Fri Jun 17 17:20:35 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.010736	127.405886	0.000000
1.563063	115.582888	0.005005
1.000823	111.188633	0.010010
1.065894	100.500788	0.015014
0.738039	94.367563	0.020019
0.655294	83.661479	0.025024
0.540771	72.538592	0.030029
0.107762	73.320781	0.035034
-0.289848	52.420613	0.040038
-0.264919	51.111928	0.045043
-0.395537	53.193600	0.050048
-0.565062	38.179033	0.055053
-1.177317	37.047106	0.060058
-1.604882	22.239035	0.065062
-1.876635	12.585605	0.070067
-2.000726	6.376317	0.075072
-2.332297	3.006181	0.080077
-3.120255	6.101083	0.085082
-3.508790	13.001027	0.090086
-3.394246	7.868767	0.095091
-3.560826	5.651639	0.100096
-3.257559	2.455004	0.105101
-4.062496	-2.266896	0.110106
-4.573949	-1.468908	0.115110
-4.057295	4.307136	0.120115
-4.600225	7.747288	0.125120
-4.945839	4.254379	0.130125
-5.556053	-1.223501	0.135130
-6.195529	-5.496153	0.140134
-5.694080	-7.682046	0.145139
-6.249553	5.823463	0.150144
-5.905005	-9.125944	0.155149
-6.851247	4.734004	0.160154
-7.300984	5.331310	0.165158
-7.206661	4.953151	0.170163
-7.777652	6.514051	0.175168
-7.601123	-2.438768	0.180173
-7.705661	5.823696	0.185178
-7.837992	1.562646	0.190182
-8.639922	-4.165745	0.195187
-9.250847	0.718132	0.200192
-8.986766	-3.188101	0.205197
-9.137874	1.833053	0.210202
-9.400074	-5.660786	0.215206
-8.906581	0.358665	0.220211
-9.788019	5.834707	0.225216
-10.423015	1.509412	0.230221
-10.590660	5.389192	0.235226
-10.890775	0.391573	0.240230
-10.606537	-3.386786	0.245235
-10.772430	8.382577	0.250240
-11.366833	-2.809668	0.255245
-12.032651	3.789456	0.260250
-12.202353	-2.630296	0.265254
-12.317561	8.066240	0.270259
-12.466129	9.241983	0.275264
-12.256376	-12.357162	0.280269
-12.571941	-0.331063	0.285274
-13.646872	-6.767085	0.290278
-13.681584	1.775029	0.295283
-13.917346	4.393546	0.300288
-13.934234	-4.484103	0.305293
-14.051691	-2.520657	0.310298
-14.215405	1.158967	0.315302
-14.247795	-7.235011	0.320307
-15.058491	-9.220749	0.325312
-15.344174	2.267197	0.330317
-15.575366	-3.313741	0.335322
-15.716217	1.510153	0.340326
-15.396492	-5.888611	0.345331
-16.345213	3.182338	0.350336
-16.544422	-8.682188	0.355341
-16.916577	-9.622353	0.360346
-17.322581	-0.168224	0.365350
-17.039342	-9.158905	0.370355
-17.239635	3.303869	0.375360
-17.145348	-1.819297	0.380365
-18.218486	0.891252	0.385370
-18.977366	2.213239	0.390374
-18.729397	-0.305647	0.395379
-19.112883	6.665086	0.400384
-19.031355	2.662115	0.405389
-19.276710	6.729056	0.410394
-19.015046	-1.845029	0.415398
-18.949476	-5.310776	0.420403
-19.788961	10.160002	0.425408
-20.067961	-5.399898	0.430413
-20.331095	-0.270338	0.435418
-20.686393	-2.777940	0.440422
-21.002287	-4.285114	0.445427
-21.567832	1.554590	0.450432
-21.800067	-7.542803	0.455437
-21.877400	4.559532	0.460442
-21.944359	-0.973721	0.465446
-21.947196	-5.583271	0.470451
-22.286643	2.082045	0.475456
-22.976467	-10.468541	0.480461
-23.135307	-8.090137	0.485466
-23.678445	2.148287	0.490470
-23.479594	-6.148366	0.495475
-23.757767	-3.781697	0.500480
-23.672148	2.625030	0.505485
-23.602485	5.733660	0.510490
-24.137990	8.880531	0.515494
-24.509158	1.998376	0.520499
-25.187809	6.715522	0.525504
-25.255564	3.988838	0.530509
-25.143755	-0.214522	0.535514
-26.024460	8.432112	0.540518
-26.472724	-7.181540	0.545523
-26.986937	8.124661	0.550528
-26.687226	-1.886988	0.555533
-26.826977	-3.827772	0.560538
-27.126344	-0.968595	0.565542
-26.606079	1.466627	0.570547
-27.077375	6.375644	0.575552
-27.180076	-5.377844	0.580557
-27.463224	-9.521864	0.585562
-28.084475	2.806056	0.590566
-28.447349	-3.212772	0.595571
-29.003413	0.760187	0.600576
-29.264352	-5.403060	0.605581
-29.605783	-2.376461	0.610586
-29.745892	-1.534429	0.615590
-29.378527	1.264829	0.620595
-29.671333	9.524648	0.625600
-29.645863	5.473177	0.630605
-30.618792	1.828810	0.635610
-31.192874	5.318148	0.640614
-31.371923	4.145593	0.645619
-31.245542	-1.058881	0.650624
-31.499624	1.881371	0.655629
-31.257837	-9.827555	0.660634
-31.609615	-5.492514	0.665638
-32.336035	-5.982086	0.670643
-32.917282	-3.446244	0.675648
-33.225449	-5.766322	0.680653
-32.896979	-1.548305	0.685658
-33.017069	3.467693	0.690662
-32.999668	1.418498	0.695667
-34.074692	6.183578	0.700672
-34.528866	1.474613	0.705677
-34.620026	1.311989	0.710682
-34.808097	1.994658	0.715686
-34.660249	4.831196	0.720691
-34.774492	-3.802745	0.725696
-34.689984	-1.470515	0.730701
-34.985578	2.720215	0.735706
-36.166221	6.530802	0.740710
-35.679033	-7.724821	0.745715
-36.484007	7.333322	0.750720
-36.151144	-5.017075	0.755725
-36.383575	2.505344	0.760730
-37.033070	-1.101421	0.765734
-37.375152	-9.842917	0.770739
-37.865138	-4.361695	0.775744
-37.475160	-1.030840	0.780749
-37.663865	1.256035	0.785754
-38.512895	-0.295119	0.790758
-38.389175	-3.392052	0.795763
-38.855093	-4.983606	0.800768
-39.086738	-0.883229	0.805773
-39.336528	-5.704901	0.810778
-39.311598	-10.856987	0.815782
-39.394423	-15.977543	0.820787
-40.059974	-12.809451	0.825792
-40.475084	-9.280831	0.830797
-40.378451	-10.309775	0.835802
-40.664008	1.049489	0.840806
-40.664367	0.034497	0.845811
-41.264281	-4.880325	0.850816
-41.565657	-2.133489	0.855821
-41.843132	-5.570626	0.860826
-42.400165	0.575500	0.865830
-42.088329	-5.808068	0.870835
-42.235504	4.798072	0.875840
-42.681065	-0.789654	0.880845
-43.253156	-0.573178	0.885850
-43.841368	2.989549	0.890854
-43.936655	-9.759909	0.895859
-44.395679	-0.691036	0.900864
-44.159333	-9.292875	0.905869
-43.742993	2.626357	0.910874
-44.304081	0.550982	0.915878
-44.024989	-2.862053	0.920883
-44.959746	-1.289221	0.925888
-45.482231	-6.586514	0.930893
-45.787431	-7.935230	0.935898
-46.164610	-2.123089	0.940902
-45.608322	-13.470687	0.945907
-45.891314	-7.900939	0.950912
-46.666955	-8.785078	0.955917
-46.988042	-2.988774	0.960922
-47.467280	-3.209625	0.965926
-47.312216	-8.128393	0.970931
-47.133098	1.614448	0.975936
-47.194436	-0.918930	0.980941
-47.717822	-5.160552	0.985946
-48.601130	4.096070	0.990950
-48.680548	-5.221686	0.995955
-48.963659	-0.741179	1.000960
-48.739015	-0.566573	1.005965
-49.038878	-13.186709	1.010970
-49.679025	2.656045	1.015974
-50.066612	-8.650089	1.020979
-50.095716	0.989234	1.025984
-50.574826	-7.078094	1.030989
-50.341321	-5.958958	1.035994
-50.690967	-9.585570	1.040998
-50.819381	-5.992918	1.046003
-51.573774	-7.094297	1.051008
-52.011781	0.825777	1.056013
-51.860074	-6.360551	1.061018
-52.196393	2.404362	1.066022
-51.777280	1.148553	1.071027
-52.162051	2.833210	1.076032
-52.937232	-9.245173	1.081037
-53.282164	-9.145587	1.086042
-53.344195	-6.793537	1.091046
-53.386064	-7.839121	1.096051
-53.838271	-10.018825	1.101056
-53.593228	-18.721165	1.106061
-54.303037	-3.030028	1.111066
-54.650538	-3.507207	1.116070
-54.863843	0.947883	1.121075
-54.962941	-7.612599	1.126080
-54.867662	-10.117942	1.131085
-55.195064	-8.784600	1.136090
-56.314255	-1.086552	1.141094
-56.239396	-14.496339	1.146099
-56.749751	-9.370281	1.151104
-56.688238	-5.434077	1.156109
-56.767802	-3.982293	1.161114
-56.736083	3.573370	1.166118
-56.903740	0.513823	1.171123
-57.747898	1.630366	1.176128
-58.154367	4.270553	1.181133
-58.532109	-4.673197	1.186138
-58.597325	-1.644168	1.191142
-58.523055	-4.578963	1.196147
-58.518149	-0.156005	1.201152
-58.700995	-2.238607	1.206157
-59.078644	-11.319711	1.211162
-59.644768	-11.116459	1.216166
-59.937227	-6.818115	1.221171
-60.460771	-16.826687	1.226176
-60.313907	-0.716950	1.231181
-60.207954	-13.010674	1.236186
-60.212752	2.283256	1.241190
-60.833407	2.709875	1.246195
-61.443202	5.529889	1.251200
-61.823792	-3.239738	1.256205
-61.875070	-10.148617	1.261210
-61.932830	2.666767	1.266214
-62.390028	-1.497056	1.271219
-62.856139	-5.250331	1.276224
-63.307543	-4.775086	1.281229
-63.365598	-10.357567	1.286234
-63.473396	-4.450893	1.291238
-63.217309	5.225281	1.296243
-63.691063	-1.637246	1.301248
-63.696360	-1.556627	1.306253
-64.645347	-11.475335	1.311258
-64.778803	1.689475	1.316262
-64.851449	7.675951	1.321267
-64.925481	-3.402099	1.326272
-65.135008	-7.206907	1.331277
-64.959817	-4.001175	1.336282
-65.829402	5.679600	1.341286
-66.200730	-2.734594	1.346291
-66.495578	-1.824411	1.351296
-66.710636	-1.719379	1.356301
-66.634825	-2.522274	1.361306
-66.680785	0.080873	1.366310
-67.136173	-3.612420	1.371315
-67.627642	-1.501945	1.376320
-67.738957	-6.871335	1.381325
-67.370806	-10.818154	1.386330
-68.883470	7.101123	1.391334
-69.241709	-4.847069	1.396339
-69.208422	-8.293635	1.401344
-69.016331	-7.702776	1.406349
-69.345769	-2.923703	1.411354
-69.622722	-8.678569	1.416358
-69.655725	-3.349089	1.421363
-69.537245	-8.123447	1.426368
-70.464321	-2.642374	1.431373
-70.504496	-6.886375	1.436378
-71.507551	-4.449321	1.441382
-71.150705	-7.887121	1.446387
-71.412501	-6.900738	1.451392
-71.236348	-4.841853	1.456397
-71.445563	-8.468720	1.461402
-72.405987	0.286677	1.466406
-72.479051	-9.058178	1.471411
-72.842666	-12.528546	1.476416
-72.960692	-7.404167	1.481421
-72.917411	-12.261530	1.486426
-73.156763	-4.396780	1.491430
-73.032051	-5.839656	1.496435
-73.774905	-5.749297	1.501440
-74.429781	-3.539434	1.506445
-74.297435	-7.927947	1.511450
-74.641071	-1.422239	1.516454
-74.365613	-7.070425	1.521459
-75.478333	1.874273	1.526464
-76.100245	-3.373531	1.531469
-75.925417	-13.366187	1.536474
-76.284308	1.247011	1.541478
-76.116608	-5.611053	1.546483
-76.067859	-13.643779	1.551488
-76.168103	-3.521016	1.556493
-76.175466	-19.154263	1.561498
-76.985882	-0.669368	1.566502
-77.097438	-14.285748	1.571507
-77.598396	-8.613264	1.576512
-77.519017	-9.081684	1.581517
-78.326530	-10.316107	1.586522
-79.343884	-11.053694	1.591526
-78.803786	-12.086902	1.596531
-79.059556	-6.478857	1.601536
-79.821614	-2.480725	1.606541
-78.954024	-14.280854	1.611546
-79.383860	-4.581825	1.616550
-79.216409	-10.748202	1.621555
-79.741889	-0.166002	1.626560
-80.610997	-3.227727	1.631565
-80.497930	-3.004777	1.636570
-80.903252	-10.642540	1.641574
-80.854623	-7.636779	1.646579
-81.205352	-9.845190	1.651584
-81.847533	-7.344204	1.656589
-82.450009	-4.639266	1.661594
-82.705201	1.696836	1.666598
-82.456003	-7.295882	1.671603
-82.521688	-7.374138	1.676608
-82.869630	-4.539246	1.681613
-82.657918	-0.487118	1.686618
-82.765332	2.620953	1.691622
-83.701442	-0.456273	1.696627
-83.538933	-13.512607	1.701632
-84.134169	-2.607030	1.706637
-84.129621	-7.861693	1.711642
-84.722214	-3.193973	1.716646
-85.227964	-1.083688	1.721651
-85.757675	-5.139549	1.726656
-85.981295	-1.283813	1.731661
-85.954070	-7.046623	1.736666
-86.209430	-7.792686	1.741670
-86.032745	-6.564257	1.746675
-86.128424	-1.433133	1.751680
-86.171989	-3.728128	1.756685
-86.133771	-4.111563	1.761690
-87.099569	1.416206	1.766694
-87.233911	-8.961548	1.771699
-87.047861	-4.998099	1.776704
-87.768017	-3.756337	1.781709
-88.514107	-2.495464	1.786714
-88.926284	2.839631	1.791718
-88.995622	-1.600799	1.796723
-88.888976	-2.195901	1.801728
-89.240073	3.205012	1.806733
-88.726234	1.034019	1.811738
-89.611435	8.693178	1.816742
-89.501660	-1.433313	1.821747
-90.080810	2.695238	1.826752
-90.341079	3.966710	1.831757
-90.251855	7.413665	1.836762
-90.901993	0.627824	1.841766
-91.528515	-2.339253	1.846771
-91.949630	-2.611990	1.851776
-92.137624	-4.501928	1.856781
-91.906651	-1.869442	1.861786
-92.240198	-6.444530	1.866790
-92.337758	-5.484265	1.871795
-92.168879	-9.362043	1.876800
-92.726182	-0.319058	1.881805
-92.792981	-4.132792	1.886810
-93.645941	8.676662	1.891814
-93.618453	-2.595465	1.896819
-93.713778	-4.381623	1.901824
-93.804750	-10.208449	1.906829
-94.238246	-7.041631	1.911834
-95.228926	-10.366111	1.916838
-95.156710	-4.784572	1.921843
-95.321187	8.793478	1.926848
-95.693759	0.448560	1.931853
-95.572795	-2.686197	1.936858
-95.528067	-0.483317	1.941862
-95.936829	3.215340	1.946867
-96.567767	-12.829471	1.951872
-97.317623	-8.677279	1.956877
-97.294245	-18.193457	1.961882
-97.406837	-7.545522	1.966886
-97.333961	-3.923386	1.971891
-97.114734	-2.983227	1.976896
-97.416831	-4.101972	1.981901
-97.744421	-4.592915	1.986906
-98.621865	-3.505165	1.991910
-98.722230	-8.827237	1.996915
-98.633795	-7.731307	2.006912
-98.860426	-7.680556	2.016909
-98.394046	-9.545790	2.026906
-97.651539	-3.251896	2.036902
-97.445663	-4.969696	2.046899
-96.565853	-7.185810	2.056896
-96.072209	-8.146299	2.066893
-95.655558	-7.234336	2.076890
-94.880214	-2.075087	2.086886
-94.532092	-1.884567	2.096883
-94.505704	-1.510549	2.106880
-93.109381	-4.514940	2.116877
-92.899059	-7.845361	2.126874
-92.857149	-12.123843	2.136870
-92.551466	-7.099313	2.146867
-91.748490	-6.052806	2.156864
-90.928387	-9.527872	2.166861
-90.158380	-9.677584	2.176858
-89.973552	-12.106343	2.186854
-90.010429	-2.207786	2.196851
-89.256864	-6.218305	2.206848
-88.652885	-5.488437	2.216845
-88.202186	-10.731907	2.226842
-87.248136	-8.329409	2.236838
-87.307991	-5.505842	2.246835
-86.900459	-0.657493	2.256832
-85.913787	-6.421391	2.266829
-85.206186	-1.835922	2.276826
-85.286671	-4.849285	2.286822
-84.385551	-3.443882	2.296819
-83.963133	-0.355311	2.306816
-83.651131	0.236382	2.316813
-83.405697	-8.950708	2.326810
-82.424335	-0.882508	2.336806
-82.089231	-1.714291	2.346803
-81.876978	-3.152977	2.356800
-81.038370	-6.773575	2.366797
-80.694380	-3.798024	2.376794
-79.645704	-6.880554	2.386790
-79.511343	-0.299430	2.396787
-79.377522	1.345761	2.406784
-78.862377	-2.696646	2.416781
-78.035764	-8.266383	2.426778
-77.477718	-2.477071	2.436774
-76.744566	-3.293820	2.446771
-76.431311	-1.704144	2.456768
-76.271546	-6.428013	2.466765
-75.726365	-10.875715	2.476762
-74.932908	-4.240169	2.486758
-75.044773	-2.886864	2.496755
-73.894946	-4.399813	2.506752
-73.338027	-5.515054	2.516749
-73.131547	-3.626664	2.526746
-72.546024	-8.105178	2.536742
-71.712491	-12.281126	2.546739
-71.493563	-1.108596	2.556736
-71.324923	-8.399558	2.566733
-70.383667	-0.538075	2.576730
-69.849905	-10.362290	2.586726
-69.808271	1.775469	2.596723
-68.865929	-5.107874	2.606720
-68.262582	-2.990863	2.616717
-68.406946	-0.370983	2.626714
-67.577297	-6.308333	2.636710
-66.884544	2.023219	2.646707
-66.742315	-6.179744	2.656704
-66.167432	-0.578561	2.666701
-65.298108	-3.930808	2.676698
-65.293198	-3.628103	2.686694
-64.875725	-4.168509	2.696691
-64.087015	2.060614	2.706688
-63.331827	0.243002	2.716685
-62.539750	-0.536910	2.726682
-62.634300	-5.601023	2.736678
-61.969950	-5.695229	2.746675
-61.914823	0.712945	2.756672
-60.980102	-3.831523	2.766669
-60.632218	-2.856554	2.776666
-59.647934	-2.212427	2.786662
-59.297625	-4.906981	2.796659
-59.207544	-8.284986	2.806656
-58.621664	-8.433720	2.816653
-57.833930	-10.275708	2.826650
-57.328959	-0.723290	2.836646
-57.328812	-7.915113	2.846643
-56.725565	-11.342069	2.856640
-56.194829	-16.515460	2.866637
-55.521567	-11.204285	2.876634
-54.579394	-6.199214	2.886630
-54.488732	-3.096389	2.896627
-54.314445	-6.127013	2.906624
-53.473246	-7.390869	2.916621
-53.125751	-6.123412	2.926618
-52.523279	1.880938	2.936614
-51.522513	-1.267122	2.946611
-51.533609	-7.096320	2.956608
-51.625978	-4.280980	2.966605
-50.818148	-7.418304	2.976602
-49.821299	-7.816539	2.986598
-49.328124	-1.143514	2.996595
-48.774291	-7.377620	3.006592
-48.451471	-1.011771	3.016589
-48.241818	-10.281431	3.026586
-47.214787	0.542984	3.036582
-46.823119	-7.527374	3.046579
-46.621961	-4.883726	3.056576
-46.137098	0.643712	3.066573
-45.076348	-6.337553	3.076570
-44.847613	-8.051049	3.086566
-44.893031	-13.371888	3.096563
-44.093710	-2.609993	3.106560
-43.306862	-2.048034	3.116557
-43.045148	-7.029901	3.126554
-42.439721	-0.249674	3.136550
-42.004926	-4.881350	3.146547
-41.613248	-2.075345	3.156544
-40.231754	-0.504583	3.166541
-40.536463	-8.294790	3.176538
-40.092427	-2.932266	3.186534
-39.789733	1.648802	3.196531
-38.996893	-6.519068	3.206528
-38.589390	-2.730740	3.216525
-37.556201	-3.705830	3.226522
-37.141030	-4.814298	3.236518
-37.375049	-10.967225	3.246515
-36.736275	-7.662893	3.256512
-35.469545	-6.471381	3.266509
-35.394040	-2.457943	3.276506
-35.134788	-6.890515	3.286502
-34.940312	-5.297293	3.296499
-33.961631	-3.295027	3.306496
-33.173545	-4.858082	3.316493
-32.640620	-2.044140	3.326490
-32.484281	-5.674804	3.336486
-32.341163	-1.747686	3.346483
-31.699071	-3.443354	3.356480
-31.141747	-2.085111	3.366477
-30.076478	-10.013546	3.376474
-29.370118	-5.753870	3.386470
-29.321872	1.819414	3.396467
-29.286528	0.793054	3.406464
-28.941324	-4.628682	3.416461
-28.017343	0.976125	3.426458
-26.964852	-1.637963	3.436454
-26.760463	-9.291704	3.446451
-26.086984	-3.492525	3.456448
-25.944366	0.559550	3.466445
-25.758993	-8.348253	3.476442
-25.097289	-7.092717	3.486438
-24.448906	-2.283406	3.496435
-23.953849	0.049000	3.506432
-22.902338	-2.321304	3.516429
-22.579343	-0.944261	3.526426
-22.617116	-3.782556	3.536422
-22.508878	-5.213630	3.546419
-21.242602	-2.852739	3.556416
-21.069025	-6.035581	3.566413
-20.412488	-3.962178	3.576410
-19.590056	-0.209823	3.586406
-19.551383	-1.159284	3.596403
-19.374117	-3.212761	3.606400
-18.413146	-3.031834	3.616397
-17.834754	-4.417966	3.626394
-17.010493	-1.179829	3.636390
-16.649624	-7.587343	3.646387
-16.372487	-2.927536	3.656384
-16.309129	-5.128839	3.666381
-15.534491	-6.985634	3.676378
-14.811703	-10.251075	3.686374
-14.474321	-5.697704	3.696371
-13.493866	-3.326840	3.706368
-13.044400	-7.042584	3.716365
-13.002309	-4.212449	3.726362
-12.797307	-6.371501	3.736358
-11.880649	-8.733414	3.746355
-11.484545	-7.728322	3.756352
-10.923274	-8.411372	3.766349
-10.068909	-8.506331	3.776346
-9.735150	-1.967830	3.786342
-9.743380	-6.066677	3.796339
-8.992042	-5.207175	3.806336
-8.356367	-2.164712	3.816333
-7.838214	-2.442266	3.826330
-6.783335	-4.646958	3.836326
-6.999444	-6.011473	3.846323
-6.530546	-3.634804	3.856320
-6.081143	-2.750996	3.866317
-5.490630	-2.924992	3.876314
-4.953377	-2.698525	3.886310
-4.516091	2.795140	3.896307
-3.867451	7.014431	3.906304
-3.771547	8.612780	3.916301
-3.178689	13.214778	3.926298
-2.667467	25.701883	3.936294
-2.496021	40.171919	3.946291
-1.933931	54.608253	3.956288
-1.430321	71.914947	3.966285
-0.782311	89.902442	3.976282
-0.101771	106.915991	3.986278
0.000000	120.869289	3.991283
0.239057	130.614884	3.996288
0.465006	130.826575	4.001293
0.757242	143.392888	4.006298
1.033004	138.105324	4.011302
0.851295	145.386134	4.016307
0.892951	143.016959	4.021312
1.019785	144.189361	4.026317
0.536074	139.998519	4.031322
0.690448	138.744086	4.036326
0.708743	140.776942	4.041331
0.828651	145.734544	4.046336
0.755075	138.071147	4.051341
0.683769	143.584056	4.056346
0.970350	138.838147	4.061350
0.941898	147.796660	4.066355
0.993404	142.325358	4.071360
1.084157	134.262677	4.076365
0.999166	147.091398	4.081370
1.202508	143.533847	4.086374
0.910197	139.144247	4.091379
0.809347	153.315891	4.096384
1.231762	173.770871	4.101389
1.109590	176.473542	4.106394
1.420800	156.459047	4.111398
0.912011	154.797637	4.116403
0.920879	149.387292	4.121408
1.371145	159.917123	4.126413
1.228223	153.159953	4.131418
1.184997	157.025602	4.136422
0.965425	156.811899	4.141427
1.333062	155.463605	4.146432
1.333692	153.907944	4.151437
1.093194	142.904218	4.156442
1.370902	144.574275	4.161446
1.112726	145.338062	4.166451
1.294870	143.546610	4.171456
1.562118	144.769672	4.176461
1.014232	148.028145	4.181466
1.206665	143.106669	4.186470
0.933819	155.554986	4.191475
1.313252	170.841662	4.196480
1.395988	158.949478	4.201485
1.453186	174.889415	4.206490
1.727206	161.698555	4.211494
1.458223	159.985245	4.216499
1.177785	148.468774	4.221504
1.285834	151.583684	4.226509
1.195383	166.294106	4.231514
1.649175	162.215402	4.236518
1.722179	167.945669	4.241523
1.545490	156.436219	4.246528
1.373751	148.289488	4.251533
1.360889	149.602918	4.256538
1.327662	149.820196	4.261542
1.173415	168.211414	4.266547
1.252473	167.324895	4.271552
1.382843	172.086393	4.276557
1.374679	167.879446	4.281562
1.666348	168.526975	4.286566
1.503698	172.170942	4.291571
1.510483	171.194020	4.296576
1.890275	176.034236	4.301581
1.815277	175.318561	4.306586
1.952472	165.904898	4.311590
1.871856	178.813430	4.316595
1.620504	170.194876	4.321600
1.251726	153.217099	4.326605
1.633181	165.761102	4.331610
1.897429	170.252497	4.336614
1.721889	171.699924	4.341619
1.532828	168.390521	4.346624
1.655599	172.844457	4.351629
1.705381	171.903210	4.356634
1.622701	169.086427	4.361638
1.815064	176.415184	4.366643
1.648223	169.154443	4.371648
1.881058	174.273251	4.376653
1.876127	174.752817	4.381658
2.199972	169.783836	4.386662
1.724321	161.364778	4.391667
1.501788	158.286888	4.396672
1.811908	173.155297	4.401677
1.512396	173.922405	4.406682
1.764044	179.931808	4.411686
1.706688	185.395447	4.416691
1.662926	176.971685	4.421696
1.694401	183.958374	4.426701
1.870823	174.861219	4.431706
1.604207	183.298324	4.436710
1.599269	175.481815	4.441715
1.805155	181.171844	4.446720
1.886746	174.850748	4.451725
1.710919	184.400125	4.456730
1.660071	177.127400	4.461734
1.730344	188.274328	4.466739
1.717204	195.440710	4.471744
2.057236	198.536999	4.476749
1.901789	213.633400	4.481754
2.387342	213.197310	4.486758
2.234790	218.794396	4.491763
2.437253	211.458434	4.496768
2.385701	197.585213	4.501773
2.102342	194.006333	4.506778
2.163533	184.404999	4.511782
2.048164	183.829036	4.516787
1.928006	181.881419	4.521792
2.124959	182.575081	4.526797
1.929095	183.502758	4.531802
2.201043	186.873012	4.536806
2.246944	202.675538	4.541811
2.208156	210.679134	4.546816
2.593207	203.080368	4.551821
1.928564	192.165461	4.556826
2.079392	188.297739	4.561830
2.173590	201.217092	4.566835
2.238987	221.030156	4.571840
2.442664	216.008516	4.576845
2.041958	217.689327	4.581850
2.139327	203.436935	4.586854
2.174507	221.424164	4.591859
2.423267	207.527063	4.596864
2.683909	209.177074	4.601869
2.246831	203.658302	4.606874
2.281581	206.321871	4.611878
2.155767	211.027693	4.616883
1.866929	207.443406	4.621888
2.315175	221.037611	4.626893
2.297874	214.697613	4.631898
2.278897	208.022430	4.636902
2.175817	209.274888	4.641907
2.366565	217.134563	4.646912
2.729035	205.725883	4.651917
2.524440	217.324830	4.656922
2.225253	216.640301	4.661926
2.232674	213.741045	4.666931
2.313834	208.711751	4.671936
2.405075	210.774523	4.676941
2.414084	208.985794	4.681946
2.123929	208.673907	4.686950
2.175100	230.231407	4.691955
2.635064	240.449276	4.696960
2.736228	237.701970	4.701965
2.823945	239.034210	4.706970
2.794624	241.961022	4.711974
2.929387	233.039084	4.716979
2.665680	232.274064	4.721984
2.616536	209.639214	4.726989
2.380468	223.232912	4.731994
2.624706	225.134292	4.736998
2.827760	238.311651	4.742003
2.563204	231.805151	4.747008
2.444736	229.532829	4.752013
2.517093	241.996060	4.757018
2.702876	240.442766	4.762022
2.736620	246.867099	4.767027
2.867234	242.634696	4.772032
2.966385	238.783839	4.777037
2.769012	238.481592	4.782042
2.864321	228.629471	4.787046
2.729178	234.687994	4.792051
2.897929	245.842077	4.797056
3.319043	243.674240	4.802061
2.392093	231.110966	4.807066
3.080192	228.291951	4.812070
2.869782	233.363292	4.817075
2.754701	240.337861	4.822080
3.103883	243.952613	4.827085
2.999705	236.004964	4.832090
3.001102	215.074561	4.837094
2.682421	222.836975	4.842099
2.960697	230.039984	4.847104
3.099059	230.043248	4.852109
2.556535	224.531340	4.857114
2.657514	237.080978	4.862118
3.111981	235.820069	4.867123
2.798529	244.286106	4.872128
2.805608	240.628746	4.877133
2.754917	242.383790	4.882138
3.061256	242.214684	4.887142
2.903738	246.707536	4.892147
2.890082	238.998609	4.897152
3.249976	233.732548	4.902157
2.692272	240.994600	4.907162
2.816916	235.262073	4.912166
3.158094	251.323211	4.917171
2.794533	236.661767	4.922176
2.910146	242.057406	4.927181
3.267911	270.370240	4.932186
3.195163	261.131524	4.937190
3.428634	257.300960	4.942195
3.255608	255.255757	4.947200
3.094066	242.840527	4.952205
3.172772	258.464398	4.957210
3.000184	241.697225	4.962214
3.052322	266.581465	4.967219
3.454526	274.852391	4.972224
3.613734	260.207629	4.977229
3.410562	260.382117	4.982234
3.085894	248.777808	4.987238
3.450022	247.321359	4.992243
3.229793	251.932972	4.997248
3.513196	239.226718	5.002253
3.227693	237.296513	5.007258
3.202939	245.765081	5.012262
3.501619	250.172434	5.017267
3.139708	255.373947	5.022272
3.697337	259.807129	5.027277
3.417602	251.053141	5.032282
3.568308	248.331145	5.037286
3.407426	249.613145	5.042291
3.210520	251.478138	5.047296
3.231076	254.879341	5.052301
3.166003	265.963179	5.057306
3.559351	276.150705	5.062310
3.832703	279.313546	5.067315
3.849163	265.594916	5.072320
3.528493	254.002963	5.077325
3.394214	250.763765	5.082330
3.271462	249.868754	5.087334
3.657116	258.932941	5.092339
3.532122	274.536619	5.097344
3.659472	281.320540	5.102349
3.511481	284.159341	5.107354
3.513633	266.238684	5.112358
3.867453	275.289426	5.117363
3.313005	279.851226	5.122368
4.137243	274.302740	5.127373
3.595111	268.830217	5.132378
3.420519	256.056419	5.137382
3.309637	263.699064	5.142387
3.248580	272.851721	5.147392
3.582280	275.002072	5.152397
3.615259	280.029420	5.157402
3.393637	276.527875	5.162406
3.353134	282.657118	5.167411
3.237336	275.699630	5.172416
3.682058	273.549769	5.177421
3.744430	278.774893	5.182426
4.048450	294.263668	5.187430
3.664887	280.188433	5.192435
3.816869	290.231187	5.197440
3.757001	294.708018	5.202445
3.691233	296.619693	5.207450
3.949365	300.796604	5.212454
4.074025	299.835009	5.217459
3.813777	301.814926	5.222464
3.808484	290.062384	5.227469
3.851787	312.358547	5.232474
3.765706	303.190891	5.237478
4.122531	302.257010	5.242483
3.789839	305.044820	5.247488
3.987508	299.543641	5.252493
3.872708	303.215404	5.257498
4.029072	297.033776	5.262502
3.718738	299.814316	5.267507
3.837482	303.981048	5.272512
4.156696	302.200736	5.277517
3.956977	306.089869	5.282522
4.178182	307.105700	5.287526
3.949383	297.861327	5.292531
3.897452	301.175132	5.297536
4.104879	305.493872	5.302541
3.925627	315.117307	5.307546
3.781460	301.937034	5.312550
3.928543	307.579461	5.317555
3.741522	304.052622	5.322560
4.008390	292.437767	5.327565
3.723382	315.318153	5.332570
4.001649	322.855886	5.337574
4.264383	335.079359	5.342579
4.296719	334.051214	5.347584
4.388053	331.181994	5.352589
4.093308	331.750587	5.357594
4.176280	327.171469	5.362598
4.186178	331.383139	5.367603
4.161222	337.920079	5.372608
4.136953	335.108751	5.377613
4.176502	338.809133	5.382618
4.329277	335.828466	5.387622
4.447568	345.156188	5.392627
4.299140	339.708183	5.397632
4.363690	340.676253	5.402637
4.191268	342.827466	5.407642
4.390426	342.419837	5.412646
4.201028	333.866473	5.417651
4.141141	344.441565	5.422656
4.494739	349.357429	5.427661
4.061961	347.222584	5.432666
4.398208	336.570408	5.437670
4.600407	346.572685	5.442675
4.518388	344.350726	5.447680
4.868941	336.946281	5.452685
4.176079	334.267598	5.457690
4.050456	334.527074	5.462694
4.197355	343.963310	5.467699
3.917601	348.658847	5.472704
4.211392	340.345043	5.477709
4.268327	355.087386	5.482714
4.748935	363.431365	5.487718
4.936141	367.714016	5.492723
4.645970	358.793768	5.497728
4.691500	339.693250	5.502733
4.432977	342.892022	5.507738
4.412471	341.089042	5.512742
4.707981	340.398009	5.517747
4.426852	350.050634	5.522752
4.915929	345.242785	5.527757
4.480609	354.308318	5.532762
4.681986	349.900137	5.537766
4.566107	349.774769	5.542771
4.576200	364.236403	5.547776
4.885613	360.691167	5.552781
4.917080	360.341998	5.557786
4.748588	364.525904	5.562790
4.715468	338.059502	5.567795
4.568717	344.769624	5.572800
4.940034	361.501740	5.577805
4.912253	355.383456	5.582810
4.940421	352.682994	5.587814
4.836595	345.798077	5.592819
4.512233	344.269580	5.597824
4.735799	342.029189	5.602829
4.439882	362.584680	5.607834
4.763360	366.167227	5.612838
5.112716	360.576482	5.617843
4.691230	373.602220	5.622848
4.980030	374.770806	5.627853
4.751391	366.879297	5.632858
5.069929	371.237603	5.637862
4.950970	370.346888	5.642867
4.719726	373.751688	5.647872
5.140146	368.488151	5.652877
4.888735	369.218264	5.657882
4.808696	373.581451	5.662886
4.973929	361.631787	5.667891
4.747858	370.939014	5.672896
4.926218	368.175302	5.677901
4.905169	380.613519	5.682906
4.885542	378.757898	5.687910
4.976759	373.190323	5.692915
4.299374	381.567940	5.697920
4.689737	380.625125	5.702925
4.634604	395.500391	5.707930
5.042465	405.111541	5.712934
5.222367	407.360292	5.717939
5.458767	415.392253	5.722944
5.323925	410.766829	5.727949
5.219532	420.078133	5.732954
5.188597	413.306575	5.737958
5.240447	410.830090	5.742963
5.454477	417.607753	5.747968
5.287369	402.758588	5.752973
5.048617	392.615961	5.757978
5.174031	399.139180	5.762982
5.230849	409.585792	5.767987
5.038165	412.719366	5.772992
5.241826	403.254255	5.777997
5.313073	409.732610	5.783002
5.100193	416.306543	5.788006
5.418857	411.848263	5.793011
5.190844	406.842471	5.798016
5.087178	408.661199	5.803021
5.195308	410.698497	5.808026
5.265496	398.330266	5.813030
5.470423	408.675100	5.818035
5.172043	409.636209	5.823040
5.235897	410.061133	5.828045
5.268034	414.767402	5.833050
5.164976	414.387115	5.838054
5.296353	407.082413	5.843059
5.410546	419.744457	5.848064
5.618185	410.642765	5.853069
5.639588	419.790683	5.858074
5.171855	406.389807	5.863078
5.278049	412.958654	5.868083
5.208460	415.227367	5.873088
5.371007	418.211911	5.878093
5.529567	424.040534	5.883098
5.444130	438.499764	5.888102
5.725452	434.384734	5.893107
5.595272	443.145231	5.898112
5.736183	428.425602	5.903117
5.628084	433.766337	5.908122
5.546313	423.817823	5.913126
5.835164	418.840372	5.918131
5.516918	420.822248	5.923136
5.831908	420.333598	5.928141
5.429408	418.649950	5.933146
5.587545	415.214702	5.938150
5.750631	423.772322	5.943155
5.803829	440.662779	5.948160
5.616108	433.719740	5.953165
5.796172	432.210594	5.958170
5.826828	434.047057	5.963174
5.956185	424.693150	5.968179
5.480563	425.160188	5.973184
5.515022	419.638736	5.978189
5.500746	429.165357	5.983194
5.675721	435.365207	5.988198
5.774586	429.714052	5.993203
5.658951	440.720974	5.998208
6.039259	427.856770	6.003213
5.965094	435.781311	6.008218
5.814737	436.131334	6.013222
5.595096	439.846998	6.018227
5.574065	437.880305	6.023232
5.889810	433.691868	6.028237
5.931576	437.548392	6.033242
5.762417	440.823498	6.038246
6.104813	431.083508	6.043251
5.592281	433.795264	6.048256
5.950986	434.811535	6.053261
5.752192	435.379179	6.058266
5.826699	436.917678	6.063270
6.089196	435.763651	6.068275
5.731788	445.958469	6.073280
6.253377	433.434665	6.078285
5.830709	421.407639	6.083290
5.755019	418.543078	6.088294
6.080420	413.782937	6.093299
5.686602	424.505351	6.098304
5.437418	419.304752	6.103309
5.944467	424.656110	6.108314
5.784549	428.628248	6.113318
5.936737	423.663052	6.118323
5.725468	429.392914	6.123328
5.777106	424.682419	6.128333
5.880819	432.134174	6.133338
5.570478	432.683655	6.138342
5.828386	424.103448	6.143347
5.923329	433.022671	6.148352
5.923315	430.205716	6.153357
5.577352	418.905361	6.158362
5.360598	417.929665	6.163366
5.596733	417.733944	6.168371
5.454501	433.572714	6.173376
5.741404	432.503432	6.178381
5.741672	429.580263	6.183386
5.473782	436.424424	6.188390
5.859269	437.121886	6.193395
6.033542	445.665621	6.198400
6.064810	440.184751	6.203405
5.808397	437.947958	6.208410
6.088071	432.176762	6.213414
6.363444	440.591010	6.218419
6.040137	444.808170	6.223424
6.359195	426.655668	6.228429
5.988409	426.123927	6.233434
5.526622	419.689993	6.238438
5.810723	420.629664	6.243443
5.734638	416.766056	6.248448
5.650072	416.164639	6.253453
5.782322	418.083473	6.258458
5.486331	422.452574	6.263462
5.844977	417.487597	6.268467
5.686253	433.389690	6.273472
6.194613	424.294047	6.278477
6.058485	419.699817	6.283482
5.733133	422.224364	6.288486
5.976579	414.467287	6.293491
5.645538	426.890566	6.298496
5.710137	422.352363	6.303501
5.768922	422.788588	6.308506
5.704482	421.730150	6.313510
5.704661	406.799103	6.318515
5.813028	418.382884	6.323520
5.965481	412.057411	6.328525
5.820536	419.224493	6.333530
5.892355	410.776853	6.338534
5.862754	416.043951	6.343539
5.647155	424.818636	6.348544
5.991490	412.780357	6.353549
5.757712	415.549573	6.358554
5.417252	424.350538	6.363558
5.824843	418.077177	6.368563
5.389967	429.341793	6.373568
5.887342	443.597590	6.378573
5.824392	439.961689	6.383578
5.860992	436.309045	6.388582
6.151404	443.343585	6.393587
6.040332	430.822133	6.398592
5.946425	424.883140	6.403597
5.710764	420.919366	6.408602
5.600517	423.762575	6.413606
5.896057	424.624963	6.418611
5.997976	421.375673	6.423616
5.760450	422.795341	6.428621
5.751486	419.799313	6.433626
5.614318	415.503234	6.438630
5.817936	419.524464	6.443635
5.584283	423.701851	6.448640
5.571475	421.737938	6.453645
6.083398	422.900422	6.458650
5.651765	422.220532	6.463654
5.771401	416.090941	6.468659
5.699442	435.371807	6.473664
5.925795	432.744754	6.478669
6.169099	445.972236	6.483674
5.607843	436.557091	6.488678
5.722123	426.399767	6.493683
5.847286	419.885043	6.498688
5.952434	415.897181	6.503693
5.692890	420.001910	6.508698
5.650812	424.043853	6.513702
6.142925	423.268434	6.518707
5.907627	429.299675	6.523712
6.019008	420.021575	6.528717
5.569912	428.546371	6.533722
5.342273	422.335183	6.538726
5.805843	422.627756	6.543731
5.860096	431.528877	6.548736
5.944827	427.802127	6.553741
5.669552	415.481835	6.558746
5.737508	424.389752	6.563750
6.075637	429.422075	6.568755
5.823258	432.256548	6.573760
5.837838	417.233112	6.578765
5.763080	419.665488	6.583770
5.528264	415.699799	6.588774
5.572018	415.585587	6.593779
5.593797	441.417237	6.598784
6.157988	440.391256	6.603789
6.169738	439.560508	6.608794
5.785102	434.455038	6.613798
5.926005	421.345286	6.618803
5.775924	422.554069	6.623808
5.950552	423.210210	6.628813
6.006189	415.635509	6.633818
5.835272	427.964882	6.638822
5.794364	416.814118	6.643827
5.703645	421.063652	6.648832
5.656180	416.971507	6.653837
5.902109	419.829907	6.658842
5.875189	427.106038	6.663846
5.965326	420.300539	6.668851
5.760025	415.069756	6.673856
5.704830	410.548311	6.678861
5.716031	415.982283	6.683866
5.699597	418.232887	6.688870
5.827602	421.790316	6.693875
5.642451	421.177794	6.698880
5.922019	417.163702	6.703885
5.863766	421.748639	6.708890
5.609429	419.563008	6.713894
5.917735	417.698260	6.718899
5.756740	417.550395	6.723904
5.755800	415.178589	6.728909
5.763727	430.366249	6.733914
5.554020	420.628051	6.738918
5.957881	421.284965	6.743923
5.622804	420.331699	6.748928
5.790743	426.649144	6.753933
5.813416	439.622421	6.758938
5.787543	439.881105	6.763942
5.935796	436.723766	6.768947
5.557575	434.040125	6.773952
5.489262	443.642634	6.778957
5.841828	447.568467	6.783962
5.674586	464.235896	6.788966
6.005425	450.597260	6.793971
5.808104	451.169791	6.798976
6.003090	445.903048	6.803981
6.010555	446.452788	6.808986
5.665662	436.088801	6.813990
5.785537	430.555121	6.818995
5.596111	441.213577	6.824000
5.638112	448.229223	6.829005
5.968370	445.695207	6.834010
6.003961	440.694528	6.839014
5.977691	437.400040	6.844019
5.742440	434.412614	6.849024
5.846890	440.429814	6.854029
5.602785	431.367679	6.859034
5.498693	439.262859	6.864038
6.039943	439.126140	6.869043
6.048832	442.630557	6.874048
6.131904	441.096882	6.879053
5.937942	422.521320	6.884058
5.777719	430.788925	6.889062
5.893696	423.174787	6.894067
5.838747	416.362228	6.899072
5.499076	424.287284	6.904077
5.600108	428.133955	6.909082
5.600410	429.950204	6.914086
5.634833	437.583385	6.919091
5.776891	447.646243	6.924096
6.018538	445.492028	6.929101
5.727986	443.217889	6.934106
5.687702	451.570552	6.939110
5.769033	449.479294	6.944115
5.844158	460.625218	6.949120
5.995982	451.418719	6.954125
6.372354	446.755473	6.959130
5.843709	434.259816	6.964134
6.028667	426.613688	6.969139
5.735855	431.917637	6.974144
5.575232	426.733493	6.979149
5.945018	417.669966	6.984154
5.430416	423.199826	6.989158
5.839837	421.182700	6.994163
5.504034	426.761381	6.999168
5.960879	426.061286	7.004173
6.039507	424.550650	7.009178
5.649131	429.420494	7.014182
6.161104	417.085771	7.019187
5.817031	427.207319	7.024192
5.799935	427.266024	7.029197
5.862503	422.290664	7.034202
5.585650	427.379625	7.039206
6.014092	423.702897	7.044211
5.919204	425.640543	7.049216
5.828115	427.255308	7.054221
5.766950	429.542752	7.059226
5.689720	427.731825	7.064230
6.049453	415.686642	7.069235
5.829903	424.377918	7.074240
5.870926	418.496224	7.079245
5.958931	423.228138	7.084250
5.654813	430.006092	7.089254
6.011596	425.626129	7.094259
5.531880	424.310324	7.099264
5.418848	430.734662	7.104269
5.819479	419.029792	7.109274
5.569497	412.481720	7.114278
5.642685	416.018462	7.119283
5.560846	431.416407	7.124288
5.696187	437.598377	7.129293
6.180232	442.336889	7.134298
5.502428	449.426794	7.139302
6.040919	441.008720	7.144307
5.659170	435.043173	7.149312
6.131857	424.080148	7.154317
5.970305	424.457290	7.159322
5.411311	439.094495	7.164326
5.691269	427.778302	7.169331
5.922842	435.774765	7.174336
5.668824	436.300480	7.179341
5.616758	435.025676	7.184346
5.924166	446.023259	7.189350
6.172377	443.508407	7.194355
5.788619	438.030811	7.199360
5.623875	438.453082	7.204365
5.860056	435.950689	7.209370
5.681669	429.563773	7.214374
6.092836	433.528801	7.219379
5.859306	429.532505	7.224384
5.499294	423.225312	7.229389
5.913606	423.063319	7.234394
5.477293	428.197533	7.239398
5.961987	447.289784	7.244403
5.738284	443.740988	7.249408
5.881428	446.088209	7.254413
5.686203	446.041347	7.259418
5.696893	450.012562	7.264422
5.782911	455.517585	7.269427
5.845815	455.145231	7.274432
5.820149	450.935196	7.279437
5.811011	442.772333	7.284442
5.718765	462.754386	7.289446
5.906680	452.224272	7.294451
5.718868	449.254612	7.299456
5.761959	450.783928	7.304461
6.013225	453.225264	7.309466
5.744547	450.400866	7.314470
5.813494	439.594728	7.319475
5.810004	446.197805	7.324480
5.788819	450.535641	7.329485
5.955696	452.390115	7.334490
5.621023	448.909690	7.339494
6.024623	439.095781	7.344499
5.821704	436.968104	7.349504
5.389147	432.898130	7.354509
5.861031	446.794082	7.359514
5.683264	444.579735	7.364518
5.776982	451.839574	7.369523
5.742968	449.093586	7.374528
5.866422	447.404997	7.379533
5.955315	445.359252	7.384538
5.885854	458.617816	7.389542
5.966759	444.071738	7.394547
5.912569	452.086109	7.399552
5.622168	450.222996	7.404557
6.027017	443.949489	7.409562
5.747110	445.038560	7.414566
5.872975	433.624444	7.419571
5.422611	435.445747	7.424576
5.525049	448.344795	7.429581
5.845943	456.483700	7.434586
5.643916	453.643092	7.439590
5.708999	460.193731	7.444595
6.036760	451.537960	7.449600
6.050381	452.025897	7.454605
6.214298	447.184053	7.459610
5.811103	435.369271	7.464614
6.253836	423.459472	7.469619
5.829410	430.073309	7.474624
6.084918	423.212102	7.479629
6.061052	418.831673	7.484634
5.720660	425.612104	7.489638
6.160123	422.810506	7.494643
6.093455	427.683770	7.499648
5.689177	418.468888	7.504653
6.065330	417.650781	7.509658
5.780458	422.428690	7.514662
6.007965	416.135732	7.519667
5.801689	425.483708	7.524672
5.572530	419.018605	7.529677
6.142459	421.439331	7.534682
5.957038	419.319798	7.539686
6.053621	426.391482	7.544691
5.789086	420.164918	7.549696
5.903111	411.034978	7.554701
6.039247	412.497319	7.559706
5.601328	403.449064	7.564710
5.831132	391.758402	7.569715
5.918758	393.550068	7.574720
5.675951	396.260595	7.579725
5.949242	380.667700	7.584730
5.419259	398.001371	7.589734
5.740596	401.314327	7.594739
5.993014	412.235186	7.599744
5.737029	423.089795	7.604749
5.928357	422.086326	7.609754
5.934957	422.030584	7.614758
5.793049	407.661882	7.619763
5.755914	395.586975	7.624768
5.792970	396.353797	7.629773
5.670070	387.694233	7.634778
5.645742	415.326298	7.639782
5.783463	405.440967	7.644787
6.124365	421.927193	7.649792
5.483645	419.162669	7.654797
6.344388	419.343835	7.659802
5.848201	411.349761	7.664806
5.815273	399.290924	7.669811
5.759638	400.548338	7.674816
5.642976	392.341805	7.679821
5.648123	397.043281	7.684826
5.507400	411.234418	7.689830
5.711951	417.354555	7.694835
5.861839	424.180969	7.699840
6.101796	425.544949	7.704845
6.128938	414.813463	7.709850
5.519200	409.521047	7.714854
5.714191	401.369465	7.719859
5.605983	398.887619	7.724864
5.844222	412.758440	7.729869
5.820334	415.439685	7.734874
5.766569	413.864228	7.739878
5.828512	421.338313	7.744883
5.841135	426.534263	7.749888
5.735106	431.294090	7.754893
5.918658	430.569368	7.759898
5.855457	429.551769	7.764902
5.776492	425.576945	7.769907
5.681434	424.258574	7.774912
5.734565	431.983956	7.779917
5.808380	431.375156	7.784922
5.955510	422.889535	7.789926
6.151143	418.240158	7.794931
5.814834	404.774617	7.799936
5.674243	398.955481	7.804941
5.745214	381.247426	7.809946
5.611414	396.772177	7.814950
5.893877	404.027260	7.819955
5.838793	414.674024	7.824960
5.710365	408.958832	7.829965
6.024371	412.196245	7.834970
5.692293	413.411205	7.839974
5.512836	400.657039	7.844979
5.962727	421.035949	7.849984
6.093991	421.254108	7.854989
6.202610	393.473671	7.859994
5.836789	395.327290	7.864998
5.945756	385.872799	7.870003
6.003246	394.022104	7.875008
5.449466	400.442138	7.880013
5.545643	390.873736	7.885018
6.106806	387.084971	7.890022
5.970491	384.371588	7.895027
5.910691	372.767756	7.900032
5.491639	389.454071	7.905037
5.435853	389.342196	7.910042
5.441890	398.126202	7.915046
6.002474	416.941174	7.920051
