Fri Jun 17 17:42:07 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.061991	101.653846	0.000000
0.132958	115.583536	0.005005
0.156432	108.888583	0.010010
0.183830	96.886754	0.015014
-0.373851	95.975083	0.020019
-0.321873	84.083828	0.025024
-0.028157	79.448305	0.030029
-0.738418	66.130962	0.035034
-1.368518	53.634620	0.040038
-1.327380	56.889505	0.045043
-1.402856	42.088519	0.050048
-1.938672	41.578731	0.055053
-2.765741	30.625117	0.060058
-2.552580	24.168620	0.065062
-2.814285	36.455311	0.070067
-2.770912	17.487309	0.075072
-3.035578	18.617256	0.080077
-3.494202	16.085822	0.085082
-4.314006	1.480223	0.090086
-4.881351	3.422171	0.095091
-4.887557	-5.552876	0.100096
-5.383108	4.136730	0.105101
-5.254779	4.256739	0.110106
-5.027890	2.215786	0.115110
-5.520040	-0.907981	0.120115
-5.234046	-0.880679	0.125120
-5.732349	-9.047955	0.130125
-6.466610	10.842818	0.135130
-6.550857	-11.734211	0.140134
-6.885527	7.999764	0.145139
-7.615435	-5.194470	0.150144
-8.031271	7.272720	0.155149
-8.001470	7.909730	0.160154
-8.119699	-0.529695	0.165158
-8.120779	3.481062	0.170163
-8.274929	-7.037177	0.175168
-8.267007	-7.408634	0.180173
-8.511455	6.837212	0.185178
-8.748667	-4.884943	0.190182
-9.796296	-3.712077	0.195187
-9.763291	5.157978	0.200192
-10.052738	2.352752	0.205197
-10.125406	2.138346	0.210202
-9.784678	-6.393542	0.215206
-10.542318	-0.535927	0.220211
-11.101746	4.126868	0.225216
-11.564132	1.583236	0.230221
-12.023626	-1.191357	0.235226
-11.419363	-10.943723	0.240230
-11.491254	-0.839897	0.245235
-11.827465	-11.318400	0.250240
-12.258349	-0.617378	0.255245
-12.632537	4.309635	0.260250
-12.522312	-1.028642	0.265254
-13.315559	-5.047372	0.270259
-13.912691	-5.173025	0.275264
-14.244829	-1.385674	0.280269
-14.200949	-0.373908	0.285274
-14.111424	-10.104651	0.290278
-14.582626	4.232753	0.295283
-14.678854	-3.694704	0.300288
-14.462780	3.607526	0.305293
-14.808045	-5.591963	0.310298
-15.127455	-2.571182	0.315302
-15.916255	-9.797846	0.320307
-16.218414	-7.373501	0.325312
-16.078239	-2.868630	0.330317
-16.506200	-4.560388	0.335322
-16.134802	-11.060536	0.340326
-17.078887	-4.858178	0.345331
-17.359331	-10.112967	0.350336
-17.543727	-12.777195	0.355341
-17.778355	-5.090445	0.360346
-17.919989	-14.766187	0.365350
-18.191043	-4.879474	0.370355
-18.048318	-12.858879	0.375360
-19.057192	-12.220309	0.380365
-19.409913	-9.151962	0.385370
-19.018933	-17.877884	0.390374
-19.423552	-11.831696	0.395379
-19.340170	-11.937658	0.400384
-19.423292	-4.606026	0.405389
-20.413416	6.580642	0.410394
-20.682605	-4.866052	0.415398
-21.223488	4.628630	0.420403
-20.930543	-4.001087	0.425408
-20.784955	-5.789362	0.430413
-21.238366	4.284348	0.435418
-21.665673	-4.762188	0.440422
-22.336105	2.793754	0.445427
-22.314476	6.231638	0.450432
-22.700620	-0.698081	0.455437
-22.814532	0.937428	0.460442
-22.776050	-2.325448	0.465446
-22.945531	-0.126207	0.470451
-22.818495	-0.301387	0.475456
-23.495098	-2.861899	0.480461
-23.970455	5.360956	0.485466
-24.101455	-5.734569	0.490470
-24.297139	0.097325	0.495475
-25.086446	-3.423011	0.500480
-25.128515	-5.937049	0.505485
-25.648396	1.761599	0.510490
-25.653141	-6.550858	0.515494
-25.897568	3.231585	0.520499
-25.487362	-4.323824	0.525504
-25.514754	-8.646458	0.530509
-26.841060	-1.317945	0.535514
-26.932176	-4.212571	0.540518
-27.604929	-5.557382	0.545523
-27.637067	-7.158647	0.550528
-27.940279	-3.426028	0.555533
-27.651076	0.938437	0.560538
-27.488217	-2.127261	0.565542
-27.694498	0.932928	0.570547
-28.251094	-4.993252	0.575552
-28.537326	-5.280493	0.580557
-28.972191	1.940300	0.585562
-28.959087	-0.218837	0.590566
-29.244953	4.048228	0.595571
-29.684357	2.189854	0.600576
-30.320701	0.917330	0.605581
-30.595098	-2.933873	0.610586
-30.908042	-12.536938	0.615590
-31.037515	6.939745	0.620595
-31.159929	6.145369	0.625600
-30.628372	-5.907027	0.630605
-30.899072	0.283255	0.635610
-31.553518	-1.644748	0.640614
-32.228317	6.840951	0.645619
-32.460517	0.984179	0.650624
-32.239173	-2.286597	0.655629
-32.693403	4.604916	0.660634
-32.659929	-1.926286	0.665638
-33.420897	-4.274654	0.670643
-33.737300	5.734449	0.675648
-34.099788	-5.399161	0.680653
-34.056910	6.379270	0.685658
-34.191046	-7.612924	0.690662
-34.261486	1.582155	0.695667
-34.523527	-4.382330	0.700672
-35.159335	6.008418	0.705677
-35.379130	4.662907	0.710682
-35.231400	-5.814341	0.715686
-35.662927	7.866468	0.720691
-35.774586	0.037281	0.725696
-36.101558	-0.106241	0.730701
-36.807969	0.766608	0.735706
-36.751590	5.172338	0.740710
-37.229849	-0.025299	0.745715
-37.107847	1.345843	0.750720
-37.155506	0.283302	0.755725
-37.553230	2.651509	0.760730
-37.834188	4.930848	0.765734
-38.103199	14.004827	0.770739
-38.233322	11.811678	0.775744
-38.460791	5.501641	0.780749
-39.339961	11.524898	0.785754
-39.578027	2.762238	0.790758
-39.996353	-1.308348	0.795763
-39.859617	4.547027	0.800768
-39.884690	5.649384	0.805773
-40.111780	8.345409	0.810778
-40.198384	6.924282	0.815782
-40.203322	7.204374	0.820787
-40.892777	14.328769	0.825792
-41.327262	-5.149782	0.830797
-41.640981	6.879924	0.835802
-41.299793	-3.401962	0.840806
-41.985922	0.923940	0.845811
-42.743273	-4.287883	0.850816
-42.766549	-3.672045	0.855821
-43.073087	8.013904	0.860826
-43.039243	1.557427	0.865830
-43.261913	8.733480	0.870835
-43.283252	-0.607267	0.875840
-43.245157	10.433948	0.880845
-43.741803	2.482475	0.885850
-44.142407	2.535499	0.890854
-45.056977	7.664028	0.895859
-44.805021	-0.202710	0.900864
-44.621324	3.113909	0.905869
-45.123484	4.480073	0.910874
-45.984847	0.173916	0.915878
-46.465024	7.178078	0.920883
-46.524893	-2.190599	0.925888
-45.918504	4.756673	0.930893
-46.471478	8.117801	0.935898
-46.513435	-4.133286	0.940902
-46.604633	1.411096	0.945907
-46.824297	-6.812552	0.950912
-47.832225	-2.558661	0.955917
-48.422552	-2.914736	0.960922
-48.046096	-5.374420	0.965926
-48.116044	-0.108056	0.970931
-48.517825	3.020743	0.975936
-48.238313	-0.645285	0.980941
-48.922943	-0.462958	0.985946
-49.128527	-1.609752	0.990950
-49.551564	-2.016525	0.995955
-49.723581	-6.786144	1.000960
-49.622760	-0.464433	1.005965
-50.330117	8.310440	1.010970
-50.969880	-11.600465	1.015974
-51.312117	-3.888723	1.020979
-50.993825	-1.212910	1.025984
-51.235405	0.480919	1.030989
-51.214483	-2.356752	1.035994
-51.208200	-4.716031	1.040998
-52.249472	6.055871	1.046003
-52.801347	-3.706189	1.051008
-53.065671	1.493229	1.056013
-52.894037	0.412983	1.061018
-52.926223	-3.660614	1.066022
-52.805777	-2.821808	1.071027
-53.001128	5.746598	1.076032
-53.485944	-3.487899	1.081037
-54.402839	-0.186650	1.086042
-54.622440	-5.617109	1.091046
-54.690228	-0.429247	1.096051
-54.517748	3.590348	1.101056
-54.606438	-6.467543	1.106061
-55.266840	-0.825782	1.111066
-55.702995	-0.801380	1.116070
-56.090190	5.467863	1.121075
-56.583609	3.537566	1.126080
-56.253498	2.332903	1.131085
-56.135311	-1.068328	1.136090
-56.257806	-0.435800	1.141094
-57.391028	0.023359	1.146099
-57.515745	5.300013	1.151104
-57.780399	-3.669166	1.156109
-57.976023	6.916584	1.161114
-57.542435	-1.077234	1.166118
-57.888664	6.638531	1.171123
-58.348027	10.242799	1.176128
-59.059662	0.024034	1.181133
-59.784945	-1.959280	1.186138
-59.746782	-1.877762	1.191142
-59.719704	-0.321140	1.196147
-59.843071	-6.661102	1.201152
-59.582544	-1.696533	1.206157
-59.634231	-0.475893	1.211162
-60.192590	1.219091	1.216166
-60.920814	-4.597254	1.221171
-60.708808	-1.116626	1.226176
-60.889971	-2.222093	1.231181
-62.115988	-5.686400	1.236186
-62.205166	-8.933775	1.241190
-62.305573	-0.911577	1.246195
-62.530725	-3.022229	1.251200
-62.555957	-8.693770	1.256205
-63.039966	-9.535581	1.261210
-62.618970	-9.957942	1.266214
-62.801254	-2.022773	1.271219
-63.560913	-9.339513	1.276224
-63.310080	-12.035830	1.281229
-64.204959	-7.863677	1.286234
-63.978465	-13.574297	1.291238
-64.354390	-6.800192	1.296243
-65.004923	-5.522235	1.301248
-65.351656	-5.955503	1.306253
-65.795820	-2.053823	1.311258
-65.713137	-9.434810	1.316262
-65.714308	-10.073123	1.321267
-65.885397	2.604973	1.326272
-65.678426	-13.101678	1.331277
-66.458152	0.113095	1.336282
-66.757313	-13.675440	1.341286
-67.132954	-0.299923	1.346291
-67.217002	-4.296228	1.351296
-67.451325	-11.010429	1.356301
-67.885768	-0.766423	1.361306
-68.615728	-2.624245	1.366310
-68.611430	-7.721533	1.371315
-69.051103	-0.718976	1.376320
-68.723295	-4.851427	1.381325
-69.217458	4.930892	1.386330
-68.700118	-1.395403	1.391334
-69.028762	-10.397746	1.396339
-69.395889	0.616495	1.401344
-69.829485	-9.244348	1.406349
-70.658575	-5.134237	1.411354
-70.816714	-9.198537	1.416358
-70.501766	-5.979318	1.421363
-71.404357	-8.571515	1.426368
-72.077738	-0.078355	1.431373
-72.040167	-4.849267	1.436378
-71.577652	-4.710420	1.441382
-72.150258	-5.941238	1.446387
-72.343617	-8.015931	1.451392
-71.931241	-11.688849	1.456397
-72.466722	-6.622152	1.461402
-73.118550	-5.886634	1.466406
-73.606712	1.525352	1.471411
-73.641614	-0.660929	1.476416
-73.596060	-7.316479	1.481421
-73.949669	2.376962	1.486426
-74.278482	-13.373031	1.491430
-74.880707	-1.304056	1.496435
-75.473760	-6.002302	1.501440
-75.186317	-10.264989	1.506445
-75.656845	-10.415821	1.511450
-75.653772	-4.401288	1.516454
-75.584754	-8.634178	1.521459
-75.702976	-4.563106	1.526464
-75.822272	-3.011752	1.531469
-76.568089	-6.001580	1.536474
-76.824490	-11.473868	1.541478
-77.011522	-6.213302	1.546483
-77.148552	2.104270	1.551488
-77.300379	-0.662456	1.556493
-78.262048	2.706033	1.561498
-78.339803	3.544438	1.566502
-78.652902	-1.856664	1.571507
-78.623408	-4.284919	1.576512
-78.375390	-2.748647	1.581517
-78.965429	-3.696950	1.586522
-79.230745	-3.633852	1.591526
-79.909447	-3.624774	1.596531
-80.315601	-2.051584	1.601536
-80.412692	-4.144056	1.606541
-80.454879	4.710076	1.611546
-80.428440	-1.384448	1.616550
-80.687085	-4.086254	1.621555
-81.117487	-6.296771	1.626560
-81.185683	-1.111999	1.631565
-81.881384	8.710140	1.636570
-81.917423	-1.322167	1.641574
-82.222209	3.665338	1.646579
-82.384034	1.694723	1.651584
-82.015510	-4.498105	1.656589
-82.473377	3.638965	1.661594
-82.901277	2.750337	1.666598
-83.393898	-3.778653	1.671603
-83.630393	-5.571690	1.676608
-83.359280	-4.898232	1.681613
-84.540679	4.377336	1.686618
-84.724630	-3.633407	1.691622
-85.259983	8.959419	1.696627
-85.329993	2.216716	1.701632
-85.300559	-8.736750	1.706637
-85.221026	3.002228	1.711642
-85.153773	-3.668178	1.716646
-85.058497	-2.381789	1.721651
-86.056590	7.102077	1.726656
-86.448415	-13.968886	1.731661
-86.723951	-10.528179	1.736666
-86.686082	-8.735767	1.741670
-86.614619	-6.149953	1.746675
-87.447667	-3.894866	1.751680
-87.596891	-7.401415	1.756685
-88.355326	0.510937	1.761690
-88.444619	1.927659	1.766694
-88.249274	-4.500802	1.771699
-88.458369	-5.041010	1.776704
-88.331178	-1.696454	1.781709
-89.400443	2.377814	1.786714
-89.628325	-3.836044	1.791718
-89.912822	3.935957	1.796723
-90.198336	-7.809131	1.801728
-89.625576	-6.308295	1.806733
-90.069305	0.221939	1.811738
-90.114791	0.039720	1.816742
-90.840622	-0.907517	1.821747
-91.397500	2.529249	1.826752
-91.348884	-2.071625	1.831757
-91.731399	-2.769481	1.836762
-91.581336	-0.900606	1.841766
-92.383796	1.632368	1.846771
-93.090182	-0.682831	1.851776
-92.822387	-8.725452	1.856781
-92.796423	-6.126352	1.861786
-93.125325	-11.153645	1.866790
-93.098493	-2.849701	1.871795
-93.454379	-9.429437	1.876800
-93.414872	-0.865941	1.881805
-94.439303	6.800559	1.886810
-94.570538	-11.508684	1.891814
-94.886941	-11.538520	1.896819
-94.963186	0.106178	1.901824
-94.779407	-9.868143	1.906829
-95.198985	-1.939900	1.911834
-95.413583	-12.634352	1.916838
-95.874007	-0.568426	1.921843
-95.995321	0.870984	1.926848
-96.319331	-1.028467	1.931853
-96.956457	2.138472	1.936858
-96.631663	-10.273419	1.941862
-97.372161	-9.375555	1.946867
-97.681986	-6.281774	1.951872
-97.926812	-11.373559	1.956877
-97.824358	-3.425737	1.961882
-98.343806	-6.252310	1.966886
-98.299843	-8.592001	1.971891
-98.713246	-2.986758	1.976896
-98.556915	2.138983	1.981901
-99.077796	1.486428	1.986906
-99.282687	-0.937002	1.991910
-99.479657	-0.045035	1.996915
-99.692715	-3.726735	2.006912
-99.967356	-3.279097	2.016909
-99.395136	-6.149951	2.026906
-98.550304	-3.236270	2.036902
-98.375688	-17.380648	2.046899
-97.607399	-9.982176	2.056896
-97.246544	-4.401295	2.066893
-96.562203	-5.258460	2.076890
-95.687459	-0.680379	2.086886
-95.573893	4.518393	2.096883
-95.702755	-1.872217	2.106880
-94.458159	0.146944	2.116877
-94.267073	-1.885634	2.126874
-93.316090	0.293773	2.136870
-92.599307	-3.049032	2.146867
-92.568152	-1.734657	2.156864
-92.688956	-1.168753	2.166861
-91.733359	3.299074	2.176858
-90.936681	-3.195801	2.186854
-90.717606	-9.291169	2.196851
-89.973491	-10.580106	2.206848
-89.850279	-7.849752	2.216845
-89.501511	-0.542364	2.226842
-88.440291	1.109550	2.236838
-87.929750	0.694423	2.246835
-87.166820	-4.479734	2.256832
-86.817674	-0.932987	2.266829
-86.810744	-5.404530	2.276826
-86.644150	-9.614934	2.286822
-85.555033	-1.958793	2.296819
-85.151101	-4.735481	2.306816
-84.124471	-4.308949	2.316813
-83.939637	-0.366001	2.326810
-83.763733	-2.383016	2.336806
-83.315385	-1.839014	2.346803
-82.375467	3.461859	2.356800
-81.976418	-2.447867	2.366797
-81.894554	-4.477107	2.376794
-80.817752	-3.995096	2.386790
-80.490581	-2.277664	2.396787
-80.316552	-8.158083	2.406784
-79.182113	-3.289847	2.416781
-78.967244	3.079949	2.426778
-78.949577	-3.282463	2.436774
-78.212823	-7.717459	2.446771
-77.554612	-7.528228	2.456768
-76.960408	3.376837	2.466765
-76.241963	-1.101153	2.476762
-76.111255	-1.086821	2.486758
-75.718362	-3.397355	2.496755
-75.072231	1.689376	2.506752
-74.614772	-1.950752	2.516749
-74.277064	-3.079660	2.526746
-73.296112	-3.637789	2.536742
-72.430730	-1.305839	2.546739
-72.555395	-2.898669	2.556736
-72.663508	-3.051505	2.566733
-71.469825	-1.915758	2.576730
-71.160921	-6.044113	2.586726
-70.699099	-0.620887	2.596723
-69.987285	-4.277808	2.606720
-69.565576	-2.937665	2.616717
-68.973398	-4.257653	2.626714
-68.334302	0.343604	2.636710
-68.044267	-7.778305	2.646707
-67.641147	-2.230526	2.656704
-66.716829	-0.640215	2.666701
-66.370063	2.425423	2.676698
-66.030086	-1.156844	2.686694
-65.826226	-7.797776	2.696691
-65.204596	-4.833153	2.706688
-64.687832	-7.859765	2.716685
-63.670831	1.594319	2.726682
-63.254431	-3.057914	2.736678
-63.459633	-6.618314	2.746675
-62.644682	-9.281547	2.756672
-61.971767	-5.396022	2.766669
-61.721014	-5.428910	2.776666
-60.556839	-0.370004	2.786662
-60.017151	-9.349030	2.796659
-60.006775	-2.745091	2.806656
-60.166346	-3.230598	2.816653
-59.088601	-5.564875	2.826650
-58.673746	-6.260860	2.836646
-57.549249	-1.127587	2.846643
-57.212596	-0.605915	2.856640
-57.111737	-2.316847	2.866637
-56.825670	-2.800560	2.876634
-55.801764	-10.446771	2.886630
-55.510185	-8.732707	2.896627
-55.404799	-6.118134	2.906624
-54.027450	-1.547124	2.916621
-53.899615	-2.906102	2.926618
-53.787422	-3.251649	2.936614
-53.054452	-6.579355	2.946611
-52.474729	-6.196681	2.956608
-52.220476	-2.244919	2.966605
-51.126091	0.323610	2.976602
-50.717725	1.500992	2.986598
-50.577268	-4.278613	2.996595
-50.363076	-3.856319	3.006592
-49.360529	-4.647820	3.016589
-49.021805	-0.208438	3.026586
-48.802623	-1.910586	3.036582
-47.952847	-9.617159	3.046579
-47.456406	-6.696727	3.056576
-46.371124	-6.586186	3.066573
-46.530598	-8.516825	3.076570
-46.195121	-3.943338	3.086566
-45.634311	-2.672154	3.096563
-44.767880	-6.825609	3.106560
-44.553464	-5.134677	3.116557
-44.075748	-5.147400	3.126554
-43.397891	-0.006463	3.136550
-43.038776	-8.548257	3.146547
-42.446171	-7.178824	3.156544
-41.518837	-6.432685	3.166541
-41.385938	-7.458985	3.176538
-41.095359	-6.749261	3.186534
-40.743583	-3.523621	3.196531
-40.095155	-11.619548	3.206528
-39.443745	-6.972322	3.216525
-38.778995	-12.304812	3.226522
-38.593400	-4.964367	3.236518
-38.218471	-5.493079	3.246515
-37.442459	-6.180336	3.256512
-37.012562	-2.100889	3.266509
-36.504483	-4.302137	3.276506
-35.308497	-4.029009	3.286502
-35.198395	-5.025045	3.296499
-35.426011	-8.553664	3.306496
-34.929188	-2.001536	3.316493
-34.080310	-10.478132	3.326490
-33.230445	-10.855803	3.336486
-32.555218	-6.458128	3.346483
-31.992456	-6.477081	3.356480
-32.124597	-8.614589	3.366477
-31.997393	-7.394619	3.376474
-30.758147	-14.451665	3.386470
-30.629156	-5.389367	3.396467
-29.530735	-12.876852	3.406464
-28.957606	-13.247051	3.416461
-28.805346	-6.519101	3.426458
-28.968067	-7.072647	3.436454
-28.181902	-8.695560	3.446451
-27.465244	-5.356895	3.456448
-26.856677	-3.478375	3.466445
-25.904851	-7.110178	3.476442
-25.780616	-7.456738	3.486438
-25.583500	-3.486585	3.496435
-25.192956	-4.298261	3.506432
-24.262083	-8.131079	3.516429
-24.099314	-7.092275	3.526426
-23.382520	-8.407086	3.536422
-22.536715	-5.109250	3.546419
-22.150176	-8.790535	3.556416
-22.400345	-7.580944	3.566413
-21.674262	-7.297674	3.576410
-20.687886	-2.505771	3.586406
-20.601340	-4.233489	3.596403
-19.333956	-10.647338	3.606400
-19.329577	-2.622574	3.616397
-19.328627	-10.179161	3.626394
-18.381617	-9.326628	3.636390
-17.781402	-10.725198	3.646387
-17.602844	-11.544315	3.656384
-16.771918	-9.309762	3.666381
-16.219200	-9.053788	3.676378
-16.180858	-1.666536	3.686374
-15.430879	-3.349623	3.696371
-14.956677	-10.698180	3.706368
-14.812278	-4.504961	3.716365
-13.470603	-4.831599	3.726362
-13.101698	-2.540205	3.736358
-13.006190	-8.251286	3.746355
-12.887497	1.411997	3.756352
-11.899125	-0.256379	3.766349
-11.499690	-0.427191	3.776346
-10.398833	-2.147260	3.786342
-9.793659	-3.665203	3.796339
-10.282009	-8.551938	3.806336
-9.889456	-4.681644	3.816333
-9.017457	-7.405523	3.826330
-8.384095	-4.956156	3.836326
-7.513478	-1.737322	3.846323
-7.089184	4.553218	3.856320
-7.319160	-2.490200	3.866317
-6.405395	1.847682	3.876314
-5.773383	2.521603	3.886310
-5.376713	2.727249	3.896307
-5.171931	2.150158	3.906304
-4.634454	8.614334	3.916301
-4.105730	17.156757	3.926298
-3.429586	29.292616	3.936294
-3.193490	24.108423	3.946291
-2.828340	40.753447	3.956288
-2.015659	60.193997	3.966285
-1.454029	70.036609	3.976282
-1.425879	69.536492	3.986278
-0.930860	92.400059	3.996275
-0.527214	111.781813	4.006272
0.000000	133.407256	4.011277
0.080892	142.195827	4.016282
0.338965	140.485334	4.021286
0.232976	146.695262	4.026291
0.690592	149.130492	4.031296
0.585753	168.602104	4.036301
0.731459	164.109557	4.041306
0.773639	169.617821	4.046310
0.488608	180.844096	4.051315
0.762577	167.181726	4.056320
0.708326	185.987049	4.061325
0.945749	177.575632	4.066330
0.708691	171.665134	4.071334
0.743049	175.297286	4.076339
1.174804	169.029750	4.081344
0.994226	173.959563	4.086349
1.169658	173.592819	4.091354
0.812851	178.638356	4.096358
0.831648	179.349624	4.101363
1.137598	189.064386	4.106368
1.221333	197.057859	4.111373
1.275047	185.728831	4.116378
0.792918	178.247257	4.121382
0.978355	195.925849	4.126387
1.372501	197.476932	4.131392
1.217616	191.890206	4.136397
1.360042	176.086539	4.141402
1.297086	180.625228	4.146406
1.285758	189.627078	4.151411
1.425696	185.255855	4.156416
1.115228	185.536414	4.161421
1.525151	177.232485	4.166426
1.447387	183.775174	4.171430
1.350026	190.638827	4.176435
1.660257	171.520708	4.181440
1.258849	186.995349	4.186445
1.527179	180.920138	4.191450
1.516559	183.422544	4.196454
1.305684	184.770296	4.201459
1.007352	176.880875	4.206464
1.013603	192.769056	4.211469
1.261355	189.139641	4.216474
1.129256	190.213428	4.221478
1.184611	181.186798	4.226483
1.415752	179.738888	4.231488
0.905482	186.481731	4.236493
1.311497	182.181921	4.241498
1.351750	185.183409	4.246502
1.258604	186.617758	4.251507
1.233952	182.285338	4.256512
1.261826	188.080342	4.261517
1.429471	181.953786	4.266522
1.453937	197.061062	4.271526
1.470143	200.421353	4.276531
1.665198	209.911842	4.281536
1.543628	205.567503	4.286541
1.508438	189.108207	4.291546
1.342327	184.886125	4.296550
1.484631	201.512811	4.301555
1.389988	199.787925	4.306560
1.699763	217.117317	4.311565
1.583451	217.258059	4.316570
1.440305	214.635280	4.321574
1.504363	217.643671	4.326579
1.724116	213.657786	4.331584
1.361288	217.928228	4.336589
1.598807	212.563194	4.341594
1.681006	216.819065	4.346598
1.789328	222.039102	4.351603
1.838228	215.450186	4.356608
1.499014	220.336920	4.361613
1.584222	218.117421	4.366618
1.840689	220.119799	4.371622
1.487367	225.309812	4.376627
2.208189	212.702266	4.381632
1.719534	220.532582	4.386637
1.755828	205.906641	4.391642
1.494798	219.395513	4.396646
1.699264	227.078660	4.401651
1.637199	230.905240	4.406656
1.945391	218.708645	4.411661
1.648715	213.416614	4.416666
1.447850	220.348790	4.421670
1.293685	219.736686	4.426675
1.742326	220.451891	4.431680
1.555253	222.770908	4.436685
2.089916	227.875487	4.441690
1.804420	228.630230	4.446694
1.694915	224.521864	4.451699
2.163098	231.066576	4.456704
2.073679	245.371333	4.461709
2.039665	238.622930	4.466714
1.535365	231.528235	4.471718
1.474775	231.843827	4.476723
2.232933	239.926111	4.481728
1.933617	249.805844	4.486733
2.277554	234.850898	4.491738
2.146419	252.980192	4.496742
2.248194	244.176295	4.501747
1.951227	242.196335	4.506752
1.819286	253.246849	4.511757
2.143116	241.938793	4.516762
2.216087	253.790361	4.521766
2.408996	241.952322	4.526771
2.229465	242.100217	4.531776
1.853640	236.050157	4.536781
1.931663	231.946534	4.541786
2.309918	245.448362	4.546790
2.176747	239.524517	4.551795
2.326485	250.315881	4.556800
2.071624	248.389306	4.561805
2.005666	242.152764	4.566810
1.827903	253.031519	4.571814
1.969446	250.058510	4.576819
2.326363	247.683536	4.581824
1.933074	250.853592	4.586829
2.537779	250.722745	4.591834
2.148288	247.498390	4.596838
2.237964	253.834889	4.601843
2.256416	250.279486	4.606848
2.148317	251.702908	4.611853
2.045463	239.432144	4.616858
1.935270	242.751491	4.621862
2.158219	251.802842	4.626867
2.362525	246.958750	4.631872
2.003754	259.445666	4.636877
2.040721	259.763592	4.641882
2.341223	270.711458	4.646886
2.715872	272.438654	4.651891
3.088967	270.454273	4.656896
2.292814	265.618991	4.661901
2.334609	266.284408	4.666906
2.772783	266.579655	4.671910
2.652515	262.495169	4.676915
2.204808	254.255405	4.681920
2.050541	267.524307	4.686925
2.466676	270.882867	4.691930
2.408019	276.568953	4.696934
2.345443	287.874955	4.701939
2.892641	270.799193	4.706944
2.694940	285.388384	4.711949
2.765655	276.713753	4.716954
2.822161	283.184242	4.721958
2.626964	263.968075	4.726963
2.931191	266.082697	4.731968
2.415167	256.953857	4.736973
2.383432	249.624123	4.741978
2.719521	257.736510	4.746982
2.715334	269.965586	4.751987
2.727869	273.779383	4.756992
2.764055	269.534507	4.761997
2.736693	278.885985	4.767002
2.685533	271.297806	4.772006
2.638387	281.571949	4.777011
2.988793	280.762707	4.782016
2.550075	273.904942	4.787021
2.928190	270.380134	4.792026
2.545915	271.227530	4.797030
2.602500	279.174252	4.802035
2.919148	273.642914	4.807040
2.501543	280.130833	4.812045
2.843243	274.313540	4.817050
2.671412	276.203396	4.822054
2.688985	278.768817	4.827059
2.856682	264.903998	4.832064
2.585238	279.164054	4.837069
2.591374	276.710628	4.842074
2.694439	277.445979	4.847078
2.640603	292.111115	4.852083
2.806766	283.124814	4.857088
2.358858	286.361182	4.862093
2.730684	292.684347	4.867098
3.100316	303.928586	4.872102
3.194649	306.082047	4.877107
3.229147	303.437620	4.882112
3.139710	304.359480	4.887117
3.303320	298.922637	4.892122
3.234052	285.567235	4.897126
3.035225	281.427918	4.902131
2.902094	273.846653	4.907136
2.549656	284.718154	4.912141
2.693467	301.297140	4.917146
3.203674	299.085923	4.922150
3.133179	313.131260	4.927155
3.414252	303.078204	4.932160
3.235698	314.833492	4.937165
3.318769	307.553123	4.942170
2.901678	299.213921	4.947174
3.109507	309.784327	4.952179
3.145888	306.202450	4.957184
2.937567	313.254701	4.962189
3.346467	310.977244	4.967194
3.816924	315.040539	4.972198
3.211825	299.756646	4.977203
3.462990	286.491445	4.982208
3.359327	290.771124	4.987213
3.012165	288.218946	4.992218
3.245310	285.974454	4.997222
3.209978	282.818309	5.002227
3.610886	282.113943	5.007232
2.847886	294.726287	5.012237
