Fri Jun 17 17:26:42 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.900056	117.476885	0.000000
1.157187	119.245037	0.005005
0.923376	104.521504	0.010010
0.739182	86.822863	0.015014
0.560943	88.533729	0.020019
0.132816	78.790799	0.025024
0.125607	65.121472	0.030029
-0.256770	70.083355	0.035034
-0.396224	52.643910	0.040038
-0.696143	50.234603	0.045043
-0.943040	50.871361	0.050048
-1.390548	34.080264	0.055053
-1.721757	31.162115	0.060058
-1.517724	25.841696	0.065062
-2.347517	17.706718	0.070067
-2.609106	15.050501	0.075072
-2.527205	6.291386	0.080077
-3.284205	19.172422	0.085082
-3.575302	12.348954	0.090086
-3.859005	21.477823	0.095091
-4.237676	12.211753	0.100096
-4.429876	19.430647	0.105101
-4.372163	25.276615	0.110106
-4.493955	24.530801	0.115110
-4.680289	26.375415	0.120115
-5.052678	12.706056	0.125120
-5.860521	16.064491	0.130125
-6.167680	18.250441	0.135130
-6.098097	22.403117	0.140134
-6.291123	27.043635	0.145139
-6.013431	20.962106	0.150144
-6.395943	25.509998	0.155149
-7.148717	28.499154	0.160154
-7.099312	12.111315	0.165158
-7.653616	25.860662	0.170163
-7.771898	22.675655	0.175168
-7.465189	21.821322	0.180173
-8.207599	26.365100	0.185178
-8.712331	18.999948	0.190182
-9.012833	21.009958	0.195187
-9.006803	21.145289	0.200192
-8.916888	14.296181	0.205197
-9.116939	17.125779	0.210202
-9.435612	15.044007	0.215206
-10.222262	23.700794	0.220211
-10.517649	27.229004	0.225216
-10.532157	18.231549	0.230221
-10.718685	17.825839	0.235226
-10.320978	18.686770	0.240230
-11.461412	17.128751	0.245235
-11.858562	30.138237	0.250240
-11.999778	10.275128	0.255245
-12.045324	22.749020	0.260250
-11.959470	13.744753	0.265254
-12.436977	18.814191	0.270259
-12.486669	28.626199	0.275264
-13.144701	18.441616	0.280269
-13.950681	31.495575	0.285274
-13.713575	30.347540	0.290278
-13.891866	22.577470	0.295283
-13.933544	33.024342	0.300288
-13.633150	20.319588	0.305293
-14.260186	26.427766	0.310298
-14.575673	20.810487	0.315302
-15.411070	26.057814	0.320307
-15.311129	26.054599	0.325312
-15.203299	16.973073	0.330317
-15.569666	33.186233	0.335322
-15.763069	19.567236	0.340326
-16.443311	34.109086	0.345331
-17.189663	24.561758	0.350336
-16.895163	15.346198	0.355341
-17.230740	32.509910	0.360346
-17.089420	22.517462	0.365350
-17.467572	22.413355	0.370355
-17.449096	23.175510	0.375360
-17.525970	26.898868	0.380365
-18.603249	23.639231	0.385370
-18.670736	16.334799	0.390374
-18.748990	25.024007	0.395379
-18.813570	28.327375	0.400384
-18.869916	28.419007	0.405389
-19.812050	29.955518	0.410394
-20.016641	30.100404	0.415398
-20.098736	25.125514	0.420403
-20.346347	36.788233	0.425408
-19.940466	23.951688	0.430413
-20.163019	34.382844	0.435418
-20.881062	27.647309	0.440422
-21.565410	28.956073	0.445427
-21.745172	24.706822	0.450432
-21.817893	28.207493	0.455437
-22.005793	23.510667	0.460442
-22.100948	21.715167	0.465446
-22.600171	28.106583	0.470451
-23.168434	24.752077	0.475456
-23.206469	19.142948	0.480461
-23.479359	33.339245	0.485466
-23.434072	18.074109	0.490470
-23.644191	19.573796	0.495475
-23.622694	18.953545	0.500480
-24.250897	17.303875	0.505485
-24.595663	20.621649	0.510490
-24.578853	12.408118	0.515494
-24.929306	21.469741	0.520499
-24.925611	18.114687	0.525504
-25.741389	21.823129	0.530509
-26.188272	23.033222	0.535514
-26.294723	15.037508	0.540518
-26.816696	16.310205	0.545523
-26.806899	13.612234	0.550528
-26.645157	23.771519	0.555533
-27.138880	26.961322	0.560538
-26.371527	14.538294	0.565542
-27.385044	28.150265	0.570547
-27.872762	25.118229	0.575552
-27.898002	23.122657	0.580557
-28.565032	25.386977	0.585562
-28.340264	21.181582	0.590566
-28.399794	14.602794	0.595571
-29.182646	18.595641	0.600576
-29.076325	10.191410	0.605581
-29.858641	26.793772	0.610586
-29.655818	17.505638	0.615590
-29.979379	20.972425	0.620595
-30.090573	25.597762	0.625600
-30.473270	10.064563	0.630605
-31.280482	24.790110	0.635610
-31.409933	15.556222	0.640614
-31.493348	15.782591	0.645619
-31.852443	25.502566	0.650624
-31.334619	21.885244	0.655629
-31.651042	28.914633	0.660634
-32.180046	22.977455	0.665638
-32.648386	29.256193	0.670643
-32.657428	27.951742	0.675648
-32.612392	22.008142	0.680653
-33.011599	26.070615	0.685658
-33.592193	31.551460	0.690662
-34.229131	30.096626	0.695667
-34.291404	30.553318	0.700672
-34.216544	25.733489	0.705677
-34.555680	31.092503	0.710682
-34.594300	28.929648	0.715686
-34.772388	28.871220	0.720691
-35.417155	34.814620	0.725696
-35.693982	21.148320	0.730701
-35.951474	30.568833	0.735706
-35.980706	16.418177	0.740710
-36.512186	19.364435	0.745715
-36.613564	32.438814	0.750720
-36.317063	22.058274	0.755725
-37.094110	24.977668	0.760730
-37.676769	17.639684	0.765734
-37.779211	23.384598	0.770739
-38.057242	23.047379	0.775744
-37.944923	27.585441	0.780749
-38.382739	27.243407	0.785754
-37.697650	24.402993	0.790758
-38.762087	23.922600	0.795763
-39.113589	30.784565	0.800768
-38.953670	22.606637	0.805773
-39.476064	30.006317	0.810778
-40.063523	23.565207	0.815782
-40.530521	18.581092	0.820787
-40.459482	25.296648	0.825792
-40.842928	27.544812	0.830797
-40.962331	22.579876	0.835802
-40.880758	29.623619	0.840806
-41.103538	19.998151	0.845811
-41.195800	22.139306	0.850816
-41.459253	16.650527	0.855821
-42.167212	15.214606	0.860826
-42.182197	24.513306	0.865830
-42.621862	25.073971	0.870835
-42.728748	24.780527	0.875840
-43.542449	19.404723	0.880845
-43.921499	21.070031	0.885850
-43.748309	19.927687	0.890854
-43.661581	28.100288	0.895859
-44.174284	31.378889	0.900864
-43.681916	21.558769	0.905869
-43.992044	29.945140	0.910874
-44.436827	14.312940	0.915878
-45.341651	21.497754	0.920883
-45.728879	16.078095	0.925888
-45.730638	29.291407	0.930893
-45.918160	25.979188	0.935898
-45.528032	16.478969	0.940902
-46.598140	26.581161	0.945907
-47.054539	26.324899	0.950912
-46.732597	18.251266	0.955917
-47.291778	26.173473	0.960922
-47.534341	22.262430	0.965926
-47.328916	18.262909	0.970931
-47.584985	18.208959	0.975936
-47.795679	20.625539	0.980941
-48.582653	27.489049	0.985946
-48.696077	20.499497	0.990950
-48.817012	29.681824	0.995955
-48.883147	18.751618	1.000960
-48.866128	10.538844	1.005965
-49.441018	29.817652	1.010970
-50.093615	17.368995	1.015974
-50.340690	31.478908	1.020979
-50.471158	27.960664	1.025984
-50.778741	17.178140	1.030989
-50.769207	27.332928	1.035994
-50.808698	21.065748	1.040998
-51.500358	27.570256	1.046003
-52.109399	20.360188	1.051008
-51.886570	27.349270	1.056013
-52.237711	31.149595	1.061018
-52.272901	17.408208	1.066022
-52.735585	18.075116	1.071027
-52.494167	20.850669	1.076032
-52.817400	18.137611	1.081037
-53.376848	20.746350	1.086042
-53.381343	14.470000	1.091046
-53.597690	20.353626	1.096051
-54.091136	21.008085	1.101056
-54.573159	21.283547	1.106061
-55.307553	32.520039	1.111066
-55.272248	17.359179	1.116070
-55.117821	23.867882	1.121075
-55.652267	22.457781	1.126080
-55.449175	14.632809	1.131085
-55.825283	24.657921	1.136090
-55.707131	14.271711	1.141094
-55.732055	24.258574	1.146099
-56.612985	23.753010	1.151104
-56.492287	10.786285	1.156109
-56.971974	13.281521	1.161114
-57.212132	15.647549	1.166118
-58.180461	19.514947	1.171123
-58.500812	22.991266	1.176128
-58.105365	18.163338	1.181133
-58.739610	22.990269	1.186138
-58.489083	20.892618	1.191142
-58.683745	21.076900	1.196147
-58.717440	25.511164	1.201152
-58.827084	21.748520	1.206157
-59.647748	26.720497	1.211162
-60.089885	18.961538	1.216166
-60.070861	26.551230	1.221171
-60.253149	22.679303	1.226176
-60.153982	28.917775	1.231181
-60.752117	30.459469	1.236186
-61.025327	24.153589	1.241190
-61.506396	22.055405	1.246195
-62.042851	27.232129	1.251200
-61.796330	19.380795	1.256205
-62.003428	22.125136	1.261210
-61.827860	16.393283	1.266214
-63.120750	13.873776	1.271219
-63.328903	11.833232	1.276224
-63.354189	20.452851	1.281229
-63.482171	21.167918	1.286234
-63.071115	19.178754	1.291238
-63.156396	20.341173	1.296243
-64.377033	28.756356	1.301248
-64.485317	24.535087	1.306253
-64.690754	27.004075	1.311258
-64.827160	23.557070	1.316262
-64.988646	18.832377	1.321267
-65.224160	33.660822	1.326272
-65.778154	19.125387	1.331277
-66.285689	24.574749	1.336282
-66.323838	12.767895	1.341286
-66.615079	18.785526	1.346291
-66.840118	23.175625	1.351296
-66.240843	18.611585	1.356301
-66.733772	28.119578	1.361306
-68.046325	26.389503	1.366310
-68.091035	27.079479	1.371315
-68.156363	28.669552	1.376320
-67.998365	18.893374	1.381325
-68.569156	24.712393	1.386330
-68.505719	28.557070	1.391334
-68.225208	23.160991	1.396339
-68.823954	34.613311	1.401344
-69.479068	17.790460	1.406349
-69.411809	30.852982	1.411354
-69.637162	20.075734	1.416358
-69.828330	28.716223	1.421363
-70.145326	32.252173	1.426368
-70.745765	30.313936	1.431373
-71.027897	25.734997	1.436378
-70.916730	22.084435	1.441382
-70.896074	17.301444	1.446387
-72.025468	28.699302	1.451392
-72.152301	25.128360	1.456397
-72.585062	22.053847	1.461402
-72.749411	32.216229	1.466406
-72.765242	20.445718	1.471411
-72.913903	28.871550	1.476416
-72.867549	19.319943	1.481421
-72.920243	29.233675	1.486426
-73.480451	27.665653	1.491430
-73.901345	23.221076	1.496435
-74.868641	20.877929	1.501440
-74.252407	21.870257	1.506445
-74.679694	28.072317	1.511450
-74.586027	23.152278	1.516454
-75.190588	25.567440	1.521459
-76.117689	22.048824	1.526464
-75.890466	18.180851	1.531469
-75.966643	17.373783	1.536474
-76.225644	20.869898	1.541478
-76.440872	12.649163	1.546483
-76.396129	32.360719	1.551488
-76.254424	10.534912	1.556493
-77.209439	24.093355	1.561498
-77.502124	24.662940	1.566502
-77.485554	24.153420	1.571507
-78.242217	22.341005	1.576512
-77.786006	18.299992	1.581517
-78.373313	15.345693	1.586522
-79.015563	29.222931	1.591526
-79.193583	24.024631	1.596531
-79.670296	21.473839	1.601536
-79.325666	25.870864	1.606541
-79.392262	24.918744	1.611546
-79.514064	29.699367	1.616550
-79.801043	12.051661	1.621555
-80.712185	26.220850	1.626560
-80.799129	11.716515	1.631565
-81.287938	22.709518	1.636570
-81.219359	27.057123	1.641574
-81.142835	26.711287	1.646579
-81.620827	24.829065	1.651584
-81.756440	19.883206	1.656589
-82.872362	22.476121	1.661594
-82.851154	25.794432	1.666598
-82.522453	28.771354	1.671603
-82.505371	27.166368	1.676608
-82.858189	19.874841	1.681613
-82.995874	30.522957	1.686618
-83.611858	14.848584	1.691622
-83.744725	25.861549	1.696627
-84.232574	30.941003	1.701632
-83.945918	25.455300	1.706637
-84.505554	20.840998	1.711642
-85.222255	34.204140	1.716646
-85.470548	25.648895	1.721651
-85.909330	33.346660	1.726656
-85.645973	28.672700	1.731661
-85.755618	35.475715	1.736666
-85.751009	27.542445	1.741670
-86.500866	28.247032	1.746675
-87.213602	24.758296	1.751680
-87.126497	21.469297	1.756685
-87.449904	34.449555	1.761690
-87.107066	34.192842	1.766694
-87.422276	34.752755	1.771699
-87.813675	29.735555	1.776704
-87.732719	29.376551	1.781709
-88.492415	35.742603	1.786714
-88.780541	37.417074	1.791718
-88.557603	29.159406	1.796723
-88.956520	32.982673	1.801728
-89.578664	35.934737	1.806733
-89.915538	36.438855	1.811738
-90.545423	30.370261	1.816742
-90.264828	21.598636	1.821747
-90.796685	29.527751	1.826752
-90.323920	28.130577	1.831757
-90.616162	23.914238	1.836762
-90.801575	19.080061	1.841766
-91.444988	25.213070	1.846771
-91.880475	17.722961	1.851776
-91.902954	14.752319	1.856781
-92.015142	17.432931	1.861786
-92.140014	19.215038	1.866790
-93.078743	25.793577	1.871795
-93.627558	39.314502	1.876800
-93.444973	30.883774	1.881805
-93.383559	22.134377	1.886810
-93.306790	23.005436	1.891814
-93.430320	20.202353	1.896819
-94.140985	27.350164	1.901824
-94.648373	16.103790	1.906829
-95.025958	26.261755	1.911834
-95.398298	25.281136	1.916838
-95.321241	21.564811	1.921843
-95.327498	23.710809	1.926848
-95.285919	13.402057	1.931853
-95.694006	28.271417	1.936858
-95.840537	22.643624	1.941862
-96.038811	19.106269	1.946867
-96.966813	23.195086	1.951872
-96.910983	21.945761	1.956877
-96.833080	24.927669	1.961882
-97.674660	27.071245	1.966886
-98.457504	22.282118	1.971891
-98.560143	19.759126	1.976896
-98.269878	24.093949	1.981901
-98.451521	24.736243	1.986906
-98.655836	28.760008	1.991910
-98.746383	9.193177	1.996915
-98.799363	20.480738	2.006912
-98.795508	20.722093	2.016909
-98.741439	20.009468	2.026906
-98.213430	21.789399	2.036902
-97.196873	32.706938	2.046899
-97.211073	22.261267	2.056896
-96.565265	29.709435	2.066893
-95.918607	25.002358	2.076890
-95.525223	24.569611	2.086886
-94.570047	20.135876	2.096883
-94.242745	26.798055	2.106880
-94.400498	27.011545	2.116877
-93.175127	23.056487	2.126874
-92.858470	22.194306	2.136870
-92.805809	26.494791	2.146867
-91.899280	26.097266	2.156864
-91.345179	24.501898	2.166861
-90.906628	31.419831	2.176858
-90.228102	22.260260	2.186854
-90.030090	26.611862	2.196851
-89.419873	25.683492	2.206848
-88.906143	27.082092	2.216845
-88.664528	21.318696	2.226842
-87.669481	26.870497	2.236838
-87.202602	27.646794	2.246835
-86.922602	32.467464	2.256832
-86.803045	24.933070	2.266829
-85.681975	29.146835	2.276826
-85.170050	35.536091	2.286822
-85.069570	26.214369	2.296819
-84.306913	21.663267	2.306816
-84.070525	19.674180	2.316813
-83.633369	22.658467	2.326810
-82.550266	17.608152	2.336806
-82.570495	18.532602	2.346803
-82.110298	20.823693	2.356800
-81.096969	28.466243	2.366797
-80.911312	22.139554	2.376794
-80.599710	26.732886	2.386790
-79.841488	27.971900	2.396787
-79.569930	31.212716	2.406784
-78.850824	26.181416	2.416781
-78.372964	29.542250	2.426778
-78.064328	18.813123	2.436774
-76.890968	19.664623	2.446771
-76.543492	23.308335	2.456768
-76.544693	20.341191	2.466765
-76.188319	23.294650	2.476762
-75.321140	20.623958	2.486758
-74.821822	25.379124	2.496755
-74.407186	23.832826	2.506752
-73.384463	24.986972	2.516749
-73.235158	27.067948	2.526746
-73.109471	26.887167	2.536742
-72.439932	27.614365	2.546739
-71.741991	10.573153	2.556736
-71.562701	18.063900	2.566733
-71.133971	16.278161	2.576730
-70.031428	16.106298	2.586726
-69.840750	21.373533	2.596723
-69.573689	15.147319	2.606720
-68.627775	20.810430	2.616717
-68.501282	25.807769	2.626714
-67.824320	27.785818	2.636710
-67.099807	21.991939	2.646707
-66.893099	29.195196	2.656704
-66.660646	25.211174	2.666701
-65.646394	18.166841	2.676698
-65.341941	24.041502	2.686694
-64.944918	23.637396	2.696691
-63.983333	23.502403	2.706688
-63.778431	32.809826	2.716685
-63.604233	27.564040	2.726682
-62.875957	23.449387	2.736678
-62.313993	23.513598	2.746675
-61.915350	26.101223	2.756672
-60.826044	29.129246	2.766669
-60.461366	27.225528	2.776666
-60.529341	22.787017	2.786662
-60.170563	21.829517	2.796659
-59.391254	18.436056	2.806656
-59.347481	23.749447	2.816653
-58.120524	21.291815	2.826650
-57.462798	23.380549	2.836646
-57.718506	21.026725	2.846643
-56.859425	22.774746	2.856640
-56.056689	27.078978	2.866637
-55.978635	22.021666	2.876634
-55.239921	19.729168	2.886630
-54.470076	25.274749	2.896627
-54.260846	19.407869	2.906624
-53.979701	23.535031	2.916621
-53.110595	21.633610	2.926618
-52.832480	20.442342	2.936614
-52.557678	25.229696	2.946611
-51.845471	14.835370	2.956608
-51.379948	13.018819	2.966605
-50.895704	18.656329	2.976602
-49.821604	18.929415	2.986598
-49.893125	17.296185	2.996595
-49.806079	17.806452	3.006592
-48.915368	29.891502	3.016589
-48.279520	12.737119	3.026586
-47.438578	17.415940	3.036582
-46.942398	20.015013	3.046579
-46.794232	18.421927	3.056576
-46.572726	22.429191	3.066573
-46.046153	23.113574	3.076570
-45.078795	22.708518	3.086566
-44.830490	17.136260	3.096563
-44.309190	27.097250	3.106560
-43.844352	31.466941	3.116557
-43.389787	24.541922	3.126554
-42.502895	18.798904	3.136550
-42.097089	23.715041	3.146547
-41.923472	28.338428	3.156544
-41.360998	21.338570	3.166541
-40.410270	25.704154	3.176538
-40.339925	21.464141	3.186534
-40.022959	19.642450	3.196531
-38.876553	23.676367	3.206528
-38.505285	24.011554	3.216525
-38.497542	17.723528	3.226522
-38.085627	18.195008	3.236518
-36.982573	20.454131	3.246515
-37.330166	20.075998	3.256512
-35.831612	21.461067	3.266509
-35.348609	25.209303	3.276506
-35.042633	20.544046	3.286502
-35.120478	18.569257	3.296499
-34.844418	21.175680	3.306496
-34.138813	26.651133	3.316493
-33.049734	25.816455	3.326490
-32.609181	18.737283	3.336486
-32.342381	18.749993	3.346483
-31.990350	21.389034	3.356480
-31.113276	28.372788	3.366477
-30.840336	28.999553	3.376474
-29.978204	24.091290	3.386470
-29.282188	26.856710	3.396467
-29.303421	29.292444	3.406464
-29.181824	31.197240	3.416461
-28.528051	24.093886	3.426458
-27.715512	26.541982	3.436454
-26.681483	24.105759	3.446451
-26.873249	24.264439	3.456448
-26.353835	27.893015	3.466445
-26.020498	33.288883	3.476442
-24.903711	27.010927	3.486438
-24.585968	22.457521	3.496435
-24.637137	25.152125	3.506432
-23.464119	33.158579	3.516429
-22.972368	20.825657	3.526426
-22.637916	20.384734	3.536422
-22.331595	23.547856	3.546419
-21.501182	22.305885	3.556416
-21.307338	27.657562	3.566413
-20.985783	21.175902	3.576410
-19.936928	20.004317	3.586406
-19.539268	16.556146	3.596403
-19.639929	21.953613	3.606400
-18.756820	18.292963	3.616397
-17.816519	21.377182	3.626394
-17.678424	24.525195	3.636390
-17.571081	23.413094	3.646387
-16.607472	23.497094	3.656384
-16.505822	24.294196	3.666381
-15.526450	19.054862	3.676378
-14.709395	17.953223	3.686374
-14.550073	24.445357	3.696371
-14.515098	16.879776	3.706368
-13.982967	20.486677	3.716365
-13.084393	21.265520	3.726362
-12.732973	25.530182	3.736358
-11.705064	20.029676	3.746355
-11.409231	25.999236	3.756352
-11.291337	22.020426	3.766349
-11.192892	25.438606	3.776346
-10.262364	20.365458	3.786342
-9.789252	20.656650	3.796339
-8.812920	20.082364	3.806336
-8.409741	27.822010	3.816333
-8.321693	24.606485	3.826330
-7.844114	20.698296	3.836326
-7.503740	16.126905	3.846323
-6.736089	16.369141	3.856320
-6.499826	23.366944	3.866317
-5.671213	18.572534	3.876314
-5.133882	26.818418	3.886310
-4.252654	29.959289	3.896307
-3.760655	27.249612	3.906304
-3.969691	24.427854	3.916301
-3.811424	25.817582	3.926298
-3.271720	35.915814	3.936294
-2.457174	54.377915	3.946291
-2.005439	70.138716	3.956288
-1.594232	83.013049	3.966285
-1.155028	95.053282	3.976282
-0.871394	111.537562	3.986278
0.000000	120.292336	3.991283
-0.061599	136.959131	3.996288
-0.237718	136.099995	4.001293
0.221732	149.509272	4.006298
0.505454	167.849700	4.011302
0.760094	161.248228	4.016307
0.632828	168.791665	4.021312
0.258885	179.182963	4.026317
0.666740	168.858012	4.031322
0.324335	169.163345	4.036326
0.729406	159.862623	4.041331
0.647282	170.568699	4.046336
0.232885	174.528161	4.051341
0.732629	158.195948	4.056346
0.739763	165.284294	4.061350
0.672204	165.104287	4.066355
0.643760	172.109554	4.071360
0.553239	170.300439	4.076365
0.540150	162.665243	4.081370
0.572280	175.967774	4.086374
0.753319	169.389187	4.091379
0.608268	168.099240	4.096384
0.864375	167.901350	4.101389
0.827644	159.027681	4.106394
0.811015	171.772364	4.111398
0.916269	178.108753	4.116403
1.060355	175.446251	4.121408
1.045014	174.097645	4.126413
0.966482	168.500716	4.131418
0.685965	174.389344	4.136422
0.784671	171.159557	4.141427
0.942716	167.153469	4.146432
0.630958	170.541168	4.151437
0.650154	162.548368	4.156442
0.641409	179.319495	4.161446
0.455250	169.711717	4.166451
0.795241	178.191585	4.171456
0.730203	197.512545	4.176461
1.131038	188.560408	4.181466
1.319943	196.261465	4.186470
1.522213	187.544993	4.191475
1.381473	177.165787	4.196480
0.980138	167.721449	4.201485
0.608822	167.742298	4.206490
0.716943	188.584314	4.211494
1.117466	186.493878	4.216499
1.101174	190.421114	4.221504
0.899399	197.124867	4.226509
1.110352	198.573724	4.231514
1.039441	210.499651	4.236518
1.378099	210.778608	4.241523
1.306366	201.267428	4.246528
1.157886	190.156606	4.251533
1.181951	181.175929	4.256538
0.724140	190.212872	4.261542
1.178849	189.085884	4.266547
0.967407	192.866182	4.271552
1.028457	217.299029	4.276557
1.065871	201.830777	4.281562
1.366799	200.812228	4.286566
1.296413	197.886017	4.291571
1.524823	200.680149	4.296576
1.083544	195.528895	4.301581
1.406353	201.610883	4.306586
1.367248	204.321412	4.311590
1.703851	200.366740	4.316595
1.562999	194.628214	4.321600
1.603295	199.712086	4.326605
1.264269	187.546818	4.331610
0.905428	183.681892	4.336614
1.394286	198.541849	4.341619
1.561590	206.384832	4.346624
1.416412	209.438986	4.351629
1.365357	204.059477	4.356634
1.512898	206.385955	4.361638
1.404974	203.469337	4.366643
1.451537	197.779381	4.371648
1.326503	198.744971	4.376653
1.594435	208.746428	4.381658
1.661560	207.682676	4.386662
1.223492	197.665649	4.391667
1.815542	196.742962	4.396672
0.959959	208.177515	4.401677
1.560690	202.726572	4.406682
1.667533	206.976507	4.411686
1.402790	192.477663	4.416691
1.522975	197.595615	4.421696
1.300565	204.894602	4.426701
1.592037	200.633278	4.431706
1.582765	201.271195	4.436710
1.417110	210.751934	4.441715
1.426215	213.576009	4.446720
1.303819	215.017325	4.451725
1.404552	203.605578	4.456730
1.624580	209.834103	4.461734
1.595191	208.046988	4.466739
1.558051	209.378624	4.471744
1.378326	215.577692	4.476749
1.856384	214.537003	4.481754
1.619180	222.526162	4.486758
1.927501	232.031338	4.491763
2.429745	217.029659	4.496768
1.807396	226.174482	4.501773
1.816550	208.798172	4.506778
1.729292	208.434367	4.511782
1.881527	206.522738	4.516787
2.121995	200.312350	4.521792
1.663204	214.665021	4.526797
1.536916	194.528056	4.531802
1.457321	215.779400	4.536806
1.680407	210.026552	4.541811
1.950053	224.460027	4.546816
2.313500	229.670362	4.551821
1.982539	218.381663	4.556826
1.713390	211.197483	4.561830
1.816413	214.206437	4.566835
1.906622	215.864805	4.571840
2.015119	235.497763	4.576845
2.164890	229.015320	4.581850
2.054581	224.602126	4.586854
1.904666	205.760026	4.591859
1.821461	214.270590	4.596864
2.249054	227.396533	4.601869
2.227865	220.213364	4.606874
1.924535	218.174399	4.611878
1.775115	214.236769	4.616883
2.187642	215.688038	4.621888
1.834446	231.699516	4.626893
2.095715	231.349610	4.631898
2.201723	238.782281	4.636902
2.431335	232.407136	4.641907
2.061129	232.340579	4.646912
1.796134	237.071857	4.651917
1.958176	241.708083	4.656922
2.134502	241.631986	4.661926
2.169476	248.071055	4.666931
2.310957	243.286261	4.671936
1.923710	254.664119	4.676941
2.193870	244.357071	4.681946
2.502848	245.841539	4.686950
2.338428	246.100713	4.691955
2.186487	238.315694	4.696960
2.301291	245.518000	4.701965
2.398958	235.876818	4.706970
2.482981	240.518908	4.711974
2.448059	239.128164	4.716979
2.633194	236.249656	4.721984
2.119587	226.631148	4.726989
2.552738	233.253656	4.731994
2.396742	230.333577	4.736998
2.108476	219.207883	4.742003
2.459239	233.094887	4.747008
2.141561	242.891783	4.752013
2.552573	246.319994	4.757018
2.279200	240.741611	4.762022
2.365027	253.512351	4.767027
2.512380	242.068357	4.772032
2.364593	243.003198	4.777037
2.637566	244.089905	4.782042
2.360988	246.882537	4.787046
2.163556	246.685044	4.792051
2.159658	240.457438	4.797056
2.561533	250.061923	4.802061
2.516732	245.749723	4.807066
2.412285	253.218368	4.812070
2.561680	252.737083	4.817075
2.783071	248.597704	4.822080
2.485162	260.387746	4.827085
2.617430	245.283156	4.832090
2.708345	243.635091	4.837094
2.507619	248.747002	4.842099
2.815607	237.034974	4.847104
2.506132	248.459298	4.852109
2.323512	246.264106	4.857114
2.511942	244.782957	4.862118
2.450031	248.822575	4.867123
2.987547	235.330141	4.872128
2.776856	242.760990	4.877133
2.595868	244.162912	4.882138
2.756958	245.449565	4.887142
2.726892	246.604600	4.892147
2.606875	241.564903	4.897152
2.635410	246.577731	4.902157
2.774813	237.914698	4.907162
2.649827	249.668097	4.912166
2.442266	248.202447	4.917171
3.138497	263.229476	4.922176
2.795237	266.101077	4.927181
3.271906	270.684424	4.932186
3.087783	252.876060	4.937190
2.552623	253.547321	4.942195
2.658469	244.613201	4.947200
2.721025	248.555367	4.952205
2.910575	264.226054	4.957210
3.147696	264.047303	4.962214
2.700224	275.301788	4.967219
3.178180	273.463687	4.972224
3.014526	273.199997	4.977229
3.060271	272.902884	4.982234
2.760652	263.962739	4.987238
3.044593	268.558583	4.992243
2.966695	269.985207	4.997248
2.975100	279.301489	5.002253
2.929490	265.991398	5.007258
3.114607	269.530766	5.012262
3.023349	272.671085	5.017267
3.404595	269.446609	5.022272
3.185850	275.021508	5.027277
3.293585	265.141440	5.032282
2.941225	255.604251	5.037286
3.035354	261.866353	5.042291
3.200367	259.445447	5.047296
3.124625	273.260114	5.052301
2.998664	269.559120	5.057306
3.019047	269.990832	5.062310
2.922397	273.633275	5.067315
3.193707	264.782542	5.072320
3.013445	283.932731	5.077325
2.943989	272.887253	5.082330
2.881070	268.232329	5.087334
2.748747	267.460231	5.092339
2.963102	275.578800	5.097344
2.824094	282.380494	5.102349
3.133227	296.409845	5.107354
3.761835	302.721852	5.112358
3.403065	285.324321	5.117363
3.427613	282.001460	5.122368
3.044258	287.796717	5.127373
3.407939	293.295536	5.132378
3.554326	292.580909	5.137382
3.169450	285.345482	5.142387
3.420263	297.327915	5.147392
3.231829	294.675868	5.152397
3.581308	300.608422	5.157402
3.327316	296.972313	5.162406
3.202615	301.904069	5.167411
3.694743	300.637851	5.172416
3.497835	299.003481	5.177421
3.414406	300.823524	5.182426
3.476743	302.543169	5.187430
3.632913	317.036638	5.192435
3.739987	299.851150	5.197440
3.508094	305.860407	5.202445
3.697403	292.824810	5.207450
3.708185	284.483669	5.212454
3.396339	280.648993	5.217459
3.780042	274.980524	5.222464
3.136234	280.530567	5.227469
3.723541	282.012978	5.232474
3.807837	287.200664	5.237478
3.235751	289.187768	5.242483
3.975318	282.646342	5.247488
3.621921	298.318113	5.252493
3.776159	292.736125	5.257498
3.793145	289.051228	5.262502
3.248231	279.580761	5.267507
3.250374	287.842155	5.272512
3.387332	299.495813	5.277517
3.424551	290.712786	5.282522
3.610241	294.343035	5.287526
3.590260	295.232956	5.292531
3.813645	296.698898	5.297536
3.668578	298.623117	5.302541
3.676518	296.823472	5.307546
3.745134	296.377319	5.312550
3.599991	306.403098	5.317555
3.974095	297.390221	5.322560
3.408200	302.456088	5.327565
3.613619	308.459950	5.332570
3.769825	313.633719	5.337574
3.917001	327.698701	5.342579
4.243970	316.623216	5.347584
4.043786	320.271236	5.352589
4.013714	306.420002	5.357594
3.994695	303.615671	5.362598
3.694784	299.268700	5.367603
3.954511	305.092643	5.372608
3.825319	312.995224	5.377613
4.109192	320.572419	5.382618
4.274404	310.184302	5.387622
4.049955	314.177939	5.392627
4.120639	299.098136	5.397632
3.758041	297.401717	5.402637
3.787672	297.239890	5.407642
3.924482	313.273410	5.412646
3.997046	326.013853	5.417651
4.166850	325.920094	5.422656
4.172374	332.253191	5.427661
4.154215	329.744122	5.432666
4.181361	332.389000	5.437670
3.829059	338.094655	5.442675
3.970072	329.867807	5.447680
4.092983	334.373615	5.452685
3.997159	326.220865	5.457690
4.209581	333.117300	5.462694
4.094731	333.025664	5.467699
4.181562	335.330481	5.472704
3.939971	337.503801	5.477709
4.139591	336.002037	5.482714
4.538960	329.921081	5.487718
4.195425	331.607944	5.492723
4.427304	330.429183	5.497728
4.301449	333.912312	5.502733
4.347622	333.607036	5.507738
4.007210	329.923123	5.512742
3.998399	333.057644	5.517747
4.329739	325.902460	5.522752
4.418034	337.489840	5.527757
4.277531	328.025927	5.532762
4.427102	338.143046	5.537766
4.262267	326.568148	5.542771
4.254640	339.410534	5.547776
4.218847	336.144263	5.552781
3.958637	336.176441	5.557786
4.277543	344.985507	5.562790
4.140264	360.667004	5.567795
4.754390	365.605429	5.572800
4.859988	369.187835	5.577805
4.622978	349.402765	5.582810
4.416853	342.243963	5.587814
4.277399	340.456182	5.592819
4.343108	331.953741	5.597824
4.336855	349.742885	5.602829
4.506270	351.197476	5.607834
4.647727	363.064148	5.612838
4.469497	369.549361	5.617843
4.611570	362.913234	5.622848
4.466243	362.993608	5.627853
4.390273	368.527444	5.632858
4.310748	360.278826	5.637862
4.783023	363.858695	5.642867
4.759173	367.414862	5.647872
4.667862	363.286974	5.652877
4.810714	363.136914	5.657882
4.981789	368.147797	5.662886
4.483578	371.610931	5.667891
4.702211	365.902180	5.672896
4.729668	378.300290	5.677901
4.356784	372.378854	5.682906
4.483380	371.301852	5.687910
4.439444	372.705278	5.692915
5.141202	362.119411	5.697920
4.503261	378.261249	5.702925
4.661197	373.147682	5.707930
4.449091	370.578687	5.712934
4.472640	374.840935	5.717939
4.662979	362.482361	5.722944
4.950973	375.638738	5.727949
4.842095	374.165554	5.732954
5.150509	368.843258	5.737958
4.790849	378.346084	5.742963
4.566161	366.088262	5.747968
4.707386	387.572302	5.752973
5.177976	381.567894	5.757978
4.847727	387.720417	5.762982
4.766954	386.474824	5.767987
4.949561	393.180090	5.772992
4.907232	397.580575	5.777997
4.796911	397.973827	5.783002
5.202101	397.453574	5.788006
4.732439	395.357969	5.793011
5.214660	388.981819	5.798016
4.809903	394.612938	5.803021
4.957035	398.521549	5.808026
5.241474	399.493684	5.813030
4.593045	392.549075	5.818035
4.875698	397.185824	5.823040
4.995692	397.165266	5.828045
4.984216	390.281339	5.833050
4.980731	391.095904	5.838054
4.565966	402.306170	5.843059
4.970691	395.140928	5.848064
5.166855	397.280173	5.853069
5.039721	402.701361	5.858074
5.272211	406.988484	5.863078
5.291271	408.785980	5.868083
5.090046	395.480528	5.873088
5.365328	403.299744	5.878093
5.184059	394.260128	5.883098
5.198382	396.207397	5.888102
5.132262	413.972821	5.893107
5.426258	415.800001	5.898112
5.224282	418.647357	5.903117
5.406991	425.199291	5.908122
5.543921	409.742509	5.913126
4.913661	405.299258	5.918131
5.073338	409.369969	5.923136
5.288669	422.083408	5.928141
5.134682	427.616024	5.933146
5.039549	422.249883	5.938150
4.988693	429.346016	5.943155
5.367628	425.796881	5.948160
5.672317	434.105945	5.953165
5.450242	426.831353	5.958170
5.949983	422.985869	5.963174
5.574089	422.579654	5.968179
5.333636	425.580421	5.973184
5.492095	427.024212	5.978189
5.545608	423.265329	5.983194
5.717092	430.851196	5.988198
5.131136	435.954184	5.993203
5.658634	422.316831	5.998208
5.586582	423.511023	6.003213
5.334916	425.929738	6.008218
6.242138	427.352282	6.013222
5.609788	427.988395	6.018227
5.572854	408.240246	6.023232
5.432984	407.399736	6.028237
5.047339	415.379528	6.033242
5.515911	419.782126	6.038246
5.057476	419.843897	6.043251
5.341495	424.327688	6.048256
5.605458	427.890890	6.053261
5.620004	426.306412	6.058266
5.665742	427.298688	6.063270
5.263348	431.903282	6.068275
5.733001	423.165915	6.073280
5.665122	426.024728	6.078285
5.463203	426.228766	6.083290
5.758084	420.965535	6.088294
5.532487	439.795085	6.093299
5.574270	434.000657	6.098304
5.532988	431.064039	6.103309
5.308416	437.476865	6.108314
5.349061	435.963628	6.113318
4.941726	438.150499	6.118323
5.581059	429.821235	6.123328
5.480753	432.930925	6.128333
5.460559	429.031158	6.133338
5.500774	422.099356	6.138342
5.427154	428.863605	6.143347
5.366770	426.754828	6.148352
4.999664	424.536796	6.153357
5.603651	423.437472	6.158362
5.599790	429.934182	6.163366
5.230994	424.206028	6.168371
5.298884	434.764413	6.173376
5.321822	431.005873	6.178381
5.292093	433.568066	6.183386
5.491644	420.670965	6.188390
5.397411	427.358126	6.193395
5.777962	424.875716	6.198400
5.697844	425.191132	6.203405
5.829013	431.562587	6.208410
5.604356	423.089810	6.213414
5.635588	437.435041	6.218419
5.716708	427.308874	6.223424
5.664234	427.273174	6.228429
5.719377	427.433104	6.233434
5.871953	425.011279	6.238438
5.760093	431.569947	6.243443
5.498961	417.980797	6.248448
5.947764	419.111702	6.253453
5.535974	410.795145	6.258458
5.446838	393.785826	6.263462
5.378297	408.509330	6.268467
5.300238	382.064766	6.273472
5.543503	403.252047	6.278477
5.424300	413.587149	6.283482
5.724045	409.900613	6.288486
5.292647	410.847280	6.293491
5.465771	412.433871	6.298496
5.501471	415.857606	6.303501
5.345770	420.472698	6.308506
5.449401	413.298489	6.313510
5.172045	426.528158	6.318515
5.511916	421.465835	6.323520
5.674880	421.514306	6.328525
5.572461	425.589514	6.333530
5.335980	427.683259	6.338534
5.492551	434.863319	6.343539
5.571651	424.921998	6.348544
5.727526	428.363649	6.353549
5.765890	436.375394	6.358554
5.947774	413.828167	6.363558
5.573875	423.818240	6.368563
5.192719	387.937734	6.373568
5.235267	390.569011	6.378573
5.306810	403.579051	6.383578
5.565228	419.377767	6.388582
5.429491	425.373851	6.393587
5.301391	415.007579	6.398592
5.389966	431.922053	6.403597
5.402606	416.612810	6.408602
5.532637	419.915687	6.413606
5.411976	422.238034	6.418611
5.494815	422.285615	6.423616
5.326738	422.013186	6.428621
5.390437	430.933985	6.433626
5.655150	414.832181	6.438630
5.549684	422.245428	6.443635
5.651998	413.552547	6.448640
5.746469	417.062419	6.453645
5.507441	429.085722	6.458650
5.754745	422.108842	6.463654
5.717863	422.089890	6.468659
5.501929	408.067781	6.473664
5.497830	408.854427	6.478669
5.515908	404.473320	6.483674
5.591890	396.382159	6.488678
5.164092	405.613348	6.493683
5.419839	415.234924	6.498688
5.508387	422.288347	6.503693
5.702925	423.697330	6.508698
5.791213	421.559106	6.513702
5.112343	412.175745	6.518707
5.484132	422.328603	6.523712
5.765646	430.289076	6.528717
5.552848	412.472862	6.533722
5.386283	403.838689	6.538726
5.145295	407.650787	6.543731
5.463151	424.123790	6.548736
6.067562	424.619854	6.553741
5.449034	421.886731	6.558746
5.672790	404.903340	6.563750
5.330492	406.948761	6.568755
5.318834	403.214133	6.573760
5.656804	419.562625	6.578765
5.511091	413.518561	6.583770
5.539749	407.483404	6.588774
5.606524	405.993256	6.593779
5.472769	392.054591	6.598784
5.253530	398.055861	6.603789
5.296672	405.216872	6.608794
5.775855	409.835364	6.613798
5.721155	414.769137	6.618803
5.285561	400.349999	6.623808
5.515123	406.836515	6.628813
5.198292	405.119452	6.633818
5.720609	419.459411	6.638822
5.679261	421.094872	6.643827
5.694976	403.042958	6.648832
5.432590	392.951609	6.653837
4.827129	403.328454	6.658842
5.274917	415.577993	6.663846
5.510082	434.342002	6.668851
5.449151	426.032833	6.673856
5.567333	438.663370	6.678861
5.879077	424.463555	6.683866
5.487574	424.386130	6.688870
5.512148	429.012701	6.693875
5.427138	437.059752	6.698880
5.552252	437.909383	6.703885
5.097852	436.012124	6.708890
5.687993	436.083525	6.713894
5.383097	431.616576	6.718899
5.706825	434.719722	6.723904
5.721398	431.816050	6.728909
5.739798	427.585844	6.733914
5.469158	404.762392	6.738918
5.445357	420.385226	6.743923
5.496458	418.681994	6.748928
5.706760	419.529107	6.753933
5.365829	415.988327	6.758938
5.372102	402.018881	6.763942
5.613420	405.708189	6.768947
5.432328	420.042913	6.773952
5.478560	419.968311	6.778957
5.070268	439.899956	6.783962
5.771025	426.039821	6.788966
5.678399	435.083695	6.793971
5.759021	423.476411	6.798976
5.326199	406.135650	6.803981
5.603646	399.491806	6.808986
5.482771	410.125752	6.813990
5.521942	398.065191	6.818995
5.460185	408.260698	6.824000
5.527341	396.928587	6.829005
5.293285	408.127370	6.834010
5.878065	411.211789	6.839014
5.452744	401.034641	6.844019
5.533869	403.998728	6.849024
5.442300	403.775743	6.854029
5.447733	401.940982	6.859034
5.426173	394.679451	6.864038
5.361299	415.347469	6.869043
5.763860	411.144782	6.874048
5.524144	407.916139	6.879053
5.324165	393.362138	6.884058
5.507230	404.486852	6.889062
5.647034	405.761467	6.894067
5.606291	401.048353	6.899072
5.717339	405.319154	6.904077
5.376571	404.089344	6.909082
5.593140	401.508293	6.914086
5.299351	400.340926	6.919091
5.449676	401.329235	6.924096
5.393554	401.389060	6.929101
5.474888	389.021943	6.934106
5.710256	401.087537	6.939110
5.328857	398.162267	6.944115
5.388749	395.281459	6.949120
5.498741	395.400896	6.954125
5.653348	400.125232	6.959130
5.651865	386.724625	6.964134
5.369325	407.170302	6.969139
5.253530	408.509503	6.974144
5.521337	408.485097	6.979149
5.541546	419.723916	6.984154
5.856889	405.820903	6.989158
5.464951	406.084547	6.994163
5.414277	396.292095	6.999168
5.714844	398.386163	7.004173
5.491245	403.965665	7.009178
5.637576	395.989500	7.014182
5.234660	402.663232	7.019187
5.340196	401.866985	7.024192
5.384680	396.772267	7.029197
5.374486	403.280675	7.034202
5.692220	405.241846	7.039206
5.583131	400.254351	7.044211
5.644596	406.490367	7.049216
5.692541	402.861076	7.054221
5.247863	406.359128	7.059226
5.459749	397.137143	7.064230
5.555005	408.402749	7.069235
5.535220	406.760043	7.074240
5.539766	407.227345	7.079245
5.545228	410.779242	7.084250
5.373256	405.864949	7.089254
5.305740	405.297562	7.094259
5.474206	397.648255	7.099264
5.759830	398.104161	7.104269
5.349983	398.347101	7.109274
5.277015	400.928118	7.114278
5.213245	405.227778	7.119283
5.494003	425.195443	7.124288
5.970650	427.267944	7.129293
5.135275	427.544118	7.134298
5.774534	421.881466	7.139302
5.553596	419.594937	7.144307
5.453680	425.309192	7.149312
5.577890	401.330231	7.154317
5.662767	412.987500	7.159322
5.530888	409.304032	7.164326
5.456596	407.821741	7.169331
5.269828	401.683864	7.174336
5.092606	413.031270	7.179341
5.214643	424.931804	7.184346
5.562095	426.592232	7.189350
5.421862	432.372391	7.194355
5.497749	428.897306	7.199360
5.553300	429.077493	7.204365
5.362539	433.782284	7.209370
5.408352	433.702028	7.214374
5.503503	438.098815	7.219379
5.564767	440.806319	7.224384
5.786376	428.352905	7.229389
5.825861	439.140385	7.234394
5.928700	416.872301	7.239398
5.918695	405.521830	7.244403
5.366276	405.496608	7.249408
5.359767	402.267092	7.254413
5.173277	395.709440	7.259418
5.641230	393.380834	7.264422
5.180720	396.587683	7.269427
5.457450	414.990544	7.274432
5.785625	414.869474	7.279437
5.395992	414.835349	7.284442
5.440740	419.564533	7.289446
5.231848	430.974443	7.294451
5.308244	437.271138	7.299456
5.695808	421.603963	7.304461
5.685801	433.259850	7.309466
5.774087	427.291539	7.314470
5.357021	418.664855	7.319475
5.449405	422.780302	7.324480
5.708449	429.324483	7.329485
5.265010	425.835273	7.334490
5.376287	427.841024	7.339494
5.453641	429.810974	7.344499
5.660518	432.011196	7.349504
5.638848	430.987250	7.354509
5.452005	434.228738	7.359514
5.466170	429.066824	7.364518
5.265581	429.175329	7.369523
5.479242	426.528255	7.374528
5.787452	427.265558	7.379533
5.444434	432.638575	7.384538
5.052298	437.357105	7.389542
5.282797	438.268943	7.394547
5.091612	437.865968	7.399552
5.444564	431.512866	7.404557
5.586791	429.435927	7.409562
5.720315	435.433437	7.414566
5.395327	440.643223	7.419571
5.380296	434.992229	7.424576
5.828852	429.147558	7.429581
5.357730	432.138714	7.434586
5.714639	428.097137	7.439590
5.517656	440.630480	7.444595
5.435515	443.053779	7.449600
5.519679	435.344661	7.454605
5.488207	433.517214	7.459610
5.515197	438.955423	7.464614
5.454540	436.941411	7.469619
5.528318	440.494392	7.474624
5.683573	434.971779	7.479629
5.757714	440.531998	7.484634
5.537751	441.879241	7.489638
5.634073	435.874860	7.494643
5.378446	437.906471	7.499648
5.750102	434.203043	7.504653
5.614498	434.886240	7.509658
5.401465	413.914469	7.514662
5.591235	426.379965	7.519667
5.486497	419.911723	7.524672
5.409975	421.808186	7.529677
5.486472	431.145406	7.534682
5.651790	424.432769	7.539686
5.675944	429.695028	7.544691
5.596729	413.627105	7.549696
5.339559	415.440914	7.554701
5.353579	415.612020	7.559706
5.566829	427.644607	7.564710
5.474963	422.757843	7.569715
5.366077	422.255349	7.574720
5.565352	422.555702	7.579725
5.532592	422.681896	7.584730
5.907131	422.598112	7.589734
5.783140	412.073882	7.594739
5.676639	405.720590	7.599744
5.749861	402.770274	7.604749
5.490371	414.807623	7.609754
5.403212	404.706875	7.614758
5.385208	403.879262	7.619763
5.116770	404.875607	7.624768
5.253091	400.244162	7.629773
5.135356	410.913699	7.634778
5.660223	411.485341	7.639782
5.739146	411.077728	7.644787
5.486913	399.979461	7.649792
5.552740	400.884331	7.654797
5.106431	405.256652	7.659802
5.543955	416.126944	7.664806
5.640331	426.972645	7.669811
5.694614	416.296236	7.674816
5.558824	405.120989	7.679821
5.529702	412.831556	7.684826
5.765625	408.402596	7.689830
5.944213	410.656456	7.694835
5.428264	404.893172	7.699840
5.573285	406.888379	7.704845
5.116431	408.390040	7.709850
5.579763	412.104609	7.714854
5.259780	404.619563	7.719859
5.580546	417.321393	7.724864
5.763755	406.504371	7.729869
5.593524	411.410182	7.734874
5.123298	411.767153	7.739878
5.670017	408.622495	7.744883
4.972374	401.806239	7.749888
5.302660	402.000555	7.754893
5.431336	417.579098	7.759898
5.918635	419.164777	7.764902
6.098758	412.063893	7.769907
5.461069	408.652756	7.774912
5.606957	393.999826	7.779917
5.592826	401.041693	7.784922
5.717662	399.756595	7.789926
5.517600	409.608047	7.794931
5.635541	400.879029	7.799936
5.673695	415.278146	7.804941
5.256570	398.755699	7.809946
5.482103	397.608378	7.814950
5.382327	399.915805	7.819955
5.379258	403.614752	7.824960
5.594658	400.889051	7.829965
5.202860	412.441633	7.834970
5.196278	409.643898	7.839974
5.395300	387.644821	7.844979
4.995928	411.313263	7.849984
5.403238	405.662333	7.854989
5.400266	422.632665	7.859994
5.769058	417.518373	7.864998
5.648387	411.869160	7.870003
5.124418	410.910351	7.875008
5.681119	418.837116	7.880013
5.790796	414.004077	7.885018
5.780157	404.892286	7.890022
5.657974	405.367036	7.895027
5.469842	400.337621	7.900032
