Fri Jun 17 17:39:01 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.350991	110.847081	0.000000
0.307856	117.391762	0.005005
0.335037	117.293840	0.010010
0.301074	114.730365	0.015014
0.283834	105.977785	0.020019
0.219734	103.116616	0.025024
0.104440	90.693808	0.030029
-0.000933	80.155052	0.035034
-0.664545	77.013879	0.040038
-0.516307	60.732495	0.045043
-1.211924	64.916813	0.050048
-1.610523	55.040514	0.055053
-1.423900	56.236820	0.060058
-1.880263	42.285000	0.065062
-2.267256	32.697650	0.070067
-2.904537	35.314541	0.075072
-2.593287	20.340449	0.080077
-2.918261	20.829908	0.085082
-3.524842	17.466349	0.090086
-3.466328	12.020515	0.095091
-4.132883	8.253916	0.100096
-4.254007	8.499728	0.105101
-4.448451	8.773318	0.110106
-4.843870	5.897387	0.115110
-4.743419	5.207333	0.120115
-5.449168	10.089896	0.125120
-6.072386	10.566378	0.130125
-6.255455	6.372900	0.135130
-6.445004	9.765261	0.140134
-6.388020	6.635742	0.145139
-6.315668	14.050942	0.150144
-6.393945	6.185498	0.155149
-6.764653	3.535744	0.160154
-7.708008	12.918441	0.165158
-7.636628	1.379694	0.170163
-8.248901	13.050053	0.175168
-8.239474	5.701243	0.180173
-7.833151	9.104860	0.185178
-8.090036	5.698172	0.190182
-8.824768	3.772154	0.195187
-9.814256	8.711354	0.200192
-9.698946	9.119535	0.205197
-9.313468	1.655332	0.210202
-9.570190	12.364990	0.215206
-9.635397	15.656369	0.220211
-10.487127	14.528857	0.225216
-10.909337	12.694939	0.230221
-10.889726	11.936234	0.235226
-11.092384	17.008078	0.240230
-10.809228	2.452671	0.245235
-11.563624	8.000033	0.250240
-12.173448	9.598280	0.255245
-12.390546	8.467294	0.260250
-12.645246	9.098792	0.265254
-12.836910	8.047048	0.270259
-12.847844	7.933756	0.275264
-12.785346	13.680591	0.280269
-12.495268	11.291383	0.285274
-13.566087	12.478856	0.290278
-13.975625	13.796359	0.295283
-14.130827	14.943319	0.300288
-14.272099	14.452494	0.305293
-14.436408	8.337656	0.310298
-15.339188	19.175431	0.315302
-15.134669	2.807401	0.320307
-15.531215	9.974949	0.325312
-15.429052	10.511015	0.330317
-15.238287	9.238428	0.335322
-16.099431	10.611466	0.340326
-16.301644	9.272979	0.345331
-16.822542	13.702334	0.350336
-16.977726	5.253740	0.355341
-16.818938	6.156701	0.360346
-17.239235	9.106724	0.365350
-17.763446	7.710864	0.370355
-18.168197	3.068019	0.375360
-18.525778	8.330186	0.380365
-18.494678	8.034283	0.385370
-18.893570	6.642850	0.390374
-18.558493	1.476839	0.395379
-18.540219	2.424271	0.400384
-19.228392	3.421255	0.405389
-19.516090	-4.652085	0.410394
-19.688455	6.233771	0.415398
-20.145667	0.985754	0.420403
-20.290700	6.839110	0.425408
-21.068273	1.295469	0.430413
-21.254246	8.868452	0.435418
-21.666541	17.263447	0.440422
-21.670079	9.454052	0.445427
-21.764558	13.384515	0.450432
-22.102266	27.801066	0.455437
-21.532715	0.516061	0.460442
-21.751863	6.976488	0.465446
-22.421578	12.257787	0.470451
-23.027375	9.729597	0.475456
-23.344829	11.650027	0.480461
-23.287461	10.164595	0.485466
-23.555671	13.101966	0.490470
-23.629596	2.485027	0.495475
-24.240180	11.045586	0.500480
-24.802867	4.478588	0.505485
-24.873114	4.564790	0.510490
-25.382489	16.465301	0.515494
-25.396941	11.791120	0.520499
-25.654999	10.202232	0.525504
-25.623365	18.987156	0.530509
-25.323251	12.527142	0.535514
-25.759386	15.893402	0.540518
-26.468618	9.912562	0.545523
-26.973353	8.408684	0.550528
-27.119002	8.184983	0.555533
-26.986667	11.178904	0.560538
-26.990042	19.716475	0.565542
-27.423539	6.968156	0.570547
-28.061804	11.539760	0.575552
-28.448820	13.248772	0.580557
-28.265729	12.412572	0.585562
-28.506358	16.651485	0.590566
-28.537152	1.956662	0.595571
-29.468745	2.318259	0.600576
-29.780652	6.701031	0.605581
-29.938867	9.246770	0.610586
-29.897604	11.098689	0.615590
-29.812286	0.128898	0.620595
-30.046269	10.894761	0.625600
-30.539268	12.685128	0.630605
-30.886001	2.509975	0.635610
-31.472629	12.147129	0.640614
-31.497197	3.974991	0.645619
-31.739623	12.538877	0.650624
-31.746873	10.354589	0.655629
-31.751129	2.997401	0.660634
-32.620726	-0.564155	0.665638
-33.045372	3.292926	0.670643
-33.074389	7.924075	0.675648
-33.238451	2.420330	0.680653
-32.914668	-6.416696	0.685658
-33.212919	-0.696724	0.690662
-33.799441	0.495100	0.695667
-34.433623	-1.401057	0.700672
-35.050189	8.943170	0.705677
-34.744257	-2.527609	0.710682
-34.937920	6.188399	0.715686
-35.037528	-2.839512	0.720691
-35.145958	10.434849	0.725696
-35.489721	-1.035868	0.730701
-35.812747	-0.847066	0.735706
-36.401629	-1.170736	0.740710
-36.268969	6.745121	0.745715
-36.368530	5.624592	0.750720
-36.821251	11.191467	0.755725
-37.174959	-8.498935	0.760730
-37.633656	4.211468	0.765734
-37.916160	3.314733	0.770739
-37.963593	-6.587138	0.775744
-37.856598	13.408370	0.780749
-38.227362	2.973186	0.785754
-39.164727	8.970885	0.790758
-39.511074	-0.486048	0.795763
-39.048159	1.932164	0.800768
-39.469910	7.490140	0.805773
-39.421621	-3.539795	0.810778
-39.762723	11.602687	0.815782
-39.759091	4.099347	0.820787
-40.543093	-4.327781	0.825792
-40.766423	0.848921	0.830797
-40.923411	-2.597850	0.835802
-41.122413	3.688932	0.840806
-40.946491	0.292389	0.845811
-41.532064	2.961462	0.850816
-41.955912	9.152426	0.855821
-42.331160	-2.771649	0.860826
-42.516999	5.271151	0.865830
-42.392093	0.677406	0.870835
-43.039017	-1.327728	0.875840
-43.528822	7.807701	0.880845
-43.359123	3.626820	0.885850
-43.956870	4.969298	0.890854
-43.718128	3.066160	0.895859
-43.908061	1.041099	0.900864
-44.335946	6.977389	0.905869
-44.893687	7.377283	0.910874
-45.502617	8.762072	0.915878
-45.590546	8.851016	0.920883
-45.548861	10.058978	0.925888
-45.573878	5.441808	0.930893
-45.658073	4.340037	0.935898
-46.048549	5.610566	0.940902
-45.990946	-0.072104	0.945907
-46.677731	6.970832	0.950912
-47.129121	6.414349	0.955917
-46.985232	-4.292071	0.960922
-47.527368	1.192974	0.965926
-47.526415	-3.847243	0.970931
-48.460802	-3.238515	0.975936
-48.539419	6.672536	0.980941
-48.605282	12.256203	0.985946
-49.106310	14.490912	0.990950
-48.824257	8.532751	0.995955
-48.755370	3.300090	1.000960
-48.704985	6.958425	1.005965
-49.293524	-4.024448	1.010970
-50.122685	0.203570	1.015974
-50.149475	3.379634	1.020979
-50.179692	-5.162736	1.025984
-50.839330	2.251400	1.030989
-51.415361	-3.743481	1.035994
-51.839535	11.276060	1.040998
-52.014809	4.921519	1.046003
-51.777788	5.288548	1.051008
-52.077568	7.951750	1.056013
-51.614451	6.819179	1.061018
-52.101064	5.732013	1.066022
-52.278394	-6.120572	1.071027
-52.709007	7.490118	1.076032
-53.227386	8.594842	1.081037
-53.226353	4.391681	1.086042
-53.317478	7.094786	1.091046
-54.033297	-3.083726	1.096051
-54.203819	7.294093	1.101056
-55.013735	8.881802	1.106061
-54.931732	-3.464794	1.111066
-54.953652	8.605681	1.116070
-54.888420	3.803213	1.121075
-55.053957	-2.941485	1.126080
-56.063220	0.787631	1.131085
-56.393412	-6.611861	1.136090
-56.677841	8.538560	1.141094
-56.843527	-0.849146	1.146099
-56.483977	2.414241	1.151104
-57.062845	4.257759	1.156109
-56.727034	-4.368942	1.161114
-57.101769	2.444324	1.166118
-57.955486	10.756216	1.171123
-57.978417	-0.208601	1.176128
-58.448315	0.206290	1.181133
-58.644116	-0.877716	1.186138
-58.497773	2.868263	1.191142
-59.272154	9.030281	1.196147
-59.403363	5.793524	1.201152
-59.932869	10.388096	1.206157
-60.053878	-1.604091	1.211162
-60.168178	12.610533	1.216166
-60.291753	-4.106480	1.221171
-60.312948	1.123050	1.226176
-60.547745	10.633045	1.231181
-60.461263	10.320634	1.236186
-61.096749	9.277161	1.241190
-61.803808	6.294788	1.246195
-61.947624	1.742755	1.251200
-61.787631	5.859814	1.256205
-61.923895	0.076177	1.261210
-62.343426	7.461845	1.266214
-63.294702	7.623671	1.271219
-63.301106	2.566126	1.276224
-63.540269	7.530177	1.281229
-63.591890	0.477058	1.286234
-63.380274	3.261650	1.291238
-63.665527	-0.422101	1.296243
-63.352639	6.840624	1.301248
-64.743064	12.950746	1.306253
-64.744251	2.859641	1.311258
-65.352178	12.406606	1.316262
-65.097144	1.723541	1.321267
-65.105962	7.021856	1.326272
-65.894849	1.074399	1.331277
-66.434691	-3.842762	1.336282
-66.695474	4.536313	1.341286
-66.825467	-1.171999	1.346291
-66.974746	0.646870	1.351296
-66.772451	4.148331	1.356301
-66.632515	-0.275052	1.361306
-67.093760	0.145703	1.366310
-67.615868	1.544083	1.371315
-67.887575	3.187554	1.376320
-68.178805	2.830391	1.381325
-67.828021	6.258229	1.386330
-69.018503	2.024644	1.391334
-69.440574	10.414947	1.396339
-69.774865	0.971800	1.401344
-69.959728	5.347859	1.406349
-69.653397	-3.950189	1.411354
-69.932533	4.807060	1.416358
-69.968051	10.365159	1.421363
-70.038673	4.668287	1.426368
-70.947163	8.020924	1.431373
-70.602901	3.457408	1.436378
-71.497645	12.146511	1.441382
-71.249834	-1.962768	1.446387
-71.278518	6.002402	1.451392
-72.613467	11.101461	1.456397
-72.396161	9.393690	1.461402
-72.733312	4.932208	1.466406
-73.003319	-0.132818	1.471411
-72.535610	0.303009	1.476416
-72.899976	4.217756	1.481421
-73.173878	-4.196486	1.486426
-74.203739	0.281766	1.491430
-74.091955	5.647251	1.496435
-74.324743	1.932677	1.501440
-74.450450	3.138867	1.506445
-74.442072	-6.451421	1.511450
-74.889104	5.326636	1.516454
-75.755870	2.922747	1.521459
-75.943543	0.400635	1.526464
-76.142917	7.950783	1.531469
-75.788432	3.194158	1.536474
-76.094477	5.843602	1.541478
-76.118071	1.631908	1.546483
-76.972708	-4.147144	1.551488
-77.650653	4.687259	1.556493
-77.370977	5.129679	1.561498
-77.585917	3.409311	1.566502
-77.893866	0.973891	1.571507
-77.735540	-0.701381	1.576512
-77.855167	4.056517	1.581517
-77.938887	-2.206484	1.586522
-78.735130	16.482098	1.591526
-79.040064	3.740049	1.596531
-79.248752	3.716069	1.601536
-79.286247	13.548260	1.606541
-80.147743	3.193878	1.611546
-80.288502	13.494331	1.616550
-80.788865	2.106092	1.621555
-80.621203	-1.916190	1.626560
-80.732252	-6.006193	1.631565
-80.508456	4.448145	1.636570
-80.488894	-5.178929	1.641574
-81.747758	6.608592	1.646579
-82.091795	-5.573637	1.651584
-82.347076	4.075521	1.656589
-82.501492	2.215840	1.661594
-82.257899	2.448183	1.666598
-82.324863	-3.677893	1.671603
-82.978480	-2.644019	1.676608
-83.530411	-0.961656	1.681613
-83.455316	-7.007750	1.686618
-83.903337	-1.032988	1.691622
-84.159337	-4.644641	1.696627
-84.088680	7.198506	1.701632
-84.660677	1.327869	1.706637
-85.294735	-6.842978	1.711642
-85.518364	-7.821718	1.716646
-85.679366	-2.250853	1.721651
-85.864832	-12.884354	1.726656
-85.965456	-3.736673	1.731661
-85.748534	-0.422545	1.736666
-85.718369	-7.614164	1.741670
-86.164667	-13.810567	1.746675
-86.505457	-17.819946	1.751680
-87.205999	-3.717046	1.756685
-87.307991	-6.211370	1.761690
-87.652182	-1.555257	1.766694
-87.478835	-6.863887	1.771699
-87.931952	-10.377648	1.776704
-88.650579	4.659660	1.781709
-88.825760	-7.836174	1.786714
-89.071678	-10.763386	1.791718
-89.352293	-0.991030	1.796723
-89.298604	-9.377048	1.801728
-89.166661	-10.648736	1.806733
-89.501921	-6.121189	1.811738
-90.198192	-8.358653	1.816742
-90.665611	-7.415722	1.821747
-90.565011	-13.832099	1.826752
-90.930771	-6.788269	1.831757
-90.897087	-14.528651	1.836762
-90.687657	-4.018851	1.841766
-91.384124	0.745161	1.846771
-92.064140	-13.670223	1.851776
-92.280433	-8.526661	1.856781
-92.218464	-9.680947	1.861786
-92.545245	-7.146060	1.866790
-92.887048	-7.366549	1.871795
-92.736402	-10.187225	1.876800
-93.506907	0.868904	1.881805
-93.638506	-8.114409	1.886810
-93.711835	-3.633762	1.891814
-93.579760	-1.282901	1.896819
-94.169369	0.124139	1.901824
-94.875653	1.284576	1.906829
-95.228984	-12.721395	1.911834
-95.301604	-2.615009	1.916838
-95.606299	-7.059976	1.921843
-95.286806	-11.491501	1.926848
-95.678922	-4.369882	1.931853
-95.704511	-9.383582	1.936858
-96.294153	-6.319563	1.941862
-96.637785	-5.034125	1.946867
-96.673964	-12.182547	1.951872
-97.213724	-9.096827	1.956877
-96.998202	-22.184275	1.961882
-97.856102	-14.562742	1.966886
-98.526166	-12.438256	1.971891
-98.177640	-12.702475	1.976896
-98.714226	-6.444425	1.981901
-98.727659	-12.970108	1.986906
-98.551928	-4.685514	1.991910
-98.817997	-0.024036	1.996915
-98.720236	-7.139288	2.006912
-99.424073	-6.007626	2.016909
-98.719197	-10.344310	2.026906
-98.091051	-5.730026	2.036902
-97.412599	-1.959875	2.046899
-97.166132	-5.093934	2.056896
-96.525139	-10.033489	2.066893
-95.857658	-3.683663	2.076890
-95.738733	-3.600431	2.086886
-95.155219	-9.273734	2.096883
-94.443871	-4.226943	2.106880
-94.057617	-6.763241	2.116877
-93.916315	-8.324449	2.126874
-93.375520	-10.583546	2.136870
-92.495944	-6.823123	2.146867
-91.622139	-11.239459	2.156864
-91.494485	-7.449460	2.166861
-91.433307	-13.766975	2.176858
-90.556942	-8.958242	2.186854
-90.216553	-13.212396	2.196851
-89.410765	-7.499055	2.206848
-88.777885	-7.129024	2.216845
-88.673870	-7.443219	2.226842
-87.840924	-2.303624	2.236838
-87.255055	0.634097	2.246835
-87.067786	-6.366877	2.256832
-86.893759	-12.148739	2.266829
-85.829760	-3.181274	2.276826
-85.682147	1.995597	2.286822
-85.148022	0.938513	2.296819
-84.077276	2.255274	2.306816
-83.688228	0.312246	2.316813
-83.916288	0.087242	2.326810
-83.141138	-0.752067	2.336806
-82.364430	2.760703	2.346803
-82.205782	7.510742	2.356800
-81.502395	-1.806740	2.366797
-80.974947	-5.821504	2.376794
-80.754158	2.835464	2.386790
-80.001305	2.902220	2.396787
-79.515591	7.828069	2.406784
-79.369824	3.352373	2.416781
-78.174943	3.179081	2.426778
-77.825212	10.680695	2.436774
-77.987266	14.562529	2.446771
-76.681009	7.596219	2.456768
-76.325346	8.350798	2.466765
-76.208127	5.289992	2.476762
-75.516664	9.924781	2.486758
-74.936854	5.177170	2.496755
-74.656954	9.571559	2.506752
-73.704037	5.850006	2.516749
-73.019048	-1.412131	2.526746
-73.129732	6.402331	2.536742
-72.958428	1.254563	2.546739
-72.035390	8.960401	2.556736
-71.455782	-0.892499	2.566733
-70.972580	-0.747522	2.576730
-70.267450	-0.178283	2.586726
-69.723303	8.569564	2.596723
-69.604535	6.682928	2.606720
-69.076646	4.610915	2.616717
-68.569524	3.980160	2.626714
-68.107955	2.735385	2.636710
-67.148464	3.803714	2.646707
-67.208042	9.246006	2.656704
-66.936996	6.630663	2.666701
-65.545083	7.690529	2.676698
-65.553700	-0.195455	2.686694
-65.050440	6.958774	2.696691
-64.153263	7.594880	2.706688
-63.815704	1.001030	2.716685
-63.805325	-1.486018	2.726682
-63.090678	1.320048	2.736678
-62.489940	6.137471	2.746675
-61.873507	4.427923	2.756672
-61.001772	6.902414	2.766669
-60.633412	6.037081	2.776666
-60.565103	4.904114	2.786662
-60.566233	5.480318	2.796659
-59.118032	6.948123	2.806656
-58.734458	5.080692	2.816653
-58.891042	3.203675	2.826650
-57.869596	9.830364	2.836646
-57.172626	5.914463	2.846643
-57.018908	6.033010	2.856640
-56.887026	2.499125	2.866637
-55.881560	-0.826509	2.876634
-55.492890	7.167133	2.886630
-54.789439	4.627896	2.896627
-54.373429	5.702012	2.906624
-53.982897	8.003596	2.916621
-53.216478	3.989214	2.926618
-52.791650	8.320984	2.936614
-52.764449	5.266053	2.946611
-51.858180	9.476889	2.956608
-51.081975	5.984671	2.966605
-50.907362	5.439227	2.976602
-50.922651	7.982344	2.986598
-49.960338	3.325857	2.996595
-49.592975	10.078276	3.006592
-48.504664	11.960376	3.016589
-48.249931	7.271155	3.026586
-48.200301	10.807002	3.036582
-47.597061	5.844086	3.046579
-46.989729	8.741103	3.056576
-46.607998	5.874411	3.066573
-45.571275	7.358463	3.076570
-45.183584	9.842296	3.086566
-45.085444	11.121394	3.096563
-44.852473	10.661088	3.106560
-43.959035	5.942946	3.116557
-43.519163	8.282958	3.126554
-42.579157	3.305355	3.136550
-42.733643	9.725849	3.146547
-42.002399	8.607155	3.156544
-40.944757	3.039775	3.166541
-40.769465	-3.311338	3.176538
-40.738810	4.057791	3.186534
-39.879742	4.804758	3.196531
-38.973852	7.777808	3.206528
-38.782564	7.545921	3.216525
-38.824691	2.507132	3.226522
-38.040004	2.229751	3.236518
-37.386965	11.964409	3.246515
-37.009844	13.559300	3.256512
-35.805515	3.360904	3.266509
-35.742263	8.626492	3.276506
-35.865322	6.081604	3.286502
-34.900582	9.380761	3.296499
-34.129630	2.143853	3.306496
-34.200991	12.323759	3.316493
-33.381771	2.247867	3.326490
-32.609370	13.275422	3.336486
-32.395070	8.859066	3.346483
-32.236877	7.022978	3.356480
-31.474973	9.041735	3.366477
-31.005928	12.278666	3.376474
-29.979581	11.417763	3.386470
-29.434648	11.505854	3.396467
-29.550160	8.701076	3.406464
-29.053427	8.974608	3.416461
-28.195702	12.486177	3.426458
-27.653806	8.238434	3.436454
-27.526830	17.603540	3.446451
-26.949864	9.427759	3.456448
-26.180988	12.740511	3.466445
-26.033522	6.398168	3.476442
-25.468142	13.227729	3.486438
-24.592623	11.214309	3.496435
-24.465442	5.253512	3.506432
-24.139022	15.016587	3.516429
-23.194182	6.072508	3.526426
-22.949408	5.347259	3.536422
-22.334168	7.261773	3.546419
-21.261877	5.246665	3.556416
-21.302497	3.668476	3.566413
-21.100656	4.730383	3.576410
-20.578226	1.574754	3.586406
-19.821251	10.182319	3.596403
-19.692568	6.745188	3.606400
-18.570370	5.186301	3.616397
-18.185315	2.491944	3.626394
-18.183192	-0.903204	3.636390
-17.554716	7.824513	3.646387
-16.549788	5.031262	3.656384
-16.467380	3.331460	3.666381
-15.319301	6.366999	3.676378
-15.109071	5.595134	3.686374
-14.957787	7.220652	3.696371
-14.916459	10.249105	3.706368
-13.593009	5.453165	3.716365
-13.190366	7.762620	3.726362
-13.073677	7.167136	3.736358
-12.215361	5.751697	3.746355
-11.821364	4.870449	3.756352
-11.536362	3.929868	3.766349
-10.422980	14.532654	3.776346
-10.329599	8.354798	3.786342
-10.133848	9.716660	3.796339
-9.037464	7.743389	3.806336
-8.818516	11.667003	3.816333
-8.739876	7.374360	3.826330
-7.635634	5.650911	3.836326
-6.905956	2.981661	3.846323
-6.843445	5.552548	3.856320
-6.566558	-0.975299	3.866317
-5.596108	2.555273	3.876314
-5.051654	6.684599	3.886310
-5.318053	8.463916	3.896307
-4.528996	7.233863	3.906304
-3.949843	14.715336	3.916301
-3.431961	29.395248	3.926298
-2.980126	32.942487	3.936294
-2.661707	43.388180	3.946291
-2.355723	58.613502	3.956288
-1.560526	69.830950	3.966285
-1.241645	77.983440	3.976282
-0.686151	93.528109	3.986278
-0.423615	108.760902	3.996275
0.000000	118.191726	4.001280
0.298138	130.431294	4.006285
0.501060	140.765087	4.011290
-0.033191	147.797328	4.016294
0.553724	142.823444	4.021299
0.925603	154.719652	4.026304
0.889205	159.356416	4.031309
1.000451	163.059138	4.036314
1.363758	166.243602	4.041318
0.890174	151.247109	4.046323
0.859237	159.417567	4.051328
0.894624	167.312187	4.056333
0.952265	167.339440	4.061338
1.124853	170.656050	4.066342
1.293972	165.505337	4.071347
1.196966	162.714549	4.076352
0.931109	163.304888	4.081357
0.737216	156.671386	4.086362
0.840053	171.839491	4.091366
0.936909	170.217241	4.096371
1.277158	169.401086	4.101376
1.008046	178.116513	4.106381
0.907940	166.297915	4.111386
0.847223	174.588771	4.116390
1.164273	169.665459	4.121395
1.321391	159.719214	4.126400
0.910017	169.190975	4.131405
1.202515	161.254742	4.136410
1.195838	171.285367	4.141414
1.031738	178.554064	4.146419
1.174929	161.303527	4.151424
0.995493	177.765300	4.156429
1.114758	167.403841	4.161434
0.988763	176.939860	4.166438
1.205072	183.268382	4.171443
1.455904	192.823468	4.176448
1.128575	192.721919	4.181453
1.515544	190.694074	4.186458
1.455600	199.410263	4.191462
1.401671	194.861579	4.196467
1.480579	178.944425	4.201472
1.065690	180.656111	4.206477
1.733708	190.041406	4.211482
1.340071	186.360424	4.216486
1.412162	184.281124	4.221491
1.487043	182.444079	4.226496
1.262919	183.315192	4.231501
1.404034	185.487776	4.236506
1.689895	199.418405	4.241510
1.420520	197.040271	4.246515
1.678748	191.559795	4.251520
1.178739	201.918517	4.256525
1.643173	191.990037	4.261530
1.706819	197.920665	4.266534
1.830046	198.791858	4.271539
1.636398	178.380978	4.276544
1.031864	175.404010	4.281549
1.474418	185.541318	4.286554
1.757251	201.186675	4.291558
1.752266	201.313927	4.296563
1.708683	186.834760	4.301568
1.237198	192.911762	4.306573
1.902128	191.338345	4.311578
1.965139	200.464280	4.316582
1.611674	181.874696	4.321587
1.733438	177.941693	4.326592
1.302846	185.571014	4.331597
1.772507	190.384540	4.336602
1.918736	197.255146	4.341606
2.021717	188.908181	4.346611
1.883069	178.995300	4.351616
1.586952	178.198297	4.356621
1.888762	180.410866	4.361626
1.678188	174.154665	4.366630
1.429669	186.456139	4.371635
1.673691	188.137429	4.376640
1.772211	191.335327	4.381645
2.094436	200.597154	4.386650
1.928262	198.559629	4.391654
2.032690	204.295818	4.396659
2.157631	207.677385	4.401664
1.665136	195.796315	4.406669
1.693433	188.263327	4.411674
1.867802	207.711745	4.416678
1.991495	207.558511	4.421683
2.199220	204.553867	4.426688
1.856825	212.915641	4.431693
2.139728	196.220815	4.436698
1.856409	185.288091	4.441702
1.630234	197.564745	4.446707
2.211138	197.556720	4.451712
1.934666	209.760443	4.456717
2.121925	209.361225	4.461722
1.831113	204.675498	4.466726
1.738921	204.802051	4.471731
2.062719	208.168521	4.476736
2.126383	205.773112	4.481741
2.317837	193.592072	4.486746
2.136351	199.115702	4.491750
2.082718	201.141087	4.496755
2.252615	198.643168	4.501760
1.766757	202.238348	4.506765
1.884925	197.050313	4.511770
1.954662	203.646124	4.516774
1.932488	201.731477	4.521779
1.958559	194.059737	4.526784
1.720176	206.959827	4.531789
1.773673	201.456744	4.536794
2.075188	218.798438	4.541798
2.189703	218.187536	4.546803
2.388019	221.780685	4.551808
2.510763	222.427396	4.556813
2.615594	218.936459	4.561818
1.878067	210.965204	4.566822
2.070649	221.330370	4.571827
2.523774	227.582448	4.576832
2.348610	237.251982	4.581837
2.477548	223.086082	4.586842
2.701483	227.758526	4.591846
2.682655	221.729925	4.596851
2.573181	197.934194	4.601856
2.090245	206.356621	4.606861
2.137052	201.416850	4.611866
2.224773	211.403197	4.616870
2.115816	219.377484	4.621875
2.731225	220.710714	4.626880
2.517284	235.832083	4.631885
2.564965	221.270620	4.636890
2.303799	209.325040	4.641894
2.483628	217.630990	4.646899
2.453431	218.296414	4.651904
2.539298	231.730479	4.656909
2.642751	211.497693	4.661914
2.641502	226.070436	4.666918
2.466057	224.036422	4.671923
2.647236	216.572530	4.676928
2.614154	227.992656	4.681933
2.639358	219.081406	4.686938
2.159446	227.070394	4.691942
2.415437	230.088994	4.696947
2.693035	227.177121	4.701952
2.654199	229.442572	4.706957
2.873352	233.701415	4.711962
2.849746	235.232034	4.716966
2.598223	236.760480	4.721971
2.794613	236.251803	4.726976
2.826793	237.196543	4.731981
2.663764	236.457926	4.736986
2.762322	225.236540	4.741990
2.557243	240.654412	4.746995
2.643624	224.904885	4.752000
2.870378	235.199655	4.757005
2.769325	232.793536	4.762010
2.517689	235.770620	4.767014
2.739916	243.030975	4.772019
2.506935	228.913784	4.777024
2.590510	235.287874	4.782029
2.752037	236.535924	4.787034
2.713597	239.477175	4.792038
2.775687	236.276905	4.797043
2.994426	239.246447	4.802048
2.879198	242.360302	4.807053
3.155962	229.224172	4.812058
3.032969	238.996923	4.817062
2.802210	234.916685	4.822067
2.965919	228.390061	4.827072
2.793423	234.972674	4.832077
2.956081	230.996945	4.837082
2.875342	239.940980	4.842086
2.399416	231.677788	4.847091
3.196823	240.990893	4.852096
2.695322	235.730618	4.857101
2.852947	231.399342	4.862106
3.005175	235.248005	4.867110
3.055411	254.155704	4.872115
3.505138	254.709781	4.877120
2.965555	253.209496	4.882125
3.048454	236.353500	4.887130
2.894787	235.790333	4.892134
2.973480	250.839196	4.897139
3.533907	250.266453	4.902144
3.009669	248.495640	4.907149
3.129535	240.417567	4.912154
3.453624	237.922032	4.917158
2.780555	244.305670	4.922163
3.159674	245.879460	4.927168
3.475657	264.920203	4.932173
3.170079	253.241266	4.937178
3.283564	250.363575	4.942182
3.080237	257.699608	4.947187
3.419337	259.587890	4.952192
3.382261	256.313722	4.957197
3.230587	245.071954	4.962202
3.247658	248.164411	4.967206
2.955359	254.984012	4.972211
3.368739	250.606470	4.977216
2.911075	267.013156	4.982221
3.172524	265.273553	4.987226
3.441828	275.569170	4.992230
3.234989	264.610259	4.997235
3.592465	263.231600	5.002240
3.650281	269.060217	5.007245
3.590443	267.719155	5.012250
3.707532	260.338119	5.017254
3.277957	269.610898	5.022259
3.369719	263.262570	5.027264
3.190811	273.814631	5.032269
3.194761	258.807720	5.037274
3.581311	271.145185	5.042278
3.234801	266.588873	5.047283
3.434008	260.215386	5.052288
3.511607	270.220226	5.057293
3.164318	262.375293	5.062298
3.382483	270.045012	5.067302
3.195102	272.370879	5.072307
3.586055	265.271693	5.077312
3.321330	272.440537	5.082317
3.269224	266.086917	5.087322
3.715832	274.240414	5.092326
3.554601	284.180179	5.097331
3.678425	282.552646	5.102336
3.337486	285.831308	5.107341
3.801618	287.858453	5.112346
3.909431	300.597474	5.117350
3.583801	289.615864	5.122355
3.458449	279.662624	5.127360
3.558515	285.627685	5.132365
3.635521	288.869830	5.137370
3.944076	295.548132	5.142374
3.818956	290.351173	5.147379
3.956952	296.614024	5.152384
3.690248	293.055378	5.157389
3.823546	293.989628	5.162394
3.697446	286.766220	5.167398
3.711902	301.161586	5.172403
3.666949	285.565055	5.177408
3.996590	291.573456	5.182413
3.486976	290.304393	5.187418
3.298124	294.221014	5.192422
3.393284	302.830375	5.197427
3.665316	295.907823	5.202432
3.454351	293.114840	5.207437
3.742101	292.697731	5.212442
3.874481	300.767315	5.217446
3.772020	313.578990	5.222451
4.269823	308.637035	5.227456
4.010245	318.537521	5.232461
3.997869	295.712958	5.237466
3.949284	286.257848	5.242470
3.615488	296.267351	5.247475
4.355806	311.339099	5.252480
4.081452	302.455493	5.257485
3.819158	299.557377	5.262490
4.157085	308.012920	5.267494
4.209641	309.364140	5.272499
4.230180	296.669552	5.277504
4.152308	291.693646	5.282509
4.018059	292.347756	5.287514
4.015330	286.184240	5.292518
4.143536	298.344051	5.297523
4.454689	277.150569	5.302528
4.119509	289.894546	5.307533
4.188785	289.210649	5.312538
4.295934	288.591300	5.317542
3.910349	286.426842	5.322547
3.943254	281.805287	5.327552
4.053110	296.554791	5.332557
4.152743	311.154850	5.337562
4.318986	305.259043	5.342566
3.987638	314.429285	5.347571
4.128675	310.340308	5.352576
4.536379	314.247361	5.357581
4.167267	321.273344	5.362586
4.025325	315.391070	5.367590
4.146598	321.458391	5.372595
4.571299	312.380434	5.377600
4.457877	313.394374	5.382605
4.647883	321.283894	5.387610
4.414068	310.660954	5.392614
4.096214	323.004056	5.397619
4.267834	319.493707	5.402624
4.280707	310.436058	5.407629
4.368372	316.678670	5.412634
4.616563	309.176954	5.417638
4.253985	324.494007	5.422643
4.395765	311.618822	5.427648
4.390360	315.892912	5.432653
4.415098	315.347448	5.437658
4.409942	314.137991	5.442662
4.252901	316.450928	5.447667
4.486407	323.220650	5.452672
4.568865	318.522767	5.457677
4.358816	314.339215	5.462682
4.901221	323.206949	5.467686
4.595761	331.132655	5.472691
4.637613	316.147805	5.477696
4.113702	325.366442	5.482701
4.240564	313.390616	5.487706
4.526553	313.091214	5.492710
4.168294	323.779484	5.497715
4.539466	316.972657	5.502720
4.660452	328.902022	5.507725
4.371046	332.930285	5.512730
4.608402	336.738774	5.517734
4.705738	350.351004	5.522739
5.003733	343.989477	5.527744
4.593763	353.235959	5.532749
4.907481	353.690301	5.537754
4.632095	337.752548	5.542758
4.598115	353.086245	5.547763
4.968711	340.451242	5.552768
5.009411	349.871252	5.557773
4.702823	340.037096	5.562778
4.738128	321.885330	5.567782
4.570022	335.538513	5.572787
4.933542	342.561321	5.577792
4.866789	348.185516	5.582797
4.787759	344.646179	5.587802
5.011367	345.349340	5.592806
4.910872	354.543393	5.597811
5.374884	339.844338	5.602816
4.814722	331.853601	5.607821
4.856087	323.032548	5.612826
4.745604	317.039273	5.617830
4.387076	319.836413	5.622835
4.700444	328.162455	5.627840
4.875117	343.963279	5.632845
4.812245	346.262738	5.637850
4.883363	341.511085	5.642854
4.942933	350.108826	5.647859
5.043063	354.381566	5.652864
4.951981	350.270975	5.657869
4.951466	350.007553	5.662874
5.155802	351.505031	5.667878
4.992457	360.497006	5.672883
4.841485	345.315469	5.677888
4.684377	355.710238	5.682893
4.750238	357.327625	5.687898
5.258446	353.858999	5.692902
4.776519	357.551439	5.697907
4.644402	357.207476	5.702912
4.811737	369.766360	5.707917
5.010514	379.048618	5.712922
5.258781	388.668188	5.717926
5.121521	389.095671	5.722931
5.516628	382.730418	5.727936
5.189274	379.783111	5.732941
5.285564	385.724764	5.737946
5.560383	380.968049	5.742950
5.192030	380.774848	5.747955
5.354067	379.338089	5.752960
5.193300	388.892450	5.757965
5.248469	389.476203	5.762970
5.340914	377.625239	5.767974
5.084663	383.121302	5.772979
5.587845	385.354696	5.777984
5.391084	377.951971	5.782989
5.011425	387.548636	5.787994
5.434807	383.025537	5.792998
5.137873	381.222646	5.798003
5.255332	385.092123	5.803008
5.276017	382.071177	5.808013
5.410190	388.062971	5.813018
5.428701	378.761229	5.818022
4.996640	384.135555	5.823027
5.394416	382.023602	5.828032
5.241403	388.446357	5.833037
5.038189	388.906312	5.838042
5.221479	385.268898	5.843046
5.186701	395.108386	5.848051
5.125338	403.419600	5.853056
5.514850	409.042567	5.858061
5.549546	408.410195	5.863066
5.554438	407.614845	5.868070
5.258442	413.007807	5.873075
5.437230	408.213964	5.878080
5.758114	410.261188	5.883085
5.610604	416.005195	5.888090
5.875957	411.548218	5.893094
5.711213	415.954988	5.898099
5.674957	415.906681	5.903104
5.469481	423.304323	5.908109
5.343602	426.275536	5.913114
5.810817	408.958036	5.918118
5.460329	416.804839	5.923123
5.666267	413.642585	5.928128
5.809411	416.576577	5.933133
5.721743	423.888726	5.938138
6.195519	412.271733	5.943142
5.887885	416.785729	5.948147
6.152086	401.627872	5.953152
5.916843	413.909954	5.958157
5.768665	410.453334	5.963162
6.167500	418.867832	5.968166
5.867796	409.451627	5.973171
5.608626	396.070551	5.978176
5.809324	394.463774	5.983181
5.694928	406.846334	5.988186
5.754954	411.880365	5.993190
5.633597	427.469014	5.998195
5.851778	424.907186	6.003200
5.737211	423.186063	6.008205
5.568360	428.710239	6.013210
5.803129	425.909444	6.018214
5.674206	421.683172	6.023219
5.971899	413.868097	6.028224
6.161838	419.626264	6.033229
5.858902	424.043378	6.038234
6.093823	413.992474	6.043238
5.840136	420.707457	6.048243
6.101918	417.193148	6.053248
6.133706	429.586356	6.058253
5.712508	423.285341	6.063258
6.011211	422.555803	6.068262
5.534848	427.388523	6.073267
5.792733	419.883958	6.078272
6.009201	427.258628	6.083277
5.959807	429.241898	6.088282
5.991753	425.117152	6.093286
5.768269	421.817694	6.098291
5.571416	419.659931	6.103296
5.873153	426.462955	6.108301
6.094320	432.142922	6.113306
6.107380	414.822171	6.118310
5.556301	431.686589	6.123315
5.747562	423.632666	6.128320
6.215014	423.831956	6.133325
5.925759	427.627559	6.138330
5.722457	425.346941	6.143334
5.707519	436.085570	6.148339
5.534300	424.289584	6.153344
5.666678	425.981367	6.158349
5.748833	423.339537	6.163354
5.950007	415.267591	6.168358
5.537701	419.751034	6.173363
5.878558	418.026631	6.178368
6.055159	422.929991	6.183373
6.025282	420.237124	6.188378
6.329122	414.917512	6.193382
6.058381	413.322399	6.198387
5.938510	414.850488	6.203392
6.142096	419.720156	6.208397
5.500009	420.956957	6.213402
5.893817	410.815707	6.218406
5.778115	419.432162	6.223411
5.777677	422.243994	6.228416
6.066423	419.048044	6.233421
5.870593	420.765374	6.238426
6.307869	415.300050	6.243430
6.138583	419.887546	6.248435
6.072234	424.579886	6.253440
5.952057	417.316754	6.258445
5.676079	412.166142	6.263450
6.190753	400.819418	6.268454
5.832843	409.059949	6.273459
5.698967	399.253089	6.278464
5.894903	404.542373	6.283469
5.944984	411.240010	6.288474
6.305865	409.816767	6.293478
5.980021	401.387442	6.298483
5.856343	388.896326	6.303488
5.996505	392.836031	6.308493
5.603016	401.045768	6.313498
5.529106	380.809880	6.318502
5.709775	402.529606	6.323507
5.827325	405.941256	6.328512
6.175152	414.403106	6.333517
5.953758	410.491170	6.338522
5.707906	400.869078	6.343526
5.860724	412.443145	6.348531
5.869109	418.163607	6.353536
6.123873	414.751304	6.358541
5.864903	400.746810	6.363546
6.227107	399.235139	6.368550
5.723190	386.131951	6.373555
5.752851	391.533329	6.378560
6.026306	393.310784	6.383565
5.920714	400.333650	6.388570
5.552934	390.654871	6.393574
5.638072	400.088443	6.398579
5.808210	411.911824	6.403584
6.195226	411.743628	6.408589
6.102484	411.105009	6.413594
6.479146	384.814384	6.418598
5.982535	401.494483	6.423603
5.893534	387.526670	6.428608
6.093420	389.066726	6.433613
6.043472	393.165905	6.438618
6.221969	376.367274	6.443622
5.998708	395.070388	6.448627
5.849473	384.917202	6.453632
5.718041	386.407349	6.458637
5.732966	389.240499	6.463642
6.032152	382.992028	6.468646
5.747599	395.941389	6.473651
5.742602	391.618552	6.478656
6.121699	384.298098	6.483661
5.889833	390.187739	6.488666
6.120188	384.820363	6.493670
5.874837	391.034296	6.498675
5.921761	386.237317	6.503680
5.839847	392.492361	6.508685
5.838471	384.278275	6.513690
5.833329	382.407740	6.518694
5.534879	387.370518	6.523699
5.661830	393.454091	6.528704
5.720452	380.826315	6.533709
5.897365	390.683103	6.538714
5.885989	386.449733	6.543718
5.815736	390.037244	6.548723
5.466534	393.381238	6.553728
5.903494	379.775928	6.558733
5.545821	385.422841	6.563738
5.982569	388.098455	6.568742
5.727025	391.244543	6.573747
5.797472	389.745653	6.578752
6.254942	384.323160	6.583757
6.036040	392.592474	6.588762
5.900876	382.502269	6.593766
5.954517	386.998038	6.598771
5.845682	389.996406	6.603776
6.012953	383.503461	6.608781
5.559551	386.102275	6.613786
5.728623	377.198592	6.618790
5.731200	393.635075	6.623795
5.861756	387.873633	6.628800
5.876580	379.689614	6.633805
5.652495	389.429536	6.638810
5.971299	377.074250	6.643814
5.905246	387.064762	6.648819
5.779725	386.300760	6.653824
6.085972	384.993359	6.658829
5.531494	376.687695	6.663834
6.026773	396.959174	6.668838
5.836937	393.426207	6.673843
6.437213	402.387573	6.678848
6.326708	392.597158	6.683853
6.021289	389.605157	6.688858
5.704112	383.364223	6.693862
5.809698	387.031828	6.698867
5.900204	383.225526	6.703872
6.189792	384.498675	6.708877
5.865126	384.178626	6.713882
6.189643	389.339971	6.718886
5.956461	381.265059	6.723891
5.719378	389.315788	6.728896
6.143809	384.161241	6.733901
5.780518	391.298965	6.738906
6.443646	387.693876	6.743910
6.094160	393.701342	6.748915
5.812708	392.695477	6.753920
6.075155	390.726194	6.758925
5.968596	393.149546	6.763930
5.860710	382.901675	6.768934
5.612495	390.903737	6.773939
5.660978	401.936090	6.778944
5.820358	387.930543	6.783949
5.755439	396.520586	6.788954
6.135157	381.238961	6.793958
5.781955	396.068688	6.798963
5.962977	391.720060	6.803968
6.093310	392.042086	6.808973
5.548882	391.487627	6.813978
5.952853	393.716201	6.818982
5.878186	397.926445	6.823987
5.834490	390.958850	6.828992
6.176342	388.366013	6.833997
6.125437	396.788163	6.839002
5.883916	387.623965	6.844006
5.841798	384.329493	6.849011
5.868488	386.571249	6.854016
6.052466	385.723241	6.859021
5.608222	380.191930	6.864026
5.795307	373.677540	6.869030
5.668889	397.573793	6.874035
6.015860	393.925547	6.879040
5.769540	394.587240	6.884045
5.743389	390.718236	6.889050
5.990884	390.977571	6.894054
5.593957	397.054098	6.899059
5.877155	397.475035	6.904064
6.309364	388.196873	6.909069
5.980636	386.691125	6.914074
6.140559	391.650922	6.919078
5.537708	383.866365	6.924083
5.722752	395.765400	6.929088
6.112949	389.181130	6.934093
5.815188	393.737483	6.939098
5.997384	386.971115	6.944102
5.969119	388.858121	6.949107
6.063559	391.858615	6.954112
5.737795	371.818327	6.959117
5.634200	394.646360	6.964122
5.716621	386.174241	6.969126
5.718826	392.323542	6.974131
6.083813	389.466180	6.979136
5.708094	387.665137	6.984141
5.568846	399.403775	6.989146
6.020803	389.885923	6.994150
5.764685	390.391179	6.999155
5.743354	391.985372	7.004160
5.897175	394.380440	7.009165
5.542094	397.376723	7.014170
5.910501	389.338166	7.019174
5.729274	398.932441	7.024179
5.637577	399.263154	7.029184
5.979889	401.080275	7.034189
5.682630	411.577904	7.039194
6.004465	391.758309	7.044198
5.693289	394.299343	7.049203
5.647877	397.590079	7.054208
6.063759	394.217895	7.059213
5.989200	391.243365	7.064218
5.857600	389.797794	7.069222
6.015427	396.337012	7.074227
5.785938	393.838158	7.079232
5.847849	389.632072	7.084237
5.710421	388.718102	7.089242
5.826815	393.244290	7.094246
6.008959	394.855771	7.099251
5.737146	390.416457	7.104256
5.588567	385.972447	7.109261
5.634140	398.222441	7.114266
5.660219	388.943312	7.119270
5.988542	408.764219	7.124275
6.015697	412.217142	7.129280
5.728504	399.483836	7.134285
5.612300	405.670190	7.139290
6.119853	413.410278	7.144294
5.877590	415.903749	7.149299
6.116566	418.217769	7.154304
6.267458	398.241678	7.159309
5.557932	396.334503	7.164314
5.568004	389.924321	7.169318
5.712709	407.089432	7.174323
5.829556	417.950592	7.179328
6.207308	414.901662	7.184333
5.951913	415.270045	7.189338
6.096803	404.068061	7.194342
5.865586	388.229080	7.199347
5.698135	395.461928	7.204352
5.982354	393.379308	7.209357
5.821848	389.769834	7.214362
5.603987	392.951889	7.219366
5.605734	408.411325	7.224371
5.832226	424.854034	7.229376
5.907565	422.326015	7.234381
5.847242	420.122469	7.239386
6.047652	417.995958	7.244390
5.955246	420.997916	7.249395
5.927567	422.953304	7.254400
6.093513	415.276358	7.259405
5.625598	416.246024	7.264410
6.083204	411.893054	7.269414
5.992621	410.536369	7.274419
6.006987	411.664446	7.279424
6.068455	403.661708	7.284429
5.403959	404.702727	7.289434
5.627683	406.826288	7.294438
6.133593	416.418046	7.299443
5.634522	432.357594	7.304448
6.043087	427.944098	7.309453
5.698249	426.591788	7.314458
6.252736	424.180076	7.319462
5.864288	422.197821	7.324467
5.798720	401.771077	7.329472
6.239273	397.084884	7.334477
5.465642	405.813063	7.339482
5.681576	403.782443	7.344486
5.766330	417.628298	7.349491
5.753434	421.761384	7.354496
6.237466	430.351366	7.359501
5.966692	428.806972	7.364506
5.983822	421.915882	7.369510
6.046181	412.882310	7.374515
5.785411	398.734260	7.379520
5.746874	399.269259	7.384525
5.913760	405.167413	7.389530
6.107331	407.658293	7.394534
5.791321	397.096120	7.399539
5.594405	403.014095	7.404544
5.857455	401.407215	7.409549
6.017262	423.456829	7.414554
5.900054	413.609893	7.419558
5.717692	400.986836	7.424563
5.557977	416.287032	7.429568
5.790699	413.395410	7.434573
5.558113	430.271217	7.439578
5.946998	420.886178	7.444582
5.849109	428.364803	7.449587
6.179987	431.548992	7.454592
6.124806	422.193563	7.459597
6.141778	425.754348	7.464602
6.036917	421.136905	7.469606
5.519265	416.079942	7.474611
5.743477	420.017325	7.479616
5.870405	426.137423	7.484621
5.927728	422.818717	7.489626
5.968824	426.532570	7.494630
5.829242	429.840742	7.499635
5.847099	429.507566	7.504640
6.099136	430.225936	7.509645
5.987638	432.472514	7.514650
6.285813	423.288046	7.519654
5.891419	399.992447	7.524659
5.806689	402.854991	7.529664
6.025481	389.471827	7.534669
5.677723	397.331979	7.539674
5.415874	394.394303	7.544678
5.779227	403.266982	7.549683
5.893360	422.068953	7.554688
6.347569	415.524352	7.559693
5.907939	418.638886	7.564698
5.828911	398.817044	7.569702
5.844530	398.365642	7.574707
5.551777	396.929690	7.579712
6.087896	409.581819	7.584717
5.813655	412.970979	7.589722
5.728054	410.769269	7.594726
5.861383	420.275749	7.599731
6.030251	420.617418	7.604736
5.975424	419.024698	7.609741
5.837917	414.719736	7.614746
5.771573	404.404363	7.619750
6.171964	419.397351	7.624755
5.867122	415.851527	7.629760
5.999323	397.065119	7.634765
6.053911	397.253905	7.639770
6.145646	395.735295	7.644774
6.032637	394.206909	7.649779
6.069691	393.194277	7.654784
6.049379	395.158500	7.659789
5.996971	397.560814	7.664794
6.047372	398.666719	7.669798
6.258700	397.231237	7.674803
6.138918	391.922454	7.679808
6.053599	383.866179	7.684813
5.904369	399.238418	7.689818
5.787465	405.207623	7.694822
5.761550	398.746192	7.699827
5.732534	402.410126	7.704832
6.000345	400.930130	7.709837
6.032957	402.498189	7.714842
5.909785	391.154291	7.719846
5.807501	396.995558	7.724851
5.758047	404.814417	7.729856
5.909690	393.594149	7.734861
5.830404	404.484152	7.739866
5.944365	393.227327	7.744870
6.204231	396.446203	7.749875
5.882656	396.231215	7.754880
5.745459	397.200173	7.759885
5.760743	399.171505	7.764890
5.640862	397.523690	7.769894
5.638238	395.348050	7.774899
5.409461	403.261836	7.779904
5.749512	398.609714	7.784909
5.668409	397.571335	7.789914
5.869532	389.256690	7.794918
5.793939	393.594368	7.799923
5.237648	398.249147	7.804928
5.857779	389.889914	7.809933
5.717615	400.142578	7.814938
5.812427	397.153510	7.819942
5.829735	404.675925	7.824947
6.140663	416.700277	7.829952
5.759146	399.749619	7.834957
5.998082	407.231051	7.839962
5.856644	405.051252	7.844966
5.967914	395.636795	7.849971
5.958163	399.154656	7.854976
5.948391	395.044154	7.859981
5.969022	397.849717	7.864986
5.812383	393.488346	7.869990
5.930635	397.114578	7.874995
5.348223	398.260353	7.880000
6.068821	404.600652	7.885005
5.827140	408.128651	7.890010
5.990077	403.094525	7.895014
6.291913	397.618371	7.900019
5.720592	400.150355	7.905024
6.175190	402.269085	7.910029
5.912954	400.555145	7.915034
5.619290	401.777047	7.920038
5.849229	395.442797	7.925043
5.843135	399.162909	7.930048
5.838894	397.204606	7.935053
5.742796	400.056607	7.940058
5.661797	398.540463	7.945062
5.889733	402.262918	7.950067
5.989048	406.813853	7.955072
