Fri Jun 17 17:17:31 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.075415	95.593330	0.000000
-0.754838	91.090406	0.005005
-0.664180	85.311990	0.010010
-0.899625	71.249920	0.015014
-1.499787	75.769454	0.020019
-0.837084	76.031200	0.025024
-1.073953	87.135897	0.030029
-1.326457	69.198301	0.035034
-1.534691	59.288316	0.040038
-2.023949	59.080486	0.045043
-2.008773	43.032670	0.050048
-2.228284	36.787244	0.055053
-2.915243	30.613207	0.060058
-3.214361	15.558934	0.065062
-3.517541	29.988591	0.070067
-3.509102	21.272778	0.075072
-4.046488	18.254270	0.080077
-4.140736	16.841785	0.085082
-4.381917	15.312040	0.090086
-4.917247	14.936048	0.095091
-4.872105	2.700466	0.100096
-5.225026	3.018358	0.105101
-5.699086	0.253357	0.110106
-5.822092	2.148973	0.115110
-5.833227	-11.423631	0.120115
-6.257277	-11.026232	0.125120
-6.873401	-5.940885	0.130125
-7.335801	-4.954985	0.135130
-7.068769	-12.729084	0.140134
-7.498677	4.218243	0.145139
-7.950122	-5.001263	0.150144
-7.427187	-2.005355	0.155149
-8.031233	-7.224658	0.160154
-8.024003	-5.799619	0.165158
-8.767896	3.063558	0.170163
-8.512100	0.486255	0.175168
-9.641807	-2.388401	0.180173
-9.989070	1.196152	0.185178
-9.611129	2.730261	0.190182
-10.639878	17.226644	0.195187
-10.581461	-2.342580	0.200192
-10.188314	5.870625	0.205197
-10.704707	5.271265	0.210202
-10.542495	-0.917029	0.215206
-10.848785	-0.611033	0.220211
-11.087469	-2.393576	0.225216
-11.619364	-1.231747	0.230221
-11.944444	-2.490026	0.235226
-12.132414	0.057714	0.240230
-12.594531	-2.240807	0.245235
-12.260802	3.000210	0.250240
-12.660344	4.955410	0.255245
-13.476197	1.446654	0.260250
-13.076652	-5.796159	0.265254
-13.697491	-3.435362	0.270259
-13.992336	-7.998433	0.275264
-14.752382	-4.339541	0.280269
-15.081876	2.056194	0.285274
-14.614389	1.152390	0.290278
-15.118147	-1.314833	0.295283
-14.893603	2.543284	0.300288
-14.894244	-3.600967	0.305293
-15.302485	-0.917552	0.310298
-15.802327	-4.840741	0.315302
-16.625662	8.761916	0.320307
-16.549404	3.380390	0.325312
-16.295625	2.244531	0.330317
-16.638375	-3.543501	0.335322
-17.140152	-8.683109	0.340326
-17.641829	2.005961	0.345331
-17.969259	-2.385344	0.350336
-18.148765	7.479599	0.355341
-18.233473	-4.861471	0.360346
-18.398396	-3.988954	0.365350
-18.485261	-0.917729	0.370355
-18.904542	-5.461101	0.375360
-19.096932	-5.472007	0.380365
-20.239546	-0.186265	0.385370
-19.739340	-9.146210	0.390374
-19.861228	2.575506	0.395379
-19.945472	-7.271376	0.400384
-19.870154	-4.519752	0.405389
-20.924323	6.725087	0.410394
-21.074229	-5.246199	0.415398
-21.534283	5.344195	0.420403
-21.656400	3.353627	0.425408
-21.593635	1.478350	0.430413
-21.330087	5.021752	0.435418
-22.026991	5.086621	0.440422
-22.346730	8.227540	0.445427
-22.604571	5.138101	0.450432
-22.962954	-6.660791	0.455437
-23.240820	4.934712	0.460442
-23.354589	-5.229109	0.465446
-24.377807	1.652532	0.470451
-24.781269	1.283235	0.475456
-23.951597	-5.215116	0.480461
-24.773606	4.203115	0.485466
-24.500916	0.596489	0.490470
-24.605883	2.661969	0.495475
-24.840309	2.444144	0.500480
-25.127951	-2.137687	0.505485
-26.065736	5.365752	0.510490
-25.813584	-10.262998	0.515494
-26.499180	-0.460154	0.520499
-26.561220	2.069416	0.525504
-26.378327	-7.356960	0.530509
-26.942854	5.615613	0.535514
-27.257370	-5.533459	0.540518
-27.291963	5.257146	0.545523
-27.603448	8.049982	0.550528
-27.548729	7.816652	0.555533
-28.732463	5.832854	0.560538
-28.855584	6.011316	0.565542
-29.248169	6.113017	0.570547
-29.003236	5.249562	0.575552
-29.427782	7.445915	0.580557
-29.646611	9.808560	0.585562
-29.308558	-1.458662	0.590566
-29.880276	0.697430	0.595571
-29.633380	0.053476	0.600576
-30.287581	-5.737243	0.605581
-30.955247	2.487134	0.610586
-30.501203	-1.439716	0.615590
-31.032586	4.151122	0.620595
-31.696652	-2.340061	0.625600
-32.467903	3.717478	0.630605
-32.579039	4.592500	0.635610
-31.996638	0.766460	0.640614
-32.656632	-5.179187	0.645619
-32.956638	2.280983	0.650624
-32.197467	-0.022435	0.655629
-32.755430	3.353639	0.660634
-33.113394	5.010472	0.665638
-33.738257	-3.034498	0.670643
-33.779670	7.547478	0.675648
-33.765788	0.169073	0.680653
-34.803242	3.153037	0.685658
-35.004025	-1.366272	0.690662
-35.766495	8.982545	0.695667
-35.776950	3.971222	0.700672
-35.586542	-1.838739	0.705677
-35.910492	5.164842	0.710682
-35.665004	-7.415815	0.715686
-35.811435	3.165067	0.720691
-36.282930	3.673364	0.725696
-36.464719	0.731122	0.730701
-36.934075	12.378394	0.735706
-37.335017	-1.349834	0.740710
-37.966518	0.686355	0.745715
-38.128450	-0.708167	0.750720
-37.563314	-10.354369	0.755725
-37.989655	-0.294876	0.760730
-38.586919	-1.883032	0.765734
-38.961312	2.640197	0.770739
-38.711412	-0.018216	0.775744
-38.914141	2.890924	0.780749
-39.638955	5.415232	0.785754
-40.031356	-5.587692	0.790758
-40.250040	4.564365	0.795763
-40.826986	0.639789	0.800768
-40.651628	-11.771342	0.805773
-40.880863	5.102567	0.810778
-40.577584	-1.117070	0.815782
-40.541871	-6.746802	0.820787
-41.341921	-6.196912	0.825792
-41.811895	-15.957365	0.830797
-42.357855	1.550922	0.835802
-42.164197	2.945562	0.840806
-42.419402	-1.214437	0.845811
-42.675297	0.781610	0.850816
-42.774824	-9.532571	0.855821
-43.478929	-0.657459	0.860826
-43.723426	-7.939825	0.865830
-43.898305	-4.407016	0.870835
-43.864862	-7.876783	0.875840
-43.656070	-2.255664	0.880845
-44.604011	4.815733	0.885850
-45.144772	-6.626648	0.890854
-45.275373	-5.321565	0.895859
-45.464164	-5.945977	0.900864
-45.357940	-7.867154	0.905869
-45.738721	-8.019603	0.910874
-45.537524	-5.592599	0.915878
-46.038270	-6.731886	0.920883
-46.813925	-2.207861	0.925888
-46.463024	-7.434748	0.930893
-47.032200	4.057236	0.935898
-46.909397	-7.648582	0.940902
-47.801247	-9.815078	0.945907
-48.168348	-2.253380	0.950912
-48.284503	-9.413029	0.955917
-48.706863	1.684947	0.960922
-48.475710	-9.011775	0.965926
-48.823243	-10.648547	0.970931
-48.807219	-0.186433	0.975936
-48.535727	1.478239	0.980941
-49.420352	6.588103	0.985946
-50.304779	-3.611190	0.990950
-50.259676	2.088052	0.995955
-50.219229	1.423756	1.000960
-50.125069	-9.699120	1.005965
-50.524024	-2.745627	1.010970
-50.737631	-8.253994	1.015974
-51.413095	-7.581944	1.020979
-52.063415	-0.913049	1.025984
-51.540981	-5.674138	1.030989
-51.995047	1.399023	1.035994
-52.042200	-8.708774	1.040998
-52.941191	-0.974197	1.046003
-53.662914	5.265537	1.051008
-52.886277	0.318333	1.056013
-53.275362	-3.520847	1.061018
-53.411463	-5.054241	1.066022
-53.321465	-2.203828	1.071027
-53.572589	8.243502	1.076032
-54.445734	-2.084747	1.081037
-55.008944	9.353956	1.086042
-55.245904	-2.294426	1.091046
-55.137961	-0.438781	1.096051
-55.323363	10.110300	1.101056
-55.055551	-1.192999	1.106061
-55.431785	1.701572	1.111066
-56.014604	0.364193	1.116070
-56.734923	3.219075	1.121075
-56.764869	-5.483628	1.126080
-56.755334	-0.526555	1.131085
-56.757570	-1.694843	1.136090
-56.781025	-7.773138	1.141094
-57.482353	2.412976	1.146099
-58.434315	-4.752175	1.151104
-58.397739	-8.179049	1.156109
-58.303440	-2.266385	1.161114
-58.501958	3.882029	1.166118
-58.413276	-0.863983	1.171123
-58.817911	4.500958	1.176128
-59.463741	-9.647511	1.181133
-59.561526	1.055914	1.186138
-59.846068	-7.812845	1.191142
-60.001879	-4.073640	1.196147
-59.984376	-3.841792	1.201152
-60.169448	-12.951646	1.206157
-61.195611	-3.827045	1.211162
-61.343523	2.960793	1.216166
-61.591859	-1.340056	1.221171
-61.402036	-3.432010	1.226176
-61.182426	-7.847156	1.231181
-62.059357	0.720637	1.236186
-62.639334	-4.887253	1.241190
-62.952427	1.717492	1.246195
-63.784477	-0.519326	1.251200
-63.036380	-10.215283	1.256205
-63.519219	-3.265803	1.261210
-63.539396	-10.795022	1.266214
-63.301827	-10.158725	1.271219
-63.458882	2.179374	1.276224
-63.785150	-5.114458	1.281229
-64.920794	-4.819963	1.286234
-64.867116	-5.091205	1.291238
-65.307997	2.823354	1.296243
-65.142466	-2.720810	1.301248
-65.034623	-5.194980	1.306253
-66.080558	-0.569978	1.311258
-66.137813	-1.754771	1.316262
-66.788657	-2.511935	1.321267
-66.903151	1.886986	1.326272
-66.886873	-0.816850	1.331277
-66.593184	0.715669	1.336282
-66.648296	-11.062982	1.341286
-67.244640	-4.946706	1.346291
-68.113031	-3.841605	1.351296
-67.815024	-2.464907	1.356301
-68.355939	4.329658	1.361306
-68.615126	-0.126264	1.366310
-69.277499	4.778923	1.371315
-69.484848	8.034556	1.376320
-69.148395	-3.482614	1.381325
-69.928166	2.964299	1.386330
-69.682854	-1.435783	1.391334
-69.520843	6.014476	1.396339
-70.403618	-2.055688	1.401344
-70.686674	-3.563862	1.406349
-71.216823	-0.928846	1.411354
-71.531470	-5.999901	1.416358
-71.302286	-0.663766	1.421363
-71.326537	-3.614829	1.426368
-70.898459	-4.780654	1.431373
-71.978360	6.641136	1.436378
-72.266173	3.399609	1.441382
-72.258965	5.491433	1.446387
-72.800653	1.021104	1.451392
-72.728305	-6.457984	1.456397
-73.784491	4.187115	1.461402
-73.829252	-4.422746	1.466406
-73.870239	-8.848440	1.471411
-73.895479	5.671536	1.476416
-73.758318	-6.094684	1.481421
-74.591721	0.506972	1.486426
-75.220229	8.122395	1.491430
-75.598722	-4.019855	1.496435
-75.796985	-3.658208	1.501440
-75.663658	-7.060713	1.506445
-75.897934	-1.966023	1.511450
-75.914713	-7.293596	1.516454
-75.701189	-8.903661	1.521459
-76.618671	1.482765	1.526464
-77.287473	-3.947755	1.531469
-77.177222	4.611818	1.536474
-77.571278	-0.874640	1.541478
-77.630406	0.465133	1.546483
-77.829606	5.445069	1.551488
-77.342891	1.976510	1.556493
-78.562269	-2.007408	1.561498
-78.809822	4.042599	1.566502
-78.714889	0.033565	1.571507
-78.979041	-0.069796	1.576512
-78.636387	-2.483153	1.581517
-79.218592	1.120926	1.586522
-80.132162	3.693592	1.591526
-80.276051	2.174912	1.596531
-80.980893	5.693217	1.601536
-80.774424	-6.958304	1.606541
-80.927354	-2.125181	1.611546
-80.827614	-8.627891	1.616550
-80.526790	-11.874527	1.621555
-81.931151	-2.587789	1.626560
-81.969594	2.550516	1.631565
-82.309622	3.383672	1.636570
-82.432671	-6.070575	1.641574
-82.123142	-6.539454	1.646579
-83.066297	2.870706	1.651584
-83.673643	-6.197165	1.656589
-83.839431	-1.363286	1.661594
-84.083464	-10.216277	1.666598
-83.849620	-1.743362	1.671603
-84.025949	2.771016	1.676608
-84.173900	-6.641794	1.681613
-84.162356	-3.454522	1.686618
-84.649167	2.577641	1.691622
-84.741905	-5.206307	1.696627
-85.279455	7.751523	1.701632
-85.130126	-4.576349	1.706637
-86.087821	3.891607	1.711642
-86.517292	0.989560	1.716646
-87.013882	-5.302323	1.721651
-87.185451	0.310395	1.726656
-86.685287	0.700574	1.731661
-87.052595	-0.238894	1.736666
-87.463912	1.617631	1.741670
-87.092344	0.726214	1.746675
-87.321157	2.359212	1.751680
-88.103380	-2.363963	1.756685
-88.678550	-8.091833	1.761690
-89.150560	-0.190845	1.766694
-88.650427	-1.359180	1.771699
-89.174046	4.243199	1.776704
-89.149220	-10.456408	1.781709
-89.463130	-7.970016	1.786714
-90.266513	-2.018029	1.791718
-89.995133	-5.394746	1.796723
-90.575265	-0.400420	1.801728
-90.374759	-4.353795	1.806733
-90.457821	-7.946664	1.811738
-91.114808	-4.684953	1.816742
-91.445696	-13.199879	1.821747
-92.063705	-7.982196	1.826752
-91.739936	-16.318842	1.831757
-92.081056	-6.134600	1.836762
-92.059036	-7.642381	1.841766
-92.624147	-10.701840	1.846771
-93.671138	-5.495519	1.851776
-93.320010	-20.474518	1.856781
-93.629137	-4.141645	1.861786
-94.192609	-17.982729	1.866790
-93.904065	-15.753572	1.871795
-93.794578	-12.122607	1.876800
-93.758079	-17.042469	1.881805
-94.306128	-14.324163	1.886810
-95.347656	-3.963685	1.891814
-94.804964	-10.874708	1.896819
-95.236059	-4.573377	1.901824
-94.919927	-14.123324	1.906829
-95.887982	-15.426643	1.911834
-96.577809	-9.326792	1.916838
-96.920025	-11.520716	1.921843
-97.045088	-7.686577	1.926848
-97.047673	-15.032436	1.931853
-97.003844	-10.616625	1.936858
-96.736089	-7.238901	1.941862
-97.101967	-19.575826	1.946867
-97.620623	-12.828971	1.951872
-98.091283	-11.407165	1.956877
-98.218272	-16.789029	1.961882
-98.276433	-7.641838	1.966886
-99.440188	-10.076082	1.971891
-99.921204	-7.009777	1.976896
-99.500405	-11.948934	1.981901
-99.640538	3.864104	1.986906
-100.537476	-1.030421	1.991910
-100.194394	-0.325434	1.996915
-100.215845	-6.148829	2.006912
-100.277193	-5.793585	2.016909
-99.356726	-10.113384	2.026906
-98.996670	-3.845576	2.036902
-98.558400	-7.348816	2.046899
-98.434630	-1.250371	2.056896
-97.383323	-3.279408	2.066893
-97.454312	-9.425225	2.076890
-96.264841	-7.152134	2.086886
-95.854793	1.094856	2.096883
-95.721590	-6.137436	2.106880
-95.755102	-11.501916	2.116877
-94.880012	-12.911869	2.126874
-93.932677	-10.246231	2.136870
-93.067974	-16.692630	2.146867
-92.863004	-11.449393	2.156864
-93.066571	-4.453639	2.166861
-92.476453	-8.697967	2.176858
-91.366121	-11.193232	2.186854
-91.242436	1.437134	2.196851
-90.434632	-0.652780	2.206848
-89.994114	-8.487815	2.216845
-89.842540	-6.769080	2.226842
-88.959872	-6.183120	2.236838
-88.675385	-9.154781	2.246835
-88.211517	6.485725	2.256832
-87.401131	1.785502	2.266829
-86.723356	-2.195400	2.276826
-86.547450	1.680458	2.286822
-86.314215	-1.028593	2.296819
-85.409579	-1.717140	2.306816
-85.258054	-0.237274	2.316813
-84.916579	1.927451	2.326810
-83.638826	-0.534396	2.336806
-83.746636	3.684808	2.346803
-83.201848	2.923111	2.356800
-82.275889	4.815609	2.366797
-82.040132	1.171569	2.376794
-81.962055	-4.078690	2.386790
-80.759246	0.219989	2.396787
-80.787012	-0.741514	2.406784
-80.189446	-0.854821	2.416781
-79.346994	-0.030012	2.426778
-78.850520	0.790076	2.436774
-79.033529	-3.558674	2.446771
-78.013006	-1.941126	2.456768
-77.730706	1.307500	2.466765
-77.150382	-3.370081	2.476762
-76.257793	0.194383	2.486758
-76.171680	5.481098	2.496755
-75.778137	2.986448	2.506752
-74.748555	-0.456830	2.516749
-74.077801	-4.597594	2.526746
-74.127332	-0.731875	2.536742
-74.027775	-3.978060	2.546739
-73.224637	-7.189664	2.556736
-72.254135	-7.456055	2.566733
-71.787829	0.721522	2.576730
-71.311154	-3.291149	2.586726
-71.307263	0.556007	2.596723
-70.825311	-3.135282	2.606720
-70.121982	-3.512360	2.616717
-69.645889	-7.275780	2.626714
-68.604032	-4.311887	2.636710
-68.149726	-2.567408	2.646707
-68.369165	-3.873443	2.656704
-68.134348	2.252385	2.666701
-66.845444	-4.756717	2.676698
-66.596821	-5.471744	2.686694
-65.868405	1.907098	2.696691
-65.333629	-0.550371	2.706688
-65.426603	6.122131	2.716685
-64.282001	-1.648376	2.726682
-63.612924	-0.628376	2.736678
-63.694704	-0.363193	2.746675
-63.438450	2.081847	2.756672
-62.464268	3.042828	2.766669
-62.085530	-0.642960	2.776666
-61.642922	0.940854	2.786662
-60.740130	-5.711239	2.796659
-60.624258	-1.678990	2.806656
-59.866882	-2.953188	2.816653
-59.125700	-1.118089	2.826650
-58.947811	-4.041602	2.836646
-58.838996	-1.789987	2.846643
-58.376098	1.052618	2.856640
-57.490538	2.302183	2.866637
-57.016506	2.994020	2.876634
-55.821257	-0.498134	2.886630
-55.792797	-1.248678	2.896627
-55.466663	3.777633	2.906624
-55.354521	0.992096	2.916621
-54.809225	6.316878	2.926618
-54.043048	-1.855038	2.936614
-53.433640	4.223339	2.946611
-52.711884	1.945807	2.956608
-52.676554	1.663578	2.966605
-52.180001	0.562751	2.976602
-51.370682	-2.901797	2.986598
-51.062521	5.695861	2.996595
-50.675711	6.772667	3.006592
-49.458282	3.011473	3.016589
-49.082156	-0.510874	3.026586
-49.011653	1.256313	3.036582
-48.862355	-3.437141	3.046579
-48.181421	-1.734482	3.056576
-47.727451	-1.636802	3.066573
-46.573347	-0.911411	3.076570
-46.403858	-1.005713	3.086566
-46.154997	-2.675107	3.096563
-45.492554	-1.092270	3.106560
-44.781143	2.119010	3.116557
-44.628845	-2.315121	3.126554
-44.091851	-7.392319	3.136550
-43.139569	-9.550893	3.146547
-43.116177	6.657796	3.156544
-42.762105	3.940119	3.166541
-42.010282	-0.956439	3.176538
-41.653856	1.400622	3.186534
-40.492566	0.257261	3.196531
-40.330976	0.944135	3.206528
-40.161997	-2.206106	3.216525
-39.733074	-1.876249	3.226522
-38.722859	-3.158095	3.236518
-38.401968	-4.854873	3.246515
-38.106088	-2.246497	3.256512
-37.012669	-0.651922	3.266509
-36.636784	-3.128616	3.276506
-36.634871	-1.082695	3.286502
-36.521506	-2.503924	3.296499
-35.414509	-2.911743	3.306496
-35.154228	-2.025514	3.316493
-34.126656	-2.690820	3.326490
-33.891886	-4.099036	3.336486
-33.472469	1.700129	3.346483
-32.807246	-0.853312	3.356480
-32.012912	-0.669159	3.366477
-31.893320	0.955907	3.376474
-32.128904	3.885386	3.386470
-30.968317	-3.132606	3.396467
-30.484923	-2.115520	3.406464
-29.634751	0.824137	3.416461
-29.182862	2.869352	3.426458
-28.960153	-4.569282	3.436454
-28.810341	-3.296195	3.446451
-27.847845	-8.643288	3.456448
-27.277324	-5.250320	3.466445
-27.162325	-4.978925	3.476442
-26.442286	0.632552	3.486438
-25.866518	-2.956766	3.496435
-25.591900	2.464191	3.506432
-24.441163	-7.157497	3.516429
-24.051038	-3.973221	3.526426
-24.065155	-0.355230	3.536422
-23.770017	-0.424776	3.546419
-22.995638	-7.055713	3.556416
-22.447198	5.181407	3.566413
-21.998923	0.255092	3.576410
-20.858804	-3.480991	3.586406
-20.857856	2.907187	3.596403
-20.912462	2.921070	3.606400
-19.825726	5.211070	3.616397
-19.166794	-1.168517	3.626394
-19.074281	-2.014275	3.636390
-18.429081	-1.341995	3.646387
-17.981388	-3.132364	3.656384
-17.736952	-0.914750	3.666381
-16.217282	1.362757	3.676378
-16.650654	-11.543213	3.686374
-16.203993	-0.884071	3.696371
-15.043535	3.657589	3.706368
-14.605333	-1.016712	3.716365
-14.725590	-1.682866	3.726362
-14.074033	1.221842	3.736358
-13.296950	-5.599421	3.746355
-12.889765	0.572447	3.756352
-12.345863	-1.061621	3.766349
-11.502877	-2.135465	3.776346
-11.202821	1.255639	3.786342
-11.233232	3.001667	3.796339
-10.658958	-4.325287	3.806336
-9.632817	-5.798266	3.816333
-9.551383	0.870734	3.826330
-8.827708	-2.752851	3.836326
-8.122568	-7.086432	3.846323
-8.143067	-7.239249	3.856320
-7.253827	0.991726	3.866317
-6.540048	-3.622675	3.876314
-6.391785	1.305768	3.886310
-6.074020	1.557290	3.896307
-5.159660	1.822660	3.906304
-4.815323	7.893938	3.916301
-4.613173	6.373977	3.926298
-4.144585	9.777969	3.936294
-4.023125	24.921412	3.946291
-3.397362	35.931358	3.956288
-2.789739	49.471824	3.966285
-2.104532	59.698759	3.976282
-1.577460	81.697006	3.986278
-1.530486	88.425713	3.996275
-0.858317	95.376317	4.006272
-0.255584	121.459360	4.016269
0.000000	128.060790	4.021274
-0.067504	142.689754	4.026278
0.282980	139.198826	4.031283
0.320734	148.065551	4.036288
0.286904	151.301249	4.041293
0.723560	164.894102	4.046298
0.521247	178.926278	4.051302
1.158566	177.071310	4.056307
1.212733	185.676229	4.061312
1.105297	183.149212	4.066317
1.292311	168.800157	4.071322
0.822077	168.200811	4.076326
0.458610	157.957222	4.081331
0.718240	169.085809	4.086336
1.154001	183.396923	4.091341
1.108209	169.603381	4.096346
0.799999	183.974226	4.101350
1.229095	180.901000	4.106355
1.397042	174.028318	4.111360
0.936256	183.402396	4.116365
1.279328	176.444166	4.121370
1.191404	171.197419	4.126374
0.929011	178.466716	4.131379
1.278575	177.011622	4.136384
0.943651	176.570541	4.141389
0.955256	186.706540	4.146394
1.217515	179.152574	4.151398
1.273281	177.985879	4.156403
1.164291	176.853477	4.161408
0.836114	176.097120	4.166413
1.108754	176.782262	4.171418
0.939277	186.442793	4.176422
1.070093	182.459122	4.181427
1.318911	182.166886	4.186432
0.959027	181.512294	4.191437
1.530602	178.921151	4.196442
0.952957	182.552525	4.201446
1.070682	181.145243	4.206451
0.812374	183.504016	4.211456
1.003445	182.501507	4.216461
0.903997	174.583401	4.221466
1.198357	178.152508	4.226470
1.479860	193.852845	4.231475
1.312785	188.688711	4.236480
1.368328	200.643538	4.241485
1.658078	191.705438	4.246490
1.179003	188.201432	4.251494
1.261870	178.889446	4.256499
1.434930	191.753777	4.261504
1.444679	206.619587	4.266509
2.043293	197.897135	4.271514
1.549728	188.542432	4.276518
1.575548	181.934907	4.281523
1.391121	179.732080	4.286528
1.342698	185.902385	4.291533
1.472707	179.307341	4.296538
1.224150	183.828449	4.301542
1.137119	179.467972	4.306547
1.286163	190.370856	4.311552
1.683769	205.929559	4.316557
2.080602	206.360810	4.321562
1.508966	200.565161	4.326566
1.568655	190.577404	4.331571
1.489499	197.293318	4.336576
1.559817	201.881998	4.341581
1.730661	203.085289	4.346586
1.659428	211.539190	4.351590
1.555689	208.204460	4.356595
1.824173	196.012507	4.361600
1.385753	206.650749	4.366605
2.058645	209.064898	4.371610
1.739992	206.339541	4.376614
1.570032	191.164368	4.381619
1.931102	201.679578	4.386624
1.634070	200.070495	4.391629
1.767528	187.290247	4.396634
1.847204	191.443432	4.401638
1.503433	196.733790	4.406643
1.782943	203.949529	4.411648
1.668102	217.755659	4.416653
1.975707	211.165416	4.421658
1.902099	220.021882	4.426662
1.832790	213.096072	4.431667
1.942145	204.558937	4.436672
1.587561	211.532380	4.441677
2.047704	207.441075	4.446682
1.866023	221.209971	4.451686
2.009416	206.161876	4.456691
2.235250	204.902184	4.461696
1.770470	196.034841	4.466701
1.719725	191.982286	4.471706
1.641362	202.929293	4.476710
2.131993	207.933944	4.481715
2.089700	213.764420	4.486720
1.843968	213.685024	4.491725
2.095031	208.395729	4.496730
2.382952	198.074227	4.501734
1.678110	200.436385	4.506739
2.278128	200.133130	4.511744
1.817971	212.065550	4.516749
2.110434	210.202781	4.521754
2.244119	220.090195	4.526758
2.244544	219.361501	4.531763
2.174401	202.833578	4.536768
1.584758	199.712424	4.541773
2.286237	204.195401	4.546778
2.178055	217.498802	4.551782
2.205980	209.619495	4.556787
2.357288	201.113672	4.561792
2.233774	213.357766	4.566797
1.908200	190.757342	4.571802
2.152721	203.689724	4.576806
2.129845	213.337152	4.581811
2.591092	212.370243	4.586816
2.093328	217.683641	4.591821
2.369301	214.920022	4.596826
2.001746	206.390134	4.601830
2.428207	212.427838	4.606835
2.372073	212.384414	4.611840
2.146523	217.838451	4.616845
2.221717	206.410728	4.621850
2.437194	213.814123	4.626854
2.245530	223.213544	4.631859
2.271019	212.634128	4.636864
2.240066	216.623374	4.641869
2.314978	208.819137	4.646874
2.138161	212.022375	4.651878
2.273853	221.745275	4.656883
2.272798	204.722398	4.661888
2.254693	224.400493	4.666893
2.398987	215.657448	4.671898
2.157436	219.148110	4.676902
2.164421	225.738619	4.681907
1.922936	223.058645	4.686912
1.998318	225.407936	4.691917
2.529640	234.914712	4.696922
2.482272	238.847886	4.701926
2.605369	242.726086	4.706931
2.762955	241.328156	4.711936
2.512786	248.289192	4.716941
3.077032	242.747533	4.721946
2.615891	221.333277	4.726950
2.491449	213.572239	4.731955
2.308056	217.469805	4.736960
2.577784	238.550081	4.741965
2.945849	240.388173	4.746970
2.707851	226.351841	4.751974
2.208720	224.468509	4.756979
2.573595	231.137269	4.761984
2.672838	246.550643	4.766989
2.708625	246.893712	4.771994
2.888708	254.233943	4.776998
2.339671	252.222939	4.782003
2.890929	242.709723	4.787008
2.541856	250.598094	4.792013
2.782947	249.552338	4.797018
2.583862	243.350397	4.802022
2.628457	246.007914	4.807027
3.060565	230.387290	4.812032
2.907635	252.047159	4.817037
2.724529	239.211152	4.822042
3.138732	246.565151	4.827046
2.760090	242.048099	4.832051
3.246925	240.983793	4.837056
2.864162	245.267339	4.842061
2.847317	230.117392	4.847066
3.027217	228.467705	4.852070
2.721478	230.141334	4.857075
2.701417	234.885154	4.862080
2.569196	241.786325	4.867085
2.703281	241.799688	4.872090
2.515892	249.516339	4.877094
2.236994	260.057455	4.882099
2.703309	249.174844	4.887104
2.955564	253.266799	4.892109
3.161258	248.008516	4.897114
2.891794	254.162507	4.902118
2.802912	254.840456	4.907123
2.921758	254.934693	4.912128
3.015302	276.106269	4.917133
3.328224	279.680801	4.922138
3.160056	265.623551	4.927142
2.887120	266.810037	4.932147
3.203618	256.977871	4.937152
3.099615	271.617957	4.942157
3.156031	270.106601	4.947162
3.183880	269.691648	4.952166
3.179236	265.458545	4.957171
3.331683	267.053451	4.962176
3.150743	253.493250	4.967181
3.261664	253.449684	4.972186
3.026418	249.623143	4.977190
2.921780	254.040232	4.982195
3.460350	266.311264	4.987200
3.227455	281.613924	4.992205
3.056898	277.249148	4.997210
3.419332	281.867440	5.002214
3.192638	287.774179	5.007219
3.385893	285.385026	5.012224
3.100589	289.011638	5.017229
3.358535	281.286264	5.022234
3.343981	271.613901	5.027238
3.388941	279.150259	5.032243
3.501996	273.637412	5.037248
3.435394	276.031624	5.042253
3.602156	264.886612	5.047258
3.434859	261.333330	5.052262
2.877249	252.815669	5.057267
3.259073	268.321805	5.062272
3.194692	276.300408	5.067277
3.540796	284.569340	5.072282
3.502137	276.584442	5.077286
3.034938	285.119397	5.082291
3.381420	278.752953	5.087296
3.185047	283.142477	5.092301
3.238271	282.951621	5.097306
3.193661	277.591867	5.102310
3.121256	279.511665	5.107315
3.257101	276.858353	5.112320
3.331910	293.499506	5.117325
4.002396	304.045840	5.122330
3.692146	293.374965	5.127334
3.578227	290.762180	5.132339
3.604391	283.312923	5.137344
3.499002	289.187857	5.142349
3.556156	295.186143	5.147354
3.516679	292.276822	5.152358
3.839975	309.856455	5.157363
3.927352	297.547315	5.162368
3.667997	291.899425	5.167373
3.260225	283.897735	5.172378
3.659583	290.736812	5.177382
3.724745	302.818979	5.182387
3.959460	295.778066	5.187392
3.844955	309.710911	5.192397
3.659276	296.936458	5.197402
3.726143	296.849303	5.202406
3.664580	302.474629	5.207411
3.861087	306.024117	5.212416
3.617452	309.155404	5.217421
3.866104	308.160879	5.222426
3.881562	304.151162	5.227430
3.433941	299.639639	5.232435
3.651840	310.726129	5.237440
3.512230	310.284545	5.242445
3.576843	311.374670	5.247450
3.754357	309.823842	5.252454
3.695893	305.002737	5.257459
4.043994	303.854336	5.262464
3.727300	313.494425	5.267469
4.060375	313.381964	5.272474
4.112177	307.676821	5.277478
3.846755	310.259982	5.282483
3.954940	304.775758	5.287488
4.049532	312.535356	5.292493
3.969904	309.099112	5.297498
4.155802	311.785841	5.302502
3.861542	313.640894	5.307507
4.235308	308.442269	5.312512
3.735934	320.024903	5.317517
3.782987	310.009174	5.322522
3.785201	312.322491	5.327526
3.966343	327.967620	5.332531
4.268579	332.075364	5.337536
4.190353	331.307840	5.342541
4.415457	327.004957	5.347546
4.372401	320.888544	5.352550
4.286038	311.995726	5.357555
4.231243	304.811321	5.362560
4.172221	314.256631	5.367565
4.112939	308.756237	5.372570
4.208228	318.974712	5.377574
4.066017	310.650228	5.382579
4.191169	306.623066	5.387584
4.025989	316.480694	5.392589
3.987741	313.944917	5.397594
4.209182	335.644103	5.402598
3.906766	345.383664	5.407603
4.039807	339.629485	5.412608
4.150384	346.819499	5.417613
4.153278	346.824675	5.422618
4.459899	341.413422	5.427622
4.461161	343.252311	5.432627
4.543269	336.690223	5.437632
4.597563	339.353248	5.442637
4.386068	343.642294	5.447642
4.337160	346.072648	5.452646
4.131093	342.137435	5.457651
4.620685	341.054905	5.462656
4.385499	344.166443	5.467661
4.419713	343.696556	5.472666
4.241311	336.834014	5.477670
4.312898	349.728565	5.482675
4.468574	337.805080	5.487680
4.410667	343.323450	5.492685
4.528696	339.861842	5.497690
4.526759	344.949599	5.502694
4.219324	336.086016	5.507699
4.230859	340.255698	5.512704
4.262807	349.931197	5.517709
4.302732	347.839252	5.522714
4.440109	346.382709	5.527718
4.251178	367.618335	5.532723
4.920467	365.920242	5.537728
4.745483	371.775596	5.542733
4.764329	367.744579	5.547738
4.660081	357.188011	5.552742
4.357087	351.821650	5.557747
4.597322	364.861638	5.562752
4.825174	371.734193	5.567757
4.802876	377.311975	5.572762
5.225219	352.206531	5.577766
4.462981	357.781204	5.582771
4.341444	344.656040	5.587776
4.456317	360.359380	5.592781
5.105789	367.914488	5.597786
4.932189	368.157387	5.602790
4.697692	354.244481	5.607795
4.660745	366.037603	5.612800
4.874174	373.670917	5.617805
4.667520	373.180289	5.622810
5.297439	373.610887	5.627814
4.550031	357.353639	5.632819
4.722005	355.251188	5.637824
4.938032	380.042005	5.642829
4.780901	377.703976	5.647834
5.093857	376.756971	5.652838
5.084362	375.718721	5.657843
4.917689	364.826398	5.662848
4.795940	360.012835	5.667853
4.719668	364.274278	5.672858
4.986270	374.437871	5.677862
5.005639	374.089445	5.682867
4.922332	380.700159	5.687872
4.640163	378.296284	5.692877
5.021215	369.411578	5.697882
4.974068	369.813033	5.702886
4.891268	384.286110	5.707891
5.318163	376.572467	5.712896
5.034747	384.365927	5.717901
4.688626	382.022409	5.722906
5.196351	383.509924	5.727910
4.859618	382.920740	5.732915
4.953146	387.180013	5.737920
5.096328	377.887481	5.742925
4.908371	385.822153	5.747930
4.957260	376.858863	5.752934
4.728065	387.191310	5.757939
5.170932	377.650444	5.762944
5.177310	385.799088	5.767949
5.022903	377.095145	5.772954
5.210792	380.281999	5.777958
5.059613	380.429805	5.782963
4.872830	393.295312	5.787968
4.914679	409.701911	5.792973
5.300931	413.074053	5.797978
5.397255	418.529516	5.802982
5.151153	419.004300	5.807987
5.141292	407.334819	5.812992
5.180182	418.316954	5.817997
5.577363	405.768762	5.823002
5.711661	413.773414	5.828006
5.130587	414.907135	5.833011
5.444037	406.822398	5.838016
5.172605	404.447320	5.843021
5.254956	408.383247	5.848026
5.954586	410.896587	5.853030
5.392955	413.571626	5.858035
5.541715	403.498674	5.863040
5.320836	411.137105	5.868045
5.237314	411.362269	5.873050
5.216923	412.770823	5.878054
4.914614	411.798214	5.883059
5.559436	412.979766	5.888064
5.294710	410.671456	5.893069
5.306798	407.931144	5.898074
5.808675	401.983615	5.903078
5.198645	408.001086	5.908083
5.359920	399.098430	5.913088
5.182461	401.673102	5.918093
5.139573	402.652045	5.923098
5.653063	413.623564	5.928102
5.655751	426.086218	5.933107
5.931276	423.370195	5.938112
5.622291	415.890742	5.943117
5.370846	407.522400	5.948122
5.753277	404.859650	5.953126
5.436094	420.349324	5.958131
5.488820	424.110998	5.963136
5.902050	429.753552	5.968141
5.808658	431.829991	5.973146
5.538673	430.777415	5.978150
5.683376	436.757849	5.983155
5.877557	439.041644	5.988160
5.633686	434.856153	5.993165
6.019892	440.537540	5.998170
6.042903	426.361538	6.003174
5.614745	416.001642	6.008179
5.553378	415.897125	6.013184
5.795994	422.135377	6.018189
5.932358	430.844186	6.023194
5.791819	438.199516	6.028198
5.709031	438.272609	6.033203
5.700199	435.909525	6.038208
5.774750	441.757961	6.043213
5.490426	435.265227	6.048218
5.370809	447.994504	6.053222
5.492588	447.800539	6.058227
5.530784	444.493669	6.063232
5.925180	442.239977	6.068237
5.410916	438.982118	6.073242
5.669460	443.458477	6.078246
5.731738	449.684487	6.083251
5.535285	452.273177	6.088256
5.698149	444.799936	6.093261
6.216742	451.877185	6.098266
6.114607	449.302868	6.103270
5.632531	445.852779	6.108275
5.559058	442.358057	6.113280
5.832334	435.060252	6.118285
5.617321	447.873270	6.123290
5.694539	443.927055	6.128294
5.658387	446.205131	6.133299
5.783344	461.331267	6.138304
6.117270	472.719062	6.143309
5.737286	461.276037	6.148314
6.004951	451.294588	6.153318
5.524011	451.875897	6.158323
6.093761	447.597588	6.163328
6.280944	441.310049	6.168333
5.785266	442.168895	6.173338
6.175939	443.958459	6.178342
5.918228	443.804091	6.183347
5.791534	434.337145	6.188352
6.005126	440.127539	6.193357
5.616981	444.247653	6.198362
6.130584	432.038846	6.203366
5.768671	443.711796	6.208371
5.988802	443.111348	6.213376
5.935714	444.524551	6.218381
6.028579	451.387611	6.223386
6.161646	440.802194	6.228390
5.775052	444.168816	6.233395
6.257777	434.003233	6.238400
5.856851	433.198964	6.243405
5.787728	424.710123	6.248410
5.583154	409.561998	6.253414
5.447616	429.475365	6.258419
5.812956	445.038292	6.263424
5.844572	442.432667	6.268429
5.879003	448.347172	6.273434
5.715738	443.795048	6.278438
5.741114	442.654303	6.283443
5.755147	437.286718	6.288448
5.709525	446.244237	6.293453
5.817858	448.526911	6.298458
6.216728	438.855975	6.303462
5.850835	449.207239	6.308467
6.078829	444.363931	6.313472
6.422046	434.962732	6.318477
5.940272	428.498086	6.323482
5.819181	421.406935	6.328486
5.299058	416.481972	6.333491
5.408314	422.797449	6.338496
5.781046	437.068955	6.343501
5.859270	451.093028	6.348506
5.908213	448.122606	6.353510
5.693421	452.610356	6.358515
5.983479	443.534911	6.363520
6.098470	448.193200	6.368525
5.791384	423.136468	6.373530
5.770135	421.050734	6.378534
5.491294	432.458658	6.383539
5.788047	436.888605	6.388544
6.222120	443.230020	6.393549
5.706668	441.452974	6.398554
5.973510	423.129871	6.403558
5.525693	421.464723	6.408563
5.754623	429.901804	6.413568
6.026058	424.755079	6.418573
5.849525	413.459821	6.423578
5.789810	418.521685	6.428582
5.493249	419.385716	6.433587
5.833951	440.638979	6.438592
5.903828	453.248947	6.443597
5.867468	449.131181	6.448602
6.120501	432.556200	6.453606
5.545788	429.804100	6.458611
5.530761	423.723835	6.463616
5.841856	441.578365	6.468621
5.438258	450.257156	6.473626
6.056438	449.621130	6.478630
5.994412	457.226073	6.483635
5.895579	449.329234	6.488640
5.825383	443.106381	6.493645
5.337794	442.897081	6.498650
6.076332	440.149874	6.503654
5.853761	449.073067	6.508659
6.294460	441.222909	6.513664
5.895799	433.789534	6.518669
5.617548	427.682770	6.523674
5.827237	419.252964	6.528678
5.809198	417.737986	6.533683
5.776457	424.116535	6.538688
5.879487	412.701003	6.543693
5.710391	425.933208	6.548698
5.582497	411.572140	6.553702
5.358194	418.328064	6.558707
5.634308	436.451057	6.563712
5.878483	443.203121	6.568717
5.984488	448.374203	6.573722
6.328822	438.878489	6.578726
5.733402	448.963218	6.583731
6.085394	447.038430	6.588736
6.146005	426.388866	6.593741
5.909213	424.581092	6.598746
5.922478	416.542301	6.603750
5.728095	424.623695	6.608755
6.058554	411.860442	6.613760
5.905673	412.987910	6.618765
5.749694	425.520549	6.623770
6.044231	413.814673	6.628774
5.792302	428.548959	6.633779
5.754271	417.694218	6.638784
5.835704	423.342588	6.643789
5.463376	425.229378	6.648794
5.889180	419.170166	6.653798
5.868697	426.472185	6.658803
5.866700	416.948606	6.663808
5.592045	417.539829	6.668813
5.630610	421.981903	6.673818
5.666799	417.881291	6.678822
5.393507	417.045744	6.683827
5.774043	428.440756	6.688832
5.959856	436.371933	6.693837
5.680301	430.964153	6.698842
5.700522	430.602166	6.703846
5.917758	435.027569	6.708851
5.833167	442.305718	6.713856
5.855739	442.856612	6.718861
5.750722	438.257512	6.723866
6.010506	429.349515	6.728870
5.737607	425.361848	6.733875
5.665199	425.047818	6.738880
5.969662	433.135295	6.743885
5.360692	429.876802	6.748890
6.200467	439.608506	6.753894
5.619551	445.614640	6.758899
5.578667	452.186562	6.763904
6.058828	447.822700	6.768909
5.730817	444.882574	6.773914
6.043254	452.395276	6.778918
5.499094	445.537439	6.783923
5.713046	449.185096	6.788928
6.116598	442.007123	6.793933
5.796519	441.430364	6.798938
5.923186	441.181318	6.803942
5.909705	441.387539	6.808947
5.574127	437.449557	6.813952
5.821606	442.711773	6.818957
5.915997	450.778332	6.823962
5.727810	448.832234	6.828966
6.106441	445.855555	6.833971
5.870237	433.567928	6.838976
5.597090	425.801902	6.843981
5.642806	433.152515	6.848986
5.678341	439.630822	6.853990
5.927296	446.809918	6.858995
5.503130	456.290160	6.864000
5.977957	460.008517	6.869005
5.621218	458.089645	6.874010
5.969292	453.152571	6.879014
5.857683	455.985472	6.884019
5.488421	464.094180	6.889024
5.911592	451.477497	6.894029
5.633375	457.784578	6.899034
5.825176	446.096545	6.904038
5.468679	461.389538	6.909043
5.734479	456.149807	6.914048
6.241289	451.359017	6.919053
5.730371	459.329255	6.924058
5.935114	457.435256	6.929062
5.927827	455.287602	6.934067
6.096017	460.199312	6.939072
6.061363	462.444384	6.944077
5.714885	454.567591	6.949082
5.829183	448.770705	6.954086
5.786278	460.001691	6.959091
5.848270	452.280584	6.964096
5.906463	440.088270	6.969101
5.748541	436.069648	6.974106
5.654778	434.874311	6.979110
5.918142	448.346836	6.984115
6.040818	452.865911	6.989120
5.698241	430.448327	6.994125
5.643425	437.356846	6.999130
5.728371	448.227942	7.004134
5.739002	458.242919	7.009139
5.673612	459.438137	7.014144
6.009244	459.292493	7.019149
5.666152	455.233209	7.024154
5.807211	453.631594	7.029158
5.727288	451.280917	7.034163
5.545462	452.479899	7.039168
5.846456	454.319694	7.044173
5.962679	465.421617	7.049178
6.295718	450.347287	7.054182
5.956416	447.896064	7.059187
5.607124	435.652887	7.064192
5.882378	447.729648	7.069197
5.684438	454.169019	7.074202
5.887056	455.814016	7.079206
5.693539	447.560937	7.084211
5.747781	456.695844	7.089216
6.013407	448.523918	7.094221
5.859559	453.673666	7.099226
5.842326	446.462231	7.104230
5.619002	437.032263	7.109235
5.401476	448.219448	7.114240
5.352296	439.876668	7.119245
5.281595	457.429015	7.124250
5.521078	451.156261	7.129254
5.252509	454.990688	7.134259
5.387449	450.834580	7.139264
5.789744	472.086134	7.144269
6.050352	474.394808	7.149274
5.803273	479.223010	7.154278
5.721313	473.885775	7.159283
5.952490	473.168245	7.164288
6.240001	470.188948	7.169293
5.871024	466.358138	7.174298
5.788511	456.746291	7.179302
5.830749	458.181143	7.184307
5.540295	459.059356	7.189312
5.894431	458.040775	7.194317
5.668238	455.833602	7.199322
5.742182	457.807636	7.204326
5.634730	446.031999	7.209331
5.834538	473.666717	7.214336
5.837606	472.448571	7.219341
5.683992	471.172010	7.224346
6.154521	469.257117	7.229350
6.001702	465.497334	7.234355
5.965890	463.105380	7.239360
5.851611	452.086674	7.244365
5.937282	442.684077	7.249370
5.904448	451.120873	7.254374
5.722382	449.807997	7.259379
5.577672	460.926650	7.264384
5.711830	447.090319	7.269389
5.966234	454.323965	7.274394
5.872839	456.725027	7.279398
5.795313	449.782715	7.284403
5.589048	450.619109	7.289408
5.964952	446.981016	7.294413
5.883594	457.669795	7.299418
5.660197	452.185974	7.304422
5.906894	447.127419	7.309427
5.804588	457.275623	7.314432
5.859799	461.746714	7.319437
5.713687	463.804688	7.324442
5.784723	458.678436	7.329446
5.813709	457.181094	7.334451
5.538311	453.464975	7.339456
5.619925	457.879381	7.344461
5.502549	458.584373	7.349466
5.927770	480.574312	7.354470
6.110904	483.935831	7.359475
5.804245	477.088231	7.364480
5.982450	461.710665	7.369485
5.570809	472.347596	7.374490
5.692989	466.112885	7.379494
5.916674	464.602123	7.384499
5.918078	475.493833	7.389504
5.972341	465.100682	7.394509
5.875113	461.803294	7.399514
6.132855	457.268803	7.404518
6.136685	459.370723	7.409523
5.909760	460.829794	7.414528
6.102050	450.956385	7.419533
6.054243	464.822238	7.424538
5.842761	452.789985	7.429542
5.759160	462.402077	7.434547
5.791891	463.221438	7.439552
5.851011	452.500106	7.444557
5.542563	464.983527	7.449562
5.849276	448.569118	7.454566
6.058181	458.904765	7.459571
5.755961	466.425120	7.464576
6.103503	453.025936	7.469581
5.858787	455.233502	7.474586
5.627213	455.746918	7.479590
5.837786	456.203810	7.484595
5.446836	459.460650	7.489600
5.914680	448.510552	7.494605
5.915782	457.941812	7.499610
5.845581	447.251847	7.504614
6.067399	457.198764	7.509619
5.575157	464.998559	7.514624
6.028858	455.662259	7.519629
5.775462	462.072567	7.524634
5.755325	453.508079	7.529638
5.868452	452.362218	7.534643
5.730799	463.655527	7.539648
6.177327	454.641684	7.544653
5.636698	466.402573	7.549658
5.759041	462.797152	7.554662
6.055798	452.520189	7.559667
5.802072	472.854836	7.564672
6.059817	460.004567	7.569677
5.778454	459.892019	7.574682
5.659193	464.731728	7.579686
5.974197	458.127127	7.584691
5.711696	470.983578	7.589696
5.916936	447.561635	7.594701
5.941303	463.929559	7.599706
5.351979	453.275164	7.604710
5.897633	450.349656	7.609715
5.531906	457.575480	7.614720
5.937485	452.118534	7.619725
5.975098	455.448587	7.624730
5.989235	449.605006	7.629734
5.962671	445.664990	7.634739
5.839048	461.267573	7.639744
5.935349	449.181991	7.644749
5.609321	455.062681	7.649754
5.855128	454.227673	7.654758
6.147366	454.314008	7.659763
5.653126	453.634771	7.664768
5.788936	445.285313	7.669773
5.782488	456.888925	7.674778
5.640160	436.913635	7.679782
5.700039	440.063960	7.684787
5.685489	454.673563	7.689792
5.694106	454.637530	7.694797
5.972352	454.829004	7.699802
5.810349	461.468818	7.704806
5.889754	454.528835	7.709811
5.714605	457.437420	7.714816
6.000488	451.491834	7.719821
6.010638	454.244703	7.724826
5.892742	454.777901	7.729830
6.075845	434.217883	7.734835
5.463710	443.422898	7.739840
5.532745	438.772172	7.744845
5.333007	455.607533	7.749850
5.535180	441.306422	7.754854
5.625796	453.813091	7.759859
5.618919	459.994754	7.764864
5.813240	460.147094	7.769869
5.969282	456.619350	7.774874
6.094451	454.805081	7.779878
5.988402	441.862362	7.784883
5.625468	456.681826	7.789888
5.864244	447.964386	7.794893
5.725872	446.923479	7.799898
5.577200	454.457575	7.804902
6.016617	452.701974	7.809907
5.904584	461.290273	7.814912
5.770382	440.508494	7.819917
5.676839	453.999107	7.824922
5.582549	448.488893	7.829926
5.839857	451.002552	7.834931
5.847859	454.453956	7.839936
6.056484	447.956041	7.844941
5.803870	450.944990	7.849946
5.851936	456.972280	7.854950
6.187304	454.988093	7.859955
6.076638	448.402155	7.864960
6.093473	442.943920	7.869965
5.905298	445.773958	7.874970
5.679735	445.168858	7.879974
5.799381	451.722581	7.884979
5.821613	458.221656	7.889984
6.232649	454.725724	7.894989
5.458774	440.214877	7.899994
5.729515	444.746436	7.904998
6.038003	443.222172	7.910003
5.504613	456.798530	7.915008
5.879051	449.309063	7.920013
5.691127	450.800130	7.925018
5.963622	446.921307	7.930022
5.955027	458.581518	7.935027
5.785642	453.395774	7.940032
5.968207	454.103992	7.945037
5.635021	457.726368	7.950042