5.650684	403.649217	7.905037
5.336869	408.223887	7.910042
5.498858	403.998237	7.915046
5.323420	408.808219	7.920051
5.267871	405.445562	7.925056
5.720864	404.697334	7.930061
5.611171	401.583045	7.935066
5.305382	391.123185	7.940070
5.803709	400.278582	7.945075
5.431653	405.560511	7.950080
5.482614	390.013648	7.955085
5.726062	409.005948	7.960090
5.759600	402.606097	7.965094
5.593665	404.198327	7.970099
5.749930	398.741864	7.975104
5.444992	397.216016	7.980109
5.906188	406.403242	7.985114
5.527111	407.945848	7.990118
5.644470	404.982742	7.995136
5.367015	399.334098	8.000154
5.660427	395.494526	8.005171
5.629377	399.854767	8.010189
5.669570	404.935973	8.015206
5.516303	399.132842	8.020224
5.343062	407.661604	8.025242
5.554779	404.280842	8.030259
5.592938	405.751112	8.035277
5.231888	399.934097	8.040294
5.570682	412.099452	8.045312
5.604124	406.694379	8.050330
5.738129	404.748250	8.055347
5.390796	402.365442	8.060365
5.379624	413.890804	8.065382
5.115059	396.361016	8.070400
5.566846	398.884673	8.075418
5.498831	398.387935	8.080435
5.362038	406.821080	8.085453
5.353424	405.229137	8.090470
5.630362	397.354100	8.095488
5.470731	405.973306	8.100506
5.562172	401.281165	8.105523
5.267845	405.261782	8.110541
5.274979	411.358233	8.115558
5.630655	416.107701	8.120576
5.586816	432.197727	8.125594
5.805631	427.622583	8.130611
6.007681	438.889316	8.135629
5.635453	423.558688	8.140646
5.840086	423.264836	8.145664
5.363603	423.771926	8.150682
5.562089	407.617388	8.155699
5.554955	414.299621	8.160717
5.523601	433.460515	8.165734
5.902584	431.257346	8.170752
5.856593	442.960352	8.175770
5.693668	431.715022	8.180787
5.685795	421.034820	8.185805
5.569797	427.276140	8.190822
5.650627	426.869611	8.195840
5.666592	437.748611	8.200858
5.771865	429.305491	8.205875
6.036370	435.170411	8.210893
5.526059	421.924553	8.215910
5.610971	424.574542	8.220928
5.576933	429.956847	8.225946
5.671536	427.802324	8.230963
5.746748	429.853785	8.235981
5.698356	435.634701	8.240998
6.155514	437.352625	8.246016
5.574309	440.066094	8.251034
5.815659	441.499248	8.256051
5.821458	438.463306	8.261069
5.672309	438.531576	8.266086
5.717017	441.550422	8.271104
5.556044	443.281529	8.276122
5.879445	440.530168	8.281139
5.882518	440.669584	8.286157
5.766209	446.426757	8.291174
5.899219	440.251255	8.296192
5.646720	446.183018	8.301210
5.641818	432.593721	8.306227
5.871602	432.750372	8.311245
5.768294	432.510853	8.316262
5.809143	424.487659	8.321280
5.886298	429.968794	8.326298
5.840660	429.345315	8.331315
5.897200	438.974773	8.336333
5.430258	434.586633	8.341350
5.928771	426.861743	8.346368
5.889011	435.496078	8.351386
5.943606	439.149836	8.356403
5.792883	436.184197	8.361421
5.842828	437.960160	8.366438
5.933711	429.652097	8.371456
5.738220	445.442374	8.376474
5.836492	439.003970	8.381491
5.822236	440.224515	8.386509
5.936320	447.429871	8.391526
5.963120	433.606978	8.396544
5.796119	438.735034	8.401562
6.242799	442.308664	8.406579
6.105727	432.999016	8.411597
5.537487	433.914826	8.416614
5.987033	424.221289	8.421632
5.832909	435.331689	8.426650
5.789911	438.994188	8.431667
5.632944	443.896385	8.436685
5.554126	443.515407	8.441702
5.908171	439.584848	8.446720
6.049521	453.595288	8.451738
6.283162	453.325549	8.456755
6.105600	441.951161	8.461773
5.923005	440.751878	8.466790
6.329892	438.335822	8.471808
6.019174	436.240991	8.476826
6.159825	429.961279	8.481843
5.864171	438.500563	8.486861
5.908466	436.090448	8.491878
5.692487	438.311952	8.496896
5.757769	446.486159	8.501914
5.817621	450.459291	8.506931
6.174660	461.112144	8.511949
6.084922	464.849735	8.516966
6.341014	468.165311	8.521984
6.268004	458.985145	8.527002
5.885162	457.504213	8.532019
6.057396	447.346171	8.537037
6.281897	459.650628	8.542054
6.292239	439.853841	8.547072
5.785251	438.461846	8.552090
6.119286	438.082516	8.557107
5.995049	447.883943	8.562125
6.200253	466.163313	8.567143
6.290838	459.262834	8.572160
5.877027	448.938640	8.577178
5.949371	455.973002	8.582195
6.324731	456.711898	8.587213
6.218729	468.202673	8.592231
6.648108	448.596636	8.597248
6.200044	446.195134	8.602266
6.178989	442.422384	8.607283
6.163807	440.266423	8.612301
5.943194	431.663118	8.617319
6.206336	446.602040	8.622336
6.487424	443.274497	8.627354
6.193887	440.640638	8.632371
6.079502	433.284324	8.637389
6.066190	438.810811	8.642407
6.305534	437.867745	8.647424
5.970593	438.376111	8.652442
5.956812	429.317798	8.657459
6.494274	437.148581	8.662477
6.136293	443.249240	8.667495
6.298500	431.395196	8.672512
5.899186	441.169119	8.677530
6.283995	462.006780	8.682547
6.345071	455.203522	8.687565
6.177124	451.887036	8.692583
6.373380	448.671024	8.697600
6.151079	449.952918	8.702618
6.360986	452.184140	8.707635
6.256034	442.008203	8.712653
6.154317	451.786600	8.717671
6.424976	455.337920	8.722688
6.271395	446.504587	8.727706
6.363654	451.407288	8.732723
6.284409	441.476072	8.737741
6.002600	451.663107	8.742759
6.388323	458.051933	8.747776
6.299200	469.142105	8.752794
6.309635	458.764711	8.757811
6.465760	473.015014	8.762829
6.159314	473.369248	8.767847
6.497875	464.857612	8.772864
6.561045	477.188898	8.777882
6.378458	462.591799	8.782899
6.319026	451.640643	8.787917
6.168080	457.934631	8.792935
6.346197	464.994325	8.797952
6.489477	472.896353	8.802970
6.432530	469.649593	8.807987
6.242047	476.259975	8.813005
6.538560	478.559673	8.818023
6.640429	467.626179	8.823040
6.234721	457.770670	8.828058
6.326493	456.400203	8.833075
6.685397	455.624846	8.838093
6.001702	457.479251	8.843111
6.467565	461.622873	8.848128
6.441954	469.533681	8.853146
6.453624	470.349758	8.858163
6.551370	464.707816	8.863181
6.313881	471.157520	8.868199
6.561332	466.852580	8.873216
6.663765	468.768431	8.878234
6.765370	471.619769	8.883251
6.357025	454.923975	8.888269
6.389948	451.261925	8.893287
6.286416	468.252185	8.898304
6.651145	478.089474	8.903322
6.377131	465.630804	8.908339
6.842640	476.367401	8.913357
6.508677	467.106992	8.918375
6.422265	452.739762	8.923392
6.453875	460.946932	8.928410
6.497941	477.047786	8.933427
6.390687	459.842534	8.938445
6.467977	475.954595	8.943463
6.685425	470.583477	8.948480
6.788112	470.522101	8.953498
6.605752	470.557706	8.958515
6.405496	463.932318	8.963533
6.430762	466.136167	8.968551
6.593875	460.239880	8.973568
6.554195	474.806956	8.978586
6.480500	471.762962	8.983603
6.530365	475.572619	8.988621
6.461314	481.744156	8.993639
6.507672	467.924477	8.998656
6.839929	471.832458	9.003674
6.484421	479.602453	9.008691
6.565123	475.566740	9.013709
6.638245	473.456132	9.018727
6.603340	468.679862	9.023744
6.715269	468.635846	9.028762
6.704553	473.414934	9.033779
6.682983	473.290164	9.038797
6.665145	472.928574	9.043815
6.836505	472.381417	9.048832
7.052926	476.853683	9.053850
6.715395	468.537680	9.058867
6.941906	467.282207	9.063885
6.786398	464.236067	9.068903
6.695537	462.025956	9.073920
6.411790	450.930998	9.078938
6.737514	477.803347	9.083955
6.653296	471.902303	9.088973
6.590333	471.078768	9.093991
6.445687	472.927232	9.099008
6.731504	470.401581	9.104026
6.424188	468.568164	9.109043
6.700528	466.379689	9.114061
6.517561	480.401150	9.119079
6.683099	479.433738	9.124096
6.929297	474.798522	9.129114
6.373450	479.876665	9.134131
6.656226	479.727685	9.139149
6.679249	482.143110	9.144167
6.378205	476.861910	9.149184
6.614614	472.717254	9.154202
6.560413	493.990887	9.159219
6.946894	490.946577	9.164237
7.154751	503.613843	9.169255
6.885474	486.526429	9.174272
6.737718	473.966459	9.179290
6.703134	479.220340	9.184307
6.879049	486.430397	9.189325
6.736784	479.252105	9.194343
6.937765	495.965423	9.199360
7.213598	495.821729	9.204378
7.076497	492.291070	9.209395
6.760737	471.065703	9.214413
6.642414	482.740804	9.219431
6.809365	485.369295	9.224448
6.870276	489.650896	9.229466
6.904914	498.367183	9.234483
6.891541	494.426622	9.239501
7.105075	502.317381	9.244519
6.841099	498.866859	9.249536
7.399719	489.302187	9.254554
7.102602	481.255420	9.259571
6.889701	477.536003	9.264589
6.732757	468.061148	9.269607
6.783183	486.955389	9.274624
7.355397	484.198291	9.279642
6.893648	486.275432	9.284659
6.860241	475.725409	9.289677
6.857295	477.016905	9.294695
6.786156	477.748526	9.299712
6.938578	494.742724	9.304730
7.013188	505.672452	9.309747
6.951535	499.997154	9.314765
6.880508	506.613675	9.319783
7.004038	503.649876	9.324800
7.282830	503.483842	9.329818
7.045128	502.607860	9.334835
7.442013	490.493328	9.339853
7.154442	486.145825	9.344871
6.650492	477.599234	9.349888
6.903399	490.840642	9.354906
7.230803	501.146708	9.359923
7.296367	495.192415	9.364941
7.552413	500.810953	9.369959
7.132743	476.415334	9.374976
7.229925	470.672902	9.379994
7.150916	474.087284	9.385011
6.720101	471.996663	9.390029
6.810165	471.621665	9.395047
6.844899	480.511730	9.400064
7.145124	490.891001	9.405082
7.291220	504.086991	9.410099
7.083895	494.786227	9.415117
7.188610	497.387469	9.420135
7.144966	502.346236	9.425152
7.291644	497.134300	9.430170
7.274861	497.721663	9.435187
7.413672	486.583805	9.440205
7.173767	475.022528	9.445223
6.934576	472.897694	9.450240
7.024784	480.270406	9.455258
7.124588	496.048460	9.460275
7.010616	494.120508	9.465293
7.411741	499.800554	9.470311
7.373066	491.494702	9.475328
7.176261	489.835810	9.480346
7.098285	499.651823	9.485363
7.172685	498.790692	9.490381
7.189844	503.081341	9.495399
7.095809	506.318125	9.500416
7.306859	503.312616	9.505434
6.993528	498.481639	9.510451
7.254254	504.975898	9.515469
7.422874	496.472808	9.520487
7.131140	511.497722	9.525504
7.383339	506.374336	9.530522
7.289979	506.994899	9.535539
7.519679	502.501184	9.540557
7.175661	502.738052	9.545575
6.981495	507.916311	9.550592
7.113000	499.242632	9.555610
7.329535	507.684815	9.560627
7.154815	502.201129	9.565645
7.282227	493.993447	9.570663
6.841403	510.574501	9.575680
7.017771	496.384399	9.580698
7.460474	512.042686	9.585715
7.160105	521.668728	9.590733
7.484393	524.907436	9.595751
7.233231	528.172113	9.600768
7.654535	519.848645	9.605786
7.654802	524.559197	9.610803
7.500549	513.873932	9.615821
7.863915	503.473867	9.620839
7.536172	497.533573	9.625856
7.687275	495.495819	9.630874
7.062581	498.768052	9.635891
7.169556	504.637333	9.640909
7.640927	498.845884	9.645927
7.202251	506.753326	9.650944
7.343983	498.518854	9.655962
7.353072	499.741035	9.660979
7.551854	519.785357	9.665997
7.537988	518.503304	9.671015
7.550902	528.908113	9.676032
7.455924	527.517110	9.681050
7.386305	522.439533	9.686067
7.624826	526.887866	9.691085
7.645706	530.319513	9.696103
7.366841	537.637859	9.701120
7.617299	527.823622	9.706138
7.589127	534.833391	9.711155
7.566920	528.344115	9.716173
7.690510	535.169225	9.721191
7.314097	521.075113	9.726208
7.381775	527.531593	9.731226
7.665301	531.666568	9.736243
7.676721	538.597324	9.741261
7.643450	533.576295	9.746279
7.538194	536.286649	9.751296
7.671767	528.304283	9.756314
7.569286	529.042101	9.761331
7.634033	538.346269	9.766349
7.661839	526.823914	9.771367
7.214060	538.006816	9.776384
7.437566	521.865912	9.781402
7.481841	530.959520	9.786419
7.402696	536.490292	9.791437
7.846221	528.916408	9.796455
7.766566	535.221017	9.801472
7.503883	531.085291	9.806490
7.630504	525.669807	9.811507
7.567519	530.935315	9.816525
7.437242	533.315998	9.821543
7.690106	526.867216	9.826560
8.010463	531.920793	9.831578
7.679840	527.793999	9.836595
7.144262	530.200712	9.841613
7.640545	528.411067	9.846631
7.782755	528.055745	9.851648
8.000702	525.755324	9.856666
7.977711	521.728961	9.861683
7.603872	521.897958	9.866701
8.041789	526.645010	9.871719
7.881610	526.213779	9.876736
7.641716	523.878050	9.881754
7.432787	530.390348	9.886771
7.131666	531.596971	9.891789
7.642530	544.360154	9.896807
8.153591	555.234498	9.901824
8.095396	558.339952	9.906842
8.206159	536.800906	9.911859
7.751463	534.880766	9.916877
7.686477	521.508643	9.921895
7.669916	534.826372	9.926912
8.248019	533.984658	9.931930
7.692424	528.478252	9.936947
7.936280	536.315371	9.941965
8.117714	525.605993	9.946983
7.883528	530.233479	9.952000
7.972698	529.939527	9.957018
8.301265	527.334130	9.962035
8.052291	524.731822	9.967053
8.159343	518.374990	9.972071
7.893657	532.810606	9.977088
7.669249	526.130549	9.982106
7.995296	528.296814	9.987123
7.856289	521.599021	9.992141
7.985359	514.704521	9.997159
7.883044	524.112426	10.002176
7.754217	523.660040	10.007194
7.929865	507.376134	10.012211
7.777468	522.877659	10.017229
7.933534	522.880042	10.022247
7.731617	533.427049	10.027264
8.071549	548.972939	10.032282
8.176128	550.187518	10.037299
7.999752	563.782011	10.042317
8.140354	551.523429	10.047335
8.288960	552.950555	10.052352
8.124861	541.569131	10.057370
8.271401	532.423487	10.062387
7.684074	527.195757	10.067405
8.028341	524.701324	10.072423
7.995016	535.375808	10.077440
8.223387	553.929557	10.082458
8.461929	547.192817	10.087475
7.984146	538.507601	10.092493
7.719703	530.984663	10.097511
7.854408	525.748528	10.102528
8.085863	554.605999	10.107546
8.445051	547.350232	10.112563
8.156475	554.403096	10.117581
8.245586	561.207769	10.122599
8.291231	556.435799	10.127616
7.861734	538.004798	10.132634
8.307357	542.229753	10.137651
8.189376	550.518523	10.142669
8.313233	558.215178	10.147687
8.280928	545.992426	10.152704
8.045330	534.277646	10.157722
8.003981	541.176823	10.162739
7.883205	555.931653	10.167757
8.419912	548.661339	10.172775
8.422244	552.473404	10.177792
8.242405	552.193655	10.182810
8.518539	553.189186	10.187827
8.005079	554.265960	10.192845
8.499851	548.075755	10.197863
8.338920	557.706987	10.202880
8.493777	558.266808	10.207898
8.088587	530.729788	10.212915
8.272079	547.812770	10.217933
8.231514	552.568303	10.222951
8.324002	557.442655	10.227968
8.141503	563.105566	10.232986
8.359380	553.901993	10.238003
8.306881	567.497156	10.243021
8.045438	554.790283	10.248039
8.269181	562.828182	10.253056
7.866277	558.598443	10.258074
8.163906	546.781640	10.263091
8.344244	556.852563	10.268109
8.250161	554.744541	10.273127
8.280472	553.129185	10.278144
8.176234	560.033115	10.283162
8.211203	547.853506	10.288179
8.234887	559.147612	10.293197
8.307100	563.831652	10.298215
8.636690	565.731410	10.303232
8.537137	567.448582	10.308250
8.663045	562.796723	10.313267
8.413015	555.420576	10.318285
7.956646	559.542133	10.323303
8.473595	572.010651	10.328320
8.409804	586.145065	10.333338
8.916218	576.020561	10.338355
8.613114	568.118432	10.343373
8.272936	563.808389	10.348391
8.559929	569.065145	10.353408
8.300493	576.260604	10.358426
8.887121	577.801920	10.363443
8.414390	577.394293	10.368461
8.646122	573.966076	10.373479
8.952361	558.985497	10.378496
8.250125	559.283481	10.383514
8.424064	552.920241	10.388531
7.862928	566.004720	10.393549
8.610308	582.101372	10.398567
8.781915	574.489795	10.403584
8.310366	591.730910	10.408602
8.552031	587.911898	10.413619
8.722406	591.726748	10.418637
8.681968	588.959857	10.423655
8.906008	585.078230	10.428672
8.423170	596.159726	10.433690
8.872249	579.217749	10.438707
9.068384	590.848735	10.443725
9.018971	576.824226	10.448743
8.684964	574.317139	10.453760
8.373135	561.789093	10.458778
8.426608	562.046304	10.463795
8.369794	574.530670	10.468813
8.906929	576.494154	10.473831
8.971977	593.310086	10.478848
8.658486	599.551627	10.483866
8.900961	585.264242	10.488883
8.845065	586.161432	10.493901
8.786724	589.806833	10.498919
9.015515	582.231019	10.503936
8.804097	576.262109	10.508954
8.833517	553.051856	10.513971
8.677087	559.686532	10.518989
8.469363	548.121229	10.524007
8.951543	567.385107	10.529024
8.766070	583.606697	10.534042
9.220435	576.502997	10.539059
8.839877	567.090640	10.544077
8.442886	564.733776	10.549095
8.711865	559.363116	10.554112
8.649372	574.398803	10.559130
8.813516	582.238368	10.564147
9.090475	581.348683	10.569165
9.057777	579.601092	10.574183
9.034882	582.120221	10.579200
9.107314	583.286214	10.584218
9.363257	573.769240	10.589235
8.749109	564.240999	10.594253
8.587405	571.855609	10.599271
9.081911	556.830355	10.604288
8.713848	553.343582	10.609306
8.921181	569.039473	10.614323
9.177020	578.479803	10.619341
8.973226	571.475067	10.624359
8.977558	559.508201	10.629376
8.616153	565.054208	10.634394
8.643531	568.201539	10.639411
8.903063	571.727572	10.644429
9.026509	578.453521	10.649447
9.262602	581.166590	10.654464
9.136872	581.436857	10.659482
9.158171	580.093053	10.664499
9.005606	586.287370	10.669517
8.832037	592.121037	10.674535
9.109654	587.685273	10.679552
8.982112	580.504486	10.684570
8.692474	582.791596	10.689587
9.071759	586.195374	10.694605
9.108781	587.796351	10.699623
9.323723	583.359590	10.704640
9.163926	589.677147	10.709658
9.147547	589.652883	10.714675
9.206083	586.380606	10.719693
9.121917	584.541381	10.724711
9.154679	584.311721	10.729728
9.066431	591.205528	10.734746
9.291891	585.492319	10.739763
8.874879	585.743682	10.744781
9.177093	582.598213	10.749799
9.441743	579.964458	10.754816
9.196230	595.060897	10.759834
9.293644	582.595117	10.764851
9.403056	581.586245	10.769869
9.112105	588.411191	10.774887
9.257544	588.581863	10.779904
9.023995	592.881336	10.784922
9.170301	581.860854	10.789939
9.266385	596.584599	10.794957
8.686447	590.354126	10.799975
9.074092	584.278752	10.804992
9.249980	590.257664	10.810010
9.453344	587.112090	10.815027
9.191933	590.924304	10.820045
8.911664	591.124596	10.825063
9.171421	588.255254	10.830080
9.172470	584.769520	10.835098
9.340476	579.747499	10.840115
9.282835	583.287476	10.845133
9.162247	586.601913	10.850151
9.133111	587.106891	10.855168
9.458444	616.490364	10.860186
9.469311	617.886654	10.865203
9.678191	614.031159	10.870221
9.367266	608.097278	10.875239
9.172641	583.056654	10.880256
9.461215	603.127692	10.885274
9.447772	598.336792	10.890291
9.878285	597.420206	10.895309
9.067809	590.589127	10.900327
9.191507	586.735987	10.905344
9.605202	617.035014	10.910362
9.537099	614.757324	10.915379
9.517046	614.563999	10.920397
9.315810	614.197655	10.925415
9.563670	616.290715	10.930432
9.741831	613.409933	10.935450
9.288232	617.790472	10.940467
9.554510	617.150572	10.945485
9.466804	616.213040	10.950503
9.654222	613.328949	10.955520
9.547043	612.895992	10.960538
9.343048	624.677558	10.965555
9.452456	616.346042	10.970573
9.331520	612.538675	10.975591
9.480380	622.506024	10.980608
9.742439	616.469225	10.985626
9.427422	632.031547	10.990643
9.760888	607.666828	10.995661
9.067775	619.313169	11.000679
9.579369	613.450824	11.005696
9.618547	621.663907	11.010714
9.778595	617.865737	11.015731
9.846809	603.116395	11.020749
9.713560	614.779117	11.025767
9.662782	607.602486	11.030784
9.631983	622.735699	11.035802
9.786512	619.333296	11.040819
9.865978	614.622217	11.045837
9.551867	611.922068	11.050855
9.773375	605.186756	11.055872
9.729851	613.467514	11.060890
9.465929	610.886178	11.065907
9.683733	615.179923	11.070925
9.662712	616.452586	11.075943
9.950735	612.504809	11.080960
9.880643	609.097227	11.085978
9.676145	620.365332	11.090995
10.071035	619.887111	11.096013
9.657208	620.728056	11.101031
9.512958	612.730412	11.106048
9.526188	619.469580	11.111066
9.539744	618.065647	11.116083
9.345984	605.097896	11.121101
9.644458	629.289824	11.126119
10.081716	634.085637	11.131136
10.298200	636.238044	11.136154
10.274716	624.991049	11.141171
10.072273	609.244645	11.146189
10.255825	616.997938	11.151207
10.353274	599.380191	11.156224
10.282026	604.097733	11.161242
10.358809	612.375421	11.166259
10.028702	603.637673	11.171277
9.894029	609.809932	11.176295
10.137261	605.531638	11.181312
10.061224	603.802074	11.186330
10.160631	598.833572	11.191347
10.110796	578.437014	11.196365
10.192025	577.429677	11.201383
9.872214	571.255181	11.206400
9.798230	573.428104	11.211418
9.791368	581.609059	11.216435
10.322028	596.257225	11.221453
10.011363	582.918011	11.226471
10.019894	597.093559	11.231488
10.283845	587.873056	11.236506
9.847198	592.696600	11.241523
9.994685	595.501952	11.246541
10.083296	601.473921	11.251559
10.186845	598.515000	11.256576
10.121465	605.176684	11.261594
10.363187	608.922007	11.266611
10.054681	588.169644	11.271629
10.136374	603.984674	11.276647
10.032874	601.802232	11.281664
10.186805	591.657177	11.286682
9.942274	600.165810	11.291699
9.996293	599.277158	11.296717
10.008557	610.984189	11.301735
9.963136	614.492815	11.306752
10.140802	601.527893	11.311770
9.911977	615.874395	11.316787
10.359047	607.399366	11.321805
9.984636	609.702931	11.326823
9.925768	604.267861	11.331840
10.323162	600.314703	11.336858
9.940431	600.564699	11.341875
10.154921	596.814567	11.346893
9.929932	610.449461	11.351911
10.100010	625.870129	11.356928
10.243239	627.798116	11.361946
10.498078	637.482132	11.366963
10.545348	639.809110	11.371981
10.164022	632.512620	11.376999
10.374430	637.178633	11.382016
10.440842	628.664508	11.387034
10.374187	647.136707	11.392051
10.646438	634.582381	11.397069
10.706690	622.974647	11.402087
10.330041	603.812597	11.407104
10.338376	615.099846	11.412122
10.116245	601.459309	11.417139
10.392735	619.765198	11.422157
10.291503	629.124172	11.427175
10.520032	640.431726	11.432192
10.672785	631.116106	11.437210
10.513486	626.480729	11.442227
10.339198	617.786359	11.447245
10.310626	618.073349	11.452263
10.870039	627.716381	11.457280
10.509318	618.198932	11.462298
10.218475	625.493721	11.467315
10.629102	623.161457	11.472333
10.626576	632.421356	11.477351
10.567425	632.832710	11.482368
10.334188	615.624211	11.487386
10.422980	627.375420	11.492403
10.415733	641.557568	11.497421
10.637551	638.177439	11.502439
10.249771	641.615425	11.507456
10.561858	638.174233	11.512474
10.402291	645.734000	11.517491
10.615466	639.197090	11.522509
10.555535	637.603220	11.527527
10.451336	644.764445	11.532544
10.723900	640.658614	11.537562
10.685905	645.024211	11.542579
10.868829	633.654327	11.547597
10.533659	628.124042	11.552615
10.486795	633.499692	11.557632
10.792643	631.225981	11.562650
10.578348	634.074348	11.567667
10.803272	630.767517	11.572685
10.995908	627.626079	11.577703
10.484558	635.373632	11.582720
10.636489	627.941467	11.587738
10.544987	642.633447	11.592755
10.451050	627.873240	11.597773
10.599345	632.642679	11.602791
10.342927	645.458484	11.607808
10.944757	651.700455	11.612826
10.915706	669.282248	11.617843
11.255464	653.872220	11.622861
10.892221	643.712312	11.627879
10.855671	640.789463	11.632896
10.766297	630.269304	11.637914
11.028379	631.211668	11.642931
10.687043	641.715391	11.647949
11.044471	647.650176	11.652967
10.916238	648.206467	11.657984
11.017250	624.872996	11.663002
10.813340	638.433944	11.668019
11.014933	639.886914	11.673037
11.252797	635.139856	11.678055
10.968020	641.527810	11.683072
11.269338	628.590734	11.688090
11.094068	635.088034	11.693107
10.918520	633.719664	11.698125
11.078543	630.597622	11.703143
10.549829	642.028875	11.708160
10.640421	639.900578	11.713178
10.901989	653.412122	11.718195
10.959229	654.971363	11.723213
11.269438	659.794798	11.728231
11.084056	670.458431	11.733248
11.504735	668.512846	11.738266
11.002768	654.394011	11.743283
11.041417	637.277294	11.748301
11.052580	632.488199	11.753319
11.198120	631.872303	11.758336
11.043942	628.718240	11.763354
10.946871	631.771120	11.768371
11.562946	650.849869	11.773389
11.257275	638.225468	11.778407
11.182741	634.856804	11.783424
11.569351	626.851030	11.788442
11.038683	634.229578	11.793459
11.081573	625.984698	11.798477
11.213496	624.648879	11.803495
10.872763	635.195013	11.808512
11.254254	630.803187	11.813530
11.012065	637.034467	11.818547
10.992654	650.209473	11.823565
11.253655	655.657178	11.828583
11.507770	662.297670	11.833600
11.836974	655.868033	11.838618
11.410870	643.756127	11.843635
11.606139	641.406313	11.848653
11.442097	631.846915	11.853671
11.298896	628.948881	11.858688
11.321966	632.251259	11.863706
11.271782	635.327644	11.868723
11.179592	635.765945	11.873741
11.525056	625.730360	11.878759
11.366332	634.562518	11.883776
11.398478	628.574952	11.888794
11.441443	625.950873	11.893811
11.186674	634.672430	11.898829
11.310093	624.871374	11.903847
11.126891	633.188350	11.908864
11.267750	655.279913	11.913882
11.441271	653.695464	11.918899
11.399721	657.073150	11.923917
11.642799	654.625237	11.928935
11.336817	670.833683	11.933952
11.338260	661.971508	11.938970
11.486001	662.481930	11.943987
11.582196	670.984162	11.949005
11.775551	666.118517	11.954023
11.280924	662.865140	11.959040
11.473232	659.584195	11.964058
11.606784	663.110324	11.969075
11.452142	664.164077	11.974093
11.397533	657.691549	11.979111
11.235506	667.704301	11.984128
11.586561	674.374155	11.989146
11.555532	671.691112	11.994163
11.261264	669.513993	11.999181
11.658482	659.776846	12.004199
11.183479	658.020093	12.009216
11.496478	663.714650	12.014234
11.770068	681.319771	12.019251
11.616068	681.081982	12.024269
11.706015	693.315689	12.029287
11.697287	697.314063	12.034304
11.993813	689.090963	12.039322
11.941735	685.475267	12.044339
11.788654	676.516336	12.049357
11.818617	655.352534	12.054375
11.734330	667.078018	12.059392
11.853604	664.831573	12.064410
11.422615	668.407051	12.069427
11.523138	674.814042	12.074445
12.056513	696.189686	12.079463
12.083596	702.016026	12.084480
11.721162	692.222065	12.089498
11.977107	695.452682	12.094515
11.426444	685.643952	12.099533
11.894889	688.445183	12.104551
11.776826	693.986614	12.109568
11.859547	694.861951	12.114586
12.206215	693.520548	12.119603
11.572469	706.343021	12.124621
11.730984	696.266619	12.129639
12.011547	694.065207	12.134656
12.030862	692.540240	12.139674
12.015655	703.168328	12.144691
12.058984	695.851220	12.149709
11.931061	692.749666	12.154727
11.971708	699.055998	12.159744
11.712368	691.120352	12.164762
11.853242	693.113497	12.169779
11.820735	692.988181	12.174797
12.044351	690.709824	12.179815
11.847635	692.733098	12.184832
11.730079	688.582459	12.189850
12.176298	690.645118	12.194867
11.930591	698.381224	12.199885
12.353891	687.051262	12.204903
12.101839	697.708280	12.209920
12.142597	682.814224	12.214938
12.220959	673.723723	12.219955
12.151007	683.487144	12.224973
12.115777	684.618681	12.229991
12.080569	688.904110	12.235008
11.925395	689.169824	12.240026
11.938999	688.013299	12.245043
12.212930	705.101697	12.250061
12.671963	711.969942	12.255079
12.265705	694.641699	12.260096
12.087033	698.962195	12.265114
12.306913	694.059655	12.270131
12.015527	689.745207	12.275149
12.469120	698.799225	12.280167
12.080678	694.630818	12.285184
12.515199	715.374543	12.290202
12.553134	702.527243	12.295219
12.111590	697.873407	12.300237
12.336453	696.574296	12.305255
12.284067	702.668156	12.310272
12.497290	713.907251	12.315290
12.452405	689.834012	12.320307
12.575676	696.191171	12.325325
12.296989	690.799102	12.330343
12.228201	684.778885	12.335360
12.450311	700.398051	12.340378
12.526621	705.569999	12.345395
12.416471	714.735835	12.350413
12.275574	707.708969	12.355431
12.448773	716.811965	12.360448
12.550133	715.577668	12.365466
12.805001	707.377820	12.370483
12.339960	716.334554	12.375501
12.771497	707.184347	12.380519
12.516182	695.698491	12.385536
12.322128	692.411880	12.390554
12.541294	710.580960	12.395571
12.677514	714.845973	12.400589
12.803758	704.589509	12.405607
12.620223	701.298983	12.410624
12.233532	683.323453	12.415642
12.699420	690.958602	12.420659
12.649890	711.208213	12.425677
12.535549	701.867067	12.430695
12.579318	713.322699	12.435712
12.400710	708.940094	12.440730
12.454324	714.402410	12.445747
12.821334	718.252517	12.450765
12.819429	713.505526	12.455783
12.742444	710.343143	12.460800
12.377999	712.836391	12.465818
12.660094	712.457815	12.470835
12.466390	729.355876	12.475853
12.864465	719.917544	12.480871
12.993840	708.103979	12.485888
12.969433	714.826218	12.490906
13.012729	706.603273	12.495923
13.130179	715.088021	12.500941
13.082526	714.328261	12.505959
12.986843	717.826564	12.510976
12.830821	717.145442	12.515994
13.085270	703.844075	12.521011
12.834807	692.017087	12.526029
12.934595	703.681297	12.531047
13.092656	689.831634	12.536064
12.570513	696.078368	12.541082
13.054366	698.484157	12.546099
12.937931	714.622761	12.551117
12.872615	704.933136	12.556135
13.131826	694.933495	12.561152
12.871823	712.220284	12.566170
13.168663	704.160104	12.571187
12.744067	704.098973	12.576205
12.978267	706.819072	12.581223
12.905000	714.594236	12.586240
13.003016	714.285623	12.591258
12.844575	703.884169	12.596275
12.863142	712.734932	12.601293
12.817671	713.449701	12.606311
12.918407	717.622981	12.611328
12.966473	720.018535	12.616346
13.034382	714.337370	12.621363
13.340493	709.439586	12.626381
12.970692	705.704857	12.631399
13.280318	708.548630	12.636416
12.780929	713.140925	12.641434
13.221463	710.117311	12.646451
13.338566	718.491694	12.651469
13.137674	707.081817	12.656487
13.432654	711.084239	12.661504
12.900619	708.096696	12.666522
13.151071	706.906511	12.671539
13.356352	714.885359	12.676557
13.394023	718.690016	12.681575
13.189363	709.483948	12.686592
13.175090	715.191586	12.691610
13.130678	703.148269	12.696627
13.292687	719.327795	12.701645
13.394857	714.954619	12.706663
13.300339	706.171158	12.711680
13.089518	716.179061	12.716698
13.220692	721.397600	12.721715
13.568291	735.859807	12.726733
13.537172	740.003832	12.731751
13.507014	729.945185	12.736768
13.344118	724.699791	12.741786
12.960688	726.956057	12.746803
13.030325	738.734352	12.751821
13.312106	738.832368	12.756839
13.195759	737.311837	12.761856
13.466550	732.392359	12.766874
13.582717	736.130237	12.771891
13.522586	736.749813	12.776909
13.676030	740.093533	12.781927
13.883705	732.654217	12.786944
13.487560	742.701403	12.791962
13.711669	729.482610	12.796979
13.732642	746.159194	12.801997
13.576422	741.952373	12.807015
13.782043	734.438010	12.812032
13.583399	736.193519	12.817050
13.878355	739.594814	12.822067
13.916531	739.767373	12.827085
13.558925	733.805377	12.832103
13.838196	742.488818	12.837120
13.445329	742.152747	12.842138
13.702013	736.937800	12.847155
13.591526	734.503960	12.852173
13.548026	732.550879	12.857191
13.846588	733.356684	12.862208
13.595321	732.305790	12.867226
13.656545	735.479811	12.872243
13.765742	733.207671	12.877261
13.675800	735.972990	12.882279
13.813215	744.483962	12.887296
13.716209	746.162150	12.892314
13.903288	727.863462	12.897331
13.587105	735.303055	12.902349
13.295784	739.491510	12.907367
13.792012	734.941224	12.912384
13.797942	738.718488	12.917402
13.617799	731.880010	12.922419
13.566166	738.107215	12.927437
13.609161	761.251537	12.932455
13.764521	763.605644	12.937472
13.933496	771.782077	12.942490
14.084486	774.065263	12.947507
14.115101	764.341548	12.952525
13.858742	762.401207	12.957543
13.999191	751.656165	12.962560
13.909008	769.127965	12.967578
13.982568	764.764451	12.972595
14.449036	761.329853	12.977613
14.344782	765.066385	12.982631
14.498180	754.778212	12.987648
14.407503	744.635330	12.992666
14.185825	737.949215	12.997683
14.115832	727.060441	13.002701
13.978556	731.116408	13.007719
13.998044	723.911903	13.012736
13.954622	729.807842	13.017754
14.102333	738.652114	13.022771
14.609166	743.531864	13.027789
14.021060	741.683868	13.032807
14.254831	734.539798	13.037824
14.358409	730.902156	13.042842
14.297496	717.728779	13.047859
14.215815	721.680233	13.052877
14.125666	733.045941	13.057895
14.441897	722.378388	13.062912
14.316109	742.807435	13.067930
14.263750	725.596109	13.072947
14.150975	739.374855	13.077965
13.827961	742.825128	13.082983
14.381210	755.131278	13.088000
14.374813	756.873142	13.093018
14.504757	755.990561	13.098035
14.674287	775.116127	13.103053
14.283230	774.584099	13.108071
14.564720	763.336113	13.113088
14.321001	765.825641	13.118106
14.274715	763.313807	13.123123
14.305891	777.916042	13.128141
13.833687	770.951497	13.133159
14.351937	763.629234	13.138176
14.343544	765.207662	13.143194
14.105707	761.653924	13.148211
13.931492	760.492196	13.153229
13.944236	775.934441	13.158247
14.727386	782.804748	13.163264
14.570436	793.088569	13.168282
14.502796	790.106888	13.173299
14.702012	783.694080	13.178317
14.567161	801.602051	13.183335
14.595937	791.797330	13.188352
14.669596	792.383254	13.193370
14.875251	793.741672	13.198387
15.508023	789.136592	13.203405
14.630594	791.294082	13.208423
14.624707	762.305533	13.213440
14.810179	769.388356	13.218458
14.369584	760.100221	13.223475
14.855840	769.070511	13.228493
14.847192	779.958370	13.233511
14.968339	783.482258	13.238528
14.847901	763.619202	13.243546
14.705607	762.211044	13.248563
14.689829	757.770655	13.253581
14.602789	775.897405	13.258599
15.091970	782.666190	13.263616
15.141775	781.472148	13.268634
14.916331	779.214877	13.273651
14.876497	756.728969	13.278669
14.855074	757.654491	13.283687
15.089683	755.935084	13.288704
15.091138	762.349523	13.293722
14.665097	755.229685	13.298739
14.995725	754.618648	13.303757
14.662714	765.881646	13.308775
14.784032	780.938356	13.313792
14.923685	784.465074	13.318810
14.853110	788.160584	13.323827
15.458089	787.105351	13.328845
15.197565	795.933656	13.333863
15.229664	787.468058	13.338880
15.154228	778.770355	13.343898
15.264681	774.277683	13.348915
15.176621	756.026858	13.353933
15.053117	759.611088	13.358951
14.934819	764.229813	13.363968
15.405847	762.494337	13.368986
14.895376	768.573424	13.374003
15.412131	762.564507	13.379021
14.959272	783.967000	13.384039
14.889464	782.676704	13.389056
15.624988	783.636640	13.394074
15.428116	787.801930	13.399091
15.390712	763.864527	13.404109
15.274928	770.411834	13.409127
15.428889	766.600860	13.414144
15.027257	760.100738	13.419162
14.978168	768.525997	13.424179
15.103569	783.770207	13.429197
15.278081	786.425641	13.434215
15.366204	784.535119	13.439232
15.496100	787.869378	13.444250
15.362598	793.535843	13.449267
15.932842	777.551003	13.454285
15.674343	791.596912	13.459303
15.087573	771.784782	13.464320
15.510607	779.670191	13.469338
15.231357	779.904958	13.474355
15.606565	779.309737	13.479373
15.133589	787.531268	13.484391
15.194499	781.620943	13.489408
15.670683	779.085451	13.494426
15.237917	786.614716	13.499443
15.582099	783.952158	13.504461
15.393549	803.233136	13.509479
15.343008	794.101197	13.514496
15.510372	790.378929	13.519514
15.455807	792.124472	13.524531
15.754226	793.789891	13.529549
15.521262	790.497916	13.534567
15.465496	783.546426	13.539584
15.652070	780.355379	13.544602
15.599262	793.778167	13.549619
15.548693	780.865400	13.554637
15.631885	785.808688	13.559655
15.623409	782.095570	13.564672
15.728498	785.093622	13.569690
15.792078	807.962368	13.574707
15.830764	802.900947	13.579725
15.795235	799.703507	13.584743
15.907210	810.432766	13.589760
15.964125	792.729613	13.594778
15.615057	785.935526	13.599795
15.996859	786.823161	13.604813
15.837772	795.243688	13.609831
15.586436	801.303731	13.614848
16.238694	809.243766	13.619866
16.059309	818.780596	13.624883
16.048468	804.946897	13.629901
16.022277	795.568801	13.634919
15.895494	782.131532	13.639936
15.798770	782.106647	13.644954
15.814563	796.434310	13.649971
16.086155	798.274648	13.654989
16.112682	810.679413	13.660007
15.984480	809.908825	13.665024
16.254134	800.345146	13.670042
15.892774	814.724096	13.675059
16.098081	802.590182	13.680077
16.158311	804.720950	13.685095
15.920022	805.991554	13.690112
16.147614	808.532074	13.695130
15.788674	816.693724	13.700147
16.437784	817.613305	13.705165
16.122244	814.512597	13.710183
16.046398	815.040109	13.715200
16.592138	812.284403	13.720218
16.400361	817.014563	13.725235
16.272198	805.348447	13.730253
16.262310	808.873059	13.735271
16.160287	819.744578	13.740288
16.382985	805.800019	13.745306
16.231523	805.853321	13.750323
16.128317	805.449814	13.755341
16.314863	817.600050	13.760359
16.396064	810.901354	13.765376
16.643964	813.903822	13.770394
16.512225	812.436626	13.775411
16.261290	800.678919	13.780429
16.118839	804.606640	13.785447
15.813808	805.980457	13.790464
16.387572	806.971021	13.795482
16.066813	821.657381	13.800499
16.374463	807.425884	13.805517
16.417760	805.893771	13.810535
16.452668	810.062665	13.815552
16.814133	806.711254	13.820570
16.776328	814.611273	13.825587
16.517049	809.759600	13.830605
16.714457	812.781483	13.835623
16.372014	812.838577	13.840640
16.333505	810.969297	13.845658
16.299906	817.277585	13.850675
16.835208	825.240021	13.855693
16.984709	830.419726	13.860711
16.664014	819.193644	13.865728
16.719411	804.746614	13.870746
16.678459	817.415732	13.875763
16.662798	813.115652	13.880781
16.885512	811.257674	13.885799
16.458766	809.979265	13.890816
16.723046	804.734688	13.895834
16.652670	822.150307	13.900851
16.861979	821.799377	13.905869
16.827462	820.575452	13.910887
16.947414	833.241853	13.915904
17.054624	825.696758	13.920922
16.958568	826.888806	13.925939
16.670723	805.725656	13.930957
17.079565	826.514741	13.935975
16.979677	826.183118	13.940992
16.815388	817.626530	13.946010
16.640025	821.068617	13.951027
16.966878	829.688297	13.956045
16.755377	830.202532	13.961063
17.207094	822.041554	13.966080
17.390238	833.293019	13.971098
16.799565	828.946391	13.976115
17.181422	830.710143	13.981133
17.211114	830.035350	13.986151
16.976099	827.934573	13.991168
16.997062	823.594941	13.996186
16.862408	828.773847	14.001203
16.953850	823.131248	14.006221
17.211285	827.622782	14.011239
17.257176	818.974768	14.016256
17.480710	819.061011	14.021274
17.264298	824.149180	14.026291
17.209553	822.341058	14.031309
17.277302	828.697068	14.036327
17.258205	824.822725	14.041344
17.086685	823.078300	14.046362
17.064471	821.059863	14.051379
16.970882	829.986024	14.056397
17.120942	819.341299	14.061415
16.912600	826.225055	14.066432
17.136363	816.402869	14.071450
17.250077	831.191226	14.076467
17.316114	850.337433	14.081485
17.727731	842.068354	14.086503
17.270313	835.631798	14.091520
17.502135	838.139535	14.096538
17.367007	845.630381	14.101555
17.549767	840.254075	14.106573
17.849352	840.157807	14.111591
17.398507	833.004263	14.116608
17.340592	826.758969	14.121626
17.685688	835.783861	14.126643
17.720981	837.138712	14.131661
18.075258	817.912778	14.136679
17.604659	822.842225	14.141696
17.708816	823.748059	14.146714
17.412395	831.510769	14.151731
17.252717	823.297090	14.156749
17.824270	812.349062	14.161767
17.482377	815.073601	14.166784
17.668639	827.018591	14.171802
17.799367	826.225437	14.176819
17.664149	838.632108	14.181837
17.903245	832.987797	14.186855
17.432610	841.796724	14.191872
17.638823	838.491778	14.196890
17.710426	852.073258	14.201907
17.648768	852.773007	14.206925
18.001191	848.784549	14.211943
17.705394	848.590205	14.216960
17.543417	847.045359	14.221978
18.033856	836.943222	14.226995
17.789856	851.322973	14.232013
17.984219	844.939685	14.237031
17.931506	849.295583	14.242048
18.061667	847.769106	14.247066
17.976370	838.712795	14.252083
17.617772	854.000711	14.257101
18.145131	836.400013	14.262119
18.002896	847.009158	14.267136
18.163127	844.219497	14.272154
18.495378	843.389305	14.277171
18.056317	851.202502	14.282189
18.278283	842.194719	14.287207
17.922487	852.279755	14.292224
18.165380	845.663218	14.297242
17.858421	847.720188	14.302259
17.889582	853.742352	14.307277
17.842231	844.237634	14.312295
18.078071	849.900207	14.317312
18.364120	856.292184	14.322330
18.578144	846.571198	14.327347
18.242375	847.663729	14.332365
18.062456	843.347638	14.337383
18.104876	846.331906	14.342400
18.114403	847.847329	14.347418
18.110255	842.993001	14.352435
18.207960	859.730572	14.357453
18.451624	865.331224	14.362471
18.248875	867.560628	14.367488
18.342751	868.429790	14.372506
18.487788	876.870281	14.377523
18.328649	880.584864	14.382541
18.728457	866.628134	14.387559
18.413102	875.668735	14.392576
18.880207	870.012889	14.397594
19.099701	869.531337	14.402611
18.480611	848.957008	14.407629
18.698446	840.472122	14.412647
18.435932	837.331889	14.417664
18.578690	828.829766	14.422682
18.579233	835.670737	14.427699
18.308247	830.068297	14.432717
18.912157	852.321549	14.437735
18.579806	844.727858	14.442752
18.638047	850.192800	14.447770
19.155081	844.415680	14.452787
18.887881	847.735250	14.457805
18.733049	828.353190	14.462823
18.623034	834.122254	14.467840
18.423197	841.500633	14.472858
18.564094	846.972503	14.477875
18.652363	869.402226	14.482893
19.066639	859.657003	14.487911
19.017866	869.196169	14.492928
18.460083	859.306626	14.497946
18.963774	860.997772	14.502963
18.530236	865.222102	14.507981
18.808494	857.924922	14.512999
18.995491	864.614844	14.518016
18.950456	872.314927	14.523034
18.832235	860.561099	14.528051
18.909007	860.893375	14.533069
18.562777	861.263282	14.538087
18.572667	869.876616	14.543104
18.613238	865.466395	14.548122
18.945203	863.157603	14.553139
18.601425	868.416553	14.558157
19.124636	891.522394	14.563175
19.060271	900.147693	14.568192
19.227497	898.870153	14.573210
19.602483	885.558831	14.578227
19.173551	892.999917	14.583245
19.599178	879.123919	14.588263
19.363658	874.598570	14.593280
19.105084	856.880266	14.598298
19.451580	859.008537	14.603315
19.367856	860.315852	14.608333
19.262421	857.234147	14.613351
19.273387	849.875499	14.618368
19.159410	851.448849	14.623386
19.319736	851.385766	14.628403
19.266529	858.081753	14.633421
19.221121	858.699674	14.638439
19.112688	876.730892	14.643456
19.346300	883.858716	14.648474