6.071464	412.139984	7.925056
6.091863	398.844854	7.930061
6.004808	392.110854	7.935066
5.861535	395.786186	7.940070
5.787304	398.699181	7.945075
5.768637	389.954999	7.950080
5.695189	385.929737	7.955085
6.003677	387.623714	7.960090
5.833886	397.608133	7.965094
5.680803	393.781010	7.970099
5.726217	395.305790	7.975104
5.500686	393.249366	7.980109
5.904699	387.603547	7.985114
5.870735	395.006931	7.990118
5.920201	385.788399	7.995136
5.837203	384.107094	8.000154
5.750582	398.113925	8.005171
6.166889	372.304010	8.010189
5.828391	388.997139	8.015206
5.745792	385.755282	8.020224
6.064739	383.164133	8.025242
5.524644	390.422556	8.030259
5.891013	382.588378	8.035277
5.791926	395.404869	8.040294
5.799916	390.996286	8.045312
5.710380	391.890831	8.050330
5.616356	388.749091	8.055347
5.729039	385.068315	8.060365
5.551023	394.770458	8.065382
5.812951	416.104521	8.070400
5.924128	419.167277	8.075418
6.028012	419.257498	8.080435
6.100935	417.495553	8.085453
5.714674	407.757317	8.090470
5.989454	404.518644	8.095488
6.056077	393.498358	8.100506
5.993129	405.420153	8.105523
5.986614	392.073852	8.110541
5.838114	394.024165	8.115558
5.875986	390.871917	8.120576
5.986662	381.626240	8.125594
5.795069	391.822326	8.130611
5.712504	386.934747	8.135629
5.969145	407.354603	8.140646
6.067855	411.140821	8.145664
6.061904	420.524642	8.150682
5.875299	419.973841	8.155699
5.951488	414.539440	8.160717
5.937472	416.699861	8.165734
6.020658	422.017264	8.170752
6.133290	410.765323	8.175770
5.911727	420.155655	8.180787
6.053153	417.225931	8.185805
6.038058	419.748507	8.190822
6.176675	422.348870	8.195840
5.899291	400.307430	8.200858
5.465760	400.998942	8.205875
6.090430	407.515784	8.210893
6.041945	416.328575	8.215910
6.001297	415.497040	8.220928
6.190207	414.561802	8.225946
6.008842	418.184359	8.230963
5.987624	417.871594	8.235981
6.356786	416.324754	8.240998
6.095475	415.505490	8.246016
6.441266	418.773124	8.251034
5.961358	403.679288	8.256051
5.876972	388.165425	8.261069
5.948595	398.572464	8.266086
6.122013	421.429572	8.271104
6.071004	418.447984	8.276122
6.068367	423.448188	8.281139
5.932227	411.133366	8.286157
6.131205	422.034362	8.291174
5.870543	421.187630	8.296192
6.070387	416.754039	8.301210
6.120506	419.903316	8.306227
6.125610	419.548581	8.311245
5.934560	416.489886	8.316262
5.996327	410.915377	8.321280
6.374273	416.775462	8.326298
5.879094	430.876018	8.331315
6.071994	424.532924	8.336333
6.048313	421.897351	8.341350
5.720303	415.050546	8.346368
6.172686	423.499994	8.351386
6.287236	423.684300	8.356403
6.325846	419.412339	8.361421
5.990347	414.668951	8.366438
6.172096	423.310812	8.371456
6.553812	413.579158	8.376474
6.182383	412.599671	8.381491
6.083098	421.572864	8.386509
6.121720	424.612449	8.391526
6.187706	425.712619	8.396544
6.306683	420.463607	8.401562
6.174932	424.446586	8.406579
6.062810	427.054182	8.411597
6.249101	424.031771	8.416614
6.165029	416.647808	8.421632
6.207224	417.142932	8.426650
6.185447	418.952116	8.431667
5.833888	423.564689	8.436685
6.349991	423.113008	8.441702
6.388919	430.152183	8.446720
6.462219	423.039473	8.451738
6.294364	421.807663	8.456755
6.082186	416.341280	8.461773
6.430625	422.608598	8.466790
6.351088	429.068700	8.471808
6.502567	411.862999	8.476826
6.485993	425.230512	8.481843
6.342390	424.224374	8.486861
6.490029	426.859653	8.491878
6.442303	425.597442	8.496896
6.521078	424.531311	8.501914
6.270147	428.699441	8.506931
5.959121	410.461665	8.511949
6.146174	423.494962	8.516966
6.059544	420.943273	8.521984
6.327179	418.332303	8.527002
6.208947	441.351492	8.532019
6.501452	444.083942	8.537037
6.664703	436.134300	8.542054
6.395338	436.999295	8.547072
6.420950	434.892290	8.552090
6.100271	422.355400	8.557107
6.528688	431.421380	8.562125
6.516691	433.073835	8.567143
6.347005	436.210050	8.572160
6.568813	423.357219	8.577178
6.039117	420.275687	8.582195
6.393976	434.026506	8.587213
6.450367	438.509271	8.592231
6.353601	439.841398	8.597248
6.368213	437.827749	8.602266
6.370372	439.065881	8.607283
6.466526	440.351573	8.612301
6.922980	434.029424	8.617319
6.287012	446.952323	8.622336
6.397690	450.453515	8.627354
6.527602	439.473263	8.632371
6.519438	445.834508	8.637389
6.486467	436.558940	8.642407
6.393488	453.187511	8.647424
6.529748	441.830644	8.652442
6.552950	451.025009	8.657459
6.645078	449.486422	8.662477
6.797990	442.540375	8.667495
6.526804	446.481582	8.672512
6.577992	440.363987	8.677530
6.473307	437.758214	8.682547
6.437668	436.986469	8.687565
6.483900	435.826937	8.692583
6.633158	449.714692	8.697600
6.692330	445.203107	8.702618
6.364958	446.949517	8.707635
6.717375	454.521781	8.712653
6.638566	440.117864	8.717671
6.374206	445.510760	8.722688
6.559446	448.225808	8.727706
6.583015	455.268926	8.732723
6.364533	449.474475	8.737741
6.436307	449.771984	8.742759
6.355588	450.693213	8.747776
6.604783	454.986862	8.752794
6.811443	454.249638	8.757811
6.381735	443.728710	8.762829
6.727525	449.228436	8.767847
6.737771	444.270693	8.772864
6.787595	440.855054	8.777882
6.637610	445.375078	8.782899
6.847579	450.459821	8.787917
6.788910	444.743325	8.792935
6.689246	448.552291	8.797952
6.758926	445.649447	8.802970
6.418996	447.301300	8.807987
6.433573	447.572297	8.813005
6.380967	435.537442	8.818023
6.586638	443.627946	8.823040
6.843653	448.503902	8.828058
6.933529	445.597701	8.833075
6.389723	437.441598	8.838093
6.583723	450.148793	8.843111
6.735412	449.517155	8.848128
6.798710	441.623293	8.853146
6.472532	442.834710	8.858163
6.405138	440.458347	8.863181
6.893830	451.262589	8.868199
6.562555	442.668436	8.873216
6.600591	449.465271	8.878234
6.673601	456.496038	8.883251
6.889363	455.035711	8.888269
6.570140	451.446394	8.893287
6.643091	457.291843	8.898304
6.921506	480.100092	8.903322
6.995273	469.411017	8.908339
6.781214	470.616790	8.913357
7.205065	455.052235	8.918375
6.905269	452.623760	8.923392
6.803350	452.518880	8.928410
6.846273	444.900427	8.933427
6.183251	443.678291	8.938445
6.576302	462.029269	8.943463
6.657829	474.958902	8.948480
7.039883	484.795743	8.953498
7.220036	475.139283	8.958515
7.196435	480.987602	8.963533
6.995786	464.106296	8.968551
7.007632	450.029989	8.973568
6.657254	462.094281	8.978586
6.805499	451.063536	8.983603
6.729988	465.765961	8.988621
7.052906	479.788446	8.993639
6.924288	482.528703	8.998656
6.986669	469.012630	9.003674
7.092664	467.179637	9.008691
6.727314	470.374954	9.013709
6.946347	460.132957	9.018727
7.162382	460.171666	9.023744
7.097547	464.752928	9.028762
6.832731	446.932390	9.033779
6.568012	457.649290	9.038797
7.279946	458.481871	9.043815
6.954279	467.523820	9.048832
7.098929	453.974599	9.053850
7.016742	446.282067	9.058867
6.544386	449.065677	9.063885
6.904166	454.086351	9.068903
6.678659	474.232926	9.073920
6.949066	466.147750	9.078938
7.072283	470.729249	9.083955
7.047825	471.501967	9.088973
7.347141	481.764924	9.093991
7.210785	485.075317	9.099008
6.804800	486.414362	9.104026
7.214474	474.481952	9.109043
7.179380	483.401799	9.114061
6.958713	474.223740	9.119079
6.956749	483.301845	9.124096
6.826564	472.482509	9.129114
7.128789	473.237340	9.134131
7.125259	482.778066	9.139149
7.606219	471.198738	9.144167
7.106799	485.664781	9.149184
6.992087	486.139340	9.154202
7.530965	475.407001	9.159219
7.115796	463.888847	9.164237
7.276455	452.536774	9.169255
7.027927	448.918780	9.174272
6.807367	450.414583	9.179290
7.110002	462.341593	9.184307
6.822911	482.096087	9.189325
7.078162	469.565584	9.194343
7.206075	479.462380	9.199360
7.346285	475.827396	9.204378
7.436079	482.924670	9.209395
7.435928	475.870007	9.214413
7.541119	466.970831	9.219431
7.252792	452.899537	9.224448
7.183516	455.606110	9.229466
7.193454	453.344635	9.234483
7.122168	453.039208	9.239501
7.057020	443.753237	9.244519
7.258561	450.135133	9.249536
6.910136	467.206538	9.254554
7.341611	462.399028	9.259571
7.154980	479.096732	9.264589
7.180652	478.811798	9.269607
7.344918	477.610598	9.274624
7.397947	477.627390	9.279642
7.903817	475.156717	9.284659
7.267443	457.776044	9.289677
7.379709	448.354291	9.294695
7.540504	454.643562	9.299712
7.053988	459.437421	9.304730
7.203720	441.693443	9.309747
6.939604	454.045331	9.314765
6.950897	454.830608	9.319783
7.137159	472.250702	9.324800
7.267390	484.691580	9.329818
7.249136	472.239605	9.334835
7.188019	489.035147	9.339853
7.139853	483.658987	9.344871
7.452288	478.825201	9.349888
7.388015	490.204020	9.354906
7.555299	481.243731	9.359923
7.471625	486.002919	9.364941
7.457751	477.751427	9.369959
7.717404	478.313154	9.374976
7.262360	488.010030	9.379994
7.615518	481.711921	9.385011
7.151376	485.432674	9.390029
7.239585	477.722433	9.395047
7.306961	476.078518	9.400064
7.090473	492.758761	9.405082
7.437178	471.378182	9.410099
7.227196	480.111170	9.415117
7.348445	478.432909	9.420135
7.515772	477.692774	9.425152
7.288375	489.865571	9.430170
7.348360	474.243379	9.435187
7.026352	479.653349	9.440205
7.132513	474.062580	9.445223
7.438491	495.267787	9.450240
6.853810	507.927509	9.455258
7.198842	511.391335	9.460275
7.606865	507.060308	9.465293
7.634542	518.397489	9.470311
7.654414	513.514101	9.475328
7.717841	513.712024	9.480346
7.787340	516.182959	9.485363
7.719802	511.792407	9.490381
7.604631	516.787136	9.495399
7.789010	511.245552	9.500416
7.690594	511.251694	9.505434
7.809452	489.293463	9.510451
7.637174	489.661655	9.515469
7.186158	475.726036	9.520487
7.422349	479.646098	9.525504
7.568195	504.761065	9.530522
7.631629	509.409004	9.535539
7.907744	512.437867	9.540557
7.761053	501.766125	9.545575
7.551366	488.061420	9.550592
7.166709	496.285703	9.555610
7.529626	506.116684	9.560627
7.614071	507.614939	9.565645
7.314416	517.401546	9.570663
7.654514	522.923897	9.575680
7.555626	513.764940	9.580698
7.585667	507.178038	9.585715
7.614442	505.697414	9.590733
7.485818	526.932781	9.595751
7.768233	514.678609	9.600768
7.624132	521.117790	9.605786
7.528271	518.208593	9.610803
7.567885	520.383931	9.615821
7.495539	519.453730	9.620839
7.382956	499.493241	9.625856
7.033213	518.241156	9.630874
7.482551	522.385227	9.635891
7.806840	541.023887	9.640909
7.869077	540.474431	9.645927
8.056570	549.658474	9.650944
7.973896	548.758726	9.655962
7.888783	537.214195	9.660979
7.584253	537.494932	9.665997
7.664737	556.467616	9.671015
8.009293	547.268981	9.676032
7.774865	548.739345	9.681050
7.883095	546.388690	9.686067
8.148343	546.760923	9.691085
7.684905	534.753142	9.696103
7.916850	524.072182	9.701120
7.805139	531.154946	9.706138
7.594812	525.113067	9.711155
7.962689	535.078467	9.716173
7.968247	537.860599	9.721191
8.095026	532.583482	9.726208
8.032466	520.013253	9.731226
7.953716	512.213040	9.736243
7.984932	510.221226	9.741261
7.762268	512.353158	9.746279
7.910578	512.061814	9.751296
7.827563	517.735983	9.756314
7.617407	509.522611	9.761331
7.861688	526.682355	9.766349
7.889399	542.111531	9.771367
8.288781	538.446641	9.776384
7.939444	528.530551	9.781402
8.113158	530.544635	9.786419
8.166828	521.302052	9.791437
8.109487	511.979903	9.796455
7.986774	513.739543	9.801472
7.798536	514.068463	9.806490
7.687036	509.038030	9.811507
7.778614	519.807747	9.816525
7.987280	542.486159	9.821543
7.837008	541.383098	9.826560
7.610936	549.635966	9.831578
7.800667	544.909555	9.836595
8.000302	548.761899	9.841613
7.979058	550.719816	9.846631
8.327037	540.159901	9.851648
8.125473	544.423981	9.856666
8.025437	542.104008	9.861683
8.105427	537.603108	9.866701
8.049021	546.624163	9.871719
8.327628	541.734764	9.876736
8.196479	547.034102	9.881754
8.139675	551.240463	9.886771
7.975128	554.554966	9.891789
7.979883	556.640638	9.896807
8.114357	539.705318	9.901824
8.128754	549.491707	9.906842
8.171491	549.166537	9.911859
8.273622	539.166540	9.916877
8.189624	546.647427	9.921895
8.165265	545.995445	9.926912
8.334724	546.488316	9.931930
8.317304	541.058408	9.936947
8.160607	540.446926	9.941965
7.995170	551.166678	9.946983
8.490897	544.625966	9.952000
7.962155	549.335147	9.957018
8.198705	541.876769	9.962035
8.513025	545.663399	9.967053
7.970880	549.963228	9.972071
8.182806	538.381526	9.977088
7.972057	547.956933	9.982106
8.001492	551.531687	9.987123
8.417718	544.974075	9.992141
7.980209	544.035088	9.997159
8.208024	551.404900	10.002176
7.976802	550.886508	10.007194
7.977942	554.624811	10.012211
7.808945	550.979007	10.017229
8.324887	569.582499	10.022247
8.548154	555.477842	10.027264
8.607702	553.585242	10.032282
8.244202	555.885263	10.037299
8.300808	554.625580	10.042317
7.952638	547.403553	10.047335
8.400474	565.298734	10.052352
8.499376	585.688948	10.057370
8.322719	561.775367	10.062387
8.559017	555.336824	10.067405
8.457108	548.842304	10.072423
8.044237	552.961800	10.077440
8.591351	560.989706	10.082458
8.502304	561.778872	10.087475
8.269351	547.627625	10.092493
8.053843	551.029135	10.097511
8.368636	568.122485	10.102528
8.388288	568.990427	10.107546
8.218552	574.112541	10.112563
8.767955	565.604000	10.117581
8.295826	581.105275	10.122599
8.477025	576.559196	10.127616
8.282693	573.371499	10.132634
8.559328	576.888438	10.137651
8.845018	579.434659	10.142669
8.801833	582.127862	10.147687
8.606965	572.102020	10.152704
8.436118	548.948850	10.157722
8.148336	559.228548	10.162739
8.506366	556.388374	10.167757
8.520207	563.192036	10.172775
8.659210	571.267312	10.177792
8.383085	579.821406	10.182810
8.663147	581.014930	10.187827
9.077303	569.946200	10.192845
8.861764	574.348034	10.197863
8.558790	552.188987	10.202880
8.406163	546.687071	10.207898
8.277528	551.682867	10.212915
8.581560	557.990493	10.217933
8.534329	569.045698	10.222951
8.871988	577.309592	10.227968
8.827841	579.867532	10.232986
8.301057	565.353528	10.238003
8.548621	558.099003	10.243021
8.517168	569.470064	10.248039
8.562694	566.193683	10.253056
8.626975	581.032220	10.258074
8.517974	575.721845	10.263091
8.464054	574.601782	10.268109
8.541220	574.699005	10.273127
8.648451	575.774812	10.278144
8.569416	571.593422	10.283162
8.496793	570.445565	10.288179
8.653250	577.252691	10.293197
8.529656	582.260060	10.298215
8.725052	578.513132	10.303232
8.806267	570.244406	10.308250
8.793583	581.224001	10.313267
8.648610	574.003419	10.318285
8.679811	576.815742	10.323303
8.204037	582.859132	10.328320
8.900516	569.509204	10.333338
8.409427	575.491559	10.338355
8.697106	590.003427	10.343373
8.529385	613.744033	10.348391
8.506254	616.011500	10.353408
8.831801	611.394768	10.358426
8.597625	615.349745	10.363443
8.787864	610.175037	10.368461
8.852073	615.242729	10.373479
8.678655	610.326878	10.378496
8.769888	608.870898	10.383514
8.560389	612.408026	10.388531
8.914908	610.744713	10.393549
8.826507	613.741674	10.398567
8.675782	609.818824	10.403584
8.836247	611.190289	10.408602
9.049582	621.378662	10.413619
8.834470	616.528002	10.418637
8.802899	611.822807	10.423655
8.888758	614.685693	10.428672
8.913831	610.846605	10.433690
8.661528	611.352501	10.438707
9.090822	623.560921	10.443725
9.313050	636.528320	10.448743
8.937946	629.956155	10.453760
8.931727	611.379703	10.458778
8.903754	620.663377	10.463795
9.054397	627.038059	10.468813
9.287744	620.927907	10.473831
9.018266	616.222495	10.478848
9.119540	618.038017	10.483866
8.809390	610.895068	10.488883
9.004755	608.790530	10.493901
9.064141	605.867321	10.498919
8.908852	612.366270	10.503936
9.498436	607.680455	10.508954
8.951644	611.368128	10.513971
9.029852	608.293377	10.518989
8.919213	614.067834	10.524007
8.952710	608.939651	10.529024
9.066598	631.800667	10.534042
9.031338	647.664594	10.539059
9.425273	639.187761	10.544077
9.170757	636.035249	10.549095
8.698317	625.551022	10.554112
9.197983	634.717474	10.559130
9.088702	642.579353	10.564147
9.202942	644.510431	10.569165
9.265526	641.523107	10.574183
9.092322	643.931262	10.579200
9.487506	636.748613	10.584218
9.468825	644.385606	10.589235
9.266565	622.610475	10.594253
9.273460	625.598094	10.599271
9.137975	629.179021	10.604288
9.389733	618.122488	10.609306
9.152825	622.391677	10.614323
9.398863	620.319656	10.619341
9.141113	617.286377	10.624359
9.340302	622.135586	10.629376
9.385413	621.400800	10.634394
8.897248	620.082266	10.639411
9.382282	628.470892	10.644429
9.424762	639.372269	10.649447
9.361667	639.722710	10.654464
9.434392	633.163697	10.659482
9.118328	630.199750	10.664499
9.321852	635.491713	10.669517
9.318854	644.543708	10.674535
9.310318	648.601925	10.679552
9.273004	635.386509	10.684570
9.204321	656.316247	10.689587
9.418762	647.298815	10.694605
9.711232	639.575603	10.699623
9.502959	642.528326	10.704640
9.307249	639.513862	10.709658
9.342666	653.148696	10.714675
9.232367	651.078819	10.719693
9.498429	639.065241	10.724711
9.749892	643.116654	10.729728
9.702367	639.317184	10.734746
9.213729	639.350986	10.739763
9.293648	642.289662	10.744781
9.424811	645.351306	10.749799
9.325246	646.778004	10.754816
9.686990	649.468079	10.759834
9.549954	638.826524	10.764851
9.373477	639.500119	10.769869
9.709005	640.477949	10.774887
9.174071	639.902564	10.779904
9.362976	636.748782	10.784922
9.404149	641.981125	10.789939
9.325673	645.239218	10.794957
9.374173	646.381482	10.799975
9.316762	642.262418	10.804992
9.533495	643.796764	10.810010
9.051532	651.564897	10.815027
9.151224	640.162000	10.820045
9.557070	659.852324	10.825063
9.588643	673.892312	10.830080
10.076108	677.327384	10.835098
9.460315	657.116107	10.840115
9.536833	676.362411	10.845133
9.817178	669.162225	10.850151
9.747139	686.089374	10.855168
9.618512	668.763032	10.860186
9.545358	670.330803	10.865203
9.950689	678.054409	10.870221
9.763322	659.848535	10.875239
9.630236	659.476806	10.880256
9.711045	646.087428	10.885274
9.735192	655.442768	10.890291
9.572652	655.078298	10.895309
9.936061	664.488857	10.900327
9.788859	669.250000	10.905344
10.199634	659.801530	10.910362
9.581782	644.941001	10.915379
9.551813	645.776647	10.920397
9.691673	643.311870	10.925415
9.456295	665.979041	10.930432
9.991717	663.998666	10.935450
9.918793	668.724433	10.940467
9.846468	675.409602	10.945485
10.340910	664.768766	10.950503
9.719344	673.383479	10.955520
9.731221	642.367896	10.960538
9.819707	662.603654	10.965555
9.714010	664.397093	10.970573
10.042446	664.330118	10.975591
10.017730	670.591065	10.980608
10.312339	659.628553	10.985626
9.880125	651.934657	10.990643
9.655866	649.468793	10.995661
9.452944	645.271167	11.000679
9.826180	671.026705	11.005696
10.185089	675.782262	11.010714
9.908364	676.636879	11.015731
9.983225	675.765856	11.020749
9.797745	674.779653	11.025767
9.630450	678.114126	11.030784
10.146790	678.593434	11.035802
9.919502	678.166896	11.040819
9.630640	682.431352	11.045837
9.792692	677.575457	11.050855
9.701959	684.106025	11.055872
10.188586	676.060582	11.060890
10.062782	676.447036	11.065907
10.052431	687.716257	11.070925
9.942654	674.656346	11.075943
9.833689	681.399967	11.080960
9.586142	683.940753	11.085978
9.722877	682.386068	11.090995
10.073751	697.722906	11.096013
10.488896	699.183139	11.101031
10.165242	692.099085	11.106048
10.073860	680.489943	11.111066
10.154291	683.609040	11.116083
9.865255	682.080839	11.121101
9.978745	693.436362	11.126119
9.751333	704.352727	11.131136
10.231954	707.639151	11.136154
10.308581	717.795984	11.141171
10.306726	718.104556	11.146189
10.350718	707.273820	11.151207
10.501943	712.130833	11.156224
10.366673	702.636891	11.161242
10.646805	688.111274	11.166259
10.550507	684.905290	11.171277
10.467002	673.471996	11.176295
10.030935	681.177992	11.181312
9.906513	674.370846	11.186330
10.052836	671.356409	11.191347
9.701667	671.542939	11.196365
10.687171	691.347173	11.201383
10.422435	706.225362	11.206400
10.183208	698.071442	11.211418
10.217241	692.130603	11.216435
10.191131	704.010679	11.221453
10.376800	692.376145	11.226471
10.352545	704.632264	11.231488
10.213661	709.856767	11.236506
10.238835	708.733193	11.241523
10.379167	712.564531	11.246541
10.472768	696.049190	11.251559
10.280398	709.326493	11.256576
10.499545	704.974448	11.261594
10.568970	709.152784	11.266611
10.488667	714.539586	11.271629
10.258522	716.528311	11.276647
10.501453	717.891000	11.281664
10.095525	707.341137	11.286682
10.417047	713.925427	11.291699
10.267223	714.052901	11.296717
10.288484	704.835476	11.301735
10.366137	703.239236	11.306752
10.382562	713.459612	11.311770
10.444258	701.301228	11.316787
10.350863	707.084270	11.321805
10.502141	702.298658	11.326823
10.332700	701.871164	11.331840
10.355034	713.336926	11.336858
10.629037	716.065414	11.341875
10.453113	740.758692	11.346893
10.836752	735.139226	11.351911
10.833527	734.973650	11.356928
10.579636	727.681934	11.361946
10.635899	718.656504	11.366963
10.509913	710.394588	11.371981
10.968524	711.017538	11.376999
10.596193	711.393006	11.382016
10.634116	706.569938	11.387034
10.679605	699.206821	11.392051
10.475093	718.770344	11.397069
10.529291	713.191867	11.402087
10.638603	736.613994	11.407104
10.362971	742.503910	11.412122
10.757301	741.401250	11.417139
10.724842	747.283816	11.422157
11.006305	731.380080	11.427175
10.856639	750.709345	11.432192
10.937688	741.419564	11.437210
10.908199	733.558102	11.442227
10.425444	737.422352	11.447245
11.193227	740.349458	11.452263
11.118091	721.015092	11.457280
10.712244	720.220229	11.462298
10.705592	705.168487	11.467315
10.577650	712.300288	11.472333
10.738184	720.581103	11.477351
10.904077	735.405457	11.482368
10.677238	746.088702	11.487386
10.735089	738.163708	11.492403
10.953076	751.503930	11.497421
10.982988	736.828140	11.502439
11.208637	742.066465	11.507456
10.969060	739.859808	11.512474
11.009728	711.754650	11.517491
10.825227	716.933395	11.522509
10.989506	719.541156	11.527527
10.952981	715.330418	11.532544
10.741914	721.558192	11.537562
11.430906	711.918377	11.542579
10.937904	721.105995	11.547597
11.147699	710.846080	11.552615
10.998741	711.571792	11.557632
10.638745	708.238387	11.562650
10.958782	710.380721	11.567667
10.914415	743.548185	11.572685
11.166194	743.617369	11.577703
10.975222	732.467034	11.582720
10.955072	741.052678	11.587738
11.385192	742.456887	11.592755
11.256142	739.791928	11.597773
11.150188	727.949953	11.602791
11.233043	714.011001	11.607808
10.839861	710.599063	11.612826
11.187821	713.461901	11.617843
11.281660	737.063360	11.622861
10.985000	715.211867	11.627879
11.179616	726.674984	11.632896
10.919610	726.417651	11.637914
11.160739	740.392751	11.642931
11.385450	741.634660	11.647949
11.080084	745.722165	11.652967
11.277071	748.174505	11.657984
11.169647	743.978300	11.663002
11.302738	747.626611	11.668019
10.943094	746.307568	11.673037
11.438078	743.773314	11.678055
11.249300	745.552228	11.683072
11.090737	740.752952	11.688090
11.188270	738.994950	11.693107
11.209800	739.250033	11.698125
10.851663	740.109525	11.703143
11.004150	741.142194	11.708160
10.875511	734.350486	11.713178
10.937488	741.844995	11.718195
11.109774	737.739297	11.723213
11.361599	754.632312	11.728231
11.474366	765.170740	11.733248
11.136823	756.180631	11.738266
11.372543	769.427769	11.743283
11.167379	774.997541	11.748301
11.291915	777.904418	11.753319
11.642644	764.461804	11.758336
11.372304	769.980207	11.763354
11.442388	769.018049	11.768371
11.546673	768.823777	11.773389
11.293771	778.836618	11.778407
11.676470	762.530813	11.783424
11.534378	784.089615	11.788442
11.520232	773.697995	11.793459
11.535937	773.854250	11.798477
11.451737	768.891631	11.803495
11.874048	774.160660	11.808512
11.735551	764.454632	11.813530
11.713801	748.054859	11.818547
11.520129	740.037823	11.823565
11.340484	752.201707	11.828583
11.613026	740.891452	11.833600
11.325234	754.049033	11.838618
11.655914	760.784764	11.843635
11.593106	773.129230	11.848653
11.678385	768.265793	11.853671
11.941185	769.167931	11.858688
11.330994	756.077752	11.863706
11.678140	749.975797	11.868723
12.088948	765.024609	11.873741
11.771071	752.689727	11.878759
11.511551	737.670931	11.883776
11.158308	747.369745	11.888794
11.470390	754.874850	11.893811
11.729775	764.455901	11.898829
11.534095	776.691756	11.903847
11.707332	769.552827	11.908864
11.967831	762.148430	11.913882
11.683478	767.544760	11.918899
11.811021	771.313282	11.923917
11.559722	774.116500	11.928935
11.782722	774.445765	11.933952
11.943261	773.479595	11.938970
12.006856	770.873744	11.943987
11.868251	767.068714	11.949005
11.626811	771.188509	11.954023
12.011685	764.338596	11.959040
11.792127	775.461171	11.964058
11.747508	768.214961	11.969075
11.802137	772.501672	11.974093
11.397814	769.077794	11.979111
11.749727	772.964917	11.984128
11.337606	774.981535	11.989146
11.545626	774.103135	11.994163
11.863938	779.817771	11.999181
12.023424	795.107782	12.004199
12.120742	803.875694	12.009216
12.065472	802.569040	12.014234
11.983213	798.169438	12.019251
12.112372	801.084212	12.024269
12.019174	798.279237	12.029287
11.954113	773.879881	12.034304
11.916695	791.737291	12.039322
11.957679	794.388589	12.044339
12.416152	799.687243	12.049357
11.713370	801.308900	12.054375
12.066857	803.130551	12.059392
12.086037	802.483526	12.064410
12.201280	807.996901	12.069427
12.272330	804.933537	12.074445
11.959841	812.800934	12.079463
12.217449	804.996235	12.084480
12.004328	810.191382	12.089498
12.121398	809.748937	12.094515
12.138952	802.641579	12.099533
12.018421	804.598710	12.104551
12.093518	796.995798	12.109568
12.135364	802.802652	12.114586
11.935064	813.432322	12.119603
12.123690	808.155855	12.124621
12.017749	803.623582	12.129639
12.287455	799.800080	12.134656
12.089253	799.600972	12.139674
11.767273	810.375661	12.144691
11.991505	800.551447	12.149709
11.958272	809.837289	12.154727
12.437087	812.681742	12.159744
12.542403	811.564523	12.164762
12.367800	815.767506	12.169779
12.366105	796.709796	12.174797
11.992081	819.725413	12.179815
12.422108	807.250227	12.184832
12.339668	805.038306	12.189850
12.489707	825.080002	12.194867
12.649482	817.304157	12.199885
12.280536	814.457224	12.204903
12.283312	802.649871	12.209920
12.277210	812.261105	12.214938
12.380192	824.241855	12.219955
12.607044	834.991078	12.224973
12.342061	828.566458	12.229991
12.710427	828.243649	12.235008
12.712660	836.063863	12.240026
12.632950	821.746350	12.245043
12.737290	817.007478	12.250061
12.170759	808.836648	12.255079
12.379331	802.024290	12.260096
12.207729	815.384839	12.265114
12.748491	829.230496	12.270131
12.977421	833.645132	12.275149
12.798897	827.533679	12.280167
12.490184	812.467676	12.285184
12.527916	807.934354	12.290202
12.354482	819.291404	12.295219
12.921401	820.914599	12.300237
12.655960	817.096979	12.305255
13.002755	806.748878	12.310272
12.876098	814.799940	12.315290
12.542784	802.903973	12.320307
12.927490	802.684741	12.325325
12.447228	808.819902	12.330343
12.537626	801.938609	12.335360
12.725484	803.244913	12.340378
12.534118	796.512813	12.345395
12.799206	813.073394	12.350413
12.585788	830.191452	12.355431
12.719870	819.272833	12.360448
12.750658	829.085412	12.365466
12.662684	835.257340	12.370483
12.972451	829.698934	12.375501
12.699275	838.238113	12.380519
12.636204	843.331563	12.385536
12.729342	840.585759	12.390554
12.586148	846.281861	12.395571
12.822586	834.857665	12.400589
12.487813	837.603513	12.405607
12.510686	828.493024	12.410624
12.694379	826.547473	12.415642
12.761845	829.552030	12.420659
12.904942	819.635785	12.425677
12.564016	838.396596	12.430695
12.974164	850.942806	12.435712
13.081767	858.152640	12.440730
12.846236	857.779432	12.445747
13.054142	871.100962	12.450765
13.098884	869.013945	12.455783
13.332269	869.229683	12.460800
13.133784	847.147327	12.465818
12.910455	843.902980	12.470835
12.957997	834.704926	12.475853
12.975266	849.064754	12.480871
13.220998	864.674730	12.485888
13.334512	850.499078	12.490906
13.077440	850.890821	12.495923
13.123931	829.262622	12.500941
12.753184	845.716735	12.505959
13.116699	855.932658	12.510976
13.127118	852.304988	12.515994
12.931586	871.645571	12.521011
13.243911	866.674881	12.526029
13.113715	860.007778	12.531047
12.978745	877.465976	12.536064
13.276390	868.283415	12.541082
13.205698	869.625220	12.546099
13.280716	860.549742	12.551117
13.088912	860.536172	12.556135
13.363003	868.555687	12.561152
13.251987	870.118749	12.566170
13.394965	866.438729	12.571187
13.189544	855.502899	12.576205
13.089547	861.087108	12.581223
13.037887	864.826389	12.586240
13.398790	865.615776	12.591258
12.892206	862.547239	12.596275
13.346022	858.013241	12.601293
13.263850	855.712690	12.606311
13.277215	861.326872	12.611328
13.323895	862.360603	12.616346
13.025197	875.464394	12.621363
13.339918	873.555716	12.626381
13.613452	893.256914	12.631399
13.658385	894.388175	12.636416
13.529899	878.117811	12.641434
13.256973	867.790007	12.646451
13.689784	875.004451	12.651469
13.663756	874.011021	12.656487
13.467481	869.614603	12.661504
13.905525	861.251570	12.666522
12.977903	862.500001	12.671539
13.387134	876.117972	12.676557
13.448166	887.277842	12.681575
13.830891	893.569967	12.686592
13.840155	885.954530	12.691610
13.588356	893.017832	12.696627
13.659148	876.003759	12.701645
13.411328	873.532327	12.706663
13.569936	892.385357	12.711680
13.769314	885.800855	12.716698
13.481267	896.469574	12.721715
13.810306	893.587312	12.726733
13.773193	896.958457	12.731751
13.662630	891.778146	12.736768
13.827546	891.513562	12.741786
13.717893	894.196805	12.746803
13.620182	884.524471	12.751821
13.852641	893.792183	12.756839
13.695707	889.070735	12.761856
14.133090	897.327674	12.766874
13.325321	895.144577	12.771891
13.624309	892.851527	12.776909
13.707892	894.385395	12.781927
13.744014	899.303723	12.786944
14.012846	893.301732	12.791962
13.759592	907.030242	12.796979
13.803282	894.427482	12.801997
13.759195	903.584878	12.807015
13.660583	903.882570	12.812032
14.087138	897.947662	12.817050
13.875210	894.956905	12.822067
13.731429	894.211380	12.827085
13.771839	897.094864	12.832103
13.088557	899.441986	12.837120
13.847877	895.446532	12.842138
13.930763	922.897111	12.847155
14.184883	927.712681	12.852173
14.371012	920.485128	12.857191
14.075861	912.913979	12.862208
14.448147	898.052001	12.867226
13.863324	893.364276	12.872243
13.960579	891.711809	12.877261
13.994193	890.549813	12.882279
13.788875	910.373931	12.887296
14.189628	929.828452	12.892314
13.844760	934.479036	12.897331
14.033542	929.606809	12.902349
14.440344	923.642500	12.907367
14.332359	916.149682	12.912384
14.438138	920.387186	12.917402
14.521915	928.001383	12.922419
14.327256	910.956595	12.927437
14.380559	893.985958	12.932455
14.267206	897.176086	12.937472
14.624230	889.184358	12.942490
14.317338	891.433485	12.947507
14.262779	890.003878	12.952525
14.108732	889.512801	12.957543
14.162243	893.264133	12.962560
14.344228	884.986167	12.967578
14.059909	892.874511	12.972595
14.223643	883.882692	12.977613
14.661453	896.275532	12.982631
14.012715	896.634746	12.987648
14.427604	891.804077	12.992666
14.414705	918.408416	12.997683
14.558709	923.373383	13.002701
14.647622	915.875787	13.007719
14.001782	898.777275	13.012736
14.235876	905.250006	13.017754
14.482030	920.224179	13.022771
14.402227	921.026196	13.027789
14.570417	917.394726	13.032807
14.221511	930.712409	13.037824
14.677053	916.557400	13.042842
14.760169	925.810981	13.047859
14.540760	926.823200	13.052877
14.834377	919.604551	13.057895
14.597392	933.223693	13.062912
14.770887	914.543388	13.067930
14.519783	925.649662	13.072947
14.551483	926.750844	13.077965
14.593085	925.916632	13.082983
14.649040	936.482533	13.088000
14.665939	921.761884	13.093018
14.533025	928.455068	13.098035
14.821365	919.032305	13.103053
14.853470	915.375426	13.108071
14.957828	927.503657	13.113088
14.907613	919.491815	13.118106
14.758111	924.225269	13.123123
14.904738	919.800579	13.128141
14.568695	908.208509	13.133159
14.674802	927.248644	13.138176
14.562544	923.360657	13.143194
14.396619	922.062150	13.148211
14.400923	929.294699	13.153229
14.887830	918.294531	13.158247
14.846327	931.504035	13.163264
14.606230	921.471902	13.168282
14.573070	921.722103	13.173299
14.993657	925.471086	13.178317
14.948302	915.512880	13.183335
14.683090	922.498115	13.188352
14.774696	918.569157	13.193370
14.839582	917.835006	13.198387
14.573580	917.729838	13.203405
14.891237	924.446153	13.208423
14.706910	932.542293	13.213440
15.173921	940.533322	13.218458
15.387994	930.491436	13.223475
14.931063	950.667647	13.228493
15.132739	942.834383	13.233511
15.014791	939.281571	13.238528
15.190076	932.869154	13.243546
15.115117	944.179614	13.248563
15.287727	943.733052	13.253581
15.212072	944.624139	13.258599
14.891986	935.946949	13.263616
15.299836	940.827517	13.268634
15.305749	939.565797	13.273651
15.097952	938.919488	13.278669
15.354588	934.826487	13.283687
15.144664	944.095325	13.288704
15.465259	940.305454	13.293722
15.045095	921.986401	13.298739
15.361458	929.070235	13.303757
15.468523	931.996580	13.308775
15.426570	942.063828	13.313792
15.162294	924.681797	13.318810
15.031366	921.989364	13.323827
15.050580	932.127930	13.328845
15.210669	936.310745	13.333863
14.905375	943.148329	13.338880
15.350779	940.212860	13.343898
15.311893	940.532907	13.348915
15.111650	940.872294	13.353933
15.130006	933.188004	13.358951
15.304092	941.022223	13.363968
15.291254	941.717052	13.368986
15.586941	941.563007	13.374003
15.129389	949.293176	13.379021
15.727181	943.357347	13.384039
15.359139	949.011336	13.389056
15.474359	967.631526	13.394074
15.612317	971.559381	13.399091
15.144853	968.172920	13.404109
15.609794	974.840367	13.409127
15.789780	972.142700	13.414144
15.616645	976.985605	13.419162
15.626046	969.483484	13.424179
15.195839	969.247744	13.429197
15.820937	977.396363	13.434215
16.071527	976.410095	13.439232
15.882092	964.833376	13.444250
15.704868	953.561705	13.449267
15.474396	967.827790	13.454285
15.729329	959.303814	13.459303
15.832016	968.545506	13.464320
15.503306	968.789719	13.469338
15.757322	968.028853	13.474355
15.604422	972.173549	13.479373
15.865992	963.791767	13.484391
15.872963	972.401375	13.489408
15.727143	973.467898	13.494426
16.053960	972.362272	13.499443
15.847608	963.470897	13.504461
15.536685	960.668620	13.509479
15.771774	966.275118	13.514496
15.622882	964.982831	13.519514
15.715091	962.054100	13.524531
15.509442	967.396080	13.529549
15.825178	963.956204	13.534567
15.839629	964.418952	13.539584
15.730165	961.397372	13.544602
15.773989	963.252799	13.549619
15.615733	982.204667	13.554637
16.119469	988.420026	13.559655
16.464981	1005.844564	13.564672
16.176070	989.450363	13.569690
16.380266	975.888624	13.574707
15.904372	977.303696	13.579725
16.030310	961.516122	13.584743
15.858244	966.651350	13.589760
15.781171	979.890822	13.594778
16.339209	993.713285	13.599795
16.101135	1011.847004	13.604813
16.249333	1000.261379	13.609831
16.476308	1000.315201	13.614848
16.330023	993.160583	13.619866
16.156000	977.992900	13.624883
16.385409	976.907402	13.629901
16.483792	981.198118	13.634919
16.101976	967.241300	13.639936
16.003320	966.328437	13.644954
16.338487	980.940254	13.649971
16.099779	995.255368	13.654989
16.080694	992.346705	13.660007
16.636528	991.341980	13.665024
16.429452	992.469077	13.670042
16.503576	994.630871	13.675059
16.395164	999.256737	13.680077
16.444039	990.272139	13.685095
16.312381	989.323030	13.690112
16.111365	996.886178	13.695130
16.710526	990.474538	13.700147
16.237899	1001.918066	13.705165
16.199945	992.539652	13.710183
16.403136	997.711329	13.715200
16.310541	1003.552220	13.720218
16.231254	993.690937	13.725235
16.323932	1004.393687	13.730253
16.540433	995.455628	13.735271
16.506670	996.618480	13.740288
16.481272	994.670265	13.745306
16.884525	989.310032	13.750323
16.460956	991.443928	13.755341
16.554062	993.211643	13.760359
16.673502	993.326250	13.765376
16.451710	997.945766	13.770394
16.734293	990.558061	13.775411
16.532062	998.687524	13.780429
16.528964	1017.771511	13.785447
16.648108	1028.534442	13.790464
16.561684	1026.936899	13.795482
16.629222	1030.472165	13.800499
16.304248	1027.602136	13.805517
16.710949	1024.986060	13.810535
16.567985	1021.087405	13.815552
16.786420	1028.022609	13.820570
17.077277	1016.704583	13.825587
16.841762	1017.573824	13.830605
17.148727	1027.109139	13.835623
17.109163	1024.313711	13.840640
17.084206	1033.488474	13.845658
17.357041	1030.354519	13.850675
17.043752	1034.000721	13.855693
16.990290	1028.995116	13.860711
17.314975	1023.794774	13.865728
17.071286	1033.542088	13.870746
17.219541	1017.727127	13.875763
16.926989	1002.385825	13.880781
16.984205	1004.031168	13.885799
17.078005	1005.384617	13.890816
17.354479	1004.704265	13.895834
17.439252	992.006413	13.900851
16.968873	996.535758	13.905869
16.884060	995.683581	13.910887
17.301151	993.900779	13.915904
17.319774	983.899613	13.920922
16.912501	996.080659	13.925939
16.976163	1000.388962	13.930957
17.419245	1017.235907	13.935975
17.312154	1018.902657	13.940992
17.056719	1020.949951	13.946010
16.955734	1022.608993	13.951027
17.337904	1029.752798	13.956045
17.092779	1027.333646	13.961063
17.633154	1023.939091	13.966080
17.223075	1032.720805	13.971098
17.458775	1036.129307	13.976115
17.424620	1028.962727	13.981133
17.187265	1026.245055	13.986151
17.440054	1025.433606	13.991168
17.148590	1032.985823	13.996186
17.527670	1023.138880	14.001203
17.213544	1040.165253	14.006221
17.061407	1026.259176	14.011239
17.202680	1029.309768	14.016256
17.072353	1031.761050	14.021274
17.479907	1029.130660	14.026291
17.528154	1034.484396	14.031309
17.554622	1032.356696	14.036327
17.671962	1020.675009	14.041344
17.315083	1027.259014	14.046362
17.551402	1021.441897	14.051379
17.549697	1027.579090	14.056397
17.828282	1035.494801	14.061415
17.730767	1033.488886	14.066432
17.396298	1035.123356	14.071450
17.627155	1037.263435	14.076467
17.506465	1046.149016	14.081485
17.722926	1057.352855	14.086503
18.035583	1050.297508	14.091520
18.054704	1060.259804	14.096538
18.288424	1047.227715	14.101555
18.021922	1033.529214	14.106573
17.938034	1022.033328	14.111591
17.992829	1022.883053	14.116608
17.777010	1021.001523	14.121626
17.801158	1024.301885	14.126643
17.981781	1026.060175	14.131661
17.570213	1028.493247	14.136679
17.955115	1021.617627	14.141696
17.801127	1026.770341	14.146714
17.950938	1021.348293	14.151731
17.498653	1023.002739	14.156749
17.626463	1021.911292	14.161767
17.500432	1026.139721	14.166784
17.858134	1050.276903	14.171802
18.145757	1046.092113	14.176819
18.045371	1044.293356	14.181837
17.977362	1054.316191	14.186855
18.063067	1051.362542	14.191872
17.906443	1053.177679	14.196890
17.787575	1052.290216	14.201907
17.923567	1049.957705	14.206925
17.744850	1057.199869	14.211943
18.128737	1054.412393	14.216960
17.926093	1050.097293	14.221978
17.979899	1045.754527	14.226995
17.987267	1044.837421	14.232013
18.032846	1069.850883	14.237031
18.449926	1081.156425	14.242048
18.474300	1078.697193	14.247066
18.527566	1072.940010	14.252083
18.455937	1055.299051	14.257101
18.108750	1057.395457	14.262119
18.463829	1045.669117	14.267136
18.439856	1064.189730	14.272154
18.070565	1054.835646	14.277171
18.298830	1055.486862	14.282189
18.113544	1069.812849	14.287207
18.621555	1078.486078	14.292224
18.417357	1077.481702	14.297242
18.026595	1081.854144	14.302259
18.295348	1085.224880	14.307277
18.021417	1082.145972	14.312295
18.317497	1081.402518	14.317312
18.319078	1079.374220	14.322330
18.250269	1083.596303	14.327347
18.514400	1076.121865	14.332365
18.419633	1086.207040	14.337383
18.325209	1080.792891	14.342400
18.455936	1093.768797	14.347418
18.533787	1104.627223	14.352435
18.871391	1115.873170	14.357453
18.694430	1115.033940	14.362471
19.165523	1106.338527	14.367488
18.899993	1094.035417	14.372506
18.530383	1077.194715	14.377523
18.692506	1075.110993	14.382541
18.587839	1090.316864	14.387559
18.656575	1096.500247	14.392576
18.661642	1105.762578	14.397594
18.563422	1108.650247	14.402611
18.808729	1102.923728	14.407629
18.903871	1111.488445	14.412647
18.873353	1102.316593	14.417664
18.801921	1116.249700	14.422682
18.949191	1114.042071	14.427699
19.232549	1104.529477	14.432717
19.085288	1118.293308	14.437735
19.109286	1109.391119	14.442752
19.136627	1115.184951	14.447770
18.862790	1110.048240	14.452787
19.237386	1112.418758	14.457805
19.268217	1112.925636	14.462823
18.973984	1109.368229	14.467840
19.300264	1092.193740	14.472858
18.925297	1093.349538	14.477875
18.905870	1103.071036	14.482893
18.815580	1112.428745	14.487911
19.002467	1112.666781	14.492928
19.208848	1109.186786	14.497946
19.148077	1111.110007	14.502963
19.315219	1105.566157	14.507981
19.086224	1115.358321	14.512999
19.002309	1104.220237	14.518016
19.427129	1108.263824	14.523034
19.062500	1110.011578	14.528051
19.491837	1095.738327	14.533069
19.254541	1111.413093	14.538087
19.481125	1105.051131	14.543104
19.518541	1108.648506	14.548122
18.928514	1112.457255	14.553139
19.427481	1100.415238	14.558157
19.442024	1110.938537	14.563175
19.253729	1099.860717	14.568192
19.384260	1099.429018	14.573210
19.239946	1098.528854	14.578227
19.530075	1112.860894	14.583245
19.149917	1112.000718	14.588263
18.993010	1111.056192	14.593280
19.060482	1113.099036	14.598298
19.454029	1122.454278	14.603315
19.933596	1138.531939	14.608333
19.814710	1131.613244	14.613351
19.915793	1131.497055	14.618368
19.451217	1113.836702	14.623386
19.204336	1107.380611	14.628403
19.898260	1124.419827	14.633421
19.728544	1141.288060	14.638439
20.066948	1125.188245	14.643456
