	43.052212
3502.434668	703063.452911	43.057217
3502.590397	703021.392905	43.062221
3502.068715	703009.405550	43.067226
3502.406933	702970.793181	43.072231
3502.398615	702964.633620	43.077236
3502.390274	702924.538036	43.082241
3502.618668	702902.389832	43.087245
3502.466641	702879.757883	43.092250
3502.640052	702842.265296	43.097255
3502.472462	702814.468271	43.102260
3502.461094	702795.290976	43.107265
3502.393944	702762.309678	43.112269
3502.259339	702736.146646	43.117274
3502.631346	702706.769464	43.122279
3502.266408	702686.606912	43.127284
3502.296419	702662.553045	43.132289
3502.486346	702631.069101	43.137293
3502.267445	702608.497185	43.142298
3502.444118	702581.089717	43.147303
3502.302347	702572.318428	43.152308
3502.134514	702545.216224	43.157313
3502.222343	702521.102721	43.162317
3502.068466	702499.314801	43.167322
3501.968261	702464.151508	43.172327
3502.075153	702456.233417	43.177332
3502.354396	702420.410964	43.182337
3502.420549	702405.294552	43.187341
3502.310794	702381.660524	43.192346
3502.370838	702359.141241	43.197351
3502.465040	702324.392465	43.202356
3502.536686	702309.771881	43.207361
3502.560981	702273.146221	43.212365
3502.097794	702258.117033	43.217370
3502.199721	702225.056065	43.222375
3502.381608	702202.814386	43.227380
3502.345048	702188.161790	43.232385
3502.278696	702157.563235	43.237389
3501.986139	702130.629425	43.242394
3502.546336	702110.759866	43.247399
3502.241271	702074.684717	43.252404
3501.801377	702062.583148	43.257409
3502.122361	702025.907416	43.262413
3502.161012	702023.714781	43.267418
3502.094919	701994.357909	43.272423
3502.183210	701976.404642	43.277428
3501.933489	701959.699815	43.282433
3501.950864	701933.558943	43.287437
3502.111101	701917.332900	43.292442
3502.258461	701895.791841	43.297447
3502.265464	701875.565936	43.302452
3502.292835	701839.832416	43.307457
3502.387823	701812.386336	43.312461
3502.017240	701800.123867	43.317466
3501.931089	701783.192895	43.322471
3502.163623	701769.141135	43.327476
3501.822415	701745.692711	43.332481
3502.091688	701729.547686	43.337485
3501.852866	701712.989665	43.342490
3502.247354	701682.213892	43.347495
3502.407980	701667.030892	43.352500
3502.008156	701638.970325	43.357505
3502.453749	701626.473337	43.362509
3502.274791	701601.854744	43.367514
3502.065952	701575.799878	43.372519
3502.136609	701552.879202	43.377524
3501.912542	701530.951373	43.382529
3501.831377	701508.751397	43.387533
3502.303217	701488.497469	43.392538
3502.156777	701469.488661	43.397543
3502.088412	701444.553175	43.402548
3501.916651	701421.771608	43.407553
3502.128146	701417.711526	43.412557
3501.995801	701398.252975	43.417562
3501.718005	701381.949242	43.422567
3502.087441	701363.650077	43.427572
3501.703589	701339.810040	43.432577
3502.054303	701319.824218	43.437581
3502.040234	701305.067028	43.442586
3501.975086	701279.832363	43.447591
3501.706072	701280.274589	43.452596
3501.871074	701251.274591	43.457601
3501.982395	701234.359614	43.462605
3502.063629	701226.444648	43.467610
3501.853066	701195.816852	43.472615
3502.082516	701184.150102	43.477620
3502.132889	701170.077787	43.482625
3501.895387	701139.106366	43.487629
3501.841962	701144.780849	43.492634
3501.388588	701110.316516	43.497639
3501.498521	701094.196652	43.502644
3501.842065	701087.033365	43.507649
3502.068633	701068.955985	43.512653
3501.810659	701046.137986	43.517658
3501.914481	701033.398451	43.522663
3502.060845	701025.124655	43.527668
3501.505163	701003.250302	43.532673
3501.977841	700988.909112	43.537677
3501.605534	700992.002408	43.542682
3501.801667	700976.265663	43.547687
3502.036281	700949.588961	43.552692
3502.069790	700945.061096	43.557697
3502.080604	700912.855080	43.562701
3501.985849	700909.938738	43.567706
3501.994244	700875.844450	43.572711
3502.018348	700850.941684	43.577716
3501.717928	700843.437335	43.582721
3501.698019	700826.095968	43.587725
3501.835006	700799.037351	43.592730
3501.696879	700787.033227	43.597735
3501.755043	700781.407824	43.602740
3501.644337	700765.423216	43.607745
3502.082201	700735.233332	43.612749
3501.850255	700737.657428	43.617754
3501.743012	700719.038100	43.622759
3502.028559	700696.526957	43.627764
3501.867272	700679.109264	43.632769
3502.066057	700651.841180	43.637773
3501.815496	700642.290727	43.642778
3501.877412	700619.219945	43.647783
3502.145374	700605.061061	43.652788
3501.900574	700593.968901	43.657793
3502.293751	700572.036052	43.662797
3501.894757	700550.234065	43.667802
3501.993615	700543.707178	43.672807
3502.434345	700512.770548	43.677812
3501.890297	700491.886997	43.682817
3502.290529	700470.698238	43.687821
3502.051892	700449.615011	43.692826
3501.691062	700434.665151	43.697831
3502.180197	700407.149517	43.702836
3501.584250	700399.246314	43.707841
3502.269689	700380.047951	43.712845
3501.653496	700361.661076	43.717850
3501.633123	700342.082261	43.722855
3501.796638	700331.667810	43.727860
3501.563205	700319.032673	43.732865
3502.173435	700287.371411	43.737869
3501.749883	700300.165269	43.742874
3501.932629	700277.272424	43.747879
3501.803624	700253.735211	43.752884
3501.624222	700244.818688	43.757889
3501.930759	700225.782011	43.762893
3501.848698	700218.986569	43.767898
3501.788198	700207.614948	43.772903
3501.842124	700200.896422	43.777908
3501.661203	700179.256278	43.782913
3501.720083	700158.172880	43.787917
3501.617778	700154.611399	43.792922
3501.725983	700144.702894	43.797927
3501.812231	700119.390153	43.802932
3501.507141	700119.291663	43.807937
3501.766702	700097.280303	43.812941
3501.673457	700094.363438	43.817946
3501.511753	700056.019610	43.822951
3501.609792	700055.307762	43.827956
3501.535273	700052.437492	43.832961
3501.896465	700045.320145	43.837965
3501.718276	700023.132427	43.842970
3501.336853	700006.395916	43.847975
3501.661413	700000.228951	43.852980
3501.452164	700003.544159	43.857985
3501.486239	699983.458509	43.862989
3501.489322	699966.558969	43.867994
3501.465599	699955.976201	43.872999
3501.640556	699958.929708	43.878004
3501.516887	699957.359826	43.883009
3501.699801	699934.863688	43.888013
3501.526619	699919.136375	43.893018
3501.854611	699908.097793	43.898023
3501.913408	699907.392418	43.903028
3501.780995	699880.524596	43.908033
3501.791254	699858.305316	43.913037
3501.813734	699851.542015	43.918042
3501.679148	699840.380978	43.923047
3501.613285	699819.168266	43.928052
3501.376091	699818.114165	43.933057
3501.456931	699801.648797	43.938061
3501.606380	699804.705981	43.943066
3501.395006	699773.675694	43.948071
3501.665779	699744.802338	43.953076
3501.590370	699747.200834	43.958081
3501.651332	699747.787416	43.963085
3501.703486	699723.175034	43.968090
