Fri Jun 17 17:32:54 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.260185	86.331454	0.000000
0.201589	94.508861	0.005005
0.766110	100.479546	0.010010
0.880946	116.732738	0.015014
0.612747	110.952807	0.020019
0.373231	99.402088	0.025024
0.491485	86.201818	0.030029
0.572443	81.280863	0.035034
0.205698	71.820723	0.040038
-0.172749	60.610236	0.045043
-0.430214	55.496112	0.050048
-1.306886	46.674848	0.055053
-0.926369	34.710918	0.060058
-1.522931	32.349094	0.065062
-1.621074	26.665446	0.070067
-1.680629	26.395460	0.075072
-2.107964	19.315757	0.080077
-2.713518	8.546794	0.085082
-2.807445	4.782279	0.090086
-2.855817	-3.489130	0.095091
-3.130934	1.861549	0.100096
-3.779673	-9.265679	0.105101
-3.976910	-10.765825	0.110106
-4.091778	-7.394166	0.115110
-4.232407	-6.511292	0.120115
-4.566645	-16.661121	0.125120
-5.441425	-5.000405	0.130125
-5.276929	-5.548767	0.135130
-5.305775	-2.840227	0.140134
-5.851211	-4.392806	0.145139
-6.389376	-9.612787	0.150144
-7.206326	3.229209	0.155149
-6.274773	-3.670241	0.160154
-6.950615	-12.678569	0.165158
-7.268440	-8.723219	0.170163
-6.855879	-6.657737	0.175168
-7.012314	-6.415927	0.180173
-7.668140	-14.127966	0.185178
-8.463629	-8.241871	0.190182
-8.466731	-3.658634	0.195187
-8.755347	0.439467	0.200192
-9.341774	-0.309282	0.205197
-8.655416	-8.118910	0.210202
-9.194597	-4.121043	0.215206
-9.301484	-5.809659	0.220211
-10.103943	-9.473374	0.225216
-10.289465	-3.481071	0.230221
-10.416658	0.047345	0.235226
-10.399480	-12.042635	0.240230
-10.609920	-3.108145	0.245235
-10.656968	-8.909987	0.250240
-11.716274	-5.694710	0.255245
-11.887523	-20.686278	0.260250
-12.080564	-17.032668	0.265254
-11.969862	-6.347371	0.270259
-12.002193	-13.367013	0.275264
-12.130284	-3.685899	0.280269
-12.768533	-17.239850	0.285274
-13.307004	-13.658075	0.290278
-14.056935	-12.246510	0.295283
-13.741145	-7.302674	0.300288
-13.825733	-4.768781	0.305293
-13.908939	-9.757138	0.310298
-13.765607	-10.827275	0.315302
-14.344754	2.011898	0.320307
-14.781815	-13.596354	0.325312
-15.198070	-4.197871	0.330317
-15.066178	-8.696097	0.335322
-15.354397	-8.055876	0.340326
-15.977538	-10.628559	0.345331
-16.570797	-8.972101	0.350336
-16.622655	-5.566121	0.355341
-17.031404	-7.853384	0.360346
-16.700021	-12.810210	0.365350
-16.940236	1.967830	0.370355
-16.697410	-13.804734	0.375360
-17.567680	-7.286198	0.380365
-17.688681	-4.508864	0.385370
-18.021218	-12.722378	0.390374
-18.178870	-8.385374	0.395379
-18.090417	-13.817839	0.400384
-18.656661	-10.924074	0.405389
-19.094574	-16.282466	0.410394
-19.633865	-4.402632	0.415398
-19.747401	-9.739366	0.420403
-19.456618	-3.968310	0.425408
-19.852305	-3.040673	0.430413
-20.513853	-11.267974	0.435418
-21.306205	-1.102705	0.440422
-21.438457	-2.990355	0.445427
-21.105708	-6.198080	0.450432
-21.386769	-2.335268	0.455437
-21.156306	-9.924279	0.460442
-21.279004	-6.807453	0.465446
-22.244040	-3.891405	0.470451
-22.215514	-21.679783	0.475456
-23.032183	-2.760868	0.480461
-23.035057	-15.766871	0.485466
-23.057776	-20.422121	0.490470
-23.062196	-11.605548	0.495475
-23.098830	-16.253357	0.500480
-23.620912	-9.351663	0.505485
-24.208386	-13.224954	0.510490
-24.418704	-13.072457	0.515494
-24.614264	-7.813739	0.520499
-24.685126	-15.530456	0.525504
-25.448085	-12.505130	0.530509
-25.685089	-14.389772	0.535514
-25.955817	-4.456837	0.540518
-25.867300	-3.285667	0.545523
-25.874861	-9.189579	0.550528
-25.838381	-4.859387	0.555533
-26.244062	-8.567934	0.560538
-27.258563	-18.163061	0.565542
-27.751039	-8.515707	0.570547
-27.612463	-3.676600	0.575552
-27.712392	-6.309215	0.580557
-27.673325	-12.606262	0.585562
-28.018450	-3.313135	0.590566
-28.018275	-8.802954	0.595571
-28.120516	-12.722761	0.600576
-29.032934	-8.359558	0.605581
-29.090145	-17.275151	0.610586
-29.589209	-24.144590	0.615590
-30.193735	-14.922804	0.620595
-29.518038	-21.397890	0.625600
-29.682662	-10.632301	0.630605
-30.609798	-10.461294	0.635610
-30.713345	-11.441457	0.640614
-30.881171	-9.554389	0.645619
-30.387658	-11.757589	0.650624
-31.213673	-2.248963	0.655629
-31.804088	-17.274456	0.660634
-32.063258	-9.191439	0.665638
-32.559459	-6.653063	0.670643
-32.450499	-12.510433	0.675648
-32.673901	-6.886368	0.680653
-32.474173	-9.124601	0.685658
-32.797317	-10.449899	0.690662
-33.513481	-6.099781	0.695667
-33.808873	-8.275646	0.700672
-34.191268	-7.000153	0.705677
-34.246700	-6.154528	0.710682
-34.177058	-8.004697	0.715686
-34.464139	1.817298	0.720691
-34.761180	-0.412560	0.725696
-35.628402	3.864203	0.730701
-35.641045	-9.667247	0.735706
-35.853302	-4.956895	0.740710
-36.127375	-6.217733	0.745715
-36.355321	-6.475514	0.750720
-36.388902	-8.719760	0.755725
-36.099712	-13.671744	0.760730
-36.416809	-17.760269	0.765734
-37.065960	-6.989915	0.770739
-36.932888	-6.914426	0.775744
-37.358661	9.642214	0.780749
-38.075019	1.540643	0.785754
-38.773417	-7.581735	0.790758
-39.160481	-2.408397	0.795763
-38.653092	-8.109014	0.800768
-39.090985	-1.921041	0.805773
-38.840111	-5.983805	0.810778
-39.048473	-6.850249	0.815782
-39.496336	0.394900	0.820787
-39.407651	-11.791617	0.825792
-40.276890	-2.187796	0.830797
-40.480620	-9.750218	0.835802
-40.706746	-8.604891	0.840806
-40.884813	-4.598375	0.845811
-40.876861	-11.333847	0.850816
-41.859674	-5.580590	0.855821
-42.179161	-13.057860	0.860826
-41.935069	-9.086787	0.865830
-42.536549	-5.371991	0.870835
-42.163787	-7.959056	0.875840
-42.442801	-12.894735	0.880845
-42.469323	-8.268734	0.885850
-42.641076	-19.892778	0.890854
-42.947140	-7.151692	0.895859
-43.302347	-12.551849	0.900864
-43.771770	2.470892	0.905869
-44.470307	-12.473878	0.910874
-44.833584	-9.473743	0.915878
-45.287725	-3.549860	0.920883
-44.907856	-15.955662	0.925888
-45.274865	-10.813088	0.930893
-45.354585	0.654701	0.935898
-45.085431	-9.725067	0.940902
-45.474826	-4.510100	0.945907
-46.276016	-11.430551	0.950912
-46.442445	-4.292371	0.955917
-46.848209	-10.351692	0.960922
-46.887430	-10.114958	0.965926
-47.115628	0.249771	0.970931
-46.903892	-16.057515	0.975936
-47.861585	0.861821	0.980941
-48.152345	-2.226280	0.985946
-48.265698	-7.810494	0.990950
-48.456644	-4.074350	0.995955
-48.194897	-6.751888	1.000960
-48.617183	2.009831	1.005965
-49.598493	1.401910	1.010970
-49.758136	-9.081218	1.015974
-50.041825	-2.122652	1.020979
-49.999515	-1.525530	1.025984
-50.118392	0.942433	1.030989
-50.476657	1.156030	1.035994
-50.214631	-9.292210	1.040998
-50.696401	-1.397144	1.046003
-51.440473	-7.332744	1.051008
-51.669924	3.342595	1.056013
-51.618850	-2.954871	1.061018
-51.687794	3.046076	1.066022
-51.835545	-2.781649	1.071027
-52.331399	-14.091150	1.076032
-52.977044	-11.094199	1.081037
-53.158235	-3.610803	1.086042
-53.417318	-6.787047	1.091046
-53.703522	-9.738168	1.096051
-53.475095	-0.897349	1.101056
-53.527252	-0.854611	1.106061
-53.923624	-6.431443	1.111066
-54.400092	-8.788547	1.116070
-54.820244	-19.521399	1.121075
-54.882243	-11.270277	1.126080
-54.792279	-2.734405	1.131085
-55.401978	-15.234218	1.136090
-55.842325	-7.497589	1.141094
-56.293360	3.982789	1.146099
-56.307992	-4.295407	1.151104
-56.461163	-7.970938	1.156109
-56.380406	-2.091174	1.161114
-56.401482	-5.394793	1.166118
-57.242172	-4.750348	1.171123
-57.422148	-8.680320	1.176128
-57.877942	-6.266661	1.181133
-58.185331	-11.911166	1.186138
-58.124344	-9.283073	1.191142
-58.411437	-2.575537	1.196147
-58.544311	-6.987523	1.201152
-59.842750	8.431136	1.206157
-59.706095	-4.611877	1.211162
-59.396403	3.693300	1.216166
-59.900994	-11.903912	1.221171
-60.134331	-6.179727	1.226176
-60.018196	-7.928304	1.231181
-59.910225	-3.373201	1.236186
-60.095810	2.157756	1.241190
-60.666326	-0.076367	1.246195
-60.878945	-5.945402	1.251200
-61.144906	3.234917	1.256205
-61.869381	0.563253	1.261210
-62.518316	-8.641340	1.266214
-63.190991	4.716772	1.271219
-62.328849	-7.634427	1.276224
-62.853517	-2.377437	1.281229
-63.195578	-7.836412	1.286234
-63.174061	-10.220645	1.291238
-63.589239	-0.360192	1.296243
-63.343258	-4.726228	1.301248
-63.269820	-1.810721	1.306253
-64.244270	-3.103724	1.311258
-64.503190	-0.433503	1.316262
-64.754286	-6.423618	1.321267
-64.580368	-5.690509	1.326272
-65.031343	-7.677120	1.331277
-65.601016	-7.969458	1.336282
-65.746360	-7.207748	1.341286
-66.153105	-6.921761	1.346291
-65.817898	-4.089037	1.351296
-66.421699	-6.306575	1.356301
-66.721261	-6.545740	1.361306
-67.339593	-8.771912	1.366310
-67.702920	-7.217997	1.371315
-67.985676	-11.525937	1.376320
-67.708863	0.917184	1.381325
-67.815961	-4.545132	1.386330
-67.730060	-2.635909	1.391334
-68.269598	-7.707455	1.396339
-68.421285	-12.656995	1.401344
-68.853897	-1.263944	1.406349
-69.093756	3.186972	1.411354
-69.584358	0.918847	1.416358
-69.792838	-0.668620	1.421363
-69.576295	-4.185783	1.426368
-70.339268	0.446413	1.431373
-71.050238	1.317341	1.436378
-70.736761	-2.528506	1.441382
-71.137920	6.233454	1.446387
-70.926441	-3.342279	1.451392
-71.173728	-2.319329	1.456397
-72.018297	-2.069685	1.461402
-72.550540	-2.211564	1.466406
-72.604375	0.385100	1.471411
-72.065122	-4.260563	1.476416
-72.424848	-5.913265	1.481421
-72.954126	-1.284989	1.486426
-72.928217	-6.176438	1.491430
-73.336627	1.128457	1.496435
-73.846038	1.198859	1.501440
-74.218111	-1.532566	1.506445
-74.429869	-2.294846	1.511450
-74.422931	-4.622983	1.516454
-74.814158	-1.637142	1.521459
-74.556537	-0.997669	1.526464
-75.323475	-0.221824	1.531469
-75.582922	3.273127	1.536474
-75.549377	0.858674	1.541478
-76.146146	2.086928	1.546483
-75.908796	0.554010	1.551488
-76.488135	0.914469	1.556493
-77.167271	4.673162	1.561498
-77.428254	-4.825019	1.566502
-77.601967	-3.206128	1.571507
-77.687577	-5.460076	1.576512
-77.736027	2.388220	1.581517
-77.959347	0.634109	1.586522
-77.864866	-0.568804	1.591526
-78.261923	4.876739	1.596531
-78.493630	-1.725953	1.601536
-78.991262	-3.836425	1.606541
-79.386169	-1.962517	1.611546
-79.470255	-9.398206	1.616550
-79.404623	-7.116214	1.621555
-79.570932	-13.518629	1.626560
-80.670396	-4.348941	1.631565
-80.989421	-3.154030	1.636570
-80.774064	-5.853063	1.641574
-81.218970	-11.859499	1.646579
-80.828904	-13.977627	1.651584
-80.846173	-6.444326	1.656589
-81.957612	-6.892870	1.661594
-81.784801	-11.851360	1.666598
-82.458259	-9.322386	1.671603
-82.483862	-7.996485	1.676608
-82.527668	-7.182786	1.681613
-82.830156	-5.179599	1.686618
-83.401168	-6.225117	1.691622
-83.963040	-2.281879	1.696627
-84.055576	-6.487255	1.701632
-84.045397	-7.020426	1.706637
-84.357137	-2.806988	1.711642
-84.408104	-7.105112	1.716646
-84.432329	-8.186863	1.721651
-84.684567	-9.846972	1.726656
-85.358248	-8.876472	1.731661
-85.800654	-1.413588	1.736666
-85.871042	-11.401251	1.741670
-86.040933	-3.429173	1.746675
-86.086895	-9.883562	1.751680
-86.240181	-8.872686	1.756685
-87.102038	-6.257140	1.761690
-87.281580	-12.072470	1.766694
-87.636359	-3.292573	1.771699
-87.471203	-7.834806	1.776704
-87.711972	-11.862411	1.781709
-87.861389	-2.346078	1.786714
-87.790428	1.433750	1.791718
-88.601709	1.491979	1.796723
-89.106142	-0.163108	1.801728
-89.078985	-10.779104	1.806733
-89.347459	-2.194307	1.811738
-89.266427	-15.589964	1.816742
-89.380267	-13.050223	1.821747
-90.113502	-7.371005	1.826752
-90.341053	-12.904065	1.831757
-90.607394	-1.802878	1.836762
-90.772660	-4.660635	1.841766
-91.205627	-14.990180	1.846771
-90.984042	-20.122730	1.851776
-91.419838	-10.841372	1.856781
-91.882967	-6.431881	1.861786
-92.377191	-12.368548	1.866790
-92.387168	-9.177913	1.871795
-92.561549	-5.564696	1.876800
-92.626851	-10.485577	1.881805
-92.715607	-8.599022	1.886810
-93.015716	-15.918877	1.891814
-93.842941	-13.690329	1.896819
-93.967983	-11.091697	1.901824
-93.998938	-12.507198	1.906829
-94.243992	-7.473101	1.911834
-93.943393	-8.791577	1.916838
-94.851723	-5.611637	1.921843
-94.776488	-5.120431	1.926848
-94.879327	-8.390131	1.931853
-95.243554	1.321750	1.936858
-96.048054	-4.688448	1.941862
-96.338105	1.171459	1.946867
-96.669595	-3.919079	1.951872
-96.671263	-12.998607	1.956877
-97.113286	-2.559068	1.961882
-96.688562	-10.001787	1.966886
-97.378396	-9.063723	1.971891
-96.929018	-10.447582	1.976896
-97.608604	-7.798400	1.981901
-98.137799	-14.349263	1.986906
-98.292624	-14.821458	1.991910
-98.683461	-0.532433	1.996915
-98.905149	-8.763048	2.006912
-99.038716	-4.789335	2.016909
-97.962381	-7.372389	2.026906
-97.225844	-4.258173	2.036902
-97.429076	-6.600459	2.046899
-96.452051	-4.766644	2.056896
-95.726835	-3.027498	2.066893
-95.627765	-4.745490	2.076890
-95.177919	-9.278662	2.086886
-94.708746	-6.977311	2.096883
-93.697534	-9.611776	2.106880
-92.987934	-12.002273	2.116877
-93.315272	-6.586006	2.126874
-92.887682	-3.599441	2.136870
-91.988800	-4.787304	2.146867
-91.466230	-14.974333	2.156864
-91.105870	-14.956334	2.166861
-90.252188	-11.253038	2.176858
-89.945925	-15.247835	2.186854
-89.742752	-6.563623	2.196851
-88.950486	-7.603159	2.206848
-88.541556	-9.890327	2.216845
-87.823271	-12.621318	2.226842
-87.339909	-13.566826	2.236838
-86.792745	-6.656590	2.246835
-86.964912	-4.944313	2.256832
-85.832684	-10.587921	2.266829
-85.472889	-8.098070	2.276826
-85.137818	-9.380898	2.286822
-84.285360	-12.407844	2.296819
-84.030642	-7.012463	2.306816
-83.672677	-7.498493	2.316813
-82.800112	-6.135535	2.326810
-82.308407	-6.595389	2.336806
-81.922176	-10.265812	2.346803
-81.626431	-5.014372	2.356800
-80.806632	-8.716759	2.366797
-80.844306	-9.409288	2.376794
-79.816680	-7.700652	2.386790
-79.344696	-5.756006	2.396787
-79.235291	-2.660038	2.406784
-78.177269	-4.475398	2.416781
-77.942076	3.665482	2.426778
-77.710893	0.301398	2.436774
-76.465172	-8.425975	2.446771
-76.272002	-6.616560	2.456768
-76.279463	-2.581813	2.466765
-75.719012	-4.561439	2.476762
-74.356584	-9.163720	2.486758
-74.261040	-6.479580	2.496755
-74.261770	-8.806924	2.506752
-73.919347	-7.129804	2.516749
-73.070773	-6.102896	2.526746
-72.064008	-0.525481	2.536742
-71.712468	-9.139382	2.546739
-71.504488	-5.146178	2.556736
-71.379001	-5.311414	2.566733
-70.435878	-3.348466	2.576730
-70.224822	-0.816895	2.586726
-69.106055	-4.756089	2.596723
-68.653282	-6.586224	2.606720
-68.554966	-4.899942	2.616717
-68.148695	-1.164942	2.626714
-67.419977	-6.146155	2.636710
-67.105971	-11.261545	2.646707
-66.469440	-11.144622	2.656704
-65.423677	-8.651235	2.666701
-65.274298	-5.047998	2.676698
-65.318761	-6.009693	2.686694
-64.597809	-10.395680	2.696691
-63.935015	-6.898929	2.706688
-63.423800	-1.031676	2.716685
-62.496574	-8.482276	2.726682
-62.165635	-10.788287	2.736678
-62.005058	-9.442910	2.746675
-61.869241	-6.385711	2.756672
-60.726369	-10.319029	2.766669
-60.829690	-13.856108	2.776666
-59.480070	-5.584149	2.786662
-59.002192	-6.091295	2.796659
-59.073837	-14.145041	2.806656
-58.754478	-13.280892	2.816653
-57.695424	-10.711667	2.826650
-57.621873	-12.095059	2.836646
-56.920952	-13.895114	2.846643
-55.751810	-11.863237	2.856640
-55.820016	-14.899157	2.866637
-55.735884	-8.334575	2.876634
-55.353789	-8.204402	2.886630
-54.398130	-10.714234	2.896627
-53.879582	-14.633868	2.906624
-52.947141	-2.732518	2.916621
-52.893901	-12.342044	2.926618
-52.452067	-3.926100	2.936614
-52.144554	-14.189014	2.946611
-51.154563	-11.142408	2.956608
-51.062466	-9.608415	2.966605
-50.253618	-1.289435	2.976602
-49.302768	-8.937986	2.986598
-49.281869	-15.903025	2.996595
-49.237942	-11.079971	3.006592
-48.600008	-6.912441	3.016589
-48.109853	-5.832469	3.026586
-47.308583	-2.635742	3.036582
-46.327572	-3.522695	3.046579
-45.923387	-2.939579	3.056576
-46.045736	-1.639837	3.066573
-46.051903	-5.321300	3.076570
-45.302794	-7.164533	3.086566
-44.212420	-5.881634	3.096563
-43.391750	-4.234215	3.106560
-43.355750	-7.541154	3.116557
-43.453782	-6.639237	3.126554
-42.197962	-7.905585	3.136550
-42.078546	-1.078152	3.146547
-41.288189	-1.125102	3.156544
-40.697292	-6.535274	3.166541
-40.520878	-2.935739	3.176538
-40.058408	-0.798048	3.186534
-38.929676	1.567948	3.196531
-38.958174	0.386061	3.206528
-38.581470	-0.850140	3.216525
-37.586964	-4.523866	3.226522
-37.167955	-10.063728	3.236518
-36.987328	-7.085698	3.246515
-36.637922	-12.037642	3.256512
-35.610237	-2.017690	3.266509
-35.599751	-3.435253	3.276506
-34.811549	-2.410155	3.286502
-33.951203	-4.214380	3.296499
-33.837773	-5.253692	3.306496
-33.360092	-7.589428	3.316493
-32.506551	-1.949583	3.326490
-32.092770	-4.984811	3.336486
-31.940768	-6.911555	3.346483
-31.785140	-6.335727	3.356480
-30.872733	-10.257798	3.366477
-30.677296	-8.926709	3.376474
-29.324460	-8.999183	3.386470
-28.823092	-10.115029	3.396467
-28.792755	-10.912716	3.406464
-28.770020	-9.785475	3.416461
-28.061425	-11.201317	3.426458
-27.283897	-5.140632	3.436454
-26.772499	-11.212134	3.446451
-25.873200	-8.982662	3.456448
-25.869371	-9.266773	3.466445
-25.643960	-7.615444	3.476442
-24.452684	-5.857133	3.486438
-24.155783	-1.246439	3.496435
-24.118497	-9.373819	3.506432
-23.665237	-3.446936	3.516429
-22.715407	-9.004295	3.526426
-22.388699	-8.299628	3.536422
-21.462197	-9.839020	3.546419
-20.958522	-8.019764	3.556416
-20.748409	-3.006000	3.566413
-20.710153	-5.887129	3.576410
-20.131192	-3.017985	3.586406
-19.445118	-3.832000	3.596403
-18.402599	-4.935247	3.606400
-18.068686	-1.384215	3.616397
-17.998870	0.678065	3.626394
-17.501962	0.616077	3.636390
-16.527651	-5.528615	3.646387
-16.290804	-7.116183	3.656384
-16.021851	-7.463329	3.666381
-15.301308	-7.394741	3.676378
-14.869470	-5.748679	3.686374
-14.369640	-5.427842	3.696371
-13.449139	-4.203437	3.706368
-13.282258	5.248507	3.716365
-13.145239	-3.369850	3.726362
-11.942851	-1.686091	3.736358
-11.473087	-6.324917	3.746355
-11.647780	-0.262636	3.756352
-11.107337	-4.539976	3.766349
-10.477565	-0.259445	3.776346
-9.379155	-5.695682	3.786342
-9.088137	-0.763924	3.796339
-8.585577	-7.113339	3.806336
-8.431026	-2.635271	3.816333
-7.847615	-6.445356	3.826330
-6.902224	-10.259887	3.836326
-7.019712	-9.971195	3.846323
-6.497062	-6.774976	3.856320
-5.308653	-6.545273	3.866317
-5.234545	-6.180151	3.876314
-5.199081	-0.669282	3.886310
-4.599628	8.329629	3.896307
-3.949007	12.718334	3.906304
-3.375567	21.161231	3.916301
-3.161788	27.689070	3.926298
-2.401010	39.473979	3.936294
-2.135348	49.262416	3.946291
-1.524107	60.245507	3.956288
-1.616401	77.041485	3.966285
-0.919238	99.835319	3.976282
-0.307636	121.151055	3.986278
0.000000	131.570118	3.991283
-0.090496	142.726248	3.996288
0.187905	136.965766	4.001293
0.594264	158.674725	4.006298
0.710590	173.945804	4.011302
0.980885	170.248977	4.016307
0.685478	168.963054	4.021312
0.916774	172.293595	4.026317
0.749820	174.090358	4.031322
0.748695	174.081595	4.036326
0.789077	164.523143	4.041331
0.634221	189.831822	4.046336
1.111828	191.106268	4.051341
1.218783	199.816244	4.056346
1.211560	196.589605	4.061350
1.214907	198.110018	4.066355
0.863495	204.385125	4.071360
1.452547	202.892993	4.076365
1.024929	201.661405	4.081370
0.918268	199.620489	4.086374
1.443571	195.702882	4.091379
1.264995	212.871430	4.096384
1.074925	208.489801	4.101389
1.427376	203.923282	4.106394
1.364683	195.948764	4.111398
1.060723	187.818400	4.116403
0.868139	189.481885	4.121408
1.102840	194.999492	4.126413
1.526160	210.175577	4.131418
1.304167	209.444977	4.136422
1.408610	205.033145	4.141427
1.362174	207.881398	4.146432
1.279899	202.429479	4.151437
1.176279	205.681507	4.156442
1.128255	208.699730	4.161446
1.193551	204.192581	4.166451
1.116850	211.056455	4.171456
1.054196	211.327673	4.176461
1.270653	203.286231	4.181466
1.421702	211.941920	4.186470
1.258817	200.545332	4.191475
1.372795	212.029237	4.196480
1.230937	201.673043	4.201485
1.171576	209.091499	4.206490
0.963248	217.362135	4.211494
1.531586	211.801285	4.216499
1.629579	236.006166	4.221504
1.528394	211.614999	4.226509
1.516898	216.460374	4.231514
1.430723	214.680674	4.236518
1.604607	211.734927	4.241523
1.145813	220.688526	4.246528
1.803782	223.693601	4.251533
2.007809	240.235201	4.256538
1.825519	223.105742	4.261542
1.802903	210.304700	4.266547
1.361574	224.096366	4.271552
1.529440	210.147154	4.276557
1.515358	214.759316	4.281562
1.357162	223.407803	4.286566
1.773554	228.641257	4.291571
1.827956	240.639665	4.296576
2.043254	237.869366	4.301581
1.764047	220.018979	4.306586
1.597167	219.147401	4.311590
1.570638	214.511063	4.316595
1.425754	223.431039	4.321600
1.661889	229.012751	4.326605
1.956645	236.805508	4.331610
1.804318	239.435356	4.336614
2.014962	237.326896	4.341619
1.854578	220.863745	4.346624
1.986706	216.665953	4.351629
1.261311	221.045486	4.356634
1.860269	227.543296	4.361638
1.943693	234.855744	4.366643
2.148528	251.452278	4.371648
1.603374	236.342834	4.376653
1.893774	240.833356	4.381658
1.836703	240.631033	4.386662
1.935852	249.030943	4.391667
2.069172	243.666706	4.396672
1.974281	243.914274	4.401677
2.170430	245.881180	4.406682
1.725978	245.879009	4.411686
2.067542	244.714142	4.416691
2.153989	253.836037	4.421696
1.832130	241.521602	4.426701
1.974680	240.058293	4.431706
1.586112	247.690930	4.436710
2.160178	237.925526	4.441715
1.948471	240.453751	4.446720
1.605584	239.558737	4.451725
1.613296	240.214308	4.456730
2.037958	249.527638	4.461734
2.028247	242.724541	4.466739
1.859516	250.725765	4.471744
1.885482	249.276900	4.476749
1.850659	248.901370	4.481754
2.180567	259.968765	4.486758
2.431537	252.017071	4.491763
2.165291	259.565841	4.496768
2.113868	247.291898	4.501773
2.026401	248.427613	4.506778
2.126334	263.305063	4.511782
2.798364	263.536853	4.516787
2.218888	262.737993	4.521792
2.019417	242.575196	4.526797
2.314501	241.885734	4.531802
2.197292	246.243121	4.536806
2.243514	244.127258	4.541811
2.373623	255.446109	4.546816
2.025051	256.454925	4.551821
2.516607	253.848471	4.556826
2.371328	266.559507	4.561830
2.413844	260.476671	4.566835
2.255468	257.577457	4.571840
2.485383	270.988633	4.576845
2.806796	258.515959	4.581850
2.422935	259.971877	4.586854
2.433439	249.051608	4.591859
2.177255	236.563066	4.596864
2.286878	236.121496	4.601869
2.609517	256.605455	4.606874
2.647060	259.333199	4.611878
2.267560	248.753427	4.616883
2.152131	253.927480	4.621888
2.466745	260.378239	4.626893
2.743771	265.331765	4.631898
2.382334	278.487614	4.636902
2.797287	277.920308	4.641907
2.738101	274.852263	4.646912
2.776790	265.304291	4.651917
2.344514	252.281420	4.656922
2.500732	263.967319	4.661926
2.526850	257.495897	4.666931
2.506388	274.328617	4.671936
2.430597	267.355340	4.676941
2.676726	271.532168	4.681946
2.482556	275.595106	4.686950
2.827183	271.708103	4.691955
2.667856	274.083377	4.696960
2.601617	269.246028	4.701965
2.626851	274.334746	4.706970
2.710609	276.990086	4.711974
2.966887	268.025772	4.716979
2.904048	278.478053	4.721984
2.657688	280.488518	4.726989
2.928071	279.537549	4.731994
2.418090	275.650904	4.736998
2.441640	273.390410	4.742003
2.887128	274.149635	4.747008
2.682365	277.014744	4.752013
2.750209	268.967777	4.757018
2.287874	276.255121	4.762022
2.875384	264.968984	4.767027
2.737234	273.904444	4.772032
2.802810	276.321863	4.777037
2.981889	276.365831	4.782042
2.581694	272.546187	4.787046
2.881224	270.870895	4.792051
2.950187	279.015358	4.797056
2.833309	272.969666	4.802061
2.896398	270.849417	4.807066
2.802280	279.187140	4.812070
3.435156	283.808219	4.817075
3.272370	274.175526	4.822080
3.316240	274.345173	4.827085
3.094970	274.751486	4.832090
2.639317	276.705174	4.837094
2.903453	268.610585	4.842099
2.564284	269.425043	4.847104
2.940954	287.256582	4.852109
3.421294	297.495655	4.857114
3.317921	292.705714	4.862118
3.062558	273.541006	4.867123
2.773538	275.668476	4.872128
2.969907	284.651548	4.877133
3.016405	299.045369	4.882138
2.887207	296.014610	4.887142
3.407366	295.428238	4.892147
3.516687	297.680521	4.897152
3.389881	301.566115	4.902157
3.528970	279.158171	4.907162
2.907851	278.529229	4.912166
3.151326	282.575274	4.917171
3.137176	300.065870	4.922176
3.202414	301.396038	4.927181
3.295692	302.405023	4.932186
3.318832	309.389493	4.937190
3.503179	312.312874	4.942195
3.503501	308.834343	4.947200
3.023595	287.484958	4.952205
3.120720	288.093701	4.957210
3.104718	299.446736	4.962214
3.307513	298.054710	4.967219
3.601718	304.450864	4.972224
3.471581	310.187612	4.977229
3.367040	299.822388	4.982234
3.143255	313.621389	4.987238
3.382588	303.501915	4.992243
3.273766	307.606522	4.997248
3.124121	298.825099	5.002253
3.295019	305.198138	5.007258
3.482793	308.038660	5.012262
3.418906	299.956937	5.017267
3.090561	305.131270	5.022272
2.936400	306.387004	5.027277
3.359148	315.090733	5.032282
3.505618	336.756707	5.037286
3.614081	337.754290	5.042291
3.415218	335.511810	5.047296
3.616139	335.681797	5.052301
3.504432	324.355150	5.057306
3.466047	339.278751	5.062310
3.849233	332.548840	5.067315
3.678161	335.470125	5.072320
3.803352	335.396756	5.077325
3.745511	334.442519	5.082330
3.689665	325.037307	5.087334
3.734556	309.926017	5.092339
3.547083	306.395820	5.097344
3.537821	319.035354	5.102349
3.730943	323.355982	5.107354
3.813928	335.488638	5.112358
3.883923	314.601142	5.117363
3.876769	314.465114	5.122368
3.600823	314.027638	5.127373
3.970763	317.784693	5.132378
3.740215	314.362096	5.137382
3.614610	308.760658	5.142387
3.685344	326.040038	5.147392
3.502395	331.944821	5.152397
4.152386	326.289649	5.157402
3.917057	331.386371	5.162406
4.032248	332.731328	5.167411
3.990220	339.759598	5.172416
3.704109	335.559459	5.177421
4.073906	323.883421	5.182426
3.792562	324.598879	5.187430
3.945918	324.970948	5.192435
4.043980	330.230114	5.197440
3.778099	330.194315	5.202445
3.828219	318.019076	5.207450
3.884223	331.425466	5.212454
4.124512	328.482472	5.217459
4.104434	328.764178	5.222464
3.652015	338.589792	5.227469
4.158590	327.925247	5.232474
3.871037	341.881886	5.237478
3.767208	328.520396	5.242483
3.705482	327.383481	5.247488
3.834150	335.777742	5.252493
4.100239	331.432938	5.257498
3.747070	328.863075	5.262502
3.935132	330.310966	5.267507
3.745640	328.880736	5.272512
3.839596	333.014990	5.277517
4.374866	343.714226	5.282522
3.743486	351.280118	5.287526
4.608680	354.618214	5.292531
4.559179	355.402291	5.297536
4.206373	349.724344	5.302541
4.210939	337.899628	5.307546
4.022662	331.754681	5.312550
3.697833	339.265866	5.317555
3.858057	348.715957	5.322560
4.258743	364.660035	5.327565
4.107341	356.941914	5.332570
4.134933	368.999540	5.337574
4.533630	361.447901	5.342579
4.476710	371.555109	5.347584
4.135856	371.405280	5.352589
4.379279	367.227430	5.357594
4.201875	368.563597	5.362598
4.387885	367.690780	5.367603
4.378757	367.670521	5.372608
4.184376	379.716110	5.377613
4.764787	367.697190	5.382618
4.056217	362.856856	5.387622
4.173156	368.580186	5.392627
4.315554	365.753900	5.397632
4.216709	365.281460	5.402637
4.229972	364.874255	5.407642
4.024702	362.116411	5.412646
4.136996	382.543343	5.417651
4.668214	385.010665	5.422656
4.495434	404.251663	5.427661
4.996387	388.375796	5.432666
4.625660	382.062831	5.437670
4.421900	372.864709	5.442675
4.138189	372.374057	5.447680
4.410848	380.434200	5.452685
4.634930	394.382414	5.457690
4.391053	393.905071	5.462694
4.638399	397.518734	5.467699
4.664685	396.224315	5.472704
4.721678	404.618292	5.477709
4.692801	395.552707	5.482714
4.608184	407.700054	5.487718
4.868813	402.048595	5.492723
4.703666	396.949403	5.497728
4.688055	401.321915	5.502733
4.910389	393.645061	5.507738
4.790992	402.912159	5.512742
4.645095	394.517230	5.517747
4.663816	394.463531	5.522752
4.712751	402.929887	5.527757
4.797077	399.935053	5.532762
4.617191	402.156092	5.537766
4.524238	397.867196	5.542771
4.739536	396.697652	5.547776
4.704803	407.685257	5.552781
4.566180	398.171016	5.557786
4.751450	410.559249	5.562790
5.043236	398.904014	5.567795
4.895341	398.008352	5.572800
4.823253	404.266909	5.577805
4.976884	397.516318	5.582810
4.766366	401.113336	5.587814
4.888221	400.346098	5.592819
5.119025	394.847995	5.597824
5.006669	409.736203	5.602829
5.190754	391.979705	5.607834
4.713974	408.047964	5.612838
4.960360	396.827902	5.617843
5.256132	401.811903	5.622848
4.994819	406.030683	5.627853
4.925193	399.615963	5.632858
4.908353	401.698408	5.637862
4.972664	390.062241	5.642867
5.261785	397.138309	5.647872
4.867470	394.301965	5.652877
5.123826	401.513919	5.657882
4.713420	397.506499	5.662886
4.870076	398.629671	5.667891
4.783193	401.433177	5.672896
4.791520	403.073750	5.677901
5.388150	416.950197	5.682906
5.167348	419.836942	5.687910
5.332523	415.400550	5.692915
5.271541	406.108821	5.697920
4.978972	407.220424	5.702925
5.317305	410.640181	5.707930
4.959784	414.659858	5.712934
5.030343	414.637996	5.717939
5.280408	423.396340	5.722944
5.289563	438.794423	5.727949
5.536613	434.554383	5.732954
5.449425	437.500226	5.737958
5.508668	423.641298	5.742963
5.479726	408.605923	5.747968
4.900165	411.436065	5.752973
5.266491	412.049009	5.757978
5.269709	428.458623	5.762982
5.333812	424.163152	5.767987
5.484196	422.973610	5.772992
5.162577	429.768570	5.777997
5.561726	422.493491	5.783002
5.268357	429.926477	5.788006
5.408652	431.564655	5.793011
5.168836	421.737470	5.798016
5.307280	426.499776	5.803021
5.502635	429.676504	5.808026
5.211362	433.614923	5.813030
5.420938	434.408632	5.818035
5.672256	434.880653	5.823040
5.288367	436.690217	5.828045
5.618792	435.165077	5.833050
5.716070	436.181891	5.838054
5.590643	433.504103	5.843059
5.503942	423.255219	5.848064
5.403638	437.130106	5.853069
5.381752	432.485433	5.858074
5.403772	440.208775	5.863078
5.740321	434.835953	5.868083
5.263111	427.598588	5.873088
5.287980	442.184592	5.878093
5.609367	426.565073	5.883098
5.212729	440.024886	5.888102
5.636136	447.100561	5.893107
5.962713	461.946058	5.898112
5.709840	462.319739	5.903117
6.104980	459.204956	5.908122
5.829662	444.395992	5.913126
5.572189	436.087469	5.918131
5.804952	436.247429	5.923136
5.494685	435.105245	5.928141
5.824587	430.859526	5.933146
5.625490	441.105457	5.938150
5.677557	460.796771	5.943155
6.219699	458.217988	5.948160
5.823424	449.086549	5.953165
5.729269	438.951967	5.958170
6.318628	445.004500	5.963174
5.682014	442.284196	5.968179
5.791231	444.377466	5.973184
5.324745	440.375606	5.978189
5.955005	444.821935	5.983194
5.627280	469.493401	5.988198
5.469333	465.301919	5.993203
5.795546	462.813096	5.998208
5.519466	465.769027	6.003213
5.588608	466.616666	6.008218
5.783855	464.526324	6.013222
5.608398	467.381664	6.018227
6.100327	453.684043	6.023232
5.672090	463.594123	6.028237
5.854776	456.581746	6.033242
5.815075	469.346639	6.038246
5.994971	479.018305	6.043251
6.051119	480.388480	6.048256
5.748911	468.632216	6.053261
5.983751	465.645308	6.058266
5.607283	477.289071	6.063270
6.238836	487.125634	6.068275
6.051675	472.898144	6.073280
5.988423	470.878985	6.078285
6.049210	460.110644	6.083290
5.873346	468.372860	6.088294
5.748537	469.868227	6.093299
5.726299	462.881618	6.098304
5.937177	494.283141	6.103309
6.105143	488.493130	6.108314
5.781636	480.580167	6.113318
5.739072	473.407687	6.118323
6.278907	480.393380	6.123328
5.947918	484.775118	6.128333
6.232064	470.644529	6.133338
5.644177	467.560324	6.138342
5.627932	466.185943	6.143347
5.873680	476.695208	6.148352
6.373551	494.086380	6.153357
6.013549	469.281978	6.158362
6.170973	472.117313	6.163366
5.717767	472.587834	6.168371
6.137819	457.917647	6.173376
5.921812	463.759696	6.178381
5.867298	466.387928	6.183386
5.451799	469.457018	6.188390
5.872060	465.010381	6.193395
6.005266	463.336073	6.198400
5.921508	469.389789	6.203405
5.927044	461.844248	6.208410
5.809320	463.464534	6.213414
6.080014	463.327514	6.218419
6.021542	462.371203	6.223424
5.636209	473.712343	6.228429
5.960463	474.191976	6.233434
6.123990	467.141929	6.238438
5.865704	467.091449	6.243443
5.897654	459.771020	6.248448
5.644484	473.051318	6.253453
6.113734	465.287606	6.258458
5.998247	469.906832	6.263462
6.140243	470.247246	6.268467
6.084192	458.596105	6.273472
5.929289	478.856819	6.278477
5.989956	477.214301	6.283482
6.194898	471.935170	6.288486
6.275114	470.058520	6.293491
6.191315	470.105334	6.298496
6.067263	472.688686	6.303501
5.997515	471.569671	6.308506
6.140664	471.439839	6.313510
6.036517	464.307199	6.318515
5.942998	472.054497	6.323520
5.788903	474.163316	6.328525
5.780128	476.802695	6.333530
5.992059	475.307310	6.338534
6.014765	464.104840	6.343539
6.083624	465.700627	6.348544
6.118976	473.986152	6.353549
6.239550	461.747979	6.358554
5.641038	452.083403	6.363558
5.651414	460.522258	6.368563
6.214033	461.731685	6.373568
5.994821	463.805939	6.378573
6.090690	458.654661	6.383578
5.549556	455.960714	6.388582
6.023080	461.844446	6.393587
5.907540	455.684399	6.398592
5.915979	473.765419	6.403597
6.216466	463.941152	6.408602
5.993554	456.290120	6.413606
5.703306	446.854923	6.418611
5.927382	445.483028	6.423616
6.049518	464.095508	6.428621
6.040854	438.139320	6.433626
5.890409	444.300410	6.438630
5.675569	444.860962	6.443635
5.874556	450.839061	6.448640
5.874071	459.124022	6.453645
6.299931	458.652974	6.458650
5.876912	444.366043	6.463654
5.579842	447.185351	6.468659
5.916189	444.992231	6.473664
6.099904	470.916432	6.478669
5.851691	464.549129	6.483674
5.966229	449.955974	6.488678
6.224483	457.806416	6.493683
5.901847	442.506256	6.498688
5.740939	446.953054	6.503693
5.426051	437.162413	6.508698
5.601345	454.763778	6.513702
5.597311	461.719089	6.518707
5.751568	462.005763	6.523712
6.137353	469.231955	6.528717
5.536683	463.796445	6.533722
5.930424	459.925703	6.538726
6.116239	467.655382	6.543731
6.272009	459.902335	6.548736
5.943049	469.195622	6.553741
6.082427	459.766759	6.558746
6.009019	458.443913	6.563750
5.605480	470.220637	6.568755
6.087591	465.009501	6.573760
5.962907	463.760297	6.578765
6.287058	458.327958	6.583770
6.071542	466.619853	6.588774
6.230196	462.800417	6.593779
6.057524	458.241380	6.598784
5.910542	441.269403	6.603789
5.627718	436.556406	6.608794
5.618930	437.937765	6.613798
5.575219	464.123731	6.618803
5.986541	466.833985	6.623808
5.945169	465.839311	6.628813
5.992727	463.616831	6.633818
6.096320	466.885188	6.638822
6.045042	474.511801	6.643827
6.173284	467.264166	6.648832
5.789898	464.795405	6.653837
5.936215	458.268992	6.658842
6.003604	464.008684	6.663846
5.745900	464.994121	6.668851
6.542189	444.663780	6.673856
5.642116	435.795266	6.678861
5.798805	439.743296	6.683866
5.813190	448.176346	6.688870
5.962064	453.745017	6.693875
6.096541	438.966812	6.698880
5.778498	446.092709	6.703885
5.999520	436.572540	6.708890
5.851846	435.659473	6.713894
5.874158	456.037521	6.718899
5.696099	462.196498	6.723904
5.862558	474.338674	6.728909
5.765626	473.204640	6.733914
6.041949	466.772847	6.738918
5.779315	473.311351	6.743923
6.369004	471.836456	6.748928
5.674845	469.428030	6.753933
5.982726	477.785675	6.758938
5.946158	472.387632	6.763942
5.884832	467.770224	6.768947
6.036996	477.297905	6.773952
6.063197	474.854405	6.778957
5.854907	468.684905	6.783962
5.752403	455.230928	6.788966
6.059396	467.489257	6.793971
5.985886	462.807373	6.798976
5.676929	459.679375	6.803981
5.903348	462.423714	6.808986
6.263138	461.125956	6.813990
5.762685	452.690074	6.818995
5.769926	457.254758	6.824000
6.092075	468.269326	6.829005
5.983240	458.976440	6.834010
5.918712	454.739440	6.839014
5.696293	467.102140	6.844019
6.067632	455.012920	6.849024
6.226647	470.449472	6.854029
5.944559	457.914340	6.859034
5.692913	449.721073	6.864038
5.781140	444.968898	6.869043
5.898143	456.345329	6.874048
6.248452	465.898086	6.879053
6.295489	452.646193	6.884058
5.790648	447.665408	6.889062
5.665073	441.378174	6.894067
6.328921	437.098458	6.899072
6.033765	440.848477	6.904077
5.747578	438.355869	6.909082
5.661408	442.634941	6.914086
5.486863	439.636554	6.919091
6.132780	452.620975	6.924096
5.784122	455.667310	6.929101
5.729103	462.893750	6.934106
5.811491	471.461144	6.939110
5.571831	479.283649	6.944115
6.002225	474.815591	6.949120
6.119646	466.076512	6.954125
6.051611	471.942909	6.959130
6.181896	473.417387	6.964134
5.836177	472.009163	6.969139
6.149109	464.410358	6.974144
6.046746	446.590307	6.979149
6.034654	436.368085	6.984154
5.856501	436.599500	6.989158
5.597406	450.872573	6.994163
5.992433	451.439899	6.999168
6.094588	466.149637	7.004173
5.854276	456.434995	7.009178
5.793921	441.723112	7.014182
5.939109	452.557708	7.019187
6.147556	448.993443	7.024192
5.959569	447.197289	7.029197
6.091037	447.197864	7.034202
5.991134	445.453966	7.039206
6.049189	458.628650	7.044211
6.046041	436.131836	7.049216
5.831619	438.294683	7.054221
5.533276	449.110839	7.059226
5.847391	440.357829	7.064230
5.651629	446.507902	7.069235
5.912954	457.690440	7.074240
6.093052	463.224127	7.079245
5.765763	451.779493	7.084250
6.095681	455.495479	7.089254
5.794328	452.026209	7.094259
6.146090	448.836743	7.099264
5.671479	455.226555	7.104269
5.982593	460.283211	7.109274
5.988666	463.422734	7.114278
5.891807	463.454155	7.119283
6.248766	445.044491	7.124288
5.587612	451.718687	7.129293
6.079326	442.499255	7.134298
5.930389	438.390546	7.139302
5.875352	452.033158	7.144307
6.084053	438.822290	7.149312
5.901853	442.630101	7.154317
5.807047	451.049136	7.159322
6.018793	434.821883	7.164326
5.603840	453.353121	7.169331
5.916618	443.750800	7.174336
5.646150	465.672933	7.179341
5.991698	463.274038	7.184346
5.947411	468.932047	7.189350
6.050262	471.408421	7.194355
6.011494	462.956577	7.199360
5.655607	464.817928	7.204365
5.876983	467.855954	7.209370
6.243892	477.490419	7.214374
6.056635	457.659401	7.219379
5.766388	444.390363	7.224384
5.731590	446.850540	7.229389
6.045005	455.128318	7.234394
6.216129	461.163150	7.239398
5.812073	443.697538	7.244403
5.825934	440.468133	7.249408
5.819946	446.549368	7.254413
5.899112	454.567314	7.259418
5.769097	467.464236	7.264422
6.253743	465.121353	7.269427
6.246364	458.618711	7.274432
6.001822	449.562496	7.279437
5.562083	446.238774	7.284442
6.104761	440.610081	7.289446
5.734298	441.559004	7.294451
6.054594	448.034946	7.299456
6.084752	447.262425	7.304461
6.093571	450.712885	7.309466
6.104835	448.541235	7.314470
6.100387	456.762719	7.319475
6.222192	438.185538	7.324480
5.877939	444.778642	7.329485
6.060775	442.968412	7.334490
6.265786	444.611424	7.339494
6.103163	451.976513	7.344499
6.164297	442.278476	7.349504
5.878839	438.682442	7.354509
5.951349	449.758222	7.359514
6.118922	448.396310	7.364518
5.575520	451.695634	7.369523
5.771001	439.349518	7.374528
5.823273	442.760983	7.379533
5.443939	448.846650	7.384538
5.898704	448.656342	7.389542
5.681800	450.747181	7.394547
5.923910	441.853795	7.399552
5.645640	448.768445	7.404557
5.608790	444.116981	7.409562
5.692399	436.140518	7.414566
5.553315	449.363156	7.419571
6.301266	464.900533	7.424576
5.887457	458.380390	7.429581
5.593358	448.393292	7.434586
6.024905	465.814338	7.439590
5.835515	477.961197	7.444595
5.966203	474.991400	7.449600
6.070370	487.292534	7.454605
5.792757	470.850771	7.459610
6.136053	466.114607	7.464614
5.892176	460.204010	7.469619
5.786479	452.865219	7.474624
5.641158	461.164190	7.479629
5.929160	471.853306	7.484634
6.080459	473.748366	7.489638
6.320857	474.797636	7.494643
5.573758	455.820600	7.499648
5.584276	453.502058	7.504653
5.617677	472.090816	7.509658
5.641196	470.834936	7.514662
5.583308	475.701917	7.519667
5.762313	473.946982	7.524672
5.912090	484.534956	7.529677
5.752503	475.802643	7.534682
5.951453	471.614988	7.539686
5.742412	478.083413	7.544691
5.543879	473.740412	7.549696
5.770361	469.361107	7.554701
6.014944	472.373372	7.559706
6.147550	474.163597	7.564710
6.000576	478.898567	7.569715
6.100549	476.791104	7.574720
5.838192	476.841349	7.579725
5.792845	478.356662	7.584730
6.120909	478.493087	7.589734
6.129914	493.480395	7.594739
5.814739	472.305842	7.599744
5.901501	486.702223	7.604749
5.966349	484.153827	7.609754
6.069240	473.473200	7.614758
5.744076	486.916634	7.619763
5.799419	476.093143	7.624768
5.872535	483.695533	7.629773
5.746041	482.953783	7.634778
5.998601	472.600525	7.639782
5.892971	480.810226	7.644787
5.791829	470.084183	7.649792
5.878339	477.195345	7.654797
5.568472	486.308261	7.659802
6.161681	476.304302	7.664806
5.910386	486.104868	7.669811
5.839101	484.439880	7.674816
5.822279	488.410052	7.679821
5.906805	482.559121	7.684826
6.101845	494.837658	7.689830
5.604137	496.617602	7.694835
5.916503	478.695824	7.699840
5.939918	489.736379	7.704845
5.837109	483.770752	7.709850
5.911793	488.678060	7.714854
5.932278	510.226489	7.719859
6.126446	512.008065	7.724864
5.916438	493.109647	7.729869
5.794013	489.396519	7.734874
6.213009	490.699874	7.739878
6.020994	485.743254	7.744883
5.732442	491.306300	7.749888
5.846472	495.370364	7.754893
5.925360	491.352240	7.759898
6.413840	482.881030	7.764902
5.909716	493.103890	7.769907
6.011764	485.297600	7.774912
6.136234	486.639251	7.779917
5.779541	482.055737	7.784922
5.979341	483.608450	7.789926
5.799447	487.756096	7.794931
5.826694	485.644143	7.799936
5.947623	483.726388	7.804941
6.216061	482.535572	7.809946
6.184802	484.106561	7.814950
6.071959	481.844434	7.819955
5.933979	485.090194	7.824960
5.908161	486.401571	7.829965
5.877286	489.306884	7.834970
6.101760	484.777933	7.839974
5.700708	493.745377	7.844979
6.110759	490.394462	7.849984
5.834835	491.197236	7.854989
5.742608	494.112353	7.859994
6.183162	485.110971	7.864998
5.557526	493.868086	7.870003
5.803474	481.395344	7.875008
5.955962	478.613734	7.880013
6.006411	485.425417	7.885018
6.162983	472.944054	7.890022
