Fri Jun 17 17:35:59 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
-0.191230	88.235380	0.000000
0.166182	86.901943	0.005005
0.288353	101.002785	0.010010
0.535600	86.830947	0.015014
0.051609	83.542304	0.020019
-0.299925	79.116331	0.025024
-0.294993	70.660812	0.030029
-0.734540	66.128508	0.035034
-0.759446	57.544955	0.040038
-0.652665	56.648039	0.045043
-1.253751	36.662018	0.050048
-1.244062	32.812998	0.055053
-1.840423	30.573504	0.060058
-2.274587	27.149906	0.065062
-2.398055	28.699875	0.070067
-2.940552	13.818354	0.075072
-3.198116	1.755308	0.080077
-3.376239	11.723971	0.085082
-3.297672	1.851458	0.090086
-3.735034	8.068555	0.095091
-4.603468	1.743780	0.100096
-4.653703	-12.201909	0.105101
-4.990577	-4.663821	0.110106
-4.810160	-2.835615	0.115110
-5.083666	-6.701882	0.120115
-5.272061	4.466276	0.125120
-5.190867	-6.513887	0.130125
-6.017381	-1.634333	0.135130
-6.182550	-2.028237	0.140134
-6.212708	-4.567852	0.145139
-7.352949	-1.322531	0.150144
-7.701652	-6.502551	0.155149
-7.348147	-0.344495	0.160154
-7.415675	-6.285784	0.165158
-7.740355	-2.528982	0.170163
-8.258314	-6.034940	0.175168
-7.910276	-13.624138	0.180173
-8.423616	-1.139654	0.185178
-8.665864	3.193267	0.190182
-9.561144	3.102069	0.195187
-9.839132	-7.051565	0.200192
-9.800449	-4.069101	0.205197
-9.936761	-4.759849	0.210202
-9.873579	3.245916	0.215206
-9.855934	-5.315272	0.220211
-10.183699	0.567483	0.225216
-10.559312	-7.889066	0.230221
-11.141389	-2.028369	0.235226
-11.360097	-3.664642	0.240230
-11.422284	-7.479406	0.245235
-11.744554	-2.255067	0.250240
-11.850471	-11.963116	0.255245
-12.344824	4.654642	0.260250
-13.087713	1.966116	0.265254
-13.160618	-7.317441	0.270259
-13.177349	2.684772	0.275264
-12.944569	-1.409110	0.280269
-13.079114	-5.093646	0.285274
-13.439869	-7.957970	0.290278
-14.253107	4.324970	0.295283
-14.309986	-7.849567	0.300288
-14.137325	-3.542400	0.305293
-14.541214	-4.900835	0.310298
-15.100774	-2.487877	0.315302
-15.440773	-3.591720	0.320307
-16.060925	1.559988	0.325312
-15.718966	2.517756	0.330317
-15.898745	-4.139533	0.335322
-15.989523	-13.475762	0.340326
-16.160983	0.146134	0.345331
-16.985717	6.242329	0.350336
-16.793846	-6.749459	0.355341
-16.922942	-12.619733	0.360346
-17.274509	-2.894762	0.365350
-18.213356	-6.182168	0.370355
-18.986676	2.479253	0.375360
-18.671145	-7.610042	0.380365
-18.915591	4.227105	0.385370
-19.100035	-0.783285	0.390374
-18.989509	-0.987799	0.395379
-19.214012	0.425835	0.400384
-19.260402	2.691334	0.405389
-19.593589	-5.848436	0.410394
-19.695845	3.804708	0.415398
-20.001639	-13.356413	0.420403
-20.349722	-2.835204	0.425408
-20.188526	-4.152003	0.430413
-21.300607	2.861588	0.435418
-21.854579	-2.840584	0.440422
-21.909218	1.708406	0.445427
-22.230756	8.408259	0.450432
-21.984193	-5.412526	0.455437
-22.153404	4.810389	0.460442
-22.134482	-2.175135	0.465446
-22.491977	-2.926796	0.470451
-23.226110	4.491249	0.475456
-23.411163	6.794401	0.480461
-24.291294	7.175070	0.485466
-23.758981	-3.850876	0.490470
-23.493306	1.891007	0.495475
-23.972067	3.874566	0.500480
-24.523314	3.316133	0.505485
-25.256093	9.652587	0.510490
-25.174210	1.126303	0.515494
-25.241186	7.768054	0.520499
-25.528586	0.104117	0.525504
-25.299858	-3.622255	0.530509
-25.979680	12.186702	0.535514
-26.689572	4.286538	0.540518
-26.934117	-4.459376	0.545523
-27.296151	-3.745503	0.550528
-26.880060	-3.411978	0.555533
-26.985000	-8.840501	0.560538
-26.923696	-13.321452	0.565542
-27.794141	-0.136088	0.570547
-28.408222	1.952251	0.575552
-27.946604	-4.131064	0.580557
-28.570334	5.553906	0.585562
-28.962171	2.269503	0.590566
-29.204023	-8.955911	0.595571
-29.930767	8.060409	0.600576
-29.700779	-8.437160	0.605581
-30.416973	-0.698873	0.610586
-29.844045	-2.103255	0.615590
-30.272551	4.526172	0.620595
-30.402835	1.110480	0.625600
-29.997825	0.663039	0.630605
-31.138862	-7.408165	0.635610
-31.546424	-2.818863	0.640614
-31.209701	-3.870819	0.645619
-31.508174	-1.446006	0.650624
-32.087872	-4.188095	0.655629
-32.832486	-12.429580	0.660634
-32.797904	0.270476	0.665638
-32.955525	-4.817382	0.670643
-33.161675	-2.135008	0.675648
-32.608945	0.874288	0.680653
-33.339756	2.049056	0.685658
-34.171193	-6.152149	0.690662
-34.673327	1.923116	0.695667
-34.866433	-3.343347	0.700672
-34.501375	-9.988982	0.705677
-34.864070	-3.140215	0.710682
-34.775099	-4.537754	0.715686
-34.790903	-5.834603	0.720691
-35.459876	7.001352	0.725696
-35.795110	-3.495194	0.730701
-35.967209	-4.516638	0.735706
-36.264027	4.989081	0.740710
-36.611354	-12.718248	0.745715
-37.534388	-8.835145	0.750720
-37.436872	-14.562727	0.755725
-37.524779	-3.651629	0.760730
-37.859219	-11.194670	0.765734
-37.637523	-10.037146	0.770739
-37.695984	-0.327942	0.775744
-37.958346	-5.037077	0.780749
-38.607121	-4.591660	0.785754
-38.899120	1.132615	0.790758
-38.915027	-8.626505	0.795763
-39.175987	3.376378	0.800768
-39.308455	-10.764411	0.805773
-40.272250	5.742735	0.810778
-40.827172	0.619295	0.815782
-40.636865	-5.892906	0.820787
-40.931921	-0.958824	0.825792
-40.956928	-11.292040	0.830797
-41.165127	-6.128301	0.835802
-41.087509	-1.500265	0.840806
-41.030128	4.102590	0.845811
-41.751233	-12.565229	0.850816
-42.391091	-13.158459	0.855821
-42.383832	3.270342	0.860826
-42.429653	-3.616409	0.865830
-42.409815	2.690445	0.870835
-42.741760	13.726381	0.875840
-43.470068	-4.785087	0.880845
-43.746660	6.015700	0.885850
-44.159401	-3.845188	0.890854
-43.833529	-1.900665	0.895859
-44.234270	-6.961919	0.900864
-44.766155	-0.048519	0.905869
-45.528877	9.976866	0.910874
-45.793415	-5.779811	0.915878
-45.315335	-6.234862	0.920883
-45.885655	-0.131623	0.925888
-45.858842	-5.989137	0.930893
-46.008040	-1.476329	0.935898
-45.945022	-1.543300	0.940902
-46.016290	-13.920462	0.945907
-46.867733	-9.587309	0.950912
-47.007425	-7.346557	0.955917
-47.517915	-3.469277	0.960922
-47.724384	-11.447587	0.965926
-47.589822	-8.518161	0.970931
-48.138149	-10.829955	0.975936
-48.577625	-10.488986	0.980941
-48.809886	3.057770	0.985946
-49.108460	-1.976662	0.990950
-48.922374	-13.597616	0.995955
-49.310259	3.057101	1.000960
-49.520544	-7.434558	1.005965
-50.173800	-0.770140	1.010970
-50.751878	-4.592086	1.015974
-50.629659	-4.988771	1.020979
-50.992625	1.365733	1.025984
-50.672710	-21.200056	1.030989
-50.636290	-6.503932	1.035994
-51.160070	-8.966224	1.040998
-51.234882	-13.736131	1.046003
-52.149462	-0.199680	1.051008
-52.227400	-4.061551	1.056013
-52.208120	4.365309	1.061018
-51.992496	2.884951	1.066022
-52.880072	-10.443604	1.071027
-53.492979	-5.844636	1.076032
-53.666207	-8.959558	1.081037
-54.048509	-6.173706	1.086042
-54.113048	-7.994257	1.091046
-53.570560	-4.893676	1.096051
-54.136659	-3.866656	1.101056
-54.751364	-3.559111	1.106061
-55.152347	2.637930	1.111066
-55.503196	-10.309018	1.116070
-55.486416	-6.712378	1.121075
-55.890655	-3.876703	1.126080
-55.733650	-1.449265	1.131085
-55.956709	-7.255375	1.136090
-56.456898	-1.710397	1.141094
-56.974854	-8.181620	1.146099
-57.378314	-3.649041	1.151104
-57.308058	-8.943689	1.156109
-57.109835	-4.176657	1.161114
-57.453319	3.002013	1.166118
-57.525990	-9.476937	1.171123
-58.259168	4.385148	1.176128
-58.690310	-1.797015	1.181133
-59.186784	-2.826102	1.186138
-59.123697	-3.961428	1.191142
-59.026924	-9.219835	1.196147
-59.280887	-10.645612	1.201152
-59.316347	-10.241961	1.206157
-59.438229	-5.607009	1.211162
-60.415490	-8.101657	1.216166
-60.547280	-9.198273	1.221171
-60.670082	-0.614403	1.226176
-60.570270	-12.711576	1.231181
-60.784598	-10.034356	1.236186
-61.418287	-0.395288	1.241190
-61.917887	-3.697488	1.246195
-62.693197	-5.760601	1.251200
-62.274819	-10.941443	1.256205
-62.420761	-7.828244	1.261210
-62.475922	-5.661334	1.266214
-62.323182	-8.269830	1.271219
-63.211418	2.466282	1.276224
-63.643638	-11.638683	1.281229
-63.821604	-11.706640	1.286234
-64.080981	-3.641145	1.291238
-63.702757	-9.266013	1.296243
-64.238627	-2.284464	1.301248
-64.118002	2.273276	1.306253
-64.896289	-2.285761	1.311258
-64.729697	4.754048	1.316262
-64.985642	-2.910770	1.321267
-66.233767	4.504519	1.326272
-66.302976	-0.764777	1.331277
-66.520598	-3.297893	1.336282
-66.730168	-0.478003	1.341286
-66.449083	-0.635492	1.346291
-66.693603	6.308284	1.351296
-66.852755	-3.749264	1.356301
-67.438259	-1.976267	1.361306
-68.325669	11.059000	1.366310
-68.430109	-14.871765	1.371315
-68.345689	1.770342	1.376320
-68.499047	-6.531734	1.381325
-68.322471	0.055119	1.386330
-68.404734	6.587129	1.391334
-68.694481	-4.109763	1.396339
-69.302682	-2.724101	1.401344
-69.836195	-9.180895	1.406349
-69.779432	-3.613066	1.411354
-70.088476	-6.769739	1.416358
-70.942875	-2.240929	1.421363
-71.129730	-9.572492	1.426368
-71.378306	-9.238984	1.431373
-71.207969	-5.649322	1.436378
-71.506961	-8.712750	1.441382
-71.412877	-8.949854	1.446387
-71.641081	5.836839	1.451392
-71.629213	-4.508824	1.456397
-72.598522	5.950300	1.461402
-72.671433	-0.088756	1.466406
-72.973894	-5.552519	1.471411
-73.342194	2.572723	1.476416
-73.593323	-2.474526	1.481421
-73.642677	-0.801905	1.486426
-73.705861	0.760932	1.491430
-74.449712	2.815401	1.496435
-74.759274	0.777475	1.501440
-74.521219	-1.863162	1.506445
-74.718869	6.529116	1.511450
-75.077319	2.288631	1.516454
-75.111104	-8.776204	1.521459
-75.864675	0.675204	1.526464
-76.166499	-10.212268	1.531469
-76.391088	-7.594711	1.536474
-76.303053	-6.330118	1.541478
-76.546369	-3.102065	1.546483
-76.741950	-3.268126	1.551488
-77.612666	-6.834418	1.556493
-77.834362	-1.896744	1.561498
-78.054596	-3.001350	1.566502
-77.891680	-4.774466	1.571507
-78.209130	-7.298877	1.576512
-78.053911	3.230029	1.581517
-78.159651	-1.573612	1.586522
-78.932041	7.690703	1.591526
-79.166569	-7.496723	1.596531
-79.660745	6.274919	1.601536
-79.895033	-10.871239	1.606541
-80.025976	-3.973975	1.611546
-79.784998	-2.756316	1.616550
-80.429488	0.379775	1.621555
-81.088073	6.045413	1.626560
-81.131421	1.173779	1.631565
-81.553472	-0.502092	1.636570
-81.668173	-1.298845	1.641574
-81.542173	-5.223031	1.646579
-81.450239	0.980470	1.651584
-81.967624	-10.386196	1.656589
-82.799948	0.358578	1.661594
-82.824351	4.440394	1.666598
-82.875895	-3.968590	1.671603
-83.003082	1.708555	1.676608
-83.365342	-8.539191	1.681613
-84.119047	-13.188342	1.686618
-84.579458	0.826120	1.691622
-84.543940	-4.506561	1.696627
-84.752243	1.214457	1.701632
-84.893234	-1.868331	1.706637
-84.687730	-2.438896	1.711642
-85.190237	-0.272603	1.716646
-84.769550	-2.015955	1.721651
-85.672134	10.535418	1.726656
-86.076864	4.331304	1.731661
-86.432722	-9.541663	1.736666
-86.624090	-2.988560	1.741670
-86.528799	-2.514097	1.746675
-86.728812	1.819302	1.751680
-87.104818	-0.034124	1.756685
-87.514387	-2.728119	1.761690
-88.027445	-4.666699	1.766694
-87.866335	-5.312762	1.771699
-88.129328	-2.243446	1.776704
-88.410700	-3.556923	1.781709
-88.942893	-2.665772	1.786714
-89.823374	-2.828871	1.791718
-89.246308	-3.790549	1.796723
-89.751742	-7.060990	1.801728
-89.347896	-10.429116	1.806733
-89.685815	-3.606172	1.811738
-89.740314	-5.618419	1.816742
-90.305761	-1.245976	1.821747
-90.550885	-0.035318	1.826752
-90.691158	-2.283520	1.831757
-91.199415	-4.142387	1.836762
-91.343286	-0.619085	1.841766
-91.821853	3.277362	1.846771
-92.399240	0.224500	1.851776
-92.468685	-1.798879	1.856781
-92.660339	-2.460099	1.861786
-92.940919	-3.367406	1.866790
-92.787199	-4.310801	1.871795
-92.949592	2.387852	1.876800
-93.499595	-9.922545	1.881805
-93.870580	-4.998927	1.886810
-94.214257	-7.307439	1.891814
-94.297940	-3.073891	1.896819
-94.621610	1.001436	1.901824
-94.302204	-3.680880	1.906829
-94.726443	-9.330799	1.911834
-95.319230	-2.118184	1.916838
-95.205064	-4.084078	1.921843
-95.653289	-4.021660	1.926848
-95.861814	-9.748879	1.931853
-96.453841	4.294570	1.936858
-97.313969	-4.309134	1.941862
-97.136322	-7.050431	1.946867
-97.449598	2.345741	1.951872
-97.506043	-4.053611	1.956877
-97.464072	7.317184	1.961882
-97.499907	5.110029	1.966886
-97.399952	0.423150	1.971891
-97.865027	0.816134	1.976896
-98.329957	-6.986399	1.981901
-98.767710	0.517157	1.986906
-99.081229	-1.520700	1.991910
-99.302877	-1.079386	1.996915
-99.149833	-3.623320	2.006912
-99.144310	-3.737376	2.016909
-99.237174	0.484469	2.026906
-98.301253	-3.838256	2.036902
-97.629703	-1.218641	2.046899
-97.512132	-4.641069	2.056896
-96.939633	-7.220370	2.066893
-96.358454	-8.248907	2.076890
-95.154714	-12.559248	2.086886
-95.318273	-8.262032	2.096883
-94.824024	-6.331944	2.106880
-94.540956	-5.857111	2.116877
-93.498694	-10.548417	2.126874
-93.140911	-14.960160	2.136870
-92.957933	-7.886039	2.146867
-91.885421	-12.707048	2.156864
-91.751980	-6.939601	2.166861
-91.592037	-5.860048	2.176858
-90.569111	-4.871602	2.186854
-90.469083	-8.866275	2.196851
-89.735501	-11.042414	2.206848
-88.939048	-2.711899	2.216845
-88.880720	-8.065526	2.226842
-88.245594	-11.230200	2.236838
-87.198260	-8.211504	2.246835
-87.174189	-2.877744	2.256832
-87.102358	-2.809785	2.266829
-86.317494	-7.574479	2.276826
-85.884670	-1.366400	2.286822
-84.900193	-3.417291	2.296819
-84.251583	-7.179523	2.306816
-84.039297	0.236290	2.316813
-84.049066	-3.867967	2.326810
-83.549670	-10.646777	2.336806
-82.906766	1.594329	2.346803
-82.153490	0.304629	2.356800
-81.530732	-4.213404	2.366797
-81.156585	-2.386046	2.376794
-81.109646	-6.136179	2.386790
-80.003297	-5.233913	2.396787
-79.555121	-5.644824	2.406784
-79.230600	2.679784	2.416781
-78.391912	1.736079	2.426778
-77.929669	0.148399	2.436774
-77.829200	4.763896	2.446771
-77.309753	1.504644	2.456768
-76.678412	1.584506	2.466765
-76.419998	-4.636776	2.476762
-75.345029	-6.309321	2.486758
-75.023131	-1.986110	2.496755
-74.929666	-1.456046	2.506752
-74.511115	-5.850231	2.516749
-73.659160	-8.966582	2.526746
-73.112057	-4.578264	2.536742
-72.267266	-8.014495	2.546739
-72.058354	-0.255314	2.556736
-71.987891	-1.938893	2.566733
-71.445305	-7.955694	2.576730
-70.462890	-3.879804	2.586726
-70.337594	-4.598812	2.596723
-69.587121	-3.475958	2.606720
-68.902728	-3.844732	2.616717
-68.742855	-12.852730	2.626714
-68.232368	-7.607339	2.636710
-67.342502	0.909388	2.646707
-67.007985	-0.442680	2.656704
-66.789781	0.597157	2.666701
-66.343244	-8.142564	2.676698
-65.709557	-8.040368	2.686694
-65.673295	-3.598543	2.696691
-64.756637	1.414547	2.706688
-63.901390	-2.140390	2.716685
-63.159128	-3.870444	2.726682
-62.808933	-2.760475	2.736678
-62.590586	-6.403956	2.746675
-62.739009	-4.953650	2.756672
-61.781276	-1.752499	2.766669
-60.849527	-14.778416	2.776666
-60.772414	-7.676419	2.786662
-60.021809	-10.522815	2.796659
-59.639913	-4.384707	2.806656
-59.303201	-2.966837	2.816653
-58.707726	-2.451465	2.826650
-57.724601	-7.328540	2.836646
-57.632025	-6.075967	2.846643
-57.324777	-2.833860	2.856640
-56.633184	-9.243130	2.866637
-56.095302	-11.891751	2.876634
-55.541320	-2.501790	2.886630
-54.712908	-6.232853	2.896627
-54.508919	-4.405066	2.906624
-54.650775	-2.369426	2.916621
-54.106287	-7.029349	2.926618
-53.012764	-8.794675	2.936614
-51.895314	-10.369952	2.946611
-52.125261	-9.094587	2.956608
-51.622796	-6.957409	2.966605
-51.611074	-8.154061	2.976602
-50.283973	-7.454056	2.986598
-49.995209	-13.258739	2.996595
-50.046067	-5.607724	3.006592
-48.943595	-11.624335	3.016589
-47.912231	-10.563778	3.026586
-48.269851	-3.455305	3.036582
-48.060356	-7.401196	3.046579
-46.970152	-4.398504	3.056576
-46.583963	-4.719877	3.066573
-46.212146	-12.028137	3.076570
-45.291915	-5.556096	3.086566
-45.138926	-9.536062	3.096563
-44.958408	-5.046691	3.106560
-43.798464	-2.530777	3.116557
-43.448645	-1.748137	3.126554
-43.406287	-1.100116	3.136550
-42.345061	-1.767637	3.146547
-42.023030	-1.384830	3.156544
-41.956400	-0.758230	3.166541
-41.414180	-0.642011	3.176538
-40.576118	-4.188357	3.186534
-39.538274	-3.919402	3.196531
-39.438247	2.040126	3.206528
-38.957158	-4.289103	3.216525
-38.806885	-2.546434	3.226522
-38.104097	-7.585551	3.236518
-37.636182	-4.176717	3.246515
-37.468557	-5.389801	3.256512
-36.239461	-4.973430	3.266509
-36.005632	-1.018883	3.276506
-35.683848	-4.080884	3.286502
-34.898869	-3.545045	3.296499
-34.440855	-7.175216	3.306496
-34.279869	-0.882621	3.316493
-33.940916	-6.298706	3.326490
-32.938402	-5.176643	3.336486
-32.616710	-2.975230	3.346483
-31.520225	-4.223969	3.356480
-31.449636	-12.465524	3.366477
-31.256239	-5.733561	3.376474
-30.775931	-9.885892	3.386470
-29.582639	-6.607119	3.396467
-29.428586	-7.701768	3.406464
-29.432042	-1.561441	3.416461
-28.549226	-1.547675	3.426458
-28.217848	-3.461537	3.436454
-27.525007	-8.386180	3.446451
-26.736313	-8.627851	3.456448
-26.251737	-6.121970	3.466445
-26.457178	-4.951249	3.476442
-25.932734	0.118948	3.486438
-24.832494	-4.835480	3.496435
-24.411531	-9.181851	3.506432
-23.999676	1.871285	3.516429
-23.152244	-0.399443	3.526426
-22.725797	-4.098459	3.536422
-22.819754	-3.716841	3.546419
-22.443995	0.020879	3.556416
-21.563686	-2.824350	3.566413
-21.140781	-1.471977	3.576410
-20.061086	-4.976685	3.586406
-19.651060	-6.798901	3.596403
-19.752726	2.703219	3.606400
-19.554176	-5.704834	3.616397
-18.468130	-8.907505	3.626394
-18.123763	-3.621054	3.636390
-17.188298	-5.934271	3.646387
-16.829981	-4.837700	3.656384
-16.416489	-9.982445	3.666381
-16.327134	-6.371979	3.676378
-15.769973	-15.022598	3.686374
-15.340911	-12.427468	3.696371
-14.180556	-7.348179	3.706368
-13.749710	-6.809979	3.716365
-13.510124	-6.417021	3.726362
-13.292653	-8.637959	3.736358
-12.286122	-7.982062	3.746355
-11.938645	-5.151287	3.756352
-11.912589	-3.766141	3.766349
-10.761419	-5.193885	3.776346
-10.186232	-0.211350	3.786342
-10.175161	0.860155	3.796339
-9.839659	-2.771977	3.806336
-9.469894	-3.652935	3.816333
-8.111463	-0.052078	3.826330
-7.518687	-4.765073	3.836326
-7.351911	-3.369729	3.846323
-7.154463	1.104188	3.856320
-7.133262	-4.220749	3.866317
-6.093878	-6.613476	3.876314
-5.215892	6.017335	3.886310
-4.721655	4.527879	3.896307
-4.561913	12.749095	3.906304
-4.523633	18.630379	3.916301
-4.232796	21.630420	3.926298
-3.311157	39.743645	3.936294
-2.554173	40.085971	3.946291
-2.128738	64.850157	3.956288
-1.990338	69.608154	3.966285
-1.287460	88.640603	3.976282
-0.916598	89.960540	3.986278
-0.259962	107.773112	3.996275
0.000000	122.345817	4.001280
0.484506	135.976408	4.006285
0.185866	132.504606	4.011290
0.345270	137.762985	4.016294
0.394901	134.697219	4.021299
0.208362	142.088044	4.026304
0.368327	144.261841	4.031309
0.597413	155.051494	4.036314
0.872885	157.180440	4.041318
0.843409	159.672648	4.046323
0.929583	164.775674	4.051328
1.546109	163.244649	4.056333
1.178054	162.136181	4.061338
0.889351	150.948624	4.066342
0.564943	148.843875	4.071347
0.388816	144.928034	4.076352
1.087728	150.749515	4.081357
1.097003	166.685424	4.086362
0.722278	159.079923	4.091366
0.809787	154.498860	4.096371
1.134304	157.988348	4.101376
1.085377	155.467218	4.106381
1.112875	161.991708	4.111386
1.142696	144.242219	4.116390
0.732835	147.728861	4.121395
0.645872	144.409730	4.126400
0.884237	157.743620	4.131405
1.099891	163.344304	4.136410
1.181324	165.733027	4.141414
1.315262	158.493092	4.146419
1.277680	157.301277	4.151424
1.284689	156.555321	4.156429
0.719963	153.628374	4.161434
1.021130	155.459418	4.166438
1.533047	160.129769	4.171443
1.058695	152.133933	4.176448
0.982204	141.249732	4.181453
0.923034	142.436590	4.186458
0.997329	152.447253	4.191462
1.504414	154.860929	4.196467
1.121151	155.721599	4.201472
1.427850	157.792074	4.206477
1.134981	159.302332	4.211482
1.461824	163.738233	4.216486
1.261117	154.280857	4.221491
1.106589	148.927414	4.226496
1.420789	155.278743	4.231501
1.029688	154.605868	4.236506
1.446671	158.479188	4.241510
1.695093	156.258503	4.246515
1.205548	153.401346	4.251520
0.929293	142.511868	4.256525
1.119656	145.881770	4.261530
0.918417	165.008596	4.266534
0.989090	159.435580	4.271539
1.139890	161.767189	4.276544
0.928593	158.137995	4.281549
0.956359	160.424146	4.286554
1.181363	164.948409	4.291558
1.525894	175.150571	4.296563
1.814661	183.639299	4.301568
1.775143	164.308052	4.306573
1.348246	168.382028	4.311578
1.292451	168.924631	4.316582
1.521165	162.080771	4.321587
1.346258	169.725023	4.326592
1.616330	161.519803	4.331597
1.680233	164.288739	4.336602
1.214636	165.058508	4.341606
1.360901	168.514283	4.346611
1.460244	182.400349	4.351616
1.877706	176.291943	4.356621
1.946519	191.417800	4.361626
1.480560	172.618985	4.366630
1.745191	168.827209	4.371635
1.492797	161.053571	4.376640
1.521159	165.630056	4.381645
1.736153	177.339464	4.386650
1.938876	174.116426	4.391654
1.637307	160.072449	4.396659
1.273109	172.275947	4.401664
1.378186	180.028176	4.406669
1.866274	195.900709	4.411674
1.655754	205.141396	4.416678
1.669877	195.532452	4.421683
1.973868	187.340721	4.426688
1.970709	185.716944	4.431693
1.889152	196.875967	4.436698
1.868365	188.435709	4.441702
2.284766	184.255413	4.446707
1.754474	177.361688	4.451712
1.812076	168.605704	4.456717
1.535982	165.452192	4.461722
1.766461	178.602906	4.466726
1.951443	176.399471	4.471731
1.935351	188.623659	4.476736
2.026559	185.462370	4.481741
1.820316	179.603266	4.486746
1.707009	183.312743	4.491750
2.250572	188.888137	4.496755
1.568983	182.944256	4.501760
2.001002	193.732568	4.506765
1.772269	195.766742	4.511770
2.004127	197.888736	4.516774
1.886033	186.821978	4.521779
1.800783	195.913572	4.526784
2.189543	193.063547	4.531789
1.795938	198.097148	4.536794
1.755136	204.659057	4.541798
1.609512	211.356791	4.546803
1.832646	209.137341	4.551808
1.980124	195.429933	4.556813
1.707962	202.921845	4.561818
1.605340	201.298615	4.566822
1.958011	208.428757	4.571827
2.103505	218.161623	4.576832
2.438859	215.771968	4.581837
2.449553	212.635108	4.586842
2.438244	210.269924	4.591846
2.444753	199.106670	4.596851
1.926552	199.753761	4.601856
1.983163	198.566019	4.606861
2.176564	196.057488	4.611866
2.091079	206.783237	4.616870
2.512952	215.065352	4.621875
2.064023	212.926630	4.626880
2.343402	205.946853	4.631885
2.662502	210.623419	4.636890
2.560918	204.553720	4.641894
2.557621	191.963612	4.646899
2.292826	195.954805	4.651904
2.383065	178.297255	4.656909
2.287274	182.607065	4.661914
2.094352	185.298322	4.666918
2.225772	189.536821	4.671923
2.090378	187.759201	4.676928
2.450067	190.322887	4.681933
2.351571	198.731349	4.686938
2.438939	198.515093	4.691942
2.593972	203.054944	4.696947
2.471130	201.416724	4.701952
2.564110	188.227498	4.706957
2.502233	196.707030	4.711962
2.468085	187.758494	4.716966
2.655579	192.604534	4.721971
2.202850	193.029399	4.726976
2.521886	195.568073	4.731981
2.044728	194.055051	4.736986
2.527283	202.987149	4.741990
2.677590	207.026366	4.746995
2.582854	211.013173	4.752000
2.766851	218.605291	4.757005
2.899386	221.473927	4.762010
2.623135	214.404562	4.767014
2.657135	201.179348	4.772019
2.454436	200.804305	4.777024
2.588066	210.634252	4.782029
2.873554	215.154002	4.787034
2.431472	215.729636	4.792038
2.896177	216.268998	4.797043
2.573969	212.420243	4.802048
3.052164	216.785220	4.807053
2.519252	203.322717	4.812058
2.350834	206.561053	4.817062
2.733568	209.651341	4.822067
2.205682	210.603540	4.827072
2.761632	215.932389	4.832077
2.699812	216.343387	4.837082
2.726427	208.240374	4.842086
3.083354	204.455546	4.847091
2.921888	206.420130	4.852096
2.581199	204.072992	4.857101
2.880945	209.977223	4.862106
2.598237	206.624707	4.867110
2.887188	216.115477	4.872115
2.669349	215.051102	4.877120
2.428886	207.717680	4.882125
2.814517	214.719408	4.887130
2.380485	212.358184	4.892134
2.883144	229.464816	4.897139
2.775108	238.916605	4.902144
3.119004	236.038510	4.907149
2.932867	237.707055	4.912154
3.090374	240.734739	4.917158
3.153788	233.070779	4.922163
3.145461	238.318988	4.927168
3.089371	211.850143	4.932173
3.048114	215.906403	4.937178
2.859899	209.548197	4.942182
3.462411	216.810073	4.947187
3.037817	211.639829	4.952192
3.023807	208.896018	4.957197
3.143647	206.095820	4.962202
3.256314	213.845029	4.967206
3.168912	211.829142	4.972211
3.011648	211.257107	4.977216
3.327610	206.323903	4.982221
3.271718	209.245959	4.987226
3.119256	218.640395	4.992230
3.136990	210.265947	4.997235
3.195924	210.347850	5.002240
3.191551	209.924252	5.007245
3.022170	211.748073	5.012250
2.838907	208.424808	5.017254
3.250126	230.297421	5.022259
3.208901	243.246883	5.027264
3.517987	233.404380	5.032269
3.038938	243.054791	5.037274
2.941748	244.374665	5.042278
3.309162	239.068819	5.047283
3.020706	251.129944	5.052288
3.204431	244.445473	5.057293
3.103061	245.713748	5.062298
3.016394	235.240243	5.067302
3.362091	240.169719	5.072307
3.011644	244.942195	5.077312
3.045151	243.000334	5.082317
3.563351	245.184850	5.087322
3.320608	250.881888	5.092326
3.525466	244.746634	5.097331
3.290838	243.257822	5.102336
3.586255	247.421125	5.107341
3.746354	250.355437	5.112346
3.364884	241.786451	5.117350
3.397269	243.141619	5.122355
3.126343	252.268451	5.127360
3.288864	256.959414	5.132365
3.875659	266.322959	5.137370
3.695662	262.839299	5.142374
3.773592	264.791133	5.147379
3.336289	260.037188	5.152384
3.785439	265.630079	5.157389
3.814072	275.224144	5.162394
3.532980	254.734138	5.167398
3.933520	247.452017	5.172403
3.603882	239.531931	5.177408
3.462752	249.955765	5.182413
3.539374	240.798953	5.187418
3.639580	255.295490	5.192422
3.919188	254.997551	5.197427
3.688146	262.122326	5.202432
3.640830	261.630484	5.207437
3.813310	257.298115	5.212442
3.758361	247.298652	5.217446
3.726329	248.552837	5.222451
3.633682	260.229774	5.227456
3.819379	264.928334	5.232461
3.889979	260.744717	5.237466
3.545372	259.540583	5.242470
3.997668	259.409301	5.247475
3.589216	263.624880	5.252480
3.805121	268.529171	5.257485
3.827146	274.407365	5.262490
3.650369	282.646351	5.267494
4.233932	278.710960	5.272499
4.062042	286.249786	5.277504
3.725100	275.028520	5.282509
3.951030	281.028717	5.287514
3.902829	280.280487	5.292518
3.989661	269.064562	5.297523
3.808557	282.582934	5.302528
4.168250	274.929302	5.307533
3.934525	274.306038	5.312538
3.938694	275.627616	5.317542
4.238628	278.376679	5.322547
4.192301	280.217547	5.327552
3.830522	275.337379	5.332557
4.120203	268.398091	5.337562
4.000243	276.439769	5.342566
4.016927	279.872116	5.347571
4.132433	279.808654	5.352576
4.000413	289.200130	5.357581
4.004391	276.762861	5.362586
3.798463	282.874111	5.367590
4.032191	285.359886	5.372595
3.799814	278.863359	5.377600
3.837714	283.036522	5.382605
3.887877	275.015597	5.387610
3.957561	282.118022	5.392614
4.301429	277.370387	5.397619
4.237263	282.612302	5.402624
3.944433	292.996655	5.407629
4.225589	281.732239	5.412634
4.192026	285.625425	5.417638
4.286996	280.278221	5.422643
3.969975	286.127527	5.427648
3.943085	283.742820	5.432653
4.279023	300.587557	5.437658
4.135814	299.792169	5.442662
4.274230	306.844306	5.447667
4.273963	319.995803	5.452672
4.468066	307.807121	5.457677
4.594073	312.587643	5.462682
4.198627	317.527856	5.467686
4.370913	316.045005	5.472691
4.226289	308.454068	5.477696
4.778018	316.356493	5.482701
4.586715	314.673597	5.487706
4.047573	313.516199	5.492710
4.504147	307.862608	5.497715
4.429579	322.479032	5.502720
4.508746	318.725347	5.507725
4.434835	314.466675	5.512730
4.332939	315.572243	5.517734
4.605700	307.450169	5.522739
4.349239	306.791216	5.527744
4.360605	301.040342	5.532749
4.250773	321.194484	5.537754
4.024045	313.161548	5.542758
4.355590	313.036128	5.547763
4.214328	314.079962	5.552768
4.273412	313.934907	5.557773
4.735580	321.837816	5.562778
4.656288	318.068439	5.567782
4.362028	319.763450	5.572787
4.474563	322.285360	5.577792
4.830978	326.945695	5.582797
4.783872	330.923037	5.587802
4.366394	332.846915	5.592806
4.813625	336.881212	5.597811
4.715388	343.297226	5.602816
4.887965	338.820962	5.607821
4.943884	336.766436	5.612826
4.661329	335.092983	5.617830
4.898242	326.369068	5.622835
4.526801	320.162236	5.627840
4.645820	324.994244	5.632845
4.855155	325.487849	5.637850
4.760625	340.017032	5.642854
4.858080	330.904853	5.647859
5.040966	340.183041	5.652864
4.995775	330.404100	5.657869
5.029221	323.447586	5.662874
4.850323	317.976381	5.667878
4.541604	312.841306	5.672883
4.919432	316.346833	5.677888
4.745554	330.090585	5.682893
4.983881	326.568162	5.687898
4.892924	344.304814	5.692902
5.089262	334.798499	5.697907
4.974079	335.599620	5.702912
4.831642	330.760331	5.707917
5.053972	335.193328	5.712922
5.056043	336.500657	5.717926
5.236901	330.332655	5.722931
5.134405	326.918387	5.727936
4.824110	315.550976	5.732941
5.039824	316.278151	5.737946
4.515467	319.855099	5.742950
5.003452	323.126040	5.747955
5.166939	341.681364	5.752960
5.053988	349.318168	5.757965
5.353738	342.132677	5.762970
5.034471	350.105697	5.767974
5.371455	344.296343	5.772979
5.126201	345.173746	5.777984
5.162144	343.691651	5.782989
5.283469	340.560056	5.787994
5.183036	349.346027	5.792998
5.216669	339.231732	5.798003
4.905929	350.567686	5.803008
4.986419	353.430790	5.808013
5.028135	342.564292	5.813018
4.754540	345.514863	5.818022
4.932736	349.766155	5.823027
5.094541	339.259763	5.828032
5.089518	336.629087	5.833037
5.068523	338.082331	5.838042
5.095243	346.106176	5.843046
5.293463	340.133013	5.848051
5.523985	344.605499	5.853056
4.842840	343.080389	5.858061
5.405924	355.491811	5.863066
5.240562	373.571991	5.868070
5.373725	368.469023	5.873075
5.428643	376.232648	5.878080
5.404870	370.721432	5.883085
5.580433	373.533808	5.888090
5.443533	378.504276	5.893094
5.556140	372.935856	5.898099
5.572225	374.723342	5.903104
5.358035	370.360099	5.908109
5.257462	376.803550	5.913114
5.463699	370.817795	5.918118
5.873187	370.419530	5.923123
5.252025	376.986809	5.928128
5.216752	376.126510	5.933133
5.569105	365.230858	5.938138
5.482566	373.720111	5.943142
5.695453	368.194817	5.948147
5.534207	373.652800	5.953152
5.464577	369.611850	5.958157
5.893054	377.799221	5.963162
5.412886	376.042775	5.968166
5.837421	370.088223	5.973171
5.801168	375.502539	5.978176
5.757531	371.988690	5.983181
5.809573	367.188696	5.988186
5.635307	373.536059	5.993190
5.738989	370.316222	5.998195
5.605795	368.074084	6.003200
5.749845	369.465167	6.008205
5.635992	365.058607	6.013210
5.822895	371.762509	6.018214
5.709725	361.531901	6.023219
5.648732	373.140713	6.028224
5.467476	365.814739	6.033229
5.507399	371.073917	6.038234
5.487514	377.551317	6.043238
5.721433	375.601387	6.048243
5.407793	384.624888	6.053248
5.300248	375.770337	6.058253
5.520723	376.307874	6.063258
5.532464	373.820236	6.068262
5.675886	379.355452	6.073267
5.281210	377.377988	6.078272
5.625654	381.020504	6.083277
5.703358	363.200644	6.088282
5.414753	389.211681	6.093286
5.617113	387.822689	6.098291
5.915738	397.349260	6.103296
5.742711	384.578229	6.108301
6.291078	380.019954	6.113306
5.749022	373.371014	6.118310
5.963883	380.819356	6.123315
6.025334	383.794954	6.128320
5.808867	373.302674	6.133325
5.727221	376.293175	6.138330
5.711534	380.559928	6.143334
6.061627	365.107010	6.148339
6.015220	376.008521	6.153344
5.757247	376.040882	6.158349
5.940191	379.165993	6.163354
5.648269	387.850416	6.168358
5.885320	383.070776	6.173363
5.875662	370.540582	6.178368
5.654653	358.309168	6.183373
5.913373	349.434207	6.188378
5.649819	364.626923	6.193382
5.522093	347.395738	6.198387
5.631538	352.685188	6.203392
5.415737	350.762849	6.208397
5.524804	362.372591	6.213402
5.262270	376.979462	6.218406
5.824752	374.979457	6.223411
5.703772	387.118622	6.228416
5.860036	386.285686	6.233421
5.947835	382.864836	6.238426
6.204494	382.541900	6.243430
6.063876	368.239112	6.248435
5.827898	357.614516	6.253440
5.572319	344.121972	6.258445
5.600611	348.805281	6.263450
5.386617	342.549774	6.268454
5.348753	342.423399	6.273459
5.322805	367.664946	6.278464
5.385081	373.860116	6.283469
5.709468	370.533540	6.288474
5.833726	383.073770	6.293478
5.550703	371.890831	6.298483
5.788696	386.756101	6.303488
5.796907	386.105247	6.308493
5.713412	383.594562	6.313498
5.509566	376.650432	6.318502
5.929646	377.444281	6.323507
5.488295	373.708036	6.328512
5.590464	376.612139	6.333517
5.737646	371.339894	6.338522
5.935567	378.593913	6.343526
5.796751	373.694808	6.348531
6.040981	379.110457	6.353536
5.798949	374.785978	6.358541
5.860004	380.915445	6.363546
5.590276	370.021563	6.368550
5.596994	366.204331	6.373555
5.626089	365.839891	6.378560
5.667447	375.311530	6.383565
6.064994	370.017207	6.388570
5.337891	365.003951	6.393574
5.511375	366.177809	6.398579
5.870106	371.161401	6.403584
5.526362	376.308330	6.408589
5.673808	375.744841	6.413594
5.689582	380.876611	6.418598
5.960562	383.758379	6.423603
5.881257	376.176877	6.428608
5.931430	376.124274	6.433613
5.509374	358.478657	6.438618
5.563684	360.139020	6.443622
5.580205	370.205011	6.448627
5.664920	374.649448	6.453632
5.557432	379.117941	6.458637
5.695458	377.502645	6.463642
5.509595	384.180502	6.468646
5.942397	383.259766	6.473651
5.455152	378.177432	6.478656
5.397121	380.508660	6.483661
5.850461	381.038078	6.488666
5.473643	377.227959	6.493670
5.495719	375.684032	6.498675
5.584130	381.552811	6.503680
5.436508	382.652368	6.508685
5.786218	374.804985	6.513690
5.841493	394.799367	6.518694
5.869417	380.883942	6.523699
5.952123	383.901394	6.528704
5.756879	384.038177	6.533709
5.963422	376.951240	6.538714
5.634032	384.295476	6.543718
5.755872	376.870770	6.548723
5.591934	380.342437	6.553728
5.689850	374.044347	6.558733
5.787105	381.200251	6.563738
5.815127	377.352834	6.568742
5.880533	375.293372	6.573747
5.820379	377.009663	6.578752
6.023543	380.150752	6.583757
6.124527	370.162192	6.588762
5.611641	362.422279	6.593766
5.121618	345.585995	6.598771
5.632040	363.714072	6.603776
5.887019	372.001319	6.608781
6.147770	364.837100	6.613786
5.442679	355.847055	6.618790
5.841638	347.773445	6.623795
5.604937	343.673445	6.628800
5.537015	343.749993	6.633805
5.607777	344.750496	6.638810
5.381064	356.168589	6.643814
5.594055	369.005058	6.648819
5.451150	374.771386	6.653824
5.687848	386.489777	6.658829
5.912883	376.288784	6.663834
5.869140	389.540315	6.668838
5.728762	384.133527	6.673843
5.956713	380.050807	6.678848
5.828408	372.637095	6.683853
5.589281	355.927620	6.688858
5.189460	362.067380	6.693862
5.653224	377.452584	6.698867
5.748098	376.722402	6.703872
5.292358	389.680305	6.708877
5.517656	378.120814	6.713882
5.326709	382.923849	6.718886
5.549536	375.748366	6.723891
5.209797	382.809567	6.728896
5.375090	381.705571	6.733901
5.810960	381.564982	6.738906
5.810315	381.878988	6.743910
6.044035	383.103615	6.748915
5.638673	386.461491	6.753920
5.311878	389.236405	6.758925
5.575923	380.912486	6.763930
5.562479	397.746336	6.768934
5.558282	392.905953	6.773939
5.791256	388.874098	6.778944
5.670004	394.720307	6.783949
5.907193	387.177756	6.788954
5.475559	392.346206	6.793958
5.713772	387.402188	6.798963
5.762482	381.582720	6.803968
5.504351	389.837258	6.808973
5.779891	396.664376	6.813978
5.812579	403.627767	6.818982
5.855608	389.175244	6.823987
6.030646	391.187716	6.828992
5.927493	389.088188	6.833997
5.925981	378.263778	6.839002
5.614218	394.661767	6.844006
5.793863	379.157444	6.849011
5.549846	381.353036	6.854016
5.602698	382.668900	6.859021
5.712494	387.426881	6.864026
5.879812	388.683067	6.869030
5.964007	384.656801	6.874035
5.945717	396.699378	6.879040
5.865588	389.408287	6.884045
6.323703	381.107758	6.889050
5.448161	389.310605	6.894054
5.784046	382.613216	6.899059
5.763442	383.794669	6.904064
5.399093	385.039376	6.909069
6.059910	376.131308	6.914074
5.913973	383.936808	6.919078
5.706494	380.262131	6.924083
6.123840	376.897409	6.929088
5.397517	366.871328	6.934093
5.846713	362.182923	6.939098
5.567327	353.791479	6.944102
5.669346	355.006420	6.949107
5.551622	367.320063	6.954112
5.678355	374.833568	6.959117
5.950647	372.213821	6.964122
5.795664	377.442842	6.969126
5.240788	355.418151	6.974131
5.530995	362.053769	6.979136
5.590243	376.986430	6.984141
5.884625	374.742485	6.989146
5.779985	381.600820	6.994150
5.831426	375.795898	6.999155
5.636364	377.252425	7.004160
5.772703	381.705452	7.009165
5.664547	385.588763	7.014170
5.627241	380.785856	7.019174
5.771378	383.320282	7.024179
5.833350	386.782619	7.029184
5.807393	383.302139	7.034189
5.944681	358.220330	7.039194
5.592357	352.100490	7.044198
5.650230	340.700478	7.049203
5.611949	348.867540	7.054208
5.702825	359.621899	7.059213
5.744173	355.380564	7.064218
5.510494	352.129782	7.069222
5.734395	358.651704	7.074227
5.843574	364.024675	7.079232
5.687908	362.945219	7.084237
5.878478	348.129583	7.089242
5.260849	357.646613	7.094246
5.537418	369.620227	7.099251
5.617714	372.777988	7.104256
5.629245	383.379594	7.109261
5.776328	374.106798	7.114266
5.865299	375.935253	7.119270
5.861674	382.999786	7.124275
6.044060	385.692827	7.129280
5.334092	371.960051	7.134285
5.662010	364.560890	7.139290
5.382805	389.419905	7.144294
6.117972	384.082680	7.149299
5.818010	380.044690	7.154304
5.840856	372.864362	7.159309
5.718847	364.531607	7.164314
5.394612	362.469818	7.169318
5.686628	371.792243	7.174323
5.751664	374.761915	7.179328
5.821310	371.706787	7.184333
5.909305	353.620010	7.189338
5.609191	359.391941	7.194342
5.583957	346.514876	7.199347
5.397290	364.947080	7.204352
5.414397	379.233966	7.209357
5.771313	375.154281	7.214362
6.022261	394.976820	7.219366
6.169135	380.592884	7.224371
5.804627	366.113204	7.229376
5.526462	358.424855	7.234381
5.586562	354.187705	7.239386
5.318865	360.652811	7.244390
5.575131	371.458030	7.249395
5.801492	380.320928	7.254400
5.323153	388.246407	7.259405
5.722167	376.577727	7.264410
6.110912	390.047058	7.269414
5.852518	383.372868	7.274419
5.807368	370.657554	7.279424
5.702641	359.448343	7.284429
5.841906	353.720592	7.289434
5.732960	359.759906	7.294438
5.875354	346.097610	7.299443
5.652049	344.369906	7.304448
5.609530	365.982860	7.309453
5.893662	354.045185	7.314458
5.263013	359.663276	7.319462
5.687483	351.568847	7.324467
5.172080	350.199511	7.329472
5.687336	369.304385	7.334477
5.773250	377.040757	7.339482
5.904455	377.458945	7.344486
6.011787	384.991269	7.349491
5.808707	369.861372	7.354496
5.487344	368.236793	7.359501
5.679820	355.004050	7.364506
5.906443	361.233465	7.369510
5.677649	352.816247	7.374515
5.739765	348.078718	7.379520
5.544318	359.698818	7.384525
5.705460	349.878070	7.389530
5.769866	352.527174	7.394534
5.481760	352.238745	7.399539
5.759948	362.397398	7.404544
5.261597	374.463117	7.409549
5.661298	377.077214	7.414554
5.501633	386.846307	7.419558
5.872096	383.313551	7.424563
6.000128	382.791966	7.429568
5.909771	390.039640	7.434573
5.801669	380.752227	7.439578
5.457215	364.942928	7.444582
5.628235	376.554617	7.449587
5.639410	389.931997	7.454592
5.835121	391.592145	7.459597
6.044799	382.947909	7.464602
5.622460	375.309959	7.469606
5.543532	365.561862	7.474611
5.666179	359.787340	7.479616
5.617630	382.237030	7.484621
5.960975	373.814882	7.489626
5.192642	374.758512	7.494630
5.064000	382.223300	7.499635
5.494819	383.667950	7.504640
5.503922	386.134246	7.509645
5.679401	380.453745	7.514650
5.694448	383.174601	7.519654
5.804720	384.975836	7.524659
5.847234	384.394663	7.529664
5.566725	401.969500	7.534669
5.953960	388.352310	7.539674
5.784029	383.341946	7.544678
5.625631	388.956145	7.549683
6.096333	389.999694	7.554688
5.764188	390.981330	7.559693
5.983219	390.834948	7.564698
5.792818	398.640544	7.569702
5.959000	391.402047	7.574707
5.707472	368.896725	7.579712
5.617404	365.490250	7.584717
5.917936	360.313683	7.589722
5.802740	364.009310	7.594726
5.821562	350.792410	7.599731
5.714256	353.069862	7.604736
5.772392	354.999344	7.609741
5.705449	358.701749	7.614746
5.453001	351.321115	7.619750
5.693264	352.210761	7.624755
5.844583	352.485300	7.629760
5.581046	354.882060	7.634765
5.582230	353.382259	7.639770
5.626681	357.529095	7.644774
5.781612	354.565368	7.649779
5.696043	345.619368	7.654784
5.313044	354.368640	7.659789
6.032955	364.482091	7.664794
5.643559	367.915849	7.669798
5.575369	362.330913	7.674803
5.867345	369.798992	7.679808
5.561246	369.313455	7.684813
5.881256	361.764255	7.689818
5.627431	356.788762	7.694822
5.400862	350.110086	7.699827
5.735085	363.810458	7.704832
5.783282	376.010688	7.709837
5.783500	374.060137	7.714842
5.665312	371.750581	7.719846
5.770929	371.345992	7.724851
5.630634	353.043587	7.729856
5.730028	364.621194	7.734861
5.856897	369.054677	7.739866
5.504407	347.222108	7.744870
5.761708	358.694925	7.749875
5.841855	356.970259	7.754880
5.364233	359.020368	7.759885
5.857965	363.482656	7.764890
5.469424	381.267236	7.769894
5.554540	377.441114	7.774899
5.806798	386.976569	7.779904
5.694551	391.311076	7.784909
5.914503	387.853065	7.789914
5.847778	381.327184	7.794918
5.665639	367.035640	7.799923
5.818241	362.492636	7.804928
5.671914	363.546984	7.809933
5.683750	354.529140	7.814938
5.646568	365.182442	7.819942
5.596046	359.011842	7.824947
5.647754	364.615183	7.829952
5.668447	373.787544	7.834957
5.734985	378.313740	7.839962
5.681301	386.191524	7.844966
5.553437	379.067029	7.849971
5.853935	389.906940	7.854976
5.920532	381.252744	7.859981
5.894317	365.072642	7.864986
5.546474	369.724940	7.869990
5.514513	363.527771	7.874995
5.636832	374.216135	7.880000
5.440994	379.723085	7.885005
5.810936	394.541763	7.890010
5.907006	387.847528	7.895014
5.686345	378.283021	7.900019
5.974641	371.849094	7.905024
5.734137	366.805869	7.910029
5.500033	361.964836	7.915034
