Fri Jun 17 17:23:38 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.753149	88.561291	0.000000
0.522751	85.526713	0.005005
0.402308	96.743116	0.010010
0.626733	87.405940	0.015014
0.134205	77.979552	0.020019
0.001872	58.963181	0.025024
0.035498	55.616552	0.030029
-0.537239	51.416019	0.035034
-0.334490	38.493613	0.040038
-0.891481	23.217438	0.045043
-1.382993	19.607048	0.050048
-1.485376	12.728121	0.055053
-1.919471	16.702465	0.060058
-1.894640	-11.022692	0.065062
-2.477002	2.246485	0.070067
-3.197076	-10.673456	0.075072
-3.458795	-3.628890	0.080077
-3.565920	-6.194953	0.085082
-3.636261	-2.190499	0.090086
-4.020286	14.754354	0.095091
-4.282349	-1.639756	0.100096
-4.040102	-6.038877	0.105101
-4.613265	-2.863107	0.110106
-5.066307	-3.398568	0.115110
-5.284637	-0.103585	0.120115
-5.621233	-9.645029	0.125120
-5.611971	2.834960	0.130125
-5.745552	-10.128591	0.135130
-6.244271	-8.229294	0.140134
-6.863697	-7.476552	0.145139
-6.876313	-7.219132	0.150144
-6.803615	-6.504865	0.155149
-7.127202	-8.592929	0.160154
-7.405198	-6.590411	0.165158
-7.921295	-3.595015	0.170163
-8.061730	-5.530990	0.175168
-8.506258	2.135166	0.180173
-8.540820	-2.377588	0.185178
-8.388134	0.472315	0.190182
-8.497009	-6.788346	0.195187
-9.293361	-2.502198	0.200192
-9.554792	-5.463915	0.205197
-10.162802	0.374704	0.210202
-9.997903	-4.739317	0.215206
-9.764100	-7.218587	0.220211
-10.472473	-4.591023	0.225216
-11.053689	-8.031787	0.230221
-11.369997	3.145077	0.235226
-11.540206	-2.558319	0.240230
-11.653542	0.139850	0.245235
-11.600202	-4.962929	0.250240
-11.610327	-9.758965	0.255245
-11.947210	2.560901	0.260250
-12.713882	-3.593315	0.265254
-12.924657	-5.979944	0.270259
-13.358239	0.457194	0.275264
-13.408419	-0.518181	0.280269
-13.404766	1.607031	0.285274
-13.425796	-4.875752	0.290278
-13.795602	-1.135277	0.295283
-14.367534	-3.928367	0.300288
-14.455663	-6.830484	0.305293
-15.075780	-2.109704	0.310298
-15.037933	-8.342189	0.315302
-14.889088	-7.349319	0.320307
-15.570032	2.953989	0.325312
-16.316399	-3.270496	0.330317
-16.381788	0.908168	0.335322
-16.267528	-8.959217	0.340326
-16.626040	4.515866	0.345331
-16.841058	5.690574	0.350336
-16.441873	-2.332562	0.355341
-17.046072	1.604934	0.360346
-17.702088	-2.845767	0.365350
-17.964413	3.874492	0.370355
-17.995738	-7.776047	0.375360
-17.885075	2.181384	0.380365
-18.083003	-1.129507	0.385370
-18.528351	-4.640805	0.390374
-19.288016	4.511537	0.395379
-19.792593	-3.502867	0.400384
-19.503074	0.313707	0.405389
-19.753114	1.522257	0.410394
-19.492788	-6.658749	0.415398
-20.221359	1.074352	0.420403
-20.302994	8.463722	0.425408
-20.480091	-5.956988	0.430413
-20.811367	9.394527	0.435418
-21.409637	-1.697660	0.440422
-21.909063	-1.533370	0.445427
-22.168941	-0.427770	0.450432
-22.305613	-6.768787	0.455437
-22.741351	-2.779965	0.460442
-22.354379	-3.820305	0.465446
-22.529757	1.519974	0.470451
-22.649252	-3.051279	0.475456
-23.133265	-3.551201	0.480461
-23.759889	0.215583	0.485466
-24.025066	-6.619896	0.490470
-23.885921	-0.846464	0.495475
-24.212216	-0.059760	0.500480
-24.287607	-6.920668	0.505485
-24.583295	3.721160	0.510490
-25.070001	-3.231417	0.515494
-25.758777	-4.321854	0.520499
-25.878605	4.393608	0.525504
-25.772221	-4.092538	0.530509
-26.003705	-1.273303	0.535514
-25.873427	-9.223521	0.540518
-26.379115	8.436346	0.545523
-26.884636	5.080679	0.550528
-26.931140	-8.168081	0.555533
-27.277850	1.515504	0.560538
-27.268830	-4.490194	0.565542
-27.879988	-2.409210	0.570547
-28.834392	-4.184828	0.575552
-28.828246	-7.754396	0.580557
-29.083991	-8.102821	0.585562
-28.409375	-1.885602	0.590566
-28.957839	2.327577	0.595571
-29.138754	7.443032	0.600576
-29.027467	-2.086230	0.605581
-29.718813	1.701771	0.610586
-29.987563	1.890668	0.615590
-30.397351	2.691842	0.620595
-30.529622	-4.237952	0.625600
-30.587465	-3.817321	0.630605
-30.568311	-4.413900	0.635610
-31.473426	-8.327694	0.640614
-31.640085	0.747587	0.645619
-31.846713	-4.691447	0.650624
-32.004631	-7.580778	0.655629
-32.419111	1.933120	0.660634
-32.571905	-3.608002	0.665638
-33.244394	8.367465	0.670643
-33.649559	6.968425	0.675648
-33.511911	-1.295792	0.680653
-33.533849	7.658549	0.685658
-33.753859	-1.140577	0.690662
-34.072595	-5.388833	0.695667
-33.881245	-1.737291	0.700672
-33.774345	-3.026285	0.705677
-34.930120	4.538467	0.710682
-35.056171	-1.905745	0.715686
-35.185348	1.816835	0.720691
-35.681853	-0.145003	0.725696
-36.239321	-2.058623	0.730701
-36.586082	0.383337	0.735706
-36.277233	-0.854571	0.740710
-36.533317	-4.825730	0.745715
-36.986956	-3.366470	0.750720
-36.928509	-5.997743	0.755725
-37.233989	-7.640282	0.760730
-37.140565	0.625534	0.765734
-37.945244	-3.032835	0.770739
-38.788828	2.747266	0.775744
-38.633475	-11.583657	0.780749
-39.143216	3.010758	0.785754
-39.275894	-8.722187	0.790758
-39.139564	5.769182	0.795763
-39.119268	-6.780488	0.800768
-38.830756	-9.156769	0.805773
-39.476583	1.111695	0.810778
-39.949981	-13.160890	0.815782
-40.030521	-3.581540	0.820787
-40.554122	-2.161957	0.825792
-40.147857	-11.413464	0.830797
-41.256504	5.952357	0.835802
-42.176930	-2.468486	0.840806
-41.882795	0.684287	0.845811
-42.502381	2.836135	0.850816
-41.982024	-0.398790	0.855821
-42.361770	6.677042	0.860826
-42.133390	-3.944173	0.865830
-42.093698	3.311955	0.870835
-43.213342	-5.446950	0.875840
-43.317729	-7.970645	0.880845
-43.745288	1.597324	0.885850
-43.700292	-5.253007	0.890854
-44.031770	-11.568545	0.895859
-44.217315	2.182659	0.900864
-44.892788	-5.208972	0.905869
-45.337378	7.170634	0.910874
-45.337361	-2.445506	0.915878
-45.257844	4.203527	0.920883
-45.266544	-1.787386	0.925888
-45.293566	-6.531674	0.930893
-46.089654	9.753909	0.935898
-46.776327	5.927729	0.940902
-46.631962	5.999415	0.945907
-46.830933	4.958592	0.950912
-46.616787	-3.909934	0.955917
-46.843598	-0.780679	0.960922
-47.514166	-0.894393	0.965926
-48.022405	-3.229207	0.970931
-48.609596	10.884961	0.975936
-48.247146	-0.366320	0.980941
-48.548276	3.251053	0.985946
-48.647342	3.211257	0.990950
-49.222837	-2.307947	0.995955
-49.980015	-2.144419	1.000960
-49.797306	-0.760940	1.005965
-50.242641	8.293180	1.010970
-50.099399	5.590190	1.015974
-49.991041	-1.757291	1.020979
-50.128885	1.379671	1.025984
-50.449113	-1.519581	1.030989
-51.332336	7.556612	1.035994
-51.463096	4.433665	1.040998
-51.485989	-4.967916	1.046003
-51.925150	6.557728	1.051008
-51.697617	-2.480756	1.056013
-52.474413	11.133912	1.061018
-52.766286	4.888941	1.066022
-52.838682	4.691387	1.071027
-53.147777	8.250886	1.076032
-53.030922	5.594708	1.081037
-53.821384	19.799701	1.086042
-54.263070	6.732257	1.091046
-54.368480	7.686287	1.096051
-54.759762	10.563660	1.101056
-54.568220	-0.166674	1.106061
-54.750260	6.054018	1.111066
-54.818891	6.862027	1.116070
-54.745609	1.869397	1.121075
-55.603324	8.744471	1.126080
-55.891105	-1.776738	1.131085
-56.271949	12.121784	1.136090
-56.316324	10.037038	1.141094
-56.205216	9.058927	1.146099
-56.891544	5.730952	1.151104
-57.370112	-4.465505	1.156109
-57.869675	-2.652887	1.161114
-57.629594	6.337223	1.166118
-58.013392	7.149670	1.171123
-58.099222	5.270527	1.176128
-57.635296	3.457274	1.181133
-58.284913	17.980432	1.186138
-58.902069	2.170060	1.191142
-58.857028	-2.198059	1.196147
-59.398968	7.611714	1.201152
-59.709307	2.534262	1.206157
-60.857697	-1.459853	1.211162
-60.108589	-1.619916	1.216166
-60.687998	3.960385	1.221171
-60.870934	3.245059	1.226176
-60.913591	1.114643	1.231181
-61.013512	5.575902	1.236186
-60.762275	11.389704	1.241190
-61.385484	-0.665443	1.246195
-62.307626	0.390211	1.251200
-62.267014	-8.448480	1.256205
-62.503045	6.126290	1.261210
-62.638215	-3.396929	1.266214
-62.808533	-2.785529	1.271219
-62.696268	8.849731	1.276224
-63.004096	-3.857131	1.281229
-63.590804	5.453141	1.286234
-64.058021	-2.429332	1.291238
-64.229019	5.283316	1.296243
-64.457421	0.637817	1.301248
-64.355078	0.794828	1.306253
-65.135194	1.320918	1.311258
-65.691557	-8.506224	1.316262
-65.737209	0.609127	1.321267
-66.342180	5.664833	1.326272
-65.848734	2.846995	1.331277
-66.265316	5.451522	1.336282
-66.030880	-5.770384	1.341286
-65.881561	4.017225	1.346291
-66.713225	13.028811	1.351296
-67.181008	6.975289	1.356301
-67.610308	0.746851	1.361306
-67.833113	8.389180	1.366310
-67.498348	1.973942	1.371315
-67.927959	1.327642	1.376320
-68.485972	-0.236213	1.381325
-69.069277	1.071348	1.386330
-69.139847	-3.799293	1.391334
-69.112672	-6.333412	1.396339
-69.369080	8.469704	1.401344
-68.941777	-10.083712	1.406349
-69.915094	4.374646	1.411354
-70.231997	-5.739557	1.416358
-70.240472	-1.209044	1.421363
-70.519583	-5.024229	1.426368
-70.784252	-1.975309	1.431373
-71.588574	1.415309	1.436378
-72.008023	0.399890	1.441382
-72.199447	-4.683117	1.446387
-72.076231	3.125858	1.451392
-72.035146	-0.682960	1.456397
-72.149638	8.618672	1.461402
-72.101751	6.640146	1.466406
-72.278584	-8.414025	1.471411
-72.936818	5.197112	1.476416
-73.354488	-0.424492	1.481421
-73.248503	8.258168	1.486426
-73.919901	-0.018768	1.491430
-74.749114	4.700076	1.496435
-75.125208	2.522871	1.501440
-75.143581	6.399697	1.506445
-75.177824	9.093205	1.511450
-75.359240	5.458911	1.516454
-75.268414	2.296764	1.521459
-75.508556	14.504258	1.526464
-75.073684	4.900683	1.531469
-75.596219	7.106654	1.536474
-76.707949	1.388293	1.541478
-76.769683	0.701166	1.546483
-76.977971	1.376302	1.551488
-77.110530	-3.781017	1.556493
-77.358904	0.463977	1.561498
-77.765654	3.861718	1.566502
-78.064405	-4.349685	1.571507
-78.793176	3.431607	1.576512
-78.436290	-4.276861	1.581517
-78.662147	3.539623	1.586522
-78.785854	-0.975278	1.591526
-78.739335	6.461652	1.596531
-79.702537	5.361196	1.601536
-79.840295	8.403427	1.606541
-80.147888	5.609425	1.611546
-80.487469	0.822769	1.616550
-80.700396	0.231026	1.621555
-80.628420	8.378653	1.626560
-80.388492	4.136199	1.631565
-80.845242	10.807678	1.636570
-81.040402	15.232675	1.641574
-81.584816	-1.120795	1.646579
-81.663612	5.522979	1.651584
-82.035251	-10.726990	1.656589
-83.002419	2.832888	1.661594
-83.099937	5.270518	1.666598
-83.345873	-1.511125	1.671603
-83.515491	-2.248397	1.676608
-83.665205	-3.442047	1.681613
-83.561692	-4.117374	1.686618
-83.700685	-3.350159	1.691622
-83.413915	3.505160	1.696627
-84.320454	8.249490	1.701632
-84.781376	-4.930176	1.706637
-85.182585	5.748530	1.711642
-85.155356	12.390665	1.716646
-85.153914	-10.559323	1.721651
-85.829694	0.012091	1.726656
-86.103593	4.307110	1.731661
-86.430528	-2.375425	1.736666
-86.609019	-1.161598	1.741670
-86.088311	-0.982967	1.746675
-86.720992	7.205627	1.751680
-86.889592	-6.245220	1.756685
-87.628739	3.580758	1.761690
-88.208010	5.903706	1.766694
-88.052385	-2.517610	1.771699
-88.086972	4.212743	1.776704
-88.163954	0.448612	1.781709
-88.583974	-1.235462	1.786714
-89.332361	10.148007	1.791718
-89.565910	3.453300	1.796723
-89.884045	-0.585090	1.801728
-89.903615	4.469602	1.806733
-90.701551	-0.397340	1.811738
-90.403572	-5.754295	1.816742
-90.053323	-6.316128	1.821747
-90.207655	5.244255	1.826752
-90.138934	-6.591426	1.831757
-91.087150	1.635608	1.836762
-91.523970	1.465483	1.841766
-91.683583	-10.905482	1.846771
-91.784351	4.447170	1.851776
-92.040189	-2.002297	1.856781
-92.962816	1.001490	1.861786
-93.460015	-7.312485	1.866790
-93.278914	-1.648449	1.871795
-93.565511	1.146799	1.876800
-93.628522	-6.536265	1.881805
-93.851251	7.428909	1.886810
-93.487892	7.429261	1.891814
-93.675691	-1.510974	1.896819
-94.083283	6.736500	1.901824
-94.697576	0.522640	1.906829
-94.838086	3.920522	1.911834
-94.982153	13.346654	1.916838
-95.527916	0.065849	1.921843
-95.970557	9.051444	1.926848
-96.680229	3.020972	1.931853
-96.732128	-0.421535	1.936858
-96.971521	10.696369	1.941862
-96.424622	-3.309126	1.946867
-96.766048	-1.418403	1.951872
-96.653150	-11.214911	1.956877
-97.006788	-1.358696	1.961882
-97.445106	10.664082	1.966886
-97.560978	2.283753	1.971891
-98.102494	7.487371	1.976896
-98.386161	3.300976	1.981901
-99.129279	4.531905	1.986906
-99.682368	10.034036	1.991910
-99.484809	0.013291	1.996915
-99.648899	6.732634	2.006912
-98.847696	6.833929	2.016909
-98.396326	-0.501342	2.026906
-98.335587	0.495595	2.036902
-98.161128	6.007765	2.046899
-97.180545	2.279322	2.056896
-96.990192	1.618133	2.066893
-95.923793	0.571644	2.076890
-95.665583	3.575603	2.086886
-95.208002	0.591857	2.096883
-94.263069	0.063866	2.106880
-94.123920	-4.228687	2.116877
-93.972256	-3.500759	2.126874
-93.415068	2.799370	2.136870
-92.686610	-4.504706	2.146867
-92.341140	-1.326562	2.156864
-91.831805	-3.412992	2.166861
-91.336885	-0.922780	2.176858
-90.367370	4.185943	2.186854
-89.890978	1.820074	2.196851
-89.620251	5.698036	2.206848
-89.686290	9.806249	2.216845
-88.793592	3.413388	2.226842
-88.179791	3.264085	2.236838
-87.568552	0.283644	2.246835
-86.863279	4.803435	2.256832
-86.751785	7.246740	2.266829
-86.538250	-0.702204	2.276826
-85.717017	-8.152105	2.286822
-85.163497	7.903707	2.296819
-84.313240	13.727555	2.306816
-83.803874	2.358464	2.316813
-83.354039	-0.353106	2.326810
-83.516084	-1.396128	2.336806
-82.997441	-1.236003	2.346803
-82.271392	8.286302	2.356800
-81.805292	7.799382	2.366797
-80.530458	3.191390	2.376794
-80.615941	0.301081	2.386790
-80.396058	8.967230	2.396787
-79.753836	6.414742	2.406784
-79.208123	-0.526029	2.416781
-78.690618	-0.221084	2.426778
-78.058548	3.662805	2.436774
-77.275163	-1.063247	2.446771
-77.247197	1.312538	2.456768
-77.120031	6.243379	2.466765
-75.943248	-2.288317	2.476762
-75.541657	7.049244	2.486758
-75.344917	3.142875	2.496755
-74.249980	-6.079399	2.506752
-74.311033	0.060520	2.516749
-73.840381	2.302060	2.526746
-73.014632	2.173246	2.536742
-72.851810	-1.824892	2.546739
-72.146028	3.934652	2.556736
-71.341897	2.674316	2.566733
-71.152645	2.125933	2.576730
-70.909476	1.111775	2.586726
-70.229868	-0.788382	2.596723
-69.755744	7.403194	2.606720
-69.000309	4.789408	2.616717
-68.218397	6.835566	2.626714
-68.072603	12.653426	2.636710
-67.964433	7.360123	2.646707
-66.863387	6.542810	2.656704
-66.332729	8.403711	2.666701
-66.310590	2.660390	2.676698
-65.799021	3.384607	2.686694
-64.867394	3.438149	2.696691
-64.823947	7.945854	2.706688
-63.951430	-0.614691	2.716685
-63.349517	-0.524915	2.726682
-63.129484	-3.564800	2.736678
-62.845094	-3.054540	2.746675
-61.715271	3.107533	2.756672
-61.434049	5.543965	2.766669
-61.558149	-5.691763	2.776666
-60.619021	-8.653795	2.786662
-59.972114	0.996662	2.796659
-59.908886	3.359078	2.806656
-59.115912	0.540681	2.816653
-58.592084	1.913305	2.826650
-58.302648	1.826223	2.836646
-57.265687	5.453134	2.846643
-57.103302	10.135886	2.856640
-56.832982	7.352994	2.866637
-55.897865	8.269199	2.876634
-55.335966	6.662461	2.886630
-55.047680	7.687173	2.896627
-54.647715	6.770442	2.906624
-53.781898	10.679698	2.916621
-53.894366	5.158705	2.926618
-53.455721	1.610850	2.936614
-52.381075	6.074190	2.946611
-52.223027	6.779721	2.956608
-51.270693	10.433150	2.966605
-50.722553	6.349227	2.976602
-50.214811	1.108058	2.986598
-50.535235	3.946208	2.996595
-49.789886	2.669566	3.006592
-49.178412	0.502344	3.016589
-48.668605	5.892586	3.026586
-48.016757	-0.510220	3.036582
-47.458408	1.062351	3.046579
-47.464863	-1.972883	3.056576
-46.401028	3.896678	3.066573
-46.167544	0.340247	3.076570
-45.276624	0.182823	3.086566
-44.647966	2.709693	3.096563
-44.517456	-1.548231	3.106560
-44.668411	0.698637	3.116557
-43.650555	-1.464213	3.126554
-43.143957	2.416632	3.136550
-42.438195	1.678268	3.146547
-41.705342	4.355567	3.156544
-41.397422	-0.024907	3.166541
-41.335603	-0.954584	3.176538
-40.780083	2.058247	3.186534
-40.003700	0.204841	3.196531
-39.463570	-0.964778	3.206528
-38.958996	4.083331	3.216525
-38.089642	4.674185	3.226522
-38.228840	-1.945867	3.236518
-37.575011	5.983092	3.246515
-36.862022	1.045082	3.256512
-36.297544	5.862139	3.266509
-36.293549	1.385576	3.276506
-35.961690	5.850084	3.286502
-35.148474	-0.280007	3.296499
-34.491138	6.511476	3.306496
-33.283525	8.009917	3.316493
-33.414961	-0.140325	3.326490
-33.406807	6.994979	3.336486
-32.845993	1.386178	3.346483
-31.933979	-0.236666	3.356480
-31.758744	8.682112	3.366477
-30.537329	1.134282	3.376474
-30.008670	4.914449	3.386470
-29.937181	8.212435	3.396467
-29.984552	4.153998	3.406464
-29.223586	-2.734622	3.416461
-28.264131	3.759468	3.426458
-28.193343	-3.714865	3.436454
-27.486837	1.868917	3.446451
-27.029252	-0.843145	3.456448
-26.759250	2.684826	3.466445
-25.510505	-2.074507	3.476442
-25.132833	-6.214655	3.486438
-25.045910	-4.867209	3.496435
-25.302742	-4.727355	3.506432
-23.959203	1.726011	3.516429
-23.444131	-1.384845	3.526426
-22.741312	-2.019775	3.536422
-22.257574	0.444447	3.546419
-22.182507	3.124785	3.556416
-22.031294	-3.686391	3.566413
-21.011608	-3.297753	3.576410
-20.641047	-4.326759	3.586406
-19.460155	-3.778595	3.596403
-19.110207	-1.079930	3.606400
-19.552969	7.887828	3.616397
-18.519558	4.457271	3.626394
-17.638687	1.512044	3.636390
-17.408696	-2.771899	3.646387
-17.384692	1.782705	3.656384
-16.613555	4.520232	3.666381
-15.837753	4.033017	3.676378
-15.517628	-1.495665	3.686374
-14.640341	-0.586040	3.696371
-14.572675	6.593117	3.706368
-14.360216	4.247020	3.716365
-13.308137	0.090801	3.726362
-12.814273	-0.908712	3.736358
-12.615436	-2.766884	3.746355
-11.630078	3.012396	3.756352
-11.187849	-6.762095	3.766349
-10.882955	2.481890	3.776346
-10.818421	0.655130	3.786342
-9.815861	-2.659649	3.796339
-9.194115	6.379931	3.806336
-9.396822	1.253689	3.816333
-8.536429	-1.304228	3.826330
-8.080118	7.586803	3.836326
-7.669177	5.562971	3.846323
-6.723283	9.435615	3.856320
-6.155967	0.506929	3.866317
-6.066902	0.543056	3.876314
-5.630641	8.470250	3.886310
-4.888584	9.599939	3.896307
-4.753084	9.984788	3.906304
-3.763322	5.960441	3.916301
-3.428943	8.303281	3.926298
-3.242705	13.072765	3.936294
-2.725425	27.185883	3.946291
-2.430246	33.578396	3.956288
-1.834022	49.334954	3.966285
-1.353757	64.190653	3.976282
-0.802374	74.630393	3.986278
-0.743556	94.585875	3.996275
-0.035330	117.892757	4.006272
0.000000	124.536475	4.011277
0.193954	146.028238	4.016282
0.707110	152.299990	4.021286
0.414853	164.070100	4.026291
0.675125	175.825343	4.031296
1.050995	183.057059	4.036301
0.756932	179.989237	4.041306
0.830063	186.761562	4.046310
1.024689	204.680187	4.051315
1.259824	210.428471	4.056320
1.529293	205.055663	4.061325
1.655656	221.279313	4.066330
1.421777	216.808898	4.071334
1.204939	214.956435	4.076339
1.538070	207.384223	4.081344
1.685334	225.491107	4.086349
1.411364	218.497934	4.091354
1.599514	197.662387	4.096358
1.311940	192.747827	4.101363
1.452765	188.657956	4.106368
1.391591	192.191876	4.111373
1.354221	198.640201	4.116378
1.778201	212.542676	4.121382
1.561474	208.923273	4.126387
1.499909	203.782494	4.131392
1.408684	207.474741	4.136397
1.596712	202.801005	4.141402
1.610446	207.864835	4.146406
1.128329	209.503680	4.151411
1.443687	222.789199	4.156416
1.648924	221.436285	4.161421
1.703850	218.408524	4.166426
1.948573	218.258898	4.171430
1.776506	227.812365	4.176435
1.635131	210.673163	4.181440
1.523423	218.240298	4.186445
1.473893	212.759286	4.191450
1.853374	223.150715	4.196454
1.727420	222.586138	4.201459
1.817841	224.571851	4.206464
1.517616	229.879284	4.211469
1.428566	230.914869	4.216474
1.364616	228.429403	4.221478
1.215726	232.263651	4.226483
1.147207	230.309772	4.231488
1.645050	234.227546	4.236493
1.835615	219.956462	4.241498
1.891383	227.156353	4.246502
1.708699	221.801858	4.251507
1.934645	229.970986	4.256512
1.656618	232.639539	4.261517
1.475744	231.891887	4.266522
2.324776	250.095477	4.271526
2.037600	251.606416	4.276531
1.624650	236.313192	4.281536
1.630020	239.352596	4.286541
1.934819	255.538336	4.291546
2.073353	252.044383	4.296550
1.954452	263.800949	4.301555
1.953046	273.593072	4.306560
2.231159	257.040429	4.311565
1.864221	254.469947	4.316570
2.155875	251.270620	4.321574
1.939599	259.109716	4.326579
2.025496	260.918585	4.331584
2.107739	263.153512	4.336589
1.697474	259.448063	4.341594
2.282217	262.066757	4.346598
2.152009	265.392338	4.351603
2.227482	261.587999	4.356608
2.196357	269.757053	4.361613
1.879471	262.283974	4.366618
2.233414	265.039302	4.371622
2.055980	268.984863	4.376627
2.312432	261.288420	4.381632
2.206255	260.156575	4.386637
2.339290	261.159985	4.391642
2.182831	236.839321	4.396646
1.993037	234.269790	4.401651
1.791658	249.892204	4.406656
2.040172	257.099342	4.411661
2.237196	262.439382	4.416666
2.321684	261.910472	4.421670
2.128981	266.624621	4.426675
2.270924	260.841815	4.431680
2.491630	262.252355	4.436685
2.483914	265.628420	4.441690
2.589466	262.262886	4.446694
2.538442	259.362839	4.451699
2.442931	255.490030	4.456704
2.264549	263.107341	4.461709
2.256845	255.920711	4.466714
2.503794	263.581783	4.471718
2.256718	268.241034	4.476723
2.473051	266.373400	4.481728
2.307006	266.161609	4.486733
2.104350	258.476553	4.491738
2.237786	258.873489	4.496742
2.089714	265.620455	4.501747
2.577946	257.582779	4.506752
2.420435	261.694734	4.511757
2.546405	276.918814	4.516762
2.458259	268.596472	4.521766
2.290345	264.507182	4.526771
2.654078	265.851721	4.531776
2.492869	262.786270	4.536781
2.164794	258.844961	4.541786
2.558500	256.951597	4.546790
2.417308	270.848211	4.551795
2.462426	254.244510	4.556800
2.738122	260.526767	4.561805
2.643464	261.112180	4.566810
2.316453	261.310760	4.571814
2.354624	271.847948	4.576819
2.548466	268.908187	4.581824
2.413929	280.070627	4.586829
2.217366	288.076564	4.591834
2.581314	293.566866	4.596838
2.483234	299.656505	4.601843
2.692625	289.456395	4.606848
2.719563	295.923869	4.611853
2.559397	298.627308	4.616858
3.052463	305.633586	4.621862
2.889073	296.606622	4.626867
2.746612	305.715357	4.631872
2.628809	303.345391	4.636877
2.638698	301.455628	4.641882
2.571008	289.618112	4.646886
2.652289	309.285727	4.651891
2.760811	298.225027	4.656896
2.917604	293.267361	4.661901
2.723232	301.147633	4.666906
3.047577	300.502092	4.671910
2.732119	297.574160	4.676915
2.672587	298.298185	4.681920
2.313270	294.404487	4.686925
2.785000	321.914608	4.691930
3.254134	324.603244	4.696934
3.082749	312.350979	4.701939
2.848799	327.156591	4.706944
2.852809	323.629530	4.711949
2.956189	338.252397	4.716954
3.140520	335.667237	4.721958
2.653086	331.933944	4.726963
2.855890	338.103238	4.731968
3.000868	333.793991	4.736973
3.180910	345.694519	4.741978
3.460534	337.401590	4.746982
3.350571	340.726190	4.751987
3.388184	329.422297	4.756992
3.013821	315.409599	4.761997
2.963020	303.865267	4.767002
3.303947	309.728811	4.772006
2.837985	318.196902	4.777011
3.285705	321.377500	4.782016
3.311694	322.892832	4.787021
3.130677	316.289096	4.792026
2.995374	316.469627	4.797030
3.027123	317.884150	4.802035
2.997621	332.221255	4.807040
3.422926	334.216835	4.812045
3.340068	345.361261	4.817050
3.479367	344.544996	4.822054
3.591023	345.031000	4.827059
3.128215	314.848977	4.832064
3.149308	316.113520	4.837069
3.148329	335.802735	4.842074
3.770579	323.458414	4.847078
3.082756	330.016088	4.852083
3.224661	327.806799	4.857088
3.257287	329.171054	4.862093
3.067100	335.821844	4.867098
3.373454	337.193489	4.872102
3.251290	338.554662	4.877107
3.247642	341.838307	4.882112
3.285639	331.868925	4.887117
3.414514	343.650871	4.892122
3.466122	325.841285	4.897126
3.236447	338.960565	4.902131
3.341863	329.410761	4.907136
3.597241	332.929198	4.912141
3.157113	343.153433	4.917146
3.623404	330.978293	4.922150
3.309784	335.488388	4.927155
3.268763	323.504135	4.932160
3.734521	330.350584	4.937165
3.228558	334.240456	4.942170
3.646940	327.553863	4.947174
3.249414	338.732232	4.952179
3.421820	343.350792	4.957184
3.724459	350.351840	4.962189
3.586914	368.626800	4.967194
3.856070	370.123822	4.972198
3.792172	349.025673	4.977203
3.779263	343.653771	4.982208
3.658284	340.663314	4.987213
3.170202	340.785460	4.992218
3.492696	357.005465	4.997222
3.606645	356.254784	5.002227
3.608351	363.887797	5.007232
3.911306	354.754477	5.012237
3.892145	363.328498	5.017242
3.841769	356.250936	5.022246
3.732231	368.517124	5.027251
3.889132	371.386524	5.032256
4.142362	369.535044	5.037261
3.737552	363.948452	5.042266
4.005692	335.990621	5.047270
3.599044	345.651624	5.052275
3.158857	340.306538	5.057280
3.702288	356.320112	5.062285
3.410695	367.396041	5.067290
3.935264	371.727957	5.072294
3.770866	368.060944	5.077299
3.724826	371.987850	5.082304
4.068897	372.452197	5.087309
3.936431	374.403539	5.092314
3.909246	371.810509	5.097318
3.461902	370.599002	5.102323
3.972513	363.167713	5.107328
3.760595	362.163943	5.112333
3.832876	370.546154	5.117338
3.782602	361.078053	5.122342
3.663845	375.168959	5.127347
4.112410	391.771597	5.132352
4.616864	390.158181	5.137357
4.126038	383.250508	5.142362
3.909911	373.924420	5.147366
3.959782	368.652189	5.152371
3.969038	396.158797	5.157376
4.255629	391.370942	5.162381
4.200608	409.544815	5.167386
4.345621	398.474032	5.172390
4.151450	392.307378	5.177395
3.862625	380.335653	5.182400
4.012579	383.505568	5.187405
3.751992	402.242261	5.192410
4.398925	402.667913	5.197414
4.125945	401.837092	5.202419
4.308821	403.694584	5.207424
4.301138	404.143988	5.212429
4.274842	404.038025	5.217434
4.254195	395.692950	5.222438
4.475677	405.518953	5.227443
4.537023	405.545241	5.232448
4.690102	384.491099	5.237453
4.103624	380.639673	5.242458
4.433263	369.100732	5.247462
4.201036	377.138888	5.252467
3.871541	375.664478	5.257472
4.336755	386.533133	5.262477
4.056581	406.187736	5.267482
4.431152	402.618405	5.272486
4.322629	400.244908	5.277491
4.454093	402.033985	5.282496
4.644597	398.086567	5.287501
4.398876	397.172083	5.292506
4.476973	397.061596	5.297510
4.703611	398.117340	5.302515
4.184604	409.304506	5.307520
4.476159	399.551249	5.312525
4.134056	405.037384	5.317530
4.429024	397.142465	5.322534
4.258578	411.266267	5.327539
4.337049	406.435050	5.332544
4.248084	402.866986	5.337549
4.211588	404.156698	5.342554
4.420405	398.342400	5.347558
4.743930	403.737438	5.352563
4.354884	402.701142	5.357568
4.580051	406.305525	5.362573
4.357550	407.594185	5.367578
4.417407	425.854163	5.372582
4.672916	431.415425	5.377587
4.529208	427.392517	5.382592
4.495279	432.461974	5.387597
4.721415	448.335978	5.392602
4.754342	437.422525	5.397606
4.580955	435.551368	5.402611
4.722108	434.482989	5.407616
4.833878	434.478795	5.412621
4.808621	442.064626	5.417626
4.817274	446.520794	5.422630
4.719195	438.547915	5.427635
4.705430	438.946628	5.432640
4.919718	433.472997	5.437645
4.743102	446.080143	5.442650
4.816085	437.422295	5.447654
4.935951	444.003049	5.452659
4.773850	444.203427	5.457664
4.871215	431.835358	5.462669
4.690917	438.518490	5.467674
4.703079	434.462964	5.472678
4.330065	435.657451	5.477683
4.513942	443.027960	5.482688
4.678603	426.791971	5.487693
4.612062	440.372037	5.492698
4.979502	447.289739	5.497702
4.893037	464.536488	5.502707
5.096729	472.241164	5.507712
5.168699	457.768753	5.512717
4.794941	449.226197	5.517722
5.211986	444.891039	5.522726
5.002467	445.042268	5.527731
5.001215	452.684302	5.532736
5.342653	435.413099	5.537741
4.665860	447.616552	5.542746
4.968230	445.763211	5.547750
4.803800	457.799027	5.552755
5.227493	454.256054	5.557760
5.593394	470.217162	5.562765
5.177730	467.332295	5.567770
5.216447	441.574030	5.572774
4.831162	443.146681	5.577779
5.172186	457.496516	5.582784
5.321690	450.805029	5.587789
5.037875	457.441832	5.592794
5.447558	454.996800	5.597798
5.207527	452.169177	5.602803
4.868843	450.555192	5.607808
5.079240	454.491396	5.612813
5.123833	466.162136	5.617818
5.045679	459.633200	5.622822
5.261747	472.551027	5.627827
5.034713	479.429217	5.632832
5.385515	476.409259	5.637837
5.172156	474.070344	5.642842
5.536880	474.240190	5.647846
5.640732	468.979278	5.652851
5.359508	468.812873	5.657856
5.453171	476.433026	5.662861
5.498970	475.093763	5.667866
5.287787	478.404235	5.672870
5.277747	469.004566	5.677875
5.203464	478.977851	5.682880
5.371462	477.497902	5.687885
5.148096	475.303521	5.692890
5.363489	475.184422	5.697894
5.330994	475.523891	5.702899
5.211179	475.559767	5.707904
5.313912	476.787469	5.712909
5.510654	476.169248	5.717914
5.358864	473.527252	5.722918
5.237626	475.080882	5.727923
4.934563	478.608698	5.732928
5.094242	485.259616	5.737933
5.035986	494.914508	5.742938
5.255411	493.799174	5.747942
5.298621	509.162350	5.752947
5.207683	504.749593	5.757952
5.424200	497.814287	5.762957
5.306847	509.777592	5.767962
5.663349	516.974600	5.772966
5.784024	533.194786	5.777971
5.653688	538.308521	5.782976
5.955169	534.927728	5.787981
5.744877	514.201000	5.792986
5.725610	505.681388	5.797990
5.482603	497.457479	5.802995
5.644552	514.728709	5.808000
5.865215	519.087301	5.813005
5.498863	531.273361	5.818010
5.868886	538.114897	5.823014
5.771387	532.777118	5.828019
5.939340	542.229863	5.833024
6.002923	538.229306	5.838029
5.732857	520.517954	5.843034
5.574369	512.686504	5.848038
5.710510	521.130605	5.853043
5.786027	542.504468	5.858048
6.167989	532.855688	5.863053
6.149197	533.841331	5.868058
5.447876	523.450648	5.873062
6.023236	524.648738	5.878067
5.581827	536.803074	5.883072
5.870079	538.129399	5.888077
5.887576	533.978830	5.893082
5.629824	532.118921	5.898086
6.188846	531.230517	5.903091
5.823129	532.549503	5.908096
6.255174	539.041705	5.913101
6.057348	534.255582	5.918106
5.861017	537.429408	5.923110
6.262123	532.643986	5.928115
5.926945	534.662193	5.933120
5.981104	536.312776	5.938125
5.858655	542.257373	5.943130
5.982154	534.387529	5.948134
6.555027	540.634124	5.953139
5.829444	537.606377	5.958144
5.903126	539.713709	5.963149
6.132758	542.625123	5.968154
6.122896	530.719596	5.973158
6.166877	537.886859	5.978163
5.470909	541.114918	5.983168
5.775330	532.959847	5.988173
5.862779	546.799761	5.993178
5.936472	538.664880	5.998182
6.027990	561.038781	6.003187
6.267336	575.754519	6.008192
6.173842	557.319148	6.013197
6.380930	560.199186	6.018202
6.098069	577.209929	6.023206
6.416961	566.622613	6.028211
6.257999	569.096000	6.033216
6.483512	560.994286	6.038221
6.431044	568.269948	6.043226
6.089630	548.740903	6.048230
6.158212	546.751370	6.053235
6.128809	557.743401	6.058240
5.865104	563.305758	6.063245
6.182978	567.041590	6.068250
6.237017	577.821837	6.073254
6.172962	575.811720	6.078259
6.195084	571.044481	6.083264
6.381434	570.197493	6.088269
5.976368	581.926086	6.093274
6.339063	573.030763	6.098278
6.412820	575.983088	6.103283
6.115543	563.391999	6.108288
6.344683	563.854735	6.113293
6.146821	580.212572	6.118298
6.252282	570.915402	6.123302
6.438046	573.831942	6.128307
6.338360	574.683030	6.133312
6.637395	559.034342	6.138317
6.284696	547.976517	6.143322
6.110882	543.873924	6.148326
6.043768	553.529536	6.153331
5.902565	563.283902	6.158336
6.860792	567.851249	6.163341
6.282414	559.065973	6.168346
6.069825	549.167504	6.173350
6.413540	542.509609	6.178355
5.992488	552.896969	6.183360
6.097206	546.003707	6.188365
6.204054	542.913577	6.193370
6.537767	553.326847	6.198374
6.101938	549.995583	6.203379
6.332423	550.018624	6.208384
6.351517	545.365365	6.213389
6.176947	543.686993	6.218394
6.524225	545.690045	6.223398
6.388974	543.549880	6.228403
6.101970	541.915257	6.233408
6.486468	539.607798	6.238413
6.488133	543.147930	6.243418
6.251775	545.618390	6.248422
6.263912	534.890664	6.253427
6.260366	546.966114	6.258432
6.350192	546.021701	6.263437
6.427901	536.914267	6.268442
6.347919	541.462155	6.273446
6.465228	536.262723	6.278451
6.421388	540.370067	6.283456
6.757758	536.852838	6.288461
6.543101	544.467831	6.293466
6.382483	519.412332	6.298470
6.361513	507.401318	6.303475
5.895555	512.974579	6.308480
6.026780	505.223249	6.313485
6.037055	521.281604	6.318490
6.447087	526.298417	6.323494
6.275026	522.096476	6.328499
5.922282	525.165856	6.333504
6.323103	524.646719	6.338509
6.550318	547.838112	6.343514
6.135190	528.160712	6.348518
6.107871	529.284330	6.353523
6.338612	527.640814	6.358528
6.382582	523.320677	6.363533
6.280794	512.338983	6.368538
6.190330	508.484413	6.373542
6.277564	504.117228	6.378547
5.964882	506.559716	6.383552
6.440003	514.248702	6.388557
5.994125	506.652887	6.393562
5.929059	524.069013	6.398566
6.657717	531.051433	6.403571
6.476529	524.381331	6.408576
6.224780	515.982446	6.413581
6.636598	515.736372	6.418586
5.928588	511.007031	6.423590
6.193677	511.640604	6.428595
5.989792	517.313378	6.433600
6.008505	512.598623	6.438605
5.878682	507.668398	6.443610
6.218176	525.297306	6.448614
6.001620	537.068140	6.453619
6.103282	537.041550	6.458624
6.607786	532.165533	6.463629
6.461193	541.779686	6.468634
6.288514	543.307142	6.473638
6.410585	533.766284	6.478643
6.154070	530.991116	6.483648
6.350505	515.183106	6.488653
6.123529	510.787827	6.493658
5.772778	515.631527	6.498662
5.942459	530.454115	6.503667
6.154148	533.392781	6.508672
6.379848	531.717542	6.513677
6.353237	540.076617	6.518682
5.946135	533.801240	6.523686
6.278424	531.034770	6.528691
6.122896	540.127068	6.533696
6.669477	534.124758	6.538701
6.638002	538.989006	6.543706
6.143542	529.591670	6.548710
6.543714	525.264623	6.553715
6.207667	521.248991	6.558720
6.006923	506.505926	6.563725
6.395980	521.894118	6.568730
6.277631	518.748674	6.573734
5.970158	513.299772	6.578739
5.911075	527.082720	6.583744
6.345408	525.314788	6.588749
6.582599	539.462124	6.593754
6.144209	527.870154	6.598758
6.407812	521.808123	6.603763
6.050849	519.448273	6.608768
6.310040	522.309975	6.613773
6.118316	513.709500	6.618778
6.412383	530.191147	6.623782
6.586452	516.637880	6.628787
5.997696	509.518503	6.633792
5.962421	500.331003	6.638797
6.040418	513.793769	6.643802
6.576828	531.830017	6.648806
6.509092	517.823202	6.653811
5.969604	513.063877	6.658816
5.847611	502.340114	6.663821
6.008709	514.509733	6.668826
6.439840	533.251991	6.673830
6.635646	539.166187	6.678835
6.136812	525.852037	6.683840
6.176825	508.036275	6.688845
6.456334	514.302807	6.693850
6.126078	514.295119	6.698854
6.101904	502.984003	6.703859
6.181627	517.346737	6.708864
6.194909	515.109071	6.713869
6.585222	526.038030	6.718874
6.221119	521.395779	6.723878
6.133812	518.509213	6.728883
6.195974	510.271083	6.733888
6.464094	505.355429	6.738893
6.296138	504.518788	6.743898
6.180372	497.462489	6.748902
6.198208	497.590730	6.753907
5.900998	509.821720	6.758912
5.952092	500.459824	6.763917
6.593214	521.845029	6.768922
6.326138	514.300005	6.773926
6.204941	505.885347	6.778931
6.078490	510.225063	6.783936
6.413289	516.435440	6.788941
6.280663	506.485227	6.793946
6.004414	506.767923	6.798950
6.148562	508.192988	6.803955
6.457775	530.484288	6.808960
6.351342	518.870698	6.813965
6.230150	505.975301	6.818970
6.281771	501.886163	6.823974
6.481577	500.142019	6.828979
6.275865	497.719145	6.833984
6.278387	496.446867	6.838989
6.049901	495.617524	6.843994
5.655345	495.578886	6.848998
6.566717	492.528901	6.854003
6.164284	497.392829	6.859008
6.149659	495.579540	6.864013
6.293920	498.111447	6.869018
6.033536	505.671268	6.874022
6.210330	495.656412	6.879027
6.409468	522.086391	6.884032
6.206561	515.412009	6.889037
6.261780	509.387184	6.894042
5.856810	506.273002	6.899046
6.327371	516.395321	6.904051
6.028022	525.797061	6.909056
6.122812	523.722266	6.914061
6.125489	537.871084	6.919066
5.837792	536.010231	6.924070
6.182485	543.205661	6.929075
5.998564	540.358435	6.934080
6.435897	538.518567	6.939085
6.103257	534.453623	6.944090
6.075204	537.648222	6.949094
6.278620	545.772914	6.954099
6.094070	537.488355	6.959104
6.480106	537.961717	6.964109
6.556772	530.435527	6.969114
6.125787	537.020258	6.974118
6.265943	533.949853	6.979123
5.979579	531.026118	6.984128
6.153093	535.247113	6.989133
6.160793	540.508406	6.994138
5.972377	536.803509	6.999142
6.211037	541.693506	7.004147
6.011504	534.701631	7.009152
6.290693	533.143798	7.014157
6.184129	539.624879	7.019162
6.140748	540.161918	7.024166
6.579279	541.939836	7.029171
6.308137	538.957327	7.034176
6.287134	534.985433	7.039181
6.295524	536.005829	7.044186
6.172531	544.691929	7.049190
6.415828	530.414953	7.054195
6.305570	530.349387	7.059200
6.445331	536.823863	7.064205
6.449783	538.059814	7.069210
6.301138	538.639213	7.074214
6.291788	530.750603	7.079219
6.371682	531.115597	7.084224
6.386193	538.199153	7.089229
6.432609	542.634272	7.094234
6.160381	540.660536	7.099238
6.525612	522.810436	7.104243
6.191713	504.676754	7.109248
6.069954	507.018639	7.114253
6.047419	516.550981	7.119258
6.148206	535.105619	7.124262
6.262644	533.616215	7.129267
6.352903	534.570709	7.134272
6.303870	536.322312	7.139277
6.601751	524.338013	7.144282
6.323536	521.849040	7.149286
6.298890	509.656493	7.154291
5.798780	517.448765	7.159296
5.907986	507.908877	7.164301
6.404543	526.575526	7.169306
6.101931	537.086259	7.174310
6.378881	540.518869	7.179315
6.687087	541.969161	7.184320
6.252173	522.233883	7.189325
5.945892	522.646288	7.194330
5.927625	509.415673	7.199334
6.159265	518.232457	7.204339
6.260023	534.595078	7.209344
6.325026	544.100456	7.214349
6.658187	532.981729	7.219354
6.204367	525.915694	7.224358
6.476792	502.973954	7.229363
6.002763	509.912352	7.234368
6.151625	510.585568	7.239373
6.225737	497.661861	7.244378
6.003692	509.122188	7.249382
6.325860	501.239075	7.254387
6.094001	519.579815	7.259392
6.148518	519.090412	7.264397
6.378639	526.056035	7.269402
6.087284	525.581297	7.274406
6.504440	524.596097	7.279411
6.004984	520.852915	7.284416
6.299076	527.710027	7.289421
6.490871	526.281373	7.294426
6.135818	517.832168	7.299430
6.253710	514.624173	7.304435
6.150724	509.611342	7.309440
6.081441	503.061180	7.314445
6.295424	514.666111	7.319450
6.401431	520.838542	7.324454
6.652580	503.612462	7.329459
6.502618	504.590107	7.334464
6.583370	511.322039	7.339469
6.626120	504.697606	7.344474
6.328674	510.895847	7.349478
6.665364	510.087022	7.354483
6.157582	506.497178	7.359488
5.799458	505.896981	7.364493
6.187798	509.589118	7.369498
6.162786	508.814363	7.374502
6.299025	507.205106	7.379507
6.488131	518.158818	7.384512
6.333157	514.909546	7.389517
6.515353	505.337992	7.394522
6.121792	516.250213	7.399526
6.446269	506.786831	7.404531
6.489154	509.542794	7.409536
6.152580	502.172328	7.414541
6.228451	497.127799	7.419546
5.951506	508.692565	7.424550
6.082492	502.579964	7.429555
5.864275	514.950370	7.434560
6.132931	506.664304	7.439565
6.180917	506.165529	7.444570
6.242834	520.346517	7.449574
6.562952	506.303664	7.454579
6.443194	510.087553	7.459584
6.193328	507.462247	7.464589
6.330687	517.256718	7.469594
5.982254	512.517736	7.474598
6.465609	505.492295	7.479603
6.020959	512.652748	7.484608
6.446878	502.224698	7.489613
6.577277	504.989795	7.494618
6.322565	506.831822	7.499622
6.250889	497.196498	7.504627
6.259324	491.758639	7.509632
5.864502	476.145636	7.514637
5.985085	494.421651	7.519642
6.101626	501.248468	7.524646
6.551851	504.161099	7.529651
6.421135	507.292637	7.534656
6.244329	506.765510	7.539661
6.118230	508.015066	7.544666
6.038750	516.277143	7.549670
6.558831	510.803177	7.554675
6.138757	512.359909	7.559680
6.346004	504.134175	7.564685
6.450434	513.655083	7.569690
5.991078	501.238197	7.574694
6.397079	501.177205	7.579699
6.247655	494.630895	7.584704
6.119203	496.570534	7.589709
6.285270	491.945157	7.594714
6.162710	499.335447	7.599718
6.173738	505.944183	7.604723
6.414874	516.030632	7.609728
6.047218	509.102825	7.614733
6.158977	503.683704	7.619738
6.202210	507.510951	7.624742
6.110032	507.530591	7.629747
6.330655	516.743879	7.634752
6.183949	513.747994	7.639757
6.361420	513.253351	7.644762
6.150434	511.151826	7.649766
6.036318	512.138906	7.654771
6.364207	520.511472	7.659776
6.393235	509.434629	7.664781
6.519264	509.234082	7.669786
6.320877	500.506058	7.674790
6.154752	492.103611	7.679795
6.044768	489.386187	7.684800
6.009138	492.558356	7.689805
6.594269	500.681149	7.694810
6.160741	504.409245	7.699814
6.191309	493.235857	7.704819
6.363870	506.569825	7.709824
5.871273	503.298328	7.714829
6.219792	504.378421	7.719834
6.039997	514.770057	7.724838
6.369108	515.859297	7.729843
6.274704	513.500209	7.734848
6.115445	518.021405	7.739853
6.236002	512.692383	7.744858
6.097610	517.549333	7.749862
6.359444	511.612910	7.754867
6.045263	515.687034	7.759872
6.383371	516.564812	7.764877
6.117954	511.619036	7.769882
6.024717	516.760343	7.774886
6.027788	512.738078	7.779891
6.173748	520.365150	7.784896
6.063970	516.056952	7.789901
6.318463	510.058996	7.794906
5.596577	519.327704	7.799910
6.194279	520.542604	7.804915
6.205219	518.337690	7.809920
5.962821	514.943105	7.814925
6.110547	523.408962	7.819930
5.934728	516.912615	7.824934
6.166678	511.200597	7.829939
6.258022	515.943190	7.834944
6.176276	520.927876	7.839949
6.036154	523.613617	7.844954
5.624591	529.532261	7.849958
6.431597	547.210772	7.854963
6.613220	552.568470	7.859968
6.293040	544.962005	7.864973
6.490750	536.488800	7.869978
6.251184	536.151286	7.874982
6.591558	517.618393	7.879987
6.465830	520.861783	7.884992
6.661223	521.650997	7.889997
6.528003	515.156450	7.895002
6.182268	521.028037	7.900006
6.403908	513.681806	7.905011
6.378447	521.257054	7.910016
6.234986	511.746529	7.915021
6.415990	517.720997	7.920026
6.213118	516.107717	7.925030
6.551087	516.875404	7.930035
6.479237	508.144696	7.935040
6.500100	515.189693	7.940045
6.390581	494.832825	7.945050
5.728172	492.908159	7.950054
6.003649	494.737445	7.955059
6.001725	507.550832	7.960064
5.950901	510.736580	7.965069
6.185928	506.753318	7.970074