6.144092	484.521484	7.895027
6.056795	483.480767	7.900032
5.996939	479.509585	7.905037
5.629058	480.061238	7.910042
6.252407	470.705456	7.915046
5.848574	482.607151	7.920051
6.214978	475.438921	7.925056
5.916892	484.267687	7.930061
5.571439	485.334212	7.935066
5.842639	479.317277	7.940070
5.721834	484.009813	7.945075
5.996706	482.013586	7.950080
5.877411	483.778585	7.955085
5.866516	486.116393	7.960090
5.820214	483.328751	7.965094
5.804487	480.531883	7.970099
6.064321	478.002979	7.975104
6.212005	488.888887	7.980109
6.195186	486.467336	7.985114
6.164671	480.522453	7.990118
6.235434	484.933295	7.995136
6.223989	484.321994	8.000154
5.860280	472.332077	8.005171
5.672950	475.693160	8.010189
6.228374	474.801239	8.015206
5.791679	482.276831	8.020224
5.948895	483.224166	8.025242
6.310591	485.621438	8.030259
6.071757	472.713798	8.035277
6.035645	462.008099	8.040294
5.340868	463.233644	8.045312
5.628261	471.797432	8.050330
5.744415	484.623365	8.055347
5.877961	489.575460	8.060365
5.927509	489.261868	8.065382
5.950213	490.435283	8.070400
5.654240	496.243149	8.075418
5.779403	494.462000	8.080435
5.646979	494.918351	8.085453
5.966850	487.408691	8.090470
5.839166	500.116517	8.095488
5.972879	489.522520	8.100506
6.087090	492.229408	8.105523
6.108715	494.399961	8.110541
6.077196	490.116141	8.115558
5.924497	494.848712	8.120576
5.786424	491.120349	8.125594
6.036842	496.768116	8.130611
5.510092	497.962586	8.135629
5.898814	506.880189	8.140646
5.683941	526.485391	8.145664
6.208270	530.970811	8.150682
6.278415	525.574705	8.155699
6.114906	520.560320	8.160717
6.702285	513.945277	8.165734
6.429602	522.694301	8.170752
6.466658	507.538015	8.175770
6.323008	496.647033	8.180787
5.492063	488.180325	8.185805
5.820212	496.801521	8.190822
6.152734	506.442181	8.195840
6.190547	514.989017	8.200858
6.244732	513.386183	8.205875
6.066671	515.765111	8.210893
6.341015	523.075104	8.215910
6.140519	513.569227	8.220928
5.969666	504.708373	8.225946
6.306196	512.102308	8.230963
6.091566	517.958271	8.235981
6.238050	513.502351	8.240998
6.376225	514.626264	8.246016
6.031787	511.667958	8.251034
6.457071	494.818953	8.256051
6.066696	508.257197	8.261069
5.991464	488.963067	8.266086
5.740933	498.558911	8.271104
6.101312	512.826231	8.276122
6.361385	516.590477	8.281139
6.365807	521.887245	8.286157
6.346412	518.986124	8.291174
6.470475	514.093023	8.296192
6.392324	518.018792	8.301210
6.227414	496.329925	8.306227
5.950155	505.323970	8.311245
6.282741	502.125394	8.316262
6.552556	519.165798	8.321280
6.306018	518.887639	8.326298
6.173680	506.468328	8.331315
6.224132	519.122351	8.336333
6.198028	510.457101	8.341350
6.222124	524.175259	8.346368
6.615388	527.806947	8.351386
6.316566	511.804985	8.356403
6.093302	497.609219	8.361421
6.777782	499.343842	8.366438
6.330405	500.382810	8.371456
5.973479	496.913045	8.376474
6.067163	490.896361	8.381491
6.219884	517.133760	8.386509
6.462015	513.355583	8.391526
6.247976	523.733104	8.396544
6.366196	520.365054	8.401562
6.408124	525.864232	8.406579
6.251653	526.752891	8.411597
6.372456	514.693039	8.416614
6.492791	518.635026	8.421632
6.396046	521.104761	8.426650
6.613719	520.932304	8.431667
6.080371	526.704446	8.436685
6.199768	523.147042	8.441702
6.317251	516.755165	8.446720
6.421851	520.643867	8.451738
6.437114	516.204836	8.456755
6.565973	527.623106	8.461773
6.646498	514.782615	8.466790
6.682334	528.236644	8.471808
6.251270	505.833601	8.476826
6.158108	511.795543	8.481843
5.990369	523.704408	8.486861
6.347692	522.212395	8.491878
6.548630	523.820519	8.496896
6.205691	522.731682	8.501914
6.589326	514.190043	8.506931
6.369095	526.620188	8.511949
6.263663	526.002264	8.516966
6.238263	521.368039	8.521984
6.227169	526.597708	8.527002
6.441080	523.523174	8.532019
6.195101	522.717015	8.537037
6.256305	514.619681	8.542054
6.171825	525.266392	8.547072
6.660580	541.917508	8.552090
6.905640	535.934106	8.557107
6.533283	524.618559	8.562125
6.948535	510.227882	8.567143
6.677265	516.835714	8.572160
6.701312	522.346130	8.577178
6.760102	517.906753	8.582195
6.617408	531.692596	8.587213
6.580280	521.568667	8.592231
6.297847	516.099485	8.597248
6.375313	526.692708	8.602266
6.583068	521.794552	8.607283
6.355546	523.607736	8.612301
6.728918	512.455628	8.617319
6.732052	525.438359	8.622336
6.738186	524.636749	8.627354
6.592962	519.316596	8.632371
6.285256	520.598469	8.637389
6.322303	524.252752	8.642407
6.523448	519.175790	8.647424
6.403192	524.770226	8.652442
6.378403	523.670632	8.657459
6.755582	545.617991	8.662477
6.500770	542.901257	8.667495
6.727170	543.843593	8.672512
6.695250	552.910855	8.677530
6.764666	545.752414	8.682547
6.714629	550.410070	8.687565
6.968152	548.170215	8.692583
6.840762	535.580978	8.697600
6.392904	534.481038	8.702618
6.968812	520.715168	8.707635
6.245821	521.991859	8.712653
6.387503	529.911059	8.717671
6.752091	543.536424	8.722688
6.736711	556.216379	8.727706
6.759118	544.139791	8.732723
6.828863	552.094972	8.737741
6.814966	555.199313	8.742759
6.735041	541.740837	8.747776
6.669357	530.918953	8.752794
6.851290	542.206376	8.757811
6.626529	546.207893	8.762829
6.463109	546.473942	8.767847
6.544065	549.230654	8.772864
6.920605	546.660733	8.777882
6.859386	547.550883	8.782899
6.677752	549.927457	8.787917
6.665070	551.828744	8.792935
6.447545	553.786124	8.797952
6.012849	563.331326	8.802970
6.264343	552.376400	8.807987
6.749346	554.959470	8.813005
6.370537	555.332376	8.818023
6.571958	568.633731	8.823040
6.701035	571.117904	8.828058
6.895442	571.152447	8.833075
7.104235	588.897303	8.838093
7.031863	575.782199	8.843111
7.213334	580.443705	8.848128
6.711393	565.707235	8.853146
6.680096	548.661838	8.858163
6.939209	561.208779	8.863181
7.308546	576.881638	8.868199
7.002451	561.703009	8.873216
6.648411	559.591297	8.878234
7.148403	547.430604	8.883251
6.531793	550.005842	8.888269
6.649798	546.328990	8.893287
6.958637	554.580822	8.898304
7.079924	574.284726	8.903322
7.217026	570.982812	8.908339
7.249328	562.391676	8.913357
6.827047	559.177031	8.918375
6.823311	547.842322	8.923392
6.898166	549.327912	8.928410
6.892346	545.930083	8.933427
7.120240	549.707560	8.938445
6.950378	547.626848	8.943463
7.108209	540.317111	8.948480
6.902656	551.215243	8.953498
6.717265	553.548548	8.958515
6.873584	551.714973	8.963533
6.742063	566.094807	8.968551
6.847711	571.899919	8.973568
6.996422	581.913472	8.978586
7.077395	572.855814	8.983603
7.312584	580.871694	8.988621
7.456421	577.560786	8.993639
7.485187	556.487030	8.998656
7.351426	555.780712	9.003674
6.896952	548.773512	9.008691
6.973180	535.435533	9.013709
6.790775	550.449936	9.018727
7.060030	539.666462	9.023744
6.780114	544.080851	9.028762
6.815541	538.721218	9.033779
7.163780	555.137261	9.038797
7.211354	553.991389	9.043815
6.827570	547.564516	9.048832
6.824001	566.243189	9.053850
6.939384	572.592307	9.058867
7.150445	572.880556	9.063885
6.854258	578.054486	9.068903
7.042938	581.668621	9.073920
6.944661	584.865923	9.078938
7.107403	585.088193	9.083955
7.414621	578.593304	9.088973
7.029748	593.887444	9.093991
7.177914	577.645386	9.099008
7.273232	586.357688	9.104026
7.383723	583.870561	9.109043
7.161157	575.942593	9.114061
7.181869	583.318982	9.119079
7.224511	586.143284	9.124096
7.179808	579.851363	9.129114
7.284674	579.833274	9.134131
7.467017	572.658413	9.139149
7.258510	584.847306	9.144167
7.576506	572.217671	9.149184
7.486323	562.193471	9.154202
7.273461	550.394544	9.159219
7.433872	546.503772	9.164237
6.978514	555.173540	9.169255
7.119757	537.313324	9.174272
7.043352	552.930334	9.179290
7.134351	574.559189	9.184307
7.449758	575.090703	9.189325
7.213133	576.995359	9.194343
7.353541	575.055577	9.199360
7.065429	570.224274	9.204378
7.424742	580.057558	9.209395
7.640620	579.102984	9.214413
7.260353	567.344466	9.219431
7.404307	558.440705	9.224448
7.138190	566.480455	9.229466
7.256872	568.147723	9.234483
7.960212	570.626402	9.239501
7.253102	553.251433	9.244519
7.449147	547.299597	9.249536
7.275575	545.106322	9.254554
6.934954	556.751648	9.259571
7.361440	561.341324	9.264589
7.233515	579.830660	9.269607
7.677769	567.695356	9.274624
7.372092	574.183351	9.279642
7.231519	565.002888	9.284659
7.564408	570.586781	9.289677
7.188845	579.739913	9.294695
7.313547	577.384075	9.299712
7.214480	580.184689	9.304730
7.212793	579.445395	9.309747
7.380680	576.652297	9.314765
7.144218	573.211505	9.319783
7.379269	578.569754	9.324800
7.592849	575.361418	9.329818
7.087329	582.295787	9.334835
7.627286	575.852759	9.339853
7.388558	574.889106	9.344871
7.369527	580.993465	9.349888
7.566073	582.249007	9.354906
7.434909	582.067803	9.359923
7.485484	578.925729	9.364941
7.445276	585.256622	9.369959
7.619149	581.039615	9.374976
7.548063	575.853170	9.379994
7.196721	574.750767	9.385011
7.464704	573.859574	9.390029
7.340923	582.882480	9.395047
7.584260	577.598897	9.400064
7.581956	580.980427	9.405082
7.286937	580.879011	9.410099
7.490859	581.153291	9.415117
7.330088	590.466578	9.420135
7.477482	582.723356	9.425152
7.474699	586.829119	9.430170
7.789080	599.111809	9.435187
7.700452	595.334851	9.440205
7.196458	599.636906	9.445223
7.740362	595.497357	9.450240
7.813766	608.741291	9.455258
7.427024	612.208573	9.460275
8.084220	607.502204	9.465293
7.653080	598.909342	9.470311
7.670081	589.607012	9.475328
7.768961	580.817611	9.480346
7.245370	586.139371	9.485363
7.969655	584.281267	9.490381
8.117418	591.270824	9.495399
7.811383	596.388331	9.500416
7.615693	587.882513	9.505434
7.596021	588.585852	9.510451
7.442534	580.491886	9.515469
7.581630	590.099793	9.520487
7.931220	586.948763	9.525504
7.926664	584.821281	9.530522
7.620222	586.096256	9.535539
7.607372	580.924735	9.540557
7.488286	583.152347	9.545575
7.539404	582.691457	9.550592
7.981569	587.422815	9.555610
7.838303	593.152781	9.560627
7.887086	579.343774	9.565645
7.549436	569.918725	9.570663
7.728794	579.693540	9.575680
7.912480	584.505454	9.580698
7.866541	591.554960	9.585715
7.998128	570.803044	9.590733
7.636738	588.108658	9.595751
7.448148	576.810360	9.600768
7.758007	590.527533	9.605786
7.984578	606.505229	9.610803
8.131467	609.722806	9.615821
7.755850	603.024890	9.620839
7.394743	591.228920	9.625856
8.000626	598.637178	9.630874
7.807913	613.973803	9.635891
8.142566	609.242505	9.640909
7.657552	612.185613	9.645927
7.572244	613.890728	9.650944
7.965582	609.130584	9.655962
8.204741	614.956826	9.660979
8.052466	609.486447	9.665997
7.980538	603.981655	9.671015
7.746378	610.114302	9.676032
7.813869	611.926490	9.681050
7.685400	616.265535	9.686067
8.060587	605.871659	9.691085
7.771845	609.957246	9.696103
7.756442	619.167065	9.701120
7.588429	620.021036	9.706138
7.666141	613.355634	9.711155
7.638600	608.777836	9.716173
7.613257	620.941431	9.721191
7.582068	616.475449	9.726208
8.104476	622.286109	9.731226
7.676302	641.377740	9.736243
8.047351	641.713212	9.741261
8.058456	652.177797	9.746279
7.801362	646.543936	9.751296
7.911603	648.577352	9.756314
7.831507	642.704444	9.761331
7.972119	640.457951	9.766349
8.113086	647.231161	9.771367
8.096319	648.631210	9.776384
8.752137	639.006549	9.781402
8.440969	648.077764	9.786419
8.066650	622.206731	9.791437
8.120309	615.666575	9.796455
7.995816	614.297940	9.801472
8.208588	614.864820	9.806490
7.993690	621.123787	9.811507
8.179274	613.818458	9.816525
8.055161	613.468378	9.821543
7.864819	628.399143	9.826560
8.491237	635.919155	9.831578
7.889036	636.728373	9.836595
8.223672	633.296377	9.841613
8.097653	633.602467	9.846631
7.794196	649.470681	9.851648
7.921971	643.098103	9.856666
8.037337	655.844984	9.861683
8.440727	644.775777	9.866701
8.550424	643.810896	9.871719
8.371366	635.270990	9.876736
8.268747	639.947648	9.881754
8.552096	641.584209	9.886771
8.387752	627.318495	9.891789
8.243150	615.639265	9.896807
8.374118	622.269846	9.901824
8.106643	605.602197	9.906842
8.016447	611.209185	9.911859
8.159863	618.412846	9.916877
8.457856	636.412004	9.921895
8.284397	629.266335	9.926912
8.465460	626.901713	9.931930
8.155883	621.455113	9.936947
8.801986	616.993478	9.941965
8.575515	615.297135	9.946983
8.296201	615.610988	9.952000
8.568195	608.645208	9.957018
8.172664	614.596821	9.962035
7.943727	610.904396	9.967053
7.956500	615.335310	9.972071
7.928817	621.168507	9.977088
8.348516	629.674176	9.982106
8.309184	647.420973	9.987123
8.535933	647.838889	9.992141
8.743871	646.171316	9.997159
8.248739	647.556983	10.002176
8.519677	644.740447	10.007194
8.447667	658.475681	10.012211
8.450422	658.651322	10.017229
8.761586	647.454933	10.022247
8.324740	629.027164	10.027264
8.524735	622.826828	10.032282
8.113431	611.577331	10.037299
8.303795	635.581492	10.042317
8.356402	643.696447	10.047335
8.164444	643.553100	10.052352
8.381216	646.342369	10.057370
8.770102	645.462571	10.062387
8.692328	649.451494	10.067405
8.730232	644.162075	10.072423
8.500866	650.039237	10.077440
8.550799	639.904304	10.082458
8.555745	650.779525	10.087475
8.737088	631.741367	10.092493
8.170905	619.713537	10.097511
8.028014	633.476277	10.102528
8.455663	637.583144	10.107546
8.448907	651.851776	10.112563
8.322565	655.196462	10.117581
8.344462	643.573192	10.122599
8.434952	648.133313	10.127616
8.560342	640.913954	10.132634
8.320802	645.002986	10.137651
8.316291	643.763410	10.142669
8.358217	647.352743	10.147687
8.299067	640.648270	10.152704
8.554815	654.793753	10.157722
8.769771	664.794381	10.162739
8.652660	663.073754	10.167757
8.668947	656.128407	10.172775
8.557265	669.758050	10.177792
8.739655	661.558810	10.182810
8.887713	668.421985	10.187827
8.466146	659.339937	10.192845
8.592739	657.942950	10.197863
8.629007	673.292751	10.202880
8.780197	671.904272	10.207898
8.778059	666.112879	10.212915
8.923427	671.635071	10.217933
8.887993	664.998688	10.222951
8.626337	655.124178	10.227968
8.733775	644.838750	10.232986
8.896993	657.085395	10.238003
8.426290	649.811379	10.243021
8.550056	660.345427	10.248039
8.769502	659.721528	10.253056
8.699935	669.436995	10.258074
9.145747	666.097332	10.263091
8.999705	674.120329	10.268109
9.013039	662.409499	10.273127
8.807775	661.716438	10.278144
8.833788	649.592321	10.283162
8.796112	643.485609	10.288179
8.753023	647.491600	10.293197
8.824362	643.472902	10.298215
8.687189	665.459271	10.303232
8.839113	662.958355	10.308250
8.619017	665.304138	10.313267
8.835824	678.235933	10.318285
9.159960	665.546545	10.323303
8.980067	676.432823	10.328320
9.034966	665.782520	10.333338
9.255290	672.430945	10.338355
8.912102	669.482833	10.343373
9.074971	653.266991	10.348391
8.701318	652.192894	10.353408
9.151521	639.969346	10.358426
8.664254	646.003733	10.363443
8.844148	649.870505	10.368461
9.068182	648.667543	10.373479
9.033134	662.472420	10.378496
8.951272	663.736057	10.383514
8.853762	663.857108	10.388531
9.211012	665.033785	10.393549
9.108754	660.241637	10.398567
8.972758	646.671336	10.403584
8.684343	646.118660	10.408602
8.862960	646.185156	10.413619
9.265953	659.615673	10.418637
9.483664	660.028793	10.423655
8.865039	648.759007	10.428672
8.719115	646.091474	10.433690
9.114584	664.548442	10.438707
8.957816	666.202453	10.443725
8.904957	664.302459	10.448743
8.947830	681.431544	10.453760
8.981486	680.666491	10.458778
9.015350	675.125587	10.463795
9.142601	677.194365	10.468813
9.443313	666.862823	10.473831
9.207036	677.475030	10.478848
9.522833	673.597176	10.483866
9.289780	670.085131	10.488883
9.034171	671.120580	10.493901
9.176481	662.797106	10.498919
9.243579	675.718548	10.503936
9.193998	674.268761	10.508954
9.192053	670.414587	10.513971
9.109091	662.830666	10.518989
9.164397	670.043484	10.524007
9.136211	668.672419	10.529024
9.211295	668.539210	10.534042
9.381235	667.417082	10.539059
9.097334	669.581556	10.544077
9.068103	668.837781	10.549095
9.001626	669.411513	10.554112
9.006449	669.002997	10.559130
9.088356	672.231387	10.564147
8.881920	670.764564	10.569165
9.318608	664.046758	10.574183
9.089015	676.319339	10.579200
9.303626	673.782217	10.584218
9.460754	658.938477	10.589235
9.002446	671.750408	10.594253
9.187776	671.523290	10.599271
9.286847	673.597342	10.604288
9.181578	684.517479	10.609306
9.817884	679.931284	10.614323
9.060426	674.472302	10.619341
9.757677	672.486212	10.624359
9.471767	656.666585	10.629376
9.141914	658.363536	10.634394
9.662486	663.138967	10.639411
9.128887	665.137872	10.644429
9.419037	667.303185	10.649447
9.812625	678.418729	10.654464
9.473800	672.679947	10.659482
9.808989	659.812362	10.664499
9.342158	668.970874	10.669517
9.794360	661.686754	10.674535
9.864352	657.480103	10.679552
9.385433	660.101365	10.684570
9.443271	658.062313	10.689587
9.383653	654.296267	10.694605
9.474704	659.600335	10.699623
9.424307	660.022586	10.704640
9.335530	663.478147	10.709658
9.627125	659.313987	10.714675
9.369237	668.579886	10.719693
9.544552	660.907372	10.724711
9.493127	668.622143	10.729728
9.544838	657.705467	10.734746
9.676193	661.520865	10.739763
9.339967	662.996845	10.744781
9.438525	660.430396	10.749799
9.472114	670.918617	10.754816
9.619408	684.355634	10.759834
10.169844	684.984102	10.764851
9.640862	667.240841	10.769869
9.470112	667.458901	10.774887
9.377921	664.617683	10.779904
9.329884	669.748234	10.784922
9.555881	679.590355	10.789939
9.363216	689.118042	10.794957
9.317603	691.850151	10.799975
9.693028	700.854716	10.804992
10.102704	703.206059	10.810010
9.731789	690.332590	10.815027
9.686940	696.367670	10.820045
9.919401	688.132930	10.825063
10.113085	689.586186	10.830080
9.955156	682.166673	10.835098
9.959430	682.271988	10.840115
9.641521	665.232567	10.845133
9.548216	673.955799	10.850151
9.734362	677.910509	10.855168
9.794319	690.181822	10.860186
9.700524	689.771785	10.865203
9.922454	695.581434	10.870221
9.979372	690.475243	10.875239
9.844739	692.362961	10.880256
10.063008	689.062491	10.885274
9.898759	670.827534	10.890291
9.893972	668.732360	10.895309
10.107630	667.640955	10.900327
9.740960	662.991170	10.905344
9.940517	661.281095	10.910362
9.894059	659.239694	10.915379
9.769100	660.168788	10.920397
10.091631	655.329658	10.925415
9.793856	655.257043	10.930432
9.485006	666.229310	10.935450
10.258053	669.197168	10.940467
9.902831	680.654281	10.945485
9.765564	669.646574	10.950503
9.870932	681.614293	10.955520
9.787988	688.657396	10.960538
9.866629	685.365568	10.965555
9.674479	694.431200	10.970573
9.784482	696.188895	10.975591
9.745179	687.448579	10.980608
9.531981	698.456541	10.985626
9.832002	691.721874	10.990643
9.970578	691.606457	10.995661
9.790180	696.564936	11.000679
9.854083	685.017521	11.005696
9.859064	712.088209	11.010714
10.170630	718.127242	11.015731
9.955897	716.168326	11.020749
10.046062	712.301391	11.025767
10.327570	712.589548	11.030784
9.956113	724.113756	11.035802
10.023165	719.583387	11.040819
10.328339	715.236654	11.045837
10.191941	711.831951	11.050855
10.406237	706.589172	11.055872
10.176149	706.546840	11.060890
10.445769	693.943649	11.065907
10.264310	693.818437	11.070925
10.080952	685.102459	11.075943
10.223850	683.536040	11.080960
9.861663	686.431584	11.085978
10.395609	688.151096	11.090995
10.326069	681.895148	11.096013
10.384888	675.183454	11.101031
10.581891	678.936572	11.106048
9.817363	683.866159	11.111066
10.170220	679.913842	11.116083
10.184500	671.548065	11.121101
9.966295	683.451661	11.126119
10.313175	694.608638	11.131136
10.503838	712.746778	11.136154
10.441958	705.079417	11.141171
10.496936	689.850687	11.146189
10.238599	686.094434	11.151207
10.407116	680.440408	11.156224
10.253504	686.868532	11.161242
10.349954	678.894771	11.166259
10.074707	671.768363	11.171277
9.991506	694.812256	11.176295
10.501507	706.688334	11.181312
10.469925	708.233360	11.186330
10.830857	712.119070	11.191347
10.724000	696.770195	11.196365
10.238699	689.306278	11.201383
10.499365	674.657109	11.206400
10.390712	682.102287	11.211418
10.160213	679.817281	11.216435
10.639944	692.315063	11.221453
10.280172	702.064809	11.226471
10.517189	692.662075	11.231488
10.443713	712.122563	11.236506
10.508953	703.008983	11.241523
10.786979	710.167875	11.246541
10.224314	706.817684	11.251559
10.615565	704.270685	11.256576
10.693173	707.004952	11.261594
10.688156	700.159970	11.266611
10.494411	687.744618	11.271629
10.378857	698.000186	11.276647
10.727114	683.494509	11.281664
10.483831	700.260382	11.286682
10.724911	690.118052	11.291699
10.688080	681.454489	11.296717
10.272010	687.295969	11.301735
10.531235	696.814690	11.306752
10.588830	706.293509	11.311770
10.672839	706.975488	11.316787
10.704463	712.795122	11.321805
10.406167	698.852962	11.326823
10.927247	705.094354	11.331840
10.740173	706.148727	11.336858
10.487608	699.063021	11.341875
10.815892	705.899801	11.346893
10.831821	705.868936	11.351911
10.856272	702.165671	11.356928
10.621021	715.681453	11.361946
10.756648	706.334733	11.366963
10.738122	714.222786	11.371981
10.917192	707.234023	11.376999
11.198802	703.547263	11.382016
10.641885	695.946242	11.387034
10.390764	689.539383	11.392051
10.660227	694.060323	11.397069
10.579969	712.963320	11.402087
10.515934	705.056768	11.407104
10.320780	710.389723	11.412122
10.546456	710.842857	11.417139
10.668196	708.836678	11.422157
10.357225	720.153403	11.427175
10.794086	699.796015	11.432192
10.861142	720.748988	11.437210
10.867228	719.063582	11.442227
10.896802	713.650928	11.447245
10.673920	730.091615	11.452263
10.963015	729.080772	11.457280
10.941988	741.076827	11.462298
11.328347	732.244873	11.467315
10.896240	726.061176	11.472333
10.861559	721.468391	11.477351
11.039183	706.793627	11.482368
11.151144	714.189554	11.487386
10.847852	711.639497	11.492403
10.802966	699.889107	11.497421
10.783249	713.723171	11.502439
11.170090	738.250503	11.507456
11.241993	741.026667	11.512474
11.125006	725.415096	11.517491
10.963318	712.856808	11.522509
10.751228	724.095295	11.527527
11.165617	727.593609	11.532544
11.274415	729.903829	11.537562
10.969415	731.853724	11.542579
11.162193	736.594100	11.547597
11.234641	738.224390	11.552615
11.386539	735.768149	11.557632
11.200739	718.323866	11.562650
11.179001	721.519693	11.567667
11.233109	708.247048	11.572685
11.016041	715.876194	11.577703
11.094336	712.790899	11.582720
11.589442	707.413461	11.587738
11.050052	716.902934	11.592755
11.179142	703.442843	11.597773
11.067392	710.801548	11.602791
11.254293	713.294439	11.607808
11.029203	700.899836	11.612826
11.038649	710.373276	11.617843
11.149109	717.811971	11.622861
11.316957	742.802056	11.627879
11.245270	741.071705	11.632896
11.229735	742.197561	11.637914
11.459282	743.159661	11.642931
11.637683	738.779862	11.647949
11.473902	732.577350	11.652967
11.170792	714.458329	11.657984
11.278053	720.371686	11.663002
11.062198	734.129518	11.668019
11.568946	725.768861	11.673037
11.356754	741.621804	11.678055
11.298211	735.269329	11.683072
11.471705	726.216871	11.688090
11.314028	739.440667	11.693107
11.304930	741.007548	11.698125
11.339159	746.066581	11.703143
11.478643	740.116395	11.708160
11.601082	739.919808	11.713178
11.199805	740.865701	11.718195
11.598095	731.163323	11.723213
11.560173	742.631912	11.728231
11.601839	733.872798	11.733248
11.506543	737.646562	11.738266
11.246171	737.928925	11.743283
11.222497	737.048406	11.748301
11.828188	743.811932	11.753319
11.691146	739.789461	11.758336
11.480018	737.462253	11.763354
11.356813	739.873827	11.768371
11.622383	732.452989	11.773389
11.427567	741.094516	11.778407
11.298419	734.987618	11.783424
11.741779	731.232238	11.788442
11.416603	737.305068	11.793459
11.800018	729.749103	11.798477
11.685684	740.704248	11.803495
11.383980	725.551694	11.808512
11.488795	735.490168	11.813530
11.679345	733.411924	11.818547
11.857125	734.432033	11.823565
11.464958	737.186910	11.828583
11.697967	739.594195	11.833600
11.760011	735.961636	11.838618
11.832537	737.794260	11.843635
11.646380	738.414459	11.848653
11.499849	731.882529	11.853671
11.763050	735.379204	11.858688
11.792089	733.645301	11.863706
11.487907	731.804195	11.868723
11.617965	729.941108	11.873741
11.571518	735.210579	11.878759
11.725818	734.211707	11.883776
11.690600	740.628640	11.888794
11.785718	744.550862	11.893811
11.689317	741.396769	11.898829
11.909860	759.506968	11.903847
12.062943	754.617236	11.908864
11.963073	746.842594	11.913882
11.759811	747.889424	11.918899
11.948913	746.731038	11.923917
11.826146	745.611495	11.928935
11.878350	755.613644	11.933952
12.388079	751.660824	11.938970
12.098699	736.948698	11.943987
11.851109	733.793163	11.949005
11.885343	733.427785	11.954023
11.889722	727.001080	11.959040
12.144122	727.904131	11.964058
12.085046	738.289305	11.969075
12.071466	731.035722	11.974093
11.769602	730.144162	11.979111
12.008221	728.830313	11.984128
12.016746	733.328301	11.989146
11.678105	731.446863	11.994163
11.868535	737.832982	11.999181
12.169388	747.684555	12.004199
12.427042	754.172098	12.009216
12.628103	748.594718	12.014234
12.096508	736.072696	12.019251
11.776161	717.305403	12.024269
12.061818	728.516672	12.029287
12.445544	736.421337	12.034304
12.371827	726.297450	12.039322
12.120428	722.857532	12.044339
12.172940	722.836334	12.049357
12.249733	727.123579	12.054375
12.597557	726.025224	12.059392
12.296062	723.934478	12.064410
12.160737	725.592805	12.069427
12.420521	731.083010	12.074445
12.224696	716.081950	12.079463
11.936149	732.606777	12.084480
12.128850	721.852828	12.089498
11.841022	730.598188	12.094515
12.324615	719.410881	12.099533
12.335347	722.475141	12.104551
12.332156	725.287403	12.109568
12.425765	719.391303	12.114586
11.797804	734.358688	12.119603
11.958949	751.345565	12.124621
12.227046	755.070941	12.129639
12.253160	753.309375	12.134656
12.171018	755.949148	12.139674
12.710686	760.162618	12.144691
12.837933	755.231120	12.149709
12.602705	752.139664	12.154727
12.411158	757.738552	12.159744
12.832300	751.966729	12.164762
12.151089	745.342769	12.169779
12.194760	739.917920	12.174797
12.464534	749.068411	12.179815
12.258303	749.834259	12.184832
12.300630	751.225874	12.189850
12.518780	753.845261	12.194867
12.693475	748.072868	12.199885
12.807918	753.302810	12.204903
12.588549	753.900776	12.209920
12.687892	750.148637	12.214938
12.746066	755.247390	12.219955
12.609794	755.155215	12.224973
12.644760	743.166142	12.229991
12.563311	751.129431	12.235008
12.802932	746.706976	12.240026
12.088046	744.906770	12.245043
12.441174	745.647361	12.250061
12.677253	749.460335	12.255079
12.939035	759.888447	12.260096
12.755926	747.922034	12.265114
12.670927	754.891695	12.270131
12.691137	752.835067	12.275149
12.962001	750.778115	12.280167
12.825232	759.083847	12.285184
12.675801	756.943808	12.290202
12.692192	749.523239	12.295219
12.384388	763.044233	12.300237
12.861298	750.833284	12.305255
12.324639	760.640024	12.310272
12.702277	757.698063	12.315290
12.605716	762.114714	12.320307
12.302584	758.999702	12.325325
12.547654	762.569076	12.330343
12.597702	758.634394	12.335360
12.977021	763.342396	12.340378
12.595442	766.298259	12.345395
12.580832	766.022489	12.350413
13.071173	771.377151	12.355431
12.892734	770.177693	12.360448
13.061401	762.386951	12.365466
12.972708	761.570777	12.370483
12.741144	768.539806	12.375501
12.763322	763.821031	12.380519
12.649473	787.102029	12.385536
13.002452	779.149355	12.390554
12.865085	788.997417	12.395571
12.886359	795.843338	12.400589
13.186126	777.712616	12.405607
12.883476	793.619423	12.410624
13.261648	776.807862	12.415642
13.360609	788.928293	12.420659
13.198188	790.539362	12.425677
13.072391	774.575293	12.430695
13.081677	781.422610	12.435712
13.013285	771.832023	12.440730
13.179246	775.788932	12.445747
12.945068	778.114830	12.450765
13.290822	779.198355	12.455783
13.108635	774.757031	12.460800
13.057703	778.855888	12.465818
12.820164	784.682100	12.470835
13.120127	789.511954	12.475853
13.055847	783.567667	12.480871
12.844328	787.565667	12.485888
12.977391	781.787781	12.490906
13.040408	782.736423	12.495923
13.136050	780.768429	12.500941
13.069775	772.429567	12.505959
13.082823	785.686440	12.510976
13.405125	783.114868	12.515994
13.282035	785.031778	12.521011
12.902213	785.644210	12.526029
13.398277	782.328255	12.531047
12.776756	784.027833	12.536064
13.013378	790.522233	12.541082
13.162390	809.326812	12.546099
13.532182	813.178401	12.551117
13.464357	806.551277	12.556135
13.307749	807.001815	12.561152
13.628391	807.263785	12.566170
13.847939	806.495189	12.571187
13.442464	803.280848	12.576205
13.745741	799.586527	12.581223
13.367930	795.238927	12.586240
13.606492	781.590900	12.591258
13.673175	779.851719	12.596275
13.619732	782.020027	12.601293
13.671162	775.671696	12.606311
13.618911	772.211264	12.611328
13.736954	774.536096	12.616346
13.486033	770.369957	12.621363
13.469707	782.251886	12.626381
13.778624	771.924028	12.631399
13.757088	769.716277	12.636416
13.523523	774.936356	12.641434
13.621072	777.408285	12.646451
13.541161	779.853414	12.651469
13.748351	772.956594	12.656487
13.431604	774.217944	12.661504
13.701774	769.072346	12.666522
13.707308	767.586817	12.671539
13.569536	773.269483	12.676557
13.576833	771.343337	12.681575
13.439639	767.230733	12.686592
13.579436	773.871328	12.691610
13.721646	777.174948	12.696627
13.630293	782.619604	12.701645
13.741373	771.917373	12.706663
13.736294	785.556563	12.711680
13.725047	784.963522	12.716698
14.027856	788.670147	12.721715
13.468732	778.345427	12.726733
13.788828	787.401166	12.731751
13.769838	797.266760	12.736768
13.347540	809.984046	12.741786
13.625908	801.019422	12.746803
13.714956	805.855992	12.751821
13.805172	806.694216	12.756839
13.400624	801.119449	12.761856
13.978699	809.910094	12.766874
14.095491	795.014861	12.771891
13.765305	801.025757	12.776909
13.794638	806.174988	12.781927
13.824102	811.762357	12.786944
13.840349	807.745097	12.791962
13.712488	812.749602	12.796979
13.788521	803.214907	12.801997
13.939558	818.952246	12.807015
13.965315	825.696458	12.812032
14.340803	836.531088	12.817050
14.314769	812.782018	12.822067
13.863474	817.818236	12.827085
14.241093	801.529146	12.832103
13.843545	816.251437	12.837120
13.949291	807.896367	12.842138
14.418707	820.428250	12.847155
14.165050	819.449740	12.852173
14.290193	805.601069	12.857191
14.024267	811.741437	12.862208
14.077757	809.282250	12.867226
14.218760	812.185712	12.872243
14.104120	819.140448	12.877261
14.067297	829.581626	12.882279
14.424243	831.234320	12.887296
14.341610	829.838040	12.892314
14.339630	818.071964	12.897331
13.758061	816.265141	12.902349
14.174567	825.168273	12.907367
14.158977	834.342230	12.912384
14.136296	836.736520	12.917402
14.397852	835.085605	12.922419
14.335124	843.356439	12.927437
14.599530	835.476131	12.932455
14.783878	830.055033	12.937472
14.560374	833.410985	12.942490
14.610250	822.089997	12.947507
14.453116	806.131695	12.952525
14.340882	807.846817	12.957543
14.379753	796.633969	12.962560
14.359600	800.932230	12.967578
14.656036	800.596690	12.972595
14.248209	813.049977	12.977613
14.386377	815.470085	12.982631
14.458893	827.832918	12.987648
14.600605	825.519882	12.992666
14.676021	835.719786	12.997683
14.721096	831.036552	13.002701
14.589521	815.221423	13.007719
14.579634	800.778706	13.012736
14.501791	801.684821	13.017754
14.501328	802.912304	13.022771
14.499533	812.532940	13.027789
14.683887	829.404832	13.032807
14.893272	825.237561	13.037824
14.429930	814.751042	13.042842
14.634714	817.554736	13.047859
14.401596	831.973748	13.052877
14.576708	828.438508	13.057895
14.924086	829.296389	13.062912
14.749784	831.064741	13.067930
14.909316	834.251132	13.072947
14.475914	834.157557	13.077965
14.554667	829.742527	13.082983
14.960308	826.436474	13.088000
15.038200	832.564978	13.093018
15.159674	827.781848	13.098035
14.896933	832.918219	13.103053
14.768342	811.945068	13.108071
14.659825	815.676366	13.113088
14.484318	827.872562	13.118106
14.644934	834.832537	13.123123
14.791109	837.546376	13.128141
14.791558	830.383717	13.133159
14.944785	831.014436	13.138176
14.810108	837.423137	13.143194
15.087151	829.194298	13.148211
14.978801	834.584518	13.153229
14.951166	829.828532	13.158247
14.921626	842.933488	13.163264
14.928004	834.753570	13.168282
15.202353	831.244156	13.173299
15.158869	843.173555	13.178317
15.305451	835.713985	13.183335
15.166929	831.060479	13.188352
15.137714	837.939218	13.193370
15.013606	831.519850	13.198387
15.250148	832.404814	13.203405
15.113438	839.343937	13.208423
15.260663	830.589663	13.213440
15.414275	834.462622	13.218458
15.193550	824.048559	13.223475
15.079436	809.495607	13.228493
15.044047	813.939701	13.233511
15.430983	819.540882	13.238528
15.480647	820.011857	13.243546
15.421505	800.865243	13.248563
14.998172	798.895714	13.253581
14.742374	799.566267	13.258599
15.350327	810.566559	13.263616
15.017719	831.077874	13.268634
15.312295	824.640296	13.273651
15.338278	832.954250	13.278669
15.176178	837.581408	13.283687
15.129004	821.010759	13.288704
15.180346	837.099703	13.293722
15.251114	831.083547	13.298739
15.041074	836.659752	13.303757
15.225640	825.174259	13.308775
15.317249	821.353313	13.313792
15.138272	832.115934	13.318810
15.329018	821.780915	13.323827
15.387315	833.386521	13.328845
15.127458	833.196587	13.333863
15.147359	836.070184	13.338880
15.349305	852.413819	13.343898
15.639475	848.193157	13.348915
15.806204	846.210977	13.353933
15.508197	846.792096	13.358951
15.840040	844.746846	13.363968
15.581743	861.946069	13.368986
15.777191	842.894678	13.374003
15.582187	841.618248	13.379021
15.607296	845.522213	13.384039
15.570390	847.485236	13.389056
15.639056	846.884620	13.394074
16.095474	855.858296	13.399091
15.744089	844.279989	13.404109
15.390110	836.633161	13.409127
15.639912	830.172905	13.414144
15.355226	853.265483	13.419162
15.612647	857.563488	13.424179
15.905203	859.604619	13.429197
15.763428	848.091661	13.434215
16.063131	852.686161	13.439232
15.908640	856.935707	13.444250
15.797348	846.071578	13.449267
15.670714	853.993024	13.454285
15.629604	853.086658	13.459303
15.642695	856.080872	13.464320
15.585878	854.122067	13.469338
15.602750	852.024645	13.474355
15.956009	848.754852	13.479373
15.726210	847.627108	13.484391
16.069461	853.785921	13.489408
15.728350	851.493684	13.494426
15.943620	854.660186	13.499443
15.774293	852.076029	13.504461
15.700780	850.242826	13.509479
15.815119	853.402483	13.514496
15.599594	852.951456	13.519514
15.763837	861.744579	13.524531
16.037658	870.825379	13.529549
16.140554	880.490071	13.534567
16.455370	876.207041	13.539584
16.467038	871.799606	13.544602
16.342791	856.987483	13.549619
16.255902	848.019567	13.554637
15.902364	849.580719	13.559655
16.083291	845.202439	13.564672
16.062986	849.731038	13.569690
15.923959	844.568984	13.574707
16.289411	851.818718	13.579725
16.185861	860.766578	13.584743
16.510277	857.869270	13.589760
15.951996	853.582157	13.594778
16.111328	861.214754	13.599795
16.239619	863.945744	13.604813
16.097725	876.188750	13.609831
16.619631	874.833711	13.614848
16.381639	868.276966	13.619866
16.472855	873.336018	13.624883
16.693448	871.625179	13.629901
16.325223	860.708869	13.634919
16.350965	845.492915	13.639936
16.221712	844.955113	13.644954
16.569947	852.167162	13.649971
16.612222	848.539240	13.654989
16.223205	843.956102	13.660007
16.519521	846.356622	13.665024
16.243583	854.280837	13.670042
16.421894	873.302067	13.675059
16.895867	870.973562	13.680077
16.334464	864.725673	13.685095
16.908592	855.297124	13.690112
16.691259	852.166651	13.695130
16.468432	842.704043	13.700147
16.294264	845.223310	13.705165
16.160141	861.623992	13.710183
16.567435	865.058561	13.715200
16.712509	874.858749	13.720218
16.770092	868.749303	13.725235
16.694587	872.163337	13.730253
16.819811	874.443292	13.735271
16.750878	865.351918	13.740288
16.738321	869.929035	13.745306
16.679086	877.367667	13.750323
16.756221	863.298396	13.755341
16.462695	876.841719	13.760359
16.897614	866.778075	13.765376
16.673202	868.638219	13.770394
16.650922	877.434007	13.775411
16.684686	873.958665	13.780429
16.890121	883.427194	13.785447
16.632379	874.293972	13.790464
16.919514	879.453918	13.795482
16.751285	872.337580	13.800499
16.681055	865.210469	13.805517
16.484747	871.961691	13.810535
16.810511	861.924458	13.815552
16.767998	866.966367	13.820570
16.615725	874.543681	13.825587
17.300167	883.089343	13.830605
17.079802	897.933828	13.835623
16.825722	881.659100	13.840640
17.237938	886.241996	13.845658
16.835253	891.531559	13.850675
17.483784	889.491734	13.855693
17.298046	878.633658	13.860711
16.909454	866.714493	13.865728
16.900965	874.050601	13.870746
16.780431	890.250839	13.875763
17.278897	881.081684	13.880781
17.001311	892.139459	13.885799
17.289309	888.664770	13.890816
17.560714	882.929596	13.895834
17.209184	894.826382	13.900851
17.718914	885.160895	13.905869
17.437944	873.305722	13.910887
17.223255	866.167977	13.915904
17.205297	857.581488	13.920922
17.247243	861.783032	13.925939
17.358711	856.548830	13.930957
17.398409	861.288115	13.935975
17.568928	855.477206	13.940992
17.324932	857.696092	13.946010
17.205879	859.864687	13.951027
17.370952	855.613637	13.956045
17.431197	855.028198	13.961063
17.369157	854.609138	13.966080
17.093769	852.457542	13.971098
17.170417	865.572032	13.976115
17.670854	879.225113	13.981133
17.644062	899.637859	13.986151
17.273639	887.905804	13.991168
17.517108	891.045187	13.996186
17.256270	902.850925	14.001203
17.691276	879.913652	14.006221
17.743033	884.223802	14.011239
17.526493	885.944065	14.016256
17.684285	887.946186	14.021274
17.480477	894.590403	14.026291
17.652963	889.622014	14.031309
17.486452	897.106437	14.036327
17.531948	895.610120	14.041344
17.562211	887.242356	14.046362
17.367451	897.700972	14.051379
17.964783	883.389327	14.056397
17.878432	893.996841	14.061415
17.436971	888.578167	14.066432
17.914132	886.203463	14.071450
18.057201	886.299883	14.076467
18.056387	887.741000	14.081485
17.912152	883.457105	14.086503
18.032827	883.391903	14.091520
18.234322	883.856935	14.096538
17.928892	891.537661	14.101555
17.835728	872.641086	14.106573
17.463698	883.098449	14.111591
17.529547	885.173327	14.116608
18.271885	877.691485	14.121626
18.155322	882.777200	14.126643
18.039275	884.212668	14.131661
18.410781	882.934984	14.136679
18.183984	887.130418	14.141696
18.357834	880.734337	14.146714
17.800157	883.808068	14.151731
18.250678	874.961432	14.156749
18.206590	881.114560	14.161767
18.092632	889.901185	14.166784
18.096928	876.590024	14.171802
17.973428	876.256370	14.176819
18.158959	870.959856	14.181837
18.141330	884.177821	14.186855
18.113851	879.504466	14.191872
18.299174	871.337303	14.196890
18.238389	883.671158	14.201907
18.130003	878.279801	14.206925
18.240203	875.604695	14.211943
17.815681	883.392608	14.216960
18.190081	883.463570	14.221978
18.100296	891.625745	14.226995
17.991438	877.391323	14.232013
18.115331	889.654728	14.237031
18.176203	885.571767	14.242048
18.007551	885.146804	14.247066
18.098372	887.937959	14.252083
18.730729	909.774533	14.257101
18.477681	910.412351	14.262119
18.247697	920.711493	14.267136
18.683632	910.389399	14.272154
18.568026	916.892596	14.277171
18.810032	906.319290	14.282189
18.566460	884.634093	14.287207
18.391350	877.425989	14.292224
18.829871	873.062954	14.297242
18.282615	878.825725	14.302259
18.312292	871.028898	14.307277
18.450838	886.261327	14.312295
18.474709	901.279776	14.317312
18.785349	895.045981	14.322330
18.493361	901.476131	14.327347
18.674242	905.136124	14.332365
19.144740	902.666075	14.337383
18.734854	909.302820	14.342400
19.155174	902.886630	14.347418
18.759973	909.258352	14.352435
18.738488	899.961838	14.357453
18.885320	894.039111	14.362471
18.737969	898.299292	14.367488
18.853764	894.156809	14.372506
19.001201	909.621234	14.377523
18.992650	895.702387	14.382541
18.870921	888.861759	14.387559
18.940563	881.685410	14.392576
18.967249	873.959547	14.397594
18.351613	882.644915	14.402611
18.355992	888.326634	14.407629
18.781879	897.370760	14.412647
18.940285	896.850890	14.417664
18.894829	902.845995	14.422682
18.934582	911.963362	14.427699
19.161851	904.603333	14.432717
19.244103	903.811492	14.437735
18.991314	903.736713	14.442752
19.030225	902.021424	14.447770
19.015583	910.714393	14.452787
18.937557	902.017004	14.457805
19.062479	907.305489	14.462823
19.137056	906.353910	14.467840
19.205895	901.031902	14.472858
19.036759	895.286091	14.477875
19.185291	900.487584	14.482893
19.234664	910.959567	14.487911
18.906409	901.285720	14.492928
19.295420	905.031585	14.497946
19.266324	913.639562	14.502963
19.338691	924.957681	14.507981
19.865091	918.399845	14.512999
19.151113	912.632779	14.518016
19.353507	899.949262	14.523034
19.444763	898.578008	14.528051
19.517266	888.023045	14.533069
19.521324	890.367626	14.538087
19.332084	897.557814	14.543104
19.578187	890.974140	14.548122
19.589426	896.139793	14.553139
19.328684	890.908391	14.558157
19.531452	892.634550	14.563175
19.434544	896.613528	14.568192
19.643557	886.965347	14.573210
19.538274	892.164537	14.578227
19.526982	898.966904	14.583245
19.951766	906.819955	14.588263
19.536243	895.867782	14.593280
19.547091	896.844392	14.598298
19.520192	902.442737	14.603315
19.872806	908.127210	14.608333
19.687750	914.074661	14.613351
19.601214	916.995687	14.618368
19.982141	915.148359	14.623386
19.956851	913.529561	14.628403
20.013965	904.307378	14.633421
19.922209	900.161597	14.638439