5.498109	374.115380	7.920038
5.349140	387.793276	7.925043
5.613404	394.463610	7.930048
5.544304	391.854626	7.935053
5.484000	390.286305	7.940058
5.614238	391.530303	7.945062
5.664418	395.618377	7.950067
5.840379	384.098064	7.955072
5.579072	396.845659	7.960077
6.191916	385.591156	7.965082
6.099441	396.047849	7.970086
5.927416	384.312661	7.975091
5.699866	363.475181	7.980096
5.407907	354.656229	7.985101
5.864246	375.863439	7.990106
5.846055	371.153460	7.995110
5.859746	369.224349	8.000115
5.673137	361.309249	8.005133
5.696836	360.097692	8.010150
5.565036	351.495390	8.015168
5.547537	355.697629	8.020186
5.404383	370.666553	8.025203
5.727297	384.893914	8.030221
5.995454	395.461843	8.035238
6.245001	384.226895	8.040256
5.755395	370.931169	8.045274
5.806497	362.594494	8.050291
5.706440	356.533907	8.055309
5.531526	368.030892	8.060326
5.603882	358.065254	8.065344
5.692086	353.068544	8.070362
5.315453	359.688514	8.075379
5.482511	368.657049	8.080397
5.803746	386.384152	8.085414
6.085837	390.171875	8.090432
5.911516	391.216047	8.095450
5.771295	397.919166	8.100467
6.149829	386.473621	8.105485
5.751176	395.562776	8.110502
5.508831	387.890355	8.115520
5.587189	384.116611	8.120538
5.168783	390.971861	8.125555
5.826800	386.643937	8.130573
5.915866	392.445049	8.135590
5.991358	388.874910	8.140608
5.818767	387.615868	8.145626
5.928153	391.289987	8.150643
5.727959	385.038574	8.155661
5.431425	398.322948	8.160678
5.609744	391.185074	8.165696
5.994725	399.270635	8.170714
5.941601	393.118580	8.175731
5.899203	393.964267	8.180749
5.623022	389.784930	8.185766
5.626179	386.576782	8.190784
5.849880	388.067542	8.195802
5.596277	394.585194	8.200819
5.751588	392.371144	8.205837
5.789499	410.710078	8.210854
6.198581	419.541967	8.215872
6.051437	410.938443	8.220890
5.598532	401.589956	8.225907
6.238326	415.639292	8.230925
6.065447	405.899211	8.235942
6.098525	395.572790	8.240960
5.940656	389.524949	8.245978
5.993190	395.261669	8.250995
6.171993	392.805351	8.256013
5.593134	397.860088	8.261030
5.905207	387.430808	8.266048
6.058045	386.735330	8.271066
5.687084	395.906488	8.276083
6.001704	398.497581	8.281101
5.963654	405.173879	8.286118
5.787958	401.933060	8.291136
5.950869	411.452258	8.296154
6.297069	421.292930	8.301171
6.358541	401.703606	8.306189
5.749655	404.481468	8.311206
5.892257	392.543098	8.316224
5.973429	394.379369	8.321242
6.162909	418.740178	8.326259
6.259215	408.794343	8.331277
5.954009	404.323989	8.336294
5.829033	402.259075	8.341312
5.798156	403.483127	8.346330
5.839502	411.521689	8.351347
6.344678	410.428111	8.356365
6.331323	418.860970	8.361382
6.252938	417.543357	8.366400
6.357469	399.911259	8.371418
5.794029	394.979745	8.376435
5.916289	404.944235	8.381453
6.025817	413.819023	8.386470
6.109011	415.776800	8.391488
6.211392	428.155012	8.396506
5.883628	420.283014	8.401523
6.556524	418.893865	8.406541
6.279536	415.618310	8.411558
5.986177	400.842045	8.416576
5.950146	395.223710	8.421594
5.977517	401.824572	8.426611
6.125054	418.396641	8.431629
6.219573	422.940874	8.436646
6.207266	420.233471	8.441664
6.210266	427.771377	8.446682
6.189967	430.166200	8.451699
6.337390	417.293043	8.456717
5.849874	407.835355	8.461734
6.209827	418.174480	8.466752
6.503771	418.654252	8.471770
5.851233	427.060300	8.476787
6.099719	420.617376	8.481805
5.964087	429.602601	8.486822
6.376310	426.989577	8.491840
6.218398	424.826798	8.496858
6.176645	437.114419	8.501875
6.257110	431.742431	8.506893
6.080477	432.786597	8.511910
5.691757	434.150635	8.516928
6.200070	422.888590	8.521946
6.044527	436.564484	8.526963
6.396665	425.304974	8.531981
6.285648	427.251139	8.536998
6.157064	431.290384	8.542016
6.458287	434.753116	8.547034
6.390744	438.663724	8.552051
6.204232	428.878851	8.557069
6.223344	426.018207	8.562087
6.172202	434.061525	8.567104
6.250777	430.278483	8.572122
6.001899	431.228565	8.577139
6.099848	423.251358	8.582157
6.045953	430.369432	8.587175
6.095272	427.920066	8.592192
6.119179	429.258624	8.597210
6.096914	441.638472	8.602227
6.410973	446.990828	8.607245
6.361853	453.880581	8.612263
6.588303	455.985401	8.617280
6.535187	451.094820	8.622298
6.076042	452.154256	8.627315
6.417098	454.500632	8.632333
6.563256	451.824948	8.637351
6.159757	452.012813	8.642368
6.605130	451.402357	8.647386
6.355988	464.534830	8.652403
6.516259	452.260634	8.657421
6.524061	442.013770	8.662439
6.402899	431.302962	8.667456
6.629812	426.973659	8.672474
6.205228	429.809859	8.677491
6.107958	426.211937	8.682509
6.338155	428.053163	8.687527
6.315829	453.583378	8.692544
6.499081	446.296836	8.697562
6.367153	455.083841	8.702579
6.665668	447.364400	8.707597
6.908217	454.058639	8.712615
6.341228	437.940743	8.717632
6.506859	434.105438	8.722650
6.419628	429.628763	8.727667
6.703603	426.742202	8.732685
6.405511	424.549579	8.737703
6.271391	428.059084	8.742720
6.316159	425.498280	8.747738
6.507910	445.782169	8.752755
6.710288	448.690718	8.757773
6.488418	439.610667	8.762791
6.383483	453.041571	8.767808
6.920959	449.827069	8.772826
6.456756	429.248808	8.777843
6.446439	426.708379	8.782861
6.305006	438.751374	8.787879
6.457492	441.455833	8.792896
6.963466	449.665589	8.797914
6.661354	446.555605	8.802931
6.597782	428.526259	8.807949
6.353032	430.864108	8.812967
6.277174	442.278547	8.817984
6.489683	440.345901	8.823002
6.474862	453.229986	8.828019
6.444176	446.201819	8.833037
6.513859	449.841021	8.838055
6.364643	459.662303	8.843072
6.700355	450.680690	8.848090
6.704612	459.818255	8.853107
6.547823	454.999230	8.858125
6.995130	456.236511	8.863143
6.660115	457.119226	8.868160
6.782170	459.434689	8.873178
6.457560	459.203376	8.878195
6.668425	456.577560	8.883213
6.760222	447.730381	8.888231
6.770540	454.373072	8.893248
6.746009	456.172594	8.898266
6.497106	454.610315	8.903283
6.781316	459.011031	8.908301
6.831018	448.975682	8.913319
6.698930	458.005016	8.918336
6.679877	456.918066	8.923354
6.508418	459.039228	8.928371
6.771586	457.422342	8.933389
6.896403	455.553281	8.938407
6.898245	468.667462	8.943424
7.121452	451.482663	8.948442
6.995840	458.661879	8.953459
6.869935	443.991978	8.958477
6.763418	422.874788	8.963495
6.164409	427.247712	8.968512
6.471320	441.202024	8.973530
6.876365	456.152738	8.978547
6.601347	457.216015	8.983565
6.810972	450.418940	8.988583
6.936279	468.825692	8.993600
7.011895	451.692194	8.998618
6.780112	456.676072	9.003635
6.632233	453.961082	9.008653
7.030813	450.683454	9.013671
6.800281	457.591946	9.018688
6.590326	448.612459	9.023706
6.785629	446.953316	9.028723
6.910945	453.882376	9.033741
7.212994	456.414747	9.038759
7.105366	467.874246	9.043776
6.833537	450.410151	9.048794
6.647431	454.978993	9.053811
6.763944	448.493039	9.058829
7.090663	453.136467	9.063847
6.724130	462.920061	9.068864
7.188570	460.493020	9.073882
6.936453	461.571583	9.078899
6.644529	459.268097	9.083917
7.048176	458.504355	9.088935
6.876706	457.774403	9.093952
6.845083	452.802696	9.098970
6.818161	461.728536	9.103987
6.813729	457.597506	9.109005
6.776494	454.440935	9.114023
6.419020	453.048066	9.119040
6.695615	453.061672	9.124058
6.577321	454.885637	9.129075
6.855910	451.560440	9.134093
6.801414	448.761431	9.139111
6.755989	456.421169	9.144128
6.690099	456.871982	9.149146
6.637244	466.234969	9.154163
6.933141	477.133353	9.159181
7.303372	473.813783	9.164199
7.227082	491.614168	9.169216
7.011277	484.808075	9.174234
7.192047	481.920944	9.179251
7.120511	477.232216	9.184269
7.166589	454.533462	9.189287
6.729449	461.104679	9.194304
6.966973	466.176482	9.199322
7.110744	472.850734	9.204339
6.881844	485.885971	9.209357
7.085155	482.923051	9.214375
6.866681	487.486654	9.219392
7.031069	488.719985	9.224410
7.244355	488.159915	9.229427
6.998876	497.014632	9.234445
7.030093	482.183354	9.239463
7.131014	492.316197	9.244480
7.303367	491.034256	9.249498
7.103728	483.302922	9.254515
7.099068	493.530474	9.259533
7.282174	482.963525	9.264551
6.876001	488.474386	9.269568
6.801122	488.213570	9.274586
7.181817	482.733595	9.279603
6.770450	487.197382	9.284621
7.385562	483.873127	9.289639
7.035392	486.697361	9.294656
6.893353	483.415698	9.299674
7.276445	490.545803	9.304691
7.088829	488.802088	9.309709
7.174184	483.983550	9.314727
7.106527	484.881665	9.319744
7.399437	485.656861	9.324762
7.142798	484.986138	9.329779
6.894258	488.289105	9.334797
7.362729	478.800019	9.339815
7.406512	481.871538	9.344832
7.347490	477.012439	9.349850
7.406683	481.258848	9.354867
7.167804	488.393722	9.359885
7.546120	487.475345	9.364903
7.395452	488.985432	9.369920
7.259064	480.324968	9.374938
7.261262	485.894710	9.379955
7.153416	486.856193	9.384973
7.164899	476.127832	9.389991
7.099469	480.977384	9.395008
7.442323	478.373913	9.400026
7.401682	481.332901	9.405043
6.881326	492.328786	9.410061
7.353569	481.263622	9.415079
7.289658	484.766588	9.420096
7.507267	490.078105	9.425114
7.485145	489.501264	9.430131
7.038647	491.459503	9.435149
7.193608	487.547816	9.440167
7.145850	481.863885	9.445184
7.458651	491.355068	9.450202
7.541778	483.542288	9.455219
7.197042	485.776696	9.460237
7.095556	485.701585	9.465255
6.996652	503.370125	9.470272
7.391909	512.133505	9.475290
7.568315	519.043276	9.480307
7.536891	515.682398	9.485325
7.461577	511.939481	9.490343
7.341367	519.531766	9.495360
7.132125	526.667439	9.500378
7.722147	518.683386	9.505395
7.384561	526.645242	9.510413
7.500634	512.546419	9.515431
7.523918	523.111244	9.520448
7.562580	521.841090	9.525466
7.443443	516.022765	9.530483
7.327467	521.021860	9.535501
7.480461	523.595355	9.540519
7.703540	521.574532	9.545536
7.862996	519.771747	9.550554
7.847277	502.167787	9.555571
7.269091	490.271401	9.560589
7.364318	490.241145	9.565607
7.262357	500.438816	9.570624
7.195608	518.113838	9.575642
7.741681	515.891507	9.580659
7.890842	519.812961	9.585677
7.785127	519.455703	9.590695
7.618619	513.756266	9.595712
7.562588	500.541694	9.600730
7.331043	506.119196	9.605747
7.157520	516.143945	9.610765
7.481311	515.670812	9.615783
7.770718	522.072278	9.620800
7.488637	517.275240	9.625818
7.785944	511.707156	9.630835
7.655619	519.974292	9.635853
7.325152	513.646851	9.640871
7.586914	512.250449	9.645888
7.377024	523.873037	9.650906
7.511055	519.189889	9.655923
7.202735	524.210523	9.660941
7.166324	522.990443	9.665959
7.228565	527.397368	9.670976
7.709912	548.399724	9.675994
7.976952	539.008644	9.681011
7.580496	543.170389	9.686029
7.507801	541.193412	9.691047
7.815563	548.446094	9.696064
7.811773	553.533827	9.701082
8.013946	543.698644	9.706099
7.720111	542.058595	9.711117
7.268979	526.196326	9.716135
7.743000	537.917039	9.721152
7.533791	549.461390	9.726170
8.073751	548.221089	9.731187
7.994384	555.714485	9.736205
7.980249	542.716909	9.741223
8.058800	529.418334	9.746240
7.788314	528.708182	9.751258
8.028284	517.337537	9.756275
7.822134	517.558538	9.761293
7.661224	510.381727	9.766311
7.485592	515.957812	9.771328
7.516810	518.004155	9.776346
7.948040	528.635416	9.781363
7.622392	544.305649	9.786381
7.796110	547.645716	9.791399
8.346182	543.505953	9.796416
8.158998	533.142829	9.801434
8.284377	521.187737	9.806451
7.951431	516.383998	9.811469
7.695300	517.173101	9.816487
7.691732	520.970348	9.821504
7.442646	518.729215	9.826522
7.861621	515.761542	9.831539
8.056741	521.389576	9.836557
7.879335	519.461106	9.841575
7.765134	519.222572	9.846592
7.896499	528.769917	9.851610
7.860098	541.547633	9.856627
7.484060	547.576689	9.861645
7.835629	545.782319	9.866663
7.842209	538.343030	9.871680
7.849186	549.728821	9.876698
8.281605	548.050922	9.881715
8.103254	554.242183	9.886733
8.159794	552.317339	9.891751
8.471290	538.628885	9.896768
8.094043	554.450606	9.901786
7.979393	534.190843	9.906803
7.854665	534.295957	9.911821
7.795490	544.318055	9.916839
8.193307	544.110152	9.921856
7.825461	554.287295	9.926874
8.076567	550.248203	9.931891
7.877408	548.157414	9.936909
8.045137	553.247343	9.941927
8.168406	545.442622	9.946944
7.996098	546.937415	9.951962
7.988265	545.730692	9.956979
8.062138	550.665172	9.961997
8.150943	549.538243	9.967015
8.303024	542.985318	9.972032
7.872449	552.662891	9.977050
8.138924	548.904488	9.982067
8.093314	543.150105	9.987085
7.741625	558.465657	9.992103
8.123475	539.773218	9.997120
7.995170	551.987726	10.002138
8.004284	545.484940	10.007155
8.358587	543.690116	10.012173
8.175519	547.474689	10.017191
8.382676	551.106614	10.022208
8.014674	545.913648	10.027226
7.803550	550.168988	10.032243
8.199132	542.518987	10.037261
8.211831	539.820594	10.042279
8.302832	539.823518	10.047296
8.447985	547.590194	10.052314
8.377660	542.339089	10.057331
8.195281	546.034580	10.062349
8.143608	555.836757	10.067367
8.472588	546.548556	10.072384
8.327855	544.161739	10.077402
8.642475	536.886388	10.082419
8.385533	543.042878	10.087437
8.118435	541.657614	10.092455
8.324174	546.801257	10.097472
7.990710	546.604679	10.102490
8.309373	540.528157	10.107507
8.031928	546.220577	10.112525
8.263506	547.565567	10.117543
8.388013	540.753864	10.122560
8.108248	551.871597	10.127578
8.127292	557.396245	10.132595
8.333371	552.469635	10.137613
8.372719	553.344849	10.142631
8.399660	554.865969	10.147648
8.224343	555.185380	10.152666
8.286635	559.196474	10.157683
8.571881	555.025339	10.162701
8.338220	559.984170	10.167719
8.718689	562.494864	10.172736
8.555979	556.772144	10.177754
8.327605	554.676959	10.182771
8.428638	544.893427	10.187789
8.508596	556.216111	10.192807
8.329206	544.553961	10.197824
8.521255	553.878459	10.202842
8.376841	562.473325	10.207859
8.457947	548.805836	10.212877
8.508086	548.300438	10.217895
8.582109	543.135961	10.222912
8.480231	537.282674	10.227930
8.307108	541.922016	10.232947
8.349589	549.197338	10.237965
8.369838	566.589474	10.242983
8.758704	566.888725	10.248000
8.605497	576.065129	10.253018
8.571627	564.943885	10.258035
8.736597	557.653245	10.263053
8.350284	548.355602	10.268071
8.680207	548.786883	10.273088
8.761597	540.423229	10.278106
8.664340	535.212033	10.283123
8.821764	537.126387	10.288141
8.617756	547.476472	10.293159
8.358430	540.046540	10.298176
8.438205	546.549981	10.303194
8.515722	550.741991	10.308211
8.848127	562.699236	10.313229
8.513420	553.556974	10.318247
8.661523	539.974214	10.323264
8.414237	554.750407	10.328282
8.255352	565.205592	10.333299
8.667018	570.769110	10.338317
8.264823	575.343002	10.343335
8.700830	574.599858	10.348352
8.550753	578.397655	10.353370
8.230517	580.133164	10.358387
8.490489	577.949325	10.363405
8.265195	576.919480	10.368423
8.439431	586.481781	10.373440
8.880383	591.305067	10.378458
9.025830	590.027590	10.383475
8.808763	591.182416	10.388493
8.493653	587.380331	10.393511
8.896109	584.285874	10.398528
8.647289	577.498416	10.403546
8.801614	586.018445	10.408563
8.973876	573.731334	10.413581
8.766787	585.883576	10.418599
8.742750	580.882814	10.423616
8.572167	584.220871	10.428634
8.832499	601.238522	10.433651
9.232702	596.782148	10.438669
8.692813	594.370461	10.443687
9.046624	583.767984	10.448704
8.644671	588.612290	10.453722
8.914085	578.810786	10.458739
8.688890	587.822604	10.463757
9.024137	601.526308	10.468775
9.156503	589.494220	10.473792
9.046052	589.305254	10.478810
8.854495	595.122183	10.483827
9.088308	580.342956	10.488845
8.540042	584.892513	10.493863
8.877342	576.376273	10.498880
9.096582	576.670256	10.503898
9.007086	579.765129	10.508915
8.908223	576.667985	10.513933
8.606197	586.481481	10.518951
9.032783	598.739412	10.523968
9.132412	607.327398	10.528986
8.824833	609.630050	10.534003
9.269534	595.397598	10.539021
9.377628	608.040927	10.544039
9.075063	586.502595	10.549056
9.056049	581.216179	10.554074
8.518544	584.747693	10.559091
8.881581	587.238653	10.564109
8.957086	604.670265	10.569127
9.059262	607.806506	10.574144
9.308357	613.823798	10.579162
9.142568	612.764574	10.584179
9.476102	594.986325	10.589197
8.883519	593.112880	10.594215
9.011759	580.006970	10.599232
9.114040	585.533343	10.604250
8.813971	579.004184	10.609267
9.204094	592.686359	10.614285
8.922052	601.201966	10.619303
9.156251	608.450370	10.624320
9.044522	605.420511	10.629338
9.291477	610.540594	10.634355
9.524426	605.988013	10.639373
9.053038	612.847246	10.644391
9.262965	614.194857	10.649408
9.277673	616.415400	10.654426
9.233582	614.728320	10.659443
9.259865	612.149693	10.664461
9.065399	600.717351	10.669479
9.161243	606.441241	10.674496
9.136790	604.618429	10.679514
9.341869	620.637298	10.684531
9.623533	603.105241	10.689549
9.125061	604.820775	10.694567
9.324562	601.263240	10.699584
9.199163	604.933330	10.704602
9.052068	615.359623	10.709619
9.300933	607.712129	10.714637
9.245979	611.336852	10.719655
9.213810	611.970041	10.724672
9.561112	607.091391	10.729690
9.515983	619.716501	10.734707
9.284441	615.094285	10.739725
9.337610	619.233672	10.744743
9.278442	613.638590	10.749760
9.845587	614.210940	10.754778
9.338872	602.617128	10.759795
9.352413	598.643690	10.764813
9.538984	595.251284	10.769831
9.490400	590.817347	10.774848
9.362131	585.139675	10.779866
9.096103	585.952471	10.784883
9.228475	593.977179	10.789901
9.159126	607.310184	10.794919
9.113060	614.667376	10.799936
9.072069	613.379551	10.804954
9.045296	617.938491	10.809971
9.215399	612.426551	10.814989
9.175865	616.573669	10.820007
9.170409	607.624463	10.825024
9.413443	616.456312	10.830042
9.580291	636.259000	10.835059
9.671149	630.746841	10.840077
9.442568	621.957342	10.845095
9.603581	617.159845	10.850112
9.815847	608.912775	10.855130
9.496396	616.781906	10.860147
9.613412	618.453204	10.865165
9.680408	617.885361	10.870183
9.578779	610.698650	10.875200
9.692637	603.142491	10.880218
9.651869	612.344909	10.885235
9.704407	611.708019	10.890253
9.321656	617.074886	10.895271
9.441286	604.594154	10.900288
9.792511	610.971406	10.905306
9.562357	609.341039	10.910323
9.350361	607.269107	10.915341
9.793255	623.803326	10.920359
9.610851	630.719446	10.925376
9.594118	633.123352	10.930394
9.535035	648.100222	10.935411
9.819867	639.145263	10.940429
9.916072	644.641961	10.945447
9.756520	633.494515	10.950464
9.883507	617.828751	10.955482
9.652939	622.558563	10.960499
9.519129	611.900318	10.965517
9.813235	623.608092	10.970535
9.835346	647.096956	10.975552
10.035990	630.026527	10.980570
9.523700	627.515767	10.985587
9.517407	625.249024	10.990605
9.896048	640.088567	10.995623
9.792776	639.212044	11.000640
10.048621	642.965809	11.005658
10.160098	635.832831	11.010675
9.926191	619.186781	11.015693
9.591811	618.462838	11.020711
9.468740	624.655764	11.025728
10.071425	626.160123	11.030746
9.635374	637.759173	11.035763
9.723124	649.059372	11.040781
9.978699	645.258863	11.045799
10.081208	643.433446	11.050816
10.113903	639.101724	11.055834
9.955351	644.273867	11.060851
9.747937	637.490129	11.065869
9.737747	646.222561	11.070887
9.874665	642.263444	11.075904
10.110432	637.264948	11.080922
10.217028	638.165011	11.085939
9.983275	631.795069	11.090957
10.065259	628.583807	11.095975
9.783680	625.247951	11.100992
10.295148	627.695743	11.106010
10.084646	628.136939	11.111027
9.730109	612.729943	11.116045
9.925968	619.469414	11.121063
9.656279	636.337820	11.126080
9.926708	637.103573	11.131098
10.104359	646.907647	11.136115
10.005543	636.096336	11.141133
10.188904	640.434150	11.146151
9.945826	647.238718	11.151168
10.237599	638.913657	11.156186
10.261351	645.266819	11.161203
9.969654	640.701244	11.166221
10.326989	641.960778	11.171239
10.006393	649.333896	11.176256
9.867484	645.125964	11.181274
9.911482	649.147601	11.186291
10.018685	651.357696	11.191309
10.240691	635.042510	11.196327
9.763917	639.229833	11.201344
9.984343	635.500716	11.206362
9.763634	652.681642	11.211379
9.890560	650.485068	11.216397
10.120873	641.010865	11.221415
9.805721	657.015661	11.226432
10.343617	666.237469	11.231450
10.516563	671.388376	11.236467
10.249208	679.303600	11.241485
10.336995	671.758630	11.246503
10.394617	672.972323	11.251520
10.585816	659.065981	11.256538
10.026257	657.152002	11.261555
10.380235	653.307776	11.266573
10.324365	646.855509	11.271591
9.908469	656.258680	11.276608
10.248649	665.995991	11.281626
10.318332	675.369640	11.286643
10.318715	675.408687	11.291661
10.489448	674.038818	11.296679
10.404456	675.085483	11.301696
10.315923	674.807643	11.306714
10.264658	672.207450	11.311731
10.602967	669.810200	11.316749
10.595549	669.885187	11.321767
10.745998	679.821352	11.326784
10.417928	657.751178	11.331802
10.244508	649.142834	11.336819
10.187740	660.294242	11.341837
10.448821	671.083007	11.346855
10.422173	672.904755	11.351872
10.516050	674.284850	11.356890
10.472719	683.229488	11.361907
10.293408	676.540463	11.366925
10.749670	686.199442	11.371943
10.195317	686.268889	11.376960
10.388341	678.197015	11.381978
10.489298	668.530731	11.386995
10.484043	678.068400	11.392013
10.771716	674.046227	11.397031
10.625056	684.448677	11.402048
10.464336	675.706131	11.407066
10.571498	669.697979	11.412083
10.444071	676.438458	11.417101
10.649978	665.088326	11.422119
10.259495	668.472400	11.427136
10.411418	678.086888	11.432154
10.452995	664.756156	11.437171
10.595363	676.426597	11.442189
10.775188	673.066396	11.447207
10.400968	685.567337	11.452224
10.329079	679.500564	11.457242
10.516615	674.328788	11.462259
10.393517	682.791054	11.467277
10.659654	689.741691	11.472295
10.951537	699.405758	11.477312
11.080077	689.988400	11.482330
11.008608	685.513952	11.487347
10.452749	683.405865	11.492365
10.805605	678.395768	11.497383
10.678519	675.702477	11.502400
10.666547	676.624808	11.507418
10.512563	679.652079	11.512435
10.724837	694.963192	11.517453
10.973660	690.249495	11.522471
10.974196	706.935671	11.527488
10.777793	700.345532	11.532506
10.952807	695.357707	11.537523
10.607799	677.928941	11.542541
10.972449	691.676653	11.547559
10.860958	696.883114	11.552576
10.937955	697.406633	11.557594
10.877851	708.197437	11.562611
10.876846	703.013687	11.567629
11.127014	692.121300	11.572647
10.875962	680.431198	11.577664
10.881411	679.482669	11.582682
11.133423	682.038748	11.587699
11.233499	687.085640	11.592717
10.815587	679.477096	11.597735
10.591288	675.343186	11.602752
10.735628	693.579732	11.607770
11.012166	705.793009	11.612787
11.106779	708.287663	11.617805
11.459696	697.456141	11.622823
10.841814	685.812443	11.627840
10.771504	680.854966	11.632858
11.066798	687.262215	11.637875
10.437184	699.128308	11.642893
10.635552	708.119000	11.647911
10.703427	706.856966	11.652928
11.374539	712.021139	11.657946
11.012420	707.458982	11.662963
10.871496	718.406129	11.667981
11.137495	708.688374	11.672999
11.195922	710.913277	11.678016
11.065463	709.825734	11.683034
11.267400	706.084713	11.688051
11.139081	716.724275	11.693069
11.134493	708.370688	11.698087
11.340507	708.963307	11.703104
11.099884	701.534716	11.708122
11.597999	706.384755	11.713139
11.131890	715.428029	11.718157
11.248335	698.539225	11.723175
10.973123	707.848773	11.728192
10.748812	699.274251	11.733210
11.528366	699.692410	11.738227
11.007121	712.335912	11.743245
11.294606	707.008940	11.748263
11.227411	710.071590	11.753280
11.116442	710.665130	11.758298
10.981581	707.647953	11.763315
10.968248	719.870646	11.768333
11.619499	728.693364	11.773351
11.683600	724.549690	11.778368
11.630261	722.860986	11.783386
11.512563	707.853275	11.788403
11.252939	711.378981	11.793421
11.501120	712.414950	11.798439
11.213128	713.697904	11.803456
11.378141	708.894990	11.808474
11.450607	703.223670	11.813491
11.696110	704.816144	11.818509
11.439048	709.873788	11.823527
11.075070	706.537438	11.828544
10.996840	710.076886	11.833562
11.323677	707.546508	11.838579
11.329590	723.093114	11.843597
11.347364	723.535540	11.848615
11.543278	726.372388	11.853632
11.692666	736.326482	11.858650
11.780559	732.442021	11.863667
11.624135	728.336380	11.868685
11.994464	716.284718	11.873703
11.325222	712.388129	11.878720
10.790343	717.982270	11.883738
11.327086	720.993747	11.888755
11.182607	726.498395	11.893773
11.306408	725.218404	11.898791
11.106284	728.724185	11.903808
11.149394	732.817836	11.908826
11.227353	738.251463	11.913843
11.613456	755.485764	11.918861
11.862262	756.850152	11.923879
12.078967	762.265844	11.928896
11.849114	739.790869	11.933914
11.678011	730.854953	11.938931
11.642577	734.204827	11.943949
11.425640	737.067980	11.948967
11.630036	731.194419	11.953984
11.448183	755.426351	11.959002
11.981414	758.348663	11.964019
12.064322	762.973070	11.969037
11.895773	750.804865	11.974055
11.852052	734.861080	11.979072
11.658811	733.988877	11.984090
11.698468	728.345637	11.989107
11.985991	743.344115	11.994125
11.959426	730.070319	11.999143
11.828634	735.538053	12.004160
11.690672	731.487408	12.009178
11.771891	726.887379	12.014195
11.735773	733.502085	12.019213
11.784091	748.177756	12.024231
11.948227	757.761328	12.029248
11.735157	757.948839	12.034266
11.631493	762.443443	12.039283
11.929072	757.747998	12.044301
11.601761	755.543255	12.049319
11.669511	749.057013	12.054336
11.640529	767.790335	12.059354
11.753599	747.417447	12.064371
11.805368	765.781268	12.069389
11.955788	752.832143	12.074407
11.935570	760.516185	12.079424
11.876229	753.908557	12.084442
11.873594	756.290456	12.089459
11.803872	757.766643	12.094477
12.023202	777.676922	12.099495
12.048965	786.396961	12.104512
12.000546	784.896592	12.109530
12.125310	783.112928	12.114547
12.211259	785.360234	12.119565
12.014137	784.315260	12.124583
12.219162	791.185753	12.129600
12.215597	776.503863	12.134618
12.162052	768.120194	12.139635
12.048185	760.045945	12.144653
12.051121	757.491449	12.149671
12.391848	775.003766	12.154688
12.206987	767.803063	12.159706
12.312148	762.597906	12.164723
12.386315	752.758870	12.169741
11.851550	764.226006	12.174759
11.971374	767.060943	12.179776
11.988609	780.103149	12.184794
12.372550	791.061131	12.189811
12.164162	796.576033	12.194829
12.536077	796.136033	12.199847
12.649711	784.781467	12.204864
12.051871	771.745887	12.209882
12.097538	773.559367	12.214899
11.967316	784.532733	12.219917
11.888923	786.726258	12.224935
12.493744	789.466019	12.229952
12.185864	789.029964	12.234970
12.358440	789.966506	12.239987
12.093070	784.043655	12.245005
12.279135	792.250473	12.250023
12.243720	790.474733	12.255040
12.285907	793.419620	12.260058
12.287049	788.485663	12.265075
12.369494	795.405861	12.270093
12.770050	788.833775	12.275111
12.203719	784.429743	12.280128
12.284108	793.508790	12.285146
12.479844	780.374564	12.290163
12.594282	790.414417	12.295181
12.502272	792.855268	12.300199
12.659343	787.983970	12.305216
12.539781	792.359974	12.310234
13.057926	787.887682	12.315251
12.646553	797.754721	12.320269
12.521052	791.064576	12.325287
12.575614	788.635539	12.330304
12.546854	798.115382	12.335322
12.457330	792.968951	12.340339
12.500686	796.371486	12.345357
12.620393	786.963017	12.350375
12.692191	782.623968	12.355392
12.607282	788.001619	12.360410
12.622046	776.125343	12.365427
12.539710	790.024008	12.370445
12.433774	787.449614	12.375463
12.438108	787.872624	12.380480
12.635375	809.045183	12.385498
13.197535	800.307403	12.390515
12.939209	797.722709	12.395533
12.366556	798.437673	12.400551
12.815531	797.488836	12.405568
12.525158	805.241425	12.410586
12.901637	816.997855	12.415603
12.986577	819.817931	12.420621
13.007925	811.978446	12.425639
12.786118	797.057436	12.430656
12.504024	786.534931	12.435674
12.817794	808.903590	12.440691
13.329664	807.252417	12.445709
12.630452	804.488857	12.450727
12.672970	801.198495	12.455744
12.776013	819.905801	12.460762
12.759741	818.744747	12.465779
12.679089	826.908521	12.470797
12.513826	820.906422	12.475815
13.008251	826.257275	12.480832
12.827197	828.574359	12.485850
12.637226	825.931058	12.490867
12.956092	825.928192	12.495885
12.835678	824.270506	12.500903
12.876963	824.123240	12.505920
13.170029	832.955951	12.510938
13.234035	825.136926	12.515955
13.013582	823.770062	12.520973
12.903077	826.524798	12.525991
13.278637	819.927525	12.531008
13.274035	826.563802	12.536026
12.950870	824.126092	12.541043
13.044008	827.583347	12.546061
12.806661	824.105853	12.551079
12.953251	822.375048	12.556096
13.145445	833.718845	12.561114
12.825995	835.843200	12.566131
13.304943	820.694281	12.571149
12.978020	821.083382	12.576167
12.957143	818.299779	12.581184
13.082385	832.672213	12.586202
13.125233	844.807325	12.591219
13.497543	848.867941	12.596237
13.062497	845.235126	12.601255
13.442161	844.522792	12.606272
13.528276	846.838381	12.611290
13.311116	832.519478	12.616307
13.301402	822.376842	12.621325
13.068943	827.099550	12.626343
13.201947	815.061080	12.631360
13.458452	839.161034	12.636378
13.241603	844.753929	12.641395
13.521265	841.411741	12.646413
13.171519	839.754379	12.651431
13.611628	841.093474	12.656448
13.647793	846.793124	12.661466
13.233569	832.314075	12.666483
13.209643	831.283811	12.671501
13.370103	835.611708	12.676519
13.501630	835.684465	12.681536
13.205863	850.016468	12.686554
13.142303	854.576277	12.691571
13.642884	850.922188	12.696589
13.629285	845.391884	12.701607
13.894225	842.061985	12.706624
13.648200	844.724494	12.711642
13.352418	848.251122	12.716659
13.820621	843.332422	12.721677
13.439073	844.951780	12.726695
13.494834	847.714315	12.731712
13.375108	844.694202	12.736730
13.355312	845.049575	12.741747
13.412569	844.270956	12.746765
13.776816	861.823160	12.751783
13.709322	841.132547	12.756800
13.638368	845.747516	12.761818
13.510056	845.545375	12.766835
13.475250	839.980411	12.771853
13.726722	838.583133	12.776871
13.768236	850.828897	12.781888
13.397367	832.128553	12.786906
13.484144	850.320328	12.791923
13.807453	846.454186	12.796941
13.559758	846.870272	12.801959
13.480769	842.322427	12.806976
13.821551	846.380213	12.811994
13.369692	856.117413	12.817011
13.878003	842.344604	12.822029
13.707082	845.231227	12.827047
13.526231	844.055601	12.832064
13.660988	857.706839	12.837082
13.972725	871.376111	12.842099
14.125558	871.016615	12.847117
14.031178	869.404988	12.852135
13.804167	858.544362	12.857152
13.835476	851.218718	12.862170
13.846128	864.999442	12.867187
14.307907	870.773230	12.872205
14.179124	849.306229	12.877223
14.200834	841.237550	12.882240
14.274860	830.975485	12.887258
14.202026	834.299906	12.892275
14.291160	834.270269	12.897293
14.088999	839.901663	12.902311
14.012296	832.526860	12.907328
14.285963	838.906273	12.912346
14.157827	837.799242	12.917363
14.373807	831.258605	12.922381
14.085300	842.869500	12.927399
13.920260	837.801743	12.932416
14.032426	838.865054	12.937434
14.025481	834.718004	12.942451
14.230628	832.807398	12.947469
14.049257	838.469586	12.952487
13.914045	831.841073	12.957504
14.400931	836.518229	12.962522
13.814029	847.032149	12.967539
13.955171	840.498830	12.972557
13.736110	840.843429	12.977575
13.927259	841.669808	12.982592
14.164319	837.904415	12.987610
14.264866	866.764269	12.992627
14.607878	869.036768	12.997645
14.358216	854.914572	13.002663
14.393948	841.204960	13.007680
14.488791	839.215057	13.012698
14.305115	840.088581	13.017715
14.209350	822.101526	13.022733
14.398118	830.675607	13.027751
14.351795	834.916623	13.032768
14.664817	829.123388	13.037786
14.337102	831.663262	13.042803
14.427261	830.080803	13.047821
14.268665	824.803332	13.052839
14.475782	835.195896	13.057856
14.466867	831.805225	13.062874
14.075321	832.964858	13.067891
14.217544	851.229893	13.072909
14.272245	867.063397	13.077927
14.480082	867.447071	13.082944
14.726333	864.090354	13.087962
14.551355	867.709498	13.092979
14.480894	863.615711	13.097997
14.416688	865.968887	13.103015
14.307796	869.146760	13.108032
14.722785	856.318327	13.113050
14.533760	865.933701	13.118067
14.865636	857.690041	13.123085
14.800108	874.468279	13.128103
14.617221	873.190633	13.133120
14.759873	871.058929	13.138138
14.378936	870.475577	13.143155
14.785262	862.811824	13.148173
14.542516	865.919038	13.153191
14.466787	873.310415	13.158208
14.718979	871.780149	13.163226
14.592765	868.715640	13.168243
14.790313	866.216174	13.173261
14.801363	872.387694	13.178279
14.550262	871.591828	13.183296
15.029175	867.650017	13.188314
14.998230	860.055994	13.193331
14.558545	865.995561	13.198349
14.796777	869.055505	13.203367
14.454434	855.859283	13.208384
14.881513	867.072533	13.213402
14.542334	871.376802	13.218419
14.274242	863.202157	13.223437
14.635797	879.101984	13.228455
14.814804	894.822932	13.233472
14.901771	893.617745	13.238490
14.828056	904.009792	13.243507
15.160327	895.487915	13.248525
15.056276	894.832163	13.253543
14.803228	897.622218	13.258560
14.907927	892.800928	13.263578
14.555143	902.748840	13.268595
14.661883	893.561739	13.273613
14.949884	889.689448	13.278631
14.905662	897.117329	13.283648
15.065785	894.949649	13.288666
14.864800	897.206281	13.293683
14.929837	890.690511	13.298701
15.282886	908.333994	13.303719
15.453573	918.189396	13.308736
15.526784	902.474412	13.313754
15.406265	914.667833	13.318771
15.309425	898.627597	13.323789
15.353209	898.516921	13.328807
15.001462	896.700447	13.333824
15.148409	897.936316	13.338842
15.049491	900.968058	13.343859
15.469642	896.884442	13.348877
15.426019	894.486472	13.353895
15.449471	903.204993	13.358912
15.159603	894.581421	13.363930
15.208669	898.888089	13.368947
15.225388	904.113464	13.373965
15.388703	891.060118	13.378983
15.212083	901.623588	13.384000
15.535565	890.813950	13.389018
15.214882	901.807246	13.394035
15.308371	896.453206	13.399053
15.703340	890.712859	13.404071
15.216470	902.532152	13.409088
15.384304	890.911036	13.414106
15.393059	894.509095	13.419123
15.427050	913.056743	13.424141
15.752084	911.361619	13.429159
15.323272	904.645270	13.434176
15.746932	903.525448	13.439194
15.618223	906.788508	13.444211
15.526811	894.944354	13.449229
15.847701	890.929597	13.454247
15.494621	902.597133	13.459264
15.855245	893.476094	13.464282
15.353429	903.734980	13.469299
15.507524	898.916894	13.474317
15.672567	896.304331	13.479335
15.620297	896.814699	13.484352
15.651832	891.694567	13.489370
15.280949	902.946192	13.494387
15.562153	918.293506	13.499405
15.935351	919.742149	13.504423
15.783802	930.856555	13.509440
15.989711	920.468776	13.514458
15.599914	921.521438	13.519475
16.003140	922.381268	13.524493
15.860073	906.949457	13.529511
15.888353	895.932206	13.534528
15.699324	892.175028	13.539546
15.492624	899.903915	13.544563
15.776510	918.512782	13.549581
15.923238	919.762468	13.554599
15.817664	926.190781	13.559616
15.831160	917.828170	13.564634
15.821031	931.563395	13.569651
16.056707	919.708947	13.574669
16.156910	927.115593	13.579687
16.112279	926.561372	13.584704
16.298372	918.171253	13.589722
16.016678	913.084675	13.594739
16.137092	901.971401	13.599757
16.054789	898.301594	13.604775
15.883918	897.288073	13.609792
16.058463	898.750837	13.614810
15.953646	903.713753	13.619827
15.897906	916.171588	13.624845
16.148356	917.602840	13.629863
16.019845	915.787051	13.634880
16.376714	921.276346	13.639898
16.338794	923.295260	13.644915
16.114792	920.930417	13.649933
16.248851	921.947578	13.654951
15.718194	926.854125	13.659968
16.034222	922.879929	13.664986
15.864933	915.011058	13.670003
15.649604	920.526567	13.675021
15.968966	910.225443	13.680039
15.855295	913.953691	13.685056
16.171016	920.637546	13.690074
16.306682	920.493882	13.695091
16.221598	939.191660	13.700109
16.427563	944.326541	13.705127
16.425994	943.500611	13.710144
16.836682	938.152886	13.715162
16.677902	920.092338	13.720179
16.550570	930.503944	13.725197
16.506898	919.580520	13.730215
16.272947	922.734311	13.735232
16.290058	914.625809	13.740250
16.518994	920.308405	13.745267
16.286835	912.148823	13.750285
16.627430	913.949319	13.755303
16.573486	915.723274	13.760320
16.644839	915.564317	13.765338
16.534380	918.565306	13.770355
16.327844	923.178623	13.775373
16.624146	918.836864	13.780391
16.458605	921.849371	13.785408
16.671083	922.211018	13.790426
16.594284	919.439054	13.795443
16.073700	930.740383	13.800461
16.538379	934.039061	13.805479
16.422717	949.699995	13.810496
16.782653	939.397225	13.815514
16.630561	944.644766	13.820531
16.413502	945.136861	13.825549
16.880459	944.984978	13.830567
17.075040	942.526936	13.835584
16.676242	953.709620	13.840602
16.687733	955.708909	13.845619
16.814365	955.878145	13.850637
16.915051	954.590363	13.855655
17.016794	950.109291	13.860672
16.619519	953.252836	13.865690
16.818572	947.839109	13.870707
16.798592	954.525237	13.875725
17.121584	946.372963	13.880743
16.454849	947.566141	13.885760
16.669674	952.335794	13.890778
16.927960	940.620871	13.895795
16.585127	947.588992	13.900813
16.842023	939.254806	13.905831
16.791450	951.207116	13.910848
16.609241	954.633005	13.915866
16.892938	966.522680	13.920883
16.984477	980.050903	13.925901
17.121990	967.554112	13.930919
17.192422	968.792469	13.935936
17.285901	979.698871	13.940954
17.136233	960.253771	13.945971
16.928564	973.906914	13.950989
17.501494	964.160029	13.956007
17.530586	956.053057	13.961024
16.989692	952.896837	13.966042
17.163068	941.162958	13.971059
16.789626	944.820619	13.976077
17.419980	953.807561	13.981095
17.255766	971.689053	13.986112
17.585660	959.131554	13.991130
17.616419	946.270263	13.996147
16.926244	946.030415	14.001165
17.181207	930.433609	14.006183
17.218824	946.993416	14.011200
17.370829	964.137341	14.016218
17.392076	959.635789	14.021235
17.255824	978.783825	14.026253
17.170032	966.386747	14.031271
17.443276	966.725696	14.036288
17.761995	974.286190	14.041306
17.880321	964.427082	14.046323
17.546547	951.614174	14.051341
17.774070	946.700410	14.056359
17.490780	944.027326	14.061376
17.751430	939.881239	14.066394
17.513637	927.833452	14.071411
17.631807	939.231360	14.076429
17.612909	940.136553	14.081447
17.580420	938.067020	14.086464
17.401977	932.599516	14.091482
17.706258	926.044359	14.096499
17.487248	936.814493	14.101517
17.427338	931.383977	14.106535
17.303236	936.264288	14.111552
17.570578	952.871344	14.116570
17.904618	956.964530	14.121587
17.668321	966.219145	14.126605
17.555031	960.767571	14.131623
17.521177	956.625552	14.136640
17.793283	966.970790	14.141658
17.993809	957.418083	14.146675
17.833780	974.052500	14.151693
17.978455	966.630994	14.156711
17.793595	966.427227	14.161728
17.863251	973.298846	14.166746
17.924584	972.080199	14.171763
17.974211	974.901056	14.176781
17.826427	966.932133	14.181799
17.921131	970.887556	14.186816
17.904370	976.200798	14.191834
17.813034	974.431970	14.196851
17.510345	979.175452	14.201869
17.834050	968.032277	14.206887
17.797219	961.712140	14.211904
18.055319	970.666878	14.216922
18.255115	969.544500	14.221939
17.909811	972.607762	14.226957
17.589018	978.347895	14.231975
17.798115	974.917020	14.236992
17.696279	979.183836	14.242010
18.063881	969.053384	14.247027
17.878181	973.306187	14.252045
18.104769	992.423457	14.257063
18.368725	995.372070	14.262080
17.945936	1003.724687	14.267098
18.402245	998.373295	14.272115
18.510862	1003.544454	14.277133
18.099098	982.771709	14.282151
18.271722	977.592666	14.287168
18.601154	980.707154	14.292186
18.396953	966.171615	14.297203
18.353385	969.103231	14.302221
17.758815	960.958195	14.307239
18.165314	973.108943	14.312256
17.855066	989.941563	14.317274
18.661917	992.683409	14.322291
18.340590	999.229105	14.327309
18.395434	993.827522	14.332327
18.529153	990.267054	14.337344
18.313478	988.657465	14.342362
18.456836	999.157582	14.347379
18.524711	992.485007	14.352397
18.591192	992.384337	14.357415
18.689249	989.029785	14.362432
18.822695	993.527561	14.367450
18.835467	991.037924	14.372467
18.675994	988.993427	14.377485
18.923210	994.376179	14.382503
18.759063	979.030078	14.387520
18.675227	982.139640	14.392538
18.919369	961.922036	14.397555
18.841067	962.380438	14.402573
18.635879	969.723304	14.407591
18.702223	958.364661	14.412608
18.474430	958.871925	14.417626
18.843097	949.359776	14.422643
18.560690	959.678680	14.427661
18.493558	969.648836	14.432679
18.681961	978.782476	14.437696
18.724105	980.202691	14.442714
18.970282	981.425223	14.447731
18.984415	983.563045	14.452749
18.904008	985.618556	14.457767
19.043032	981.026559	14.462784
18.885170	996.289853	14.467802
18.947827	987.649363	14.472819
18.848388	986.690889	14.477837
18.981406	983.238013	14.482855
18.827489	988.381548	14.487872
18.736854	989.372286	14.492890
18.675691	980.106355	14.497907
19.034215	984.369091	14.502925
18.662038	982.284364	14.507943
18.613391	982.081182	14.512960
18.674883	989.221080	14.517978
19.063676	993.487054	14.522995
19.268823	1001.775847	14.528013
19.090863	1010.224774	14.533031
19.114968	1002.668182	14.538048
19.084395	1021.581396	14.543066
19.098575	1003.901821	14.548083
19.122949	1015.683071	14.553101
19.162022	1020.800445	14.558119
19.781191	1011.395038	14.563136
19.518336	1023.937776	14.568154
19.470581	1001.362865	14.573171
18.934786	990.471585	14.578189
19.123848	1013.258294	14.583207
19.438116	1012.596781	14.588224
19.046295	1025.303468	14.593242
19.276543	1018.494844	14.598259
19.361134	1021.211872	14.603277
18.894156	1020.710921	14.608295
19.464820	1021.095707	14.613312
19.285282	1016.010223	14.618330
19.552968	1014.584449	14.623347
19.359191	1014.193197	14.628365
19.327824	1025.391627	14.633383
19.330904	1021.343051	14.638400
19.095340	1029.484258	14.643418
19.524711	1030.873578	14.648435
19.874906	1040.114607	14.653453
19.774165	1041.129466	14.658471