19.613171	879.476227	14.653491
19.128985	888.733467	14.658509
19.427406	882.437586	14.663527
19.702620	875.930224	14.668544
19.443757	886.057828	14.673562
19.691493	885.490877	14.678579
19.432688	896.166869	14.683597
19.654742	879.060737	14.688615
19.963603	895.509329	14.693632
19.828362	890.102008	14.698650
20.229195	883.839495	14.703667
19.527626	874.136822	14.708685
19.626764	852.373888	14.713703
19.888961	846.149392	14.718720
19.189079	857.796642	14.723738
19.194333	865.147833	14.728755
19.431178	885.862837	14.733773
19.839572	873.240417	14.738791
19.778684	882.652480	14.743808
19.481954	882.911017	14.748826
19.555876	887.562787	14.753843
19.778632	890.425364	14.758861
19.764832	889.680243	14.763879
20.055663	890.423370	14.768896
19.570501	881.718517	14.773914
20.089092	882.190731	14.778931
19.952431	893.275526	14.783949
19.669356	897.064645	14.788967
19.958438	885.479306	14.793984
20.088799	895.443017	14.799002
19.993526	882.699199	14.804019
20.002311	884.383242	14.809037
19.891618	888.946413	14.814055
20.359498	896.463231	14.819072
20.457225	898.509241	14.824090
20.024458	896.460613	14.829107
20.145144	894.951847	14.834125
19.976042	885.077994	14.839143
20.103735	887.293814	14.844160
19.751716	889.419692	14.849178
20.345614	898.167062	14.854195
20.078107	908.961431	14.859213
20.339341	923.956642	14.864231
20.644325	913.774853	14.869248
20.458877	908.271152	14.874266
20.251125	888.121679	14.879283
20.221696	893.209500	14.884301
20.611701	899.529496	14.889319
20.748345	882.446218	14.894336
19.917026	888.000368	14.899354
20.217517	886.218032	14.904371
20.818121	899.147490	14.909389
20.089990	896.863720	14.914407
20.285578	886.715091	14.919424
20.565938	907.150073	14.924442
20.455191	903.509433	14.929459
20.847580	905.900145	14.934477
20.640909	911.837853	14.939495
20.620886	905.223260	14.944512
20.707290	916.458386	14.949530
20.396354	901.907596	14.954547
20.860991	898.085896	14.959565
20.673862	903.096788	14.964583
20.790007	901.456894	14.969600
20.723292	895.476405	14.974618
20.979004	890.158031	14.979635
20.708987	879.896255	14.984653
20.766289	882.640671	14.989671
20.683270	874.276043	14.994688
20.255587	885.238347	14.999706
20.958061	892.010311	15.004723
21.197283	896.379507	15.009741
20.899339	901.341498	15.014759
20.924303	895.720551	15.019776
20.842474	904.354266	15.024794
20.833727	902.324919	15.029811
20.864644	899.794129	15.034829
21.111952	914.220421	15.039847
21.421521	896.775335	15.044864
20.854064	897.069028	15.049882
21.160614	895.670305	15.054899
20.614655	887.931793	15.059917
20.585150	897.277235	15.064935
20.911606	892.486439	15.069952
20.921290	910.653567	15.074970
20.677084	900.483544	15.079987
21.073186	906.808829	15.085005
20.928191	896.100698	15.090023
21.081991	906.564426	15.095040
20.945053	903.090335	15.100058
20.964622	909.466787	15.105075
21.184996	930.602673	15.110093
21.228302	927.147040	15.115111
21.931279	924.241174	15.120128
21.280033	916.679192	15.125146
21.705379	908.972919	15.130163
21.149029	900.085804	15.135181
21.185326	898.645785	15.140199
21.436584	907.406019	15.145216
21.158960	935.438438	15.150234
21.093573	931.269024	15.155251
21.508337	923.980225	15.160269
20.940457	921.090717	15.165287
21.028771	926.564072	15.170304
21.302478	920.750207	15.175322
21.248882	915.607243	15.180339
21.352522	924.629015	15.185357
21.214558	924.302537	15.190375
21.443889	943.657532	15.195392
21.446280	950.249049	15.200410
21.899732	952.543404	15.205427
21.999885	951.871854	15.210445
21.778194	952.837563	15.215463
22.172594	925.097848	15.220480
21.742289	921.542993	15.225498
21.898651	908.366801	15.230515
22.163866	917.015279	15.235533
21.644279	919.667407	15.240551
22.043155	913.507564	15.245568
21.883597	921.039315	15.250586
21.897841	918.276662	15.255603
22.049979	919.786498	15.260621
21.738998	915.179984	15.265639
22.439228	908.470479	15.270656
22.187556	915.026654	15.275674
21.905518	918.512868	15.280691
22.194388	907.574753	15.285709
21.786694	923.301186	15.290727
22.228042	904.098860	15.295744
21.873833	914.954884	15.300762
21.863162	912.016857	15.305779
21.781571	910.091343	15.310797
21.915947	907.600045	15.315815
22.041760	908.204075	15.320832
22.150115	909.446007	15.325850
22.062611	908.831633	15.330867
22.027939	905.608636	15.335885
22.073037	907.724809	15.340903
22.183183	926.648832	15.345920
22.311618	935.072825	15.350938
22.259422	936.093034	15.355955
22.588105	931.758521	15.360973
22.568726	934.683397	15.365991
22.353333	916.865726	15.371008
22.215601	915.866416	15.376026
22.394896	930.726837	15.381043
22.821341	935.381836	15.386061
22.481882	926.437792	15.391079
22.516737	902.643863	15.396096
22.274033	909.315073	15.401114
22.258213	917.046147	15.406131
22.259634	930.843679	15.411149
22.219581	946.609812	15.416167
22.391807	938.080685	15.421184
22.111478	937.701890	15.426202
22.477958	940.473269	15.431219
22.714638	929.576882	15.436237
22.566355	940.739622	15.441255
22.629579	931.963277	15.446272
22.425672	942.632932	15.451290
22.080520	941.359058	15.456307
22.646847	944.088955	15.461325
23.084326	965.809634	15.466343
23.090148	955.729506	15.471360
23.078802	961.462338	15.476378
22.878032	950.168986	15.481395
23.514357	941.179278	15.486413
23.113377	937.485694	15.491431
23.212596	929.306089	15.496448
23.141290	932.830898	15.501466
22.803184	923.746482	15.506483
23.205390	921.468525	15.511501
22.907617	925.847853	15.516519
23.173430	926.899453	15.521536
23.255878	924.372298	15.526554
23.221579	926.002093	15.531571
23.036961	919.236515	15.536589
22.687816	924.329851	15.541607
22.927303	922.564736	15.546624
23.131797	919.323244	15.551642
22.829071	927.702367	15.556659
22.923182	923.436764	15.561677
22.746771	941.843114	15.566695
23.452934	940.810621	15.571712
23.603336	950.370666	15.576730
23.404455	945.137673	15.581747
23.479186	927.213898	15.586765
23.215649	931.348970	15.591783
23.209109	925.338784	15.596800
23.323536	934.271766	15.601818
23.626008	943.838814	15.606835
23.802495	944.152157	15.611853
23.309324	930.355601	15.616871
23.263071	928.746633	15.621888
23.502242	933.197339	15.626906
23.476853	953.196222	15.631923
23.716934	952.126240	15.636941
23.818063	956.032214	15.641959
23.538754	941.676117	15.646976
23.820901	941.884108	15.651994
23.770363	944.853533	15.657011
23.472640	930.990635	15.662029
23.742913	934.209081	15.667047
23.647621	938.700026	15.672064
23.784976	939.665897	15.677082
23.714236	949.979978	15.682099
24.152889	941.880161	15.687117
23.903182	935.575368	15.692135
23.468928	935.129248	15.697152
23.629847	937.359631	15.702170
23.394114	955.138099	15.707187
24.011431	954.872690	15.712205
24.015046	953.234960	15.717223
23.756531	959.320271	15.722240
23.685162	944.135169	15.727258
23.707376	962.121152	15.732275
23.872419	954.279784	15.737293
23.763485	956.493214	15.742311
23.839988	949.907044	15.747328
23.931255	960.151295	15.752346
24.028439	972.584207	15.757363
24.079616	979.194004	15.762381
24.033388	969.897671	15.767399
23.954723	978.515155	15.772416
24.371340	975.758444	15.777434
24.024352	969.292650	15.782451
24.619579	973.181068	15.787469
25.027100	969.549543	15.792487
24.289173	958.496637	15.797504
24.625622	938.894798	15.802522
24.429584	947.199115	15.807539
24.453658	947.388586	15.812557
24.266468	944.517684	15.817575
24.191316	940.801438	15.822592
24.327319	946.046809	15.827610
24.366371	970.390259	15.832627
24.883894	959.436149	15.837645
24.718332	971.919030	15.842663
24.445149	950.509163	15.847680
24.708205	938.532464	15.852698
24.478735	946.819111	15.857715
24.670250	939.981559	15.862733
24.666211	946.752873	15.867751
24.334657	944.628757	15.872768
24.363520	951.903630	15.877786
24.362135	970.588779	15.882803
24.661995	969.138016	15.887821
24.506249	971.208843	15.892839
24.454140	972.416037	15.897856
24.869297	966.138120	15.902874
24.744892	970.120162	15.907891
24.506962	967.960405	15.912909
24.811082	979.494017	15.917927
24.358109	974.582758	15.922944
24.829088	980.289758	15.927962
24.790903	993.225080	15.932979
25.151543	1001.985297	15.937997
25.196392	1008.941021	15.943015
25.090070	998.910211	15.948032
25.465720	1000.225828	15.953050
25.177482	993.339652	15.958067
25.029038	970.643348	15.963085
25.522850	977.770486	15.968103
24.989894	971.979658	15.973120
24.768873	969.377352	15.978138
25.021210	986.071643	15.983155
24.999612	990.447210	15.988173
25.570429	989.575391	15.993191
25.234350	993.665846	15.998208
25.211534	993.513524	16.003226
25.290795	999.959222	16.008243
25.421598	992.688456	16.013261
25.140589	997.794505	16.018279
25.481991	998.417427	16.023296
25.388190	985.987434	16.028314
25.597964	1002.157745	16.033331
25.386793	989.727967	16.038349
25.524805	997.985844	16.043367
25.535198	999.463345	16.048384
25.518262	991.357340	16.053402
25.393236	997.555117	16.058419
25.416125	994.760306	16.063437
25.354503	996.995404	16.068455
25.337575	993.021057	16.073472
25.496359	1001.356187	16.078490
25.177941	999.404674	16.083507
25.720289	1021.271379	16.088525
25.793868	1010.830760	16.093543
25.492231	1030.300885	16.098560
26.103313	1014.316101	16.103578
26.092360	1021.684234	16.108595
26.251776	1018.547846	16.113613
26.338463	1016.610097	16.118631
25.988674	1006.097337	16.123648
25.661155	989.249740	16.128666
25.664771	1000.676630	16.133683
25.741396	1006.337380	16.138701
26.191693	1021.714232	16.143719
25.942409	1019.863031	16.148736
26.183457	1021.157323	16.153754
26.086047	1015.787762	16.158771
26.107157	1018.875600	16.163789
26.247277	1013.424043	16.168807
26.191693	1017.026569	16.173824
26.080022	1010.000022	16.178842
26.038392	1018.594051	16.183859
25.991539	1015.979322	16.188877
26.127713	1026.066161	16.193895
25.958030	1012.283872	16.198912
26.146822	1003.517717	16.203930
26.403394	1008.062792	16.208947
26.298635	1010.960143	16.213965
26.340829	1003.136020	16.218983
26.246229	1016.774008	16.224000
26.325904	1012.713131	16.229018
26.325804	1019.892067	16.234035
26.354346	1017.455742	16.239053
26.794542	1028.699466	16.244071
26.530034	1031.110408	16.249088
26.440173	1038.843613	16.254106
26.698117	1040.352410	16.259123
26.702554	1036.194983	16.264141
26.883758	1039.247162	16.269159
26.565257	1032.635670	16.274176
26.728600	1026.735390	16.279194
26.748003	1035.277947	16.284211
26.309039	1036.220722	16.289229
26.575878	1040.825120	16.294247
26.852835	1043.486208	16.299264
27.130985	1041.152479	16.304282
27.356898	1040.203345	16.309299
27.181083	1037.304158	16.314317
27.095864	1019.518666	16.319335
26.942524	1009.973984	16.324352
27.076935	998.512295	16.329370
26.795175	1005.071146	16.334387
27.069093	1017.435746	16.339405
27.338266	1003.845863	16.344423
27.228716	1002.847768	16.349440
27.099400	993.233753	16.354458
26.993335	1010.221091	16.359475
26.788703	1005.090209	16.364493
27.256192	1019.601258	16.369511
27.062465	1040.653374	16.374528
27.349709	1031.872020	16.379546
27.423143	1037.904945	16.384563
27.399661	1032.386484	16.389581
27.571891	1021.628690	16.394599
27.661443	1035.430170	16.399616
27.179639	1007.900108	16.404634
27.118963	1026.227877	16.409651
27.052319	1023.641633	16.414669
27.052599	1028.013181	16.419687
27.162100	1039.315814	16.424704
27.282105	1031.516144	16.429722
27.544804	1029.010191	16.434739
27.582113	1039.424478	16.439757
27.736312	1036.225178	16.444775
27.603417	1028.847444	16.449792
27.623821	1032.048388	16.454810
27.709982	1029.635160	16.459827
27.336121	1027.862927	16.464845
27.681914	1031.400320	16.469863
27.890525	1044.874950	16.474880
27.753160	1035.664194	16.479898
27.715322	1030.226855	16.484915
27.512102	1051.956906	16.489933
27.860470	1051.273623	16.494951
27.818673	1072.549731	16.499968
27.806187	1056.744526	16.504986
27.897781	1055.342543	16.510003
27.957986	1073.771924	16.515021
28.006748	1052.808774	16.520039
27.884303	1067.841519	16.525056
28.061701	1054.990430	16.530074
28.065047	1055.035324	16.535091
27.896656	1064.151208	16.540109
27.924435	1061.596111	16.545127
27.982066	1068.944993	16.550144
28.084602	1060.206528	16.555162
28.193408	1053.758638	16.560179
27.645323	1066.099672	16.565197
28.239716	1059.477375	16.570215
28.005777	1085.364334	16.575232
28.310231	1077.917035	16.580250
28.117393	1083.597797	16.585267
28.268459	1087.696675	16.590285
28.338843	1081.780725	16.595303
28.814330	1085.453652	16.600320
28.442459	1087.673796	16.605338
28.697065	1083.410607	16.610355
28.511845	1081.371987	16.615373
28.959530	1085.738871	16.620391
28.954348	1087.870118	16.625408
28.526913	1078.985092	16.630426
29.026873	1078.406134	16.635443
28.582776	1069.588447	16.640461
28.853266	1070.579441	16.645479
28.488663	1070.392198	16.650496
28.739186	1073.589941	16.655514
28.870996	1086.787230	16.660531
29.103434	1078.504699	16.665549
28.900837	1074.112788	16.670567
28.682807	1069.837611	16.675584
28.638645	1076.848709	16.680602
28.937072	1086.503522	16.685619
28.907539	1096.208126	16.690637
28.887084	1087.377888	16.695655
29.039627	1095.614900	16.700672
28.850790	1085.670579	16.705690
28.999526	1091.069781	16.710707
28.993943	1088.389522	16.715725
28.881227	1083.899603	16.720743
29.128502	1087.556921	16.725760
28.807187	1080.422673	16.730778
29.388979	1087.481699	16.735795
28.838483	1086.259264	16.740813
28.980647	1083.450518	16.745831
28.678719	1098.253688	16.750848
29.004739	1112.311983	16.755866
29.223291	1110.089720	16.760883
29.195570	1117.687839	16.765901
29.352113	1110.620997	16.770919
29.224831	1112.265873	16.775936
29.128714	1116.088534	16.780954
29.329191	1116.394744	16.785971
29.832617	1135.107601	16.790989
30.025129	1117.525037	16.796007
29.952241	1111.649422	16.801024
29.890194	1110.701690	16.806042
29.892222	1101.269704	16.811059
29.792593	1105.952747	16.816077
29.946589	1106.888699	16.821095
29.848231	1097.854485	16.826112
29.765189	1106.407022	16.831130
29.956454	1107.924153	16.836147
29.727610	1096.766062	16.841165
29.571586	1107.857771	16.846183
30.107194	1104.581680	16.851200
29.821022	1110.807073	16.856218
30.182972	1106.443756	16.861235
29.831376	1109.492776	16.866253
29.939572	1107.795130	16.871271
29.721315	1100.676026	16.876288
29.633190	1109.600652	16.881306
30.185333	1098.481249	16.886323
29.742750	1113.181046	16.891341
30.022558	1115.991666	16.896359
30.038703	1131.384097	16.901376
30.302221	1137.842533	16.906394
30.405321	1124.743512	16.911411
30.584337	1133.665875	16.916429
30.055987	1109.081814	16.921447
30.641141	1123.163975	16.926464
30.363698	1110.424656	16.931482
30.639389	1110.231774	16.936499
30.416295	1099.922684	16.941517
30.390490	1094.736460	16.946535
30.434557	1097.461067	16.951552
30.298164	1114.184282	16.956570
30.538360	1115.823196	16.961587
30.548899	1126.641577	16.966605
30.739843	1133.744721	16.971623
30.670501	1126.958318	16.976640
30.316247	1141.042701	16.981658
30.846859	1129.086343	16.986675
30.717738	1135.746645	16.991693
30.662128	1126.957659	16.996711
30.737489	1130.073509	17.001728
30.558219	1120.929113	17.006746
30.997012	1122.842092	17.011763
30.665818	1132.582684	17.016781
30.894847	1137.755574	17.021799
31.135490	1126.606433	17.026816
31.236935	1119.841645	17.031834
31.234509	1122.576346	17.036851
30.988114	1135.140506	17.041869
30.842632	1129.619847	17.046887
31.271686	1120.793222	17.051904
30.593040	1124.417050	17.056922
31.137572	1129.296960	17.061939
31.041185	1126.835320	17.066957
30.838827	1125.582971	17.071975
31.427945	1126.332830	17.076992
31.022060	1130.680973	17.082010
31.155081	1135.034033	17.087027
31.188889	1139.918520	17.092045
31.298234	1141.899642	17.097063
31.637814	1142.432328	17.102080
31.149286	1140.689769	17.107098
31.558317	1139.253522	17.112115
31.382166	1139.086922	17.117133
31.450263	1144.605052	17.122151
32.117243	1132.560282	17.127168
31.562454	1153.763502	17.132186
32.043019	1137.007803	17.137203
31.865331	1142.038855	17.142221
31.492233	1138.777575	17.147239
31.710388	1139.074941	17.152256
31.542789	1142.840596	17.157274
31.697680	1131.906482	17.162291
31.623670	1141.433870	17.167309
31.752736	1145.725781	17.172327
31.999860	1138.462777	17.177344
31.677825	1134.643037	17.182362
31.734665	1141.281094	17.187379
31.913768	1144.017123	17.192397
31.215199	1142.766146	17.197415
31.633378	1138.944237	17.202432
31.767369	1158.720054	17.207450
32.437664	1146.433789	17.212467
32.310506	1171.472079	17.217485
32.745022	1153.418168	17.222503
32.506560	1135.792651	17.227520
31.972405	1136.248519	17.232538
32.276272	1138.306755	17.237555
31.982993	1136.810866	17.242573
31.945737	1136.862902	17.247591
32.273945	1133.911026	17.252608
32.193375	1154.016185	17.257626
32.528906	1156.542367	17.262643
32.233210	1158.706555	17.267661
32.407445	1155.753889	17.272679
32.693263	1151.376443	17.277696
32.507156	1161.830307	17.282714
32.732753	1154.996445	17.287731
32.869421	1153.190130	17.292749
32.490215	1160.454187	17.297767
32.999100	1158.799383	17.302784
32.724479	1152.615564	17.307802
32.874391	1155.600136	17.312819
32.731494	1151.897461	17.317837
32.871829	1151.227099	17.322855
32.816330	1154.696972	17.327872
32.685361	1160.650143	17.332890
32.753296	1151.434722	17.337907
33.226370	1149.858308	17.342925
32.855216	1156.715138	17.347943
32.857065	1155.203265	17.352960
32.489281	1153.767393	17.357978
32.734000	1145.689469	17.362995
32.798350	1148.917384	17.368013
32.493557	1154.027437	17.373031
33.201190	1161.982863	17.378048
33.060236	1183.381898	17.383066
33.054543	1188.517049	17.388083
33.408665	1178.177321	17.393101
33.445130	1176.486472	17.398119
33.400821	1172.244988	17.403136
33.181325	1185.799950	17.408154
33.132163	1181.262433	17.413171
33.170325	1178.274114	17.418189
33.343874	1178.912346	17.423207
33.446921	1179.601663	17.428224
33.515521	1184.038669	17.433242
33.094171	1180.578322	17.438259
33.573701	1181.651503	17.443277
33.179512	1182.614007	17.448295
33.563729	1180.537814	17.453312
33.326733	1187.460939	17.458330
33.924991	1204.653461	17.463347
34.025702	1211.431889	17.468365
33.818338	1212.022412	17.473383
34.148045	1194.694112	17.478400
34.118627	1189.244688	17.483418
34.125920	1176.296974	17.488435
33.983314	1169.921135	17.493453
33.894283	1171.610444	17.498471
33.886813	1169.876507	17.503488
33.859554	1170.716216	17.508506
34.059277	1175.360549	17.513523
34.382294	1167.532580	17.518541
33.768387	1168.979220	17.523559
34.028029	1181.637256	17.528576
34.255291	1194.912864	17.533594
34.355562	1202.996423	17.538611
34.510431	1209.946944	17.543629
34.091513	1204.072902	17.548647
34.471315	1206.776766	17.553664
34.356593	1205.001597	17.558682
34.315358	1203.751594	17.563699
34.338679	1207.315067	17.568717
34.215219	1199.658135	17.573735
34.447272	1202.167666	17.578752
34.307762	1206.079842	17.583770
34.077064	1202.503554	17.588787
34.264100	1207.246852	17.593805
34.007911	1200.860353	17.598823
34.519591	1203.265144	17.603840
34.591825	1210.483719	17.608858
34.587404	1221.978641	17.613875
34.766508	1222.167938	17.618893
34.541845	1226.019472	17.623911
34.868314	1229.854993	17.628928
34.734816	1219.238817	17.633946
34.899507	1226.606199	17.638963
35.019858	1215.739575	17.643981
34.956712	1234.620734	17.648999
35.044725	1231.636717	17.654016
34.941286	1234.120522	17.659034
34.942275	1230.087232	17.664051
35.156124	1219.385767	17.669069
35.037421	1226.191615	17.674087
35.326426	1221.135695	17.679104
35.357684	1216.498978	17.684122
34.976193	1223.074102	17.689139
35.523636	1215.597376	17.694157
35.758086	1222.446490	17.699175
35.823344	1212.190181	17.704192
35.755897	1220.056754	17.709210
35.298937	1213.811094	17.714227
35.455330	1210.485809	17.719245
35.594401	1220.339232	17.724263
35.669951	1212.016960	17.729280
35.679571	1211.161637	17.734298
35.381256	1208.361120	17.739315
35.566470	1209.494638	17.744333
35.526125	1219.644799	17.749351
35.426379	1216.212090	17.754368
35.691125	1211.899544	17.759386
35.489071	1217.507481	17.764403
35.961499	1206.404795	17.769421
35.701531	1211.477102	17.774439
35.973544	1210.495100	17.779456
35.677374	1212.412927	17.784474
35.823766	1220.735277	17.789491
35.490822	1211.759275	17.794509
35.757693	1238.009689	17.799527
35.870118	1237.878586	17.804544
36.435084	1241.464243	17.809562
35.963752	1255.716608	17.814579
35.838564	1241.431856	17.819597
35.667541	1244.644977	17.824615
35.952606	1239.186179	17.829632
36.045589	1243.014448	17.834650
36.061369	1244.937122	17.839667
36.200237	1246.812568	17.844685
36.090686	1266.203821	17.849703
36.468739	1264.233756	17.854720
36.663633	1259.307241	17.859738
36.924122	1257.621667	17.864755
37.052461	1257.283202	17.869773
36.807854	1245.771731	17.874791
36.868788	1244.935041	17.879808
36.839720	1235.130204	17.884826
36.885418	1241.761496	17.889843
36.991449	1235.064790	17.894861
36.463766	1235.573913	17.899879
36.583450	1227.313192	17.904896
36.627779	1232.193598	17.909914
36.821894	1233.546101	17.914931
36.978537	1234.625316	17.919949
37.039278	1232.487137	17.924967
36.552631	1227.233374	17.929984
36.922619	1233.023000	17.935002
37.141634	1248.919604	17.940019
37.172327	1247.369858	17.945037
36.806910	1250.939292	17.950055
37.406514	1250.811073	17.955072
37.239694	1248.927633	17.960090
37.049256	1268.168559	17.965107
37.288014	1261.163179	17.970125
37.429277	1263.872448	17.975143
37.045251	1261.533788	17.980160
37.314619	1254.044995	17.985178
36.727679	1260.193670	17.990195
37.181537	1254.603667	17.995213
37.076557	1259.101432	18.000231
36.894290	1253.530545	18.005248
37.555912	1270.033109	18.010266
37.398980	1291.095197	18.015283
37.750592	1281.384141	18.020301
37.555206	1285.809936	18.025319
37.561402	1286.955103	18.030336
37.985753	1288.465795	18.035354
37.860928	1281.278717	18.040371
37.972531	1281.438291	18.045389
37.759747	1287.684232	18.050407
37.808557	1276.851109	18.055424
37.891219	1281.977512	18.060442
37.863832	1289.704395	18.065459
38.031947	1283.601264	18.070477
37.770553	1275.531410	18.075495
37.573357	1278.874867	18.080512
37.802879	1271.840702	18.085530
37.557959	1280.881247	18.090547
38.244273	1303.321254	18.095565
38.188053	1308.201073	18.100583
38.328487	1304.837477	18.105600
38.891330	1292.848080	18.110618
38.938140	1283.770338	18.115635
38.948358	1269.897290	18.120653
38.700469	1256.662405	18.125671
39.002756	1257.307589	18.130688
38.686209	1252.481433	18.135706
38.906833	1268.493928	18.140723
39.173540	1252.292920	18.145741
38.899809	1256.219149	18.150759
38.612368	1239.485084	18.155776
38.815069	1228.788221	18.160794
38.671170	1227.871408	18.165811
38.846705	1223.276454	18.170829
38.585642	1237.011985	18.175847
38.841454	1250.385647	18.180864
38.869422	1263.801126	18.185882
38.504314	1265.303269	18.190899
39.031330	1262.339585	18.195917
38.857842	1263.544535	18.200935
38.669109	1270.637228	18.205952
38.940635	1254.464943	18.210970
38.685691	1262.755598	18.215987
38.898768	1266.935160	18.221005
38.898611	1268.144765	18.226023
39.124327	1285.046160	18.231040
39.295353	1286.327705	18.236058
39.574038	1299.787369	18.241075
39.403674	1290.839809	18.246093
39.340978	1285.770672	18.251111
38.975412	1287.645713	18.256128
39.658186	1286.135611	18.261146
39.759394	1294.080485	18.266163
39.651135	1280.276724	18.271181
39.406993	1291.959173	18.276199
39.287554	1280.434746	18.281216
39.580352	1277.290705	18.286234
39.687461	1288.086457	18.291251
39.739305	1276.164287	18.296269
39.691604	1281.202124	18.301287
39.869804	1279.901471	18.306304
39.990277	1284.154300	18.311322
39.704512	1287.189656	18.316339
39.644558	1279.558349	18.321357
39.969489	1287.331789	18.326375
39.538945	1282.158442	18.331392
39.622393	1275.578460	18.336410
39.831541	1288.899283	18.341427
40.234813	1300.683972	18.346445
40.306811	1307.946331	18.351463
40.452546	1310.257242	18.356480
40.545772	1294.918459	18.361498
40.398795	1281.769532	18.366515
40.364169	1283.251787	18.371533
40.425944	1278.912330	18.376551
40.277034	1279.529360	18.381568
40.291697	1283.462386	18.386586
40.232900	1309.457218	18.391603
40.256860	1305.998811	18.396621
40.443356	1307.108501	18.401639
40.501211	1305.201492	18.406656
40.529121	1302.131785	18.411674
40.515258	1314.866097	18.416691
40.606329	1307.572261	18.421709
40.308756	1311.921349	18.426727
40.084532	1314.778378	18.431744
40.875267	1318.622189	18.436762
41.371277	1320.894570	18.441779
41.432605	1323.288407	18.446797
41.339821	1311.852042	18.451815
40.926604	1304.008186	18.456832
41.213284	1294.520505	18.461850
40.979879	1300.768698	18.466867
40.809358	1293.969117	18.471885
41.031518	1308.295632	18.476903
41.092628	1321.218269	18.481920
41.305340	1326.593141	18.486938
41.491038	1331.782748	18.491955
41.136244	1324.342937	18.496973
41.445624	1328.591545	18.501991
41.046626	1333.623616	18.507008
41.332349	1321.763323	18.512026
41.592852	1331.860012	18.517043
41.170392	1322.083103	18.522061
41.542607	1320.369505	18.527079
41.603619	1328.978142	18.532096
41.757611	1325.475678	18.537114
41.747896	1326.186107	18.542131
41.694673	1316.004538	18.547149
41.660996	1318.281492	18.552167
41.183967	1323.613526	18.557184
41.701122	1343.252671	18.562202
41.708336	1348.911697	18.567219
41.609479	1363.888055	18.572237
41.887194	1354.600247	18.577255
41.787147	1356.399671	18.582272
42.090439	1347.243831	18.587290
42.367692	1363.517082	18.592307
42.377332	1353.708099	18.597325
42.347560	1353.891171	18.602343
42.206360	1359.397708	18.607360
42.397355	1344.770161	18.612378
42.248844	1354.023458	18.617395
41.920959	1353.936796	18.622413
42.434673	1339.270184	18.627431
42.265730	1340.276753	18.632448
42.273103	1342.826406	18.637466
42.348503	1354.177850	18.642483
42.435414	1366.256499	18.647501
42.812256	1369.968333	18.652519
42.834932	1373.235504	18.657536
42.729540	1374.207892	18.662554
42.810194	1376.962687	18.667571
42.428238	1361.907532	18.672589
43.037235	1364.151298	18.677607
42.884245	1363.297797	18.682624
42.892214	1360.481778	18.687642
42.567193	1356.055017	18.692659
42.451811	1361.326563	18.697677
42.547741	1366.433860	18.702695
42.597308	1378.998238	18.707712
43.215151	1390.151288	18.712730
43.328673	1385.496518	18.717747
43.228045	1398.056348	18.722765
43.387511	1382.117116	18.727783
43.287899	1398.555793	18.732800
43.474923	1391.540843	18.737818
43.775346	1395.978748	18.742835
43.543487	1394.461602	18.747853
43.824948	1389.064372	18.752871
43.497164	1394.876334	18.757888
43.407819	1379.821346	18.762906
43.471993	1383.004459	18.767923
43.541069	1397.564368	18.772941
43.688404	1387.574609	18.777959
43.426364	1404.375317	18.782976
43.651007	1389.127193	18.787994
43.661012	1388.326519	18.793011
43.832798	1391.649617	18.798029
43.903250	1381.814762	18.803047
43.468970	1393.761559	18.808064
43.635007	1398.784776	18.813082
44.270661	1402.719343	18.818099
44.284970	1418.025754	18.823117
44.330861	1404.287597	18.828135
43.932954	1402.558290	18.833152
44.018030	1404.988350	18.838170
44.081520	1418.768127	18.843187
44.054315	1420.162156	18.848205
44.581312	1420.121200	18.853223
44.315137	1420.872288	18.858240
44.377315	1430.904763	18.863258
44.655956	1423.726544	18.868275
44.372473	1424.566727	18.873293
44.519543	1419.760705	18.878311
45.009090	1421.960949	18.883328
44.859087	1414.665399	18.888346
44.743084	1416.096232	18.893363
44.783384	1425.172131	18.898381
44.875743	1417.204820	18.903399
44.563884	1425.339670	18.908416
44.680732	1417.560016	18.913434
44.925052	1427.322853	18.918451
44.577787	1422.487969	18.923469
44.673313	1416.097647	18.928487
44.634042	1424.936384	18.933504
45.064783	1436.552049	18.938522
45.348318	1452.240507	18.943539
45.261682	1453.797562	18.948557
45.555628	1437.775294	18.953575
45.644275	1442.763358	18.958592
45.194568	1420.388502	18.963610
45.461096	1413.078052	18.968627
45.470118	1431.616365	18.973645
45.737580	1422.892015	18.978663
45.552416	1407.991504	18.983680
45.452587	1398.301471	18.988698
45.615719	1409.003747	18.993715
45.263602	1434.467242	18.998733
45.795317	1431.745653	19.003751
45.844091	1433.719165	19.008768
46.064348	1429.902917	19.013786
45.796410	1433.003447	19.018803
45.660033	1427.374084	19.023821
45.959132	1428.724904	19.028839
46.112775	1427.348795	19.033856
46.047700	1439.266940	19.038874
46.229729	1429.624134	19.043891
45.938113	1432.264439	19.048909
46.336465	1428.576855	19.053927
46.036833	1433.481028	19.058944
46.012791	1425.300387	19.063962
46.185120	1419.200046	19.068979
45.907418	1426.257204	19.073997
46.217607	1421.643356	19.079015
46.189471	1434.008495	19.084032
46.103264	1430.771907	19.089050
46.154340	1436.269743	19.094067
45.889799	1440.598022	19.099085
46.619929	1449.612039	19.104103
46.545446	1447.416779	19.109120
46.502247	1450.412639	19.114138
46.700800	1443.783928	19.119155
46.677957	1457.053693	19.124173
46.618196	1453.907979	19.129191
46.382263	1457.281139	19.134208
46.835675	1469.615877	19.139226
46.977423	1473.196736	19.144243
46.701876	1472.205727	19.149261
46.805565	1476.716510	19.154279
46.905020	1470.429447	19.159296
47.331977	1468.983106	19.164314
47.205481	1469.097611	19.169331
47.103770	1469.270988	19.174349
47.180757	1475.033421	19.179367
47.312899	1478.508006	19.184384
47.074057	1491.387333	19.189402
47.406502	1499.271440	19.194419
47.563314	1496.602702	19.199437
47.711402	1501.414768	19.204455
47.811911	1493.532675	19.209472
47.527862	1499.683856	19.214490
48.022877	1487.238272	19.219507
48.346252	1485.918591	19.224525
47.598276	1486.113160	19.229543
48.160019	1475.198584	19.234560
48.086891	1469.992540	19.239578
47.970508	1464.983840	19.244595
47.698375	1469.653932	19.249613
48.148795	1482.065948	19.254631
48.230066	1480.063295	19.259648
48.302603	1486.833535	19.264666
48.230444	1468.365450	19.269683
48.153982	1465.661081	19.274701
48.166637	1461.164780	19.279719
48.031592	1467.219531	19.284736
47.775925	1479.452448	19.289754
48.052420	1481.590870	19.294771
48.046896	1483.600577	19.299789
48.119502	1491.221574	19.304807
48.590689	1481.093286	19.309824
48.110609	1498.033088	19.314842
48.395591	1505.479034	19.319859
48.635308	1512.662828	19.324877
48.460714	1524.454363	19.329895
48.897503	1520.866272	19.334912
48.713369	1532.448773	19.339930
49.008826	1519.563899	19.344947
49.221196	1525.791636	19.349965
48.668833	1519.332183	19.354983
49.333842	1512.922761	19.360000
48.861770	1522.506699	19.365018
48.781811	1518.406475	19.370035
48.766943	1515.131636	19.375053
48.962923	1520.054250	19.380071
48.764036	1520.522511	19.385088
49.024438	1531.427599	19.390106
49.097465	1544.148445	19.395123
49.303753	1544.609995	19.400141
49.302325	1548.700878	19.405159
49.653409	1541.100337	19.410176
49.428091	1549.102367	19.415194
49.606347	1549.963845	19.420211
49.410904	1543.937177	19.425229
49.640265	1546.733428	19.430247
49.816941	1539.788634	19.435264
50.086456	1548.363133	19.440282
49.725723	1532.044860	19.445299
49.842187	1545.250604	19.450317
49.819580	1556.888558	19.455335
50.207165	1568.570944	19.460352
50.135481	1574.882524	19.465370
50.233110	1568.814618	19.470387
50.552001	1569.833428	19.475405
49.962844	1570.348838	19.480423
50.638511	1569.792238	19.485440
50.581484	1560.907179	19.490458
50.288795	1551.773896	19.495475
50.419121	1545.891112	19.500493
50.338719	1557.442218	19.505511
50.374028	1559.419952	19.510528
50.520892	1571.828950	19.515546
50.745623	1564.429315	19.520563
50.576027	1565.137587	19.525581
50.440056	1569.724056	19.530599
50.578961	1556.897453	19.535616
50.530362	1562.656383	19.540634
50.832746	1565.735771	19.545651
50.779926	1559.401934	19.550669
50.645129	1568.264897	19.555687
51.302070	1567.397242	19.560704
50.520482	1584.395516	19.565722
50.695744	1583.738228	19.570739
50.733724	1591.549672	19.575757
50.750726	1595.767029	19.580775
51.039596	1588.404754	19.585792
51.256773	1594.683294	19.590810
51.429192	1593.872544	19.595827
51.281609	1593.420091	19.600845
51.502294	1611.277782	19.605863
51.855612	1610.181064	19.610880
51.787960	1593.169145	19.615898
51.684118	1583.180062	19.620915
51.704377	1581.505641	19.625933
51.690155	1578.526345	19.630951
51.642012	1584.547408	19.635968
51.371296	1594.714055	19.640986
51.865336	1605.753590	19.646003
51.498119	1618.378771	19.651021
52.183828	1622.696411	19.656039
52.508249	1612.473141	19.661056
52.217579	1608.882315	19.666074
52.132308	1607.728573	19.671091
52.281090	1607.671345	19.676109
52.282642	1597.365922	19.681127
52.653701	1603.496451	19.686144
52.488499	1603.601248	19.691162
52.486984	1601.768242	19.696179
52.662512	1598.161353	19.701197
52.334596	1602.873432	19.706215
52.633711	1591.786680	19.711232
52.600965	1593.923365	19.716250
52.577844	1606.657093	19.721267
52.693855	1599.516846	19.726285
52.228123	1595.017339	19.731303
52.360720	1597.169063	19.736320
52.557262	1599.334962	19.741338
52.794765	1598.407098	19.746355
52.978604	1611.850909	19.751373
52.683314	1628.009758	19.756391
53.327758	1619.951767	19.761408
53.115547	1619.881309	19.766426
53.219527	1612.800141	19.771443
53.468905	1610.456151	19.776461
53.527940	1613.144111	19.781479
53.616455	1612.919344	19.786496
53.930338	1610.060704	19.791514
53.467164	1597.536887	19.796531
53.583475	1582.610116	19.801549
53.353706	1601.810356	19.806567
53.845150	1594.162840	19.811584
53.771748	1609.131267	19.816602
53.724136	1605.103989	19.821619
54.224119	1607.468666	19.826637
53.585640	1615.758686	19.831655
53.897615	1606.865027	19.836672
53.801612	1616.232585	19.841690
53.922935	1611.881564	19.846707
53.778558	1616.769045	19.851725
53.607603	1612.518567	19.856743
54.108626	1613.308295	19.861760
54.101996	1609.025783	19.866778
53.865577	1605.151143	19.871795
54.099300	1616.965041	19.876813
54.049962	1637.229021	19.881831
54.808546	1629.958736	19.886848
54.338079	1640.913326	19.891866
54.403812	1641.419893	19.896883
54.237942	1636.478810	19.901901
54.251798	1638.768777	19.906919
54.432289	1635.293335	19.911936
54.439324	1639.630863	19.916954
54.627397	1639.012783	19.921971
55.165350	1653.021390	19.926989
55.042715	1657.795823	19.932007
55.072608	1649.175003	19.937024
54.975708	1645.877550	19.942042
54.850043	1638.667217	19.947059
55.160583	1646.294808	19.952077
54.913494	1650.934808	19.957095
55.171853	1649.012936	19.962112
55.481450	1652.332873	19.967130
55.432619	1658.759191	19.972147
55.717690	1645.052328	19.977165
55.443301	1653.760590	19.982183
55.812573	1639.977533	19.987200
55.639366	1643.919434	19.992218
55.645100	1649.591021	19.997235
55.793728	1643.394533	20.002253
55.688258	1653.399899	20.007271
55.880534	1648.965028	20.012288
55.590663	1654.036542	20.017306
55.699992	1645.228116	20.022323
55.863369	1651.749082	20.027341
55.866266	1647.375607	20.032359
55.823832	1649.527689	20.037376
55.912813	1649.873702	20.042394
55.985547	1649.656675	20.047411
56.044223	1651.932502	20.052429
55.940688	1653.584903	20.057447
56.303561	1676.594168	20.062464
56.340789	1672.479151	20.067482
56.024826	1670.862963	20.072499
56.791408	1670.613294	20.077517
56.510697	1683.161553	20.082535
56.497674	1681.232026	20.087552
56.539785	1668.125753	20.092570
56.667619	1670.486150	20.097587
56.832509	1664.197188	20.102605
56.725820	1671.266191	20.107623
56.878545	1669.065027	20.112640
57.098407	1668.099146	20.117658
56.765182	1680.523455	20.122675
56.689499	1687.471171	20.127693
56.989440	1690.125799	20.132711
57.051890	1690.827400	20.137728
57.596141	1692.754423	20.142746
57.373032	1699.625073	20.147763
57.575991	1692.715212	20.152781
57.433291	1698.561879	20.157799
57.415060	1695.599368	20.162816
57.519920	1683.364140	20.167834
57.699792	1698.045286	20.172851
57.406673	1690.502921	20.177869
57.341750	1691.027661	20.182887
57.467671	1687.044354	20.187904
57.447095	1697.197842	20.192922
57.509741	1710.989831	20.197939
57.887716	1712.716936	20.202957
57.890919	1726.047956	20.207975
57.987613	1715.347118	20.212992
58.705108	1710.752105	20.218010
58.129705	1716.205343	20.223027
58.305541	1718.833358	20.228045
58.242479	1719.726291	20.233063
58.264415	1717.424417	20.238080
58.443348	1710.260276	20.243098
58.325274	1718.639448	20.248115
58.636469	1717.954839	20.253133
58.372083	1712.137199	20.258151
58.247080	1705.196014	20.263168
58.687720	1711.111481	20.268186
58.484790	1736.813272	20.273203
58.950979	1740.676489	20.278221
58.866809	1736.256043	20.283239
58.950098	1741.404542	20.288256
59.419627	1732.239746	20.293274
58.795564	1742.244351	20.298291
59.192660	1736.042358	20.303309
59.035161	1738.809240	20.308327
58.848215	1739.974730	20.313344
59.316733	1734.891173	20.318362
58.960475	1736.943850	20.323379
59.421913	1733.025635	20.328397
59.037564	1736.838085	20.333415
58.909370	1734.094235	20.338432
59.540167	1741.647782	20.343450
59.184646	1765.214760	20.348467
59.479047	1763.200271	20.353485
59.742570	1757.607473	20.358503
59.614701	1758.195827	20.363520
59.818088	1758.609442	20.368538
59.472313	1764.220988	20.373555
59.921229	1755.689522	20.378573
59.877660	1760.515019	20.383591
59.857111	1759.789875	20.388608
59.717406	1758.546743	20.393626
60.081299	1765.041125	20.398643
60.351505	1765.260959	20.403661
60.759173	1764.402835	20.408679
60.336871	1781.408143	20.413696
60.767912	1765.537555	20.418714
60.448299	1759.238528	20.423731
60.666419	1763.151248	20.428749
60.921290	1767.481873	20.433767
60.864997	1765.448504	20.438784
60.546982	1767.247981	20.443802
60.536197	1773.084168	20.448819
60.935769	1762.180205	20.453837
60.721868	1766.250553	20.458855
60.526701	1762.017050	20.463872
60.749896	1766.528135	20.468890
61.274873	1790.344088	20.473907
61.610385	1791.393616	20.478925
61.202882	1792.029233	20.483943
61.220896	1790.570123	20.488960
61.734541	1792.669175	20.493978
61.290332	1794.729784	20.498995
61.347483	1794.537786	20.504013
61.751943	1790.893592	20.509031
61.638632	1799.065323	20.514048
61.626257	1791.692389	20.519066
61.477314	1803.168455	20.524083
61.726102	1795.998571	20.529101
61.745340	1795.235317	20.534119
61.716818	1796.070151	20.539136
61.687460	1789.564605	20.544154
61.889381	1809.097290	20.549171
62.004186	1811.124049	20.554189
61.951220	1823.174728	20.559207
62.089279	1819.932676	20.564224
62.121184	1825.158640	20.569242
61.984996	1821.134216	20.574259
62.096562	1814.042247	20.579277
62.372295	1809.082045	20.584295
62.006231	1829.807969	20.589312
62.746321	1833.399311	20.594330
62.882350	1838.333172	20.599347
63.082724	1836.942568	20.604365
63.242958	1836.441311	20.609383
63.168942	1834.802611	20.614400
63.700841	1809.253816	20.619418
63.505270	1812.322314	20.624435
63.315462	1796.457241	20.629453
63.288466	1800.079606	20.634471
63.120648	1804.451753	20.639488
63.223861	1797.585588	20.644506
62.930638	1793.690025	20.649523
63.108074	1797.409516	20.654541
63.107217	1798.085817	20.659559
63.058502	1801.462974	20.664576
63.126983	1812.794645	20.669594
63.325023	1828.009902	20.674611
63.676228	1831.426900	20.679629
63.750141	1837.395885	20.684647
63.301466	1841.751727	20.689664
63.638052	1824.922763	20.694682
63.786496	1840.692731	20.699699
63.631285	1840.306499	20.704717
64.061709	1851.840249	20.709735
63.550048	1856.635697	20.714752
63.776436	1868.746283	20.719770
63.609033	1870.893968	20.724787
64.009137	1866.207173	20.729805
64.478105	1865.882951	20.734823
64.606032	1892.020562	20.739840
64.435138	1885.111332	20.744858
64.623237	1887.339700	20.749875
64.926539	1885.879230	20.754893
64.739202	1880.295572	20.759911
64.743681	1895.200150	20.764928
64.814762	1886.973929	20.769946
65.148029	1890.158881	20.774963
64.739352	1894.153365	20.779981
64.682051	1877.707524	20.784999
64.466002	1887.574331	20.790016
64.723385	1885.557712	20.795034
64.734796	1889.322928	20.800051
64.851924	1904.090289	20.805069
65.248015	1906.443934	20.810087
65.162262	1919.398959	20.815104
65.203734	1919.057203	20.820122
65.373227	1912.818557	20.825139
65.382253	1923.065304	20.830157
65.600224	1927.850535	20.835175
65.768168	1942.449250	20.840192
65.955379	1937.098993	20.845210
65.969465	1946.055144	20.850227
65.593935	1955.291015	20.855245
66.031665	1945.881379	20.860263
66.070768	1950.721935	20.865280
66.136973	1942.233108	20.870298
66.365620	1941.683470	20.875315
66.159055	1945.465242	20.880333
66.603377	1946.790007	20.885351
66.192038	1941.424264	20.890368
66.570276	1932.261533	20.895386
66.438071	1938.454578	20.900403
66.247042	1945.473548	20.905421
66.609897	1942.405135	20.910439
66.452936	1959.329924	20.915456
66.729431	1960.237697	20.920474
66.974460	1962.601104	20.925491
67.164500	1970.179985	20.930509
67.110561	1962.664665	20.935527
66.770730	1968.492619	20.940544
67.000942	1959.833611	20.945562
67.313925	1952.000226	20.950579
67.160145	1967.291807	20.955597
67.078868	1966.130680	20.960615
67.122221	1959.433056	20.965632
67.174581	1962.358801	20.970650
67.185293	1965.906828	20.975667
66.901963	1993.235014	20.980685
67.506383	1979.595256	20.985703
67.080430	1993.501378	20.990720
67.348862	1986.863579	20.995738
68.062201	1996.275204	21.000755
67.990749	2004.773948	21.005773
68.074127	2004.375618	21.010791
67.973626	2011.303193	21.015808
68.512986	2015.913383	21.020826
68.468069	2002.058292	21.025843
68.099186	1985.275141	21.030861
68.166181	1985.153552	21.035879
68.608251	2005.518627	21.040896
68.786268	2003.265181	21.045914
68.816831	1998.414171	21.050931
68.894850	1994.978910	21.055949
68.952403	1984.618253	21.060967
68.774574	1974.821135	21.065984