3501.777713	699704.970901	43.973095
3501.611713	699702.861211	43.978100
3501.527844	699707.299028	43.983105
3501.612949	699684.371065	43.988109
3501.527814	699669.821680	43.993114
3501.296905	699664.143922	43.998119
3501.599664	699647.890117	44.003124
3501.246305	699651.676622	44.008129
3501.532603	699645.664850	44.013133
3501.574483	699624.533272	44.018138
3500.941308	699608.036424	44.023143
3501.097848	699591.856386	44.028148
3501.102544	699602.890486	44.033153
3501.082614	699591.461654	44.038157
3501.432701	699608.353653	44.043162
3501.475204	699599.996267	44.048167
3501.878600	699603.409199	44.053172
3501.940495	699588.537145	44.058177
3501.539976	699564.148244	44.063181
3501.788940	699562.765237	44.068186
3501.783362	699552.129277	44.073191
3502.080113	699528.320927	44.078196
3501.567596	699520.751076	44.083201
3501.652445	699501.152990	44.088205
3501.616957	699485.203316	44.093210
3501.479990	699465.890342	44.098215
3501.758704	699456.996717	44.103220
3501.315293	699464.277643	44.108225
3501.817566	699450.823772	44.113229
3501.769469	699436.665530	44.118234
3501.649208	699420.133267	44.123239
3501.811246	699418.814310	44.128244
3501.324727	699400.602803	44.133249
3501.343550	699372.266927	44.138253
3501.653453	699366.748135	44.143258
3501.611117	699364.767047	44.148263
3501.650748	699365.009231	44.153268
3501.540817	699352.749941	44.158273
3501.683202	699317.185929	44.163277
3501.249846	699324.912673	44.168282
3501.364163	699318.481734	44.173287
3501.587815	699323.763654	44.178292
3501.482192	699299.424694	44.183297
3501.471242	699275.368265	44.188301
3501.553546	699273.018605	44.193306
3501.100438	699274.087837	44.198311
3501.529392	699266.213050	44.203316
3501.422893	699276.520323	44.208321
3501.467098	699253.498578	44.213325
3501.719591	699247.094459	44.218330
3501.405549	699231.488605	44.223335
3501.471339	699225.413573	44.228340
3501.463183	699225.216288	44.233345
3501.670266	699203.012526	44.238349
3501.582258	699176.483161	44.243354
3501.285292	699175.836523	44.248359
3501.605975	699170.315826	44.253364
3501.339280	699163.003287	44.258369
3501.448549	699155.728024	44.263373
3501.483206	699140.312920	44.268378
3501.332890	699135.019166	44.273383
3501.744333	699120.685051	44.278388
3501.500952	699114.959289	44.283393
3501.438850	699113.528204	44.288397
3501.554644	699098.000200	44.293402
3501.538539	699071.955722	44.298407
3501.845245	699076.180183	44.303412
3501.109392	699073.816555	44.308417
3501.597045	699061.607225	44.313421
3501.659662	699052.500361	44.318426
3501.743690	699038.717311	44.323431
3501.788299	699018.677419	44.328436
3501.407164	699039.071577	44.333441
3501.151554	699007.449379	44.338445
3501.490874	698991.983665	44.343450
3501.225355	698979.948403	44.348455
3501.345709	698980.376095	44.353460
3501.603911	698981.327806	44.358465
3501.509303	698975.577365	44.363469
3501.300135	698973.872307	44.368474
3501.257415	698960.060371	44.373479
3501.639788	698937.180747	44.378484
3501.263003	698930.731268	44.383489
3501.427506	698921.756559	44.388493
3501.701622	698921.462908	44.393498
3501.503890	698914.188472	44.398503
3501.490227	698884.116552	44.403508
3501.542457	698888.134611	44.408513
3501.805679	698872.333295	44.413517
3501.428875	698872.445475	44.418522
3501.573280	698863.871708	44.423527
3501.576928	698835.337767	44.428532
3501.179336	698834.608311	44.433537
3501.428651	698840.532514	44.438541
3501.465755	698833.169491	44.443546
3501.451819	698831.929240	44.448551
3501.379946	698807.086234	44.453556
3501.293209	698793.331021	44.458561
3501.053728	698778.755953	44.463565
3501.344351	698783.828291	44.468570
3501.144374	698782.569069	44.473575
3501.198015	698786.736072	44.478580
3501.096639	698787.647811	44.483585
3500.961576	698786.029889	44.488589
3501.222754	698785.738372	44.493594
3501.489734	698789.720986	44.498599
3501.574503	698782.002070	44.503604
3501.313982	698768.275538	44.508609
3501.551054	698741.790555	44.513613
3501.677661	698739.930537	44.518618
3501.225440	698741.944185	44.523623
3501.640594	698731.784515	44.528628
3501.207456	698716.644820	44.533633
3501.445981	698689.264645	44.538637
3501.331842	698693.509132	44.543642
3501.464407	698682.948710	44.548647
3501.662166	698685.650327	44.553652
3501.182028	698682.598086	44.558657
3501.341764	698679.539518	44.563661
3501.404349	698663.621853	44.568666
3501.391370	698661.586043	44.573671
3501.559239	698650.124947	44.578676
3501.650209	698649.016467	44.583681
3501.468283	698643.926483	44.588685
3501.636852	698616.706777	44.593690
3501.179048	698612.805728	44.598695
3501.095274	698600.441641	44.603700
3501.340988	698610.840620	44.608705
3501.844132	698591.817623	44.613709
3501.441065	698597.750384	44.618714
3501.320369	698589.717275	44.623719
3501.879016	698560.096489	44.628724
3501.525025	698563.535580	44.633729
3501.595385	698556.415387	44.638733
3501.711694	698554.805590	44.643738
3501.562946	698532.112112	44.648743
3501.882125	698504.370050	44.653748
3501.695333	698507.632395	44.658753
3501.759581	698506.180329	44.663757
3501.758669	698477.695692	44.668762
3501.540824	698468.883134	44.673767
3501.698968	698463.339147	44.678772
3501.390693	698449.122885	44.683777
3501.364985	698422.928931	44.688781
3501.583813	698419.512521	44.693786
3501.577064	698414.244316	44.698791
3501.809719	698421.563505	44.703796
3501.592298	698400.024420	44.708801
3501.616143	698384.659490	44.713805
3501.793850	698385.077733	44.718810
3501.613856	698369.547614	44.723815
3502.014472	698344.177799	44.728820
3501.592597	698333.857725	44.733825
3501.842554	698323.128332	44.738829
3501.503268	698314.087123	44.743834
3501.580942	698286.086008	44.748839
3501.568432	698277.786168	44.753844
3501.600235	698284.989526	44.758849
3501.746474	698261.550613	44.763853
3501.504505	698239.965479	44.768858
3501.636015	698244.070159	44.773863
3501.889024	698226.429975	44.778868
3501.714673	698216.068856	44.783873
3501.409006	698195.289556	44.788877
3501.420602	698188.029636	44.793882
3501.500145	698184.636154	44.798887
3501.949990	698178.099218	44.803892
3501.585389	698154.495875	44.808897
3501.396542	698132.454272	44.813901
3501.753803	698132.594284	44.818906
3501.402279	698132.950861	44.823911
3501.419111	698124.944312	44.828916
3501.296331	698103.736858	44.833921
3501.432121	698087.308909	44.838925
3501.422358	698082.687289	44.843930
3500.819752	698100.236790	44.848935
3501.197154	698089.784336	44.853940
3501.299120	698084.100252	44.858945
3501.334799	698083.796268	44.863949
3501.588838	698091.708771	44.868954
3501.430082	698075.031192	44.873959
3501.573809	698048.211548	44.878964