19.640144	1019.949108	14.663488
19.329088	1028.447724	14.668506
19.845526	1034.554596	14.673523
19.773803	1038.420776	14.678541
19.883340	1026.592331	14.683559
20.066351	1015.870124	14.688576
19.666691	1009.557914	14.693594
19.803481	1015.040519	14.698611
19.962408	1016.922402	14.703629
19.728411	1007.398190	14.708647
19.939303	1006.666464	14.713664
19.750212	1008.409745	14.718682
19.753532	1012.598072	14.723699
19.844161	1009.353013	14.728717
19.807587	1016.019880	14.733735
19.994326	1025.765995	14.738752
19.930456	1021.556116	14.743770
19.985456	1028.022739	14.748787
19.887738	1021.907962	14.753805
19.894633	1037.878123	14.758823
19.493583	1032.080281	14.763840
20.135307	1035.321209	14.768858
19.969372	1031.918801	14.773875
20.233703	1036.851109	14.778893
20.413283	1042.475421	14.783911
20.480779	1037.015424	14.788928
20.323667	1036.488556	14.793946
20.172318	1030.414972	14.798963
20.328287	1020.853491	14.803981
19.961480	1014.767696	14.808999
20.196602	1019.047016	14.814016
20.136515	1031.400554	14.819034
20.090341	1038.279644	14.824051
20.113452	1034.458826	14.829069
20.406630	1038.362774	14.834087
20.166797	1033.540442	14.839104
20.283845	1038.679112	14.844122
20.326359	1044.315578	14.849139
20.472487	1036.288712	14.854157
20.082974	1036.895689	14.859175
19.930464	1033.855201	14.864192
20.507937	1030.297340	14.869210
20.239930	1032.491119	14.874227
20.179980	1031.896530	14.879245
19.961150	1022.324122	14.884263
20.443153	1027.737541	14.889280
20.083506	1047.747945	14.894298
20.086345	1058.717497	14.899315
20.377726	1053.560421	14.904333
20.581247	1063.360460	14.909351
20.635918	1062.362193	14.914368
20.839445	1053.362836	14.919386
20.930297	1052.010150	14.924403
21.042447	1044.185373	14.929421
20.864459	1053.629156	14.934439
20.934311	1056.066372	14.939456
20.997829	1047.396967	14.944474
20.689755	1033.537255	14.949491
20.974467	1015.554448	14.954509
20.642163	1028.215419	14.959527
20.750153	1031.788748	14.964544
20.794623	1045.292571	14.969562
20.905199	1048.771385	14.974579
21.085456	1042.541502	14.979597
20.898041	1038.558836	14.984615
20.668811	1032.959194	14.989632
20.801264	1043.102510	14.994650
21.220302	1049.007086	14.999667
21.539008	1042.582153	15.004685
20.708516	1033.243680	15.009703
20.884726	1029.961559	15.014720
21.199604	1036.342472	15.019738
20.889338	1041.728929	15.024755
20.728393	1040.956649	15.029773
20.824955	1053.884922	15.034791
20.961756	1047.885870	15.039808
21.103271	1050.670210	15.044826
21.039162	1051.281365	15.049843
21.054201	1048.224049	15.054861
20.870772	1043.617130	15.059879
21.007780	1036.668099	15.064896
21.427613	1042.961102	15.069914
20.920495	1046.577229	15.074931
21.209615	1037.521137	15.079949
21.049476	1055.276071	15.084967
21.251740	1056.470477	15.089984
21.501488	1068.851675	15.095002
21.385024	1073.302041	15.100019
21.656674	1056.000456	15.105037
21.328538	1051.833707	15.110055
21.377170	1052.979243	15.115072
21.850209	1045.862156	15.120090
21.223771	1041.073374	15.125107
21.537951	1034.181112	15.130125
21.318715	1050.383350	15.135143
21.361205	1066.568873	15.140160
21.577032	1074.287849	15.145178
21.856381	1074.943094	15.150195
22.131012	1072.555580	15.155213
21.803073	1058.214134	15.160231
21.817958	1041.376087	15.165248
21.585363	1039.916935	15.170266
21.451361	1043.867479	15.175283
21.836465	1035.577676	15.180301
21.659020	1046.108313	15.185319
21.737933	1047.875160	15.190336
21.481663	1043.748039	15.195354
21.408314	1049.122678	15.200371
21.577991	1062.108487	15.205389
21.674665	1067.222601	15.210407
21.497139	1079.150838	15.215424
21.708536	1072.879548	15.220442
21.610230	1084.535580	15.225459
21.982349	1069.802581	15.230477
21.826195	1079.605724	15.235495
21.883743	1078.072360	15.240512
22.205290	1071.484746	15.245530
22.148659	1074.461465	15.250547
22.002042	1073.636017	15.255565
21.727632	1075.971804	15.260583
21.683620	1073.205386	15.265600
22.064342	1061.362546	15.270618
21.968767	1081.620031	15.275635
21.751980	1079.140978	15.280653
22.003510	1084.044328	15.285671
22.132719	1108.343411	15.290688
22.575184	1099.140542	15.295706
22.468516	1088.110152	15.300723
22.582227	1081.108284	15.305741
22.231990	1068.063381	15.310759
22.210537	1066.151044	15.315776
22.525622	1059.800718	15.320794
22.355393	1071.183276	15.325811
22.574184	1059.442546	15.330829
22.301026	1059.243218	15.335847
22.480005	1068.011174	15.340864
22.547003	1061.715468	15.345882
22.091507	1068.329947	15.350899
22.503378	1061.210423	15.355917
22.469047	1072.121599	15.360935
22.279239	1058.703600	15.365952
22.476654	1057.693812	15.370970
22.468984	1072.163360	15.375987
22.299444	1059.569113	15.381005
22.405867	1074.118513	15.386023
22.781415	1088.591306	15.391040
22.979345	1084.253254	15.396058
22.967049	1076.110975	15.401075
22.910858	1061.538933	15.406093
22.817962	1065.633430	15.411111
22.931838	1059.654325	15.416128
23.119086	1058.761181	15.421146
22.649379	1056.011194	15.426163
22.600144	1052.875983	15.431181
22.766428	1049.029001	15.436199
22.572257	1060.057283	15.441216
22.904016	1059.659383	15.446234
22.843740	1059.556553	15.451251
22.643224	1062.999288	15.456269
22.781945	1054.731137	15.461287
22.783389	1063.991961	15.466304
23.207642	1069.007929	15.471322
23.095661	1065.709137	15.476339
23.015696	1061.678291	15.481357
22.789050	1069.357431	15.486375
23.071830	1084.246405	15.491392
23.319825	1082.405022	15.496410
23.261196	1081.718090	15.501427
23.189608	1064.357411	15.506445
23.237677	1065.718778	15.511463
23.030736	1062.653082	15.516480
23.096426	1063.433204	15.521498
22.823369	1062.125256	15.526515
23.476536	1076.712516	15.531533
23.491199	1085.691643	15.536551
23.225249	1071.702460	15.541568
23.057670	1067.282259	15.546586
23.219778	1075.177873	15.551603
23.275308	1088.168110	15.556621
23.480152	1085.777234	15.561639
23.398064	1091.330890	15.566656
23.505453	1096.138524	15.571674
23.357429	1093.303568	15.576691
23.475435	1096.037101	15.581709
23.612286	1092.196183	15.586727
23.348607	1100.245254	15.591744
23.614757	1090.644945	15.596762
23.536264	1096.486968	15.601779
23.752879	1094.415377	15.606797
23.717919	1093.857575	15.611815
23.400619	1103.843809	15.616832
23.688060	1088.102478	15.621850
23.482155	1093.020449	15.626867
23.677137	1089.965497	15.631885
23.732231	1099.476073	15.636903
23.450542	1098.503004	15.641920
23.803765	1080.237488	15.646938
23.849617	1081.455138	15.651955
23.652026	1085.241468	15.656973
23.895159	1087.903418	15.661991
23.628308	1093.114182	15.667008
23.448938	1088.723099	15.672026
23.516942	1090.457513	15.677043
23.387077	1084.952354	15.682061
23.627948	1088.810681	15.687079
23.851387	1099.651081	15.692096
23.981967	1109.133763	15.697114
23.782950	1110.622419	15.702131
24.042167	1107.068229	15.707149
24.192752	1109.491641	15.712167
23.935203	1117.489704	15.717184
24.100760	1099.139223	15.722202
23.988996	1114.620156	15.727219
24.115941	1114.322436	15.732237
24.002281	1117.706260	15.737255
24.269668	1118.019418	15.742272
24.228370	1106.361251	15.747290
23.917271	1105.038757	15.752307
23.946678	1111.744695	15.757325
24.204246	1108.778939	15.762343
24.150816	1109.132822	15.767360
24.158969	1112.686546	15.772378
24.155593	1130.524560	15.777395
24.137064	1143.292519	15.782413
24.534995	1137.871653	15.787431
24.557480	1133.406063	15.792448
24.893562	1130.604016	15.797466
24.931291	1126.930738	15.802483
24.531827	1106.608120	15.807501
24.558716	1108.848559	15.812519
24.439855	1101.639287	15.817536
24.405244	1102.463640	15.822554
24.655683	1108.389176	15.827571
24.657948	1110.353800	15.832589
24.792682	1100.802493	15.837607
24.628568	1110.242036	15.842624
24.899066	1097.878933	15.847642
24.460896	1106.899089	15.852659
24.742594	1122.794136	15.857677
24.856287	1119.325152	15.862695
24.856019	1116.527441	15.867712
25.049257	1118.983133	15.872730
25.010436	1106.756865	15.877747
24.657104	1099.669240	15.882765
24.840247	1100.220403	15.887783
24.559751	1111.771312	15.892800
25.089119	1122.517574	15.897818
25.235230	1125.987350	15.902835
24.991865	1127.780215	15.907853
24.980116	1111.483106	15.912871
24.936117	1110.925231	15.917888
24.893040	1128.079718	15.922906
25.101641	1133.696091	15.927923
25.106224	1129.919665	15.932941
25.472315	1126.877996	15.937959
25.015685	1125.963529	15.942976
25.327566	1126.705097	15.947994
25.026418	1120.812666	15.953011
24.990775	1133.393707	15.958029
25.247301	1124.683517	15.963047
25.217927	1131.586234	15.968064
24.852366	1127.099715	15.973082
25.208325	1128.899259	15.978099
25.300146	1132.451285	15.983117
25.351177	1128.052602	15.988135
25.008745	1133.433021	15.993152
25.450974	1125.554915	15.998170
25.511693	1131.002963	16.003187
24.972516	1132.213138	16.008205
25.474337	1130.871266	16.013223
25.187693	1136.766403	16.018240
25.651085	1143.006540	16.023258
25.968167	1156.574592	16.028275
25.638838	1139.868844	16.033293
25.968002	1131.943389	16.038311
25.539866	1134.994466	16.043328
25.396906	1138.178843	16.048346
25.755468	1134.762065	16.053363
25.606269	1149.630782	16.058381
25.778419	1155.372901	16.063399
25.986498	1159.869737	16.068416
25.804300	1151.159623	16.073434
26.263252	1140.880418	16.078451
25.789894	1138.234561	16.083469
25.643422	1124.763634	16.088487
25.684839	1136.523641	16.093504
25.651397	1150.228685	16.098522
26.216774	1150.695060	16.103539
25.706084	1154.605492	16.108557
26.321247	1141.111889	16.113575
26.073076	1148.909994	16.118592
25.930940	1151.165148	16.123610
26.556756	1149.878252	16.128627
26.123985	1150.712491	16.133645
26.235822	1142.730638	16.138663
26.004273	1156.876470	16.143680
26.088514	1149.936553	16.148698
25.828466	1152.798679	16.153715
25.928507	1160.139719	16.158733
25.897687	1154.583822	16.163751
26.063278	1163.576095	16.168768
25.747278	1158.844726	16.173786
26.240018	1164.894963	16.178803
25.921649	1183.500321	16.183821
26.417118	1189.558381	16.188839
26.460557	1189.655625	16.193856
26.312175	1184.810565	16.198874
26.816758	1181.201797	16.203891
26.739485	1175.953993	16.208909
26.990539	1167.894660	16.213927
26.925632	1153.148398	16.218944
26.573393	1148.218341	16.223962
26.974626	1136.848784	16.228979
26.516258	1145.567609	16.233997
26.539761	1142.426588	16.239015
26.685181	1148.538878	16.244032
26.590778	1142.810491	16.249050
26.646592	1138.171652	16.254067
26.848896	1148.554204	16.259085
26.887467	1135.006451	16.264103
26.639807	1128.968913	16.269120
26.939372	1137.865678	16.274138
27.110342	1135.205241	16.279155
27.055848	1141.630271	16.284173
26.814270	1138.163249	16.289191
26.931158	1140.683995	16.294208
26.975507	1137.809576	16.299226
27.026864	1139.925879	16.304243
26.866757	1143.290264	16.309261
26.874416	1138.993665	16.314279
26.741588	1138.291899	16.319296
27.153500	1146.733403	16.324314
27.381989	1157.894249	16.329331
26.973152	1159.726432	16.334349
27.074679	1155.263052	16.339367
26.878447	1166.859442	16.344384
26.975141	1168.763104	16.349402
27.364612	1171.710574	16.354419
27.183156	1184.807602	16.359437
27.160986	1174.106398	16.364455
27.134958	1173.392391	16.369472
27.319708	1168.647076	16.374490
27.442523	1171.106214	16.379507
27.226979	1170.237101	16.384525
27.219640	1180.063996	16.389543
27.231659	1172.664834	16.394560
26.963076	1175.397680	16.399578
27.293815	1190.570506	16.404595
27.804836	1196.322848	16.409613
27.892808	1195.515092	16.414631
27.730309	1194.539921	16.419648
27.597574	1186.689637	16.424666
28.095277	1182.362360	16.429683
27.807175	1182.178111	16.434701
27.432160	1175.125155	16.439719
27.380507	1178.837253	16.444736
27.782755	1185.997372	16.449754
28.052947	1197.357605	16.454771
27.878484	1196.990695	16.459789
27.764391	1201.983987	16.464807
27.765380	1199.830118	16.469824
27.936035	1207.840516	16.474842
27.812239	1187.402684	16.479859
28.063754	1198.075501	16.484877
27.963714	1194.197951	16.489895
28.132843	1195.284495	16.494912
28.135983	1191.145318	16.499930
28.167809	1205.653700	16.504947
28.011494	1205.819577	16.509965
28.215817	1195.626357	16.514983
28.359456	1196.157714	16.520000
27.844864	1199.283013	16.525018
28.218575	1192.986272	16.530035
28.228903	1203.438169	16.535053
27.826806	1197.286122	16.540071
27.894097	1198.829732	16.545088
28.039321	1197.276665	16.550106
28.098916	1193.917833	16.555123
28.274947	1195.377623	16.560141
28.172035	1190.435243	16.565159
28.145260	1194.356586	16.570176
28.007380	1208.315644	16.575194
28.389739	1216.629034	16.580211
28.586440	1218.939684	16.585229
28.695453	1218.424480	16.590247
28.671604	1212.178456	16.595264
28.435503	1221.750499	16.600282
28.709510	1220.642541	16.605299
28.896418	1219.317967	16.610317
28.811519	1218.617286	16.615335
28.883502	1215.919354	16.620352
28.756374	1214.860353	16.625370
28.924762	1217.390661	16.630387
28.811801	1213.340457	16.635405
28.729027	1209.738761	16.640423
28.740405	1217.007167	16.645440
28.977481	1214.840826	16.650458
29.047140	1220.441744	16.655475
29.201585	1212.563792	16.660493
28.951741	1197.409663	16.665511
28.975753	1196.364910	16.670528
28.745606	1215.069811	16.675546
29.077461	1205.307337	16.680563
28.752556	1218.518390	16.685581
29.084933	1208.601503	16.690599
29.266891	1205.859704	16.695616
29.045702	1211.947131	16.700634
29.148434	1213.941130	16.705651
29.342786	1217.583216	16.710669
29.234051	1213.820093	16.715687
29.228296	1209.462321	16.720704
28.822218	1212.204247	16.725722
29.002794	1210.599636	16.730739
29.160262	1219.164570	16.735757
28.679444	1211.882343	16.740775
29.273079	1222.741610	16.745792
29.415242	1231.879937	16.750810
29.640570	1229.997819	16.755827
29.644328	1229.063119	16.760845
29.733576	1236.517402	16.765863
29.797000	1226.403484	16.770880
29.677687	1232.294860	16.775898
29.649626	1217.779016	16.780915
29.746006	1211.559858	16.785933
29.717533	1219.008897	16.790951
29.686804	1212.676225	16.795968
29.647861	1228.026276	16.800986
29.865198	1229.332753	16.806003
30.033804	1224.844031	16.811021
29.875153	1219.627848	16.816039
30.064922	1202.184992	16.821056
29.596824	1206.842261	16.826074
29.574023	1218.437815	16.831091
30.021808	1221.907075	16.836109
29.785700	1232.760961	16.841127
29.987943	1222.219266	16.846144
29.832030	1234.832977	16.851162
29.491903	1220.780400	16.856179
29.779675	1232.262141	16.861197
29.575340	1226.827574	16.866215
29.938787	1237.044825	16.871232
30.120175	1246.316399	16.876250
30.246786	1260.226818	16.881267
30.256330	1262.630785	16.886285
30.459462	1259.023287	16.891303
30.547891	1247.334397	16.896320
30.773369	1237.582104	16.901338
30.671120	1232.589209	16.906355
30.222377	1225.753987	16.911373
30.292640	1226.618394	16.916391
30.151155	1222.467028	16.921408
30.316954	1243.254486	16.926426
30.236479	1233.619187	16.931443
30.807868	1252.710572	16.936461
30.535662	1235.759407	16.941479
30.660518	1241.182661	16.946496
30.584762	1254.019670	16.951514
30.560567	1248.935059	16.956531
30.277640	1251.731717	16.961549
30.142619	1262.631812	16.966567
30.575576	1252.576924	16.971584
30.554397	1259.166143	16.976602
30.331610	1261.303621	16.981619
30.831477	1252.115136	16.986637
30.656164	1256.218264	16.991655
30.792711	1259.534154	16.996672
30.679803	1261.454558	17.001690
30.729267	1281.092158	17.006707
31.021531	1286.726963	17.011725
31.277714	1286.512480	17.016743
31.108536	1284.822693	17.021760
31.101790	1283.877138	17.026778
31.543783	1280.839753	17.031795
31.488861	1278.036530	17.036813
31.389051	1263.614062	17.041831
31.544994	1252.194644	17.046848
31.384766	1253.189091	17.051866
30.976708	1250.640623	17.056883
31.015634	1254.712078	17.061901
31.126118	1257.384295	17.066919
31.558689	1253.333561	17.071936
31.408546	1252.742538	17.076954
31.425032	1252.272238	17.081971
31.657704	1256.148112	17.086989
31.029913	1257.813556	17.092007
31.509590	1264.886830	17.097024
31.529857	1270.472748	17.102042
31.448410	1278.235726	17.107059
31.506693	1273.044096	17.112077
31.542006	1271.122691	17.117095
31.940494	1266.794953	17.122112
31.535966	1268.771701	17.127130
31.474192	1271.252876	17.132147
31.527855	1261.594476	17.137165
31.496752	1266.658244	17.142183
31.483934	1270.772161	17.147200
31.191060	1268.571460	17.152218
31.185154	1291.198080	17.157235
31.864219	1293.670685	17.162253
31.697303	1295.239846	17.167271
32.033116	1296.688442	17.172288
31.943059	1294.881963	17.177306
31.825037	1295.949316	17.182323
32.151520	1296.244782	17.187341
31.993965	1296.691170	17.192359
32.211717	1289.410114	17.197376
32.318394	1300.718864	17.202394
32.042649	1302.185647	17.207411
32.386813	1296.078808	17.212429
32.215927	1300.159559	17.217447
32.149109	1302.320328	17.222464
32.423675	1295.277849	17.227482
32.510799	1299.901127	17.232499
32.426186	1298.764190	17.237517
32.503603	1305.990954	17.242535
32.469786	1298.920599	17.247552
32.853952	1292.725619	17.252570
32.475850	1300.207220	17.257587
32.725344	1294.523188	17.262605
32.678979	1294.361353	17.267623
32.572648	1289.818708	17.272640
32.520328	1299.316159	17.277658
31.656994	1296.974059	17.282675
32.241940	1300.310308	17.287693
32.126152	1309.458880	17.292711
32.432325	1319.188085	17.297728
33.106756	1315.309727	17.302746
32.999965	1317.197232	17.307763
33.208175	1310.678748	17.312781
33.105758	1313.900909	17.317799
33.309571	1315.001775	17.322816
33.099288	1301.690507	17.327834
32.976001	1310.096258	17.332851
33.163861	1303.195741	17.337869
33.380806	1307.970665	17.342887
33.002111	1295.644839	17.347904
33.158293	1290.236938	17.352922
32.963181	1305.222880	17.357939
33.275946	1305.284415	17.362957
33.142346	1317.212620	17.367975
33.231232	1307.698726	17.372992
33.866089	1308.999197	17.378010
33.307510	1298.159907	17.383027
33.297495	1300.255332	17.388045
33.250080	1310.922797	17.393063
33.572657	1304.398692	17.398080
33.425251	1301.251008	17.403098
33.189725	1310.260826	17.408115
33.473761	1306.709553	17.413133
33.190974	1310.881344	17.418151
33.219905	1303.021452	17.423168
33.659309	1305.826402	17.428186
33.153502	1310.267536	17.433203
33.764411	1302.622319	17.438221
33.714011	1306.980672	17.443239
33.637867	1302.885744	17.448256
33.758209	1304.002058	17.453274
33.560221	1310.602971	17.458291
33.648753	1329.339290	17.463309
34.190241	1334.187835	17.468327
34.362222	1320.451609	17.473344
34.309762	1305.952336	17.478362
34.181103	1303.067274	17.483379
34.283436	1301.529199	17.488397
33.936835	1297.909131	17.493415
34.320013	1304.363053	17.498432
34.212510	1296.816776	17.503450
33.992079	1300.154215	17.508467
34.256107	1285.193711	17.513485
34.300298	1299.125345	17.518503
34.041660	1300.786127	17.523520
34.393608	1292.128879	17.528538
34.266330	1305.306371	17.533555
34.101936	1296.682187	17.538573
34.154725	1300.453724	17.543591
34.298800	1321.354343	17.548608
34.228320	1328.424603	17.553626
34.515911	1335.097175	17.558643
34.877607	1331.420000	17.563661
34.438453	1331.381717	17.568679
34.361706	1330.110798	17.573696
34.721701	1325.187495	17.578714
34.523788	1330.717182	17.583731
34.573238	1323.303066	17.588749
34.480350	1325.146136	17.593767
34.477894	1325.983660	17.598784
34.722257	1323.936955	17.603802
34.410683	1329.992996	17.608819
34.540156	1333.521488	17.613837
34.897148	1325.186207	17.618855
34.632072	1330.231012	17.623872
34.892504	1339.194632	17.628890
34.872522	1347.154508	17.633907
35.007470	1345.890921	17.638925
35.203335	1353.940510	17.643943
35.275089	1345.859313	17.648960
35.577491	1342.835670	17.653978
35.328767	1335.843929	17.658995
35.320069	1319.700419	17.664013
35.196583	1318.531754	17.669031
34.917749	1318.619180	17.674048
35.346579	1327.258359	17.679066
35.173080	1340.390809	17.684083
35.226882	1350.273395	17.689101
35.462397	1355.582631	17.694119
35.205858	1352.149542	17.699136
35.412347	1342.191291	17.704154
35.206255	1348.008161	17.709171
35.070700	1344.103012	17.714189
34.963023	1345.738314	17.719207
35.545881	1349.068228	17.724224
35.832505	1357.529886	17.729242
35.756920	1361.503083	17.734259
35.785629	1353.981774	17.739277
35.766453	1349.571470	17.744295
35.538512	1367.469916	17.749312
35.774409	1360.733824	17.754330
36.082737	1368.162781	17.759347
36.428832	1357.868728	17.764365
36.427834	1347.257976	17.769383
35.836721	1353.208918	17.774400
36.264611	1341.615498	17.779418
36.033452	1343.047709	17.784435
36.103606	1349.177313	17.789453
36.063356	1338.473488	17.794471
35.852326	1345.402163	17.799488
36.107229	1342.678136	17.804506
35.961251	1362.208565	17.809523
36.161310	1370.912563	17.814541
36.035955	1370.663466	17.819559
35.840337	1379.085214	17.824576
36.246033	1375.954635	17.829594
36.352647	1374.940628	17.834611
36.110819	1382.661814	17.839629
36.212794	1376.253870	17.844647
36.282694	1379.263552	17.849664
36.341659	1387.376069	17.854682
36.752318	1400.299669	17.859699
36.607478	1401.223460	17.864717
36.966329	1391.670942	17.869735
37.066011	1404.026961	17.874752
36.950776	1379.204910	17.879770
36.612785	1371.449669	17.884787
36.494222	1372.057682	17.889805
37.139377	1375.611493	17.894823
36.772592	1389.185939	17.899840
37.151910	1379.520976	17.904858
36.981103	1373.281597	17.909875
36.712451	1370.042637	17.914893
36.920218	1378.217816	17.919911
36.807180	1393.707508	17.924928
37.072498	1386.355118	17.929946
37.069104	1396.574788	17.934963
36.801045	1394.348291	17.939981
37.188531	1389.827473	17.944999
37.114995	1395.792795	17.950016
37.499536	1385.541545	17.955034
36.931517	1392.170138	17.960051
36.998540	1387.436845	17.965069
37.215307	1394.717258	17.970087
37.154502	1398.912805	17.975104
37.286850	1396.176856	17.980122
37.427479	1404.145892	17.985139
37.225403	1419.164203	17.990157
37.858143	1411.910175	17.995175
37.986974	1423.103525	18.000192
37.702255	1409.804929	18.005210
37.575665	1404.416430	18.010227
37.791482	1412.501710	18.015245
37.917943	1417.411389	18.020263
37.869998	1404.669488	18.025280
37.666885	1398.006348	18.030298
38.035683	1402.053723	18.035315
38.040480	1403.367983	18.040333
37.776791	1392.924873	18.045351
37.780409	1409.403428	18.050368
37.776378	1405.300030	18.055386
37.967947	1414.129869	18.060403
37.966430	1412.268898	18.065421
38.270791	1412.336948	18.070439
37.936208	1412.473403	18.075456
38.134506	1405.692756	18.080474
38.173860	1420.265834	18.085491
37.994129	1415.443234	18.090509
38.204950	1417.400004	18.095527
37.662512	1413.617188	18.100544
38.026345	1421.683382	18.105562
38.346380	1422.210231	18.110579
38.139989	1430.705449	18.115597
38.539870	1428.749807	18.120615
38.512437	1426.975423	18.125632
38.752613	1424.593190	18.130650
38.691988	1431.700441	18.135667
38.772293	1424.681531	18.140685
38.828868	1416.985092	18.145703
38.475788	1427.945561	18.150720
38.850980	1418.484403	18.155738
39.007549	1433.521462	18.160755
38.564871	1430.842500	18.165773
38.774114	1426.909942	18.170791
38.815604	1427.735443	18.175808
39.112815	1423.667796	18.180826
38.952931	1423.810646	18.185843
39.025957	1429.731543	18.190861
38.975234	1426.613038	18.195879
39.206605	1428.971893	18.200896
39.133181	1427.439792	18.205914
39.535364	1421.681912	18.210931
38.692869	1432.944196	18.215949
38.936888	1431.109733	18.220967
39.293530	1449.118978	18.225984
39.453688	1452.666806	18.231002
39.636508	1455.006178	18.236019
39.539433	1458.729435	18.241037
39.618404	1439.716976	18.246055
39.615605	1446.168972	18.251072
39.527924	1430.243980	18.256090
39.670517	1424.728452	18.261107
39.406717	1425.280295	18.266125
39.739138	1434.757975	18.271143
39.796664	1443.140439	18.276160
39.508301	1444.595946	18.281178
39.963123	1445.406684	18.286195
39.798289	1446.358996	18.291213
40.005791	1432.325437	18.296231
39.858988	1446.729881	18.301248
39.932983	1448.954272	18.306266
40.289279	1437.230164	18.311283
40.116987	1434.510592	18.316301
39.896849	1415.412448	18.321319
39.860872	1440.599720	18.326336
40.010221	1448.420877	18.331354
40.040586	1445.079447	18.336371
39.762339	1451.274480	18.341389
39.769712	1434.669924	18.346407
39.623549	1445.238544	18.351424
40.075773	1448.394136	18.356442
40.471869	1456.321132	18.361459
40.108836	1466.111661	18.366477
40.609386	1475.044506	18.371495
40.212469	1468.643069	18.376512
39.894245	1468.515788	18.381530
40.486757	1465.527365	18.386547
40.392827	1469.899692	18.391565
40.284885	1460.463693	18.396583
40.332365	1472.919386	18.401600
40.479953	1483.727389	18.406618
40.828584	1488.078131	18.411635
40.858019	1502.710414	18.416653
40.588310	1498.833035	18.421671
40.938752	1503.309067	18.426688
40.654507	1507.121712	18.431706
41.273237	1490.851299	18.436723
40.927692	1497.076433	18.441741
41.486525	1496.704561	18.446759
41.138039	1495.917759	18.451776
41.293930	1496.058124	18.456794
41.417175	1487.688774	18.461811
41.069263	1493.040699	18.466829
41.080729	1486.480041	18.471847
41.589187	1492.354967	18.476864
41.549117	1488.384700	18.481882
41.806224	1488.387773	18.486899
41.228430	1496.745943	18.491917
41.405298	1492.815599	18.496935
41.178915	1487.319251	18.501952
41.204637	1487.508416	18.506970
41.702349	1488.004949	18.511987
41.506727	1484.955002	18.517005
41.222008	1480.565962	18.522023
41.544724	1483.411600	18.527040
41.352823	1484.280620	18.532058
41.841809	1491.628036	18.537075
41.705316	1503.469860	18.542093
41.730426	1517.010382	18.547111
41.616915	1511.231886	18.552128
42.011512	1510.286144	18.557146
41.903191	1510.979860	18.562163
41.838567	1518.092146	18.567181
42.078668	1510.414369	18.572199
42.068026	1504.223117	18.577216
41.931602	1513.411064	18.582234
42.110894	1508.039798	18.587251
42.038571	1510.253478	18.592269
42.027262	1509.532678	18.597287
42.288112	1511.827987	18.602304
42.159821	1514.428127	18.607322
42.413394	1527.112596	18.612339
42.257467	1531.129504	18.617357
42.601093	1535.742503	18.622375
42.888437	1531.981972	18.627392
42.965756	1532.993252	18.632410
42.811735	1515.009954	18.637427
42.694496	1507.871875	18.642445
42.758895	1499.789851	18.647463
42.590291	1502.945101	18.652480
42.618774	1507.552598	18.657498
42.862253	1503.996998	18.662515
42.678652	1510.762923	18.667533
42.789103	1515.408766	18.672551
43.023378	1528.664933	18.677568
43.409401	1535.618470	18.682586
43.461798	1514.505658	18.687603
43.219988	1506.894594	18.692621
43.237770	1492.994874	18.697639
43.162491	1493.634279	18.702656
43.152042	1494.794786	18.707674
43.320473	1493.775616	18.712691
42.902925	1502.379195	18.717709
43.271440	1511.650535	18.722727
43.821513	1516.598891	18.727744
43.534262	1518.269175	18.732762
43.427068	1501.325724	18.737779
43.449781	1524.550276	18.742797
43.246012	1525.240566	18.747815
43.502741	1512.759741	18.752832
43.230980	1525.363810	18.757850
43.677781	1522.415342	18.762867
43.518184	1528.487931	18.767885
43.340128	1524.302405	18.772903
43.696274	1524.602395	18.777920
43.594069	1526.539162	18.782938
43.791396	1529.521394	18.787955
43.746522	1553.534765	18.792973
43.759962	1553.859434	18.797991
44.009508	1562.454923	18.803008
43.943563	1549.588338	18.808026
44.075354	1542.289957	18.813043
44.346939	1547.118078	18.818061
44.215102	1540.754440	18.823079
44.418899	1551.136622	18.828096
44.160459	1551.837181	18.833114
44.569138	1542.306998	18.838131
44.408192	1540.546524	18.843149
44.499603	1556.203968	18.848167
44.596229	1547.076821	18.853184
44.295100	1549.703725	18.858202
44.529305	1545.231567	18.863219
44.527786	1549.107465	18.868237
44.113126	1553.966972	18.873255
44.356212	1544.957213	18.878272
44.556799	1566.254667	18.883290
44.986236	1580.065044	18.888307
44.576529	1577.098692	18.893325
44.851771	1578.618012	18.898343
45.185098	1578.457239	18.903360
45.021870	1574.738911	18.908378
45.283942	1571.366816	18.913395
45.185683	1578.154411	18.918413
45.162452	1578.293841	18.923431
45.068234	1568.764158	18.928448
45.035862	1577.021481	18.933466
45.347561	1575.227327	18.938483
45.089621	1573.576669	18.943501
45.241580	1569.168173	18.948519
45.536864	1569.628671	18.953536
45.026768	1574.144998	18.958554
45.267573	1565.406861	18.963571
45.332669	1572.199193	18.968589
45.189036	1570.644494	18.973607
45.588907	1561.722445	18.978624
45.306876	1567.265409	18.983642
45.473181	1571.064207	18.988659
45.253832	1567.961889	18.993677
45.489727	1587.688181	18.998695
45.646031	1590.075681	19.003712
45.589600	1602.293242	19.008730
45.717828	1590.200635	19.013747
45.605547	1599.756660	19.018765
45.643415	1595.878134	19.023783
45.983073	1588.994386	19.028800
45.762981	1591.157443	19.033818
45.955406	1598.704986	19.038835
46.182838	1614.372164	19.043853
45.866300	1616.451649	19.048871
46.333321	1626.836589	19.053888
46.545818	1621.174729	19.058906
46.734763	1615.519936	19.063923
46.429372	1609.945339	19.068941
46.481667	1612.878466	19.073959
46.953471	1603.914122	19.078976
46.907442	1599.733796	19.083994
46.705862	1585.951159	19.089011
46.567905	1582.486104	19.094029
46.487745	1579.051206	19.099047
46.445844	1585.816446	19.104064
46.066081	1597.682633	19.109082
46.849973	1602.601997	19.114099
46.857602	1608.226358	19.119117
46.652629	1614.238413	19.124135
46.973578	1603.849954	19.129152
47.178511	1612.516272	19.134170
46.983814	1599.771830	19.139187
47.015833	1613.357745	19.144205
46.860841	1609.899845	19.149223
47.205841	1603.526218	19.154240
47.406188	1616.911721	19.159258
47.221670	1606.265546	19.164275
47.045143	1601.669122	19.169293
46.965156	1625.047506	19.174311
47.447830	1628.604762	19.179328
47.516611	1636.503972	19.184346
47.359039	1637.590519	19.189363
47.441743	1632.358489	19.194381
47.259189	1631.796459	19.199399
47.800839	1624.360627	19.204416
47.979916	1625.695152	19.209434
47.570524	1635.302943	19.214451
47.805331	1626.101210	19.219469
47.419617	1634.873977	19.224487
47.800065	1632.133759	19.229504
47.903221	1628.723893	19.234522
47.680782	1629.023990	19.239539
47.459180	1627.738146	19.244557
47.810407	1653.980289	19.249575
47.695667	1654.198707	19.254592
48.168464	1657.751706	19.259610
48.161107	1658.688092	19.264627
48.326929	1657.489427	19.269645
48.174443	1662.336100	19.274663
48.349424	1660.322143	19.279680
48.435907	1650.319469	19.284698
48.397810	1665.655640	19.289715
48.300435	1654.854793	19.294733
47.990384	1662.070534	19.299751
47.902143	1667.373847	19.304768
48.324349	1681.004023	19.309786
48.425405	1684.280630	19.314803
48.938945	1676.437246	19.319821
48.784732	1684.218427	19.324839
48.952708	1674.023062	19.329856
49.334452	1695.126807	19.334874
48.805493	1677.873739	19.339891
49.165397	1673.135774	19.344909
49.153779	1684.668402	19.349927
49.467498	1681.418013	19.354944
49.318871	1677.549990	19.359962
49.117879	1680.711446	19.364979
49.346035	1669.486410	19.369997
48.885874	1677.645992	19.375015
49.609788	1679.168703	19.380032
49.758186	1675.383595	19.385050
49.356347	1669.717527	19.390067
49.509994	1674.862531	19.395085
49.168434	1679.165839	19.400103
49.396992	1674.976075	19.405120
49.293946	1673.085491	19.410138
49.145979	1688.286011	19.415155
49.562127	1697.082623	19.420173
49.650960	1709.641868	19.425191
49.796995	1710.075210	19.430208
49.594953	1708.136509	19.435226
49.807305	1704.293127	19.440243
50.111833	1700.634818	19.445261
50.322871	1705.790372	19.450279
50.132427	1701.569455	19.455296
50.081027	1702.976545	19.460314
50.233638	1697.586813	19.465331
50.327763	1693.527654	19.470349
50.334881	1699.290320	19.475367
50.210856	1691.913522	19.480384
50.297670	1690.329959	19.485402
50.143935	1695.474878	19.490419
50.266463	1694.571197	19.495437
50.080175	1697.114078	19.500455
50.340770	1710.327839	19.505472
50.507080	1716.675069	19.510490
50.696204	1721.267347	19.515507
50.943504	1705.886784	19.520525
50.966949	1729.598918	19.525543
50.554363	1719.504740	19.530560
51.159066	1724.861010	19.535578
50.826586	1726.869538	19.540595
51.297447	1719.671409	19.545613
51.091621	1726.967494	19.550631
51.199323	1715.080168	19.555648
50.772611	1716.831525	19.560666
50.611820	1724.703976	19.565683
51.070792	1716.722399	19.570701
50.846024	1721.819685	19.575719
51.091085	1720.344461	19.580736
51.279592	1739.888669	19.585754
51.260789	1749.883577	19.590771
51.087489	1746.762938	19.595789
51.635077	1751.373993	19.600807
51.655171	1749.899543	19.605824
51.786167	1747.316907	19.610842
51.786535	1749.927591	19.615859
51.798774	1735.188424	19.620877
51.766452	1745.915885	19.625895
52.029763	1739.408537	19.630912
52.049106	1747.991211	19.635930
51.941758	1742.421837	19.640947
51.820329	1739.709898	19.645965
51.790216	1745.497273	19.650983
52.094766	1746.908591	19.656000
52.032412	1738.152241	19.661018
51.688105	1746.291423	19.666035
51.912655	1738.623598	19.671053
51.818832	1736.454311	19.676071
52.009160	1749.418763	19.681088
52.090760	1760.196589	19.686106
52.367070	1767.124373	19.691123
52.283020	1755.880692	19.696141
52.068795	1768.256499	19.701159
52.309697	1761.297357	19.706176
52.668164	1755.561583	19.711194
52.428331	1761.819250	19.716211
52.563940	1779.326646	19.721229
52.901259	1789.068690	19.726247
52.719350	1794.210057	19.731264
52.990975	1790.398928	19.736282
53.262269	1784.223698	19.741299
53.572996	1791.251676	19.746317
53.860431	1775.594296	19.751335
53.438187	1756.867113	19.756352
53.437211	1747.815519	19.761370
53.009766	1751.944147	19.766387
53.434519	1739.434426	19.771405
53.154682	1748.322729	19.776423
53.469491	1740.883600	19.781440
53.847394	1749.027550	19.786458
53.528116	1747.909110	19.791475
53.657267	1743.347270	19.796493
53.558985	1742.515719	19.801511
53.538416	1747.540492	19.806528
54.018268	1741.702658	19.811546
53.362353	1746.990901	19.816563
53.464733	1748.904321	19.821581
53.864380	1755.002158	19.826599
53.690181	1781.592868	19.831616
53.544992	1766.776294	19.836634
53.611753	1785.066393	19.841651
53.926013	1780.372203	19.846669
53.542378	1775.778259	19.851687
53.768329	1791.476571	19.856704
53.914774	1801.169246	19.861722
53.653255	1804.920311	19.866739
53.833620	1815.144362	19.871757
54.152771	1818.331206	19.876775
54.269922	1831.949225	19.881792
54.417382	1832.140208	19.886810
54.704813	1839.109483	19.891827
54.640814	1836.347824	19.896845
55.058219	1834.340404	19.901863
54.674330	1836.500403	19.906880
54.876103	1829.899308	19.911898
54.951017	1832.014941	19.916915
55.071145	1832.522670	19.921933
55.004231	1834.178413	19.926951
54.609066	1840.998147	19.931968
55.148503	1838.862570	19.936986
54.879430	1837.810582	19.942003
54.840121	1841.602282	19.947021
55.137479	1831.938064	19.952039
55.146256	1848.566621	19.957056
55.451745	1827.856986	19.962074
55.217071	1835.211853	19.967091
55.376837	1842.243292	19.972109
55.564575	1840.981128	19.977127
55.309564	1837.098070	19.982144
55.562146	1842.075899	19.987162
55.649048	1854.380859	19.992179
55.732330	1864.843125	19.997197
56.038367	1859.234531	20.002215
55.713250	1863.451691	20.007232
56.197507	1854.772930	20.012250
55.977866	1854.959179	20.017267
56.264682	1854.897867	20.022285
56.087103	1837.227165	20.027303
55.760450	1831.029250	20.032320
56.099953	1836.197749	20.037338
55.861712	1853.097287	20.042355
55.997082	1851.857605	20.047373
56.228396	1845.099232	20.052391
55.934003	1863.930552	20.057408
56.534143	1853.291588	20.062426
56.187062	1849.054932	20.067443
55.744316	1864.249893	20.072461
56.189572	1871.338620	20.077479
56.321047	1884.282652	20.082496
56.377739	1882.150926	20.087514
56.594928	1881.185438	20.092531
56.849396	1881.716117	20.097549
56.730200	1892.180952	20.102567
56.497405	1890.633166	20.107584
57.029051	1905.089840	20.112602
57.104001	1905.240513	20.117619
57.362073	1923.250160	20.122637
57.463625	1912.403472	20.127655
57.221645	1917.762738	20.132672
57.646237	1908.697799	20.137690
57.539799	1911.938468	20.142707
57.356314	1905.125389	20.147725
57.435395	1908.573806	20.152743
57.381085	1906.103833	20.157760
57.429425	1903.883728	20.162778
57.572967	1913.520262	20.167795
57.488676	1906.777703	20.172813
57.536605	1903.906879	20.177831
57.676320	1902.456628	20.182848
57.623335	1901.801398	20.187866
57.696198	1908.301640	20.192883
57.591009	1917.294083	20.197901
57.785091	1923.624972	20.202919
57.555804	1932.689230	20.207936
58.570601	1922.017523	20.212954
58.620928	1921.248271	20.217971
58.419032	1921.303225	20.222989
58.479000	1912.616210	20.228007
58.568487	1919.412907	20.233024
58.732562	1910.045203	20.238042
58.856914	1917.856974	20.243059
58.621575	1907.415101	20.248077
59.032239	1900.026502	20.253095
58.709166	1891.263004	20.258112
58.957880	1877.262352	20.263130
58.439644	1874.298230	20.268147
58.455591	1889.621703	20.273165
59.205605	1893.074747	20.278183
59.053480	1902.778133	20.283200
58.801568	1905.977624	20.288218
59.418974	1895.954661	20.293235
59.232169	1910.416577	20.298253
59.293863	1904.848183	20.303271
58.849683	1902.133952	20.308288
58.887985	1910.665534	20.313306
59.145876	1901.873976	20.318323
59.123510	1904.841615	20.323341
59.005944	1904.232945	20.328359
59.045860	1912.230400	20.333376
58.993459	1912.600665	20.338394
59.248391	1931.229742	20.343411
59.199052	1939.066848	20.348429
59.490626	1940.088608	20.353447
59.415904	1940.829514	20.358464
59.591271	1952.582052	20.363482
59.894425	1961.546416	20.368499
59.636552	1964.218955	20.373517
60.040251	1963.246480	20.378535
59.528426	1968.404547	20.383552
60.020134	1962.787892	20.388570
60.427833	1966.586037	20.393587
59.952891	1967.150942	20.398605
60.672571	1971.337003	20.403623
60.694712	1958.797959	20.408640
60.630835	1957.122484	20.413658
60.870743	1952.008315	20.418675
60.447348	1949.333141	20.423693
60.700807	1933.881249	20.428711
60.765923	1949.571020	20.433728
60.485625	1957.548097	20.438746
60.793234	1972.188528	20.443763
60.733960	1982.334407	20.448781
60.776254	1972.393595	20.453799
61.053688	1971.268876	20.458816
61.195758	1980.591129	20.463834
61.176059	1979.198468	20.468851
60.944102	1990.389595	20.473869
61.588177	1978.518434	20.478887
61.456936	1985.246727	20.483904
61.288254	1978.935883	20.488922
61.239113	1975.959130	20.493939
61.110308	1976.767688	20.498957
61.207429	1979.327291	20.503975
61.433728	1999.292713	20.508992
61.375636	2007.329735	20.514010
61.733003	2008.705529	20.519027
61.773709	2012.957992	20.524045
61.851516	2004.322686	20.529063
61.981536	2007.371711	20.534080
61.730193	1997.598585	20.539098
62.207575	2001.273346	20.544115
61.907036	2006.781746	20.549133
62.027890	2001.737348	20.554151
62.395455	2009.326851	20.559168
62.246815	2012.470223	20.564186
62.575671	2028.375297	20.569203
62.215521	2031.177839	20.574221
62.531868	2027.486387	20.579239
62.485662	2023.885510	20.584256
62.416764	2025.355773	20.589274
62.932404	2029.685607	20.594291
62.694454	2031.156802	20.599309
62.482019	2026.146136	20.604327
62.712293	2029.896227	20.609344
62.503652	2032.835794	20.614362
62.395885	2031.713674	20.619379
62.375105	2049.800130	20.624397
62.848289	2055.697280	20.629415
62.963383	2058.105875	20.634432
62.998421	2048.009526	20.639450
63.114199	2060.532688	20.644467
63.074171	2067.322630	20.649485
63.558515	2080.206997	20.654503
63.522987	2085.275704	20.659520
63.753643	2089.087557	20.664538
63.942186	2075.787682	20.669555
64.029443	2078.322169	20.674573
64.121617	2063.211920	20.679591
63.628425	2047.129672	20.684608
63.761275	2056.407045	20.689626
63.985259	2034.964216	20.694643
63.780910	2061.027339	20.699661
64.188138	2077.340308	20.704679
64.329084	2079.130823	20.709696
64.237064	2081.226990	20.714714
64.203685	2074.757003	20.719731
64.178472	2082.037408	20.724749
64.287325	2082.117487	20.729767
64.551369	2082.174135	20.734784
64.079407	2084.258252	20.739802
64.611127	2081.117615	20.744819
64.656087	2077.651575	20.749837
64.683302	2075.265269	20.754855
64.730648	2079.333574	20.759872
64.458812	2079.258418	20.764890
64.763707	2069.030982	20.769907
64.706513	2087.492436	20.774925
64.922178	2100.639589	20.779943
65.170647	2095.624345	20.784960
65.174271	2111.142213	20.789978
65.251426	2096.806881	20.794995
65.033048	2103.981603	20.800013
65.139790	2091.011851	20.805031
65.594044	2101.390573	20.810048
65.370394	2102.214901	20.815066
65.555999	2094.005730	20.820083
65.264349	2097.506357	20.825101
65.493567	2093.306923	20.830119
65.680942	2108.858030	20.835136
65.480688	2112.783241	20.840154
65.827090	2113.900627	20.845171
65.757435	2120.020702	20.850189
66.102662	2112.724376	20.855207
66.198558	2105.358074	20.860224
66.215929	2107.373858	20.865242
66.367766	2108.275939	20.870259
66.307729	2104.921045	20.875277
66.644810	2101.685192	20.880295
66.504491	2103.366549	20.885312
66.249652	2101.109009	20.890330
66.438918	2107.743141	20.895347
66.237291	2109.923671	20.900365
66.346900	2110.135123	20.905383
66.405021	2124.639208	20.910400
66.506595	2137.980555	20.915418
66.500832	2137.137148	20.920435
66.626050	2135.679836	20.925453
66.643939	2133.725788	20.930471
66.940259	2134.266844	20.935488
66.993506	2157.749085	20.940506
67.281666	2152.814236	20.945523
67.345803	2161.390088	20.950541
67.237364	2157.777081	20.955559
67.572920	2152.076467	20.960576
67.444768	2156.028288	20.965594
67.890181	2154.643351	20.970611
67.923139	2154.388400	20.975629
67.914181	2155.517605	20.980647
68.161942	2143.935420	20.985664
67.497933	2139.420642	20.990682
67.647311	2126.846536	20.995699
67.725150	2154.487350	21.000717
67.839293	2149.102675	21.005735
67.868894	2157.758676	21.010752
67.874172	2157.070523	21.015770
67.985198	2150.993833	21.020787
68.082825	2148.652902	21.025805
67.975784	2148.018063	21.030823