19.863177	1117.478583	14.648474
19.874849	1120.240120	14.653491
19.660971	1116.687070	14.658509
19.763541	1113.998310	14.663527
19.724393	1099.096659	14.668544
19.994549	1100.983376	14.673562
19.580982	1098.149318	14.678579
19.966031	1114.008030	14.683597
19.568074	1115.571175	14.688615
19.857412	1135.566105	14.693632
19.984056	1122.856856	14.698650
19.996017	1136.017885	14.703667
20.181648	1129.554458	14.708685
19.391535	1140.100900	14.713703
19.732940	1143.039513	14.718720
20.200092	1135.218323	14.723738
19.645509	1146.518105	14.728755
19.808926	1142.476370	14.733773
19.963905	1140.383593	14.738791
20.099920	1136.742460	14.743808
20.280912	1140.177006	14.748826
19.968314	1137.989515	14.753843
20.037700	1137.451448	14.758861
20.027543	1143.325536	14.763879
19.997581	1133.310697	14.768896
20.061292	1139.140617	14.773914
19.975764	1148.612906	14.778931
20.312791	1138.744929	14.783949
20.055608	1155.863533	14.788967
20.120439	1157.127721	14.793984
19.938114	1170.151789	14.799002
20.083663	1178.520377	14.804019
20.027702	1169.968437	14.809037
19.984163	1171.600231	14.814055
20.002875	1172.939012	14.819072
19.970766	1164.901200	14.824090
20.026550	1167.761707	14.829107
20.611922	1185.766632	14.834125
20.699505	1192.400446	14.839143
20.773051	1178.229170	14.844160
21.011330	1167.855956	14.849178
20.761768	1164.183241	14.854195
20.815165	1153.129773	14.859213
20.882575	1154.629349	14.864231
20.907960	1156.374876	14.869248
21.149047	1148.123953	14.874266
20.738840	1153.900768	14.879283
20.754345	1150.854442	14.884301
20.648564	1143.203279	14.889319
20.794153	1141.632905	14.894336
20.898203	1123.952824	14.899354
20.533411	1132.316455	14.904371
21.121424	1116.682224	14.909389
20.774771	1117.005401	14.914407
20.957551	1114.543848	14.919424
21.135026	1112.471743	14.924442
20.932767	1122.866921	14.929459
20.676899	1124.923749	14.934477
20.676633	1123.462263	14.939495
20.456428	1119.294937	14.944512
20.924754	1114.161631	14.949530
20.666512	1131.609110	14.954547
20.938244	1137.802861	14.959565
20.900013	1147.010212	14.964583
20.931197	1152.081797	14.969600
20.938154	1142.863143	14.974618
20.784720	1149.085050	14.979635
21.207937	1141.858142	14.984653
20.897891	1139.945017	14.989671
20.875147	1146.723522	14.994688
21.134997	1153.071216	14.999706
20.713715	1154.911852	15.004723
21.084168	1151.452999	15.009741
21.005541	1153.336675	15.014759
20.951711	1155.262291	15.019776
21.152147	1136.567399	15.024794
21.099584	1155.697178	15.029811
20.914340	1158.799313	15.034829
20.916555	1155.809523	15.039847
20.624002	1175.839811	15.044864
21.310094	1181.485197	15.049882
21.137834	1188.820440	15.054899
21.348777	1183.211410	15.059917
21.458868	1193.034266	15.064935
21.446189	1193.805455	15.069952
21.546347	1188.079410	15.074970
21.152310	1187.205395	15.079987
21.446755	1194.047729	15.085005
21.253519	1192.684056	15.090023
21.167942	1193.943327	15.095040
21.174464	1183.789719	15.100058
21.262992	1194.729107	15.105075
21.332706	1201.343455	15.110093
21.347591	1214.856413	15.115111
21.689431	1225.110042	15.120128
21.630194	1219.608110	15.125146
21.707682	1210.301317	15.130163
21.737064	1219.378186	15.135181
22.017002	1219.516115	15.140199
21.711251	1217.467232	15.145216
21.847403	1213.621736	15.150234
21.562390	1222.224900	15.155251
21.586123	1209.900782	15.160269
21.590150	1211.496722	15.165287
21.296537	1214.324766	15.170304
21.896287	1214.696534	15.175322
21.992883	1216.279843	15.180339
22.085387	1210.677498	15.185357
22.010003	1213.385020	15.190375
21.721453	1220.335293	15.195392
21.985886	1214.004002	15.200410
21.964307	1214.236142	15.205427
22.148437	1211.644433	15.210445
22.173536	1207.130811	15.215463
21.897937	1217.724849	15.220480
22.005054	1214.205033	15.225498
21.918592	1212.979510	15.230515
21.822518	1213.569294	15.235533
21.754692	1206.738137	15.240551
22.236871	1211.855640	15.245568
21.849604	1217.932984	15.250586
21.954541	1215.165863	15.255603
21.876581	1205.840425	15.260621
22.291188	1207.201197	15.265639
21.993286	1210.470881	15.270656
22.116383	1210.468351	15.275674
22.510347	1219.840906	15.280691
22.294282	1225.652404	15.285709
22.344194	1214.779386	15.290727
21.974407	1219.233022	15.295744
22.186291	1231.006229	15.300762
22.036772	1245.318953	15.305779
22.360437	1241.039148	15.310797
22.457300	1241.900395	15.315815
22.701316	1244.830807	15.320832
22.385001	1230.737277	15.325850
22.464147	1238.043747	15.330867
22.843541	1244.310586	15.335885
22.696633	1232.992729	15.340903
22.021600	1244.462991	15.345920
22.649882	1243.362748	15.350938
22.355606	1226.157406	15.355955
22.689312	1231.525964	15.360973
22.499950	1241.183278	15.365991
22.557523	1248.983872	15.371008
22.802478	1241.567659	15.376026
23.107842	1237.926700	15.381043
22.908392	1235.138125	15.386061
23.050790	1236.809883	15.391079
22.726953	1238.575672	15.396096
22.781262	1235.702400	15.401114
23.096988	1232.935278	15.406131
22.425620	1246.818227	15.411149
22.887105	1244.089864	15.416167
22.663430	1232.426513	15.421184
22.678989	1230.254539	15.426202
22.546040	1234.122770	15.431219
22.717561	1241.711121	15.436237
22.643035	1247.262495	15.441255
22.825064	1247.217888	15.446272
22.984712	1262.278028	15.451290
22.942150	1257.646507	15.456307
22.775315	1269.189791	15.461325
23.159931	1264.358135	15.466343
23.143986	1270.079301	15.471360
23.395021	1261.739660	15.476378
23.538283	1260.828692	15.481395
23.328520	1258.684718	15.486413
23.335406	1231.405266	15.491431
23.141231	1234.648659	15.496448
23.314822	1237.826593	15.501466
23.158151	1236.200155	15.506483
23.435183	1239.468766	15.511501
23.178209	1238.097574	15.516519
23.339350	1245.157750	15.521536
23.414640	1243.007734	15.526554
23.510698	1244.450984	15.531571
23.346302	1243.373841	15.536589
23.637005	1229.753802	15.541607
23.341538	1237.300485	15.546624
23.243291	1221.737699	15.551642
23.434314	1239.620840	15.556659
23.331705	1265.409221	15.561677
23.695294	1257.697306	15.566695
23.408560	1264.441005	15.571712
23.557812	1260.510645	15.576730
23.405908	1263.455296	15.581747
23.610095	1271.592936	15.586765
23.422117	1264.171904	15.591783
23.320662	1263.668923	15.596800
23.130965	1259.808288	15.601818
23.340152	1258.139933	15.606835
23.460032	1270.662295	15.611853
23.733241	1276.218871	15.616871
23.596529	1291.842849	15.621888
24.012463	1297.574127	15.626906
23.955364	1289.151834	15.631923
23.671766	1291.780202	15.636941
24.006644	1292.827867	15.641959
23.719183	1299.397692	15.646976
23.738642	1292.592538	15.651994
24.127584	1288.542020	15.657011
24.052648	1293.438777	15.662029
24.064660	1286.761238	15.667047
23.926648	1296.704135	15.672064
23.864002	1287.760341	15.677082
24.120097	1289.287621	15.682099
24.036770	1295.103459	15.687117
23.888174	1293.354023	15.692135
24.052818	1295.426013	15.697152
24.104747	1288.191857	15.702170
24.353704	1289.696308	15.707187
24.117758	1294.709589	15.712205
23.992604	1291.546462	15.717223
24.080945	1292.571328	15.722240
23.897182	1300.756145	15.727258
23.989681	1286.875311	15.732275
23.938787	1297.098994	15.737293
24.146033	1306.977819	15.742311
24.165046	1314.873041	15.747328
24.204734	1317.898845	15.752346
24.665402	1309.720783	15.757363
24.504672	1317.428961	15.762381
24.592594	1313.989476	15.767399
25.076183	1311.883392	15.772416
24.701615	1321.021558	15.777434
25.077397	1299.939525	15.782451
24.621667	1286.067536	15.787469
24.499443	1285.795163	15.792487
24.673094	1280.915106	15.797504
24.633517	1291.842393	15.802522
24.522348	1273.545574	15.807539
24.344000	1280.218116	15.812557
24.705226	1293.300360	15.817575
24.685644	1300.068564	15.822592
24.532453	1319.623131	15.827610
24.991740	1309.396153	15.832627
24.659662	1314.078579	15.837645
24.822778	1307.949912	15.842663
25.002803	1310.306740	15.847680
24.985881	1313.044719	15.852698
24.978219	1299.839555	15.857715
24.755070	1313.511452	15.862733
24.988052	1315.953570	15.867751
25.016717	1304.444672	15.872768
25.112131	1309.096197	15.877786
25.142182	1303.135707	15.882803
24.849695	1309.031590	15.887821
24.910640	1308.535864	15.892839
24.803671	1311.286053	15.897856
24.851768	1314.639582	15.902874
25.184937	1299.473892	15.907891
24.705715	1312.589159	15.912909
24.750171	1310.302138	15.917927
25.120007	1303.647002	15.922944
25.045680	1312.401017	15.927962
25.089605	1304.863469	15.932979
24.766521	1324.925400	15.937997
25.028182	1338.418707	15.943015
25.365259	1343.470219	15.948032
25.703276	1348.053479	15.953050
25.509474	1334.152082	15.958067
25.486113	1346.327460	15.963085
25.574385	1343.632769	15.968103
25.624146	1334.902147	15.973120
25.577726	1340.259912	15.978138
25.686159	1331.242777	15.983155
25.405513	1347.563942	15.988173
25.602608	1339.358024	15.993191
25.738310	1342.255673	15.998208
25.311541	1338.367102	16.003226
25.879982	1334.879238	16.008243
25.701995	1342.277708	16.013261
25.620059	1345.347748	16.018279
25.667796	1340.958666	16.023296
25.366351	1338.113405	16.028314
25.830636	1339.122242	16.033331
25.600338	1339.719381	16.038349
25.565047	1338.414872	16.043367
25.565433	1329.907807	16.048384
25.501138	1338.442853	16.053402
25.982814	1332.864751	16.058419
25.763255	1341.096483	16.063437
25.564708	1335.022801	16.068455
25.933217	1329.742636	16.073472
25.818472	1345.868119	16.078490
25.819522	1349.743633	16.083507
26.176722	1351.400960	16.088525
26.203515	1351.970326	16.093543
26.235359	1351.262513	16.098560
26.284216	1366.533291	16.103578
26.403242	1354.535334	16.108595
26.157111	1344.059847	16.113613
26.008037	1348.130387	16.118631
26.131745	1341.468903	16.123648
26.563413	1358.113795	16.128666
26.671499	1340.380042	16.133683
26.026068	1339.488356	16.138701
26.214929	1338.021003	16.143719
26.197656	1335.552512	16.148736
26.277231	1353.686586	16.153754
26.387463	1341.625536	16.158771
26.332165	1350.871276	16.163789
26.424952	1356.318504	16.168807
26.649850	1356.668334	16.173824
26.293382	1364.833467	16.178842
26.800543	1353.157206	16.183859
26.407215	1355.014871	16.188877
26.315689	1356.677101	16.193895
26.617610	1348.380922	16.198912
26.714502	1357.169493	16.203930
26.823731	1354.598478	16.208947
26.702130	1351.467425	16.213965
26.657018	1361.217763	16.218983
26.673591	1354.959502	16.224000
26.729588	1353.993745	16.229018
26.365076	1341.515557	16.234035
26.560669	1351.524689	16.239053
26.457957	1358.342168	16.244071
27.096584	1346.691303	16.249088
26.931572	1360.247675	16.254106
26.722632	1349.518767	16.259123
26.626189	1354.806114	16.264141
26.573098	1354.014390	16.269159
26.652909	1356.809917	16.274176
26.821757	1379.929430	16.279194
26.852572	1376.956103	16.284211
27.018505	1387.598517	16.289229
26.876804	1386.235316	16.294247
27.318192	1375.724663	16.299264
26.797694	1382.202157	16.304282
27.171908	1387.408530	16.309299
27.162505	1380.028230	16.314317
26.765963	1385.160356	16.319335
27.029045	1388.219119	16.324352
27.356146	1383.528086	16.329370
26.952589	1375.063729	16.334387
27.064493	1386.926113	16.339405
26.950807	1412.602409	16.344423
27.145985	1404.753852	16.349440
26.888087	1425.809382	16.354458
27.411279	1418.533841	16.359475
27.678924	1415.954595	16.364493
27.386681	1419.241885	16.369511
27.718664	1410.343841	16.374528
27.794220	1402.692723	16.379546
27.789581	1416.143356	16.384563
27.998594	1402.314704	16.389581
27.696718	1409.678681	16.394599
27.874002	1408.543946	16.399616
27.820086	1415.695850	16.404634
28.097240	1410.184786	16.409651
27.846644	1405.513392	16.414669
27.639105	1421.985472	16.419687
27.925722	1406.279398	16.424704
27.704521	1408.707262	16.429722
27.607498	1412.004226	16.434739
27.734382	1411.052273	16.439757
27.514323	1402.507009	16.444775
27.695785	1411.934292	16.449792
27.607185	1410.120148	16.454810
27.447455	1415.034581	16.459827
27.878861	1397.655673	16.464845
28.181716	1421.097846	16.469863
28.147262	1412.467002	16.474880
27.742684	1418.616984	16.479898
27.963016	1430.350358	16.484915
28.239095	1437.943866	16.489933
28.025882	1444.205354	16.494951
28.636739	1445.633132	16.499968
28.468381	1444.175934	16.504986
28.471083	1442.679279	16.510003
28.260599	1423.768097	16.515021
28.024314	1421.000178	16.520039
28.128775	1430.435154	16.525056
28.095632	1442.449244	16.530074
28.156644	1442.491286	16.535091
28.368284	1440.940218	16.540109
28.393487	1442.963360	16.545127
28.645024	1426.223358	16.550144
28.712375	1445.030420	16.555162
28.629004	1441.029235	16.560179
28.519424	1436.895009	16.565197
28.349873	1441.389045	16.570215
28.366284	1429.959254	16.575232
28.687281	1434.839063	16.580250
28.615074	1434.642230	16.585267
28.679654	1433.422292	16.590285
28.049482	1428.523045	16.595303
28.279367	1435.664399	16.600320
28.778061	1440.331608	16.605338
28.829940	1448.474579	16.610355
28.918459	1438.713859	16.615373
29.106552	1462.003519	16.620391
28.973696	1447.236398	16.625408
28.984468	1438.612589	16.630426
28.894856	1444.704324	16.635443
29.103711	1429.204061	16.640461
28.962187	1432.669446	16.645479
29.093629	1425.131466	16.650496
29.077978	1431.998284	16.655514
28.965389	1426.049252	16.660531
29.074758	1429.959930	16.665549
29.190038	1452.965623	16.670567
29.480380	1444.370144	16.675584
29.558780	1434.962674	16.680602
29.372256	1426.283479	16.685619
29.536518	1419.700258	16.690637
29.306868	1424.407030	16.695655
29.607926	1426.351249	16.700672
29.399473	1413.923832	16.705690
29.418380	1417.198772	16.710707
29.751897	1412.038172	16.715725
29.519037	1422.565405	16.720743
29.253769	1420.676690	16.725760
29.581497	1410.580171	16.730778
29.481872	1425.148934	16.735795
29.122235	1412.926170	16.740813
29.357443	1422.204373	16.745831
29.443647	1424.876805	16.750848
29.475390	1430.379874	16.755866
29.262757	1451.378704	16.760883
29.538098	1442.562890	16.765901
29.291255	1447.820938	16.770919
29.076435	1452.371713	16.775936
29.328332	1451.982036	16.780954
29.239372	1455.810728	16.785971
29.725040	1472.887308	16.790989
29.760199	1482.137776	16.796007
30.110217	1482.895543	16.801024
30.139746	1472.308404	16.806042
29.870873	1475.243010	16.811059
30.452327	1474.056051	16.816077
30.057438	1479.541469	16.821095
30.360472	1473.711521	16.826112
30.497038	1473.392193	16.831130
30.353292	1452.173084	16.836147
30.248758	1450.591499	16.841165
29.953264	1450.510518	16.846183
30.052136	1439.409131	16.851200
30.208100	1437.749210	16.856218
30.182654	1452.763138	16.861235
30.212938	1444.857326	16.866253
30.450189	1456.142642	16.871271
30.323946	1454.621751	16.876288
30.373325	1446.152934	16.881306
30.348595	1455.939313	16.886323
30.583662	1455.233543	16.891341
30.240865	1460.523292	16.896359
30.404876	1463.565073	16.901376
30.457200	1470.396988	16.906394
30.503483	1473.630777	16.911411
30.434820	1466.150446	16.916429
30.965169	1471.633251	16.921447
30.536186	1465.024604	16.926464
30.820368	1470.866034	16.931482
30.415327	1465.593142	16.936499
30.534701	1466.460109	16.941517
30.863839	1468.575253	16.946535
30.501210	1469.805007	16.951552
30.809896	1462.743836	16.956570
30.812767	1468.961150	16.961587
30.653892	1465.243762	16.966605
30.585883	1473.028729	16.971623
30.685600	1470.847064	16.976640
30.761054	1463.671906	16.981658
30.789935	1465.860972	16.986675
31.123643	1471.888654	16.991693
30.982816	1486.727309	16.996711
30.915297	1487.394245	17.001728
31.312374	1493.673209	17.006746
31.242361	1500.987666	17.011763
31.215356	1489.994960	17.016781
31.287163	1504.601836	17.021799
31.107482	1495.114001	17.026816
31.347478	1496.504217	17.031834
30.901175	1499.561230	17.036851
31.584066	1489.081618	17.041869
31.650110	1487.238611	17.046887
31.522610	1494.314595	17.051904
31.700737	1497.008375	17.056922
31.333406	1505.360028	17.061939
31.582819	1508.102196	17.066957
31.301340	1496.027789	17.071975
31.443379	1505.266411	17.076992
31.542007	1488.480500	17.082010
31.508798	1496.449848	17.087027
31.825523	1497.611173	17.092045
31.270640	1497.198510	17.097063
31.523397	1499.016124	17.102080
31.818073	1496.610321	17.107098
31.525633	1504.648351	17.112115
31.888667	1490.153482	17.117133
31.612806	1500.484376	17.122151
31.483370	1496.788465	17.127168
31.865809	1498.153036	17.132186
31.401430	1502.139413	17.137203
32.060660	1521.774155	17.142221
32.063326	1522.563676	17.147239
31.568230	1524.002457	17.152256
31.906474	1516.784383	17.157274
32.255678	1517.506461	17.162291
32.058485	1521.163399	17.167309
32.072451	1529.376886	17.172327
32.074787	1522.377238	17.177344
32.404575	1514.905457	17.182362
32.546722	1522.070490	17.187379
32.370412	1529.149484	17.192397
32.235542	1514.241298	17.197415
32.460580	1530.328212	17.202432
32.581743	1509.042947	17.207450
32.146798	1517.517654	17.212467
32.494106	1510.913025	17.217485
31.950696	1511.600401	17.222503
32.234599	1516.911590	17.227520
32.122923	1520.411797	17.232538
32.179372	1520.995138	17.237555
32.048934	1518.816288	17.242573
32.426140	1525.561551	17.247591
32.801596	1543.885640	17.252608
32.524038	1546.266988	17.257626
32.842283	1545.129285	17.262643
32.821477	1542.593239	17.267661
33.061847	1547.245939	17.272679
32.784885	1547.767378	17.277696
33.025361	1539.508475	17.282714
33.082130	1552.676584	17.287731
33.175820	1536.041046	17.292749
32.939891	1525.073985	17.297767
32.330285	1523.097218	17.302784
32.815595	1527.022204	17.307802
32.819709	1537.094386	17.312819
33.111588	1539.248015	17.317837
33.285579	1540.879123	17.322855
32.801517	1551.412370	17.327872
33.394708	1548.392779	17.332890
33.287498	1542.257772	17.337907
33.236605	1541.319612	17.342925
33.150055	1540.538558	17.347943
32.991507	1545.566612	17.352960
33.299862	1539.970003	17.357978
33.059194	1546.701835	17.362995
33.009222	1544.688344	17.368013
33.513431	1546.756683	17.373031
33.079676	1549.280133	17.378048
33.451588	1560.545112	17.383066
33.370085	1580.166437	17.388083
33.248390	1576.214106	17.393101
33.333246	1567.863734	17.398119
33.219388	1581.683052	17.403136
33.403903	1578.843192	17.408154
33.615396	1570.510745	17.413171
33.259098	1583.178649	17.418189
33.558421	1573.098951	17.423207
33.692386	1595.849394	17.428224
33.861033	1596.334168	17.433242
34.312954	1598.260814	17.438259
34.066349	1587.528552	17.443277
33.766456	1567.964742	17.448295
33.638643	1579.019099	17.453312
34.263821	1586.829061	17.458330
34.278960	1596.133318	17.463347
34.089834	1592.983124	17.468365
34.151901	1589.197881	17.473383
34.359079	1585.173955	17.478400
34.291720	1581.770457	17.483418
34.169803	1572.098172	17.488435
33.941857	1570.390240	17.493453
34.455715	1569.318840	17.498471
34.309103	1599.293763	17.503488
34.486292	1592.574858	17.508506
34.442634	1588.323730	17.513523
34.162292	1571.969217	17.518541
34.696550	1577.604164	17.523559
34.346526	1594.467820	17.528576
34.288271	1587.153021	17.533594
34.249825	1598.594894	17.538611
34.364423	1594.588717	17.543629
34.621236	1594.412389	17.548647
34.439517	1602.989539	17.553664
34.439521	1595.380805	17.558682
34.745813	1605.663824	17.563699
34.607953	1597.195733	17.568717
34.818975	1595.636879	17.573735
34.817521	1602.030947	17.578752
34.821935	1590.289650	17.583770
34.453421	1594.368382	17.588787
34.463093	1595.379967	17.593805
34.654808	1590.878695	17.598823
34.499896	1610.159509	17.603840
34.780289	1607.726537	17.608858
34.719807	1624.823198	17.613875
34.992808	1622.433971	17.618893
35.385077	1617.842665	17.623911
35.122609	1622.216372	17.628928
35.190030	1625.939587	17.633946
35.134355	1619.497168	17.638963
35.224860	1620.757914	17.643981
35.480208	1617.064946	17.648999
35.401209	1618.547564	17.654016
35.219974	1615.552745	17.659034
35.239999	1620.004299	17.664051
35.243884	1617.990114	17.669069
35.358389	1616.676038	17.674087
35.102373	1615.738898	17.679104
35.236476	1607.362997	17.684122
35.214738	1612.932105	17.689139
35.645281	1636.416766	17.694157
35.843058	1638.988408	17.699175
35.435555	1648.266489	17.704192
35.697735	1652.075054	17.709210
35.894914	1639.613892	17.714227
36.003046	1640.307543	17.719245
36.053177	1633.250688	17.724263
35.792456	1639.759124	17.729280
35.946083	1640.690486	17.734298
35.856477	1640.074500	17.739315
35.781307	1642.769069	17.744333
36.322283	1633.449945	17.749351
35.892909	1640.800184	17.754368
36.032994	1630.055980	17.759386
36.089616	1624.003550	17.764403
35.849118	1629.515326	17.769421
35.857060	1631.873248	17.774439
36.094535	1628.806075	17.779456
35.963386	1631.525300	17.784474
36.267746	1628.482443	17.789491
36.107379	1637.219840	17.794509
36.042159	1636.632083	17.799527
35.972945	1633.487540	17.804544
36.187356	1652.297182	17.809562
36.623948	1664.068803	17.814579
36.625548	1665.198269	17.819597
36.717986	1663.531955	17.824615
36.552989	1664.621001	17.829632
36.856812	1659.524704	17.834650
36.427493	1653.083746	17.839667
36.364702	1651.364889	17.844685
36.879670	1653.404684	17.849703
36.715069	1664.730568	17.854720
36.653460	1666.958719	17.859738
36.900917	1663.431617	17.864755
36.946022	1665.265261	17.869773
37.110207	1656.577644	17.874791
36.894902	1665.993079	17.879808
36.866381	1660.802416	17.884826
37.019547	1658.927192	17.889843
36.874775	1663.160089	17.894861
36.825266	1653.749338	17.899879
36.849977	1669.907883	17.904896
36.789124	1660.471848	17.909914
37.084951	1647.727356	17.914931
36.761402	1655.391504	17.919949
37.132252	1651.064376	17.924967
37.083351	1663.363932	17.929984
37.219499	1661.773029	17.935002
37.229655	1666.195922	17.940019
37.102634	1679.553740	17.945037
37.577151	1682.958518	17.950055
37.511089	1689.382258	17.955072
37.546088	1694.097484	17.960090
37.694921	1702.295733	17.965107
37.696446	1683.774976	17.970125
37.623671	1687.938827	17.975143
37.513450	1683.173938	17.980160
37.673499	1682.665665	17.985178
37.988796	1685.689826	17.990195
37.725120	1675.631199	17.995213
38.014208	1683.301800	18.000231
37.863074	1666.571776	18.005248
37.646092	1666.412783	18.010266
37.635307	1673.876137	18.015283
37.633494	1682.727362	18.020301
37.940919	1672.813969	18.025319
38.053010	1679.304943	18.030336
38.007453	1680.480830	18.035354
38.196468	1676.250453	18.040371
37.869343	1681.679403	18.045389
38.040788	1682.712530	18.050407
38.194513	1691.148934	18.055424
37.942693	1687.672136	18.060442
37.969567	1677.921511	18.065459
38.171350	1685.903866	18.070477
38.117366	1686.140611	18.075495
38.323553	1700.518645	18.080512
38.186703	1704.860866	18.085530
38.447785	1703.005888	18.090547
38.206815	1714.647650	18.095565
38.493858	1704.059676	18.100583
38.745556	1711.642806	18.105600
38.150669	1713.155275	18.110618
38.819092	1703.920044	18.115635
38.768301	1703.143667	18.120653
38.994970	1701.153465	18.125671
38.791010	1710.589482	18.130688
38.645620	1712.249679	18.135706
38.491192	1699.552818	18.140723
38.452921	1712.641584	18.145741
38.510349	1710.786991	18.150759
39.047971	1714.213965	18.155776
39.160626	1713.475381	18.160794
39.031380	1721.913560	18.165811
39.269678	1723.981241	18.170829
39.299227	1723.884813	18.175847
39.179873	1708.410478	18.180864
38.824997	1708.067712	18.185882
39.064290	1718.190291	18.190899
39.070190	1723.324533	18.195917
38.969068	1729.634039	18.200935
39.431211	1722.787007	18.205952
39.392423	1721.675172	18.210970
39.486366	1713.906278	18.215987
39.224272	1727.904301	18.221005
39.198974	1725.798497	18.226023
39.353327	1719.897895	18.231040
39.193295	1727.804584	18.236058
39.462852	1727.456060	18.241075
39.505327	1723.713016	18.246093
39.394816	1744.249601	18.251111
40.141103	1750.291101	18.256128
39.695040	1754.544180	18.261146
39.899099	1738.041261	18.266163
39.923627	1735.671269	18.271181
39.902311	1731.994338	18.276199
40.043076	1743.812435	18.281216
39.915286	1737.294552	18.286234
39.997815	1738.529862	18.291251
39.961502	1755.025803	18.296269
39.718570	1738.397967	18.301287
40.507497	1749.964636	18.306304
40.252186	1748.266350	18.311322
40.611112	1740.977806	18.316339
40.591048	1732.534155	18.321357
40.384021	1715.057074	18.326375
40.405734	1703.563208	18.331392
40.357461	1706.302923	18.336410
40.301712	1706.663583	18.341427
40.050959	1708.259402	18.346445
40.337289	1723.938696	18.351463
40.263599	1726.937362	18.356480
40.255818	1754.075746	18.361498
40.662006	1738.613241	18.366515
40.404175	1752.207036	18.371533
40.346152	1744.537008	18.376551
40.689023	1744.999129	18.381568
40.138786	1759.497040	18.386586
40.419450	1746.148297	18.391603
40.458049	1762.303843	18.396621
40.465178	1764.619400	18.401639
40.770368	1777.864126	18.406656
40.854922	1775.396356	18.411674
41.158853	1773.335430	18.416691
41.194383	1772.146672	18.421709
40.927928	1779.042732	18.426727
40.864223	1763.405549	18.431744
40.779277	1776.126538	18.436762
41.288094	1768.697321	18.441779
41.406759	1768.100649	18.446797
41.237131	1762.490494	18.451815
41.472882	1777.985336	18.456832
40.986085	1770.313728	18.461850
41.262410	1782.667589	18.466867
41.622073	1796.260756	18.471885
41.258378	1805.127711	18.476903
41.614373	1795.907741	18.481920
41.600531	1803.859068	18.486938
41.757223	1790.272232	18.491955
41.905653	1797.493041	18.496973
41.755508	1799.659548	18.501991
42.353372	1787.058048	18.507008
42.084663	1764.213615	18.512026
42.245576	1739.450966	18.517043
41.997461	1742.782956	18.522061
41.833089	1749.611249	18.527079
42.467163	1738.249039	18.532096
42.051838	1741.822993	18.537114
42.607050	1743.161234	18.542131
42.217525	1743.984063	18.547149
41.638062	1753.984485	18.552167
42.124734	1740.903474	18.557184
42.221221	1740.438835	18.562202
42.302474	1740.102711	18.567219
42.386679	1754.422332	18.572237
42.102306	1750.848568	18.577255
42.320341	1736.445287	18.582272
42.030704	1740.209372	18.587290
42.524597	1743.603858	18.592307
42.589332	1740.562619	18.597325
42.177315	1740.717930	18.602343
42.482167	1740.135194	18.607360
42.066167	1744.093511	18.612378
42.345875	1757.061747	18.617395
42.596907	1763.749741	18.622413
42.354939	1768.606694	18.627431
42.898369	1756.875680	18.632448
42.732449	1770.510907	18.637466
42.819728	1768.696621	18.642483
43.163202	1773.670834	18.647501
43.049228	1775.542744	18.652519
42.998798	1771.347809	18.657536
42.806968	1778.656661	18.662554
42.967162	1763.271633	18.667571
43.167368	1771.738939	18.672589
42.860986	1769.634179	18.677607
43.069520	1774.089090	18.682624
43.022639	1767.706565	18.687642
42.837507	1771.559193	18.692659
43.066119	1787.354444	18.697677
43.319360	1793.884210	18.702695
43.404076	1798.185693	18.707712
43.284149	1803.019616	18.712730
43.273222	1804.958653	18.717747
43.429036	1796.530616	18.722765
43.416836	1805.818283	18.727783
43.644849	1803.077059	18.732800
43.637472	1804.099759	18.737818
43.430822	1801.346922	18.742835
43.557623	1805.318578	18.747853
43.377594	1808.133360	18.752871
43.665656	1811.316403	18.757888
43.506777	1824.164680	18.762906
43.366243	1833.124481	18.767923
44.057142	1826.205918	18.772941
43.697192	1830.347854	18.777959
43.843153	1833.980505	18.782976
43.639610	1819.505486	18.787994
43.718070	1836.154484	18.793011
44.218941	1845.241148	18.798029
44.140609	1857.181968	18.803047
44.506436	1852.200500	18.808064
44.581911	1851.057853	18.813082
44.637985	1851.896782	18.818099
44.836132	1838.941203	18.823117
44.482618	1829.822213	18.828135
44.763944	1816.755190	18.833152
44.496213	1812.506598	18.838170
44.228500	1810.462334	18.843187
44.687221	1819.021343	18.848205
44.522209	1837.973410	18.853223
45.077362	1839.412457	18.858240
45.086625	1846.464294	18.863258
45.113002	1823.441593	18.868275
44.942374	1807.228043	18.873293
44.826829	1813.710453	18.878311
44.743585	1807.591829	18.883328
44.761184	1809.981637	18.888346
44.592245	1825.957965	18.893363
44.898859	1834.186752	18.898381
44.895078	1846.339189	18.903399
44.728608	1843.271399	18.908416
44.985409	1841.224203	18.913434
44.824798	1841.075129	18.918451
44.930986	1839.301392	18.923469
44.884569	1858.035345	18.928487
45.286427	1870.190065	18.933504
45.220042	1866.261143	18.938522
45.610810	1877.367314	18.943539
45.755697	1867.008765	18.948557
45.132147	1876.527221	18.953575
45.449218	1874.971580	18.958592
45.726972	1884.533543	18.963610
45.552217	1883.498232	18.968627
45.892641	1871.105990	18.973645
45.558548	1878.782630	18.978663
45.694453	1864.181070	18.983680
45.873012	1865.286256	18.988698
45.592291	1867.326837	18.993715
46.060504	1870.435855	18.998733
45.945304	1872.887116	19.003751
45.837064	1866.386401	19.008768
46.016664	1870.376857	19.013786
45.610398	1882.846221	19.018803
46.078544	1887.331638	19.023821
46.201254	1894.317396	19.028839
46.290123	1895.833950	19.033856
46.361808	1898.204153	19.038874
46.276633	1907.123692	19.043891
46.193509	1911.660979	19.048909
46.055328	1910.040056	19.053927
46.139390	1905.769581	19.058944
46.467873	1897.126175	19.063962
46.172615	1906.846779	19.068979
46.651893	1907.857497	19.073997
46.689399	1925.353559	19.079015
46.682915	1925.343041	19.084032
47.297526	1925.326535	19.089050
46.908123	1919.573323	19.094067
47.170317	1926.574101	19.099085
46.984836	1927.761846	19.104103
46.955134	1912.243272	19.109120
47.354024	1912.324433	19.114138
46.972334	1901.578970	19.119155
47.097732	1899.073684	19.124173
46.982524	1907.273408	19.129191
47.022978	1927.315849	19.134208
47.548516	1916.577067	19.139226
46.776401	1923.892277	19.144243
47.140412	1914.976026	19.149261
46.934981	1922.163976	19.154279
47.078436	1919.077334	19.159296
47.125388	1914.610662	19.164314
47.211142	1922.123838	19.169331
47.569863	1933.337739	19.174349
47.508665	1948.964393	19.179367
47.400572	1953.077886	19.184384
47.606241	1938.612300	19.189402
47.684930	1948.859756	19.194419
47.861538	1942.404580	19.199437
47.682062	1947.243327	19.204455
47.672526	1945.799445	19.209472
48.006675	1941.328337	19.214490
47.725937	1952.316251	19.219507
47.889949	1938.485153	19.224525
48.024593	1950.981990	19.229543
48.093418	1965.017351	19.234560
48.262873	1974.182405	19.239578
47.861089	1976.664386	19.244595
48.485826	1967.687052	19.249613
48.505759	1984.713263	19.254631
48.572575	1979.797202	19.259648
48.475565	1967.755545	19.264666
48.282297	1986.797135	19.269683
48.428259	1971.625293	19.274701
48.351144	1967.693798	19.279719
48.262429	1974.961981	19.284736
48.731439	1962.210495	19.289754
48.494965	1973.393824	19.294771
48.673887	1976.502915	19.299789
48.874725	1984.341092	19.304807
48.755042	1966.485819	19.309824
48.920218	1970.020426	19.314842
48.755390	1973.384685	19.319859
48.644619	1970.397376	19.324877
48.665366	1983.639555	19.329895
48.976724	1988.837289	19.334912
49.496507	1992.882654	19.339930
49.190952	1998.114817	19.344947
49.345436	1985.652207	19.349965
49.564957	1981.123761	19.354983
49.145097	1975.922446	19.360000
49.435286	1976.534672	19.365018
49.306838	1983.753950	19.370035
49.705055	1981.674570	19.375053
50.087294	1982.766777	19.380071
49.507341	1980.400761	19.385088
49.562597	1956.339588	19.390106
49.672669	1956.338044	19.395123
49.636904	1970.725442	19.400141
49.968175	1982.095911	19.405159
49.832844	1993.686464	19.410176
49.992086	1982.622294	19.415194
49.400831	1990.367322	19.420211
49.983560	1989.259647	19.425229
49.902068	1987.496615	19.430247
49.852010	1991.023694	19.435264
49.858555	1980.197506	19.440282
49.884794	1990.858043	19.445299
49.964009	1980.864668	19.450317
49.977677	1979.968113	19.455335
49.771756	2007.976496	19.460352
50.184974	2001.341416	19.465370
50.266553	2019.008607	19.470387
50.359952	2004.738788	19.475405
50.346134	2000.219592	19.480423
50.287860	2005.037424	19.485440
50.472045	2007.826746	19.490458
50.679789	1998.191135	19.495475
50.851032	2017.721397	19.500493
50.907726	2011.565654	19.505511
50.823083	2020.950924	19.510528
51.075661	2017.346120	19.515546
50.880907	2008.668358	19.520563
51.004415	2017.319808	19.525581
51.360445	2016.684463	19.530599
50.855685	2020.884769	19.535616
51.440558	2024.824047	19.540634
51.247076	2014.218486	19.545651
51.319900	2010.401824	19.550669
51.468637	2000.911848	19.555687
51.130337	2000.281669	19.560704
51.347229	1998.146203	19.565722
51.698527	2011.694494	19.570739
51.882609	2020.379973	19.575757
51.790685	2004.454320	19.580775
51.439778	1993.278082	19.585792
51.444876	1993.252252	19.590810
51.624152	1996.466802	19.595827
51.431425	2016.595359	19.600845
51.883557	2012.214071	19.605863
51.634027	2024.045284	19.610880
52.264600	2022.187519	19.615898
52.088842	2024.893361	19.620915
52.143010	2022.884152	19.625933
52.185166	2022.817123	19.630951
51.628559	2023.003553	19.635968
52.067927	2017.240903	19.640986
52.123092	2024.878900	19.646003
52.025961	2024.494073	19.651021
52.006195	2021.336114	19.656039
52.037999	2026.432686	19.661056
52.195970	2012.516699	19.666074
52.241041	2028.755306	19.671091
51.723653	2019.886277	19.676109
52.434436	2045.054926	19.681127
52.234287	2044.867539	19.686144
52.390609	2053.215125	19.691162
52.412869	2057.790451	19.696179
52.262008	2055.927522	19.701197
52.200165	2049.576109	19.706215
52.848359	2071.709489	19.711232
52.933249	2078.623269	19.716250
53.149905	2066.329004	19.721267
53.059492	2074.573515	19.726285
52.987038	2070.589250	19.731303
52.786944	2071.910932	19.736320
52.807616	2066.459985	19.741338
53.106723	2067.277035	19.746355
52.992540	2067.861986	19.751373
53.459457	2066.588513	19.756391
53.191280	2069.689256	19.761408
53.421185	2079.402602	19.766426
53.627904	2083.121279	19.771443
53.562886	2098.156975	19.776461
54.015697	2085.423437	19.781479
53.689264	2077.643128	19.786496
53.780145	2074.523462	19.791514
53.806177	2073.702407	19.796531
53.764538	2092.527190	19.801549
54.065012	2084.899377	19.806567
53.747649	2098.126196	19.811584
54.066710	2088.478328	19.816602
53.761437	2100.283429	19.821619
53.689243	2101.644487	19.826637
53.795137	2093.948616	19.831655
53.666024	2085.911881	19.836672
53.965154	2084.146994	19.841690
54.152101	2097.739212	19.846707
54.305253	2119.182093	19.851725
54.691633	2110.827771	19.856743
54.551411	2123.765322	19.861760
54.595902	2109.640940	19.866778
55.014627	2110.938909	19.871795
54.644616	2091.077816	19.876813
54.910938	2085.786036	19.881831
54.851109	2074.786559	19.886848
54.788682	2077.606646	19.891866
54.807493	2073.699338	19.896883
55.008507	2090.208552	19.901901
55.515275	2092.324578	19.906919
54.892987	2081.705987	19.911936
54.936466	2068.159380	19.916954
55.169342	2083.256969	19.921971
54.840227	2089.102144	19.926989
55.153650	2101.069773	19.932007
55.415656	2109.012416	19.937024
55.105539	2107.431467	19.942042
55.374293	2104.830666	19.947059
55.194302	2105.656481	19.952077
55.356275	2101.619858	19.957095
55.577443	2108.316903	19.962112
55.292245	2107.552694	19.967130
55.640322	2095.389321	19.972147
55.247409	2112.140190	19.977165
55.361901	2103.852716	19.982183
55.096292	2122.823424	19.987200
55.165293	2135.322265	19.992218
55.472798	2138.405687	19.997235
55.268145	2145.036906	20.002253
55.950578	2152.292356	20.007271
56.352785	2170.333998	20.012288
55.891723	2166.005627	20.017306
56.225382	2163.894040	20.022323
56.364299	2162.275067	20.027341
56.211883	2160.531284	20.032359
56.332311	2153.451486	20.037376
56.238411	2161.875760	20.042394
56.356214	2158.454745	20.047411
56.051808	2169.897149	20.052429
56.393924	2160.709981	20.057447
56.343082	2161.916311	20.062464
56.615544	2160.076319	20.067482
56.882072	2173.604589	20.072499
56.809069	2190.533477	20.077517
57.008183	2185.379610	20.082535
57.065400	2193.418540	20.087552
56.956777	2185.892533	20.092570
57.280926	2185.441224	20.097587
57.106765	2194.007993	20.102605
57.037080	2196.665524	20.107623
57.338946	2181.837653	20.112640
56.957573	2183.646965	20.117658
57.128485	2187.748793	20.122675
57.103481	2192.844625	20.127693
57.314913	2197.398787	20.132711
57.095755	2187.429673	20.137728
57.220068	2202.838343	20.142746
57.250776	2208.322962	20.147763
57.021513	2228.009428	20.152781
57.303605	2217.637290	20.157799
57.457434	2221.480148	20.162816
57.215203	2225.109694	20.167834
57.837311	2243.758983	20.172851
57.881024	2246.116959	20.177869
57.990193	2241.115821	20.182887
58.409849	2239.740345	20.187904
58.430104	2243.209336	20.192922
58.345135	2230.768218	20.197939
58.793182	2230.690027	20.202957
58.699271	2225.420278	20.207975
58.919016	2228.860046	20.212992
58.711660	2212.162793	20.218010
58.857698	2200.077409	20.223027
58.887988	2197.907182	20.228045
58.897712	2200.436158	20.233063
58.850087	2199.636001	20.238080
58.656847	2200.764818	20.243098
58.580885	2194.760581	20.248115
58.770716	2199.528969	20.253133
58.629182	2191.813936	20.258151
58.328921	2186.130455	20.263168
58.692487	2209.805472	20.268186
58.893802	2220.446517	20.273203
58.980925	2220.794072	20.278221
58.505959	2228.276574	20.283239
59.104687	2227.203234	20.288256
58.867149	2231.369811	20.293274
58.987575	2217.282318	20.298291
59.071469	2242.925966	20.303309
59.151540	2247.581505	20.308327
59.259535	2253.285190	20.313344
59.412616	2252.206783	20.318362
59.889397	2253.231328	20.323379
59.737855	2255.258755	20.328397
59.719701	2252.207571	20.333415
59.779026	2255.459829	20.338432
59.655345	2252.892732	20.343450
59.719426	2244.157250	20.348467
59.858286	2251.236552	20.353485
59.942393	2249.777865	20.358503
60.123384	2268.899332	20.363520
60.005107	2280.460885	20.368538
60.359141	2284.791365	20.373555
60.215220	2282.922924	20.378573
60.392640	2287.689071	20.383591
60.644300	2282.626834	20.388608
60.613054	2291.440777	20.393626
60.990561	2268.815370	20.398643
60.868704	2276.874657	20.403661
61.267834	2256.556372	20.408679
60.704811	2236.769693	20.413696
60.903791	2241.706262	20.418714
61.119832	2225.895343	20.423731
61.115899	2231.583764	20.428749
61.191977	2236.870690	20.433767
61.226537	2223.129755	20.438784
61.274090	2224.135479	20.443802
61.281602	2221.727296	20.448819
61.164925	2225.443063	20.453837
61.063604	2229.485816	20.458855
61.257654	2223.721343	20.463872
60.832899	2226.848929	20.468890
61.098346	2241.388095	20.473907
61.241597	2255.525131	20.478925
61.297687	2258.259014	20.483943
61.377314	2263.589061	20.488960
61.237524	2261.838050	20.493978
61.657105	2247.834670	20.498995
61.397130	2258.573671	20.504013
61.346626	2276.161924	20.509031
61.817057	2284.903112	20.514048
61.443214	2285.171768	20.519066
61.770801	2291.638600	20.524083
61.759317	2281.669162	20.529101
62.017677	2299.295479	20.534119
62.323693	2304.015454	20.539136
62.000539	2307.502165	20.544154
62.821339	2306.642313	20.549171
62.395830	2314.413495	20.554189
62.743226	2303.303652	20.559207
62.647262	2307.835313	20.564224
62.645675	2310.287445	20.569242
62.769115	2308.533230	20.574259
63.117064	2309.658328	20.579277
62.681309	2294.375763	20.584295
63.108136	2307.020001	20.589312
62.821801	2291.701187	20.594330
63.168252	2297.327459	20.599347
62.801789	2297.568509	20.604365
62.884892	2294.125279	20.609383
62.895450	2299.855412	20.614400
62.656118	2297.486276	20.619418
62.853284	2295.611144	20.624435
62.877065	2306.491998	20.629453
63.118928	2331.263053	20.634471
63.257300	2324.740450	20.639488
63.240859	2330.887694	20.644506
63.548715	2327.403557	20.649523
63.373344	2332.694512	20.654541
63.344634	2331.607336	20.659559
63.749519	2338.922393	20.664576
63.746633	2356.414237	20.669594
63.646438	2357.790995	20.674611
63.829466	2355.979626	20.679629
63.914883	2367.521955	20.684647
64.225776	2356.569328	20.689664
63.834205	2347.345327	20.694682
64.265238	2351.708700	20.699699
64.513877	2352.826291	20.704717
64.432543	2346.986674	20.709735
64.570245	2342.437470	20.714752
64.350274	2356.958207	20.719770
64.448625	2351.774574	20.724787
64.528602	2348.923997	20.729805
64.339126	2351.353818	20.734823
64.754181	2353.466226	20.739840
64.940573	2369.513585	20.744858
65.004992	2377.165967	20.749875
65.367422	2377.716990	20.754893
65.068351	2379.138615	20.759911
65.246482	2364.662644	20.764928
64.900147	2367.556349	20.769946
64.797217	2373.395533	20.774963
65.086564	2378.192319	20.779981
64.835709	2382.758014	20.784999
65.137781	2383.577346	20.790016
65.104403	2378.723483	20.795034
65.012225	2393.139941	20.800051
65.659560	2396.883496	20.805069
65.598253	2397.044300	20.810087
66.004177	2400.881525	20.815104
65.907470	2401.754539	20.820122
65.960021	2397.738782	20.825139
66.258673	2402.150158	20.830157
65.916864	2388.299184	20.835175
66.404053	2395.260419	20.840192
66.216851	2393.922799	20.845210
66.261560	2396.688522	20.850227
66.053097	2402.377533	20.855245
66.087639	2404.924860	20.860263
66.401292	2409.882584	20.865280
66.301846	2395.137746	20.870298
66.556952	2399.851645	20.875315
66.475617	2395.606557	20.880333
66.229805	2403.047905	20.885351
66.434945	2390.691517	20.890368
66.399555	2404.507580	20.895386
66.757154	2414.614890	20.900403
67.169287	2415.104896	20.905421
66.964340	2414.509229	20.910439
67.243518	2407.619867	20.915456
66.963857	2420.436740	20.920474
67.150837	2413.598528	20.925491
67.328585	2408.632791	20.930509
66.945254	2415.926129	20.935527
67.014197	2421.187530	20.940544
67.034476	2415.058941	20.945562
67.133573	2439.035361	20.950579
67.404401	2437.146001	20.955597
67.328099	2446.315566	20.960615
67.448233	2438.418331	20.965632
67.246397	2451.919173	20.970650
67.328762	2451.510407	20.975667
67.671795	2457.228254	20.980685
67.521868	2477.521560	20.985703
67.891449	2461.826227	20.990720
67.633205	2465.464789	20.995738
67.766243	2461.928179	21.000755
67.994839	2465.364954	21.005773
68.016625	2478.313276	21.010791
68.134326	2495.464355	21.015808