3501.420275	698037.995922	44.883969
3501.696878	698040.137849	44.888973
3501.528394	698043.099051	44.893978
3501.447616	698025.215341	44.898983
3501.779695	697996.872973	44.903988
3501.650468	697997.192817	44.908993
3501.562986	697983.585603	44.913997
3501.474356	697974.005469	44.919002
3501.586378	697957.332631	44.924007
3501.639729	697942.011767	44.929012
3501.125240	697942.991864	44.934017
3501.389022	697947.571974	44.939021
3501.390654	697936.137423	44.944026
3501.164313	697935.628161	44.949031
3501.275570	697923.380033	44.954036
3501.541824	697916.376094	44.959041
3501.210981	697904.996449	44.964045
3501.599389	697904.982173	44.969050
3501.199239	697905.843947	44.974055
3501.157307	697904.558476	44.979060
3501.199881	697905.893953	44.984065
3501.380977	697900.196673	44.989069
3501.709123	697878.466715	44.994074
3501.396955	697864.598157	44.999079
3501.599153	697855.019545	45.004084
3501.826329	697859.208026	45.009089
3501.717169	697845.455034	45.014093
3501.652755	697826.623618	45.019098
3501.159898	697814.425462	45.024103
3501.446125	697801.004784	45.029108
3501.448749	697805.379549	45.034113
3501.277323	697802.673703	45.039117
3501.577815	697780.053186	45.044122
3501.538433	697769.022925	45.049127
3501.530799	697760.522927	45.054132
3501.169596	697764.112665	45.059137
3501.284944	697760.365090	45.064141
3501.531146	697755.651280	45.069146
3501.256513	697744.361569	45.074151
3501.426138	697711.620386	45.079156
3500.870199	697721.506592	45.084161
3500.766401	697713.022440	45.089165
3500.944816	697710.407899	45.094170
3501.235020	697710.559002	45.099175
3501.436163	697706.498927	45.104180
3501.438290	697715.547164	45.109185
3501.438933	697711.818525	45.114189
3501.168113	697716.636256	45.119194
3501.046855	697713.375211	45.124199
3501.501905	697709.074309	45.129204
3501.571161	697691.214840	45.134209
3501.316197	697668.089236	45.139213
3501.397309	697675.384377	45.144218
3501.407635	697671.355821	45.149223
3501.694428	697665.243188	45.154228
3501.490553	697661.399177	45.159233
3501.499803	697641.361989	45.164237
3501.547796	697637.426626	45.169242
3501.260587	697627.878933	45.174247
3501.461398	697619.095765	45.179252
3501.546330	697624.849092	45.184257
3501.385493	697613.938142	45.189261
3501.784540	697584.738194	45.194266
3501.517992	697574.590422	45.199271
3501.690712	697571.131589	45.204276
3501.501376	697571.063643	45.209281
3501.432148	697549.398547	45.214285
3501.813719	697532.630642	45.219290
3501.784471	697523.885400	45.224295
3501.617378	697510.042023	45.229300
3501.343696	697504.171059	45.234305
3501.311096	697471.760710	45.239309
3501.808247	697470.634674	45.244314
3501.287442	697486.083726	45.249319
3501.519739	697464.219436	45.254324
3501.621254	697467.384797	45.259329
3501.499567	697448.114576	45.264333
3501.567019	697426.128281	45.269338
3501.527130	697429.913642	45.274343
3501.510270	697425.591158	45.279348
3501.496147	697428.228746	45.284353
3501.425169	697393.537423	45.289357
3501.761793	697379.212847	45.294362
3501.316356	697381.076519	45.299367
3501.293306	697369.148128	45.304372
3500.943198	697372.587035	45.309377
3501.219499	697376.817347	45.314381
3501.360170	697360.834703	45.319386
3501.282733	697350.953730	45.324391
3501.357235	697333.639573	45.329396
3501.206635	697330.084923	45.334401
3501.216468	697331.376179	45.339405
3501.284276	697340.861414	45.344410
3501.035465	697340.753576	45.349415
3501.665836	697331.153354	45.354420
3501.389398	697327.172032	45.359425
3501.323108	697315.101558	45.364429
3501.215371	697291.354007	45.369434
3501.339844	697297.299888	45.374439
3501.863865	697275.386919	45.379444
3501.077047	697286.554737	45.384449
3501.357366	697288.944831	45.389453
3501.538593	697283.048257	45.394458
3501.321854	697266.030693	45.399463
3501.946814	697246.338323	45.404468
3501.359663	697249.617575	45.409473
3501.757976	697236.227235	45.414477
3501.429406	697236.430891	45.419482
3501.577207	697210.950442	45.424487
3501.709356	697197.753189	45.429492
3501.403664	697203.471909	45.434497
3501.534926	697191.617214	45.439501
3501.545636	697192.560310	45.444506
3501.162674	697175.222006	45.449511
3501.285936	697162.423925	45.454516
3501.567629	697155.217954	45.459521
3501.542824	697157.708230	45.464525
3501.635064	697157.941782	45.469530
3501.137494	697147.334501	45.474535
3501.399264	697125.563940	45.479540
3501.257616	697126.084745	45.484545
3501.582378	697106.541116	45.489549
3501.575365	697106.244154	45.494554
3501.529561	697108.539034	45.499559
3501.400182	697096.677567	45.504564
3501.319869	697081.029256	45.509569
3500.784609	697073.958233	45.514573
3501.276786	697068.606768	45.519578
3501.651598	697071.876266	45.524583
3501.663734	697068.046015	45.529588
3501.336295	697061.636717	45.534593
3501.057673	697062.925964	45.539597
3501.539332	697054.891343	45.544602
3501.228857	697043.358054	45.549607
3501.390799	697026.178004	45.554612
3501.355852	697020.515862	45.559617
3501.416303	697016.975926	45.564621
3501.721061	697018.268208	45.569626
3501.474604	697008.713106	45.574631
3501.820576	696984.143939	45.579636
3501.385991	696981.978535	45.584641
3501.619551	696979.106062	45.589645
3501.851654	696971.908139	45.594650
3501.388119	696956.770426	45.599655
3501.669950	696938.575978	45.604660
3501.828160	696923.782943	45.609665
3501.513038	696923.536895	45.614669
3501.511800	696900.118735	45.619674
3501.493699	696896.044802	45.624679
3501.309434	696876.535067	45.629684
3501.511451	696885.849448	45.634689
3501.204330	696888.833946	45.639693
3501.598639	696874.648184	45.644698
3501.713033	696860.260053	45.649703
3501.620399	696840.088718	45.654708
3501.621393	696836.807143	45.659713
3501.452105	696836.089498	45.664717
3501.412560	696825.306688	45.669722
3501.250148	696804.699311	45.674727
3501.600548	696789.426796	45.679732
3501.443190	696777.818130	45.684737
3501.273436	696788.586263	45.689741
3501.364102	696782.057941	45.694746
3501.313522	696784.403416	45.699751
3501.621409	696766.254030	45.704756
3501.655163	696758.740661	45.709761
3501.383580	696739.891437	45.714765
3501.595584	696733.094417	45.719770
3501.409003	696740.285407	45.724775
3501.593374	696716.885809	45.729780
3501.393258	696695.588299	45.734785
3501.278979	696694.165441	45.739789
3501.788383	696683.291736	45.744794
3501.367885	696698.327806	45.749799
3501.640889	696684.360675	45.754804
3501.033747	696655.870889	45.759809
3501.445946	696647.897103	45.764813
3501.476573	696643.815000	45.769818
3501.307439	696575.573963	45.774823
3501.224282	696445.661184	45.779828
3500.999291	696283.051286	45.784833
3501.013978	696054.214036	45.789837
3501.107701	695770.956236	45.794842