5.993838	394.363144	7.960077
5.766169	402.512758	7.965082
6.125136	397.286602	7.970086
6.239046	386.425446	7.975091
5.883951	388.484785	7.980096
6.139086	395.361452	7.985101
5.843397	394.223963	7.990106
6.094732	396.963352	7.995110
6.141808	389.383337	8.000115
6.002927	399.314511	8.005133
5.654819	395.026866	8.010150
5.767935	404.382284	8.015168
5.822309	399.276233	8.020186
5.558909	395.893709	8.025203
5.835852	401.837381	8.030221
5.933319	399.247151	8.035238
5.502351	399.532284	8.040256
5.807918	407.311179	8.045274
5.639090	400.075510	8.050291
5.952640	414.541804	8.055309
6.216812	418.505906	8.060326
5.919107	412.026229	8.065344
5.406830	412.941945	8.070362
5.912643	413.383144	8.075379
5.504531	428.064675	8.080397
6.029291	426.220462	8.085414
5.989859	425.081981	8.090432
6.161048	432.402366	8.095450
6.110377	427.599960	8.100467
5.936504	441.059412	8.105485
6.422530	432.644110	8.110502
6.140204	425.464102	8.115520
5.677856	434.455987	8.120538
6.029051	424.355586	8.125555
5.961951	433.939188	8.130573
5.926748	426.711409	8.135590
5.942729	435.525566	8.140608
6.357154	427.995116	8.145626
6.377702	432.755749	8.150643
5.608183	409.576574	8.155661
5.898669	413.782931	8.160678
5.825929	423.953037	8.165696
5.930582	427.348045	8.170714
6.174102	425.993453	8.175731
6.059323	432.051261	8.180749
6.184367	428.108342	8.185766
6.297778	432.559866	8.190784
6.150517	426.390773	8.195802
6.509394	420.252106	8.200819
5.800028	418.627011	8.205837
6.118493	413.549491	8.210854
6.028960	421.467683	8.215872
6.045477	432.018197	8.220890
6.114975	422.461622	8.225907
6.208554	420.350729	8.230925
6.426749	422.030765	8.235942
6.197673	403.569179	8.240960
5.827224	413.394119	8.245978
5.740149	402.944576	8.250995
5.726110	429.228769	8.256013
6.016357	423.611107	8.261030
6.220575	429.913892	8.266048
5.823267	432.680990	8.271066
6.017922	427.367377	8.276083
5.721052	434.266598	8.281101
5.765763	424.700167	8.286118
5.944737	431.048877	8.291136
6.149164	442.765096	8.296154
6.354446	434.721625	8.301171
5.885699	448.633407	8.306189
6.159297	447.865490	8.311206
6.665088	448.025027	8.316224
6.572103	443.664255	8.321242
6.180568	430.041788	8.326259
6.150821	424.734574	8.331277
6.239510	423.029376	8.336294
6.386059	426.934890	8.341312
6.195727	431.268415	8.346330
6.474586	425.077896	8.351347
5.961533	437.354867	8.356365
6.217812	428.765375	8.361382
6.308584	428.679951	8.366400
6.048382	437.961040	8.371418
6.257233	429.285149	8.376435
5.888437	432.147104	8.381453
6.015408	442.157857	8.386470
6.299188	451.113513	8.391488
6.625750	465.604855	8.396506
6.327750	450.337643	8.401523
6.287141	440.158279	8.406541
6.255024	436.530627	8.411558
6.259238	440.571408	8.416576
6.064951	456.310626	8.421594
6.360511	447.417378	8.426611
6.398427	459.926768	8.431629
6.300150	459.762543	8.436646
6.272638	466.667393	8.441664
6.284030	461.106698	8.446682
6.340883	460.840513	8.451699
6.319344	468.883044	8.456717
6.255323	466.161984	8.461734
6.784122	460.112368	8.466752
6.529786	465.596790	8.471770
6.607331	453.080669	8.476787
6.321756	446.684976	8.481805
6.297541	429.811201	8.486822
6.161420	435.096845	8.491840
5.873265	460.944025	8.496858
6.623862	462.334995	8.501875
6.377058	464.367698	8.506893
6.386906	472.287309	8.511910
6.876751	467.956212	8.516928
6.460871	468.617543	8.521946
6.446375	461.850634	8.526963
6.499893	462.180223	8.531981
6.303696	449.613750	8.536998
6.420592	452.604798	8.542016
6.763084	461.424532	8.547034
6.599968	447.761325	8.552051
6.264996	442.033429	8.557069
6.417368	432.976803	8.562087
6.436595	439.102685	8.567104
6.204920	448.455409	8.572122
6.512629	464.769004	8.577139
6.556258	465.120511	8.582157
6.623217	462.594391	8.587175
6.823371	467.416313	8.592192
6.156750	455.780314	8.597210
6.478205	450.311377	8.602227
6.457222	466.743385	8.607245
6.537145	470.999520	8.612263
6.621724	460.559788	8.617280
6.688684	472.675617	8.622298
6.229486	457.791655	8.627315
6.462417	473.754732	8.632333
6.306785	469.127226	8.637351
6.627090	466.038176	8.642368
6.296476	464.849087	8.647386
6.366036	460.929554	8.652403
6.583813	467.062794	8.657421
6.491358	464.126795	8.662439
6.822277	466.922836	8.667456
6.599594	466.472232	8.672474
6.567870	463.204712	8.677491
6.793951	460.894640	8.682509
6.659492	456.339202	8.687527
6.562676	461.284690	8.692544
6.543307	468.903279	8.697562
6.597585	459.169110	8.702579
6.489252	461.508095	8.707597
6.467403	470.018942	8.712615
6.546964	470.366248	8.717632
6.246096	474.726032	8.722650
6.587081	457.494699	8.727667
6.789487	468.134602	8.732685
6.510330	472.707882	8.737703
6.861893	465.554562	8.742720
6.514954	464.587261	8.747738
6.460088	464.547698	8.752755
6.457571	469.237773	8.757773
6.261917	460.941278	8.762791
6.457459	475.614827	8.767808
6.238536	496.526209	8.772826
6.533935	493.927076	8.777843
6.675011	498.165181	8.782861
6.724039	498.295929	8.787879
6.947909	489.468309	8.792896
6.840730	494.197047	8.797914
7.084634	495.126625	8.802931
6.997016	487.407774	8.807949
6.873979	498.336812	8.812967
7.283956	487.360930	8.817984
7.134570	479.634437	8.823002
6.597551	472.190670	8.828019
6.846517	468.315913	8.833037
6.754355	468.119178	8.838055
6.908685	459.917250	8.843072
6.768906	467.243087	8.848090
6.565182	464.170677	8.853107
6.498366	465.683350	8.858125
6.273448	480.079778	8.863143
7.122163	483.070828	8.868160
7.160526	500.315569	8.873178
6.754510	486.030756	8.878195
6.782081	484.926011	8.883213
6.891230	491.696945	8.888231
6.810548	488.114162	8.893248
6.732413	497.544534	8.898266
7.108368	497.366631	8.903283
6.885128	506.990011	8.908301
6.793537	495.741622	8.913319
6.909022	490.047877	8.918336
6.702799	498.719296	8.923354
6.901639	498.208860	8.928371
7.177440	489.650141	8.933389
6.724492	496.174582	8.938407
7.108098	484.404536	8.943424
6.956867	492.845572	8.948442
6.699945	500.338127	8.953459
7.272489	492.953591	8.958477
6.512084	490.023706	8.963495
6.709413	485.752447	8.968512
7.055256	489.177055	8.973530
6.894855	500.688238	8.978547
7.070954	491.975437	8.983565
6.806309	493.659369	8.988583
7.030671	488.224667	8.993600
6.649709	488.826263	8.998618
6.595503	492.243558	9.003635
6.905948	500.593487	9.008653
6.712919	497.869655	9.013671
6.878346	493.228534	9.018688
6.497608	494.764260	9.023706
6.907105	503.615987	9.028723
7.160329	495.199588	9.033741
6.752818	495.594789	9.038759
6.708762	495.413875	9.043776
6.885022	513.515747	9.048794
7.308422	522.950948	9.053811
7.215975	522.230487	9.058829
6.996171	521.555014	9.063847
7.122784	520.967220	9.068864
7.213483	526.085479	9.073882
6.981119	523.747674	9.078899
7.025570	520.306077	9.083917
7.136073	535.213286	9.088935
7.284613	519.549564	9.093952
7.002910	505.693045	9.098970
6.797426	508.469211	9.103987
7.480481	529.113395	9.109005
7.250265	515.242010	9.114023
7.393452	505.460556	9.119040
7.105700	497.904285	9.124058
6.820055	497.661569	9.129075
7.063252	492.340062	9.134093
6.946712	514.436507	9.139111
7.235415	522.939459	9.144128
7.646266	516.688384	9.149146
7.032384	513.642414	9.154163
7.052997	500.795197	9.159181
6.772887	514.451490	9.164199
7.134197	520.544752	9.169216
7.117529	518.341158	9.174234
7.324599	524.463800	9.179251
7.352023	521.035268	9.184269
7.229786	529.476819	9.189287
7.359780	523.448592	9.194304
7.476741	526.342408	9.199322
6.892544	517.476469	9.204339
7.160891	513.525652	9.209357
7.279568	523.688610	9.214375
7.050417	519.666170	9.219392
7.352377	527.820102	9.224410
7.210046	518.318756	9.229427
7.192481	518.428490	9.234445
6.893223	521.939079	9.239463
7.240351	525.964413	9.244480
7.064065	530.343264	9.249498
7.042825	531.884979	9.254515
7.514956	525.425897	9.259533
7.468531	522.465899	9.264551
7.092156	530.440291	9.269568
7.332273	531.378768	9.274586
6.956222	537.271995	9.279603
6.974053	524.183511	9.284621
6.796655	531.840011	9.289639
7.490214	538.160114	9.294656
7.697908	542.700910	9.299674
7.462759	541.397923	9.304691
7.376628	528.560357	9.309709
7.273318	531.564797	9.314727
7.271472	529.826413	9.319744
7.174705	531.512559	9.324762
7.321732	550.930242	9.329779
7.445782	547.859626	9.334797
7.389104	558.842434	9.339815
7.567563	558.970368	9.344832
7.620026	560.581716	9.349850
7.285156	551.511730	9.354867
7.258056	549.834426	9.359885
7.454824	559.785822	9.364903
7.670201	561.281122	9.369920
7.403984	552.612483	9.374938
7.551246	555.438674	9.379955
7.878272	540.578654	9.384973
7.375734	531.505647	9.389991
7.302277	538.941742	9.395008
7.342330	526.246378	9.400026
7.396562	541.094251	9.405043
7.639026	539.750453	9.410061
7.426698	555.125283	9.415079
7.368247	557.334545	9.420096
7.658260	553.347442	9.425114
7.482119	564.192842	9.430131
7.642027	554.225129	9.435149
7.473923	551.618984	9.440167
7.377726	560.719551	9.445184
7.714958	554.272252	9.450202
7.337353	566.656326	9.455219
7.782024	556.280285	9.460237
7.633422	561.691264	9.465255
7.564165	562.444969	9.470272
7.683976	554.654796	9.475290
7.426756	551.455249	9.480307
7.583336	559.900269	9.485325
7.611540	557.519541	9.490343
7.771340	560.768415	9.495360
8.053691	555.656698	9.500378
7.491528	548.105272	9.505395
7.360013	536.222404	9.510413
7.482046	540.664062	9.515431
7.302774	550.522265	9.520448
7.931371	551.808928	9.525466
7.780738	551.382365	9.530483
7.729333	545.144147	9.535501
7.807172	557.333227	9.540519
7.917474	552.807935	9.545536
7.742910	545.664678	9.550554
7.387835	548.425366	9.555571
7.525453	549.309432	9.560589
7.880003	556.416736	9.565607
7.668997	555.461673	9.570624
7.778591	555.510904	9.575642
7.983191	566.012923	9.580659
7.739542	555.303699	9.585677
7.256202	544.521342	9.590695
7.631268	554.607257	9.595712
7.837156	549.786771	9.600730
7.911323	552.894380	9.605747
7.934130	545.637417	9.610765
8.209998	556.078965	9.615783
7.599410	546.448369	9.620800
7.584383	538.256245	9.625818
7.799689	551.638308	9.630835
7.562848	550.987120	9.635853
7.362164	550.630093	9.640871
7.429904	566.340827	9.645888
8.244984	557.270026	9.650906
7.552503	560.613133	9.655923
7.544885	548.835437	9.660941
7.433935	552.910743	9.665959
7.781824	555.146941	9.670976
7.979809	560.390476	9.675994
7.909465	557.697810	9.681011
7.880238	564.972445	9.686029
8.144257	558.986685	9.691047
7.781833	567.151673	9.696064
8.139025	553.701268	9.701082
7.653492	558.020517	9.706099
8.007782	562.019475	9.711117
7.763011	553.009308	9.716135
7.588961	559.094143	9.721152
7.942612	553.237764	9.726170
7.858460	553.320578	9.731187
7.789781	562.111284	9.736205
7.856416	559.122841	9.741223
7.726040	587.855958	9.746240
8.184943	578.201097	9.751258
7.850868	595.942264	9.756275
7.937105	595.724731	9.761293
8.358134	589.017644	9.766311
8.008683	584.529398	9.771328
8.259288	566.077640	9.776346
7.778565	564.381650	9.781363
7.856512	564.308397	9.786381
8.157798	572.530962	9.791399
8.023948	580.421960	9.796416
8.052560	573.283890	9.801434
7.906743	567.789246	9.806451
7.911997	583.943419	9.811469
7.914843	590.694078	9.816487
8.081330	595.591709	9.821504
8.278793	587.619138	9.826522
7.912480	596.264077	9.831539
8.028972	587.771546	9.836557
8.300732	593.297292	9.841575
8.199805	597.465424	9.846592
8.293733	593.873472	9.851610
8.347354	593.730449	9.856627
8.023581	576.440402	9.861645
8.115012	569.310199	9.866663
7.893818	582.197964	9.871680
8.081401	581.873829	9.876698
8.019083	591.213841	9.881715
8.245656	584.023965	9.886733
8.032278	593.665836	9.891751
8.203507	596.790388	9.896768
8.012895	593.267582	9.901786
8.294249	597.627660	9.906803
7.824999	600.514216	9.911821
8.023648	590.743566	9.916839
7.792411	604.524677	9.921856
8.219192	585.599160	9.926874
8.309780	598.528413	9.931891
8.170845	588.655230	9.936909
8.246868	594.045220	9.941927
8.011128	597.456102	9.946944
8.371972	602.351150	9.951962
8.298334	595.416666	9.956979
8.384929	592.110752	9.961997
8.564930	596.906342	9.967015
8.414131	596.732737	9.972032
8.302161	584.205299	9.977050
8.272055	590.901992	9.982067
8.183367	599.766905	9.987085
7.947754	602.666393	9.992103
8.454988	602.239129	9.997120
7.995898	597.689976	10.002138
8.209952	596.096784	10.007155
8.440770	590.433039	10.012173
8.192533	594.950825	10.017191
8.149175	592.119427	10.022208
8.367774	590.642793	10.027226
8.458562	596.265938	10.032243
8.523024	602.618204	10.037261
8.573410	598.144588	10.042279
8.502734	606.460100	10.047296
8.156580	599.841165	10.052314
8.553939	602.257320	10.057331
8.245913	591.989247	10.062349
8.603795	592.457207	10.067367
8.332694	598.826671	10.072384
8.234960	598.476543	10.077402
8.338754	602.856492	10.082419
8.707149	611.273024	10.087437
8.664202	605.272528	10.092455
8.352973	597.628386	10.097472
8.314517	607.106555	10.102490
8.527836	606.308692	10.107507
8.403739	613.430236	10.112525
8.907341	612.140655	10.117543
8.588544	600.999833	10.122560
8.622285	600.097186	10.127578
8.612744	605.877158	10.132595
7.992606	599.252786	10.137613
8.387543	598.652472	10.142631
8.695554	619.289439	10.147648
8.602490	618.867084	10.152666
8.314753	620.198205	10.157683
8.720372	629.201030	10.162701
8.759756	621.659409	10.167719
8.342185	624.557063	10.172736
8.590290	623.582172	10.177754
8.780391	625.491488	10.182771
8.291901	628.877270	10.187789
8.943065	622.399215	10.192807
8.685930	626.707287	10.197824
8.740757	619.643375	10.202842
8.237549	621.769896	10.207859
8.492779	628.464644	10.212877
8.361897	617.531137	10.217895
8.272798	625.746187	10.222912
8.535273	627.192526	10.227930
8.630129	625.059151	10.232947
8.569657	635.742866	10.237965
8.425696	620.430985	10.242983
8.499624	629.632634	10.248000
8.500623	627.084974	10.253018
8.524075	628.081715	10.258035
8.461728	640.013279	10.263053
9.060628	650.963946	10.268071
8.986643	643.280542	10.273088
8.608871	625.990362	10.278106
8.982736	625.483502	10.283123
8.547042	629.735043	10.288141
8.933884	618.478882	10.293159
9.129389	621.434851	10.298176
8.834552	626.518023	10.303194
8.801581	628.960245	10.308211
8.618054	630.300618	10.313229
8.786796	626.688940	10.318247
8.581784	622.380790	10.323264
8.939424	626.082186	10.328282
8.856746	628.068339	10.333299
8.773569	639.726223	10.338317
9.029432	629.862581	10.343335
8.703542	635.836082	10.348352
9.072800	647.085329	10.353370
9.051517	628.315729	10.358387
8.575880	624.958788	10.363405
8.970469	630.617464	10.368423
8.748082	635.443932	10.373440
9.186357	645.587307	10.378458
8.745138	638.470616	10.383475
8.964148	656.429931	10.388493
9.226302	645.312972	10.393511
8.947345	638.115574	10.398528
8.885214	631.573419	10.403546
9.066630	627.223671	10.408563
8.707088	631.019283	10.413581
8.818461	639.515755	10.418599
9.168063	650.940306	10.423616
8.826240	652.082995	10.428634
9.481017	653.505069	10.433651
9.088685	643.628700	10.438669
8.789371	630.028519	10.443687
8.852125	638.649598	10.448704
8.882003	654.425372	10.453722
9.222993	663.617292	10.458739
9.120509	666.960373	10.463757
9.448025	653.271922	10.468775
8.711232	642.566072	10.473792
8.812044	647.644898	10.478810
9.390663	651.442234	10.483827
9.058928	657.356090	10.488845
9.324561	657.203217	10.493863
8.976641	648.800643	10.498880
9.280630	643.699670	10.503898
9.080783	638.885974	10.508915
8.729331	643.158157	10.513933
9.251455	657.738423	10.518951
9.124903	652.024225	10.523968
8.882071	664.269645	10.528986
9.350987	663.007083	10.534003
9.252101	660.261865	10.539021
9.553757	657.422117	10.544039
9.379189	639.775335	10.549056
8.872375	639.404433	10.554074
9.072358	638.120046	10.559091
9.174896	648.225734	10.564109
9.417887	651.180114	10.569127
9.265131	652.377983	10.574144
9.045732	656.177665	10.579162
9.183047	649.245293	10.584179
9.151114	653.297649	10.589197
9.165899	659.150363	10.594215
9.350733	653.441684	10.599232
9.275332	664.140300	10.604250
9.131513	648.931705	10.609267
9.105679	660.615898	10.614285
9.247011	651.418472	10.619303
9.378034	655.611444	10.624320
9.126186	649.999170	10.629338
9.418645	647.722128	10.634355
9.558131	650.234891	10.639373
9.177005	649.485448	10.644391
9.338757	646.595735	10.649408
9.080078	657.699782	10.654426
9.442153	650.862715	10.659443
9.389661	656.140044	10.664461
9.291805	639.736905	10.669479
9.480646	652.789624	10.674496
9.345165	656.782625	10.679514
9.621267	643.316490	10.684531
9.333487	660.310332	10.689549
9.448962	657.817057	10.694567
9.461149	659.009555	10.699584
9.359654	654.487552	10.704602
9.167954	646.244823	10.709619
9.601203	651.907907	10.714637
9.698998	649.142792	10.719655
9.620367	648.180678	10.724672
9.238271	661.316301	10.729690
9.507683	650.343592	10.734707
9.218657	652.671700	10.739725
9.332397	656.946673	10.744743
9.755556	650.200429	10.749760
9.146643	649.483337	10.754778
9.475648	661.873447	10.759795
9.704297	667.775254	10.764813
9.887345	670.504187	10.769831
9.526587	659.585634	10.774848
9.533930	663.342511	10.779866
9.647954	657.636743	10.784883
9.622602	652.991463	10.789901
9.398144	650.766489	10.794919
9.678772	646.996061	10.799936
9.499693	660.697888	10.804954
9.460300	662.682558	10.809971
9.726054	680.493591	10.814989
9.647769	668.819473	10.820007
9.846526	679.900644	10.825024
9.713231	678.671850	10.830042
9.743871	682.149487	10.835059
9.567948	673.559660	10.840077
9.785809	676.389689	10.845095
9.787585	665.022319	10.850112
9.285272	672.793326	10.855130
9.873526	664.221548	10.860147
9.918047	664.814230	10.865165
9.489535	665.184188	10.870183
10.157413	663.633063	10.875200
9.807160	664.492925	10.880218
9.882948	661.326774	10.885235
9.582649	660.676484	10.890253
9.708779	664.006955	10.895271
9.985293	664.879160	10.900288
10.002208	670.051657	10.905306
9.738692	661.104576	10.910323
9.497766	655.497571	10.915341
9.725780	666.182366	10.920359
9.840891	663.286624	10.925376
9.829360	667.625924	10.930394
9.815672	670.139547	10.935411
9.767908	679.394325	10.940429
9.856562	687.933180	10.945447
10.350271	678.079771	10.950464
10.069929	675.206654	10.955482
10.106813	674.953823	10.960499
9.967028	653.951312	10.965517
9.742462	651.889137	10.970535
9.881995	658.788548	10.975552
10.066499	667.906884	10.980570
9.971815	671.211862	10.985587
10.105193	658.466627	10.990605
10.020031	663.260255	10.995623
10.061881	658.030620	11.000640
9.861416	657.655445	11.005658
9.621970	660.630181	11.010675
9.893757	663.252440	11.015693
9.826015	677.307792	11.020711
9.735817	671.269066	11.025728
9.992785	686.474490	11.030746
9.966510	671.766569	11.035763
10.372649	674.893621	11.040781
9.657833	674.498439	11.045799
9.891258	675.075862	11.050816
9.883403	680.848889	11.055834
10.010237	678.656062	11.060851
10.068008	670.952318	11.065869
10.190109	676.248857	11.070887
10.007446	677.233606	11.075904
9.976890	682.700393	11.080922
9.860203	673.817868	11.085939
9.817469	676.724872	11.090957
9.993394	694.067623	11.095975
10.365935	696.525908	11.100992
10.143644	704.705664	11.106010
10.537518	695.853801	11.111027
10.139642	683.549187	11.116045
9.756390	674.875525	11.121063
10.520239	685.821238	11.126080
10.236214	684.388185	11.131098
10.471449	686.999990	11.136115
10.341263	673.100813	11.141133
10.079023	677.182403	11.146151
9.976873	672.378243	11.151168
9.959137	682.935605	11.156186
10.281593	692.515238	11.161203
10.050543	703.142715	11.166221
9.983200	701.632111	11.171239
10.510964	701.941728	11.176256
10.296950	700.764929	11.181274
10.006200	705.383901	11.186291
10.341300	707.586031	11.191309
10.157017	710.069557	11.196327
10.370782	701.913720	11.201344
10.568620	705.475373	11.206362
10.665602	702.032286	11.211379
10.589431	697.343082	11.216397
10.368131	701.791269	11.221415
10.541991	705.389582	11.226432
10.240812	708.300775	11.231450
10.414342	700.619110	11.236467
10.611134	700.989845	11.241485
10.505961	707.769533	11.246503
10.384630	710.061704	11.251520
10.307799	701.277649	11.256538
10.315730	704.461648	11.261555
10.635233	695.595575	11.266573
10.529007	702.379176	11.271591
10.584509	695.885349	11.276608
10.545493	712.897342	11.281626
10.260547	707.766102	11.286643
10.302984	702.603279	11.291661
10.430415	709.056727	11.296679
10.268299	700.875779	11.301696
10.195616	709.047400	11.306714
10.069237	711.346315	11.311731
10.554442	706.738978	11.316749
10.668836	724.987197	11.321767
10.365215	725.229515	11.326784
10.729321	735.057744	11.331802
10.777744	726.873870	11.336819
10.892510	709.219463	11.341837
10.477452	708.304016	11.346855
10.708775	706.973276	11.351872
10.667876	703.917056	11.356890
10.328012	704.952739	11.361907
10.259244	709.739128	11.366925
10.477613	729.945509	11.371943
10.942595	726.692213	11.376960
11.042771	731.462337	11.381978
10.842778	732.280101	11.386995
11.076996	732.613712	11.392013
10.912374	723.134842	11.397031
10.999289	705.338229	11.402048
10.957622	705.674001	11.407066
10.531040	703.116897	11.412083
10.877988	701.693321	11.417101
10.429057	699.889087	11.422119
10.754398	690.136289	11.427136
10.595106	697.732976	11.432154
10.679220	722.702437	11.437171
11.128585	715.094197	11.442189
10.539352	714.796633	11.447207
10.415193	715.960622	11.452224
10.823451	722.562853	11.457242
10.897465	731.635818	11.462259
11.086749	721.415693	11.467277
11.060769	733.957971	11.472295
11.221223	731.446185	11.477312
11.144781	721.434981	11.482330
10.649955	708.622486	11.487347
10.996694	705.289053	11.492365
10.874321	708.839962	11.497383
11.075469	712.479996	11.502400
11.061954	695.630529	11.507418
10.819190	708.404277	11.512435
10.918280	697.629322	11.517453
10.804125	707.193948	11.522471
10.870090	719.229629	11.527488
11.259504	720.639524	11.532506
11.499945	727.143875	11.537523
11.253321	702.469377	11.542541
11.091263	706.297333	11.547559
10.824502	693.669365	11.552576
11.011653	694.322389	11.557594
10.986040	696.120141	11.562611
11.364547	693.681557	11.567629
11.059670	699.010301	11.572647
10.953231	695.927775	11.577664
11.034347	692.966228	11.582682
10.760746	698.980270	11.587699
11.168026	701.971322	11.592717
10.994112	714.212608	11.597735
11.155635	718.995562	11.602752
11.335538	727.127371	11.607770
11.263380	729.728670	11.612787
11.100527	709.929433	11.617805
10.974664	720.996882	11.622823
11.230297	720.399839	11.627840
11.587174	725.583950	11.632858
11.375630	722.890319	11.637875
11.210639	698.370946	11.642893
10.976875	708.333378	11.647911
11.141605	711.758814	11.652928
11.516942	720.490369	11.657946
11.181990	729.362829	11.662963
11.403025	720.700103	11.667981
11.349418	716.841331	11.672999
11.207245	709.324138	11.678016
11.412290	707.696017	11.683034
11.254306	720.313962	11.688051
11.264385	724.064887	11.693069
11.507527	725.840606	11.698087
11.526642	731.499925	11.703104
11.513847	715.787041	11.708122
11.392068	706.340427	11.713139
11.056125	704.617009	11.718157
11.367717	703.917168	11.723175
11.237889	728.632657	11.728192
11.670761	722.776825	11.733210
11.328091	731.564355	11.738227
11.491796	729.219734	11.743245
11.585976	727.475994	11.748263
11.301223	726.507984	11.753280
11.559985	724.037138	11.758298
11.563871	731.121912	11.763315
11.404878	723.939373	11.768333
11.431364	723.842391	11.773351
11.574449	729.818676	11.778368
11.646958	725.254738	11.783386
11.549513	731.467053	11.788403
11.557878	727.626321	11.793421
11.643824	723.714430	11.798439
11.285699	719.625194	11.803456
11.346328	726.692660	11.808474
11.413136	732.994397	11.813491
11.215745	725.412562	11.818509
11.269900	728.599315	11.823527
11.299584	730.024324	11.828544
11.446070	726.709804	11.833562
11.319581	728.220021	11.838579
11.398323	716.756952	11.843597
11.840874	733.484802	11.848615
11.475690	723.535173	11.853632
11.673982	723.863733	11.858650
11.542014	746.727188	11.863667
11.922292	751.158459	11.868685
12.199174	755.298869	11.873703
11.548645	738.669799	11.878720
11.601081	727.589216	11.883738
11.830528	729.421538	11.888755
11.596701	722.922647	11.893773
11.716087	739.656981	11.898791
11.590920	753.489878	11.903808
12.249640	763.915957	11.908826
11.863503	748.463312	11.913843
11.959430	737.070397	11.918861
11.686089	733.772908	11.923879
11.427999	730.608505	11.928896
12.134266	739.350216	11.933914
11.957706	750.187155	11.938931
12.127340	738.542241	11.943949
11.789394	733.166279	11.948967
11.400399	725.229707	11.953984
12.040527	739.629031	11.959002
12.018297	751.582358	11.964019
12.030213	768.468238	11.969037
12.110164	752.627113	11.974055
11.942430	743.087729	11.979072
11.765226	731.660303	11.984090
11.727946	750.180202	11.989107
12.041076	756.067804	11.994125
12.393646	749.314157	11.999143
11.945698	741.558034	12.004160
12.353276	739.327586	12.009178
11.964421	734.678535	12.014195
11.728279	732.961752	12.019213
12.011540	737.942372	12.024231
11.791823	757.500010	12.029248
12.263173	746.512366	12.034266
12.204732	764.939745	12.039283
12.215676	764.514662	12.044301
12.232942	762.788822	12.049319
11.856840	758.237833	12.054336
12.222733	748.807761	12.059354
11.806622	755.530896	12.064371
12.257324	763.413003	12.069389
11.899736	752.139946	12.074407
11.986177	753.526786	12.079424
11.873495	754.491640	12.084442
11.882801	760.050836	12.089459
11.640338	758.041225	12.094477
11.888132	762.637816	12.099495
11.688791	758.645001	12.104512
12.323817	775.045846	12.109530
12.603535	782.848912	12.114547
12.336037	782.158914	12.119565
12.392701	773.904950	12.124583
12.158503	766.376060	12.129600
12.339549	772.460216	12.134618
12.296664	764.770598	12.139635
12.016603	760.829977	12.144653
12.398081	772.357973	12.149671
12.608896	784.595005	12.154688
12.626323	780.396480	12.159706
12.287757	771.182697	12.164723
12.180134	763.525492	12.169741
12.265974	767.734864	12.174759
12.032515	770.546236	12.179776
12.599333	783.325228	12.184794
12.534008	790.533927	12.189811
12.206160	776.860806	12.194829
12.521142	784.400550	12.199847
12.020980	788.580374	12.204864
11.965685	782.503915	12.209882
12.124954	788.155508	12.214899
12.512154	787.511398	12.219917
12.470863	784.093640	12.224935
12.461978	785.059548	12.229952
12.606703	781.548079	12.234970
12.404612	786.178714	12.239987
12.132732	774.618580	12.245005
12.575771	788.698767	12.250023
12.598526	786.934219	12.255040
12.895367	778.026200	12.260058
12.455384	793.219635	12.265075
12.402775	790.075982	12.270093
12.715238	793.154461	12.275111
12.823686	788.895728	12.280128
12.641522	786.892034	12.285146
12.561310	773.042527	12.290163
12.689271	792.384357	12.295181
13.051427	784.163460	12.300199
12.807814	783.893477	12.305216
12.948983	784.179963	12.310234
12.745132	780.970118	12.315251
12.771887	793.200354	12.320269
12.857164	778.841281	12.325287
12.802084	780.079022	12.330304
12.875054	779.273183	12.335322
12.908451	786.215686	12.340339
12.469272	782.680811	12.345357
12.798855	786.880772	12.350375
12.453535	787.581367	12.355392
12.610470	779.578823	12.360410
12.929458	779.139738	12.365427
12.744256	796.382997	12.370445
12.943653	783.259783	12.375463
12.836449	783.881627	12.380480
12.631705	781.389202	12.385498
12.895969	796.690760	12.390515
13.057076	811.655961	12.395533
13.442052	803.879653	12.400551
12.914706	793.211909	12.405568
12.753305	782.990787	12.410586
12.705257	792.993854	12.415603
13.059570	807.160258	12.420621
13.008852	801.788099	12.425639
13.141064	812.144653	12.430656
13.280421	797.347667	12.435674
13.130190	786.754240	12.440691
12.828426	783.222113	12.445709
12.957039	787.888519	12.450727
12.722196	782.289904	12.455744
13.260460	797.584497	12.460762
13.445224	804.087113	12.465779
13.018507	793.128645	12.470797
12.478349	792.323745	12.475815
12.979662	799.613642	12.480832
13.157662	810.314920	12.485850
13.048698	808.510261	12.490867
13.015949	819.527856	12.495885
13.406679	818.951658	12.500903
13.305142	817.990388	12.505920
13.360314	817.728610	12.510938
12.970554	815.402751	12.515955
13.115962	815.951506	12.520973
12.818505	811.304955	12.525991
13.076084	817.316175	12.531008
13.009607	816.082562	12.536026
13.243209	808.121193	12.541043
13.203138	826.412135	12.546061
13.163311	811.224281	12.551079
13.191088	822.225322	12.556096
13.630437	820.253344	12.561114
13.436720	815.376570	12.566131
12.964296	816.366188	12.571149
13.249093	811.701194	12.576167
13.190706	818.267065	12.581184
13.397789	814.510201	12.586202
13.325800	811.760288	12.591219
13.225546	821.271496	12.596237
13.069367	819.054831	12.601255
13.493876	834.791174	12.606272
13.753891	834.565420	12.611290
13.887593	824.835142	12.616307
13.569563	817.293785	12.621325
13.358770	821.098966	12.626343
13.578521	814.704550	12.631360
13.038080	811.461875	12.636378
13.660806	821.672929	12.641395
13.055698	821.856314	12.646413
13.248890	836.281991	12.651431
13.772722	846.384705	12.656448
13.674081	845.811509	12.661466
13.813109	843.612695	12.666483
13.649765	851.294770	12.671501
13.706761	848.269688	12.676519
13.888855	839.078957	12.681536
13.674212	831.843417	12.686554
13.710058	809.924553	12.691571
13.650787	820.695789	12.696589
13.673817	810.553630	12.701607
13.495781	816.620332	12.706624
13.560007	821.423426	12.711642
13.769999	825.994827	12.716659
13.729735	854.129641	12.721677
13.771138	840.347058	12.726695
13.877237	843.786402	12.731712
13.643244	844.857641	12.736730
13.827199	831.256278	12.741747
13.568401	845.078400	12.746765
13.630112	849.870702	12.751783
13.917232	850.600810	12.756800
13.939684	844.201582	12.761818
13.784896	847.833889	12.766835
13.954326	847.644451	12.771853
14.114585	846.704620	12.776871
13.768090	845.997437	12.781888
13.938813	847.986769	12.786906
14.024403	843.980426	12.791923
13.825415	851.865067	12.796941
14.009525	849.170602	12.801959
13.434444	851.611047	12.806976
13.996023	850.049033	12.811994
13.986187	846.407740	12.817011
14.058857	853.697264	12.822029
13.904491	856.692144	12.827047
13.992223	846.891742	12.832064
13.817102	848.223650	12.837082
14.048577	852.718658	12.842099
13.990829	853.222252	12.847117
14.107067	851.805518	12.852135
14.186979	849.715932	12.857152
13.822910	853.351337	12.862170
14.199673	847.196342	12.867187
13.973652	862.613317	12.872205
14.061663	849.525096	12.877223
14.028788	847.681015	12.882240
14.182989	853.690930	12.887258
14.329672	841.803708	12.892275
14.206644	842.523651	12.897293
14.268862	840.181907	12.902311
14.210078	841.299607	12.907328
13.796934	846.704267	12.912346
14.213280	851.251807	12.917363
14.201204	846.547573	12.922381
14.079050	843.396178	12.927399
14.054135	847.637366	12.932416
13.816329	849.709761	12.937434
14.447411	852.041047	12.942451
13.986171	850.089441	12.947469
14.144667	874.743261	12.952487
14.510553	868.196391	12.957504
14.543865	871.767321	12.962522
14.688820	869.820454	12.967539
14.694478	857.666129	12.972557
14.245745	855.864992	12.977575
14.651788	841.641901	12.982592
14.110875	851.524385	12.987610
14.564322	841.885426	12.992627
14.102053	844.675596	12.997645
14.518329	860.791656	13.002663
14.675542	869.880004	13.007680
14.365295	872.193562	13.012698
14.424110	872.141991	13.017715
14.348037	878.761612	13.022733
14.320512	875.178760	13.027751
14.758568	870.075506	13.032768
14.206451	884.518823	13.037786
14.357697	874.312990	13.042803
14.327813	875.259364	13.047821
14.349474	871.967334	13.052839
14.387527	867.398649	13.057856
14.404904	878.239264	13.062874
14.683678	879.200077	13.067891
14.618553	882.921418	13.072909
14.238651	887.623172	13.077927
14.499649	876.040129	13.082944
14.632099	910.868334	13.087962
14.707628	903.639445	13.092979
14.480383	908.175485	13.097997
14.487082	915.455533	13.103015
14.946669	907.656930	13.108032
14.548398	910.898649	13.113050
14.828852	904.221093	13.118067
14.664486	907.719975	13.123085
14.456394	908.705815	13.128103
14.798049	905.445425	13.133120
14.411382	917.211835	13.138138
14.522846	912.205174	13.143155
14.763244	898.724479	13.148173
14.811030	912.518927	13.153191
15.001140	911.242262	13.158208
14.440832	906.257114	13.163226
14.971240	926.458338	13.168243
15.302813	924.786134	13.173261
15.145285	921.426049	13.178279
14.998206	908.920718	13.183296
15.000310	905.335297	13.188314
15.125641	903.832801	13.193331
15.175221	906.313113	13.198349
15.052387	908.329597	13.203367
15.247204	887.823870	13.208384
15.377583	903.823728	13.213402
15.031578	897.595559	13.218419
15.120812	896.345505	13.223437
14.857703	907.144580	13.228455
15.377098	906.468257	13.233472
14.882755	908.187461	13.238490
15.079191	904.010325	13.243507
15.408550	894.550413	13.248525
15.266591	911.853734	13.253543
15.459934	904.405275	13.258560
15.229530	910.223253	13.263578
15.181511	901.398077	13.268595
15.345285	898.636910	13.273613
15.477038	896.000350	13.278631
15.741208	891.392300	13.283648
15.277434	898.050195	13.288666
15.266968	895.999443	13.293683
15.563747	901.201871	13.298701
15.078823	908.067996	13.303719
15.490435	894.007306	13.308736
15.382236	895.815463	13.313754
15.416653	899.940314	13.318771
15.498180	899.543453	13.323789
15.238862	901.096827	13.328807
15.439197	892.286276	13.333824
15.368802	897.306049	13.338842
15.617350	898.221891	13.343859
15.582725	899.347783	13.348877
15.243377	899.268503	13.353895
15.334740	881.422133	13.358912
15.263176	895.216524	13.363930
15.221871	891.181659	13.368947
15.452752	894.351471	13.373965
15.542715	892.315126	13.378983
15.785891	890.864692	13.384000
15.260216	895.800704	13.389018
15.253231	889.749635	13.394035
15.092429	890.396139	13.399053
15.105280	892.176301	13.404071
15.091200	894.645147	13.409088
15.284786	915.799530	13.414106
15.190614	924.054555	13.419123
15.330867	925.094298	13.424141
15.354491	933.791136	13.429159
15.757586	917.353250	13.434176
15.456993	930.824152	13.439194
15.170173	928.521319	13.444211
15.811647	931.032768	13.449229
16.013832	944.253190	13.454247
16.155199	932.781323	13.459264
15.732358	924.536121	13.464282
15.915820	924.099877	13.469299
16.054195	927.349635	13.474317
16.095942	931.511462	13.479335
15.875593	915.725205	13.484352
15.580051	919.949786	13.489370
16.067001	911.766342	13.494387
16.110766	919.874823	13.499405
15.843766	919.693759	13.504423
15.863859	915.913231	13.509440
16.009480	915.824594	13.514458
15.592382	912.249800	13.519475
16.370528	908.575932	13.524493
15.781507	921.619995	13.529511
16.021637	925.421307	13.534528
15.642089	919.392393	13.539546
15.875664	921.983453	13.544563
16.247017	917.665041	13.549581
16.044358	924.741719	13.554599
16.074874	920.768525	13.559616
16.036588	929.032372	13.564634
15.746314	926.230145	13.569651
16.167214	918.156096	13.574669
16.262136	932.801728	13.579687
16.101637	923.755093	13.584704
16.254645	921.070116	13.589722
16.035598	920.184669	13.594739
16.103768	911.691332	13.599757
15.684490	925.426429	13.604775
16.139662	936.738769	13.609792
15.892465	950.169711	13.614810
16.359045	953.430270	13.619827
16.446068	947.889897	13.624845
16.238952	946.755630	13.629863
16.293567	947.975741	13.634880
16.054419	942.526593	13.639898
16.516573	950.263988	13.644915
16.607202	944.354930	13.649933
16.583151	950.788977	13.654951
16.462802	941.079399	13.659968
16.804902	943.837452	13.664986
16.611708	936.890208	13.670003
16.485027	910.986657	13.675021
16.252400	910.938060	13.680039
16.381746	917.361948	13.685056
16.361407	928.041950	13.690074
16.548032	949.875446	13.695091
17.032274	933.383113	13.700109
16.426974	916.964822	13.705127
16.192588	922.129178	13.710144
16.753843	928.074217	13.715162
16.688712	928.620574	13.720179
16.315487	915.239106	13.725197
16.443119	927.124748	13.730215
16.515346	937.635442	13.735232
16.719576	934.705349	13.740250
16.848032	949.801301	13.745267
17.019523	931.847662	13.750285
16.263533	921.527656	13.755303
16.478334	924.228917	13.760320
16.853871	932.357055	13.765338
16.276781	937.190610	13.770355
17.004345	934.389263	13.775373
16.793812	944.480457	13.780391
16.887963	937.690949	13.785408
16.867302	938.988528	13.790426
16.632029	939.765516	13.795443
17.030495	936.075623	13.800461
16.790376	944.511208	13.805479
16.941389	930.842600	13.810496
16.835628	935.004933	13.815514
16.908897	939.161523	13.820531
17.139686	929.738839	13.825549
17.291025	939.772241	13.830567
16.748556	917.298607	13.835584
17.087728	923.218752	13.840602
16.795990	919.449115	13.845619
16.616644	909.030511	13.850637
17.198850	926.533141	13.855655
16.830820	936.796563	13.860672
16.824828	934.652548	13.865690
17.027117	945.808516	13.870707
16.964786	940.201246	13.875725
16.868425	942.856600	13.880743
17.012854	927.064418	13.885760
17.205315	934.645466	13.890778
17.163361	939.234175	13.895795
17.162561	929.541738	13.900813
17.083581	932.922896	13.905831
16.685044	936.243006	13.910848
17.329985	930.006790	13.915866
16.909668	944.357392	13.920883
16.970549	941.496399	13.925901
16.970472	930.708634	13.930919
16.858526	936.919898	13.935936
17.004276	951.600404	13.940954
16.769553	960.139819	13.945971
17.332829	965.891242	13.950989
17.128588	964.856883	13.956007
17.495314	968.189945	13.961024
17.666923	978.712493	13.966042
17.271240	977.067473	13.971059
17.446115	979.776168	13.976077
17.656344	975.399488	13.981095
17.261669	972.546500	13.986112
17.425589	974.979079	13.991130
17.422141	982.669875	13.996147
17.430121	982.279333	14.001165
17.411672	979.589777	14.006183
17.185550	978.277968	14.011200
17.480620	979.707311	14.016218
16.969808	980.900158	14.021235
17.256615	978.292925	14.026253
17.330906	975.169870	14.031271
17.389891	976.136516	14.036288
18.023645	990.038739	14.041306
17.572946	987.382451	14.046323
17.366646	984.055262	14.051341
17.702903	990.893186	14.056359
17.852687	1000.417467	14.061376
18.053692	998.237461	14.066394
17.819803	987.362544	14.071411
17.872829	970.296217	14.076429
17.865417	979.855669	14.081447
17.469980	975.609583	14.086464
17.589664	976.298045	14.091482
17.871627	980.077458	14.096499
17.454761	981.237367	14.101517
17.517718	987.329033	14.106535
17.527455	1005.606791	14.111552
18.187542	996.802825	14.116570
17.906572	1001.548992	14.121587
17.980719	991.322041	14.126605
18.079537	1006.434785	14.131623
17.987449	996.248061	14.136640
18.121072	993.645817	14.141658
17.809914	999.239471	14.146675
18.006387	1005.200296	14.151693
18.134446	1003.706391	14.156711
17.924604	1005.426344	14.161728
17.998732	996.183195	14.166746
18.404153	1002.973411	14.171763
18.207638	994.370097	14.176781
18.027228	977.283513	14.181799
17.856065	980.889834	14.186816
18.215421	982.656108	14.191834
18.141337	995.174508	14.196851
18.200245	993.710602	14.201869
18.046169	982.570468	14.206887
17.726944	985.424282	14.211904
17.546888	988.813986	14.216922
18.082505	995.726643	14.221939
18.037148	1001.968201	14.226957
18.219413	994.754597	14.231975
18.054057	999.749640	14.236992
17.945540	996.943957	14.242010
17.822661	1008.577224	14.247027
18.256432	1023.670133	14.252045
18.724250	1018.377445	14.257063
18.425010	1022.467637	14.262080
18.485667	997.023326	14.267098
18.580002	1003.647547	14.272115
18.573626	999.538741	14.277133
18.210492	990.598972	14.282151
18.315863	997.057586	14.287168
18.667876	990.849172	14.292186
18.517685	996.744396	14.297203
18.429234	994.099543	14.302221
18.594256	992.634927	14.307239
18.218776	1002.084717	14.312256
18.656089	1001.942870	14.317274
18.389533	1008.087348	14.322291
18.598559	1017.634467	14.327309
18.922368	1022.322630	14.332327
18.748400	1008.846940	14.337344
18.512713	995.600799	14.342362
18.695301	995.856390	14.347379
18.732814	1002.614064	14.352397
18.821191	988.337348	14.357415
18.830290	987.843476	14.362432
18.971908	986.819339	14.367450
18.902064	992.275641	14.372467
19.019156	996.574953	14.377485
18.906125	984.689455	14.382503
18.815289	990.433874	14.387520
18.713599	991.610682	14.392538
19.075792	991.310859	14.397555
18.825137	993.739128	14.402573
18.817254	986.183141	14.407591
18.734303	991.442026	14.412608
18.731931	992.089757	14.417626
18.987161	993.076537	14.422643
18.596426	994.437997	14.427661
18.815759	985.820286	14.432679
18.634863	1009.584138	14.437696
19.197575	1007.604229	14.442714
19.233661	1015.250677	14.447731
18.910392	1021.044372	14.452749
19.440746	1011.102974	14.457767
18.999049	1007.856244	14.462784
18.900681	991.265033	14.467802
19.527980	995.853925	14.472819
19.163100	1008.341149	14.477837
19.017458	991.742048	14.482855
18.895691	997.869148	14.487872
18.805018	1011.325304	14.492890
18.985390	1022.581422	14.497907
18.835506	1028.010884	14.502925
19.026614	1015.039041	14.507943
18.916579	1030.769955	14.512960
18.768134	1015.235802	14.517978
19.037536	1019.900332	14.522995
18.799414	1027.217977	14.528013
19.568904	1038.590344	14.533031
19.444383	1052.710393	14.538048
19.738732	1047.914221	14.543066
19.412098	1035.245730	14.548083
19.325797	1026.158750	14.553101
19.290337	1017.723524	14.558119
19.205448	1034.832466	14.563136
19.488637	1044.397982	14.568154
19.710651	1046.365429	14.573171
19.419286	1046.480129	14.578189
19.662086	1049.747199	14.583207
19.701180	1050.606139	14.588224
19.835162	1033.136150	14.593242
19.541014	1020.275275	14.598259
19.075123	1024.713623	14.603277
19.677817	1030.925028	14.608295
19.523720	1043.054820	14.613312
19.709109	1051.167387	14.618330
19.788536	1046.632124	14.623347
19.304451	1056.667290	14.628365
19.740290	1043.163432	14.633383
19.598214	1047.266481	14.638400
19.571130	1045.880246	14.643418
19.872308	1049.521450	14.648435
19.753668	1060.459994	14.653453
19.609283	1048.643042	14.658471
19.627555	1056.535371	14.663488
19.663455	1049.181907	14.668506
19.722243	1047.581802	14.673523
19.811719	1055.838653	14.678541
19.944407	1053.381823	14.683559