68.343777	2502.403293	21.020826
68.185017	2486.344153	21.025843
68.802732	2492.900651	21.030861
68.442489	2501.553636	21.035879
68.796642	2485.643905	21.040896
69.326406	2481.991351	21.045914
69.311663	2489.390791	21.050931
69.668937	2470.669017	21.055949
69.670141	2477.500030	21.060967
69.569972	2457.151473	21.065984
69.613375	2452.970287	21.071002
69.395396	2439.914074	21.076019
69.621201	2426.540402	21.081037
69.295104	2443.393517	21.086055
69.254098	2435.110451	21.091072
69.445405	2438.935717	21.096090
69.250600	2437.635185	21.101107
69.374367	2436.350212	21.106125
69.205381	2446.941931	21.111143
69.593169	2457.865545	21.116160
69.776844	2471.342883	21.121178
69.729415	2469.283965	21.126195
69.831784	2465.668196	21.131213
69.887443	2475.756042	21.136231
70.027661	2471.863497	21.141248
70.246509	2473.177396	21.146266
69.745656	2476.476346	21.151283
70.238995	2472.222735	21.156301
70.068625	2500.213102	21.161319
70.160229	2502.388347	21.166336
70.731905	2498.685120	21.171354
70.268483	2509.032497	21.176371
70.325311	2502.045399	21.181389
70.461782	2507.657040	21.186407
70.563177	2505.518655	21.191424
70.673618	2514.542650	21.196442
70.600832	2534.961011	21.201459
71.208397	2528.215452	21.206477
70.836735	2537.264861	21.211495
70.910171	2528.388289	21.216512
71.258023	2523.308019	21.221530
71.032200	2531.379993	21.226547
71.354182	2523.092458	21.231565
71.020230	2533.987650	21.236583
71.369166	2548.308101	21.241600
71.790489	2553.064896	21.246618
71.254306	2560.787268	21.251635
71.994794	2556.378380	21.256653
71.780287	2554.317296	21.261671
71.872712	2567.364587	21.266688
71.742981	2565.661084	21.271706
71.449424	2562.218189	21.276723
71.552157	2559.646482	21.281741
71.595606	2567.511114	21.286759
71.848277	2583.897302	21.291776
71.983539	2590.386777	21.296794
72.423475	2583.841898	21.301811
72.620013	2586.124917	21.306829
72.725189	2589.735784	21.311847
72.815197	2598.156501	21.316864
72.618376	2574.079966	21.321882
72.625402	2582.611715	21.326899
72.473416	2582.743495	21.331917
72.491976	2579.858200	21.336935
72.504558	2583.478550	21.341952
72.957054	2590.745655	21.346970
72.737495	2609.089977	21.351987
73.117757	2595.081798	21.357005
73.365671	2595.724308	21.362023
73.606880	2599.828736	21.367040
73.835670	2583.535390	21.372058
73.416457	2594.479049	21.377075
73.902202	2592.502373	21.382093
74.179322	2592.574253	21.387111
73.884541	2569.935730	21.392128
73.853919	2558.352681	21.397146
73.572640	2564.996813	21.402163
73.791889	2555.505804	21.407181
73.822654	2574.300237	21.412199
73.676144	2595.149061	21.417216
74.215791	2587.385580	21.422234
73.894758	2597.827466	21.427251
74.192379	2592.662605	21.432269
74.095750	2586.715591	21.437287
74.305303	2587.134543	21.442304
74.226108	2589.205503	21.447322
74.038842	2600.068488	21.452339
74.241287	2603.605708	21.457357
74.305510	2623.356893	21.462375
74.635827	2632.739316	21.467392
74.672343	2616.357019	21.472410
74.506428	2609.853372	21.477427
74.696524	2621.580078	21.482445
75.212971	2619.959733	21.487463
74.735607	2621.761424	21.492480
75.368496	2634.695715	21.497498
75.292114	2638.881286	21.502515
75.732245	2633.967150	21.507533
75.735397	2632.745517	21.512551
75.539464	2624.534165	21.517568
75.616370	2622.199823	21.522586
75.744797	2629.166459	21.527603
75.549484	2629.899566	21.532621
75.768479	2625.899791	21.537639
75.538216	2628.253751	21.542656
76.086665	2623.423589	21.547674
75.908331	2616.286144	21.552691
76.116833	2620.534210	21.557709
75.974791	2628.552149	21.562727
76.029315	2656.303833	21.567744
76.414573	2643.983454	21.572762
76.385124	2650.070779	21.577779
76.342458	2652.590425	21.582797
76.343931	2652.317939	21.587815
76.469641	2655.429713	21.592832
76.810692	2648.237428	21.597850
76.265183	2658.267820	21.602867
76.412178	2664.840419	21.607885
76.623630	2671.951945	21.612903
76.883622	2678.533725	21.617920
77.052806	2668.385184	21.622938
76.691172	2684.538520	21.627955
76.877460	2676.531740	21.632973
77.181875	2698.067216	21.637991
77.256134	2701.019824	21.643008
77.382383	2703.316905	21.648026
77.551255	2697.148940	21.653043
77.780242	2702.245641	21.658061
77.883195	2705.085207	21.663079
77.551662	2706.238224	21.668096
77.875535	2698.931048	21.673114
77.759276	2703.909923	21.678131
77.838859	2702.622822	21.683149
78.019407	2699.171182	21.688167
77.703640	2696.202840	21.693184
77.857989	2704.388893	21.698202
78.200280	2719.551599	21.703219
78.475688	2730.838200	21.708237
78.335924	2728.385908	21.713255
78.117995	2739.150142	21.718272
78.234206	2735.293807	21.723290
78.473364	2738.373356	21.728307
78.456757	2734.566656	21.733325
78.784824	2751.197593	21.738343
79.313704	2764.555997	21.743360
79.353607	2759.303198	21.748378
79.612478	2748.777866	21.753395
79.721164	2737.512890	21.758413
79.503670	2720.830948	21.763431
79.526957	2724.494042	21.768448
79.785517	2714.121549	21.773466
79.503062	2714.559676	21.778483
79.652324	2690.600254	21.783501
79.959761	2705.968752	21.788519
79.784286	2704.695694	21.793536
79.797698	2703.871586	21.798554
79.756345	2706.949716	21.803571
79.924918	2707.934570	21.808589
79.852712	2720.774299	21.813607
79.949899	2738.091663	21.818624
79.780196	2732.218553	21.823642
79.992142	2746.559593	21.828659
79.984220	2745.218525	21.833677
80.108807	2744.614534	21.838695
80.511829	2763.742625	21.843712
80.461649	2762.977511	21.848730
80.452610	2769.068183	21.853747
80.583480	2769.149410	21.858765
80.395578	2757.050588	21.863783
80.460072	2771.931543	21.868800
80.796888	2782.645342	21.873818
81.009650	2786.825420	21.878835
81.661176	2782.397790	21.883853
82.021509	2760.672218	21.888871
81.888177	2774.297788	21.893888
81.848449	2743.348791	21.898906
81.958726	2732.544605	21.903923
81.839575	2735.205724	21.908941
82.237669	2727.688943	21.913959
81.737605	2727.825028	21.918976
81.958697	2724.486335	21.923994
82.337812	2726.913844	21.929011
82.239870	2718.802697	21.934029
82.191386	2723.121064	21.939047
81.953909	2725.233704	21.944064
82.255529	2722.001320	21.949082
82.266443	2727.513429	21.954099
82.075540	2735.582067	21.959117
82.067522	2729.921469	21.964135
81.932923	2754.076595	21.969152
82.303651	2754.862490	21.974170
82.744034	2755.015511	21.979187
82.124795	2755.885619	21.984205
82.728097	2760.125198	21.989223
82.564598	2785.978193	21.994240
82.890127	2791.162034	21.999258
82.864747	2787.255592	22.004275
83.030840	2788.495211	22.009293
83.132625	2786.733518	22.014311
83.070583	2790.866744	22.019328
83.068354	2796.522803	22.024346
83.448083	2808.864631	22.029363
83.458364	2813.741796	22.034381
83.732503	2822.499379	22.039399
83.610836	2828.014266	22.044416
83.769365	2828.917722	22.049434
83.955308	2820.169538	22.054451
83.565113	2823.138729	22.059469
83.857249	2804.628969	22.064487
83.512831	2822.736010	22.069504
84.006186	2830.634276	22.074522
84.181819	2843.247469	22.079539
83.669464	2848.287497	22.084557
84.279328	2843.867956	22.089575
84.544764	2860.392482	22.094592
84.512581	2865.199550	22.099610
84.886745	2865.890780	22.104627
84.786481	2870.224486	22.109645
85.007695	2866.706598	22.114663
85.186021	2865.675532	22.119680
85.246157	2861.016621	22.124698
85.330402	2866.062624	22.129715
85.067423	2864.081212	22.134733
85.568924	2861.239231	22.139751
85.110732	2860.094649	22.144768
85.455197	2870.712744	22.149786
85.451324	2879.496878	22.154803
85.319983	2885.638239	22.159821
85.711018	2890.423011	22.164839
85.687010	2878.060619	22.169856
86.165013	2875.432003	22.174874
86.252680	2887.091676	22.179891
85.958401	2881.834136	22.184909
85.921915	2887.103769	22.189927
86.139308	2897.348880	22.194944
86.073792	2916.948366	22.199962
86.110571	2915.156516	22.204979
86.182983	2913.899332	22.209997
86.517831	2913.901380	22.215015
86.953448	2921.291535	22.220032
86.615535	2934.314980	22.225050
87.468565	2933.904898	22.230067
87.091946	2938.294003	22.235085
87.361254	2941.307161	22.240103
87.127037	2936.555405	22.245120
87.459181	2933.643520	22.250138
87.683494	2930.218022	22.255155
87.499240	2942.233187	22.260173
87.336411	2939.005899	22.265191
87.611763	2939.557244	22.270208
87.694079	2942.427845	22.275226
87.692374	2935.810936	22.280243
87.242971	2932.499771	22.285261
87.735738	2944.814259	22.290279
87.574334	2959.197073	22.295296
87.857114	2962.524160	22.300314
88.138497	2959.678978	22.305331
87.719789	2968.528958	22.310349
88.215497	2972.245100	22.315367
88.387697	2994.210865	22.320384
88.284420	2989.394809	22.325402
88.460385	2990.989523	22.330419
88.486496	3001.854334	22.335437
88.759853	2986.620171	22.340455
88.603539	2992.651149	22.345472
88.720921	2992.132211	22.350490
88.969116	3001.949012	22.355507
88.909855	3024.504905	22.360525
88.974906	3022.924108	22.365543
89.214836	3017.841537	22.370560
89.362322	3026.237972	22.375578
89.414716	3014.817572	22.380595
89.351900	3016.612616	22.385613
89.633914	3017.917246	22.390631
90.028399	3049.057884	22.395648
90.028340	3037.076849	22.400666
90.227103	3032.512178	22.405683
89.955361	3037.418961	22.410701
90.408007	3032.731381	22.415719
90.216187	3031.334624	22.420736
89.982112	3041.668251	22.425754
90.378125	3032.231441	22.430771
90.240330	3034.433861	22.435789
90.615220	3042.654705	22.440807
90.457558	3027.128723	22.445824
90.132186	3055.259635	22.450842
90.524837	3056.656126	22.455859
90.618840	3070.199285	22.460877
90.596659	3059.851175	22.465895
90.692710	3070.609519	22.470912
90.544715	3083.803509	22.475930
91.102083	3091.998775	22.480947
91.173615	3098.135639	22.485965
91.368187	3110.126165	22.490983
91.713739	3118.796843	22.496000
91.642157	3125.901676	22.501018
92.009483	3125.179369	22.506035
91.949334	3119.744242	22.511053
92.166314	3122.018038	22.516071
92.233402	3116.715321	22.521088
92.395824	3125.442819	22.526106
92.619592	3109.461204	22.531123
92.430759	3106.085827	22.536141
92.660022	3108.244972	22.541159
92.527450	3113.054626	22.546176
92.233404	3121.775696	22.551194
92.574808	3107.079760	22.556211
92.363976	3121.411877	22.561229
92.744129	3125.491779	22.566247
92.885907	3130.424360	22.571264
92.680451	3130.232325	22.576282
92.730922	3137.351920	22.581299
92.970374	3129.175430	22.586317
93.066940	3157.012758	22.591335
93.068281	3163.636945	22.596352
93.157637	3162.858069	22.601370
93.378676	3155.477607	22.606387
93.781497	3166.348434	22.611405
93.564412	3192.066111	22.616423
94.038672	3190.677941	22.621440
93.921801	3193.060780	22.626458
94.434589	3188.143061	22.631475
94.439448	3176.044556	22.636493
94.252892	3183.566984	22.641511
94.383496	3171.630671	22.646528
94.479437	3188.618400	22.651546
94.949790	3181.036634	22.656563
94.913390	3175.329800	22.661581
94.866416	3172.250938	22.666599
94.872435	3177.846311	22.671616
94.838581	3175.297992	22.676634
94.963378	3177.901317	22.681651
95.044938	3176.818986	22.686669
94.982439	3177.175682	22.691687
95.293763	3188.612566	22.696704
95.049445	3205.206823	22.701722
95.635703	3204.091403	22.706739
95.392017	3208.248233	22.711757
95.444511	3208.158614	22.716775
95.320367	3208.485395	22.721792
95.483691	3219.359838	22.726810
95.867882	3223.069771	22.731827
96.088829	3233.053466	22.736845
96.170109	3235.265965	22.741863
96.597410	3229.465115	22.746880
95.966806	3228.345220	22.751898
96.275987	3231.233688	22.756915
96.391103	3235.114338	22.761933
96.316428	3234.465880	22.766951
96.887884	3240.797299	22.771968
96.533544	3264.332192	22.776986
96.738344	3253.499731	22.782003
96.858056	3265.404385	22.787021
96.625839	3266.211375	22.792039
97.116240	3267.484150	22.797056
96.840448	3281.381499	22.802074
97.657842	3277.645921	22.807091
98.053012	3269.513169	22.812109
98.244365	3272.680306	22.817127
98.297939	3269.041357	22.822144
98.128276	3269.137098	22.827162
98.230773	3261.526658	22.832179
97.956980	3248.794029	22.837197
98.059723	3272.699075	22.842215
98.596285	3256.334191	22.847232
98.739808	3268.514837	22.852250
98.646008	3260.171595	22.857267
98.900403	3269.545368	22.862285
98.840842	3262.257951	22.867303
99.202503	3261.851177	22.872320
98.836061	3248.868961	22.877338
98.866479	3255.761608	22.882355
98.901130	3263.893827	22.887373
98.864414	3266.955153	22.892391
98.808584	3261.350344	22.897408
98.864011	3252.990968	22.902426
98.954186	3273.298558	22.907443
99.206307	3270.811367	22.912461
99.342579	3286.964864	22.917479
99.610700	3287.660746	22.922496
99.668529	3283.952970	22.927514
99.622006	3290.394202	22.932531
99.812560	3300.514500	22.937549
99.766780	3301.683851	22.942567
100.051995	3297.208684	22.947584
100.144762	3311.995684	22.952602
100.082470	3315.541238	22.957619
100.208375	3322.531047	22.962637
100.428626	3343.462449	22.967655
100.427166	3341.894249	22.972672
100.490722	3334.930859	22.977690
100.655760	3340.027374	22.982707
100.768365	3345.802750	22.987725
101.146148	3364.981452	22.992743
101.246949	3363.131661	22.997760
101.329354	3366.195652	23.002778
101.405016	3353.008758	23.007795
101.578201	3353.096343	23.012813
101.508401	3357.813742	23.017831
101.678675	3354.659365	23.022848
101.456836	3362.054658	23.027866
101.592017	3362.644278	23.032883
101.913746	3362.799312	23.037901
101.597163	3386.829345	23.042919
101.740688	3389.126020	23.047936
101.715465	3389.760806	23.052954
102.067029	3387.442522	23.057971
102.147273	3403.346369	23.062989
102.392865	3410.441536	23.068007
102.326614	3421.898033	23.073024
102.487056	3408.450520	23.078042
102.582228	3411.941576	23.083059
102.489913	3430.044824	23.088077
102.538658	3447.755714	23.093095
103.002457	3447.267387	23.098112
103.149288	3446.790002	23.103130
103.401527	3465.817234	23.108147
104.079787	3460.238399	23.113165
103.974063	3462.303646	23.118183
104.216704	3449.318471	23.123200
103.878946	3444.199475	23.128218
103.678700	3434.180347	23.133235
104.333503	3444.053092	23.138253
104.236206	3460.774776	23.143271
104.344964	3456.758069	23.148288
104.170953	3453.545524	23.153306
104.298868	3461.320184	23.158323
104.275061	3455.982453	23.163341
104.601550	3456.268601	23.168359
104.627772	3453.257055	23.173376
104.456081	3479.056251	23.178394
104.559237	3490.542523	23.183411
105.123254	3482.037470	23.188429
104.729770	3493.744093	23.193447
105.163608	3499.117676	23.198464
105.119977	3512.653775	23.203482
105.221906	3513.564317	23.208499
105.461713	3507.107050	23.213517
105.603128	3505.908832	23.218535
105.674378	3498.771237	23.223552
106.071785	3515.340282	23.228570
106.077269	3531.314172	23.233587
106.308315	3528.246915	23.238605
106.110911	3530.182509	23.243623
106.557730	3521.313405	23.248640
106.871146	3523.555090	23.253658
106.361353	3538.001847	23.258675
106.740282	3522.937042	23.263693
106.654459	3532.793940	23.268711
107.004271	3529.000962	23.273728
107.019285	3527.665070	23.278746
106.880560	3539.228196	23.283763
107.167804	3547.321733	23.288781
107.222417	3563.161492	23.293799
107.398693	3560.169480	23.298816
107.442173	3560.986183	23.303834
107.338129	3565.605387	23.308851
107.585801	3556.165356	23.313869
107.580724	3570.919645	23.318887
107.686332	3586.029217	23.323904
107.873654	3583.521247	23.328922
107.961257	3595.934696	23.333939
107.922029	3598.653945	23.338957
107.946975	3606.187099	23.343975
108.208506	3609.235150	23.348992
109.086239	3598.668216	23.354010
109.086983	3603.008962	23.359027
109.524960	3587.138915	23.364045
109.726503	3588.281753	23.369063
109.879396	3576.394583	23.374080
110.182075	3552.180758	23.379098
109.897232	3551.058497	23.384115
109.808425	3543.430495	23.389133
109.796034	3546.307498	23.394151
109.743608	3531.711660	23.399168
109.428577	3531.046042	23.404186
109.580344	3538.403345	23.409203
109.899098	3537.348506	23.414221
109.822394	3542.636068	23.419239
109.961019	3549.816407	23.424256
110.073158	3547.379213	23.429274
109.892902	3559.998979	23.434291
109.936060	3568.638661	23.439309
110.148235	3576.953375	23.444327
109.934071	3574.297146	23.449344
110.351881	3585.798132	23.454362
110.096052	3604.495357	23.459379
110.447631	3618.763991	23.464397
110.242385	3629.383009	23.469415
110.477927	3637.371787	23.474432
110.896232	3641.428556	23.479450
110.836939	3673.271915	23.484467
111.288551	3670.873964	23.489485
111.442230	3682.672492	23.494503
111.157115	3678.132140	23.499520
111.370048	3691.997454	23.504538
111.575267	3701.923427	23.509555
111.834637	3698.367513	23.514573
111.919187	3706.800368	23.519591
112.055485	3727.713557	23.524608
112.460817	3725.281158	23.529626
112.408008	3728.803966	23.534643
112.943741	3727.794167	23.539661
113.220636	3728.941818	23.544679
112.715149	3726.630865	23.549696
112.953875	3721.190351	23.554714
113.197913	3731.300859	23.559731
113.473216	3737.412772	23.564749
113.407035	3739.828219	23.569767
113.599974	3740.619306	23.574784
113.536923	3741.801010	23.579802
113.416764	3762.220579	23.584819
113.847123	3744.197434	23.589837
113.803836	3756.892245	23.594855
113.768950	3749.522144	23.599872
113.933872	3765.337475	23.604890
113.837129	3785.358251	23.609907
114.169645	3783.237196	23.614925
114.149526	3780.599870	23.619943
114.314290	3788.364238	23.624960
114.975850	3810.067519	23.629978
114.977590	3810.348583	23.634995
114.753736	3800.679250	23.640013
115.082208	3808.514071	23.645031
114.873838	3799.940337	23.650048
114.558516	3806.079165	23.655066
114.777534	3827.952487	23.660083
115.285683	3826.331833	23.665101
115.491199	3835.497113	23.670119
115.296369	3829.369068	23.675136
115.699854	3845.693723	23.680154
115.626933	3855.450636	23.685171
115.946984	3861.376397	23.690189
115.947544	3856.748747	23.695207
115.702948	3867.979663	23.700224
116.442182	3871.187384	23.705242
116.553023	3888.899872	23.710259
116.732531	3881.026300	23.715277
116.849414	3888.947120	23.720295
116.844910	3883.699749	23.725312
117.236021	3872.216525	23.730330
117.049935	3886.641304	23.735347
116.997970	3882.823269	23.740365
117.034368	3877.791573	23.745383
117.258475	3883.347410	23.750400
117.757018	3891.509961	23.755418
117.721826	3904.056282	23.760435
117.572918	3893.085287	23.765453
117.727694	3904.506979	23.770471
117.285992	3905.033417	23.775488
117.715357	3907.985516	23.780506
117.684546	3931.434172	23.785523
117.803935	3936.516419	23.790541
118.240363	3946.947505	23.795559
118.207570	3959.365894	23.800576
118.298177	3962.772388	23.805594
118.585155	3986.606956	23.810611
118.833063	3989.272254	23.815629
119.110903	3993.147707	23.820647
118.998679	3999.944292	23.825664
119.157811	4003.492578	23.830682
119.348753	4001.578512	23.835699
119.590367	4005.808857	23.840717
120.123161	4012.475808	23.845735
119.955756	4019.002792	23.850752
120.402763	4010.224736	23.855770
120.331160	4020.213848	23.860787
120.453013	4000.516634	23.865805
120.309033	4006.632970	23.870823
120.189577	4006.844797	23.875840
120.673349	4003.594877	23.880858
120.529669	4007.022992	23.885875
120.408118	4009.133859	23.890893
120.882203	4019.924928	23.895911
121.078115	4033.446474	23.900928
121.014399	4021.598904	23.905946
121.123722	4031.411478	23.910963
121.180290	4035.684790	23.915981
121.345292	4041.185143	23.920999
121.428307	4058.328743	23.926016
121.686838	4062.127491	23.931034
121.880513	4061.498189	23.936051
121.510416	4056.527297	23.941069
122.167019	4072.390772	23.946087
122.128033	4090.046092	23.951104
122.351704	4088.301013	23.956122
122.100298	4096.124459	23.961139
122.375182	4092.368213	23.966157
122.663015	4087.489968	23.971175
123.062156	4103.089131	23.976192
123.260200	4107.005832	23.981210
123.302173	4108.837136	23.986227
123.545742	4114.578826	23.991245
123.757503	4104.090343	23.996263
123.555917	4109.140544	24.001280
123.730235	4097.979448	24.006298
123.810331	4110.298082	24.011315
123.409177	4102.624458	24.016333
123.622856	4107.728499	24.021351
123.650968	4126.096831	24.026368
123.819919	4126.255610	24.031386
123.642117	4141.194676	24.036403
123.802789	4139.545112	24.041421
124.109953	4158.324655	24.046439
124.468071	4152.843281	24.051456
125.026473	4154.540728	24.056474
124.687703	4164.923204	24.061491
124.869482	4154.577486	24.066509
125.613311	4164.914711	24.071527
126.250518	4162.989071	24.076544
127.008999	4134.073102	24.081562
126.446958	4139.090290	24.086579
125.958298	4129.719915	24.091597
126.803502	4128.711822	24.096615
126.205265	4105.808850	24.101632
126.031750	4099.577928	24.106650
126.634343	4100.504921	24.111667
126.176341	4111.499390	24.116685
126.553378	4101.759146	24.121703
126.448998	4121.699326	24.126720
126.629736	4121.226131	24.131738
126.511228	4128.446320	24.136755
126.471338	4132.480533	24.141773
126.888501	4135.777275	24.146791
126.514022	4153.694359	24.151808
126.726308	4160.117744	24.156826
127.109472	4174.263510	24.161843
127.026108	4189.471222	24.166861
127.417245	4187.869980	24.171879
127.056533	4208.527775	24.176896
127.642317	4214.358321	24.181914
127.610598	4223.074598	24.186931
127.383284	4230.742115	24.191949
127.855043	4246.362430	24.196967
128.287133	4252.242158	24.201984
128.680810	4236.113819	24.207002
129.226709	4251.194177	24.212019
129.176340	4257.710079	24.217037
129.309653	4255.102695	24.222055
129.736188	4261.114079	24.227072
129.766104	4253.945997	24.232090
129.560168	4248.513441	24.237107
129.751843	4249.492983	24.242125
130.207683	4257.191099	24.247143
129.920797	4258.473829	24.252160
129.923557	4247.481317	24.257178
130.069695	4256.698847	24.262195
130.093518	4259.879853	24.267213
130.290915	4256.656212	24.272231
129.975906	4259.406838	24.277248
130.242412	4261.985221	24.282266
130.482734	4272.343194	24.287283
130.397646	4284.579164	24.292301
130.861054	4284.798476	24.297319
130.808090	4293.171811	24.302336
130.872576	4301.082254	24.307354
131.193520	4307.454566	24.312371
131.102319	4301.522532	24.317389
131.622090	4306.129242	24.322407
131.617737	4329.515820	24.327424
132.049585	4327.803846	24.332442
132.103949	4326.811403	24.337459
132.048016	4332.187920	24.342477
132.310753	4323.098921	24.347495
132.178491	4322.289486	24.352512
132.151443	4336.526410	24.357530
132.479851	4349.134728	24.362547
132.792706	4358.039525	24.367565
133.106179	4360.428988	24.372583
133.036961	4354.676775	24.377600
132.915711	4348.184271	24.382618
132.970297	4354.670171	24.387635
133.261650	4372.712322	24.392653
133.311269	4379.388852	24.397671
133.473864	4388.076078	24.402688
133.647188	4391.829215	24.407706
133.560952	4387.781674	24.412723
133.738650	4406.279044	24.417741
133.854595	4407.187703	24.422759
134.024144	4410.123226	24.427776
133.709348	4418.919731	24.432794
134.178770	4427.743422	24.437811
134.060463	4446.771214	24.442829
134.160584	4452.041509	24.447847
134.296385	4471.027889	24.452864
134.422139	4485.779803	24.457882
135.362461	4500.191602	24.462899
135.040626	4505.776175	24.467917
135.585674	4494.429544	24.472935
135.422672	4499.045825	24.477952
135.754155	4516.574299	24.482970
136.113967	4525.946273	24.487987
136.220660	4534.497964	24.493005
136.368100	4523.570994	24.498023
136.700374	4523.478188	24.503040
136.527657	4532.766983	24.508058
136.431479	4528.948656	24.513075
136.432479	4544.224595	24.518093
136.795146	4544.170840	24.523111
136.894949	4553.432471	24.528128
137.132452	4547.503996	24.533146
137.293019	4553.210815	24.538163
137.597563	4580.303784	24.543181
137.772476	4576.074975	24.548199
138.050771	4572.929969	24.553216
138.170903	4578.184380	24.558234
138.222643	4573.197164	24.563251
137.771215	4583.592335	24.568269
138.289617	4571.327868	24.573287
138.464906	4578.970387	24.578304
138.449457	4589.505745	24.583322
138.832204	4593.639949	24.588339
138.981684	4592.065441	24.593357
138.846306	4598.201053	24.598375
138.971133	4598.415999	24.603392
139.369798	4613.519601	24.608410
139.470077	4620.628051	24.613427
139.560561	4624.876200	24.618445
139.652633	4618.583608	24.623463
139.651222	4620.927785	24.628480
139.132439	4631.624786	24.633498
139.773565	4644.729504	24.638515
139.926272	4652.779034	24.643533
140.097799	4654.163599	24.648551
140.249810	4678.099618	24.653568
140.000013	4682.328727	24.658586
140.860295	4698.292090	24.663603
140.635752	4710.345228	24.668621
140.682740	4713.673686	24.673639
140.788574	4707.422874	24.678656
140.887669	4719.994783	24.683674
141.312352	4733.640364	24.688691
141.474165	4732.840316	24.693709
141.819076	4736.261027	24.698727
142.035923	4745.373375	24.703744
142.217704	4769.021067	24.708762
142.317732	4766.624682	24.713779
142.263952	4773.678473	24.718797
142.332516	4761.221636	24.723815
142.699022	4765.258567	24.728832
142.550555	4764.906218	24.733850
142.908504	4760.857218	24.738867
142.971210	4774.022730	24.743885
143.343357	4783.867704	24.748903
143.270189	4789.674881	24.753920
143.161730	4783.567546	24.758938
143.651975	4780.975577	24.763955
143.467363	4789.456896	24.768973
143.664470	4809.343907	24.773991
144.067235	4802.463287	24.779008
143.876624	4819.077097	24.784026
144.144944	4814.953198	24.789043
144.059191	4823.561441	24.794061
144.289045	4835.457256	24.799079
144.384807	4840.960735	24.804096
144.543638	4845.321231	24.809114
144.814356	4862.923983	24.814131
144.821181	4871.926397	24.819149
145.065611	4866.682613	24.824167
145.387996	4869.158881	24.829184
145.977005	4887.584527	24.834202
146.526656	4869.316609	24.839219
146.481478	4875.136492	24.844237
146.768064	4871.252897	24.849255
147.109230	4867.924123	24.854272
146.567707	4854.191164	24.859290
147.207539	4841.389672	24.864307
147.069178	4842.784800	24.869325
147.258333	4829.272234	24.874343
147.370849	4829.012760	24.879360
147.056793	4842.869409	24.884378
147.321254	4857.041034	24.889395
147.107858	4858.412405	24.894413
147.146304	4867.030747	24.899431
147.668605	4868.198740	24.904448
147.597072	4891.940693	24.909466
147.846386	4887.278095	24.914483
148.066128	4892.334133	24.919501
148.291027	4892.607271	24.924519
148.260133	4901.823098	24.929536
147.919868	4923.491228	24.934554
148.744345	4909.876952	24.939571
149.101690	4912.821527	24.944589
149.072898	4935.599561	24.949607
149.557012	4931.478361	24.954624
149.515859	4937.577969	24.959642
149.743369	4933.419868	24.964659
149.676209	4948.142847	24.969677
149.337099	4936.159212	24.974695
149.841783	4938.672140	24.979712
149.559565	4959.465934	24.984730
149.987804	4974.297200	24.989747
150.055593	4975.458828	24.994765
150.015253	4999.784855	24.999783
150.492685	4999.252093	25.004800
150.544416	4998.590035	25.009818
150.513784	5021.284229	25.014835
150.736997	5024.755157	25.019853
150.994871	5038.069596	25.024871
151.562144	5049.904776	25.029888
151.633571	5057.357659	25.034906
151.538411	5068.411413	25.039923
151.577276	5064.595716	25.044941
151.621145	5066.755233	25.049959
152.165548	5071.617190	25.054976
152.308721	5091.897854	25.059994
152.617927	5087.248871	25.065011
152.884840	5082.088700	25.070029
153.099579	5081.178243	25.075047
153.127919	5075.606445	25.080064
153.347555	5085.458052	25.085082
153.189347	5077.204089	25.090099
153.443298	5068.397283	25.095117
153.283771	5093.082702	25.100135
153.743761	5082.468837	25.105152
153.624790	5091.320592	25.110170
153.328143	5094.733014	25.115187
153.849402	5104.206093	25.120205
153.988942	5123.135149	25.125223
154.299614	5113.878642	25.130240
154.489947	5134.001098	25.135258
154.523380	5136.660890	25.140275
154.742383	5155.290103	25.145293
154.784949	5139.807506	25.150311
154.825510	5143.630142	25.155328
154.968668	5169.519190	25.160346
155.087588	5176.469643	25.165363
155.579322	5184.912810	25.170381
155.939480	5197.652787	25.175399
156.306257	5190.318826	25.180416
155.745972	5201.138878	25.185434
156.289107	5204.114853	25.190451
156.585060	5209.031530	25.195469
156.331739	5235.947412	25.200487
156.794043	5222.796294	25.205504
156.624873	5232.262114	25.210522
156.727820	5235.823168	25.215539
157.409441	5254.503209	25.220557
157.299940	5269.577694	25.225575
157.296959	5272.227021	25.230592
157.165461	5275.811293	25.235610
157.438811	5298.549092	25.240627
157.683173	5301.091952	25.245645
157.851492	5323.631445	25.250663
158.154733	5314.639107	25.255680
158.656936	5327.489473	25.260698
158.192686	5336.655494	25.265715
158.408261	5348.205961	25.270733
158.505326	5366.422520	25.275751
158.822806	5374.136307	25.280768
158.815812	5381.111713	25.285786
159.118321	5389.340711	25.290803
159.454233	5395.126597	25.295821
159.767221	5417.464978	25.300839
160.130597	5420.559864	25.305856
160.148209	5421.036003	25.310874
160.213708	5419.773864	25.315891
160.658785	5435.291117	25.320909
160.722380	5446.802331	25.325927
160.855224	5441.276044	25.330944
160.636440	5436.268928	25.335962
161.024389	5447.751445	25.340979
161.277592	5458.120664	25.345997
161.382209	5465.215387	25.351015
161.472480	5474.111343	25.356032
161.572566	5471.962144	25.361050
161.787031	5495.888242	25.366067
162.156935	5494.043102	25.371085
162.159427	5511.366669	25.376103
162.301121	5507.903943	25.381120
162.331686	5500.556404	25.386138
162.315985	5531.090856	25.391155
162.554975	5526.313224	25.396173
162.432451	5542.133616	25.401191
162.772632	5544.013982	25.406208
163.248526	5563.412206	25.411226
163.184319	5556.108743	25.416243
163.317208	5551.473962	25.421261
163.452694	5583.256135	25.426279
163.321253	5579.570214	25.431296
163.476691	5595.477572	25.436314
163.776975	5610.440179	25.441331
164.132105	5607.060890	25.446349
164.305970	5627.111104	25.451367
164.500320	5637.814710	25.456384
164.726040	5642.301355	25.461402
164.868128	5635.373122	25.466419
165.003961	5655.467497	25.471437
165.238642	5670.781304	25.476455
165.747318	5661.096990	25.481472
165.982412	5661.111694	25.486490
166.212782	5667.168038	25.491507
166.572606	5683.002140	25.496525
166.851568	5692.956109	25.501543
166.939661	5684.419892	25.506560
167.334140	5686.827605	25.511578
166.957076	5694.014290	25.516595
167.203675	5674.366319	25.521613
167.136401	5684.787369	25.526631
167.110701	5675.601397	25.531648
167.462262	5686.412803	25.536666
167.328709	5699.319505	25.541683
167.896855	5708.003077	25.546701
167.511167	5713.738874	25.551719
167.361544	5721.645445	25.556736
167.673651	5738.961129	25.561754
167.731315	5752.604794	25.566771
168.229389	5779.252605	25.571789
168.574449	5788.593924	25.576807
168.175959	5792.349484	25.581824
168.724490	5800.929253	25.586842
168.809412	5814.744078	25.591859
169.584272	5823.664299	25.596877
169.539480	5836.546123	25.601895
169.747957	5827.292007	25.606912
169.868195	5842.948705	25.611930
170.466416	5860.787203	25.616947
170.478725	5856.219627	25.621965
170.813878	5852.186744	25.626983
170.802445	5864.929155	25.632000
170.829909	5861.325451	25.637018
171.028861	5879.583954	25.642035
171.389584	5874.773387	25.647053
171.347711	5881.476785	25.652071
171.369143	5885.099577	25.657088
171.613422	5902.952834	25.662106
171.748904	5917.366592	25.667123
171.674052	5911.990434	25.672141
172.170731	5911.100815	25.677159
172.344092	5939.265444	25.682176
172.507336	5936.979669	25.687194
172.504379	5951.874852	25.692212
172.961561	5956.598787	25.697229
172.871529	5971.350149	25.702247
172.828913	5978.542818	25.707264
173.534602	5976.968684	25.712282
173.315428	5978.908188	25.717300
173.806567	5979.401744	25.722317
173.871040	5984.487088	25.727335
173.761387	5993.395294	25.732352
174.182965	6016.500941	25.737370
174.296941	6024.422929	25.742388
174.363991	6021.296205	25.747405
174.487940	6032.292957	25.752423
174.513061	6037.184803	25.757440
174.907805	6047.513564	25.762458
175.052619	6056.407873	25.767476
175.234092	6060.162421	25.772493
175.118633	6076.909197	25.777511
175.537805	6083.726669	25.782528
176.005493	6083.073418	25.787546
176.143592	6107.885814	25.792564
175.838876	6107.831124	25.797581
175.990805	6116.791232	25.802599
176.177848	6133.642960	25.807616
176.757354	6144.940570	25.812634
176.613815	6148.401808	25.817652
176.780998	6161.209290	25.822669
177.420287	6157.699179	25.827687
177.451905	6163.913974	25.832704
177.668679	6185.969349	25.837722
177.879554	6197.819730	25.842740
177.947087	6200.503965	25.847757
178.237261	6198.123812	25.852775
178.186946	6218.733436	25.857792
178.382592	6217.291295	25.862810
178.232260	6238.220800	25.867828
178.601340	6254.587948	25.872845
178.837539	6260.453735	25.877863
178.869265	6283.733249	25.882880
179.396100	6281.691030	25.887898
179.470021	6302.294295	25.892916
179.496357	6313.002651	25.897933
180.023149	6324.428082	25.902951
179.857927	6329.951822	25.907968
180.266923	6336.411937	25.912986
180.254191	6360.853615	25.918004
180.648326	6360.641049	25.923021
181.087352	6371.373806	25.928039
180.947571	6379.026239	25.933056
181.348178	6378.421932	25.938074
181.823591	6394.961375	25.943092
182.222257	6396.662788	25.948109
182.598365	6399.523405	25.953127
182.590224	6404.247613	25.958144
182.905597	6394.805276	25.963162
182.898127	6405.531914	25.968180
183.072125	6389.359917	25.973197
183.462910	6392.159021	25.978215
183.153270	6397.310604	25.983232
183.273716	6378.371115	25.988250
183.586688	6391.393211	25.993268
183.609223	6397.652927	25.998285
184.080047	6412.862055	26.003303
183.876775	6416.848388	26.008320
184.341242	6407.393082	26.013338
183.960611	6417.054636	26.018356
184.179811	6428.108298	26.023373
184.414888	6433.931017	26.028391
184.210567	6451.310459	26.033408
184.616217	6455.041239	26.038426
184.831560	6464.124905	26.043444
185.008098	6483.029753	26.048461
185.081752	6485.218384	26.053479
185.376646	6507.291157	26.058496
186.025876	6526.415235	26.063514
185.983925	6519.832255	26.068532
186.038568	6535.193360	26.073549
186.512070	6546.832595	26.078567
186.650962	6546.847537	26.083584
186.854740	6544.743974	26.088602
188.015585	6523.472508	26.093620
188.268862	6516.084338	26.098637
188.298587	6512.250908	26.103655
188.167137	6496.104353	26.108672
188.538454	6492.843486	26.113690
188.391207	6504.619710	26.118708
188.303939	6499.697518	26.123725
188.844226	6501.247813	26.128743
188.620560	6507.889531	26.133760
188.979884	6511.156229	26.138778
188.840475	6511.374944	26.143796
188.991164	6535.633785	26.148813
189.059288	6533.121139	26.153831
189.118310	6540.572847	26.158848
189.455097	6559.322773	26.163866
189.277395	6567.788929	26.168884
189.511962	6584.924669	26.173901
189.643069	6591.474388	26.178919
189.723924	6615.298362	26.183936
190.133016	6628.987568	26.188954
190.510637	6645.057549	26.193972
190.422452	6665.132936	26.198989
190.786636	6664.551213	26.204007
191.086911	6683.113592	26.209024
191.194041	6692.492623	26.214042
191.462589	6717.331556	26.219060
191.293678	6734.169035	26.224077
191.793964	6735.720488	26.229095
191.741332	6761.910118	26.234112
191.968315	6764.378917	26.239130
192.371692	6787.374509	26.244148
192.484612	6790.853918	26.249165
193.038073	6802.933743	26.254183
193.233727	6821.924037	26.259200
193.574850	6820.400170	26.264218
194.285511	6820.836802	26.269236
194.575443	6833.702411	26.274253
194.850791	6825.113985	26.279271
194.982964	6829.576346	26.284288
195.059278	6828.857355	26.289306
195.304855	6836.501896	26.294324
195.399742	6834.443958	26.299341
195.581799	6822.351801	26.304359
195.525256	6837.396135	26.309376
195.251875	6825.546639	26.314394
195.765315	6829.837736	26.319412
195.828595	6842.487390	26.324429
195.951313	6844.524565	26.329447
196.059828	6855.002240	26.334464
196.489695	6863.401462	26.339482
196.595557	6871.836412	26.344500
196.778287	6878.030316	26.349517
196.945070	6881.744181	26.354535
196.829238	6903.981853	26.359552
197.027644	6910.195219	26.364570
196.947421	6926.977206	26.369588
196.947968	6949.167247	26.374605
197.605673	6954.401651	26.379623
197.613562	6981.261337	26.384640
198.151988	6987.431623	26.389658
198.309814	7004.878305	26.394676
198.835668	7001.382927	26.399693
199.171670	7011.941841	26.404711
199.099517	7023.037245	26.409728
199.189783	7028.143057	26.414746
199.793708	7052.179294	26.419764
199.331067	7067.509509	26.424781
199.891589	7059.672263	26.429799
199.829410	7070.491147	26.434816
199.974873	7086.411116	26.439834
200.303098	7093.760064	26.444852
199.981583	7097.873337	26.449869
200.469666	7119.229592	26.454887
200.420427	7144.104672	26.459904
200.787853	7155.235821	26.464922
200.978486	7173.552338	26.469940
201.117477	7187.794171	26.474957
201.312098	7191.135641	26.479975
201.406146	7215.241885	26.484992
201.877733	7226.021015	26.490010
202.270427	7255.029794	26.495028
202.304778	7261.580115	26.500045
202.691865	7271.963727	26.505063
202.800198	7297.402044	26.510080
202.998486	7291.839035	26.515098
203.512229	7321.554059	26.520116
203.469692	7324.945205	26.525133
203.858792	7335.794830	26.530151
204.004576	7345.810570	26.535168
204.407948	7350.831375	26.540186
204.710748	7357.948368	26.545204
204.665258	7373.311169	26.550221
204.706558	7365.823926	26.555239
205.364606	7383.029580	26.560256
205.740119	7391.019070	26.565274
206.283797	7375.231257	26.570292
206.367466	7384.117570	26.575309
206.502691	7383.172153	26.580327
206.702537	7379.084181	26.585344
206.717242	7382.535932	26.590362
206.948669	7394.416090	26.595380
206.936583	7413.890591	26.600397
207.522177	7406.234904	26.605415
207.336694	7402.210167	26.610432
207.267485	7413.306141	26.615450
207.637848	7426.552708	26.620468
207.824620	7436.372651	26.625485
207.741484	7448.308270	26.630503
208.093473	7473.920633	26.635520
208.224783	7474.760756	26.640538
208.654005	7493.279816	26.645556
208.443769	7517.344921	26.650573
208.869956	7534.721599	26.655591
209.201363	7533.446617	26.660608
209.135505	7556.535475	26.665626
209.604754	7551.586648	26.670644
209.487898	7575.362208	26.675661
209.918099	7582.034355	26.680679
210.338013	7616.577524	26.685696
210.543351	7625.236591	26.690714
211.014187	7632.885048	26.695732
210.757616	7640.676433	26.700749
211.104404	7657.585947	26.705767
211.545717	7660.988926	26.710784
211.316636	7671.959619	26.715802
212.041757	7675.013755	26.720820
211.843133	7691.212059	26.725837
212.178939	7701.947911	26.730855
211.992979	7713.795263	26.735872
212.321021	7733.423952	26.740890
212.901743	7744.188454	26.745908
213.016655	7758.551379	26.750925
213.462713	7762.749167	26.755943
213.733476	7775.673866	26.760960
213.682547	7787.468903	26.765978
213.845991	7788.768447	26.770996
213.902543	7797.582302	26.776013
214.083517	7800.403136	26.781031
214.620800	7806.791342	26.786048
214.620710	7820.853626	26.791066
215.103841	7827.124018	26.796084
215.295976	7828.511747	26.801101
215.800782	7822.845634	26.806119
215.762033	7840.277848	26.811136
216.102914	7854.982985	26.816154
216.530567	7851.499807	26.821172
216.147584	7853.925983	26.826189
216.251821	7873.617240	26.831207
216.590019	7875.957457	26.836224
216.531870	7886.565120	26.841242
216.876131	7901.098807	26.846260
216.856259	7926.944621	26.851277
217.197360	7933.024400	26.856295
217.269784	7952.096388	26.861312
217.581527	7980.800134	26.866330
218.100319	7983.471131	26.871348
218.557006	7992.965356	26.876365
218.943990	8014.094639	26.881383
219.600040	8003.939370	26.886400
219.457456	8016.748624	26.891418
219.843909	8018.900458	26.896436
219.883377	8026.159184	26.901453
220.275691	8028.846479	26.906471
220.567745	8028.994305	26.911488
220.349353	8040.665327	26.916506
220.622833	8041.191979	26.921524
220.463454	8061.098205	26.926541
220.701801	8067.309328	26.931559
220.926040	8081.814285	26.936576
220.842542	8098.437356	26.941594
221.288169	8120.870947	26.946612
221.644806	8130.230638	26.951629
221.666046	8140.696880	26.956647
221.960058	8157.666110	26.961664
222.403260	8172.291522	26.966682
222.868811	8170.927247	26.971700
223.103654	8185.165862	26.976717
223.212449	8200.351794	26.981735
223.910159	8217.252433	26.986752
223.399010	8222.531820	26.991770
223.869321	8225.287324	26.996788
224.190792	8235.921153	27.001805
224.677208	8238.692101	27.006823
224.926734	8239.941932	27.011840
224.824545	8249.938791	27.016858
224.908591	8250.608785	27.021876
224.781860	8272.738319	27.026893
225.179522	8285.531278	27.031911
225.404086	8295.563673	27.036928
225.539213	8318.723430	27.041946
225.928003	8326.292118	27.046964
226.128105	8338.923378	27.051981
226.620475	8350.233116	27.056999
227.034580	8358.861834	27.062016
226.733054	8377.926359	27.067034
227.277362	8374.688364	27.072052
227.430042	8392.636844	27.077069
227.469438	8418.357810	27.082087
227.685637	8411.869792	27.087104
227.694338	8441.335256	27.092122
227.923839	8446.126140	27.097140
227.878433	8467.259339	27.102157
228.274882	8487.005205	27.107175
228.794140	8487.583988	27.112192
228.784638	8525.642098	27.117210
229.092499	8524.201591	27.122228
229.647361	8547.109180	27.127245
229.902916	8552.480269	27.132263
230.128198	8544.680680	27.137280
230.398935	8576.354996	27.142298
230.676508	8584.906480	27.147316
230.804789	8590.044289	27.152333
230.924981	8598.662106	27.157351
231.242081	8605.407047	27.162368
231.457691	8627.263559	27.167386
231.666532	8618.208642	27.172404
232.296385	8629.472103	27.177421
232.230499	8643.975363	27.182439
232.567509	8653.908951	27.187456
232.749592	8664.016383	27.192474
232.851771	8656.365596	27.197492
233.070593	8670.167747	27.202509
233.200312	8688.767114	27.207527
233.615500	8697.375355	27.212544
233.464196	8720.346176	27.217562
234.154501	8720.449109	27.222580
234.338911	8731.181667	27.227597
234.330687	8743.367338	27.232615
235.186598	8734.305671	27.237632
235.183199	8757.373283	27.242650
235.864693	8756.154263	27.247668
236.159059	8756.670382	27.252685
236.053938	8754.024687	27.257703