3500.508045	695428.327936	45.799847
3500.477105	695020.046409	45.804852
3500.834539	694568.164655	45.809857
3500.023843	694056.967732	45.814861
3499.715807	693477.962148	45.819866
3499.425330	692857.330371	45.824871
3499.231185	692158.685355	45.829876
3498.927563	691424.381654	45.834881
3498.282737	690622.704546	45.839885
3498.052248	689774.012694	45.844890
3497.574423	688851.279928	45.849895
3497.232443	687875.921587	45.854900
3496.327241	686837.085475	45.859905
3495.835777	685749.523462	45.864909
3495.147993	684604.058444	45.869914
3494.402721	683401.343168	45.874919
3494.150092	682121.791706	45.879924
3493.559243	680808.595476	45.884929
3492.655719	679416.203431	45.889933
3492.239224	677957.103912	45.894938
3491.171222	676452.733342	45.899943
3490.441194	674887.356524	45.904948
3489.294727	673260.570060	45.909953
3488.657359	671579.020932	45.914957
3487.576689	669843.137817	45.919962
3486.860633	668057.147982	45.924967
3485.720126	666191.871258	45.929972
3485.296284	664276.064932	45.934977
3483.655253	662307.375334	45.939981
3483.007304	660263.193226	45.944986
3481.665092	658189.986602	45.949991
3480.752888	656033.868358	45.954996
3479.324348	653847.291928	45.960001
3478.028027	651589.763309	45.965005
3477.161993	649274.681111	45.970010
3475.550494	646921.047861	45.975015
3474.343725	644500.251422	45.980020
3473.633961	642041.938252	45.985025
3471.595757	639501.367431	45.990029
3470.222067	636916.029241	45.995034
3469.312683	634285.227525	46.000039
3467.872603	631602.739896	46.005044
3466.400482	628850.673783	46.010049
3464.815706	626055.840331	46.015053
3463.765414	623214.648247	46.020058
3461.608626	620314.660003	46.025063
3460.320901	617371.699430	46.030068
3459.054312	614377.205060	46.035073
3457.353553	611315.820539	46.040077
3455.529945	608205.607898	46.045082
3453.670885	605057.811394	46.050087
3452.108075	601852.375793	46.055092
3450.672869	598606.812979	46.060097
3448.406804	595307.546032	46.065101
3446.911367	591951.712470	46.070106
3444.745351	588553.030761	46.075111
3443.380761	585090.572119	46.080116
3441.376696	581595.303495	46.085121
3439.162116	578043.750006	46.090125
3437.305075	574449.063317	46.095130
3435.402249	570816.167102	46.100135
3433.297010	567133.992829	46.105140
3431.413323	563400.578391	46.110145
3429.064662	559622.101695	46.115149
3427.039233	555798.256968	46.120154
3424.848651	551944.774390	46.125159
3422.974853	548030.208596	46.130164
3420.599819	544089.048758	46.135169
3418.347147	540087.996147	46.140173
3416.003494	536049.403276	46.145178
3414.016558	531976.008093	46.150183
3411.373213	527848.531142	46.155188
3409.476065	523674.035688	46.160193
3406.836709	519472.396335	46.165197
3404.889642	515219.222465	46.170202
3401.931685	510931.349964	46.175207
3399.694570	506588.466435	46.180212
3397.036347	502229.318673	46.185217
3394.380823	497816.720713	46.190221
3392.373148	493384.239828	46.195226
3389.702311	488888.276283	46.200231
3387.220475	484360.653635	46.205236
3384.623132	479794.586816	46.210241
3381.536207	475201.325170	46.215245
3379.311877	470553.700964	46.220250
3376.283670	465894.181743	46.225255
3373.840706	461173.800991	46.230260
3370.677255	456439.546504	46.235265
3367.991140	451677.750383	46.240269
3365.517605	446855.703062	46.245274
3362.308040	442014.738672	46.250279
3359.349677	437139.184480	46.255284
3356.706816	432238.881796	46.260289
3353.663511	427304.420335	46.265293
3351.123523	422333.908085	46.270298
3347.720927	417335.247507	46.275303
3344.986902	412311.018794	46.280308
3341.921268	407259.296256	46.285313
3339.015415	402170.565172	46.290317
3336.032632	397048.053411	46.295322
3332.461479	391917.096015	46.300327
3329.462180	386742.327914	46.305332
3326.188441	381554.966322	46.310337
3323.097342	376349.421668	46.315341
3320.238450	371090.341005	46.320346
3316.614258	365832.199660	46.325351
3313.451392	360545.681719	46.330356
3310.395629	355232.829601	46.335361
3307.094075	349901.233959	46.340365
3303.400630	344542.832418	46.345370
3300.195238	339177.739185	46.350375
3296.679795	333763.237804	46.355380
3293.228225	328344.902108	46.360385
3289.970289	322910.250069	46.365389
3286.533064	317458.538327	46.370394
3282.934297	311990.283230	46.375399
3279.213011	306504.063413	46.380404
3275.890110	301007.213704	46.385409
3272.052582	295498.014049	46.390413
3268.940403	289974.439377	46.395418
3264.873522	284444.726770	46.400423
3261.203093	278888.370772	46.405428
3257.834450	273332.269319	46.410433
3254.011221	267752.980616	46.415437
3250.362164	262169.543164	46.420442
3246.697610	256591.428555	46.425447
3242.655965	250982.115906	46.430452
3238.769624	245385.187148	46.435457
3234.997175	239776.064693	46.440461
3231.115307	234161.832684	46.445466
3227.249723	228543.074298	46.450471
3223.010964	222917.453266	46.455476
3219.537812	217295.774829	46.460481
3215.451582	211679.659315	46.465485
3211.384847	206036.099625	46.470490
3207.472836	200334.255558	46.475495
3203.240500	194706.455464	46.480500
3199.221486	189095.862629	46.485505
3195.096818	183461.032823	46.490509
3190.939102	177845.330500	46.495514
3186.340768	172243.148079	46.500519
3182.156070	166642.119897	46.505524
3177.918471	161040.826949	46.510529
3173.511411	155473.300714	46.515533
3169.377283	149901.756390	46.520538
3164.478031	144346.790480	46.525543
3160.068130	138800.552515	46.530548
3155.553137	133275.392971	46.535553
3151.146920	127780.889350	46.540557
3146.342644	122280.597933	46.545562
3141.571584	116810.911062	46.550567
3136.783955	111365.243768	46.555572
3132.085135	105942.081329	46.560577
3126.817405	100551.518419	46.565581
3121.977837	95178.064031	46.570586
3117.339163	89851.674579	46.575591
3111.913504	84544.983779	46.580596
3106.728045	79270.904469	46.585601
3101.411517	74038.541587	46.590605
3096.134763	68837.921584	46.595610
3090.630049	63687.429513	46.600615
3084.693920	58600.833258	46.605620
3078.868206	53546.345184	46.610625
3072.333294	48554.724724	46.615629
3065.582736	43643.578563	46.620634
3056.521725	38860.976612	46.625639
3041.832938	34329.251272	46.630644
3026.727772	29950.588728	46.635649
3011.271383	25778.881386	46.640653
2996.429382	21830.818174	46.645658
2981.950857	18131.453888	46.650663
2968.010840	14690.360308	46.655668
2954.317267	11488.770148	46.660673
2939.289521	8588.374669	46.665677
2919.257560	6118.670035	46.670682
2896.668065	4022.458759	46.675687
2875.596178	2262.900657	46.680692
2857.193831	846.364812	46.685697
2823.002785	237.023059	46.690701
2784.873332	251.153463	46.695706
2769.843603	247.294433	46.700711
2772.640877	243.597795	46.705716
2783.845167	244.139294	46.710721
2796.647188	256.268211	46.715725
2807.043107	253.424606	46.720730