19.647001	1059.465704	14.688576
19.794520	1053.640844	14.693594
19.998525	1039.914909	14.698611
19.593455	1053.440288	14.703629
19.731487	1056.895631	14.708647
19.685358	1073.221445	14.713664
20.351367	1074.879674	14.718682
20.153019	1080.828995	14.723699
19.938421	1072.558547	14.728717
20.484604	1086.396284	14.733735
20.401620	1084.062695	14.738752
20.270663	1063.678206	14.743770
20.358719	1055.938924	14.748787
19.922189	1053.136182	14.753805
20.245533	1051.211409	14.758823
19.862058	1047.935702	14.763840
20.003359	1066.495977	14.768858
20.464158	1071.527900	14.773875
20.622950	1081.097974	14.778893
20.302612	1067.164699	14.783911
20.185938	1055.702958	14.788928
19.987275	1068.817290	14.793946
19.956668	1074.677706	14.798963
20.000684	1075.401978	14.803981
20.138691	1074.120575	14.808999
20.414415	1085.129405	14.814016
20.171361	1082.405122	14.819034
20.536186	1072.392387	14.824051
20.297240	1086.048047	14.829069
20.220638	1082.640619	14.834087
20.344109	1078.550364	14.839104
20.243263	1091.500826	14.844122
20.490484	1076.290194	14.849139
20.277853	1094.329048	14.854157
20.617663	1089.106038	14.859175
20.641284	1096.854593	14.864192
20.967391	1095.202176	14.869210
20.840765	1073.031221	14.874227
20.835878	1083.539479	14.879245
20.680528	1070.503530	14.884263
20.695867	1086.344363	14.889280
20.796918	1078.654088	14.894298
20.775112	1069.906737	14.899315
20.342059	1077.116657	14.904333
20.180153	1074.971768	14.909351
20.820318	1088.089986	14.914368
20.690064	1097.204993	14.919386
20.932812	1090.363949	14.924403
20.830177	1097.429197	14.929421
20.854467	1095.886000	14.934439
21.046330	1099.602470	14.939456
20.739890	1088.807647	14.944474
21.044145	1092.566847	14.949491
20.981176	1104.161489	14.954509
21.039766	1098.723422	14.959527
21.126529	1084.665772	14.964544
21.102561	1097.021995	14.969562
20.856601	1093.605710	14.974579
20.755073	1097.082379	14.979597
20.991023	1094.811517	14.984615
20.848509	1088.116003	14.989632
20.843549	1100.964713	14.994650
20.659977	1092.802871	14.999667
21.097044	1089.541937	15.004685
21.101912	1086.542597	15.009703
21.087146	1086.230632	15.014720
21.159395	1091.936170	15.019738
21.203630	1091.691953	15.024755
20.951595	1098.116715	15.029773
21.345886	1111.275035	15.034791
21.283695	1112.776372	15.039808
21.619627	1128.714345	15.044826
21.633190	1100.123913	15.049843
21.582952	1104.846718	15.054861
21.200258	1098.153723	15.059879
21.287763	1100.482888	15.064896
20.960119	1100.801640	15.069914
21.468091	1109.182254	15.074931
21.611051	1127.777364	15.079949
21.708592	1126.362533	15.084967
21.643031	1117.686991	15.089984
21.624477	1118.020111	15.095002
21.793162	1095.092987	15.100019
21.396313	1106.343148	15.105037
21.386791	1092.355430	15.110055
21.486858	1113.220133	15.115072
21.360536	1121.788072	15.120090
21.496173	1124.098217	15.125107
21.566205	1125.521674	15.130125
21.602816	1125.050389	15.135143
21.846569	1126.877626	15.140160
21.368772	1130.878634	15.145178
21.602420	1129.868323	15.150195
21.866349	1126.914886	15.155213
21.566251	1123.381221	15.160231
21.862686	1129.121159	15.165248
21.875984	1127.677419	15.170266
21.768984	1119.704399	15.175283
21.584262	1122.198102	15.180301
21.793339	1126.260912	15.185319
21.562969	1122.463701	15.190336
21.568605	1137.085787	15.195354
22.261726	1141.930306	15.200371
22.350599	1142.505793	15.205389
22.220180	1128.308228	15.210407
22.158641	1119.907200	15.215424
22.170692	1120.989525	15.220442
22.025783	1119.831125	15.225459
21.873694	1113.315136	15.230477
22.004962	1112.695053	15.235495
22.024401	1116.272873	15.240512
22.036462	1117.341024	15.245530
22.427587	1126.384344	15.250547
22.049592	1108.112015	15.255565
22.072799	1120.627336	15.260583
22.154238	1133.420375	15.265600
21.867395	1148.009595	15.270618
22.294542	1141.316215	15.275635
22.259525	1152.585003	15.280653
22.184762	1150.211456	15.285671
22.531262	1144.727092	15.290688
22.621506	1148.956897	15.295706
22.611733	1141.715699	15.300723
22.784184	1141.099793	15.305741
22.326467	1140.781143	15.310759
22.409099	1145.081107	15.315776
22.409358	1142.699815	15.320794
22.366988	1145.368670	15.325811
22.670646	1150.036601	15.330829
22.596997	1138.969595	15.335847
22.998628	1147.379716	15.340864
22.636938	1149.611121	15.345882
22.485696	1132.258506	15.350899
22.686026	1133.974858	15.355917
22.347750	1137.344832	15.360935
22.501172	1143.593169	15.365952
22.607413	1139.184517	15.370970
22.821188	1141.225390	15.375987
22.604267	1150.159568	15.381005
22.545042	1148.121218	15.386023
22.924785	1138.435472	15.391040
22.673347	1138.221110	15.396058
22.613678	1147.361814	15.401075
22.773772	1147.958532	15.406093
22.870957	1152.495043	15.411111
22.799864	1142.013802	15.416128
22.802997	1148.648521	15.421146
22.650745	1140.786156	15.426163
22.677655	1139.412591	15.431181
22.687525	1145.073008	15.436199
23.027954	1157.704520	15.441216
23.174889	1173.145239	15.446234
23.021328	1178.409231	15.451251
22.902821	1182.139517	15.456269
22.992094	1179.880819	15.461287
23.368723	1178.735327	15.466304
22.808821	1186.464390	15.471322
23.183631	1178.204570	15.476339
23.256756	1180.991234	15.481357
23.062748	1184.180946	15.486375
23.271952	1179.458333	15.491392
22.559803	1176.534066	15.496410
22.938534	1188.439585	15.501427
23.242250	1179.967183	15.506445
22.762698	1183.756694	15.511463
23.024870	1180.920464	15.516480
23.288307	1197.817364	15.521498
23.688453	1201.157521	15.526515
23.907220	1192.770095	15.531533
23.208427	1192.847010	15.536551
23.396267	1181.014102	15.541568
23.340420	1178.314981	15.546586
23.130078	1192.562802	15.551603
23.640846	1192.259540	15.556621
23.343270	1209.734328	15.561639
23.482722	1198.944836	15.566656
23.525865	1204.178110	15.571674
23.862339	1202.108230	15.576691
24.057827	1203.203768	15.581709
23.442692	1197.828836	15.586727
23.535528	1195.266014	15.591744
23.621352	1203.010582	15.596762
23.344840	1197.166391	15.601779
23.284610	1204.927757	15.606797
23.826482	1196.340566	15.611815
23.941563	1197.006182	15.616832
23.396582	1201.229783	15.621850
23.873013	1196.917450	15.626867
23.648379	1192.383868	15.631885
23.572141	1199.248327	15.636903
23.795920	1199.505737	15.641920
24.003180	1183.401683	15.646938
23.942132	1199.088406	15.651955
24.040574	1196.310095	15.656973
23.961840	1191.672739	15.661991
24.169243	1192.226557	15.667008
24.083963	1192.413690	15.672026
24.036031	1193.004439	15.677043
24.017019	1193.076231	15.682061
24.347562	1214.003148	15.687079
24.710367	1200.377442	15.692096
24.523713	1197.198114	15.697114
24.083400	1194.699504	15.702131
24.428187	1187.676897	15.707149
24.284793	1186.768229	15.712167
24.188992	1190.797878	15.717184
24.509750	1188.346378	15.722202
24.084609	1187.374310	15.727219
24.486635	1184.047532	15.732237
24.324335	1203.187150	15.737255
24.159011	1181.063416	15.742272
24.262824	1184.792574	15.747290
24.465294	1200.143384	15.752307
24.474956	1194.658694	15.757325
24.519563	1191.941692	15.762343
24.092939	1191.943448	15.767360
24.074702	1203.259087	15.772378
24.258921	1211.240836	15.777395
24.782690	1212.575496	15.782413
24.746773	1226.162494	15.787431
24.486886	1213.911090	15.792448
24.701482	1227.764703	15.797466
24.652889	1222.989262	15.802483
24.676371	1220.759603	15.807501
24.629556	1219.975425	15.812519
24.777573	1223.272066	15.817536
24.729480	1232.701828	15.822554
24.561936	1219.990207	15.827571
24.847245	1221.262935	15.832589
24.544292	1227.779281	15.837607
24.434747	1218.883051	15.842624
24.802712	1223.228911	15.847642
24.400178	1222.388117	15.852659
24.985348	1216.019211	15.857677
24.900807	1220.817435	15.862695
24.766466	1219.244691	15.867712
24.908372	1233.393843	15.872730
25.059695	1240.913773	15.877747
25.160858	1237.198034	15.882765
25.339962	1241.151295	15.887783
25.034786	1229.384551	15.892800
25.293865	1222.006112	15.897818
25.045010	1209.276915	15.902835
25.224261	1212.052637	15.907853
25.389519	1214.060641	15.912871
25.483036	1213.970035	15.917888
24.885468	1202.666855	15.922906
24.749197	1221.847443	15.927923
25.481812	1226.729518	15.932941
25.572772	1239.745855	15.937959
25.205803	1244.872516	15.942976
25.707314	1240.138697	15.947994
25.424909	1232.074701	15.953011
25.305880	1214.624911	15.958029
25.484623	1227.085332	15.963047
25.238096	1223.882095	15.968064
25.341142	1237.371204	15.973082
25.519799	1243.912617	15.978099
25.558954	1232.265008	15.983117
25.471496	1243.710287	15.988135
25.605613	1246.737602	15.993152
25.535956	1236.943037	15.998170
24.827756	1238.527357	16.003187
25.338994	1238.793283	16.008205
25.278988	1242.393785	16.013223
25.147248	1240.700139	16.018240
25.189479	1256.231177	16.023258
25.695269	1266.663729	16.028275
26.129188	1265.006367	16.033293
25.830065	1271.764998	16.038311
26.037654	1275.543067	16.043328
25.975612	1269.493521	16.048346
26.259433	1275.890308	16.053363
25.944208	1263.744909	16.058381
26.223455	1270.705029	16.063399
25.891921	1255.888440	16.068416
26.073855	1246.959886	16.073434
25.949438	1259.322305	16.078451
26.021269	1260.887596	16.083469
26.180578	1264.906356	16.088487
26.207190	1267.487390	16.093504
26.095680	1258.703270	16.098522
26.251059	1266.447725	16.103539
26.549587	1260.751224	16.108557
25.888502	1251.117553	16.113575
26.102007	1256.439057	16.118592
26.549737	1266.015548	16.123610
26.110292	1256.142679	16.128627
26.284060	1256.720987	16.133645
26.515691	1263.553198	16.138663
26.371494	1259.081420	16.143680
26.505246	1249.927418	16.148698
26.296465	1251.933823	16.153715
26.436777	1256.718698	16.158733
26.291004	1261.640493	16.163751
26.262904	1256.060488	16.168768
26.396327	1263.322391	16.173786
26.255109	1264.527442	16.178803
26.525939	1265.774235	16.183821
26.364374	1274.883134	16.188839
26.191824	1269.434610	16.193856
26.432116	1258.048811	16.198874
26.394019	1270.799237	16.203891
26.478716	1259.874322	16.208909
26.500910	1268.195224	16.213927
26.343701	1262.425661	16.218944
26.918082	1274.325104	16.223962
26.593141	1291.543913	16.228979
27.041702	1286.172844	16.233997
27.232347	1288.243959	16.239015
26.855769	1277.040993	16.244032
27.320068	1257.058073	16.249050
26.922519	1267.759278	16.254067
27.028062	1258.682004	16.259085
26.857206	1251.939557	16.264103
26.864113	1252.220024	16.269120
26.988832	1247.200029	16.274138
26.701479	1255.863309	16.279155
27.199012	1265.759855	16.284173
27.044761	1257.099371	16.289191
27.254352	1274.083649	16.294208
27.318509	1253.210197	16.299226
27.054496	1264.078171	16.304243
26.923220	1259.133399	16.309261
27.176160	1261.379974	16.314279
27.245958	1275.895861	16.319296
27.069089	1266.164766	16.324314
27.163256	1285.786639	16.329331
26.934726	1275.686974	16.334349
27.491345	1280.114874	16.339367
27.325633	1281.814136	16.344384
27.286663	1279.330687	16.349402
27.335458	1276.321254	16.354419
27.242203	1268.849001	16.359437
27.538917	1273.542927	16.364455
27.394711	1272.268655	16.369472
27.522172	1269.144970	16.374490
27.240841	1269.956006	16.379507
27.337814	1266.858648	16.384525
27.651882	1279.009228	16.389543
27.395895	1300.323114	16.394560
28.013968	1298.561913	16.399578
27.661928	1299.846102	16.404595
27.764295	1308.316291	16.409613
28.269653	1304.132974	16.414631
27.522973	1292.683653	16.419648
27.593986	1289.121333	16.424666
27.949395	1294.990501	16.429683
27.858299	1294.434537	16.434701
27.981746	1300.577687	16.439719
28.053810	1304.020037	16.444736
27.934155	1304.707747	16.449754
28.091563	1310.654713	16.454771
27.901474	1299.301446	16.459789
28.057539	1296.458030	16.464807
28.000520	1293.621687	16.469824
28.176248	1294.416592	16.474842
27.743145	1299.127508	16.479859
27.926226	1303.108469	16.484877
27.976433	1289.680307	16.489895
27.815513	1309.909549	16.494912
28.489511	1305.241132	16.499930
28.281187	1308.462775	16.504947
27.753858	1305.341626	16.509965
28.359914	1303.959573	16.514983
28.184855	1302.626650	16.520000
28.480626	1292.515019	16.525018
28.246313	1292.766687	16.530035
28.208762	1302.778968	16.535053
28.510546	1288.333045	16.540071
28.581600	1302.858197	16.545088
28.439056	1293.650886	16.550106
28.292382	1308.533087	16.555123
28.474742	1318.065141	16.560141
28.755268	1330.733129	16.565159
28.688361	1336.193000	16.570176
28.675569	1329.068354	16.575194
28.541148	1333.343427	16.580211
28.617654	1331.965931	16.585229
28.816020	1336.988023	16.590247
29.055527	1338.259319	16.595264
28.650395	1320.325882	16.600282
28.798902	1315.244039	16.605299
28.615239	1323.126371	16.610317
28.816533	1324.348902	16.615335
28.628725	1323.866489	16.620352
28.747996	1325.829399	16.625370
29.053530	1324.488241	16.630387
28.836939	1331.955988	16.635405
29.149657	1324.186709	16.640423
29.087634	1323.518041	16.645440
28.904522	1318.466909	16.650458
28.767009	1322.969257	16.655475
29.089222	1325.967685	16.660493
28.966918	1314.748410	16.665511
28.789209	1323.798212	16.670528
29.090625	1314.687166	16.675546
29.306489	1312.300325	16.680563
29.070823	1317.785484	16.685581
29.224750	1313.407439	16.690599
28.897798	1323.478860	16.695616
29.541159	1339.447444	16.700634
29.721038	1347.010315	16.705651
29.577501	1337.396464	16.710669
29.642269	1317.826713	16.715687
29.345299	1313.672035	16.720704
29.604451	1316.382135	16.725722
29.523787	1319.759720	16.730739
29.519691	1319.518021	16.735757
29.671964	1311.915570	16.740775
29.634886	1313.888324	16.745792
29.557184	1307.682317	16.750810
29.619823	1315.537091	16.755827
29.687009	1338.469689	16.760845
29.963426	1326.483763	16.765863
29.622945	1330.943475	16.770880
29.659933	1320.989009	16.775898
29.791766	1341.808584	16.780915
29.795875	1357.471646	16.785933
30.100646	1328.952856	16.790951
29.983602	1353.701860	16.795968
30.008068	1347.754829	16.800986
29.992864	1342.055724	16.806003
29.943380	1351.361778	16.811021
30.070388	1350.201075	16.816039
29.738566	1357.460436	16.821056
29.911999	1345.815617	16.826074
30.268324	1345.210477	16.831091
29.772557	1348.383847	16.836109
30.036736	1347.936144	16.841127
30.474626	1341.552300	16.846144
30.290168	1346.180957	16.851162
30.055179	1345.542219	16.856179
30.081957	1355.515496	16.861197
30.514463	1352.195820	16.866215
30.040633	1349.830309	16.871232
30.030338	1347.519635	16.876250
30.701797	1347.348318	16.881267
30.420576	1348.303821	16.886285
30.279912	1333.062927	16.891303
30.353520	1347.857765	16.896320
30.280631	1354.100892	16.901338
30.211768	1341.189310	16.906355
30.372005	1342.852903	16.911373
30.607540	1346.007470	16.916391
30.644905	1347.898172	16.921408
30.707444	1354.630582	16.926426
30.945303	1360.313809	16.931443
30.784933	1357.735570	16.936461
30.909599	1350.571138	16.941479
31.032538	1346.343505	16.946496
30.690753	1344.178872	16.951514
30.815147	1340.292719	16.956531
30.540138	1347.118631	16.961549
30.776023	1338.916069	16.966567
30.975120	1362.257077	16.971584
30.948722	1360.782907	16.976602
31.129318	1369.489725	16.981619
30.803946	1371.113569	16.986637
31.258092	1369.394963	16.991655
31.018508	1366.483837	16.996672
31.032281	1370.051634	17.001690
31.015778	1368.868723	17.006707
31.012549	1365.402975	17.011725
31.439728	1356.467451	17.016743
31.304107	1367.333053	17.021760
31.060660	1360.403812	17.026778
30.860227	1355.804351	17.031795
30.647644	1368.657086	17.036813
30.826207	1361.658881	17.041831
30.982152	1365.050295	17.046848
31.089660	1386.749140	17.051866
31.381055	1383.275754	17.056883
31.347851	1392.431887	17.061901
31.481534	1388.481187	17.066919
31.817101	1395.133981	17.071936
31.642205	1396.415111	17.076954
31.968381	1388.959301	17.081971
31.574578	1393.012552	17.086989
31.763911	1384.343310	17.092007
31.979489	1388.444872	17.097024
31.905724	1388.373409	17.102042
32.060240	1376.738798	17.107059
31.764711	1380.583198	17.112077
31.945267	1371.522522	17.117095
31.698098	1370.549992	17.122112
31.714286	1381.602962	17.127130
31.838660	1378.067578	17.132147
31.795481	1386.416337	17.137165
32.021911	1381.080584	17.142183
32.165116	1394.543471	17.147200
32.042546	1395.186790	17.152218
32.424083	1383.770336	17.157235
31.985492	1386.590520	17.162253
32.094511	1380.211327	17.167271
32.193598	1388.561637	17.172288
31.963423	1387.311880	17.177306
31.965446	1386.077858	17.182323
31.954016	1386.440900	17.187341
32.256198	1379.042625	17.192359
32.116699	1382.729206	17.197376
31.826684	1389.682036	17.202394
32.272123	1392.563148	17.207411
31.882537	1395.639353	17.212429
32.285180	1404.142358	17.217447
32.231183	1407.550175	17.222464
32.319023	1421.160078	17.227482
32.676582	1417.737102	17.232499
32.464541	1415.437906	17.237517
32.424630	1418.517409	17.242535
32.779422	1413.238259	17.247552
32.712725	1414.236847	17.252570
32.933085	1405.682511	17.257587
32.809907	1417.116140	17.262605
32.882541	1416.514059	17.267623
32.796384	1413.565612	17.272640
32.548027	1418.211997	17.277658
33.077264	1408.436277	17.282675
32.680500	1415.380485	17.287693
32.703661	1410.773762	17.292711
32.766246	1410.751286	17.297728
32.621893	1407.781806	17.302746
32.956642	1404.851191	17.307763
32.597747	1405.999918	17.312781
32.839428	1397.299134	17.317799
33.224141	1425.647804	17.322816
33.230300	1431.837273	17.327834
33.035847	1427.724576	17.332851
33.563265	1436.308037	17.337869
33.504188	1423.850652	17.342887
33.537317	1407.325323	17.347904
33.226525	1400.861181	17.352922
33.426858	1400.682349	17.357939
33.441463	1404.263007	17.362957
33.362377	1401.426376	17.367975
33.463008	1396.931579	17.372992
33.335704	1400.925182	17.378010
33.467738	1401.705309	17.383027
33.514099	1403.976795	17.388045
33.382458	1428.550398	17.393063
33.856730	1429.780318	17.398080
33.862482	1434.359669	17.403098
33.720877	1410.030943	17.408115
33.802675	1406.370350	17.413133
33.426290	1410.773455	17.418151
33.618542	1418.379579	17.423168
33.580233	1437.498877	17.428186
33.931226	1429.382250	17.433203
34.237282	1436.178152	17.438221
33.665042	1433.573874	17.443239
34.024225	1430.241567	17.448256
34.047000	1437.365650	17.453274
33.842768	1435.968275	17.458291
34.127355	1431.035030	17.463309
33.931572	1434.348312	17.468327
34.051405	1420.181715	17.473344
33.995738	1437.582693	17.478362
34.294332	1432.123120	17.483379
33.976006	1427.836924	17.488397
33.851406	1428.688843	17.493415
34.168891	1424.855216	17.498432
34.291884	1431.691780	17.503450
34.346451	1431.401354	17.508467
34.004973	1433.537708	17.513485
33.995298	1431.560374	17.518503
34.276270	1440.384401	17.523520
34.518075	1441.368325	17.528538
34.939451	1444.740441	17.533555
34.724945	1443.625079	17.538573
34.619520	1445.034818	17.543591
34.953401	1435.464382	17.548608
34.616335	1427.730225	17.553626
34.731276	1415.883665	17.558643
34.682981	1415.744584	17.563661
34.547549	1420.588729	17.568679
34.897044	1409.650008	17.573696
34.673985	1417.991284	17.578714
34.897772	1436.725689	17.583731
34.927778	1438.305824	17.588749
34.906144	1444.258980	17.593767
35.106776	1432.485563	17.598784
35.024247	1434.545413	17.603802
35.305675	1421.347200	17.608819
35.197296	1417.360746	17.613837
34.953572	1421.669759	17.618855
34.964955	1418.033859	17.623872
34.968071	1417.053975	17.628890
35.021364	1426.017017	17.633907
35.288120	1431.228553	17.638925
34.887607	1429.198863	17.643943
35.403135	1434.791085	17.648960
35.044255	1442.277417	17.653978
35.192619	1432.326020	17.658995
35.106254	1444.655098	17.664013
35.083790	1445.816016	17.669031
35.397093	1436.541904	17.674048
35.052962	1438.873970	17.679066
35.002727	1442.629977	17.684083
35.064353	1460.300846	17.689101
35.373152	1467.083314	17.694119
35.378456	1462.470095	17.699136
35.451248	1467.679239	17.704154
35.467724	1468.426611	17.709171
35.631392	1460.442282	17.714189
35.418123	1471.142915	17.719207
35.793085	1471.926367	17.724224
35.997543	1485.242936	17.729242
35.954378	1475.421376	17.734259
36.091018	1457.444182	17.739277
36.101707	1465.049407	17.744295
36.152364	1464.951750	17.749312
36.034109	1464.465252	17.754330
36.211033	1463.460806	17.759347
35.927448	1458.113345	17.764365
35.916308	1464.724195	17.769383
36.119698	1449.091361	17.774400
36.299445	1474.058935	17.779418
36.045624	1481.563649	17.784435
36.394119	1478.830731	17.789453
36.285173	1487.164887	17.794471
36.615875	1483.372749	17.799488
36.404102	1490.211834	17.804506
36.753729	1482.580039	17.809523
36.494149	1461.556186	17.814541
36.671881	1454.871848	17.819559
36.537328	1446.281996	17.824576
36.272740	1450.041351	17.829594
36.562728	1469.408868	17.834611
37.055373	1465.740600	17.839629
36.382382	1461.347603	17.844647
36.842596	1462.557816	17.849664
36.978521	1472.092566	17.854682
36.381026	1465.073312	17.859699
36.854690	1464.371502	17.864717
36.718000	1477.806971	17.869735
36.883160	1472.658138	17.874752
37.160366	1474.458598	17.879770
37.290330	1472.010029	17.884787
37.279594	1469.410442	17.889805
36.937477	1458.814984	17.894823
36.806757	1461.612748	17.899840
36.944914	1464.263461	17.904858
36.892567	1468.353674	17.909875
37.173988	1465.677968	17.914893
36.704333	1477.655439	17.919911
36.867405	1473.123471	17.924928
36.828137	1476.500508	17.929946
37.049035	1478.919367	17.934963
37.353315	1475.360750	17.939981
36.973469	1474.807105	17.944999
37.052652	1484.981592	17.950016
37.478471	1501.053825	17.955034
37.183325	1503.986011	17.960051
37.518091	1497.539719	17.965069
37.262975	1508.915427	17.970087
37.596843	1510.199006	17.975104
37.505941	1510.933126	17.980122
37.446625	1509.343157	17.985139
37.715544	1500.139769	17.990157
37.399560	1511.398827	17.995175
37.297103	1501.622144	18.000192
37.686763	1515.805570	18.005210
37.568666	1533.546552	18.010227
37.938810	1530.812389	18.015245
37.941231	1532.158935	18.020263
38.391956	1526.737821	18.025280
38.354318	1528.281966	18.030298
38.147089	1535.238423	18.035315
38.532004	1523.498478	18.040333
38.333225	1511.284316	18.045351
38.233945	1495.100185	18.050368
38.009143	1489.837429	18.055386
37.955452	1499.784018	18.060403
38.377327	1499.546708	18.065421
38.575094	1518.548523	18.070439
38.726794	1503.227762	18.075456
38.357618	1485.546416	18.080474
38.038560	1492.865528	18.085491
38.493511	1501.420128	18.090509
38.524464	1518.760738	18.095527
38.611876	1514.557861	18.100544
38.685383	1517.412238	18.105562
38.175044	1522.887220	18.110579
38.776508	1523.107055	18.115597
38.573672	1523.406642	18.120615
38.099181	1523.919488	18.125632
38.777357	1521.899462	18.130650
38.750000	1528.561852	18.135667
38.665419	1520.992369	18.140685
38.804273	1522.907168	18.145703
38.685440	1530.936305	18.150720
38.644658	1518.138803	18.155738
38.929358	1522.281273	18.160755
39.268281	1533.104727	18.165773
39.048411	1529.282441	18.170791
39.196325	1526.067906	18.175808
39.407624	1522.338125	18.180826
38.945739	1519.032828	18.185843
39.486260	1524.348495	18.190861
39.443932	1519.624675	18.195879
39.022254	1510.801417	18.200896
39.503724	1517.707959	18.205914
39.309770	1539.573660	18.210931
39.613626	1538.255992	18.215949
39.550848	1543.183766	18.220967
39.518771	1539.485771	18.225984
39.608931	1524.433875	18.231002
39.533601	1520.040335	18.236019
39.707393	1519.647021	18.241037
39.239785	1525.647565	18.246055
39.426753	1534.266412	18.251072
40.239425	1536.077087	18.256090
39.796694	1542.273891	18.261107
39.660587	1542.722620	18.266125
39.865185	1540.869495	18.271143
39.978892	1536.628384	18.276160
40.057993	1532.281218	18.281178
39.749831	1534.550628	18.286195
39.951171	1543.045439	18.291213
39.652698	1534.454439	18.296231
39.950017	1535.082694	18.301248
39.877640	1528.762329	18.306266
39.684829	1538.706083	18.311283
40.016846	1540.891133	18.316301
39.825211	1537.909801	18.321319
39.801336	1540.252035	18.326336
40.404372	1555.610634	18.331354
40.157608	1562.285098	18.336371
40.429652	1564.273431	18.341389
40.296464	1571.441608	18.346407
39.911442	1570.440798	18.351424
40.297057	1562.742748	18.356442
40.042814	1571.833367	18.361459
40.440594	1565.444683	18.366477
40.682900	1568.868243	18.371495
40.554772	1584.609025	18.376512
40.796254	1590.237013	18.381530
40.731517	1594.630100	18.386547
41.108719	1591.083746	18.391565
41.037710	1590.968123	18.396583
40.870480	1567.246152	18.401600
41.296300	1556.267084	18.406618
41.006842	1555.983445	18.411635
41.150763	1548.951151	18.416653
41.044423	1555.560934	18.421671
40.972821	1555.071797	18.426688
41.049640	1543.994450	18.431706
40.903378	1555.688706	18.436723
41.115125	1575.483918	18.441741
41.670307	1581.840848	18.446759
41.240784	1583.303682	18.451776
41.670097	1571.490968	18.456794
41.118148	1579.816920	18.461811
41.245644	1578.884854	18.466829
41.367772	1588.631808	18.471847
41.090621	1593.901522	18.476864
41.324371	1586.091304	18.481882
41.202176	1596.026900	18.486899
41.187372	1587.489900	18.491917
41.378992	1588.427846	18.496935
41.384987	1594.865827	18.501952
41.904221	1594.873353	18.506970
41.846299	1614.731549	18.511987
41.835955	1609.309485	18.517005
42.011481	1613.616580	18.522023
41.569839	1615.927085	18.527040
42.033288	1613.531329	18.532058
41.986156	1614.493607	18.537075
41.972713	1605.169377	18.542093
42.170201	1599.126169	18.547111
42.078368	1609.546876	18.552128
42.400417	1599.775948	18.557146
41.898837	1604.700300	18.562163
42.219777	1608.390715	18.567181
42.717015	1601.927218	18.572199
42.600533	1607.663135	18.577216
42.634356	1591.680791	18.582234
42.525186	1592.706922	18.587251
42.592635	1569.079796	18.592269
42.799903	1568.917132	18.597287
42.373377	1569.338938	18.602304
42.639521	1568.490125	18.607322
42.479814	1573.169064	18.612339
42.343582	1570.300168	18.617357
42.447305	1575.139255	18.622375
42.427525	1586.560153	18.627392
42.536039	1591.781512	18.632410
42.517450	1603.310490	18.637427
42.539693	1607.739122	18.642445
42.846580	1599.608479	18.647463
42.332667	1596.469290	18.652480
42.833417	1599.012909	18.657498
42.478226	1601.523211	18.662515
42.786031	1613.972336	18.667533
43.059168	1618.449425	18.672551
43.064793	1627.997268	18.677568
43.166662	1621.953803	18.682586
43.110993	1628.526455	18.687603
43.068149	1632.861978	18.692621
42.993415	1621.195605	18.697639
42.796262	1636.439260	18.702656
43.068989	1618.930984	18.707674
43.258814	1640.103127	18.712691
43.033377	1652.030689	18.717709
43.531206	1647.542240	18.722727
43.488329	1646.195977	18.727744
43.626419	1646.408191	18.732762
43.584582	1640.303173	18.737779
43.516973	1657.005213	18.742797
44.249108	1644.906288	18.747815
43.879743	1652.011005	18.752832
44.219607	1642.000479	18.757850
44.185206	1644.687779	18.762867
43.922835	1647.298012	18.767885
44.103314	1647.924827	18.772903
43.883883	1646.929952	18.777920
44.197249	1648.092150	18.782938
44.404523	1651.744383	18.787955
43.941204	1646.769245	18.792973
44.111681	1649.496113	18.797991
43.872122	1644.608584	18.803008
43.764571	1642.225057	18.808026
43.842510	1637.730813	18.813043
43.978459	1648.512104	18.818061
44.323819	1654.057102	18.823079
44.420851	1666.487367	18.828096
44.852995	1662.816513	18.833114
45.049914	1666.874795	18.838131
44.661720	1645.189008	18.843149
44.830578	1634.767941	18.848167
44.946316	1633.821685	18.853184
44.789413	1625.970869	18.858202
44.748541	1630.821015	18.863219
44.736911	1637.535561	18.868237
44.904349	1626.398213	18.873255
44.833995	1633.568180	18.878272
44.772511	1626.342830	18.883290
44.876809	1624.898879	18.888307
44.859506	1633.841886	18.893325
45.056906	1640.674050	18.898343
45.185960	1657.127264	18.903360
45.047447	1653.572916	18.908378
45.242344	1654.008755	18.913395
45.239473	1662.418286	18.918413
45.559976	1656.272327	18.923431
45.531314	1655.677231	18.928448
45.274361	1640.204578	18.933466
45.263814	1639.865129	18.938483
45.114555	1649.089522	18.943501
45.152278	1646.940505	18.948519
45.336267	1654.351666	18.953536
45.241782	1652.548239	18.958554
45.107166	1652.642398	18.963571
45.177268	1665.118870	18.968589
45.611697	1657.668561	18.973607
45.958299	1678.530844	18.978624
45.840944	1682.721681	18.983642
45.636140	1664.337622	18.988659
45.718461	1680.908076	18.993677
45.878733	1677.128865	18.998695
46.111443	1674.086817	19.003712
46.040447	1678.407347	19.008730
46.133378	1674.127527	19.013747
45.960865	1684.512089	19.018765
46.052452	1682.585606	19.023783
46.009370	1684.415313	19.028800
45.655937	1683.932071	19.033818
46.006778	1685.635280	19.038835
45.899508	1690.466560	19.043853
46.433423	1692.451541	19.048871
46.332437	1708.776119	19.053888
45.773843	1717.276473	19.058906
46.321027	1706.160987	19.063923
46.335336	1710.829941	19.068941
46.277285	1713.687718	19.073959
46.398769	1705.948067	19.078976
46.345377	1718.940772	19.083994
46.894164	1725.778740	19.089011
47.062323	1735.843722	19.094029
47.348214	1730.241277	19.099047
47.416406	1706.447679	19.104064
47.170186	1707.824545	19.109082
47.166715	1698.991902	19.114099
46.970470	1699.798263	19.119117
47.315745	1693.062353	19.124135
47.064627	1691.671172	19.129152
47.072548	1685.639754	19.134170
47.328875	1693.944016	19.139187
47.349042	1687.827493	19.144205
47.455381	1683.611582	19.149223
47.411323	1689.149274	19.154240
47.244700	1692.836499	19.159258
47.348157	1694.898540	19.164275
47.075074	1700.676662	19.169293
47.584096	1717.138437	19.174311
47.494197	1720.484574	19.179328
47.448406	1731.513056	19.184346
47.851645	1723.885619	19.189363
47.790027	1725.458178	19.194381
47.753834	1722.262787	19.199399
47.591895	1715.669441	19.204416
47.833214	1715.826703	19.209434
47.703629	1720.075881	19.214451
47.574042	1720.825495	19.219469
47.829536	1717.020212	19.224487
48.067804	1718.935441	19.229504
47.880758	1726.500039	19.234522
48.202411	1731.039175	19.239539
48.110661	1745.150076	19.244557
48.582902	1748.884275	19.249575
48.844453	1746.411429	19.254592
48.395076	1734.940310	19.259610
48.672825	1709.200086	19.264627
48.528887	1720.228732	19.269645
48.221521	1709.485200	19.274663
48.743295	1708.223030	19.279680
48.339018	1703.888444	19.284698
48.459837	1719.766329	19.289715
49.076599	1722.973357	19.294733
48.739087	1724.788228	19.299751
48.629504	1714.650787	19.304768
48.879519	1729.021005	19.309786
49.205351	1724.682382	19.314803
48.788620	1727.433244	19.319821
49.800931	1720.103781	19.324839
49.623885	1702.005217	19.329856
49.535571	1701.994043	19.334874
49.803287	1685.725090	19.339891
49.752741	1688.671377	19.344909
49.602879	1680.335511	19.349927
49.424806	1657.742745	19.354944
49.577132	1659.639181	19.359962
49.417701	1649.879353	19.364979
49.012680	1656.857716	19.369997
49.205241	1659.248638	19.375015
49.400390	1665.041439	19.380032
49.245488	1670.709751	19.385050
49.677643	1673.408878	19.390067
49.422430	1685.859518	19.395085
49.574660	1684.398540	19.400103
49.669462	1685.246681	19.405120
49.440636	1689.558802	19.410138
49.577995	1684.836955	19.415155
49.421184	1690.849681	19.420173
49.525716	1697.654394	19.425191
49.951095	1709.346663	19.430208
49.735182	1709.696850	19.435226
49.989196	1718.646778	19.440243
49.747729	1720.459858	19.445261
49.558761	1720.107150	19.450279
49.983279	1724.507141	19.455296
50.032137	1730.006570	19.460314
50.498053	1733.461504	19.465331
50.035189	1738.596782	19.470349
50.072551	1737.633627	19.475367
50.140227	1738.504783	19.480384
50.011266	1736.392907	19.485402
50.234764	1743.177078	19.490419
50.156472	1765.873865	19.495437
50.356415	1772.684011	19.500455
50.655693	1759.864432	19.505472
50.547193	1772.603745	19.510490
51.058634	1765.673651	19.515507
50.935751	1765.815072	19.520525
50.768645	1761.631598	19.525543
50.881638	1764.851502	19.530560
50.763295	1764.482724	19.535578
50.996582	1763.124800	19.540595
51.162025	1787.181880	19.545613
51.257509	1783.177588	19.550631
51.601751	1792.667676	19.555648
51.289730	1794.701150	19.560666
51.383977	1791.614772	19.565683
51.256228	1786.072397	19.570701
51.402725	1782.791117	19.575719
51.519135	1787.203755	19.580736
51.484718	1787.684800	19.585754
51.868797	1793.497035	19.590771
51.404381	1784.738988	19.595789
51.776326	1788.238688	19.600807
51.715957	1785.050452	19.605824
51.619391	1791.809497	19.610842
51.842305	1785.152153	19.615859
52.054458	1782.063502	19.620877
51.692995	1784.176453	19.625895
51.714817	1778.735597	19.630912
51.667692	1781.593932	19.635930
51.885162	1783.504752	19.640947
51.866504	1792.587839	19.645965
52.157851	1813.760669	19.650983
52.369076	1806.983212	19.656000
52.108356	1815.352219	19.661018
52.038235	1805.287293	19.666035
52.354236	1809.167160	19.671053
52.178306	1811.027624	19.676071
52.508567	1808.585868	19.681088
52.414547	1817.853936	19.686106
52.624191	1813.155074	19.691123
52.373666	1801.617782	19.696141
52.243914	1811.847685	19.701159
52.898284	1811.908735	19.706176
52.806319	1832.074048	19.711194
53.053451	1827.893752	19.716211
53.324534	1832.643291	19.721229
53.351695	1833.126307	19.726247
53.291459	1809.993263	19.731264
53.259823	1806.577807	19.736282
53.231605	1797.983865	19.741299
53.369208	1790.985582	19.746317
53.064423	1793.514307	19.751335
53.512242	1796.378568	19.756352
53.120358	1796.493441	19.761370
53.544893	1799.926135	19.766387
53.547760	1800.597045	19.771405
53.218369	1823.528563	19.776423
53.693401	1816.687570	19.781440
53.324715	1828.144985	19.786458
53.665634	1822.615250	19.791475
53.852781	1816.339426	19.796493
53.661598	1822.518939	19.801511
53.830144	1819.907604	19.806528
53.569009	1824.125527	19.811546
53.653944	1821.138328	19.816563
53.746038	1823.864082	19.821581
53.631850	1823.247763	19.826599
53.791511	1839.829154	19.831616
53.724536	1848.560070	19.836634
54.050496	1853.913879	19.841651
54.168631	1850.620369	19.846669
53.728058	1847.442952	19.851687
54.143889	1846.551923	19.856704
54.113429	1864.282260	19.861722
54.311388	1875.060489	19.866739
54.407212	1877.867129	19.871757
53.910316	1879.779768	19.876775
54.412237	1884.423239	19.881792
54.563521	1889.178535	19.886810
54.676946	1888.881861	19.891827
54.517604	1886.304936	19.896845
54.761789	1898.056992	19.901863
55.310370	1900.473817	19.906880
55.521536	1897.931370	19.911898
55.506139	1887.743908	19.916915
55.696176	1871.996728	19.921933
55.288171	1869.463104	19.926951
55.363031	1868.368118	19.931968
55.544556	1869.340437	19.936986
55.466715	1860.141717	19.942003
55.746548	1860.238644	19.947021
55.635354	1851.261220	19.952039
55.638638	1855.441107	19.957056
55.552107	1857.498922	19.962074
55.201282	1849.531011	19.967091
55.758207	1848.541334	19.972109
55.431188	1855.136743	19.977127
55.536319	1854.987904	19.982144
55.535243	1862.906695	19.987162
55.449708	1864.411591	19.992179
55.591069	1867.006724	19.997197
55.670192	1861.364584	20.002215
55.911864	1884.251274	20.007232
56.020311	1888.951879	20.012250
55.718015	1896.936109	20.017267
56.057929	1894.210058	20.022285
55.934076	1886.261490	20.027303
56.117562	1885.535848	20.032320
55.822566	1895.516500	20.037338
56.200325	1884.170781	20.042355
56.104072	1898.411310	20.047373
56.363473	1909.723051	20.052391
56.120329	1917.882499	20.057408
56.213830	1915.613544	20.062426
56.224463	1924.260342	20.067443
56.648048	1915.771162	20.072461
56.830886	1917.938543	20.077479
57.063959	1917.873163	20.082496
56.990889	1906.859447	20.087514
56.850293	1910.584917	20.092531
57.332508	1903.702928	20.097549
56.850434	1906.071374	20.102567
56.857539	1902.551032	20.107584
57.034109	1917.401350	20.112602
57.188610	1936.073863	20.117619
57.394726	1924.946801	20.122637
57.497040	1938.621291	20.127655
57.682560	1932.270101	20.132672
57.769866	1936.839982	20.137690
57.684785	1931.286133	20.142707
57.852501	1923.886722	20.147725
57.640728	1928.776390	20.152743
57.639818	1931.667622	20.157760
57.691604	1927.003232	20.162778
57.868422	1942.753141	20.167795
57.538801	1922.076129	20.172813
57.774862	1931.177589	20.177831
57.923103	1925.900316	20.182848
57.975387	1927.168925	20.187866
58.195069	1930.517587	20.192883
58.066777	1927.700454	20.197901
58.176172	1926.824921	20.202919
58.143198	1926.072263	20.207936
58.362573	1924.154827	20.212954
58.042770	1925.222287	20.217971
58.297561	1921.868253	20.222989
57.950526	1943.179256	20.228007
58.427786	1953.998913	20.233024
58.642404	1950.690921	20.238042
58.360769	1959.844587	20.243059
58.734892	1954.335665	20.248077
58.958743	1959.011598	20.253095
59.166169	1960.232769	20.258112
59.080757	1951.994706	20.263130
58.691405	1950.483562	20.268147
58.843034	1947.078165	20.273165
58.960189	1951.324979	20.278183
58.887080	1955.654598	20.283200
59.157802	1952.367989	20.288218
58.952650	1950.725835	20.293235
59.283583	1966.074955	20.298253
59.161024	1975.269512	20.303271
59.541077	1983.068325	20.308288
59.726228	1982.692404	20.313306
59.349189	1986.088291	20.318323
59.645371	1979.573806	20.323341
59.423352	1988.838447	20.328359
59.505769	1980.117746	20.333376
59.474076	1976.468796	20.338394
59.620605	1985.569816	20.343411
59.434673	1972.638975	20.348429
59.279530	1978.658622	20.353447
59.520072	1993.395230	20.358464
59.875028	2006.739991	20.363482
59.677828	2010.881589	20.368499
59.999890	2003.688378	20.373517
60.081921	2006.063079	20.378535
60.006683	2017.119494	20.383552
60.286464	2013.484907	20.388570
60.311675	2040.170038	20.393587
60.684270	2027.746718	20.398605
60.784819	2035.820362	20.403623
60.721274	2036.166491	20.408640
61.196185	2036.863678	20.413658
61.145746	2028.178812	20.418675
61.063805	2007.674693	20.423693
61.104083	2000.386192	20.428711
60.998415	2003.092879	20.433728
61.109314	2000.897398	20.438746
61.225690	2003.142768	20.443763
61.043548	1989.880179	20.448781
61.043036	1991.849697	20.453799
60.771476	1997.834370	20.458816
61.347234	2007.188471	20.463834
61.181091	2022.867906	20.468851
61.054305	2025.089127	20.473869
61.260483	2026.930988	20.478887
61.080869	2032.767714	20.483904
61.185094	2023.487060	20.488922
61.244534	2031.748638	20.493939
61.285559	2040.843998	20.498957
61.619824	2051.151659	20.503975
61.504025	2059.654585	20.508992
61.877275	2051.338266	20.514010
61.685800	2047.756802	20.519027
61.774502	2059.132852	20.524045
61.945117	2051.167539	20.529063
61.946225	2069.152708	20.534080
62.179598	2071.829040	20.539098
62.069471	2080.972775	20.544115
62.564018	2081.859222	20.549133
62.459797	2075.367153	20.554151
62.670862	2081.270459	20.559168
62.883760	2078.984392	20.564186
62.744347	2079.955343	20.569203
62.799559	2079.019909	20.574221
62.862919	2081.024492	20.579239
62.825408	2070.903185	20.584256
62.776340	2082.750581	20.589274
62.523421	2087.556585	20.594291
62.665466	2074.794378	20.599309
62.938911	2076.944360	20.604327
62.770349	2079.088673	20.609344
62.877413	2074.425287	20.614362
63.100612	2072.454441	20.619379
62.932327	2077.045192	20.624397
63.188910	2079.268450	20.629415
62.755515	2097.024291	20.634432
63.432505	2107.458099	20.639450
63.266153	2104.025204	20.644467
63.275855	2098.161049	20.649485
63.486031	2099.363270	20.654503
63.272415	2086.971588	20.659520
62.916627	2089.365134	20.664538
62.978216	2104.561518	20.669555
63.297006	2123.992000	20.674573
63.518887	2122.107588	20.679591
63.594818	2130.542859	20.684608
63.997606	2134.165074	20.689626
64.251471	2138.278585	20.694643
64.655165	2145.307003	20.699661
64.720577	2128.598372	20.704679
64.294910	2130.180692	20.709696
64.509194	2113.060320	20.714714
64.590479	2101.918841	20.719731
64.635926	2103.358681	20.724749
64.668318	2100.695520	20.729767
64.184898	2107.937903	20.734784
64.678832	2123.456940	20.739802
64.542292	2122.301402	20.744819
64.805934	2124.340420	20.749837
64.749386	2129.050805	20.754855
64.919422	2130.566792	20.759872
65.072591	2126.111873	20.764890
65.016420	2135.663606	20.769907
65.039523	2142.616303	20.774925
65.264794	2132.733567	20.779943
65.005705	2133.506693	20.784960
65.336908	2128.083586	20.789978
65.096876	2131.190192	20.794995
65.188343	2154.620760	20.800013
65.526703	2152.366585	20.805031
65.717961	2167.587149	20.810048
65.625994	2162.907605	20.815066
65.557077	2158.651009	20.820083
65.664574	2167.666496	20.825101
65.768783	2162.873241	20.830119
65.481420	2164.447538	20.835136
65.470390	2167.067263	20.840154
65.454865	2172.039745	20.845171
65.454006	2193.960887	20.850189
66.091337	2182.020619	20.855207
66.013135	2187.373608	20.860224
66.703292	2173.739890	20.865242
66.512100	2173.860776	20.870259
66.811175	2168.714654	20.875277
66.964335	2173.193343	20.880295
66.898536	2177.587558	20.885312
66.754811	2167.889755	20.890330
67.111356	2172.799608	20.895347
66.645415	2176.159130	20.900365
67.139065	2169.508987	20.905383
66.740660	2176.590420	20.910400
66.757559	2171.286074	20.915418
66.879507	2164.777243	20.920435
67.129105	2171.858845	20.925453
67.009324	2174.606491	20.930471
67.416114	2194.151572	20.935488
67.296427	2193.890094	20.940506
67.725634	2192.210196	20.945523
67.264629	2204.966719	20.950541
67.341535	2196.322406	20.955559
67.341543	2201.325781	20.960576
67.223516	2196.002513	20.965594
67.663605	2197.577561	20.970611
67.510245	2198.018544	20.975629
67.903206	2198.391952	20.980647
67.652966	2200.081738	20.985664
68.068909	2194.932325	20.990682
67.770348	2192.448567	20.995699
67.958277	2209.214636	21.000717
68.229182	2215.226160	21.005735
68.103298	2220.851265	21.010752
68.552979	2216.495860	21.015770
68.476079	2222.422673	21.020787
68.154465	2224.292831	21.025805
68.552168	2219.394478	21.030823
68.459434	2226.383395	21.035840
68.331312	2220.749191	21.040858
68.618402	2215.614495	21.045875
68.495896	2222.806787	21.050893
69.090937	2213.495232	21.055911