3.051167	301.334201	5.017242
3.493677	305.279595	5.022246
3.382476	314.592933	5.027251
3.915303	308.762014	5.032256
3.347852	306.992566	5.037261
3.097073	287.706083	5.042266
3.376626	303.579934	5.047270
3.440238	306.946774	5.052275
3.671302	304.023798	5.057280
3.631237	308.997195	5.062285
3.579472	307.432903	5.067290
3.510139	289.387483	5.072294
3.066396	289.823395	5.077299
3.329251	296.836988	5.082304
3.298856	307.911117	5.087309
3.561006	309.289186	5.092314
3.457909	320.372448	5.097318
3.446020	318.411004	5.102323
3.518827	312.634837	5.107328
3.842666	319.515563	5.112333
3.719012	312.261067	5.117338
3.751540	310.684541	5.122342
3.327675	316.437855	5.127347
3.772441	317.286713	5.132352
3.490705	318.404323	5.137357
3.542766	323.628221	5.142362
3.608834	316.250034	5.147366
3.312847	323.318242	5.152371
3.797169	309.247429	5.157376
3.699261	322.366115	5.162381
3.496908	315.905941	5.167386
3.304209	316.847136	5.172390
3.413845	325.188020	5.177395
3.480838	315.768854	5.182400
3.298481	319.238147	5.187405
3.522687	329.580490	5.192410
3.647566	335.576296	5.197414
3.642679	353.017933	5.202419
3.791465	343.542531	5.207424
3.593370	352.021206	5.212429
3.843925	352.770921	5.217434
4.070429	346.222681	5.222438
3.697742	353.929990	5.227443
4.060681	339.561420	5.232448
3.277477	355.326226	5.237453
3.502502	349.101661	5.242458
3.857194	352.016780	5.247462
3.694487	354.128906	5.252467
3.794683	350.911938	5.257472
3.534987	357.585777	5.262477
3.801804	359.874561	5.267482
3.858767	370.442458	5.272486
3.677624	381.969516	5.277491
4.157040	374.376177	5.282496
4.238499	382.947525	5.287501
4.340824	377.781914	5.292506
4.362708	375.093987	5.297510
3.885187	361.894781	5.302515
4.145797	340.066620	5.307520
4.204793	358.407749	5.312525
3.952773	356.005112	5.317530
4.252541	351.789417	5.322534
3.932718	355.062131	5.327539
4.293275	353.882579	5.332544
4.289149	351.013288	5.337549
4.202521	350.871843	5.342554
4.339292	360.879656	5.347558
3.990888	356.375445	5.352563
4.133869	348.992155	5.357568
4.145912	361.213869	5.362573
3.965596	356.164114	5.367578
4.112488	356.902445	5.372582
4.164533	369.494229	5.377587
4.501385	371.985877	5.382592
4.171922	363.046585	5.387597
4.633773	362.593751	5.392602
4.576388	354.220583	5.397606
4.182884	358.027296	5.402611
4.366272	350.401278	5.407616
4.062747	351.009246	5.412621
4.412805	353.605454	5.417626
4.501134	345.062241	5.422630
4.189445	353.570849	5.427635
4.462112	351.466595	5.432640
4.293636	365.191022	5.437645
4.027651	354.256001	5.442650
4.301110	355.740926	5.447654
4.563528	366.613494	5.452659
4.654276	372.285242	5.457664
4.191768	360.919540	5.462669
4.064252	366.219870	5.467674
4.579266	370.779570	5.472678
4.467145	383.722871	5.477683
4.639260	378.490604	5.482688
4.464370	389.482050	5.487693
4.704954	374.052982	5.492698
4.595738	384.190299	5.497702
4.355533	383.997616	5.502707
4.527873	384.491761	5.507712
4.305051	380.629122	5.512717
4.477095	381.889171	5.517722
4.580280	380.210712	5.522726
4.456163	382.276172	5.527731
4.583561	372.963161	5.532736
4.313526	381.891103	5.537741
4.485506	380.056761	5.542746
4.428287	381.968231	5.547750
4.006468	392.281042	5.552755
4.291312	389.286556	5.557760
4.522665	401.252415	5.562765
4.513432	416.339063	5.567770
4.697916	407.371943	5.572774
4.781921	416.555415	5.577779
5.232801	408.464781	5.582784
5.151895	410.825971	5.587789
4.496184	389.849990	5.592794
4.584991	403.571549	5.597798
4.663630	412.903319	5.602803
4.814343	412.323019	5.607808
4.748947	414.171521	5.612813
5.027431	413.472895	5.617818
4.712882	413.222910	5.622822
4.771667	412.410431	5.627827
5.015849	415.475158	5.632832
4.830247	420.027790	5.637837
4.729477	418.645287	5.642842
4.659067	406.381035	5.647846
4.989284	407.113960	5.652851
4.844321	413.626080	5.657856
4.599350	410.758526	5.662861
4.846175	417.799506	5.667866
5.060353	407.262190	5.672870
4.745950	422.433706	5.677875
5.134285	404.070149	5.682880
4.718030	417.763779	5.687885
4.997722	419.065534	5.692890
5.355707	414.442515	5.697894
4.597836	419.909204	5.702899
4.711737	417.000550	5.707904
4.812646	417.173467	5.712909
5.135474	436.125199	5.717914
5.335174	436.670447	5.722918
5.036202	427.184759	5.727923
5.178192	426.413112	5.732928
5.065554	422.258445	5.737933
5.263401	443.807563	5.742938
5.407693	425.500528	5.747942
4.931263	422.457137	5.752947
5.008457	419.292522	5.757952
5.235035	433.067577	5.762957
5.212935	443.705300	5.767962
5.377405	446.864584	5.772966
5.185515	443.066250	5.777971
5.202480	435.060354	5.782976
5.285781	442.756840	5.787981
5.109395	452.181737	5.792986
5.342523	445.498166	5.797990
5.181699	451.139334	5.802995
5.543409	452.046997	5.808000
5.359111	446.641486	5.813005
5.081517	451.377744	5.818010
5.326168	447.027129	5.823014
4.950915	451.594322	5.828019
5.260596	441.619894	5.833024
5.117761	449.696741	5.838029
5.076087	444.973985	5.843034
5.079819	447.440501	5.848038
4.473904	443.921737	5.853043
5.160394	461.002701	5.858048
5.452588	470.180412	5.863053
5.375953	477.244989	5.868058
5.823642	467.286679	5.873062
5.465354	479.988787	5.878067
5.387382	476.947632	5.883072
5.734107	481.085410	5.888077
5.595752	481.734800	5.893082
6.287377	473.483547	5.898086
5.326500	466.625656	5.903091
5.400916	448.196415	5.908096
5.199699	461.403232	5.913101
5.661517	467.390447	5.918106
5.797429	479.021170	5.923110
5.515097	481.037360	5.928115
5.702726	469.222324	5.933120
5.772778	478.794929	5.938125
5.689113	465.861694	5.943130
5.579664	471.241544	5.948134
5.540844	477.520953	5.953139
5.986074	473.843257	5.958144
5.774606	469.057546	5.963149
5.735382	449.130273	5.968154
5.576815	448.158360	5.973158
5.369503	470.918415	5.978163
5.363313	474.050224	5.983168
5.520641	481.327519	5.988173
5.562108	486.959942	5.993178
6.233523	477.722012	5.998182
5.592220	477.371427	6.003187
5.750056	473.662170	6.008192
5.593648	480.594177	6.013197
5.613933	476.816020	6.018202
5.881737	478.572839	6.023206
5.668985	480.522013	6.028211
5.626021	470.730304	6.033216
5.895303	473.121113	6.038221
5.807266	477.986110	6.043226
5.622469	473.337059	6.048230
5.749789	481.703307	6.053235
5.791009	472.385221	6.058240
5.922270	476.056789	6.063245
5.711824	485.047703	6.068250
5.690867	484.056072	6.073254
5.377496	484.893012	6.078259
5.700953	477.990961	6.083264
5.866623	497.850586	6.088269
5.811652	503.059576	6.093274
6.346676	494.549782	6.098278
6.048101	491.483327	6.103283
5.922205	473.894453	6.108288
5.884672	478.542472	6.113293
5.618493	481.305656	6.118298
6.223669	472.180958	6.123302
5.730973	481.327712	6.128307
6.056417	473.013000	6.133312
5.719529	485.215651	6.138317
5.787616	485.314300	6.143322
5.615253	478.746656	6.148326
5.881145	479.889685	6.153331
5.731999	476.774124	6.158336
5.662118	483.502703	6.163341
5.803271	483.042785	6.168346
6.221554	481.563941	6.173350
5.788604	482.875615	6.178355
5.722113	476.484159	6.183360
5.936951	476.442383	6.188365
5.964636	484.120112	6.193370
5.900162	480.739664	6.198374
5.706656	479.707645	6.203379
6.086792	461.318743	6.208384
5.595835	474.535447	6.213389
5.858058	472.616238	6.218394
6.000793	464.332293	6.223398
5.780368	480.779610	6.228403
5.774697	469.397097	6.233408
6.138719	477.338998	6.238413
5.610975	472.544483	6.243418
5.641178	474.171874	6.248422
5.675481	483.316286	6.253427
5.962529	473.155959	6.258432
5.552571	476.666472	6.263437
5.895010	480.593024	6.268442
6.000532	469.947431	6.273446
5.613975	469.928850	6.278451
5.923074	474.885114	6.283456
6.136632	478.059926	6.288461
5.511582	473.835110	6.293466
5.742067	478.498966	6.298470
5.850120	476.149733	6.303475
5.841998	486.360101	6.308480
5.949579	476.424965	6.313485
5.860454	478.788518	6.318490
5.853833	476.508073	6.323494
5.636039	478.753299	6.328499
5.926262	476.872257	6.333504
6.050096	484.134203	6.338509
6.009250	479.434585	6.343514
6.131792	481.631926	6.348518
6.039284	484.012224	6.353523
6.137728	473.554090	6.358528
6.125644	475.081158	6.363533
5.847968	466.212133	6.368538
5.988972	450.971815	6.373542
5.986797	448.339378	6.378547
5.868644	442.325145	6.383552
5.381702	452.651188	6.388557
5.607582	455.033422	6.393562
5.714890	462.434068	6.398566
5.737735	474.252499	6.403571
6.075001	465.903661	6.408576
5.805755	468.525468	6.413581
5.769008	475.814297	6.418586
6.065181	473.537201	6.423590
5.677838	468.962271	6.428595
5.871819	469.872160	6.433600
6.045611	475.191120	6.438605
5.977768	459.994977	6.443610
5.963314	441.806661	6.448614
5.561923	451.492931	6.453619
5.695700	444.328194	6.458624
5.675434	443.566544	6.463629
5.795530	459.685312	6.468634
5.930870	465.478148	6.473638
5.775633	470.955396	6.478643
5.707154	465.661263	6.483648
6.108976	471.243850	6.488653
5.573939	465.047690	6.493658
5.718503	462.610694	6.498662
5.663069	476.821214	6.503667
6.017467	477.954070	6.508672
5.951074	473.012030	6.513677
5.570752	479.829503	6.518682
6.077879	476.232095	6.523686
5.970422	474.443990	6.528691
5.727441	457.383722	6.533696
5.512837	457.031085	6.538701
5.560550	471.716612	6.543706
5.793690	484.810011	6.548710
5.739301	477.962079	6.553715
5.786775	478.643335	6.558720
5.893461	471.662072	6.563725
5.839485	480.789975	6.568730
6.017937	477.770729	6.573734
5.680509	485.365681	6.578739
5.829673	476.278689	6.583744
5.885891	483.187197	6.588749
5.940812	479.928591	6.593754
6.097213	479.351684	6.598758
5.658959	477.206721	6.603763
5.926085	480.948258	6.608768
5.939215	482.585394	6.613773
5.702055	479.053875	6.618778
5.875286	467.024362	6.623782
5.702654	482.893832	6.628787
5.726209	484.057406	6.633792
5.890409	484.116005	6.638797
5.792419	482.031308	6.643802
5.971352	484.350309	6.648806
5.980139	484.584912	6.653811
5.753716	471.809391	6.658816
5.881774	461.816396	6.663821
5.617268	473.220427	6.668826
5.936482	467.320564	6.673830
5.825346	488.347051	6.678835
5.798603	471.538541	6.683840
5.773056	464.411524	6.688845
5.800112	474.319245	6.693850
5.946046	468.530076	6.698854
5.457240	480.722650	6.703859
5.929408	478.692571	6.708864
6.138780	478.950668	6.713869
5.773315	475.707273	6.718874
5.872195	453.415061	6.723878
5.555570	457.584944	6.728883
5.928299	469.574323	6.733888
5.908734	475.093157	6.738893
5.735782	479.314350	6.743898
5.993752	470.110017	6.748902
5.730154	453.000689	6.753907
6.017974	461.783465	6.758912
5.848638	449.032613	6.763917
5.746267	451.033096	6.768922
5.844472	449.237253	6.773926
5.719514	446.191087	6.778931
5.651710	454.559954	6.783936
6.245283	463.972917	6.788941
5.684003	467.527128	6.793946
6.004085	452.331242	6.798950
5.580306	455.392939	6.803955
5.788341	448.416942	6.808960
5.902484	442.587286	6.813965
5.675749	448.482723	6.818970
5.730086	441.638836	6.823974
5.811068	465.620030	6.828979
5.871004	463.063503	6.833984
6.157319	456.887909	6.838989
5.815823	452.127367	6.843994
6.098534	445.665056	6.848998
5.684627	453.244091	6.854003
5.917590	444.255276	6.859008
5.950186	443.855040	6.864013
5.554898	449.402964	6.869018
5.940000	445.836896	6.874022
5.570275	444.260713	6.879027
5.715540	447.466406	6.884032
5.460463	444.583159	6.889037
5.566190	467.468386	6.894042
6.260168	475.125746	6.899046
5.984834	472.922920	6.904051
6.132159	458.004188	6.909056
5.642499	455.207684	6.914061
5.510966	453.502715	6.919066
6.023346	449.608437	6.924070
5.720512	448.526906	6.929075
5.602056	448.718327	6.934080
5.967681	460.615146	6.939085
5.723925	471.867725	6.944090
5.677739	467.276743	6.949094
5.659681	480.729010	6.954099
5.897525	477.436251	6.959104
6.180559	474.954333	6.964109
5.914972	475.862857	6.969114
5.942404	445.291672	6.974118
5.559082	445.481335	6.979123
6.025518	449.580658	6.984128
6.113232	436.543580	6.989133
5.701828	451.184826	6.994138
5.644385	438.429198	6.999142
5.511940	442.255491	7.004147
5.928283	448.822924	7.009152
5.746860	447.682338	7.014157
5.706862	462.769015	7.019162
6.015861	469.792975	7.024166
5.819680	469.622180	7.029171
5.815463	463.698720	7.034176
6.071663	452.068649	7.039181
5.556826	442.084644	7.044186
5.774114	450.460983	7.049190
5.986818	466.103982	7.054195
5.719813	454.474439	7.059200
6.003536	451.906372	7.064205
5.685125	450.161422	7.069210
5.557272	454.054443	7.074214
6.020811	465.417381	7.079219
5.676277	470.688697	7.084224
6.041941	486.997363	7.089229
5.784341	475.486221	7.094234
5.712739	459.917936	7.099238
5.642195	465.416626	7.104243
5.782938	472.920057	7.109248
5.771368	477.818718	7.114253
5.823006	476.021535	7.119258
6.080450	484.217562	7.124262
5.760904	488.343144	7.129267
5.900866	476.916094	7.134272
5.911407	469.703550	7.139277
5.544722	468.630065	7.144282
6.275620	466.960929	7.149286
5.855280	467.045447	7.154291
5.548362	456.827368	7.159296
5.751912	455.050325	7.164301
5.938173	478.829927	7.169306
6.247389	468.286837	7.174310
5.870596	458.900103	7.179315
5.588789	451.500540	7.184320
6.081378	451.732480	7.189325
5.930705	449.336269	7.194330
5.658107	457.675043	7.199334
5.604677	453.205446	7.204339
5.841103	451.741241	7.209344
5.952810	452.156468	7.214349
5.678822	458.132382	7.219354
6.052330	452.978308	7.224358
5.607181	449.467157	7.229363
5.735295	459.504100	7.234368
5.831899	439.383568	7.239373
5.222705	461.581302	7.244378
6.014683	465.378273	7.249382
5.861214	476.476136	7.254387
5.925416	474.800200	7.259392
6.228723	470.015755	7.264397
5.820124	468.593440	7.269402
5.994782	448.336392	7.274406
5.463799	451.003475	7.279411
5.745208	451.620588	7.284416
6.082981	447.294160	7.289421
6.047156	450.629804	7.294426
5.966710	446.229032	7.299430
6.108231	459.577006	7.304435
6.094800	448.778727	7.309440
6.005129	453.564461	7.314445
5.565181	453.667433	7.319450
6.205687	448.478652	7.324454
5.792222	454.429203	7.329459
5.690219	456.829624	7.334464
5.511088	442.638673	7.339469
5.618139	460.643570	7.344474
6.142695	439.897000	7.349478
5.526544	449.966472	7.354483
5.520572	457.557824	7.359488
5.451170	448.235840	7.364493
5.194429	460.325101	7.369498
5.337587	468.958270	7.374502
5.505120	483.440764	7.379507
5.538660	489.909828	7.384512
5.801627	483.670221	7.389517
5.817042	484.717732	7.394522
5.644470	481.658161	7.399526
5.868598	485.099002	7.404531
5.697548	485.801187	7.409536
6.004512	486.649871	7.414541
5.999210	482.051694	7.419546
5.746335	488.282818	7.424550
6.006788	485.534499	7.429555
6.063869	491.133938	7.434560
6.338430	488.401231	7.439565
6.109890	487.772074	7.444570
6.096994	478.715964	7.449574
5.688037	473.047833	7.454579
5.748733	481.152042	7.459584
6.119045	474.136827	7.464589
5.476026	469.363446	7.469594
5.760883	471.141307	7.474598
5.839673	481.842998	7.479603
5.723801	490.888447	7.484608
5.845622	492.581323	7.489613
5.695277	488.730883	7.494618
5.846203	486.551729	7.499622
5.910884	491.812264	7.504627
6.035557	492.375707	7.509632
5.873831	487.250593	7.514637
5.790444	480.600474	7.519642
6.051171	472.646592	7.524646
5.782402	464.329811	7.529651
5.902347	463.437110	7.534656
6.034750	453.566338	7.539661
5.648301	460.726803	7.544666
5.721139	456.819542	7.549670
5.917669	452.270709	7.554675
5.735596	462.012293	7.559680
5.598452	458.592029	7.564685
5.811002	469.357714	7.569690
5.980693	474.186779	7.574694
5.708526	460.801210	7.579699
5.539247	484.999066	7.584704
5.779659	474.302238	7.589709
5.916122	489.249695	7.594714
5.723258	482.454771	7.599718
5.944341	494.341699	7.604723
5.962240	484.280960	7.609728
6.279460	486.193553	7.614733
5.838600	471.713764	7.619738
6.068757	461.551061	7.624742
5.605633	453.986469	7.629747
5.604548	462.154611	7.634752
5.708744	457.030104	7.639757
5.634661	466.612647	7.644762
5.971031	470.476072	7.649766
5.746353	473.574536	7.654771
5.565385	471.743790	7.659776
5.832873	475.894342	7.664781
5.659123	489.626662	7.669786
5.735590	485.968421	7.674790
5.569434	489.152277	7.679795
5.608978	489.077082	7.684800
6.309940	480.726197	7.689805
5.990131	491.316346	7.694810
6.199294	485.504427	7.699814
5.794921	479.914466	7.704819
5.627894	465.901058	7.709824
5.823139	477.026407	7.714829
5.637553	496.240516	7.719834
5.847497	487.329701	7.724838
5.660192	496.377949	7.729843
5.888422	486.260148	7.734848
5.929466	489.342077	7.739853
5.750958	493.361139	7.744858
5.933694	480.020516	7.749862
5.881594	489.179686	7.754867
6.126725	487.936034	7.759872
5.905931	471.101367	7.764877
5.588631	465.438528	7.769882
5.755069	457.635896	7.774886
5.927883	472.099545	7.779891
5.400670	466.820484	7.784896
6.086871	487.217159	7.789901
6.061277	488.142232	7.794906
5.662112	473.384372	7.799910
5.614070	473.842332	7.804915
5.666400	490.153352	7.809920
6.237619	490.333743	7.814925
5.610658	488.686251	7.819930
5.866426	488.245961	7.824934
5.758642	486.315037	7.829939
5.557767	489.106440	7.834944
6.231971	488.093396	7.839949
5.824492	493.913316	7.844954
5.891879	474.001444	7.849958
5.473454	475.017463	7.854963
5.899568	482.742634	7.859968
5.954912	478.524708	7.864973
5.780987	493.798648	7.869978
5.595865	488.363658	7.874982
6.114739	489.317031	7.879987
5.830485	490.095062	7.884992
5.755668	484.507749	7.889997
5.493566	495.460485	7.895002
5.791519	494.956350	7.900006
5.591564	492.201870	7.905011
5.254951	494.092896	7.910016
5.604630	486.092847	7.915021
5.485149	486.879011	7.920026
5.533061	492.005974	7.925030
5.580905	493.723183	7.930035
5.832658	487.552926	7.935040
5.681083	481.733478	7.940045
5.870183	497.380826	7.945050
5.621969	492.720012	7.950054
5.594773	503.415456	7.955059
5.798241	509.744592	7.960064
6.177747	512.743826	7.965069
5.734027	506.109976	7.970074
5.750572	505.764109	7.975078
6.087782	499.416249	7.980083
5.877415	498.071689	7.985088
6.337266	485.012777	7.990093
6.047735	486.441512	7.995098
5.948978	489.031236	8.000102
6.048404	483.789702	8.005107
6.004750	492.603515	8.010112
6.425196	492.111795	8.015130
6.011544	490.695301	8.020147
6.156884	490.991047	8.025165
5.981851	467.499909	8.030182
5.666266	458.253473	8.035200
5.990588	450.403102	8.040218
5.644197	463.630758	8.045235
5.644873	478.987546	8.050253
6.190090	467.319697	8.055270
5.831643	480.342303	8.060288
5.835602	469.707242	8.065306
5.916646	470.294947	8.070323
5.716173	478.342934	8.075341
6.149492	484.315684	8.080358
5.838774	474.382469	8.085376
6.138457	446.225875	8.090394
5.502031	457.210216	8.095411
5.536184	468.974362	8.100429
5.986003	470.965205	8.105446
5.595280	483.213723	8.110464
6.149076	477.334069	8.115482
6.064045	483.387856	8.120499
5.774696	484.068224	8.125517
5.946510	476.733301	8.130534
5.824341	479.826210	8.135552
6.078384	481.333894	8.140570
6.044380	481.725584	8.145587
6.028098	482.332813	8.150605
5.964622	485.980482	8.155622
5.576814	490.947299	8.160640
5.835040	469.874076	8.165658
5.940686	478.086517	8.170675
5.767647	486.285839	8.175693
5.782701	476.036689	8.180710
5.517309	487.867959	8.185728
6.032419	476.594835	8.190746
5.531992	479.596298	8.195763
5.775712	476.999578	8.200781
5.922979	487.113789	8.205798
5.857817	506.053268	8.210816
6.152816	504.101702	8.215834
6.096495	512.193260	8.220851
6.119789	510.477782	8.225869
6.235504	505.663952	8.230886
6.009633	506.018445	8.235904
6.140012	489.813646	8.240922
5.625526	492.460393	8.245939
5.885755	502.109422	8.250957
5.917288	513.386090	8.255974
6.094340	515.949788	8.260992
5.848914	511.858127	8.266010
5.745661	508.262671	8.271027
5.869116	509.236404	8.276045
6.220877	513.631722	8.281062
5.878083	521.726416	8.286080
6.267530	516.470468	8.291098
6.089753	521.338217	8.296115
6.120210	518.959598	8.301133
6.457241	517.968478	8.306150
6.146959	521.067269	8.311168
6.194181	517.171235	8.316186
5.937625	512.427939	8.321203
5.876873	512.903990	8.326221
6.343974	505.269406	8.331238
6.031702	511.702281	8.336256
6.454225	504.417399	8.341274
6.171114	508.382262	8.346291
6.133553	511.934694	8.351309
6.254074	511.621825	8.356326
6.039799	512.239722	8.361344
6.171174	512.358475	8.366362
6.031059	513.343538	8.371379
5.798594	507.766196	8.376397
6.186319	508.303717	8.381414
6.235981	522.047431	8.386432
6.143324	505.263207	8.391450
6.381656	519.111178	8.396467
5.820540	519.801879	8.401485
5.931956	507.808893	8.406502
5.928608	522.893583	8.411520
6.266294	525.686466	8.416538
5.853286	540.173573	8.421555
6.222470	542.372693	8.426573
6.751957	540.527805	8.431590
6.280903	546.787891	8.436608
6.555268	529.924921	8.441626
6.231576	516.719519	8.446643
6.333902	520.408727	8.451661
6.375087	509.099991	8.456678
6.129826	522.274474	8.461696
6.264429	512.407166	8.466714
5.993846	511.721350	8.471731
6.099404	531.531223	8.476749
6.332104	532.258276	8.481766
6.335250	534.956778	8.486784
6.154925	542.730214	8.491802
6.370082	543.286970	8.496819
6.238075	548.865562	8.501837
5.929273	546.855308	8.506854
5.971417	556.066250	8.511872
6.483794	539.065885	8.516890
6.573107	551.007524	8.521907
5.943631	546.682468	8.526925
6.673034	551.149270	8.531942
6.247752	553.978231	8.536960
6.382656	546.202992	8.541978
6.410230	544.372044	8.546995
6.376693	538.323476	8.552013
6.224250	543.975732	8.557030
6.436557	548.213940	8.562048
6.766876	546.567298	8.567066
6.585269	546.090688	8.572083
6.501999	544.061844	8.577101
6.818166	546.342211	8.582119
6.331728	553.302433	8.587136
6.856885	550.376468	8.592154
6.561920	556.058912	8.597171
6.397419	547.498864	8.602189
6.419765	544.352955	8.607207
6.250543	549.314953	8.612224
6.486727	547.630418	8.617242
6.822028	545.758755	8.622259
6.489867	558.439095	8.627277
6.700983	530.408674	8.632295
6.517492	528.966322	8.637312
6.373884	515.181235	8.642330
6.414947	514.885116	8.647347
6.321235	529.315600	8.652365
6.794796	537.371655	8.657383
6.442629	535.144613	8.662400
6.509684	529.222624	8.667418
6.674235	531.302224	8.672435
6.630606	528.443638	8.677453
6.503081	516.721442	8.682471
6.527397	515.686834	8.687488
6.504872	518.111278	8.692506
6.713069	503.738248	8.697523
6.571360	507.456794	8.702541
6.697849	507.337011	8.707559
6.542460	506.306291	8.712576
6.704866	508.131937	8.717594
6.836018	505.724576	8.722611
6.480818	517.328888	8.727629
6.326922	515.627704	8.732647
6.342430	511.379494	8.737664
6.414768	499.681960	8.742682
6.715528	517.661896	8.747699
6.466229	532.176112	8.752717
6.882750	530.484635	8.757735
6.540141	522.374835	8.762752
6.301188	523.123791	8.767770
6.584236	545.967295	8.772787
6.496988	549.648456	8.777805
6.648414	542.316497	8.782823
6.767254	555.059263	8.787840
6.839605	542.706043	8.792858
7.001191	543.864565	8.797875
6.737200	534.462671	8.802893
6.639007	515.555723	8.807911
6.663025	527.392459	8.812928
6.300084	521.746452	8.817946
6.427984	528.405162	8.822963
6.287321	541.367411	8.827981
6.482095	545.421540	8.832999
6.311898	545.171557	8.838016
6.216694	551.672888	8.843034
6.420682	543.676935	8.848051
6.079833	553.599902	8.853069
6.599035	566.064340	8.858087
6.661922	578.878034	8.863104
6.538072	581.012662	8.868122
6.713400	580.138762	8.873139
6.694617	580.714720	8.878157
6.657655	567.118143	8.883175
6.948104	571.106185	8.888192
6.743669	577.831373	8.893210
7.002632	567.426672	8.898227
6.806847	580.471534	8.903245
6.901854	574.233294	8.908263
6.890534	581.017126	8.913280
7.016265	577.587515	8.918298
7.051196	578.939517	8.923315
6.775018	581.952147	8.928333
7.168601	573.618196	8.933351
6.827758	581.937971	8.938368
6.807636	579.447484	8.943386
6.908312	577.677408	8.948403
6.849880	579.413597	8.953421
6.921736	572.267472	8.958439
6.980770	570.218910	8.963456
6.823760	561.453886	8.968474
6.770325	560.715441	8.973491
6.859034	570.707365	8.978509
7.094948	565.928848	8.983527
7.100934	565.598798	8.988544
6.750989	558.411970	8.993562
6.852438	544.005862	8.998579
6.658793	544.572697	9.003597
6.746713	568.179704	9.008615
6.880946	563.651533	9.013632
6.709334	580.195028	9.018650
7.117838	564.537771	9.023667
7.048174	579.470954	9.028685
7.132976	572.454359	9.033703
7.360183	572.589859	9.038720
6.910517	563.000913	9.043738
6.743439	544.969085	9.048755
7.011738	560.864689	9.053773
6.673826	567.609302	9.058791
6.883680	575.885373	9.063808
6.829600	582.810554	9.068826
6.853614	566.628275	9.073843
6.813023	580.503174	9.078861
6.842499	573.879797	9.083879
7.086724	571.476465	9.088896
6.879498	574.150299	9.093914
7.005600	573.661910	9.098931
6.928488	578.861342	9.103949
6.848258	579.551441	9.108967
6.939958	571.955600	9.113984
7.163839	577.128819	9.119002