6.098565	517.692004	7.975078
6.558799	506.715373	7.980083
6.231115	513.995114	7.985088
6.168466	517.204340	7.990093
6.597989	520.168565	7.995098
6.348717	519.200199	8.000102
6.459307	519.066944	8.005107
6.436396	509.677481	8.010112
5.865778	501.365398	8.015130
6.361664	503.152088	8.020147
6.231375	515.067002	8.025165
6.281377	505.919090	8.030182
6.389191	509.891951	8.035200
6.007781	509.315023	8.040218
6.482233	509.157213	8.045235
6.170118	505.576896	8.050253
6.322813	504.335259	8.055270
6.457150	500.950795	8.060288
5.940281	492.074064	8.065306
6.249222	498.869940	8.070323
6.109786	515.720009	8.075341
6.411514	507.949035	8.080358
6.537890	520.768851	8.085376
6.054915	519.819269	8.090394
6.403372	512.956787	8.095411
6.135477	517.914065	8.100429
6.412162	518.126105	8.105446
6.162440	522.319798	8.110464
6.099891	517.970894	8.115482
5.920724	520.439422	8.120499
6.161268	523.779057	8.125517
6.241552	521.656223	8.130534
6.651855	511.286907	8.135552
6.361947	530.472435	8.140570
6.466665	516.826035	8.145587
6.181882	533.984115	8.150605
6.033532	513.664200	8.155622
6.363741	512.140521	8.160640
6.335422	518.714729	8.165658
6.701930	519.882034	8.170675
6.151261	522.058008	8.175693
6.179547	529.239689	8.180710
6.622675	511.524392	8.185728
6.309895	515.962402	8.190746
6.158056	513.040032	8.195763
6.441679	510.709796	8.200781
6.224585	515.186228	8.205798
6.388602	524.837067	8.210816
6.302156	520.999572	8.215834
6.722050	511.715381	8.220851
6.255403	524.271591	8.225869
6.320854	514.025923	8.230886
6.558846	521.870326	8.235904
6.315166	513.721536	8.240922
6.588597	521.096701	8.245939
6.000340	519.030855	8.250957
6.546930	531.960546	8.255974
6.522878	544.500488	8.260992
6.536311	549.964515	8.266010
6.722988	545.679880	8.271027
6.310931	539.586453	8.276045
6.478003	557.038324	8.281062
6.786637	545.178724	8.286080
6.298991	537.600742	8.291098
6.331065	543.505332	8.296115
6.220450	551.746245	8.301133
6.331168	554.823827	8.306150
6.592725	555.010825	8.311168
6.319595	563.118729	8.316186
6.714691	554.435043	8.321203
6.594675	559.709066	8.326221
6.057121	555.400915	8.331238
6.509551	551.956484	8.336256
6.309247	564.459010	8.341274
6.634354	547.081373	8.346291
6.765054	550.481589	8.351309
6.570768	566.295443	8.356326
6.817525	572.015948	8.361344
6.540936	560.183139	8.366362
6.693585	550.407954	8.371379
6.536750	558.560498	8.376397
6.642234	559.052154	8.381414
6.761941	561.578091	8.386432
6.817054	553.293012	8.391450
6.661296	551.527096	8.396467
6.424086	557.160333	8.401485
6.638121	551.902133	8.406502
6.269209	549.916746	8.411520
6.286412	551.581247	8.416538
6.601349	555.029970	8.421555
6.466785	556.211274	8.426573
6.199947	558.610135	8.431590
6.623238	552.465453	8.436608
6.413666	569.449077	8.441626
6.903151	581.572816	8.446643
6.940570	573.324129	8.451661
6.772398	563.912864	8.456678
6.724970	556.732138	8.461696
6.420534	558.409355	8.466714
6.804084	556.383146	8.471731
6.442095	548.371512	8.476749
6.431570	571.968950	8.481766
6.978496	569.410114	8.486784
6.654755	582.169175	8.491802
6.845084	581.277155	8.496819
6.818022	586.903031	8.501837
6.417043	591.114403	8.506854
6.916614	583.176661	8.511872
6.700514	593.476894	8.516890
6.714179	587.115856	8.521907
6.732902	586.796015	8.526925
6.449660	591.737365	8.531942
6.729574	584.191221	8.536960
6.900581	580.064090	8.541978
7.078596	587.312047	8.546995
7.115606	588.606951	8.552013
6.783245	587.653589	8.557030
7.038218	587.618668	8.562048
6.822457	582.105739	8.567066
7.051195	565.726303	8.572083
6.745008	567.505181	8.577101
6.157250	567.870347	8.582119
6.354408	571.610872	8.587136
6.940561	578.460701	8.592154
6.523757	585.932510	8.597171
6.922244	578.805209	8.602189
6.571475	582.796440	8.607207
6.926857	575.642055	8.612224
6.785777	586.376629	8.617242
6.836426	576.249513	8.622259
6.671025	578.895078	8.627277
6.786811	588.317968	8.632295
7.271863	584.532899	8.637312
6.771079	590.483162	8.642330
7.372945	586.277921	8.647347
7.112885	594.658254	8.652365
6.740419	591.045431	8.657383
6.656370	592.818097	8.662400
6.553765	595.615814	8.667418
6.946214	583.931805	8.672435
6.866058	586.818498	8.677453
6.627824	588.583722	8.682471
7.042288	590.077090	8.687488
6.855995	592.187590	8.692506
7.134204	592.323203	8.697523
6.804056	583.555924	8.702541
6.762646	585.741941	8.707559
7.070893	579.568933	8.712576
6.820538	586.314118	8.717594
6.683506	582.310226	8.722611
6.931186	601.930268	8.727629
7.011980	621.982371	8.732647
7.094802	620.795643	8.737664
7.558909	625.480122	8.742682
7.372365	615.219189	8.747699
7.355390	593.770332	8.752717
6.939750	590.871716	8.757735
7.185280	595.263406	8.762752
6.869373	592.965093	8.767770
7.054502	590.709282	8.772787
7.197404	586.458287	8.777805
7.001912	597.405833	8.782823
6.747611	589.095002	8.787840
6.817175	591.103139	8.792858
6.931962	591.842443	8.797875
7.003636	590.972899	8.802893
6.793990	595.955951	8.807911
6.869997	605.094541	8.812928
7.022886	610.573006	8.817946
7.218717	623.335106	8.822963
7.306316	619.372800	8.827981
7.144535	632.788198	8.832999
7.369436	614.254199	8.838016
6.992690	615.212788	8.843034
7.132136	619.067436	8.848051
6.982933	614.381360	8.853069
7.031994	619.407830	8.858087
7.588589	618.138421	8.863104
7.106945	618.673929	8.868122
7.016499	622.490219	8.873139
7.238038	617.017972	8.878157
7.253333	628.266896	8.883175
7.354349	614.492492	8.888192
6.719612	612.092850	8.893210
7.094442	616.587849	8.898227
7.457727	626.146187	8.903245
7.377533	620.801839	8.908263
7.735382	615.330556	8.913280
7.342540	599.881496	8.918298
7.144119	588.175032	8.923315
7.402010	588.818312	8.928333
7.092540	597.801497	8.933351
7.157740	588.575426	8.938368
6.738820	589.372336	8.943386
6.673682	601.375692	8.948403
7.431033	607.954579	8.953421
7.257550	623.801251	8.958439
7.402488	614.235953	8.963456
7.594076	624.504270	8.968474
7.174628	624.505859	8.973491
7.569262	621.943983	8.978509
7.215855	627.379252	8.983527
7.345418	625.491108	8.988544
7.382259	623.217618	8.993562
7.278384	626.025196	8.998579
7.296383	634.452635	9.003597
7.433553	630.281512	9.008615
7.373221	620.341697	9.013632
7.432795	622.826068	9.018650
7.002134	618.782985	9.023667
7.128484	617.618941	9.028685
7.207158	624.947989	9.033703
7.529618	619.551676	9.038720
7.551332	616.930139	9.043738
7.333951	627.577235	9.048755
7.373617	615.286338	9.053773
7.460658	634.798486	9.058791
7.388085	621.413530	9.063808
7.407704	616.548028	9.068826
7.553769	623.759977	9.073843
7.251450	611.709177	9.078861
7.219718	623.135980	9.083879
7.407437	628.749399	9.088896
7.530325	615.939198	9.093914
7.508575	624.352963	9.098931
7.829272	619.397854	9.103949
7.487567	628.456487	9.108967
7.370816	627.826511	9.113984
7.200213	622.736737	9.119002
7.323937	630.013618	9.124019
7.489569	624.789618	9.129037
7.481356	633.090911	9.134055
7.222870	623.788708	9.139072
7.158841	623.912705	9.144090
7.176922	630.301112	9.149107
6.865878	622.547684	9.154125
7.586459	615.995916	9.159143
7.400130	632.183288	9.164160
7.223038	624.495383	9.169178
7.469260	633.257891	9.174195
7.857858	646.853850	9.179213
7.236674	637.939258	9.184231
7.669762	638.626251	9.189248
7.578566	633.697868	9.194266
7.683554	644.504174	9.199283
7.988292	640.462271	9.204301
7.853969	640.639091	9.209319
7.324807	633.172284	9.214336
7.563114	624.924233	9.219354
7.569164	629.144926	9.224371
7.462087	622.461645	9.229389
7.524272	622.265081	9.234407
7.087011	625.672713	9.239424
7.806650	629.473054	9.244442
7.593445	644.311073	9.249459
7.930331	643.191556	9.254477
7.739766	640.298825	9.259495
7.583211	648.026008	9.264512
7.798669	632.646664	9.269530
7.370868	637.335895	9.274547
7.685350	633.828358	9.279565
7.768668	652.606557	9.284583
7.863065	645.993906	9.289600
7.863532	635.088932	9.294618
7.729754	629.977682	9.299635
7.790253	625.324263	9.304653
7.761910	636.715081	9.309671
7.278023	636.824617	9.314688
7.833450	622.026130	9.319706
7.512200	624.953492	9.324723
7.369688	636.263885	9.329741
7.834712	644.978026	9.334759
7.569501	647.138065	9.339776
7.710885	644.232874	9.344794
7.748332	649.326633	9.349811
7.589914	644.896981	9.354829
7.637803	654.567793	9.359847
7.806469	645.385511	9.364864
8.019083	643.238698	9.369882
7.568011	646.852551	9.374899
7.540613	654.580710	9.379917
7.877745	649.264619	9.384935
7.840511	646.399154	9.389952
7.887282	645.971508	9.394970
8.097123	646.433225	9.399987
7.908449	647.048966	9.405005
7.994467	644.207501	9.410023
7.807826	651.623175	9.415040
7.908693	645.088773	9.420058
7.823771	647.865254	9.425075
7.785913	658.055596	9.430093
7.791615	648.141400	9.435111
7.489930	650.747429	9.440128
7.768572	642.261186	9.445146
7.775706	658.862656	9.450163
7.751030	645.575616	9.455181
7.746433	649.991770	9.460199
7.827720	660.373122	9.465216
8.200224	647.997157	9.470234
7.772604	651.455550	9.475251
7.775338	636.796153	9.480269
8.382683	638.634603	9.485287
7.676281	648.878581	9.490304
7.684339	644.956849	9.495322
7.477754	646.895348	9.500339
7.874782	648.356583	9.505357
7.791295	662.343595	9.510375
7.695769	663.658172	9.515392
7.942246	670.121618	9.520410
8.012832	679.507788	9.525427
7.994920	675.731299	9.530445
8.237909	683.975908	9.535463
7.751637	694.071524	9.540480
8.094953	671.735966	9.545498
8.340031	678.727955	9.550515
8.302478	676.026699	9.555533
8.260296	671.414543	9.560551
8.000639	681.414616	9.565568
8.386797	657.275240	9.570586
8.102759	650.989442	9.575603
8.015226	647.842004	9.580621
8.124091	655.005037	9.585639
7.982230	655.129570	9.590656
8.311426	644.946467	9.595674
7.941811	659.320180	9.600691
7.936877	648.948337	9.605709
8.337274	643.076106	9.610727
8.026352	651.706243	9.615744
8.028994	638.142642	9.620762
8.200681	648.923890	9.625779
7.998493	651.529719	9.630797
8.231068	642.406890	9.635815
7.939239	659.080686	9.640832
8.226945	670.646346	9.645850
8.357980	669.078597	9.650867
7.755383	656.223405	9.655885
8.112435	671.083391	9.660903
7.777276	682.972647	9.665920
8.127985	678.759523	9.670938
8.146301	691.486032	9.675955
8.230693	681.865800	9.680973
8.498885	682.520954	9.685991
8.186516	686.651487	9.691008
8.625781	677.346263	9.696026
8.519939	685.046139	9.701043
8.300308	667.865592	9.706061
8.200324	660.315826	9.711079
8.051168	661.931814	9.716096
8.492599	671.652966	9.721114
8.278417	661.516075	9.726131
8.233029	654.430627	9.731149
8.450739	662.412124	9.736167
8.023607	669.272547	9.741184
8.129041	674.303641	9.746202
8.491999	676.711023	9.751219
8.365266	679.729480	9.756237
8.319914	670.997488	9.761255
8.105808	682.098963	9.766272
8.321627	681.789666	9.771290
8.434939	685.083362	9.776307
8.108610	687.736009	9.781325
8.117816	684.306559	9.786343
8.162618	694.830799	9.791360
8.283118	677.033513	9.796378
8.299960	688.169831	9.801395
8.083778	692.217651	9.806413
8.220249	684.325446	9.811431
8.300699	687.052599	9.816448
8.381646	672.771477	9.821466
8.404872	682.520022	9.826483
8.332842	681.061017	9.831501
8.327790	679.155480	9.836519
8.227047	681.041749	9.841536
8.533454	682.121425	9.846554
8.681480	679.034231	9.851571
8.345307	693.733102	9.856589
8.455409	679.897488	9.861607
8.354922	682.033893	9.866624
8.406190	680.530382	9.871642
8.466669	682.282580	9.876659
8.469050	678.994413	9.881677
8.490289	671.356388	9.886695
8.309940	682.306201	9.891712
8.340246	681.964553	9.896730
8.194093	679.987199	9.901747
8.554288	705.066810	9.906765
8.803568	698.999808	9.911783
8.770403	710.684966	9.916800
8.826824	700.098969	9.921818
8.446375	689.135229	9.926835
8.468226	688.537721	9.931853
8.326600	686.392304	9.936871
8.733438	698.172024	9.941888
8.814295	696.457703	9.946906
8.572324	689.538761	9.951923
8.333336	695.313278	9.956941
8.945199	691.584856	9.961959
8.063786	690.025748	9.966976
8.467799	703.532783	9.971994
8.763409	701.211746	9.977011
8.673970	711.787638	9.982029
8.601951	702.662451	9.987047
8.952275	711.146302	9.992064
8.856190	713.942956	9.997082
9.274241	702.360501	10.002099
8.639602	696.615009	10.007117
8.407006	678.361879	10.012135
8.625510	680.996603	10.017152
8.188629	684.461463	10.022170
8.477820	695.051572	10.027187
8.503946	709.969748	10.032205
8.971451	714.927882	10.037223
8.916129	713.014358	10.042240
8.750213	706.875428	10.047258
8.885575	707.358186	10.052275
8.835149	708.543822	10.057293
8.902994	704.233819	10.062311
8.693632	708.146070	10.067328
8.948639	715.712763	10.072346
8.627263	702.892084	10.077363
8.624678	716.371245	10.082381
8.944079	699.994904	10.087399
8.839400	710.713082	10.092416
8.919384	706.497116	10.097434
8.802674	698.791265	10.102451
8.498458	704.910066	10.107469
8.908535	700.945515	10.112487
8.945115	711.497312	10.117504
8.900135	712.400371	10.122522
9.354764	711.370327	10.127539
8.729721	693.317438	10.132557
8.605343	687.986315	10.137575
8.941001	695.105767	10.142592
8.891562	701.488892	10.147610
9.058474	701.657373	10.152627
8.539886	702.069308	10.157645
8.815624	700.215320	10.162663
9.106421	708.057143	10.167680
8.705014	713.865157	10.172698
9.039287	710.016345	10.177715
8.838448	708.027409	10.182733
8.981998	709.808122	10.187751
8.980383	722.136619	10.192768
8.916935	708.630789	10.197786
9.115074	705.150446	10.202803
9.112423	715.542833	10.207821
9.084611	703.181198	10.212839
9.088621	705.074861	10.217856
9.140452	703.674396	10.222874
9.158825	706.434113	10.227891
9.151279	696.832498	10.232909
9.156379	677.951126	10.237927
8.712016	678.726089	10.242944
8.768886	685.308058	10.247962
9.378696	694.254640	10.252979
8.982141	699.723088	10.257997
9.219703	692.924822	10.263015
9.070359	684.943713	10.268032
8.865717	692.860787	10.273050
9.229432	692.209805	10.278067
9.156513	701.341711	10.283085
9.181893	699.221679	10.288103
8.853062	681.440808	10.293120
9.035745	702.654341	10.298138
9.209589	702.518936	10.303155
9.299114	709.982431	10.308173
9.204175	708.492982	10.313191
9.074374	700.542276	10.318208
8.846827	708.102955	10.323226
9.067567	706.713980	10.328243
9.264312	718.414076	10.333261
9.369296	706.598437	10.338279
9.279800	708.335804	10.343296
8.853557	707.790332	10.348314
9.407113	706.671214	10.353331
9.124105	706.790666	10.358349
9.109887	716.861181	10.363367
9.235181	703.912721	10.368384
8.751227	718.140740	10.373402
8.941037	700.508077	10.378419
8.990898	712.610901	10.383437
9.076283	704.992117	10.388455
9.165705	695.718062	10.393472
9.065893	707.030858	10.398490
9.419938	700.634457	10.403507
8.718181	713.715098	10.408525
9.211580	713.862383	10.413543
9.569580	733.665423	10.418560
9.398138	731.755844	10.423578
9.365645	727.124346	10.428595
9.442196	732.252772	10.433613
9.490930	725.028035	10.438631
9.181815	710.519605	10.443648
9.080555	722.433396	10.448666
9.485180	730.555502	10.453683
9.352959	740.294292	10.458701
9.261059	739.938114	10.463719
9.591946	737.713760	10.468736
9.958745	735.899157	10.473754
9.650568	710.088614	10.478771
9.266889	708.477876	10.483789
9.416503	702.985076	10.488807
9.612961	707.152097	10.493824
9.334798	702.480342	10.498842
9.419766	706.967447	10.503859
9.315671	698.314292	10.508877
9.284978	706.891388	10.513895
9.497138	703.523864	10.518912
9.260570	713.914974	10.523930
9.473832	721.944481	10.528947
9.725495	742.866703	10.533965
9.462411	725.227598	10.538983
9.492946	723.584232	10.544000
9.455964	743.283653	10.549018
9.860180	737.366267	10.554035
9.654801	717.393728	10.559053
9.319157	708.022414	10.564071
9.660261	704.979102	10.569088
9.181845	711.452821	10.574106
9.609884	734.775857	10.579123
9.839703	740.030179	10.584141
9.794700	742.241420	10.589159
9.670497	723.896210	10.594176
9.494831	717.230981	10.599194
9.846079	705.830481	10.604211
9.539884	709.846222	10.609229
9.558868	702.756746	10.614247
9.938490	707.011623	10.619264
9.410515	703.792113	10.624282
9.684081	702.682133	10.629299
9.830045	703.357603	10.634317
9.536411	701.408302	10.639335
9.727106	694.228483	10.644352
9.710423	716.319794	10.649370
9.652557	702.959880	10.654387
9.521323	719.809398	10.659405
9.752733	734.127573	10.664423
9.930602	728.532830	10.669440
10.252579	734.073780	10.674458
9.927576	717.182522	10.679475
9.756668	705.538517	10.684493
9.448123	720.445404	10.689511
9.369608	705.227439	10.694528
9.629788	729.498576	10.699546
9.591798	737.020283	10.704563
9.904149	733.240262	10.709581
9.626122	753.222065	10.714599
10.054504	738.737674	10.719616
9.832886	754.206680	10.724634
9.835649	747.789911	10.729651
9.797938	746.601949	10.734669
9.922056	743.724017	10.739687
10.191520	745.960938	10.744704
9.895434	744.858437	10.749722
10.008982	741.102992	10.754739
9.923178	731.508065	10.759757
9.421171	720.497385	10.764775
9.911988	734.440776	10.769792
9.818623	745.227959	10.774810
10.075174	745.675616	10.779827
9.980931	752.692937	10.784845
9.809241	732.352993	10.789863
10.127839	748.432943	10.794880
9.672067	743.860572	10.799898
9.667183	753.492779	10.804915
9.781385	751.296368	10.809933
9.709947	747.346290	10.814951
9.747067	746.880879	10.819968
9.606398	752.846147	10.824986
9.814820	739.205345	10.830003
9.931966	755.177850	10.835021
9.616194	745.017832	10.840039
9.915136	759.642894	10.845056
10.023436	772.763344	10.850074
10.004547	768.874207	10.855091
10.247252	767.991974	10.860109
9.784243	782.671264	10.865127
10.088530	778.680972	10.870144
10.029554	778.159489	10.875162
10.357660	774.414042	10.880179
10.383582	765.418789	10.885197
9.952864	777.068504	10.890215
10.397192	766.471529	10.895232
10.014952	760.765945	10.900250
9.843270	763.361801	10.905267
10.533140	757.464248	10.910285
10.155649	770.698113	10.915303
10.192835	759.296430	10.920320
9.762194	762.543947	10.925338
10.295744	768.474125	10.930355
10.428392	764.783212	10.935373
10.202488	774.952133	10.940391
10.052657	770.575935	10.945408
10.357449	771.877328	10.950426
10.468095	778.254939	10.955443
10.516402	766.896675	10.960461
10.143469	758.243881	10.965479
10.401854	746.033056	10.970496
10.106058	744.490576	10.975514
9.921081	742.371449	10.980531
10.462318	754.821936	10.985549
10.192571	780.424846	10.990567
10.290787	760.695668	10.995584
10.327340	779.257204	11.000602
10.302623	771.131329	11.005619
10.652077	762.451964	11.010637
10.192501	772.566421	11.015655
10.210731	764.707016	11.020672
10.220755	778.842752	11.025690
10.367454	777.446983	11.030707
10.612713	762.495993	11.035725
10.646144	773.038710	11.040743
10.837477	768.081829	11.045760
10.267342	751.288163	11.050778
10.348639	749.225558	11.055795
10.685767	732.768879	11.060813
10.061039	748.015726	11.065831
10.191573	745.295574	11.070848
10.340166	764.617156	11.075866
10.609180	768.812880	11.080883
10.626902	770.328510	11.085901
10.726622	771.269526	11.090919
10.747702	748.255969	11.095936
10.777976	751.469983	11.100954
10.651110	739.708010	11.105971
10.730264	736.750944	11.110989
10.542762	742.281110	11.116007
10.339129	738.148493	11.121024
10.275419	741.930253	11.126042
10.084593	736.241679	11.131059
10.539442	746.357274	11.136077
10.616873	754.616447	11.141095
10.578968	759.459399	11.146112
10.392730	746.501073	11.151130
10.426697	768.661004	11.156147
10.627204	767.013790	11.161165
10.677915	766.037492	11.166183
10.454529	772.390113	11.171200
10.819844	767.726930	11.176218
10.714936	767.635888	11.181235
10.599756	764.622934	11.186253
10.766367	769.392530	11.191271
11.067432	767.736673	11.196288
10.857904	754.049387	11.201306
10.475731	752.701762	11.206323
10.771748	732.239597	11.211341
10.664684	749.438647	11.216359
10.386935	747.643382	11.221376
11.009568	760.433667	11.226394
10.732233	765.659897	11.231411
10.988739	770.321252	11.236429
10.588808	760.821230	11.241447
11.058924	762.787813	11.246464
10.653980	748.770241	11.251482
10.631985	754.048115	11.256499
10.800710	754.660360	11.261517
10.761799	768.677261	11.266535
10.800791	771.112521	11.271552
10.816464	759.797479	11.276570
10.522199	774.419977	11.281587
11.240183	772.462557	11.286605
11.115849	766.424164	11.291623
10.635678	758.340140	11.296640
10.795921	749.493032	11.301658
10.574998	775.699587	11.306675
10.887743	767.820164	11.311693
10.996559	762.310306	11.316711
10.905089	777.237463	11.321728
10.929891	768.981911	11.326746
10.922433	769.445695	11.331763
11.106424	769.875888	11.336781
10.746954	760.264424	11.341799
10.776725	777.947421	11.346816
10.804194	764.694916	11.351834
10.584506	776.918767	11.356851
10.908643	765.802632	11.361869
10.838196	770.868305	11.366887
10.453758	776.458772	11.371904
10.999772	762.551815	11.376922
10.923036	780.651309	11.381939
10.846368	775.699995	11.386957
11.021470	786.092411	11.391975
10.604422	803.801674	11.396992
10.967678	798.752236	11.402010
10.667420	801.418482	11.407027
11.199378	795.104670	11.412045
10.970666	804.107619	11.417063
10.745777	799.989147	11.422080
10.991242	807.356697	11.427098
10.710975	804.275314	11.432115
11.186244	792.060293	11.437133
11.125661	796.522012	11.442151
10.820382	788.310289	11.447168
11.217463	801.812461	11.452186
11.432821	792.327076	11.457203
10.716314	808.620269	11.462221
11.173665	808.574742	11.467239
11.302382	821.040110	11.472256
11.651036	819.631243	11.477274
11.439445	810.023907	11.482291
11.416585	798.764057	11.487309
11.155551	801.282454	11.492327
10.814273	795.024416	11.497344
11.425125	790.608784	11.502362
11.101048	803.226949	11.507379
11.322023	795.430674	11.512397
11.374681	802.021266	11.517415
11.196287	805.542199	11.522432
11.442481	808.298712	11.527450
11.175112	806.710362	11.532467
11.449348	810.326134	11.537485
11.304733	818.763969	11.542503
11.432884	831.130627	11.547520
11.813404	810.445272	11.552538
11.158796	808.487060	11.557555
11.700460	796.711758	11.562573
11.540522	792.030758	11.567591
11.293211	805.308956	11.572608
11.547216	799.419465	11.577626
11.406155	804.383900	11.582643
11.523161	795.708508	11.587661
11.457688	799.292359	11.592679
11.213467	797.690518	11.597696
11.292332	792.621819	11.602714
11.361320	811.761625	11.607731
11.819455	810.529037	11.612749
11.340633	803.584060	11.617767
11.196215	795.468423	11.622784
11.593651	799.828232	11.627802
11.329965	823.255939	11.632819
11.793492	821.503985	11.637837
11.695282	826.880766	11.642855
11.399700	830.428663	11.647872
11.946224	823.401834	11.652890
11.418636	817.676296	11.657907
11.324591	822.160709	11.662925
11.553411	832.756813	11.667943
11.602124	833.212248	11.672960
12.038829	823.972713	11.677978
11.641141	826.049880	11.682995
11.579800	824.011170	11.688013
11.647629	826.420387	11.693031
11.072003	832.285549	11.698048
11.641292	833.156003	11.703066
11.653109	823.220208	11.708083
11.803193	834.865947	11.713101
11.725935	819.970474	11.718119
11.772169	825.777549	11.723136
11.601253	832.947798	11.728154
11.534169	829.092048	11.733171
11.714753	832.773388	11.738189
11.924705	827.654742	11.743207
11.695379	831.850639	11.748224
11.924702	826.386276	11.753242
11.981340	832.682931	11.758259
12.050295	825.418962	11.763277
11.877859	828.835768	11.768295
11.199789	841.072671	11.773312
11.573227	826.653823	11.778330
11.623870	830.879166	11.783347
11.794156	837.414792	11.788365
11.839527	829.547299	11.793383
11.686462	839.950597	11.798400
11.766785	833.310286	11.803418
11.942797	836.268023	11.808435
11.878485	834.269567	11.813453
11.788100	823.009112	11.818471
11.611996	825.928921	11.823488
11.975208	850.591562	11.828506
12.189739	860.209019	11.833523
12.304271	842.215304	11.838541
12.197240	834.501871	11.843559
11.475027	829.158260	11.848576
11.745407	826.823879	11.853594
11.969372	846.370619	11.858611
11.956261	847.749658	11.863629
11.992188	857.061780	11.868647
11.874725	855.911472	11.873664
12.616596	853.786106	11.878682
12.248023	853.500712	11.883699
12.334381	840.585380	11.888717
12.338462	829.302921	11.893735
11.855560	830.451005	11.898752
12.256977	816.352299	11.903770
12.114522	811.634334	11.908787
11.929176	828.237467	11.913805
11.958402	824.116121	11.918823
12.033860	842.057722	11.923840
12.360923	849.780211	11.928858
12.556014	847.417399	11.933875
12.127803	836.776039	11.938893
12.408803	817.715381	11.943911
12.102919	820.934300	11.948928
11.950708	827.173939	11.953946
12.336833	832.738709	11.958963
12.169797	828.929098	11.963981
12.335536	836.936251	11.968999
12.174820	839.168902	11.974016
12.429669	843.794533	11.979034
12.265878	842.718458	11.984051
12.494014	839.691535	11.989069
12.297253	828.011777	11.994087
12.205301	830.918781	11.999104
12.229877	826.830882	12.004122
12.344975	837.939560	12.009139
12.445591	847.087391	12.014157
12.348758	845.914759	12.019175
12.292142	859.346336	12.024192
12.436366	847.361086	12.029210
12.336042	851.478464	12.034227
12.409041	854.023038	12.039245
12.482910	853.018085	12.044263
12.291089	856.802269	12.049280
12.344751	853.584670	12.054298
12.527143	853.252187	12.059315
12.421168	858.282654	12.064333
12.696496	846.222468	12.069351
12.780961	861.673777	12.074368
12.745295	849.736926	12.079386
12.729756	835.353589	12.084403
12.230885	828.504447	12.089421
12.402386	828.098976	12.094439
12.422455	849.645230	12.099456
12.567491	846.629362	12.104474
12.755862	855.404761	12.109491
12.951665	843.678247	12.114509
12.601258	825.429959	12.119527
12.133875	829.835490	12.124544
12.431741	839.723711	12.129562
12.603073	843.717988	12.134579
12.525211	852.048296	12.139597
12.472417	853.952402	12.144615
12.370488	859.226670	12.149632
12.552153	858.720303	12.154650
12.947191	851.737930	12.159667
12.584738	859.391573	12.164685
13.152697	849.852665	12.169703
12.819559	863.447914	12.174720
12.787530	847.912653	12.179738
12.824841	856.084066	12.184755
12.448684	849.440095	12.189773
12.557271	847.785711	12.194791
12.447216	860.908474	12.199808
12.704257	858.071220	12.204826
12.399211	861.294338	12.209843
12.695109	848.028839	12.214861
13.186944	842.274791	12.219879
12.842380	846.726445	12.224896
12.588352	859.981398	12.229914
12.605958	853.386539	12.234931
12.642506	853.151914	12.239949
12.687929	853.493730	12.244967
12.586183	855.303223	12.249984
12.824827	877.789505	12.255002
13.236883	870.522423	12.260019
12.944115	877.133453	12.265037
12.958317	861.352320	12.270055
12.860046	870.008450	12.275072
12.863573	878.689002	12.280090
13.161982	867.356808	12.285107
13.130073	879.370210	12.290125
13.322852	867.443406	12.295143
12.965568	851.964168	12.300160
12.699956	855.359461	12.305178
12.769226	857.499169	12.310195
12.892714	874.064012	12.315213
12.949985	872.072113	12.320231
12.891822	882.110082	12.325248
12.862839	892.239657	12.330266
13.262746	879.474923	12.335283
12.647412	867.087980	12.340301
13.150851	876.263359	12.345319
13.265434	877.636530	12.350336
13.049419	886.840554	12.355354
13.248838	871.865977	12.360371
13.102110	875.534410	12.365389
13.117533	875.433602	12.370407
13.216917	871.148623	12.375424
13.401452	878.407837	12.380442
13.278135	875.927874	12.385459
12.926896	882.525004	12.390477
12.919122	876.455188	12.395495
13.237045	882.410423	12.400512
13.098346	871.999644	12.405530
13.386347	867.194371	12.410547
12.943008	866.721808	12.415565
12.819466	868.408162	12.420583
13.295757	894.174056	12.425600
13.591859	906.418377	12.430618
13.761266	903.770472	12.435635
13.431855	898.647753	12.440653
13.296932	880.603728	12.445671
13.101451	878.776271	12.450688
13.198909	881.554565	12.455706
13.551224	898.827026	12.460723
13.667402	897.782756	12.465741
13.267374	896.070391	12.470759
13.095572	888.962936	12.475776
13.205567	903.980542	12.480794
13.502217	897.226300	12.485811
13.342132	910.613705	12.490829
13.246081	911.762454	12.495847
13.698221	902.727382	12.500864
13.294390	914.744756	12.505882
13.308624	894.772886	12.510899
13.333090	897.544419	12.515917
13.384639	905.179271	12.520935
13.416503	905.666246	12.525952
13.368635	908.073447	12.530970
13.667417	901.595998	12.535987
13.456039	905.368879	12.541005
13.441335	907.886702	12.546023
13.424415	904.838296	12.551040
13.332188	913.898146	12.556058
13.863018	921.734433	12.561075
13.690226	918.358014	12.566093
13.468920	908.485712	12.571111
13.692648	910.545429	12.576128
13.331460	930.303303	12.581146
13.724806	923.337715	12.586163
13.956934	939.126348	12.591181
13.930212	931.804613	12.596199
14.277805	924.043919	12.601216
13.552920	909.028848	12.606234
13.925242	907.782565	12.611251
13.693675	903.576992	12.616269
13.675514	906.552056	12.621287
13.894299	893.791037	12.626304
13.592257	898.834420	12.631322
13.786358	902.437551	12.636339
13.524385	936.651316	12.641357
14.033380	925.301402	12.646375
14.304563	925.262016	12.651392
13.607420	929.728989	12.656410
14.105687	917.422651	12.661427
13.605749	927.800201	12.666445
13.358360	922.389448	12.671463
13.777767	934.265286	12.676480
13.884016	930.098041	12.681498
13.961215	934.565835	12.686515
14.000990	947.609835	12.691533
13.925835	939.727675	12.696551
14.456887	933.206097	12.701568
14.038910	942.748034	12.706586
14.170946	931.063940	12.711603
14.086493	931.850942	12.716621
13.689742	928.038543	12.721639
13.856678	935.189692	12.726656
13.907672	943.028580	12.731674
14.371067	932.560993	12.736691
14.262704	938.976449	12.741709
14.149043	936.844851	12.746727
14.157442	946.750151	12.751744
13.820570	939.544525	12.756762
13.975807	938.286686	12.761779
14.157921	938.696331	12.766797
13.863474	935.099197	12.771815
14.226621	935.644886	12.776832
13.952517	932.142791	12.781850
14.082525	940.104758	12.786867
14.215956	936.188490	12.791885
14.024703	937.514867	12.796903
14.134163	929.757137	12.801920
13.796959	944.090491	12.806938
14.144061	951.097535	12.811955
14.353408	957.099190	12.816973
14.260182	964.802620	12.821991
14.382675	960.885015	12.827008
14.792543	971.599146	12.832026
14.706143	949.836157	12.837043
14.551234	930.199816	12.842061
14.286895	929.431768	12.847079
14.492797	919.299096	12.852096
14.522600	931.515261	12.857114
14.355757	920.717023	12.862131
14.609282	925.441712	12.867149
14.354938	930.246877	12.872167
14.335322	917.895912	12.877184
14.053797	929.462287	12.882202
14.439415	924.646677	12.887219
14.361958	940.968234	12.892237
14.431739	956.039816	12.897255
14.660730	960.963464	12.902272
14.672680	953.694737	12.907290
14.686273	951.586472	12.912307
15.000023	935.501948	12.917325
14.206222	932.151975	12.922343
14.438594	927.490567	12.927360
14.443520	945.525896	12.932378
14.565389	953.709683	12.937395
14.883859	955.970969	12.942413
14.588180	958.382360	12.947431
14.913493	956.650607	12.952448
14.457358	936.675370	12.957466
14.605034	944.323002	12.962483
14.844504	951.856175	12.967501
14.693387	963.766234	12.972519
14.767095	958.545000	12.977536
14.784061	961.206380	12.982554
14.678904	964.676596	12.987571
14.841926	957.678411	12.992589
14.646500	957.997272	12.997607
14.891973	960.259274	13.002624
14.837667	964.134402	13.007642
14.671472	959.685283	13.012659
14.792065	961.833798	13.017677
14.760796	962.677706	13.022695
14.800673	962.817308	13.027712
14.513531	965.681980	13.032730
14.665933	961.069678	13.037747
15.107522	955.596367	13.042765
14.773748	951.981751	13.047783
14.909057	962.112411	13.052800
15.039586	964.505718	13.057818
14.770066	959.793473	13.062835
14.813202	963.600833	13.067853
14.777939	966.671265	13.072871
14.995875	958.385678	13.077888
15.128171	962.564023	13.082906
14.959027	968.638432	13.087923
14.969958	954.945821	13.092941
14.517744	967.913351	13.097959
14.836052	953.527957	13.102976
15.075307	960.432071	13.107994
15.084084	980.919027	13.113011
15.054756	974.996842	13.118029
15.214296	981.563447	13.123047
15.395005	986.653387	13.128064
15.173102	965.572310	13.133082
14.923298	965.728565	13.138099
14.981898	971.286015	13.143117
15.304466	995.706050	13.148135
15.197417	981.325189	13.153152
15.504399	988.882196	13.158170
15.312222	980.132112	13.163187
15.378377	963.406464	13.168205
15.374730	970.845416	13.173223
15.175944	961.271683	13.178240
15.452513	974.111791	13.183258
15.201890	956.703409	13.188275
15.173433	955.836315	13.193293
14.838216	958.549930	13.198311
14.909913	971.037100	13.203328
15.174083	981.626250	13.208346
15.197704	985.360485	13.213363
15.500676	991.982778	13.218381
15.181446	1002.028390	13.223399
15.495922	995.043203	13.228416
15.282448	996.568542	13.233434
14.884266	993.965749	13.238451
15.442793	981.518250	13.243469
15.426421	995.169621	13.248487
15.209228	986.712258	13.253504
15.266829	988.365368	13.258522
15.311852	989.950887	13.263539
15.619420	989.608619	13.268557
15.719800	1019.196840	13.273575
15.806201	1007.174623	13.278592
15.788203	996.835426	13.283610
15.576822	981.802649	13.288627
16.008761	981.072801	13.293645
15.410563	987.330727	13.298663
15.607523	979.910772	13.303680
15.637523	984.815930	13.308698
15.544834	992.661796	13.313715
15.673569	977.694141	13.318733
15.216090	987.162754	13.323751
15.879221	1000.772449	13.328768
15.805177	1006.184644	13.333786
15.753933	1004.462719	13.338803
15.707269	987.515258	13.343821
15.651795	999.533457	13.348839
15.968008	1005.537053	13.353856
15.703892	1006.021260	13.358874
15.853244	1015.594532	13.363891
16.069884	1016.285433	13.368909
15.813670	1001.928952	13.373927
15.546627	999.516948	13.378944
15.805906	1006.362640	13.383962
15.773679	1020.769385	13.388979
16.437607	1022.656352	13.393997
15.864090	1004.902784	13.399015
15.796030	993.280245	13.404032
15.796104	1003.688514	13.409050
15.747779	1017.623547	13.414067
16.207744	1010.448433	13.419085
15.848863	1015.229268	13.424103
15.951402	1021.147130	13.429120
16.210089	1015.184933	13.434138
15.914802	1014.768463	13.439155
16.148473	1012.923989	13.444173
16.052422	1021.718411	13.449191
16.006919	1023.091826	13.454208
16.255255	1020.383541	13.459226
16.135996	1016.531298	13.464243
16.196738	1013.744751	13.469261
15.902058	1016.233934	13.474279
15.933181	1026.768940	13.479296
16.146888	1017.243930	13.484314
15.776937	1018.397662	13.489331
16.220853	1014.821876	13.494349
16.115946	1019.186111	13.499367
15.800784	1019.559517	13.504384
16.358485	1018.248952	13.509402
16.270585	1019.155816	13.514419
16.171375	1022.538841	13.519437
16.407660	1021.515543	13.524455
16.259346	1021.843896	13.529472
16.412409	1016.870857	13.534490
16.134586	1023.779843	13.539507
16.177373	1025.566908	13.544525
16.285771	1028.344198	13.549543
15.854348	1028.292856	13.554560
16.051217	1023.879434	13.559578
16.158079	1046.196534	13.564595
16.279110	1047.046235	13.569613
16.530698	1051.203203	13.574631
16.867339	1058.449031	13.579648
16.500159	1058.909033	13.584666
16.512426	1052.435443	13.589683
16.750841	1041.173328	13.594701
16.620971	1040.011683	13.599719
16.342864	1022.170416	13.604736
16.369666	1023.953445	13.609754
16.682878	1039.285420	13.614771
16.682148	1036.886231	13.619789
16.727970	1034.713153	13.624807
16.373701	1034.735203	13.629824
16.641356	1031.441846	13.634842
16.391812	1042.356565	13.639859
16.848775	1047.700202	13.644877
16.708565	1055.831937	13.649895
16.828171	1041.628298	13.654912
17.016329	1030.972939	13.659930
16.717750	1036.817718	13.664947
16.561611	1017.129113	13.669965
16.640903	1020.978506	13.674983
16.270455	1022.246488	13.680000
16.770304	1035.919965	13.685018
16.520087	1053.592335	13.690035
16.684261	1037.202661	13.695053
16.576070	1051.324044	13.700071
16.130597	1053.115890	13.705088
16.574757	1037.696952	13.710106
16.365564	1059.188300	13.715123
16.842905	1058.199341	13.720141
17.070619	1070.801205	13.725159
17.213223	1069.881265	13.730176
17.277775	1049.848866	13.735194
17.118058	1045.460848	13.740211
17.103592	1047.299555	13.745229
16.933238	1050.105070	13.750247
16.801196	1050.641339	13.755264
16.791778	1042.918664	13.760282
16.871249	1049.365542	13.765299
16.687701	1054.632182	13.770317
17.120056	1066.982325	13.775335
17.068131	1086.691359	13.780352
17.329916	1070.299600	13.785370
17.146448	1076.718934	13.790387
16.761218	1076.159151	13.795405
17.390353	1082.001324	13.800423
17.437763	1081.565687	13.805440
17.330380	1061.631531	13.810458
17.083976	1065.876390	13.815475
16.915732	1056.878201	13.820493
16.955544	1073.373705	13.825511
16.997985	1084.610379	13.830528
17.576453	1083.075502	13.835546
17.015230	1087.805741	13.840563
17.083183	1089.712247	13.845581
17.425127	1084.780625	13.850599
17.286017	1089.970210	13.855616
17.245962	1074.163234	13.860634
17.236433	1086.370311	13.865651
17.412775	1080.232021	13.870669
17.321906	1075.118806	13.875687
17.007449	1085.896320	13.880704
17.532391	1087.690259	13.885722
17.290321	1093.652434	13.890739
17.191024	1078.680458	13.895757
17.165481	1087.101797	13.900775
17.253580	1085.257890	13.905792
17.268414	1079.675945	13.910810
17.337012	1088.253284	13.915827
17.095243	1096.631043	13.920845
17.546991	1106.691094	13.925863
17.363537	1114.045832	13.930880
17.834806	1110.786330	13.935898
17.683068	1110.246002	13.940915
17.720291	1110.264792	13.945933
17.818293	1105.526850	13.950951
17.712962	1104.477652	13.955968
17.565176	1101.454894	13.960986
17.651485	1107.104634	13.966003
18.065715	1101.658653	13.971021
17.591021	1088.115926	13.976039
17.220759	1106.311433	13.981056
17.599258	1092.530839	13.986074
17.909251	1101.269629	13.991091
17.854143	1103.807191	13.996109
18.038780	1100.720129	14.001127
17.847276	1112.938575	14.006144
17.738221	1094.262077	14.011162
17.845018	1102.336642	14.016179
17.766315	1097.913885	14.021197
17.986592	1104.255497	14.026215
17.870027	1108.113843	14.031232
18.105164	1096.401073	14.036250
18.068744	1110.149180	14.041267
18.090458	1106.573077	14.046285
18.311233	1099.091629	14.051303
17.971878	1095.636561	14.056320
17.937158	1087.045276	14.061338
17.631953	1084.758494	14.066355
17.395638	1093.158572	14.071373
17.767919	1086.567654	14.076391
17.662449	1106.126565	14.081408
17.838873	1089.983607	14.086426
17.769871	1100.186108	14.091443
17.793577	1102.518454	14.096461
17.987894	1091.455749	14.101479
17.968834	1113.961192	14.106496
18.492280	1123.763680	14.111514
18.226139	1116.791873	14.116531
17.942440	1108.055746	14.121549
18.241665	1112.712664	14.126567
18.232184	1132.496981	14.131584
18.152853	1130.618300	14.136602
18.259236	1139.001994	14.141619
17.677945	1138.755884	14.146637
18.124844	1134.810694	14.151655
17.903773	1142.422867	14.156672
17.887909	1143.511064	14.161690
17.856327	1145.783711	14.166707
18.152500	1141.995848	14.171725
18.669765	1153.195778	14.176743
18.560606	1147.108062	14.181760
18.372817	1139.672849	14.186778
18.417993	1129.234878	14.191795
18.245515	1137.168484	14.196813
18.606256	1125.116326	14.201831
18.587297	1129.619450	14.206848
18.541508	1119.631231	14.211866
18.575516	1136.952139	14.216883
18.389871	1130.731873	14.221901
18.503356	1128.990822	14.226919
18.352899	1131.928078	14.231936
18.470424	1144.784133	14.236954
18.677655	1156.230860	14.241971
18.828590	1153.529294	14.246989
18.815152	1147.434330	14.252007
18.613210	1133.713559	14.257024
18.587873	1135.448576	14.262042
19.176412	1124.400244	14.267059
18.632531	1131.215708	14.272077
18.709101	1136.002549	14.277095
18.787946	1128.100209	14.282112
18.579187	1132.037661	14.287130
18.798128	1133.710819	14.292147
18.508456	1136.254303	14.297165
18.498924	1142.092418	14.302183
18.353910	1158.774236	14.307200
18.681723	1164.103161	14.312218
18.704450	1162.179168	14.317235
18.789806	1164.492616	14.322253
19.062820	1157.865413	14.327271
18.942797	1167.918966	14.332288
18.725429	1158.126555	14.337306
18.710277	1158.772528	14.342323
18.694432	1163.019642	14.347341
18.881416	1164.664258	14.352359
18.962817	1165.320167	14.357376
19.106566	1165.855481	14.362394
19.076983	1155.855884	14.367411
19.148004	1174.470626	14.372429
19.321035	1151.356810	14.377447
19.176938	1162.825322	14.382464
18.848375	1163.413941	14.387482
18.988473	1162.469217	14.392499
19.056854	1169.465996	14.397517
18.981683	1176.583483	14.402535
18.975942	1193.570524	14.407552
19.349831	1200.804324	14.412570
19.661802	1200.813275	14.417587
19.217700	1198.604677	14.422605
19.527546	1176.333797	14.427623
19.640638	1174.872716	14.432640
19.095953	1161.547454	14.437658
19.061522	1163.992618	14.442675
19.286352	1170.768521	14.447693
19.427696	1166.980797	14.452711
19.436376	1176.460625	14.457728
19.582324	1166.652703	14.462746
19.803242	1171.707283	14.467763
19.341304	1165.922279	14.472781
19.178127	1169.005744	14.477799
19.148487	1168.017186	14.482816
19.446922	1188.535404	14.487834
19.996663	1183.364892	14.492851
19.711183	1173.498362	14.497869
19.242444	1178.973855	14.502887
19.267550	1169.941497	14.507904
19.448610	1179.287562	14.512922
20.042229	1192.420418	14.517939
19.392281	1177.619785	14.522957
19.878438	1169.659569	14.527975
19.389290	1167.810022	14.532992
19.200286	1178.788000	14.538010
19.719837	1187.166432	14.543027
19.221581	1187.323826	14.548045
19.452023	1191.014681	14.553063
19.604404	1188.990792	14.558080
19.352795	1197.929273	14.563098
19.655532	1196.629970	14.568115
19.453111	1197.019679	14.573133
19.810465	1199.345797	14.578151
19.598957	1193.422312	14.583168
19.604399	1202.390117	14.588186
19.909089	1207.376850	14.593203
19.867964	1217.095680	14.598221
20.109536	1220.817762	14.603239
20.096625	1217.749731	14.608256
19.840277	1212.510830	14.613274
19.800766	1209.266126	14.618291
19.964023	1215.307825	14.623309
19.943657	1211.103677	14.628327
20.200371	1215.789738	14.633344
20.043081	1218.240369	14.638362
20.243650	1221.614949	14.643379
20.152973	1226.727241	14.648397
20.298924	1218.827874	14.653415
19.815175	1210.071398	14.658432
19.989610	1211.287020	14.663450
20.161452	1216.752117	14.668467
19.813356	1224.303556	14.673485