2811.530695	237.156100	46.725735
2812.043610	242.216646	46.730740
2809.697170	235.560978	46.735745
2805.498573	242.757293	46.740749
2801.832466	233.700571	46.745754
2798.219984	242.379387	46.750759
2795.506335	232.689233	46.755764
2792.976375	230.497588	46.760769
2790.005652	234.889735	46.765773
2787.227432	232.452057	46.770778
2784.599903	222.721022	46.775783
2781.278002	228.830336	46.780788
2778.712855	228.445842	46.785793
2775.479131	221.081800	46.790797
2772.739933	225.263749	46.795802
2769.502282	227.248540	46.800807
2765.990971	227.391077	46.805812
2763.334865	218.217736	46.810817
2759.647018	228.709970	46.815821
2756.476970	216.908090	46.820826
2753.238237	228.902334	46.825831
2749.974074	234.219071	46.830836
2746.790399	223.340829	46.835841
2743.081407	224.636603	46.840845
2739.940925	218.446325	46.845850
2736.944157	220.040987	46.850855
2733.565323	222.439315	46.855860
2730.328606	215.245126	46.860865
2726.757697	219.127870	46.865869
2723.458004	216.474041	46.870874
2720.184955	216.058172	46.875879
2716.583687	214.290990	46.880884
2713.344601	211.119974	46.885889
2709.606444	221.880070	46.890893
2706.834559	206.577043	46.895898
2703.001260	214.166846	46.900903
2699.230600	214.434466	46.905908
2696.559686	195.185124	46.910913
2692.878291	209.527006	46.915917
2689.316281	208.122769	46.920922
2685.976401	205.185338	46.925927
2682.908539	205.595535	46.930932
2680.183096	197.752563	46.935937
2675.780274	210.043159	46.940941
2671.966730	205.352846	46.945946
2668.743445	201.939880	46.950951
2665.868526	212.062166	46.955956
2661.954707	202.219162	46.960961
2658.370916	213.759077	46.965965
2655.265586	205.575452	46.970970
2651.920350	204.192391	46.975975
2648.173542	204.239428	46.980980
2645.545976	201.677056	46.985985
2641.803124	206.141473	46.990989
2637.849161	205.470361	46.995994
2634.409484	198.716775	47.000999
2630.980362	209.319986	47.006004
2627.721248	209.815759	47.011009
2624.017505	213.627037	47.016013
2620.903626	201.400193	47.021018
2617.472096	206.447334	47.026023
2613.747923	196.906291	47.031028
2610.515907	202.533734	47.036033
2606.919512	208.190330	47.041037
2603.365937	194.162177	47.046042
2599.719532	195.831336	47.051047
2596.180288	204.409552	47.056052
2593.157336	188.995069	47.061057
2589.706599	202.329895	47.066061
2586.054398	197.038301	47.071066
2582.146626	194.545458	47.076071
2579.025936	203.003669	47.081076
2575.786663	193.189382	47.086081
2572.234812	195.756983	47.091085
2568.855461	197.750777	47.096090
2565.736461	191.004348	47.101095
2561.580359	198.744404	47.106100
2558.150237	195.410965	47.111105
2554.644891	205.849636	47.116109
2551.355775	195.809578	47.121114
2547.945898	191.917682	47.126119
2544.308871	195.496758	47.131124
2540.992970	181.964310	47.136129
2537.253431	194.162162	47.141133
2534.028553	191.425060	47.146138
2530.755286	188.556455	47.151143
2526.895258	194.407134	47.156148
2523.783566	183.142647	47.161153
2520.115705	187.122314	47.166157
2516.652771	186.160436	47.171162
2513.333806	182.299498	47.176167
2509.154865	187.631111	47.181172
2505.887641	188.820782	47.186177
2502.421789	186.107821	47.191181
2499.034843	184.790795	47.196186
2496.030524	173.562037	47.201191
2492.158320	180.853947	47.206196
2488.530400	173.466643	47.211201
2485.117464	188.724646	47.216205
2481.720386	185.559263	47.221210
2478.067459	185.567619	47.226215
2474.386580	189.780168	47.231220
2471.356805	179.055698	47.236225
2467.750850	184.699771	47.241229
2464.312786	176.516953	47.246234
2461.033185	183.043160	47.251239
2457.286055	187.162303	47.256244
2453.911539	173.581632	47.261249
2450.314882	177.716314	47.266253
2446.526496	171.248975	47.271258
2443.337289	176.361094	47.276263
2440.011103	181.738232	47.281268
2436.521612	178.179900	47.286273
2432.981216	178.352986	47.291277
2429.408277	174.702312	47.296282
2425.879519	177.944062	47.301287
2422.270901	180.021917	47.306292
2418.362547	172.742100	47.311297
2415.000515	177.435889	47.316301
2411.998204	183.579944	47.321306
2408.922180	178.335577	47.326311
2405.140980	175.847204	47.331316
2401.722772	172.522389	47.336321
2398.084604	184.099695	47.341325
2394.640852	173.655993	47.346330
2391.063316	175.881071	47.351335
2387.409858	174.319768	47.356340
2383.972395	177.001186	47.361345
2380.125219	180.376223	47.366349
2376.715639	178.353418	47.371354
2373.285104	176.826841	47.376359
2369.735264	176.903862	47.381364
2366.679690	177.762183	47.386369
2362.859717	183.951707	47.391373
2359.386801	179.386836	47.396378
2356.012719	175.903589	47.401383
2352.653835	174.914552	47.406388
2349.434797	173.761850	47.411393
2345.564953	172.783248	47.416397
2341.682602	173.461795	47.421402
2338.362122	172.094032	47.426407
2334.966835	167.780169	47.431412
2331.899670	171.020529	47.436417
2327.957302	180.133591	47.441421
2324.551346	169.109048	47.446426
2320.943018	171.412694	47.451431
2317.647604	168.410981	47.456436
2314.397014	170.219657	47.461441
2310.496404	172.085483	47.466445
2306.841516	165.582949	47.471450
2303.747191	164.756152	47.476455
2299.936328	167.736092	47.481460
2296.666068	160.134824	47.486465
2292.897395	172.360563	47.491469
2289.562455	173.718893	47.496474
2286.049205	162.605600	47.501479
2282.539969	166.480250	47.506484
2279.107187	161.888087	47.511489
2275.423538	171.065488	47.516493
2272.226945	168.347003	47.521498
2268.693000	164.064652	47.526503
2265.224988	170.329748	47.531508
2261.666394	163.764143	47.536513
2258.108790	166.164028	47.541517
2254.309063	165.410900	47.546522
2251.278369	172.694253	47.551527
2247.454569	172.197908	47.556532
2244.266575	166.237930	47.561537
2240.396179	170.667759	47.566541
2236.458655	161.502270	47.571546
2233.429183	163.484345	47.576551
2230.190256	164.233816	47.581556
2227.142450	165.983312	47.586561
2223.011442	167.843378	47.591565
2219.580783	165.570423	47.596570
2216.339496	164.025653	47.601575
2212.706087	169.519365	47.606580
2209.167428	159.674110	47.611585
2205.480500	164.080087	47.616589
2201.853989	165.753983	47.621594
2198.462343	166.217971	47.626599
2195.166014	166.160396	47.631604
2191.804646	160.828895	47.636609
2188.174357	162.558090	47.641613
2184.751146	164.371584	47.646618
2181.111280	160.183427	47.651623
2177.433407	156.319680	47.656628
2174.238887	158.007874	47.661633
2170.790460	161.434054	47.666637
2167.253476	157.696557	47.671642
2163.658277	157.631885	47.676647
2160.449604	156.119449	47.681652
2156.800443	159.127980	47.686657
2152.829933	158.026325	47.691661
2149.215236	156.412047	47.696666
2146.257934	154.458171	47.701671
2142.415648	160.299916	47.706676
2139.153205	160.070021	47.711681
2135.542100	165.670609	47.716685