68.698183	1969.444204	21.071002
68.850144	1973.836480	21.076019
68.629658	1983.086758	21.081037
68.687165	1991.283744	21.086055
68.605876	1999.703804	21.091072
68.718071	2002.822764	21.096090
69.146984	2003.277646	21.101107
68.923288	2008.146148	21.106125
69.111033	2019.843586	21.111143
69.315099	2028.172142	21.116160
69.518144	2024.976728	21.121178
69.777719	2016.464384	21.126195
69.573045	2024.705749	21.131213
69.752526	2014.499219	21.136231
69.610549	2015.728515	21.141248
69.714391	2020.666997	21.146266
69.887908	2016.626877	21.151283
69.687153	2024.988064	21.156301
69.926986	2024.710583	21.161319
70.194426	2037.433777	21.166336
70.218659	2042.811091	21.171354
70.398647	2050.006639	21.176371
70.238060	2050.425241	21.181389
70.440634	2046.670446	21.186407
70.850889	2052.767870	21.191424
70.940490	2050.592498	21.196442
70.911853	2052.555726	21.201459
70.528563	2046.436063	21.206477
70.489874	2041.314655	21.211495
70.653709	2041.744695	21.216512
70.377136	2038.743164	21.221530
70.895669	2033.160643	21.226547
70.618967	2045.017967	21.231565
70.543896	2051.027543	21.236583
71.025511	2073.966877	21.241600
71.046416	2070.998184	21.246618
71.221503	2068.407023	21.251635
71.164789	2075.294672	21.256653
71.416328	2067.483646	21.261671
71.471069	2074.454348	21.266688
71.619738	2095.633275	21.271706
71.798779	2088.326421	21.276723
71.972404	2103.253482	21.281741
71.829935	2097.257164	21.286759
71.709792	2089.630735	21.291776
71.433328	2094.430473	21.296794
71.826188	2092.459424	21.301811
71.958670	2090.346213	21.306829
72.227967	2093.885546	21.311847
72.326722	2103.664343	21.316864
72.318570	2094.353525	21.321882
72.331661	2084.734848	21.326899
72.299965	2092.606944	21.331917
72.426813	2092.336035	21.336935
72.235820	2101.522819	21.341952
72.853470	2116.640669	21.346970
73.312195	2110.195212	21.351987
73.532681	2106.403566	21.357005
73.459420	2092.137350	21.362023
73.096686	2074.308969	21.367040
72.880906	2071.958360	21.372058
73.275653	2073.189013	21.377075
73.411789	2074.148467	21.382093
73.332542	2068.952294	21.387111
73.658063	2068.916875	21.392128
73.350383	2062.670858	21.397146
73.808148	2068.202117	21.402163
73.603806	2080.397841	21.407181
73.412437	2073.575395	21.412199
73.648594	2079.832475	21.417216
73.197217	2082.504162	21.422234
74.105710	2093.375562	21.427251
73.540858	2099.339782	21.432269
73.833541	2113.036812	21.437287
74.292533	2100.772322	21.442304
73.917348	2116.789834	21.447322
74.089773	2107.078125	21.452339
74.014838	2104.592290	21.457357
73.930022	2104.962868	21.462375
73.841170	2108.581412	21.467392
74.101623	2129.350069	21.472410
74.308725	2118.423120	21.477427
74.428987	2132.596468	21.482445
74.298845	2124.815381	21.487463
74.597552	2145.965111	21.492480
75.029748	2159.320092	21.497498
75.120502	2151.256606	21.502515
75.159479	2157.887046	21.507533
74.680623	2153.413175	21.512551
75.026811	2148.208476	21.517568
75.022045	2152.256371	21.522586
75.117117	2154.229761	21.527603
75.104580	2157.937604	21.532621
75.622962	2180.020969	21.537639
75.579972	2187.152061	21.542656
75.831455	2175.612172	21.547674
75.945579	2173.583499	21.552691
75.826541	2181.493384	21.557709
75.833296	2170.317407	21.562727
75.968332	2173.583396	21.567744
75.629104	2173.371048	21.572762
75.726222	2164.911607	21.577779
75.985399	2170.403860	21.582797
76.134395	2193.643538	21.587815
76.239396	2197.468080	21.592832
76.212969	2197.675409	21.597850
76.779055	2195.304290	21.602867
76.619138	2197.248409	21.607885
76.474741	2196.080037	21.612903
76.736691	2193.866947	21.617920
76.577447	2193.834139	21.622938
76.877792	2194.654104	21.627955
76.949714	2196.636859	21.632973
76.603434	2201.367128	21.637991
76.650583	2195.934153	21.643008
76.534712	2201.595443	21.648026
76.978112	2212.008384	21.653043
76.966295	2228.334527	21.658061
76.972857	2225.738276	21.663079
77.138985	2219.197698	21.668096
77.226487	2242.205144	21.673114
77.929690	2231.332285	21.678131
78.206826	2234.167575	21.683149
77.900886	2245.994476	21.688167
78.304116	2233.434812	21.693184
77.766477	2228.749423	21.698202
78.049881	2229.101328	21.703219
78.356495	2223.295687	21.708237
78.287300	2225.180242	21.713255
78.163127	2219.827307	21.718272
78.365747	2227.494384	21.723290
78.555442	2227.964621	21.728307
78.389761	2230.031752	21.733325
78.647024	2232.054970	21.738343
78.503292	2231.788476	21.743360
78.508395	2228.217246	21.748378
78.370345	2232.731025	21.753395
78.784667	2226.956695	21.758413
78.300523	2233.030784	21.763431
78.898570	2244.090503	21.768448
78.522554	2261.033521	21.773466
79.135116	2258.710970	21.778483
78.624758	2264.013817	21.783501
78.894355	2263.925880	21.788519
79.095603	2284.830966	21.793536
79.376024	2285.879057	21.798554
79.685434	2286.044353	21.803571
79.911783	2281.031578	21.808589
79.874821	2278.390976	21.813607
80.128787	2284.456591	21.818624
80.054136	2280.580485	21.823642
80.322230	2278.310849	21.828659
80.260854	2274.086073	21.833677
80.186139	2292.941308	21.838695
80.516530	2278.533031	21.843712
80.493592	2290.029855	21.848730
80.290430	2286.079433	21.853747
80.427202	2283.533188	21.858765
80.331984	2293.604192	21.863783
80.357439	2280.554896	21.868800
80.467752	2293.550484	21.873818
80.517831	2307.271075	21.878835
80.823542	2318.462506	21.883853
80.742020	2310.968530	21.888871
80.900872	2307.486300	21.893888
80.853630	2304.480855	21.898906
80.931433	2309.668645	21.903923
81.089471	2315.071062	21.908941
81.206871	2330.401399	21.913959
81.244890	2335.935190	21.918976
81.281422	2335.431642	21.923994
81.331187	2329.225328	21.929011
81.602869	2337.463283	21.934029
81.382350	2333.029892	21.939047
81.981319	2341.434330	21.944064
81.880237	2354.011543	21.949082
81.879245	2345.327752	21.954099
81.986099	2357.509376	21.959117
81.799469	2358.476032	21.964135
82.010355	2356.493854	21.969152
82.048750	2358.907413	21.974170
81.904353	2353.268413	21.979187
82.238058	2359.029459	21.984205
82.609507	2383.479342	21.989223
82.962739	2383.567276	21.994240
82.862120	2389.384371	21.999258
82.934351	2380.701384	22.004275
83.038475	2386.499413	22.009293
82.811154	2377.704000	22.014311
83.486361	2369.434211	22.019328
83.264631	2375.758847	22.024346
83.225207	2367.920434	22.029363
83.509145	2374.809478	22.034381
83.055093	2379.899849	22.039399
83.075338	2365.181213	22.044416
83.517833	2365.835040	22.049434
83.222057	2367.985622	22.054451
83.370362	2374.429869	22.059469
83.531379	2392.218848	22.064487
83.571398	2378.463876	22.069504
83.226307	2406.238104	22.074522
83.379769	2402.318939	22.079539
83.912739	2420.829627	22.084557
83.743194	2427.148761	22.089575
84.310589	2426.340835	22.094592
84.123800	2432.007301	22.099610
84.507009	2425.573479	22.104627
84.610886	2423.777193	22.109645
84.758993	2418.089952	22.114663
84.956415	2418.342368	22.119680
84.780944	2420.567455	22.124698
84.779598	2421.665926	22.129715
85.426145	2433.877214	22.134733
85.275728	2447.875747	22.139751
85.511701	2435.626406	22.144768
85.513640	2411.662396	22.149786
85.423482	2415.654863	22.154803
85.771750	2401.275393	22.159821
85.237202	2408.129212	22.164839
85.305965	2423.831123	22.169856
85.548097	2442.418914	22.174874
85.683550	2442.196965	22.179891
85.863482	2433.880709	22.184909
85.195050	2447.203492	22.189927
85.448510	2440.339635	22.194944
85.785879	2456.181985	22.199962
85.918896	2467.939646	22.204979
86.018665	2461.847808	22.209997
86.303670	2474.140473	22.215015
86.366455	2469.888316	22.220032
86.338180	2469.704995	22.225050
86.366368	2482.802583	22.230067
86.784269	2481.837209	22.235085
86.880361	2490.562713	22.240103
86.865412	2486.128974	22.245120
86.863582	2484.134099	22.250138
87.184806	2488.098376	22.255155
87.329154	2487.790299	22.260173
86.645351	2491.237718	22.265191
87.368078	2487.187703	22.270208
87.359125	2494.072718	22.275226
87.670329	2516.088629	22.280243
87.678625	2514.692486	22.285261
87.761873	2511.955484	22.290279
87.905420	2507.123729	22.295296
87.943064	2491.548109	22.300314
87.883556	2503.935850	22.305331
88.037998	2504.276123	22.310349
87.966106	2509.604217	22.315367
88.438678	2500.411698	22.320384
87.898757	2503.598583	22.325402
87.863038	2508.317490	22.330419
87.822191	2507.415362	22.335437
88.056843	2531.285826	22.340455
87.718590	2526.369561	22.345472
88.338910	2532.109025	22.350490
88.317091	2540.634459	22.355507
88.808996	2561.452242	22.360525
88.841154	2565.347251	22.365543
89.152285	2563.886601	22.370560
89.446445	2563.590635	22.375578
89.026865	2566.481930	22.380595
88.781744	2572.848724	22.385613
89.448342	2563.312884	22.390631
89.379965	2559.168331	22.395648
89.412179	2569.993567	22.400666
89.447174	2584.255517	22.405683
89.832622	2583.375849	22.410701
89.917902	2581.705083	22.415719
89.784627	2579.926931	22.420736
90.022572	2584.466123	22.425754
89.880757	2593.395798	22.430771
90.153366	2570.918129	22.435789
90.191861	2586.572476	22.440807
90.068976	2608.585459	22.445824
90.710702	2605.498529	22.450842
90.894557	2620.577545	22.455859
90.853654	2610.832469	22.460877
90.749575	2616.783696	22.465895
91.142148	2608.620600	22.470912
91.040612	2600.198269	22.475930
90.716686	2612.779260	22.480947
90.971297	2604.183954	22.485965
90.741087	2607.402069	22.490983
90.965472	2612.083687	22.496000
90.994064	2616.281285	22.501018
91.056209	2627.028748	22.506035
91.350586	2625.453549	22.511053
91.316594	2633.930661	22.516071
91.570825	2651.097722	22.521088
91.976258	2648.001625	22.526106
91.914039	2672.465372	22.531123
92.237378	2655.066820	22.536141
92.238509	2661.019870	22.541159
91.986325	2657.994476	22.546176
92.705190	2654.730141	22.551194
92.473203	2658.084790	22.556211
92.829982	2657.292959	22.561229
92.850120	2664.416140	22.566247
92.742136	2654.285708	22.571264
93.023305	2654.552559	22.576282
92.708288	2661.602693	22.581299
92.656529	2652.044444	22.586317
92.785265	2659.457859	22.591335
92.820108	2682.878273	22.596352
93.351896	2681.227784	22.601370
93.411980	2684.577996	22.606387
93.488196	2679.746353	22.611405
93.669888	2671.645831	22.616423
93.441335	2673.940015	22.621440
93.729720	2677.943659	22.626458
93.849335	2677.815289	22.631475
93.967942	2669.333106	22.636493
94.059032	2674.165642	22.641511
93.968374	2689.111991	22.646528
94.192553	2696.024890	22.651546
93.969935	2704.631425	22.656563
94.144955	2696.756421	22.661581
93.971995	2694.524983	22.666599
94.116117	2706.046322	22.671616
94.336247	2711.124368	22.676634
94.444309	2722.763135	22.681651
94.971824	2722.812660	22.686669
94.863168	2720.392569	22.691687
94.453447	2724.266166	22.696704
94.977496	2727.972377	22.701722
95.043738	2735.384008	22.706739
95.475621	2734.309598	22.711757
95.197405	2749.357651	22.716775
95.244680	2761.595953	22.721792
95.241460	2763.938927	22.726810
95.268292	2761.877438	22.731827
95.516433	2756.717969	22.736845
95.600504	2760.072085	22.741863
95.726939	2782.133648	22.746880
95.890007	2776.748927	22.751898
95.839805	2788.104577	22.756915
96.316315	2786.051823	22.761933
96.119262	2779.192212	22.766951
96.241009	2782.532591	22.771968
96.617844	2788.668149	22.776986
96.512148	2808.861126	22.782003
96.518383	2815.689426	22.787021
97.002967	2809.696896	22.792039
96.776175	2799.114038	22.797056
97.060672	2801.363924	22.802074
97.276332	2801.743246	22.807091
97.520920	2796.231578	22.812109
97.619755	2783.594494	22.817127
97.634206	2790.089901	22.822144
97.819367	2787.580418	22.827162
97.593474	2797.313993	22.832179
97.575730	2793.925182	22.837197
98.098707	2785.879307	22.842215
97.955528	2793.039926	22.847232
98.074518	2793.225852	22.852250
97.925461	2804.828666	22.857267
97.880094	2817.785994	22.862285
98.231548	2813.601919	22.867303
98.243221	2817.292115	22.872320
98.443052	2808.177422	22.877338
98.142872	2828.121232	22.882355
98.364358	2837.211550	22.887373
98.868246	2834.816030	22.892391
98.457657	2838.078343	22.897408
98.764493	2833.906402	22.902426
98.832183	2840.081939	22.907443
99.401197	2855.389319	22.912461
99.567025	2856.030484	22.917479
99.409503	2861.965093	22.922496
99.517443	2851.793136	22.927514
99.552305	2868.494106	22.932531
99.486839	2850.367381	22.937549
99.520780	2865.593998	22.942567
99.913064	2854.390469	22.947584
99.998402	2863.161281	22.952602
99.658979	2865.402258	22.957619
99.934706	2878.077913	22.962637
99.910958	2879.001388	22.967655
100.387317	2889.311274	22.972672
100.355976	2888.349272	22.977690
100.328529	2889.139495	22.982707
100.544353	2890.869669	22.987725
100.978577	2907.949225	22.992743
100.889413	2905.004177	22.997760
101.127795	2906.034888	23.002778
101.116241	2904.425853	23.007795
101.147643	2906.601272	23.012813
101.284307	2895.316565	23.017831
101.495078	2911.718645	23.022848
101.554841	2898.979686	23.027866
101.081220	2899.213701	23.032883
101.281051	2893.931893	23.037901
101.644910	2903.483267	23.042919
101.730024	2912.596293	23.047936
101.950137	2920.264744	23.052954
101.829735	2930.852584	23.057971
101.941632	2927.123279	23.062989
102.566327	2933.008241	23.068007
102.386488	2923.013599	23.073024
102.391973	2929.384168	23.078042
102.547974	2936.310080	23.083059
102.448554	2945.076206	23.088077
102.797350	2946.527184	23.093095
102.935390	2948.464400	23.098112
102.767613	2950.481969	23.103130
102.792372	2950.288647	23.108147
102.746647	2956.451974	23.113165
103.132626	2964.377942	23.118183
103.284517	2985.822527	23.123200
103.459973	2979.214330	23.128218
103.523058	2983.125171	23.133235
103.396929	2981.343423	23.138253
103.847891	2975.307990	23.143271
103.654140	2991.808879	23.148288
103.953805	2997.877025	23.153306
104.172828	3000.188219	23.158323
104.490792	2997.345192	23.163341
104.646290	2997.065572	23.168359
104.762190	3002.578389	23.173376
104.800340	2997.080484	23.178394
105.030792	2985.584048	23.183411
104.852828	2994.743991	23.188429
105.059611	2983.717272	23.193447
104.678914	3002.245841	23.198464
104.828205	2985.543218	23.203482
104.913811	3004.115172	23.208499
105.089169	3018.064407	23.213517
105.496280	3017.894558	23.218535
105.422998	3035.201912	23.223552
105.641957	3022.307253	23.228570
105.761128	3024.140519	23.233587
105.419455	3027.859563	23.238605
105.650523	3036.793670	23.243623
105.695531	3050.876810	23.248640
106.080739	3054.242367	23.253658
105.868437	3057.078434	23.258675
105.975690	3060.389784	23.263693
106.300954	3066.259987	23.268711
106.354402	3081.266627	23.273728
106.450837	3075.780270	23.278746
106.817634	3072.289301	23.283763
106.800198	3075.764693	23.288781
107.166891	3090.288543	23.293799
107.380994	3105.480729	23.298816
107.768161	3103.971173	23.303834
107.574128	3080.717102	23.308851
107.303907	3089.999528	23.313869
107.678932	3090.943366	23.318887
107.865450	3094.365970	23.323904
107.854440	3096.075592	23.328922
107.806742	3093.749258	23.333939
107.371712	3099.254445	23.338957
107.968444	3087.914798	23.343975
107.767984	3105.326836	23.348992
108.136207	3115.304422	23.354010
108.288653	3126.986907	23.359027
108.282488	3128.689428	23.364045
108.741422	3123.029023	23.369063
108.737892	3121.057973	23.374080
108.589334	3122.644381	23.379098
108.955384	3117.104935	23.384115
108.900290	3119.286490	23.389133
108.838159	3126.711768	23.394151
108.868240	3143.325238	23.399168
109.083927	3144.642438	23.404186
109.660186	3148.388112	23.409203
109.463799	3143.364207	23.414221
109.552698	3150.255300	23.419239
109.325674	3150.838919	23.424256
109.708746	3166.062538	23.429274
109.977871	3179.839630	23.434291
109.643861	3179.268489	23.439309
109.899461	3179.738043	23.444327
109.820570	3180.033637	23.449344
110.314055	3195.047188	23.454362
110.360760	3198.270982	23.459379
110.530707	3206.397557	23.464397
110.802531	3197.912856	23.469415
110.560538	3205.231041	23.474432
110.653846	3224.255559	23.479450
110.893553	3231.590171	23.484467
110.646923	3236.048653	23.489485
110.922366	3236.429077	23.494503
111.095492	3248.030650	23.499520
111.285648	3252.003914	23.504538
111.398496	3254.814724	23.509555
111.317632	3259.054703	23.514573
111.693590	3267.207709	23.519591
111.847862	3271.346799	23.524608
112.044759	3277.542773	23.529626
112.436826	3267.669423	23.534643
112.457668	3279.470359	23.539661
112.840047	3271.202700	23.544679
112.599625	3271.990536	23.549696
112.565803	3280.205349	23.554714
112.963763	3277.984076	23.559731
112.996920	3303.012541	23.564749
113.138644	3292.047209	23.569767
113.340186	3288.975030	23.574784
113.196667	3293.124633	23.579802
113.319290	3284.633968	23.584819
113.321574	3288.841238	23.589837
113.153779	3297.247630	23.594855
113.413190	3308.214380	23.599872
113.526903	3325.339784	23.604890
114.135740	3326.621195	23.609907
114.048309	3333.793665	23.614925
113.960958	3324.901217	23.619943
114.372538	3341.589701	23.624960
114.629493	3348.626591	23.629978
114.608399	3343.931793	23.634995
114.671462	3346.926501	23.640013
115.003218	3349.044194	23.645031
115.203983	3345.240961	23.650048
115.109430	3346.621941	23.655066
115.063287	3343.530278	23.660083
114.863739	3355.403726	23.665101
115.223821	3337.881370	23.670119
115.386966	3346.436748	23.675136
115.330615	3368.377141	23.680154
115.674923	3363.914554	23.685171
115.269442	3374.361074	23.690189
115.606061	3367.198321	23.695207
116.292409	3375.409656	23.700224
116.278989	3371.203386	23.705242
116.367738	3365.573308	23.710259
116.160274	3362.334023	23.715277
116.209820	3368.590352	23.720295
116.557506	3391.856288	23.725312
116.286490	3396.582279	23.730330
116.965100	3394.199773	23.735347
116.589508	3391.560919	23.740365
116.831518	3401.158838	23.745383
117.067303	3398.506580	23.750400
117.228204	3419.711659	23.755418
117.572778	3409.430717	23.760435
117.512932	3428.056090	23.765453
117.609850	3419.614510	23.770471
117.599240	3414.022583	23.775488
117.491905	3433.493339	23.780506
117.575023	3419.175113	23.785523
117.245115	3443.934578	23.790541
117.741489	3456.518127	23.795559
117.724461	3471.490787	23.800576
117.568723	3480.116949	23.805594
117.913246	3479.162141	23.810611
118.028414	3500.467459	23.815629
118.233418	3509.059676	23.820647
118.467936	3514.707703	23.825664
118.401643	3528.114027	23.830682
119.000780	3527.856746	23.835699
119.373003	3530.854055	23.840717
119.395213	3531.974284	23.845735
119.350891	3533.135493	23.850752
119.478316	3546.712418	23.855770
119.799493	3553.712348	23.860787
119.935615	3561.766375	23.865805
119.888686	3557.629803	23.870823
120.073839	3555.169418	23.875840
119.564236	3569.025866	23.880858
120.335857	3583.899861	23.885875
120.155717	3590.273590	23.890893
120.465060	3594.160987	23.895911
120.837120	3581.466436	23.900928
120.761809	3593.866329	23.905946
121.460307	3601.238665	23.910963
121.396088	3617.878941	23.915981
121.564951	3605.982004	23.920999
121.702591	3599.937373	23.926016
121.842133	3600.261249	23.931034
122.176368	3597.368163	23.936051
122.248903	3581.232054	23.941069
121.909351	3566.698074	23.946087
122.300065	3562.734863	23.951104
122.154535	3564.499178	23.956122
122.462927	3581.630705	23.961139
122.251524	3581.797523	23.966157
122.273081	3593.154827	23.971175
122.600668	3594.278649	23.976192
122.493624	3596.401967	23.981210
122.581087	3598.783151	23.986227
122.709139	3596.108208	23.991245
122.953054	3614.313203	23.996263
123.085811	3624.917322	24.001280
123.078829	3632.640009	24.006298
123.245849	3626.088853	24.011315
123.395889	3619.118034	24.016333
123.377427	3647.743043	24.021351
123.663892	3641.978030	24.026368
123.867878	3654.993050	24.031386
123.714641	3643.240567	24.036403
123.920374	3647.549966	24.041421
123.599516	3660.811284	24.046439
124.419602	3670.842499	24.051456
124.256860	3665.198983	24.056474
124.199398	3671.600002	24.061491
124.189484	3672.603517	24.066509
124.486331	3696.072866	24.071527
124.854889	3704.961279	24.076544
124.682529	3711.976360	24.081562
124.970757	3715.980302	24.086579
125.138514	3727.767399	24.091597
124.936820	3745.744594	24.096615
125.342278	3743.050302	24.101632
125.537529	3744.430013	24.106650
125.766746	3751.427990	24.111667
125.958062	3749.205557	24.116685
125.765558	3766.331538	24.121703
125.998893	3755.291990	24.126720
126.125184	3760.391095	24.131738
126.616027	3775.654890	24.136755
126.583123	3794.592401	24.141773
126.651827	3798.293827	24.146791
127.112997	3787.727088	24.151808
126.696467	3795.739988	24.156826
127.043156	3785.790775	24.161843
126.894601	3796.596108	24.166861
126.819861	3810.041089	24.171879
127.214203	3813.352535	24.176896
127.473209	3828.155239	24.181914
127.838462	3846.206071	24.186931
128.242360	3844.291648	24.191949
128.161895	3843.449182	24.196967
128.475091	3835.143113	24.201984
127.965144	3847.888698	24.207002
128.341215	3839.663923	24.212019
128.720238	3840.362627	24.217037
128.720370	3840.496657	24.222055
129.350427	3835.858090	24.227072
129.316217	3843.061717	24.232090
129.444318	3858.496124	24.237107
129.487261	3856.585771	24.242125
129.458032	3854.966187	24.247143
130.126436	3853.777985	24.252160
129.951173	3852.109038	24.257178
129.876539	3855.506302	24.262195
129.898131	3841.938166	24.267213
130.085726	3852.376614	24.272231
129.944484	3849.226628	24.277248
130.047488	3848.795855	24.282266
129.929740	3847.359901	24.287283
130.220829	3862.029337	24.292301
130.402443	3876.746117	24.297319
130.714893	3876.273450	24.302336
130.708885	3886.666919	24.307354
130.958063	3897.234157	24.312371
131.035586	3898.419245	24.317389
130.774705	3908.163259	24.322407
131.016393	3907.757083	24.327424
131.528826	3925.728818	24.332442
131.371035	3943.825338	24.337459
131.502825	3939.641640	24.342477
131.468364	3941.802950	24.347495
131.920384	3954.685652	24.352512
131.802380	3968.305303	24.357530
132.440591	3968.550651	24.362547
132.745918	3949.217964	24.367565
132.735137	3958.870442	24.372583
132.762918	3946.131221	24.377600
132.785167	3954.849342	24.382618
132.550788	3967.803595	24.387635
133.101399	3970.669758	24.392653
133.076984	3986.311551	24.397671
133.561827	3980.083469	24.402688
133.417078	3993.085061	24.407706
133.376729	3988.541320	24.412723
133.843631	3983.985344	24.417741
133.608573	4007.854226	24.422759
133.722266	4009.088438	24.427776
133.680716	4003.812508	24.432794
133.727589	4005.197606	24.437811
134.436281	4032.284963	24.442829
134.548087	4032.871762	24.447847
134.544116	4030.612047	24.452864
134.588967	4035.698394	24.457882
134.664213	4044.800333	24.462899
134.855136	4043.825343	24.467917
134.835405	4064.488399	24.472935
135.299209	4063.356234	24.477952
135.186356	4062.789649	24.482970
135.174065	4082.065075	24.487987
135.632999	4093.416604	24.493005
135.524542	4087.146897	24.498023
135.766567	4105.693378	24.503040
136.120505	4116.679640	24.508058
136.124532	4111.868216	24.513075
136.653762	4110.154621	24.518093
136.537437	4112.614638	24.523111
136.564432	4132.957376	24.528128
136.827805	4130.322857	24.533146
136.673517	4145.656421	24.538163
137.117225	4131.928899	24.543181
136.858041	4161.411109	24.548199
137.359981	4162.142955	24.553216
137.547694	4151.366261	24.558234
137.458532	4163.376722	24.563251
137.644212	4165.885788	24.568269
138.046399	4185.414166	24.573287
138.340929	4187.558639	24.578304
138.179390	4179.114319	24.583322
138.373074	4194.692513	24.588339
138.353628	4184.625125	24.593357
138.741811	4205.920686	24.598375
138.924864	4205.716401	24.603392
139.293044	4212.992720	24.608410
139.306058	4219.440528	24.613427
139.345272	4213.616773	24.618445
139.171112	4205.796677	24.623463
139.392047	4213.253394	24.628480
139.613201	4225.480880	24.633498
139.681834	4237.271446	24.638515
140.032196	4235.510778	24.643533
139.823151	4245.465318	24.648551
139.931730	4245.205681	24.653568
140.339919	4250.546729	24.658586
140.201380	4269.439760	24.663603
140.378047	4262.967065	24.668621
140.413729	4275.890080	24.673639
140.450686	4289.751624	24.678656
141.001142	4294.804437	24.683674
141.404364	4294.918738	24.688691
141.491408	4282.641123	24.693709
141.868199	4295.696477	24.698727
142.572605	4292.974467	24.703744
142.306372	4282.418022	24.708762
142.115202	4282.186933	24.713779
142.219226	4274.162283	24.718797
142.382466	4275.279604	24.723815
142.512906	4274.111470	24.728832
142.794235	4267.565467	24.733850
142.553664	4271.384945	24.738867
142.741539	4290.030815	24.743885
142.933877	4294.899007	24.748903
142.855336	4300.380018	24.753920
143.001680	4300.948095	24.758938
143.020264	4304.696164	24.763955
143.036216	4314.983495	24.768973
143.026386	4329.573435	24.773991
143.141398	4317.338396	24.779008
143.859848	4337.994912	24.784026
143.595269	4357.138951	24.789043
143.865833	4363.398326	24.794061
143.916363	4364.988000	24.799079
144.173284	4384.584081	24.804096
144.340142	4394.893639	24.809114
144.318971	4398.281348	24.814131
144.644051	4393.062886	24.819149
144.696492	4407.385028	24.824167
145.174693	4416.692313	24.829184
145.328298	4414.872182	24.834202
145.268579	4429.146830	24.839219
145.388660	4434.108975	24.844237
145.754196	4448.604360	24.849255
145.912451	4442.289795	24.854272
146.427126	4438.118730	24.859290
145.844975	4433.888947	24.864307
146.497088	4444.725087	24.869325
146.483301	4461.482308	24.874343
146.697921	4461.620077	24.879360
146.703841	4460.637216	24.884378
146.678678	4476.452879	24.889395
147.070639	4481.211565	24.894413
147.003644	4492.475950	24.899431
147.279635	4494.987388	24.904448
147.349015	4490.661134	24.909466
147.488374	4512.661566	24.914483
147.358978	4514.822979	24.919501
147.616852	4535.534241	24.924519
147.745593	4538.859267	24.929536
148.015186	4549.153430	24.934554
148.006122	4556.840690	24.939571
148.720383	4552.940419	24.944589
148.809834	4564.449771	24.949607
149.053132	4573.444157	24.954624
149.348113	4562.813951	24.959642
149.272942	4572.433798	24.964659
149.233062	4561.750558	24.969677
149.489155	4562.841446	24.974695
149.506774	4579.534508	24.979712
149.731435	4588.383154	24.984730
149.977491	4600.854871	24.989747
150.595930	4590.180347	24.994765
150.788669	4589.192423	24.999783
150.720989	4584.749524	25.004800
150.933705	4576.138055	25.009818
150.898098	4580.986724	25.014835
150.746470	4584.137839	25.019853
150.977425	4592.223892	25.024871
151.109245	4602.050347	25.029888
151.240563	4599.721210	25.034906
151.189681	4606.663344	25.039923
151.502600	4598.680994	25.044941
151.652179	4613.335275	25.049959
151.799991	4626.680182	25.054976
151.914011	4632.222240	25.059994
152.025418	4634.546840	25.065011
151.827935	4635.891877	25.070029
151.832652	4640.718901	25.075047
152.383148	4661.237583	25.080064
152.561600	4662.284677	25.085082
152.250124	4674.804209	25.090099
152.575993	4685.475794	25.095117
152.548123	4690.720921	25.100135
152.998442	4709.298479	25.105152
153.410095	4716.934019	25.110170
153.869314	4725.539004	25.115187
153.472361	4728.667911	25.120205
153.468747	4736.070837	25.125223
153.932076	4754.076889	25.130240
154.148912	4748.637670	25.135258
154.223621	4749.318474	25.140275
154.545892	4773.101810	25.145293
154.808461	4772.845716	25.150311
154.821934	4782.904589	25.155328
155.176719	4768.908562	25.160346
155.044440	4778.617566	25.165363
155.244016	4792.475370	25.170381
155.695135	4796.615548	25.175399
155.650684	4798.119455	25.180416
155.830838	4791.649902	25.185434
155.671787	4805.402713	25.190451
156.013353	4813.352367	25.195469
155.836872	4824.491061	25.200487
155.982801	4828.893813	25.205504
156.780163	4842.499541	25.210522
156.807133	4854.435315	25.215539
156.693688	4856.498042	25.220557
157.314799	4858.078795	25.225575
157.191363	4873.682797	25.230592
157.461982	4867.135964	25.235610
158.013020	4877.133920	25.240627
158.363607	4874.292625	25.245645
158.723190	4850.805710	25.250663
158.848517	4865.057879	25.255680
158.805385	4855.470467	25.260698
158.732751	4849.917079	25.265715
158.961305	4850.015523	25.270733
158.801689	4851.863045	25.275751
158.772292	4861.173828	25.280768
159.053799	4853.443075	25.285786
159.111163	4859.834947	25.290803
159.062625	4876.140028	25.295821
159.606791	4880.451418	25.300839
159.362042	4885.621604	25.305856
159.487940	4893.426787	25.310874
159.754026	4905.234660	25.315891
159.848417	4904.644236	25.320909
160.268490	4913.422005	25.325927
159.837585	4941.975756	25.330944
160.225404	4940.936493	25.335962
160.490483	4949.806980	25.340979
160.792353	4967.043887	25.345997
161.104075	4966.802463	25.351015
160.857362	4977.655239	25.356032
160.761303	4992.761797	25.361050
161.136790	4997.812416	25.366067
161.113965	5010.562257	25.371085
161.621865	5020.713173	25.376103
161.705966	5028.218220	25.381120
161.975255	5037.891370	25.386138
162.225531	5052.767959	25.391155
162.437109	5053.237805	25.396173
163.170467	5059.248869	25.401191
163.044275	5063.235395	25.406208
163.317370	5050.079635	25.411226
163.134366	5049.242327	25.416243
163.360128	5054.536787	25.421261
164.239461	5062.810678	25.426279
164.333380	5056.718413	25.431296
164.077283	5053.236803	25.436314
164.256057	5052.379544	25.441331
164.438967	5066.627053	25.446349
164.719341	5056.799108	25.451367
164.344778	5068.545022	25.456384
164.388796	5070.282337	25.461402
164.639857	5061.010555	25.466419
164.811019	5072.167262	25.471437
164.776810	5088.448130	25.476455
164.785590	5088.076692	25.481472
165.148098	5093.828856	25.486490
165.250726	5122.227333	25.491507
165.287880	5133.407927	25.496525
165.556464	5146.229165	25.501543
165.639703	5158.872506	25.506560
166.157026	5155.404903	25.511578
166.288785	5171.722860	25.516595
166.636323	5179.906404	25.521613
166.879990	5185.031755	25.526631
166.367983	5194.025208	25.531648
167.021213	5199.783445	25.536666
167.254505	5211.380416	25.541683
167.106695	5212.711733	25.546701
167.674636	5227.608947	25.551719
167.777523	5245.091869	25.556736
167.811760	5245.222606	25.561754
167.952354	5251.345634	25.566771
168.251510	5271.599730	25.571789
168.473509	5275.589093	25.576807
168.468225	5270.850530	25.581824
168.733447	5272.825973	25.586842
168.922248	5291.074368	25.591859
168.893750	5291.046990	25.596877
169.853801	5294.286807	25.601895
169.328515	5294.677486	25.606912
169.753037	5309.033130	25.611930
169.755316	5321.701081	25.616947
169.913208	5325.859413	25.621965
170.215953	5319.628386	25.626983
170.265262	5331.213490	25.632000
170.659296	5344.717350	25.637018
170.477611	5345.696747	25.642035
170.468099	5353.104881	25.647053
170.967552	5361.584609	25.652071
171.324037	5381.267777	25.657088
171.370727	5375.131257	25.662106
171.714328	5377.334689	25.667123
171.540600	5397.514735	25.672141
171.687373	5396.991985	25.677159
171.853366	5400.998562	25.682176
171.920937	5411.070899	25.687194
172.414094	5423.356508	25.692212
172.351518	5434.290835	25.697229
172.666626	5432.301988	25.702247
172.662605	5458.343447	25.707264
172.889896	5470.433058	25.712282
173.084179	5461.722573	25.717300
173.062496	5479.757286	25.722317
173.596580	5493.671961	25.727335
173.214486	5500.530910	25.732352
173.524980	5513.031237	25.737370
174.114412	5519.004967	25.742388
174.346864	5520.565316	25.747405
174.423169	5514.056807	25.752423
174.471921	5529.039792	25.757440
175.082374	5533.471091	25.762458
175.365236	5548.767245	25.767476
175.132824	5561.048302	25.772493
175.684057	5559.356503	25.777511
175.169312	5552.042828	25.782528
175.462775	5561.324791	25.787546
175.683916	5559.613022	25.792564
175.698658	5584.020476	25.797581
176.082785	5572.044544	25.802599
176.423846	5598.365981	25.807616
176.171355	5610.922919	25.812634
176.473977	5595.803851	25.817652
176.595001	5621.701937	25.822669
176.666160	5627.297150	25.827687
177.468408	5626.793064	25.832704
177.217983	5627.923304	25.837722
177.464231	5645.111917	25.842740
177.909838	5654.187508	25.847757
178.191450	5644.748852	25.852775
178.597326	5649.908835	25.857792
178.614177	5643.051797	25.862810
178.902149	5655.399250	25.867828
178.951084	5680.474563	25.872845
179.142344	5674.599801	25.877863
179.269861	5672.958709	25.882880
179.269402	5677.656170	25.887898
179.438408	5672.005633	25.892916
179.329961	5689.917962	25.897933
179.626206	5697.707841	25.902951
179.871323	5703.855420	25.907968
179.865381	5718.614546	25.912986
179.887764	5724.907044	25.918004
179.955053	5734.295214	25.923021
180.411625	5761.695639	25.928039
180.277693	5765.905729	25.933056
180.651855	5774.786124	25.938074
180.980633	5779.700629	25.943092
180.729476	5811.437908	25.948109
181.425500	5814.487008	25.953127
181.561498	5817.383434	25.958144
181.889791	5829.095818	25.963162
182.261826	5837.694641	25.968180
182.416066	5841.822212	25.973197
182.692889	5842.363154	25.978215
183.091337	5841.408707	25.983232
182.948148	5862.193875	25.988250
183.695541	5856.646429	25.993268
183.962295	5856.018666	25.998285
184.138738	5858.724868	26.003303
184.171704	5861.903845	26.008320
184.347505	5864.627482	26.013338
184.282777	5865.260620	26.018356
184.387040	5864.087271	26.023373
184.549967	5856.968799	26.028391
184.539886	5857.743289	26.033408
184.546075	5876.132970	26.038426
184.912542	5881.691805	26.043444
184.843177	5890.946042	26.048461
184.840688	5892.657309	26.053479
184.852044	5911.033570	26.058496
184.843794	5923.866001	26.063514
185.309177	5946.551464	26.068532
185.270661	5955.318596	26.073549
185.672315	5972.643204	26.078567
185.683085	5979.945085	26.083584
186.455804	6013.241439	26.088602
186.143288	6012.728827	26.093620
186.468116	6019.179117	26.098637
186.947988	6029.966225	26.103655
186.700834	6037.283424	26.108672
187.267616	6056.114164	26.113690
187.766891	6052.020069	26.118708
187.950449	6064.689212	26.123725
188.069006	6059.565957	26.128743
188.127316	6067.890177	26.133760
188.533826	6080.898765	26.138778
188.765981	6103.197108	26.143796
188.543225	6093.482054	26.148813
188.505629	6099.100231	26.153831
188.798102	6116.139119	26.158848
188.676996	6134.881052	26.163866
189.421946	6143.440918	26.168884
189.660904	6153.360808	26.173901
189.906875	6151.218750	26.178919
190.154709	6147.372767	26.183936
190.317459	6171.634455	26.188954
190.459375	6173.389492	26.193972
190.547850	6179.875183	26.198989
190.632650	6192.565564	26.204007
191.001114	6202.138678	26.209024
190.731020	6214.697443	26.214042
191.257202	6226.635581	26.219060
191.057195	6236.199996	26.224077
191.556971	6246.358574	26.229095
191.746852	6258.225810	26.234112
191.909200	6272.891329	26.239130
192.492314	6279.126319	26.244148
192.514057	6302.501932	26.249165
192.605529	6302.213604	26.254183
193.007676	6318.660308	26.259200
193.192657	6323.917080	26.264218
193.618488	6330.001796	26.269236
193.448090	6334.896242	26.274253
193.423635	6346.123375	26.279271
194.179409	6353.629290	26.284288
194.223848	6352.028712	26.289306
194.787200	6356.316852	26.294324
195.180054	6374.887029	26.299341
195.024941	6373.847318	26.304359
195.272156	6369.194853	26.309376
195.240997	6379.094395	26.314394
195.425729	6374.524773	26.319412
195.357306	6382.982060	26.324429
195.652831	6397.808296	26.329447
196.104974	6403.754773	26.334464
195.903255	6409.204999	26.339482
195.915111	6434.482214	26.344500
196.508223	6439.945304	26.349517
196.665085	6441.555327	26.354535
196.784870	6452.447454	26.359552
197.171465	6465.992897	26.364570
197.112718	6467.287464	26.369588
197.446279	6492.599532	26.374605
197.351074	6498.247114	26.379623
197.884608	6500.195461	26.384640
197.862373	6520.499840	26.389658
198.040072	6521.484964	26.394676
198.147083	6536.739623	26.399693
198.373711	6551.961031	26.404711
198.453512	6546.551059	26.409728
198.825281	6585.597259	26.414746
199.220260	6578.472200	26.419764
199.704566	6567.764301	26.424781
200.311512	6567.440726	26.429799
200.580000	6560.876224	26.434816
200.803685	6552.008242	26.439834
200.946458	6543.386850	26.444852
200.911147	6538.679676	26.449869
200.838783	6556.934337	26.454887
201.488215	6572.161125	26.459904
201.406831	6578.559421	26.464922
201.421217	6582.936478	26.469940
201.584563	6578.078925	26.474957
201.602876	6585.599584	26.479975
201.658341	6589.627194	26.484992
201.649571	6599.579863	26.490010
201.929970	6601.610455	26.495028
201.980902	6614.580112	26.500045
201.992031	6628.837099	26.505063
202.391581	6642.074937	26.510080
202.565652	6666.909694	26.515098
202.697938	6674.659565	26.520116
202.810081	6694.105361	26.525133
203.134742	6705.642569	26.530151
203.478770	6714.317416	26.535168
203.498738	6736.080079	26.540186
203.786420	6754.676842	26.545204
204.056862	6761.110482	26.550221
203.827446	6787.776015	26.555239
204.566479	6799.023898	26.560256
204.955074	6812.120347	26.565274
204.836451	6827.401750	26.570292
205.365048	6839.419506	26.575309
205.158468	6852.536904	26.580327
206.075990	6859.914583	26.585344
206.347455	6871.344966	26.590362
206.834792	6864.050842	26.595380
206.924159	6865.687878	26.600397
207.115595	6887.349006	26.605415
207.562496	6889.001463	26.610432
207.613657	6894.609112	26.615450
207.669731	6897.877401	26.620468
207.712412	6894.798634	26.625485
207.662416	6905.319155	26.630503
208.239700	6922.863736	26.635520
208.154688	6934.755102	26.640538
208.095975	6940.296745	26.645556
208.551681	6945.681238	26.650573
208.712476	6959.694685	26.655591
209.037958	6968.730349	26.660608
209.252833	6983.597317	26.665626
209.316955	6980.733940	26.670644
209.674452	6997.576301	26.675661
209.638503	7021.268959	26.680679
210.261570	7015.559042	26.685696
210.442770	7035.668020	26.690714
210.728001	7051.775743	26.695732
210.928515	7049.320542	26.700749
210.816491	7055.395666	26.705767
211.222761	7062.473223	26.710784
211.266863	7078.777783	26.715802
211.395774	7085.270518	26.720820
211.863863	7100.301890	26.725837
211.379712	7110.750541	26.730855
212.012254	7123.077337	26.735872
212.467746	7140.448632	26.740890
212.345241	7158.572898	26.745908
212.662083	7159.334090	26.750925
212.410528	7174.220450	26.755943
212.784877	7190.105561	26.760960
213.240116	7200.046885	26.765978
213.445223	7201.326026	26.770996
213.458591	7229.421750	26.776013
213.438550	7236.988473	26.781031
214.056137	7257.627792	26.786048
213.770136	7262.965497	26.791066
214.186693	7288.286315	26.796084
214.306300	7292.609064	26.801101
214.649714	7313.416100	26.806119
215.235048	7313.377308	26.811136
215.562326	7326.890025	26.816154
215.680520	7347.073668	26.821172
216.007543	7346.935226	26.826189
216.355601	7355.128486	26.831207
216.568774	7365.888360	26.836224
216.876138	7378.630142	26.841242
216.964985	7377.234757	26.846260
217.053821	7385.586892	26.851277
217.429931	7405.998717	26.856295
217.562926	7408.864429	26.861312
217.614366	7425.699022	26.866330
217.879508	7422.491820	26.871348
218.317633	7435.090618	26.876365
218.144499	7448.720456	26.881383
218.449686	7451.043996	26.886400
219.137093	7466.271642	26.891418
219.118135	7475.226983	26.896436
219.601007	7477.305967	26.901453
219.753573	7476.205607	26.906471
220.401451	7473.479877	26.911488
220.382912	7476.536193	26.916506
220.841968	7493.965573	26.921524
220.948092	7501.654030	26.926541
220.898136	7508.279844	26.931559
221.286456	7511.322916	26.936576
221.393877	7508.909107	26.941594
221.174575	7509.527033	26.946612
221.314233	7520.008571	26.951629
221.698078	7534.779452	26.956647
221.658874	7547.768000	26.961664
221.947273	7565.647227	26.966682
222.110726	7574.376969	26.971700
222.852074	7589.420905	26.976717
222.543944	7596.517367	26.981735
222.956688	7617.759117	26.986752
223.058807	7632.313810	26.991770
223.233381	7643.660027	26.996788
223.306566	7643.823699	27.001805
223.515127	7673.870394	27.006823
223.736330	7677.583235	27.011840
224.104748	7695.953437	27.016858
224.405504	7701.498632	27.021876
224.775197	7725.276965	27.026893
225.119737	7739.946654	27.031911
225.130654	7747.828281	27.036928
225.630603	7770.325512	27.041946
225.599282	7766.263223	27.046964
225.772718	7787.633184	27.051981
225.855716	7816.325690	27.056999
226.002862	7822.010667	27.062016
226.339867	7831.667194	27.067034
226.354677	7853.114800	27.072052
226.697033	7867.268237	27.077069
226.806366	7892.912823	27.082087
227.359169	7914.308932	27.087104
227.666072	7925.067790	27.092122
227.467866	7954.333454	27.097140
227.862219	7960.065630	27.102157
228.156200	7969.982244	27.107175
228.263706	7976.541129	27.112192
229.051777	7997.094797	27.117210
229.201619	8010.664360	27.122228
229.583744	8001.266692	27.127245
229.380565	8014.771244	27.132263
229.429062	8027.777119	27.137280
229.953108	8029.100225	27.142298
229.649394	8061.074434	27.147316
230.065012	8061.236354	27.152333
230.295889	8081.896102	27.157351
230.547992	8091.294346	27.162368
230.727343	8112.803973	27.167386
230.838126	8136.257288	27.172404
231.087994	8145.373933	27.177421
231.340221	8167.348881	27.182439
231.491763	8195.577743	27.187456
232.033084	8210.622422	27.192474
232.114096	8228.289507	27.197492
232.318117	8250.395463	27.202509
232.406230	8260.175529	27.207527
232.556433	8288.518997	27.212544
233.083387	8295.503011	27.217562
233.624805	8314.716406	27.222580
233.893861	8317.902337	27.227597
234.403855	8337.824419	27.232615
234.703498	8344.127030	27.237632
235.134649	8342.792058	27.242650
235.512551	8358.799061	27.247668
236.083018	8358.582356	27.252685
236.524380	8356.937686	27.257703
236.584547	8356.891630	27.262720
236.734176	8344.309802	27.267738
236.794961	8361.516426	27.272756
237.073792	8360.587233	27.277773
237.294549	8355.749537	27.282791
236.712093	8355.006772	27.287808
236.859615	8364.284702	27.292826
237.247949	8389.859312	27.297844
237.446259	8392.068413	27.302861