20.185274	1226.876853	14.678503
20.346100	1230.227727	14.683520
19.598403	1227.107022	14.688538
20.110712	1220.961261	14.693555
19.708106	1222.493648	14.698573
20.085460	1218.105683	14.703591
20.108869	1220.568800	14.708608
19.951405	1219.138510	14.713626
20.388676	1232.658396	14.718643
20.500272	1255.458063	14.723661
20.810207	1253.454435	14.728679
20.520881	1231.246056	14.733696
20.407925	1238.238754	14.738714
20.162981	1228.789845	14.743731
20.307221	1230.495114	14.748749
20.607115	1248.805774	14.753767
20.538228	1262.657440	14.758784
20.674467	1256.088360	14.763802
20.887776	1243.666929	14.768819
20.481494	1233.236602	14.773837
20.509289	1222.041251	14.778855
20.773844	1217.397636	14.783872
20.678120	1216.131487	14.788890
20.684040	1217.043634	14.793907
20.321630	1216.320216	14.798925
20.151375	1228.215155	14.803943
20.661435	1236.316069	14.808960
20.778294	1246.996418	14.813978
20.742236	1254.775132	14.818995
20.528091	1256.988771	14.824013
20.196356	1252.182057	14.829031
20.453117	1243.728847	14.834048
20.549593	1251.825283	14.839066
20.578650	1247.961323	14.844083
20.633746	1243.531640	14.849101
20.960079	1249.513965	14.854119
20.740846	1242.224868	14.859136
20.676478	1253.692400	14.864154
21.210313	1263.065313	14.869171
21.211748	1260.892888	14.874189
20.943199	1258.837774	14.879207
21.390042	1242.239885	14.884224
20.879095	1251.418343	14.889242
20.958532	1250.589204	14.894259
21.098173	1254.482166	14.899277
20.739900	1251.314448	14.904295
20.750310	1250.842438	14.909312
21.379855	1265.010291	14.914330
21.348129	1266.224750	14.919347
21.568856	1254.359537	14.924365
21.306053	1248.698091	14.929383
21.598529	1257.214299	14.934400
21.205273	1242.663055	14.939418
21.274657	1242.402495	14.944435
21.241472	1251.246831	14.949453
21.214685	1253.584837	14.954471
21.564979	1246.533350	14.959488
21.435970	1246.930544	14.964506
21.441056	1249.107351	14.969523
21.232737	1253.329789	14.974541
21.277184	1245.909861	14.979559
21.670456	1243.545939	14.984576
21.304548	1238.556727	14.989594
21.582912	1244.866696	14.994611
21.370320	1237.713105	14.999629
21.488216	1246.824838	15.004647
21.521742	1243.520351	15.009664
21.459041	1252.143225	15.014682
21.595396	1240.617624	15.019699
21.633398	1236.269521	15.024717
21.583956	1253.170193	15.029735
21.501661	1246.857510	15.034752
21.131037	1246.782281	15.039770
21.332723	1243.686451	15.044787
21.607693	1246.213663	15.049805
21.117978	1251.272211	15.054823
21.402106	1246.297393	15.059840
21.473040	1274.608367	15.064858
21.526613	1273.124100	15.069875
21.615352	1278.281389	15.074893
21.998153	1284.133481	15.079911
22.013960	1277.714719	15.084928
21.484313	1278.248971	15.089946
21.814088	1284.438211	15.094963
22.292449	1270.451498	15.099981
21.595899	1280.347016	15.104999
21.856730	1273.062365	15.110016
21.756767	1273.755508	15.115034
21.688189	1276.620916	15.120051
21.756945	1282.731101	15.125069
21.630283	1286.266378	15.130087
21.904222	1269.000373	15.135104
21.867891	1282.930895	15.140122
21.951693	1278.356278	15.145139
22.296788	1286.834231	15.150157
22.219008	1291.528667	15.155175
21.854289	1281.867751	15.160192
22.149774	1299.850082	15.165210
22.198160	1299.213102	15.170227
22.339312	1305.919118	15.175245
22.372064	1296.137802	15.180263
22.163031	1275.623042	15.185280
22.038072	1271.158319	15.190298
22.354188	1277.963190	15.195315
22.342835	1268.708889	15.200333
22.081290	1267.515177	15.205351
22.707080	1279.093210	15.210368
22.165356	1269.553843	15.215386
22.166255	1270.743196	15.220403
22.545439	1278.889112	15.225421
22.510442	1281.554459	15.230439
22.406175	1276.017828	15.235456
22.530312	1272.805753	15.240474
22.627036	1273.833515	15.245491
22.793813	1271.038747	15.250509
22.580961	1280.852692	15.255527
22.677641	1268.241971	15.260544
22.358890	1273.079598	15.265562
22.396775	1266.041445	15.270579
22.233022	1267.124310	15.275597
22.151296	1285.766541	15.280615
22.645358	1295.166557	15.285632
22.635132	1303.966557	15.290650
22.643931	1297.011175	15.295667
22.830348	1309.401995	15.300685
22.573223	1309.477975	15.305703
22.728922	1300.199827	15.310720
22.659176	1307.701893	15.315738
22.629497	1308.045966	15.320755
22.709201	1304.582222	15.325773
22.608552	1302.807453	15.330791
22.644434	1302.947329	15.335808
22.356166	1307.179526	15.340826
22.494911	1304.145719	15.345843
22.820220	1314.235976	15.350861
22.970296	1327.501325	15.355879
23.105912	1340.046671	15.360896
23.151711	1329.304141	15.365914
22.752729	1317.048194	15.370931
22.912799	1322.503869	15.375949
23.229128	1330.263815	15.380967
23.021211	1332.917754	15.385984
22.936778	1332.391822	15.391002
23.016620	1328.400508	15.396019
23.274973	1329.335271	15.401037
23.379114	1330.601561	15.406055
23.340676	1330.828590	15.411072
23.164566	1322.903567	15.416090
22.970616	1333.401389	15.421107
23.538758	1325.230230	15.426125
23.253047	1330.047816	15.431143
23.493450	1326.943173	15.436160
23.586004	1331.421915	15.441178
23.211987	1319.588181	15.446195
23.408667	1312.605502	15.451213
23.174377	1339.917753	15.456231
23.276698	1327.366674	15.461248
23.314539	1319.120276	15.466266
23.123314	1322.620624	15.471283
23.831332	1317.990279	15.476301
23.140178	1324.482284	15.481319
23.437221	1319.389158	15.486336
23.437076	1325.984419	15.491354
23.310464	1324.342305	15.496371
23.166717	1317.743753	15.501389
23.292685	1315.582117	15.506407
23.361152	1321.175059	15.511424
23.511921	1319.367163	15.516442
23.248938	1343.936642	15.521459
23.455444	1340.871881	15.526477
23.872658	1346.543873	15.531495
23.984299	1352.704043	15.536512
24.277325	1346.686802	15.541530
24.271845	1338.734986	15.546547
24.209361	1317.701340	15.551565
23.640107	1324.687241	15.556583
23.403387	1317.113622	15.561600
23.539398	1312.166944	15.566618
23.568366	1335.532413	15.571635
23.813777	1336.952778	15.576653
23.724514	1348.525695	15.581671
23.956593	1354.846158	15.586688
24.086724	1348.928429	15.591706
23.931659	1350.231896	15.596723
23.776652	1347.624056	15.601741
23.760454	1345.074247	15.606759
23.883216	1348.727920	15.611776
24.034301	1351.541480	15.616794
23.626800	1352.827849	15.621811
23.746679	1344.592211	15.626829
23.984696	1357.215431	15.631847
24.141775	1360.191770	15.636864
24.397771	1358.963213	15.641882
24.454316	1361.583045	15.646899
24.908538	1359.955017	15.651917
24.480718	1351.861584	15.656935
24.419896	1348.711335	15.661952
24.105100	1334.483174	15.666970
24.272641	1342.007234	15.671987
24.491763	1334.492879	15.677005
24.379310	1348.689647	15.682023
24.534062	1331.285513	15.687040
24.594858	1331.927531	15.692058
24.329522	1339.339683	15.697075
24.455005	1327.077659	15.702093
24.322036	1336.977571	15.707111
24.316154	1344.297392	15.712128
24.629976	1350.120818	15.717146
24.496257	1354.145851	15.722163
24.749833	1369.652234	15.727181
24.753181	1370.636863	15.732199
24.537667	1368.224110	15.737216
24.952374	1368.136856	15.742234
24.624417	1356.635191	15.747251
24.676561	1360.186828	15.752269
24.524558	1360.357144	15.757287
24.610315	1370.992750	15.762304
24.832411	1366.621887	15.767322
24.692258	1370.831453	15.772339
25.068285	1366.875151	15.777357
24.873012	1367.581777	15.782375
24.436558	1380.857257	15.787392
24.832160	1365.092534	15.792410
24.670679	1374.523995	15.797427
24.583442	1369.001824	15.802445
24.927827	1378.244489	15.807463
24.589610	1370.176310	15.812480
24.964122	1369.472527	15.817498
25.289181	1383.772984	15.822515
25.029960	1377.138088	15.827533
25.571379	1369.940217	15.832551
25.262132	1375.352263	15.837568
25.137508	1369.102074	15.842586
25.017909	1374.361737	15.847603
25.118413	1370.940189	15.852621
25.060158	1373.144471	15.857639
25.107022	1376.089133	15.862656
25.191698	1386.448952	15.867674
25.176077	1403.742581	15.872691
25.358555	1406.169447	15.877709
25.407081	1403.726190	15.882727
25.439320	1416.399406	15.887744
25.225680	1403.176784	15.892762
25.447985	1406.141110	15.897779
25.305412	1395.528265	15.902797
25.554926	1392.648860	15.907815
25.309939	1397.914411	15.912832
25.679781	1387.394748	15.917850
25.297150	1393.706373	15.922867
25.383278	1395.492183	15.927885
25.828289	1391.886605	15.932903
25.614530	1396.056050	15.937920
25.671353	1396.023947	15.942938
25.481290	1399.991429	15.947955
25.904455	1392.830130	15.952973
25.559151	1389.440548	15.957991
25.616814	1396.105362	15.963008
25.935975	1386.193713	15.968026
25.335991	1396.062625	15.973043
25.323644	1387.995786	15.978061
25.512845	1386.292909	15.983079
25.350311	1400.186246	15.988096
25.870519	1416.842029	15.993114
25.812051	1431.479888	15.998131
25.945395	1417.507082	16.003149
25.840613	1427.092139	16.008167
26.075757	1431.323595	16.013184
26.065474	1416.942388	16.018202
26.226460	1426.113597	16.023219
26.271307	1423.508354	16.028237
26.446267	1429.039543	16.033255
26.189222	1422.293639	16.038272
26.109115	1418.717064	16.043290
26.026671	1421.231663	16.048307
26.178480	1420.083015	16.053325
26.322084	1416.065726	16.058343
26.011868	1416.250134	16.063360
26.436333	1413.496368	16.068378
25.987322	1422.204407	16.073395
26.031809	1422.375924	16.078413
26.513010	1417.810018	16.083431
25.932485	1429.110324	16.088448
26.236367	1414.618244	16.093466
26.213802	1417.252414	16.098483
26.349630	1421.193296	16.103501
26.496100	1429.089395	16.108519
26.362767	1422.327653	16.113536
26.415050	1417.061009	16.118554
26.167166	1417.790554	16.123571
26.487681	1440.573093	16.128589
26.686010	1444.485877	16.133607
26.617996	1449.042914	16.138624
26.847969	1446.765551	16.143642
26.775584	1453.482712	16.148659
26.959498	1443.536420	16.153677
26.688786	1431.995264	16.158695
26.459621	1422.849118	16.163712
26.622003	1429.905980	16.168730
26.623460	1444.912229	16.173747
26.502703	1458.620726	16.178765
26.593034	1449.894679	16.183783
26.530758	1456.913697	16.188800
26.650592	1446.837112	16.193818
26.407308	1451.752406	16.198835
26.578361	1453.641428	16.203853
26.573656	1450.251915	16.208871
26.873059	1475.060800	16.213888
27.271299	1471.562975	16.218906
27.528384	1467.734682	16.223923
27.417723	1465.825341	16.228941
27.256009	1445.324932	16.233959
27.324287	1437.182071	16.238976
27.547328	1440.947837	16.243994
27.509550	1435.073335	16.249011
27.249780	1449.028151	16.254029
27.489471	1440.634363	16.259047
27.496658	1447.915054	16.264064
27.566714	1435.802704	16.269082
27.555405	1441.143995	16.274099
27.307075	1445.733756	16.279117
27.707585	1423.817523	16.284135
27.599702	1439.056501	16.289152
27.386747	1436.904723	16.294170
27.564189	1430.388956	16.299187
27.411367	1429.565340	16.304205
27.721500	1431.425338	16.309223
27.511190	1425.584634	16.314240
27.309828	1416.386233	16.319258
27.538046	1421.870774	16.324275
27.354117	1438.216062	16.329293
27.407147	1440.106982	16.334311
27.381421	1444.022753	16.339328
27.468417	1441.626638	16.344346
27.559995	1436.431013	16.349363
27.671193	1434.340318	16.354381
27.798605	1437.646004	16.359399
27.661324	1450.569859	16.364416
27.409265	1438.496871	16.369434
27.734094	1428.608662	16.374451
27.502469	1433.706653	16.379469
27.936415	1445.281265	16.384487
27.915881	1469.699626	16.389504
28.161503	1463.477625	16.394522
28.282017	1466.398647	16.399539
28.026416	1459.689887	16.404557
27.776846	1445.120476	16.409575
27.789834	1458.274080	16.414592
28.399073	1458.940302	16.419610
28.341082	1475.405246	16.424627
28.385181	1460.546466	16.429645
28.188227	1438.292515	16.434663
28.163126	1443.492796	16.439680
28.233160	1439.702685	16.444698
28.286434	1433.573687	16.449715
27.510568	1440.251467	16.454733
27.989860	1454.839734	16.459751
27.830783	1460.944157	16.464768
28.522012	1462.017215	16.469786
28.355979	1463.996514	16.474803
28.189629	1472.512329	16.479821
28.310919	1465.012991	16.484839
28.310836	1472.470488	16.489856
28.036863	1469.054072	16.494874
28.457084	1476.883044	16.499891
28.644652	1487.220319	16.504909
29.467177	1462.452850	16.509927
29.279719	1457.366585	16.514944
29.424940	1465.247556	16.519962
29.223854	1438.734155	16.524979
28.903184	1422.554575	16.529997
29.099274	1410.417754	16.535015
29.150344	1418.148212	16.540032
28.777700	1409.953848	16.545050
29.183527	1406.760673	16.550067
28.447805	1411.578276	16.555085
28.946349	1409.751150	16.560103
28.800935	1417.146557	16.565120
28.580222	1396.465078	16.570138
28.882091	1402.879470	16.575155
29.047356	1410.673620	16.580173
29.034959	1407.143667	16.585191
28.932337	1404.529079	16.590208
28.920797	1408.307054	16.595226
29.141614	1405.882404	16.600243
28.684161	1406.651504	16.605261
28.971652	1423.695964	16.610279
29.129724	1432.505467	16.615296
28.889870	1442.099991	16.620314
29.251589	1438.480687	16.625331
29.113774	1442.648940	16.630349
29.058537	1437.089930	16.635367
29.265045	1441.364730	16.640384
29.305275	1441.611756	16.645402
29.208768	1443.756658	16.650419
29.221760	1441.285837	16.655437
29.375516	1430.815838	16.660455
29.446639	1431.113633	16.665472
29.388197	1434.553749	16.670490
29.031426	1439.921749	16.675507
29.080527	1442.347954	16.680525
29.612650	1450.847668	16.685543
29.635726	1458.280444	16.690560
29.525668	1465.655037	16.695578
29.660897	1461.581650	16.700595
29.653245	1467.438866	16.705613
29.737823	1476.356669	16.710631
29.645018	1472.892032	16.715648
29.303981	1473.226835	16.720666
29.581576	1469.564420	16.725683
29.644557	1477.418122	16.730701
29.726886	1471.574431	16.735719
29.802376	1472.587233	16.740736
29.842945	1473.915674	16.745754
30.002946	1476.297076	16.750771
29.556097	1480.122615	16.755789
29.777933	1475.198628	16.760807
29.730928	1478.204186	16.765824
29.785348	1475.121369	16.770842
29.916400	1483.752326	16.775859
29.906055	1487.313984	16.780877
29.977494	1492.233281	16.785895
29.759618	1503.908791	16.790912
29.644697	1502.714706	16.795930
29.705060	1501.464323	16.800947
30.052857	1503.641686	16.805965
30.284089	1516.677179	16.810983
30.397321	1518.838806	16.816000
30.428309	1528.308449	16.821018
30.789066	1521.688557	16.826035
30.611567	1508.204330	16.831053
30.535837	1494.805561	16.836071
30.344409	1488.719967	16.841088
30.387354	1486.448487	16.846106
30.625486	1478.510834	16.851123
30.896448	1488.409456	16.856141
30.799615	1484.671476	16.861159
30.857216	1486.651010	16.866176
30.540844	1497.423220	16.871194
30.674838	1486.297821	16.876211
30.470421	1492.242079	16.881229
30.581321	1484.230295	16.886247
30.922231	1485.368272	16.891264
30.466479	1488.972069	16.896282
30.499815	1483.408558	16.901299
30.611749	1492.318281	16.906317
30.585322	1502.396256	16.911335
30.929091	1516.416568	16.916352
30.823980	1514.381891	16.921370
30.736651	1521.107471	16.926387
30.882315	1514.613880	16.931405
30.964043	1510.637165	16.936423
31.229059	1507.869728	16.941440
30.773329	1513.990011	16.946458
31.069219	1517.675973	16.951475
31.235509	1519.137457	16.956493
31.427488	1520.566326	16.961511
31.389516	1519.128352	16.966528
31.277556	1516.952690	16.971546
31.512047	1522.502365	16.976563
31.539646	1517.025620	16.981581
31.322114	1525.625954	16.986599
31.548350	1521.371681	16.991616
31.249219	1516.219707	16.996634
31.277383	1517.536828	17.001651
31.339636	1511.512604	17.006669
31.175337	1525.204775	17.011687
31.478132	1508.547476	17.016704
31.150506	1513.420902	17.021722
31.590219	1510.214201	17.026739
31.182261	1527.784589	17.031757
31.222372	1513.869316	17.036775
31.391559	1517.318074	17.041792
31.139513	1520.198272	17.046810
31.818902	1534.130142	17.051827
31.109430	1536.453309	17.056845
31.454062	1549.486124	17.061863
31.913366	1541.779785	17.066880
31.559144	1553.159101	17.071898
31.737436	1548.869089	17.076915
31.973544	1549.101671	17.081933
32.046513	1548.197215	17.086951
32.062708	1550.116711	17.091968
31.679470	1546.488915	17.096986
31.870257	1541.754316	17.102003
31.797747	1544.195632	17.107021
31.728515	1553.144949	17.112039
32.163607	1556.944397	17.117056
32.206616	1576.570953	17.122074
32.199415	1575.368013	17.127091
32.366975	1573.632100	17.132109
32.611397	1574.338883	17.137127
32.414825	1564.249455	17.142144
32.248089	1553.900356	17.147162
32.080929	1541.643494	17.152179
32.165395	1556.789596	17.157197
32.296197	1562.295495	17.162215
32.532307	1566.031955	17.167232
32.042718	1569.257936	17.172250
32.396148	1578.207885	17.177267
32.321512	1576.218528	17.182285
32.379102	1567.696279	17.187303
32.732749	1569.305760	17.192320
32.415964	1572.730183	17.197338
32.668688	1578.389050	17.202355
32.875706	1572.653336	17.207373
32.671025	1569.750176	17.212391
32.766667	1564.138485	17.217408
32.421900	1570.751757	17.222426
32.962223	1569.075935	17.227443
32.848909	1571.181523	17.232461
32.585232	1579.886405	17.237479
32.717876	1572.083557	17.242496
32.808037	1575.095076	17.247514
32.817917	1577.658134	17.252531
32.604264	1576.872966	17.257549
32.808099	1588.709549	17.262567
32.771504	1590.923253	17.267584
32.876021	1597.048484	17.272602
32.969569	1599.709844	17.277619
32.837378	1600.134345	17.282637
32.994395	1605.767004	17.287655
33.293894	1593.151837	17.292672
33.150068	1597.816792	17.297690
33.303999	1593.461920	17.302707
33.588832	1587.769959	17.307725
33.519377	1589.405275	17.312743
33.572874	1594.736242	17.317760
33.840996	1593.643445	17.322778
33.416055	1599.961791	17.327795
33.685631	1597.940026	17.332813
33.605067	1588.357672	17.337831
33.701265	1584.135230	17.342848
33.729430	1586.088961	17.347866
33.463797	1587.874597	17.352883
33.555378	1590.966590	17.357901
33.484760	1595.959529	17.362919
33.529324	1583.904450	17.367936
33.364859	1591.150351	17.372954
33.236695	1595.672941	17.377971
33.763012	1591.313658	17.382989
33.438917	1588.917735	17.388007
33.731449	1593.235367	17.393024
33.560924	1604.562930	17.398042
33.873709	1615.810962	17.403059
34.068129	1611.312744	17.408077
34.281061	1618.614437	17.413095
34.442994	1604.686316	17.418112
34.209395	1601.286782	17.423130
34.236997	1592.936036	17.428147
33.795389	1581.153490	17.433165
34.118675	1594.660750	17.438183
34.416405	1606.086078	17.443200
34.361469	1601.024590	17.448218
34.352689	1599.984507	17.453235
34.304481	1581.859898	17.458253
33.911050	1587.291126	17.463271
34.206373	1592.163797	17.468288
34.289252	1601.429194	17.473306
34.317236	1615.451292	17.478323
34.295030	1608.295414	17.483341
34.512484	1606.513016	17.488359
34.386621	1604.042413	17.493376
34.491868	1605.554995	17.498394
34.794045	1607.057682	17.503411
34.892186	1595.429509	17.508429
34.761697	1613.674339	17.513447
34.779980	1612.112048	17.518464
35.050871	1606.189724	17.523482
34.892772	1607.613006	17.528499
34.816982	1604.502987	17.533517
34.647716	1609.140284	17.538535
34.733275	1599.362599	17.543552
35.008681	1610.825105	17.548570
34.730691	1602.003497	17.553587
35.041438	1603.590585	17.558605
34.842469	1598.404219	17.563623
35.140808	1605.403133	17.568640
35.055302	1596.294423	17.573658
35.069464	1595.556428	17.578675
35.305014	1594.410779	17.583693
34.852161	1602.848694	17.588711
34.696654	1600.027117	17.593728
35.170002	1607.394578	17.598746
34.857074	1605.925523	17.603763
35.100344	1598.818833	17.608781
34.868135	1617.537654	17.613799
34.983716	1621.244947	17.618816
34.968955	1630.222262	17.623834
35.108007	1634.707538	17.628851
35.448616	1634.402682	17.633869
35.426023	1624.964211	17.638887
35.699736	1623.374427	17.643904
35.543636	1631.331940	17.648922
35.477377	1631.630132	17.653939
35.843702	1629.021424	17.658957
35.403792	1635.698173	17.663975
35.416911	1626.659667	17.668992
35.611823	1629.388829	17.674010
35.818307	1634.667612	17.679027
36.189948	1636.757568	17.684045
35.593762	1631.573037	17.689063
35.775027	1622.784143	17.694080
36.029267	1634.123414	17.699098
35.775516	1644.996734	17.704115
36.039122	1646.925909	17.709133
36.310096	1650.443212	17.714151
35.851772	1654.097867	17.719168
36.266004	1664.653886	17.724186
35.814577	1656.583505	17.729203
36.074043	1656.815751	17.734221
36.104220	1654.127869	17.739239
35.929749	1654.536564	17.744256
36.087054	1653.999183	17.749274
35.967518	1654.691265	17.754291
36.107044	1651.763952	17.759309
36.168323	1660.606602	17.764327
36.299364	1665.117233	17.769344
36.308960	1647.071129	17.774362
36.384058	1677.371494	17.779379
36.562043	1672.598040	17.784397
36.455039	1670.238857	17.789415
36.614560	1660.607501	17.794432
36.996528	1670.003150	17.799450
36.937743	1663.759616	17.804467
37.144461	1646.690976	17.809485
37.033627	1644.397000	17.814503
37.203866	1638.927213	17.819520
37.014256	1636.450664	17.824538
37.189268	1628.850193	17.829555
37.383567	1639.843530	17.834573
36.963657	1634.381671	17.839591
37.064960	1631.672523	17.844608
37.414254	1629.052473	17.849626
36.682868	1638.404405	17.854643
37.215415	1642.473108	17.859661
36.922136	1643.740121	17.864679
36.930612	1634.087035	17.869696
37.253016	1627.580558	17.874714
36.897033	1631.730791	17.879731
36.957736	1633.475579	17.884749
36.782343	1634.004111	17.889767
37.050649	1639.015537	17.894784
37.290875	1632.382954	17.899802
37.086205	1634.872626	17.904819
37.522287	1642.930148	17.909837
37.127376	1644.854990	17.914855
37.019669	1652.487546	17.919872
37.583609	1657.764013	17.924890
37.272496	1658.956828	17.929907
37.580251	1652.652773	17.934925
37.336731	1666.509808	17.939943
37.420601	1667.580678	17.944960
37.744804	1665.682501	17.949978
37.423887	1672.166656	17.954995
37.687457	1661.404238	17.960013
37.612387	1671.864026	17.965031
37.523964	1664.302596	17.970048
37.609898	1669.580167	17.975066
37.774916	1681.266188	17.980083
37.941937	1676.530381	17.985101
38.135903	1684.522259	17.990119
37.892667	1686.790399	17.995136
38.096961	1681.684226	18.000154
38.213826	1690.780643	18.005171
37.755963	1684.484137	18.010189
38.050146	1691.412522	18.015207
38.016828	1689.297781	18.020224
38.206163	1684.542121	18.025242
38.290681	1678.894837	18.030259
38.333323	1678.998160	18.035277
38.456239	1685.620758	18.040295
38.150806	1689.681503	18.045312
38.297120	1680.298784	18.050330
38.146248	1689.575130	18.055347
38.417975	1688.450233	18.060365
38.473549	1702.112316	18.065383
38.636610	1711.665631	18.070400
38.856096	1710.000600	18.075418
38.835823	1709.477376	18.080435
38.441256	1693.983017	18.085453
38.897850	1702.842271	18.090471
38.754656	1707.498886	18.095488
39.094539	1703.524099	18.100506
38.752073	1700.257597	18.105523
39.004125	1709.499273	18.110541
39.028044	1696.210932	18.115559
39.055660	1704.735582	18.120576
39.095984	1693.367730	18.125594
39.052690	1692.340464	18.130611
39.020250	1690.170065	18.135629
39.125853	1695.929805	18.140647
39.095204	1708.258597	18.145664
39.294371	1705.504432	18.150682
39.245651	1705.367429	18.155699
39.404740	1712.650951	18.160717
39.393406	1716.115977	18.165735
39.258584	1711.275208	18.170752
39.083576	1704.841920	18.175770
39.620335	1710.189852	18.180787
39.506627	1703.960154	18.185805
39.488020	1708.245279	18.190823
39.519292	1708.999305	18.195840
39.596600	1698.656792	18.200858
39.572653	1701.468404	18.205875
39.606483	1695.478754	18.210893
39.843427	1708.167006	18.215911
39.192761	1709.003268	18.220928
39.630794	1702.317702	18.225946
39.584823	1705.027464	18.230963
39.339297	1701.518080	18.235981
39.686250	1697.670465	18.240999
39.400520	1723.515967	18.246016
39.731122	1723.722612	18.251034
39.879842	1730.779914	18.256051
40.156414	1751.326924	18.261069
40.018868	1731.803608	18.266087
39.928160	1728.021245	18.271104
40.275857	1716.036153	18.276122
40.101846	1730.085234	18.281139
39.970511	1725.379314	18.286157
40.289782	1725.861069	18.291175
39.894653	1726.195023	18.296192
40.295104	1728.636501	18.301210
40.415366	1714.418752	18.306227
40.108531	1718.047063	18.311245
40.181811	1730.385371	18.316263
40.546573	1748.330334	18.321280
40.736457	1749.122569	18.326298
40.512335	1748.564720	18.331315
40.658499	1753.119714	18.336333
40.996809	1745.794407	18.341351
40.886274	1753.883385	18.346368
40.858779	1735.611454	18.351386
40.647255	1721.703564	18.356403
40.773645	1733.266912	18.361421
40.901139	1739.650978	18.366439
40.593331	1747.621954	18.371456
40.861056	1745.234338	18.376474
41.082977	1745.623218	18.381491
40.881268	1746.807698	18.386509
41.051021	1752.919394	18.391527
40.960175	1754.446078	18.396544
41.201774	1747.971878	18.401562
41.352950	1744.933163	18.406579
41.294950	1750.567359	18.411597
41.416883	1746.250834	18.416615
41.161710	1744.282798	18.421632
41.502207	1741.615767	18.426650
41.554890	1748.183924	18.431667
41.513597	1754.005500	18.436685
41.663601	1741.267423	18.441703
41.552042	1751.543173	18.446720
41.336149	1743.615489	18.451738
41.430415	1746.153134	18.456755
41.171562	1749.442376	18.461773
41.661422	1739.471425	18.466791
41.292826	1743.271029	18.471808
41.549637	1747.221021	18.476826
41.411530	1752.773256	18.481843
41.601202	1776.522129	18.486861
42.002680	1764.344598	18.491879
41.904937	1784.291267	18.496896
41.796786	1768.682300	18.501914
41.938687	1775.872252	18.506931
41.785150	1780.893993	18.511949
41.895884	1774.100194	18.516967
41.978450	1784.802363	18.521984
41.722762	1782.020631	18.527002
42.023005	1783.284288	18.532019
41.762808	1788.608402	18.537037
42.398504	1794.211968	18.542055
41.991701	1801.386826	18.547072
42.168268	1796.857664	18.552090
42.512495	1791.729773	18.557107
42.142142	1794.363935	18.562125
42.353838	1788.888781	18.567143
42.257516	1800.305729	18.572160
42.354058	1793.339085	18.577178
42.630123	1783.738676	18.582195
42.368107	1801.700076	18.587213
42.643898	1796.977651	18.592231
43.079105	1824.872004	18.597248
43.047385	1798.336924	18.602266
43.122442	1793.320697	18.607283
42.720414	1793.577452	18.612301
43.178378	1790.178686	18.617319
43.107918	1796.838196	18.622336
42.864112	1792.946221	18.627354
43.142473	1787.519043	18.632371
42.994842	1792.198861	18.637389
42.951931	1785.808545	18.642407
43.007890	1795.063572	18.647424
43.097325	1795.995338	18.652442
42.919070	1795.112935	18.657459
42.789207	1819.733089	18.662477
43.401832	1811.523578	18.667495
43.068376	1820.095309	18.672512
43.216084	1812.749680	18.677530
43.436350	1819.476235	18.682547
43.192974	1821.625519	18.687565
43.557717	1814.425708	18.692583
43.853192	1816.861419	18.697600
43.680952	1809.733533	18.702618
43.725790	1798.860129	18.707635
43.793539	1810.335249	18.712653
44.052813	1811.515954	18.717671
43.854458	1814.308935	18.722688
43.634630	1816.801549	18.727706
43.781984	1808.080391	18.732723
43.468616	1808.848395	18.737741
43.981887	1805.175080	18.742759
43.800163	1806.360180	18.747776
43.754878	1814.405275	18.752794
44.156070	1818.926171	18.757811
43.851892	1825.214300	18.762829
44.465347	1819.578269	18.767847
44.597499	1817.952150	18.772864
44.693572	1824.448955	18.777882
44.766749	1806.661389	18.782899
44.340685	1806.352060	18.787917
44.683508	1783.273651	18.792935
44.500070	1787.373987	18.797952
44.468379	1786.616833	18.802970
44.662183	1793.271790	18.807987
44.566204	1793.328074	18.813005
44.911745	1791.317281	18.818023
44.655830	1794.609588	18.823040
44.689960	1787.847807	18.828058
44.928773	1782.094527	18.833075
44.476676	1795.088706	18.838093
44.809779	1783.232367	18.843111
44.643210	1786.318091	18.848128
44.016566	1792.171612	18.853146
44.654223	1801.191776	18.858163
44.783466	1806.844086	18.863181
45.230385	1820.187296	18.868199
45.196819	1813.983210	18.873216
44.928429	1818.325232	18.878234
45.259952	1820.020702	18.883251
44.654597	1820.074635	18.888269
45.119950	1806.125433	18.893287
45.037961	1818.138437	18.898304
44.852298	1836.447817	18.903322
45.167536	1834.125913	18.908339
45.276894	1846.316586	18.913357
45.426184	1847.098249	18.918375
45.481919	1837.567104	18.923392
45.344918	1841.119972	18.928410
45.931287	1834.132925	18.933427
45.347678	1840.126162	18.938445
45.812898	1839.452955	18.943463
45.557594	1838.630205	18.948480
45.651346	1847.049454	18.953498
45.825753	1831.772204	18.958515
45.820766	1841.240537	18.963533
46.116235	1839.228612	18.968551
45.954330	1833.971439	18.973568
45.461465	1838.914554	18.978586
45.563460	1844.410382	18.983603
45.917026	1856.064412	18.988621
46.469677	1843.106182	18.993639
47.113812	1843.599697	18.998656
46.994678	1844.626760	19.003674
46.879171	1826.769348	19.008691
46.688447	1827.559095	19.013709
46.559251	1815.141376	19.018727
46.745939	1815.047531	19.023744
46.523775	1812.786206	19.028762
46.421805	1808.210025	19.033779
46.288817	1818.752767	19.038797
46.460674	1813.714540	19.043815
46.513910	1805.100758	19.048832
46.471677	1814.896918	19.053850
46.919858	1805.932851	19.058867
46.778729	1812.550175	19.063885
46.426265	1814.208140	19.068903
46.668013	1810.706723	19.073920
46.464472	1838.248992	19.078938
46.849208	1830.732071	19.083955
46.553950	1847.407709	19.088973
46.606997	1837.804963	19.093991
46.825719	1841.776664	19.099008
46.839343	1849.188364	19.104026
47.266938	1861.214741	19.109043
47.059416	1875.978580	19.114061
47.090492	1875.120044	19.119079
47.297897	1876.792053	19.124096
47.466238	1869.431551	19.129114
47.406233	1865.986571	19.134131
47.484561	1875.144621	19.139149
47.586882	1872.176994	19.144167
47.598519	1870.484678	19.149184
47.871566	1864.514261	19.154202
47.818833	1867.583838	19.159219
47.720982	1867.285313	19.164237
47.711685	1879.778804	19.169255
48.042602	1867.736937	19.174272
47.666361	1871.942567	19.179290
47.803389	1858.150642	19.184307
47.715821	1875.745338	19.189325
47.783724	1872.006264	19.194343
48.077271	1858.565491	19.199360
47.544069	1870.104706	19.204378
48.085186	1883.235464	19.209395
48.104508	1887.433625	19.214413
48.043815	1890.450198	19.219431
48.270161	1896.899004	19.224448
48.207654	1894.694203	19.229466
48.538060	1893.310326	19.234483
48.411564	1896.883902	19.239501
48.226567	1895.367966	19.244519
48.238205	1892.400839	19.249536
48.434999	1890.706095	19.254554
48.693908	1891.493165	19.259571
48.743335	1888.013851	19.264589
48.773850	1893.106220	19.269607
48.815583	1889.169915	19.274624
48.484784	1894.018001	19.279642
48.868686	1884.266932	19.284659
48.745906	1881.889472	19.289677
48.766186	1896.749723	19.294695
48.915610	1899.245155	19.299712
48.905139	1918.617253	19.304730
49.223052	1917.355529	19.309747
49.519781	1915.675277	19.314765
49.192040	1906.642469	19.319783
49.242635	1890.556207	19.324800
49.186809	1895.760564	19.329818
49.153423	1895.339121	19.334835
49.509409	1914.496372	19.339853
49.411434	1918.210883	19.344871
49.253455	1913.056181	19.349888
49.281876	1910.163034	19.354906
49.524432	1905.444525	19.359923
49.336335	1912.450408	19.364941
49.346187	1905.493790	19.369959
49.557085	1907.934912	19.374976
49.454271	1910.692740	19.379994
49.801631	1898.289453	19.385011
49.954210	1910.350945	19.390029
49.569951	1912.990588	19.395047
50.156287	1922.652035	19.400064
50.127345	1935.900415	19.405082
49.906308	1939.575147	19.410099
50.207977	1928.498337	19.415117
50.123861	1933.529061	19.420135
50.501010	1931.145673	19.425152
50.513837	1946.778083	19.430170
50.649232	1925.580801	19.435187
50.546547	1916.347198	19.440205
50.020831	1917.486719	19.445223
50.267797	1912.463931	19.450240
50.159427	1930.014902	19.455258
50.304160	1935.474131	19.460275
50.526848	1933.443581	19.465293
50.482421	1933.173579	19.470311
50.742524	1930.881298	19.475328
50.796566	1928.379561	19.480346
50.792462	1933.004465	19.485363
50.556451	1928.124146	19.490381
50.556962	1936.276654	19.495399
50.809732	1931.068248	19.500416
50.694557	1942.031737	19.505434
50.856896	1954.291643	19.510451
51.289388	1958.913680	19.515469
50.644158	1963.243961	19.520487
51.124322	1955.251668	19.525504
50.952853	1953.956707	19.530522
51.046636	1960.103947	19.535539
51.381589	1958.852380	19.540557
51.495810	1959.535940	19.545575
51.277687	1951.780569	19.550592
51.458010	1957.512633	19.555610
51.536517	1978.516095	19.560627
51.897696	1979.931061	19.565645
51.695130	1976.975896	19.570663
51.905104	1974.127761	19.575680
51.943732	1966.608848	19.580698
52.251319	1958.684999	19.585715
52.245986	1946.999743	19.590733
51.909997	1957.150723	19.595751
52.048278	1944.653405	19.600768
51.717116	1953.868140	19.605786
51.705038	1949.852573	19.610803
52.233171	1950.159859	19.615821
51.589216	1964.028985	19.620839
51.991038	1962.841502	19.625856
51.999456	1979.097517	19.630874
51.746529	1981.036203	19.635891
51.800166	1982.336532	19.640909
51.728715	1977.741843	19.645927
52.359032	2001.115856	19.650944
52.588208	2006.474068	19.655962
52.448972	2010.854127	19.660979
52.353281	2009.193020	19.665997
52.606403	2009.830663	19.671015
52.303686	2017.070212	19.676032
52.423654	2010.641315	19.681050
52.449571	2012.818312	19.686067
52.797400	2011.509876	19.691085
52.749077	2023.196967	19.696103
53.049352	2026.673267	19.701120
52.864328	2032.843643	19.706138
53.016243	2028.700405	19.711155
53.379277	2039.104953	19.716173
53.028994	2036.160152	19.721191
53.155086	2041.494957	19.726208
53.213293	2032.684944	19.731226
53.204542	2039.567769	19.736243
53.498431	2030.405986	19.741261
53.334040	2049.625479	19.746279
53.261837	2029.590134	19.751296
53.484971	2030.716232	19.756314
53.278486	2033.376349	19.761331
53.771133	2033.261971	19.766349
53.347865	2041.433389	19.771367
53.609900	2052.797658	19.776384
53.747734	2056.601360	19.781402
53.673563	2070.470766	19.786419
53.603904	2069.535653	19.791437
53.943058	2070.534203	19.796455
54.055742	2054.739819	19.801472
54.523724	2059.163072	19.806490
54.089592	2060.200373	19.811507
54.770854	2055.495130	19.816525
54.542950	2057.132418	19.821543
54.587328	2056.522846	19.826560
54.651374	2056.082843	19.831578
54.274883	2061.600002	19.836595
54.743365	2049.006384	19.841613
54.942141	2039.858040	19.846631
55.073738	2033.983902	19.851648
55.093249	2020.681449	19.856666
55.118364	2011.322217	19.861683
55.355597	2008.941992	19.866701
55.114149	2002.087332	19.871719
55.452692	1997.321741	19.876736
55.434042	1993.379697	19.881754
55.147882	1998.160553	19.886771
55.388200	1973.890616	19.891789
54.729191	1965.919531	19.896807
54.712670	1971.503999	19.901824
55.034252	1986.697730	19.906842
54.822583	1993.065040	19.911859
54.891658	2000.945161	19.916877
54.899875	2003.798334	19.921895
54.852862	2001.387003	19.926912
54.911038	2005.695276	19.931930
55.051435	2023.788086	19.936947
55.284951	2032.777916	19.941965
55.294409	2033.431646	19.946983
55.111180	2038.473365	19.952000
55.350208	2034.967232	19.957018
55.108437	2058.888243	19.962035
55.613968	2051.692879	19.967053
55.984053	2063.856140	19.972071
55.915732	2059.935326	19.977088
56.171299	2061.339505	19.982106
55.830448	2057.487214	19.987123
55.897696	2062.077463	19.992141
56.016299	2065.372938	19.997159
55.861114	2058.845261	20.002176
55.689570	2053.512055	20.007194
55.707411	2066.331899	20.012211
56.019328	2075.767787	20.017229
56.143570	2085.185264	20.022247
56.334264	2083.182454	20.027264
56.662376	2082.429267	20.032282
56.425622	2084.080627	20.037299
56.632683	2086.930296	20.042317
56.713472	2073.237686	20.047335
56.862261	2075.429704	20.052352
56.868760	2074.509099	20.057370
56.906820	2077.098266	20.062387
56.807789	2069.972265	20.067405
56.631734	2079.444371	20.072423
56.879392	2087.094459	20.077440
57.248541	2099.724054	20.082458
57.214093	2104.096567	20.087475
57.518997	2111.092259	20.092493
57.364120	2087.198461	20.097511
57.166258	2075.512429	20.102528
57.532037	2080.814892	20.107546
57.484197	2102.290315	20.112563
57.623094	2097.473227	20.117581
57.206619	2097.889474	20.122599
57.186190	2101.743900	20.127616
57.748974	2100.584776	20.132634
57.478357	2099.981489	20.137651
57.733259	2097.296735	20.142669
57.676561	2106.687996	20.147687
57.888985	2110.340336	20.152704
57.940283	2107.218542	20.157722
57.628399	2112.393479	20.162739
57.894402	2112.336454	20.167757
57.934397	2115.182397	20.172775
57.745875	2136.845030	20.177792
58.660882	2128.378011	20.182810
57.941158	2135.225492	20.187827
58.278579	2135.038090	20.192845
58.621752	2129.962235	20.197863
58.245687	2132.271411	20.202880
58.557720	2126.554262	20.207898
58.115563	2128.897257	20.212915
58.968806	2126.021322	20.217933
58.624342	2119.663268	20.222951
58.750404	2126.643020	20.227968
58.850121	2119.661922	20.232986
58.862720	2131.815750	20.238003
58.740485	2121.269499	20.243021
58.803156	2124.189630	20.248039
58.834776	2123.464850	20.253056
59.215300	2134.807126	20.258074
59.006785	2146.908341	20.263091
59.186667	2143.759266	20.268109
59.355464	2152.302825	20.273127
59.355598	2146.042611	20.278144
59.794142	2130.051078	20.283162
59.778391	2137.019757	20.288179
59.791013	2127.142442	20.293197
59.739618	2123.078245	20.298215
59.306583	2107.131191	20.303232
59.786912	2103.069183	20.308250
59.610427	2106.173153	20.313267
59.668488	2113.527987	20.318285
59.918304	2125.248284	20.323303
59.786270	2123.172331	20.328320
59.546598	2132.745988	20.333338
59.728557	2131.550151	20.338355
59.828687	2144.028425	20.343373
59.864021	2125.881421	20.348391
59.849248	2134.556268	20.353408
59.809838	2126.360076	20.358426
60.241376	2146.491693	20.363443
60.476238	2151.221438	20.368461
59.985108	2149.328391	20.373479
60.132272	2163.552050	20.378496
60.334747	2159.966136	20.383514
60.174364	2168.323068	20.388531
60.259783	2162.601048	20.393549
60.495166	2161.758937	20.398567
60.489417	2174.614288	20.403584
60.578384	2181.689602	20.408602
60.383962	2181.682324	20.413619
60.892661	2170.029585	20.418637
60.751131	2186.802481	20.423655
60.583096	2179.333559	20.428672
61.238854	2193.862099	20.433690
61.020013	2207.259597	20.438707
61.073085	2214.841691	20.443725
61.723703	2211.974220	20.448743
61.485254	2216.501931	20.453760
61.933026	2206.941233	20.458778
61.726447	2204.948131	20.463795
61.617564	2185.645469	20.468813
61.943676	2172.952575	20.473831
61.452975	2179.649411	20.478848
61.923651	2184.802979	20.483866
61.963911	2196.493195	20.488883
61.727553	2199.447682	20.493901
62.018502	2205.600835	20.498919
61.953886	2207.220055	20.503936
61.939737	2196.777447	20.508954
61.842925	2203.500566	20.513971
61.924051	2202.689994	20.518989
62.251602	2196.745433	20.524007
62.090683	2200.491732	20.529024
62.071143	2202.998365	20.534042
62.363433	2197.236833	20.539059
62.077194	2204.989096	20.544077
62.250179	2217.075784	20.549095
62.564790	2219.261131	20.554112
62.638562	2229.274893	20.559130
62.553186	2227.916781	20.564147
62.420444	2229.778434	20.569165
62.658319	2230.903673	20.574183
62.449560	2230.936968	20.579200
62.922298	2240.621827	20.584218
63.095563	2246.546122	20.589235
63.168120	2251.068614	20.594253
63.432291	2253.163527	20.599271
63.258144	2263.559469	20.604288
63.113645	2261.554074	20.609306
63.326788	2262.533421	20.614323
63.182540	2255.684542	20.619341
63.333507	2245.977079	20.624359
63.080475	2262.395742	20.629376
63.214340	2251.501320	20.634394
63.401018	2257.189526	20.639411
63.244715	2268.287249	20.644429
63.682051	2278.371728	20.649447
63.344510	2288.609009	20.654464
63.911955	2284.882881	20.659482
63.633622	2283.203277	20.664499
63.392989	2285.616742	20.669517
63.994050	2274.635210	20.674535
63.887449	2293.000493	20.679552
64.167027	2295.346402	20.684570
64.155474	2308.068179	20.689587
64.044038	2314.629991	20.694605
64.299249	2312.767222	20.699623
64.354356	2309.297107	20.704640
64.829837	2309.732844	20.709658
65.003465	2310.966407	20.714675
64.754828	2311.475241	20.719693
64.835692	2302.455792	20.724711
64.821434	2312.900393	20.729728
65.037311	2306.234169	20.734746
65.292215	2296.548378	20.739763
65.129308	2310.954023	20.744781
65.222745	2303.608520	20.749799
64.904848	2307.671100	20.754816
65.089323	2302.672353	20.759834
65.115372	2299.549599	20.764851
65.202238	2314.275558	20.769869
65.169834	2298.014473	20.774887
65.198019	2301.221086	20.779904
65.080238	2308.148528	20.784922
65.532204	2319.666868	20.789939
65.423502	2335.795078	20.794957
65.598403	2330.955792	20.799975
65.560555	2335.057273	20.804992
65.473948	2329.504337	20.810010
65.610014	2338.551880	20.815027
65.688560	2335.277083	20.820045
65.836974	2324.021519	20.825063
65.859339	2355.493823	20.830080
66.031112	2358.901788	20.835098
66.338862	2358.101973	20.840115
66.113624	2362.372010	20.845133
66.392853	2355.049151	20.850151
66.309182	2358.756271	20.855168
66.329049	2359.261823	20.860186
66.386998	2351.486748	20.865203
66.578465	2362.677534	20.870221
66.540923	2356.751461	20.875239
66.693126	2365.261281	20.880256
66.568319	2364.978644	20.885274
67.049669	2366.415804	20.890291
66.882282	2385.375177	20.895309
66.488016	2379.524915	20.900327
66.828959	2383.591410	20.905344
66.900360	2387.317255	20.910362
67.169918	2379.026273	20.915379
66.917934	2381.732594	20.920397
67.381356	2370.163218	20.925415
67.151636	2380.902343	20.930432
67.423510	2402.898296	20.935450
67.625195	2400.522740	20.940467
67.713489	2404.479255	20.945485
67.893543	2408.414615	20.950503
68.008998	2401.507944	20.955520
68.033445	2404.957727	20.960538
68.145908	2397.163727	20.965555
67.808038	2392.263572	20.970573
67.827654	2389.643069	20.975591
68.103903	2403.100192	20.980608
68.156134	2394.742953	20.985626
68.786180	2396.942047	20.990643
68.301627	2389.829181	20.995661
68.335412	2396.986207	21.000679
68.311843	2392.523994	21.005696
68.124436	2394.308922	21.010714
68.655307	2392.458207	21.015731
68.370595	2395.649909	21.020749
68.569132	2388.160123	21.025767
68.535129	2390.899119	21.030784
68.662234	2388.978102	21.035802
68.696791	2376.153963	21.040819
68.626636	2393.814465	21.045837
68.877414	2383.692675	21.050855