2131.906401	162.284971	47.721690
2128.403418	150.738759	47.726695
2124.943148	154.904189	47.731700
2121.706862	153.687826	47.736705
2118.450706	154.754005	47.741709
2114.819438	153.086854	47.746714
2111.191464	149.609381	47.751719
2107.559604	158.030418	47.756724
2104.063691	147.588151	47.761729
2100.697796	151.722176	47.766733
2097.043532	151.854029	47.771738
2094.006881	142.939047	47.776743
2089.939151	153.791086	47.781748
2086.611283	151.162388	47.786753
2083.107224	155.882125	47.791757
2079.329356	155.335111	47.796762
2076.032762	151.221012	47.801767
2072.368574	154.627370	47.806772
2069.294265	153.038279	47.811777
2065.323145	153.054925	47.816781
2061.979857	157.028944	47.821786
2058.550482	159.514310	47.826791
2055.290281	148.163564	47.831796
2051.865190	144.142808	47.836801
2048.058731	152.176241	47.841805
2044.459724	164.190727	47.846810
2041.293808	151.699546	47.851815
2037.612071	159.484795	47.856820
2034.074520	149.883046	47.861825
2030.819345	160.070254	47.866829
2027.189941	158.894242	47.871834
2023.643668	160.262344	47.876839
2019.975567	160.608301	47.881844
2016.557343	144.582022	47.886849
2013.070831	151.796800	47.891853
2009.513605	151.249796	47.896858
2006.001061	149.236280	47.901863
2002.259046	159.797030	47.906868
1999.213696	152.787866	47.911873
1995.623940	151.164463	47.916877
1992.232764	153.647104	47.921882
1988.761796	156.147706	47.926887
1984.764474	162.297867	47.931892
1981.374279	149.609076	47.936897
1978.142876	157.749941	47.941901
1974.587194	154.302053	47.946906
1971.021435	155.799330	47.951911
1967.531925	154.099743	47.956916
1964.234048	143.499684	47.961921
1960.826454	158.511629	47.966925
1957.169010	158.291098	47.971930
1953.651510	155.671045	47.976935
1950.061867	151.455444	47.981940
1946.508602	148.151830	47.986945
1942.743610	145.921696	47.991949
1938.811953	158.655029	47.996954
1936.333731	149.066077	48.001959
1932.789769	147.947033	48.006964
1929.478193	147.163433	48.011969
1925.852004	145.837795	48.016973
1921.767332	148.331230	48.021978
1918.479699	149.062770	48.026983
1914.988613	152.625480	48.031988
1911.640860	145.424574	48.036993
1907.985567	147.760625	48.041997
1904.623213	142.311144	48.047002
1901.154472	146.469077	48.052007
1897.630274	151.026538	48.057012
1894.286974	148.726165	48.062017
1891.045717	152.019959	48.067021
1887.325024	148.609564	48.072026
1883.809689	144.782700	48.077031
1879.931092	144.555478	48.082036
1876.586198	152.849806	48.087041
1872.934748	144.940707	48.092045
1869.320697	149.645891	48.097050
1866.163599	142.072430	48.102055
1861.965871	147.998192	48.107060
1858.819448	149.302136	48.112065
1855.730036	142.579630	48.117069
1851.703349	151.508540	48.122074
1848.599378	150.082799	48.127079
1844.782211	160.341577	48.132084
1841.438339	150.181615	48.137089
1838.176544	161.039617	48.142093
1833.945173	161.133960	48.147098
1830.843997	154.190429	48.152103
1827.762934	152.995540	48.157108
1824.256865	151.690735	48.162113
1820.499336	145.279888	48.167117
1816.695555	162.989681	48.172122
1813.716921	152.506154	48.177127
1810.009013	161.545859	48.182132
1806.492606	149.090297	48.187137
1803.017314	148.161860	48.192141
1799.694172	158.829167	48.197146
1796.120174	146.770733	48.202151
1792.315081	147.072705	48.207156
1789.210651	153.169559	48.212161
1785.446818	154.115318	48.217165
1781.593008	152.361037	48.222170
1778.725988	147.561281	48.227175
1774.844813	149.019447	48.232180
1771.145949	151.002307	48.237185
1767.982420	152.253506	48.242189
1764.348580	153.263774	48.247194
1761.087389	143.977608	48.252199
1757.412192	154.832360	48.257204
1754.199105	141.331407	48.262209
1750.461243	147.496784	48.267213
1746.882564	150.171337	48.272218
1743.907305	139.602266	48.277223
1739.998033	157.112133	48.282228
1736.514705	152.534359	48.287233
1732.601971	155.098541	48.292237
1729.077324	149.395505	48.297242
1725.833512	144.621944	48.302247
1722.347316	148.156571	48.307252
1719.036958	150.142165	48.312257
1715.751205	138.370914	48.317261
1711.878319	158.102305	48.322266
1708.569757	143.471090	48.327271
1704.999671	136.835307	48.332276
1701.700600	147.985119	48.337281
1698.191458	136.932520	48.342285
1694.301107	151.705581	48.347290
1690.856947	145.865311	48.352295
1687.631684	152.350894	48.357300
1683.960901	142.341188	48.362305
1680.360393	143.245955	48.367309
1676.253229	148.299655	48.372314
1673.446385	140.090493	48.377319
1669.864322	146.727594	48.382324
1666.156845	141.191883	48.387329
1662.885083	148.354950	48.392333
1659.344835	137.601380	48.397338
1656.114063	143.824057	48.402343
1652.582735	147.652757	48.407348
1648.983535	141.297531	48.412353
1645.464575	143.605486	48.417357
1642.028799	138.599988	48.422362
1638.553066	145.943709	48.427367
1634.497260	142.397506	48.432372
1630.984026	133.259224	48.437377
1627.692195	131.080988	48.442381
1624.107976	135.344527	48.447386
1620.821450	134.914800	48.452391
1617.403488	133.088023	48.457396
1613.856825	134.037005	48.462401
1610.606986	136.264452	48.467405
1606.886015	135.894930	48.472410
1603.622575	132.317038	48.477415
1599.763663	143.556391	48.482420
1596.400103	146.208823	48.487425
1592.930595	134.789423	48.492429
1589.333046	142.476418	48.497434
1585.973138	128.516113	48.502439
1582.095742	138.259577	48.507444
1578.438425	142.239273	48.512449
1575.223059	141.441593	48.517453
1571.584882	136.752504	48.522458
1568.572358	140.964907	48.527463
1564.478458	141.139157	48.532468
1561.325129	138.881177	48.537473
1557.894272	136.789199	48.542477
1554.271674	141.843574	48.547482
1551.365176	137.151973	48.552487
1547.696144	141.912523	48.557492
1543.669276	139.476962	48.562497
1540.046008	134.846803	48.567501
1536.418369	142.351954	48.572506
1533.256044	130.471417	48.577511
1529.650312	140.387739	48.582516
1526.440597	135.780776	48.587521
1522.796479	138.468346	48.592525
1518.855961	142.782378	48.597530
1515.702989	133.319642	48.602535
1512.102441	142.318692	48.607540
1508.918880	132.053735	48.612545
1505.416602	127.446370	48.617549
1501.341155	142.994230	48.622554
1498.672723	135.262108	48.627559
1495.300472	136.177732	48.632564
1491.279245	136.466696	48.637569
1487.694575	132.659984	48.642573
1484.258821	130.339581	48.647578
1480.957449	130.635668	48.652583
1477.029651	142.102236	48.657588
1473.611245	137.905457	48.662593
1470.321979	133.937093	48.667597
1466.561600	135.012027	48.672602
1463.131802	130.521935	48.677607
1459.400078	134.834349	48.682612
1456.433728	133.620729	48.687617
1452.571043	133.456009	48.692621
1448.952694	144.077795	48.697626
1445.985128	135.939082	48.702631
1442.326922	140.698718	48.707636
1438.663434	129.352692	48.712641
1434.861431	131.589368	48.717645