68.012041	2155.190253	21.035840
67.736036	2182.130463	21.040858
68.190335	2181.300357	21.045875
68.575678	2183.320349	21.050893
68.089498	2181.760707	21.055911
68.637965	2178.752704	21.060928
68.882366	2191.696335	21.065946
68.866543	2198.130336	21.070963
69.273772	2193.434351	21.075981
69.210985	2195.836705	21.080999
69.620953	2191.453658	21.086016
69.330861	2175.696976	21.091034
69.215558	2167.188952	21.096051
69.389456	2166.846796	21.101069
69.207297	2170.430424	21.106087
69.642726	2169.523138	21.111104
69.593403	2179.881276	21.116122
69.691770	2188.844375	21.121139
69.585996	2178.323698	21.126157
69.431102	2195.392435	21.131175
69.897471	2182.972297	21.136192
69.464515	2185.829880	21.141210
69.822206	2190.562790	21.146227
69.932151	2185.170139	21.151245
69.802631	2196.928653	21.156263
69.881317	2189.833680	21.161280
69.648824	2196.721022	21.166298
69.988643	2210.373628	21.171315
69.988283	2224.919811	21.176333
70.098634	2225.603199	21.181351
70.176851	2221.450088	21.186368
70.325171	2225.455192	21.191386
70.264050	2232.979436	21.196403
70.667651	2236.972430	21.201421
70.685005	2255.263422	21.206439
70.843662	2249.980766	21.211456
70.535803	2251.582894	21.216474
70.687646	2255.666949	21.221491
71.176276	2253.808275	21.226509
70.735298	2262.442935	21.231527
71.129099	2241.460587	21.236544
70.894016	2262.782983	21.241562
71.381899	2268.747066	21.246579
71.596606	2275.713271	21.251597
71.261526	2271.723327	21.256615
71.518233	2273.993457	21.261632
71.275563	2279.411229	21.266650
71.273835	2278.825025	21.271667
71.567199	2273.025866	21.276685
71.214198	2285.356641	21.281703
71.758402	2291.053098	21.286720
71.840774	2307.367545	21.291738
71.524782	2299.944800	21.296755
71.723758	2305.893920	21.301773
71.742492	2308.713857	21.306791
72.142331	2313.314994	21.311808
72.159386	2333.014827	21.316826
72.272308	2334.583645	21.321843
72.476240	2332.707709	21.326861
72.328285	2328.427588	21.331879
72.921300	2306.051769	21.336896
72.922775	2314.312126	21.341914
73.143859	2314.168430	21.346931
73.643260	2317.665196	21.351949
73.375477	2304.097650	21.356967
73.255066	2283.252678	21.361984
72.985773	2282.807796	21.367002
73.163345	2280.091344	21.372019
73.101584	2275.202802	21.377037
73.142977	2283.197841	21.382055
73.319555	2275.934587	21.387072
73.029518	2284.298497	21.392090
73.331042	2299.273329	21.397107
73.653355	2311.426139	21.402125
73.769498	2318.310316	21.407143
74.079863	2315.750927	21.412160
73.855012	2309.138643	21.417178
73.855557	2315.940848	21.422195
73.936774	2311.386810	21.427213
73.937584	2318.743712	21.432231
73.829010	2306.408008	21.437248
73.577529	2304.779817	21.442266
73.387967	2312.881761	21.447283
73.867752	2316.151859	21.452301
73.673002	2330.520994	21.457319
73.818520	2335.909703	21.462336
73.965984	2346.952590	21.467354
74.119432	2362.310371	21.472371
74.835735	2361.510730	21.477389
74.751503	2359.764183	21.482407
75.448177	2341.237347	21.487424
75.703407	2339.382807	21.492442
75.750680	2325.086877	21.497459
75.738817	2312.457133	21.502477
75.309317	2309.099031	21.507495
75.520115	2291.728231	21.512512
75.358238	2295.793176	21.517530
75.871674	2304.160966	21.522547
75.494319	2296.986222	21.527565
75.291105	2306.334560	21.532583
75.458428	2300.353183	21.537600
75.595552	2309.222113	21.542618
75.754576	2307.212302	21.547635
75.778168	2301.716636	21.552653
75.560960	2303.911988	21.557671
75.704293	2302.417791	21.562688
75.480319	2318.370555	21.567706
75.910439	2328.079801	21.572723
76.103544	2328.596286	21.577741
76.200365	2340.227917	21.582759
76.090726	2342.246730	21.587776
75.988685	2333.072218	21.592794
76.206314	2348.681925	21.597811
76.556591	2346.192278	21.602829
76.069089	2367.946151	21.607847
76.058656	2363.664425	21.612864
76.127550	2370.772627	21.617882
76.372377	2383.726191	21.622899
76.827078	2387.738293	21.627917
77.217200	2379.997360	21.632935
77.147465	2377.312544	21.637952
77.069354	2381.899827	21.642970
77.114275	2381.045621	21.647987
77.329188	2385.799959	21.653005
77.114166	2376.394978	21.658023
77.691180	2384.023481	21.663040
77.531048	2379.069363	21.668058
77.180422	2390.651377	21.673075
77.512488	2387.719067	21.678093
77.305843	2394.297071	21.683111
77.642404	2409.405955	21.688128
78.142037	2404.287845	21.693146
77.969915	2425.464955	21.698163
78.222931	2404.031360	21.703181
78.002555	2408.153302	21.708199
78.191815	2413.225703	21.713216
78.230210	2407.922428	21.718234
77.914330	2407.638439	21.723251
78.239368	2404.841943	21.728269
78.196422	2406.171311	21.733287
78.318228	2415.950752	21.738304
78.895396	2429.406226	21.743322
78.609015	2435.721900	21.748339
78.435559	2434.385856	21.753357
78.851398	2435.796069	21.758375
78.803132	2431.168236	21.763392
78.728144	2432.934443	21.768410
78.819263	2437.276679	21.773427
78.875347	2440.219964	21.778445
78.991120	2444.165571	21.783463
79.104467	2446.371755	21.788480
79.512924	2450.685270	21.793498
79.356777	2457.215930	21.798515
79.665445	2440.674400	21.803533
79.220816	2458.949890	21.808551
79.583273	2475.928621	21.813568
79.743129	2484.452915	21.818586
79.875213	2480.891987	21.823603
80.345608	2482.486845	21.828621
79.784921	2481.931718	21.833639
80.410282	2482.593700	21.838656
80.041582	2483.316951	21.843674
80.229858	2476.820194	21.848691
80.160954	2480.200811	21.853709
80.176995	2487.101700	21.858727
80.399561	2506.073870	21.863744
80.600318	2505.518180	21.868762
80.598218	2516.328161	21.873779
81.142986	2506.242078	21.878797
81.004291	2507.036951	21.883815
81.145236	2510.761454	21.888832
81.572160	2509.087030	21.893850
80.896430	2508.231323	21.898867
81.235126	2498.770068	21.903885
81.061545	2505.903670	21.908903
80.739966	2507.555743	21.913920
80.993006	2519.545813	21.918938
81.327433	2537.262765	21.923955
81.647608	2537.383319	21.928973
81.581262	2542.941963	21.933991
81.988237	2538.358523	21.939008
82.003573	2536.769824	21.944026
81.826938	2531.962894	21.949043
81.709201	2532.864133	21.954061
82.072861	2549.302958	21.959079
81.887659	2549.190956	21.964096
82.395258	2553.051391	21.969114
82.037280	2558.552205	21.974131
82.277696	2562.271606	21.979149
82.465399	2554.096492	21.984167
82.628945	2560.220504	21.989184
82.533028	2555.779696	21.994202
82.582735	2552.455287	21.999219
82.477955	2558.257736	22.004237
82.677141	2566.777901	22.009255
82.955610	2580.070936	22.014272
83.463328	2580.887914	22.019290
82.921731	2580.067393	22.024307
83.302188	2572.655152	22.029325
83.489691	2575.300231	22.034343
83.313034	2576.575847	22.039360
84.260173	2570.196642	22.044378
84.014511	2568.012706	22.049395
84.046319	2563.451845	22.054413
84.182338	2560.305618	22.059431
83.750559	2568.332984	22.064448
83.813498	2564.715416	22.069466
84.006255	2564.817382	22.074483
84.034708	2565.658498	22.079501
84.050038	2562.804781	22.084519
83.719233	2573.010741	22.089536
84.569424	2562.178555	22.094554
84.135419	2572.940272	22.099571
84.180681	2571.572197	22.104589
84.317521	2585.982131	22.109607
84.311217	2587.868442	22.114624
84.579693	2589.541755	22.119642
84.757359	2605.181199	22.124659
84.451624	2595.561228	22.129677
84.857879	2596.860052	22.134695
84.866258	2620.150046	22.139712
85.060005	2615.885106	22.144730
84.803667	2616.175102	22.149747
85.185352	2621.246301	22.154765
85.449024	2623.190901	22.159783
85.134581	2616.248871	22.164800
85.333594	2631.726519	22.169818
85.429367	2636.031815	22.174835
85.573846	2645.559589	22.179853
86.103438	2635.868091	22.184871
85.903387	2636.263305	22.189888
86.125008	2629.914888	22.194906
86.239871	2628.555713	22.199923
86.360059	2633.468004	22.204941
86.598583	2637.833045	22.209959
86.410051	2633.518636	22.214976
86.472769	2618.448966	22.219994
86.045385	2629.048196	22.225011
86.304527	2649.648400	22.230029
86.818900	2659.514334	22.235047
86.772841	2659.185102	22.240064
87.054164	2650.958943	22.245082
87.329602	2660.890180	22.250099
87.260717	2664.874408	22.255117
87.151800	2655.273266	22.260135
87.336310	2656.405396	22.265152
87.405760	2656.626680	22.270170
87.469928	2650.192212	22.275187
87.666432	2656.411971	22.280205
87.623765	2655.722315	22.285223
87.268785	2652.840357	22.290240
87.539346	2671.753963	22.295258
87.586155	2684.293423	22.300275
87.405463	2680.525363	22.305293
87.720090	2683.017043	22.310311
87.487657	2685.634290	22.315328
87.789052	2703.714028	22.320346
87.817905	2700.126110	22.325363
88.604200	2702.018510	22.330381
88.645102	2693.238948	22.335399
88.399127	2704.264402	22.340416
88.943729	2696.697651	22.345434
88.862524	2688.441561	22.350451
88.740238	2696.865217	22.355469
89.069750	2688.596383	22.360487
88.665201	2691.352477	22.365504
89.198580	2689.002041	22.370522
89.133053	2699.687250	22.375539
89.054437	2707.900101	22.380557
89.579624	2714.777895	22.385575
89.561679	2712.952964	22.390592
89.528591	2716.548164	22.395610
89.693846	2713.720686	22.400627
89.752603	2715.167830	22.405645
89.973662	2708.721437	22.410663
89.867131	2714.620697	22.415680
89.994112	2704.783065	22.420698
90.021091	2710.726674	22.425715
90.038131	2710.062527	22.430733
90.256799	2713.931257	22.435751
90.232828	2716.139040	22.440768
90.177935	2708.800269	22.445786
90.164107	2730.051097	22.450803
90.261735	2737.605110	22.455821
90.260012	2738.922142	22.460839
90.229849	2747.643919	22.465856
90.676284	2750.536169	22.470874
90.843305	2769.887992	22.475891
90.944240	2774.343659	22.480909
91.308316	2772.022530	22.485927
91.220718	2774.723994	22.490944
91.353628	2767.376033	22.495962
91.661952	2754.575781	22.500979
91.993782	2760.009269	22.505997
92.016386	2749.321584	22.511015
92.143318	2768.874962	22.516032
92.148910	2751.462948	22.521050
92.110638	2761.636949	22.526067
91.775882	2754.225371	22.531085
92.159982	2755.979886	22.536103
91.900640	2757.935831	22.541120
91.890749	2753.149548	22.546138
92.181033	2742.509906	22.551155
92.096795	2756.052359	22.556173
92.526505	2763.262989	22.561191
92.416868	2769.723842	22.566208
92.557701	2774.589437	22.571226
92.460666	2775.339602	22.576243
92.802612	2777.237354	22.581261
92.712027	2767.257878	22.586279
93.029616	2785.351163	22.591296
92.935555	2783.825111	22.596314
93.408172	2792.942122	22.601331
93.094496	2791.187592	22.606349
93.510153	2790.698152	22.611367
93.281942	2798.695741	22.616384
93.529966	2796.010802	22.621402
93.616014	2808.049323	22.626419
93.765133	2808.326664	22.631437
94.109426	2807.948697	22.636455
94.080805	2819.749970	22.641472
94.101133	2813.785346	22.646490
94.091243	2816.004977	22.651507
94.376382	2813.486318	22.656525
94.611979	2808.283606	22.661543
94.559310	2812.866393	22.666560
94.374817	2817.395101	22.671578
94.836238	2808.113670	22.676595
94.354017	2814.779384	22.681613
94.695724	2807.167949	22.686631
94.825010	2823.796028	22.691648
94.912975	2835.797635	22.696666
94.678511	2844.026615	22.701683
94.904009	2847.434372	22.706701
95.081949	2838.140190	22.711719
95.033635	2846.641009	22.716736
95.222755	2863.743075	22.721754
95.588125	2854.695704	22.726771
95.510223	2867.557237	22.731789
96.006640	2849.867466	22.736807
95.884919	2861.568881	22.741824
95.725103	2865.987195	22.746842
95.901286	2864.136677	22.751859
95.799449	2862.918622	22.756877
96.054831	2877.130375	22.761895
96.388229	2887.850602	22.766912
96.344538	2881.697366	22.771930
96.773609	2877.147561	22.776947
96.632024	2878.478006	22.781965
96.623069	2882.786996	22.786983
96.854894	2883.303366	22.792000
96.503533	2880.962924	22.797018
96.825620	2893.206787	22.802035
96.941821	2913.412959	22.807053
97.120339	2905.795525	22.812071
97.272132	2908.081612	22.817088
96.851567	2914.680030	22.822106
97.466575	2910.094196	22.827123
97.440040	2927.336903	22.832141
97.372504	2941.061793	22.837159
97.651143	2938.202832	22.842176
97.919610	2936.099158	22.847194
97.819895	2949.508909	22.852211
97.660602	2938.792265	22.857229
98.224553	2951.981084	22.862247
98.528383	2963.533500	22.867264
98.233420	2971.648577	22.872282
98.405506	2964.220385	22.877299
98.246234	2962.394502	22.882317
98.562554	2955.022664	22.887335
98.813623	2955.064152	22.892352
98.621728	2963.152646	22.897370
99.060521	2975.108261	22.902387
98.893449	2982.549681	22.907405
99.262751	2990.180723	22.912423
99.293043	2987.601627	22.917440
99.183844	2991.799345	22.922458
99.795454	2986.319108	22.927475
99.488886	2981.742307	22.932493
99.478154	2984.282598	22.937511
99.371489	2993.881854	22.942528
99.511080	3011.790009	22.947546
100.233456	3020.754221	22.952563
100.025506	3024.169482	22.957581
100.159082	3022.831969	22.962599
100.279823	3014.494897	22.967616
99.942506	3018.267901	22.972634
100.536697	3018.153933	22.977651
100.299813	3040.234438	22.982669
100.259885	3039.212788	22.987687
100.405633	3045.245062	22.992704
100.553392	3037.395256	22.997722
100.993650	3050.963798	23.002739
101.144482	3067.137734	23.007757
101.172233	3063.630631	23.012775
101.188950	3067.598372	23.017792
101.133737	3069.342070	23.022810
101.711750	3060.606118	23.027827
101.636734	3056.982621	23.032845
101.760571	3057.020450	23.037863
101.710100	3058.270802	23.042880
101.811445	3065.620011	23.047898
101.928894	3056.218422	23.052915
101.918236	3065.337164	23.057933
101.760514	3075.815101	23.062951
102.309843	3077.402814	23.067968
102.326653	3083.779785	23.072986
102.376742	3074.150384	23.078003
102.163954	3077.243995	23.083021
102.298506	3091.319713	23.088039
102.943353	3095.405529	23.093056
102.764041	3117.562802	23.098074
102.925154	3108.283856	23.103091
103.110929	3128.238174	23.108109
102.866768	3113.859236	23.113127
102.708311	3117.483631	23.118144
102.981877	3132.521795	23.123162
103.485427	3138.152487	23.128179
103.470293	3150.229743	23.133197
103.458013	3153.203818	23.138215
103.635984	3142.282153	23.143232
103.846313	3147.341057	23.148250
104.572031	3141.392160	23.153267
104.290819	3137.260742	23.158285
104.257283	3150.451382	23.163303
104.521246	3154.870222	23.168320
104.343717	3159.984139	23.173338
104.946082	3158.661627	23.178355
104.528414	3159.567861	23.183373
104.691665	3164.260154	23.188391
104.791720	3150.623254	23.193408
104.824834	3159.702491	23.198426
104.971862	3146.275523	23.203443
105.224629	3152.043576	23.208461
105.453745	3169.429118	23.213479
105.762313	3170.318604	23.218496
105.655961	3181.030220	23.223514
105.676958	3174.372377	23.228531
105.681301	3175.420699	23.233549
105.745321	3173.682494	23.238567
105.704175	3170.680953	23.243584
105.684018	3178.260267	23.248602
105.781302	3172.009467	23.253619
106.005342	3189.438398	23.258637
106.221518	3202.214323	23.263655
106.343078	3201.564283	23.268672
106.157338	3214.336140	23.273690
106.492416	3207.563088	23.278707
106.507234	3227.794785	23.283725
106.390016	3231.069410	23.288743
106.786745	3232.541151	23.293760
106.813520	3235.930835	23.298778
106.935576	3238.035283	23.303795
107.143753	3256.557965	23.308813
107.791934	3268.367582	23.313831
107.738089	3256.244882	23.318848
107.682386	3261.275982	23.323866
107.974422	3257.583169	23.328883
107.887335	3260.454332	23.333901
108.096535	3264.364935	23.338919
108.045763	3253.957627	23.343936
107.682531	3259.051252	23.348954
108.202596	3260.713147	23.353971
108.387550	3276.184717	23.358989
108.319538	3278.515264	23.364007
108.627281	3283.530462	23.369024
108.251058	3285.679927	23.374042
108.665337	3273.633367	23.379059
108.817267	3276.682546	23.384077
108.621196	3278.654420	23.389095
108.985041	3296.497678	23.394112
108.849652	3311.049991	23.399130
108.868767	3313.617267	23.404147
109.159647	3313.272580	23.409165
108.971538	3316.245589	23.414183
109.472219	3324.338472	23.419200
109.712420	3336.091522	23.424218
109.442704	3337.153902	23.429235
109.562171	3345.415277	23.434253
109.704419	3350.070956	23.439271
110.166860	3360.657850	23.444288
110.080242	3370.465049	23.449306
110.029121	3370.465021	23.454323
110.360817	3365.960790	23.459341
110.489720	3385.738258	23.464359
111.026997	3386.828747	23.469376
110.521259	3392.407561	23.474394
111.034916	3384.352664	23.479411
111.448835	3377.959781	23.484429
111.447540	3389.783324	23.489447
111.535285	3381.737394	23.494464
111.603956	3379.329432	23.499482
111.728933	3377.649978	23.504499
111.987059	3377.546189	23.509517
111.926862	3384.605436	23.514535
112.117570	3366.509152	23.519552
111.831664	3380.623508	23.524570
111.868990	3375.037378	23.529587
112.317079	3389.852675	23.534605
112.265780	3399.682372	23.539623
112.399588	3397.689214	23.544640
112.575110	3407.701321	23.549658
112.548631	3402.550630	23.554675
112.752949	3392.196909	23.559693
112.699670	3395.147132	23.564711
113.062875	3408.874871	23.569728
112.830488	3418.061774	23.574746
113.078624	3429.590720	23.579763
113.461825	3421.947287	23.584781
113.066951	3434.174100	23.589799
113.165112	3422.139013	23.594816
113.373790	3441.509555	23.599834
113.587143	3445.191932	23.604851
114.022268	3449.700533	23.609869
113.719815	3447.134529	23.614887
114.325251	3440.253842	23.619904
114.189995	3462.885039	23.624922
114.370629	3471.208765	23.629939
114.697004	3469.998639	23.634957
114.437715	3477.877709	23.639975
114.888674	3460.947639	23.644992
114.886319	3476.607246	23.650010
114.856761	3467.835415	23.655027
114.948340	3469.598073	23.660045
114.885923	3478.107092	23.665063
115.023518	3486.632880	23.670080
115.100842	3500.753522	23.675098
115.223773	3498.354242	23.680115
115.453592	3493.983060	23.685133
115.232058	3524.962622	23.690151
115.660342	3520.083596	23.695168
116.045868	3530.596766	23.700186
116.031455	3532.019134	23.705203
116.195182	3526.129631	23.710221
116.150566	3538.260123	23.715239
115.948173	3528.444819	23.720256
116.448719	3547.928422	23.725274
116.359081	3558.163452	23.730291
116.689215	3550.945751	23.735309
116.652248	3549.893651	23.740327
117.018995	3554.763290	23.745344
116.914441	3559.234826	23.750362
116.860266	3575.013392	23.755379
117.306542	3565.506844	23.760397
116.899437	3587.967628	23.765415
117.283642	3582.639954	23.770432
117.448087	3594.464850	23.775450
117.247430	3610.061473	23.780467
117.222363	3609.462166	23.785485
117.560783	3619.011462	23.790503
117.904956	3632.273612	23.795520
118.233191	3631.444311	23.800538
118.255892	3634.315802	23.805555
118.529659	3626.780626	23.810573
118.497911	3636.304039	23.815591
118.271712	3636.422486	23.820608
119.071806	3641.208323	23.825626
119.673006	3635.676834	23.830643
120.058558	3630.866694	23.835661
119.865756	3629.458554	23.840679
120.009352	3619.019882	23.845696
120.041046	3599.024345	23.850714
119.972332	3603.686416	23.855731
120.201235	3586.370626	23.860749
119.874587	3585.391471	23.865767
120.159157	3597.503527	23.870784
120.479105	3590.115435	23.875802
120.274943	3593.808565	23.880819
120.256726	3591.752842	23.885837
120.257164	3610.828244	23.890855
120.363550	3617.250789	23.895872
120.660419	3620.927991	23.900890
120.205791	3626.466892	23.905907
120.883955	3636.585793	23.910925
120.361821	3655.808337	23.915943
120.803309	3658.031824	23.920960
121.072234	3644.136089	23.925978
120.779712	3671.757672	23.930995
121.216272	3683.043656	23.936013
121.188157	3686.425235	23.941031
121.201578	3696.347131	23.946048
121.415692	3713.870829	23.951066
121.691000	3718.987634	23.956083
121.591029	3718.741362	23.961101
121.750126	3745.687558	23.966119
121.945976	3752.004334	23.971136
122.368099	3752.981297	23.976154
122.190645	3776.438168	23.981171
122.862670	3769.738029	23.986189
123.002071	3779.999715	23.991207
123.108847	3777.546772	23.996224
123.010478	3772.961123	24.001242
123.002993	3778.227318	24.006259
123.466127	3783.678329	24.011277
123.863656	3798.979248	24.016295
123.780360	3800.237083	24.021312
124.048053	3799.049286	24.026330
123.911680	3794.359696	24.031347
124.190022	3795.842112	24.036365
124.053433	3786.062172	24.041383
124.117047	3783.674676	24.046400
124.610502	3781.752032	24.051418
124.556589	3785.656094	24.056435
124.772252	3782.354638	24.061453
124.659243	3786.882769	24.066471
124.632498	3786.912157	24.071488
124.923157	3787.581009	24.076506
124.620858	3808.016176	24.081523
124.872364	3806.817288	24.086541
125.261579	3816.872502	24.091559
125.134537	3817.483983	24.096576
125.171199	3816.096754	24.101594
125.076978	3845.379993	24.106611
125.407916	3848.442849	24.111629
125.480616	3847.587098	24.116647
125.584415	3868.132044	24.121664
125.926648	3876.710269	24.126682
125.582739	3888.800208	24.131699
126.268116	3892.804300	24.136717
126.382889	3897.678910	24.141735
126.590628	3895.233583	24.146752
126.883978	3897.247442	24.151770
126.856189	3899.496189	24.156787
126.865934	3903.515701	24.161805
127.104384	3924.016293	24.166823
127.460875	3931.073870	24.171840
127.502727	3925.966383	24.176858
127.289791	3938.477959	24.181875
127.760394	3926.256165	24.186893
127.616592	3942.379566	24.191911
127.865128	3954.930229	24.196928
128.510805	3950.259466	24.201946
128.078585	3961.651443	24.206963
128.544502	3949.841095	24.211981
128.340597	3955.679040	24.216999
128.504910	3956.566953	24.222016
128.631088	3964.243212	24.227034
128.834764	3974.330150	24.232051
128.862972	3973.642043	24.237069
129.245652	3967.478949	24.242087
129.436158	3968.201466	24.247104
129.332705	3961.752183	24.252122
128.915068	3983.872323	24.257139
129.201711	3987.131965	24.262157
129.474485	3994.194427	24.267175
129.399538	4003.514583	24.272192
129.832905	4021.585341	24.277210
130.321146	4031.412003	24.282227
130.382138	4029.176502	24.287245
130.336606	4021.336670	24.292263
130.234139	4039.525239	24.297280
130.496319	4042.564124	24.302298
130.304144	4065.046965	24.307315
130.885017	4065.515217	24.312333
131.030953	4070.347689	24.317351
130.888584	4083.338667	24.322368
131.636024	4069.832787	24.327386
132.666881	4060.044911	24.332403
132.950627	4037.744800	24.337421
133.080951	4029.262662	24.342439
132.869676	4030.642978	24.347456
132.899732	4016.637771	24.352474
132.873831	4012.198691	24.357491
132.715652	3995.599229	24.362509
133.084159	3987.655957	24.367527
132.580650	3981.790541	24.372544
132.813010	3975.516579	24.377562
132.679444	3986.641197	24.382579
132.737591	4002.740944	24.387597
133.142374	4010.271700	24.392615
132.911471	4012.387659	24.397632
133.311152	4013.625098	24.402650
133.115668	4011.157380	24.407667
133.039815	4017.705270	24.412685
133.657407	4028.845265	24.417703
133.498627	4046.937282	24.422720
133.386271	4046.005566	24.427738
133.804087	4058.969187	24.432755
133.874216	4071.257426	24.437773
133.920091	4081.729763	24.442791
133.508525	4086.666307	24.447808
134.343091	4087.459775	24.452826
133.803573	4112.880343	24.457843
134.294289	4132.361194	24.462861
134.524113	4135.989417	24.467879
134.395309	4149.458974	24.472896
134.753650	4166.486308	24.477914
134.930035	4171.084585	24.482931
135.238232	4181.861083	24.487949
135.396456	4201.227564	24.492967
135.656616	4205.427620	24.497984
135.854578	4194.864947	24.503002
135.811584	4202.299318	24.508019
135.956556	4221.666451	24.513037
136.574357	4225.495220	24.518055
136.357801	4237.101594	24.523072
136.283283	4230.149285	24.528090
136.320674	4246.464573	24.533107
136.583754	4257.715622	24.538125
136.975326	4257.230151	24.543143
136.970402	4271.683710	24.548160
137.239404	4283.844169	24.553178
137.411634	4286.455462	24.558195
137.027738	4292.164363	24.563213
137.420752	4296.826692	24.568231
137.420978	4313.037972	24.573248
138.251604	4311.226586	24.578266
138.691653	4308.691007	24.583283
138.817889	4301.310755	24.588301
139.422246	4292.696543	24.593319
138.998100	4298.187690	24.598336
139.292186	4294.977049	24.603354
139.308101	4303.035634	24.608371
139.081531	4289.012192	24.613389
139.191355	4283.868879	24.618407
139.167973	4291.867049	24.623424
139.407878	4295.848414	24.628442
139.823475	4304.228829	24.633459
139.925989	4311.438252	24.638477
140.634369	4303.946294	24.643495
140.428886	4300.041385	24.648512
140.240799	4300.377551	24.653530
140.668012	4305.505927	24.658547
140.706086	4299.114494	24.663565
140.874523	4292.179272	24.668583
141.074665	4294.576447	24.673600
141.011917	4294.011333	24.678618
140.987484	4295.952051	24.683635
141.176167	4293.082599	24.688653
141.391365	4300.398507	24.693671
141.283556	4328.904471	24.698688
141.532060	4320.817169	24.703706
141.369971	4325.426850	24.708723
141.392036	4329.268019	24.713741
141.654307	4335.701968	24.718759
141.604447	4343.976262	24.723776
141.866859	4354.021790	24.728794
142.169347	4355.298642	24.733811
141.883036	4371.226839	24.738829
142.007985	4379.505965	24.743847
142.100775	4397.305357	24.748864
142.451616	4401.818008	24.753882
142.907576	4416.627464	24.758899
142.460587	4418.148574	24.763917
142.785826	4422.886782	24.768935
143.095830	4441.147846	24.773952
143.242927	4446.468512	24.778970
143.762856	4459.660027	24.783987
143.884424	4469.238402	24.789005
144.116404	4458.145403	24.794023
144.201634	4469.871116	24.799040
144.324494	4462.194451	24.804058
144.562161	4467.026766	24.809075
144.688371	4484.553730	24.814093
145.211612	4484.448015	24.819111
145.321721	4490.990005	24.824128
145.358842	4483.814273	24.829146
145.538891	4479.371944	24.834163
145.179511	4486.474710	24.839181
145.632942	4478.034322	24.844199
145.596496	4482.875968	24.849216
145.708124	4490.623419	24.854234
145.924189	4497.910138	24.859251
145.767291	4506.122763	24.864269
146.128249	4505.198992	24.869287
145.940009	4513.726331	24.874304
146.399279	4530.228543	24.879322
147.004895	4536.003054	24.884339
146.669609	4540.382481	24.889357
146.984165	4531.994282	24.894375
146.780787	4543.056078	24.899392
147.173588	4565.606625	24.904410
147.016029	4559.838250	24.909427
146.991509	4583.903303	24.914445
147.053510	4583.653726	24.919463
147.269829	4600.757901	24.924480
147.928684	4600.457967	24.929498
148.664942	4599.226899	24.934515
148.658277	4615.682200	24.939533
149.155441	4608.248827	24.944551
149.133850	4601.737242	24.949568
149.262453	4605.763171	24.954586
149.438932	4605.143328	24.959603
149.309815	4611.102180	24.964621
149.546415	4610.869265	24.969639
149.557093	4611.246435	24.974656
149.460431	4608.830715	24.979674
149.906206	4615.194121	24.984691
149.855258	4638.182358	24.989709
149.857079	4629.029398	24.994727
150.122143	4637.309003	24.999744
150.089093	4638.915703	25.004762
150.183904	4627.523276	25.009779
150.200167	4658.326162	25.014797
150.685541	4650.914417	25.019815
150.687979	4657.082962	25.024832
150.525927	4659.390750	25.029850
150.715527	4684.793061	25.034867
150.794678	4699.678792	25.039885
151.111162	4697.943356	25.044903
151.178617	4714.295087	25.049920
150.978443	4717.627514	25.054938
151.578666	4736.699119	25.059955
151.578718	4747.757967	25.064973
152.009714	4751.660441	25.069991
152.521767	4754.196442	25.075008
152.353103	4761.101465	25.080026
152.556966	4760.433750	25.085043
152.695630	4774.400045	25.090061
152.796881	4766.641767	25.095079
153.035950	4764.906588	25.100096
153.288973	4791.436538	25.105114
153.248042	4800.202593	25.110131
153.615240	4793.355404	25.115149
154.077953	4788.098944	25.120167
154.294858	4776.278958	25.125184
154.448217	4778.502059	25.130202
154.672338	4778.063304	25.135219
154.686342	4772.125368	25.140237
155.007196	4769.518171	25.145255
154.880160	4765.624523	25.150272
154.848306	4771.155385	25.155290
154.988024	4766.953579	25.160307
154.758336	4788.221021	25.165325
155.106771	4791.318963	25.170343
155.383315	4788.591543	25.175360
155.204460	4804.559812	25.180378
155.469794	4815.310008	25.185395
155.507840	4826.498057	25.190413
155.521772	4837.245154	25.195431
155.957032	4841.079214	25.200448
156.176179	4856.466338	25.205466
156.059592	4861.921532	25.210483
156.008177	4880.195127	25.215501
156.287739	4895.210763	25.220519
156.839418	4895.423220	25.225536
156.494633	4912.570575	25.230554
157.363775	4915.659193	25.235571
157.424384	4920.711660	25.240589
157.562494	4926.918407	25.245607
158.080469	4931.344374	25.250624
157.934982	4936.277521	25.255642
158.121293	4934.479424	25.260659
158.224738	4941.251889	25.265677
157.917402	4956.481670	25.270695
158.229995	4963.212302	25.275712
158.357761	4976.805711	25.280730
158.869514	4982.374684	25.285747
158.775996	5000.687706	25.290765
158.923512	5004.439675	25.295783
159.023617	5016.272795	25.300800
159.056433	5026.460080	25.305818
159.747146	5024.820721	25.310835
160.244943	5025.403625	25.315853
160.110008	5045.265624	25.320871
160.294236	5046.309381	25.325888
160.254998	5065.258470	25.330906
160.335702	5059.948843	25.335923
160.439800	5068.283777	25.340941
160.949376	5080.349750	25.345959
161.008374	5081.150486	25.350976
160.967631	5086.442730	25.355994
161.530120	5091.656784	25.361011
161.459287	5081.653252	25.366029
161.205538	5099.198364	25.371047
161.815864	5107.801238	25.376064
161.490485	5124.218675	25.381082
161.844529	5122.666756	25.386099
162.088567	5138.605254	25.391117
162.019630	5146.448402	25.396135
162.368845	5145.519461	25.401152
162.463489	5167.862100	25.406170
162.945139	5168.696565	25.411187
163.086062	5172.560717	25.416205
163.195480	5170.606045	25.421223
163.670494	5167.790451	25.426240
163.738691	5167.087772	25.431258
163.989115	5169.848459	25.436275
163.840591	5186.069608	25.441293
164.246247	5193.029807	25.446311
164.256354	5179.291503	25.451328
164.323327	5188.094972	25.456346
164.485612	5186.689898	25.461363
164.507338	5188.179655	25.466381
164.635513	5212.636132	25.471399
165.117718	5210.408438	25.476416
165.069903	5223.223979	25.481434
164.793208	5213.367195	25.486451
164.934127	5231.585610	25.491469
165.026110	5236.603038	25.496487
165.190581	5253.883506	25.501504
165.439054	5270.123040	25.506522
165.645553	5270.267642	25.511539
166.096776	5294.901323	25.516557
166.454294	5304.676484	25.521575
166.568524	5299.260396	25.526592
166.787239	5312.773614	25.531610
167.128757	5317.465287	25.536627
167.403461	5317.556814	25.541645
166.962155	5333.000600	25.546663
167.387628	5331.306055	25.551680
167.584954	5349.496331	25.556698
167.584422	5354.745754	25.561715
168.170817	5350.231720	25.566733
168.202376	5352.445216	25.571751
168.931010	5351.743830	25.576768
169.190320	5363.368826	25.581786
169.359150	5350.779061	25.586803
169.608046	5358.737254	25.591821
169.663352	5357.168799	25.596839
169.788071	5348.614034	25.601856
169.738987	5352.831136	25.606874
169.834445	5352.908345	25.611891
170.204229	5359.411486	25.616909
170.340654	5359.580335	25.621927
170.292884	5353.518557	25.626944
169.726049	5356.081153	25.631962
169.979417	5353.439397	25.636979
170.188851	5364.763952	25.641997
170.001374	5384.846968	25.647015
170.347941	5404.531747	25.652032
170.542723	5414.786878	25.657050
170.672897	5431.758997	25.662067
171.247607	5440.821620	25.667085
171.511379	5453.341421	25.672103
171.486590	5448.801333	25.677120
171.580683	5470.074958	25.682138
171.940861	5457.985717	25.687156
172.909238	5468.004433	25.692173
172.991779	5480.322034	25.697191
173.480224	5451.778576	25.702208
173.422183	5458.090587	25.707226
173.098975	5450.463938	25.712244
173.543732	5461.017795	25.717261
173.355944	5475.190177	25.722279
173.534570	5465.616709	25.727296
173.810199	5477.392656	25.732314
173.486435	5491.011137	25.737332
173.817883	5497.591588	25.742349
173.918746	5514.348144	25.747367
173.905623	5512.214533	25.752384
173.986412	5519.855781	25.757402
174.482565	5531.602212	25.762420
175.112394	5529.856362	25.767437
174.879651	5545.830397	25.772455
174.937176	5534.525420	25.777472
176.151629	5545.039642	25.782490
176.211222	5533.471268	25.787508
176.583765	5517.327013	25.792525
176.169800	5521.277157	25.797543
176.669597	5516.352960	25.802560
176.489098	5521.708740	25.807578
176.312976	5529.039057	25.812596
176.902176	5542.636613	25.817613
176.515368	5544.332118	25.822631
177.061309	5548.557508	25.827648
176.777048	5541.526058	25.832666
177.044043	5560.653256	25.837684
176.896888	5569.681542	25.842701
176.769653	5583.595868	25.847719
177.217974	5590.996507	25.852736
177.345540	5605.552927	25.857754
177.544654	5621.052029	25.862772
177.880072	5640.440460	25.867789
178.061674	5663.345082	25.872807
178.035536	5664.035556	25.877824
178.244110	5690.069563	25.882842
178.423754	5708.290759	25.887860
178.929222	5725.708830	25.892877
178.460244	5737.448035	25.897895
178.912413	5760.703210	25.902912
179.219635	5772.126011	25.907930
179.358625	5790.417065	25.912948
179.565003	5797.464994	25.917965
180.096604	5827.897059	25.922983
180.357448	5828.616249	25.928000
180.683271	5826.525511	25.933018
180.482791	5853.220822	25.938036
180.779364	5856.553639	25.943053
180.677617	5871.696580	25.948071
181.000441	5884.990576	25.953088
181.053882	5890.077625	25.958106
181.202854	5915.245305	25.963124
181.690438	5921.198260	25.968141
181.713304	5932.123406	25.973159
182.421629	5937.735671	25.978176
182.737567	5945.207308	25.983194
183.150346	5936.983196	25.988212
183.558041	5942.521765	25.993229
183.940652	5962.157147	25.998247
183.585096	5957.921548	26.003264
183.967910	5952.700039	26.008282
183.852326	5955.648491	26.013300
184.247363	5956.458017	26.018317
184.180071	5958.287920	26.023335
184.635244	5954.063311	26.028352
184.312212	5961.438718	26.033370
184.282152	5968.070776	26.038388
184.685696	5976.076044	26.043405
184.708521	5986.745262	26.048423
184.869848	5990.010795	26.053440
185.192349	6002.848919	26.058458
185.186313	6024.090310	26.063476
185.466706	6012.736931	26.068493
185.597955	6040.215452	26.073511
185.771894	6036.168297	26.078528
185.678355	6047.479892	26.083546
185.798907	6065.340354	26.088564
186.443177	6063.141537	26.093581
186.434165	6080.283191	26.098599
186.587220	6094.171868	26.103616
186.947450	6099.586061	26.108634
186.938317	6102.245913	26.113652
187.215080	6116.482657	26.118669
187.590361	6122.050304	26.123687
188.047949	6114.498367	26.128704
188.422213	6115.231805	26.133722
188.248752	6143.380990	26.138740
188.493303	6145.531639	26.143757
188.375854	6143.331004	26.148775
188.711743	6141.952920	26.153792
188.684217	6157.815496	26.158810
188.789763	6174.824800	26.163828
189.350883	6171.416616	26.168845
189.319269	6176.257190	26.173863
190.007445	6185.984259	26.178880
190.345744	6185.104334	26.183898
190.390379	6193.017343	26.188916
190.745428	6187.164764	26.193933
190.492820	6190.163595	26.198951
190.358205	6213.971401	26.203968
190.885580	6216.107356	26.208986
190.871006	6230.517845	26.214004
191.352130	6233.230150	26.219021
191.309641	6260.923014	26.224039
191.347747	6260.237890	26.229056
192.066286	6267.971220	26.234074
191.878060	6286.284929	26.239092
192.014029	6277.924699	26.244109
192.451634	6289.827926	26.249127
192.598517	6302.554493	26.254144
192.970459	6301.721743	26.259162
193.071158	6313.964516	26.264180
193.276282	6309.227665	26.269197
193.659131	6337.145345	26.274215
193.632054	6329.371394	26.279232
193.992598	6331.463413	26.284250
193.996789	6336.890381	26.289268
194.135719	6349.554510	26.294285
194.590917	6363.186860	26.299303
194.557728	6360.208195	26.304320
194.560129	6365.477945	26.309338
194.792826	6383.372116	26.314356
194.691126	6388.230701	26.319373
194.691914	6409.016226	26.324391
194.804444	6416.406106	26.329408
195.213905	6436.529886	26.334426
195.229736	6456.203989	26.339444
195.838298	6462.568672	26.344461
195.718166	6476.541674	26.349479
195.840129	6504.393518	26.354496
196.401182	6502.717284	26.359514
196.620006	6523.142223	26.364532
196.868410	6535.097554	26.369549
197.340952	6542.549755	26.374567
197.362928	6550.682520	26.379584
197.896198	6560.182731	26.384602
198.125956	6571.696173	26.389620
198.029538	6572.373948	26.394637
198.414707	6583.083389	26.399655
198.462808	6592.764268	26.404672
198.857514	6595.401207	26.409690
199.046219	6588.770368	26.414708
199.429157	6600.314300	26.419725
199.795910	6600.670945	26.424743
199.815043	6603.226941	26.429760
200.363486	6608.880198	26.434778
200.396651	6609.945226	26.439796
200.199976	6604.377931	26.444813
200.543210	6608.805851	26.449831
200.501028	6611.799726	26.454848
200.590927	6604.382694	26.459866
200.610533	6633.962527	26.464884
200.767247	6630.211874	26.469901
200.886375	6643.552961	26.474919
201.041542	6669.566740	26.479936
201.247627	6675.187117	26.484954
201.139069	6693.618018	26.489972
201.650465	6705.350983	26.494989
201.780605	6711.573937	26.500007
201.858563	6739.787160	26.505024
202.500179	6737.557980	26.510042
202.396645	6763.362065	26.515060
202.562785	6760.316334	26.520077
203.209607	6781.770044	26.525095
203.303234	6795.809414	26.530112
203.762218	6787.801669	26.535130
204.039019	6795.009263	26.540148
204.195271	6827.674024	26.545165
204.380211	6826.757326	26.550183
204.333708	6825.454541	26.555200
204.759249	6841.658397	26.560218
205.075911	6854.795131	26.565236
205.028591	6848.353845	26.570253
205.339484	6860.666873	26.575271
205.124620	6878.505222	26.580288
205.534157	6883.566503	26.585306
205.586654	6904.445692	26.590324
206.027812	6911.339324	26.595341
205.849842	6912.496166	26.600359
205.709023	6931.974771	26.605376
206.150899	6950.854051	26.610394
206.279894	6973.485757	26.615412
206.298906	6983.560024	26.620429
207.060203	6989.423799	26.625447
207.137280	7010.366781	26.630464
207.566463	7028.716595	26.635482
207.860168	7047.309486	26.640500
208.360874	7049.761905	26.645517
208.683763	7050.924539	26.650535
208.821613	7064.925293	26.655552
208.916217	7064.734062	26.660570
209.150927	7079.611155	26.665588
209.227872	7073.653233	26.670605
209.599357	7090.787104	26.675623
209.458919	7105.539093	26.680640
209.743425	7108.422065	26.685658
209.708582	7127.075944	26.690676
210.117611	7132.287046	26.695693
210.434032	7153.140036	26.700711
210.222016	7163.464688	26.705728
210.824490	7172.441001	26.710746
211.242381	7189.419186	26.715764
211.105970	7192.647010	26.720781
211.993464	7191.960916	26.725799
211.974251	7214.355298	26.730816
212.194503	7215.750033	26.735834
212.442129	7228.920604	26.740852
212.717608	7221.254265	26.745869
212.771985	7234.506575	26.750887
212.826624	7245.766833	26.755904
212.924508	7256.871831	26.760922
213.213545	7259.594969	26.765940
213.163145	7287.470528	26.770957
213.853332	7279.635218	26.775975
213.776257	7291.169449	26.780992
213.919556	7305.529476	26.786010
214.036749	7318.310629	26.791028
214.211431	7319.560137	26.796045
214.895665	7330.316490	26.801063
214.901865	7340.673524	26.806080
214.986747	7352.348664	26.811098
215.295290	7346.249759	26.816116
214.905213	7368.386973	26.821133
215.434164	7375.268584	26.826151
215.572142	7395.781336	26.831168
215.909371	7392.136779	26.836186
215.844743	7418.293067	26.841204
216.022725	7439.417556	26.846221
216.665142	7444.667176	26.851239
216.739859	7466.324790	26.856256
216.925455	7490.901278	26.861274
217.206291	7492.986221	26.866292
217.338637	7506.408545	26.871309
217.988061	7518.906866	26.876327
218.366640	7524.685565	26.881344
218.621222	7535.622938	26.886362
218.643807	7554.955425	26.891380
218.625537	7557.744644	26.896397
218.969656	7568.862508	26.901415
218.855775	7588.646212	26.906432
219.077210	7586.349681	26.911450
219.774999	7608.486848	26.916468
219.607164	7622.007196	26.921485
220.195017	7625.766183	26.926503
220.099572	7642.807307	26.931520
220.709974	7644.928883	26.936538
221.372156	7643.857223	26.941556
222.014602	7646.543763	26.946573
223.046622	7635.837853	26.951591
223.335281	7612.054585	26.956608
223.650647	7583.840899	26.961626
223.917543	7575.813480	26.966644
223.754150	7573.986552	26.971661
223.947200	7550.609954	26.976679
223.466534	7542.238093	26.981696
223.701807	7534.928017	26.986714
223.937835	7535.722307	26.991732
223.971419	7541.580393	26.996749
224.280931	7537.225979	27.001767
224.100405	7536.166744	27.006784
224.035533	7542.279070	27.011802
224.128583	7559.444748	27.016820
224.103652	7573.282379	27.021837
224.413341	7586.836779	27.026855
224.118177	7610.868701	27.031872
224.391531	7621.437527	27.036890
224.749893	7646.390423	27.041908
224.821268	7680.132848	27.046925
225.260580	7687.988901	27.051943
225.251614	7716.542832	27.056960
225.804935	7729.601587	27.061978
225.769516	7742.429707	27.066996
225.840953	7766.192996	27.072013
226.446731	7764.192556	27.077031
226.328010	7790.026823	27.082048
226.961632	7817.273712	27.087066
227.406924	7824.368710	27.092084
227.291939	7836.568939	27.097101
227.668353	7845.341377	27.102119
227.809081	7868.401705	27.107136
228.278883	7883.646945	27.112154
228.504681	7887.514205	27.117172
229.118944	7900.096654	27.122189
229.633136	7901.028280	27.127207
229.401695	7899.292178	27.132224
229.968567	7903.639984	27.137242
230.305332	7897.872531	27.142260
230.371815	7903.634698	27.147277
230.521288	7909.620176	27.152295
230.592204	7909.303690	27.157312
230.650608	7920.928507	27.162330
230.938196	7932.909893	27.167348
230.652426	7955.128263	27.172365
231.054309	7960.722079	27.177383
231.447792	7976.491311	27.182400
231.388968	7985.873360	27.187418
231.493599	8011.967841	27.192436
231.356903	8028.996539	27.197453
231.417226	8041.222148	27.202471
231.669225	8065.671123	27.207488
231.874466	8095.270092	27.212506
232.790243	8124.290243	27.217524
232.799491	8154.585930	27.222541
234.528151	8149.159786	27.227559
234.473518	8149.638480	27.232576
234.776175	8163.992498	27.237594
235.239382	8158.964877	27.242612
234.834767	8165.748310	27.247629
235.351457	8162.603108	27.252647
235.450343	8184.330941	27.257664
235.553444	8190.422694	27.262682
235.855975	8196.678243	27.267700