237.637505	8413.119587	27.307879
237.584707	8433.935631	27.312896
238.159269	8443.320681	27.317914
238.332393	8463.429656	27.322932
238.497242	8481.557307	27.327949
238.909591	8479.527518	27.332967
239.014322	8498.756974	27.337984
239.764429	8503.199013	27.343002
239.734817	8531.006408	27.348020
240.080424	8524.002915	27.353037
240.547966	8541.903103	27.358055
240.989194	8546.064837	27.363072
241.176746	8545.594295	27.368090
241.062953	8545.703180	27.373108
241.453463	8552.360225	27.378125
241.657914	8569.046929	27.383143
242.097184	8586.710817	27.388160
242.129032	8576.123235	27.393178
242.219519	8594.282275	27.398196
242.539018	8605.144272	27.403213
242.543955	8615.068352	27.408231
242.685668	8636.825200	27.413248
243.267341	8638.334935	27.418266
243.341244	8650.028659	27.423284
243.372921	8671.293381	27.428301
243.539204	8682.151740	27.433319
243.675620	8707.149550	27.438336
244.078680	8700.385362	27.443354
244.245334	8734.934310	27.448372
244.499140	8742.423162	27.453389
244.604139	8746.413155	27.458407
244.811419	8773.179600	27.463424
245.507700	8771.938400	27.468442
245.553048	8796.104652	27.473460
245.888179	8798.768454	27.478477
246.394572	8819.737081	27.483495
246.640776	8815.614235	27.488512
246.961912	8809.968038	27.493530
247.327566	8832.287422	27.498548
247.752624	8835.765002	27.503565
247.724860	8838.912915	27.508583
247.558571	8846.274677	27.513600
248.146342	8854.844819	27.518618
248.251674	8866.152996	27.523636
248.341516	8881.623874	27.528653
248.824340	8892.840992	27.533671
248.798661	8897.295451	27.538688
249.256936	8914.754882	27.543706
249.074009	8942.216644	27.548724
249.527582	8949.248591	27.553741
249.872553	8953.929803	27.558759
249.753528	8974.722105	27.563776
250.113969	8985.962772	27.568794
250.265360	9013.650341	27.573812
250.417252	9027.654485	27.578829
250.709292	9053.976412	27.583847
250.667135	9068.400410	27.588864
250.934460	9084.302049	27.593882
251.324838	9114.650534	27.598900
251.456610	9140.152385	27.603917
252.324781	9157.432116	27.608935
252.092556	9193.842856	27.613952
252.728306	9203.939788	27.618970
252.448757	9220.463379	27.623988
252.830501	9246.826651	27.629005
253.430143	9258.342089	27.634023
253.550961	9291.827697	27.639040
254.089844	9297.593067	27.644058
254.130011	9318.286101	27.649076
254.633477	9330.005849	27.654093
254.720713	9346.081043	27.659111
255.116548	9375.036329	27.664128
255.841047	9377.381087	27.669146
255.950393	9400.006966	27.674164
255.921597	9412.216973	27.679181
256.226736	9427.164973	27.684199
256.504588	9444.363480	27.689216
256.815114	9460.886177	27.694234
256.900560	9462.281497	27.699252
257.187026	9476.483465	27.704269
257.533472	9491.879212	27.709287
257.531708	9510.363429	27.714304
258.454414	9521.496878	27.719322
258.663589	9534.090480	27.724340
258.774979	9537.825943	27.729357
258.875428	9561.331119	27.734375
259.102539	9571.483574	27.739392
259.234580	9583.025731	27.744410
259.323037	9609.381608	27.749428
259.736420	9632.192061	27.754445
260.110039	9627.328589	27.759463
260.071050	9661.044768	27.764480
260.322273	9670.409428	27.769498
260.728244	9689.135710	27.774516
260.930219	9706.579505	27.779533
261.809813	9727.051670	27.784551
261.723236	9739.201412	27.789568
261.831935	9748.294374	27.794586
262.322971	9764.681829	27.799604
262.352308	9757.425473	27.804621
262.620401	9778.256910	27.809639
262.624623	9800.915000	27.814656
263.078938	9819.327737	27.819674
263.407975	9829.523294	27.824692
263.706592	9842.088098	27.829709
264.526867	9844.268911	27.834727
264.608266	9851.642762	27.839744
264.938389	9858.124469	27.844762
265.347766	9873.462072	27.849780
265.308270	9875.071198	27.854797
265.506654	9879.933024	27.859815
265.629629	9907.294404	27.864832
265.762921	9912.160751	27.869850
266.147421	9935.992702	27.874868
266.135037	9942.161868	27.879885
266.532504	9962.943689	27.884903
266.397855	9981.222850	27.889920
266.877638	10005.425098	27.894938
267.038367	10016.437333	27.899956
267.143730	10045.909261	27.904973
267.345885	10056.070897	27.909991
267.824506	10085.229572	27.915008
268.247257	10106.487157	27.920026
268.594567	10125.875216	27.925044
268.607815	10150.019690	27.930061
269.230198	10172.967146	27.935079
269.679452	10195.404531	27.940096
269.670574	10200.411183	27.945114
270.441895	10225.424048	27.950132
271.042328	10229.615715	27.955149
271.293990	10223.820643	27.960167
271.584957	10239.060885	27.965184
272.009134	10250.830724	27.970202
272.323120	10251.464137	27.975220
272.187935	10260.015710	27.980237
272.556446	10270.274319	27.985255
272.951072	10282.457969	27.990272
272.748430	10277.996506	27.995290
273.340412	10299.474394	28.000308
273.154500	10306.048320	28.005325
273.836281	10313.870961	28.010343
273.981403	10328.272064	28.015360
274.050965	10343.854078	28.020378
274.524351	10367.091276	28.025396
274.714001	10374.191339	28.030413
275.277419	10392.039070	28.035431
275.242641	10401.818014	28.040448
275.354892	10432.353073	28.045466
275.602229	10438.068032	28.050484
275.890687	10457.920060	28.055501
275.954244	10470.153342	28.060519
275.910931	10486.320696	28.065536
276.396099	10514.376100	28.070554
276.934707	10538.385028	28.075572
276.869065	10565.083206	28.080589
277.071648	10570.785952	28.085607
277.544869	10601.946777	28.090624
277.791286	10622.464624	28.095642
278.570726	10629.648804	28.100660
278.699005	10644.361821	28.105677
279.152331	10661.627811	28.110695
278.957954	10685.646862	28.115712
279.442502	10700.930226	28.120730
279.907263	10723.376016	28.125748
279.700925	10735.354171	28.130765
280.194547	10746.787457	28.135783
280.593384	10776.079607	28.140800
280.772472	10802.543708	28.145818
281.322912	10798.434419	28.150836
281.240813	10820.381890	28.155853
281.496741	10828.413408	28.160871
281.838319	10844.722017	28.165888
281.876504	10860.609912	28.170906
282.248919	10886.372361	28.175924
282.424585	10914.036322	28.180941
282.729568	10927.062600	28.185959
283.037549	10960.125084	28.190976
283.359957	10966.861425	28.195994
283.740815	10988.454884	28.201012
283.967433	11009.621768	28.206029
284.652980	11024.732597	28.211047
284.481246	11055.290802	28.216064
284.834252	11059.718400	28.221082
285.413188	11074.377423	28.226100
285.659382	11101.317764	28.231117
286.203662	11111.034812	28.236135
286.404375	11118.788867	28.241152
286.767053	11142.881501	28.246170
287.163531	11151.034797	28.251188
287.147445	11180.688125	28.256205
287.559771	11184.620578	28.261223
287.470900	11210.280547	28.266240
287.858736	11226.424284	28.271258
288.248076	11239.012927	28.276276
288.297720	11268.504226	28.281293
288.557406	11291.925595	28.286311
289.016217	11306.190368	28.291328
288.873728	11335.523043	28.296346
289.337354	11359.730016	28.301364
289.631868	11390.235030	28.306381
289.933201	11409.611003	28.311399
290.225579	11438.086893	28.316416
290.513137	11459.822545	28.321434
291.011759	11481.126069	28.326452
291.075170	11500.773316	28.331469
291.681879	11526.532529	28.336487
291.820796	11540.945201	28.341504
292.026291	11560.936069	28.346522
292.511588	11584.402320	28.351540
292.727255	11605.581258	28.356557
293.488249	11634.277461	28.361575
293.580885	11645.557399	28.366592
293.613874	11662.301015	28.371610
294.443048	11685.059487	28.376628
294.671513	11707.122020	28.381645
294.855340	11719.250387	28.386663
295.165413	11737.528558	28.391680
294.912668	11759.141644	28.396698
295.437194	11782.396813	28.401716
295.459163	11800.834800	28.406733
295.910241	11825.569294	28.411751
296.259007	11833.266005	28.416768
296.702502	11871.088797	28.421786
297.639921	11864.412591	28.426804
298.132866	11881.584275	28.431821
298.242993	11885.039214	28.436839
298.886775	11913.564716	28.441856
299.160615	11906.150955	28.446874
299.718874	11906.885682	28.451892
299.500959	11922.801409	28.456909
299.795650	11924.815352	28.461927
300.202218	11929.700732	28.466944
299.964993	11953.005485	28.471962
300.436661	11963.001425	28.476980
300.247441	11970.871097	28.481997
300.664561	11995.203360	28.487015
301.207426	12006.979194	28.492032
300.728164	12022.238777	28.497050
301.108750	12041.435306	28.502068
301.314050	12063.336713	28.507085
301.850344	12089.062824	28.512103
301.901539	12096.739762	28.517120
302.283965	12134.381065	28.522138
302.744503	12156.621544	28.527156
303.243899	12187.982789	28.532173
303.048176	12203.148161	28.537191
303.713405	12229.532258	28.542208
303.595110	12258.424500	28.547226
304.453511	12266.983829	28.552244
304.951356	12283.945542	28.557261
305.280333	12297.712737	28.562279
305.996637	12304.505541	28.567296
306.117341	12324.825031	28.572314
306.553109	12332.896760	28.577332
307.033320	12343.384757	28.582349
307.577636	12371.511570	28.587367
307.383863	12378.446143	28.592384
307.455442	12398.338952	28.597402
308.176939	12399.672198	28.602420
308.009753	12416.602705	28.607437
307.636810	12440.097742	28.612455
308.153509	12463.303189	28.617472
308.471594	12506.353347	28.622490
308.794527	12522.904704	28.627508
308.802012	12545.893876	28.632525
309.497758	12572.207276	28.637543
309.959865	12592.741433	28.642560
310.018424	12620.709845	28.647578
310.475093	12638.948921	28.652596
310.791218	12665.342874	28.657613
311.195345	12695.356221	28.662631
311.312569	12704.354093	28.667648
311.869517	12731.081628	28.672666
312.313038	12754.246069	28.677684
312.615701	12778.215582	28.682701
313.387045	12788.499491	28.687719
313.761186	12790.848617	28.692736
314.037316	12821.822691	28.697754
314.424811	12821.339306	28.702772
314.557233	12840.834881	28.707789
314.684449	12857.362361	28.712807
315.190975	12881.331254	28.717824
315.319712	12898.908070	28.722842
316.040173	12918.783544	28.727860
316.239858	12934.537906	28.732877
316.282010	12942.035517	28.737895
316.976435	12960.662527	28.742912
316.955861	12980.992124	28.747930
317.683776	12986.073435	28.752948
317.594006	13021.057892	28.757965
317.846084	13024.473735	28.762983
318.076396	13039.480857	28.768000
318.250573	13073.293226	28.773018
318.423593	13088.109769	28.778036
318.821552	13100.999434	28.783053
319.202627	13121.913336	28.788071
319.884339	13147.049640	28.793088
319.661444	13167.439871	28.798106
319.888754	13183.166244	28.803124
320.180717	13210.920392	28.808141
320.260778	13239.201479	28.813159
321.166569	13248.402747	28.818176
320.999729	13289.373360	28.823194
321.375554	13302.126603	28.828212
321.755138	13326.746040	28.833229
321.806334	13351.033963	28.838247
322.529084	13380.574868	28.843264
322.531130	13406.700709	28.848282
322.681956	13432.801875	28.853300
323.456654	13449.090013	28.858317
323.595909	13488.095494	28.863335
323.922561	13504.484911	28.868352
324.057344	13540.050950	28.873370
324.387231	13565.747503	28.878388
324.629070	13587.247751	28.883405
325.061718	13619.757544	28.888423
325.525249	13642.989270	28.893440
325.814688	13681.926138	28.898458
326.276512	13705.514407	28.903476
326.471675	13737.397249	28.908493
326.491137	13764.274084	28.913511
327.197021	13795.935087	28.918528
327.243995	13837.798230	28.923546
327.681069	13860.100101	28.928564
328.317206	13889.690991	28.933581
328.437787	13903.519384	28.938599
329.027956	13932.683014	28.943616
329.539605	13960.132445	28.948634
329.986096	13992.122176	28.953652
330.464928	14011.348842	28.958669
330.446943	14037.494778	28.963687
331.172253	14065.132685	28.968704
331.503317	14079.649648	28.973722
331.997212	14093.622643	28.978740
332.151794	14111.492763	28.983757
332.401604	14126.043754	28.988775
332.918041	14138.591478	28.993792
333.032162	14167.799939	28.998810
333.129649	14195.712574	29.003828
333.578051	14203.587715	29.008845
333.592264	14241.931772	29.013863
334.566163	14257.407499	29.018880
334.821223	14287.636091	29.023898
335.054023	14311.521752	29.028916
335.455547	14334.077614	29.033933
335.464343	14351.255117	29.038951
336.018427	14375.744707	29.043968
336.065213	14406.403703	29.048986
336.654248	14433.177561	29.054004
337.040205	14455.379991	29.059021
337.140438	14489.990869	29.064039
337.443900	14503.404833	29.069056
338.156351	14531.575220	29.074074
338.509485	14559.452310	29.079092
338.837833	14579.067137	29.084109
338.914940	14604.496834	29.089127
339.830202	14611.319036	29.094144
339.748266	14628.352720	29.099162
340.492308	14657.365999	29.104180
341.298209	14661.468763	29.109197
341.759269	14682.609366	29.114215
341.957868	14678.984692	29.119232
342.501403	14685.643300	29.124250
343.034654	14694.158653	29.129268
343.348999	14706.105231	29.134285
342.826468	14712.504375	29.139303
342.904021	14722.094672	29.144320
343.257489	14742.936436	29.149338
343.605026	14773.245127	29.154356
343.726610	14773.277116	29.159373
343.643374	14805.209862	29.164391
343.473348	14831.022973	29.169408
344.073949	14862.504949	29.174426
344.251704	14890.465324	29.179444
344.235347	14929.788513	29.184461
344.699642	14970.946907	29.189479
345.295315	15004.794119	29.194496
345.884571	15035.594286	29.199514
346.040048	15070.651129	29.204532
346.991993	15086.134447	29.209549
347.155079	15130.577449	29.214567
347.925851	15147.563010	29.219584
348.201022	15164.277868	29.224602
348.937022	15185.578343	29.229620
350.253653	15179.876494	29.234637
350.657954	15190.779279	29.239655
351.423482	15183.802484	29.244672
351.720621	15187.837018	29.249690
351.346477	15192.251006	29.254708
351.799715	15199.262115	29.259725
351.912861	15209.056409	29.264743
352.252880	15216.935862	29.269760
352.334484	15238.597293	29.274778
352.671378	15248.977010	29.279796
352.932788	15261.805960	29.284813
352.925403	15288.814267	29.289831
352.975253	15316.278069	29.294848
353.577360	15338.028116	29.299866
353.239977	15368.643973	29.304884
354.082714	15386.163171	29.309901
354.365105	15421.811222	29.314919
355.125750	15445.089149	29.319936
354.781768	15475.003340	29.324954
355.281929	15514.234243	29.329972
355.818302	15536.763058	29.334989
355.971923	15570.175774	29.340007
356.399545	15590.951132	29.345024
357.581639	15606.206001	29.350042
358.042278	15619.591618	29.355060
358.899539	15635.259839	29.360077
359.435022	15645.102447	29.365095
359.581029	15660.839982	29.370112
360.006701	15673.725505	29.375130
360.212790	15674.112282	29.380148
360.808040	15690.963647	29.385165
360.703658	15703.352486	29.390183
360.837308	15715.460640	29.395200
361.329190	15728.466029	29.400218
361.339346	15756.041185	29.405236
361.905809	15770.370812	29.410253
361.706125	15801.495767	29.415271
361.927878	15827.809629	29.420288
362.689391	15843.440365	29.425306
362.936265	15872.569911	29.430324
363.430202	15891.411692	29.435341
363.596391	15921.762086	29.440359
363.771524	15954.208958	29.445376
364.177194	15975.384073	29.450394
364.423719	16013.348485	29.455412
365.266795	16020.541078	29.460429
365.388859	16062.343825	29.465447
365.554570	16083.521112	29.470464
365.985195	16115.434085	29.475482
366.296814	16147.705773	29.480500
366.450427	16174.761293	29.485517
366.643361	16216.328835	29.490535
367.140827	16239.423057	29.495552
367.860261	16261.362901	29.500570
367.870558	16293.357074	29.505588
368.306518	16320.387997	29.510605
368.523297	16345.630103	29.515623
369.058307	16369.492199	29.520640
369.331065	16398.700338	29.525658
369.379585	16434.096249	29.530676
369.870575	16462.224781	29.535693
369.999131	16507.451165	29.540711
370.603229	16539.373972	29.545728
371.221685	16568.069451	29.550746
371.715065	16603.603044	29.555764
372.039626	16636.243957	29.560781
372.294532	16659.933902	29.565799
372.521668	16698.394901	29.570816
373.169829	16737.022491	29.575834
373.176283	16772.285825	29.580852
373.457164	16802.770105	29.585869
373.872612	16832.002596	29.590887
374.412730	16868.112215	29.595904
374.974600	16899.210458	29.600922
375.149477	16928.234028	29.605940
375.775752	16964.589633	29.610957
376.173916	16994.949175	29.615975
376.886844	17020.420423	29.620992
377.861628	17046.442477	29.626010
377.889261	17060.796532	29.631028
378.674850	17080.940537	29.636045
379.111677	17110.058051	29.641063
379.055595	17124.460745	29.646080
379.430361	17141.737994	29.651098
379.611238	17178.286278	29.656116
379.972595	17201.190079	29.661133
380.204319	17236.869381	29.666151
380.589462	17260.305259	29.671168
380.988918	17287.607073	29.676186
381.435332	17330.631233	29.681204
381.990626	17349.535424	29.686221
382.438803	17380.790599	29.691239
382.363624	17415.504535	29.696256
382.878943	17441.006105	29.701274
382.816090	17481.474894	29.706292
383.329094	17509.368255	29.711309
384.084210	17549.215825	29.716327
383.962474	17583.567405	29.721344
384.492041	17625.016357	29.726362
384.818423	17661.806362	29.731380
385.679595	17668.088703	29.736397
386.121797	17711.607949	29.741415
386.535193	17734.098719	29.746432
387.134663	17761.790555	29.751450
387.538421	17795.853509	29.756468
387.750263	17827.977952	29.761485
388.361252	17844.931374	29.766503
389.218051	17861.541319	29.771520
389.953541	17882.938384	29.776538
389.693878	17905.402465	29.781556
390.284643	17918.035324	29.786573
390.541412	17941.822953	29.791591
390.833432	17952.443559	29.796608
391.637831	17968.456986	29.801626
391.831623	17984.021698	29.806644
391.877194	18006.654332	29.811661
391.755506	18027.989037	29.816679
392.558069	18058.289659	29.821696
393.121223	18083.388599	29.826714
393.308528	18099.682790	29.831732
394.154152	18115.695818	29.836749
394.495274	18134.335392	29.841767
394.909246	18152.791058	29.846784
395.278485	18168.596364	29.851802
395.412059	18189.009244	29.856820
395.554023	18209.485388	29.861837
395.901253	18231.650473	29.866855
395.837311	18265.940262	29.871872
396.446374	18287.614229	29.876890
396.899261	18311.316212	29.881908
397.251802	18342.847618	29.886925
397.981178	18372.606073	29.891943
398.031602	18402.102170	29.896960
398.440144	18427.999760	29.901978
398.881296	18464.061510	29.906996
399.028450	18486.580183	29.912013
399.856668	18514.159612	29.917031
400.089565	18549.543591	29.922048
400.629909	18575.704853	29.927066
400.776459	18599.620504	29.932084
401.316290	18633.908499	29.937101
401.973643	18661.343144	29.942119
402.595052	18684.309843	29.947136
403.127387	18708.402766	29.952154
403.419534	18742.981207	29.957172
403.915013	18763.350441	29.962189
404.088216	18782.023362	29.967207
404.318780	18815.045181	29.972224
404.608602	18846.441347	29.977242
404.704243	18877.384273	29.982260
405.027184	18915.779313	29.987277
405.521783	18949.466953	29.992295
405.631476	19002.402758	29.997312
406.337782	19027.403674	30.002330
406.350788	19066.325063	30.007348
406.685784	19112.653004	30.012365
407.561619	19144.647623	30.017383
408.222124	19184.434430	30.022400
408.904506	19204.974951	30.027418
409.792560	19220.868496	30.032436
410.773665	19242.883921	30.037453
411.279036	19246.861224	30.042471
411.069610	19276.373649	30.047488
411.500356	19300.145355	30.052506
412.068433	19319.801666	30.057524
412.365770	19344.945087	30.062541
412.461272	19369.877711	30.067559
412.670728	19389.858526	30.072576
413.362761	19429.505102	30.077594
413.031396	19466.480865	30.082612
413.242818	19497.698940	30.087629
413.670359	19518.988462	30.092647
414.142704	19556.727971	30.097664
414.895560	19580.574272	30.102682
415.309474	19614.371247	30.107700
415.577769	19656.693183	30.112717
416.574538	19683.939131	30.117735
416.780892	19721.245499	30.122752
417.180889	19749.462508	30.127770
417.425999	19781.876848	30.132788
417.784699	19812.612271	30.137805
418.390800	19846.885444	30.142823
418.408485	19887.026641	30.147840
418.757403	19918.210049	30.152858
419.536284	19952.651811	30.157876
419.952976	19979.543693	30.162893
420.456133	20011.196699	30.167911
420.688085	20047.583552	30.172928
421.178820	20074.740767	30.177946
421.687179	20094.683811	30.182964
422.081289	20132.639415	30.187981
422.410659	20142.820079	30.192999
422.768772	20176.537591	30.198016
423.200348	20201.973744	30.203034
423.565221	20238.070911	30.208052
423.721425	20270.554566	30.213069
424.043320	20304.685114	30.218087
424.477481	20343.939969	30.223104
424.883323	20374.832560	30.228122
425.385866	20415.905090	30.233140
425.524994	20466.437869	30.238157
426.229054	20488.266043	30.243175
426.054061	20541.134165	30.248192
426.741663	20566.816867	30.253210
427.346276	20618.412687	30.258228
427.964663	20663.198466	30.263245
428.698030	20695.905558	30.268263
428.925582	20732.269397	30.273280
429.183512	20757.588605	30.278298
429.990922	20791.530711	30.283316
430.402487	20834.858215	30.288333
431.141777	20865.956471	30.293351
431.567787	20899.381935	30.298368
431.908719	20925.458595	30.303386
432.564079	20966.166530	30.308404
432.887960	20990.926456	30.313421
433.438148	21015.757621	30.318439
433.363027	21052.594971	30.323456
434.263833	21085.792161	30.328474
435.081948	21120.005917	30.333492
434.841147	21153.085403	30.338509
435.745407	21183.937689	30.343527
435.693527	21217.346981	30.348544
435.840534	21261.071125	30.353562
436.432877	21286.422302	30.358580
437.248890	21326.235666	30.363597
437.933712	21346.458346	30.368615
438.364831	21364.343949	30.373632
438.947311	21395.068748	30.378650
439.258666	21426.046761	30.383668
439.440329	21476.053610	30.388685
440.129764	21499.525311	30.393703
440.137814	21538.457971	30.398720
440.616212	21573.695603	30.403738
441.151498	21601.656744	30.408756
441.005490	21664.423809	30.413773
441.717534	21684.801626	30.418791
441.950472	21733.001669	30.423808
442.212568	21766.419812	30.428826
442.867839	21808.924126	30.433844
443.683684	21841.693855	30.438861
444.273259	21874.956909	30.443879
444.755544	21902.887934	30.448896
445.062447	21948.457323	30.453914
445.594126	21972.480945	30.458932
446.050226	21999.993908	30.463949
446.798195	22034.027232	30.468967
447.306726	22066.134167	30.473984
447.994587	22094.277339	30.479002
448.614586	22117.412968	30.484020
449.010338	22138.925533	30.489037
449.743920	22155.957586	30.494055
450.292012	22179.098936	30.499072
450.403967	22204.064558	30.504090
450.735768	22226.305290	30.509108
450.862144	22256.259105	30.514125
451.167421	22268.526415	30.519143
451.460945	22296.364876	30.524160
451.905214	22331.444195	30.529178
452.508460	22355.861711	30.534196
452.550793	22397.811787	30.539213
452.671426	22415.862026	30.544231
453.099049	22454.760217	30.549248
453.476016	22495.005619	30.554266
454.273191	22529.302980	30.559284
454.418967	22577.636587	30.564301
455.047288	22605.615475	30.569319
455.300337	22659.163373	30.574336
455.769980	22693.518619	30.579354
455.967643	22742.798057	30.584372
456.271398	22780.391455	30.589389
456.827958	22823.968037	30.594407
456.710433	22883.824040	30.599424
457.073618	22944.805124	30.604442
458.202384	22994.193978	30.609460
458.506597	23047.395577	30.614477
459.526895	23089.558645	30.619495
459.693980	23129.898754	30.624512
460.264039	23174.129968	30.629530
460.943195	23221.299815	30.634548
461.374911	23264.895109	30.639565
462.207836	23301.326340	30.644583
462.371485	23340.007062	30.649600
462.955662	23380.597022	30.654618
463.706778	23413.177129	30.659636
463.839703	23464.380599	30.664653
464.407499	23495.926907	30.669671
464.940437	23542.426517	30.674688
465.459680	23587.149778	30.679706
466.126606	23617.415169	30.684724
466.503907	23662.316739	30.689741
466.892579	23693.664512	30.694759
467.581127	23730.801871	30.699776
467.847732	23765.921544	30.704794
468.453614	23810.083808	30.709812
468.599276	23847.428280	30.714829
468.984878	23893.981704	30.719847
469.652783	23943.076127	30.724864
469.938722	23997.799166	30.729882
470.494841	24031.892019	30.734900
470.811381	24070.131112	30.739917
471.705553	24107.306104	30.744935
472.405523	24143.305481	30.749952
472.810142	24184.867046	30.754970
473.253784	24214.118749	30.759988
473.564677	24250.375361	30.765005
474.670188	24287.402105	30.770023
475.127681	24325.233578	30.775040
474.979145	24367.830489	30.780058
475.406245	24393.395116	30.785076
476.138856	24440.040632	30.790093
476.672044	24473.598848	30.795111
476.966925	24505.367398	30.800128
477.610838	24542.291583	30.805146
478.276899	24565.795074	30.810164
478.872888	24606.632003	30.815181
479.296265	24636.733067	30.820199
479.760616	24673.942834	30.825216
480.693974	24703.590298	30.830234
481.430097	24725.937466	30.835252
481.606951	24751.834361	30.840269
482.185267	24761.146959	30.845287
482.722812	24788.453784	30.850304
483.178423	24798.493284	30.855322
483.369834	24823.908458	30.860340
483.862386	24854.039420	30.865357
484.051001	24875.701819	30.870375
484.223083	24906.277199	30.875392
484.895728	24936.144996	30.880410
485.361931	24959.067180	30.885428
485.323637	24996.487291	30.890445
486.124995	25034.594402	30.895463
486.398501	25066.017440	30.900480
486.672958	25107.347382	30.905498
487.021841	25142.811053	30.910516
487.210080	25195.570218	30.915533
487.577942	25242.546601	30.920551
488.020303	25289.781994	30.925568
488.111845	25360.100986	30.930586
488.343517	25411.610869	30.935604
489.181053	25470.350550	30.940621
489.928494	25510.603040	30.945639
490.928679	25551.744131	30.950656
491.406771	25615.004008	30.955674
492.253647	25648.111847	30.960692
492.461417	25696.377735	30.965709
492.907995	25747.310409	30.970727
493.548721	25790.120418	30.975744
494.184918	25838.037979	30.980762
494.557750	25886.299065	30.985780
494.889658	25925.937071	30.990797
495.710275	25967.058513	30.995815
496.707373	26005.580023	31.000832
496.693250	26046.644723	31.005850
497.291955	26085.390290	31.010868
497.954243	26131.512708	31.015885
498.445406	26176.121223	31.020903
498.739342	26216.415987	31.025920
499.098006	26267.143999	31.030938
500.132614	26299.042206	31.035956
500.561560	26349.238325	31.040973
500.812191	26386.436827	31.045991
501.260825	26425.501435	31.051008
501.797828	26474.342535	31.056026
502.310446	26525.774391	31.061044
502.968833	26555.467577	31.066061
503.194830	26609.060703	31.071079
504.172447	26640.732432	31.076096
504.173786	26687.776781	31.081114
504.572632	26728.941699	31.086132
505.312283	26784.462564	31.091149
505.666055	26827.764424	31.096167
506.196590	26875.241873	31.101184
506.286459	26930.539906	31.106202
507.134933	26971.413075	31.111220
507.546957	27040.247263	31.116237
507.523902	27097.403624	31.121255
508.111383	27142.509661	31.126272
508.943949	27194.237362	31.131290
509.108128	27248.177106	31.136308
509.711129	27309.731645	31.141325
510.038403	27361.714105	31.146343
510.694349	27414.172095	31.151360
511.230345	27476.255693	31.156378
511.881038	27530.128134	31.161396
512.296466	27595.900908	31.166413
512.680148	27645.051529	31.171431
513.367401	27714.337949	31.176448
513.685006	27775.070874	31.181466
514.215335	27819.866398	31.186484
514.795456	27881.117613	31.191501
515.168130	27945.996597	31.196519
515.974115	27981.478515	31.201536
516.363359	28040.276153	31.206554
516.933303	28088.990149	31.211572
517.593398	28122.420833	31.216589
517.955158	28175.879529	31.221607
518.988020	28211.248527	31.226624
519.557702	28267.086288	31.231642
519.870533	28320.048806	31.236660
520.516679	28358.649626	31.241677
520.763689	28401.704994	31.246695
521.418247	28447.863261	31.251712
522.456317	28481.768166	31.256730
522.647396	28528.060402	31.261748
523.452968	28572.215913	31.266765
523.429860	28626.099545	31.271783
524.386732	28661.901663	31.276800
524.544234	28721.670735	31.281818
525.125760	28766.788290	31.286836
525.542480	28818.514177	31.291853
525.990276	28871.585302	31.296871
526.617506	28906.758080	31.301888
527.320963	28968.689848	31.306906
527.734246	29007.731437	31.311924
528.377661	29066.821582	31.316941
528.662174	29121.482216	31.321959
529.452140	29162.158891	31.326976
529.614865	29227.610676	31.331994
530.444089	29278.979177	31.337012
530.780360	29332.104925	31.342029
531.112835	29375.798404	31.347047
532.259867	29431.553478	31.352064
533.128927	29483.802488	31.357082
533.975702	29517.078654	31.362100
534.555687	29559.308631	31.367117
534.686171	29608.405879	31.372135
535.437042	29641.231282	31.377152
535.713456	29678.293727	31.382170
536.552669	29717.133662	31.387188
537.145321	29754.251019	31.392205
537.649289	29800.106604	31.397223
537.998573	29846.167830	31.402240
538.784595	29891.292189	31.407258
538.969875	29939.210773	31.412276
539.502425	29984.607779	31.417293
539.548597	30032.303629	31.422311
540.364572	30080.808804	31.427328
541.048056	30142.725961	31.432346
541.467444	30197.509529	31.437364
542.163953	30231.547129	31.442381
542.384844	30277.946312	31.447399
543.143466	30328.973104	31.452416
544.031225	30366.727396	31.457434
544.373925	30407.601137	31.462452
545.114890	30464.774148	31.467469
545.499091	30515.343074	31.472487
546.145839	30561.022339	31.477504
546.363670	30591.126866	31.482522
546.929155	30651.399526	31.487540
547.762486	30686.453316	31.492557
548.043205	30747.877882	31.497575
548.870543	30799.213296	31.502592
549.065303	30845.097719	31.507610
549.798149	30892.546198	31.512628
550.723999	30938.823746	31.517645
550.575034	30984.383838	31.522663
551.375734	31031.180926	31.527680
551.841376	31082.264869	31.532698
551.866204	31140.890486	31.537716
552.774189	31188.197092	31.542733
552.761061	31245.665092	31.547751
553.257466	31299.700983	31.552768
553.814184	31353.313689	31.557786
554.505615	31422.462649	31.562804
554.973970	31466.574184	31.567821
555.321432	31527.125843	31.572839
555.825936	31585.528136	31.577856
556.420940	31646.048560	31.582874
556.976378	31708.333257	31.587892
557.625180	31758.167643	31.592909
557.927321	31821.693814	31.597927
558.541793	31893.495234	31.602944
559.049833	31947.515397	31.607962
559.825838	32015.649238	31.612980
561.035799	32071.970212	31.617997
561.193827	32133.407347	31.623015
562.233934	32177.245855	31.628032
563.268562	32217.885828	31.633050
563.704237	32273.503003	31.638068
564.453871	32306.970983	31.643085
564.967141	32366.365192	31.648103
565.510852	32409.854418	31.653120
565.946271	32468.267941	31.658138
566.454135	32513.798622	31.663156
567.154236	32555.350045	31.668173
567.357060	32618.949208	31.673191
567.695737	32672.072002	31.678208
568.514981	32722.240523	31.683226
569.050030	32789.903014	31.688244
569.887083	32821.252745	31.693261
570.710558	32875.258066	31.698279
571.703612	32917.099328	31.703296
572.195860	32964.896255	31.708314
572.547650	33016.074107	31.713332
573.231194	33055.253345	31.718349
573.775893	33114.076842	31.723367
573.802126	33152.999404	31.728384
574.591454	33198.819590	31.733402
575.260407	33254.524167	31.738420
575.984094	33297.010612	31.743437
576.606905	33349.252022	31.748455
577.404674	33382.783465	31.753472
578.297429	33424.450089	31.758490
578.773149	33456.870737	31.763508
579.572934	33501.913693	31.768525
579.736590	33542.067060	31.773543
580.181802	33587.462583	31.778560
580.758885	33627.954567	31.783578
581.104811	33687.087504	31.788596
581.867573	33735.482175	31.793613
581.852366	33782.835415	31.798631
582.808951	33836.707950	31.803648
583.337276	33900.405954	31.808666
583.488423	33955.842116	31.813684
584.024403	34010.182635	31.818701
584.503908	34073.829404	31.823719
584.757557	34131.290831	31.828736
585.546683	34189.171597	31.833754
586.069129	34271.064669	31.838772
586.896666	34326.399130	31.843789
587.391364	34375.834112	31.848807
587.955078	34434.062365	31.853824
589.056746	34493.776214	31.858842
589.321577	34560.688726	31.863860
589.647215	34609.180441	31.868877
590.213314	34677.239410	31.873895
590.771228	34736.277497	31.878912
591.768544	34791.357986	31.883930
591.730660	34849.248824	31.888948
592.657406	34898.856508	31.893965
592.714062	34968.121501	31.898983
593.421463	35034.125985	31.904000
593.954463	35092.714936	31.909018
593.945155	35169.666774	31.914036
594.676536	35225.730057	31.919053
595.204817	35304.587739	31.924071
595.685034	35371.047766	31.929088
596.455758	35438.027871	31.934106
596.830366	35529.712577	31.939124
597.611653	35598.285285	31.944141
598.694938	35672.842354	31.949159
599.195564	35733.821540	31.954176
600.469681	35799.725265	31.959194
601.356575	35858.624045	31.964212
602.485655	35909.406525	31.969229
602.868376	35957.002397	31.974247
603.400589	36009.478067	31.979264
604.509871	36045.986276	31.984282
605.338446	36106.931207	31.989300
606.083692	36137.749704	31.994317
606.421640	36189.232432	31.999335
607.119546	36234.857809	32.004352
607.919509	36281.286939	32.009370
608.101544	36324.186121	32.014388
608.958400	36373.332912	32.019405
609.737642	36419.989924	32.024423
609.546343	36476.216625	32.029440
610.573919	36515.210602	32.034458
610.882549	36572.112061	32.039476
611.305942	36621.281005	32.044493
611.342093	36692.847392	32.049511
612.106828	36756.064930	32.054528
612.664207	36805.480402	32.059546
613.123792	36890.810824	32.064564
613.802124	36950.947158	32.069581
614.331901	37023.483904	32.074599
614.415457	37094.229698	32.079616
615.168876	37155.266395	32.084634
615.605427	37250.083696	32.089652
616.105663	37320.691747	32.094669
616.739139	37399.556889	32.099687
617.088748	37481.704718	32.104704
617.875133	37570.534913	32.109722
618.008012	37658.666031	32.114740
618.847988	37741.308062	32.119757
620.420179	37814.321933	32.124775
620.995693	37888.281213	32.129792
621.657160	37949.234844	32.134810
622.310889	38035.510572	32.139828
623.195580	38098.895943	32.144845
623.521758	38174.188756	32.149863
624.457668	38240.580500	32.154880
625.051979	38296.638192	32.159898
625.767094	38371.971405	32.164916
626.573562	38437.157497	32.169933
627.215715	38500.063720	32.174951
627.780441	38576.972581	32.179968
628.710425	38625.674586	32.184986
629.196945	38700.340056	32.190004
630.371998	38755.175856	32.195021
631.107049	38807.856368	32.200039
631.814349	38854.768329	32.205056
632.593140	38908.998045	32.210074
632.916462	38967.539650	32.215092
633.730522	39019.039727	32.220109
634.226045	39061.855436	32.225127
634.798981	39106.852217	32.230144
635.724716	39149.738747	32.235162
635.890027	39199.639335	32.240180
636.476269	39242.077395	32.245197
636.982556	39288.430404	32.250215
637.389313	39347.240309	32.255232
637.992552	39415.756000	32.260250
638.231875	39481.472448	32.265268
638.962352	39531.062290	32.270285
640.076373	39581.715514	32.275303
640.755264	39637.984246	32.280320
641.606722	39688.542468	32.285338
642.192312	39736.319734	32.290356
642.694533	39802.135731	32.295373
643.684792	39840.095026	32.300391
644.721011	39886.320523	32.305408
645.594161	39930.754939	32.310426
646.081060	39983.173838	32.315444
646.374234	40034.176107	32.320461
647.136596	40088.936069	32.325479
647.453815	40139.656844	32.330496
647.906732	40195.270319	32.335514
648.428560	40258.278327	32.340532
649.092403	40331.484666	32.345549
649.937086	40377.657971	32.350567
650.123565	40440.138273	32.355584
650.796216	40495.690918	32.360602
651.544299	40564.600391	32.365620
652.037983	40639.398839	32.370637
652.638514	40709.864425	32.375655
653.014184	40779.051199	32.380672
653.986780	40845.629402	32.385690
654.417620	40913.446905	32.390708
655.345922	40977.090713	32.395725
656.096752	41040.590577	32.400743
656.479112	41116.770074	32.405760
657.210712	41182.862302	32.410778
658.029535	41257.246222	32.415796
658.018068	41331.575722	32.420813
659.081105	41407.371903	32.425831
659.573184	41488.320691	32.430848
660.424417	41566.564632	32.435866
661.085873	41641.067778	32.440884
661.506837	41712.523577	32.445901
661.996897	41789.985502	32.450919
662.617531	41872.442633	32.455936
663.138838	41957.912682	32.460954
663.657916	42048.523230	32.465972
663.926068	42130.291800	32.470989
665.126408	42213.749712	32.476007
665.905338	42299.213287	32.481024
666.360641	42383.929072	32.486042
667.427186	42465.534988	32.491060
668.098992	42554.796642	32.496077
669.020690	42620.092084	32.501095
669.575572	42705.594726	32.506112
670.724572	42775.402497	32.511130
671.362984	42852.414840	32.516148
671.938357	42931.521743	32.521165
672.586946	43001.119821	32.526183
673.014773	43082.544024	32.531200
673.763451	43150.875769	32.536218
674.170669	43241.775909	32.541236
674.766278	43315.513691	32.546253
675.613600	43397.892586	32.551271
676.099751	43480.707532	32.556288
676.378189	43556.529086	32.561306
677.281134	43637.993649	32.566324
677.731891	43721.011290	32.571341
678.752152	43786.316557	32.576359
678.831513	43870.694208	32.581376
679.780998	43946.617476	32.586394
680.414535	44033.155082	32.591412
681.028785	44105.563609	32.596429
682.054796	44191.146387	32.601447
682.583720	44277.178352	32.606464
683.498176	44362.695183	32.611482
684.112902	44437.602479	32.616500
684.646610	44513.998078	32.621517
685.552745	44591.822503	32.626535
686.210939	44681.194454	32.631552
687.337313	44749.952434	32.636570
688.136419	44825.177994	32.641588
688.334774	44913.421208	32.646605
689.299260	44981.903788	32.651623
690.142961	45065.411558	32.656640
690.730220	45129.659819	32.661658
691.571722	45206.111331	32.666676
692.420342	45291.946454	32.671693
693.266669	45353.582155	32.676711
693.761543	45430.628926	32.681728
694.420268	45513.171573	32.686746
695.272869	45588.517609	32.691764
695.877922	45671.271950	32.696781
696.746940	45731.035762	32.701799
697.461208	45807.040337	32.706816
698.218984	45882.567493	32.711834
699.063717	45953.227061	32.716852
700.038258	46018.733991	32.721869
701.505752	46069.355710	32.726887
702.525030	46120.863527	32.731904
703.243078	46182.220088	32.736922
703.598801	46216.385277	32.741940
704.146638	46298.040322	32.746957
704.798735	46331.329170	32.751975
705.532739	46401.007773	32.756992
706.249109	46452.926775	32.762010
706.885173	46521.883151	32.767028
707.011481	46595.487501	32.772045
708.067180	46650.107513	32.777063
708.466848	46728.432206	32.782080
708.787466	46803.325092	32.787098
709.368219	46881.857195	32.792116
709.759697	46962.836849	32.797133
710.599934	47048.403442	32.802151
711.146748	47128.606427	32.807168
711.585748	47226.556401	32.812186
712.220765	47306.413906	32.817204
712.420298	47411.491069	32.822221
713.318248	47505.804077	32.827239
713.753246	47606.627292	32.832256
714.616872	47690.073857	32.837274
716.003911	47786.634529	32.842292
716.198118	47877.548144	32.847309
717.103593	47962.413241	32.852327
717.927417	48068.429385	32.857344
718.455957	48160.839467	32.862362
719.587669	48244.903998	32.867380
719.627529	48344.217643	32.872397
720.747144	48423.740406	32.877415
721.464897	48530.319923	32.882432
722.262108	48611.886640	32.887450
723.107454	48710.781068	32.892468
723.661131	48802.258404	32.897485
724.417268	48882.386629	32.902503
725.404896	48963.190521	32.907520
726.679776	49030.442373	32.912538
727.938762	49090.745761	32.917556
728.571298	49155.104339	32.922573
729.360695	49228.561377	32.927591
730.203368	49294.597328	32.932608
730.494065	49360.810416	32.937626
730.722049	49428.426961	32.942644
731.369316	49521.051288	32.947661
731.996062	49593.083888	32.952679
732.602083	49678.757988	32.957696
732.865285	49772.713787	32.962714
733.879744	49852.954779	32.967732
734.075480	49944.474864	32.972749
734.726741	50047.555375	32.977767
735.416235	50144.562735	32.982784
736.407766	50246.125462	32.987802
737.124999	50346.085540	32.992820
737.825784	50439.125469	32.997837
738.219728	50527.529572	33.002855
739.131853	50637.565999	33.007872
740.121396	50732.094439	33.012890
741.148127	50825.663287	33.017908
741.814143	50926.759311	33.022925
742.811624	51025.292924	33.027943
743.633249	51113.729779	33.032960
744.453573	51208.465519	33.037978
745.252072	51298.505312	33.042996
746.080680	51390.145113	33.048013
746.500813	51489.958263	33.053031
747.299096	51589.784957	33.058048
747.666114	51687.497945	33.063066
748.883472	51783.440371	33.068084
749.218671	51877.994579	33.073101
750.033714	51981.257184	33.078119
751.111021	52081.362272	33.083136
751.803577	52178.006562	33.088154
753.291927	52252.174015	33.093172
754.198264	52361.033470	33.098189
754.752370	52448.838507	33.103207
755.594918	52530.480575	33.108224
756.284271	52626.887550	33.113242
757.478547	52689.240893	33.118260
758.330412	52778.236251	33.123277
758.818051	52867.216665	33.128295
759.605210	52948.143131	33.133312
760.696986	53028.507623	33.138330
761.555825	53114.325497	33.143348
762.850022	53179.803785	33.148365
765.040593	53197.913738	33.153383
766.956921	53240.064510	33.158400
767.827309	53281.864619	33.163418
768.696043	53295.443043	33.168436
769.186155	53344.230824	33.173453
769.599081	53385.437395	33.178471
770.273166	53401.347929	33.183488
770.742515	53455.509673	33.188506
771.784263	53486.932985	33.193524
772.248268	53531.271408	33.198541
772.493421	53572.657855	33.203559
772.776201	53622.024092	33.208576
773.285436	53697.882220	33.213594
773.687363	53756.409105	33.218612
773.830874	53824.544606	33.223629
774.538811	53909.405398	33.228647
775.267303	53975.934293	33.233664
775.597726	54052.366829	33.238682
776.031851	54130.311441	33.243700
776.292320	54225.818164	33.248717
777.323623	54304.656291	33.253735
777.795320	54394.834103	33.258752
778.164652	54480.676029	33.263770
779.156811	54560.734788	33.268788
779.903353	54654.374819	33.273805
780.404443	54755.416928	33.278823
781.314562	54837.019471	33.283840
782.246637	54945.554121	33.288858
783.296592	55028.208373	33.293876
783.832112	55128.008256	33.298893
784.966005	55218.610658	33.303911
786.152281	55319.504000	33.308928
786.680261	55393.444701	33.313946
787.450644	55488.316845	33.318964