68.720444	2220.316133	21.060928
68.744445	2226.864379	21.065946
69.059906	2224.922669	21.070963
69.100982	2242.223035	21.075981
69.364935	2242.846239	21.080999
69.160450	2250.366349	21.086016
68.960308	2249.712328	21.091034
69.345461	2240.584465	21.096051
69.380100	2246.618735	21.101069
69.409576	2248.373848	21.106087
69.490531	2244.106099	21.111104
69.314576	2243.747671	21.116122
69.701148	2241.386650	21.121139
69.326284	2251.643801	21.126157
69.618646	2266.230321	21.131175
69.751218	2279.294950	21.136192
69.949466	2276.607342	21.141210
70.232475	2270.972506	21.146227
70.422724	2261.615601	21.151245
70.521461	2261.934368	21.156263
70.184230	2268.990713	21.161280
70.541258	2265.854265	21.166298
70.441404	2258.470428	21.171315
70.598043	2259.911881	21.176333
70.128151	2258.415271	21.181351
70.056785	2264.554571	21.186368
70.389174	2283.464478	21.191386
70.757816	2286.618378	21.196403
70.746663	2289.423582	21.201421
71.031673	2282.669483	21.206439
71.001897	2289.169606	21.211456
71.146592	2287.688958	21.216474
71.657449	2279.509494	21.221491
71.243861	2286.330500	21.226509
71.059805	2284.868272	21.231527
71.190636	2285.603370	21.236544
71.228066	2284.225199	21.241562
71.608205	2276.969059	21.246579
71.377399	2285.510515	21.251597
71.922779	2290.312248	21.256615
71.770964	2310.380645	21.261632
71.976536	2306.790610	21.266650
72.131526	2308.184703	21.271667
72.073569	2307.701934	21.276685
72.179528	2300.581908	21.281703
71.976112	2307.750678	21.286720
71.858929	2307.830917	21.291738
71.948293	2296.873394	21.296755
71.809740	2306.720034	21.301773
72.099103	2310.253267	21.306791
72.035431	2299.319996	21.311808
71.884072	2310.736131	21.316826
72.392964	2325.600113	21.321843
72.246807	2332.637327	21.326861
72.577059	2339.185902	21.331879
72.566234	2338.309855	21.336896
72.340370	2333.629284	21.341914
72.691584	2327.844504	21.346931
72.658462	2348.331030	21.351949
72.729106	2361.598547	21.356967
73.092852	2360.713394	21.361984
72.780551	2365.021463	21.367002
73.149837	2357.971033	21.372019
72.828547	2360.292347	21.377037
73.254657	2362.051632	21.382055
73.430487	2373.273663	21.387072
73.583707	2390.409094	21.392090
73.628888	2389.709568	21.397107
73.860886	2387.804152	21.402125
74.008069	2388.290466	21.407143
73.936148	2387.625364	21.412160
73.932396	2386.223713	21.417178
73.936856	2373.016003	21.422195
73.888122	2388.494002	21.427213
73.993593	2384.981219	21.432231
74.081472	2393.792217	21.437248
73.836887	2388.810400	21.442266
74.672605	2387.486160	21.447283
74.625058	2382.055442	21.452301
74.849014	2369.089216	21.457319
74.430931	2367.739894	21.462336
75.077743	2381.614837	21.467354
75.237659	2373.318844	21.472371
74.987024	2363.488288	21.477389
74.922285	2368.183571	21.482407
75.033514	2362.954430	21.487424
74.960191	2363.457707	21.492442
75.208940	2365.156704	21.497459
75.233079	2374.364124	21.502477
75.018593	2391.929186	21.507495
75.589176	2381.811730	21.512512
75.418282	2394.157579	21.517530
75.466387	2386.479394	21.522547
75.756130	2386.897918	21.527565
75.676099	2390.557528	21.532583
75.673614	2387.554828	21.537600
75.243518	2389.116648	21.542618
75.782765	2384.438033	21.547635
75.736250	2386.999912	21.552653
76.005904	2383.141720	21.557671
76.323021	2401.960213	21.562688
76.364687	2412.318717	21.567706
76.506051	2401.242237	21.572723
76.218743	2395.061181	21.577741
76.455788	2406.216368	21.582759
76.684808	2406.281194	21.587776
76.483339	2416.543492	21.592794
76.273616	2408.417582	21.597811
76.302981	2410.024696	21.602829
76.694539	2408.415603	21.607847
77.054303	2411.347376	21.612864
76.901725	2412.500855	21.617882
76.803165	2404.104495	21.622899
77.061179	2409.286716	21.627917
77.083077	2413.608546	21.632935
77.492700	2423.803929	21.637952
77.215896	2428.139975	21.642970
77.043571	2427.364783	21.647987
77.192132	2427.359908	21.653005
77.045333	2430.586121	21.658023
77.355849	2429.152312	21.663040
77.134460	2439.020678	21.668058
77.585972	2435.111775	21.673075
77.943582	2455.960287	21.678093
77.604708	2449.877941	21.683111
77.613982	2453.581386	21.688128
77.282203	2460.317213	21.693146
77.668056	2453.977399	21.698163
77.835310	2469.282961	21.703181
78.276503	2477.191947	21.708199
78.567934	2474.740796	21.713216
78.851560	2468.829792	21.718234
78.958750	2464.309582	21.723251
79.272431	2463.183129	21.728269
79.083556	2460.726767	21.733287
78.929606	2445.166893	21.738304
78.917561	2441.679140	21.743322
78.920875	2433.393002	21.748339
78.746888	2436.407586	21.753357
78.722109	2449.348112	21.758375
79.195510	2455.276468	21.763392
78.609229	2458.745421	21.768410
78.986272	2462.892880	21.773427
79.073783	2470.035419	21.778445
79.426020	2483.423961	21.783463
79.819759	2486.800512	21.788480
79.346077	2501.198815	21.793498
79.666836	2495.399744	21.798515
79.397648	2491.694079	21.803533
79.482082	2501.271095	21.808551
79.680783	2492.818587	21.813568
79.693858	2502.546839	21.818586
79.782691	2515.649647	21.823603
79.940341	2520.986781	21.828621
80.090494	2531.631282	21.833639
80.223917	2516.030268	21.838656
80.420165	2517.984080	21.843674
79.982469	2519.896008	21.848691
80.219414	2546.499572	21.853709
80.644371	2545.256977	21.858727
80.678201	2543.284081	21.863744
80.564123	2550.435752	21.868762
80.838060	2548.061910	21.873779
80.945025	2549.936074	21.878797
80.928546	2551.893356	21.883815
81.311443	2557.370238	21.888832
81.660456	2572.785069	21.893850
81.983013	2564.587146	21.898867
81.719558	2547.093319	21.903885
81.678446	2542.101650	21.908903
81.712648	2536.382083	21.913920
81.368830	2538.096512	21.918938
81.538471	2537.051871	21.923955
81.692818	2557.586652	21.928973
81.851289	2566.460429	21.933991
81.638674	2564.616683	21.939008
81.827279	2559.045468	21.944026
81.607033	2571.312648	21.949043
81.953166	2573.892765	21.954061
82.019234	2584.863497	21.959079
82.314327	2575.600794	21.964096
83.010473	2585.478967	21.969114
82.589530	2583.017453	21.974131
83.052423	2582.271328	21.979149
82.568230	2584.553605	21.984167
83.072392	2572.238702	21.989184
82.911185	2589.642369	21.994202
82.759477	2581.826425	21.999219
82.941376	2575.906697	22.004237
82.979210	2576.150157	22.009255
82.881672	2575.117634	22.014272
82.913530	2576.134562	22.019290
83.223460	2574.330743	22.024307
83.548892	2590.128268	22.029325
83.311431	2605.862269	22.034343
83.656426	2601.572193	22.039360
83.497133	2604.292227	22.044378
83.534539	2611.554188	22.049395
83.624983	2603.428289	22.054413
83.606447	2607.544679	22.059431
83.799390	2603.684616	22.064448
83.773354	2608.018010	22.069466
83.807422	2626.707434	22.074483
84.089337	2635.185519	22.079501
84.277256	2635.433958	22.084519
84.510415	2625.740948	22.089536
84.709888	2634.601649	22.094554
84.389831	2628.014899	22.099571
84.497843	2636.904584	22.104589
84.233061	2647.213778	22.109607
84.866563	2652.648649	22.114624
84.709028	2661.938011	22.119642
84.872843	2656.986266	22.124659
85.094718	2659.932343	22.129677
85.160966	2663.307456	22.134695
85.335056	2657.438210	22.139712
85.877096	2652.398800	22.144730
85.469819	2661.070583	22.149747
85.490729	2651.284874	22.154765
85.620188	2660.168645	22.159783
85.588980	2646.221714	22.164800
85.389880	2662.432490	22.169818
85.560714	2676.784466	22.174835
85.829332	2677.706142	22.179853
85.475953	2686.249683	22.184871
86.097033	2678.025315	22.189888
86.282704	2689.009314	22.194906
86.107402	2702.922360	22.199923
86.666338	2710.189031	22.204941
86.408860	2713.884508	22.209959
86.509746	2710.005072	22.214976
86.722408	2707.803603	22.219994
86.766958	2700.739273	22.225011
87.019759	2701.739567	22.230029
86.753225	2704.506184	22.235047
86.592603	2704.138109	22.240064
86.804217	2697.155074	22.245082
86.706585	2720.149790	22.250099
87.552761	2724.415422	22.255117
87.792224	2737.664258	22.260135
87.590919	2734.917776	22.265152
87.417342	2733.475811	22.270170
87.438752	2731.850643	22.275187
87.704359	2726.827624	22.280205
87.699314	2729.932302	22.285223
87.660818	2729.256118	22.290240
87.736544	2724.004015	22.295258
87.448232	2726.959698	22.300275
88.132252	2746.960609	22.305293
88.191134	2757.358216	22.310311
88.179977	2759.849315	22.315328
88.377017	2754.884930	22.320346
88.431492	2757.626552	22.325363
88.516495	2754.562388	22.330381
88.137669	2761.203795	22.335399
88.402929	2760.212149	22.340416
88.860303	2772.311744	22.345434
89.145794	2770.607640	22.350451
89.903408	2754.282139	22.355469
89.679532	2747.510051	22.360487
89.676284	2733.877309	22.365504
89.731480	2722.148352	22.370522
89.506588	2728.063731	22.375539
89.735862	2724.266895	22.380557
89.494114	2721.322008	22.385575
89.496056	2724.987364	22.390592
89.652677	2706.417974	22.395610
89.591675	2722.322381	22.400627
89.785535	2718.356227	22.405645
89.588248	2725.124542	22.410663
89.845526	2741.645004	22.415680
90.176283	2749.392948	22.420698
89.893885	2754.529269	22.425715
90.117275	2751.685819	22.430733
89.837815	2761.606955	22.435751
90.018970	2758.098440	22.440768
90.787450	2780.100035	22.445786
90.441017	2792.118267	22.450803
90.223482	2780.514126	22.455821
90.564571	2785.986622	22.460839
90.810627	2783.519736	22.465856
91.220378	2802.490258	22.470874
90.762107	2813.238042	22.475891
90.623909	2810.421999	22.480909
90.581193	2808.175555	22.485927
90.721542	2821.905923	22.490944
91.144813	2834.724663	22.495962
91.314879	2840.694527	22.500979
91.526009	2834.454077	22.505997
91.550959	2835.747383	22.511015
91.988338	2856.814688	22.516032
92.177409	2855.012420	22.521050
92.099921	2866.274548	22.526067
92.282783	2854.132124	22.531085
92.665810	2865.504733	22.536103
92.648827	2863.764271	22.541120
92.885462	2858.058976	22.546138
92.494819	2856.471568	22.551155
92.662263	2852.083760	22.556173
92.727088	2853.160585	22.561191
92.674815	2854.563190	22.566208
92.871556	2847.831001	22.571226
92.692270	2864.267054	22.576243
92.890304	2856.211336	22.581261
92.380069	2851.724335	22.586279
92.235893	2871.978811	22.591296
92.821805	2876.307036	22.596314
92.627716	2895.105179	22.601331
93.167222	2906.681747	22.606349
93.639403	2914.840156	22.611367
93.306317	2912.678967	22.616384
93.197249	2914.774525	22.621402
93.611032	2934.334735	22.626419
93.691976	2935.831749	22.631437
94.187706	2931.246829	22.636455
94.262349	2941.335619	22.641472
94.632031	2930.891335	22.646490
94.434801	2934.060280	22.651507
94.753950	2930.425635	22.656525
94.974416	2930.430072	22.661543
94.427341	2925.374725	22.666560
94.886346	2926.746696	22.671578
94.667820	2936.701125	22.676595
94.991265	2938.023969	22.681613
95.453629	2947.687277	22.686631
95.133752	2956.084836	22.691648
94.962735	2945.974517	22.696666
95.141151	2960.320376	22.701683
95.334334	2967.582599	22.706701
95.519867	2963.183879	22.711719
95.463858	2962.285383	22.716736
95.693996	2945.724887	22.721754
95.722010	2957.984182	22.726771
95.646918	2951.599117	22.731789
95.562304	2958.683474	22.736807
95.964772	2973.100383	22.741824
96.302434	2979.324356	22.746842
96.024403	2983.241830	22.751859
96.095520	2981.476476	22.756877
96.175577	2980.179354	22.761895
96.019897	2978.680844	22.766912
96.527522	2996.533687	22.771930
96.895732	3000.748513	22.776947
96.792929	3008.636760	22.781965
97.153746	3005.260153	22.786983
97.139567	3006.916301	22.792000
97.125483	2998.871353	22.797018
97.210462	2999.353852	22.802035
97.506458	2995.450974	22.807053
97.437672	2994.161658	22.812071
97.598923	3003.623847	22.817088
97.823515	2988.145801	22.822106
97.566234	2995.657326	22.827123
97.695263	2995.014709	22.832141
97.507837	2997.021326	22.837159
97.637335	3021.467818	22.842176
97.879069	3017.283380	22.847194
97.783559	3013.802284	22.852211
97.803979	3028.650484	22.857229
98.002183	3037.546669	22.862247
98.090945	3060.966059	22.867264
98.381778	3057.562092	22.872282
98.555048	3058.370102	22.877299
98.637731	3052.778125	22.882317
99.091565	3071.876700	22.887335
98.964696	3078.004282	22.892352
99.420959	3073.038450	22.897370
99.032522	3076.367558	22.902387
99.262546	3067.950877	22.907405
99.662024	3071.940431	22.912423
99.859310	3067.579102	22.917440
100.248266	3056.297611	22.922458
100.106013	3061.843054	22.927475
100.145631	3062.892979	22.932493
100.586913	3052.917852	22.937511
100.494522	3048.213305	22.942528
100.485754	3020.645563	22.947546
100.217114	3020.517888	22.952563
100.095260	3021.911992	22.957581
100.419206	3024.402561	22.962599
99.963850	3049.489646	22.967616
100.610676	3049.477558	22.972634
100.690258	3062.282736	22.977651
100.529551	3063.615973	22.982669
100.639895	3052.426068	22.987687
100.716334	3053.748240	22.992704
100.712608	3071.416450	22.997722
100.897504	3085.192407	23.002739
100.767473	3088.145869	23.007757
100.990369	3095.947743	23.012775
100.704547	3102.739597	23.017792
100.990845	3108.762694	23.022810
101.417723	3125.393971	23.027827
101.315082	3121.246266	23.032845
101.558741	3134.221888	23.037863
101.930114	3151.497900	23.042880
101.840488	3150.565213	23.047898
101.949297	3158.266385	23.052915
101.825434	3158.561140	23.057933
102.108949	3149.054729	23.062951
102.042575	3153.026051	23.067968
102.203311	3170.282757	23.072986
102.228827	3174.544744	23.078003
102.380310	3173.331412	23.083021
102.946344	3167.378724	23.088039
102.777911	3178.502636	23.093056
102.680202	3185.676288	23.098074
102.960826	3188.196527	23.103091
103.182415	3191.293554	23.108109
103.305254	3189.842443	23.113127
103.153527	3195.405258	23.118144
103.151171	3205.901144	23.123162
103.584654	3208.710969	23.128179
103.758562	3226.399442	23.133197
104.157278	3212.766804	23.138215
103.947387	3217.265188	23.143232
104.465288	3215.763771	23.148250
104.436853	3215.128022	23.153267
104.135130	3216.380369	23.158285
104.414046	3205.565128	23.163303
104.451129	3228.294482	23.168320
104.244992	3234.430575	23.173338
104.410867	3235.941852	23.178355
104.329220	3247.125805	23.183373
104.708202	3245.557702	23.188391
104.792784	3262.893708	23.193408
105.046391	3270.360223	23.198426
105.170977	3268.493816	23.203443
105.223599	3267.044130	23.208461
105.281552	3265.160449	23.213479
105.282802	3272.742535	23.218496
105.554606	3283.537033	23.223514
105.757879	3292.730581	23.228531
105.688661	3304.194030	23.233549
105.856689	3297.029767	23.238567
105.930138	3299.063544	23.243584
106.371302	3294.386399	23.248602
106.185653	3301.967668	23.253619
106.090656	3320.636063	23.258637
106.765963	3315.734548	23.263655
106.492781	3320.560830	23.268672
106.706036	3317.499259	23.273690
107.092743	3319.842426	23.278707
106.935819	3320.850223	23.283725
107.196419	3304.348071	23.288743
106.937314	3315.557235	23.293760
106.918934	3333.132105	23.298778
107.286147	3329.973678	23.303795
107.445339	3345.437757	23.308813
107.501279	3335.137876	23.313831
107.279389	3346.342058	23.318848
107.722949	3352.376519	23.323866
107.803817	3357.821593	23.328883
107.824240	3358.970012	23.333901
108.563267	3345.131869	23.338919
108.515282	3352.455615	23.343936
108.451845	3351.653615	23.348954
108.785836	3346.276484	23.353971
108.372184	3355.923419	23.358989
108.675035	3346.442812	23.364007
108.665845	3349.774701	23.369024
108.852518	3349.404406	23.374042
109.089057	3345.790089	23.379059
108.882767	3349.281913	23.384077
109.080242	3363.443857	23.389095
109.326369	3377.794598	23.394112
109.329440	3375.290044	23.399130
109.525718	3378.525187	23.404147
109.502775	3381.671555	23.409165
109.366690	3373.399028	23.414183
109.422825	3376.503117	23.419200
109.673816	3397.819477	23.424218
110.117995	3403.879842	23.429235
109.622370	3411.259900	23.434253
109.807730	3410.970538	23.439271
109.996620	3418.073040	23.444288
110.204005	3432.512955	23.449306
110.487012	3433.353934	23.454323
110.865261	3438.013714	23.459341
110.900257	3440.654353	23.464359
110.971662	3440.372511	23.469376
110.603730	3440.307401	23.474394
111.077785	3438.056484	23.479411
111.119081	3460.777207	23.484429
111.762905	3451.683613	23.489447
111.561042	3467.575572	23.494464
111.731232	3464.790449	23.499482
111.676791	3460.231453	23.504499
111.623255	3460.673596	23.509517
111.719203	3445.185373	23.514535
111.812330	3462.641059	23.519552
111.959935	3484.200333	23.524570
112.120803	3472.921802	23.529587
112.313321	3484.408033	23.534605
112.544103	3487.611083	23.539623
112.450939	3477.376445	23.544640
112.537947	3506.333970	23.549658
113.154568	3505.654397	23.554675
113.087537	3508.384059	23.559693
112.871708	3509.438668	23.564711
113.442820	3508.907224	23.569728
113.535199	3510.933158	23.574746
113.388216	3506.106822	23.579763
113.106210	3507.086201	23.584781
113.483301	3520.198253	23.589799
113.773964	3529.197476	23.594816
113.627719	3528.668705	23.599834
113.934452	3532.752149	23.604851
114.098296	3546.592650	23.609869
114.014395	3525.826198	23.614887
114.236881	3538.418627	23.619904
114.179677	3549.194755	23.624922
114.502582	3547.252044	23.629939
114.494556	3556.466296	23.634957
114.712627	3562.049680	23.639975
114.689737	3552.371878	23.644992
114.617330	3566.750926	23.650010
114.899448	3575.959099	23.655027
114.840883	3584.017861	23.660045
115.171114	3578.941702	23.665063
115.377941	3578.309758	23.670080
115.509081	3602.840755	23.675098
115.663529	3608.939510	23.680115
115.748278	3607.874260	23.685133
115.686818	3613.311972	23.690151
116.273661	3604.569137	23.695168
116.165873	3604.064290	23.700186
116.286940	3594.482235	23.705203
116.230453	3601.622057	23.710221
116.538764	3601.092550	23.715239
116.674894	3610.418324	23.720256
116.876171	3628.391319	23.725274
117.128602	3616.962020	23.730291
117.020078	3625.535068	23.735309
117.359902	3623.132793	23.740327
117.461911	3618.853296	23.745344
117.462839	3624.694469	23.750362
117.662684	3621.902814	23.755379
117.793267	3618.610016	23.760397
117.592003	3614.788841	23.765415
117.598408	3614.560717	23.770432
117.137324	3602.385347	23.775450
117.780290	3608.004444	23.780467
117.780457	3621.051651	23.785485
117.982612	3638.652031	23.790503
118.237221	3638.259415	23.795520
118.024717	3644.142366	23.800538
118.044842	3652.114849	23.805555
118.147680	3662.508511	23.810573
117.941904	3668.708893	23.815591
118.386431	3683.833333	23.820608
118.636878	3699.623188	23.825626
119.163100	3696.733572	23.830643
118.943268	3700.018250	23.835661
119.142803	3714.582974	23.840679
119.415083	3721.505595	23.845696
119.453938	3726.267543	23.850714
119.721711	3721.861638	23.855731
120.088392	3713.497499	23.860749
120.207274	3717.424789	23.865767
120.430592	3726.856628	23.870784
120.727498	3735.335582	23.875802
120.679440	3737.986137	23.880819
120.896006	3722.607531	23.885837
120.680598	3738.299629	23.890855
121.319766	3735.041589	23.895872
121.110175	3737.779233	23.900890
120.935939	3738.237505	23.905907
121.106663	3734.019006	23.910925
121.410024	3726.028812	23.915943
121.337221	3730.492352	23.920960
121.099121	3736.284698	23.925978
121.549198	3726.447465	23.930995
121.459928	3740.886963	23.936013
121.541802	3762.978080	23.941031
121.924481	3763.831651	23.946048
122.017449	3765.290523	23.951066
122.199918	3765.578084	23.956083
122.562135	3757.615893	23.961101
122.719235	3751.423433	23.966119
122.901437	3746.702176	23.971136
122.685493	3750.459897	23.976154
122.703862	3765.235900	23.981171
122.891427	3778.829329	23.986189
123.070583	3779.679319	23.991207
122.931777	3774.238476	23.996224
123.008573	3775.034208	24.001242
123.153593	3794.154677	24.006259
123.169124	3800.488431	24.011277
123.175184	3808.428288	24.016295
123.396818	3809.906337	24.021312
123.695385	3827.025889	24.026330
123.312990	3836.089110	24.031347
123.955593	3829.233578	24.036365
124.099725	3842.692925	24.041383
124.372422	3848.996165	24.046400
124.344733	3867.293351	24.051418
124.773920	3866.502378	24.056435
124.444330	3865.958390	24.061453
124.928969	3858.561704	24.066471
125.299508	3848.512783	24.071488
124.872941	3864.603925	24.076506
124.978271	3864.219969	24.081523
125.423528	3866.797617	24.086541
125.236306	3887.243655	24.091559
125.696642	3875.577621	24.096576
125.584810	3892.342955	24.101594
125.676451	3877.974455	24.106611
125.943558	3887.017964	24.111629
125.809207	3893.300276	24.116647
126.590073	3907.938669	24.121664
126.434797	3923.307139	24.126682
126.249504	3909.607943	24.131699
126.336415	3909.097503	24.136717
126.355227	3913.328124	24.141735
126.281455	3921.166724	24.146752
126.511197	3930.116849	24.151770
126.622582	3927.568612	24.156787
127.313482	3952.687535	24.161805
126.987881	3956.923825	24.166823
127.681206	3957.342660	24.171840
127.653978	3961.562439	24.176858
127.274820	3965.706044	24.181875
127.822476	3971.159201	24.186893
127.947343	3988.963397	24.191911
128.325361	3986.388951	24.196928
127.882069	3996.270367	24.201946
128.241829	3996.189840	24.206963
128.701495	4012.631160	24.211981
128.310353	4020.274094	24.216999
128.495863	4023.610782	24.222016
128.559956	4027.728776	24.227034
128.555679	4034.766012	24.232051
128.854741	4048.284051	24.237069
128.740746	4060.993855	24.242087
128.627718	4076.701170	24.247104
128.776735	4084.038194	24.252122
129.464422	4093.650204	24.257139
129.792944	4099.170538	24.262157
129.713102	4124.806466	24.267175
129.987613	4122.003890	24.272192
130.175525	4119.793348	24.277210
130.436293	4121.884697	24.282227
130.824527	4119.131736	24.287245
130.696092	4140.657858	24.292263
131.042164	4143.803297	24.297280
131.177671	4144.853897	24.302298
131.108210	4139.467946	24.307315
131.473775	4129.965421	24.312333
131.764358	4135.630676	24.317351
131.737734	4136.384551	24.322368
131.686714	4129.818205	24.327386
131.625177	4133.133366	24.332403
131.676886	4130.530438	24.337421
131.803181	4132.157453	24.342439
131.636507	4136.433136	24.347456
131.848230	4156.449391	24.352474
131.913367	4165.677436	24.357491
132.407633	4159.339794	24.362509
132.393900	4173.056796	24.367527
133.087054	4157.204410	24.372544
133.582574	4169.997679	24.377562
133.705745	4155.333879	24.382579
133.956058	4132.814376	24.387597
133.969239	4128.054156	24.392615
133.795907	4125.848523	24.397632
134.048614	4116.905783	24.402650
134.269077	4127.506223	24.407667
134.314477	4112.480137	24.412685
134.029341	4113.050564	24.417703
134.124713	4116.611730	24.422720
134.216337	4111.196656	24.427738
133.708749	4122.577235	24.432755
134.286031	4117.264150	24.437773
134.383658	4123.463508	24.442791
134.353771	4141.903920	24.447808
134.703465	4148.814261	24.452826
134.264318	4158.762027	24.457843
134.233676	4160.504510	24.462861
134.000311	4179.485548	24.467879
134.597499	4196.263709	24.472896
134.885378	4214.953410	24.477914
134.760794	4222.675390	24.482931
135.305429	4238.797664	24.487949
135.326595	4251.569425	24.492967
135.964025	4255.490213	24.497984
136.081697	4276.877969	24.503002
135.858535	4282.625506	24.508019
136.327120	4272.524190	24.513037
136.057476	4291.988631	24.518055
136.569848	4298.060461	24.523072
136.507802	4301.188705	24.528090
136.728328	4298.954999	24.533107
136.925543	4322.485048	24.538125
137.310385	4335.407494	24.543143
137.047975	4331.801847	24.548160
137.437137	4329.258965	24.553178
137.519169	4341.567070	24.558195
137.839532	4345.774469	24.563213
138.001175	4349.924769	24.568231
138.032943	4351.730929	24.573248
138.081701	4348.185394	24.578266
138.312780	4348.444806	24.583283
139.017951	4348.830975	24.588301
139.154333	4360.989883	24.593319
139.845643	4351.477586	24.598336
140.688927	4309.240470	24.603354
140.524973	4301.098085	24.608371
140.759284	4283.403028	24.613389
140.360064	4281.259718	24.618407
140.459960	4269.050841	24.623424
140.112310	4263.325194	24.628442
140.310257	4259.946253	24.633459
140.428634	4257.012097	24.638477
140.718090	4255.806469	24.643495
140.448231	4247.867567	24.648512
140.719928	4243.301394	24.653530
139.995968	4257.832669	24.658547
140.263693	4251.317253	24.663565
140.327263	4248.589087	24.668583
140.785296	4271.378760	24.673600
141.131309	4278.788666	24.678618
140.933054	4284.065852	24.683635
140.914559	4284.925880	24.688653
140.782980	4296.230708	24.693671
140.898981	4307.410922	24.698688
141.136329	4309.011231	24.703706
141.192539	4335.594335	24.708723
141.291699	4352.221537	24.713741
141.258898	4363.287915	24.718759
141.786782	4383.475183	24.723776
142.088906	4389.204765	24.728794
142.122623	4410.999633	24.733811
141.927211	4410.054917	24.738829
142.090641	4423.611179	24.743847
141.987534	4445.618628	24.748864
142.544633	4440.981341	24.753882
142.826886	4462.482968	24.758899
142.584231	4484.052168	24.763917
143.090433	4487.713677	24.768935
143.165937	4496.216058	24.773952
143.965638	4501.559791	24.778970
143.595879	4514.028167	24.783987
144.068927	4503.567635	24.789005
144.060602	4519.286737	24.794023
143.921593	4528.145312	24.799040
144.449393	4526.490537	24.804058
144.494997	4537.284121	24.809075
144.697731	4538.447613	24.814093
144.925783	4548.087072	24.819111
144.900547	4563.938973	24.824128
146.104269	4537.976423	24.829146
145.873153	4544.923217	24.834163
146.258547	4539.518240	24.839181
146.003699	4548.011759	24.844199
145.877767	4539.284094	24.849216
146.260698	4537.291127	24.854234
146.144695	4543.787222	24.859251
146.141994	4548.118456	24.864269
146.199395	4556.013539	24.869287
146.272459	4573.950259	24.874304
146.883156	4562.680851	24.879322
146.547699	4574.145766	24.884339
146.675553	4589.677713	24.889357
146.806708	4595.747649	24.894375
146.490370	4612.973402	24.899392
147.360981	4624.328488	24.904410
146.875593	4645.026277	24.909427
147.318541	4646.094730	24.914445
147.481591	4671.386407	24.919463
147.390374	4672.825571	24.924480
147.881392	4670.841402	24.929498
148.169424	4694.115141	24.934515
148.505478	4692.423700	24.939533
148.795370	4691.215605	24.944551
148.980695	4698.053883	24.949568
149.090492	4704.625137	24.954586
149.269872	4727.161728	24.959603
149.727721	4718.089658	24.964621
149.618865	4717.257332	24.969639
149.356029	4723.509350	24.974656
149.561837	4720.660597	24.979674
149.476794	4731.224800	24.984691
149.714157	4729.315067	24.989709
149.968905	4740.574913	24.994727
149.375400	4745.053212	24.999744
149.979383	4763.728052	25.004762
149.887415	4781.278973	25.009779
150.084533	4791.918395	25.014797
150.501208	4792.979411	25.019815
150.792859	4799.625228	25.024832
151.256827	4812.193912	25.029850
151.454826	4820.225635	25.034867
151.652498	4833.851379	25.039885
151.997592	4820.383775	25.044903
151.828879	4829.949949	25.049920
151.959102	4828.198193	25.054938
151.964710	4834.914400	25.059955
152.092731	4851.155372	25.064973
152.319472	4846.865839	25.069991
152.077707	4859.738493	25.075008
152.239677	4862.459472	25.080026
152.453039	4884.175525	25.085043
152.462184	4881.709099	25.090061
152.753099	4885.334814	25.095079
152.712435	4905.444767	25.100096
153.097423	4907.050531	25.105114
152.790110	4921.736050	25.110131
152.854163	4938.355530	25.115149
153.606623	4936.008135	25.120167
153.921260	4956.905729	25.125184
154.030919	4974.205204	25.130202
154.265708	4970.790063	25.135219
154.152420	4976.351055	25.140237
154.349561	4989.829749	25.145255
154.584082	4995.742477	25.150272
155.086193	4995.144102	25.155290
155.038978	5002.874082	25.160307
155.417697	5010.800265	25.165325
155.857995	5024.522889	25.170343
155.798866	5020.671445	25.175360
156.004101	5018.384264	25.180378
156.310765	5011.221780	25.185395
156.583697	5009.602225	25.190413
157.175774	4996.651019	25.195431
156.914903	5010.102675	25.200448
157.175584	4998.051590	25.205466
157.380940	5011.196588	25.210483
157.347338	5010.090271	25.215501
157.829807	5003.259277	25.220519
157.238046	5011.105744	25.225536
157.387162	5008.137990	25.230554
157.368181	5009.095008	25.235571
157.293388	5011.769515	25.240589
157.621713	5020.223078	25.245607
157.354455	5038.253111	25.250624
157.484495	5043.157818	25.255642
157.585980	5060.738331	25.260659
157.637412	5073.542745	25.265677
157.947707	5081.592956	25.270695
158.078430	5107.130913	25.275712
158.393554	5125.072926	25.280730
158.684435	5133.226411	25.285747
158.724689	5138.749342	25.290765
159.166462	5159.808794	25.295783
158.997134	5168.702693	25.300800
159.446916	5168.069694	25.305818
159.773980	5182.262550	25.310835
159.973221	5192.889290	25.315853
159.909050	5177.238529	25.320871
160.061302	5207.758369	25.325888
160.300141	5208.097629	25.330906
159.972652	5207.448097	25.335923
160.169731	5226.130468	25.340941
161.082676	5243.238467	25.345959
160.680515	5250.573914	25.350976
161.009206	5259.438657	25.355994
161.261068	5273.823659	25.361011
161.308651	5277.485178	25.366029
161.752905	5287.466410	25.371047
161.828047	5307.684430	25.376064
161.770449	5295.775007	25.381082
162.169728	5306.031501	25.386099
162.540982	5312.547747	25.391117
162.847301	5321.856497	25.396135
162.941248	5319.317629	25.401152
163.233219	5320.415160	25.406170
163.373612	5320.793623	25.411187
163.214687	5319.972735	25.416205
163.483190	5320.620523	25.421223
163.385042	5323.626594	25.426240
163.659862	5337.327375	25.431258
163.957181	5345.619301	25.436275
163.684784	5353.894072	25.441293
163.890245	5342.995461	25.446311
164.060109	5370.417521	25.451328
164.253963	5377.743763	25.456346
164.604932	5380.268821	25.461363
164.648168	5389.561475	25.466381
164.932740	5396.456809	25.471399
165.325300	5401.928375	25.476416
165.575329	5401.574287	25.481434
165.863074	5387.094245	25.486451
165.676609	5403.142325	25.491469
165.885597	5397.419053	25.496487
166.117936	5425.145069	25.501504
166.179053	5419.135268	25.506522
166.426239	5413.851412	25.511539
166.077522	5419.855710	25.516557
166.668910	5425.523428	25.521575
166.548460	5447.658808	25.526592
166.620115	5455.001456	25.531610
166.921848	5462.347614	25.536627
166.883422	5476.514052	25.541645
167.162804	5476.302363	25.546663
167.228656	5501.995080	25.551680
167.358729	5511.005598	25.556698
167.692879	5517.035856	25.561715
167.406626	5539.922707	25.566733
167.989321	5546.343270	25.571751
168.018661	5563.627600	25.576768
168.146144	5572.101449	25.581786
168.701040	5579.856091	25.586803
168.774180	5609.804679	25.591821
169.224121	5613.749889	25.596839
169.177333	5612.224361	25.601856
169.210820	5607.928934	25.606874
169.921324	5628.156769	25.611891
169.678296	5631.433490	25.616909
169.928306	5631.756728	25.621927
170.147432	5647.326533	25.626944
169.992692	5661.186403	25.631962
170.678418	5662.239790	25.636979
170.486275	5665.532477	25.641997
170.833200	5675.798701	25.647015
170.959327	5687.286162	25.652032
170.878426	5691.239273	25.657050
171.648224	5689.515030	25.662067
171.507586	5716.740412	25.667085
172.041789	5715.712958	25.672103
172.348229	5706.702505	25.677120
172.075225	5717.789273	25.682138
172.107323	5718.467701	25.687156
172.176305	5737.192443	25.692173
172.478089	5739.698956	25.697191
172.822347	5739.033855	25.702208
173.034445	5750.918989	25.707226
173.423482	5759.845659	25.712244
173.343702	5764.011252	25.717261
173.544896	5757.682697	25.722279
173.348296	5761.669229	25.727296
173.477097	5774.524363	25.732314
174.128605	5786.337290	25.737332
174.017062	5785.410841	25.742349
174.582923	5786.778718	25.747367
175.059133	5799.065778	25.752384
175.342722	5791.863460	25.757402
176.065738	5770.866616	25.762420
175.954658	5759.039764	25.767437
175.798804	5740.799887	25.772455
176.025258	5741.773658	25.777472
176.098489	5747.370871	25.782490
176.320958	5747.371049	25.787508
176.214795	5747.213976	25.792525
176.296347	5751.357482	25.797543
176.274573	5746.344250	25.802560
176.289860	5752.737901	25.807578
176.484057	5763.072093	25.812596
176.526151	5782.067564	25.817613
176.800509	5775.469299	25.822631
176.765487	5780.014169	25.827648
176.733334	5801.881766	25.832666
177.272635	5809.089372	25.837684
177.141952	5828.235688	25.842701
177.382622	5836.991734	25.847719
177.394999	5848.431270	25.852736
177.499814	5867.679479	25.857754
177.485914	5873.681866	25.862772
177.512313	5891.282084	25.867789
177.771562	5915.228726	25.872807
178.311953	5925.889059	25.877824
178.218459	5950.192874	25.882842
178.917279	5956.315498	25.887860
178.719215	5977.487099	25.892877
179.463936	5985.131639	25.897895
179.553400	5989.080929	25.902912
179.532996	6015.134575	25.907930
179.827560	6025.094686	25.912948
180.110358	6034.080911	25.917965
180.320859	6053.178678	25.922983
180.753885	6049.020728	25.928000
180.672045	6051.203537	25.933018
181.383893	6056.405684	25.938036
181.368380	6078.234667	25.943053
181.676495	6075.953868	25.948071
182.043988	6072.619618	25.953088
181.717875	6074.600438	25.958106
181.792551	6087.255318	25.963124
182.011831	6104.846562	25.968141
182.111789	6102.777564	25.973159
182.469345	6119.918961	25.978176
182.734857	6134.387544	25.983194
182.694396	6147.808263	25.988212
182.878487	6142.552766	25.993229
183.112510	6158.842844	25.998247
183.084669	6163.977342	26.003264
182.783592	6177.417766	26.008282
183.509557	6188.650753	26.013300
183.552504	6197.754116	26.018317
183.863493	6213.113886	26.023335
184.093033	6230.779964	26.028352
184.035366	6245.093635	26.033370
184.643834	6254.300746	26.038388
184.968385	6269.511820	26.043405
185.709693	6259.744348	26.048423
185.964911	6241.376512	26.053440
186.007479	6257.108579	26.058458
185.809903	6242.154709	26.063476
186.207063	6255.393318	26.068493
186.134969	6269.255739	26.073511
186.380248	6266.586819	26.078528
186.771057	6269.371620	26.083546
186.621880	6264.263615	26.088564
186.537291	6276.979768	26.093581
186.658404	6293.851897	26.098599
187.397726	6287.741669	26.103616
187.447704	6291.929157	26.108634
187.637333	6287.214576	26.113652
187.750236	6289.438305	26.118669
187.479117	6300.499174	26.123687
187.699797	6312.795233	26.128704
187.940249	6319.673890	26.133722
188.588245	6328.927249	26.138740
188.624727	6342.090396	26.143757
188.695265	6341.577876	26.148775
189.109107	6346.123142	26.153792
188.825039	6349.710852	26.158810
188.995938	6366.047077	26.163828
189.633888	6370.131367	26.168845
189.244813	6374.746269	26.173863
189.452983	6397.394672	26.178880
189.551323	6416.906118	26.183898
189.906961	6431.241066	26.188916
190.482820	6443.996465	26.193933
190.144881	6455.265453	26.198951
190.765478	6466.207399	26.203968
190.697389	6472.726252	26.208986
190.482745	6487.766431	26.214004
191.276349	6491.541340	26.219021
192.088146	6481.460358	26.224039
192.269545	6489.860368	26.229056
192.092178	6499.410083	26.234074
192.330441	6501.011259	26.239092
192.546813	6497.216065	26.244109
192.360215	6505.135344	26.249127
192.605719	6527.635956	26.254144
192.791451	6539.031431	26.259162
193.145701	6544.645239	26.264180
193.481479	6560.401347	26.269197
193.110021	6574.004240	26.274215
193.506230	6576.916584	26.279232
193.542584	6601.112392	26.284250
193.886626	6613.589821	26.289268
194.117276	6625.772622	26.294285
193.756706	6647.735342	26.299303
194.683174	6648.143107	26.304320
194.411792	6670.104427	26.309338
194.772671	6674.602668	26.314356
194.996030	6699.428383	26.319373
194.984382	6709.027087	26.324391
195.204084	6717.401950	26.329408
195.388458	6728.312599	26.334426
195.852999	6739.249163	26.339444
197.101906	6731.432330	26.344461
197.384372	6726.943212	26.349479
197.538968	6725.606227	26.354496
197.493745	6722.971328	26.359514
197.549561	6730.429046	26.364532
197.828407	6727.919879	26.369549
197.799357	6726.596082	26.374567
198.139825	6724.105030	26.379584
198.017515	6741.697824	26.384602
198.438180	6741.995882	26.389620
198.144352	6753.654723	26.394637
198.254825	6767.221805	26.399655
198.590322	6780.230871	26.404672
198.594448	6798.758134	26.409690
198.350635	6804.754970	26.414708
198.983658	6813.489681	26.419725
199.014220	6823.516223	26.424743
199.340935	6846.010094	26.429760
199.583135	6850.902241	26.434778
200.114686	6852.438177	26.439796
200.038218	6854.754104	26.444813
200.167034	6887.699170	26.449831
200.566516	6877.711661	26.454848
200.563801	6890.030325	26.459866
200.942461	6898.843585	26.464884
200.965990	6916.020875	26.469901
201.216722	6922.333340	26.474919
201.019431	6926.678658	26.479936
201.122990	6947.854992	26.484954
201.920535	6957.528898	26.489972
202.021129	6961.207204	26.494989
202.067170	6970.728742	26.500007
202.697784	6984.411217	26.505024
202.789638	6988.583268	26.510042
202.557840	6984.971128	26.515060
203.447402	7000.893217	26.520077
203.312912	7024.186262	26.525095
203.762146	7019.147921	26.530112
203.367685	7029.959624	26.535130
203.576913	7046.572165	26.540148
204.298430	7049.704648	26.545165
204.442205	7074.971875	26.550183
204.804028	7084.129094	26.555200
204.958721	7083.611231	26.560218
204.702950	7097.830200	26.565236
205.653523	7108.342837	26.570253
205.334067	7111.323007	26.575271
205.708072	7121.787319	26.580288
205.786987	7134.730616	26.585306
206.196459	7147.873411	26.590324
206.623353	7140.040960	26.595341
206.509894	7159.513688	26.600359
206.769738	7163.187633	26.605376
207.041544	7163.400165	26.610394
206.939078	7172.909481	26.615412
207.330981	7186.860222	26.620429
207.482632	7191.274443	26.625447
207.796998	7203.180697	26.630464
207.554112	7214.764458	26.635482
207.578233	7224.671022	26.640500
208.358028	7248.856918	26.645517
208.172644	7250.447440	26.650535
208.595976	7271.287508	26.655552
209.171654	7276.767114	26.660570
209.143255	7289.752787	26.665588
209.955456	7303.416394	26.670605
209.725031	7315.876412	26.675623
210.153724	7310.430228	26.680640
210.194625	7316.587890	26.685658
210.056348	7328.080309	26.690676
210.478122	7342.044340	26.695693
210.323922	7350.569889	26.700711
210.601272	7361.197717	26.705728
210.791637	7367.199808	26.710746
210.839303	7388.606566	26.715764
211.558415	7391.925412	26.720781
211.413434	7404.010545	26.725799
211.837554	7428.450374	26.730816
212.192706	7426.704283	26.735834
212.265756	7457.462176	26.740852
212.625211	7460.673025	26.745869
212.399699	7471.419931	26.750887
212.880016	7493.271656	26.755904
213.121903	7495.800223	26.760922
212.937378	7504.688501	26.765940
213.650404	7514.054636	26.770957
213.859618	7523.058664	26.775975
213.962604	7527.267603	26.780992
213.852691	7546.141575	26.786010
213.632127	7565.646774	26.791028
214.337004	7573.657904	26.796045
214.441978	7591.111471	26.801063
214.647944	7605.357353	26.806080
215.288270	7608.861054	26.811098
215.062674	7627.699206	26.816116
215.906706	7646.091830	26.821133
215.740764	7656.462686	26.826151
215.761254	7661.673132	26.831168
215.782989	7681.891243	26.836186
216.180610	7688.167792	26.841204
216.530801	7702.239347	26.846221
216.423495	7713.973445	26.851239
216.947421	7742.763355	26.856256
217.349068	7746.131092	26.861274
217.240004	7764.034741	26.866292
217.697759	7769.728676	26.871309
217.739773	7792.053005	26.876327
218.030862	7807.384549	26.881344
218.593032	7819.993677	26.886362
218.393574	7836.515839	26.891380
218.436862	7838.104655	26.896397
218.572570	7859.996030	26.901415
219.226896	7873.869113	26.906432
220.039983	7882.122362	26.911450
219.777730	7895.609768	26.916468
219.399397	7909.978220	26.921485
219.907767	7919.320314	26.926503
220.246106	7936.061207	26.931520
220.841020	7947.522038	26.936538
220.642888	7975.101131	26.941556
220.953752	7976.096467	26.946573
221.252345	7992.817243	26.951591
221.685916	8018.914533	26.956608
222.180761	8011.464222	26.961626
222.562501	8019.511946	26.966644
222.741232	8014.156687	26.971661
222.818430	8037.045813	26.976679
223.214404	8043.611080	26.981696
223.417731	8037.647553	26.986714
223.452282	8052.795101	26.991732
223.747942	8059.302998	26.996749
223.874521	8074.313967	27.001767
223.705150	8086.361919	27.006784
223.961256	8083.629462	27.011802
224.077537	8115.836344	27.016820
224.253341	8117.467760	27.021837
224.009657	8136.281160	27.026855
224.304891	8152.362250	27.031872
225.096048	8162.004093	27.036890
225.018710	8190.165299	27.041908
225.449537	8200.034823	27.046925
226.154352	8218.736400	27.051943
227.845728	8193.706207	27.056960
229.061404	8157.866514	27.061978
229.283907	8146.128965	27.066996
229.313641	8118.209170	27.072013
229.159277	8104.006504	27.077031
228.804012	8080.841572	27.082048
229.193754	8062.124749	27.087066
229.162565	8052.557027	27.092084
228.977883	8058.788695	27.097101
229.316719	8049.302854	27.102119
229.033733	8045.090863	27.107136
229.405440	8043.500287	27.112154
229.354180	8047.448268	27.117172
229.135604	8048.609567	27.122189
229.402731	8051.505043	27.127207
229.206907	8055.170628	27.132224
229.334325	8063.816757	27.137242
229.128434	8086.562370	27.142260
229.345969	8107.536198	27.147277
229.400245	8123.083057	27.152295
229.590661	8152.630194	27.157312
229.661305	8183.542705	27.162330
229.767825	8206.001837	27.167348
230.049482	8235.018798	27.172365
230.730205	8263.476390	27.177383
230.723979	8297.692989	27.182400
230.969528	8313.840003	27.187418
231.232518	8335.758147	27.192436
231.646318	8350.730317	27.197453
231.932705	8372.267303	27.202471
232.126026	8396.463392	27.207488
232.643007	8417.363452	27.212506
232.864795	8442.739623	27.217524
233.261162	8455.440616	27.222541
234.122392	8469.276692	27.227559
234.113116	8482.612275	27.232576
234.802329	8485.800052	27.237594
234.622640	8501.032463	27.242612
234.794545	8508.269279	27.247629
235.428487	8521.564186	27.252647
235.295688	8546.085670	27.257664
235.480146	8541.954998	27.262682
235.474804	8561.762013	27.267700
235.974767	8573.717232	27.272717
236.230751	8588.730816	27.277735
236.206023	8607.625760	27.282752
236.424174	8610.784703	27.287770
236.794002	8638.844827	27.292788