236.639650	8759.109389	27.262720
236.836014	8771.840871	27.267738
237.146887	8769.687717	27.272756
237.122990	8763.972846	27.277773
237.026466	8783.886069	27.282791
237.439538	8788.852158	27.287808
237.649450	8805.791940	27.292826
237.772427	8810.835384	27.297844
238.413219	8805.239290	27.302861
238.234338	8818.605854	27.307879
238.816411	8818.046155	27.312896
238.855105	8825.207692	27.317914
238.939386	8825.851676	27.322932
239.261223	8845.708854	27.327949
239.043040	8857.346561	27.332967
239.344457	8866.336165	27.337984
239.330856	8879.808447	27.343002
239.728494	8895.242455	27.348020
239.870595	8925.408230	27.353037
240.030711	8939.130564	27.358055
240.546486	8949.827905	27.363072
240.644616	8969.703502	27.368090
241.154225	8983.203949	27.373108
241.143040	9010.089126	27.378125
241.486409	9026.053775	27.383143
241.789255	9036.874785	27.388160
241.943378	9055.530393	27.393178
242.241038	9064.475831	27.398196
242.416110	9078.520358	27.403213
242.724808	9094.041023	27.408231
242.859263	9117.922855	27.413248
243.143847	9124.661604	27.418266
243.182774	9146.472558	27.423284
243.593005	9156.724368	27.428301
244.044139	9177.611358	27.433319
244.373880	9179.285937	27.438336
244.456018	9201.852348	27.443354
244.805412	9213.644941	27.448372
245.089502	9213.476636	27.453389
245.036933	9237.638657	27.458407
245.168786	9235.784606	27.463424
245.265080	9264.510706	27.468442
245.404422	9283.864641	27.473460
246.067037	9293.281315	27.478477
245.848403	9319.631919	27.483495
246.006884	9328.020827	27.488512
246.477886	9352.966520	27.493530
246.862057	9370.321465	27.498548
246.916203	9379.288634	27.503565
247.387276	9408.278859	27.508583
247.808207	9426.750344	27.513600
248.251223	9433.146999	27.518618
248.322073	9447.764553	27.523636
248.594568	9466.450602	27.528653
248.508382	9483.776683	27.533671
249.288269	9487.080479	27.538688
249.898919	9504.401090	27.543706
249.623257	9513.739823	27.548724
250.258598	9518.227264	27.553741
250.732119	9539.534048	27.558759
250.758495	9550.683370	27.563776
251.257307	9548.992831	27.568794
251.214616	9555.312681	27.573812
251.465908	9568.469741	27.578829
251.185199	9576.993989	27.583847
251.961240	9584.706911	27.588864
252.731920	9590.334662	27.593882
253.263206	9573.283144	27.598900
253.727286	9570.128361	27.603917
253.440669	9572.916126	27.608935
253.842927	9561.933911	27.613952
253.998381	9564.068411	27.618970
253.978932	9589.431563	27.623988
254.595897	9593.220159	27.629005
254.586710	9606.865632	27.634023
254.493266	9594.809281	27.639040
254.712340	9619.285975	27.644058
255.029680	9633.397159	27.649076
255.371383	9636.609934	27.654093
255.108268	9659.959910	27.659111
255.344317	9659.834247	27.664128
255.644749	9678.341801	27.669146
255.513504	9705.363897	27.674164
256.151804	9725.191645	27.679181
256.115836	9740.793840	27.684199
256.253538	9756.104857	27.689216
256.707081	9779.938597	27.694234
256.792055	9815.134604	27.699252
257.270856	9820.172028	27.704269
257.327857	9848.916732	27.709287
257.429207	9871.429684	27.714304
258.152553	9883.542725	27.719322
258.259527	9913.494821	27.724340
258.789048	9927.869589	27.729357
259.019091	9940.203289	27.734375
259.403002	9957.997724	27.739392
259.892589	9967.449852	27.744410
260.054537	9973.320689	27.749428
260.803659	9969.535492	27.754445
260.753558	9993.943249	27.759463
261.171105	10006.104041	27.764480
261.421211	10018.846493	27.769498
262.667916	9984.926047	27.774516
263.064853	9981.081193	27.779533
263.574805	9977.888774	27.784551
263.413092	9970.469495	27.789568
263.579695	9961.631975	27.794586
263.464723	9951.860423	27.799604
263.440397	9957.321820	27.804621
263.623276	9960.850176	27.809639
263.819342	9954.132481	27.814656
264.039880	9966.036064	27.819674
263.721311	9962.627582	27.824692
264.173765	9973.778884	27.829709
264.190786	9993.998530	27.834727
264.624548	10008.256930	27.839744
264.953016	10018.944360	27.844762
264.659519	10038.671279	27.849780
264.938920	10056.510761	27.854797
264.997106	10080.593411	27.859815
264.980741	10097.772261	27.864832
265.427274	10120.135248	27.869850
265.287778	10149.753737	27.874868
265.848173	10175.478405	27.879885
266.419447	10200.044000	27.884903
266.440484	10223.595743	27.889920
266.927102	10244.282852	27.894938
266.979392	10275.224759	27.899956
267.872831	10289.034393	27.904973
268.044392	10306.685661	27.909991
268.236326	10326.984595	27.915008
269.223588	10338.781547	27.920026
269.232722	10364.727314	27.925044
269.430132	10368.432182	27.930061
269.701526	10388.042824	27.935079
269.912680	10420.561057	27.940096
270.271210	10418.435225	27.945114
270.519143	10435.449196	27.950132
271.185874	10434.951021	27.955149
271.341916	10457.287900	27.960167
271.070454	10478.725228	27.965184
271.455767	10486.616961	27.970202
271.705681	10507.973217	27.975220
271.919351	10533.333000	27.980237
271.923714	10544.483517	27.985255
272.532865	10554.785901	27.990272
272.816406	10580.099484	27.995290
273.208200	10593.978549	28.000308
273.993783	10608.140425	28.005325
274.386981	10611.756095	28.010343
274.396573	10622.166804	28.015360
275.006012	10637.472765	28.020378
274.625966	10648.811702	28.025396
275.058263	10657.192054	28.030413
275.701076	10662.156803	28.035431
275.953531	10675.205070	28.040448
276.178895	10666.414914	28.045466
276.452999	10698.056624	28.050484
276.549435	10706.009067	28.055501
276.692368	10708.314401	28.060519
276.753500	10726.662811	28.065536
277.257731	10740.981061	28.070554
277.262731	10762.817965	28.075572
277.709203	10777.344382	28.080589
277.797011	10805.393156	28.085607
277.994253	10812.241673	28.090624
278.433879	10836.346376	28.095642
278.226547	10862.112249	28.100660
278.670632	10880.260121	28.105677
278.940499	10899.015244	28.110695
279.115616	10925.820670	28.115712
279.546269	10942.935604	28.120730
279.639177	10968.845575	28.125748
279.784061	10976.816890	28.130765
280.461943	11001.299819	28.135783
280.896240	11025.987132	28.140800
281.574179	11036.822809	28.145818
281.390598	11041.599595	28.150836
281.347549	11056.592072	28.155853
282.023568	11078.800087	28.160871
282.478984	11101.342597	28.165888
282.794713	11113.347817	28.170906
283.476741	11119.915802	28.175924
283.359032	11127.517980	28.180941
283.574003	11127.945743	28.185959
283.337580	11145.266267	28.190976
283.527608	11150.923299	28.195994
283.899310	11180.759708	28.201012
283.964669	11198.135724	28.206029
284.172533	11229.923419	28.211047
284.523432	11269.093400	28.216064
284.995798	11271.871956	28.221082
285.028332	11304.186862	28.226100
285.288099	11331.238895	28.231117
285.935660	11354.131166	28.236135
286.126888	11384.951267	28.241152
287.014248	11399.510570	28.246170
287.141772	11417.513098	28.251188
287.577835	11429.495410	28.256205
287.897447	11450.638062	28.261223
287.957399	11472.060247	28.266240
288.423825	11475.073039	28.271258
288.861672	11501.596253	28.276276
288.811948	11523.348730	28.281293
288.990155	11535.752147	28.286311
289.374098	11546.261983	28.291328
289.767241	11568.853312	28.296346
290.155316	11585.555272	28.301364
290.603370	11596.941650	28.306381
290.810407	11611.637815	28.311399
291.242294	11625.812872	28.316416
291.675093	11630.944398	28.321434
291.894392	11648.136167	28.326452
291.893220	11668.312871	28.331469
292.250812	11680.130344	28.336487
292.464103	11696.847277	28.341504
293.336561	11702.750400	28.346522
293.452897	11729.412498	28.351540
293.497126	11728.050188	28.356557
294.135947	11755.454386	28.361575
294.097738	11765.024422	28.366592
293.965236	11778.587428	28.371610
294.277144	11796.577078	28.376628
294.706542	11822.517604	28.381645
295.124876	11830.584155	28.386663
295.432444	11866.965745	28.391680
295.488256	11871.039587	28.396698
295.981401	11892.344659	28.401716
296.110255	11907.547308	28.406733
296.614908	11927.541020	28.411751
296.990062	11941.178976	28.416768
297.037877	11949.069199	28.421786
297.639581	11975.266564	28.426804
297.640436	11988.700435	28.431821
298.279130	11995.729817	28.436839
298.474719	12024.755561	28.441856
298.954152	12041.787919	28.446874
299.433404	12051.114570	28.451892
300.026919	12058.126273	28.456909
300.831388	12065.575678	28.461927
300.594438	12068.335126	28.466944
300.935865	12066.201685	28.471962
301.015610	12064.505675	28.476980
301.018573	12067.723222	28.481997
301.526891	12085.379580	28.487015
301.554757	12095.882751	28.492032
301.765699	12104.365246	28.497050
302.085489	12116.660491	28.502068
302.228996	12113.978447	28.507085
302.323120	12136.792015	28.512103
302.209617	12154.124709	28.517120
302.748612	12176.390097	28.522138
302.914540	12206.465870	28.527156
302.800886	12234.243304	28.532173
303.072349	12261.657392	28.537191
303.519697	12290.767851	28.542208
303.655447	12323.305592	28.547226
303.780995	12354.221969	28.552244
304.231727	12385.870729	28.557261
304.544477	12414.906071	28.562279
305.043592	12455.144789	28.567296
305.947604	12469.852007	28.572314
306.375252	12483.166527	28.577332
306.452095	12516.202957	28.582349
307.168998	12525.791391	28.587367
307.571643	12551.452299	28.592384
307.932786	12556.663791	28.597402
308.394740	12581.703456	28.602420
308.595392	12590.306106	28.607437
308.949735	12607.101400	28.612455
309.310420	12617.321112	28.617472
309.509675	12636.023795	28.622490
310.111727	12641.329239	28.627508
309.978259	12662.403769	28.632525
309.919839	12680.561510	28.637543
310.425763	12692.468545	28.642560
310.920512	12709.817391	28.647578
311.278416	12725.534313	28.652596
311.747897	12739.503966	28.657613
311.956960	12763.624638	28.662631
312.236003	12782.451336	28.667648
312.267053	12798.829349	28.672666
312.669954	12816.617483	28.677684
312.657389	12840.489853	28.682701
313.122138	12865.305715	28.687719
313.521801	12880.979604	28.692736
313.895350	12904.452253	28.697754
314.189276	12921.967067	28.702772
314.608878	12944.631564	28.707789
314.548103	12971.942881	28.712807
314.861165	12996.705350	28.717824
315.076739	13021.025462	28.722842
315.433102	13037.814562	28.727860
315.841928	13079.685141	28.732877
316.035940	13094.849710	28.737895
316.440899	13129.810653	28.742912
316.738319	13139.484905	28.747930
317.345629	13160.651333	28.752948
317.848733	13191.233939	28.757965
317.856524	13205.178262	28.762983
317.811842	13237.159984	28.768000
318.254631	13259.989694	28.773018
318.741178	13292.994304	28.778036
318.962914	13309.423098	28.783053
319.240770	13332.942206	28.788071
319.336595	13358.942185	28.793088
319.767668	13390.749035	28.798106
320.074996	13406.014841	28.803124
320.062467	13442.445257	28.808141
321.010118	13458.372221	28.813159
321.386782	13485.772471	28.818176
321.754238	13512.118404	28.823194
321.888897	13531.808367	28.828212
322.306569	13549.445134	28.833229
322.706614	13557.389513	28.838247
323.025937	13567.741197	28.843264
323.170788	13605.836843	28.848282
324.124029	13618.749785	28.853300
323.819339	13641.392169	28.858317
324.217801	13672.815722	28.863335
325.010020	13678.250669	28.868352
325.643359	13691.639178	28.873370
326.493048	13682.014002	28.878388
326.448298	13681.526794	28.883405
327.094698	13683.276121	28.888423
326.831653	13691.987910	28.893440
327.098304	13710.311852	28.898458
327.580893	13713.908653	28.903476
327.381072	13747.847723	28.908493
327.625997	13746.562221	28.913511
328.014159	13774.925550	28.918528
328.294363	13800.977552	28.923546
328.730978	13817.240354	28.928564
329.034751	13843.186069	28.933581
329.691597	13850.837347	28.938599
329.948768	13869.642145	28.943616
330.322631	13896.369026	28.948634
330.757106	13906.939772	28.953652
331.043108	13925.651589	28.958669
331.166418	13931.095311	28.963687
331.197371	13965.508693	28.968704
331.549534	13986.959716	28.973722
331.771745	14011.158849	28.978740
331.826539	14039.625301	28.983757
332.369631	14064.296016	28.988775
332.783781	14084.755013	28.993792
333.188460	14108.389708	28.998810
333.698785	14133.537201	29.003828
333.928832	14155.287688	29.008845
334.439012	14183.212232	29.013863
334.800715	14198.042645	29.018880
334.739904	14215.501157	29.023898
334.856891	14233.243779	29.028916
335.049203	14273.851592	29.033933
335.690682	14302.747429	29.038951
335.757223	14320.284186	29.043968
336.087853	14360.963797	29.048986
336.533281	14388.653588	29.054004
337.050151	14418.590032	29.059021
337.590724	14451.414646	29.064039
338.083247	14469.066767	29.069056
337.843358	14503.980178	29.074074
338.308806	14519.706184	29.079092
338.566675	14561.903516	29.084109
338.728994	14584.253695	29.089127
339.357941	14613.319226	29.094144
340.140939	14631.717604	29.099162
341.381464	14620.176656	29.104180
341.845350	14639.881030	29.109197
342.712258	14646.125034	29.114215
342.965812	14650.002810	29.119232
343.284476	14659.657101	29.124250
343.871162	14648.511600	29.129268
344.379254	14639.249957	29.134285
344.254328	14647.983435	29.139303
344.344287	14648.567611	29.144320
344.603178	14651.547718	29.149338
344.590805	14649.102353	29.154356
345.083560	14636.576067	29.159373
344.901291	14659.379189	29.164391
345.265120	14668.628812	29.169408
345.414047	14689.566049	29.174426
345.607317	14698.245116	29.179444
345.677375	14721.797594	29.184461
345.978066	14745.277118	29.189479
346.228769	14769.130631	29.194496
346.284310	14798.072676	29.199514
346.851606	14809.296509	29.204532
347.287436	14837.203003	29.209549
347.289277	14870.225131	29.214567
347.680706	14906.804467	29.219584
348.333601	14938.118838	29.224602
348.545376	14954.374420	29.229620
348.800481	14990.725992	29.234637
348.747118	15020.365820	29.239655
349.563956	15046.641150	29.244672
349.329482	15077.318301	29.249690
350.025183	15122.987439	29.254708
350.165053	15150.628409	29.259725
350.572275	15191.713454	29.264743
351.077557	15219.635854	29.269760
351.218232	15261.227157	29.274778
351.916711	15287.051273	29.279796
352.225930	15320.622170	29.284813
352.698365	15355.365462	29.289831
353.347381	15379.973283	29.294848
354.168977	15389.973165	29.299866
354.797120	15412.841292	29.304884
355.413648	15423.130598	29.309901
355.620491	15436.014529	29.314919
356.024270	15447.526030	29.319936
356.215858	15471.388808	29.324954
356.805213	15487.087281	29.329972
357.036571	15506.743065	29.334989
357.030725	15520.595477	29.340007
357.141875	15547.687080	29.345024
357.035843	15560.515907	29.350042
357.559294	15593.195919	29.355060
358.146901	15614.425551	29.360077
358.256687	15646.140426	29.365095
358.725618	15675.839675	29.370112
359.054886	15712.588749	29.375130
359.380508	15734.743138	29.380148
359.992289	15759.758064	29.385165
359.996999	15784.602774	29.390183
360.806507	15810.253229	29.395200
360.572410	15836.345042	29.400218
361.029050	15861.362252	29.405236
361.931047	15891.246866	29.410253
362.156201	15920.793183	29.415271
362.706920	15943.005031	29.420288
362.800475	15967.379737	29.425306
363.028068	15988.920275	29.430324
363.396197	16019.343026	29.435341
363.327664	16067.012695	29.440359
364.019259	16089.292757	29.445376
364.152050	16128.638311	29.450394
364.445934	16159.451945	29.455412
365.131722	16179.838486	29.460429
365.227822	16216.327936	29.465447
365.635076	16248.163207	29.470464
366.124425	16277.620563	29.475482
366.809178	16319.707356	29.480500
367.274525	16334.115819	29.485517
367.509503	16364.758355	29.490535
367.921690	16379.066928	29.495552
368.125927	16409.977887	29.500570
368.336872	16420.024679	29.505588
369.066476	16450.862625	29.510605
368.988553	16487.844998	29.515623
369.332373	16497.308621	29.520640
369.737813	16529.352800	29.525658
370.101890	16549.810582	29.530676
370.567463	16584.489828	29.535693
370.618644	16621.812016	29.540711
371.366221	16643.320621	29.545728
371.458165	16678.449892	29.550746
372.043805	16706.887940	29.555764
372.266588	16743.403219	29.560781
372.484930	16771.158394	29.565799
372.764547	16797.260958	29.570816
373.641732	16827.149818	29.575834
373.987647	16865.396157	29.580852
374.773500	16880.678709	29.585869
374.551892	16920.879466	29.590887
375.095604	16938.599829	29.595904
375.354542	16970.648709	29.600922
375.574416	17011.101061	29.605940
376.605177	17036.541707	29.610957
376.954278	17067.894837	29.615975
377.414731	17075.706370	29.620992
377.729883	17095.096341	29.626010
378.295818	17129.949217	29.631028
378.611718	17151.561722	29.636045
379.045939	17178.525090	29.641063
379.322540	17207.458280	29.646080
379.741567	17227.739108	29.651098
379.932629	17256.117544	29.656116
380.195507	17278.055862	29.661133
380.582362	17314.505737	29.666151
380.968433	17339.845871	29.671168
381.139365	17369.339154	29.676186
381.555374	17397.872776	29.681204
381.913054	17435.090706	29.686221
382.408642	17461.399620	29.691239
382.813731	17481.728788	29.696256
383.077684	17516.421412	29.701274
383.509255	17545.821269	29.706292
384.031127	17580.226847	29.711309
384.387455	17621.578608	29.716327
384.615887	17654.034270	29.721344
385.034859	17686.078441	29.726362
385.322426	17721.253088	29.731380
386.336035	17731.090100	29.736397
387.309767	17744.496326	29.741415
388.221725	17749.447742	29.746432
388.743446	17760.468362	29.751450
388.735961	17775.048060	29.756468
389.429786	17772.231126	29.761485
389.732354	17793.313872	29.766503
389.584983	17804.061034	29.771520
390.025305	17818.471800	29.776538
390.146610	17833.090057	29.781556
390.694276	17849.371513	29.786573
390.722596	17883.970056	29.791591
390.615248	17893.011292	29.796608
391.309184	17923.900477	29.801626
391.466307	17963.312551	29.806644
391.724831	17983.253669	29.811661
391.993366	18007.512455	29.816679
392.632958	18052.707188	29.821696
392.735186	18079.463914	29.826714
393.124532	18124.484446	29.831732
393.388710	18142.570969	29.836749
393.459098	18181.153015	29.841767
393.939626	18206.855545	29.846784
394.203901	18241.248534	29.851802
393.990489	18291.995859	29.856820
394.693106	18322.851239	29.861837
394.959732	18359.115290	29.866855
395.757196	18394.495146	29.871872
396.645784	18426.621954	29.876890
397.348845	18459.377112	29.881908
398.112251	18482.326344	29.886925
398.489921	18511.036926	29.891943
398.424919	18531.300438	29.896960
399.199056	18550.776664	29.901978
399.365331	18581.767336	29.906996
399.920085	18604.127125	29.912013
399.882160	18628.729365	29.917031
400.377917	18664.610778	29.922048
400.810039	18698.198062	29.927066
401.118331	18741.628894	29.932084
401.506551	18763.948774	29.937101
401.748797	18805.861578	29.942119
401.898628	18833.978401	29.947136
402.628001	18864.918625	29.952154
402.851358	18911.974127	29.957172
403.162629	18946.266175	29.962189
403.185778	18987.107564	29.967207
403.986242	19034.934612	29.972224
404.325547	19072.917548	29.977242
404.838219	19115.457791	29.982260
405.281351	19140.048663	29.987277
405.673772	19180.617933	29.992295
406.368439	19215.609873	29.997312
407.411814	19244.118123	30.002330
408.006799	19273.772930	30.007348
408.208130	19299.424204	30.012365
408.372804	19326.306557	30.017383
408.809208	19360.786770	30.022400
409.312865	19383.622743	30.027418
409.297080	19429.626896	30.032436
409.941022	19445.496643	30.037453
410.157653	19483.590751	30.042471
410.318846	19514.472061	30.047488
411.155812	19538.837295	30.052506
411.507029	19587.227699	30.057524
412.151105	19612.971446	30.062541
412.461362	19640.999915	30.067559
412.646962	19680.111765	30.072576
413.195154	19707.851728	30.077594
413.436780	19743.865959	30.082612
414.015933	19770.385361	30.087629
414.059588	19805.081501	30.092647
414.500542	19850.424460	30.097664
415.196845	19871.015604	30.102682
415.502733	19918.612023	30.107700
416.152955	19940.338155	30.112717
416.331274	19981.223982	30.117735
416.344566	20008.093160	30.122752
417.025699	20047.208689	30.127770
417.247320	20089.899080	30.132788
418.361739	20119.339825	30.137805
418.541618	20158.983474	30.142823
418.707713	20193.794088	30.147840
419.458515	20229.923436	30.152858
419.476583	20255.627110	30.157876
420.475025	20291.959829	30.162893
420.992637	20325.337528	30.167911
421.641056	20338.167682	30.172928
421.988856	20352.315376	30.177946
422.281660	20376.624021	30.182964
422.459853	20396.305457	30.187981
423.073097	20414.834668	30.192999
423.389332	20444.222530	30.198016
423.897624	20470.329125	30.203034
424.197982	20502.529265	30.208052
424.678953	20528.977887	30.213069
425.119643	20541.377598	30.218087
425.601731	20573.328537	30.223104
426.223342	20590.699306	30.228122
426.315505	20626.193166	30.233140
426.586581	20646.053391	30.238157
427.287937	20679.833273	30.243175
427.263152	20714.394453	30.248192
427.767099	20737.199116	30.253210
427.932985	20779.211521	30.258228
428.387239	20807.337845	30.263245
428.902854	20834.035033	30.268263
429.099885	20872.633770	30.273280
429.708666	20901.956495	30.278298
430.205958	20947.475950	30.283316
430.940283	20980.215090	30.288333
431.218042	21017.758572	30.293351
431.581250	21055.242220	30.298368
432.373705	21074.202783	30.303386
433.246522	21093.944666	30.308404
433.941006	21118.372135	30.313421
434.585476	21133.109766	30.318439
434.782905	21147.631556	30.323456
436.305848	21153.237766	30.328474
437.386191	21151.585909	30.333492
437.854374	21153.056662	30.338509
438.192032	21155.941309	30.343527
438.264649	21166.901618	30.348544
438.759451	21156.801383	30.353562
438.697264	21155.046040	30.358580
439.088313	21168.744192	30.363597
439.060959	21176.842084	30.368615
439.376519	21186.212170	30.373632
439.587894	21192.074090	30.378650
439.774170	21239.159618	30.383668
439.883915	21259.690657	30.388685
440.120289	21289.027040	30.393703
440.220602	21319.535488	30.398720
440.768510	21346.250203	30.403738
441.024190	21387.557037	30.408756
441.323802	21436.754421	30.413773
441.715485	21475.863020	30.418791
442.169894	21522.505890	30.423808
442.442552	21562.697169	30.428826
442.463318	21608.605023	30.433844
443.154690	21664.808047	30.438861
443.570453	21714.251836	30.443879
443.731926	21777.518738	30.448896
444.317578	21819.760437	30.453914
444.308875	21875.807667	30.458932
444.947250	21937.548494	30.463949
445.845851	21982.554709	30.468967
446.089975	22039.307870	30.473984
446.428725	22081.146583	30.479002
446.585615	22144.172792	30.484020
447.537632	22202.846115	30.489037
448.275841	22236.850056	30.494055
448.752905	22284.028947	30.499072
449.592482	22327.426521	30.504090
450.008693	22370.626471	30.509108
450.705657	22394.120338	30.514125
451.839139	22421.069041	30.519143
452.232489	22454.816918	30.524160
452.790939	22459.871072	30.529178
453.091763	22492.407637	30.534196
453.501630	22515.993512	30.539213
454.067443	22535.941036	30.544231
454.021136	22563.644121	30.549248
454.474436	22585.499418	30.554266
454.902387	22616.523436	30.559284
455.303783	22643.524713	30.564301
456.070117	22671.559736	30.569319
456.172513	22704.520719	30.574336
457.098296	22734.003697	30.579354
457.509256	22762.820086	30.584372
457.593921	22790.851844	30.589389
458.674211	22805.311990	30.594407
458.810469	22838.899922	30.599424
459.254584	22880.445584	30.604442
459.461455	22908.670112	30.609460
459.860297	22941.156567	30.614477
460.196088	22974.101383	30.619495
460.098941	23012.201961	30.624512
460.709159	23054.065790	30.629530
461.451081	23087.968330	30.634548
461.614328	23130.043773	30.639565
462.309478	23167.227820	30.644583
462.454738	23224.414503	30.649600
462.841870	23260.434142	30.654618
463.317884	23317.101019	30.659636
463.910220	23353.000041	30.664653
465.520055	23366.379276	30.669671
466.026843	23404.396189	30.674688
466.645816	23431.750498	30.679706
467.349810	23455.088560	30.684724
467.479903	23491.320109	30.689741
468.361336	23504.203870	30.694759
468.324580	23542.839635	30.699776
468.978496	23562.646007	30.704794
469.231293	23598.486830	30.709812
469.238547	23631.323488	30.714829
469.991683	23654.846047	30.719847
470.579875	23680.602144	30.724864
470.704275	23725.784158	30.729882
471.470748	23748.125092	30.734900
471.849830	23785.347220	30.739917
472.566203	23809.139446	30.744935
472.952498	23854.614188	30.749952
473.509016	23888.109155	30.754970
473.714403	23914.457463	30.759988
473.839356	23949.855060	30.765005
474.483606	23990.253714	30.770023
474.911168	24030.098673	30.775040
475.447405	24054.222359	30.780058
475.819739	24101.046796	30.785076
476.354301	24144.012396	30.790093
476.973508	24168.835251	30.795111
477.264268	24217.651070	30.800128
477.462398	24246.691404	30.805146
477.996636	24290.316601	30.810164
478.449390	24325.247363	30.815181
479.133552	24366.725240	30.820199
479.253940	24413.043587	30.825216
479.715293	24454.605993	30.830234
480.289680	24501.334887	30.835252
480.598000	24539.374678	30.840269
481.696464	24566.799410	30.845287
482.156327	24604.877258	30.850304
482.819294	24643.974898	30.855322
483.213733	24672.674257	30.860340
483.569498	24709.473323	30.865357
484.013897	24748.137553	30.870375
484.523951	24775.701354	30.875392
484.866588	24809.222613	30.880410
485.411654	24835.679933	30.885428
485.544050	24883.309642	30.890445
486.144503	24910.073284	30.895463
486.721028	24947.523782	30.900480
487.019456	24987.307259	30.905498
487.735508	25027.668053	30.910516
487.753300	25068.993368	30.915533
488.442633	25106.693576	30.920551
488.802847	25153.869855	30.925568
489.423763	25199.350207	30.930586
490.535013	25220.437246	30.935604
491.119507	25265.974289	30.940621
491.609914	25293.614733	30.945639
491.953703	25323.815502	30.950656
492.153516	25359.285584	30.955674
492.873211	25391.445848	30.960692
493.157990	25434.188070	30.965709
493.566825	25468.444005	30.970727
493.879630	25516.988602	30.975744
494.172813	25566.498622	30.980762
494.833239	25601.690835	30.985780
495.424862	25649.877234	30.990797
496.410968	25679.719613	30.995815
497.681918	25710.789037	31.000832
497.843952	25739.743268	31.005850
498.266751	25772.997605	31.010868
498.539538	25818.420709	31.015885
498.907709	25844.467375	31.020903
499.807193	25880.762290	31.025920
499.923336	25914.522042	31.030938
500.604389	25949.982809	31.035956
500.577204	25990.895136	31.040973
501.552438	26028.786457	31.045991
501.933671	26065.259310	31.051008
502.047042	26117.125479	31.056026
502.651259	26159.217133	31.061044
502.726289	26208.601207	31.066061
503.392283	26247.717772	31.071079
503.662633	26294.931031	31.076096
503.857978	26353.017230	31.081114
504.371041	26403.928357	31.086132
504.656629	26472.169560	31.091149
504.929242	26531.779695	31.096167
505.462692	26574.344652	31.101184
506.350803	26637.038841	31.106202
507.500211	26666.177622	31.111220
507.775949	26728.734115	31.116237
508.752951	26776.799727	31.121255
509.475035	26812.485727	31.126272
510.202600	26861.769600	31.131290
510.570276	26902.833005	31.136308
511.188622	26952.176283	31.141325
511.436721	26994.124080	31.146343
511.630881	27034.043159	31.151360
512.024908	27088.092672	31.156378
512.829236	27116.989855	31.161396
513.078030	27178.826921	31.166413
513.374266	27217.694802	31.171431
514.043885	27276.481334	31.176448
514.149675	27322.907713	31.181466
514.753733	27370.585823	31.186484
515.128645	27424.197926	31.191501
515.777164	27479.162213	31.196519
517.256476	27508.216085	31.201536
517.536487	27560.330191	31.206554
517.923850	27589.013505	31.211572
518.369392	27639.201315	31.216589
518.549940	27673.064210	31.221607
519.150138	27709.993124	31.226624
519.403320	27769.673835	31.231642
520.178747	27811.886190	31.236660
520.586627	27858.087171	31.241677
521.064331	27907.989656	31.246695
521.045296	27954.135609	31.251712
521.461355	28006.329405	31.256730
522.615281	28057.719412	31.261748
522.983090	28119.726184	31.266765
523.602639	28173.075989	31.271783
523.986139	28232.093093	31.276800
524.333189	28287.034292	31.281818
525.031584	28336.661599	31.286836
525.676249	28398.165953	31.291853
525.829559	28444.701002	31.296871
526.841572	28490.241789	31.301888
527.357343	28542.761344	31.306906
528.066136	28589.122502	31.311924
529.092425	28647.103612	31.316941
529.224254	28700.933531	31.321959
530.528075	28733.586643	31.326976
530.426742	28784.695128	31.331994
531.325937	28814.185105	31.337012
531.964863	28870.038720	31.342029
532.867313	28893.010504	31.347047
533.556303	28919.058992	31.352064
534.296889	28959.812942	31.357082
534.518794	28982.837926	31.362100
535.118803	29015.188866	31.367117
535.425768	29062.002905	31.372135
536.575226	29098.733133	31.377152
536.365890	29132.676233	31.382170
536.773179	29169.605582	31.387188
537.596992	29199.701843	31.392205
537.991109	29235.011927	31.397223
538.536915	29279.647894	31.402240
538.834304	29327.234020	31.407258
539.371431	29372.234474	31.412276
539.698091	29421.835117	31.417293
540.202173	29469.907860	31.422311
540.513528	29505.610822	31.427328
540.846032	29561.867733	31.432346
541.319998	29625.042159	31.437364
542.187763	29680.983405	31.442381
542.738151	29731.327037	31.447399
543.192969	29785.314879	31.452416
543.789395	29831.297320	31.457434
544.577057	29881.210763	31.462452
544.997189	29930.847803	31.467469
545.671339	29981.058020	31.472487
546.191666	30016.058461	31.477504
546.371661	30074.471963	31.482522
547.335703	30133.900722	31.487540
547.814128	30172.445204	31.492557
548.232776	30228.021081	31.497575
548.810647	30267.132937	31.502592
549.458133	30325.633699	31.507610
549.879503	30378.530964	31.512628
550.458285	30422.508115	31.517645
551.036908	30474.562392	31.522663
551.829723	30528.234516	31.527680
551.968814	30585.325063	31.532698
552.810906	30628.132631	31.537716
553.515935	30661.983626	31.542733
553.556846	30712.272701	31.547751
554.453518	30750.256795	31.552768
554.813401	30794.495243	31.557786
554.987251	30844.491277	31.562804
555.637792	30876.657423	31.567821
555.825422	30938.871323	31.572839
556.355157	30980.611543	31.577856
557.162285	31059.322321	31.582874
557.421123	31116.773324	31.587892
557.696773	31176.730105	31.592909
558.093360	31243.229846	31.597927
558.978640	31299.473086	31.602944
559.623459	31362.398204	31.607962
560.397480	31414.713092	31.612980
561.114169	31471.240452	31.617997
561.711815	31534.984920	31.623015
562.288957	31583.590861	31.628032
562.755456	31639.955217	31.633050
563.355991	31702.368279	31.638068
564.179898	31763.387686	31.643085
564.414182	31820.646269	31.648103
565.048983	31879.756963	31.653120
565.380882	31937.173255	31.658138
565.953496	31998.736903	31.663156
566.557105	32060.510183	31.668173
567.347029	32119.321399	31.673191
567.913253	32166.753804	31.678208
568.561324	32232.483453	31.683226
568.810770	32294.281653	31.688244
569.935401	32358.118274	31.693261
570.116238	32421.859423	31.698279
570.860020	32467.625483	31.703296
571.810383	32538.253781	31.708314
571.824465	32590.830876	31.713332
572.567840	32659.928928	31.718349
573.125999	32717.212351	31.723367
573.911321	32777.929269	31.728384
574.213199	32834.652933	31.733402
574.465369	32893.458199	31.738420
575.533537	32957.678705	31.743437
575.536868	33025.907086	31.748455
576.165739	33093.113586	31.753472
576.766441	33156.954888	31.758490
577.327326	33223.721928	31.763508
578.353186	33297.388982	31.768525
578.746493	33367.664991	31.773543
579.298004	33420.183687	31.778560
580.405399	33485.144305	31.783578
580.893438	33533.262332	31.788596
581.721424	33584.403929	31.793613
582.408249	33653.228068	31.798631
583.488843	33691.667601	31.803648
583.798558	33748.219311	31.808666
584.408484	33805.324079	31.813684
585.215264	33838.413210	31.818701
585.634838	33905.376676	31.823719
586.390801	33940.471984	31.828736
586.763238	34004.022879	31.833754
587.144019	34052.693432	31.838772
588.059968	34099.495422	31.843789
588.195901	34146.878334	31.848807
588.645967	34198.677728	31.853824
589.155684	34258.284149	31.858842
589.619318	34312.397937	31.863860
590.055290	34366.847838	31.868877
590.654210	34443.705266	31.873895
591.210246	34494.869387	31.878912
591.961559	34555.121484	31.883930
592.320464	34608.013328	31.888948
592.745454	34665.202045	31.893965
593.347916	34721.515711	31.898983
594.009944	34777.456742	31.904000
594.774518	34834.747402	31.909018
594.798075	34898.725482	31.914036
595.736628	34949.568601	31.919053
596.027047	35011.407272	31.924071
597.202221	35067.882549	31.929088
597.991776	35109.737649	31.934106
598.887212	35178.280540	31.939124
599.296499	35217.709027	31.944141
600.252209	35273.621773	31.949159
601.339129	35312.253106	31.954176
601.859500	35349.066103	31.959194
602.380850	35404.868344	31.964212
603.056447	35452.780498	31.969229
603.006130	35511.306909	31.974247
603.359944	35555.479299	31.979264
604.029932	35608.379239	31.984282
604.341069	35678.513847	31.989300
605.014737	35738.318879	31.994317
605.606551	35806.999799	31.999335
606.115168	35867.400751	32.004352
606.940516	35923.220393	32.009370
607.181456	35989.372321	32.014388
607.845056	36057.253262	32.019405
608.224283	36135.707190	32.024423
608.817277	36188.864638	32.029440
609.643968	36259.465052	32.034458
610.286051	36318.860650	32.039476
611.236995	36397.129250	32.044493
611.673081	36461.896527	32.049511
612.186515	36528.144048	32.054528
612.969131	36586.062206	32.059546
613.937272	36652.054775	32.064564
614.681908	36707.874468	32.069581
615.555711	36764.076877	32.074599
616.304968	36820.584199	32.079616
617.008075	36866.892197	32.084634
617.159839	36926.478522	32.089652
617.655262	36986.774939	32.094669
618.563097	37052.217176	32.099687
618.700971	37111.579165	32.104704
619.431572	37166.948106	32.109722
619.796463	37247.015765	32.114740
620.752303	37297.480737	32.119757
621.164849	37367.248393	32.124775
621.722412	37437.377305	32.129792
622.215979	37500.030338	32.134810
622.729329	37561.660810	32.139828
624.019465	37614.754031	32.144845
624.711828	37678.192159	32.149863
625.379587	37741.966011	32.154880
626.169445	37792.690338	32.159898
626.679248	37852.037176	32.164916
627.376245	37905.273928	32.169933
627.572842	37970.206301	32.174951
627.943653	38028.219543	32.179968
628.607948	38091.824752	32.184986
629.046111	38176.555832	32.190004
629.445317	38239.378589	32.195021
630.404867	38303.825627	32.200039
630.902495	38374.763531	32.205056
631.508893	38441.015220	32.210074
631.853226	38522.206137	32.215092
632.350171	38582.349768	32.220109
632.815508	38661.434764	32.225127
633.646843	38725.831984	32.230144
634.411989	38796.307287	32.235162
634.536712	38863.145535	32.240180
635.226447	38930.957125	32.245197
636.134460	39017.719515	32.250215
636.929300	39079.532494	32.255232
637.770062	39149.194829	32.260250
638.269610	39224.299265	32.265268
638.895174	39286.191556	32.270285
639.290144	39353.071946	32.275303
640.042843	39424.053639	32.280320
641.203170	39493.121278	32.285338
641.722582	39558.782226	32.290356
641.913675	39636.565917	32.295373
643.049586	39703.936953	32.300391
643.700248	39772.301099	32.305408
643.956437	39837.040798	32.310426
644.559419	39919.744908	32.315444
645.244544	39982.292572	32.320461
645.943804	40061.660443	32.325479
647.241783	40122.512663	32.330496
648.164489	40178.641726	32.335514
648.584266	40250.205920	32.340532
649.468159	40311.244325	32.345549
650.187388	40367.903369	32.350567
650.735385	40433.013411	32.355584
651.474807	40498.918988	32.360602
651.992667	40562.664428	32.365620
652.905564	40620.580085	32.370637
653.321199	40683.083332	32.375655
653.780073	40754.144208	32.380672
654.555745	40814.580347	32.385690
654.965063	40888.421712	32.390708
655.544138	40959.422380	32.395725
656.310142	41014.844454	32.400743
657.207396	41091.538391	32.405760
657.937683	41148.936725	32.410778
658.295219	41230.377342	32.415796
658.848375	41300.193451	32.420813
659.588968	41380.541955	32.425831
659.865644	41454.120318	32.430848
660.781668	41513.127422	32.435866
661.341729	41598.090816	32.440884
661.975629	41677.571203	32.445901
662.571479	41751.353470	32.450919
663.211336	41817.655973	32.455936
663.566854	41902.815735	32.460954
664.088633	41980.844844	32.465972
664.672404	42067.820671	32.470989
666.148414	42130.181157	32.476007
666.351068	42222.660687	32.481024
667.489320	42295.392136	32.486042
668.661890	42374.536655	32.491060
668.827892	42440.639077	32.496077
670.033108	42506.812286	32.501095
670.121437	42578.449987	32.506112
671.165606	42646.579474	32.511130
671.658445	42721.939199	32.516148
672.543018	42791.424900	32.521165
673.791528	42840.041131	32.526183
673.989496	42918.200556	32.531200
675.165212	42976.010490	32.536218
675.756284	43036.149860	32.541236
676.246284	43089.113942	32.546253
677.194256	43147.217962	32.551271
677.685524	43215.068774	32.556288
678.323584	43274.588597	32.561306
678.668027	43333.386977	32.566324
679.397520	43395.818834	32.571341
679.929613	43457.023899	32.576359
681.119140	43499.895834	32.581376
681.666000	43546.574984	32.586394
682.484521	43620.861286	32.591412
682.530005	43675.350066	32.596429
683.549402	43731.053918	32.601447
683.875453	43787.974984	32.606464
685.616537	43822.913136	32.611482
686.101517	43889.930734	32.616500
686.511315	43956.616896	32.621517
687.081523	44009.712356	32.626535
687.527219	44079.455698	32.631552
688.382997	44136.381438	32.636570
688.808072	44199.611681	32.641588
689.395389	44268.719667	32.646605
689.825740	44335.321669	32.651623
690.025513	44408.542405	32.656640
690.977229	44481.739620	32.661658
691.393477	44567.798187	32.666676
691.904440	44652.600511	32.671693
693.080844	44727.330673	32.676711
693.069358	44815.659043	32.681728
694.188575	44898.962690	32.686746
694.885781	44984.982833	32.691764
695.115148	45069.540134	32.696781
696.130950	45153.057848	32.701799
696.356046	45243.290876	32.706816
697.370954	45339.856910	32.711834
698.058442	45439.502843	32.716852
698.550048	45545.989788	32.721869
699.224333	45628.205348	32.726887
699.661711	45737.651666	32.731904
700.502210	45828.069506	32.736922
701.613152	45922.873196	32.741940
701.476015	46021.560214	32.746957
702.804957	46113.960346	32.751975
703.436825	46207.825042	32.756992
704.854950	46293.144102	32.762010
705.626121	46380.790910	32.767028
706.599605	46465.000385	32.772045
707.705929	46543.343001	32.777063
707.862368	46627.212014	32.782080
708.740952	46703.202598	32.787098
709.443374	46791.023768	32.792116
709.702127	46887.107455	32.797133
710.655442	46965.268795	32.802151
711.277142	47064.346827	32.807168
712.112062	47141.391692	32.812186
712.710863	47224.924629	32.817204
713.689916	47314.208637	32.822221
714.557598	47397.805063	32.827239
715.318665	47465.307423	32.832256
716.388514	47560.119805	32.837274
716.998694	47620.194844	32.842292
717.720347	47699.742985	32.847309
718.864917	47778.349621	32.852327
719.261205	47856.041810	32.857344
719.901268	47938.876252	32.862362
720.345998	48013.914569	32.867380
720.800293	48100.229191	32.872397
721.807837	48181.310928	32.877415
722.232951	48271.834628	32.882432
723.088658	48369.168879	32.887450
723.972133	48442.042180	32.892468
724.359285	48528.477258	32.897485
725.093802	48606.511113	32.902503
726.221315	48685.917023	32.907520
726.672497	48760.650851	32.912538
727.198527	48827.773848	32.917556
727.813554	48905.219220	32.922573
728.996320	48967.518422	32.927591
729.981996	49039.401131	32.932608
730.932167	49113.551328	32.937626
731.761186	49171.848385	32.942644
732.643646	49238.651508	32.947661
733.645250	49290.755284	32.952679
734.073478	49366.370131	32.957696
734.667484	49432.492247	32.962714
735.566205	49492.768454	32.967732
736.048755	49574.116956	32.972749
736.635928	49632.196578	32.977767
737.642325	49710.369812	32.982784
738.187369	49781.071420	32.987802
739.039281	49841.233313	32.992820
739.908087	49917.421494	32.997837
740.310151	49991.091244	33.002855
741.303063	50064.761095	33.007872
741.562574	50151.467859	33.012890
742.590286	50221.402409	33.017908
743.130362	50302.539135	33.022925
743.684769	50379.413030	33.027943
744.348281	50463.849505	33.032960
744.966387	50554.181348	33.037978
745.781670	50634.203042	33.042996
746.370712	50729.044580	33.048013
746.819664	50821.016606	33.053031
748.075961	50900.334474	33.058048
748.837525	50993.904193	33.063066
749.824285	51072.496822	33.068084
750.505310	51161.172264	33.073101
751.543124	51236.219440	33.078119
752.191181	51319.954682	33.083136
753.138190	51411.265633	33.088154
753.681836	51485.290284	33.093172
754.289237	51569.810384	33.098189
754.964853	51655.507193	33.103207
756.212566	51744.249155	33.108224
756.761684	51823.606079	33.113242
757.530895	51905.175802	33.118260
758.093109	51991.752093	33.123277
759.005621	52081.119815	33.128295
759.038626	52174.102288	33.133312
759.941891	52276.688751	33.138330
760.649671	52359.635173	33.143348
761.048864	52445.905710	33.148365
761.864948	52552.216546	33.153383
762.593733	52654.897140	33.158400
763.155421	52767.752296	33.163418
764.437053	52864.593072	33.168436
764.480481	52971.723095	33.173453
765.729481	53072.398906	33.178471
766.495999	53173.325916	33.183488
767.260983	53278.025486	33.188506
768.285512	53370.969080	33.193524
768.675299	53469.123402	33.198541
769.657483	53573.731632	33.203559
770.351708	53679.525469	33.208576
771.270772	53777.808281	33.213594
772.282063	53866.517000	33.218612
773.059283	53962.006412	33.223629
774.233323	54053.089843	33.228647
775.047025	54144.069242	33.233664
775.491332	54234.409063	33.238682
776.087741	54328.514991	33.243700
776.827564	54424.341402	33.248717
777.283182	54514.042481	33.253735
778.013312	54599.749442	33.258752
778.491815	54699.929671	33.263770
779.242120	54793.822719	33.268788
779.443192	54905.145136	33.273805
780.073465	55009.124383	33.278823