68.761954	2391.565079	21.055872
69.032511	2410.778484	21.060890
69.286326	2410.403787	21.065907
69.280380	2406.979231	21.070925
69.897739	2398.755638	21.075943
69.913898	2401.054000	21.080960
69.617606	2397.236738	21.085978
69.426344	2383.498906	21.090995
69.569095	2385.291958	21.096013
70.017061	2390.454489	21.101031
69.930449	2391.601382	21.106048
69.809656	2393.842186	21.111066
70.053304	2383.047541	21.116083
70.030704	2393.697528	21.121101
70.326187	2398.421999	21.126119
70.432541	2395.741803	21.131136
70.227859	2391.813644	21.136154
70.474211	2379.793311	21.141171
69.953032	2380.023807	21.146189
69.713405	2385.363603	21.151207
70.185444	2390.081172	21.156224
70.428330	2399.572827	21.161242
70.580989	2391.774511	21.166259
70.413972	2400.602766	21.171277
70.238618	2401.020681	21.176295
70.533561	2420.274141	21.181312
70.362301	2423.097373	21.186330
70.830129	2426.545920	21.191347
70.567201	2425.420060	21.196365
70.407264	2427.347283	21.201383
70.864487	2443.357142	21.206400
71.006155	2449.024945	21.211418
71.405181	2452.460915	21.216435
71.236459	2462.278505	21.221453
71.270635	2457.684624	21.226471
71.511026	2460.437088	21.231488
71.324844	2461.635969	21.236506
71.433556	2462.716153	21.241523
71.745469	2473.478324	21.246541
72.116389	2480.923863	21.251559
72.244463	2479.768847	21.256576
71.762408	2445.582375	21.261594
71.904599	2461.299320	21.266611
71.716642	2475.707704	21.271629
71.762408	2475.234506	21.276647
72.392998	2487.151256	21.281664
72.049476	2481.236221	21.286682
72.156780	2485.727021	21.291699
72.079820	2491.694965	21.296717
72.429627	2487.130907	21.301735
72.812282	2485.725305	21.306752
72.333833	2488.796460	21.311770
72.706463	2491.420649	21.316787
72.763968	2495.479946	21.321805
72.529841	2502.045297	21.326823
72.886024	2504.720256	21.331840
72.364069	2507.071841	21.336858
72.914624	2498.054933	21.341875
72.631113	2496.227340	21.346893
72.893379	2502.823587	21.351911
73.125162	2521.174243	21.356928
72.706234	2530.667693	21.361946
73.215474	2533.555026	21.366963
73.335321	2524.461251	21.371981
73.028805	2531.025258	21.376999
73.286537	2531.102291	21.382016
73.580659	2552.882939	21.387034
73.833909	2556.564035	21.392051
74.019424	2548.409377	21.397069
74.686787	2528.534744	21.402087
75.158183	2522.768919	21.407104
74.932329	2502.766372	21.412122
75.216930	2495.615004	21.417139
75.329048	2479.741932	21.422157
75.369202	2469.279485	21.427175
74.968408	2456.072888	21.432192
74.772107	2451.235804	21.437210
74.736052	2449.429299	21.442227
74.945844	2432.551027	21.447245
74.720210	2437.403850	21.452263
74.835367	2434.780060	21.457280
74.551384	2436.531828	21.462298
74.680343	2437.228710	21.467315
75.027544	2454.794723	21.472333
74.672493	2450.078514	21.477351
74.604681	2450.157284	21.482368
74.681563	2455.467338	21.487386
74.709475	2459.728402	21.492403
74.897039	2475.253167	21.497421
74.935945	2475.928401	21.502439
74.732601	2480.167664	21.507456
74.809243	2501.784376	21.512474
75.368403	2510.349090	21.517491
75.334840	2512.737625	21.522509
75.091058	2521.811788	21.527527
75.270097	2532.080311	21.532544
75.266375	2554.298666	21.537562
75.903562	2543.805062	21.542579
76.039177	2543.025971	21.547597
75.869454	2543.512247	21.552615
76.253018	2555.727597	21.557632
76.360587	2566.196612	21.562650
76.383094	2565.255207	21.567667
76.474903	2569.631278	21.572685
76.145980	2566.454860	21.577703
76.835279	2562.458406	21.582720
76.700823	2562.436436	21.587738
76.625019	2564.100468	21.592755
76.574613	2562.036874	21.597773
76.517162	2565.865676	21.602791
76.831077	2562.767474	21.607808
76.729855	2583.175216	21.612826
76.873716	2592.861408	21.617843
77.136201	2594.991690	21.622861
76.991640	2601.352031	21.627879
77.426796	2590.881735	21.632896
77.158563	2588.531487	21.637914
77.223909	2582.307506	21.642931
77.483414	2595.649858	21.647949
77.516006	2618.008733	21.652967
77.774761	2621.328676	21.657984
77.651537	2630.113560	21.663002
77.925517	2618.018371	21.668019
78.114983	2619.508396	21.673037
77.870140	2619.660290	21.678055
78.251667	2617.431595	21.683072
78.219579	2620.773887	21.688090
78.114270	2615.805482	21.693107
78.096845	2615.743195	21.698125
77.849821	2615.693079	21.703143
78.115709	2620.959967	21.708160
78.522725	2646.432806	21.713178
78.560128	2647.792191	21.718195
78.547018	2640.553612	21.723213
78.686007	2648.696867	21.728231
78.825404	2637.407928	21.733248
78.867612	2642.967129	21.738266
78.698578	2633.476787	21.743283
79.183610	2642.140907	21.748301
79.322909	2659.698393	21.753319
79.554684	2666.914378	21.758336
79.047368	2663.634902	21.763354
79.317234	2664.470590	21.768371
79.650866	2664.667695	21.773389
79.487642	2664.228829	21.778407
79.917855	2657.111459	21.783424
79.915288	2662.594639	21.788442
79.862058	2657.156517	21.793459
79.750454	2658.217421	21.798477
79.447966	2661.850342	21.803495
79.715798	2657.479396	21.808512
79.883914	2671.869340	21.813530
80.177232	2681.176399	21.818547
80.535592	2683.447462	21.823565
80.459006	2687.887381	21.828583
80.744654	2684.904095	21.833600
80.666250	2695.925000	21.838618
80.618007	2693.451557	21.843635
80.761872	2690.383559	21.848653
80.526666	2691.232710	21.853671
80.728792	2686.617937	21.858688
80.745864	2690.086727	21.863706
80.565043	2685.697022	21.868723
80.990199	2700.276572	21.873741
80.681675	2713.369310	21.878759
81.020936	2716.518799	21.883776
80.914313	2720.236119	21.888794
81.048685	2719.433996	21.893811
81.646962	2738.911867	21.898829
81.123691	2749.592543	21.903847
81.451165	2740.631863	21.908864
81.530298	2743.173762	21.913882
81.292389	2748.755929	21.918899
81.748554	2741.225129	21.923917
81.944285	2768.940499	21.928935
82.295568	2772.054928	21.933952
82.536653	2772.185914	21.938970
82.158895	2770.920834	21.943987
82.503049	2772.402098	21.949005
82.564942	2765.353764	21.954023
82.635857	2772.058309	21.959040
82.773622	2758.783607	21.964058
82.847167	2762.142235	21.969075
83.111342	2756.624162	21.974093
82.983216	2757.207081	21.979111
83.034930	2752.189701	21.984128
83.044968	2755.793541	21.989146
82.920510	2758.472039	21.994163
83.499363	2760.836400	21.999181
83.275124	2763.239337	22.004199
83.248428	2759.685073	22.009216
83.069688	2750.544325	22.014234
83.150693	2757.585790	22.019251
83.365227	2757.770404	22.024269
83.200450	2759.679178	22.029287
83.154635	2764.367564	22.034304
83.645384	2784.796096	22.039322
83.305661	2794.135588	22.044339
83.778392	2780.324461	22.049357
83.461986	2796.105358	22.054375
84.101077	2794.251971	22.059392
84.354380	2797.876027	22.064410
84.423129	2794.790176	22.069427
84.648378	2799.150042	22.074445
84.933567	2788.581300	22.079463
85.025218	2783.319857	22.084480
85.022122	2769.835863	22.089498
84.676652	2757.266703	22.094515
84.862689	2762.050818	22.099533
84.395025	2771.368642	22.104551
84.784762	2779.041922	22.109568
85.005957	2783.806420	22.114586
84.981515	2795.649974	22.119603
85.426759	2788.417049	22.124621
85.548260	2788.947066	22.129639
85.324938	2792.506620	22.134656
85.552226	2794.736093	22.139674
85.468299	2796.585763	22.144691
85.974651	2783.498619	22.149709
85.229025	2794.022959	22.154727
85.299321	2792.101884	22.159744
85.319016	2800.843426	22.164762
85.371420	2820.610162	22.169779
85.717792	2819.378289	22.174797
85.643513	2821.275969	22.179815
85.937985	2828.211907	22.184832
86.085560	2843.762979	22.189850
86.475719	2852.079181	22.194867
86.480083	2841.321624	22.199885
86.089287	2846.406758	22.204903
86.274403	2855.137771	22.209920
86.818890	2853.468221	22.214938
86.769036	2864.913268	22.219955
86.757707	2873.787969	22.224973
86.838275	2877.667143	22.229991
86.890293	2872.192163	22.235008
86.731729	2875.203929	22.240026
87.076232	2884.460082	22.245043
87.473921	2893.170358	22.250061
87.308373	2891.776687	22.255079
87.769788	2898.635304	22.260096
88.023418	2900.178084	22.265114
87.711849	2897.457011	22.270131
88.173427	2889.403552	22.275149
88.259747	2895.728400	22.280167
88.165517	2889.909582	22.285184
88.347560	2884.168090	22.290202
87.941788	2886.427974	22.295219
88.024437	2881.415648	22.300237
88.176335	2892.332272	22.305255
88.190745	2894.732579	22.310272
88.565159	2880.676662	22.315290
87.958542	2896.756300	22.320307
88.302068	2891.872676	22.325325
88.520631	2912.430475	22.330343
88.420002	2922.044897	22.335360
88.783139	2929.221062	22.340378
88.566311	2926.123978	22.345395
88.424366	2916.708888	22.350413
88.996307	2934.357395	22.355431
88.967191	2941.801524	22.360448
89.062348	2940.797625	22.365466
89.170106	2948.442254	22.370483
89.274962	2939.119610	22.375501
89.454796	2942.468094	22.380519
89.357498	2962.978050	22.385536
89.742994	2964.341431	22.390554
89.891820	2977.362716	22.395571
90.111122	2970.336953	22.400589
90.132674	2970.207553	22.405607
90.279443	2986.029000	22.410624
90.610844	2965.085154	22.415642
90.364762	2969.319445	22.420659
90.844357	2964.270656	22.425677
90.810652	2964.956403	22.430695
90.613036	2957.618408	22.435712
90.819999	2948.881195	22.440730
90.897056	2953.300775	22.445747
90.915250	2940.083588	22.450765
91.256003	2941.961131	22.455783
90.932752	2948.004040	22.460800
91.091324	2946.260415	22.465818
90.880913	2947.785823	22.470835
91.224909	2948.575742	22.475853
91.185124	2952.415483	22.480871
91.048842	2979.059550	22.485888
91.670362	2976.766117	22.490906
91.622436	2984.969354	22.495923
91.640559	2979.512568	22.500941
91.982739	2982.100168	22.505959
91.796938	2985.557460	22.510976
91.935860	2976.279923	22.515994
91.949853	2985.371756	22.521011
92.170749	3011.648230	22.526029
92.187399	3007.467367	22.531047
92.206183	3017.910099	22.536064
92.405925	3012.781414	22.541082
92.429518	3014.024614	22.546099
92.388941	3012.048310	22.551117
92.771467	3023.343266	22.556135
92.433063	3037.670863	22.561152
92.955690	3037.584185	22.566170
92.862983	3039.975936	22.571187
92.891287	3033.761869	22.576205
93.058923	3034.869706	22.581223
93.138732	3040.542494	22.586240
92.993025	3058.184805	22.591258
93.186217	3068.404084	22.596275
93.214524	3065.054799	22.601293
93.568742	3061.207225	22.606311
93.369337	3072.199680	22.611328
93.865985	3076.084173	22.616346
93.704128	3087.901962	22.621363
93.955458	3084.971553	22.626381
94.110760	3078.939529	22.631399
94.008420	3088.591348	22.636416
94.317214	3082.779110	22.641434
94.273034	3089.769476	22.646451
94.459786	3103.688181	22.651469
94.687373	3108.991919	22.656487
94.709617	3109.727041	22.661504
95.316842	3100.096387	22.666522
95.062650	3102.258270	22.671539
95.149243	3104.030421	22.676557
95.213145	3100.642140	22.681575
95.236418	3102.688616	22.686592
95.278912	3103.036876	22.691610
95.427302	3102.377693	22.696627
95.114273	3105.037977	22.701645
95.306985	3101.001073	22.706663
95.313535	3113.398819	22.711680
95.304143	3113.916739	22.716698
95.413155	3127.320781	22.721715
95.695517	3135.092798	22.726733
95.666492	3126.773870	22.731751
95.691357	3142.672038	22.736768
95.938017	3156.069373	22.741786
95.894790	3161.294896	22.746803
96.152808	3165.455703	22.751821
96.329121	3159.481185	22.756839
96.303783	3165.664842	22.761856
96.617698	3167.405129	22.766874
96.393650	3189.262938	22.771891
96.249761	3195.537968	22.776909
96.398464	3191.217384	22.781927
96.731157	3211.701488	22.786944
96.947809	3219.546284	22.791962
97.128649	3223.295485	22.796979
96.876809	3226.673245	22.801997
97.274342	3220.985592	22.807015
97.055575	3224.954365	22.812032
97.208566	3236.779004	22.817050
98.056250	3237.840779	22.822067
98.090080	3238.562563	22.827085
98.446106	3228.800726	22.832103
98.124996	3238.274801	22.837120
98.428449	3237.377620	22.842138
98.240239	3232.355465	22.847155
98.159262	3234.509448	22.852173
98.688971	3229.777080	22.857191
98.423676	3237.912626	22.862208
98.600323	3229.841378	22.867226
98.456435	3245.358603	22.872243
98.419086	3262.086992	22.877261
98.715940	3258.114244	22.882279
98.927735	3261.203132	22.887296
99.000915	3266.081755	22.892314
98.909105	3260.093483	22.897331
99.094385	3276.889231	22.902349
99.468263	3286.641578	22.907367
99.515555	3288.012369	22.912384
99.545318	3288.519063	22.917402
99.780649	3287.519410	22.922419
99.736915	3296.063090	22.927437
99.842489	3287.575631	22.932455
99.488256	3300.037024	22.937472
100.174898	3297.979206	22.942490
100.933998	3299.984536	22.947507
100.852027	3309.700436	22.952525
101.282276	3297.187772	22.957543
100.872598	3295.433021	22.962560
100.978748	3275.869234	22.967578
101.001579	3268.382635	22.972595
100.623769	3266.815917	22.977613
100.754903	3268.711407	22.982631
100.867963	3289.062412	22.987648
100.967382	3300.106164	22.992666
101.049043	3296.918846	22.997683
100.923010	3297.179358	23.002701
101.212705	3296.088379	23.007719
101.485285	3304.028264	23.012736
101.510128	3311.988061	23.017754
101.981030	3318.883089	23.022771
101.866917	3321.811168	23.027789
101.795459	3321.018810	23.032807
101.938769	3324.556535	23.037824
101.659716	3319.407703	23.042842
102.005182	3321.832202	23.047859
101.917227	3333.597340	23.052877
101.914814	3339.485889	23.057895
101.964326	3350.888792	23.062912
101.961389	3357.251103	23.067930
102.162711	3356.763447	23.072947
102.238806	3383.694988	23.077965
102.524041	3384.261996	23.082983
103.038010	3379.801518	23.088000
102.693234	3383.981842	23.093018
103.256061	3392.872457	23.098035
102.980283	3420.388968	23.103053
103.286771	3411.078603	23.108071
103.286422	3414.478001	23.113088
103.229844	3414.099744	23.118106
103.636795	3411.704100	23.123123
103.595804	3416.409204	23.128141
103.873218	3432.976008	23.133159
103.840654	3443.408658	23.138176
103.932992	3437.759833	23.143194
104.202640	3440.900961	23.148211
104.136865	3444.890038	23.153229
104.461704	3441.262631	23.158247
104.689703	3451.701598	23.163264
104.742757	3460.927388	23.168282
105.128950	3464.158613	23.173299
105.105943	3450.862792	23.178317
105.102799	3454.031537	23.183335
105.314175	3453.303599	23.188352
105.416765	3451.574735	23.193370
105.828577	3445.968496	23.198387
105.660587	3455.263303	23.203405
105.554989	3446.879755	23.208423
105.943744	3449.100604	23.213440
105.716381	3448.219175	23.218458
106.000183	3435.658683	23.223475
105.848850	3444.589261	23.228493
105.966532	3440.085949	23.233511
105.734152	3433.091730	23.238528
105.975051	3448.225100	23.243546
106.366421	3462.112090	23.248563
106.319518	3476.731051	23.253581
106.233807	3470.744047	23.258599
106.464875	3467.288533	23.263616
106.277580	3475.217911	23.268634
106.544041	3484.468494	23.273651
106.577603	3504.094329	23.278669
106.747320	3503.664682	23.283687
107.125161	3500.421409	23.288704
107.199298	3514.379276	23.293722
107.579673	3513.677982	23.298739
107.391630	3526.883674	23.303757
107.819492	3519.607237	23.308775
107.764650	3515.959435	23.313792
107.642666	3525.385630	23.318810
107.654758	3516.949806	23.323827
107.881140	3523.149260	23.328845
108.017729	3537.834645	23.333863
108.459215	3540.853526	23.338880
108.607176	3557.125798	23.343898
108.738202	3546.119911	23.348915
108.566984	3554.241167	23.353933
108.599118	3554.345463	23.358951
108.921159	3535.518001	23.363968
108.688567	3550.845129	23.368986
108.805794	3546.075297	23.374003
108.683211	3540.782658	23.379021
109.130346	3556.292142	23.384039
109.143042	3561.610484	23.389056
109.117561	3572.792521	23.394074
109.331472	3563.447445	23.399091
109.398070	3569.056866	23.404109
109.262388	3569.895428	23.409127
109.828132	3582.054933	23.414144
109.629402	3613.044411	23.419162
109.825366	3599.638838	23.424179
109.848913	3595.215699	23.429197
109.983382	3594.301301	23.434215
110.514433	3607.363543	23.439232
110.270537	3620.361642	23.444250
110.650990	3623.378475	23.449267
110.742994	3619.515673	23.454285
110.822825	3619.426195	23.459303
110.527318	3615.905382	23.464320
110.604154	3633.748787	23.469338
111.378270	3647.834574	23.474355
111.082741	3651.043285	23.479373
111.159535	3645.350506	23.484391
111.702778	3642.498666	23.489408
111.521788	3634.487824	23.494426
111.321669	3639.833683	23.499443
112.102909	3651.742447	23.504461
111.685378	3665.671905	23.509479
112.340029	3654.755718	23.514496
112.343099	3674.341160	23.519514
112.279628	3668.137760	23.524531
112.579998	3668.122669	23.529549
112.417350	3675.054235	23.534567
112.690063	3665.917856	23.539584
112.656713	3676.264168	23.544602
112.627933	3688.616266	23.549619
112.870432	3689.859761	23.554637
112.800601	3698.713546	23.559655
113.083239	3692.399858	23.564672
112.991980	3702.785342	23.569690
113.443375	3714.090226	23.574707
113.487822	3714.994936	23.579725
113.282796	3727.453135	23.584743
113.856393	3715.934159	23.589760
113.865475	3719.075726	23.594778
113.866930	3708.579111	23.599795
113.973006	3719.436205	23.604813
114.217351	3743.398710	23.609831
114.518795	3735.701395	23.614848
114.334839	3736.964181	23.619866
114.764949	3731.729649	23.624883
114.569130	3740.441382	23.629901
114.789856	3749.164224	23.634919
114.910009	3739.969286	23.639936
114.549931	3744.655064	23.644954
115.026477	3754.534363	23.649971
115.341862	3763.668307	23.654989
115.181936	3764.876702	23.660007
115.413232	3770.980938	23.665024
115.100136	3768.902956	23.670042
114.955995	3784.465250	23.675059
115.068041	3790.104210	23.680077
114.964105	3806.939140	23.685095
115.368288	3821.537405	23.690112
115.966190	3828.376513	23.695130
116.120475	3842.092978	23.700147
116.432990	3850.796292	23.705165
116.312180	3856.838980	23.710183
117.080988	3846.160812	23.715200
116.968062	3852.375833	23.720218
117.169122	3837.959630	23.725235
117.408378	3838.387035	23.730253
116.975238	3854.260449	23.735271
117.390879	3846.083808	23.740288
117.268597	3854.994041	23.745306
117.558396	3836.245996	23.750323
117.717657	3845.615408	23.755341
117.635618	3835.650761	23.760359
117.911961	3838.885752	23.765376
118.026227	3843.078506	23.770394
118.154822	3833.851398	23.775411
118.180077	3837.045820	23.780429
117.977806	3844.683741	23.785447
118.143418	3844.751289	23.790464
118.153434	3869.440419	23.795482
118.175079	3872.684274	23.800499
118.180490	3874.052627	23.805517
118.473792	3882.849321	23.810535
118.429292	3892.547149	23.815552
118.864653	3895.957722	23.820570
118.698311	3901.459890	23.825587
119.016171	3918.336672	23.830605
119.266535	3926.812923	23.835623
119.685431	3927.745591	23.840640
119.902597	3928.797619	23.845658
120.076584	3931.485784	23.850675
119.444366	3930.053804	23.855693
119.417372	3928.218058	23.860711
119.739543	3937.926252	23.865728
120.306600	3954.209619	23.870746
119.923770	3954.121816	23.875763
120.256655	3950.469725	23.880781
120.522666	3964.263808	23.885799
120.975166	3970.417990	23.890816
120.910388	3967.783684	23.895834
121.160618	3977.104982	23.900851
121.295011	3973.449252	23.905869
121.395072	3960.895250	23.910887
122.005593	3960.448254	23.915904
121.879194	3959.007028	23.920922
122.049331	3968.010878	23.925939
122.372485	3957.740203	23.930957
122.225155	3965.208794	23.935975
121.899672	3955.088041	23.940992
121.958184	3963.548944	23.946010
122.049845	3961.012281	23.951027
122.212542	3954.657782	23.956045
122.677304	3966.796965	23.961063
122.483899	3973.751098	23.966080
122.509360	3984.926932	23.971098
122.692147	3985.927978	23.976115
122.761447	3991.756817	23.981133
122.567850	3997.087932	23.986151
122.947164	3995.175603	23.991168
122.901981	4004.472377	23.996186
123.028471	4007.688993	24.001203
122.950646	4004.411483	24.006221
123.140528	4029.426931	24.011239
123.291055	4033.219955	24.016256
123.731209	4030.184363	24.021274
123.734441	4040.756365	24.026291
124.053821	4054.227834	24.031309
124.076881	4065.055257	24.036327
124.453554	4064.120665	24.041344
124.369658	4056.164741	24.046362
124.265439	4060.822270	24.051379
125.127112	4075.660937	24.056397
124.930238	4090.417219	24.061415
124.614012	4092.098133	24.066432
125.062349	4094.528893	24.071450
124.954892	4101.062835	24.076467
125.173194	4098.490143	24.081485
125.113824	4102.011719	24.086503
125.415552	4109.860547	24.091520
125.453032	4120.687580	24.096538
125.102494	4130.818357	24.101555
125.814834	4122.992722	24.106573
125.736433	4144.504382	24.111591
126.187585	4151.765325	24.116608
126.399760	4160.711111	24.121626
126.115286	4167.700544	24.126643
126.488241	4155.499917	24.131661
126.359951	4175.896908	24.136679
126.878011	4176.509524	24.141696
126.849391	4188.617859	24.146714
127.291203	4192.333379	24.151731
127.445747	4171.548043	24.156749
127.129583	4187.637823	24.161767
127.241385	4186.005001	24.166784
127.295828	4203.504300	24.171802
127.335255	4217.122053	24.176819
127.301877	4204.065935	24.181837
127.240433	4223.806112	24.186855
127.572886	4241.879823	24.191872
128.207612	4242.906194	24.196890
127.925682	4252.892557	24.201907
128.510576	4260.372308	24.206925
128.764879	4268.005439	24.211943
128.553259	4272.406818	24.216960
128.728959	4266.135086	24.221978
128.994972	4266.871493	24.226995
129.416229	4282.283623	24.232013
129.136986	4297.445975	24.237031
128.893517	4288.705692	24.242048
129.495506	4279.857996	24.247066
129.729528	4279.788569	24.252083
130.093660	4285.592937	24.257101
130.276277	4302.333923	24.262119
129.974517	4310.306762	24.267136
130.328731	4305.943454	24.272154
130.308912	4309.499455	24.277171
130.408939	4309.442844	24.282189
130.379670	4317.270390	24.287207
130.587096	4309.337986	24.292224
130.944380	4321.057047	24.297242
130.704888	4324.786586	24.302259
130.802185	4333.013647	24.307277
130.942398	4329.800246	24.312295
131.025406	4337.988733	24.317312
131.395186	4351.188656	24.322330
131.446727	4360.488862	24.327347
131.727707	4343.497082	24.332365
132.176101	4347.785655	24.337383
132.428863	4343.407693	24.342400
132.477135	4337.886360	24.347418
132.527341	4352.558515	24.352435
132.320210	4348.716892	24.357453
132.587362	4362.247315	24.362471
132.362770	4378.641021	24.367488
132.604397	4369.128631	24.372506
132.625965	4378.072352	24.377523
132.745726	4388.307062	24.382541
132.951457	4411.812366	24.387559
133.238967	4419.378626	24.392576
133.271855	4405.748243	24.397594
133.279917	4408.204965	24.402611
133.707705	4413.419180	24.407629
133.710081	4429.275140	24.412647
133.817818	4432.053942	24.417664
134.085396	4421.978059	24.422682
134.229203	4435.968485	24.427699
134.399561	4425.679583	24.432717
134.090876	4427.069859	24.437735
134.238577	4448.078931	24.442752
134.497059	4453.699310	24.447770
134.681452	4453.082919	24.452787
134.612618	4462.009421	24.457805
134.903033	4475.383294	24.462823
134.807823	4474.196724	24.467840
135.178278	4472.989475	24.472858
135.294356	4489.125865	24.477875
135.746155	4495.287462	24.482893
135.593665	4502.422068	24.487911
135.628347	4512.389846	24.492928
136.098675	4502.917338	24.497946
135.923676	4520.234607	24.502963
136.166164	4525.692287	24.507981
136.556253	4525.361451	24.512999
136.319156	4525.450640	24.518016
136.734973	4527.763232	24.523034
137.121969	4548.866556	24.528051
137.055505	4553.402975	24.533069
137.545177	4563.109319	24.538087
137.491360	4564.431266	24.543104
137.691049	4552.445772	24.548122
137.448509	4554.878007	24.553139
137.759100	4561.452927	24.558157
137.480246	4561.971176	24.563175
137.630390	4578.964353	24.568192
138.161418	4582.788787	24.573210
138.258662	4588.710860	24.578227
138.561870	4598.978227	24.583245
138.843002	4617.178244	24.588263
138.785173	4622.983554	24.593280
139.394288	4607.538037	24.598298
139.189049	4616.604638	24.603315
139.224475	4605.191379	24.608333
139.646817	4597.469618	24.613351
139.471214	4607.563756	24.618368
139.531712	4596.280219	24.623386
139.443813	4599.958643	24.628403
139.632345	4612.538397	24.633421
140.159837	4618.539407	24.638439
139.936922	4626.476464	24.643456
140.499480	4618.102934	24.648474
140.438079	4618.474794	24.653491
140.146648	4635.809175	24.658509
140.602055	4647.527927	24.663527
140.553354	4656.406304	24.668544
140.663747	4650.860362	24.673562
140.892337	4666.382067	24.678579
141.126239	4683.264572	24.683597
141.392132	4686.125031	24.688615
141.222548	4687.096078	24.693632
141.272304	4692.407859	24.698650
141.622394	4710.596525	24.703667
141.767098	4720.048423	24.708685
141.984122	4715.299064	24.713703
141.569655	4720.648617	24.718720
141.873630	4730.241802	24.723738
141.922102	4749.619429	24.728755
142.328407	4744.356628	24.733773
142.562521	4765.865248	24.738791
142.674376	4775.809344	24.743808
142.870982	4775.362597	24.748826
142.742322	4779.237635	24.753843
142.860912	4794.287889	24.758861
143.156560	4794.491740	24.763879
143.522521	4799.644693	24.768896
143.788414	4801.235641	24.773914
143.709430	4808.309342	24.778931
144.327870	4824.215326	24.783949
144.443780	4829.453156	24.788967
144.595777	4831.527689	24.793984
144.669653	4822.145284	24.799002
144.414100	4831.837810	24.804019
144.497734	4824.894409	24.809037
144.754829	4825.782750	24.814055
144.762716	4834.885727	24.819072
144.919041	4844.757110	24.824090
145.373797	4846.636427	24.829107
145.059233	4849.407509	24.834125
145.859236	4855.296386	24.839143
145.479575	4869.937286	24.844160
146.249478	4861.467745	24.849178
145.868555	4870.681817	24.854195
146.195695	4867.038743	24.859213
145.984588	4868.556176	24.864231
146.146802	4887.050337	24.869248
146.434930	4890.683670	24.874266
146.765543	4888.000832	24.879283
146.738366	4902.543025	24.884301
146.930832	4906.303303	24.889319
147.083434	4915.758732	24.894336
147.742929	4901.377212	24.899354
148.163487	4902.929869	24.904371
148.032958	4902.133462	24.909389
148.534694	4896.002618	24.914407
148.644178	4900.135810	24.919424
148.558821	4893.097601	24.924442
148.622420	4897.214790	24.929459
148.669486	4900.864556	24.934477
148.787407	4888.067036	24.939495
148.574531	4905.817090	24.944512
148.939588	4914.589844	24.949530
148.715106	4922.969917	24.954547
148.717926	4929.861542	24.959565
148.970977	4932.261885	24.964583
149.094855	4950.312007	24.969600
149.463248	4949.406703	24.974618
149.888879	4950.136311	24.979635
150.029513	4949.179859	24.984653
150.087899	4965.183778	24.989671
150.102526	4975.238664	24.994688
150.502343	4974.891242	24.999706
150.693203	4978.061135	25.004723
150.218627	4977.799156	25.009741
150.889546	4973.241279	25.014759
150.863035	4994.269793	25.019776
151.293164	4999.356234	25.024794
151.966960	4990.126848	25.029811
151.835016	4995.138147	25.034829
152.153235	4993.545762	25.039847
151.951164	5002.415167	25.044864
151.688096	4994.768517	25.049882
152.080975	4987.874466	25.054899
151.945102	4997.243994	25.059917
152.280603	5005.672821	25.064935
152.459642	5011.922477	25.069952
152.463024	5008.552112	25.074970
152.570599	5021.003885	25.079987
152.488402	5016.034810	25.085005
152.978311	5031.670180	25.090023
153.047499	5048.215806	25.095040
152.577124	5044.928095	25.100058
153.087489	5054.931371	25.105075
153.052672	5064.300686	25.110093
153.134675	5065.577265	25.115111
153.726777	5096.083063	25.120128
153.977840	5104.376336	25.125146
154.563401	5096.629575	25.130163
154.489294	5098.699975	25.135181
154.488012	5095.218532	25.140199
154.709876	5101.022433	25.145216
154.685164	5116.454364	25.150234
154.974708	5124.344319	25.155251
154.577447	5121.917067	25.160269
155.099617	5126.324335	25.165287
155.341184	5146.457933	25.170304
155.516107	5150.177082	25.175322
156.005655	5158.559129	25.180339
155.978848	5151.963928	25.185357
156.192339	5167.267332	25.190375
156.347076	5164.727871	25.195392
156.633188	5179.896359	25.200410
156.754712	5172.811834	25.205427
156.737877	5182.687790	25.210445
157.075089	5175.141348	25.215463
156.972555	5186.945342	25.220480
157.068245	5199.704809	25.225498
156.999647	5209.375951	25.230515
157.279235	5215.928734	25.235533
157.658840	5218.797176	25.240551
157.668333	5236.952480	25.245568
157.695612	5234.378270	25.250586
158.122234	5232.841093	25.255603
158.141041	5251.557981	25.260621
157.893507	5259.278138	25.265639
158.262577	5266.787153	25.270656
158.269423	5280.817631	25.275674
158.979824	5279.171076	25.280691
158.769587	5294.659212	25.285709
158.882560	5303.722947	25.290727
159.371776	5307.518283	25.295744
159.399848	5313.632480	25.300762
159.906890	5309.242717	25.305779
159.633152	5332.100562	25.310797
160.281029	5336.192449	25.315815
160.159313	5338.299144	25.320832
160.329626	5343.268992	25.325850
160.581214	5345.359337	25.330867
160.568970	5360.561825	25.335885
160.749311	5363.416937	25.340903
161.177271	5365.925323	25.345920
160.669661	5376.273590	25.350938
161.480215	5381.919919	25.355955
161.339764	5400.607529	25.360973
161.739070	5400.757150	25.365991
161.497977	5401.741696	25.371008
161.553866	5421.376457	25.376026
162.079664	5429.888879	25.381043
161.684433	5444.459651	25.386061
162.234555	5444.032904	25.391079
162.311991	5462.123621	25.396096
162.551450	5469.518019	25.401114
162.558000	5475.861892	25.406131
162.867988	5498.893912	25.411149
163.062497	5489.218560	25.416167
163.272123	5478.333334	25.421184
163.542148	5509.918103	25.426202
163.835902	5507.783936	25.431219
163.949124	5517.114744	25.436237
164.203966	5513.645781	25.441255
164.231716	5504.777841	25.446272
164.361274	5513.920850	25.451290
164.531930	5527.947955	25.456307
164.439315	5529.662347	25.461325
164.753295	5540.908303	25.466343
164.937050	5544.021210	25.471360
164.857809	5554.820583	25.476378
165.092670	5564.720324	25.481395
165.041838	5578.254230	25.486413
165.149305	5581.152208	25.491431
165.163245	5601.981063	25.496448
165.661749	5604.812493	25.501466
166.010721	5624.613819	25.506483
166.350200	5641.095465	25.511501
166.479911	5630.551053	25.516519
167.031310	5635.550607	25.521536
166.830022	5636.187525	25.526554
166.990898	5644.938698	25.531571
167.217574	5665.330615	25.536589
167.067106	5661.224858	25.541607
167.700609	5660.981151	25.546624
167.504676	5679.025393	25.551642
167.796999	5677.794025	25.556659
167.580088	5680.727807	25.561677
167.807510	5694.407750	25.566695
168.459147	5695.723620	25.571712
168.479244	5713.603626	25.576730
168.903534	5698.733568	25.581747
168.808996	5705.431421	25.586765
168.928059	5730.323518	25.591783
169.284634	5723.781724	25.596800
169.441004	5723.253429	25.601818
169.772878	5717.131595	25.606835
169.816986	5739.628476	25.611853
169.975643	5755.892195	25.616871
170.132961	5754.726573	25.621888
170.188461	5759.164312	25.626906
170.387973	5749.418662	25.631923
170.458546	5774.883594	25.636941
170.354661	5788.723421	25.641959
170.830783	5782.260977	25.646976
170.742819	5807.868083	25.651994
170.825815	5815.788771	25.657011
171.006249	5820.114405	25.662029
171.677984	5839.648930	25.667047
171.842912	5836.047556	25.672064
171.813767	5854.205265	25.677082
172.056128	5857.222648	25.682100
171.951952	5860.655186	25.687117
172.499104	5874.030911	25.692135
172.722176	5878.200620	25.697152
172.697513	5878.401794	25.702170
172.630613	5896.497303	25.707188
172.926826	5905.975146	25.712205
173.201474	5902.505959	25.717223
173.387133	5932.419327	25.722240
172.883371	5946.929044	25.727258
173.164759	5947.126622	25.732276
173.503812	5961.085963	25.737293
173.930317	5965.210865	25.742311
175.262091	5946.751869	25.747328
175.196636	5950.852973	25.752346
175.581306	5926.966439	25.757364
175.689493	5934.208808	25.762381
175.797114	5912.000255	25.767399
176.130179	5919.726647	25.772416
175.919662	5923.484035	25.777434
176.381936	5925.105479	25.782452
176.145618	5920.100295	25.787469
176.035530	5911.748072	25.792487
176.058103	5922.689875	25.797504
176.012749	5917.868765	25.802522
176.481740	5910.591494	25.807540
176.681302	5919.604178	25.812557
176.427037	5946.415827	25.817575
176.903605	5944.567845	25.822592
176.810871	5948.206429	25.827610
177.311790	5967.689163	25.832628
177.197317	5972.838850	25.837645
177.273276	5983.449692	25.842663
177.237733	5995.508583	25.847680
177.500870	6021.135668	25.852698
177.356707	6021.660719	25.857716
177.403644	6040.512488	25.862733
178.286331	6063.011473	25.867751
178.306153	6080.514673	25.872768
178.191497	6085.782570	25.877786
178.664934	6097.459246	25.882804
178.898318	6104.043709	25.887821
178.863382	6135.919840	25.892839
179.383587	6132.731149	25.897856
179.622620	6136.501315	25.902874
179.632702	6158.552353	25.907892
180.065091	6162.080890	25.912909
180.200252	6164.350579	25.917927
180.816536	6158.845282	25.922944
181.374342	6150.062182	25.927962
181.595468	6154.965561	25.932980
181.968246	6164.273315	25.937997
182.011594	6154.267459	25.943015
182.456115	6143.252958	25.948032
182.217418	6129.075498	25.953050
182.235624	6121.271294	25.958068
182.630941	6112.861765	25.963085
182.000529	6131.148053	25.968103
182.598245	6137.674355	25.973120
182.325776	6162.543190	25.978138
182.523733	6159.322189	25.983156
182.701556	6166.666511	25.988173
182.686464	6182.672060	25.993191
183.088209	6185.264488	25.998208
182.917169	6204.968648	26.003226
183.245319	6220.005135	26.008244
183.264089	6231.924436	26.013261
183.129218	6254.734547	26.018279
183.481223	6260.108477	26.023296
183.698109	6277.501176	26.028314
183.343325	6299.626427	26.033332
183.892123	6312.799834	26.038349
184.284518	6337.060688	26.043367
184.893399	6357.630220	26.048384
184.745265	6375.330206	26.053402
185.304814	6384.822080	26.058420
185.451345	6384.388340	26.063437
185.196188	6408.702554	26.068455
185.851369	6418.790548	26.073472
186.293294	6426.081657	26.078490
186.178142	6449.480282	26.083508
186.395886	6449.308016	26.088525
186.104351	6455.835709	26.093543
186.288609	6473.695599	26.098560
186.281624	6480.610009	26.103578
186.686910	6499.067248	26.108596
187.049541	6512.441098	26.113613
187.259743	6522.102947	26.118631
187.552733	6537.142428	26.123648
187.514436	6548.105805	26.128666
187.781021	6553.220718	26.133684
187.653380	6561.082262	26.138701
187.941938	6579.329000	26.143719
188.419420	6590.024759	26.148736
188.510875	6602.370977	26.153754
188.670087	6612.558834	26.158772
189.244663	6616.374181	26.163789
189.164578	6643.750372	26.168807
189.415585	6652.691916	26.173824
189.843441	6652.757262	26.178842
189.669000	6653.195996	26.183860
190.728785	6663.673754	26.188877
190.498426	6681.992655	26.193895
190.472236	6684.023793	26.198912
190.768961	6690.223058	26.203930
190.961085	6701.916208	26.208948
191.369287	6712.463670	26.213965
191.152837	6721.033178	26.218983
191.999871	6699.074010	26.224000
192.192573	6719.624949	26.229018
191.908147	6734.829086	26.234036
192.662706	6729.191138	26.239053
192.593709	6739.765137	26.244071
193.030452	6725.739561	26.249088
192.977636	6733.814025	26.254106
193.348786	6759.985954	26.259124
193.531657	6751.723235	26.264141
193.302703	6758.016961	26.269159
193.817600	6768.523103	26.274176
193.251099	6772.867564	26.279194
193.168308	6782.006422	26.284212
193.845972	6793.972620	26.289229
194.322959	6810.071110	26.294247
194.193192	6821.784753	26.299264
194.403504	6836.398747	26.304282
194.483673	6850.535794	26.309300
194.972207	6853.289561	26.314317
194.756181	6866.473942	26.319335
195.365495	6882.778939	26.324352
195.634950	6884.999639	26.329370
195.974274	6907.074990	26.334388
196.091229	6911.103499	26.339405
196.278458	6909.643756	26.344423
196.591387	6922.256672	26.349440
197.171397	6921.708359	26.354458
196.969019	6938.141192	26.359476
197.350765	6924.342762	26.364493
197.405381	6944.332496	26.369511
197.702991	6937.882710	26.374528
197.464209	6951.239501	26.379546
197.305903	6957.212803	26.384564
197.915564	6965.189125	26.389581
197.693833	6985.257120	26.394599
198.129566	6985.864646	26.399616
198.821682	7000.372744	26.404634
198.487995	7013.301115	26.409652
198.941732	7014.711429	26.414669
198.910075	7035.554472	26.419687
199.039934	7046.996720	26.424704
199.487878	7049.847848	26.429722
199.753079	7066.979760	26.434740
200.322697	7068.633117	26.439757
200.533313	7069.078773	26.444775
200.624895	7068.638392	26.449792
201.252145	7046.313557	26.454810
200.951519	7061.789290	26.459828
201.451730	7053.739919	26.464845
201.340505	7069.262169	26.469863
201.405785	7082.669369	26.474880
202.078457	7082.146614	26.479898
202.004377	7087.653851	26.484916
202.291759	7082.992133	26.489933
202.403098	7071.125751	26.494951
202.497685	7088.950037	26.499968
202.911723	7100.749179	26.504986
202.613543	7110.601406	26.510004
202.633039	7109.140371	26.515021
202.795093	7126.688833	26.520039
203.103350	7142.730631	26.525056
203.464127	7139.664332	26.530074
203.769466	7164.594685	26.535092
203.953224	7164.578506	26.540109
204.111418	7165.801640	26.545127
203.943133	7195.021617	26.550144
204.279030	7191.682969	26.555162
204.521021	7219.584789	26.560180
204.486079	7223.225876	26.565197
204.683585	7237.799047	26.570215
204.957394	7257.857516	26.575232
205.658635	7260.338138	26.580250
205.741132	7285.155261	26.585268
206.126185	7285.841325	26.590285
206.614102	7285.911664	26.595303
206.539043	7297.047077	26.600320
207.188827	7304.430875	26.605338
206.911416	7318.701006	26.610356
207.205056	7317.652830	26.615373
206.968364	7320.484647	26.620391
207.102028	7345.317781	26.625408
207.662181	7340.768201	26.630426
207.637611	7374.484326	26.635444
207.809409	7382.702177	26.640461
208.074342	7392.923382	26.645479
208.495093	7394.253356	26.650496
208.571689	7410.782895	26.655514
208.574604	7432.212262	26.660532
209.092877	7440.228429	26.665549
208.976701	7451.436160	26.670567
209.268052	7466.785570	26.675584
209.519889	7472.281323	26.680602
209.933949	7494.285211	26.685620
209.688996	7499.895812	26.690637
210.369540	7519.247430	26.695655
210.187063	7538.051663	26.700672
210.609389	7540.514084	26.705690
210.945014	7562.976144	26.710708
211.123803	7558.055852	26.715725
211.300531	7577.636975	26.720743
211.236220	7595.620562	26.725760
211.338409	7603.529503	26.730778
211.605022	7634.347930	26.735796
211.569461	7643.234462	26.740813
211.992632	7657.504283	26.745831
212.169220	7681.448592	26.750848
212.694244	7685.316550	26.755866
212.857467	7709.407270	26.760884
213.103181	7726.581729	26.765901
213.324960	7732.633955	26.770919
213.761024	7749.715372	26.775936
214.245064	7748.035308	26.780954
214.097428	7761.433558	26.785972
214.183014	7777.747729	26.790989
214.478998	7784.496575	26.796007
214.807567	7782.879361	26.801024
215.209766	7793.835786	26.806042
215.421767	7810.240052	26.811060
215.410686	7811.073881	26.816077
215.442773	7818.139920	26.821095
215.659781	7829.991248	26.826112
216.120796	7840.549596	26.831130
215.960547	7842.101389	26.836148
216.897977	7857.282390	26.841165
217.273713	7849.146176	26.846183
217.487364	7854.439665	26.851200
217.854259	7853.477748	26.856218
217.831986	7853.876263	26.861236
217.993249	7859.884240	26.866253
218.167670	7858.878682	26.871271
218.027068	7877.729134	26.876288
218.302902	7883.424271	26.881306
218.610797	7886.497327	26.886324
218.526435	7905.179350	26.891341
218.884774	7908.728468	26.896359
218.457752	7924.356008	26.901376
219.262094	7940.003469	26.906394
219.682211	7936.912195	26.911412
219.760835	7957.877546	26.916429
219.708684	7966.525975	26.921447
220.074356	7980.191228	26.926464
220.478518	7981.491715	26.931482
220.531360	7992.377139	26.936500
220.740405	8013.909314	26.941517
221.090652	8029.088002	26.946535
221.478707	8034.851984	26.951552
221.567250	8050.842983	26.956570
221.910375	8058.146540	26.961588
222.032206	8056.250927	26.966605
222.428005	8073.422094	26.971623
222.467668	8093.744233	26.976640
222.703257	8094.050284	26.981658
222.912544	8105.008256	26.986676
223.496750	8124.090681	26.991693
223.512409	8113.767593	26.996711
223.225596	8130.754480	27.001728
223.499918	8138.275101	27.006746
223.867965	8149.151585	27.011764
224.493642	8156.624866	27.016781
224.864020	8164.132690	27.021799
224.595250	8175.797951	27.026816
224.966785	8186.977942	27.031834
225.054400	8212.035914	27.036852
224.497822	8213.791443	27.041869
225.275048	8230.356666	27.046887
225.497993	8257.485989	27.051904
225.865602	8270.150762	27.056922
226.370093	8277.270065	27.061940
226.457040	8299.192355	27.066957
226.588515	8305.667846	27.071975
226.330707	8325.611969	27.076992
226.635758	8338.440796	27.082010
226.711557	8367.203293	27.087028
226.865433	8390.639631	27.092045
227.257811	8400.246363	27.097063
227.448121	8422.413174	27.102080
228.442920	8407.257543	27.107098
228.499443	8423.739478	27.112116
229.167104	8435.922853	27.117133
229.395326	8434.159975	27.122151
229.139859	8451.668199	27.127168
229.662167	8441.063000	27.132186
229.724417	8452.378065	27.137204
230.105976	8464.983958	27.142221
230.384893	8464.762127	27.147239
230.114041	8468.399368	27.152256
230.557983	8482.707444	27.157274
230.464876	8493.727742	27.162292
230.696679	8506.968257	27.167309
230.777443	8518.475651	27.172327
231.147976	8538.057264	27.177344
231.161765	8561.205183	27.182362
231.381574	8570.758766	27.187380
231.380197	8592.152593	27.192397
232.061024	8609.137552	27.197415
231.881158	8636.080004	27.202432
232.267204	8653.861555	27.207450
232.586437	8664.688210	27.212468
232.741649	8689.300865	27.217485
233.238332	8709.079934	27.222503
233.349897	8726.422706	27.227520
234.196872	8727.051787	27.232538
234.277192	8741.788388	27.237556
234.403337	8750.444642	27.242573
234.896532	8753.974697	27.247591
234.998175	8779.969437	27.252608
235.209373	8782.949238	27.257626
235.478248	8799.551464	27.262644
235.604065	8815.567758	27.267661
236.084362	8818.219265	27.272679
235.871594	8833.411913	27.277696
236.407747	8846.860527	27.282714
236.817477	8860.850073	27.287732
236.808547	8870.867227	27.292749
237.512576	8878.583853	27.297767