1431.283516	127.298118	48.722650
1428.131044	134.740928	48.727655
1424.511609	133.362930	48.732660
1421.045922	131.712371	48.737665
1417.905576	129.030650	48.742669
1414.210932	139.977102	48.747674
1410.805195	127.850915	48.752679
1407.149400	141.959153	48.757684
1403.454996	135.549313	48.762689
1400.607935	132.495727	48.767693
1396.908480	142.282462	48.772698
1393.036074	135.926625	48.777703
1389.432814	135.518841	48.782708
1385.869874	132.338517	48.787713
1382.775536	126.376978	48.792717
1379.287351	128.566785	48.797722
1375.863427	120.624602	48.802727
1371.939858	134.911463	48.807732
1368.588704	130.114976	48.812737
1365.207067	135.426336	48.817741
1361.403807	132.399364	48.822746
1358.472593	121.873456	48.827751
1354.611616	127.606312	48.832756
1351.302450	125.734690	48.837761
1348.004940	121.236380	48.842765
1343.754416	133.168624	48.847770
1340.705853	126.971407	48.852775
1336.907201	130.554038	48.857780
1333.356203	127.525311	48.862785
1330.179473	133.592643	48.867789
1326.023380	135.699108	48.872794
1322.817665	126.157486	48.877799
1319.461919	123.418633	48.882804
1315.976570	130.535488	48.887809
1312.777708	129.082304	48.892813
1308.890948	134.611292	48.897818
1305.882337	124.947795	48.902823
1302.189202	133.773717	48.907828
1298.796191	129.776340	48.912833
1295.163010	129.718943	48.917837
1291.500747	139.613260	48.922842
1288.200805	131.078711	48.927847
1284.562671	129.589885	48.932852
1280.748613	142.646236	48.937857
1277.893866	126.596328	48.942861
1274.037462	139.529268	48.947866
1270.491112	127.111798	48.952871
1266.870276	130.957446	48.957876
1263.479468	125.517217	48.962881
1259.641934	123.854293	48.967885
1256.324978	132.887013	48.972890
1253.229196	126.128984	48.977895
1249.436820	126.499419	48.982900
1245.679997	128.914666	48.987905
1242.635390	122.021074	48.992909
1239.153003	135.919517	48.997914
1235.932194	124.789562	49.002919
1232.347967	129.928225	49.007924
1228.613674	122.335254	49.012929
1225.014915	130.635866	49.017933
1221.146676	130.294892	49.022938
1218.009620	126.862721	49.027943
1214.412110	121.679820	49.032948
1210.763492	126.911471	49.037953
1207.651889	120.204062	49.042957
1203.874052	133.488302	49.047962
1200.554441	127.740907	49.052967
1196.978884	131.598839	49.057972
1193.333234	132.227963	49.062977
1189.959428	123.256236	49.067981
1186.363136	125.371398	49.072986
1183.570602	131.381608	49.077991
1179.303712	129.366519	49.082996
1175.678572	126.987633	49.088001
1172.467687	124.442537	49.093005
1168.876140	129.557210	49.098010
1165.567217	130.487470	49.103015
1161.951158	133.842634	49.108020
1158.627568	132.647273	49.113025
1155.177487	129.432260	49.118029
1151.371744	136.945972	49.123034
1148.009861	134.041145	49.128039
1144.568905	125.760223	49.133044
1140.339341	130.394895	49.138049
1137.488442	127.201250	49.143053
1133.865702	124.480815	49.148058
1130.861302	132.686242	49.153063
1126.791177	130.198702	49.158068
1122.994752	133.758865	49.163073
1120.057339	119.105551	49.168077
1116.123576	125.503488	49.173082
1113.005650	124.436645	49.178087
1109.624431	133.180190	49.183092
1105.850247	127.568103	49.188097
1102.510241	127.488089	49.193101
1098.790857	134.316775	49.198106
1095.281858	126.239988	49.203111
1091.709531	133.379353	49.208116
1088.172051	129.816204	49.213121
1085.136109	132.198019	49.218125
1081.328650	124.541763	49.223130
1077.731044	119.411307	49.228135
1074.249797	131.604707	49.233140
1070.559117	129.053276	49.238145
1067.381528	123.159103	49.243149
1063.844876	132.343274	49.248154
1060.196455	132.921478	49.253159
1056.858023	128.374371	49.258164
1053.385370	135.563534	49.263169
1050.012673	135.035119	49.268173
1046.627732	136.508334	49.273178
1042.725275	132.584682	49.278183
1038.832389	127.637450	49.283188
1035.610649	130.233263	49.288193
1032.445002	115.152988	49.293197
1029.012411	122.831024	49.298202
1025.319025	125.720605	49.303207
1021.840872	128.665640	49.308212
1017.934412	136.695442	49.313217
1014.946976	129.229362	49.318221
1011.466530	127.754094	49.323226
1008.187902	124.593448	49.328231
1004.466936	121.766106	49.333236
1000.557040	138.235117	49.338241
997.454308	127.986230	49.343245
993.569438	128.073697	49.348250
990.367315	116.902598	49.353255
986.873647	122.041834	49.358260
983.118604	125.782332	49.363265
980.136301	117.456241	49.368269
975.932502	125.779528	49.373274
972.439250	122.840424	49.378279
968.809864	123.946187	49.383284
965.499716	129.948319	49.388289
962.716199	119.976630	49.393293
958.631292	128.350060	49.398298
955.582296	124.443115	49.403303
951.873102	124.419178	49.408308
948.141241	132.897417	49.413313
944.613692	121.672231	49.418317
940.806909	135.158633	49.423322
937.799051	117.285827	49.428327
934.200568	112.506127	49.433332
930.674719	116.886869	49.438337
927.317772	106.956721	49.443341
923.533723	122.079595	49.448346
920.083845	113.331515	49.453351
916.724705	114.019509	49.458356
913.246161	118.531931	49.463361
910.119778	111.483681	49.468365
906.018534	120.329722	49.473370
902.477848	124.899633	49.478375
899.305392	124.148477	49.483380
895.767695	130.901404	49.488385
892.465729	113.315055	49.493389
888.671209	127.994516	49.498394
885.157128	117.285360	49.503399
881.548810	119.951582	49.508404
877.839620	121.148624	49.513409
874.734915	118.759419	49.518413
870.722524	124.691316	49.523418
867.874292	125.139835	49.528423
864.361555	128.123703	49.533428
860.487304	129.639427	49.538433
857.322398	124.616737	49.543437
853.838582	125.550838	49.548442
849.928654	116.245553	49.553447
846.290485	121.692860	49.558452
843.020954	124.567307	49.563457
840.075888	124.773414	49.568461
836.182289	122.836656	49.573466
832.500705	119.956180	49.578471
828.749748	126.239980	49.583476
825.427387	133.510152	49.588481
822.486878	119.707545	49.593485
818.662128	128.090612	49.598490
815.231309	118.952102	49.603495
811.368716	113.033547	49.608500
808.090445	124.668741	49.613505
804.845189	113.518796	49.618509
800.998243	121.419132	49.623514
797.702140	112.663012	49.628519
794.064124	120.795464	49.633524
790.481894	116.308419	49.638529
787.300623	115.181913	49.643533
783.645367	114.590533	49.648538
780.072195	117.737639	49.653543
776.795559	111.397031	49.658548
772.764147	108.573511	49.663553
769.523879	106.432061	49.668557
766.324011	112.539569	49.673562
762.532912	116.103330	49.678567
758.726750	113.869359	49.683572
755.121338	113.323801	49.688577
752.296924	113.591837	49.693581
748.422491	118.795875	49.698586
744.970206	119.694252	49.703591
741.394232	115.594768	49.708596
737.925055	115.643868	49.713601
734.660750	110.116242	49.718605
730.741142	112.590182	49.723610
727.595495	106.649577	49.728615