5.635998	452.007321	7.955046
5.733339	441.861392	7.960051
5.542007	452.350786	7.965056
5.773257	452.799110	7.970061
5.603847	461.712882	7.975066
5.849180	449.772039	7.980070
6.102227	450.752904	7.985075
5.628172	457.521943	7.990080
5.772577	452.768699	7.995085
5.918828	462.477168	8.000090
5.834362	460.936128	8.005094
6.142895	456.466603	8.010099
5.836661	456.964802	8.015104
6.151195	448.835660	8.020109
5.614834	459.274743	8.025126
5.594784	458.017686	8.030144
5.895243	457.591529	8.035162
5.930053	460.558058	8.040179
6.219916	463.118050	8.045197
5.872441	434.208585	8.050214
5.447517	434.346075	8.055232
5.300005	444.829256	8.060250
5.969725	456.801658	8.065267
5.776189	455.728346	8.070285
5.979479	458.762137	8.075302
5.954537	458.220989	8.080320
6.218648	453.258945	8.085338
5.877032	459.144292	8.090355
5.664220	462.412983	8.095373
5.724839	454.964312	8.100390
6.003474	463.696698	8.105408
5.884791	452.813565	8.110426
5.391410	459.765387	8.115443
5.641025	455.088208	8.120461
5.717853	459.102779	8.125478
5.752248	454.407639	8.130496
5.787657	453.278951	8.135514
5.877177	468.344788	8.140531
5.832688	451.198680	8.145549
6.156632	462.688845	8.150566
5.663393	457.629677	8.155584
6.284387	452.580754	8.160602
5.857397	453.296293	8.165619
5.988185	451.740369	8.170637
6.176776	453.136391	8.175654
5.474305	461.302001	8.180672
5.948651	446.057477	8.185690
5.638043	459.153183	8.190707
5.814871	452.549688	8.195725
5.999452	466.396677	8.200742
5.960071	480.401762	8.205760
6.403930	476.923286	8.210778
5.492040	475.006668	8.215795
5.846387	470.076268	8.220813
6.095317	483.971233	8.225830
5.764308	484.305102	8.230848
5.996642	479.353646	8.235866
5.909033	481.318765	8.240883
6.271457	483.916104	8.245901
6.226637	481.296743	8.250918
6.012782	488.058229	8.255936
6.363062	480.685994	8.260954
5.885741	488.804351	8.265971
5.377466	488.357912	8.270989
5.563262	486.018694	8.276006
5.573140	486.276217	8.281024
5.927796	482.471651	8.286042
6.096910	488.832500	8.291059
6.060001	489.209404	8.296077
6.170789	485.760505	8.301094
5.845716	494.632626	8.306112
6.221517	478.874377	8.311130
5.990550	477.134903	8.316147
5.970142	480.245642	8.321165
6.151144	495.689572	8.326182
6.126934	492.446364	8.331200
6.242301	483.334782	8.336218
5.910209	492.321641	8.341235
6.375202	498.899825	8.346253
6.333603	487.575937	8.351270
6.325833	497.358227	8.356288
6.312717	484.956075	8.361306
6.064065	490.567145	8.366323
6.109113	489.497477	8.371341
6.301491	484.837086	8.376358
6.106453	506.440852	8.381376
6.002594	484.254212	8.386394
5.798420	488.780617	8.391411
6.299428	504.227068	8.396429
5.991045	499.925084	8.401446
6.179620	515.052645	8.406464
6.783920	504.696488	8.411482
6.383624	501.305574	8.416499
6.210805	492.433212	8.421517
6.535956	493.170174	8.426534
6.003513	492.998202	8.431552
5.982145	485.129716	8.436570
6.300876	488.579523	8.441587
6.176600	497.645809	8.446605
6.500551	482.668551	8.451622
6.639332	503.110422	8.456640
6.407156	487.264658	8.461658
6.518699	497.016092	8.466675
6.297634	490.473997	8.471693
6.693941	483.814520	8.476710
6.439398	496.436608	8.481728
6.248148	492.537364	8.486746
6.604292	480.105133	8.491763
6.534736	494.245550	8.496781
6.386033	487.404641	8.501798
6.409998	489.907663	8.506816
6.626962	483.380154	8.511834
6.756492	476.717785	8.516851
6.148545	464.391101	8.521869
6.385170	454.214195	8.526886
6.070121	456.186607	8.531904
6.291837	455.846366	8.536922
6.248201	463.547180	8.541939
6.354162	476.974607	8.546957
6.250241	469.226930	8.551974
6.333820	487.558060	8.556992
6.540013	482.048004	8.562010
6.474110	485.234607	8.567027
5.956131	484.188061	8.572045
6.480503	478.260385	8.577063
6.125937	486.233741	8.582080
6.361978	488.735957	8.587098
6.115130	474.081521	8.592115
6.182355	485.630910	8.597133
6.687064	479.851568	8.602151
6.350723	491.769002	8.607168
6.405922	484.244256	8.612186
6.357887	484.266544	8.617203
6.379319	489.331187	8.622221
6.581028	481.689774	8.627239
6.250895	483.565099	8.632256
6.481425	480.072677	8.637274
6.751261	480.462958	8.642291
6.285010	489.658518	8.647309
6.418559	474.036596	8.652327
6.545045	484.418753	8.657344
6.615320	484.017078	8.662362
6.659465	479.214217	8.667379
6.347247	484.546506	8.672397
6.283964	476.112600	8.677415
6.332966	486.584009	8.682432
6.412254	480.495099	8.687450
6.518433	486.579228	8.692467
6.299619	482.045450	8.697485
6.539013	480.743691	8.702503
6.587109	485.573409	8.707520
6.183255	481.518973	8.712538
6.256941	485.192173	8.717555
6.384574	507.861895	8.722573
6.682033	509.433510	8.727591
6.862016	512.397963	8.732608
6.988168	507.346245	8.737626
6.987298	486.272113	8.742643
6.434083	493.026630	8.747661
6.365555	484.887267	8.752679
6.534563	492.047673	8.757696
6.437657	482.595620	8.762714
6.692061	485.008570	8.767731
6.455514	482.798015	8.772749
6.571845	471.588033	8.777767
6.742654	482.394280	8.782784
6.812523	483.882867	8.787802
6.608951	485.582837	8.792819
6.366116	490.030833	8.797837
6.580217	472.858252	8.802855
6.760069	491.639486	8.807872
6.469051	489.716898	8.812890
6.928646	496.825461	8.817907
6.887186	495.490471	8.822925
6.478223	478.773193	8.827943
6.344073	483.354093	8.832960
6.611042	500.201729	8.837978
6.856189	502.296956	8.842995
6.764511	508.193921	8.848013
6.766426	509.678256	8.853031
7.047382	510.753049	8.858048
6.671841	497.907038	8.863066
6.683498	484.309727	8.868083
6.583562	482.637440	8.873101
7.089677	497.362428	8.878119
6.991116	490.418112	8.883136
6.643131	481.086725	8.888154
6.606281	478.505801	8.893171
6.379673	480.362539	8.898189
6.621343	484.854988	8.903207
6.763798	503.876291	8.908224
6.807579	508.231773	8.913242
7.291883	505.637635	8.918259
6.407827	502.664309	8.923277
6.703474	509.850716	8.928295
6.912148	509.190426	8.933312
6.679693	515.123982	8.938330
7.214641	505.608418	8.943347
6.956632	508.499230	8.948365
6.946203	497.127638	8.953383
6.732715	490.899217	8.958400
6.659933	487.612120	8.963418
6.641075	504.312602	8.968435
6.979362	511.286034	8.973453
7.052961	499.472556	8.978471
6.830902	510.692915	8.983488
6.731036	505.726991	8.988506
6.735152	505.150109	8.993523
6.972252	507.643097	8.998541
6.845314	510.541648	9.003559
6.700985	516.200145	9.008576
6.984641	509.357628	9.013594
7.157407	508.912541	9.018611
6.729762	518.587290	9.023629
6.938175	516.728126	9.028647
7.072414	508.031468	9.033664
6.936877	510.569864	9.038682
6.745262	505.309964	9.043699
6.850899	509.028445	9.048717
6.784116	508.446420	9.053735
6.966259	516.106777	9.058752
6.604586	517.632850	9.063770
7.039177	511.939949	9.068787
6.703214	512.764759	9.073805
6.975440	517.822760	9.078823
7.012107	508.729756	9.083840
6.623642	509.089710	9.088858
7.202290	510.188242	9.093875
6.768210	517.180623	9.098893
6.773125	510.930456	9.103911
6.952821	511.141249	9.108928
6.469025	517.911007	9.113946
6.555340	526.040607	9.118963
6.724139	543.079986	9.123981
7.206380	544.248479	9.128999
7.575759	550.019219	9.134016
7.201077	554.359436	9.139034
7.325638	541.518246	9.144051
7.284270	535.900121	9.149069
7.266188	524.647487	9.154087
7.022601	517.800882	9.159104
6.706688	516.617013	9.164122
6.897505	521.973564	9.169139
7.038112	541.563284	9.174157
7.076088	543.556744	9.179175
7.242227	539.763226	9.184192
7.392352	548.438485	9.189210
7.672833	526.964607	9.194227
7.339517	523.775921	9.199245
7.056511	522.144099	9.204263
7.376148	516.573446	9.209280
7.072844	525.293750	9.214298
7.328088	514.322829	9.219315
6.909998	515.256558	9.224333
7.107826	508.078140	9.229351
7.153167	506.564758	9.234368
6.958081	507.839143	9.239386
6.939657	511.768191	9.244403
6.786951	515.454819	9.249421
7.288180	534.077181	9.254439
7.237902	545.465059	9.259456
7.105306	548.010255	9.264474
7.506012	542.019063	9.269491
7.249936	547.081038	9.274509
7.236021	537.802740	9.279527
7.362621	533.029656	9.284544
6.992782	534.495676	9.289562
7.526206	533.984340	9.294579
7.602092	528.587653	9.299597
7.016093	525.081550	9.304615
6.758015	517.239404	9.309632
7.224005	535.060802	9.314650
7.304680	539.622347	9.319667
7.330264	541.265926	9.324685
7.464477	547.273181	9.329703
7.531518	536.788610	9.334720
7.565589	544.061423	9.339738
7.540545	534.431462	9.344755
7.388264	518.983768	9.349773
7.162654	519.327084	9.354791
7.448470	506.663825	9.359808
6.950636	519.719843	9.364826
7.212554	523.501516	9.369843
7.397100	533.578016	9.374861
7.269942	543.821876	9.379879
7.695272	540.051412	9.384896
7.503881	536.681665	9.389914
7.292567	519.826970	9.394931
7.285121	532.305856	9.399949
7.213027	538.815669	9.404967
7.381313	539.418878	9.409984
7.365794	547.233948	9.415002
7.442303	550.776192	9.420019
7.455021	544.178680	9.425037
7.289583	545.160564	9.430055
7.461238	536.197062	9.435072
7.291340	548.400037	9.440090
7.032071	544.593773	9.445107
7.302707	543.134663	9.450125
7.524208	555.556419	9.455143
7.574801	542.258269	9.460160
7.383234	541.707416	9.465178
7.429915	545.176671	9.470195
7.237908	547.841380	9.475213
7.302490	553.515750	9.480231
7.666683	537.816650	9.485248
7.310935	545.026318	9.490266
7.379744	549.077085	9.495283
7.638517	539.773733	9.500301
7.712673	550.705336	9.505319
7.741286	539.789587	9.510336
7.799683	544.634736	9.515354
7.657431	540.131518	9.520371
7.774386	546.466417	9.525389
7.507177	546.400935	9.530407
7.849016	539.707381	9.535424
7.807593	545.647381	9.540442
7.709754	548.446818	9.545459
7.846804	544.737065	9.550477
7.871380	547.270898	9.555495
7.833803	532.083039	9.560512
7.298169	521.439033	9.565530
7.721316	530.220264	9.570547
7.910997	534.430842	9.575565
7.660302	536.120148	9.580583
7.678899	515.197649	9.585600
7.446751	512.375976	9.590618
7.523235	522.012202	9.595635
7.944622	524.854647	9.600653
7.666361	523.362182	9.605671
7.936036	516.030294	9.610688
7.897067	520.484173	9.615706
7.588643	513.371598	9.620723
7.726620	507.300282	9.625741
7.700284	520.666674	9.630759
7.684657	504.737459	9.635776
7.470582	517.249302	9.640794
7.354369	511.229094	9.645811
7.969398	513.949397	9.650829
7.497945	526.878998	9.655847
7.736285	524.625521	9.660864
7.578116	540.414630	9.665882
7.455593	532.479281	9.670899
8.031486	541.580574	9.675917
7.933719	547.458489	9.680935
7.910487	544.645190	9.685952
7.822942	544.280180	9.690970
7.725696	540.442852	9.695987
7.849727	538.606963	9.701005
7.438364	544.330524	9.706023
7.780398	539.572412	9.711040
7.683329	541.842629	9.716058
7.563718	542.882835	9.721075
7.995985	541.671639	9.726093
7.803161	551.950041	9.731111
7.509908	547.672692	9.736128
7.792796	548.691069	9.741146
7.521078	551.631211	9.746163
8.208114	532.279334	9.751181
7.713538	556.016253	9.756199
7.852782	543.561565	9.761216
7.889414	549.824392	9.766234
7.665460	546.381519	9.771251
8.109664	550.356502	9.776269
7.618174	559.216561	9.781287
7.975404	541.635301	9.786304
7.704687	545.609050	9.791322
7.874593	547.904373	9.796339
8.152997	543.922916	9.801357
7.734839	545.913856	9.806375
7.873577	553.352725	9.811392
7.816235	548.667885	9.816410
7.931363	548.525661	9.821427
8.038636	546.897068	9.826445
7.741354	554.779447	9.831463
7.964671	562.855390	9.836480
7.805257	583.719346	9.841498
7.986254	579.090935	9.846515
8.047152	576.001068	9.851533
8.059234	585.988563	9.856551
7.927290	585.632309	9.861568
8.120588	580.536141	9.866586
8.187210	581.525907	9.871603
8.300680	565.725946	9.876621
8.159368	574.781330	9.881639
7.990367	560.758702	9.886656
7.846215	565.828849	9.891674
8.070142	579.038346	9.896691
8.295043	576.746547	9.901709
8.089518	578.534640	9.906727
8.027776	577.646484	9.911744
7.930433	574.274677	9.916762
8.175911	592.127481	9.921779
8.388077	583.947116	9.926797
8.147600	585.456594	9.931815
8.181268	585.372001	9.936832
8.389893	567.574290	9.941850
8.013677	567.858790	9.946867
8.216702	548.982589	9.951885
8.122216	565.508716	9.956903
8.475602	566.824407	9.961920
8.167320	552.800924	9.966938
7.808160	558.165448	9.971955
8.024265	567.925726	9.976973
8.231363	576.986381	9.981991
8.316342	584.910345	9.987008
8.545388	584.945036	9.992026
8.241004	567.883532	9.997043
7.893857	555.047516	10.002061
8.126939	574.468179	10.007079
7.920043	579.609188	10.012096
8.249228	581.888669	10.017114
7.951115	580.509923	10.022131
8.411707	583.245280	10.027149
8.281193	581.995552	10.032167
8.104757	582.108075	10.037184
8.278157	579.108948	10.042202
8.134881	584.764145	10.047219
7.930975	584.417492	10.052237
8.026058	591.695342	10.057255
7.894431	589.583661	10.062272
8.158540	586.539339	10.067290
8.377460	593.947775	10.072307
8.452635	595.047135	10.077325
8.438917	590.571155	10.082343
8.412701	587.816805	10.087360
8.481792	583.152076	10.092378
8.218395	588.466050	10.097395
8.496369	573.342225	10.102413
8.456251	581.131088	10.107431
8.183044	584.414567	10.112448
8.513784	579.556950	10.117466
8.437121	592.668010	10.122483
8.591645	584.159458	10.127501
8.367927	582.272518	10.132519
8.120154	584.315450	10.137536
8.216509	582.334365	10.142554
8.506591	602.739014	10.147571
8.505660	602.476525	10.152589
8.467814	614.793615	10.157607
8.429717	607.087285	10.162624
8.387979	605.855867	10.167642
8.487268	612.817698	10.172659
8.417736	608.749779	10.177677
8.535057	612.297851	10.182695
8.684087	604.783236	10.187712
8.308896	601.602282	10.192730
8.490854	616.239544	10.197747
8.440938	603.170434	10.202765
8.865369	607.141633	10.207783
8.402524	611.488056	10.212800
8.641672	608.010904	10.217818
7.911119	612.488435	10.222835
8.433748	602.517415	10.227853
8.603262	607.637004	10.232871
8.171114	613.609696	10.237888
8.480486	609.888605	10.242906
8.628204	619.023324	10.247923
8.741318	609.183358	10.252941
8.663262	612.609981	10.257959
8.300840	609.847344	10.262976
8.238035	595.585790	10.267994
8.828345	608.669062	10.273011
8.600818	605.219487	10.278029
8.393644	603.130204	10.283047
8.546987	615.856622	10.288064
9.124372	633.541516	10.293082
8.216216	618.295739	10.298099
8.670045	633.191149	10.303117
8.662325	630.145156	10.308135
8.425464	635.420091	10.313152
9.054658	633.261854	10.318170
8.988246	638.172656	10.323187
8.968411	622.561712	10.328205
8.983827	619.210520	10.333223
8.491890	617.266986	10.338240
8.999799	601.867333	10.343258
8.681644	607.582117	10.348275
8.916542	599.388715	10.353293
8.929363	603.793658	10.358311
8.627390	604.117978	10.363328
8.674836	601.646831	10.368346
8.666872	606.622311	10.373363
9.003754	616.368843	10.378381
8.864344	605.645137	10.383399
8.648897	614.496742	10.388416
9.130994	611.108724	10.393434
8.793233	607.957568	10.398451
8.888687	604.153739	10.403469
8.975849	600.481988	10.408487
8.483443	610.088627	10.413504
8.835670	615.392595	10.418522
8.868489	631.576592	10.423539
9.004889	640.646478	10.428557
8.947401	627.892559	10.433575
8.591093	634.673457	10.438592
9.022348	629.260968	10.443610
9.016996	647.492905	10.448627
9.289591	629.044774	10.453645
8.939553	619.630187	10.458663
8.796952	616.611144	10.463680
9.191933	621.530870	10.468698
9.064521	605.061908	10.473715
8.789895	614.636287	10.478733
8.717858	605.756556	10.483751
8.565647	629.092807	10.488768
9.248942	623.065831	10.493786
8.900464	637.107870	10.498803
8.676695	637.528633	10.503821
9.054067	637.250698	10.508839
8.839581	641.775516	10.513856
9.104202	633.495862	10.518874
8.889581	636.950309	10.523891
8.642418	631.692316	10.528909
9.260451	629.868587	10.533927
8.771575	639.863998	10.538944
9.441622	632.871577	10.543962
9.039253	646.001589	10.548979
9.147877	642.645724	10.553997
9.350218	640.108472	10.559015
9.230951	648.596497	10.564032
9.270911	635.151621	10.569050
9.199937	640.918630	10.574067
9.118218	640.332784	10.579085
9.109985	640.614577	10.584103
8.890226	647.072018	10.589120
9.088496	641.776987	10.594138
9.119680	647.050281	10.599155
9.205463	645.466979	10.604173
9.134129	640.621456	10.609191
9.190459	644.454850	10.614208
8.909343	645.055605	10.619226
9.033426	634.852016	10.624243
8.948649	640.175289	10.629261
9.037068	632.366821	10.634279
9.123535	649.511335	10.639296
9.458573	658.545851	10.644314
9.273882	652.355094	10.649331
9.111343	652.130293	10.654349
9.521541	656.947312	10.659367
9.264901	663.178624	10.664384
9.155031	652.327938	10.669402
9.467440	661.538645	10.674419
9.412791	654.047429	10.679437
9.196353	643.358941	10.684455
9.203582	656.555513	10.689472
9.484624	663.880630	10.694490
9.340750	667.890605	10.699507
8.860753	672.720964	10.704525
9.117504	665.845845	10.709543
8.931713	675.030129	10.714560
9.425419	685.613959	10.719578
9.396840	679.745052	10.724595
9.253225	675.392798	10.729613
9.623697	668.675731	10.734631
9.291572	671.965872	10.739648
9.181687	656.036029	10.744666
9.161940	667.070128	10.749683
9.140400	672.532891	10.754701
9.144673	660.559959	10.759719
9.534430	660.963774	10.764736
9.132417	662.078290	10.769754
9.812974	686.344234	10.774771
9.454038	682.439353	10.779789
9.608945	664.743761	10.784807
9.589973	674.284932	10.789824
9.795225	668.612380	10.794842
9.914622	670.612990	10.799859
9.363331	672.844367	10.804877
9.747497	671.517741	10.809895
9.511112	667.143314	10.814912
9.630316	675.173044	10.819930
9.518315	677.750268	10.824947
9.250694	676.073355	10.829965
9.579768	676.612051	10.834983
9.153792	674.504801	10.840000
9.161168	676.639772	10.845018
9.447864	682.413087	10.850035
9.480961	698.813234	10.855053
9.756626	698.348282	10.860071
9.891150	698.467381	10.865088
9.732616	702.055423	10.870106
9.878827	695.943101	10.875123
9.197799	686.899412	10.880141
9.588547	698.235352	10.885159
9.648061	699.793393	10.890176
9.433727	704.087905	10.895194
9.506667	698.692435	10.900211
9.462251	702.473500	10.905229
9.760722	706.025733	10.910247
9.568123	702.890780	10.915264
9.578804	696.192367	10.920282
9.798958	704.602745	10.925299
9.808109	699.267088	10.930317
9.926614	697.836204	10.935335
9.871511	706.651170	10.940352
10.033110	699.219846	10.945370
9.974562	708.793206	10.950387
9.622910	707.240486	10.955405
10.437550	704.958507	10.960423
9.910175	697.410622	10.965440
10.284102	696.936029	10.970458
9.726353	685.041146	10.975475
9.642175	693.918414	10.980493
10.121392	699.363298	10.985511
10.066213	687.254373	10.990528
9.975889	676.114418	10.995546
10.054234	656.155545	11.000563
9.858469	671.524100	11.005581
9.786373	671.021293	11.010599
9.766670	673.061165	11.015616
9.398469	669.805812	11.020634
9.875135	675.925866	11.025651
9.806840	700.585187	11.030669
9.845421	701.982742	11.035687
10.205207	704.444741	11.040704
10.029374	700.134053	11.045722
10.143683	701.234002	11.050739
10.044116	706.969177	11.055757
10.165432	694.584666	11.060775
9.691477	694.082518	11.065792
9.877084	698.730204	11.070810
10.181175	695.999664	11.075827
10.014653	709.459989	11.080845
10.415925	697.201566	11.085863
9.930528	698.094331	11.090880
10.231264	700.130152	11.095898
10.198382	689.621932	11.100915
9.787606	681.377753	11.105933
10.087204	692.151126	11.110951
10.095622	700.357540	11.115968
9.996000	699.162113	11.120986
9.909092	707.075343	11.126003
9.787199	707.426224	11.131021
10.113587	713.310858	11.136039
10.150259	694.330056	11.141056
10.002113	705.130621	11.146074
10.313857	700.049763	11.151091
10.269185	698.481644	11.156109
10.267828	695.358208	11.161127
10.732587	697.526792	11.166144
10.275716	703.654011	11.171162
10.536206	689.203995	11.176179
9.956935	671.026145	11.181197
9.693822	673.356065	11.186215
9.796675	691.814145	11.191232
9.702201	702.584333	11.196250
10.175784	691.061874	11.201267
10.016750	707.839416	11.206285
10.010463	704.216635	11.211303
9.966551	705.320642	11.216320
9.949797	709.269736	11.221338
10.305349	721.972472	11.226355
10.062648	721.108875	11.231373
10.057893	721.221796	11.236391
10.265038	728.941682	11.241408
10.198195	732.274348	11.246426
10.512262	722.718208	11.251443
10.377860	730.227169	11.256461
10.282642	723.952422	11.261479
10.668166	733.961593	11.266496
10.226958	739.627592	11.271514
10.466552	732.611212	11.276531
10.453247	731.013665	11.281549
10.912521	728.741937	11.286567
10.945329	728.367349	11.291584
10.398604	719.212544	11.296602
10.434370	700.009657	11.301619
10.547175	707.215329	11.306637
10.059087	698.479500	11.311655
10.204850	704.202435	11.316672
10.031907	727.710182	11.321690
10.418232	723.753060	11.326707
10.677939	727.384768	11.331725
10.260790	735.808584	11.336743
10.662126	733.336264	11.341760
10.429119	727.666072	11.346778
10.782470	729.997460	11.351795
10.419421	739.654523	11.356813
10.553072	740.777635	11.361831
10.835314	737.681848	11.366848
10.340294	733.389760	11.371866
10.509934	726.208054	11.376883
10.644538	738.320998	11.381901
10.435635	733.108970	11.386919
10.870462	722.609986	11.391936
10.561605	736.228629	11.396954
10.694591	731.666810	11.401971
10.804330	729.491172	11.406989
10.560478	731.646258	11.412007
10.713437	732.205570	11.417024
10.730892	739.791058	11.422042
10.830699	730.668138	11.427059
10.863124	735.654465	11.432077
10.725839	734.780431	11.437095
10.708808	725.440732	11.442112
10.552776	732.249794	11.447130
10.734807	732.116132	11.452147
10.560201	731.363057	11.457165
10.544567	729.470642	11.462183
11.058347	731.005733	11.467200
10.629510	732.589247	11.472218
10.512067	739.906036	11.477235
10.465827	734.017605	11.482253
10.509633	735.148959	11.487271
10.432228	725.795084	11.492288
10.720047	727.318131	11.497306
10.775824	737.408688	11.502323
10.800045	729.641942	11.507341
10.694996	728.380883	11.512359
11.213673	733.014945	11.517376
11.047955	738.879230	11.522394
11.122491	728.517290	11.527411
11.078072	728.796046	11.532429
10.649562	733.709985	11.537447
10.647114	728.734488	11.542464
10.452214	737.052469	11.547482
10.917651	742.657719	11.552499
10.891177	757.507505	11.557517
10.894444	762.361688	11.562535
11.179296	763.281729	11.567552
11.111945	762.283675	11.572570
11.252271	755.525894	11.577587
10.965899	743.682504	11.582605
10.682306	740.698682	11.587623
11.003120	752.800173	11.592640
11.107755	763.778628	11.597658
11.027346	765.350289	11.602675
10.887099	767.370253	11.607693
10.970435	769.495563	11.612711
11.260803	765.245346	11.617728
11.409657	758.319426	11.622746
10.857272	749.448792	11.627763
11.051814	757.776258	11.632781
11.215544	765.288038	11.637799
11.333462	763.472232	11.642816
11.390094	752.183788	11.647834
11.049764	744.949055	11.652851
10.911577	737.153006	11.657869
11.163914	745.576363	11.662887
11.295005	751.535991	11.667904
10.931024	769.935551	11.672922
11.278451	761.160404	11.677939
11.075665	763.255916	11.682957
11.140618	767.731959	11.687975
11.180406	761.562502	11.692992
11.097734	771.345212	11.698010
10.868898	765.411141	11.703027
11.362207	759.390892	11.708045
11.010200	767.298025	11.713063
11.037720	755.808131	11.718080
10.752327	760.333747	11.723098
11.106200	762.832365	11.728115
10.951867	751.764409	11.733133
11.305220	771.308821	11.738151
11.526464	780.301501	11.743168
11.310863	780.773662	11.748186
11.287157	773.258152	11.753203
11.370343	772.424825	11.758221
11.110507	780.625482	11.763239
11.430407	791.562467	11.768256
11.655495	797.599986	11.773274
11.595976	778.678177	11.778291
11.421019	769.530439	11.783309
11.356137	767.021051	11.788327
11.205119	760.813237	11.793344
11.122166	784.092149	11.798362
11.474488	786.709525	11.803379
11.801438	786.328560	11.808397
11.321244	797.183793	11.813415
11.336534	795.936188	11.818432
11.670232	793.299523	11.823450
11.668188	803.332416	11.828467
11.791743	779.586586	11.833485
11.292065	785.217639	11.838503
11.688986	786.888294	11.843520
11.548561	779.612049	11.848538
11.353087	792.305458	11.853555
12.010198	791.538531	11.858573
11.414847	777.314743	11.863591
11.652541	769.353449	11.868608
11.655640	773.504758	11.873626
11.433366	774.843325	11.878643
11.619914	765.953588	11.883661
11.478679	795.290424	11.888679
11.965625	787.756162	11.893696
11.653430	796.228112	11.898714
11.510464	797.265721	11.903731
11.778573	786.576310	11.908749
11.617391	799.592940	11.913767
11.957112	780.181566	11.918784
11.848012	790.475930	11.923802
11.710184	783.728154	11.928819
11.803107	773.878646	11.933837
11.546387	771.619437	11.938855
11.901675	774.526063	11.943872
12.057022	775.295398	11.948890
11.329580	767.387059	11.953907
11.431902	781.869615	11.958925
11.546154	787.840324	11.963943
11.707408	784.441037	11.968960
12.008586	795.693913	11.973978
11.855530	788.747498	11.978995
12.175388	786.997722	11.984013
11.793482	800.356534	11.989031
11.796813	794.912763	11.994048
11.944628	788.604088	11.999066
11.571516	793.100595	12.004083
12.091606	785.716327	12.009101
11.926930	788.725920	12.014119
11.893532	795.576039	12.019136
11.863855	776.705764	12.024154
11.609630	792.344178	12.029171
11.994227	782.084591	12.034189
12.054713	784.721345	12.039207
11.877339	798.043795	12.044224
11.952941	790.849148	12.049242
11.714127	793.655331	12.054259
11.890152	792.742403	12.059277
11.662973	788.440421	12.064295
11.940649	793.858608	12.069312
12.119771	792.716439	12.074330
11.955761	796.627832	12.079347
11.937696	787.898070	12.084365
11.939162	799.625542	12.089383
11.754813	816.183211	12.094400
12.196071	814.754176	12.099418
12.224931	830.880776	12.104435
12.355326	816.538088	12.109453
12.248973	826.815092	12.114471
12.399468	820.909476	12.119488
12.622413	798.317692	12.124506
11.858169	799.303463	12.129523
11.888469	785.513628	12.134541
12.148136	791.123378	12.139559
12.255244	799.311078	12.144576
12.527190	797.474784	12.149594
11.974081	796.072856	12.154611
12.185881	791.003857	12.159629
11.816304	802.257608	12.164647
12.214990	822.933848	12.169664
12.794420	820.641741	12.174682
12.422481	814.433622	12.179699
12.522090	794.773576	12.184717
12.302260	795.593662	12.189735
12.145336	799.289325	12.194752
12.327786	788.322044	12.199770
12.118725	804.386202	12.204787
12.476507	813.717600	12.209805
12.692448	818.313827	12.214823
12.602330	793.153388	12.219840
12.614488	790.593398	12.224858
12.055084	801.598012	12.229875
11.862108	785.640708	12.234893
12.542857	803.254879	12.239911
12.381966	819.655512	12.244928
12.555978	818.603162	12.249946
12.397151	821.994441	12.254963
12.502776	819.359464	12.259981
12.594723	828.204777	12.264999
12.677180	823.056880	12.270016
12.726290	808.821012	12.275034
12.533801	797.223966	12.280051
12.452007	786.230142	12.285069
12.711441	789.960526	12.290087
12.234616	786.464559	12.295104
12.498187	790.302909	12.300122
12.172242	811.957401	12.305139
12.488337	818.460873	12.310157
12.845480	815.690394	12.315175
12.577535	815.453979	12.320192
12.692540	812.952081	12.325210
12.296190	814.720742	12.330227
12.144601	821.490919	12.335245
12.746399	822.605902	12.340263
12.576618	822.828337	12.345280
12.566005	820.659110	12.350298
12.583816	821.330647	12.355315
12.676163	826.061586	12.360333
12.289960	825.527132	12.365351
12.529620	824.151683	12.370368
12.667360	818.445027	12.375386
12.512153	826.233459	12.380403
12.881425	841.109073	12.385421
13.034383	844.222955	12.390439
12.627290	836.127874	12.395456
12.629130	845.056674	12.400474
12.804053	855.376307	12.405491
12.932813	855.307007	12.410509
13.198614	850.349478	12.415527
12.813522	841.433070	12.420544
13.268427	830.807850	12.425562
12.971079	827.619027	12.430579
12.682669	821.091134	12.435597
12.737309	823.342671	12.440615
12.466471	834.819782	12.445632
12.957666	842.530302	12.450650
12.518251	854.716115	12.455667
12.957222	858.029688	12.460685
13.518491	859.350218	12.465703
13.111488	863.228401	12.470720
13.212583	861.401995	12.475738
12.832856	843.401390	12.480755
13.153048	839.555620	12.485773
12.944594	833.340002	12.490791
12.692533	852.071821	12.495808
12.963759	843.994292	12.500826
13.061801	850.936753	12.505843
12.996675	849.753295	12.510861
13.243557	847.638895	12.515879
12.925264	853.551416	12.520896
12.963525	847.145974	12.525914
12.965441	860.742200	12.530931
12.893146	848.743664	12.535949
13.047542	856.692841	12.540967
13.017214	863.994028	12.545984
13.043108	857.198534	12.551002
12.787454	860.016189	12.556019
12.708396	849.656079	12.561037
12.788317	854.726079	12.566055
12.816296	881.752217	12.571072
13.406112	886.679995	12.576090
13.570634	886.301225	12.581107
13.397181	885.392448	12.586125
13.694328	893.191938	12.591143
13.158907	865.303204	12.596160
13.480068	859.990821	12.601178
13.049096	865.438642	12.606195
13.482725	864.735237	12.611213
13.559059	864.720318	12.616231
13.298151	864.339434	12.621248
13.287286	859.682992	12.626266
13.010647	858.272108	12.631283
13.246458	876.119761	12.636301
13.362933	872.028334	12.641319
13.409571	887.680019	12.646336
13.516841	878.089658	12.651354
13.422930	889.279541	12.656371
13.441328	897.029310	12.661389
13.519942	883.997060	12.666407
13.274758	877.963110	12.671424
13.274731	881.750422	12.676442
13.346288	887.698150	12.681459
13.421436	892.987053	12.686477
13.716264	878.478795	12.691495
13.188808	894.310948	12.696512
13.228850	881.381169	12.701530
13.372865	880.194439	12.706547
13.286379	891.928333	12.711565
13.510212	884.888127	12.716583
13.152738	888.958466	12.721600
13.463904	898.469701	12.726618
13.407858	909.988718	12.731635
13.836778	914.509023	12.736653
14.056287	912.108236	12.741671
13.695522	922.118554	12.746688
13.524813	913.226309	12.751706
13.944742	910.965426	12.756723
13.668993	907.886770	12.761741
14.153674	902.835758	12.766759
14.007652	894.474429	12.771776
14.008811	888.814857	12.776794
13.913794	885.738838	12.781811
13.546407	887.932195	12.786829
13.740103	877.141712	12.791847
13.671327	880.213723	12.796864
13.734220	880.161671	12.801882
14.031105	876.883118	12.806899
13.766645	881.882819	12.811917
13.720020	877.214207	12.816935
13.607685	886.032489	12.821952
13.633116	881.532990	12.826970
13.874294	892.206967	12.831987
13.707379	907.531592	12.837005
13.638618	905.479099	12.842023
13.803980	908.610223	12.847040
13.862234	904.747350	12.852058
14.099502	911.463559	12.857075
13.941836	913.730320	12.862093
13.619303	913.633679	12.867111
13.669027	912.175628	12.872128
13.879243	908.234348	12.877146
14.158603	912.381897	12.882163
13.974731	908.767920	12.887181
14.270394	909.574368	12.892199
13.963340	911.843521	12.897216
14.020070	908.378516	12.902234
13.997896	902.048447	12.907251
13.941108	906.083375	12.912269
14.347319	908.988649	12.917287
14.312669	905.942354	12.922304
14.252405	908.548809	12.927322
14.292916	901.603631	12.932339
14.298947	907.052445	12.937357
14.088281	906.098281	12.942375
14.189795	917.664338	12.947392
14.306962	914.757364	12.952410
14.287548	904.564458	12.957427
14.142047	910.396314	12.962445
14.177550	899.562429	12.967463
13.850280	914.292492	12.972480
14.129386	907.668261	12.977498
14.193559	904.720099	12.982515
14.252913	903.973793	12.987533
14.244182	904.053718	12.992551
14.094212	902.948134	12.997568
14.105374	903.492048	13.002586
14.102877	918.035854	13.007603
14.002555	937.024820	13.012621
14.329372	935.577792	13.017639
14.654635	940.311386	13.022656
14.376645	948.594672	13.027674
14.749354	934.996987	13.032691
14.501751	937.407041	13.037709
14.654858	942.529468	13.042727
14.230531	941.413189	13.047744
14.337568	947.478657	13.052762
14.670323	940.861242	13.057779
14.213699	952.335858	13.062797
14.300334	942.133961	13.067815
14.069306	935.370117	13.072832
14.209472	942.247353	13.077850
14.495801	941.575122	13.082867
14.465043	931.036466	13.087885
14.533390	933.560921	13.092903
14.486741	941.999046	13.097920
14.474917	937.838775	13.102938
14.763862	935.753983	13.107955
14.469029	938.953341	13.112973
14.612284	934.456681	13.117991
14.555301	936.237051	13.123008
14.656546	955.542516	13.128026
14.915732	955.829469	13.133043
14.947247	946.574868	13.138061
14.729833	942.455463	13.143079
14.577209	929.430904	13.148096
14.698725	937.469835	13.153114
14.814613	940.964287	13.158131
14.831832	934.880399	13.163149
14.866962	940.552327	13.168167
14.763773	937.424510	13.173184
14.768680	938.838708	13.178202
15.012092	944.853949	13.183219
14.929508	940.473562	13.188237
14.707259	947.186645	13.193255
14.839039	940.949467	13.198272
14.900221	952.416356	13.203290
15.135572	952.155331	13.208307
14.874606	934.643513	13.213325
14.878772	939.412371	13.218343
14.852279	939.944829	13.223360
14.757398	955.151628	13.228378
15.474476	959.501614	13.233395
14.853211	949.137474	13.238413
14.767265	947.300418	13.243431
15.186128	957.817748	13.248448
15.248519	962.990299	13.253466
14.918300	938.191564	13.258483
15.245884	946.742280	13.263501
15.059402	946.443111	13.268519
15.020149	934.748448	13.273536
15.156221	942.729454	13.278554
14.779189	950.924091	13.283571
15.234390	961.536559	13.288589
14.907997	960.588635	13.293607
15.567291	959.403252	13.298624
15.117739	965.259686	13.303642
15.620591	960.737496	13.308659
15.546477	943.841817	13.313677
15.467012	939.517602	13.318695
15.621573	933.512454	13.323712
15.217990	940.810369	13.328730
15.103153	929.508961	13.333747
15.133814	940.676600	13.338765
14.942740	929.802408	13.343783
15.124190	919.398162	13.348800
15.270070	938.659575	13.353818
15.577227	938.948789	13.358835
15.285259	948.325282	13.363853
15.027796	926.780041	13.368871
15.622008	950.882025	13.373888
15.560526	956.927873	13.378906
15.510745	949.070961	13.383923
15.270690	945.781257	13.388941
15.341264	951.305967	13.393959
15.637065	957.325496	13.398976
15.457462	963.499636	13.403994
15.583873	965.397549	13.409011
15.150810	955.198175	13.414029
15.174065	961.647240	13.419047
15.500513	958.211008	13.424064
15.651586	965.461225	13.429082
15.626196	957.307751	13.434099
15.684953	960.973113	13.439117
15.378563	971.161028	13.444135
15.799971	957.739471	13.449152
15.343412	969.111732	13.454170
15.594450	955.605510	13.459187
15.583262	962.914190	13.464205
15.725444	956.857551	13.469223
15.998922	958.764087	13.474240
15.854725	967.399532	13.479258
15.771548	959.454077	13.484275
15.658046	959.199861	13.489293
15.153619	967.863690	13.494311
15.463145	962.332746	13.499328
15.508944	970.010678	13.504346
15.560413	965.271799	13.509363
15.553008	969.081618	13.514381
15.584964	968.403639	13.519399
15.784735	965.308524	13.524416
16.072528	986.012470	13.529434
15.961384	968.158797	13.534451
15.946115	958.062012	13.539469
16.086443	956.088924	13.544487
15.853332	953.433856	13.549504
15.761837	965.424136	13.554522
15.785980	957.456119	13.559539
16.126216	956.404081	13.564557
15.762081	959.080738	13.569575
15.830805	956.571551	13.574592
15.971968	975.329490	13.579610
16.062995	988.759056	13.584627
16.157647	978.844370	13.589645
16.227796	986.609202	13.594663
16.038723	968.874775	13.599680
15.926237	966.762616	13.604698
16.358160	966.421676	13.609715
16.129423	961.603791	13.614733
15.757444	958.632059	13.619751
16.304907	979.289290	13.624768
16.163619	984.155171	13.629786
16.608502	988.727566	13.634803
16.261327	969.531307	13.639821
16.086258	972.979253	13.644839
16.411298	957.332889	13.649856
16.248567	961.214192	13.654874
16.180573	957.362055	13.659891
16.471028	952.673609	13.664909
16.346347	964.256435	13.669927
16.350368	959.043188	13.674944
16.169436	957.983296	13.679962
16.259200	955.156455	13.684979
16.189848	956.229473	13.689997
16.190925	964.082937	13.695015
16.362742	967.320474	13.700032
16.311852	985.370625	13.705050
16.539256	985.678214	13.710067
15.924683	985.252182	13.715085
16.183570	988.227233	13.720103
16.232732	996.228617	13.725120
16.481562	989.575527	13.730138
16.408967	985.680056	13.735155
16.272359	984.729718	13.740173
16.289045	992.523517	13.745191
16.362071	991.784777	13.750208
16.270782	995.173528	13.755226
16.479815	993.986218	13.760243
16.826631	989.341539	13.765261
16.785192	995.621854	13.770279
16.906308	993.749587	13.775296
16.579989	999.380442	13.780314
16.263695	994.284596	13.785331
16.566926	997.018825	13.790349
16.327996	997.761785	13.795367
16.466711	1001.420558	13.800384
16.809065	1003.854600	13.805402
16.954954	1007.803900	13.810419
16.798489	992.306431	13.815437
16.576756	991.858011	13.820455
16.469698	987.260038	13.825472
17.018601	1003.188964	13.830490
16.812987	1012.427526	13.835507
16.788990	994.194395	13.840525
16.666505	1011.695089	13.845543
16.918741	1016.459742	13.850560
16.810782	1011.950095	13.855578
17.021252	1018.468847	13.860595
17.103074	1013.328866	13.865613
16.886768	997.644105	13.870631
16.826740	994.472883	13.875648
17.128201	994.152053	13.880666
16.546794	995.753473	13.885683
16.889668	1003.138746	13.890701
16.984736	1017.460533	13.895719
17.083191	1005.609863	13.900736
17.131881	1013.371189	13.905754
17.375021	1022.673347	13.910771
17.023807	993.018023	13.915789
17.009763	994.771185	13.920807
17.061673	997.015720	13.925824
17.019164	1013.207520	13.930842
17.164896	1014.206210	13.935859
17.320351	1010.036618	13.940877
17.084965	1006.363073	13.945895
17.247948	1012.785391	13.950912
17.291051	1018.172966	13.955930
17.071333	1017.220693	13.960947
17.446365	1010.950927	13.965965
17.089707	1010.584380	13.970983
16.904698	999.123333	13.976000
17.194712	1008.815703	13.981018
17.110316	1011.641924	13.986035
17.535392	1010.840727	13.991053
17.508338	1021.468440	13.996071
17.325735	1015.288213	14.001088
17.565394	1008.825213	14.006106
17.362091	1020.937266	14.011123
17.275798	1011.972667	14.016141
17.630711	1016.103750	14.021159
17.504684	1007.408738	14.026176
17.397727	1003.931157	14.031194
17.452325	1018.361242	14.036211
17.511536	1010.181867	14.041229
17.352217	1013.674052	14.046247
17.201196	1015.751150	14.051264
17.612467	1012.594888	14.056282
17.172252	1016.729797	14.061299
17.494995	1019.232058	14.066317
17.331983	1019.712018	14.071335
17.346650	1013.989529	14.076352
17.207264	1016.608760	14.081370
17.146527	1029.494326	14.086387
17.707079	1013.113124	14.091405
17.108487	1020.027763	14.096423
17.609546	1038.635017	14.101440
17.732706	1045.459617	14.106458
17.646089	1045.913101	14.111475
17.725927	1051.750465	14.116493
17.927496	1053.266229	14.121511
17.530856	1044.617753	14.126528
18.120939	1045.658721	14.131546
17.710979	1050.814544	14.136563
17.658319	1054.969292	14.141581
17.640481	1054.501151	14.146599
17.681825	1045.019672	14.151616
17.857822	1047.344765	14.156634
17.525082	1048.037576	14.161651
17.514455	1041.425623	14.166669
17.662319	1050.989686	14.171687
17.662165	1058.478065	14.176704
18.060102	1048.747556	14.181722
17.782455	1053.953431	14.186739
17.823288	1049.390696	14.191757
18.054026	1051.980693	14.196775
17.916714	1055.283412	14.201792
17.953686	1051.469707	14.206810
18.059441	1075.740869	14.211827
17.993123	1055.958080	14.216845
18.370272	1063.699086	14.221863
18.052200	1062.567891	14.226880
18.305036	1046.661405	14.231898
18.253961	1058.297418	14.236915
18.394220	1044.954800	14.241933
18.311361	1053.740327	14.246951
18.075551	1051.345520	14.251968
18.319729	1043.136563	14.256986
18.309856	1051.323371	14.262003
18.256143	1043.683589	14.267021
18.244849	1049.559328	14.272039
18.157001	1056.978429	14.277056
18.266946	1047.165876	14.282074
18.056547	1049.944548	14.287091
18.062048	1046.951784	14.292109
17.933972	1058.894676	14.297127
17.751573	1071.532796	14.302144
18.073986	1061.784913	14.307162
17.907873	1073.975860	14.312179
18.463713	1066.011923	14.317197
18.069308	1071.506884	14.322215
17.996560	1066.249277	14.327232
18.068107	1082.097796	14.332250
18.274392	1099.740782	14.337267
18.518015	1096.838343	14.342285
18.433438	1103.762457	14.347303
18.095647	1107.324484	14.352320
18.519596	1098.033696	14.357338
18.466189	1102.044098	14.362355
18.529484	1099.153917	14.367373
18.907784	1109.616679	14.372391
18.892666	1110.128749	14.377408
18.997918	1103.282951	14.382426
18.787748	1098.700509	14.387443
18.841634	1105.922066	14.392461
19.039366	1088.707040	14.397479
18.943051	1101.621412	14.402496
18.843911	1093.629724	14.407514
19.087440	1099.158808	14.412531
18.685620	1084.964571	14.417549
18.681185	1067.058403	14.422567
18.468266	1077.798934	14.427584
18.753189	1086.918604	14.432602
18.809660	1099.150128	14.437619
18.862430	1098.817093	14.442637
18.888288	1101.323443	14.447655
18.749573	1094.636306	14.452672
18.919084	1099.776530	14.457690
19.120414	1107.714886	14.462707
18.838103	1096.392376	14.467725
19.086179	1096.306393	14.472743
18.933133	1097.624424	14.477760
19.161787	1101.780847	14.482778
18.682820	1107.560730	14.487795
18.807322	1096.414684	14.492813
19.011236	1104.262848	14.497831
18.837483	1110.812829	14.502848
19.049188	1100.480201	14.507866
18.991628	1101.857948	14.512883
18.889263	1100.347605	14.517901
18.885292	1091.302351	14.522919
19.031793	1106.758926	14.527936
19.281915	1101.341739	14.532954
19.131278	1106.979650	14.537971
18.992979	1102.210858	14.542989
18.925982	1107.366383	14.548007
19.062771	1127.973577	14.553024
19.291128	1119.829805	14.558042
19.051367	1119.273753	14.563059
19.062309	1131.627826	14.568077
19.265778	1122.935852	14.573095
19.254160	1134.403165	14.578112
19.423444	1125.861353	14.583130
19.747209	1130.647222	14.588147
19.701249	1125.607181	14.593165
19.911035	1123.921332	14.598183
19.397049	1129.517288	14.603200
19.452608	1116.351674	14.608218
19.628332	1121.325526	14.613235
19.497898	1124.405078	14.618253
19.344531	1117.282590	14.623271
19.610558	1118.372311	14.628288
19.842450	1111.567661	14.633306
19.777165	1123.691102	14.638323
19.346645	1111.216104	14.643341
19.687300	1107.944794	14.648359
19.159456	1120.830916	14.653376
19.869492	1114.517235	14.658394
19.612516	1122.510518	14.663411
20.008480	1122.789699	14.668429
19.863790	1121.647397	14.673447