19.967027	904.790602	14.643456
19.695348	890.642675	14.648474
19.826842	890.115861	14.653491
19.594868	892.915001	14.658509
19.835495	896.540261	14.663527
19.697234	907.417419	14.668544
19.827952	912.847847	14.673562
19.901559	919.737681	14.678579
19.758658	921.396500	14.683597
20.190887	918.606451	14.688615
19.888256	928.093706	14.693632
19.927984	921.318350	14.698650
19.879405	925.671957	14.703667
19.865918	932.297549	14.708685
20.300407	917.799171	14.713703
20.370253	925.608474	14.718720
20.480382	926.550083	14.723738
20.167653	921.067484	14.728755
20.160271	923.539554	14.733773
20.236204	924.676205	14.738791
19.903015	919.607612	14.743808
20.538056	917.951106	14.748826
20.302087	918.197921	14.753843
19.962125	919.887524	14.758861
20.376224	918.440957	14.763879
19.977023	917.805115	14.768896
20.033641	920.805098	14.773914
20.423970	928.291074	14.778931
20.221703	921.443741	14.783949
20.020310	916.776446	14.788967
20.052178	924.458999	14.793984
20.468386	912.808373	14.799002
20.376408	911.866760	14.804019
20.174065	927.437367	14.809037
20.509985	929.104394	14.814055
20.378158	947.119058	14.819072
20.440759	939.779689	14.824090
20.848971	941.519736	14.829107
20.846649	936.006012	14.834125
20.697906	915.289991	14.839143
20.439474	915.160641	14.844160
20.377646	913.461307	14.849178
20.585183	921.026871	14.854195
20.779282	933.977025	14.859213
21.312435	929.619899	14.864231
20.692468	926.374845	14.869248
20.436867	915.582681	14.874266
20.428838	909.159341	14.879283
20.269655	929.112664	14.884301
20.921768	929.311869	14.889319
20.995942	933.114006	14.894336
20.685214	941.166875	14.899354
20.768271	935.333073	14.904371
20.657518	947.863463	14.909389
20.794909	939.041672	14.914407
20.733947	940.490428	14.919424
20.824027	929.114061	14.924442
20.826527	940.191062	14.929459
20.974477	949.782565	14.934477
21.046217	935.286984	14.939495
20.806288	938.664979	14.944512
21.054777	938.347839	14.949530
21.449072	937.278555	14.954547
21.195472	936.516944	14.959565
21.101912	937.653815	14.964583
21.008917	937.295799	14.969600
21.248718	936.759643	14.974618
21.420121	930.571416	14.979635
21.496400	945.841025	14.984653
21.503719	937.508542	14.989671
21.473125	940.102576	14.994688
21.254528	924.858852	14.999706
21.343982	909.969823	15.004723
20.760153	917.605107	15.009741
21.021736	915.928393	15.014759
21.143491	923.787726	15.019776
21.098906	930.375181	15.024794
21.367899	934.357524	15.029811
21.111097	951.830008	15.034829
21.201365	937.300639	15.039847
21.419081	934.542303	15.044864
21.283116	935.246878	15.049882
21.403110	936.854523	15.054899
21.076708	936.474281	15.059917
21.296437	940.224277	15.064935
21.543021	944.067442	15.069952
21.010912	940.886518	15.074970
21.308144	944.141379	15.079987
21.274322	967.876054	15.085005
21.664945	961.856879	15.090023
21.300547	960.738900	15.095040
21.344579	970.383118	15.100058
21.869573	966.602896	15.105075
22.041632	968.660920	15.110093
21.917207	961.439234	15.115111
21.615564	963.690943	15.120128
21.520620	972.020544	15.125146
21.935753	956.905697	15.130163
21.679218	970.466575	15.135181
21.687394	967.846991	15.140199
21.987682	961.056262	15.145216
21.691620	970.464109	15.150234
21.929474	962.364935	15.155251
22.025838	964.089497	15.160269
21.978333	956.939669	15.165287
21.835171	956.759666	15.170304
21.765432	959.081092	15.175322
22.121313	961.416026	15.180339
22.023412	961.162756	15.185357
22.156461	955.097816	15.190375
22.032170	958.825078	15.195392
21.591816	969.237558	15.200410
21.862670	963.393398	15.205427
22.008897	967.311514	15.210445
21.853576	961.977138	15.215463
21.957060	962.153361	15.220480
21.941819	959.327053	15.225498
22.201940	958.275739	15.230515
21.592730	972.182226	15.235533
22.134973	974.448787	15.240551
22.425467	987.278247	15.245568
22.317672	989.270195	15.250586
22.711046	989.283677	15.255603
22.597529	988.156280	15.260621
22.490080	975.922995	15.265639
22.420356	958.786884	15.270656
22.411317	953.892344	15.275674
22.507710	951.430138	15.280691
22.323364	952.475018	15.285709
22.453549	954.573857	15.290727
22.402512	961.057285	15.295744
22.225873	952.018011	15.300762
22.513332	955.744549	15.305779
22.506074	972.686239	15.310797
22.820264	968.730828	15.315815
22.583718	959.013357	15.320832
22.309480	952.559052	15.325850
22.724512	954.487326	15.330867
22.779185	978.915929	15.335885
22.923982	975.761461	15.340903
22.773882	961.558224	15.345920
22.696013	956.761732	15.350938
22.759720	945.518074	15.355955
22.438339	947.403398	15.360973
22.491491	945.779827	15.365991
22.592180	957.838887	15.371008
22.806641	972.758409	15.376026
23.002476	972.250425	15.381043
23.254127	974.473558	15.386061
23.164897	964.587119	15.391079
22.837858	948.917325	15.396096
22.813085	952.250114	15.401114
22.782930	949.080244	15.406131
22.947739	967.858968	15.411149
23.406313	968.179706	15.416167
23.298419	959.487249	15.421184
22.798004	949.697898	15.426202
22.970092	942.154121	15.431219
22.893879	948.867700	15.436237
22.713467	965.617308	15.441255
23.050201	969.245508	15.446272
22.892013	982.590849	15.451290
22.898809	979.511676	15.456307
22.887896	980.006110	15.461325
22.995095	972.961263	15.466343
22.838714	966.682628	15.471360
22.464807	980.923614	15.476378
23.061064	969.540642	15.481395
23.512101	991.795636	15.486413
23.315711	998.022152	15.491431
23.599486	989.491339	15.496448
23.423874	993.550349	15.501466
23.328402	993.439187	15.506483
23.380308	985.099661	15.511501
23.226260	988.986591	15.516519
23.058552	990.947555	15.521536
23.153199	999.735002	15.526554
23.256477	993.215572	15.531571
23.153263	994.639075	15.536589
23.263417	992.039937	15.541607
23.378267	989.653000	15.546624
23.288322	1000.285592	15.551642
23.353883	1012.040708	15.556659
23.938318	1013.795960	15.561677
24.007422	1004.569756	15.566695
24.098065	993.936513	15.571712
23.799309	995.311812	15.576730
23.848566	983.340254	15.581747
23.938210	983.459333	15.586765
23.680483	983.846371	15.591783
23.921961	971.535412	15.596800
23.669187	981.942707	15.601818
24.177266	975.761887	15.606835
23.926951	975.752834	15.611853
23.812637	972.327671	15.616871
23.811769	977.993366	15.621888
23.977345	980.955568	15.626906
24.023771	977.732415	15.631923
24.010034	976.132555	15.636941
24.047690	978.869968	15.641959
24.161291	970.093449	15.646976
24.168768	977.452542	15.651994
24.131012	979.745428	15.657011
24.176849	982.195278	15.662029
23.920010	976.138836	15.667047
24.083047	978.486927	15.672064
23.955707	984.920846	15.677082
23.881329	976.107855	15.682099
24.061218	978.731476	15.687117
24.126418	979.563632	15.692135
24.027106	981.765181	15.697152
24.389332	992.973366	15.702170
24.107072	999.944035	15.707187
24.041214	1004.667445	15.712205
23.928069	1011.259637	15.717223
24.763053	1010.015536	15.722240
24.195579	1006.871970	15.727258
24.580565	1006.537260	15.732275
24.418722	1004.071118	15.737293
24.285778	1011.666546	15.742311
24.774667	1003.020931	15.747328
24.327325	1013.814896	15.752346
24.643394	1010.522118	15.757363
24.595573	1008.946817	15.762381
24.362429	1010.639540	15.767399
24.773828	1007.247065	15.772416
24.502026	1001.237191	15.777434
24.572638	1011.713980	15.782451
24.830170	1002.481655	15.787469
24.327989	1009.062132	15.792487
24.760557	1003.545390	15.797504
24.796571	1007.177520	15.802522
24.656230	1012.916406	15.807539
24.976840	1004.337340	15.812557
24.682990	1003.376520	15.817575
24.780219	995.189290	15.822592
24.888000	1005.107958	15.827610
25.136262	1004.188526	15.832627
25.015621	998.876324	15.837645
24.907284	1005.831081	15.842663
24.751698	998.981071	15.847680
24.840717	1008.332813	15.852698
24.909856	1006.383762	15.857715
25.042619	993.744022	15.862733
25.102142	998.080471	15.867751
25.043485	998.903688	15.872768
25.087100	1000.260270	15.877786
25.027507	1004.731078	15.882803
25.222282	1009.656040	15.887821
25.281343	1019.789891	15.892839
25.097763	1001.188879	15.897856
25.376900	1012.434115	15.902874
25.272587	1017.750896	15.907891
25.227407	1014.722872	15.912909
25.385686	1025.557126	15.917927
25.410483	1018.782633	15.922944
25.262264	1013.516740	15.927962
25.114252	1020.362749	15.932979
25.582302	1028.318508	15.937997
25.317820	1032.884005	15.943015
25.435566	1030.571772	15.948032
25.859417	1032.212780	15.953050
25.522279	1022.915115	15.958067
25.319353	1011.003559	15.963085
25.630524	1025.649593	15.968103
25.764526	1022.924052	15.973120
26.068966	1026.104115	15.978138
25.270857	1009.802354	15.983155
25.685263	1003.768188	15.988173
25.362467	1029.774091	15.993191
25.802953	1025.010710	15.998208
25.579221	1020.406149	16.003226
25.650109	1018.355630	16.008243
25.855597	1022.981194	16.013261
25.745186	1033.712874	16.018279
25.831234	1017.616105	16.023296
25.747072	1028.087134	16.028314
25.240915	1020.612741	16.033331
25.669706	1025.283078	16.038349
25.702752	1028.633044	16.043367
25.479563	1019.382580	16.048384
25.731480	1044.150925	16.053402
25.764706	1055.513438	16.058419
25.942521	1050.449629	16.063437
26.264470	1056.733318	16.068455
26.193198	1049.903130	16.073472
26.299237	1059.277269	16.078490
25.770194	1057.481959	16.083507
26.408841	1052.943889	16.088525
26.089534	1055.818987	16.093543
25.833579	1052.878740	16.098560
26.133132	1054.223103	16.103578
26.160708	1056.620884	16.108595
26.436053	1056.727209	16.113613
26.172697	1059.266254	16.118631
26.568798	1045.601653	16.123648
26.620569	1053.080578	16.128666
25.966006	1060.484393	16.133683
26.390218	1050.109434	16.138701
26.145911	1055.967185	16.143719
26.236795	1053.890504	16.148736
26.454923	1052.747743	16.153754
26.243427	1058.598074	16.158771
26.282911	1052.193547	16.163789
26.468893	1065.344363	16.168807
26.569856	1076.355493	16.173824
26.659774	1077.653996	16.178842
26.856585	1080.134278	16.183859
27.177140	1066.865266	16.188877
27.076006	1058.441694	16.193895
26.803202	1048.847902	16.198912
26.834898	1049.145502	16.203930
26.860665	1050.141688	16.208947
26.978026	1046.822877	16.213965
26.680652	1044.823325	16.218983
26.885784	1042.979612	16.224000
27.046534	1042.423917	16.229018
26.513536	1048.210362	16.234035
26.547589	1044.619586	16.239053
26.573268	1046.704312	16.244071
27.163435	1056.041684	16.249088
27.036665	1047.588128	16.254106
26.865975	1046.414326	16.259123
26.980658	1060.852512	16.264141
27.101886	1073.023204	16.269159
26.952375	1079.270306	16.274176
27.136118	1080.202445	16.279194
26.837066	1083.611555	16.284211
27.360634	1070.227307	16.289229
26.960035	1075.509498	16.294247
27.214092	1080.787604	16.299264
27.148598	1073.487964	16.304282
27.288822	1083.003673	16.309299
27.107212	1067.469028	16.314317
26.877738	1078.252417	16.319335
27.109603	1071.273809	16.324352
27.429168	1070.657467	16.329370
27.014472	1075.948694	16.334387
27.323235	1086.601688	16.339405
27.522838	1095.367416	16.344423
27.689014	1099.974735	16.349440
27.765945	1096.098488	16.354458
27.550716	1086.253383	16.359475
27.791737	1078.785480	16.364493
27.751970	1076.475799	16.369511
27.711875	1058.095346	16.374528
27.867194	1055.893001	16.379546
27.600358	1070.391456	16.384563
27.549895	1060.073731	16.389581
27.713498	1069.216667	16.394599
27.473792	1063.321113	16.399616
27.809594	1086.536687	16.404634
27.979604	1100.630692	16.409651
28.289694	1097.167245	16.414669
27.936949	1069.130564	16.419687
27.715879	1072.277511	16.424704
27.989967	1069.194445	16.429722
27.560390	1085.241144	16.434739
27.963349	1097.833511	16.439757
27.803886	1104.502335	16.444775
27.939796	1110.996092	16.449792
28.047049	1098.140046	16.454810
27.847089	1107.218633	16.459827
28.131295	1102.187910	16.464845
27.878403	1097.152761	16.469863
27.659358	1101.055246	16.474880
28.057074	1104.386349	16.479898
27.976421	1106.034447	16.484915
28.285569	1111.007752	16.489933
28.312148	1113.960406	16.494951
28.051292	1124.495905	16.499968
28.732524	1126.503968	16.504986
28.288490	1128.765194	16.510003
28.535818	1126.399916	16.515021
28.546663	1123.239730	16.520039
28.575258	1120.590350	16.525056
28.813640	1098.322411	16.530074
28.395215	1094.602506	16.535091
28.652620	1088.758172	16.540109
28.693379	1078.829584	16.545127
28.145163	1094.920419	16.550144
28.872439	1097.901486	16.555162
28.490683	1098.842973	16.560179
28.587765	1102.034681	16.565197
28.910986	1117.551592	16.570215
28.841775	1108.234540	16.575232
29.005073	1096.174653	16.580250
28.746458	1095.984704	16.585267
28.839171	1085.403808	16.590285
28.779071	1086.817791	16.595303
28.589734	1090.634237	16.600320
28.877354	1098.595614	16.605338
28.784225	1107.675342	16.610355
28.788896	1112.914596	16.615373
29.086315	1113.038906	16.620391
28.914578	1128.105833	16.625408
29.104359	1114.474282	16.630426
28.913154	1118.890623	16.635443
29.150856	1108.487178	16.640461
29.252244	1115.352799	16.645479
28.892601	1108.598070	16.650496
29.281739	1116.963035	16.655514
29.064965	1122.202485	16.660531
29.190900	1117.683866	16.665549
29.195048	1117.661652	16.670567
28.980314	1108.977025	16.675584
29.471215	1115.145260	16.680602
29.461240	1117.084354	16.685619
29.017598	1120.343103	16.690637
29.563567	1122.735441	16.695655
29.178950	1108.254919	16.700672
29.076492	1121.910394	16.705690
28.926005	1124.535409	16.710707
29.210806	1142.184613	16.715725
29.666777	1149.979065	16.720743
29.487046	1139.876857	16.725760
29.812713	1145.954069	16.730778
29.673719	1147.734697	16.735795
29.785626	1139.297719	16.740813
29.875538	1141.564292	16.745831
29.874821	1137.761961	16.750848
30.396889	1136.223813	16.755866
30.023379	1132.314159	16.760883
30.107496	1115.320800	16.765901
30.057612	1104.442740	16.770919
29.788967	1106.701583	16.775936
30.056796	1101.953883	16.780954
29.828652	1103.707199	16.785971
30.082688	1108.068040	16.790989
29.448748	1100.136916	16.796007
29.406670	1117.578228	16.801024
29.547939	1118.185555	16.806042
29.586744	1134.797341	16.811059
29.644742	1140.491106	16.816077
29.910485	1134.124134	16.821095
30.002593	1144.534845	16.826112
29.926276	1163.509781	16.831130
30.138662	1157.053247	16.836147
30.191584	1168.844834	16.841165
30.699144	1155.513171	16.846183
30.536605	1164.607618	16.851200
30.651114	1149.999615	16.856218
30.559004	1152.117317	16.861235
30.302173	1145.078568	16.866253
30.554957	1128.078028	16.871271
30.324592	1130.327362	16.876288
30.548820	1123.773603	16.881306
30.419975	1129.611798	16.886323
30.156800	1134.415284	16.891341
30.604805	1159.381527	16.896359
30.314104	1167.973679	16.901376
30.366895	1161.162977	16.906394
30.312535	1158.660049	16.911411
30.361892	1172.028537	16.916429
30.817460	1165.143804	16.921447
30.672613	1167.505696	16.926464
30.419543	1155.405521	16.931482
30.768475	1165.109418	16.936499
30.503186	1162.280932	16.941517
31.066883	1166.815903	16.946535
30.885707	1173.877325	16.951552
31.165359	1171.292504	16.956570
31.074353	1162.496342	16.961587
30.678759	1173.564481	16.966605
31.019821	1170.340348	16.971623
30.876268	1180.938275	16.976640
31.111428	1178.532100	16.981658
31.588904	1178.286342	16.986675
31.686748	1174.909727	16.991693
31.472643	1152.839350	16.996711
31.254932	1160.131237	17.001728
31.366802	1146.335843	17.006746
31.522423	1151.009496	17.011763
31.283957	1144.820017	17.016781
31.429720	1143.081431	17.021799
31.220507	1147.374008	17.026816
31.183801	1154.127957	17.031834
31.326699	1133.150583	17.036851
31.218183	1150.246692	17.041869
31.474331	1143.764781	17.046887
31.540905	1154.627359	17.051904
31.402096	1148.477218	17.056922
31.660973	1169.406202	17.061939
31.860403	1167.288238	17.066957
31.945136	1165.614515	17.071975
31.330693	1153.941709	17.076992
31.717883	1169.728342	17.082010
32.090331	1163.242054	17.087027
31.436762	1150.627764	17.092045
31.499691	1158.727692	17.097063
31.624387	1177.757422	17.102080
31.793492	1187.172730	17.107098
31.441895	1186.700215	17.112115
31.411445	1184.294092	17.117133
31.774767	1180.163935	17.122151
31.749389	1182.180003	17.127168
31.753475	1182.252283	17.132186
32.020789	1175.103178	17.137203
32.174265	1198.323240	17.142221
32.047900	1197.853840	17.147239
32.154879	1216.642479	17.152256
32.265089	1201.857589	17.157274
32.453553	1200.424091	17.162291
32.240831	1204.616877	17.167309
32.322806	1194.056194	17.172327
32.110729	1193.447897	17.177344
32.222333	1200.131550	17.182362
32.763370	1194.716788	17.187379
32.345869	1200.096313	17.192397
32.261538	1187.557849	17.197415
31.800345	1192.863142	17.202432
32.380221	1195.514018	17.207450
32.591298	1201.879971	17.212467
32.492763	1201.303588	17.217485
32.559537	1196.251495	17.222503
32.827737	1199.551392	17.227520
32.774245	1203.378751	17.232538
32.663579	1200.470625	17.237555
32.617230	1205.902241	17.242573
32.631380	1204.107967	17.247591
32.555087	1202.970824	17.252608
32.365573	1202.587900	17.257626
32.729822	1201.198411	17.262643
32.878946	1204.566130	17.267661
33.037749	1201.234887	17.272679
32.751057	1205.656887	17.277696
32.700480	1208.254681	17.282714
32.860695	1201.189897	17.287731
32.857143	1202.638191	17.292749
32.772552	1206.743936	17.297767
33.406638	1221.582147	17.302784
33.172354	1230.083070	17.307802
33.335232	1223.126884	17.312819
33.120425	1218.685339	17.317837
33.306927	1219.589077	17.322855
33.555453	1213.189109	17.327872
33.405391	1210.703653	17.332890
33.412975	1193.685923	17.337907
33.907657	1198.288672	17.342925
33.363634	1181.872847	17.347943
33.212248	1196.051457	17.352960
33.311387	1190.713290	17.357978
33.646087	1187.894918	17.362995
33.187697	1190.540017	17.368013
33.458228	1186.486695	17.373031
33.495596	1198.904091	17.378048
33.572733	1211.288904	17.383066
33.827580	1212.518669	17.388083
33.489367	1224.581596	17.393101
33.574896	1216.922944	17.398119
33.837432	1213.511468	17.403136
33.295769	1218.056553	17.408154
33.670949	1215.084210	17.413171
33.379830	1221.434429	17.418189
33.589816	1221.806726	17.423207
33.557925	1219.352414	17.428224
33.430984	1221.028295	17.433242
33.648382	1231.520599	17.438259
33.778588	1241.247117	17.443277
33.907160	1254.724159	17.448295
34.348716	1243.910380	17.453312
34.169985	1243.437871	17.458330
34.511684	1234.160713	17.463347
34.404254	1241.004798	17.468365
34.663536	1239.659129	17.473383
34.582328	1234.814682	17.478400
34.193915	1233.396354	17.483418
34.617887	1232.338262	17.488435
34.171726	1224.736085	17.493453
34.204950	1217.303046	17.498471
34.968137	1222.950501	17.503488
34.648232	1227.344957	17.508506
34.546683	1209.983944	17.513523
34.266919	1205.180774	17.518541
34.398362	1195.190584	17.523559
34.358422	1209.711299	17.528576
34.097760	1234.277751	17.533594
34.425096	1232.740464	17.538611
34.556136	1240.886200	17.543629
34.093114	1243.217917	17.548647
34.668424	1232.086652	17.553664
34.437364	1238.249343	17.558682
34.777219	1230.172052	17.563699
34.487621	1234.532734	17.568717
34.617334	1261.259062	17.573735
35.133247	1262.695038	17.578752
35.035434	1274.406644	17.583770
35.211217	1267.655765	17.588787
35.135380	1261.682508	17.593805
34.978340	1257.977385	17.598823
35.470300	1254.921455	17.603840
35.318154	1243.801642	17.608858
35.445103	1225.007022	17.613875
35.431501	1233.715747	17.618893
35.251788	1223.257984	17.623911
35.175921	1227.208354	17.628928
35.133079	1225.732592	17.633946
35.085483	1225.404817	17.638963
34.955922	1235.510713	17.643981
35.078571	1245.535722	17.648999
35.427859	1255.033719	17.654016
35.194236	1259.978783	17.659034
35.304750	1255.890230	17.664051
35.402575	1258.279910	17.669069
35.437952	1255.233726	17.674087
35.821489	1261.592694	17.679104
35.362046	1260.726305	17.684122
35.663735	1256.946909	17.689139
35.802105	1260.042422	17.694157
35.649783	1256.516823	17.699175
35.551535	1249.131209	17.704192
35.894325	1257.642138	17.709210
35.807725	1248.857398	17.714227
35.751694	1246.333081	17.719245
35.901509	1249.931787	17.724263
35.724019	1257.773706	17.729280
35.883991	1266.056766	17.734298
36.044953	1277.302941	17.739315
36.100616	1275.384441	17.744333
36.366488	1283.496373	17.749351
36.319971	1271.654285	17.754368
35.905401	1264.614926	17.759386
36.436709	1272.683917	17.764403
36.113124	1284.562577	17.769421
36.123335	1277.266006	17.774439
36.597037	1276.067761	17.779456
36.368519	1278.055007	17.784474
36.293486	1275.642500	17.789491
36.505719	1276.122690	17.794509
36.586677	1280.171808	17.799527
36.614493	1264.044698	17.804544
36.635190	1276.230290	17.809562
36.721600	1276.481007	17.814579
37.052645	1272.837668	17.819597
36.757810	1255.174096	17.824615
36.525132	1239.884763	17.829632
36.482537	1240.264002	17.834650
36.808293	1250.050542	17.839667
36.732571	1260.471508	17.844685
36.802479	1275.527156	17.849703
36.604508	1270.107245	17.854720
36.571443	1277.396843	17.859738
36.993039	1269.112647	17.864755
36.734429	1273.039072	17.869773
36.777074	1269.814518	17.874791
37.043507	1265.924449	17.879808
36.855207	1271.661953	17.884826
36.783883	1260.442871	17.889843
36.787093	1271.083788	17.894861
36.718497	1264.015667	17.899879
36.853792	1278.464016	17.904896
37.071502	1298.050068	17.909914
37.442024	1295.137144	17.914931
37.468687	1293.823440	17.919949
37.730177	1299.653515	17.924967
37.637576	1307.290018	17.929984
37.354532	1291.515322	17.935002
37.823036	1298.835738	17.940019
37.901016	1269.477938	17.945037
37.243833	1259.436106	17.950055
37.598348	1257.834066	17.955072
37.509501	1258.507596	17.960090
37.395153	1264.041869	17.965107
38.213660	1270.334848	17.970125
37.870416	1275.030429	17.975143
37.654727	1268.732000	17.980160
37.571238	1266.703169	17.985178
37.467020	1275.370681	17.990195
37.808651	1289.467043	17.995213
37.721623	1298.855307	18.000231
37.975924	1297.734863	18.005248
37.746707	1295.362545	18.010266
37.383004	1298.555289	18.015283
37.773663	1295.406350	18.020301
37.814631	1298.547192	18.025319
37.878897	1284.870212	18.030336
37.904465	1302.420958	18.035354
37.934036	1311.678438	18.040371
38.126018	1319.581417	18.045389
38.140319	1317.559160	18.050407
38.020686	1318.673227	18.055424
37.921959	1316.471338	18.060442
38.039442	1313.296146	18.065459
38.379542	1311.552013	18.070477
38.003183	1309.382094	18.075495
38.504612	1315.891564	18.080512
38.193498	1332.129451	18.085530
38.962568	1327.935363	18.090547
39.109899	1332.114403	18.095565
39.020148	1326.508775	18.100583
39.234840	1307.016425	18.105600
39.165989	1296.828365	18.110618
39.032431	1293.866547	18.115635
39.259269	1289.747235	18.120653
38.982103	1297.884076	18.125671
38.876899	1296.254111	18.130688
38.837495	1286.380836	18.135706
38.893472	1293.867447	18.140723
39.205219	1289.197822	18.145741
38.823270	1296.132043	18.150759
39.168692	1293.017000	18.155776
38.861642	1292.263465	18.160794
38.733540	1294.098596	18.165811
38.960150	1286.819596	18.170829
38.768272	1302.116803	18.175847
39.132834	1308.560043	18.180864
39.326997	1325.907211	18.185882
39.482727	1322.141035	18.190899
40.008141	1323.863225	18.195917
39.507607	1313.859100	18.200935
39.429525	1288.979405	18.205952
39.467079	1291.558629	18.210970
39.477035	1300.581182	18.215987
39.483758	1305.579618	18.221005
39.617961	1329.333771	18.226023
39.530401	1321.362901	18.231040
39.439033	1322.986032	18.236058
39.510842	1327.196520	18.241075
39.657007	1327.728241	18.246093
39.459923	1323.188448	18.251111
39.905604	1314.750623	18.256128
39.575721	1311.942293	18.261146
39.799488	1315.028349	18.266163
40.006403	1304.133451	18.271181
39.840379	1308.935804	18.276199
40.052472	1315.687842	18.281216
40.170970	1317.031220	18.286234
40.147803	1314.421117	18.291251
40.013858	1313.636842	18.296269
39.909211	1320.722224	18.301287
40.228495	1334.269604	18.306304
40.497728	1344.945884	18.311322
40.046986	1337.249533	18.316339
40.376346	1339.356659	18.321357
40.273881	1342.497727	18.326375
40.182976	1355.527493	18.331392
40.510855	1343.944374	18.336410
40.287499	1344.795770	18.341427
40.453152	1346.072654	18.346445
40.149288	1352.595510	18.351463
40.113939	1347.093034	18.356480
40.394626	1347.743338	18.361498
40.239073	1361.216516	18.366515
40.752609	1373.608849	18.371533
40.752491	1376.864012	18.376551
40.769954	1376.425030	18.381568
41.189200	1371.397762	18.386586
41.232478	1371.359989	18.391603
41.242647	1370.818680	18.396621
41.282472	1359.122406	18.401639
41.446713	1353.299364	18.406656
41.423538	1338.909728	18.411674
40.954020	1334.803779	18.416691
41.180827	1331.691119	18.421709
41.094238	1335.314177	18.426727
41.105573	1331.094848	18.431744
41.209144	1332.113160	18.436762
41.068993	1347.103793	18.441779
41.506759	1357.674514	18.446797
41.363427	1364.738394	18.451815
41.501913	1372.445180	18.456832
41.486415	1366.500435	18.461850
41.372358	1369.039911	18.466867
41.388645	1366.238996	18.471885
41.551298	1367.283710	18.476903
41.428506	1364.257887	18.481920
41.979018	1364.924763	18.486938
41.567631	1360.050903	18.491955
41.513478	1359.776969	18.496973
41.535851	1368.468768	18.501991
41.445842	1364.844602	18.507008
41.639703	1362.260624	18.512026
41.885067	1380.424907	18.517043
41.845065	1382.291468	18.522061
42.165133	1379.362112	18.527079
42.287831	1389.321855	18.532096
42.071967	1380.729778	18.537114
42.116218	1381.764645	18.542131
42.221835	1377.453652	18.547149
42.313842	1386.117353	18.552167
42.390914	1388.728213	18.557184
42.462062	1385.339454	18.562202
42.162973	1384.621991	18.567219
42.212327	1382.069507	18.572237
42.429511	1390.353756	18.577255
42.553753	1386.503037	18.582272
42.412579	1391.570174	18.587290
42.165740	1388.164581	18.592307
42.278545	1393.356038	18.597325
42.368457	1386.074122	18.602343
42.460482	1383.875164	18.607360
42.785504	1382.681545	18.612378
42.694820	1386.771028	18.617395
42.745262	1375.559970	18.622413
42.789863	1382.119803	18.627431
42.799324	1379.466079	18.632448
42.704957	1382.125903	18.637466
42.518608	1387.446209	18.642483
43.037665	1409.328704	18.647501
42.965163	1406.264987	18.652519
42.985700	1410.409612	18.657536
43.350820	1400.405649	18.662554
43.038991	1413.890673	18.667571
43.283618	1399.078137	18.672589
43.280306	1412.590228	18.677607
43.067271	1412.137981	18.682624
43.611173	1407.532096	18.687642
43.507141	1406.671981	18.692659
43.539786	1402.350275	18.697677
43.581995	1398.832862	18.702695
43.102955	1402.452265	18.707712
43.182624	1396.668851	18.712730
43.010243	1399.626281	18.717747
43.175747	1404.955436	18.722765
43.043512	1425.476556	18.727783
43.397009	1433.721245	18.732800
43.552122	1433.126711	18.737818
43.803916	1434.543612	18.742835
43.985744	1432.667902	18.747853
43.656424	1419.754623	18.752871
43.518828	1432.783159	18.757888
43.865143	1440.757398	18.762906
44.223000	1441.761014	18.767923
44.311107	1450.916725	18.772941
44.555912	1437.751323	18.777959
44.406825	1435.684554	18.782976
44.504214	1410.382992	18.787994
44.526535	1411.188048	18.793011
44.520552	1407.395973	18.798029
44.525016	1410.719672	18.803047
44.236584	1411.057098	18.808064
44.603571	1396.635240	18.813082
44.445381	1404.857084	18.818099
44.561708	1402.165910	18.823117
44.788214	1411.626933	18.828135
44.575307	1412.252192	18.833152
44.871024	1406.073430	18.838170
44.694636	1411.594839	18.843187
44.474416	1408.959597	18.848205
44.584418	1408.204850	18.853223
44.733398	1405.112985	18.858240
44.830955	1403.776466	18.863258
44.801347	1430.681530	18.868275
44.768144	1436.584257	18.873293
45.136322	1436.610987	18.878311
44.991511	1440.812233	18.883328
45.314212	1439.957175	18.888346
45.488211	1439.750043	18.893363
45.611047	1433.570870	18.898381
45.164333	1410.827778	18.903399
44.965756	1410.771541	18.908416
45.364528	1422.123175	18.913434
45.398757	1430.061092	18.918451
45.318300	1436.179934	18.923469
45.250480	1431.118639	18.928487
45.241210	1437.724062	18.933504
45.408214	1433.456000	18.938522
45.284958	1438.458366	18.943539
45.550304	1434.003491	18.948557
45.445971	1426.586520	18.953575
45.461478	1430.704821	18.958592
45.449989	1431.113146	18.963610
45.481339	1438.631085	18.968627
45.592621	1450.596647	18.973645
45.677356	1458.489177	18.978663
45.629692	1456.984667	18.983680
45.866819	1462.783029	18.988698
45.872648	1459.577152	18.993715
45.583207	1457.299067	18.998733
45.928642	1456.415822	19.003751
45.968800	1462.062278	19.008768
46.227275	1456.866432	19.013786
45.960891	1468.725882	19.018803
46.110990	1476.687871	19.023821
46.786663	1474.800157	19.028839
46.324757	1485.586631	19.033856
46.343140	1491.083965	19.038874
46.544996	1485.635321	19.043891
46.553452	1481.316038	19.048909
46.630170	1483.193527	19.053927
46.419782	1486.690347	19.058944
46.972969	1477.912135	19.063962
46.898704	1483.888632	19.068979
46.649549	1483.345144	19.073997
46.943702	1476.993783	19.079015
47.080696	1486.648071	19.084032
47.066965	1471.333930	19.089050
46.981238	1477.468625	19.094067
46.874531	1476.514857	19.099085
46.872872	1464.897444	19.104103
46.643499	1476.446033	19.109120
46.898031	1482.961176	19.114138
47.113323	1483.924711	19.119155
46.893013	1478.872602	19.124173
47.068360	1473.757100	19.129191
46.921014	1482.752360	19.134208
47.303452	1489.860801	19.139226
47.451871	1497.821112	19.144243
47.160702	1505.803699	19.149261
47.006516	1503.174789	19.154279
47.456843	1509.715276	19.159296
47.554532	1509.135401	19.164314
47.671236	1498.546298	19.169331
47.213312	1503.296833	19.174349
47.541767	1503.608899	19.179367
47.903958	1521.320477	19.184384
47.767293	1522.416917	19.189402
48.135304	1522.388165	19.194419
48.021672	1527.464155	19.199437
48.238020	1500.379327	19.204455
48.046002	1501.215286	19.209472
47.993087	1503.523761	19.214490
48.108476	1498.433570	19.219507
48.276052	1510.192976	19.224525
48.390005	1512.058768	19.229543
48.369225	1507.423479	19.234560
48.489239	1502.654951	19.239578
48.441651	1494.023426	19.244595
48.332127	1498.611728	19.249613
48.305285	1489.776368	19.254631
48.276268	1505.269537	19.259648
48.469431	1519.051030	19.264666
48.954556	1522.584624	19.269683
48.556875	1529.105037	19.274701
48.915314	1522.231174	19.279719
48.860557	1522.549844	19.284736
48.726955	1509.125626	19.289754
48.951660	1506.664841	19.294771
48.608816	1512.953304	19.299789
49.108265	1509.125233	19.304807
48.883438	1528.120575	19.309824
48.977827	1523.300789	19.314842
48.972281	1520.440877	19.319859
48.702255	1533.032068	19.324877
48.778756	1515.163178	19.329895
49.104520	1516.688263	19.334912
49.053307	1516.099278	19.339930
49.494154	1511.516003	19.344947
48.715084	1507.307520	19.349965
49.269502	1513.564573	19.354983
49.371282	1524.634548	19.360000
49.211661	1543.621827	19.365018
49.686508	1537.556940	19.370035
49.628387	1537.235632	19.375053
49.706972	1536.285711	19.380071
49.434042	1538.935869	19.385088
49.712362	1532.998132	19.390106
50.055980	1536.793039	19.395123
49.770731	1540.260581	19.400141
49.792407	1540.768907	19.405159
49.843834	1534.759432	19.410176
49.576650	1538.899942	19.415194
49.826775	1541.903712	19.420211
49.916921	1537.776739	19.425229
49.726249	1536.569999	19.430247
49.779686	1557.151772	19.435264
49.983166	1563.270718	19.440282
50.337531	1559.704933	19.445299
50.161565	1565.852298	19.450317
50.283064	1561.067364	19.455335
50.249397	1556.200347	19.460352
50.034535	1563.599821	19.465370
50.448925	1566.922352	19.470387
50.712131	1579.744637	19.475405
50.868490	1581.415598	19.480423
50.480848	1576.540871	19.485440
50.928560	1579.727554	19.490458
51.297596	1574.332983	19.495475
50.609097	1569.276374	19.500493
50.879074	1558.455068	19.505511
51.070680	1572.686858	19.510528
50.867985	1581.090204	19.515546
51.163929	1576.497529	19.520563
51.119057	1580.001901	19.525581
51.161794	1576.325702	19.530599
51.059900	1576.997870	19.535616
50.663569	1576.684740	19.540634
51.204149	1576.512349	19.545651
51.096358	1585.801090	19.550669
51.342155	1581.980514	19.555687
51.113182	1583.353318	19.560704
51.259645	1580.897651	19.565722
51.744856	1599.928221	19.570739
51.452879	1601.794954	19.575757
51.944181	1600.444946	19.580775
51.866995	1597.141817	19.585792
51.643107	1588.897408	19.590810
51.967191	1592.657780	19.595827
51.308858	1596.384188	19.600845
51.809088	1609.231671	19.605863
52.037646	1611.773693	19.610880
51.746998	1615.450808	19.615898
51.966991	1608.981012	19.620915
52.147565	1609.656236	19.625933
51.972723	1606.449648	19.630951
52.423947	1602.090603	19.635968
52.319598	1600.745104	19.640986
52.345400	1599.782298	19.646003
52.130130	1605.885031	19.651021
52.329548	1602.228848	19.656039
52.457264	1603.004193	19.661056
52.458542	1608.286304	19.666074
52.439089	1601.639775	19.671091
52.507759	1603.923334	19.676109
52.431414	1601.894845	19.681127
52.663313	1595.871888	19.686144
52.608177	1612.059650	19.691162
52.725563	1612.233967	19.696179
52.890582	1626.599357	19.701197
53.099056	1618.145282	19.706215
53.240902	1618.227346	19.711232
52.915834	1628.798660	19.716250
53.293105	1623.679864	19.721267
53.487148	1619.884021	19.726285
53.077521	1608.476427	19.731303
53.314219	1619.720894	19.736320
53.321553	1613.278960	19.741338
53.590142	1613.491138	19.746355
53.186099	1619.753987	19.751373
53.389563	1618.255363	19.756391
53.467093	1616.993018	19.761408
53.514059	1617.107780	19.766426
53.555781	1612.101053	19.771443
53.349962	1613.760558	19.776461
53.060205	1612.259654	19.781479
53.383336	1613.645032	19.786496
53.037156	1629.115841	19.791514
53.507916	1644.237509	19.796531
53.558081	1651.296525	19.801549
53.358729	1655.904526	19.806567
53.610395	1654.669536	19.811584
53.836988	1680.269872	19.816602
54.029396	1671.940091	19.821619
54.192320	1671.317085	19.826637
54.000807	1673.289963	19.831655
54.585524	1662.029273	19.836672
54.401209	1665.204875	19.841690
54.808928	1656.342474	19.846707
54.848021	1667.111162	19.851725
54.599474	1670.727356	19.856743
54.991109	1658.509401	19.861760
54.734260	1660.363609	19.866778
54.680587	1656.168775	19.871795
54.705727	1659.396966	19.876813
54.780565	1666.995582	19.881831
54.655881	1659.490938	19.886848
54.905843	1661.160130	19.891866
54.997352	1651.466438	19.896883
54.962477	1660.855702	19.901901
55.088500	1658.144369	19.906919
54.809433	1647.453226	19.911936
54.770270	1663.021466	19.916954
55.134188	1656.468677	19.921971
54.854178	1668.558100	19.926989
55.042493	1689.696760	19.932007
55.057741	1685.605029	19.937024
54.848145	1700.633135	19.942042
55.461922	1687.412500	19.947059
55.550361	1684.602292	19.952077
55.628629	1694.653079	19.957095
55.582406	1690.005428	19.962112
55.373224	1691.020231	19.967130
55.796943	1684.369698	19.972147
55.720989	1691.625675	19.977165
55.963638	1701.508598	19.982183
56.242451	1705.356443	19.987200
55.908398	1701.489294	19.992218
56.263685	1695.590672	19.997235
56.139980	1698.711720	20.002253
56.465531	1688.789739	20.007271
56.529416	1681.115951	20.012288
56.481583	1677.314625	20.017306
56.522688	1666.232466	20.022323
56.216818	1668.740090	20.027341
56.326522	1664.305112	20.032359
56.466108	1664.309206	20.037376
56.382746	1670.360120	20.042394
56.524143	1681.961413	20.047411
56.652627	1687.632248	20.052429
56.701951	1702.976769	20.057447
56.826171	1693.437849	20.062464
56.742978	1696.045869	20.067482
56.936318	1697.463849	20.072499
56.859535	1702.469600	20.077517
56.706176	1700.805469	20.082535
56.906233	1693.957459	20.087552
57.044548	1699.074702	20.092570
57.061886	1692.453909	20.097587
57.066159	1692.242305	20.102605
57.002950	1694.528110	20.107623
57.364838	1691.060651	20.112640
57.446446	1699.876255	20.117658
57.429581	1716.395557	20.122675
57.513557	1720.985623	20.127693
57.579401	1721.817320	20.132711
58.015404	1718.234782	20.137728
57.981750	1727.049086	20.142746
57.551319	1710.496099	20.147763
57.626591	1705.329043	20.152781
57.521225	1720.179611	20.157799
58.022773	1714.485412	20.162816
57.639044	1725.967320	20.167834
57.849804	1727.442644	20.172851
58.074986	1711.849190	20.177869
58.219335	1720.254777	20.182887
58.162867	1708.500621	20.187904
58.125584	1709.428983	20.192922
58.268692	1710.472246	20.197939
58.243343	1710.844693	20.202957
57.998594	1724.314900	20.207975
58.634729	1731.413967	20.212992
58.625035	1742.804591	20.218010
58.406653	1741.500866	20.223027
58.547024	1736.811953	20.228045
58.428610	1751.034409	20.233063
58.811913	1742.850421	20.238080
58.613884	1755.962499	20.243098
58.452332	1738.982909	20.248115
58.465022	1741.953739	20.253133
58.650304	1753.670625	20.258151
59.203365	1766.496075	20.263168
59.575100	1764.367900	20.268186
59.332288	1772.031958	20.273203
59.470346	1764.475722	20.278221
59.121009	1747.107649	20.283239
59.330352	1754.876472	20.288256
59.536109	1763.936439	20.293274
59.577369	1756.126217	20.298291
59.528131	1752.858172	20.303309
59.684501	1764.403889	20.308327
59.932802	1759.357271	20.313344
59.701789	1750.100580	20.318362
59.436271	1745.638176	20.323379
59.896950	1744.192066	20.328397
59.755353	1760.396321	20.333415
59.949109	1752.264697	20.338432
59.513966	1764.515802	20.343450
59.784525	1751.559239	20.348467
59.985399	1753.358253	20.353485
59.695034	1765.508133	20.358503
59.617599	1759.709357	20.363520
59.906308	1784.902695	20.368538
59.997503	1786.525454	20.373555
60.022007	1778.607771	20.378573
60.183755	1788.060496	20.383591
60.366134	1780.915782	20.388608
60.200513	1784.440268	20.393626
60.941687	1806.089958	20.398643
61.033229	1790.614305	20.403661
61.122383	1795.966521	20.408679
60.637772	1786.918884	20.413696
60.553448	1787.732234	20.418714
60.857089	1809.744407	20.423731
61.173532	1799.614028	20.428749
61.302867	1800.814310	20.433767
61.409907	1795.639976	20.438784
61.840808	1796.614943	20.443802
61.489907	1791.167901	20.448819
61.709000	1769.509289	20.453837
61.249117	1765.379179	20.458855
61.291214	1769.367168	20.463872
61.423513	1765.758322	20.468890
61.362406	1773.142971	20.473907
61.680341	1780.511873	20.478925
61.487194	1794.507420	20.483943
61.833408	1795.042526	20.488960
61.892484	1797.527707	20.493978
61.660829	1802.305292	20.498995
62.182580	1794.064411	20.504013
61.780114	1794.083395	20.509031
62.158539	1798.719036	20.514048
62.153398	1788.232269	20.519066
61.701364	1802.483446	20.524083
61.772441	1792.519440	20.529101
62.159914	1804.161817	20.534119
61.923327	1819.917356	20.539136
62.548817	1818.946210	20.544154
62.259554	1829.420371	20.549171
62.516839	1819.372251	20.554189
62.395388	1832.774423	20.559207
62.303009	1812.009247	20.564224
62.312188	1828.267255	20.569242
62.189002	1828.364627	20.574259
62.089444	1841.103325	20.579277
62.843695	1846.139906	20.584295
62.751193	1838.626283	20.589312
62.886919	1851.497934	20.594330
62.940243	1838.158899	20.599347
63.377209	1843.972619	20.604365
62.866186	1843.380904	20.609383
63.124343	1858.784181	20.614400
63.391161	1861.065555	20.619418
63.240233	1874.511244	20.624435
63.378684	1855.527728	20.629453
63.739020	1862.081355	20.634471
63.884761	1862.011198	20.639488
64.182949	1857.237754	20.644506
63.697985	1857.634227	20.649523
63.928040	1858.251633	20.654541
64.089676	1858.001670	20.659559
63.787854	1851.168497	20.664576
63.784309	1834.440100	20.669594
63.745895	1847.596201	20.674611
63.919910	1852.809531	20.679629
63.532375	1856.013827	20.684647
63.803595	1856.407068	20.689664
63.908241	1859.642166	20.694682
63.896935	1878.892607	20.699699
64.253594	1877.633459	20.704717
64.505217	1887.959893	20.709735
64.288040	1887.368948	20.714752
65.055627	1892.610415	20.719770
64.601831	1891.353675	20.724787
64.916794	1885.069164	20.729805
64.683467	1885.042714	20.734823
64.641062	1887.354618	20.739840
64.730645	1880.587092	20.744858
64.667206	1879.074532	20.749875
64.676996	1883.252566	20.754893
65.077472	1907.709813	20.759911
65.409474	1910.030362	20.764928
65.736317	1911.244285	20.769946
65.692752	1916.268992	20.774963
65.699823	1900.347031	20.779981
65.533531	1886.075947	20.784999
65.225490	1878.462692	20.790016
65.536597	1884.396556	20.795034
65.526276	1905.024034	20.800051
65.955768	1915.160689	20.805069
66.118928	1913.240781	20.810087
65.556006	1913.508479	20.815104
65.678358	1911.908740	20.820122
65.413765	1915.272537	20.825139
65.816257	1910.545916	20.830157
65.698759	1916.999451	20.835175
65.728715	1919.945005	20.840192
66.007568	1927.262991	20.845210
65.838831	1941.236503	20.850227
66.389085	1941.140458	20.855245
66.212766	1936.006477	20.860263
66.065967	1941.917645	20.865280
66.656110	1936.838962	20.870298
66.518141	1944.669933	20.875315
66.588031	1949.256896	20.880333
66.588454	1959.660165	20.885351
66.595479	1960.698502	20.890368
67.401481	1954.283143	20.895386
67.169142	1958.810888	20.900403
67.171780	1966.814960	20.905421
67.261147	1954.001335	20.910439
67.340561	1956.907574	20.915456
67.849403	1946.579769	20.920474
67.496123	1948.544132	20.925491
67.403664	1925.026047	20.930509
67.538828	1922.501733	20.935527
67.315707	1930.272045	20.940544
67.738751	1928.831781	20.945562
67.618044	1948.432382	20.950579
67.495566	1945.857181	20.955597
68.022274	1948.619396	20.960615
67.642666	1940.116817	20.965632
67.556655	1945.711584	20.970650
67.786904	1949.549845	20.975667
67.818374	1942.871085	20.980685
68.053320	1942.460904	20.985703
68.002624	1940.122201	20.990720
68.106792	1927.832125	20.995738
67.911366	1943.039607	21.000755
67.973200	1946.765698	21.005773
68.008768	1957.462734	21.010791
68.105011	1970.884357	21.015808
68.613122	1975.053614	21.020826
68.012047	1976.704435	21.025843
68.124066	1980.246603	21.030861
68.331069	1984.247005	21.035879
68.491508	2005.577345	21.040896
68.899339	1999.463971	21.045914