236.905163	8891.712826	27.302784
237.258818	8904.654561	27.307802
237.650748	8927.743335	27.312820
237.719352	8937.894959	27.317837
237.982960	8946.365414	27.322855
238.019348	8978.361425	27.327872
238.171106	8993.693750	27.332890
238.771244	9007.230339	27.337908
238.746708	9022.383226	27.342925
239.479765	9036.717027	27.347943
239.551553	9052.736232	27.352960
239.968914	9066.185862	27.357978
240.415824	9081.463720	27.362996
240.704491	9093.145742	27.368013
241.058935	9086.870780	27.373031
240.978798	9091.636063	27.378048
241.412727	9106.479681	27.383066
241.869398	9105.377525	27.388084
241.961689	9115.707300	27.393101
242.484902	9129.482074	27.398119
242.520750	9139.476988	27.403136
242.398749	9150.541926	27.408154
242.776364	9143.315409	27.413172
242.775029	9170.869552	27.418189
243.299786	9169.543382	27.423207
243.862842	9180.088822	27.428224
243.618644	9201.714446	27.433242
244.207955	9204.078491	27.438260
244.137634	9203.383720	27.443277
244.286652	9227.984053	27.448295
244.511168	9241.443813	27.453312
244.411527	9252.299498	27.458330
244.870905	9266.099177	27.463348
244.709856	9285.735364	27.468365
245.095529	9292.161933	27.473383
245.240127	9315.799687	27.478400
245.505081	9334.857042	27.483418
245.735640	9347.940906	27.488436
245.726941	9376.439595	27.493453
246.070288	9394.016365	27.498471
246.397919	9403.968481	27.503488
246.529199	9423.052089	27.508506
246.939881	9435.159186	27.513524
246.395248	9469.133141	27.518541
247.204688	9477.262678	27.523559
247.747917	9498.239514	27.528576
247.638872	9530.204067	27.533594
247.995571	9547.186372	27.538612
248.397445	9569.132130	27.543629
248.847051	9586.903372	27.548647
249.005472	9597.902333	27.553664
248.823378	9632.344218	27.558682
249.564480	9637.109507	27.563700
249.944454	9664.156831	27.568717
250.340192	9678.172265	27.573735
250.668230	9689.435379	27.578752
250.914436	9714.571767	27.583770
251.278500	9726.309477	27.588788
251.222841	9733.718664	27.593805
251.471683	9747.678997	27.598823
251.865455	9757.497448	27.603840
251.822123	9789.316885	27.608858
252.415095	9786.657410	27.613876
252.628974	9815.613059	27.618893
252.847450	9822.123555	27.623911
253.054255	9839.933054	27.628928
253.495682	9850.008347	27.633946
253.742994	9861.025807	27.638964
254.329942	9865.748240	27.643981
254.828522	9877.488134	27.648999
255.332823	9872.899868	27.654016
255.385521	9894.076891	27.659034
255.645396	9891.330936	27.664052
255.779426	9905.939149	27.669069
256.139330	9903.251415	27.674087
256.312049	9901.373918	27.679104
256.033991	9929.750537	27.684122
256.516233	9919.170724	27.689140
256.912087	9935.429246	27.694157
256.934246	9943.826902	27.699175
257.316694	9948.318633	27.704192
257.243508	9966.001474	27.709210
258.066214	9979.167883	27.714228
257.548291	9999.752092	27.719245
257.882138	10000.479883	27.724263
258.281002	10023.353228	27.729280
258.509555	10044.770664	27.734298
258.678697	10044.486699	27.739316
258.585124	10065.288041	27.744333
259.280858	10087.948290	27.749351
259.754689	10106.726063	27.754368
259.539590	10127.799777	27.759386
259.738528	10150.040813	27.764404
260.110177	10164.841403	27.769421
260.208582	10192.736032	27.774439
260.335655	10200.337239	27.779456
260.804787	10228.791928	27.784474
261.135944	10245.575172	27.789492
261.504160	10256.484582	27.794509
261.815027	10286.457012	27.799527
262.260956	10278.095206	27.804544
262.161153	10299.235861	27.809562
262.877685	10308.442462	27.814580
262.787740	10330.924760	27.819597
262.946744	10346.967007	27.824615
263.272282	10347.372400	27.829632
263.187085	10369.843721	27.834650
263.949230	10369.956774	27.839668
264.355344	10395.435576	27.844685
264.354529	10404.648753	27.849703
264.454095	10416.584539	27.854720
264.569691	10438.226889	27.859738
264.882188	10452.492393	27.864756
264.817065	10479.500803	27.869773
265.136944	10494.710517	27.874791
265.880985	10509.659120	27.879808
265.934721	10539.961514	27.884826
266.422393	10545.617686	27.889844
266.655016	10568.229502	27.894861
266.766213	10590.954488	27.899879
267.221014	10607.155052	27.904896
267.340747	10627.481278	27.909914
267.886692	10638.541049	27.914932
268.081311	10672.610585	27.919949
268.203167	10694.189999	27.924967
268.446234	10695.872016	27.929984
268.957344	10724.285155	27.935002
269.396801	10725.597350	27.940020
269.763785	10739.199358	27.945037
270.273963	10755.943152	27.950055
270.199879	10757.580173	27.955072
270.403357	10772.326539	27.960090
270.745190	10780.625826	27.965108
271.160359	10796.241493	27.970125
271.774214	10810.566760	27.975143
271.868791	10814.745728	27.980160
271.502418	10842.504403	27.985178
271.859736	10853.041801	27.990196
272.200409	10877.468641	27.995213
272.669438	10884.424835	28.000231
273.284068	10901.255424	28.005248
273.413797	10920.968199	28.010266
273.691685	10925.129347	28.015284
273.910430	10939.893814	28.020301
273.928603	10940.289624	28.025319
274.384249	10961.306563	28.030336
274.432637	10978.648870	28.035354
274.844864	10991.394266	28.040372
274.837028	11012.362215	28.045389
275.190350	11034.711973	28.050407
275.665206	11051.368976	28.055424
275.585449	11066.227271	28.060442
276.224709	11091.086999	28.065460
276.116067	11105.816192	28.070477
276.282132	11132.409111	28.075495
276.654419	11152.842948	28.080512
276.820536	11175.687267	28.085530
276.921371	11196.564917	28.090548
277.442547	11205.936069	28.095565
277.757924	11232.794282	28.100583
278.390178	11255.673151	28.105600
278.512046	11278.203515	28.110618
278.625625	11289.512838	28.115636
278.970605	11307.116644	28.120653
279.016972	11330.876100	28.125671
280.042116	11345.866240	28.130688
279.747750	11380.537715	28.135706
280.323199	11380.955984	28.140724
282.528913	11357.285929	28.145741
283.160487	11334.452573	28.150759
283.267767	11315.404626	28.155776
283.452657	11304.227260	28.160794
283.506115	11278.935742	28.165812
283.748718	11274.173113	28.170829
283.656219	11281.356708	28.175847
283.860647	11266.914333	28.180864
283.919430	11274.737755	28.185882
283.769885	11273.060973	28.190900
283.966434	11269.917980	28.195917
284.006605	11271.143711	28.200935
283.728330	11271.530477	28.205952
284.054254	11294.877866	28.210970
283.953865	11306.673411	28.215988
284.416446	11327.599860	28.221005
284.399201	11359.154122	28.226023
284.909506	11371.464377	28.231040
284.675612	11398.461392	28.236058
284.923967	11428.403788	28.241076
285.242727	11462.448852	28.246093
285.613394	11495.265724	28.251111
286.171863	11517.769587	28.256128
286.399150	11553.457807	28.261146
286.404162	11584.172075	28.266164
286.831991	11609.877678	28.271181
286.810118	11627.851633	28.276199
287.316533	11662.348131	28.281216
287.270539	11704.579025	28.286234
288.088910	11729.969389	28.291252
288.388611	11766.564731	28.296269
288.678706	11786.907448	28.301287
289.169373	11815.264452	28.306304
289.274960	11843.323046	28.311322
289.481606	11865.436739	28.316340
289.780050	11892.766876	28.321357
290.046507	11919.238831	28.326375
290.605927	11933.780575	28.331392
291.091462	11969.921612	28.336410
291.498631	11991.512088	28.341428
292.235037	12008.312576	28.346445
292.260660	12021.367266	28.351463
292.379359	12049.676169	28.356480
292.481184	12069.869300	28.361498
292.723389	12090.949960	28.366516
293.182770	12110.059456	28.371533
293.130803	12138.352743	28.376551
293.627909	12163.359081	28.381568
294.188847	12181.685938	28.386586
294.238163	12197.953104	28.391604
295.155475	12222.423279	28.396621
295.434431	12240.346359	28.401639
296.242885	12237.246503	28.406656
296.736287	12239.145535	28.411674
296.657800	12262.602477	28.416692
297.199724	12269.525104	28.421709
297.230589	12280.067245	28.426727
297.556392	12275.224317	28.431744
297.630445	12294.081302	28.436762
297.806058	12300.176023	28.441780
298.677730	12325.504892	28.446797
298.324037	12350.088709	28.451815
298.260476	12361.464453	28.456832
298.963489	12365.052656	28.461850
299.104314	12394.645953	28.466868
299.631832	12401.218040	28.471885
299.581046	12427.081671	28.476903
299.734770	12437.450645	28.481920
299.504331	12458.225793	28.486938
299.830802	12483.667545	28.491956
300.252968	12502.203771	28.496973
300.532854	12529.427754	28.501991
300.810039	12558.987665	28.507008
301.128051	12585.277222	28.512026
301.315057	12606.842060	28.517044
302.146230	12624.117543	28.522061
302.432332	12640.492372	28.527079
302.762948	12670.836276	28.532096
302.775490	12681.525125	28.537114
303.215786	12710.278155	28.542132
303.578252	12724.935279	28.547149
303.499137	12749.179391	28.552167
304.140446	12765.993317	28.557184
304.604301	12786.514864	28.562202
304.521770	12809.708516	28.567220
305.291469	12814.789145	28.572237
305.610081	12847.526001	28.577255
305.988171	12861.187839	28.582272
306.572869	12877.423476	28.587290
306.355210	12906.758927	28.592308
307.222984	12926.728173	28.597325
307.375482	12943.276789	28.602343
307.450080	12955.726825	28.607360
308.129257	12968.509809	28.612378
308.118506	12988.628229	28.617396
308.775760	13000.787670	28.622413
308.933433	13021.470693	28.627431
309.033792	13038.633218	28.632448
309.055387	13053.965025	28.637466
309.169373	13079.855899	28.642484
309.712611	13106.723492	28.647501
309.778155	13138.640946	28.652519
310.040260	13144.299269	28.657536
310.680374	13176.212750	28.662554
310.743343	13207.722602	28.667572
311.331139	13220.248331	28.672589
311.191291	13254.288240	28.677607
311.639481	13286.922505	28.682624
312.209579	13312.378664	28.687642
312.478232	13345.479407	28.692660
312.962574	13359.741783	28.697677
313.241367	13388.656798	28.702695
313.167369	13401.150771	28.707712
313.792523	13431.803328	28.712730
314.130415	13468.561634	28.717748
314.434182	13483.906855	28.722765
314.766549	13503.017031	28.727783
314.895116	13529.174109	28.732800
315.478349	13549.114171	28.737818
315.219442	13587.926081	28.742836
315.651486	13607.522554	28.747853
316.103575	13645.444263	28.752871
316.795006	13665.259327	28.757888
316.897461	13682.447396	28.762906
316.954048	13710.540988	28.767924
318.006830	13728.877721	28.772941
318.222836	13748.683611	28.777959
318.748259	13769.062213	28.782976
318.834075	13786.557321	28.787994
318.777739	13816.991281	28.793012
319.174108	13839.244773	28.798029
319.572232	13858.204178	28.803047
320.020896	13882.491528	28.808064
320.464160	13890.056914	28.813082
320.781020	13915.278709	28.818100
320.570263	13933.493041	28.823117
321.467299	13953.305821	28.828135
321.582555	13986.548394	28.833152
322.015917	13992.199052	28.838170
322.253834	14028.628505	28.843188
322.545093	14033.889870	28.848205
322.566388	14046.806636	28.853223
323.496614	14050.994190	28.858240
323.941108	14067.727114	28.863258
324.041075	14074.482809	28.868276
324.711140	14098.621804	28.873293
325.291465	14108.492300	28.878311
325.142112	14122.113585	28.883328
325.505864	14134.737129	28.888346
325.601568	14153.860590	28.893364
325.869435	14168.868849	28.898381
325.854327	14187.605720	28.903399
326.116851	14208.794494	28.908416
326.709502	14227.617997	28.913434
326.650726	14264.620504	28.918452
326.949004	14285.764038	28.923469
327.783589	14304.774389	28.928487
327.450353	14339.464909	28.933504
327.850495	14361.144808	28.938522
328.046077	14394.513557	28.943540
328.534373	14421.217505	28.948557
329.128684	14453.027620	28.953575
329.242699	14481.614179	28.958592
329.888661	14491.530742	28.963610
330.564688	14513.699296	28.968628
331.094065	14532.776375	28.973645
331.403498	14549.325766	28.978663
332.048988	14570.348947	28.983680
332.331413	14578.165175	28.988698
332.440711	14598.732146	28.993716
332.672098	14602.768008	28.998733
332.750345	14629.988016	29.003751
333.072280	14645.640222	29.008768
333.725182	14661.511699	29.013786
333.457586	14689.180121	29.018804
333.810428	14716.605253	29.023821
334.248662	14739.034265	29.028839
334.417681	14772.423957	29.033856
334.782622	14797.169454	29.038874
335.296929	14816.427465	29.043892
335.700183	14841.565414	29.048909
335.645262	14871.446313	29.053927
336.371952	14898.481819	29.058944
336.875664	14913.363322	29.063962
337.252397	14942.444489	29.068980
337.520930	14966.213316	29.073997
337.905991	14981.081492	29.079015
338.222959	14994.695383	29.084032
338.479553	15023.144145	29.089050
338.656927	15060.169107	29.094068
338.888430	15087.514145	29.099085
339.124199	15106.159954	29.104103
339.103739	15139.394310	29.109120
339.773722	15162.794119	29.114138
339.516517	15203.284976	29.119156
339.999193	15227.860256	29.124173
340.518898	15265.312683	29.129191
340.829488	15303.767678	29.134208
341.194857	15325.331691	29.139226
341.818903	15361.662136	29.144244
342.147145	15397.805378	29.149261
342.981946	15415.489880	29.154279
342.976470	15451.248932	29.159296
343.409493	15465.163893	29.164314
343.654794	15499.398238	29.169332
344.001772	15526.642863	29.174349
344.117053	15542.788915	29.179367
344.247035	15578.338178	29.184384
344.700902	15595.966367	29.189402
344.773846	15630.910517	29.194420
345.176593	15665.636033	29.199437
345.560769	15684.429648	29.204455
345.577787	15730.657628	29.209472
346.203669	15744.432034	29.214490
346.926099	15782.463518	29.219508
346.748158	15811.747120	29.224525
347.168977	15842.411345	29.229543
347.373022	15881.519013	29.234560
347.990623	15907.210903	29.239578
348.294054	15949.670538	29.244596
348.757121	15979.404352	29.249613
349.795827	16010.918274	29.254631
349.694680	16033.705032	29.259648
350.392890	16055.124870	29.264666
350.776109	16080.335818	29.269684
350.893582	16108.339856	29.274701
351.502730	16129.773010	29.279719
351.542155	16159.140911	29.284736
351.888830	16174.095355	29.289754
351.934164	16217.985623	29.294772
351.960016	16233.426874	29.299789
352.881069	16278.913558	29.304807
352.977286	16306.549474	29.309824
353.230487	16340.494226	29.314842
353.922732	16380.875961	29.319860
354.014656	16412.142833	29.324877
354.605376	16442.032815	29.329895
354.729621	16475.591020	29.334912
355.286536	16502.569101	29.339930
355.825068	16536.964954	29.344948
356.151082	16573.177344	29.349965
356.278903	16606.747831	29.354983
356.659711	16645.695539	29.360000
356.937791	16671.497037	29.365018
357.229647	16698.145895	29.370036
358.333742	16727.441983	29.375053
360.972370	16692.508863	29.380071
361.430857	16701.770667	29.385088
361.977356	16701.927536	29.390106
362.599940	16680.867869	29.395124
362.418198	16673.726240	29.400141
362.758565	16661.702901	29.405159
362.572526	16669.377269	29.410176
362.716525	16664.071473	29.415194
362.743529	16667.389920	29.420212
362.667504	16669.989368	29.425229
363.035334	16682.790741	29.430247
362.767895	16711.271144	29.435264
363.143622	16730.313254	29.440282
363.285347	16745.860262	29.445300
363.460044	16773.412990	29.450317
363.736886	16790.409833	29.455335
363.820830	16836.492653	29.460352
364.226405	16857.903826	29.465370
364.631341	16889.548355	29.470388
364.841232	16936.442809	29.475405
365.324027	16968.938361	29.480423
365.234672	17008.500963	29.485440
365.551121	17049.175321	29.490458
366.364004	17082.043441	29.495476
366.429498	17113.763698	29.500493
367.220559	17138.977876	29.505511
367.203057	17191.366418	29.510528
367.805174	17209.651101	29.515546
368.324718	17242.536741	29.520564
368.989882	17256.173482	29.525581
369.987894	17276.395977	29.530599
370.497984	17277.140565	29.535616
371.287012	17268.254802	29.540634
371.787427	17293.886355	29.545652
372.011307	17299.637592	29.550669
372.551052	17296.185818	29.555687
372.822602	17293.434343	29.560704
373.253553	17314.602293	29.565722
373.567393	17316.930584	29.570740
373.336217	17333.723904	29.575757
373.950327	17352.079265	29.580775
373.911021	17359.724848	29.585792
374.088715	17383.395600	29.590810
374.323739	17401.812409	29.595828
374.207426	17427.756265	29.600845
374.381085	17464.246551	29.605863
374.854144	17503.871393	29.610880
375.299519	17539.607357	29.615898
376.091805	17566.224932	29.620916
375.846195	17613.507502	29.625933
376.009092	17639.317033	29.630951
376.110915	17680.362777	29.635968
376.556088	17721.201836	29.640986
376.922045	17769.469376	29.646004
377.116679	17819.704450	29.651021
377.947525	17856.748510	29.656039
377.814510	17897.613105	29.661056
378.229308	17947.588148	29.666074
378.856359	17995.395233	29.671092
378.846261	18044.233632	29.676109
379.405584	18085.897994	29.681127
379.838782	18137.229404	29.686144
380.071824	18191.404949	29.691162
381.093358	18225.123469	29.696180
381.511597	18273.412161	29.701197
382.030569	18293.176342	29.706215
382.561382	18339.085056	29.711232
382.813650	18374.998346	29.716250
383.554811	18404.546871	29.721268
383.827148	18444.874124	29.726285
384.583757	18464.600613	29.731303
384.909166	18493.515267	29.736320
385.520428	18520.246417	29.741338
385.945486	18550.076291	29.746356
386.199699	18579.855774	29.751373
386.648282	18613.815287	29.756391
387.200230	18629.001123	29.761408
386.894224	18668.743957	29.766426
387.757768	18695.773998	29.771444
387.530992	18725.996220	29.776461
387.921038	18761.605272	29.781479
389.081039	18786.213646	29.786496
389.749109	18793.021945	29.791514
390.354504	18821.800803	29.796532
390.663784	18843.068159	29.801549
391.105405	18859.322458	29.806567
391.795190	18880.999600	29.811584
391.794003	18913.782715	29.816602
392.257243	18920.924620	29.821620
392.210982	18944.374672	29.826637
392.419084	18970.401039	29.831655
392.854842	18998.900967	29.836672
392.846453	19021.353229	29.841690
393.221412	19040.866336	29.846708
393.498134	19086.874492	29.851725
394.004210	19119.688836	29.856743
394.145394	19146.320930	29.861760
394.586448	19182.617642	29.866778
394.942783	19206.396891	29.871796
394.948001	19239.058187	29.876813
395.055668	19278.140989	29.881831
395.692360	19318.950575	29.886848
396.107453	19370.470085	29.891866
396.446906	19404.020519	29.896884
396.703281	19450.996309	29.901901
397.403925	19476.861249	29.906919
398.005659	19521.615301	29.911936
398.231231	19556.644825	29.916954
398.839781	19584.845888	29.921972
399.060433	19624.617019	29.926989
399.863734	19652.934044	29.932007
401.053952	19679.968180	29.937024
400.879144	19700.431015	29.942042
401.909251	19724.077015	29.947060
402.299141	19759.815920	29.952077
402.438805	19782.055423	29.957095
402.997904	19812.685098	29.962112
402.725288	19844.444633	29.967130
402.963248	19864.069745	29.972148
403.480882	19900.823535	29.977165
403.908673	19930.418935	29.982183
404.257268	19982.730198	29.987200
404.721788	20013.546220	29.992218
405.266308	20039.122648	29.997236
405.425689	20073.342848	30.002253
405.973258	20118.742856	30.007271
406.575133	20142.086927	30.012288
406.895004	20178.185203	30.017306
408.275838	20177.025835	30.022324
408.872000	20197.376983	30.027341
409.249784	20221.453665	30.032359
409.798020	20241.741881	30.037376
409.687823	20275.797583	30.042394
410.047677	20283.594196	30.047412
410.539697	20310.947132	30.052429
410.661007	20336.726744	30.057447
411.148604	20357.206482	30.062464
411.383522	20399.669930	30.067482
411.604462	20422.579455	30.072500
412.235726	20454.461187	30.077517
412.094974	20494.554549	30.082535
412.590123	20523.885974	30.087552
412.671707	20561.615468	30.092570
413.027342	20597.060710	30.097588
413.489829	20640.579573	30.102605
413.669438	20687.137996	30.107623
414.351860	20718.519820	30.112640
415.199331	20751.275928	30.117658
415.741576	20779.075358	30.122676
416.891901	20796.120404	30.127693
418.621552	20786.408078	30.132711
418.934166	20800.629744	30.137728
419.116973	20792.509762	30.142746
419.676441	20804.617136	30.147764
419.619823	20817.232047	30.152781
420.156838	20825.660106	30.157799
420.114837	20840.410549	30.162816
420.283340	20866.585182	30.167834
420.522931	20881.542731	30.172852
420.887068	20901.895436	30.177869
421.431073	20943.031823	30.182887
421.524543	20951.577763	30.187904
421.356333	20993.803794	30.192922
421.924067	21023.912371	30.197940
421.657492	21051.267955	30.202957
421.664996	21094.371640	30.207975
422.381455	21123.597980	30.212992
422.294141	21180.004329	30.218010
422.714307	21216.436623	30.223028
423.409843	21275.614375	30.228045
423.342818	21318.852417	30.233063
423.771972	21363.239562	30.238080
423.757081	21423.021452	30.243098
424.291238	21479.095376	30.248116
424.758456	21537.545684	30.253133
425.260459	21603.361608	30.258151
425.698965	21657.071154	30.263168
426.116067	21718.770594	30.268186
426.706531	21766.708045	30.273204
427.016199	21821.524310	30.278221
427.484024	21878.747411	30.283239
428.885899	21922.815212	30.288256
429.216797	21979.340818	30.293274
429.730525	22013.036224	30.298292
430.523409	22059.126029	30.303309
430.778309	22089.575439	30.308327
431.717346	22133.586640	30.313344
432.175253	22163.680803	30.318362
432.846001	22201.366559	30.323380
433.320066	22225.357582	30.328397
433.642229	22266.694871	30.333415
434.343531	22281.581706	30.338432
434.343469	22325.129704	30.343450
434.622089	22353.839600	30.348468
435.359095	22402.669056	30.353485
435.630627	22433.332343	30.358503
436.313166	22451.738716	30.363520
436.780170	22484.045772	30.368538
437.271427	22518.433406	30.373556
437.227740	22548.674636	30.378573
437.654357	22588.655069	30.383591
438.160566	22623.079852	30.388608
438.298614	22666.670436	30.393626
438.710588	22708.231984	30.398644
439.245723	22755.394587	30.403661
439.520204	22801.252417	30.408679
439.979731	22840.590936	30.413696
440.424708	22886.157345	30.418714
440.700010	22931.893973	30.423732
441.404556	22966.518308	30.428749
441.931639	23004.324323	30.433767
442.467052	23055.235899	30.438784
442.512689	23091.378062	30.443802
443.015714	23136.402521	30.448820
443.454492	23181.150779	30.453837
444.023447	23224.868332	30.458855
444.294141	23268.968257	30.463872
444.605076	23314.731534	30.468890
444.984328	23361.959555	30.473908
445.724675	23409.315384	30.478925
446.141442	23454.031746	30.483943
447.011545	23495.572743	30.488960
447.076374	23543.063216	30.493978
447.798526	23583.809011	30.498996
448.181083	23622.367358	30.504013
448.668058	23665.692816	30.509031
449.903156	23687.906902	30.514048
450.399039	23706.399258	30.519066
450.848631	23739.427516	30.524084
451.353197	23766.180000	30.529101
451.725205	23814.501712	30.534119
452.116937	23816.322835	30.539136
452.394637	23857.978878	30.544154
452.419894	23887.455679	30.549172
453.029010	23913.516102	30.554189
453.330503	23944.210251	30.559207
453.493679	23977.236077	30.564224
454.022908	24017.764218	30.569242
454.352311	24061.621477	30.574260
454.416627	24097.751630	30.579277
454.944995	24140.068474	30.584295
455.558208	24181.825701	30.589312
455.903779	24228.673782	30.594330
456.344274	24275.190831	30.599348
457.053348	24306.893435	30.604365
457.211582	24349.650746	30.609383
457.828763	24393.877384	30.614400
458.386918	24426.554620	30.619418
459.097408	24470.986739	30.624436
460.021071	24511.860562	30.629453
460.265048	24548.706169	30.634471
460.659742	24581.385618	30.639488
460.980580	24629.771750	30.644506
461.257302	24667.981016	30.649524
462.081452	24694.902662	30.654541
462.284616	24745.494403	30.659559
462.866067	24776.774357	30.664576
463.486420	24829.971685	30.669594
463.739361	24866.188830	30.674612
464.399760	24892.753190	30.679629
464.745136	24936.092770	30.684647
465.006945	24972.299204	30.689664
465.308217	25010.237060	30.694682
465.779429	25071.455505	30.699700
466.295556	25112.083039	30.704717
466.822180	25173.882463	30.709735
467.226486	25208.800931	30.714752
467.733514	25253.795611	30.719770
467.984447	25296.580890	30.724788
468.532877	25340.531211	30.729805
468.677926	25403.763732	30.734823
469.334036	25440.053912	30.739840
469.681001	25494.746465	30.744858
470.203322	25545.505193	30.749876
470.611705	25592.157315	30.754893
471.494723	25653.006637	30.759911
471.889200	25695.964630	30.764928
472.184998	25750.527708	30.769946
472.740330	25796.667076	30.774964
473.303626	25842.729543	30.779981
474.391499	25894.130310	30.784999
474.520539	25927.774327	30.790016
475.399806	25977.241737	30.795034
475.136014	26021.830220	30.800052
475.707203	26061.059820	30.805069
476.427498	26097.466900	30.810087
476.878886	26146.106886	30.815104
477.649046	26192.785718	30.820122
477.933295	26245.368228	30.825140
478.600687	26273.091195	30.830157
478.843630	26324.176198	30.835175
479.495423	26363.714842	30.840192
479.679326	26412.683893	30.845210
480.161784	26471.154865	30.850228
480.482534	26505.515750	30.855245
480.717709	26563.580184	30.860263
481.237798	26603.235881	30.865280
481.712824	26659.869726	30.870298
482.378262	26706.081565	30.875316
482.897270	26735.075905	30.880333
482.760577	26782.846952	30.885351
483.164165	26838.893911	30.890368
484.182990	26883.624894	30.895386
484.544806	26938.243849	30.900404
485.573672	26971.929725	30.905421
486.157188	27016.033060	30.910439
486.458588	27061.031910	30.915456
487.003252	27094.804749	30.920474
487.098330	27147.960831	30.925492
487.574690	27192.533502	30.930509
488.229067	27240.357392	30.935527
488.680490	27283.243632	30.940544
489.063730	27326.832138	30.945562
489.330710	27379.562913	30.950580
489.585581	27435.775300	30.955597
490.336162	27488.561737	30.960615
490.409573	27534.754238	30.965632
490.981376	27596.472815	30.970650
491.612850	27656.645428	30.975668
492.072617	27715.193769	30.980685
492.755399	27775.307799	30.985703
493.429086	27819.959722	30.990720
494.450311	27853.162779	30.995738
496.848407	27847.922384	31.000756
498.524970	27854.073201	31.005773
500.094091	27843.547722	31.010791
500.367860	27839.988209	31.015808
500.847701	27834.274585	31.020826
500.836680	27820.601419	31.025844
501.537780	27826.005701	31.030861
501.505495	27825.689469	31.035879
501.745928	27831.886350	31.040896
501.989003	27836.477105	31.045914
501.527515	27838.986115	31.050932
502.058624	27844.784567	31.055949
502.259942	27871.089073	31.060967
502.633748	27888.263931	31.065984
502.787568	27911.093700	31.071002
502.361623	27958.363961	31.076020
502.841738	27991.562512	31.081037
503.366742	28040.182980	31.086055
503.966010	28095.841879	31.091072
504.255509	28140.066308	31.096090
503.995306	28202.010388	31.101108
504.551805	28259.020798	31.106125
505.484124	28318.344459	31.111143
505.417248	28381.307580	31.116160
506.047367	28432.911804	31.121178
506.198943	28510.454866	31.126196
506.687080	28563.644642	31.131213
507.132523	28628.618313	31.136231
507.433556	28707.964026	31.141248
508.329923	28760.089704	31.146266
508.511512	28831.322833	31.151284
508.792550	28889.819630	31.156301
509.333933	28971.517953	31.161319
510.167702	29051.373012	31.166336
511.053344	29099.791422	31.171354
511.175412	29188.327496	31.176372
511.910237	29248.838638	31.181389
512.730534	29309.004535	31.186407
513.209467	29378.890710	31.191424
514.322504	29429.023227	31.196442
514.979696	29490.015020	31.201460
516.052546	29529.923178	31.206477
516.754694	29561.974167	31.211495
517.126605	29607.330702	31.216512
517.448104	29643.710502	31.221530
518.212586	29676.275067	31.226548
519.911504	29670.623419	31.231565
520.789303	29697.758506	31.236583
520.895183	29697.021772	31.241600
521.842878	29718.810294	31.246618
521.777854	29731.646090	31.251636
522.122286	29757.431192	31.256653
522.912444	29769.667533	31.261671
522.810894	29809.711417	31.266688
523.618587	29820.323236	31.271706
523.757826	29843.697450	31.276724
523.865900	29891.751859	31.281741
524.084814	29932.361178	31.286759
524.230672	29970.165324	31.291776
524.963699	30014.150473	31.296794
525.283911	30069.609606	31.301812
525.551331	30128.005531	31.306829
525.884303	30173.565609	31.311847
526.130665	30235.735636	31.316864
526.754318	30292.627946	31.321882
527.156088	30357.201976	31.326900
527.817212	30415.195883	31.331917
528.460688	30467.961804	31.336935
528.193877	30534.433282	31.341952
529.580397	30582.955617	31.346970
531.095710	30635.220734	31.351988
532.008362	30668.630195	31.357005
532.773337	30704.708227	31.362023
533.615013	30743.837219	31.367040
533.932646	30780.532376	31.372058
534.018450	30825.093996	31.377076
534.654435	30863.828315	31.382093
535.099697	30898.827143	31.387111
535.303359	30945.625427	31.392128
535.984205	30988.817118	31.397146
536.406245	31044.618949	31.402164
536.322831	31089.307147	31.407181
536.806555	31141.495823	31.412199
536.857067	31208.358870	31.417216
537.715544	31265.868459	31.422234
538.165016	31335.268786	31.427252
538.563426	31402.103190	31.432269
539.153160	31463.781949	31.437287
539.175774	31534.228913	31.442304
539.752332	31599.889121	31.447322
540.260742	31666.008940	31.452340
540.466364	31748.858195	31.457357
541.617588	31814.161879	31.462375
542.101141	31880.223520	31.467392
542.655167	31955.739713	31.472410
543.412684	32025.419748	31.477428
543.762029	32095.152061	31.482445
544.392459	32155.794671	31.487463
545.054217	32224.611043	31.492480
545.652544	32280.343322	31.497498
546.739749	32343.419263	31.502516
547.353861	32404.822733	31.507533
547.848048	32465.832970	31.512551
548.499565	32513.416149	31.517568
549.430989	32569.056158	31.522586
549.934115	32616.692655	31.527604
550.245438	32666.516312	31.532621
551.202807	32711.960318	31.537639
551.782021	32769.827254	31.542656
552.493500	32799.970374	31.547674
553.282597	32828.589177	31.552692
553.796702	32875.116967	31.557709
554.450592	32905.711601	31.562727
554.919358	32944.516115	31.567744
555.462124	32981.683334	31.572762
556.369634	33013.501402	31.577780
556.526456	33052.651417	31.582797
557.133723	33080.994735	31.587815
557.085963	33120.096827	31.592832
557.570348	33161.950633	31.597850
558.254563	33216.011770	31.602868
558.136944	33260.872047	31.607885
559.041778	33310.037260	31.612903
559.360177	33368.836172	31.617920
559.791502	33426.657225	31.622938
559.962612	33477.421559	31.627956
560.173343	33546.980626	31.632973
560.919086	33603.771800	31.637991
561.273302	33676.740870	31.643008
561.871543	33748.688308	31.648026
562.204156	33822.734484	31.653044
562.563925	33905.044343	31.658061
563.242700	33983.211825	31.663079
563.851609	34056.275846	31.668096
564.814596	34117.157092	31.673114
566.232045	34165.668359	31.678132
567.064256	34231.560918	31.683149
568.039624	34279.467421	31.688167
567.988159	34339.852016	31.693184
568.450574	34395.058073	31.698202
569.163398	34444.861052	31.703220
569.516929	34516.981603	31.708237
570.104584	34573.675881	31.713255
570.589456	34635.001201	31.718272
570.907517	34699.945754	31.723290
571.918964	34757.024679	31.728308
572.723735	34811.291536	31.733325
573.352042	34861.258033	31.738343
573.592862	34935.469221	31.743360
574.384017	34981.277986	31.748378
575.800336	35010.361049	31.753396
576.825463	35064.989725	31.758413
577.881131	35105.973721	31.763431
578.633637	35144.489742	31.768448
578.782479	35165.865374	31.773466
579.635910	35196.828452	31.778484
579.583042	35242.386703	31.783501
580.621355	35275.152806	31.788519
580.900911	35307.322253	31.793536
582.798276	35308.367576	31.798554
583.573241	35320.723928	31.803572
583.633091	35344.535149	31.808589
584.444446	35357.731275	31.813607
584.919298	35393.207430	31.818624
585.024405	35407.776931	31.823642
585.687106	35438.806816	31.828660
585.975764	35479.107949	31.833677
586.583098	35502.241462	31.838695
586.833865	35539.187922	31.843712
587.062324	35584.028103	31.848730
587.716189	35615.186000	31.853748
587.892339	35667.161284	31.858765
588.370879	35720.254228	31.863783
588.689591	35764.761116	31.868800
588.795114	35826.838352	31.873818
589.741420	35878.519094	31.878836
589.684623	35938.184055	31.883853
590.187747	35984.260976	31.888871
590.798899	36066.242334	31.893888
591.031234	36124.250309	31.898906
591.447811	36194.318829	31.903924
591.775647	36266.911454	31.908941
592.173598	36329.702479	31.913959
592.901625	36401.891491	31.918976
593.286162	36481.652581	31.923994
593.949757	36550.882966	31.929012
594.359942	36634.326848	31.934029
594.976147	36703.401565	31.939047
595.377316	36791.875454	31.944064
595.987082	36872.471975	31.949082
596.652063	36948.094958	31.954100
598.049083	37021.428378	31.959117
598.805572	37095.155670	31.964135
599.159310	37164.512444	31.969152
599.913435	37239.910375	31.974170
600.751711	37303.922577	31.979188
600.962564	37377.230299	31.984205
601.718978	37446.615978	31.989223
602.405705	37506.762340	31.994240
602.988279	37588.938402	31.999258
603.711523	37654.858426	32.004276
604.312888	37740.876476	32.009293
605.357094	37802.542637	32.014311
605.990212	37875.646530	32.019328
606.349532	37935.132176	32.024346
607.063977	37998.255191	32.029364
607.185302	38077.198986	32.034381
608.337446	38138.807333	32.039399
608.860558	38204.914089	32.044416
609.667701	38281.942572	32.049434
610.590437	38340.098663	32.054452
610.855144	38413.243790	32.059469
611.387344	38472.150101	32.064487
612.137030	38535.973024	32.069504
612.611913	38612.316297	32.074522
613.311753	38667.862137	32.079540
613.833372	38752.250501	32.084557
614.233429	38813.540938	32.089575
615.385285	38879.662534	32.094592
615.601199	38951.416407	32.099610
616.592236	39012.502062	32.104628
616.788533	39087.750897	32.109645
617.479751	39144.713770	32.114663
617.949684	39223.143767	32.119680
619.033544	39289.644304	32.124698
619.553199	39353.527216	32.129716
620.478198	39437.933838	32.134733
621.216251	39492.257374	32.139751
621.989640	39549.188922	32.144768
622.500318	39610.214282	32.149786
623.339071	39677.366164	32.154804
624.138152	39737.933694	32.159821
624.738643	39795.011513	32.164839
625.204436	39850.637687	32.169856
625.486108	39903.238889	32.174874
626.502710	39964.074095	32.179892
626.865576	40032.019713	32.184909
627.123291	40092.132182	32.189927
628.077013	40155.320777	32.194944
628.537430	40225.508002	32.199962
629.218216	40288.597161	32.204980
629.562459	40354.217348	32.209997
630.195377	40419.780368	32.215015
631.286425	40479.995658	32.220032
631.408832	40545.662830	32.225050
632.725750	40603.100887	32.230068
633.596447	40661.127781	32.235085
634.154898	40719.411898	32.240103
634.824165	40767.518977	32.245120
635.168605	40823.423948	32.250138
635.619338	40882.241036	32.255156
635.859931	40927.209146	32.260173
636.607545	40988.272347	32.265191
637.144094	41049.364481	32.270208
637.567114	41120.587322	32.275226
638.095024	41173.018674	32.280244
638.798659	41236.744988	32.285261
639.343817	41322.877571	32.290279
640.157875	41377.673917	32.295296
640.315408	41458.599338	32.300314
640.658737	41527.245086	32.305332
641.143728	41611.927310	32.310349
641.528388	41700.976970	32.315367
642.420993	41774.195373	32.320384
643.131700	41867.390568	32.325402
644.064394	41935.712667	32.330420
644.531395	42025.754164	32.335437
644.912626	42113.294126	32.340455
646.030482	42202.477027	32.345472
646.839176	42274.732633	32.350490
647.513828	42358.117606	32.355508
647.830834	42436.116235	32.360525
648.533118	42520.997001	32.365543
649.542603	42586.442034	32.370560
650.132295	42667.231509	32.375578
651.450053	42721.714568	32.380596
652.458952	42786.636309	32.385613
653.130789	42871.444799	32.390631
654.049720	42932.233384	32.395648
654.490382	42998.238424	32.400666
655.418716	43063.670197	32.405684
655.840809	43123.099025	32.410701
656.437763	43183.162041	32.415719
656.983456	43253.864373	32.420736
657.241719	43338.026944	32.425754
657.881787	43405.888390	32.430772
658.571699	43472.627269	32.435789
659.447622	43550.471460	32.440807
660.107647	43621.547713	32.445824
660.892350	43684.508041	32.450842
661.430184	43756.422852	32.455860
662.051797	43834.673548	32.460877
662.475690	43904.362938	32.465895
663.422434	43974.931949	32.470912
663.599649	44055.360190	32.475930
664.598567	44130.723579	32.480948
665.137974	44209.235769	32.485965
665.592158	44288.400246	32.490983
666.419306	44362.770067	32.496000
666.978024	44436.992143	32.501018
667.534006	44520.801162	32.506036
668.016112	44599.750762	32.511053
668.657545	44680.492982	32.516071
669.567810	44754.711625	32.521088
669.919886	44842.048179	32.526106
670.972958	44929.341380	32.531124
671.749720	45004.258895	32.536141
672.158802	45092.111304	32.541159
672.759242	45162.350734	32.546176
673.572016	45258.078302	32.551194
673.930146	45336.577931	32.556212
674.623998	45413.935913	32.561229
674.848863	45514.192584	32.566247
675.931484	45602.848116	32.571264
676.425699	45700.613848	32.576282
677.120396	45774.790201	32.581300
678.220703	45853.152969	32.586317
678.364110	45932.195958	32.591335
679.474849	46012.528090	32.596352
680.150240	46097.094785	32.601370
680.778576	46164.317638	32.606388
681.644427	46241.135733	32.611405
681.990024	46325.215059	32.616423
682.997069	46391.646392	32.621440
684.098058	46464.078035	32.626458
684.602472	46533.631150	32.631476
685.814595	46591.629271	32.636493
686.612923	46664.866658	32.641511
687.163288	46729.136066	32.646528
687.638236	46808.307664	32.651546
688.499599	46878.860678	32.656564
688.962032	46954.599165	32.661581
689.384329	47031.784633	32.666599
690.281011	47109.005342	32.671616
690.766684	47187.624100	32.676634
691.227546	47266.073613	32.681652
691.655735	47350.503773	32.686669
691.798566	47439.083918	32.691687
692.808423	47531.594365	32.696704
693.297515	47624.087503	32.701722
694.258101	47725.177956	32.706740
694.625432	47813.498346	32.711757
695.155765	47913.445374	32.716775
695.694202	48018.239248	32.721792
696.697213	48119.400540	32.726810
697.121184	48223.049198	32.731828
698.073637	48308.334520	32.736845
700.005874	48392.238514	32.741863
701.899286	48433.864673	32.746880
703.213476	48496.165711	32.751898
704.121385	48548.175572	32.756916
704.930202	48598.784000	32.761933
705.432952	48667.764075	32.766951
706.276315	48716.288984	32.771968
706.684068	48774.938934	32.776986
707.458454	48817.560213	32.782004
708.394601	48877.234450	32.787021
708.768665	48930.603588	32.792039
709.138134	48991.575548	32.797056
710.086883	49054.254900	32.802074
709.880263	49117.492625	32.807092
710.908253	49182.385823	32.812109
711.405371	49251.927951	32.817127
712.000192	49325.313560	32.822144
712.545135	49397.138046	32.827162
712.865890	49483.762059	32.832180
713.495773	49558.447128	32.837197
714.065417	49649.348026	32.842215
714.611586	49731.488761	32.847232
715.449003	49818.385403	32.852250
715.690046	49910.725458	32.857268
716.636613	49999.818838	32.862285
716.884716	50093.788340	32.867303
717.840466	50176.981062	32.872320
718.589944	50274.231954	32.877338
719.050591	50374.424450	32.882356
719.946880	50469.788451	32.887373
720.662067	50569.876533	32.892391
721.643831	50640.098094	32.897408
722.868857	50727.310345	32.902426
723.215235	50800.916532	32.907444
724.355546	50889.103774	32.912461
725.100042	50981.147421	32.917479
725.522212	51060.124226	32.922496
726.324517	51134.849939	32.927514
726.965833	51220.468303	32.932532
727.636865	51289.714098	32.937549
728.327358	51379.096399	32.942567
728.713079	51451.371893	32.947584
729.904624	51529.856482	32.952602
730.040252	51618.378079	32.957620
731.195018	51696.743102	32.962637
731.202380	51793.941612	32.967655
732.362470	51883.140879	32.972672
733.495273	51964.397701	32.977690
734.126313	52033.779135	32.982708
735.024843	52119.478792	32.987725
735.652949	52209.001614	32.992743
736.433496	52297.886735	32.997760
737.095724	52391.580653	33.002778
737.317381	52477.179447	33.007796
738.323707	52577.412751	33.012813
738.513193	52673.663026	33.017831
739.112766	52765.783395	33.022848
739.855427	52872.562930	33.027866
740.335416	52973.327881	33.032884
741.504600	53086.147089	33.037901
741.856478	53197.908546	33.042919
742.958001	53290.971555	33.047936
743.969521	53376.828553	33.052954
744.359250	53493.197497	33.057972
745.331265	53583.061230	33.062989
746.209495	53686.493109	33.068007
747.108837	53793.321147	33.073024
748.012455	53879.432025	33.078042
748.630684	53990.086016	33.083060
749.487175	54084.065365	33.088077
750.060526	54193.413772	33.093095
750.511837	54294.139713	33.098112
751.429643	54401.846222	33.103130
752.262656	54509.011386	33.108148
753.374714	54604.953693	33.113165
753.991404	54702.286598	33.118183
755.540552	54783.681874	33.123200
757.737583	54841.560256	33.128218
758.553886	54925.908417	33.133236
759.871685	54979.453396	33.138253
760.411452	55046.257438	33.143271
761.200805	55112.868632	33.148288
762.100061	55157.846206	33.153306
762.291775	55238.129171	33.158324
763.235910	55303.167274	33.163341
763.631846	55372.113006	33.168359
764.104992	55448.464187	33.173376
764.808847	55514.812908	33.178394
765.214782	55598.391681	33.183412
765.957123	55681.839140	33.188429
766.567616	55763.185755	33.193447
767.102797	55858.105179	33.198464
767.968401	55934.911220	33.203482
767.912629	56032.855155	33.208500
768.717213	56121.595584	33.213517
769.290715	56221.862413	33.218535
769.566883	56314.444808	33.223552
770.633806	56422.927418	33.228570
771.281776	56543.258664	33.233588
772.069822	56648.597731	33.238605
772.661867	56756.813443	33.243623
773.232244	56865.842175	33.248640
774.017308	56976.996989	33.253658
774.779724	57092.693304	33.258676
775.392104	57187.726308	33.263693
776.194429	57291.158012	33.268711
776.911377	57398.914124	33.273728
777.559337	57506.814971	33.278746
777.899135	57621.491266	33.283764
779.180694	57730.191800	33.288781
780.157780	57841.686061	33.293799
780.880618	57949.033395	33.298816
781.600010	58054.081607	33.303834
782.273354	58167.903091	33.308852
783.277168	58270.952514	33.313869
784.368064	58372.079517	33.318887