19.506274	1126.399269	14.678464
19.457242	1119.636587	14.683482
19.595991	1121.015956	14.688499
19.655281	1121.007020	14.693517
19.706731	1121.400156	14.698535
19.497671	1131.392084	14.703552
19.796581	1118.685209	14.708570
19.826517	1122.982538	14.713587
19.849825	1125.207831	14.718605
19.727142	1111.442741	14.723623
19.635749	1124.549613	14.728640
19.335329	1130.463205	14.733658
19.668356	1142.894060	14.738675
19.633047	1142.756366	14.743693
19.864234	1148.495778	14.748711
19.981192	1153.562869	14.753728
20.207436	1153.402959	14.758746
20.302086	1150.190247	14.763763
20.260341	1153.108613	14.768781
20.372975	1146.556044	14.773799
19.884587	1158.314820	14.778816
20.124307	1151.126978	14.783834
20.368913	1155.344540	14.788851
20.167974	1154.945019	14.793869
20.554247	1153.332584	14.798887
20.298459	1162.074084	14.803904
20.428551	1147.879166	14.808922
20.696981	1148.519689	14.813939
19.895132	1126.410748	14.818957
19.806154	1128.846037	14.823975
20.081161	1149.485794	14.828992
20.025753	1140.269542	14.834010
20.403302	1148.048317	14.839027
20.262774	1156.858447	14.844045
20.083163	1151.560703	14.849063
19.988486	1154.021351	14.854080
20.095469	1143.597838	14.859098
20.605174	1141.147599	14.864115
20.523690	1151.991920	14.869133
20.505358	1147.490957	14.874151
20.390302	1144.166653	14.879168
20.493045	1151.007292	14.884186
20.456640	1154.123580	14.889203
20.390522	1149.018774	14.894221
20.686369	1154.025818	14.899239
20.337813	1165.603095	14.904256
20.425718	1173.565061	14.909274
20.474209	1174.615357	14.914291
20.517987	1171.329998	14.919309
20.649426	1171.672046	14.924327
20.516033	1177.002797	14.929344
20.722532	1181.256621	14.934362
20.914454	1171.253993	14.939379
20.312627	1181.141167	14.944397
20.653840	1173.521107	14.949415
20.696322	1176.343984	14.954432
20.658751	1178.994742	14.959450
20.812908	1165.638688	14.964467
20.689915	1175.934042	14.969485
20.915043	1161.526079	14.974503
20.487953	1179.554739	14.979520
20.404469	1191.198600	14.984538
21.068226	1201.454139	14.989555
20.729763	1221.647559	14.994573
21.214025	1207.379545	14.999591
20.840768	1207.603523	15.004608
20.711643	1209.973847	15.009626
21.021248	1206.569494	15.014643
20.884683	1210.330372	15.019661
21.260067	1205.452149	15.024679
21.163161	1205.551456	15.029696
21.239463	1206.866413	15.034714
21.190738	1198.043882	15.039731
20.968580	1206.519197	15.044749
21.169926	1201.684077	15.049767
21.065370	1200.941381	15.054784
21.036352	1212.631320	15.059802
21.231868	1209.935669	15.064819
21.137813	1206.352753	15.069837
21.191341	1203.277963	15.074855
21.178264	1206.435658	15.079872
21.092393	1201.293175	15.084890
21.172773	1208.860363	15.089907
20.861758	1219.027950	15.094925
21.060471	1237.629402	15.099943
21.305808	1229.903208	15.104960
21.493656	1235.638046	15.109978
21.548429	1227.488820	15.114995
21.618151	1242.917350	15.120013
21.672887	1237.694792	15.125031
21.719228	1235.626666	15.130048
21.947089	1229.194669	15.135066
22.049436	1232.492233	15.140083
21.892631	1221.010981	15.145101
21.576019	1201.717624	15.150119
21.448036	1194.068461	15.155136
21.191319	1201.027530	15.160154
21.623743	1211.744347	15.165171
21.872676	1224.713242	15.170189
22.123050	1224.659552	15.175207
21.752946	1212.770075	15.180224
21.629310	1206.503596	15.185242
21.966914	1203.080417	15.190259
21.491020	1203.554124	15.195277
21.602151	1207.569487	15.200295
22.162698	1219.908651	15.205312
22.183521	1223.348499	15.210330
22.062008	1209.083934	15.215347
21.668706	1201.738701	15.220365
21.573471	1200.262594	15.225383
21.877058	1209.485135	15.230400
22.122831	1220.227865	15.235418
22.267008	1213.386571	15.240435
21.870842	1209.424360	15.245453
22.040050	1198.130658	15.250471
22.087902	1210.033400	15.255488
21.780687	1224.323431	15.260506
22.146008	1226.405672	15.265523
22.071932	1226.344497	15.270541
22.216544	1221.394790	15.275559
22.377066	1217.206585	15.280576
22.266455	1226.592862	15.285594
22.548471	1220.680588	15.290611
22.100207	1203.198022	15.295629
21.925531	1203.172859	15.300647
22.273855	1218.576315	15.305664
22.280815	1222.936150	15.310682
22.424741	1222.213565	15.315699
22.224123	1226.425234	15.320717
22.148446	1229.107924	15.325735
22.531869	1225.762949	15.330752
22.415678	1240.415716	15.335770
22.599801	1225.335006	15.340787
22.330673	1232.605589	15.345805
22.654515	1236.008459	15.350823
22.799443	1224.204225	15.355840
22.216859	1215.446013	15.360858
22.583177	1216.020271	15.365875
22.226715	1228.411870	15.370893
22.236389	1232.805114	15.375911
22.416661	1222.602034	15.380928
22.379562	1227.088481	15.385946
22.595969	1229.084849	15.390963
22.688106	1224.898167	15.395981
22.441262	1228.692339	15.400999
22.669904	1229.367431	15.406016
22.641618	1232.295385	15.411034
22.375268	1229.937121	15.416051
22.719823	1230.011866	15.421069
22.746624	1231.090180	15.426087
22.532200	1222.105814	15.431104
22.515151	1241.801364	15.436122
22.648909	1249.472687	15.441139
23.037437	1257.523306	15.446157
23.079835	1264.618504	15.451175
23.397144	1256.561054	15.456192
23.073665	1250.856495	15.461210
23.161602	1225.616941	15.466227
22.827166	1231.412607	15.471245
22.747719	1224.505334	15.476263
22.678598	1233.833147	15.481280
23.187355	1250.364256	15.486298
23.284148	1254.108401	15.491315
23.078459	1255.480470	15.496333
23.086395	1257.724086	15.501351
23.080329	1259.503509	15.506368
22.945458	1255.913981	15.511386
23.289501	1249.113070	15.516403
23.127773	1264.217113	15.521421
23.223850	1252.467039	15.526439
23.515690	1251.438775	15.531456
23.224669	1261.910142	15.536474
23.359044	1247.923862	15.541491
23.442346	1258.080260	15.546509
23.316290	1257.393495	15.551527
23.443634	1243.221388	15.556544
23.478311	1261.696597	15.561562
23.399096	1251.248452	15.566579
23.615585	1253.441260	15.571597
23.351599	1260.570455	15.576615
23.619258	1250.270552	15.581632
23.766335	1253.383920	15.586650
23.710153	1239.917888	15.591667
23.490627	1230.055263	15.596685
22.982422	1222.731875	15.601703
23.370284	1229.877899	15.606720
23.613216	1251.625052	15.611738
23.637923	1240.572259	15.616755
23.225103	1250.359952	15.621773
23.226003	1259.439536	15.626791
23.426549	1249.126380	15.631808
23.101852	1251.642993	15.636826
23.334097	1253.236747	15.641843
23.834937	1275.709148	15.646861
24.020805	1272.970602	15.651879
24.281049	1269.445312	15.656896
23.955317	1264.600148	15.661914
23.954150	1261.508061	15.666931
24.197613	1244.513205	15.671949
24.206178	1246.441371	15.676967
24.323577	1244.468909	15.681984
23.891474	1244.895182	15.687002
23.931235	1248.335431	15.692019
24.084141	1247.399943	15.697037
23.849529	1249.233889	15.702055
24.158735	1246.761845	15.707072
24.201244	1248.269817	15.712090
23.777343	1254.122487	15.717107
23.892181	1250.609953	15.722125
23.693953	1255.978672	15.727143
24.054639	1258.077043	15.732160
23.843841	1269.739763	15.737178
24.085621	1282.392977	15.742195
24.142924	1280.613957	15.747213
23.727585	1292.303606	15.752231
24.087370	1267.073915	15.757248
24.332481	1275.636947	15.762266
24.425120	1274.197713	15.767283
24.369027	1276.537010	15.772301
24.334767	1276.083797	15.777319
24.569254	1275.238680	15.782336
24.467164	1274.582575	15.787354
24.241892	1271.510414	15.792371
24.390812	1277.252525	15.797389
24.331469	1271.126115	15.802407
24.429640	1275.014520	15.807424
24.073501	1287.229346	15.812442
24.203012	1295.917113	15.817459
24.363281	1306.142636	15.822477
24.587118	1303.261558	15.827495
24.696449	1298.848777	15.832512
24.270199	1305.389629	15.837530
24.566955	1305.840812	15.842547
24.770400	1305.165415	15.847565
24.485407	1312.239466	15.852583
24.673860	1299.208295	15.857600
24.562886	1303.723971	15.862618
25.013866	1307.379337	15.867635
25.071997	1297.652008	15.872653
24.624666	1298.511902	15.877671
24.884074	1305.180116	15.882688
24.841321	1302.928764	15.887706
24.793970	1288.516370	15.892723
25.185867	1293.063808	15.897741
24.805942	1299.231615	15.902759
24.894197	1285.944284	15.907776
24.510695	1297.534947	15.912794
24.951819	1313.255345	15.917811
25.215352	1322.919638	15.922829
25.187514	1319.429229	15.927847
25.576455	1304.545493	15.932864
25.618148	1306.972475	15.937882
25.417948	1286.632530	15.942899
25.665567	1285.659643	15.947917
25.315705	1288.041867	15.952935
25.485806	1291.341567	15.957952
25.468702	1279.559500	15.962970
25.203751	1278.900152	15.967987
25.322377	1282.083607	15.973005
25.242584	1283.031223	15.978023
25.494108	1283.154501	15.983040
25.459349	1280.268775	15.988058
25.330273	1280.328548	15.993075
25.494764	1280.970607	15.998093
25.561733	1284.631925	16.003111
25.603691	1287.612779	16.008128
25.574739	1278.479051	16.013146
25.589264	1280.303084	16.018163
25.849215	1275.948735	16.023181
25.659015	1283.498339	16.028199
25.715442	1270.932428	16.033216
25.550160	1281.854152	16.038234
25.640330	1284.156541	16.043251
26.090768	1278.435928	16.048269
25.375699	1288.991576	16.053287
25.533923	1281.913674	16.058304
25.825337	1277.390320	16.063322
25.612551	1279.308434	16.068339
25.456020	1289.723608	16.073357
25.390969	1282.361175	16.078375
25.432470	1286.673556	16.083392
25.389360	1296.439981	16.088410
25.636831	1307.167529	16.093427
25.750119	1307.599603	16.098445
25.709969	1319.258798	16.103463
25.673356	1327.788768	16.108480
25.735620	1319.769741	16.113498
25.878525	1315.817108	16.118515
25.788460	1319.256512	16.123533
25.648193	1329.258392	16.128551
26.215041	1327.287982	16.133568
26.468846	1338.622748	16.138586
26.322228	1350.276436	16.143603
26.911519	1331.840577	16.148621
26.344072	1317.661057	16.153639
26.212481	1306.865686	16.158656
26.570133	1310.699946	16.163674
26.297318	1317.170813	16.168691
26.552009	1307.078139	16.173709
26.199938	1307.065534	16.178727
26.142010	1304.215149	16.183744
26.371040	1311.642328	16.188762
26.338706	1314.007996	16.193779
26.339110	1310.767611	16.198797
26.386414	1306.285612	16.203815
26.207707	1322.562576	16.208832
26.487149	1335.862704	16.213850
26.126509	1337.675877	16.218867
26.657283	1336.166960	16.223885
26.920293	1342.483028	16.228903
27.077067	1344.936949	16.233920
26.864041	1337.332952	16.238938
26.491848	1326.042536	16.243955
26.738913	1320.491534	16.248973
26.954030	1329.553268	16.253991
26.842529	1321.792249	16.259008
26.674864	1300.615801	16.264026
26.701260	1319.523938	16.269043
26.629094	1326.768126	16.274061
26.511009	1335.041178	16.279079
26.828295	1339.779372	16.284096
26.588533	1331.558581	16.289114
26.883285	1332.821490	16.294131
27.030823	1330.777081	16.299149
26.549870	1336.982561	16.304167
26.580482	1349.183543	16.309184
27.074918	1335.464886	16.314202
26.691841	1355.969036	16.319219
26.894691	1346.951852	16.324237
27.378294	1360.806631	16.329255
27.100351	1371.858165	16.334272
27.416703	1362.392197	16.339290
27.214710	1354.332040	16.344307
26.895058	1350.468487	16.349325
27.425707	1361.268685	16.354343
27.172627	1367.486694	16.359360
27.523553	1359.197625	16.364378
27.325960	1368.061453	16.369395
27.588239	1359.545786	16.374413
27.568957	1361.902206	16.379431
27.431993	1358.927550	16.384448
27.547691	1346.145040	16.389466
27.745681	1333.335082	16.394483
27.504808	1322.013787	16.399501
27.699065	1328.250728	16.404519
27.286402	1328.858411	16.409536
27.559479	1329.806823	16.414554
27.641621	1346.506976	16.419571
27.679457	1349.995598	16.424589
27.222539	1345.924160	16.429607
27.909461	1343.756630	16.434624
27.794344	1345.618755	16.439642
28.048291	1355.785435	16.444659
27.714931	1350.054136	16.449677
27.877514	1352.316153	16.454695
27.861496	1363.436346	16.459712
27.902421	1351.085540	16.464730
28.104425	1364.394626	16.469747
27.702914	1354.481071	16.474765
27.978826	1356.873854	16.479783
27.782202	1348.646276	16.484800
27.917195	1355.409600	16.489818
27.777647	1353.479439	16.494835
28.028082	1358.765350	16.499853
27.966929	1352.191583	16.504871
27.995010	1349.737906	16.509888
27.929782	1352.206682	16.514906
27.642816	1345.684625	16.519923
27.832289	1348.966551	16.524941
27.874237	1349.095533	16.529959
27.961678	1372.750144	16.534976
27.974058	1383.883347	16.539994
27.968903	1383.963860	16.545011
28.509354	1381.192736	16.550029
28.468293	1382.435092	16.555047
28.361003	1381.681817	16.560064
28.497914	1377.888034	16.565082
28.473168	1386.928649	16.570099
28.423129	1379.456197	16.575117
28.405558	1377.626228	16.580135
28.471115	1373.545102	16.585152
28.459573	1376.608485	16.590170
28.612116	1379.416255	16.595187
28.636278	1380.668635	16.600205
28.826779	1380.163492	16.605223
28.655417	1379.888178	16.610240
28.409170	1383.083092	16.615258
28.612253	1388.064687	16.620275
28.573751	1380.645434	16.625293
28.758600	1366.386885	16.630311
28.723490	1376.466196	16.635328
28.861909	1381.545149	16.640346
28.672178	1382.320891	16.645363
28.520290	1373.900043	16.650381
29.038031	1374.933771	16.655399
28.483026	1377.918200	16.660416
28.540007	1383.963421	16.665434
28.867336	1403.778702	16.670451
28.916289	1407.640677	16.675469
29.260301	1409.195397	16.680487
28.914870	1402.300760	16.685504
29.251077	1401.335189	16.690522
29.138552	1404.688190	16.695539
28.988266	1407.229379	16.700557
29.520242	1406.464333	16.705575
29.296257	1410.678754	16.710592
29.164213	1412.679917	16.715610
29.428778	1403.893381	16.720627
29.292315	1407.808222	16.725645
29.393691	1405.569512	16.730663
29.223361	1407.873882	16.735680
29.367263	1404.008460	16.740698
29.241182	1397.933248	16.745715
29.109442	1406.169239	16.750733
29.342123	1401.375698	16.755751
29.140253	1407.789930	16.760768
29.183279	1404.690862	16.765786
29.529235	1403.938232	16.770803
29.559460	1411.307955	16.775821
29.535661	1424.332587	16.780839
29.405852	1436.658332	16.785856
29.837353	1430.313267	16.790874
29.934862	1439.672954	16.795891
29.978293	1430.858593	16.800909
30.030384	1425.502557	16.805927
29.546675	1401.757306	16.810944
29.603427	1413.886673	16.815962
29.835089	1424.028756	16.820979
29.752390	1429.056685	16.825997
29.941264	1422.729905	16.831015
29.697803	1434.454082	16.836032
29.763640	1427.718627	16.841050
30.191448	1433.984506	16.846067
30.021489	1428.711439	16.851085
29.987914	1427.218762	16.856103
29.639219	1426.861902	16.861120
29.940083	1434.175628	16.866138
30.017102	1426.437158	16.871155
29.749857	1425.099066	16.876173
29.966702	1430.910258	16.881191
30.443069	1447.133978	16.886208
30.179461	1434.227439	16.891226
30.369600	1439.693081	16.896243
30.361656	1444.319229	16.901261
30.610659	1433.927032	16.906279
30.445753	1426.098462	16.911296
30.320796	1422.780468	16.916314
30.114026	1419.082776	16.921331
30.254955	1435.026814	16.926349
30.847205	1446.560517	16.931367
30.339036	1444.249107	16.936384
30.489358	1455.526358	16.941402
30.716470	1442.275654	16.946419
30.448498	1449.689843	16.951437
30.726352	1441.494764	16.956455
30.582445	1439.470438	16.961472
30.681769	1441.296930	16.966490
31.064016	1439.443410	16.971507
30.853292	1450.981059	16.976525
30.920874	1438.414340	16.981543
30.905219	1445.796037	16.986560
30.948339	1438.409250	16.991578
31.146856	1442.024332	16.996595
30.713954	1428.331782	17.001613
31.038398	1422.874573	17.006631
30.958689	1438.356482	17.011648
30.825394	1431.412792	17.016666
31.356970	1435.087469	17.021683
30.962148	1443.721531	17.026701
30.909134	1440.436062	17.031719
31.191236	1432.181228	17.036736
31.079159	1432.941703	17.041754
30.879366	1428.554677	17.046771
30.900494	1438.548303	17.051789
31.124847	1437.767854	17.056807
31.146301	1437.385294	17.061824
30.905644	1441.669029	17.066842
30.916601	1432.960062	17.071859
30.940754	1447.617256	17.076877
31.161422	1458.159605	17.081895
31.212332	1469.258513	17.086912
31.187070	1477.487079	17.091930
31.605738	1464.450180	17.096947
31.599981	1462.572963	17.101965
31.414424	1472.004128	17.106983
31.368579	1468.696203	17.112000
31.228440	1467.657839	17.117018
31.633428	1469.608328	17.122035
31.498398	1463.379070	17.127053
31.719413	1464.469999	17.132071
31.809213	1467.338607	17.137088
31.528198	1473.469570	17.142106
31.960491	1475.497015	17.147123
31.978621	1490.990273	17.152141
31.967640	1488.738731	17.157159
32.031181	1485.802376	17.162176
31.747688	1478.469858	17.167194
31.986241	1477.219340	17.172211
32.125916	1495.384863	17.177229
32.040348	1492.005977	17.182247
32.130916	1490.841077	17.187264
32.109321	1500.527285	17.192282
32.458231	1482.554818	17.197299
31.778269	1480.368411	17.202317
31.783373	1489.135626	17.207335
31.943434	1488.847740	17.212352
32.007811	1495.483495	17.217370
32.495515	1493.901805	17.222387
32.556375	1494.070557	17.227405
32.005051	1493.372973	17.232423
32.700990	1483.630850	17.237440
32.357305	1495.443383	17.242458
32.417464	1484.239645	17.247475
32.447485	1491.918489	17.252493
32.364308	1500.539364	17.257511
32.561395	1491.018340	17.262528
32.328250	1489.656858	17.267546
32.559770	1488.541757	17.272563
32.084034	1487.137135	17.277581
32.326527	1499.047511	17.282599
32.654870	1490.876691	17.287616
32.264950	1509.294820	17.292634
32.716279	1511.815948	17.297651
32.541595	1528.045609	17.302669
32.931032	1522.318118	17.307687
33.096190	1526.104902	17.312704
32.993604	1528.104333	17.317722
33.214384	1517.119539	17.322739
32.944486	1521.069185	17.327757
32.977354	1521.883523	17.332775
32.995765	1523.561667	17.337792
33.003665	1522.034922	17.342810
33.574963	1513.040650	17.347827
33.028310	1513.869426	17.352845
32.908748	1511.302077	17.357863
33.416062	1503.923928	17.362880
33.020964	1511.374237	17.367898
33.451325	1514.741354	17.372915
33.134358	1507.112030	17.377933
33.545475	1510.623288	17.382951
33.795082	1508.250084	17.387968
33.074685	1502.918092	17.392986
33.498371	1494.718825	17.398003
33.256584	1508.681711	17.403021
33.306441	1503.522472	17.408039
33.668011	1503.675099	17.413056
33.393967	1516.774474	17.418074
33.262779	1505.039544	17.423091
33.331941	1507.296640	17.428109
33.367635	1504.785768	17.433127
33.614376	1502.928780	17.438144
33.113486	1508.706941	17.443162
33.329811	1510.529742	17.448179
33.426112	1514.709064	17.453197
33.803752	1531.004007	17.458215
34.021765	1535.691048	17.463232
34.077018	1531.603325	17.468250
33.999390	1534.683629	17.473267
33.855367	1536.337987	17.478285
33.947386	1537.758232	17.483303
34.180914	1531.692485	17.488320
33.977997	1536.495554	17.493338
34.224874	1518.811260	17.498355
34.392582	1527.026675	17.503373
34.110833	1532.986526	17.508391
34.508429	1526.062029	17.513408
34.173412	1523.778517	17.518426
34.356627	1521.889174	17.523443
34.308773	1511.421073	17.528461
34.207205	1514.746293	17.533479
34.312984	1516.043385	17.538496
34.318821	1520.512543	17.543514
34.398363	1522.983661	17.548531
34.571298	1531.568675	17.553549
34.099173	1525.322589	17.558567
34.688391	1522.659475	17.563584
34.494732	1522.999270	17.568602
34.642007	1524.551665	17.573619
34.826179	1519.300018	17.578637
34.654489	1517.280299	17.583655
34.834097	1516.392719	17.588672
34.396259	1525.148540	17.593690
34.873280	1511.069244	17.598707
34.936460	1517.607572	17.603725
34.524294	1518.393915	17.608743
34.829006	1515.106056	17.613760
34.820655	1513.653665	17.618778
34.702585	1513.286815	17.623795
34.784577	1519.698397	17.628813
34.707284	1521.314890	17.633831
34.853393	1511.243282	17.638848
34.835365	1521.581653	17.643866
34.644401	1524.216235	17.648883
34.747751	1526.005062	17.653901
34.729792	1541.022093	17.658919
35.581981	1549.299336	17.663936
35.114836	1553.995544	17.668954
35.150154	1549.504837	17.673971
35.488016	1545.729580	17.678989
35.234758	1544.548205	17.684007
35.423027	1553.812562	17.689024
35.371343	1545.322209	17.694042
35.182416	1548.056848	17.699059
35.471634	1550.393120	17.704077
35.016265	1547.450092	17.709095
35.177393	1545.868349	17.714112
35.134294	1542.861127	17.719130
35.172202	1541.461673	17.724147
34.639338	1558.693405	17.729165
34.917226	1573.093585	17.734183
35.309794	1571.239122	17.739200
35.297007	1578.419227	17.744218
35.960777	1598.945755	17.749235
36.051482	1596.619816	17.754253
36.215462	1584.980250	17.759271
36.054031	1575.704590	17.764288
36.045934	1565.575115	17.769306
35.960127	1562.554516	17.774323
36.399944	1555.750939	17.779341
36.176165	1559.958673	17.784359
36.038215	1561.334862	17.789376
35.953936	1563.652510	17.794394
36.157696	1562.519184	17.799411
36.513416	1560.385418	17.804429
36.785611	1561.415880	17.809447
36.398274	1559.009565	17.814464
36.458726	1560.117741	17.819482
36.253099	1558.821363	17.824499
36.464271	1557.298228	17.829517
36.246403	1562.751812	17.834535
36.428584	1561.475618	17.839552
36.782925	1552.823286	17.844570
36.541796	1555.897701	17.849587
36.748654	1559.636618	17.854605
35.984825	1556.962966	17.859623
36.420677	1558.717395	17.864640
36.434803	1563.380855	17.869658
36.377365	1557.868571	17.874675
36.737670	1550.699872	17.879693
36.462586	1561.860906	17.884711
36.711919	1566.923060	17.889728
36.920779	1573.369482	17.894746
36.779944	1592.826608	17.899763
37.219622	1585.279744	17.904781
36.904355	1582.715779	17.909799
36.874964	1571.372533	17.914816
36.625404	1577.018788	17.919834
36.667837	1591.719536	17.924851
37.286974	1594.751361	17.929869
37.034447	1592.456095	17.934887
37.071527	1594.224449	17.939904
37.270737	1590.421834	17.944922
37.350973	1605.234813	17.949939
37.433674	1589.213534	17.954957
37.044155	1601.587302	17.959975
37.394499	1589.108893	17.964992
37.055789	1595.281776	17.970010
36.937982	1584.631949	17.975027
37.433709	1585.579983	17.980045
37.395911	1597.178367	17.985063
37.129066	1591.709146	17.990080
37.098194	1596.639933	17.995098
37.178052	1591.620558	18.000115
37.444280	1600.737735	18.005133
37.476115	1627.988153	18.010151
37.505968	1614.242537	18.015168
37.651765	1627.603713	18.020186
37.454689	1618.768198	18.025203
37.746279	1620.387167	18.030221
37.640610	1630.242152	18.035239
37.544581	1613.055687	18.040256
37.614662	1620.938171	18.045274
37.531487	1614.247482	18.050291
37.657207	1635.071362	18.055309
37.896713	1637.171032	18.060327
38.287100	1645.645557	18.065344
38.421870	1634.584819	18.070362
38.270164	1636.716049	18.075379
38.669244	1621.818516	18.080397
38.607052	1625.420675	18.085415
38.305731	1607.780549	18.090432
38.506434	1598.211222	18.095450
38.164710	1600.338992	18.100467
38.675730	1594.701501	18.105485
38.464296	1598.054842	18.110503
38.525130	1592.526431	18.115520
38.717320	1595.219778	18.120538
38.219470	1597.323893	18.125555
38.707736	1589.497695	18.130573
38.241197	1598.363837	18.135591
38.277028	1591.183305	18.140608
38.779064	1607.449385	18.145626
38.753392	1619.166241	18.150643
38.908412	1629.396001	18.155661
39.103513	1625.127137	18.160679
38.865195	1603.212419	18.165696
38.747463	1604.562023	18.170714
38.956584	1603.919923	18.175731
38.883287	1602.348006	18.180749
39.135816	1618.515413	18.185767
38.762754	1610.733159	18.190784
38.888311	1618.095403	18.195802
38.850364	1621.629360	18.200819
39.149968	1617.485252	18.205837
39.072149	1621.170322	18.210855
38.989904	1627.736018	18.215872
38.952652	1630.217117	18.220890
38.773023	1617.263789	18.225907
39.102680	1620.512237	18.230925
39.146852	1629.070678	18.235943
39.438710	1637.300555	18.240960
39.359108	1640.498924	18.245978
39.114746	1652.293098	18.250995
39.436251	1651.951604	18.256013
39.521988	1641.533257	18.261031
39.502966	1646.682562	18.266048
39.626763	1648.741229	18.271066
39.544927	1651.497850	18.276083
39.636821	1645.142218	18.281101
39.340398	1647.497502	18.286119
39.548909	1646.505505	18.291136
39.729335	1650.124823	18.296154
39.761007	1655.624362	18.301171
39.873814	1652.016014	18.306189
39.814518	1647.405180	18.311207
39.807222	1650.729326	18.316224
39.790364	1644.627595	18.321242
39.677931	1661.222241	18.326259
40.130296	1675.275802	18.331277
40.175479	1677.840057	18.336295
40.131956	1678.980090	18.341312
40.536127	1666.259210	18.346330
40.397571	1678.433452	18.351347
40.205746	1671.203322	18.356365
40.780229	1669.216643	18.361383
40.144482	1660.567797	18.366400
40.296562	1675.252367	18.371418
40.401131	1671.372944	18.376435
40.931669	1667.101857	18.381453
40.691555	1655.875858	18.386471
40.538634	1651.554991	18.391488
40.672477	1654.972607	18.396506
40.926441	1647.927444	18.401523
40.661684	1633.866214	18.406541
40.670403	1635.562910	18.411559
40.529910	1639.512336	18.416576
40.712698	1654.220522	18.421594
40.670663	1663.948812	18.426611
40.978035	1657.284921	18.431629
41.173527	1664.861939	18.436647
41.286498	1659.413027	18.441664
40.959485	1664.751324	18.446682
40.862536	1667.130541	18.451699
41.036829	1660.276565	18.456717
40.765885	1666.429552	18.461735
41.291320	1661.281369	18.466752
41.381252	1656.943363	18.471770
41.048785	1667.036067	18.476787
41.156232	1664.856154	18.481805
41.070325	1663.895376	18.486823
41.196800	1654.247407	18.491840
41.204150	1663.119071	18.496858
41.488363	1660.938122	18.501875
40.960541	1662.850379	18.506893
41.343468	1673.392283	18.511911
41.216913	1684.599583	18.516928
41.471111	1682.301968	18.521946
41.412412	1693.044849	18.526963
41.638730	1684.844036	18.531981
41.459204	1694.687323	18.536999
41.129088	1699.305679	18.542016
41.459102	1694.365951	18.547034
41.442541	1715.555319	18.552051
41.668806	1712.854471	18.557069
41.829388	1710.833828	18.562087
41.676554	1713.075098	18.567104
42.214393	1697.746950	18.572122
42.599999	1710.611648	18.577139
42.135594	1704.750423	18.582157
42.260382	1704.035722	18.587175
42.498733	1710.127302	18.592192
42.550162	1702.909874	18.597210
42.570960	1699.058147	18.602227
42.211308	1704.424323	18.607245
42.525930	1703.679645	18.612263
42.187251	1693.848732	18.617280
42.156491	1705.621223	18.622298
42.381344	1703.469033	18.627315
42.216491	1699.050137	18.632333
42.381872	1702.194019	18.637351
42.159881	1704.317256	18.642368
42.227064	1699.056254	18.647386
42.577558	1711.555138	18.652403
42.379371	1730.859372	18.657421
42.987375	1724.326585	18.662439
43.033401	1735.179253	18.667456
43.158758	1732.328246	18.672474
43.024671	1734.220341	18.677491
42.894963	1729.159771	18.682509
43.124534	1728.149701	18.687527
42.948467	1735.618828	18.692544
43.354194	1728.202736	18.697562
43.538784	1716.273427	18.702579
43.082103	1703.806624	18.707597
43.215518	1696.398407	18.712615
42.773394	1706.515269	18.717632
43.323823	1707.188867	18.722650
43.289400	1725.789108	18.727667
43.356334	1726.644252	18.732685
43.463556	1723.531694	18.737703
43.084219	1735.126320	18.742720
43.536529	1724.086361	18.747738
43.785246	1724.040427	18.752755
43.477678	1731.793220	18.757773
43.591078	1728.246959	18.762791
43.608813	1741.791330	18.767808
43.354369	1736.329838	18.772826
43.390330	1727.359858	18.777843
43.265924	1729.888136	18.782861
43.590388	1733.046528	18.787879
43.214261	1750.935487	18.792896
43.631681	1757.688659	18.797914
43.577284	1755.855317	18.802931
43.907904	1759.888673	18.807949
43.785552	1757.392218	18.812967
43.551175	1757.873824	18.817984
43.822317	1777.735933	18.823002
44.029035	1792.540667	18.828019
43.871021	1787.961160	18.833037
44.117724	1775.024238	18.838055
44.434442	1781.630379	18.843072
44.322539	1782.432967	18.848090
44.646508	1772.952493	18.853107
44.405535	1778.961565	18.858125
44.415318	1772.988427	18.863143
44.448573	1787.249547	18.868160
44.465640	1780.762990	18.873178
44.707025	1773.334035	18.878195
44.672958	1783.740995	18.883213
44.864646	1775.407308	18.888231
44.641699	1785.033066	18.893248
44.563026	1779.804942	18.898266
44.807704	1787.475813	18.903283
44.961099	1803.681546	18.908301
45.202590	1807.253744	18.913319
45.371053	1801.587290	18.918336
45.129910	1776.605867	18.923354
45.201650	1776.877145	18.928371
44.981958	1772.004745	18.933389
45.165605	1764.056652	18.938407
45.200642	1780.402111	18.943424
45.376706	1788.088718	18.948442
45.562996	1779.325612	18.953459
45.516045	1767.483961	18.958477
45.717149	1762.103041	18.963495
45.389535	1755.265125	18.968512
45.427369	1757.169198	18.973530
45.369173	1757.901441	18.978547
45.342518	1765.049686	18.983565
45.493114	1758.394882	18.988583
45.539097	1767.720812	18.993600
45.346176	1776.809292	18.998618
45.725229	1795.467663	19.003635
45.768283	1784.678755	19.008653
45.648910	1777.667241	19.013671
45.990112	1793.094897	19.018688
45.767482	1784.701724	19.023706
45.867206	1788.486851	19.028723
45.805338	1786.813015	19.033741
45.762402	1784.192332	19.038759
46.149577	1777.155678	19.043776
45.838631	1789.700393	19.048794
45.806692	1782.215288	19.053811
45.659079	1800.454905	19.058829
45.953609	1808.480099	19.063847
46.171453	1807.707802	19.068864
45.833221	1819.506681	19.073882
46.095882	1814.919055	19.078899
46.182287	1824.217435	19.083917
46.430289	1829.087377	19.088935
46.334477	1840.261726	19.093952
46.413024	1840.103132	19.098970
47.249734	1846.095705	19.103987
47.096438	1844.885092	19.109005
47.305239	1831.350878	19.114023
47.371598	1820.326576	19.119040
47.180925	1820.266667	19.124058
47.182198	1807.737048	19.129075
46.957019	1806.391536	19.134093
46.882827	1801.388643	19.139111
47.070560	1811.484740	19.144128
47.098515	1802.849119	19.149146
46.868434	1803.191430	19.154163
47.091493	1807.592676	19.159181
47.213878	1812.756721	19.164199
46.962280	1804.567958	19.169216
47.065791	1801.023325	19.174234
47.285183	1815.763376	19.179251
47.003883	1836.954393	19.184269
47.296401	1845.481911	19.189287
47.234970	1838.041839	19.194304
47.070731	1838.424782	19.199322
47.146060	1832.620253	19.204339
47.244462	1838.093018	19.209357
47.403090	1846.373105	19.214375
47.588314	1855.490511	19.219392
47.645254	1862.881994	19.224410
47.812965	1858.040058	19.229427
47.811898	1863.404954	19.234445
48.084664	1871.250727	19.239463
48.070217	1859.900456	19.244480
47.822140	1868.376895	19.249498
48.031967	1856.479505	19.254515
48.091056	1861.252510	19.259533
48.383706	1861.610300	19.264551
48.257148	1868.350786	19.269568
47.992837	1857.741657	19.274586
48.381827	1861.991717	19.279603
48.181798	1865.582590	19.284621
48.366686	1852.890132	19.289639
48.097896	1851.936117	19.294656
48.528464	1863.655277	19.299674
48.541450	1855.380778	19.304691
47.836489	1851.435863	19.309709
48.376166	1865.875876	19.314727
48.477449	1867.619810	19.319744
48.852913	1862.393734	19.324762
49.410168	1867.422918	19.329779
49.638128	1861.532773	19.334797
48.943397	1854.836147	19.339815
49.147114	1833.385034	19.344832
49.596828	1837.463577	19.349850
49.494661	1830.522800	19.354867
49.276718	1836.064680	19.359885
49.227074	1833.085655	19.364903
49.672517	1832.156628	19.369920
49.408417	1835.253419	19.374938
49.433291	1830.329326	19.379955
49.223134	1828.538007	19.384973
49.088423	1827.223912	19.389991
49.119287	1825.340564	19.395008
49.180822	1842.352158	19.400026
49.620073	1835.500523	19.405043
49.286435	1840.009663	19.410061
49.298907	1830.599826	19.415079
49.429255	1828.484981	19.420096
48.970857	1834.857380	19.425114
49.419123	1843.360191	19.430131
49.410937	1862.062140	19.435149
49.361002	1869.089104	19.440167
49.356692	1868.206877	19.445184
49.413610	1874.358206	19.450202
49.540156	1889.800378	19.455219
49.764491	1902.795192	19.460237
49.677584	1892.184505	19.465255
50.139566	1886.286163	19.470272
50.087787	1890.048071	19.475290
50.011647	1890.544326	19.480307
50.220199	1890.466486	19.485325
50.177998	1874.295199	19.490343
50.293462	1888.993146	19.495360
50.237166	1892.264464	19.500378
50.708150	1911.949040	19.505395
50.961202	1915.235482	19.510413
50.723082	1909.256251	19.515431
50.654963	1894.092802	19.520448
50.640975	1889.062158	19.525466
50.792445	1899.584421	19.530483
50.960834	1899.458532	19.535501
50.900070	1905.674316	19.540519
50.924029	1899.584992	19.545536
50.858041	1900.005149	19.550554
50.932122	1917.778131	19.555571
50.972770	1915.100226	19.560589
51.143769	1913.571531	19.565607
51.323707	1924.007582	19.570624
50.755559	1914.272544	19.575642
51.060650	1914.600708	19.580659
51.050650	1914.048954	19.585677
51.217086	1920.071468	19.590695
51.095630	1908.875168	19.595712
51.182017	1914.699172	19.600730
51.000405	1912.700734	19.605747
51.220035	1929.319608	19.610765
51.270161	1934.602398	19.615783
51.406955	1946.636595	19.620800
51.414406	1945.472091	19.625818
51.715627	1935.722855	19.630835
51.869134	1939.333725	19.635853
51.868720	1948.811178	19.640871
51.979882	1934.635224	19.645888
51.503651	1938.680293	19.650906
51.960135	1943.352626	19.655923
51.972028	1934.821177	19.660941
51.590335	1936.564686	19.665959
52.264593	1956.921839	19.670976
51.944535	1961.574821	19.675994
52.147052	1969.368540	19.681011
52.570845	1961.715474	19.686029
52.539446	1962.657055	19.691047
52.281498	1964.716223	19.696064
52.518741	1967.405691	19.701082
52.421918	1973.092450	19.706099
52.756844	1970.628618	19.711117
52.851066	1973.191464	19.716135
52.708795	1959.094619	19.721152
52.592502	1963.668851	19.726170
52.536329	1968.029547	19.731187
52.748477	1965.058165	19.736205
52.519750	1959.192314	19.741223
52.674075	1964.755042	19.746240
52.471251	1966.834183	19.751258
52.496585	1970.460458	19.756275
52.935248	1989.702863	19.761293
52.719153	1998.176812	19.766311
53.117262	1988.308289	19.771328
52.851590	1995.691251	19.776346
52.883315	1994.417590	19.781363
53.261786	2000.912379	19.786381
52.958497	2017.459992	19.791399
53.403957	2008.868644	19.796416
53.208771	2023.288818	19.801434
53.616227	2018.709351	19.806451
53.730161	2022.016577	19.811469
53.837514	2031.788378	19.816487
53.928026	2010.637731	19.821504
53.800796	2025.404886	19.826522
53.527586	2009.452172	19.831539
53.749400	2021.491587	19.836557
53.566584	2022.270934	19.841575
53.946842	2019.364121	19.846592
53.940544	2025.000813	19.851610
53.800126	2017.660399	19.856627
54.344557	2030.027306	19.861645
54.343529	2034.057590	19.866663
54.300972	2039.468814	19.871680
54.279439	2048.420302	19.876698
54.449980	2042.169942	19.881715
54.933534	2024.332743	19.886733
54.795104	2024.502341	19.891751
55.145457	2006.962108	19.896768
54.793768	1994.164228	19.901786
54.575143	1997.541291	19.906803
55.012792	1994.093047	19.911821
55.013173	1994.394694	19.916839
55.062282	1995.161082	19.921856
54.835357	1995.169402	19.926874
54.990810	1992.009798	19.931891
55.012075	1993.831221	19.936909
54.778806	1996.118184	19.941927
55.237034	1991.783045	19.946944
55.645648	1992.791258	19.951962
55.187006	1993.131009	19.956979
55.395465	1991.290171	19.961997
55.098795	2000.673982	19.967015
54.954881	1989.701832	19.972032
55.349561	1994.601779	19.977050
54.917246	1998.737597	19.982067
55.302036	2002.359252	19.987085
55.246679	2017.598712	19.992103
55.103231	2015.166746	19.997120
55.490990	2027.365201	20.002138
55.449708	2027.654875	20.007155
55.515920	2030.249945	20.012173
55.222777	2034.609101	20.017191
55.572496	2014.841765	20.022208
55.610952	2044.823743	20.027226
55.691693	2057.291759	20.032243
55.756295	2059.456779	20.037261
56.079929	2066.141029	20.042279
56.357313	2052.661367	20.047296
56.164479	2058.410572	20.052314
56.063010	2061.247695	20.057331
56.443778	2054.386788	20.062349
55.862617	2060.196995	20.067367
55.902133	2061.787435	20.072384
56.385996	2080.796060	20.077402
56.106957	2085.465882	20.082419
56.345751	2075.929696	20.087437
56.578997	2084.685312	20.092455
56.807398	2084.518345	20.097472
57.147370	2079.206362	20.102490
56.944319	2081.302091	20.107507
57.123617	2076.455406	20.112525
56.911765	2092.205603	20.117543
57.265572	2074.858818	20.122560
57.107219	2074.280140	20.127578
56.940597	2085.274699	20.132595
57.222791	2081.090843	20.137613
57.016026	2085.306126	20.142631
57.190881	2068.377287	20.147648
57.354005	2069.223943	20.152666
57.093859	2080.022621	20.157683
57.433640	2073.725221	20.162701
57.441661	2088.916421	20.167719
57.970255	2085.118784	20.172736
57.927588	2079.534960	20.177754
57.487529	2081.682680	20.182771
57.714347	2082.961278	20.187789
57.866204	2103.748373	20.192807
57.840665	2097.404201	20.197824
57.932458	2099.825737	20.202842
58.117071	2095.536834	20.207859
57.752187	2099.532334	20.212877
58.090562	2098.875031	20.217895
58.099775	2098.229918	20.222912
58.359856	2097.579330	20.227930
58.001314	2103.125381	20.232947
58.172877	2083.533635	20.237965
58.049093	2091.481259	20.242983
58.010524	2090.530302	20.248000
58.399790	2096.310333	20.253018
58.010398	2113.523159	20.258035
58.617055	2117.725695	20.263053
58.381625	2121.367000	20.268071
58.540751	2116.792952	20.273088
58.510938	2125.214748	20.278106
58.644777	2123.877645	20.283123
58.448698	2114.133001	20.288141
58.646247	2136.162570	20.293159
58.817394	2144.624205	20.298176
58.942502	2143.762973	20.303194
59.064451	2152.150503	20.308211
59.469178	2135.784580	20.313229
59.503346	2139.740142	20.318247
59.173449	2128.348402	20.323264
59.650674	2124.903002	20.328282
59.632377	2131.821675	20.333299
60.338650	2124.766475	20.338317
60.073245	2106.855629	20.343335
59.448661	2097.126310	20.348352
59.596489	2086.074892	20.353370
59.599939	2094.799810	20.358387
59.641698	2093.312658	20.363405
59.774785	2094.074148	20.368423
59.987278	2104.942321	20.373440
59.960755	2113.482858	20.378458
59.966643	2124.890513	20.383475
59.899453	2131.590142	20.388493
60.134646	2124.966791	20.393511
59.951336	2129.352600	20.398528
60.172074	2121.033979	20.403546
60.106793	2118.464199	20.408563
60.029957	2113.629759	20.413581
60.081985	2124.325793	20.418599
60.153348	2116.886744	20.423616
60.393354	2125.931031	20.428634
60.143401	2145.194382	20.433651
60.180838	2148.980108	20.438669
60.069063	2140.004917	20.443687
60.345446	2148.141182	20.448704
60.614256	2156.272411	20.453722
60.975542	2170.335264	20.458739
61.553396	2168.449151	20.463757
61.187493	2166.643913	20.468775
61.392042	2164.680080	20.473792
61.431745	2139.841159	20.478810
61.498668	2144.232233	20.483827
61.692531	2130.398268	20.488845
61.659695	2131.920818	20.493863
61.381190	2137.043333	20.498880
61.381437	2130.213749	20.503898
60.889945	2133.427527	20.508915
60.871124	2142.413265	20.513933
61.276877	2154.791906	20.518951
61.282196	2168.019808	20.523968
61.404918	2165.035298	20.528986
61.472868	2173.610560	20.534003
61.774187	2182.233262	20.539021
62.203700	2190.822850	20.544039
61.744718	2192.607185	20.549056
62.029983	2198.131698	20.554074
61.993833	2189.369112	20.559091
61.886691	2188.678372	20.564109
62.239559	2188.395439	20.569127
62.055059	2201.596649	20.574144
62.220090	2189.994646	20.579162
62.061490	2184.681241	20.584179
62.241383	2191.377625	20.589197
62.252053	2205.425950	20.594215
62.426615	2219.241923	20.599232
62.841774	2213.548885	20.604250
62.592587	2217.935432	20.609267
62.324887	2220.396658	20.614285
62.745812	2225.417517	20.619303
62.606934	2230.081804	20.624320
62.791995	2220.339494	20.629338
62.956879	2237.021736	20.634355
63.110317	2246.492698	20.639373
63.115041	2252.650096	20.644391
63.276080	2249.648178	20.649408
63.523321	2248.374109	20.654426
63.600824	2251.086241	20.659443
63.365466	2248.868339	20.664461
63.754116	2243.162767	20.669479
63.664695	2245.277821	20.674496
63.848967	2231.630011	20.679514
63.834937	2238.459831	20.684531
63.354113	2234.426771	20.689549
63.633571	2231.215406	20.694567
63.515666	2245.874917	20.699584
63.991205	2237.987914	20.704602
63.758475	2244.222966	20.709619
63.802631	2238.467563	20.714637
63.869153	2244.423343	20.719655
63.798652	2238.599593	20.724672
64.168373	2238.616229	20.729690
64.068568	2258.377219	20.734707
64.310256	2272.535244	20.739725
64.609892	2262.669530	20.744743
64.130582	2262.717829	20.749760
64.568442	2255.798525	20.754778
64.218878	2257.289083	20.759795
64.306701	2251.061049	20.764813
64.469513	2258.768205	20.769831
64.586990	2279.040368	20.774848
64.450925	2287.093679	20.779866
64.958332	2288.006751	20.784883
64.776689	2286.670494	20.789901
65.161095	2292.823466	20.794919
65.180116	2286.884028	20.799936
65.271765	2284.427512	20.804954
65.182592	2291.904510	20.809971
65.165851	2278.925128	20.814989
65.136113	2275.433638	20.820007
64.746301	2284.332297	20.825024
65.488227	2296.952824	20.830042
65.728227	2316.540083	20.835059
65.510895	2312.835268	20.840077
65.936056	2307.941741	20.845095
65.806302	2317.911799	20.850112
65.767396	2308.220832	20.855130
65.794186	2310.920143	20.860147
65.715330	2311.694823	20.865165
65.994062	2308.313478	20.870183
65.903504	2312.149259	20.875200
66.143728	2314.178035	20.880218
66.021404	2330.110056	20.885235
65.669445	2331.398255	20.890253
66.315017	2338.862608	20.895271
66.418774	2334.324078	20.900288
66.479330	2331.783349	20.905306
66.820541	2334.826088	20.910323
66.823646	2330.042862	20.915341
66.764796	2330.480348	20.920359
66.669198	2331.746805	20.925376
66.624045	2323.867559	20.930394
66.928131	2340.750013	20.935411
66.999269	2329.510769	20.940429
67.197289	2325.968813	20.945447
66.870017	2340.871881	20.950464
67.312345	2353.661939	20.955482
67.606380	2354.203772	20.960499
66.915595	2364.694681	20.965517
67.811226	2353.636504	20.970535
67.345137	2356.598064	20.975552
67.418928	2355.371321	20.980570
67.613289	2351.315776	20.985587
67.497032	2354.225884	20.990605
67.687788	2353.401763	20.995623
67.828313	2349.916997	21.000640
67.804719	2348.596594	21.005658
67.498663	2349.847243	21.010675
67.727479	2353.858306	21.015693
68.013351	2347.316992	21.020711
67.811554	2354.827307	21.025728
68.033150	2349.688851	21.030746
67.899144	2367.054792	21.035763
67.869022	2369.883655	21.040781
68.534215	2377.927465	21.045799
68.510417	2372.450246	21.050816
68.407910	2370.153551	21.055834