236.474264	8645.667910	27.297805
237.364966	8667.475119	27.302823
237.293493	8681.642815	27.307840
237.670751	8692.072178	27.312858
238.023999	8713.059700	27.317876
238.179747	8722.467165	27.322893
238.543866	8730.172360	27.327911
239.008436	8747.628098	27.332928
239.342462	8744.506042	27.337946
239.716876	8766.584294	27.342964
239.935651	8781.556977	27.347981
240.296217	8791.145504	27.352999
240.021398	8801.308321	27.358016
240.226840	8806.517556	27.363034
240.437730	8816.541384	27.368052
240.453121	8831.715699	27.373069
240.842844	8853.874242	27.378087
240.612037	8876.412422	27.383104
240.778236	8881.466713	27.388122
241.329527	8909.721671	27.393140
241.635860	8928.161018	27.398157
242.139668	8937.188585	27.403175
242.006641	8967.466863	27.408192
242.432529	8980.424905	27.413210
242.760217	8996.161146	27.418228
243.208861	9010.030015	27.423245
243.468561	9022.300422	27.428263
243.641302	9039.443390	27.433280
244.111640	9052.646187	27.438298
243.780124	9066.453311	27.443316
243.917336	9081.000258	27.448333
244.149405	9099.749916	27.453351
244.507787	9112.342732	27.458368
244.424656	9137.155429	27.463386
244.957727	9150.315585	27.468404
245.046770	9178.869187	27.473421
245.692441	9174.454537	27.478439
245.921265	9200.674438	27.483456
246.616145	9197.263885	27.488474
246.887208	9203.165821	27.493492
246.897311	9226.033925	27.498509
247.766105	9213.534364	27.503527
247.987419	9216.387250	27.508544
247.937008	9212.345849	27.513562
248.368254	9219.441426	27.518580
248.382021	9238.033729	27.523597
249.206244	9226.763391	27.528615
249.410587	9220.583410	27.533632
249.861096	9221.770688	27.538650
249.913227	9218.581154	27.543668
250.023601	9228.209153	27.548685
249.914407	9216.629922	27.553703
250.055579	9233.156008	27.558720
250.364607	9259.972413	27.563738
250.719332	9255.171236	27.568756
250.249275	9258.886598	27.573773
251.018053	9271.701250	27.578791
250.934059	9292.397449	27.583808
250.967683	9310.554051	27.588826
251.308742	9325.186303	27.593844
251.143798	9345.152363	27.598861
251.515206	9353.972137	27.603879
251.716891	9375.415839	27.608896
252.067860	9398.629318	27.613914
252.517189	9415.324966	27.618932
252.310944	9446.217388	27.623949
252.360517	9454.874842	27.628967
252.648383	9491.763750	27.633984
252.905276	9520.424781	27.639002
253.967770	9537.774947	27.644020
254.232497	9557.758898	27.649037
254.568118	9560.235987	27.654055
255.165160	9585.560287	27.659072
255.264576	9594.579794	27.664090
255.410387	9597.706839	27.669108
255.389224	9629.691454	27.674125
256.421547	9617.855302	27.679143
256.796636	9635.464744	27.684160
256.761325	9642.654575	27.689178
257.387988	9643.194993	27.694196
257.347103	9650.222682	27.699213
257.610026	9667.846070	27.704231
258.548811	9670.541226	27.709248
258.562112	9681.233386	27.714266
258.498601	9668.339294	27.719284
258.708298	9684.670905	27.724301
259.008630	9685.473523	27.729319
258.837213	9705.988621	27.734336
259.104776	9708.933961	27.739354
259.199277	9728.912535	27.744372
259.575636	9745.882201	27.749389
259.358867	9750.622259	27.754407
259.425911	9767.246294	27.759424
259.606678	9799.675100	27.764442
260.397503	9808.803580	27.769460
260.256949	9841.540317	27.774477
260.452824	9853.630533	27.779495
260.970946	9876.128395	27.784512
261.251044	9897.072119	27.789530
261.724868	9920.056386	27.794548
261.966461	9932.067374	27.799565
262.102161	9938.408823	27.804583
262.530783	9950.491952	27.809600
262.553406	9968.103602	27.814618
263.092190	9984.814919	27.819636
262.978404	10002.817177	27.824653
263.435739	10023.051740	27.829671
263.281276	10038.280628	27.834688
263.367815	10065.224370	27.839706
263.797756	10078.821544	27.844724
264.448336	10108.211538	27.849741
264.552775	10116.644372	27.854759
264.706497	10144.783223	27.859776
264.875750	10165.334476	27.864794
265.351801	10186.554841	27.869812
265.275864	10225.324157	27.874829
266.011265	10240.353386	27.879847
265.596592	10254.146980	27.884864
266.011809	10272.845522	27.889882
266.560142	10286.264062	27.894900
266.777744	10312.318264	27.899917
267.392601	10321.877279	27.904935
268.353998	10332.804679	27.909952
268.438582	10354.744990	27.914970
268.898482	10344.014200	27.919988
268.976527	10365.021254	27.925005
269.175038	10375.047329	27.930023
269.389073	10386.741805	27.935040
269.630072	10403.179242	27.940058
269.946570	10402.474467	27.945076
270.015505	10424.212639	27.950093
270.335477	10443.433777	27.955111
270.873375	10453.235704	27.960128
271.060912	10469.370111	27.965146
271.540669	10472.568683	27.970164
271.536451	10503.747847	27.975181
271.819110	10499.158388	27.980199
271.916672	10514.509719	27.985216
272.294997	10542.577283	27.990234
272.541460	10553.611805	27.995252
272.751820	10561.315074	28.000269
272.682981	10582.631225	28.005287
273.125931	10601.108100	28.010304
273.000721	10634.497012	28.015322
273.702137	10646.226510	28.020340
273.683811	10666.577946	28.025357
274.105566	10696.766512	28.030375
274.626590	10708.877406	28.035392
274.353379	10731.505585	28.040410
275.079552	10744.634975	28.045428
275.324694	10765.329590	28.050445
275.758407	10778.044348	28.055463
276.228334	10789.779325	28.060480
276.404909	10812.328159	28.065498
276.748635	10808.971686	28.070516
277.104202	10833.592780	28.075533
277.495631	10859.362937	28.080551
277.786830	10858.747436	28.085568
277.561015	10879.388876	28.090586
278.251312	10889.182294	28.095604
278.588880	10911.424044	28.100621
278.519880	10911.298554	28.105639
278.875522	10935.174485	28.110656
278.754257	10947.592389	28.115674
279.769096	10961.830562	28.120692
280.513992	10970.863349	28.125709
280.780880	10967.232833	28.130727
280.875561	10957.302901	28.135744
281.053063	10968.889633	28.140762
281.398990	10985.172357	28.145780
281.491321	11003.996305	28.150797
281.484761	11007.794984	28.155815
281.738980	11001.678520	28.160832
281.728101	11027.964867	28.165850
281.989697	11040.327110	28.170868
281.876948	11055.464936	28.175885
282.368371	11087.271161	28.180903
282.398693	11097.051456	28.185920
282.612028	11128.008957	28.190938
282.843653	11139.865721	28.195956
283.045114	11170.957638	28.200973
283.638845	11194.124712	28.205991
284.421050	11203.097858	28.211008
284.414395	11230.638112	28.216026
284.686131	11254.747484	28.221044
284.794987	11275.960966	28.226061
285.420680	11276.221134	28.231079
285.775043	11298.232146	28.236096
285.635119	11315.954213	28.241114
286.114298	11343.689693	28.246132
286.601304	11355.742123	28.251149
286.579658	11384.630814	28.256167
287.013462	11396.933203	28.261184
287.070815	11420.607293	28.266202
287.634785	11446.477358	28.271220
287.774856	11464.405187	28.276237
287.891129	11487.458194	28.281255
288.717405	11506.540542	28.286272
288.419001	11530.314870	28.291290
288.939484	11555.432818	28.296308
289.313901	11584.380546	28.301325
289.093569	11604.664299	28.306343
289.728001	11625.830311	28.311360
289.950996	11653.010095	28.316378
290.549372	11671.410376	28.321396
290.918091	11702.620497	28.326413
291.188342	11724.214302	28.331431
291.763640	11735.812705	28.336448
292.050472	11748.869368	28.341466
292.422247	11770.988436	28.346484
293.030070	11775.408502	28.351501
293.173224	11800.791225	28.356519
293.620953	11797.762369	28.361536
293.728346	11815.781109	28.366554
294.225199	11825.703367	28.371572
294.285373	11840.324701	28.376589
294.618685	11846.426066	28.381607
294.750645	11861.026037	28.386624
294.811773	11882.492492	28.391642
295.066665	11902.812694	28.396660
295.836738	11914.624691	28.401677
295.825005	11922.114960	28.406695
296.235663	11940.185879	28.411712
296.472192	11973.344112	28.416730
296.609265	11974.777511	28.421748
296.943079	11995.751282	28.426765
296.882532	12017.885787	28.431783
297.141909	12026.950991	28.436800
297.374163	12059.252871	28.441818
297.716560	12085.721762	28.446836
298.189109	12095.812110	28.451853
298.330933	12128.001510	28.456871
298.581533	12152.281193	28.461888
298.755713	12176.586215	28.466906
298.990043	12199.368489	28.471924
299.734452	12226.174229	28.476941
299.667069	12251.649367	28.481959
300.278371	12264.870003	28.486976
300.426321	12287.780212	28.491994
300.848906	12303.744243	28.497012
301.490208	12321.906488	28.502029
301.239940	12330.118913	28.507047
301.670396	12346.918449	28.512064
301.710251	12368.729462	28.517082
302.261633	12392.064454	28.522100
302.753240	12408.701037	28.527117
302.822460	12440.874755	28.532135
303.416247	12441.743803	28.537152
304.026098	12463.882571	28.542170
303.861382	12487.574628	28.547188
304.612770	12500.650843	28.552205
304.642713	12515.158043	28.557223
304.697778	12531.786913	28.562240
305.121394	12556.730257	28.567258
305.373391	12579.229627	28.572276
305.622466	12593.719400	28.577293
306.397144	12602.456631	28.582311
307.541542	12615.837973	28.587328
307.537125	12632.973227	28.592346
307.585596	12645.879536	28.597364
307.883866	12647.070320	28.602381
307.760921	12669.658898	28.607399
308.274746	12688.057053	28.612416
308.408407	12706.157515	28.617434
308.413354	12717.397535	28.622452
308.893606	12722.242485	28.627469
309.469524	12748.943137	28.632487
310.538492	12753.537428	28.637504
310.720801	12770.170616	28.642522
311.097808	12790.329814	28.647540
311.654987	12786.749949	28.652557
311.538339	12792.617557	28.657575
311.986201	12793.608576	28.662592
312.128965	12795.849531	28.667610
312.407285	12807.186024	28.672628
312.652916	12826.432596	28.677645
312.621652	12845.334373	28.682663
312.766055	12854.340349	28.687680
313.305287	12881.630394	28.692698
313.221726	12891.424388	28.697716
313.301118	12911.863263	28.702733
313.507508	12941.769535	28.707751
313.923464	12974.047443	28.712768
313.792234	12991.163168	28.717786
314.374119	13026.072157	28.722804
314.823506	13049.165018	28.727821
315.085181	13079.190005	28.732839
315.674771	13097.807697	28.737856
316.428752	13123.305329	28.742874
316.615490	13150.621295	28.747892
316.734731	13177.185775	28.752909
316.990827	13195.256984	28.757927
317.217020	13203.140117	28.762944
317.680319	13231.956251	28.767962
317.878503	13255.806609	28.772980
318.254648	13272.832032	28.777997
318.468027	13309.222764	28.783015
318.775701	13327.134261	28.788032
319.119524	13346.250090	28.793050
319.057655	13379.946157	28.798068
319.507595	13394.247256	28.803085
319.968264	13426.261754	28.808103
319.898441	13457.336933	28.813120
320.466527	13482.090647	28.818138
320.454162	13503.134912	28.823156
321.109396	13528.693713	28.828173
321.087312	13562.709769	28.833191
321.335023	13585.364110	28.838208
321.924161	13621.606433	28.843226
322.252576	13658.974841	28.848244
322.806714	13677.603816	28.853261
323.117874	13705.076547	28.858279
323.405231	13723.483558	28.863296
323.789200	13748.769426	28.868314
324.182053	13771.440887	28.873332
324.650460	13793.507260	28.878349
324.598216	13820.112308	28.883367
324.871755	13847.339372	28.888384
325.367256	13872.214481	28.893402
325.613133	13893.031954	28.898420
326.109562	13919.375803	28.903437
326.554880	13939.592844	28.908455
327.234283	13952.652255	28.913472
327.687345	13968.797254	28.918490
327.788512	13989.586884	28.923508
328.213216	14003.407305	28.928525
328.723590	14026.336972	28.933543
328.615063	14051.777627	28.938560
329.102343	14073.656851	28.943578
329.239858	14107.157387	28.948596
329.637226	14127.474036	28.953613
329.784388	14143.168858	28.958631
330.089921	14166.908152	28.963648
330.771251	14182.492203	28.968666
331.011023	14217.358142	28.973684
331.465921	14228.344783	28.978701
331.734384	14249.724750	28.983719
332.380268	14271.975049	28.988736
332.985912	14279.124277	28.993754
332.925115	14300.505427	28.998772
333.402552	14312.437149	29.003789
333.508833	14342.870100	29.008807
333.774379	14360.222361	29.013824
334.046055	14378.174090	29.018842
333.976242	14413.055629	29.023860
334.525223	14423.610698	29.028877
334.953809	14452.946970	29.033895
335.647223	14463.810614	29.038912
336.120268	14482.089918	29.043930
336.154999	14503.230087	29.048948
336.407578	14520.617769	29.053965
336.672911	14546.752008	29.058983
336.768712	14574.725339	29.064000
337.693309	14592.587745	29.069018
337.707383	14623.176804	29.074036
338.167777	14650.585355	29.079053
338.754453	14663.698569	29.084071
339.085584	14686.640031	29.089088
339.590320	14690.253757	29.094106
339.269910	14724.110593	29.099124
339.861836	14739.003953	29.104141
340.185122	14767.615955	29.109159
340.114140	14796.769481	29.114176
340.565612	14811.549123	29.119194
341.082552	14836.234588	29.124212
341.542284	14863.385128	29.129229
341.973749	14879.457390	29.134247
343.014574	14900.856470	29.139264
343.299369	14900.071680	29.144282
343.085014	14922.680128	29.149300
343.692488	14932.858582	29.154317
343.976952	14945.974948	29.159335
343.834967	14966.273495	29.164352
344.659606	14980.613033	29.169370
344.681870	15006.132732	29.174388
345.245046	15015.809519	29.179405
345.013543	15025.955618	29.184423
345.381736	15053.372281	29.189440
345.656800	15070.369091	29.194458
345.580020	15101.446965	29.199476
346.116042	15125.155663	29.204493
346.594083	15153.936490	29.209511
346.534746	15194.154654	29.214528
347.006755	15220.113781	29.219546
347.565626	15240.472757	29.224564
347.954878	15256.407400	29.229581
348.781728	15285.294427	29.234599
349.106094	15300.653575	29.239616
349.645675	15320.104855	29.244634
350.190589	15341.687773	29.249652
350.273314	15360.936025	29.254669
350.487446	15383.973554	29.259687
351.009629	15405.388534	29.264704
351.465656	15426.232938	29.269722
351.370550	15454.289919	29.274740
351.522687	15478.428567	29.279757
351.695064	15499.178334	29.284775
351.936730	15523.089395	29.289792
352.503555	15556.625594	29.294810
352.886176	15588.687238	29.299828
353.038270	15613.691399	29.304845
353.732324	15639.174555	29.309863
354.269812	15671.710275	29.314880
354.703859	15693.811717	29.319898
355.046189	15718.179187	29.324916
355.281507	15740.550131	29.329933
355.477849	15770.136973	29.334951
355.929510	15797.775861	29.339968
356.422741	15822.728395	29.344986
356.587974	15852.873790	29.350004
356.714294	15882.800312	29.355021
357.470565	15912.617506	29.360039
357.291288	15935.647083	29.365056
358.184350	15956.802570	29.370074
358.448355	16000.479152	29.375092
358.822799	16029.639672	29.380109
358.958806	16053.983596	29.385127
359.591666	16078.907018	29.390144
359.729388	16111.182170	29.395162
359.998768	16134.596164	29.400180
360.498470	16174.169023	29.405197
361.327368	16202.124211	29.410215
361.220554	16231.483254	29.415232
361.651159	16241.441292	29.420250
362.767287	16269.851691	29.425268
364.290015	16262.384519	29.430285
364.800852	16263.890188	29.435303
364.960510	16261.021879	29.440320
365.873827	16252.669239	29.445338
366.283065	16263.593909	29.450356
366.242651	16250.567033	29.455373
366.458609	16260.981591	29.460391
366.231333	16254.949475	29.465408
366.764212	16253.853880	29.470426
366.692026	16258.339300	29.475444
366.695278	16284.595501	29.480461
366.990491	16299.832754	29.485479
367.015203	16328.668883	29.490496
367.121165	16342.555268	29.495514
367.379418	16375.988355	29.500532
367.352034	16398.254092	29.505549
367.637869	16429.457071	29.510567
367.892138	16461.748225	29.515584
368.298831	16503.337568	29.520602
368.549829	16537.714777	29.525620
368.354420	16567.621904	29.530637
369.079346	16608.324812	29.535655
369.086756	16656.038392	29.540672
369.386702	16689.477796	29.545690
369.802925	16733.222452	29.550708
370.613383	16779.939193	29.555725
371.445044	16810.327134	29.560743
371.747046	16853.260390	29.565760
372.054320	16881.665931	29.570778
372.495639	16923.770749	29.575796
372.696977	16959.541057	29.580813
373.733650	16975.726055	29.585831
373.907238	17016.373388	29.590848
374.469423	17046.850667	29.595866
375.119261	17067.519936	29.600884
375.419693	17091.625274	29.605901
375.905009	17112.069723	29.610919
376.329765	17141.636840	29.615936
376.842044	17156.331256	29.620954
377.204152	17185.741771	29.625972
377.654726	17207.784177	29.630989
377.941778	17219.145924	29.636007
378.042909	17246.585382	29.641024
378.602833	17273.650747	29.646042
379.464614	17288.139047	29.651060
379.191143	17316.813628	29.656077
379.810647	17331.145174	29.661095
379.798056	17367.847250	29.666112
380.586197	17386.075869	29.671130
381.224127	17413.019737	29.676148
382.356731	17418.266888	29.681165
382.869377	17423.178810	29.686183
383.075470	17446.980343	29.691200
383.658241	17464.979920	29.696218
383.641289	17477.341296	29.701236
383.364184	17489.495262	29.706253
384.052811	17497.872701	29.711271
384.517945	17532.025667	29.716288
384.690114	17552.188499	29.721306
385.189835	17570.632327	29.726324
384.861587	17592.148866	29.731341
385.388347	17616.849484	29.736359
385.571700	17651.976397	29.741376
385.632574	17684.101865	29.746394
386.039894	17712.208469	29.751412
386.208672	17750.274756	29.756429
386.935063	17776.597625	29.761447
386.942477	17815.058158	29.766464
387.504178	17862.771406	29.771482
388.405510	17891.114673	29.776500
388.514716	17920.529095	29.781517
388.960510	17944.756553	29.786535
389.475185	17981.247860	29.791552
390.324133	18002.504742	29.796570
390.875207	18027.887661	29.801588
391.219354	18050.259416	29.806605
391.517272	18075.507905	29.811623
392.207752	18085.598871	29.816640
392.652338	18110.714280	29.821658
392.937561	18127.759845	29.826676
393.102744	18152.459848	29.831693
393.454295	18176.225652	29.836711
393.892360	18205.165050	29.841728
393.835159	18209.263865	29.846746
394.450865	18241.241491	29.851764
394.717667	18268.971974	29.856781
394.912470	18277.513818	29.861799
395.249549	18313.959691	29.866816
395.209731	18348.040575	29.871834
395.712535	18373.670079	29.876852
396.128680	18410.303233	29.881869
396.305510	18446.240033	29.886887
396.804538	18477.595892	29.891904
396.984100	18518.329457	29.896922
397.548034	18558.565751	29.901940
398.007996	18586.575232	29.906957
398.560023	18625.711738	29.911975
399.372621	18652.655407	29.916992
399.323725	18688.683824	29.922010
399.755307	18709.440273	29.927028
399.883907	18753.681015	29.932045
400.220804	18785.152667	29.937063
400.767090	18830.766685	29.942080
400.998054	18861.915564	29.947098
401.632328	18906.168873	29.952116
402.105228	18941.239371	29.957133
403.047651	18972.706955	29.962151
403.266285	19009.938613	29.967168
403.627386	19051.180899	29.972186
404.170876	19079.508395	29.977204
404.644378	19107.773470	29.982221
405.809645	19114.997397	29.987239
406.876325	19119.226615	29.992256
407.032149	19129.088585	29.997274
407.621595	19146.841373	30.002292
407.729540	19155.371297	30.007309
408.133962	19186.520346	30.012327
408.358451	19196.700436	30.017344
408.744044	19227.818007	30.022362
409.160060	19233.265194	30.027380
409.260587	19255.909207	30.032397
409.361145	19278.985206	30.037415
409.742426	19294.619231	30.042432
410.142769	19330.200774	30.047450
410.631036	19359.896869	30.052468
410.886010	19400.484478	30.057485
411.617210	19416.978022	30.062503
411.947976	19442.300375	30.067520
412.260091	19468.437773	30.072538
412.601321	19494.822618	30.077556
412.902521	19518.989679	30.082573
413.264618	19550.619395	30.087591
413.544685	19592.447181	30.092608
413.732563	19622.687094	30.097626
414.323171	19657.066364	30.102644
414.582086	19698.552667	30.107661
415.212023	19731.749457	30.112679
415.131141	19778.739362	30.117696
415.405906	19809.138599	30.122714
416.086828	19846.151861	30.127732
416.132641	19896.332490	30.132749
416.254702	19939.653589	30.137767
416.952002	19971.324587	30.142784
417.959975	20025.679760	30.147802
418.151601	20063.812163	30.152820
418.707303	20088.552635	30.157837
420.151757	20111.903168	30.162855
420.703262	20132.321422	30.167872
421.093382	20161.414070	30.172890
421.438545	20178.197945	30.177908
422.115413	20199.052667	30.182925
422.588484	20220.073701	30.187943
423.062741	20228.607964	30.192960
423.279166	20247.847549	30.197978
423.872694	20255.515384	30.202996
423.868427	20269.238894	30.208013
424.074569	20294.165440	30.213031
424.824986	20314.345918	30.218048
425.154638	20325.120949	30.223066
425.707657	20340.079443	30.228084
425.796040	20366.778838	30.233101
426.131837	20391.865302	30.238119
426.517117	20412.991028	30.243136
426.563670	20419.609909	30.248154
427.170107	20459.280873	30.253172
427.537707	20499.218635	30.258189
427.901929	20524.808246	30.263207
428.115756	20559.642957	30.268224
428.367444	20601.903662	30.273242
428.413323	20630.609696	30.278260
428.622967	20687.901295	30.283277
429.052936	20726.862761	30.288295
429.628375	20778.566218	30.293312
429.482830	20828.571721	30.298330
430.456859	20877.825385	30.303348
431.010763	20922.270807	30.308365
431.993094	20948.106831	30.313383
432.765416	20974.572180	30.318400
433.044106	21013.116397	30.323418
433.613633	21043.159880	30.328436
434.100262	21075.288930	30.333453
434.545529	21110.564068	30.338471
435.134335	21141.088563	30.343488
435.344562	21180.276780	30.348506
435.947270	21208.572817	30.353524
435.996104	21246.052069	30.358541
436.489927	21277.027752	30.363559
437.129425	21300.817965	30.368576
437.390929	21351.050667	30.373594
437.599572	21371.896330	30.378612
438.203063	21425.831294	30.383629
438.366173	21461.727954	30.388647
439.112532	21492.307327	30.393664
439.218351	21535.212670	30.398682
439.842800	21576.713839	30.403700
440.165743	21626.588700	30.408717
440.431957	21665.384024	30.413735
440.953853	21694.222502	30.418752
441.130080	21753.021157	30.423770
441.523621	21791.369902	30.428788
442.238118	21845.032336	30.433805
442.610923	21883.204985	30.438823
443.509839	21928.765697	30.443840
443.762658	21961.214357	30.448858
444.969113	21992.478209	30.453876
445.521862	22029.654749	30.458893
445.590843	22062.468412	30.463911
446.522349	22089.000527	30.468928
446.382053	22130.237469	30.473946
446.772698	22163.738979	30.478964
447.004632	22194.800843	30.483981
447.469549	22233.397326	30.488999
447.853357	22275.665501	30.494016
448.174133	22314.645617	30.499034
448.946815	22348.503461	30.504052
449.115911	22383.967465	30.509069
449.294129	22430.827104	30.514087
449.733975	22464.965947	30.519104
450.573392	22512.318322	30.524122
451.296997	22543.464722	30.529140
451.960478	22573.142120	30.534157
451.892967	22604.962461	30.539175
452.497354	22628.736729	30.544192
452.950226	22672.041426	30.549210
453.299694	22690.388141	30.554228
454.024940	22728.485233	30.559245
454.039731	22764.246875	30.564263
454.739043	22805.092126	30.569280
454.656523	22844.968284	30.574298
455.278843	22881.490214	30.579316
455.478174	22925.421100	30.584333
456.206235	22973.632140	30.589351
456.785277	23015.880769	30.594368
457.052279	23057.678317	30.599386
457.649808	23092.990642	30.604404
458.143926	23136.231327	30.609421
458.300453	23177.506656	30.614439
459.143552	23213.125352	30.619456
459.305082	23259.431835	30.624474
459.958417	23290.168679	30.629492
460.256375	23326.251880	30.634509
460.645140	23373.348791	30.639527
461.552217	23422.341888	30.644544
461.556949	23457.546862	30.649562
462.329751	23509.039808	30.654580
462.657432	23552.768073	30.659597
463.001536	23607.527322	30.664615
463.816789	23639.884193	30.669632
464.060259	23691.017769	30.674650
464.730929	23729.837360	30.679668
465.145760	23770.978184	30.684685
465.452863	23822.588852	30.689703
466.001708	23853.500186	30.694720
467.607970	23863.461476	30.699738
468.926207	23880.462718	30.704756
469.305926	23895.807968	30.709773
469.269622	23919.603731	30.714791
470.392570	23936.738392	30.719808
470.492996	23958.322713	30.724826
470.796902	23989.256055	30.729844
471.368244	24012.764942	30.734861
471.520155	24035.996599	30.739879
471.663223	24064.326448	30.744896
472.001591	24091.094265	30.749914
472.209746	24130.789530	30.754932
472.935922	24162.659145	30.759949
472.755817	24210.549870	30.764967
473.425242	24242.053743	30.769984
473.620413	24287.535830	30.775002
473.680875	24340.944197	30.780020
474.395425	24389.163069	30.785037
474.976103	24434.303968	30.790055
475.491353	24477.216534	30.795072
475.752456	24524.650070	30.800090
476.703428	24554.997557	30.805108
478.061407	24571.917201	30.810125
478.584474	24613.857385	30.815143
479.063020	24642.482565	30.820160
479.508100	24675.841206	30.825178
479.859491	24701.261055	30.830196
480.182714	24732.485857	30.835213
480.499225	24769.092593	30.840231
480.753365	24800.909334	30.845248
481.330949	24837.204761	30.850266
481.621064	24872.942436	30.855284
481.822585	24912.492375	30.860301
482.532038	24957.155929	30.865319
483.050808	24982.482160	30.870336
483.131389	25017.387570	30.875354
483.709263	25050.384246	30.880372
484.008293	25095.128943	30.885389
484.179267	25136.270976	30.890407
484.845082	25184.970146	30.895424
485.430439	25224.835545	30.900442
486.034370	25274.078291	30.905460
486.575895	25312.516051	30.910477
486.264385	25359.939763	30.915495
486.875625	25401.144933	30.920512
487.408838	25458.089746	30.925530
487.851755	25520.304577	30.930548
488.620253	25573.088204	30.935565
488.657217	25608.951464	30.940583
489.337625	25656.643366	30.945600
489.572692	25722.650087	30.950618
489.725980	25781.977409	30.955636
490.625835	25832.270269	30.960653
490.651663	25885.805895	30.965671
491.420842	25940.612397	30.970688
492.268084	25997.040009	30.975706
492.660659	26068.024530	30.980724
493.651200	26108.496541	30.985741
494.585839	26165.828083	30.990759
495.250334	26201.108899	30.995776
495.978720	26236.177301	31.000794
496.705956	26279.220034	31.005812
497.406326	26303.742097	31.010829
497.499004	26351.464146	31.015847
498.054771	26383.870890	31.020864
498.324840	26423.050169	31.025882
498.706481	26458.258626	31.030900
499.263533	26503.572916	31.035917
499.972597	26540.963590	31.040935
500.313924	26584.894466	31.045952
501.235792	26622.202657	31.050970
501.566923	26664.662343	31.055988
502.143471	26688.754445	31.061005
502.432391	26740.413179	31.066023
502.756152	26771.054877	31.071040
503.604248	26811.113740	31.076058
503.648300	26856.523623	31.081076
504.225766	26889.773095	31.086093
504.358679	26943.597037	31.091111
505.200888	26979.976060	31.096128
505.966428	27031.304148	31.101146
506.357334	27079.486538	31.106164
506.875734	27113.156329	31.111181
506.855442	27171.917907	31.116199
507.124664	27207.774301	31.121216
507.961319	27249.877024	31.126234
508.438025	27327.726353	31.131252
509.075616	27353.408572	31.136269
509.613058	27420.188570	31.141287
510.273151	27463.034056	31.146304
510.585778	27502.905859	31.151322
510.843671	27550.827744	31.156340
511.699949	27605.539896	31.161357
511.650264	27659.661367	31.166375
512.272803	27708.327535	31.171392
513.173697	27761.392397	31.176410
513.137752	27815.931631	31.181428
513.685750	27863.386637	31.186445
514.158603	27928.103597	31.191463
514.574782	27981.615569	31.196480
515.369877	28033.578949	31.201498
515.862994	28086.122616	31.206516
517.015623	28105.881197	31.211533
517.843084	28149.858333	31.216551
518.166691	28191.960226	31.221568
518.634834	28225.832958	31.226586
519.013515	28256.023354	31.231604
519.671654	28304.284639	31.236621
520.211375	28337.811307	31.241639
520.722077	28380.179121	31.246656
521.218069	28416.577656	31.251674
521.395998	28463.215604	31.256692
522.133371	28490.599094	31.261709
522.964906	28535.630202	31.266727
523.485462	28574.419412	31.271744
523.955914	28602.901086	31.276762
524.256797	28641.610205	31.281780
524.798573	28692.803708	31.286797
525.218382	28736.708070	31.291815
525.275279	28790.613449	31.296832
525.804703	28830.029552	31.301850
526.216813	28902.688144	31.306868
526.901242	28950.602984	31.311885
527.272957	29012.457298	31.316903
527.808378	29061.160649	31.321920
528.468754	29110.720422	31.326938
528.837919	29166.064169	31.331956
529.311257	29220.059449	31.336973
530.146763	29273.502593	31.341991
530.478870	29329.591245	31.347008
530.795151	29389.541103	31.352026
531.159778	29450.331798	31.357044
531.896541	29507.931254	31.362061
532.224410	29570.286984	31.367079
532.477464	29641.088431	31.372096
533.198907	29703.066933	31.377114
533.674941	29778.387608	31.382132
534.494566	29832.295717	31.387149
535.183265	29899.826745	31.392167
535.783576	29941.754393	31.397184
536.574610	29992.850363	31.402202
537.355327	30058.625177	31.407220
537.834558	30104.529673	31.412237
538.351814	30167.878293	31.417255
538.581691	30226.545500	31.422272
539.813661	30274.051221	31.427290
539.849157	30335.483325	31.432308
540.267031	30393.561427	31.437325
541.146611	30443.394607	31.442343
541.373192	30486.142837	31.447360
541.801121	30550.870659	31.452378
542.590131	30600.447991	31.457396
542.996067	30657.462530	31.462413
543.780450	30704.318080	31.467431
544.235391	30773.642371	31.472448
544.927897	30821.419009	31.477466
545.423675	30889.399203	31.482484
545.787339	30939.568728	31.487501
546.156957	31002.755565	31.492519
546.714228	31063.488297	31.497536
547.744885	31106.773392	31.502554
548.117687	31162.908466	31.507572
549.020023	31213.304829	31.512589
549.718470	31269.518680	31.517607
550.459468	31320.036799	31.522624
551.259450	31355.930299	31.527642
551.861242	31397.466773	31.532660
552.361874	31435.448424	31.537677
552.919849	31470.874357	31.542695
553.107276	31527.300106	31.547712
553.791771	31558.685420	31.552730
554.171197	31606.563512	31.557748
554.405627	31636.332488	31.562765
554.940151	31679.672989	31.567783
555.019992	31728.863275	31.572800
555.647224	31772.441030	31.577818
556.057715	31828.518322	31.582836
556.426337	31885.587201	31.587853
557.115640	31941.971944	31.592871
557.608450	32001.734150	31.597888
558.240755	32043.551057	31.602906
558.845462	32097.479714	31.607924
559.296485	32154.923885	31.612941
559.872599	32217.844122	31.617959
560.241115	32288.504500	31.622976
561.093430	32339.571863	31.627994
561.553134	32416.294892	31.633012
561.924888	32465.924676	31.638029
562.250018	32533.333692	31.643047
563.226093	32588.079378	31.648064
564.037786	32630.924953	31.653082
564.487494	32704.918276	31.658100
564.862994	32763.418260	31.663117
566.066841	32813.437794	31.668135
566.701427	32866.543406	31.673152
567.257634	32915.746224	31.678170
567.851305	32976.548900	31.683188
568.306693	33020.871410	31.688205
569.338419	33079.679985	31.693223
569.418834	33130.253021	31.698240
570.152008	33190.531532	31.703258
570.574175	33241.436260	31.708276
570.953354	33305.724700	31.713293
571.736173	33358.677787	31.718311
572.147398	33414.027873	31.723328
572.956377	33471.435790	31.728346
573.898666	33521.731116	31.733364
574.633168	33571.243789	31.738381
575.215450	33613.407200	31.743399
575.609685	33677.104378	31.748416
576.116394	33717.816374	31.753434
576.325582	33780.291863	31.758452
576.778848	33841.284902	31.763469
577.634073	33894.947050	31.768487
577.890332	33958.305243	31.773504
578.241688	34013.824916	31.778522
578.569027	34081.618106	31.783540
578.990189	34158.039469	31.788557
579.680467	34207.349819	31.793575
580.520499	34278.785524	31.798592
581.287170	34336.790220	31.803610
582.305478	34395.453893	31.808628
583.136049	34462.877786	31.813645
584.211424	34511.926213	31.818663
584.150980	34568.121900	31.823680
584.538867	34617.354211	31.828698
585.212511	34682.160434	31.833716
585.693242	34738.800117	31.838733
585.941661	34795.049365	31.843751
586.649931	34856.281229	31.848768
587.354855	34916.838508	31.853786
587.742894	34977.672679	31.858804
587.745520	35051.721567	31.863821
588.656538	35100.331833	31.868839
589.070514	35177.623447	31.873856
589.823393	35240.455564	31.878874
590.307051	35323.192791	31.883892
590.980772	35374.023944	31.888909
591.709639	35444.179358	31.893927
592.214584	35503.140202	31.898944
593.043581	35563.764269	31.903962
593.331775	35628.937735	31.908980
593.970170	35683.793184	31.913997
594.260568	35746.268344	31.919015
594.758904	35808.387278	31.924032
595.672877	35886.608827	31.929050
596.262005	35947.274020	31.934068
596.208486	36008.311242	31.939085
597.079360	36082.835612	31.944103
597.528962	36154.428830	31.949120
598.347472	36224.916410	31.954138
599.298410	36282.306606	31.959156
599.741132	36357.146228	31.964173
600.487695	36425.314181	31.969191
600.771562	36492.274685	31.974208
601.618916	36557.585891	31.979226
602.077172	36631.903308	31.984244
602.445865	36701.820436	31.989261
603.561758	36763.167843	31.994279
604.175505	36838.978407	31.999296
605.287277	36896.204976	32.004314
606.281137	36945.819610	32.009332
606.527388	37003.812019	32.014349
607.545793	37059.703752	32.019367
608.986993	37100.463922	32.024384
610.849008	37111.854995	32.029402
611.446997	37137.296061	32.034420
612.009347	37172.644206	32.039437
612.624373	37204.868457	32.044455
613.280945	37238.534587	32.049472
613.352699	37272.559862	32.054490
613.631869	37301.462860	32.059508
613.643170	37345.124915	32.064525
614.293962	37378.767015	32.069543
614.856029	37434.050773	32.074560
614.915441	37473.677727	32.079578
615.400154	37530.019355	32.084596
615.605694	37596.835977	32.089613
616.600730	37654.671408	32.094631
616.785772	37721.712835	32.099648
617.337845	37772.981269	32.104666
618.140730	37843.016923	32.109684
618.416840	37918.427239	32.114701
619.464978	37969.806393	32.119719
620.149418	38043.893186	32.124736
620.714999	38093.566303	32.129754
621.455938	38160.823209	32.134772
621.799328	38225.056239	32.139789
622.944553	38285.305499	32.144807
623.534023	38344.652963	32.149824
623.774381	38404.749855	32.154842
624.726654	38462.907450	32.159860
624.872018	38533.045473	32.164877
625.542212	38584.015651	32.169895
626.297190	38652.566200	32.174912
626.861444	38722.338682	32.179930
627.789339	38781.830233	32.184948
628.328427	38850.436314	32.189965
628.710371	38906.130080	32.194983
629.212693	38972.766731	32.200000
629.527345	39048.134280	32.205018
630.481157	39113.282331	32.210036
630.416566	39190.610542	32.215053
631.518364	39256.517365	32.220071
631.882397	39339.681034	32.225088
632.166761	39401.030225	32.230106
632.996990	39475.770982	32.235124
633.046904	39555.846934	32.240141
633.710598	39622.313946	32.245159
634.512204	39710.236333	32.250176
635.067775	39787.779750	32.255194
635.504517	39860.977501	32.260212
636.408984	39942.305347	32.265229
637.414617	40014.806315	32.270247
638.158265	40085.112940	32.275264
638.897723	40148.191560	32.280282
639.987526	40201.685108	32.285300
640.753783	40271.470984	32.290317
641.913642	40324.138808	32.295335
642.424713	40386.855260	32.300352
643.308164	40450.870677	32.305370
644.406073	40493.725296	32.310388
644.690141	40550.447330	32.315405
645.438300	40597.353648	32.320423
646.058827	40642.055708	32.325440
647.026871	40697.777551	32.330458
648.013734	40724.835344	32.335476
648.486078	40784.737357	32.340493
648.907074	40834.552410	32.345511
649.078888	40886.549338	32.350528
649.269803	40949.077787	32.355546
649.723141	41012.854045	32.360564
650.100420	41081.451132	32.365581
650.204451	41162.645788	32.370599
650.783219	41233.574523	32.375616
651.910836	41315.231275	32.380634
653.086435	41385.085993	32.385652
653.697155	41464.351015	32.390669
654.235676	41536.354654	32.395687
655.040889	41612.263703	32.400704
655.517149	41684.483461	32.405722
656.190488	41748.629825	32.410740
656.628377	41828.654378	32.415757
656.940658	41903.393123	32.420775
657.336825	41986.869631	32.425792
657.938468	42073.362140	32.430810
658.638985	42157.391883	32.435828
659.404548	42244.031609	32.440845
660.239018	42330.148843	32.445863
660.916365	42418.938251	32.450880
661.492966	42504.401382	32.455898
662.374364	42576.326867	32.460916
663.327764	42648.796339	32.465933
664.284115	42726.235028	32.470951
665.071338	42791.606865	32.475968
665.456102	42878.969477	32.480986
666.506096	42947.351262	32.486004
667.134094	43024.972004	32.491021
667.828442	43100.514047	32.496039
668.229651	43168.246627	32.501056
668.674670	43244.875710	32.506074
669.399791	43313.757960	32.511092
670.271686	43400.151773	32.516109
671.083857	43468.044531	32.521127
671.493898	43544.623820	32.526144
671.590943	43623.967552	32.531162
672.410348	43702.806482	32.536180
673.311248	43783.795014	32.541197
674.015768	43863.948222	32.546215
674.572325	43943.258056	32.551232
674.814243	44030.371919	32.556250
676.041947	44098.898919	32.561268
676.780016	44179.543624	32.566285
677.292136	44256.194125	32.571303
678.417153	44321.786776	32.576320
679.425817	44387.073755	32.581338
680.264191	44439.633002	32.586356
680.597742	44505.398756	32.591373
681.374287	44565.499246	32.596391
681.689591	44619.279389	32.601408
682.894478	44693.208547	32.606426
683.358900	44762.404647	32.611444
683.805453	44825.112050	32.616461
684.011965	44892.693739	32.621479
684.968051	44966.731592	32.626496
684.833633	45051.872886	32.631514
685.880175	45124.405960	32.636532
686.742291	45213.291629	32.641549
686.809536	45297.049088	32.646567
688.058099	45367.680243	32.651584
689.019364	45437.746782	32.656602
689.820512	45514.979641	32.661620
690.612586	45595.097282	32.666637
691.102147	45673.554023	32.671655
691.900253	45741.665753	32.676672
692.486258	45836.400902	32.681690
693.298103	45903.686771	32.686708
694.010506	45989.620063	32.691725
694.515201	46063.544550	32.696743
695.514143	46141.801824	32.701760
695.958090	46228.494429	32.706778
696.446243	46303.995178	32.711796
696.963898	46391.225745	32.716813
697.763833	46472.918391	32.721831
698.569872	46551.282017	32.726848
699.281290	46643.540429	32.731866
700.424719	46719.521397	32.736884
700.735213	46799.193575	32.741901
701.582522	46878.192749	32.746919
702.643264	46961.672619	32.751936
703.000843	47046.741192	32.756954
703.744003	47129.781893	32.761972
704.559142	47220.301656	32.766989
705.183514	47300.782784	32.772007
706.491343	47367.202014	32.777024
707.104264	47447.300391	32.782042
707.605091	47529.072507	32.787060
708.648820	47598.268062	32.792077
708.811572	47686.011934	32.797095
709.648555	47757.863555	32.802112
710.213192	47842.879200	32.807130
711.171800	47927.731914	32.812148
712.395146	48002.814173	32.817165
712.434610	48072.582421	32.822183
713.087476	48153.103473	32.827200
713.973495	48242.615206	32.832218
714.944056	48302.998536	32.837236
715.576315	48385.182004	32.842253
716.330460	48469.578402	32.847271
717.257259	48540.814853	32.852288
717.639273	48619.611107	32.857306
718.144601	48702.451805	32.862324
719.003510	48774.733127	32.867341
719.592773	48857.181573	32.872359
720.446732	48940.492840	32.877376
721.237202	49023.284425	32.882394
721.854884	49111.287757	32.887412
722.300968	49191.029516	32.892429
723.328007	49272.393260	32.897447
724.202851	49339.598702	32.902464
724.928936	49435.879212	32.907482
725.198138	49509.451893	32.912500
726.137568	49587.692144	32.917517
726.813453	49657.726859	32.922535
727.231148	49718.951814	32.927552
727.771344	49807.208073	32.932570
728.768384	49874.445632	32.937588
729.619029	49956.299523	32.942605
729.989420	50035.330915	32.947623
730.788177	50123.068774	32.952640
731.285688	50205.831969	32.957658
731.800489	50301.090646	32.962676
732.727222	50386.638598	32.967693
733.045342	50481.087505	32.972711
734.003373	50573.105978	32.977728
734.691295	50660.931010	32.982746
735.489917	50758.504229	32.987764
736.454608	50852.127458	32.992781
736.952621	50949.827354	32.997799
737.822600	51035.874019	33.002816
738.835824	51112.105666	33.007834
739.651418	51209.419336	33.012852
740.709367	51289.055545	33.017869
740.959778	51373.399842	33.022887
742.076035	51447.366759	33.027904
742.674460	51554.926946	33.032922
743.268234	51646.834109	33.037940
744.041037	51741.864356	33.042957
744.876316	51841.054184	33.047975
745.774811	51922.178785	33.052992
746.503098	52016.882942	33.058010
746.790707	52111.079510	33.063028
747.861376	52202.537392	33.068045
748.499610	52300.505086	33.073063
749.271874	52389.037815	33.078080
750.368755	52479.980923	33.083098
751.325694	52571.901654	33.088116
752.151116	52648.031516	33.093133
752.907372	52747.896117	33.098151
753.897712	52828.889208	33.103168
754.475028	52922.934194	33.108186
754.851974	53007.163466	33.113204
755.794030	53095.292141	33.118221
756.044139	53189.411682	33.123239
756.654770	53288.639844	33.128256
757.588166	53380.473516	33.133274
757.951730	53481.152562	33.138292
759.123097	53575.746489	33.143309
759.659104	53678.204857	33.148327
760.871591	53770.960679	33.153344
761.554227	53859.306443	33.158362
762.049563	53974.308142	33.163380
762.936021	54067.429076	33.168397
763.728284	54176.784804	33.173415
764.532100	54261.447724	33.178432
765.164294	54364.999383	33.183450
766.115202	54464.600312	33.188468
766.540898	54558.968941	33.193485
767.087212	54679.115691	33.198503
768.402440	54774.291743	33.203520
769.076134	54869.682169	33.208538
769.360137	54969.737555	33.213556
770.398360	55061.340525	33.218573
770.928503	55170.189251	33.223591
771.824265	55278.876781	33.228608
773.128999	55374.822010	33.233626
773.351611	55483.148521	33.238644
774.824655	55571.819355	33.243661
775.971560	55673.447388	33.248679
776.692229	55740.097059	33.253696
777.393639	55839.449357	33.258714
778.036675	55910.346012	33.263732
779.351806	55976.063720	33.268749
779.759147	56065.198024	33.273767
780.698500	56147.900341	33.278784
780.975432	56224.482619	33.283802
781.536618	56304.107915	33.288820
782.593018	56398.361643	33.293837
783.057790	56489.415568	33.298855
784.077835	56577.035017	33.303872