784.646205	58481.254015	33.323904
785.475001	58592.366287	33.328922
786.401652	58714.212606	33.333940
787.566913	58821.023502	33.338957
788.549970	58922.272285	33.343975
789.166562	59031.185030	33.348992
790.365675	59122.281080	33.354010
790.758187	59236.717675	33.359028
791.910174	59345.435808	33.364045
792.577766	59447.390530	33.369063
793.457300	59554.707767	33.374080
794.142274	59651.952320	33.379098
794.761500	59771.321759	33.384116
795.549463	59873.132245	33.389133
796.616994	59990.899126	33.394151
797.151829	60090.515432	33.399168
798.447924	60205.458478	33.404186
799.430255	60303.750174	33.409204
799.901259	60411.386242	33.414221
800.810201	60508.477641	33.419239
801.382028	60625.407736	33.424256
802.246488	60735.148043	33.429274
803.438146	60838.975724	33.434292
804.295783	60944.338334	33.439309
805.175811	61040.122443	33.444327
805.887575	61160.110388	33.449344
806.808472	61249.871693	33.454362
807.714163	61365.884722	33.459380
808.141783	61469.317837	33.464397
809.117593	61576.143085	33.469415
809.522176	61690.787416	33.474432
810.517537	61797.629537	33.479450
811.030489	61913.344266	33.484468
811.647577	62019.409690	33.489485
812.834924	62137.086915	33.494503
813.072429	62257.160010	33.499520
814.252181	62377.393446	33.504538
815.046000	62498.513349	33.509556
815.751102	62603.846612	33.514573
816.789600	62720.660652	33.519591
817.629150	62839.771260	33.524608
819.098747	62946.565932	33.529626
820.199431	63053.909106	33.534644
821.221459	63153.282474	33.539661
821.843326	63251.370041	33.544679
822.568790	63350.243653	33.549696
823.449627	63449.768306	33.554714
824.207927	63550.628571	33.559732
824.472054	63667.715575	33.564749
825.593037	63776.070522	33.569767
826.289195	63877.574814	33.574784
827.452835	63973.850193	33.579802
828.164158	64069.847105	33.584820
829.117870	64170.311322	33.589837
830.228860	64278.645275	33.594855
831.184539	64380.153204	33.599872
831.978539	64474.229212	33.604890
832.522295	64566.773145	33.609908
833.088139	64663.650344	33.614925
834.190860	64753.004816	33.619943
834.030442	64857.197312	33.624960
835.317898	64941.496327	33.629978
835.850591	65052.743390	33.634996
836.316164	65159.343160	33.640013
837.372191	65266.306953	33.645031
837.663397	65388.051882	33.650048
838.480063	65508.060337	33.655066
838.959374	65630.376019	33.660084
839.320724	65774.781368	33.665101
840.149643	65888.411284	33.670119
840.644615	66041.943985	33.675136
841.570293	66163.543863	33.680154
842.619241	66305.796769	33.685172
843.270783	66463.011231	33.690189
845.354602	66551.388703	33.695207
846.671780	66669.923577	33.700224
848.148204	66788.736151	33.705242
849.420091	66906.894233	33.710260
849.759530	67007.176918	33.715277
851.176896	67113.483248	33.720295
852.134249	67218.260619	33.725312
852.879933	67318.597484	33.730330
853.973535	67424.225738	33.735348
854.800277	67523.816740	33.740365
855.586794	67628.940624	33.745383
855.841930	67731.877167	33.750400
856.718641	67826.093600	33.755418
857.654320	67953.992968	33.760436
858.234682	68062.339738	33.765453
859.003771	68179.159520	33.770471
859.510986	68308.320775	33.775488
860.031575	68424.588833	33.780506
860.635509	68547.052512	33.785524
861.573557	68687.259745	33.790541
862.407874	68818.690234	33.795559
862.672819	68965.093459	33.800576
863.726139	69113.282648	33.805594
864.587120	69247.423838	33.810612
865.777753	69379.652235	33.815629
867.921087	69486.596098	33.820647
869.536084	69593.919043	33.825664
870.467618	69703.391958	33.830682
872.193648	69789.262608	33.835700
873.393791	69878.654285	33.840717
874.129372	69975.394944	33.845735
874.996960	70069.496379	33.850752
875.978162	70151.502245	33.855770
877.407795	70238.783366	33.860788
878.129343	70315.161110	33.865805
878.850105	70400.745798	33.870823
879.683917	70494.797801	33.875840
880.065406	70581.786361	33.880858
881.074234	70663.637848	33.885876
881.408051	70755.895971	33.890893
882.209153	70851.788719	33.895911
882.515093	70968.827114	33.900928
883.398615	71061.766766	33.905946
884.208800	71183.003560	33.910964
884.594362	71298.285272	33.915981
885.232209	71411.337808	33.920999
885.646426	71524.541875	33.926016
885.982401	71661.131327	33.931034
887.210235	71795.885230	33.936052
887.842680	71938.447284	33.941069
888.212125	72067.590844	33.946087
888.497536	72204.381828	33.951104
889.492486	72347.721143	33.956122
890.285234	72473.401017	33.961140
890.965939	72626.817526	33.966157
891.826841	72776.379272	33.971175
893.003990	72916.865340	33.976192
893.912418	73068.457508	33.981210
895.482199	73196.472627	33.986228
896.014376	73346.655687	33.991245
897.260586	73480.449430	33.996263
898.214852	73625.758066	34.001280
899.441915	73742.766076	34.006298
900.567616	73886.789493	34.011316
901.794122	74009.155615	34.016333
902.958213	74130.128796	34.021351
904.865512	74237.995526	34.026368
905.799505	74341.028104	34.031386
906.821362	74447.139194	34.036404
908.172637	74551.343083	34.041421
908.955062	74658.285480	34.046439
909.807366	74763.509201	34.051456
910.513315	74878.497408	34.056474
911.246559	74979.536146	34.061492
911.707045	75091.176267	34.066509
912.381699	75205.203721	34.071527
913.111255	75327.387721	34.076544
914.047916	75447.767128	34.081562
915.151538	75572.527783	34.086580
915.712893	75698.005284	34.091597
916.774436	75827.732942	34.096615
917.887696	75955.549019	34.101632
918.606974	76089.180484	34.106650
919.797141	76199.522376	34.111668
920.135634	76351.181213	34.116685
921.358021	76479.064428	34.121703
922.168929	76607.054619	34.126720
922.551344	76743.453021	34.131738
923.100865	76880.014279	34.136756
924.121183	77025.492523	34.141773
925.384822	77169.444933	34.146791
926.624923	77317.026506	34.151808
927.576770	77445.453547	34.156826
928.608976	77573.286070	34.161844
929.843527	77712.490234	34.166861
930.732558	77846.382406	34.171879
931.616445	77972.850261	34.176896
932.671909	78109.556477	34.181914
933.723013	78231.083209	34.186932
934.852906	78369.144954	34.191949
935.968357	78495.286362	34.196967
936.675842	78622.242597	34.201984
937.518858	78757.001801	34.207002
938.542848	78865.012384	34.212020
939.183992	78997.307914	34.217037
940.548608	79122.918101	34.222055
942.294908	79240.305476	34.227072
942.798178	79371.095261	34.232090
943.989307	79488.436894	34.237108
944.485195	79619.842947	34.242125
945.095192	79740.072016	34.247143
946.176700	79863.424378	34.252160
946.620110	79996.302610	34.257178
947.658084	80129.696575	34.262196
948.241430	80272.535581	34.267213
949.071233	80410.267428	34.272231
949.936897	80552.972787	34.277248
950.101517	80709.035959	34.282266
951.321312	80846.503300	34.287284
952.059274	80999.841639	34.292301
953.082458	81135.027960	34.297319
953.860038	81280.763798	34.302336
954.638829	81426.595262	34.307354
955.613722	81573.109996	34.312372
956.132101	81735.897035	34.317389
957.337408	81887.057092	34.322407
958.048732	82045.702124	34.327424
958.368471	82202.692417	34.332442
959.539042	82367.001637	34.337460
960.530825	82540.388788	34.342477
961.180132	82704.065687	34.347495
962.392488	82876.665900	34.352512
963.609245	83036.119647	34.357530
966.255611	83173.155470	34.362548
967.274810	83325.589619	34.367565
968.352774	83471.226272	34.372583
969.689631	83609.076723	34.377600
970.741956	83744.216657	34.382618
971.853134	83884.529431	34.387636
972.569349	84027.698821	34.392653
973.420591	84167.942561	34.397671
974.372571	84307.284636	34.402688
974.989732	84447.549930	34.407706
976.859753	84578.288217	34.412724
977.335300	84731.397618	34.417741
977.946370	84876.823209	34.422759
979.142138	85015.610245	34.427776
980.076583	85172.518714	34.432794
980.932952	85324.056581	34.437812
981.797761	85472.594828	34.442829
982.940240	85627.725466	34.447847
983.825589	85778.584435	34.452864
984.603609	85932.081796	34.457882
985.853149	86083.660589	34.462900
986.631558	86243.639390	34.467917
987.556433	86403.658254	34.472935
988.548039	86556.763585	34.477952
989.464938	86719.025937	34.482970
990.373773	86876.684098	34.487988
991.559623	87035.138953	34.493005
992.561113	87201.604947	34.498023
993.578504	87356.172944	34.503040
995.223554	87507.720605	34.508058
996.556193	87658.416171	34.513076
997.664540	87805.555577	34.518093
998.301584	87956.570963	34.523111
999.873963	88098.541072	34.528128
1000.396982	88260.411092	34.533146
1001.414487	88403.183852	34.538164
1002.081651	88549.553101	34.543181
1002.754305	88712.059506	34.548199
1003.997897	88864.302634	34.553216
1004.332596	89039.853116	34.558234
1005.159022	89204.672541	34.563252
1006.272288	89366.262283	34.568269
1006.894992	89540.990256	34.573287
1007.761979	89723.741568	34.578304
1008.655043	89902.262431	34.583322
1009.798993	90071.996780	34.588340
1010.869840	90247.807362	34.593357
1011.888133	90437.519572	34.598375
1012.848439	90602.623848	34.603392
1013.681095	90788.224261	34.608410
1014.726561	90966.297376	34.613428
1015.749725	91144.742584	34.618445
1017.167920	91319.054023	34.623463
1018.236057	91488.551448	34.628480
1019.243065	91652.629854	34.633498
1020.516515	91811.956297	34.638516
1021.329278	91975.012154	34.643533
1022.328934	92140.721677	34.648551
1023.350180	92287.839756	34.653568
1024.634318	92456.922024	34.658586
1026.329274	92591.815907	34.663604
1028.199415	92734.143784	34.668621
1029.096330	92880.165779	34.673639
1030.204438	93012.241513	34.678656
1031.044903	93164.274874	34.683674
1032.165088	93301.084610	34.688692
1033.185830	93449.469355	34.693709
1034.069465	93582.382938	34.698727
1035.400922	93737.477864	34.703744
1036.220176	93871.099952	34.708762
1037.551074	94008.948392	34.713780
1038.402977	94148.446853	34.718797
1038.952364	94296.009775	34.723815
1040.114484	94453.403373	34.728832
1040.553615	94615.203239	34.733850
1041.958235	94769.703861	34.738868
1042.978182	94929.497793	34.743885
1043.765649	95094.990321	34.748903
1044.587880	95255.686371	34.753920
1045.573662	95431.592757	34.758938
1046.274672	95588.740930	34.763956
1047.540185	95763.248615	34.768973
1048.126970	95947.941460	34.773991
1049.327484	96124.893260	34.779008
1049.951536	96310.145998	34.784026
1051.239377	96498.423487	34.789044
1052.532873	96662.753677	34.794061
1053.219401	96856.811974	34.799079
1054.583767	97036.800643	34.804096
1055.706288	97231.125017	34.809114
1056.739264	97418.717381	34.814132
1057.801726	97595.727818	34.819149
1058.645321	97789.855901	34.824167
1059.793187	97973.653947	34.829184
1060.845276	98168.339109	34.834202
1061.779364	98366.204418	34.839220
1063.292996	98542.849107	34.844237
1064.124440	98713.657189	34.849255
1066.868484	98873.215594	34.854272
1068.753626	99021.471140	34.859290
1069.806461	99177.431183	34.864308
1071.398666	99324.565871	34.869325
1072.389795	99467.945517	34.874343
1073.921739	99598.156187	34.879360
1075.317405	99732.448391	34.884378
1076.686304	99863.605487	34.889396
1077.911585	99982.928752	34.894413
1079.083262	100117.640023	34.899431
1080.146756	100238.871704	34.904448
1080.865924	100361.788229	34.909466
1081.199721	100497.083704	34.914484
1082.555115	100618.946210	34.919501
1082.944026	100767.707094	34.924519
1084.031355	100902.031281	34.929536
1084.915636	101058.087771	34.934554
1085.689898	101197.100073	34.939572
1086.573977	101356.444454	34.944589
1087.126113	101527.805240	34.949607
1088.282840	101680.464567	34.954624
1089.395603	101832.536916	34.959642
1090.359177	101986.648391	34.964660
1091.600434	102144.975968	34.969677
1092.513184	102299.034419	34.974695
1093.569187	102450.929871	34.979712
1094.172607	102608.156727	34.984730
1095.041794	102760.547210	34.989748
1096.351041	102916.582414	34.994765
1097.322466	103078.518995	34.999783
1098.728407	103233.501619	35.004800
1099.867230	103390.403762	35.009818
1100.566808	103566.090995	35.014836
1101.531695	103721.852554	35.019853
1102.402512	103897.830214	35.024871
1103.762571	104058.150689	35.029888
1104.950146	104221.780858	35.034906
1105.754987	104410.880634	35.039924
1106.942693	104573.132536	35.044941
1107.782223	104771.056400	35.049959
1109.057190	104940.616308	35.054976
1110.245312	105133.241830	35.059994
1110.789870	105325.456262	35.065012
1111.717415	105507.818442	35.070029
1112.533147	105697.242264	35.075047
1113.660013	105899.939684	35.080064
1115.110230	106093.237970	35.085082
1117.151394	106274.648091	35.090100
1119.044702	106446.597498	35.095117
1119.975712	106634.780328	35.100135
1121.384221	106798.465795	35.105152
1122.288302	106973.483161	35.110170
1122.989680	107147.978004	35.115188
1124.045306	107327.570256	35.120205
1125.009804	107520.098188	35.125223
1126.019510	107701.017830	35.130240
1126.996673	107913.685630	35.135258
1127.424526	108110.106687	35.140276
1129.008390	108313.633251	35.145293
1130.054015	108525.775205	35.150311
1130.733049	108717.257073	35.155328
1132.267359	108924.596448	35.160346
1133.907694	109128.081783	35.165364
1135.581032	109303.493362	35.170381
1136.914727	109496.354160	35.175399
1137.782017	109682.656165	35.180416
1138.998657	109874.069684	35.185434
1140.109538	110069.124920	35.190452
1141.294723	110259.203636	35.195469
1141.614963	110465.907465	35.200487
1143.084494	110664.454333	35.205504
1144.064997	110869.113544	35.210522
1145.142664	111080.054010	35.215540
1146.214743	111288.640812	35.220557
1147.088897	111496.083916	35.225575
1147.726045	111711.282703	35.230592
1148.750507	111925.772843	35.235610
1149.783631	112152.183977	35.240628
1151.008583	112377.615018	35.245645
1151.839711	112610.980300	35.250663
1153.315408	112827.543528	35.255680
1154.991075	113041.883604	35.260698
1156.317529	113263.479082	35.265716
1157.671858	113468.614933	35.270733
1159.145287	113680.839779	35.275751
1160.588779	113882.517942	35.280768
1162.190713	114075.492965	35.285786
1163.535923	114278.317829	35.290804
1164.860339	114468.212309	35.295821
1165.768856	114674.241777	35.300839
1166.895640	114873.762467	35.305856
1168.748438	115044.480369	35.310874
1169.686856	115229.959014	35.315892
1170.508047	115408.173264	35.320909
1171.726297	115580.950800	35.325927
1172.369834	115765.303582	35.330944
1173.716582	115956.471350	35.335962
1174.096666	116153.210845	35.340980
1175.449561	116338.539294	35.345997
1176.081243	116543.690693	35.351015
1177.442608	116733.226800	35.356032
1178.492371	116936.512492	35.361050
1179.304241	117151.077767	35.366068
1180.429443	117363.590728	35.371085
1181.457699	117573.815289	35.376103
1182.700238	117799.413438	35.381120
1184.062960	118023.662983	35.386138
1184.814433	118245.924964	35.391156
1186.122797	118468.780512	35.396173
1186.915321	118686.806952	35.401191
1188.593567	118919.323358	35.406208
1189.700446	119139.404476	35.411226
1191.214341	119372.509311	35.416244
1193.019966	119574.623803	35.421261
1193.958168	119804.494985	35.426279
1195.008845	120023.755780	35.431296
1196.602614	120224.047172	35.436314
1197.661672	120451.749189	35.441332
1199.169133	120680.519070	35.446349
1200.504368	120893.517226	35.451367
1201.771893	121111.685725	35.456384
1203.431926	121319.158709	35.461402
1204.510386	121533.674064	35.466420
1205.663025	121750.827209	35.471437
1206.826260	121968.955972	35.476455
1208.039044	122180.653101	35.481472
1209.316266	122394.102556	35.486490
1210.296737	122609.300919	35.491508
1211.999490	122818.893666	35.496525
1213.054765	123026.897106	35.501543
1214.361237	123250.676316	35.506560
1216.027617	123450.191758	35.511578
1217.899567	123654.046699	35.516596
1219.439474	123845.449528	35.521613
1220.806362	124040.950437	35.526631
1221.776417	124237.532316	35.531648
1223.355219	124424.167140	35.536666
1224.506169	124626.285242	35.541684
1225.430209	124808.177032	35.546701
1226.933247	125002.736400	35.551719
1228.005029	125200.663759	35.556736
1229.001123	125390.138747	35.561754
1229.950653	125596.390410	35.566772
1230.723077	125795.562650	35.571789
1231.913273	126001.244815	35.576807
1232.847694	126220.785788	35.581824
1234.146748	126431.509841	35.586842
1235.183204	126648.121836	35.591860
1236.142800	126861.262596	35.596877
1237.340415	127082.185622	35.601895
1238.197507	127315.866824	35.606912
1239.440766	127528.432803	35.611930
1240.405861	127768.931259	35.616948
1241.782140	128003.887758	35.621965
1243.155729	128235.474893	35.626983
1244.351305	128466.560917	35.632000
1245.766115	128703.328866	35.637018
1246.684560	128938.064142	35.642036
1247.862321	129165.761280	35.647053
1248.930726	129400.196284	35.652071
1250.165744	129632.856156	35.657088
1251.264247	129836.728311	35.662106
1253.166982	130056.351263	35.667124
1255.098372	130251.379631	35.672141
1257.228052	130454.400247	35.677159
1258.181106	130659.214513	35.682176
1259.332975	130865.581650	35.687194
1260.128271	131072.744494	35.692212
1260.937721	131275.089320	35.697229
1262.378758	131496.611552	35.702247
1263.654064	131713.447137	35.707264
1264.840044	131932.834333	35.712282
1265.925874	132148.690164	35.717300
1267.204660	132383.023567	35.722317
1268.072505	132613.623768	35.727335
1268.994473	132850.795997	35.732352
1270.368853	133063.428182	35.737370
1271.571216	133311.877914	35.742388
1273.044483	133536.920434	35.747405
1274.238115	133779.683113	35.752423
1275.250951	134030.362961	35.757440
1276.852068	134264.187460	35.762458
1277.787368	134499.797510	35.767476
1279.189284	134753.144067	35.772493
1280.325103	134998.701821	35.777511
1281.369176	135257.448984	35.782528
1283.165016	135503.179954	35.787546
1284.094959	135780.700944	35.792564
1285.229745	136033.024017	35.797581
1286.557575	136281.729032	35.802599
1287.595008	136554.864661	35.807616
1289.293267	136810.434614	35.812634
1289.955916	137083.205664	35.817652
1291.166187	137362.734625	35.822669
1292.570028	137639.545904	35.827687
1293.801669	137914.194569	35.832704
1295.208189	138180.562422	35.837722
1296.269551	138458.984085	35.842740
1297.644570	138747.017604	35.847757
1299.491197	139011.353732	35.852775
1300.923577	139283.761350	35.857792
1302.616251	139540.722336	35.862810
1303.926450	139815.183194	35.867828
1305.108423	140084.443468	35.872845
1306.636722	140358.821796	35.877863
1307.867650	140618.035705	35.882880
1309.105354	140893.582330	35.887898
1310.072992	141160.769011	35.892916
1312.047200	141423.035735	35.897933
1313.917548	141682.227669	35.902951
1314.671337	141962.884470	35.907968
1316.603414	142220.485127	35.912986
1318.552005	142470.210287	35.918004
1320.348547	142706.812561	35.923021
1322.479676	142937.312211	35.928039
1323.823973	143164.241053	35.933056
1325.153716	143390.831387	35.938074
1326.305659	143615.575874	35.943092
1327.118486	143855.646086	35.948109
1328.509699	144077.665433	35.953127
1329.633466	144318.955337	35.958144
1330.991163	144559.903731	35.963162
1331.963975	144805.508271	35.968180
1332.939734	145050.835017	35.973197
1334.409786	145291.008822	35.978215
1335.375765	145531.179060	35.983232
1336.880561	145782.611754	35.988250
1338.284893	146029.078884	35.993268
1338.881161	146278.142007	35.998285
1340.385790	146506.828327	36.003303
1340.996607	146759.329182	36.008320
1342.166313	147011.903976	36.013338
1343.635792	147268.755478	36.018356
1344.429717	147527.585134	36.023373
1346.173453	147777.596964	36.028391
1347.059690	148027.930260	36.033408
1348.390835	148281.324099	36.038426
1349.990203	148560.712904	36.043444
1351.187800	148830.189042	36.048461
1353.166200	149091.598135	36.053479
1353.902704	149362.638514	36.058496
1355.213312	149636.401317	36.063514
1356.599614	149918.334257	36.068532
1357.653255	150211.105313	36.073549
1358.992809	150485.211980	36.078567
1359.932256	150778.298114	36.083584
1360.905657	151064.620530	36.088602
1362.456446	151357.368792	36.093620
1363.933752	151661.090314	36.098637
1366.378503	151925.739610	36.103655
1367.914077	152212.142352	36.108672
1369.225551	152500.537754	36.113690
1370.837080	152770.049559	36.118708
1372.084069	153056.278156	36.123725
1373.904528	153336.096969	36.128743
1375.132508	153626.823219	36.133760
1376.480158	153906.470877	36.138778
1377.851311	154194.437778	36.143796
1379.902701	154464.319738	36.148813
1381.756206	154718.722847	36.153831
1383.861322	154992.214721	36.158848
1385.330330	155250.909122	36.163866
1386.858158	155506.563740	36.168884
1387.951768	155778.224575	36.173901
1389.475227	156033.832593	36.178919
1390.581449	156301.283427	36.183936
1391.781083	156559.079661	36.188954
1393.096779	156820.321457	36.193972
1394.204399	157091.684497	36.198989
1395.510336	157349.265236	36.204007
1396.895185	157628.171961	36.209024
1397.900053	157906.839167	36.214042
1399.382000	158184.921750	36.219060
1400.763610	158470.964324	36.224077
1401.870513	158767.254090	36.229095
1402.958908	159059.375322	36.234112
1404.164763	159345.681535	36.239130
1405.681521	159637.824672	36.244148
1407.001114	159938.806987	36.249165
1408.490455	160228.535751	36.254183
1410.013423	160533.561065	36.259200
1411.182208	160815.811226	36.264218
1412.811143	161109.087972	36.269236
1413.943826	161426.262407	36.274253
1415.410274	161719.164399	36.279271
1416.678545	162026.437716	36.284288
1417.777919	162333.170359	36.289306
1419.275046	162646.157542	36.294324
1420.379150	162964.401346	36.299341
1422.219213	163262.897978	36.304359
1423.904515	163578.664758	36.309376
1425.443971	163879.296304	36.314394
1426.980651	164177.570498	36.319412
1428.197724	164488.511455	36.324429
1429.864198	164784.243444	36.329447
1431.194497	165079.563738	36.334464
1432.790656	165379.764935	36.339482
1434.513286	165657.248081	36.344500
1435.534666	165946.852351	36.349517
1437.018828	166236.445240	36.354535
1438.536052	166516.480171	36.359552
1440.387440	166786.069590	36.364570
1441.968834	167054.296988	36.369588
1443.193645	167335.387981	36.374605
1444.637710	167630.871487	36.379623
1446.158632	167920.456589	36.384640
1446.840748	168210.081131	36.389658
1448.579593	168501.955919	36.394676
1449.661792	168812.074151	36.399693
1450.784353	169117.442069	36.404711
1452.101079	169424.987772	36.409728
1453.459704	169731.411942	36.414746
1455.584295	170025.351677	36.419764
1458.277840	170308.349450	36.424781
1460.379257	170589.467569	36.429799
1461.676630	170869.832439	36.434816
1462.991023	171154.294962	36.439834
1464.464168	171433.035185	36.444852
1465.880025	171722.344546	36.449869
1467.001153	172016.095284	36.454887
1469.213784	172305.809119	36.459904
1470.323819	172590.441152	36.464922
1472.352564	172862.816143	36.469940
1473.780319	173150.939428	36.474957
1475.164874	173434.147771	36.479975
1477.078573	173708.957847	36.484992
1478.370958	173990.801514	36.490010
1479.842973	174274.266824	36.495028
1480.831315	174573.156964	36.500045
1481.852147	174863.477333	36.505063
1482.898515	175157.932398	36.510080
1484.209060	175475.100162	36.515098
1485.487756	175769.063521	36.520116
1486.713759	176091.744469	36.525133
1487.950532	176420.035214	36.530151
1488.967411	176737.716682	36.535168
1490.133898	177083.080432	36.540186
1491.500800	177415.798125	36.545204
1493.031746	177761.677247	36.550221
1494.569145	178109.664472	36.555239
1496.099645	178446.220084	36.560256
1497.471036	178806.804330	36.565274
1498.967494	179135.602819	36.570292
1500.398761	179493.643626	36.575309
1501.670147	179852.106884	36.580327
1503.288946	180202.557111	36.585344
1505.368792	180550.191765	36.590362
1507.560047	180893.279144	36.595380
1509.196287	181228.058482	36.600397
1510.902379	181561.736826	36.605415
1512.835999	181901.091168	36.610432
1514.196721	182234.627934	36.615450
1515.967819	182560.495871	36.620468
1517.482001	182896.917945	36.625485
1518.771490	183232.820893	36.630503
1520.381697	183565.220303	36.635520
1521.259962	183921.859685	36.640538
1523.017192	184248.527075	36.645556
1524.626242	184602.701542	36.650573
1526.016352	184943.764450	36.655591
1527.856637	185270.830330	36.660608
1529.130067	185607.689818	36.665626
1530.629941	185939.347585	36.670644
1533.155586	186253.269484	36.675661
1534.623510	186564.271263	36.680679
1536.420798	186856.230503	36.685696
1538.234034	187151.285861	36.690714
1539.523307	187448.359062	36.695732
1541.235578	187744.310095	36.700749
1542.659813	188036.172201	36.705767
1544.235612	188341.326604	36.710784
1545.730438	188644.236505	36.715802
1547.262478	188935.590208	36.720820
1548.660548	189236.983248	36.725837
1550.162266	189556.830723	36.730855
1551.483636	189843.527005	36.735872
1552.666608	190159.711165	36.740890
1554.276244	190482.059229	36.745908
1555.324277	190812.372707	36.750925
1556.805910	191136.014958	36.755943
1558.797600	191445.876909	36.760960
1559.733328	191778.258126	36.765978
1561.406224	192103.041747	36.770996
1562.830663	192456.444308	36.776013
1564.291593	192800.474023	36.781031
1566.048186	193137.537886	36.786048
1567.500907	193494.559755	36.791066
1568.842573	193837.878670	36.796084
1570.228436	194197.556208	36.801101
1571.186152	194550.146651	36.806119
1572.859447	194909.348944	36.811136
1574.232886	195280.473150	36.816154
1575.982422	195645.252901	36.821172
1577.663421	196029.394064	36.826189
1579.032187	196403.128074	36.831207
1581.075597	196766.697407	36.836224
1582.105436	197150.546835	36.841242
1583.832756	197530.753427	36.846260
1585.665693	197892.649898	36.851277
1586.821867	198286.260762	36.856295
1588.456901	198672.100743	36.861312
1590.080188	199062.413895	36.866330
1591.503046	199457.028418	36.871348
1593.243076	199846.298289	36.876365
1594.530132	200238.311665	36.881383
1596.324170	200637.353188	36.886400
1598.174337	201036.959017	36.891418
1599.709537	201428.912514	36.896436
1601.644012	201816.434351	36.901453
1603.098785	202226.345870	36.906471
1604.928543	202608.429760	36.911488
1606.630117	203001.303809	36.916506
1608.557045	203387.006963	36.921524
1610.520797	203781.289173	36.926541
1612.249482	204154.573483	36.931559
1614.590421	204520.774779	36.936576
1616.527783	204897.469109	36.941594
1618.603418	205259.020023	36.946612
1620.621650	205616.392072	36.951629
1621.861655	205968.155593	36.956647
1623.938266	206324.480071	36.961664
1625.385336	206680.694676	36.966682
1627.098799	207026.073875	36.971700
1629.044096	207371.124117	36.976717
1630.168213	207726.127220	36.981735
1632.063471	208070.884045	36.986752
1633.453469	208421.973370	36.991770
1635.145939	208758.157693	36.996788
1637.182195	209106.984237	37.001805
1639.027834	209459.957968	37.006823
1640.244009	209787.578200	37.011840
1642.155851	210127.871271	37.016858
1644.259287	210433.087422	37.021876
1646.158232	210743.722553	37.026893
1647.656614	211043.428647	37.031911
1649.828449	211329.437142	37.036928
1651.597175	211628.973493	37.041946
1653.287234	211928.066784	37.046964
1654.896527	212209.549270	37.051981
1656.039890	212517.547801	37.056999
1657.842194	212829.247701	37.062016
1658.923794	213143.607833	37.067034
1660.198602	213455.219574	37.072052
1661.882755	213773.697930	37.077069
1662.717568	214105.397686	37.082087
1663.677223	214432.608046	37.087104
1665.199639	214792.793563	37.092122
1666.609816	215144.160789	37.097140
1668.387500	215496.687501	37.102157
1669.433976	215862.949827	37.107175
1670.970814	216231.849839	37.112192
1672.426334	216620.625810	37.117210
1673.979028	216993.284978	37.122228
1675.583555	217373.784952	37.127245
1676.860078	217780.221398	37.132263
1678.297524	218183.508854	37.137280
1679.781756	218648.127048	37.142298
1681.413697	219052.554053	37.147316
1683.376647	219454.362539	37.152333
1684.697182	219870.832450	37.157351
1687.146245	220288.031326	37.162368
1688.902028	220686.145255	37.167386
1690.694720	221100.636831	37.172404
1691.981826	221499.314020	37.177421
1693.971856	221923.275239	37.182439
1695.922898	222332.894006	37.187456
1697.891268	222743.552769	37.192474
1699.630316	223150.034734	37.197492
1701.470642	223557.644331	37.202509
1703.278621	223970.239030	37.207527
1704.870195	224388.763760	37.212544
1706.777290	224805.561291	37.217562
1708.305070	225218.663961	37.222580
1710.565883	225626.007770	37.227597
1711.872312	226043.036088	37.232615
1713.891696	226446.688811	37.237632
1716.348218	226851.057782	37.242650
1717.954711	227261.893561	37.247668
1720.230696	227646.228783	37.252685
1722.160277	228043.322723	37.257703
1724.176812	228427.474616	37.262720
1726.055453	228821.023248	37.267738
1727.545860	229206.788575	37.272756
1729.291917	229584.359002	37.277773
1730.454957	229987.072183	37.282791
1731.930421	230367.610636	37.287808
1733.900433	230766.991780	37.292826
1735.660283	231178.017073	37.297844
1737.426823	231574.690832	37.302861
1738.636348	231991.346988	37.307879
1740.254445	232390.206576	37.312896
1741.541394	232814.142258	37.317914
1743.083274	233223.075483	37.322932
1744.772631	233640.367754	37.327949
1746.534094	234065.218765	37.332967
1748.223690	234479.617373	37.337984
1750.108960	234903.205331	37.343002
1751.512599	235330.531982	37.348020
1753.555572	235742.792157	37.353037
1755.009691	236177.682193	37.358055
1756.377582	236581.368787	37.363072
1758.225954	236984.798828	37.368090
1759.617826	237405.096030	37.373108
1761.626046	237811.727382	37.378125
1763.285349	238220.678182	37.383143
1765.020751	238635.993124	37.388160
1767.293265	239049.441762	37.393178
1769.582293	239447.952030	37.398196
1771.980102	239846.902264	37.403213
1773.696226	240253.739284	37.408231
1775.485850	240647.990746	37.413248
1777.584890	241044.604845	37.418266
1779.122116	241448.984241	37.423284
1780.930116	241851.414279	37.428301
1782.447040	242256.382663	37.433319
1783.901774	242675.028557	37.438336
1785.659737	243095.809510	37.443354
1787.030418	243518.306487	37.448372
1788.557462	243936.383566	37.453389
1790.095810	244373.409787	37.458407
1791.774361	244804.367606	37.463424
1793.707391	245255.326645	37.468442
1795.302099	245705.072281	37.473460
1796.568585	246149.766989	37.478477
1798.392105	246618.477296	37.483495
1799.636481	247086.649153	37.488512
1801.502564	247556.191984	37.493530
1802.908817	248043.619077	37.498548
1804.892965	248513.041937	37.503565
1806.583305	248999.838883	37.508583
1808.712793	249485.115653	37.513600
1810.904818	249956.360108	37.518618
1812.586759	250448.443884	37.523636
1815.004224	250923.132161	37.528653
1816.492501	251412.276801	37.533671
1817.929318	251906.942882	37.538688
1820.254974	252382.993987	37.543706
1821.745298	252876.966093	37.548724
1823.652897	253364.544009	37.553741
1825.362447	253865.745781	37.558759
1827.055723	254361.844499	37.563776
1829.176185	254858.279150	37.568794
1830.592515	255368.167422	37.573812
1832.960482	255857.448592	37.578829
1834.721698	256362.504294	37.583847
1836.738131	256862.945265	37.588864
1838.831029	257347.318803	37.593882
1840.603855	257856.920121	37.598900
1842.584993	258345.072002	37.603917
1844.823604	258846.594186	37.608935
1846.866278	259323.177391	37.613952
1849.062427	259817.517441	37.618970
1850.627551	260299.514372	37.623988
1852.668416	260783.159812	37.629005
1855.298322	261255.961952	37.634023
1857.817217	261734.777521	37.639040
1859.983700	262191.956931	37.644058
1861.187910	262659.660130	37.649076
1863.401215	263128.186651	37.654093
1865.203754	263595.917287	37.659111
1867.088143	264053.574431	37.664128
1869.253929	264510.879842	37.669146
1870.971670	264981.392637	37.674164
1873.717202	265399.607522	37.679181
1875.681675	265842.211534	37.684199
1877.396905	266298.091529	37.689216
1879.252074	266730.348476	37.694234
1880.856061	267177.837715	37.699252
1882.613260	267592.353397	37.704269
1884.583649	268023.726401	37.709287
1885.918763	268452.562325	37.714304
1887.303850	268869.221506	37.719322
1888.913880	269317.012409	37.724340
1890.409069	269752.221973	37.729357
1892.118562	270204.745694	37.734375
1893.539374	270658.790036	37.739392
1895.299303	271112.828398	37.744410
1896.969234	271585.323470	37.749428
1898.627417	272057.997606	37.754445
1900.488470	272539.375935	37.759463
1901.763772	273022.323883	37.764480
1903.905310	273508.480646	37.769498
1905.429043	274007.719628	37.774516
1907.356814	274511.056753	37.779533
1909.177869	275017.306464	37.784551
1910.593519	275527.102453	37.789568
1912.369473	276051.850480	37.794586
1914.073299	276579.378143	37.799604
1916.289871	277107.099068	37.804621
1918.337894	277639.266647	37.809639
1920.208665	278174.586745	37.814656
1922.388492	278691.615599	37.819674
1923.988327	279242.777909	37.824692
1926.056584	279782.684247	37.829709
1927.727809	280324.280579	37.834727
1929.954516	280877.620563	37.839744
1931.964642	281419.386194	37.844762
1933.823915	281979.515159	37.849780
1936.259569	282514.805753	37.854797
1938.631232	283063.415647	37.859815
1940.436599	283610.009253	37.864832
1943.185325	284132.567543	37.869850
1945.422135	284676.342750	37.874868
1947.026543	285206.936062	37.879885
1949.347565	285748.890101	37.884903
1951.521208	286285.507015	37.889920
1953.517841	286809.857303	37.894938
1955.140036	287354.054921	37.899956
1957.225155	287892.560232	37.904973
1958.800685	288422.130696	37.909991
1960.880111	288966.728920	37.915008
1963.167505	289504.102198	37.920026
1964.968603	290058.800633	37.925044
1966.860058	290596.438246	37.930061
1968.802101	291131.220420	37.935079
1970.086384	291695.446207	37.940096
1972.214438	292243.654769	37.945114
1973.996117	292807.158062	37.950132
1975.557986	293366.250197	37.955149
1977.836385	293927.913326	37.960167
1979.785869	294506.112388	37.965184
1981.556918	295064.628306	37.970202
1983.446295	295633.078285	37.975220
1985.676602	296199.614747	37.980237
1987.659612	296781.072931	37.985255
1989.333563	297366.846139	37.990272
1991.246313	297934.416603	37.995290
1993.523406	298500.882288	38.000308
1995.810182	299079.432810	38.005325
1997.964379	299652.617592	38.010343
2000.421896	300219.221566	38.015360
2002.222952	300780.572086	38.020378
2004.890723	301340.023354	38.025396
2007.046218	301891.936962	38.030413
2009.145408	302443.297938	38.035431
2011.378102	302985.719124	38.040448
2013.354645	303498.134823	38.045466
2015.531415	304028.139944	38.050484
2017.723335	304536.171229	38.055501
2019.938476	305055.700449	38.060519
2021.535906	305579.951087	38.065536
2023.736805	306090.536974	38.070554
2025.090881	306610.072583	38.075572
2027.072674	307138.999163	38.080589
2029.333583	307650.327655	38.085607
2031.291069	308184.508617	38.090624
2033.613216	308703.566167	38.095642
2035.690717	309227.816206	38.100660
2037.587257	309751.483337	38.105677
2040.331897	310271.248096	38.110695
2042.920293	310774.020756	38.115712
2045.151787	311295.565218	38.120730
2047.492067	311796.569366	38.125748
2049.584975	312307.108725	38.130765
2051.654120	312810.690587	38.135783
2053.251726	313330.091498	38.140800
2055.383973	313853.056964	38.145818
2057.017431	314369.930690	38.150836
2058.447034	314910.932971	38.155853
2060.695802	315437.067427	38.160871
2062.101923	315986.394560	38.165888
2063.865070	316525.069481	38.170906
2065.691528	317078.330625	38.175924
2067.395736	317641.053660	38.180941
2069.461419	318215.138793	38.185959
2070.912384	318809.939317	38.190976
2072.838682	319390.715774	38.195994
2075.149472	319977.873014	38.201012
2076.731711	320571.036560	38.206029
2079.350125	321148.915401	38.211047
2081.375550	321743.442259	38.216064
2083.671677	322337.055542	38.221082
2086.043826	322929.584342	38.226100
2087.940215	323545.520059	38.231117
2089.935403	324133.758288	38.236135
2091.893933	324747.640704	38.241152
2094.324724	325341.533434	38.246170
2096.644944	325945.467480	38.251188
2098.778630	326542.799883	38.256205
2100.595013	327157.951038	38.261223
2102.829884	327769.802201	38.266240
2105.074539	328373.343461	38.271258
2107.600333	328989.449761	38.276276
2109.181432	329601.339303	38.281293
2111.494612	330214.472020	38.286311
2114.047757	330815.067931	38.291328
2116.068212	331408.078855	38.296346
2118.441552	332026.462455	38.301364
2120.675819	332638.871047	38.306381
2122.604652	333246.373153	38.311399
2124.236604	333858.030181	38.316416
2126.092548	334469.084746	38.321434
2128.605504	335095.787766	38.326452
2130.085312	335718.897576	38.331469
2132.545045	336345.137769	38.336487
2134.692973	336963.019944	38.341504
2136.768385	337588.775840	38.346522
2138.386465	338221.732717	38.351540
2140.169938	338854.654398	38.356557
2142.540432	339494.552860	38.361575
2144.237526	340145.646977	38.366592
2146.192237	340791.664263	38.371610
2147.836513	341444.704624	38.376628
2149.780324	342095.453146	38.381645
2152.160849	342738.100179	38.386663
2154.203116	343374.373324	38.391680
2156.353868	344008.462743	38.396698
2158.773214	344643.336826	38.401716
2161.268009	345278.139164	38.406733
2163.992619	345892.083553	38.411751
2166.426164	346517.438033	38.416768
2168.947840	347131.019021	38.421786
2171.491580	347746.770757	38.426804
2173.346757	348371.561412	38.431821
2175.520202	348999.995965	38.436839
2177.596560	349617.626987	38.441856
2179.487857	350252.511315	38.446874
2181.625036	350876.205418	38.451892
2183.401555	351529.463368	38.456909
2185.431715	352167.773801	38.461927
2187.288950	352823.029178	38.466944
2189.140306	353473.099040	38.471962
2191.751858	354131.736824	38.476980
2193.573711	354804.476634	38.481997
2196.113789	355457.980066	38.487015
2198.324506	356138.500263	38.492032
2200.374480	356801.985090	38.497050
2202.321023	357488.641989	38.502068
2204.333788	358182.837518	38.507085
2206.532333	358875.874151	38.512103
2208.854703	359567.051717	38.517120
2211.347281	360250.882356	38.522138
2213.710013	360940.887954	38.527156
2215.559269	361640.683489	38.532173
2217.798278	362330.457109	38.537191
2220.320731	363029.456926	38.542208
2222.644820	363730.354388	38.547226
2225.682644	364409.506984	38.552244
2228.906382	365080.118505	38.557261
2232.022253	365763.445350	38.562279
2234.492855	366412.468802	38.567296
2237.011770	367076.414165	38.572314
2239.471779	367730.312479	38.577332
2241.623267	368382.829943	38.582349
2244.337378	369031.488696	38.587367
2246.607547	369681.401715	38.592384
2248.663786	370327.812974	38.597402
2250.916760	370974.966495	38.602420
2252.777190	371631.659479	38.607437
2255.044283	372279.827228	38.612455
2256.757808	372930.459017	38.617472
2259.187656	373601.757390	38.622490
2261.515007	374246.379414	38.627508
2263.204577	374920.996252	38.632525
2265.398172	375578.017675	38.637543
2267.809989	376249.724941	38.642560
2270.280602	376909.338152	38.647578
2272.637550	377565.407237	38.652596
2275.043944	378235.910134	38.657613
2277.100931	378901.259214	38.662631
2279.193460	379578.989342	38.667648
2281.097329	380269.643966	38.672666
2283.127711	380943.046106	38.677684
2285.080016	381638.710407	38.682701
2286.751842	382326.394104	38.687719
2288.526283	383038.286064	38.692736
2290.856317	383740.156874	38.697754
2292.953616	384447.451513	38.702772
2294.962217	385181.138449	38.707789
2297.156927	385896.599749	38.712807
2299.393114	386628.720074	38.717824
2301.873008	387350.490354	38.722842
2304.841952	388039.992427	38.727860
2306.735762	388744.538260	38.732877
2309.276326	389428.985228	38.737895
2311.728402	390120.276182	38.742912
2313.737162	390817.151178	38.747930
2316.080770	391525.158976	38.752948
2317.988101	392234.287244	38.757965
2320.121015	392949.318262	38.762983
2322.268485	393650.592103	38.768000
2324.588949	394369.892730	38.773018
2327.240058	395095.913934	38.778036
2329.462462	395811.064808	38.783053
2332.691259	396528.591586	38.788071
2335.417341	397233.005456	38.793088
2338.275536	397945.895791	38.798106
2340.612198	398648.591392	38.803124
2342.420716	399368.539145	38.808141
2345.003166	400080.763839	38.813159
2347.461082	400803.811895	38.818176
2349.055849	401529.974669	38.823194
2351.411583	402250.798401	38.828212
2353.873250	402978.452988	38.833229
2356.058570	403713.203795	38.838247
2358.839967	404450.218355	38.843264
2360.361008	405202.776022	38.848282
2362.750918	405952.331817	38.853300
2365.078413	406707.501985	38.858317
2366.911975	407470.738832	38.863335
2369.521288	408236.536634	38.868352
2371.608487	409017.675084	38.873370
2373.599391	409788.471327	38.878388
2376.156024	410574.376076	38.883405
2378.474753	411365.515250	38.888423
2381.463531	412144.741504	38.893440
2383.556312	412942.710159	38.898458
2386.297892	413722.006749	38.903476
2388.882593	414517.186623	38.908493
2391.927696	415284.684914	38.913511
2394.810655	416061.659337	38.918528
2397.343012	416843.480230	38.923546
2399.954267	417604.979148	38.928564
2403.206025	418359.689127	38.933581
2405.841179	419115.314425	38.938599
2408.765021	419867.020346	38.943616
2411.855943	420596.975445	38.948634
2414.482987	421329.391558	38.953652
2416.973773	422060.314824	38.958669
2419.459374	422794.230453	38.963687
2421.770832	423521.114505	38.968704
2423.815831	424265.490608	38.973722
2425.898846	424995.913330	38.978740
2428.063647	425735.768996	38.983757
2430.362841	426491.174325	38.988775
2432.966565	427226.152466	38.993792
2435.079127	427962.910812	38.998810
2437.501712	428709.264874	39.003828
2439.551691	429459.504757	39.008845
2441.644849	430232.139968	39.013863
2444.419361	430985.097131	39.018880
2446.175842	431757.687460	39.023898
2448.422023	432521.262400	39.028916
2451.179873	433291.105356	39.033933
2453.058003	434057.019178	39.038951
2455.652822	434835.695413	39.043968
2457.716381	435629.313059	39.048986
2460.083936	436404.430868	39.054004
2462.343785	437205.755197	39.059021
2464.593837	437988.328483	39.064039
2467.149175	438754.681234	39.069056