68.710766	2367.537110	21.060851
68.430526	2379.098810	21.065869
68.807844	2369.535090	21.070887
68.905775	2374.782131	21.075904
68.834634	2370.242738	21.080922
68.741716	2375.101011	21.085939
68.812203	2377.922602	21.090957
69.104969	2368.274508	21.095975
68.715812	2383.181995	21.100992
68.806560	2397.717990	21.106010
69.046547	2400.112186	21.111027
68.956863	2403.578538	21.116045
69.081477	2401.881121	21.121063
69.285903	2404.901725	21.126080
69.344230	2394.578378	21.131098
69.840743	2410.424163	21.136115
70.028647	2428.274878	21.141133
69.960512	2414.715713	21.146151
69.758898	2399.941688	21.151168
69.674355	2412.199262	21.156186
69.861154	2416.736243	21.161203
69.847417	2414.511010	21.166221
70.158607	2415.535447	21.171239
69.836422	2417.618735	21.176256
70.074448	2425.538285	21.181274
70.206813	2425.492793	21.186291
70.270062	2416.640720	21.191309
70.185444	2405.733620	21.196327
70.312357	2423.196420	21.201344
70.442867	2439.353863	21.206362
70.946427	2448.993144	21.211379
70.700666	2451.677934	21.216397
70.873037	2448.738664	21.221415
70.833659	2448.689826	21.226432
71.159227	2448.341739	21.231450
71.077484	2440.411033	21.236467
71.205762	2449.110284	21.241485
71.598517	2434.661866	21.246503
71.193399	2446.319178	21.251520
71.544139	2434.938500	21.256538
71.655707	2448.227331	21.261555
71.505507	2442.928977	21.266573
71.759576	2437.068531	21.271591
71.627337	2438.359590	21.276608
71.966445	2440.140444	21.281626
71.775901	2438.248543	21.286643
71.536918	2438.315561	21.291661
71.564165	2436.496523	21.296679
71.470654	2436.829532	21.301696
71.440010	2438.216703	21.306714
71.564643	2445.422796	21.311731
71.426217	2456.406630	21.316749
71.578963	2446.530174	21.321767
71.518233	2457.466447	21.326784
71.502999	2488.442499	21.331802
72.005081	2482.466008	21.336819
71.896647	2492.016473	21.341837
72.079228	2496.888446	21.346855
72.773831	2518.435534	21.351872
72.640791	2522.853257	21.356890
73.108698	2515.407168	21.361907
73.246039	2521.856819	21.366925
73.746242	2506.618393	21.371943
73.386659	2484.353668	21.376960
73.424117	2483.647936	21.381978
73.622556	2463.219320	21.386995
73.544365	2477.648817	21.392013
73.266691	2477.339178	21.397031
73.630741	2466.846068	21.402048
73.415433	2468.030459	21.407066
73.558854	2466.863791	21.412083
73.372491	2473.302653	21.417101
73.299945	2463.553792	21.422119
72.996790	2464.221659	21.427136
73.163411	2496.146283	21.432154
73.898310	2493.321000	21.437171
73.888312	2499.143132	21.442189
73.966900	2500.856264	21.447207
73.905975	2500.924791	21.452224
74.054459	2504.842548	21.457242
73.825573	2505.552012	21.462259
74.009604	2520.667527	21.467277
74.123363	2521.709430	21.472295
74.433723	2525.279013	21.477312
74.350880	2525.391736	21.482330
74.448197	2533.169366	21.487347
74.408281	2531.064615	21.492365
74.614970	2532.897410	21.497383
74.728700	2543.233462	21.502400
74.466706	2559.025143	21.507418
74.523242	2558.752479	21.512435
74.527341	2564.262829	21.517453
74.953135	2567.375025	21.522471
75.019041	2559.921317	21.527488
75.289871	2581.610977	21.532506
75.480013	2576.945022	21.537523
75.435582	2578.811686	21.542541
75.434795	2571.952945	21.547559
76.052514	2569.374301	21.552576
76.055406	2569.697984	21.557594
76.384834	2565.429769	21.562611
76.528971	2549.787466	21.567629
76.522984	2537.095465	21.572647
76.561306	2524.237048	21.577664
76.861104	2529.784857	21.582682
76.697254	2520.604705	21.587699
76.437156	2522.996206	21.592717
76.288312	2501.923258	21.597735
76.425581	2517.096150	21.602752
76.257826	2525.634008	21.607770
76.375201	2519.604902	21.612787
76.536419	2528.469598	21.617805
76.489069	2521.682400	21.622823
76.443351	2517.205276	21.627840
76.369081	2531.434950	21.632858
76.737381	2530.138771	21.637875
76.678188	2534.917075	21.642893
76.777885	2547.063421	21.647911
76.742428	2556.060826	21.652928
76.810587	2554.122763	21.657946
76.840552	2556.160927	21.662963
76.598226	2561.600810	21.667981
76.660878	2579.488660	21.672999
76.875972	2584.217848	21.678016
76.898168	2596.112533	21.683034
77.170991	2603.944891	21.688051
77.511735	2611.556504	21.693069
77.686456	2623.243960	21.698087
78.025118	2619.660059	21.703104
77.876410	2614.642122	21.708122
77.921705	2611.311716	21.713139
78.322044	2601.660560	21.718157
77.933901	2618.826094	21.723175
78.183918	2607.319111	21.728192
78.222584	2615.627817	21.733210
78.319418	2605.325491	21.738227
78.347496	2605.437497	21.743245
78.563946	2622.467508	21.748263
79.040068	2633.851322	21.753280
78.950742	2635.491977	21.758298
78.665717	2613.775334	21.763315
78.715894	2624.416112	21.768333
78.865951	2636.481319	21.773351
79.129488	2635.107657	21.778368
78.955019	2645.839333	21.783386
78.942332	2637.238745	21.788403
79.348724	2636.277977	21.793421
79.132847	2631.935407	21.798439
79.149430	2625.866710	21.803456
79.043141	2635.667314	21.808474
79.222265	2642.280158	21.813491
79.167967	2662.602239	21.818509
79.376287	2664.206814	21.823527
79.857479	2666.955867	21.828544
79.919129	2664.040079	21.833562
80.130663	2658.543333	21.838579
80.064835	2653.280492	21.843597
80.240258	2649.877267	21.848615
80.355685	2642.976343	21.853632
80.502990	2662.084537	21.858650
80.607882	2661.260498	21.863667
80.657706	2649.474534	21.868685
80.560653	2663.776623	21.873703
81.002264	2665.271555	21.878720
80.951740	2651.171036	21.883738
80.906514	2645.310254	21.888755
80.672388	2650.435402	21.893773
80.864400	2663.037387	21.898791
80.947700	2663.356370	21.903808
81.023347	2670.488028	21.908826
80.976915	2661.031569	21.913843
81.129621	2677.059187	21.918861
81.079805	2664.438543	21.923879
81.215869	2670.600658	21.928896
81.004390	2673.624294	21.933914
81.264789	2691.679024	21.938931
81.454290	2691.183854	21.943949
81.478954	2709.227782	21.948967
81.726751	2704.280537	21.953984
81.681383	2690.980353	21.959002
82.082984	2695.694327	21.964019
82.206678	2704.972864	21.969037
82.039392	2716.936537	21.974055
82.285415	2718.506504	21.979072
82.155797	2724.424197	21.984090
82.272985	2728.252718	21.989107
82.126668	2725.029337	21.994125
82.000250	2729.288133	21.999143
82.428452	2723.677396	22.004160
82.261209	2737.171484	22.009178
82.526758	2746.150074	22.014195
82.648634	2749.892383	22.019213
82.640628	2747.911834	22.024231
83.384418	2751.770085	22.029248
83.069544	2750.391753	22.034266
83.177261	2739.231572	22.039283
83.549981	2744.336211	22.044301
83.253327	2745.969602	22.049319
83.811511	2740.833348	22.054336
83.345166	2739.970773	22.059354
83.468101	2734.774176	22.064371
83.981700	2723.202432	22.069389
83.676630	2739.818040	22.074407
83.858972	2749.855012	22.079424
84.257367	2759.753715	22.084442
84.172906	2762.947214	22.089459
84.368278	2753.242625	22.094477
84.130383	2765.348000	22.099495
84.337018	2760.583574	22.104512
84.298597	2763.865097	22.109530
83.949406	2762.176699	22.114547
84.070251	2761.742153	22.119565
84.378268	2764.105414	22.124583
84.519511	2765.932973	22.129600
84.692478	2782.523115	22.134618
84.787550	2798.176160	22.139635
84.811927	2797.520229	22.144653
85.025284	2808.404896	22.149671
84.743246	2793.947425	22.154688
84.829257	2806.426978	22.159706
84.506400	2804.064865	22.164723
85.128180	2809.737226	22.169741
85.127474	2828.269004	22.174759
85.013398	2820.521835	22.179776
85.413893	2831.388014	22.184794
85.001815	2832.173611	22.189811
85.505408	2842.466326	22.194829
85.438292	2857.650684	22.199847
85.571258	2844.593584	22.204864
86.370647	2866.285958	22.209882
86.585443	2862.236336	22.214899
86.558881	2865.089108	22.219917
86.720963	2856.394387	22.224935
86.383309	2837.856078	22.229952
86.551300	2831.370772	22.234970
86.674833	2853.018360	22.239987
87.155682	2853.767763	22.245005
86.953709	2848.754271	22.250023
87.139282	2840.506473	22.255040
87.254438	2827.964978	22.260058
87.118011	2834.307888	22.265075
86.980782	2838.037767	22.270093
86.957889	2850.958319	22.275111
87.184550	2863.057824	22.280128
86.991652	2865.981552	22.285146
87.256560	2865.419903	22.290163
87.322560	2853.685038	22.295181
87.160322	2872.344904	22.300199
87.171228	2886.359156	22.305216
87.611286	2887.681128	22.310234
87.453700	2898.334181	22.315251
87.591532	2890.345096	22.320269
87.839855	2907.578011	22.325287
87.716659	2914.283741	22.330304
88.062859	2921.952873	22.335322
88.140252	2926.761356	22.340339
88.373086	2917.391802	22.345357
88.500298	2925.493817	22.350375
88.686569	2926.398097	22.355392
88.607463	2924.026558	22.360410
88.607095	2918.763772	22.365427
88.507029	2932.522080	22.370445
88.810349	2943.290701	22.375463
89.058276	2948.050374	22.380480
88.921508	2951.080939	22.385498
88.753383	2953.462337	22.390515
88.858820	2948.631596	22.395533
89.042644	2956.430890	22.400551
89.031754	2966.474132	22.405568
89.573292	2972.555983	22.410586
89.285053	2980.877086	22.415603
89.716389	2973.575061	22.420621
89.725519	2979.756032	22.425639
89.663280	2968.411714	22.430656
89.964282	2975.838366	22.435674
89.890669	2991.933845	22.440691
90.081432	3006.924296	22.445709
90.433036	3006.412412	22.450727
90.452272	2998.875693	22.455744
90.619813	2993.876337	22.460762
89.977742	3002.814176	22.465779
90.414718	3005.308415	22.470797
90.750342	2993.768022	22.475815
90.441515	2996.442910	22.480832
90.499219	3000.787330	22.485850
90.467493	3024.219757	22.490867
90.549830	3028.237230	22.495885
90.623198	3037.074687	22.500903
90.785063	3040.674977	22.505920
91.165411	3053.703101	22.510938
90.958406	3060.453533	22.515955
91.119271	3058.392118	22.520973
91.581478	3065.879036	22.525991
91.705378	3075.175871	22.531008
92.280373	3074.430779	22.536026
91.875118	3076.494097	22.541043
92.631937	3057.802366	22.546061
92.800025	3070.156275	22.551079
92.699763	3055.344308	22.556096
92.745997	3037.998358	22.561114
92.791651	3040.827348	22.566131
92.561839	3035.086868	22.571149
92.369837	3029.786204	22.576167
92.594480	3040.330154	22.581184
92.696891	3036.579503	22.586202
92.390276	3052.323582	22.591219
92.786833	3050.845093	22.596237
93.025647	3066.390259	22.601255
92.989685	3068.335107	22.606272
93.248351	3061.456653	22.611290
92.890280	3070.963128	22.616307
92.950705	3066.880050	22.621325
93.171856	3080.005133	22.626343
93.252652	3092.580278	22.631360
93.348291	3097.016459	22.636378
93.182361	3106.112249	22.641395
93.621376	3116.215471	22.646413
93.445890	3128.626528	22.651431
93.197331	3128.006102	22.656448
93.737467	3133.362204	22.661466
94.007236	3153.995269	22.666483
94.391295	3148.655915	22.671501
94.759417	3157.417285	22.676519
94.520409	3155.239230	22.681536
94.963287	3143.547425	22.686554
94.979438	3145.948229	22.691571
95.238130	3143.022834	22.696589
95.462727	3148.857799	22.701607
95.258789	3135.962363	22.706624
95.388970	3129.207998	22.711642
95.127747	3110.136144	22.716659
95.222418	3102.487617	22.721677
95.328842	3118.172957	22.726695
95.329004	3129.809879	22.731712
95.542773	3138.655952	22.736730
95.705301	3133.764087	22.741747
95.589348	3141.925134	22.746765
95.501018	3135.822884	22.751783
95.634029	3148.861878	22.756800
95.775434	3140.890971	22.761818
95.527555	3136.682721	22.766835
95.553985	3163.378414	22.771853
95.879595	3162.082194	22.776871
95.433648	3175.233575	22.781888
95.908690	3187.849189	22.786906
95.938478	3201.801919	22.791923
96.142978	3208.746646	22.796941
96.737668	3215.340673	22.801959
96.444835	3221.354977	22.806976
96.586706	3214.113156	22.811994
96.793085	3208.165065	22.817011
96.796139	3217.652558	22.822029
96.844179	3223.725181	22.827047
97.196903	3240.995056	22.832064
97.707734	3244.842936	22.837082
97.597947	3236.644018	22.842099
97.488808	3246.598641	22.847117
97.349718	3237.348983	22.852135
97.278229	3240.334892	22.857152
97.545962	3259.756513	22.862170
97.623112	3265.418764	22.867187
97.851928	3275.711764	22.872205
98.077889	3274.383274	22.877223
98.408528	3286.685534	22.882240
98.799128	3285.484025	22.887258
98.943051	3288.372326	22.892275
98.702630	3294.865001	22.897293
99.014269	3276.632470	22.902311
98.608860	3292.778285	22.907328
99.035017	3293.199369	22.912346
98.963872	3291.198139	22.917363
98.897316	3293.086677	22.922381
99.263974	3295.788340	22.927399
99.077375	3303.180823	22.932416
99.401159	3291.266159	22.937434
99.702129	3293.665323	22.942451
99.577550	3293.682616	22.947469
99.688975	3285.051200	22.952487
99.513386	3314.035664	22.957504
99.801695	3311.376996	22.962522
99.726280	3321.585142	22.967539
99.869648	3314.631636	22.972557
100.031021	3309.421767	22.977575
99.905719	3325.206464	22.982592
100.370170	3332.997107	22.987610
100.690954	3325.152608	22.992627
100.890493	3338.666579	22.997645
100.875965	3337.315841	23.002663
100.813590	3344.829837	23.007680
100.929161	3342.996014	23.012698
100.935420	3335.666428	23.017715
100.734508	3342.415969	23.022733
101.166384	3332.586273	23.027751
101.011476	3355.589231	23.032768
101.016539	3359.482218	23.037786
101.259301	3364.438960	23.042803
101.036535	3368.578102	23.047821
101.429983	3354.935891	23.052839
101.409429	3373.879924	23.057856
101.556912	3394.023343	23.062874
101.907822	3388.380331	23.067891
101.744821	3394.301856	23.072909
101.886253	3385.500027	23.077927
101.817078	3406.187001	23.082944
102.142399	3415.872261	23.087962
102.388876	3419.351086	23.092979
102.515498	3425.172907	23.097997
102.678156	3415.787945	23.103015
102.788883	3426.716483	23.108032
102.888614	3424.643919	23.113050
103.195980	3420.390954	23.118067
102.699859	3431.390033	23.123085
102.928767	3434.378028	23.128103
102.935023	3446.828825	23.133120
102.958610	3456.942645	23.138138
103.019360	3451.575024	23.143155
103.030626	3472.860200	23.148173
103.204676	3477.633496	23.153191
103.201019	3487.240784	23.158208
103.174243	3495.198984	23.163226
103.929169	3505.606295	23.168243
104.154588	3506.228090	23.173261
104.201744	3509.336473	23.178279
104.303624	3511.184838	23.183296
104.257387	3506.207461	23.188314
104.649068	3516.783429	23.193331
104.940238	3515.546849	23.198349
105.671572	3520.086973	23.203367
105.332433	3517.931413	23.208384
105.400040	3508.395638	23.213402
105.610653	3497.803313	23.218419
105.285599	3480.847749	23.223437
105.814406	3487.958017	23.228455
105.595279	3476.046819	23.233472
105.467302	3474.987001	23.238490
105.573520	3492.111490	23.243507
105.631593	3509.780278	23.248525
106.050699	3506.719089	23.253543
106.175228	3514.282033	23.258560
105.900287	3507.196761	23.263578
105.917427	3511.927240	23.268595
105.854787	3519.202361	23.273613
106.157869	3506.936211	23.278631
106.323825	3528.602886	23.283648
106.151392	3540.514888	23.288666
106.190069	3538.609954	23.293683
106.466657	3552.134929	23.298701
106.570025	3543.916173	23.303719
106.757262	3569.381762	23.308736
106.302459	3577.886785	23.313754
106.384243	3581.956468	23.318771
106.986126	3604.660767	23.323789
107.193492	3603.456221	23.328807
107.753454	3608.665085	23.333824
107.648154	3603.862866	23.338842
107.873118	3595.294703	23.343859
107.510345	3600.872692	23.348877
108.040218	3608.771118	23.353895
108.309284	3616.313241	23.358912
107.989071	3621.358905	23.363930
108.816092	3611.876012	23.368947
108.536403	3618.196979	23.373965
108.860032	3613.560901	23.378983
108.980098	3611.144342	23.384000
108.460446	3616.783452	23.389018
108.837961	3611.839172	23.394035
108.701320	3618.000129	23.399053
109.063643	3610.079680	23.404071
109.063467	3616.008876	23.409088
108.971993	3614.180689	23.414106
109.117537	3607.927954	23.419123
108.686164	3629.407395	23.424141
108.854959	3637.365845	23.429159
109.225519	3642.002584	23.434176
109.107679	3651.096997	23.439194
109.776989	3664.953305	23.444211
109.702695	3680.473946	23.449229
110.110032	3672.771996	23.454247
110.295332	3675.820836	23.459264
110.276817	3675.407065	23.464282
110.552582	3671.368366	23.469299
110.607761	3691.510184	23.474317
110.538980	3695.807307	23.479335
110.861421	3697.921043	23.484352
110.915761	3704.503104	23.489370
111.057275	3697.181583	23.494387
110.798001	3698.722231	23.499405
111.219007	3699.818677	23.504423
111.160677	3693.541910	23.509440
110.943097	3720.744125	23.514458
111.383666	3714.846303	23.519475
111.517653	3717.335499	23.524493
111.455330	3719.822277	23.529511
111.332403	3728.645893	23.534528
111.641095	3745.054641	23.539546
112.105060	3748.369819	23.544563
111.816614	3747.537070	23.549581
112.039785	3744.882462	23.554599
112.768627	3743.834576	23.559616
112.623516	3761.868955	23.564634
113.066917	3749.932489	23.569651
112.955291	3773.850637	23.574669
113.410655	3758.942116	23.579687
113.587326	3763.267764	23.584704
113.423788	3760.895560	23.589722
113.834826	3756.689457	23.594739
113.762683	3735.774950	23.599757
113.605301	3717.854530	23.604775
113.659576	3722.463533	23.609792
113.723666	3747.606136	23.614810
114.133380	3747.800806	23.619827
114.072705	3759.271119	23.624845
113.980749	3745.568673	23.629863
114.140272	3750.678367	23.634880
113.875067	3752.904344	23.639898
113.924871	3745.785072	23.644915
113.959726	3767.537260	23.649933
114.038407	3768.340954	23.654951
114.386906	3779.627516	23.659968
114.303756	3788.786725	23.664986
114.892873	3795.948932	23.670003
114.555837	3806.369005	23.675021
114.729954	3813.450565	23.680039
115.131544	3813.836769	23.685056
115.034101	3836.677319	23.690074
115.622600	3838.082204	23.695091
115.452098	3833.816410	23.700109
115.380323	3848.070098	23.705127
115.720289	3843.261925	23.710144
115.781978	3854.978542	23.715162
115.916351	3870.126458	23.720179
116.120646	3863.383874	23.725197
115.781753	3874.222072	23.730215
116.066185	3870.304340	23.735232
116.294583	3882.863860	23.740250
116.522667	3894.624516	23.745267
116.642600	3893.374235	23.750285
116.639586	3904.242078	23.755303
116.898332	3904.953246	23.760320
116.766687	3904.811454	23.765338
116.952661	3918.492377	23.770355
117.204106	3922.930069	23.775373
116.819142	3928.448465	23.780391
117.103258	3937.770770	23.785408
117.421265	3943.113673	23.790426
117.565283	3947.476694	23.795443
118.050890	3946.893295	23.800461
117.744074	3951.549383	23.805479
117.975326	3950.538113	23.810496
117.804140	3959.109213	23.815514
118.338615	3974.916427	23.820531
118.769992	3972.609910	23.825549
118.822693	3976.734536	23.830567
118.836794	3979.213772	23.835584
118.602392	3981.489787	23.840602
119.137204	3967.603443	23.845619
119.542242	3976.496169	23.850637
119.124240	3973.052287	23.855655
119.177735	3972.624966	23.860672
119.319819	3999.379646	23.865690
119.304983	4012.688850	23.870707
119.677980	4005.535042	23.875725
119.655393	4006.981257	23.880743
119.758909	4010.352460	23.885760
119.866713	4023.655072	23.890778
119.972274	4022.493009	23.895795
120.184443	4025.997754	23.900813
119.645959	4031.887419	23.905831
120.337022	4037.411697	23.910848
120.251137	4060.599915	23.915866
120.539486	4055.860895	23.920883
120.506294	4064.125613	23.925901
120.562797	4076.048011	23.930919
120.909679	4081.192828	23.935936
120.721400	4078.973527	23.940954
121.184643	4092.351398	23.945971
121.061642	4104.148509	23.950989
121.627097	4120.882357	23.956007
121.502774	4110.758337	23.961024
121.957499	4122.212167	23.966042
122.085700	4129.173923	23.971059
122.517034	4128.541657	23.976077
122.140924	4129.399689	23.981095
122.668848	4132.026662	23.986112
122.467274	4131.286950	23.991130
122.859925	4129.136475	23.996147
122.982101	4131.671014	24.001165
123.061232	4131.639094	24.006183
123.256320	4126.418627	24.011200
122.697453	4132.553484	24.016218
122.866966	4143.434165	24.021235
123.318337	4152.798498	24.026253
123.570349	4154.635770	24.031271
123.795580	4155.423004	24.036288
123.623243	4159.349216	24.041306
123.575852	4177.003995	24.046323
123.926641	4165.871705	24.051341
123.952417	4180.649328	24.056359
123.888563	4187.998988	24.061376
124.184566	4194.003609	24.066394
123.953590	4183.260949	24.071411
124.513215	4190.977932	24.076429
124.512589	4212.582279	24.081447
125.063014	4213.189468	24.086464
124.870791	4224.753254	24.091482
124.796267	4229.768123	24.096499
124.929283	4216.837845	24.101517
124.807407	4226.768430	24.106535
125.113199	4229.904851	24.111552
125.074129	4257.123610	24.116570
124.919541	4255.208970	24.121587
125.127598	4264.793362	24.126605
125.380965	4284.041846	24.131623
125.573527	4281.854514	24.136640
125.896937	4291.796191	24.141658
126.266761	4304.305376	24.146675
126.572275	4304.836717	24.151693
126.301629	4311.130075	24.156711
127.104988	4307.010228	24.161728
127.053854	4306.410886	24.166746
127.103784	4306.922488	24.171763
127.401463	4300.665853	24.176781
127.286188	4308.247772	24.181799
127.476552	4308.437562	24.186816
127.561619	4318.396028	24.191834
127.601054	4323.164392	24.196851
127.781126	4329.857733	24.201869
127.850069	4335.695387	24.206887
127.691027	4317.556805	24.211904
127.815082	4333.998038	24.216922
127.772008	4334.584949	24.221939
128.297420	4342.481738	24.226957
129.020033	4350.819063	24.231975
129.372731	4335.215527	24.236992
129.178021	4330.444876	24.242010
129.074182	4337.763450	24.247027
129.558379	4335.858406	24.252045
129.298415	4338.558866	24.257063
129.618511	4324.820904	24.262080
129.677971	4326.367311	24.267098
129.461039	4342.025715	24.272115
129.533386	4327.713076	24.277133
129.404093	4332.128320	24.282151
129.643270	4334.605646	24.287168
129.820780	4359.379537	24.292186
129.501772	4375.776317	24.297203
129.858139	4372.160731	24.302221
129.926248	4385.484817	24.307239
130.146031	4399.801988	24.312256
130.425983	4392.500057	24.317274
130.451431	4423.247552	24.322291
130.711245	4420.618244	24.327309
130.676889	4428.571090	24.332327
131.555974	4418.688845	24.337344
131.657144	4410.791315	24.342362
131.808163	4409.511021	24.347379
132.164326	4397.917755	24.352397
132.222146	4402.587009	24.357415
132.366362	4403.639730	24.362432
132.575280	4399.334352	24.367450
132.449332	4405.376103	24.372467
132.657632	4398.497169	24.377485
132.575031	4400.431820	24.382503
132.732574	4399.315824	24.387520
132.764825	4392.642558	24.392538
132.621416	4406.477483	24.397555
133.156069	4417.781218	24.402573
132.632390	4434.195535	24.407591
132.910766	4420.354168	24.412608
132.911403	4423.776816	24.417626
132.928584	4431.640770	24.422643
133.243229	4441.324901	24.427661
133.323854	4461.687535	24.432679
133.336726	4458.693678	24.437696
133.606966	4465.157095	24.442714
133.426174	4479.485782	24.447731
133.757068	4478.748128	24.452749
133.489772	4488.721159	24.457767
133.973504	4509.710683	24.462784
134.221929	4515.253176	24.467802
134.280440	4523.503289	24.472819
134.689174	4535.467518	24.477837
134.255501	4545.498949	24.482855
134.595450	4559.118222	24.487872
135.058525	4568.821867	24.492890
135.389121	4570.295675	24.497907
135.761906	4569.738490	24.502925
135.876650	4555.953338	24.507943
136.016349	4555.879062	24.512960
136.186979	4566.682673	24.517978
136.054498	4582.300505	24.522995
136.608345	4575.864946	24.528013
136.363601	4583.244064	24.533031
136.450657	4592.269924	24.538048
136.663135	4578.749662	24.543066
136.455066	4593.567324	24.548083
136.503776	4596.729219	24.553101
136.897470	4611.072021	24.558119
136.716352	4620.147189	24.563136
137.145640	4616.449340	24.568154
136.909484	4645.110439	24.573171
137.110697	4650.412750	24.578189
137.332433	4657.640351	24.583207
137.294597	4669.426882	24.588224
137.740821	4669.422948	24.593242
137.838642	4673.782430	24.598259
138.224006	4687.990441	24.603277
138.546401	4695.359628	24.608295
138.452463	4699.472194	24.613312
138.796844	4692.672111	24.618330
138.514207	4698.280874	24.623347
138.960325	4713.753852	24.628365
139.055200	4727.205300	24.633383
138.991319	4728.686402	24.638400
139.444336	4727.967033	24.643418
139.466922	4734.342560	24.648435
139.540893	4752.190455	24.653453
139.534793	4763.268500	24.658471
139.651229	4759.684039	24.663488
139.797058	4761.014522	24.668506
139.906234	4790.922681	24.673523
140.058639	4791.540915	24.678541
140.211135	4800.477264	24.683559
140.288165	4818.475149	24.688576
140.643235	4813.828773	24.693594
140.606111	4817.039629	24.698611
140.635184	4824.433996	24.703629
141.257402	4840.445661	24.708647
141.293110	4847.199442	24.713664
141.549746	4853.717259	24.718682
141.589166	4861.225695	24.723699
141.660701	4868.091665	24.728717
141.614898	4873.126380	24.733735
141.801567	4874.791886	24.738752
142.213357	4877.687159	24.743770
142.092312	4880.915124	24.748787
141.798982	4888.679699	24.753805
142.573779	4893.970252	24.758823
142.238859	4905.887449	24.763840
142.310292	4908.121825	24.768858
142.598242	4928.451396	24.773875
142.618711	4926.709195	24.778893
142.963392	4948.498949	24.783911
143.731943	4945.395956	24.788928
143.851577	4944.946198	24.793946
143.951243	4947.155411	24.798963
144.124553	4936.044986	24.803981
144.153989	4942.093410	24.808999
144.253826	4946.277007	24.814016
144.465888	4945.204680	24.819034
144.557165	4954.381258	24.824051
144.497893	4970.251928	24.829069
144.654956	4969.402956	24.834087
144.927321	4972.834120	24.839104
145.069060	4977.656562	24.844122
144.893999	4971.638889	24.849139
144.867957	4992.354650	24.854157
145.450060	4997.546526	24.859175
145.479921	5008.215535	24.864192
145.369251	5006.568362	24.869210
145.412611	5029.165939	24.874227
145.650972	5039.454579	24.879245
145.891663	5037.760037	24.884263
145.631984	5063.600024	24.889280
146.459782	5067.097205	24.894298
146.630909	5065.998595	24.899315
146.586791	5076.294825	24.904333
146.955932	5074.277295	24.909351
147.176047	5091.157783	24.914368
147.216035	5087.281164	24.919386
147.325762	5091.635633	24.924403
147.486225	5107.494339	24.929421
147.850268	5106.025013	24.934439
147.793161	5123.079979	24.939456
148.404285	5119.410864	24.944474
148.418866	5118.935244	24.949491
148.269550	5120.803887	24.954509
148.403640	5117.121116	24.959527
148.671720	5132.318519	24.964544
148.811389	5134.061170	24.969562
148.365391	5141.017990	24.974579
148.699939	5134.310712	24.979597
149.174129	5151.002553	24.984615
149.032337	5170.184695	24.989632
149.859704	5156.015968	24.994650
149.954729	5166.697094	24.999667
149.957125	5163.625300	25.004685
150.178532	5149.681716	25.009703
150.064708	5164.453536	25.014720
150.392839	5171.461287	25.019738
150.621829	5184.155247	25.024755
150.801399	5170.110700	25.029773
150.860519	5179.680239	25.034791
150.777842	5178.207174	25.039808
151.215525	5170.139932	25.044826
151.353731	5173.305972	25.049843
151.362112	5180.149495	25.054861
151.044975	5195.406410	25.059879
151.087186	5211.931470	25.064896
151.165708	5210.130761	25.069914
151.497661	5224.591496	25.074931
151.340995	5242.697222	25.079949
152.000160	5246.980116	25.084967
151.812261	5273.961529	25.089984
152.246370	5273.388620	25.095002
152.173008	5273.274143	25.100019
152.380411	5287.093282	25.105037
152.595430	5290.330852	25.110055
152.708281	5296.178893	25.115072
152.736093	5305.329207	25.120090
153.235940	5314.590100	25.125107
153.165137	5333.730715	25.130125
153.264601	5324.607539	25.135143
153.448785	5341.543885	25.140160
153.946299	5352.749723	25.145178
154.205028	5348.309010	25.150195
154.148262	5357.347397	25.155213
154.268699	5353.937767	25.160231
154.611652	5368.333013	25.165248
154.686875	5381.103878	25.170266
154.879314	5386.492956	25.175283
154.970490	5388.015296	25.180301
154.863190	5392.260212	25.185319
155.153364	5410.051660	25.190336
155.148066	5416.723503	25.195354
155.531545	5413.588331	25.200371
155.644666	5436.420625	25.205389
156.093870	5444.417275	25.210407
155.912144	5437.952394	25.215424
156.290386	5435.415865	25.220442
157.037866	5436.733058	25.225459
157.257236	5447.105455	25.230477
157.655606	5441.357747	25.235495
157.351253	5430.527976	25.240512
157.240947	5431.506503	25.245530
157.467178	5440.897214	25.250547
157.504582	5446.842121	25.255565
157.713659	5439.788551	25.260583
157.974315	5441.530820	25.265600
157.936199	5440.814283	25.270618
158.292791	5436.151723	25.275635
157.935469	5451.174561	25.280653
158.227559	5459.210717	25.285671
158.440093	5477.232517	25.290688
158.275693	5471.950848	25.295706
158.698585	5481.857062	25.300723
158.613077	5503.331583	25.305741
159.040717	5500.461562	25.310759
159.473216	5514.320678	25.315776
159.380982	5526.204312	25.320794
159.385457	5533.863005	25.325811
159.155043	5544.846561	25.330829
159.722832	5551.541363	25.335847
159.744262	5561.588376	25.340864
160.196703	5563.421653	25.345882
160.502202	5578.428186	25.350899
160.392931	5597.458950	25.355917
160.634133	5582.577610	25.360935
160.892088	5587.462050	25.365952
160.942498	5590.133192	25.370970
161.572614	5604.186375	25.375987
161.720215	5605.892319	25.381005
161.670995	5604.130908	25.386023
161.785049	5604.497219	25.391040
161.690564	5607.824881	25.396058
162.004533	5618.776304	25.401075
162.166293	5627.107500	25.406093
162.486223	5633.017341	25.411111
162.518499	5643.383942	25.416128
162.341625	5650.135590	25.421146
162.722140	5655.824296	25.426163
162.573859	5663.762831	25.431181
162.562919	5671.804561	25.436199
162.626168	5691.875537	25.441216
162.940643	5698.075358	25.446234
163.446790	5699.434256	25.451251
163.292050	5728.485466	25.456269
163.286577	5737.018571	25.461287
163.679897	5735.114295	25.466304
163.861246	5750.940250	25.471322
164.288815	5747.560619	25.476339
164.331328	5764.112986	25.481357
164.678131	5767.442170	25.486375
165.278520	5768.485338	25.491392
165.727679	5773.560165	25.496410
165.868703	5766.729624	25.501427
165.761353	5768.486617	25.506445
166.084595	5766.676682	25.511463
166.093436	5766.284694	25.516480
165.933794	5776.276086	25.521498
166.007716	5757.683636	25.526515
166.268530	5785.371079	25.531533
166.418756	5790.763373	25.536551
166.404532	5799.472814	25.541568
166.420924	5808.699352	25.546586
166.692761	5815.536387	25.551603
166.651004	5830.225968	25.556621
166.707473	5829.622074	25.561639
167.258609	5840.050650	25.566656
166.795278	5858.358474	25.571674
167.639348	5864.801935	25.576691
168.631829	5863.841655	25.581709
168.791854	5857.741178	25.586727
169.183816	5852.967868	25.591744
168.845936	5861.632676	25.596762
169.359388	5858.491573	25.601779
169.457032	5862.990034	25.606797
169.189171	5857.778985	25.611815
169.141640	5861.911706	25.616832
169.180135	5857.909916	25.621850
169.580129	5857.562402	25.626867
169.593225	5867.154971	25.631885
169.596285	5885.733444	25.636903
170.009707	5887.217247	25.641920
169.587669	5901.819657	25.646938
169.920996	5901.014593	25.651955
170.122357	5914.768342	25.656973
170.351877	5925.745040	25.661991
170.632695	5942.118586	25.667008
170.491872	5952.309377	25.672026
170.857802	5957.468980	25.677044
171.590286	5979.211473	25.682061
171.138119	5979.949126	25.687079
171.730101	5987.862470	25.692096
171.775239	6010.492663	25.697114
171.941698	6014.271667	25.702132
171.894565	6013.013149	25.707149
172.156143	6024.560333	25.712167
172.564588	6033.434373	25.717184
171.914028	6048.060715	25.722202
172.431153	6052.133519	25.727220
172.554645	6068.683775	25.732237
172.614988	6084.390765	25.737255
173.032696	6092.315008	25.742272
172.972712	6111.484696	25.747290
172.987333	6127.863290	25.752308
173.325962	6143.604431	25.757325
173.934140	6161.133588	25.762343
174.132219	6155.457502	25.767360
173.767238	6175.653813	25.772378
174.521606	6177.181803	25.777396
174.806729	6193.425724	25.782413
175.120632	6191.273891	25.787431
175.614892	6177.353372	25.792448
175.223338	6191.219280	25.797466
175.849098	6174.461950	25.802484
175.764869	6184.892374	25.807501
176.008916	6194.771263	25.812519
176.441242	6208.800361	25.817536
176.004616	6216.445260	25.822554
176.088103	6216.233036	25.827572
176.337464	6209.922248	25.832589
176.067297	6220.794734	25.837607
177.562782	6211.016895	25.842624
177.707597	6210.742497	25.847642
177.854528	6212.847945	25.852660
177.888691	6220.996665	25.857677
177.951354	6213.885957	25.862695
178.463731	6214.649214	25.867712
178.166965	6214.441108	25.872730
178.255721	6206.726686	25.877748
178.330437	6211.030576	25.882765
178.518815	6235.856810	25.887783
178.659741	6234.774168	25.892800
178.815764	6240.016792	25.897818
178.683068	6246.499861	25.902836
178.552400	6260.280732	25.907853
178.564686	6270.942488	25.912871
178.940816	6283.650692	25.917888
178.891459	6314.797880	25.922906
179.377321	6327.658012	25.927924
179.703265	6333.600987	25.932941
179.859477	6354.674186	25.937959
180.480404	6364.411003	25.942976
180.452481	6368.186951	25.947994
180.860906	6388.132141	25.953012
180.806698	6397.270725	25.958029
180.934114	6397.675004	25.963047
181.211123	6400.062888	25.968064
181.254909	6421.235984	25.973082
181.500469	6429.153562	25.978100
181.928931	6438.049709	25.983117
181.780370	6453.727982	25.988135
182.181263	6459.722349	25.993152
182.364031	6469.760457	25.998170
182.405494	6474.668548	26.003188
182.947427	6483.804210	26.008205
182.777421	6492.083877	26.013223
183.303047	6506.940508	26.018240
183.437385	6516.166763	26.023258
183.245399	6520.732444	26.028276
183.367265	6525.400350	26.033293
183.574277	6547.371149	26.038311
184.149892	6554.940153	26.043328
184.163546	6556.989818	26.048346
183.846551	6586.140450	26.053364
184.295637	6585.817060	26.058381
184.278871	6601.089209	26.063399
184.537903	6610.140419	26.068416
184.820570	6631.410362	26.073434
185.048042	6646.478138	26.078452
185.116123	6650.946293	26.083469
185.499875	6663.776409	26.088487
185.630630	6675.083523	26.093504
186.029143	6691.717116	26.098522
185.821043	6701.866007	26.103540
186.258795	6696.863510	26.108557
186.721605	6725.219252	26.113575
186.700368	6721.575311	26.118592
186.799914	6732.303218	26.123610
186.996241	6725.155892	26.128628
187.374650	6737.630939	26.133645
186.990070	6759.716880	26.138663
187.444918	6753.069274	26.143680
187.768352	6774.487015	26.148698
187.825830	6786.246682	26.153716
187.870465	6792.894267	26.158733
188.213218	6810.093333	26.163751
188.601069	6825.499312	26.168768
188.124649	6833.553607	26.173786
188.056451	6854.951469	26.178804
189.202472	6854.976979	26.183821
188.936964	6880.137998	26.188839
189.823801	6893.117847	26.193856
189.791337	6886.540137	26.198874
189.705287	6895.412557	26.203892
190.122421	6911.612439	26.208909
190.278479	6916.659155	26.213927
190.392775	6928.177915	26.218944
190.443690	6950.361099	26.223962
190.718035	6944.205765	26.228980
191.196965	6952.144688	26.233997
191.157767	6967.576873	26.239015
191.351328	6982.180370	26.244032
191.645586	6991.969498	26.249050
191.564999	7010.115796	26.254068
192.264503	7003.144661	26.259085
191.940965	7021.123401	26.264103
192.535288	7027.997170	26.269120
192.504157	7039.981268	26.274138
192.474226	7056.371375	26.279156
193.082574	7062.899406	26.284173
193.298702	7064.376729	26.289191
194.058985	7067.609128	26.294208
194.563220	7060.519973	26.299226
194.746015	7070.857771	26.304244
194.931751	7064.293351	26.309261
194.890625	7056.157432	26.314279
195.258847	7050.426763	26.319296
195.289462	7055.341562	26.324314
195.278033	7053.910043	26.329332
195.519031	7051.377955	26.334349
195.604728	7057.087020	26.339367
195.561139	7058.427124	26.344384
195.382351	7054.144498	26.349402
195.372293	7084.142976	26.354420
195.888044	7081.313175	26.359437
195.822593	7101.415988	26.364455
196.234618	7112.454554	26.369472
196.217872	7124.025951	26.374490
196.344018	7153.977510	26.379508
196.404553	7157.919323	26.384525
197.017636	7178.198556	26.389543
196.948844	7176.237002	26.394560
197.436415	7194.248140	26.399578
197.600994	7211.607216	26.404596
197.723489	7215.497788	26.409613
197.858112	7235.161085	26.414631
198.013959	7233.517437	26.419648
198.380571	7254.170910	26.424666
198.539547	7268.213292	26.429684
198.710049	7281.066743	26.434701
198.768228	7302.461536	26.439719
199.284865	7297.027489	26.444736
199.405378	7307.593190	26.449754
199.532626	7329.656308	26.454772
199.961809	7336.095287	26.459789
200.138160	7336.260671	26.464807
200.066397	7342.627722	26.469824
200.506115	7358.478518	26.474842
200.504788	7370.303528	26.479860
200.727390	7376.188454	26.484877
200.834807	7402.129571	26.489895
201.109735	7402.774815	26.494912
201.118426	7409.793328	26.499930
201.300453	7433.592204	26.504948
201.347208	7437.033046	26.509965
201.889805	7461.852752	26.514983
201.567563	7469.862052	26.520000
202.337885	7478.685441	26.525018
202.597795	7494.429982	26.530036
202.794912	7494.730550	26.535053
203.116220	7518.778162	26.540071
203.160652	7521.111919	26.545088
203.751006	7525.441547	26.550106
203.712994	7542.264362	26.555124
203.581313	7553.722838	26.560141
203.759733	7566.556300	26.565159
204.391470	7577.604368	26.570176
204.382429	7589.307942	26.575194
204.332408	7607.092229	26.580212
204.925427	7604.678791	26.585229
205.051546	7604.842286	26.590247
205.258302	7629.798405	26.595264
205.646277	7624.492755	26.600282
205.531845	7640.292556	26.605300
205.738959	7659.600897	26.610317
205.810327	7670.593272	26.615335
206.096123	7688.773198	26.620352
206.581685	7700.296992	26.625370
206.557930	7705.890569	26.630388
207.294306	7720.063474	26.635405
208.033376	7711.648701	26.640423
208.252887	7716.329091	26.645440
208.223974	7717.130389	26.650458
208.151871	7713.474193	26.655476
208.652693	7739.226820	26.660493
208.724691	7751.180926	26.665511
209.046709	7754.702129	26.670528
208.929241	7746.693546	26.675546
208.930189	7744.220932	26.680564
209.267511	7753.439384	26.685581
209.397293	7775.345159	26.690599
209.442655	7778.985595	26.695616
209.592143	7789.066304	26.700634
209.475600	7816.200081	26.705652
209.675519	7810.990211	26.710669
210.120880	7831.736115	26.715687
210.073722	7855.234206	26.720704
210.664076	7863.750580	26.725722
210.585851	7874.476502	26.730740
211.380874	7876.737576	26.735757
211.987122	7890.063418	26.740775
211.969094	7899.426075	26.745792
211.916221	7891.048280	26.750810
212.330792	7915.366932	26.755828
212.349513	7912.135927	26.760845
212.379050	7926.031043	26.765863
212.347473	7935.814245	26.770880
212.883587	7947.691378	26.775898
213.164097	7954.271109	26.780916
213.688533	7965.174224	26.785933
213.943478	7967.723559	26.790951
214.001582	7982.540324	26.795968
214.294497	7970.487072	26.800986
214.348056	7978.465688	26.806004
214.927943	7972.224532	26.811021
214.734523	7979.228042	26.816039
215.034922	7994.776513	26.821056
215.321460	7987.760937	26.826074
215.113542	7993.430116	26.831092
215.082913	8007.043059	26.836109
215.603184	8017.084357	26.841127
215.590034	8032.939398	26.846144
215.603861	8045.264165	26.851162
215.583047	8059.166187	26.856180
216.128102	8085.598913	26.861197
216.323552	8086.056527	26.866215
216.357243	8112.330076	26.871232
217.016295	8116.854838	26.876250
217.545879	8138.807323	26.881268
217.605748	8145.366293	26.886285
217.701237	8138.331983	26.891303
218.013204	8164.928032	26.896320
218.407247	8174.092404	26.901338
218.625719	8179.409582	26.906356
218.406768	8199.874068	26.911373
219.042672	8204.693371	26.916391
219.000619	8210.878594	26.921408
219.331001	8225.696030	26.926426
219.410183	8240.816744	26.931444
219.587950	8245.249792	26.936461
219.881241	8259.134455	26.941479
219.934082	8268.523363	26.946496
220.586476	8281.721346	26.951514
220.584628	8303.432307	26.956532
221.163459	8306.164985	26.961549
221.181802	8332.235850	26.966567
221.109445	8346.671314	26.971584
221.627340	8354.596595	26.976602
221.864268	8362.916742	26.981620
221.588245	8367.229871	26.986637
222.235052	8384.913416	26.991655
222.112033	8389.290928	26.996672
222.569020	8401.888934	27.001690
222.890623	8423.954358	27.006708
222.959667	8430.021163	27.011725
223.290301	8447.182269	27.016743
223.616043	8455.316769	27.021760
224.201476	8463.544401	27.026778
224.136745	8467.221405	27.031796
224.137918	8481.004344	27.036813
224.389987	8479.157101	27.041831
224.184945	8503.753700	27.046848
224.452604	8515.790090	27.051866
224.815730	8538.625482	27.056884
224.942970	8537.591439	27.061901
225.805108	8547.909483	27.066919
225.537167	8568.855224	27.071936
226.270845	8583.096312	27.076954
226.364335	8581.810283	27.081972
226.247096	8601.523419	27.086989
226.621635	8610.425816	27.092007
226.829661	8630.149536	27.097024
226.877828	8640.559566	27.102042
226.993356	8659.028061	27.107060
227.343755	8675.301491	27.112077
227.624077	8673.426687	27.117095
228.275353	8685.812241	27.122112
228.594675	8687.730253	27.127130
228.901840	8699.450633	27.132148
229.361692	8706.299434	27.137165
229.645865	8692.210769	27.142183
229.564233	8702.181576	27.147200
229.929364	8724.072393	27.152218
230.010513	8718.664546	27.157236
230.170118	8725.575849	27.162253
230.050603	8724.953824	27.167271
229.932982	8734.231900	27.172288
230.062598	8757.214327	27.177306
230.537943	8775.546757	27.182324
230.490783	8793.295652	27.187341
230.586256	8811.033471	27.192359
231.278411	8814.964487	27.197376
232.448655	8810.660467	27.202394
232.770216	8816.698853	27.207412
232.558139	8824.647194	27.212429
233.465118	8827.095417	27.217447
233.442345	8830.715904	27.222464
233.365160	8824.369334	27.227482
233.555510	8834.180806	27.232500
233.563170	8823.930215	27.237517
233.774233	8833.640564	27.242535
233.723075	8858.723390	27.247552
233.993026	8870.023905	27.252570
234.459955	8877.663297	27.257588
234.360577	8896.322964	27.262605
234.187751	8903.532209	27.267623
234.368368	8928.889372	27.272640
234.747942	8945.671850	27.277658
235.297704	8957.409617	27.282676
235.355263	8982.320959	27.287693
235.809713	8998.341103	27.292711
235.496104	9019.666843	27.297728