235.817049	8201.422971	27.272717
236.304790	8218.226022	27.277735
236.627692	8219.770001	27.282752
236.446161	8236.476316	27.287770
237.235824	8249.322146	27.292788
236.985464	8259.969751	27.297805
237.256021	8258.226608	27.302823
237.633186	8271.636470	27.307840
237.922945	8276.201360	27.312858
238.549179	8288.878234	27.317876
238.557583	8303.233218	27.322893
239.199428	8299.275534	27.327911
239.269589	8292.773180	27.332928
239.158713	8307.029041	27.337946
239.579154	8307.816364	27.342964
239.724464	8324.587411	27.347981
239.857898	8324.272345	27.352999
239.834015	8349.277253	27.358016
240.081083	8358.892277	27.363034
240.387621	8365.786073	27.368052
240.550354	8392.197641	27.373069
240.861375	8400.593691	27.378087
241.107908	8415.167584	27.383104
240.930832	8437.556043	27.388122
241.438725	8438.518685	27.393140
241.490809	8466.104359	27.398157
241.574725	8481.817609	27.403175
241.770962	8496.696121	27.408192
242.149935	8522.052649	27.413210
242.230557	8529.362953	27.418228
242.254920	8562.911821	27.423245
242.705249	8573.919004	27.428263
242.941894	8596.464236	27.433280
243.277813	8631.564527	27.438298
244.254750	8610.751778	27.443316
244.882489	8627.883333	27.448333
244.905106	8626.763486	27.453351
245.522822	8634.846386	27.458368
245.273809	8630.996466	27.463386
245.876479	8625.837609	27.468404
245.885623	8631.418934	27.473421
246.175676	8639.864283	27.478439
246.137645	8654.093383	27.483456
246.008798	8663.518186	27.488474
246.474870	8668.549384	27.493492
246.231166	8679.456115	27.498509
246.254375	8697.215188	27.503527
246.917543	8714.098324	27.508544
246.658004	8733.528743	27.513562
247.122368	8741.150350	27.518580
247.276920	8768.647049	27.523597
247.158117	8785.337211	27.528615
247.694798	8799.162941	27.533632
247.835239	8826.193373	27.538650
248.306593	8841.090303	27.543668
250.801806	8826.318344	27.548685
251.393242	8805.838018	27.553703
251.657741	8795.607847	27.558720
251.602208	8785.163023	27.563738
251.679577	8781.142251	27.568756
251.776832	8782.393714	27.573773
251.760081	8771.714008	27.578791
252.069702	8752.600835	27.583808
251.617691	8752.674499	27.588826
252.055215	8758.404474	27.593844
252.461283	8765.708078	27.598861
252.447208	8773.937772	27.603879
252.783095	8773.396063	27.608896
252.422255	8783.001277	27.613914
252.738907	8795.336909	27.618932
252.513381	8817.281782	27.623949
252.595040	8833.075316	27.628967
252.918621	8851.497567	27.633984
252.886116	8877.446094	27.639002
252.987022	8903.626154	27.644020
253.142445	8921.996862	27.649037
254.045932	8948.450914	27.654055
254.521460	8966.777154	27.659072
254.681944	8980.034555	27.664090
255.050868	8994.988037	27.669108
255.447796	9011.527363	27.674125
255.441462	9031.152399	27.679143
255.924262	9052.500948	27.684160
256.041244	9070.752960	27.689178
256.158157	9092.776808	27.694196
256.566883	9093.678771	27.699213
256.992122	9116.926022	27.704231
257.874069	9114.966982	27.709248
258.251303	9118.776298	27.714266
258.742964	9127.987991	27.719284
258.542887	9145.011076	27.724301
258.729459	9141.871697	27.729319
259.155055	9135.720372	27.734336
259.073820	9136.624180	27.739354
259.844812	9138.850845	27.744372
260.200967	9145.101012	27.749389
260.195135	9151.364846	27.754407
260.482551	9144.388841	27.759424
260.527696	9170.380086	27.764442
260.275790	9171.357155	27.769460
260.625858	9186.034293	27.774477
261.110414	9205.701662	27.779495
261.031187	9221.902015	27.784512
260.990790	9239.391812	27.789530
261.348944	9257.447989	27.794548
261.559742	9274.063416	27.799565
261.715969	9288.998157	27.804583
261.855143	9305.369491	27.809600
262.015962	9325.625693	27.814618
262.139893	9350.102643	27.819636
262.856006	9364.371718	27.824653
263.008828	9400.893758	27.829671
263.266843	9398.919398	27.834688
263.263994	9429.053288	27.839706
263.603996	9441.288645	27.844724
263.893345	9460.577540	27.849741
264.255807	9486.151832	27.854759
264.693060	9511.641263	27.859776
264.972785	9525.579643	27.864794
265.710835	9531.669615	27.869812
265.798246	9548.167964	27.874829
265.797059	9567.808557	27.879847
266.256491	9578.519507	27.884864
266.407095	9599.747517	27.889882
266.735153	9605.847339	27.894900
267.238258	9636.992582	27.899917
267.195297	9645.129049	27.904935
267.495050	9653.767122	27.909952
267.737761	9676.109619	27.914970
267.834166	9697.003286	27.919988
268.604695	9707.490897	27.925005
268.903588	9722.700124	27.930023
269.217311	9732.186735	27.935040
269.376460	9750.360826	27.940058
269.649411	9755.277142	27.945076
270.015532	9771.819224	27.950093
269.739219	9796.516185	27.955111
270.634486	9801.273186	27.960128
270.583476	9827.664339	27.965146
270.372688	9843.511396	27.970164
270.587396	9863.950760	27.975181
271.178203	9888.866183	27.980199
271.973313	9900.889988	27.985216
272.081098	9916.030312	27.990234
272.109989	9930.609450	27.995252
272.781407	9940.734749	28.000269
272.698851	9967.872696	28.005287
273.154679	9973.546500	28.010304
273.385973	9994.378752	28.015322
273.775197	10010.539095	28.020340
274.294397	10029.133456	28.025357
274.480087	10034.215615	28.030375
274.498412	10042.156966	28.035392
274.650615	10063.207278	28.040410
275.224517	10075.960454	28.045428
275.970071	10088.613429	28.050445
275.882472	10098.508057	28.055463
276.600380	10107.597645	28.060480
276.733638	10123.223951	28.065498
276.817325	10122.885606	28.070516
277.000580	10126.717154	28.075533
277.289250	10137.343406	28.080551
277.592737	10152.315146	28.085568
277.662491	10157.138509	28.090586
277.731777	10183.406267	28.095604
278.217908	10194.385779	28.100621
278.341457	10212.921614	28.105639
278.685161	10228.368888	28.110656
278.902931	10238.602836	28.115674
278.942218	10270.290394	28.120692
279.107335	10281.829081	28.125709
279.360993	10302.284591	28.130727
279.772037	10323.207154	28.135744
280.049758	10331.608969	28.140762
280.255689	10355.317517	28.145780
280.420065	10375.637479	28.150797
280.789262	10394.573892	28.155815
281.404406	10407.873535	28.160832
281.527067	10420.422278	28.165850
281.730698	10442.036504	28.170868
282.239531	10450.538642	28.175885
282.212764	10482.461334	28.180903
282.399992	10494.478652	28.185920
282.641540	10506.175761	28.190938
283.067951	10533.334093	28.195956
283.408924	10554.529372	28.200973
283.327202	10577.844852	28.205991
283.313505	10600.332866	28.211008
283.850093	10618.945507	28.216026
284.516565	10647.962834	28.221044
285.141473	10652.870587	28.226061
285.247760	10679.068403	28.231079
285.969284	10687.207589	28.236096
286.290702	10700.716995	28.241114
286.526246	10702.219803	28.246132
286.802369	10710.508633	28.251149
286.942516	10728.311187	28.256167
287.306267	10741.006056	28.261184
287.299353	10764.382646	28.266202
287.368070	10780.991725	28.271220
287.853785	10795.357087	28.276237
288.280808	10814.273358	28.281255
288.436387	10825.764386	28.286272
288.729751	10841.111890	28.291290
288.866761	10871.486021	28.296308
289.203157	10889.905336	28.301325
289.199353	10910.483179	28.306343
289.362041	10935.768376	28.311360
289.766075	10965.277378	28.316378
289.954301	10989.991163	28.321396
289.929235	11014.231467	28.326413
290.776822	11046.577266	28.331431
291.218337	11066.517216	28.336448
291.270452	11079.891263	28.341466
291.329749	11115.721294	28.346484
292.020550	11141.420153	28.351501
292.593639	11169.374565	28.356519
293.007867	11179.942042	28.361536
293.452488	11184.497799	28.366554
293.794033	11208.370219	28.371572
294.643606	11210.299720	28.376589
294.628449	11212.029377	28.381607
294.568719	11231.367365	28.386624
295.442538	11233.732470	28.391642
295.542866	11256.368693	28.396660
295.937947	11272.030613	28.401677
296.188631	11282.518179	28.406695
296.268677	11282.128417	28.411712
296.503783	11292.451549	28.416730
296.395209	11308.269665	28.421748
296.776802	11316.296258	28.426765
296.841509	11343.774472	28.431783
297.066946	11377.202836	28.436800
297.833464	11384.406002	28.441818
297.945854	11402.804817	28.446836
298.304907	11415.638090	28.451853
298.310663	11434.812593	28.456871
298.780280	11459.422045	28.461888
299.390146	11467.900849	28.466906
299.193155	11495.172252	28.471924
299.810713	11504.919859	28.476941
299.782313	11527.831546	28.481959
300.063425	11544.866246	28.486976
300.314164	11552.090572	28.491994
300.328598	11581.725308	28.497012
300.598262	11595.210185	28.502029
300.909239	11619.318353	28.507047
301.633871	11653.323025	28.512064
302.141185	11660.709625	28.517082
302.310006	11678.957559	28.522100
303.031936	11680.054257	28.527117
303.398803	11692.230929	28.532135
303.566483	11702.158976	28.537152
303.803857	11721.824800	28.542170
303.979524	11745.175626	28.547188
304.041938	11748.854302	28.552205
304.395025	11771.064761	28.557223
304.257962	11789.522793	28.562240
304.795903	11822.941130	28.567258
304.943272	11838.121592	28.572276
305.267803	11851.279258	28.577293
306.037299	11871.416266	28.582311
306.558666	11903.794348	28.587328
306.924436	11915.411963	28.592346
306.712556	11940.343374	28.597364
307.247246	11948.710435	28.602381
307.580335	11966.614666	28.607399
308.497603	11978.072944	28.612416
309.028364	11981.711684	28.617434
308.799024	11997.361438	28.622452
309.088880	12011.700548	28.627469
309.250192	12027.457193	28.632487
309.428385	12040.927698	28.637504
310.168185	12051.528331	28.642522
310.825689	12064.307810	28.647540
310.797794	12064.277914	28.652557
311.497777	12077.786253	28.657575
311.973184	12087.778446	28.662592
312.296401	12085.879606	28.667610
312.363835	12095.038216	28.672628
312.590897	12111.204764	28.677645
313.135547	12116.153884	28.682663
313.148399	12130.162498	28.687680
313.446097	12142.842659	28.692698
313.537729	12160.007188	28.697716
313.526996	12170.026619	28.702733
313.769547	12194.154893	28.707751
313.557325	12211.456627	28.712768
314.231714	12226.910763	28.717786
314.520687	12262.065388	28.722804
314.825824	12281.983800	28.727821
315.207092	12294.714805	28.732839
315.574685	12321.627483	28.737856
316.015404	12337.451472	28.742874
316.253228	12376.086418	28.747892
316.398320	12390.585436	28.752909
316.840717	12409.455326	28.757927
316.900960	12439.882974	28.762944
317.459033	12448.287384	28.767962
317.928816	12474.805135	28.772980
319.053942	12487.296101	28.777997
319.305491	12502.908997	28.783015
319.133010	12531.300077	28.788032
320.005308	12528.668592	28.793050
320.231586	12548.910878	28.798068
320.218594	12555.812294	28.803085
320.212362	12583.102683	28.808103
320.293178	12595.124273	28.813120
320.619253	12614.445515	28.818138
320.896255	12632.019413	28.823156
321.096660	12652.059687	28.828173
322.153862	12663.477876	28.833191
322.199936	12674.375396	28.838208
322.625107	12688.100098	28.843226
322.729097	12694.845037	28.848244
323.102343	12721.833083	28.853261
323.078925	12726.823188	28.858279
323.470334	12758.201825	28.863296
323.632333	12758.899955	28.868314
323.862161	12795.149767	28.873332
324.331390	12826.364322	28.878349
324.609547	12833.901422	28.883367
325.246671	12864.405799	28.888384
325.366691	12890.102989	28.893402
325.900574	12913.823053	28.898420
325.887464	12933.347582	28.903437
326.192126	12962.314141	28.908455
326.192369	12997.185809	28.913472
326.550083	13021.395461	28.918490
326.802937	13053.396530	28.923508
327.156339	13087.333514	28.928525
327.759629	13107.372030	28.933543
327.665764	13150.175481	28.938560
328.209296	13174.125982	28.943578
328.568171	13205.039686	28.948596
329.114162	13234.365346	28.953613
329.394757	13255.292895	28.958631
329.612745	13291.466981	28.963648
329.873663	13312.534979	28.968666
330.361418	13345.542443	28.973684
330.968677	13375.381391	28.978701
332.060191	13391.868930	28.983719
332.442795	13400.085509	28.988736
333.140316	13395.287642	28.993754
333.746828	13411.915661	28.998772
333.833790	13428.516540	29.003789
334.051200	13422.975782	29.008807
334.369896	13436.127826	29.013824
334.920213	13454.938455	29.018842
334.668476	13457.561817	29.023860
334.648090	13486.515543	29.028877
335.078751	13492.130170	29.033895
334.945112	13520.521245	29.038912
335.442652	13543.354701	29.043930
335.734810	13560.660749	29.048948
335.779713	13596.314257	29.053965
336.148030	13616.140283	29.058983
336.477622	13645.018814	29.064000
337.095971	13677.556105	29.069018
337.444159	13695.494409	29.074036
337.695399	13725.181963	29.079053
338.034120	13748.212296	29.084071
337.914980	13783.352903	29.089088
338.170124	13796.596171	29.094106
338.677493	13834.707548	29.099124
339.565776	13857.796457	29.104141
340.134571	13877.676177	29.109159
339.895412	13914.521736	29.114176
340.683291	13931.466876	29.119194
341.193442	13958.673780	29.124212
340.995743	13981.044956	29.129229
341.652361	13995.673186	29.134247
341.720130	14024.130963	29.139264
342.345704	14047.027383	29.144282
342.693024	14073.000724	29.149300
342.928164	14099.969869	29.154317
343.223634	14116.428063	29.159335
343.356829	14151.544877	29.164352
343.526025	14170.726970	29.169370
344.300716	14197.308775	29.174388
344.536472	14209.786503	29.179405
344.871829	14230.755063	29.184423
345.056502	14250.903934	29.189440
345.626200	14272.158280	29.194458
345.869058	14291.269964	29.199476
345.887360	14324.792383	29.204493
346.802638	14350.919251	29.209511
346.726623	14377.196654	29.214528
347.089367	14398.004852	29.219546
347.637609	14421.620712	29.224564
347.636075	14446.264106	29.229581
348.183617	14471.741462	29.234599
348.733812	14497.511562	29.239616
349.669783	14496.936984	29.244634
350.859823	14503.954581	29.249652
350.968383	14507.154977	29.254669
351.519960	14506.429913	29.259687
351.963419	14527.347800	29.264704
351.787307	14535.344137	29.269722
352.195196	14540.266298	29.274740
352.103374	14551.396018	29.279757
353.023042	14548.584575	29.284775
352.929937	14565.646785	29.289792
353.123142	14591.551989	29.294810
353.323882	14603.807307	29.299828
353.048502	14642.688906	29.304845
353.738531	14665.172016	29.309863
353.957174	14693.546002	29.314880
353.931586	14713.465592	29.319898
354.280387	14740.424791	29.324916
354.638502	14766.835590	29.329933
355.823509	14797.490561	29.334951
356.253492	14819.854748	29.339968
356.453358	14838.706281	29.344986
356.917095	14863.388065	29.350004
356.931473	14887.220947	29.355021
357.017328	14917.169824	29.360039
357.348767	14939.169131	29.365056
357.637481	14967.339666	29.370074
358.297966	14994.562725	29.375092
358.111787	15033.280699	29.380109
358.897231	15059.313641	29.385127
359.541871	15082.627592	29.390144
359.838829	15115.229020	29.395162
360.177431	15139.150257	29.400180
360.322886	15162.098055	29.405197
360.757723	15194.361513	29.410215
361.483935	15214.572915	29.415232
361.912070	15232.261632	29.420250
362.379660	15267.246479	29.425268
362.219160	15286.839276	29.430285
362.514744	15312.433875	29.435303
363.123014	15334.543762	29.440320
363.138620	15350.931481	29.445338
363.816857	15379.378460	29.450356
364.357760	15406.223307	29.455373
364.994690	15432.632993	29.460391
365.194877	15457.398856	29.465408
365.461183	15480.924380	29.470426
366.427562	15497.775304	29.475444
366.161292	15516.760215	29.480461
366.622707	15540.376353	29.485479
366.796959	15561.352891	29.490496
366.972374	15606.100815	29.495514
367.136470	15618.367706	29.500532
367.521414	15649.496057	29.505549
367.502825	15670.299868	29.510567
368.040431	15701.839554	29.515584
368.657803	15734.606494	29.520602
368.886813	15759.434222	29.525620
369.252908	15788.966155	29.530637
369.748763	15820.896015	29.535655
370.207561	15839.555947	29.540672
370.200419	15865.198543	29.545690
370.801270	15892.049987	29.550708
370.785170	15934.456886	29.555725
371.535645	15961.382888	29.560743
371.902232	15989.381467	29.565760
372.031655	16031.529588	29.570778
372.565189	16050.751080	29.575796
372.815352	16087.742461	29.580813
373.568458	16097.610612	29.585831
374.133640	16131.446220	29.590848
374.570309	16164.184138	29.595866
375.231853	16177.781095	29.600884
375.296125	16203.423386	29.605901
375.692671	16227.855156	29.610919
376.105963	16254.684758	29.615936
376.684904	16267.687092	29.620954
376.957835	16284.236324	29.625972
377.471089	16317.292830	29.630989
377.509995	16336.842713	29.636007
378.352853	16365.243565	29.641024
378.223276	16379.454432	29.646042
378.770168	16407.352841	29.651060
379.199252	16432.610183	29.656077
379.641132	16457.952132	29.661095
379.482710	16487.618159	29.666112
379.718377	16523.451236	29.671130
380.107526	16551.765424	29.676148
380.846640	16570.595566	29.681165
381.519660	16606.901555	29.686183
381.943199	16624.293049	29.691200
381.873855	16652.094053	29.696218
382.947567	16679.473516	29.701236
383.218431	16713.854155	29.706253
383.278830	16732.124164	29.711271
383.523573	16762.513419	29.716288
383.901769	16793.872034	29.721306
384.183786	16820.934008	29.726324
384.573811	16846.501116	29.731341
385.123668	16870.898914	29.736359
385.766701	16903.827850	29.741376
386.109856	16932.586961	29.746394
386.984149	16956.518006	29.751412
387.482317	16972.740479	29.756429
388.083722	16970.601002	29.761447
388.901131	16981.622307	29.766464
389.003132	16990.648657	29.771482
389.321710	17000.794455	29.776500
389.712822	17016.274982	29.781517
389.780838	17034.179937	29.786535
390.069923	17057.251531	29.791552
390.392935	17077.599990	29.796570
390.617862	17092.542304	29.801588
390.369676	17116.310103	29.806605
390.750368	17153.488682	29.811623
391.416194	17179.210682	29.816640
391.414387	17212.253656	29.821658
392.214281	17238.665969	29.826676
392.179171	17280.828841	29.831693
392.659108	17312.247202	29.836711
392.662940	17335.628237	29.841728
392.876422	17379.249144	29.846746
393.637792	17415.201748	29.851764
394.094197	17454.669864	29.856781
394.414135	17480.326835	29.861799
394.799936	17502.277974	29.866816
395.528408	17532.066521	29.871834
396.610945	17544.136568	29.876852
396.914364	17557.798887	29.881869
396.783787	17582.123179	29.886887
397.750052	17591.290035	29.891904
397.924374	17628.015292	29.896922
398.206748	17637.336760	29.901940
398.957568	17674.149214	29.906957
399.179643	17687.525646	29.911975
399.464741	17714.270145	29.916992
399.660803	17733.543354	29.922010
400.347789	17756.948646	29.927028
400.524366	17790.901073	29.932045
400.850783	17821.925013	29.937063
401.511848	17836.089340	29.942080
401.533127	17869.429295	29.947098
401.591687	17897.999324	29.952116
401.917214	17930.215352	29.957133
402.066735	17978.189796	29.962151
402.575035	18011.691900	29.967168
402.676921	18052.829815	29.972186
403.339117	18091.150755	29.977204
403.927545	18126.958652	29.982221
404.255882	18174.077928	29.987239
404.642831	18198.476369	29.992256
405.428354	18247.241340	29.997274
405.969195	18277.106534	30.002292
406.369080	18311.601471	30.007309
406.787097	18346.077704	30.012327
407.315047	18375.689837	30.017344
407.328380	18411.814575	30.022362
407.882794	18440.599536	30.027380
409.289558	18454.300020	30.032397
409.403141	18483.629632	30.037415
410.251914	18501.245682	30.042432
410.156168	18532.162934	30.047450
411.260852	18545.142797	30.052468
411.673710	18561.278531	30.057485
411.987671	18574.815399	30.062503
412.554459	18596.687478	30.067520
412.487722	18617.012707	30.072538
412.780135	18634.785948	30.077556
413.382496	18657.197647	30.082573
413.400964	18685.223929	30.087591
413.767834	18712.462490	30.092608
414.109010	18738.086346	30.097626
414.538795	18765.300355	30.102644
414.971379	18790.830287	30.107661
415.317443	18827.728296	30.112679
415.847162	18847.519628	30.117696
416.242031	18874.006559	30.122714
416.861754	18894.237018	30.127732
418.127589	18903.364312	30.132749
418.864354	18926.015743	30.137767
418.895917	18925.903438	30.142784
419.032728	18959.319392	30.147802
419.404401	18968.445483	30.152820
419.917298	18987.404245	30.157837
420.079736	19017.114493	30.162855
420.247850	19026.889254	30.167872
420.177184	19066.891738	30.172890
420.748461	19089.668621	30.177908
421.132984	19104.234681	30.182925
421.165540	19140.610040	30.187943
421.395721	19169.210492	30.192960
421.865912	19203.875319	30.197978
421.783434	19234.157914	30.202996
422.195216	19272.556277	30.208013
422.343312	19313.145729	30.213031
422.751832	19360.160446	30.218048
423.448600	19401.461420	30.223066
423.741829	19447.084551	30.228084
424.570037	19485.436304	30.233101
424.540781	19540.597619	30.238119
424.782755	19578.315451	30.243136
425.526660	19630.744208	30.248154
425.700808	19672.894128	30.253172
426.587198	19717.136165	30.258189
427.155978	19753.151042	30.263207
427.742129	19781.526299	30.268224
428.437990	19829.982870	30.273242
428.654540	19859.616257	30.278260
430.025849	19866.323898	30.283277
430.594510	19891.522329	30.288295
431.239752	19920.904890	30.293312
431.556795	19946.911408	30.298330
431.503289	19965.219646	30.303348
432.440838	19991.225644	30.308365
432.847993	20013.848168	30.313383
433.650125	20026.165269	30.318400
433.897062	20044.094186	30.323418
433.832375	20072.477141	30.328436
434.459058	20085.934916	30.333453
434.514954	20133.093932	30.338471
434.934432	20149.826055	30.343488
434.790728	20198.309630	30.348506
435.338688	20231.111176	30.353524
436.100363	20259.084436	30.358541
436.247290	20304.180815	30.363559
436.206795	20338.535514	30.368576
436.861356	20374.747169	30.373594
437.253980	20416.211528	30.378612
437.675635	20463.501488	30.383629
437.885676	20507.168974	30.388647
438.247358	20550.656877	30.393664
438.953286	20604.684224	30.398682
439.379575	20644.642606	30.403700
440.316228	20673.512978	30.408717
440.590606	20701.448093	30.413735
441.766332	20733.548804	30.418752
442.151450	20765.170735	30.423770
442.756199	20790.198977	30.428788
443.325057	20817.561926	30.433805
443.511018	20849.188715	30.438823
443.840153	20882.617548	30.443840
444.189410	20906.155892	30.448858
444.654505	20944.815683	30.453876
444.847769	20973.682339	30.458893
444.992980	21019.316982	30.463911
445.675465	21038.500594	30.468928
445.677864	21086.735417	30.473946
445.905559	21125.384601	30.478964
446.543916	21174.233007	30.483981
446.968457	21228.845168	30.488999
447.305811	21262.606070	30.494016
448.063268	21300.410852	30.499034
448.506487	21345.091856	30.504052
449.328829	21370.174693	30.509069
449.944925	21412.378547	30.514087
450.229293	21439.414506	30.519104
451.016162	21470.516941	30.524122
450.981927	21494.584932	30.529140
451.638964	21517.079682	30.534157
452.265934	21535.956164	30.539175
452.839095	21557.329664	30.544192
453.960706	21579.430414	30.549210
454.170919	21617.443481	30.554228
454.348880	21629.598975	30.559245
454.582533	21653.811906	30.564263
454.759229	21688.959483	30.569280
455.303741	21711.443225	30.574298
455.962537	21735.289233	30.579316
456.059271	21770.885440	30.584333
456.338794	21809.907576	30.589351
456.967712	21843.424121	30.594368
457.781918	21859.983591	30.599386
458.310076	21894.325843	30.604404
458.924750	21919.098684	30.609421
458.825946	21950.303385	30.614439
458.885948	21987.586968	30.619456
459.648692	22015.228706	30.624474
459.806704	22060.334243	30.629492
460.194939	22094.805785	30.634509
460.537951	22142.709534	30.639527
460.793360	22188.262805	30.644544
461.696796	22225.017358	30.649562
461.948403	22281.763492	30.654580
462.510429	22315.750928	30.659597
462.957797	22362.989907	30.664615
463.327915	22399.533829	30.669632
464.085405	22434.690557	30.674650
464.604851	22481.627765	30.679668
465.347915	22514.379277	30.684685
465.915569	22547.361818	30.689703
466.291450	22591.951656	30.694720
466.969724	22632.981391	30.699738
467.196660	22664.048153	30.704756
467.527052	22690.220676	30.709773
468.005425	22739.525922	30.714791
468.159121	22770.586121	30.719808
469.141041	22817.991453	30.724826
469.093361	22853.963975	30.729844
469.955911	22898.924763	30.734861
470.371699	22946.779274	30.739879
470.803558	22980.344992	30.744896
471.544999	23020.229842	30.749914
471.793552	23071.091154	30.754932
471.994071	23096.363412	30.759949
472.453887	23148.098136	30.764967
472.947330	23185.613539	30.769984
473.620192	23222.112104	30.775002
473.788727	23274.930019	30.780020
474.222805	23312.015612	30.785037
474.594720	23356.098781	30.790055
475.034555	23418.158351	30.795072
476.184332	23455.464419	30.800090
476.225575	23506.333077	30.805108
476.720026	23548.885725	30.810125
477.288193	23601.275590	30.815143
477.433078	23640.589215	30.820160
478.063450	23683.848157	30.825178
478.851466	23729.709749	30.830196
479.233958	23768.004938	30.835213
479.639942	23811.908589	30.840231
480.037489	23862.048935	30.845248
480.523888	23893.346078	30.850266
480.976049	23953.524268	30.855284
481.476583	23993.110793	30.860301
482.204862	24027.783667	30.865319
482.514435	24072.773171	30.870336
483.341681	24106.978762	30.875354
483.333269	24146.211778	30.880372
483.847383	24193.022128	30.885389
484.562277	24219.087411	30.890407
484.768875	24255.137348	30.895424
485.341145	24298.639314	30.900442
485.866904	24345.224217	30.905460
486.886585	24368.640254	30.910477
488.064784	24386.488492	30.915495
488.617986	24409.392270	30.920512
489.127083	24427.897315	30.925530
489.585498	24461.070450	30.930548
490.383989	24491.468439	30.935565
490.669137	24511.843230	30.940583
490.347650	24535.144769	30.945600
491.044980	24566.304033	30.950618
491.569851	24603.402588	30.955636
491.912406	24637.415347	30.960653
492.177361	24678.329420	30.965671
492.627907	24709.066293	30.970688
493.284351	24749.486570	30.975706
493.388209	24794.452212	30.980724
493.696395	24837.425377	30.985741
494.276460	24868.207259	30.990759
494.453370	24926.263025	30.995776
495.003770	24971.971870	31.000794
495.131557	25019.652931	31.005812
495.740440	25072.739173	31.010829
495.993855	25123.642057	31.015847
496.208841	25192.047288	31.020864
496.986435	25235.151659	31.025882
497.604339	25298.377578	31.030900
497.960780	25362.959276	31.035917
498.833041	25414.687558	31.040935
498.832471	25479.095578	31.045952
499.512890	25539.927460	31.050970
500.368967	25584.088937	31.055988
500.839501	25643.830004	31.061005
501.306986	25697.014205	31.066023
501.555742	25762.498462	31.071040
502.575946	25814.821605	31.076058
504.189515	25848.953712	31.081076
505.388994	25855.832724	31.086093
506.238760	25869.034118	31.091111
507.019241	25899.374518	31.096128
507.556515	25921.753056	31.101146
507.927664	25936.614265	31.106164
507.896975	25962.806036	31.111181
508.602616	25980.053118	31.116199
508.270869	26015.174183	31.121216
508.770321	26035.291241	31.126234
508.952240	26068.056037	31.131252
509.339212	26112.454497	31.136269
509.862468	26154.808541	31.141287
509.831807	26203.478099	31.146304
510.054818	26256.562689	31.151322
510.424469	26299.258029	31.156340
510.792327	26364.475602	31.161357
511.356590	26418.179039	31.166375
511.535303	26481.362380	31.171392
512.524968	26520.476059	31.176410
513.182517	26576.120190	31.181428
513.345770	26633.821228	31.186445
514.198912	26682.701797	31.191463
514.689368	26748.263211	31.196480
515.625679	26792.534334	31.201498
515.796367	26837.377494	31.206516
516.579161	26881.535547	31.211533
517.344898	26917.838881	31.216551
517.532606	26965.808733	31.221568
517.972751	26998.519790	31.226586
518.392400	27050.785553	31.231604
518.868723	27097.528075	31.236621
519.447873	27145.332472	31.241639
519.867730	27205.595231	31.246656
520.543241	27243.655504	31.251674
521.174822	27277.518226	31.256692
521.388047	27326.607836	31.261709
522.228205	27368.230856	31.266727
522.980004	27427.133294	31.271744
523.678388	27455.155730	31.276762
524.687336	27475.549470	31.281780
525.179787	27520.568088	31.286797
525.899683	27552.751091	31.291815
526.333363	27595.451615	31.296832
526.795275	27622.056195	31.301850
527.359685	27651.183210	31.306868
527.893869	27698.157491	31.311885
528.465611	27720.974281	31.316903
528.693883	27761.977471	31.321920
529.090766	27805.653079	31.326938
529.694733	27848.499448	31.331956
530.111225	27887.865991	31.336973
530.428754	27923.665429	31.341991
530.561111	27974.697765	31.347008
531.107136	28030.743648	31.352026
531.634370	28077.404646	31.357044
531.773713	28133.508935	31.362061
532.585298	28188.476502	31.367079
532.816364	28247.780516	31.372096
533.330537	28310.725529	31.377114
533.705560	28369.649573	31.382132
534.083542	28444.217463	31.387149
534.558424	28489.064844	31.392167
535.295662	28558.617519	31.397184
535.697331	28614.395865	31.402202
536.376981	28675.361937	31.407220
536.910849	28745.226748	31.412237
538.567213	28788.045778	31.417255
539.187443	28837.299202	31.422272
540.001303	28885.842331	31.427290
540.598834	28918.855812	31.432308
541.146386	28970.405745	31.437325
541.848191	28996.881102	31.442343
542.568670	29052.418618	31.447360
542.888733	29087.134772	31.452378
543.999486	29122.322256	31.457396
544.141361	29167.580025	31.462413
544.882814	29184.325906	31.467431
545.064492	29222.636580	31.472448
545.603835	29261.247594	31.477466
546.279525	29301.438715	31.482484
546.367522	29336.793326	31.487501
547.489826	29376.882059	31.492519
547.815911	29414.629690	31.497536
548.021089	29447.854456	31.502554
548.811986	29483.171506	31.507572
548.855215	29535.075023	31.512589
549.722006	29576.506464	31.517607
550.463518	29616.526480	31.522624
551.095454	29646.995925	31.527642
552.085169	29691.836620	31.532660
552.066773	29741.734987	31.537677
552.291693	29772.376356	31.542695
552.471981	29822.872947	31.547712
552.822686	29870.624966	31.552730
553.214240	29917.994890	31.557748
553.479523	29980.785336	31.562765
553.880587	30028.926950	31.567783
554.321048	30083.681327	31.572800
554.760477	30152.463195	31.577818
555.683124	30213.321713	31.582836
556.028941	30272.326428	31.587853
557.371608	30291.462851	31.592871
558.263161	30356.318144	31.597888
558.780301	30388.057340	31.602906
559.589669	30434.453776	31.607924
560.396828	30475.575434	31.612941
560.954917	30515.101070	31.617959
561.012624	30561.373415	31.622976
561.463880	30609.388392	31.627994
562.118745	30661.105321	31.633012
562.270717	30716.177761	31.638029
563.106850	30772.058052	31.643047
563.236313	30827.844480	31.648064
563.526809	30884.576125	31.653082
564.365538	30936.212848	31.658100
564.841415	30993.434657	31.663117
565.395611	31054.701190	31.668135
565.921429	31121.260727	31.673152
566.438994	31180.675381	31.678170
567.347662	31222.554952	31.683188
568.131632	31288.005793	31.688205
569.002071	31336.372784	31.693223
569.635928	31390.887714	31.698240
570.002045	31435.322122	31.703258
571.061343	31478.133325	31.708276
571.570457	31515.545862	31.713293
572.598625	31561.277887	31.718311
573.291073	31601.020294	31.723328
573.908664	31643.296283	31.728346
574.122535	31684.017603	31.733364
574.463752	31727.526074	31.738381
575.080112	31771.354975	31.743399
575.706457	31822.430060	31.748416
576.189043	31860.750151	31.753434
577.016569	31907.573424	31.758452
577.554238	31953.040834	31.763469
577.821406	31994.669062	31.768487
578.283280	32048.242739	31.773504
578.616644	32107.340856	31.778522
579.307006	32148.845530	31.783540
580.027621	32203.001470	31.788557
580.513250	32259.742991	31.793575
580.735700	32302.499529	31.798592
581.152828	32370.833063	31.803610
581.740041	32421.152767	31.808628
582.205485	32491.867389	31.813645
583.521320	32535.367462	31.818663
584.641931	32576.817471	31.823680
585.139682	32622.725525	31.828698
586.034130	32664.579328	31.833716
586.285334	32722.266872	31.838733
586.833434	32756.135130	31.843751
587.152324	32798.681210	31.848768
587.498414	32850.831330	31.853786
588.106780	32912.603336	31.858804
588.356627	32968.837221	31.863821
588.919554	33022.438081	31.868839
589.559750	33070.027616	31.873856
590.117150	33139.520980	31.878874
590.844279	33183.562182	31.883892
591.200027	33252.414186	31.888909
591.647523	33294.914852	31.893927
592.384714	33340.343220	31.898944
592.872458	33396.655707	31.903962
593.883189	33442.808877	31.908980
594.375353	33503.298971	31.913997
594.788681	33552.678830	31.919015
595.517879	33603.846100	31.924032
596.532536	33646.313382	31.929050
597.095137	33694.700070	31.934068
597.760196	33745.900488	31.939085
598.111062	33792.609086	31.944103
598.712914	33842.100445	31.949120
598.599372	33903.203693	31.954138
599.441134	33964.432529	31.959156
599.533894	34017.394960	31.964173
600.211900	34091.984234	31.969191
601.189639	34151.758442	31.974208
601.719629	34215.381451	31.979226
602.212969	34269.174337	31.984244
602.678249	34337.677830	31.989261
603.152002	34403.573519	31.994279
603.902561	34476.612338	31.999296
604.665937	34535.511407	32.004314
605.047710	34595.666927	32.009332
605.859352	34662.151242	32.014349
606.062430	34737.355400	32.019367
606.671052	34810.996666	32.024384
607.124003	34887.015189	32.029402
608.029532	34964.208603	32.034420
608.883966	35035.881744	32.039437
609.409550	35113.094707	32.044455
610.335110	35164.274865	32.049472
610.545765	35237.598945	32.054490
611.611746	35295.945320	32.059508
612.394874	35370.203711	32.064525
612.725209	35436.085979	32.069543
613.515429	35503.126103	32.074560
614.241888	35570.243339	32.079578
614.738658	35628.170889	32.084596
615.074761	35684.683019	32.089613
615.375267	35761.409089	32.094631
616.374727	35832.370163	32.099648
617.063243	35905.374600	32.104666
617.728318	35969.467422	32.109684
618.013421	36042.208015	32.114701
618.750175	36111.661035	32.119719
619.215861	36185.063396	32.124736
619.894138	36270.243989	32.129754
620.445806	36336.124354	32.134772
621.202703	36410.239894	32.139789
621.825684	36475.165247	32.144807
622.892567	36535.778436	32.149824
623.969158	36605.827093	32.154842
625.298335	36636.827155	32.159860
626.655795	36681.412994	32.164877
627.208073	36723.550897	32.169895
628.019369	36759.885872	32.174912
628.563135	36803.578212	32.179930
629.071624	36840.304496	32.184948
629.452097	36875.032147	32.189965
629.670739	36926.230544	32.194983
630.441898	36971.930754	32.200000
630.685490	37024.968514	32.205018
630.831852	37084.025722	32.210036
631.632138	37133.395355	32.215053
631.982778	37190.316935	32.220071
632.637434	37242.961984	32.225088
633.003873	37306.320071	32.230106
633.897173	37351.123514	32.235124
634.713870	37416.092674	32.240141
635.061932	37463.344676	32.245159
635.786888	37511.954556	32.250176
636.049964	37570.810902	32.255194
636.846061	37634.240826	32.260212
637.758600	37681.096660	32.265229
638.431295	37739.853976	32.270247
638.843512	37781.667243	32.275264
639.569367	37847.644126	32.280282
640.181782	37896.560953	32.285300
640.474678	37956.764523	32.290317
640.722207	38034.074008	32.295335
641.717859	38091.708819	32.300352
642.007044	38174.643011	32.305370
642.233896	38244.602367	32.310388
642.896527	38320.556318	32.315405
642.986921	38401.292941	32.320423
644.026935	38463.350074	32.325440
644.372856	38557.838735	32.330458
645.217935	38635.199904	32.335476
646.379443	38707.101755	32.340493
648.738848	38757.466905	32.345511
650.565913	38780.626104	32.350528
651.364636	38818.447705	32.355546
651.745692	38849.978312	32.360564
652.617908	38883.883212	32.365581
653.024519	38937.126747	32.370599
653.749235	38970.718549	32.375616
654.011055	39000.514169	32.380634
654.653906	39043.207441	32.385652
655.359312	39082.247737	32.390669
655.772329	39133.470572	32.395687
656.470028	39166.609515	32.400704
656.569714	39211.224189	32.405722
657.127771	39273.859693	32.410740
657.665269	39326.242971	32.415757
657.774010	39390.070920	32.420775
658.385532	39449.721448	32.425792
658.931461	39520.832232	32.430810
659.309526	39587.457135	32.435828
660.180765	39649.764139	32.440845
660.694587	39721.089371	32.445863
661.508114	39774.927526	32.450880
662.312257	39842.189710	32.455898
663.380008	39899.022772	32.460916
664.241325	39950.176612	32.465933
664.712185	40024.108141	32.470951
665.503222	40084.554837	32.475968
665.867600	40154.836430	32.480986
666.401855	40216.816187	32.486004
666.982231	40278.624342	32.491021
667.507058	40355.215722	32.496039
668.159883	40408.141693	32.501056
668.636651	40494.884445	32.506074
668.817649	40567.076365	32.511092
669.943715	40647.376271	32.516109
669.926319	40734.944059	32.521127
670.684532	40816.066580	32.526144
671.885936	40885.362785	32.531162
672.814247	40957.072266	32.536180
673.517689	41017.277705	32.541197
674.498662	41090.112291	32.546215
675.281846	41152.461107	32.551232
675.832172	41225.475065	32.556250
676.048474	41303.990519	32.561268
676.888772	41370.469359	32.566285
677.412139	41456.839529	32.571303
678.207815	41511.954839	32.576320
678.807924	41575.430955	32.581338
679.075049	41639.625549	32.586356
680.120923	41714.428111	32.591373
680.317476	41784.023967	32.596391
680.911771	41857.601385	32.601408
681.406792	41926.504182	32.606426
681.850631	42010.920130	32.611444
683.080690	42086.334502	32.616461
683.123438	42170.401033	32.621479
683.644830	42250.205294	32.626496
684.676579	42334.465117	32.631514
685.615906	42419.501540	32.636532
686.238012	42489.828143	32.641549
687.168385	42575.971775	32.646567
688.040260	42653.222252	32.651584
688.833184	42734.975696	32.656602
689.324433	42822.424684	32.661620
690.108856	42886.528227	32.666637
690.917115	42961.372111	32.671655
691.540932	43039.372597	32.676672
692.081123	43122.078989	32.681690
692.712004	43201.856523	32.686708
693.755880	43285.263018	32.691725
694.173234	43364.293689	32.696743
695.272016	43438.399804	32.701760
696.263749	43520.246820	32.706778
696.826467	43591.392561	32.711796
697.941885	43647.837727	32.716813
698.670632	43714.011954	32.721831
699.165843	43797.587609	32.726848
699.756465	43865.010366	32.731866
700.536989	43942.297138	32.736884
701.614854	43994.913344	32.741901
702.327378	44053.551567	32.746919
703.251175	44127.260059	32.751936
703.862847	44193.676442	32.756954
704.629841	44248.157348	32.761972
705.577158	44319.671419	32.766989
706.245894	44385.194916	32.772007
706.799898	44452.010158	32.777024
707.648402	44507.267658	32.782042
707.706568	44592.144526	32.787060
708.629951	44658.052963	32.792077
709.050333	44730.000253	32.797095
709.278408	44808.190644	32.802112
710.547938	44878.819760	32.807130
710.545702	44960.064490	32.812148
711.529608	45045.282289	32.817165
711.862585	45119.980054	32.822183
712.575453	45205.035172	32.827200
713.294756	45305.454640	32.832218
713.534434	45395.341415	32.837236
714.306934	45479.456366	32.842253
714.774905	45590.310944	32.847271
715.450584	45674.322846	32.852288
716.264876	45768.056799	32.857306
717.294077	45869.621433	32.862324
718.338055	45953.766054	32.867341
719.730040	46016.491075	32.872359
720.926946	46089.012495	32.877376
722.433497	46151.390538	32.882394
722.925704	46222.046382	32.887412
723.666139	46275.009199	32.892429
723.986280	46344.247795	32.897447
724.558697	46410.132211	32.902464
725.456578	46493.081414	32.907482
725.792880	46557.991880	32.912500
726.150618	46627.689472	32.917517
726.849752	46688.715988	32.922535
727.638314	46752.273100	32.927552
728.521292	46814.807386	32.932570
729.225908	46875.378859	32.937588
730.485784	46928.412005	32.942605
730.860929	46994.943837	32.947623
731.664378	47067.164852	32.952640
732.616454	47120.202267	32.957658
733.137346	47200.548698	32.962676
733.746139	47264.150002	32.967693
734.257084	47330.303613	32.972711
734.443398	47393.940751	32.977728
735.423342	47477.395385	32.982746
736.123874	47567.234894	32.987764
736.573782	47641.430537	32.992781
737.146951	47720.962031	32.997799
737.688893	47799.987436	33.002816
738.411919	47897.028272	33.007834
739.219313	47990.682767	33.012852
740.019211	48071.229720	33.017869
740.794885	48165.932510	33.022887
741.203856	48260.109237	33.027904
742.057925	48348.006793	33.032922
742.545324	48443.320963	33.037940
743.840841	48524.728678	33.042957
744.995548	48626.757780	33.047975
745.122557	48714.054495	33.052992
746.688972	48790.848459	33.058010
748.328870	48846.862068	33.063028
749.226472	48930.283033	33.068045
750.471043	48995.707924	33.073063
750.603697	49064.384297	33.078080
751.538100	49132.056133	33.083098
751.887926	49203.280411	33.088116
752.613880	49282.391930	33.093133
753.382946	49355.852728	33.098151
753.385972	49433.783663	33.103168
754.191907	49520.172278	33.108186
754.588627	49604.175182	33.113204
755.418845	49689.613023	33.118221
756.047060	49792.547427	33.123239
756.707491	49877.707927	33.128256
757.241529	49983.533119	33.133274
757.885568	50086.659129	33.138292
758.513534	50189.987339	33.143309
759.454778	50280.800828	33.148327
760.096896	50377.734982	33.153344
761.382170	50465.125297	33.158362
762.196093	50571.949550	33.163380
762.768158	50657.943055	33.168397
764.319770	50744.153353	33.173415
765.403435	50831.995724	33.178432
766.391227	50902.577098	33.183450
767.048356	50985.930021	33.188468
767.507904	51063.580116	33.193485
768.072256	51148.812705	33.198503
768.660674	51233.580517	33.203520
769.517438	51319.226469	33.208538
770.082777	51415.294149	33.213556
770.729676	51504.892473	33.218573
771.763003	51593.403652	33.223591
772.574178	51683.518821	33.228608
773.551515	51768.091738	33.233626
774.247020	51856.060042	33.238644
774.393068	51943.835672	33.243661
775.413010	52034.265268	33.248679
775.623030	52138.545055	33.253696
776.439865	52227.796304	33.258714
777.298241	52326.586920	33.263732
778.033205	52410.950162	33.268749
778.921459	52488.162036	33.273767
779.417189	52591.360721	33.278784
780.028573	52677.716741	33.283802