6.887152	575.817887	9.124019
6.917207	580.417667	9.129037
7.212323	569.055462	9.134055
6.981567	574.899273	9.139072
6.828215	577.786969	9.144090
7.062286	575.482363	9.149107
7.005902	576.345649	9.154125
7.228430	571.468577	9.159143
6.951969	573.316982	9.164160
6.847081	585.573382	9.169178
7.574340	582.786640	9.174195
7.115328	587.994042	9.179213
6.960161	575.163105	9.184231
7.455241	579.915100	9.189248
6.920943	584.231155	9.194266
7.087662	575.702646	9.199283
7.009694	577.104710	9.204301
7.364715	580.067738	9.209319
7.300611	579.252530	9.214336
6.895231	579.629184	9.219354
7.337056	587.367535	9.224371
7.390712	587.417521	9.229389
6.921370	585.348715	9.234407
7.440162	580.605257	9.239424
7.162642	587.561476	9.244442
7.164292	576.922591	9.249459
7.007077	586.937488	9.254477
7.226612	601.562411	9.259495
7.734580	597.934235	9.264512
6.868924	594.465675	9.269530
7.438444	585.787147	9.274547
7.211221	580.862394	9.279565
7.169987	586.157234	9.284583
7.716217	589.838813	9.289600
7.261848	582.917144	9.294618
7.307201	573.891135	9.299635
7.439769	579.210821	9.304653
7.419786	575.554466	9.309671
7.429628	571.929569	9.314688
7.057887	568.149611	9.319706
7.376436	572.872683	9.324723
7.349035	573.449876	9.329741
7.308362	566.749980	9.334759
7.804316	568.585936	9.339776
7.285085	578.734614	9.344794
7.511653	572.512891	9.349811
7.624037	584.212355	9.354829
7.442627	579.614999	9.359847
7.212616	582.736481	9.364864
7.003054	589.903435	9.369882
7.411266	578.831454	9.374899
7.440463	582.183452	9.379917
7.361100	584.744114	9.384935
7.510332	572.457022	9.389952
7.300281	580.683804	9.394970
7.339028	582.305622	9.399987
7.294724	576.010425	9.405005
7.333504	574.397080	9.410023
7.489562	579.791595	9.415040
7.432352	576.492776	9.420058
7.470199	578.840665	9.425075
7.571332	577.651565	9.430093
6.982194	581.624599	9.435111
7.394228	566.352350	9.440128
7.553246	591.464965	9.445146
7.441412	578.260318	9.450163
7.339460	586.384695	9.455181
7.542020	606.668066	9.460199
7.822950	594.191168	9.465216
7.505933	592.841470	9.470234
7.509258	579.026786	9.475251
7.392942	588.535323	9.480269
7.547574	590.041235	9.485287
7.364016	580.418678	9.490304
7.459625	607.024802	9.495322
7.391180	611.831498	9.500339
7.723399	613.039414	9.505357
7.722449	611.116751	9.510375
7.977798	602.052083	9.515392
7.497139	590.695979	9.520410
7.248350	578.004802	9.525427
7.490583	588.173761	9.530445
7.588064	608.758632	9.535463
8.115902	602.095516	9.540480
7.518012	594.486535	9.545498
7.299847	588.256842	9.550515
7.550219	601.380702	9.555533
7.307154	607.721412	9.560551
7.726210	603.146677	9.565568
7.653498	609.641735	9.570586
7.730226	607.853393	9.575603
7.581858	610.513120	9.580621
7.417289	615.111403	9.585639
7.366204	604.759785	9.590656
7.419751	606.567122	9.595674
7.593554	610.233448	9.600691
7.705772	611.356878	9.605709
7.722251	606.910662	9.610727
8.003206	615.095810	9.615744
7.423280	617.209995	9.620762
7.502733	611.928970	9.625779
7.807274	619.725783	9.630797
7.233672	611.623427	9.635815
7.677321	608.319300	9.640832
7.666063	613.416072	9.645850
7.643718	619.708685	9.650867
7.821385	617.203033	9.655885
7.863795	612.955244	9.660903
7.941972	609.607736	9.665920
8.090088	617.164428	9.670938
8.117006	617.283025	9.675955
7.963587	614.857401	9.680973
7.848603	624.895025	9.685991
8.162318	617.838000	9.691008
7.981159	621.456446	9.696026
7.935698	616.597133	9.701043
8.148854	614.776076	9.706061
7.640806	610.206823	9.711079
7.802641	605.575044	9.716096
7.755787	613.334991	9.721114
7.826997	611.945565	9.726131
8.170879	602.171554	9.731149
7.597944	611.844575	9.736167
8.067571	607.078771	9.741184
8.154837	616.073803	9.746202
7.740091	619.173245	9.751219
7.933638	609.485236	9.756237
7.976060	616.046586	9.761255
7.476717	614.212862	9.766272
7.248552	612.943858	9.771290
7.507117	608.558775	9.776307
8.117585	617.453855	9.781325
7.792341	608.504776	9.786343
7.998764	614.019070	9.791360
8.091943	613.099181	9.796378
7.957098	610.556504	9.801395
8.122909	607.225727	9.806413
8.039053	609.267892	9.811431
7.876003	604.557250	9.816448
8.031630	609.970349	9.821466
7.671299	613.421740	9.826483
7.902017	606.326945	9.831501
7.781673	607.926393	9.836519
8.203121	613.104382	9.841536
8.378859	612.566801	9.846554
8.008518	614.943371	9.851571
8.420344	614.001619	9.856589
8.226242	619.080560	9.861607
8.190485	607.159593	9.866624
7.989559	614.934520	9.871642
8.070098	607.371813	9.876659
8.176890	613.532142	9.881677
7.701088	619.975511	9.886695
8.128769	603.288931	9.891712
7.879033	611.138105	9.896730
7.756289	617.646600	9.901747
8.031197	607.608089	9.906765
8.176283	613.387281	9.911783
8.266269	603.610788	9.916800
8.139505	608.886193	9.921818
7.751395	616.531223	9.926835
8.094537	618.705945	9.931853
8.230696	643.425035	9.936871
8.295654	633.037576	9.941888
8.063717	637.482510	9.946906
8.074263	634.065338	9.951923
8.611676	633.277304	9.956941
7.928837	643.554193	9.961959
8.367828	631.707436	9.966976
8.340628	641.532465	9.971994
8.212737	635.139729	9.977011
8.170485	622.232903	9.982029
7.996846	622.739333	9.987047
8.356048	627.331266	9.992064
8.306337	627.954489	9.997082
8.078647	643.162403	10.002099
8.192038	639.642711	10.007117
8.191071	637.426961	10.012135
8.400101	627.527722	10.017152
8.300087	635.262267	10.022170
8.230291	638.293750	10.027187
8.399830	625.175750	10.032205
8.120545	638.306187	10.037223
7.979812	635.768027	10.042240
8.198917	637.670478	10.047258
7.800797	635.005820	10.052275
8.305424	630.073181	10.057293
8.269475	638.506470	10.062311
8.083003	645.398767	10.067328
8.462675	632.352125	10.072346
8.102031	635.958678	10.077363
8.399076	632.503336	10.082381
8.120626	638.955443	10.087399
8.050052	635.842676	10.092416
8.563995	659.149504	10.097434
8.564779	669.885181	10.102451
8.580650	657.444611	10.107469
8.633201	648.977947	10.112487
8.585189	643.842300	10.117504
8.748587	640.983926	10.122522
8.071350	642.454697	10.127539
8.477369	641.714090	10.132557
8.387790	634.593981	10.137575
8.443594	645.401001	10.142592
8.722882	637.325757	10.147610
8.332269	647.806420	10.152627
8.274473	637.750950	10.157645
8.800860	633.607345	10.162663
8.437519	635.885321	10.167680
8.556251	643.380773	10.172698
8.346587	642.420871	10.177715
8.483632	634.269869	10.182733
8.587092	638.473441	10.187751
8.566984	636.916725	10.192768
8.539953	641.391770	10.197786
8.290930	650.705884	10.202803
8.826970	664.419864	10.207821
8.898536	660.580373	10.212839
8.549768	651.923542	10.217856
8.670364	637.805873	10.222874
8.288158	639.687608	10.227891
8.540339	631.603094	10.232909
8.507347	645.745664	10.237927
8.653164	659.334948	10.242944
8.911438	655.074693	10.247962
8.471740	657.445672	10.252979
8.656862	649.058934	10.257997
9.011022	647.280180	10.263015
8.433442	638.192330	10.268032
8.915201	631.925806	10.273050
8.583027	643.028000	10.278067
8.414259	636.153317	10.283085
8.632968	647.256661	10.288103
8.782505	666.036645	10.293120
9.134636	666.058673	10.298138
8.618301	646.971871	10.303155
8.667614	637.679835	10.308173
8.864074	646.189647	10.313191
8.529306	641.478994	10.318208
9.075734	640.091084	10.323226
8.636225	645.040954	10.328243
8.517269	641.987010	10.333261
8.788434	659.912586	10.338279
8.649520	664.488511	10.343296
8.740305	669.108339	10.348314
8.557853	670.227014	10.353331
8.786821	665.786996	10.358349
9.403493	665.607784	10.363367
8.834830	677.400241	10.368384
9.115788	658.833809	10.373402
8.929493	659.086853	10.378419
9.022086	634.217621	10.383437
8.806096	642.841651	10.388455
8.748902	639.198158	10.393472
8.497041	629.883552	10.398490
8.970119	654.922615	10.403507
9.097239	659.581673	10.408525
9.207025	637.640052	10.413543
8.789404	633.946831	10.418560
8.908812	628.635539	10.423578
8.583165	641.313683	10.428595
8.893092	640.634713	10.433613
9.120981	644.198365	10.438631
8.714952	650.966736	10.443648
9.264518	664.886523	10.448666
8.970503	650.335827	10.453683
8.814640	643.332235	10.458701
8.931648	648.663978	10.463719
8.780679	668.319632	10.468736
9.302793	665.557131	10.473754
9.342204	666.810964	10.478771
9.216283	651.380624	10.483789
9.126326	640.375653	10.488807
8.779002	641.949450	10.493824
8.980788	641.115830	10.498842
8.765918	643.266186	10.503859
8.856955	649.414385	10.508877
9.160235	664.538989	10.513895
8.919528	669.213914	10.518912
9.409764	659.022267	10.523930
9.122601	663.705896	10.528947
8.829839	662.861567	10.533965
9.349712	660.946419	10.538983
8.924534	666.791677	10.544000
9.181552	659.977305	10.549018
8.977925	672.798764	10.554035
9.441872	670.275045	10.559053
9.195823	662.980356	10.564071
9.066082	658.753098	10.569088
9.219368	661.980560	10.574106
9.125403	653.863220	10.579123
8.985824	665.496759	10.584141
9.233428	667.850346	10.589159
9.122449	679.779316	10.594176
9.371266	669.149479	10.599194
9.371287	658.113400	10.604211
9.345864	662.062242	10.609229
9.122312	651.572145	10.614247
8.966646	667.517461	10.619264
9.317018	664.153635	10.624282
9.095255	671.015591	10.629299
9.323752	666.016247	10.634317
9.399061	661.601770	10.639335
9.179125	669.834966	10.644352
9.335700	666.805885	10.649370
9.362064	662.987094	10.654387
9.110096	670.393791	10.659405
9.535619	667.810126	10.664423
9.187405	661.815977	10.669440
9.557311	667.388938	10.674458
9.306184	664.603592	10.679475
9.721219	674.410449	10.684493
9.275256	661.431135	10.689511
9.078187	669.729028	10.694528
9.416120	663.876522	10.699546
9.437349	673.888783	10.704563
9.380660	673.620325	10.709581
9.573748	669.089033	10.714599
9.444892	671.799066	10.719616
9.589527	662.977550	10.724634
9.464851	658.719138	10.729651
9.085668	649.967961	10.734669
9.514911	669.454154	10.739687
9.069558	674.340049	10.744704
9.412921	663.126240	10.749722
9.559584	672.251382	10.754739
9.212068	671.247860	10.759757
9.444052	674.022318	10.764775
9.370929	673.177700	10.769792
9.632158	668.899629	10.774810
9.354922	660.453130	10.779827
9.410797	671.152094	10.784845
9.500486	665.013315	10.789863
9.442330	672.381501	10.794880
9.327213	676.886550	10.799898
9.093481	669.400455	10.804915
9.051375	681.111302	10.809933
9.149541	684.100705	10.814951
9.384013	696.161035	10.819968
9.465171	710.590376	10.824986
9.508144	710.266773	10.830003
9.306135	717.769708	10.835021
9.774036	697.154793	10.840039
9.619433	707.030564	10.845056
9.740608	701.590027	10.850074
9.739178	702.305614	10.855091
9.800232	703.885551	10.860109
9.840202	704.610398	10.865127
9.704880	699.601834	10.870144
9.718052	696.981788	10.875162
9.691070	696.924517	10.880179
9.078485	698.514851	10.885197
9.757408	695.734549	10.890215
9.878287	700.614325	10.895232
10.039911	701.719707	10.900250
10.077569	697.348286	10.905267
9.683190	700.473491	10.910285
9.564109	698.564940	10.915303
9.305337	703.859759	10.920320
9.624795	700.841982	10.925338
9.712563	698.568564	10.930355
9.259455	698.325249	10.935373
9.922024	698.031528	10.940391
9.578771	697.894157	10.945408
9.587980	697.138207	10.950426
9.668472	691.877847	10.955443
9.534019	702.432103	10.960461
9.964038	707.368955	10.965479
10.077927	717.426862	10.970496
10.050635	705.417804	10.975514
10.108354	702.178590	10.980531
9.765067	701.137357	10.985549
9.865361	690.712493	10.990567
9.893903	698.878816	10.995584
9.910811	688.051310	11.000602
10.043062	701.815707	11.005619
9.667701	689.500763	11.010637
10.135157	699.495955	11.015655
10.128696	700.191710	11.020672
9.869877	702.689904	11.025690
9.697746	696.130689	11.030707
10.029554	697.331398	11.035725
10.138411	690.811106	11.040743
9.599593	700.053347	11.045760
9.919026	710.768764	11.050778
9.945734	719.804628	11.055795
9.637937	728.044191	11.060813
9.958809	720.975301	11.065831
10.042374	731.439407	11.070848
10.204009	732.528847	11.075866
10.105265	728.784767	11.080883
10.286405	728.663772	11.085901
10.301687	720.618193	11.090919
10.295003	712.414863	11.095936
9.896848	698.649875	11.100954
10.224182	697.712911	11.105971
10.171891	698.742440	11.110989
10.098571	688.323994	11.116007
10.091436	694.497779	11.121024
9.991020	687.874291	11.126042
10.077453	694.310652	11.131059
10.443315	712.066231	11.136077
10.355845	697.928370	11.141095
10.137678	702.842650	11.146112
9.977378	691.414329	11.151130
9.957313	690.110730	11.156147
10.169250	702.242718	11.161165
10.268232	713.231374	11.166183
10.287269	724.654159	11.171200
10.219693	714.131009	11.176218
10.556610	714.280163	11.181235
10.236154	709.533648	11.186253
10.364759	696.658987	11.191271
10.258379	697.478625	11.196288
10.248236	692.287852	11.201306
10.447516	685.381893	11.206323
9.923052	698.668477	11.211341
10.078321	701.123434	11.216359
10.300797	713.208800	11.221376
10.292162	727.707212	11.226394
10.444422	721.346216	11.231411
10.081490	717.266748	11.236429
10.429655	717.569138	11.241447
10.473090	731.514059	11.246464
10.512297	726.707759	11.251482
10.664327	711.777379	11.256499
10.336610	718.352660	11.261517
10.592464	707.253947	11.266535
10.418306	701.854033	11.271552
10.240855	699.534350	11.276570
10.506867	703.615260	11.281587
10.036644	701.276724	11.286605
10.399419	707.786640	11.291623
10.505628	725.978471	11.296640
10.601573	721.188922	11.301658
10.879642	715.282966	11.306675
10.396365	724.760459	11.311693
10.516269	712.011829	11.316711
10.633096	705.198890	11.321728
10.383289	702.004097	11.326746
10.698852	691.834374	11.331763
10.397997	708.342798	11.336781
10.340734	717.224717	11.341799
10.810729	718.916594	11.346816
10.654205	722.785674	11.351834
10.472740	703.616964	11.356851
10.182235	711.450723	11.361869
10.725377	718.870553	11.366887
10.680276	718.559029	11.371904
10.622147	725.567421	11.376922
10.781009	719.393504	11.381939
10.860248	723.038373	11.386957
10.494084	715.255393	11.391975
10.432273	714.467747	11.396992
10.357032	720.652469	11.402010
10.942671	718.458884	11.407027
10.638809	724.874899	11.412045
10.420538	719.437039	11.417063
10.502854	721.283699	11.422080
10.242836	730.057012	11.427098
10.529453	720.753434	11.432115
10.710981	722.274573	11.437133
10.396479	727.932967	11.442151
10.385914	723.700449	11.447168
10.426949	731.408842	11.452186
11.084611	740.786271	11.457203
10.611896	738.398540	11.462221
10.733681	736.175759	11.467239
10.897403	731.555636	11.472256
11.035431	746.441075	11.477274
11.066186	736.924521	11.482291
10.389171	728.808584	11.487309
10.830558	736.269743	11.492327
11.145653	742.096508	11.497344
10.789339	739.770527	11.502362
11.003469	725.970277	11.507379
10.955408	727.277036	11.512397
10.658076	715.837617	11.517415
11.015512	725.661954	11.522432
10.775075	725.465174	11.527450
11.176506	727.545781	11.532467
10.717345	730.098142	11.537485
10.760923	727.904107	11.542503
11.009660	739.372577	11.547520
10.658857	748.123395	11.552538
10.961560	741.515946	11.557555
11.179489	745.844409	11.562573
11.251896	742.325206	11.567591
11.072247	740.148588	11.572608
11.000339	747.334464	11.577626
11.092191	745.879591	11.582643
10.902751	744.209286	11.587661
11.150240	751.199962	11.592679
11.083547	738.380953	11.597696
10.919102	750.110414	11.602714
11.225691	740.164379	11.607731
11.395983	742.151329	11.612749
11.068406	735.772450	11.617767
10.933419	732.484556	11.622784
10.965142	744.750066	11.627802
11.107944	733.929947	11.632819
11.470669	732.876281	11.637837
11.114918	737.976222	11.642855
11.316565	725.255920	11.647872
11.286808	721.122451	11.652890
11.194117	725.720827	11.657907
11.428069	715.963442	11.662925
11.053452	727.355603	11.667943
11.068450	721.969514	11.672960
11.316995	724.175130	11.677978
11.039015	722.583319	11.682995
11.014996	720.264704	11.688013
11.101042	730.791582	11.693031
11.106886	738.638298	11.698048
10.905649	746.879449	11.703066
11.487049	741.875752	11.708083
11.250291	740.244216	11.713101
11.172393	743.130030	11.718119
11.170990	746.033247	11.723136
10.741566	748.434222	11.728154
11.313839	743.564512	11.733171
11.423847	736.575344	11.738189
11.125820	747.523129	11.743207
11.481136	746.230356	11.748224
11.226944	745.855758	11.753242
10.946253	740.727651	11.758259
11.282107	745.038286	11.763277
11.287825	766.449778	11.768295
11.448247	765.557087	11.773312
11.497434	782.570754	11.778330
11.698978	774.146773	11.783347
11.351301	765.420606	11.788365
11.398680	770.523825	11.793383
11.566803	765.924613	11.798400
11.372428	769.182128	11.803418
11.398984	771.441969	11.808435
11.509632	774.628513	11.813453
11.429841	778.790540	11.818471
11.513878	770.387863	11.823488
11.377312	768.218056	11.828506
11.574119	774.297351	11.833523
11.542729	760.854194	11.838541
11.273007	779.550861	11.843559
11.687439	767.666748	11.848576
11.391809	771.797723	11.853594
11.442577	763.804290	11.858611
11.757575	762.774695	11.863629
11.453978	775.154816	11.868647
11.916349	773.119497	11.873664
11.507157	779.572922	11.878682
11.451345	772.879389	11.883699
11.679459	772.922818	11.888717
11.617462	767.321182	11.893735
11.724293	765.463847	11.898752
11.781393	776.220550	11.903770
11.491379	767.382837	11.908787
11.641395	775.889024	11.913805
11.623798	776.896257	11.918823
11.598752	767.216531	11.923840
11.490456	767.116676	11.928858
11.119980	773.826439	11.933875
11.495603	777.114995	11.938893
11.555456	792.934665	11.943911
12.040749	798.524517	11.948928
12.257902	802.437800	11.953946
12.228725	789.781399	11.958963
12.432782	782.647257	11.963981
11.936209	777.551477	11.968999
11.963894	760.903654	11.974016
11.854365	774.136296	11.979034
12.237461	768.969305	11.984051
12.547856	759.630061	11.989069
12.272702	773.497273	11.994087
12.176873	764.380651	11.999104
11.983839	768.470165	12.004122
12.168534	766.468992	12.009139
11.976374	752.038859	12.014157
11.783492	748.892464	12.019175
12.162066	755.354895	12.024192
11.994953	748.195262	12.029210
11.834627	745.084793	12.034227
12.256325	747.670658	12.039245
11.861221	753.159990	12.044263
12.261457	753.870429	12.049280
12.004415	744.436348	12.054298
11.773904	738.433038	12.059315
12.018468	744.125278	12.064333
11.996444	762.350473	12.069351
12.020444	757.972841	12.074368
11.934094	768.887820	12.079386
12.049798	765.370471	12.084403
12.194258	767.325893	12.089421
12.143789	766.867831	12.094439
11.966345	760.711607	12.099456
12.307566	772.815470	12.104474
12.106443	766.869858	12.109491
12.262584	769.280393	12.114509
12.163529	776.196011	12.119527
12.211797	760.208499	12.124544
12.325965	771.756836	12.129562
12.154952	769.551615	12.134579
12.107943	767.034466	12.139597
11.841858	773.850295	12.144615
11.909510	768.937294	12.149632
11.886530	769.502540	12.154650
11.870040	781.253886	12.159667
12.173323	764.855113	12.164685
12.068011	772.334523	12.169703
12.131906	782.667494	12.174720
12.512226	785.211231	12.179738
12.283437	790.291859	12.184755
12.457297	792.288458	12.189773
12.222280	787.379893	12.194791
12.559639	796.418496	12.199808
12.373733	787.161528	12.204826
12.540486	782.409794	12.209843
12.501769	779.748756	12.214861
11.942050	783.388824	12.219879
12.447965	791.490025	12.224896
12.551362	793.244810	12.229914
12.407425	799.057938	12.234931
12.551353	801.501607	12.239949
12.644887	793.678597	12.244967
12.620773	794.052314	12.249984
12.489033	776.289125	12.255002
12.216067	772.510217	12.260019
12.314901	783.407812	12.265037
12.526201	796.190130	12.270055
12.459364	794.417362	12.275072
12.762292	796.710399	12.280090
12.334487	797.925568	12.285107
12.289398	798.232304	12.290125
12.293516	806.782244	12.295143
12.281972	804.033030	12.300160
12.390288	800.882228	12.305178
12.299728	803.525687	12.310195
12.593303	803.747790	12.315213
12.491803	801.628838	12.320231
12.556464	789.146788	12.325248
12.343256	799.600035	12.330266
12.366080	821.208549	12.335283
12.757921	822.221350	12.340301
12.967567	834.643960	12.345319
13.087476	828.897114	12.350336
12.913715	819.069840	12.355354
12.331357	798.093367	12.360371
12.858073	809.710949	12.365389
12.778142	821.726593	12.370407
12.947589	825.313976	12.375424
13.009801	808.581235	12.380442
12.633252	799.011089	12.385459
12.996064	802.288789	12.390477
12.877888	796.138448	12.395495
12.744778	794.781587	12.400512
12.535114	795.406601	12.405530
12.832774	820.331005	12.410547
12.932986	818.631052	12.415565
12.641640	832.510062	12.420583
12.735577	826.624039	12.425600
13.269636	823.615843	12.430618
12.739641	821.385050	12.435635
13.444212	825.942275	12.440653
13.113281	835.148665	12.445671
13.007039	815.374639	12.450688
12.977873	808.753428	12.455706
12.804728	806.591466	12.460723
13.006752	809.863611	12.465741
13.057670	818.522306	12.470759
13.074631	820.989838	12.475776
12.854979	814.136130	12.480794
13.048097	831.220607	12.485811
13.200687	825.000056	12.490829
12.484287	833.234758	12.495847
12.675651	828.453921	12.500864
13.021024	821.212421	12.505882
12.921602	831.869202	12.510899
13.076863	827.015435	12.515917
13.047983	832.378773	12.520935
12.689228	831.516665	12.525952
12.835472	833.000178	12.530970
12.618387	826.716275	12.535987
13.160807	842.248322	12.541005
13.423251	857.157674	12.546023
13.487837	850.203168	12.551040
13.368316	833.033512	12.556058
13.566729	830.630669	12.561075
13.452512	825.169768	12.566093
13.437637	810.905572	12.571111
13.464171	822.116962	12.576128
13.212889	817.008744	12.581146
13.092368	823.009904	12.586163
13.165875	809.226655	12.591181
13.339564	815.622779	12.596199
13.454063	815.525261	12.601216
13.651179	810.947592	12.606234
13.444006	813.847623	12.611251
13.379273	818.439805	12.616269
13.078774	813.383859	12.621287
13.497785	820.364757	12.626304
13.283776	815.151335	12.631322
13.408306	820.555308	12.636339
13.594570	816.496335	12.641357
13.592775	827.000283	12.646375
13.393904	823.372224	12.651392
13.598071	806.200960	12.656410
13.302888	823.662040	12.661427
13.398946	813.608637	12.666445
13.622973	815.070363	12.671463
13.336567	823.373739	12.676480
13.499905	813.925646	12.681498
13.555982	821.456400	12.686515
13.481222	815.445281	12.691533
13.501073	819.903334	12.696551
13.148100	828.111682	12.701568
13.581308	822.817651	12.706586
13.506655	841.166639	12.711603
13.444028	844.797717	12.716621
13.819699	849.613342	12.721639
13.609835	844.169906	12.726656
13.953975	846.442520	12.731674
13.773745	850.238019	12.736691
13.722083	842.032648	12.741709
13.757355	854.653340	12.746727
13.429427	844.976862	12.751744
13.785763	842.783581	12.756762
13.470516	851.472841	12.761779
13.504251	851.454687	12.766797
13.797084	847.708483	12.771815
13.571198	849.980768	12.776832
13.590904	842.556985	12.781850
13.609169	855.468674	12.786867
13.719545	848.242206	12.791885
13.892720	847.775117	12.796903
13.711116	857.473398	12.801920
13.824983	845.277002	12.806938
14.028893	861.296405	12.811955
13.922671	849.453887	12.816973
13.928266	849.716376	12.821991
13.659045	857.775788	12.827008
13.690424	850.499068	12.832026
13.572035	853.906361	12.837043
13.666168	852.183401	12.842061
13.765121	857.805797	12.847079
14.160553	888.731176	12.852096
14.205144	872.264664	12.857114
13.857458	878.192783	12.862131
13.861025	877.706643	12.867149
14.321921	872.819974	12.872167
14.250233	871.707999	12.877184
14.209275	849.831484	12.882202
13.992921	850.398757	12.887219
13.783060	843.995544	12.892237
14.052666	855.697624	12.897255
14.193955	865.963263	12.902272
14.434779	859.175708	12.907290
14.230764	856.333483	12.912307
13.986399	849.341948	12.917325
14.061827	843.157835	12.922343
14.272208	867.846052	12.927360
14.282165	857.677413	12.932378
13.991686	853.041807	12.937395
14.296975	865.773524	12.942413
14.282652	856.725578	12.947431
13.878646	861.682606	12.952448
14.323665	865.565512	12.957466
14.612921	867.560657	12.962483
14.529129	867.271898	12.967501
14.638520	843.385694	12.972519
14.354628	835.775974	12.977536
14.304354	838.523562	12.982554
14.114734	833.615705	12.987571
14.657549	838.366934	12.992589
14.705807	830.674650	12.997607
14.701589	836.569090	13.002624
14.529532	832.437985	13.007642
14.575408	827.400049	13.012659
14.311898	833.175391	13.017677
14.361579	833.836429	13.022695
14.392224	838.819232	13.027712
14.475723	827.730380	13.032730
14.779326	837.923751	13.037747
14.342308	836.848091	13.042765
14.296804	830.139042	13.047783
14.251651	835.636769	13.052800
14.348802	835.710430	13.057818