236.028570	9027.608948	27.302746
236.148841	9045.446891	27.307764
236.174918	9074.168504	27.312781
236.672096	9069.980982	27.317799
237.262945	9098.003792	27.322816
237.446060	9106.813020	27.327834
238.258027	9108.173416	27.332852
238.261386	9140.991370	27.337869
239.141734	9123.185050	27.342887
239.084535	9133.796459	27.347904
239.126236	9140.443148	27.352922
239.179129	9153.752501	27.357940
239.181389	9159.825955	27.362957
239.621129	9180.112920	27.367975
239.613402	9192.219212	27.372992
239.892969	9204.607065	27.378010
240.525426	9211.421891	27.383028
240.279399	9235.680590	27.388045
240.520117	9242.449444	27.393063
240.895359	9261.029096	27.398080
241.116542	9280.638781	27.403098
241.618809	9292.068002	27.408116
241.432423	9298.902333	27.413133
241.711334	9317.555565	27.418151
241.856229	9333.365151	27.423168
241.993125	9355.229371	27.428186
242.399987	9376.342914	27.433204
242.342474	9396.047102	27.438221
242.813484	9403.923980	27.443239
242.872083	9425.510615	27.448256
242.904139	9449.963705	27.453274
243.671935	9468.810816	27.458292
243.297108	9495.562587	27.463309
243.769746	9513.266875	27.468327
244.112280	9526.188875	27.473344
244.184134	9546.047428	27.478362
244.681710	9556.618142	27.483380
244.530586	9578.813340	27.488397
244.887522	9586.995231	27.493415
245.638643	9607.339714	27.498432
245.527138	9631.276509	27.503450
245.822080	9650.072418	27.508468
245.841576	9669.296196	27.513485
246.091640	9676.601745	27.518503
246.990198	9710.756324	27.523520
246.796332	9732.426285	27.528538
247.316117	9737.770335	27.533556
247.449914	9751.247935	27.538573
247.940616	9756.447143	27.543591
248.095650	9781.802815	27.548608
248.333248	9791.881179	27.553626
248.764604	9807.191438	27.558644
249.156488	9817.664868	27.563661
249.419187	9823.711842	27.568679
249.643562	9846.962120	27.573696
249.836327	9852.664638	27.578714
250.325502	9861.145334	27.583732
250.123591	9878.877025	27.588749
250.778320	9866.850472	27.593767
250.912510	9880.696019	27.598784
251.146605	9900.716338	27.603802
251.375861	9901.572536	27.608820
251.526946	9921.423903	27.613837
251.955198	9926.925820	27.618855
252.043038	9935.339313	27.623872
252.006212	9956.417837	27.628890
252.387240	9972.018651	27.633908
252.661119	9985.874955	27.638925
252.855421	10004.576920	27.643943
252.998309	10021.528268	27.648960
253.581608	10036.818228	27.653978
253.513858	10048.723216	27.658996
253.727256	10074.887403	27.664013
254.297041	10075.540497	27.669031
254.643687	10082.265322	27.674048
254.851946	10111.590345	27.679066
254.868658	10112.845841	27.684084
254.956272	10139.802305	27.689101
255.479113	10143.746824	27.694119
255.996360	10172.770881	27.699136
256.103235	10180.121723	27.704154
256.224883	10204.516956	27.709172
256.285761	10222.977425	27.714189
256.500904	10241.236599	27.719207
256.713931	10252.805167	27.724224
256.982923	10286.528286	27.729242
257.707414	10293.991636	27.734260
257.482123	10309.301973	27.739277
257.745810	10324.088320	27.744295
258.514830	10325.704923	27.749312
258.856567	10341.158211	27.754330
259.872711	10340.925692	27.759348
260.797274	10330.844802	27.764365
260.928289	10328.602282	27.769383
261.168075	10324.379216	27.774400
261.311757	10325.132270	27.779418
261.223912	10334.916831	27.784436
261.223499	10334.824855	27.789453
261.062048	10334.493351	27.794471
261.426989	10329.324580	27.799488
261.662612	10341.945146	27.804506
261.601664	10362.855676	27.809524
261.340131	10374.009214	27.814541
261.651935	10387.414441	27.819559
262.006626	10403.045262	27.824576
261.799974	10417.404845	27.829594
262.117466	10435.442398	27.834612
262.766157	10455.303923	27.839629
262.833285	10464.299403	27.844647
263.202027	10492.646755	27.849664
263.031299	10517.703977	27.854682
263.537716	10540.505024	27.859700
263.545751	10564.168871	27.864717
263.880590	10585.461420	27.869735
264.095160	10601.890162	27.874752
264.367905	10634.416658	27.879770
265.252006	10644.175423	27.884788
265.375634	10664.942226	27.889805
265.514048	10684.698948	27.894823
265.875874	10700.228817	27.899840
266.119368	10716.736382	27.904858
266.437659	10730.384261	27.909876
267.238302	10757.898472	27.914893
267.569353	10763.391619	27.919911
267.715697	10770.656601	27.924928
267.805053	10786.844771	27.929946
268.127586	10806.361482	27.934964
268.727776	10806.835446	27.939981
268.418412	10817.329139	27.944999
268.933505	10840.422252	27.950016
269.275689	10853.157085	27.955034
269.270533	10882.600121	27.960052
269.527021	10885.973768	27.965069
269.502083	10912.024497	27.970087
270.083109	10923.663977	27.975104
270.463748	10944.387650	27.980122
270.724217	10954.982143	27.985140
270.967867	10965.517984	27.990157
270.855047	10987.273856	27.995175
271.062756	11007.407086	28.000192
271.488631	11033.030146	28.005210
271.771266	11057.615008	28.010228
271.932650	11074.505301	28.015245
272.074057	11110.329724	28.020263
273.110534	11128.741798	28.025280
272.865571	11142.699487	28.030298
273.432385	11164.714549	28.035316
273.683710	11178.154908	28.040333
273.913838	11201.363641	28.045351
274.252829	11216.078419	28.050368
274.631275	11242.535379	28.055386
274.810607	11249.796672	28.060404
275.527774	11261.769897	28.065421
275.756793	11269.260880	28.070439
276.370674	11280.324742	28.075456
276.321268	11301.621413	28.080474
276.647315	11292.532040	28.085492
277.063382	11315.635985	28.090509
276.940529	11327.684222	28.095527
277.400361	11333.170350	28.100544
277.558428	11341.364910	28.105562
277.815553	11359.597892	28.110580
278.230651	11376.033500	28.115597
278.363714	11393.059620	28.120615
278.831214	11399.385951	28.125632
278.775138	11410.991397	28.130650
279.234150	11421.559512	28.135668
279.377421	11436.530768	28.140685
279.329887	11452.275924	28.145703
279.862435	11465.258524	28.150720
280.061471	11489.769691	28.155738
280.122895	11510.452583	28.160756
280.685826	11509.973122	28.165773
280.711778	11540.816196	28.170791
281.235108	11542.227935	28.175808
281.432840	11561.055623	28.180826
281.765054	11566.745825	28.185844
282.404788	11586.086293	28.190861
282.440598	11606.784595	28.195879
282.597537	11610.151299	28.200896
283.107889	11631.235643	28.205914
283.205654	11643.475947	28.210932
283.168928	11662.960414	28.215949
283.524594	11684.210772	28.220967
283.822887	11701.069519	28.225984
283.970150	11719.578014	28.231002
283.821050	11739.295551	28.236020
284.438178	11760.650692	28.241037
284.413265	11785.705346	28.246055
284.895151	11799.798113	28.251072
285.286116	11833.827238	28.256090
285.458095	11867.574506	28.261108
285.999438	11878.915569	28.266125
286.256662	11906.758403	28.271143
287.106087	11912.077575	28.276160
287.160843	11945.582898	28.281178
287.104313	11960.904573	28.286196
287.762237	11975.708878	28.291213
287.662843	12005.684902	28.296231
287.631085	12019.557494	28.301248
287.781728	12056.578521	28.306266
288.771012	12069.052373	28.311284
289.437508	12093.229928	28.316301
289.162746	12126.598122	28.321319
289.605800	12133.289670	28.326336
290.344917	12161.117486	28.331354
290.636948	12170.719488	28.336372
291.236951	12179.584841	28.341389
291.123410	12199.060652	28.346407
291.762467	12198.091050	28.351424
292.220729	12215.119159	28.356442
291.805544	12238.835283	28.361460
292.562586	12248.621661	28.366477
292.559483	12263.621153	28.371495
293.076183	12265.554089	28.376512
293.066215	12289.039075	28.381530
293.005375	12311.687893	28.386548
293.509797	12321.689630	28.391565
293.626831	12352.804342	28.396583
293.789763	12375.365643	28.401600
293.980045	12405.825340	28.406618
294.043070	12431.435261	28.411636
294.817050	12441.439564	28.416653
295.006171	12476.212709	28.421671
295.679641	12489.385463	28.426688
296.236464	12499.676443	28.431706
296.429291	12520.694937	28.436724
296.825031	12520.069886	28.441741
296.747496	12550.131531	28.446759
297.303924	12569.329432	28.451776
297.589336	12587.382601	28.456794
298.135441	12599.872192	28.461812
298.003792	12612.929824	28.466829
298.114575	12635.957155	28.471847
298.628746	12654.842276	28.476864
300.503101	12618.429234	28.481882
300.724166	12631.001219	28.486900
301.166582	12610.285455	28.491917
301.584492	12606.742927	28.496935
301.622908	12607.214166	28.501952
301.550025	12606.752068	28.506970
301.767693	12607.548097	28.511988
301.910885	12605.425374	28.517005
302.226967	12605.760656	28.522023
302.112033	12610.573691	28.527040
302.565896	12624.252654	28.532058
302.361741	12643.376873	28.537076
302.763820	12637.320293	28.542093
302.600202	12668.633523	28.547111
302.663543	12691.536442	28.552128
302.720628	12705.714762	28.557146
302.875183	12741.463387	28.562164
303.146264	12754.260389	28.567181
303.179601	12801.069961	28.572199
303.621847	12825.648325	28.577216
304.131842	12863.341127	28.582234
303.726534	12907.016926	28.587252
304.315945	12934.716508	28.592269
304.682868	12971.714718	28.597287
304.910835	13009.443683	28.602304
305.086142	13042.015631	28.607322
305.365519	13090.469809	28.612340
305.768974	13118.745868	28.617357
306.447837	13155.109577	28.622375
306.681260	13187.130040	28.627392
307.429599	13209.566871	28.632410
307.736448	13250.734581	28.637428
308.517363	13252.243945	28.642445
309.479531	13281.560561	28.647463
309.666293	13289.918390	28.652480
309.905255	13303.335777	28.657498
310.315493	13323.745545	28.662516
310.581345	13336.980411	28.667533
310.829615	13351.466357	28.672551
311.049887	13362.545043	28.677568
311.526983	13373.475479	28.682586
311.441140	13397.433268	28.687604
311.860606	13400.674782	28.692621
311.893911	13426.938922	28.697639
312.461491	13452.151432	28.702656
312.813488	13469.319863	28.707674
313.218516	13481.827271	28.712692
313.365272	13499.548323	28.717709
313.572743	13525.878245	28.722727
313.946525	13537.506772	28.727744
314.695603	13553.285511	28.732762
314.604153	13568.650746	28.737780
314.942204	13587.314059	28.742797
315.302254	13610.652796	28.747815
315.428497	13640.135731	28.752832
315.834242	13646.137529	28.757850
315.937700	13677.729819	28.762868
316.740220	13697.022130	28.767885
316.824517	13715.010677	28.772903
316.955109	13741.579084	28.777920
317.126768	13756.705361	28.782938
317.451004	13785.290448	28.787956
318.041378	13804.741060	28.792973
318.322526	13826.756775	28.797991
318.280372	13855.574640	28.803008
318.818899	13864.001978	28.808026
318.960023	13895.055744	28.813044
319.788619	13905.362359	28.818061
320.203595	13932.364509	28.823079
320.615816	13937.355122	28.828096
320.860297	13961.438523	28.833114
321.403928	13986.097933	28.838132
321.636178	13982.404719	28.843149
321.857704	14002.624474	28.848167
321.985519	14007.537854	28.853184
322.432339	14020.316112	28.858202
322.572941	14034.279982	28.863220
322.663263	14056.080276	28.868237
322.776080	14066.791170	28.873255
323.427288	14097.577760	28.878272
323.662123	14111.210837	28.883290
323.468130	14136.938633	28.888308
323.852995	14154.805232	28.893325
325.107921	14165.786644	28.898343
325.361794	14183.634060	28.903360
325.954654	14198.881470	28.908378
326.002439	14214.230482	28.913396
326.413080	14221.955856	28.918413
326.870020	14238.742025	28.923431
326.879906	14256.418868	28.928448
327.424622	14274.995049	28.933466
327.503852	14287.415361	28.938484
328.023718	14313.622156	28.943501
328.452477	14321.689720	28.948519
328.290415	14345.023263	28.953536
328.511224	14354.685673	28.958554
329.041048	14371.399980	28.963572
329.138740	14403.117561	28.968589
329.456564	14420.057840	28.973607
329.683769	14457.560174	28.978624
330.036999	14479.145564	28.983642
329.778865	14513.095851	28.988660
330.387330	14533.789414	28.993677
330.868567	14564.401811	28.998695
331.161957	14593.932771	29.003712
331.521738	14614.060966	29.008730
331.624525	14641.097240	29.013748
332.087755	14675.682958	29.018765
332.752856	14697.773177	29.023783
332.804554	14738.659201	29.028800
333.486195	14758.370027	29.033818
333.774978	14785.148683	29.038836
333.874097	14809.440306	29.043853
334.527042	14833.669902	29.048871
334.590800	14872.573112	29.053888
335.402816	14885.921815	29.058906
335.670283	14920.247418	29.063924
335.566892	14946.662792	29.068941
336.129549	14958.541502	29.073959
336.084236	14997.092743	29.078976
336.617280	15021.422918	29.083994
336.967709	15063.085999	29.089012
337.005790	15083.561371	29.094029
338.000482	15101.066058	29.099047
338.771920	15123.219569	29.104064
339.055649	15140.741541	29.109082
339.254152	15166.497156	29.114100
339.400540	15185.293432	29.119117
339.936323	15204.211021	29.124135
340.218105	15224.047155	29.129152
340.583157	15251.710717	29.134170
340.657230	15273.553155	29.139188
340.829771	15301.756298	29.144205
341.407750	15321.909006	29.149223
341.661087	15353.385057	29.154240
342.069461	15376.582738	29.159258
342.456874	15401.516114	29.164276
342.591506	15416.408926	29.169293
343.101003	15451.693129	29.174311
343.018637	15459.502572	29.179328
343.197285	15491.232445	29.184346
343.413220	15522.207512	29.189364
344.039609	15556.867279	29.194381
344.439020	15580.878458	29.199399
344.347700	15602.572279	29.204416
345.095323	15625.877874	29.209434
345.215634	15652.091717	29.214452
345.622280	15687.185458	29.219469
346.179386	15711.838928	29.224487
346.193942	15748.158000	29.229504
346.492779	15780.022927	29.234522
346.843325	15808.605596	29.239540
347.508595	15848.419938	29.244557
347.873278	15867.565316	29.249575
348.348547	15896.441079	29.254592
348.548382	15925.307483	29.259610
348.786616	15953.172979	29.264628
349.061100	15989.679525	29.269645
349.776071	16012.980061	29.274663
350.298740	16028.820883	29.279680
352.157183	16007.173655	29.284698
353.670940	15984.563917	29.289716
353.843729	15982.546181	29.294733
354.220762	15974.854878	29.299751
354.628166	15982.959915	29.304768
354.365727	15962.207295	29.309786
354.771086	15950.731579	29.314804
354.722531	15962.565975	29.319821
355.010054	15945.952524	29.324839
355.213614	15959.125781	29.329856
355.275129	15981.956367	29.334874
355.281280	15984.056549	29.339892
355.422664	16003.909069	29.344909
355.631506	16020.260694	29.349927
355.421934	16048.137697	29.354944
355.518211	16068.773281	29.359962
356.051872	16106.799053	29.364980
356.108544	16144.157028	29.369997
356.462700	16170.975945	29.375015
356.480006	16203.291973	29.380032
356.636644	16244.436986	29.385050
357.011712	16287.011705	29.390068
357.386491	16338.489140	29.395085
357.531764	16367.786237	29.400103
358.232347	16415.656954	29.405120
358.890068	16456.758658	29.410138
359.309284	16498.576296	29.415156
359.516605	16541.039250	29.420173
359.772803	16571.899262	29.425191
360.057012	16609.195267	29.430208
360.485190	16651.654916	29.435226
361.232855	16671.974974	29.440244
361.454068	16722.783983	29.445261
361.689302	16749.793832	29.450279
362.326514	16794.198919	29.455296
362.438855	16822.446187	29.460314
363.338202	16850.476066	29.465332
363.478076	16898.663585	29.470349
364.789429	16902.876808	29.475367
365.957642	16922.722207	29.480384
365.955714	16928.597484	29.485402
366.344270	16933.678073	29.490420
366.655247	16957.430100	29.495437
366.920834	16969.449472	29.500455
367.385293	16980.288274	29.505472
367.760950	16996.291590	29.510490
367.973621	17002.233703	29.515508
367.931106	17019.767735	29.520525
368.366081	17032.474653	29.525543
368.413501	17056.224892	29.530560
368.703141	17080.524464	29.535578
369.350633	17089.909531	29.540596
369.415687	17121.286246	29.545613
369.526817	17142.113010	29.550631
369.937767	17168.065022	29.555648
370.234537	17197.059413	29.560666
370.800769	17208.015444	29.565684
370.823535	17242.446431	29.570701
371.481867	17272.478007	29.575719
371.467773	17299.183381	29.580736
371.489015	17336.721750	29.585754
372.307425	17369.573757	29.590772
372.350402	17403.572958	29.595789
372.820493	17424.750292	29.600807
372.892049	17475.190809	29.605824
373.117004	17522.752811	29.610842
373.927866	17544.209449	29.615860
374.293021	17580.302475	29.620877
374.717221	17603.130217	29.625895
375.228308	17643.830463	29.630912
375.444948	17673.646092	29.635930
376.543827	17695.144934	29.640948
376.816727	17730.774399	29.645965
377.448060	17762.294708	29.650983
378.069688	17787.437119	29.656000
378.172727	17798.647044	29.661018
378.585593	17823.009205	29.666036
378.908221	17850.868606	29.671053
379.267007	17876.341717	29.676071
379.734148	17900.581476	29.681088
379.757743	17932.802092	29.686106
380.320144	17974.692677	29.691124
380.667200	17998.933612	29.696141
381.026240	18023.867780	29.701159
381.249708	18058.684859	29.706176
381.369317	18091.599210	29.711194
382.098076	18114.671850	29.716212
382.594470	18144.921078	29.721229
382.935324	18162.911266	29.726247
383.421554	18194.506946	29.731264
383.768670	18223.780096	29.736282
384.021049	18242.915355	29.741300
384.643272	18279.495294	29.746317
384.833370	18310.088918	29.751335
385.350545	18331.708868	29.756352
385.263045	18368.832536	29.761370
386.015331	18386.797184	29.766388
386.090542	18430.913789	29.771405
386.397743	18452.299208	29.776423
387.003836	18493.364095	29.781440
387.309186	18528.898445	29.786458
388.043497	18560.373210	29.791476
388.411957	18591.508393	29.796493
388.865546	18614.116671	29.801511
389.762769	18634.723285	29.806528
390.157453	18662.077070	29.811546
390.683514	18667.064415	29.816564
391.181217	18684.668105	29.821581
391.319487	18701.461319	29.826599
392.234131	18723.651066	29.831616
392.368009	18736.076678	29.836634
392.803232	18748.505840	29.841652
393.111539	18757.371221	29.846669
393.350350	18781.111046	29.851687
393.880416	18804.009559	29.856704
394.283777	18817.591734	29.861722
394.969433	18813.718092	29.866740
395.229734	18817.523140	29.871757
395.485324	18835.015868	29.876775
396.002490	18845.358435	29.881792
395.984065	18850.029555	29.886810
396.239922	18870.634229	29.891828
396.547194	18892.739074	29.896845
396.782922	18905.341800	29.901863
396.930916	18936.326650	29.906880
397.009700	18964.335623	29.911898
397.228009	18992.786528	29.916916
397.610788	19027.661144	29.921933
397.682154	19054.449722	29.926951
397.837505	19090.424802	29.931968
398.438457	19133.432785	29.936986
398.696134	19180.204257	29.942004
399.251640	19232.803600	29.947021
399.282786	19266.531098	29.952039
400.043680	19317.564223	29.957056
400.427015	19368.860439	29.962074
400.824053	19401.315085	29.967092
401.540849	19431.621476	29.972109
402.051776	19472.535896	29.977127
402.799879	19498.553780	29.982144
403.195526	19543.350025	29.987162
403.385297	19571.917012	29.992180
403.612765	19607.435062	29.997197
403.938734	19641.175825	30.002215
404.576711	19687.715274	30.007232
404.866314	19730.546336	30.012250
405.347657	19755.268862	30.017268
406.110756	19787.827412	30.022285
406.223622	19831.947762	30.027303
406.964949	19853.721642	30.032320
407.688251	19893.545514	30.037338
407.913953	19919.286644	30.042356
408.512790	19949.582038	30.047373
409.185900	19973.114250	30.052391
409.811298	19989.055316	30.057408
410.066939	20026.798855	30.062426
410.595970	20034.891989	30.067444
410.870866	20068.867548	30.072461
410.935477	20095.195394	30.077479
410.949871	20119.001197	30.082496
411.273444	20155.276973	30.087514
411.602273	20186.467430	30.092532
412.098464	20232.981495	30.097549
412.498452	20257.175926	30.102567
413.415312	20288.011908	30.107584
413.766488	20324.974018	30.112602
414.529556	20355.561341	30.117620
415.089552	20370.766322	30.122637
415.294360	20406.931511	30.127655
415.850725	20429.717522	30.132672
415.968070	20457.478206	30.137690
416.327883	20476.090505	30.142708
417.129070	20510.934970	30.147725
417.699984	20524.949501	30.152743
418.538242	20540.067422	30.157760
418.793670	20554.187989	30.162778
419.482508	20563.221310	30.167796
419.962661	20582.783367	30.172813
420.083243	20590.145266	30.177831
420.193522	20606.566647	30.182848
420.666684	20622.662891	30.187866
420.414227	20649.572447	30.192884
421.311167	20671.029867	30.197901
421.376534	20698.618269	30.202919
421.798432	20719.210250	30.207936
421.981214	20759.680946	30.212954
422.077929	20782.755062	30.217972
422.513696	20808.541494	30.222989
422.509994	20856.253439	30.228007
423.054005	20884.852110	30.233024
423.154316	20927.405487	30.238042
423.391438	20965.918893	30.243060
423.768778	20997.467009	30.248077
423.986043	21065.108246	30.253095
424.665729	21107.857525	30.258112
424.852563	21165.203757	30.263130
425.146422	21199.247822	30.268148
425.969188	21235.499768	30.273165
426.456208	21285.113316	30.278183
427.112443	21332.091035	30.283200
427.283793	21384.459779	30.288218
427.783429	21426.470339	30.293236
428.145985	21473.404208	30.298253
428.782668	21519.337180	30.303271
429.285474	21554.794684	30.308288
430.020472	21600.060358	30.313306
430.628022	21645.881836	30.318324
431.273713	21681.697443	30.323341
431.712372	21719.439601	30.328359
431.914469	21738.814256	30.333376
432.502193	21782.088229	30.338394
432.576789	21826.861892	30.343412
432.957210	21854.894948	30.348429
433.606072	21898.543792	30.353447
433.936395	21935.050906	30.358464
434.619526	21978.397834	30.363482
434.870655	22013.294206	30.368500
435.946448	22035.064245	30.373517
436.975425	22054.749715	30.378535
438.346260	22060.490222	30.383552
438.905069	22074.421338	30.388570
439.522912	22084.244627	30.393588
439.883365	22078.636222	30.398605
439.890985	22105.840743	30.403623
440.314714	22114.944171	30.408640
440.316447	22132.053619	30.413658
440.508171	22156.774175	30.418676
440.968084	22174.657445	30.423693
440.971979	22208.305479	30.428711
441.477975	22230.837399	30.433728
441.760111	22257.123025	30.438746
441.933126	22298.366923	30.443764
442.335107	22317.896678	30.448781
442.264087	22371.248503	30.453799
442.152842	22408.359789	30.458816
442.484104	22453.699543	30.463834
442.894312	22505.992660	30.468852
443.466161	22552.767036	30.473869
444.062671	22614.435254	30.478887
444.600860	22657.082658	30.483904
445.422287	22711.335901	30.488922
445.775446	22753.553847	30.493940
446.259667	22795.836854	30.498957
446.697464	22830.475260	30.503975
447.653572	22868.299599	30.508992
448.141988	22911.747487	30.514010
447.795343	22951.699543	30.519028
448.998133	22983.341322	30.524045
449.654468	22998.346611	30.529063
450.715871	23026.885047	30.534080
451.240172	23042.025840	30.539098
451.514193	23075.998132	30.544116
452.844556	23072.286111	30.549133
453.861817	23075.203200	30.554151
454.076835	23068.489595	30.559168
454.806745	23074.970820	30.564186
454.814910	23078.020830	30.569204
455.245198	23074.847797	30.574221
455.308607	23091.203685	30.579239
455.563395	23092.318916	30.584256
455.570016	23117.364915	30.589274
455.656291	23141.268681	30.594292
456.155912	23163.140616	30.599309
456.187501	23196.704009	30.604327
456.334593	23217.321031	30.609344
456.809489	23265.151061	30.614362
456.848389	23314.807143	30.619380
457.280256	23348.405269	30.624397
457.421424	23390.305209	30.629415
458.368007	23430.989720	30.634432
459.024335	23468.597122	30.639450
459.447204	23512.801732	30.644468
460.167348	23540.349078	30.649485
460.636480	23583.984810	30.654503
460.785876	23611.024689	30.659520
461.746240	23651.157096	30.664538
462.070050	23692.030828	30.669556
462.703206	23721.776953	30.674573
462.984740	23772.687145	30.679591
463.930141	23790.757985	30.684608
464.320702	23828.474980	30.689626
464.374706	23868.996562	30.694644
464.874676	23911.796964	30.699661
465.189033	23949.582077	30.704679
465.514597	23990.525618	30.709696
466.056845	24024.895219	30.714714
466.385020	24078.668630	30.719732
467.005614	24120.761968	30.724749
467.130722	24167.350057	30.729767
467.982476	24216.905288	30.734784
468.138182	24253.096297	30.739802
468.541378	24302.373037	30.744820
469.243202	24341.756795	30.749837
469.531415	24397.269370	30.754855
469.889063	24446.036838	30.759872
470.343165	24489.953355	30.764890
470.938084	24539.006539	30.769908
471.350034	24581.902089	30.774925
471.723250	24632.181424	30.779943
471.843450	24686.852335	30.784960
472.905236	24724.940809	30.789978
473.254812	24776.839361	30.794996
473.794464	24821.256627	30.800013
474.364966	24879.672917	30.805031
474.689124	24937.641440	30.810048
475.477940	24982.721099	30.815066
476.011105	25019.557546	30.820084
476.263637	25069.053915	30.825101
477.327086	25112.978060	30.830119
477.674791	25153.819773	30.835136
478.128355	25199.226938	30.840154
478.357741	25245.277050	30.845172
478.652081	25276.829548	30.850189
479.345740	25324.657392	30.855207
479.925076	25364.284638	30.860224
480.649741	25406.221915	30.865242
480.858371	25450.159583	30.870260
481.326504	25485.014397	30.875277
482.331388	25522.937468	30.880295
482.094106	25574.513242	30.885312
482.602145	25608.692992	30.890330
482.993407	25647.976780	30.895348
483.386763	25686.326664	30.900365
484.079204	25725.320886	30.905383
484.832284	25755.883347	30.910400
485.324287	25793.113107	30.915418
485.790009	25833.078882	30.920436
485.804978	25867.542912	30.925453
486.586888	25914.219058	30.930471
486.775958	25960.312477	30.935488
487.281684	26002.334887	30.940506
487.513211	26049.159589	30.945524
488.157239	26103.189690	30.950541
488.308440	26151.835419	30.955559
488.337184	26204.911342	30.960576
488.890606	26254.440000	30.965594
489.355861	26320.868546	30.970612
490.073186	26365.518947	30.975629
490.714079	26427.512126	30.980647
491.290399	26478.807214	30.985664
491.827309	26532.430613	30.990682
492.249539	26593.725739	30.995700
492.601870	26639.920029	31.000717
493.199066	26707.072580	31.005735
494.153216	26758.674810	31.010752
494.645807	26794.578629	31.015770
495.349199	26855.581942	31.020788
495.377293	26902.294486	31.025805
496.172530	26950.270850	31.030823
496.254213	27010.103572	31.035840
497.458545	27043.312509	31.040858
498.179305	27090.169182	31.045876
498.593865	27126.345317	31.050893
499.414103	27170.835604	31.055911
499.851026	27223.329520	31.060928
500.494002	27256.010668	31.065946
500.733018	27304.468400	31.070964
501.071757	27354.341853	31.075981
501.856215	27379.047207	31.080999
501.941622	27430.366715	31.086016
502.664635	27469.044349	31.091034
503.316004	27524.677025	31.096052
503.689402	27564.248892	31.101069
504.104334	27599.883372	31.106087
504.278052	27659.201470	31.111104
505.339632	27687.854925	31.116122
505.996114	27734.477960	31.121140
506.435647	27774.092951	31.126157
507.058939	27814.737457	31.131175
507.585785	27856.353922	31.136192
507.991382	27892.558382	31.141210
508.413335	27935.637270	31.146228
509.374036	27979.210394	31.151245
509.474945	28018.080906	31.156263
509.931185	28046.945907	31.161280
510.775090	28086.841462	31.166298
511.188206	28130.051641	31.171316
511.222981	28171.125963	31.176333
512.267417	28209.357534	31.181351
512.655111	28250.483844	31.186368
513.230821	28281.083392	31.191386
513.578502	28320.487747	31.196404
514.043761	28369.917219	31.201421
514.673423	28395.359542	31.206439
515.471913	28437.594772	31.211456
515.875995	28477.725162	31.216474
516.256038	28512.711127	31.221492
516.572997	28549.591014	31.226509
517.465865	28578.185633	31.231527
517.648689	28627.249473	31.236544
518.234207	28647.333276	31.241562
518.445228	28681.334977	31.246580
518.717503	28729.967822	31.251597
520.049807	28744.441577	31.256615
519.910408	28789.455039	31.261632
520.839030	28823.539742	31.266650
521.828252	28858.706005	31.271668
522.064831	28891.404098	31.276685
522.568769	28925.117862	31.281703
522.783390	28951.276663	31.286720
523.229036	28996.089383	31.291738
523.685801	29035.729623	31.296756
524.139888	29080.389727	31.301773
524.965746	29114.485759	31.306791
525.328246	29160.896437	31.311808
525.902643	29194.352942	31.316826
527.016745	29231.420521	31.321844
527.348830	29271.637258	31.326861
527.901621	29299.948821	31.331879
528.133023	29346.100981	31.336896
528.283813	29388.401919	31.341914
528.758633	29433.485391	31.346932
528.798667	29486.266579	31.351949
529.441558	29526.927603	31.356967
529.698509	29592.093958	31.361984
530.183631	29661.548072	31.367002
530.475815	29717.143290	31.372020
531.125797	29795.678873	31.377037
531.690037	29842.799269	31.382055
532.292706	29906.366598	31.387072
533.042207	29956.125639	31.392090
533.908125	30013.699339	31.397108
534.281423	30067.925550	31.402125
535.011784	30120.795918	31.407143
535.293575	30170.566989	31.412160
535.896414	30227.503597	31.417178
536.922534	30276.779060	31.422196
537.129571	30333.806986	31.427213
537.764605	30398.897769	31.432231
538.483134	30445.255874	31.437248
538.968528	30497.871485	31.442266
539.263374	30559.532995	31.447284
539.407418	30616.550213	31.452301
540.156475	30675.508495	31.457319
540.348917	30728.753988	31.462336
540.469387	30792.868409	31.467354
541.142650	30859.860248	31.472372
541.876368	30935.515835	31.477389
542.452312	31001.580983	31.482407
542.758879	31067.561754	31.487424
543.626920	31135.752816	31.492442
544.579210	31193.991250	31.497460
544.723489	31256.737196	31.502477
545.838094	31306.035558	31.507495
546.431540	31363.832467	31.512512
546.820914	31422.373387	31.517530
547.942786	31468.357989	31.522548
548.373397	31529.186285	31.527565
548.609125	31570.433967	31.532583
549.681499	31619.954780	31.537600
550.556496	31659.913276	31.542618
550.972415	31710.871741	31.547636
551.062979	31762.906705	31.552653
551.673558	31804.370347	31.557671
552.393709	31844.370753	31.562688
553.178428	31897.524564	31.567706
553.442608	31932.293626	31.572724
554.001218	31968.077211	31.577741
554.918180	32010.853566	31.582759
555.426623	32046.696127	31.587776
555.646931	32087.496360	31.592794
556.392675	32126.966210	31.597812
556.270859	32167.848687	31.602829
556.753815	32223.284444	31.607847
557.633342	32273.710007	31.612864
558.384006	32324.128715	31.617882
559.004741	32354.406046	31.622900
559.661489	32408.961562	31.627917
560.004659	32456.479067	31.632935
560.489082	32498.356561	31.637952
561.167441	32539.687609	31.642970
561.474791	32576.555449	31.647988
561.928457	32638.974076	31.653005
562.305082	32695.460804	31.658023
562.828777	32751.569873	31.663040
563.032504	32808.713615	31.668058
563.583736	32873.799033	31.673076
563.871075	32947.552542	31.678093
564.602109	32996.894079	31.683111
565.272533	33068.826843	31.688128
565.616132	33135.386625	31.693146
566.315874	33187.532863	31.698164
566.604484	33271.363207	31.703181
567.067359	33334.404391	31.708199
567.798719	33412.702710	31.713216
568.244592	33496.233457	31.718234
568.867135	33559.652840	31.723252
569.326336	33638.988216	31.728269
570.209390	33704.327660	31.733287
570.635014	33776.168238	31.738304
571.336353	33845.441933	31.743322
572.565859	33896.855357	31.748340
573.228541	33961.380304	31.753357
573.585705	34025.807903	31.758375
574.581401	34086.525864	31.763392
575.036458	34140.179776	31.768410
576.152601	34187.788123	31.773428
576.485212	34259.999535	31.778445
577.276673	34312.077027	31.783463
577.546435	34365.803411	31.788480
578.060119	34421.644846	31.793498
578.828570	34474.692300	31.798516
579.824809	34522.002717	31.803533
580.477113	34577.666985	31.808551
580.934499	34612.144106	31.813568
581.524050	34669.330714	31.818586
582.691418	34704.491691	31.823604
583.176050	34756.555158	31.828621
583.433682	34800.366067	31.833639
584.093947	34835.033993	31.838656
584.369849	34888.751458	31.843674
585.214682	34929.599650	31.848692
585.510627	34986.700325	31.853709
586.318004	35033.765743	31.858727
586.774466	35076.865793	31.863744
586.991214	35134.967886	31.868762
587.626238	35188.708665	31.873780
588.007218	35247.014229	31.878797
588.405730	35299.390228	31.883815
589.334314	35352.369507	31.888832
589.889693	35410.037542	31.893850
590.620483	35458.331832	31.898868
591.007373	35528.648915	31.903885
591.540108	35582.085947	31.908903
592.096336	35628.241523	31.913920
592.739737	35682.279050	31.918938
593.279077	35719.638742	31.923956
593.881030	35771.382691	31.928973
594.376401	35823.703104	31.933991
596.052300	35859.804458	31.939008
596.542661	35908.370275	31.944026
596.954449	35937.306043	31.949044
597.336465	35980.161826	31.954061
597.698309	36031.987426	31.959079
598.551878	36074.900839	31.964096
599.113831	36122.817819	31.969114
599.667867	36166.576522	31.974132
600.228369	36225.975854	31.979149
600.884251	36277.627088	31.984167
601.049972	36324.777191	31.989184
601.289630	36398.268756	31.994202
601.973131	36433.033748	31.999220
602.421871	36503.899840	32.004237
603.148695	36578.608415	32.009255
603.610376	36635.790945	32.014272
604.016780	36703.464497	32.019290
604.578504	36768.395032	32.024308
604.699016	36845.020197	32.029325
605.357289	36910.673760	32.034343
606.062369	36982.676426	32.039360
606.212489	37056.993525	32.044378
606.994460	37138.074009	32.049396
607.973886	37209.845802	32.054413
608.073330	37295.522226	32.059431
609.019324	37377.327738	32.064448
609.380165	37467.989545	32.069466
609.881180	37543.828522	32.074484
610.834196	37626.369413	32.079501
611.209122	37706.415309	32.084519
612.320023	37777.069103	32.089536
613.516403	37847.317587	32.094554
614.256717	37927.101772	32.099572
614.771881	37979.769175	32.104589
615.489756	38048.608075	32.109607
616.425186	38113.853822	32.114624
617.999924	38156.238930	32.119642
618.992925	38197.148831	32.124660
619.782705	38245.538623	32.129677
620.464802	38286.711835	32.134695
621.441632	38301.271459	32.139712
622.074210	38341.013674	32.144730
622.674400	38386.477720	32.149748
623.022693	38407.094902	32.154765
623.415238	38460.652089	32.159783
623.927950	38499.161430	32.164800
624.115136	38552.386834	32.169818
624.606839	38596.654166	32.174836
625.188161	38645.603617	32.179853
625.341870	38703.478252	32.184871
625.902281	38765.237518	32.189888
626.336085	38827.646169	32.194906
626.620812	38885.872097	32.199924
627.114595	38954.997843	32.204941
627.288373	39032.863895	32.209959
627.737506	39104.851170	32.214976
628.324105	39186.459334	32.219994
629.209318	39271.111765	32.225012
630.073311	39337.364931	32.230029
630.376029	39416.180287	32.235047
631.100340	39485.616987	32.240064
631.717457	39561.325116	32.245082
632.418405	39632.092052	32.250100
633.593862	39697.953882	32.255117
633.740457	39761.022644	32.260135
634.359960	39825.771388	32.265152
634.968757	39902.744993	32.270170
635.485103	39974.364652	32.275188
636.282130	40046.458848	32.280205
636.472238	40129.361862	32.285223
637.192402	40192.485231	32.290240
637.617564	40275.078388	32.295258
638.131335	40348.534028	32.300276
638.457894	40442.133153	32.305293
639.066637	40516.814325	32.310311
640.132062	40587.069833	32.315328
640.953426	40685.045499	32.320346
641.212196	40763.444589	32.325364
642.014240	40835.023312	32.330381
642.701367	40921.843982	32.335399
644.053202	40989.067034	32.340416
644.435809	41083.847107	32.345434
645.287764	41159.510186	32.350452
646.573316	41230.072545	32.355469
646.796717	41310.396100	32.360487
647.694796	41371.075724	32.365504
648.326333	41446.157808	32.370522
648.326158	41513.222113	32.375540
649.221731	41589.233293	32.380557
649.609240	41682.686513	32.385575
650.451498	41741.883345	32.390592
651.154903	41824.099420	32.395610
651.693329	41907.953361	32.400628
652.528682	41979.549927	32.405645
652.943501	42068.441725	32.410663
654.185826	42135.469295	32.415680
654.379877	42222.040123	32.420698
654.817364	42288.434702	32.425716
655.512665	42386.481349	32.430733
655.716073	42476.638334	32.435751
656.539667	42555.364805	32.440768
657.328658	42650.521094	32.445786
658.157744	42741.901498	32.450804
658.976732	42817.384226	32.455821
659.773052	42895.374716	32.460839
660.988247	42970.467083	32.465856
661.510112	43044.263578	32.470874
662.577090	43105.037648	32.475892
663.494244	43186.400208	32.480909
664.199291	43237.415640	32.485927
665.939852	43297.784870	32.490944
666.293446	43347.160327	32.495962
666.899333	43398.173720	32.500980
667.780132	43443.442620	32.505997
668.069261	43505.205947	32.511015
668.905687	43551.625436	32.516032
669.799488	43604.735430	32.521050
670.706557	43661.755353	32.526068
671.521935	43689.837532	32.531085
671.838079	43743.324841	32.536103
672.168213	43790.659381	32.541120
672.928838	43842.500792	32.546138
673.058107	43898.444456	32.551156
673.796171	43958.069792	32.556173
674.424227	44025.948161	32.561191
674.601297	44094.763638	32.566208
675.161691	44153.623420	32.571226
675.290078	44234.591058	32.576244
676.345238	44303.807748	32.581261
676.307679	44387.357997	32.586279
676.986190	44463.783219	32.591296
677.316858	44540.733819	32.596314
678.259013	44629.957569	32.601332
678.616050	44695.284709	32.606349
679.376605	44781.849107	32.611367
679.498896	44859.416599	32.616384
680.759807	44941.490686	32.621402
681.031635	45026.305956	32.626420
681.612858	45105.336012	32.631437
682.383290	45200.483086	32.636455
682.984024	45288.686740	32.641472
683.922138	45386.007786	32.646490
684.061030	45476.840390	32.651508
684.876063	45567.646425	32.656525
685.370179	45678.652344	32.661543
686.187522	45764.368717	32.666560
687.203769	45860.968752	32.671578
687.716982	45957.775953	32.676596
688.982889	46037.823551	32.681613
689.828926	46138.510997	32.686631
690.476027	46214.446444	32.691648
691.118743	46302.951010	32.696666
692.258676	46376.888490	32.701684
693.216613	46454.664828	32.706701
693.960643	46541.088460	32.711719
695.719446	46589.515966	32.716736
696.881452	46657.908839	32.721754
697.434353	46712.239994	32.726772
698.115902	46788.045707	32.731789
698.389489	46847.040461	32.736807
698.872801	46913.184830	32.741824
699.964420	46970.297823	32.746842
700.393373	47050.946566	32.751860
701.099501	47112.901950	32.756877
701.461864	47181.609481	32.761895
702.059847	47262.733173	32.766912
702.850018	47325.250046	32.771930
703.291124	47417.270218	32.776948
704.057482	47489.145571	32.781965
704.509988	47566.618790	32.786983
704.843585	47650.273391	32.792000
705.517441	47738.747894	32.797018
706.052521	47827.650080	32.802036
707.065439	47910.444573	32.807053
707.739187	48007.901918	32.812071
707.744556	48096.201678	32.817088
708.896224	48171.110576	32.822106
709.796370	48270.177051	32.827124
710.404480	48363.699436	32.832141
710.987626	48461.117286	32.837159
711.439148	48543.316090	32.842176
712.566979	48619.967705	32.847194
713.337745	48729.094783	32.852212
713.963014	48811.528022	32.857229
715.003365	48896.056095	32.862247
715.641016	48996.717448	32.867264
716.554352	49080.661038	32.872282
717.292228	49174.661682	32.877300
717.988181	49259.835979	32.882317
718.524114	49338.069980	32.887335
719.317205	49435.988519	32.892352
719.705563	49511.961099	32.897370
720.425442	49607.482851	32.902388
721.099457	49702.226257	32.907405
721.703037	49784.594627	32.912423
722.364711	49897.084862	32.917440
723.142564	49992.030382	32.922458
723.808011	50088.087851	32.927476
724.156996	50183.235010	32.932493
724.736278	50268.660545	32.937511
725.596335	50374.822647	32.942528
726.281981	50457.581392	32.947546
726.830979	50562.971803	32.952564
727.847628	50645.284741	32.957581
728.257131	50754.729636	32.962599
728.968676	50847.574143	32.967616
730.135394	50944.102230	32.972634
730.585029	51039.656978	32.977652
731.525909	51125.067321	32.982669
732.031930	51217.960357	32.987687
732.779698	51326.707961	32.992704
733.981041	51415.803535	32.997722
734.733307	51511.026081	33.002740
735.319448	51605.973440	33.007757
736.331662	51700.534656	33.012775
737.081106	51797.970164	33.017792
737.892301	51887.499086	33.022810
738.918235	51976.986451	33.027828
740.170237	52047.673684	33.032845
740.921400	52120.118470	33.037863
741.858255	52212.843651	33.042880
742.899094	52288.273402	33.047898
743.531908	52368.907403	33.052916
744.134781	52442.559400	33.057933
744.766539	52529.764585	33.062951
745.117607	52613.030294	33.067968
745.745064	52697.153906	33.072986
746.694332	52792.248923	33.078004
747.436357	52873.625007	33.083021
748.184659	52958.304597	33.088039
748.630930	53053.117957	33.093056
749.313030	53142.528757	33.098074
750.330899	53246.592279	33.103092
751.602902	53315.770812	33.108109
753.328363	53385.897816	33.113127
754.045633	53443.505981	33.118144
755.201170	53505.224058	33.123162
756.213622	53590.014160	33.128180
756.939390	53644.854220	33.133197
757.822251	53692.244655	33.138215
758.204530	53757.408871	33.143232
758.959252	53817.709731	33.148250
759.487650	53881.005219	33.153268
760.071608	53949.946406	33.158285
760.615358	54020.568818	33.163303
761.087247	54096.479085	33.168320
761.281896	54178.709636	33.173338
761.943811	54279.255310	33.178356
762.165968	54355.833538	33.183373
763.187299	54450.937269	33.188391
763.534893	54551.865065	33.193408
764.173073	54643.874177	33.198426
764.435758	54755.286607	33.203444
765.463600	54856.880191	33.208461
766.625014	54944.248264	33.213479
767.365554	55051.077983	33.218496
768.052509	55154.397765	33.223514
769.150434	55247.679207	33.228532
769.965934	55345.355150	33.233549
770.658134	55446.830565	33.238567
771.308761	55549.330702	33.243584
772.009180	55634.200351	33.248602
772.790490	55739.826470	33.253620
773.483685	55844.298814	33.258637
774.470105	55943.573240	33.263655
775.174970	56049.750792	33.268672
775.789513	56147.546188	33.273690
776.155548	56239.797452	33.278708
776.559828	56345.520973	33.283725
777.784629	56428.891533	33.288743
778.518980	56545.663653	33.293760
779.065110	56634.721055	33.298778
779.760427	56743.709517	33.303796
780.363975	56853.389946	33.308813
781.040785	56956.638630	33.313831