780.735072	52773.230678	33.288820
781.384579	52874.787995	33.293837
782.661247	52963.486125	33.298855
783.297072	53059.227996	33.303872
783.960765	53147.788641	33.308890
784.676412	53248.509281	33.313908
785.585041	53351.706611	33.318925
786.356683	53454.156436	33.323943
786.906240	53562.235067	33.328960
787.639293	53661.564984	33.333978
788.340751	53769.253095	33.338996
788.814768	53885.401545	33.344013
790.049101	53988.737699	33.349031
791.263042	54087.465538	33.354048
792.449665	54185.680317	33.359066
793.415201	54293.605462	33.364084
794.125710	54392.740631	33.369101
794.746926	54485.572852	33.374119
795.546967	54581.225377	33.379136
796.420051	54685.256986	33.384154
797.288209	54785.239889	33.389172
797.740921	54880.111177	33.394189
798.801558	54983.841534	33.399207
799.970881	55083.554810	33.404224
800.811040	55177.187974	33.409242
801.765074	55279.901350	33.414260
802.206362	55374.663172	33.419277
802.858173	55476.233527	33.424295
803.647256	55577.674200	33.429312
804.905803	55669.944927	33.434330
805.673161	55767.036628	33.439348
806.324190	55866.934664	33.444365
807.427031	55969.216195	33.449383
808.406342	56059.936448	33.454400
809.077278	56151.131663	33.459418
810.212879	56231.008972	33.464436
810.929591	56332.389689	33.469453
811.854742	56410.312212	33.474471
812.663936	56508.556946	33.479488
813.467352	56597.160418	33.484506
814.081870	56692.582215	33.489524
814.830590	56781.018652	33.494541
815.569154	56867.725754	33.499559
816.612982	56977.908414	33.504576
817.241479	57070.732563	33.509594
817.924792	57165.159421	33.514612
818.582773	57263.887952	33.519629
819.303304	57356.502258	33.524647
820.108416	57452.831287	33.529664
821.073927	57555.781999	33.534682
822.148044	57651.176317	33.539700
822.933594	57756.843627	33.544717
823.987150	57856.204541	33.549735
824.475541	57950.117674	33.554752
825.272730	58045.850529	33.559770
825.970954	58149.588028	33.564788
826.646980	58251.275921	33.569805
827.474075	58344.123560	33.574823
828.504972	58444.736089	33.579840
829.309409	58550.164296	33.584858
830.232769	58655.295253	33.589876
831.262932	58748.566062	33.594893
832.521194	58830.405119	33.599911
833.382897	58904.473944	33.604928
834.015508	58997.894054	33.609946
835.261471	59065.112334	33.614964
836.103125	59144.614009	33.619981
836.828554	59217.771285	33.624999
837.350026	59307.558451	33.630016
837.783769	59390.712126	33.635034
838.659968	59476.150004	33.640052
838.983473	59580.216179	33.645069
839.669999	59676.487062	33.650087
840.475899	59781.870901	33.655104
840.949501	59884.510697	33.660122
841.893967	59999.061910	33.665140
842.292112	60110.885711	33.670157
842.971073	60223.605208	33.675175
843.576017	60342.202683	33.680192
844.772591	60459.400695	33.685210
845.583795	60574.236398	33.690228
846.771696	60704.279889	33.695245
848.125531	60798.195326	33.700263
849.150880	60905.665858	33.705280
850.239004	61011.186199	33.710298
851.189775	61118.834563	33.715316
852.095852	61223.463447	33.720333
852.706738	61333.116037	33.725351
853.216518	61446.786847	33.730368
854.406228	61535.284692	33.735386
855.377955	61641.952662	33.740404
855.962597	61757.616378	33.745421
857.168733	61866.717949	33.750439
857.846902	61987.784185	33.755456
858.688359	62097.225622	33.760474
859.718393	62203.627693	33.765492
860.057926	62311.017187	33.770509
860.961493	62423.212211	33.775527
861.460499	62546.049687	33.780544
862.304137	62660.702102	33.785562
863.362989	62790.868774	33.790580
864.135437	62910.635343	33.795597
864.744233	63024.652429	33.800615
866.035916	63153.910461	33.805632
866.823692	63282.968496	33.810650
867.815080	63401.108678	33.815668
868.434887	63512.711988	33.820685
869.553029	63643.234504	33.825703
870.752351	63762.663359	33.830720
871.515884	63885.591329	33.835738
872.275937	63994.108175	33.840756
873.181081	64116.192248	33.845773
874.563480	64237.135847	33.850791
875.708503	64343.966052	33.855808
876.865488	64442.450605	33.860826
878.187908	64534.738476	33.865844
879.705327	64618.302426	33.870861
881.100026	64703.726626	33.875879
882.015028	64770.291645	33.880896
882.674002	64871.149267	33.885914
883.892676	64934.193904	33.890932
884.897231	65007.578392	33.895949
885.819697	65086.400671	33.900967
886.592847	65160.614303	33.905984
887.056744	65247.453228	33.911002
887.896090	65325.278749	33.916020
888.188045	65408.967096	33.921037
888.886438	65499.769768	33.926055
890.007334	65568.711738	33.931072
890.722601	65670.942023	33.936090
891.723115	65748.432608	33.941108
892.307213	65828.160971	33.946125
893.063984	65912.671885	33.951143
893.546916	65998.878593	33.956160
894.036575	66103.873156	33.961178
894.529270	66195.945758	33.966196
895.012977	66316.848300	33.971213
896.397614	66421.247054	33.976231
897.237072	66522.196489	33.981248
898.302955	66616.944847	33.986266
899.841573	66704.224683	33.991284
900.392698	66820.510156	33.996301
901.463647	66917.060825	34.001319
902.546243	67017.270533	34.006336
903.030032	67116.315665	34.011354
903.978279	67221.884568	34.016372
904.886939	67329.003200	34.021389
905.253693	67436.149094	34.026407
906.161542	67544.508122	34.031424
906.723430	67678.467413	34.036442
907.624430	67792.253429	34.041460
908.293421	67924.540038	34.046477
908.440574	68059.411457	34.051495
909.682824	68197.838584	34.056512
910.700087	68338.365108	34.061530
911.522449	68467.259734	34.066548
912.153971	68616.956652	34.071565
913.247051	68738.865749	34.076583
914.483350	68865.715100	34.081600
915.434409	69007.325579	34.086618
916.735250	69138.888943	34.091636
917.505510	69280.967522	34.096653
918.317740	69405.418248	34.101671
919.711853	69537.088728	34.106688
920.332589	69678.043999	34.111706
921.193348	69807.610605	34.116724
922.133511	69949.463101	34.121741
922.614153	70093.409862	34.126759
923.721306	70222.135057	34.131776
925.130808	70364.513108	34.136794
926.842270	70475.346199	34.141812
927.878446	70601.967192	34.146829
928.949164	70721.899519	34.151847
930.035374	70834.545517	34.156864
931.277923	70951.010739	34.161882
932.652497	71049.850466	34.166900
933.840117	71151.086620	34.171917
934.550243	71261.267919	34.176935
935.309562	71364.498476	34.181952
936.005069	71486.590402	34.186970
936.674610	71600.308672	34.191988
937.206258	71716.535580	34.197005
938.080990	71843.816709	34.202023
938.832746	71974.388310	34.207040
939.333334	72104.218248	34.212058
940.274945	72231.560121	34.217076
941.269705	72357.173867	34.222093
942.365981	72495.539190	34.227111
943.422403	72623.996272	34.232128
944.499189	72753.000911	34.237146
945.381817	72887.281041	34.242164
945.893865	73018.202257	34.247181
946.798786	73148.186354	34.252199
947.688221	73277.301086	34.257216
948.191384	73418.173838	34.262234
949.047380	73561.290911	34.267252
950.041217	73706.169451	34.272269
950.942981	73860.676969	34.277287
952.239559	73977.541607	34.282304
952.937048	74113.251341	34.287322
954.091124	74241.208466	34.292340
954.783341	74378.514439	34.297357
955.418573	74511.675625	34.302375
956.510728	74642.029651	34.307392
957.035029	74789.042388	34.312410
957.971881	74931.294879	34.317428
958.994425	75083.862013	34.322445
960.148564	75222.848501	34.327463
962.608596	75321.565480	34.332480
963.989121	75453.457616	34.337498
965.424444	75571.692823	34.342516
966.476650	75688.044237	34.347533
966.900021	75800.958774	34.352551
967.829312	75921.442891	34.357568
968.788604	76046.135002	34.362586
969.878833	76152.963738	34.367604
970.705081	76292.492071	34.372621
971.613232	76404.038965	34.377639
972.642906	76523.200448	34.382656
973.356267	76657.917567	34.387674
974.198963	76789.053060	34.392692
974.874347	76914.847128	34.397709
975.239355	77057.442237	34.402727
976.456495	77193.103663	34.407744
977.037687	77344.697017	34.412762
978.061196	77489.114790	34.417780
979.112282	77635.331618	34.422797
980.197965	77790.810218	34.427815
981.322480	77935.840325	34.432832
982.113839	78091.648176	34.437850
983.123721	78235.782073	34.442868
984.229241	78385.277670	34.447885
985.433949	78534.599667	34.452903
986.280343	78671.931957	34.457920
987.316647	78839.191548	34.462938
988.578570	78982.921539	34.467956
989.594956	79128.160752	34.472973
991.351458	79242.478213	34.477991
992.630920	79373.138892	34.483008
993.666319	79516.365871	34.488026
994.461822	79651.738947	34.493044
995.557677	79773.873588	34.498061
996.017042	79921.778648	34.503079
996.476291	80058.968562	34.508096
996.944781	80211.314804	34.513114
998.188251	80366.304263	34.518132
999.360874	80526.924083	34.523149
1000.241632	80667.584005	34.528167
1001.183334	80813.637210	34.533184
1002.417501	80989.825063	34.538202
1003.249489	81139.042683	34.543220
1004.437570	81282.388345	34.548237
1005.016455	81443.264998	34.553255
1006.273361	81600.107931	34.558272
1007.206619	81766.065060	34.563290
1007.917369	81916.535209	34.568308
1009.348906	82073.497924	34.573325
1010.498886	82219.614147	34.578343
1011.834153	82366.586278	34.583360
1012.830929	82517.107811	34.588378
1014.158671	82665.418022	34.593396
1015.761103	82787.687234	34.598413
1017.089988	82924.851311	34.603431
1018.524488	83046.371581	34.608448
1019.490998	83182.091557	34.613466
1020.346845	83296.749695	34.618484
1021.654899	83401.444486	34.623501
1022.238878	83517.698917	34.628519
1023.796696	83621.967326	34.633536
1024.650928	83729.813797	34.638554
1025.475307	83840.278768	34.643572
1026.434470	83956.435190	34.648589
1026.777577	84075.073388	34.653607
1028.103155	84193.998390	34.658624
1028.841192	84319.304314	34.663642
1029.735854	84443.971193	34.668660
1030.871271	84572.888619	34.673677
1031.746738	84691.726359	34.678695
1032.870261	84815.933338	34.683712
1034.020915	84953.847693	34.688730
1035.020158	85086.915957	34.693748
1036.000764	85206.567761	34.698765
1036.767636	85340.644116	34.703783
1037.812415	85475.573623	34.708800
1038.586062	85614.781970	34.713818
1039.340922	85775.090150	34.718836
1040.383946	85907.738216	34.723853
1040.349238	86068.786865	34.728871
1041.616450	86223.122119	34.733888
1042.930031	86373.400991	34.738906
1044.005593	86536.590877	34.743924
1046.034134	86679.387625	34.748941
1047.201723	86829.294994	34.753959
1048.285692	86963.929167	34.758976
1049.624163	87109.753835	34.763994
1050.573678	87246.531769	34.769012
1051.889878	87391.355740	34.774029
1052.688315	87531.419282	34.779047
1053.697536	87669.910972	34.784064
1054.386415	87832.553853	34.789082
1055.188973	87984.022552	34.794100
1056.557295	88131.348337	34.799117
1057.365955	88280.001895	34.804135
1058.839133	88435.317314	34.809152
1059.985896	88575.101416	34.814170
1061.152497	88727.311816	34.819188
1062.583704	88858.450238	34.824205
1063.494686	89017.355983	34.829223
1064.366827	89157.068833	34.834240
1065.695910	89312.205051	34.839258
1066.401485	89462.623424	34.844276
1067.420221	89609.117723	34.849293
1067.998025	89774.437631	34.854311
1069.271066	89924.460980	34.859328
1070.270608	90083.238875	34.864346
1070.809686	90253.080839	34.869364
1071.906236	90406.737518	34.874381
1073.065872	90584.067015	34.879399
1074.168732	90746.300324	34.884416
1075.542143	90905.249453	34.889434
1076.770269	91063.318704	34.894452
1078.980772	91183.992797	34.899469
1080.555235	91318.880316	34.904487
1082.150144	91446.695691	34.909504
1084.012778	91572.334434	34.914522
1084.936117	91695.408176	34.919540
1086.089085	91801.165983	34.924557
1086.481118	91938.234157	34.929575
1087.610704	92057.395755	34.934592
1088.383886	92194.984423	34.939610
1088.946846	92327.627636	34.944628
1089.936457	92461.340053	34.949645
1090.609988	92604.947728	34.954663
1091.589833	92742.492544	34.959680
1092.349199	92873.397218	34.964698
1093.304654	93018.099840	34.969716
1094.460566	93140.572662	34.974733
1095.124141	93288.958421	34.979751
1095.946147	93444.325583	34.984768
1096.885133	93594.218232	34.989786
1097.715914	93745.762790	34.994804
1098.593388	93915.295730	34.999821
1099.487369	94084.592903	35.004839
1100.106684	94250.942846	35.009856
1101.112620	94422.072050	35.014874
1102.211637	94598.940812	35.019892
1103.643491	94767.995197	35.024909
1104.667181	94947.929957	35.029927
1105.514141	95133.142888	35.034944
1107.116003	95307.167100	35.039962
1108.271979	95469.220426	35.044980
1110.406045	95646.665574	35.049997
1111.229199	95814.372180	35.055015
1112.082158	95979.732807	35.060032
1113.221075	96169.215887	35.065050
1114.099840	96341.265685	35.070068
1115.233542	96519.034962	35.075085
1116.240805	96701.378012	35.080103
1117.325011	96893.806633	35.085120
1118.956261	97082.892117	35.090138
1119.434646	97268.916421	35.095156
1120.571284	97450.958594	35.100173
1121.751575	97638.939278	35.105191
1122.937214	97817.949956	35.110208
1124.348812	98005.331577	35.115226
1125.419559	98196.759508	35.120244
1127.650174	98350.454920	35.125261
1129.021360	98538.366333	35.130279
1130.219060	98697.185932	35.135296
1131.146749	98864.610709	35.140314
1132.070496	99045.313249	35.145332
1133.511564	99228.577607	35.150349
1134.471005	99392.980719	35.155367
1135.413993	99566.048542	35.160384
1136.623951	99741.409436	35.165402
1137.649667	99911.572560	35.170420
1138.806405	100093.598765	35.175437
1140.067052	100272.291451	35.180455
1140.946555	100454.537167	35.185472
1142.182379	100630.140466	35.190490
1143.247511	100817.929557	35.195508
1144.114957	101003.321547	35.200525
1145.038678	101191.326772	35.205543
1146.253000	101379.677716	35.210560
1147.548668	101561.849589	35.215578
1148.318348	101759.191933	35.220596
1149.376295	101948.155484	35.225613
1150.565757	102142.398244	35.230631
1152.418373	102326.085039	35.235648
1154.820491	102474.204889	35.240666
1156.577423	102636.888207	35.245684
1158.609807	102782.513101	35.250701
1159.758678	102936.136956	35.255719
1160.785784	103080.385310	35.260736
1162.166068	103217.047150	35.265754
1162.611343	103370.891608	35.270772
1164.109090	103521.966230	35.275789
1165.017039	103665.743693	35.280807
1166.059614	103826.140437	35.285824
1167.061816	103975.070982	35.290842
1167.733998	104134.429266	35.295860
1168.671002	104288.425506	35.300877
1169.384547	104438.128445	35.305895
1170.274264	104590.095307	35.310912
1171.676274	104747.056605	35.315930
1172.509892	104915.562089	35.320948
1173.290725	105068.550296	35.325965
1174.330945	105239.341243	35.330983
1174.952897	105417.523064	35.336000
1176.401925	105591.440055	35.341018
1177.515083	105787.033388	35.346036
1178.162211	105971.838661	35.351053
1179.305534	106150.217555	35.356071
1180.540048	106341.602608	35.361088
1182.044844	106521.722528	35.366106
1182.826078	106708.663818	35.371124
1184.095652	106906.557255	35.376141
1185.549517	107100.064545	35.381159
1186.158695	107308.266497	35.386176
1187.147401	107508.972158	35.391194
1188.296374	107710.412700	35.396212
1189.235535	107921.971860	35.401229
1190.666647	108121.240758	35.406247
1191.862796	108352.456777	35.411264
1193.649694	108554.836468	35.416282
1194.819287	108757.674746	35.421300
1197.169438	108946.790680	35.426317
1198.843697	109116.538567	35.431335
1200.735870	109301.008251	35.436352
1201.969326	109474.859568	35.441370
1203.482866	109651.680287	35.446388
1204.956582	109820.047142	35.451405
1206.377089	109975.136005	35.456423
1207.317689	110151.408990	35.461440
1209.381310	110298.197302	35.466458
1210.035585	110464.702638	35.471476
1211.228391	110626.952058	35.476493
1212.266821	110803.669052	35.481511
1213.466615	110950.224137	35.486528
1214.336697	111109.008349	35.491546
1215.832968	111284.588409	35.496564
1216.701732	111437.851592	35.501581
1218.256562	111617.705797	35.506599
1219.405253	111778.955911	35.511616
1220.516410	111964.282545	35.516634
1222.164407	112134.661612	35.521652
1223.365518	112291.611518	35.526669
1224.651857	112454.844327	35.531687
1225.315741	112626.631163	35.536704
1226.353234	112807.567064	35.541722
1227.011248	112983.689700	35.546740
1227.547110	113183.182007	35.551757
1228.916871	113376.013020	35.556775
1229.820918	113571.393037	35.561792
1230.769531	113772.898779	35.566810
1231.731784	113976.367404	35.571828
1232.748677	114191.876753	35.576845
1233.837480	114399.596944	35.581863
1234.888216	114617.599776	35.586880
1236.141068	114834.531881	35.591898
1237.795258	115050.499551	35.596916
1238.782769	115273.129634	35.601933
1240.353111	115490.558910	35.606951
1241.327305	115728.018312	35.611968
1242.587118	115938.660852	35.616986
1244.052646	116160.610463	35.622004
1245.119253	116379.067684	35.627021
1246.965647	116589.731780	35.632039
1247.669713	116816.247365	35.637056
1249.186137	117024.055238	35.642074
1250.568967	117225.551553	35.647092
1251.371644	117438.029514	35.652109
1252.724047	117634.072743	35.657127
1253.501189	117845.303558	35.662144
1254.949654	118061.822337	35.667162
1256.210093	118271.214864	35.672180
1257.396566	118477.161996	35.677197
1258.721575	118683.505761	35.682215
1259.846130	118912.857108	35.687232
1261.158539	119131.345156	35.692250
1262.136605	119342.300146	35.697268
1263.270196	119583.997217	35.702285
1265.213421	119797.684515	35.707303
1266.369104	120024.479799	35.712320
1267.800469	120230.753537	35.717338
1269.233116	120455.085913	35.722356
1270.113344	120685.505468	35.727373
1271.519994	120904.890856	35.732391
1272.954463	121115.846288	35.737408
1274.887901	121327.620196	35.742426
1276.552212	121549.692180	35.747444
1277.769363	121759.560421	35.752461
1279.405774	121963.049699	35.757479
1280.428169	122182.457621	35.762496
1281.574296	122387.488479	35.767514
1282.720705	122601.252247	35.772532
1283.987943	122821.409980	35.777549
1285.200797	123025.686461	35.782567
1286.263915	123259.289271	35.787584
1287.488434	123476.011836	35.792602
1289.385788	123705.829892	35.797620
1290.454742	123926.383485	35.802637
1292.043380	124149.906797	35.807655
1293.134349	124368.191429	35.812672
1294.472141	124583.585137	35.817690
1295.420064	124811.110412	35.822708
1296.657582	125044.127816	35.827725
1298.096533	125262.145721	35.832743
1299.297523	125484.336379	35.837760
1301.109476	125707.187769	35.842778
1302.580066	125931.985859	35.847796
1304.340316	126147.764179	35.852813
1305.532739	126363.029831	35.857831
1306.935910	126580.416695	35.862848
1307.886646	126806.055214	35.867866
1309.357132	127022.927062	35.872884
1310.442515	127243.616025	35.877901
1311.977206	127459.795862	35.882919
1313.722376	127669.376708	35.887936
1314.939080	127883.204016	35.892954
1316.522412	128087.795244	35.897972
1317.335616	128308.422861	35.902989
1318.970234	128523.554180	35.908007
1320.179060	128734.777551	35.913024
1321.449573	128946.777995	35.918042
1322.893338	129161.159487	35.923060
1323.972734	129387.543281	35.928077
1325.524155	129605.636581	35.933095
1326.877855	129834.779430	35.938112
1327.627446	130052.755298	35.943130
1328.639264	130264.237125	35.948148
1329.588435	130511.172949	35.953165
1330.886981	130726.337067	35.958183
1332.129866	130973.278481	35.963200
1333.162448	131219.090471	35.968218
1334.445554	131459.703505	35.973236
1336.141787	131695.027114	35.978253
1337.678574	131918.551630	35.983271
1339.184981	132132.904825	35.988288
1340.275782	132363.148993	35.993306
1342.342139	132557.864578	35.998324
1343.710764	132771.294121	36.003341
1345.056519	132985.920510	36.008359
1345.978875	133209.517875	36.013376
1347.337562	133419.353052	36.018394
1348.729750	133628.461427	36.023412
1349.981013	133851.463550	36.028429
1351.215645	134068.612981	36.033447
1352.326219	134299.222616	36.038464
1353.438761	134532.483177	36.043482
1354.698885	134767.330996	36.048500
1355.649561	135005.756248	36.053517
1357.069808	135251.065524	36.058535
1358.506614	135495.068049	36.063552
1359.517107	135739.320574	36.068570
1361.169197	135980.387704	36.073588
1362.379823	136235.260377	36.078605
1364.454447	136472.660387	36.083623
1366.307148	136697.674012	36.088640
1367.849245	136944.459017	36.093658
1369.270512	137175.797948	36.098676
1370.878442	137402.847473	36.103693
1372.815964	137617.405971	36.108711
1374.490032	137830.614858	36.113728
1376.167434	138069.791075	36.118746
1377.852404	138275.609137	36.123764
1378.897650	138498.245641	36.128781
1380.211911	138713.307545	36.133799
1381.474109	138936.773145	36.138816
1382.541113	139174.017041	36.143834
1383.469734	139392.190256	36.148852
1384.679926	139621.831207	36.153869
1386.121541	139860.805581	36.158887
1387.204407	140103.860595	36.163904
1388.252433	140344.551984	36.168922
1390.071283	140578.904076	36.173940
1391.179381	140834.842870	36.178957
1392.652206	141087.654497	36.183975
1393.949311	141332.432517	36.188992
1395.062742	141586.600771	36.194010
1396.378260	141853.620632	36.199028
1397.267571	142103.391702	36.204045
1398.803884	142368.109092	36.209063
1400.288983	142641.548595	36.214080
1401.099479	142909.192870	36.219098
1402.620921	143174.020267	36.224116
1403.514940	143454.944384	36.229133
1404.779115	143739.651714	36.234151
1406.275156	144025.679771	36.239168
1407.402462	144315.994144	36.244186
1409.396176	144604.417186	36.249204
1410.296939	144897.677905	36.254221
1411.517464	145190.634375	36.259239
1414.165686	145453.973057	36.264256
1415.744190	145723.223219	36.269274
1417.954773	145987.602206	36.274292
1420.022003	146238.335769	36.279309
1421.602331	146503.951746	36.284327
1423.315374	146755.559281	36.289344
1424.770539	147010.166278	36.294362
1426.290637	147251.866392	36.299380
1427.518558	147498.245628	36.304397
1429.054035	147735.964130	36.309415
1430.615601	147973.933502	36.314432
1431.990368	148224.288275	36.319450
1433.341835	148463.944402	36.324468
1434.854112	148687.912171	36.329485
1435.581586	148925.125523	36.334503
1437.268859	149154.901225	36.339520
1438.403857	149396.273439	36.344538
1439.918711	149616.657097	36.349556
1441.246489	149843.642970	36.354573
1442.935362	150075.910001	36.359591
1444.340074	150305.409892	36.364608
1445.447011	150550.104571	36.369626
1447.198042	150777.025919	36.374644
1448.357903	151021.892461	36.379661
1450.008956	151261.783247	36.384679
1451.348787	151507.193856	36.389696
1452.276192	151766.702757	36.394714
1453.878143	152014.546529	36.399732
1455.281137	152262.310749	36.404749
1456.658713	152516.879458	36.409767
1458.451239	152781.059076	36.414784
1459.396352	153038.874003	36.419802
1460.798230	153290.019063	36.424820
1461.945932	153557.735707	36.429837
1463.220811	153834.248853	36.434855
1465.127839	154094.245277	36.439872
1466.079038	154371.830691	36.444890
1467.675913	154652.659802	36.449908
1469.461584	154937.150926	36.454925
1470.830437	155203.535678	36.459943
1472.382535	155486.090659	36.464960
1473.649420	155774.136884	36.469978
1475.141109	156046.075744	36.474996
1476.892254	156338.028943	36.480013
1477.959762	156622.207314	36.485031
1479.535046	156893.288191	36.490048
1481.301310	157181.858042	36.495066
1482.957161	157456.899973	36.500084
1484.231001	157754.638540	36.505101
1485.954327	158034.595314	36.510119
1487.953445	158313.024046	36.515136
1488.986431	158600.748830	36.520154
1490.676982	158887.262929	36.525172
1492.403629	159165.679254	36.530189
1493.727170	159458.347599	36.535207
1495.623311	159721.858576	36.540224
1496.912434	160013.407499	36.545242
1498.933377	160279.121487	36.550260
1500.467354	160557.249341	36.555277
1501.960959	160842.655251	36.560295
1503.749438	161097.895739	36.565312
1504.919779	161389.499413	36.570330
1506.222315	161662.382592	36.575348
1507.797018	161941.439082	36.580365
1508.899053	162227.947027	36.585383
1510.364832	162506.149907	36.590400
1511.645129	162802.921542	36.595418
1513.056395	163093.126836	36.600436
1514.765234	163384.502772	36.605453
1515.742389	163687.496960	36.610471
1517.276346	163975.734026	36.615488
1519.003603	164277.732569	36.620506
1520.407213	164566.832600	36.625524
1522.259628	164869.271296	36.630541
1523.970342	165166.609638	36.635559
1525.777815	165450.256195	36.640576
1527.009864	165750.951417	36.645594
1528.980330	166038.114773	36.650612
1530.586890	166317.943033	36.655629
1531.699856	166609.705905	36.660647
1533.366110	166892.040221	36.665664
1534.531917	167174.941475	36.670682
1535.747350	167451.060547	36.675700
1537.439470	167728.472683	36.680717
1539.026970	167994.928047	36.685735
1540.514902	168268.443845	36.690752
1541.873652	168554.988935	36.695770
1543.235784	168833.896464	36.700788
1544.605034	169119.682048	36.705805
1545.820630	169422.371578	36.710823
1547.802968	169708.769817	36.715840
1549.553539	169994.484980	36.720858
1551.152851	170270.570316	36.725876
1552.789292	170573.337268	36.730893
1554.205296	170871.092278	36.735911
1555.729955	171161.420397	36.740928
1557.303393	171464.876176	36.745946
1559.227163	171762.920723	36.750964
1560.220602	172055.842384	36.755981
1561.078172	172378.280038	36.760999
1562.593190	172677.743299	36.766016
1564.282064	172998.448412	36.771034
1566.227211	173300.458483	36.776052
1567.948451	173610.692876	36.781069
1569.868395	173931.188296	36.786087
1571.610686	174230.572878	36.791104
1573.473555	174537.655224	36.796122
1575.483232	174837.456108	36.801140
1577.697219	175134.826419	36.806157
1578.665954	175432.544586	36.811175
1580.413206	175725.858662	36.816192
1581.960043	176025.895874	36.821210
1583.573179	176329.210913	36.826228
1585.201147	176642.399075	36.831245
1586.228915	176956.513646	36.836263
1587.778534	177251.988983	36.841280
1589.407139	177574.054128	36.846298
1591.228183	177866.505619	36.851316
1593.144329	178168.537850	36.856333
1594.656076	178481.388731	36.861351
1596.294255	178786.694403	36.866368
1597.880949	179099.282828	36.871386
1598.987201	179405.061134	36.876404
1600.479851	179723.304138	36.881421
1601.026053	180063.485495	36.886439
1602.945487	180383.286393	36.891456
1604.598521	180724.202428	36.896474
1605.613583	181061.494925	36.901492
1606.842863	181404.046783	36.906509
1608.197742	181759.780167	36.911527
1609.873258	182122.329438	36.916544
1611.337689	182489.599742	36.921562
1612.777488	182861.509484	36.926580
1614.584391	183220.706253	36.931597
1616.185664	183580.193358	36.936615
1618.079503	183944.191115	36.941632
1619.453466	184316.451794	36.946650
1621.199505	184671.784180	36.951668
1623.414148	185023.207840	36.956685
1625.470505	185379.216859	36.961703
1627.505574	185709.908459	36.966720
1629.754610	186048.487247	36.971738
1631.449029	186387.045779	36.976756
1633.326262	186716.677847	36.981773
1634.906882	187044.812379	36.986791
1636.954816	187373.175992	36.991808
1638.285488	187705.240042	36.996826
1639.872354	188021.180419	37.001844
1641.310068	188355.566153	37.006861
1642.679695	188671.457240	37.011879
1644.310685	188981.416668	37.016896
1645.380079	189297.132421	37.021914
1647.121801	189611.392840	37.026932
1648.714292	189926.720602	37.031949
1649.952388	190263.828818	37.036967
1651.489495	190589.007401	37.041984
1653.410280	190909.389111	37.047002
1655.096881	191237.301138	37.052020
1657.395335	191550.628961	37.057037
1659.157798	191879.649022	37.062055
1661.666667	192191.523470	37.067072
1663.467077	192500.889114	37.072090
1665.162847	192801.450717	37.077108
1667.024428	193111.139352	37.082125
1668.617390	193416.113432	37.087143
1670.641294	193728.634613	37.092160
1672.134806	194019.574681	37.097178
1673.714194	194343.953686	37.102196
1674.951127	194656.495662	37.107213
1676.526184	194978.758524	37.112231
1678.152685	195306.054552	37.117248
1679.525890	195622.196848	37.122266
1680.265338	195972.253888	37.127284
1681.788441	196303.139547	37.132301
1683.063516	196664.550245	37.137319
1684.078997	197032.049123	37.142336
1685.827420	197396.597397	37.147354
1687.520607	197767.479366	37.152372
1689.345669	198145.451257	37.157389
1690.856390	198519.744749	37.162407
1692.961948	198889.586965	37.167424
1694.678715	199260.232009	37.172442
1696.213239	199632.318544	37.177460
1697.927731	200007.576720	37.182477
1699.662379	200393.498517	37.187495
1701.127456	200772.560275	37.192512
1703.061025	201158.161295	37.197530
1705.103302	201531.875120	37.202548
1707.194424	201906.992136	37.207565
1708.776699	202293.470112	37.212583
1710.616964	202669.661115	37.217600
1712.978278	203033.401004	37.222618
1714.344049	203420.809637	37.227636
1716.182676	203786.557121	37.232653
1717.957311	204174.752634	37.237671
1719.400661	204545.914807	37.242688
1721.397766	204925.100503	37.247706
1722.530340	205313.421007	37.252724
1724.397290	205684.937560	37.257741
1726.173486	206072.215640	37.262759
1727.718074	206458.632531	37.267776
1729.423468	206850.192549	37.272794
1731.028126	207242.634646	37.277812
1733.761500	207605.103096	37.282829
1735.688374	207989.089684	37.287847
1737.354670	208368.880265	37.292864
1738.914901	208735.548030	37.297882
1740.692075	209111.019166	37.302900
1743.086193	209473.717296	37.307917
1745.126612	209835.358220	37.312935
1747.241900	210204.416625	37.317952
1749.485185	210548.948234	37.322970
1751.410936	210897.876618	37.327988
1752.938172	211242.301150	37.333005
1754.461648	211595.768797	37.338023
1755.952782	211947.541686	37.343040
1757.765760	212297.637274	37.348058
1758.884360	212656.915955	37.353076
1760.491040	212986.527953	37.358093
1762.118559	213322.740905	37.363111
1763.713421	213665.766917	37.368128
1765.592898	213996.404088	37.373146
1767.250179	214342.723932	37.378164
1769.336462	214683.158015	37.383181
1771.390472	215020.500225	37.388199
1772.762437	215369.233151	37.393216
1774.592776	215709.764197	37.398234
1776.201455	216064.987632	37.403252
1778.288988	216407.967522	37.408269
1779.883011	216763.907111	37.413287
1781.265348	217118.181428	37.418304
1782.729386	217488.723600	37.423322
1784.303072	217858.995010	37.428340
1785.865208	218233.511206	37.433357
1787.525538	218614.006517	37.438375
1789.316197	218997.097688	37.443392
1791.216124	219398.662272	37.448410
1792.798353	219844.017415	37.453428
1794.381754	220226.106134	37.458445
1795.789900	220635.122574	37.463463
1797.427428	221037.448060	37.468480
1799.164847	221444.787485	37.473498
1800.971327	221867.127827	37.478516
1802.688427	222273.483127	37.483533
1804.624100	222691.665132	37.488551
1806.559169	223094.329787	37.493568
1809.134624	223485.586993	37.498586
1810.853258	223904.622185	37.503604
1813.014156	224309.844402	37.508621
1815.525679	224719.048453	37.513639
1817.136183	225114.738137	37.518656
1819.532822	225505.904665	37.523674
1821.552931	225903.078422	37.528692
1823.624234	226290.846962	37.533709
1825.342227	226688.327284	37.538727
1827.691991	227067.441433	37.543744
1829.824248	227449.945576	37.548762
1831.573958	227840.667738	37.553780
1833.258396	228220.428904	37.558797
1835.091131	228604.357653	37.563815
1836.505246	228989.220480	37.568832
1838.254551	229368.440710	37.573850
1840.401761	229765.173311	37.578868
1841.932311	230156.751262	37.583885
1843.751593	230544.370717	37.588903
1845.704857	230940.910123	37.593920
1847.604814	231318.865937	37.598938
1849.518919	231725.244109	37.603956
1851.358653	232113.397719	37.608973
1853.255981	232496.462541	37.613991
1855.013443	232906.019550	37.619008
1857.692518	233279.710710	37.624026
1858.923320	233651.712227	37.629044
1861.021276	234051.690250	37.634061
1863.284391	234413.615898	37.639079
1865.239679	234813.035161	37.644096
1867.174545	235184.161398	37.649114
1868.703740	235567.192809	37.654132
1870.686703	235945.298144	37.659149
1872.670465	236320.000316	37.664167
1874.293050	236713.687436	37.669184
1876.471790	237082.592656	37.674202
1878.204547	237462.317496	37.679220
1879.748620	237849.466318	37.684237
1881.363547	238224.004783	37.689255
1882.808983	238593.593242	37.694272
1884.839011	238971.874630	37.699290
1886.398470	239345.027250	37.704308
1888.089020	239725.830267	37.709325
1889.713839	240101.183377	37.714343
1891.050155	240485.856759	37.719360
1893.423213	240871.044885	37.724378
1895.494550	241261.745161	37.729396
1897.094834	241657.426803	37.734413
1899.267543	242037.518775	37.739431
1901.019652	242432.287449	37.744448
1902.746279	242827.797643	37.749466
1903.995319	243240.686714	37.754484
1905.428870	243658.829600	37.759501
1907.183991	244084.235810	37.764519
1909.074772	244512.668514	37.769536
1910.708752	244950.086160	37.774554
1912.479795	245400.691171	37.779572
1913.801955	245845.299958	37.784589
1915.788034	246296.683530	37.789607
1917.036345	246774.227885	37.794624
1918.768147	247232.615237	37.799642
1920.499624	247723.493567	37.804660
1922.130098	248207.784518	37.809677
1924.215777	248692.813552	37.814695
1926.074600	249187.025838	37.819712
1928.157678	249672.742332	37.824730
1930.268690	250178.904193	37.829748
1932.598667	250673.725940	37.834765
1934.994576	251164.447350	37.839783
1936.925699	251657.380080	37.844800
1939.226987	252133.536626	37.849818
1941.236325	252628.972120	37.854836
1943.156734	253117.081194	37.859853
1945.490080	253610.507667	37.864871
1947.155945	254114.841408	37.869888
1948.828501	254605.786824	37.874906
1950.783939	255113.807413	37.879924
1953.135289	255612.541256	37.884941
1955.458854	256097.511322	37.889959
1957.255326	256590.951954	37.894976
1959.461111	257089.608788	37.899994
1961.684017	257589.736281	37.905012
1963.644525	258079.796809	37.910029
1965.354830	258571.880289	37.915047
1967.665816	259070.011863	37.920064
1969.745134	259556.369270	37.925082
1971.642865	260052.511581	37.930100
1974.095289	260534.869548	37.935117
1976.212184	261024.497536	37.940135
1978.113972	261513.983208	37.945152
1980.029757	262007.124471	37.950170
1982.419048	262475.850780	37.955188
1984.511860	262965.329653	37.960205
1986.725827	263439.368449	37.965223
1988.556408	263925.257597	37.970240
1990.766242	264385.223162	37.975258
1992.838185	264860.732627	37.980276
1995.033230	265334.824188	37.985293
1997.347745	265795.965398	37.990311
1999.212517	266258.755744	37.995328
2001.760094	266709.899574	38.000346
2004.375512	267160.828548	38.005364
2006.069525	267619.835501	38.010381
2008.922789	268056.066663	38.015399
2011.324256	268481.194917	38.020416
2013.341918	268902.931520	38.025434
2014.900812	269330.281526	38.030452
2016.530367	269748.982361	38.035469
2018.397739	270158.041036	38.040487
2019.658081	270581.730244	38.045504
2020.929486	271016.568944	38.050522
2023.113648	271443.965271	38.055540
2024.654425	271884.829467	38.060557
2026.688626	272326.500398	38.065575
2028.058548	272790.939922	38.070592
2029.904696	273236.705079	38.075610
2031.391234	273704.324542	38.080628
2032.869507	274185.661959	38.085645
2035.245419	274658.670195	38.090663
2036.728488	275148.768910	38.095680
2038.984109	275636.401666	38.100698
2041.712667	276100.711935	38.105716
2043.850695	276592.324991	38.110733
2045.814974	277070.782005	38.115751
2049.055450	277546.562578	38.120768
2051.473597	278010.767942	38.125786
2053.634785	278482.025834	38.130804
2055.310906	278972.211315	38.135821
2057.763010	279439.633913	38.140839
2059.566912	279920.854409	38.145856
2061.195948	280412.263412	38.150874
2063.054106	280890.652875	38.155892
2064.755043	281402.038562	38.160909
2066.356967	281902.973729	38.165927
2068.263800	282411.299627	38.170944
2070.206727	282935.493981	38.175962
2072.043855	283440.653181	38.180980
2074.262013	283969.294757	38.185997
2076.471079	284483.863828	38.191015
2078.682334	285002.749068	38.196032
2080.792997	285533.943363	38.201050
2083.159723	286050.106815	38.206068
2085.062755	286593.016236	38.211085
2087.472863	287117.754289	38.216103
2089.087655	287663.603152	38.221120
2091.186268	288195.958249	38.226138
2093.461191	288726.199260	38.231156
2095.484684	289269.484867	38.236173
2097.953132	289792.196523	38.241191
2100.361686	290331.400759	38.246208
2102.638496	290865.823953	38.251226
2104.707624	291387.071307	38.256244
2106.759558	291925.464264	38.261261
2109.016897	292458.817092	38.266279
2111.384933	292990.295065	38.271296
2113.300590	293529.236869	38.276314
2115.555064	294059.509677	38.281332
2117.413116	294601.732594	38.286349
2119.307033	295129.825044	38.291367
2121.405498	295676.092265	38.296384
2123.658439	296207.599820	38.301402
2126.082432	296755.382495	38.306420
2128.065211	297290.104337	38.311437
2130.742256	297824.048131	38.316455
2133.088880	298358.678888	38.321472
2134.782901	298893.110183	38.326490
2137.151105	299434.233720	38.331508
2139.120167	299980.220676	38.336525
2141.496691	300490.173733	38.341543
2143.967657	301019.004422	38.346560
2145.915575	301558.331868	38.351578
2147.904842	302083.579223	38.356596
2149.798158	302626.135122	38.361613
2152.183875	303161.037951	38.366631
2154.550822	303677.807300	38.371648
2156.472369	304176.641086	38.376666
2158.896426	304681.458703	38.381684
2160.480864	305186.768065	38.386701
2163.068181	305680.124473	38.391719
2165.439615	306169.958356	38.396736
2167.433910	306674.378523	38.401754
2169.428520	307174.452936	38.406772
2170.956608	307700.657803	38.411789
2173.182358	308214.020564	38.416807
2175.393702	308723.243047	38.421824
2177.273037	309257.506399	38.426842
2179.522898	309766.766759	38.431860
2181.270943	310305.895382	38.436877
2183.486337	310845.730179	38.441895
2185.747134	311394.898988	38.446912
2187.029426	311935.845774	38.451930
2189.391514	312482.577592	38.456948
2191.831086	313032.492309	38.461965
2193.944663	313601.324707	38.466983
2196.072271	314160.043718	38.472000
2198.109550	314731.800356	38.477018
2200.746026	315301.777319	38.482036
2202.901657	315877.999954	38.487053
2205.199865	316434.844896	38.492071
2207.984211	317002.193734	38.497088
2209.865219	317575.731005	38.502106
2212.136962	318138.305516	38.507124
2214.192357	318728.741028	38.512141
2216.126395	319307.536633	38.517159
2218.477676	319887.451583	38.522176
2220.523461	320475.969014	38.527194
2223.139520	321053.950971	38.532212
2225.375122	321650.551666	38.537229
2227.387973	322242.714989	38.542247
2229.842569	322828.223556	38.547264
2231.462648	323427.321802	38.552282
2233.804117	324025.812491	38.557300
2236.894898	324622.040623	38.562317
2240.343332	325189.945187	38.567335
2242.989771	325764.832434	38.572352
2244.604001	326346.156294	38.577370
2247.227112	326928.500769	38.582388
2249.748690	327510.323233	38.587405
2252.050308	328071.814948	38.592423
2254.481125	328643.308224	38.597440
2256.511555	329221.843874	38.602458
2258.604815	329800.896481	38.607476
2260.467749	330373.913813	38.612493
2262.495346	330951.873989	38.617511
2265.666090	331518.951100	38.622528
2268.271200	332072.889724	38.627546
2271.196327	332630.247771	38.632564
2273.757294	333185.578834	38.637581
2276.020304	333754.814270	38.642599
2278.308048	334301.649591	38.647616
2280.431225	334863.407799	38.652634
2282.830159	335415.239680	38.657652
2284.816026	335966.169616	38.662669
2286.613260	336534.310353	38.667687
2288.776939	337091.342121	38.672704
2290.697052	337651.352801	38.677722
2292.719108	338228.779122	38.682740
2294.841458	338808.847597	38.687757
2296.894959	339382.575096	38.692775
2299.995578	339945.766519	38.697792
2302.786506	340509.104436	38.702810
2305.044557	341068.082333	38.707828
2307.416606	341631.730710	38.712845
2309.561113	342157.896196	38.717863
2311.693382	342693.043065	38.722880
2314.375991	343228.879731	38.727898
2316.314971	343765.696525	38.732916
2318.534862	344301.496339	38.737933
2320.397115	344843.364471	38.742951
2322.431847	345388.522624	38.747968
2324.079069	345962.214616	38.752986
2326.571362	346520.075208	38.758004
2328.213484	347085.582067	38.763021
2330.210486	347665.793664	38.768039
2332.675398	348244.550014	38.773056
2334.515360	348852.638032	38.778074
2336.787903	349439.633494	38.783092
2339.265950	350043.412485	38.788109
2341.239870	350651.657011	38.793127
2343.969660	351263.219281	38.798144
2346.050414	351877.874932	38.803162
2348.203746	352509.511846	38.808180
2350.672108	353124.238019	38.813197
2352.964319	353762.456713	38.818215
2355.886500	354382.317082	38.823232
2358.435779	355008.421553	38.828250
2361.310392	355631.697123	38.833268
2363.800626	356246.755254	38.838285
2366.336943	356874.458020	38.843303
2368.556060	357491.572532	38.848320
2370.997608	358127.112251	38.853338
2373.357465	358746.645780	38.858356
2376.072921	359364.791681	38.863373
2378.527445	360002.684954	38.868391
2381.193276	360616.024711	38.873408
2383.501371	361250.015255	38.878426
2385.732452	361876.169034	38.883444
2388.126743	362516.467606	38.888461
2390.664796	363151.505837	38.893479
2392.946477	363776.555419	38.898496
2395.057052	364412.455648	38.903514
2397.407019	365062.790981	38.908532
2399.710689	365709.723665	38.913549
2401.817756	366366.292115	38.918567
2404.847649	367011.382782	38.923584
2407.134141	367666.351530	38.928602
2409.633126	368310.772114	38.933620
2412.224820	368960.087092	38.938637
2414.001071	369620.483375	38.943655
2416.365441	370268.646132	38.948672
2418.467395	370937.563358	38.953690
2420.695640	371608.730084	38.958708
2423.424076	372284.975617	38.963725
2425.800375	372959.034773	38.968743
2428.324069	373620.198114	38.973760
2430.830254	374300.525533	38.978778
2433.541716	374966.020197	38.983796
2435.923546	375653.950382	38.988813
2438.033354	376334.633602	38.993831
2440.409926	377009.477242	38.998848
2442.515964	377692.670291	39.003866
2445.254331	378376.023971	39.008884
2448.237289	379048.951895	39.013901
2450.448462	379731.782297	39.018919
2453.027848	380410.531439	39.023936
2455.651768	381097.779303	39.028954
2458.156219	381782.142133	39.033972