14.209173	832.128425	13.062835
14.276113	838.804881	13.067853
14.667902	854.869227	13.072871
14.763560	868.352866	13.077888
15.033416	851.335189	13.082906
14.651224	843.620158	13.087923
14.384452	847.330440	13.092941
14.779825	832.170535	13.097959
14.614679	843.045321	13.102976
14.529491	838.184667	13.107994
14.505347	849.430089	13.113011
14.370314	862.767629	13.118029
14.772068	863.098713	13.123047
14.827284	875.755278	13.128064
14.909466	871.441167	13.133082
14.852855	874.872053	13.138099
14.749030	870.225103	13.143117
15.193327	862.784477	13.148135
14.621227	845.998275	13.153152
14.754906	847.094141	13.158170
14.700617	841.594535	13.163187
14.577584	862.865171	13.168205
14.933361	863.113744	13.173223
14.708714	871.150205	13.178240
14.982256	865.108340	13.183258
15.030993	866.882061	13.188275
14.915269	868.160317	13.193293
15.155828	863.686035	13.198311
14.603705	862.172055	13.203328
14.752285	869.671710	13.208346
15.019072	867.176401	13.213363
14.821486	875.293400	13.218381
14.940097	868.010439	13.223399
15.055266	869.128280	13.228416
15.007868	872.614126	13.233434
14.957743	866.537677	13.238451
14.710884	871.603816	13.243469
15.218545	871.977923	13.248487
14.935245	878.118948	13.253504
14.954624	871.190843	13.258522
15.194155	872.094719	13.263539
15.232889	872.783561	13.268557
15.002450	873.669887	13.273575
14.787358	876.464560	13.278592
14.564780	878.817593	13.283610
14.796406	867.495643	13.288627
14.898592	884.462821	13.293645
15.158412	886.791185	13.298663
15.326838	882.694021	13.303680
15.369399	894.462802	13.308698
15.620106	886.078027	13.313715
15.370404	883.985861	13.318733
15.287356	866.327854	13.323751
15.478079	861.250086	13.328768
15.516298	853.801372	13.333786
15.385551	855.230539	13.338803
15.397665	862.494229	13.343821
15.372697	845.688935	13.348839
15.265080	862.708873	13.353856
15.297416	854.938323	13.358874
15.406139	854.677013	13.363891
14.996613	861.625375	13.368909
15.445775	861.781464	13.373927
15.695845	890.031582	13.378944
15.303587	876.228252	13.383962
15.533224	878.749809	13.388979
15.211352	887.917521	13.393997
15.662042	884.805067	13.399015
15.299213	895.521814	13.404032
15.577781	893.967001	13.409050
15.904010	890.263461	13.414067
15.374413	894.104439	13.419085
15.387060	889.733381	13.424103
15.700128	892.593806	13.429120
15.692597	884.719638	13.434138
15.508170	885.634929	13.439155
15.337973	887.602117	13.444173
15.737877	885.324034	13.449191
15.810824	883.856150	13.454208
15.544807	885.783362	13.459226
15.910647	882.252559	13.464243
15.799952	880.369952	13.469261
15.707876	887.217338	13.474279
15.844255	883.587871	13.479296
15.637723	886.468912	13.484314
15.585965	883.502170	13.489331
15.372128	888.215014	13.494349
15.903235	885.552550	13.499367
15.939587	876.792016	13.504384
15.426634	884.077636	13.509402
15.841810	888.597357	13.514419
15.801526	889.266264	13.519437
15.875833	882.552632	13.524455
15.849113	888.782896	13.529472
15.659783	894.580181	13.534490
16.087404	879.607968	13.539507
15.677232	885.621667	13.544525
15.654525	888.956376	13.549543
15.598741	887.313837	13.554560
15.599641	889.594298	13.559578
16.091394	898.151423	13.564595
16.266641	910.154249	13.569613
15.968216	887.297902	13.574631
16.380795	887.792728	13.579648
16.396083	882.604553	13.584666
16.689526	881.126201	13.589683
16.377817	879.669498	13.594701
16.344782	878.591055	13.599719
15.982839	870.763203	13.604736
16.142866	879.711258	13.609754
16.497675	876.017931	13.614771
15.990648	883.558652	13.619789
15.994124	869.515943	13.624807
16.034863	881.496420	13.629824
16.111638	880.916622	13.634842
16.569203	879.493269	13.639859
16.162860	888.939375	13.644877
16.255376	882.023517	13.649895
16.225761	878.311018	13.654912
16.099614	880.412409	13.659930
16.862340	869.170481	13.664947
16.225185	874.191852	13.669965
16.285353	865.652549	13.674983
16.280630	875.815503	13.680000
16.135890	877.426317	13.685018
16.317362	877.766653	13.690035
16.286210	884.025209	13.695053
16.586773	879.083894	13.700071
16.788683	872.980905	13.705088
16.439766	880.129817	13.710106
16.823643	872.204971	13.715123
16.491488	878.797000	13.720141
16.397557	875.716804	13.725159
16.696560	877.916221	13.730176
16.534916	881.890122	13.735194
16.758548	873.766530	13.740211
16.468161	875.036220	13.745229
16.566600	880.485493	13.750247
16.519697	878.443868	13.755264
16.119842	871.690160	13.760282
16.453855	872.434445	13.765299
16.530290	882.560294	13.770317
16.509146	877.795669	13.775335
16.764479	875.780774	13.780352
16.352699	893.464054	13.785370
16.845974	877.424897	13.790387
16.859037	873.378556	13.795405
16.617833	879.108674	13.800423
16.471975	877.636610	13.805440
16.508612	876.724134	13.810458
16.603643	872.368914	13.815475
16.818750	898.180729	13.820493
16.622842	906.936401	13.825511
16.826456	918.633750	13.830528
16.419595	927.909504	13.835546
16.711166	904.107486	13.840563
16.598368	913.371755	13.845581
16.698615	915.127078	13.850599
16.901458	913.023467	13.855616
16.336955	914.654252	13.860634
16.991605	914.936021	13.865651
17.060770	916.331573	13.870669
17.148187	914.277066	13.875687
17.239756	914.531565	13.880704
16.707254	908.436658	13.885722
16.908605	900.315968	13.890739
16.945769	915.802942	13.895757
16.967299	907.207443	13.900775
16.860210	905.274237	13.905792
16.937850	904.339001	13.910810
17.161946	914.940495	13.915827
16.960611	908.350809	13.920845
17.215397	908.439213	13.925863
17.227038	914.190110	13.930880
16.779959	913.699938	13.935898
17.113691	913.598853	13.940915
17.081834	924.109437	13.945933
17.334374	940.022421	13.950951
17.679214	929.461875	13.955968
17.313538	925.057236	13.960986
17.360571	903.936641	13.966003
17.559279	893.770068	13.971021
17.543720	897.420499	13.976039
17.075427	886.713652	13.981056
16.719958	903.470519	13.986074
17.227737	907.179236	13.991091
17.454207	930.743299	13.996109
17.437534	918.566967	14.001127
17.849437	913.085121	14.006144
17.314143	902.620487	14.011162
17.543289	895.379768	14.016179
17.304046	900.365325	14.021197
17.620508	895.860703	14.026215
17.431421	902.559466	14.031232
17.158569	898.597251	14.036250
17.448431	912.418706	14.041267
17.675581	913.616750	14.046285
17.704549	937.064052	14.051303
18.094479	922.200615	14.056320
17.550924	908.646600	14.061338
17.801566	898.772161	14.066355
17.750798	894.942315	14.071373
17.298679	895.079318	14.076391
17.568100	894.013789	14.081408
17.268207	892.167744	14.086426
17.359235	908.845681	14.091443
17.838309	913.692563	14.096461
17.506988	924.112772	14.101479
17.705843	930.602983	14.106496
17.595681	932.050388	14.111514
17.942881	923.010618	14.116531
17.789334	922.994853	14.121549
17.630858	925.671470	14.126567
18.050373	928.720890	14.131584
17.750689	928.786890	14.136602
17.776370	918.997463	14.141619
18.142052	929.090425	14.146637
17.805281	932.481279	14.151655
18.017820	924.925216	14.156672
17.796343	926.241131	14.161690
17.999396	932.740094	14.166707
18.046405	928.534562	14.171725
17.988207	931.822033	14.176743
17.993009	931.056766	14.181760
17.729211	932.482465	14.186778
17.634421	926.244332	14.191795
17.587740	926.412761	14.196813
17.601429	928.106492	14.201831
18.151795	916.973639	14.206848
17.972583	926.862695	14.211866
17.952831	924.447283	14.216883
18.051371	914.139088	14.221901
17.994455	935.547644	14.226919
18.316021	932.547188	14.231936
18.287016	935.232206	14.236954
18.271698	929.920568	14.241971
18.209080	918.247904	14.246989
17.965662	915.228371	14.252007
18.412206	929.873745	14.257024
18.695974	940.830276	14.262042
18.478510	920.459087	14.267059
18.296618	927.402713	14.272077
18.146644	913.374643	14.277095
18.602619	909.909753	14.282112
18.446626	916.147933	14.287130
18.387343	908.658709	14.292147
18.284735	904.710714	14.297165
18.101105	909.828360	14.302183
18.450087	916.562100	14.307200
18.289085	910.325923	14.312218
18.162093	917.845422	14.317235
18.598622	931.105936	14.322253
18.489615	950.865794	14.327271
18.562110	945.944255	14.332288
18.454622	949.071821	14.337306
18.938894	952.415975	14.342323
18.530511	922.269246	14.347341
18.440230	922.892531	14.352359
18.695470	938.857030	14.357376
18.919698	946.395328	14.362394
18.510778	932.030382	14.367411
18.891517	911.031466	14.372429
18.536558	905.034209	14.377447
18.568613	906.926447	14.382464
18.853951	918.372040	14.387482
18.589432	923.753119	14.392499
19.077875	924.600275	14.397517
18.969000	930.785357	14.402535
18.949311	915.215253	14.407552
19.041552	909.357038	14.412570
18.838082	906.317088	14.417587
19.071121	905.920161	14.422605
18.860239	901.691363	14.427623
18.745199	902.247507	14.432640
18.759308	912.540615	14.437658
18.677734	902.836736	14.442675
18.961318	903.245923	14.447693
18.854941	906.282357	14.452711
18.736720	898.600978	14.457728
19.097147	916.658465	14.462746
18.951668	911.742853	14.467763
18.788254	920.625013	14.472781
18.861501	935.900905	14.477799
19.166964	937.236713	14.482816
18.885505	945.991666	14.487834
18.903813	943.233726	14.492851
19.104364	938.238940	14.497869
18.999612	942.316779	14.502887
19.124176	933.025442	14.507904
19.167668	935.741323	14.512922
18.786402	940.622553	14.517939
19.142941	925.398150	14.522957
19.055519	936.658877	14.527975
18.875157	928.861834	14.532992
19.135788	936.659021	14.538010
19.353318	936.830778	14.543027
19.501884	932.894175	14.548045
19.185404	936.747770	14.553063
19.159092	934.716494	14.558080
19.277074	927.118276	14.563098
19.112571	931.916628	14.568115
19.210046	930.547806	14.573133
19.305556	941.075026	14.578151
19.648469	961.784920	14.583168
19.439739	952.383229	14.588186
19.163822	952.740144	14.593203
19.665131	952.249418	14.598221
19.667561	965.587229	14.603239
19.667387	950.386659	14.608256
19.501596	942.167529	14.613274
19.421415	943.411539	14.618291
19.719350	950.102994	14.623309
19.521875	944.348427	14.628327
19.585454	951.344566	14.633344
19.572907	960.304422	14.638362
19.757714	967.700079	14.643379
19.934376	953.996794	14.648397
19.765692	945.384466	14.653415
19.878405	938.762648	14.658432
19.631118	931.090895	14.663450
19.573999	927.966777	14.668467
19.656225	926.134771	14.673485
19.729471	939.184823	14.678503
19.633856	946.932964	14.683520
19.920809	956.252858	14.688538
19.810021	962.787461	14.693555
20.295938	943.580754	14.698573
20.050667	943.044440	14.703591
19.777989	929.257995	14.708608
19.943800	929.765493	14.713626
19.582382	934.507998	14.718643
20.023543	942.666103	14.723661
19.657140	957.509215	14.728679
20.034067	961.079862	14.733696
19.796243	953.719103	14.738714
19.882016	950.655478	14.743731
19.862420	957.556395	14.748749
19.820721	953.360877	14.753767
19.974828	955.360387	14.758784
19.953519	958.169713	14.763802
19.787672	954.493617	14.768819
19.884556	957.843108	14.773837
19.962082	958.993194	14.778855
19.837934	975.259750	14.783872
20.013523	972.419367	14.788890
20.460057	990.273271	14.793907
20.741077	977.691529	14.798925
20.665766	965.185950	14.803943
19.985260	958.797136	14.808960
20.189069	951.733820	14.813978
20.271078	963.290795	14.818995
20.501733	954.723894	14.824013
20.579106	955.469700	14.829031
20.149830	953.470359	14.834048
20.310603	957.472182	14.839066
20.367364	977.982822	14.844083
20.504576	976.281427	14.849101
20.807933	973.805218	14.854119
20.580428	970.555090	14.859136
20.733621	953.558266	14.864154
20.107999	944.268388	14.869171
20.424680	935.934427	14.874189
20.563259	964.010114	14.879207
20.711362	962.050627	14.884224
20.866520	963.095690	14.889242
20.080434	960.303735	14.894259
20.467042	968.316206	14.899277
20.331615	981.607657	14.904295
20.441096	979.883313	14.909312
20.825890	978.544288	14.914330
20.616587	981.153776	14.919347
21.000448	981.228207	14.924365
20.804592	981.299784	14.929383
20.908028	979.498890	14.934400
21.088895	972.166559	14.939418
20.771739	984.682754	14.944435
21.087455	977.176442	14.949453
20.660334	977.323856	14.954471
20.539206	983.599179	14.959488
20.858963	972.836092	14.964506
20.588081	983.077801	14.969523
20.805169	979.463242	14.974541
21.071171	985.497068	14.979559
20.696476	984.236638	14.984576
20.984536	975.958986	14.989594
20.859712	982.419163	14.994611
20.825932	982.786618	14.999629
21.159153	972.962575	15.004647
20.802998	979.917472	15.009664
21.034136	973.487755	15.014682
20.802754	975.791088	15.019699
21.217048	993.451153	15.024717
21.219768	989.789549	15.029735
21.222978	994.303368	15.034752
21.239699	982.166708	15.039770
20.872274	988.999474	15.044787
21.070580	993.460001	15.049805
21.479232	987.504289	15.054823
21.214565	999.155916	15.059840
21.439226	985.342269	15.064858
21.503684	989.414436	15.069875
21.431134	990.558762	15.074893
21.315979	995.746940	15.079911
21.534429	998.031807	15.084928
21.696584	998.985951	15.089946
21.168572	992.119049	15.094963
20.999178	995.726965	15.099981
21.187066	1003.870903	15.104999
21.180447	1006.715590	15.110016
21.412210	997.109564	15.115034
21.232021	1000.831474	15.120051
21.185099	995.630966	15.125069
21.244512	995.244785	15.130087
21.038764	1004.569830	15.135104
21.671834	1017.512730	15.140122
21.703357	1024.988613	15.145139
21.913977	1028.309766	15.150157
21.958471	1019.634802	15.155175
21.941032	1009.574153	15.160192
21.968004	1001.970554	15.165210
21.842383	996.262683	15.170227
21.878745	992.584857	15.175245
21.713505	998.814371	15.180263
21.608901	997.887374	15.185280
22.225784	987.587067	15.190298
21.878114	993.785880	15.195315
21.801296	986.109780	15.200333
21.993967	994.970199	15.205351
21.867556	998.420587	15.210368
21.893683	984.454516	15.215386
21.877332	997.904132	15.220403
21.717528	989.846177	15.225421
21.971790	992.651044	15.230439
21.767062	996.608514	15.235456
22.088652	990.078328	15.240474
22.023474	985.148558	15.245491
22.091048	997.557908	15.250509
22.417436	1000.001203	15.255527
22.130440	994.843352	15.260544
21.972937	989.351006	15.265562
22.072803	996.464749	15.270579
22.005021	997.709852	15.275597
22.447869	1005.233101	15.280615
22.116379	1015.260902	15.285632
22.133200	1014.438125	15.290650
22.239892	1020.126416	15.295667
22.498382	1020.984634	15.300685
22.493767	1013.148891	15.305703
22.125425	1014.361277	15.310720
22.325323	1016.412630	15.315738
22.228389	1015.647733	15.320755
22.416358	1021.441801	15.325773
22.549799	1013.990962	15.330791
22.330186	1013.429123	15.335808
22.507790	1007.537786	15.340826
22.716587	1021.266519	15.345843
22.296516	1017.731081	15.350861
22.542518	1019.038987	15.355879
22.629834	1020.644905	15.360896
22.516184	1017.818337	15.365914
22.427062	1017.637936	15.370931
22.356045	1023.784874	15.375949
22.779910	1013.892200	15.380967
22.266790	1024.264744	15.385984
22.469582	1030.849220	15.391002
22.444465	1025.095502	15.396019
22.527288	1018.541213	15.401037
22.574839	1020.522617	15.406055
22.376570	1018.513611	15.411072
22.713762	1041.214212	15.416090
23.100152	1045.743883	15.421107
23.017837	1051.174639	15.426125
22.910580	1038.978230	15.431143
22.637175	1028.514862	15.436160
22.838159	1041.661480	15.441178
22.793042	1044.871607	15.446195
22.605951	1055.226202	15.451213
22.823354	1048.590874	15.456231
22.776877	1058.002465	15.461248
23.200158	1043.263284	15.466266
22.969429	1053.810947	15.471283
22.810585	1062.769590	15.476301
23.424423	1048.171164	15.481319
22.949306	1050.325658	15.486336
22.989454	1050.147785	15.491354
23.224660	1049.024944	15.496371
23.168302	1056.528046	15.501389
23.219333	1045.911928	15.506407
23.154473	1054.514020	15.511424
23.190867	1049.513413	15.516442
23.217369	1043.895982	15.521459
22.955631	1060.977972	15.526477
23.190806	1047.162522	15.531495
22.806872	1046.198882	15.536512
23.028026	1060.632250	15.541530
23.377928	1061.529605	15.546547
23.322583	1074.823573	15.551565
23.840239	1069.009546	15.556583
23.698377	1071.664924	15.561600
23.633977	1048.676926	15.566618
23.612423	1039.435007	15.571635
23.195574	1038.339444	15.576653
23.819939	1036.775173	15.581671
23.460104	1035.922482	15.586688
23.249208	1036.164266	15.591706
23.630668	1045.298436	15.596723
23.702925	1064.308667	15.601741
23.899947	1060.210837	15.606759
23.936558	1048.830227	15.611776
23.513168	1038.854352	15.616794
23.665431	1032.505827	15.621811
23.921263	1040.897138	15.626829
24.183088	1032.566339	15.631847
23.756275	1040.195961	15.636864
23.277154	1035.040503	15.641882
23.747362	1046.338542	15.646899
23.919716	1067.832002	15.651917
23.982850	1057.669353	15.656935
23.797174	1053.457188	15.661952
23.614946	1069.818531	15.666970
23.768452	1066.682211	15.671987
23.846277	1068.974715	15.677005
24.117061	1071.274515	15.682023
23.912178	1068.136741	15.687040
23.914078	1066.672381	15.692058
24.159804	1065.853680	15.697075
23.723559	1073.443156	15.702093
24.024886	1070.231089	15.707111
24.300316	1066.764285	15.712128
23.979769	1069.441487	15.717146
24.211264	1066.616991	15.722163
24.013691	1066.418002	15.727181
24.168613	1068.142996	15.732199
24.187926	1071.189280	15.737216
24.254212	1075.678860	15.742234
24.448021	1053.836852	15.747251
24.178335	1057.161074	15.752269
24.133952	1058.305053	15.757287
24.130118	1067.120618	15.762304
24.279194	1073.882929	15.767322
24.826118	1072.774810	15.772339
24.302583	1076.626241	15.777357
24.513236	1068.118504	15.782375
24.274829	1074.371232	15.787392
24.416479	1066.906406	15.792410
24.187237	1070.738842	15.797427
24.423519	1078.496843	15.802445
24.678071	1081.824092	15.807463
24.676297	1076.690458	15.812480
24.522081	1086.596720	15.817498
24.782415	1078.932250	15.822515
24.880618	1086.975789	15.827533
24.852540	1079.339177	15.832551
24.878551	1078.606203	15.837568
24.893570	1079.876918	15.842586
24.932676	1075.545502	15.847603
24.854733	1081.675899	15.852621
24.956512	1077.293516	15.857639
25.246537	1079.106288	15.862656
25.155902	1062.107747	15.867674
25.240779	1060.404805	15.872691
25.007561	1062.934428	15.877709
24.823693	1055.024918	15.882727
25.062400	1066.117761	15.887744
24.757962	1054.257246	15.892762
24.880176	1051.081644	15.897779
24.968162	1058.362342	15.902797
25.020538	1053.989358	15.907815
24.943813	1046.808067	15.912832
24.711519	1051.760629	15.917850
24.950179	1052.413889	15.922867
24.846502	1070.781358	15.927885
25.260603	1074.099016	15.932903
25.388387	1073.949095	15.937920
25.343232	1080.719677	15.942938
25.153465	1077.607733	15.947955
25.064712	1081.007001	15.952973
25.251409	1077.266769	15.957991
25.144605	1077.760530	15.963008
25.364150	1074.253409	15.968026
25.446935	1075.082569	15.973043
25.302183	1078.930097	15.978061
25.099694	1072.162983	15.983079
25.314012	1072.753757	15.988096
25.211562	1081.300303	15.993114
25.544566	1079.461242	15.998131
25.312353	1079.193999	16.003149
25.263324	1078.140049	16.008167
25.597728	1090.104753	16.013184
25.418964	1095.799967	16.018202
25.872173	1097.829701	16.023219
25.781905	1093.650090	16.028237
25.523095	1088.774909	16.033255
25.483603	1092.060092	16.038272
25.605044	1095.789370	16.043290
25.541008	1085.305730	16.048307
25.933030	1091.185982	16.053325
25.847688	1094.192974	16.058343
25.855234	1094.365383	16.063360
25.685751	1100.331484	16.068378
26.175629	1090.435269	16.073395
26.222337	1097.836620	16.078413
26.153582	1092.272797	16.083431
26.005032	1090.089779	16.088448
26.055149	1091.050346	16.093466
26.363993	1093.335558	16.098483
26.193211	1084.388085	16.103501
26.062955	1071.365989	16.108519
25.881740	1061.665186	16.113536
26.245763	1070.158210	16.118554
26.099557	1063.148687	16.123571
26.266164	1074.881439	16.128589
26.015839	1067.019975	16.133607
26.191446	1076.264752	16.138624
26.050547	1090.195754	16.143642
26.430341	1084.347945	16.148659
26.535128	1091.016843	16.153677
26.171480	1079.371257	16.158695
26.140494	1083.782523	16.163712
25.878846	1091.167802	16.168730
26.420103	1085.914777	16.173747
26.350352	1096.829394	16.178765
26.375618	1093.084495	16.183783
26.630237	1076.567897	16.188800
26.360910	1100.682316	16.193818
26.430837	1083.412983	16.198835
26.515084	1089.035349	16.203853
26.103299	1088.537334	16.208871
25.999700	1078.440176	16.213888
26.173512	1098.047317	16.218906
26.515573	1107.012097	16.223923
26.638049	1113.312729	16.228941
26.788909	1125.975255	16.233959
26.912244	1118.554785	16.238976
26.792907	1118.606558	16.243994
27.017464	1117.701613	16.249011
26.604622	1105.426420	16.254029
26.833739	1110.668829	16.259047
27.115333	1122.712804	16.264064
26.854721	1114.194003	16.269082
26.699607	1108.577995	16.274099
26.984518	1119.097872	16.279117
27.008088	1122.383210	16.284135
27.232012	1116.703807	16.289152
26.785368	1107.551790	16.294170
27.127217	1116.521336	16.299187
27.037109	1120.378688	16.304205
27.072486	1119.468967	16.309223
27.440954	1110.721209	16.314240
26.673004	1115.755340	16.319258
26.841146	1114.971577	16.324275
27.042866	1115.545550	16.329293
26.723642	1120.351173	16.334311
26.948989	1114.743972	16.339328
26.931559	1114.223324	16.344346
27.042755	1103.855816	16.349363
27.194937	1115.469742	16.354381
27.144809	1124.042260	16.359399
27.530815	1127.895675	16.364416
27.707723	1137.082007	16.369434
27.571507	1123.214837	16.374451
27.508947	1120.367555	16.379469
27.214929	1123.924564	16.384487
27.583500	1127.442311	16.389504
27.610684	1140.537982	16.394522
27.610519	1130.737363	16.399539
27.554781	1125.833930	16.404557
27.327697	1131.804498	16.409575
27.423698	1130.766202	16.414592
27.488824	1141.473010	16.419610
27.583112	1140.482240	16.424627
27.764574	1139.581701	16.429645
27.687839	1142.605381	16.434663
27.985670	1128.458202	16.439680
27.599861	1141.784712	16.444698
27.724829	1140.170763	16.449715
27.974400	1141.815472	16.454733
27.498420	1154.494808	16.459751
27.417525	1138.661437	16.464768
27.575496	1148.192245	16.469786
27.994446	1155.002253	16.474803
28.108212	1162.400756	16.479821
28.131060	1162.956037	16.484839
28.796780	1149.401994	16.489856
28.633228	1140.006852	16.494874
28.562770	1129.377800	16.499891
28.608998	1127.315545	16.504909
28.512816	1132.094730	16.509927
28.315978	1118.670689	16.514944
28.417903	1137.002490	16.519962
28.446320	1128.166365	16.524979
28.508957	1123.854645	16.529997
28.192624	1106.120378	16.535015
28.136744	1102.069688	16.540032
28.468488	1123.805226	16.545050
28.400020	1135.323564	16.550067
28.798013	1115.604906	16.555085
28.644910	1108.531157	16.560103
28.779623	1093.746193	16.565120
28.714374	1096.882910	16.570138
28.374233	1098.978364	16.575155
28.611305	1086.121570	16.580173
28.117957	1095.175196	16.585191
28.562814	1090.124797	16.590208
28.217592	1090.045224	16.595226
28.316251	1112.369850	16.600243
28.628718	1119.680981	16.605261
28.300229	1125.462112	16.610279
28.513535	1117.401522	16.615296
28.358725	1124.062008	16.620314
28.537354	1133.825977	16.625331
28.807004	1130.848285	16.630349
28.162684	1132.962411	16.635367
28.561987	1136.738425	16.640384
28.544261	1142.715538	16.645402
28.831131	1154.414190	16.650419
28.887822	1159.429380	16.655437
28.611677	1156.924268	16.660455
28.803925	1153.061054	16.665472
28.896836	1157.341912	16.670490
28.797064	1154.501990	16.675507
29.222238	1155.069926	16.680525
28.960378	1160.221916	16.685543
29.300478	1162.292897	16.690560
29.174584	1167.819910	16.695578
29.443527	1164.003393	16.700595
29.531324	1151.509134	16.705613
29.288138	1158.941373	16.710631
28.969943	1153.581577	16.715648
28.736850	1157.824890	16.720666
29.128599	1175.276324	16.725683
29.767599	1182.783988	16.730701
29.287839	1184.303868	16.735719
29.390450	1181.850756	16.740736
29.571580	1175.086764	16.745754
29.634849	1177.780897	16.750771
29.549659	1173.867337	16.755789
29.548096	1184.338813	16.760807
29.619297	1181.064976	16.765824
29.645736	1175.544354	16.770842
29.618089	1174.896668	16.775859
29.915742	1178.858477	16.780877
29.743135	1179.358847	16.785895
29.781737	1177.385644	16.790912
29.849594	1169.624386	16.795930
29.962937	1173.843194	16.800947
29.763580	1181.432325	16.805965
30.117536	1171.111428	16.810983
29.868441	1180.168993	16.816000
29.945798	1179.353467	16.821018
30.060729	1175.751906	16.826035
29.855669	1174.464446	16.831053
29.765509	1189.227617	16.836071
30.001746	1176.681502	16.841088
29.915259	1176.961663	16.846106
29.799184	1176.845972	16.851123