781.492601	57092.689819	33.318848
782.183125	57193.264459	33.323866
783.137618	57307.369400	33.328884
783.679756	57423.161167	33.333901
784.345724	57542.541345	33.338919
785.012075	57661.827381	33.343936
786.852458	57765.127208	33.348954
788.247492	57875.427527	33.353972
788.520153	57979.487942	33.358989
789.753264	58096.211590	33.364007
790.318684	58196.622450	33.369024
791.515081	58299.172488	33.374042
792.590781	58394.033257	33.379060
793.837231	58499.723138	33.384077
795.003354	58592.610769	33.389095
795.685354	58693.864223	33.394112
796.031723	58779.956172	33.399130
796.823182	58868.154892	33.404148
797.237218	58969.119267	33.409165
798.234528	59073.747569	33.414183
798.801892	59182.473484	33.419200
800.069109	59280.479164	33.424218
800.756714	59386.727812	33.429236
801.071728	59493.121027	33.434253
801.984987	59590.125228	33.439271
802.296279	59716.415305	33.444288
802.798685	59817.723161	33.449306
803.751167	59937.316441	33.454324
804.303542	60060.939516	33.459341
805.378117	60168.050749	33.464359
805.987144	60283.525507	33.469376
806.782195	60412.969192	33.474394
808.025902	60539.969148	33.479412
808.520859	60658.839959	33.484429
810.237548	60774.753016	33.489447
810.808426	60884.953771	33.494464
811.283289	61000.650797	33.499482
812.446463	61110.539558	33.504500
813.078575	61219.752298	33.509517
814.068725	61333.147206	33.514535
814.841899	61459.124921	33.519552
815.635064	61568.274866	33.524570
816.608645	61680.530439	33.529588
817.006031	61795.758142	33.534605
818.454111	61903.625532	33.539623
819.266361	62011.276683	33.544640
819.591495	62135.398811	33.549658
820.405866	62242.570451	33.554676
821.000593	62364.911015	33.559693
821.688082	62493.911676	33.564711
822.449069	62604.779095	33.569728
823.527812	62729.316984	33.574746
824.251843	62848.459558	33.579764
825.606851	62961.455257	33.584781
826.627388	63060.329140	33.589799
827.826494	63173.459338	33.594816
828.364318	63287.875641	33.599834
829.653429	63388.318383	33.604852
830.253386	63501.031505	33.609869
831.232610	63601.356054	33.614887
831.842653	63691.748599	33.619904
832.594872	63789.709698	33.624922
833.646381	63872.962654	33.629940
834.173966	63969.767182	33.634957
835.440008	64055.576977	33.639975
837.071869	64144.278457	33.644992
837.804561	64224.286026	33.650010
838.673418	64307.842869	33.655028
839.245275	64406.639639	33.660045
840.040869	64487.314170	33.665063
840.771397	64586.641742	33.670080
840.750113	64680.481116	33.675098
841.894658	64775.202050	33.680116
842.030651	64891.223708	33.685133
842.615127	64996.070893	33.690151
843.386059	65117.665185	33.695168
843.935096	65236.325848	33.700186
845.176046	65354.347636	33.705204
845.543476	65481.928118	33.710221
846.424861	65598.797203	33.715239
847.627551	65712.338925	33.720256
848.775251	65836.321394	33.725274
850.575809	65933.650765	33.730292
851.246748	66044.361862	33.735309
851.966665	66145.753232	33.740327
852.736980	66257.460465	33.745344
853.533662	66385.778092	33.750362
854.076354	66491.202367	33.755380
854.801689	66609.879487	33.760397
855.570459	66723.309054	33.765415
856.576350	66853.649492	33.770432
856.954776	66985.283456	33.775450
857.891816	67106.046160	33.780468
858.491014	67246.040995	33.785485
858.895045	67380.865911	33.790503
859.689217	67500.061371	33.795520
860.781284	67647.032767	33.800538
862.106020	67773.216430	33.805556
862.674419	67919.530599	33.810573
863.763970	68053.443069	33.815591
864.552513	68183.770896	33.820608
865.728937	68317.139523	33.825626
866.771698	68443.152696	33.830644
867.568175	68591.924755	33.835661
868.327261	68710.677624	33.840679
869.327064	68852.134028	33.845696
870.354667	68980.321600	33.850714
871.365274	69092.452859	33.855732
872.734444	69216.184494	33.860749
874.137174	69324.496130	33.865767
875.461802	69425.221162	33.870784
876.023628	69535.108741	33.875802
877.234349	69634.753481	33.880820
877.781267	69747.850369	33.885837
878.800336	69855.406396	33.890855
879.923256	69953.518058	33.895872
881.018049	70045.065161	33.900890
882.062624	70142.368694	33.905908
882.860039	70244.500307	33.910925
883.807399	70339.133539	33.915943
884.720395	70431.041274	33.920960
885.325942	70534.989258	33.925978
886.047944	70640.682604	33.930996
886.639874	70746.202037	33.936013
887.707214	70847.849093	33.941031
888.461409	70955.258585	33.946048
888.798357	71060.461452	33.951066
889.450853	71172.941289	33.956084
890.349428	71284.988816	33.961101
890.801641	71390.382835	33.966119
891.638639	71503.598915	33.971136
891.943314	71625.181456	33.976154
893.072263	71743.149905	33.981172
893.466841	71883.481035	33.986189
894.619503	71987.490664	33.991207
895.898763	72102.255332	33.996224
896.503089	72217.739708	34.001242
897.986172	72345.492369	34.006260
898.408208	72475.331677	34.011277
899.332041	72597.588417	34.016295
900.084585	72721.531128	34.021312
900.713815	72866.294321	34.026330
901.265013	72990.031672	34.031348
902.122163	73130.977083	34.036365
903.181520	73281.103945	34.041383
904.377262	73414.184824	34.046400
904.719312	73562.200283	34.051418
905.695695	73707.461644	34.056436
906.509842	73853.345373	34.061453
907.566559	73998.867280	34.066471
909.105550	74132.622856	34.071488
910.468382	74269.033078	34.076506
911.633494	74402.934579	34.081524
912.367954	74533.379366	34.086541
912.898904	74672.637007	34.091559
914.814800	74794.425183	34.096576
915.950471	74916.248664	34.101594
917.024369	75032.953879	34.106612
917.774350	75154.988161	34.111629
918.609048	75282.656926	34.116647
919.435675	75401.726266	34.121664
920.188048	75533.457915	34.126682
920.676971	75658.706975	34.131700
921.379783	75799.347304	34.136717
922.432751	75932.435538	34.141735
923.091192	76070.757436	34.146752
924.074238	76221.334517	34.151770
924.910904	76350.565048	34.156788
926.118279	76500.581829	34.161805
926.292530	76651.605989	34.166823
927.172051	76793.020248	34.171840
928.080953	76951.875088	34.176858
929.342263	77097.067240	34.181876
930.102280	77245.025406	34.186893
931.380261	77401.450266	34.191911
932.651529	77533.278457	34.196928
933.296873	77680.537468	34.201946
934.299202	77822.437580	34.206964
935.957103	77955.639950	34.211981
937.333536	78083.348779	34.216999
938.806821	78203.704762	34.222016
939.890030	78323.297496	34.227034
940.658942	78453.614151	34.232052
941.713175	78561.428557	34.237069
942.929122	78685.757998	34.242087
943.585681	78794.373290	34.247104
944.020272	78927.208837	34.252122
944.767826	79055.052879	34.257140
946.084148	79180.342553	34.262157
946.507541	79325.346646	34.267175
947.564514	79439.009800	34.272192
948.203226	79570.531132	34.277210
948.897533	79703.903804	34.282228
949.942166	79833.885379	34.287245
950.343160	79976.297429	34.292263
951.926560	80107.620825	34.297280
952.545085	80243.387820	34.302298
953.109838	80384.965533	34.307316
954.047374	80509.015954	34.312333
955.235266	80647.468025	34.317351
956.434326	80775.265844	34.322368
956.910697	80908.745040	34.327386
957.784089	81046.416680	34.332404
959.102081	81177.442379	34.337421
960.214709	81308.553525	34.342439
961.468185	81418.569033	34.347456
963.152572	81550.396456	34.352474
964.519837	81653.087261	34.357492
965.900652	81760.033964	34.362509
966.414252	81881.321658	34.367527
967.184051	81988.541648	34.372544
968.215473	82103.380138	34.377562
969.495196	82235.126837	34.382580
970.168798	82338.220536	34.387597
971.058111	82459.100977	34.392615
972.293459	82572.585715	34.397632
972.954529	82705.829652	34.402650
973.514371	82827.715715	34.407668
974.432615	82960.507213	34.412685
974.882212	83090.555500	34.417703
975.494709	83226.227346	34.422720
976.453739	83378.526435	34.427738
977.302880	83520.089017	34.432756
978.573655	83666.954076	34.437773
979.206001	83811.135816	34.442791
980.872052	83952.438940	34.447808
981.612469	84095.471980	34.452826
982.592022	84249.285571	34.457844
983.585097	84394.727120	34.462861
984.426612	84552.235375	34.467879
984.964196	84699.418473	34.472896
985.835527	84858.182972	34.477914
986.251259	85013.063260	34.482932
987.390188	85186.642136	34.487949
988.498652	85352.919201	34.492967
990.085970	85511.771814	34.497984
991.217594	85672.010922	34.503002
991.914575	85841.251415	34.508020
992.710428	86000.434847	34.513037
993.577450	86170.048136	34.518055
995.315427	86322.794079	34.523072
996.010485	86494.659265	34.528090
996.826202	86654.887914	34.533108
998.075126	86819.557489	34.538125
998.807760	86988.869945	34.543143
999.695629	87150.766876	34.548160
1000.581387	87321.802811	34.553178
1001.249543	87497.748644	34.558196
1002.468167	87666.131032	34.563213
1003.368305	87835.611603	34.568231
1004.544636	88001.712633	34.573248
1005.753401	88179.541868	34.578266
1006.495629	88360.038095	34.583284
1007.997891	88524.652196	34.588301
1008.812341	88690.514344	34.593319
1010.289237	88847.091615	34.598336
1011.330362	89023.531105	34.603354
1012.206068	89185.450273	34.608372
1013.378790	89355.522961	34.613389
1014.095918	89520.628627	34.618407
1015.530863	89684.958146	34.623424
1016.906888	89827.844590	34.628442
1017.665902	89992.218769	34.633460
1018.765251	90146.031972	34.638477
1019.965799	90297.437109	34.643495
1021.060458	90433.203402	34.648512
1021.527676	90575.840069	34.653530
1022.493590	90728.274147	34.658548
1023.567095	90880.001487	34.663565
1024.634046	91032.610591	34.668583
1025.480721	91179.940884	34.673600
1027.227478	91318.812744	34.678618
1028.458600	91450.619160	34.683636
1029.781375	91592.809745	34.688653
1030.712287	91738.294033	34.693671
1031.688809	91875.626020	34.698688
1032.970744	92013.097980	34.703706
1033.785261	92148.597616	34.708724
1034.533255	92300.052428	34.713741
1035.589011	92458.273763	34.718759
1036.848619	92584.954891	34.723776
1038.367509	92730.043745	34.728794
1038.941187	92873.062359	34.733812
1040.119134	93022.304650	34.738829
1040.864512	93167.587754	34.743847
1042.458095	93312.724645	34.748864
1043.189004	93450.916448	34.753882
1044.063618	93593.370314	34.758900
1044.893566	93742.313957	34.763917
1046.464387	93894.895388	34.768935
1046.995567	94034.345244	34.773952
1048.162145	94197.059858	34.778970
1048.487755	94353.572648	34.783988
1049.551834	94522.914716	34.789005
1050.239597	94695.415698	34.794023
1051.531688	94865.216011	34.799040
1052.603623	95036.965671	34.804058
1053.480891	95198.981632	34.809076
1054.323992	95369.385299	34.814093
1055.484049	95549.447898	34.819111
1056.594048	95734.951367	34.824128
1057.528282	95902.127860	34.829146
1057.939332	96085.945822	34.834164
1059.580768	96267.851809	34.839181
1060.337893	96462.382917	34.844199
1061.017805	96649.749713	34.849216
1062.252038	96833.968344	34.854234
1063.219472	97046.586754	34.859252
1064.438288	97226.119953	34.864269
1065.020512	97429.746566	34.869287
1066.297135	97620.535072	34.874304
1067.470036	97811.202963	34.879322
1068.247468	98019.309387	34.884340
1069.731956	98206.896161	34.889357
1070.952351	98409.145989	34.894375
1072.193488	98591.534089	34.899392
1073.386636	98781.756463	34.904410
1074.866857	98970.831048	34.909428
1076.294319	99152.432560	34.914445
1077.475915	99341.838025	34.919463
1078.545786	99518.689897	34.924480
1079.956293	99690.256964	34.929498
1081.161556	99859.731968	34.934516
1081.884430	100026.521398	34.939533
1083.225406	100213.000871	34.944551
1084.322722	100390.607657	34.949568
1085.219022	100548.469906	34.954586
1086.247386	100726.527325	34.959604
1087.799331	100894.723380	34.964621
1089.284044	101057.955160	34.969639
1089.950189	101224.603517	34.974656
1091.442323	101379.111288	34.979674
1092.396076	101531.094371	34.984692
1093.278424	101684.901041	34.989709
1094.465010	101823.873728	34.994727
1094.987125	102001.086879	34.999744
1096.134351	102155.593214	35.004762
1096.747037	102327.557226	35.009780
1097.803033	102484.087832	35.014797
1098.447800	102664.577716	35.019815
1099.630328	102839.926769	35.024832
1100.626654	103033.227315	35.029850
1101.407998	103222.132568	35.034868
1102.479587	103403.867485	35.039885
1103.345381	103591.836925	35.044903
1103.865235	103795.315521	35.049920
1105.082126	103995.285997	35.054938
1105.916382	104202.502238	35.059956
1106.784497	104416.110105	35.064973
1107.913574	104623.369403	35.069991
1109.141585	104835.667164	35.075008
1110.499945	105042.157162	35.080026
1111.526125	105259.101834	35.085044
1112.751009	105474.178882	35.090061
1114.615048	105675.156613	35.095079
1115.802146	105881.972888	35.100096
1117.047059	106077.749645	35.105114
1118.081037	106292.257070	35.110132
1119.302581	106488.167384	35.115149
1120.848582	106690.041495	35.120167
1121.627289	106895.312203	35.125184
1122.963270	107085.976967	35.130202
1124.314504	107290.218448	35.135220
1125.798995	107473.033781	35.140237
1127.572210	107667.113303	35.145255
1128.478240	107867.291225	35.150272
1129.577854	108050.921659	35.155290
1130.764049	108237.464917	35.160308
1131.566969	108430.127632	35.165325
1133.377843	108610.983918	35.170343
1134.440907	108812.814798	35.175360
1135.908209	108974.641875	35.180378
1137.079962	109171.428705	35.185396
1138.075207	109341.405061	35.190413
1139.124433	109525.737890	35.195431
1140.019236	109714.391729	35.200448
1141.430894	109887.583189	35.205466
1142.580221	110072.435135	35.210484
1143.319073	110266.134896	35.215501
1144.772784	110449.406149	35.220519
1146.064146	110635.606425	35.225536
1147.380462	110818.522921	35.230554
1148.252187	111007.873571	35.235572
1148.833125	111192.346009	35.240589
1150.080969	111384.347755	35.245607
1151.296554	111589.049470	35.250624
1152.308847	111776.038516	35.255642
1153.490272	111974.262727	35.260660
1154.577428	112164.294998	35.265677
1155.722052	112360.121121	35.270695
1157.461996	112533.718198	35.275712
1159.245226	112723.461470	35.280730
1160.642060	112895.230133	35.285748
1161.508670	113060.031401	35.290765
1162.902392	113243.850591	35.295783
1163.834732	113421.603177	35.300800
1164.841168	113604.918903	35.305818
1165.734466	113779.804413	35.310836
1167.317610	113960.239625	35.315853
1168.483520	114129.824451	35.320871
1169.237679	114305.357110	35.325888
1170.142644	114471.034504	35.330906
1170.965082	114639.843220	35.335924
1172.266093	114812.412384	35.340941
1173.735700	114979.570105	35.345959
1174.123970	115177.213808	35.350976
1175.584343	115348.277473	35.355994
1176.345362	115544.455572	35.361012
1177.372956	115737.423350	35.366029
1178.580823	115911.623744	35.371047
1179.196650	116119.283494	35.376064
1180.310356	116321.553398	35.381082
1181.472921	116532.001565	35.386100
1182.244000	116747.584337	35.391117
1183.389507	116957.734384	35.396135
1184.781191	117182.922982	35.401152
1185.833673	117399.439605	35.406170
1186.867517	117630.722268	35.411188
1187.700801	117855.007789	35.416205
1188.931545	118072.538907	35.421223
1190.006306	118307.684826	35.426240
1191.021267	118541.055959	35.431258
1192.422503	118790.254534	35.436276
1193.325493	119017.667288	35.441293
1195.191926	119254.260793	35.446311
1196.490527	119491.254538	35.451328
1197.835213	119715.596332	35.456346
1199.381001	119930.111292	35.461364
1200.749207	120151.930875	35.466381
1202.472932	120377.621437	35.471399
1203.808144	120598.258718	35.476416
1205.165094	120816.080854	35.481434
1206.272800	121045.249502	35.486452
1207.254411	121265.266145	35.491469
1208.510582	121481.373818	35.496487
1209.515772	121707.916096	35.501504
1210.537943	121939.006725	35.506522
1212.181244	122162.607976	35.511540
1212.984277	122390.975841	35.516557
1213.843180	122624.937574	35.521575
1214.742288	122863.583452	35.526592
1215.943599	123092.663665	35.531610
1217.406161	123338.190021	35.536628
1218.281982	123587.186796	35.541645
1219.880900	123812.734089	35.546663
1221.010522	124056.002323	35.551680
1222.419776	124306.665493	35.556698
1223.887924	124546.155505	35.561716
1225.672075	124782.832121	35.566733
1227.229960	124988.053676	35.571751
1228.602486	125213.522243	35.576768
1230.346612	125428.626879	35.581786
1231.636480	125649.625795	35.586804
1232.912360	125877.143161	35.591821
1234.264600	126091.113430	35.596839
1235.196218	126300.858358	35.601856
1236.466657	126520.688075	35.606874
1237.432833	126729.644386	35.611892
1239.333053	126950.652839	35.616909
1240.711824	127154.866658	35.621927
1242.291591	127355.436172	35.626944
1242.874302	127567.072772	35.631962
1244.361462	127777.825641	35.636980
1245.485304	127989.755614	35.641997
1246.181330	128192.733301	35.647015
1247.851143	128408.644284	35.652032
1249.000456	128613.983168	35.657050
1250.394162	128808.876373	35.662068
1251.719450	129006.912982	35.667085
1253.131644	129201.374601	35.672103
1254.421391	129377.972441	35.677120
1255.737234	129582.022493	35.682138
1257.111183	129757.315578	35.687156
1258.330808	129942.560420	35.692173
1259.194427	130140.896247	35.697191
1260.545008	130338.151140	35.702208
1261.232873	130543.008754	35.707226
1262.468701	130732.425969	35.712244
1263.279724	130943.274237	35.717261
1264.366903	131145.927221	35.722279
1265.536769	131377.343225	35.727296
1266.412419	131589.642839	35.732314
1267.572754	131815.929622	35.737332
1268.547550	132046.039106	35.742349
1269.936748	132285.867971	35.747367
1270.816262	132530.663761	35.752384
1272.188219	132762.918275	35.757402
1273.627890	132998.446587	35.762420
1275.051543	133248.950986	35.767437
1276.918490	133468.248485	35.772455
1278.355611	133710.361888	35.777472
1279.305399	133950.123861	35.782490
1280.538013	134181.828497	35.787508
1281.454871	134429.662359	35.792525
1282.935358	134670.393840	35.797543
1284.064181	134915.153570	35.802560
1285.421086	135171.769160	35.807578
1285.951889	135414.717438	35.812596
1287.008144	135694.448240	35.817613
1288.466658	135946.070511	35.822631
1289.978914	136211.226198	35.827648
1290.894834	136476.001137	35.832666
1292.498098	136746.521644	35.837684
1293.918686	137009.264629	35.842701
1295.323803	137265.989865	35.847719
1296.709915	137532.254679	35.852736
1298.276800	137784.735021	35.857754
1300.568129	138025.533869	35.862772
1302.322020	138270.176587	35.867789
1303.564170	138511.913676	35.872807
1305.495837	138751.534806	35.877824
1306.527567	138992.739663	35.882842
1308.186888	139227.908166	35.887860
1309.278207	139457.580835	35.892877
1310.340471	139689.275928	35.897895
1311.866716	139913.097628	35.902912
1313.087911	140150.881100	35.907930
1314.823822	140382.342359	35.912948
1315.831739	140621.571930	35.917965
1316.887455	140860.211954	35.922983
1318.713292	141098.244055	35.928000
1319.375208	141342.227656	35.933018
1320.675742	141571.245744	35.938036
1321.640656	141818.656843	35.943053
1323.027181	142075.281886	35.948071
1323.879732	142321.041366	35.953088
1324.575824	142579.001958	35.958106
1326.174501	142833.416309	35.963124
1327.360851	143106.427614	35.968141
1328.395112	143373.772516	35.973159
1329.454200	143642.155172	35.978176
1330.522676	143917.538299	35.983194
1332.116324	144190.439711	35.988212
1333.871619	144454.097079	35.993229
1335.520682	144717.571117	35.998247
1337.106225	144983.150089	36.003264
1338.097864	145230.580689	36.008282
1339.560203	145479.520144	36.013300
1341.020887	145720.624256	36.018317
1342.446176	145966.326691	36.023335
1343.458352	146212.226134	36.028352
1344.774745	146465.597248	36.033370
1346.379154	146709.816595	36.038388
1347.800342	146961.892901	36.043405
1349.015700	147211.481311	36.048423
1350.390685	147463.454610	36.053440
1352.205851	147702.978544	36.058458
1353.794005	147957.405657	36.063476
1355.057805	148196.631100	36.068493
1356.242986	148439.764735	36.073511
1357.767494	148691.049477	36.078528
1358.804295	148942.074374	36.083546
1360.226737	149197.539475	36.088564
1361.311138	149454.216556	36.093581
1362.738032	149706.589745	36.098599
1364.568279	149958.086021	36.103616
1366.061421	150227.054116	36.108634
1367.067626	150474.948941	36.113652
1368.374990	150740.920191	36.118669
1369.528253	150994.171856	36.123687
1371.500644	151245.234618	36.128704
1372.568158	151527.549719	36.133722
1373.626968	151783.447869	36.138740
1374.996204	152052.525618	36.143757
1376.168141	152325.582721	36.148775
1377.981355	152601.211777	36.153792
1378.969744	152870.967282	36.158810
1380.840390	153147.110787	36.163828
1382.073449	153406.555177	36.168845
1383.831281	153672.738535	36.173863
1385.650330	153938.583773	36.178880
1386.934655	154203.999437	36.183898
1388.119657	154468.583505	36.188916
1389.243922	154743.390727	36.193933
1390.621458	155015.430619	36.198951
1391.815802	155293.718432	36.203968
1393.055273	155582.250291	36.208986
1394.396478	155853.655062	36.214004
1395.909059	156138.974398	36.219021
1397.056223	156426.322617	36.224039
1398.719111	156712.293469	36.229056
1400.047733	156991.230579	36.234074
1401.696189	157281.800073	36.239092
1403.687346	157558.893333	36.244109
1404.869044	157825.403221	36.249127
1406.562535	158114.816856	36.254144
1407.420019	158395.338768	36.259162
1408.649295	158679.315009	36.264180
1409.794914	158947.221042	36.269197
1411.282916	159251.139080	36.274215
1412.194631	159546.160316	36.279232
1413.610057	159843.967277	36.284250
1414.944482	160136.271182	36.289268
1416.660902	160430.353371	36.294285
1418.141591	160738.267199	36.299303
1419.568628	161025.043297	36.304320
1421.151713	161326.854836	36.309338
1422.440051	161620.445515	36.314356
1423.826507	161904.100689	36.319373
1424.926639	162209.766730	36.324391
1426.892930	162503.834763	36.329408
1428.293611	162807.323830	36.334426
1430.199475	163099.921603	36.339444
1431.609997	163374.320821	36.344461
1432.624400	163655.981353	36.349479
1434.149079	163926.520843	36.354496
1435.296111	164216.765308	36.359514
1436.871549	164492.121288	36.364532
1438.083316	164767.767710	36.369549
1439.283250	165054.646731	36.374567
1441.106407	165328.101808	36.379584
1442.424778	165614.013269	36.384602
1444.072583	165899.110677	36.389620
1445.479248	166195.199957	36.394637
1446.457655	166483.076704	36.399655
1447.988550	166770.711451	36.404672
1449.033626	167065.623053	36.409690
1451.037969	167343.171714	36.414708
1453.191503	167628.767409	36.419725
1454.903441	167919.475619	36.424743
1456.497406	168194.179186	36.429760
1457.552209	168489.606124	36.434778
1458.800472	168780.181069	36.439796
1460.544285	169067.300394	36.444813
1461.826723	169362.339982	36.449831
1463.284122	169658.456440	36.454848
1465.020702	169957.079091	36.459866
1466.509462	170239.540316	36.464884
1467.778898	170529.957923	36.469901
1468.901513	170843.268429	36.474919
1470.473813	171130.289520	36.479936
1471.729358	171446.031166	36.484954
1473.076927	171749.653534	36.489972
1474.503860	172057.490471	36.494989
1475.594982	172387.402354	36.500007
1477.139842	172702.520737	36.505024
1478.224224	173035.280849	36.510042
1479.459559	173348.741664	36.515060
1480.824895	173687.322670	36.520077
1482.332981	174029.981430	36.525095
1483.654338	174370.503500	36.530112
1484.997509	174713.740159	36.535130
1486.823298	175052.635126	36.540148
1488.280770	175399.461852	36.545165
1489.925620	175741.348574	36.550183
1491.526615	176070.414317	36.555200
1493.873924	176403.546580	36.560218
1495.089871	176738.315471	36.565236
1497.049418	177062.696076	36.570253
1499.008276	177396.686268	36.575271
1500.777503	177701.392887	36.580288
1502.853438	178015.708748	36.585306
1504.374825	178327.554810	36.590324
1506.308218	178635.730042	36.595341
1507.359549	178942.517688	36.600359
1508.688622	179259.084603	36.605376
1510.059428	179561.825064	36.610394
1511.709111	179871.273201	36.615412
1513.237131	180182.786785	36.620429
1514.607680	180512.566950	36.625447
1516.121898	180810.975608	36.630464
1518.261720	181116.859538	36.635482
1519.715571	181420.561668	36.640500
1521.086302	181730.536698	36.645517
1522.607048	182048.154946	36.650535
1523.793787	182346.525052	36.655552
1525.315361	182655.934688	36.660570
1526.655335	182975.149621	36.665588
1528.156401	183284.248961	36.670605
1529.569997	183609.179895	36.675623
1530.937743	183922.899806	36.680640
1532.445282	184240.863202	36.685658
1533.665251	184557.632200	36.690676
1535.205836	184845.117502	36.695693
1536.716795	185165.992419	36.700711
1537.915370	185474.710022	36.705728
1539.030318	185800.160384	36.710746
1540.294104	186127.618916	36.715764
1541.717668	186457.286929	36.720781
1542.705336	186789.758261	36.725799
1543.867495	187122.659586	36.730816
1546.093963	187457.214303	36.735834
1548.600804	187789.299974	36.740852
1549.846838	188113.015521	36.745869
1551.446955	188454.940804	36.750887
1552.936030	188780.980872	36.755904
1554.762094	189103.196742	36.760922
1555.949545	189453.929852	36.765940
1557.479071	189792.510705	36.770957
1558.724891	190148.595245	36.775975
1560.180751	190493.298289	36.780992
1561.586376	190836.335977	36.786010
1563.088484	191204.647192	36.791028
1564.772571	191562.533574	36.796045
1566.040595	191923.639333	36.801063
1567.540171	192283.731340	36.806080
1569.719125	192658.400785	36.811098
1570.784806	193023.659695	36.816116
1572.555766	193384.817594	36.821133
1574.402453	193754.039105	36.826151
1576.251746	194120.837581	36.831168
1577.905692	194475.203854	36.836186
1580.264938	194829.810648	36.841204
1582.988398	195162.497605	36.846221
1585.109254	195485.586879	36.851239
1586.900133	195827.331382	36.856256
1588.485631	196152.874107	36.861274
1589.944766	196478.883754	36.866292
1591.966601	196798.974417	36.871309
1593.159790	197125.437624	36.876327
1594.721700	197447.473954	36.881344
1596.188046	197792.773835	36.886362
1597.034897	198130.852635	36.891380
1598.454494	198464.635807	36.896397
1600.068433	198802.451148	36.901415
1601.513146	199157.397911	36.906432
1603.642398	199496.261216	36.911450
1604.316893	199850.221978	36.916468
1605.788144	200208.546964	36.921485
1607.680798	200569.190855	36.926503
1609.124257	200927.930419	36.931520
1611.022709	201286.723346	36.936538
1612.513545	201636.951980	36.941556
1614.479045	201986.037126	36.946573
1616.135137	202341.917212	36.951591
1617.533449	202691.645757	36.956608
1619.260756	203059.846122	36.961626
1620.545243	203415.094729	36.966644
1622.186289	203763.556553	36.971661
1624.193551	204121.202732	36.976679
1625.833688	204480.765256	36.981696
1627.654057	204824.948785	36.986714
1629.078583	205185.464603	36.991732
1631.098613	205543.813759	36.996749
1632.564268	205890.905090	37.001767
1633.974641	206244.165369	37.006784
1635.540183	206604.753341	37.011802
1636.959389	206970.395436	37.016820
1638.429161	207319.435156	37.021837
1639.835711	207691.761590	37.026855
1641.179978	208038.234953	37.031872
1642.795356	208375.078094	37.036890
1644.266404	208731.437628	37.041908
1646.055809	209088.291952	37.046925
1647.541199	209437.935036	37.051943
1648.674061	209809.161023	37.056960
1650.482858	210173.648267	37.061978
1652.024881	210531.324372	37.066996
1653.737341	210907.208199	37.072013
1655.017936	211281.692284	37.077031
1656.456948	211658.691380	37.082048
1658.419500	212033.218060	37.087066
1660.468308	212406.309838	37.092084
1662.734395	212774.592593	37.097101
1664.813329	213133.587261	37.102119
1666.589095	213505.128917	37.107136
1668.210056	213867.707209	37.112154
1669.834220	214240.800834	37.117172
1671.441930	214616.082868	37.122189
1673.107632	214989.756778	37.127207
1674.378277	215371.929623	37.132224
1676.258332	215737.393004	37.137242
1677.786147	216126.764577	37.142260
1679.378351	216493.675441	37.147277
1681.124147	216884.410825	37.152295
1682.735939	217266.560078	37.157312
1684.833412	217658.586350	37.162330
1686.262369	218049.785245	37.167348
1688.066179	218429.773700	37.172365
1689.804592	218849.141866	37.177383
1691.139817	219282.801717	37.182400
1693.084660	219672.905397	37.187418
1694.282646	220081.853135	37.192436
1695.976856	220476.954081	37.197453
1697.901757	220872.348440	37.202471
1699.410344	221279.242774	37.207488
1701.474679	221671.569065	37.212506
1703.224733	222081.347244	37.217524
1705.186882	222479.255742	37.222541
1707.017938	222874.825240	37.227559
1708.452749	223283.110687	37.232576
1710.120589	223677.084448	37.237594
1711.529132	224092.463556	37.242612
1713.395682	224497.963947	37.247629
1714.816022	224909.483214	37.252647
1716.704075	225326.361927	37.257664
1718.670875	225730.325854	37.262682
1720.642311	226143.866130	37.267700
1722.457033	226555.833542	37.272717
1724.027715	226962.711906	37.277735
1725.546332	227381.766905	37.282752
1727.648419	227793.335052	37.287770
1728.844280	228206.121498	37.292788
1730.353931	228622.413278	37.297805
1732.481840	229033.498353	37.302823
1734.174895	229453.521552	37.307840
1736.225356	229871.276919	37.312858
1738.090592	230285.228700	37.317876
1739.818536	230685.538770	37.322893
1741.819156	231095.787311	37.327911
1743.930261	231501.116289	37.332928
1745.661853	231901.403649	37.337946
1747.681544	232299.536020	37.342964
1749.464286	232706.421299	37.347981
1751.541471	233093.141037	37.352999
1753.435008	233478.012455	37.358016
1755.939173	233846.958531	37.363034
1758.100694	234220.788498	37.368052
1759.464183	234576.208478	37.373069
1761.860326	234908.545877	37.378087
1763.250082	235251.693975	37.383104
1765.178747	235605.625337	37.388122
1766.651502	235950.716975	37.393140
1768.353827	236298.158994	37.398157
1770.014797	236637.175139	37.403175
1771.145951	236994.746841	37.408192
1772.726216	237358.773077	37.413210
1774.142513	237721.912710	37.418228
1775.326109	238102.441137	37.423245
1776.861656	238483.013574	37.428263
1778.371790	238874.361420	37.433280
1780.018076	239266.805140	37.438298
1781.734900	239664.877186	37.443316
1783.110502	240077.714404	37.448333
1784.851625	240475.021846	37.453351
1786.661158	240893.758205	37.458368
1788.150265	241304.038644	37.463386
1789.598330	241733.683230	37.468404
1790.858278	242168.567262	37.473421
1792.630525	242600.369667	37.478439
1794.426003	243047.588295	37.483456
1795.921710	243496.787967	37.488474
1798.232278	243949.562134	37.493492
1800.087025	244403.784326	37.498509
1801.746180	244849.605959	37.503527
1803.620272	245298.644200	37.508544
1806.017995	245745.462495	37.513562
1807.857369	246189.452631	37.518580
1809.437201	246659.448091	37.523597
1811.450147	247106.205003	37.528615
1813.492350	247571.654178	37.533632
1815.625309	248025.835402	37.538650
1817.661485	248476.654611	37.543668
1819.288524	248921.597828	37.548685
1820.943734	249378.628694	37.553703
1822.822402	249835.673813	37.558720
1825.159265	250286.140271	37.563738
1827.096244	250735.250842	37.568756
1829.197573	251190.583742	37.573773
1831.090051	251639.626251	37.578791
1832.338428	252087.251656	37.583808
1834.157784	252552.412575	37.588826
1835.761888	253006.838536	37.593844
1837.179143	253470.974373	37.598861
1838.751504	253950.885591	37.603879
1840.699681	254430.633189	37.608896
1842.614570	254896.338547	37.613914
1844.662284	255377.772123	37.618932
1846.227428	255849.810433	37.623949
1847.998394	256332.052317	37.628967
1850.231179	256813.938374	37.633984
1851.823321	257286.480676	37.639002
1854.398567	257765.896863	37.644020
1856.220217	258235.327468	37.649037
1858.478811	258704.584083	37.654055
1860.305065	259170.787736	37.659072
1862.255242	259647.081342	37.664090
1864.053654	260114.635910	37.669108
1865.865855	260589.428055	37.674125
1867.684980	261051.669731	37.679143
1869.673348	261524.832052	37.684160
1871.418174	261989.041821	37.689178
1873.556791	262451.814391	37.694196
1874.859713	262926.817183	37.699213
1877.018774	263398.197640	37.704231
1878.556387	263875.523556	37.709248
1880.421566	264325.080018	37.714266
1882.572716	264761.455373	37.719284
1884.625504	265216.467267	37.724301
1886.618360	265651.394873	37.729319
1888.598135	266088.407384	37.734336
1890.316432	266526.987063	37.739354
1892.551781	266980.976584	37.744372
1894.026078	267437.479679	37.749389
1895.884459	267873.824888	37.754407
1897.763453	268328.481827	37.759424
1899.468463	268779.991735	37.764442
1901.768944	269226.626721	37.769460
1903.292564	269686.320003	37.774477
1905.073969	270158.290408	37.779495
1907.479333	270610.317174	37.784512
1909.082861	271071.799039	37.789530
1910.955199	271535.725195	37.794548
1912.688087	272012.857807	37.799565
1914.569905	272483.741341	37.804583
1916.555285	272955.800894	37.809600
1917.841603	273444.766631	37.814618
1919.750258	273920.698482	37.819636
1921.684537	274421.189494	37.824653
1923.489574	274906.103833	37.829671
1925.444723	275408.520048	37.834688
1926.952302	275914.946756	37.839706
1928.950023	276413.822894	37.844724
1930.818506	276925.979351	37.849741
1933.137919	277434.706836	37.854759
1935.507709	277939.462055	37.859776
1937.131579	278448.378594	37.864794
1939.187626	278949.271445	37.869812
1940.948085	279468.653851	37.874829
1942.934176	279977.557327	37.879847
1944.894531	280487.632204	37.884864
1946.935726	281017.454865	37.889882
1948.764374	281534.534165	37.894900
1950.508469	282074.589031	37.899917
1952.179925	282585.366307	37.904935
1954.127760	283127.238444	37.909952
1955.878785	283658.676073	37.914970
1958.183783	284184.558923	37.919988
1960.550199	284732.300303	37.925005
1962.610565	285258.601143	37.930023
1965.293637	285789.267597	37.935040
1966.828673	286314.483379	37.940058
1969.070808	286842.679053	37.945076
1970.777740	287369.996247	37.950093
1972.973860	287902.589983	37.955111
1974.909853	288440.838311	37.960128
1976.809400	288974.213683	37.965146
1978.470066	289508.134531	37.970164
1980.578893	290042.817193	37.975181
1982.041994	290592.920925	37.980199
1984.465632	291128.156547	37.985216
1986.323884	291660.816571	37.990234
1988.453294	292204.351305	37.995252
1990.371540	292762.650425	38.000269
1992.202174	293292.183739	38.005287
1993.840884	293842.929629	38.010304
1996.222820	294393.016398	38.015322
1998.407982	294935.818149	38.020340
2000.177107	295486.102745	38.025357
2002.006200	296036.450879	38.030375
2004.504787	296584.602631	38.035392
2006.217869	297131.256209	38.040410
2008.377433	297667.902167	38.045428
2010.287963	298216.422311	38.050445
2012.311241	298743.865665	38.055463
2014.205626	299268.965615	38.060480
2015.904962	299790.082246	38.065498
2018.270696	300312.203261	38.070516
2019.788538	300849.497446	38.075533
2021.780181	301384.500571	38.080551
2024.036364	301907.342277	38.085568
2026.195703	302447.822900	38.090586
2028.221283	302973.388994	38.095604
2030.584955	303510.934297	38.100621
2032.538418	304042.372934	38.105639
2034.518474	304576.292914	38.110656
2036.434000	305117.001277	38.115674
2038.815951	305646.632390	38.120692
2041.234174	306193.955488	38.125709
2043.106140	306716.071044	38.130727
2044.991328	307258.624967	38.135744
2046.895361	307814.632047	38.140762
2049.262886	308346.255007	38.145780
2051.418133	308901.527486	38.150797
2053.165831	309447.340449	38.155815
2055.148333	310003.675189	38.160832
2057.204026	310552.223063	38.165850
2059.422050	311096.829434	38.170868
2062.119236	311643.739720	38.175885
2064.167468	312200.200345	38.180903
2066.336775	312737.591190	38.185920
2068.413468	313284.440140	38.190938
2070.298664	313836.801885	38.195956
2072.209290	314405.077126	38.200973
2074.314814	314960.441192	38.205991
2076.295580	315521.814486	38.211008
2077.918696	316089.717870	38.216026
2080.429628	316652.670411	38.221044
2082.832139	317218.683532	38.226061
2085.224725	317771.946694	38.231079
2087.684759	318315.748336	38.236096
2089.952233	318878.926298	38.241114
2092.198625	319428.975497	38.246132
2094.530515	319993.555438	38.251149
2096.568925	320549.571515	38.256167
2098.727267	321102.008277	38.261184
2100.914656	321654.080089	38.266202
2102.895940	322194.349241	38.271220
2104.764296	322746.236041	38.276237
2106.854250	323293.739613	38.281255
2108.891993	323856.862008	38.286272
2110.424325	324414.781959	38.291290
2112.369261	324977.960386	38.296308
2115.011618	325546.908493	38.301325
2117.447853	326116.824838	38.306343
2120.068349	326661.468690	38.311360
2122.089896	327221.008426	38.316378
2124.667828	327760.673132	38.321396
2127.152884	328313.067801	38.326413
2129.238674	328853.184825	38.331431
2131.149579	329384.922448	38.336448
2133.341699	329934.481422	38.341466
2135.633263	330480.058236	38.346484
2137.653909	331020.318020	38.351501
2139.565531	331568.105180	38.356519
2141.677831	332108.313940	38.361536
2143.455261	332661.748404	38.366554
2145.282521	333210.701119	38.371572
2147.268228	333771.654954	38.376589
2149.346071	334342.691176	38.381607
2151.724413	334889.225585	38.386624
2154.096747	335445.731714	38.391642
2156.000335	335977.457997	38.396660
2157.880852	336509.131977	38.401677
2159.571993	337049.157956	38.406695
2161.642074	337593.151625	38.411712
2163.340062	338146.136253	38.416730
2165.182569	338693.481258	38.421748
2167.454423	339252.603206	38.426765
2169.387137	339819.313854	38.431783
2171.408481	340392.958258	38.436800
2173.092110	340959.976467	38.441818
2175.187087	341546.362658	38.446836
2177.512301	342130.292476	38.451853
2179.369249	342722.770245	38.456871
2181.579592	343319.877749	38.461888
2183.229749	343922.222917	38.466906
2185.545714	344527.724311	38.471924
2187.719274	345151.236045	38.476941
2189.702876	345763.908470	38.481959
2191.850746	346391.874836	38.486976
2194.507085	347020.103821	38.491994
2196.840074	347651.397873	38.497012
2199.228206	348268.995163	38.502029
2201.228264	348902.636490	38.507047
2203.893432	349522.607121	38.512064
2206.102782	350155.917005	38.517082
2208.295995	350792.646450	38.522100
2210.473009	351418.914273	38.527117
2212.550418	352063.257531	38.532135
2215.159762	352690.019242	38.537152
2217.116310	353328.146707	38.542170
2219.328467	353975.712672	38.547188
2221.928675	354608.512622	38.552205
2224.355398	355264.853871	38.557223
2226.668636	355905.522625	38.562240
2228.692507	356561.884977	38.567258
2230.792075	357212.921467	38.572276
2233.110284	357853.660922	38.577293
2234.626245	358524.919288	38.582311
2236.875997	359192.645271	38.587328
2239.270899	359845.493903	38.592346
2241.466886	360521.757024	38.597364
2243.417125	361189.677101	38.602381
2245.445853	361867.441974	38.607399
2247.888573	362555.705854	38.612416
2249.630812	363233.722971	38.617434
2251.811862	363936.035119	38.622452
2254.010903	364633.689129	38.627469
2256.046998	365343.052088	38.632487
2257.908349	366047.484155	38.637504
2259.796259	366763.922704	38.642522
2261.923654	367487.588168	38.647540
2264.991585	368208.978525	38.652557
2267.349045	368923.370187	38.657575
2270.137542	369637.169362	38.662592
2272.590120	370350.223980	38.667610
2274.515036	371059.496698	38.672628
2277.402795	371764.233573	38.677645
2279.229762	372488.991570	38.682663
2282.085111	373194.897786	38.687680
2284.944915	373881.615552	38.692698
2287.178999	374594.748859	38.697716
2290.330876	375273.452974	38.702733
2292.750802	375964.843920	38.707751
2295.626993	376638.621763	38.712768
2297.975499	377317.850047	38.717786
2301.057196	377979.090718	38.722804
2303.801254	378622.141669	38.727821
2306.285933	379261.292878	38.732839
2308.346019	379887.367041	38.737856
2310.524809	380490.055937	38.742874
2312.409794	381114.285089	38.747892
2314.543856	381714.271443	38.752909
2317.300082	382331.690087	38.757927
2319.780159	382948.838605	38.762944
2322.043095	383560.205194	38.767962
2324.211258	384173.021199	38.772980
2326.029336	384788.647156	38.777997
2328.226627	385423.720663	38.783015
2330.230937	386053.971164	38.788032
2332.205500	386689.563501	38.793050
2333.922860	387345.746042	38.798068
2336.158947	387986.998575	38.803085
2337.889735	388653.723174	38.808103
2339.639848	389324.435707	38.813120
2342.012793	390004.511449	38.818138
2344.495064	390687.342558	38.823156
2346.849239	391375.933858	38.828173
2349.071368	392078.042013	38.833191
2351.804818	392766.995442	38.838208
2354.005299	393472.192715	38.843226
2355.845834	394177.661213	38.848244
2358.369288	394871.822651	38.853261
2360.705877	395604.979497	38.858279
2363.077957	396324.857262	38.863296
2365.338666	397055.937854	38.868314
2367.090205	397788.706512	38.873332
2369.342754	398533.310152	38.878349
2371.540877	399290.245185	38.883367
2373.736926	400041.484327	38.888384
2375.890314	400800.566450	38.893402
2378.096642	401575.811783	38.898420
2380.728188	402346.708619	38.903437
2383.040089	403123.059778	38.908455
2386.026603	403899.353839	38.913472
2388.458051	404663.100428	38.918490
2390.853897	405453.359046	38.923508
2393.791361	406218.093864	38.928525
2396.575732	406986.557008	38.933543
2399.246013	407748.734604	38.938560
2402.099668	408510.581851	38.943578
2404.529747	409269.488543	38.948596
2406.872007	410025.956541	38.953613
2409.606944	410784.795342	38.958631
2412.143864	411548.660807	38.963648
2415.031847	412302.668859	38.968666
2417.656962	413049.302803	38.973684
2420.404262	413795.642035	38.978701
2422.947635	414534.750015	38.983719
2425.282150	415273.111784	38.988736
2427.767410	416001.069120	38.993754
2430.343147	416740.539389	38.998772
2433.280635	417472.381675	39.003789
2435.950908	418208.729599	39.008807
2438.509652	418921.270698	39.013824
2441.581050	419626.363302	39.018842
2444.904819	420318.910667	39.023860
2447.882151	421006.052187	39.028877
2450.806736	421700.551829	39.033895
2453.178127	422380.210247	39.038912
2455.555640	423051.949417	39.043930
2457.372025	423730.042175	39.048948
2459.832428	424399.452196	39.053965
2463.203740	425056.692797	39.058983
2465.294347	425716.102349	39.064000