784.706040	56670.286900	33.308890
785.632266	56768.127881	33.313908
786.137939	56854.001431	33.318925
786.714522	56948.552263	33.323943
787.444928	57046.427116	33.328960
788.309351	57151.408154	33.333978
789.116901	57263.558773	33.338996
790.122798	57346.286615	33.344013
790.881990	57448.234522	33.349031
792.019905	57541.753415	33.354048
792.457224	57635.742926	33.359066
793.211692	57728.871360	33.364084
794.177659	57828.796303	33.369101
794.510515	57944.321903	33.374119
795.509377	58050.397545	33.379136
796.586576	58141.117186	33.384154
797.113561	58256.656592	33.389172
798.042879	58344.330444	33.394189
799.389613	58450.710664	33.399207
799.949796	58545.398142	33.404224
801.192835	58643.050343	33.409242
802.041703	58730.132554	33.414260
803.282099	58811.500397	33.419277
803.917917	58919.732691	33.424295
804.548244	59007.496986	33.429312
805.597599	59094.591730	33.434330
805.898323	59193.104513	33.439348
806.884525	59282.327668	33.444365
807.601614	59383.413929	33.449383
808.430071	59484.520127	33.454400
808.847039	59575.671824	33.459418
809.560961	59676.292404	33.464436
810.644926	59766.506331	33.469453
811.176795	59875.525709	33.474471
811.466695	59991.417757	33.479488
812.768455	60097.656128	33.484506
813.070292	60214.343791	33.489524
814.165109	60310.707767	33.494541
815.030766	60425.091012	33.499559
815.685504	60537.209372	33.504576
816.674457	60635.956207	33.509594
817.191806	60746.215106	33.514612
818.166610	60867.054638	33.519629
819.200149	60969.139113	33.524647
820.014616	61081.303478	33.529664
821.189230	61180.015813	33.534682
821.884077	61290.273472	33.539700
823.135104	61386.009853	33.544717
823.759319	61491.318784	33.549735
824.548453	61610.708234	33.554752
825.212556	61702.782831	33.559770
825.574982	61820.177521	33.564788
826.646684	61926.425702	33.569805
827.207015	62038.005443	33.574823
827.877036	62151.046619	33.579840
829.014800	62267.929610	33.584858
829.513530	62377.031064	33.589876
829.875597	62493.709103	33.594893
830.730950	62599.206585	33.599911
831.171098	62718.850040	33.604928
832.393900	62820.191757	33.609946
832.823388	62942.075868	33.614964
833.747060	63060.553849	33.619981
834.716514	63171.427092	33.624999
835.452901	63290.677039	33.630016
836.264183	63399.005109	33.635034
836.921265	63537.314976	33.640052
837.692982	63658.887346	33.645069
838.597357	63780.571156	33.650087
839.286706	63917.525480	33.655104
840.212934	64038.271639	33.660122
840.939496	64168.451392	33.665140
841.914379	64287.490502	33.670157
842.756730	64423.354468	33.675175
843.786718	64561.154133	33.680192
844.763897	64671.142815	33.685210
845.474844	64807.416712	33.690228
846.612891	64931.274683	33.695245
848.048271	65045.431026	33.700263
848.958309	65170.952910	33.705280
850.251607	65288.098996	33.710298
850.663038	65408.148365	33.715316
851.937109	65510.449316	33.720333
852.585466	65629.449160	33.725351
853.605642	65755.657993	33.730368
854.661606	65859.014661	33.735386
855.146897	65978.056200	33.740404
855.925370	66102.018740	33.745421
856.842574	66208.915130	33.750439
857.468191	66331.842323	33.755456
858.503427	66442.165769	33.760474
858.952581	66579.019401	33.765492
859.841282	66694.249090	33.770509
861.289800	66812.850992	33.775527
862.183682	66928.251802	33.780544
863.203483	67038.328059	33.785562
864.113229	67165.391911	33.790580
864.477085	67272.461430	33.795597
865.839443	67392.863773	33.800615
866.498316	67509.305693	33.805632
867.414361	67627.178671	33.810650
868.265842	67753.914335	33.815668
869.430209	67870.318599	33.820685
870.111081	67989.459180	33.825703
870.600366	68114.373038	33.830720
871.736030	68227.730280	33.835738
872.649327	68359.416158	33.840756
873.385184	68468.718751	33.845773
874.366401	68599.446461	33.850791
874.639674	68723.786468	33.855808
875.853615	68854.129372	33.860826
876.074626	68986.288117	33.865844
877.023381	69112.939889	33.870861
878.009600	69251.808188	33.875879
878.665595	69390.460322	33.880896
879.256655	69518.685038	33.885914
879.974914	69668.785728	33.890932
881.150579	69804.698665	33.895949
882.110364	69947.015577	33.900967
882.882102	70091.324797	33.905984
883.895126	70220.046437	33.911002
884.796150	70363.722695	33.916020
886.122426	70498.584372	33.921037
887.423978	70621.152343	33.926055
888.598642	70737.064722	33.931072
890.083146	70831.964622	33.936090
891.439572	70939.937510	33.941108
891.957998	71042.099766	33.946125
892.910729	71141.755925	33.951143
893.722324	71245.128838	33.956160
894.469486	71341.784812	33.961178
895.012450	71448.396618	33.966196
895.859715	71543.032344	33.971213
896.933415	71640.451191	33.976231
897.960620	71758.872373	33.981248
898.312303	71875.401750	33.986266
899.200650	71985.443179	33.991284
900.018141	72095.458988	33.996301
900.816022	72225.910435	34.001319
901.478525	72347.019702	34.006336
901.873722	72469.976283	34.011354
902.959540	72598.554617	34.016372
903.741140	72730.491571	34.021389
905.076138	72849.348248	34.026407
905.648941	72987.797063	34.031424
906.498164	73106.767394	34.036442
907.548364	73235.424975	34.041460
908.512941	73375.544005	34.046477
910.514146	73489.746643	34.051495
911.893487	73600.087892	34.056512
912.679987	73720.671983	34.061530
913.795988	73829.565609	34.066548
914.526414	73938.447883	34.071565
915.692909	74046.727090	34.076583
916.371249	74167.793270	34.081600
917.367883	74288.718753	34.086618
918.393751	74389.370614	34.091636
919.079234	74502.835637	34.096653
919.672789	74604.325483	34.101671
920.427538	74740.105298	34.106688
921.356801	74862.145576	34.111706
921.934693	74986.901133	34.116724
922.537143	75130.797660	34.121741
923.345770	75249.476487	34.126759
923.776321	75398.519865	34.131776
924.374560	75540.003764	34.136794
925.204434	75690.216144	34.141812
926.130209	75844.961111	34.146829
927.170827	75989.947948	34.151847
928.219601	76144.839047	34.156864
929.403285	76294.149286	34.161882
930.373724	76433.768225	34.166900
931.603844	76568.133195	34.171917
933.147168	76701.163028	34.176935
933.890953	76854.465214	34.181952
934.694701	76988.795971	34.186970
935.318551	77126.446447	34.191988
936.189562	77272.696894	34.197005
937.120431	77412.625837	34.202023
937.883640	77569.187190	34.207040
938.894849	77706.030584	34.212058
940.050535	77842.661079	34.217076
941.452083	77989.081188	34.222093
942.943296	78116.049479	34.227111
944.331905	78240.650841	34.232128
945.205399	78371.372867	34.237146
945.897494	78483.977945	34.242164
946.961176	78625.929253	34.247181
948.262036	78726.643749	34.252199
949.621837	78850.937012	34.257216
950.439845	78966.996366	34.262234
951.881947	79079.011865	34.267252
952.778608	79180.143390	34.272269
953.720226	79286.492943	34.277287
954.401489	79394.916770	34.282304
955.237668	79499.494645	34.287322
955.806091	79609.348877	34.292340
956.734523	79708.649348	34.297357
957.357650	79815.680513	34.302375
958.047623	79928.065444	34.307392
959.017707	80050.734675	34.312410
959.834859	80173.132632	34.317428
960.287576	80299.659345	34.322445
960.938576	80421.801551	34.327463
961.882713	80561.558132	34.332480
962.269352	80697.751608	34.337498
963.384419	80835.836725	34.342516
963.576536	80999.380583	34.347533
964.963749	81153.440374	34.352551
965.526786	81305.619906	34.357568
966.711657	81468.793613	34.362586
966.985354	81623.863803	34.367604
967.941858	81796.181384	34.372621
969.064039	81954.775999	34.377639
970.202209	82129.349792	34.382656
971.244692	82292.318933	34.387674
972.552154	82455.238931	34.392692
973.620879	82626.829239	34.397709
974.323771	82783.968133	34.402727
975.597795	82947.314736	34.407744
976.778174	83122.382568	34.412762
977.906884	83275.031738	34.417780
978.763760	83432.839132	34.422797
979.894024	83591.323503	34.427815
981.794362	83722.045090	34.432832
983.573087	83857.235464	34.437850
985.745603	83968.919717	34.442868
987.051632	84100.893596	34.447885
988.343380	84214.648624	34.452903
989.083727	84330.039531	34.457920
989.767139	84453.874532	34.462938
990.620239	84555.214262	34.467956
991.125996	84700.339343	34.472973
991.990228	84814.611167	34.477991
992.882427	84953.295846	34.483008
993.703532	85076.877209	34.488026
994.849183	85195.242262	34.493044
995.954788	85334.741662	34.498061
996.696727	85462.672463	34.503079
997.384100	85598.977905	34.508096
998.142892	85735.658268	34.513114
999.632958	85866.485342	34.518132
1000.814490	86000.059889	34.523149
1002.202511	86138.681991	34.528167
1003.125643	86267.586889	34.533184
1003.645797	86402.659237	34.538202
1004.922102	86532.658621	34.543220
1005.545126	86667.867289	34.548237
1006.248543	86803.791087	34.553255
1007.139895	86939.406061	34.558272
1008.116191	87089.985735	34.563290
1009.204398	87220.760497	34.568308
1009.814863	87376.629544	34.573325
1010.890884	87522.683622	34.578343
1011.775223	87674.092265	34.583360
1012.595185	87839.446923	34.588378
1013.415820	87978.003160	34.593396
1014.375273	88147.279218	34.598413
1015.377129	88307.576095	34.603431
1016.480435	88459.440692	34.608448
1017.559323	88620.764728	34.613466
1018.359747	88761.796916	34.618484
1018.707100	88923.332992	34.623501
1019.521298	89083.868750	34.628519
1020.649905	89229.158874	34.633536
1021.069529	89413.822992	34.638554
1022.729298	89561.121718	34.643572
1023.745430	89725.824084	34.648589
1024.784879	89889.485824	34.653607
1026.129614	90044.858139	34.658624
1026.619550	90220.884556	34.663642
1028.113190	90384.524937	34.668660
1028.604234	90551.035188	34.673677
1030.041058	90704.364956	34.678695
1031.523112	90873.598929	34.683712
1032.695551	91040.556434	34.688730
1033.634167	91200.433838	34.693748
1034.525837	91364.174440	34.698765
1035.519484	91515.817125	34.703783
1037.087790	91676.188115	34.708800
1038.150780	91841.650343	34.713818
1039.253475	91999.505804	34.718836
1039.935424	92163.084076	34.723853
1041.381310	92319.346676	34.728871
1042.656226	92475.005726	34.733888
1043.521430	92646.892496	34.738906
1044.591667	92806.891566	34.743924
1045.486179	92964.186546	34.748941
1046.590012	93132.416725	34.753959
1047.802727	93290.756001	34.758976
1048.910340	93456.487639	34.763994
1049.952677	93606.755441	34.769012
1050.924690	93774.834684	34.774029
1051.788381	93938.837769	34.779047
1052.878102	94097.443195	34.784064
1053.953242	94267.097449	34.789082
1055.298194	94425.744929	34.794100
1056.286713	94583.768955	34.799117
1057.975145	94745.735295	34.804135
1059.171374	94906.765258	34.809152
1059.791426	95060.460528	34.814170
1060.955657	95223.694355	34.819188
1061.581383	95395.880644	34.824205
1062.616188	95558.017736	34.829223
1063.621763	95717.831259	34.834240
1064.297732	95896.741590	34.839258
1065.651455	96064.348963	34.844276
1066.565157	96243.716098	34.849293
1067.587725	96418.920123	34.854311
1068.658966	96593.047478	34.859328
1069.647986	96775.444497	34.864346
1070.631641	96937.782643	34.869364
1071.831875	97118.216340	34.874381
1072.875639	97297.012376	34.879399
1074.368670	97461.155888	34.884416
1076.009888	97630.397333	34.889434
1077.554599	97785.019515	34.894452
1078.995253	97939.185115	34.899469
1079.688674	98103.142634	34.904487
1080.692412	98263.194305	34.909504
1081.883675	98417.448528	34.914522
1082.777421	98578.818262	34.919540
1083.821378	98734.687902	34.924557
1084.621665	98899.240621	34.929575
1085.935639	99050.122963	34.934592
1087.320397	99213.308225	34.939610
1088.117174	99373.274638	34.944628
1089.137668	99530.298980	34.949645
1089.974917	99691.292643	34.954663
1090.987700	99853.771343	34.959680
1091.524946	100013.449291	34.964698
1092.075884	100179.786415	34.969716
1093.089547	100343.198776	34.974733
1093.344511	100528.543096	34.979751
1094.866539	100698.097057	34.984768
1095.442620	100892.539538	34.989786
1096.460437	101068.764268	34.994804
1097.367382	101261.875697	34.999821
1098.058538	101467.706457	35.004839
1099.413314	101660.309694	35.009856
1100.727058	101857.733224	35.014874
1101.960397	102049.441429	35.019892
1103.065589	102251.999584	35.024909
1104.230628	102462.768053	35.029927
1105.360996	102646.279105	35.034944
1106.120215	102849.044960	35.039962
1107.443895	103048.172863	35.044980
1109.164896	103257.981738	35.049997
1110.359150	103443.792661	35.055015
1111.751517	103630.255903	35.060032
1113.052170	103821.560767	35.065050
1114.423524	104015.540138	35.070068
1115.877045	104196.906217	35.075085
1116.774481	104387.306956	35.080103
1118.066743	104573.122307	35.085120
1118.942154	104751.561299	35.090138
1120.168605	104945.926202	35.095156
1121.386273	105118.675072	35.100173
1122.272185	105320.178894	35.105191
1123.438063	105502.348933	35.110208
1124.527819	105709.153884	35.115226
1125.843258	105887.362902	35.120244
1126.824540	106074.874240	35.125261
1127.251192	106278.285354	35.130279
1128.862070	106476.587330	35.135296
1129.994047	106670.131979	35.140314
1131.796522	106852.420985	35.145332
1133.215513	107034.914186	35.150349
1134.721616	107223.765111	35.155367
1136.302743	107399.305677	35.160384
1137.277126	107587.601426	35.165402
1138.483455	107744.726700	35.170420
1140.035583	107916.576965	35.175437
1140.658991	108093.712252	35.180455
1141.868336	108259.693766	35.185472
1143.020944	108442.810736	35.190490
1144.128013	108618.881252	35.195508
1145.713117	108793.353615	35.200525
1146.148477	108978.138538	35.205543
1147.169805	109150.388736	35.210560
1148.294404	109328.880320	35.215578
1149.233332	109520.045487	35.220596
1150.492826	109695.109694	35.225613
1151.446385	109883.044896	35.230631
1152.574121	110072.143216	35.235648
1153.429472	110259.818632	35.240666
1154.932097	110442.549017	35.245684
1156.320540	110631.506622	35.250701
1158.365925	110797.618311	35.255719
1159.652372	110961.298063	35.260736
1160.662624	111132.118518	35.265754
1161.579424	111317.738827	35.270772
1162.896897	111488.155830	35.275789
1163.559643	111676.784988	35.280807
1164.651819	111854.576372	35.285824
1165.809415	112036.981907	35.290842
1166.525407	112228.000269	35.295860
1167.459800	112403.135703	35.300877
1168.585652	112592.391034	35.305895
1169.940004	112753.840532	35.310912
1170.940038	112927.106127	35.315930
1172.639499	113103.411246	35.320948
1174.400272	113252.900418	35.325965
1175.503252	113423.022865	35.330983
1176.970949	113574.918772	35.336000
1177.936489	113739.276305	35.341018
1178.567352	113909.467370	35.346036
1180.207626	114088.119624	35.351053
1180.689473	114260.047860	35.356071
1182.011615	114427.175484	35.361088
1183.217876	114608.284861	35.366106
1183.862688	114792.009748	35.371124
1185.442467	114969.575413	35.376141
1186.075595	115164.605803	35.381159
1187.198963	115351.029566	35.386176
1188.197359	115549.486156	35.391194
1188.957016	115751.163858	35.396212
1190.147081	115950.807761	35.401229
1191.345188	116153.112426	35.406247
1192.738487	116363.773725	35.411264
1194.053405	116571.193357	35.416282
1195.107981	116776.237671	35.421300
1196.175811	116976.846643	35.426317
1197.327218	117185.526884	35.431335
1198.683542	117400.345191	35.436352
1200.023874	117609.909457	35.441370
1200.666157	117819.958503	35.446388
1202.079331	118038.003175	35.451405
1203.368846	118255.981315	35.456423
1204.612565	118478.821687	35.461440
1205.739943	118690.177731	35.466458
1206.528398	118925.261304	35.471476
1207.906130	119143.054095	35.476493
1208.924730	119371.336637	35.481511
1210.359737	119591.302762	35.486528
1211.500037	119824.282453	35.491546
1212.365750	120054.534457	35.496564
1214.004602	120283.456200	35.501581
1214.922815	120525.513294	35.506599
1216.492534	120756.591747	35.511616
1218.015830	120990.999804	35.516634
1218.924911	121218.149080	35.521652
1220.450496	121433.412625	35.526669
1222.058835	121669.091863	35.531687
1223.768401	121881.565576	35.536704
1225.825979	122082.298995	35.541722
1227.095929	122287.422432	35.546740
1228.851966	122481.694842	35.551757
1230.417040	122678.015173	35.556775
1231.358044	122860.525498	35.561792
1232.633998	123055.261471	35.566810
1233.826256	123257.261578	35.571828
1235.534749	123437.962602	35.576845
1236.358688	123629.811783	35.581863
1237.733748	123810.380264	35.586880
1239.083377	124011.776376	35.591898
1239.602459	124202.602545	35.596916
1241.295558	124405.845333	35.601933
1242.320513	124605.296849	35.606951
1242.925221	124810.357795	35.611968
1244.225185	125002.390217	35.616986
1245.085513	125225.636466	35.622004
1246.249929	125426.591113	35.627021
1247.283544	125642.169280	35.632039
1247.999323	125858.942365	35.637056
1249.282476	126072.986634	35.642074
1250.341033	126290.909973	35.647092
1251.473581	126493.537263	35.652109
1252.648578	126706.209713	35.657127
1253.589327	126923.498012	35.662144
1254.880372	127142.745009	35.667162
1255.928934	127356.545619	35.672180
1256.942160	127585.081737	35.677197
1258.020984	127819.464482	35.682215
1258.928710	128052.597201	35.687232
1260.592179	128290.245409	35.692250
1261.496500	128538.427721	35.697268
1262.473763	128773.392213	35.702285
1263.390516	129027.622483	35.707303
1264.699816	129281.827731	35.712320
1265.879610	129535.283307	35.717338
1266.790347	129805.644293	35.722356
1268.087197	130060.314230	35.727373
1269.664686	130338.162021	35.732391
1271.039152	130600.961409	35.737408
1272.740210	130857.510160	35.742426
1273.944218	131130.369059	35.747444
1275.372972	131378.917753	35.752461
1276.623607	131647.019704	35.757479
1277.799536	131915.148972	35.762496
1279.875506	132170.885514	35.767514
1280.735764	132437.740462	35.772532
1282.565011	132693.877045	35.777549
1284.384560	132943.805549	35.782567
1285.398997	133199.941857	35.787584
1286.989111	133444.752716	35.792602
1288.277529	133697.881057	35.797620
1289.683613	133936.552315	35.802637
1291.368292	134175.572117	35.807655
1293.418950	134408.016702	35.812672
1295.159717	134642.580801	35.817690
1296.370653	134871.060402	35.822708
1297.890787	135091.477922	35.827725
1299.344254	135323.318104	35.832743
1300.661694	135538.739112	35.837760
1302.270796	135744.680661	35.842778
1303.493901	135961.311815	35.847796
1304.860176	136180.938065	35.852813
1306.427502	136407.163191	35.857831
1307.203163	136614.959967	35.862848
1308.646370	136831.598336	35.867866
1309.649236	137068.710985	35.872884
1310.807081	137283.066758	35.877901
1312.279282	137512.472157	35.882919
1313.046006	137748.703244	35.887936
1314.845314	137957.581113	35.892954
1315.951538	138209.696537	35.897972
1317.304303	138436.731723	35.902989
1318.275634	138668.206020	35.908007
1319.187373	138904.129529	35.913024
1321.152747	139138.155534	35.918042
1321.833264	139383.604890	35.923060
1323.230017	139608.827471	35.928077
1324.500186	139847.817246	35.933095
1325.809613	140099.557977	35.938112
1327.534505	140334.443585	35.943130
1328.278198	140576.416760	35.948148
1329.201417	140820.644259	35.953165
1330.564950	141060.362435	35.958183
1331.463449	141323.693790	35.963200
1332.865727	141578.561940	35.968218
1334.022885	141843.997314	35.973236
1334.836716	142106.220098	35.978253
1336.325895	142369.334611	35.983271
1337.507160	142627.176303	35.988288
1338.893349	142876.743430	35.993306
1340.150997	143141.499921	35.998324
1341.446957	143392.201590	36.003341
1343.483361	143643.441652	36.008359
1345.031427	143885.279034	36.013376
1347.258780	144100.298848	36.018394
1348.671344	144346.638311	36.023412
1349.867170	144588.031658	36.028429
1351.190629	144823.280342	36.033447
1352.030390	145068.844783	36.038464
1353.157582	145310.989932	36.043482
1354.687907	145565.738870	36.048500
1355.904604	145820.769902	36.053517
1356.935199	146082.922774	36.058535
1358.038822	146345.991222	36.063552
1359.175582	146613.520173	36.068570
1360.671085	146871.048794	36.073588
1361.627311	147153.322964	36.078605
1362.856702	147428.058749	36.083623
1364.417413	147708.195104	36.088640
1366.614732	147952.387186	36.093658
1368.828694	148216.033267	36.098676
1370.197817	148476.105318	36.103693
1371.835660	148728.905446	36.108711
1372.877958	148985.788495	36.113728
1374.666720	149235.827557	36.118746
1375.814821	149499.862499	36.123764
1377.023448	149756.964278	36.128781
1378.835597	150011.215479	36.133799
1380.093255	150274.172342	36.138816
1381.643130	150532.161425	36.143834
1382.972980	150777.035988	36.148852
1384.832454	151033.620036	36.153869
1386.402465	151275.705676	36.158887
1388.054671	151522.510269	36.163904
1389.219528	151765.097476	36.168922
1390.341294	152013.908489	36.173940
1392.007442	152270.000246	36.178957
1393.392346	152521.510676	36.183975
1394.559901	152778.779357	36.188992
1395.761602	153035.701626	36.194010
1396.684879	153293.141103	36.199028
1397.925780	153565.192808	36.204045
1399.216675	153824.528264	36.209063
1400.818907	154094.773308	36.214080
1402.928068	154342.978997	36.219098
1404.401178	154598.839175	36.224116
1405.535770	154858.829002	36.229133
1407.353523	155106.085769	36.234151
1408.663749	155369.817280	36.239168
1409.838606	155630.909140	36.244186
1411.285334	155897.868933	36.249204
1412.287270	156161.847143	36.254221
1413.722734	156422.951756	36.259239
1414.637637	156697.438737	36.264256
1416.395215	156970.532000	36.269274
1418.056206	157231.198575	36.274292
1419.295841	157512.119641	36.279309
1421.105008	157762.527751	36.284327
1422.379993	158042.596714	36.289344
1424.205917	158290.074892	36.294362
1425.761881	158550.716684	36.299380
1426.842292	158804.182566	36.304397
1428.448623	159067.077443	36.309415
1429.941863	159334.826231	36.314432
1431.135919	159589.178867	36.319450
1432.300055	159855.881924	36.324468
1433.513297	160113.393543	36.329485
1435.023817	160366.924635	36.334503
1435.721519	160634.217533	36.339520
1437.013113	160880.734295	36.344538
1438.523361	161163.157998	36.349556
1439.305574	161434.920474	36.354573
1440.759728	161701.523874	36.359591
1441.890731	161990.448352	36.364608
1443.235248	162265.104426	36.369626
1445.176595	162552.008000	36.374644
1446.076243	162841.585660	36.379661
1447.274675	163135.772030	36.384679
1448.527251	163434.823455	36.389696
1450.210117	163739.515039	36.394714
1451.781028	164050.774198	36.399732
1452.994299	164337.810526	36.404749
1454.900567	164632.130870	36.409767
1456.833750	164936.941683	36.414784
1458.582861	165225.569862	36.419802
1460.497226	165500.824665	36.424820
1462.459184	165784.472895	36.429837
1464.342805	166052.097983	36.434855
1466.370407	166333.937154	36.439872
1467.289524	166613.589198	36.444890
1468.877142	166890.340693	36.449908
1469.907364	167179.887618	36.454925
1471.333058	167451.454453	36.459943
1472.926616	167729.073018	36.464960
1474.770678	168013.630624	36.469978
1475.904940	168287.522161	36.474996
1477.582229	168576.412526	36.480013
1479.144357	168853.167712	36.485031
1480.273767	169129.082723	36.490048
1481.764852	169420.839031	36.495066
1483.326701	169712.141348	36.500084
1484.688822	169991.804409	36.505101
1486.662405	170286.683966	36.510119
1487.841998	170581.595550	36.515136
1489.514920	170865.907522	36.520154
1491.160149	171159.679659	36.525172
1491.854908	171451.174811	36.530189
1493.496579	171744.354808	36.535207
1495.040525	172040.408083	36.540224
1496.280294	172339.597335	36.545242
1498.154734	172631.513348	36.550260
1499.658162	172939.634589	36.555277
1500.837619	173225.844708	36.560295
1502.636272	173540.062977	36.565312
1503.745237	173847.570221	36.570330
1505.296121	174142.759829	36.575348
1506.768096	174452.063567	36.580365
1508.018126	174749.121525	36.585383
1509.539768	175067.723218	36.590400
1510.737414	175384.984726	36.595418
1512.349329	175701.088190	36.600436
1513.658927	176032.003440	36.605453
1515.094374	176344.168021	36.610471
1516.410857	176670.555701	36.615488
1517.685079	177003.234698	36.620506
1519.126881	177331.864983	36.625524
1520.449725	177669.883410	36.630541
1522.155703	178001.418692	36.635559
1523.490690	178337.713548	36.640576
1525.217926	178678.793818	36.645594
1526.775102	179008.837369	36.650612
1528.365920	179334.371878	36.655629
1530.994266	179650.027127	36.660647
1532.532605	179976.209001	36.665664
1534.374503	180265.522940	36.670682
1536.937221	180560.417750	36.675700
1538.056761	180848.636259	36.680717
1539.415423	181133.262876	36.685735
1541.104091	181417.049400	36.690752
1542.531655	181695.588012	36.695770
1543.783850	181989.134282	36.700788
1545.153985	182278.397929	36.705805
1546.609560	182576.787662	36.710823
1548.259463	182868.978199	36.715840
1549.391324	183178.442201	36.720858
1551.062291	183474.884611	36.725876
1552.860140	183782.883530	36.730893
1554.031202	184099.543173	36.735911
1556.068024	184413.738292	36.740928
1557.913175	184710.387031	36.745946
1560.052954	184991.490156	36.750964
1561.532477	185291.553642	36.755981
1563.228886	185591.646261	36.760999
1564.657426	185882.582209	36.766016
1565.916057	186183.232939	36.771034
1567.791985	186481.091915	36.776052
1569.133623	186779.371078	36.781069
1570.995416	187085.207154	36.786087
1572.614649	187380.574694	36.791104
1574.472948	187667.462767	36.796122
1576.414000	187950.593875	36.801140
1577.930082	188245.589469	36.806157
1579.000390	188544.494052	36.811175
1580.727143	188835.649536	36.816192
1582.139112	189152.119924	36.821210
1583.567574	189454.714561	36.826228
1585.033448	189753.889804	36.831245
1586.258460	190071.843281	36.836263
1587.971207	190376.515462	36.841280
1589.144715	190706.400883	36.846298
1590.945579	191018.386422	36.851316
1592.101065	191354.359060	36.856333
1593.367196	191683.206221	36.861351
1594.986267	192010.549456	36.866368
1596.148775	192360.249475	36.871386
1597.786321	192701.925757	36.876404
1599.037654	193043.591788	36.881421
1600.378283	193400.682012	36.886439
1602.348332	193740.556987	36.891456
1603.777444	194105.901059	36.896474
1605.495824	194458.224790	36.901492
1607.144875	194816.477975	36.906509
1608.626889	195178.264781	36.911527
1610.358937	195546.905797	36.916544
1611.622640	195917.353150	36.921562
1613.371328	196275.267866	36.926580
1615.312254	196628.391815	36.931597
1616.686602	196989.622581	36.936615
1618.764448	197360.400190	36.941632
1620.205297	197716.101236	36.946650
1622.117945	198064.984437	36.951668
1623.805791	198431.719176	36.956685
1626.242215	198776.977063	36.961703
1627.903859	199117.083562	36.966720
1629.668570	199463.687805	36.971738
1631.671213	199800.249722	36.976756
1632.995025	200146.892402	36.981773
1634.771341	200491.646219	36.986791
1636.456388	200823.860105	36.991808
1638.048550	201174.196142	36.996826
1639.544576	201511.078815	37.001844
1640.861909	201848.398996	37.006861
1642.145699	202180.406424	37.011879
1643.976774	202494.866672	37.016896
1645.674360	202840.368637	37.021914
1647.356072	203147.644702	37.026932
1648.940207	203484.966370	37.031949
1650.565306	203807.605121	37.036967
1651.969228	204143.740761	37.041984
1653.343741	204479.793911	37.047002
1655.012589	204814.415790	37.052020
1656.145300	205167.284981	37.057037
1657.424839	205520.423507	37.062055
1659.232359	205873.565023	37.067072
1660.551006	206244.603579	37.072090
1662.224711	206608.804635	37.077108
1663.683480	206972.624000	37.082125
1665.450506	207340.203210	37.087143
1667.278728	207706.440735	37.092160
1668.595306	208089.741505	37.097178
1671.058909	208439.141561	37.102196
1673.021026	208822.465787	37.107213
1674.519948	209197.830869	37.112231
1676.443126	209561.902418	37.117248
1678.247583	209932.839432	37.122266
1679.943459	210287.593460	37.127284
1681.882394	210665.977849	37.132301
1683.613185	211032.030480	37.137319
1685.550276	211391.853787	37.142336
1687.010085	211751.173593	37.147354
1689.312633	212123.586789	37.152372
1691.148389	212484.625066	37.157389
1692.671202	212840.256400	37.162407
1694.798770	213200.182571	37.167424
1696.449046	213568.875054	37.172442
1697.891060	213931.889232	37.177460
1699.651789	214294.217103	37.182477
1701.354697	214653.584515	37.187495
1703.108741	215020.919612	37.192512
1704.883631	215384.290704	37.197530
1706.551962	215750.982542	37.202548
1708.440969	216125.741068	37.207565
1709.479565	216490.838494	37.212583
1711.222446	216861.890648	37.217600
1713.028379	217247.715360	37.222618
1714.721523	217612.352934	37.227636
1716.517964	217979.006580	37.232653
1717.992758	218410.150152	37.237671
1720.059466	218808.001845	37.242688
1721.208759	219187.669490	37.247706
1722.970061	219576.964727	37.252724
1725.071758	219957.467883	37.257741
1726.513800	220354.641703	37.262759
1728.267490	220727.458713	37.267776
1729.478432	221111.745674	37.272794
1731.235667	221512.732175	37.277812
1733.966620	221880.666977	37.282829
1735.424961	222262.097682	37.287847
1737.810003	222642.563323	37.292864
1739.441288	223017.516529	37.297882
1740.749843	223392.829250	37.302900
1742.683758	223782.822044	37.307917
1744.169047	224170.223545	37.312935
1746.110495	224547.848052	37.317952
1747.624640	224930.141928	37.322970
1749.118019	225319.247608	37.327988
1751.059980	225701.346014	37.333005
1753.010613	226087.965363	37.338023
1754.533922	226471.354728	37.343040
1756.057650	226855.684993	37.348058
1757.850414	227229.557745	37.353076
1759.723966	227599.912954	37.358093
1760.824677	227971.692715	37.363111
1762.322985	228346.328673	37.368128
1763.813710	228727.774265	37.373146
1765.443776	229119.485060	37.378164
1766.972171	229512.458454	37.383181
1768.740315	229905.825034	37.388199
1770.664038	230299.878148	37.393216
1772.340012	230702.939904	37.398234
1773.951833	231107.080250	37.403252
1775.697442	231519.277043	37.408269
1777.181867	231930.908634	37.413287
1778.922721	232336.935998	37.418304
1780.887958	232768.201426	37.423322
1782.203985	233192.539485	37.428340
1784.170495	233612.071627	37.433357
1785.519040	234051.545755	37.438375
1787.499062	234482.965746	37.443392
1789.184514	234931.911912	37.448410
1790.518611	235367.022817	37.453428
1792.887711	235808.466107	37.458445
1794.608528	236261.753525	37.463463
1796.355284	236702.209882	37.468480
1798.132568	237158.995612	37.473498
1799.840646	237609.697464	37.478516
1802.088242	238059.752118	37.483533
1804.056495	238518.719399	37.488551
1806.118581	238968.552835	37.493568
1807.551619	239424.791229	37.498586
1809.682972	239878.806506	37.503604
1811.361778	240333.558194	37.508621
1813.552507	240797.015174	37.513639
1815.389464	241241.861012	37.518656
1817.535217	241695.166329	37.523674
1819.257209	242160.431072	37.528692
1820.778602	242618.261611	37.533709
1822.394504	243076.153529	37.538727
1824.457022	243524.801915	37.543744
1826.251837	243999.634708	37.548762
1828.238404	244462.573504	37.553780
1830.127701	244916.536617	37.558797
1831.985726	245381.276375	37.563815
1833.889713	245841.131896	37.568832
1835.724690	246320.788315	37.573850
1837.651695	246775.713218	37.578868
1839.877979	247236.380995	37.583885
1841.502896	247689.477349	37.588903
1843.415374	248159.775209	37.593920
1845.520611	248616.070070	37.598938
1847.651755	249076.882893	37.603956
1849.795483	249532.664340	37.608973
1851.006210	249993.478251	37.613991
1852.914252	250444.041243	37.619008
1854.486956	250912.950454	37.624026
1856.320592	251380.724518	37.629044
1858.802041	251835.054983	37.634061
1860.863262	252289.379228	37.639079
1862.978966	252738.690348	37.644096
1864.988192	253184.081919	37.649114
1866.498210	253642.918575	37.654132
1868.549754	254097.423427	37.659149
1869.882292	254554.003709	37.664167
1871.755585	255016.794611	37.669184
1873.006586	255470.696074	37.674202
1874.713576	255938.849593	37.679220
1876.466439	256406.131954	37.684237
1878.478759	256874.006535	37.689255
1880.980031	257306.845275	37.694272
1882.576702	257757.540073	37.699290
1884.407387	258198.796929	37.704308
1886.127697	258643.501550	37.709325
1887.641088	259094.769113	37.714343
1889.371008	259550.827411	37.719360
1891.460600	259993.590960	37.724378
1893.773494	260437.536812	37.729396
1896.525240	260867.844517	37.734413
1898.395242	261325.073287	37.739431
1900.383272	261751.646029	37.744448
1902.578729	262201.250433	37.749466
1904.158650	262643.792945	37.754484
1906.024512	263077.091922	37.759501
1907.599500	263537.747370	37.764519
1909.044116	263990.625388	37.769536
1910.777438	264445.385955	37.774554
1912.346330	264928.955286	37.779572
1914.051981	265406.760494	37.784589
1915.677152	265889.913329	37.789607
1917.663738	266373.793374	37.794624
1919.029157	266862.526287	37.799642
1920.592356	267369.592380	37.804660
1922.630382	267861.642273	37.809677
1924.782209	268378.313699	37.814695
1926.555096	268888.975974	37.819712
1928.319861	269393.897886	37.824730
1930.312511	269914.785218	37.829748
1932.710320	270423.436707	37.834765
1934.425217	270943.631888	37.839783
1936.204303	271461.529379	37.844800
1938.450916	271977.875220	37.849818
1940.369616	272514.114052	37.854836
1942.801427	273039.445372	37.859853
1944.147969	273556.394858	37.864871
1946.048459	274093.446647	37.869888
1947.997612	274622.004853	37.874906
1949.680187	275171.944219	37.879924
1951.426683	275703.759866	37.884941
1953.291084	276259.864863	37.889959
1955.155805	276813.352050	37.894976
1957.458593	277361.659464	37.899994
1959.109261	277915.814444	37.905012
1960.790260	278474.255919	37.910029
1962.822695	279039.242196	37.915047
1964.904867	279604.320262	37.920064
1967.248760	280161.859788	37.925082
1969.389139	280721.971589	37.930100
1971.643624	281278.836785	37.935117
1973.447028	281846.570710	37.940135
1975.448494	282404.490402	37.945152
1977.606498	282959.308783	37.950170
1979.502189	283525.091407	37.955188
1982.429282	284068.144855	37.960205
1984.689765	284606.099667	37.965223
1986.873628	285154.911634	37.970240
1989.173580	285688.004578	37.975258
1991.288682	286227.781329	37.980276
1993.662788	286753.441135	37.985293
1995.594521	287285.065319	37.990311
1997.610134	287801.382426	37.995328
2000.038749	288332.488568	38.000346
2001.669791	288857.755686	38.005364
2003.653762	289381.057279	38.010381
2005.724720	289916.382152	38.015399
2007.545345	290439.757426	38.020416
2009.522292	290964.323887	38.025434
2010.628701	291493.629795	38.030452
2012.899088	291999.880750	38.035469
2014.632516	292504.643791	38.040487
2016.398247	293019.711643	38.045504
2018.184364	293527.458827	38.050522
2019.743576	294059.701069	38.055540
2021.789345	294576.011089	38.060557
2023.894557	295107.675448	38.065575
2025.643019	295646.457339	38.070592
2027.953253	296180.419345	38.075610
2029.964386	296708.230976	38.080628
2031.593997	297251.393247	38.085645
2033.678078	297787.924624	38.090663
2035.992520	298341.508248	38.095680
2038.393951	298878.464002	38.100698
2040.148553	299420.425927	38.105716
2041.868028	299958.682638	38.110733
2044.272390	300527.402041	38.115751
2046.639712	301066.002551	38.120768
2048.530726	301634.775122	38.125786
2050.327830	302180.879935	38.130804
2052.243740	302738.009728	38.135821
2054.467211	303308.672710	38.140839
2056.530908	303874.609374	38.145856
2058.965576	304432.988989	38.150874
2060.820751	305008.451485	38.155892
2063.003127	305570.091132	38.160909
2065.107910	306149.873005	38.165927
2067.238334	306716.974048	38.170944
2069.139325	307298.127913	38.175962
2070.784379	307880.513767	38.180980
2073.141522	308459.882490	38.185997
2075.398089	309039.695515	38.191015
2077.170234	309621.514687	38.196032
2079.327287	310205.602239	38.201050
2081.541700	310792.240881	38.206068
2083.580112	311378.421796	38.211085
2086.109596	311964.110635	38.216103
2088.459501	312554.929012	38.221120
2090.570603	313143.242937	38.226138
2092.261911	313735.303912	38.231156
2094.531188	314332.063850	38.236173
2096.129084	314925.806751	38.241191
2098.468363	315529.122248	38.246208
2100.575748	316117.870072	38.251226
2102.583207	316728.695993	38.256244
2104.284233	317328.572359	38.261261
2106.484231	317949.131931	38.266279
2108.244748	318562.242626	38.271296
2110.492997	319176.765162	38.276314
2112.798845	319790.434646	38.281332
2114.969356	320397.747653	38.286349
2117.787696	321005.988836	38.291367
2119.781829	321616.925391	38.296384
2121.990065	322233.939925	38.301402
2124.064827	322849.701123	38.306420
2126.193147	323469.484560	38.311437
2128.480287	324069.329802	38.316455
2130.440671	324687.656417	38.321472
2132.334747	325294.435594	38.326490
2134.793785	325913.073565	38.331508
2136.970345	326522.815085	38.336525
2139.331683	327127.340520	38.341543
2140.987237	327747.539902	38.346560
2143.239846	328349.760562	38.351578
2145.714069	328974.203616	38.356596
2147.548171	329585.366652	38.361613
2149.564330	330195.198298	38.366631
2151.393288	330818.433490	38.371648
2153.878921	331400.451661	38.376666
2155.481602	332005.711892	38.381684
2157.644827	332603.993009	38.386701
2159.803516	333192.824776	38.391719
2161.689428	333796.495334	38.396736
2163.865998	334393.383888	38.401754
2165.906282	335011.612027	38.406772
2167.600382	335619.558685	38.411789
2170.026993	336236.642471	38.416807
2171.798789	336862.915081	38.421824
2173.949826	337483.456734	38.426842
2175.911674	338124.329293	38.431860
2177.639728	338758.962880	38.436877
2179.955937	339386.815409	38.441895
2181.836392	340053.212627	38.446912
2184.287908	340691.890321	38.451930
2186.634263	341354.030324	38.456948
2188.747829	342013.281103	38.461965
2192.043275	342635.473424	38.466983
2194.852264	343279.769164	38.472000
2197.589734	343903.865044	38.477018
2200.065856	344549.417179	38.482036
2202.239313	345188.158047	38.487053
2204.692425	345802.580905	38.492071
2206.487864	346442.128743	38.497088
2209.035743	347079.259066	38.502106
2211.300356	347712.798354	38.507124
2213.179229	348347.712445	38.512141
2215.384478	348990.253175	38.517159
2217.415472	349633.295806	38.522176
2219.535731	350276.618971	38.527194
2222.113263	350916.964156	38.532212
2224.163256	351558.935406	38.537229
2226.533287	352215.638593	38.542247
2228.270916	352868.884014	38.547264
2230.288506	353537.425347	38.552282
2232.606457	354202.151053	38.557300
2234.559531	354863.272899	38.562317
2237.058362	355531.906331	38.567335
2239.048276	356198.405908	38.572352
2241.140037	356869.140737	38.577370
2244.096016	357520.894867	38.582388
2246.330495	358200.439680	38.587405
2248.951844	358866.817129	38.592423
2251.142925	359538.633734	38.597440
2253.874217	360201.444390	38.602458
2256.603481	360859.500088	38.607476
2258.656572	361529.682520	38.612493
2260.996165	362174.233159	38.617511
2263.247224	362841.519126	38.622528
2265.900036	363477.751377	38.627546
2268.354004	364141.302988	38.632564
2270.357032	364790.838442	38.637581
2272.921311	365437.758556	38.642599
2275.219643	366099.754683	38.647616
2277.253557	366749.150253	38.652634
2279.606949	367399.115912	38.657652
2281.408443	368070.443919	38.662669
2283.545414	368722.223413	38.667687
2285.315108	369392.010871	38.672704
2287.252180	370058.410281	38.677722
2289.961921	370736.489400	38.682740
2291.697674	371415.782438	38.687757
2293.891985	372095.417965	38.692775
2296.072003	372788.612158	38.697792
2298.318584	373466.665885	38.702810
2300.897919	374144.144327	38.707828
2302.948859	374836.660502	38.712845
2305.475123	375489.242269	38.717863
2307.563181	376156.390577	38.722880
2309.882939	376814.053776	38.727898
2312.166155	377471.837283	38.732916
2313.964756	378133.644423	38.737933
2316.750614	378783.686412	38.742951
2319.263845	379456.811532	38.747968
2321.758191	380119.377617	38.752986
2324.212884	380785.005379	38.758004
2326.443466	381454.840790	38.763021
2328.683575	382114.011580	38.768039
2331.065251	382789.931096	38.773056
2333.503877	383466.030100	38.778074
2336.028387	384128.916570	38.783092
2337.913721	384815.753364	38.788109
2340.402207	385491.599090	38.793127
2342.521580	386176.669429	38.798144
2344.677050	386859.107812	38.803162
2347.021265	387554.911352	38.808180
2349.380252	388269.583737	38.813197
2351.397670	388957.526196	38.818215
2353.689575	389663.558688	38.823232
2356.170946	390381.483359	38.828250
2358.775240	391098.585187	38.833268
2360.891061	391825.434189	38.838285
2362.903712	392536.947662	38.843303
2365.425882	393264.556897	38.848320
2367.575753	393998.217366	38.853338
2370.024950	394732.900251	38.858356
2372.068813	395486.514354	38.863373
2374.564615	396220.823381	38.868391
2376.900704	396971.512785	38.873408
2378.685146	397721.919558	38.878426
2381.162493	398489.957530	38.883444
2383.582447	399266.753030	38.888461
2385.826061	400030.176699	38.893479
2388.333781	400815.329265	38.898496
2390.565994	401584.845868	38.903514
2393.089577	402373.247122	38.908532
2395.215257	403148.313582	38.913549
2397.981047	403924.595628	38.918567
2400.329546	404710.527971	38.923584
2403.028919	405493.973089	38.928602
2405.685677	406282.850250	38.933620
2408.163741	407060.359031	38.938637
2411.911376	407826.184517	38.943655
2414.537406	408579.558081	38.948672
2417.476387	409355.481060	38.953690
2420.136130	410106.982525	38.958708
2422.535384	410859.519319	38.963725
2424.872915	411615.312771	38.968743
2427.044905	412376.279424	38.973760
2428.771379	413139.425573	38.978778
2431.324889	413904.286977	38.983796
2433.377389	414679.289376	38.988813
2436.030911	415443.050699	38.993831
2438.487428	416222.726949	38.998848
2440.601910	416978.579710	39.003866
2443.381591	417757.066950	39.008884
2445.575899	418522.762818	39.013901
2448.578586	419293.062534	39.018919
2451.166858	420060.951106	39.023936
2453.645001	420825.264126	39.028954
2456.518869	421583.968369	39.033972
2458.873936	422347.419592	39.038989
2461.374731	423116.747892	39.044007
2463.827017	423871.957860	39.049024