781.328120	55118.074273	33.283840
782.040083	55231.657875	33.288858
782.919208	55331.484144	33.293876
783.314877	55442.562445	33.298893
784.188092	55547.192914	33.303911
785.529123	55657.888016	33.308928
786.507423	55749.334017	33.313946
788.528154	55820.798211	33.318964
789.714196	55907.964284	33.323981
790.692243	55995.670770	33.328999
791.439582	56068.370889	33.334016
791.688583	56163.623725	33.339034
792.767259	56247.624425	33.344052
793.123876	56329.691710	33.349069
793.325207	56420.321950	33.354087
794.371759	56517.788397	33.359104
795.246678	56617.211098	33.364122
796.536288	56686.834586	33.369140
797.099290	56772.281688	33.374157
798.210841	56876.020201	33.379175
799.140085	56955.290451	33.384192
799.357938	57039.955556	33.389210
800.651922	57127.500839	33.394228
801.472541	57222.783904	33.399245
801.923779	57321.800190	33.404263
802.638182	57411.660965	33.409280
803.078350	57504.878952	33.414298
803.645814	57607.782654	33.419316
804.521406	57714.591624	33.424333
805.000916	57820.746507	33.429351
805.932894	57920.115661	33.434368
806.245014	58040.669765	33.439386
807.478228	58138.233196	33.444404
808.258354	58238.242117	33.449421
809.313636	58360.905553	33.454439
810.496311	58467.345257	33.459456
810.880119	58571.693642	33.464474
812.109566	58680.464955	33.469492
812.696660	58786.025668	33.474509
813.169174	58884.085533	33.479527
814.688451	58972.498868	33.484544
816.033273	59076.247958	33.489562
816.576055	59172.907219	33.494580
817.457306	59270.774718	33.499597
818.582348	59358.781205	33.504615
819.367691	59453.372878	33.509632
819.854118	59543.356855	33.514650
820.373282	59641.874005	33.519668
821.112370	59745.550125	33.524685
821.774253	59849.947429	33.529703
823.069629	59935.665599	33.534720
824.362714	60025.991819	33.539738
825.574499	60113.961914	33.544756
826.512314	60196.510989	33.549773
827.201977	60284.796018	33.554791
827.997677	60364.405232	33.559808
828.424212	60454.213587	33.564826
829.442673	60555.047635	33.569844
830.212802	60642.827886	33.574861
830.687806	60731.276889	33.579879
831.852487	60811.256382	33.584896
833.731541	60867.631367	33.589914
834.987760	60924.419591	33.594932
835.484758	60994.461336	33.599949
836.001697	61052.870554	33.604967
836.381388	61121.440603	33.609984
837.162328	61194.014615	33.615002
837.959365	61257.901956	33.620020
839.099599	61341.047801	33.625037
839.271988	61415.581826	33.630055
839.968214	61502.499503	33.635072
840.503716	61599.430655	33.640090
841.052669	61696.486445	33.645108
841.546836	61793.109347	33.650125
841.817992	61884.567858	33.655143
844.154881	61965.115778	33.660160
844.701437	62059.417888	33.665178
845.574610	62153.432350	33.670196
846.736851	62247.525677	33.675213
847.729751	62334.094245	33.680231
848.451604	62434.455866	33.685248
848.745427	62533.074951	33.690266
849.345287	62638.413334	33.695284
850.286959	62742.083695	33.700301
850.650572	62845.161551	33.705319
851.042642	62962.786006	33.710336
851.876355	63079.806863	33.715354
852.488053	63198.622477	33.720372
853.734991	63300.291784	33.725389
855.578220	63414.378356	33.730407
856.957739	63511.418631	33.735424
857.870117	63610.850439	33.740442
858.367582	63703.044321	33.745460
859.326547	63802.861232	33.750477
860.216432	63915.730796	33.755495
860.956114	64011.596414	33.760512
861.847746	64113.183310	33.765530
862.573956	64223.546880	33.770548
863.502442	64321.689879	33.775565
864.177913	64442.145603	33.780583
864.694705	64556.667253	33.785600
865.633128	64668.287535	33.790618
867.222757	64766.202790	33.795636
868.261948	64869.975100	33.800653
868.997131	64968.071059	33.805671
870.254313	65071.239252	33.810688
870.790390	65170.191017	33.815706
871.683395	65255.688444	33.820724
873.052901	65352.897047	33.825741
873.526592	65450.754206	33.830759
874.111553	65549.826092	33.835776
874.964600	65662.736544	33.840794
875.367092	65761.631102	33.845812
876.088284	65886.746751	33.850829
876.622575	66007.500470	33.855847
877.609416	66127.730915	33.860864
878.573031	66250.001571	33.865882
879.243799	66364.551836	33.870900
880.081503	66494.507053	33.875917
880.575054	66628.951958	33.880935
881.355494	66754.688834	33.885952
881.560325	66889.891402	33.890970
882.269240	67033.173100	33.895988
883.028522	67181.530479	33.901005
884.162129	67317.675379	33.906023
885.444516	67451.090519	33.911040
886.742393	67583.479712	33.916058
887.419950	67716.320427	33.921076
888.614043	67838.087876	33.926093
889.696504	67969.762878	33.931111
890.398023	68081.377428	33.936128
891.073424	68194.438437	33.941146
892.058659	68310.198937	33.946164
893.486953	68429.635832	33.951181
894.294469	68555.467452	33.956199
894.762305	68669.513840	33.961216
895.969116	68793.567156	33.966234
896.352765	68909.089346	33.971252
897.507505	69037.237216	33.976269
898.176717	69173.104403	33.981287
898.814237	69304.203960	33.986304
899.886244	69426.835410	33.991322
901.079920	69554.031494	33.996340
902.487790	69677.304163	34.001357
903.200557	69799.845630	34.006375
904.277528	69927.341522	34.011392
905.356652	70042.292836	34.016410
906.176562	70163.863823	34.021428
907.046966	70287.286124	34.026445
908.019339	70407.789872	34.031463
909.112821	70521.375570	34.036480
910.224083	70645.847554	34.041498
910.817531	70777.469315	34.046516
911.972321	70898.337587	34.051533
912.643250	71017.364545	34.056551
913.398881	71151.307643	34.061568
914.335313	71269.128422	34.066586
915.204963	71400.335069	34.071604
916.132927	71527.156967	34.076621
917.017123	71664.540877	34.081639
917.775267	71794.870486	34.086656
918.705723	71929.478673	34.091674
919.518256	72063.462255	34.096692
921.297151	72177.335001	34.101709
921.743370	72315.137216	34.106727
922.634484	72445.454999	34.111744
924.087810	72568.578614	34.116762
925.137962	72689.822097	34.121780
926.447148	72810.397202	34.126797
927.344560	72925.286552	34.131815
928.096005	73043.893923	34.136832
929.313734	73161.741564	34.141850
930.098077	73292.853680	34.146868
931.029370	73406.279099	34.151885
932.181921	73523.399600	34.156903
932.932936	73644.457737	34.161920
933.889460	73758.943257	34.166938
934.729896	73874.972774	34.171956
935.536226	73985.955512	34.176973
936.468843	74115.213936	34.181991
937.462905	74241.926883	34.187008
937.944854	74367.498633	34.192026
938.907026	74504.242463	34.197044
939.416956	74633.902965	34.202061
939.915188	74776.961361	34.207079
941.208825	74910.231181	34.212096
942.333571	75040.911484	34.217114
942.675565	75190.417896	34.222132
943.958133	75326.070114	34.227149
944.692074	75465.558410	34.232167
945.234299	75608.981740	34.237184
946.187336	75759.478447	34.242202
947.179291	75911.759633	34.247220
947.993723	76059.131645	34.252237
948.914914	76208.706947	34.257255
949.904778	76349.119727	34.262272
951.260613	76491.332194	34.267290
951.743291	76643.759858	34.272308
952.586376	76789.107974	34.277325
953.330960	76937.218467	34.282343
953.782327	77075.555712	34.287360
955.096549	77226.059361	34.292378
956.089471	77379.691395	34.297396
956.802916	77527.089908	34.302413
957.769262	77670.038705	34.307431
958.654309	77831.838715	34.312448
959.783232	77988.127980	34.317466
960.376559	78159.517431	34.322484
961.876215	78314.444415	34.327501
962.643661	78463.092578	34.332519
963.217833	78635.633764	34.337536
964.519157	78786.732016	34.342554
965.104284	78961.842080	34.347572
966.293999	79123.790623	34.352589
968.498233	79256.245889	34.357607
969.585633	79418.099668	34.362624
970.992632	79552.865051	34.367642
971.987013	79709.738974	34.372660
973.311123	79847.265293	34.377677
974.324485	79991.834171	34.382695
974.985212	80130.845033	34.387712
975.714102	80262.437682	34.392730
976.512467	80415.483840	34.397748
977.529320	80557.443093	34.402765
978.490958	80713.582928	34.407783
978.977877	80861.818985	34.412800
980.567461	81005.482627	34.417818
981.607475	81159.518543	34.422836
982.530481	81304.983807	34.427853
983.974846	81442.866772	34.432871
985.199022	81583.526433	34.437888
986.523707	81710.416665	34.442906
987.118209	81863.689860	34.447924
987.715964	82002.741588	34.452941
988.919671	82153.220541	34.457959
989.519169	82305.913826	34.462976
990.645453	82448.442413	34.467994
991.257121	82605.792061	34.473012
992.077545	82766.505582	34.478029
993.136246	82926.497397	34.483047
993.389478	83099.366143	34.488064
995.481664	83236.570343	34.493082
996.595125	83387.293798	34.498100
998.777007	83513.786034	34.503117
1000.332053	83637.706692	34.508135
1001.298247	83768.894195	34.513152
1002.841667	83897.240732	34.518170
1003.806152	84020.059312	34.523188
1004.708245	84140.345414	34.528205
1005.620369	84256.903808	34.533223
1005.831451	84396.844027	34.538240
1006.737003	84513.910975	34.543258
1007.647140	84661.797613	34.548276
1008.404258	84788.545915	34.553293
1009.217923	84926.459515	34.558311
1009.971476	85088.041798	34.563328
1010.991495	85217.773277	34.568346
1012.006482	85381.914763	34.573364
1012.892072	85529.766695	34.578381
1013.720941	85671.858301	34.583399
1014.494402	85829.848400	34.588416
1015.334705	85982.608223	34.593434
1016.299237	86153.337851	34.598452
1017.414273	86302.953638	34.603469
1018.184613	86459.208391	34.608487
1018.611377	86613.186258	34.613504
1019.471531	86763.644571	34.618522
1020.561942	86931.125465	34.623540
1021.603933	87086.523017	34.628557
1022.983836	87246.396308	34.633575
1023.420112	87415.248444	34.638592
1024.355133	87575.697697	34.643610
1025.691028	87745.687497	34.648628
1026.642061	87907.553828	34.653645
1027.590767	88079.046748	34.658663
1028.368142	88250.544025	34.663680
1029.766821	88424.717537	34.668698
1030.455463	88595.504283	34.673716
1031.474854	88763.282044	34.678733
1032.585821	88943.689869	34.683751
1033.232659	89133.580103	34.688768
1034.274226	89310.603859	34.693786
1035.088043	89498.779587	34.698804
1036.130979	89687.538977	34.703821
1037.518255	89862.826056	34.708839
1038.342150	90078.015192	34.713856
1039.536605	90261.494836	34.718874
1041.601401	90421.503648	34.723892
1043.107225	90589.074267	34.728909
1044.897076	90743.662765	34.733927
1046.021703	90916.678435	34.738944
1047.361212	91066.654029	34.743962
1048.527212	91219.026379	34.748980
1049.565552	91375.844850	34.753997
1050.830586	91516.348413	34.759015
1051.537316	91674.641552	34.764032
1052.735023	91828.335260	34.769050
1053.858035	91985.846166	34.774068
1054.472171	92127.530906	34.779085
1055.711720	92293.239778	34.784103
1056.804428	92458.290582	34.789120
1057.872036	92609.903169	34.794138
1058.933561	92767.055908	34.799156
1060.177880	92915.970083	34.804173
1060.894001	93077.745640	34.809191
1061.687483	93240.110733	34.814208
1062.441504	93398.040117	34.819226
1063.761327	93568.523131	34.824244
1064.650805	93743.199321	34.829261
1066.155627	93894.430849	34.834279
1066.881554	94066.414722	34.839296
1068.034259	94225.770762	34.844314
1069.216727	94394.737846	34.849332
1069.880870	94576.394795	34.854349
1071.090217	94731.041637	34.859367
1072.169087	94917.873424	34.864384
1073.006443	95090.124464	34.869402
1073.482108	95272.210257	34.874420
1074.507838	95439.982474	34.879437
1076.094985	95614.511844	34.884455
1077.231465	95803.853804	34.889472
1078.369351	95965.496040	34.894490
1079.534759	96152.898820	34.899508
1080.428877	96329.194060	34.904525
1081.991947	96507.658471	34.909543
1082.597611	96682.978559	34.914560
1083.902597	96861.133817	34.919578
1084.964460	97024.397126	34.924596
1085.746578	97212.124668	34.929613
1086.798114	97391.534879	34.934631
1088.013908	97554.187356	34.939648
1088.900929	97748.776530	34.944666
1090.023957	97925.849018	34.949684
1090.731395	98099.408512	34.954701
1092.020992	98265.301004	34.959719
1092.613312	98448.314849	34.964736
1093.923730	98626.798260	34.969754
1095.311387	98798.793600	34.974772
1096.335177	98983.132523	34.979789
1097.263017	99147.235854	34.984807
1098.251605	99326.461339	34.989824
1099.569502	99496.896560	34.994842
1100.943238	99681.321773	34.999860
1102.092032	99859.840675	35.004877
1103.279021	100016.435838	35.009895
1104.352945	100209.683342	35.014912
1105.491956	100376.595961	35.019930
1106.993557	100552.015813	35.024948
1107.586276	100727.467368	35.029965
1109.141514	100896.808886	35.034983
1110.281935	101081.453861	35.040000
1111.547851	101255.005522	35.045018
1112.925742	101429.451521	35.050036
1113.812906	101590.690096	35.055053
1115.283058	101756.290426	35.060071
1116.247720	101936.177643	35.065088
1117.489960	102106.693430	35.070106
1118.948457	102270.272839	35.075124
1120.041337	102433.128799	35.080141
1121.655914	102594.417577	35.085159
1122.313317	102762.767915	35.090176
1123.217349	102940.652296	35.095194
1124.359649	103114.914467	35.100212
1125.282127	103291.582447	35.105229
1126.128820	103456.416927	35.110247
1127.193660	103641.301656	35.115264
1128.289613	103827.993524	35.120282
1129.120972	104002.129575	35.125300
1130.037635	104202.176772	35.130317
1131.265877	104393.435258	35.135335
1132.576996	104586.695065	35.140352
1133.394717	104795.413152	35.145370
1134.336195	104973.868719	35.150388
1135.277429	105185.355666	35.155405
1136.564247	105386.047022	35.160423
1137.436844	105593.888432	35.165440
1138.445788	105810.080570	35.170458
1139.573941	106007.725312	35.175476
1141.328795	106215.931840	35.180493
1142.630695	106403.962979	35.185511
1143.634179	106606.901716	35.190528
1144.846254	106810.073372	35.195546
1146.186993	107006.056384	35.200564
1147.292215	107220.483459	35.205581
1148.805762	107396.010566	35.210599
1149.955775	107586.570434	35.215616
1151.357183	107771.896822	35.220634
1152.288979	107964.560162	35.225652
1153.407055	108166.643073	35.230669
1154.712214	108364.339207	35.235687
1156.123977	108546.641935	35.240704
1156.775537	108741.827297	35.245722
1158.202840	108938.405376	35.250740
1159.405614	109135.554138	35.255757
1160.466438	109329.383824	35.260775
1161.336514	109524.981916	35.265792
1162.102501	109731.783715	35.270810
1163.497669	109932.035110	35.275828
1164.461332	110140.808633	35.280845
1165.314888	110359.229220	35.285863
1166.402525	110558.801526	35.290880
1167.318912	110765.332851	35.295898
1168.302848	110958.515488	35.300916
1169.073925	111172.028522	35.305933
1170.174951	111373.504696	35.310951
1171.634955	111575.062139	35.315968
1172.644029	111784.689389	35.320986
1174.418833	111980.433619	35.326004
1175.517029	112198.777564	35.331021
1176.834026	112396.171546	35.336039
1178.214010	112603.754548	35.341056
1179.515923	112810.718630	35.346074
1180.676990	113010.499191	35.351092
1182.537789	113202.563898	35.356109
1184.124319	113385.135853	35.361127
1184.892863	113580.310846	35.366144
1185.912825	113796.615292	35.371162
1187.048535	113984.574241	35.376180
1188.046819	114194.424150	35.381197
1189.548067	114375.407738	35.386215
1191.507834	114571.532248	35.391232
1192.621159	114759.044002	35.396250
1194.006875	114950.059267	35.401268
1194.476117	115147.930052	35.406285
1195.514080	115351.510574	35.411303
1196.790875	115554.470132	35.416320
1197.769346	115774.698932	35.421338
1198.582729	115977.332957	35.426356
1199.894360	116183.572746	35.431373
1202.218531	116371.768546	35.436391
1204.565663	116550.028361	35.441408
1205.791619	116743.692267	35.446426
1207.158351	116918.467986	35.451444
1208.341615	117113.281809	35.456461
1209.215315	117294.046030	35.461479
1210.844685	117464.866331	35.466496
1211.723207	117657.288978	35.471514
1213.043272	117829.733922	35.476532
1213.788943	118031.874231	35.481549
1214.641494	118213.027860	35.486567
1215.815533	118421.029822	35.491584
1216.447919	118616.806831	35.496602
1217.782140	118818.196110	35.501620
1218.482783	119037.228923	35.506637
1219.475321	119247.129597	35.511655
1220.530158	119460.011913	35.516672
1221.224112	119695.865817	35.521690
1222.607893	119920.963001	35.526708
1223.298646	120159.355506	35.531725
1224.357390	120407.864413	35.536743
1225.562941	120635.911185	35.541760
1226.550277	120894.066744	35.546778
1227.861388	121138.320160	35.551796
1228.741120	121383.420166	35.556813
1229.880276	121634.980105	35.561831
1231.437157	121873.673667	35.566848
1232.725721	122133.374141	35.571866
1234.205428	122386.531402	35.576884
1235.851948	122622.415440	35.581901
1237.237358	122862.678795	35.586919
1238.587956	123112.758774	35.591936
1239.951761	123351.838378	35.596954
1241.452215	123578.971722	35.601972
1242.646815	123807.614949	35.606989
1244.285015	124038.505564	35.612007
1246.054002	124259.921820	35.617024
1247.186328	124481.419960	35.622042
1248.685295	124697.029008	35.627060
1249.837900	124920.187249	35.632077
1251.275721	125122.907564	35.637095
1252.841092	125320.982085	35.642112
1254.085205	125520.910896	35.647130
1255.298507	125717.842365	35.652148
1256.505529	125914.028369	35.657165
1257.947395	126104.777438	35.662183
1259.240766	126300.951601	35.667200
1260.695334	126491.523532	35.672218
1262.110454	126683.674828	35.677236
1263.665243	126874.346582	35.682253
1264.660003	127047.557999	35.687271
1265.830963	127236.673305	35.692288
1266.534250	127445.259818	35.697306
1267.614063	127650.375731	35.702324
1268.970729	127858.932704	35.707341
1269.524875	128082.986390	35.712359
1270.665918	128290.352542	35.717376
1271.682316	128510.745561	35.722394
1272.676790	128736.505446	35.727412
1273.492700	128977.811325	35.732429
1274.753277	129220.110051	35.737447
1276.234823	129445.515397	35.742464
1277.109786	129695.905436	35.747482
1278.695973	129928.293894	35.752500
1280.215158	130163.458530	35.757517
1281.824597	130412.300052	35.762535
1283.407318	130639.497149	35.767552
1284.462051	130893.327437	35.772570
1285.531411	131135.127502	35.777588
1286.709694	131376.683161	35.782605
1288.003137	131632.076970	35.787623
1289.307175	131868.544887	35.792640
1290.565884	132122.718744	35.797658
1292.340002	132354.459928	35.802676
1294.341475	132587.787715	35.807693
1295.670875	132821.570946	35.812711
1297.906019	133026.644214	35.817728
1299.703421	133241.704917	35.822746
1300.969848	133457.336852	35.827764
1302.408602	133665.981795	35.832781
1303.523304	133892.772468	35.837799
1305.173844	134100.523011	35.842816
1306.148655	134309.692743	35.847834
1307.943279	134507.989882	35.852852
1309.203641	134721.032277	35.857869
1310.456848	134932.403775	35.862887
1311.949720	135130.830802	35.867904
1313.113076	135353.084852	35.872922
1314.167001	135562.857998	35.877940
1315.266420	135775.997314	35.882957
1316.040669	135996.241019	35.887975
1317.098174	136215.323519	35.892992
1317.956464	136458.922461	35.898010
1319.000772	136681.395353	35.903028
1320.124309	136933.308887	35.908045
1320.770845	137174.818183	35.913063
1322.090187	137432.801443	35.918080
1323.412137	137702.514197	35.923098
1324.519675	137955.832751	35.928116
1326.047963	138201.539396	35.933133
1327.421201	138451.191401	35.938151
1328.944498	138700.731608	35.943168
1330.164939	138961.126671	35.948186
1331.148917	139223.338069	35.953204
1332.504680	139487.252280	35.958221
1333.585964	139757.566549	35.963239
1334.811753	140031.447351	35.968256
1336.325422	140284.208731	35.973274
1338.219328	140513.286238	35.978292
1340.127618	140749.362244	35.983309
1341.552226	140990.465317	35.988327
1343.249444	141207.178948	35.993344
1344.754935	141439.687276	35.998362
1346.290302	141667.437087	36.003380
1347.840365	141882.023690	36.008397
1348.992634	142102.802266	36.013415
1350.240243	142322.133523	36.018432
1352.212515	142534.840806	36.023450
1353.649045	142755.246667	36.028468
1355.511260	142957.551220	36.033485
1356.508719	143175.268126	36.038503
1357.943930	143379.979210	36.043520
1359.582965	143608.726269	36.048538
1360.730629	143822.402375	36.053556
1362.024863	144041.939533	36.058573
1363.251257	144250.520010	36.063591
1364.350280	144476.318730	36.068608
1365.461463	144701.863237	36.073626
1366.540766	144943.507285	36.078644
1367.721626	145177.552533	36.083661
1368.426379	145424.689666	36.088679
1369.514842	145680.971827	36.093696
1370.460384	145939.701749	36.098714
1371.571096	146210.745673	36.103732
1373.393888	146469.866552	36.108749
1374.364965	146755.991305	36.113767
1375.754998	147017.610156	36.118784
1377.113057	147297.283144	36.123802
1378.866867	147546.492875	36.128820
1381.029667	147806.543434	36.133837
1382.568746	148070.542104	36.138855
1384.206338	148331.419074	36.143872
1385.317367	148600.020250	36.148890
1386.544643	148855.413914	36.153908
1387.905588	149108.491558	36.158925
1388.845033	149388.503520	36.163943
1390.379926	149668.292011	36.168960
1391.738382	149937.331106	36.173978
1392.865983	150214.984352	36.178996
1393.786878	150494.589130	36.184013
1395.143834	150784.473426	36.189031
1396.605210	151075.230489	36.194048
1398.983737	151334.382087	36.199066
1401.939879	151578.853313	36.204084
1403.772033	151825.643402	36.209101
1405.281132	152075.482079	36.214119
1406.671379	152324.289327	36.219136
1408.360378	152567.835480	36.224154
1409.773643	152813.915009	36.229172
1411.324625	153046.236205	36.234189
1412.466375	153291.196861	36.239207
1414.193415	153517.910590	36.244224
1415.248222	153764.968915	36.249242
1416.315227	154009.591350	36.254260
1417.690020	154257.221290	36.259277
1418.607899	154511.752972	36.264295
1420.315995	154761.652155	36.269312
1421.348057	155004.345844	36.274330
1422.663919	155265.831190	36.279348
1424.039376	155511.020750	36.284365
1425.137796	155786.105958	36.289383
1426.653875	156038.683614	36.294400
1428.159171	156308.909963	36.299418
1429.006364	156583.446154	36.304436
1430.544902	156844.575183	36.309453
1431.524364	157102.500376	36.314471
1433.081651	157367.130930	36.319488
1434.591895	157613.566980	36.324506
1435.769659	157877.591484	36.329524
1437.567082	158129.209629	36.334541
1438.641059	158399.014153	36.339559
1439.713355	158657.834609	36.344576
1441.183254	158924.671861	36.349594
1442.350714	159206.924049	36.354612
1443.920332	159476.196814	36.359629
1444.570670	159765.008623	36.364647
1445.879931	160037.385666	36.369664
1447.578975	160333.918570	36.374682
1448.476367	160638.287346	36.379700
1450.177497	160938.820539	36.384717
1451.447232	161231.295154	36.389735
1452.476843	161541.357695	36.394752
1454.167178	161860.409587	36.399770
1455.456615	162168.949294	36.404788
1456.914110	162477.818635	36.409805
1458.415663	162792.988531	36.414823
1460.219657	163132.546613	36.419840
1461.730664	163435.374830	36.424858
1462.957675	163759.059980	36.429876
1464.723081	164069.869081	36.434893
1466.450363	164381.879405	36.439911
1468.066969	164696.244909	36.444928
1470.195045	165001.988872	36.449946
1471.505649	165319.924210	36.454964
1473.376178	165623.558273	36.459981
1475.045046	165927.354766	36.464999
1476.587008	166225.325079	36.470016
1478.322149	166523.189248	36.475034
1479.671539	166834.290066	36.480052
1481.335908	167130.139895	36.485069
1482.961306	167434.372688	36.490087
1484.600834	167736.803408	36.495104
1486.374152	168030.395233	36.500122
1487.797874	168328.285050	36.505140
1489.240517	168621.047334	36.510157
1490.842972	168919.050995	36.515175
1492.078618	169205.443382	36.520192
1493.801322	169503.900443	36.525210
1495.525458	169812.358429	36.530228
1496.781943	170100.567555	36.535245
1497.914053	170405.714234	36.540263
1499.221498	170707.242702	36.545280
1500.929661	171004.582548	36.550298
1502.242186	171323.384843	36.555316
1503.759698	171617.676605	36.560333
1505.988569	171924.263026	36.565351
1507.231261	172222.779145	36.570368
1509.189369	172523.234333	36.575386
1510.134999	172820.851733	36.580404
1511.536298	173117.938600	36.585421
1513.049124	173428.485964	36.590439
1514.411929	173733.641414	36.595456
1515.944071	174047.336815	36.600474
1517.274123	174354.354452	36.605492
1518.919950	174660.179527	36.610509
1520.902557	174979.847055	36.615527
1522.062651	175282.964624	36.620544
1523.601564	175592.074826	36.625562
1525.084667	175901.411978	36.630580
1526.678082	176205.960948	36.635597
1528.157848	176519.719024	36.640615
1529.588370	176829.096088	36.645632
1531.910177	177135.078333	36.650650
1533.550426	177419.409752	36.655668
1535.336214	177697.588690	36.660685
1536.811739	177980.427625	36.665703
1537.804810	178259.261446	36.670720
1539.378351	178533.977309	36.675738
1541.018903	178816.006671	36.680756
1542.455767	179107.082535	36.685773
1543.478610	179392.504665	36.690791
1544.551597	179693.251925	36.695808
1546.072919	179992.949323	36.700826
1547.339238	180290.634617	36.705844
1548.985997	180593.640016	36.710861
1550.432934	180908.547542	36.715879
1551.705768	181227.953520	36.720896
1553.200034	181539.683909	36.725914
1554.399795	181863.751267	36.730932
1556.024893	182193.626736	36.735949
1557.372238	182519.222114	36.740967
1558.096391	182866.614613	36.745984
1560.210134	183200.680028	36.751002
1561.671606	183548.602019	36.756020
1562.944881	183902.028102	36.761037
1564.874345	184257.137406	36.766055
1566.043547	184635.425745	36.771072
1567.739422	184986.897495	36.776090
1569.117533	185352.488312	36.781108
1570.869973	185702.939764	36.786125
1572.329325	186076.087103	36.791143
1573.615409	186448.732521	36.796160
1575.383694	186819.586821	36.801178
1576.891101	187192.822436	36.806196
1578.319079	187575.454364	36.811213
1579.886231	187949.345092	36.816231
1581.628034	188329.251609	36.821248
1583.284034	188701.786921	36.826266
1584.391595	189098.178908	36.831284
1586.417709	189473.729762	36.836301
1588.510575	189856.875817	36.841319
1589.798337	190237.593562	36.846336
1591.900029	190616.693560	36.851354
1593.673957	190991.216798	36.856372
1595.232544	191380.300683	36.861389
1597.828277	191724.669522	36.866407
1599.911094	192087.989731	36.871424
1601.822463	192433.199625	36.876442
1604.069048	192789.933626	36.881460
1605.560568	193133.465148	36.886477
1607.336804	193471.898748	36.891495
1608.850310	193822.945884	36.896512
1610.845885	194141.631256	36.901530
1612.729159	194486.095478	36.906548
1614.000448	194801.235318	36.911565
1616.418207	195131.243359	36.916583
1617.946948	195460.461013	36.921600
1619.763947	195773.534683	36.926618
1621.480916	196098.649136	36.931636
1622.637217	196419.630515	36.936653
1624.778238	196727.348296	36.941671
1626.122056	197053.951268	36.946688
1627.993412	197365.512756	36.951706
1629.054353	197690.959659	36.956724
1630.421916	198012.510455	36.961741
1631.667256	198344.760370	36.966759
1632.772600	198679.244237	36.971776
1634.369927	199020.859584	36.976794
1635.634382	199375.405738	36.981812
1636.999842	199730.140116	36.986829
1638.967130	200056.476499	36.991847
1640.370187	200406.688226	36.996864
1641.980145	200735.131134	37.001882
1643.670789	201071.929182	37.006900
1644.863505	201400.533228	37.011917
1646.933522	201739.366488	37.016935
1648.294677	202082.584935	37.021952
1649.517066	202410.642743	37.026970
1651.182055	202750.754092	37.031988
1652.360188	203107.796436	37.037005
1653.958329	203462.561636	37.042023
1655.216082	203825.168202	37.047040
1657.202522	204187.516082	37.052058
1659.077462	204528.972104	37.057076
1660.705206	204896.207757	37.062093
1662.859111	205242.661533	37.067111
1664.651326	205612.577890	37.072128
1666.721282	205968.292477	37.077146
1668.358806	206322.391628	37.082164
1669.761248	206685.800487	37.087181
1671.531746	207039.753875	37.092199
1673.367793	207411.080938	37.097216
1674.519397	207781.164541	37.102234
1676.272387	208133.944827	37.107252
1677.638026	208522.166732	37.112269
1679.434234	208889.659818	37.117287
1681.331947	209266.432554	37.122304
1682.975193	209639.350933	37.127322
1684.492992	210021.637479	37.132340
1685.824793	210410.559568	37.137357
1687.736057	210788.213094	37.142375
1689.398844	211182.467847	37.147392
1690.949012	211569.936848	37.152410
1692.837587	211965.478372	37.157428
1694.120778	212365.083905	37.162445
1695.869833	212756.258511	37.167463
1697.952029	213160.560583	37.172480
1699.501334	213550.197177	37.177498
1701.007614	213959.855471	37.182516
1702.773460	214363.580437	37.187533
1704.321670	214776.689451	37.192551
1706.497501	215176.007077	37.197568
1708.055420	215580.355940	37.202586
1709.791920	215979.698999	37.207604
1711.548706	216403.650763	37.212621
1713.321828	216804.743631	37.217639
1714.886120	217208.310966	37.222656
1716.658853	217625.687345	37.227674
1718.836012	218029.918400	37.232692
1720.555689	218472.070311	37.237709
1722.496068	218906.999832	37.242727
1724.174211	219313.579171	37.247744
1726.346781	219710.985474	37.252762
1727.886236	220109.945944	37.257780
1729.290447	220505.298314	37.262797
1731.434410	220903.247218	37.267815
1733.298805	221313.359223	37.272832
1734.886789	221714.654318	37.277850
1736.860946	222116.217059	37.282868
1738.436447	222524.171725	37.287885
1740.264028	222913.696987	37.292903
1742.054356	223317.529616	37.297920
1743.659493	223717.127240	37.302938
1745.456489	224112.960698	37.307956
1746.751724	224507.532464	37.312973
1748.683174	224915.004759	37.317991
1750.169685	225318.843798	37.323008
1751.629066	225739.935209	37.328026
1753.741546	226148.905612	37.333044
1755.624366	226537.849352	37.338061
1757.972154	226915.693560	37.343079
1759.925255	227285.679424	37.348096
1761.683115	227661.210566	37.353114
1763.205486	228032.031940	37.358132
1764.945804	228416.585267	37.363149
1766.436788	228787.667943	37.368167
1767.915333	229179.988576	37.373184
1769.348688	229557.179023	37.378202
1771.561482	229937.899016	37.383220
1772.829186	230337.344637	37.388237
1774.790575	230720.978674	37.393255
1776.382996	231121.896698	37.398272
1778.324979	231524.586750	37.403290
1780.290707	231922.904965	37.408308
1781.907452	232326.794103	37.413325
1783.271694	232724.375844	37.418343
1785.125795	233139.277273	37.423360
1786.563227	233562.529667	37.428378
1787.893169	233984.505508	37.433396
1789.176461	234416.828553	37.438413
1790.752491	234842.042574	37.443431
1792.475866	235304.014735	37.448448
1794.315960	235752.099474	37.453466
1796.199548	236202.896119	37.458484
1797.600750	236664.391772	37.463501
1799.418803	237123.380919	37.468519
1801.131647	237592.396968	37.473536
1802.916220	238059.547926	37.478554
1805.416872	238504.354547	37.483572
1807.374290	238976.407000	37.488589
1809.125087	239437.495646	37.493607
1810.920934	239901.702302	37.498624
1812.606137	240371.872413	37.503642
1814.937340	240827.101522	37.508660
1816.893396	241302.995017	37.513677
1818.643873	241773.335017	37.518695
1820.641565	242225.904058	37.523712
1822.450745	242698.319115	37.528730
1824.520490	243149.201318	37.533748
1826.328114	243621.008661	37.538765
1828.603300	244074.779688	37.543783
1830.832005	244527.136607	37.548800
1833.138124	244974.273857	37.553818
1836.087386	245407.765542	37.558836
1837.781211	245832.930547	37.563853
1839.915063	246267.879498	37.568871
1841.770159	246692.358442	37.573888
1843.478230	247122.857360	37.578906
1845.734019	247539.142028	37.583924
1847.485317	247966.510241	37.588941
1849.512492	248378.108786	37.593959
1851.462266	248803.616024	37.598976
1853.298204	249229.269581	37.603994
1854.874233	249644.398964	37.609012
1856.636930	250062.063508	37.614029
1858.351785	250486.290347	37.619047
1859.891341	250910.673613	37.624064
1861.143048	251349.330673	37.629082
1863.033373	251779.753254	37.634100
1864.275065	252234.518250	37.639117
1866.229138	252686.447392	37.644135
1868.229287	253127.217198	37.649152
1869.470439	253593.516252	37.654170
1870.915240	254038.493929	37.659188
1872.507310	254513.855112	37.664205
1874.307232	254968.656258	37.669223
1876.102209	255435.601176	37.674240
1878.233025	255900.737796	37.679258
1879.793519	256356.976307	37.684276
1881.871214	256800.021146	37.689293
1884.018772	257247.119029	37.694311
1886.694737	257669.386623	37.699328
1888.369847	258127.181490	37.704346
1890.523411	258556.902678	37.709364
1891.870440	259002.355138	37.714381
1893.809711	259443.568716	37.719399
1895.672390	259881.289298	37.724416
1897.461751	260343.078890	37.729434
1899.614538	260772.012542	37.734452
1901.829663	261228.625347	37.739469
1903.416130	261686.510740	37.744487
1905.082825	262134.958078	37.749504
1906.479081	262608.548470	37.754522
1908.160750	263066.290546	37.759540
1910.283967	263555.510045	37.764557
1911.698932	264037.479682	37.769575
1913.779195	264517.255723	37.774592
1915.578182	264992.353053	37.779610
1917.843392	265472.021567	37.784628
1919.704575	265962.324349	37.789645
1921.774181	266453.913136	37.794663
1923.730949	266940.922203	37.799680
1925.605835	267436.987851	37.804698
1927.508400	267919.254541	37.809716
1929.608792	268416.780542	37.814733
1931.316783	268918.765687	37.819751
1933.962578	269407.766339	37.824768
1935.049815	269908.684529	37.829786
1937.558001	270397.986119	37.834804
1939.937677	270886.215997	37.839821
1942.426722	271384.207124	37.844839
1944.420372	271871.051541	37.849856
1946.167179	272363.169054	37.854874
1948.041233	272850.158739	37.859892
1949.910342	273351.856549	37.864909
1951.807086	273847.122025	37.869927
1953.915394	274343.494658	37.874944
1955.457702	274852.610563	37.879962
1957.820040	275347.288014	37.884980
1959.509889	275862.346988	37.889997
1961.055452	276362.924026	37.895015
1963.519012	276860.299621	37.900032
1965.535891	277369.509349	37.905050
1967.415105	277874.447737	37.910068
1969.614958	278380.703523	37.915085
1971.105479	278893.807133	37.920103
1973.134589	279418.124091	37.925120
1974.835762	279937.896243	37.930138
1976.594432	280453.491567	37.935156
1978.817526	280979.194643	37.940173
1980.462706	281510.605730	37.945191
1982.938327	282024.985593	37.950208
1984.641204	282552.167334	37.955226
1986.604834	283081.437978	37.960244
1988.671515	283602.332829	37.965261
1990.795612	284118.872896	37.970279
1994.140830	284623.041826	37.975296
1996.280592	285135.892826	37.980314
1998.447056	285629.991730	37.985332
2001.006601	286124.684333	37.990349
2002.965027	286624.402650	37.995367
2005.483406	287109.598848	38.000384
2007.173332	287596.175289	38.005402
2008.951058	288086.520205	38.010420
2010.978429	288570.598907	38.015437
2012.778875	289059.387170	38.020455
2014.820097	289510.465057	38.025472
2016.118932	289991.789105	38.030490
2018.022561	290460.311108	38.035508
2019.922919	290925.479138	38.040525
2021.510139	291413.100118	38.045543
2023.611441	291900.481636	38.050560
2025.041410	292398.487942	38.055578
2027.089185	292882.750238	38.060596
2029.117768	293378.265761	38.065613
2030.668147	293888.513906	38.070631
2032.849489	294392.711841	38.075648
2034.173193	294905.532971	38.080666
2036.084458	295418.051248	38.085684
2038.046343	295947.017328	38.090701
2040.069407	296488.619361	38.095719
2042.657256	297008.536195	38.100736
2044.769572	297533.735985	38.105754
2046.770075	298065.174306	38.110772
2049.089421	298601.179592	38.115789
2050.749977	299140.796157	38.120807
2052.848574	299685.518489	38.125824
2054.640995	300227.697973	38.130842
2056.472277	300791.964120	38.135860
2058.953181	301340.550619	38.140877
2061.003047	301901.243796	38.145895
2063.207960	302459.012669	38.150912
2065.084370	303015.359589	38.155930
2067.546423	303564.215602	38.160948
2069.669145	304116.070556	38.165965
2071.641533	304678.156516	38.170983
2074.566736	305231.065309	38.176000
2076.460834	305777.233591	38.181018
2078.850875	306343.785667	38.186036
2081.215431	306886.389713	38.191053
2083.229383	307437.403621	38.196071
2085.715918	307983.180290	38.201088
2088.005510	308520.097530	38.206106
2089.896583	309079.729981	38.211124
2092.236689	309615.031734	38.216141
2094.270538	310172.220408	38.221159
2095.968887	310709.068641	38.226176
2098.383583	311271.138483	38.231194
2100.289877	311828.996792	38.236212
2102.554541	312374.348464	38.241229
2104.039433	312934.122302	38.246247
2106.157194	313493.990307	38.251264
2108.165328	314065.197892	38.256282
2110.054739	314635.531943	38.261300
2112.780448	315180.050308	38.266317
2114.661344	315754.262178	38.271335
2116.972759	316311.714943	38.276352
2119.004559	316889.041403	38.281370
2121.118505	317450.682290	38.286388
2123.126157	318017.389326	38.291405
2125.321749	318594.750668	38.296423
2127.524568	319155.321849	38.301440
2130.369729	319709.230921	38.306458
2132.767913	320263.158656	38.311476
2135.585248	320801.904509	38.316493
2137.933653	321356.389927	38.321511
2140.062778	321901.283798	38.326528
2141.889137	322435.025930	38.331546
2144.009818	322985.218670	38.336564
2146.144749	323526.949334	38.341581
2147.973385	324075.048183	38.346599
2150.045736	324630.794967	38.351616
2151.944303	325172.728229	38.356634
2153.712524	325722.625163	38.361652
2155.941614	326259.340020	38.366669
2157.235793	326804.380173	38.371687
2158.874291	327340.446925	38.376704
2160.867776	327889.905921	38.381722
2162.548314	328462.870313	38.386740
2164.513798	329014.709917	38.391757
2166.545802	329590.473853	38.396775
2168.325921	330164.471240	38.401792
2170.659309	330746.114316	38.406810
2172.282913	331340.130850	38.411828
2174.166573	331940.825494	38.416845
2175.811693	332550.438394	38.421863
2177.643647	333173.595176	38.426880
2179.974784	333794.428254	38.431898
2181.436378	334435.528935	38.436916
2183.635148	335078.149941	38.441933
2185.960241	335723.966176	38.446951
2187.831635	336375.611970	38.451968
2190.300631	337034.791367	38.456986
2192.673266	337685.550922	38.462004
2196.127735	338323.152099	38.467021
2199.597392	338955.793084	38.472039
2201.870531	339590.121940	38.477056
2204.206400	340218.061385	38.482074
2206.398477	340846.752852	38.487092
2209.219089	341475.560710	38.492109
2211.203900	342103.585215	38.497127
2213.390600	342730.096104	38.502144
2216.382873	343348.039000	38.507162
2218.953126	343967.490557	38.512180
2221.319474	344562.856496	38.517197
2223.817058	345184.233183	38.522215
2226.128825	345798.449993	38.527232
2228.824871	346401.326659	38.532250
2230.489128	347005.939873	38.537268
2232.847693	347617.840786	38.542285
2234.144656	348244.045095	38.547303
2236.687309	348865.669491	38.552320
2238.534956	349493.161167	38.557338
2240.741578	350117.869259	38.562356
2242.957220	350736.476633	38.567373
2245.104746	351380.793157	38.572391
2247.470459	352005.600540	38.577408
2249.716133	352643.259059	38.582426
2251.910256	353281.043623	38.587444
2254.361126	353926.947023	38.592461
2256.138235	354570.161026	38.597479
2258.229433	355220.164363	38.602496
2260.643482	355852.875320	38.607514
2262.468223	356522.136135	38.612532
2264.948692	357159.358188	38.617549
2267.599506	357808.162954	38.622567
2269.396308	358473.286465	38.627584
2272.526792	359121.255216	38.632602
2274.430277	359786.035154	38.637620
2276.773950	360424.649726	38.642637
2278.822629	361090.525746	38.647655
2280.889379	361744.260636	38.652672
2283.105911	362405.190331	38.657690
2285.352073	363073.562616	38.662708
2288.050311	363724.242512	38.667725
2290.350582	364391.644546	38.672743
2292.849050	365058.444108	38.677760
2295.197296	365703.060200	38.682778
2297.113340	366370.085504	38.687796
2299.574279	367030.743223	38.692813
2301.708664	367683.833493	38.697831
2304.374506	368344.484864	38.702848
2306.400899	368975.197633	38.707866
2308.504169	369616.844606	38.712884
2310.522373	370246.243345	38.717901
2312.988128	370888.416767	38.722919
2315.025677	371536.534109	38.727936
2316.916093	372180.200241	38.732954
2318.863045	372830.465160	38.737972
2320.948727	373494.213380	38.742989
2323.438765	374156.461966	38.748007
2325.294001	374837.291658	38.753024
2327.339572	375511.051655	38.758042
2329.876492	376203.965798	38.763060
2332.344847	376878.948010	38.768077
2334.781820	377562.265423	38.773095
2336.843949	378269.925044	38.778112
2339.607547	378957.293949	38.783130
2341.622572	379655.930269	38.788148
2343.937421	380352.118859	38.793165
2346.498885	381059.890877	38.798183
2348.592350	381777.588877	38.803200
2351.240987	382474.996288	38.808218
2353.795962	383183.433883	38.813236
2356.592014	383900.563531	38.818253
2358.816722	384613.106811	38.823271
2360.795726	385332.900787	38.828288
2363.543410	386041.801761	38.833306
2365.552680	386775.350275	38.838324
2367.745676	387503.755741	38.843341
2370.104556	388232.801424	38.848359
2372.282984	388981.456006	38.853376
2374.865265	389718.339469	38.858394
2377.036459	390458.188669	38.863412
2379.462308	391200.183313	38.868429
2382.420878	391947.673747	38.873447
2385.293849	392685.882873	38.878464
2387.958908	393416.985998	38.883482
2390.522889	394147.201027	38.888500
2393.044377	394881.714080	38.893517
2395.660947	395612.771746	38.898535
2398.022928	396340.457415	38.903552
2400.103564	397077.396851	38.908570
2402.569326	397817.776733	38.913588
2404.876440	398554.388093	38.918605
2407.793035	399290.778514	38.923623
2409.790529	400027.048919	38.928640
2412.153924	400762.276961	38.933658
2414.656432	401517.354855	38.938676
2417.161954	402269.878295	38.943693
2419.672090	403003.351746	38.948711
2421.552897	403748.565679	38.953728
2423.948651	404494.612017	38.958746
2425.988385	405264.158888	38.963764
2428.351673	406016.655871	38.968781
2430.781718	406780.978081	38.973799
2433.007776	407557.447916	38.978816
2435.319336	408331.170803	38.983834
2437.578661	409113.569465	38.988852
2439.443178	409887.600535	38.993869
2442.931292	410664.937593	38.998887
2445.086385	411446.930898	39.003904
2447.700195	412217.046837	39.008922
2449.632034	413020.181200	39.013940
2452.142038	413798.474800	39.018957
2455.085519	414578.269141	39.023975
2457.149553	415378.903116	39.028992