2467.491447	426393.197383	39.069018
2469.727575	427057.660106	39.074036
2471.910853	427705.152625	39.079053
2474.225070	428347.543254	39.084071
2475.818468	429003.958072	39.089088
2477.979125	429653.831568	39.094106
2479.660447	430336.519776	39.099124
2481.527425	431003.211689	39.104141
2483.847999	431693.196167	39.109159
2485.530181	432401.893667	39.114176
2487.459967	433102.227444	39.119194
2489.345543	433838.838798	39.124212
2491.454086	434593.104658	39.129229
2493.708830	435329.202433	39.134247
2495.793883	436091.976460	39.139264
2498.263285	436852.738249	39.144282
2500.479591	437634.467840	39.149300
2502.798097	438417.772887	39.154317
2505.007049	439214.326984	39.159335
2507.126324	440016.180828	39.164352
2509.515183	440824.842852	39.169370
2512.240569	441662.412452	39.174388
2514.715851	442484.509322	39.179405
2517.501566	443315.175739	39.184423
2520.164655	444145.881568	39.189440
2522.822977	444983.082722	39.194458
2525.296686	445824.379828	39.199476
2527.995629	446664.139915	39.204493
2530.653239	447505.088106	39.209511
2533.466157	448361.911060	39.214528
2536.130594	449204.662808	39.219546
2538.668803	450055.798012	39.224564
2541.029577	450923.921961	39.229581
2543.477387	451773.738377	39.234599
2546.097695	452639.624295	39.239616
2548.708989	453507.751394	39.244634
2551.110171	454390.389951	39.249652
2553.681833	455252.331743	39.254669
2556.330333	456129.090409	39.259687
2559.038060	457009.947762	39.264704
2562.395895	457874.379346	39.269722
2566.075172	458727.497196	39.274740
2568.911510	459577.179659	39.279757
2571.693075	460425.571462	39.284775
2573.926330	461286.857960	39.289792
2576.340862	462138.321380	39.294810
2578.855731	463011.921539	39.299828
2581.732921	463855.349353	39.304845
2584.779484	464704.120984	39.309863
2587.237496	465560.786927	39.314880
2589.685605	466410.341645	39.319898
2592.206849	467268.033854	39.324916
2594.822497	468115.414202	39.329933
2598.108929	468962.545216	39.334951
2601.914590	469784.339070	39.339968
2605.123361	470602.962661	39.344986
2607.946774	471430.557638	39.350004
2610.520966	472248.558524	39.355021
2613.139134	473049.895618	39.360039
2615.687469	473855.554680	39.365056
2618.478135	474669.928740	39.370074
2620.805831	475474.241196	39.375092
2623.009028	476285.661573	39.380109
2625.882124	477081.479773	39.385127
2627.955432	477912.447803	39.390144
2630.629294	478720.804358	39.395162
2632.773020	479540.778016	39.400180
2635.312674	480366.810325	39.405197
2638.092211	481191.704948	39.410215
2639.908490	482013.388698	39.415232
2642.376699	482806.448971	39.420250
2644.987921	483617.324404	39.425268
2647.419865	484414.762792	39.430285
2649.702158	485202.143495	39.435303
2652.622885	486016.746129	39.440320
2654.995446	486821.255152	39.445338
2657.690672	487631.933577	39.450356
2660.424901	488449.382598	39.455373
2663.326937	489262.677245	39.460391
2665.412728	490087.980577	39.465408
2668.105467	490922.027049	39.470426
2670.428784	491756.851521	39.475444
2672.760988	492598.043235	39.480461
2675.608935	493459.343995	39.485479
2678.206093	494311.156460	39.490496
2680.738249	495168.033396	39.495514
2683.427641	496032.258031	39.500532
2685.945539	496909.433233	39.505549
2688.622906	497785.880619	39.510567
2691.461799	498680.214766	39.515584
2694.162081	499560.197887	39.520602
2696.843517	500448.561494	39.525620
2699.359499	501336.652811	39.530637
2702.173639	502232.212620	39.535655
2704.718070	503143.806310	39.540672
2707.358485	504053.971928	39.545690
2709.674143	504970.847596	39.550708
2712.001350	505900.276073	39.555725
2715.067871	506823.932194	39.560743
2717.674134	507765.258480	39.565760
2720.013467	508710.254351	39.570778
2722.577083	509656.216181	39.575796
2725.340970	510619.278827	39.580813
2728.116394	511573.056826	39.585831
2730.465535	512537.533712	39.590848
2733.860970	513501.677832	39.595866
2736.593844	514463.302226	39.600884
2739.635283	515438.473607	39.605901
2742.950653	516390.207412	39.610919
2745.784520	517361.866178	39.615936
2748.540079	518322.896040	39.620954
2751.518198	519291.638523	39.625972
2754.304167	520260.603675	39.630989
2757.033154	521214.504935	39.636007
2760.126826	522188.586486	39.641024
2763.237864	523140.843094	39.646042
2766.195615	524102.685183	39.651060
2768.933939	525072.812192	39.656077
2772.068774	526011.537455	39.661095
2775.092904	526962.609978	39.666112
2777.448676	527907.992148	39.671130
2780.639336	528872.863087	39.676148
2783.529359	529826.191426	39.681165
2786.378346	530766.224534	39.686183
2789.291106	531719.023865	39.691200
2792.225565	532659.475325	39.696218
2794.810066	533603.548158	39.701236
2797.493578	534557.257199	39.706253
2800.508526	535478.689340	39.711271
2803.980345	536424.646050	39.716288
2806.619942	537350.952406	39.721306
2809.822059	538283.949099	39.726324
2812.711881	539222.169254	39.731341
2815.520104	540154.857183	39.736359
2818.708756	541083.597484	39.741376
2821.492823	542002.634938	39.746394
2824.562238	542918.748390	39.751412
2826.960695	543819.823667	39.756429
2829.975780	544701.174229	39.761447
2832.426001	545577.986023	39.766464
2834.766754	546468.740899	39.771482
2837.391254	547345.060295	39.776500
2839.276339	548249.453613	39.781517
2841.900335	549152.307816	39.786535
2844.629149	550065.944824	39.791552
2846.896212	550990.506272	39.796570
2849.830099	551920.625383	39.801588
2852.128537	552851.489698	39.806605
2855.323139	553799.632895	39.811623
2858.303900	554749.051609	39.816640
2860.460891	555697.836063	39.821658
2863.432873	556643.051791	39.826676
2866.475176	557610.800399	39.831693
2869.893477	558574.698485	39.836711
2872.284813	559545.127208	39.841728
2875.140404	560508.575840	39.846746
2878.142350	561487.903886	39.851764
2880.723546	562473.507184	39.856781
2884.070901	563470.160021	39.861799
2886.525571	564447.097253	39.866816
2889.617465	565440.628378	39.871834
2892.786343	566449.385782	39.876852
2895.451276	567451.520121	39.881869
2898.447061	568455.329162	39.886887
2901.624545	569468.567971	39.891904
2904.433600	570477.370042	39.896922
2907.844163	571474.247415	39.901940
2910.311454	572503.675413	39.906957
2913.002771	573523.999411	39.911975
2916.069485	574564.251455	39.916992
2918.551332	575590.213586	39.922010
2921.300851	576619.509402	39.927028
2924.232141	577673.574218	39.932045
2927.088059	578720.539122	39.937063
2929.930477	579765.010146	39.942080
2932.910569	580838.109712	39.947098
2935.611237	581897.420336	39.952116
2937.973534	582981.919725	39.957133
2941.338120	584049.609923	39.962151
2944.323325	585129.001763	39.967168
2947.100226	586228.686586	39.972186
2950.178989	587313.433286	39.977204
2952.573158	588412.080270	39.982221
2955.919476	589495.032183	39.987239
2959.403615	590597.859601	39.992256
2962.066227	591693.454785	39.997274
2965.322373	592783.038451	40.002292
2968.125156	593901.355454	40.007309
2970.959989	595003.029106	40.012327
2973.974056	596112.634844	40.017344
2977.506287	597217.842459	40.022362
2981.802778	598283.854356	40.027380
2985.547259	599358.072794	40.032397
2989.246590	600416.425891	40.037415
2992.231671	601479.006064	40.042432
2995.610480	602538.919908	40.047450
2998.595935	603588.488584	40.052468
3001.673472	604633.090413	40.057485
3004.880640	605667.314703	40.062503
3008.259552	606698.814131	40.067520
3011.143937	607736.806972	40.072538
3014.149139	608762.675527	40.077556
3016.608218	609802.199981	40.082573
3019.551147	610825.339068	40.087591
3022.501992	611878.647667	40.092608
3024.601074	612908.788957	40.097626
3027.816838	613906.641004	40.102644
3030.431555	614916.205007	40.107661
3033.041242	615924.377551	40.112679
3035.978179	616932.153793	40.117696
3038.594182	617960.489126	40.122714
3041.795239	618960.835963	40.127732
3044.982383	619988.386337	40.132749
3048.065937	621008.309599	40.137767
3051.303262	622041.755463	40.142784
3053.967598	623076.596655	40.147802
3056.937328	624107.190769	40.152820
3059.567863	625158.177120	40.157837
3062.369739	626216.525874	40.162855
3065.267391	627281.897332	40.167872
3068.306998	628348.986920	40.172890
3071.200831	629424.733480	40.177908
3073.998675	630525.805019	40.182925
3076.540851	631621.211592	40.187943
3079.521954	632730.561035	40.192960
3082.337798	633848.506944	40.197978
3085.379539	634962.202844	40.202996
3088.239813	636104.009624	40.208013
3091.391918	637249.235896	40.213031
3094.171072	638396.692610	40.218048
3097.188565	639563.640818	40.223066
3099.957141	640723.912513	40.228084
3103.402637	641906.637832	40.233101
3106.179863	643090.084938	40.238119
3109.226981	644287.164331	40.243136
3112.134815	645491.306239	40.248154
3115.606550	646683.843617	40.253172
3119.172322	647876.224401	40.258189
3121.979641	649078.309427	40.263207
3125.560141	650293.978352	40.268224
3128.558026	651505.907718	40.273242
3132.324494	652704.158217	40.278260
3135.511306	653912.523744	40.283277
3138.842307	655127.791756	40.288295
3142.411714	656332.360220	40.293312
3146.292098	657530.553603	40.298330
3150.035979	658713.234866	40.303348
3153.594896	659889.778300	40.308365
3156.695190	661070.088767	40.313383
3160.153279	662254.527260	40.318400
3163.379510	663432.487646	40.323418
3166.518553	664611.662087	40.328436
3169.925489	665790.448306	40.333453
3172.773900	666955.399038	40.338471
3175.926533	668133.838575	40.343488
3179.116012	669318.990657	40.348506
3182.195569	670492.970841	40.353524
3185.952603	671677.087089	40.358541
3188.673888	672868.734232	40.363559
3191.702376	674025.823263	40.368576
3195.294810	675215.884403	40.373594
3198.215871	676403.966149	40.378612
3201.508348	677581.844925	40.383629
3204.080160	678767.992107	40.388647
3207.093783	679954.013405	40.393664
3210.773601	681148.565473	40.398682
3214.165965	682325.822180	40.403700
3218.035736	683506.673051	40.408717
3220.792736	684692.421974	40.413735
3224.145993	685878.265413	40.418752
3226.708006	687076.397592	40.423770
3229.748056	688267.093882	40.428788
3233.008342	689458.539592	40.433805
3235.804577	690656.901800	40.438823
3239.011500	691816.578272	40.443840
3241.936358	692984.833686	40.448858
3245.100266	694138.360675	40.453876
3249.289248	695284.475064	40.458893
3252.138015	696436.316677	40.463911
3255.426327	697594.282938	40.468928
3258.423408	698758.739669	40.473946
3261.306443	699939.966612	40.478964
3264.938047	701095.678920	40.483981
3268.244959	702265.962754	40.488999
3271.776481	703447.053732	40.494016
3274.221304	704635.249223	40.499034
3277.272249	705822.537213	40.504052
3280.638838	707036.260307	40.509069
3283.711190	708238.518345	40.514087
3287.287366	709440.425389	40.519104
3290.116491	710658.131885	40.524122
3293.801502	711871.413620	40.529140
3297.045247	713105.979607	40.534157
3300.240961	714338.938183	40.539175
3303.397988	715563.607187	40.544192
3306.592933	716820.748344	40.549210
3310.120851	718069.384219	40.554228
3313.277973	719327.144896	40.559245
3316.433454	720589.464030	40.564263
3319.572198	721838.539479	40.569280
3322.827211	723128.938991	40.574298
3326.378603	724398.325455	40.579316
3329.977283	725677.888090	40.584333
3333.669565	726951.157255	40.589351
3336.945936	728227.311177	40.594368
3340.227973	729512.256056	40.599386
3342.970908	730817.783929	40.604404
3346.392120	732106.247045	40.609421
3349.650203	733426.233677	40.614439
3353.167006	734731.890374	40.619456
3356.291087	736050.777344	40.624474
3359.920351	737367.932298	40.629492
3363.723503	738679.560993	40.634509
3367.378684	739991.935390	40.639527
3370.544311	741312.855865	40.644544
3374.017270	742629.164517	40.649562
3377.498816	743951.810816	40.654580
3381.226038	745257.183232	40.659597
3384.896793	746576.003063	40.664615
3388.648388	747876.990389	40.669632
3391.819133	749197.470402	40.674650
3395.127814	750511.248245	40.679668
3398.411062	751837.320520	40.684685
3401.458752	753155.470594	40.689703
3404.996271	754485.921269	40.694720
3408.209640	755803.983351	40.699738
3411.658131	757145.557750	40.704756
3415.542183	758455.075790	40.709773
3419.282365	759774.037755	40.714791
3423.100797	761093.445981	40.719808
3426.403201	762418.612522	40.724826
3429.792465	763740.924531	40.729844
3433.610696	765049.703538	40.734861
3436.929765	766363.056506	40.739879
3440.931860	767662.545912	40.744896
3444.631380	768973.212703	40.749914
3447.645632	770281.844490	40.754932
3451.723104	771580.290976	40.759949
3454.920126	772869.860495	40.764967
3458.088488	774170.407615	40.769984
3461.433116	775470.743986	40.775002
3464.633533	776766.029417	40.780007
3467.485374	778014.530650	40.785012
3470.425841	779209.508315	40.790016
3474.688200	780331.595477	40.795021
3478.065813	781385.322542	40.800026
3480.989342	782381.321862	40.805031
3484.189477	783303.167818	40.810036
3487.020298	784176.616294	40.815040
3488.936348	784958.750460	40.820045
3491.277539	785693.431448	40.825050
3493.512875	786369.749375	40.830055
3495.863717	786978.885043	40.835060
3497.676709	787530.351831	40.840064
3499.699120	788031.706979	40.845069
3501.438490	788479.897032	40.850074
3503.196195	788883.678983	40.855079
3504.761587	789211.448090	40.860084
3505.928784	789515.484363	40.865088
3507.503783	789767.010425	40.870093
3509.294425	789960.953434	40.875098
3510.270574	790139.056807	40.880103
3511.676488	790265.346477	40.885108
3512.313762	790361.494672	40.890112
3513.128852	790415.554260	40.895117
3514.354007	790426.750832	40.900122
3515.183654	790443.417379	40.905127
3515.741917	790401.267261	40.910132
3516.213444	790361.194837	40.915136
3516.685052	790289.971229	40.920141
3517.643998	790199.258186	40.925146
3517.778499	790091.384561	40.930151
3518.690270	789943.138173	40.935156
3518.554146	789807.297084	40.940160
3519.603016	789639.464967	40.945165
3519.923406	789451.798491	40.950170
3519.847658	789248.319885	40.955175
3520.710448	789037.112366	40.960180
3520.493206	788825.585599	40.965184
3520.740669	788591.958425	40.970189
3520.820745	788354.566874	40.975194
3520.646306	788104.971305	40.980199
3521.144319	787846.113767	40.985204
3521.021866	787594.181584	40.990208
3521.289900	787321.875120	40.995213
3521.290057	787051.077211	41.000218
3521.117267	786771.547396	41.005223
3521.391112	786483.575550	41.010228
3521.679065	786204.930604	41.015232
3521.539457	785915.627627	41.020237
3521.745158	785606.785985	41.025242
3521.726961	785306.965845	41.030247
3521.786077	785001.711601	41.035252
3522.030436	784685.251518	41.040256
3521.805789	784371.608759	41.045261
3521.880866	784052.296557	41.050266
3521.843943	783744.594959	41.055271
3521.946784	783429.922504	41.060276
3521.713691	783103.930375	41.065280
3521.422213	782774.293355	41.070285
3521.802634	782453.531618	41.075290
3521.369228	782132.840890	41.080295
3521.472605	781792.862102	41.085300
3521.299269	781479.871760	41.090304
3520.984177	781152.378182	41.095309
3520.850254	780830.300913	41.100314
3520.936608	780517.422729	41.105319
3520.786428	780191.235965	41.110324
3520.635378	779863.755291	41.115328
3520.537148	779550.964232	41.120333
3520.444559	779225.708611	41.125338
3520.030465	778920.520884	41.130343
3520.302051	778590.895163	41.135348
3520.248932	778280.305716	41.140352
3520.368954	777954.958022	41.145357
3520.293994	777640.555016	41.150362
3520.010232	777319.823174	41.155367
3519.649009	776988.752723	41.160372
3519.583046	776681.296785	41.165376
3519.338363	776366.029952	41.170381
3519.148452	776059.552880	41.175386
3519.024271	775760.289408	41.180391
3519.320325	775436.375688	41.185396
3519.046194	775132.089242	41.190400
3518.595816	774832.250843	41.195405
3519.265734	774527.487825	41.200410
3518.807031	774223.932768	41.205415
3519.090223	773916.893824	41.210420
3518.568352	773613.028447	41.215424
3518.367650	773318.011650	41.220429
3518.562170	773015.332906	41.225434
3517.957143	772708.784264	41.230439
3518.208253	772414.099824	41.235444
3518.173139	772116.741708	41.240448
3517.924954	771830.638052	41.245453
3518.012316	771525.058691	41.250458
3517.394700	771231.061658	41.255463
3517.279288	770941.058980	41.260468
3516.700436	770660.186753	41.265472
3517.345030	770381.368070	41.270477
3517.290809	770103.491980	41.275482
3517.198962	769837.880692	41.280487
3516.924601	769538.536669	41.285492
3516.975013	769252.037471	41.290496
3516.693062	768985.096554	41.295501
3516.720095	768707.893891	41.300506
3515.940172	768426.970198	41.305511
3516.147709	768156.173118	41.310516
3515.899349	767895.495869	41.315520
3515.988945	767627.360472	41.320525
3515.995606	767358.489779	41.325530
3516.020278	767099.563250	41.330535
3515.518207	766839.876791	41.335540
3515.647185	766583.921988	41.340544
3515.377174	766321.763699	41.345549
3515.343311	766054.528766	41.350554
3515.025295	765812.523459	41.355559
3515.170812	765551.107550	41.360564
3515.196717	765308.930506	41.365568
3514.983010	765049.972303	41.370573
3515.077293	764800.864847	41.375578
3514.757039	764547.231961	41.380583
3514.828957	764302.943845	41.385588
3514.703135	764050.938570	41.390592
3514.453299	763818.966389	41.395597
3514.307795	763562.164604	41.400602
3513.910748	763322.015173	41.405607
3514.183552	763073.166080	41.410612
3514.312093	762852.493936	41.415616
3513.741626	762619.058126	41.420621
3513.886674	762384.806321	41.425626
3513.476279	762163.907123	41.430631
3513.297401	761931.223783	41.435636
3513.367945	761705.348466	41.440640
3513.101514	761484.158926	41.445645
3513.148377	761262.812471	41.450650
3513.151230	761061.445866	41.455655
3513.129567	760829.294549	41.460660
3512.738025	760610.862728	41.465664
3512.405840	760398.187018	41.470669
3513.059226	760179.816751	41.475674
3512.615637	759972.969232	41.480679
3512.525557	759760.877004	41.485684
3512.387283	759547.997352	41.490688
3512.357322	759335.932641	41.495693
3512.378117	759131.551209	41.500698
3512.328482	758919.576802	41.505703
3512.185358	758716.987714	41.510708
3512.062724	758503.928153	41.515712
3511.562859	758309.529503	41.520717
3511.914789	758108.322847	41.525722
3511.781593	757915.185977	41.530727
3511.749979	757703.668201	41.535732
3511.625316	757510.667717	41.540736
3511.037109	757316.554418	41.545741
3511.418085	757123.263140	41.550746
3511.016053	756939.030119	41.555751
3511.220640	756751.730862	41.560756
3511.110628	756563.639877	41.565760
3511.006409	756377.221587	41.570765
3510.845387	756189.672796	41.575770
3510.752540	756015.090802	41.580775
3510.683759	755830.825329	41.585780
3510.746763	755647.076665	41.590784
3510.185673	755479.816642	41.595789
3510.421595	755294.352449	41.600794
3510.191315	755131.078341	41.605799
3510.207724	754951.961418	41.610804
3510.280100	754784.384035	41.615808
3509.679934	754619.185277	41.620813
3510.016781	754444.743330	41.625818
3509.731005	754286.200282	41.630823
3509.872379	754114.992509	41.635828
3509.642845	753938.509492	41.640832
3509.439515	753786.657783	41.645837
3509.688964	753624.457401	41.650842
3509.590728	753472.088319	41.655847
3509.437425	753308.120758	41.660852
3509.281713	753147.804382	41.665856
3509.344004	752990.609163	41.670861
3509.346600	752837.321950	41.675866
3509.140891	752692.017114	41.680871
3509.184886	752524.987775	41.685876
3509.198146	752375.788668	41.690880
3509.080042	752227.398592	41.695885
3509.141567	752078.877197	41.700890
3508.670227	751917.056309	41.705895
3508.577511	751766.776353	41.710900
3508.698188	751622.681594	41.715904
3508.499348	751481.995665	41.720909
3508.668813	751335.170875	41.725914
3508.491940	751190.919662	41.730919
3508.584565	751049.486165	41.735924
3508.205339	750911.388228	41.740928
3508.304306	750777.654562	41.745933
3508.360710	750636.565284	41.750938
3508.194770	750495.016188	41.755943
3508.467024	750354.429490	41.760948
3508.495565	750224.205307	41.765952
3508.264159	750087.797276	41.770957
3508.504656	749945.034725	41.775962
3508.300344	749803.825161	41.780967
3508.046737	749670.031835	41.785972
3508.079222	749529.914453	41.790976
3507.764535	749399.189677	41.795981
3508.048499	749265.349942	41.800986
3507.668017	749140.264072	41.805991
3507.669366	749002.909159	41.810996
3507.462616	748887.276957	41.816000
3507.234560	748773.227679	41.821005
3507.619858	748642.275665	41.826010
3507.424331	748524.659776	41.831015
3507.117659	748400.735683	41.836020
3507.446399	748277.099913	41.841024
3506.950353	748166.446124	41.846029
3507.099737	748045.801160	41.851034
3506.905238	747938.059173	41.856039
3506.885590	747809.334349	41.861044
3507.051313	747694.957111	41.866048
3506.804251	747582.277193	41.871053
3507.214359	747471.859126	41.876058
3506.881468	747366.108836	41.881063
3506.736338	747249.206641	41.886068
3506.619141	747134.719683	41.891072
3506.735340	747030.719188	41.896077
3506.548566	746914.214225	41.901082
3506.579412	746816.748673	41.906087
3506.509787	746704.965788	41.911092
3506.618949	746593.991964	41.916096
3506.506983	746494.766735	41.921101
3506.501019	746378.619300	41.926106
3506.636072	746280.339033	41.931111
3506.142222	746172.572712	41.936116
3506.391273	746066.807505	41.941120
3506.406618	745967.356835	41.946125
3506.532811	745858.989447	41.951130
3506.374595	745763.222578	41.956135
3506.155920	745656.194533	41.961140
3506.410814	745559.862610	41.966144
3505.958078	745453.809657	41.971149
3506.107956	745348.743179	41.976154
3506.019294	745249.152282	41.981159
3505.769744	745156.902794	41.986164
3505.898910	745060.684381	41.991168
3505.550716	744975.518062	41.996173
3505.705529	744881.913226	42.001178
3505.382214	744792.687160	42.006183
3505.431134	744698.207798	42.011188
3505.880431	744605.144228	42.016192
3505.262453	744513.689606	42.021197
3505.826794	744416.452076	42.026202
3505.547561	744341.748257	42.031207
3505.355227	744263.716978	42.036212
3505.208125	744170.054675	42.041216
3504.580548	744084.331582	42.046221
3505.073529	743998.224608	42.051226
3505.042306	743935.044954	42.056231
3505.204096	743841.970423	42.061236
3505.522062	743759.795625	42.066240
3505.195647	743680.495228	42.071245
3505.183676	743594.022301	42.076250
3504.968972	743519.843875	42.081255
3504.956787	743445.779613	42.086260
3505.218866	743357.824933	42.091264
3505.068507	743281.507522	42.096269
3505.022405	743197.112557	42.101274
3505.008724	743119.435964	42.106279
3504.998219	743042.499774	42.111284
3505.085049	742959.810920	42.116288
3504.786102	742887.222752	42.121293
3504.556071	742807.205366	42.126298
3504.791017	742741.746999	42.131303
3504.620041	742680.014367	42.136308
3504.810456	742586.673032	42.141312
3504.267357	742533.951044	42.146317
3504.522349	742449.547767	42.151322
3504.467103	742382.601428	42.156327
3504.313184	742320.170854	42.161332
3504.385089	742244.746237	42.166336
3504.400054	742178.528334	42.171341
3504.173173	742105.822160	42.176346
3504.462680	742036.392755	42.181351
3504.238504	741982.773681	42.186356
3504.253403	741911.756616	42.191360
3504.181203	741861.029348	42.196365
3504.206434	741783.827711	42.201370
3504.467449	741726.219832	42.206375
3504.373127	741656.108702	42.211380
3504.501206	741592.883951	42.216384
3503.808025	741530.486796	42.221389
3503.943764	741457.615818	42.226394
3503.683679	741400.932442	42.231399
3503.892990	741345.902079	42.236404
3504.260526	741290.498986	42.241408
3503.907410	741230.763414	42.246413
3504.049853	741163.081666	42.251418
3504.200786	741112.906221	42.256423
3503.937802	741049.840675	42.261428
3504.106028	740986.851742	42.266432
3503.628543	740923.870099	42.271437
3503.931578	740863.330883	42.276442
3503.808251	740808.104457	42.281447
3503.567132	740755.666906	42.286452
3503.834061	740697.259194	42.291456
3503.605863	740643.532780	42.296461
3503.467941	740597.358709	42.301466
3503.777660	740540.080386	42.306471
3503.815779	740488.089536	42.311476
3503.855046	740423.584108	42.316480
3503.793565	740377.841290	42.321485
3503.702714	740312.268275	42.326490
3503.853860	740263.076683	42.331495
3503.395513	740208.000367	42.336500
3503.854253	740148.617102	42.341504
3503.487600	740100.252038	42.346509
3503.617451	740042.505202	42.351514
3503.309486	739991.755454	42.356519
3503.392761	739941.880572	42.361524
3503.495860	739886.461909	42.366528
3503.641487	739839.098845	42.371533
3503.717409	739793.181550	42.376538
3503.340255	739744.074050	42.381543
3503.206583	739696.360556	42.386548
3503.547756	739645.303447	42.391552
3503.485963	739588.277525	42.396557
3503.465029	739546.084899	42.401562
3503.347367	739505.787833	42.406567
3503.123912	739461.204272	42.411572
3503.481374	739401.139600	42.416576
3503.124060	739360.831935	42.421581
3502.890397	739311.796984	42.426586
3503.582791	739262.163462	42.431591
3503.478643	739213.799082	42.436596
3503.208965	739164.472353	42.441600
3503.089287	739132.781594	42.446605
3503.054480	739074.708643	42.451610
3503.288124	739029.502938	42.456615
3503.130615	738986.884672	42.461620
3503.164665	738940.078880	42.466624
3503.135719	738898.923054	42.471629
3503.409187	738848.564633	42.476634
3502.846737	738810.811173	42.481639
3503.022048	738771.698787	42.486644
3503.143251	738720.523680	42.491648
3502.965463	738692.303898	42.496653
3503.110611	738633.257990	42.501658
3503.185160	738605.095146	42.506663
3503.073622	738555.194289	42.511668
3503.268385	738513.059486	42.516672
3503.244783	738470.663698	42.521677
3503.003025	738428.996388	42.526682
3502.904538	738377.608009	42.531687
3502.863542	738336.748120	42.536692
3503.220545	738286.520771	42.541696
3502.780259	738250.129785	42.546701
3502.992025	738216.846842	42.551706
3503.025928	738174.835788	42.556711
3502.800912	738127.721699	42.561716
3503.095545	738092.643373	42.566720
3502.541212	738056.963031	42.571725
3502.864923	738006.887856	42.576730
3502.509236	737977.507474	42.581735
3502.793712	737943.122860	42.586740
3502.405976	737907.117446	42.591744
3502.464941	737879.053569	42.596749
3502.303714	737845.335932	42.601754
3502.537642	737813.086696	42.606759
3502.292739	737787.942492	42.611764
3502.579305	737747.124407	42.616768
3502.836878	737723.133942	42.621773
3502.731607	737685.942821	42.626778
3502.729046	737656.403938	42.631783
3502.819306	737607.700796	42.636788
3503.070838	737566.739139	42.641792
3502.719594	737540.424198	42.646797
3502.686649	737501.735847	42.651802
3502.766745	737464.513059	42.656807
3502.418514	737426.123851	42.661812
3502.882571	737391.657706	42.666816
3502.738393	737353.333389	42.671821
3502.753683	737326.462350	42.676826
3502.867896	737280.326314	42.681831
3502.524935	737249.951502	42.686836
3502.571161	737201.352125	42.691840
3502.331197	737179.174146	42.696845
3502.316802	737151.565182	42.701850
3502.595845	737117.573779	42.706855
3502.287444	737091.002857	42.711860
3502.629745	737060.761495	42.716864
3502.439324	737028.826641	42.721869
3502.493269	736999.226506	42.726874
3502.412195	736959.009477	42.731879
3502.380439	736932.887153	42.736884
3502.563207	736899.455062	42.741888
3502.443274	736876.316198	42.746893
3502.336681	736837.537832	42.751898
3502.711191	736799.966386	42.756903
3502.361870	736774.984700	42.761908
3502.432171	736739.541628	42.766912
3502.443413	736715.539367	42.771917
3502.356186	736684.971684	42.776922
3502.659514	736648.796898	42.781927
3502.651122	736622.867644	42.786932
3502.759269	736584.943319	42.791937
3502.605896	736553.693255	42.796941
3502.524752	736514.562710	42.801946
3502.595570	736479.316348	42.806951
3502.172033	736447.269233	42.811956
3502.302921	736420.277071	42.816961
3502.202605	736388.968107	42.821965
3502.319837	736354.257889	42.826970
3502.097966	736342.219618	42.831975
3502.272014	736318.733630	42.836980
3502.618713	736283.787232	42.841985
3502.301762	736272.457406	42.846989
3502.156877	736230.960563	42.851994
3502.121276	736204.787007	42.856999
3502.363815	736174.509300	42.862004
3502.361818	736152.932503	42.867009
3501.941802	736131.226772	42.872013
3502.028994	736105.131577	42.877018
3502.143653	736071.707287	42.882023
3502.069003	736061.920789	42.887028
3502.257287	736017.843803	42.892033
3502.303113	736005.117414	42.897037
3502.195881	735975.144208	42.902042
3502.573676	735945.981562	42.907047
3502.519931	735919.216187	42.912052
3502.206879	735883.040827	42.917057
3502.370163	735862.475242	42.922061
3502.319117	735828.681395	42.927066
3502.165375	735796.686068	42.932071
3501.827482	735771.699356	42.937076
3502.186000	735749.863929	42.942081
3502.321788	735723.610987	42.947085
3502.173276	735700.671413	42.952090
3501.963730	735670.614992	42.957095
3502.126007	735652.226689	42.962100
3502.624851	735624.478148	42.967105
3502.184794	735589.708241	42.972109
3502.088425	735563.196184	42.977114
3502.305514	735549.599391	42.982119
3501.592810	735529.227210	42.987124
3501.883217	735505.769105	42.992129
3502.231548	735478.143919	42.997133
3501.986722	735458.436637	43.002138
3502.019172	735419.281969	43.007143
3501.736500	735411.855259	43.012148
3501.999495	735387.807415	43.017153
3501.982706	735365.785499	43.022157
3502.025319	735348.455651	43.027162
3502.089980	735318.946525	43.032167
3501.759151	735315.586218	43.037172
3501.914073	735274.381335	43.042177
3502.193811	735266.762557	43.047181
3501.792319	735233.321084	43.052186
3501.955784	735219.336636	43.057191
3502.002494	735200.372458	43.062196
3502.072520	735160.121425	43.067201
3501.884979	735155.499987	43.072205
3501.904175	735124.017845	43.077210
3502.146170	735107.297969	43.082215
3502.006098	735087.572462	43.087220
3501.940096	735060.113305	43.092225
3502.035525	735036.884039	43.097229
3501.675559	735009.423792	43.102234
3501.969342	734995.219433	43.107239
3501.718228	734974.918044	43.112244
3501.777884	734955.604674	43.117249
3501.839359	734944.309417	43.122253
3501.880865	734920.494767	43.127258
3502.399090	734906.154166	43.132263
3502.216933	734874.110357	43.137268
3502.103184	734850.420150	43.142273
3502.024859	734817.468005	43.147277
3501.793973	734800.479159	43.152282
3502.315144	734763.715406	43.157287
3502.023458	734760.150403	43.162292
3501.862954	734729.587372	43.167297
3502.149575	734723.946862	43.172301
3502.031434	734691.891747	43.177306
3501.903097	734681.815447	43.182311
3501.812915	734658.665260	43.187316
3501.871784	734628.461578	43.192321
3501.853332	734622.673420	43.197325
3501.639719	734595.187569	43.202330
3501.686318	734578.350390	43.207335
3501.677126	734576.817573	43.212340
3501.743430	734540.573463	43.217345
3501.524948	734525.363952	43.222349
3501.664270	734519.549646	43.227354
3501.936896	734490.052608	43.232359
3501.503854	734475.026959	43.237364
3501.971780	734457.872401	43.242369
3501.830057	734437.056577	43.247373
3501.676825	734420.945089	43.252378
3501.787876	734404.740394	43.257383
3501.620994	734384.819591	43.262388
3501.779990	734359.647360	43.267393
3501.473759	734360.490102	43.272397
3501.496214	734334.845356	43.277402
3501.985871	734315.459387	43.282407
3501.834633	734311.672970	43.287412
3501.737931	734274.563590	43.292417
3501.879136	734267.857778	43.297421
3501.911595	734249.586724	43.302426
3502.226269	734223.645827	43.307431
3501.765298	734209.465813	43.312436
3502.075701	734184.119509	43.317441
3501.878082	734166.034793	43.322445
3501.611342	734141.328248	43.327450
3501.988583	734129.979665	43.332455
3501.734342	734111.805181	43.337460
3502.025503	734085.570714	43.342465
3501.714555	734070.375623	43.347469
3502.017775	734058.197638	43.352474
3502.041809	734039.630487	43.357479
3502.020187	734023.298444	43.362484
3502.010023	733981.767705	43.367489
3501.977920	733978.703981	43.372493
3501.795358	733955.765048	43.377498
3501.864462	733947.932323	43.382503
3501.650275	733924.255984	43.387508
3501.711567	733899.197467	43.392513
3501.685071	733886.331166	43.397517
3501.565087	733865.559772	43.402522
3501.978344	733847.967426	43.407527
3501.659187	733832.476220	43.412532
3501.531587	733811.161406	43.417537
3501.961224	733798.467102	43.422541
3501.979594	733782.276471	43.427546
3502.010126	733749.945512	43.432551
3501.793586	733748.446804	43.437556
3501.837131	733710.767103	43.442561
3501.892513	733700.213672	43.447565
3501.857095	733687.150510	43.452570
3501.991912	733664.653340	43.457575
3501.731473	733648.360003	43.462580
3501.850779	733621.607879	43.467585
3501.849683	733595.073583	43.472589
3501.807333	733590.229226	43.477594
3501.998819	733560.890712	43.482599
3501.566450	733551.704826	43.487604
3501.839444	733532.748828	43.492609
3501.888264	733503.730716	43.497613
3501.507237	733497.407602	43.502618
3501.739626	733461.279704	43.507623
3501.280600	733460.811129	43.512628
3501.716739	733451.976657	43.517633
3501.724796	733439.004919	43.522637
3501.475268	733415.976502	43.527642
3501.945130	733393.274688	43.532647
3501.672199	733403.419178	43.537652
3501.702583	733367.720294	43.542657
3501.673194	733357.279436	43.547661
3501.994553	733341.780445	43.552666
3502.124556	733303.391461	43.557671
3501.525738	733297.252701	43.562676
3502.025616	733264.990754	43.567681
3501.867170	733256.452358	43.572685
3501.649673	733248.567304	43.577690
3501.896961	733213.376469	43.582695
3501.769461	733205.625022	43.587700
3501.796281	733197.204468	43.592705
3501.449378	733170.527894	43.597709
3501.290229	733173.178225	43.602714
3501.779251	733155.076775	43.607719
3501.166591	733143.791388	43.612724
3501.271869	733127.189017	43.617729
3501.522932	733122.196873	43.622733
3501.297393	733119.313313	43.627738
3501.931738	733107.970317	43.632743
3501.426756	733077.210398	43.637748
3501.526092	733073.530510	43.642753
3501.524547	733062.044997	43.647757
3501.617188	733029.651378	43.652762
3501.488349	733023.929822	43.657767
3501.753865	733021.856226	43.662772
3501.474459	733008.832286	43.667777
3501.776825	732977.047407	43.672781
3501.391953	732972.308793	43.677786
3501.625101	732963.111265	43.682791
3501.583845	732936.036841	43.687796
3501.620089	732914.643069	43.692801
3501.675814	732913.693317	43.697805
3501.411049	732892.200703	43.702810
3501.367987	732873.740975	43.707815
3501.128980	732873.632076	43.712820
3501.446092	732861.301466	43.717825
3501.671486	732869.730458	43.722829
3501.487892	732839.213574	43.727834
3501.227525	732814.650431	43.732839
3501.618475	732815.180070	43.737844
3501.663111	732797.398810	43.742849
3501.515171	732783.065522	43.747853
3501.428786	732764.612704	43.752858
3501.935678	732761.558462	43.757863
3501.544740	732738.254416	43.762868
3501.527368	732730.830884	43.767873
3501.802959	732719.695166	43.772877
3501.460399	732697.868318	43.777882
3501.740076	732677.275366	43.782887
3501.323579	732671.799140	43.787892
3501.429035	732654.601642	43.792897
3501.655724	732632.333967	43.797901
3501.602306	732635.115533	43.802906
3501.772574	732604.291726	43.807911
3501.715078	732600.191942	43.812916
3501.858843	732578.829023	43.817921
3501.632705	732573.915405	43.822925
3501.747871	732547.556496	43.827930
3501.535810	732525.559081	43.832935
3501.232884	732530.213842	43.837940
3501.599291	732513.071941	43.842945
3501.598987	732487.623128	43.847949
3501.313605	732478.758302	43.852954
3501.640287	732475.436666	43.857959
3501.717288	732454.332010	43.862964
3501.639868	732428.499659	43.867969
3501.479791	732420.802353	43.872973
3501.379015	732419.581333	43.877978
3501.324754	732398.498225	43.882983
3501.386401	732387.595457	43.887988
3501.684171	732379.426347	43.892993
3501.599554	732379.192900	43.897997
3501.289728	732350.873575	43.903002
3501.559314	732342.956649	43.908007
3501.032455	732341.756520	43.913012
3501.112359	732339.762940	43.918017
3501.301660	732334.631982	43.923021
3501.191162	732315.488945	43.928026
3501.324414	732288.829126	43.933031
3501.203938	732280.233907	43.938036
3501.194533	732287.514001	43.943041
3501.357236	732287.091139	43.948045
3501.359909	732278.029949	43.953050
3501.429350	732251.727146	43.958055
3501.562863	732238.386154	43.963060
3501.582562	732234.223913	43.968065
3501.589841	732224.716283	43.973069
3501.280710	732203.179651	43.978074
3501.532130	732200.910124	43.983079
3501.324221	732196.785479	43.988084
3500.875572	732192.354022	43.993089
3501.088380	732183.604594	43.998093
3500.794797	732185.534759	44.003098
3501.338539	732164.847350	44.008103
3501.052244	732154.100796	44.013108
3501.084265	732141.717179	44.018113
3501.295719	732140.246463	44.023117
3501.115106	732147.010324	44.028122
3501.291331	732142.426058	44.033127
3501.266525	732136.142026	44.038132
3501.609233	732113.111041	44.043137
3501.385764	732101.215211	44.048141
3501.061595	732098.545638	44.053146
3501.115955	732083.335934	44.058151
3501.228459	732079.950505	44.063156
3501.583785	732081.228798	44.068161
3501.518700	732050.095175	44.073165
3501.302194	732038.099072	44.078170
3501.209408	732034.896094	44.083175
3501.052187	732037.893077	44.088180
3501.115646	732034.367190	44.093185
3501.354431	732011.402605	44.098189
3501.054272	732008.927092	44.103194
3501.005108	731997.101332	44.108199
3501.014243	731997.842674	44.113204
3501.179200	731994.002907	44.118209
3501.372581	731992.485636	44.123213
3501.184028	731995.933445	44.128218
3501.279099	731979.776039	44.133223
3501.011630	731966.302806	44.138228
3501.215279	731949.879822	44.143233
3501.250194	731936.703173	44.148237
3501.133132	731943.506217	44.153242
3501.397491	731928.162487	44.158247
3501.066426	731937.575690	44.163252
3500.895215	731939.238113	44.168257
3501.264895	731919.420602	44.173261
3501.266981	731909.616368	44.178266
3501.665711	731895.092130	44.183271
3501.405855	731895.877934	44.188276
3501.338220	731883.956031	44.193281
3501.192984	731850.507659	44.198285
3501.593225	731853.610646	44.203290
3501.504075	731842.286424	44.208295
3501.484225	731840.903395	44.213300
3501.404704	731825.764849	44.218305
3501.388998	731807.001068	44.223309
3501.461023	731797.680299	44.228314
3501.548904	731790.783184	44.233319
3501.171288	731779.952191	44.238324
3501.100801	731762.880907	44.243329
3501.678385	731752.634763	44.248333
3501.525581	731751.224175	44.253338
3501.493087	731747.119826	44.258343
3501.288482	731710.561161	44.263348
3501.399449	731709.503106	44.268353
3501.372797	731700.792732	44.273357
3501.259191	731706.605072	44.278362
3501.362966	731695.545860	44.283367
3501.541964	731682.840153	44.288372
3501.253893	731659.763574	44.293377
3501.482455	731652.942126	44.298381
3501.356095	731654.894296	44.303386
3501.686647	731645.382077	44.308391
3501.734264	731625.369488	44.313396
3500.886639	731617.438420	44.318401
3501.281179	731617.422865	44.323405
3501.064729	731623.301778	44.328410
3501.172008	731595.505077	44.333415
3501.496053	731588.667797	44.338420
3501.204643	731592.528912	44.343425
3501.644277	731567.945328	44.348429
3501.289020	731565.033126	44.353434
3501.156849	731552.279603	44.358439
3501.275316	731536.265998	44.363444
3501.079760	731530.405854	44.368449
3501.330432	731521.104762	44.373453
3501.235017	731525.478213	44.378458
3501.510538	731520.976223	44.383463
3500.968501	731498.040188	44.388468
3501.235365	731486.409043	44.393473
3501.669410	731471.927731	44.398477
3501.000031	731468.869334	44.403482
3501.377175	731463.211604	44.408487
3501.540671	731457.341587	44.413492
3501.373348	731444.296595	44.418497
3501.618794	731436.382777	44.423501
3501.431722	731431.709595	44.428506
3501.389091	731418.148773	44.433511
3501.244578	731401.237514	44.438516
3501.483072	731375.448628	44.443521
3501.588603	731388.504204	44.448525
3501.405608	731381.899099	44.453530
3501.563994	731356.668096	44.458535
3501.559898	731341.862810	44.463540
3501.602431	731338.042967	44.468545
3501.694579	731329.906785	44.473549
3501.568342	731310.120224	44.478554
3501.627100	731293.472262	44.483559
3501.780661	731288.940780	44.488564
3501.073099	731265.041057	44.493569
3501.596906	731247.127683	44.498573
3501.465652	731241.801415	44.503578
3501.251640	731233.864292	44.508583
3501.276741	731206.822631	44.513588
3501.307795	731197.210826	44.518593
3501.808133	731183.510359	44.523597
3501.422081	731190.358487	44.528602
3501.335871	731169.029856	44.533607
3501.480256	731162.073349	44.538612
3501.096475	731139.357741	44.543617
3501.099721	731146.735810	44.548621
3501.065307	731144.562750	44.553626
3501.281643	731145.814647	44.558631
3501.426227	731133.658486	44.563636
3501.351031	731109.356676	44.568641
3501.536038	731097.342342	44.573645
3501.028188	731105.547716	44.578650
3501.397651	731088.996547	44.583655
3501.548830	731090.358261	44.588660
3501.345264	731068.553557	44.593665
3501.471473	731061.055243	44.598669
3501.273208	731052.768696	44.603674
3501.478087	731046.891545	44.608679
3501.297921	731027.509370	44.613684
3501.132087	731015.800499	44.618689
3501.471489	731005.939426	44.623693
3501.220842	731019.549667	44.628698
3501.219039	731006.823261	44.633703
3501.271338	730999.634229	44.638708
3501.200379	730978.054971	44.643713
3501.342851	730958.322185	44.648717
3501.146635	730966.525718	44.653722
3501.433237	730945.233929	44.658727
3501.407490	730951.477980	44.663732
3501.118147	730930.330854	44.668737
3501.344849	730921.429208	44.673741
3501.141972	730905.764593	44.678746
3501.149017	730915.222143	44.683751
3501.538431	730902.728048	44.688756
3501.273044	730905.693801	44.693761
3501.231556	730881.583823	44.698765
3501.228306	730873.661036	44.703770
3501.251257	730869.794687	44.708775
3501.176218	730867.133050	44.713780
3500.945373	730862.169642	44.718785
3501.162740	730855.002724	44.723789