68.968513	1996.213204	21.050931
69.104236	1996.349832	21.055949
69.111372	1994.988132	21.060967
68.927955	1997.098288	21.065984
68.998766	1985.948365	21.071002
68.886572	1990.736862	21.076019
69.195357	2006.573214	21.081037
69.503723	2019.859232	21.086055
69.428372	2018.225016	21.091072
69.428463	2017.339293	21.096090
69.452114	2030.156490	21.101107
69.482701	2026.729057	21.106125
69.739438	2019.438803	21.111143
69.576727	2018.859667	21.116160
69.737425	2015.256674	21.121178
69.688913	2028.095312	21.126195
69.778378	2039.995270	21.131213
70.072742	2033.701525	21.136231
70.057230	2039.884615	21.141248
70.786896	2035.054763	21.146266
70.848415	2034.479306	21.151283
70.384881	2027.875295	21.156301
70.528171	2024.833072	21.161319
70.907890	2035.188318	21.166336
71.084580	2027.436162	21.171354
70.799285	2026.139594	21.176371
70.978563	2025.939847	21.181389
70.932563	2019.992046	21.186407
70.650929	2038.964380	21.191424
71.024159	2028.873629	21.196442
71.005341	2030.503280	21.201459
71.018921	2025.433773	21.206477
70.859532	2033.841583	21.211495
70.836336	2034.138089	21.216512
71.264810	2031.814621	21.221530
71.102758	2035.969679	21.226547
71.454120	2059.651462	21.231565
71.636305	2065.247763	21.236583
71.251215	2065.358347	21.241600
71.106051	2060.179776	21.246618
71.331733	2059.471916	21.251635
71.395003	2068.991181	21.256653
71.360419	2082.079914	21.261671
71.574948	2095.082374	21.266688
71.763070	2082.440817	21.271706
72.139767	2090.047350	21.276723
72.259939	2088.570792	21.281741
72.475784	2082.051883	21.286759
72.039018	2091.294022	21.291776
72.814231	2090.454676	21.296794
72.393385	2087.366824	21.301811
72.565700	2083.378021	21.306829
72.777363	2074.909783	21.311847
72.443257	2077.766263	21.316864
72.563139	2099.996006	21.321882
73.180283	2104.398757	21.326899
73.486615	2113.128430	21.331917
73.380329	2085.056028	21.336935
73.222005	2076.549276	21.341952
73.255318	2073.135947	21.346970
73.411985	2072.777750	21.351987
73.565389	2068.757841	21.357005
73.287600	2069.150596	21.362023
73.430557	2070.441944	21.367040
73.240725	2065.691273	21.372058
73.454425	2064.336183	21.377075
73.283964	2070.074165	21.382093
73.701773	2083.283387	21.387111
73.644799	2097.146731	21.392128
73.529567	2100.797561	21.397146
73.644991	2100.142276	21.402163
73.300928	2105.333522	21.407181
73.717755	2096.444556	21.412199
73.726149	2111.024618	21.417216
73.776310	2110.768374	21.422234
73.857426	2120.661877	21.427251
73.992905	2134.240115	21.432269
73.908406	2125.109246	21.437287
74.131615	2142.814322	21.442304
74.202556	2155.056430	21.447322
74.690395	2152.041177	21.452339
74.517534	2159.183553	21.457357
74.682872	2155.888818	21.462375
74.570442	2159.753767	21.467392
74.770917	2151.348372	21.472410
75.108567	2166.176528	21.477427
75.044215	2183.887314	21.482445
75.375085	2173.292476	21.487463
75.249871	2184.734119	21.492480
75.615771	2175.564195	21.497498
75.856311	2182.950090	21.502515
75.985882	2168.830368	21.507533
75.895837	2150.251008	21.512551
75.351346	2135.292140	21.517568
75.493592	2143.082153	21.522586
75.944862	2159.783976	21.527603
75.929774	2176.477492	21.532621
76.092144	2164.614179	21.537639
76.124497	2179.228907	21.542656
76.119275	2182.568554	21.547674
76.066329	2184.591696	21.552691
75.690771	2172.476037	21.557709
76.336423	2174.499221	21.562727
75.927871	2165.520610	21.567744
76.100613	2169.178322	21.572762
76.477628	2175.679705	21.577779
76.255327	2201.313773	21.582797
76.535117	2198.951997	21.587815
76.514237	2205.298254	21.592832
76.003208	2207.205397	21.597850
76.596181	2207.773135	21.602867
76.509852	2231.054288	21.607885
76.566077	2229.578501	21.612903
77.072023	2223.681417	21.617920
77.073778	2231.111349	21.622938
77.389624	2220.018177	21.627955
77.525041	2222.858464	21.632973
77.798469	2223.127332	21.637991
77.579950	2218.168384	21.643008
77.739235	2219.587349	21.648026
77.735946	2224.140491	21.653043
77.705817	2223.147178	21.658061
77.939813	2215.590134	21.663079
77.718383	2214.086081	21.668096
77.718313	2223.005323	21.673114
78.034865	2233.154659	21.678131
77.723666	2255.790920	21.683149
77.847596	2242.888634	21.688167
77.983379	2249.637624	21.693184
77.965034	2256.924448	21.698202
78.206626	2244.553802	21.703219
78.090909	2258.814070	21.708237
78.196321	2264.408635	21.713255
78.737768	2271.024860	21.718272
78.668092	2275.446133	21.723290
78.918046	2270.169149	21.728307
78.896811	2273.228792	21.733325
79.300816	2262.751664	21.738343
79.005086	2265.131708	21.743360
79.162449	2262.452465	21.748378
78.958382	2262.686512	21.753395
79.154504	2271.401519	21.758413
79.265792	2267.456670	21.763431
79.264082	2275.992741	21.768448
79.574252	2287.210524	21.773466
79.993731	2296.956959	21.778483
79.633883	2302.778076	21.783501
79.755871	2297.281791	21.788519
80.059047	2301.249758	21.793536
79.494784	2295.190338	21.798554
79.870121	2294.367044	21.803571
79.818136	2293.338774	21.808589
80.201494	2292.792107	21.813607
80.319489	2297.810562	21.818624
79.712741	2290.143198	21.823642
80.287740	2300.434671	21.828659
80.344115	2309.252060	21.833677
80.276589	2308.184245	21.838695
80.019748	2314.749687	21.843712
80.137111	2322.317541	21.848730
80.510536	2320.568158	21.853747
80.590790	2328.266202	21.858765
81.067517	2330.959233	21.863783
80.756325	2337.957352	21.868800
80.810482	2345.674703	21.873818
81.331052	2329.750431	21.878835
81.222334	2336.591274	21.883853
81.199880	2352.014510	21.888871
81.395253	2360.275347	21.893888
81.341535	2368.247651	21.898906
81.782228	2360.518781	21.903923
81.699469	2367.232486	21.908941
81.756870	2360.152767	21.913959
81.684436	2364.609170	21.918976
81.408038	2362.235469	21.923994
82.055181	2357.890117	21.929011
81.885932	2377.396960	21.934029
82.014016	2380.836153	21.939047
82.549824	2384.539882	21.944064
82.293400	2388.554412	21.949082
82.780857	2368.305143	21.954099
82.579258	2380.091130	21.959117
82.942915	2372.751054	21.964135
83.196017	2367.175079	21.969152
82.983484	2371.621302	21.974170
83.196328	2370.307669	21.979187
83.380403	2361.266283	21.984205
82.972616	2346.640407	21.989223
83.289796	2340.553384	21.994240
83.129544	2343.558582	21.999258
82.571352	2346.772438	22.004275
82.619170	2359.312654	22.009293
82.893159	2365.119405	22.014311
83.345161	2365.442460	22.019328
83.290346	2378.263142	22.024346
83.466555	2381.139594	22.029363
83.560041	2393.016321	22.034381
83.794882	2405.547541	22.039399
83.655482	2394.807863	22.044416
83.692092	2404.568387	22.049434
83.879436	2397.587139	22.054451
84.223602	2391.095598	22.059469
83.672484	2405.578363	22.064487
84.150333	2402.761187	22.069504
84.270032	2418.907348	22.074522
84.409260	2414.388902	22.079539
84.474941	2417.076636	22.084557
84.793854	2421.756611	22.089575
84.817676	2423.481582	22.094592
84.472257	2421.131154	22.099610
84.802515	2414.359227	22.104627
84.670488	2410.613839	22.109645
84.687560	2423.204494	22.114663
85.049724	2432.793998	22.119680
85.198039	2436.821203	22.124698
85.173526	2437.196284	22.129715
85.241748	2441.134433	22.134733
85.043937	2441.759189	22.139751
85.619004	2434.761129	22.144768
85.394744	2457.927743	22.149786
85.599600	2464.259033	22.154803
85.827723	2468.487163	22.159821
85.436379	2477.387321	22.164839
85.765165	2482.410176	22.169856
85.494588	2482.999386	22.174874
86.232824	2490.467685	22.179891
86.328152	2496.366778	22.184909
86.402260	2499.675592	22.189927
86.861672	2496.118126	22.194944
86.764234	2497.337646	22.199962
86.928484	2494.752105	22.204979
87.025240	2493.707765	22.209997
86.751777	2492.930864	22.215015
87.134842	2486.478097	22.220032
87.003063	2494.147284	22.225050
86.898029	2480.738736	22.230067
87.184382	2486.947038	22.235085
86.806444	2486.685158	22.240103
87.010463	2478.669171	22.245120
86.808177	2495.633520	22.250138
87.392896	2502.708028	22.255155
87.466577	2513.995594	22.260173
87.431236	2511.970801	22.265191
88.083468	2513.017309	22.270208
87.532183	2520.403062	22.275226
87.981164	2509.704506	22.280243
88.117230	2507.113410	22.285261
87.554692	2511.148134	22.290279
88.256420	2514.340050	22.295296
88.534362	2521.182073	22.300314
88.668542	2526.549108	22.305331
88.977207	2515.849456	22.310349
88.550678	2503.143163	22.315367
89.052777	2487.827731	22.320384
88.586931	2490.704995	22.325402
88.721773	2491.243760	22.330419
88.805167	2498.971684	22.335437
88.663496	2506.328335	22.340455
89.072411	2516.814491	22.345472
88.870122	2527.722715	22.350490
88.747039	2521.896198	22.355507
88.937037	2520.146567	22.360525
88.940929	2525.933302	22.365543
89.395923	2535.453505	22.370560
89.114593	2550.733338	22.375578
89.627474	2548.728855	22.380595
89.817566	2548.430845	22.385613
89.590204	2553.340627	22.390631
90.129695	2546.718919	22.395648
90.072898	2544.371295	22.400666
90.099495	2544.125260	22.405683
90.025922	2540.738253	22.410701
90.063832	2542.156946	22.415719
90.381861	2555.205195	22.420736
90.543678	2568.425091	22.425754
90.401660	2573.754574	22.430771
90.654608	2562.054655	22.435789
90.368189	2570.377954	22.440807
90.787796	2579.015835	22.445824
90.782577	2577.249819	22.450842
91.436628	2555.798946	22.455859
91.393176	2545.660569	22.460877
91.258630	2556.244549	22.465895
91.568235	2544.127335	22.470912
91.607373	2545.598189	22.475930
91.612688	2550.185038	22.480947
91.683786	2544.989263	22.485965
91.845890	2552.994303	22.490983
91.892859	2544.513415	22.496000
91.905846	2546.720143	22.501018
91.729548	2541.192632	22.506035
91.903188	2559.769453	22.511053
92.255361	2572.409662	22.516071
92.126428	2569.067284	22.521088
91.697102	2581.942497	22.526106
91.568963	2576.123493	22.531123
92.186008	2580.783895	22.536141
92.177920	2602.490324	22.541159
92.218381	2608.969471	22.546176
92.501018	2609.027751	22.551194
92.625726	2616.957539	22.556211
92.919510	2620.846044	22.561229
92.972887	2635.169898	22.566247
92.905990	2626.766947	22.571264
93.192125	2629.813376	22.576282
93.347192	2633.183572	22.581299
93.615003	2634.989285	22.586317
93.630343	2631.079583	22.591335
93.787013	2626.284148	22.596352
93.297338	2626.676691	22.601370
93.715192	2632.242695	22.606387
93.600353	2621.570042	22.611405
93.686929	2642.649742	22.616423
94.175036	2640.588733	22.621440
93.818752	2650.208001	22.626458
93.968844	2654.742079	22.631475
94.353452	2639.918489	22.636493
94.267893	2644.489757	22.641511
94.493812	2639.005610	22.646528
94.666737	2663.133740	22.651546
94.687542	2674.533758	22.656563
94.664859	2666.714414	22.661581
95.155205	2674.972070	22.666599
95.168068	2669.078414	22.671616
95.214157	2675.957856	22.676634
95.012915	2667.418540	22.681651
95.540933	2667.051377	22.686669
95.279329	2671.233777	22.691687
95.048987	2673.315204	22.696704
95.135992	2674.621021	22.701722
95.032882	2671.995626	22.706739
95.074480	2680.578661	22.711757
95.047102	2697.405100	22.716775
95.314640	2697.716692	22.721792
95.545079	2712.161594	22.726810
95.632822	2735.938224	22.731827
95.962469	2725.660950	22.736845
95.961108	2736.857600	22.741863
96.174836	2732.315263	22.746880
96.297483	2751.978801	22.751898
96.389890	2754.981068	22.756915
96.815444	2749.849949	22.761933
96.544316	2754.115454	22.766951
96.823228	2754.729505	22.771968
96.983840	2754.164722	22.776986
96.632417	2755.134721	22.782003
97.140015	2766.588169	22.787021
97.092607	2775.511263	22.792039
97.239807	2776.461395	22.797056
97.481925	2773.854601	22.802074
97.684834	2785.070097	22.807091
97.450328	2777.198492	22.812109
97.548824	2779.902097	22.817127
97.387802	2779.273040	22.822144
98.048387	2786.210657	22.827162
97.899555	2805.999304	22.832179
97.972441	2810.530510	22.837197
98.160185	2810.936472	22.842215
98.259929	2808.243482	22.847232
98.478224	2805.712299	22.852250
98.454773	2811.169806	22.857267
98.491553	2802.508571	22.862285
98.757879	2824.746512	22.867303
98.934197	2832.583576	22.872320
98.908850	2823.699962	22.877338
98.848803	2830.734915	22.882355
99.409106	2820.677138	22.887373
99.290396	2826.063861	22.892391
99.543314	2820.165296	22.897408
99.959776	2817.983880	22.902426
99.925416	2821.480090	22.907443
99.945965	2815.099639	22.912461
99.557564	2817.258929	22.917479
99.775135	2816.783897	22.922496
100.165660	2798.435336	22.927514
100.042107	2807.970352	22.932531
100.380247	2808.428491	22.937549
100.118000	2813.574873	22.942567
99.987934	2813.534408	22.947584
100.366176	2820.808743	22.952602
100.660850	2837.714499	22.957619
100.702554	2832.433350	22.962637
100.774065	2854.349751	22.967655
100.813048	2842.989530	22.972672
100.811123	2837.188431	22.977690
100.329484	2846.095140	22.982707
100.658801	2836.650579	22.987725
100.926124	2856.107911	22.992743
101.130959	2861.862952	22.997760
101.255961	2863.617224	23.002778
101.129390	2873.900468	23.007795
100.897088	2879.576577	23.012813
101.665996	2891.997783	23.017831
101.617479	2904.830844	23.022848
102.075852	2894.621050	23.027866
101.790999	2902.457618	23.032883
101.725340	2895.996572	23.037901
102.013567	2901.316875	23.042919
101.921915	2906.508172	23.047936
102.436211	2923.775976	23.052954
102.289071	2937.169585	23.057971
102.609769	2936.646701	23.062989
102.606462	2946.009445	23.068007
102.213042	2931.537332	23.073024
102.597452	2934.256840	23.078042
102.829098	2953.902913	23.083059
102.840838	2958.636856	23.088077
103.459332	2959.251180	23.093095
103.156093	2961.469177	23.098112
103.345925	2958.401323	23.103130
103.156567	2964.674305	23.108147
103.468858	2956.490465	23.113165
103.905747	2968.956672	23.118183
103.766979	2982.097335	23.123200
104.097271	2976.924096	23.128218
103.959408	2984.548075	23.133235
104.184917	2971.735400	23.138253
103.993780	2972.414188	23.143271
103.894196	2975.913004	23.148288
104.129889	2981.460585	23.153306
104.337946	2994.772380	23.158323
104.403947	2995.713184	23.163341
104.391891	3001.117284	23.168359
104.765468	3007.506198	23.173376
105.135808	3019.120449	23.178394
104.955215	3036.336916	23.183411
104.996569	3033.500430	23.188429
105.539453	3033.288284	23.193447
105.432998	3041.459081	23.198464
105.534072	3032.614186	23.203482
105.463095	3033.571455	23.208499
105.374117	3028.332431	23.213517
105.596359	3038.005413	23.218535
105.595691	3057.396500	23.223552
105.650628	3055.336947	23.228570
105.775458	3058.952043	23.233587
105.986738	3074.713952	23.238605
106.162061	3082.478074	23.243623
105.885570	3088.470680	23.248640
106.492541	3077.552949	23.253658
106.626868	3080.487678	23.258675
106.841488	3093.105105	23.263693
107.031162	3109.727795	23.268711
107.073867	3106.756022	23.273728
107.451820	3100.786963	23.278746
107.271035	3092.788544	23.283763
107.539055	3093.992262	23.288781
107.681718	3091.948050	23.293799
107.660529	3107.365130	23.298816
107.679110	3092.491301	23.303834
108.003608	3098.339152	23.308851
107.966307	3091.306732	23.313869
108.016953	3090.650361	23.318887
108.068681	3102.379438	23.323904
108.407937	3086.825109	23.328922
108.104530	3086.095674	23.333939
108.238389	3097.072852	23.338957
108.566930	3107.636552	23.343975
108.308194	3122.744670	23.348992
108.638526	3110.511361	23.354010
108.421109	3123.266363	23.359027
108.602474	3123.790726	23.364045
108.627979	3115.640682	23.369063
108.562532	3141.051784	23.374080
109.008957	3146.742767	23.379098
109.146776	3148.533527	23.384115
109.265725	3151.818098	23.389133
109.469750	3144.471118	23.394151
108.995151	3154.147366	23.399168
109.451570	3168.288581	23.404186
109.513669	3170.999484	23.409203
109.225649	3167.675932	23.414221
109.719982	3181.115130	23.419239
109.713882	3201.405012	23.424256
110.222656	3198.386087	23.429274
109.930342	3203.159608	23.434291
110.069005	3222.481679	23.439309
110.775750	3217.895465	23.444327
110.881859	3222.784293	23.449344
111.217390	3212.562422	23.454362
111.093875	3221.391717	23.459379
111.110973	3213.865119	23.464397
111.231907	3207.131182	23.469415
111.149120	3211.634433	23.474432
111.253557	3214.275704	23.479450
111.305414	3240.793951	23.484467
111.576372	3244.570256	23.489485
111.768147	3239.847941	23.494503
111.836795	3251.765281	23.499520
111.938295	3236.540891	23.504538
111.808468	3246.326057	23.509555
111.825664	3264.791517	23.514573
112.194129	3273.851710	23.519591
112.190654	3280.919200	23.524608
112.348388	3270.710694	23.529626
112.414877	3275.060010	23.534643
112.765455	3288.270412	23.539661
112.710075	3301.616010	23.544679
112.764011	3298.526575	23.549696
112.781509	3300.913386	23.554714
113.144732	3294.647069	23.559731
113.168894	3323.280095	23.564749
113.586603	3327.547830	23.569767
113.841215	3334.098394	23.574784
113.926371	3329.612689	23.579802
113.958993	3323.432405	23.584819
113.748419	3331.227705	23.589837
114.063459	3322.732953	23.594855
113.865499	3329.268951	23.599872
113.975488	3315.530222	23.604890
114.272019	3341.456748	23.609907
114.110811	3357.979730	23.614925
114.212523	3359.331985	23.619943
114.192447	3364.454839	23.624960
114.234993	3385.956680	23.629978
114.488636	3380.269224	23.634995
114.899548	3378.900152	23.640013
115.280696	3380.548919	23.645031
115.434907	3395.448899	23.650048
115.533411	3395.606690	23.655066
115.998040	3400.204477	23.660083
115.987848	3406.927830	23.665101
116.191617	3393.922341	23.670119
115.925864	3399.881388	23.675136
116.156158	3387.811353	23.680154
116.175110	3391.822898	23.685171
116.480972	3394.051950	23.690189
116.572251	3393.681362	23.695207
116.462798	3390.443453	23.700224
116.460211	3389.471081	23.705242
116.788236	3380.437866	23.710259
116.577465	3394.265316	23.715277
116.691661	3390.094484	23.720295
116.834565	3394.392155	23.725312
116.579077	3390.215821	23.730330
117.149221	3401.679428	23.735347
116.760975	3424.585326	23.740365
117.669616	3421.783403	23.745383
117.574242	3416.340960	23.750400
117.319078	3416.135041	23.755418
117.470347	3422.424836	23.760435
117.475891	3435.272973	23.765453
118.219551	3435.057385	23.770471
118.788325	3429.158472	23.775488
118.405444	3427.670102	23.780506
119.008962	3423.645134	23.785523
118.656201	3429.442255	23.790541
118.773778	3429.077928	23.795559
118.752155	3420.603238	23.800576
119.118283	3423.024662	23.805594
119.514394	3410.944378	23.810611
119.067571	3410.692742	23.815629
119.139094	3403.276312	23.820647
119.262752	3406.132553	23.825664
119.389381	3420.107915	23.830682
119.467202	3430.246524	23.835699
119.481371	3436.085437	23.840717
119.412790	3442.331058	23.845735
119.639858	3443.445538	23.850752
119.424102	3463.546169	23.855770
120.016951	3463.258782	23.860787
119.517040	3479.680287	23.865805
120.053415	3491.635057	23.870823
120.319408	3501.679837	23.875840
120.281791	3506.279613	23.880858
120.722436	3499.097105	23.885875
120.577135	3513.826475	23.890893
120.659947	3515.766198	23.895911
120.996764	3524.985357	23.900928
121.096971	3530.537933	23.905946
121.121364	3524.393193	23.910963
121.248062	3556.757646	23.915981
121.561803	3548.976845	23.920999
121.543871	3561.688815	23.926016
121.544031	3569.306679	23.931034
121.868486	3561.233902	23.936051
122.002874	3579.079011	23.941069
122.333412	3581.555986	23.946087
122.396701	3576.095784	23.951104
122.581841	3582.082738	23.956122
122.772772	3580.889591	23.961139
122.354062	3578.838199	23.966157
123.025139	3591.708560	23.971175
123.145512	3601.459064	23.976192
123.085792	3609.260539	23.981210
123.433227	3596.023112	23.986227
123.711426	3609.580498	23.991245
123.571561	3603.636665	23.996263
123.810323	3611.590137	24.001280
123.661476	3599.807379	24.006298
123.683999	3598.090581	24.011315
123.458702	3601.076508	24.016333
123.682517	3618.923339	24.021351
123.597691	3625.869449	24.026368
123.745384	3633.122237	24.031386
124.045853	3643.225560	24.036403
124.310005	3658.937932	24.041421
124.409649	3662.478211	24.046439
124.501181	3653.759369	24.051456
124.384681	3674.581657	24.056474
124.902482	3677.400800	24.061491
124.747524	3691.134187	24.066509
124.667690	3687.008907	24.071527
125.439111	3703.441059	24.076544
125.491223	3716.510062	24.081562
125.821098	3715.540303	24.086579
125.540125	3716.161206	24.091597
125.612946	3725.272368	24.096615
125.721906	3713.741993	24.101632
125.817240	3736.246294	24.106650
125.940205	3736.334268	24.111667
126.084015	3746.923196	24.116685
126.330237	3739.115328	24.121703
126.799683	3739.328818	24.126720
126.964517	3755.685033	24.131738
127.097892	3770.289978	24.136755
127.279275	3764.441536	24.141773
127.159370	3763.321293	24.146791
127.710687	3752.673402	24.151808
127.431692	3771.972634	24.156826
127.416339	3768.342191	24.161843
127.332380	3766.958068	24.166861
127.543633	3779.298230	24.171879
127.746256	3784.628733	24.176896
127.879226	3796.340106	24.181914
127.819370	3794.781089	24.186931
128.201545	3798.424467	24.191949
128.350964	3807.850548	24.196967
128.504325	3820.550407	24.201984
128.274255	3829.164650	24.207002
128.731093	3820.114504	24.212019
128.665052	3831.433724	24.217037
128.615053	3834.068477	24.222055
129.309015	3839.722520	24.227072
129.413155	3854.309170	24.232090
129.112109	3840.061441	24.237107
129.113933	3868.749971	24.242125
129.618419	3868.491834	24.247143
129.780377	3863.703019	24.252160
129.751678	3871.686107	24.257178
130.271911	3884.236852	24.262195
130.316458	3890.916667	24.267213
130.488965	3903.942982	24.272231
130.342198	3894.418614	24.277248
130.195605	3908.543371	24.282266
130.881590	3900.150862	24.287283
131.144868	3920.393369	24.292301
130.975717	3918.957633	24.297319
131.324081	3924.104495	24.302336
131.276981	3919.157858	24.307354
131.625285	3914.832615	24.312371
131.308963	3908.100951	24.317389
131.386868	3932.150759	24.322407
131.899388	3937.583381	24.327424
131.922069	3942.642225	24.332442
132.345499	3935.443875	24.337459
132.330545	3940.136088	24.342477
132.387797	3939.364396	24.347495
132.701751	3931.929874	24.352512
132.363797	3945.537573	24.357530
132.644117	3953.672923	24.362547
133.019397	3970.330657	24.367565
132.745383	3968.041358	24.372583
132.952741	3960.149669	24.377600
133.101921	3965.481634	24.382618
133.316533	3964.453445	24.387635
133.704143	3976.143114	24.392653
134.121595	3964.299838	24.397671
134.557615	3963.540410	24.402688
134.600635	3951.493582	24.407706
134.260929	3939.691882	24.412723
134.310375	3940.864659	24.417741
134.257541	3943.328225	24.422759
134.638594	3945.507457	24.427776
134.711571	3957.576605	24.432794
134.626740	3965.158777	24.437811
134.815516	3964.062825	24.442829
134.527359	3968.212965	24.447847
134.658781	3977.496057	24.452864
134.444861	3990.005084	24.457882
135.039873	3997.043139	24.462899
135.144549	3989.779212	24.467917
135.662003	4008.160057	24.472935
136.145663	4009.832810	24.477952
136.047483	4008.308096	24.482970
136.281950	4012.274537	24.487987
136.619693	4004.197752	24.493005
136.269092	4021.969214	24.498023
136.708022	4007.564503	24.503040
136.633954	4008.402249	24.508058
136.606074	4029.172087	24.513075
136.922451	4041.670997	24.518093
136.868521	4048.664529	24.523111
136.822253	4046.280672	24.528128
136.845546	4046.267479	24.533146
137.160027	4057.815009	24.538163
137.362116	4064.610077	24.543181
137.256181	4071.963492	24.548199
137.664745	4081.571117	24.553216
137.945054	4094.836801	24.558234
137.669046	4102.891030	24.563251
138.051635	4099.564908	24.568269
138.321348	4112.627221	24.573287
138.746851	4116.341046	24.578304
138.626772	4125.992444	24.583322
139.037124	4127.475395	24.588339
138.911477	4117.823740	24.593357
139.094913	4132.478194	24.598375
139.203913	4147.043441	24.603392
139.415770	4156.898792	24.608410
139.361757	4152.219017	24.613427
139.396326	4145.006045	24.618445
139.526569	4148.429916	24.623463
139.881922	4173.305378	24.628480
139.921785	4175.927617	24.633498
140.148223	4188.241561	24.638515
140.349387	4181.457649	24.643533
140.059991	4195.122858	24.648551
140.469154	4196.181146	24.653568
140.391315	4209.426116	24.658586
140.613457	4207.845003	24.663603
141.005102	4212.170474	24.668621
140.856115	4229.271170	24.673639
141.335146	4229.373613	24.678656
141.347092	4242.091014	24.683674
141.514415	4242.902048	24.688691
141.724630	4253.334986	24.693709
141.801066	4266.546492	24.698727
142.146019	4262.866693	24.703744
142.016489	4256.544063	24.708762
141.955743	4259.512220	24.713779
142.391276	4280.885804	24.718797
142.018722	4296.828262	24.723815
142.328057	4286.853395	24.728832
142.369335	4294.985726	24.733850
142.607786	4320.988894	24.738867
142.813403	4320.854838	24.743885
142.804697	4332.340904	24.748903
143.659001	4336.513927	24.753920
143.579873	4336.086189	24.758938
144.139780	4336.099592	24.763955
144.281287	4335.854910	24.768973
144.307802	4331.280617	24.773991
144.474251	4332.463513	24.779008
144.635522	4326.505983	24.784026
144.147409	4335.783952	24.789043
144.480476	4325.250698	24.794061
144.626422	4333.264852	24.799079
144.776544	4349.939538	24.804096
144.956637	4370.625655	24.809114
144.760092	4364.761433	24.814131
145.158085	4355.656970	24.819149
145.008211	4376.647572	24.824167
145.322382	4388.688785	24.829184
145.403338	4393.139963	24.834202
145.418001	4409.395418	24.839219
145.589552	4421.661964	24.844237
145.330708	4438.125915	24.849255
145.837278	4445.625009	24.854272
146.220406	4447.888629	24.859290
146.090937	4465.700629	24.864307
146.516947	4464.213195	24.869325
146.386911	4478.420766	24.874343
147.013731	4482.608006	24.879360
147.132109	4505.293865	24.884378
147.315314	4513.297195	24.889395
147.535330	4506.660430	24.894413
147.744245	4509.191632	24.899431
147.481504	4512.105198	24.904448
147.703082	4524.146151	24.909466
147.679986	4536.390003	24.914483
148.043391	4539.846882	24.919501
148.132362	4546.505812	24.924519
148.171767	4560.665614	24.929536
148.509163	4567.818798	24.934554
148.670954	4570.326338	24.939571
149.102562	4579.498084	24.944589
149.686881	4582.410300	24.949607
150.281094	4577.987313	24.954624
150.815931	4567.232936	24.959642
150.437376	4551.425509	24.964659
150.591511	4531.416279	24.969677
150.508801	4532.904419	24.974695
150.618733	4527.894087	24.979712
151.041425	4526.031545	24.984730
150.623344	4522.599760	24.989747
150.870608	4527.616356	24.994765
150.665922	4532.161503	24.999783
150.685611	4524.221571	25.004800
151.127689	4522.958272	25.009818
150.760295	4538.069266	25.014835
151.104292	4552.446996	25.019853
151.078376	4560.991487	25.024871
151.175907	4560.423344	25.029888
151.567615	4573.619735	25.034906
151.682468	4597.186781	25.039923
151.517465	4593.899574	25.044941
151.508928	4613.100554	25.049959
151.537879	4633.217539	25.054976
151.952685	4627.362674	25.059994
151.599652	4651.642308	25.065011
152.117454	4658.095358	25.070029
152.147528	4668.856986	25.075047
152.318715	4686.151476	25.080064
152.929965	4676.336468	25.085082
153.003462	4708.038791	25.090099
153.282928	4702.853749	25.095117
153.294803	4716.637882	25.100135
153.366986	4714.935942	25.105152
153.782147	4727.364646	25.110170
153.803787	4743.571247	25.115187
153.729598	4736.610764	25.120205
154.360951	4749.914753	25.125223
154.520759	4758.941970	25.130240
154.745945	4767.445636	25.135258
154.547108	4765.353212	25.140275
154.854101	4763.107431	25.145293
155.156071	4778.356292	25.150311
155.349153	4785.120882	25.155328
155.852117	4779.953805	25.160346
155.905609	4783.615809	25.165363
155.953301	4777.888833	25.170381
156.294079	4767.186256	25.175399
156.252554	4775.464116	25.180416
156.704632	4787.133837	25.185434
156.155696	4807.520332	25.190451
156.542117	4806.105601	25.195469
157.013387	4800.495668	25.200487
157.035656	4804.272335	25.205504
157.159756	4794.383056	25.210522
156.925837	4818.975501	25.215539
156.804342	4835.855710	25.220557
157.182062	4832.958676	25.225575
157.050464	4854.304425	25.230592
157.324710	4866.603870	25.235610
157.376761	4882.335391	25.240627
157.793151	4889.726827	25.245645
158.153199	4892.881923	25.250663
158.582975	4896.895681	25.255680
158.950006	4907.967694	25.260698
159.173903	4920.983561	25.265715
159.180577	4914.586841	25.270733
159.517741	4905.225191	25.275751
159.408484	4907.385623	25.280768
159.522720	4898.095673	25.285786
159.670511	4914.178318	25.290803
159.781989	4917.996104	25.295821
160.042931	4945.678003	25.300839
160.020166	4937.966220	25.305856
160.072492	4936.699925	25.310874
160.238328	4942.344480	25.315891
160.466794	4955.135949	25.320909
160.684512	4964.763232	25.325927
160.574083	4980.179262	25.330944
160.351534	4971.911566	25.335962
160.550348	4989.771204	25.340979
161.009839	5003.300858	25.345997
161.610837	5013.531546	25.351015
161.539179	5030.790374	25.356032
161.772763	5027.859764	25.361050
162.009776	5026.430462	25.366067
162.119137	5035.051964	25.371085
162.012504	5051.094332	25.376103
162.061418	5060.738698	25.381120
162.301940	5063.560074	25.386138
162.550472	5072.740480	25.391155
162.620015	5085.569490	25.396173
163.112410	5076.040184	25.401191
162.710587	5097.356346	25.406208
163.258450	5107.744775	25.411226
163.180748	5109.287265	25.416243
163.519462	5109.068872	25.421261
163.400506	5122.413586	25.426279
163.578848	5138.132253	25.431296
163.793997	5129.654706	25.436314
164.067516	5155.191129	25.441331
164.046115	5167.414714	25.446349
164.820288	5168.477791	25.451367
164.739425	5191.072524	25.456384
165.080195	5193.164517	25.461402
165.240276	5197.011311	25.466419
165.248841	5192.533471	25.471437
165.437486	5197.429287	25.476455
165.469416	5222.603515	25.481472
166.029403	5221.970319	25.486490
166.011156	5230.372135	25.491507
166.061668	5225.479354	25.496525
166.448095	5229.830394	25.501543
166.191605	5252.885200	25.506560
166.689455	5244.036138	25.511578
166.674178	5248.576794	25.516595
167.028583	5259.354240	25.521613
167.490043	5281.407708	25.526631
167.301307	5279.933357	25.531648
167.539939	5281.484731	25.536666
167.487551	5284.850203	25.541683
167.719781	5298.014637	25.546701
168.084277	5289.998122	25.551719
168.194088	5306.237118	25.556736
168.517983	5306.801672	25.561754
168.888002	5315.930531	25.566771
168.878492	5334.693873	25.571789
168.904859	5322.058474	25.576807
168.986565	5323.796594	25.581824
169.189553	5324.824644	25.586842
169.208956	5353.993387	25.591859
169.312250	5367.351783	25.596877
169.844109	5357.373920	25.601895
169.682158	5378.135526	25.606912
170.136407	5384.020570	25.611930
170.148203	5390.910841	25.616947
170.165603	5400.153473	25.621965
170.364583	5401.835098	25.626983
170.379854	5428.655316	25.632000
170.730753	5417.649763	25.637018
171.008865	5446.132234	25.642035
170.894548	5451.164317	25.647053
170.807551	5453.710978	25.652071
171.033837	5474.931942	25.657088
171.373232	5481.359062	25.662106
171.627319	5497.451418	25.667123
172.089171	5514.467759	25.672141
172.140778	5508.875332	25.677159
172.354767	5522.899091	25.682176
172.557803	5531.834511	25.687194
172.953575	5530.022009	25.692212
172.831827	5532.281475	25.697229
173.045198	5540.864707	25.702247
173.302682	5564.570957	25.707264
173.295185	5566.570441	25.712282
173.488995	5568.438027	25.717300
173.702273	5583.859927	25.722317
174.208176	5579.426139	25.727335
173.971345	5587.985756	25.732352
174.069990	5591.171830	25.737370
174.795108	5600.615956	25.742388
174.656006	5613.220947	25.747405
174.777616	5610.949935	25.752423
174.804232	5615.160035	25.757440
175.133786	5626.304943	25.762458
175.399423	5635.111881	25.767476
175.704407	5648.403923	25.772493
175.468829	5641.348568	25.777511
175.797196	5650.146666	25.782528
175.939627	5677.563649	25.787546
175.979751	5670.235642	25.792564
175.815497	5687.781507	25.797581
175.945092	5683.939483	25.802599
176.186464	5703.043558	25.807616
176.848044	5722.982781	25.812634
177.139421	5727.555318	25.817652
177.336890	5736.324022	25.822669
177.820988	5731.457488	25.827687
177.668584	5739.019449	25.832704
177.730926	5750.330923	25.837722
177.886594	5756.100325	25.842740
178.045136	5762.297705	25.847757
178.406905	5778.219662	25.852775
178.277599	5786.501611	25.857792
178.241187	5799.463797	25.862810
178.481203	5811.060044	25.867828
178.664421	5825.476684	25.872845
179.133253	5823.974140	25.877863
179.180108	5852.373693	25.882880
179.282555	5849.483625	25.887898
179.596337	5863.810085	25.892916
179.916471	5881.905760	25.897933
179.969397	5874.317985	25.902951
179.959120	5898.707975	25.907968
180.043516	5905.628151	25.912986
180.484355	5911.144661	25.918004
180.414796	5934.144983	25.923021
180.570019	5941.547235	25.928039
180.943670	5965.946783	25.933056
181.650585	5961.875657	25.938074
182.170636	5956.133563	25.943092
181.878520	5967.115799	25.948109
182.597212	5962.110189	25.953127
182.665355	5959.851162	25.958144
183.018567	5963.878708	25.963162
183.566432	5977.554405	25.968180
183.201857	5973.617210	25.973197
183.622080	5974.981748	25.978215
183.540603	5973.938444	25.983232
183.631639	5966.335628	25.988250
183.850065	5968.876516	25.993268
183.722370	5979.815688	25.998285
183.617633	5967.450441	26.003303
183.841563	5982.700839	26.008320
183.845760	5988.350575	26.013338
184.084529	6000.572530	26.018356
184.080279	6013.279088	26.023373
184.107933	6023.892398	26.028391
184.381673	6056.483302	26.033408
184.695473	6066.649774	26.038426
185.072224	6071.535874	26.043444
185.019444	6091.275280	26.048461
185.534558	6098.133424	26.053479
185.647959	6105.601774	26.058496
185.730081	6127.773807	26.063514
186.046082	6129.824362	26.068532
186.289283	6139.642673	26.073549
186.561474	6151.782793	26.078567
186.759406	6154.763456	26.083584
186.921466	6153.252785	26.088602
186.959584	6149.446326	26.093620
187.147612	6174.609524	26.098637
187.550192	6173.538546	26.103655
187.733590	6173.505050	26.108672
188.159225	6183.590795	26.113690
188.497976	6178.130785	26.118708
188.457034	6197.314661	26.123725
188.492442	6197.775176	26.128743
188.503841	6201.921014	26.133760
188.447548	6210.077635	26.138778
189.032608	6219.891963	26.143796
188.833768	6240.385949	26.148813
189.182476	6232.918194	26.153831
189.345907	6249.744693	26.158848
189.399603	6265.871919	26.163866
189.767158	6278.008893	26.168884
189.612133	6297.020454	26.173901
189.903456	6301.709737	26.178919
190.512678	6305.381359	26.183936
190.503318	6322.801374	26.188954
190.542528	6323.242358	26.193972
190.630349	6338.855181	26.198989
190.681285	6353.583343	26.204007
191.089995	6358.706812	26.209024
190.733374	6387.981686	26.214042
191.485173	6399.372822	26.219060
191.686885	6417.844010	26.224077
192.207934	6414.785044	26.229095
192.594382	6424.619112	26.234112
192.534884	6439.065616	26.239130
192.949609	6426.948440	26.244148
193.053662	6428.654615	26.249165
193.258294	6451.955900	26.254183
193.465841	6460.313763	26.259200
193.400739	6473.364757	26.264218
193.927465	6471.120826	26.269236
194.004476	6487.487782	26.274253
194.157118	6493.398156	26.279271
194.362252	6503.501842	26.284288
194.426431	6523.523229	26.289306
194.744061	6529.032864	26.294324
194.914544	6533.748596	26.299341
195.144467	6545.844060	26.304359
195.346191	6563.348199	26.309376
195.606538	6559.807169	26.314394
196.089409	6536.467361	26.319412
196.021300	6567.788166	26.324429
196.276706	6572.053447	26.329447
196.576597	6583.713565	26.334464
196.616389	6572.748669	26.339482
196.964373	6591.599815	26.344500
197.042091	6600.518070	26.349517
197.161665	6605.025682	26.354535
197.544239	6604.002897	26.359552
197.737656	6621.020144	26.364570
197.897799	6631.360590	26.369588
197.834544	6645.756709	26.374605
198.038425	6640.700170	26.379623
198.108195	6646.192745	26.384640
198.605372	6654.296226	26.389658
198.973856	6654.052394	26.394676
198.725939	6661.017091	26.399693
198.765907	6673.708167	26.404711
199.266180	6683.821214	26.409728
199.329749	6691.692730	26.414746
199.666694	6708.617698	26.419764
199.708766	6721.153296	26.424781
199.612869	6728.389705	26.429799
200.433591	6733.333781	26.434816
200.234754	6750.454937	26.439834
200.655787	6755.441013	26.444852
200.891506	6761.319569	26.449869
200.615844	6777.303553	26.454887
201.094894	6783.537873	26.459904
200.808651	6789.878087	26.464922
201.334518	6807.629520	26.469940
201.393125	6811.539255	26.474957
201.468662	6838.437702	26.479975
201.902548	6843.093221	26.484992
201.953911	6860.370623	26.490010
201.842195	6872.594778	26.495028
202.774821	6879.288589	26.500045
203.972697	6864.944224	26.505063
205.081993	6856.439277	26.510080
204.593016	6847.622546	26.515098
204.707094	6830.004439	26.520116
204.674262	6827.966068	26.525133
204.994001	6829.352107	26.530151
204.969509	6822.331248	26.535168
205.058754	6830.218259	26.540186
205.056884	6821.776658	26.545204
205.208379	6822.744054	26.550221
205.084118	6842.330078	26.555239
205.478304	6857.869669	26.560256
205.393803	6863.146142	26.565274
205.488684	6862.972187	26.570292
205.421970	6884.199621	26.575309
205.675503	6905.202164	26.580327
205.743146	6907.861990	26.585344
205.716691	6935.394282	26.590362
206.167557	6955.007759	26.595380
206.612123	6970.772236	26.600397
206.606959	6992.520470	26.605415
206.998425	7005.967060	26.610432
207.423122	7026.480543	26.615450
207.579478	7040.021364	26.620468
207.429798	7057.449746	26.625485
207.541974	7068.553029	26.630503
208.260793	7081.545160	26.635520
207.925885	7103.227033	26.640538
208.796792	7109.547606	26.645556
209.150871	7109.953625	26.650573
209.358323	7129.172972	26.655591
210.050949	7135.609034	26.660608
209.787691	7139.955923	26.665626
210.014608	7137.657745	26.670644
210.242516	7142.472029	26.675661
210.191397	7159.367438	26.680679
210.395848	7163.995799	26.685696
210.681810	7180.531971	26.690714
210.504667	7199.216677	26.695732
211.101902	7205.056598	26.700749
210.974787	7231.352945	26.705767
211.285881	7236.925354	26.710784
211.259861	7255.983578	26.715802
211.827381	7270.964671	26.720820
212.025546	7281.930939	26.725837
211.984670	7299.254076	26.730855
212.283525	7310.135893	26.735872
212.684387	7325.317229	26.740890
212.659598	7339.318473	26.745908
212.784791	7344.580744	26.750925
212.892313	7364.495957	26.755943
213.610009	7377.469615	26.760960
213.846271	7383.509787	26.765978
214.236817	7377.642988	26.770996
214.751110	7376.951152	26.776013
214.502720	7395.124120	26.781031
215.072584	7386.473798	26.786048
215.525161	7406.404986	26.791066
215.195342	7403.450191	26.796084
215.701228	7406.888767	26.801101
215.159755	7410.574618	26.806119
215.503844	7427.253412	26.811136
215.557031	7433.161760	26.816154
215.766748	7459.328476	26.821172
216.392278	7466.507580	26.826189
216.248322	7478.122377	26.831207
216.472445	7494.267433	26.836224
216.431276	7512.351753	26.841242
217.187645	7525.608189	26.846260
217.365723	7532.249637	26.851277
217.026263	7563.674202	26.856295
217.753667	7563.880361	26.861312
217.727794	7586.543413	26.866330
217.686610	7589.497914	26.871348
218.109622	7614.362055	26.876365
218.189897	7632.820966	26.881383
218.793698	7642.471597	26.886400
218.909664	7661.880081	26.891418
219.104659	7678.939161	26.896436
219.623186	7692.750406	26.901453
219.504101	7709.743550	26.906471
220.296975	7714.125430	26.911488
220.546749	7721.080363	26.916506
220.655478	7733.114163	26.921524
221.415916	7745.339015	26.926541
221.442556	7732.139236	26.931559
221.756069	7731.364956	26.936576
222.042875	7742.186057	26.941594
222.365678	7751.581755	26.946612
222.500205	7744.148096	26.951629
222.295923	7764.058902	26.956647
222.442929	7758.293081	26.961664
222.616108	7772.365790	26.966682
222.632732	7789.813028	26.971700
222.824884	7789.654410	26.976717
222.769536	7816.621158	26.981735
223.082780	7829.975894	26.986752
223.653693	7842.111005	26.991770
223.600988	7851.195783	26.996788
223.950656	7868.061586	27.001805
223.924981	7883.563241	27.006823
224.580321	7898.099465	27.011840
224.563233	7914.627677	27.016858
224.689799	7926.594855	27.021876
224.936344	7940.846148	27.026893
224.940792	7967.172262	27.031911
225.315433	7977.946634	27.036928
225.702839	8003.354517	27.041946
225.673367	8012.329185	27.046964
225.906601	8035.584719	27.051981
226.190486	8048.291505	27.056999
226.333404	8066.907506	27.062016
227.030762	8076.174209	27.067034
227.630351	8087.150745	27.072052
227.984664	8094.758817	27.077069
228.143975	8106.087368	27.082087
228.108250	8102.203701	27.087104
228.183312	8110.703394	27.092122
228.391286	8133.636367	27.097140
228.687682	8135.209942	27.102157
228.353281	8149.365742	27.107175
229.001961	8162.534266	27.112192
229.209026	8156.699245	27.117210
229.707660	8179.164925	27.122228
230.066691	8177.398417	27.127245
229.845101	8191.299195	27.132263
230.061444	8201.236681	27.137280
230.220204	8214.678063	27.142298
230.301420	8225.180753	27.147316
230.446312	8251.500544	27.152333
230.825356	8272.850333	27.157351
230.867501	8289.914195	27.162368
231.327356	8299.524552	27.167386
231.264389	8314.104094	27.172404
231.474865	8315.866839	27.177421
232.191628	8348.243114	27.182439
231.734561	8364.328144	27.187456
232.263989	8372.052984	27.192474
232.392565	8396.936548	27.197492
232.957744	8411.108539	27.202509
233.021016	8431.735092	27.207527
233.006695	8456.511727	27.212544
233.871566	8457.823099	27.217562
233.791052	8473.146957	27.222580
234.767463	8477.579699	27.227597
235.077539	8492.259697	27.232615
235.702756	8482.477074	27.237632
235.890332	8477.310809	27.242650
236.030189	8482.234660	27.247668
236.596682	8472.264079	27.252685
236.690310	8473.536593	27.257703
236.675998	8484.581531	27.262720
237.253869	8492.627654	27.267738
237.041819	8499.396557	27.272756
237.532668	8493.656844	27.277773
237.269708	8501.473226	27.282791