2460.555808	382454.413490	39.038989
2462.672749	383139.192647	39.044007
2465.052935	383815.927178	39.049024
2467.339970	384507.596628	39.054042
2469.504433	385164.030099	39.059060
2472.891608	385818.168828	39.064077
2475.155381	386471.313928	39.069095
2477.596813	387107.886690	39.074112
2479.825304	387769.579932	39.079130
2482.406313	388418.576137	39.084148
2485.195049	389073.862145	39.089165
2487.048389	389729.821575	39.094183
2489.934311	390388.131167	39.099200
2492.525065	391055.550475	39.104218
2495.132511	391712.306240	39.109236
2497.655525	392376.108550	39.114253
2500.065299	393044.350883	39.119271
2502.617864	393717.041184	39.124288
2504.619378	394378.173828	39.129306
2506.937038	395067.474452	39.134324
2509.614071	395734.269411	39.139341
2511.904681	396433.554099	39.144359
2514.394930	397125.718281	39.149376
2516.741034	397821.666137	39.154394
2518.997755	398535.934853	39.159412
2521.547057	399235.616691	39.164429
2523.804232	399959.834967	39.169447
2526.496464	400669.518850	39.174464
2529.076611	401393.115352	39.179482
2531.793629	402110.285300	39.184500
2534.863208	402816.179032	39.189517
2537.773177	403541.363782	39.194535
2540.815010	404238.864832	39.199552
2543.828106	404954.367668	39.204570
2547.408172	405630.360520	39.209588
2551.427605	406286.831747	39.214605
2554.841837	406944.704893	39.219623
2557.680408	407585.455489	39.224640
2560.218909	408232.042131	39.229658
2562.799831	408885.522312	39.234676
2565.130123	409512.530333	39.239693
2567.799893	410162.646314	39.244711
2570.075692	410813.217036	39.249728
2572.445028	411458.259658	39.254746
2574.325979	412114.766004	39.259764
2576.148775	412787.273912	39.264781
2578.245723	413469.850807	39.269799
2580.543871	414148.552094	39.274816
2582.873041	414847.289966	39.279834
2584.776988	415548.384172	39.284852
2587.060094	416265.580002	39.289869
2589.206208	416976.345896	39.294887
2591.564055	417707.266127	39.299904
2594.243001	418431.148207	39.304922
2596.629154	419169.796219	39.309940
2599.219414	419915.909645	39.314957
2601.017654	420671.551699	39.319975
2603.428410	421433.627711	39.324992
2605.960979	422182.240596	39.330010
2608.336525	422956.378808	39.335028
2611.129216	423726.879121	39.340045
2614.358017	424491.257476	39.345063
2617.436517	425247.535380	39.350080
2620.331556	426002.250549	39.355098
2623.111061	426762.834512	39.360116
2626.103150	427533.485158	39.365133
2628.291143	428290.675951	39.370151
2630.424984	429065.722695	39.375168
2633.073111	429827.749891	39.380186
2635.229979	430614.638981	39.385204
2637.710511	431392.994552	39.390221
2639.910547	432176.584516	39.395239
2641.950796	432939.978223	39.400256
2644.930416	433698.433523	39.405274
2647.492711	434469.232313	39.410292
2650.152221	435224.400560	39.415309
2653.400609	435978.282456	39.420327
2656.062716	436733.248683	39.425344
2659.257715	437490.530837	39.430362
2661.238631	438255.579467	39.435380
2664.050719	439016.466883	39.440397
2666.823265	439786.038682	39.445415
2669.053068	440556.837627	39.450432
2671.987289	441338.827483	39.455450
2674.496415	442122.327414	39.460468
2677.378951	442899.109756	39.465485
2680.078567	443681.814353	39.470503
2682.936432	444469.928671	39.475520
2685.992449	445252.872114	39.480538
2688.466892	446047.063489	39.485556
2691.278997	446838.235795	39.490573
2693.624350	447631.783110	39.495591
2696.528723	448428.546961	39.500608
2699.507250	449224.762963	39.505626
2701.924857	450037.125919	39.510644
2704.849404	450831.115604	39.515661
2707.757765	451642.273433	39.520679
2710.717006	452442.821741	39.525696
2713.455079	453246.309048	39.530714
2716.213065	454061.645684	39.535732
2719.298628	454855.506202	39.540749
2721.840806	455666.213612	39.545767
2724.622809	456481.855046	39.550784
2727.285271	457298.798291	39.555802
2729.538142	458119.922341	39.560820
2732.383283	458945.566353	39.565837
2735.389506	459758.814577	39.570855
2737.768796	460583.912396	39.575872
2740.788625	461415.593442	39.580890
2743.042376	462252.421376	39.585908
2745.853054	463095.895081	39.590925
2748.315036	463942.726390	39.595943
2750.587379	464809.567231	39.600960
2753.345201	465668.910613	39.605978
2755.695308	466549.256625	39.610996
2758.061548	467415.915600	39.616013
2760.954708	468295.738701	39.621031
2763.529194	469178.252451	39.626048
2766.611047	470060.995342	39.631066
2769.146474	470954.751928	39.636084
2772.666036	471828.245867	39.641101
2775.782113	472711.769434	39.646119
2778.219787	473602.284897	39.651136
2781.958033	474474.761188	39.656154
2784.438196	475357.608719	39.661172
2787.516604	476230.415135	39.666189
2790.781040	477097.997735	39.671207
2793.780262	477958.967040	39.676224
2797.567885	478810.876795	39.681242
2800.263443	479669.795882	39.686260
2803.149489	480522.886037	39.691277
2805.814891	481359.459976	39.696295
2808.418855	482224.232167	39.701312
2811.430697	483062.942170	39.706330
2813.955201	483921.738274	39.711348
2816.896775	484778.960002	39.716365
2819.165216	485645.288736	39.721383
2821.747597	486499.255895	39.726400
2824.569832	487359.805553	39.731418
2827.036392	488231.275253	39.736436
2829.551251	489064.635112	39.741453
2832.020341	489904.221480	39.746471
2834.526025	490740.934949	39.751488
2836.912018	491588.276671	39.756506
2839.223449	492449.971930	39.761524
2841.683279	493329.312096	39.766541
2843.800280	494206.191323	39.771559
2846.717809	495102.470807	39.776576
2850.316330	495981.687897	39.781594
2853.154127	496868.199954	39.786612
2856.110211	497760.498101	39.791629
2858.826923	498660.002478	39.796647
2861.083853	499574.567113	39.801664
2864.404855	500468.678447	39.806682
2867.406682	501382.970129	39.811700
2870.726227	502288.433296	39.816717
2873.538164	503209.111217	39.821735
2876.269392	504138.223258	39.826752
2879.511733	505046.068768	39.831770
2881.906850	505983.603337	39.836788
2884.917282	506907.821863	39.841805
2888.205255	507842.479286	39.846823
2890.991117	508777.619305	39.851840
2894.045146	509703.686934	39.856858
2896.718395	510654.666628	39.861876
2899.835377	511602.592534	39.866893
2902.713085	512548.737244	39.871911
2905.348111	513511.699477	39.876928
2907.731899	514470.058154	39.881946
2910.429515	515442.265793	39.886964
2913.221212	516417.924804	39.891981
2916.865845	517394.137390	39.896999
2919.803236	518373.478983	39.902016
2922.996277	519342.690091	39.907034
2926.287627	520313.687883	39.912052
2929.010281	521287.942257	39.917069
2932.939832	522250.449827	39.922087
2936.258416	523213.299720	39.927104
2939.715000	524172.136993	39.932122
2942.716333	525130.434633	39.937140
2945.182080	526092.637485	39.942157
2948.516439	527056.850547	39.947175
2951.250397	528022.460141	39.952192
2954.375475	528973.340769	39.957210
2957.354028	529930.981413	39.962228
2960.286473	530885.446222	39.967245
2963.390583	531847.170367	39.972263
2966.053304	532818.367732	39.977280
2969.440577	533767.737131	39.982298
2972.817088	534728.672647	39.987316
2975.480759	535684.126339	39.992333
2978.771154	536645.854579	39.997351
2981.408126	537604.154473	40.002368
2984.232263	538566.686602	40.007386
2987.220066	539548.145313	40.012404
2989.755918	540515.725490	40.017421
2992.574368	541497.530290	40.022439
2995.487713	542472.711750	40.027456
2998.323500	543451.309146	40.032474
3001.078432	544446.097270	40.037492
3003.743860	545438.867972	40.042509
3007.084124	546425.371318	40.047527
3009.945905	547417.364739	40.052544
3013.582751	548403.929484	40.057562
3016.551528	549393.651277	40.062580
3019.647590	550392.430594	40.067597
3022.906065	551378.693212	40.072615
3025.847696	552353.727254	40.077632
3028.799670	553303.457223	40.082650
3031.870880	554245.411010	40.087668
3034.861807	555193.594363	40.092685
3038.340956	556121.880604	40.097703
3040.764485	557059.171280	40.102720
3044.214314	557980.348663	40.107738
3047.134594	558929.384278	40.112756
3050.231157	559871.038188	40.117773
3053.910354	560809.162900	40.122791
3056.396833	561746.765045	40.127808
3060.094712	562680.684415	40.132826
3063.898707	563620.295441	40.137844
3066.965827	564546.601846	40.142861
3069.911680	565466.233625	40.147879
3072.886223	566419.740057	40.152896
3075.890169	567376.183895	40.157914
3078.369120	568318.033467	40.162932
3080.569429	569281.447229	40.167949
3083.069727	570252.118123	40.172967
3086.341714	571253.005734	40.177984
3088.814831	572253.344364	40.183002
3092.294339	573248.720032	40.188020
3094.722397	574255.181202	40.193037
3097.820274	575266.619580	40.198055
3100.643543	576289.110474	40.203072
3103.580557	577329.911603	40.208090
3106.796407	578368.573014	40.213108
3109.685696	579419.240482	40.218125
3113.179959	580457.680760	40.223143
3116.529592	581518.977768	40.228160
3120.190729	582548.988766	40.233178
3124.108588	583599.580654	40.238196
3126.677738	584650.004248	40.243213
3129.949642	585703.279254	40.248231
3133.089995	586770.922538	40.253248
3135.531409	587826.355855	40.258266
3138.842643	588904.308796	40.263284
3141.305451	589980.751471	40.268301
3144.434528	591067.360702	40.273319
3147.372510	592153.651865	40.278336
3150.545285	593261.299839	40.283354
3153.329892	594367.004470	40.288372
3156.344792	595480.432312	40.293389
3159.543773	596588.815283	40.298407
3162.518771	597714.860768	40.303424
3165.394962	598839.061045	40.308442
3168.331193	599982.321854	40.313460
3171.279501	601135.482053	40.318477
3174.505281	602280.470552	40.323495
3177.883413	603435.081774	40.328512
3181.184838	604580.028590	40.333530
3184.786806	605722.008020	40.338548
3188.294228	606887.209900	40.343565
3191.935296	608028.700627	40.348583
3195.607457	609174.874290	40.353600
3198.952477	610313.880941	40.358618
3202.543102	611449.729776	40.363636
3205.448140	612566.018442	40.368653
3208.593386	613709.564123	40.373671
3212.368366	614831.883493	40.378688
3215.930711	615962.075018	40.383706
3219.466581	617080.054988	40.388724
3222.831936	618195.499634	40.393741
3226.081456	619305.950789	40.398759
3229.733257	620413.723216	40.403776
3232.942564	621521.356038	40.408794
3237.088000	622608.431129	40.413812
3240.360936	623671.905295	40.418829
3243.920219	624718.988475	40.423847
3247.116592	625748.443522	40.428864
3250.011509	626779.547934	40.433882
3253.564409	627800.453835	40.438900
3255.427183	628835.775834	40.443917
3258.873167	629872.832654	40.448935
3261.361458	630931.468610	40.453952
3263.981784	631981.687956	40.458970
3266.911032	633058.511716	40.463988
3269.433810	634141.182730	40.469005
3272.400669	635223.768020	40.474023
3275.237625	636339.003493	40.479040
3278.413275	637456.259039	40.484058
3281.478009	638589.430069	40.489076
3284.423814	639715.710741	40.494093
3287.939186	640857.588578	40.499111
3291.090635	642006.782045	40.504128
3294.228167	643174.901657	40.509146
3297.566249	644332.929733	40.514164
3300.679783	645514.898091	40.519181
3303.980133	646685.329454	40.524199
3307.441605	647882.519500	40.529216
3310.768971	649068.672394	40.534234
3314.167664	650265.688152	40.539252
3317.818898	651465.558650	40.544269
3320.807845	652670.277282	40.549287
3324.229241	653882.052400	40.554304
3327.056485	655114.202464	40.559322
3330.232251	656342.753641	40.564340
3332.972373	657587.808241	40.569357
3336.818375	658827.740939	40.574375
3340.278221	660072.608825	40.579392
3343.536175	661321.482859	40.584410
3347.724909	662566.358303	40.589428
3351.726319	663794.828256	40.594445
3355.969501	665036.588182	40.599463
3359.308438	666270.972164	40.604480
3362.939692	667497.635511	40.609498
3366.564689	668709.217582	40.614516
3369.925411	669951.975977	40.619533
3372.965181	671194.375519	40.624551
3376.155729	672432.160670	40.629568
3379.037315	673671.226098	40.634586
3382.649941	674889.872234	40.639604
3385.997902	676150.655294	40.644621
3389.913427	677389.354703	40.649639
3393.833833	678632.211352	40.654656
3397.260150	679865.442401	40.659674
3401.128993	681098.286240	40.664692
3404.383722	682333.549865	40.669709
3408.516650	683555.240231	40.674727
3411.963183	684776.632184	40.679744
3416.638480	685966.622558	40.684762
3422.106666	687117.351315	40.689780
3425.830292	688287.632161	40.694797
3429.290084	689438.198395	40.699815
3432.913822	690576.331667	40.704832
3436.514878	691723.603760	40.709850
3439.847829	692849.139727	40.714868
3442.908819	693992.587258	40.719885
3446.280296	695124.080025	40.724903
3449.513094	696251.433721	40.729920
3452.541582	697402.828560	40.734938
3455.586812	698541.326675	40.739956
3458.743243	699683.228510	40.744973
3461.764979	700847.460011	40.749991
3464.831281	702009.348017	40.755008
3467.809878	703152.750309	40.760013
3470.960780	704254.691956	40.765018
3474.172724	705315.800662	40.770023
3476.798246	706319.857399	40.775028
3479.311311	707277.778852	40.780032
3481.932815	708185.322813	40.785037
3484.726948	709027.449830	40.790042
3486.530531	709823.833084	40.795047
3488.947654	710551.582846	40.800052
3491.412213	711226.446498	40.805056
3493.355085	711847.488222	40.810061
3495.436473	712409.101448	40.815066
3496.960357	712930.669159	40.820071
3499.023685	713410.429385	40.825076
3500.865001	713816.507480	40.830080
3501.967415	714178.723129	40.835085
3503.940285	714497.113734	40.840090
3505.363288	714787.002982	40.845095
3506.355453	715031.157043	40.850100
3507.465920	715226.909117	40.855104
3508.427237	715405.911485	40.860109
3509.920159	715532.826785	40.865114
3510.777516	715638.362591	40.870119
3511.668647	715712.635338	40.875124
3513.114946	715743.503778	40.880128
3513.632179	715760.782918	40.885133
3514.359072	715736.104586	40.890138
3515.145287	715691.372689	40.895143
3515.662554	715627.038066	40.900148
3516.289570	715540.308913	40.905152
3516.755578	715441.400287	40.910157
3517.535331	715309.891016	40.915162
3518.012564	715177.338134	40.920167
3518.356807	715007.443497	40.925172
3519.060096	714841.703648	40.930176
3519.146709	714659.191938	40.935181
3519.424334	714445.036529	40.940186
3519.626493	714243.095102	40.945191
3520.196264	714012.753403	40.950196
3520.698301	713782.912871	40.955200
3520.668815	713538.117330	40.960205
3520.783673	713283.117265	40.965210
3520.784859	713020.237328	40.970215
3520.736385	712749.069166	40.975220
3521.228145	712476.065936	40.980224
3521.045442	712196.514481	40.985229
3521.190828	711910.595919	40.990234
3521.102311	711625.053851	40.995239
3521.361875	711332.544897	41.000244
3521.639037	711037.193480	41.005248
3521.543518	710731.915336	41.010253
3521.647544	710417.955223	41.015258
3521.215905	710118.816884	41.020263
3521.267068	709807.623213	41.025268
3521.558258	709495.584152	41.030272
3521.609647	709183.722287	41.035277
3521.314281	708863.117772	41.040282
3521.455613	708546.798715	41.045287
3521.350806	708231.452137	41.050292
3521.266975	707901.292238	41.055296
3521.399389	707571.729489	41.060301
3521.196002	707247.175836	41.065306
3520.941111	706931.160692	41.070311
3520.673489	706610.616430	41.075316
3521.127351	706290.288680	41.080320
3520.921663	705961.067788	41.085325
3520.900993	705637.665015	41.090330
3520.664167	705314.186499	41.095335
3520.436032	705000.381132	41.100340
3520.474967	704670.524179	41.105344
3519.930829	704357.840617	41.110349
3520.090188	704032.808007	41.115354
3519.991765	703720.524589	41.120359
3519.810448	703407.895835	41.125364
3519.768463	703092.649108	41.130368
3519.615391	702784.862510	41.135373
3519.520498	702462.993172	41.140378
3519.395291	702160.297922	41.145383
3518.998073	701840.691654	41.150388
3519.062997	701522.686928	41.155392
3518.793011	701218.144151	41.160397
3519.265933	700910.038763	41.165402
3518.953777	700614.576769	41.170407
3518.665107	700307.023285	41.175412
3518.833168	700000.129067	41.180416
3518.466108	699705.639521	41.185421
3518.631701	699394.002443	41.190426
3518.063072	699098.879622	41.195431
3518.089256	698799.771137	41.200436
3518.289692	698500.921944	41.205440
3517.932859	698214.434058	41.210445
3517.777403	697913.535724	41.215450
3517.699823	697632.004008	41.220455
3517.374132	697333.898166	41.225460
3517.319156	697046.178837	41.230464
3516.985246	696771.622883	41.235469
3517.054218	696487.295677	41.240474
3516.817024	696205.844263	41.245479
3516.795322	695931.658132	41.250484
3516.759113	695649.111518	41.255488
3516.309752	695379.504242	41.260493
3516.189553	695108.392146	41.265498
3516.044162	694839.563642	41.270503
3515.982544	694567.132258	41.275508
3516.091319	694295.907756	41.280512
3515.742269	694043.650899	41.285517
3515.975824	693777.164742	41.290522
3515.817075	693524.662755	41.295527
3515.425310	693251.648727	41.300532
3515.564055	692984.607352	41.305536
3514.752237	692740.547943	41.310541
3515.199352	692482.941828	41.315546
3514.949231	692240.666269	41.320551
3515.030970	691994.747372	41.325556
3515.327327	691738.487924	41.330560
3514.854766	691485.781078	41.335565
3514.944255	691234.317542	41.340570
3514.609609	690992.221132	41.345575
3514.138867	690747.205074	41.350580
3514.197168	690508.414050	41.355584
3513.830156	690269.686957	41.360589
3513.769093	690036.227251	41.365594
3513.764515	689807.230638	41.370599
3513.785407	689576.183725	41.375604
3513.788976	689339.410920	41.380608
3513.477808	689123.087509	41.385613
3513.602787	688885.386928	41.390618
3513.394093	688664.855214	41.395623
3513.101990	688437.264743	41.400628
3513.003129	688201.374785	41.405632
3512.820248	687991.323782	41.410637
3512.712974	687772.097296	41.415642
3512.781897	687562.890616	41.420647
3512.485361	687344.630732	41.425652
3512.778304	687126.815695	41.430656
3512.244863	686929.839218	41.435661
3512.295430	686711.904922	41.440666
3512.204636	686509.470106	41.445671
3512.100379	686316.341915	41.450676
3512.171857	686109.789370	41.455680
3512.124557	685913.556741	41.460685
3511.916360	685701.415694	41.465690
3512.004693	685503.907204	41.470695
3511.708701	685305.711148	41.475700
3512.014946	685100.690005	41.480704
3511.635104	684898.715123	41.485709
3511.654896	684702.943149	41.490714
3511.317358	684508.321403	41.495719
3511.014458	684313.092278	41.500724
3511.309715	684120.150150	41.505728
3510.811003	683939.733700	41.510733
3510.995957	683758.951725	41.515738
3510.742535	683576.844349	41.520743
3510.524630	683391.490711	41.525748
3510.844004	683205.397155	41.530752
3510.516376	683032.304498	41.535757
3510.421865	682858.672046	41.540762
3510.458927	682684.367153	41.545767
3510.426779	682509.223760	41.550772
3510.598657	682326.722394	41.555776
3510.346129	682156.638691	41.560781
3510.254831	681974.223601	41.565786
3509.875521	681803.755870	41.570791
3510.193575	681637.602443	41.575796
3509.931791	681466.212512	41.580800
3509.705051	681309.257814	41.585805
3509.600849	681140.525374	41.590810
3509.771142	680968.905332	41.595815
3509.723420	680808.226589	41.600820
3509.734700	680646.887744	41.605824
3509.058994	680494.227278	41.610829
3509.254770	680329.016842	41.615834
3509.408751	680175.915104	41.620839
3509.410234	680021.590659	41.625844
3509.380857	679860.194938	41.630848
3508.921843	679717.847401	41.635853
3508.888623	679552.162726	41.640858
3508.908908	679410.129767	41.645863
3508.629459	679254.095284	41.650868
3508.737036	679110.947285	41.655872
3508.766379	678957.148451	41.660877
3508.551382	678813.401489	41.665882
3508.765209	678674.015571	41.670887
3508.254565	678535.195685	41.675892
3508.348578	678390.743392	41.680896
3508.031171	678260.905484	41.685901
3508.428303	678110.967905	41.690906
3508.265430	677967.846918	41.695911
3507.813696	677845.798190	41.700916
3507.994150	677705.107722	41.705920
3507.589571	677581.752220	41.710925
3508.144935	677439.351448	41.715930
3508.121834	677316.078855	41.720935
3507.705115	677181.757616	41.725940
3507.729261	677044.969705	41.730944
3507.624453	676921.854874	41.735949
3507.693185	676794.175023	41.740954
3507.516407	676660.055746	41.745959
3507.315587	676531.370346	41.750964
3507.333002	676406.085650	41.755968
3507.124480	676290.703876	41.760973
3507.190732	676170.042555	41.765978
3506.872001	676059.510152	41.770983
3506.922043	675939.596062	41.775988
3507.279911	675819.131185	41.780992
3506.857114	675709.359383	41.785997
3507.173762	675586.755292	41.791002
3506.681708	675465.130504	41.796007
3506.995263	675360.914561	41.801012
3506.987411	675246.184444	41.806016
3506.888632	675137.099959	41.811021
3507.052156	675012.270793	41.816026
3507.111649	674899.568789	41.821031
3506.702382	674787.241952	41.826036
3506.471173	674676.878068	41.831040
3506.583083	674565.658673	41.836045
3506.583857	674448.624518	41.841050
3506.545964	674340.916323	41.846055
3506.382333	674240.056520	41.851060
3506.693737	674123.764496	41.856064
3506.175002	674032.132841	41.861069
3505.958592	673921.857296	41.866074
3506.106215	673831.559123	41.871079
3506.173459	673734.842936	41.876084
3506.234258	673630.599641	41.881088
3505.861478	673536.396720	41.886093
3506.118677	673421.002224	41.891098
3505.953968	673321.777761	41.896103
3505.943450	673232.945624	41.901108
3506.134506	673134.906664	41.906112
3506.082214	673046.079663	41.911117
3505.762865	672931.272949	41.916122
3505.765473	672839.842590	41.921127
3505.279383	672744.753089	41.926132
3505.880365	672654.568083	41.931136
3505.582461	672567.621748	41.936141
3505.813549	672482.980222	41.941146
3505.721109	672382.238239	41.946151
3505.794372	672288.796624	41.951156
3505.709041	672192.289190	41.956160
3505.464776	672113.456394	41.961165
3505.465875	672012.894425	41.966170
3505.488117	671921.402035	41.971175
3505.156420	671828.571214	41.976180
3505.438697	671741.072628	41.981184
3504.677981	671662.470982	41.986189
3505.134368	671580.626092	41.991194
3505.123764	671496.165220	41.996199
3505.096897	671423.622960	42.001204
3505.325035	671341.165528	42.006208
3505.108203	671265.462342	42.011213
3504.935881	671171.252448	42.016218
3505.036855	671087.367818	42.021223
3504.733462	671003.848447	42.026228
3505.008322	670931.501854	42.031232
3504.621517	670863.452593	42.036237
3504.782813	670774.618726	42.041242
3504.944343	670701.740599	42.046247
3504.621665	670623.955455	42.051252
3504.821078	670551.418962	42.056256
3504.830506	670482.603360	42.061261
3505.001625	670397.155179	42.066266
3504.786185	670324.236710	42.071271
3504.305135	670244.031159	42.076276
3504.492814	670173.288909	42.081280
3504.418049	670103.836192	42.086285
3504.274396	670038.284045	42.091290
3504.401740	669960.768146	42.096295
3504.285615	669906.680235	42.101300
3504.661297	669833.261341	42.106304
3503.976309	669765.851881	42.111309
3504.125751	669696.608469	42.116314
3504.142794	669629.630584	42.121319
3504.133523	669567.942832	42.126324
3504.251890	669493.915521	42.131328
3504.373823	669429.163067	42.136333
3504.064574	669363.982717	42.141338
3504.006009	669297.713182	42.146343
3503.692365	669238.866409	42.151348
3504.098190	669168.379840	42.156352
3503.924961	669118.935006	42.161357
3504.084956	669057.515196	42.166362
3504.210452	668988.669558	42.171367
3503.905678	668939.544769	42.176372
3504.229146	668863.683194	42.181376
3503.769787	668802.812961	42.186381
3503.821656	668737.219501	42.191386
3503.637910	668683.484910	42.196391
3503.669922	668630.362735	42.201396
3504.177901	668564.942084	42.206400
3503.643934	668510.117252	42.211405
3503.461348	668452.341211	42.216410
3503.537263	668389.135432	42.221415
3503.316253	668347.824351	42.226420
3503.446809	668296.429711	42.231424
3503.376681	668248.659124	42.236429
3503.188676	668201.705818	42.241434
3503.632733	668147.664932	42.246439
3503.486886	668089.681104	42.251444
3503.385420	668037.525361	42.256448
3503.088132	667982.608489	42.261453
3503.375460	667935.076524	42.266458
3503.059145	667897.570033	42.271463
3503.287790	667854.137450	42.276468
3503.009060	667796.872109	42.281472
3502.982441	667755.925366	42.286477
3503.125505	667704.824744	42.291482
3503.365103	667650.016745	42.296487
3503.033954	667614.107761	42.301492
3503.019388	667563.381595	42.306496
3503.144205	667525.900497	42.311501
3502.877448	667479.854503	42.316506
3503.186787	667439.748743	42.321511
3502.840002	667399.152669	42.326516
3503.086984	667343.593461	42.331520
3502.875367	667305.668278	42.336525
3502.830290	667266.917302	42.341530
3503.053990	667216.948035	42.346535
3502.880663	667182.008992	42.351540
3503.221368	667132.219476	42.356544
3502.917682	667104.285327	42.361549
3502.604802	667050.812271	42.366554
3502.705023	667013.083805	42.371559
3502.459833	666983.293935	42.376564
3502.980732	666938.412134	42.381568
3502.731997	666900.291935	42.386573
3502.677837	666855.405013	42.391578
3502.901304	666812.966238	42.396583
3502.805590	666781.454950	42.401588
3502.943128	666735.139003	42.406592
3502.819879	666701.636595	42.411597
3503.019623	666662.194192	42.416602
3503.168535	666614.628642	42.421607
3502.825918	666584.354768	42.426612
3503.253827	666525.418539	42.431616
3503.090637	666494.366432	42.436621
3502.690068	666439.357961	42.441626
3502.765682	666394.547199	42.446631
3502.453232	666360.975090	42.451636
3502.511045	666329.436939	42.456640
3502.610216	666298.191173	42.461645
3502.542650	666259.589487	42.466650
3502.733172	666224.985910	42.471655
3502.661882	666187.132864	42.476660
3502.466018	666148.502045	42.481664
3502.435387	666113.635285	42.486669
3502.325107	666079.729444	42.491674
3502.605108	666042.316655	42.496679
3502.294570	666018.571118	42.501684
3502.528766	665983.360783	42.506688
3502.644386	665948.070135	42.511693
3502.195017	665924.596755	42.516698
3502.547741	665894.105997	42.521703
3502.469512	665860.243972	42.526708
3502.390434	665821.143521	42.531712
3502.683072	665787.419506	42.536717
3502.583143	665748.920888	42.541722
3502.561987	665722.532492	42.546727
3502.350806	665693.082208	42.551732
3502.381604	665644.084524	42.556736
3502.255814	665616.715311	42.561741
3502.242886	665593.518225	42.566746
3502.344545	665545.456257	42.571751
3502.052379	665543.459131	42.576756
3502.393835	665503.290054	42.581760
3502.353658	665479.298929	42.586765
3502.234164	665447.936851	42.591770
3502.271781	665410.461871	42.596775
3502.015871	665386.805520	42.601780
3502.097208	665351.917480	42.606784
3502.420900	665330.510145	42.611789
3502.167665	665300.516786	42.616794
3502.746375	665269.487770	42.621799
3502.447626	665239.950778	42.626804
3502.382877	665205.236028	42.631808
3502.758900	665173.042761	42.636813
3502.284488	665136.299943	42.641818
3502.119520	665106.640644	42.646823
3502.035562	665089.940255	42.651828
3501.943428	665053.333517	42.656832
3501.849553	665037.632555	42.661837
3501.707787	665007.071020	42.666842
3502.127280	664985.996344	42.671847
3502.082676	664956.316688	42.676852
3502.220701	664932.095165	42.681856
3502.359535	664902.734289	42.686861
3502.189648	664868.784117	42.691866
3502.276857	664844.570771	42.696871
3502.035917	664815.521867	42.701876
3502.145016	664789.458642	42.706880
3501.897373	664765.998972	42.711885
3501.587973	664735.314589	42.716890
3502.113942	664716.666612	42.721895
3501.828641	664699.050799	42.726900
3501.635079	664676.180722	42.731904
3501.522592	664652.798230	42.736909
3501.863703	664634.679606	42.741914
3502.040805	664615.839609	42.746919
3501.819534	664606.246335	42.751924
3501.750718	664563.995593	42.756928
3501.929653	664552.489954	42.761933
3501.778459	664525.121821	42.766938
3502.050748	664497.434139	42.771943
3501.915701	664487.028146	42.776948
3502.031483	664462.908910	42.781952
3502.014337	664440.557983	42.786957
3501.499594	664406.862758	42.791962
3501.789773	664392.843676	42.796967
3501.604459	664382.595569	42.801972
3501.904941	664355.900770	42.806977
3501.979192	664329.792160	42.811981
3501.830009	664312.751914	42.816986
3502.028784	664300.544125	42.821991
3501.861011	664277.419346	42.826996
3501.930530	664244.125970	42.832001
3501.937092	664223.367361	42.837005
3501.796013	664207.423351	42.842010
3501.743477	664177.692700	42.847015
3501.909290	664165.190797	42.852020
3502.044533	664132.135665	42.857025
3501.912840	664110.451584	42.862029
3501.931868	664101.466776	42.867034
3502.140954	664060.914357	42.872039
3502.060542	664044.061865	42.877044
3502.151135	664016.352929	42.882049
3501.665077	663999.218102	42.887053
3501.653898	663964.889209	42.892058
3501.786206	663952.592166	42.897063
3501.558424	663937.859629	42.902068
3501.799571	663904.836114	42.907073
3501.651902	663902.465459	42.912077
3501.703980	663881.898190	42.917082
3501.637800	663861.749622	42.922087
3501.279819	663834.214096	42.927092
3501.359686	663826.017381	42.932097
3501.546183	663790.657190	42.937101
3501.475029	663786.527342	42.942106
3501.315414	663778.769369	42.947111
3501.443614	663771.063625	42.952116
3501.708066	663742.526758	42.957121
3501.877268	663736.959944	42.962125
3501.877753	663716.600452	42.967130
3501.730202	663701.654690	42.972135
3501.618230	663682.710939	42.977140
3501.693734	663650.462444	42.982145
3501.733246	663644.368096	42.987149
3501.563742	663618.647151	42.992154
3502.093651	663595.006215	42.997159
3501.588373	663579.919777	43.002164
3501.635933	663551.517993	43.007169
3501.789341	663543.458589	43.012173
3501.795348	663529.086003	43.017178
3502.081052	663509.776778	43.022183
3501.861731	663498.535307	43.027188
3501.768599	663459.527363	43.032193
3501.893992	663444.985215	43.037197
3501.257027	663422.285235	43.042202
3501.565842	663404.818371	43.047207
3501.277173	663406.662705	43.052212
3501.577980	663382.410379	43.057217
3501.486948	663360.119055	43.062221
3501.624050	663363.390115	43.067226
3501.802093	663325.833896	43.072231
3501.431734	663327.492134	43.077236
3501.868206	663297.977367	43.082241
3501.803174	663279.025064	43.087245
3501.424546	663266.462264	43.092250
3501.339880	663249.858600	43.097255
3501.171749	663232.170826	43.102260
3501.239335	663212.897055	43.107265
3501.274377	663216.185032	43.112269
3501.239049	663208.006830	43.117274
3501.360673	663186.777838	43.122279
3501.334144	663179.296808	43.127284
3501.175417	663156.167837	43.132289
3501.448826	663166.902005	43.137293
3501.435376	663153.629957	43.142298
3501.784699	663125.676085	43.147303
3501.301774	663117.172547	43.152308
3501.451745	663106.817762	43.157313
3501.601204	663070.163545	43.162317
3501.516632	663061.244793	43.167322
3501.782731	663047.826590	43.172327
3501.468228	663024.224003	43.177332
3501.423261	663011.406109	43.182337
3501.338931	663009.623618	43.187341
3501.415792	662985.756639	43.192346
3501.647765	662970.547400	43.197351
3501.428720	662966.391736	43.202356
3501.327409	662949.890116	43.207361
3501.510104	662933.990295	43.212365
3501.279939	662914.715232	43.217370
3501.676328	662912.004890	43.222375
3501.377695	662902.522507	43.227380
3501.356800	662878.022651	43.232385
3501.210203	662869.463309	43.237389
3501.035654	662858.563027	43.242394
3501.475330	662853.549869	43.247399
3501.223851	662834.926938	43.252404
3501.116463	662818.825342	43.257409
3501.199729	662815.917195	43.262413
3501.064534	662813.893546	43.267418
3501.323123	662807.612747	43.272423
3501.146628	662789.875638	43.277428
3501.210685	662765.511173	43.282433
3501.140649	662759.035125	43.287437
3501.359504	662757.501916	43.292442
3501.398680	662759.092566	43.297447
3501.129131	662749.255884	43.302452
3501.126583	662727.946592	43.307457
3501.693386	662729.300330	43.312461
3501.220574	662718.848431	43.317466
3501.339871	662699.515183	43.322471
3501.317913	662692.282551	43.327476
3501.442700	662679.635785	43.332481
3501.576353	662677.368051	43.337485
3501.504626	662665.951496	43.342490
3501.187391	662642.248611	43.347495
3500.939673	662645.982765	43.352500
3501.174334	662632.569183	43.357505
3501.605355	662634.145001	43.362509
3501.639947	662605.493042	43.367514
3501.444318	662595.544173	43.372519
3501.396805	662583.973798	43.377524
3501.369837	662569.655139	43.382529
3501.179268	662543.884898	43.387533
3501.211509	662551.415657	43.392538
3501.043023	662540.464106	43.397543
3500.815294	662534.463130	43.402548
3501.327198	662529.288149	43.407553
3501.318842	662500.143904	43.412557
3501.050843	662492.851971	43.417562
3501.526938	662482.891786	43.422567
3501.189295	662489.785020	43.427572
3501.257918	662472.855242	43.432577
3501.370151	662446.934884	43.437581
3500.836048	662442.581524	43.442586
3501.402254	662439.942803	43.447591
3501.156982	662446.820801	43.452596
3500.955414	662434.127835	43.457601
3501.057307	662406.911483	43.462605
3501.312372	662401.728973	43.467610
3501.377997	662398.474263	43.472615
3501.113819	662398.767598	43.477620
3501.079222	662390.788213	43.482625
3501.462911	662389.377429	43.487629
3500.968531	662359.414743	43.492634
3501.354476	662350.018309	43.497639
3501.115543	662332.939481	43.502644
3500.957364	662336.708864	43.507649
3501.357808	662342.531969	43.512653
3500.985407	662319.885476	43.517658
3501.346004	662295.071553	43.522663
3500.813029	662290.967477	43.527668
3501.099988	662293.565328	43.532673
3501.294520	662289.740286	43.537677
3501.169311	662287.265701	43.542682
3501.088239	662265.868551	43.547687
3500.870301	662251.231621	43.552692
3500.887640	662246.437676	43.557697
3501.016528	662241.275934	43.562701
3500.891691	662240.847525	43.567706
3500.857392	662237.309823	43.572711
3501.019982	662240.127876	43.577716
3500.970723	662231.202520	43.582721
3500.801547	662239.565347	43.587725
3500.999513	662246.519961	43.592730
3501.061200	662221.505706	43.597735
3500.711468	662205.942224	43.602740
3500.820621	662189.254794	43.607745
3500.750166	662195.155812	43.612749
3500.906844	662198.124581	43.617754
3500.834035	662189.652258	43.622759
3500.863834	662195.337072	43.627764
3500.997137	662192.620103	43.632769
3501.078108	662191.558774	43.637773
3500.737501	662198.702248	43.642778
3501.203030	662189.092870	43.647783
3500.910113	662193.134120	43.652788
3500.892531	662186.449383	43.657793
3501.074635	662162.962249	43.662797
3500.837025	662154.317494	43.667802
3501.224479	662154.702779	43.672807
3500.855005	662153.067071	43.677812
3500.603067	662148.517216	43.682817
3500.890199	662148.569718	43.687821
3500.880933	662151.466108	43.692826
3500.828800	662149.179046	43.697831
3500.581546	662152.863403	43.702836
3500.927555	662156.349894	43.707841
3500.863882	662150.670929	43.712845
3500.850615	662150.822985	43.717850
3500.892186	662146.174713	43.722855
3500.787124	662150.035207	43.727860
3500.893565	662139.087673	43.732865
3500.926027	662116.273975	43.737869
3501.124982	662108.355576	43.742874
3500.913731	662096.961407	43.747879
3500.726673	662102.732023	43.752884
3501.102878	662093.087404	43.757889
3500.959323	662105.688402	43.762893
3500.684612	662101.391835	43.767898
3500.809996	662098.276875	43.772903
3500.968413	662105.787129	43.777908
3500.820651	662095.730014	43.782913
3500.870661	662097.867985	43.787917
3500.862210	662101.812350	43.792922
3501.261601	662091.614896	43.797927
3501.149280	662071.570032	43.802932
3501.163831	662055.996014	43.807937
3501.182583	662052.649114	43.812941
3500.846248	662059.193070	43.817946
3501.209400	662049.101380	43.822951
3501.161398	662057.843614	43.827956
3501.258583	662038.412879	43.832961
3501.088334	662011.539848	43.837965
3501.237848	662012.313831	43.842970
3501.113157	662006.445226	43.847975
3500.752783	662011.246345	43.852980
3500.824023	662012.532361	43.857985
3501.300151	662007.412927	43.862989
3500.522767	661996.212020	43.867994
3500.719900	661983.552389	43.872999
3500.631348	661972.836532	43.878004
3500.782182	661981.396244	43.883009
3501.093869	661965.772974	43.888013
3500.940737	661977.227793	43.893018
3501.236200	661968.245223	43.898023
3500.855343	661983.530824	43.903028
3500.885308	661975.590336	43.908033
3501.142157	661973.900997	43.913037
3500.998343	661979.065622	43.918042
3501.104651	661972.559901	43.923047
3500.890525	661949.537012	43.928052
3500.764258	661938.228430	43.933057
3500.919977	661923.728891	43.938061
3501.104340	661933.680589	43.943066
3501.478308	661923.836531	43.948071
3501.204891	661929.322062	43.953076
3501.207351	661922.933291	43.958081
3501.058481	661908.683709	43.963085
3500.730121	661894.663410	43.968090
3501.103520	661869.696551	43.973095
3501.377513	661886.720766	43.978100
3500.926453	661872.021968	43.983105
3501.151407	661880.819072	43.988109
3500.949510	661886.891732	43.993114
3501.195126	661870.580483	43.998119
3500.973535	661857.890067	44.003124
3501.062584	661837.412153	44.008129
3501.164647	661829.509541	44.013133
3500.709345	661832.330010	44.018138
3501.019492	661825.890324	44.023143
3501.212718	661832.197182	44.028148
3501.046313	661832.773837	44.033153
3501.402839	661808.907644	44.038157
3500.852652	661803.807986	44.043162
3501.123915	661789.738348	44.048167
3500.964423	661796.802273	44.053172
3500.574972	661794.121677	44.058177
3500.779239	661803.271647	44.063181
3500.629584	661791.517561	44.068186
3501.035450	661785.860603	44.073191
3500.847035	661791.731451	44.078196
3500.585731	661784.737339	44.083201
3501.049296	661796.040541	44.088205
3500.927357	661790.570637	44.093210
3500.974570	661793.357978	44.098215
3500.696214	661770.445100	44.103220
3501.052461	661756.461190	44.108225
3501.377796	661745.277392	44.113229
3500.926005	661752.888767	44.118234
3500.854009	661744.815207	44.123239
3501.001201	661753.675190	44.128244
3500.999944	661740.848385	44.133249
3501.169372	661747.658342	44.138253
3500.802697	661736.888366	44.143258
3500.690866	661709.905019	44.148263
3500.641282	661707.018496	44.153268
3500.857441	661711.524835	44.158273
3500.835295	661702.295042	44.163277
3500.513656	661700.601439	44.168282
3500.678088	661704.866773	44.173287
3500.793425	661707.842527	44.178292
3500.686715	661700.173957	44.183297
3500.710860	661704.312743	44.188301
3500.612737	661698.639205	44.193306
3501.109511	661705.295270	44.198311
3500.856804	661707.782824	44.203316
3501.122527	661709.935142	44.208321
3501.030546	661717.137702	44.213325
3500.536079	661712.428077	44.218330
3500.436782	661702.662011	44.223335
3500.640219	661701.979679	44.228340
3500.851846	661699.000072	44.233345
3501.086106	661698.262735	44.238349
3500.947409	661712.310870	44.243354
3501.055263	661702.810036	44.248359
3500.822753	661711.882543	44.253364
3500.613799	661703.532116	44.258369
3501.180360	661703.288885	44.263373
3501.158338	661687.021559	44.268378
3500.812743	661665.517063	44.273383
3501.153456	661661.368147	44.278388
3500.954298	661668.838013	44.283393
3501.262207	661657.307612	44.288397
3500.892880	661673.390381	44.293402
3501.290768	661664.490426	44.298407
3501.018705	661650.310734	44.303412
3501.089033	661633.079734	44.308417
3501.070601	661633.881504	44.313421
3500.869420	661627.126899	44.318426
3500.848035	661622.289133	44.323431
3500.676353	661624.663494	44.328436
3500.501053	661629.583950	44.333441
3500.760054	661627.894196	44.338445
3500.813308	661629.682353	44.343450
3501.126061	661624.839278	44.348455
3501.173835	661622.535580	44.353460
3500.880433	661625.029880	44.358465
3501.247351	661616.733941	44.363469
3500.820600	661600.433534	44.368474
3500.914954	661581.052262	44.373479
3501.055376	661591.360958	44.378484
3500.763358	661573.490970	44.383489
3501.027609	661576.242506	44.388493
3500.779999	661586.665248	44.393498
3501.000462	661581.388197	44.398503
3501.218324	661584.945988	44.403508
3501.282990	661581.840897	44.408513
3500.978187	661564.422213	44.413517
3500.642099	661551.999878	44.418522
3500.681806	661535.821920	44.423527
3500.941466	661542.267724	44.428532
3500.785170	661535.355901	44.433537
3500.913431	661535.384753	44.438541
3500.982276	661542.910248	44.443546
3501.137734	661538.592247	44.448551
3500.827944	661543.734621	44.453556
3500.875253	661531.698107	44.458561
3501.216238	661533.987763	44.463565
3500.962271	661513.266380	44.468570
3500.953971	661503.934285	44.473575
3501.077812	661495.329028	44.478580
3500.755550	661514.149463	44.483585
3500.982555	661499.288122	44.488589
3500.674263	661501.834827	44.493594
3501.030734	661499.579907	44.498599
3500.722625	661502.176494	44.503604
3500.569625	661495.164272	44.508609
3500.800436	661498.021182	44.513613
3500.666022	661505.580298	44.518618
3500.964977	661500.439968	44.523623
3501.099393	661494.079018	44.528628
3500.905526	661494.510494	44.533633
3501.217648	661489.318069	44.538637
3500.873559	661481.189433	44.543642
3500.897029	661467.759230	44.548647
3501.011332	661459.904206	44.553652
3501.204689	661470.254196	44.558657
3501.431696	661456.041651	44.563661
3500.965654	661466.001496	44.568666
3501.035281	661447.222993	44.573671
3501.000946	661429.060588	44.578676
3501.165003	661420.847921	44.583681
3501.404854	661418.163041	44.588685
3501.062166	661417.371295	44.593690
3501.044815	661410.336594	44.598695
3501.497653	661404.621741	44.603700
3501.232472	661392.736524	44.608705
3501.384015	661368.254256	44.613709
3501.069246	661370.502587	44.618714
3501.244370	661363.136564	44.623719
3501.193505	661340.334808	44.628724
3501.113855	661331.463557	44.633729
3501.266762	661327.095971	44.638733
3501.041846	661329.229635	44.643738
3501.539257	661333.290365	44.648743
3501.173822	661312.487147	44.653748
3501.238215	661312.077335	44.658753
3501.298944	661292.102082	44.663757
3501.127051	661295.774307	44.668762
3501.395414	661290.339442	44.673767
3501.251034	661276.138099	44.678772
3500.926624	661254.828841	44.683777
3501.530781	661240.353996	44.688781