30.079607	1172.199631	16.856141
29.799813	1178.085674	16.861159
29.638415	1174.981200	16.866176
29.882181	1182.559278	16.871194
29.789927	1198.264888	16.876211
30.287101	1206.635075	16.881229
30.032257	1205.931058	16.886247
30.252284	1202.339974	16.891264
29.966316	1209.300630	16.896282
29.868109	1202.495655	16.901299
30.192188	1205.912552	16.906317
30.058951	1219.377457	16.911335
30.407678	1215.707502	16.916352
30.957918	1219.797413	16.921370
30.621847	1230.690249	16.926387
31.031272	1219.456596	16.931405
31.199522	1203.546318	16.936423
30.846023	1194.661038	16.941440
30.820134	1193.259549	16.946458
30.637131	1189.763799	16.951475
30.861157	1189.988414	16.956493
30.611187	1186.357738	16.961511
30.678244	1195.733616	16.966528
31.251423	1194.052647	16.971546
30.476535	1190.781642	16.976563
30.991225	1189.176927	16.981581
31.191344	1191.546757	16.986599
30.879862	1190.662005	16.991616
31.103272	1186.088125	16.996634
31.101744	1196.186786	17.001651
31.138300	1185.211184	17.006669
31.235851	1189.789298	17.011687
31.050157	1189.733207	17.016704
31.446481	1191.981848	17.021722
31.297163	1192.546849	17.026739
31.230884	1184.501986	17.031757
30.656411	1195.751729	17.036775
31.168007	1187.369492	17.041792
31.099853	1184.077085	17.046810
31.120581	1191.668223	17.051827
31.182794	1180.356486	17.056845
31.105038	1188.109259	17.061863
31.217775	1189.425550	17.066880
31.220881	1185.179217	17.071898
31.335523	1195.711699	17.076915
31.569228	1202.930452	17.081933
31.646998	1220.917958	17.086951
31.280643	1218.771121	17.091968
31.816988	1214.297577	17.096986
31.494814	1217.826217	17.102003
31.732354	1215.413664	17.107021
31.604027	1216.022812	17.112039
31.661194	1218.090435	17.117056
31.988208	1210.058929	17.122074
31.338742	1226.321723	17.127091
31.537764	1213.791213	17.132109
31.648132	1221.563915	17.137127
31.884645	1205.101368	17.142144
31.940706	1208.207710	17.147162
31.763298	1211.200893	17.152179
32.033605	1210.738714	17.157197
31.675801	1207.736558	17.162215
31.875236	1218.151029	17.167232
31.873445	1215.271977	17.172250
31.768287	1215.175337	17.177267
31.828440	1208.258216	17.182285
31.787483	1217.584739	17.187303
31.256197	1234.740459	17.192320
31.697558	1246.782779	17.197338
32.128462	1239.318612	17.202355
32.060180	1238.766256	17.207373
32.239077	1239.214112	17.212391
32.415608	1249.615483	17.217408
32.311452	1241.629639	17.222426
32.345291	1251.651595	17.227443
32.705467	1255.164469	17.232461
32.736767	1246.101429	17.237479
32.539383	1240.186112	17.242496
32.896468	1237.873367	17.247514
32.386190	1238.162549	17.252531
32.544896	1232.573862	17.257549
32.616300	1229.631463	17.262567
32.411767	1234.867252	17.267584
32.664915	1223.139514	17.272602
32.511523	1240.704459	17.277619
32.597637	1234.585734	17.282637
32.900285	1239.905332	17.287655
32.840954	1249.997494	17.292672
32.817232	1241.491217	17.297690
32.540485	1242.117554	17.302707
32.817155	1259.088624	17.307725
33.129328	1258.577754	17.312743
33.112949	1261.239078	17.317760
33.349574	1253.209975	17.322778
33.048042	1244.567987	17.327795
33.183431	1228.763927	17.332813
33.053404	1217.932913	17.337831
32.703018	1230.761508	17.342848
33.333163	1239.921783	17.347866
32.895372	1254.276671	17.352883
33.297411	1259.975410	17.357901
33.348652	1248.726074	17.362919
33.038314	1256.930118	17.367936
33.488638	1253.807025	17.372954
33.627665	1262.431249	17.377971
33.438310	1262.184042	17.382989
33.375530	1261.258738	17.388007
33.571237	1258.851556	17.393024
33.953182	1255.821320	17.398042
33.646147	1249.464401	17.403059
33.351813	1235.649392	17.408077
33.587670	1238.975059	17.413095
33.406104	1254.637304	17.418112
33.737220	1257.594401	17.423130
33.529667	1261.987823	17.428147
33.481694	1256.782676	17.433165
33.543182	1257.398859	17.438183
33.492846	1264.055426	17.443200
33.557603	1262.585325	17.448218
33.289539	1261.519344	17.453235
33.300589	1266.258308	17.458253
33.931195	1268.353460	17.463271
33.644762	1285.881516	17.468288
33.819961	1286.201253	17.473306
33.937914	1288.853247	17.478323
33.955792	1286.748834	17.483341
34.076193	1278.048905	17.488359
33.918822	1288.581385	17.493376
34.033871	1277.161981	17.498394
33.994092	1287.567835	17.503411
33.843337	1287.440978	17.508429
33.920962	1286.540367	17.513447
33.765249	1292.968801	17.518464
34.317123	1303.199956	17.523482
34.740225	1305.656360	17.528499
34.741467	1308.373029	17.533517
34.879643	1294.400260	17.538535
34.615754	1276.494487	17.543552
34.426708	1273.231209	17.548570
34.673200	1273.185961	17.553587
34.692591	1275.478365	17.558605
34.726301	1272.955592	17.563623
34.521850	1278.381137	17.568640
34.411398	1262.096664	17.573658
34.112492	1286.419823	17.578675
34.503246	1294.888452	17.583693
34.719448	1294.554155	17.588711
34.809508	1303.796752	17.593728
34.721172	1303.689048	17.598746
34.595099	1301.200306	17.603763
34.748140	1305.153508	17.608781
35.162106	1303.616309	17.613799
34.959938	1305.900661	17.618816
34.931420	1305.296025	17.623834
35.162106	1305.631737	17.628851
35.048358	1299.118661	17.633869
35.114187	1296.343704	17.638887
35.221990	1300.998491	17.643904
35.355766	1290.826703	17.648922
35.370329	1297.885474	17.653939
35.272921	1307.382845	17.658957
35.358534	1299.476450	17.663975
35.066560	1308.197528	17.668992
35.296339	1290.797857	17.674010
35.095548	1289.402202	17.679027
34.938131	1293.633762	17.684045
35.312605	1294.602242	17.689063
35.167483	1295.811799	17.694080
35.084889	1302.930420	17.699098
35.426839	1300.625299	17.704115
35.492094	1320.378712	17.709133
35.669794	1321.689336	17.714151
35.826354	1333.689299	17.719168
35.774199	1326.538045	17.724186
35.541828	1310.244258	17.729203
35.819110	1322.793025	17.734221
36.105584	1316.317751	17.739239
35.603985	1311.723392	17.744256
35.748784	1318.610533	17.749274
36.191756	1308.483798	17.754291
36.006838	1324.760821	17.759309
36.165843	1318.087448	17.764327
35.819454	1319.753277	17.769344
35.943557	1315.319875	17.774362
36.030781	1316.757736	17.779379
35.489891	1316.593362	17.784397
36.087715	1306.898748	17.789415
35.871755	1310.967608	17.794432
35.920677	1318.521447	17.799450
36.397661	1307.822938	17.804467
36.044464	1311.840202	17.809485
36.081285	1310.655830	17.814503
36.098164	1325.992264	17.819520
36.175637	1334.878717	17.824538
36.765642	1337.989646	17.829555
36.702128	1338.812034	17.834573
36.616522	1323.736708	17.839591
36.619516	1313.608295	17.844608
36.386463	1310.450350	17.849626
36.537919	1322.222421	17.854643
36.792462	1336.737504	17.859661
37.076194	1323.910553	17.864679
36.555461	1315.495106	17.869696
36.549641	1319.039691	17.874714
36.437587	1326.201800	17.879731
36.585876	1328.758605	17.884749
36.791042	1326.994305	17.889767
36.784944	1339.559083	17.894784
36.867949	1331.465317	17.899802
37.250654	1333.665852	17.904819
37.001465	1341.894422	17.909837
36.994747	1330.236958	17.914855
36.681034	1330.168287	17.919872
36.748198	1330.468187	17.924890
36.885435	1328.748640	17.929907
36.717343	1332.271775	17.934925
37.232834	1345.089619	17.939943
37.289091	1345.671637	17.944960
37.581917	1356.649794	17.949978
37.434716	1333.294832	17.954995
37.468903	1334.509628	17.960013
37.651826	1326.636257	17.965031
37.606445	1320.685410	17.970048
37.334217	1324.645914	17.975066
37.574388	1313.162776	17.980083
37.372295	1334.120046	17.985101
37.718397	1322.984242	17.990119
37.887008	1318.320615	17.995136
37.799955	1325.504158	18.000154
37.784360	1319.651506	18.005171
37.601107	1323.212591	18.010189
37.595453	1327.778766	18.015207
37.651301	1321.654407	18.020224
37.820798	1319.790135	18.025242
38.074558	1311.606584	18.030259
37.532847	1325.416626	18.035277
38.041516	1337.746246	18.040295
37.981082	1333.900182	18.045312
37.915844	1343.384354	18.050330
38.046561	1345.813379	18.055347
37.966104	1357.653154	18.060365
38.142380	1349.658046	18.065383
38.319381	1349.801901	18.070400
38.211863	1353.912590	18.075418
38.316133	1345.769221	18.080435
38.153937	1352.458590	18.085453
38.058756	1342.017746	18.090471
37.961887	1355.791281	18.095488
38.022199	1351.504687	18.100506
38.252053	1337.818599	18.105523
38.096966	1352.847431	18.110541
38.088193	1357.682234	18.115559
38.619930	1373.283132	18.120576
38.600786	1374.081219	18.125594
38.743821	1371.542228	18.130611
39.324559	1364.184591	18.135629
39.737494	1346.389075	18.140647
39.610529	1332.822529	18.145664
39.154609	1325.570277	18.150682
39.265083	1317.265268	18.155699
39.451535	1316.786709	18.160717
39.004984	1305.531485	18.165735
39.359315	1293.716407	18.170752
39.352193	1290.316200	18.175770
39.515461	1287.698272	18.180787
39.039050	1295.886240	18.185805
38.934077	1288.176874	18.190823
39.184627	1286.133787	18.195840
38.625810	1290.501742	18.200858
39.091631	1280.483821	18.205875
38.581777	1297.621088	18.210893
39.203081	1305.558512	18.215911
39.118937	1316.296155	18.220928
39.327213	1320.016567	18.225946
39.775380	1323.691204	18.230963
39.581731	1314.652126	18.235981
39.559064	1319.196718	18.240999
39.746233	1320.816780	18.246016
39.569101	1320.196688	18.251034
39.497982	1311.834857	18.256051
39.580469	1318.860697	18.261069
39.462207	1312.493635	18.266087
39.368328	1312.817938	18.271104
39.451361	1326.022985	18.276122
39.638821	1316.054849	18.281139
39.565678	1330.190940	18.286157
39.586292	1320.438319	18.291175
39.463933	1316.137608	18.296192
39.570427	1326.602638	18.301210
39.795598	1334.028770	18.306227
39.507346	1344.107075	18.311245
39.320192	1358.033407	18.316263
39.879333	1353.778076	18.321280
39.931009	1357.162725	18.326298
40.005265	1343.851693	18.331315
39.810288	1358.164352	18.336333
40.047530	1363.546044	18.341351
40.065859	1367.130326	18.346368
39.729519	1376.491865	18.351386
40.273288	1380.558881	18.356403
40.283607	1376.850648	18.361421
40.327864	1381.281776	18.366439
40.572918	1378.332928	18.371456
40.475850	1373.933512	18.376474
40.705787	1381.147465	18.381491
40.210038	1384.230990	18.386509
40.117018	1393.126916	18.391527
40.845943	1395.040004	18.396544
40.602462	1396.842669	18.401562
40.869082	1401.352197	18.406579
40.906878	1397.099646	18.411597
40.948573	1391.398464	18.416615
40.820880	1396.770744	18.421632
40.842691	1405.271620	18.426650
40.841665	1392.634060	18.431667
40.999529	1400.118653	18.436685
40.999445	1409.942026	18.441703
41.148952	1402.059604	18.446720
40.866885	1411.999133	18.451738
40.797794	1403.431805	18.456755
41.038823	1405.626764	18.461773
40.901286	1403.298961	18.466791
41.669661	1409.147495	18.471808
41.606348	1412.209940	18.476826
41.563854	1413.033169	18.481843
41.139893	1397.801021	18.486861
41.235613	1401.340559	18.491879
41.473890	1414.076193	18.496896
41.437613	1430.003829	18.501914
41.713174	1424.471634	18.506931
41.622876	1430.197542	18.511949
41.364406	1425.088345	18.516967
41.817426	1418.550704	18.521984
41.919670	1427.494903	18.527002
42.010215	1423.269010	18.532019
41.922757	1420.869891	18.537037
41.655707	1420.158443	18.542055
41.917826	1417.792560	18.547072
41.686081	1424.425805	18.552090
42.087263	1411.070615	18.557107
42.039870	1419.315293	18.562125
41.663597	1427.063077	18.567143
41.931198	1421.488900	18.572160
41.997860	1419.048813	18.577178
42.091742	1418.046676	18.582195
42.089950	1418.355676	18.587213
41.725781	1425.601857	18.592231
42.217618	1429.052339	18.597248
41.923088	1455.006088	18.602266
42.086787	1441.228938	18.607283
42.438785	1437.418236	18.612301
42.238552	1441.534121	18.617319
42.573106	1437.716081	18.622336
42.519045	1447.145311	18.627354
42.480215	1436.045844	18.632371
42.671091	1439.380606	18.637389
42.603553	1438.015151	18.642407
42.844839	1438.232178	18.647424
42.576362	1439.042575	18.652442
42.679841	1437.834517	18.657459
42.903652	1454.974033	18.662477
42.716526	1460.253066	18.667495
42.937165	1466.270213	18.672512
42.712648	1476.601781	18.677530
43.316019	1466.505371	18.682547
43.377511	1466.803461	18.687565
43.399042	1465.855077	18.692583
43.715270	1463.370355	18.697600
43.505452	1456.524764	18.702618
43.621961	1440.990941	18.707635
43.643655	1430.558564	18.712653
43.279165	1427.774003	18.717671
43.334759	1431.274156	18.722688
43.466573	1437.143461	18.727706
43.039391	1432.200093	18.732723
43.587267	1422.097974	18.737741
43.318168	1426.715836	18.742759
43.443678	1421.113702	18.747776
43.504729	1434.183523	18.752794
43.388733	1448.267003	18.757811
43.703215	1448.747448	18.762829
43.866181	1452.327002	18.767847
43.977529	1448.117329	18.772864
44.084641	1457.968978	18.777882
43.939201	1454.232678	18.782899
44.022114	1457.431455	18.787917
43.781317	1467.264950	18.792935
43.899514	1457.453113	18.797952
43.886072	1456.620382	18.802970
43.673752	1466.943618	18.807987
43.832166	1454.487771	18.813005
43.800333	1449.348379	18.818023
43.911098	1467.680679	18.823040
44.195294	1468.182299	18.828058
44.198017	1487.130594	18.833075
44.136296	1486.505486	18.838093
44.063600	1488.493550	18.843111
44.331312	1480.526878	18.848128
44.327138	1477.436761	18.853146
44.422362	1480.137841	18.858163
44.676016	1475.952540	18.863181
44.702218	1489.268349	18.868199
44.672530	1474.189489	18.873216
44.702397	1477.492752	18.878234
44.449768	1483.592500	18.883251
44.829136	1488.008120	18.888269
44.880243	1504.041385	18.893287
45.219619	1503.118124	18.898304
45.027108	1480.878314	18.903322
45.054520	1488.538171	18.908339
45.000663	1474.722741	18.913357
45.108974	1492.951545	18.918375
45.336113	1483.075130	18.923392
45.471360	1474.188770	18.928410
45.276783	1472.596400	18.933427
45.506854	1465.922177	18.938445
45.305808	1469.990568	18.943463
45.114228	1464.176559	18.948480
45.323316	1471.776292	18.953498
45.118849	1466.375830	18.958515
45.383152	1483.006300	18.963533
45.216522	1502.455975	18.968551
45.460471	1495.140866	18.973568
45.372850	1505.089869	18.978586
45.348653	1496.024489	18.983603
45.283554	1499.243937	18.988621
45.275303	1502.011036	18.993639
45.725688	1492.794344	18.998656
45.959746	1495.686913	19.003674
45.484406	1501.905570	19.008691
45.796647	1509.608647	19.013709
45.897174	1523.069216	19.018727
46.213619	1518.351433	19.023744
46.443188	1526.773359	19.028762
46.175639	1521.710913	19.033779
46.381784	1524.852216	19.038797
46.411981	1520.011932	19.043815
46.161451	1500.310809	19.048832
46.013846	1494.757584	19.053850
46.221801	1512.674582	19.058867
46.506373	1517.389817	19.063885
46.235531	1509.034697	19.068903
46.400023	1518.907950	19.073920
46.725223	1517.807915	19.078938
46.413316	1515.610647	19.083955
46.617662	1511.922495	19.088973
46.638203	1519.483118	19.093991
46.458425	1516.169429	19.099008
46.637119	1507.710857	19.104026
46.672425	1519.654742	19.109043
46.861080	1515.532988	19.114061
46.545092	1519.200427	19.119079
46.791688	1508.513695	19.124096
47.062319	1521.612535	19.129114
46.905111	1534.429746	19.134131
47.264514	1553.177506	19.139149
47.016686	1545.308294	19.144167
47.074975	1544.727804	19.149184
46.978500	1540.379028	19.154202
46.796079	1549.032821	19.159219
47.086209	1543.417456	19.164237
47.266470	1534.814912	19.169255
47.430376	1544.939848	19.174272
47.134419	1539.915188	19.179290
47.338757	1545.159109	19.184307
46.970948	1548.028492	19.189325
47.414622	1564.594593	19.194343
47.292089	1568.192491	19.199360
47.824135	1567.763572	19.204378
48.212954	1563.605388	19.209395
48.569431	1554.300726	19.214413
48.720686	1542.505826	19.219431
48.411658	1527.658768	19.224448
48.445048	1508.106112	19.229466
48.310135	1512.306039	19.234483
48.544538	1518.503591	19.239501
48.342225	1520.345883	19.244519
48.368984	1509.246879	19.249536
48.469418	1498.323823	19.254554
47.723695	1494.064067	19.259571
48.370757	1501.249695	19.264589
48.201019	1512.346179	19.269607
47.968641	1511.006932	19.274624
48.422148	1509.172993	19.279642
48.354173	1515.473554	19.284659
48.498923	1516.400311	19.289677
48.402461	1518.082888	19.294695
48.395516	1512.819262	19.299712
48.712456	1514.048101	19.304730
48.395131	1507.951045	19.309747
48.350137	1511.603364	19.314765
48.266650	1515.605773	19.319783
48.273393	1527.189460	19.324800
48.741662	1538.984632	19.329818
48.372291	1545.810483	19.334835
48.497276	1550.883346	19.339853
48.776203	1541.223479	19.344871
48.800468	1547.600453	19.349888
49.006033	1549.077328	19.354906
48.578840	1554.321883	19.359923
48.842165	1566.709000	19.364941
49.133265	1571.732609	19.369959
49.086928	1580.923634	19.374976
49.357056	1572.491562	19.379994
49.090566	1580.788881	19.385011
49.157223	1576.449202	19.390029
49.167541	1581.025002	19.395047
49.449313	1590.309136	19.400064
49.587032	1601.572297	19.405082
49.663990	1602.648119	19.410099
49.897377	1594.780005	19.415117
49.870748	1593.859696	19.420135
50.133369	1599.034108	19.425152
50.201495	1588.646662	19.430170
49.657369	1578.664122	19.435187
50.332426	1581.669632	19.440205
50.156749	1568.632223	19.445223
49.670797	1574.668030	19.450240
50.109426	1579.138788	19.455258
49.870880	1588.415698	19.460275
50.210370	1594.343065	19.465293
50.520625	1596.467887	19.470311
50.327151	1601.477948	19.475328
50.732612	1589.631709	19.480346
50.113045	1590.108345	19.485363
50.833957	1593.716460	19.490381
50.832441	1592.969139	19.495399
50.431060	1597.321641	19.500416
50.519806	1592.323181	19.505434
50.553473	1597.834457	19.510451
50.520605	1601.268644	19.515469
50.635383	1585.496780	19.520487
50.471829	1594.863984	19.525504
50.773217	1584.624384	19.530522
50.560659	1588.925029	19.535539
50.576236	1589.353978	19.540557
50.562177	1599.329004	19.545575
50.494460	1617.023047	19.550592
50.941643	1620.004233	19.555610
50.870251	1617.782331	19.560627
50.724357	1624.919493	19.565645
50.975642	1620.833364	19.570663
51.111950	1627.229544	19.575680
51.245533	1648.583411	19.580698
51.601654	1648.429788	19.585715
51.585292	1661.255977	19.590733
51.602746	1650.560775	19.595751
51.811507	1652.614679	19.600768
51.490106	1638.349482	19.605786
51.122530	1642.764488	19.610803
51.543792	1649.983382	19.615821
51.688755	1653.139604	19.620839
51.686726	1648.392430	19.625856
51.831850	1654.808810	19.630874
51.742084	1644.432214	19.635891
51.815615	1640.827584	19.640909
51.947393	1641.345881	19.645927
51.935036	1644.919186	19.650944
52.026013	1645.780086	19.655962
51.792855	1638.606802	19.660979
51.678781	1648.815407	19.665997
52.172397	1655.348274	19.671015
51.969072	1681.014805	19.676032
52.257796	1664.801359	19.681050
52.420701	1680.272927	19.686067
52.207479	1665.190525	19.691085
52.521980	1665.029253	19.696103
52.272035	1670.547927	19.701120
52.657183	1671.648516	19.706138
52.831828	1667.422359	19.711155
52.748706	1661.948906	19.716173
52.911380	1660.569972	19.721191
52.442536	1663.925846	19.726208
52.651762	1659.224660	19.731226
52.957726	1685.695519	19.736243
52.835713	1692.005132	19.741261
53.117914	1683.447374	19.746279
53.120180	1691.941420	19.751296
53.242990	1698.722939	19.756314
53.420769	1694.208068	19.761331
53.245443	1682.864971	19.766349
53.582022	1684.293314	19.771367
53.430338	1693.510182	19.776384
53.697106	1687.632116	19.781402
53.696271	1691.267689	19.786419
53.505751	1684.151469	19.791437
53.867778	1676.966649	19.796455
53.902977	1662.637833	19.801472
53.824496	1639.302088	19.806490
53.401641	1648.148649	19.811507
53.389304	1666.343773	19.816525
53.749589	1664.028467	19.821543
53.478127	1670.610544	19.826560
54.050150	1677.170154	19.831578
53.502950	1682.018166	19.836595
53.621795	1678.881186	19.841613
53.711412	1674.477429	19.846631
53.560127	1687.867395	19.851648
54.519692	1681.891120	19.856666
54.082335	1697.736086	19.861683
53.845160	1691.546896	19.866701
54.329447	1702.987569	19.871719
54.306097	1695.504195	19.876736
54.030511	1687.629287	19.881754
54.054149	1698.460698	19.886771
53.820717	1723.234676	19.891789
54.150279	1734.341248	19.896807
54.236932	1730.924966	19.901824
54.350611	1733.067123	19.906842
54.669521	1741.521957	19.911859
55.293935	1739.742264	19.916877
55.415838	1731.654817	19.921895
55.066625	1731.804637	19.926912
55.273454	1713.859099	19.931930
55.389813	1711.304409	19.936947
54.869390	1717.621980	19.941965
55.087767	1710.847628	19.946983
55.211619	1711.910546	19.952000
55.436118	1721.662934	19.957018
55.668385	1705.948192	19.962035
55.099825	1720.216581	19.967053
55.277257	1712.089600	19.972071
55.223528	1727.699581	19.977088
55.485740	1736.374462	19.982106
55.444173	1729.733854	19.987123
55.208649	1748.754348	19.992141
55.675262	1732.190404	19.997159
55.723570	1737.181191	20.002176
55.498665	1744.889802	20.007194
54.976522	1740.434944	20.012211
55.385344	1761.420785	20.017229
55.882312	1765.441355	20.022247
56.231354	1764.240886	20.027264
56.453107	1761.272611	20.032282
56.302990	1758.235827	20.037299
56.010343	1773.338322	20.042317
56.125940	1762.064138	20.047335
56.329252	1759.004047	20.052352
56.546742	1763.450983	20.057370
56.566913	1754.371779	20.062387
56.409928	1759.193545	20.067405
56.561388	1764.298299	20.072423
56.391781	1754.478988	20.077440
56.369316	1762.218529	20.082458
56.426789	1748.862300	20.087475
56.375469	1774.519078	20.092493
56.980011	1773.552520	20.097511
56.893515	1786.247951	20.102528
57.048396	1793.816695	20.107546
57.602234	1790.995585	20.112563
57.225750	1785.314152	20.117581
57.404097	1782.811745	20.122599
57.094615	1765.761794	20.127616
57.316887	1767.743390	20.132634
57.351551	1768.560113	20.137651
57.035090	1779.285901	20.142669
57.280555	1778.616814	20.147687
57.346039	1786.890958	20.152704
57.245881	1784.289957	20.157722
57.579574	1776.088155	20.162739
57.246819	1786.972953	20.167757
57.688569	1782.923631	20.172775
57.468431	1777.034329	20.177792
57.526970	1782.770276	20.182810
57.607044	1793.146707	20.187827
57.704425	1806.606865	20.192845
57.835527	1796.371018	20.197863
57.775361	1807.079819	20.202880
57.904010	1812.346253	20.207898
57.937577	1802.402201	20.212915
57.925996	1816.903698	20.217933
58.207110	1797.264232	20.222951
58.950863	1791.484019	20.227968
58.876433	1793.860990	20.232986
59.588207	1777.605463	20.238003
59.077637	1778.213199	20.243021
59.457998	1778.308301	20.248039
59.254972	1756.363934	20.253056
58.815747	1741.254845	20.258074
58.969198	1742.710086	20.263091
58.962898	1744.750927	20.268109
59.105119	1739.648652	20.273127
59.335206	1743.489951	20.278144
58.872237	1742.693725	20.283162
59.035173	1737.423837	20.288179
58.901378	1738.322886	20.293197
58.691210	1743.446790	20.298215
58.806558	1733.827769	20.303232
58.664668	1743.487915	20.308250
59.545996	1757.983085	20.313267
59.183757	1768.618442	20.318285
59.252684	1768.491684	20.323303
59.305639	1775.361224	20.328320
59.168531	1770.449455	20.333338
59.359065	1778.154392	20.338355
59.190275	1787.161561	20.343373
59.181795	1774.666265	20.348391
59.425726	1781.424148	20.353408
59.386552	1804.604960	20.358426
59.651001	1804.483501	20.363443
59.722200	1815.248428	20.368461
59.727852	1815.427066	20.373479
59.827215	1809.321266	20.378496
59.812462	1821.622127	20.383514
59.833116	1820.093950	20.388531
60.008117	1837.001453	20.393549
60.241617	1837.265451	20.398567
60.257295	1837.861712	20.403584
60.228434	1835.541372	20.408602
60.400638	1838.847435	20.413619
60.353544	1839.623813	20.418637
60.517111	1835.630160	20.423655
60.703331	1836.176424	20.428672
60.293062	1837.075759	20.433690
60.718963	1847.495539	20.438707
60.720265	1872.740191	20.443725
60.693982	1868.743829	20.448743
60.966319	1866.549804	20.453760
61.042312	1866.229745	20.458778
61.104331	1862.552961	20.463795
60.972836	1865.380765	20.468813
60.828994	1868.120857	20.473831
61.465208	1859.966765	20.478848
60.798291	1869.051255	20.483866
61.216453	1873.359360	20.488883
61.269307	1889.302970	20.493901
61.432841	1890.775841	20.498919
61.733272	1886.155886	20.503936
61.362857	1893.563162	20.508954
61.617509	1892.364198	20.513971
61.591815	1888.110647	20.518989
61.870424	1894.575415	20.524007
62.039938	1893.039419	20.529024
61.540731	1896.807080	20.534042
61.839091	1887.361486	20.539059
62.045628	1911.599652	20.544077
62.351621	1912.252785	20.549095
62.654413	1901.189909	20.554112
62.484740	1897.193749	20.559130
62.483908	1878.208125	20.564147
62.714939	1873.936715	20.569165
62.627865	1878.902804	20.574183
62.488966	1864.914152	20.579200