237.130548	8505.157860	27.287808
237.569464	8513.820245	27.292826
237.759513	8543.034239	27.297844
237.897553	8543.855097	27.302861
237.948089	8566.553322	27.307879
237.898050	8578.132832	27.312896
238.317510	8594.422216	27.317914
238.538924	8611.367622	27.322932
238.489923	8623.607905	27.327949
239.020454	8638.306552	27.332967
239.449782	8658.791443	27.337984
240.244223	8674.663337	27.343002
240.437084	8693.081926	27.348020
240.372269	8693.708049	27.353037
240.915518	8712.756145	27.358055
241.075217	8717.134804	27.363072
241.279992	8709.685876	27.368090
241.267418	8733.092764	27.373108
241.760016	8748.012082	27.378125
241.974056	8743.436870	27.383143
242.120191	8762.465928	27.388160
242.706200	8762.996527	27.393178
242.589584	8778.458229	27.398196
242.608161	8792.633149	27.403213
242.948392	8803.440583	27.408231
242.876059	8822.316161	27.413248
243.358264	8833.527775	27.418266
243.366362	8866.292257	27.423284
243.447124	8871.271736	27.428301
243.814682	8894.597585	27.433319
243.874654	8915.444306	27.438336
244.266953	8931.116222	27.443354
244.457948	8953.805052	27.448372
244.847820	8982.567563	27.453389
245.050723	8988.810830	27.458407
245.104808	9005.816754	27.463424
245.170648	9013.625234	27.468442
245.505959	9036.204337	27.473460
245.712285	9059.435899	27.478477
246.312160	9071.519876	27.483495
246.398878	9100.340057	27.488512
246.936078	9106.568792	27.493530
247.283461	9133.195131	27.498548
247.113605	9141.581663	27.503565
247.611296	9155.192039	27.508583
247.463617	9177.194591	27.513600
248.162961	9188.532659	27.518618
248.153490	9201.653841	27.523636
248.574325	9224.356861	27.528653
249.106113	9247.729990	27.533671
248.897033	9270.395932	27.538688
249.323560	9276.181488	27.543706
249.500800	9291.165526	27.548724
249.830785	9299.972482	27.553741
250.626570	9308.300290	27.558759
251.087347	9315.163358	27.563776
251.544778	9309.866913	27.568794
251.433228	9328.333658	27.573812
251.868614	9332.191655	27.578829
252.378447	9332.691607	27.583847
252.451622	9322.533047	27.588864
253.097725	9324.116393	27.593882
253.303909	9344.547069	27.598900
253.144008	9350.284344	27.603917
253.687463	9352.014730	27.608935
253.677103	9355.155864	27.613952
253.742252	9358.753180	27.618970
253.883486	9367.517482	27.623988
253.988372	9382.218999	27.629005
254.204302	9381.981581	27.634023
254.385314	9405.936305	27.639040
254.593480	9405.021112	27.644058
254.718176	9427.675937	27.649076
254.918821	9440.230656	27.654093
254.941212	9473.038118	27.659111
255.056073	9489.057609	27.664128
255.436413	9506.777948	27.669146
255.524789	9532.774429	27.674164
255.666296	9556.921859	27.679181
256.023385	9571.743931	27.684199
256.225737	9601.017684	27.689216
256.640669	9624.240617	27.694234
256.848536	9649.785727	27.699252
257.397911	9678.142487	27.704269
257.699365	9692.551659	27.709287
257.596903	9722.449788	27.714304
257.847154	9734.352867	27.719322
258.113131	9755.931403	27.724340
258.537810	9782.739777	27.729357
258.983282	9798.147677	27.734375
259.141505	9823.455518	27.739392
259.495085	9837.064422	27.744410
259.986622	9865.480754	27.749428
259.746278	9880.616652	27.754445
260.497366	9894.360453	27.759463
260.854609	9904.180267	27.764480
261.192504	9911.087643	27.769498
261.513959	9930.939787	27.774516
261.826418	9936.663393	27.779533
262.235125	9943.813480	27.784551
262.309805	9953.556584	27.789568
262.548032	9960.874443	27.794586
262.950830	9974.746293	27.799604
262.889129	9989.147527	27.804621
263.365094	9985.174451	27.809639
263.402676	10004.223018	27.814656
263.514072	10018.482075	27.819674
263.521329	10035.615042	27.824692
263.803548	10059.561016	27.829709
264.039794	10072.437256	27.834727
264.053337	10099.508268	27.839744
264.444550	10122.643689	27.844762
264.839726	10140.573399	27.849780
264.806891	10163.566620	27.854797
265.365986	10179.152176	27.859815
265.698904	10204.304755	27.864832
266.458419	10219.521442	27.869850
266.325433	10224.504553	27.874868
266.496578	10261.356415	27.879885
267.064980	10264.922321	27.884903
267.230184	10285.089992	27.889920
267.347348	10289.658925	27.894938
267.746067	10310.048601	27.899956
268.152385	10327.223510	27.904973
268.522887	10343.303010	27.909991
269.206408	10333.599403	27.915008
269.703084	10347.254296	27.920026
270.060063	10364.364963	27.925044
270.357729	10366.998181	27.930061
270.497976	10359.890100	27.935079
270.818277	10364.766433	27.940096
270.789851	10382.355545	27.945114
270.874740	10392.750326	27.950132
270.896979	10398.990284	27.955149
271.468372	10423.894814	27.960167
271.580560	10445.261115	27.965184
271.420252	10459.564916	27.970202
272.415391	10443.138922	27.975220
272.845077	10455.397975	27.980237
273.335612	10469.600747	27.985255
273.456106	10482.372070	27.990272
273.542046	10479.689538	27.995290
273.653301	10495.131575	28.000308
273.913469	10501.938674	28.005325
274.227564	10511.601374	28.010343
274.340264	10528.365186	28.015360
274.630442	10534.218762	28.020378
275.166345	10543.190729	28.025396
275.305392	10554.659101	28.030413
275.422717	10555.003717	28.035431
275.767339	10578.090812	28.040448
275.975313	10590.590065	28.045466
276.402744	10608.992369	28.050484
276.433804	10630.907336	28.055501
276.710568	10635.391552	28.060519
276.835111	10670.114687	28.065536
276.832616	10674.579918	28.070554
277.377070	10707.304740	28.075572
277.162591	10728.528726	28.080589
277.772743	10742.128076	28.085607
277.847100	10771.039181	28.090624
278.450564	10798.127597	28.095642
278.863422	10797.296500	28.100660
278.839227	10824.429360	28.105677
279.142343	10842.444479	28.110695
279.519717	10860.756118	28.115712
279.777519	10881.213263	28.120730
280.291789	10893.790285	28.125748
280.584904	10906.698715	28.130765
281.284676	10909.943561	28.135783
281.735372	10908.754791	28.140800
282.065656	10912.738574	28.145818
282.512684	10910.250458	28.150836
282.341959	10915.910513	28.155853
282.678680	10931.525080	28.160871
282.818026	10948.932518	28.165888
282.801672	10949.346622	28.170906
283.306119	10966.926628	28.175924
282.871320	10982.730873	28.180941
283.415972	10995.881213	28.185959
283.555593	11021.329540	28.190976
283.461944	11046.310857	28.195994
283.701712	11066.498634	28.201012
283.748286	11100.652633	28.206029
284.270695	11125.010159	28.211047
284.703593	11155.906101	28.216064
284.540695	11180.339746	28.221082
285.170503	11202.175712	28.226100
285.680901	11235.961430	28.231117
285.939613	11241.813402	28.236135
286.594418	11261.685082	28.241152
286.670643	11275.966066	28.246170
287.203453	11298.141304	28.251188
287.362847	11314.379756	28.256205
287.773440	11324.353881	28.261223
288.095753	11359.581395	28.266240
288.277419	11386.116880	28.271258
288.787966	11389.853382	28.276276
289.201359	11417.291144	28.281293
289.295557	11427.160320	28.286311
289.497375	11447.896938	28.291328
289.864666	11469.874578	28.296346
290.569144	11488.387862	28.301364
290.810753	11510.589710	28.306381
291.115841	11509.535393	28.311399
291.306608	11528.030066	28.316416
292.292371	11528.383278	28.321434
292.565048	11523.941727	28.326452
292.952623	11547.748716	28.331469
292.962047	11547.080729	28.336487
293.315659	11548.944544	28.341504
293.220070	11551.647232	28.346522
293.654692	11568.478402	28.351540
293.612756	11578.928109	28.356557
293.870300	11589.121644	28.361575
294.135419	11612.570887	28.366592
294.307287	11634.653703	28.371610
294.612919	11643.476240	28.376628
294.458368	11673.758517	28.381645
294.733894	11694.527328	28.386663
295.257195	11711.682708	28.391680
295.286208	11746.280629	28.396698
295.785244	11764.618783	28.401716
295.710186	11788.710987	28.406733
296.112451	11817.717612	28.411751
297.086457	11815.981713	28.416768
297.488359	11836.127759	28.421786
298.153297	11839.759931	28.426804
298.259896	11868.347755	28.431821
298.866863	11879.553390	28.436839
298.957093	11890.975670	28.441856
298.874998	11894.769777	28.446874
299.717638	11903.317299	28.451892
299.373786	11923.601529	28.456909
300.064710	11940.852218	28.461927
300.334201	11951.948509	28.466944
300.015489	11968.448263	28.471962
300.622982	11984.770528	28.476980
300.577358	11991.231169	28.481997
300.406975	12011.984645	28.487015
301.045651	12033.084363	28.492032
300.978198	12062.884880	28.497050
301.476572	12093.743375	28.502068
301.198255	12121.324033	28.507085
301.375520	12139.870499	28.512103
301.973092	12179.690142	28.517120
301.939131	12216.192094	28.522138
302.283950	12253.111832	28.527156
302.599621	12289.513318	28.532173
303.103046	12310.971521	28.537191
303.594877	12336.752635	28.542208
303.963826	12369.670720	28.547226
304.060282	12400.867613	28.552244
304.642919	12422.957327	28.557261
304.981598	12449.082386	28.562279
305.882204	12473.420090	28.567296
305.963406	12501.718563	28.572314
306.460829	12521.115244	28.577332
306.821539	12537.962855	28.582349
307.145548	12564.616874	28.587367
307.939873	12574.141939	28.592384
307.705638	12600.507397	28.597402
308.126714	12615.740827	28.602420
308.499833	12630.069810	28.607437
308.679589	12647.885239	28.612455
308.975119	12670.938569	28.617472
309.214040	12700.607411	28.622490
309.572059	12714.040727	28.627508
309.816865	12729.208994	28.632525
310.185707	12759.121108	28.637543
310.805921	12764.206009	28.642560
311.031458	12802.190045	28.647578
311.857715	12802.621806	28.652596
311.983255	12811.782198	28.657613
312.431533	12818.693767	28.662631
312.800119	12834.319064	28.667648
312.656418	12867.132639	28.672666
312.928818	12869.224425	28.677684
313.055923	12880.803592	28.682701
312.912414	12914.602164	28.687719
313.498125	12932.561636	28.692736
313.795424	12971.779108	28.697754
314.000267	12989.894893	28.702772
314.136773	13016.278229	28.707789
314.105833	13043.255176	28.712807
314.940821	13070.378283	28.717824
314.956179	13099.024402	28.722842
315.373734	13134.942809	28.727860
315.714075	13157.466180	28.732877
315.732181	13199.502626	28.737895
316.530901	13219.828740	28.742912
316.679909	13250.731713	28.747930
317.153202	13279.289467	28.752948
317.353258	13297.324441	28.757965
317.758641	13336.055206	28.762983
318.171603	13357.079103	28.768000
318.229639	13384.260888	28.773018
318.707078	13407.820864	28.778036
318.965083	13423.282288	28.783053
318.937053	13455.105468	28.788071
319.446022	13476.220735	28.793088
320.126713	13510.703116	28.798106
320.484614	13526.586159	28.803124
321.016615	13554.307265	28.808141
320.527633	13581.837132	28.813159
320.948779	13597.972924	28.818176
321.628638	13633.725931	28.823194
321.938439	13654.343414	28.828212
322.360971	13681.952118	28.833229
322.824202	13700.244829	28.838247
323.092075	13718.798530	28.843264
323.430383	13738.683285	28.848282
323.462138	13747.913366	28.853300
324.280310	13768.829506	28.858317
324.651087	13805.756334	28.863335
325.129008	13813.612148	28.868352
324.991832	13831.896005	28.873370
325.056127	13852.470996	28.878388
325.690519	13881.168522	28.883405
326.047893	13902.976170	28.888423
326.731865	13916.728268	28.893440
327.056529	13927.451115	28.898458
327.276791	13938.352064	28.903476
328.286286	13952.232932	28.908493
328.352710	13978.523873	28.913511
328.318210	13976.099539	28.918528
328.602170	14003.011574	28.923546
329.095999	14008.169877	28.928564
329.797623	14021.211506	28.933581
329.796484	14043.732941	28.938599
329.862730	14058.962055	28.943616
330.339643	14081.137782	28.948634
330.483155	14105.227043	28.953652
330.947069	14117.731418	28.958669
331.220511	14142.872416	28.963687
331.638841	14156.295330	28.968704
331.902114	14181.362427	28.973722
332.282162	14205.067393	28.978740
332.893094	14218.597054	28.983757
332.551154	14242.426739	28.988775
332.898657	14261.658129	28.993792
333.061689	14288.097426	28.998810
333.338613	14313.871672	29.003828
333.464651	14337.308547	29.008845
333.726601	14375.398942	29.013863
334.200813	14401.841891	29.018880
334.660768	14435.526020	29.023898
334.946817	14475.730848	29.028916
335.105640	14492.429623	29.033933
335.676657	14523.359462	29.038951
335.842337	14550.739645	29.043968
336.505683	14582.716520	29.048986
337.316445	14615.278904	29.054004
337.669443	14629.871467	29.059021
337.768090	14648.686017	29.064039
338.535196	14667.116887	29.069056
339.101149	14686.104448	29.074074
339.095579	14698.900028	29.079092
339.653500	14709.310406	29.084109
340.005198	14725.718904	29.089127
339.964967	14754.002048	29.094144
340.461030	14766.200551	29.099162
340.625004	14792.342626	29.104180
340.875189	14816.992058	29.109197
341.440201	14817.147348	29.114215
342.115144	14841.325933	29.119232
342.499304	14858.677973	29.124250
342.679809	14883.718917	29.129268
342.939639	14885.619198	29.134285
343.049477	14905.042130	29.139303
343.405562	14926.945926	29.144320
343.635153	14952.796812	29.149338
343.785662	14963.751012	29.154356
344.083142	14990.812154	29.159373
344.142431	15016.592137	29.164391
344.407867	15043.203196	29.169408
344.624029	15069.450523	29.174426
344.591816	15107.930347	29.179444
345.014080	15133.163199	29.184461
345.488238	15173.467730	29.189479
345.899049	15200.414249	29.194496
345.842347	15230.187227	29.199514
346.077893	15269.366878	29.204532
347.051818	15308.107164	29.209549
347.227036	15338.932494	29.214567
347.722666	15362.517487	29.219584
348.605987	15399.039659	29.224602
348.331516	15421.318378	29.229620
349.399276	15446.403506	29.234637
349.978159	15474.909730	29.239655
350.176177	15486.679134	29.244672
350.949758	15514.703884	29.249690
351.098316	15533.572627	29.254708
351.652491	15538.546443	29.259725
351.624598	15567.605978	29.264743
351.761438	15584.916335	29.269760
352.045155	15602.046273	29.274778
351.926877	15645.618448	29.279796
352.463177	15664.591581	29.284813
352.397171	15701.434468	29.289831
353.170413	15730.627582	29.294848
353.893158	15755.724788	29.299866
354.357811	15786.208132	29.304884
355.625608	15795.762060	29.309901
356.178595	15814.051687	29.314919
356.682756	15818.687139	29.319936
357.073580	15820.088191	29.324954
356.980876	15837.838869	29.329972
356.889047	15841.334454	29.334989
357.507804	15856.397798	29.340007
357.742742	15880.244354	29.345024
358.087799	15880.437776	29.350042
358.276620	15917.489429	29.355060
358.755312	15925.923024	29.360077
358.684236	15954.642077	29.365095
358.846492	15973.840049	29.370112
359.632427	15998.853050	29.375130
359.474383	16038.178721	29.380148
359.915411	16053.079473	29.385165
360.546065	16083.658738	29.390183
360.639310	16107.010588	29.395200
361.018243	16123.570429	29.400218
361.306537	16163.003519	29.405236
361.772784	16185.038856	29.410253
362.020343	16222.817528	29.415271
362.256041	16252.069339	29.420288
362.845855	16278.770373	29.425306
363.207428	16319.725327	29.430324
363.613063	16338.938464	29.435341
363.376655	16367.367299	29.440359
364.007581	16407.451784	29.445376
363.888175	16424.468274	29.450394
364.367930	16463.882887	29.455412
365.127002	16502.180929	29.460429
365.628704	16539.317561	29.465447
366.093664	16567.472610	29.470464
366.841375	16585.002523	29.475482
367.135746	16612.211863	29.480500
367.462445	16625.082997	29.485517
367.767869	16648.159200	29.490535
368.520939	16661.571126	29.495552
369.298090	16663.565380	29.500570
369.628873	16682.548608	29.505588
369.699999	16695.520572	29.510605
370.000777	16706.484072	29.515623
370.024144	16722.532972	29.520640
370.285441	16738.879686	29.525658
370.631260	16777.868062	29.530676
370.687459	16797.172880	29.535693
371.391679	16829.702190	29.540711
371.477585	16853.965824	29.545728
371.812971	16870.930871	29.550746
371.781876	16909.469876	29.555764
372.282485	16944.783845	29.560781
372.745876	16976.942039	29.565799
373.164582	17008.477202	29.570816
373.902604	17034.190152	29.575834
374.053922	17068.867261	29.580852
374.432885	17097.882394	29.585869
374.598331	17135.580636	29.590887
374.670712	17170.282102	29.595904
375.143729	17195.369393	29.600922
375.726938	17224.967159	29.605940
376.034296	17254.396419	29.610957
376.302956	17292.330083	29.615975
376.938842	17331.206950	29.620992
377.620703	17351.196646	29.626010
377.939726	17387.703472	29.631028
378.508243	17417.225206	29.636045
379.120219	17446.679873	29.641063
379.689180	17464.040222	29.646080
379.971705	17480.336852	29.651098
380.742740	17503.814537	29.656116
380.909111	17513.620223	29.661133
381.533350	17541.750475	29.666151
381.921772	17552.630621	29.671168
382.009649	17574.557267	29.676186
382.402309	17595.939919	29.681204
382.650409	17611.556686	29.686221
383.280424	17629.350022	29.691239
383.123188	17653.852257	29.696256
383.647795	17674.573095	29.701274
383.828110	17715.303088	29.706292
384.312208	17730.029533	29.711309
384.721549	17752.650211	29.716327
384.587521	17786.052073	29.721344
385.144964	17808.120144	29.726362
385.426207	17856.230028	29.731380
386.035621	17885.455751	29.736397
386.256895	17912.829125	29.741415
386.562940	17956.734139	29.746432
386.746704	17986.815780	29.751450
387.043168	18037.095914	29.756468
387.431389	18072.248093	29.761485
388.001872	18104.590888	29.766503
388.399508	18156.616987	29.771520
388.599145	18181.172641	29.776538
388.987886	18228.157534	29.781556
389.541012	18263.495540	29.786573
390.357951	18288.223112	29.791591
390.369749	18333.781206	29.796608
390.930274	18358.554627	29.801626
391.469687	18390.570515	29.806644
391.657710	18428.739289	29.811661
392.454520	18459.870746	29.816679
392.593290	18485.808452	29.821696
393.337563	18515.118504	29.826714
393.134998	18537.234963	29.831732
393.500485	18571.091412	29.836749
394.227889	18599.622502	29.841767
394.844618	18631.547190	29.846784
395.324666	18635.534806	29.851802
395.525916	18668.039344	29.856820
396.312753	18682.856655	29.861837
397.203367	18692.288931	29.866855
397.129987	18706.278055	29.871872
397.301109	18737.969555	29.876890
397.575486	18757.079610	29.881908
398.055441	18786.448233	29.886925
398.567721	18798.137842	29.891943
399.031591	18835.435663	29.896960
399.128876	18852.864780	29.901978
399.733867	18867.794439	29.906996
399.474504	18910.969814	29.912013
400.016083	18933.521263	29.917031
400.366652	18967.969021	29.922048
400.555365	19001.915614	29.927066
400.854279	19042.138864	29.932084
401.229225	19084.523557	29.937101
401.371059	19121.319007	29.942119
401.536306	19174.216114	29.947136
402.345174	19210.145824	29.952154
402.753276	19245.254608	29.957172
403.124856	19287.637222	29.962189
403.934742	19324.432511	29.967207
404.274926	19365.207767	29.972224
404.980095	19393.171637	29.977242
405.436889	19423.495867	29.982260
405.698983	19462.036215	29.987277
406.317674	19486.265637	29.992295
406.734256	19525.627065	29.997312
406.712298	19550.800127	30.002330
407.068889	19588.921479	30.007348
407.489646	19632.658924	30.012365
408.414408	19659.905703	30.017383
408.792521	19694.646772	30.022400
409.449808	19721.255435	30.027418
410.218747	19727.523893	30.032436
411.049049	19749.088868	30.037453
411.773273	19764.513484	30.042471
412.139520	19784.191201	30.047488
412.276165	19789.741746	30.052506
413.028487	19814.978939	30.057524
413.085215	19831.274385	30.062541
413.394618	19849.572675	30.067559
413.672517	19871.374605	30.072576
413.854871	19895.498945	30.077594
414.674514	19924.139956	30.082612
414.423225	19942.116840	30.087629
415.226547	19959.240650	30.092647
415.098939	19985.918618	30.097664
415.649512	20010.730835	30.102682
416.016727	20031.029852	30.107700
416.257999	20070.327085	30.112717
416.600252	20092.041361	30.117735
416.508425	20132.371546	30.122752
417.405478	20168.304437	30.127770
417.847892	20193.642551	30.132788
418.072596	20226.587666	30.137805
419.130568	20252.506293	30.142823
419.520766	20278.237897	30.147840
420.199111	20303.667848	30.152858
420.395912	20326.675751	30.157876
420.737440	20357.485917	30.162893
421.172997	20374.062669	30.167911
421.722572	20407.127606	30.172928
421.953490	20421.083381	30.177946
422.460920	20441.991830	30.182964
422.494011	20484.045844	30.187981
423.000687	20497.476590	30.192999
423.202347	20518.237266	30.198016
423.321963	20547.687753	30.203034
423.827119	20581.310652	30.208052
424.052030	20615.073187	30.213069
424.471946	20657.279383	30.218087
424.629069	20694.741084	30.223104
425.059418	20743.499847	30.228122
425.692117	20783.507864	30.233140
425.976281	20819.644856	30.238157
426.212714	20865.180399	30.243175
426.037687	20914.664561	30.248192
426.641193	20964.257634	30.253210
426.928745	21013.628991	30.258228
427.344054	21067.617843	30.263245
428.545063	21099.213697	30.268263
429.285591	21143.554709	30.273280
429.704880	21182.580586	30.278298
430.763601	21209.236883	30.283316
430.697599	21255.467000	30.288333
431.218199	21289.681584	30.293351
431.699036	21333.679940	30.298368
431.812373	21361.155712	30.303386
432.325293	21404.776823	30.308404
432.740531	21450.752529	30.313421
433.226197	21482.810065	30.318439
433.876998	21520.355581	30.323456
434.010911	21566.007798	30.328474
434.616988	21600.412213	30.333492
435.189546	21639.609204	30.338509
435.512534	21669.493005	30.343527
436.384350	21693.677271	30.348544
437.130011	21726.942435	30.353562
437.885320	21756.295756	30.358580
438.152573	21786.148026	30.363597
438.298542	21809.707217	30.368615
439.183575	21842.156360	30.373632
439.222831	21862.261358	30.378650
440.442330	21875.875974	30.383668
440.416650	21918.665472	30.388685
440.954804	21930.004519	30.393703
441.427530	21956.790868	30.398720
441.468134	21994.180198	30.403738
442.115772	22015.966070	30.408756
442.050198	22041.258891	30.413773
442.825029	22071.733751	30.418791
443.075251	22099.292054	30.423808
443.270423	22135.832952	30.428826
443.507951	22167.294409	30.433844
443.959225	22210.782777	30.438861
444.311708	22240.246418	30.443879
444.530172	22285.101294	30.448896
445.202409	22329.370043	30.453914
445.612575	22366.310923	30.458932
445.939299	22416.122949	30.463949
446.296930	22448.652970	30.468967
446.874923	22490.861147	30.473984
447.321472	22538.488677	30.479002
447.905492	22578.758173	30.484020
447.867650	22633.585734	30.489037
448.551024	22664.515209	30.494055
449.133212	22708.207018	30.499072
449.511651	22754.104074	30.504090
449.949174	22790.342799	30.509108
450.315757	22842.866339	30.514125
451.063605	22861.096658	30.519143
451.672384	22887.513402	30.524160
451.980666	22932.862814	30.529178
452.964279	22947.678043	30.534196
453.069331	22992.682925	30.539213
453.626175	23011.547487	30.544231
454.587091	23049.746594	30.549248
455.455666	23060.148485	30.554266
455.997950	23054.765037	30.559284
456.781944	23074.492329	30.564301
457.947928	23074.989469	30.569319
458.413284	23072.605363	30.574336
458.277684	23083.554071	30.579354
458.691274	23088.525153	30.584372
459.079550	23104.059104	30.589389
459.468310	23123.494149	30.594407
459.764632	23132.518337	30.599424
459.631783	23150.160422	30.604442
460.273585	23186.648326	30.609460
460.661346	23209.997427	30.614477
460.508544	23240.297317	30.619495
461.046634	23271.641520	30.624512
461.381065	23306.312132	30.629530
462.138150	23327.236311	30.634548
462.309846	23369.993528	30.639565
462.785716	23394.028386	30.644583
463.322001	23434.987483	30.649600
463.431807	23476.157853	30.654618
463.699052	23512.798548	30.659636
463.971209	23559.087579	30.664653
464.351856	23610.160403	30.669671
464.627318	23647.930667	30.674688
464.508834	23708.015159	30.679706
465.268658	23760.274376	30.684724
466.093322	23812.534023	30.689741
466.496914	23863.193792	30.694759
467.091304	23923.001373	30.699776
467.580184	23963.927037	30.704794
468.638744	24006.697827	30.709812
469.117691	24051.977721	30.714829
469.404993	24091.470607	30.719847
469.826632	24145.789902	30.724864
469.922653	24189.963655	30.729882
470.538933	24236.432336	30.734900
470.925618	24296.274144	30.739917
471.145933	24343.496438	30.744935
471.927143	24400.462915	30.749952
472.555464	24427.741418	30.754970
473.285377	24474.898364	30.759988
473.935938	24515.773266	30.765005
475.368036	24540.735902	30.770023
476.065110	24567.060167	30.775040
476.099680	24595.080962	30.780058
476.629834	24623.833230	30.785076
476.944078	24650.801542	30.790093
477.080441	24686.577061	30.795111
477.775791	24714.885716	30.800128
477.624254	24757.146554	30.805146
477.968361	24800.375474	30.810164
478.657358	24834.801060	30.815181
479.252148	24871.068557	30.820199
479.980825	24909.442883	30.825216
480.728073	24947.161319	30.830234
480.885787	24981.583969	30.835252
481.536734	25023.358930	30.840269
481.874359	25057.411212	30.845287
482.465924	25086.122518	30.850304
482.367728	25121.206150	30.855322
483.335665	25156.374582	30.860340
483.925896	25178.648744	30.865357
484.225440	25207.143806	30.870375
485.163861	25232.735111	30.875392
484.961307	25262.023327	30.880410
485.804707	25289.567129	30.885428
486.184215	25322.799218	30.890445
486.562540	25356.706553	30.895463
487.073436	25387.371557	30.900480
487.323583	25431.289504	30.905498
487.709910	25464.258939	30.910516
488.610563	25506.845233	30.915533
488.631897	25540.547269	30.920551
489.182464	25577.416590	30.925568
489.494262	25630.175434	30.930586
489.662186	25665.758500	30.935604
490.073918	25715.523450	30.940621
490.459017	25763.785252	30.945639
491.146242	25804.493122	30.950656
491.320266	25858.635016	30.955674
491.723281	25919.697306	30.960692
492.179966	25975.010160	30.965709
492.621347	26040.573932	30.970727
493.183389	26089.633678	30.975744
493.463986	26151.177642	30.980762
493.735601	26209.395535	30.985780
494.327738	26269.582304	30.990797
495.178443	26345.406455	30.995815
495.704088	26388.596601	31.000832
496.211749	26459.677340	31.005850
496.731599	26517.085386	31.010868
497.387617	26571.408125	31.015885
497.812623	26627.135242	31.020903
498.351289	26681.607146	31.025920
499.204974	26740.966681	31.030938
499.674004	26784.321785	31.035956
500.477221	26838.835418	31.040973
501.222514	26891.327398	31.045991
501.880101	26925.724539	31.051008
502.252557	26972.417763	31.056026
502.954911	27005.142087	31.061044
503.533013	27045.902556	31.066061
504.077652	27083.365966	31.071079
504.502964	27127.792242	31.076096
504.994768	27172.775394	31.081114
505.220091	27220.957397	31.086132
506.148059	27262.253315	31.091149
506.052776	27311.280588	31.096167
506.418653	27351.660629	31.101184
507.015277	27413.270161	31.106202
507.608106	27455.707350	31.111220
507.883047	27509.727244	31.116237
508.311494	27563.321185	31.121255
508.733792	27605.941636	31.126272
509.425674	27657.930619	31.131290
510.011362	27712.479976	31.136308
510.696984	27755.268419	31.141325
510.900491	27809.197006	31.146343
511.882535	27856.649424	31.151360
512.503015	27905.155717	31.156378
512.741069	27946.529986	31.161396
513.743708	27990.439878	31.166413
514.233310	28026.179426	31.171431
514.903456	28059.207628	31.176448
515.381487	28111.845485	31.181466
515.862667	28149.009427	31.186484
516.238079	28189.358286	31.191501
516.855985	28215.584564	31.196519
517.499446	28252.469406	31.201536
517.994314	28283.924574	31.206554
518.190512	28317.464166	31.211572
518.337530	28362.242667	31.216589
518.834767	28405.452024	31.221607
518.916589	28447.067948	31.226624
519.301664	28488.926999	31.231642
519.674468	28552.574671	31.236660
520.463841	28598.818155	31.241677
521.141274	28645.932131	31.246695
521.559429	28707.667377	31.251712
522.400048	28745.949624	31.256730
522.898903	28792.159844	31.261748
524.054125	28831.727656	31.266765
524.575587	28881.884133	31.271783
524.772669	28924.803908	31.276800
525.340355	28969.965244	31.281818
525.552497	29008.286186	31.286836
526.570253	29043.154569	31.291853
526.843566	29090.106556	31.296871
527.428118	29134.013054	31.301888
528.357118	29185.446681	31.306906
528.559227	29226.511320	31.311924
528.916417	29268.629260	31.316941
529.131866	29321.121927	31.321959
529.744087	29374.255553	31.326976
530.176076	29422.737432	31.331994
530.549365	29479.460293	31.337012
531.025365	29531.415005	31.342029
531.536314	29596.576819	31.347047
531.814395	29652.457914	31.352064
532.399150	29701.199138	31.357082
532.849932	29764.365034	31.362100
533.911829	29811.528734	31.367117
534.865562	29872.847884	31.372135
535.366904	29927.336148	31.377152
536.128950	29961.409612	31.382170
536.706396	30017.573430	31.387188
537.582044	30055.480448	31.392205
538.152549	30092.923956	31.397223
539.315691	30128.010146	31.402240
540.118769	30149.002831	31.407258
540.438728	30192.596255	31.412276
541.209746	30210.234246	31.417293
541.067742	30250.124815	31.422311
541.372174	30284.965852	31.427328
541.647997	30325.279391	31.432346
542.349471	30380.534055	31.437364
542.769286	30414.274006	31.442381
543.206679	30465.969720	31.447399
543.794076	30507.096424	31.452416
544.610811	30549.620700	31.457434
544.733220	30605.839880	31.462452
545.218457	30633.158247	31.467469
545.165367	30694.944046	31.472487
545.693311	30751.689508	31.477504
546.168192	30807.008381	31.482522
546.330626	30877.378834	31.487540
546.772935	30939.382960	31.492557
547.564173	31008.097182	31.497575
548.483041	31060.039668	31.502592
549.057983	31117.191830	31.507610
549.677566	31181.824034	31.512628
550.197436	31220.619311	31.517645
550.936138	31288.731243	31.522663
551.506396	31346.121565	31.527680
551.932494	31401.384146	31.532698
552.186413	31458.294129	31.537716
552.919819	31503.437624	31.542733
553.562749	31553.657294	31.547751
554.075987	31606.356596	31.552768
554.730191	31653.245869	31.557786
555.247008	31705.323283	31.562804
556.117835	31743.657555	31.567821
556.834848	31790.811274	31.572839
556.894291	31840.002208	31.577856
557.259353	31879.562983	31.582874
557.609182	31943.485494	31.587892
558.243896	31996.273068	31.592909
559.192722	32054.543118	31.597927
559.193690	32108.423888	31.602944
559.886734	32180.727689	31.607962
559.863376	32239.020948	31.612980
560.304766	32302.636098	31.617997
560.639357	32367.600792	31.623015
561.424511	32445.163055	31.628032
562.287771	32516.591153	31.633050
562.756169	32585.008551	31.638068
563.288664	32643.901877	31.643085
564.178435	32714.016855	31.648103
564.695260	32788.668507	31.653120
565.529260	32848.834592	31.658138
566.211502	32907.180114	31.663156
567.178705	32966.131699	31.668173
567.900913	33020.996743	31.673191
568.873966	33071.579271	31.678208
570.383271	33086.970735	31.683226
571.098788	33126.741163	31.688244
572.112005	33152.622030	31.693261
572.271221	33182.683845	31.698279
572.525297	33227.422223	31.703296
573.131108	33255.362047	31.708314
573.553974	33300.429159	31.713332
573.835992	33347.271118	31.718349
574.628539	33384.801495	31.723367
574.522753	33421.089507	31.728384
575.114230	33473.156558	31.733402
575.755106	33533.659970	31.738420
576.222108	33576.763973	31.743437
577.213488	33629.386734	31.748455
577.200950	33676.082819	31.753472
578.037163	33714.452352	31.758490
578.764998	33766.301968	31.763508
578.996500	33820.963798	31.768525
579.564108	33866.222890	31.773543
580.161471	33924.585843	31.778560
580.712960	33977.330011	31.783578
580.855141	34042.967061	31.788596
581.022914	34096.204471	31.793613
581.929442	34160.105619	31.798631
582.234263	34233.485747	31.803648
582.997407	34297.086153	31.808666
583.376767	34347.688844	31.813684
583.777556	34419.535881	31.818701
585.143210	34466.718384	31.823719
586.702243	34507.383769	31.828736
587.910649	34546.037271	31.833754
588.491529	34592.337410	31.838772
588.942122	34635.263658	31.843789
589.385042	34663.759759	31.848807
589.647367	34717.784893	31.853824
590.233449	34758.451462	31.858842
590.523422	34802.080126	31.863860
590.850007	34852.743501	31.868877
591.717353	34898.403566	31.873895
591.856859	34953.406026	31.878912
592.576633	34995.824528	31.883930
592.954944	35041.177988	31.888948
593.582835	35079.903793	31.893965
594.042670	35138.104188	31.898983
593.925549	35192.670296	31.904000
594.729146	35240.146993	31.909018
595.122527	35306.479127	31.914036
595.458862	35377.236130	31.919053
596.228982	35432.602422	31.924071
596.547629	35499.468407	31.929088
597.498756	35564.834682	31.934106
597.684111	35622.637229	31.939124
598.298150	35707.639690	31.944141
599.097697	35766.562084	31.949159
599.174888	35846.929808	31.954176
599.950370	35920.099809	31.959194
600.695516	35992.397766	31.964212
601.322364	36058.649718	31.969229
602.905181	36115.155056	31.974247
603.663966	36179.438255	31.979264
604.685614	36208.364622	31.984282
605.365240	36269.176973	31.989300
605.934069	36322.963510	31.994317
607.023246	36367.422720	31.999335
606.711538	36417.839843	32.004352
607.230097	36469.141830	32.009370
607.668470	36526.668550	32.014388
608.487561	36604.814472	32.019405
609.285906	36649.010209	32.024423
609.667106	36715.791410	32.029440
610.364641	36779.398871	32.034458
610.921261	36834.445116	32.039476
611.497208	36892.827579	32.044493
612.188654	36942.969128	32.049511
613.050537	37010.675278	32.054528
613.759007	37054.539746	32.059546
614.149780	37114.348723	32.064564
614.426008	37174.397853	32.069581
615.356828	37241.118137	32.074599
615.886084	37302.956310	32.079616
616.780387	37354.668703	32.084634
617.372402	37418.318023	32.089652
617.947469	37464.639136	32.094669
619.059271	37517.313271	32.099687
619.634687	37569.669455	32.104704
620.032327	37623.573502	32.109722
620.557505	37678.504435	32.114740
620.965153	37741.232286	32.119757
621.369801	37804.510058	32.124775
621.925585	37869.038127	32.129792
622.319050	37936.471996	32.134810
623.068692	38006.918145	32.139828
623.129103	38075.004384	32.144845
623.893590	38144.230227	32.149863
624.014069	38230.191336	32.154880
625.095065	38294.750497	32.159898
625.591668	38373.497333	32.164916
625.943396	38459.092852	32.169933
626.756675	38523.488947	32.174951
627.425746	38612.593007	32.179968
628.117123	38688.531145	32.184986
628.472546	38760.863812	32.190004
628.857332	38842.914022	32.195021
629.962868	38917.512261	32.200039
630.338681	39007.888524	32.205056
630.930206	39088.349321	32.210074
631.706233	39162.217282	32.215092
632.402970	39236.300729	32.220109
633.074736	39311.925894	32.225127
633.833453	39376.697068	32.230144
634.867866	39433.587917	32.235162
635.574608	39495.571360	32.240180
636.203584	39552.580402	32.245197
636.965443	39608.137588	32.250215
637.529777	39674.349963	32.255232
638.127741	39743.978848	32.260250
638.890095	39804.397853	32.265268
639.214020	39873.804411	32.270285
640.226142	39917.508561	32.275303
641.055967	39985.890843	32.280320
641.489738	40046.223147	32.285338
642.544710	40093.626621	32.290356
643.192085	40149.027676	32.295373
644.371415	40194.803973	32.300391
645.101997	40240.721184	32.305408
645.149940	40307.091029	32.310426
645.736071	40367.828416	32.315444
645.977392	40427.767757	32.320461
646.842047	40494.277318	32.325479
647.178359	40559.495305	32.330496
647.690080	40637.996812	32.335514
647.943488	40703.295366	32.340532
648.399219	40788.755052	32.345549
649.172375	40857.030021	32.350567
649.817037	40928.098330	32.355584
650.294077	41013.422929	32.360602
651.285367	41082.881084	32.365620
651.372689	41176.747477	32.370637
651.946849	41260.617529	32.375655
652.827510	41350.583686	32.380672
653.067522	41428.357048	32.385690
653.971574	41509.758367	32.390708
654.711592	41598.382102	32.395725
655.502240	41680.023990	32.400743
656.395388	41764.215890	32.405760
657.075170	41853.125507	32.410778
658.139243	41929.277182	32.415796
658.403053	42008.750687	32.420813
659.381356	42083.572321	32.425831
660.216585	42161.995012	32.430848
660.862221	42240.294813	32.435866
661.976171	42308.565915	32.440884
662.568651	42380.254631	32.445901
663.830777	42434.824863	32.450919
664.764916	42491.527123	32.455936
665.401257	42552.591694	32.460954
666.080883	42618.129320	32.465972
666.585132	42677.183006	32.470989
666.976627	42737.707912	32.476007
667.592821	42802.284301	32.481024
667.992200	42870.060449	32.486042
668.442503	42924.975284	32.491060
669.159874	43009.473538	32.496077
669.901932	43078.162825	32.501095
670.236800	43154.926812	32.506112
670.940306	43231.816192	32.511130
671.914923	43298.267051	32.516148
672.423383	43373.042433	32.521165
672.902313	43439.623452	32.526183
673.421463	43515.960505	32.531200
673.972379	43599.510292	32.536218
674.981330	43671.387420	32.541236
675.122757	43757.042393	32.546253
675.682251	43835.123237	32.551271
676.489297	43907.599966	32.556288
676.803061	44002.128161	32.561306
677.673898	44067.850680	32.566324
678.316485	44149.603757	32.571341
679.245455	44218.108331	32.576359
680.209663	44294.971430	32.581376
680.429234	44376.918869	32.586394
681.486485	44439.337438	32.591412
682.056873	44518.543387	32.596429
683.006754	44586.269090	32.601447
683.574465	44658.501125	32.606464
684.307697	44730.273375	32.611482
684.966107	44793.693973	32.616500
685.517777	44869.769063	32.621517
686.549286	44940.371662	32.626535
687.490201	45015.965922	32.631552
687.870757	45092.989181	32.636570
688.704198	45168.118783	32.641588
689.068973	45239.464718	32.646605
689.408167	45329.097890	32.651623
690.498625	45391.043623	32.656640
691.369426	45468.293318	32.661658
692.410707	45537.425065	32.666676
692.996141	45610.052519	32.671693
693.961686	45673.819803	32.676711
695.205958	45731.986623	32.681728
695.994431	45804.126406	32.686746
696.694560	45862.797630	32.691764
697.297603	45916.767494	32.696781
698.211223	45974.307885	32.701799
698.979930	46029.867336	32.706816
699.261216	46100.257797	32.711834
699.984328	46163.640687	32.716852
700.016553	46230.356275	32.721869
700.559988	46305.074357	32.726887
701.046429	46370.969791	32.731904
702.092336	46455.425846	32.736922
703.014872	46522.534644	32.741940
703.831834	46608.358841	32.746957
704.115610	46677.389997	32.751975
704.683484	46749.816323	32.756992
705.361867	46820.860373	32.762010
706.790920	46897.543232	32.767028
707.688641	46963.738764	32.772045
707.958396	47040.109395	32.777063
708.845724	47110.384044	32.782080
709.302380	47185.293685	32.787098
710.183824	47259.855200	32.792116
710.770452	47339.736607	32.797133
711.063896	47407.259297	32.802151
711.734588	47480.719791	32.807168
712.246103	47568.351721	32.812186
713.005060	47647.267880	32.817204
713.554166	47737.142858	32.822221
714.263916	47822.633477	32.827239
715.194917	47898.304057	32.832256
715.921891	47985.387369	32.837274
716.619463	48066.788232	32.842292
717.463266	48149.330507	32.847309
717.975729	48240.515078	32.852327
719.872873	48295.287465	32.857344
720.484602	48376.710216	32.862362
722.499481	48409.290065	32.867380
723.493488	48471.325047	32.872397
723.679382	48517.052956	32.877415
724.653552	48573.798475	32.882432
725.173576	48623.485213	32.887450
725.611570	48674.910073	32.892468
726.472666	48728.924037	32.897485
726.766782	48783.638655	32.902503
727.865114	48830.842319	32.907520
727.797021	48891.179000	32.912538
728.556785	48947.708564	32.917556
728.787725	49005.993640	32.922573
729.615665	49079.551033	32.927591
730.150720	49137.369132	32.932608
730.146744	49215.916256	32.937626
730.724894	49292.920563	32.942644
731.223950	49372.809212	32.947661
731.619282	49459.458429	32.952679
732.453567	49551.906516	32.957696
733.057242	49650.091000	32.962714
733.419318	49750.015296	32.967732
734.870766	49822.271844	32.972749
736.499633	49892.297811	32.977767
737.543935	49974.745177	32.982784
738.424607	50046.080314	32.987802
739.362528	50122.045946	32.992820
740.137649	50179.713621	32.997837
740.631228	50264.748821	33.002855
741.187563	50324.304103	33.007872
741.678009	50409.451006	33.012890
742.621507	50474.435074	33.017908
743.666428	50555.207664	33.022925
744.185421	50631.355393	33.027943
744.921342	50704.612103	33.032960
745.595641	50775.712563	33.037978
746.406384	50861.541066	33.042996
747.722336	50920.052946	33.048013
748.253309	50995.833728	33.053031
749.364707	51070.349777	33.058048
750.184469	51136.942226	33.063066
750.984300	51211.017796	33.068084
751.918626	51266.460737	33.073101
752.396218	51342.333860	33.078119
752.703928	51411.254881	33.083136
753.373950	51488.726490	33.088154
754.084775	51571.428705	33.093172
754.446440	51648.857381	33.098189
754.839326	51744.911160	33.103207
755.682647	51824.338999	33.108224
756.598269	51911.525618	33.113242
756.821498	52002.845479	33.118260
757.654972	52100.571497	33.123277
758.679627	52186.439841	33.128295
759.165800	52280.869804	33.133312
759.676566	52377.406219	33.138330
760.542166	52474.168502	33.143348
761.194221	52578.276245	33.148365
761.910342	52673.655492	33.153383
763.469214	52769.337548	33.158400
763.711141	52864.992294	33.163418
764.351612	52948.906086	33.168436
765.584307	53043.373757	33.173453
766.707697	53129.034006	33.178471
767.886889	53226.657727	33.183488
768.440474	53313.095699	33.188506
768.870632	53401.866902	33.193524
769.881694	53475.315811	33.198541
770.491358	53572.018604	33.203559
771.202196	53658.665760	33.208576
771.611119	53760.899474	33.213594
772.043751	53856.337854	33.218612
772.910194	53953.530618	33.223629
773.423997	54065.225661	33.228647
774.473200	54156.468994	33.233664
775.021605	54255.434584	33.238682
775.605967	54349.535982	33.243700
776.630299	54434.314865	33.248717
777.253168	54535.379798	33.253735
777.813356	54630.112059	33.258752
778.709513	54725.547207	33.263770
779.275160	54818.257592	33.268788
780.059946	54916.801840	33.273805
781.031204	55035.307190	33.278823
781.539149	55117.830583	33.283840
782.163778	55219.461066	33.288858
782.941040	55336.149097	33.293876
783.932246	55439.823938	33.298893