2466.217437	424622.293856	39.054042
2468.590940	425355.090322	39.059060
2471.022198	426090.639945	39.064077
2473.596369	426810.245516	39.069095
2475.692847	427531.376947	39.074112
2477.834093	428272.426659	39.079130
2480.500369	428997.115500	39.084148
2482.802858	429750.445417	39.089165
2485.173058	430487.085220	39.094183
2487.725307	431232.480029	39.099200
2489.505877	431996.202052	39.104218
2491.417015	432751.930492	39.109236
2493.530046	433538.072102	39.114253
2496.437179	434313.072221	39.119271
2498.651753	435078.544475	39.124288
2500.986306	435878.285844	39.129306
2503.563486	436665.357321	39.134324
2506.033120	437464.767689	39.139341
2508.572692	438268.389187	39.144359
2511.427033	439066.312901	39.149376
2513.449425	439880.994143	39.154394
2516.084039	440699.693608	39.159412
2518.668081	441512.957276	39.164429
2520.824373	442339.670028	39.169447
2523.341853	443165.482493	39.174464
2525.679070	443998.983853	39.179482
2528.652441	444823.292343	39.184500
2531.105993	445658.633458	39.189517
2534.379302	446495.526627	39.194535
2536.793609	447321.198406	39.199552
2539.191264	448169.097767	39.204570
2541.744739	449021.692311	39.209588
2544.192889	449872.550413	39.214605
2546.843482	450713.427703	39.219623
2549.852154	451559.927153	39.224640
2552.009554	452414.321575	39.229658
2554.804195	453261.343935	39.234676
2557.173639	454124.280776	39.239693
2559.673860	454996.969934	39.244711
2562.301432	455843.610861	39.249728
2564.910576	456721.973126	39.254746
2566.960709	457587.901741	39.259764
2570.435185	458441.019319	39.264781
2574.002872	459283.974292	39.269799
2577.316495	460127.441580	39.274816
2580.175665	460971.807998	39.279834
2583.058269	461802.031490	39.284852
2585.969913	462632.266076	39.289869
2588.504257	463460.809766	39.294887
2591.181359	464274.688007	39.299904
2593.637489	465113.991356	39.304922
2596.399627	465930.061170	39.309940
2598.869627	466752.866576	39.314957
2601.345494	467587.966628	39.319975
2603.745780	468416.322276	39.324992
2606.165426	469252.218647	39.330010
2608.790430	470082.890716	39.335028
2611.290177	470912.840018	39.340045
2613.601299	471754.101655	39.345063
2616.088881	472597.772290	39.350080
2618.317627	473451.046694	39.355098
2621.033921	474285.510389	39.360116
2623.595582	475128.802545	39.365133
2625.879790	475995.489708	39.370151
2628.586214	476841.913037	39.375168
2630.649465	477706.637343	39.380186
2633.579839	478566.480558	39.385204
2635.740162	479437.168020	39.390221
2638.152286	480295.500687	39.395239
2640.859611	481147.583232	39.400256
2643.372733	481980.873398	39.405274
2645.992481	482829.558469	39.410292
2648.102792	483679.903503	39.415309
2650.659336	484537.758123	39.420327
2653.154406	485386.393172	39.425344
2656.035335	486248.604968	39.430362
2658.251121	487110.783875	39.435380
2661.057891	487974.993432	39.440397
2663.400786	488857.055388	39.445415
2666.159811	489731.786269	39.450432
2668.819085	490641.213954	39.455450
2671.524255	491521.970724	39.460468
2673.907645	492419.692455	39.465485
2676.366522	493316.244711	39.470503
2679.517956	494216.268684	39.475520
2681.882488	495131.462401	39.480538
2684.895573	496042.210889	39.485556
2687.655103	496951.993799	39.490573
2690.072882	497882.569562	39.495591
2692.947322	498798.741765	39.500608
2695.622415	499731.341666	39.505626
2698.312018	500664.542772	39.510644
2701.040632	501596.676244	39.515661
2703.720168	502536.885489	39.520679
2706.389264	503470.335271	39.525696
2708.830329	504432.716494	39.530714
2711.399563	505377.925152	39.535732
2714.288576	506352.877044	39.540749
2716.231951	507337.960566	39.545767
2718.708946	508320.677362	39.550784
2721.055118	509297.205193	39.555802
2724.291721	510293.085899	39.560820
2726.785939	511295.126709	39.565837
2729.666241	512302.433827	39.570855
2732.992539	513280.773069	39.575872
2736.005617	514272.509532	39.580890
2739.420193	515256.910326	39.585908
2742.641325	516243.397640	39.590925
2745.196461	517235.626662	39.595943
2748.339610	518209.807853	39.600960
2751.438556	519204.440811	39.605978
2754.643806	520176.572930	39.610996
2757.674417	521136.833805	39.616013
2760.621837	522102.438026	39.621031
2763.523030	523073.730818	39.626048
2765.969194	524041.259133	39.631066
2768.946497	525006.572672	39.636084
2772.208356	525960.143904	39.641101
2774.884610	526924.276023	39.646119
2777.685859	527877.750856	39.651136
2780.839665	528833.724490	39.656154
2783.804255	529780.101718	39.661172
2787.148150	530728.973445	39.666189
2789.502019	531671.504098	39.671207
2792.419742	532615.491689	39.676224
2794.903880	533557.275284	39.681242
2797.420342	534505.233691	39.686260
2800.552922	535443.868499	39.691277
2802.913698	536403.857412	39.696295
2805.670104	537364.320739	39.701312
2808.000254	538318.701809	39.706330
2810.700620	539277.737823	39.711348
2813.428358	540242.691787	39.716365
2815.669131	541215.106274	39.721383
2818.789147	542190.779455	39.726400
2821.235915	543168.759997	39.731418
2823.743806	544137.960881	39.736436
2826.842066	545082.252363	39.741453
2829.412719	546035.267433	39.746471
2832.216527	546972.740434	39.751488
2834.727144	547928.099458	39.756506
2837.235179	548891.337037	39.761524
2839.992445	549846.120001	39.766541
2842.080720	550826.737206	39.771559
2844.814471	551789.281305	39.776576
2847.577738	552797.444089	39.781594
2849.792000	553798.183961	39.786612
2852.294841	554809.456748	39.791629
2854.999996	555826.198362	39.796647
2857.914246	556863.431082	39.801664
2860.555549	557902.236355	39.806682
2862.977886	558950.743914	39.811700
2865.925554	559993.856895	39.816717
2868.872780	561059.945387	39.821735
2871.531469	562134.835902	39.826752
2874.607348	563200.829953	39.831770
2877.250676	564278.761557	39.836788
2880.418389	565362.543397	39.841805
2883.518335	566453.175448	39.846823
2886.956792	567529.399927	39.851840
2890.259524	568612.535488	39.856858
2893.875819	569688.951378	39.861876
2897.601986	570742.970932	39.866893
2900.303553	571812.331409	39.871911
2903.503459	572882.874469	39.876928
2906.667767	573953.332799	39.881946
2909.400674	575028.187413	39.886964
2912.632371	576089.320034	39.891981
2915.202391	577154.887211	39.896999
2918.188015	578225.963498	39.902016
2921.156989	579296.599061	39.907034
2924.494658	580358.754710	39.912052
2927.182645	581437.577599	39.917069
2930.001657	582521.750483	39.922087
2933.271363	583589.305157	39.927104
2936.400054	584661.503044	39.932122
2939.352421	585733.785991	39.937140
2942.336129	586795.491263	39.942157
2945.487660	587888.054428	39.947175
2948.095528	588955.195877	39.952192
2950.923485	590048.418103	39.957210
2953.313262	591138.756325	39.962228
2956.457537	592229.922269	39.967245
2959.240740	593329.465248	39.972263
2961.544119	594429.837092	39.977280
2964.595915	595547.766348	39.982298
2967.366797	596668.691196	39.987316
2970.026937	597793.884486	39.992333
2972.575414	598924.246207	39.997351
2975.595085	600059.477752	40.002368
2978.669927	601196.040950	40.007386
2981.558716	602344.438726	40.012404
2984.435005	603487.066965	40.017421
2987.584836	604647.055666	40.022439
2990.356664	605793.775544	40.027456
2993.277046	606958.622052	40.032474
2996.024632	608129.132128	40.037492
2999.338366	609283.866204	40.042509
3002.338982	610458.845944	40.047527
3005.353655	611611.989315	40.052544
3008.604082	612772.827855	40.057562
3011.711914	613938.170324	40.062580
3015.468299	615089.830570	40.067597
3018.255402	616257.182517	40.072615
3020.882138	617406.287666	40.077632
3024.219551	618519.959313	40.082650
3027.328528	619638.404327	40.087668
3030.369420	620741.700788	40.092685
3034.067482	621851.623691	40.097703
3037.105922	622943.301587	40.102720
3040.430179	624030.974290	40.107738
3043.722388	625124.987700	40.112756
3046.878153	626208.620687	40.117773
3050.225437	627298.606171	40.122791
3053.670317	628391.411037	40.127808
3056.833535	629472.713124	40.132826
3059.528176	630559.275782	40.137844
3062.800327	631631.350337	40.142861
3066.369592	632714.999645	40.147879
3069.409763	633789.788228	40.152896
3072.521576	634866.800690	40.157914
3075.436872	635954.465611	40.162932
3078.679123	637047.452487	40.167949
3081.902025	638133.041634	40.172967
3084.880671	639221.600816	40.177984
3088.207353	640308.889809	40.183002
3090.930998	641406.888898	40.188020
3093.818424	642498.308544	40.193037
3096.850731	643618.614942	40.198055
3099.127935	644735.880787	40.203072
3102.285715	645853.725657	40.208090
3104.752779	646993.149940	40.213108
3107.648555	648135.216145	40.218125
3110.389750	649287.945084	40.223143
3113.877494	650448.542043	40.228160
3117.000794	651599.545685	40.233178
3119.809854	652770.848539	40.238196
3122.982523	653945.639902	40.243213
3125.770572	655125.934847	40.248231
3128.759142	656306.702808	40.253248
3132.484886	657509.370541	40.258266
3135.106186	658704.503538	40.263284
3138.433393	659908.386076	40.268301
3141.636600	661115.376247	40.273319
3144.615790	662317.424366	40.278336
3148.009842	663525.277102	40.283354
3150.905711	664741.620908	40.288372
3154.214954	665955.652195	40.293389
3158.041261	667167.951220	40.298407
3161.070430	668389.033581	40.303424
3164.157051	669608.904940	40.308442
3167.557912	670847.168830	40.313460
3170.502491	672057.297826	40.318477
3173.379171	673285.978654	40.323495
3176.602254	674512.750880	40.328512
3179.700220	675745.248698	40.333530
3182.610630	676994.762475	40.338548
3185.606365	678236.241855	40.343565
3188.861677	679485.462373	40.348583
3191.932889	680745.971531	40.353600
3195.063412	682000.038798	40.358618
3197.890695	683269.531466	40.363636
3201.453624	684528.495458	40.368653
3204.472444	685791.397524	40.373671
3208.126853	687055.111089	40.378688
3211.667371	688307.695893	40.383706
3214.512063	689575.757747	40.388724
3217.625578	690846.226596	40.393741
3220.805462	692116.305820	40.398759
3223.451114	693400.085583	40.403776
3226.423358	694679.806433	40.408794
3229.566261	695971.020127	40.413812
3232.620401	697247.082855	40.418829
3236.019009	698502.127385	40.423847
3239.075637	699742.175469	40.428864
3242.054853	700986.571810	40.433882
3245.208603	702252.372164	40.438900
3248.137221	703499.094635	40.443917
3251.479438	704752.655278	40.448935
3254.680010	706022.605037	40.453952
3258.111630	707291.239716	40.458970
3261.430698	708562.726928	40.463988
3264.529235	709838.518750	40.469005
3268.062226	711111.720983	40.474023
3271.093955	712397.192175	40.479040
3274.723852	713681.280756	40.484058
3277.850487	714965.208055	40.489076
3281.011222	716258.682463	40.494093
3284.208278	717545.668330	40.499111
3287.669106	718856.405019	40.504128
3290.928505	720165.534897	40.509146
3294.323835	721487.393006	40.514164
3297.538087	722800.516495	40.519181
3301.117233	724122.665313	40.524199
3304.207751	725444.287405	40.529216
3308.013943	726766.418798	40.534234
3311.333510	728093.259667	40.539252
3315.323282	729405.545494	40.544269
3318.864814	730716.854039	40.549287
3322.228450	732039.438288	40.554304
3325.424594	733368.895396	40.559322
3328.618641	734704.255831	40.564340
3331.970367	736031.469994	40.569357
3335.411790	737364.322832	40.574375
3338.359697	738721.116568	40.579392
3341.752045	740059.349963	40.584410
3344.964393	741407.450960	40.589428
3348.485095	742755.320534	40.594445
3352.037581	744117.600744	40.599463
3354.994330	745477.869648	40.604480
3358.647419	746848.287546	40.609498
3362.020926	748208.752017	40.614516
3364.759650	749591.505900	40.619533
3368.358418	750955.246806	40.624551
3371.668040	752343.327599	40.629568
3375.284928	753721.207753	40.634586
3378.855037	755113.868104	40.639604
3381.735839	756501.761024	40.644621
3385.137083	757890.743222	40.649639
3388.418754	759291.943691	40.654656
3392.073215	760697.203270	40.659674
3395.981772	762081.200814	40.664692
3399.280476	763486.295136	40.669709
3402.984910	764879.403750	40.674727
3406.061010	766302.695982	40.679744
3409.582350	767684.396076	40.684762
3413.278107	769089.158578	40.689780
3416.532642	770497.806889	40.694797
3419.646575	771906.259214	40.699815
3422.705241	773327.666173	40.704832
3425.783809	774745.062085	40.709850
3428.987575	776184.309752	40.714868
3431.677466	777624.880572	40.719885
3435.619090	779069.278953	40.724903
3438.538897	780522.146906	40.729920
3442.087615	781968.191230	40.734938
3445.424235	783443.954059	40.739956
3448.413894	784911.721644	40.744973
3452.124188	786370.389753	40.749991
3455.403722	787840.352068	40.755008
3458.997559	789296.503335	40.760013
3462.379511	790700.768364	40.765018
3465.586263	792070.545027	40.770023
3469.211769	793355.265887	40.775028
3472.607282	794597.510678	40.780032
3475.528980	795744.906466	40.785037
3479.239054	796830.475167	40.790042
3482.433546	797839.441530	40.795047
3485.917576	798780.735353	40.800052
3489.148261	799629.399133	40.805056
3491.822839	800407.644543	40.810061
3494.545550	801105.534505	40.815066
3496.851867	801749.953716	40.820071
3498.682629	802304.580615	40.825076
3500.514720	802834.394135	40.830080
3502.218408	803295.184455	40.835085
3504.071612	803692.264906	40.840090
3505.241098	804052.264726	40.845095
3506.924325	804350.670162	40.850100
3508.011417	804618.907282	40.855104
3509.218702	804828.373514	40.860109
3510.364709	805012.592518	40.865114
3511.035023	805159.328293	40.870119
3512.260333	805262.235249	40.875124
3512.768770	805348.540370	40.880128
3513.339636	805384.629206	40.885133
3514.667726	805403.285772	40.890138
3514.852701	805394.038018	40.895143
3515.566076	805368.866751	40.900148
3516.200937	805330.519641	40.905152
3516.322211	805247.150322	40.910157
3517.223174	805167.132274	40.915162
3517.673613	805056.494577	40.920167
3518.475906	804921.085025	40.925172
3518.533465	804795.259165	40.930176
3518.894703	804625.642800	40.935181
3519.379294	804448.254322	40.940186
3519.444752	804263.476996	40.945191
3519.601447	804066.076915	40.950196
3519.832882	803858.213451	40.955200
3520.081483	803636.413271	40.960205
3520.305192	803406.321871	40.965210
3520.504527	803176.619155	40.970215
3520.700511	802928.173811	40.975220
3520.447427	802689.308955	40.980224
3520.611969	802426.185444	40.985229
3520.649935	802163.318061	40.990234
3520.687077	801908.877945	40.995239
3520.823692	801640.431324	41.000244
3521.168964	801362.864238	41.005248
3521.090528	801080.597292	41.010253
3521.007430	800783.208765	41.015258
3521.049710	800502.713541	41.020263
3520.991376	800197.494698	41.025268
3521.055718	799921.093748	41.030272
3521.200421	799625.384258	41.035277
3521.155591	799328.417621	41.040282
3520.928184	799019.985219	41.045287
3521.231407	798713.463533	41.050292
3520.575965	798403.307741	41.055296
3520.907621	798098.079325	41.060301
3521.005143	797786.740919	41.065306
3520.701863	797491.799959	41.070311
3520.800170	797174.053054	41.075316
3520.742355	796874.578515	41.080320
3520.544384	796557.441537	41.085325
3520.953939	796245.442729	41.090330
3520.690796	795933.737535	41.095335
3520.692894	795611.025837	41.100340
3520.699996	795294.435911	41.105344
3520.424771	794987.011306	41.110349
3520.766597	794664.739963	41.115354
3520.170974	794354.345177	41.120359
3519.861375	794018.745710	41.125364
3519.881597	793716.864093	41.130368
3519.639439	793408.284369	41.135373
3519.774708	793099.137573	41.140378
3519.704361	792790.600577	41.145383
3519.535292	792473.077484	41.150388
3519.280111	792173.139898	41.155392
3519.519068	791868.392001	41.160397
3519.431249	791555.333522	41.165402
3518.970081	791265.707831	41.170407
3518.811399	790943.545237	41.175412
3519.052124	790642.969355	41.180416
3518.793269	790348.605058	41.185421
3518.799431	790053.349400	41.190426
3518.333114	789753.589625	41.195431
3518.932868	789457.473961	41.200436
3518.536758	789155.416816	41.205440
3518.573830	788862.268709	41.210445
3518.223129	788562.537765	41.215450
3518.016639	788274.320311	41.220455
3518.001840	787972.002360	41.225460
3517.949807	787680.098131	41.230464
3517.835902	787394.828062	41.235469
3517.532563	787104.907972	41.240474
3517.698491	786827.286557	41.245479
3517.673117	786535.773465	41.250484
3517.309434	786258.659888	41.255488
3516.954326	785964.965649	41.260493
3517.357849	785687.211470	41.265498
3517.080631	785403.068751	41.270503
3517.037419	785123.252249	41.275508
3516.487603	784853.785551	41.280512
3516.724335	784581.769196	41.285517
3516.614097	784304.980602	41.290522
3516.048720	784040.501847	41.295527
3516.162267	783762.966865	41.300532
3516.067135	783506.357841	41.305536
3515.820220	783243.518448	41.310541
3515.960688	782978.047796	41.315546
3515.905839	782713.583366	41.320551
3515.739484	782444.503894	41.325556
3515.301729	782189.921259	41.330560
3515.469806	781928.293391	41.335565
3515.554515	781673.901343	41.340570
3514.823397	781436.755270	41.345575
3515.047535	781181.535690	41.350580
3515.080813	780937.211647	41.355584
3515.124032	780696.420154	41.360589
3515.199196	780433.326646	41.365594
3514.894366	780195.282123	41.370599
3515.164889	779933.073023	41.375604
3514.988081	779701.043420	41.380608
3514.825332	779439.232497	41.385613
3514.954469	779196.802232	41.390618
3514.655508	778951.826343	41.395623
3514.473360	778699.834450	41.400628
3514.182242	778457.005993	41.405632
3513.943417	778233.798573	41.410637
3514.499738	777984.858982	41.415642
3513.936919	777753.076988	41.420647
3513.691949	777524.828307	41.425652
3513.699103	777294.315733	41.430656
3513.817786	777055.655242	41.435661
3513.848281	776828.274497	41.440666
3513.797156	776611.681185	41.445671
3513.871405	776379.011762	41.450676
3513.320126	776155.201509	41.455680
3513.279696	775925.342775	41.460685
3513.054496	775690.633116	41.465690
3512.918365	775485.393639	41.470695
3512.835625	775260.592304	41.475700
3512.922025	775049.641510	41.480704
3512.945623	774841.846401	41.485709
3512.750641	774627.581605	41.490714
3512.276512	774425.864444	41.495719
3512.557480	774192.845110	41.500724
3512.650328	773994.961976	41.505728
3512.228470	773789.081992	41.510733
3512.644376	773580.299855	41.515738
3512.053930	773379.311871	41.520743
3512.071235	773165.067787	41.525748
3512.196288	772971.239637	41.530752
3511.892249	772763.341322	41.535757
3511.981332	772565.617342	41.540762
3511.949099	772365.100455	41.545767
3511.691450	772163.580936	41.550772
3511.729825	771969.937786	41.555776
3511.437953	771771.664338	41.560781
3511.668289	771586.649319	41.565786
3511.222412	771404.450896	41.570791
3511.226823	771195.718429	41.575796
3511.161024	771019.310195	41.580800
3510.936649	770820.556648	41.585805
3511.366011	770640.313227	41.590810
3511.152800	770462.487279	41.595815
3510.915285	770269.288554	41.600820
3510.840991	770091.726363	41.605824
3510.655968	769908.708873	41.610829
3510.756940	769721.352710	41.615834
3510.575197	769550.003884	41.620839
3510.352339	769364.613970	41.625844
3510.187662	769194.486030	41.630848
3510.198934	769031.470594	41.635853
3510.285888	768851.979448	41.640858
3510.082505	768695.152142	41.645863
3510.119076	768515.661195	41.650868
3510.084231	768348.794352	41.655872
3510.026102	768179.364801	41.660877
3510.122724	768011.975826	41.665882
3509.718044	767854.474042	41.670887
3509.657093	767682.470716	41.675892
3509.888690	767533.383827	41.680896
3509.536728	767365.167232	41.685901
3509.709670	767210.020867	41.690906
3509.626104	767047.815574	41.695911
3509.681218	766884.597966	41.700916
3509.720832	766729.857991	41.705920
3509.420507	766566.593574	41.710925
3509.448489	766402.729068	41.715930
3509.184440	766253.008341	41.720935
3509.073172	766091.674195	41.725940
3509.142275	765939.229997	41.730944
3509.010168	765795.443548	41.735949
3509.196196	765641.347035	41.740954
3508.816043	765487.143702	41.745959
3509.265681	765332.602847	41.750964
3508.917383	765190.812647	41.755968
3508.904090	765047.731761	41.760973
3508.939072	764881.416791	41.765978
3508.595503	764746.816161	41.770983
3508.640424	764606.872914	41.775988
3508.625758	764466.197262	41.780992
3508.404376	764326.539338	41.785997
3508.403415	764180.431932	41.791002
3508.387640	764049.265703	41.796007
3508.461331	763899.984528	41.801012
3508.004838	763763.264443	41.806016
3508.047738	763629.319600	41.811021
3507.881286	763487.664396	41.816026
3507.768635	763373.121760	41.821031
3507.908817	763227.810880	41.826036
3508.208617	763106.192936	41.831040
3508.137737	762978.272124	41.836045
3508.197780	762834.988986	41.841050
3507.913213	762713.757192	41.846055
3507.988530	762567.556510	41.851060
3508.064257	762446.507482	41.856064
3507.730466	762317.977705	41.861069
3507.249289	762191.591034	41.866074
3507.252537	762059.005876	41.871079
3507.446354	761935.512195	41.876084
3507.308067	761822.627290	41.881088
3507.327435	761698.566641	41.886093
3507.553532	761583.250219	41.891098
3507.140017	761463.302153	41.896103
3507.260005	761335.864542	41.901108
3506.883278	761228.683087	41.906112
3506.746846	761116.576604	41.911117
3507.212051	760987.694798	41.916122
3506.744574	760881.658054	41.921127
3507.151943	760763.092528	41.926132
3507.123254	760654.760078	41.931136
3507.077579	760539.867326	41.936141
3506.840445	760424.412440	41.941146
3506.597817	760313.693007	41.946151
3506.684106	760198.822607	41.951156
3506.867338	760091.039114	41.956160
3506.644464	759985.294746	41.961165
3506.830354	759872.179126	41.966170
3506.710632	759770.312522	41.971175
3506.568469	759659.714946	41.976180
3506.264558	759557.037121	41.981184
3506.478065	759444.157259	41.986189
3506.736596	759343.307938	41.991194
3506.472761	759244.171937	41.996199
3506.608028	759134.359693	42.001204
3506.517699	759029.715011	42.006208
3506.061769	758930.656003	42.011213
3506.524271	758824.782191	42.016218
3505.906936	758722.687678	42.021223
3506.024283	758624.368833	42.026228
3506.086689	758522.850167	42.031232
3505.598759	758427.589691	42.036237
3505.844178	758329.640661	42.041242
3505.837653	758249.053853	42.046247
3505.827164	758157.511036	42.051252
3505.691646	758059.029269	42.056256
3505.268005	757971.401880	42.061261
3505.351385	757880.185677	42.066266
3505.509307	757798.678581	42.071271
3505.396933	757716.672395	42.076276
3505.558598	757618.728061	42.081280
3505.591730	757538.077819	42.086285
3505.722706	757441.616917	42.091290
3505.290120	757362.325013	42.096295
3505.414627	757275.339360	42.101300
3505.337229	757192.532053	42.106304
3505.371140	757111.679744	42.111309
3505.526454	757020.095860	42.116314
3505.577544	756943.878576	42.121319
3505.090420	756848.055254	42.126324
3505.380605	756757.630548	42.131328
3505.094666	756674.704004	42.136333
3505.347347	756591.193941	42.141338
3504.970695	756521.756177	42.146343
3505.010237	756435.959667	42.151348
3505.334212	756355.989292	42.156352
3505.046775	756279.574509	42.161357
3505.024696	756189.935130	42.166362
3504.659988	756129.475932	42.171367
3505.068835	756045.193642	42.176372
3505.056759	755970.408645	42.181376
3504.535287	755899.557579	42.186381
3504.974678	755815.317075	42.191386
3504.713918	755747.087258	42.196391
3504.884712	755670.541294	42.201396
3504.720379	755597.456277	42.206400
3504.470705	755517.325100	42.211405
3504.724289	755446.144278	42.216410
3504.496234	755386.100930	42.221415
3504.444951	755313.636309	42.226420
3504.504653	755239.375364	42.231424
3504.214658	755185.758699	42.236429
3504.412017	755108.758403	42.241434
3504.315198	755052.442887	42.246439
3504.434984	754972.936145	42.251444
3504.610405	754919.388815	42.256448
3504.302448	754845.036693	42.261453
3504.243764	754773.999979	42.266458
3503.963115	754718.946701	42.271463
3503.857223	754651.915848	42.276468
3504.500278	754592.462919	42.281472
3504.003671	754539.073366	42.286477
3504.314075	754465.306606	42.291482
3504.350628	754414.049920	42.296487
3504.395555	754346.843354	42.301492
3504.506158	754277.008441	42.306496
3504.339209	754218.328361	42.311501
3504.389542	754145.539653	42.316506
3504.262609	754086.901332	42.321511
3503.962760	754027.994875	42.326516
3503.703656	753955.304879	42.331520
3503.794892	753900.134890	42.336525
3504.250298	753837.941970	42.341530
3503.754037	753786.966664	42.346535
3503.651695	753723.037974	42.351540
3504.120965	753670.174061	42.356544
3503.770131	753627.518792	42.361549
3503.985240	753550.697459	42.366554
3504.136278	753497.884953	42.371559
3504.294336	753444.873402	42.376564
3504.414380	753376.065744	42.381568
3503.847252	753328.407656	42.386573
3504.027094	753258.700196	42.391578
3503.879024	753206.972149	42.396583
3503.777427	753139.631095	42.401588
3504.084906	753084.320755	42.406592
3503.809079	753022.291474	42.411597
3503.870155	752965.193803	42.416602
3504.170834	752905.833815	42.421607
3503.562130	752848.105197	42.426612
3503.885274	752801.679492	42.431616
3503.666225	752738.107600	42.436621
3503.779278	752681.196777	42.441626
3503.676525	752630.938946	42.446631
3503.588419	752578.060882	42.451636
3503.528995	752524.782620	42.456640
3503.626974	752475.379565	42.461645
3503.515667	752422.751205	42.466650
3503.551577	752370.838975	42.471655
3503.675918	752327.159598	42.476660
3503.540331	752268.261905	42.481664
3503.234977	752229.443667	42.486669
3503.337860	752173.913665	42.491674
3503.489922	752135.858979	42.496679
3503.647617	752076.219901	42.501684
3503.364632	752027.321441	42.506688
3503.448361	751988.091958	42.511693
3503.558712	751922.878418	42.516698
3503.178999	751884.515247	42.521703
3503.039980	751834.406390	42.526708
3502.947075	751794.019720	42.531712
3503.168344	751758.421312	42.536717
3503.122746	751710.617624	42.541722
3503.337563	751674.032053	42.546727
3503.088556	751630.410434	42.551732
3503.351935	751576.677139	42.556736
3502.998614	751549.865872	42.561741
3503.215565	751481.667406	42.566746
3503.157614	751459.104245	42.571751
3503.236428	751410.685418	42.576756
3503.267197	751367.213652	42.581760
3503.165269	751323.862361	42.586765
3503.287148	751266.297521	42.591770
3503.077320	751229.533049	42.596775
3503.011267	751190.867618	42.601780
3503.201398	751144.058771	42.606784
3503.160925	751098.275671	42.611789
3503.387409	751043.359267	42.616794
3503.153820	751008.672315	42.621799
3503.024377	750958.408004	42.626804
3503.441411	750922.378223	42.631808
3503.311705	750881.647088	42.636813
3503.251188	750832.309116	42.641818
3503.090282	750795.139312	42.646823
3502.990673	750749.907300	42.651828
3503.100533	750700.441535	42.656832
3502.683574	750671.217205	42.661837
3502.746531	750624.969623	42.666842
3503.024216	750597.507380	42.671847
3502.570146	750546.553053	42.676852
3502.971813	750501.187347	42.681856
3502.864218	750477.839132	42.686861
3503.021776	750434.390573	42.691866
3503.148436	750397.961742	42.696871
3502.754657	750358.407702	42.701876
3503.177855	750313.037339	42.706880
3502.938698	750284.177370	42.711885
3503.046120	750234.165619	42.716890
3503.071009	750195.035571	42.721895
3502.758418	750160.012058	42.726900
3503.000451	750123.612272	42.731904
3502.873087	750092.707626	42.736909
3503.042526	750046.587203	42.741914
3502.753242	750015.066770	42.746919
3502.304664	749967.862342	42.751924
3502.472352	749936.463684	42.756928
3502.603451	749907.985755	42.761933
3502.634913	749873.249912	42.766938
3502.813190	749835.920642	42.771943
3502.490866	749804.553025	42.776948
3502.873451	749765.262888	42.781952
3502.690782	749743.456404	42.786957
3502.937112	749688.477718	42.791962
3502.630220	749659.824236	42.796967
3502.661586	749631.757017	42.801972
3502.888437	749589.329787	42.806977
3502.409552	749559.666841	42.811981
3502.669138	749524.397679	42.816986
3502.757119	749498.296861	42.821991
3502.591202	749464.481117	42.826996
3502.514142	749427.488520	42.832001
3502.301225	749400.300746	42.837005
3502.584241	749366.064537	42.842010
3502.447238	749347.806696	42.847015
3502.436656	749304.033746	42.852020
3502.139950	749270.386992	42.857025
3502.183330	749250.863923	42.862029
3502.538137	749222.346511	42.867034
3502.292727	749188.937967	42.872039
3502.442900	749164.505627	42.877044
3502.423618	749141.089382	42.882049
3502.202648	749103.921391	42.887053
3502.313087	749079.347123	42.892058
3502.218068	749049.668196	42.897063
3501.914698	749029.707785	42.902068
3502.206804	748998.334184	42.907073
3501.952961	748980.638290	42.912077
3502.289201	748960.028495	42.917082
3502.305393	748937.989244	42.922087
3502.215288	748906.085518	42.927092
3502.418041	748877.987253	42.932097
3501.833948	748855.404639	42.937101
3501.752847	748826.167250	42.942106
3501.830066	748818.001893	42.947111
3502.348440	748781.401922	42.952116
3502.091643	748767.856531	42.957121
3501.877097	748738.245578	42.962125
3501.707709	748725.673887	42.967130
3501.777169	748707.083953	42.972135
3501.951613	748683.387258	42.977140
3501.870502	748670.800891	42.982145
3502.331476	748644.190862	42.987149
3502.360502	748617.059186	42.992154
3502.116224	748590.417288	42.997159
3501.602193	748571.281101	43.002164
3501.938498	748553.832592	43.007169
3502.081162	748528.707726	43.012173
3501.983171	748512.665028	43.017178
3501.482582	748494.366441	43.022183
3501.631979	748475.021554	43.027188
3501.654941	748465.234176	43.032193
3501.549344	748455.171554	43.037197
3501.723233	748422.530437	43.042202
3501.760111	748416.446672	43.047207
3501.505795	748402.406102	43.052212
3501.761913	748374.346614	43.057217
3501.615101	748366.711940	43.062221
3501.839119	748348.145020	43.067226
3501.627518	748329.402978	43.072231
3501.638193	748310.179434	43.077236
3502.129585	748295.867195	43.082241
3501.876182	748278.812009	43.087245
3501.830262	748249.764294	43.092250
3502.004168	748241.236456	43.097255
3501.892078	748218.178669	43.102260
3502.022685	748193.054713	43.107265
3501.728067	748176.796745	43.112269
3501.910576	748154.579546	43.117274
3501.768164	748159.198776	43.122279
3501.701314	748130.549393	43.127284
3501.780209	748109.732805	43.132289
3501.637986	748116.674533	43.137293
3501.818157	748071.578334	43.142298
3501.952602	748055.644528	43.147303
3501.739841	748046.488562	43.152308
3502.141082	748010.892642	43.157313
3501.616355	748007.965135	43.162317
3501.629222	747982.810543	43.167322
3501.577433	747972.441910	43.172327
3501.721311	747947.759713	43.177332
3501.736907	747943.260407	43.182337
3501.648346	747935.763931	43.187341
3501.500280	747904.261004	43.192346
3501.733905	747913.216284	43.197351
3501.961030	747890.595630	43.202356
3502.001638	747860.593254	43.207361
3501.818420	747846.144596	43.212365
3501.906345	747819.148656	43.217370
3501.894955	747807.587123	43.222375
3501.357615	747785.932588	43.227380
3501.912156	747756.833221	43.232385
3501.858279	747743.104255	43.237389
3501.638375	747744.771497	43.242394
3501.667045	747718.180338	43.247399
3501.880932	747714.636480	43.252404
3501.830591	747698.485394	43.257409
3501.256193	747669.374599	43.262413
3501.686045	747655.664374	43.267418
3501.639157	747649.939779	43.272423
3501.522143	747637.604762	43.277428
3501.581484	747612.490713	43.282433
3501.779536	747603.908771	43.287437
3501.897951	747596.278927	43.292442
3501.962460	747564.640660	43.297447
3501.578394	747553.436849	43.302452
3501.862816	747543.160337	43.307457
3501.582790	747534.805582	43.312461
3501.881996	747509.305631	43.317466
3501.528400	747505.756623	43.322471
3501.495401	747481.596370	43.327476
3501.827132	747459.006599	43.332481
3502.039232	747450.669263	43.337485
3501.854030	747426.830508	43.342490
3501.769247	747406.434447	43.347495
3501.836321	747400.591996	43.352500
3501.778471	747369.071997	43.357505
3501.999744	747370.320471	43.362509
3501.987310	747344.031347	43.367514
3502.038262	747314.667620	43.372519
3501.515735	747308.082396	43.377524
3501.800105	747277.988075	43.382529
3501.692708	747268.368998	43.387533
3501.784699	747258.371016	43.392538
3501.743259	747244.392015	43.397543
3501.364093	747218.261914	43.402548
3501.835323	747203.506227	43.407553
3501.661254	747194.441705	43.412557
3501.766431	747176.534110	43.417562
3501.721930	747161.319943	43.422567
3501.609621	747155.556375	43.427572
3501.823162	747129.377447	43.432577
3501.503259	747123.055107	43.437581
3501.799112	747103.287247	43.442586
3501.605613	747085.824174	43.447591
3501.386140	747066.289647	43.452596
3502.046769	747059.113311	43.457601
3501.591065	747043.917448	43.462605
3501.823730	747015.511001	43.467610
3501.762044	747010.677976	43.472615
3501.769707	747001.237242	43.477620
3501.717958	746973.520129	43.482625
3501.624492	746967.259086	43.487629
3501.782973	746956.656663	43.492634
3501.780908	746931.945951	43.497639
3501.577009	746927.630601	43.502644
3501.942094	746914.522854	43.507649
3501.619202	746900.985131	43.512653
3501.596598	746866.294226	43.517658
3502.140876	746868.724974	43.522663
3501.554763	746850.189531	43.527668
3501.562700	746826.959523	43.532673
3501.427073	746827.822259	43.537677
3501.421028	746802.617565	43.542682
3501.533519	746779.172443	43.547687
3501.496985	746767.218136	43.552692
3501.694209	746768.371836	43.557697
3501.560435	746760.881701	43.562701
3501.781838	746742.360822	43.567706
3501.500991	746732.967443	43.572711
3501.248342	746734.343765	43.577716
3501.754360	746713.848258	43.582721
3501.229585	746694.363253	43.587725
3501.492437	746673.710131	43.592730
3501.334817	746672.994948	43.597735
3500.893032	746677.812798	43.602740
3501.525532	746675.088926	43.607745
3501.391158	746660.679421	43.612749
3501.677532	746633.745436	43.617754
3501.821118	746622.551930	43.622759
3501.715360	746625.782123	43.627764
3501.349278	746592.876620	43.632769
3501.507329	746577.380719	43.637773
3501.531114	746563.735693	43.642778
3501.536095	746562.598229	43.647783
3501.457701	746556.334365	43.652788
3501.386347	746535.488985	43.657793
3501.720062	746522.286917	43.662797
3501.759251	746520.204719	43.667802
3501.924062	746498.381136	43.672807
3501.831522	746490.389675	43.677812
3501.709474	746471.331810	43.682817
3501.813555	746449.864105	43.687821
3501.900810	746425.186456	43.692826
3501.726324	746423.930354	43.697831
3501.803402	746390.209376	43.702836
3501.824101	746377.651905	43.707841
3501.526714	746378.640273	43.712845
3501.753520	746347.365663	43.717850
3501.915512	746341.556162	43.722855
3501.531358	746322.986086	43.727860
3501.657597	746297.955609	43.732865
3501.573761	746295.695976	43.737869
3501.373211	746285.003698	43.742874
3501.878250	746279.038606	43.747879
3501.606016	746258.225684	43.752884
3501.391269	746237.403206	43.757889
3501.503367	746245.540234	43.762893
3501.488392	746221.471958	43.767898
3501.926557	746202.666846	43.772903
3501.783714	746194.238551	43.777908
3501.863375	746183.351545	43.782913
3501.880428	746157.399547	43.787917
3501.652455	746147.156458	43.792922
3501.997524	746118.382187	43.797927
3501.871240	746116.178944	43.802932
3501.455476	746098.206688	43.807937
3501.442803	746087.285380	43.812941
3501.395832	746065.050738	43.817946
3501.681298	746053.190409	43.822951
3501.348647	746053.789221	43.827956
3501.608369	746036.248900	43.832961
3501.639005	746018.746398	43.837965
3501.395694	746009.889653	43.842970
3501.632632	746001.101818	43.847975
3501.281564	745990.137440	43.852980
3501.501123	745956.143903	43.857985
3501.061414	745956.513271	43.862989
3501.331220	745950.438520	43.867994
3501.687338	745953.197231	43.872999
3501.505767	745948.976503	43.878004
3501.957165	745916.971058	43.883009
3501.678830	745910.294858	43.888013
3501.853004	745892.224635	43.893018
3501.655658	745872.436318	43.898023
3501.669611	745867.491226	43.903028
3501.688307	745859.925600	43.908033
3501.155595	745833.223083	43.913037
3501.462630	745826.845508	43.918042
3501.462844	745806.184075	43.923047
3501.363818	745820.090263	43.928052
3501.392270	745801.005892	43.933057
3501.623278	745779.021077	43.938061
3501.303006	745767.062701	43.943066
3501.706759	745763.536020	43.948071
3501.337559	745762.756857	43.953076
3501.452349	745733.870941	43.958081
3501.419463	745725.522829	43.963085
3501.399535	745711.240949	43.968090
3501.504125	745707.269381	43.973095
3501.305402	745701.963891	43.978100
3501.320765	745680.854751	43.983105
3501.522040	745674.889974	43.988109
3501.796669	745665.749522	43.993114
3501.538216	745654.719937	43.998119
3501.536355	745635.244728	44.003124
3502.044019	745610.297312	44.008129
3501.724246	745620.088147	44.013133
3501.482087	745587.306222	44.018138
3501.758816	745579.549389	44.023143
3501.717625	745572.042812	44.028148
3502.012552	745560.526194	44.033153
3501.541450	745538.656736	44.038157
3501.386142	745519.107734	44.043162
3501.616790	745510.715841	44.048167
3501.603001	745505.725675	44.053172
3502.122300	745466.737335	44.058177
3501.979648	745457.369011	44.063181
3501.991912	745440.955753	44.068186
3501.598333	745418.727124	44.073191
3501.293791	745419.469631	44.078196
3501.610361	745394.404814	44.083201
3501.554666	745385.714083	44.088205
3501.632916	745384.465476	44.093210
3501.804780	745375.440535	44.098215
3501.410117	745363.988158	44.103220
3501.730178	745332.002034	44.108225
3501.405428	745344.117364	44.113229
3501.390916	745333.047011	44.118234
3501.785826	745298.230723	44.123239
3501.273802	745293.026163	44.128244
3501.636594	745285.996311	44.133249
3501.305928	745287.830668	44.138253
3501.129803	745256.766594	44.143258
3501.281708	745246.014647	44.148263
3501.148477	745244.553801	44.153268
3501.665031	745229.292589	44.158273
3501.513061	745230.454797	44.163277
3501.473514	745226.655106	44.168282
3501.626753	745200.183098	44.173287
3501.285433	745194.999694	44.178292
3501.464662	745187.209155	44.183297
3501.523541	745184.975048	44.188301
3501.301406	745158.713235	44.193306
3501.754152	745142.275992	44.198311
3501.441107	745149.050842	44.203316
3501.631154	745139.874324	44.208321
3501.544659	745123.377855	44.213325
3501.188693	745115.922861	44.218330
3501.189521	745096.940209	44.223335
3501.145477	745100.605735	44.228340
3501.194029	745095.753307	44.233345
3501.425008	745095.665831	44.238349
3501.449247	745070.895463	44.243354
3501.360650	745062.803022	44.248359
3501.009552	745053.518096	44.253364
3501.361854	745034.328905	44.258369
3501.325816	745040.217685	44.263373
3501.504157	745038.013229	44.268378
3501.540099	745020.952532	44.273383
3501.483426	745012.113246	44.278388
3501.542594	744999.003427	44.283393
3501.340921	745005.018475	44.288397
3501.086252	744999.672317	44.293402
3501.614050	744969.331163	44.298407
3501.244253	744958.368429	44.303412
3501.379417	744946.234661	44.308417
3501.312396	744941.005757	44.313421
3501.289668	744939.773768	44.318426
3501.338180	744940.853451	44.323431
3501.037591	744911.143321	44.328436
3501.326319	744895.968549	44.333441
3501.317690	744900.122669	44.338445
3501.541962	744898.454372	44.343450
3501.615802	744893.449334	44.348455
3501.357938	744881.528724	44.353460
3501.484709	744848.188381	44.358465
3501.306764	744857.066885	44.363469
3501.126721	744854.773298	44.368474
3501.295746	744848.417741	44.373479
3501.624760	744847.226479	44.378484
3501.727612	744820.118854	44.383489
3501.524441	744810.463142	44.388493
3501.620099	744805.998238	44.393498
3501.754944	744790.107155	44.398503
3501.454097	744777.748566	44.403508
3501.812553	744757.717271	44.408513
3501.851911	744757.661461	44.413517
3501.603047	744729.820670	44.418522
3502.011179	744715.416799	44.423527
3501.733541	744693.661314	44.428532
3501.775454	744675.709022	44.433537
3501.923868	744671.877999	44.438541
3501.831712	744648.954693	44.443546
3501.948700	744634.351605	44.448551
3501.548857	744631.402158	44.453556
3501.409869	744608.980844	44.458561
3501.549036	744581.322586	44.463565
3501.500056	744571.591660	44.468570
3501.669307	744576.309803	44.473575
3501.360673	744551.938869	44.478580
3501.598932	744526.142664	44.483585
3501.609367	744525.547817	44.488589
3501.390542	744528.846993	44.493594
3501.891659	744513.488073	44.498599
3501.818601	744487.397125	44.503604
3501.573962	744474.682703	44.508609
3501.628824	744464.835608	44.513613
3501.570015	744442.598321	44.518618
3501.598630	744429.789230	44.523623
3500.844224	744444.448859	44.528628
3501.539474	744425.250947	44.533633
3501.419392	744415.284387	44.538637
3501.507995	744389.215835	44.543642
3501.505755	744381.405050	44.548647
3501.546071	744384.463706	44.553652
3501.241035	744380.410848	44.558657
3501.153550	744365.742175	44.563661
3500.808720	744343.700190	44.568666
3501.334471	744332.440264	44.573671
3501.339339	744341.585770	44.578676
3501.421467	744325.653022	44.583681
3501.347691	744332.290152	44.588685
3501.368918	744332.632846	44.593690
3501.998393	744304.151002	44.598695
3501.396368	744293.423469	44.603700
3501.597761	744284.342958	44.608705
3501.707903	744279.133774	44.613709
3501.593318	744250.725261	44.618714
3501.690333	744244.529436	44.623719
3501.221177	744239.613718	44.628724
3501.632542	744207.261852	44.633729
3501.410197	744197.954631	44.638733
3501.444673	744179.854116	44.643738
3501.282329	744185.319452	44.648743
3501.138833	744192.561499	44.653748
3501.440729	744175.702213	44.658753
3501.556750	744165.498558	44.663757
3501.656320	744144.668010	44.668762
3501.334851	744135.179335	44.673767
3501.488390	744142.174580	44.678772
3501.440817	744115.633225	44.683777
3501.639961	744096.912024	44.688781
3501.386298	744092.652764	44.693786
3501.775182	744079.684685	44.698791
3501.489558	744069.052876	44.703796