2459.617293	416167.010397	39.034010
2462.395106	416957.321531	39.039028
2465.304916	417730.872237	39.044045
2467.624937	418488.036635	39.049063
2470.042057	419230.981460	39.054080
2472.251916	419974.293265	39.059098
2475.019856	420722.681652	39.064116
2477.263102	421478.477557	39.069133
2479.853813	422226.141247	39.074151
2482.071860	422981.895618	39.079168
2484.612750	423744.991735	39.084186
2486.846924	424519.153443	39.089204
2489.156362	425277.885509	39.094221
2492.016508	426038.882484	39.099239
2494.387532	426815.125706	39.104256
2497.080521	427573.874272	39.109274
2499.853058	428350.052139	39.114292
2502.743760	429112.668156	39.119309
2505.288384	429874.102022	39.124327
2507.675528	430645.864454	39.129344
2510.608541	431418.422438	39.134362
2512.855212	432186.462240	39.139380
2515.972459	432966.835207	39.144397
2518.148148	433732.507398	39.149415
2520.753011	434504.916132	39.154432
2523.421602	435278.604347	39.159450
2526.108365	436050.087199	39.164468
2528.623029	436824.406576	39.169485
2531.619270	437595.077367	39.174503
2533.956498	438385.567142	39.179520
2536.677979	439149.601043	39.184538
2538.908157	439937.321386	39.189556
2541.778988	440713.978272	39.194573
2544.248276	441492.749033	39.199591
2546.615260	442269.738457	39.204608
2549.628968	443044.974426	39.209626
2552.405492	443819.817529	39.214644
2554.883644	444609.252841	39.219661
2557.792420	445375.873583	39.224679
2560.482262	446155.706827	39.229696
2563.184779	446932.929918	39.234714
2565.722406	447703.626854	39.239732
2567.760875	448484.191596	39.244749
2570.689404	449275.859856	39.249767
2573.127614	450064.646183	39.254784
2575.583795	450846.673419	39.259802
2578.012685	451635.958863	39.264820
2580.940228	452420.226500	39.269837
2583.560831	453204.313179	39.274855
2586.254673	454002.669159	39.279872
2588.415578	454799.161003	39.284890
2591.046691	455588.111201	39.289908
2593.181948	456388.287573	39.294925
2595.893174	457182.623909	39.299943
2599.018947	457982.725500	39.304960
2601.289211	458774.645733	39.309978
2604.381971	459572.162076	39.314996
2607.440863	460359.238455	39.320013
2610.443308	461145.787733	39.325031
2613.138296	461936.097515	39.330048
2615.555110	462727.230655	39.335066
2618.447626	463516.231647	39.340084
2620.802435	464312.062815	39.345101
2622.823090	465098.112078	39.350119
2625.229523	465895.689880	39.355136
2627.022393	466706.627767	39.360154
2629.475369	467512.520667	39.365172
2631.967666	468342.477513	39.370189
2634.874428	469163.234517	39.375207
2636.837453	469994.672961	39.380224
2638.997114	470823.819529	39.385242
2641.790344	471631.857715	39.390260
2643.522286	472444.937668	39.395277
2646.241813	473252.868258	39.400295
2649.022969	474076.515334	39.405312
2651.079266	474900.448190	39.410330
2654.075407	475722.320154	39.415348
2656.719360	476553.558500	39.420365
2659.260574	477379.523644	39.425383
2661.840686	478233.779232	39.430400
2664.098154	479084.664723	39.435418
2667.088624	479925.289071	39.440436
2669.411639	480788.457112	39.445453
2672.047874	481636.231809	39.450471
2674.847000	482513.175901	39.455488
2677.180556	483378.894666	39.460506
2680.357473	484257.761235	39.465524
2682.865918	485133.262059	39.470541
2685.774650	486007.795322	39.475559
2688.583992	486897.244446	39.480576
2691.518860	487777.895065	39.485594
2694.758136	488658.703565	39.490612
2697.788501	489541.824115	39.495629
2700.446242	490406.640414	39.500647
2703.405857	491284.536123	39.505664
2705.759434	492174.498578	39.510682
2708.932325	493050.755202	39.515700
2711.550928	493945.880854	39.520717
2715.252682	494794.963975	39.525735
2718.553907	495670.913709	39.530752
2721.289721	496529.555763	39.535770
2724.164354	497389.594319	39.540788
2726.623159	498275.941366	39.545805
2729.290821	499140.212720	39.550823
2731.992487	500016.086123	39.555840
2734.648125	500896.309398	39.560858
2737.108651	501762.849631	39.565876
2739.693636	502650.607463	39.570893
2742.525037	503539.638346	39.575911
2744.741799	504433.765712	39.580928
2746.862323	505339.407839	39.585946
2749.647316	506240.805325	39.590964
2751.966070	507166.179911	39.595981
2754.189999	508100.441228	39.600999
2756.777092	509037.562745	39.606016
2759.019636	509986.382154	39.611034
2761.576597	510944.670948	39.616052
2764.013191	511916.834043	39.621069
2766.628432	512889.260769	39.626087
2769.378796	513864.528429	39.631104
2771.804213	514859.696074	39.636122
2775.305498	515820.455626	39.641140
2778.308159	516803.611859	39.646157
2781.571929	517781.623942	39.651175
2784.755130	518758.781389	39.656192
2787.883026	519733.115084	39.661210
2790.959078	520685.430827	39.666228
2793.959591	521661.678078	39.671245
2796.636179	522620.387138	39.676263
2799.530339	523592.599060	39.681280
2802.294308	524558.524763	39.686298
2805.349866	525519.052312	39.691316
2807.997841	526478.830434	39.696333
2811.352186	527426.747665	39.701351
2815.109714	528380.227648	39.706368
2817.721268	529333.382806	39.711386
2820.665760	530271.871571	39.716404
2823.377667	531208.224652	39.721421
2826.539928	532128.133599	39.726439
2829.336029	533022.726195	39.731456
2831.819347	533925.419265	39.736474
2834.752673	534810.919957	39.741492
2837.486635	535719.650488	39.746509
2840.109372	536601.569990	39.751527
2842.810685	537500.581751	39.756544
2845.106863	538397.239233	39.761562
2847.938881	539305.475027	39.766580
2850.894553	540227.719509	39.771597
2853.702829	541138.055809	39.776615
2857.084833	542044.968804	39.781632
2859.338300	542965.692061	39.786650
2862.309303	543878.389800	39.791668
2865.196777	544805.828474	39.796685
2867.862482	545718.858873	39.801703
2871.544719	546635.633920	39.806720
2874.944336	547569.240409	39.811738
2877.821953	548491.908824	39.816756
2880.826629	549414.544656	39.821773
2883.219031	550343.252658	39.826791
2886.335827	551268.309064	39.831808
2888.981140	552212.231019	39.836826
2892.006078	553139.588225	39.841844
2895.315506	554066.231715	39.846861
2898.570900	554989.855318	39.851879
2901.978510	555911.229390	39.856896
2904.449357	556841.890884	39.861914
2907.363842	557766.284067	39.866932
2910.385970	558717.827137	39.871949
2912.701233	559667.057652	39.876967
2915.608390	560613.861543	39.881984
2918.073764	561566.196088	39.887002
2920.626442	562523.269150	39.892020
2923.166489	563505.236210	39.897037
2925.851520	564492.177769	39.902055
2928.717773	565472.034275	39.907072
2931.052629	566470.634279	39.912090
2933.850899	567469.130683	39.917108
2936.976413	568481.101285	39.922125
2939.590729	569493.679059	39.927143
2942.588063	570517.508194	39.932160
2945.251546	571556.217805	39.937178
2948.558371	572574.961393	39.942196
2951.291155	573617.104342	39.947213
2954.055284	574651.929899	39.952231
2957.280365	575700.894498	39.957248
2959.849505	576764.379686	39.962266
2962.881846	577820.272704	39.967284
2965.820403	578876.844049	39.972301
2968.383569	579946.077888	39.977319
2971.637316	581010.741403	39.982336
2974.259798	582091.565920	39.987354
2977.516604	583167.075295	39.992372
2980.944700	584228.271361	39.997389
2984.235196	585310.606088	40.002407
2987.482596	586380.769209	40.007424
2990.566942	587445.851667	40.012442
2994.056742	588496.687873	40.017460
2996.925842	589573.046023	40.022477
2999.774001	590631.720191	40.027495
3002.930517	591703.478796	40.032512
3005.672199	592769.296765	40.037530
3008.316921	593838.441841	40.042548
3011.101607	594920.943248	40.047565
3014.368841	596003.465631	40.052583
3017.483913	597069.233760	40.057600
3020.160043	598150.102623	40.062618
3023.702735	599214.201708	40.067636
3026.797645	600258.247376	40.072653
3029.883838	601278.917561	40.077671
3033.725180	602281.398835	40.082688
3036.744618	603299.047196	40.087706
3039.511046	604313.693657	40.092724
3042.787308	605313.450187	40.097741
3045.748851	606335.342389	40.102759
3048.857244	607347.559960	40.107776
3051.606366	608380.212468	40.112794
3054.178949	609399.340328	40.117812
3057.433528	610432.171439	40.122829
3060.146053	611457.543232	40.127847
3063.368316	612500.744176	40.132864
3065.855820	613569.727224	40.137882
3068.358760	614615.399605	40.142900
3071.119688	615686.183857	40.147917
3073.774932	616771.832156	40.152935
3076.739538	617859.671982	40.157952
3079.425584	618968.346407	40.162970
3082.588675	620074.480096	40.167988
3085.907216	621188.672668	40.173005
3088.339077	622328.035488	40.178023
3091.076018	623452.236621	40.183040
3094.160622	624596.998790	40.188058
3097.639221	625749.817288	40.193076
3100.918174	626900.046945	40.198093
3103.949875	628061.482089	40.203111
3107.130158	629225.812427	40.208128
3109.897870	630401.968438	40.213146
3112.968491	631580.789598	40.218164
3115.705887	632774.162529	40.223181
3118.363263	633973.203856	40.228199
3121.750025	635168.193496	40.233216
3124.673695	636382.138333	40.238234
3127.629848	637608.711310	40.243252
3131.074811	638816.296383	40.248269
3134.978892	640040.178442	40.253287
3138.619134	641247.396074	40.258304
3142.013657	642466.034376	40.263322
3145.090618	643676.400241	40.268340
3148.423602	644879.997079	40.273357
3151.878542	646097.342479	40.278375
3155.232191	647298.005516	40.283392
3158.404934	648515.504468	40.288410
3161.678481	649728.751750	40.293428
3165.019699	650939.697565	40.298445
3167.638157	652160.482539	40.303463
3170.987828	653366.497117	40.308480
3174.318833	654587.762275	40.313498
3177.225075	655808.846833	40.318516
3180.725390	657028.984209	40.323533
3183.612814	658255.893788	40.328551
3186.716422	659481.219224	40.333568
3190.445497	660699.216943	40.338586
3193.361011	661929.741478	40.343604
3197.335861	663135.494021	40.348621
3200.699348	664346.123997	40.353639
3204.370582	665536.296531	40.358656
3208.172205	666736.798441	40.363674
3211.424464	667936.593360	40.368692
3214.755539	669120.802858	40.373709
3217.700554	670323.083053	40.378727
3221.064462	671507.535664	40.383744
3223.740594	672710.053520	40.388762
3226.678890	673915.357284	40.393780
3230.109943	675102.477757	40.398797
3233.430702	676300.450775	40.403815
3237.032204	677469.545596	40.408832
3240.360541	678615.330654	40.413850
3243.552616	679750.164069	40.418868
3246.741072	680890.273784	40.423885
3249.868517	682031.891472	40.428903
3253.183704	683156.795651	40.433920
3256.213919	684297.351994	40.438938
3258.991080	685445.504347	40.443956
3261.658329	686596.707438	40.448973
3264.483565	687774.645796	40.453991
3267.507202	688945.746074	40.459008
3270.431425	690132.940143	40.464026
3273.099913	691332.078428	40.469044
3276.526873	692530.831357	40.474061
3279.402584	693759.976097	40.479079
3282.774555	694978.550980	40.484096
3286.416254	696173.354432	40.489114
3289.505411	697422.588852	40.494132
3293.275122	698643.270387	40.499149
3296.228837	699897.927316	40.504167
3299.440418	701140.613566	40.509184
3302.267414	702403.705610	40.514202
3305.265554	703675.307798	40.519220
3308.342199	704959.494063	40.524237
3311.495906	706258.785000	40.529255
3314.905041	707548.872104	40.534272
3318.535113	708829.665492	40.539290
3321.822423	710126.665076	40.544308
3325.613551	711431.801096	40.549325
3328.741663	712751.004391	40.554343
3331.997370	714056.270883	40.559360
3335.420016	715377.144342	40.564378
3338.647581	716713.923963	40.569396
3341.721480	718037.356375	40.574413
3344.991095	719374.446640	40.579431
3348.176377	720722.958736	40.584448
3351.781154	722065.298297	40.589466
3354.714646	723419.743082	40.594484
3358.831462	724775.648520	40.599501
3362.213116	726126.213040	40.604519
3365.746880	727479.445573	40.609536
3370.069757	728818.489436	40.614554
3373.892652	730160.606833	40.619572
3378.441903	731485.095276	40.624589
3382.029489	732805.278930	40.629607
3385.937116	734113.590442	40.634624
3389.670377	735406.364636	40.639642
3393.156895	736706.671338	40.644660
3396.839287	737991.879318	40.649677
3400.098490	739301.967288	40.654695
3403.490808	740584.633355	40.659712
3407.046510	741867.262053	40.664730
3409.957412	743175.879086	40.669748
3413.450433	744454.792849	40.674765
3416.294565	745767.476895	40.679783
3419.184253	747074.067157	40.684800
3422.197751	748390.768380	40.689818
3425.202760	749719.469144	40.694836
3428.245796	751050.892149	40.699853
3431.142377	752389.794806	40.704871
3433.921348	753758.873126	40.709888
3437.301731	755110.815966	40.714906
3439.911787	756497.407317	40.719924
3443.689913	757873.364020	40.724941
3446.879416	759254.779899	40.729959
3449.966472	760651.215599	40.734976
3453.674091	762042.961332	40.739994
3457.231267	763435.212738	40.745012
3460.845419	764807.756471	40.750016
3464.005247	766145.245635	40.755021
3467.475082	767434.929308	40.760026
3471.386797	768643.200069	40.765031
3474.415006	769804.413360	40.770036
3477.761367	770871.540077	40.775040
3481.527122	771870.120362	40.780045
3484.721988	772803.005029	40.785050
3488.046752	773644.641924	40.790055
3490.548674	774427.769054	40.795060
3493.344809	775134.790280	40.800064
3496.196300	775763.896113	40.805069
3498.228559	776334.155356	40.810074
3500.911596	776838.890198	40.815079
3502.618218	777282.567064	40.820084
3504.915334	777650.516487	40.825088
3506.590620	777972.924484	40.830093
3508.179756	778242.375293	40.835098
3509.869282	778453.134990	40.840103
3511.149376	778623.354581	40.845108
3512.578107	778748.958418	40.850112
3513.594902	778851.842708	40.855117
3514.681891	778897.037254	40.860122
3515.745548	778905.424648	40.865127
3516.318831	778904.444304	40.870132
3517.631946	778850.979590	40.875136
3518.112239	778786.480737	40.880141
3518.639896	778685.161646	40.885146
3519.530693	778564.931958	40.890151
3519.675649	778422.036750	40.895156
3520.325530	778261.583392	40.900160
3520.837538	778077.524714	40.905165
3521.008623	777884.264508	40.910170
3521.202415	777662.152123	40.915175
3521.442228	777444.110800	40.920180
3521.835056	777201.918019	40.925184
3522.020401	776969.744244	40.930189
3521.789430	776707.406442	40.935194
3522.225815	776445.588897	40.940199
3522.265580	776169.156736	40.945204
3522.359538	775886.698767	40.950208
3522.402200	775615.020730	40.955213
3522.551667	775310.178792	40.960218
3522.983357	775012.367879	40.965223
3522.761898	774708.842396	40.970228
3522.968988	774393.759964	40.975232
3522.779614	774076.562732	40.980237
3522.638082	773761.658489	40.985242
3522.918653	773426.675815	40.990247
3522.613753	773115.366050	40.995252
3522.907403	772783.750259	41.000256
3522.819924	772454.546785	41.005261
3522.596005	772124.710786	41.010266
3522.677626	771779.637381	41.015271
3522.487580	771455.627814	41.020276
3522.346117	771114.501156	41.025280
3522.289654	770782.064946	41.030285
3522.041928	770452.059577	41.035290
3522.201601	770111.181732	41.040295
3522.087798	769782.356148	41.045300
3521.914080	769430.021289	41.050304
3522.181766	769101.496662	41.055309
3521.685831	768773.675046	41.060314
3521.798425	768430.657941	41.065319
3522.024556	768098.153189	41.070324
3521.713348	767750.049097	41.075328
3521.284467	767412.397504	41.080333
3520.901564	767068.758722	41.085338
3521.272389	766735.479122	41.090343
3521.215466	766405.706040	41.095348
3520.628447	766069.942316	41.100352
3520.933035	765741.016808	41.105357
3520.568721	765412.976210	41.110362
3520.496797	765080.139657	41.115367
3520.459736	764764.687861	41.120372
3520.388302	764435.027502	41.125376
3520.545263	764098.263415	41.130381
3520.068831	763785.653774	41.135386
3520.139564	763455.778963	41.140391
3519.724746	763137.658161	41.145396
3519.541347	762819.929531	41.150400
3519.766182	762497.878365	41.155405
3519.233753	762194.040372	41.160410
3519.460874	761866.240287	41.165415
3519.224554	761560.453445	41.170420
3518.996989	761234.871494	41.175424
3519.276895	760926.359179	41.180429
3518.443784	760625.862298	41.185434
3518.496014	760308.679637	41.190439
3518.010124	760008.791565	41.195444
3518.181157	759706.217383	41.200448
3517.988552	759412.572748	41.205453
3517.860734	759120.682410	41.210458
3517.748587	758817.132690	41.215463
3517.590524	758531.886377	41.220468
3517.485234	758241.784398	41.225472
3517.480923	757954.763796	41.230477
3517.353620	757669.282643	41.235482
3517.554319	757381.515611	41.240487
3517.059507	757089.607963	41.245492
3517.266128	756803.644346	41.250496
3517.074230	756523.955302	41.255501
3516.748975	756237.021784	41.260506
3516.749347	755954.663914	41.265511
3516.601764	755682.933756	41.270516
3516.300911	755403.764747	41.275520
3516.491354	755130.231234	41.280525
3516.369021	754862.367968	41.285530
3516.362970	754586.477700	41.290535
3515.903237	754321.761804	41.295540
3515.998086	754040.255876	41.300544
3515.554070	753777.197404	41.305549
3515.338345	753516.314292	41.310554
3515.389850	753252.810325	41.315559
3515.089116	753007.429804	41.320564
3514.972306	752759.936906	41.325568
3515.051177	752504.600674	41.330573
3515.045214	752248.825511	41.335578
3515.090002	751997.132820	41.340583
3514.901046	751761.325124	41.345588
3514.769211	751501.989845	41.350592
3514.940256	751246.744941	41.355597
3514.393541	751010.331312	41.360602
3514.379377	750760.781506	41.365607
3514.019598	750518.344841	41.370612
3513.988202	750280.539374	41.375616
3514.099400	750034.996310	41.380621
3513.748790	749809.036237	41.385626
3514.105779	749565.265617	41.390631
3513.776468	749336.422757	41.395636
3513.470407	749109.249183	41.400640
3513.715835	748880.396724	41.405645
3513.237345	748657.191187	41.410650
3513.522084	748420.363528	41.415655
3513.176804	748199.395812	41.420660
3513.203511	747980.979356	41.425664
3512.969281	747755.335651	41.430669
3512.704292	747542.341517	41.435674
3512.851379	747320.130877	41.440679
3512.833735	747105.897882	41.445684
3512.705454	746890.491160	41.450688
3512.894136	746668.601058	41.455693
3512.118864	746459.516731	41.460698
3512.443280	746253.012942	41.465703
3512.395010	746044.044491	41.470708
3512.170531	745827.141536	41.475712
3512.165346	745618.846617	41.480717
3511.976119	745420.364001	41.485722
3512.001992	745216.600946	41.490727
3511.645671	745021.843303	41.495732
3511.660827	744818.318839	41.500736
3511.701082	744623.782388	41.505741
3511.561792	744433.225801	41.510746
3511.544586	744231.718422	41.515751
3511.325700	744043.241963	41.520756
3510.947333	743862.302412	41.525760
3511.328024	743663.582308	41.530765
3511.072863	743473.911579	41.535770
3510.721364	743283.609416	41.540775
3510.760806	743099.122127	41.545780
3510.479842	742918.837030	41.550784
3510.285572	742745.307896	41.555789
3510.284790	742570.506733	41.560794
3510.689063	742396.129264	41.565799
3510.314363	742215.843587	41.570804
3509.998839	742053.643678	41.575808
3509.982351	741866.070735	41.580813
3509.764983	741709.584174	41.585818
3510.121463	741532.524988	41.590823
3509.828795	741376.835578	41.595828
3509.831195	741214.516451	41.600832
3509.927311	741037.538676	41.605837
3509.905600	740882.042049	41.610842
3510.109497	740711.864651	41.615847
3509.852836	740545.370438	41.620852
3509.669772	740377.722915	41.625856
3509.790907	740212.791564	41.630861
3509.297795	740051.618712	41.635866
3509.456433	739886.674386	41.640871
3509.431263	739741.642777	41.645876
3509.169178	739581.411537	41.650880
3509.293165	739428.484143	41.655885
3508.888653	739284.892015	41.660890
3509.162553	739123.573571	41.665895
3509.030168	738968.601923	41.670900
3508.813821	738818.736828	41.675904
3508.633494	738660.007161	41.680909
3508.876457	738530.542842	41.685914
3508.709901	738364.334345	41.690919
3508.477196	738228.808756	41.695924
3508.494993	738081.364912	41.700928
3508.514070	737945.693946	41.705933
3508.288529	737804.865798	41.710938
3507.831896	737653.732041	41.715943
3507.963909	737523.576990	41.720948
3508.415031	737392.476415	41.725952
3508.306353	737253.499527	41.730957
3507.715242	737126.228522	41.735962
3507.868833	736983.294413	41.740967
3507.870445	736858.741790	41.745972
3507.750266	736729.357756	41.750976
3507.971141	736603.973161	41.755981
3507.675058	736482.532039	41.760986
3507.688991	736336.046364	41.765991
3507.592075	736220.061528	41.770996
3507.886199	736078.374744	41.776000
3507.770656	735957.638170	41.781005
3507.228915	735827.071957	41.786010
3507.540777	735712.051531	41.791015
3507.351254	735594.687170	41.796020
3507.439724	735466.188611	41.801024
3507.484951	735336.606265	41.806029
3507.229415	735218.702875	41.811034
3507.253751	735096.940326	41.816039
3507.358372	734978.577925	41.821044
3507.368533	734854.784690	41.826048
3506.648539	734741.603793	41.831053
3507.056167	734625.463024	41.836058
3506.651506	734505.296863	41.841063
3506.887963	734384.379453	41.846068
3506.658450	734280.268529	41.851072
3506.912269	734168.304649	41.856077
3506.772262	734066.354232	41.861082
3506.428072	733963.941238	41.866087
3506.632467	733847.525815	41.871092
3506.546240	733747.344595	41.876096
3506.682443	733626.184848	41.881101
3506.489539	733525.374935	41.886106
3506.536401	733417.147727	41.891111
3506.571029	733317.337240	41.896116
3506.161561	733217.846444	41.901120
3506.169378	733115.562522	41.906125
3505.902333	733004.658715	41.911130
3506.295190	732897.506056	41.916135
3505.952768	732807.108823	41.921140
3505.649618	732711.406470	41.926144
3506.100282	732595.674941	41.931149
3505.920163	732513.367424	41.936154
3505.784582	732409.612906	41.941159
3505.621744	732326.260869	41.946164
3505.795657	732231.216679	41.951168
3505.725587	732132.349601	41.956173
3505.476501	732047.127406	41.961178
3505.795269	731954.284178	41.966183
3505.310611	731867.514537	41.971188
3505.484388	731775.287405	41.976192
3505.726476	731679.136109	41.981197
3505.051454	731604.922845	41.986202
3505.088822	731512.715265	41.991207
3505.261747	731428.308131	41.996212
3505.325903	731344.809432	42.001216
3505.248790	731271.633234	42.006221
3505.040414	731187.088525	42.011226
3505.268423	731095.290369	42.016231
3505.377563	731019.704140	42.021236
3505.302398	730936.719470	42.026240
3505.456576	730846.762992	42.031245
3505.029271	730769.084118	42.036250
3505.144814	730683.143519	42.041255
3504.866249	730597.861422	42.046260
3504.941945	730521.037990	42.051264
3505.158846	730444.438118	42.056269
3504.744421	730368.139956	42.061274
3505.070167	730284.636641	42.066279
3504.852293	730213.504698	42.071284
3504.737620	730138.145351	42.076288
3504.882776	730068.388403	42.081293
3504.589589	729998.406133	42.086298
3504.865930	729914.015691	42.091303
3504.825093	729835.174404	42.096308
3504.395097	729754.068824	42.101312
3504.788683	729685.307634	42.106317
3504.657252	729616.731686	42.111322
3504.539657	729542.209297	42.116327
3504.847402	729460.186391	42.121332
3504.618184	729405.592361	42.126336
3504.707690	729322.861178	42.131341
3504.645123	729254.419390	42.136346
3504.516745	729176.973076	42.141351
3504.363752	729112.012277	42.146356
3504.631885	729053.767360	42.151360
3504.495264	728973.794304	42.156365
3504.369015	728905.855444	42.161370
3504.322456	728836.664495	42.166375
3504.655337	728772.710446	42.171380
3504.348514	728700.539749	42.176384
3504.603440	728640.758482	42.181389
3504.129072	728569.753626	42.186394
3504.247961	728496.371445	42.191399
3503.962178	728440.640963	42.196404
3503.639129	728384.569500	42.201408
3504.086430	728316.035572	42.206413
3504.453916	728258.412543	42.211418
3504.050883	728184.123056	42.216423
3504.442734	728126.148302	42.221428
3504.238941	728055.886871	42.226432
3504.294398	727990.139604	42.231437
3504.161856	727920.311084	42.236442
3503.891980	727868.884017	42.241447
3504.008176	727808.723268	42.246452
3503.832556	727757.478084	42.251456
3503.862042	727681.130914	42.256461
3503.628491	727646.490866	42.261466
3503.436141	727570.971989	42.266471
3503.478193	727519.986594	42.271476
3503.623792	727462.939593	42.276480
3503.940633	727411.858570	42.281485
3503.763475	727366.209516	42.286490
3503.905963	727300.491862	42.291495
3503.804617	727239.223377	42.296500
3503.484122	727189.732608	42.301504
3503.641365	727133.325459	42.306509
3503.357572	727087.642928	42.311514
3503.549177	727038.264792	42.316519
3503.941450	726991.726824	42.321524
3503.666203	726941.582987	42.326528
3503.637104	726878.912588	42.331533
3503.390176	726825.691509	42.336538
3503.491465	726775.385336	42.341543
3503.565450	726713.885756	42.346548
3503.242794	726678.116750	42.351552
3503.516763	726617.227510	42.356557
3503.249605	726577.683278	42.361562
3503.541140	726523.479389	42.366567
3503.299981	726475.556729	42.371572
3503.127497	726418.257729	42.376576
3502.781327	726372.086025	42.381581
3503.106238	726335.217523	42.386586
3503.262175	726287.971381	42.391591
3503.270411	726243.821466	42.396596
3503.111278	726207.428782	42.401600
3502.872353	726149.593834	42.406605
3502.959520	726121.335873	42.411610
3503.424336	726069.676980	42.416615
3503.308395	726026.933844	42.421620
3502.799806	725983.958065	42.426624
3502.978121	725938.390960	42.431629
3502.828038	725903.630637	42.436634
3502.649798	725852.770378	42.441639
3502.890490	725816.508093	42.446644
3502.565147	725776.325428	42.451648
3502.760090	725734.619550	42.456653
3502.497023	725701.611393	42.461658
3502.547896	725663.050805	42.466663
3502.685393	725627.746255	42.471668
3502.731313	725591.465611	42.476672
3502.733021	725558.512230	42.481677
3502.696276	725518.528379	42.486682
3502.734214	725484.874956	42.491687
3502.866619	725449.124491	42.496692
3502.825407	725419.497804	42.501696
3502.818158	725385.752333	42.506701
3502.701863	725345.830343	42.511706
3502.556430	725307.944749	42.516711
3502.654364	725265.657859	42.521716
3502.584760	725241.833240	42.526720
3502.800711	725200.616742	42.531725
3502.675124	725166.939486	42.536730
3502.439625	725131.991787	42.541735
3502.514756	725095.852799	42.546740
3502.295242	725061.496839	42.551744
3502.506208	725022.609449	42.556749
3502.114468	724995.863922	42.561754
3502.354924	724972.036838	42.566759
3502.521139	724939.252019	42.571764
3502.228632	724926.366006	42.576768
3502.788500	724876.616668	42.581773
3502.681217	724843.281968	42.586778
3502.546280	724814.957107	42.591783
3502.365671	724782.377654	42.596788
3502.283103	724750.773047	42.601792
3502.488925	724711.191213	42.606797
3502.435473	724686.073780	42.611802
3502.556021	724655.228186	42.616807
3502.785324	724616.633206	42.621812
3502.438880	724592.753339	42.626816
3502.679155	724563.324848	42.631821
3502.699265	724537.748766	42.636826
3502.737286	724492.543760	42.641831
3502.336602	724455.192025	42.646836
3502.227255	724433.800103	42.651840
3502.590531	724393.645556	42.656845
3502.547297	724374.918847	42.661850
3501.975597	724333.877740	42.666855
3502.213421	724306.530314	42.671860
3502.261244	724271.284328	42.676864
3502.388623	724240.535177	42.681869
3502.377377	724219.374296	42.686874
3502.410202	724188.244080	42.691879
3502.569403	724147.477753	42.696884
3502.405609	724126.639218	42.701888
3502.615463	724100.534796	42.706893
3502.394529	724066.373167	42.711898
3502.274771	724022.232478	42.716903
3502.390935	723999.662207	42.721908
3502.111863	723976.215485	42.726912
3502.302960	723943.273903	42.731917
3502.254104	723914.783028	42.736922
3502.338211	723882.998855	42.741927
3502.443246	723861.619583	42.746932
3502.202779	723839.752146	42.751936
3502.375444	723799.477518	42.756941
3502.236896	723788.051211	42.761946
3502.408262	723758.234722	42.766951
3502.319371	723725.437672	42.771956
3502.415900	723701.928097	42.776960
3502.114816	723674.618074	42.781965
3502.127750	723639.672547	42.786970
3502.249513	723620.371637	42.791975
3502.372966	723591.652907	42.796980
3502.264793	723567.829820	42.801985
3502.286991	723530.602268	42.806989
3502.273608	723511.373003	42.811994
3501.977879	723474.643836	42.816999
3502.413166	723455.637693	42.822004
3502.130665	723424.655841	42.827009
3502.389237	723396.558472	42.832013
3502.073482	723382.335572	42.837018
3501.932151	723344.440267	42.842023
3502.189444	723319.911692	42.847028
3502.315264	723303.930388	42.852033
3502.358299	723266.797339	42.857037
3501.766620	723243.301058	42.862042
3501.912019	723216.262705	42.867047
3502.227444	723195.392188	42.872052
3501.493060	723175.587340	42.877057
3501.614363	723168.082693	42.882061
3501.907995	723143.993706	42.887066
3502.090439	723116.651495	42.892071
3502.213540	723093.036660	42.897076
3501.952840	723069.832167	42.902081
3501.987742	723054.162820	42.907085
3502.209394	723021.609068	42.912090
3502.131969	723008.981919	42.917095
3502.134815	722989.649620	42.922100
3501.940870	722972.382147	42.927105
3501.936071	722928.067900	42.932109
3502.139548	722919.458912	42.937114
3502.248144	722888.112994	42.942119
3502.432347	722864.636120	42.947124
3501.558649	722834.245455	42.952129
3501.863843	722816.796027	42.957133
3501.866052	722794.836144	42.962138
3501.518237	722776.304855	42.967143
3502.148328	722751.712988	42.972148
3502.073565	722732.442484	42.977153
3501.910469	722709.567845	42.982157
3502.163606	722683.501369	42.987162
3502.052422	722665.872579	42.992167
3502.117572	722636.367027	42.997172
3501.697662	722634.354631	43.002177
3501.984014	722605.952559	43.007181
3502.255443	722582.857045	43.012186
3501.905128	722555.055733	43.017191
3502.012215	722529.260768	43.022196
3501.746225	722520.927241	43.027201
3502.284124	722493.028506	43.032205
3502.053489	722474.873753	43.037210
3501.746115	722442.405152	43.042215
3501.808624	722429.307838	43.047220
3501.413811	722408.205705	43.052225
3501.944949	722390.222312	43.057229
3501.857429	722369.713747	43.062234
3502.066310	722349.651879	43.067239
3502.178294	722324.599066	43.072244
3502.101751	722308.351844	43.077249
3502.143282	722279.047216	43.082253
3502.228146	722259.501362	43.087258
3502.062425	722228.198280	43.092263
3501.997513	722207.388132	43.097268
3502.067964	722196.619119	43.102273
3501.786508	722165.037480	43.107277
3501.760020	722142.485717	43.112282
3501.773037	722129.941428	43.117287
3501.639232	722097.294064	43.122292
3501.791802	722092.361163	43.127297
3502.039657	722074.622203	43.132301
3502.018029	722056.134541	43.137306
3501.529150	722041.095161	43.142311
3501.843617	722014.818148	43.147316
3501.632426	721990.710088	43.152321
3501.809408	721979.477010	43.157325
3501.971449	721959.868120	43.162330
3501.774866	721940.070571	43.167335
3502.006040	721929.324226	43.172340
3501.835365	721901.937213	43.177345
3501.857437	721882.202543	43.182349
3501.813787	721856.926157	43.187354
3501.655691	721836.923697	43.192359
3501.896917	721828.902257	43.197364
3501.675137	721803.208958	43.202369
3501.869598	721788.998143	43.207373
3501.887537	721764.752406	43.212378
3501.840710	721745.921179	43.217383
3502.073030	721733.439202	43.222388
3501.994522	721708.416009	43.227393
3502.329655	721679.556512	43.232397
3501.957183	721657.903421	43.237402
3501.849772	721643.048161	43.242407
3501.967479	721612.588308	43.247412
3501.719698	721603.110557	43.252417
3501.818942	721578.751685	43.257421
3501.730291	721551.796159	43.262426
3501.442089	721539.251178	43.267431
3502.047245	721520.113379	43.272436
3501.881029	721511.762343	43.277441
3501.797951	721491.052555	43.282445
3502.073049	721474.150644	43.287450
3501.493394	721458.232791	43.292455
3501.910962	721427.871440	43.297460
3501.854718	721414.494677	43.302465
3501.615180	721399.710395	43.307469
3502.011090	721381.598436	43.312474
3501.918205	721351.916114	43.317479
3502.088664	721341.426940	43.322484
3501.835565	721316.828053	43.327489
3501.993754	721302.077027	43.332493
3502.037881	721267.860026	43.337498
3501.684843	721264.100945	43.342503
3502.047268	721232.409341	43.347508
3501.784863	721226.156269	43.352513
3501.853860	721202.247511	43.357517
3502.090643	721178.757177	43.362522
3501.856463	721162.385019	43.367527
3502.192223	721133.226040	43.372532
3502.012595	721120.712063	43.377537
3501.831303	721086.234083	43.382541
3501.872595	721065.453099	43.387546
3501.805525	721051.829635	43.392551
3501.867319	721024.797954	43.397556
3501.585142	721009.325886	43.402561
3502.107375	720994.712478	43.407565
3501.941299	720971.783950	43.412570
3501.684864	720952.241840	43.417575
3502.052631	720920.944820	43.422580
3501.932878	720906.834008	43.427585
3501.693294	720880.694555	43.432589
3501.939855	720868.506421	43.437594
3501.578601	720853.691697	43.442599
3501.468046	720833.480631	43.447604
3501.365336	720815.747339	43.452609
3501.520186	720806.053388	43.457613
3501.301614	720810.105901	43.462618
3501.363970	720782.875010	43.467623
3501.806211	720755.283754	43.472628
3501.529917	720749.181363	43.477633
3501.815800	720737.482366	43.482637
3501.979757	720713.011096	43.487642
3501.668154	720708.501168	43.492647
3501.879262	720685.063267	43.497652
3501.796606	720666.979261	43.502657
3501.703533	720649.987772	43.507661
3502.005168	720625.195991	43.512666
3501.662562	720627.831167	43.517671
3501.949788	720596.794157	43.522676
3501.575513	720586.691558	43.527681
3501.543066	720572.516165	43.532685
3501.717673	720556.719844	43.537690
3501.534112	720537.759722	43.542695
3501.823855	720525.762286	43.547700
3501.618083	720516.623437	43.552705
3501.563189	720484.551696	43.557709
3501.886518	720482.713438	43.562714
3501.668232	720467.725644	43.567719
3501.809710	720441.075573	43.572724
3501.723474	720432.660646	43.577729
3501.789876	720415.295230	43.582733
3501.867070	720378.639450	43.587738
3501.766858	720379.647924	43.592743
3501.845935	720353.850831	43.597748
3501.432709	720344.002298	43.602753
3500.805140	720330.172769	43.607757
3501.618638	720322.799087	43.612762
3501.310290	720309.115109	43.617767
3501.581717	720275.897756	43.622772
3501.390183	720289.912754	43.627777
3501.368377	720273.652501	43.632781
3501.606405	720252.192358	43.637786
3501.611849	720239.696052	43.642791
3501.463075	720227.770658	43.647796
3501.351971	720228.632193	43.652801
3501.642938	720202.700442	43.657805
3501.892851	720189.023180	43.662810
3501.529370	720183.133124	43.667815
3501.878361	720158.084197	43.672820
3501.842759	720145.098669	43.677825
3501.737966	720120.075034	43.682829
3501.866622	720096.202825	43.687834
3501.462120	720086.848411	43.692839
3501.692009	720071.190795	43.697844
3501.428083	720041.779993	43.702849
3501.193115	720033.785938	43.707853
3501.726358	720029.582300	43.712858
3501.390471	720024.976836	43.717863
3501.823695	719993.417580	43.722868
3501.901919	719986.214705	43.727873
3501.691639	719975.092510	43.732877
3501.840134	719946.952077	43.737882
3501.680796	719946.135634	43.742887
3501.960288	719917.675927	43.747892
3501.496639	719900.000331	43.752897
3501.784527	719896.035526	43.757901
3502.325918	719873.284578	43.762906
3501.648170	719861.049373	43.767911
3502.061619	719831.377120	43.772916
3501.699633	719814.081247	43.777921
3501.838167	719799.727516	43.782925
3502.049017	719763.294883	43.787930
3501.775054	719750.397720	43.792935
3502.088206	719723.171506	43.797940
3501.584258	719707.138592	43.802945
3501.602891	719703.714085	43.807949
3501.689940	719671.714932	43.812954
3501.313853	719668.603588	43.817959
3501.786552	719663.417990	43.822964
3501.651270	719643.456065	43.827969
3501.369299	719616.575800	43.832973
3501.766046	719601.435213	43.837978
3501.451247	719599.156738	43.842983
3501.584476	719574.885563	43.847988
3501.423224	719567.176414	43.852993
3501.474415	719556.208807	43.857997
3501.391357	719545.263372	43.863002
3501.258274	719530.458167	43.868007
3501.312910	719501.538301	43.873012
3501.229149	719505.370803	43.878017
3501.020158	719505.355964	43.883021
3501.213468	719500.067667	43.888026
3501.375721	719507.231647	43.893031
3501.401430	719474.150890	43.898036
3501.569960	719464.949025	43.903041
3501.469893	719453.659147	43.908045
3501.538988	719439.068320	43.913050
3501.359554	719429.527196	43.918055
3501.420813	719407.548598	43.923060
3501.440733	719403.479074	43.928065
3501.434784	719398.124462	43.933069
3501.408990	719370.605977	43.938074
3501.310701	719361.844822	43.943079
3501.573295	719352.131378	43.948084
3501.373005	719346.114573	43.953089
3501.033099	719336.500680	43.958093
3501.314691	719305.509388	43.963098
3501.318336	719307.492654	43.968103
3501.325769	719292.961353	43.973108
3501.320013	719304.616503	43.978113
3501.315325	719295.393487	43.983117
3501.591729	719274.222037	43.988122
3501.382589	719250.601599	43.993127
3501.419090	719260.910850	43.998132
3501.775999	719252.917412	44.003137
3501.656307	719231.860906	44.008141
3501.642617	719208.852742	44.013146
3501.406431	719215.438125	44.018151
3501.436507	719187.165923	44.023156
3501.295685	719162.542103	44.028161
3501.003287	719166.805977	44.033165
3501.561781	719153.720723	44.038170
3501.284406	719162.643791	44.043175
3501.352656	719146.068901	44.048180
3501.306450	719125.644683	44.053185
3501.211065	719115.097460	44.058189
3501.488120	719102.405784	44.063194
3501.020922	719111.657832	44.068199
3501.064922	719108.972776	44.073204
3501.169523	719104.244409	44.078209
3501.385491	719080.949976	44.083213
3501.274069	719069.562269	44.088218
3501.008369	719071.242954	44.093223
3501.545579	719071.799094	44.098228
3501.089376	719069.940581	44.103233
3501.227100	719055.833670	44.108237
3501.464755	719027.427437	44.113242
3501.177229	719023.656502	44.118247
3501.440657	719022.472540	44.123252
3501.286083	719016.398349	44.128257
3501.073271	719005.523241	44.133261
3501.602340	718982.176790	44.138266
3501.320266	718986.141490	44.143271
3501.334317	718973.989017	44.148276
3501.345410	718972.846749	44.153281
3501.060419	718957.073762	44.158285
3501.526345	718933.092894	44.163290
3500.943517	718919.055238	44.168295
3501.445073	718915.848161	44.173300
3501.592181	718923.759052	44.178305
3501.318032	718918.002111	44.183309
3501.309507	718884.230362	44.188314
3501.122859	718882.029695	44.193319
3501.466838	718870.120110	44.198324
3501.372065	718879.211679	44.203329
3501.111243	718877.420020	44.208333
3501.177713	718848.198372	44.213338
3501.190804	718836.194639	44.218343
3501.241574	718830.433536	44.223348
3500.967131	718825.122927	44.228353
3501.112441	718838.043214	44.233357
3501.345344	718827.937315	44.238362
3501.086471	718839.188598	44.243367
3501.020172	718808.401738	44.248372
3501.024382	718792.878212	44.253377
3500.965065	718784.159603	44.258381
3500.991112	718771.459314	44.263386
3500.978049	718779.496001	44.268391
3500.963157	718773.001792	44.273396
3501.269346	718769.380595	44.278401
3500.999650	718778.749153	44.283405
3501.101273	718770.698256	44.288410
3501.211457	718765.671208	44.293415
3501.148363	718773.121034	44.298420
3501.122763	718746.939514	44.303425
3500.986682	718734.067582	44.308429
3501.146267	718723.725701	44.313434
3501.082020	718722.149497	44.318439
3501.228646	718721.976694	44.323444
3501.221666	718720.143051	44.328449
3501.255350	718724.601234	44.333453
3501.395144	718710.295019	44.338458
3501.256133	718692.067253	44.343463
3501.060986	718684.462078	44.348468
3501.072522	718676.773145	44.353473
3500.743350	718679.952249	44.358477
3500.641440	718674.067485	44.363482
3500.799194	718684.456600	44.368487
3500.837388	718671.307796	44.373492
3501.144249	718674.828147	44.378497
3500.966466	718674.213004	44.383501
3500.838782	718668.530876	44.388506
3501.078819	718675.037980	44.393511
3501.309487	718669.296631	44.398516
3501.163474	718652.210624	44.403521
3501.012339	718633.092019	44.408525
3500.951249	718618.570868	44.413530
3501.155899	718633.316697	44.418535
3501.057224	718621.876677	44.423540
3501.398027	718614.778011	44.428545
3501.440570	718620.177101	44.433549
3501.270588	718616.882509	44.438554
3501.391060	718591.370698	44.443559
3501.341047	718583.245489	44.448564
3501.103998	718575.795927	44.453569
3501.068985	718577.587372	44.458573
3501.410904	718567.165569	44.463578
3501.249095	718554.099229	44.468583
3501.375189	718536.720038	44.473588
3501.414927	718525.802567	44.478593
3501.228917	718524.593620	44.483597
3501.704164	718517.175078	44.488602
3501.220779	718507.534341	44.493607
3501.085590	718488.412769	44.498612
3501.261533	718485.606515	44.503617
3501.063799	718493.673996	44.508621
3501.201173	718481.401234	44.513626
3501.186074	718477.833010	44.518631
3501.026612	718481.777683	44.523636
3501.159482	718454.130764	44.528641
3500.952926	718443.898643	44.533645
3501.148214	718431.368254	44.538650
3501.265844	718436.606263	44.543655
3501.127512	718422.246326	44.548660
3501.388885	718423.195277	44.553665
3501.185024	718435.975504	44.558669
3501.090224	718412.135409	44.563674
3500.804366	718403.553034	44.568679
3500.771368	718396.416767	44.573684
3501.341581	718387.444916	44.578689
3501.050232	718382.285608	44.583693
3501.070799	718378.215478	44.588698
3501.017372	718387.995104	44.593703
3501.071350	718381.290821	44.598708
3500.929886	718376.900289	44.603713
3501.100236	718387.138903	44.608717
3501.388631	718386.645084	44.613722
3501.133979	718371.262748	44.618727
3501.199614	718353.099617	44.623732
3501.174553	718343.730125	44.628737
3501.236659	718345.604764	44.633741
3501.065869	718334.721836	44.638746
3501.000886	718350.256683	44.643751
3500.942458	718340.843105	44.648756
3501.458231	718343.188339	44.653761
3501.487809	718328.403715	44.658765
3501.500721	718314.712959	44.663770
3501.295805	718314.399856	44.668775
3501.398185	718295.734554	44.673780
3501.443747	718281.542374	44.678785
3501.182897	718266.408857	44.683789
3501.325712	718246.546422	44.688794