3501.371630	730857.741549	44.728794
3501.386364	730844.120764	44.733799
3501.369481	730840.855245	44.738804
3501.119685	730820.196514	44.743809
3501.446371	730819.152217	44.748813
3501.370700	730823.324695	44.753818
3501.377923	730799.206422	44.758823
3501.397775	730781.424831	44.763828
3501.419486	730776.172021	44.768833
3501.531614	730768.131020	44.773837
3501.059325	730760.335159	44.778842
3501.178711	730738.030493	44.783847
3501.269925	730729.349118	44.788852
3501.134085	730726.400347	44.793857
3501.010441	730720.973433	44.798861
3500.925435	730716.431536	44.803866
3501.091192	730718.236608	44.808871
3501.284278	730717.164855	44.813876
3501.146329	730722.635263	44.818881
3501.075280	730700.213397	44.823885
3500.910809	730683.502029	44.828890
3501.002905	730673.483333	44.833895
3501.262476	730679.432827	44.838900
3500.993096	730686.163050	44.843905
3501.233463	730683.003523	44.848909
3501.321974	730684.623277	44.853914
3501.277216	730687.998351	44.858919
3500.943418	730662.697961	44.863924
3500.881752	730643.691468	44.868929
3501.520619	730630.710024	44.873933
3501.355317	730636.482149	44.878938
3501.573511	730622.183567	44.883943
3501.311207	730625.049865	44.888948
3501.308036	730606.231709	44.893953
3501.451099	730592.787387	44.898957
3501.478358	730593.823002	44.903962
3501.479044	730581.244087	44.908967
3501.331204	730570.026831	44.913972
3501.359534	730551.153818	44.918977
3501.562338	730541.562377	44.923981
3501.160723	730538.360318	44.928986
3501.158666	730533.854134	44.933991
3501.230472	730531.069071	44.938996
3500.919110	730523.692098	44.944001
3501.385436	730504.053260	44.949005
3501.274930	730502.883080	44.954010
3501.471599	730495.075456	44.959015
3501.330179	730496.337056	44.964020
3500.974796	730488.719707	44.969025
3501.387870	730450.171365	44.974029
3501.033424	730448.645297	44.979034
3501.461970	730441.839311	44.984039
3501.572364	730446.872669	44.989044
3501.195217	730441.536985	44.994049
3501.369354	730423.134821	44.999053
3501.391303	730414.910277	45.004058
3501.431094	730398.263613	45.009063
3501.224415	730394.236888	45.014068
3501.191584	730398.154881	45.019073
3501.101251	730380.786818	45.024077
3501.096318	730370.189489	45.029082
3501.153692	730354.332224	45.034087
3501.731179	730348.145368	45.039092
3501.385590	730364.545783	45.044097
3501.278824	730348.567059	45.049101
3501.072040	730326.414216	45.054106
3501.306524	730311.270471	45.059111
3501.019821	730311.268457	45.064116
3501.207408	730309.058485	45.069121
3501.189108	730313.816043	45.074125
3500.914232	730305.689966	45.079130
3501.211553	730302.768506	45.084135
3501.300268	730299.831994	45.089140
3501.190578	730290.242375	45.094145
3501.361263	730257.478095	45.099149
3501.237416	730251.704222	45.104154
3501.035224	730248.716717	45.109159
3501.410049	730252.121682	45.114164
3500.927082	730256.262710	45.119169
3500.949858	730240.906195	45.124173
3500.847139	730228.591449	45.129178
3500.940843	730218.423350	45.134183
3500.861274	730201.399804	45.139188
3500.859461	730213.831177	45.144193
3500.979068	730213.068657	45.149197
3501.265817	730216.042462	45.154202
3501.068057	730208.299748	45.159207
3500.961660	730205.147818	45.164212
3500.945280	730211.242313	45.169217
3500.885369	730205.903572	45.174221
3500.923531	730204.461150	45.179226
3500.828678	730207.002766	45.184231
3501.083416	730201.661549	45.189236
3501.122442	730216.215775	45.194241
3501.160241	730209.771325	45.199245
3501.346511	730194.536281	45.204250
3501.360235	730170.365540	45.209255
3501.203658	730167.816199	45.214260
3501.198170	730166.876244	45.219265
3501.235109	730157.163183	45.224269
3501.302255	730159.479938	45.229274
3501.258303	730149.879288	45.234279
3501.288879	730133.481235	45.239284
3500.778370	730135.596303	45.244289
3500.902918	730120.817056	45.249293
3500.879274	730128.448125	45.254298
3500.748824	730132.679536	45.259303
3500.996266	730127.289950	45.264308
3500.933738	730129.182407	45.269313
3501.307212	730130.061814	45.274317
3501.385330	730132.079606	45.279322
3501.202567	730123.492388	45.284327
3501.545083	730094.215412	45.289332
3500.906964	730087.882568	45.294337
3501.405120	730082.055308	45.299341
3500.909990	730088.625225	45.304346
3501.040559	730074.191582	45.309351
3500.944770	730081.091722	45.314356
3500.634724	730090.008319	45.319361
3500.919167	730075.252091	45.324365
3500.892794	730088.975403	45.329370
3500.592691	730086.746914	45.334375
3501.135941	730077.247243	45.339380
3501.289435	730074.448524	45.344385
3500.825831	730053.823173	45.349389
3501.267043	730043.498373	45.354394
3500.970724	730045.330433	45.359399
3500.964027	730035.773019	45.364404
3500.964237	730041.221052	45.369409
3500.835870	730027.275859	45.374413
3500.780528	730036.893323	45.379418
3501.025416	730031.454569	45.384423
3500.970177	730032.751523	45.389428
3500.762318	730037.045303	45.394433
3500.906404	730037.071148	45.399437
3501.320786	730035.071255	45.404442
3500.967946	730026.214881	45.409447
3501.179287	730034.054839	45.414452
3500.895391	730045.146339	45.419457
3500.808177	730033.175421	45.424461
3500.997580	730030.172646	45.429466
3500.935258	730008.242694	45.434471
3501.374830	729989.300414	45.439476
3500.976808	729987.187133	45.444481
3501.103102	729988.701729	45.449485
3500.960327	729983.525117	45.454490
3501.081217	729988.656080	45.459495
3500.991208	729977.329392	45.464500
3500.966609	729985.753186	45.469505
3501.276105	729981.690479	45.474509
3500.947375	729987.242436	45.479514
3500.464886	729982.171492	45.484519
3501.168938	729981.114256	45.489524
3500.839783	729969.678498	45.494529
3501.381970	729949.381935	45.499533
3501.073935	729950.027298	45.504538
3501.104833	729941.305523	45.509543
3501.194995	729942.380353	45.514548
3500.964092	729948.609551	45.519553
3501.150447	729942.387976	45.524557
3501.220921	729947.824459	45.529562
3501.084719	729939.873206	45.534567
3501.146546	729916.288088	45.539572
3500.482541	729905.749544	45.544577
3500.816001	729900.642759	45.549581
3501.058621	729897.333975	45.554586
3501.072895	729899.758596	45.559591
3501.169066	729892.709918	45.564596
3501.273986	729897.546412	45.569601
3501.025816	729892.387159	45.574605
3501.188668	729899.244709	45.579610
3500.925891	729897.604329	45.584615
3501.133520	729898.659753	45.589620
3501.035296	729902.390681	45.594625
3501.046180	729886.441132	45.599629
3501.084111	729869.347943	45.604634
3500.832385	729858.146871	45.609639
3500.532545	729853.887633	45.614644
3500.782985	729857.016156	45.619649
3500.910930	729859.620115	45.624653
3500.929870	729857.586475	45.629658
3501.424542	729855.077993	45.634663
3501.069637	729866.330055	45.639668
3501.010745	729861.733835	45.644673
3501.017236	729859.949892	45.649677
3501.008919	729861.338175	45.654682
3501.031550	729867.426480	45.659687
3501.165512	729859.281918	45.664692
3501.057903	729862.865832	45.669697
3501.237566	729843.272777	45.674701
3501.293076	729831.872310	45.679706
3501.221663	729818.164985	45.684711
3501.281431	729815.332139	45.689716
3500.743451	729819.234836	45.694721
3501.252688	729815.881958	45.699725
3500.636710	729820.738578	45.704730
3500.868905	729819.511663	45.709735
3501.100870	729820.265907	45.714740
3501.285147	729815.233250	45.719745
3501.280884	729791.212939	45.724749
3501.150658	729775.187435	45.729754
3501.172463	729776.323113	45.734759
3501.445793	729775.138921	45.739764
3501.191568	729778.499461	45.744769
3501.546764	729775.072967	45.749773
3501.492997	729746.058343	45.754778
3501.366391	729735.975579	45.759783
3501.490452	729727.485821	45.764788
3501.564091	729718.657687	45.769793
3501.359321	729704.229278	45.774797
3501.713929	729691.243795	45.779802
3501.352890	729676.197287	45.784807
3501.498051	729644.227219	45.789812
3501.185517	729580.831969	45.794817
3501.349904	729454.751404	45.799821
3501.588834	729277.441328	45.804826
3500.968076	729043.009795	45.809831
3501.056533	728746.585872	45.814836
3500.952583	728411.891273	45.819841
3500.522638	727994.804131	45.824845
3500.398310	727540.786105	45.829850
3499.849632	727021.810190	45.834855
3499.888275	726450.827220	45.839860
3499.197150	725818.876899	45.844865
3499.290916	725134.664587	45.849869
3498.785793	724387.106170	45.854874
3497.993332	723590.358375	45.859879
3497.856421	722740.087316	45.864884
3497.077480	721824.592840	45.869889
3496.724650	720848.932699	45.874893
3496.500961	719830.094242	45.879898
3495.735823	718735.688311	45.884903
3495.284731	717577.200526	45.889908
3494.471458	716379.768916	45.894913
3493.636332	715105.761727	45.899917
3493.327192	713799.169964	45.904922
3492.241996	712413.689408	45.909927
3491.943643	710965.405146	45.914932
3490.905523	709459.999776	45.919937
3490.187307	707896.970957	45.924941
3489.107309	706280.076387	45.929946
3488.409421	704601.414344	45.934951
3487.581714	702839.023428	45.939956
3486.454947	701057.041867	45.944961
3485.131415	699204.640993	45.949965
3484.213990	697296.544267	45.954970
3483.499486	695336.978174	45.959975
3482.747301	693313.415757	45.964980
3481.014125	691230.449398	45.969985
3480.107544	689083.760191	45.974989
3478.991910	686899.659206	45.979994
3477.783226	684646.686364	45.984999
3476.826093	682333.850531	45.990004
3475.593105	679980.375662	45.995009
3473.863223	677560.809099	46.000013
3472.975020	675089.834061	46.005018
3471.233430	672573.577091	46.010023
3469.933354	669999.175745	46.015028
3468.383366	667369.694646	46.020033
3467.116945	664691.890739	46.025037
3465.907859	661952.091252	46.030042
3463.671789	659173.293706	46.035047
3462.295759	656336.382008	46.040052
3460.714043	653453.477223	46.045057
3459.213059	650515.904126	46.050061
3457.930081	647525.198341	46.055066
3456.082335	644499.948568	46.060071
3454.708582	641406.751524	46.065076
3452.938734	638270.211509	46.070081
3451.382791	635075.984482	46.075085
3449.168571	631838.537594	46.080090
3447.162245	628565.258406	46.085095
3445.953770	625221.814629	46.090100
3443.864863	621851.018443	46.095105
3441.944512	618414.238310	46.100109
3440.044690	614933.758878	46.105114
3437.880338	611418.926169	46.110119
3436.077055	607842.374477	46.115124
3434.000264	604242.152833	46.120129
3431.892697	600570.922205	46.125133
3429.621722	596861.944260	46.130138
3427.653528	593100.903950	46.135143
3426.082060	589317.045888	46.140148
3423.647589	585484.333177	46.145153
3421.224494	581592.483526	46.150157
3419.212151	577660.151384	46.155162
3416.943020	573700.456263	46.160167
3414.788150	569681.670889	46.165172
3412.729573	565643.079131	46.170177
3410.270898	561545.732902	46.175181
3407.751556	557399.916848	46.180186
3405.199278	553230.493739	46.185191
3403.109223	549006.781886	46.190196
3400.674537	544752.230429	46.195201
3398.314268	540464.391634	46.200205
3396.358072	536106.269491	46.205210
3393.382697	531734.532008	46.210215
3390.714302	527301.363260	46.215220
3388.093331	522847.779305	46.220225
3385.444656	518358.138473	46.225229
3382.986275	513828.253493	46.230234
3380.196770	509257.340695	46.235239
3377.760668	504648.512146	46.240244
3374.915073	500018.626461	46.245249
3372.460349	495339.686690	46.250253
3369.417811	490644.173602	46.255258
3366.557377	485889.204909	46.260263
3363.796504	481113.098312	46.265268
3360.850168	476315.051318	46.270273
3357.964139	471474.165422	46.275277
3355.247979	466608.303612	46.280282
3352.280828	461708.322545	46.285287
3349.555994	456772.371050	46.290292
3346.455607	451814.701800	46.295297
3343.244050	446822.049832	46.300301
3340.444148	441803.162129	46.305306
3337.161060	436764.035564	46.310311
3334.120976	431684.624294	46.315316
3331.449873	426579.685304	46.320321
3327.876272	421460.869447	46.325325
3325.063119	416299.946339	46.330330
3321.434698	411125.730118	46.335335
3318.463236	405914.280100	46.340340
3315.347108	400701.716705	46.345345
3312.046984	395451.033759	46.350349
3308.839433	390183.447369	46.355354
3305.381576	384884.400822	46.360359
3302.025186	379563.949904	46.365364
3298.625069	374236.638824	46.370369
3295.052369	368876.813195	46.375373
3291.911850	363519.851567	46.380378
3288.599788	358125.702080	46.385383
3285.213666	352711.697388	46.390388
3281.631007	347291.094565	46.395393
3278.178560	341842.170481	46.400397
3274.971320	336372.596503	46.405402
3271.107341	330891.285413	46.410407
3267.769439	325394.056752	46.415412
3263.972997	319892.183314	46.420417
3260.392928	314365.786410	46.425421
3257.039209	308847.107365	46.430426
3252.950406	303298.817040	46.435431
3249.484078	297752.734619	46.440436
3245.710790	292182.037896	46.445441
3242.112120	286613.399511	46.450445
3238.445368	281028.005832	46.455450
3234.437791	275444.966979	46.460455
3230.433716	269842.264510	46.465460
3226.545318	264245.771917	46.470465
3222.362780	258648.545334	46.475469
3218.977847	253035.981125	46.480474
3214.651061	247448.242137	46.485479
3210.831151	241821.054573	46.490484
3206.897557	236221.697166	46.495489
3202.817247	230612.348356	46.500493
3198.747536	224993.917590	46.505498
3194.950107	219394.339598	46.510503
3191.222064	213784.126649	46.515508
3186.853012	208140.068680	46.520513
3182.550163	202492.866058	46.525517
3178.907128	196894.485694	46.530522
3174.180551	191303.196798	46.535527
3170.133278	185712.780428	46.540532
3165.745364	180145.983165	46.545537
3161.378102	174567.270016	46.550541
3157.400813	169019.307777	46.555546
3152.869551	163481.181164	46.560551
3148.449939	157934.796356	46.565556
3143.735230	152410.188230	46.570561
3139.530110	146912.812591	46.575565
3134.975141	141418.355890	46.580570
3130.288777	135959.234173	46.585575
3126.153347	130507.691293	46.590580
3121.717760	125072.138210	46.595585
3116.223525	119660.748338	46.600589
3111.822350	114255.752765	46.605594
3106.922269	108901.453464	46.610599
3102.172182	103554.913407	46.615604
3097.700758	98243.411838	46.620609
3092.761221	92962.056114	46.625613
3088.053365	87702.691133	46.630618
3082.828835	82472.186457	46.635623
3077.829554	77280.734701	46.640628
3072.560896	72116.621281	46.645633
3067.455399	66995.871033	46.650637
3062.348785	61895.416160	46.655642
3056.779343	56865.483390	46.660647
3051.743757	51855.218097	46.665652
3046.232714	46906.045438	46.670657
3040.276738	42002.197556	46.675661
3034.264685	37142.209645	46.680666
3028.120060	32334.580239	46.685671
3021.757088	27608.220629	46.690676
3013.755913	22989.528544	46.695681
2998.331731	18651.138052	46.700685
2982.236759	14501.105464	46.705690
2965.859483	10556.612012	46.710695
2949.986063	6849.261360	46.715700
2929.988946	3524.833579	46.720705
2896.077825	901.277152	46.725709
2808.173913	246.631994	46.730714
2731.887303	267.629585	46.735719
2702.222086	253.267329	46.740724
2709.783555	245.097164	46.745729
2736.294784	230.800980	46.750733
2765.629908	223.976299	46.755738
2787.015008	223.175476	46.760743
2798.831675	231.133421	46.765748
2801.590582	224.609876	46.770753
2798.096723	225.841513	46.775757
2793.325565	224.158912	46.780762
2787.888814	226.302002	46.785767
2782.999602	222.938478	46.790772
2779.530102	229.643460	46.795777
2776.538363	227.356117	46.800781
2774.558358	219.948673	46.805786
2772.319125	214.121616	46.810791
2769.601329	218.822710	46.815796
2766.990224	218.023262	46.820801
2763.642474	223.886773	46.825805
2760.801817	216.164369	46.830810
2757.449118	207.949316	46.835815
2754.965730	206.481659	46.840820
2751.745873	211.637263	46.845825
2748.133667	212.497206	46.850829
2745.029308	210.424095	46.855834
2742.207067	213.345915	46.860839
2738.726382	209.238965	46.865844
2735.509215	204.566631	46.870849
2731.747502	205.294452	46.875853
2728.788186	202.709127	46.880858
2725.293950	206.364211	46.885863
2722.072162	195.733996	46.890868
2718.806207	195.654538	46.895873
2715.548994	201.718188	46.900877
2712.696609	200.847417	46.905882
2709.233662	200.364655	46.910887
2705.476098	204.835337	46.915892
2702.236835	202.861160	46.920897
2698.544021	199.943404	46.925901
2695.571312	203.022378	46.930906
2692.143493	200.067666	46.935911
2688.937436	196.701695	46.940916
2685.598029	204.077860	46.945921
2681.920241	202.480198	46.950925
2678.982158	194.358005	46.955930
2675.547272	201.184605	46.960935
2672.019631	194.733010	46.965940
2668.302745	193.740167	46.970945
2664.349907	192.523731	46.975949
2661.132332	191.993085	46.980954
2658.183597	194.010770	46.985959
2654.903691	187.454834	46.990964
2651.168369	192.442457	46.995969
2647.569082	199.150461	47.000973
2644.655450	192.731625	47.005978
2640.854033	195.279644	47.010983
2637.000136	188.518007	47.015988
2633.345302	189.722749	47.020993
2629.975947	191.576443	47.025997
2627.634171	174.253515	47.031002
2623.953562	186.895160	47.036007
2620.808655	185.766614	47.041012
2616.807283	188.648108	47.046017
2613.118071	193.240554	47.051021
2610.176409	187.450373	47.056026
2606.775020	188.771442	47.061031
2603.029292	187.447167	47.066036
2599.787985	190.401751	47.071041
2595.904056	192.066367	47.076045
2592.235019	179.512074	47.081050
2588.531822	185.996372	47.086055
2585.532368	178.541955	47.091060
2582.235603	186.139247	47.096065
2578.970395	190.586726	47.101069
2575.688047	183.483647	47.106074
2571.773312	189.129367	47.111079
2568.533733	179.493080	47.116084
2564.925379	175.726723	47.121089
2561.002420	192.792227	47.126093
2557.675344	177.749936	47.131098
2554.717934	189.102853	47.136103
2550.968373	178.855011	47.141108
2547.823477	179.946776	47.146113
2543.882751	188.323846	47.151117
2540.530409	177.338108	47.156122
2537.379451	182.286881	47.161127
2533.307069	183.437313	47.166132
2530.186690	175.133293	47.171137
2526.275554	183.472717	47.176141
2523.361115	187.988055	47.181146
2519.675519	177.454958	47.186151
2516.371794	176.831731	47.191156
2512.953624	173.232056	47.196161
2509.040329	181.898841	47.201165
2506.161613	173.198629	47.206170
2502.036301	179.163837	47.211175
2498.380275	171.125556	47.216180
2495.300040	174.810928	47.221185
2491.647492	170.611496	47.226189
2488.704779	179.644271	47.231194
2485.043507	172.977386	47.236199
2481.237933	177.351216	47.241204
2477.902651	174.444513	47.246209
2474.351018	174.921685	47.251213
2470.923607	171.651158	47.256218
2467.410760	177.876695	47.261223
2463.764365	172.381334	47.266228
2460.424305	167.135795	47.271233
2457.045196	177.002581	47.276237
2453.776448	164.813137	47.281242
2449.851093	175.301425	47.286247
2446.560254	169.557755	47.291252
2443.270181	172.864093	47.296257
2439.539648	176.258376	47.301261
2436.332616	174.280060	47.306266
2432.642605	174.796365	47.311271
2429.164541	175.075301	47.316276
2425.774589	165.126208	47.321281
2422.018437	171.660649	47.326285
2418.267758	169.855067	47.331290
2415.007609	174.000092	47.336295
2411.083075	175.476628	47.341300
2408.599694	168.634675	47.346305
2404.758192	174.717153	47.351309
2401.587058	173.902939	47.356314
2397.811085	169.904598	47.361319
2393.876750	179.000622	47.366324
2390.545627	168.327254	47.371329
2387.017427	182.107925	47.376333
2383.497767	164.019627	47.381338
2379.864248	166.576175	47.386343
2376.600105	172.273559	47.391348
2373.593182	169.013988	47.396353
2369.700732	176.053736	47.401357
2366.124442	173.018121	47.406362
2362.551537	175.401645	47.411367
2359.259496	163.429863	47.416372
2356.038783	171.381167	47.421377
2352.175771	170.716513	47.426381
2348.637778	166.179341	47.431386
2345.283328	169.969237	47.436391
2341.787378	168.629286	47.441396
2338.338144	166.301422	47.446401
2334.333550	164.825298	47.451405
2331.320709	167.995618	47.456410
2327.845165	170.612676	47.461415
2324.389646	169.211972	47.466420
2321.144663	167.006387	47.471425
2317.329104	160.927832	47.476429
2313.919839	167.276437	47.481434
2310.609545	165.155482	47.486439
2306.492113	168.820180	47.491444
2303.570593	143.480203	47.496449
2299.658949	170.712028	47.501453
2296.125008	159.837318	47.506458
2293.003582	160.292717	47.511463
2289.033728	164.132888	47.516468
2285.798910	158.459804	47.521473
2282.193337	163.696586	47.526477
2278.695694	156.427560	47.531482
2275.238043	151.132793	47.536487
2272.283802	157.745671	47.541492
2268.742271	147.584050	47.546497
2264.553525	158.335746	47.551501
2260.891742	159.545904	47.556506
2257.726003	157.153390	47.561511
2254.232959	156.069375	47.566516
2251.320408	150.988825	47.571521
2247.483054	167.308628	47.576525
2244.072268	154.987805	47.581530
2240.104698	152.367595	47.586535
2236.734443	155.740255	47.591540
2233.425804	151.158685	47.596545
2229.789676	152.524266	47.601549
2226.594018	152.899263	47.606554
2223.105102	160.033507	47.611559
2219.225377	162.148288	47.616564
2215.865344	144.172472	47.621569
2211.967062	162.861561	47.626573
2208.520691	154.037177	47.631578
2205.263497	160.798955	47.636583
2201.964964	157.402328	47.641588
2198.664157	157.821801	47.646593
2195.140190	158.392504	47.651597
2192.059432	145.685142	47.656602
2188.331692	157.140213	47.661607
2184.427618	163.635614	47.666612
2180.729862	157.187799	47.671617
2177.282897	148.036756	47.676621
2173.330922	164.417436	47.681626
2170.153915	156.802147	47.686631
2166.799180	162.307483	47.691636
2163.801466	147.008566	47.696641
2159.568533	156.295144	47.701645
2156.180545	150.892838	47.706650
2153.157493	152.247886	47.711655
2149.136004	156.057074	47.716660
2146.078862	152.066773	47.721665
2142.241047	158.323700	47.726669
2139.265717	159.964886	47.731674
2135.612470	156.250562	47.736679
2131.646521	159.360475	47.741684
2128.385394	154.426177	47.746689
2124.926869	157.468010	47.751693
2121.349501	148.525699	47.756698
2117.833901	151.530225	47.761703
2114.380154	157.170998	47.766708
2110.952772	154.290521	47.771713
2107.220868	158.662132	47.776717
2104.078889	155.915726	47.781722
2100.558377	146.767469	47.786727
2096.878455	160.975834	47.791732
2093.376845	154.194864	47.796737
2089.738788	166.786030	47.801741
2086.276890	155.737181	47.806746
2083.350949	163.245943	47.811751
2079.587564	155.489112	47.816756
2076.117324	151.709593	47.821761
2072.428401	157.938950	47.826765
2068.545272	147.616461	47.831770
2065.078313	156.798112	47.836775
2061.499142	151.044142	47.841780
2058.451528	144.704414	47.846785
2054.695190	149.386188	47.851789
2051.286410	148.279702	47.856794
2048.019880	146.680381	47.861799
2044.233657	148.390482	47.866804
2040.833199	155.089286	47.871809
2037.293601	153.445630	47.876813
2034.150941	140.998498	47.881818
2030.632492	147.629438	47.886823
2026.976659	141.941290	47.891828
2023.771295	139.754644	47.896833
2019.827857	139.567176	47.901837
2016.485792	147.319177	47.906842
2013.065817	142.320724	47.911847
2009.224130	144.062938	47.916852
2005.903068	136.076602	47.921857
2001.982466	141.015339	47.926861
1998.742426	144.292603	47.931866
1995.467961	141.112985	47.936871
1991.795695	148.127414	47.941876
1988.303341	141.484926	47.946881
1984.417054	145.874922	47.951885
1981.375382	147.385130	47.956890
1978.359814	146.703730	47.961895
1974.634385	152.659195	47.966900
1971.381408	135.747105	47.971905
1967.385519	150.318922	47.976909
1963.482778	139.853770	47.981914
1960.251644	142.290510	47.986919
1956.690473	139.217836	47.991924
1953.373224	137.106819	47.996929
1950.013824	137.297028	48.001933
1946.458147	139.205419	48.006938
1943.029840	137.064665	48.011943
1939.195619	144.076968	48.016948
1936.134868	135.841930	48.021953
1932.369015	146.020032	48.026957
1928.330314	144.431956	48.031962
1925.439424	152.322179	48.036967
1921.930022	144.337725	48.041972
1918.427738	138.028080	48.046977
1914.584526	141.993435	48.051981
1911.140396	144.190820	48.056986
1907.822478	142.327609	48.061991
1904.406122	150.141932	48.066996
1900.937626	135.984538	48.072001
1897.234545	141.062752	48.077005
1893.758235	137.224020	48.082010
1890.346249	139.447669	48.087015
1886.793361	142.608342	48.092020
1883.672404	131.419331	48.097025
1880.226153	145.257196	48.102029
1876.078503	135.761398	48.107034
1873.025105	130.029795	48.112039
1868.994083	136.925587	48.117044
1866.155116	133.409270	48.122049
1862.295251	137.170030	48.127053
1858.726218	141.281211	48.132058
1855.393456	135.022069	48.137063
1851.515760	136.597134	48.142068
1848.297912	127.594723	48.147073
1844.524119	131.385633	48.152077
1841.217770	131.342767	48.157082
1837.794117	131.387428	48.162087
1834.214609	133.618761	48.167092
1830.936832	138.336056	48.172097
1827.515144	135.426863	48.177101
1823.928898	135.118811	48.182106
1820.515702	129.409790	48.187111
1816.568784	136.203480	48.192116
1813.126929	135.606875	48.197121
1809.436161	135.888042	48.202125
1806.287524	135.320393	48.207130
1802.963349	133.213808	48.212135
1799.235944	127.711405	48.217140
1796.044445	125.703012	48.222145
1792.254693	126.332128	48.227149
1788.785531	132.804122	48.232154
1785.137338	132.420926	48.237159
1781.622396	129.339369	48.242164
1778.292098	125.779847	48.247169
1774.748165	137.176542	48.252173
1771.359711	133.634952	48.257178
1768.072608	128.562009	48.262183
1764.094256	128.986598	48.267188
1760.853228	131.264104	48.272193
1757.249767	136.150293	48.277197
1753.625819	122.497765	48.282202
1750.524011	123.831824	48.287207
1746.628632	127.736316	48.292212
1743.153651	120.853987	48.297217
1739.627960	138.666835	48.302221
1736.084419	131.197155	48.307226
1733.086252	128.077729	48.312231
1729.080624	127.475990	48.317236
1726.265403	130.083921	48.322241
1722.165953	135.395925	48.327245
1718.337366	126.388909	48.332250
1715.063223	130.978209	48.337255
1711.639367	131.564699	48.342260
1708.078176	123.689292	48.347265
1704.768456	124.096629	48.352269
1701.548043	124.563164	48.357274
1697.691764	133.827778	48.362279
1693.817727	130.112986	48.367284
1690.966834	119.410218	48.372289
1687.086050	125.347472	48.377293
1683.489684	118.539987	48.382298
1680.268316	120.214985	48.387303
1676.705881	129.732033	48.392308
1673.434506	121.156220	48.397313
1669.691773	123.998277	48.402317
1666.283570	122.988327	48.407322
1662.599792	124.901030	48.412327
1658.988179	131.463049	48.417332
1655.634991	124.299927	48.422337
1652.179064	125.873926	48.427341
1648.957997	122.508938	48.432346
1645.482492	120.351605	48.437351
1641.455502	132.048516	48.442356
1638.082592	121.265592	48.447361
1634.568041	129.795750	48.452365
1630.838471	124.367479	48.457370
1627.529210	117.717083	48.462375
1624.424562	125.332516	48.467380
1621.182349	118.425326	48.472385
1617.490780	123.082725	48.477389
1613.729883	124.085714	48.482394
1609.506477	113.665054	48.487399
1606.089427	123.978570	48.492404
1603.111922	115.833822	48.497409
1599.742975	129.191959	48.502413
1596.101048	127.942776	48.507418
1593.143346	114.672307	48.512423
1589.135029	118.572581	48.517428
1585.478708	112.368130	48.522433
1582.088911	120.042317	48.527437
1578.466774	123.929876	48.532442
1575.225962	114.130342	48.537447
1571.745667	126.948105	48.542452
1568.494307	125.614649	48.547457
1564.730499	124.543772	48.552461
1560.848139	122.334195	48.557466
1557.509140	110.282981	48.562471
1553.961342	119.436174	48.567476
1550.387403	114.135707	48.572481
1546.967366	117.077300	48.577485
1543.388909	123.909789	48.582490
1540.511367	113.320696	48.587495
1536.445356	123.022194	48.592500
1532.955732	119.365578	48.597505
1529.871163	111.092619	48.602509
1525.829269	126.844387	48.607514
1522.548771	116.709893	48.612519
1518.973621	128.087088	48.617524
1515.518695	121.124688	48.622529
1511.690522	123.509622	48.627533
1508.293669	128.852137	48.632538
1505.026330	126.580289	48.637543
1501.116423	137.588944	48.642548
1497.934501	130.708169	48.647553
1494.447206	128.637976	48.652557
1490.997714	133.249424	48.657562
1487.869509	122.802579	48.662567
1484.202690	125.692205	48.667572
1480.832867	124.339396	48.672577
1476.880406	128.061599	48.677581
1473.484327	125.609649	48.682586
1470.203548	124.835075	48.687591
1466.634481	131.862620	48.692596
1462.937599	122.505864	48.697601
1459.338029	123.239914	48.702605
1455.694060	125.455230	48.707610
1452.698542	117.943686	48.712615
1449.182411	117.790894	48.717620
1445.532485	116.897199	48.722625
1441.887600	122.574142	48.727629
1438.177723	123.930154	48.732634
1435.330429	116.169672	48.737639
1431.595239	127.890991	48.742644
1428.234340	122.680218	48.747649
1424.536911	110.192676	48.752653
1420.682879	118.392919	48.757658
1417.621481	115.373229	48.762663
1413.897495	134.231911	48.767668
1410.401067	119.787806	48.772673
1407.058647	116.374281	48.777677
1403.014831	125.981646	48.782682
1399.929121	120.952587	48.787687
1396.367123	115.508008	48.792692
1393.100769	113.928939	48.797697
1389.617337	123.490927	48.802701
1385.758679	121.469996	48.807706
1382.390452	118.151943	48.812711
1378.868845	126.199014	48.817716
1375.807849	117.850839	48.822721
1372.135520	116.032861	48.827725
1368.268082	121.037951	48.832730
1364.849219	113.049097	48.837735
1360.938721	115.336728	48.842740
1357.680678	123.235313	48.847745
1354.156350	116.009296	48.852749
1351.002066	116.716550	48.857754
1347.777488	121.604174	48.862759
1343.780212	122.772524	48.867764
1340.390372	118.935943	48.872769
1336.835453	115.342239	48.877773
1333.494896	122.770663	48.882778
1330.046910	117.164561	48.887783
1326.332704	126.517816	48.892788
1323.262979	116.171340	48.897793
1319.629040	119.394879	48.902797
1315.649131	122.487553	48.907802
1312.483703	115.749254	48.912807
1308.682684	123.407013	48.917812
1305.391886	121.032865	48.922817
1301.924432	120.145936	48.927821
1298.282125	118.593989	48.932826
1295.179574	116.858575	48.937831
1290.902808	126.191911	48.942836
1287.837634	118.400991	48.947841
1284.165198	115.124807	48.952845
1280.671452	116.307964	48.957850
1277.643935	114.661943	48.962855
1274.145305	118.286162	48.967860
1270.409056	120.460318	48.972865
1267.228559	122.877751	48.977869
1263.092733	126.170788	48.982874
1259.536218	124.582345	48.987879
1255.769469	118.306552	48.992884
1252.806430	120.836713	48.997889
1249.600744	114.577963	49.002893
1245.952906	117.064853	49.007898
1242.499050	118.319373	49.012903
1238.845859	120.526350	49.017908
1235.007926	118.731437	49.022913
1231.980088	120.110848	49.027917
1227.992962	118.259787	49.032922
1224.968441	116.243109	49.037927
1221.599180	114.079979	49.042932
1218.016101	117.706416	49.047937
1214.283215	122.674330	49.052941
1209.932139	121.539808	49.057946
1207.125272	108.701692	49.062951
1203.881771	114.002035	49.067956
1200.466466	113.343742	49.072961
1196.679967	116.678739	49.077965
1193.353010	114.455927	49.082970
1189.937687	113.166767	49.087975
1186.240445	121.808103	49.092980
1182.577868	105.470760	49.097985
1179.382496	112.041470	49.102989
1175.624318	107.086093	49.107994
1172.554085	103.768517	49.112999
1168.616117	105.213733	49.118004
1165.134803	109.157616	49.123009
1161.416446	106.897751	49.128013
1158.266688	105.329730	49.133018
1154.496033	105.961413	49.138023
1151.412320	109.464401	49.143028
1147.852426	113.471460	49.148033
1144.388753	111.327024	49.153037
1140.684987	115.842024	49.158042
1137.155436	108.778116	49.163047
1133.571077	107.585530	49.168052
1129.956396	115.292250	49.173057
1126.735845	103.624965	49.178061
1123.305816	124.301269	49.183066
1119.721603	113.499254	49.188071
1116.148837	115.294382	49.193076
1112.665633	104.358009	49.198081
1109.497735	115.100407	49.203085
1105.774742	123.233607	49.208090
1102.268643	104.119346	49.213095
1098.516186	116.683259	49.218100
1094.849376	113.280822	49.223105
1091.535022	120.653777	49.228109
1087.930553	115.789210	49.233114
1084.923886	114.440818	49.238119
1080.948129	110.480885	49.243124
1077.939797	115.612652	49.248129
1074.471165	108.495876	49.253133
1070.735866	115.403723	49.258138
1067.258784	109.163732	49.263143
1063.749556	117.893161	49.268148
1059.990286	104.712584	49.273153
1056.426204	107.628763	49.278157
1052.936361	114.880301	49.283162
1049.585722	107.039090	49.288167
1046.039870	105.879663	49.293172
1042.342573	100.963654	49.298177
1038.915451	115.435328	49.303181
1035.528744	113.055428	49.308186
1032.335062	110.374926	49.313191
1029.166067	112.810964	49.318196
1025.309607	113.629679	49.323201
1021.686606	107.461704	49.328205
1017.981151	118.650160	49.333210
1014.601156	108.636266	49.338215
1011.259000	115.320264	49.343220
1007.391077	112.159676	49.348225
1004.013731	107.119170	49.353229
1000.413476	110.298726	49.358234
997.098495	115.105522	49.363239
993.420822	106.190676	49.368244
990.103685	113.177196	49.373249
986.586968	110.012807	49.378253
983.013540	113.417624	49.383258
979.724442	113.005773	49.388263
976.310564	113.098103	49.393268
972.562175	111.316617	49.398273
969.317633	108.685459	49.403277
965.353323	108.747991	49.408282
961.956127	101.097719	49.413287
958.316939	99.492104	49.418292
954.744560	108.922176	49.423297
951.414691	108.501724	49.428301
948.114107	103.650207	49.433306
944.748708	105.520197	49.438311
941.299550	96.873154	49.443316
937.596739	101.544071	49.448321
933.898799	109.713710	49.453325
930.194675	107.129859	49.458330
927.129817	104.435961	49.463335
923.662336	103.512281	49.468340
919.873325	120.156181	49.473345
916.830556	111.574507	49.478349
912.821626	104.086795	49.483354
909.478134	108.801699	49.488359
905.855370	114.792157	49.493364
902.321435	110.384737	49.498369
898.905614	109.828624	49.503373
895.495887	109.453445	49.508378
891.957793	104.677120	49.513383
888.707427	120.183199	49.518388
885.009776	113.246702	49.523393
881.806619	100.941548	49.528397
878.142411	111.649077	49.533402
874.626317	107.470985	49.538407
870.641529	105.974720	49.543412
867.366416	123.599558	49.548417
864.202378	102.292838	49.553421
860.325812	118.639531	49.558426
857.103617	96.841844	49.563431
853.377745	109.586248	49.568436
849.576523	110.406230	49.573441
846.244963	114.757494	49.578445
842.780138	109.173204	49.583450
839.585196	93.456406	49.588455
836.404950	106.299687	49.593460
832.255041	106.473088	49.598465
828.652642	96.216486	49.603469
825.187027	106.003086	49.608474
821.867965	102.873531	49.613479
818.658960	109.045005	49.618484
814.972577	101.878992	49.623489
811.163200	96.247744	49.628493
808.024691	103.461284	49.633498
804.606465	108.199731	49.638503
800.909027	111.491112	49.643508
797.438149	114.027377	49.648513
793.772254	101.537465	49.653517
790.054232	95.911991	49.658522
786.678319	103.523910	49.663527
783.711981	106.711888	49.668532
780.190713	98.153345	49.673537
776.706035	99.588427	49.678541
772.598320	104.098206	49.683546
769.414775	101.786843	49.688551
765.650069	108.294520	49.693556
762.223854	110.982255	49.698561
758.765633	95.501845	49.703565
755.134010	103.570052	49.708570
752.263452	97.573234	49.713575
748.725357	97.495569	49.718580
744.675103	105.323082	49.723585
741.104747	100.278955	49.728589
737.252906	104.294393	49.733594
734.006005	109.410371	49.738599
730.783077	100.117990	49.743604
727.343944	112.180270	49.748609
724.279573	104.005709	49.753613
720.062269	109.870675	49.758618
716.545786	105.471590	49.763623
713.420821	110.291269	49.768628
709.734600	109.932170	49.773633
706.350260	99.767166	49.778637
702.517652	102.915714	49.783642
699.254405	106.020643	49.788647
695.779357	98.835848	49.793652
692.412798	105.616502	49.798657
688.559281	91.978995	49.803661
685.171828	101.911383	49.808666
682.449197	106.936207	49.813671
678.619019	95.649024	49.818676
674.401875	107.914329	49.823681
671.445787	100.380340	49.828685
667.998948	110.645248	49.833690
664.300486	109.114091	49.838695
660.696836	101.027556	49.843700
657.043528	105.097525	49.848705
653.829675	94.156768	49.853709
650.143511	112.461137	49.858714
646.658843	104.015444	49.863719
643.318587	110.066769	49.868724
639.495864	105.629023	49.873729
636.213570	107.623416	49.878733
632.608983	101.837582	49.883738
629.114762	102.306265	49.888743
625.731993	103.681542	49.893748
622.342341	99.868883	49.898753
618.847330	100.883531	49.903757
614.955132	100.538799	49.908762
611.670303	106.273104	49.913767
608.261735	102.514709	49.918772
604.684033	101.610417	49.923777
601.410576	95.378513	49.928781
597.732550	98.859654	49.933786
594.091527	96.900090	49.938791
590.790010	100.456845	49.943796
587.327725	108.643303	49.948801
583.824756	106.749030	49.953805
580.088331	112.540205	49.958810
576.605355	112.478214	49.963815
573.113658	103.291790	49.968820
569.423224	109.325554	49.973825
566.556305	100.529502	49.978829
562.698097	106.726703	49.983834
559.007343	100.596306	49.988839
555.783375	98.915810	49.993844
551.893383	113.558844	49.998849
548.768156	96.798114	50.003853
544.989888	111.188362	50.008858
541.498243	99.041568	50.013863
538.204220	107.667407	50.018868
534.581172	102.322227	50.023873
531.000740	100.643334	50.028877
527.857447	101.250371	50.033882
524.179583	99.472819	50.038887
520.629832	101.958099	50.043892
517.120954	108.332743	50.048897
513.738345	102.513715	50.053901
509.781760	104.574426	50.058906
506.473378	105.418073	50.063911
503.122459	102.539386	50.068916
499.664430	105.641905	50.073921
496.444597	93.761014	50.078925
492.890908	103.554222	50.083930
489.340123	103.289272	50.088935
485.750607	99.003187	50.093940
481.975880	97.768251	50.098945
478.317435	96.247013	50.103949
474.928262	98.638570	50.108954
471.343052	100.620468	50.113959
468.113077	99.140156	50.118964
464.578711	98.640241	50.123969
461.242807	95.871581	50.128973
457.750001	99.424109	50.133978
453.959189	96.091657	50.138983
450.623201	95.202618	50.143988
446.626477	96.346543	50.148993
443.314269	102.896571	50.153997
440.122737	100.990960	50.159002
436.547089	98.389424	50.164007
433.577996	100.048594	50.169012
429.383531	102.491868	50.174017
426.301888	97.545267	50.179021
422.342739	94.509382	50.184026
418.960134	95.821867	50.189031
415.467476	97.083372	50.194036
411.634634	103.741026	50.199041
408.340426	93.484000	50.204045
404.698855	95.987007	50.209050
401.341894	101.091737	50.214055
398.187941	91.153994	50.219060
394.557504	96.970749	50.224065
391.161447	94.989441	50.229069
387.528561	101.218642	50.234074
383.987598	100.725623	50.239079
380.321866	89.851915	50.244084
376.952374	93.844012	50.249089
373.996561	96.633121	50.254093
370.067568	103.210686	50.259098
366.645143	98.838948	50.264103
363.028622	89.542062	50.269108
359.262667	97.657795	50.274113
355.906296	88.159439	50.279117
352.371632	101.203227	50.284122
348.842899	95.444157	50.289127
345.371451	91.859656	50.294132
341.944692	102.323358	50.299137
338.318981	89.809132	50.304141
334.915930	95.783524	50.309146
331.420740	98.499081	50.314151
327.881844	96.945306	50.319156
324.209371	91.056026	50.324161
320.818951	89.521991	50.329165
317.251722	101.772021	50.334170
313.942123	94.047059	50.339175
310.376540	92.973307	50.344180
306.920763	101.559501	50.349185
303.246165	101.011802	50.354189
299.507678	104.866364	50.359194
295.921072	93.044243	50.364199
293.556336	105.905939	50.369204
289.438990	104.547368	50.374209
286.457512	102.728549	50.379213
282.478445	107.860575	50.384218
278.869848	102.210944	50.389223
275.314741	100.455081	50.394228
271.991017	105.116321	50.399233
268.393897	92.974917	50.404237
264.611526	101.259227	50.409242
261.186748	98.837629	50.414247
258.015905	94.071759	50.419252
254.177000	95.707072	50.424257
250.732126	83.406015	50.429261
247.252579	101.502113	50.434266
243.994991	102.950270	50.439271
240.572613	96.396936	50.444276
236.659587	100.686473	50.449281
233.536040	96.310984	50.454285
229.740880	100.977581	50.459290
226.191458	101.272884	50.464295
223.023504	90.713276	50.469300
219.154327	97.167583	50.474305
215.701814	101.030946	50.479309
212.465285	100.598010	50.484314
208.789228	107.411157	50.489319
205.129970	92.090464	50.494324
201.488799	105.314876	50.499329
198.470330	91.476830	50.504333
195.006472	101.485058	50.509338
191.654380	95.982533	50.514343
187.937312	91.388798	50.519348
184.218660	101.475290	50.524353
180.393296	91.823179	50.529357
177.316881	99.650054	50.534362
173.771265	95.988653	50.539367
170.234383	85.443048	50.544372
166.562311	96.391062	50.549377
163.305424	90.469594	50.554381
159.605308	94.874589	50.559386
156.221183	86.504856	50.564391
152.867357	87.504564	50.569396
149.370876	91.888948	50.574401
146.036161	97.720131	50.579405
142.614799	94.524536	50.584410
138.943097	98.135894	50.589415
135.326875	94.722473	50.594420
131.337990	92.393763	50.599425
128.112259	97.533156	50.604429
124.525392	95.244398	50.609434
120.906570	84.242617	50.614439
118.128606	87.442810	50.619444
114.185443	88.878528	50.624449
110.706870	89.716080	50.629453
107.065047	95.304902	50.634458
103.284739	94.678675	50.639463
100.200259	87.733073	50.644468
96.494329	98.545882	50.649473
93.403675	89.631343	50.654477
90.026166	88.581802	50.659482
86.476697	86.319626	50.664487
82.965836	87.378846	50.669492
78.997315	95.541531	50.674497
75.598901	91.111032	50.679501
71.980851	88.993467	50.684506
68.330796	87.850324	50.689511
65.227757	87.609242	50.694516
61.767238	94.257640	50.699521
58.457612	85.932654	50.704525
54.509516	94.702710	50.709530
50.992732	84.959997	50.714535
47.878725	91.268034	50.719540
44.027387	94.454096	50.724545
40.859826	82.369623	50.729549
37.369084	90.813656	50.734554
33.440562	95.919378	50.739559
30.515767	89.948166	50.744564
26.389174	86.332179	50.749569
22.981834	85.199058	50.754573
19.326918	90.142099	50.759578
15.768784	90.784582	50.764583
12.528872	91.010885	50.769588
9.050259	92.506247	50.774593
5.606262	90.876630	50.779597
2.569546	82.324397	50.784602