3502.049839	744050.815729	44.708801
3501.412092	744050.179644	44.713805
3501.403676	744032.481403	44.718810
3501.668919	744013.749081	44.723815
3501.287307	744005.357886	44.728820
3501.672237	743994.466838	44.733825
3501.734423	743999.944636	44.738829
3501.309281	743967.482823	44.743834
3501.764323	743948.867303	44.748839
3501.601922	743948.548183	44.753844
3501.634101	743930.991329	44.758849
3501.256746	743915.825864	44.763853
3501.510868	743906.439555	44.768858
3501.853451	743888.930193	44.773863
3501.686901	743884.458657	44.778868
3501.610735	743873.841410	44.783873
3501.561733	743873.602430	44.788877
3500.894994	743870.251823	44.793882
3501.254999	743862.875076	44.798887
3501.323812	743846.894117	44.803892
3501.425425	743824.925221	44.808897
3501.722477	743820.624245	44.813901
3501.695096	743824.485379	44.818906
3501.387058	743799.864800	44.823911
3501.438469	743789.374682	44.828916
3501.356486	743769.957529	44.833921
3501.575857	743770.168617	44.838925
3501.361908	743767.385888	44.843930
3501.158476	743742.797285	44.848935
3501.162331	743731.622754	44.853940
3501.220122	743726.471299	44.858945
3501.463215	743725.640172	44.863949
3501.126678	743731.480707	44.868954
3501.474177	743722.177634	44.873959
3501.422469	743716.253185	44.878964
3501.448153	743691.577116	44.883969
3501.575559	743683.694770	44.888973
3501.343567	743688.677529	44.893978
3501.632569	743679.285187	44.898983
3501.741313	743658.254064	44.903988
3501.573802	743638.603505	44.908993
3501.533174	743630.897206	44.913997
3501.401758	743625.381407	44.919002
3501.515952	743597.723818	44.924007
3501.246814	743592.774635	44.929012
3501.547011	743585.011965	44.934017
3501.401594	743580.487319	44.939021
3501.301516	743571.851359	44.944026
3501.818216	743546.253147	44.949031
3501.591133	743545.104154	44.954036
3501.304577	743533.927891	44.959041
3501.644364	743525.219187	44.964045
3501.397862	743509.784092	44.969050
3501.259965	743493.539913	44.974055
3501.232087	743499.131833	44.979060
3501.133970	743481.002179	44.984065
3500.817392	743483.675169	44.989069
3500.832817	743488.567722	44.994074
3501.156687	743488.316552	44.999079
3501.125366	743490.645733	45.004084
3501.470386	743480.205570	45.009089
3501.506270	743448.555418	45.014093
3501.483914	743448.064798	45.019098
3501.365262	743435.278426	45.024103
3501.304536	743436.821370	45.029108
3501.045872	743425.788677	45.034113
3501.484944	743403.317836	45.039117
3501.266794	743397.766766	45.044122
3501.073256	743388.849381	45.049127
3501.209733	743392.337535	45.054132
3501.514056	743396.589065	45.059137
3501.370389	743389.740118	45.064141
3501.718905	743382.809826	45.069146
3501.781141	743351.352708	45.074151
3501.573305	743347.134913	45.079156
3501.365611	743330.308591	45.084161
3501.714959	743313.637403	45.089165
3500.948745	743309.660201	45.094170
3501.319339	743301.242831	45.099175
3501.285067	743310.000442	45.104180
3501.413441	743294.453527	45.109185
3501.026837	743278.299450	45.114189
3501.139028	743270.963107	45.119194
3501.579496	743248.986052	45.124199
3501.216703	743259.380271	45.129204
3501.591663	743250.220442	45.134209
3501.530833	743248.005570	45.139213
3501.606461	743225.940408	45.144218
3501.599578	743214.074675	45.149223
3501.521087	743212.851630	45.154228
3501.398131	743215.393818	45.159233
3501.524467	743187.930569	45.164237
3501.098756	743172.969443	45.169242
3501.201991	743159.305368	45.174247
3501.221945	743159.945001	45.179252
3501.268995	743160.629603	45.184257
3501.327008	743154.488813	45.189261
3501.358146	743152.209270	45.194266
3501.214894	743130.377797	45.199271
3500.990528	743122.503578	45.204276
3501.063676	743122.788298	45.209281
3501.648150	743117.796639	45.214285
3501.526728	743118.014620	45.219290
3501.324909	743110.878361	45.224295
3501.468878	743091.273853	45.229300
3501.416280	743078.871559	45.234305
3501.349934	743066.422070	45.239309
3501.336528	743073.248070	45.244314
3501.613925	743055.994868	45.249319
3501.490530	743045.829330	45.254324
3501.332878	743029.834693	45.259329
3501.430273	743020.127104	45.264333
3501.106137	743030.663576	45.269338
3501.383527	743016.030980	45.274343
3501.388663	743000.306063	45.279348
3501.184694	742986.643011	45.284353
3501.384339	742974.990024	45.289357
3501.481411	742976.210296	45.294362
3501.390441	742969.105037	45.299367
3501.224262	742970.269919	45.304372
3501.390305	742945.271632	45.309377
3501.462759	742930.623298	45.314381
3501.422701	742935.426468	45.319386
3501.850593	742927.938739	45.324391
3501.812528	742902.974048	45.329396
3501.400816	742895.180010	45.334401
3501.292529	742873.539838	45.339405
3501.099826	742882.274659	45.344410
3501.439372	742870.993982	45.349415
3501.040959	742856.423325	45.354420
3500.948312	742835.225496	45.359425
3501.383553	742832.582389	45.364429
3501.073495	742829.617414	45.369434
3501.215598	742827.517232	45.374439
3501.309346	742819.095655	45.379444
3501.119221	742827.187281	45.384449
3501.492446	742832.070560	45.389453
3501.161693	742811.208706	45.394458
3501.313849	742793.876732	45.399463
3501.486085	742782.326888	45.404468
3501.243384	742781.032015	45.409473
3501.419024	742775.415426	45.414477
3501.249996	742788.399018	45.419482
3501.662691	742766.425212	45.424487
3501.624798	742753.921078	45.429492
3501.318535	742737.703163	45.434497
3501.580127	742731.676749	45.439501
3500.869002	742721.212328	45.444506
3501.351766	742702.342048	45.449511
3501.444900	742693.870990	45.454516
3501.192672	742680.264830	45.459521
3501.453270	742677.699983	45.464525
3501.517365	742685.502496	45.469530
3501.973392	742670.938638	45.474535
3501.656191	742645.524770	45.479540
3501.518739	742645.893761	45.484545
3501.442369	742627.758549	45.489549
3501.122647	742610.405256	45.494554
3501.711567	742597.698389	45.499559
3501.302709	742598.952880	45.504564
3501.200519	742589.277745	45.509569
3501.202129	742583.788681	45.514573
3501.170294	742582.656726	45.519578
3500.971781	742566.272301	45.524583
3501.024157	742559.538581	45.529588
3500.980039	742535.266027	45.534593
3501.307862	742537.832837	45.539597
3501.203001	742532.855833	45.544602
3501.362430	742537.774629	45.549607
3501.157386	742541.072351	45.554612
3501.009813	742546.338576	45.559617
3501.192621	742545.517294	45.564621
3501.059418	742544.995487	45.569626
3501.136983	742524.559894	45.574631
3501.058479	742508.353318	45.579636
3500.919562	742501.156658	45.584641
3501.231572	742497.346998	45.589645
3500.905749	742502.939413	45.594650
3501.059457	742490.106495	45.599655
3500.920241	742498.041693	45.604660
3500.947062	742489.581375	45.609665
3501.043760	742494.955618	45.614669
3500.758411	742490.107315	45.619674
3500.765012	742485.210762	45.624679
3500.779467	742499.400767	45.629684
3500.932299	742490.177869	45.634689
3500.882115	742495.971988	45.639693
3500.732505	742489.321039	45.644698
3501.073162	742486.792351	45.649703
3500.981107	742487.203297	45.654708
3500.784128	742488.719492	45.659713
3501.162064	742489.398921	45.664717
3500.800398	742489.607171	45.669722
3500.392493	742481.268136	45.674727
3500.478428	742495.446336	45.679732
3501.204983	742497.304410	45.684737
3501.103070	742497.321382	45.689741
3501.017455	742495.802699	45.694746
3501.403412	742490.200602	45.699751
3501.456444	742491.279876	45.704756
3501.235363	742494.085764	45.709761
3501.487342	742477.181653	45.714765
3501.224760	742461.648257	45.719770
3501.212913	742448.496477	45.724775
3501.136855	742450.437752	45.729780
3500.950057	742443.051150	45.734785
3501.171304	742447.267476	45.739789
3501.232197	742451.114695	45.744794
3501.323765	742445.017259	45.749799
3501.014552	742435.227796	45.754804
3501.024654	742403.824965	45.759809
3501.259678	742397.604883	45.764813
3501.071227	742394.026233	45.769818
3501.181842	742331.996270	45.774823
3500.980715	742217.153199	45.779828
3501.076162	742032.629541	45.784833
3501.125001	741804.885988	45.789837
3500.997741	741522.021206	45.794842
3500.933838	741175.779584	45.799847
3500.467344	740772.165161	45.804852
3500.241415	740313.931801	45.809857
3500.314564	739797.548231	45.814861
3500.229124	739226.591215	45.819866
3499.771176	738597.373798	45.824871
3499.398662	737915.694541	45.829876
3498.933810	737155.392666	45.834881
3498.419841	736348.507401	45.839885
3497.630319	735494.022862	45.844890
3497.597015	734574.676162	45.849895
3496.924510	733599.339406	45.854900
3496.679912	732561.132037	45.859905
3495.969597	731469.586390	45.864909
3494.934606	730315.198551	45.869914
3494.779738	729111.711350	45.874919
3494.435014	727847.886093	45.879924
3493.855119	726514.437239	45.884929
3493.312605	725116.539497	45.889933
3492.323947	723671.241819	45.894938
3492.064846	722137.823154	45.899943
3491.098205	720557.132539	45.904948
3489.987644	718930.687585	45.909953
3489.455910	717233.144470	45.914957
3488.500548	715472.714348	45.919962
3487.549632	713649.487082	45.924967
3486.399464	711779.241849	45.929972
3485.647989	709841.098047	45.934977
3484.769221	707853.224114	45.939981
3483.404206	705801.192891	45.944986
3481.877759	703694.446507	45.949991
3481.586092	701534.257605	45.954996
3480.417856	699310.102171	45.960001
3479.443776	697039.657165	45.965005
3478.074439	694701.602126	45.970010
3476.994269	692303.086987	45.975015
3475.576135	689856.809983	45.980020
3474.569840	687360.173429	45.985025
3473.186483	684795.794712	45.990029
3471.789910	682185.972614	45.995034
3470.533460	679514.557084	46.000039
3469.248007	676787.707264	46.005044
3467.587850	674018.945853	46.010049
3466.274391	671177.856327	46.015053
3464.833795	668291.790960	46.020058
3463.643725	665354.217122	46.025063
3462.135276	662363.441972	46.030068
3460.740377	659306.671650	46.035073
3458.945512	656203.962793	46.040077
3457.330826	653064.725932	46.045082
3455.876116	649861.204364	46.050087
3454.111627	646607.169842	46.055092
3452.463124	643299.112514	46.060097
3450.874075	639939.550315	46.065101
3449.069376	636532.942167	46.070106
3447.226987	633076.970986	46.075111
3445.924572	629563.142293	46.080116
3443.931942	626012.349989	46.085121
3442.149236	622383.536286	46.090125
3440.129991	618737.105082	46.095130
3438.247794	615026.262507	46.100135
3436.537225	611262.487577	46.105140
3434.754513	607464.746634	46.110145
3432.163045	603600.268997	46.115149
3430.197349	599703.658330	46.120154
3428.470651	595737.094870	46.125159
3426.472324	591745.372400	46.130164
3424.235410	587703.550362	46.135169
3422.219538	583601.063323	46.140173
3419.882341	579483.923700	46.145178
3417.745426	575301.239571	46.150183
3415.709198	571076.482694	46.155188
3413.200918	566807.259412	46.160193
3411.293838	562491.304293	46.165197
3408.805818	558135.588596	46.170202
3406.377987	553739.888440	46.175207
3403.923824	549299.917110	46.180212
3402.019404	544825.442535	46.185217
3399.362284	540286.810532	46.190221
3397.115552	535725.417461	46.195226
3394.792490	531102.989060	46.200231
3392.638877	526450.452068	46.205236
3390.159325	521752.836825	46.210241
3387.208312	517002.978995	46.215245
3384.718805	512232.995369	46.220250
3382.165690	507413.866631	46.225255
3379.239170	502564.034278	46.230260
3376.919255	497686.373413	46.235265
3374.185147	492744.884174	46.240269
3371.198822	487786.682369	46.245274
3368.605396	482777.204769	46.250279
3365.949491	477750.138512	46.255284
3362.984806	472681.534333	46.260289
3360.250772	467571.505279	46.265293
3357.484720	462443.356579	46.270298
3354.488941	457264.344767	46.275303
3351.725221	452073.177345	46.280308
3349.026180	446830.705574	46.285313
3345.832978	441553.862060	46.290317
3342.728602	436259.661975	46.295322
3339.885811	430926.126818	46.300327
3337.135582	425571.976411	46.305332
3333.788728	420186.458648	46.310337
3330.861721	414767.595990	46.315341
3327.881002	409325.619145	46.320346
3324.587273	403836.744220	46.325351
3321.519998	398336.008342	46.330356
3318.064782	392811.629586	46.335361
3315.198816	387245.175212	46.340365
3311.668343	381682.757918	46.345370
3308.653212	376090.767830	46.350375
3305.415586	370462.617017	46.355380
3302.150770	364813.712686	46.360385
3299.065222	359140.571093	46.365389
3295.124555	353453.446902	46.370394
3292.097362	347740.001660	46.375399
3288.985821	342005.194786	46.380404
3285.113522	336244.061497	46.385409
3281.755917	330468.493282	46.390413
3277.677025	324674.104612	46.395418
3274.213246	318868.124717	46.400423
3270.655784	313062.656054	46.405428
3266.954632	307236.698849	46.410433
3263.488129	301400.317668	46.415437
3259.658890	295562.086568	46.420442
3256.354635	289693.462447	46.425447
3252.878376	283820.428419	46.430452
3248.732261	277932.648855	46.435457
3245.540749	272043.095864	46.440461
3241.708474	266141.437457	46.445466
3237.818344	260216.675570	46.450471
3233.859986	254305.842141	46.455476
3229.807657	248381.613778	46.460481
3226.194695	242438.630816	46.465485
3222.275678	236508.800498	46.470490
3218.555166	230566.445173	46.475495
3214.345990	224622.477275	46.480500
3210.407432	218687.441032	46.485505
3206.287408	212748.882848	46.490509
3202.580731	206727.792374	46.495514
3198.495379	200772.307409	46.500519
3194.202323	194831.817256	46.505524
3189.862700	188894.634290	46.510529
3185.726755	182948.589514	46.515533
3181.721972	177036.882993	46.520538
3176.797086	171117.451767	46.525543
3173.017669	165211.773019	46.530548
3168.288946	159321.421417	46.535553
3164.348504	153432.724606	46.540557
3159.578411	147576.426742	46.545562
3155.509639	141709.975441	46.550567
3150.696830	135875.165102	46.555572
3146.129582	130044.491244	46.560577
3141.784122	124242.718008	46.565581
3136.331970	118450.419774	46.570586
3131.925749	112693.904669	46.575591
3127.586018	106947.468749	46.580596
3122.659976	101237.972537	46.585601
3117.850898	95550.002322	46.590605
3113.329204	89881.931036	46.595610
3108.155281	84244.108194	46.600615
3103.308035	78646.390216	46.605620
3097.887475	73064.867114	46.610625
3092.656313	67519.195629	46.615629
3087.437102	62020.827140	46.620634
3082.143189	56563.680162	46.625639
3076.665421	51146.241981	46.630644
3070.932018	45771.616048	46.635649
3064.692257	40463.224140	46.640653
3058.473285	35221.160646	46.645658
3051.451278	30035.752095	46.650663
3040.670302	25032.881148	46.655668
3023.413139	20315.484016	46.660673
3006.790681	15776.790597	46.665677
2989.002217	11509.794178	46.670682
2964.263018	7711.016216	46.675687
2931.180772	4488.260019	46.680692
2898.336653	1763.801432	46.685697
2841.236629	268.896834	46.690701
2760.866193	266.418517	46.695706
2722.494243	245.426370	46.700711
2722.564589	247.295886	46.705716
2744.083095	241.062108	46.710721
2771.918021	248.802121	46.715725
2795.024606	244.728448	46.720730
2808.910455	239.899484	46.725735
2813.833690	232.131295	46.730740
2811.908167	238.517510	46.735745
2807.260858	225.879489	46.740749
2801.888785	236.019059	46.745754
2796.799630	240.383267	46.750759
2793.418931	232.890190	46.755764
2790.419096	225.295003	46.760769
2788.200384	217.479949	46.765773
2786.021831	222.930437	46.770778
2783.516658	227.568677	46.775783
2780.519475	224.457971	46.780788
2777.686392	218.169795	46.785793
2775.060364	218.323204	46.790797
2771.598887	205.286090	46.795802
2768.228280	216.976597	46.800807
2765.158728	213.434070	46.805812
2761.992146	220.524800	46.810817
2758.895071	215.242560	46.815821
2755.813496	211.590535	46.820826
2752.764030	210.493858	46.825831
2749.634404	214.085789	46.830836
2745.774064	217.040113	46.835841
2742.591490	221.383200	46.840845
2739.638975	206.672304	46.845850
2735.988817	211.833209	46.850855
2733.149895	197.577727	46.855860
2729.636213	209.143540	46.860865
2726.195422	203.780290	46.865869
2723.155891	204.476385	46.870874
2719.716606	207.945543	46.875879
2716.036137	202.663617	46.880884
2712.777406	212.493881	46.885889
2709.668039	198.462371	46.890893
2706.060407	205.925309	46.895898
2702.858488	209.648036	46.900903
2699.478542	196.431146	46.905908
2695.849980	206.172270	46.910913
2693.008661	193.629918	46.915917
2689.035838	191.291168	46.920922
2685.378925	201.930339	46.925927
2682.422206	201.183040	46.930932
2678.879913	206.011970	46.935937
2675.509573	200.438184	46.940941
2672.164304	199.247270	46.945946
2668.633689	197.444314	46.950951
2665.291942	193.532127	46.955956
2661.578350	199.307640	46.960961
2658.116397	198.246169	46.965965
2654.544886	202.440185	46.970970
2651.099826	196.549830	46.975975
2648.360924	184.532849	46.980980
2644.899532	200.562715	46.985985
2641.681338	200.147242	46.990989
2638.180985	198.545914	46.995994
2634.294201	197.401269	47.000999
2630.749810	191.553428	47.006004
2627.642885	195.390721	47.011009
2623.880916	198.420426	47.016013
2620.204173	189.438091	47.021018
2616.801274	192.035187	47.026023
2613.962156	186.307399	47.031028
2609.918017	195.283044	47.036033
2606.524561	190.654646	47.041037
2603.294218	193.609767	47.046042
2599.248011	189.954184	47.051047
2596.298434	186.425080	47.056052
2592.749057	189.946701	47.061057
2589.198344	185.798627	47.066061
2586.105445	183.348426	47.071066
2582.315514	187.177670	47.076071
2579.279971	182.025900	47.081076
2575.726115	192.739450	47.086081
2572.023384	188.618140	47.091085
2568.327204	181.805647	47.096090
2565.055125	184.234894	47.101095
2561.581919	184.700785	47.106100
2558.191171	184.578775	47.111105
2554.690225	178.542263	47.116109
2550.793430	188.543392	47.121114
2547.536886	192.745328	47.126119
2544.784805	179.111658	47.131124
2540.680625	191.227071	47.136129
2537.229581	177.333020	47.141133
2533.466355	183.148029	47.146138
2530.104429	187.390121	47.151143
2527.106055	171.552344	47.156148
2523.169333	181.492021	47.161153
2519.923203	186.179477	47.166157
2516.585304	172.270464	47.171162
2512.930849	177.375613	47.176167
2509.248012	171.453725	47.181172
2505.893600	174.195219	47.186177
2502.535655	174.126234	47.191181
2498.977058	165.009616	47.196186
2495.001119	169.477728	47.201191
2492.044386	169.162539	47.206196
2488.403557	175.789880	47.211201
2485.228376	181.101234	47.216205
2481.672396	174.506361	47.221210
2477.950636	182.291472	47.226215
2474.531865	170.852544	47.231220
2470.830986	178.687878	47.236225
2467.520589	173.305835	47.241229
2463.995558	169.196052	47.246234
2460.487196	181.434269	47.251239
2457.387092	160.192364	47.256244
2453.486646	176.685765	47.261249
2450.343220	167.908728	47.266253
2446.594810	169.085709	47.271258
2442.979303	179.012710	47.276263
2439.610697	167.524661	47.281268
2436.197201	173.060812	47.286273
2432.770622	174.895316	47.291277
2429.685449	175.694096	47.296282
2425.777576	168.440628	47.301287
2422.430850	172.563061	47.306292
2418.613656	168.682859	47.311297
2415.251765	174.339933	47.316301
2411.622610	168.698543	47.321306
2408.014473	176.126260	47.326311
2404.778811	168.463901	47.331316
2401.303201	174.573764	47.336321
2397.573458	173.465297	47.341325
2394.483314	168.929331	47.346330
2391.012026	169.549165	47.351335
2387.523081	159.698078	47.356340
2383.769176	165.938304	47.361345
2380.285927	168.607695	47.366349
2376.376815	163.871516	47.371354
2372.614569	174.356074	47.376359
2370.124674	167.010093	47.381364
2366.456553	173.587783	47.386369
2362.732261	174.900755	47.391373
2359.675336	178.118205	47.396378
2355.911840	169.216220	47.401383
2352.188482	171.211240	47.406388
2348.487749	176.353196	47.411393
2345.446312	183.463718	47.416397
2341.635269	166.673385	47.421402
2338.081887	170.280725	47.426407
2335.049841	167.259412	47.431412
2331.644953	167.382849	47.436417
2328.213987	162.647442	47.441421
2324.917280	160.657448	47.446426
2320.900488	172.574839	47.451431
2317.286987	160.999991	47.456436
2313.675257	161.804769	47.461441
2310.294512	162.884464	47.466445
2306.853643	162.960205	47.471450
2303.263753	165.538588	47.476455
2300.133316	154.468457	47.481460
2296.643082	161.890934	47.486465
2292.966174	165.669140	47.491469
2289.471810	159.505291	47.496474
2285.709551	162.728720	47.501479
2282.399583	150.129584	47.506484
2278.366653	160.936105	47.511489
2275.329333	158.454442	47.516493
2272.201268	163.661440	47.521498
2268.128230	173.341911	47.526503
2265.345273	159.738264	47.531508
2261.484063	155.553517	47.536513
2257.761769	154.240492	47.541517
2254.138196	155.552070	47.546522
2251.141255	155.969318	47.551527
2247.836361	151.206590	47.556532
2244.050690	158.192005	47.561537
2240.147508	157.851241	47.566541
2236.750214	152.441567	47.571546
2233.656550	159.035297	47.576551
2230.081059	147.275661	47.581556
2226.273377	156.509240	47.586561
2222.967894	161.109450	47.591565
2219.622218	158.947683	47.596570
2215.578055	160.158667	47.601575
2212.634585	159.806156	47.606580
2208.714063	157.858424	47.611585
2205.830012	159.159225	47.616589
2202.192958	153.352990	47.621594
2198.318573	165.089609	47.626599
2195.032133	163.485982	47.631604
2191.550674	159.336665	47.636609
2187.986694	156.660128	47.641613
2184.706596	146.473310	47.646618
2180.640795	165.491588	47.651623
2177.259438	147.934069	47.656628
2173.827897	150.871723	47.661633
2170.505135	162.473758	47.666637
2167.089803	149.624006	47.671642
2163.349679	153.753000	47.676647
2159.970576	152.586068	47.681652
2156.619216	144.572703	47.686657
2152.773555	157.204249	47.691661
2149.641550	149.814044	47.696666
2145.786495	149.093615	47.701671
2142.593393	154.983800	47.706676
2138.880148	158.306586	47.711681
2135.608631	155.565261	47.716685
2132.157797	153.384681	47.721690
2128.083113	150.846487	47.726695
2124.751751	158.587912	47.731700
2121.448423	152.004802	47.736705
2118.021952	152.044176	47.741709
2114.707571	148.048600	47.746714
2110.918291	154.691359	47.751719
2107.666758	137.050646	47.756724
2103.959359	146.230605	47.761729
2100.425692	157.621945	47.766733
2097.224538	149.741613	47.771738
2093.610358	148.225921	47.776743
2090.043524	152.391189	47.781748
2086.396769	151.234921	47.786753
2083.141656	149.123977	47.791757
2079.560518	145.456400	47.796762
2075.609004	153.905645	47.801767
2072.471059	147.813974	47.806772
2069.032915	153.592470	47.811777
2065.256856	156.457251	47.816781
2062.191730	144.008187	47.821786
2058.053790	152.559772	47.826791
2054.869318	149.454018	47.831796
2051.472746	147.467773	47.836801
2047.976562	153.049686	47.841805
2044.537595	148.423013	47.846810
2040.923337	148.189473	47.851815
2037.683313	136.182244	47.856820
2034.044989	141.919143	47.861825
2030.022245	142.780038	47.866829
2027.083726	146.763096	47.871834
2023.352736	146.669487	47.876839
2020.153581	144.931956	47.881844
2016.747363	147.241563	47.886849
2012.732772	143.375919	47.891853
2009.601529	144.666114	47.896858
2006.313006	148.077685	47.901863
2002.658276	143.863717	47.906868
1999.080328	142.053009	47.911873
1995.309894	142.425951	47.916877
1992.315429	142.062317	47.921882
1988.258557	141.125260	47.926887
1984.787387	136.663230	47.931892
1981.535692	147.670086	47.936897
1977.697566	135.825175	47.941901
1974.544911	143.193131	47.946906
1971.014249	144.199275	47.951911
1967.383880	133.229666	47.956916
1963.830489	137.945543	47.961921
1960.062093	147.786934	47.966925
1957.197823	142.915126	47.971930
1953.234424	141.312590	47.976935
1949.909336	139.842459	47.981940
1946.613018	147.392508	47.986945
1942.962276	134.870109	47.991949
1939.372282	132.852672	47.996954
1935.702369	133.139153	48.001959
1932.677332	138.203802	48.006964
1928.700892	136.898075	48.011969
1925.117674	137.643802	48.016973
1921.939317	139.688983	48.021978
1918.271560	140.286715	48.026983
1915.075376	131.409182	48.031988
1911.582681	140.292832	48.036993
1907.960922	130.353133	48.041997
1904.578627	128.972048	48.047002
1900.676853	143.246429	48.052007
1897.504381	138.431668	48.057012
1894.060377	144.542200	48.062017
1890.251375	138.925987	48.067021
1887.176548	131.693087	48.072026
1883.228868	140.072791	48.077031
1879.848066	140.068682	48.082036
1876.447940	138.590131	48.087041
1872.808843	135.295647	48.092045
1869.474152	130.395120	48.097050
1865.975255	144.312674	48.102055
1862.491443	145.635762	48.107060
1858.729290	131.203953	48.112065
1855.122506	144.560020	48.117069
1852.045849	134.750250	48.122074
1848.551191	141.098516	48.127079
1845.170461	125.794233	48.132084
1841.227442	139.739237	48.137089
1838.009674	133.526613	48.142093
1834.398663	127.946711	48.147098
1830.811832	138.086078	48.152103
1827.270003	130.294822	48.157108
1824.020767	134.525077	48.162113
1820.078833	138.247365	48.167117
1816.801613	134.605236	48.172122
1813.599459	142.839324	48.177127
1810.078025	132.146242	48.182132
1806.348081	136.745684	48.187137
1802.710470	134.010662	48.192141
1799.569930	129.878208	48.197146
1795.733741	142.318031	48.202151
1792.415946	136.170373	48.207156
1789.084469	141.534758	48.212161
1785.332860	138.342676	48.217165
1782.055253	122.776473	48.222170
1778.471299	128.427212	48.227175
1774.842304	132.345519	48.232180
1771.228945	137.307509	48.237185
1767.342504	137.550903	48.242189
1764.417261	125.128264	48.247194
1760.533558	137.684128	48.252199
1757.155812	130.465046	48.257204
1754.069737	136.074911	48.262209
1750.059427	137.505896	48.267213
1746.999055	127.284448	48.272218
1743.176428	138.004065	48.277223
1740.088243	133.713596	48.282228
1736.383616	138.356263	48.287233
1732.893672	133.438770	48.292237
1729.476434	133.897066	48.297242
1725.695058	144.197038	48.302247
1722.326512	135.627280	48.307252
1718.862457	132.545263	48.312257
1715.136431	134.816766	48.317261
1711.707693	123.031761	48.322266
1707.781700	131.962136	48.327271
1705.062594	129.825595	48.332276
1701.361672	133.244990	48.337281
1697.964418	128.938111	48.342285
1694.344195	126.200112	48.347290
1690.797632	124.755274	48.352295
1687.493834	132.864810	48.357300
1683.709637	130.842900	48.362305
1680.157015	133.657760	48.367309
1677.204264	131.986810	48.372314
1673.354281	128.829105	48.377319
1669.588037	124.301437	48.382324
1666.509688	120.347832	48.387329
1662.662603	128.811688	48.392333
1659.407510	122.987846	48.397338
1655.185606	126.166870	48.402343
1652.067057	137.945550	48.407348
1648.669729	127.144241	48.412353
1644.894682	125.500722	48.417357
1641.820438	112.583519	48.422362
1638.157865	124.536066	48.427367
1635.056809	118.028400	48.432372
1631.603401	125.274575	48.437377
1628.065882	122.344930	48.442381
1624.319200	125.329160	48.447386
1620.314383	125.983047	48.452391
1616.976312	122.462280	48.457396
1613.514892	125.622604	48.462401
1609.967542	125.646140	48.467405
1606.786066	125.603488	48.472410
1603.398544	126.044531	48.477415
1599.512311	123.672975	48.482420
1596.477699	120.892630	48.487425
1592.800082	122.812064	48.492429
1589.166791	119.925765	48.497434
1585.674778	128.542356	48.502439
1582.368148	121.514309	48.507444
1578.959644	119.983139	48.512449
1575.251513	122.142871	48.517453
1571.765440	122.409263	48.522458
1568.241799	129.300291	48.527463
1564.855323	125.070087	48.532468
1561.219556	118.741330	48.537473
1557.610296	125.494220	48.542477
1554.016303	125.247298	48.547482
1550.209164	124.280130	48.552487
1546.718987	122.727208	48.557492
1543.745214	123.541327	48.562497
1540.045666	127.804438	48.567501
1536.803619	121.840407	48.572506
1532.972972	128.228849	48.577511
1529.607834	118.273033	48.582516
1526.059447	127.287372	48.587521
1522.271685	127.883063	48.592525
1519.281387	130.204616	48.597530
1515.471040	128.375070	48.602535
1512.408168	131.530956	48.607540
1509.027246	123.058177	48.612545
1505.064843	127.082524	48.617549
1501.880628	123.704866	48.622554
1497.785078	123.362386	48.627559
1494.333117	129.028967	48.632564
1491.166489	138.646231	48.637569
1487.369294	127.854361	48.642573
1483.957883	128.955801	48.647578
1480.593933	141.855107	48.652583
1477.229808	131.455358	48.657588
1473.686309	128.276034	48.662593
1469.965942	143.180371	48.667597
1466.785200	129.935441	48.672602
1463.108014	141.263237	48.677607
1459.539597	130.803653	48.682612
1456.129040	131.496493	48.687617
1452.444149	123.451878	48.692621
1449.322832	126.120220	48.697626
1445.300986	131.058274	48.702631
1441.925284	135.265397	48.707636
1438.534603	126.546646	48.712641
1434.998846	125.993383	48.717645
1431.971555	118.032326	48.722650
1428.177281	126.523345	48.727655
1424.615768	121.705432	48.732660
1421.098377	127.367926	48.737665
1417.559980	131.258097	48.742669
1414.178123	121.293322	48.747674
1410.402542	129.707060	48.752679
1406.793837	125.259098	48.757684
1403.419389	125.292818	48.762689
1399.755835	129.925020	48.767693
1396.290952	121.920932	48.772698
1393.117791	132.000317	48.777703
1389.730126	131.377933	48.782708
1386.443693	123.126005	48.787713
1383.030777	120.582625	48.792717
1379.078124	123.474947	48.797722
1375.461160	127.115139	48.802727
1371.266579	127.929018	48.807732
1368.221552	124.999818	48.812737
1365.039769	127.827241	48.817741
1362.010448	120.803718	48.822746
1358.153894	124.188454	48.827751
1354.629934	129.002767	48.832756
1351.137118	115.363947	48.837761
1347.196159	130.315417	48.842765
1343.918419	125.522733	48.847770
1340.124649	130.137317	48.852775
1336.885017	128.588608	48.857780
1333.620543	121.914917	48.862785
1329.724741	130.461345	48.867789
1326.682981	118.434143	48.872794
1323.018036	128.769989	48.877799
1319.343102	120.748724	48.882804
1316.041113	120.513571	48.887809
1312.488004	122.281379	48.892813
1308.730923	115.573395	48.897818
1305.494780	124.880066	48.902823
1302.081404	122.975407	48.907828
1298.367027	128.750009	48.912833
1294.488060	124.614968	48.917837
1291.367544	118.685460	48.922842
1287.828059	132.951938	48.927847
1284.747489	117.638104	48.932852
1281.813906	123.571695	48.937857
1277.399576	127.598809	48.942861
1273.809715	122.482835	48.947866
1269.933520	116.328045	48.952871
1266.473681	117.622607	48.957876
1263.516935	118.842985	48.962881
1259.671975	121.400837	48.967885
1256.725770	121.448691	48.972890
1252.821722	124.548759	48.977895
1249.164136	120.497216	48.982900
1245.985216	123.020757	48.987905
1242.553988	124.347297	48.992909
1239.127454	124.044663	48.997914
1235.599348	118.951042	49.002919
1231.918914	119.358906	49.007924
1228.336396	121.230138	49.012929
1224.521052	128.123073	49.017933
1221.303173	119.395402	49.022938
1217.812037	120.695396	49.027943
1214.244161	116.562504	49.032948
1210.994499	123.090264	49.037953
1207.170326	128.580650	49.042957
1204.014432	120.096877	49.047962
1199.971267	123.957513	49.052967
1196.822362	120.505387	49.057972
1193.465411	117.265185	49.062977
1190.233929	117.151641	49.067981
1186.696697	107.520716	49.072986
1183.108647	110.244596	49.077991
1179.232047	120.812019	49.082996
1175.837728	108.663293	49.088001
1171.814212	117.949933	49.093005
1168.651152	114.857157	49.098010
1165.413699	119.015712	49.103015
1161.959238	115.177616	49.108020
1158.421756	114.337178	49.113025
1154.541440	119.787790	49.118029
1151.781895	105.293833	49.123034
1147.874729	111.647954	49.128039
1144.106460	113.618754	49.133044
1140.656610	104.552157	49.138049
1137.151879	115.132108	49.143053
1134.138104	111.026149	49.148058
1130.118279	111.259938	49.153063
1126.508892	115.770515	49.158068
1123.305568	107.939775	49.163073
1119.668346	108.097460	49.168077
1116.435885	109.587277	49.173082
1112.509040	118.197457	49.178087
1108.978479	107.730782	49.183092
1106.077600	104.663032	49.188097
1102.236553	117.240973	49.193101
1098.619864	100.598060	49.198106
1094.832913	106.776388	49.203111
1091.754187	105.987760	49.208116
1088.809545	107.993225	49.213121
1085.375129	111.549704	49.218125
1081.077183	118.248160	49.223130
1077.364540	110.199071	49.228135
1073.921383	105.983264	49.233140
1070.696706	106.427144	49.238145
1067.021346	116.081557	49.243149
1064.004328	105.064201	49.248154
1060.028137	113.142910	49.253159
1056.581883	109.478191	49.258164
1053.498654	114.761101	49.263169
1049.961909	108.239023	49.268173
1046.306938	105.478401	49.273178
1042.797924	114.634589	49.278183
1038.796468	115.484854	49.283188
1035.711478	99.506799	49.288193
1032.183309	114.568013	49.293197
1028.638476	101.528201	49.298202
1025.015644	113.833192	49.303207
1021.543942	112.526717	49.308212
1018.598829	107.397534	49.313217
1014.765212	105.830857	49.318221
1011.311291	105.821669	49.323226
1007.405970	103.671348	49.328231
1003.620481	119.600145	49.333236
1000.763046	107.114447	49.338241
997.023636	106.729767	49.343245
993.738891	96.806332	49.348250
990.741565	111.471634	49.353255
986.904843	116.657647	49.358260
983.023487	106.143158	49.363265
979.351352	111.283510	49.368269
976.063023	106.329528	49.373274
972.742947	107.686990	49.378279
969.257411	105.964316	49.383284
965.775349	107.908701	49.388289
961.871869	114.458733	49.393293
958.612258	111.099975	49.398298
954.994308	110.495673	49.403303
951.315658	109.388384	49.408308
948.093784	106.595047	49.413313
944.798870	111.227637	49.418317
940.951599	105.361442	49.423322
937.910447	109.337028	49.428327
933.968283	110.942225	49.433332
930.336297	104.941641	49.438337
927.025938	111.181915	49.443341
923.943063	107.027611	49.448346
920.527176	106.010924	49.453351
916.382161	107.541077	49.458356
912.870908	106.701448	49.463361
909.581032	113.208879	49.468365
905.898084	104.021762	49.473370
902.466976	100.617524	49.478375
898.861747	100.305585	49.483380
895.627166	100.588061	49.488385
892.272088	103.399035	49.493389
888.912861	99.439817	49.498394
885.191769	102.193942	49.503399
881.392580	110.961531	49.508404
878.341078	102.677802	49.513409
874.359588	104.798705	49.518413
871.055516	101.356438	49.523418
867.272379	104.712088	49.528423
863.936712	107.324899	49.533428
860.731068	103.395860	49.538433
856.956601	105.822223	49.543437
853.631309	95.260968	49.548442
850.159536	105.156056	49.553447
846.199486	112.330081	49.558452
843.068641	98.516677	49.563457
839.357106	101.423375	49.568461
836.268382	107.680404	49.573466
832.352313	103.856103	49.578471
828.893491	114.012108	49.583476
825.513407	107.271255	49.588481
821.734276	108.141470	49.593485
818.758485	101.853876	49.598490
814.810388	102.422800	49.603495
811.324098	101.655094	49.608500
808.224776	97.628731	49.613505
804.307420	108.577191	49.618509
801.106533	95.741007	49.623514
797.755116	106.503759	49.628519
793.995880	114.536046	49.633524
790.631106	105.026475	49.638529
786.794211	114.093253	49.643533
783.820578	102.237588	49.648538
779.996503	99.801698	49.653543
776.284226	89.202355	49.658548
772.801553	94.387802	49.663553
769.073305	101.969187	49.668557
765.827071	91.185724	49.673562
762.325275	94.887850	49.678567
758.887298	95.286300	49.683572
755.696764	88.872013	49.688577
751.702634	102.700109	49.693581
748.103323	102.326552	49.698586
745.045532	97.507372	49.703591
741.311765	102.655998	49.708596
738.290305	101.147358	49.713601
734.530246	96.191608	49.718605
730.725698	103.478648	49.723610
727.394939	101.504753	49.728615
723.554782	101.606129	49.733620
720.336066	94.813332	49.738625
716.638249	98.857462	49.743629
713.283126	103.605216	49.748634
709.854269	99.831773	49.753639
706.171011	100.102080	49.758644
703.504972	95.375164	49.763649
699.898580	92.828228	49.768653
695.988780	107.085189	49.773658
692.532543	103.339001	49.778663
688.609816	107.794843	49.783668
685.489087	98.997879	49.788673
681.888612	107.599649	49.793677
678.420954	91.146383	49.798682
674.861445	102.145255	49.803687
671.057585	94.675925	49.808692
667.791484	101.087837	49.813697
663.997885	101.535951	49.818701
660.427853	93.526384	49.823706
656.962794	94.453340	49.828711
653.534419	98.533300	49.833716
650.759759	100.555266	49.838721
647.219706	93.349797	49.843725
643.490068	92.556353	49.848730
639.600801	89.325926	49.853735
636.051769	99.755562	49.858740
633.064097	92.127653	49.863745
629.361787	99.561987	49.868749
625.700619	93.628922	49.873754
622.324194	93.608008	49.878759
618.351903	101.426795	49.883764
615.039994	91.313277	49.888769
611.673572	101.597368	49.893773
608.854416	97.271671	49.898778
605.027059	101.671699	49.903783
601.239304	110.090733	49.908788
597.922660	95.480616	49.913793
594.411338	101.793599	49.918797
590.773381	95.286623	49.923802
587.281059	96.890677	49.928807
583.218336	114.056162	49.933812
580.385455	97.288603	49.938817
576.889004	101.305344	49.943821
573.135754	99.049713	49.948826
569.564177	101.521395	49.953831
566.018622	92.053918	49.958836
563.194055	92.260098	49.963841
559.215263	95.024178	49.968845
555.877500	89.952308	49.973850
552.081715	93.285299	49.978855
548.888463	98.549955	49.983860
545.178799	96.495498	49.988865
541.599523	97.105077	49.993869
538.332365	101.950453	49.998874
534.933057	88.615879	50.003879
531.498120	107.597571	50.008884
527.872116	93.802979	50.013889
523.883621	103.864663	50.018893
520.527256	98.407169	50.023898
517.135575	97.901275	50.028903
513.843463	108.290320	50.033908
509.791049	89.571706	50.038913
506.522278	104.021124	50.043917
503.387737	97.954146	50.048922
500.299728	90.289345	50.053927
496.289705	105.933795	50.058932
492.680847	96.098030	50.063937
488.899775	105.340507	50.068941
485.738707	93.548025	50.073946
482.559755	92.458050	50.078951
478.378371	90.411171	50.083956
475.184522	95.297897	50.088961
471.091752	93.671620	50.093965
468.159519	87.523913	50.098970
464.888364	97.823669	50.103975
461.480636	97.220444	50.108980
457.646423	98.741499	50.113985
453.849691	102.801912	50.118989
450.248419	92.749251	50.123994
446.913595	94.920847	50.128999
443.618909	93.012259	50.134004
440.024994	86.859047	50.139009
436.711007	93.278504	50.144013
433.255873	96.081627	50.149018
430.084163	90.456009	50.154023
425.961689	98.838053	50.159028
422.536065	96.931107	50.164033
418.743384	99.874773	50.169037
415.251976	92.125903	50.174042
411.977363	95.919854	50.179047
408.767760	98.721680	50.184052
405.730705	98.981430	50.189057
401.790828	97.907422	50.194061
397.960255	93.223036	50.199066
394.511797	103.413381	50.204071
390.630732	95.829706	50.209076
387.703254	90.650569	50.214081
384.196893	91.486365	50.219085
380.624068	89.182412	50.224090
377.043750	93.385729	50.229095
373.420884	97.399971	50.234100
369.725006	94.776468	50.239105
366.233417	104.654720	50.244109
363.178059	99.572818	50.249114
360.177258	94.267555	50.254119
356.191939	95.519002	50.259124
352.837102	89.062329	50.264129
348.731317	93.531159	50.269133
345.401987	99.817280	50.274138
341.527441	100.363231	50.279143
338.106088	102.231397	50.284148
335.102426	94.735066	50.289153
331.376908	95.271266	50.294157
328.272549	98.074222	50.299162
324.670316	98.778200	50.304167
320.578902	103.125487	50.309172
317.940005	94.818117	50.314177
314.115534	100.374509	50.319181
310.259360	101.820824	50.324186
307.333540	90.950044	50.329191
303.576144	95.788657	50.334196
299.983066	99.239768	50.339201
296.123397	90.481684	50.344205
292.944288	94.824827	50.349210
289.422658	94.579307	50.354215
285.897612	98.023272	50.359220
282.195598	96.069239	50.364225
279.105012	93.909825	50.369229
275.551049	94.181765	50.374234
272.177859	96.848481	50.379239
268.345152	105.415789	50.384244
265.067997	94.166333	50.389249
261.363474	103.414650	50.394253
257.824699	98.816904	50.399258
254.776785	100.114967	50.404263
250.983247	94.996771	50.409268
247.446030	95.397379	50.414273
243.857573	95.245096	50.419277
240.477024	94.677619	50.424282
236.812580	96.106753	50.429287
233.251562	113.204185	50.434292
229.885079	97.396447	50.439297
226.258312	93.218083	50.444301
222.824228	87.375185	50.449306
219.382728	96.709083	50.454311
215.638655	96.134547	50.459316
212.803776	90.872290	50.464321
209.374479	92.888311	50.469325
205.256270	88.843334	50.474330
202.235559	85.825233	50.479335
198.305770	94.985533	50.484340
194.777600	96.767191	50.489345
191.379451	88.566164	50.494349
187.876267	93.283712	50.499354
184.590825	93.120797	50.504359
180.708328	94.185442	50.509364
177.347569	84.073973	50.514369
173.792401	95.157588	50.519373
170.307037	95.151044	50.524378
167.009676	89.924438	50.529383
163.436860	95.812111	50.534388
160.071766	87.679623	50.539393
156.066363	96.615537	50.544397
152.601558	97.636253	50.549402
149.558266	92.248252	50.554407
145.596470	99.373127	50.559412
142.294329	89.025216	50.564417
138.732511	97.885455	50.569421
135.232575	90.711736	50.574426
131.874757	86.462924	50.579431
128.097766	92.072185	50.584436
124.575236	88.167075	50.589441
121.408506	94.919884	50.594445
117.946739	98.164838	50.599450
114.734129	92.865786	50.604455
110.689594	90.548147	50.609460
107.391639	89.586020	50.614465
103.908633	96.068771	50.619469
100.019265	94.708853	50.624474
96.629510	93.291161	50.629479
93.202993	92.754942	50.634484
89.998111	96.896917	50.639489
85.809404	95.838756	50.644493
82.468933	97.132304	50.649498
79.575203	86.728221	50.654503
75.811106	100.438194	50.659508
72.594029	98.336488	50.664513
68.993222	94.429840	50.669517
64.852759	94.178859	50.674522
61.473140	95.077957	50.679527
58.141741	94.212600	50.684532
54.850174	81.301078	50.689537
51.297419	89.443376	50.694541
47.706505	99.331100	50.699546
44.396511	91.027560	50.704551
40.671773	93.856118	50.709556
37.117836	84.771450	50.714561
33.586461	94.282844	50.719565
30.404856	93.926394	50.724570
26.793264	86.025833	50.729575
22.941076	94.871687	50.734580
20.123794	94.354246	50.739585
16.627784	91.039591	50.744589
12.666436	102.540930	50.749594
9.237119	92.244680	50.754599
5.329936	102.047279	50.759604
2.128035	97.828121	50.764609