2469.264669	439538.184475	39.074074
2471.622041	440303.808653	39.079092
2474.054920	441075.971973	39.084109
2475.915233	441863.584897	39.089127
2478.529252	442657.875449	39.094144
2481.046409	443444.463074	39.099162
2483.700815	444221.893144	39.104180
2485.853167	445028.619846	39.109197
2488.142868	445835.091502	39.114215
2490.605806	446621.573291	39.119232
2492.702578	447448.605323	39.124250
2495.439402	448262.550336	39.129268
2497.963380	449084.288978	39.134285
2500.798623	449913.227675	39.139303
2503.180788	450733.762542	39.144320
2505.762530	451555.446210	39.149338
2508.726059	452401.157751	39.154356
2510.926286	453228.250161	39.159373
2513.326539	454080.257540	39.164391
2516.145014	454913.248680	39.169408
2518.207325	455771.613608	39.174426
2521.030394	456610.754648	39.179444
2523.916689	457467.496333	39.184461
2526.007284	458335.001400	39.189479
2528.827281	459185.361730	39.194496
2531.260761	460044.192663	39.199514
2533.791226	460916.569218	39.204532
2536.737398	461780.953152	39.209549
2538.639156	462654.520346	39.214567
2541.397267	463510.671400	39.219584
2544.179721	464384.420738	39.224602
2546.095261	465261.408182	39.229620
2549.277663	466137.893938	39.234637
2551.282103	467037.023719	39.239655
2554.433739	467922.429432	39.244672
2556.882059	468827.517077	39.249690
2559.410535	469725.373698	39.254708
2561.759598	470614.880967	39.259725
2564.323446	471510.778250	39.264743
2567.127604	472394.973401	39.269760
2569.592550	473305.200813	39.274778
2572.233218	474199.745311	39.279796
2575.376144	475100.074149	39.284813
2577.216842	476001.181138	39.289831
2580.217959	476890.990719	39.294848
2583.384245	477814.670993	39.299866
2585.887566	478703.667359	39.304884
2588.613771	479603.845724	39.309901
2591.145503	480520.070786	39.314919
2593.746554	481411.343046	39.319936
2596.369951	482327.461612	39.324954
2598.672761	483228.338023	39.329972
2601.745618	484124.851142	39.334989
2604.173640	485047.022931	39.340007
2607.416371	485930.896347	39.345024
2609.837993	486827.784941	39.350042
2612.572905	487728.816395	39.355060
2614.965264	488631.322181	39.360077
2617.455806	489536.087019	39.365095
2620.324426	490423.632492	39.370112
2622.584356	491334.751881	39.375130
2624.929123	492252.319404	39.380148
2627.777963	493154.211869	39.385165
2629.903838	494075.250800	39.390183
2632.528877	494977.538431	39.395200
2634.963623	495908.569377	39.400218
2637.582900	496805.816233	39.405236
2640.218067	497706.443403	39.410253
2642.483535	498600.979399	39.415271
2645.214505	499483.283889	39.420288
2648.296446	500368.005781	39.425306
2650.448660	501268.470652	39.430324
2653.251772	502154.152269	39.435341
2656.004246	503047.309395	39.440359
2658.905299	503945.486971	39.445376
2661.110034	504846.201505	39.450394
2664.269607	505741.363228	39.455412
2667.397463	506626.850141	39.460429
2670.122459	507516.237646	39.465447
2673.328265	508401.614447	39.470464
2676.445726	509289.881145	39.475482
2678.736875	510173.547014	39.480500
2681.563338	511062.670787	39.485517
2684.495141	511953.340413	39.490535
2686.853858	512850.708021	39.495552
2689.462209	513744.707298	39.500570
2691.429660	514655.745762	39.505588
2694.098912	515571.856192	39.510605
2696.326480	516504.867111	39.515623
2699.504901	517407.733972	39.520640
2702.916182	518329.807385	39.525658
2705.220651	519252.361528	39.530676
2708.287472	520169.545132	39.535693
2710.587303	521112.240874	39.540711
2713.674573	522019.537153	39.545728
2717.097054	522945.763879	39.550746
2719.231493	523874.312906	39.555764
2721.979264	524801.494652	39.560781
2724.299559	525760.568538	39.565799
2727.031150	526698.815993	39.570816
2729.459224	527651.305102	39.575834
2731.822896	528613.109278	39.580852
2734.701352	529566.861265	39.585869
2737.239177	530534.503214	39.590887
2740.023209	531504.910292	39.595904
2742.965709	532478.448586	39.600922
2745.419242	533446.164073	39.605940
2747.866161	534428.513109	39.610957
2750.794547	535417.711551	39.615975
2753.445027	536414.386599	39.620992
2756.318998	537411.005993	39.626010
2758.527426	538414.761002	39.631028
2761.682421	539411.798415	39.636045
2763.701459	540420.575618	39.641063
2766.646822	541445.075080	39.646080
2770.029747	542455.192081	39.651098
2772.677242	543485.377439	39.656116
2775.364594	544483.794167	39.661133
2778.024726	545499.545160	39.666151
2781.302862	546518.740568	39.671168
2784.068074	547537.443065	39.676186
2786.956063	548559.268131	39.681204
2790.208084	549573.616626	39.686221
2793.167104	550578.989847	39.691239
2796.167949	551589.359445	39.696256
2799.740104	552590.863492	39.701274
2802.534580	553583.827342	39.706292
2805.739147	554576.600159	39.711309
2808.328519	555568.848764	39.716327
2810.617088	556564.340134	39.721344
2813.732682	557556.002787	39.726362
2816.423334	558562.081963	39.731380
2819.319651	559545.141412	39.736397
2822.412492	560540.453503	39.741415
2825.112741	561508.428863	39.746432
2828.437807	562464.777375	39.751450
2831.042695	563406.810736	39.756468
2833.671471	564357.008572	39.761485
2836.154366	565296.062975	39.766503
2839.617740	566232.225864	39.771520
2842.730316	567153.265516	39.776538
2845.307033	568098.678543	39.781556
2848.563898	569030.003122	39.786573
2851.140075	569970.408565	39.791591
2853.567219	570911.070585	39.796608
2856.385104	571856.868675	39.801626
2859.127170	572817.063154	39.806644
2862.267681	573757.295787	39.811661
2865.320486	574720.054318	39.816679
2867.986024	575678.387540	39.821696
2870.728237	576650.733493	39.826714
2873.170950	577613.470892	39.831732
2875.722658	578596.081702	39.836749
2878.118428	579578.991611	39.841767
2880.273002	580591.757173	39.846784
2883.154611	581608.181076	39.851802
2885.392812	582644.937682	39.856820
2888.504639	583665.766661	39.861837
2891.143721	584727.553281	39.866855
2893.441840	585770.452381	39.871872
2896.065769	586823.885937	39.876890
2898.750378	587909.750249	39.881908
2901.625891	588986.513026	39.886925
2904.410623	590081.336960	39.891943
2907.592061	591180.104299	39.896960
2910.225086	592272.296670	39.901978
2913.084256	593384.442976	39.906996
2916.193880	594493.036485	39.912013
2919.086534	595625.406727	39.917031
2921.639758	596752.714899	39.922048
2924.694139	597879.280633	39.927066
2927.646760	599019.927047	39.932084
2930.514866	600164.581608	39.937101
2933.258515	601316.954528	39.942119
2935.813906	602481.359244	39.947136
2938.499730	603646.225134	39.952154
2941.356513	604822.707185	39.957172
2944.406182	605997.884866	39.962189
2947.750134	607180.449120	39.967207
2950.719332	608360.600010	39.972224
2954.053371	609534.412933	39.977242
2956.970410	610719.478814	39.982260
2960.426555	611899.577939	39.987277
2964.211911	613074.796126	39.992295
2967.371660	614230.438451	39.997312
2971.094794	615392.768208	40.002330
2974.445228	616538.636384	40.007348
2977.713049	617691.948549	40.012365
2980.696847	618832.538381	40.017383
2983.441627	619988.944608	40.022400
2986.507808	621122.783134	40.027418
2989.667629	622274.929095	40.032436
2993.049609	623404.578516	40.037453
2996.175609	624537.749477	40.042471
2998.938234	625662.767420	40.047488
3002.654104	626777.218749	40.052506
3005.556384	627905.174855	40.057524
3008.544434	629030.899544	40.062541
3011.815384	630135.483305	40.067559
3014.667012	631268.084170	40.072576
3017.810785	632376.748764	40.077594
3020.902199	633497.636187	40.082612
3023.784967	634585.641644	40.087629
3026.823879	635657.685310	40.092647
3029.688361	636733.490306	40.097664
3032.709193	637782.309961	40.102682
3035.454276	638867.244971	40.107700
3038.154577	639930.968566	40.112717
3041.151094	640995.979846	40.117735
3043.480912	642086.430727	40.122752
3046.563729	643164.769978	40.127770
3049.205515	644279.025497	40.132788
3051.975798	645366.608662	40.137805
3054.838372	646473.455595	40.142823
3057.835375	647601.347394	40.147840
3061.009214	648710.240294	40.152858
3064.644602	649841.264430	40.157876
3068.051493	650955.452611	40.162893
3071.202388	652061.635081	40.167911
3073.763981	653197.638417	40.172928
3077.077223	654329.650550	40.177946
3080.092784	655475.530528	40.182964
3083.222262	656610.549086	40.187981
3086.403021	657757.331061	40.192999
3089.041261	658907.155759	40.198016
3092.105737	660051.645748	40.203034
3095.092160	661219.961206	40.208052
3098.199103	662384.481860	40.213069
3101.406926	663550.935931	40.218087
3103.950856	664743.088688	40.223104
3107.610341	665919.333334	40.228122
3110.501039	667115.612109	40.233140
3113.301578	668300.910245	40.238157
3116.565161	669511.651662	40.243175
3119.649926	670725.848964	40.248192
3122.305316	671934.291825	40.253210
3125.068670	673166.429334	40.258228
3127.985949	674404.793150	40.263245
3130.660447	675639.652755	40.268263
3133.829025	676901.107434	40.273280
3136.862251	678147.901486	40.278298
3140.022086	679408.867371	40.283316
3142.826039	680682.488573	40.288333
3146.069461	681961.672973	40.293351
3149.198131	683243.727702	40.298368
3152.459297	684532.682430	40.303386
3155.605784	685817.401843	40.308404
3158.607647	687113.829394	40.313421
3161.846468	688409.386596	40.318439
3164.957234	689707.310125	40.323456
3168.049059	691018.448685	40.328474
3171.106548	692345.974039	40.333492
3174.086904	693671.181304	40.338509
3177.203603	694992.448158	40.343527
3180.379140	696327.742897	40.348544
3183.607106	697637.040106	40.353562
3186.999382	698980.674748	40.358580
3190.126674	700309.473118	40.363597
3193.624325	701641.973751	40.368615
3196.613173	702968.159706	40.373632
3200.273032	704301.613795	40.378650
3204.082136	705626.613308	40.383668
3207.488496	706954.299509	40.388685
3211.010557	708259.968468	40.393703
3214.756595	709576.296376	40.398720
3218.289632	710876.364380	40.403738
3221.459698	712183.818956	40.408756
3224.518641	713483.517078	40.413773
3228.203970	714785.436077	40.418791
3231.400963	716074.913206	40.423808
3234.176256	717357.929227	40.428826
3237.126653	718611.186755	40.433844
3240.093803	719881.119988	40.438861
3243.038330	721131.131057	40.443879
3246.018056	722403.693654	40.448896
3248.444262	723664.879969	40.453914
3251.869185	724931.145940	40.458932
3254.790689	726210.941205	40.463949
3258.147039	727496.147736	40.468967
3261.333683	728794.026433	40.473984
3264.705879	730080.206856	40.479002
3267.483968	731390.731190	40.484020
3270.351498	732704.732537	40.489037
3273.535689	734024.047232	40.494055
3276.849514	735352.652301	40.499072
3280.029261	736690.339184	40.504090
3283.233346	738025.429401	40.509108
3286.845697	739370.886718	40.514125
3290.199065	740715.912332	40.519143
3293.524434	742071.615358	40.524160
3296.909568	743426.040040	40.529178
3299.953773	744787.684421	40.534196
3303.235105	746164.632391	40.539213
3306.417072	747542.931678	40.544231
3309.377680	748934.971052	40.549248
3312.362822	750326.067131	40.554266
3315.902442	751732.882296	40.559284
3319.200626	753146.770924	40.564301
3322.561413	754541.429050	40.569319
3326.301719	755958.617504	40.574336
3329.831970	757367.208889	40.579354
3333.104385	758787.838289	40.584372
3335.881190	760227.672948	40.589389
3339.397153	761655.401593	40.594407
3342.456856	763083.378153	40.599424
3346.132167	764522.490584	40.604442
3349.786021	765962.707049	40.609460
3352.929692	767420.724090	40.614477
3356.036476	768855.998239	40.619495
3359.240812	770312.504045	40.624512
3363.007242	771765.976853	40.629530
3366.556245	773221.950011	40.634548
3370.055528	774682.456181	40.639565
3374.104045	776123.036237	40.644583
3378.157193	777566.227855	40.649600
3382.260422	779004.363525	40.654618
3385.565992	780437.094606	40.659636
3389.127297	781852.276986	40.664653
3392.938761	783281.170488	40.669671
3396.799661	784697.509684	40.674688
3400.060823	786108.911151	40.679706
3403.848192	787528.575553	40.684724
3407.031851	788943.742854	40.689741
3410.467017	790339.668945	40.694759
3414.115315	791751.404917	40.699776
3417.291231	793162.103417	40.704794
3420.838119	794571.183994	40.709812
3423.972427	795994.397363	40.714829
3427.440396	797407.424768	40.719847
3430.536736	798834.373186	40.724864
3433.569115	800264.905037	40.729882
3436.246620	801698.575911	40.734900
3439.414319	803146.054310	40.739917
3442.690846	804596.144545	40.744935
3445.532368	806062.331851	40.749952
3448.395433	807517.152442	40.754970
3451.988123	808997.251079	40.759988
3454.916099	810496.927701	40.765005
3458.240539	811969.652947	40.770010
3461.407084	813410.273640	40.775015
3464.504356	814802.518853	40.780020
3468.110834	816119.497515	40.785024
3471.103393	817405.191946	40.790029
3474.239061	818601.510328	40.795034
3477.062331	819727.264341	40.800039
3479.712190	820801.396828	40.805044
3482.620990	821807.868031	40.810048
3485.570758	822746.157664	40.815053
3488.350612	823608.897332	40.820058
3490.884122	824399.209145	40.825063
3493.135692	825133.452078	40.830068
3495.444655	825797.120687	40.835072
3497.337140	826409.326643	40.840077
3499.230370	826954.474739	40.845082
3500.945567	827442.824307	40.850087
3502.932231	827891.220393	40.855092
3504.433746	828262.173967	40.860096
3505.578033	828604.828071	40.865101
3507.011818	828901.101539	40.870106
3508.126981	829162.826009	40.875111
3509.438420	829377.023701	40.880116
3510.461299	829557.164463	40.885120
3511.423652	829708.831126	40.890125
3512.345960	829805.888351	40.895130
3513.054801	829879.532373	40.900135
3513.328554	829941.230954	40.905140
3514.838239	829952.118917	40.910144
3515.451400	829957.146762	40.915149
3516.059119	829912.937112	40.920154
3516.234573	829860.005919	40.925159
3517.000012	829795.985868	40.930164
3517.734703	829710.623155	40.935168
3518.065703	829600.021701	40.940173
3518.519453	829469.027198	40.945178
3518.457108	829332.204226	40.950183
3519.026577	829170.896196	40.955188
3519.769701	828994.703670	40.960192
3519.767908	828815.453824	40.965197
3520.523974	828609.202209	40.970202
3520.731403	828410.168152	40.975207
3520.759782	828176.710816	40.980212
3521.107188	827944.902598	40.985216
3520.988041	827700.458508	40.990221
3521.268388	827455.939253	40.995226
3521.571853	827192.397327	41.000231
3521.519806	826935.452116	41.005236
3521.611693	826657.702377	41.010240
3521.586391	826392.569756	41.015245
3521.962587	826091.338237	41.020250
3521.985558	825818.060887	41.025255
3521.715317	825524.926199	41.030260
3521.962619	825225.631415	41.035264
3521.834004	824924.331921	41.040269
3521.781411	824627.063686	41.045274
3522.052873	824326.110627	41.050279
3521.973567	824030.775415	41.055284
3522.252747	823716.494615	41.060288
3522.144182	823403.436396	41.065293
3521.957069	823074.826455	41.070298
3522.354596	822762.827747	41.075303
3522.050089	822437.677429	41.080308
3521.954144	822114.970830	41.085312
3521.882495	821790.728289	41.090317
3521.874889	821469.393902	41.095322
3522.036734	821139.211536	41.100327
3522.060404	820812.948779	41.105332
3521.654578	820480.626163	41.110336
3521.733982	820158.431080	41.115341
3521.590237	819818.008984	41.120346
3521.406641	819499.103172	41.125351
3521.237662	819168.828408	41.130356
3521.370278	818841.129622	41.135360
3520.762386	818514.173171	41.140365
3520.713508	818194.301713	41.145370
3520.589813	817875.112375	41.150375
3520.811158	817557.661500	41.155380
3521.081291	817243.368679	41.160384
3520.492170	816918.680031	41.165389
3520.461179	816590.652888	41.170394
3520.465202	816269.016181	41.175399
3520.453384	815955.051981	41.180404
3520.230789	815637.436358	41.185408
3519.593119	815322.958475	41.190413
3519.756945	815014.600040	41.195418
3520.032371	814694.899117	41.200423
3519.457677	814395.398172	41.205428
3519.742014	814074.931810	41.210432
3519.477818	813776.918855	41.215437
3519.157079	813458.432799	41.220442
3519.368165	813156.200361	41.225447
3518.905385	812852.400590	41.230452
3519.230258	812544.979658	41.235456
3518.840504	812251.376730	41.240461
3518.724896	811940.523565	41.245466
3518.568512	811643.769855	41.250471
3518.374326	811345.833714	41.255476
3518.478117	811052.342006	41.260480
3518.153526	810767.138513	41.265485
3518.424556	810465.853451	41.270490
3518.053623	810178.036254	41.275495
3517.922666	809888.158361	41.280500
3517.905693	809585.607867	41.285504
3517.460305	809306.095532	41.290509
3517.613176	809020.543628	41.295514
3517.673334	808744.501760	41.300519
3517.188480	808464.373255	41.305524
3517.299662	808174.382175	41.310528
3517.255497	807894.745483	41.315533
3517.355794	807616.347743	41.320538
3516.971752	807341.547651	41.325543
3516.717878	807070.048039	41.330548
3516.460151	806779.568385	41.335552
3516.274225	806523.672465	41.340557
3516.339629	806263.852726	41.345562
3516.621303	805995.751440	41.350567
3516.158190	805730.704232	41.355572
3516.475707	805459.242270	41.360576
3515.871402	805191.599057	41.365581
3515.825829	804939.248808	41.370586
3515.935834	804675.536970	41.375591
3515.770315	804414.851637	41.380596
3515.646070	804160.867592	41.385600
3515.129086	803912.137109	41.390605
3515.451163	803658.256874	41.395610
3515.293569	803417.246465	41.400615
3515.021527	803159.571673	41.405620
3514.836941	802911.779970	41.410624
3514.503854	802681.611823	41.415629
3514.870971	802439.499517	41.420634
3515.161351	802200.334422	41.425639
3514.479586	801965.491106	41.430644
3514.514338	801714.235480	41.435648
3514.687628	801474.819307	41.440653
3514.332663	801245.146425	41.445658
3514.143077	801001.015223	41.450663
3514.191166	800778.864390	41.455668
3514.006760	800540.603347	41.460672
3513.793944	800326.772634	41.465677
3513.862820	800082.271908	41.470682
3513.829649	799872.862459	41.475687
3513.464258	799642.990889	41.480692
3513.724559	799416.737648	41.485696
3513.308542	799189.116626	41.490701
3513.336983	798982.369054	41.495706
3513.328751	798756.727547	41.500711
3513.022742	798535.839262	41.505716
3512.907030	798328.703438	41.510720
3512.559187	798128.421839	41.515725
3512.895559	797910.352294	41.520730
3512.835486	797702.845069	41.525735
3512.534614	797496.058622	41.530740
3512.487972	797284.855428	41.535744
3512.573294	797078.140016	41.540749
3512.404784	796882.750708	41.545754
3512.091281	796680.409163	41.550759
3512.141589	796494.741653	41.555764
3511.976429	796286.767813	41.560768
3512.236239	796090.647348	41.565773
3512.302332	795900.984850	41.570778
3512.072628	795697.079010	41.575783
3511.758529	795499.563897	41.580788
3511.827422	795297.168187	41.585792
3511.484574	795114.474932	41.590797
3511.390791	794934.534558	41.595802
3511.586953	794736.226158	41.600807
3511.542078	794547.822005	41.605812
3511.386003	794365.274761	41.610816
3511.138288	794182.787014	41.615821
3510.879929	793999.117675	41.620826
3511.062186	793812.080369	41.625831
3510.576341	793645.873306	41.630836
3510.890518	793468.283442	41.635840
3510.758084	793294.004372	41.640845
3510.894075	793124.489852	41.645850
3510.784955	792946.563840	41.650855
3510.819950	792773.324746	41.655860
3510.742498	792597.054639	41.660864
3510.402324	792430.893010	41.665869
3510.376574	792263.152766	41.670874
3510.390293	792079.044456	41.675879
3510.004383	791927.320305	41.680884
3510.211360	791749.852173	41.685888
3510.210839	791594.176364	41.690893
3510.031710	791424.034363	41.695898
3510.204706	791255.598667	41.700903
3509.789562	791102.780802	41.705908
3510.048112	790930.442053	41.710912
3509.967755	790773.926144	41.715917
3509.661715	790607.322860	41.720922
3509.779024	790471.992627	41.725927
3509.584024	790313.814952	41.730932
3509.723245	790158.674031	41.735936
3509.603652	789999.887256	41.740941
3509.245155	789841.578632	41.745946
3509.663444	789696.946013	41.750951
3509.361232	789549.038881	41.755956
3509.644895	789392.530548	41.760960
3509.261899	789239.667115	41.765965
3509.697143	789082.733768	41.770970
3509.689467	788934.961726	41.775975
3509.349736	788788.715817	41.780980
3508.755889	788635.628482	41.785984
3508.905504	788488.902369	41.790989
3509.082762	788353.521786	41.795994
3508.988953	788205.306462	41.800999
3508.813003	788061.377648	41.806004
3508.765352	787916.048499	41.811008
3508.686021	787778.880797	41.816013
3508.342792	787648.389656	41.821018
3508.606009	787494.447975	41.826023
3508.264668	787373.831361	41.831028
3508.520788	787233.255210	41.836032
3508.447829	787108.313227	41.841037
3508.305944	786967.306033	41.846042
3508.438222	786833.132897	41.851047
3508.199854	786708.997776	41.856052
3508.019221	786572.167687	41.861056
3507.893579	786456.514218	41.866061
3507.538873	786324.476735	41.871066
3507.997189	786210.295957	41.876071
3507.811519	786082.404875	41.881076
3507.839723	785955.705267	41.886080
3507.661820	785830.414093	41.891085
3507.558332	785720.054863	41.896090
3507.683500	785590.776137	41.901095
3507.426604	785478.717693	41.906100
3507.517075	785356.618922	41.911104
3507.257574	785244.262224	41.916109
3507.303434	785129.345636	41.921114
3507.608713	785006.369506	41.926119
3507.263981	784893.185475	41.931124
3507.074317	784787.349874	41.936128
3507.318701	784679.572411	41.941133
3507.210172	784564.770621	41.946138
3507.725360	784451.929260	41.951143
3507.317944	784338.697649	41.956148
3507.459690	784218.587195	41.961152
3507.068754	784109.775097	41.966157
3506.901806	783999.891603	41.971162
3507.299353	783887.650941	41.976167
3506.985413	783779.411248	41.981172
3507.084112	783666.724723	41.986176
3506.682531	783559.676516	41.991181
3506.682317	783443.707729	41.996186
3506.729364	783343.320024	42.001191
3506.904951	783250.631382	42.006196
3506.955101	783135.091937	42.011200
3506.392252	783042.178342	42.016205
3506.631491	782937.621737	42.021210
3506.871894	782826.079055	42.026215
3506.743244	782730.335280	42.031220
3506.829260	782628.701501	42.036224
3506.655364	782523.469342	42.041229
3506.748968	782422.421651	42.046234
3506.462308	782307.465644	42.051239
3506.362269	782226.172059	42.056244
3506.221985	782123.240415	42.061248
3506.321936	782031.188044	42.066253
3506.473389	781932.288329	42.071258
3506.427840	781828.844908	42.076263
3506.084032	781738.436287	42.081268
3506.004161	781641.932083	42.086272
3506.173090	781553.453362	42.091277
3506.088300	781459.505639	42.096282
3506.069168	781367.956431	42.101287
3505.746781	781284.278377	42.106292
3505.992636	781189.288575	42.111296
3505.917059	781100.647919	42.116301
3505.905069	781022.770040	42.121306
3506.230325	780922.745416	42.126311
3505.849595	780846.156531	42.131316
3506.168223	780742.784964	42.136320
3505.874036	780651.321322	42.141325
3505.366527	780575.144117	42.146330
3505.785627	780488.037838	42.151335
3505.612230	780400.339586	42.156340
3505.475730	780317.800470	42.161344
3505.615911	780234.673456	42.166349
3505.400864	780153.916770	42.171354
3505.496651	780068.827030	42.176359
3505.657734	780002.029767	42.181364
3505.171305	779910.244081	42.186368
3505.770209	779841.650797	42.191373
3505.006114	779756.847097	42.196378
3505.471169	779666.721743	42.201383
3505.331964	779603.956215	42.206388
3505.259519	779528.532621	42.211392
3505.111435	779444.607634	42.216397
3505.011064	779377.208100	42.221402
3505.219943	779294.157360	42.226407
3505.171398	779220.399743	42.231412
3505.289323	779143.562799	42.236416
3505.058108	779073.918371	42.241421
3504.684586	778996.865813	42.246426
3504.981876	778922.555902	42.251431
3505.065534	778859.107338	42.256436
3504.850575	778785.077517	42.261440
3504.869269	778718.833308	42.266445
3504.736903	778652.564241	42.271450
3504.938146	778586.633160	42.276455
3505.072523	778523.074851	42.281460
3504.831039	778444.173649	42.286464
3504.688176	778378.789699	42.291469
3504.774509	778315.532808	42.296474
3504.824288	778241.699782	42.301479
3504.746838	778174.186854	42.306484
3504.804655	778101.236985	42.311488
3505.097276	778042.816200	42.316493
3504.581304	777969.024673	42.321498
3504.779322	777894.917536	42.326503
3504.479930	777839.103122	42.331508
3504.603014	777776.327665	42.336512
3504.639845	777708.397768	42.341517
3504.429385	777642.575380	42.346522
3504.580008	777582.156303	42.351527
3504.346916	777533.318016	42.356532
3504.707497	777455.192583	42.361536
3504.740609	777395.185151	42.366541
3504.535397	777333.493799	42.371546
3504.840111	777275.360198	42.376551
3504.622495	777217.115550	42.381556
3504.484505	777143.696201	42.386560
3504.541759	777080.088808	42.391565
3504.319512	777011.555299	42.396570
3504.723429	776950.055397	42.401575
3504.106948	776893.695419	42.406580
3504.388029	776826.307647	42.411584
3504.470377	776777.904433	42.416589
3504.128547	776714.556702	42.421594
3504.386034	776658.099711	42.426599
3504.159001	776597.144143	42.431604
3504.323988	776535.532546	42.436608
3504.169984	776482.785097	42.441613
3504.105476	776412.644571	42.446618
3504.220596	776355.076488	42.451623
3504.070891	776306.265424	42.456628
3503.991325	776246.857920	42.461632
3504.212203	776191.338747	42.466637
3503.926757	776148.358283	42.471642
3504.067069	776092.457823	42.476647
3503.711685	776045.402100	42.481652
3503.948863	776001.103616	42.486656
3503.767473	775953.280067	42.491661
3504.068849	775899.222344	42.496666
3504.013880	775839.118199	42.501671
3503.915594	775796.646302	42.506676
3503.728339	775740.403409	42.511680
3503.569001	775692.476041	42.516685
3503.161796	775641.979891	42.521690
3503.733029	775592.109468	42.526695
3503.646114	775555.591697	42.531700
3504.017081	775512.991375	42.536704
3503.654834	775463.274326	42.541709
3503.827586	775420.263097	42.546714
3504.025601	775360.851756	42.551719
3503.697127	775330.822738	42.556724
3503.572332	775275.944573	42.561728
3504.003000	775224.519295	42.566733
3503.459161	775179.901761	42.571738
3503.321424	775137.777217	42.576743
3503.254166	775095.640784	42.581748
3503.475342	775036.075265	42.586752
3503.545867	774999.380986	42.591757
3503.259008	774961.810036	42.596762
3503.625227	774921.176619	42.601767
3503.491005	774881.561223	42.606772
3503.414320	774823.668103	42.611776
3503.152139	774786.584575	42.616781
3503.293093	774746.036651	42.621786
3503.375480	774707.369329	42.626791
3503.314412	774670.547425	42.631796
3503.276956	774627.664760	42.636800
3503.569568	774591.128703	42.641805
3503.190154	774555.343654	42.646810
3503.535233	774510.821357	42.651815
3503.512290	774478.276246	42.656820
3503.109337	774425.259632	42.661824
3503.110693	774393.448768	42.666829
3502.867919	774354.390129	42.671834
3503.196664	774305.880594	42.676839
3503.055420	774284.089230	42.681844
3503.004820	774243.816400	42.686848
3503.374062	774217.213072	42.691853
3502.964215	774173.010448	42.696858
3503.210811	774139.582140	42.701863
3503.241224	774100.969454	42.706868
3503.224992	774054.337320	42.711872
3503.351229	774010.291356	42.716877
3503.214226	773978.156836	42.721882
3503.197688	773935.906861	42.726887
3503.155211	773911.734265	42.731892
3503.571649	773865.866622	42.736896
3503.035213	773829.956236	42.741901
3503.144817	773790.540885	42.746906
3503.120162	773746.222789	42.751911
3502.842066	773718.887424	42.756916
3502.920431	773681.742030	42.761920
3503.159956	773648.903629	42.766925
3502.977808	773611.702433	42.771930
3503.278302	773574.322798	42.776935
3502.953305	773544.581364	42.781940
3503.175974	773512.139126	42.786945
3503.226827	773471.943793	42.791949
3503.023387	773434.351225	42.796954
3503.130298	773400.647142	42.801959
3503.021435	773368.653051	42.806964
3502.654500	773323.108468	42.811969
3503.235833	773294.496756	42.816973
3502.918211	773251.947846	42.821978
3503.192277	773221.958361	42.826983
3502.950243	773197.126878	42.831988
3502.994092	773160.033802	42.836993
3502.881361	773125.084221	42.841997
3502.900260	773103.262886	42.847002
3502.864811	773049.830839	42.852007
3503.095078	773035.263648	42.857012
3502.973470	772993.518135	42.862017
3502.960544	772960.816884	42.867021
3502.793793	772936.858625	42.872026
3503.224591	772898.616732	42.877031
3502.611479	772876.357378	42.882036
3502.746460	772841.267009	42.887041
3503.176958	772814.254462	42.892045
3502.747796	772790.831623	42.897050
3502.787016	772747.038737	42.902055
3502.596396	772717.123982	42.907060
3502.506400	772695.073161	42.912065
3502.993998	772657.953481	42.917069
3502.601476	772631.913591	42.922074
3502.744381	772592.978865	42.927079
3502.705919	772573.825204	42.932084
3502.786332	772534.555710	42.937089
3502.818702	772513.222953	42.942093
3502.809505	772495.443405	42.947098
3502.697976	772462.263676	42.952103
3502.542317	772420.520537	42.957108
3502.998037	772403.944602	42.962113
3502.900025	772367.265021	42.967117
3502.418641	772343.947898	42.972122
3502.837901	772310.778289	42.977127
3502.564081	772294.273403	42.982132
3502.523446	772259.800366	42.987137
3502.687409	772229.775780	42.992141
3502.837209	772203.250697	42.997146
3502.748653	772177.060452	43.002151
3502.741980	772155.782370	43.007156
3502.432871	772120.909726	43.012161
3502.766971	772106.077253	43.017165
3502.451073	772065.491517	43.022170
3502.823261	772038.337992	43.027175
3502.646388	772018.614655	43.032180
3502.810054	771987.406921	43.037185
3502.584643	771956.657421	43.042189
3502.631565	771937.438737	43.047194
3502.345201	771901.083513	43.052199
3502.121521	771888.608713	43.057204
3502.399605	771867.873860	43.062209
3502.476994	771836.778265	43.067213
3502.343254	771830.396738	43.072218
3502.513295	771794.753732	43.077223
3502.508758	771787.217832	43.082228
3502.306912	771740.355396	43.087233
3502.492455	771737.714096	43.092237
3502.858374	771715.486483	43.097242
3502.771388	771676.141556	43.102247
3502.837712	771655.933711	43.107252
3502.265788	771620.905083	43.112257
3502.308069	771609.371088	43.117261
3502.292882	771588.585391	43.122266
3502.266222	771552.530364	43.127271
3502.503234	771532.638810	43.132276
3502.233994	771513.766838	43.137281
3502.378565	771482.757174	43.142285
3502.186487	771480.523019	43.147290
3502.225994	771441.845613	43.152295
3502.279896	771426.417664	43.157300
3502.183120	771416.926119	43.162305
3502.338968	771376.012317	43.167309
3502.224516	771367.508890	43.172314
3502.090533	771339.943809	43.177319
3502.030090	771320.790524	43.182324
3502.245619	771305.040034	43.187329
3501.964571	771285.775320	43.192333
3502.134204	771278.505702	43.197338
3502.429603	771281.166566	43.202343
3502.067560	771247.480862	43.207348
3502.203337	771224.895693	43.212353
3502.207101	771219.476195	43.217357
3502.335465	771196.695108	43.222362
3502.367159	771178.018870	43.227367
3502.636402	771153.046737	43.232372
3502.367996	771130.626597	43.237377
3502.320251	771104.967711	43.242381
3502.409908	771076.182334	43.247386
3502.218487	771068.380991	43.252391
3502.235479	771044.878863	43.257396
3502.383849	771029.335945	43.262401
3502.593144	770995.603946	43.267405
3501.916013	770988.720293	43.272410
3502.425375	770961.392350	43.277415
3502.333382	770935.838720	43.282420
3502.051416	770917.312184	43.287425
3502.330328	770902.831284	43.292429
3502.372534	770880.309791	43.297434
3502.425311	770866.260317	43.302439
3502.192657	770836.689736	43.307444
3502.166158	770812.799924	43.312449
3502.368173	770794.340906	43.317453
3501.832031	770779.551044	43.322458
3502.465324	770760.035333	43.327463
3502.455947	770742.202322	43.332468
3502.105791	770717.281803	43.337473
3502.422452	770700.133826	43.342477
3502.304991	770675.618123	43.347482
3502.439417	770659.978198	43.352487
3502.118346	770638.008674	43.357492
3502.009884	770624.675137	43.362497
3502.113376	770599.088039	43.367501
3501.421599	770585.013259	43.372506
3502.362535	770574.462324	43.377511
3502.301097	770570.531177	43.382516
3502.381786	770550.761352	43.387521
3502.538207	770529.550168	43.392525
3501.983255	770510.279420	43.397530
3502.006198	770486.577459	43.402535
3502.555877	770478.160338	43.407540
3502.313088	770453.171916	43.412545
3502.248656	770426.675856	43.417549
3502.251235	770410.318150	43.422554
3502.512020	770387.709768	43.427559
3502.077315	770370.734458	43.432564
3501.472157	770357.334705	43.437569
3501.986958	770325.027261	43.442573
3501.887141	770327.655241	43.447578
3502.237873	770311.781758	43.452583
3501.985628	770299.161174	43.457588
3501.895342	770278.532010	43.462593
3502.117561	770280.072115	43.467597
3501.876987	770259.566273	43.472602
3502.152480	770231.978664	43.477607
3502.177523	770236.113436	43.482612
3501.776722	770219.033632	43.487617
3501.895277	770186.298354	43.492621
3501.740688	770173.957045	43.497626
3502.220173	770167.078576	43.502631
3502.317710	770162.923858	43.507636
3501.995237	770138.834420	43.512641
3502.241653	770122.977770	43.517645
3502.080512	770107.828963	43.522650
3502.125443	770080.525247	43.527655
3501.955281	770076.759618	43.532660
3501.834732	770056.923184	43.537665
3501.875275	770030.063454	43.542669
3501.708786	770032.160563	43.547674
3502.016314	770013.829981	43.552679
3501.871121	770015.332311	43.557684
3501.887278	769991.137163	43.562689
3502.062743	769969.477778	43.567693
3501.967398	769969.247344	43.572698
3502.164494	769949.752314	43.577703
3502.200452	769932.451857	43.582708
3502.065285	769919.417097	43.587713
3502.383448	769901.626481	43.592717
3501.934730	769883.026358	43.597722
3502.158506	769861.309401	43.602727
3502.056153	769848.515458	43.607732
3501.895627	769833.415260	43.612737
3502.430196	769814.258295	43.617741
3502.000659	769809.697740	43.622746
3502.110565	769773.414375	43.627751
3502.068058	769778.348944	43.632756
3502.083130	769761.347181	43.637761
3502.384788	769726.115923	43.642765
3502.148007	769724.677001	43.647770
3502.093036	769698.866609	43.652775
3501.854991	769695.752566	43.657780
3502.135917	769689.645584	43.662785
3502.186079	769664.211892	43.667789
3502.318452	769650.048409	43.672794
3502.168784	769636.128603	43.677799
3502.560187	769598.467450	43.682804
3502.175325	769586.951611	43.687809
3502.257553	769570.726713	43.692813
3502.140883	769540.441931	43.697818
3502.309848	769530.263469	43.702823
3502.032395	769505.228296	43.707828
3502.412772	769489.495984	43.712833
3502.629121	769476.747286	43.717837
3501.920871	769451.388912	43.722842
3502.259272	769433.298175	43.727847
3502.297948	769418.410593	43.732852
3502.021203	769399.485178	43.737857
3502.321831	769379.528056	43.742861
3502.102368	769361.972816	43.747866
3502.169155	769340.083170	43.752871
3502.085411	769330.438960	43.757876
3502.072355	769306.098573	43.762881
3502.055526	769290.086538	43.767885
3501.648858	769288.429218	43.772890
3501.801324	769278.105306	43.777895
3501.789805	769254.700760	43.782900
3502.036406	769249.338247	43.787905
3502.146348	769236.508166	43.792909
3501.807972	769223.456480	43.797914
3501.971202	769200.417106	43.802919
3501.748683	769190.105759	43.807924
3501.795311	769188.964842	43.812929
3502.085190	769172.556928	43.817933
3501.594330	769153.814099	43.822938
3502.006524	769142.116578	43.827943
3501.997016	769135.909301	43.832948
3501.868566	769133.269689	43.837953
3502.157293	769100.649332	43.842957
3501.771478	769101.353876	43.847962
3502.253518	769072.643707	43.852967
3501.827625	769054.727623	43.857972
3501.565539	769041.022388	43.862977
3502.106647	769035.463220	43.867981
3501.987119	769033.019213	43.872986
3502.135884	769008.059764	43.877991
3501.956658	768999.416477	43.882996
3501.887072	769003.912525	43.888001
3501.993480	768980.438348	43.893005
3501.937070	768956.153256	43.898010
3501.855491	768944.537019	43.903015
3501.984523	768943.924519	43.908020
3501.998283	768931.848995	43.913025
3502.263621	768911.157258	43.918029
3502.060960	768904.390351	43.923034
3501.897189	768879.186437	43.928039
3501.967625	768863.848977	43.933044
3501.549962	768860.567142	43.938049
3501.846190	768849.233283	43.943053
3501.594296	768854.695864	43.948058
3501.724891	768822.001855	43.953063
3501.955489	768808.559737	43.958068
3501.972637	768800.820090	43.963073
3501.980937	768798.650563	43.968077
3501.708692	768770.950915	43.973082
3501.863203	768750.671288	43.978087
3501.867466	768750.375074	43.983092
3501.746600	768748.325437	43.988097
3501.979780	768735.868372	43.993101
3501.555076	768722.682226	43.998106
3501.817869	768710.417348	44.003111
3501.702696	768702.354499	44.008116
3501.595006	768709.074659	44.013121
3501.872657	768686.704715	44.018125
3501.935871	768666.637069	44.023130
3501.468152	768647.445602	44.028135
3501.549861	768650.290583	44.033140
3501.807266	768643.250289	44.038145
3502.335670	768632.124141	44.043149
3501.670364	768610.599725	44.048154
3501.699956	768598.373198	44.053159
3502.016904	768593.195716	44.058164
3501.697972	768584.969283	44.063169
3501.889269	768552.707592	44.068173
3501.722398	768548.201410	44.073178
3501.610886	768551.571176	44.078183
3501.898688	768545.166431	44.083188
3501.634522	768547.674351	44.088193
3502.064392	768521.927590	44.093197
3501.862878	768516.687882	44.098202
3502.078929	768497.530883	44.103207
3502.071700	768498.320767	44.108212
3501.810028	768467.661306	44.113217
3502.010436	768455.554165	44.118221
3501.838014	768453.907225	44.123226
3501.701033	768447.868285	44.128231
3501.880260	768407.772033	44.133236
3501.753007	768413.115775	44.138241
3501.856647	768405.262859	44.143245
3501.738230	768413.217129	44.148250
3501.948266	768389.132567	44.153255
3502.038792	768370.784512	44.158260
3501.787283	768353.133611	44.163265
3501.890521	768359.277118	44.168269
3501.652640	768340.244007	44.173274
3502.043492	768306.026225	44.178279
3502.200535	768309.992408	44.183284
3501.842845	768300.737110	44.188289
3501.832698	768269.049595	44.193293
3501.869086	768271.015105	44.198298
3501.671545	768248.328097	44.203303
3501.975976	768265.379444	44.208308
3501.767618	768249.938935	44.213313
3501.685828	768232.111850	44.218317
3501.640840	768221.868386	44.223322
3501.621268	768210.339320	44.228327
3501.410430	768205.840194	44.233332
3501.402131	768209.883037	44.238337
3501.795146	768199.813586	44.243341
3501.963912	768177.854379	44.248346
3501.988259	768165.085879	44.253351
3501.964352	768159.471578	44.258356
3501.941762	768153.167072	44.263361
3501.936988	768135.869159	44.268365
3501.752563	768136.737646	44.273370
3501.623410	768129.612891	44.278375
3501.847298	768125.682580	44.283380
3501.836623	768107.202743	44.288385
3502.099111	768082.664960	44.293389
3501.599150	768071.510770	44.298394
3502.137947	768077.286827	44.303399
3502.084033	768041.712061	44.308404
3501.656591	768037.248624	44.313409
3501.860345	768031.498036	44.318413
3501.979857	768031.922029	44.323418
3502.052153	768007.563282	44.328423
3502.098438	767989.960879	44.333428
3501.763778	767975.526382	44.338433
3501.744829	767975.135401	44.343437
3501.662270	767950.309199	44.348442
3501.672441	767946.611253	44.353447
3501.811131	767937.569192	44.358452
3501.728357	767944.088781	44.363457
3501.725267	767934.035140	44.368461
3501.668433	767903.536645	44.373466
3501.749785	767888.638946	44.378471
3501.752726	767876.957785	44.383476
3501.445129	767890.414654	44.388481
3501.800944	767875.323715	44.393485
3501.729157	767882.827269	44.398490
3501.708419	767859.025559	44.403495
3502.029643	767835.610843	44.408500
3501.782703	767849.895634	44.413505
3501.756609	767833.881990	44.418509
3501.883298	767836.818425	44.423514
3501.837770	767811.394200	44.428519
3501.965545	767791.461385	44.433524
3501.540292	767789.560354	44.438529
3501.634441	767783.679826	44.443533
3501.836829	767766.938266	44.448538
3501.787986	767750.780341	44.453543
3502.133285	767737.908785	44.458548
3501.631877	767743.314833	44.463553
3502.135421	767731.649297	44.468557
3501.866815	767710.845307	44.473562
3501.542814	767701.485117	44.478567
3501.368173	767689.487994	44.483572
3501.209087	767692.126695	44.488577
3501.467857	767685.627438	44.493581
3501.580631	767681.567393	44.498586
3501.750141	767680.356653	44.503591
3501.769730	767668.918852	44.508596
3501.738061	767653.842209	44.513601
3502.092656	767644.517676	44.518605
3501.630860	767658.148307	44.523610
3501.516176	767644.120404	44.528615
3502.108838	767617.259287	44.533620
3501.803320	767602.424943	44.538625
3501.729086	767589.474592	44.543629
3501.844377	767596.947521	44.548634
3501.757289	767578.331132	44.553639
3501.530813	767553.773829	44.558644
3501.636628	767559.276823	44.563649
3501.719692	767547.335463	44.568653
3501.650728	767549.910034	44.573658
3501.187372	767550.233216	44.578663
3502.078281	767548.853960	44.583668
3501.597426	767532.914815	44.588673
3501.698367	767513.478576	44.593677
3501.430225	767500.461535	44.598682
3501.845443	767497.238611	44.603687
3501.911472	767497.720762	44.608692
3501.472503	767484.929077	44.613697
3501.976169	767461.975931	44.618701
3501.748606	767452.451623	44.623706
3501.683810	767452.955395	44.628711
3501.844724	767445.831341	44.633716
3501.755582	767444.367569	44.638721
3502.081712	767412.867287	44.643725
3501.887856	767424.433202	44.648730
3502.055700	767406.809334	44.653735
3501.922099	767388.791631	44.658740
3501.658999	767389.032439	44.663745
3501.740050	767376.548953	44.668749
3501.945139	767360.939696	44.673754
3501.912493	767355.178363	44.678759
3501.980617	767336.486432	44.683764
3501.751075	767326.370811	44.688769
3502.073076	767313.206633	44.693773
3502.029561	767306.609128	44.698778
3501.857829	767279.429497	44.703783
3501.821329	767262.529119	44.708788
3501.730682	767275.754083	44.713793
3501.823417	767257.649371	44.718797
3501.933073	767228.599312	44.723802
3501.686683	767219.521432	44.728807