788.104530	55594.177917	33.323981
788.586652	55703.991957	33.328999
789.629641	55794.384612	33.334016
789.929810	55904.861835	33.339034
790.230716	56000.616837	33.344052
790.916386	56123.175936	33.349069
791.491445	56236.591842	33.354087
792.212242	56359.727899	33.359104
792.746073	56474.624300	33.364122
793.807051	56593.357925	33.369140
795.180986	56710.839701	33.374157
795.708540	56825.499045	33.379175
796.524604	56950.329071	33.384192
797.238727	57081.053560	33.389210
797.868144	57203.723423	33.394228
798.848149	57330.247414	33.399245
799.628294	57439.244280	33.404263
801.132736	57547.186263	33.409280
802.114265	57671.753194	33.414298
803.674088	57768.666348	33.419316
804.422119	57880.729498	33.424333
804.972075	57983.271241	33.429351
805.878264	58082.417724	33.434368
806.717029	58190.549505	33.439386
807.538890	58288.276488	33.444404
808.049847	58403.175114	33.449421
809.200632	58519.048834	33.454439
809.941851	58619.059529	33.459456
810.680923	58727.292897	33.464474
811.865706	58823.546644	33.469492
812.555528	58941.249852	33.474509
813.045630	59048.869026	33.479527
813.627959	59143.720209	33.484544
814.172453	59272.843980	33.489562
815.271214	59389.957380	33.494580
816.011641	59499.540786	33.499597
816.356237	59619.972229	33.504615
817.799318	59728.745056	33.509632
818.317659	59840.357948	33.514650
819.307153	59952.708529	33.519668
820.352719	60065.454908	33.524685
821.350016	60176.731029	33.529703
822.739198	60279.012408	33.534720
823.605519	60370.674788	33.539738
825.191318	60454.336923	33.544756
826.129790	60545.583627	33.549773
827.059872	60634.019639	33.554791
828.166653	60717.345235	33.559808
828.715858	60811.394408	33.564826
829.452022	60895.351074	33.569844
830.218680	60968.659611	33.574861
830.765401	61059.278409	33.579879
832.176329	61140.905647	33.584896
832.908245	61207.786677	33.589914
834.121623	61267.376424	33.594932
834.559641	61336.322868	33.599949
835.008654	61422.882823	33.604967
835.679262	61490.596616	33.609984
836.414424	61585.250539	33.615002
836.929079	61660.113990	33.620020
837.956793	61747.084906	33.625037
838.203298	61836.391742	33.630055
839.029330	61923.093493	33.635072
839.454349	62036.099154	33.640090
840.483833	62127.780274	33.645108
841.119475	62235.379502	33.650125
841.916745	62349.829431	33.655143
842.637170	62434.831634	33.660160
843.304391	62554.329300	33.665178
844.325681	62648.536109	33.670196
845.182462	62768.129971	33.675213
845.766609	62878.673997	33.680231
847.274305	62977.877268	33.685248
847.947026	63089.393789	33.690266
848.947353	63190.907282	33.695284
849.677185	63306.227060	33.700301
849.934494	63414.110160	33.705319
851.229737	63530.348714	33.710336
851.969301	63648.557533	33.715354
852.798644	63762.706574	33.720372
853.935590	63865.787325	33.725389
854.705001	63982.513935	33.730407
855.874078	64093.947173	33.735424
856.662188	64214.388898	33.740442
857.193367	64323.900108	33.745460
858.392015	64451.095799	33.750477
859.092929	64548.803289	33.755495
860.230127	64658.297856	33.760512
861.437569	64774.608542	33.765530
862.228499	64883.776160	33.770548
863.147121	64993.751280	33.775565
864.266445	65092.896410	33.780583
865.426656	65194.488010	33.785600
866.394067	65294.955247	33.790618
867.291668	65396.616707	33.795636
867.921431	65497.121994	33.800653
868.336542	65610.698806	33.805671
868.970813	65722.159998	33.810688
869.473209	65833.706890	33.815706
870.694240	65948.119009	33.820724
871.784309	66036.254519	33.825741
872.119779	66162.402769	33.830759
873.111849	66280.831185	33.835776
873.753397	66404.843854	33.840794
874.631695	66531.814595	33.845812
875.513404	66656.509599	33.850829
876.274855	66781.143116	33.855847
877.854631	66888.989081	33.860864
878.733549	66995.516795	33.865882
879.549239	67111.355477	33.870900
880.340069	67216.014915	33.875917
881.130169	67340.526868	33.880935
882.368904	67456.126533	33.885952
883.279701	67565.168108	33.890970
884.037378	67684.047959	33.895988
885.373790	67782.556518	33.901005
885.964043	67912.927938	33.906023
886.967812	68005.600245	33.911040
887.535842	68130.248548	33.916058
888.086330	68226.215200	33.921076
889.112831	68350.782387	33.926093
889.576340	68466.573146	33.931111
890.699398	68575.572057	33.936128
891.158265	68687.672380	33.941146
891.502946	68811.154124	33.946164
892.656664	68926.421863	33.951181
893.383614	69052.844863	33.956199
894.368305	69172.093715	33.961216
895.124795	69299.588154	33.966234
895.689892	69424.244534	33.971252
896.907425	69550.361443	33.976269
897.630265	69682.884153	33.981287
898.438844	69808.855481	33.986304
900.000671	69938.793539	33.991322
901.020665	70061.810033	33.996340
901.966648	70173.622339	34.001357
903.115992	70298.199500	34.006375
904.024703	70413.478001	34.011392
905.398595	70544.051630	34.016410
905.900666	70662.535268	34.021428
906.857961	70793.780265	34.026445
907.565985	70922.873242	34.031463
908.681421	71034.649270	34.036480
909.397276	71161.503914	34.041498
909.926085	71300.215157	34.046516
910.700131	71424.620850	34.051533
911.366863	71574.332770	34.056551
912.415159	71713.542220	34.061568
913.929314	71843.189868	34.066586
914.910402	71971.788512	34.071604
915.866875	72091.709618	34.076621
917.053213	72225.284046	34.081639
917.699288	72358.594833	34.086656
918.453650	72493.501031	34.091674
919.322955	72624.967807	34.096692
920.110426	72752.660972	34.101709
920.697945	72905.980873	34.106727
922.566046	73031.238705	34.111744
923.642825	73161.377890	34.116762
924.389279	73295.335461	34.121780
925.426406	73427.892269	34.126797
926.280658	73568.050168	34.131815
926.758316	73690.791576	34.136832
927.911471	73824.141025	34.141850
928.733201	73964.888693	34.146868
929.397958	74102.178658	34.151885
930.499216	74236.000903	34.156903
931.098063	74380.557507	34.161920
931.948630	74529.392831	34.166938
932.882420	74665.743620	34.171956
934.315327	74795.264242	34.176973
935.463047	74933.092732	34.181991
936.492678	75077.285183	34.187008
937.599276	75200.050833	34.192026
938.704762	75351.594284	34.197044
939.971111	75453.944326	34.202061
941.058495	75574.773593	34.207079
941.941866	75703.157454	34.212096
943.463596	75819.045957	34.217114
944.119022	75945.900523	34.222132
944.787034	76047.922534	34.227149
945.657503	76187.714976	34.232167
946.446911	76315.732174	34.237184
946.961229	76441.841364	34.242202
947.565481	76584.564651	34.247220
948.377940	76715.970511	34.252237
948.922654	76865.903331	34.257255
949.554537	77007.638046	34.262272
950.999363	77152.666968	34.267290
951.226009	77297.064073	34.272308
952.391081	77442.931958	34.277325
953.466554	77570.567352	34.282343
954.511860	77704.982851	34.287360
955.631184	77834.307651	34.292378
956.244175	77984.198712	34.297396
956.789435	78127.744995	34.302413
957.555405	78282.552801	34.307431
958.639380	78427.491759	34.312448
959.763826	78584.361198	34.317466
960.795983	78735.560364	34.322484
962.246589	78867.670014	34.327501
963.082056	79012.578085	34.332519
964.697741	79155.023437	34.337536
965.691223	79286.344789	34.342554
967.020158	79418.730900	34.347572
968.337124	79539.619483	34.352589
969.821588	79661.081874	34.357607
970.809999	79785.391639	34.362624
972.326939	79893.584569	34.367642
973.264696	80011.647681	34.372660
974.540514	80121.558088	34.377677
975.838905	80235.425350	34.382695
976.719984	80339.708936	34.387712
977.459110	80452.487134	34.392730
978.148903	80561.642910	34.397748
978.823021	80683.656467	34.402765
979.591161	80808.906715	34.407783
979.876600	80932.586622	34.412800
980.819234	81062.566601	34.417818
981.394709	81213.529175	34.422836
982.206979	81345.664352	34.427853
983.209895	81505.661472	34.432871
983.868891	81653.829513	34.437888
984.520483	81813.861787	34.442906
984.972379	81974.978512	34.447924
986.152906	82139.980144	34.452941
986.800673	82302.458504	34.457959
987.641349	82472.466296	34.462976
989.289812	82630.636999	34.467994
990.617598	82802.742775	34.473012
992.062963	82938.331371	34.478029
993.591024	83084.409488	34.483047
994.786342	83232.713847	34.488064
996.035409	83367.559350	34.493082
996.643402	83523.207286	34.498100
997.729452	83653.330013	34.503117
998.935709	83810.437036	34.508135
999.992553	83940.756040	34.513152
1001.741183	84059.325553	34.518170
1002.780559	84203.074920	34.523188
1004.321629	84306.919072	34.528205
1005.909383	84432.546616	34.533223
1006.718439	84537.456014	34.538240
1008.216532	84651.571520	34.543258
1009.260630	84753.285619	34.548276
1009.868289	84858.868940	34.553293
1010.895016	84972.172095	34.558311
1011.555822	85093.344437	34.563328
1012.669352	85211.006532	34.568346
1013.163696	85330.796731	34.573364
1014.214960	85447.274475	34.578381
1015.108822	85570.441727	34.583399
1015.907697	85698.788619	34.588416
1016.946634	85815.055111	34.593434
1017.232940	85940.995342	34.598452
1018.345503	86080.865376	34.603469
1019.569017	86210.872049	34.608487
1020.045089	86340.269459	34.613504
1021.327682	86451.322656	34.618522
1021.558925	86594.575444	34.623540
1022.321577	86730.084330	34.628557
1023.402986	86867.357184	34.633575
1024.106676	87025.682966	34.638592
1025.006631	87166.803365	34.643610
1025.624489	87323.968406	34.648628
1026.308082	87476.048556	34.653645
1027.649049	87641.505592	34.658663
1028.026632	87802.573770	34.663680
1029.271536	87965.384902	34.668698
1030.413483	88138.630356	34.673716
1031.352372	88294.970215	34.678733
1032.553493	88470.049774	34.683751
1033.549034	88630.198363	34.688768
1034.934424	88807.009089	34.693786
1035.770711	88965.895386	34.698804
1036.483384	89137.561319	34.703821
1037.948358	89303.097958	34.708839
1038.833815	89491.489184	34.713856
1040.015172	89664.618964	34.718874
1040.903383	89833.463551	34.723892
1041.924606	90022.690790	34.728909
1042.769391	90192.734898	34.733927
1043.847080	90385.094654	34.738944
1045.111995	90558.514474	34.743962
1046.073908	90742.327127	34.748980
1047.316099	90918.778495	34.753997
1048.522022	91089.908220	34.759015
1049.353853	91280.600783	34.764032
1050.858481	91472.113584	34.769050
1052.106254	91637.202355	34.774068
1053.081276	91816.217246	34.779085
1054.376253	91976.597970	34.784103
1055.249889	92167.100701	34.789120
1056.446415	92335.728098	34.794138
1057.707602	92493.712730	34.799156
1059.360535	92664.538894	34.804173
1061.805109	92794.834531	34.809191
1062.903276	92941.627156	34.814208
1064.474885	93077.240272	34.819226
1065.322860	93223.487466	34.824244
1066.474328	93357.874307	34.829261
1067.611890	93484.478854	34.834279
1068.519681	93631.129981	34.839296
1069.431976	93765.432152	34.844314
1070.325226	93900.295227	34.849332
1071.091488	94061.593910	34.854349
1072.463147	94198.233845	34.859367
1072.877353	94351.965522	34.864384
1073.947845	94497.594724	34.869402
1074.747041	94661.544061	34.874420
1075.765652	94804.012427	34.879437
1076.564115	94963.153178	34.884455
1077.431531	95128.404590	34.889472
1078.633142	95294.810689	34.894490
1080.252990	95449.311320	34.899508
1081.432492	95602.259144	34.904525
1082.952641	95738.585457	34.909543
1084.276196	95886.605289	34.914560
1085.450781	96031.333697	34.919578
1086.621864	96155.718165	34.924596
1088.084228	96298.520304	34.929613
1089.847192	96420.047899	34.934631
1090.891628	96546.797544	34.939648
1092.227983	96666.865184	34.944666
1092.994516	96784.945245	34.949684
1093.590050	96904.377291	34.954701
1094.656640	97030.878832	34.959719
1095.051302	97155.707296	34.964736
1095.787871	97278.871706	34.969754
1096.861682	97424.530176	34.974772
1097.205917	97561.454047	34.979789
1098.292383	97715.221583	34.984807
1098.899462	97877.020907	34.989824
1099.267776	98026.952832	34.994842
1100.135788	98205.860850	34.999860
1100.928331	98385.485376	35.004877
1102.305356	98567.413595	35.009895
1102.884572	98738.896585	35.014912
1104.106024	98932.331126	35.019930
1105.160525	99099.160441	35.024948
1106.457669	99292.066030	35.029965
1107.992914	99472.942547	35.034983
1108.556680	99676.374663	35.040000
1110.037774	99847.981422	35.045018
1111.828460	100013.384050	35.050036
1113.220841	100190.965494	35.055053
1114.666782	100356.471862	35.060071
1116.043732	100525.150079	35.065088
1117.558223	100704.012752	35.070106
1118.878202	100866.972787	35.075124
1119.716262	101028.241005	35.080141
1120.953183	101184.011647	35.085159
1121.882450	101359.018800	35.090176
1122.585110	101525.745053	35.095194
1124.156754	101695.835930	35.100212
1124.792579	101870.401373	35.105229
1126.003594	102046.316196	35.110247
1127.478316	102215.964367	35.115264
1128.364318	102384.077722	35.120282
1129.704820	102562.690909	35.125300
1130.045922	102752.703861	35.130317
1131.282894	102931.628028	35.135335
1132.343728	103113.381372	35.140352
1133.153037	103298.919927	35.145370
1134.391577	103496.926050	35.150388
1135.131953	103707.914807	35.155405
1135.986725	103892.455897	35.160423
1137.135647	104094.489662	35.165440
1137.949943	104297.302375	35.170458
1139.439494	104505.627708	35.175476
1140.077207	104714.020023	35.180493
1142.281728	104898.774870	35.185511
1143.717898	105102.934415	35.190528
1144.814556	105296.247326	35.195546
1146.153652	105490.053365	35.200564
1147.092657	105683.686561	35.205581
1148.379852	105888.776120	35.210599
1149.676457	106089.812793	35.215616
1150.725768	106275.592164	35.220634
1151.872412	106469.703267	35.225652
1152.776413	106670.302841	35.230669
1153.786773	106860.259744	35.235687
1155.250917	107075.233687	35.240704
1156.291784	107264.403123	35.245722
1157.828696	107458.292019	35.250740
1158.461910	107654.219483	35.255757
1160.024634	107841.203850	35.260775
1161.030852	108042.810049	35.265792
1162.250153	108236.630595	35.270810
1163.522300	108427.175825	35.275828
1164.728931	108631.881801	35.280845
1166.060886	108816.884581	35.285863
1167.425701	109009.723879	35.290880
1168.401883	109174.762042	35.295898
1170.215959	109334.570129	35.300916
1171.237405	109519.147878	35.305933
1171.993752	109691.078479	35.310951
1173.162330	109869.300677	35.315968
1174.230430	110046.045980	35.320986
1175.324099	110226.588375	35.326004
1176.764668	110407.720454	35.331021
1177.651329	110581.155134	35.336039
1178.673888	110773.835698	35.341056
1179.800488	110969.603927	35.346074
1180.242191	111157.696519	35.351092
1181.183618	111373.678034	35.356109
1182.080382	111576.139317	35.361127
1182.915957	111782.336631	35.366144
1183.540009	112018.163278	35.371162
1185.236997	112223.017515	35.376180
1185.868987	112461.278918	35.381197
1187.150126	112682.484331	35.386215
1188.825970	112904.753530	35.391232
1189.504313	113141.416843	35.396250
1190.597703	113369.981337	35.401268
1191.748188	113606.658958	35.406285
1193.190155	113845.139897	35.411303
1194.398234	114086.144801	35.416320
1195.373068	114331.662683	35.421338
1197.370012	114554.411179	35.426356
1198.536939	114802.371815	35.431373
1200.077779	115032.624013	35.436391
1201.265867	115262.518508	35.441408
1202.430711	115494.825970	35.446426
1204.355357	115699.021743	35.451444
1205.495126	115925.863554	35.456461
1206.621381	116154.255156	35.461479
1208.239296	116371.860816	35.466496
1209.556491	116598.285785	35.471514
1211.207785	116811.429362	35.476532
1212.577096	117031.399952	35.481549
1213.865147	117231.417060	35.486567
1214.777887	117453.088442	35.491584
1216.015171	117664.887944	35.496602
1217.432646	117875.835519	35.501620
1218.771331	118083.148508	35.506637
1219.805418	118297.013698	35.511655
1222.549301	118466.235643	35.516672
1223.890594	118673.197650	35.521690
1225.407029	118866.345839	35.526708
1226.301412	119047.560801	35.531725
1227.340546	119237.888918	35.536743
1228.536340	119425.227182	35.541760
1229.419517	119626.582506	35.546778
1230.620974	119823.185263	35.551796
1231.577012	120031.589374	35.556813
1232.521832	120231.316664	35.561831
1233.407714	120437.923240	35.566848
1234.320685	120656.146956	35.571866
1235.675330	120862.628077	35.576884
1236.598959	121094.184266	35.581901
1237.878761	121316.090309	35.586919
1239.194615	121528.982013	35.591936
1240.123406	121751.228337	35.596954
1241.316551	121969.389946	35.601972
1243.006163	122196.531728	35.606989
1244.348380	122409.121238	35.612007
1245.231850	122633.624750	35.617024
1246.582601	122863.096257	35.622042
1247.631632	123088.500851	35.627060
1248.211950	123305.899457	35.632077
1249.025130	123532.106892	35.637095
1250.391583	123757.590598	35.642112
1251.375980	123993.873710	35.647130
1253.026231	124209.225724	35.652148
1254.648155	124441.034253	35.657165
1255.572702	124669.386260	35.662183
1257.351792	124870.058197	35.667200
1259.286465	125075.458344	35.672218
1260.730402	125279.217626	35.677236
1262.277972	125498.816259	35.682253
1263.481157	125706.940172	35.687271
1264.556412	125921.702645	35.692288
1265.417533	126136.831674	35.697306
1266.730030	126348.123065	35.702324
1267.737977	126568.807490	35.707341
1268.831190	126800.645626	35.712359
1270.438282	127023.958970	35.717376
1271.357460	127249.606108	35.722394
1272.662378	127466.762161	35.727412
1273.414180	127696.508937	35.732429
1274.674193	127946.085559	35.737447
1275.992887	128184.082079	35.742464
1276.864602	128439.228061	35.747482
1278.541836	128666.876535	35.752500
1279.875002	128906.283130	35.757517
1281.021636	129162.099243	35.762535
1283.002735	129383.047896	35.767552
1284.048434	129630.290517	35.772570
1285.470908	129874.645889	35.777588
1287.058623	130121.333465	35.782605
1288.126490	130347.079730	35.787623
1289.417031	130596.203387	35.792640
1290.304163	130853.736836	35.797658
1291.852924	131102.035714	35.802676
1292.786273	131358.057104	35.807693
1293.628060	131611.661850	35.812711
1295.121885	131870.826898	35.817728
1296.523407	132128.386738	35.822746
1297.810483	132383.280147	35.827764
1299.070250	132647.129992	35.832781
1300.108762	132908.179046	35.837799
1301.645022	133175.258019	35.842816
1302.692372	133447.275654	35.847834
1304.377862	133709.757814	35.852852
1306.096731	133958.392830	35.857869
1307.715942	134218.810999	35.862887
1309.250368	134456.590432	35.867904
1310.348193	134716.059476	35.872922
1311.783464	134981.813510	35.877940
1313.413222	135232.209857	35.882957
1314.327027	135478.961487	35.887975
1315.565920	135741.736868	35.892992
1316.712620	136008.257018	35.898010
1317.575187	136273.089509	35.903028
1319.759173	136522.655703	35.908045
1320.653327	136783.265119	35.913063
1321.893901	137042.855546	35.918080
1323.265275	137305.697401	35.923098
1325.016499	137548.851562	35.928116
1326.404679	137807.155562	35.933133
1327.708557	138055.395744	35.938151
1329.277390	138310.833562	35.943168
1330.463319	138577.760746	35.948186
1331.472989	138834.119402	35.953204
1333.310502	139090.444137	35.958221
1334.523761	139338.341064	35.963239
1336.013957	139583.087380	35.968256
1337.715681	139822.119897	35.973274
1339.210760	140043.132439	35.978292
1340.628442	140268.508414	35.983309
1341.635851	140504.148537	35.988327
1343.022625	140726.755752	35.993344
1344.203095	140958.033735	35.998362
1345.500544	141190.156117	36.003380
1346.513463	141414.769832	36.008397
1347.008760	141664.235483	36.013415
1348.688721	141914.990068	36.018432
1349.839479	142171.439003	36.023450
1351.395593	142413.899316	36.028468
1353.103738	142647.408908	36.033485
1354.886848	142898.052009	36.038503
1356.979404	143122.865428	36.043520
1358.534579	143346.057481	36.048538
1359.629708	143578.470243	36.053556
1360.970482	143808.053960	36.058573
1362.304725	144052.210915	36.063591
1363.770603	144276.235250	36.068608
1364.822341	144519.668715	36.073626
1365.757752	144764.809765	36.078644
1367.187192	145004.734560	36.083661
1368.138458	145273.755769	36.088679
1369.758734	145521.235982	36.093696
1370.425264	145787.264653	36.098714
1371.457706	146053.183880	36.103732
1372.768632	146325.590102	36.108749
1373.915328	146612.914366	36.113767
1375.275499	146873.243205	36.118784
1376.250942	147176.174030	36.123802
1377.529972	147449.900250	36.128820
1379.065692	147733.110484	36.133837
1380.245943	148024.625525	36.138855
1381.803862	148314.976857	36.143872
1383.231566	148614.255377	36.148890
1384.815712	148906.293825	36.153908
1386.630506	149193.070946	36.158925
1387.650714	149488.238725	36.163943
1389.033493	149784.693136	36.168960
1390.181343	150094.861426	36.173978
1391.773529	150377.727395	36.178996
1393.672243	150673.672056	36.184013
1395.032549	150976.988698	36.189031
1396.750412	151255.959257	36.194048
1397.916870	151543.978046	36.199066
1399.590959	151840.273505	36.204084
1401.256763	152112.029193	36.209101
1402.591939	152406.127511	36.214119
1404.521475	152682.663467	36.219136
1406.793738	152965.004701	36.224154
1407.978165	153244.966165	36.229172
1409.577853	153498.604065	36.234189
1411.541503	153752.957033	36.239207
1413.399335	154001.786060	36.244224
1415.163340	154262.035748	36.249242
1416.355949	154521.430570	36.254260
1417.464197	154772.697446	36.259277
1418.322404	155025.313943	36.264295
1419.641225	155272.274293	36.269312
1421.189570	155539.570355	36.274330
1421.997770	155806.876793	36.279348
1423.375912	156076.272393	36.284365
1424.163502	156349.674831	36.289383
1425.270348	156653.027236	36.294400
1426.901464	156912.694892	36.299418
1427.767477	157216.941446	36.304436
1429.296110	157499.413259	36.309453
1430.151013	157794.760675	36.314471
1431.601060	158080.256128	36.319488
1433.163103	158364.567918	36.324506
1434.098828	158648.199019	36.329524
1435.853838	158916.193784	36.334541
1436.633043	159212.984929	36.339559
1438.469211	159497.817374	36.344576
1440.284055	159784.976948	36.349594
1441.467710	160069.236488	36.354612
1443.149206	160360.545299	36.359629
1444.723341	160653.650099	36.364647
1445.806255	160951.443716	36.369664
1447.129163	161246.129450	36.374682
1448.313715	161551.383057	36.379700
1449.798950	161854.051625	36.384717
1451.584500	162174.840552	36.389735
1452.577943	162481.008013	36.394752
1453.949942	162786.810426	36.399770
1455.166452	163105.340924	36.404788
1456.825815	163421.186751	36.409805
1458.328693	163750.230593	36.414823
1459.710204	164066.101876	36.419840
1461.396510	164385.896222	36.424858
1462.351741	164724.351162	36.429876
1463.835836	165044.247346	36.434893
1465.272912	165387.702763	36.439911
1466.651841	165712.696531	36.444928
1468.709301	166045.599199	36.449946
1470.523997	166357.355067	36.454964
1472.711947	166677.349505	36.459981
1474.417064	166997.451694	36.464999
1476.281710	167315.385362	36.470016
1478.010062	167609.070363	36.475034
1479.568939	167926.120119	36.480052
1481.060076	168231.078136	36.485069
1482.936090	168525.886665	36.490087
1485.075532	168822.785208	36.495104
1486.938726	169098.908614	36.500122
1488.291994	169384.520958	36.505140
1489.800503	169681.986543	36.510157
1490.875883	169980.325307	36.515175
1492.590744	170263.802134	36.520192
1494.029061	170558.874046	36.525210
1494.958294	170854.476385	36.530228
1496.466310	171153.119007	36.535245
1498.220927	171454.565175	36.540263
1499.540151	171748.027410	36.545280
1501.421815	172031.982291	36.550298
1502.729717	172334.764499	36.555316
1504.403428	172630.914525	36.560333
1506.040683	172913.988868	36.565351
1507.775762	173198.178116	36.570368
1510.043917	173455.377174	36.575386
1511.753295	173747.099324	36.580404
1513.379932	174017.237769	36.585421
1514.573529	174291.079026	36.590439
1515.481806	174582.304535	36.595456
1516.832392	174856.554451	36.600474
1517.938901	175160.517412	36.605492
1519.566454	175444.230116	36.610509
1520.771039	175749.386114	36.615527
1521.699058	176050.769868	36.620544
1522.944099	176364.895521	36.625562
1523.557700	176689.344248	36.630580
1524.840565	177014.217170	36.635597
1525.722023	177361.064010	36.640615
1526.924952	177695.955395	36.645632
1528.287782	178046.953415	36.650650
1529.564406	178392.409245	36.655668
1530.964164	178723.200808	36.660685
1532.490212	179067.921837	36.665703
1533.564641	179413.011975	36.670720
1535.230290	179760.570187	36.675738
1536.732479	180118.514535	36.680756
1538.290468	180473.241000	36.685773
1539.581568	180823.889163	36.690791
1541.316557	181175.341855	36.695808
1543.382324	181529.800922	36.700826
1545.095892	181881.490344	36.705844
1547.486474	182224.045467	36.710861
1549.036210	182552.171070	36.715879
1550.728327	182913.022241	36.720896
1552.214213	183253.741192	36.725914
1553.526353	183610.991820	36.730932
1555.396312	183968.114246	36.735949
1557.035928	184313.003040	36.740967
1558.308980	184674.938158	36.745984
1560.083281	185017.041951	36.751002
1561.232626	185386.618161	36.756020
1563.159523	185724.664566	36.761037
1564.977016	186088.041859	36.766055
1566.826725	186442.175288	36.771072
1568.420952	186780.994049	36.776090
1570.026774	187147.675520	36.781108
1572.087283	187480.683620	36.786125
1574.731064	187797.805859	36.791143
1576.386559	188128.346105	36.796160
1577.913181	188449.985753	36.801178
1579.630707	188802.023138	36.806196
1581.042811	189133.739234	36.811213
1582.861073	189453.622374	36.816231
1583.788292	189789.281586	36.821248
1585.425364	190137.417798	36.826266
1586.676313	190473.319188	36.831284
1588.046882	190819.751741	36.836301
1590.094490	191152.782875	36.841319
1591.717444	191495.635707	36.846336
1593.511433	191838.906441	36.851354
1594.716291	192186.834187	36.856372
1596.015186	192546.313309	36.861389
1597.475513	192894.837459	36.866407
1598.745643	193253.855758	36.871424
1600.294243	193609.922800	36.876442
1601.533822	193985.606275	36.881460
1602.668310	194358.491079	36.886477
1604.356214	194735.640818	36.891495
1606.238914	195115.870862	36.896512
1607.916784	195481.740507	36.901530
1610.201695	195855.065423	36.906548
1612.574037	196196.943781	36.911565
1613.960156	196550.781655	36.916583
1615.654360	196916.961371	36.921600
1617.598708	197270.266235	36.926618
1619.112702	197631.756958	36.931636
1621.247236	197967.716883	36.936653
1623.466731	198300.350764	36.941671
1624.700192	198648.676975	36.946688
1627.022324	198986.540679	36.951706
1628.350588	199325.827723	36.956724
1629.505521	199670.376018	36.961741
1631.307094	200006.540870	36.966759
1632.832014	200357.938035	36.971776
1634.109935	200696.402183	36.976794
1635.581782	201048.598789	36.981812
1636.822719	201396.569390	36.986829
1638.461881	201746.926128	36.991847
1639.428919	202100.633640	36.996864
1641.005735	202446.242881	37.001882
1642.370391	202800.205328	37.006900
1643.992486	203160.970420	37.011917
1645.477765	203501.508406	37.016935
1647.017272	203867.597957	37.021952
1648.227345	204213.365194	37.026970
1649.918970	204590.098578	37.031988
1651.280988	204950.267915	37.037005
1652.919060	205319.878020	37.042023
1654.279099	205712.264114	37.047040
1655.707485	206080.223906	37.052058
1657.161958	206483.987779	37.057076
1658.976837	206877.167807	37.062093
1660.899691	207259.031107	37.067111
1662.279705	207663.587930	37.072128
1664.173428	208052.088010	37.077146
1666.547406	208440.789715	37.082164
1667.945356	208837.997499	37.087181
1670.225836	209226.261336	37.092199
1672.061631	209600.239396	37.097216
1674.075726	209982.481350	37.102234
1676.168758	210370.743522	37.107252
1678.651232	210722.220138	37.112269
1681.285213	211074.663553	37.117287
1682.917020	211432.887118	37.122304
1684.697843	211791.214455	37.127322
1686.402301	212149.251170	37.132340
1687.916519	212493.835265	37.137357
1689.654081	212852.986816	37.142375
1691.394679	213198.958354	37.147392
1693.116203	213555.931266	37.152410
1694.774672	213918.681170	37.157428
1696.102904	214275.010984	37.162445
1697.981901	214620.177701	37.167463
1699.782763	214986.667023	37.172480
1701.196069	215354.060136	37.177498
1702.786524	215705.323288	37.182516
1704.329584	216087.199742	37.187533
1705.888530	216462.268495	37.192551
1706.991434	216838.836569	37.197568
1708.471950	217224.258188	37.202586
1709.853149	217617.240996	37.207604
1711.404010	218010.857593	37.212621
1713.374493	218410.196988	37.217639
1714.343635	218819.583871	37.222656
1716.328872	219210.821899	37.227674
1718.022647	219687.855182	37.232692
1719.477323	220102.932151	37.237709
1721.250324	220503.785495	37.242727
1722.864837	220928.465329	37.247744
1725.140013	221322.228425	37.252762
1726.919872	221731.035065	37.257780
1728.580058	222141.564798	37.262797
1730.628011	222539.992549	37.267815
1732.488290	222955.368753	37.272832
1734.201937	223355.378737	37.277850
1736.424651	223746.542920	37.282868
1738.370808	224156.905528	37.287885
1740.096501	224556.206451	37.292903
1741.446077	224952.751673	37.297920
1743.363408	225355.122265	37.302938
1745.188248	225755.528318	37.307956
1747.094529	226145.558976	37.312973
1749.128572	226545.526505	37.317991
1750.959370	226936.410327	37.323008
1751.953514	227340.565914	37.328026
1754.174519	227734.384714	37.333044
1755.755673	228114.238926	37.338061
1757.672180	228487.053523	37.343079
1759.300804	228868.476836	37.348096
1760.726144	229248.283866	37.353114
1762.629992	229627.580828	37.358132
1763.864105	230016.946893	37.363149
1764.885724	230399.491026	37.368167
1766.641424	230801.905002	37.373184
1768.060294	231203.639281	37.378202
1769.889696	231611.733071	37.383220
1771.306843	232034.984526	37.388237
1773.088626	232436.128535	37.393255
1774.861057	232866.435720	37.398272
1776.641249	233281.959250	37.403290
1778.921717	233692.828713	37.408308
1780.989082	234119.407198	37.413325
1782.994112	234533.448786	37.418343
1784.855309	234954.322839	37.423360
1786.535989	235370.249128	37.428378
1788.164704	235779.707599	37.433396
1789.933857	236212.716532	37.438413
1791.741794	236633.400215	37.443431
1792.923035	237073.900532	37.448448
1794.259661	237516.586095	37.453466
1796.347043	237964.127050	37.458484
1797.871138	238420.449859	37.463501
1799.586337	238874.938490	37.468519
1800.740829	239336.887660	37.473536
1802.239018	239810.338883	37.478554
1804.195753	240273.173233	37.483572
1805.722280	240755.182365	37.488589
1807.727895	241250.322350	37.493607
1809.599128	241730.472842	37.498624
1811.230271	242210.968910	37.503642
1813.499257	242686.203514	37.508660
1815.405989	243188.451133	37.513677
1817.242154	243670.821182	37.518695
1819.951602	244130.845484	37.523712
1822.364401	244592.875709	37.528730
1824.370051	245063.357040	37.533748
1826.015443	245531.155314	37.538765
1828.022337	246003.035050	37.543783
1829.794553	246487.528771	37.548800
1831.660012	246959.382524	37.553818
1833.201999	247435.609016	37.558836
1834.938306	247910.482986	37.563853
1837.174774	248382.556562	37.568871
1840.004140	248847.470431	37.573888
1841.494494	249308.110369	37.578906
1843.365124	249764.978943	37.583924
1845.031234	250236.488633	37.588941
1847.301906	250686.610819	37.593959
1849.317955	251156.691643	37.598976
1851.308307	251616.057013	37.603994
1852.913103	252072.641486	37.609012
1854.740657	252523.702306	37.614029
1856.521636	252983.001790	37.619047
1858.078975	253446.962014	37.624064
1859.733834	253916.215635	37.629082
1861.729784	254394.202522	37.634100
1862.946427	254867.847809	37.639117
1865.071523	255339.158106	37.644135
1867.143049	255786.318958	37.649152
1869.767893	256242.533456	37.654170
1872.624522	256698.379438	37.659188
1874.322030	257167.932134	37.664205
1875.886474	257595.312096	37.669223
1878.350640	258042.789462	37.674240
1880.419530	258478.240389	37.679258
1882.678100	258899.484864	37.684276
1884.123516	259312.684204	37.689293
1885.445291	259724.252794	37.694311
1887.166292	260139.413272	37.699328
1888.900645	260558.636007	37.704346
1890.915738	260977.888361	37.709364
1892.386045	261403.861139	37.714381
1894.170460	261825.107557	37.719399
1896.271803	262259.231592	37.724416
1897.701584	262708.149814	37.729434
1899.772008	263136.207252	37.734452
1901.361281	263576.868004	37.739469
1902.421274	264044.594433	37.744487
1904.314597	264496.991400	37.749504
1905.946331	264968.128162	37.754522
1907.823993	265432.720633	37.759540
1909.606319	265926.897802	37.764557
1911.057970	266408.072130	37.769575
1913.286988	266887.694658	37.774592
1915.116787	267371.879216	37.779610
1917.601084	267853.871795	37.784628
1919.391166	268337.299833	37.789645
1921.478878	268815.546611	37.794663
1923.770213	269309.864565	37.799680
1925.543677	269795.579890	37.804698
1927.669096	270278.060909	37.809716
1929.450260	270781.530256	37.814733
1931.403542	271264.648094	37.819751
1933.934319	271738.118100	37.824768
1936.105875	272239.285085	37.829786
1938.343112	272703.911290	37.834804
1940.325641	273195.226340	37.839821
1942.137140	273674.832869	37.844839
1943.738430	274161.814726	37.849856
1945.561400	274658.538933	37.854874
1947.327185	275135.076696	37.859892
1949.593786	275641.429222	37.864909
1951.787413	276134.481943	37.869927
1954.087310	276625.407636	37.874944
1955.537052	277125.617930	37.879962
1957.437029	277617.496799	37.884980
1959.146796	278126.654113	37.889997
1961.041991	278631.257913	37.895015
1962.872652	279138.614583	37.900032
1964.493867	279649.611746	37.905050
1967.412600	280138.419997	37.910068
1969.965944	280628.379809	37.915085
1972.238929	281116.505055	37.920103
1974.720692	281609.090508	37.925120
1976.197704	282111.392060	37.930138
1978.055827	282603.493824	37.935156
1980.422676	283089.108731	37.940173
1982.291867	283577.954451	37.945191
1984.391428	284071.815417	37.950208
1985.899630	284563.918549	37.955226
1987.765484	285061.041133	37.960244
1989.214273	285566.892983	37.965261
1991.200120	286073.289212	37.970279
1993.552908	286576.473229	37.975296
1995.145532	287090.144980	37.980314
1996.371896	287593.359681	37.985332
1998.725592	288101.592973	37.990349
2000.715924	288629.189008	37.995367
2002.585845	289140.140273	38.000384
2004.216190	289667.842704	38.005402
2006.523606	290188.852210	38.010420
2008.434431	290716.427759	38.015437
2010.620397	291226.734339	38.020455
2013.231360	291710.628728	38.025472
2015.339203	292191.810591	38.030490
2017.621960	292675.323761	38.035508
2019.669734	293155.825960	38.040525
2021.425929	293640.209845	38.045543
2023.793485	294120.375750	38.050560
2025.466441	294597.784598	38.055578
2027.298984	295090.785521	38.060596
2029.194547	295582.072105	38.065613
2031.179375	296095.489630	38.070631
2032.946092	296586.945472	38.075648
2034.689901	297106.976449	38.080666
2036.107453	297607.832185	38.085684
2038.746287	298140.434530	38.090701
2040.502983	298663.198711	38.095719
2042.772840	299173.938057	38.100736
2045.150598	299693.927254	38.105754
2048.281012	300185.165564	38.110772
2051.451358	300682.998252	38.115789
2053.321966	301181.577038	38.120807
2055.658691	301666.056573	38.125824
2057.443296	302177.520991	38.130842
2058.803970	302672.950958	38.135860
2060.302259	303188.546241	38.140877
2061.974596	303714.776554	38.145895
2063.554250	304238.581073	38.150912
2065.459933	304782.950672	38.155930
2067.056461	305323.330087	38.160948
2069.373856	305858.913833	38.165965
2071.441352	306394.205513	38.170983
2073.826355	306957.453144	38.176000
2075.934046	307508.679905	38.181018
2077.692863	308063.947957	38.186036
2080.261395	308625.046132	38.191053
2082.636788	309159.913607	38.196071
2085.172446	309691.068697	38.201088
2087.727264	310242.685519	38.206106
2089.690441	310779.743649	38.211124
2092.243768	311327.086797	38.216141
2094.080304	311857.403499	38.221159
2096.645832	312387.671984	38.226176
2098.566802	312927.337806	38.231194
2100.668499	313465.827101	38.236212
2102.812954	313998.007764	38.241229
2104.625388	314535.038984	38.246247
2106.998573	315075.934767	38.251264
2108.679735	315621.080232	38.256282
2111.062823	316166.283054	38.261300
2113.223958	316702.250062	38.266317
2115.537147	317256.546710	38.271335
2117.576565	317804.561575	38.276352
2119.054036	318364.345609	38.281370
2120.945184	318917.962463	38.286388
2122.954090	319473.028025	38.291405
2124.704766	320051.745990	38.296423
2126.093442	320606.803307	38.301440
2128.226687	321192.252856	38.306458
2129.921973	321785.590113	38.311476
2131.912317	322374.556645	38.316493
2133.752853	322978.827657	38.321511
2135.993000	323573.860865	38.326528
2138.575849	324176.727984	38.331546
2140.843569	324767.073539	38.336564
2143.448591	325356.418184	38.341581
2145.021895	325947.197493	38.346599
2148.031401	326526.663587	38.351616
2150.432413	327125.418796	38.356634
2152.205999	327702.437780	38.361652
2154.435674	328272.139946	38.366669
2156.616961	328839.889719	38.371687
2158.156679	329408.578006	38.376704
2160.555272	329971.710910	38.381722
2162.165410	330542.280395	38.386740
2164.952448	331100.590408	38.391757
2166.730414	331679.828390	38.396775
2169.255218	332242.333914	38.401792
2171.305684	332826.998335	38.406810
2173.331221	333401.201656	38.411828
2175.402178	333986.484981	38.416845
2177.186222	334563.914633	38.421863
2179.655123	335161.431264	38.426880
2181.143325	335761.845184	38.431898
2183.563194	336360.930323	38.436916
2185.895949	336969.339095	38.441933
2187.743637	337593.153028	38.446951
2189.417728	338203.154085	38.451968
2191.445642	338833.040637	38.456986
2193.411973	339464.147986	38.462004
2196.133064	340087.228435	38.467021
2198.744063	340708.745663	38.472039
2201.261471	341344.230785	38.477056
2203.639627	341965.872341	38.482074
2206.208213	342590.088767	38.487092
2208.933279	343195.971475	38.492109
2211.226422	343813.694804	38.497127
2213.809338	344438.214920	38.502144
2215.666197	345062.136430	38.507162
2218.231510	345687.125236	38.512180
2220.318272	346294.495466	38.517197
2222.488150	346923.695456	38.522215
2224.149039	347550.103369	38.527232
2226.371622	348179.099842	38.532250
2228.555952	348826.696110	38.537268
2230.671508	349466.122877	38.542285
2232.369325	350106.041138	38.547303
2234.659669	350758.337588	38.552320
2236.941073	351401.541089	38.557338
2238.860808	352069.790673	38.562356
2241.523789	352722.579952	38.567373
2244.662574	353366.475331	38.572391
2246.618593	354017.560461	38.577408
2249.079295	354674.388298	38.582426
2251.042391	355327.938971	38.587444
2253.587392	355996.506019	38.592461
2255.386139	356652.067871	38.597479
2257.676167	357300.027614	38.602496
2260.451368	357954.113181	38.607514
2262.898677	358602.127902	38.612532
2265.566957	359252.277728	38.617549
2267.479908	359909.392499	38.622567
2269.586771	360554.692265	38.627584
2272.291101	361214.242497	38.632602
2274.732508	361850.839880	38.637620
2277.216641	362502.185180	38.642637
2279.014124	363142.952846	38.647655
2281.468840	363775.001078	38.652672
2284.175122	364424.755369	38.657690
2286.294872	365084.540138	38.662708
2288.871368	365725.212133	38.667725
2291.053880	366359.825064	38.672743
2293.388961	366995.949473	38.677760
2295.386291	367645.258865	38.682778
2297.524045	368300.418645	38.687796
2299.876772	368937.369558	38.692813
2301.967105	369588.937876	38.697831
2304.661567	370222.385707	38.702848
2307.783951	370822.803562	38.707866
2309.967572	371431.635529	38.712884
2312.493403	372025.943443	38.717901
2314.886708	372631.778263	38.722919
2316.696423	373231.206630	38.727936
2318.984284	373832.625422	38.732954
2321.358804	374437.113768	38.737972
2323.547160	375047.506361	38.742989
2325.290999	375664.657157	38.748007
2327.269631	376280.718369	38.753024
2329.623771	376906.444650	38.758042
2331.503347	377544.106344	38.763060
2333.690176	378165.551654	38.768077
2335.950899	378817.657159	38.773095
2338.406199	379462.490879	38.778112
2340.922088	380113.869826	38.783130
2342.426638	380777.752413	38.788148
2344.775989	381438.210936	38.793165
2346.984140	382106.565394	38.798183
2349.453416	382776.840804	38.803200
2351.640752	383466.342880	38.808218
2353.471533	384161.771632	38.813236
2355.895232	384855.211134	38.818253
2357.930161	385554.480644	38.823271
2360.237148	386263.780261	38.828288
2362.571639	386965.580666	38.833306
2364.672936	387689.586801	38.838324
2367.063339	388411.475026	38.843341
2369.473038	389135.396830	38.848359
2371.876124	389871.749691	38.853376
2374.727708	390613.182061	38.858394
2377.458116	391339.432849	38.863412
2380.391315	392046.469762	38.868429
2382.886187	392767.579981	38.873447
2384.862655	393497.858388	38.878464
2387.687607	394224.024651	38.883482
2389.964919	394952.393030	38.888500
2392.489570	395677.002324	38.893517
2394.678845	396406.211435	38.898535
2397.135325	397145.064948	38.903552
2399.589546	397865.501171	38.908570
2401.833397	398612.944164	38.913588
2404.839719	399339.106653	38.918605
2407.231511	400087.880915	38.923623
2409.267716	400823.390785	38.928640
2411.633898	401557.078669	38.933658
2414.403230	402299.955037	38.938676
2417.532902	403023.114899	38.943693
2420.272217	403756.177237	38.948711
2422.787806	404475.245947	38.953728
2425.748607	405181.630132	38.958746
2428.140765	405901.467825	38.963764
2430.382292	406643.708036	38.968781
2432.946608	407356.841346	38.973799
2434.985514	408078.276540	38.978816
2437.175958	408800.402177	38.983834
2439.588040	409534.200827	38.988852
2441.723069	410269.317268	38.993869
2444.011084	410994.129100	38.998887
2446.719446	411725.488235	39.003904
2449.488796	412464.973301	39.008922
2451.536182	413194.096264	39.013940
2453.717803	413931.307185	39.018957
2456.371206	414668.343251	39.023975
2458.719889	415404.826368	39.028992
2461.026149	416144.663953	39.034010
2463.535398	416893.589200	39.039028
2466.056412	417607.694460	39.044045
2468.919602	418318.760202	39.049063
2471.225468	419030.100892	39.054080
2473.832383	419728.001414	39.059098
2476.091009	420445.362168	39.064116