3501.101439	661240.375175	44.693786
3501.341038	661236.442445	44.698791
3501.440204	661219.555340	44.703796
3501.489549	661216.502579	44.708801
3501.981907	661201.796585	44.713805
3501.389277	661184.674353	44.718810
3501.207621	661163.341302	44.723815
3501.012549	661164.621530	44.728820
3501.013044	661164.471842	44.733825
3501.193036	661156.905202	44.738829
3501.165036	661150.021814	44.743834
3501.170869	661123.516528	44.748839
3501.356344	661120.690811	44.753844
3500.996612	661110.168559	44.758849
3501.365072	661116.496838	44.763853
3501.006183	661105.674956	44.768858
3501.044910	661083.806163	44.773863
3501.084924	661078.908064	44.778868
3500.997087	661077.874512	44.783873
3500.961549	661066.100684	44.788877
3500.979026	661076.430249	44.793882
3501.206096	661070.602769	44.798887
3501.509374	661074.895351	44.803892
3501.193488	661047.195163	44.808897
3500.992171	661034.450401	44.813901
3501.073637	661042.423432	44.818906
3501.382483	661024.253467	44.823911
3501.639878	661017.821967	44.828916
3501.516292	660996.578781	44.833921
3501.239232	660988.338820	44.838925
3501.111849	660984.266978	44.843930
3501.157839	660978.469371	44.848935
3501.193091	660962.191362	44.853940
3501.137139	660943.183062	44.858945
3501.270228	660936.222984	44.863949
3501.171606	660948.268991	44.868954
3501.196885	660940.578006	44.873959
3501.289982	660907.768386	44.878964
3501.042681	660902.718020	44.883969
3501.299277	660895.537840	44.888973
3500.983751	660898.934459	44.893978
3500.971053	660886.807230	44.898983
3501.115820	660894.121021	44.903988
3500.801349	660872.759363	44.908993
3501.426891	660854.586658	44.913997
3501.097360	660855.389990	44.919002
3501.192706	660844.941986	44.924007
3501.169719	660845.794489	44.929012
3500.967022	660854.713121	44.934017
3501.256973	660842.336156	44.939021
3500.831432	660820.942825	44.944026
3501.068692	660802.285118	44.949031
3501.037321	660802.140691	44.954036
3500.818377	660802.077180	44.959041
3501.030297	660793.107333	44.964045
3500.974867	660804.297809	44.969050
3501.035717	660794.903687	44.974055
3501.322583	660804.490196	44.979060
3501.305959	660778.087510	44.984065
3501.115739	660765.490308	44.989069
3500.966357	660765.065887	44.994074
3500.924597	660759.132902	44.999079
3501.023775	660764.407761	45.004084
3501.011329	660762.662889	45.009089
3501.055635	660753.870456	45.014093
3500.957360	660728.529369	45.019098
3501.048539	660719.828991	45.024103
3500.853701	660717.165843	45.029108
3500.861121	660712.722194	45.034113
3500.878853	660715.814217	45.039117
3500.920018	660713.411563	45.044122
3501.003901	660711.850428	45.049127
3500.936054	660715.106344	45.054132
3500.711012	660718.737653	45.059137
3501.195737	660714.614453	45.064141
3501.186148	660691.904184	45.069146
3501.035697	660684.291954	45.074151
3501.113301	660677.241028	45.079156
3500.896507	660676.528244	45.084161
3501.253043	660669.281464	45.089165
3501.183449	660670.291435	45.094170
3501.283941	660658.245048	45.099175
3501.119776	660641.400458	45.104180
3501.062043	660633.573198	45.109185
3501.391775	660634.317510	45.114189
3500.987161	660633.735597	45.119194
3501.058989	660632.825360	45.124199
3501.195540	660621.272136	45.129204
3501.312458	660603.582357	45.134209
3501.463417	660600.862028	45.139213
3501.240129	660599.551308	45.144218
3501.138579	660594.177190	45.149223
3501.435386	660567.173044	45.154228
3501.200207	660552.236887	45.159233
3500.955835	660546.337257	45.164237
3501.180539	660560.077414	45.169242
3501.168677	660549.946315	45.174247
3501.243060	660531.464758	45.179252
3501.074350	660517.266322	45.184257
3501.380982	660505.385347	45.189261
3501.318533	660508.291018	45.194266
3501.470247	660503.773508	45.199271
3501.339174	660491.266009	45.204276
3501.309647	660469.407113	45.209281
3501.553762	660464.175467	45.214285
3501.410049	660464.948120	45.219290
3501.228243	660437.972796	45.224295
3501.310467	660421.636201	45.229300
3501.095456	660423.768424	45.234305
3501.221199	660409.670921	45.239309
3501.086129	660418.878283	45.244314
3501.182981	660384.618656	45.249319
3501.293576	660372.270736	45.254324
3501.362974	660372.758585	45.259329
3501.280076	660372.722504	45.264333
3501.107164	660359.672650	45.269338
3501.267351	660334.487493	45.274343
3501.120357	660325.227104	45.279348
3501.268359	660329.595599	45.284353
3500.826607	660322.979677	45.289357
3500.820524	660326.924373	45.294362
3500.965840	660321.010121	45.299367
3500.922514	660322.015787	45.304372
3500.926103	660306.740281	45.309377
3501.271176	660280.326384	45.314381
3500.985473	660281.921215	45.319386
3501.221717	660271.000042	45.324391
3501.160575	660268.664105	45.329396
3501.063868	660265.086077	45.334401
3501.139280	660270.814401	45.339405
3501.349212	660261.594800	45.344410
3501.341468	660240.330813	45.349415
3501.542614	660228.766448	45.354420
3500.857110	660227.432227	45.359425
3501.381019	660226.896509	45.364429
3501.154400	660206.167809	45.369434
3501.018974	660189.816875	45.374439
3501.523115	660186.938224	45.379444
3500.700119	660188.422191	45.384449
3501.046399	660194.754743	45.389453
3501.401920	660176.974835	45.394458
3500.953633	660158.079757	45.399463
3501.154648	660142.471849	45.404468
3500.939202	660143.306301	45.409473
3501.131147	660138.831893	45.414477
3501.117792	660142.378511	45.419482
3500.985621	660128.273306	45.424487
3500.894746	660110.966408	45.429492
3500.636860	660105.318339	45.434497
3500.839902	660096.099721	45.439501
3500.765312	660098.807842	45.444506
3500.739248	660096.166549	45.449511
3501.149922	660092.354845	45.454516
3500.914084	660101.579160	45.459521
3501.177945	660092.849683	45.464525
3501.017150	660096.670283	45.469530
3501.198439	660090.400509	45.474535
3501.156860	660093.652291	45.479540
3500.597073	660088.752981	45.484545
3500.981260	660060.484998	45.489549
3501.000680	660067.870048	45.494554
3501.164619	660054.614354	45.499559
3501.039967	660049.992549	45.504564
3500.737640	660052.638480	45.509569
3500.911009	660050.213814	45.514573
3501.101254	660057.121362	45.519578
3501.170108	660058.108515	45.524583
3501.261954	660046.112718	45.529588
3501.078662	660024.977112	45.534593
3501.211561	660006.235286	45.539597
3501.094083	660007.053559	45.544602
3501.301331	660002.227119	45.549607
3501.177051	659999.651952	45.554612
3500.783835	659985.390001	45.559617
3500.976105	659965.090759	45.564621
3500.557726	659963.512671	45.569626
3501.103163	659953.189006	45.574631
3501.011155	659943.469882	45.579636
3501.129428	659948.192905	45.584641
3500.837659	659957.676202	45.589645
3500.940530	659962.900967	45.594650
3500.940910	659958.358295	45.599655
3501.173045	659961.165524	45.604660
3500.958769	659950.767730	45.609665
3501.317436	659932.787176	45.614669
3500.853418	659928.920286	45.619674
3500.926932	659917.626246	45.624679
3500.819871	659913.101310	45.629684
3500.450544	659914.510338	45.634689
3501.224135	659900.354951	45.639693
3500.814174	659909.508384	45.644698
3501.046154	659910.917877	45.649703
3501.123943	659909.457462	45.654708
3500.971921	659911.729147	45.659713
3500.887729	659892.124410	45.664717
3500.934231	659890.769004	45.669722
3500.752236	659884.958503	45.674727
3500.949013	659898.604372	45.679732
3500.761780	659891.596645	45.684737
3500.983528	659889.263785	45.689741
3500.695630	659897.448563	45.694746
3500.797195	659888.995329	45.699751
3501.131093	659883.099566	45.704756
3500.931667	659889.672267	45.709761
3500.897107	659887.182083	45.714765
3500.855201	659891.582162	45.719770
3500.930147	659891.819516	45.724775
3501.329754	659868.240965	45.729780
3500.806526	659855.248328	45.734785
3500.858903	659833.574149	45.739789
3500.847054	659841.363906	45.744794
3500.983301	659828.312164	45.749799
3500.933550	659834.161273	45.754804
3500.563426	659839.713880	45.759809
3500.948204	659843.494334	45.764813
3501.045087	659812.777069	45.769818
3500.659562	659752.286514	45.774823
3500.802393	659632.051698	45.779828
3500.497319	659472.500425	45.784833
3500.962175	659245.022809	45.789837
3500.625895	658962.804436	45.794842
3500.677802	658613.361912	45.799847
3500.500803	658218.659034	45.804852
3500.069225	657766.711018	45.809857
3499.408887	657249.715956	45.814861
3499.356341	656696.139246	45.819866
3499.007697	656075.161318	45.824871
3498.975929	655394.858891	45.829876
3498.282256	654673.312597	45.834881
3497.950626	653877.176663	45.839885
3497.475114	653029.945999	45.844890
3497.069325	652124.378109	45.849895
3496.245153	651163.835597	45.854900
3495.615686	650155.547041	45.859905
3495.181655	649086.654510	45.864909
3494.751743	647959.669612	45.869914
3493.978557	646756.235456	45.874919
3493.460145	645514.171050	45.879924
3492.641357	644215.804687	45.884929
3492.048787	642854.227496	45.889933
3491.281538	641427.580612	45.894938
3490.419310	639944.928134	45.899943
3489.780156	638409.045732	45.904948
3488.804220	636824.756556	45.909953
3488.058656	635157.916275	45.914957
3487.214104	633459.093185	45.919962
3485.748767	631691.465166	45.924967
3485.306994	629860.234786	45.929972
3484.238154	627979.515085	45.934977
3483.252795	626033.987903	45.939981
3482.091955	624040.645251	45.944986
3480.834171	621992.034134	45.949991
3480.084959	619870.485121	45.954996
3478.715091	617711.984413	45.960001
3477.570607	615491.205205	45.965005
3476.272989	613212.588281	45.970010
3475.027224	610898.838221	45.975015
3473.582208	608513.657601	45.980020
3472.317289	606086.546700	45.985025
3471.257880	603595.295162	45.990029
3469.594919	601065.751319	45.995034
3467.862699	598470.692354	46.000039
3466.583207	595827.570522	46.005044
3465.186027	593145.343970	46.010049
3463.463118	590400.460853	46.015053
3462.101170	587611.867481	46.020058
3460.338296	584767.952770	46.025063
3458.913085	581880.729770	46.030068
3457.152821	578951.542916	46.035073
3455.564224	575958.956385	46.040077
3454.064929	572924.078373	46.045082
3451.888712	569824.062679	46.050087
3450.540124	566687.214719	46.055092
3448.387574	563490.623138	46.060097
3446.831938	560258.549189	46.065101
3445.042731	556990.256720	46.070106
3442.724806	553659.624445	46.075111
3441.192983	550283.586057	46.080116
3439.180987	546875.990129	46.085121
3437.283761	543402.535158	46.090125
3435.465882	539895.370212	46.095130
3433.321931	536340.320902	46.100135
3430.866158	532742.559080	46.105140
3428.851198	529107.443012	46.110145
3427.026775	525421.063720	46.115149
3424.756798	521688.955954	46.120154
3422.831803	517916.677126	46.125159
3420.642014	514101.533575	46.130164
3418.083565	510242.868547	46.135169
3416.021473	506336.275850	46.140173
3413.737175	502397.782909	46.145178
3411.192994	498407.107548	46.150183
3409.027088	494381.829360	46.155188
3406.414760	490330.729724	46.160193
3403.986505	486210.632104	46.165197
3401.682904	482084.340730	46.170202
3399.271804	477899.550375	46.175207
3396.690875	473685.878692	46.180212
3394.079695	469434.690210	46.185217
3391.705367	465129.163494	46.190221
3389.236508	460802.381688	46.195226
3386.223710	456442.158384	46.200231
3383.931864	452022.577601	46.205236
3381.569931	447593.909853	46.210241
3378.863689	443105.645106	46.215245
3376.096734	438601.303184	46.220250
3373.116180	434044.285324	46.225255
3370.766275	429455.964162	46.230260
3367.805117	424852.491004	46.235265
3364.977535	420196.896960	46.240269
3362.014220	415510.602199	46.245274
3359.118339	410811.003727	46.250279
3356.412895	406047.375450	46.255284
3353.609364	401281.187271	46.260289
3350.912497	396477.087225	46.265293
3347.777169	391642.467860	46.270298
3344.591957	386773.669126	46.275303
3341.699927	381884.298046	46.280308
3338.529329	376955.222513	46.285313
3335.390379	371996.422259	46.290317
3332.301840	367032.377090	46.295322
3328.950648	362040.072055	46.300327
3326.354503	357018.570079	46.305332
3322.977219	351960.793150	46.310337
3319.653671	346878.428201	46.315341
3316.635005	341781.610987	46.320346
3312.876173	336666.852164	46.325351
3310.265441	331518.061468	46.330356
3306.480069	326364.486228	46.335361
3303.634965	321169.737808	46.340365
3300.417113	315954.169390	46.345370
3296.726934	310723.224941	46.350375
3293.333601	305467.974014	46.355380
3289.692834	300199.384737	46.360385
3286.606703	294916.008413	46.365389
3282.935987	289618.372900	46.370394
3279.211395	284296.187528	46.375399
3275.640382	278963.968330	46.380404
3272.028242	273628.558053	46.385409
3268.751337	268278.088762	46.390413
3265.025294	262909.899913	46.395418
3261.305936	257526.296528	46.400423
3257.847905	252131.884266	46.405428
3254.336496	246739.996974	46.410433
3250.533978	241318.164922	46.415437
3246.695298	235891.522249	46.420442
3242.722684	230471.915256	46.425447
3238.900487	225024.575725	46.430452
3235.069193	219591.282275	46.435457
3231.048336	214141.343722	46.440461
3227.297486	208694.203783	46.445466
3223.291262	203170.124360	46.450471
3219.549564	197695.826206	46.455476
3215.547487	192240.993791	46.460481
3211.558456	186777.250279	46.465485
3207.647180	181321.831496	46.470490
3203.447996	175862.455402	46.475495
3199.511253	170401.807535	46.480500
3195.277347	164959.877673	46.485505
3191.041240	159504.852840	46.490509
3187.026024	154065.787183	46.495514
3182.698884	148619.749232	46.500519
3178.389845	143191.149825	46.505524
3173.894337	137780.779149	46.510529
3169.598899	132371.726023	46.515533
3165.160333	126982.701857	46.520538
3160.732765	121598.641860	46.525543
3156.466299	116219.150975	46.530548
3151.861359	110869.176909	46.535553
3147.208571	105524.453259	46.540557
3142.758948	100201.972280	46.545562
3138.000830	94909.001324	46.550567
3133.590260	89616.911643	46.555572
3128.866533	84367.113040	46.560577
3124.078772	79125.338826	46.565581
3119.108796	73910.147292	46.570586
3114.466760	68732.139781	46.575591
3109.753580	63576.174752	46.580596
3104.359451	58443.854363	46.585601
3099.400092	53343.587316	46.590605
3094.230199	48291.922598	46.595610
3088.640312	43270.210843	46.600615
3083.369351	38285.788039	46.605620
3077.850905	33358.111620	46.610625
3071.880607	28471.426879	46.615629
3065.271968	23648.233088	46.620634
3055.457039	18978.001331	46.625639
3038.133208	14607.646582	46.630644
3020.483123	10414.197073	46.635649
3002.977771	6470.621582	46.640653
2982.692511	2878.249185	46.645658
2931.360520	427.469635	46.650663
2822.023254	224.123608	46.655668
2750.558687	230.938846	46.660673
2730.665055	236.714133	46.665677
2746.470312	228.980804	46.670682
2778.708924	223.244395	46.675687
2810.279588	208.830110	46.680692
2831.755580	218.886135	46.685697
2842.134569	215.098369	46.690701
2842.528168	217.656190	46.695706
2838.253330	221.497194	46.700711
2832.331529	214.614881	46.705716
2826.849574	204.876714	46.710721
2822.351692	198.687621	46.715725
2818.894925	203.411702	46.720730
2815.940935	220.062598	46.725735
2813.900300	210.957441	46.730740
2811.419080	202.866519	46.735745
2808.956841	201.742059	46.740749
2806.222760	196.449815	46.745754
2803.270617	200.707744	46.750759
2799.952595	213.183421	46.755764
2796.304963	209.842905	46.760769
2793.589009	194.061104	46.765773
2790.667696	197.790597	46.770778
2787.207047	193.621107	46.775783
2784.615402	192.851781	46.780788
2780.977315	190.980268	46.785793
2777.351115	199.009028	46.790797
2774.336284	182.758910	46.795802
2771.009795	187.750165	46.800807
2767.737272	188.234560	46.805812
2764.555278	187.174208	46.810817
2761.241829	195.606864	46.815821
2758.135510	184.211822	46.820826
2754.555124	194.085426	46.825831
2751.458816	189.572874	46.830836
2747.528308	189.170629	46.835841
2744.230507	188.203266	46.840845
2741.335067	184.192259	46.845850
2737.406880	192.909622	46.850855
2734.391431	179.613797	46.855860
2731.166712	187.240062	46.860865
2727.663708	184.537347	46.865869
2724.144441	178.696101	46.870874
2720.082260	186.178020	46.875879
2717.485794	178.947305	46.880884
2714.490094	178.676487	46.885889
2711.051662	179.822239	46.890893
2706.952724	178.672968	46.895898
2703.086404	187.433789	46.900903
2700.095354	173.573718	46.905908
2697.214490	181.965980	46.910913
2693.301436	174.647360	46.915917
2689.475846	175.597919	46.920922
2685.872102	168.290267	46.925927
2683.337307	172.126337	46.930932
2679.749270	175.796558	46.935937
2676.505796	181.078430	46.940941
2672.907176	172.945265	46.945946
2668.999427	177.714707	46.950951
2666.073464	183.697066	46.955956
2662.462528	184.640924	46.960961
2659.029123	184.138508	46.965965
2655.608559	178.208363	46.970970
2652.143922	176.283187	46.975975
2648.500134	181.311468	46.980980
2644.646686	179.261617	46.985985
2641.620550	178.975563	46.990989
2638.630531	163.652517	46.995994
2634.713496	174.167826	47.000999
2631.398601	173.887947	47.006004
2627.790484	174.886226	47.011009
2624.318412	176.008805	47.016013
2621.063670	166.187566	47.021018
2617.255848	181.715147	47.026023
2613.720992	178.389085	47.031028
2610.512972	173.866330	47.036033
2606.838782	168.830522	47.041037
2603.422316	158.286197	47.046042
2599.846965	183.260133	47.051047
2596.785047	170.489744	47.056052
2593.137799	171.928674	47.061057
2589.645490	171.718063	47.066061
2586.466112	161.430503	47.071066
2582.462403	174.766542	47.076071
2579.149577	165.617222	47.081076
2575.595251	166.637029	47.086081
2572.272953	168.134657	47.091085
2569.080157	158.863256	47.096090
2565.230355	167.190656	47.101095
2561.584309	165.385383	47.106100
2558.172070	169.278790	47.111105
2555.090923	172.663109	47.116109
2551.455934	163.715949	47.121114
2547.830226	167.531437	47.126119
2544.454350	158.405221	47.131124
2541.307905	170.950896	47.136129
2537.170458	168.392666	47.141133
2534.175945	158.106710	47.146138
2530.460647	164.340022	47.151143
2527.321039	157.167217	47.156148
2523.114810	159.308139	47.161153
2519.591627	174.975334	47.166157
2516.337159	156.962671	47.171162
2512.864886	175.019877	47.176167
2509.339901	164.727250	47.181172
2506.270895	163.475519	47.186177
2502.741725	164.001034	47.191181
2499.458837	160.109818	47.196186
2495.798251	163.245968	47.201191
2492.316323	150.043801	47.206196
2488.383622	155.872292	47.211201
2484.865288	154.978358	47.216205
2481.312039	147.919083	47.221210
2477.746937	160.620943	47.226215
2474.831240	155.703767	47.231220
2471.328184	153.413523	47.236225
2467.855011	153.616423	47.241229
2464.283882	148.157766	47.246234
2460.401172	156.906288	47.251239
2457.269238	144.010093	47.256244
2453.609257	153.951934	47.261249
2449.968561	154.526944	47.266253
2446.876462	149.516457	47.271258
2443.263144	154.045125	47.276263
2439.770266	151.954901	47.281268
2436.470787	156.099682	47.286273
2432.763112	156.462018	47.291277
2429.292786	148.174844	47.296282
2425.691947	157.531480	47.301287
2422.400266	151.126133	47.306292
2418.758012	155.710131	47.311297
2414.857741	157.135662	47.316301
2411.865035	149.341485	47.321306
2408.352322	155.701186	47.326311
2405.063826	150.111118	47.331316
2401.731818	154.468909	47.336321
2397.716441	159.441509	47.341325
2394.223704	147.181738	47.346330
2390.501403	147.998830	47.351335
2387.360389	141.414642	47.356340
2383.725084	142.692124	47.361345
2380.235534	151.968397	47.366349
2377.241309	142.748152	47.371354
2373.344154	156.378291	47.376359
2370.275343	143.768315	47.381364
2366.547340	144.968219	47.386369
2362.612635	145.497276	47.391373
2359.430117	148.719728	47.396378
2355.517386	149.385656	47.401383
2352.578282	141.610872	47.406388
2349.389515	148.495752	47.411393
2345.616828	139.455181	47.416397
2341.858303	144.497768	47.421402
2337.854144	160.425097	47.426407
2334.748502	149.065852	47.431412
2331.078058	156.894270	47.436417
2327.242539	151.501628	47.441421
2324.444298	149.531281	47.446426
2321.208423	150.923421	47.451431
2317.754580	147.494418	47.456436
2314.267582	150.324116	47.461441
2310.419999	153.464160	47.466445
2306.886485	151.979105	47.471450
2303.356608	153.857647	47.476455
2300.052562	144.796724	47.481460
2296.510373	148.910767	47.486465
2292.326246	150.326395	47.491469
2289.646452	152.989061	47.496474
2285.825199	144.053682	47.501479
2282.482967	145.174961	47.506484
2278.772426	140.890237	47.511489
2275.305065	145.958061	47.516493
2272.112310	139.219539	47.521498
2268.277818	150.241638	47.526503
2265.292523	143.400279	47.531508
2261.672376	153.087025	47.536513
2257.616488	146.035045	47.541517
2254.572596	139.351010	47.546522
2250.900404	144.620716	47.551527
2247.370627	137.570404	47.556532
2243.899131	139.606270	47.561537
2240.425678	140.661701	47.566541
2236.802844	130.862922	47.571546
2233.280527	142.420408	47.576551
2229.968856	130.113254	47.581556
2226.432752	147.520107	47.586561
2223.162400	132.766441	47.591565
2219.164359	143.043490	47.596570
2215.322858	135.909671	47.601575
2212.765004	133.673831	47.606580
2209.291548	141.396691	47.611585
2205.592336	135.702955	47.616589
2202.361568	123.965953	47.621594
2198.209376	141.266491	47.626599
2194.857366	131.428611	47.631604
2191.360123	136.222021	47.636609
2188.029920	137.493725	47.641613
2184.310341	129.484092	47.646618
2180.851855	138.120725	47.651623
2177.327510	134.397655	47.656628
2173.744695	130.178702	47.661633
2169.962317	134.080833	47.666637
2167.062272	133.801073	47.671642
2163.645624	140.558857	47.676647
2160.238847	132.981886	47.681652
2156.854823	136.657206	47.686657
2153.177203	129.047363	47.691661
2149.437194	133.219750	47.696666
2145.927492	141.283345	47.701671
2142.067630	126.201576	47.706676
2139.337150	127.915253	47.711681
2135.118556	130.251597	47.716685
2131.858935	121.929409	47.721690
2127.935861	131.412263	47.726695
2125.052137	129.152718	47.731700
2121.388374	132.789359	47.736705
2117.990523	137.287327	47.741709
2114.778022	126.814273	47.746714
2110.845891	128.071902	47.751719
2107.772585	136.495388	47.756724
2103.720226	128.219905	47.761729
2100.218228	138.385464	47.766733
2096.769228	134.968287	47.771738
2093.483310	135.754189	47.776743
2089.803160	127.974920	47.781748
2086.539475	123.875053	47.786753
2082.798182	130.017122	47.791757
2079.249796	129.395906	47.796762
2075.730108	129.774377	47.801767
2072.389573	126.760170	47.806772
2068.941186	127.807840	47.811777
2065.387725	128.464437	47.816781
2062.062685	122.052705	47.821786
2058.479868	124.994191	47.826791
2055.145536	126.227809	47.831796
2051.182309	124.340179	47.836801
2048.004676	127.547443	47.841805
2044.470191	120.082322	47.846810
2040.430115	130.018577	47.851815
2037.418932	125.902171	47.856820
2033.765947	126.211793	47.861825
2030.484142	129.101453	47.866829
2027.225274	122.899210	47.871834
2023.340982	126.373758	47.876839
2019.886058	123.548653	47.881844
2016.517179	130.652847	47.886849
2012.573590	122.454755	47.891853
2009.459629	117.963494	47.896858
2006.285940	120.651536	47.901863
2002.608226	125.192215	47.906868
1998.995350	122.382054	47.911873
1994.955305	129.923676	47.916877
1991.755055	112.321735	47.921882
1988.368374	119.980053	47.926887
1985.042980	122.301736	47.931892
1981.638248	120.617631	47.936897
1977.675488	128.043057	47.941901
1974.312823	123.967382	47.946906
1970.810724	127.844750	47.951911
1967.421936	122.064484	47.956916
1963.798983	125.563267	47.961921
1960.343154	120.632793	47.966925
1957.238926	111.833115	47.971930
1953.560540	127.290353	47.976935
1949.766177	121.471936	47.981940
1946.497160	118.154323	47.986945
1942.913298	133.365027	47.991949
1939.424462	116.374548	47.996954
1935.991816	122.673778	48.001959
1932.530237	122.388970	48.006964
1928.719066	120.566445	48.011969
1924.954219	126.668938	48.016973
1921.916209	118.170300	48.021978
1918.044048	126.380565	48.026983
1914.936259	115.733463	48.031988
1911.250226	120.377620	48.036993
1907.804907	117.467352	48.041997
1904.462351	118.960174	48.047002
1900.942226	124.794404	48.052007
1897.415371	124.030460	48.057012
1893.460892	126.719721	48.062017
1889.627642	132.192243	48.067021
1886.802753	113.198940	48.072026
1883.594152	119.332810	48.077031
1879.974587	123.196765	48.082036
1876.416472	122.361454	48.087041
1872.757481	119.417760	48.092045
1869.580289	124.219355	48.097050
1865.818251	127.507037	48.102055
1862.480996	124.308153	48.107060
1859.270704	125.543274	48.112065
1855.635194	123.722094	48.117069
1851.674588	119.782137	48.122074
1848.015418	124.437486	48.127079
1844.617130	117.572969	48.132084
1841.216807	124.395380	48.137089
1837.521391	121.513207	48.142093
1834.438048	113.513326	48.147098
1830.737360	117.012476	48.152103
1827.220011	121.094559	48.157108
1824.065684	115.136440	48.162113
1820.144624	122.705265	48.167117
1817.037161	124.761655	48.172122
1813.360012	119.360255	48.177127
1810.002913	111.635075	48.182132
1806.302204	118.922691	48.187137
1802.780182	111.525593	48.192141
1799.207872	116.075613	48.197146
1795.700549	113.025945	48.202151
1792.126582	118.602586	48.207156
1788.877612	102.180312	48.212161
1785.185185	119.239197	48.217165
1781.927369	112.297188	48.222170
1778.289451	114.953422	48.227175
1774.759582	114.745781	48.232180
1770.900113	118.570266	48.237185
1767.830472	120.508731	48.242189
1764.333767	101.522329	48.247194
1760.616693	111.366799	48.252199
1757.308431	112.190416	48.257204
1754.064786	114.083142	48.262209
1750.335598	114.301655	48.267213
1747.110397	105.609634	48.272218
1743.096589	110.421340	48.277223
1739.407959	106.605928	48.282228
1736.497217	104.954403	48.287233
1732.584945	116.355669	48.292237
1729.215076	110.130059	48.297242
1725.350892	110.835105	48.302247
1722.076552	99.039679	48.307252
1718.527262	108.795785	48.312257
1714.832582	110.430803	48.317261
1712.046475	112.572724	48.322266
1708.481969	115.977772	48.327271
1704.735983	115.542381	48.332276
1701.425843	116.200594	48.337281
1697.643834	119.308213	48.342285
1694.354868	112.702573	48.347290
1690.470498	113.163936	48.352295
1686.657577	122.432160	48.357300
1683.554135	112.463772	48.362305
1680.103536	116.269692	48.367309
1676.996437	112.255314	48.372314
1673.154481	125.249706	48.377319
1669.558282	109.256888	48.382324
1666.218503	110.791869	48.387329
1662.767016	119.020817	48.392333
1659.456097	118.517482	48.397338
1655.546270	113.076274	48.402343
1652.079671	117.396953	48.407348
1648.663495	115.881780	48.412353
1644.900702	119.019611	48.417357
1641.538166	103.836037	48.422362
1638.257859	113.817961	48.427367
1634.851867	113.099923	48.432372
1630.992509	106.724677	48.437377
1627.222704	108.111945	48.442381
1624.398319	115.832216	48.447386
1620.741305	120.628496	48.452391
1616.901966	109.068129	48.457396
1613.570243	113.445213	48.462401
1610.463015	113.294726	48.467405
1606.634887	100.910619	48.472410
1603.081621	106.541405	48.477415
1599.366785	112.079597	48.482420
1596.066406	118.913842	48.487425
1592.315805	111.198064	48.492429
1589.219976	110.440083	48.497434
1585.598665	109.339440	48.502439
1582.013692	104.599845	48.507444
1578.692192	107.309756	48.512449
1575.006071	113.432647	48.517453
1571.824451	112.031583	48.522458
1568.019329	117.055720	48.527463
1564.508939	112.955766	48.532468
1561.483403	100.684704	48.537473
1557.766363	114.323289	48.542477
1554.299955	108.714928	48.547482
1550.648908	107.145842	48.552487
1546.775853	106.740352	48.557492
1543.370294	108.388560	48.562497
1539.834821	111.938912	48.567501
1536.575546	107.707558	48.572506
1533.137061	113.637474	48.577511
1529.475461	117.353988	48.582516
1526.178082	110.268398	48.587521
1522.752073	116.516726	48.592525
1518.924321	105.789864	48.597530
1515.357129	109.414958	48.602535
1512.270970	115.615226	48.607540
1508.524287	110.489690	48.612545
1504.847864	115.043606	48.617549
1501.676873	98.773661	48.622554
1497.972705	109.107567	48.627559
1494.343799	104.224774	48.632564
1491.007294	98.710177	48.637569
1487.378585	103.885887	48.642573
1483.943986	101.649697	48.647578
1480.521663	101.038102	48.652583
1476.974609	106.861152	48.657588
1473.472304	110.995300	48.662593
1469.718240	109.749242	48.667597
1466.791672	112.224239	48.672602
1463.381716	117.437696	48.677607
1459.457811	112.895122	48.682612
1455.768670	105.643095	48.687617
1452.138354	117.872427	48.692621
1448.812516	101.733784	48.697626
1445.701297	114.235193	48.702631
1442.149251	101.782983	48.707636
1438.396136	108.220797	48.712641
1434.893057	103.805202	48.717645
1431.541703	102.107592	48.722650
1428.090477	108.094168	48.727655
1424.557771	102.279858	48.732660
1420.944810	109.609878	48.737665
1417.414789	111.609566	48.742669
1414.027359	108.899708	48.747674
1410.189893	104.824545	48.752679
1406.884062	106.709507	48.757684
1403.822522	105.469423	48.762689
1399.767662	108.211717	48.767693
1396.462716	108.242389	48.772698
1392.835823	113.644816	48.777703
1389.340488	106.089179	48.782708
1386.206083	106.043029	48.787713
1382.763518	101.680792	48.792717
1379.165155	102.089494	48.797722
1375.052623	106.011372	48.802727
1371.601480	100.168193	48.807732
1368.828820	96.816505	48.812737
1364.905257	105.197189	48.817741
1361.529038	108.811065	48.822746
1357.506563	111.078966	48.827751
1354.165086	107.875308	48.832756
1351.201824	100.676250	48.837761
1347.338172	98.263694	48.842765
1343.662447	102.989116	48.847770
1340.424453	105.305895	48.852775
1336.536396	108.373023	48.857780
1333.305400	101.649564	48.862785
1329.699046	102.969149	48.867789
1326.629789	101.432236	48.872794
1323.125504	100.799445	48.877799
1319.234440	113.657620	48.882804
1315.847373	96.813741	48.887809
1312.209601	111.206998	48.892813
1308.832955	104.915016	48.897818
1304.900092	111.530174	48.902823
1301.743228	107.552187	48.907828
1298.349833	101.767381	48.912833
1294.566669	108.528409	48.917837
1291.478461	94.728588	48.922842
1287.760783	107.267943	48.927847
1284.296904	99.242078	48.932852
1281.036897	100.763945	48.937857
1277.328132	112.993599	48.942861
1273.943713	105.573004	48.947866
1270.700390	104.133682	48.952871
1266.680938	105.168428	48.957876
1263.576430	105.302713	48.962881
1259.828216	105.012167	48.967885
1256.039742	94.287767	48.972890
1252.876881	97.172312	48.977895
1248.759100	96.657741	48.982900
1246.053133	91.869937	48.987905
1242.022058	106.937857	48.992909
1238.782178	95.941116	48.997914
1235.109968	99.216239	49.002919
1231.592460	99.484777	49.007924
1228.628137	92.005392	49.012929
1224.862630	98.295671	49.017933
1221.372808	94.622818	49.022938
1217.996907	96.972242	49.027943
1214.090304	98.432715	49.032948
1210.601521	98.650527	49.037953
1206.799893	107.601747	49.042957
1203.919243	102.333830	49.047962
1200.147181	106.168022	49.052967
1196.617380	102.000792	49.057972
1193.463177	95.783116	49.062977
1189.784192	103.108691	49.067981
1186.570017	97.529280	49.072986
1182.562494	102.181429	49.077991
1179.079524	95.095974	49.082996
1175.895666	104.870811	49.088001
1172.260346	107.744612	49.093005
1169.116541	104.832345	49.098010
1164.988340	109.473158	49.103015
1161.395994	105.510909	49.108020
1157.882857	106.033546	49.113025
1154.306592	104.119327	49.118029
1150.995388	104.711080	49.123034
1148.194751	107.423918	49.128039
1144.965536	112.519830	49.133044
1140.932626	107.168850	49.138049
1136.621504	110.761417	49.143053
1133.513094	111.180021	49.148058
1130.333249	104.546330	49.153063
1126.496507	104.313424	49.158068
1123.248692	97.218604	49.163073
1119.599987	111.488715	49.168077
1115.932309	107.702993	49.173082
1112.672672	110.300406	49.178087
1108.921047	109.892171	49.183092
1105.982095	107.336291	49.188097
1102.019397	107.886016	49.193101
1098.342156	102.275380	49.198106
1095.261669	106.068718	49.203111
1091.860286	105.208112	49.208116
1088.463106	102.737754	49.213121
1084.704048	106.179570	49.218125
1081.040566	96.332485	49.223130
1077.871270	106.635014	49.228135
1074.302688	110.633879	49.233140
1070.751672	105.798565	49.238145
1066.786256	114.557458	49.243149
1063.578455	107.049935	49.248154
1059.736684	115.513037	49.253159
1056.242890	107.619832	49.258164
1053.506682	93.609286	49.263169
1049.887981	109.247713	49.268173
1046.236044	101.637692	49.273178
1042.348380	109.543260	49.278183
1038.773068	102.185154	49.283188
1035.403219	94.865579	49.288193
1032.000715	110.784865	49.293197
1028.635085	99.999023	49.298202
1025.271850	102.866679	49.303207
1021.449162	104.716372	49.308212
1018.447830	98.042503	49.313217
1014.644992	106.812348	49.318221
1011.148134	103.155263	49.323226
1007.384488	107.378169	49.328231
1004.034345	106.116838	49.333236
1000.870947	103.958818	49.338241
996.644206	109.001547	49.343245
993.262034	104.399952	49.348250
989.773909	105.495987	49.353255
986.272921	102.424112	49.358260
983.635858	96.385025	49.363265
979.806178	110.200432	49.368269
976.127028	102.043058	49.373274
972.244367	101.823254	49.378279
968.727277	105.859446	49.383284
965.632774	94.672092	49.388289
962.193029	108.377411	49.393293
958.843892	94.699353	49.398298
954.863948	96.061353	49.403303
951.106187	103.146243	49.408308
948.112015	101.894160	49.413313
944.461857	101.219027	49.418317
940.802397	97.739760	49.423322
937.721056	102.830232	49.428327
934.017370	107.827851	49.433332
930.594257	105.295241	49.438337
926.760079	108.899647	49.443341
923.630711	103.193715	49.448346
920.262183	103.325920	49.453351
916.127856	98.715841	49.458356
912.966562	96.094407	49.463361
909.060229	107.862635	49.468365
906.076237	105.596181	49.473370
902.535391	102.383396	49.478375
898.738369	105.020253	49.483380
895.906579	88.723033	49.488385
892.105921	107.198053	49.493389
888.483750	107.767053	49.498394
884.744099	104.331539	49.503399
880.874610	105.514652	49.508404
877.922310	108.105643	49.513409
874.387685	101.947247	49.518413
871.007166	96.493607	49.523418
867.326683	95.588559	49.528423
863.851720	101.077127	49.533428
860.637212	93.238405	49.538433
857.218468	93.643032	49.543437
853.344933	106.534609	49.548442
849.690555	103.858127	49.553447
846.522708	97.907645	49.558452
843.381669	96.503609	49.563457
839.354509	106.007827	49.568461
835.768233	102.937031	49.573466
832.177258	100.518809	49.578471
828.414189	107.285013	49.583476
825.341564	98.477938	49.588481
821.700962	105.172511	49.593485
818.630360	99.896970	49.598490
815.137866	99.091598	49.603495
811.249315	98.614823	49.608500
807.896451	96.580180	49.613505
804.194271	100.735449	49.618509
800.962432	97.249072	49.623514
797.508955	94.316503	49.628519
793.850425	101.149643	49.633524
790.569078	95.184311	49.638529
786.644544	111.570300	49.643533
783.278783	100.127803	49.648538
779.878212	95.341406	49.653543
776.372179	94.097870	49.658548
773.046683	96.354847	49.663553
769.016673	100.610552	49.668557
766.009632	94.245096	49.673562
762.779856	103.939646	49.678567
758.646355	100.368368	49.683572
755.145841	90.449191	49.688577
751.433939	96.283450	49.693581
748.152293	94.550599	49.698586
744.756649	104.345516	49.703591
741.306356	105.334853	49.708596
738.149226	90.946718	49.713601
734.407189	98.740773	49.718605
730.608010	86.946031	49.723610
727.388006	91.327971	49.728615
723.680431	100.161191	49.733620
720.406961	91.644290	49.738625
716.697019	106.854716	49.743629
712.955729	100.911748	49.748634
709.768307	102.748031	49.753639
705.664246	93.831119	49.758644
703.062515	89.579542	49.763649
699.293622	103.947093	49.768653
696.059788	92.333799	49.773658
692.664569	95.813450	49.778663
688.492086	102.548302	49.783668
685.557854	95.365709	49.788673
681.680168	102.372681	49.793677
677.967159	95.114374	49.798682
674.701167	90.681848	49.803687
671.031234	93.225007	49.808692
668.091770	92.015963	49.813697
664.375643	95.372310	49.818701
661.016399	93.198556	49.823706
657.468278	93.982608	49.828711
653.620894	91.123673	49.833716
650.073624	85.237756	49.838721
646.628296	100.788106	49.843725
643.108954	97.511421	49.848730
639.517237	100.331899	49.853735
636.157003	99.107895	49.858740
632.998910	90.372022	49.863745
629.314693	101.958181	49.868749
625.732879	84.600974	49.873754
621.648177	88.307852	49.878759
618.265059	95.368323	49.883764
615.230317	90.883441	49.888769
612.069382	88.635560	49.893773
608.596245	89.951251	49.898778
604.858809	87.480615	49.903783
601.231696	92.751162	49.908788
597.354117	84.194399	49.913793
594.134647	100.008213	49.918797
590.308702	89.390623	49.923802
587.087737	91.329072	49.928807
583.751606	103.506492	49.933812
580.625159	85.598143	49.938817
576.504613	91.252178	49.943821
573.336051	90.263985	49.948826
569.514157	88.622984	49.953831
565.822791	98.675730	49.958836
562.693403	89.239757	49.963841
558.912127	95.763155	49.968845
555.709589	98.537036	49.973850
552.470648	98.742765	49.978855
548.576840	95.300442	49.983860
545.030932	95.108620	49.988865
540.904310	95.403568	49.993869
537.933949	94.240606	49.998874
534.632809	91.030599	50.003879
531.024152	90.750744	50.008884
527.744369	93.813939	50.013889
523.854414	101.233351	50.018893
520.572004	90.549644	50.023898
517.213766	95.098764	50.028903
513.576532	95.919852	50.033908
510.247226	88.060467	50.038913
506.623104	89.572216	50.043917
503.130514	89.479126	50.048922
499.546408	99.431631	50.053927
495.827637	106.526643	50.058932
492.264013	92.879364	50.063937
488.965165	96.171111	50.068941
486.009918	99.723497	50.073946
482.492251	93.596622	50.078951
478.229979	91.826396	50.083956
475.246079	94.568962	50.088961
471.424462	95.810051	50.093965
467.772280	104.740070	50.098970
464.621799	97.799402	50.103975
461.327800	94.068108	50.108980
457.807322	94.887419	50.113985
453.658848	102.172635	50.118989
450.227661	112.631797	50.123994
447.234720	97.000515	50.128999
443.415354	100.257400	50.134004
439.989766	90.379582	50.139009
436.612210	93.134877	50.144013
432.880813	92.776838	50.149018
429.515276	84.894544	50.154023
425.756335	101.860125	50.159028
422.774569	83.387613	50.164033
419.142691	89.366946	50.169037
415.673897	88.242281	50.174042
412.014823	93.569221	50.179047
408.414270	99.797923	50.184052
404.995558	86.485621	50.189057
401.573130	83.387645	50.194061
397.565619	89.722039	50.199066
394.613712	80.519001	50.204071
391.008183	89.079621	50.209076
387.623399	85.369990	50.214081
383.951224	94.816067	50.219085
380.141803	90.261954	50.224090
376.892538	96.249598	50.229095
373.060795	91.840292	50.234100
369.911966	92.558283	50.239105
366.285123	97.247070	50.244109
362.777409	102.804262	50.249114
359.695316	92.119009	50.254119
356.064736	96.879071	50.259124
352.769272	85.257022	50.264129
349.057502	96.162464	50.269133
345.224776	89.550143	50.274138
341.887284	84.500710	50.279143
337.975149	91.601543	50.284148
334.927456	89.614709	50.289153
331.427136	97.899994	50.294157
327.817348	88.700734	50.299162
324.549443	92.609863	50.304167
321.076606	95.562043	50.309172
317.504356	96.191965	50.314177
313.694160	91.542938	50.319181
310.212034	91.632203	50.324186
306.813752	91.289988	50.329191
303.422689	93.707642	50.334196
300.089947	83.502170	50.339201
296.371447	88.587689	50.344205
292.826517	92.104005	50.349210
289.364009	93.337712	50.354215
285.791784	95.415680	50.359220
282.429786	89.926970	50.364225
278.547075	86.968928	50.369229
274.897579	93.905419	50.374234
271.986843	90.137856	50.379239
268.248257	96.367515	50.384244
265.359906	91.153151	50.389249
261.859351	94.601740	50.394253
257.770992	90.586446	50.399258
254.172817	93.819199	50.404263
250.612542	87.224665	50.409268
247.254807	90.557974	50.414273
243.603220	85.852676	50.419277
240.065074	91.944668	50.424282
236.820002	91.143721	50.429287
233.307213	89.721660	50.434292
229.891724	91.243409	50.439297
226.360587	98.656569	50.444301
222.732354	94.412126	50.449306
219.457385	89.221984	50.454311
215.766474	90.659468	50.459316
212.195891	91.153846	50.464321
208.928318	97.441060	50.469325
205.121310	94.206684	50.474330
201.794072	83.700059	50.479335
198.334940	99.889237	50.484340
194.754783	102.020509	50.489345
191.407864	97.990815	50.494349
187.972419	98.424873	50.499354
184.595225	84.537595	50.504359
180.417393	95.539576	50.509364
176.984503	90.842404	50.514369
173.587026	99.391144	50.519373
170.295651	85.981764	50.524378
166.925109	95.466907	50.529383
163.207667	98.568410	50.534388
159.724666	84.682165	50.539393
156.121436	90.414065	50.544397
152.190143	80.123116	50.549402
149.212122	87.226963	50.554407
145.686325	89.730096	50.559412
142.400104	88.189764	50.564417
138.611829	81.843395	50.569421
135.287259	85.573846	50.574426
132.081355	87.577269	50.579431
128.550614	86.930057	50.584436
124.939728	81.623365	50.589441
121.037930	89.404668	50.594445
117.245278	92.014335	50.599450
114.012912	80.317717	50.604455
110.612114	90.377823	50.609460
107.227737	74.703813	50.614465
103.937504	81.013225	50.619469
99.960705	77.622680	50.624474
96.413771	81.124709	50.629479
92.934622	85.851953	50.634484
89.751026	86.576946	50.639489
86.242286	81.406446	50.644493
82.421410	80.689101	50.649498
79.413446	70.178091	50.654503
75.789801	88.032736	50.659508
72.364960	83.625396	50.664513
68.529919	83.125313	50.669517
65.223909	83.501071	50.674522
61.759330	80.540666	50.679527
57.881510	94.762684	50.684532
54.699577	85.028487	50.689537
51.260394	83.199511	50.694541
47.525385	89.944606	50.699546
44.299964	82.527212	50.704551
39.997137	88.573421	50.709556
36.802057	79.790592	50.714561
33.945721	91.771463	50.719565
30.449499	87.596841	50.724570
26.959227	84.415783	50.729575
23.017542	88.368488	50.734580
19.673713	83.218399	50.739585
16.002941	92.676410	50.744589
12.750145	90.297312	50.749594
9.290043	81.551851	50.754599
5.500867	84.615308	50.759604
1.873894	83.413929	50.764609