3501.979458	767214.396285	44.733812
3502.006846	767216.610014	44.738817
3502.071873	767186.285607	44.743821
3502.048792	767181.705540	44.748826
3501.740778	767163.469657	44.753831
3501.999045	767145.978104	44.758836
3501.807143	767136.299624	44.763841
3501.781082	767115.010267	44.768845
3501.566703	767125.347752	44.773850
3501.887712	767112.380551	44.778855
3501.958256	767092.307449	44.783860
3501.927331	767084.919002	44.788865
3501.797496	767073.603563	44.793869
3501.716385	767079.236384	44.798874
3501.585584	767051.753409	44.803879
3501.659214	767038.432623	44.808884
3501.526926	767038.996867	44.813889
3501.903729	767019.858800	44.818893
3501.654947	767023.547689	44.823898
3501.711761	767021.665380	44.828903
3501.972492	767007.623534	44.833908
3501.602448	766987.376494	44.838913
3501.753090	766980.795908	44.843917
3501.582840	766993.492312	44.848922
3501.891044	766978.703184	44.853927
3501.728853	766950.781394	44.858932
3501.408420	766946.792535	44.863937
3501.682814	766940.782975	44.868941
3501.824244	766941.301995	44.873946
3501.555459	766942.973237	44.878951
3501.463420	766923.370179	44.883956
3501.508530	766929.425889	44.888961
3501.939026	766908.602716	44.893965
3501.577709	766894.071934	44.898970
3501.712691	766885.423554	44.903975
3501.901114	766883.963098	44.908980
3501.353467	766889.229518	44.913985
3501.356039	766875.821598	44.918989
3501.516594	766877.076857	44.923994
3501.269808	766852.274130	44.928999
3501.628029	766841.370620	44.934004
3501.509967	766831.482369	44.939009
3501.540080	766834.139400	44.944013
3501.412481	766837.068958	44.949018
3501.531821	766839.711244	44.954023
3501.844477	766829.603936	44.959028
3501.694332	766843.184551	44.964033
3501.478155	766812.165692	44.969037
3501.742575	766797.432735	44.974042
3501.408999	766795.072650	44.979047
3501.679297	766794.288756	44.984052
3501.560039	766789.477874	44.989057
3501.427125	766790.338000	44.994061
3501.359141	766793.060550	44.999066
3501.432859	766797.238487	45.004071
3501.491655	766785.497092	45.009076
3501.267423	766783.661163	45.014081
3501.576806	766765.125108	45.019085
3501.402020	766759.879739	45.024090
3501.396915	766745.043335	45.029095
3501.967481	766742.188771	45.034100
3501.480430	766744.783412	45.039105
3501.271469	766742.994244	45.044109
3501.503761	766744.286966	45.049114
3501.685811	766743.665530	45.054119
3502.012608	766722.908271	45.059124
3501.826094	766718.453514	45.064129
3501.693894	766698.314266	45.069133
3501.621059	766696.305416	45.074138
3501.591374	766693.895082	45.079143
3501.957895	766685.109621	45.084148
3501.582826	766665.947009	45.089153
3501.833468	766655.110299	45.094157
3501.393114	766646.704597	45.099162
3501.513837	766648.558011	45.104167
3501.597242	766645.241673	45.109172
3501.222859	766650.183862	45.114177
3501.509403	766640.129909	45.119181
3501.452794	766633.780443	45.124186
3501.545476	766620.652942	45.129191
3501.728552	766611.947003	45.134196
3501.348996	766614.277451	45.139201
3501.818924	766605.869168	45.144205
3501.718518	766607.759132	45.149210
3501.599521	766602.553728	45.154215
3501.733424	766599.130436	45.159220
3501.464968	766574.182479	45.164225
3501.608473	766565.680206	45.169229
3501.808319	766558.992529	45.174234
3501.809092	766560.717900	45.179239
3501.646323	766549.998647	45.184244
3501.435171	766541.407066	45.189249
3501.607510	766510.766409	45.194253
3501.281941	766513.580920	45.199258
3501.525997	766515.660464	45.204263
3502.030451	766505.225254	45.209268
3501.541382	766516.101926	45.214273
3501.427349	766516.761782	45.219277
3501.834026	766517.335593	45.224282
3501.539536	766494.609961	45.229287
3502.013227	766475.602378	45.234292
3501.533334	766472.576229	45.239297
3501.367365	766464.420753	45.244301
3501.818878	766470.853340	45.249306
3501.491833	766468.393479	45.254311
3501.839107	766462.322198	45.259316
3501.691731	766442.973499	45.264321
3501.576050	766423.274441	45.269325
3501.724104	766427.144527	45.274330
3501.733884	766431.875490	45.279335
3501.892541	766423.271959	45.284340
3501.766995	766394.356110	45.289345
3501.808296	766388.877587	45.294349
3501.798237	766383.506139	45.299354
3501.569525	766381.276481	45.304359
3501.850680	766379.061161	45.309364
3501.796515	766350.724902	45.314369
3501.730879	766338.461105	45.319373
3501.997836	766327.719819	45.324378
3501.682106	766337.828657	45.329383
3501.883627	766312.604978	45.334388
3501.775674	766307.644026	45.339393
3501.854064	766287.764651	45.344397
3501.762670	766283.836179	45.349402
3501.703149	766283.205329	45.354407
3502.026585	766272.109552	45.359412
3501.940647	766255.017872	45.364417
3501.905671	766252.460378	45.369421
3501.852051	766250.398935	45.374426
3501.917937	766228.894667	45.379431
3502.008909	766204.970620	45.384436
3501.716097	766193.089205	45.389441
3501.894135	766185.813229	45.394445
3501.899954	766164.220105	45.399450
3501.708333	766159.667261	45.404455
3501.831729	766153.879214	45.409460
3501.798376	766152.455265	45.414465
3501.598490	766135.283544	45.419469
3501.735405	766112.929141	45.424474
3501.639738	766105.353230	45.429479
3501.560411	766094.570235	45.434484
3501.659746	766108.258854	45.439489
3501.871015	766101.568882	45.444493
3501.682294	766091.642026	45.449498
3501.513485	766072.443802	45.454503
3501.837828	766063.565988	45.459508
3501.466557	766056.282061	45.464513
3501.651628	766057.286918	45.469517
3501.560495	766052.963895	45.474522
3501.228908	766057.061327	45.479527
3501.641067	766048.021088	45.484532
3501.628369	766039.790521	45.489537
3501.699915	766017.545231	45.494541
3501.710739	766002.408928	45.499546
3501.437557	766016.948050	45.504551
3501.605726	766004.053484	45.509556
3501.660370	765995.663845	45.514561
3501.977970	765993.738184	45.519565
3501.814529	765969.017343	45.524570
3501.516508	765966.010228	45.529575
3501.801018	765960.343305	45.534580
3501.768806	765971.884756	45.539585
3501.804324	765948.067648	45.544589
3501.979157	765919.198920	45.549594
3501.882615	765914.580915	45.554599
3502.210874	765909.892711	45.559604
3501.927451	765905.009785	45.564609
3502.072993	765879.054404	45.569613
3501.892391	765878.049130	45.574618
3501.582065	765874.748215	45.579623
3501.993768	765846.480959	45.584628
3501.617648	765831.851948	45.589633
3501.634420	765826.968665	45.594637
3501.535417	765828.365594	45.599642
3501.608969	765823.325026	45.604647
3501.870386	765817.711112	45.609652
3501.592367	765796.804728	45.614657
3501.507275	765783.655833	45.619661
3501.793192	765779.122445	45.624666
3501.714974	765773.515320	45.629671
3501.661736	765772.834088	45.634676
3501.715062	765765.134610	45.639681
3501.595801	765744.004643	45.644685
3501.814947	765734.848022	45.649690
3501.389809	765722.001711	45.654695
3501.572285	765727.591993	45.659700
3501.239982	765730.161404	45.664705
3501.674851	765727.526091	45.669709
3501.717738	765721.603113	45.674714
3501.532017	765703.540647	45.679719
3501.953342	765690.406507	45.684724
3501.669701	765686.509488	45.689729
3501.886549	765677.895486	45.694733
3501.916566	765670.249063	45.699738
3502.059447	765654.202816	45.704743
3502.002667	765632.766404	45.709748
3501.317688	765641.063753	45.714753
3501.510372	765638.369827	45.719757
3502.052437	765622.208247	45.724762
3501.438612	765613.139820	45.729767
3501.795745	765597.353855	45.734772
3501.703029	765597.714459	45.739777
3501.595936	765588.512965	45.744781
3501.566259	765586.743191	45.749786
3501.778504	765581.186527	45.754791
3501.691743	765552.606120	45.759796
3501.755011	765548.454496	45.764801
3501.852308	765544.987472	45.769805
3501.855948	765546.614001	45.774810
3501.487400	765513.001927	45.779815
3501.565037	765445.938336	45.784820
3501.467870	765317.865888	45.789825
3501.633234	765152.819028	45.794829
3501.389684	764919.695735	45.799834
3501.367917	764622.527283	45.804839
3500.930153	764277.486558	45.809844
3500.653003	763873.573567	45.814849
3500.744162	763415.429506	45.819853
3500.386769	762904.215179	45.824858
3500.185638	762335.824703	45.829863
3499.878044	761699.535338	45.834868
3499.458474	761019.700639	45.839873
3499.279530	760270.447838	45.844877
3498.927213	759461.298451	45.849882
3498.351836	758599.298309	45.854887
3498.314139	757671.965608	45.859892
3497.562605	756688.022762	45.864897
3497.245646	755648.689962	45.869901
3496.854915	754541.241300	45.874906
3495.884500	753381.928203	45.879911
3495.187467	752162.338769	45.884916
3494.487844	750889.554313	45.889921
3493.870642	749537.943183	45.894925
3493.376015	748143.629621	45.899930
3492.550191	746690.900427	45.904935
3492.033970	745158.262909	45.909940
3491.088962	743586.781706	45.914945
3490.387737	741940.766649	45.919949
3489.505934	740243.540181	45.924954
3488.358340	738484.497336	45.929959
3488.062864	736655.050840	45.934964
3486.853076	734780.393154	45.939969
3485.677302	732847.712839	45.944973
3484.855118	730848.449323	45.949978
3483.751025	728791.577015	45.954983
3482.797141	726676.587079	45.959988
3481.777924	724512.096471	45.964993
3480.670829	722277.103250	45.969997
3479.531045	719985.924859	45.975002
3477.812200	717652.943568	45.980007
3477.239201	715248.669272	45.985012
3475.960432	712797.421689	45.990017
3474.023031	710291.809183	45.995021
3473.368527	707725.558078	46.000026
3471.814857	705108.715957	46.005031
3470.739462	702432.169597	46.010036
3469.184714	699704.179517	46.015041
3468.066753	696925.148796	46.020045
3466.671747	694084.857979	46.025050
3464.975690	691189.677069	46.030055
3463.499987	688236.835886	46.035060
3462.118447	685245.523555	46.040065
3460.426231	682186.194152	46.045069
3459.278927	679085.249930	46.050074
3457.409722	675931.703773	46.055079
3455.670563	672716.995011	46.060084
3454.220852	669464.583029	46.065089
3452.200865	666144.648317	46.070093
3450.982986	662780.708993	46.075098
3448.650434	659357.670564	46.080103
3447.097228	655904.534094	46.085108
3445.483983	652385.198680	46.090113
3443.611918	648829.375013	46.095117
3441.947125	645212.512824	46.100122
3439.812082	641552.926515	46.105127
3437.810007	637831.022531	46.110132
3436.227691	634080.132991	46.115137
3434.020934	630270.274257	46.120141
3431.854853	626413.308242	46.125146
3429.608428	622522.296798	46.130151
3427.880040	618569.504077	46.135156
3425.813113	614584.002277	46.140161
3423.767626	610535.519419	46.145165
3421.635537	606449.763380	46.150170
3419.355672	602310.811422	46.155175
3417.471949	598136.159907	46.160180
3414.785195	593916.997541	46.165185
3412.818463	589649.276601	46.170189
3410.770480	585343.704898	46.175194
3407.883356	580994.958443	46.180199
3405.494091	576596.957587	46.185204
3403.498602	572159.603376	46.190209
3400.941595	567679.915081	46.195213
3398.714902	563163.415140	46.200218
3396.129741	558604.209724	46.205223
3393.764999	553998.254000	46.210228
3391.026756	549362.308779	46.215233
3388.488938	544674.038528	46.220237
3385.876088	539956.867576	46.225242
3383.220823	535212.908704	46.230247
3381.001316	530397.516502	46.235252
3378.255699	525577.052050	46.240257
3375.422405	520712.325218	46.245261
3373.041301	515795.908767	46.250266
3369.883602	510847.798801	46.255271
3367.293509	505862.214017	46.260276
3364.741126	500857.899751	46.265281
3361.724478	495817.907643	46.270285
3359.365851	490726.266260	46.275290
3355.815542	485610.398999	46.280295
3353.091382	480450.544178	46.285300
3350.457720	475278.371712	46.290305
3347.485938	470064.343431	46.295309
3344.683937	464805.894172	46.300314
3341.807346	459535.604699	46.305319
3338.787302	454218.330431	46.310324
3335.705850	448882.964314	46.315329
3332.496586	443522.745319	46.320333
3329.596377	438116.465232	46.325338
3326.519756	432708.462427	46.330343
3323.134769	427240.932372	46.335348
3319.875669	421771.706836	46.340353
3316.905348	416277.160293	46.345357
3313.827837	410738.615807	46.350362
3310.458719	405197.014577	46.355367
3307.454258	399618.219130	46.360372
3304.182060	394021.566215	46.365377
3300.546692	388398.743398	46.370381
3297.351751	382744.436561	46.375386
3293.998359	377088.697696	46.380391
3290.764893	371393.661852	46.385396
3287.296207	365697.410678	46.390401
3283.937399	359970.578945	46.395405
3280.545369	354228.029285	46.400410
3277.006898	348476.995610	46.405415
3273.788647	342672.404571	46.410420
3269.964425	336868.084513	46.415425
3266.047098	331054.988876	46.420429
3263.014326	325219.383371	46.425434
3258.739411	319387.067659	46.430439
3255.436579	313542.678979	46.435444
3251.686860	307681.736825	46.440449
3248.080980	301814.781524	46.445453
3244.169570	295921.004335	46.450458
3240.503073	290047.470265	46.455463
3236.716992	284134.828562	46.460468
3233.019436	278242.174124	46.465473
3228.971492	272326.947710	46.470477
3225.253955	266404.926841	46.475482
3221.157223	260494.590997	46.480487
3217.273582	254561.994734	46.485492
3213.497055	248643.498564	46.490497
3209.267538	242709.270122	46.495501
3205.309566	236791.125990	46.500506
3201.471958	230875.618143	46.505511
3197.654510	224941.092051	46.510516
3193.359616	219015.642504	46.515521
3189.381441	213075.355360	46.520525
3185.816539	207076.706582	46.525530
3181.277372	201146.071743	46.530535
3177.291069	195233.874536	46.535540
3172.871844	189316.003166	46.540545
3168.433404	183412.815046	46.545549
3164.433609	177508.731785	46.550554
3160.066292	171636.112532	46.555559
3155.597602	165751.548602	46.560564
3151.030043	159889.651943	46.565569
3146.522355	154032.899753	46.570573
3142.324814	148200.675962	46.575578
3137.528785	142395.965533	46.580583
3132.877243	136591.631820	46.585588
3128.402240	130823.149775	46.590593
3123.288292	125067.366764	46.595597
3118.766214	119320.588003	46.600602
3113.751198	113623.400078	46.605607
3109.123259	107947.889109	46.610612
3104.610988	102300.074073	46.615617
3099.150711	96671.749081	46.620621
3094.636413	91068.273724	46.625626
3089.400682	85517.425749	46.630631
3084.276056	79995.531626	46.635636
3079.352611	74503.105475	46.640641
3074.178842	69044.502079	46.645645
3069.199865	63620.791665	46.650650
3063.343209	58253.846265	46.655655
3058.034208	52907.067456	46.660660
3052.475609	47630.654333	46.665665
3046.397688	42399.309460	46.670669
3040.483444	37221.922046	46.675674
3033.936342	32112.916424	46.680679
3025.546348	27123.402988	46.685684
3011.247350	22392.055068	46.690689
2995.665143	17842.807498	46.695693
2980.263187	13467.863232	46.700698
2964.842392	9348.856099	46.705703
2947.608564	5531.935766	46.710708
2919.657249	2298.230934	46.715713
2860.619833	317.862673	46.720717
2757.540344	273.805845	46.725722
2700.457965	282.891953	46.730727
2690.958317	264.585418	46.735732
2712.463623	239.460096	46.740737
2744.812384	237.921447	46.745741
2774.109963	243.707718	46.750746
2792.284768	252.156065	46.755751
2799.465509	256.210867	46.760756
2799.698510	246.811862	46.765761
2794.736120	239.399763	46.770765
2788.980135	222.098719	46.775770
2783.404540	234.817890	46.780775
2779.161187	245.249242	46.785780
2775.852352	241.954876	46.790785
2773.323391	233.988874	46.795789
2771.323937	235.451337	46.800794
2769.536700	228.517009	46.805799
2766.706512	234.352077	46.810804
2764.371382	227.493834	46.815809
2760.872212	238.487184	46.820813
2757.470147	228.172721	46.825818
2754.326131	225.705575	46.830823
2751.487674	221.698733	46.835828
2748.445559	222.335055	46.840833
2744.979367	234.089814	46.845837
2742.014018	220.115059	46.850842
2738.415135	230.820232	46.855847
2735.152167	223.821159	46.860852
2732.359211	217.322299	46.865857
2728.990139	217.804166	46.870861
2725.497540	203.359429	46.875866
2722.415486	213.316388	46.880871
2718.847743	215.675678	46.885876
2715.761682	215.323129	46.890881
2712.287070	222.730732	46.895885
2709.339432	207.508268	46.900890
2706.222037	212.535442	46.905895
2702.150277	216.461180	46.910900
2698.983512	215.464270	46.915905
2695.844443	220.260997	46.920909
2692.537289	210.529423	46.925914
2688.515221	217.445711	46.930919
2685.318188	219.354510	46.935924
2682.527789	222.414765	46.940929
2678.991397	221.050634	46.945933
2675.314304	218.521422	46.950938
2671.871673	205.911017	46.955943
2668.479217	203.880337	46.960948
2665.114526	216.055046	46.965953
2661.237373	210.767606	46.970957
2658.165385	202.992432	46.975962
2654.611486	209.465575	46.980967
2651.795335	211.529602	46.985972
2648.719748	205.465958	46.990977
2644.676806	213.228770	46.995981
2640.965831	210.838007	47.000986
2637.226703	210.763143	47.005991
2634.225602	213.141769	47.010996
2630.753623	205.194646	47.016001
2626.952056	211.353405	47.021005
2624.043938	210.239337	47.026010
2620.226673	206.181114	47.031015
2617.073756	212.692493	47.036020
2614.027513	199.818594	47.041025
2610.591330	206.359111	47.046029
2606.956029	207.839677	47.051034
2603.347701	200.975849	47.056039
2600.240492	206.653611	47.061044
2596.635144	200.736128	47.066049
2592.842950	210.423160	47.071053
2589.453692	199.850603	47.076058
2585.678538	202.574090	47.081063
2582.391955	202.025332	47.086068
2579.522719	200.651081	47.091073
2575.346294	208.441377	47.096077
2571.954670	205.332182	47.101082
2568.276890	209.903823	47.106087
2564.894858	203.067488	47.111092
2562.084368	194.357327	47.116097
2557.941149	206.219748	47.121101
2555.094436	198.748559	47.126106
2551.403214	199.145174	47.131111
2547.703136	198.242205	47.136116
2544.421602	186.990580	47.141121
2540.788423	191.798370	47.146125
2537.213668	193.338827	47.151130
2534.078650	194.346482	47.156135
2530.085327	194.710055	47.161140
2527.050207	193.195964	47.166145
2523.438990	199.581209	47.171149
2520.087976	194.841239	47.176154
2516.524225	192.616252	47.181159
2512.819235	195.005535	47.186164
2509.914473	184.576227	47.191169
2506.015104	194.189894	47.196173
2502.701987	190.175002	47.201178
2499.054758	192.129863	47.206183
2495.505849	189.159458	47.211188
2492.654013	185.936485	47.216193
2488.789822	189.039675	47.221197
2485.187061	182.180174	47.226202
2481.590880	194.290111	47.231207
2478.325014	188.177010	47.236212
2475.034065	190.429093	47.241217
2471.197693	199.792594	47.246221
2467.849531	190.923088	47.251226
2464.328211	182.027010	47.256231
2460.921691	191.713421	47.261236
2456.948596	181.103090	47.266241
2453.472327	194.794787	47.271245
2450.416262	179.833649	47.276250
2446.880529	178.855603	47.281255
2443.479540	178.774844	47.286260
2440.013252	168.812740	47.291265
2435.900236	182.770119	47.296269
2432.876969	180.330988	47.301274
2429.373469	184.212793	47.306279
2425.976242	178.182076	47.311284
2422.605714	177.620902	47.316289
2419.222350	181.134519	47.321293
2415.650695	178.553551	47.326298
2411.780106	179.572991	47.331303
2408.215154	183.079193	47.336308
2405.149741	188.902701	47.341313
2401.230757	183.992459	47.346317
2398.246817	184.500793	47.351322
2394.818170	179.813061	47.356327
2390.944669	181.927636	47.361332
2387.397833	188.617865	47.366337
2384.303438	185.438493	47.371341
2380.601413	185.249372	47.376346
2376.812956	184.424143	47.381351
2372.972837	182.581315	47.386356
2369.855932	186.671076	47.391361
2366.728878	181.286349	47.396365
2363.120706	181.555904	47.401370
2359.592231	185.909789	47.406375
2356.145805	190.210030	47.411380
2352.854940	176.146288	47.416385
2348.999734	182.122536	47.421389
2346.024052	176.798402	47.426394
2342.337157	177.248948	47.431399
2338.481981	178.165654	47.436404
2335.295878	177.902771	47.441409
2331.357270	183.652095	47.446413
2328.571732	176.979450	47.451418
2324.558061	176.176571	47.456423
2321.089841	178.136468	47.461428
2317.613186	166.512244	47.466433
2314.169132	180.930417	47.471437
2310.659983	182.400599	47.476442
2306.744759	177.374979	47.481447
2303.513128	175.138982	47.486452
2300.387052	174.077030	47.491457
2296.789722	182.511868	47.496461
2293.134559	172.437717	47.501466
2289.480477	163.423297	47.506471
2286.031628	172.699265	47.511476
2282.837857	166.474544	47.516481
2279.233058	170.474873	47.521485
2275.871016	167.280520	47.526490
2272.304798	168.566795	47.531495
2268.728110	173.241120	47.536500
2265.196996	167.216346	47.541505
2261.565268	168.401392	47.546509
2258.254260	176.139195	47.551514
2254.968672	175.826547	47.556519
2251.394798	175.242360	47.561524
2248.140763	174.831544	47.566529
2244.188980	174.724961	47.571533
2240.766054	165.724790	47.576538
2237.217641	165.237239	47.581543
2233.440385	165.465647	47.586548
2230.313242	153.278835	47.591553
2226.628459	181.970888	47.596557
2223.292768	171.830666	47.601562
2220.196271	171.337931	47.606567
2216.312899	172.892083	47.611572
2212.715197	164.242156	47.616577
2208.816363	179.348266	47.621581
2205.213033	170.467601	47.626586
2201.976028	171.838326	47.631591
2198.829595	169.705519	47.636596
2195.594001	163.849520	47.641601
2191.831869	169.127693	47.646605
2188.512555	164.757704	47.651610
2184.719319	167.082554	47.656615
2180.778631	169.223839	47.661620
2177.886884	168.068107	47.666625
2174.138921	170.169382	47.671629
2170.905599	161.845521	47.676634
2167.807015	162.277696	47.681639
2163.715651	177.292003	47.686644
2160.251232	169.527993	47.691649
2156.594192	169.512776	47.696653
2153.400209	165.677757	47.701658
2149.959833	169.276604	47.706663
2146.390516	167.306248	47.711668
2142.707764	167.006006	47.716673
2138.979374	174.925324	47.721677
2135.563823	167.548114	47.726682
2132.268198	167.937576	47.731687
2128.760401	167.531006	47.736692
2125.292536	167.029417	47.741697
2121.446892	170.035925	47.746701
2117.900491	162.548591	47.751706
2115.062684	165.175801	47.756711
2111.641249	168.717470	47.761716
2108.227682	165.201058	47.766721
2104.353840	171.334523	47.771725
2100.807628	166.037418	47.776730
2097.010891	162.595352	47.781735
2093.467415	162.782394	47.786740
2090.615804	161.754066	47.791745
2087.050083	163.662026	47.796749
2083.422856	158.767511	47.801754
2079.735212	165.792303	47.806759
2075.946731	165.972196	47.811764
2072.802514	158.220145	47.816769
2068.783303	160.538728	47.821773
2065.732036	162.936906	47.826778
2062.496461	153.699649	47.831783
2058.832166	161.776340	47.836788
2055.453388	156.440686	47.841793
2051.628104	162.934577	47.846797
2048.347300	156.176669	47.851802
2044.701854	163.551874	47.856807
2041.043224	156.185431	47.861812
2038.146052	159.317448	47.866817
2034.084419	159.703270	47.871821
2030.648112	156.691735	47.876826
2027.366892	159.492324	47.881831
2023.445093	160.335503	47.886836
2020.276678	156.061625	47.891841
2016.658480	160.518263	47.896845
2013.313489	155.450754	47.901850
2009.867801	156.330696	47.906855
2006.513197	163.086252	47.911860
2003.239538	163.178934	47.916865
1999.355694	164.183781	47.921869
1995.614528	155.251178	47.926874
1992.219325	155.208114	47.931879
1988.552613	160.774545	47.936884
1985.582298	161.652107	47.941889
1981.613140	151.627348	47.946893
1977.850916	160.890736	47.951898
1975.003264	150.346254	47.956903
1970.988663	162.107520	47.961908
1967.805020	160.624775	47.966913
1964.251589	159.431233	47.971917
1960.833267	154.806312	47.976922
1957.414164	156.245881	47.981927
1953.441879	161.671167	47.986932
1950.317623	153.672401	47.991937
1946.817164	158.863018	47.996941
1943.160456	150.073754	48.001946
1939.884936	152.881950	48.006951
1936.062090	149.110081	48.011956
1932.914906	155.029735	48.016961
1929.173330	161.221156	48.021965
1925.916473	145.345198	48.026970
1922.188460	153.147206	48.031975
1918.562573	154.774404	48.036980
1915.258858	152.962117	48.041985
1911.567764	159.524072	48.046989
1908.217680	153.155866	48.051994
1904.868466	142.947156	48.056999
1901.138342	154.329808	48.062004
1898.035610	150.310959	48.067009
1894.235174	156.147879	48.072013
1890.753379	159.481865	48.077018
1887.620201	161.309233	48.082023
1883.789188	152.937074	48.087028
1880.159262	156.801193	48.092033
1876.528596	152.985099	48.097037
1873.010004	154.357554	48.102042
1869.990095	148.362885	48.107047
1865.805335	156.772065	48.112052
1862.767552	156.862078	48.117057
1858.960877	144.408942	48.122061
1855.666482	151.617185	48.127066
1852.100625	152.799168	48.132071
1848.283568	155.776319	48.137076
1845.589877	152.053214	48.142081
1841.651558	155.106709	48.147085
1838.165607	149.266859	48.152090
1834.925449	157.739147	48.157095
1831.524680	160.653042	48.162100
1827.883754	146.445378	48.167105
1823.824087	156.094646	48.172109
1820.918237	165.806265	48.177114
1816.935659	145.574510	48.182119
1813.411497	145.925145	48.187124
1810.179297	146.472483	48.192129
1806.219889	148.101777	48.197133
1803.051317	147.599797	48.202138
1799.968808	147.189918	48.207143
1796.587733	153.585930	48.212148
1793.288498	151.248481	48.217153
1789.209889	144.530490	48.222157
1785.395267	151.170447	48.227162
1781.904704	148.628510	48.232167
1778.280613	148.940484	48.237172
1775.042067	147.051996	48.242177
1771.747945	142.040603	48.247181
1768.240113	142.458032	48.252186
1764.911327	146.195765	48.257191
1760.785175	144.723779	48.262196
1757.454171	137.183730	48.267201
1753.680251	144.793188	48.272205
1750.737972	140.995521	48.277210
1747.627953	144.678258	48.282215
1743.740465	150.778380	48.287220
1740.363769	145.821155	48.292225
1736.432421	143.869542	48.297229
1733.167671	148.284402	48.302234
1730.060245	144.820786	48.307239
1726.086348	151.954884	48.312244
1722.542664	144.984110	48.317249
1718.865982	147.897062	48.322253
1715.063894	146.400215	48.327258
1712.106399	144.622072	48.332263
1708.598727	153.248315	48.337268
1705.273881	142.823814	48.342273
1701.845086	146.707628	48.347277
1698.203697	148.497431	48.352282
1694.742310	145.953103	48.357287
1690.695021	141.151292	48.362292
1687.557521	144.753972	48.367297
1683.993283	134.760104	48.372301
1680.844925	150.110619	48.377306
1677.323736	140.128562	48.382311
1673.408879	139.606543	48.387316
1670.004344	142.718723	48.392321
1666.691343	143.802511	48.397325
1663.205081	144.576790	48.402330
1659.524769	143.938349	48.407335
1655.441234	146.217473	48.412340
1652.345706	139.316330	48.417345
1648.871076	146.185387	48.422349
1645.692318	142.560208	48.427354
1642.635362	134.109711	48.432359
1638.833613	145.838924	48.437364
1635.275583	144.053642	48.442369
1631.227162	149.785479	48.447373
1627.726339	137.574343	48.452378
1624.590738	140.750903	48.457383
1620.869620	150.280088	48.462388
1617.810094	151.154946	48.467393
1613.800318	134.514740	48.472397
1610.393379	139.695642	48.477402
1607.178099	145.229381	48.482407
1603.565779	148.429939	48.487412
1600.023023	142.202691	48.492417
1596.388166	141.698262	48.497421
1593.205788	148.295525	48.502426
1590.078867	138.418487	48.507431
1586.070369	139.715531	48.512436
1582.423615	132.553007	48.517441
1579.221611	140.202173	48.522445
1575.468264	144.841231	48.527450
1572.050082	138.932380	48.532455
1568.325753	146.897267	48.537460
1564.930809	131.208361	48.542465
1561.377714	143.121371	48.547469
1557.724537	138.345920	48.552474
1554.673073	137.041297	48.557479
1550.501803	150.471518	48.562484
1547.364749	143.810795	48.567489
1543.505466	147.903857	48.572493
1540.449607	139.519963	48.577498
1537.619603	133.172228	48.582503
1533.233638	142.438361	48.587508
1529.859512	135.249035	48.592513
1526.610273	145.851505	48.597517
1522.710420	149.357925	48.602522
1519.510611	131.549884	48.607527
1515.888231	140.694945	48.612532
1512.494908	139.072892	48.617537
1508.968093	139.353981	48.622541
1505.280172	141.975349	48.627546
1501.995282	140.877998	48.632551
1498.320200	145.653136	48.637556
1494.964378	136.168161	48.642561
1491.583535	138.185490	48.647565
1487.824414	136.441779	48.652570
1484.572022	141.043234	48.657575
1480.833054	143.221981	48.662580
1477.672384	134.463614	48.667585
1473.996781	135.743849	48.672589
1470.368633	127.017825	48.677594
1467.267771	129.251792	48.682599
1463.306440	139.205543	48.687604
1459.574616	139.845683	48.692609
1456.465809	135.873790	48.697613
1452.728894	141.383047	48.702618
1449.442432	134.128543	48.707623
1445.744560	138.852251	48.712628
1442.395649	135.644803	48.717633
1438.900555	137.536081	48.722637
1435.192210	141.462129	48.727642
1431.877495	128.214714	48.732647
1428.293736	134.132531	48.737652
1424.902949	138.494132	48.742657
1421.595751	138.304739	48.747661
1417.958431	134.608193	48.752666
1414.281593	134.692836	48.757671
1410.532530	142.217755	48.762676
1407.001963	129.059639	48.767681
1404.074404	132.303685	48.772685
1400.043597	138.185950	48.777690
1396.935480	131.103989	48.782695
1393.632531	139.668103	48.787700
1390.060176	130.506265	48.792705
1386.499965	137.996922	48.797709
1383.067971	137.068123	48.802714
1379.348731	125.107385	48.807719
1375.462056	129.453192	48.812724
1372.129571	124.917190	48.817729
1368.655109	124.264416	48.822733
1365.116292	135.644568	48.827738
1361.883184	127.022250	48.832743
1358.116475	132.990992	48.837748
1355.163249	138.334834	48.842753
1351.378761	131.043832	48.847757
1347.878052	128.105355	48.852762
1344.271116	131.427986	48.857767
1340.953418	134.021051	48.862772
1337.563448	137.788609	48.867777
1334.016272	134.106793	48.872781
1329.962290	134.100936	48.877786
1326.411839	127.801824	48.882791
1322.904757	138.878771	48.887796
1319.679236	130.620696	48.892801
1316.373825	137.822479	48.897805
1312.626813	130.362894	48.902810
1309.671485	111.535754	48.907815
1305.738069	125.490509	48.912820
1302.254604	130.609757	48.917825
1298.950025	123.598557	48.922829
1294.947350	135.093198	48.927834
1291.824294	137.879178	48.932839
1288.261921	133.490111	48.937844
1285.051106	137.452364	48.942849
1281.343027	125.670244	48.947853
1277.474568	138.140365	48.952858
1274.293527	136.468903	48.957863
1270.305654	134.416630	48.962868
1267.295931	129.954461	48.967873
1264.034829	130.782709	48.972877
1260.130054	133.593600	48.977882
1256.623821	123.786303	48.982887
1253.003298	127.228287	48.987892
1249.804278	128.760798	48.992897
1246.368913	131.113570	48.997901
1242.976438	132.379018	49.002906
1239.610680	126.808303	49.007911
1235.435821	131.381426	49.012916
1232.242966	128.956759	49.017921
1228.452727	131.024658	49.022925
1224.943027	131.357822	49.027930
1221.369490	121.532127	49.032935
1218.277587	125.315453	49.037940
1214.733558	129.220359	49.042945
1210.842154	124.827147	49.047949
1207.289338	123.850073	49.052954
1204.561377	122.788851	49.057959
1200.502766	137.379962	49.062964
1197.220667	127.877520	49.067969
1193.978553	128.819104	49.072973
1190.245408	136.254349	49.077978
1186.707689	123.319656	49.082983
1183.304239	130.306920	49.087988
1179.893338	131.230341	49.092993
1176.167984	125.376572	49.097997
1172.431276	123.816130	49.103002
1169.329627	124.915188	49.108007
1165.496887	129.075236	49.113012
1161.984619	121.908981	49.118017
1158.484904	124.132789	49.123021
1155.341046	120.884278	49.128026
1151.827663	115.872128	49.133031
1148.197884	127.957417	49.138036
1144.836127	127.563399	49.143041
1141.196629	127.575797	49.148045
1137.302466	123.608377	49.153050
1133.734928	117.171790	49.158055
1130.314303	121.646323	49.163060
1126.900460	114.175865	49.168065
1123.659958	122.898927	49.173069
1120.200554	127.413845	49.178074
1116.706265	127.968129	49.183079
1113.026144	128.341904	49.188084
1109.423141	120.349913	49.193089
1106.178143	116.510830	49.198093
1102.423493	122.420964	49.203098
1099.279384	125.235053	49.208103
1095.491426	138.907948	49.213108
1092.169822	131.676574	49.218113
1089.115228	122.038809	49.223117
1084.804915	124.992342	49.228122
1081.286236	127.068602	49.233127
1077.633497	123.315352	49.238132
1074.641423	134.183898	49.243137
1071.127129	125.178908	49.248141
1067.656489	127.532752	49.253146
1064.255789	126.169644	49.258151
1060.191148	128.861819	49.263156
1057.000508	134.439637	49.268161
1053.766404	121.657170	49.273165
1049.984788	123.735647	49.278170
1046.637650	122.413198	49.283175
1042.852439	134.347753	49.288180
1039.794620	123.253646	49.293185
1035.860038	127.573388	49.298189
1032.153541	135.498870	49.303194
1029.165418	125.070853	49.308199
1025.461326	127.716652	49.313204
1022.099266	132.913670	49.318209
1018.710703	125.736300	49.323213
1014.860212	127.570101	49.328218
1011.428934	129.081750	49.333223
1007.525050	130.427136	49.338228
1004.277284	127.746754	49.343233
1001.039696	122.752718	49.348237
997.353786	129.030622	49.353242
994.166984	127.295033	49.358247
990.740378	123.942819	49.363252
987.206659	125.530690	49.368257
983.565932	134.479331	49.373261
979.637279	140.386491	49.378266
976.507913	128.744868	49.383271
972.856137	136.130492	49.388276
969.377753	131.211765	49.393281
965.780256	130.478933	49.398285
962.104111	125.966391	49.403290
959.203453	116.380554	49.408295
955.660038	132.170825	49.413300
952.055234	141.486694	49.418305
948.453268	131.195348	49.423309
945.072248	124.692076	49.428314
941.318590	129.215132	49.433319
937.980196	134.228717	49.438324
934.541009	129.428826	49.443329
930.776919	126.005002	49.448333
926.785409	128.227559	49.453338
924.123675	129.489021	49.458343
920.480499	127.254996	49.463348
916.936033	125.738674	49.468353
913.253677	133.467852	49.473357
909.698254	127.413682	49.478362
906.593893	128.753948	49.483367
902.982317	129.936469	49.488372
899.057984	128.164714	49.493377
896.076648	130.146429	49.498381
892.410065	127.324313	49.503386
889.197015	117.651659	49.508391
885.385009	125.675487	49.513396
881.803275	129.351916	49.518401
878.383397	129.876895	49.523405
874.768343	126.450690	49.528410
871.497365	125.561137	49.533415
868.081952	120.428016	49.538420
864.638080	126.244358	49.543425
860.951069	118.762071	49.548429
856.863645	124.536251	49.553434
853.587873	124.994709	49.558439
849.826482	128.938971	49.563444
846.902721	126.023202	49.568449
843.678810	123.316309	49.573453
839.845350	134.036168	49.578458
836.566089	118.751322	49.583463
832.667407	124.827888	49.588468
829.054275	126.497559	49.593473
825.927280	127.853289	49.598477
822.314548	123.028245	49.603482
818.770301	122.256323	49.608487
815.235469	128.674282	49.613492
811.872614	125.663103	49.618497
808.443863	128.856783	49.623501
804.527161	132.367477	49.628506
801.328980	123.795925	49.633511
797.629642	136.529650	49.638516
794.337853	129.068845	49.643521
790.998055	127.679296	49.648525
787.210904	131.123312	49.653530
784.008548	133.529760	49.658535
780.079503	134.103238	49.663540
776.773169	126.714327	49.668545
773.384477	120.642287	49.673549
769.660215	130.150208	49.678554
766.477969	129.533334	49.683559
762.696397	126.289000	49.688564
759.163806	119.954926	49.693569
755.570729	122.257736	49.698573
752.233549	124.763157	49.703578
748.957131	115.526609	49.708583
745.433940	128.102861	49.713588
741.635221	124.896126	49.718593
738.224130	126.361053	49.723597
734.282456	127.734298	49.728602
731.066861	124.234419	49.733607
727.780534	131.577147	49.738612
724.346704	123.947592	49.743617
721.004281	123.429770	49.748621
716.865887	129.082709	49.753626
713.626942	120.702319	49.758631
710.200183	126.524040	49.763636
706.596308	120.566722	49.768641
703.142478	120.615211	49.773645
699.672080	123.091290	49.778650
696.661182	118.062458	49.783655
692.772273	122.713773	49.788660
688.900149	124.199838	49.793665
685.691722	122.337073	49.798669
681.866919	115.073608	49.803674
678.512823	119.682910	49.808679
675.257832	131.084955	49.813684
671.522202	130.191619	49.818689
667.959571	114.277935	49.823693
664.030067	126.559802	49.828698
661.819067	111.020026	49.833703
657.785523	120.622805	49.838708
654.005669	121.396208	49.843713
650.871919	122.176789	49.848717
647.359234	119.104208	49.853722
643.840722	119.837187	49.858727
640.254510	121.752782	49.863732
636.127646	127.270689	49.868737
632.826463	119.585852	49.873741
629.182682	121.525816	49.878746
626.046584	118.365270	49.883751
623.034820	117.703239	49.888756
619.418287	120.034737	49.893761
615.797794	121.426404	49.898765
611.909451	123.307143	49.903770
608.525657	121.568680	49.908775
604.888220	114.668657	49.913780
601.360487	123.301475	49.918785
598.456501	116.611977	49.923789
594.352595	124.597319	49.928794
591.306412	117.604654	49.933799
587.762991	120.128675	49.938804
584.239135	126.138700	49.943809
580.817894	119.762437	49.948813
576.770916	123.552114	49.953818
573.439920	117.389582	49.958823
570.117265	118.080634	49.963828
566.417132	123.409349	49.968833
563.451987	111.380135	49.973837
559.397001	127.116533	49.978842
555.992696	118.421972	49.983847
552.573180	116.528864	49.988852
548.985163	119.227270	49.993857
545.867309	121.392551	49.998861
541.867233	123.784854	50.003866
538.621508	122.454107	50.008871
534.849094	118.289509	50.013876
531.169679	123.173776	50.018881
528.044702	111.940737	50.023885
524.270423	118.483365	50.028890
520.985872	114.787729	50.033895
517.926598	110.679752	50.038900
513.886669	120.276430	50.043905
510.818839	113.941395	50.048909
506.912026	119.977000	50.053914
503.305087	111.761924	50.058919
499.987821	120.106694	50.063924
496.453673	124.227263	50.068929
493.162335	120.722613	50.073933
489.158557	123.681538	50.078938
486.174930	119.078148	50.083943
482.702962	125.376828	50.088948
479.204864	115.782297	50.093953
475.901305	117.675372	50.098957
471.743140	115.191067	50.103962
468.254354	108.323530	50.108967
464.624077	118.113090	50.113972
460.999828	118.243977	50.118977
458.177197	114.081553	50.123981
454.397311	119.095056	50.128986
451.184248	123.945355	50.133991
447.678800	112.040717	50.138996
443.783120	122.751919	50.144001
440.524551	113.242162	50.149005
436.786292	122.398880	50.154010
433.418419	111.978243	50.159015
430.192948	113.158645	50.164020
426.468983	120.053140	50.169025
422.665792	110.503229	50.174029
419.244401	112.409216	50.179034
416.160442	103.759669	50.184039
412.613546	112.660448	50.189044
408.703544	111.841135	50.194049
405.183451	113.831411	50.199053
401.834803	119.417233	50.204058
398.528568	113.040795	50.209063
395.345863	113.821826	50.214068
391.435246	122.053504	50.219073
388.047245	112.895831	50.224077
383.751561	117.525429	50.229082
380.962232	114.938368	50.234087
377.532926	111.520286	50.239092
373.680062	116.274459	50.244097
370.333714	112.579558	50.249101
366.646371	119.579518	50.254106
363.227407	115.172474	50.259111
359.987931	113.311602	50.264116
356.431925	117.596950	50.269121
353.097779	102.167425	50.274125
349.335150	114.943203	50.279130
346.022237	113.814412	50.284135
342.367228	105.748588	50.289140
338.340565	120.839145	50.294145
335.103183	105.472495	50.299149
331.707065	118.463869	50.304154
328.391022	108.506553	50.309159
324.801025	113.747929	50.314164
321.247683	113.980837	50.319169
317.913950	102.485898	50.324173
314.035308	115.514621	50.329178
310.786235	115.837492	50.334183
307.608401	109.142037	50.339188
303.813968	113.201037	50.344193
300.593743	107.875806	50.349197
296.823212	111.802181	50.354202
293.069170	111.354311	50.359207
289.845477	119.431907	50.364212
286.106843	114.432373	50.369217
282.989475	106.906388	50.374221
279.136734	107.648861	50.379226
275.983848	107.727468	50.384231
272.548391	109.450628	50.389236
268.740269	114.307188	50.394241
265.303775	109.661618	50.399245
261.664445	113.731989	50.404250
258.001238	102.738612	50.409255
254.701666	97.031748	50.414260
251.408578	104.795889	50.419265
247.756928	94.065233	50.424269
244.074247	101.032949	50.429274
240.958913	100.706539	50.434279
237.347860	103.672302	50.439284
233.583446	110.839105	50.444289
230.526675	104.613388	50.449293
226.520718	111.664043	50.454298
223.065514	108.821099	50.459303
219.430649	109.887565	50.464308
216.015472	107.719563	50.469313
212.673435	107.120834	50.474317
208.989341	113.376059	50.479322
205.792002	103.916157	50.484327
202.388726	114.197668	50.489332
198.769482	115.934660	50.494337
195.545561	108.016008	50.499341
191.769732	110.204473	50.504346
188.354426	98.834914	50.509351
184.791302	101.873077	50.514356
180.935738	99.694420	50.519361
177.763338	97.223466	50.524365
174.174399	99.573292	50.529370
170.544004	107.280083	50.534375
166.772238	108.788680	50.539380
163.530873	114.147307	50.544385
160.158389	99.359575	50.549389
156.539883	100.377800	50.554394
153.048847	109.205977	50.559399
150.229012	108.654716	50.564404
146.045196	104.240009	50.569409
142.701727	102.296369	50.574413
138.873093	114.478279	50.579418
135.454100	106.949667	50.584423
132.373821	103.680628	50.589428
128.308650	109.775280	50.594433
124.628722	103.845810	50.599437
121.363524	111.521362	50.604442
118.082291	102.341097	50.609447
115.266382	107.272085	50.614452
111.329430	108.345248	50.619457
108.164178	102.127606	50.624461
104.294423	109.375774	50.629466
100.465408	102.343945	50.634471
96.785923	108.327964	50.639476
93.559509	110.796010	50.644481
90.683873	109.976027	50.649485
86.590434	100.632407	50.654490
82.958881	97.101804	50.659495
79.530323	98.739141	50.664500
75.767439	109.666789	50.669505
72.681905	111.208053	50.674509
69.025884	106.843458	50.679514
65.759521	105.116769	50.684519
62.098997	102.367897	50.689524
58.384193	111.027726	50.694529
55.154712	101.989882	50.699533
51.495174	104.167842	50.704538
47.853879	98.319257	50.709543
44.667939	97.759464	50.714548
41.119567	97.708249	50.719553
37.829538	104.850855	50.724557
34.209911	106.563600	50.729562
30.627177	101.388856	50.734567
26.817730	100.784907	50.739572
23.230167	105.721078	50.744577
20.121281	93.923276	50.749581
16.486891	105.797137	50.754586
12.976484	105.675901	50.759591
9.220963	104.487981	50.764596
5.991169	105.336765	50.769601
2.986401	99.534967	50.774605