784.666135	55548.299949	33.303911
785.781166	55644.436158	33.308928
786.348532	55747.709066	33.313946
787.038415	55859.498752	33.318964
788.123208	55972.506220	33.323981
788.911062	56076.875295	33.328999
789.694966	56178.591672	33.334016
790.978658	56271.966880	33.339034
791.625940	56368.146324	33.344052
792.530967	56468.833060	33.349069
793.110991	56577.295996	33.354087
794.343244	56663.338973	33.359104
795.467822	56769.766324	33.364122
796.021330	56865.761528	33.369140
797.375093	56936.600891	33.374157
798.195676	57023.465725	33.379175
799.362223	57104.440975	33.384192
800.689361	57186.691639	33.389210
801.487705	57266.780796	33.394228
802.457863	57350.026623	33.399245
802.750517	57433.600108	33.404263
803.358976	57524.331772	33.409280
804.045487	57603.733087	33.414298
804.523059	57700.383148	33.419316
805.113136	57782.960826	33.424333
805.754463	57865.846305	33.429351
806.653467	57971.142098	33.434368
807.756646	58060.504918	33.439386
808.311293	58165.410211	33.444404
809.071039	58254.420136	33.449421
809.237773	58367.448195	33.454439
810.056239	58469.145211	33.459456
810.907281	58575.595968	33.464474
811.366136	58690.713367	33.469492
812.372699	58804.217477	33.474509
812.610111	58930.223825	33.479527
813.330490	59045.457829	33.484544
814.374919	59159.558027	33.489562
815.013201	59292.420224	33.494580
815.940472	59403.318150	33.499597
816.841078	59534.135008	33.504615
817.368496	59646.092854	33.509632
818.317562	59766.412131	33.514650
819.554258	59880.446564	33.519668
820.993272	59992.438294	33.524685
822.106979	60091.781349	33.529703
824.166437	60171.287215	33.534720
825.403747	60265.409193	33.539738
826.165418	60348.272253	33.544756
826.981135	60430.418824	33.549773
827.607246	60502.560766	33.554791
828.464624	60587.715780	33.559808
829.260436	60658.414384	33.564826
830.025971	60742.175880	33.569844
830.529624	60829.217168	33.574861
831.171709	60925.046347	33.579879
831.813018	61014.372487	33.584896
832.759420	61087.632602	33.589914
833.175928	61178.488376	33.594932
833.774243	61267.487780	33.599949
834.141639	61359.913654	33.604967
835.128452	61459.543592	33.609984
835.726305	61556.779902	33.615002
836.200406	61660.610564	33.620020
836.977967	61767.349406	33.625037
837.609850	61869.233486	33.630055
838.324246	61989.876640	33.635072
838.800231	62091.345256	33.640090
839.241283	62220.928309	33.645108
841.039237	62333.549650	33.650125
842.059431	62458.721018	33.655143
842.757027	62563.543120	33.660160
844.331313	62663.675564	33.665178
845.241385	62764.399127	33.670196
846.217918	62872.027218	33.675213
846.647623	62981.213088	33.680231
847.216938	63101.267395	33.685248
848.321487	63201.164375	33.690266
848.804086	63320.842450	33.695284
849.434405	63442.146502	33.700301
850.447114	63554.247471	33.705319
851.203924	63681.973148	33.710336
851.743555	63809.242607	33.715354
852.571847	63936.913745	33.720372
852.914186	64067.700533	33.725389
854.046602	64192.528769	33.730407
855.006135	64340.573149	33.735424
856.091093	64470.720871	33.740442
856.187619	64612.892467	33.745460
857.108810	64742.354750	33.750477
858.465531	64862.193752	33.755495
859.024462	65011.504165	33.760512
860.113393	65147.205786	33.765530
860.547047	65280.899302	33.770548
861.384756	65424.641295	33.775565
862.387037	65558.912313	33.780583
863.416589	65711.120829	33.785600
864.773855	65839.828480	33.790618
865.123215	65982.605943	33.795636
866.060252	66132.980583	33.800653
866.803600	66271.300907	33.805671
867.913863	66421.048279	33.810688
868.944408	66552.273785	33.815706
869.765416	66684.084908	33.820724
870.788234	66830.081765	33.825741
871.676488	66964.108863	33.830759
872.974145	67092.606501	33.835776
873.744622	67211.336083	33.840794
874.958001	67343.927073	33.845812
876.199494	67468.364795	33.850829
877.245279	67594.523795	33.855847
878.220149	67721.643674	33.860864
880.092740	67808.986517	33.865882
881.279006	67905.541597	33.870900
882.558920	68006.115302	33.875917
883.432755	68099.637765	33.880935
884.189897	68197.333898	33.885952
884.954922	68289.977465	33.890970
885.631017	68393.093723	33.895988
886.451185	68480.512852	33.901005
887.542257	68574.835943	33.906023
888.029481	68674.260890	33.911040
888.786958	68777.890293	33.916058
889.231583	68889.494486	33.921076
890.026758	68985.664163	33.926093
891.009040	69091.268417	33.931111
891.412539	69198.410853	33.936128
892.536134	69292.358688	33.941146
893.071284	69394.788718	33.946164
894.203915	69488.356546	33.951181
895.468522	69592.424228	33.956199
895.772801	69697.606564	33.961216
896.723422	69808.796478	33.966234
897.780192	69905.072320	33.971252
898.808097	70015.302031	33.976269
900.102265	70115.959238	33.981287
900.649776	70226.130655	33.986304
901.371943	70327.459190	33.991322
901.484981	70443.091147	33.996340
902.546348	70562.082045	34.001357
903.441097	70689.599701	34.006375
903.926974	70818.855319	34.011392
904.828687	70942.882869	34.016410
905.357511	71070.823946	34.021428
906.006573	71214.080075	34.026445
907.504575	71338.188000	34.031463
908.393074	71476.663560	34.036480
909.522361	71593.568472	34.041498
911.015231	71727.265942	34.046516
912.158334	71835.601460	34.051533
913.394177	71955.443765	34.056551
914.116672	72077.673740	34.061568
915.610081	72194.603688	34.066586
916.410461	72296.232047	34.071604
917.310888	72405.502342	34.076621
918.492278	72516.927238	34.081639
919.440527	72637.693734	34.086656
920.452459	72740.471624	34.091674
921.131078	72854.745216	34.096692
923.160143	72926.033021	34.101709
924.936853	73005.350059	34.106727
925.500464	73098.477850	34.111744
926.391990	73197.926195	34.116762
927.029757	73297.246358	34.121780
926.984035	73396.522301	34.126797
927.966512	73505.556852	34.131815
928.461063	73619.397027	34.136832
929.307996	73723.161885	34.141850
929.955996	73844.161984	34.146868
930.148411	73973.017132	34.151885
930.986079	74106.053794	34.156903
931.225702	74240.278289	34.161920
932.432209	74384.778284	34.166938
933.253938	74526.123984	34.171956
933.697205	74672.681469	34.176973
934.768476	74820.584013	34.181991
935.212827	74983.289719	34.187008
936.102182	75133.697438	34.192026
937.803568	75276.584315	34.197044
939.051827	75412.533313	34.202061
940.736422	75551.111370	34.207079
941.703398	75692.421490	34.212096
942.566127	75825.875513	34.217114
943.542579	75956.851132	34.222132
944.192095	76091.354105	34.227149
945.080410	76231.883803	34.232167
945.764051	76371.727320	34.237184
946.983779	76496.853187	34.242202
948.178205	76630.370867	34.247220
949.034766	76780.599169	34.252237
950.394201	76906.532742	34.257255
951.118716	77048.650760	34.262272
951.619476	77180.604388	34.267290
952.665048	77305.156502	34.272308
953.462218	77449.921592	34.277325
954.276604	77562.520930	34.282343
955.840483	77684.300929	34.287360
957.120447	77797.754010	34.292378
958.123354	77920.513933	34.297396
958.557196	78052.958226	34.302413
959.531913	78172.302184	34.307431
960.340613	78297.411503	34.312448
961.420291	78425.816406	34.317466
962.522511	78555.970471	34.322484
963.743728	78673.435471	34.327501
965.181301	78790.131417	34.332519
966.547635	78914.961881	34.337536
967.277764	79025.861999	34.342554
968.033756	79142.767767	34.347572
968.642904	79271.464338	34.352589
969.737922	79388.093722	34.357607
971.173595	79513.681421	34.362624
972.906770	79608.027862	34.367642
974.459354	79702.176938	34.372660
975.525423	79799.114610	34.377677
976.857794	79891.574060	34.382695
977.868649	79997.681638	34.387712
978.027673	80093.126350	34.392730
979.267227	80191.485561	34.397748
979.793895	80317.348770	34.402765
980.376113	80418.658424	34.407783
981.234477	80535.832767	34.412800
982.007577	80650.801402	34.417818
982.625005	80777.297365	34.422836
982.968841	80914.827993	34.427853
983.962958	81052.770296	34.432871
984.760357	81198.887966	34.437888
985.386064	81333.692020	34.442906
986.120522	81480.960675	34.447924
986.843637	81645.262764	34.452941
988.334479	81784.455611	34.457959
989.488049	81944.633193	34.462976
990.330681	82090.692129	34.467994
991.084482	82242.346747	34.473012
992.044607	82406.393546	34.478029
992.831736	82564.776256	34.483047
993.770850	82727.822905	34.488064
994.680452	82876.779680	34.493082
995.807885	83045.864659	34.498100
996.974128	83208.725188	34.503117
997.622529	83376.696319	34.508135
998.554761	83544.608921	34.513152
999.771868	83709.767541	34.518170
1000.784936	83879.428055	34.523188
1001.590950	84053.344306	34.528205
1002.921605	84217.342517	34.533223
1003.328311	84388.075418	34.538240
1004.360973	84558.857559	34.543258
1005.251370	84733.808895	34.548276
1006.586875	84909.421654	34.553293
1007.371926	85088.385646	34.558311
1008.546065	85253.688939	34.563328
1009.491046	85438.133888	34.568346
1010.636563	85604.355563	34.573364
1012.232929	85769.301386	34.578381
1013.547071	85923.683905	34.583399
1014.612098	86092.339531	34.588416
1015.612354	86254.964224	34.593434
1017.092741	86398.407119	34.598452
1017.983425	86563.266818	34.603469
1018.457199	86706.024377	34.608487
1020.104662	86849.853614	34.613504
1021.030230	86988.254003	34.618522
1022.463545	87126.482366	34.623540
1023.339266	87256.679029	34.628557
1024.468797	87396.794478	34.633575
1025.903648	87526.811267	34.638592
1026.786510	87651.269447	34.643610
1027.704284	87786.473841	34.648628
1028.273808	87933.519685	34.653645
1029.094721	88075.721682	34.658663
1030.309950	88227.756354	34.663680
1031.147294	88361.351036	34.668698
1032.528097	88497.374934	34.673716
1033.495646	88659.325519	34.678733
1034.599528	88795.618563	34.683751
1035.622676	88940.595628	34.688768
1036.624669	89089.342480	34.693786
1037.682848	89231.277872	34.698804
1038.434378	89388.276123	34.703821
1039.074780	89549.907331	34.708839
1040.143139	89714.917688	34.713856
1040.535409	89879.250285	34.718874
1041.401006	90038.417242	34.723892
1042.428274	90220.025278	34.728909
1043.474034	90400.720282	34.733927
1044.392659	90578.798633	34.738944
1045.236037	90767.257419	34.743962
1046.468607	90944.678818	34.748980
1047.670196	91134.669591	34.753997
1048.366767	91313.942082	34.759015
1050.018316	91482.772785	34.764032
1050.772106	91678.930658	34.769050
1052.540792	91840.896368	34.774068
1053.736807	92010.230384	34.779085
1054.989113	92184.068967	34.784103
1056.213019	92341.153652	34.789120
1057.070187	92521.971752	34.794138
1058.482609	92682.673039	34.799156
1060.445298	92837.328145	34.804173
1061.534011	92992.338111	34.809191
1062.981984	93125.047754	34.814208
1064.751600	93269.142137	34.819226
1066.341618	93396.228092	34.824244
1067.853331	93536.645086	34.829261
1069.162791	93655.727743	34.834279
1070.521832	93760.871268	34.839296
1071.182036	93886.791152	34.844314
1072.064655	93997.034145	34.849332
1072.781595	94140.415828	34.854349
1073.285953	94260.293289	34.859367
1074.248945	94386.266771	34.864384
1074.543252	94535.322726	34.869402
1075.339468	94679.264076	34.874420
1076.217932	94845.625754	34.879437
1077.139639	94995.460249	34.884455
1077.908473	95159.506483	34.889472
1078.478876	95337.120304	34.894490
1079.313443	95499.872892	34.899508
1080.340051	95681.926826	34.904525
1081.094471	95854.930825	34.909543
1082.100747	96042.156176	34.914560
1083.019999	96223.909050	34.919578
1084.113231	96395.012158	34.924596
1085.762578	96572.658365	34.929613
1086.956099	96749.704113	34.934631
1088.659652	96912.853517	34.939648
1089.581485	97094.207153	34.944666
1090.638295	97259.795731	34.949684
1091.602568	97417.114069	34.954701
1093.189077	97567.018333	34.959719
1095.032510	97701.541774	34.964736
1096.193467	97851.227131	34.969754
1096.890752	97997.153904	34.974772
1098.067211	98145.021526	34.979789
1098.786770	98305.962887	34.984807
1099.791503	98452.252786	34.989824
1100.707932	98607.263094	34.994842
1101.800703	98768.037856	34.999860
1102.469093	98921.464202	35.004877
1103.297654	99096.896661	35.009895
1105.223048	99257.042576	35.014912
1105.695398	99427.439957	35.019930
1106.649448	99592.218857	35.024948
1107.511688	99771.746604	35.029965
1108.443520	99955.613592	35.034983
1109.490624	100127.775339	35.040000
1110.369195	100327.570543	35.045018
1111.264957	100515.600861	35.050036
1112.573628	100709.578856	35.055053
1113.382775	100899.361155	35.060071
1114.711936	101098.809037	35.065088
1115.542180	101303.476097	35.070106
1116.642175	101496.215687	35.075124
1117.646931	101706.169175	35.080141
1119.042625	101911.443732	35.085159
1120.370878	102110.741309	35.090176
1122.115755	102313.934987	35.095194
1123.697997	102499.497827	35.100212
1125.424319	102672.159110	35.105229
1126.082702	102858.080402	35.110247
1127.392494	103032.997690	35.115264
1128.255244	103226.701324	35.120282
1129.332618	103423.467155	35.125300
1130.290265	103600.998486	35.130317
1131.562643	103804.351857	35.135335
1132.417705	103999.075636	35.140352
1133.212845	104197.344181	35.145370
1134.460092	104401.922147	35.150388
1135.385608	104591.940097	35.155405
1136.956913	104793.085895	35.160423
1138.762046	104976.653669	35.165440
1139.947822	105170.178767	35.170458
1140.965855	105354.892945	35.175476
1142.104924	105545.667575	35.180493
1143.138067	105750.418181	35.185511
1144.435946	105932.708915	35.190528
1145.135504	106125.599742	35.195546
1146.564596	106319.726149	35.200564
1147.720309	106517.433013	35.205581
1149.194019	106701.903662	35.210599
1150.441948	106899.560068	35.215616
1151.109872	107094.629002	35.220634
1152.427877	107290.085486	35.225652
1153.815932	107465.886808	35.230669
1154.968601	107653.051812	35.235687
1156.875903	107827.806749	35.240704
1158.133224	108031.144398	35.245722
1158.911570	108206.633733	35.250740
1160.292960	108381.314852	35.255757
1161.571520	108560.295443	35.260775
1163.019362	108726.734546	35.265792
1163.808766	108909.332576	35.270810
1165.036558	109074.480324	35.275828
1166.472427	109251.729388	35.280845
1167.564075	109429.226717	35.285863
1168.424097	109597.998067	35.290880
1169.702922	109762.166179	35.295898
1171.044635	109918.179873	35.300916
1172.102705	110066.869193	35.305933
1173.407693	110232.353191	35.310951
1174.904774	110384.201577	35.315968
1175.698438	110554.750625	35.320986
1176.548572	110715.233358	35.326004
1177.810893	110872.101732	35.331021
1178.514494	111055.513774	35.336039
1179.550312	111213.612436	35.341056
1180.291938	111393.334111	35.346074
1181.120866	111572.510426	35.351092
1182.651349	111758.741615	35.356109
1183.688537	111950.427158	35.361127
1185.021380	112141.330234	35.366144
1185.638517	112332.099985	35.371162
1186.965954	112534.990848	35.376180
1188.688635	112716.268618	35.381197
1189.494384	112910.342857	35.386215
1191.240821	113098.510860	35.391232
1192.244084	113295.481470	35.396250
1193.247372	113492.504143	35.401268
1194.878967	113672.701071	35.406285
1196.431845	113868.457026	35.411303
1197.985224	114043.018963	35.416320
1199.505424	114227.038654	35.421338
1200.506908	114405.849870	35.426356
1201.567388	114591.240464	35.431373
1202.353678	114775.917600	35.436391
1203.175637	114977.161673	35.441408
1204.451759	115180.054904	35.446426
1205.369428	115370.694166	35.451444
1207.947707	115537.202190	35.456461
1209.690529	115713.998275	35.461479
1211.376525	115875.905133	35.466496
1212.953351	116051.919991	35.471514
1213.611631	116219.219293	35.476532
1215.288723	116383.449136	35.481549
1216.592361	116545.930040	35.486567
1218.354561	116708.196436	35.491584
1218.883730	116872.720869	35.496602
1219.620439	117037.579265	35.501620
1220.763914	117221.883633	35.506637
1221.476791	117414.281061	35.511655
1222.524802	117591.672855	35.516672
1223.506238	117777.426778	35.521690
1224.377708	117971.968321	35.526708
1225.767005	118173.698367	35.531725
1226.298143	118366.499758	35.536743
1227.311801	118568.472261	35.541760
1228.663416	118764.345986	35.546778
1229.673642	118988.154354	35.551796
1230.892440	119204.263699	35.556813
1232.553664	119403.258214	35.561831
1233.228915	119609.424970	35.566848
1234.739377	119827.758764	35.571866
1235.627461	120052.444567	35.576884
1236.955262	120261.244771	35.581901
1237.840521	120490.876401	35.586919
1238.839249	120704.600347	35.591936
1240.588090	120935.334065	35.596954
1241.194858	121157.527899	35.601972
1242.489039	121383.639166	35.606989
1243.522395	121630.818883	35.612007
1244.490531	121855.403790	35.617024
1245.788269	122094.952720	35.622042
1246.715639	122335.262010	35.627060
1248.549122	122562.851558	35.632077
1249.592762	122782.881425	35.637095
1251.509196	122995.354470	35.642112
1252.504655	123207.196055	35.647130
1254.114011	123435.387044	35.652148
1255.261991	123640.730423	35.657165
1256.372459	123861.428811	35.662183
1257.276730	124075.927700	35.667200
1259.328972	124294.267883	35.672218
1260.596000	124507.670449	35.677236
1262.272320	124716.000533	35.682253
1263.719342	124930.339426	35.687271
1264.848165	125140.664304	35.692288
1266.062435	125361.597230	35.697306
1267.275764	125574.902146	35.702324
1268.328112	125792.379693	35.707341
1269.393989	126008.956676	35.712359
1270.722863	126223.020083	35.717376
1272.630894	126431.133361	35.722394
1273.675425	126659.150782	35.727412
1275.186371	126858.600101	35.732429
1276.887275	127073.114716	35.737447
1278.703691	127271.654173	35.742464
1280.307901	127469.862534	35.747482
1281.866167	127668.434683	35.752500
1283.318027	127861.524815	35.757517
1284.970621	128039.398146	35.762535
1286.373184	128233.855003	35.767552
1287.507854	128414.313381	35.772570
1288.739945	128615.113145	35.777588
1290.182299	128797.740887	35.782605
1291.550407	128989.166087	35.787623
1292.404831	129184.645090	35.792640
1293.594632	129372.515036	35.797658
1294.295797	129580.583434	35.802676
1295.737147	129778.782793	35.807693
1297.053690	129962.274786	35.812711
1297.990644	130170.840362	35.817728
1299.927644	130368.010530	35.822746
1300.719196	130582.078963	35.827764
1301.775331	130792.264084	35.832781
1303.257427	130996.916492	35.837799
1304.651524	131208.315940	35.842816
1306.435289	131411.868853	35.847834
1307.471419	131604.417108	35.852852
1308.910562	131810.970667	35.857869
1310.218668	132017.458556	35.862887
1310.898017	132239.923318	35.867904
1312.341293	132447.088775	35.872922
1312.972021	132680.694895	35.877940
1314.022751	132899.768601	35.882957
1315.003232	133127.501212	35.887975
1316.154521	133370.952148	35.892992
1317.523404	133609.259885	35.898010
1318.367338	133858.850546	35.903028
1319.684264	134105.981314	35.908045
1320.878365	134354.478147	35.913063
1322.432693	134598.682793	35.918080
1324.444932	134839.225518	35.923098
1326.018577	135075.012491	35.928116
1327.237324	135300.781063	35.933133
1329.019463	135539.085052	35.938151
1330.056946	135772.950140	35.943168
1331.706169	136004.965841	35.948186
1332.971933	136236.653736	35.953204
1335.091489	136461.431407	35.958221
1336.138667	136683.485077	35.963239
1337.449740	136909.616990	35.968256
1338.818843	137126.054343	35.973274
1339.599256	137339.192835	35.978292
1340.695353	137552.863554	35.983309
1342.128707	137764.425729	35.988327
1343.078876	137998.232169	35.993344
1344.093659	138213.087036	35.998362
1345.916755	138448.184566	36.003380
1347.099300	138674.210214	36.008397
1348.850138	138895.654660	36.013415
1349.479212	139135.329332	36.018432
1350.532049	139355.155455	36.023450
1351.093114	139607.219883	36.028468
1352.358342	139851.625007	36.033485
1353.817886	140105.674293	36.038503
1354.859824	140379.245585	36.043520
1356.454608	140641.645109	36.048538
1357.405551	140905.028327	36.053556
1358.584451	141176.719278	36.058573
1359.923793	141455.499368	36.063591
1361.142744	141731.511991	36.068608
1362.978620	142008.121925	36.073626
1364.077642	142280.443425	36.078644
1365.286204	142565.023738	36.083661
1367.077067	142835.142527	36.088679
1368.262812	143130.319631	36.093696
1370.167830	143406.637500	36.098714
1371.322771	143695.357171	36.103732
1373.033814	143967.818521	36.108749
1374.989244	144242.384573	36.113767
1376.269124	144516.075630	36.118784
1378.219894	144775.276794	36.123802
1379.729634	145047.564223	36.128820
1380.980474	145310.461532	36.133837
1382.565209	145581.776785	36.138855
1383.870538	145846.812198	36.143872
1385.300128	146104.562226	36.148890
1387.066893	146370.438067	36.153908
1388.189934	146636.295788	36.158925
1390.037518	146897.609230	36.163943
1391.187114	147169.135382	36.168960
1392.502182	147438.251833	36.173978
1394.058420	147700.481747	36.178996
1395.018938	147967.669740	36.184013
1397.168589	148216.462907	36.189031
1398.779262	148482.887340	36.194048
1400.825247	148728.809501	36.199066
1402.522637	148964.479914	36.204084
1404.388607	149193.947267	36.209101
1406.186950	149433.852720	36.214119
1407.054647	149660.330410	36.219136
1408.712945	149908.341297	36.224154
1409.899907	150146.298037	36.229172
1411.038408	150386.357080	36.234189
1412.671838	150624.154036	36.239207
1413.508232	150869.682098	36.244224
1415.012513	151123.484883	36.249242
1416.045763	151365.292591	36.254260
1416.934438	151621.217501	36.259277
1418.012514	151868.880897	36.264295
1419.152892	152160.104977	36.269312
1420.893829	152407.002391	36.274330
1421.794924	152681.920388	36.279348
1423.322060	152947.946377	36.284365
1424.974196	153205.936994	36.289383
1426.069671	153485.864180	36.294400
1427.712438	153754.603712	36.299418
1429.167162	154021.651185	36.304436
1430.512663	154287.171076	36.309453
1432.461272	154552.897209	36.314471
1434.002604	154795.213053	36.319488
1435.716411	155024.626618	36.324506
1436.732218	155266.017721	36.329524
1438.340360	155517.333289	36.334541
1440.261901	155746.767368	36.339559
1441.660797	155987.909097	36.344576
1443.002820	156235.772245	36.349594
1444.202131	156473.651846	36.354612
1445.421356	156728.261676	36.359629
1446.816539	156979.964339	36.364647
1447.461675	157235.966518	36.369664
1449.115579	157505.351391	36.374682
1451.198090	157746.111318	36.379700
1452.233275	158014.802989	36.384717
1453.493662	158278.105639	36.389735
1454.661436	158557.676155	36.394752
1456.174874	158820.470985	36.399770
1457.380199	159111.164799	36.404788
1458.529353	159397.138008	36.409805
1459.983232	159670.439745	36.414823
1461.097057	159964.009216	36.419840
1462.307155	160267.105104	36.424858
1463.737481	160564.698755	36.429876
1464.458088	160878.257955	36.434893
1466.329912	161185.183729	36.439911
1467.248353	161506.009783	36.444928
1468.830390	161826.246161	36.449946
1470.202656	162146.976498	36.454964
1471.758253	162475.418088	36.459981
1473.683920	162794.577186	36.464999
1474.887628	163127.256304	36.470016
1476.788156	163433.292891	36.475034
1478.651001	163751.454583	36.480052
1480.196550	164078.704890	36.485069
1481.757929	164397.466925	36.490087
1483.286725	164721.299187	36.495104
1484.923171	165045.369783	36.500122
1486.754828	165348.373598	36.505140
1488.415618	165657.079459	36.510157
1490.509896	165970.067700	36.515175
1491.968788	166270.069150	36.520192
1493.301002	166573.582965	36.525210
1495.092826	166885.054496	36.530228
1496.291394	167199.202362	36.535245
1497.850276	167508.432938	36.540263
1499.035300	167818.945764	36.545280
1500.305366	168144.584469	36.550298
1501.829557	168451.505245	36.555316
1502.608417	168796.707665	36.560333
1504.451149	169102.323833	36.565351
1505.276933	169444.097330	36.570368
1506.806873	169782.584310	36.575386
1508.397852	170110.163457	36.580404
1509.569766	170459.894177	36.585421
1511.328571	170781.194342	36.590439
1513.460585	171107.409225	36.595456
1515.764077	171433.674111	36.600474
1517.667065	171735.351259	36.605492
1518.919407	172068.533170	36.610509
1521.376727	172362.952631	36.615527
1523.407699	172660.350655	36.620544
1524.988684	172961.708352	36.625562
1526.461767	173255.903155	36.630580
1527.568741	173557.863516	36.635597
1529.442064	173837.630070	36.640615
1531.676721	174127.909545	36.645632
1533.362507	174400.096164	36.650650
1535.083431	174686.606241	36.655668
1536.327206	174949.592365	36.660685
1537.798096	175211.628523	36.665703
1538.861602	175485.117330	36.670720
1539.736197	175757.776000	36.675738
1540.888581	176018.714410	36.680756
1541.948269	176312.577519	36.685773
1543.395458	176599.639133	36.690791
1544.725364	176895.174208	36.695808
1545.829111	177197.386081	36.700826
1547.375212	177504.818753	36.705844
1548.305032	177817.432060	36.710861
1549.517718	178135.140487	36.715879
1551.539923	178447.843129	36.720896
1552.901093	178780.837083	36.725914
1555.728361	179075.629061	36.730932
1558.238084	179364.700595	36.735949
1560.950734	179631.465813	36.740967
1563.134083	179917.776965	36.745984
1565.136139	180174.737670	36.751002
1567.348665	180426.943298	36.756020
1568.938070	180680.446511	36.761037
1570.406691	180942.398621	36.766055
1571.621488	181198.492203	36.771072
1572.653706	181475.991228	36.776090
1574.068730	181732.396909	36.781108
1575.095420	182022.401758	36.786125
1576.190590	182306.088635	36.791143
1577.463144	182601.209059	36.796160
1578.503917	182911.372304	36.801178
1580.943179	183179.419370	36.806196
1582.166926	183484.618102	36.811213
1583.778859	183788.116819	36.816231
1585.551211	184087.198869	36.821248
1586.238097	184396.375766	36.826266
1587.914384	184700.033898	36.831284
1589.060891	185013.339498	36.836301
1590.246561	185345.337560	36.841319
1591.490703	185670.752763	36.846336
1592.816899	186011.604150	36.851354
1594.123928	186353.527042	36.856372
1594.954337	186711.296436	36.861389
1596.339804	187072.746096	36.866407
1598.190690	187438.068655	36.871424
1599.382547	187811.449126	36.876442
1600.822826	188181.490428	36.881460
1602.190787	188554.998851	36.886477
1603.563895	188935.528642	36.891495
1605.208002	189324.939978	36.896512
1606.881362	189714.095162	36.901530
1608.933746	190096.436707	36.906548
1610.423093	190491.466890	36.911565
1612.285788	190883.340345	36.916583
1614.002498	191266.227415	36.921600
1615.438840	191654.215855	36.926618
1617.827115	192031.334631	36.931636
1620.005134	192397.192218	36.936653
1622.450819	192753.118310	36.941671
1624.281048	193111.827106	36.946688
1626.038067	193476.999181	36.951706
1627.684904	193832.911542	36.956724
1629.400200	194188.801878	36.961741
1631.255204	194531.264895	36.966759
1632.753089	194883.437385	36.971776
1634.451629	195233.534604	36.976794
1636.452807	195578.251483	36.981812
1637.983797	195911.241320	36.986829
1639.154585	196267.830164	36.991847
1640.979610	196611.883480	36.996864
1642.787195	196940.236901	37.001882
1644.420571	197256.039328	37.006900
1645.869340	197596.034022	37.011917
1647.312587	197928.045647	37.016935
1648.815121	198260.925111	37.021952
1650.405639	198602.767722	37.026970
1651.744944	198921.610306	37.031988
1653.247626	199276.001895	37.037005
1654.770510	199622.558405	37.042023
1656.175163	199957.671519	37.047040
1657.343324	200318.624404	37.052058
1658.762554	200685.961922	37.057076
1660.306878	201053.052090	37.062093
1661.673590	201425.099859	37.067111
1663.457797	201799.695876	37.072128
1664.940625	202174.407290	37.077146
1666.474226	202565.072033	37.082164
1668.040626	202945.334760	37.087181
1669.378482	203340.784714	37.092199
1671.811992	203741.121271	37.097216
1673.462124	204137.844216	37.102234
1675.289681	204529.105514	37.107252
1676.846121	204928.032068	37.112269
1678.303775	205312.781618	37.117287
1680.771747	205695.372183	37.122304
1683.315455	206080.161439	37.127322
1685.001594	206468.865871	37.132340
1686.703763	206844.783243	37.137357
1688.738859	207215.085722	37.142375
1691.134808	207597.113479	37.147392
1692.904092	207954.524634	37.152410
1695.039983	208305.692844	37.157428
1696.936179	208667.619206	37.162445
1699.128381	209010.933932	37.167463
1701.310020	209351.331343	37.172480
1702.984848	209701.121721	37.177498
1704.858124	210040.404865	37.182516
1706.210183	210386.937447	37.187533
1707.392293	210737.359830	37.192551
1709.558695	211083.887281	37.197568
1710.573982	211451.812855	37.202586
1713.090440	211773.168101	37.207604
1715.343739	212111.228275	37.212621
1717.170499	212452.052492	37.217639
1718.956125	212783.538852	37.222656
1720.394343	213121.357041	37.227674
1722.151949	213461.612473	37.232692
1723.526706	213803.227889	37.237709
1724.559383	214154.145831	37.242727
1726.403047	214503.787840	37.247744
1727.749482	214863.164556	37.252762
1729.031974	215219.048418	37.257780
1730.961345	215587.195007	37.262797
1732.396842	215960.580593	37.267815
1734.265877	216311.520422	37.272832
1736.385805	216677.379250	37.277850
1737.828092	217044.647056	37.282868
1739.101968	217411.918753	37.287885
1740.643080	217797.332552	37.292903
1742.097360	218178.266756	37.297920
1743.621975	218590.608412	37.302938
1744.751186	219018.129309	37.307956
1746.861343	219410.261719	37.312973
1748.318320	219817.793805	37.317991
1749.690494	220212.540596	37.323008
1750.957422	220625.314031	37.328026
1752.386713	221039.179701	37.333044
1754.316130	221454.741999	37.338061
1755.690492	221855.869599	37.343079
1757.490097	222257.461564	37.348096
1759.948648	222651.427595	37.353114
1761.355740	223039.575009	37.358132
1763.402706	223441.079391	37.363149
1764.502191	223847.491895	37.368167
1766.706486	224245.798049	37.373184
1768.250072	224662.299611	37.378202
1769.856888	225067.209849	37.383220
1771.505047	225480.928339	37.388237
1772.838633	225929.980874	37.393255
1774.806123	226351.802747	37.398272
1776.910216	226771.266586	37.403290
1779.398420	227175.377235	37.408308
1781.583877	227582.790555	37.413325
1783.418463	228002.328457	37.418343
1785.638649	228402.499458	37.423360
1787.254812	228817.580243	37.428378
1789.368015	229233.595950	37.433396
1790.922918	229638.859345	37.438413
1792.681576	230058.289159	37.443431
1794.615174	230469.283553	37.448448
1796.443337	230896.527754	37.453466
1797.963418	231317.093001	37.458484
1800.027288	231735.537245	37.463501
1801.809740	232159.896937	37.468519
1803.559768	232576.541221	37.473536
1805.515685	232994.574972	37.478554
1807.820996	233398.784426	37.483572
1810.357610	233806.741372	37.488589
1812.023720	234221.320949	37.493607
1814.107767	234616.196958	37.498624
1815.926361	235025.037923	37.503642
1818.030250	235425.475459	37.508660
1820.452643	235818.393047	37.513677
1822.852740	236211.061183	37.518695
1824.819900	236585.487237	37.523712
1826.868690	236978.443856	37.528730
1828.804469	237343.986004	37.533748
1830.991702	237709.182366	37.538765
1832.802351	238088.158880	37.543783
1834.467477	238442.850508	37.548800
1836.250182	238830.393545	37.553818
1837.516026	239219.851911	37.558836
1839.681807	239579.568376	37.563853
1840.984804	239975.956772	37.568871
1842.758026	240350.726873	37.573888
1844.553459	240734.156107	37.578906
1846.206066	241129.193121	37.583924
1848.213056	241510.607222	37.588941
1849.497421	241912.565216	37.593959
1851.433528	242316.016240	37.598976
1852.871668	242717.137195	37.603994
1854.319109	243123.845800	37.609012
1855.807488	243528.185817	37.614029
1856.858956	243971.363228	37.619047
1858.244057	244397.009042	37.624064
1860.098895	244843.280858	37.629082
1860.892862	245299.153546	37.634100
1863.027138	245757.395923	37.639117
1864.448698	246215.071185	37.644135
1866.396258	246687.977853	37.649152
1868.263871	247163.464120	37.654170
1869.953290	247631.004042	37.659188
1872.600858	248096.277362	37.664205
1873.902896	248579.403852	37.669223
1875.879200	249051.241886	37.674240
1877.635822	249518.341079	37.679258
1879.050652	249978.155914	37.684276
1881.098288	250447.519529	37.689293
1882.454977	250909.351740	37.694311
1884.267600	251387.214402	37.699328
1885.707047	251859.093359	37.704346
1887.237343	252352.042271	37.709364
1889.445611	252827.274826	37.714381
1890.623044	253336.312348	37.719399
1892.434031	253823.855733	37.724416
1894.634694	254334.146949	37.729434
1896.095468	254844.738860	37.734452
1898.654477	255347.578892	37.739469
1900.625699	255851.456444	37.744487
1902.667507	256359.031364	37.749504
1905.487055	256852.429563	37.754522
1907.772639	257356.738148	37.759540
1909.821583	257849.044867	37.764557
1912.043387	258351.154079	37.769575
1914.308755	258835.118146	37.774592
1916.374740	259324.881792	37.779610
1918.351926	259811.002046	37.784628
1920.951069	260277.128420	37.789645
1923.063915	260764.724850	37.794663
1924.487299	261260.056375	37.799680
1926.508507	261740.300778	37.804698
1927.824983	262239.460183	37.809716
1929.879216	262731.460450	37.814733
1932.828334	263194.758988	37.819751
1935.660334	263653.478716	37.824768
1937.813994	264123.843632	37.829786
1939.709551	264604.336087	37.834804
1941.870581	265054.681472	37.839821
1943.217842	265528.532266	37.844839
1945.011453	266009.929683	37.849856
1946.918335	266486.151093	37.854874
1948.637641	266964.333786	37.859892
1950.272996	267441.463000	37.864909
1952.153737	267934.148545	37.869927
1953.745119	268426.983095	37.874944
1955.850153	268918.309411	37.879962
1957.672810	269419.919295	37.884980
1959.822869	269903.616038	37.889997
1961.704875	270417.763795	37.895015
1963.888947	270905.645029	37.900032
1966.337226	271391.424161	37.905050
1968.402018	271874.116151	37.910068
1970.719990	272360.296432	37.915085
1972.889439	272842.004257	37.920103
1974.939450	273328.938612	37.925120
1977.044720	273809.588527	37.930138
1978.736686	274290.915722	37.935156
1980.624385	274765.350938	37.940173
1982.606565	275256.992485	37.945191
1984.020205	275748.422412	37.950208
1987.067839	276217.937850	37.955226
1989.222562	276693.315782	37.960244
1991.408934	277159.491868	37.965261
1993.572589	277646.068699	37.970279
1995.353268	278108.194821	37.975296
1997.904971	278583.629908	37.980314
1999.279222	279058.750909	37.985332
2001.311918	279525.379070	37.990349
2003.570331	279992.146547	37.995367
2005.410981	280456.899147	38.000384
2007.470389	280922.579631	38.005402
2008.987385	281404.453473	38.010420
2010.815854	281882.692802	38.015437
2012.346038	282360.853242	38.020455
2013.831151	282836.327269	38.025472
2015.588063	283299.384447	38.030490
2016.998941	283784.292020	38.035508
2018.873065	284268.562591	38.040525
2020.535205	284760.436370	38.045543
2022.103864	285271.806752	38.050560
2023.898565	285762.893373	38.055578
2025.835359	286266.629938	38.060596
2029.066399	286746.171993	38.065613
2031.548956	287248.620957	38.070631
2033.298543	287751.875392	38.075648
2035.039216	288247.458527	38.080666
2037.183094	288756.079763	38.085684
2038.983199	289264.603642	38.090701
2040.836553	289786.324931	38.095719
2042.408642	290319.317635	38.100736
2044.789160	290840.261589	38.105754
2046.759711	291362.744520	38.110772
2049.289406	291884.624659	38.115789
2051.903703	292411.593932	38.120807
2054.203595	292928.021335	38.125824
2056.348257	293448.688547	38.130842
2058.199650	293971.764183	38.135860
2060.955530	294483.943727	38.140877
2063.570027	294985.603720	38.145895
2065.198593	295501.597488	38.150912
2067.572014	296022.824674	38.155930
2069.168893	296538.463261	38.160948
2070.973836	297067.526260	38.165965
2072.906350	297592.146146	38.170983
2074.567078	298134.206396	38.176000
2076.748107	298662.208542	38.181018
2079.032795	299203.423269	38.186036
2080.794065	299753.966691	38.191053
2082.513426	300306.571247	38.196071
2084.267943	300858.303350	38.201088
2086.629792	301411.074618	38.206106
2088.231347	301977.708670	38.211124
2090.154898	302549.365462	38.216141
2092.256730	303117.789178	38.221159
2094.027349	303702.848501	38.226176
2096.062054	304284.203172	38.231194
2097.746962	304874.069111	38.236212
2099.812431	305470.420394	38.241229
2101.683813	306066.393415	38.246247
2103.470451	306687.289997	38.251264
2105.589958	307297.435219	38.256282
2107.391673	307916.187033	38.261300
2109.213206	308539.324397	38.266317
2112.217407	309146.719163	38.271335
2114.768410	309760.685613	38.276352
2117.403806	310359.904264	38.281370
2119.627951	310981.178412	38.286388
2121.641916	311590.115253	38.291405
2123.863498	312209.246864	38.296423
2125.637397	312823.724280	38.301440
2127.971713	313425.152936	38.306458
2130.551088	314038.902948	38.311476
2132.640019	314641.759054	38.316493
2134.840127	315254.241260	38.321511
2136.501929	315882.068718	38.326528
2138.995316	316489.717912	38.331546
2141.174456	317096.601361	38.336564
2143.797088	317691.674763	38.341581
2146.567071	318284.458736	38.346599
2148.462078	318892.338419	38.351616
2150.870955	319471.460170	38.356634
2153.265638	320063.757537	38.361652
2155.245719	320639.334585	38.366669
2157.362708	321192.514307	38.371687
2159.147284	321769.637300	38.376704
2161.220864	322321.849757	38.381722
2163.253251	322890.111097	38.386740
2165.526270	323466.173113	38.391757
2168.105117	324011.000227	38.396775
2170.334470	324577.385668	38.401792
2172.866313	325127.695000	38.406810
2175.099544	325697.522512	38.411828
2176.869947	326255.716953	38.416845
2178.779883	326820.408083	38.421863
2180.323227	327398.356708	38.426880
2183.173819	327966.004033	38.431898
2185.851853	328535.730910	38.436916
2187.914885	329094.205681	38.441933
2190.474716	329677.828154	38.446951
2192.250421	330258.655006	38.451968
2194.169510	330828.459566	38.456986
2196.493727	331423.552811	38.462004
2198.178371	332018.872596	38.467021
2200.720679	332608.585926	38.472039
2202.180707	333212.332981	38.477056
2204.213215	333817.679433	38.482074
2205.968300	334431.569229	38.487092
2208.548347	335034.729792	38.492109
2211.793936	335634.777921	38.497127
2214.251062	336240.331371	38.502144
2216.894215	336819.802706	38.507162
2219.550729	337417.135789	38.512180
2221.428558	338013.550201	38.517197
2223.704835	338613.750012	38.522215
2226.220479	339222.203433	38.527232
2228.321848	339813.153201	38.532250
2230.687581	340406.945869	38.537268
2232.893394	341008.601081	38.542285
2234.822440	341605.142285	38.547303
2236.402102	342221.709474	38.552320
2239.033491	342837.003336	38.557338
2241.295976	343458.467299	38.562356
2242.820486	344082.405842	38.567373
2244.768605	344704.946322	38.572391
2246.840220	345338.676145	38.577408
2249.403682	345977.163513	38.582426
2251.728543	346614.057395	38.587444
2253.824245	347254.584293	38.592461
2256.099195	347889.362422	38.597479
2258.590492	348524.222811	38.602496
2261.272716	349147.698791	38.607514
2264.039563	349783.409495	38.612532
2266.209709	350414.895855	38.617549
2268.651130	351039.501967	38.622567
2270.914844	351672.376023	38.627584
2273.237348	352298.861815	38.632602
2275.673766	352921.462628	38.637620
2277.896502	353548.835060	38.642637
2280.161964	354185.757636	38.647655
2282.394483	354820.874572	38.652672
2284.327121	355458.949690	38.657690
2286.494675	356088.805875	38.662708
2288.278739	356734.549121	38.667725
2290.176472	357380.973970	38.672743
2292.166705	358046.834218	38.677760
2294.407865	358703.178274	38.682778
2296.680097	359355.396383	38.687796
2298.768645	360023.110969	38.692813
2301.136047	360692.493534	38.697831
2303.493355	361347.100888	38.702848
2305.644752	361997.875281	38.707866
2308.130503	362633.869133	38.712884
2310.242305	363288.358088	38.717901
2312.816592	363916.933935	38.722919
2314.821051	364554.574373	38.727936
2316.747071	365203.734344	38.732954
2319.987745	365827.424838	38.737972
2322.249700	366473.006858	38.742989
2324.979007	367099.576852	38.748007
2327.127123	367753.907329	38.753024
2329.271291	368410.636764	38.758042
2331.844962	369060.155783	38.763060
2333.719416	369720.838283	38.768077
2336.520664	370355.027036	38.773095
2338.680581	371019.798612	38.778112
2340.835562	371679.739730	38.783130
2343.341940	372345.570941	38.788148
2344.711031	373025.705091	38.793165
2346.974750	373710.217986	38.798183
2349.433731	374390.500642	38.803200
2351.716292	375068.567573	38.808218
2354.328434	375757.903048	38.813236
2356.559931	376464.735710	38.818253
2358.888524	377161.089658	38.823271
2361.025421	377868.086731	38.828288
2362.909589	378577.494732	38.833306
2365.421550	379297.561183	38.838324
2367.675562	380027.062635	38.843341
2370.535709	380740.117969	38.848359
2373.008527	381466.204694	38.853376
2375.522422	382176.193071	38.858394
2378.316788	382885.384420	38.863412
2380.804329	383607.161852	38.868429
2383.282318	384328.772753	38.873447
2385.841219	385048.858318	38.878464
2387.940229	385774.404133	38.883482
2390.605253	386497.355262	38.888500
2392.576766	387224.866729	38.893517
2394.632038	387965.682437	38.898535
2397.411660	388687.626579	38.903552
2399.936113	389436.391454	38.908570
2402.648523	390162.520731	38.913588
2404.153963	390921.000616	38.918605
2406.661340	391659.701682	38.923623
2409.192434	392400.129979	38.928640
2411.517520	393146.049334	38.933658
2414.508117	393882.259159	38.938676
2416.980743	394637.850255	38.943693
2419.315291	395376.108996	38.948711
2422.155904	396122.021093	38.953728
2424.571532	396869.758811	38.958746
2427.325055	397607.436335	38.963764
2429.673255	398349.622670	38.968781
2431.831245	399095.876294	38.973799
2434.280211	399847.865693	38.978816
2436.789129	400588.650287	38.983834
2439.874392	401315.028531	38.988852
2442.125262	402062.634098	38.993869
2444.694720	402793.418316	38.998887
2447.046039	403537.091447	39.003904
2449.448922	404287.121357	39.008922
2452.194683	405010.318780	39.013940
2455.418129	405734.862455	39.018957
2458.543393	406434.574671	39.023975
2462.000284	407123.193554	39.028992
2464.362123	407817.499208	39.034010
2467.616807	408494.235258	39.039028
2469.936389	409168.930566	39.044045
2472.648172	409823.151623	39.049063