3501.124753	718257.540925	44.693799
3501.036478	718254.827858	44.698804
3501.120431	718250.697593	44.703809
3501.263495	718240.903420	44.708813
3501.167148	718224.304307	44.713818
3501.411191	718210.376792	44.718823
3501.412308	718205.417030	44.723828
3501.230886	718205.744813	44.728833
3501.236075	718216.159725	44.733837
3501.280888	718175.680585	44.738842
3501.267214	718174.195115	44.743847
3501.417128	718160.878250	44.748852
3501.458228	718166.178675	44.753857
3500.801158	718159.839715	44.758861
3501.163605	718154.225031	44.763866
3500.926707	718142.955992	44.768871
3501.028999	718125.728676	44.773876
3501.210634	718119.846259	44.778881
3501.170721	718120.249856	44.783885
3501.510835	718104.074358	44.788890
3501.256100	718116.565889	44.793895
3501.087809	718113.320416	44.798900
3501.581518	718093.598023	44.803905
3500.992041	718078.865665	44.808909
3501.308779	718062.197963	44.813914
3501.180211	718061.773035	44.818919
3501.339416	718063.433295	44.823924
3501.144679	718053.248340	44.828929
3501.175581	718032.213520	44.833933
3501.306082	718022.520367	44.838938
3501.178351	718028.989557	44.843943
3501.323982	718018.897107	44.848948
3501.179819	718022.839467	44.853953
3501.055897	718017.007475	44.858957
3501.434301	718004.842979	44.863962
3501.251112	717989.894523	44.868967
3501.110598	717980.146910	44.873972
3501.409101	717969.235549	44.878977
3501.166749	717983.858001	44.883981
3501.306810	717977.635161	44.888986
3501.174645	717951.319963	44.893991
3501.070567	717927.827216	44.898996
3501.208306	717923.489503	44.904001
3501.273309	717926.851745	44.909005
3501.412565	717921.521789	44.914010
3501.327019	717926.099302	44.919015
3501.335430	717903.232690	44.924020
3501.512651	717882.818110	44.929025
3501.221122	717883.808898	44.934029
3501.306334	717865.691074	44.939034
3501.249272	717880.977482	44.944039
3501.219562	717854.496248	44.949044
3501.149661	717848.754412	44.954049
3501.214722	717827.217431	44.959053
3501.228577	717833.316172	44.964058
3501.313530	717835.831952	44.969063
3501.276744	717825.620616	44.974068
3501.130366	717816.270582	44.979073
3501.324754	717807.062624	44.984077
3501.392955	717782.400191	44.989082
3501.212078	717788.431946	44.994087
3500.905722	717784.465155	44.999092
3501.576362	717786.884158	45.004097
3501.115685	717772.873979	45.009101
3501.276179	717752.015440	45.014106
3501.426896	717745.641866	45.019111
3501.315352	717741.295655	45.024116
3501.337545	717741.292201	45.029121
3500.979303	717744.774063	45.034125
3501.209377	717731.443270	45.039130
3501.077526	717708.896912	45.044135
3501.274737	717702.267616	45.049140
3501.685277	717695.603061	45.054145
3501.228324	717694.885176	45.059149
3501.281030	717684.559676	45.064154
3501.396568	717669.462076	45.069159
3501.345309	717660.939368	45.074164
3501.414339	717654.281617	45.079169
3501.467168	717654.868314	45.084173
3501.419931	717635.680655	45.089178
3501.451093	717615.884779	45.094183
3501.439503	717617.771761	45.099188
3501.488514	717599.659344	45.104193
3501.733502	717597.684611	45.109197
3501.736672	717580.472556	45.114202
3501.398825	717578.842147	45.119207
3501.152840	717563.060077	45.124212
3501.366999	717547.400340	45.129217
3501.102494	717528.992370	45.134221
3501.387299	717527.407856	45.139226
3501.401134	717527.008967	45.144231
3501.264667	717529.412626	45.149236
3501.572030	717511.604537	45.154241
3501.308875	717494.089103	45.159245
3501.362932	717476.818823	45.164250
3501.182794	717485.975612	45.169255
3501.320539	717478.363924	45.174260
3501.598309	717453.814698	45.179265
3501.313615	717441.510961	45.184269
3501.220817	717430.961183	45.189274
3500.958233	717440.330057	45.194279
3501.121008	717424.827391	45.199284
3501.523591	717424.017034	45.204289
3501.190112	717405.322575	45.209293
3501.505394	717384.983173	45.214298
3501.328537	717396.024423	45.219303
3501.383495	717389.467993	45.224308
3501.548195	717382.149380	45.229313
3501.113283	717362.727547	45.234317
3501.558062	717351.195975	45.239322
3501.449293	717339.706265	45.244327
3501.095282	717357.671663	45.249332
3501.673618	717330.840273	45.254337
3501.253669	717312.903944	45.259341
3501.309194	717296.674717	45.264346
3501.596555	717297.421093	45.269351
3501.329445	717278.715383	45.274356
3501.533279	717257.154004	45.279361
3501.216979	717253.238206	45.284365
3501.652065	717246.271619	45.289370
3501.353724	717241.261568	45.294375
3501.310132	717221.774737	45.299380
3501.399658	717202.017842	45.304385
3501.332102	717203.170108	45.309389
3501.459639	717203.843698	45.314394
3501.742817	717195.910097	45.319399
3501.433980	717178.401552	45.324404
3501.723162	717158.760372	45.329409
3501.332877	717152.029317	45.334413
3501.407855	717128.851967	45.339418
3501.340121	717120.480244	45.344423
3501.378100	717111.247768	45.349428
3501.412153	717106.331517	45.354433
3501.052733	717111.599592	45.359437
3501.292431	717085.319426	45.364442
3501.400513	717066.501632	45.369447
3501.074803	717059.214179	45.374452
3501.238374	717051.647442	45.379457
3501.198665	717064.799466	45.384461
3501.701757	717045.221879	45.389466
3501.525633	717030.667379	45.394471
3500.995252	717013.889570	45.399476
3501.196555	717011.177846	45.404481
3501.135736	717017.140707	45.409485
3501.422952	717014.513996	45.414490
3501.733375	716991.743802	45.419495
3501.233576	716973.026258	45.424500
3501.507282	716960.183083	45.429505
3501.255152	716958.935226	45.434509
3501.196874	716957.456911	45.439514
3501.519936	716935.775793	45.444519
3501.135636	716920.957873	45.449524
3501.268828	716917.959743	45.454529
3501.298697	716922.320306	45.459533
3501.220092	716910.180150	45.464538
3501.444499	716886.828620	45.469543
3500.983969	716876.190098	45.474548
3501.495480	716868.664907	45.479553
3501.622075	716873.703992	45.484557
3501.356876	716863.529231	45.489562
3501.428838	716846.552330	45.494567
3501.451987	716837.917276	45.499572
3501.545254	716839.588680	45.504577
3501.209754	716826.895586	45.509581
3501.073350	716816.798696	45.514586
3501.356162	716794.727017	45.519591
3501.258102	716791.171784	45.524596
3501.471840	716780.719347	45.529601
3501.235725	716777.732593	45.534605
3500.999037	716757.334074	45.539610
3500.961750	716746.575834	45.544615
3500.955688	716729.313951	45.549620
3501.156340	716725.957357	45.554625
3500.973276	716742.159584	45.559629
3501.214123	716732.744346	45.564634
3501.168325	716737.167117	45.569639
3501.150674	716729.630040	45.574644
3501.228471	716734.826093	45.579649
3501.010622	716737.789099	45.584653
3501.011627	716719.285862	45.589658
3501.136312	716701.754281	45.594663
3501.062631	716689.662599	45.599668
3501.222874	716690.727681	45.604673
3501.147873	716689.450511	45.609677
3501.120947	716696.945811	45.614682
3501.354408	716688.275846	45.619687
3501.061258	716697.600990	45.624692
3501.201906	716674.163498	45.629697
3500.900331	716660.670833	45.634701
3501.054660	716643.927946	45.639706
3501.025597	716645.520391	45.644711
3501.361377	716638.520109	45.649716
3501.333953	716639.913856	45.654721
3501.181343	716652.737933	45.659725
3500.965589	716646.324875	45.664730
3501.195428	716646.733569	45.669735
3501.309601	716618.686832	45.674740
3501.204151	716607.393998	45.679745
3501.317458	716601.224169	45.684749
3501.340573	716600.476451	45.689754
3501.047975	716594.274483	45.694759
3500.893255	716598.219254	45.699764
3501.302044	716584.410641	45.704769
3501.139683	716558.145664	45.709773
3501.222216	716558.777138	45.714778
3501.172423	716549.012865	45.719783
3500.988273	716545.967832	45.724788
3501.293948	716546.711252	45.729793
3500.816121	716557.059227	45.734797
3500.971295	716548.501271	45.739802
3501.068480	716542.929357	45.744807
3501.359333	716537.077394	45.749812
3501.392541	716509.936614	45.754817
3501.214864	716485.658260	45.759821
3501.352158	716420.946581	45.764826
3501.499675	716290.798376	45.769831
3501.206422	716125.299377	45.774836
3501.356387	715894.484895	45.779841
3500.898233	715600.805523	45.784845
3500.705455	715256.960704	45.789850
3500.168839	714842.552873	45.794855
3499.822031	714397.477580	45.799860
3499.825529	713875.404920	45.804865
3499.395056	713315.854011	45.809869
3499.114621	712693.508743	45.814874
3499.108034	712013.050166	45.819879
3498.395221	711269.215761	45.824884
3497.951855	710460.884521	45.829889
3497.452819	709613.511980	45.834893
3496.987771	708710.735861	45.839898
3497.129298	707739.284541	45.844903
3496.050423	706714.783465	45.849908
3495.690058	705615.882483	45.854913
3495.163770	704476.232472	45.859917
3494.065554	703261.403545	45.864922
3493.766235	702002.146015	45.869927
3492.688175	700673.255740	45.874932
3492.125464	699294.420436	45.879937
3491.519917	697858.749387	45.884941
3491.164578	696358.658842	45.889946
3490.172491	694791.229836	45.894951
3489.225776	693176.957914	45.899956
3488.399164	691495.308931	45.904961
3487.285581	689766.068638	45.909965
3486.396313	687966.928722	45.914970
3485.338727	686104.285928	45.919975
3484.303626	684199.780562	45.924980
3483.069211	682227.179252	45.929985
3482.069588	680216.455646	45.934989
3480.721145	678137.988292	45.939994
3479.557808	676013.125093	45.944999
3478.163246	673834.279210	45.950004
3477.572179	671579.057461	45.955009
3476.448866	669298.398346	45.960013
3474.816477	666939.605886	45.965018
3473.728727	664530.443479	45.970023
3472.199569	662071.838769	45.975028
3471.010757	659554.842707	45.980033
3469.702338	656992.323891	45.985037
3468.431200	654358.701785	45.990042
3466.807263	651693.509036	45.995047
3464.929852	648978.118312	46.000052
3463.545769	646193.125087	46.005057
3462.194256	643376.806561	46.010061
3460.490934	640489.943040	46.015066
3459.099072	637563.291534	46.020071
3457.213130	634592.754661	46.025076
3455.899728	631559.803852	46.030081
3454.043918	628482.153557	46.035085
3452.328142	625352.647631	46.040090
3450.682218	622178.425695	46.045095
3448.734862	618952.050892	46.050100
3447.235587	615656.667668	46.055105
3445.285797	612347.436503	46.060109
3443.152568	608985.132774	46.065114
3441.952100	605565.219396	46.070119
3439.789319	602096.903348	46.075124
3438.029648	598574.503740	46.080129
3435.363688	595020.047747	46.085133
3433.619258	591401.112707	46.090138
3431.539021	587739.822339	46.095143
3429.281099	584056.283851	46.100148
3427.379034	580309.318480	46.105153
3425.063837	576540.005653	46.110157
3422.914335	572717.802146	46.115162
3420.724394	568856.902754	46.120167
3418.591760	564947.504356	46.125172
3416.587049	560995.459863	46.130177
3414.263180	557003.037870	46.135181
3411.792619	552960.414285	46.140186
3409.943359	548876.407305	46.145191
3407.185622	544761.184389	46.150196
3405.069671	540591.782883	46.155201
3402.370196	536389.365012	46.160205
3399.965754	532147.770446	46.165210
3397.879222	527857.086845	46.170215
3395.073037	523539.833981	46.175220
3392.557897	519171.496588	46.180225
3390.232007	514777.484016	46.185229
3387.059493	510340.076993	46.190234
3384.951824	505869.208206	46.195239
3382.063789	501366.442549	46.200244
3379.553911	496820.103990	46.205249
3376.881213	492247.169680	46.210253
3374.087013	487635.591442	46.215258
3371.392466	482976.620490	46.220263
3368.421884	478304.536897	46.225268
3366.052889	473586.696051	46.230273
3363.022966	468840.118087	46.235277
3360.160602	464056.057526	46.240282
3357.776783	459237.555136	46.245287
3354.573841	454398.365209	46.250292
3351.710688	449513.006581	46.255297
3348.599025	444605.868986	46.260301
3345.470283	439666.579974	46.265306
3342.827072	434702.067935	46.270311
3339.794340	429701.986007	46.275316
3336.652725	424670.357638	46.280321
3333.388046	419629.665276	46.285325
3330.353790	414553.646910	46.290330
3327.265797	409445.967823	46.295335
3323.796127	404319.169717	46.300340
3320.771327	399154.033148	46.305345
3317.367011	393993.093673	46.310349
3314.083858	388799.122338	46.315354
3311.266605	383584.713780	46.320359
3307.774213	378339.658322	46.325364
3304.559277	373077.067433	46.330369
3301.307627	367793.893270	46.335373
3297.921097	362487.737933	46.340378
3294.910649	357165.539776	46.345383
3291.243515	351820.122574	46.350388
3287.742457	346453.745506	46.355393
3284.453819	341076.126871	46.360397
3280.688523	335666.953579	46.365402
3277.352665	330235.751124	46.370407
3273.657485	324814.933786	46.375412
3270.573921	319351.967565	46.380417
3266.697285	313891.157665	46.385421
3262.883481	308423.008046	46.390426
3259.264784	302928.133232	46.395431
3255.130995	297451.222010	46.400436
3251.951510	291942.723853	46.405441
3248.097860	286424.615826	46.410445
3244.451762	280905.985502	46.415450
3240.716767	275370.751179	46.420455
3236.929869	269845.560810	46.425460
3232.982082	264298.613555	46.430465
3229.229660	258757.855618	46.435469
3224.945120	253199.101383	46.440474
3221.386750	247636.497879	46.445479
3217.369529	242080.979607	46.450484
3213.576433	236516.354675	46.455489
3209.440088	230958.344900	46.460493
3205.402517	225401.825531	46.465498
3201.427931	219839.663534	46.470503
3197.549042	214280.044337	46.475508
3193.418482	208692.667139	46.480513
3189.438047	203083.458186	46.485517
3185.555165	197514.639371	46.490522
3181.620827	191978.186295	46.495527
3176.885351	186428.480624	46.500532
3173.062487	180880.554371	46.505537
3168.768009	175343.953232	46.510541
3164.643547	169813.418642	46.515546
3160.063575	164301.941140	46.520551
3155.904310	158784.277990	46.525556
3151.553645	153296.219773	46.530561
3147.209509	147804.779535	46.535565
3142.470937	142329.275575	46.540570
3138.450147	136879.052527	46.545575
3134.029673	131443.940075	46.550580
3129.357121	126013.539369	46.555585
3124.846319	120606.710976	46.560589
3120.161397	115216.423963	46.565594
3115.710760	109839.122842	46.570599
3110.725643	104502.671336	46.575604
3106.186887	99168.710362	46.580609
3101.657212	93870.588747	46.585613
3096.561114	88605.574034	46.590618
3092.079734	83342.759939	46.595623
3087.078423	78132.557497	46.600628
3082.154028	72943.547148	46.605633
3077.190369	67771.502705	46.610637
3071.695883	62655.565114	46.615642
3066.963980	57564.158782	46.620647
3061.421600	52519.525280	46.625652
3056.171114	47509.198041	46.630657
3050.870495	42556.064387	46.635661
3044.681277	37633.759496	46.640666
3038.787033	32760.929957	46.645671
3032.499570	27973.741298	46.650676
3025.800469	23232.592086	46.655681
3018.537021	18594.316983	46.660685
3006.414851	14153.555160	46.665690
2986.341088	10068.606294	46.670695
2957.703684	6428.954059	46.675700
2922.660786	3330.115868	46.680705
2884.884396	800.038574	46.685709
2798.515354	261.627951	46.690714
2731.060841	254.836927	46.695719
2709.162908	250.274887	46.700724
2721.004540	234.169919	46.705729
2748.952041	232.474891	46.710733
2776.829676	229.025419	46.715738
2797.434596	232.521904	46.720743
2807.207023	235.341563	46.725748
2808.840647	233.517922	46.730753
2805.564772	226.591052	46.735757
2800.019025	228.370786	46.740762
2794.804664	217.641183	46.745767
2789.695404	226.840676	46.750772
2786.358035	219.321329	46.755777
2784.041233	221.467075	46.760781
2781.669321	207.215147	46.765786
2779.741609	209.326287	46.770791
2777.090849	218.877417	46.775796
2773.988146	204.775274	46.780801
2770.799531	221.147075	46.785805
2767.713479	216.687927	46.790810
2764.934681	213.814656	46.795815
2762.047412	217.671446	46.800820
2758.530145	225.850653	46.805825
2755.114049	215.641803	46.810829
2752.071426	218.761993	46.815834
2748.924096	218.877463	46.820839
2746.171112	213.316906	46.825844
2742.534477	207.341395	46.830849
2739.213910	204.973027	46.835853
2735.469309	214.207752	46.840858
2732.761645	209.858077	46.845863
2729.361917	212.042411	46.850868
2725.822257	205.918843	46.855873
2722.962898	202.850154	46.860877
2719.720826	197.299543	46.865882
2716.002787	208.144313	46.870887
2712.497834	209.006146	46.875892
2709.301138	203.495786	46.880897
2705.845698	197.881640	46.885901
2702.638322	196.883239	46.890906
2699.332734	199.387487	46.895911
2695.648731	200.779624	46.900916
2692.337871	199.211870	46.905921
2689.115292	202.701906	46.910925
2685.894954	208.715541	46.915930
2683.119826	195.683893	46.920935
2679.483649	203.894278	46.925940
2675.515467	204.556948	46.930945
2671.602742	197.608943	46.935949
2668.310906	200.766892	46.940954
2664.550424	193.287716	46.945959
2661.380587	202.293740	46.950964
2657.759032	193.922686	46.955969
2654.567538	199.758695	46.960973
2651.197114	202.217867	46.965978
2648.105958	189.784805	46.970983
2644.562255	201.159034	46.975988
2641.131475	186.147734	46.980993
2637.739062	194.480199	46.985997
2634.573822	190.227468	46.991002
2631.061414	188.448235	46.996007
2627.194039	188.502638	47.001012
2623.948404	196.663007	47.006017
2621.068503	192.592943	47.011021
2616.740713	197.419260	47.016026
2613.250232	186.581523	47.021031
2609.733641	191.900090	47.026036
2606.292373	196.248702	47.031041
2602.979621	181.185934	47.036045
2599.306465	193.771180	47.041050
2596.401730	183.971376	47.046055
2592.908831	197.627736	47.051060
2589.279073	186.730200	47.056065
2585.935225	181.066707	47.061069
2581.977000	188.405752	47.066074
2578.597084	181.351080	47.071079
2575.482373	180.474585	47.076084
2572.012928	181.379001	47.081089
2568.386145	186.272817	47.086093
2564.782487	174.059283	47.091098
2561.837172	182.065568	47.096103
2557.922300	182.574871	47.101108
2554.704299	177.721561	47.106113
2551.055764	176.132280	47.111117
2547.396262	187.618689	47.116122
2544.029017	176.965654	47.121127
2540.783560	176.236341	47.126132
2537.143737	179.028121	47.131137
2533.846382	177.637444	47.136141
2530.146493	176.936221	47.141146
2526.923076	178.657765	47.146151
2523.179017	173.231492	47.151156
2519.566868	187.018938	47.156161
2516.362608	178.699305	47.161165
2513.066256	176.337375	47.166170
2509.692312	169.392290	47.171175
2505.840207	173.314671	47.176180
2502.087049	173.804746	47.181185
2499.005218	177.832246	47.186189
2495.143964	186.145945	47.191194
2491.614600	180.687305	47.196199
2488.563626	167.298549	47.201204
2485.042498	170.525382	47.206209
2481.964690	176.492062	47.211213
2477.734318	173.138691	47.216218
2474.436813	169.901987	47.221223
2471.124752	169.127715	47.226228
2467.225326	162.120500	47.231233
2463.903486	168.257844	47.236237
2460.397663	174.097683	47.241242
2457.162859	168.961690	47.246247
2453.689111	167.044584	47.251252
2449.995761	178.253680	47.256257
2446.948063	162.138392	47.261261
2443.188324	169.194059	47.266266
2439.634830	171.163523	47.271271
2436.183275	171.334343	47.276276
2432.707524	165.913257	47.281281
2429.260494	159.500928	47.286285
2425.307005	172.569616	47.291290
2422.341243	166.834379	47.296295
2418.762594	172.457596	47.301300
2414.806702	168.854787	47.306305
2411.418828	166.092110	47.311309
2408.055197	171.784709	47.316314
2404.640846	161.556589	47.321319
2401.380363	159.866471	47.326324
2397.586427	163.200519	47.331329
2393.896967	164.920606	47.336333
2390.484963	163.669803	47.341338
2387.279394	162.608989	47.346343
2383.778160	169.405017	47.351348
2380.164456	164.009787	47.356353
2377.195989	155.845413	47.361357
2373.447178	166.909230	47.366362
2370.297755	165.401829	47.371367
2366.611594	157.834083	47.376372
2362.596374	166.466232	47.381377
2359.469159	155.786651	47.386381
2355.168210	163.261579	47.391386
2351.951198	157.953808	47.396391
2348.723105	161.181945	47.401396
2345.660764	157.773000	47.406401
2342.169911	158.028552	47.411405
2337.779179	166.905455	47.416410
2334.588256	155.701859	47.421415
2331.282774	159.295666	47.426420
2327.590438	161.519695	47.431425
2324.355565	149.923783	47.436429
2320.791803	161.550776	47.441434
2317.603156	148.309114	47.446439
2313.830798	157.929992	47.451444
2310.283436	167.993932	47.456449
2306.939328	153.243132	47.461453
2303.212117	158.626217	47.466458
2300.082497	154.471859	47.471463
2296.287972	164.878082	47.476468
2292.685578	166.587387	47.481473
2289.451356	148.043535	47.486477
2285.822536	169.200306	47.491482
2282.249878	158.360925	47.496487
2278.745115	165.949927	47.501492
2274.958414	164.104349	47.506497
2271.957467	155.825260	47.511501
2268.529762	164.297023	47.516506
2265.116912	168.396091	47.521511
2261.487103	153.336860	47.526516
2257.772616	160.754990	47.531521
2254.465876	162.808647	47.536525
2250.692196	158.725889	47.541530
2247.500363	162.845388	47.546535
2244.216606	162.586199	47.551540
2240.251458	162.214329	47.556545
2236.944696	147.746121	47.561549
2233.047887	164.096760	47.566554
2229.886260	164.845480	47.571559
2226.604719	160.243525	47.576564
2222.965167	164.158568	47.581569
2219.635200	162.870637	47.586573
2215.676822	169.775281	47.591578
2212.384999	161.922917	47.596583
2208.949307	158.553825	47.601588
2205.256933	166.803469	47.606593
2202.176157	152.392179	47.611597
2198.648803	158.355962	47.616602
2194.948343	162.748414	47.621607
2191.659093	156.730489	47.626612
2187.631789	161.659978	47.631617
2184.273881	153.852928	47.636621
2180.670757	152.909050	47.641626
2177.101679	152.197920	47.646631
2173.901928	151.909083	47.651636
2170.427435	153.343329	47.656641
2167.452098	146.656152	47.661645
2163.711423	145.650815	47.666650
2159.992716	158.570498	47.671655
2156.372680	150.936355	47.676660
2152.632506	148.538732	47.681665
2149.332289	145.274729	47.686669
2145.525535	152.251004	47.691674
2142.407110	147.719979	47.696679
2139.505711	157.621962	47.701684
2135.657152	156.859686	47.706689
2132.006189	152.221533	47.711693
2128.077803	149.001631	47.716698
2124.765776	152.571024	47.721703
2121.442844	141.187821	47.726708
2117.618900	156.724886	47.731713
2114.340908	142.595597	47.736717
2110.804330	156.811245	47.741722
2107.608945	156.084240	47.746727
2104.061606	147.879442	47.751732
2100.018558	152.098244	47.756737
2097.031467	142.706002	47.761741
2093.422185	144.565211	47.766746
2090.087903	142.057376	47.771751
2086.731057	151.441852	47.776756
2082.674949	146.480543	47.781761
2079.535348	148.077236	47.786765
2075.945524	153.298031	47.791770
2072.175237	143.868038	47.796775
2069.050436	142.260691	47.801780
2065.062099	152.906410	47.806785
2062.058527	147.157991	47.811789
2058.322580	152.087470	47.816794
2055.256822	132.648065	47.821799
2051.718389	142.895015	47.826804
2047.688920	138.693026	47.831809
2044.417071	138.791374	47.836813
2040.492563	142.732274	47.841818
2037.652905	136.803387	47.846823
2034.336015	142.675784	47.851828
2030.011308	145.979699	47.856833
2026.776322	144.163508	47.861837
2023.169584	140.487452	47.866842
2019.991639	135.946461	47.871847
2016.518544	131.674019	47.876852
2012.879027	143.368440	47.881857
2009.667651	124.776508	47.886861
2005.731765	148.165083	47.891866
2002.129145	143.173310	47.896871
1998.900754	143.436571	47.901876
1995.314253	140.943774	47.906881
1992.167237	132.253018	47.911885
1988.355642	146.303365	47.916890
1985.207271	133.543952	47.921895
1981.960863	138.070119	47.926900
1977.722380	136.615034	47.931905
1974.270768	139.465685	47.936909
1970.748263	139.516631	47.941914
1967.079220	140.289449	47.946919
1963.437074	141.915636	47.951924
1959.980260	143.199321	47.956929
1957.209084	140.929609	47.961933
1953.540322	140.655916	47.966938
1949.922980	131.270765	47.971943
1946.235925	136.735699	47.976948
1942.852286	140.194353	47.981953
1939.647853	131.561901	47.986957
1935.937927	154.042044	47.991962
1932.580627	140.853556	47.996967
1929.139645	139.559005	48.001972
1925.296555	142.586465	48.006977
1921.672718	140.170568	48.011981
1918.259270	130.885057	48.016986
1914.864330	135.621978	48.021991
1911.483492	134.640318	48.026996
1907.636245	134.653574	48.032001
1904.405009	140.464116	48.037005
1900.776882	131.608085	48.042010
1897.334830	135.734375	48.047015
1893.892839	128.065858	48.052020
1890.297026	133.695292	48.057025
1887.353124	120.868544	48.062029
1883.605053	139.712591	48.067034
1879.572204	137.983172	48.072039
1876.121287	122.841050	48.077044
1872.497959	134.968609	48.082049
1869.664155	130.063848	48.087053
1865.812832	141.549578	48.092058
1862.303589	138.395846	48.097063
1859.023258	130.668993	48.102068
1855.137246	135.880447	48.107073
1851.980243	128.127635	48.112077
1847.968566	130.056908	48.117082
1844.575545	125.994339	48.122087
1841.509856	128.095585	48.127092
1837.604240	135.695705	48.132097
1834.409300	130.377814	48.137101
1830.983890	143.699050	48.142106
1827.411327	127.058041	48.147111
1824.068653	126.572350	48.152116
1819.838863	141.685138	48.157121
1816.581315	133.795491	48.162125
1813.602878	134.869171	48.167130
1809.748629	120.830778	48.172135
1806.652330	126.868848	48.177140
1802.886109	139.335097	48.182145
1799.273056	124.101920	48.187149
1795.582204	127.281666	48.192154
1791.923128	125.900446	48.197159
1788.596848	124.584242	48.202164
1785.475967	134.016837	48.207169
1782.058742	125.275942	48.212173
1778.684183	127.754827	48.217178
1774.971477	133.551341	48.222183
1771.403664	130.689592	48.227188
1767.248281	129.775865	48.232193
1764.149678	124.278869	48.237197
1760.648771	129.863866	48.242202
1757.306270	128.373761	48.247207
1754.005906	119.139918	48.252212
1750.196298	128.656906	48.257217
1746.651689	125.818567	48.262221
1743.088173	134.063786	48.267226
1739.676487	134.388817	48.272231
1736.107200	128.050876	48.277236
1732.655036	137.391016	48.282241
1729.715744	126.619483	48.287245
1725.736923	128.412791	48.292250
1722.161692	127.904959	48.297255
1718.666658	121.899078	48.302260
1715.051737	130.580270	48.307265
1711.616862	124.389977	48.312269
1708.387555	127.877103	48.317274
1705.037639	120.301051	48.322279
1701.440698	120.154212	48.327284
1697.660888	130.863542	48.332289
1694.164615	109.947391	48.337293
1690.536075	122.781419	48.342298
1687.128716	123.323439	48.347303
1683.927998	121.993216	48.352308
1680.178905	126.528156	48.357313
1676.657990	123.501641	48.362317
1673.006340	131.416978	48.367322
1669.515079	126.730299	48.372327
1666.556248	116.068037	48.377332
1662.927254	124.877896	48.382337
1659.534496	120.006372	48.387341
1655.590568	125.760018	48.392346
1652.141295	124.401568	48.397351
1648.518954	116.713657	48.402356
1644.893627	120.632547	48.407361
1641.567224	127.439619	48.412365
1638.323036	116.192625	48.417370
1634.577459	125.128792	48.422375
1631.345428	120.804695	48.427380
1627.400569	126.396509	48.432385
1624.371844	115.817307	48.437389
1620.642298	124.116788	48.442394
1617.213712	132.726711	48.447399
1613.588756	115.789942	48.452404
1610.165073	129.889921	48.457409
1606.379104	124.970370	48.462413
1603.126644	126.043264	48.467418
1599.612992	122.940825	48.472423
1596.331109	119.407263	48.477428
1592.578399	123.294434	48.482433
1589.076312	112.570961	48.487437
1585.606616	127.467532	48.492442
1581.859744	124.376350	48.497447
1578.861812	118.870514	48.502452
1575.334097	123.442050	48.507457
1571.632981	111.429646	48.512461
1568.323919	122.886672	48.517466
1564.414627	120.303939	48.522471
1561.122906	115.075151	48.527476
1557.698916	121.689290	48.532481
1554.068648	117.148119	48.537485
1550.763608	124.084720	48.542490
1546.691142	117.489801	48.547495
1543.517945	119.794984	48.552500
1539.893094	123.028737	48.557505
1536.653064	125.852950	48.562509
1533.232890	122.148195	48.567514
1529.225511	127.479329	48.572519
1525.949749	116.806792	48.577524
1522.453418	126.191509	48.582529
1519.664092	124.322357	48.587533
1516.012075	126.257828	48.592538
1512.077109	125.817733	48.597543
1508.639268	115.225568	48.602548
1504.829040	117.332523	48.607553
1501.195416	115.780803	48.612557
1498.276704	119.397539	48.617562
1494.164160	121.427555	48.622567
1491.016976	108.714795	48.627572
1487.452648	123.828605	48.632577
1484.087276	128.441574	48.637581
1480.717700	121.194789	48.642586
1476.863904	120.770474	48.647591
1473.584221	117.846222	48.652596
1469.879231	124.652469	48.657601
1466.346397	120.063649	48.662605
1463.176294	135.606829	48.667610
1459.412423	119.712106	48.672615
1456.031945	117.521505	48.677620
1452.543843	120.069807	48.682625
1448.884274	125.357345	48.687629
1445.246316	123.623464	48.692634
1441.748076	126.225554	48.697639
1438.430990	120.055645	48.702644
1435.094600	116.088246	48.707649
1431.865579	118.892164	48.712653
1428.249071	125.607206	48.717658
1424.473935	126.198605	48.722663
1420.912971	122.179069	48.727668
1417.314737	122.878086	48.732673
1413.680490	118.341854	48.737677
1410.698458	118.948543	48.742682
1406.815298	121.362900	48.747687
1403.482766	109.540357	48.752692
1399.967737	115.943375	48.757697
1396.325065	121.482717	48.762701
1392.921441	113.485872	48.767706
1389.421175	117.477777	48.772711
1386.177329	104.777007	48.777716
1382.670084	121.071354	48.782721
1378.974641	112.259385	48.787725
1375.618433	114.391797	48.792730
1371.939792	118.905458	48.797735
1368.295284	104.902641	48.802740
1364.696417	114.275276	48.807745
1361.592386	114.685367	48.812749
1358.066944	109.770613	48.817754
1354.327117	111.260213	48.822759
1350.985616	104.283592	48.827764
1347.405296	109.745536	48.832769
1343.749907	110.653211	48.837773
1340.393552	108.451016	48.842778
1336.909021	111.725016	48.847783
1333.725428	101.814488	48.852788
1329.900662	114.536296	48.857793
1326.604281	113.047989	48.862797
1322.759797	117.564733	48.867802
1318.876710	116.713268	48.872807
1315.695965	113.517785	48.877812
1312.503146	117.433893	48.882817
1309.119433	111.862032	48.887821
1305.297018	117.791010	48.892826
1301.439064	109.048508	48.897831
1298.589624	111.799234	48.902836
1294.941217	120.052181	48.907841
1291.393741	118.162737	48.912845
1287.990944	113.303875	48.917850
1284.230034	108.077786	48.922855
1280.562271	104.099983	48.927860
1277.308816	108.548717	48.932865
1274.080652	114.917077	48.937869
1270.817970	108.663117	48.942874
1266.846366	113.859309	48.947879
1263.298689	102.821682	48.952884
1259.527520	105.720805	48.957889
1256.044921	110.222567	48.962893
1252.847649	110.109092	48.967898
1249.304840	113.034278	48.972903
1245.947835	110.964093	48.977908
1242.190158	107.893591	48.982913
1238.771782	110.685267	48.987917
1235.778458	110.207041	48.992922
1231.811034	115.478153	48.997927
1228.455644	110.655685	49.002932
1224.656294	122.619355	49.007937
1221.018666	116.824679	49.012941
1217.561045	103.922539	49.017946
1214.247221	121.706762	49.022951
1210.784294	103.208503	49.027956
1207.331280	116.041802	49.032961
1203.844242	105.324710	49.037965
1199.969098	111.555966	49.042970
1196.641080	107.589564	49.047975
1193.520763	103.155753	49.052980
1189.743212	106.056394	49.057985
1186.420787	110.311415	49.062989
1183.256846	105.818743	49.067994
1179.152483	106.996422	49.072999
1175.829129	106.121892	49.078004
1172.384873	110.166454	49.083009
1168.883033	103.055185	49.088013
1165.195162	102.341983	49.093018
1161.413714	104.660963	49.098023
1158.222472	102.084423	49.103028
1154.552288	111.815581	49.108033
1151.244032	102.752539	49.113037
1148.113134	97.065083	49.118042
1144.096476	105.357742	49.123047
1140.747079	102.725565	49.128052
1137.448186	115.080855	49.133057
1133.865776	111.458048	49.138061
1130.418456	111.889169	49.143066
1126.277156	121.677018	49.148071
1122.995357	105.565160	49.153076
1119.548803	121.153628	49.158081
1116.128400	105.660331	49.163085
1112.997162	91.299132	49.168090
1109.126145	108.180906	49.173095
1105.851415	94.781451	49.178100
1101.677370	108.670423	49.183105
1098.517548	101.913716	49.188109
1095.118117	106.624011	49.193114
1091.643687	110.128413	49.198119
1088.370493	101.804748	49.203124
1084.548467	109.409032	49.208129
1081.399419	107.688893	49.213133
1077.805918	113.825773	49.218138
1073.853323	112.090190	49.223143
1070.406247	102.586526	49.228148
1066.919817	109.334156	49.233153
1063.464633	105.328592	49.238157
1060.633902	95.062777	49.243162
1056.947822	115.537955	49.248167
1053.271098	108.852066	49.253172
1049.209876	107.958407	49.258177
1046.053584	108.524631	49.263181
1042.741964	101.041518	49.268186
1038.798668	112.196674	49.273191
1035.726664	105.140497	49.278196
1032.077999	105.383907	49.283201
1028.694960	111.374606	49.288205
1025.384851	99.283701	49.293210
1021.682077	105.184398	49.298215
1018.090425	111.720624	49.303220
1014.504436	107.216048	49.308225
1010.675720	109.534333	49.313229
1007.799219	106.189364	49.318234
1003.732551	111.113676	49.323239
1000.505264	97.963575	49.328244
997.196006	104.986936	49.333249
993.567499	106.421106	49.338253
990.371918	93.390670	49.343258
986.691740	102.957665	49.348263
983.418268	95.031777	49.353268
979.642714	114.376139	49.358273
976.000847	106.557174	49.363277
972.669831	102.100111	49.368282
968.703647	97.207972	49.373287
965.798521	103.735083	49.378292
961.935802	104.394940	49.383297
958.569501	99.830477	49.388301
955.079340	99.425459	49.393306
951.275381	106.344483	49.398311
947.944778	102.772811	49.403316
944.380264	104.755453	49.408321
941.233302	102.295083	49.413325
938.057019	108.850250	49.418330
934.115959	107.868294	49.423335
930.325517	110.730275	49.428340
926.861250	107.917653	49.433345
923.305978	104.974112	49.438349
920.224613	101.502389	49.443354
916.269032	102.891265	49.448359
913.135392	97.870668	49.453364
909.602519	105.413499	49.458369
906.287845	99.939882	49.463373
902.423038	101.567674	49.468378
898.581185	102.427386	49.473383
895.622726	98.697496	49.478388
892.070773	111.755639	49.483393
888.425052	104.976961	49.488397
884.936045	99.954399	49.493402
881.290157	105.696792	49.498407
877.929933	102.131878	49.503412
874.370432	105.170474	49.508417
870.852694	92.244148	49.513421
867.669517	99.607801	49.518426
863.852137	101.304719	49.523431
860.303582	93.808622	49.528436
856.483095	105.112864	49.533441
853.351012	107.055774	49.538445
850.183016	97.035563	49.543450
846.476881	99.154677	49.548455
843.326910	100.218877	49.553460
839.885328	105.125625	49.558465
835.939248	103.367307	49.563469
832.412534	106.656046	49.568474
828.539568	114.601727	49.573479
825.400399	99.145333	49.578484
822.220257	110.221159	49.583489
818.295654	109.107140	49.588493
815.068048	107.546885	49.593498
811.146510	108.613299	49.598503
807.871781	111.402612	49.603508
804.323859	100.174485	49.608513
800.362852	94.482075	49.613517
797.743525	103.263161	49.618522
793.409605	114.279543	49.623527
790.815728	97.013290	49.628532
787.403048	101.093389	49.633537
783.256371	99.035922	49.638541
780.220888	103.752954	49.643546
776.394123	103.459630	49.648551
773.034097	106.976098	49.653556
769.220178	100.292958	49.658561
765.602630	101.879836	49.663565
762.677672	109.361924	49.668570
758.701723	108.805475	49.673575
755.373489	100.126394	49.678580
751.763915	102.741253	49.683585
748.472664	110.428614	49.688589
744.977892	95.104160	49.693594
741.161923	101.922953	49.698599
737.805439	102.062090	49.703604
734.642287	103.118701	49.708609
730.747882	103.989081	49.713613
727.209343	92.310748	49.718618
723.923844	106.099116	49.723623
720.531017	89.938636	49.728628
717.182025	108.201235	49.733633
713.209011	109.741016	49.738637
709.690442	94.814036	49.743642
705.895649	106.485724	49.748647
702.675994	96.506789	49.753652
699.272773	109.874869	49.758657
695.495196	107.835542	49.763661
692.603306	100.993865	49.768666
688.555278	106.373805	49.773671
684.850007	102.910366	49.778676
681.950309	101.110484	49.783681
678.095390	100.390168	49.788685
674.891778	98.156500	49.793690
671.091612	92.656369	49.798695
667.695211	92.134026	49.803700
664.049236	102.616179	49.808705
660.453003	104.237702	49.813709
657.135993	97.275826	49.818714
653.665562	102.535421	49.823719
650.503563	94.698293	49.828724
646.974487	102.105146	49.833729
643.260807	97.492693	49.838733
640.206594	99.803500	49.843738
636.021680	98.131822	49.848743
632.760996	98.726968	49.853748
629.131744	93.958629	49.858753
625.583031	87.845119	49.863757
622.642840	90.056689	49.868762
618.423109	94.806117	49.873767
615.290978	91.425570	49.878772
611.762724	98.027985	49.883777
608.115162	100.987317	49.888781
604.981655	89.714864	49.893786
601.058340	103.515306	49.898791
597.743182	97.872154	49.903796
594.363629	94.993486	49.908801
590.509024	110.367711	49.913805
587.335142	95.031383	49.918810
583.621248	92.676125	49.923815
580.309167	95.380069	49.928820
576.559248	89.494198	49.933825
572.654963	103.001425	49.938829
569.660537	95.623757	49.943834
566.183408	108.390307	49.948839
562.701014	96.063264	49.953844
559.391395	99.807750	49.958849
555.367294	101.679016	49.963853
552.500034	94.075413	49.968858
548.874255	98.771661	49.973863
545.428804	95.420714	49.978868
541.673198	99.296707	49.983873
538.104028	103.016434	49.988877
534.553150	93.714667	49.993882
531.291094	97.677814	49.998887
527.540107	95.020738	50.003892
523.968583	103.549284	50.008897
520.789200	92.633610	50.013901
516.954704	108.052705	50.018906
513.461225	97.843361	50.023911
510.094424	97.205146	50.028916
506.578020	101.592595	50.033921
502.993023	95.462342	50.038925
499.589949	97.542504	50.043930
496.051458	95.345866	50.048935
492.466969	99.831068	50.053940
489.004858	93.148804	50.058945
485.304442	104.811917	50.063949
482.189424	90.528167	50.068954
478.861014	90.957490	50.073959
475.178561	101.362391	50.078964
471.895914	101.378797	50.083969
468.064285	101.601832	50.088973
464.811222	92.557919	50.093978
460.993867	98.141111	50.098983
457.660267	94.880400	50.103988
454.002706	95.323570	50.108993
450.455361	86.336253	50.113997
447.394321	95.172167	50.119002
443.556607	100.154328	50.124007
440.099050	102.476051	50.129012
436.350496	94.171589	50.134017
432.648148	96.857605	50.139021
429.663245	82.577757	50.144026
426.203122	92.093485	50.149031
422.539120	93.219737	50.154036
418.997888	99.013438	50.159041
415.143062	96.451673	50.164045
411.900006	87.374579	50.169050
408.580589	98.331555	50.174055
405.191010	90.473458	50.179060
401.370274	91.330163	50.184065
397.869269	95.918798	50.189069
394.612800	93.728295	50.194074
390.957193	98.365313	50.199079
387.092848	98.529535	50.204084
384.618052	92.121441	50.209089
380.660487	99.898663	50.214093
377.141048	86.304987	50.219098
373.232325	98.307084	50.224103
369.766972	100.173340	50.229108
366.335924	96.916076	50.234113
362.514707	103.492787	50.239117
359.903764	89.231189	50.244122
356.290876	102.296325	50.249127
352.758891	93.424756	50.254132
349.412299	95.900397	50.259137
345.230072	100.670727	50.264141
341.948664	89.119995	50.269146
338.175272	96.085025	50.274151
335.031927	88.112882	50.279156
331.529453	89.771431	50.284161
327.662867	93.597592	50.289165
324.497677	97.890348	50.294170
320.771840	91.801443	50.299175
316.750932	99.673315	50.304180
313.952237	92.634144	50.309185
310.305191	94.260887	50.314189
307.218771	95.715557	50.319194
303.590932	98.385373	50.324199
299.868045	95.877388	50.329204
296.484629	91.699418	50.334209
293.144491	95.342244	50.339213
289.278842	82.578944	50.344218
285.814882	97.065639	50.349223
282.026493	95.181667	50.354228
279.061958	94.504651	50.359233
275.226773	96.388436	50.364237
272.127028	86.670412	50.369242
268.180583	94.487729	50.374247
264.982475	98.643134	50.379252
261.614563	87.060484	50.384257
257.676923	96.462902	50.389261
254.364060	92.403489	50.394266
250.864999	91.869972	50.399271
247.391507	90.299372	50.404276
244.038921	90.897299	50.409281
240.409792	90.351463	50.414285
237.250561	97.177442	50.419290
233.213410	90.399574	50.424295
229.539201	88.122939	50.429300
226.244825	94.151663	50.434305
222.407516	100.089062	50.439309
219.252369	90.834156	50.444314
215.838663	91.305711	50.449319
212.457653	85.366035	50.454324
209.130177	84.624672	50.459329
204.994040	94.006646	50.464333
201.991164	89.473284	50.469338
198.441352	94.373113	50.474343
194.894715	93.456048	50.479348
191.190517	95.487463	50.484353
187.717508	93.427653	50.489357
184.426162	88.891331	50.494362
180.831474	84.459886	50.499367
177.037911	90.588573	50.504372
173.901220	101.817484	50.509377
170.228499	85.151786	50.514381
166.756903	90.074164	50.519386
163.271290	84.201254	50.524391
159.922998	95.188872	50.529396
156.619507	80.927699	50.534401
152.604964	94.757711	50.539405
149.330282	92.063906	50.544410
145.419849	88.308340	50.549415
142.226900	86.531578	50.554420
139.065155	87.609765	50.559425
134.957686	92.741051	50.564429
131.720402	87.136122	50.569434
128.375621	87.188220	50.574439
124.625978	97.442980	50.579444
121.310746	83.310480	50.584449
117.158107	90.550878	50.589453
114.087189	88.835358	50.594458
110.883838	84.211470	50.599463
107.053272	95.218505	50.604468
104.013783	88.678328	50.609473
100.390328	91.410558	50.614477
96.577338	87.653060	50.619482
93.110685	88.961138	50.624487
89.596107	89.148644	50.629492
86.326245	83.709604	50.634497
82.515387	94.782057	50.639501
79.232378	86.774760	50.644506
75.773432	87.171874	50.649511
72.155337	96.120383	50.654516
68.794091	90.935514	50.659521
65.166727	92.419514	50.664525
61.817739	86.452563	50.669530
58.217186	94.521225	50.674535
54.649744	92.167429	50.679540
51.199614	88.594952	50.684545
47.717933	100.017258	50.689549
44.365866	94.762807	50.694554
40.445422	93.384108	50.699559
36.881700	84.363841	50.704564
33.544923	88.544852	50.709569
29.971480	90.319473	50.714573
26.447764	85.886651	50.719578
22.908993	100.220429	50.724583
19.490265	90.950919	50.729588
16.615012	83.984125	50.734593
12.716425	93.598142	50.739597
9.526106	88.429320	50.744602
5.873274	84.098098	50.749607
1.983887	86.857064	50.754612