62.713123	1874.243466	20.584218
62.859504	1880.682566	20.589235
62.757991	1870.573124	20.594253
62.539968	1877.397587	20.599271
62.642578	1870.834532	20.604288
62.516595	1887.289357	20.609306
62.891235	1889.694072	20.614323
62.722880	1897.717768	20.619341
62.630874	1906.333898	20.624359
62.848283	1897.854114	20.629376
62.650675	1904.646456	20.634394
63.077489	1904.136202	20.639411
63.234767	1933.246764	20.644429
63.333946	1926.787011	20.649447
63.098659	1932.052553	20.654464
63.630030	1925.713100	20.659482
63.868530	1927.647926	20.664499
63.331009	1930.525110	20.669517
63.331722	1919.710850	20.674535
63.444298	1929.904806	20.679552
63.351417	1933.156914	20.684570
63.505367	1921.438838	20.689587
63.775588	1935.518809	20.694605
64.036442	1948.183416	20.699623
64.276398	1953.329037	20.704640
64.196326	1956.286500	20.709658
64.167017	1951.458333	20.714675
63.909279	1947.096480	20.719693
64.632779	1947.510936	20.724711
64.758592	1943.385340	20.729728
64.558992	1941.087061	20.734746
64.876767	1932.495695	20.739763
64.813306	1943.414981	20.744781
64.963077	1938.348394	20.749799
64.654948	1914.128745	20.754816
64.765570	1918.046636	20.759834
64.940450	1912.527853	20.764851
64.985247	1922.522832	20.769869
64.771263	1934.691146	20.774887
65.089256	1923.222971	20.779904
64.814681	1937.041910	20.784922
65.225122	1946.055269	20.789939
65.058278	1941.273191	20.794957
65.027045	1932.032741	20.799975
65.395786	1923.314012	20.804992
64.983070	1935.230708	20.810010
65.323099	1925.097456	20.815027
65.242324	1939.312929	20.820045
64.911027	1956.885811	20.825063
65.619229	1966.150484	20.830080
65.070789	1971.547217	20.835098
65.325286	1978.236501	20.840115
65.586870	1976.099760	20.845133
65.279039	1997.618414	20.850151
65.927322	2000.191843	20.855168
66.064991	2000.402873	20.860186
65.904086	2001.592665	20.865203
65.774147	2009.702555	20.870221
65.811995	2004.743525	20.875239
66.573356	2012.473790	20.880256
66.824129	2024.172411	20.885274
66.788302	2017.750019	20.890291
66.915981	1995.189324	20.895309
66.481427	2005.145517	20.900327
66.794555	1984.487888	20.905344
66.625610	1988.620764	20.910362
66.515653	2000.221443	20.915379
66.954714	2010.158435	20.920397
66.755707	2018.106972	20.925415
66.958255	2022.595837	20.930432
67.051478	2030.259591	20.935450
67.461540	2022.654028	20.940467
67.200010	2021.162492	20.945485
67.218950	2033.064610	20.950503
67.418826	2018.347465	20.955520
67.167456	2028.221260	20.960538
67.229866	2026.823525	20.965555
67.382902	2021.591407	20.970573
66.911476	2020.195778	20.975591
67.387035	2025.805421	20.980608
67.101499	2035.838444	20.985626
67.478979	2032.045018	20.990643
67.578488	2027.636368	20.995661
67.347521	2041.002479	21.000679
67.976862	2033.740393	21.005696
67.644441	2039.309124	21.010714
67.914132	2064.079164	21.015731
68.119662	2058.954846	21.020749
68.105240	2054.187166	21.025767
68.607666	2053.817887	21.030784
68.681921	2046.898443	21.035802
68.615858	2057.935172	21.040819
68.991352	2040.270285	21.045837
68.833266	2041.326933	21.050855
68.854138	2050.301946	21.055872
68.883792	2037.687501	21.060890
69.111548	2043.170617	21.065907
69.149690	2028.527191	21.070925
68.726651	2023.895147	21.075943
69.167398	2032.880292	21.080960
68.856504	2038.005283	21.085978
68.943511	2037.567248	21.090995
69.139825	2046.408770	21.096013
69.071980	2048.038615	21.101031
68.786858	2048.201800	21.106048
69.188807	2049.390573	21.111066
69.037647	2045.049562	21.116083
69.343996	2053.783430	21.121101
69.443326	2074.497114	21.126119
69.510884	2073.263482	21.131136
69.464878	2064.105724	21.136154
69.402127	2081.592776	21.141171
69.958899	2074.706122	21.146189
69.845236	2071.849046	21.151207
69.925333	2073.599584	21.156224
69.976026	2086.132694	21.161242
69.866551	2089.354915	21.166259
70.251463	2079.724739	21.171277
70.555128	2089.661450	21.176295
70.702490	2087.298399	21.181312
70.964125	2084.460052	21.186330
70.663212	2086.243597	21.191347
70.807564	2085.255866	21.196365
70.731051	2086.637940	21.201383
70.644040	2079.716936	21.206400
70.835132	2077.995445	21.211418
70.913333	2092.495272	21.216435
71.194327	2074.024388	21.221453
70.895320	2084.069917	21.226471
71.047993	2082.261502	21.231488
71.053693	2068.987226	21.236506
70.977828	2082.767364	21.241523
71.202041	2069.093776	21.246541
70.821453	2072.768928	21.251559
71.356723	2093.053490	21.256576
71.604493	2092.747006	21.261594
71.566134	2105.131937	21.266611
71.687834	2097.370322	21.271629
71.658573	2109.032476	21.276647
71.518917	2104.460399	21.281664
71.521181	2102.445873	21.286682
71.222452	2111.113796	21.291699
71.586689	2113.700199	21.296717
71.895565	2129.123941	21.301735
72.068253	2137.450143	21.306752
72.054794	2132.497237	21.311770
72.028036	2140.048700	21.316787
72.465403	2130.910964	21.321805
72.208946	2137.332867	21.326823
72.192846	2130.965417	21.331840
72.479723	2135.122973	21.336858
72.307382	2155.543720	21.341875
72.796779	2149.766281	21.346893
73.006276	2165.082164	21.351911
73.000403	2158.829541	21.356928
72.715442	2152.686296	21.361946
73.023759	2158.130473	21.366963
73.882450	2148.740026	21.371981
73.377667	2150.070838	21.376999
73.614403	2146.417314	21.382016
73.335275	2120.920847	21.387034
73.007700	2125.184847	21.392051
73.594563	2131.024461	21.397069
73.956175	2141.736233	21.402087
73.802561	2134.416818	21.407104
73.668776	2136.876541	21.412122
73.641564	2142.886325	21.417139
73.704750	2135.535603	21.422157
73.690105	2145.442179	21.427175
73.492376	2149.850357	21.432192
74.065648	2141.560122	21.437210
73.786970	2144.371490	21.442227
73.874744	2134.173725	21.447245
73.616812	2150.790917	21.452263
74.036404	2163.494676	21.457280
74.357185	2172.995124	21.462298
74.246997	2183.027053	21.467315
74.176422	2169.358273	21.472333
74.472868	2175.587907	21.477351
74.816166	2179.009313	21.482368
74.847051	2170.583608	21.487386
74.573979	2190.704602	21.492403
74.874704	2190.134586	21.497421
74.719788	2200.396798	21.502439
74.616779	2200.826180	21.507456
74.681576	2190.718025	21.512474
74.632412	2203.863113	21.517491
75.070386	2217.392223	21.522509
74.941880	2223.957466	21.527527
75.053707	2231.156408	21.532544
75.523646	2211.228340	21.537562
75.538302	2222.933675	21.542579
75.658642	2214.686391	21.547597
75.708648	2228.900474	21.552615
75.565034	2234.461912	21.557632
75.808470	2242.325615	21.562650
76.548996	2248.880698	21.567667
76.500004	2243.286797	21.572685
76.397294	2245.810272	21.577703
76.097591	2240.011575	21.582720
76.988640	2233.228752	21.587738
76.643986	2223.216969	21.592755
76.994961	2219.154277	21.597773
76.601520	2213.930235	21.602791
76.352994	2212.465258	21.607808
76.451428	2207.464205	21.612826
76.463187	2218.142438	21.617843
76.738834	2237.732921	21.622861
76.615616	2234.691178	21.627879
76.292620	2238.698537	21.632896
76.739086	2240.003946	21.637914
76.620382	2247.963664	21.642931
76.526613	2257.648416	21.647949
77.145148	2263.944246	21.652967
77.011998	2271.808737	21.657984
77.270293	2264.488916	21.663002
77.376495	2271.611250	21.668019
77.378939	2275.695245	21.673037
77.407198	2271.568846	21.678055
77.632478	2289.741353	21.683072
78.200358	2291.235650	21.688090
78.245064	2284.808031	21.693107
78.131202	2279.059146	21.698125
77.881213	2265.152769	21.703143
77.743827	2266.373318	21.708160
78.231401	2273.576764	21.713178
78.325811	2280.408141	21.718195
78.505918	2274.954505	21.723213
78.570094	2286.816229	21.728231
78.451175	2277.577153	21.733248
78.744331	2278.291888	21.738266
78.621320	2279.075393	21.743283
78.551403	2277.469307	21.748301
78.567821	2277.902072	21.753319
78.565308	2271.018122	21.758336
78.731405	2271.499635	21.763354
78.603034	2284.865834	21.768371
78.760261	2296.875098	21.773389
78.933271	2304.725340	21.778407
78.787638	2304.738963	21.783424
79.035521	2304.597815	21.788442
79.191950	2304.117132	21.793459
79.289402	2325.137376	21.798477
79.359471	2322.335942	21.803495
79.394857	2338.951833	21.808512
79.694074	2338.768295	21.813530
79.671573	2344.010029	21.818547
79.705363	2340.104353	21.823565
80.243023	2332.917999	21.828583
80.045967	2342.029007	21.833600
80.063625	2330.708088	21.838618
79.995810	2344.712717	21.843635
79.878144	2362.245827	21.848653
80.548883	2363.697052	21.853671
80.660638	2361.134753	21.858688
80.626141	2364.480794	21.863706
80.746158	2353.223952	21.868723
80.756624	2362.676479	21.873741
80.938185	2355.980017	21.878759
80.741476	2357.236810	21.883776
81.114467	2350.413651	21.888794
81.159529	2355.554001	21.893811
81.113191	2348.805650	21.898829
81.228674	2347.286071	21.903847
80.795991	2356.900827	21.908864
81.487132	2348.153087	21.913882
81.529582	2370.952271	21.918899
81.417610	2376.033290	21.923917
81.655394	2369.534571	21.928935
81.572589	2366.106940	21.933952
81.660047	2363.722306	21.938970
81.667841	2362.567483	21.943987
81.724415	2362.691600	21.949005
82.028361	2360.766279	21.954023
81.921888	2366.755463	21.959040
82.018236	2364.281159	21.964058
82.320937	2378.898280	21.969075
82.047122	2387.064167	21.974093
82.672541	2382.642034	21.979111
82.426584	2390.971803	21.984128
82.546086	2395.152520	21.989146
82.379581	2393.016000	21.994163
82.550039	2394.224769	21.999181
82.838900	2381.066165	22.004199
82.580419	2393.397748	22.009216
82.215549	2393.608441	22.014234
82.697600	2407.926482	22.019251
82.817563	2424.791017	22.024269
83.293949	2415.516313	22.029287
83.482867	2420.615453	22.034304
83.145337	2418.586882	22.039322
83.256468	2424.301727	22.044339
83.158733	2427.564587	22.049357
83.414244	2429.574213	22.054375
83.230877	2455.852112	22.059392
83.420529	2450.599198	22.064410
83.647938	2445.488048	22.069427
83.864930	2449.150592	22.074445
83.993141	2449.057679	22.079463
83.777744	2458.234404	22.084480
84.275832	2460.367112	22.089498
84.343677	2470.815717	22.094515
84.156095	2467.795649	22.099533
84.414279	2467.032687	22.104551
83.992012	2477.100920	22.109568
84.467140	2460.499356	22.114586
84.392158	2464.650207	22.119603
84.555505	2479.184277	22.124621
84.685989	2488.713002	22.129639
84.770302	2498.422247	22.134656
85.540534	2482.968907	22.139674
85.347962	2487.506249	22.144691
85.406090	2485.915477	22.149709
85.558300	2481.004221	22.154727
85.914742	2480.156423	22.159744
85.426562	2485.905139	22.164762
85.582777	2480.342012	22.169779
85.655525	2488.779110	22.174797
86.059795	2483.007036	22.179815
85.630926	2490.966453	22.184832
85.773959	2484.349176	22.189850
86.219165	2482.186183	22.194867
85.868286	2490.180279	22.199885
85.968467	2478.397095	22.204903
85.799764	2488.825573	22.209920
85.672470	2505.011968	22.214938
86.332674	2507.802807	22.219955
86.202951	2518.429953	22.224973
86.382126	2509.621533	22.229991
86.043791	2527.919876	22.235008
86.636796	2543.640922	22.240026
87.067944	2536.656044	22.245043
86.916152	2553.637537	22.250061
87.026018	2544.068929	22.255079
86.958403	2537.694126	22.260096
87.466488	2539.988183	22.265114
87.279605	2536.221497	22.270131
86.975695	2547.917418	22.275149
87.273361	2559.025950	22.280167
87.138745	2566.232930	22.285184
87.117983	2572.979636	22.290202
87.640650	2571.978218	22.295219
87.403680	2571.141628	22.300237
87.796362	2580.384699	22.305255
87.815859	2587.305830	22.310272
88.351654	2586.806977	22.315290
88.365400	2594.795650	22.320307
88.229945	2589.891220	22.325325
88.297407	2586.266119	22.330343
88.449328	2591.674234	22.335360
88.556134	2588.972557	22.340378
88.748877	2584.461244	22.345395
88.985295	2589.606092	22.350413
89.046858	2585.998508	22.355431
88.669689	2589.211773	22.360448
88.716389	2596.015783	22.365466
89.180148	2578.498620	22.370483
89.152108	2587.989969	22.375501
89.330651	2576.320072	22.380519
88.884213	2585.715984	22.385536
88.935634	2589.510413	22.390554
89.426774	2597.097689	22.395571
89.346166	2606.264698	22.400589
89.371867	2613.344266	22.405607
89.272225	2614.712119	22.410624
89.124855	2619.893986	22.415642
89.601175	2631.137848	22.420659
89.667712	2636.879475	22.425677
90.026869	2637.666728	22.430695
90.068610	2645.932284	22.435712
89.972263	2638.482635	22.440730
90.067664	2637.769160	22.445747
90.305347	2662.029310	22.450765
90.359275	2662.343642	22.455783
90.611426	2662.769921	22.460800
90.427290	2658.977945	22.465818
90.531380	2651.472931	22.470835
90.482572	2667.259423	22.475853
90.994525	2677.408761	22.480871
91.247047	2688.426458	22.485888
91.198218	2697.235073	22.490906
91.228435	2690.464401	22.495923
91.172632	2697.094142	22.500941
91.543534	2691.878353	22.505959
91.462058	2694.713741	22.510976
91.111998	2695.077101	22.515994
91.721699	2692.857215	22.521011
91.715401	2705.406595	22.526029
92.002390	2712.633740	22.531047
92.008743	2709.838494	22.536064
91.637281	2721.599317	22.541082
91.882802	2717.099668	22.546099
92.090378	2707.964352	22.551117
92.056979	2714.102950	22.556135
92.327095	2732.239390	22.561152
92.419931	2746.565732	22.566170
92.689043	2745.513524	22.571187
92.682382	2743.001553	22.576205
93.305984	2749.360132	22.581223
93.036934	2742.631691	22.586240
93.113962	2738.854564	22.591258
93.142846	2736.331962	22.596275
93.265768	2739.166463	22.601293
93.374521	2740.530404	22.606311
93.541197	2732.192072	22.611328
93.612183	2743.621100	22.616346
93.662301	2724.858270	22.621363
93.604726	2731.306028	22.626381
93.826153	2726.357207	22.631399
93.940265	2736.804602	22.636416
93.782357	2747.752353	22.641434
94.038672	2750.798559	22.646451
93.892593	2758.479606	22.651469
94.057081	2753.137461	22.656487
94.222909	2750.227905	22.661504
94.018775	2760.162031	22.666522
94.178873	2757.010893	22.671539
94.402733	2771.954496	22.676557
94.222653	2783.676867	22.681575
94.456683	2780.982362	22.686592
94.397602	2778.877544	22.691610
94.415316	2790.732019	22.696627
94.809814	2807.445433	22.701645
94.947244	2801.999888	22.706663
94.982760	2792.297807	22.711680
94.938542	2805.589439	22.716698
95.408241	2793.435536	22.721715
95.538003	2820.957756	22.726733
95.456662	2821.674122	22.731751
95.572113	2821.174642	22.736768
95.841758	2823.464666	22.741786
96.320953	2826.558498	22.746803
96.233447	2822.275591	22.751821
96.289289	2813.002822	22.756839
96.423555	2817.452476	22.761856
96.145124	2824.930735	22.766874
96.359987	2810.176886	22.771891
96.356269	2817.544523	22.776909
96.172699	2819.258250	22.781927
96.426155	2815.489976	22.786944
96.194380	2828.428522	22.791962
96.687311	2838.750823	22.796979
96.633503	2843.950287	22.801997
96.804634	2846.709469	22.807015
96.972366	2853.662387	22.812032
97.058291	2867.631700	22.817050
97.449395	2864.645707	22.822067
97.468697	2876.324775	22.827085
97.271723	2872.854978	22.832103
97.366365	2872.660942	22.837120
97.100449	2881.566371	22.842138
97.287443	2893.429409	22.847155
97.362799	2911.623229	22.852173
97.772004	2904.152039	22.857191
98.206852	2904.350314	22.862208
98.091307	2928.210889	22.867226
98.539042	2929.914210	22.872243
98.245927	2934.145139	22.877261
98.091487	2937.601792	22.882279
98.164153	2931.514165	22.887296
97.956576	2943.151455	22.892314
98.780080	2949.354054	22.897331
98.956053	2962.942321	22.902349
99.245449	2968.451352	22.907367
99.358614	2954.851354	22.912384
99.268665	2955.860908	22.917402
99.721152	2960.565221	22.922419
99.745662	2952.245279	22.927437
99.544178	2945.090926	22.932455
99.686232	2945.071306	22.937472
99.507330	2946.716944	22.942490
99.445102	2943.323958	22.947507
99.797931	2954.367304	22.952525
99.581564	2969.761447	22.957543
100.071397	2973.641391	22.962560
100.204469	2979.586276	22.967578
100.301436	2968.543466	22.972595
100.686579	2980.971714	22.977613
100.587305	2969.982776	22.982631
100.629948	2980.071714	22.987648
100.366647	2980.865179	22.992666
100.914590	2991.655245	22.997683
100.984557	3004.635137	23.002701
101.064110	3002.134389	23.007719
101.379003	2993.872080	23.012736
101.088238	2999.314532	23.017754
101.263752	3002.449419	23.022771
101.218985	2991.717568	23.027789
100.803625	2994.443524	23.032807
100.921496	2997.930533	23.037824
101.396864	3014.811059	23.042842
101.681496	3032.644629	23.047859
101.575892	3030.925882	23.052877
101.843208	3025.289370	23.057895
102.131883	3021.703397	23.062912
102.178867	3035.093856	23.067930
102.543654	3046.508142	23.072947
102.738925	3039.148431	23.077965
102.532596	3044.426856	23.082983
102.858154	3041.994283	23.088000
102.576565	3052.966344	23.093018
103.147646	3041.137160	23.098035
103.039707	3049.647112	23.103053
102.875604	3055.628025	23.108071
103.374032	3042.995498	23.113088
103.207642	3042.245977	23.118106
103.369607	3045.520142	23.123123
103.465478	3043.150150	23.128141
103.429409	3045.684727	23.133159
103.272019	3038.945475	23.138176
103.367772	3056.510832	23.143194
103.659846	3069.127859	23.148211
103.809136	3069.621643	23.153229
103.296951	3078.843720	23.158247
103.552362	3077.865034	23.163264
103.771244	3092.405411	23.168282
103.845938	3098.224993	23.173299
104.244387	3108.031245	23.178317
104.332400	3128.721047	23.183335
104.611280	3122.457334	23.188352
104.806360	3122.399372	23.193370
104.919414	3122.356224	23.198387
105.324677	3112.281844	23.203405
104.902240	3123.485645	23.208423
105.098250	3118.196410	23.213440
105.252624	3129.788649	23.218458
105.556760	3122.860844	23.223475
105.525262	3132.488542	23.228493
105.550717	3128.792731	23.233511
105.615578	3138.678851	23.238528
105.843525	3143.311472	23.243546
105.825834	3135.525259	23.248563
106.126743	3133.169215	23.253581
106.000529	3139.093858	23.258599
106.296045	3132.163150	23.263616
106.234116	3144.245319	23.268634
106.532411	3163.376085	23.273651
106.887271	3160.212975	23.278669
106.782982	3163.188076	23.283687
106.893907	3158.724451	23.288704
106.616919	3156.661700	23.293722
106.872196	3152.070929	23.298739
107.026105	3155.130690	23.303757
106.846457	3162.035561	23.308775
107.149133	3181.859378	23.313792
107.262635	3182.730797	23.318810
107.278269	3197.103064	23.323827
107.117637	3194.951281	23.328845
107.292098	3198.417118	23.333863
107.601045	3206.191285	23.338880
107.894987	3214.077408	23.343898
107.829621	3221.806691	23.348915
107.937799	3215.451613	23.353933
108.071014	3225.331547	23.358951
108.426693	3236.227758	23.363968
108.582230	3236.185424	23.368986
108.506896	3247.545429	23.374003
108.617817	3240.220903	23.379021
108.732580	3245.877175	23.384039
108.902167	3233.787768	23.389056
108.776965	3240.724968	23.394074
108.908759	3240.650749	23.399091
108.994380	3240.752329	23.404109
109.290746	3265.681286	23.409127
109.295911	3264.049626	23.414144
109.408204	3270.579622	23.419162
109.169727	3257.001968	23.424179
109.305990	3262.584195	23.429197
109.741612	3284.278341	23.434215
109.799550	3285.856306	23.439232
109.950870	3292.205007	23.444250
109.992186	3292.200948	23.449267
110.202675	3288.244015	23.454285
110.292550	3314.401565	23.459303
110.128107	3321.526440	23.464320
110.415253	3314.860846	23.469338
110.317862	3316.622515	23.474355
110.694189	3326.830651	23.479373
110.747509	3338.911930	23.484391
111.289432	3334.339619	23.489408
111.626921	3323.733403	23.494426
111.518885	3333.657435	23.499443
111.580178	3325.690269	23.504461
111.596367	3325.200971	23.509479
111.782237	3324.133818	23.514496
112.141386	3310.984409	23.519514
112.144144	3327.021290	23.524531
112.244737	3319.417316	23.529549
112.229028	3331.887261	23.534567
112.346011	3319.842753	23.539584
112.298550	3326.889917	23.544602
111.921966	3343.157193	23.549619
112.530349	3346.553317	23.554637
112.186235	3362.058059	23.559655
111.932261	3364.944283	23.564672
112.528996	3375.792265	23.569690
112.896991	3378.238880	23.574707
113.126022	3388.894015	23.579725
112.919483	3389.691060	23.584743
113.285396	3392.425846	23.589760
113.643887	3410.231825	23.594778
113.119416	3420.496795	23.599795
113.695016	3420.994163	23.604813
113.791640	3423.546517	23.609831
113.893932	3425.478185	23.614848
113.849430	3408.601308	23.619866
113.578829	3433.489306	23.624883
114.202625	3433.299464	23.629901
114.603606	3436.759211	23.634919
114.394626	3437.108588	23.639936
114.363491	3435.987717	23.644954
114.399283	3444.036947	23.649971
114.690491	3453.215900	23.654989
115.020703	3468.623256	23.660007
115.268100	3470.893845	23.665024
115.468668	3462.220719	23.670042
115.407612	3469.789156	23.675059
115.346964	3460.805861	23.680077
115.642259	3462.520008	23.685095
115.770750	3465.865186	23.690112
115.869190	3458.020139	23.695130
115.422248	3470.303957	23.700147
115.701621	3478.297764	23.705165
115.888539	3484.253581	23.710183
115.403593	3493.574533	23.715200
116.141628	3500.348707	23.720218
116.436654	3506.296411	23.725235
117.225751	3505.497543	23.730253
117.098985	3505.555278	23.735271
117.106856	3487.078110	23.740288
117.411989	3477.396159	23.745306
117.090113	3476.399986	23.750323
117.152048	3462.683638	23.755341
117.280550	3471.112003	23.760359
117.467828	3487.677891	23.765376
118.176780	3487.864096	23.770394
117.599913	3473.611309	23.775411
117.739341	3476.958215	23.780429
117.722484	3488.618552	23.785447
117.425305	3492.584136	23.790464
118.066927	3495.678677	23.795482
117.716822	3485.828808	23.800499
117.907295	3494.368160	23.805517
117.819270	3508.062198	23.810535
117.553235	3522.517402	23.815552
118.203756	3528.064271	23.820570
118.439987	3537.698913	23.825587
118.803925	3544.719546	23.830605
118.988443	3545.713845	23.835623
118.972897	3552.519562	23.840640
119.319111	3546.244097	23.845658
119.178372	3570.337816	23.850675
119.780360	3563.069344	23.855693
120.179813	3559.304194	23.860711
120.139826	3555.660894	23.865728
120.140885	3556.108848	23.870746
120.149187	3566.932690	23.875763
120.380356	3550.144115	23.880781
120.434485	3560.366967	23.885799
120.062827	3564.044126	23.890816
120.407476	3556.957806	23.895834
120.413707	3560.403645	23.900851
120.110507	3568.067100	23.905869
120.675313	3584.317571	23.910887
120.677243	3589.182000	23.915904
120.765399	3599.791392	23.920922
120.659708	3608.065815	23.925939
120.820466	3620.524778	23.930957
120.911199	3623.086807	23.935975
120.988473	3633.613374	23.940992
121.267251	3644.116307	23.946010
121.404387	3655.721253	23.951027
121.485867	3650.633176	23.956045
121.938377	3655.076254	23.961063
121.789131	3673.253556	23.966080
122.354570	3677.401465	23.971098
122.215305	3677.588456	23.976115
122.434115	3676.024018	23.981133
122.736374	3681.546917	23.986151
122.834489	3700.650184	23.991168
123.387630	3701.448181	23.996186
123.204468	3706.320962	24.001203
123.512064	3704.716174	24.006221
123.409099	3694.835340	24.011239
123.739825	3694.194537	24.016256
123.964835	3687.063467	24.021274
123.775519	3685.646386	24.026291
123.839376	3681.767665	24.031309
124.086206	3675.992972	24.036327
124.093772	3687.295814	24.041344
124.283900	3679.480307	24.046362
124.456068	3669.558887	24.051379
124.543407	3665.475064	24.056397
124.789039	3669.165034	24.061415
124.793538	3670.775544	24.066432
125.079388	3672.166839	24.071450
124.970963	3665.776305	24.076467
124.710617	3668.727036	24.081485
124.671022	3663.212567	24.086503
124.443135	3681.675419	24.091520
125.059683	3693.165682	24.096538
124.980183	3693.938086	24.101555
124.741418	3698.607482	24.106573
125.420310	3713.792553	24.111591
125.274808	3725.656749	24.116608
125.390117	3721.898223	24.121626
125.524102	3743.061178	24.126643
125.294452	3761.643722	24.131661
125.931491	3760.576379	24.136679
125.967486	3789.990919	24.141696
126.636209	3783.624754	24.146714
126.875648	3778.856491	24.151731
126.782468	3774.223434	24.156749
126.929934	3772.732268	24.161767
126.695119	3795.631978	24.166784
127.197710	3799.743509	24.171802
127.392981	3807.404175	24.176819
127.507210	3804.327389	24.181837
127.947529	3788.705525	24.186855
127.805992	3804.118371	24.191872
127.895629	3801.336258	24.196890
127.768649	3808.398429	24.201907
127.562647	3818.232734	24.206925
128.054693	3820.159927	24.211943
128.214489	3846.836343	24.216960
128.464906	3832.767837	24.221978
128.419747	3843.331429	24.226995
128.510238	3857.101632	24.232013
129.153038	3861.983287	24.237031
128.736135	3869.173200	24.242048
129.041552	3866.104400	24.247066
129.000658	3873.710238	24.252083
128.948670	3892.070081	24.257101
129.336398	3895.905018	24.262119
129.435355	3901.947669	24.267136