2474.643490	410465.062830	39.054080
2476.660495	411127.701177	39.059098
2479.001777	411761.747319	39.064116
2480.666689	412417.623240	39.069133
2482.322738	413088.580532	39.074151
2484.091251	413773.736715	39.079168
2486.271885	414470.786820	39.084186
2488.795867	415155.680404	39.089204
2491.193687	415848.681263	39.094221
2493.546872	416555.346845	39.099239
2495.839381	417266.409614	39.104256
2497.778085	417996.985631	39.109274
2500.076540	418709.830580	39.114292
2502.117253	419464.708871	39.119309
2503.881130	420218.141727	39.124327
2505.874216	420982.832708	39.129344
2507.900529	421770.435249	39.134362
2510.347063	422561.488077	39.139380
2512.657090	423357.855203	39.144397
2515.108507	424169.313419	39.149415
2517.691440	424979.609049	39.154432
2519.732543	425813.612970	39.159450
2522.106893	426634.774050	39.164468
2524.653133	427478.712591	39.169485
2526.724780	428338.293312	39.174503
2529.175834	429195.046545	39.179520
2531.567192	430061.903561	39.184538
2533.841583	430938.416970	39.189556
2536.884252	431813.555706	39.194573
2539.337220	432681.622163	39.199591
2542.461156	433564.730112	39.204608
2544.891247	434459.206230	39.209626
2547.670712	435343.366134	39.214644
2550.168199	436221.161714	39.219661
2552.800755	437114.792233	39.224679
2556.287780	437988.762683	39.229696
2559.463356	438869.481262	39.234714
2563.424562	439707.073736	39.239732
2566.746334	440558.149850	39.244749
2569.633773	441404.509026	39.249767
2572.641780	442247.931906	39.254784
2575.186914	443092.613415	39.259802
2577.432259	443911.863779	39.264820
2580.102069	444754.082721	39.269837
2582.106648	445586.868399	39.274855
2584.631142	446431.221648	39.279872
2587.071250	447271.913662	39.284890
2589.474238	448116.473789	39.289908
2592.060245	448965.775449	39.294925
2594.715764	449827.676461	39.299943
2597.237506	450682.079115	39.304960
2599.369225	451539.242717	39.309978
2602.286541	452385.772695	39.314996
2605.542461	453224.272687	39.320013
2608.668146	454058.664326	39.325031
2611.931571	454895.730137	39.330048
2614.870122	455738.984601	39.335066
2618.084416	456546.613191	39.340084
2621.560476	457340.464565	39.345101
2624.358825	458145.671715	39.350119
2627.671243	458925.736185	39.355136
2630.611396	459695.670567	39.360154
2633.405139	460461.504895	39.365172
2636.398435	461221.210786	39.370189
2639.280600	461966.752370	39.375207
2642.246878	462716.093653	39.380224
2644.883061	463439.430330	39.385242
2647.672064	464143.255921	39.390260
2650.407649	464828.516306	39.395277
2652.920544	465516.720888	39.400295
2655.498321	466205.143163	39.405312
2657.517418	466914.100786	39.410330
2659.967103	467604.516112	39.415348
2662.425380	468303.192727	39.420365
2664.288722	469021.750559	39.425383
2666.493536	469741.993503	39.430400
2668.301857	470474.047740	39.435418
2670.549812	471214.539858	39.440436
2673.185776	471960.092254	39.445453
2675.164005	472729.772140	39.450471
2677.532857	473489.706838	39.455488
2679.881335	474277.499506	39.460506
2681.777939	475074.325403	39.465524
2685.490054	475872.786832	39.470541
2687.083813	476672.019019	39.475559
2690.190179	477486.825980	39.480576
2692.321020	478317.869707	39.485594
2694.578944	479159.208026	39.490612
2696.864800	480005.906650	39.495629
2698.916109	480872.753766	39.500647
2701.242464	481754.915357	39.505664
2703.838970	482642.493015	39.510682
2705.719128	483541.253518	39.515700
2708.276099	484457.124138	39.520717
2711.453031	485367.443158	39.525735
2714.298986	486287.059280	39.530752
2717.012230	487206.649573	39.535770
2720.472982	488117.840239	39.540788
2723.751051	489036.383265	39.545805
2726.641662	489950.298602	39.550823
2730.512421	490846.541029	39.555840
2734.479823	491744.588430	39.560858
2737.412615	492630.093523	39.565876
2740.908368	493507.486793	39.570893
2743.698773	494401.553176	39.575911
2745.979898	495280.721601	39.580928
2748.595968	496167.054646	39.585946
2751.139472	497057.288584	39.590964
2753.596087	497947.843076	39.595981
2755.953357	498850.776722	39.600999
2758.386832	499762.274994	39.606016
2760.890984	500665.439397	39.611034
2763.302321	501590.208161	39.616052
2766.094813	502511.987359	39.621069
2769.019411	503436.416523	39.626087
2771.829310	504356.475634	39.631104
2775.094637	505289.569110	39.636122
2777.829874	506204.644963	39.641140
2780.765740	507128.762293	39.646157
2783.110236	508060.084051	39.651175
2785.622997	509000.852649	39.656192
2788.144895	509951.193357	39.661210
2790.616578	510889.690023	39.666228
2794.010565	511830.650322	39.671245
2796.564280	512784.899504	39.676263
2799.052122	513734.817889	39.681280
2801.692495	514699.420131	39.686298
2804.369126	515656.498646	39.691316
2808.432197	516592.729493	39.696333
2811.726850	517545.961511	39.701351
2815.011136	518473.037084	39.706368
2817.768740	519410.119749	39.711386
2820.568740	520356.811062	39.716404
2823.709888	521280.466391	39.721421
2826.518050	522200.393303	39.726439
2828.877659	523096.161212	39.731456
2831.446959	523993.805796	39.736474
2834.030128	524889.480896	39.741492
2836.732019	525784.327627	39.746509
2839.163759	526707.114283	39.751527
2841.042723	527615.080733	39.756544
2843.960783	528548.700701	39.761562
2845.862932	529482.127869	39.766580
2848.793265	530434.608256	39.771597
2850.498776	531392.414869	39.776615
2853.817662	532349.590069	39.781632
2857.004591	533313.066671	39.786650
2859.768517	534291.548435	39.791668
2862.504668	535274.750032	39.796685
2864.736662	536268.586760	39.801703
2867.372145	537272.654431	39.806720
2870.609655	538275.445274	39.811738
2873.907754	539284.495373	39.816756
2876.850728	540293.532718	39.821773
2879.472754	541320.963861	39.826791
2882.355976	542339.323086	39.831808
2885.492011	543378.038928	39.836826
2887.852527	544413.738067	39.841844
2891.525103	545428.523518	39.846861
2894.597633	546449.620348	39.851879
2897.855523	547486.602012	39.856896
2901.077646	548512.701291	39.861914
2904.165320	549550.762665	39.866932
2906.916497	550583.019655	39.871949
2909.529375	551622.661501	39.876967
2912.085770	552670.275877	39.881984
2914.662758	553731.376718	39.887002
2917.213288	554792.097072	39.892020
2920.226217	555863.713293	39.897037
2922.424067	556955.327982	39.902055
2925.025848	558052.514720	39.907072
2927.669208	559155.080485	39.912090
2930.281302	560273.635738	39.917108
2932.591576	561392.296873	39.922125
2935.062995	562540.370832	39.927143
2937.960778	563689.780415	39.932160
2940.803089	564837.038915	39.937178
2943.950355	566004.483011	39.942196
2947.080776	567152.794644	39.947213
2950.134156	568329.534048	39.952231
2953.089692	569496.292053	39.957248
2956.545005	570646.546857	39.962266
2960.324792	571804.373843	39.967284
2963.575778	572960.124930	39.972301
2967.065890	574120.698990	39.977319
2970.435889	575274.863401	39.982336
2973.794100	576408.402240	39.987354
2976.726674	577556.106722	39.992372
2979.749164	578696.516913	39.997389
2982.869996	579839.915942	40.002407
2985.554663	580978.817417	40.007424
2988.386028	582110.066573	40.012442
2991.312149	583267.422423	40.017460
2994.459495	584414.252692	40.022477
2997.285616	585568.197643	40.027495
3000.105598	586711.907069	40.032512
3003.452230	587858.980199	40.037530
3005.615748	589020.875776	40.042548
3008.994107	590175.441388	40.047565
3011.640877	591340.339697	40.052583
3014.787794	592499.629622	40.057600
3018.022543	593653.530847	40.062618
3022.190978	594771.194272	40.067636
3026.715043	595845.261362	40.072653
3030.103393	596915.711284	40.077671
3033.235218	597979.394257	40.082688
3036.849458	599018.361018	40.087706
3039.810424	600071.213869	40.092724
3042.864764	601104.928443	40.097741
3045.883314	602145.415493	40.102759
3048.728847	603178.678126	40.107776
3052.086327	604216.067960	40.112794
3055.079660	605253.523943	40.117812
3058.673868	606269.014898	40.122829
3061.706167	607305.776747	40.127847
3065.017128	608338.644593	40.132864
3067.824801	609358.792213	40.137882
3070.875280	610404.372751	40.142900
3073.560722	611437.809917	40.147917
3076.450604	612489.225397	40.152935
3078.780390	613554.488811	40.157952
3082.534952	614583.056054	40.162970
3085.991240	615636.830561	40.167988
3089.064135	616692.117907	40.173005
3092.088951	617735.762595	40.178023
3095.190783	618807.990957	40.183040
3098.145977	619864.942173	40.188058
3101.165953	620938.324460	40.193076
3104.103238	621999.069937	40.198093
3107.219774	623088.915995	40.203111
3109.837554	624176.336032	40.208128
3112.799378	625261.590790	40.213146
3115.013674	626373.936348	40.218164
3117.693416	627496.029739	40.223181
3120.756946	628633.075452	40.228199
3123.615485	629788.162098	40.233216
3126.028289	630935.106757	40.238234
3128.686090	632102.507564	40.243252
3131.371877	633284.601846	40.248269
3134.179762	634468.090090	40.253287
3137.402465	635670.592345	40.258304
3141.041804	636865.999482	40.263322
3144.176031	638079.366929	40.268340
3147.324205	639293.487739	40.273357
3150.238781	640517.781406	40.278375
3153.030954	641744.243941	40.283392
3156.058750	642978.002173	40.288410
3159.034806	644223.987877	40.293428
3162.592524	645480.146516	40.298445
3166.344443	646721.956964	40.303463
3169.294374	647973.618067	40.308480
3172.440824	649221.850717	40.313498
3175.040463	650497.430744	40.318516
3177.811665	651765.144850	40.323533
3181.170568	653036.088165	40.328551
3183.940809	654327.243240	40.333568
3187.758534	655598.329471	40.338586
3191.017941	656886.378383	40.343604
3194.184253	658180.747747	40.348621
3197.797655	659454.604880	40.353639
3201.137205	660743.974367	40.358656
3204.369213	662021.740287	40.363674
3207.994443	663307.684437	40.368692
3211.467717	664570.190010	40.373709
3215.320821	665827.241660	40.378727
3218.966869	667101.278503	40.383744
3222.567220	668350.775353	40.388762
3226.248471	669588.355144	40.393780
3229.698963	670842.721806	40.398797
3233.816766	672049.915998	40.403815
3237.078350	673258.439359	40.408832
3240.368257	674429.862215	40.413850
3243.631871	675597.364580	40.418868
3246.563493	676761.544748	40.423885
3249.517559	677928.557291	40.428903
3252.232793	679090.194882	40.433920
3255.293777	680254.709775	40.438938
3258.481241	681433.811452	40.443956
3261.631176	682600.647486	40.448973
3265.232569	683771.183823	40.453991
3267.950835	684947.277961	40.459008
3271.520561	686128.342655	40.464026
3274.490509	687327.772019	40.469044
3277.793845	688513.782526	40.474061
3281.003239	689704.069957	40.479079
3284.313636	690918.649661	40.484096
3287.864602	692125.234313	40.489114
3290.791345	693323.721481	40.494132
3294.133615	694548.270811	40.499149
3297.431241	695758.323797	40.504167
3301.423555	696974.097320	40.509184
3305.097089	698181.028479	40.514202
3308.246863	699396.656261	40.519220
3310.952715	700625.821569	40.524237
3314.438380	701862.516601	40.529255
3317.279974	703107.369363	40.534272
3320.746494	704333.655491	40.539290
3324.143917	705585.741095	40.544308
3327.132294	706844.003950	40.549325
3330.419919	708089.353369	40.554343
3333.992121	709359.979561	40.559360
3337.340335	710629.909192	40.564378
3340.864433	711894.669583	40.569396
3344.022597	713163.658241	40.574413
3348.049681	714415.386116	40.579431
3351.345143	715690.654417	40.584448
3354.547455	716973.166699	40.589466
3357.822261	718255.916148	40.594484
3360.703133	719537.099460	40.599501
3363.936425	720830.292774	40.604519
3366.725339	722144.324419	40.609536
3369.696310	723462.715493	40.614554
3372.615882	724785.897238	40.619572
3375.904797	726114.686737	40.624589
3379.556125	727437.172261	40.629607
3383.133137	728785.543865	40.634624
3386.423795	730128.700877	40.639642
3389.817128	731467.716869	40.644660
3393.207917	732820.487517	40.649677
3397.763890	734140.942157	40.654695
3401.195155	735474.349599	40.659712
3405.502379	736803.096312	40.664730
3408.917206	738122.343534	40.669748
3412.085070	739461.545147	40.674765
3416.056124	740777.546309	40.679783
3420.646528	742066.836640	40.684800
3425.015286	743354.374802	40.689818
3429.411887	744625.967605	40.694836
3432.500530	745897.521166	40.699853
3436.184874	747159.995191	40.704871
3439.435591	748429.680275	40.709888
3443.049845	749683.427392	40.714906
3446.095619	750937.115021	40.719924
3449.305024	752206.632014	40.724941
3452.167584	753466.688169	40.729959
3455.038262	754742.541573	40.734976
3457.995062	756028.951553	40.739994
3460.711879	757316.464634	40.745012
3463.566037	758607.071326	40.750016
3466.495468	759851.125546	40.755021
3468.957729	761067.180479	40.760026
3471.594158	762222.096199	40.765031
3474.315885	763328.145473	40.770036
3476.813652	764384.907405	40.775040
3479.441641	765391.308546	40.780045
3481.998956	766320.140923	40.785050
3484.327897	767193.936039	40.790055
3486.372835	768015.038652	40.795060
3488.479387	768791.145967	40.800064
3490.622706	769505.719390	40.805069
3492.683935	770152.144576	40.810074
3494.992581	770759.945353	40.815079
3497.252601	771309.277547	40.820084
3498.842016	771792.325991	40.825088
3500.765996	772228.739179	40.830093
3502.155787	772618.028605	40.835098
3503.730016	772966.830608	40.840103
3505.266233	773261.939264	40.845108
3505.842850	773526.069363	40.850112
3507.352059	773750.490283	40.855117
3508.565928	773940.924125	40.860122
3509.456676	774108.113552	40.865127
3510.242279	774229.618058	40.870132
3510.943399	774327.990078	40.875136
3512.007289	774387.595824	40.880141
3512.428632	774428.053321	40.885146
3513.007395	774447.408720	40.890151
3513.945461	774433.909045	40.895156
3514.509650	774418.550652	40.900160
3515.137445	774366.889511	40.905165
3515.429877	774292.877540	40.910170
3516.182535	774211.993063	40.915175
3516.668135	774112.340266	40.920180
3516.845492	773986.784546	40.925184
3517.453328	773849.484077	40.930189
3517.577781	773702.559121	40.935194
3517.413972	773542.874182	40.940199
3517.812694	773376.050082	40.945204
3517.983766	773202.561671	40.950208
3518.498579	773017.191819	40.955213
3518.252440	772813.472929	40.960218
3518.468199	772612.430356	40.965223
3519.041459	772399.550937	40.970228
3518.856615	772187.184703	40.975232
3519.087867	771961.689866	40.980237
3519.374195	771726.523893	40.985242
3518.969825	771486.045678	40.990247
3519.171277	771233.882429	40.995252
3519.144673	770997.217739	41.000256
3519.470261	770743.046593	41.005261
3519.254917	770487.773636	41.010266
3519.115820	770237.110732	41.015271
3519.242264	769981.074021	41.020276
3519.319853	769720.059829	41.025280
3519.293586	769451.218706	41.030285
3518.999690	769177.533546	41.035290
3519.112974	768915.647413	41.040295
3519.330951	768644.321989	41.045300
3518.870232	768382.807603	41.050304
3519.117355	768096.376681	41.055309
3519.004556	767823.498831	41.060314
3519.050251	767547.479595	41.065319
3519.018615	767274.371049	41.070324
3518.914843	767001.855921	41.075328
3518.957166	766715.602906	41.080333
3518.842702	766444.597304	41.085338
3518.638263	766168.568352	41.090343
3518.707004	765874.933353	41.095348
3518.430163	765612.305344	41.100352
3518.585256	765338.651408	41.105357
3518.280104	765054.610826	41.110362
3518.062978	764776.264539	41.115367
3517.996779	764509.174691	41.120372
3518.060359	764234.460058	41.125376
3518.052010	763952.843516	41.130381
3517.931689	763679.618336	41.135386
3517.769627	763413.491621	41.140391
3518.016651	763133.084367	41.145396
3517.840357	762865.017197	41.150400
3517.607966	762577.813047	41.155405
3517.615245	762310.386294	41.160410
3517.226893	762033.594354	41.165415
3517.708162	761767.796407	41.170420
3517.252338	761499.874839	41.175424
3517.159548	761225.421505	41.180429
3517.187122	760962.827335	41.185434
3516.798829	760703.252786	41.190439
3516.729830	760423.438359	41.195444
3516.755430	760171.670858	41.200448
3516.741308	759901.744847	41.205453
3516.452787	759647.692908	41.210458
3516.157109	759380.656618	41.215463
3516.326937	759113.731381	41.220468
3516.007085	758874.511269	41.225472
3516.020402	758606.755200	41.230477
3515.747176	758359.566241	41.235482
3515.819943	758101.948448	41.240487
3516.032253	757856.834348	41.245492
3515.544000	757609.014955	41.250496
3515.395487	757355.998391	41.255501
3515.244979	757110.574746	41.260506
3514.930943	756864.183052	41.265511
3515.067295	756622.842438	41.270516
3514.746029	756390.997907	41.275520
3514.747754	756150.602491	41.280525
3514.882415	755918.026547	41.285530
3514.634300	755686.987771	41.290535
3514.768956	755453.114174	41.295540
3514.355083	755224.162261	41.300544
3514.339827	754986.645867	41.305549
3514.099457	754749.751778	41.310554
3513.966594	754529.175319	41.315559
3513.912102	754294.310143	41.320564
3513.499636	754078.901963	41.325568
3513.684275	753859.389452	41.330573
3513.837403	753640.616572	41.335578
3513.517143	753414.113519	41.340583
3513.750464	753195.265339	41.345588
3513.516869	752988.587086	41.350592
3513.146888	752765.283082	41.355597
3513.081731	752548.540016	41.360602
3512.705696	752340.287537	41.365607
3513.368846	752119.757375	41.370612
3512.749995	751926.548139	41.375616
3512.809966	751710.847446	41.380621
3512.759822	751511.508045	41.385626
3512.468692	751311.709379	41.390631
3512.735225	751099.662066	41.395636
3512.243599	750895.835334	41.400640
3512.626567	750686.573088	41.405645
3512.231641	750485.732871	41.410650
3511.988115	750293.458175	41.415655
3512.261859	750098.227910	41.420660
3511.766873	749912.555788	41.425664
3512.017381	749709.118622	41.430669
3512.140528	749521.408215	41.435674
3512.130883	749331.541307	41.440679
3511.715952	749129.681127	41.445684
3511.616664	748939.522999	41.450688
3511.765575	748742.154657	41.455693
3511.614500	748564.200342	41.460698
3511.227217	748376.596041	41.465703
3511.538279	748180.965538	41.470708
3511.211586	748006.338242	41.475712
3510.997795	747819.284825	41.480717
3511.328804	747634.558361	41.485722
3510.852572	747467.158676	41.490727
3510.986124	747267.927019	41.495732
3510.605891	747108.163869	41.500736
3510.729491	746920.094132	41.505741
3510.688209	746754.337057	41.510746
3510.332710	746580.275668	41.515751
3510.500828	746413.537699	41.520756
3510.197163	746244.501662	41.525760
3510.199350	746085.346371	41.530765
3510.006029	745915.593006	41.535770
3509.820977	745767.583623	41.540775
3510.268486	745590.105153	41.545780
3509.872513	745431.348378	41.550784
3510.203671	745260.752677	41.555789
3509.641402	745106.218575	41.560794
3509.861803	744960.796374	41.565799
3509.947007	744790.428828	41.570804
3509.912555	744631.299499	41.575808
3509.635723	744477.101328	41.580813
3509.331159	744318.900181	41.585818
3509.256531	744168.419874	41.590823
3509.067611	744017.461167	41.595828
3509.049307	743876.952963	41.600832
3508.929576	743722.021834	41.605837
3508.787045	743578.463395	41.610842
3508.487009	743435.274474	41.615847
3508.828736	743300.234231	41.620852
3508.670371	743153.901743	41.625856
3508.341491	743015.901790	41.630861
3508.354877	742876.013295	41.635866
3508.285297	742745.630157	41.640871
3508.935783	742616.708255	41.645876
3508.700010	742484.518638	41.650880
3508.492670	742330.464726	41.655885
3508.522791	742199.165963	41.660890
3508.153831	742073.914751	41.665895
3508.601004	741926.964911	41.670900
3508.216398	741807.794864	41.675904
3508.482773	741655.380411	41.680909
3508.367121	741525.281469	41.685914
3508.064906	741396.497098	41.690919
3508.239917	741260.114179	41.695924
3508.043993	741130.219836	41.700928
3508.169125	741007.392469	41.705933
3508.131134	740871.582111	41.710938
3508.068609	740749.770965	41.715943
3508.184000	740607.105101	41.720948
3508.003335	740479.225500	41.725952
3507.719407	740346.562936	41.730957
3507.717936	740234.082383	41.735962
3507.573305	740117.864555	41.740967
3507.663652	739987.360059	41.745972
3507.372181	739873.636208	41.750976
3507.411762	739747.588144	41.755981
3507.636770	739630.757963	41.760986
3507.434223	739516.123873	41.765991
3507.717569	739389.238344	41.770996
3507.608390	739279.037662	41.776000
3506.985626	739157.443065	41.781005
3506.844468	739039.230043	41.786010
3506.994844	738936.254054	41.791015
3506.975763	738833.156318	41.796020
3507.052285	738717.722508	41.801024
3506.716609	738610.271041	41.806029
3507.095869	738503.541058	41.811034
3506.662834	738394.766945	41.816039
3506.693802	738286.013624	41.821044
3506.802966	738169.428519	41.826048
3506.648258	738075.991424	41.831053
3506.330737	737972.041262	41.836058
3506.349584	737867.291976	41.841063
3506.334012	737764.427227	41.846068
3506.222532	737673.056411	41.851072
3505.880278	737572.964587	41.856077
3505.964889	737473.345264	41.861082
3505.979132	737382.098787	41.866087
3506.473887	737286.417398	41.871092
3506.485940	737191.309462	41.876096
3506.192374	737104.267261	41.881101
3506.467089	737002.532341	41.886106
3506.004444	736909.577837	41.891111
3506.090996	736802.774522	41.896116
3506.065386	736714.793059	41.901120
3505.941828	736615.939744	41.906125
3506.191814	736530.780947	41.911130
3505.872821	736442.449073	41.916135
3505.840207	736344.517645	41.921140
3505.518097	736264.498368	41.926144
3505.933377	736161.937714	41.931149
3506.169142	736074.499898	41.936154
3505.979092	735995.445912	41.941159
3506.169063	735890.246525	41.946164
3505.695592	735811.089081	41.951168
3505.670269	735714.188069	41.956173
3505.663266	735628.369259	41.961178
3505.514144	735544.750723	41.966183
3505.685285	735459.593576	41.971188
3505.330277	735371.651796	41.976192
3505.262763	735288.413058	41.981197
3505.778049	735203.394304	41.986202
3505.185281	735117.320357	41.991207
3505.686047	735035.370976	41.996212
3505.215665	734969.816234	42.001216
3505.005152	734878.033907	42.006221
3505.265280	734795.131893	42.011226
3505.136585	734722.341460	42.016231
3505.365039	734637.166125	42.021236
3505.453715	734558.150917	42.026240
3505.051786	734484.512492	42.031245
3505.327647	734405.514353	42.036250
3504.916159	734325.143996	42.041255
3505.060739	734248.245042	42.046260
3504.910566	734180.254878	42.051264
3504.528438	734102.402032	42.056269
3504.860671	734018.935583	42.061274
3504.928489	733963.035722	42.066279
3505.185701	733874.431852	42.071284
3504.878319	733807.355582	42.076288
3504.792049	733730.341319	42.081293
3504.827529	733671.870547	42.086298
3504.520529	733610.089589	42.091303
3504.629457	733521.605355	42.096308
3504.180000	733462.866661	42.101312
3504.394741	733409.562508	42.106317
3504.617631	733327.592165	42.111322
3504.412819	733272.871231	42.116327
3504.265065	733200.565259	42.121332
3504.703966	733140.538738	42.126336
3504.388540	733072.269481	42.131341
3504.689525	732999.590505	42.136346
3504.169969	732949.474212	42.141351
3504.273198	732874.846420	42.146356
3504.509640	732815.098485	42.151360
3504.138054	732753.915760	42.156365
3504.213550	732680.181940	42.161370
3504.148253	732626.225740	42.166375
3504.195402	732562.150222	42.171380
3504.516993	732505.901259	42.176384
3504.157458	732455.507894	42.181389
3504.323044	732387.252381	42.186394
3503.912137	732329.835907	42.191399
3503.847218	732262.904776	42.196404
3503.872386	732208.633757	42.201408
3503.468183	732148.244053	42.206413
3503.949757	732093.401698	42.211418
3503.543473	732055.095099	42.216423
3503.816699	732003.257449	42.221428
3503.577797	731947.641893	42.226432
3503.889779	731907.581893	42.231437
3504.073189	731847.241385	42.236442
3503.921105	731796.512531	42.241447
3503.491961	731741.273608	42.246452
3503.819303	731688.385151	42.251456
3503.309397	731641.279678	42.256461
3503.686100	731587.689164	42.261466
3503.338911	731543.725362	42.266471
3503.349656	731481.281391	42.271476
3503.633964	731450.186508	42.276480
3503.437164	731397.036134	42.281485
3503.766556	731359.644565	42.286490
3503.025728	731302.423870	42.291495
3503.139660	731255.312099	42.296500
3503.231482	731214.938420	42.301504
3502.980253	731173.432745	42.306509
3503.301186	731126.335539	42.311514
3503.199510	731105.306246	42.316519
3503.175844	731052.570687	42.321524
3503.406227	731008.855183	42.326528
3503.237669	730971.989804	42.331533
3503.516616	730929.107710	42.336538
3502.849115	730881.875294	42.341543
3503.318410	730835.841369	42.346548
3503.209885	730796.142502	42.351552
3502.975248	730745.816890	42.356557
3503.536699	730692.338504	42.361562
3503.124644	730667.347991	42.366567
3503.483367	730618.805423	42.371572
3503.401672	730573.702965	42.376576
3503.210855	730529.113530	42.381581
3503.343907	730493.830432	42.386586
3502.942050	730442.292462	42.391591
3503.149035	730400.409962	42.396596
3503.487714	730367.221904	42.401600
3503.210680	730328.588623	42.406605
3503.315517	730279.590731	42.411610
3502.902318	730245.238757	42.416615
3502.999898	730207.236355	42.421620
3502.857883	730169.322895	42.426624
3503.197624	730130.933435	42.431629
3503.204933	730085.120185	42.436634
3502.928509	730056.985187	42.441639
3503.106672	730009.162195	42.446644
3503.010842	729974.707103	42.451648
3502.724748	729936.420145	42.456653
3503.019330	729888.775318	42.461658
3502.937439	729859.963627	42.466663
3502.903666	729814.056582	42.471668
3502.725174	729786.696919	42.476672
3502.270909	729751.903884	42.481677
3502.893218	729717.180442	42.486682
3502.488471	729687.975732	42.491687
3502.753202	729650.636517	42.496692
3502.789978	729619.575539	42.501696
3502.478734	729592.633398	42.506701
3502.906478	729554.721978	42.511706
3502.696640	729531.774810	42.516711
3502.362067	729501.666290	42.521716
3502.908540	729457.493970	42.526720
3502.434293	729430.132450	42.531725
3502.739158	729388.773408	42.536730
3502.435543	729364.305801	42.541735
3502.693764	729328.996967	42.546740
3502.615535	729301.817231	42.551744
3502.545877	729275.032240	42.556749
3502.736216	729241.071601	42.561754
3502.215204	729204.603165	42.566759
3502.495150	729182.069395	42.571764
3502.666797	729149.993692	42.576768
3502.440664	729128.236858	42.581773
3502.595325	729088.931954	42.586778
3502.373484	729065.242459	42.591783
3502.885118	729031.425985	42.596788
3502.773326	728999.941395	42.601792
3502.428016	728964.235382	42.606797
3502.309210	728935.872322	42.611802
3502.215011	728911.022008	42.616807
3502.557199	728888.179938	42.621812
3502.722332	728854.221852	42.626816
3502.247607	728830.523929	42.631821
3502.709258	728792.801505	42.636826
3502.434912	728773.924701	42.641831
3502.250667	728751.367380	42.646836
3502.451540	728725.922857	42.651840
3502.516845	728697.330402	42.656845
3502.448348	728666.828076	42.661850
3502.268831	728642.981752	42.666855
3502.395399	728612.298381	42.671860
3502.235787	728588.646752	42.676864
3502.109654	728563.552976	42.681869
3502.327654	728535.331009	42.686874
3502.177252	728518.612725	42.691879
3502.013806	728490.651783	42.696884
3502.238723	728470.552432	42.701888
3501.914089	728454.110491	42.706893
3502.170857	728417.410925	42.711898
3502.419415	728413.060261	42.716903
3501.995656	728373.500736	42.721908
3502.450572	728357.078390	42.726912
3502.227383	728326.947117	42.731917
3502.242483	728306.535272	42.736922
3502.129797	728282.280548	42.741927
3502.116341	728252.262954	42.746932
3502.417683	728227.989189	42.751936
3502.553952	728214.591499	42.756941
3502.910422	728171.087618	42.761946
3502.156409	728152.140022	42.766951
3502.566440	728116.255933	42.771956
3502.323170	728086.523401	42.776960
3502.384038	728067.589565	42.781965
3502.362939	728031.528653	42.786970
3502.349267	728012.607008	42.791975
3502.502289	727993.410075	42.796980
3502.128218	727959.834611	42.801985
3501.988125	727937.614521	42.806989
3502.509873	727913.600640	42.811994
3502.335286	727895.993356	42.816999
3502.365640	727867.156069	42.822004
3502.700337	727842.281165	42.827009
3502.049055	727821.730527	42.832013
3502.116252	727789.617201	42.837018
3502.170085	727764.045360	42.842023
3502.123844	727735.071642	42.847028
3502.313831	727718.939504	42.852033
3502.037642	727693.719227	42.857037
3502.349373	727667.410887	42.862042
3502.070249	727651.207512	42.867047
3502.325295	727625.601988	42.872052
3502.227577	727603.473069	42.877057
3501.918658	727581.824869	42.882061
3502.396832	727545.827936	42.887066
3502.399880	727532.252975	42.892071
3502.053646	727499.909577	42.897076
3502.102501	727488.407759	42.902081
3502.220708	727458.315949	42.907085
3502.193170	727430.378459	42.912090
3501.842001	727413.344286	42.917095
3502.145425	727395.706474	42.922100
3502.338437	727361.935754	42.927105
3502.174809	727357.751735	42.932109
3502.164023	727318.465653	42.937114
3502.039508	727301.691054	42.942119
3502.032990	727274.542258	42.947124
3502.130256	727254.312384	42.952129
3501.576652	727250.589105	42.957133
3502.193374	727219.423156	42.962138
3502.176053	727227.898201	42.967143
3501.943620	727201.331480	42.972148
3502.079148	727175.347944	42.977153
3501.581019	727157.742989	42.982157
3501.927450	727129.445405	42.987162
3501.978588	727119.379490	42.992167
3502.162448	727096.211771	42.997172
3502.005565	727069.731227	43.002177
3501.702332	727070.475095	43.007181
3502.129204	727042.362099	43.012186
3502.058868	727029.987518	43.017191
3501.882506	727008.216802	43.022196
3501.988505	726984.219360	43.027201
3502.132860	726968.687833	43.032205
3502.409765	726946.842052	43.037210
3502.037614	726936.796314	43.042215
3501.862680	726890.995243	43.047220
3502.170396	726880.886635	43.052225
3501.800994	726865.043440	43.057229
3502.263849	726843.117108	43.062234
3502.014712	726820.317441	43.067239
3501.823204	726794.733569	43.072244
3501.804452	726783.836495	43.077249
3501.551811	726771.243915	43.082253
3501.678217	726736.887063	43.087258
3501.805703	726742.019023	43.092263
3501.705379	726722.860978	43.097268
3501.785487	726709.371012	43.102273
3501.614087	726688.242740	43.107277
3502.076493	726673.847235	43.112282
3502.103765	726663.388323	43.117287
3501.819230	726638.413906	43.122292
3501.915472	726612.881010	43.127297
3501.811339	726595.903404	43.132301
3501.976933	726583.439613	43.137306
3501.963455	726573.036868	43.142311
3501.943144	726556.342617	43.147316
3501.985612	726542.115373	43.152321
3501.806353	726520.492483	43.157325
3502.071070	726488.390963	43.162330
3501.766990	726483.238731	43.167335
3501.809915	726458.853785	43.172340
3502.070436	726450.734400	43.177345
3501.561635	726438.530480	43.182349
3501.626823	726407.502142	43.187354
3501.609188	726406.662848	43.192359
3501.927788	726390.506844	43.197364
3501.930265	726370.290453	43.202369
3501.414636	726357.988441	43.207373
3501.798077	726349.006303	43.212378
3501.795746	726326.610422	43.217383
3501.888004	726307.766429	43.222388
3501.793087	726298.367788	43.227393
3501.749242	726281.429118	43.232397
3501.749090	726256.059690	43.237402
3501.921192	726258.211578	43.242407
3501.544183	726230.724146	43.247412
3501.998446	726213.653473	43.252417
3501.459099	726217.706750	43.257421
3501.919293	726192.954758	43.262426
3501.974212	726177.486065	43.267431
3501.838802	726161.553288	43.272436
3502.116387	726134.106012	43.277441
3502.110948	726127.516782	43.282445
3502.082174	726098.187530	43.287450
3501.501017	726085.301324	43.292455
3501.861459	726076.570446	43.297460
3501.909190	726046.534651	43.302465
3501.557147	726033.114988	43.307469
3501.723187	726018.668211	43.312474
3501.703455	726009.256814	43.317479
3501.827274	725987.631986	43.322484
3501.856470	725973.604157	43.327489
3501.650978	725974.431069	43.332493
3501.515482	725941.006096	43.337498
3501.659486	725928.941296	43.342503
3501.246347	725929.108798	43.347508
3501.608125	725921.616335	43.352513
3501.458923	725905.041162	43.357517
3501.644202	725890.491877	43.362522
3501.437072	725885.967424	43.367527
3501.832666	725873.910521	43.372532
3501.799899	725848.347013	43.377537
3501.670115	725838.904054	43.382541
3501.575805	725824.995486	43.387546
3501.757582	725826.848574	43.392551
3501.635384	725788.614176	43.397556
3502.025253	725790.779755	43.402561
3501.607127	725775.983111	43.407565
3501.809201	725749.042557	43.412570
3501.807457	725742.402854	43.417575
3501.801181	725736.754959	43.422580
3501.464124	725710.745775	43.427585
3501.149725	725715.356761	43.432589
3501.281061	725696.703122	43.437594
3501.247986	725696.411394	43.442599
3501.092238	725702.482773	43.447604
3501.480671	725694.093739	43.452609
3501.315288	725676.579263	43.457613
3501.566556	725660.284292	43.462618
3501.356486	725653.034746	43.467623
3501.327656	725641.741391	43.472628
3501.701998	725645.891724	43.477633
3501.171074	725625.761644	43.482637
3501.443634	725601.683082	43.487642
3501.404290	725602.730344	43.492647
3501.501660	725603.556798	43.497652
3501.720308	725595.889477	43.502657
3501.363044	725576.672105	43.507661
3501.575293	725570.541997	43.512666
3501.471745	725561.490816	43.517671
3501.126524	725558.624291	43.522676
3501.462310	725548.410302	43.527681
3501.481694	725549.249649	43.532685
3501.393121	725512.941029	43.537690
3501.359133	725516.316478	43.542695
3501.429324	725509.367373	43.547700
3501.635200	725507.995506	43.552705
3501.488659	725484.778732	43.557709
3501.454708	725461.989279	43.562714
3501.617910	725460.327127	43.567719
3501.793196	725468.425277	43.572724
3501.906973	725448.634218	43.577729
3501.624029	725423.209839	43.582733
3501.675093	725410.317201	43.587738
3501.509638	725407.272250	43.592743
3501.024770	725383.615547	43.597748
3501.529218	725376.991011	43.602753
3501.453748	725377.945160	43.607757
3501.180061	725370.804987	43.612762
3501.441395	725368.631047	43.617767
3501.517966	725359.847211	43.622772
3501.803971	725334.328538	43.627777
3501.474400	725334.184904	43.632781
3501.507824	725322.236599	43.637786
3501.662794	725320.972225	43.642791
3501.726547	725296.035273	43.647796
3501.667251	725270.523908	43.652801
3501.623515	725275.288635	43.657805
3501.514172	725251.519938	43.662810
3501.644208	725233.856587	43.667815
3501.647393	725241.289615	43.672820
3502.095016	725215.347416	43.677825
3501.577318	725204.877591	43.682829
3501.530506	725187.540703	43.687834
3501.673378	725182.412901	43.692839
3501.393983	725168.583363	43.697844
3501.695060	725147.967723	43.702849
3501.563517	725141.844552	43.707853
3501.505031	725148.395833	43.712858
3501.710099	725128.341134	43.717863
3501.612065	725107.345334	43.722868
3501.511440	725091.256060	43.727873
3501.308354	725090.397719	43.732877
3501.415462	725073.530726	43.737882
3501.696411	725059.261506	43.742887
3501.371962	725047.768400	43.747892
3501.311277	725039.700707	43.752897
3501.514246	725048.934517	43.757901
3501.737716	725029.719011	43.762906
3501.578837	725011.161334	43.767911
3501.231222	724997.887914	43.772916
3501.540600	724997.985589	43.777921
3501.326830	724999.606885	43.782925
3501.213646	724978.068125	43.787930
3501.258711	724974.591762	43.792935
3501.204026	724966.572564	43.797940
3501.183478	724962.314113	43.802945
3501.081678	724955.838983	43.807949
3501.193257	724957.654312	43.812954
3501.519563	724956.906706	43.817959
3501.508687	724963.450267	43.822964
3501.325031	724942.616869	43.827969
3501.603307	724925.869962	43.832973
3501.604706	724912.836078	43.837978
3501.526370	724913.889871	43.842983
3501.266045	724912.941854	43.847988
3501.571493	724876.565311	43.852993
3501.533724	724881.428397	43.857997
3501.510505	724873.056999	43.863002
3501.618284	724870.511837	43.868007
3501.284047	724851.982779	43.873012
3501.582195	724826.014499	43.878017
3501.341102	724829.870483	43.883021
3501.831094	724820.670844	43.888026
3501.355823	724820.006129	43.893031
3501.449441	724801.059342	43.898036
3501.640088	724790.125019	43.903041
3501.370334	724781.596033	43.908045
3501.569450	724778.391483	43.913050
3501.708635	724758.941480	43.918055
3501.373190	724753.991572	43.923060
3501.625605	724730.409385	43.928065
3501.432288	724736.289445	43.933069
3501.621017	724724.017253	43.938074
3501.619707	724702.360165	43.943079
3501.217721	724702.278042	43.948084
3501.790340	724697.128482	43.953089
3501.420767	724691.341666	43.958093
3501.688421	724657.398816	43.963098
3501.399988	724650.409130	43.968103
3501.604018	724648.244472	43.973108
3501.540308	724642.803555	43.978113
3501.537732	724633.833786	43.983117
3501.408977	724605.209566	43.988122
3501.636403	724602.842791	43.993127
3501.737212	724608.575217	43.998132
3501.944501	724578.953735	44.003137
3501.839420	724561.129555	44.008141
3501.523452	724549.188306	44.013146
3501.444350	724538.347786	44.018151
3501.737388	724525.017293	44.023156
3502.095010	724506.521807	44.028161
3501.614128	724499.018627	44.033165
3501.629999	724469.279702	44.038170
3501.808773	724457.405245	44.043175
3501.390271	724461.786325	44.048180
3501.660356	724438.844675	44.053185
3501.466063	724429.559437	44.058189
3501.257664	724419.780910	44.063194
3501.653463	724422.094563	44.068199
3501.720295	724417.623146	44.073204
3501.774604	724383.169251	44.078209
3501.428096	724373.116122	44.083213
3501.679110	724369.605471	44.088218
3501.386584	724354.785503	44.093223
3501.493906	724343.467866	44.098228
3501.656125	724318.164751	44.103233
3501.543104	724328.690631	44.108237
3501.545225	724312.929787	44.113242
3501.546662	724292.658898	44.118247
3501.232845	724287.903380	44.123252
3501.648850	724281.143903	44.128257
3501.457522	724292.822694	44.133261
3501.094723	724276.775151	44.138266
3501.667472	724258.045311	44.143271
3501.595782	724245.765881	44.148276
3501.587260	724244.825735	44.153281
3501.567272	724245.919532	44.158285
3501.381272	724218.195546	44.163290
3501.359345	724205.907833	44.168295
3501.016902	724198.183250	44.173300
3501.175777	724190.673191	44.178305
3500.967294	724197.993451	44.183309
3501.141238	724202.574139	44.188314
3501.233223	724201.766066	44.193319
3500.940144	724203.450184	44.198324
3501.310851	724195.806000	44.203329
3501.044805	724192.430281	44.208333
3501.060318	724171.066392	44.213338
3501.074685	724160.903805	44.218343
3501.054273	724149.260072	44.223348
3501.517830	724149.431409	44.228353
3500.977336	724150.660795	44.233357
3501.221046	724155.279543	44.238362
3501.316492	724140.742015	44.243367
3501.120265	724141.567573	44.248372
3501.183360	724151.568948	44.253377
3501.342775	724154.665182	44.258381
3501.350027	724139.943976	44.263386
3501.282679	724118.147578	44.268391
3501.358424	724107.677405	44.273396
3501.693457	724098.601700	44.278401
3501.200302	724097.295556	44.283405
3501.191546	724099.973534	44.288410
3501.541357	724092.332708	44.293415
3501.079298	724080.464481	44.298420
3501.445112	724066.526465	44.303425
3501.174457	724059.037704	44.308429
3501.133191	724058.102947	44.313434
3501.802803	724066.566863	44.318439
3501.628905	724060.648137	44.323444
3501.157436	724033.664589	44.328449
3501.441698	724021.226876	44.333453
3501.067264	724024.113997	44.338458
3501.411518	724025.544140	44.343463
3500.935380	724025.870766	44.348468
3501.620157	724011.681695	44.353473
3501.156935	724005.166414	44.358477
3501.138777	723987.822264	44.363482
3501.323541	723976.986965	44.368487
3501.227527	723978.390743	44.373492
3501.604138	723973.223566	44.378497
3501.588015	723978.579245	44.383501
3501.464353	723971.611314	44.388506
3501.511602	723944.591320	44.393511
3501.365563	723936.933162	44.398516
3501.829693	723934.279262	44.403521
3501.305345	723938.132902	44.408525
3501.339325	723896.295294	44.413530
3501.412781	723897.125874	44.418535
3501.098955	723898.912609	44.423540
3501.622717	723897.289692	44.428545
3501.310090	723892.038105	44.433549
3501.479179	723887.004296	44.438554
3501.580941	723857.348099	44.443559
3501.567623	723851.600945	44.448564
3501.647237	723842.121087	44.453569
3501.329720	723832.855538	44.458573
3501.215301	723827.224203	44.463578
3501.050282	723795.777977	44.468583
3501.330557	723799.498716	44.473588
3501.520684	723795.551802	44.478593
3501.204300	723796.645073	44.483597
3501.440305	723789.766248	44.488602
3501.442869	723792.591149	44.493607
3501.059682	723777.735558	44.498612
3501.158707	723749.615939	44.503617
3501.129701	723752.297376	44.508621
3501.478599	723752.239847	44.513626
3501.842409	723742.316390	44.518631
3501.375412	723749.679766	44.523636
3501.331738	723730.852339	44.528641
3501.192496	723709.958916	44.533645
3500.885409	723707.085432	44.538650
3501.245441	723695.378189	44.543655
3501.083694	723701.402463	44.548660
3501.266153	723696.019371	44.553665
3501.361098	723706.065588	44.558669
3501.134352	723711.357115	44.563674
3501.116125	723705.214147	44.568679
3500.899221	723708.323171	44.573684
3501.239803	723706.829620	44.578689
3501.337293	723700.617961	44.583693
3501.311296	723683.076205	44.588698
3501.486606	723669.268133	44.593703
3501.063021	723668.297379	44.598708
3501.347697	723667.308716	44.603713
3501.364772	723661.853800	44.608717
3501.280996	723660.380801	44.613722
3501.578502	723640.604606	44.618727
3501.065293	723631.172905	44.623732
3501.360672	723610.703068	44.628737
3501.258212	723625.788166	44.633741
3501.152476	723623.971828	44.638746
3501.249178	723616.669786	44.643751
3501.140175	723616.539228	44.648756
3501.442708	723609.054468	44.653761
3501.204347	723581.683955	44.658765
3501.208692	723589.316546	44.663770
3501.559394	723579.345494	44.668775
3501.263974	723574.784786	44.673780
3501.228280	723584.010115	44.678785
3501.165951	723584.962298	44.683789
3501.437433	723575.896524	44.688794
3501.102616	723558.901198	44.693799
3501.252784	723546.633630	44.698804
3501.296160	723550.938860	44.703809