2478.338654	421136.547431	39.069133
2480.347035	421844.084895	39.074151
2482.609723	422560.801851	39.079168
2485.238494	423296.300133	39.084186
2487.037329	424037.382577	39.089204
2489.316191	424768.438732	39.094221
2491.390948	425535.203353	39.099239
2493.648828	426284.091086	39.104256
2496.110017	427038.086280	39.109274
2498.482062	427821.234715	39.114292
2500.734632	428587.417317	39.119309
2503.295862	429373.369361	39.124327
2505.137591	430171.867898	39.129344
2507.907078	430966.693004	39.134362
2510.586100	431774.718096	39.139380
2512.844277	432578.684873	39.144397
2515.837905	433381.742947	39.149415
2518.261284	434195.597959	39.154432
2521.492153	435002.204803	39.159450
2523.924149	435823.390391	39.164468
2526.593953	436627.097473	39.169485
2529.847424	437426.782787	39.174503
2532.858315	438228.200630	39.179520
2535.139931	439024.751496	39.184538
2537.369283	439832.415281	39.189556
2540.444571	440638.644874	39.194573
2542.921727	441449.396934	39.199591
2544.689405	442279.412930	39.204608
2547.565164	443102.535786	39.209626
2549.909488	443921.820073	39.214644
2552.232000	444745.731640	39.219661
2555.139302	445576.344758	39.224679
2557.491852	446415.263540	39.229696
2560.373281	447237.014935	39.234714
2562.732046	448080.420421	39.239732
2565.444515	448914.073060	39.244749
2567.965625	449759.155608	39.249767
2570.417407	450613.522112	39.254784
2572.947521	451453.528251	39.259802
2575.546163	452298.243301	39.264820
2578.020217	453148.709919	39.269837
2580.448036	453991.108938	39.274855
2583.230877	454850.961665	39.279872
2586.201124	455711.404850	39.284890
2588.633440	456569.726781	39.289908
2590.787927	457428.614799	39.294925
2593.906895	458284.172319	39.299943
2596.244505	459148.265894	39.304960
2599.602831	459998.200582	39.309978
2602.461852	460850.911712	39.314996
2605.306994	461700.454668	39.320013
2608.341180	462537.141505	39.325031
2610.880808	463382.467602	39.330048
2614.062862	464218.755539	39.335066
2616.861573	465055.627272	39.340084
2619.235990	465883.689088	39.345101
2621.914631	466713.838470	39.350119
2624.291596	467574.777928	39.355136
2627.021853	468394.891379	39.360154
2629.993146	469230.442830	39.365172
2632.059183	470063.278087	39.370189
2634.772540	470895.313069	39.375207
2637.249642	471724.571938	39.380224
2639.803668	472547.315017	39.385242
2642.302937	473360.786238	39.390260
2645.174332	474163.097405	39.395277
2647.455304	474956.833811	39.400295
2650.138733	475755.167544	39.405312
2652.722337	476561.009588	39.410330
2654.864541	477364.364165	39.415348
2657.367384	478178.684949	39.420365
2660.391281	478980.257401	39.425383
2662.663660	479802.321832	39.430400
2665.602732	480614.189474	39.435418
2668.197632	481442.085401	39.440436
2670.629820	482276.534710	39.445453
2673.498642	483099.209351	39.450471
2675.746947	483939.469091	39.455488
2678.548207	484782.223236	39.460506
2681.358298	485631.448679	39.465524
2684.149305	486472.256462	39.470541
2687.275015	487315.190028	39.475559
2690.022831	488156.984777	39.480576
2693.306389	488979.015402	39.485594
2696.042845	489814.877146	39.490612
2698.407939	490669.787783	39.495629
2700.806649	491526.972291	39.500647
2702.990166	492390.458146	39.505664
2705.224425	493255.052973	39.510682
2707.891717	494133.712075	39.515700
2710.935689	495022.254396	39.520717
2713.501007	495895.188305	39.525735
2716.212408	496788.284745	39.530752
2718.765478	497686.253839	39.535770
2721.049204	498587.801355	39.540788
2723.262625	499493.852052	39.545805
2726.552861	500408.906321	39.550823
2728.848189	501327.605592	39.555840
2731.564032	502249.462717	39.560858
2734.435006	503185.263212	39.565876
2736.746299	504128.768488	39.570893
2739.612068	505072.631934	39.575911
2742.292926	506009.109310	39.580928
2745.326492	506953.188891	39.585946
2748.288824	507887.645553	39.590964
2751.171657	508844.445900	39.595981
2753.901388	509785.838571	39.600999
2757.184590	510746.240061	39.606016
2760.085704	511684.064504	39.611034
2763.023816	512628.329506	39.616052
2765.869242	513574.871864	39.621069
2768.911661	514510.892333	39.626087
2771.467922	515449.860271	39.631104
2774.592131	516393.767402	39.636122
2777.736848	517338.319332	39.641140
2780.109792	518274.073492	39.646157
2783.462924	519205.678952	39.651175
2785.962326	520144.674303	39.656192
2788.817113	521078.112679	39.661210
2791.889736	522013.422542	39.666228
2795.226271	522943.543839	39.671245
2797.681676	523876.272206	39.676263
2800.583506	524818.740526	39.681280
2802.881578	525740.349860	39.686298
2805.997862	526673.550980	39.691316
2808.835904	527605.783103	39.696333
2811.807645	528530.734444	39.701351
2814.745978	529466.357880	39.706368
2817.325886	530395.033729	39.711386
2820.123096	531327.894167	39.716404
2822.439567	532265.456362	39.721421
2825.433781	533190.061065	39.726439
2827.474461	534114.664176	39.731456
2829.684099	535024.433974	39.736474
2832.489607	535943.509346	39.741492
2834.619636	536872.853451	39.746509
2837.678707	537787.340745	39.751527
2840.693029	538716.871996	39.756544
2843.310339	539662.810472	39.761562
2846.406509	540587.225146	39.766580
2849.154054	541542.122945	39.771597
2852.047449	542483.048406	39.776615
2854.425613	543438.633408	39.781632
2857.379338	544391.794771	39.786650
2859.986886	545369.742737	39.791668
2862.690058	546328.898615	39.796685
2865.979502	547302.876384	39.801703
2869.010823	548270.392117	39.806720
2872.399000	549237.730607	39.811738
2875.446762	550213.805121	39.816756
2878.460504	551196.602286	39.821773
2881.402841	552159.233262	39.826791
2883.926765	553143.780498	39.831808
2886.691840	554128.467569	39.836826
2889.922670	555106.824136	39.841844
2892.248590	556105.662022	39.846861
2895.640587	557093.244480	39.851879
2898.776243	558082.303656	39.856896
2901.487253	559084.824413	39.861914
2904.657513	560080.712681	39.866932
2907.681289	561080.468396	39.871949
2911.153049	562073.996193	39.876967
2914.089508	563078.436507	39.881984
2916.863264	564081.118995	39.887002
2920.035588	565074.920288	39.892020
2923.328854	566054.966963	39.897037
2926.822929	567045.952723	39.902055
2929.359906	568047.614431	39.907072
2931.690431	569061.030089	39.912090
2934.508091	570067.206871	39.917108
2936.692410	571091.529732	39.922125
2939.755075	572122.400720	39.927143
2942.267886	573151.020392	39.932160
2945.075140	574190.196681	39.937178
2948.011218	575222.993496	39.942196
2950.747336	576282.682345	39.947213
2953.899581	577334.436098	39.952231
2957.172934	578382.770039	39.957248
2959.664442	579444.036456	39.962266
2962.266516	580502.083774	39.967284
2965.195369	581581.803051	39.972301
2968.579553	582641.643518	39.977319
2971.641782	583713.430078	39.982336
2974.019588	584797.620335	39.987354
2977.363546	585877.693666	39.992372
2980.032025	586961.792913	39.997389
2983.235521	588064.704389	40.002407
2986.135817	589145.410855	40.007424
2988.704682	590235.947893	40.012442
2991.731574	591337.334509	40.017460
2994.751221	592431.304575	40.022477
2998.823350	593512.323405	40.027495
3002.171291	594601.278791	40.032512
3004.989334	595690.872361	40.037530
3008.304223	596763.752931	40.042548
3011.129900	597860.005881	40.047565
3014.098729	598938.153124	40.052583
3017.436731	600014.837296	40.057600
3020.400864	601109.408721	40.062618
3023.512093	602158.491613	40.067636
3026.226205	603216.655806	40.072653
3029.041642	604250.778063	40.077671
3032.010570	605284.430990	40.082688
3034.597842	606336.821427	40.087706
3037.039707	607383.933821	40.092724
3039.753375	608452.471283	40.097741
3042.604206	609514.280321	40.102759
3045.679975	610591.761262	40.107776
3048.251642	611674.074376	40.112794
3051.171690	612765.578748	40.117812
3053.910851	613858.306417	40.122829
3057.266462	614965.877559	40.127847
3060.055148	616067.230911	40.132864
3062.746674	617197.190241	40.137882
3065.709771	618313.289902	40.142900
3069.079805	619460.202041	40.147917
3071.835190	620595.848804	40.152935
3074.691340	621747.153695	40.157952
3077.856118	622902.383098	40.162970
3081.352681	624050.838258	40.167988
3084.525743	625221.208065	40.173005
3087.343276	626390.210075	40.178023
3090.627175	627554.311662	40.183040
3093.807726	628732.687729	40.188058
3097.517774	629907.849001	40.193076
3101.106473	631063.025503	40.198093
3104.844205	632233.579020	40.203111
3108.602721	633371.497901	40.208128
3111.801743	634524.660882	40.213146
3115.582839	635656.436906	40.218164
3118.977314	636806.270381	40.223181
3121.967371	637961.782033	40.228199
3124.924712	639093.219394	40.233216
3127.846934	640250.681464	40.238234
3131.262804	641393.115383	40.243252
3134.132855	642548.131747	40.248269
3137.156327	643702.293763	40.253287
3140.548700	644844.145657	40.258304
3143.519690	646000.398955	40.263322
3146.568773	647159.149487	40.268340
3149.086598	648326.030238	40.273357
3152.677298	649502.068717	40.278375
3156.501440	650657.794959	40.283392
3159.446107	651830.775337	40.288410
3162.232198	653012.911617	40.293428
3165.629053	654186.983779	40.298445
3168.333820	655360.283542	40.303463
3171.420191	656534.775090	40.308480
3174.888395	657720.219158	40.313498
3178.147717	658899.727649	40.318516
3181.675892	660081.190063	40.323533
3184.407603	661281.310393	40.328551
3187.417471	662444.896486	40.333568
3190.491930	663656.662429	40.338586
3193.427814	664852.771147	40.343604
3196.172473	666063.740598	40.348621
3198.645168	667276.343096	40.353639
3202.078596	668502.263702	40.358656
3205.024671	669741.537105	40.363674
3208.053735	670973.174203	40.368692
3211.226002	672196.968552	40.373709
3214.202956	673445.049898	40.378727
3217.510702	674704.693134	40.383744
3220.530136	675964.711303	40.388762
3224.022952	677208.824371	40.393780
3227.027059	678473.773490	40.398797
3230.525646	679726.641870	40.403815
3233.979544	680954.704836	40.408832
3237.579606	682164.646486	40.413850
3241.810566	683344.472603	40.418868
3245.600906	684511.256987	40.423885
3249.037479	685681.624921	40.428903
3252.854657	686836.337705	40.433920
3256.360046	687996.365897	40.438938
3260.046078	689136.459195	40.443956
3263.717369	690271.397628	40.448973
3267.229880	691417.483644	40.453991
3270.055744	692554.704109	40.459008
3272.755523	693710.057849	40.464026
3275.535513	694868.522221	40.469044
3278.412910	696033.316668	40.474061
3280.935038	697210.960125	40.479079
3283.739496	698399.953170	40.484096
3286.264389	699623.338831	40.489114
3288.962715	700823.721633	40.494132
3292.287483	702057.243126	40.499149
3295.126910	703311.385479	40.504167
3298.634054	704553.740332	40.509184
3301.086263	705814.224272	40.514202
3304.000179	707087.872148	40.519220
3307.257323	708387.376534	40.524237
3310.041146	709707.759247	40.529255
3312.969720	711016.773276	40.534272
3316.132269	712350.993582	40.539290
3319.469853	713683.292202	40.544308
3323.445151	715011.068802	40.549325
3326.583498	716367.721957	40.554343
3330.119619	717728.839849	40.559360
3333.237103	719085.155792	40.564378
3336.458720	720452.659006	40.569396
3340.636690	721805.982639	40.574413
3344.030643	723185.617050	40.579431
3347.894890	724535.727832	40.584448
3351.749149	725906.674321	40.589466
3355.262054	727262.375816	40.594484
3358.947572	728613.080781	40.599501
3362.502964	729967.831993	40.604519
3365.793899	731313.115171	40.609536
3369.974814	732665.978808	40.614554
3373.811107	733996.798840	40.619572
3377.524206	735331.566117	40.624589
3381.100542	736658.285628	40.629607
3385.168035	737982.285606	40.634624
3388.977807	739305.466792	40.639642
3392.806992	740603.953890	40.644660
3396.572768	741911.462922	40.649677
3399.821251	743205.228773	40.654695
3403.204438	744502.014356	40.659712
3406.400720	745796.693780	40.664730
3409.418133	747100.505385	40.669748
3413.300342	748388.233682	40.674765
3416.514251	749681.329173	40.679783
3419.628817	750984.128862	40.684800
3422.879706	752294.026580	40.689818
3425.724137	753599.483805	40.694836
3429.521854	754892.595111	40.699853
3432.838908	756215.257544	40.704871
3436.229080	757516.461383	40.709888
3439.686122	758847.997501	40.714906
3442.719423	760158.258433	40.719924
3445.871759	761487.511227	40.724941
3448.589477	762820.389664	40.729959
3452.075808	764153.642758	40.734976
3455.041439	765503.415757	40.739994
3458.073457	766851.360791	40.745012
3461.915745	768195.641227	40.750016
3464.827136	769482.950870	40.755021
3468.107574	770735.439392	40.760026
3471.268545	771913.796842	40.765031
3474.680003	773040.160582	40.770036
3477.713204	774095.698542	40.775040
3480.036581	775115.602658	40.780045
3482.357154	776035.030788	40.785050
3485.293319	776925.444208	40.790055
3487.394398	777743.385294	40.795060
3489.811615	778491.444161	40.800064
3491.942594	779190.410304	40.805069
3493.876688	779820.452874	40.810074
3495.824459	780400.104346	40.815079
3497.417013	780929.683719	40.820084
3499.419436	781393.628091	40.825088
3501.080615	781807.865133	40.830093
3502.723890	782183.958895	40.835098
3504.191894	782516.776594	40.840103
3505.242135	782814.578366	40.845108
3506.714329	783048.358598	40.850112
3507.989026	783261.752947	40.855117
3509.055787	783423.878813	40.860122
3509.944890	783568.522003	40.865127
3510.528089	783664.377041	40.870132
3511.875418	783737.727797	40.875136
3512.630908	783783.143396	40.880141
3513.625248	783798.077322	40.885146
3514.399889	783785.753019	40.890151
3514.744226	783759.975435	40.895156
3515.522365	783699.257565	40.900160
3515.806364	783623.522445	40.905165
3516.256612	783522.824243	40.910170
3516.625840	783416.236194	40.915175
3517.101964	783296.251214	40.920180
3517.740475	783153.563751	40.925184
3517.778721	782991.102014	40.930189
3517.935400	782809.188572	40.935194
3518.134169	782640.888445	40.940199
3518.481978	782456.721090	40.945204
3518.900492	782257.829603	40.950208
3518.749248	782051.057802	40.955213
3519.117998	781831.895972	40.960218
3519.172566	781599.644531	40.965223
3519.481633	781366.753210	40.970228
3519.736928	781116.398135	40.975232
3519.261237	780879.438976	40.980237
3519.657568	780612.610584	40.985242
3519.923672	780360.899127	40.990247
3520.059348	780097.834230	40.995252
3520.054610	779822.875037	41.000256
3519.851323	779552.268541	41.005261
3520.005937	779269.979212	41.010266
3519.955187	778990.616343	41.015271
3519.809269	778707.862681	41.020276
3520.308809	778421.792318	41.025280
3520.151338	778140.544175	41.030285
3519.811585	777849.126784	41.035290
3520.006891	777556.772531	41.040295
3519.680334	777259.078162	41.045300
3519.862851	776957.694020	41.050304
3519.825182	776677.452518	41.055309
3520.082594	776374.259694	41.060314
3519.886957	776076.396942	41.065319
3519.698975	775767.590874	41.070324
3519.572208	775462.355863	41.075328
3519.532536	775168.172249	41.080333
3519.530253	774877.417421	41.085338
3519.797472	774572.424871	41.090343
3519.376232	774272.900982	41.095348
3519.188892	773962.147378	41.100352
3518.935943	773670.154940	41.105357
3519.045466	773362.478763	41.110362
3518.892137	773073.007125	41.115367
3518.631580	772779.158215	41.120372
3518.804690	772475.374728	41.125376
3518.751641	772181.221378	41.130381
3518.495080	771882.952086	41.135386
3518.611610	771587.515524	41.140391
3518.193244	771298.017918	41.145396
3518.163419	771006.227794	41.150400
3518.075658	770709.164074	41.155405
3517.776422	770422.667072	41.160410
3517.887790	770123.625412	41.165415
3517.065919	769849.313377	41.170420
3517.683966	769555.732958	41.175424
3517.355417	769280.677767	41.180429
3517.416931	768995.790658	41.185434
3517.663416	768721.556022	41.190439
3517.166650	768427.770234	41.195444
3517.473562	768149.808292	41.200448
3517.060544	767870.180613	41.205453
3516.922066	767582.709478	41.210458
3516.940371	767300.278243	41.215463
3516.730510	767038.034499	41.220468
3517.003670	766753.420870	41.225472
3516.622916	766474.869237	41.230477
3516.417367	766201.848887	41.235482
3516.485049	765931.780669	41.240487
3515.999033	765659.920744	41.245492
3515.997643	765390.682513	41.250496
3515.992622	765139.677926	41.255501
3515.994271	764865.834985	41.260506
3515.780831	764593.348900	41.265511
3515.452878	764330.142106	41.270516
3515.792431	764070.957951	41.275520
3515.241471	763822.415739	41.280525
3515.318983	763557.043671	41.285530
3515.328585	763298.577798	41.290535
3515.008001	763061.759035	41.295540
3515.191483	762789.931006	41.300544
3514.670971	762555.989922	41.305549
3514.708777	762294.624253	41.310554
3514.699831	762057.081185	41.315559
3514.359447	761809.128199	41.320564
3514.726028	761565.144468	41.325568
3514.411658	761326.099685	41.330573
3514.295024	761077.049752	41.335578
3513.919347	760832.622374	41.340583
3513.909436	760607.317723	41.345588
3513.943243	760366.705029	41.350592
3513.563422	760136.069860	41.355597
3513.654632	759901.205361	41.360602
3513.685358	759678.974722	41.365607
3513.314501	759449.451997	41.370612
3513.418470	759217.129976	41.375616
3513.370795	758984.727214	41.380621
3513.383289	758755.514912	41.385626
3513.056082	758534.296830	41.390631
3512.996883	758314.459148	41.395636
3513.336628	758094.154382	41.400640
3513.134562	757875.956210	41.405645
3512.846941	757646.019781	41.410650
3512.794776	757427.932059	41.415655
3512.492952	757221.478094	41.420660
3512.718634	756998.347180	41.425664
3512.359814	756782.265973	41.430669
3512.320926	756571.160553	41.435674
3512.338026	756364.680060	41.440679
3512.142858	756159.216329	41.445684
3512.390666	755951.205646	41.450688
3512.118678	755756.357146	41.455693
3512.038330	755540.490994	41.460698
3511.839645	755330.562534	41.465703
3511.562785	755136.242103	41.470708
3511.878995	754927.106157	41.475712
3511.497776	754732.891484	41.480717
3511.981116	754530.727986	41.485722
3511.727640	754328.730298	41.490727
3511.400226	754127.430778	41.495732
3511.605282	753923.470357	41.500736
3511.044107	753749.554692	41.505741
3511.258608	753547.607261	41.510746
3511.039390	753352.145766	41.515751
3510.804757	753162.410219	41.520756
3510.810832	752979.494547	41.525760
3510.724534	752797.133028	41.530765
3510.779407	752600.026826	41.535770
3510.868103	752422.516744	41.540775
3510.458669	752234.170057	41.545780
3510.611913	752054.517136	41.550784
3510.228231	751881.023816	41.555789
3510.129620	751695.773623	41.560794
3510.400525	751522.954356	41.565799
3509.901548	751354.061791	41.570804
3510.134819	751168.398352	41.575808
3509.983382	751007.689786	41.580813
3509.730759	750821.060982	41.585818
3509.805809	750666.186190	41.590823
3509.848550	750503.459126	41.595828
3509.825294	750326.462787	41.600832
3509.619749	750152.407229	41.605837
3509.558431	750001.740833	41.610842
3509.330837	749831.386910	41.615847
3509.318621	749679.125211	41.620852
3509.350278	749512.624419	41.625856
3508.944692	749354.047996	41.630861
3509.299814	749197.269531	41.635866
3509.403790	749035.786160	41.640871
3508.889948	748884.530541	41.645876
3509.087338	748721.888787	41.650880
3509.000614	748574.460007	41.655885
3509.139118	748416.812193	41.660890
3509.160902	748261.354679	41.665895
3508.688004	748102.912093	41.670900
3508.353992	747948.198927	41.675904
3508.675828	747800.391479	41.680909
3508.373953	747654.117407	41.685914
3508.660714	747509.176456	41.690919
3508.395848	747371.143847	41.695924
3508.267027	747219.594570	41.700928
3508.120207	747080.301799	41.705933
3508.045535	746937.139693	41.710938
3508.134375	746792.712366	41.715943
3507.886585	746661.781305	41.720948
3507.942468	746522.889910	41.725952
3507.712518	746396.597383	41.730957
3507.874501	746255.607834	41.735962
3507.862667	746117.461825	41.740967
3507.604058	745997.049430	41.745972
3507.818488	745855.599155	41.750976
3507.723936	745727.543437	41.755981
3507.754715	745586.860104	41.760986
3507.928522	745448.523325	41.765991
3507.862281	745320.011384	41.770996
3507.609986	745192.319012	41.776000
3507.246526	745062.319533	41.781005
3507.169821	744928.117987	41.786010
3507.366347	744808.897424	41.791015
3507.204327	744698.187907	41.796020
3507.202489	744556.651067	41.801024
3507.292114	744447.923360	41.806029
3507.254083	744324.334232	41.811034
3507.188272	744189.623878	41.816039
3506.857646	744064.398071	41.821044
3507.005598	743945.320752	41.826048
3506.927776	743831.420882	41.831053
3506.700853	743718.829504	41.836058
3506.407888	743605.752996	41.841063
3506.255669	743492.602160	41.846068
3506.534683	743385.509560	41.851072
3506.476519	743261.412612	41.856077
3506.570200	743160.577688	41.861082
3506.738292	743042.323965	41.866087
3506.124329	742930.823655	41.871092
3506.268904	742819.146969	41.876096
3506.299767	742727.959260	41.881101
3506.675507	742620.889740	41.886106
3506.589483	742504.400671	41.891111
3506.358397	742399.752582	41.896116
3506.522199	742282.773901	41.901120
3506.037726	742178.461458	41.906125
3506.232511	742077.546532	41.911130
3506.012065	741967.550058	41.916135
3505.609011	741872.418444	41.921140
3505.922620	741770.688699	41.926144
3505.986706	741664.745725	41.931149
3505.533023	741566.997669	41.936154
3505.904599	741460.358217	41.941159
3505.396682	741367.413942	41.946164
3505.417657	741279.129116	41.951168
3505.400153	741186.794084	41.956173
3505.413693	741099.003061	41.961178
3505.401466	741002.263167	41.966183
3505.485555	740914.656280	41.971188
3505.608613	740833.620233	41.976192
3505.333397	740736.425947	41.981197
3505.163925	740646.483862	41.986202
3505.497255	740555.023263	41.991207
3505.395739	740462.990452	41.996212
3505.384399	740376.333178	42.001216
3505.271614	740286.031393	42.006221
3504.976324	740199.666431	42.011226
3505.588608	740118.097049	42.016231
3505.115352	740022.262286	42.021236
3505.356944	739927.792219	42.026240
3505.091230	739844.930604	42.031245
3504.873667	739758.646931	42.036250
3505.310297	739669.978696	42.041255
3504.886134	739594.758684	42.046260
3504.819422	739511.366020	42.051264
3504.805256	739423.115809	42.056269
3504.868382	739341.480801	42.061274
3504.666273	739250.390481	42.066279
3504.601730	739181.340389	42.071284
3504.821563	739101.556913	42.076288
3504.948962	739024.063614	42.081293
3504.438503	738946.081300	42.086298
3504.903860	738860.565524	42.091303
3504.358108	738793.619972	42.096308
3504.667774	738699.816695	42.101312
3504.532634	738640.124114	42.106317
3504.412712	738562.271397	42.111322
3504.623192	738476.744146	42.116327
3504.669071	738403.612095	42.121332
3504.580073	738333.420750	42.126336
3504.373374	738256.469954	42.131341
3504.480698	738184.908991	42.136346
3504.658538	738107.052098	42.141351
3504.320356	738042.589277	42.146356
3504.232403	737955.472982	42.151360
3504.498683	737897.044416	42.156365
3504.129678	737828.032904	42.161370
3504.167307	737754.995226	42.166375
3504.172641	737682.902339	42.171380
3504.628084	737608.161431	42.176384
3504.016497	737543.690276	42.181389
3503.635887	737470.719112	42.186394
3504.129188	737397.701828	42.191399
3504.134843	737351.237460	42.196404
3503.937142	737278.283793	42.201408
3503.801620	737214.275612	42.206413
3503.925283	737153.539475	42.211418
3503.972611	737088.658855	42.216423
3504.155265	737024.398640	42.221428
3504.021530	736949.847910	42.226432
3503.606641	736886.378115	42.231437
3503.659326	736835.251381	42.236442
3504.067138	736762.489855	42.241447
3503.591731	736705.511262	42.246452
3503.433458	736638.434088	42.251456
3503.686045	736596.180369	42.256461
3503.305822	736538.294091	42.261466
3503.877373	736478.270609	42.266471
3503.512379	736418.203492	42.271476
3503.545249	736366.087277	42.276480
3503.472808	736304.436825	42.281485
3503.393857	736258.524465	42.286490
3503.741592	736187.994650	42.291495
3503.365281	736134.954762	42.296500
3503.635669	736075.522420	42.301504
3503.401683	736023.596545	42.306509
3503.418855	735979.596825	42.311514
3503.804323	735914.898267	42.316519
3503.374437	735864.686429	42.321524
3503.289652	735801.499915	42.326528
3503.214871	735751.228684	42.331533
3503.219304	735692.579835	42.336538
3503.328954	735637.080707	42.341543
3503.152034	735598.258213	42.346548
3503.084968	735541.847262	42.351552
3503.368793	735490.129321	42.356557
3502.889400	735432.993843	42.361562
3503.451310	735385.287780	42.366567
3503.010476	735340.568333	42.371572
3502.924331	735287.276902	42.376576
3503.137153	735236.064007	42.381581
3502.820847	735187.759472	42.386586
3503.048353	735139.760745	42.391591
3502.994033	735101.905505	42.396596
3503.000506	735046.369848	42.401600
3503.257551	735001.929157	42.406605
3502.820727	734958.642319	42.411610
3503.059584	734906.829061	42.416615
3503.054435	734878.369116	42.421620
3502.832177	734812.920653	42.426624
3502.954478	734769.589897	42.431629
3502.871737	734730.401154	42.436634
3503.074071	734675.820536	42.441639
3502.833501	734644.973232	42.446644
3502.929024	734591.944160	42.451648
3502.558175	734552.505166	42.456653
3502.765045	734502.476569	42.461658
3503.029363	734461.051172	42.466663
3502.897939	734409.444401	42.471668
3502.549557	734374.158843	42.476672
3502.647271	734341.967459	42.481677
3502.676811	734294.243905	42.486682
3503.051915	734243.938396	42.491687
3502.744747	734209.536329	42.496692
3502.668263	734158.908902	42.501696
3502.806467	734126.412954	42.506701
3502.514066	734086.612194	42.511706
3502.518692	734036.812134	42.516711
3502.108011	734008.762645	42.521716
3502.266589	733971.510437	42.526720
3502.353035	733936.151100	42.531725
3502.336081	733910.560867	42.536730
3502.205628	733866.623474	42.541735
3502.354510	733831.005839	42.546740
3502.576019	733795.029517	42.551744
3502.002839	733767.055541	42.556749
3502.224482	733725.979947	42.561754
3502.294657	733689.483613	42.566759
3502.171672	733651.533884	42.571764
3502.074776	733629.223296	42.576768
3502.200138	733595.291680	42.581773
3502.202674	733571.182309	42.586778
3501.981459	733525.376845	42.591783
3501.830339	733509.164090	42.596788
3502.043635	733472.247074	42.601792
3502.223733	733449.395153	42.606797
3501.942632	733420.876643	42.611802
3502.203766	733389.496057	42.616807
3502.082924	733362.337041	42.621812
3502.090107	733331.839812	42.626816
3502.290830	733302.548163	42.631821
3502.053835	733284.566890	42.636826
3502.210725	733235.182280	42.641831
3501.992259	733211.652937	42.646836
3502.025822	733180.358653	42.651840
3502.002812	733152.192604	42.656845
3502.028287	733127.929593	42.661850
3501.993432	733091.596434	42.666855
3501.778052	733071.878320	42.671860
3502.180357	733025.075821	42.676864
3501.840465	733008.596201	42.681869
3501.874770	732982.053881	42.686874
3501.989945	732960.944125	42.691879
3502.026919	732936.233054	42.696884
3502.019472	732893.953350	42.701888
3501.957387	732871.783442	42.706893
3501.859247	732847.440995	42.711898
3502.281770	732817.665346	42.716903
3501.872556	732790.007445	42.721908
3502.022600	732757.850600	42.726912
3501.826171	732735.207413	42.731917
3501.811753	732709.365397	42.736922
3502.188473	732678.804634	42.741927
3501.877044	732652.169831	42.746932
3502.118502	732616.977141	42.751936
3501.898520	732597.704229	42.756941
3501.786606	732578.561948	42.761946
3502.065872	732531.133273	42.766951
3502.068412	732514.199958	42.771956
3501.979259	732488.320073	42.776960
3502.259227	732455.496898	42.781965
3502.011452	732422.513239	42.786970
3502.486073	732394.757438	42.791975
3501.980169	732362.459855	42.796980
3502.042904	732336.257306	42.801985
3501.904680	732295.283419	42.806989
3501.825644	732284.106643	42.811994
3501.857336	732233.449252	42.816999
3501.989649	732226.198563	42.822004
3502.068161	732197.962896	42.827009
3501.905745	732175.362031	42.832013
3501.680410	732138.412380	42.837018
3501.963477	732126.680405	42.842023
3501.707490	732103.203544	42.847028
3501.939818	732071.723576	42.852033
3501.933124	732040.382015	42.857037
3501.821793	732021.337347	42.862042
3502.071780	731976.485038	42.867047
3502.166234	731961.961625	42.872052
3501.719068	731934.356576	42.877057
3501.488423	731900.229096	42.882061
3501.968573	731882.373765	42.887066
3502.078794	731852.448115	42.892071
3501.945749	731838.556267	42.897076
3501.881709	731812.818617	42.902081
3501.759309	731797.488969	42.907085
3501.743581	731771.347073	42.912090
3501.810201	731745.785684	42.917095
3501.659562	731720.359151	42.922100
3501.912515	731692.885165	42.927105
3501.725108	731668.652953	42.932109
3501.372900	731649.944318	42.937114
3501.747896	731637.008030	42.942119
3501.569799	731614.012049	42.947124
3501.748426	731587.837443	42.952129
3501.475839	731568.620286	42.957133
3501.451905	731550.996081	42.962138
3501.721711	731530.302701	42.967143
3502.036303	731509.651386	42.972148
3501.843486	731481.210467	42.977153
3502.029550	731456.173127	42.982157
3501.915311	731432.720412	42.987162
3501.745163	731398.333225	42.992167
3501.389755	731366.848608	42.997172
3501.859534	731342.506817	43.002177
3501.678955	731337.634439	43.007181
3501.467621	731310.483478	43.012186
3501.636850	731287.775808	43.017191
3501.807634	731264.671661	43.022196
3501.728655	731248.838601	43.027201
3501.870759	731228.710272	43.032205
3501.462063	731206.147398	43.037210
3501.388728	731180.458794	43.042215
3501.576664	731157.153426	43.047220
3501.775541	731137.510692	43.052225
3501.742437	731107.011730	43.057229
3501.553127	731104.270037	43.062234
3501.725010	731069.379246	43.067239
3501.491674	731057.285378	43.072244
3501.486513	731030.148927	43.077249
3501.592402	731013.641084	43.082253
3501.481878	731000.883062	43.087258
3501.796414	730968.890017	43.092263
3501.390272	730955.190346	43.097268
3501.672812	730940.336892	43.102273
3501.821108	730910.500516	43.107277
3501.270720	730902.519594	43.112282
3501.711465	730867.979682	43.117287
3501.639591	730860.315818	43.122292
3501.490494	730843.651678	43.127297
3501.547309	730818.584208	43.132301
3501.643807	730804.553608	43.137306
3501.626987	730767.662286	43.142311
3501.105649	730760.716397	43.147316
3501.506744	730736.631757	43.152321
3501.796117	730711.426480	43.157325
3501.139066	730718.815109	43.162330
3501.644721	730690.057895	43.167335
3501.498677	730670.074845	43.172340
3501.521386	730649.023869	43.177345
3501.641837	730631.670946	43.182349
3501.515454	730617.478760	43.187354
3501.436001	730593.225490	43.192359
3501.568062	730574.929578	43.197364
3501.644908	730559.663707	43.202369
3501.772599	730527.749326	43.207373
3501.494763	730510.610535	43.212378
3502.051997	730486.945072	43.217383
3501.615953	730471.219023	43.222388
3501.596185	730446.955453	43.227393
3501.799476	730420.624435	43.232397
3501.396153	730401.673735	43.237402
3501.721930	730373.539428	43.242407
3501.271179	730376.833217	43.247412
3501.053492	730346.906676	43.252417
3501.612008	730325.865369	43.257421
3501.444258	730310.045145	43.262426
3501.634320	730283.517767	43.267431
3501.599131	730272.826224	43.272436
3501.215804	730259.814963	43.277441
3501.396175	730242.748463	43.282445
3501.560351	730243.365343	43.287450
3501.317972	730224.734313	43.292455
3501.070047	730194.267420	43.297460
3501.305366	730188.285570	43.302465
3501.576477	730177.691864	43.307469
3501.079122	730149.098491	43.312474
3501.296686	730137.374473	43.317479
3501.412467	730129.381748	43.322484
3501.386794	730108.188786	43.327489
3501.356660	730088.531836	43.332493
3501.279294	730082.007259	43.337498
3501.612405	730067.242910	43.342503
3501.436798	730038.843613	43.347508
3501.480012	730030.466567	43.352513
3501.570476	730003.707100	43.357517
3501.302454	729988.348565	43.362522
3501.647856	729970.957059	43.367527
3501.272873	729951.505347	43.372532
3500.920857	729936.754925	43.377537
3501.204237	729917.689613	43.382541
3501.020024	729926.486648	43.387546
3501.576143	729900.590919	43.392551
3501.159538	729886.098718	43.397556
3501.150220	729880.602823	43.402561
3501.221294	729852.211636	43.407565
3500.831112	729846.976770	43.412570
3500.998772	729828.277069	43.417575
3501.096062	729833.610227	43.422580
3500.739516	729832.579699	43.427585
3501.174763	729812.894705	43.432589
3500.726549	729799.942956	43.437594
3501.141734	729777.685708	43.442599
3501.013708	729784.591522	43.447604
3501.199951	729786.046778	43.452609
3501.276365	729772.413945	43.457613
3501.028998	729748.284957	43.462618
3501.069491	729737.827848	43.467623
3500.775690	729739.659615	43.472628
3501.000147	729729.568325	43.477633
3501.188817	729712.004051	43.482637
3500.759446	729693.353173	43.487642
3501.174054	729687.638504	43.492647
3501.079050	729677.154179	43.497652
3500.992703	729667.262761	43.502657
3501.232624	729655.286709	43.507661
3501.146546	729644.008395	43.512666
3501.228685	729645.530410	43.517671
3501.072592	729635.551421	43.522676
3500.989095	729616.446973	43.527681
3501.005062	729593.858958	43.532685
3500.850840	729580.065797	43.537690
3500.946683	729583.021926	43.542695
3500.713075	729586.032496	43.547700
3500.851112	729579.570979	43.552705
3501.229101	729569.602709	43.557709
3501.134839	729547.874792	43.562714
3501.282404	729533.833561	43.567719
3500.896728	729535.482435	43.572724
3501.327542	729522.186858	43.577729
3501.463847	729498.439498	43.582733
3501.294646	729492.325867	43.587738
3501.337011	729476.419766	43.592743
3501.110264	729466.749428	43.597748
3501.158060	729453.715157	43.602753
3501.065383	729454.721260	43.607757
3500.952315	729448.103013	43.612762
3501.197844	729429.587652	43.617767
3500.975086	729406.691853	43.622772
3501.269774	729402.482731	43.627777
3501.323845	729395.935882	43.632781
3501.046035	729383.004837	43.637786
3501.310555	729360.523695	43.642791
3500.982126	729351.167209	43.647796
3501.180661	729348.360825	43.652801
3501.508173	729330.327003	43.657805
3501.054745	729308.954990	43.662810
3501.146750	729303.689618	43.667815
3501.035673	729311.682724	43.672820
3500.987470	729282.516758	43.677825
3501.067189	729274.974941	43.682829
3500.901406	729265.641011	43.687834
3501.281051	729257.405700	43.692839
3501.357238	729249.666315	43.697844
3501.299162	729228.278288	43.702849
3501.636997	729217.127457	43.707853
3501.578418	729202.376741	43.712858
3501.544515	729172.762229	43.717863
3501.222665	729172.369800	43.722868
3501.220624	729145.077942	43.727873
3501.263504	729123.821555	43.732877
3501.065852	729114.789914	43.737882
3501.045655	729117.616789	43.742887
3501.009040	729090.479060	43.747892
3501.009130	729080.523112	43.752897
3501.456079	729073.465285	43.757901
3501.023853	729077.747186	43.762906
3501.295247	729056.601459	43.767911
3501.271018	729037.139126	43.772916
3501.035535	729027.321108	43.777921
3501.496330	729010.057086	43.782925
3501.202413	728990.193407	43.787930
3501.554270	728968.241619	43.792935
3501.344467	728964.561445	43.797940
3501.188759	728942.247662	43.802945
3501.296915	728926.874487	43.807949
3501.236139	728921.980854	43.812954
3501.437577	728903.025780	43.817959
3501.368168	728880.202226	43.822964
3501.081358	728883.519049	43.827969
3501.322532	728872.581859	43.832973
3501.020150	728849.549048	43.837978
3501.444526	728830.012086	43.842983
3501.488633	728830.401247	43.847988
3501.435299	728807.376695	43.852993
3501.534406	728797.552642	43.857997
3501.149694	728783.053199	43.863002
3501.236258	728740.983988	43.868007
3501.318155	728743.199703	43.873012
3501.126712	728728.024268	43.878017
3501.385060	728721.096376	43.883021
3500.971738	728704.570581	43.888026
3501.135194	728699.094872	43.893031
3501.309022	728696.837236	43.898036
3501.399843	728674.432444	43.903041
3501.248638	728655.089252	43.908045
3501.068759	728659.280133	43.913050
3500.924713	728643.452747	43.918055
3501.288691	728631.207016	43.923060
3500.945442	728615.907852	43.928065
3501.263683	728602.777994	43.933069
3500.904506	728609.326712	43.938074
3501.211059	728603.133791	43.943079
3501.414619	728571.496421	43.948084
3501.210105	728562.415763	43.953089
3501.085165	728558.770916	43.958093
3501.046843	728555.111754	43.963098
3501.443446	728519.875683	43.968103
3501.404666	728516.910087	43.973108
3501.251441	728506.830165	43.978113
3501.335989	728470.753795	43.983117
3501.130312	728474.205985	43.988122
3501.166110	728472.169244	43.993127
3501.416092	728454.740742	43.998132
3501.029955	728429.342820	44.003137
3501.135251	728420.260344	44.008141
3500.789170	728428.838055	44.013146
3501.239865	728409.246203	44.018151
3500.918422	728384.085134	44.023156
3500.731113	728375.050961	44.028161
3501.111211	728363.842448	44.033165
3501.049010	728367.964493	44.038170
3501.030087	728363.311294	44.043175
3500.969338	728346.627433	44.048180
3500.700887	728327.352376	44.053185
3500.903406	728323.405622	44.058189
3500.640346	728324.687706	44.063194
3500.987866	728316.159535	44.068199
3500.846841	728322.523819	44.073204
3500.509803	728324.907954	44.078209
3500.879998	728318.258463	44.083213
3500.737435	728321.403061	44.088218
3501.141322	728294.388038	44.093223
3500.696733	728278.560072	44.098228
3500.555152	728267.487174	44.103233
3500.672742	728270.786952	44.108237
3500.705580	728276.825313	44.113242
3501.163530	728262.235225	44.118247
3500.822629	728275.369724	44.123252
3500.592348	728268.769886	44.128257
3500.846598	728265.111783	44.133261
3500.582034	728232.113859	44.138266
3501.006746	728227.734037	44.143271
3500.967586	728213.919545	44.148276
3501.152599	728216.910974	44.153281
3500.794090	728209.391053	44.158285
3500.990569	728230.263852	44.163290
3500.810730	728196.855480	44.168295
3500.778732	728183.287445	44.173300
3500.888274	728172.668302	44.178305
3500.920253	728175.437344	44.183309
3500.780933	728168.772855	44.188314
3500.996812	728163.189048	44.193319
3501.080189	728178.829588	44.198324
3501.058446	728162.782905	44.203329
3501.195819	728130.560303	44.208333
3500.800538	728140.236297	44.213338
3500.841246	728131.411866	44.218343
3500.925067	728122.877534	44.223348
3500.847288	728119.918238	44.228353
3501.034973	728090.461333	44.233357
3500.990585	728081.304138	44.238362
3500.961863	728076.157005	44.243367
3500.942670	728074.525564	44.248372
3500.829974	728075.832377	44.253377
3500.877443	728070.474493	44.258381
3500.608132	728062.295688	44.263386
3500.879481	728041.543656	44.268391
3501.152140	728035.454986	44.273396
3500.664619	728033.752313	44.278401
3500.692406	728036.670712	44.283405
3501.040625	728033.938223	44.288410
3500.918439	728032.323794	44.293415
3500.970038	728029.194467	44.298420
3500.859800	728003.601006	44.303425
3501.228008	727986.251049	44.308429
3500.789928	727989.940005	44.313434
3500.849469	727985.224084	44.318439
3501.155550	727980.071102	44.323444
3501.155566	727978.386928	44.328449
3500.978302	727967.517678	44.333453
3501.137523	727959.317492	44.338458
3501.107277	727950.603671	44.343463
3501.007125	727938.780384	44.348468
3501.102136	727919.493839	44.353473
3500.989232	727901.529648	44.358477
3500.314161	727915.017187	44.363482
3500.552085	727907.695664	44.368487
3500.922202	727899.856888	44.373492
3500.822423	727910.970521	44.378497
3501.056473	727905.928476	44.383501
3500.967439	727889.991456	44.388506
3500.678089	727870.718772	44.393511
3500.981745	727861.404735	44.398516
3500.772949	727858.813778	44.403521
3500.572227	727852.803201	44.408525
3500.659974	727860.517168	44.413530
3500.945050	727854.872176	44.418535
3500.821234	727863.562368	44.423540
3500.901111	727860.676006	44.428545
3501.160700	727840.767593	44.433549
3500.972034	727831.832123	44.438554
3500.950103	727826.188305	44.443559
3501.187359	727809.107316	44.448564
3500.825788	727814.715790	44.453569
3500.861886	727800.145053	44.458573
3501.015426	727792.391505	44.463578
3501.026464	727777.923951	44.468583
3501.036725	727770.838092	44.473588
3500.971200	727768.570215	44.478593
3501.213851	727756.045982	44.483597
3500.990578	727736.217111	44.488602
3501.121488	727727.823208	44.493607
3501.154175	727728.214310	44.498612
3500.816922	727725.050045	44.503617
3501.263812	727704.367232	44.508621
3500.966688	727694.260543	44.513626
3500.704315	727677.856341	44.518631
3500.519756	727681.305373	44.523636
3500.748385	727670.764983	44.528641
3500.877542	727677.431909	44.533645
3500.631472	727678.760825	44.538650
3500.586740	727668.166522	44.543655
3500.674585	727670.183381	44.548660
3500.683996	727681.031575	44.553665
3500.608827	727662.367042	44.558669
3500.507941	727659.163690	44.563674
3500.664081	727638.330592	44.568679
3500.826453	727632.210308	44.573684
3500.587113	727629.872033	44.578689
3500.796497	727622.703597	44.583693
3500.697643	727629.804576	44.588698
3500.901742	727631.950858	44.593703
3501.116486	727631.023795	44.598708
3500.909510	727635.467384	44.603713
3501.205362	727622.636906	44.608717
3500.950353	727606.825845	44.613722
3500.938908	727589.537788	44.618727
3501.111516	727597.287522	44.623732
3500.778534	727599.076690	44.628737
3500.984757	727586.905012	44.633741
3500.698077	727575.012939	44.638746
3501.040989	727564.651695	44.643751
3501.133765	727547.445410	44.648756
3500.888439	727543.076868	44.653761
3500.946652	727534.496611	44.658765
3500.887930	727540.203852	44.663770
3500.821169	727516.632912	44.668775
3500.665477	727501.152031	44.673780
3500.507910	727487.207251	44.678785
3500.622187	727487.039913	44.683789
3500.524757	727493.942604	44.688794
3500.503427	727488.694794	44.693799
3500.917603	727492.441301	44.698804
3500.852482	727503.599302	44.703809
3500.789408	727488.152634	44.708813
3500.848175	727509.743629	44.713818
3500.867329	727501.912930	44.718823