129.781873	3898.432606	24.272154
130.096776	3914.773777	24.277171
129.849044	3924.732421	24.282189
129.982473	3911.689321	24.287207
129.736157	3912.809577	24.292224
130.604699	3917.936844	24.297242
131.188896	3921.752133	24.302259
131.059410	3923.683791	24.307277
131.187880	3920.067932	24.312295
131.342030	3911.323128	24.317312
131.670866	3909.426958	24.322330
131.409139	3898.838425	24.327347
131.589776	3911.789262	24.332365
131.956118	3914.893018	24.337383
131.607712	3911.982865	24.342400
131.548338	3916.038580	24.347418
132.041062	3910.263890	24.352435
132.196024	3916.862274	24.357453
132.088596	3910.228529	24.362471
131.791206	3915.749572	24.367488
131.948265	3931.599206	24.372506
132.081758	3935.670521	24.377523
131.925697	3945.041036	24.382541
132.607917	3966.064758	24.387559
132.873400	3964.235809	24.392576
133.682652	3949.907776	24.397594
133.959768	3942.246997	24.402611
133.839982	3944.774762	24.407629
134.028687	3931.801210	24.412647
134.219795	3916.781335	24.417664
134.470405	3906.257678	24.422682
134.384792	3898.438665	24.427699
134.206357	3903.462315	24.432717
134.264550	3899.886883	24.437735
134.383579	3909.303407	24.442752
134.426936	3900.479370	24.447770
134.438619	3893.754176	24.452787
134.400078	3915.639824	24.457805
134.641687	3922.898703	24.462823
134.506363	3933.353701	24.467840
134.779394	3926.784302	24.472858
134.939947	3940.213760	24.477875
134.941449	3958.475412	24.482893
135.109156	3958.833471	24.487911
134.974538	3965.667423	24.492928
135.250258	3984.346984	24.497946
135.516652	3996.121675	24.502963
135.275354	3998.870061	24.507981
135.427354	4009.961709	24.512999
135.682453	4026.739765	24.518016
135.628080	4031.183314	24.523034
136.607946	4035.956645	24.528051
136.666472	4046.855555	24.533069
136.797134	4049.804775	24.538087
136.837641	4061.235109	24.543104
136.906092	4050.403784	24.548122
137.172813	4067.105138	24.553139
136.873004	4072.771539	24.558157
137.419935	4073.169355	24.563175
137.622634	4082.980011	24.568192
137.692171	4093.767660	24.573210
137.838820	4105.002804	24.578227
137.760832	4102.837553	24.583245
138.250410	4104.725424	24.588263
138.078059	4107.218637	24.593280
138.168699	4131.606706	24.598298
138.595325	4134.543379	24.603315
138.515371	4136.312480	24.608333
138.524447	4137.998272	24.613351
138.739085	4149.480848	24.618368
138.857099	4164.904075	24.623386
139.137565	4168.752573	24.628403
139.354447	4164.087958	24.633421
139.498506	4177.018318	24.638439
139.748566	4182.319329	24.643456
139.632753	4186.152569	24.648474
140.081698	4185.554317	24.653491
139.778461	4182.702758	24.658509
140.003995	4193.613394	24.663527
140.420429	4198.613494	24.668544
140.716081	4200.809628	24.673562
141.039279	4200.472465	24.678579
140.592080	4210.177386	24.683597
141.208585	4197.921225	24.688615
141.322502	4202.662890	24.693632
141.294879	4230.314158	24.698650
141.504601	4223.753975	24.703667
141.380855	4232.912174	24.708685
141.813277	4228.352295	24.713703
142.145484	4228.392431	24.718720
141.952108	4231.182508	24.723738
142.288600	4226.960665	24.728755
142.184572	4236.837745	24.733773
142.263907	4242.026967	24.738791
142.469505	4250.640611	24.743808
142.781358	4255.706147	24.748826
143.016922	4246.964166	24.753843
142.721994	4257.011584	24.758861
142.991490	4256.138380	24.763879
143.034035	4251.735421	24.768896
142.984180	4263.671544	24.773914
143.860395	4267.156463	24.778931
143.249714	4275.953015	24.783949
143.638544	4272.433596	24.788967
144.020069	4264.046148	24.793984
143.695708	4272.154865	24.799002
144.046581	4286.624811	24.804019
144.168743	4295.131853	24.809037
144.286876	4302.092874	24.814055
144.495015	4303.035654	24.819072
144.274253	4321.500436	24.824090
145.059064	4326.438577	24.829107
144.694432	4331.818945	24.834125
144.973280	4329.529002	24.839143
145.284733	4350.186836	24.844160
145.170365	4362.978769	24.849178
145.635349	4357.544014	24.854195
145.693196	4355.772757	24.859213
145.315115	4370.052052	24.864231
145.889715	4380.838662	24.869248
145.899907	4387.846796	24.874266
146.222726	4392.243520	24.879283
146.325984	4403.896785	24.884301
146.527344	4415.432952	24.889319
146.943391	4412.120825	24.894336
146.599001	4422.201768	24.899354
146.727755	4433.151492	24.904371
147.074620	4435.219445	24.909389
147.254847	4437.982127	24.914407
147.432157	4439.745131	24.919424
147.723887	4464.158973	24.924442
148.097229	4455.754671	24.929459
147.876108	4464.237733	24.934477
148.078381	4453.996198	24.939495
148.297963	4451.951558	24.944512
148.515202	4482.460692	24.949530
148.682039	4473.959178	24.954547
148.780577	4485.436093	24.959565
148.867536	4479.078912	24.964583
149.238100	4477.756547	24.969600
149.334482	4478.794298	24.974618
149.757911	4496.178850	24.979635
149.705974	4508.080853	24.984653
149.673045	4516.679940	24.989671
149.893724	4516.799252	24.994688
149.547623	4519.265092	24.999706
149.804322	4509.112131	25.004723
150.016164	4535.690114	25.009741
150.187645	4538.959864	25.014759
150.465266	4544.918736	25.019776
150.482480	4551.806071	25.024794
150.619395	4566.013354	25.029811
150.793143	4573.498416	25.034829
150.967823	4564.273379	25.039847
151.205283	4581.043148	25.044864
151.408607	4594.713347	25.049882
151.387597	4598.319873	25.054899
151.306152	4598.195638	25.059917
151.450269	4607.867120	25.064935
151.747869	4619.255140	25.069952
151.931072	4626.440179	25.074970
152.270195	4625.274235	25.079987
152.252838	4641.195705	25.085005
152.421332	4649.632237	25.090023
152.790041	4652.725119	25.095040
152.844629	4639.321616	25.100058
153.105687	4641.058126	25.105075
153.181236	4648.486301	25.110093
153.382225	4665.379565	25.115111
153.866038	4661.410342	25.120128
153.670967	4677.584254	25.125146
153.592577	4675.380401	25.130163
153.670595	4673.648284	25.135181
153.824829	4677.556475	25.140199
154.265136	4682.774066	25.145216
154.836988	4674.502833	25.150234
154.973871	4671.872588	25.155251
155.950770	4669.840685	25.160269
155.787802	4667.331933	25.165287
155.669126	4663.692787	25.170304
155.769832	4658.824064	25.175322
156.064868	4647.015534	25.180339
156.080761	4657.817998	25.185357
156.234162	4655.023565	25.190375
156.413659	4649.981881	25.195392
156.634423	4661.143288	25.200410
156.587959	4646.898938	25.205427
156.464917	4651.787221	25.210445
156.477373	4650.266823	25.215463
156.168011	4651.231039	25.220480
156.436414	4664.158073	25.225498
156.383255	4674.083676	25.230515
156.792546	4688.374179	25.235533
156.327359	4691.801734	25.240551
157.065277	4709.230346	25.245568
156.791005	4720.774108	25.250586
156.934255	4734.634760	25.255603
157.009705	4754.647181	25.260621
156.959234	4777.392075	25.265639
157.584739	4791.115149	25.270656
157.463478	4807.965246	25.275674
157.790440	4823.010635	25.280691
158.298137	4834.508809	25.285709
158.275229	4842.904009	25.290727
158.736584	4866.289316	25.295744
158.983556	4873.126800	25.300762
159.077824	4879.291104	25.305779
159.358764	4885.342486	25.310797
159.526950	4904.775014	25.315815
159.878382	4893.270375	25.320832
160.226903	4895.420810	25.325850
160.143720	4898.880225	25.330867
160.283759	4910.599422	25.335885
160.403052	4930.163752	25.340903
160.563697	4931.700403	25.345920
160.776256	4940.321146	25.350938
160.648774	4950.019070	25.355955
160.975962	4950.706629	25.360973
160.736580	4967.070125	25.365991
161.062820	4968.239828	25.371008
161.696731	4982.319224	25.376026
161.388968	4994.552351	25.381043
161.906902	4991.194823	25.386061
161.872312	4997.207323	25.391079
161.963709	5016.329062	25.396096
162.038188	5017.415381	25.401114
162.198627	5025.322640	25.406131
162.538039	5031.081629	25.411149
162.620975	5042.943510	25.416167
162.698453	5046.499121	25.421184
163.143052	5050.986055	25.426202
163.293094	5071.140846	25.431219
163.817144	5066.812799	25.436237
163.682927	5072.686732	25.441255
163.978957	5067.999644	25.446272
164.109980	5060.233834	25.451290
164.402833	5060.361636	25.456307
164.475711	5058.457068	25.461325
164.501305	5061.575544	25.466343
165.097883	5073.589155	25.471360
164.765113	5085.134240	25.476378
164.543063	5096.267154	25.481395
165.029407	5093.292885	25.486413
164.910144	5095.313949	25.491431
165.544136	5092.718379	25.496448
165.552369	5109.709518	25.501466
165.406847	5126.971945	25.506483
165.873613	5117.010507	25.511501
165.430109	5143.965400	25.516519
165.766141	5134.456473	25.521536
166.111416	5156.525004	25.526554
166.067173	5171.424493	25.531571
166.769626	5172.208795	25.536589
166.320959	5190.408463	25.541607
166.930969	5201.207087	25.546624
167.181567	5206.712338	25.551642
167.310466	5220.657710	25.556659
167.628194	5231.555326	25.561677
167.566899	5226.071478	25.566695
168.090765	5223.954914	25.571712
168.242925	5237.082877	25.576730
168.394877	5246.381718	25.581747
168.562388	5247.090312	25.586765
168.599824	5252.349050	25.591783
168.638985	5242.562546	25.596800
169.074024	5255.182790	25.601818
169.053670	5272.775835	25.606835
169.602581	5262.365129	25.611853
169.586051	5266.512125	25.616871
169.796831	5260.632587	25.621888
170.289736	5273.562197	25.626906
170.362880	5293.572537	25.631923
170.678572	5296.087617	25.636941
170.247165	5305.652756	25.641959
170.377778	5291.821802	25.646976
170.671182	5295.912580	25.651994
170.392309	5305.787879	25.657011
170.957726	5305.756982	25.662029
171.017930	5333.579888	25.667047
171.143561	5336.860576	25.672064
171.304884	5354.598364	25.677082
171.273133	5357.901270	25.682100
171.992957	5353.118476	25.687117
171.670762	5385.914761	25.692135
171.643791	5392.493988	25.697152
172.236462	5403.772906	25.702170
171.904419	5416.425445	25.707188
172.315213	5421.486737	25.712205
172.510174	5447.869022	25.717223
172.982040	5448.378988	25.722240
173.356744	5452.976888	25.727258
173.169749	5468.995902	25.732276
173.590482	5483.866466	25.737293
173.620280	5487.949116	25.742311
173.772436	5482.283221	25.747328
174.004412	5489.562938	25.752346
174.296959	5513.769568	25.757364
174.411532	5504.482301	25.762381
174.513957	5507.226598	25.767399
174.970464	5499.457683	25.772416
175.076679	5502.834566	25.777434
174.768284	5528.101137	25.782452
175.211953	5525.122068	25.787469
175.355544	5527.335785	25.792487
175.494361	5531.044343	25.797504
176.161465	5536.038668	25.802522
176.139493	5539.824351	25.807540
176.537107	5539.685875	25.812557
176.500811	5538.716139	25.817575
176.374156	5549.056173	25.822592
176.439660	5544.942808	25.827610
176.622673	5559.472540	25.832628
176.840474	5574.208366	25.837645
176.946758	5571.425540	25.842663
176.952995	5588.894805	25.847680
177.187132	5604.700639	25.852698
177.085526	5612.152405	25.857716
177.213695	5636.141598	25.862733
177.831792	5636.979325	25.867751
177.648597	5665.403236	25.872768
178.446448	5650.825512	25.877786
178.904017	5673.023389	25.882804
179.117904	5674.249621	25.887821
179.499553	5681.098160	25.892839
179.724748	5665.192399	25.897856
180.035781	5671.287917	25.902874
179.756504	5661.031893	25.907892
180.178476	5665.124246	25.912909
180.215137	5662.316743	25.917927
180.430062	5659.741101	25.922944
180.685670	5661.194313	25.927962
180.645390	5687.937427	25.932980
180.786366	5691.569269	25.937997
180.778064	5701.419544	25.943015
180.859016	5697.812358	25.948032
181.111832	5707.003351	25.953050
181.165531	5723.010982	25.958068
180.951391	5727.227163	25.963085
180.962470	5743.417530	25.968103
181.257722	5758.762859	25.973120
181.413052	5776.989641	25.978138
181.490383	5792.576776	25.983156
182.060744	5811.572640	25.988173
182.145352	5832.074007	25.993191
182.122683	5853.491878	25.998208
182.826652	5857.501195	26.003226
183.170906	5866.829096	26.008244
183.304879	5883.306349	26.013261
183.550954	5884.546152	26.018279
183.777379	5887.506981	26.023296
183.923973	5895.383112	26.028314
183.799558	5913.796728	26.033332
184.272388	5910.025928	26.038349
184.362263	5919.042494	26.043367
184.541785	5938.874517	26.048384
184.930047	5941.780111	26.053402
184.961592	5945.131692	26.058420
185.295170	5954.063678	26.063437
185.560924	5975.542480	26.068455
185.627812	5981.452643	26.073472
186.175550	5966.206557	26.078490
186.109332	5974.225991	26.083508
185.937520	5966.900710	26.088525
186.129784	5976.992706	26.093543
186.068713	5992.198205	26.098560
186.302089	5995.788773	26.103578
186.656381	6015.102748	26.108596
186.910015	6016.374386	26.113613
187.324812	6030.728996	26.118631
187.360983	6036.317426	26.123648
187.577324	6040.855966	26.128666
187.432013	6057.772037	26.133684
187.823074	6049.751456	26.138701
188.372628	6059.819580	26.143719
188.294881	6074.467150	26.148736
188.456757	6071.309548	26.153754
188.536917	6082.935603	26.158772
188.763890	6089.857280	26.163789
189.239090	6090.485647	26.168807
189.590967	6087.964366	26.173824
190.630943	6055.707478	26.178842
190.726605	6061.699528	26.183860
191.294247	6056.489728	26.188877
191.456614	6049.085252	26.193895
191.138054	6032.963879	26.198912
191.468030	6023.143535	26.203930
191.490497	6019.210471	26.208948
191.254319	6018.221935	26.213965
191.695531	6019.669547	26.218983
191.455990	6014.530872	26.224000
191.681826	6015.529103	26.229018
191.399950	6019.381715	26.234036
191.389746	6034.344884	26.239053
191.775414	6044.712743	26.244071
191.893111	6060.995197	26.249088
192.041715	6069.663419	26.254106
191.936312	6088.592328	26.259124
192.046296	6102.534536	26.264141
192.369471	6120.556614	26.269159
192.455141	6148.065617	26.274176
192.527573	6151.000100	26.279194
192.708464	6172.279040	26.284212
192.880230	6192.081167	26.289229
193.055239	6216.852652	26.294247
193.317416	6231.655756	26.299264
194.001422	6232.829123	26.304282
194.386945	6255.858132	26.309300
194.473848	6273.212359	26.314317
194.705051	6282.983033	26.319335
194.979943	6302.754773	26.324352
195.457866	6305.024104	26.329370
195.357343	6306.673600	26.334388
195.251346	6330.007284	26.339405
195.537168	6335.451947	26.344423
195.701035	6348.097652	26.349440
196.236409	6361.199896	26.354458
196.054417	6375.657921	26.359476
196.263100	6391.816118	26.364493
196.074368	6401.183276	26.369511
196.356998	6423.581408	26.374528
196.272548	6435.628101	26.379546
196.612603	6457.417353	26.384564
197.086485	6469.005839	26.389581
197.461613	6489.942605	26.394599
197.448658	6497.278453	26.399616
197.900941	6513.858638	26.404634
198.186729	6532.752220	26.409652
198.269639	6537.349306	26.414669
198.917663	6554.175833	26.419687
198.962900	6544.118931	26.424704
199.652103	6543.830398	26.429722
199.602082	6565.879947	26.434740
200.066806	6560.749309	26.439757
200.324475	6555.938201	26.444775
200.918204	6546.641595	26.449792
201.454221	6536.158955	26.454810
201.405012	6519.993904	26.459828
201.596522	6512.763952	26.464845
201.795804	6501.730808	26.469863
201.219997	6496.264271	26.474880
201.501351	6500.203780	26.479898
201.662392	6497.055685	26.484916
201.491037	6507.503801	26.489933
202.017763	6508.867940	26.494951
201.511748	6528.372749	26.499968
201.553521	6540.782127	26.504986
201.749414	6553.056425	26.510004
201.990357	6564.663996	26.515021
202.043011	6590.239307	26.520039
202.379313	6603.704850	26.525056
202.723546	6621.416035	26.530074
202.978491	6637.955103	26.535092
202.786496	6661.819469	26.540109
203.083465	6674.307057	26.545127
203.345986	6701.686031	26.550144
203.539205	6710.999360	26.555162
204.106223	6729.121030	26.560180
204.322505	6731.231474	26.565197
204.686860	6748.430639	26.570215
204.664069	6772.263118	26.575232
204.713722	6776.879977	26.580250
205.387396	6792.821910	26.585268
205.600017	6796.019136	26.590285
205.990474	6806.195304	26.595303
206.138107	6812.846141	26.600320
206.208356	6817.822696	26.605338
206.485225	6825.382278	26.610356
206.638074	6844.219557	26.615373
207.205664	6843.315595	26.620391
207.429536	6848.598235	26.625408
207.522163	6846.770512	26.630426
208.103313	6853.064994	26.635444
207.805129	6864.685962	26.640461
208.026947	6862.560307	26.645479
208.238408	6865.925510	26.650496
208.223105	6880.325579	26.655514
208.811550	6894.700960	26.660532
208.828951	6906.098602	26.665549
209.157562	6906.370928	26.670567
209.078035	6921.789113	26.675584
209.188222	6929.066105	26.680602
209.513506	6927.683336	26.685620
209.774544	6954.138288	26.690637
209.962959	6947.467100	26.695655
210.071714	6958.191121	26.700672
210.230655	6979.279455	26.705690
210.291677	6994.412856	26.710708
210.374198	7013.318732	26.715725
211.048169	7002.382805	26.720743
211.162789	7023.351749	26.725760
211.416243	7043.445405	26.730778
211.978412	7032.606012	26.735796
211.969542	7047.461218	26.740813
212.661151	7068.479282	26.745831
212.645219	7063.425198	26.750848
212.604019	7057.437997	26.755866
213.124844	7064.928017	26.760884
212.866890	7084.133148	26.765901
213.380133	7083.342965	26.770919
213.424270	7088.350724	26.775936
213.818564	7087.639378	26.780954
214.066636	7103.778368	26.785972
214.338763	7112.803929	26.790989
214.476475	7102.613946	26.796007
214.487084	7108.681963	26.801024
214.809955	7111.608096	26.806042
214.674497	7114.838017	26.811060
214.769264	7134.642302	26.816077
215.241023	7141.556065	26.821095
215.167203	7156.614355	26.826112
215.158680	7171.262463	26.831130
215.447518	7179.203820	26.836148
215.686011	7198.701533	26.841165
215.872169	7203.432102	26.846183
216.297602	7236.219839	26.851200
216.370285	7246.761008	26.856218
216.401628	7258.399189	26.861236
216.661987	7286.857067	26.866253
216.819585	7284.163875	26.871271
217.229269	7308.614515	26.876288
217.552079	7319.931777	26.881306
217.992324	7323.907322	26.886324
218.075664	7336.796410	26.891341
218.297020	7353.248073	26.896359
218.573152	7364.507747	26.901376
218.582905	7382.074501	26.906394
219.224893	7384.893314	26.911412
219.223081	7411.055576	26.916429
219.582822	7420.949743	26.921447
219.951752	7410.543131	26.926464
220.257741	7439.385177	26.931482
220.505799	7449.820937	26.936500
220.539641	7455.122751	26.941517
220.516711	7461.947134	26.946535
220.884710	7466.984697	26.951552
220.985340	7481.420398	26.956570
221.248182	7485.719264	26.961588
221.476470	7515.270668	26.966605
221.660692	7518.799650	26.971623
222.258988	7521.512322	26.976640
222.089093	7540.239425	26.981658
222.467205	7549.729689	26.986676
222.776497	7562.095417	26.991693
222.998579	7563.745002	26.996711
223.243189	7583.876259	27.001728
223.151318	7593.116959	27.006746
223.645514	7591.580829	27.011764
223.508198	7620.572477	27.016781
223.671649	7617.950725	27.021799
223.892483	7648.596926	27.026816
224.246915	7657.620939	27.031834
224.562619	7665.377696	27.036852
224.322169	7696.619720	27.041869
225.161929	7700.830667	27.046887
225.609428	7710.745881	27.051904
225.457113	7726.747229	27.056922
225.966171	7742.244071	27.061940
225.930188	7744.927473	27.066957
226.344007	7762.191203	27.071975
226.617089	7778.092778	27.076992
226.752110	7786.981602	27.082010
227.251181	7786.048020	27.087028
227.430066	7801.179935	27.092045
227.612058	7799.808300	27.097063
227.550375	7802.528277	27.102080
228.075806	7821.924729	27.107098
228.335204	7823.168780	27.112116
227.910472	7833.873328	27.117133
228.067812	7851.678383	27.122151
228.359686	7854.736626	27.127168
228.734551	7888.618775	27.132186
229.550741	7877.237995	27.137204
229.540457	7886.262870	27.142221
229.903809	7906.344086	27.147239
230.220869	7894.524764	27.152256
230.479875	7910.399666	27.157274
230.467889	7904.464795	27.162292
230.649186	7920.732290	27.167309
230.580513	7930.534903	27.172327
230.714717	7927.911658	27.177344
230.851132	7970.409329	27.182362
231.455806	7961.914339	27.187380
231.611014	7987.417356	27.192397
231.955425	7997.620061	27.197415
232.197626	8006.114676	27.202432
231.876375	8028.386976	27.207450
232.425977	8032.228739	27.212468
232.456800	8051.676930	27.217485
232.535342	8066.108166	27.222503
233.226778	8085.608120	27.227520
233.297333	8094.602352	27.232538
233.454725	8123.814559	27.237556
234.114617	8119.683695	27.242573
234.278736	8141.894414	27.247591
234.618088	8152.118541	27.252608
235.093412	8161.688334	27.257626
235.479395	8183.533773	27.262644
235.692738	8187.608679	27.267661
235.738813	8188.094973	27.272679
235.897814	8182.985473	27.277696
236.320794	8197.887372	27.282714
236.302901	8209.831397	27.287732
236.870861	8216.494911	27.292749
237.007473	8240.844266	27.297767
237.034945	8236.033880	27.302784
236.967668	8248.500520	27.307802
237.184712	8243.780731	27.312820
237.865105	8260.271286	27.317837
237.991889	8265.391719	27.322855
238.337898	8274.787713	27.327872
238.807156	8276.983159	27.332890
238.951086	8276.534715	27.337908
239.302209	8287.753440	27.342925
239.609163	8305.622370	27.347943
239.920320	8300.224454	27.352960
240.211687	8304.081620	27.357978
241.245059	8280.389407	27.362996
241.340892	8276.282113	27.368013
241.146757	8279.728400	27.373031
241.795446	8269.019531	27.378048
241.665846	8276.095938	27.383066
241.587179	8272.969992	27.388084
241.852453	8270.127198	27.393101
241.796782	8271.702486	27.398119
242.102662	8283.872414	27.403136
242.271851	8305.111260	27.408154
242.330733	8307.880611	27.413172
242.529778	8321.832029	27.418189
242.400111	8330.285411	27.423207
242.559539	8340.801865	27.428224
242.694320	8361.874779	27.433242
242.872682	8385.161868	27.438260
243.135222	8396.348912	27.443277
243.325300	8423.570379	27.448295
243.463290	8437.869190	27.453312
243.609544	8460.056539	27.458330
243.785458	8477.487400	27.463348
244.347366	8501.969728	27.468365
244.256699	8529.141917	27.473383
244.677401	8535.091927	27.478400
244.737700	8562.822013	27.483418
244.998687	8586.892067	27.488436
245.194003	8607.137578	27.493453
245.481906	8631.567162	27.498471
246.034251	8641.207950	27.503488
246.242098	8664.154182	27.508506
246.695095	8684.006434	27.513524
246.929536	8691.854395	27.518541
246.804995	8717.091536	27.523559
247.679412	8715.207760	27.528576
248.375893	8736.729813	27.533594
248.825273	8721.886597	27.538612
248.976765	8732.318764	27.543629
248.875961	8735.619663	27.548647
249.664652	8753.613872	27.553664
249.612393	8756.713713	27.558682
249.633887	8754.265822	27.563700
250.302694	8769.892316	27.568717
250.316549	8784.121470	27.573735
250.533746	8786.532173	27.578752
250.711663	8793.603405	27.583770
250.987798	8810.364937	27.588788
251.267098	8826.157819	27.593805
250.762324	8838.774805	27.598823
251.470868	8848.734803	27.603840
251.592677	8860.772691	27.608858
252.036390	8890.566568	27.613876
252.210657	8898.388392	27.618893
252.260533	8907.473171	27.623911
253.058008	8906.123651	27.628928
253.215772	8928.745365	27.633946
253.417948	8942.439211	27.638964
253.575262	8950.435608	27.643981
253.544238	8980.040689	27.648999
253.913938	8974.959741	27.654016
254.182364	9015.847785	27.659034
254.300726	9010.784951	27.664052
254.793302	9035.763302	27.669069
254.706676	9055.530788	27.674087
255.160901	9067.497849	27.679104
255.423226	9087.973102	27.684122
255.772634	9100.886372	27.689140
256.169304	9108.210509	27.694157
256.139654	9133.182032	27.699175
256.330536	9146.453324	27.704192
256.554213	9167.761465	27.709210
256.925993	9182.821681	27.714228
257.069169	9188.005073	27.719245
257.171131	9213.534650	27.724263
257.669368	9214.482322	27.729280
258.151067	9247.186078	27.734298
258.570275	9252.262973	27.739316
258.786955	9273.494428	27.744333
258.827753	9293.307997	27.749351
259.138850	9297.940447	27.754368
259.607706	9312.635675	27.759386
259.680999	9323.560185	27.764404
259.918730	9335.541358	27.769421
260.082624	9360.686689	27.774439
260.255871	9376.446529	27.779456
260.379054	9383.541297	27.784474
260.787171	9409.099886	27.789492
261.527773	9416.641958	27.794509
261.622677	9437.720552	27.799527
261.862171	9448.790846	27.804544
261.976184	9458.139429	27.809562
262.050229	9480.523742	27.814580
262.655004	9474.440129	27.819597
262.529393	9501.442520	27.824615
263.002147	9508.651790	27.829632
263.652777	9519.528570	27.834650
263.716140	9529.555224	27.839668
264.312400	9535.902635	27.844685
264.178735	9555.171220	27.849703
264.461743	9559.321562	27.854720
264.648925	9571.835975	27.859738
264.581816	9582.119098	27.864756
265.194209	9584.440632	27.869773
265.314307	9610.248280	27.874791
265.218771	9632.186732	27.879808