724.083731	118.819890	49.733620
720.651986	112.119891	49.738625
717.175534	115.466089	49.743629
713.646562	111.482952	49.748634
710.285108	116.100033	49.753639
706.583716	111.910704	49.758644
703.024062	110.273446	49.763649
699.431838	111.383356	49.768653
695.868301	112.157380	49.773658
692.211917	112.468092	49.778663
689.046579	105.627791	49.783668
685.574432	115.119064	49.788673
682.267344	116.985583	49.793677
678.110863	115.473298	49.798682
674.763849	112.885723	49.803687
671.465019	115.388861	49.808692
668.136815	119.961780	49.813697
664.517051	117.661433	49.818701
660.766451	115.352624	49.823706
656.863764	117.640704	49.828711
653.773257	110.725848	49.833716
650.183526	118.897373	49.838721
647.080697	110.451285	49.843725
643.702436	115.027207	49.848730
640.300080	112.881803	49.853735
636.485171	121.827183	49.858740
632.492313	119.231647	49.863745
629.260710	113.666127	49.868749
625.690467	119.705601	49.873754
622.358092	110.256916	49.878759
619.372650	110.018596	49.883764
615.541618	115.523592	49.888769
612.231156	108.624382	49.893773
608.417866	116.043337	49.898778
604.774530	114.914193	49.903783
601.339889	114.706478	49.908788
597.787502	115.572081	49.913793
594.320513	106.029946	49.918797
590.659784	117.102669	49.923802
587.317123	114.788547	49.928807
583.666924	112.053874	49.933812
580.053658	112.346680	49.938817
577.261998	104.319427	49.943821
573.445063	108.793420	49.948826
569.754712	112.478177	49.953831
566.451715	111.306167	49.958836
562.784236	113.921531	49.963841
559.774853	106.913368	49.968845
556.029074	116.266473	49.973850
552.323270	105.750735	49.978855
548.949045	105.544874	49.983860
544.746863	106.876998	49.988865
541.615389	106.829345	49.993869
537.902799	109.627062	49.998874
534.908223	108.580668	50.003879
531.682668	109.585044	50.008884
527.893443	109.346499	50.013889
524.482405	95.878082	50.018893
520.918695	109.700372	50.023898
517.197295	108.235198	50.028903
514.048754	112.188377	50.033908
510.241502	115.313236	50.038913
506.685889	114.100749	50.043917
502.932252	111.433657	50.048922
499.761273	107.287278	50.053927
496.385539	108.024968	50.058932
492.598928	108.038415	50.063937
489.423082	110.590741	50.068941
485.723095	113.937370	50.073946
482.197814	116.905310	50.078951
479.102650	108.599198	50.083956
475.048059	110.259717	50.088961
471.998717	109.028689	50.093965
468.263749	111.915240	50.098970
464.930219	113.759304	50.103975
461.436266	109.333900	50.108980
457.747105	106.478546	50.113985
454.065666	103.903706	50.118989
450.773887	114.232293	50.123994
447.019628	114.179436	50.128999
443.740483	110.536513	50.134004
440.184518	116.408808	50.139009
436.797669	97.597810	50.144013
432.940973	116.178198	50.149018
429.479431	112.186508	50.154023
426.517516	101.989765	50.159028
422.960910	107.926116	50.164033
419.365407	103.354824	50.169037
415.751963	113.258535	50.174042
411.782259	112.264110	50.179047
408.516606	114.669411	50.184052
405.273333	114.828898	50.189057
402.031140	100.783182	50.194061
398.522829	106.256679	50.199066
394.575147	101.498039	50.204071
391.080918	102.688852	50.209076
387.444867	111.847858	50.214081
384.392007	107.388131	50.219085
380.814533	113.086254	50.224090
376.971758	113.098097	50.229095
373.706457	108.755169	50.234100
370.206790	115.139528	50.239105
366.970345	106.843572	50.244109
363.282928	110.485808	50.249114
359.686034	100.610299	50.254119
356.176039	101.604852	50.259124
352.207341	106.766522	50.264129
349.106461	108.406671	50.269133
345.440333	113.850590	50.274138
342.119866	109.415624	50.279143
338.607490	104.628337	50.284148
334.908314	109.544562	50.289153
331.655729	102.839854	50.294157
328.196934	117.463215	50.299162
324.641411	114.089106	50.304167
321.511652	105.776457	50.309172
317.600245	120.481735	50.314177
314.356616	109.991098	50.319181
310.363981	112.837141	50.324186
307.019826	113.126348	50.329191
303.949006	101.040785	50.334196
300.078474	106.946522	50.339201
296.627054	96.300011	50.344205
292.865446	101.566255	50.349210
289.288284	104.859906	50.354215
285.868866	106.105480	50.359220
282.344628	107.418793	50.364225
279.185774	111.368349	50.369229
275.698693	111.993315	50.374234
272.109127	111.562808	50.379239
268.776891	114.935567	50.384244
264.905875	113.483075	50.389249
261.501726	108.500283	50.394253
258.096121	113.829956	50.399258
254.717482	107.705505	50.404263
250.734663	102.898203	50.409268
247.122861	110.690918	50.414273
243.966743	108.272513	50.419277
240.393633	117.534462	50.424282
237.019888	104.041993	50.429287
233.835608	106.473585	50.434292
230.293381	114.886221	50.439297
226.729864	101.717745	50.444301
223.060633	104.921973	50.449306
219.607476	106.136707	50.454311
216.441827	110.123160	50.459316
212.134132	111.162981	50.464321
209.056600	106.538985	50.469325
205.358793	114.877447	50.474330
202.192076	108.873923	50.479335
198.609493	102.431575	50.484340
195.039665	108.788278	50.489345
191.421138	108.218017	50.494349
187.897987	101.856381	50.499354
184.484341	106.855933	50.504359
180.848117	99.187809	50.509364
177.284969	104.145512	50.514369
174.156150	103.922103	50.519373
170.459323	107.753749	50.524378
166.879623	102.911323	50.529383
163.661966	102.358143	50.534388
159.859468	110.618731	50.539393
156.515613	108.172402	50.544397
153.072309	104.490332	50.549402
149.175701	112.328886	50.554407
145.654436	106.666916	50.559412
142.273815	105.945873	50.564417
138.990861	101.026929	50.569421
135.747677	115.786483	50.574426
132.069027	111.252981	50.579431
128.523335	104.418395	50.584436
124.757430	112.493363	50.589441
121.384702	99.638630	50.594445
117.924393	104.556406	50.599450
114.029300	91.794817	50.604455
110.941179	99.330713	50.609460
107.121474	102.642940	50.614465
103.828842	95.494402	50.619469
100.543400	104.424892	50.624474
97.158099	103.348681	50.629479
93.688698	95.112236	50.634484
89.859020	108.521860	50.639489
86.566270	97.739678	50.644493
83.003630	96.423005	50.649498
79.192744	105.873790	50.654503
75.966502	105.635873	50.659508
72.443457	113.597316	50.664513
68.732501	99.464099	50.669517
65.025762	106.733840	50.674522
61.621709	111.787555	50.679527
58.294244	102.775715	50.684532
54.625653	102.963380	50.689537
51.394890	101.005301	50.694541
47.936009	97.752163	50.699546
44.242785	97.541573	50.704551
41.003674	90.458794	50.709556
37.352649	100.416631	50.714561
33.911099	95.162045	50.719565
30.499320	96.714422	50.724570
26.628875	102.884444	50.729575
23.539287	95.529767	50.734580
19.948345	113.192145	50.739585
16.692617	102.728489	50.744589
12.085209	99.605319	50.749594
8.834865	101.518047	50.754599
6.013097	99.911357	50.759604
2.391988	112.839042	50.764609