3501.063171	723549.044402	44.708813
3500.991314	723544.198901	44.713818
3501.714060	723545.913548	44.718823
3501.074339	723551.273421	44.723828
3501.110734	723535.802827	44.728833
3500.910225	723545.402400	44.733837
3501.117716	723537.338485	44.738842
3501.222040	723506.738844	44.743847
3501.099828	723512.261056	44.748852
3501.082706	723505.423824	44.753857
3501.061321	723498.190759	44.758861
3501.088009	723494.815943	44.763866
3501.525118	723500.790967	44.768871
3500.798129	723511.419347	44.773876
3501.199503	723491.576065	44.778881
3501.172655	723504.368822	44.783885
3501.186468	723502.879668	44.788890
3501.112584	723499.471907	44.793895
3500.999756	723503.505575	44.798900
3501.190642	723489.595495	44.803905
3501.005403	723465.288952	44.808909
3500.820302	723464.923132	44.813914
3501.099632	723458.978643	44.818919
3501.109848	723469.138285	44.823924
3501.179900	723459.461301	44.828929
3501.294226	723457.112892	44.833933
3501.102267	723458.978714	44.838938
3501.379364	723457.396477	44.843943
3501.346885	723464.688300	44.848948
3501.407690	723456.945948	44.853953
3501.173633	723436.761438	44.858957
3500.972827	723427.228310	44.863962
3501.249830	723418.607555	44.868967
3501.116331	723416.101819	44.873972
3501.188437	723419.956266	44.878977
3501.513602	723421.587940	44.883981
3501.138664	723421.650026	44.888986
3501.222939	723412.615009	44.893991
3500.821087	723416.250376	44.898996
3501.431849	723413.026844	44.904001
3501.328312	723395.150320	44.909005
3501.061475	723376.656366	44.914010
3501.273448	723379.099832	44.919015
3501.273585	723381.033063	44.924020
3501.232384	723376.083262	44.929025
3501.428606	723377.587552	44.934029
3501.329738	723374.828243	44.939034
3501.073040	723352.069764	44.944039
3501.393252	723344.234871	44.949044
3501.381024	723334.224365	44.954049
3501.240767	723332.165829	44.959053
3501.196707	723339.707514	44.964058
3501.322382	723335.176220	44.969063
3500.993303	723335.924674	44.974068
3501.467311	723331.682790	44.979073
3501.429556	723322.816544	44.984077
3500.991782	723299.939140	44.989082
3501.456599	723286.776538	44.994087
3501.310298	723296.813552	44.999092
3501.067541	723288.179417	45.004097
3501.315398	723291.410066	45.009101
3501.521461	723286.815894	45.014106
3501.224535	723268.871918	45.019111
3501.107320	723256.053289	45.024116
3501.465796	723250.293845	45.029121
3501.328113	723243.030206	45.034125
3501.243627	723253.404035	45.039130
3501.172291	723253.316814	45.044135
3501.376437	723251.300481	45.049140
3501.122933	723239.693982	45.054145
3501.633096	723225.383721	45.059149
3501.350739	723217.350875	45.064154
3501.453912	723212.971938	45.069159
3501.156588	723216.193572	45.074164
3501.750193	723210.246540	45.079169
3501.396493	723192.163074	45.084173
3501.061716	723171.845854	45.089178
3501.652302	723159.703208	45.094183
3501.370017	723167.879241	45.099188
3501.233179	723158.682211	45.104193
3501.000637	723172.104297	45.109197
3501.140792	723163.258049	45.114202
3501.178232	723151.752054	45.119207
3500.972848	723131.859472	45.124212
3501.283953	723115.301749	45.129217
3501.448780	723121.619459	45.134221
3501.312418	723121.493413	45.139226
3501.565945	723113.520617	45.144231
3500.934669	723113.922476	45.149236
3501.206003	723114.869143	45.154241
3501.224110	723117.642138	45.159245
3501.090779	723095.953081	45.164250
3501.532911	723078.977081	45.169255
3501.337778	723077.819794	45.174260
3501.488716	723074.176428	45.179265
3501.380299	723070.873335	45.184269
3501.372165	723076.525693	45.189274
3501.291487	723047.838554	45.194279
3500.965768	723046.108009	45.199284
3501.142013	723031.208192	45.204289
3500.950510	723030.099868	45.209293
3501.292846	723038.024101	45.214298
3501.381152	723035.283317	45.219303
3501.329669	723039.059226	45.224308
3501.216611	723039.524160	45.229313
3501.449659	723035.817640	45.234317
3501.164051	723015.739758	45.239322
3501.822344	722993.374351	45.244327
3501.529687	722992.134028	45.249332
3501.379237	722987.896023	45.254337
3501.609641	722988.849469	45.259341
3501.537938	722961.251080	45.264346
3501.568545	722952.918408	45.269351
3501.213934	722958.082833	45.274356
3501.483342	722946.934780	45.279361
3501.283526	722923.174319	45.284365
3501.035870	722917.068677	45.289370
3501.229794	722897.902668	45.294375
3501.422706	722915.517902	45.299380
3501.496507	722908.318160	45.304385
3501.494032	722910.945915	45.309389
3501.284738	722902.851117	45.314394
3501.480061	722878.628669	45.319399
3501.465598	722886.364158	45.324404
3501.226150	722878.918733	45.329409
3501.328590	722883.809395	45.334413
3501.283113	722882.726490	45.339418
3501.777242	722869.211391	45.344423
3501.180499	722857.760216	45.349428
3501.359321	722843.851046	45.354433
3501.387310	722827.736099	45.359437
3501.434328	722831.743678	45.364442
3501.777064	722822.417454	45.369447
3501.493540	722809.625614	45.374452
3501.272460	722787.404970	45.379457
3501.699930	722790.358281	45.384461
3501.409504	722782.475056	45.389466
3501.785928	722767.145117	45.394471
3501.207862	722759.705971	45.399476
3501.474680	722747.913655	45.404481
3501.495953	722750.785391	45.409485
3501.328266	722740.353715	45.414490
3501.437498	722719.615011	45.419495
3501.489599	722713.310970	45.424500
3501.556842	722708.541134	45.429505
3501.434406	722703.306926	45.434509
3501.127401	722694.434928	45.439514
3501.413930	722689.331415	45.444519
3501.330088	722676.208942	45.449524
3501.668951	722667.527614	45.454529
3501.542648	722655.750558	45.459533
3501.418257	722652.499509	45.464538
3501.683314	722632.280124	45.469543
3501.261639	722625.806449	45.474548
3501.447301	722609.367590	45.479553
3501.547096	722607.170058	45.484557
3501.554604	722608.705676	45.489562
3501.513230	722581.497582	45.494567
3501.498483	722579.219828	45.499572
3501.694990	722557.772286	45.504577
3501.893279	722564.630188	45.509581
3501.392771	722546.073843	45.514586
3501.523603	722526.223387	45.519591
3501.223741	722529.049124	45.524596
3501.128446	722521.529983	45.529601
3501.413104	722514.691635	45.534605
3501.130331	722506.311155	45.539610
3501.548368	722497.120840	45.544615
3501.549913	722471.789054	45.549620
3501.534109	722469.808880	45.554625
3501.497263	722468.377485	45.559629
3500.985241	722465.636573	45.564634
3501.474333	722462.036205	45.569639
3501.639006	722442.477393	45.574644
3501.182781	722426.342536	45.579649
3501.808326	722425.198256	45.584653
3501.515545	722428.716879	45.589658
3501.552039	722401.346607	45.594663
3501.627463	722384.181920	45.599668
3501.313794	722378.879961	45.604673
3501.557527	722372.692714	45.609677
3501.380345	722372.077666	45.614682
3501.630889	722344.473540	45.619687
3501.342169	722348.041100	45.624692
3501.539560	722329.170644	45.629697
3501.826187	722335.667123	45.634701
3501.706838	722307.479543	45.639706
3501.689934	722295.089010	45.644711
3501.376595	722295.487933	45.649716
3501.563149	722288.467317	45.654721
3501.299170	722264.665991	45.659725
3501.410101	722254.732974	45.664730
3501.708525	722260.979693	45.669735
3501.438415	722256.909809	45.674740
3501.467853	722233.704370	45.679745
3501.527831	722216.442740	45.684749
3501.377647	722210.171744	45.689754
3501.398653	722208.879466	45.694759
3501.126728	722205.603045	45.699764
3501.204625	722200.682434	45.704769
3501.168630	722197.961916	45.709773
3500.837382	722188.944656	45.714778
3501.519269	722176.190597	45.719783
3501.391505	722175.765665	45.724788
3501.629955	722173.991278	45.729793
3501.752689	722172.285587	45.734797
3501.116194	722147.306118	45.739802
3501.549921	722131.965539	45.744807
3501.416387	722131.144960	45.749812
3501.192833	722121.812381	45.754817
3501.549672	722098.949061	45.759821
3501.041392	722037.014597	45.764826
3501.441238	721924.510894	45.769831
3500.899638	721741.067895	45.774836
3501.142026	721520.208346	45.779841
3501.016302	721223.942954	45.784845
3500.013325	720879.915590	45.789850
3500.162357	720480.991878	45.794855
3500.006849	720030.776604	45.799860
3500.152121	719528.219220	45.804865
3499.959264	718958.686559	45.809869
3499.370297	718337.252168	45.814874
3499.226173	717653.746067	45.819879
3498.816251	716923.896441	45.824884
3498.443026	716108.101745	45.829889
3498.207593	715263.031216	45.834893
3497.127827	714355.294847	45.839898
3496.815704	713388.526710	45.844903
3495.939122	712369.428880	45.849908
3495.679583	711287.760478	45.854913
3495.516679	710150.732993	45.859917
3494.401901	708953.135529	45.864922
3493.948486	707689.114591	45.869927
3493.304283	706378.053239	45.874932
3492.652307	705001.768931	45.879937
3491.917646	703568.689828	45.884941
3490.927451	702083.239772	45.889946
3490.170082	700531.892966	45.894951
3489.256173	698930.586937	45.899956
3488.550272	697265.413310	45.904961
3487.770280	695541.207558	45.909965
3486.604680	693754.854574	45.914970
3485.786311	691911.669817	45.919975
3484.769068	690023.304239	45.924980
3483.473925	688080.287923	45.929985
3482.376868	686066.578880	45.934989
3481.107442	684023.023774	45.939994
3480.143687	681905.648504	45.944999
3478.939758	679731.631613	45.950004
3477.936407	677518.701558	45.955009
3476.736277	675228.422695	45.960013
3475.038369	672905.110285	45.965018
3474.206827	670509.672921	45.970023
3472.906064	668077.095452	45.975028
3471.648274	665576.535893	45.980033
3470.223354	663037.922784	45.985037
3468.662921	660434.569444	45.990042
3467.411503	657780.685601	45.995047
3465.720952	655077.108279	46.000052
3464.191688	652328.249147	46.005057
3462.718986	649526.397959	46.010061
3460.956901	646671.473598	46.015066
3459.566390	643755.378002	46.020071
3457.929655	640806.626806	46.025076
3456.296671	637798.791612	46.030081
3454.629352	634746.848363	46.035085
3452.639729	631644.806681	46.040090
3451.298372	628489.315403	46.045095
3449.603837	625293.975474	46.050100
3447.838066	622053.703202	46.055105
3445.974881	618740.655219	46.060109
3443.953177	615399.807278	46.065114
3442.159762	611990.759231	46.070119
3439.938010	608557.012085	46.075124
3438.207647	605083.347912	46.080129
3436.267861	601549.778780	46.085133
3434.363678	597971.535917	46.090138
3432.177390	594348.643186	46.095143
3429.918719	590674.807429	46.100148
3428.105695	586959.860708	46.105153
3426.257891	583191.440550	46.110157
3423.817762	579398.772496	46.115162
3421.793067	575542.594736	46.120167
3419.775025	571658.559204	46.125172
3417.191531	567721.380917	46.130177
3415.249604	563740.294023	46.135181
3412.666994	559732.058199	46.140186
3410.290692	555657.277496	46.145191
3408.158428	551562.118323	46.150196
3405.781108	547420.143976	46.155201
3403.337092	543237.605196	46.160205
3400.611830	539021.733932	46.165210
3398.356877	534761.799778	46.170215
3396.123968	530468.659637	46.175220
3393.384226	526121.843926	46.180225
3391.052920	521740.569042	46.185229
3388.242309	517331.440249	46.190234
3386.031827	512874.772378	46.195239
3382.911664	508393.088550	46.200244
3380.376707	503869.509740	46.205249
3378.134349	499306.652856	46.210253
3375.375316	494717.594493	46.215258
3372.197090	490082.132284	46.220263
3369.472398	485418.432872	46.225268
3367.161455	480727.569882	46.230273
3364.075212	475993.489520	46.235277
3361.329179	471226.030683	46.240282
3358.419625	466419.351128	46.245287
3355.783387	461601.099148	46.250292
3352.585513	456727.585006	46.255297
3349.782362	451825.867737	46.260301
3346.605503	446912.161082	46.265306
3343.570545	441955.306220	46.270311
3340.433802	436975.741581	46.275316
3337.559380	431978.903983	46.280321
3334.429670	426939.621056	46.285325
3331.132408	421888.371026	46.290330
3328.506601	416794.927487	46.295335
3325.124961	411693.817662	46.300340
3321.651648	406556.385538	46.305345
3318.899888	401394.424694	46.310349
3315.662638	396211.712883	46.315354
3312.460165	390997.818949	46.320359
3308.910884	385767.618340	46.325364
3305.865271	380511.998523	46.330369
3302.634412	375230.436210	46.335373
3298.947319	369945.531390	46.340378
3295.660080	364620.502905	46.345383
3292.076606	359287.968821	46.350388
3288.600060	353941.155337	46.355393
3285.477851	348569.215076	46.360397
3281.982113	343180.745533	46.365402
3278.180951	337781.367001	46.370407
3274.817715	332350.987037	46.375412
3271.247514	326910.461573	46.380417
3267.656541	321465.014983	46.385421
3264.163999	316001.045897	46.390426
3260.230981	310523.847348	46.395431
3256.900574	305035.881301	46.400436
3252.844903	299553.803932	46.405441
3249.436259	294030.065994	46.410445
3245.506990	288535.867701	46.415450
3242.187631	283000.346359	46.420455
3238.359498	277465.388182	46.425460
3234.205212	271924.179135	46.430465
3230.720120	266378.505907	46.435469
3226.502861	260824.108401	46.440474
3222.424643	255268.270036	46.445479
3218.558298	249704.577275	46.450484
3214.778626	244156.421456	46.455489
3211.152747	238575.776201	46.460493
3206.702320	233028.194456	46.465498
3202.817207	227474.701466	46.470503
3198.618458	221905.121277	46.475508
3194.415296	216344.986373	46.480513
3190.532469	210784.837513	46.485517
3186.505446	205161.908882	46.490522
3182.473764	199584.886387	46.495527
3178.499265	194057.482811	46.500532
3173.842288	188510.935482	46.505537
3170.163553	182974.768517	46.510541
3165.154760	177450.382036	46.515546
3161.177547	171931.418236	46.520551
3156.878664	166431.510130	46.525556
3152.254631	160941.356484	46.530561
3148.123165	155455.098108	46.535565
3143.291158	149994.130597	46.540570
3138.878988	144544.147665	46.545575
3134.493550	139109.596977	46.550580
3129.546987	133705.783942	46.555585
3125.289689	128305.026560	46.560589
3120.480973	122937.743129	46.565594
3116.093897	117578.730322	46.570599
3110.954839	112250.137653	46.575604
3106.204883	106956.508160	46.580609
3101.467699	101664.372311	46.585613
3096.032474	96430.317642	46.590618
3091.317099	91219.826589	46.595623
3086.377463	86035.378754	46.600628
3081.342713	80882.171794	46.605633
3075.972626	75766.898232	46.610637
3070.796316	70698.030625	46.615642
3065.287878	65658.715180	46.620647
3059.819971	60670.369892	46.625652
3054.170027	55732.145844	46.630657
3048.374919	50840.021918	46.635661
3042.243915	46014.017933	46.640666
3035.718702	41245.906067	46.645671
3025.060408	36670.375659	46.650676
3008.729943	32310.511115	46.655681
2993.559537	28127.451387	46.660685
2975.617445	24226.357130	46.665690
2952.779378	20740.866073	46.670695
2926.632276	17669.865608	46.675700
2900.004083	15010.748635	46.680705
2877.207272	12748.771291	46.685709
2857.048403	10876.069301	46.690714
2840.345457	9349.343949	46.695719
2827.057553	8143.167065	46.700724
2815.951981	7224.909784	46.705729
2808.152957	6530.885503	46.710733
2801.686298	6027.322314	46.715738
2797.060542	5668.539699	46.720743
2793.378588	5418.437585	46.725748
2791.367387	5251.854363	46.730753
2789.528523	5129.774732	46.735757
2788.216300	5053.216030	46.740762
2786.932019	4987.862168	46.745767
2785.891274	4930.958755	46.750772
2785.060857	4875.076417	46.755777
2784.240435	4803.243766	46.760781
2783.439732	4721.652889	46.765786
2782.383513	4612.077892	46.770791
2780.953420	4486.635949	46.775796
2778.958637	4350.215629	46.780801
2777.624014	4196.292514	46.785805
2775.482878	4028.665993	46.790810
2773.574234	3858.491258	46.795815
2771.154742	3659.793527	46.800820
2768.519760	3452.985755	46.805825
2766.394886	3234.375643	46.810829
2763.551502	3012.436619	46.815834
2760.667190	2779.034726	46.820839
2757.682014	2525.573972	46.825844
2754.688228	2280.292818	46.830849
2751.571217	2015.600929	46.835853
2748.730244	1761.515324	46.840858
2745.336587	1500.044012	46.845863
2741.889514	1237.393543	46.850868
2737.940318	970.759731	46.855873
2734.500397	709.818548	46.860877
2730.463128	474.324850	46.865882
2726.120110	239.144261	46.870887
2717.323045	149.052317	46.875892
2704.918941	198.360484	46.880897
2697.883392	195.440322	46.885901
2694.036939	213.370530	46.890906
2692.312316	208.542312	46.895911
2690.791155	212.071051	46.900916
2688.722344	203.055652	46.905921
2686.367046	207.959586	46.910925
2683.459012	201.591088	46.915930
2679.929246	199.292410	46.920935
2676.582908	201.796188	46.925940
2673.414790	207.251065	46.930945
2670.017358	193.976237	46.935949
2666.627779	199.610650	46.940954
2663.504912	206.292987	46.945959
2660.217625	198.455746	46.950964
2656.329248	202.287173	46.955969
2653.365422	195.571938	46.960973
2649.986318	200.942170	46.965978
2646.264180	197.135931	46.970983
2643.414400	192.658388	46.975988
2639.673753	194.403187	46.980993
2636.662675	194.283136	46.985997
2633.196712	197.601036	46.991002
2629.530523	192.337681	46.996007
2626.136495	190.899470	47.001012
2622.462311	202.900985	47.006017
2619.794989	182.446358	47.011021
2616.239753	197.525995	47.016026
2612.651562	191.416778	47.021031
2609.108826	194.320761	47.026036
2605.464640	196.369900	47.031041
2602.180422	188.977796	47.036045
2598.583765	192.698221	47.041050
2595.161884	188.043892	47.046055
2591.867313	189.154440	47.051060
2588.533621	198.914285	47.056065
2585.396771	183.039494	47.061069
2581.919042	192.805229	47.066074
2578.653358	191.164651	47.071079
2574.889234	194.371327	47.076084
2571.260644	190.314049	47.081089
2567.988775	189.899973	47.086093
2564.385643	190.564929	47.091098
2560.551280	182.201283	47.096103
2557.623119	184.312476	47.101108
2554.293617	191.067176	47.106113
2550.537230	180.046302	47.111117
2547.020396	185.966696	47.116122
2544.005897	190.916493	47.121127
2540.324043	189.009377	47.126132
2536.784270	181.539663	47.131137
2533.292524	185.471878	47.136141
2529.954764	184.898044	47.141146
2525.856527	183.569212	47.146151
2522.938750	188.093730	47.151156
2519.138571	184.040836	47.156161
2515.810475	177.868519	47.161165
2512.786013	182.312235	47.166170
2509.388142	189.795610	47.171175
2505.905877	184.177296	47.176180
2501.955407	186.485426	47.181185
2498.674885	183.187956	47.186189
2495.237994	179.569461	47.191194
2490.982120	188.109973	47.196199
2488.336493	184.172006	47.201204
2484.543811	193.299081	47.206209
2481.358501	185.545955	47.211213
2477.647874	179.134296	47.216218
2474.067191	182.162281	47.221223
2470.905603	184.561422	47.226228
2467.054724	180.872181	47.231233
2464.179078	174.592824	47.236237
2460.526526	175.342815	47.241242
2456.992443	171.487265	47.246247
2453.589116	171.761258	47.251252
2449.931328	175.980333	47.256257
2446.727876	175.799524	47.261261
2442.909088	172.810279	47.266266
2439.465665	178.771482	47.271271
2436.279337	176.553492	47.276276
2432.427324	175.010520	47.281281
2429.378929	166.264072	47.286285
2425.525213	173.749774	47.291290
2421.599477	174.001372	47.296295
2418.507563	160.718645	47.301300
2414.687582	174.166252	47.306305
2411.517184	165.849892	47.311309
2408.001460	171.511296	47.316314
2404.116645	161.790598	47.321319
2401.359797	154.948551	47.326324
2397.435131	167.699338	47.331329
2394.251281	155.849336	47.336333
2390.691398	163.760998	47.341338
2386.780497	162.709325	47.346343
2384.162737	152.439599	47.351348
2379.985582	168.602930	47.356353
2377.060116	160.529416	47.361357
2373.420945	164.127605	47.366362
2369.908627	160.289645	47.371367
2366.442085	164.630247	47.376372
2362.715987	168.437219	47.381377
2358.966932	154.383059	47.386381
2355.504391	164.135372	47.391386
2352.029810	158.810360	47.396391
2348.757130	151.972677	47.401396
2345.095712	165.436694	47.406401
2341.758697	156.259975	47.411405
2338.323676	158.048150	47.416410
2334.733217	157.507445	47.421415
2331.228321	158.208426	47.426420
2327.754008	159.956545	47.431425
2324.216616	150.064336	47.436429
2320.436745	157.663197	47.441434
2317.189167	163.141333	47.446439
2314.065813	150.850797	47.451444
2310.759441	156.028853	47.456449
2307.229526	145.368179	47.461453
2303.633676	155.679952	47.466458
2299.810667	153.760914	47.471463
2296.253625	147.267368	47.476468
2292.652073	155.821823	47.481473
2289.166394	151.289634	47.486477
2285.658623	149.513564	47.491482
2282.342810	155.442296	47.496487
2279.011742	153.314712	47.501492
2275.184528	154.042682	47.506497
2271.789951	150.432967	47.511501
2268.253943	157.199764	47.516506
2265.239617	145.900989	47.521511
2261.820217	151.832092	47.526516
2257.688356	158.369816	47.531521
2254.338765	160.108387	47.536525
2250.994463	159.220517	47.541530
2247.332041	158.705226	47.546535
2244.105760	151.632023	47.551540
2240.090754	158.518440	47.556545
2236.724213	147.280595	47.561549
2233.415575	160.353149	47.566554
2229.576402	165.460075	47.571559
2226.599905	154.071192	47.576564
2222.771327	158.619285	47.581569
2219.554317	157.348045	47.586573
2215.908441	153.965302	47.591578
2212.426332	155.297439	47.596583
2209.252907	152.696042	47.601588
2205.355705	155.687874	47.606593
2201.553773	152.460054	47.611597
2198.406545	155.357456	47.616602
2194.908126	154.695261	47.621607
2191.480832	153.644769	47.626612
2187.904932	153.397390	47.631617
2184.506917	145.730683	47.636621
2181.135434	151.390465	47.641626
2177.473259	159.174784	47.646631
2174.110067	152.506956	47.651636
2170.364526	160.108741	47.656641
2166.964829	151.556875	47.661645
2163.801287	152.456998	47.666650
2159.731615	150.752413	47.671655
2156.418875	149.522933	47.676660
2152.455061	156.596705	47.681665
2149.322573	152.402776	47.686669
2145.809754	158.351813	47.691674
2142.277458	155.847415	47.696679
2139.479006	149.380685	47.701684
2135.830036	157.434975	47.706689
2132.011194	146.427660	47.711693
2128.461328	158.214341	47.716698
2124.926348	160.600405	47.721703
2121.324231	150.828041	47.726708
2117.773924	157.895302	47.731713
2114.482105	152.749403	47.736717
2110.792273	152.109125	47.741722
2107.360347	153.321539	47.746727
2104.105083	150.783710	47.751732
2100.645862	152.332178	47.756737
2097.098689	145.878227	47.761741
2093.369210	152.931973	47.766746
2089.735703	148.667573	47.771751
2086.754721	142.656584	47.776756
2083.161055	145.223494	47.781761
2079.434458	146.799700	47.786765
2076.015898	143.103748	47.791770
2072.234124	151.306977	47.796775
2069.367383	142.729460	47.801780
2065.454522	152.777407	47.806785
2061.988308	152.848620	47.811789
2058.348473	140.589032	47.816794
2054.695934	138.396891	47.821799
2051.779265	150.284927	47.826804
2047.926084	139.658333	47.831809
2044.338773	148.261530	47.836813
2040.534675	140.077137	47.841818
2037.167978	149.947390	47.846823
2034.277453	137.624455	47.851828
2030.472531	146.532489	47.856833
2027.356149	143.906986	47.861837
2023.823491	144.876662	47.866842
2019.918373	146.126309	47.871847
2016.125637	144.450181	47.876852
2012.668473	144.368580	47.881857
2009.492268	142.447628	47.886861
2006.013238	142.613365	47.891866
2002.509241	147.575355	47.896871
1998.967859	140.104258	47.901876
1995.553258	147.844142	47.906881
1991.674414	137.286194	47.911885
1988.532426	140.767585	47.916890
1984.839558	146.937996	47.921895
1981.381221	131.858873	47.926900
1978.259193	139.278752	47.931905
1974.750748	147.845649	47.936909
1971.319649	143.673523	47.941914
1967.611297	143.406843	47.946919
1963.931031	138.141726	47.951924
1960.400531	147.908539	47.956929
1956.668479	144.543278	47.961933
1953.719308	146.369260	47.966938
1949.988625	147.444039	47.971943
1946.330779	137.232940	47.976948
1942.911802	144.892286	47.981953
1939.257615	145.357061	47.986957
1935.825638	136.552453	47.991962
1932.288783	151.064300	47.996967
1928.884432	142.355758	48.001972
1925.778739	145.870057	48.006977
1921.966509	141.273715	48.011981
1918.595850	146.542042	48.016986
1915.250361	144.623762	48.021991
1911.685118	149.567164	48.026996
1907.952751	148.286856	48.032001
1904.466863	139.811683	48.037005
1900.942045	141.639168	48.042010
1897.352319	133.960296	48.047015
1894.018053	132.483589	48.052020
1890.102006	147.174929	48.057025
1886.517227	141.595885	48.062029
1883.542934	133.970928	48.067034
1879.726031	146.483637	48.072039
1876.301797	136.952788	48.077044
1872.849563	144.665651	48.082049
1869.609385	143.329462	48.087053
1866.072809	141.130313	48.092058
1862.559643	145.344847	48.097063
1859.013536	137.134854	48.102068
1855.115916	147.258989	48.107073
1851.892479	147.077021	48.112077
1848.650245	146.835615	48.117082
1844.720595	139.880123	48.122087
1841.270530	135.404006	48.127092
1837.941986	137.727874	48.132097
1834.525930	133.601923	48.137101
1830.878152	135.939633	48.142106
1827.587444	141.775340	48.147111
1824.021279	132.148088	48.152116
1820.357946	142.135934	48.157121
1816.986315	143.418318	48.162125
1813.075774	139.038477	48.167130
1809.614820	146.944644	48.172135
1806.550140	138.282732	48.177140
1803.000913	143.909308	48.182145
1799.426315	142.404038	48.187149
1796.074079	139.347363	48.192154
1792.463612	146.111873	48.197159
1788.947683	131.951815	48.202164
1785.036968	136.610992	48.207169
1781.459337	137.027501	48.212173
1778.594443	134.498055	48.217178
1774.615136	143.001463	48.222183
1771.773724	135.767594	48.227188
1768.155639	138.530037	48.232193
1764.306398	139.400461	48.237197
1760.964833	132.849604	48.242202
1756.985400	136.379794	48.247207
1754.002803	141.593395	48.252212
1750.187961	143.986101	48.257217
1746.824485	135.561436	48.262221
1743.473113	134.537812	48.267226
1739.577044	154.047863	48.272231
1736.340239	132.657582	48.277236
1732.681758	138.561426	48.282241
1729.361465	134.550331	48.287245
1726.062693	137.937332	48.292250
1722.175252	136.025975	48.297255
1718.980370	124.802606	48.302260
1715.608417	141.508273	48.307265
1711.925697	129.740222	48.312269
1708.336106	136.263153	48.317274
1704.553222	142.397807	48.322279
1701.519823	132.358530	48.327284
1697.761214	137.644766	48.332289
1694.167871	142.052699	48.337293
1690.855766	137.020054	48.342298
1687.300286	134.411966	48.347303
1683.892152	130.641225	48.352308
1680.340273	130.079704	48.357313
1676.797532	143.589845	48.362317
1673.206942	131.273161	48.367322
1669.797122	143.778541	48.372327
1666.508555	131.003311	48.377332
1662.782616	132.946826	48.382337
1659.135610	132.049837	48.387341
1655.839868	128.183528	48.392346
1652.320127	147.427006	48.397351
1649.055127	138.356406	48.402356
1645.296081	138.977753	48.407361
1641.861910	129.869695	48.412365
1638.148899	130.563732	48.417370
1634.537459	136.170566	48.422375
1631.037972	129.622723	48.427380
1627.588439	146.981668	48.432385
1624.417925	138.518414	48.437389
1621.135198	134.181896	48.442394
1617.276118	133.967563	48.447399
1613.800898	123.916172	48.452404
1610.172448	137.133315	48.457409
1606.696807	129.941978	48.462413
1602.964529	133.723591	48.467418
1599.715874	133.027606	48.472423
1596.693297	127.264068	48.477428
1592.951701	127.909802	48.482433
1589.148914	136.621697	48.487437
1585.468986	124.037535	48.492442
1582.095112	142.245724	48.497447
1578.646734	127.356780	48.502452
1574.831790	125.494724	48.507457
1571.918769	127.712414	48.512461
1568.556192	128.781957	48.517466
1564.782553	130.885023	48.522471
1561.627006	124.818550	48.527476
1557.698938	128.016586	48.532481
1553.904352	127.840362	48.537485
1550.710486	127.597492	48.542490
1547.023557	134.786322	48.547495
1543.824382	120.900989	48.552500
1540.124093	122.244014	48.557505
1536.844713	121.722688	48.562509
1533.470353	120.209718	48.567514
1529.415715	121.137313	48.572519
1526.271392	119.222123	48.577524
1522.523754	120.721017	48.582529
1519.224398	120.144606	48.587533
1515.878283	124.863343	48.592538
1512.113731	125.376798	48.597543
1508.569190	123.114766	48.602548
1505.363943	123.050435	48.607553
1501.705631	121.261540	48.612557
1498.193880	115.857642	48.617562
1494.688281	115.489501	48.622567
1490.994061	118.587055	48.627572
1487.671171	115.242809	48.632577
1484.029567	124.199197	48.637581
1480.476953	114.875524	48.642586
1476.893948	129.721132	48.647591
1473.545473	120.201993	48.652596
1470.412527	113.316864	48.657601
1466.652300	121.922736	48.662605
1463.619894	113.459035	48.667610
1459.626634	121.240613	48.672615
1456.425976	123.594095	48.677620
1452.873062	121.913667	48.682625
1449.008851	127.921722	48.687629
1445.496080	120.549232	48.692634
1441.970954	123.708182	48.697639
1438.528046	124.370831	48.702644
1434.924437	122.589504	48.707649
1431.419226	122.535116	48.712653
1428.552287	117.130514	48.717658
1424.018881	119.101791	48.722663
1420.749655	125.038036	48.727668
1417.356633	120.122659	48.732673
1414.234623	128.179918	48.737677
1410.853980	118.057594	48.742682
1406.765746	133.143138	48.747687
1403.457424	119.746883	48.752692
1400.066018	125.356097	48.757697
1396.810027	126.386794	48.762701
1393.308811	126.157728	48.767706
1389.682853	132.088831	48.772711
1385.932363	121.817312	48.777716
1382.040842	125.590801	48.782721
1378.613981	135.230162	48.787725
1376.011128	123.158852	48.792730
1372.405153	135.073987	48.797735
1368.765897	124.290107	48.802740
1364.954185	122.784699	48.807745
1361.218535	128.396970	48.812749
1358.553556	114.192932	48.817754
1354.185913	139.922128	48.822759
1350.969627	127.040693	48.827764
1347.709372	127.516246	48.832769
1343.940922	123.583572	48.837773
1340.509049	112.309293	48.842778
1336.947987	125.570713	48.847783
1333.362416	126.749466	48.852788
1329.774107	121.566019	48.857793
1326.486516	120.196112	48.862797
1323.349667	119.500164	48.867802
1319.443749	130.574123	48.872807
1316.155495	116.738518	48.877812
1312.519149	121.144038	48.882817
1308.737665	132.050353	48.887821
1305.594376	116.566058	48.892826
1302.038267	125.062834	48.897831
1298.647997	121.641917	48.902836
1294.855122	123.786706	48.907841
1291.494111	128.609917	48.912845
1287.978918	111.414481	48.917850
1284.070870	127.929328	48.922855
1280.904373	117.944276	48.927860
1277.220618	115.957942	48.932865
1274.055760	120.726526	48.937869
1270.898144	113.802840	48.942874
1267.008235	119.566877	48.947879
1263.651420	113.195624	48.952884
1259.601229	116.182925	48.957889
1256.138520	113.636613	48.962893
1252.665781	113.762492	48.967898
1249.198077	123.011092	48.972903
1246.213739	112.126798	48.977908
1242.560270	118.979993	48.982913
1238.800691	114.382123	48.987917
1235.387037	115.725832	48.992922
1232.041269	114.509514	48.997927
1228.649704	118.527982	49.002932
1225.291908	114.820347	49.007937
1221.428210	120.896406	49.012941
1218.047399	112.062696	49.017946
1214.194098	118.946106	49.022951
1210.868329	126.707958	49.027956
1207.322601	119.280783	49.032961
1203.755803	113.571352	49.037965
1200.317408	110.567781	49.042970
1196.715574	114.821649	49.047975
1193.510309	121.393527	49.052980
1189.816719	117.030834	49.057985
1186.101673	112.411619	49.062989
1183.233811	109.473056	49.067994
1179.536227	117.112895	49.072999
1175.849156	109.101810	49.078004
1172.391790	117.011025	49.083009
1168.540597	118.098030	49.088013
1165.736350	105.779902	49.093018
1162.090315	124.853028	49.098023
1158.512059	113.928422	49.103028
1154.919990	109.975755	49.108033
1151.274648	109.606439	49.113037
1147.904919	105.620248	49.118042
1144.153443	109.946348	49.123047
1140.550334	106.363556	49.128052
1137.335642	110.428528	49.133057
1133.688202	116.518514	49.138061
1130.313473	107.915553	49.143066
1126.581989	110.965943	49.148071
1123.445982	103.243157	49.153076
1119.899446	103.788498	49.158081
1116.387860	106.936994	49.163085
1112.976048	109.778069	49.168090
1109.382425	113.276835	49.173095
1105.747667	104.558189	49.178100
1102.337761	111.088704	49.183105
1098.628450	107.068522	49.188109
1095.505297	104.165282	49.193114
1091.663335	113.163917	49.198119
1088.430304	107.227935	49.203124
1084.736401	111.720559	49.208129
1080.839945	106.338270	49.213133
1078.182616	115.610010	49.218138
1074.660479	110.207451	49.223143
1070.687566	104.990991	49.228148
1067.399801	108.653347	49.233153
1063.575474	104.468370	49.238157
1060.287242	105.022409	49.243162
1056.592244	108.047865	49.248167
1053.299726	105.811927	49.253172
1050.044849	110.423541	49.258177
1045.966653	115.345430	49.263181
1042.598737	101.371580	49.268186
1038.926646	112.342445	49.273191
1035.724245	110.299360	49.278196
1032.372426	103.076990	49.283201
1028.532664	110.900193	49.288205
1025.473520	113.294863	49.293210
1021.811123	116.864320	49.298215
1018.275483	109.531173	49.303220
1014.547574	116.687391	49.308225
1011.065483	116.788595	49.313229
1008.000569	110.073141	49.318234
1004.300469	112.207348	49.323239
1000.687961	114.177246	49.328244
997.075581	107.793204	49.333249
993.579466	111.516244	49.338253
990.065321	110.218954	49.343258
986.456361	116.009051	49.348263
983.213727	108.273101	49.353268
979.778532	110.688969	49.358273
976.306972	108.081039	49.363277
973.235537	109.273067	49.368282
969.031372	114.554563	49.373287
965.542271	114.596192	49.378292
961.874927	114.700162	49.383297
958.524284	110.076745	49.388301
955.421954	113.426625	49.393306
951.652590	112.184554	49.398311
948.148967	109.380099	49.403316
944.586713	111.538055	49.408321
940.806767	106.611167	49.413325
937.596498	99.285082	49.418330
934.235020	107.605402	49.423335
930.556428	104.709433	49.428340
927.753535	108.040027	49.433345
923.709318	115.537126	49.438349
920.576903	107.924429	49.443354
916.047103	111.292807	49.448359
912.736148	105.976323	49.453364
909.382338	99.544919	49.458369
906.052770	101.912535	49.463373
902.515801	98.517911	49.468378
899.083783	111.834016	49.473383
895.659792	103.939204	49.478388
892.346685	111.457067	49.483393
888.619753	108.331967	49.488397
885.217365	100.119427	49.493402
881.659772	104.051876	49.498407
878.246856	105.574949	49.503412
874.706077	103.186397	49.508417
871.211783	107.354818	49.513421
867.743998	102.119266	49.518426
863.964343	106.644872	49.523431
860.372566	102.358952	49.528436
856.949224	93.184371	49.533441
853.544464	102.336788	49.538445
850.454501	103.240131	49.543450
846.214271	103.264664	49.548455
842.754456	106.603915	49.553460
839.692629	101.111764	49.558465
836.091959	107.524975	49.563469
832.820484	105.179573	49.568474
828.847102	106.227798	49.573479
825.384747	109.925054	49.578484
822.093176	99.019527	49.583489
818.658024	103.740575	49.588493
815.136969	102.176223	49.593498
811.335825	103.436424	49.598503
807.690279	105.403103	49.603508
804.407204	103.469908	49.608513
801.103930	111.697003	49.613517
797.600840	107.033329	49.618522
793.842087	108.495092	49.623527
790.547613	105.616404	49.628532
787.378734	106.814690	49.633537
783.988566	101.843982	49.638541
780.233726	95.255302	49.643546
776.469934	106.521620	49.648551
773.106288	108.528953	49.653556
769.501593	95.365479	49.658561
765.682926	120.030169	49.663565
762.470668	99.255530	49.668570
758.824933	103.374597	49.673575
755.318184	107.467635	49.678580
752.348767	98.054801	49.683585
748.212252	101.726895	49.688589
744.890362	99.673114	49.693594
741.674710	111.087633	49.698599
737.850250	103.268933	49.703604
734.381311	105.401128	49.708609
731.069225	105.090944	49.713613
727.403473	98.357091	49.718618
723.830474	97.621565	49.723623
720.436541	97.504157	49.728628
716.903690	101.262543	49.733633
713.348957	102.042668	49.738637
710.234998	93.032553	49.743642
706.515525	100.209148	49.748647
702.785698	92.568561	49.753652
699.290606	100.590778	49.758657
695.582491	101.497222	49.763661
692.423943	97.033180	49.768666
688.723859	104.591966	49.773671
685.622676	102.547573	49.778676
682.029064	100.675319	49.783681
678.438241	92.444939	49.788685
675.213985	92.460029	49.793690
671.288716	97.875689	49.798695
667.691630	105.564998	49.803700
664.444374	92.636517	49.808705
660.892112	96.429156	49.813709
657.578713	102.473567	49.818714
653.697437	103.073140	49.823719
650.486994	97.763300	49.828724
646.740226	96.778460	49.833729
643.248277	99.981338	49.838733
640.091208	100.972360	49.843738
636.458906	104.011675	49.848743
632.985262	101.110389	49.853748
629.374975	99.709423	49.858753
625.756855	109.328822	49.863757
622.003749	105.613577	49.868762
618.644786	102.805544	49.873767
615.134513	103.537135	49.878772
611.943664	97.348118	49.883777
608.191988	113.234698	49.888781
604.769640	102.061808	49.893786
601.306990	112.152495	49.898791
598.159327	108.063434	49.903796
594.359830	105.514856	49.908801
590.444307	107.267275	49.913805
587.481429	103.924242	49.918810
584.260144	97.514752	49.923815
580.601571	99.508671	49.928820
576.830604	101.426341	49.933825
572.938901	105.663778	49.938829
569.351709	102.090546	49.943834
566.354262	108.572149	49.948839
562.737786	103.753881	49.953844
559.582581	105.747505	49.958849
555.678502	105.933211	49.963853
552.215769	113.470073	49.968858
548.555038	102.939481	49.973863
545.044242	109.182132	49.978868
542.207207	101.698525	49.983873
538.540429	104.657422	49.988877
534.691070	100.668175	49.993882
530.997550	98.572703	49.998887
527.731389	110.975522	50.003892
524.260677	103.096533	50.008897
520.517059	110.770643	50.013901
517.097102	100.052892	50.018906
513.870770	102.959779	50.023911
510.139883	106.742163	50.028916
506.740523	95.560430	50.033921
502.898505	103.628195	50.038925
499.632505	98.652923	50.043930
496.010952	108.131713	50.048935
492.850391	111.278900	50.053940
489.803125	99.003895	50.058945
485.650747	105.128586	50.063949
482.485817	104.454177	50.068954
478.833319	101.952346	50.073959
474.988821	112.956860	50.078964
471.857113	96.992953	50.083969
467.956173	104.879125	50.088973
464.723333	89.736554	50.093978
461.220938	105.848836	50.098983
457.455932	107.972043	50.103988
454.323122	101.047543	50.108993
450.349407	109.319962	50.113997
447.460776	94.797676	50.119002
443.637706	105.298417	50.124007
439.983821	106.468027	50.129012
436.912882	97.861270	50.134017
433.153952	106.953072	50.139021
429.724903	101.918514	50.144026
426.001023	95.763344	50.149031
422.394623	100.156398	50.154036
419.534773	92.526913	50.159041
415.562275	98.412822	50.164045
412.207040	94.929684	50.169050
408.494535	95.327428	50.174055
404.981633	98.036326	50.179060
401.577646	92.379197	50.184065
397.772466	102.767092	50.189069
394.704621	98.142026	50.194074
391.536189	104.991172	50.199079
387.703549	107.545408	50.204084
384.199137	99.954740	50.209089
380.220152	106.504603	50.214093
377.120076	104.296106	50.219098
373.576402	101.468269	50.224103
369.992328	96.106693	50.229108
366.581229	93.637298	50.234113
363.215685	101.303998	50.239117
360.069266	99.044804	50.244122
356.331666	101.248805	50.249127
352.294278	95.652936	50.254132
349.073380	97.731842	50.259137
345.332200	100.921925	50.264141
342.251162	101.549510	50.269146
338.556167	97.872270	50.274151
334.649973	101.983098	50.279156
331.734368	103.770557	50.284161
328.194790	102.559220	50.289165
324.736669	93.078970	50.294170
321.345704	99.068856	50.299175
317.630299	103.162806	50.304180
313.979239	97.401175	50.309185
310.452011	106.831697	50.314189
306.921624	102.442202	50.319194
303.389194	95.179109	50.324199
300.164857	104.343636	50.329204
296.589854	88.049031	50.334209
292.676530	107.453522	50.339213
289.686924	94.157016	50.344218
286.073046	105.426485	50.349223
282.121593	105.545558	50.354228
279.011508	98.163383	50.359233
275.427069	100.998936	50.364237
272.080195	94.129508	50.369242
268.524125	91.308374	50.374247
265.086164	94.541890	50.379252
261.703061	86.892128	50.384257
257.738006	93.922665	50.389261
254.576412	96.968788	50.394266
251.068265	97.737068	50.399271
247.288095	97.684852	50.404276
244.255503	102.590715	50.409281
240.395845	97.666565	50.414285
237.130095	101.974383	50.419290
233.845379	98.652952	50.424295
229.826461	104.800926	50.429300
226.397537	94.403265	50.434305
222.833954	104.092881	50.439309
219.413781	101.276051	50.444314
216.171520	115.375147	50.449319
212.194382	97.225432	50.454324
208.697672	99.734883	50.459329
205.109770	102.542465	50.464333
202.109311	100.828656	50.469338
198.493445	107.686786	50.474343
194.984035	99.488571	50.479348
192.002726	96.209511	50.484353
187.969249	98.254853	50.489357
184.595491	92.840762	50.494362
180.903054	100.057353	50.499367
177.087697	97.010232	50.504372
173.846287	88.659178	50.509377
170.275505	93.176784	50.514381
166.624899	89.275679	50.519386
163.059479	95.169775	50.524391
159.767040	99.645088	50.529396
156.580628	90.622665	50.534401
152.929221	94.773822	50.539405
149.343170	93.364368	50.544410
146.336087	96.466994	50.549415
142.448392	101.911075	50.554420
139.069722	87.730008	50.559425
135.258903	88.502716	50.564429
131.742466	90.538565	50.569434
128.187208	90.775483	50.574439
124.911564	88.406549	50.579444
121.587785	87.471535	50.584449
117.819290	96.624013	50.589453
114.220519	98.033813	50.594458
110.904660	92.448558	50.599463
107.362634	95.669318	50.604468
104.018956	98.881588	50.609473
100.185976	94.797739	50.614477
97.106386	94.994710	50.619482
93.287348	93.032431	50.624487
89.814367	96.372366	50.629492
86.455671	96.022748	50.634497
82.977486	105.223513	50.639501
79.604875	89.413910	50.644506
75.748781	95.627922	50.649511
71.746088	87.330869	50.654516
68.352158	87.230039	50.659521
65.083618	102.372354	50.664525
62.045509	94.682225	50.669530
58.372280	94.406219	50.674535
55.025815	99.473713	50.679540
51.500957	92.510357	50.684545
47.629245	101.952771	50.689549
44.320192	98.577546	50.694554
40.521436	99.637635	50.699559
37.092766	99.136499	50.704564
33.759404	93.292960	50.709569
30.526047	98.943143	50.714573
26.953154	98.774811	50.719578
23.351852	93.851177	50.724583
19.397617	98.661166	50.729588
16.627650	88.725481	50.734593
12.728515	98.127689	50.739597
9.313502	96.953186	50.744602
5.982293	91.235215	50.749607
2.237391	103.351154	50.754612