3501.024817	727496.338319	44.723828
3500.649019	727460.828990	44.728833
3500.980350	727460.179898	44.733837
3500.838991	727455.298701	44.738842
3500.588854	727444.837139	44.743847
3501.011002	727437.484753	44.748852
3500.856976	727456.039395	44.753857
3500.675400	727442.891191	44.758861
3500.717045	727442.438598	44.763866
3500.650884	727426.447352	44.768871
3500.871795	727416.502426	44.773876
3500.443640	727415.929296	44.778881
3501.114430	727407.891736	44.783885
3500.643750	727406.136599	44.788890
3501.000771	727401.817070	44.793895
3500.953899	727407.522445	44.798900
3501.093490	727407.846353	44.803905
3500.891672	727383.256944	44.808909
3501.100518	727373.313960	44.813914
3501.090230	727361.128183	44.818919
3500.947284	727362.241934	44.823924
3500.800681	727358.451498	44.828929
3501.286099	727349.899538	44.833933
3501.355738	727336.412387	44.838938
3501.276833	727318.837645	44.843943
3501.279721	727312.148955	44.848948
3501.050425	727296.878025	44.853953
3501.203152	727279.908989	44.858957
3501.260991	727273.855256	44.863962
3501.384185	727269.970650	44.868967
3501.229053	727250.377058	44.873972
3501.102099	727243.907945	44.878977
3501.202642	727224.073862	44.883981
3501.242866	727222.184711	44.888986
3501.110094	727199.069663	44.893991
3501.329713	727189.124675	44.898996
3501.297192	727189.080680	44.904001
3501.309911	727167.824187	44.909005
3500.938181	727149.653393	44.914010
3501.083672	727146.260490	44.919015
3500.784753	727131.694381	44.924020
3500.931335	727139.052494	44.929025
3500.836093	727105.427500	44.934029
3500.861354	727102.054447	44.939034
3501.026727	727092.366031	44.944039
3500.888424	727088.078649	44.949044
3500.748245	727090.876508	44.954049
3501.166056	727089.767193	44.959053
3500.664415	727076.819926	44.964058
3500.964825	727056.754229	44.969063
3500.998229	727052.141181	44.974068
3500.809257	727055.095751	44.979073
3501.116388	727045.086582	44.984077
3500.909916	727053.989473	44.989082
3500.728277	727039.304727	44.994087
3501.190959	727020.153485	44.999092
3501.176437	727016.341063	45.004097
3500.932728	726998.099230	45.009101
3501.045743	727005.066646	45.014106
3501.346268	726999.517607	45.019111
3501.386804	726976.918292	45.024116
3500.601472	726963.571815	45.029121
3501.000839	726955.479579	45.034125
3501.162656	726966.848537	45.039130
3501.125650	726938.019165	45.044135
3501.121951	726924.989370	45.049140
3500.755552	726917.023642	45.054145
3501.004130	726911.185851	45.059149
3500.888360	726906.052366	45.064154
3500.871039	726911.703656	45.069159
3500.884864	726877.019232	45.074164
3501.008753	726871.102926	45.079169
3501.294766	726873.830429	45.084173
3500.966173	726869.623924	45.089178
3500.979618	726864.568151	45.094183
3501.112142	726838.385916	45.099188
3500.893889	726827.274187	45.104193
3501.014515	726814.223671	45.109197
3501.201475	726825.687764	45.114202
3500.951733	726807.446502	45.119207
3501.195942	726791.254085	45.124212
3500.898881	726785.952295	45.129217
3500.964407	726777.716866	45.134221
3501.005448	726774.588806	45.139226
3500.925773	726780.052303	45.144231
3501.214528	726755.776313	45.149236
3501.093033	726744.301653	45.154241
3501.182976	726727.143661	45.159245
3501.233215	726736.846774	45.164250
3501.251317	726713.309044	45.169255
3501.130921	726700.496366	45.174260
3501.098258	726688.263737	45.179265
3500.735173	726693.229106	45.184269
3501.013426	726688.129464	45.189274
3501.106528	726660.962228	45.194279
3500.903614	726637.708543	45.199284
3500.654217	726637.551741	45.204289
3500.896832	726637.809109	45.209293
3501.022248	726637.739011	45.214298
3500.721388	726637.541166	45.219303
3501.050998	726622.523448	45.224308
3500.870169	726602.040688	45.229313
3501.276320	726583.343702	45.234317
3501.066367	726582.833544	45.239322
3501.173520	726583.014204	45.244327
3501.250966	726560.308545	45.249332
3501.291791	726553.266129	45.254337
3501.198915	726535.642465	45.259341
3501.017926	726539.884156	45.264346
3500.937907	726527.262727	45.269351
3501.386231	726518.765585	45.274356
3500.885660	726512.357634	45.279361
3501.227891	726492.580939	45.284365
3501.244402	726494.956717	45.289370
3500.951988	726475.433504	45.294375
3501.192161	726460.132977	45.299380
3501.412008	726460.939151	45.304385
3501.396623	726436.563831	45.309389
3501.403375	726426.306256	45.314394
3501.199642	726428.123862	45.319399
3501.580053	726394.565993	45.324404
3501.359140	726380.629794	45.329409
3501.785409	726367.032565	45.334413
3501.235364	726340.267846	45.339418
3501.139931	726331.414424	45.344423
3501.153079	726328.439452	45.349428
3500.919959	726302.315929	45.354433
3501.214680	726274.222199	45.359437
3500.840939	726290.437391	45.364442
3500.728391	726267.365920	45.369447
3501.003033	726262.514363	45.374452
3500.745740	726280.196831	45.379457
3501.047649	726273.854278	45.384461
3500.897141	726244.644824	45.389466
3500.975510	726230.658911	45.394471
3501.216110	726224.177801	45.399476
3500.825370	726227.958813	45.404481
3501.245168	726213.718248	45.409485
3500.891894	726205.452352	45.414490
3500.945594	726177.596323	45.419495
3501.067204	726181.986394	45.424500
3500.883805	726181.719574	45.429505
3500.849938	726166.414236	45.434509
3500.707747	726170.302852	45.439514
3500.292070	726159.966099	45.444519
3501.132047	726149.867788	45.449524
3500.934108	726143.558186	45.454529
3501.148231	726132.473163	45.459533
3501.069117	726137.738792	45.464538
3500.985123	726134.730251	45.469543
3501.562542	726112.783095	45.474548
3501.372839	726098.890809	45.479553
3501.401365	726084.367823	45.484557
3501.047357	726062.524903	45.489562
3500.988142	726048.412762	45.494567
3501.343744	726050.484877	45.499572
3501.451523	726040.903843	45.504577
3501.194926	726008.242486	45.509581
3500.980467	726002.480571	45.514586
3500.902655	725995.655488	45.519591
3501.287613	725986.870963	45.524596
3500.891583	725975.490145	45.529601
3501.347759	725953.463497	45.534605
3501.254088	725956.303606	45.539610
3500.989657	725954.117647	45.544615
3501.027381	725946.877015	45.549620
3501.056053	725930.173449	45.554625
3500.987074	725908.332568	45.559629
3500.815292	725907.766505	45.564634
3500.601384	725911.617542	45.569639
3501.177740	725902.702193	45.574644
3500.831840	725903.502812	45.579649
3500.842047	725877.238620	45.584653
3501.045122	725870.812985	45.589658
3500.750865	725869.424769	45.594663
3500.914424	725864.442679	45.599668
3500.597509	725864.742987	45.604673
3501.196106	725859.342135	45.609677
3500.827783	725845.478937	45.614682
3500.851254	725827.190341	45.619687
3500.864600	725807.268137	45.624692
3500.576991	725815.392932	45.629697
3500.743715	725806.594726	45.634701
3501.008791	725811.010841	45.639706
3501.268798	725808.093991	45.644711
3501.383999	725805.547939	45.649716
3501.074764	725788.007975	45.654721
3501.523492	725774.653823	45.659725
3501.421347	725771.400384	45.664730
3501.374887	725750.695080	45.669735
3501.342044	725731.226303	45.674740
3501.226107	725729.610381	45.679745
3500.943786	725696.753822	45.684749
3500.981272	725696.400929	45.689754
3500.949111	725680.797083	45.694759
3501.363560	725683.801085	45.699764
3501.056364	725670.026595	45.704769
3500.964969	725654.729810	45.709773
3500.984020	725646.401819	45.714778
3500.987079	725634.558146	45.719783
3501.078105	725634.691940	45.724788
3500.761366	725634.397581	45.729793
3501.135732	725610.649153	45.734797
3501.280648	725607.800807	45.739802
3501.144144	725600.786878	45.744807
3501.294106	725593.230064	45.749812
3501.003447	725571.375366	45.754817
3500.994625	725537.382780	45.759821
3501.217076	725467.325590	45.764826
3500.788249	725345.689192	45.769831
3500.884894	725171.483925	45.774836
3500.759859	724944.383904	45.779841
3500.736274	724648.769618	45.784845
3500.388726	724308.344989	45.789850
3500.111839	723900.685831	45.794855
3500.187156	723438.573524	45.799860
3499.839134	722927.827687	45.804865
3499.533115	722347.244139	45.809869
3499.199309	721705.942016	45.814874
3498.968126	721026.990723	45.819879
3499.026253	720275.937737	45.824884
3498.431582	719478.904890	45.829889
3497.743433	718614.609315	45.834893
3496.955183	717689.826784	45.839898
3496.327380	716728.901066	45.844903
3496.164234	715686.423510	45.849908
3495.596455	714591.485667	45.854913
3495.100773	713441.507373	45.859917
3494.616517	712233.101593	45.864922
3493.813838	710962.078926	45.869927
3493.245305	709622.561351	45.874932
3492.638955	708247.335674	45.879937
3491.986203	706791.638887	45.884941
3490.861277	705288.931778	45.889946
3490.112906	703718.680645	45.894951
3489.332580	702086.880479	45.899956
3488.706944	700413.944106	45.904961
3487.654827	698648.295255	45.909965
3486.947344	696849.418251	45.914970
3485.772199	694985.649987	45.919975
3484.970055	693072.431670	45.924980
3483.338638	691100.478979	45.929985
3482.802984	689067.496245	45.934989
3481.500070	686982.363883	45.939994
3480.733321	684842.044816	45.944999
3479.788095	682632.129193	45.950004
3478.387878	680378.019800	45.955009
3477.138444	678059.009572	45.960013
3475.859465	675696.712746	45.965018
3474.731831	673266.045279	45.970023
3473.396699	670781.079042	45.975028
3471.938144	668257.373186	45.980033
3470.443839	665667.497022	45.985037
3469.224999	663031.012660	45.990042
3467.877376	660343.361464	45.995047
3466.579859	657574.317755	46.000052
3465.088894	654796.630985	46.005057
3463.431243	651935.504326	46.010061
3462.350862	649034.777742	46.015066
3460.473196	646077.804347	46.020071
3459.152480	643058.167459	46.025076
3457.424904	640002.539060	46.030081
3455.551930	636894.890670	46.035085
3454.043964	633729.894305	46.040090
3452.234118	630525.840866	46.045095
3450.691773	627256.868323	46.050100
3448.638450	623960.327012	46.055105
3447.056515	620595.949791	46.060109
3445.083326	617190.645024	46.065114
3442.808284	613739.155868	46.070119
3441.686162	610238.551665	46.075124
3439.389819	606695.655563	46.080129
3437.706148	603097.195502	46.085133
3435.796467	599459.989288	46.090138
3433.642381	595767.895364	46.095143
3431.940790	592013.676787	46.100148
3429.799609	588230.905647	46.105153
3427.729719	584392.791942	46.110157
3425.515168	580508.536567	46.115162
3423.791055	576596.920160	46.120167
3421.952781	572608.923292	46.125172
3419.278218	568609.439566	46.130177
3417.051958	564533.262302	46.135181
3414.686377	560437.800403	46.140186
3412.313639	556303.484800	46.145191
3410.427089	552100.230932	46.150196
3408.061708	547878.515545	46.155201
3405.504609	543598.254892	46.160205
3403.082228	539293.108195	46.165210
3400.749857	534936.893681	46.170215
3398.611738	530525.885104	46.175220
3395.988121	526099.145066	46.180225
3393.389393	521623.518373	46.185229
3391.030037	517102.334524	46.190234
3388.577270	512540.332292	46.195239
3386.319234	507945.945284	46.200244
3383.784048	503308.125375	46.205249
3380.899916	498629.098676	46.210253
3378.499247	493920.304535	46.215258
3375.603439	489173.759862	46.220263
3372.921496	484378.562445	46.225268
3370.068006	479561.599544	46.230273
3367.531266	474700.771448	46.235277
3364.819640	469797.167567	46.240282
3361.772710	464875.184009	46.245287
3359.122902	459903.241855	46.250292
3355.896947	454910.899521	46.255297
3353.502333	449883.641342	46.260301
3350.871127	444818.506478	46.265306
3347.455150	439741.211237	46.270311
3344.763776	434615.807674	46.275316
3341.453123	429463.988624	46.280321
3338.499998	424272.918312	46.285325
3335.610785	419070.201149	46.290330
3332.554334	413845.213023	46.295335
3329.309456	408567.857553	46.300340
3326.044609	403282.008963	46.305345
3323.055019	397953.451791	46.310349
3319.772808	392612.991950	46.315354
3316.594525	387251.750455	46.320359
3313.842567	381851.779886	46.325364
3309.958379	376443.638887	46.330369
3306.695531	370989.107487	46.335373
3303.805573	365528.556348	46.340378
3300.251544	360052.757812	46.345383
3296.765068	354544.046338	46.350388
3293.452509	349024.618596	46.355393
3290.135073	343474.846547	46.360397
3286.538569	337924.759893	46.365402
3282.955430	332333.986480	46.370407
3279.779754	326730.465076	46.375412
3275.940420	321116.907039	46.380417
3272.578147	315476.794843	46.385421
3269.188304	309846.606418	46.390426
3265.178485	304192.265075	46.395431
3261.714260	298515.730952	46.400436
3258.092202	292833.102082	46.405441
3254.517186	287137.563744	46.410445
3250.989053	281433.743476	46.415450
3247.116139	275715.612914	46.420455
3243.367888	269988.079704	46.425460
3239.384315	264264.364859	46.430465
3235.661062	258517.257737	46.435469
3231.918624	252775.731580	46.440474
3227.617380	247029.097984	46.445479
3224.148729	241279.974824	46.450484
3219.760890	235521.822420	46.455489
3215.866788	229771.898563	46.460493
3212.277140	224005.808700	46.465498
3208.492976	218228.013164	46.470503
3204.406987	212468.216146	46.475508
3199.945182	206653.441682	46.480513
3196.167216	200868.629041	46.485517
3192.027018	195109.778785	46.490522
3187.796132	189350.720173	46.495527
3184.001523	183596.414095	46.500532
3179.369493	177856.341479	46.505537
3175.094384	172110.321462	46.510541
3170.830136	166383.316730	46.515546
3166.578661	160664.783739	46.520551
3162.593450	154954.112895	46.525556
3157.858743	149254.019850	46.530561
3153.259248	143570.285798	46.535565
3148.974861	137895.520726	46.540570
3143.996435	132249.924161	46.545575
3139.651861	126611.628089	46.550580
3134.728226	120994.543984	46.555585
3129.666564	115409.148720	46.560589
3124.830519	109851.051371	46.565594
3120.110107	104314.367213	46.570599
3115.113972	98807.644691	46.575604
3110.218052	93337.729627	46.580609
3105.306494	87887.522083	46.585613
3100.145253	82471.613460	46.590618
3094.576294	77109.761607	46.595623
3088.972235	71772.647205	46.600628
3082.801628	66500.886693	46.605633
3076.417849	61300.310070	46.610637
3064.113999	56304.007168	46.615642
3049.112200	51489.386862	46.620647
3035.176823	46824.897983	46.625652
3021.408356	42377.950898	46.630657
3007.742740	38118.463087	46.635661
2994.792529	34076.343399	46.640666
2982.039099	30260.608641	46.645671
2970.187148	26685.602991	46.650676
2958.106126	23337.799093	46.655681
2946.511020	20201.173205	46.660685
2934.326261	17307.233141	46.665690
2919.607635	14733.741180	46.670695
2902.484640	12456.483348	46.675700
2884.231028	10488.248515	46.680705
2867.537969	8793.447084	46.685709
2853.339783	7371.643585	46.690714
2840.250050	6204.679354	46.695719
2830.114868	5244.407637	46.700724
2820.985048	4498.397435	46.705729
2813.884949	3903.123648	46.710733
2808.254670	3441.131009	46.715738
2803.311116	3104.456440	46.720743
2799.808839	2838.674990	46.725748
2796.867790	2647.226748	46.730753
2794.802566	2491.272157	46.735757
2792.924405	2370.872045	46.740762
2791.077607	2254.569700	46.745767
2789.662392	2149.681355	46.750772
2787.803477	2044.815448	46.755777
2786.415888	1938.826619	46.760781
2784.954585	1821.415324	46.765786
2782.988661	1699.667628	46.770791
2781.633692	1565.564349	46.775796
2779.242542	1412.512489	46.780801
2777.022747	1251.641530	46.785805
2774.891480	1081.097310	46.790810
2772.317115	919.317130	46.795815
2769.054077	737.912944	46.800820
2765.911217	554.560980	46.805825
2762.720277	394.184499	46.810829
2759.430099	227.405294	46.815834
2754.545375	104.069378	46.820839
2740.846168	223.869721	46.825844
2734.543298	231.799142	46.830849
2731.745500	228.920698	46.835853
2730.237786	220.702439	46.840858
2728.531992	236.360632	46.845863
2727.014360	220.343406	46.850868
2724.271360	242.610883	46.855873
2720.976428	228.488073	46.860877
2717.877859	226.830435	46.865882
2714.122677	231.410243	46.870887
2710.836536	227.261077	46.875892
2707.621577	225.450634	46.880897
2704.107974	216.507882	46.885901
2700.981153	225.967077	46.890906
2697.356173	230.055285	46.895911
2694.192287	221.497476	46.900916
2691.018970	221.634003	46.905921
2687.684460	226.033882	46.910925
2684.401795	222.823496	46.915930
2680.845489	230.187222	46.920935
2677.705830	219.467123	46.925940
2674.180298	230.733658	46.930945
2670.695114	224.333082	46.935949
2668.018204	222.507798	46.940954
2664.271535	220.300550	46.945959
2660.929829	216.292251	46.950964
2656.856365	224.801906	46.955969
2653.441488	223.484794	46.960973
2650.452395	224.351002	46.965978
2647.067187	228.510066	46.970983
2643.783577	220.823833	46.975988
2639.838360	223.124326	46.980993
2636.538065	230.130158	46.985997
2634.107706	223.994855	46.991002
2629.875107	221.220418	46.996007
2626.375147	209.509586	47.001012
2622.424026	220.979812	47.006017
2619.024005	222.731449	47.011021
2616.837908	203.497444	47.016026
2612.849143	213.958008	47.021031
2609.444808	207.107596	47.026036
2606.257605	220.463226	47.031041
2602.331863	217.208015	47.036045
2599.049058	211.910474	47.041050
2595.380902	225.698978	47.046055
2592.079610	210.752284	47.051060
2588.599217	205.135811	47.056065
2584.431909	206.177991	47.061069
2581.451694	202.615492	47.066074
2578.138694	213.231989	47.071079
2575.002297	195.048318	47.076084
2571.593061	202.814409	47.081089
2567.994155	205.815604	47.086093
2563.898412	198.765350	47.091098
2560.475329	203.752657	47.096103
2557.540547	197.951155	47.101108
2554.177189	205.379518	47.106113
2550.698465	206.230759	47.111117
2547.281219	191.799433	47.116122
2543.345849	202.963201	47.121127
2539.944639	193.194892	47.126132
2536.783072	204.632918	47.131137
2532.987430	198.584622	47.136141
2529.775832	208.241082	47.141146
2525.923154	207.985033	47.146151
2522.823307	196.569386	47.151156
2519.465166	199.459317	47.156161
2515.822682	202.927172	47.161165
2512.434277	201.562380	47.166170
2508.698610	195.206791	47.171175
2505.063521	199.448573	47.176180
2501.829838	204.004756	47.181185
2498.237845	207.373490	47.186189
2495.233913	198.072446	47.191194
2491.313205	197.004202	47.196199
2487.970676	201.627555	47.201204
2484.794682	200.851596	47.206209
2481.092121	201.287068	47.211213
2477.388464	191.507131	47.216218
2473.623600	195.298987	47.221223
2470.566206	197.390652	47.226228
2467.204545	191.314567	47.231233
2463.484607	190.099043	47.236237
2460.320372	186.788523	47.241242
2456.679793	188.696549	47.246247
2452.765619	194.084745	47.251252
2449.488032	184.663496	47.256257
2446.188081	194.396005	47.261261
2442.757307	194.108648	47.266266
2438.972604	193.222768	47.271271
2435.545710	192.194758	47.276276
2432.160231	194.900627	47.281281
2428.704491	190.568242	47.286285
2425.404369	183.706270	47.291290
2421.711008	191.239099	47.296295
2418.447685	182.318135	47.301300
2414.951647	178.468220	47.306305
2410.813061	183.089463	47.311309
2407.929642	185.894151	47.316314
2404.193496	195.552304	47.321319
2400.857294	193.256208	47.326324
2397.500017	195.055600	47.331329
2393.400417	195.503028	47.336333
2390.332059	185.180473	47.341338
2386.882693	191.945535	47.346343
2383.716371	177.645101	47.351348
2380.148081	181.052626	47.356353
2376.125185	183.214466	47.361357
2372.536808	176.565058	47.366362
2368.794928	186.590442	47.371367
2365.557859	180.075853	47.376372
2362.571983	186.535654	47.381377
2358.627438	181.752462	47.386381
2355.826908	178.739367	47.391386
2352.293230	187.966783	47.396391
2348.801961	180.378365	47.401396
2345.232517	182.575643	47.406401
2341.404827	196.879728	47.411405
2337.647357	184.855448	47.416410
2333.768660	171.967386	47.421415
2330.937928	184.369387	47.426420
2327.545888	176.813496	47.431425
2323.657786	184.643481	47.436429
2320.457575	175.414569	47.441434
2316.969020	187.270373	47.446439
2313.421515	182.875735	47.451444
2309.878520	171.182428	47.456449
2306.518683	182.485289	47.461453
2303.382865	169.905204	47.466458
2299.555320	181.965955	47.471463
2295.918362	182.707055	47.476468
2292.130702	178.820299	47.481473
2288.713511	184.793911	47.486477
2285.196488	177.538978	47.491482
2281.990842	184.420631	47.496487
2278.837549	181.712691	47.501492
2275.240919	185.301810	47.506497
2271.356773	183.849621	47.511501
2268.102765	179.229203	47.516506
2264.358571	186.455428	47.521511
2261.039890	178.617881	47.526516
2257.664286	175.464095	47.531521
2254.061003	175.354655	47.536525
2250.543506	173.285264	47.541530
2246.678355	181.038496	47.546535
2243.469813	178.506683	47.551540
2239.905404	177.254746	47.556545
2236.505918	182.923341	47.561549
2233.219543	177.031936	47.566554
2229.844517	177.971245	47.571559
2225.928201	182.297331	47.576564
2222.445218	182.923003	47.581569
2218.742270	189.814657	47.586573
2215.739390	168.293381	47.591578
2211.914136	177.821985	47.596583
2208.793408	173.904161	47.601588
2205.088527	178.961302	47.606593
2201.586290	176.236832	47.611597
2198.223784	176.904727	47.616602
2194.479637	173.974652	47.621607
2190.784448	170.316585	47.626612
2187.693644	171.848414	47.631617
2183.434538	184.328655	47.636621
2180.546863	169.824581	47.641626
2177.191529	177.382905	47.646631
2173.963530	168.916897	47.651636
2170.261054	170.369505	47.656641
2166.519788	183.817162	47.661645
2163.209410	173.281520	47.666650
2159.765963	177.707325	47.671655
2156.204513	171.329735	47.676660
2152.354283	175.810503	47.681665
2148.759950	177.960561	47.686669
2145.349435	169.919488	47.691674
2141.968277	174.077265	47.696679
2138.718587	181.906229	47.701684
2135.324016	165.992333	47.706689
2131.543733	169.781704	47.711693
2128.090226	169.527382	47.716698
2124.293743	172.746575	47.721703
2121.077235	174.009785	47.726708
2117.829496	170.787969	47.731713
2113.906504	173.243716	47.736717
2110.749394	165.361584	47.741722
2106.899880	170.022045	47.746727
2103.704615	163.841363	47.751732
2100.195210	167.362300	47.756737
2096.515640	167.048369	47.761741
2093.107340	168.504008	47.766746
2089.546168	171.122822	47.771751
2085.886418	156.452334	47.776756
2082.529680	162.789045	47.781761
2078.867677	173.116956	47.786765
2075.746205	170.789700	47.791770
2072.323546	173.047146	47.796775
2068.600186	170.268655	47.801780
2065.115312	172.332172	47.806785
2061.141728	169.789524	47.811789
2058.064719	158.863076	47.816794
2054.420576	164.354678	47.821799
2050.889962	168.400533	47.826804
2047.658094	166.205454	47.831809
2044.056861	167.567396	47.836813
2040.541127	166.434063	47.841818
2036.936082	168.751160	47.846823
2033.514568	160.404370	47.851828
2030.236825	159.693182	47.856833
2026.440451	161.727436	47.861837
2023.251702	152.629706	47.866842
2019.558961	152.236132	47.871847
2016.403151	165.064135	47.876852
2012.748600	159.357663	47.881857
2009.162115	159.680978	47.886861
2005.575100	159.458157	47.891866
2001.909102	167.221018	47.896871
1998.377353	162.490562	47.901876
1995.034121	160.320294	47.906881
1991.386330	163.469972	47.911885
1988.160358	165.351726	47.916890
1984.596146	164.533924	47.921895
1980.743110	162.800984	47.926900
1977.437093	157.244390	47.931905
1973.794575	164.340529	47.936909
1970.648210	169.209803	47.941914
1967.307639	165.224016	47.946919
1963.619340	167.943331	47.951924
1960.495019	155.523672	47.956929
1956.513794	162.764753	47.961933
1953.300100	153.103876	47.966938
1949.477598	164.170863	47.971943
1945.817652	163.746464	47.976948
1942.564468	151.149660	47.981953
1938.901934	157.288114	47.986957
1935.651924	152.633970	47.991962
1931.772530	161.182916	47.996967
1928.480325	159.125413	48.001972
1925.259629	161.110928	48.006977
1921.278414	155.301206	48.011981
1917.818548	152.605094	48.016986
1914.297820	162.289487	48.021991
1911.141640	158.643790	48.026996
1907.998088	157.713521	48.032001
1904.024855	170.136759	48.037005
1900.872642	149.133705	48.042010
1897.157078	167.203840	48.047015
1893.459506	152.034250	48.052020
1890.218460	160.757854	48.057025
1886.518310	162.429173	48.062029
1882.966808	160.520651	48.067034
1879.303625	157.317369	48.072039
1875.679973	159.056335	48.077044
1872.723936	159.088209	48.082049
1869.117347	164.283854	48.087053
1865.341698	156.759605	48.092058
1861.718724	156.742969	48.097063
1858.463557	158.544411	48.102068
1855.448933	152.599423	48.107073
1851.497044	155.911312	48.112077
1847.524578	154.425627	48.117082
1844.258668	159.416430	48.122087
1841.377379	159.865934	48.127092
1837.779015	154.744103	48.132097
1834.241121	159.789268	48.137101
1830.756860	150.556573	48.142106
1826.659929	163.324004	48.147111
1822.980671	154.818060	48.152116
1820.251397	159.642778	48.157121
1816.291820	161.481678	48.162125
1813.033359	162.921393	48.167130
1809.450675	157.601232	48.172135
1806.138725	156.272511	48.177140
1802.883942	151.651042	48.182145
1799.000588	151.247428	48.187149
1795.394996	151.039120	48.192154
1791.829022	159.128145	48.197159
1788.161555	146.709284	48.202164
1784.800094	148.795002	48.207169
1781.179910	148.510981	48.212173
1778.152662	150.626359	48.217178
1774.103071	150.688212	48.222183
1770.877604	151.254805	48.227188
1767.593084	149.318118	48.232193
1763.775363	148.135430	48.237197
1760.632685	144.604642	48.242202
1757.240820	150.550377	48.247207
1753.380318	151.638430	48.252212
1750.176230	155.235139	48.257217
1746.498212	156.241642	48.262221
1742.678057	147.761308	48.267226
1738.924379	152.607884	48.272231
1735.629399	149.082628	48.277236
1732.251869	147.563362	48.282241
1728.989605	149.879549	48.287245
1725.751689	151.786178	48.292250
1722.236274	154.547098	48.297255
1718.262188	155.581393	48.302260
1715.036031	149.839913	48.307265
1711.018824	154.549835	48.312269
1707.831093	154.813824	48.317274
1704.739784	151.201156	48.322279
1701.282277	152.256788	48.327284
1697.490280	147.508780	48.332289
1693.881050	153.473628	48.337293
1690.170874	149.692821	48.342298
1686.638988	144.724299	48.347303
1683.150577	155.309672	48.352308
1679.987441	138.964013	48.357313
1675.993996	144.401746	48.362317
1673.014240	151.263536	48.367322
1669.543760	153.296579	48.372327
1665.797571	146.580676	48.377332
1662.701886	145.723178	48.382337
1659.267115	159.295035	48.387341
1655.595814	143.071333	48.392346
1652.112985	152.429164	48.397351
1648.281816	154.692915	48.402356
1644.723053	146.498504	48.407361
1641.088616	157.538903	48.412365
1637.646621	150.791144	48.417370
1634.509113	152.380656	48.422375
1631.043550	142.718813	48.427380
1627.135535	150.447308	48.432385
1623.494297	158.984859	48.437389
1620.155371	145.778405	48.442394
1616.641241	144.064619	48.447399
1613.321199	147.897724	48.452404
1609.882590	150.522275	48.457409
1606.414778	148.043445	48.462413
1603.270291	138.520011	48.467418
1599.728044	140.974875	48.472423
1595.659970	154.042995	48.477428
1592.364916	143.084447	48.482433
1588.595981	145.808579	48.487437
1585.335972	141.017670	48.492442
1581.971937	141.176408	48.497447
1577.994339	142.188137	48.502452
1574.885285	136.177146	48.507457
1570.928709	144.777280	48.512461
1567.747749	136.978914	48.517466
1564.331433	142.389533	48.522471
1560.720975	140.325713	48.527476
1557.580000	142.359073	48.532481
1553.997315	153.089034	48.537485
1550.401742	133.860111	48.542490
1546.620556	140.114073	48.547495
1543.293643	140.471325	48.552500
1539.891355	144.462969	48.557505
1536.336626	144.706843	48.562509
1532.918159	144.447813	48.567514
1528.971963	141.045125	48.572519
1525.418111	146.892395	48.577524
1522.193475	139.982017	48.582529
1518.761921	138.607068	48.587533
1515.478993	136.698746	48.592538
1511.551902	136.265961	48.597543
1508.035469	137.250226	48.602548
1505.401439	135.297853	48.607553
1501.445171	140.980791	48.612557
1497.724972	135.200661	48.617562
1493.993548	139.779923	48.622567
1490.495912	136.966136	48.627572
1487.410086	140.816346	48.632577
1483.484612	138.859301	48.637581
1480.473339	135.040355	48.642586
1476.891171	136.993413	48.647591
1472.730822	144.691663	48.652596
1469.670486	136.234805	48.657601
1465.618112	144.157089	48.662605
1462.759901	130.995010	48.667610
1459.313942	138.746482	48.672615
1456.084035	147.091630	48.677620
1452.547835	135.937197	48.682625
1448.439183	144.109776	48.687629
1445.262069	142.256388	48.692634
1441.480553	138.254209	48.697639
1437.845624	134.517610	48.702644
1434.716106	143.850557	48.707649
1431.144822	137.615804	48.712653
1427.744449	131.724293	48.717658
1424.352289	136.273202	48.722663
1420.449147	150.552003	48.727668
1416.912651	137.285971	48.732673
1413.766377	145.586495	48.737677
1410.064389	138.753017	48.742682
1406.410870	141.523294	48.747687
1403.388179	148.990311	48.752692
1399.925236	138.870839	48.757697
1396.157685	139.710567	48.762701
1392.801236	138.310248	48.767706
1389.071943	133.090982	48.772711
1385.365749	142.579992	48.777716
1382.302424	131.491260	48.782721
1378.488395	133.601260	48.787725
1374.990027	129.507394	48.792730
1371.569187	132.332252	48.797735
1368.147926	134.285358	48.802740
1364.612121	136.750407	48.807745
1360.925277	141.752189	48.812749
1357.665112	147.429133	48.817754
1354.530183	145.825159	48.822759
1350.678206	141.295441	48.827764
1347.190986	133.688374	48.832769
1343.373717	130.973915	48.837773
1339.878970	142.713618	48.842778
1336.588176	137.431539	48.847783
1332.832535	134.232672	48.852788
1329.734241	139.183233	48.857793
1326.104137	146.616470	48.862797
1322.775509	139.815871	48.867802
1319.094282	132.378752	48.872807
1315.540645	145.707316	48.877812
1312.242727	130.816044	48.882817
1308.720749	144.098118	48.887821
1305.364682	128.025783	48.892826
1301.770820	135.607734	48.897831
1297.768374	136.779165	48.902836
1294.505674	130.978606	48.907841
1290.529913	147.802940	48.912845
1287.577206	139.486054	48.917850
1284.050110	146.292870	48.922855
1280.344889	145.769046	48.927860
1277.226492	134.524767	48.932865
1273.711592	146.251290	48.937869
1269.949797	141.748333	48.942874
1266.767446	147.716136	48.947879
1262.974142	139.207585	48.952884
1259.415683	135.223250	48.957889
1256.120965	137.169865	48.962893
1252.342684	137.614077	48.967898
1248.934586	136.429850	48.972903
1245.479455	138.232982	48.977908
1242.200298	141.120879	48.982913
1238.589808	133.914236	48.987917
1235.176438	131.865584	48.992922
1231.346881	136.677639	48.997927
1228.011964	140.153382	49.002932
1224.314636	140.774027	49.007937
1220.833606	140.156630	49.012941
1217.163940	133.754690	49.017946
1214.242047	132.386628	49.022951
1210.699731	146.191733	49.027956
1207.277562	140.592740	49.032961
1203.363588	143.938226	49.037965
1200.166198	137.097223	49.042970
1196.291692	142.397672	49.047975
1192.733606	146.140364	49.052980
1189.415973	133.047241	49.057985
1185.951183	142.952211	49.062989
1182.833427	134.933542	49.067994
1179.059637	131.331922	49.072999
1175.386740	139.412535	49.078004
1172.092844	134.587356	49.083009
1167.545213	135.808324	49.088013
1164.897590	136.109828	49.093018
1161.749501	130.392001	49.098023
1158.310027	141.184939	49.103028
1154.846996	131.494341	49.108033
1151.007470	144.540322	49.113037
1147.364726	131.850070	49.118042
1143.727043	136.285825	49.123047
1140.430494	137.815871	49.128052
1136.673995	132.613807	49.133057
1133.457981	130.569009	49.138061
1129.780647	133.777029	49.143066
1126.021879	125.843262	49.148071
1122.633617	133.396971	49.153076
1119.478248	121.841668	49.158081
1116.174831	136.631559	49.163085
1112.603590	136.532628	49.168090
1109.033876	133.262484	49.173095
1105.523817	139.703128	49.178100
1101.961254	142.049712	49.183105
1098.533046	139.616474	49.188109
1094.938626	129.684493	49.193114
1091.288900	123.293979	49.198119
1087.379981	128.799544	49.203124
1084.280817	126.582465	49.208129
1080.858441	136.002138	49.213133
1077.284995	136.624072	49.218138
1073.825399	134.175148	49.223143
1070.374565	138.803150	49.228148
1067.386850	125.835379	49.233153
1063.452482	138.074086	49.238157
1059.627538	132.661457	49.243162
1055.992389	128.430352	49.248167
1052.060993	138.800416	49.253172
1048.977052	123.213037	49.258177
1045.818796	137.467795	49.263181
1042.440563	128.774379	49.268186
1039.298093	139.132729	49.273191
1035.498558	134.258182	49.278196
1032.288028	135.286827	49.283201
1028.296966	144.465052	49.288205
1024.569031	132.688912	49.293210
1021.214345	145.008869	49.298215
1017.456091	136.339464	49.303220
1014.443532	134.979497	49.308225
1010.955880	139.228857	49.313229
1007.451267	135.702522	49.318234
1003.913490	131.280668	49.323239
1000.061955	135.499650	49.328244
997.019792	125.949332	49.333249
992.867016	135.085159	49.338253
989.504295	128.200549	49.343258
986.220415	131.433388	49.348263
982.798874	143.182727	49.353268
979.479330	139.600840	49.358273
975.489080	130.562293	49.363277
972.483662	136.816684	49.368282
968.817315	128.927733	49.373287
965.788599	126.725504	49.378292
961.723652	125.166880	49.383297
957.837554	132.074390	49.388301
954.775500	133.851216	49.393306
951.355203	124.563201	49.398311
947.647539	132.885985	49.403316
944.393805	123.263678	49.408321
940.929163	132.488205	49.413325
937.147174	141.981491	49.418330
933.760056	129.514065	49.423335
929.947258	136.620190	49.428340
926.622170	128.816724	49.433345
923.243576	130.881136	49.438349
919.618925	125.281888	49.443354
916.286736	134.798213	49.448359
912.755667	137.601106	49.453364
909.467687	132.194232	49.458369
905.734364	134.004564	49.463373
901.995061	137.128556	49.468378
898.524103	133.262653	49.473383
894.832078	132.259266	49.478388
891.940339	132.764867	49.483393
888.063991	126.593127	49.488397
884.395515	130.860570	49.493402
881.331214	136.214500	49.498407
877.531423	137.053366	49.503412
874.456900	131.747847	49.508417
870.715738	132.917784	49.513421
866.917779	128.762237	49.518426
863.569263	134.348652	49.523431
860.010311	125.945892	49.528436
856.743160	121.618186	49.533441
853.001349	125.148554	49.538445
849.504226	128.848865	49.543450
846.099252	132.680305	49.548455
842.228737	137.342840	49.553460
838.820869	135.662844	49.558465
835.533342	130.224786	49.563469
832.023093	134.439964	49.568474
828.686727	129.206367	49.573479
825.145563	144.518216	49.578484
822.071285	122.581624	49.583489
818.669423	133.258662	49.588493
814.742676	130.318415	49.593498
811.524691	127.241180	49.598503
807.345754	129.689359	49.603508
804.252557	124.697014	49.608513
800.436787	131.259701	49.613517
796.696069	126.128186	49.618522
793.562921	120.657043	49.623527
789.990397	131.928583	49.628532
786.454635	122.909725	49.633537
783.077258	129.466350	49.638541
779.600961	131.967622	49.643546
776.272199	128.442705	49.648551
772.328942	129.176436	49.653556
769.459906	120.970631	49.658561
765.774842	127.982487	49.663565
762.168947	139.657419	49.668570
758.456862	123.990491	49.673575
754.821525	120.019212	49.678580
751.493975	117.781127	49.683585
747.864297	130.803654	49.688589
744.521208	121.509147	49.693594
741.198603	117.369931	49.698599
737.176186	128.721136	49.703604
734.056982	116.895376	49.708609
730.558562	120.549039	49.713613
726.898166	123.670159	49.718618
723.533835	127.281243	49.723623
720.061669	123.073340	49.728628
717.056358	115.581268	49.733633
713.322246	122.078379	49.738637
709.382370	123.214370	49.743642
705.780955	117.032903	49.748647
702.309662	120.218355	49.753652
698.986280	116.071414	49.758657
695.355901	118.657936	49.763661
692.052722	121.787859	49.768666
688.809814	118.367367	49.773671
684.915181	122.995180	49.778676
681.576678	119.169656	49.783681
678.010470	113.114981	49.788685
674.406849	120.080636	49.793690
671.297955	117.432570	49.798695
667.154187	125.558450	49.803700
663.640822	117.974956	49.808705
660.245365	125.863128	49.813709
656.853301	118.770001	49.818714
653.549546	123.078524	49.823719
649.904102	129.724563	49.828724
646.710322	119.757319	49.833729
643.035240	119.742175	49.838733
639.292624	123.892504	49.843738
635.745204	114.894489	49.848743
631.909007	121.597670	49.853748
628.947383	117.717114	49.858753
625.466238	125.810560	49.863757
622.159189	122.227323	49.868762
618.604007	114.460788	49.873767
614.987026	118.045244	49.878772
611.659811	117.749380	49.883777
607.956907	121.421913	49.888781
603.851251	119.451105	49.893786
600.880918	127.729899	49.898791
597.127786	126.429704	49.903796
594.206367	125.362979	49.908801
590.459065	130.034500	49.913805
586.881230	127.924951	49.918810
583.521699	123.078455	49.923815
579.596719	122.771774	49.928820
576.461062	113.888173	49.933825
572.944725	109.266445	49.938829
569.302288	121.132295	49.943834
565.982830	117.945244	49.948839
562.035840	128.993613	49.953844
558.738513	128.059592	49.958849
555.374801	129.575041	49.963853
551.927278	129.342228	49.968858
548.377558	116.126496	49.973863
544.785512	122.287989	49.978868
541.572499	125.334787	49.983873
537.879676	125.615732	49.988877
534.399477	127.191194	49.993882
530.960032	121.761680	49.998887
527.210479	126.149278	50.003892
523.773466	121.417137	50.008897
520.549501	119.539160	50.013901
516.762198	124.750587	50.018906
513.400337	131.747672	50.023911
509.848836	129.962975	50.028916
506.419649	118.383879	50.033921
502.750340	117.816960	50.038925
499.107715	123.233083	50.043930
496.077172	112.685951	50.048935
492.085491	118.254179	50.053940
488.753132	115.397901	50.058945
484.844911	119.869907	50.063949
481.487108	124.541762	50.068954
477.992842	123.686895	50.073959
474.980561	117.426562	50.078964
471.469527	111.103835	50.083969
467.916108	124.585151	50.088973
463.905728	122.797388	50.093978
460.656202	119.223098	50.098983
457.398230	127.737430	50.103988
454.014911	117.268463	50.108993
450.404485	121.259474	50.113997
446.809533	126.101581	50.119002
443.299417	120.702045	50.124007
439.899655	122.917010	50.129012
436.374393	120.021189	50.134017
432.851790	117.050339	50.139021
428.821770	130.564877	50.144026
426.036332	123.132045	50.149031
422.023763	125.336927	50.154036
418.796110	118.641383	50.159041
415.267448	124.435687	50.164045
411.715074	129.441052	50.169050
408.166112	114.497504	50.174055
404.555273	127.936908	50.179060
400.998759	116.495104	50.184065
397.765207	118.696310	50.189069
394.246773	121.974522	50.194074
390.911301	116.298576	50.199079
387.180909	132.448091	50.204084
383.692656	116.258787	50.209089
380.093476	112.969388	50.214093
376.718099	114.067995	50.219098
373.248883	109.856982	50.224103
369.370426	117.062538	50.229108
365.843527	119.960739	50.234113
362.345541	120.138253	50.239117
359.037386	122.353267	50.244122
355.829098	114.683889	50.249127
352.498252	117.537890	50.254132
348.799943	105.383262	50.259137
345.192528	110.719674	50.264141
341.464786	119.875319	50.269146
338.030445	117.839068	50.274151
334.576608	118.719473	50.279156
331.206513	117.813334	50.284161
327.531671	106.488165	50.289165
323.982394	130.194473	50.294170
320.970910	114.018585	50.299175
317.539202	121.417952	50.304180
314.261759	108.974403	50.309185
310.186332	119.328023	50.314189
306.200559	109.998254	50.319194
302.994345	108.687814	50.324199
299.426444	121.218950	50.329204
295.875445	106.331719	50.334209
292.421604	104.988428	50.339213
288.948172	115.353348	50.344218
285.951741	108.827508	50.349223
281.823637	119.540370	50.354228
278.999789	113.454327	50.359233
274.984475	109.509963	50.364237
271.074024	123.925333	50.369242
267.993459	110.329653	50.374247
264.141836	121.437636	50.379252
261.206228	118.118618	50.384257
257.929557	123.100216	50.389261
254.227330	126.545647	50.394266
250.678964	119.012790	50.399271
247.144251	120.019390	50.404276
243.310718	114.507640	50.409281
239.927904	116.562693	50.414285
236.348308	115.215485	50.419290
232.886261	118.852105	50.424295
229.802810	129.549713	50.429300
226.500491	124.404762	50.434305
222.344682	125.050853	50.439309
218.976150	131.846236	50.444314
215.788388	116.574514	50.449319
211.618041	130.208870	50.454324
208.211047	118.997579	50.459329
204.737801	118.558613	50.464333
201.500371	125.535475	50.469338
198.275444	111.262335	50.474343
194.457967	115.869919	50.479348
191.299486	118.814213	50.484353
187.631883	108.286797	50.489357
184.177168	119.421448	50.494362
180.773548	109.690215	50.499367
176.942350	125.128888	50.504372
173.086024	123.768328	50.509377
169.681311	121.304430	50.514381
166.382701	118.703321	50.519386
163.228274	112.456822	50.524391
159.493123	121.418901	50.529396
155.727335	111.856803	50.534401
152.282575	114.964140	50.539405
149.006551	119.578486	50.544410
145.415272	115.967741	50.549415
141.866001	116.284620	50.554420
138.404454	111.361379	50.559425
135.150305	116.807210	50.564429
131.650923	117.307614	50.569434
128.277977	109.210969	50.574439
124.300406	119.320594	50.579444
120.669174	107.986632	50.584449
117.302540	124.543984	50.589453
114.032444	123.754428	50.594458
110.822699	107.061346	50.599463
106.952418	119.529623	50.604468
103.236537	112.993465	50.609473
99.999670	110.854965	50.614477
96.253850	114.433492	50.619482
92.852763	104.976027	50.624487
89.057058	110.863540	50.629492
85.887338	110.631564	50.634497
82.372974	117.154110	50.639501
78.925290	117.677349	50.644506
75.393347	111.743495	50.649511
71.970198	114.296955	50.654516
68.453690	115.876710	50.659521
64.707844	113.200647	50.664525
61.109121	121.656285	50.669530
58.104247	109.883222	50.674535
54.292415	113.903734	50.679540
50.427926	114.436876	50.684545
47.345422	125.029870	50.689549
43.926126	120.047800	50.694554
40.723331	111.139161	50.699559
36.802484	114.137674	50.704564
33.471689	112.137587	50.709569
29.995155	114.110726	50.714573
26.230476	118.256036	50.719578
22.962072	104.788714	50.724583
19.403189	113.650384	50.729588
15.877204	110.476468	50.734593
12.250022	107.078435	50.739597
8.681384	121.477284	50.744602
5.087657	110.430845	50.749607
1.879881	113.380332	50.754612