265.435351	9645.130388	27.884826
265.778692	9677.954122	27.889844
265.900318	9686.457850	27.894861
266.299912	9706.772439	27.899879
266.544438	9729.205979	27.904896
267.127769	9747.025092	27.909914
266.988215	9762.934179	27.914932
267.392855	9777.043357	27.919949
267.746476	9794.457158	27.924967
268.192325	9816.300402	27.929984
268.503141	9832.549903	27.935002
268.607885	9855.312509	27.940020
268.996408	9877.260683	27.945037
269.297997	9889.152094	27.950055
269.578781	9909.922333	27.955072
269.654373	9916.732969	27.960090
269.897225	9944.261800	27.965108
270.657407	9967.173282	27.970125
270.400598	9990.254545	27.975143
270.504464	10000.952276	27.980160
271.021294	10025.939174	27.985178
271.376718	10049.404884	27.990196
271.861090	10055.157391	27.995213
272.833252	10058.001418	28.000231
273.472239	10056.437076	28.005248
273.886077	10048.021548	28.010266
273.747904	10076.661693	28.015284
274.240679	10083.408606	28.020301
274.498979	10082.120216	28.025319
274.740330	10085.302310	28.030336
274.844550	10076.809006	28.035354
274.508807	10088.702459	28.040372
274.799041	10104.099306	28.045389
275.124629	10115.689106	28.050407
275.293671	10133.378951	28.055424
275.455397	10152.744921	28.060442
275.280227	10175.719137	28.065460
275.746785	10185.514562	28.070477
275.865484	10209.947093	28.075495
276.292016	10224.569836	28.080512
276.630877	10238.700591	28.085530
276.768966	10274.744790	28.090548
277.030304	10274.760509	28.095565
277.429101	10315.780680	28.100583
277.546894	10331.701146	28.105600
277.913513	10347.636224	28.110618
278.653833	10361.144976	28.115636
279.759140	10339.186772	28.120653
280.650437	10339.104924	28.125671
280.575516	10328.679572	28.130688
281.073029	10327.640553	28.135706
281.040653	10321.174031	28.140724
281.371557	10323.610197	28.145741
281.777888	10321.495195	28.150759
281.626273	10322.647018	28.155776
281.985937	10310.218529	28.160794
282.211003	10315.443830	28.165812
282.568642	10311.029392	28.170829
282.200588	10307.261781	28.175847
282.411817	10326.753667	28.180864
282.539025	10333.996298	28.185882
282.790298	10352.624412	28.190900
282.783494	10366.583451	28.195917
282.916197	10379.057125	28.200935
283.177021	10399.643025	28.205952
283.494019	10415.182261	28.210970
283.456921	10447.927390	28.215988
283.974807	10468.983547	28.221005
283.817674	10481.045360	28.226023
284.147508	10506.483987	28.231040
284.449743	10534.346671	28.236058
284.603658	10564.922916	28.241076
284.803697	10590.209916	28.246093
285.325196	10611.541402	28.251111
285.747430	10646.750605	28.256128
286.221649	10670.502381	28.261146
286.449354	10692.950305	28.266164
286.464735	10713.965000	28.271181
287.154973	10736.266812	28.276199
287.221287	10764.484224	28.281216
287.989390	10777.270990	28.286234
288.324203	10793.903522	28.291252
289.154042	10813.482308	28.296269
289.368210	10821.837331	28.301287
289.250238	10843.139852	28.306304
289.732010	10861.523846	28.311322
289.715999	10870.930306	28.316340
290.146935	10891.377487	28.321357
290.413012	10905.777761	28.326375
290.485897	10936.164120	28.331392
291.037757	10945.495190	28.336410
291.342465	10961.176445	28.341428
291.725727	10970.604870	28.346445
292.263541	10989.899913	28.351463
292.055172	10998.712848	28.356480
292.650678	11022.947647	28.361498
292.895570	11040.742491	28.366516
293.309264	11052.236395	28.371533
293.269297	11067.316367	28.376551
293.620847	11081.574966	28.381568
293.742473	11101.276487	28.386586
294.186266	11133.999842	28.391604
294.409461	11142.403954	28.396621
294.770571	11149.359130	28.401639
295.101212	11160.851152	28.406656
295.740686	11185.954995	28.411674
295.826238	11204.490295	28.416692
296.062916	11213.363347	28.421709
296.181534	11231.245560	28.426727
296.500496	11255.491986	28.431744
297.010197	11262.855852	28.436762
297.339450	11281.401178	28.441780
297.866766	11291.748151	28.446797
299.187438	11265.554374	28.451815
299.265226	11274.482220	28.456832
299.479700	11264.049943	28.461850
299.738645	11287.683973	28.466868
300.085844	11299.783154	28.471885
300.368499	11296.108900	28.476903
300.194431	11304.935211	28.481920
300.714894	11297.764281	28.486938
300.708368	11296.786882	28.491956
300.721708	11313.243301	28.496973
301.353223	11328.267115	28.501991
301.254615	11342.868606	28.507008
301.483173	11339.174966	28.512026
301.242381	11363.281336	28.517044
301.476824	11372.841873	28.522061
301.578691	11392.981939	28.527079
301.731936	11430.183589	28.532096
302.277590	11459.502820	28.537114
302.427576	11486.968566	28.542132
302.657314	11503.820985	28.547149
303.145238	11531.607272	28.552167
303.539412	11559.955971	28.557184
303.969953	11574.039580	28.562202
304.097800	11599.320458	28.567220
304.552828	11627.030434	28.572237
304.877856	11634.932550	28.577255
304.878440	11672.949579	28.582272
305.252741	11691.538318	28.587290
305.705491	11722.064747	28.592308
306.128335	11738.886907	28.597325
306.767498	11756.711589	28.602343
306.960941	11794.110673	28.607360
307.810434	11791.870653	28.612378
308.209427	11803.682694	28.617396
308.467354	11815.004473	28.622413
309.081246	11826.787135	28.627431
308.809547	11852.722553	28.632448
309.287206	11868.814031	28.637466
309.469497	11867.124488	28.642484
309.689007	11886.248147	28.647501
310.299433	11899.462260	28.652519
310.599886	11904.577857	28.657536
311.134047	11923.920326	28.662554
311.206918	11942.220633	28.667572
311.454498	11948.329903	28.672589
312.065246	11958.353014	28.677607
312.054599	11972.072192	28.682624
312.440212	11990.615275	28.687642
312.653482	12010.904638	28.692660
312.661812	12034.155926	28.697677
313.018993	12032.768232	28.702695
313.910654	12040.543324	28.707712
314.591489	12045.684020	28.712730
315.166861	12057.161241	28.717748
314.965798	12071.452639	28.722765
315.244128	12072.295210	28.727783
315.466236	12083.506518	28.732800
315.533446	12096.191740	28.737818
315.710559	12103.633308	28.742836
315.852542	12125.220524	28.747853
316.311777	12130.971659	28.752871
316.414264	12156.408899	28.757888
316.441531	12181.437929	28.762906
317.250293	12204.614795	28.767924
317.100077	12233.428583	28.772941
317.256442	12253.485026	28.777959
317.475965	12288.398986	28.782976
317.758302	12312.530167	28.787994
317.922572	12338.636614	28.793012
318.061645	12383.937892	28.798029
318.346189	12410.150540	28.803047
318.918141	12441.347169	28.808064
319.103659	12475.622658	28.813082
319.741619	12507.791780	28.818100
320.106024	12529.142449	28.823117
320.940417	12537.121128	28.828135
321.511265	12566.015853	28.833152
322.078849	12559.977469	28.838170
323.230805	12565.564833	28.843188
322.766786	12578.319770	28.848205
323.549914	12573.859258	28.853223
323.595921	12581.024988	28.858240
324.058979	12574.956687	28.863258
324.288352	12580.443605	28.868276
324.135972	12590.352778	28.873293
324.412836	12603.808835	28.878311
324.336028	12619.980565	28.883328
324.828905	12645.468756	28.888346
324.793115	12646.552646	28.893364
324.859785	12674.579496	28.898381
325.338193	12696.626893	28.903399
325.866316	12724.712696	28.908416
326.162169	12741.946240	28.913434
326.423529	12763.585387	28.918452
326.291335	12783.906317	28.923469
326.851291	12814.177463	28.928487
327.174751	12841.594624	28.933504
327.725896	12874.530595	28.938522
327.964799	12896.217775	28.943540
328.121669	12928.768649	28.948557
328.727049	12949.572402	28.953575
329.267735	12973.636435	28.958592
330.000179	12991.933941	28.963610
330.359293	12997.884826	28.968628
330.480099	13021.746050	28.973645
331.077370	13044.478604	28.978663
331.285212	13059.471983	28.983680
331.504681	13078.704217	28.988698
331.813833	13090.960774	28.993716
331.612915	13118.723962	28.998733
331.984686	13134.378852	29.003751
332.650796	13164.976567	29.008768
332.679223	13188.093788	29.013786
333.643227	13210.382705	29.018804
333.483703	13224.403457	29.023821
333.920281	13258.976139	29.028839
334.009685	13272.985523	29.033856
334.371066	13317.155623	29.038874
335.049052	13336.633484	29.043892
335.135528	13362.259653	29.048909
335.483735	13381.243924	29.053927
335.764821	13412.263803	29.058944
336.118227	13440.444482	29.063962
336.536059	13450.462750	29.068980
336.932475	13483.359470	29.073997
337.495641	13496.697789	29.079015
337.788627	13512.087187	29.084032
338.557090	13525.646731	29.089050
339.297405	13540.697087	29.094068
338.955230	13567.885639	29.099085
339.744912	13574.031548	29.104103
340.198265	13587.840485	29.109120
339.919079	13612.284358	29.114138
340.658361	13612.635965	29.119156
340.413999	13636.965348	29.124173
341.682929	13627.932362	29.129191
342.215932	13637.219279	29.134208
342.199268	13642.025637	29.139226
343.082699	13641.291099	29.144244
343.193753	13665.265203	29.149261
343.662993	13672.408387	29.154279
343.911515	13671.579169	29.159296
343.644923	13687.781908	29.164314
345.089760	13673.605658	29.169332
345.508890	13682.010064	29.174349
345.702903	13680.490171	29.179367
345.868060	13678.016884	29.184384
345.989501	13675.884964	29.189402
345.938837	13674.129922	29.194420
346.113773	13675.188330	29.199437
346.593986	13677.524568	29.204455
346.722835	13688.739871	29.209472
346.631817	13697.389778	29.214490
346.915450	13720.113919	29.219508
346.974746	13750.555082	29.224525
347.231979	13772.435806	29.229543
347.847680	13792.866999	29.234560
347.926365	13816.429068	29.239578
348.588837	13844.499220	29.244596
348.423860	13882.876719	29.249613
348.751908	13916.173364	29.254631
349.013493	13941.038518	29.259648
348.957135	13980.618022	29.264666
349.862558	14004.534739	29.269684
350.067465	14032.466887	29.274701
350.294916	14056.718519	29.279719
350.780422	14093.975086	29.284736
350.949509	14128.635024	29.289754
351.681960	14147.707659	29.294772
351.835591	14186.800462	29.299789
352.397834	14215.497821	29.304807
352.663963	14249.760499	29.309824
353.092635	14283.468279	29.314842
353.558674	14299.174825	29.319860
353.679059	14345.083547	29.324877
354.026036	14371.895755	29.329895
354.343505	14400.496984	29.334912
354.955189	14439.821630	29.339930
355.518267	14464.079578	29.344948
355.482983	14500.448011	29.349965
355.988878	14529.334950	29.354983
356.497397	14559.513868	29.360000
356.563395	14587.146946	29.365018
357.244351	14614.553409	29.370036
357.778977	14643.955878	29.375053
358.006515	14675.433077	29.380071
358.342067	14705.051548	29.385088
358.698259	14721.747605	29.390106
359.109552	14753.090409	29.395124
359.514440	14779.778613	29.400141
360.355220	14797.852120	29.405159
361.237780	14810.073038	29.410176
361.599464	14823.564123	29.415194
361.994896	14826.292874	29.420212
362.452386	14840.630174	29.425229
362.439068	14844.194378	29.430247
362.923012	14857.706161	29.435264
363.245368	14884.036290	29.440282
363.539286	14895.532337	29.445300
364.074378	14918.197459	29.450317
364.279905	14929.102995	29.455335
364.384709	14952.359750	29.460352
364.248652	14969.716255	29.465370
364.821741	14995.770076	29.470388
364.715473	15024.638219	29.475405
365.189551	15058.054778	29.480423
365.715504	15085.798272	29.485440
365.896581	15118.116221	29.490458
366.260453	15141.552440	29.495476
366.679590	15170.136549	29.500493
367.075317	15196.373034	29.505511
367.701810	15210.143554	29.510528
368.216519	15236.585724	29.515546
368.291427	15253.759329	29.520564
368.662762	15276.428508	29.525581
368.668929	15291.799455	29.530599
369.012105	15317.239464	29.535616
369.230178	15352.871050	29.540634
370.030492	15377.757650	29.545652
370.770203	15393.462346	29.550669
370.779260	15421.528689	29.555687
371.395310	15430.399350	29.560704
371.721387	15459.894667	29.565722
372.633191	15464.443306	29.570740
372.963527	15482.862428	29.575757
373.254175	15499.340050	29.580775
373.614060	15514.001503	29.585792
373.700574	15550.298437	29.590810
374.333106	15557.829856	29.595828
374.194109	15571.650606	29.600845
374.399823	15612.293812	29.605863
374.929708	15633.807046	29.610880
375.075637	15673.916562	29.615898
375.527046	15687.150727	29.620916
375.671640	15721.463461	29.625933
376.314036	15740.551343	29.630951
376.959578	15763.334839	29.635968
376.979393	15792.337847	29.640986
377.329259	15810.862849	29.646004
377.812971	15838.676104	29.651021
377.875953	15881.268193	29.656039
378.584702	15914.097427	29.661056
379.089370	15949.583400	29.666074
379.201062	15978.057636	29.671092
379.895448	16009.677358	29.676109
379.804105	16043.049561	29.681127
380.387142	16068.159293	29.686144
380.587892	16107.400153	29.691162
380.812048	16135.915876	29.696180
381.416733	16170.679572	29.701197
381.907280	16210.977462	29.706215
382.363333	16242.101307	29.711232
382.877318	16274.341008	29.716250
382.985348	16307.570292	29.721268
383.621444	16331.940247	29.726285
383.905909	16372.178189	29.731303
384.118935	16394.742802	29.736320
384.622710	16424.746248	29.741338
385.209184	16454.409732	29.746356
385.957779	16476.548182	29.751373
386.580530	16512.696687	29.756391
386.809769	16529.852291	29.761408
387.134532	16551.972975	29.766426
387.617228	16573.232044	29.771444
388.320987	16594.377185	29.776461
388.460806	16614.558364	29.781479
389.090395	16630.785364	29.786496
389.756237	16652.893664	29.791514
390.657589	16646.618677	29.796532
391.216997	16643.590826	29.801549
391.343273	16643.918253	29.806567
391.597922	16660.409323	29.811584
391.948958	16681.359389	29.816602
392.079870	16690.303439	29.821620
392.236736	16702.855967	29.826637
392.575124	16724.139202	29.831655
392.853867	16755.197317	29.836672
393.187187	16772.830833	29.841690
393.287523	16787.087298	29.846708
393.409865	16807.742919	29.851725
393.413755	16841.887472	29.856743
393.626469	16862.710998	29.861760
394.030155	16890.236677	29.866778
394.575540	16926.668484	29.871796
395.028273	16961.760158	29.876813
394.814883	17002.088634	29.881831
395.333192	17033.104325	29.886848
396.452626	17057.466005	29.891866
397.455080	17054.950871	29.896884
398.203893	17062.797849	29.901901
398.642198	17101.730489	29.906919
399.054172	17103.471697	29.911936
399.374335	17131.801377	29.916954
399.576399	17144.354614	29.921972
400.161107	17154.750974	29.926989
400.202961	17173.352314	29.932007
400.292174	17203.192744	29.937024
400.817898	17234.972092	29.942042
401.034750	17242.357384	29.947060
402.054112	17258.156137	29.952077
402.368414	17277.500495	29.957095
402.759535	17296.486904	29.962112
402.700998	17318.602923	29.967130
402.994513	17349.653396	29.972148
403.405936	17373.633453	29.977165
403.401360	17406.402870	29.982183
403.924681	17439.284860	29.987200
404.405746	17476.338601	29.992218
404.668403	17506.265839	29.997236
405.002144	17543.088834	30.002253
405.293188	17591.615458	30.007271
405.695681	17633.764730	30.012288
406.110581	17663.660658	30.017306
406.366647	17709.961327	30.022324
407.106827	17737.017942	30.027341
407.097685	17776.069049	30.032359
407.634843	17808.434003	30.037376
408.317546	17851.238765	30.042394
408.174861	17897.899394	30.047412
408.723692	17925.353818	30.052429
409.012237	17973.528864	30.057447
409.763688	18010.660268	30.062464
410.285050	18056.917837	30.067482
410.433650	18089.524434	30.072500
410.880660	18124.099311	30.077517
411.344825	18179.929123	30.082535
411.882411	18214.541165	30.087552
412.276118	18257.100187	30.092570
412.295990	18298.160767	30.097588
412.951850	18341.603391	30.102605
413.451700	18378.969731	30.107623
414.717406	18409.833906	30.112640
414.912401	18446.374545	30.117658
415.354912	18474.217995	30.122676
416.129930	18498.514475	30.127693
416.679140	18519.050877	30.132711
418.637052	18491.770370	30.137728
419.909251	18491.943761	30.142746
420.227550	18488.525271	30.147764
420.418658	18477.491697	30.152781
420.760688	18480.419113	30.157799
420.937721	18481.613066	30.162816
421.631220	18471.273230	30.167834
421.560285	18475.613927	30.172852
421.980568	18474.588856	30.177869
421.665030	18475.856740	30.182887
421.807378	18487.464022	30.187904
422.242301	18494.749021	30.192922
421.897518	18517.019797	30.197940
422.277967	18530.059946	30.202957
422.972451	18555.429251	30.207975
422.868905	18580.606397	30.212992
423.155555	18599.767719	30.218010
423.172337	18630.669495	30.223028
423.610736	18667.649430	30.228045
423.553588	18702.179980	30.233063
424.208756	18748.656871	30.238080
424.913966	18785.722021	30.243098
425.076444	18829.728689	30.248116
425.447646	18856.471645	30.253133
425.930227	18901.227754	30.258151
426.626258	18921.722928	30.263168
427.190541	18954.913257	30.268186
427.729437	18989.376930	30.273204
428.326224	19012.593931	30.278221
428.759705	19050.184051	30.283239
429.495471	19082.647772	30.288256
429.459947	19111.709910	30.293274
429.933579	19136.680097	30.298292
430.422954	19165.574745	30.303309
430.835049	19206.205091	30.308327
431.339122	19243.005132	30.313344
431.651143	19280.420459	30.318362
432.540611	19303.352778	30.323380
433.006164	19325.251983	30.328397
432.986314	19364.567131	30.333415
433.313055	19390.857988	30.338432
433.846505	19425.463776	30.343450
434.153819	19457.567425	30.348468
434.800171	19484.264110	30.353485
435.396594	19512.063238	30.358503
436.023930	19544.112323	30.363520
436.439737	19571.637280	30.368538
436.363661	19617.441896	30.373556
437.048653	19651.059720	30.378573
437.453598	19689.140014	30.383591
437.387776	19722.918947	30.388608
438.305870	19753.770841	30.393626
438.439738	19785.754155	30.398644
438.959745	19822.396747	30.403661
439.997675	19855.760871	30.408679
440.316973	19893.192124	30.413696
440.852610	19917.177290	30.418714
440.905312	19949.696239	30.423732
441.095818	19983.831993	30.428749
441.803492	20015.521794	30.433767
442.365081	20053.034557	30.438784
443.074306	20085.577160	30.443802
443.110426	20126.138175	30.448820
443.442997	20160.711056	30.453837
443.935241	20198.413816	30.458855
444.141107	20235.145748	30.463872
445.212727	20268.763663	30.468890
445.316236	20310.833768	30.473908
445.792180	20339.876147	30.478925
446.455421	20382.085226	30.483943
446.686260	20414.990135	30.488960
447.305368	20450.154548	30.493978
447.480396	20484.924536	30.498996
447.934428	20518.759044	30.504013
448.889423	20550.468691	30.509031
449.296626	20582.939446	30.514048
449.970541	20597.504367	30.519066
450.146461	20633.321394	30.524084
450.594812	20653.743165	30.529101
451.031582	20687.721201	30.534119
451.427529	20712.828044	30.539136
452.113591	20739.176432	30.544154
452.098286	20775.916322	30.549172
452.451073	20798.408507	30.554189
453.272555	20825.696292	30.559207
453.546564	20857.390339	30.564224
454.115722	20884.138343	30.569242
454.363697	20919.196677	30.574260
454.675768	20954.052086	30.579277
455.108989	20988.316694	30.584295
455.276541	21022.932945	30.589312
455.599360	21056.993719	30.594330
456.125936	21100.532783	30.599348
456.604520	21144.464639	30.604365
456.852106	21178.840877	30.609383
457.090965	21221.970803	30.614400
457.875677	21265.412236	30.619418
458.036550	21305.362535	30.624436
458.559186	21349.774807	30.629453
459.143384	21403.099519	30.634471
459.392300	21454.625879	30.639488
460.242627	21498.298251	30.644506
460.095116	21551.897899	30.649524
460.744457	21606.319286	30.654541
461.741449	21643.648185	30.659559
461.736287	21702.063630	30.664576
462.302695	21740.049222	30.669594
463.096370	21791.344226	30.674612
463.298882	21824.896747	30.679629
463.722473	21874.906933	30.684647
464.506001	21913.485976	30.689664
465.201279	21963.478107	30.694682
465.612163	22000.656013	30.699700
466.309625	22041.438181	30.704717
467.389393	22055.590079	30.709735
468.390961	22075.989497	30.714752
469.455362	22082.310612	30.719770
469.905282	22112.412074	30.724788
470.118163	22122.124344	30.729805
470.828825	22139.582604	30.734823
471.145337	22155.307248	30.739840
471.407154	22177.737543	30.744858
471.695917	22206.126757	30.749876
472.075780	22232.050575	30.754893
472.061185	22252.229511	30.759911
472.195625	22283.074302	30.764928
472.481258	22321.956144	30.769946
472.782629	22361.902948	30.774964
473.076665	22400.990135	30.779981
473.393860	22440.116140	30.784999
473.586352	22490.626952	30.790016
473.883480	22537.165907	30.795034
474.424103	22594.965553	30.800052
474.912112	22650.091969	30.805069
475.701059	22694.435162	30.810087
476.111365	22748.340152	30.815104
476.385265	22792.556269	30.820122
477.357110	22849.291761	30.825140
477.980496	22889.974745	30.830157
478.703443	22912.506034	30.835175
479.364608	22947.692323	30.840192
479.782155	22985.051043	30.845210
480.333421	23026.594677	30.850228
480.620285	23069.224625	30.855245
481.083988	23097.176293	30.860263
481.364217	23150.659488	30.865280
481.718877	23185.422539	30.870298
482.097343	23227.233468	30.875316
482.441399	23267.047585	30.880333
483.066800	23311.734928	30.885351
483.258047	23357.286087	30.890368
483.972184	23392.243736	30.895386
484.361662	23433.985539	30.900404
484.353108	23482.695610	30.905421
484.882645	23523.334198	30.910439
485.598580	23582.246605	30.915456
485.811361	23622.961691	30.920474
486.312215	23672.095465	30.925492
486.638053	23721.324678	30.930509
487.444270	23754.761825	30.935527
488.575532	23819.339755	30.940544
489.104827	23847.272301	30.945562
489.727944	23892.584434	30.950580
490.139692	23922.963525	30.955597
491.017322	23960.489247	30.960615
491.492147	23994.311483	30.965632
492.002700	24024.147647	30.970650
492.745059	24058.562665	30.975668
493.484495	24068.986537	30.980685
495.943872	24054.149078	30.985703
496.277719	24066.999420	30.990720
496.772429	24067.362011	30.995738
497.035969	24080.381734	31.000756
497.355043	24104.279512	31.005773
497.547944	24116.052586	31.010791
497.604686	24120.610068	31.015808
497.861223	24145.678926	31.020826
498.463543	24168.734969	31.025844
498.222619	24203.332503	31.030861
498.561864	24231.327206	31.035879
498.692581	24279.349365	31.040896
499.053015	24312.771758	31.045914
499.348014	24350.156980	31.050932
499.256194	24395.992890	31.055949
500.075368	24451.417076	31.060967
499.851705	24511.121106	31.065984
500.382237	24579.717347	31.071002
501.070555	24632.350491	31.076020
501.966506	24683.413313	31.081037
502.869902	24733.263909	31.086055
503.905349	24774.053280	31.091072
504.439674	24817.278880	31.096090
505.216869	24837.969647	31.101108
505.190166	24888.470343	31.106125
505.782880	24933.150017	31.111143
505.929685	24980.124321	31.116160
506.782541	25031.043944	31.121178
507.338748	25060.934265	31.126196
507.254150	25117.384379	31.131213
507.953861	25155.836465	31.136231
508.492730	25208.969316	31.141248
508.397519	25260.416096	31.146266
509.088597	25310.199546	31.151284
509.264514	25363.699102	31.156301
510.049080	25425.323752	31.161319
510.659752	25475.404908	31.166336
511.462307	25528.469723	31.171354
512.267341	25572.033923	31.176372
512.556273	25629.991308	31.181389
513.090181	25667.986334	31.186407
513.650955	25723.252524	31.191424
513.975068	25771.672555	31.196442
514.957993	25815.166825	31.201460
514.915154	25868.713741	31.206477
515.475142	25923.905005	31.211495
515.862763	25966.665802	31.216512
516.444371	26014.179490	31.221530
516.719209	26047.824504	31.226548
517.108409	26104.489360	31.231565
517.529037	26151.389844	31.236583
518.494252	26199.070599	31.241600
518.932470	26245.041057	31.246618
519.905461	26284.787709	31.251636
520.368707	26331.334632	31.256653
520.670120	26383.343449	31.261671
521.530506	26424.891317	31.266688
522.069302	26458.881281	31.271706
522.671087	26497.901488	31.276724
523.418473	26531.626689	31.281741
524.484295	26557.422656	31.286759
525.277076	26594.256941	31.291776
525.524356	26623.040480	31.296794
526.043361	26645.028594	31.301812
526.437330	26684.919644	31.306829
526.970686	26718.390552	31.311847
527.505367	26747.142343	31.316864
527.712463	26781.869376	31.321882
528.304117	26818.381095	31.326900
528.796525	26861.035231	31.331917
528.986655	26906.774217	31.336935
529.488859	26953.597093	31.341952
529.836024	27000.843300	31.346970
530.706867	27032.851896	31.351988
530.919465	27084.965898	31.357005
531.431615	27129.346055	31.362023
531.561564	27190.562089	31.367040
531.999658	27248.916528	31.372058
532.576309	27294.608123	31.377076
533.092686	27351.921546	31.382093
533.496070	27409.522056	31.387111
534.106160	27474.201868	31.392128
534.385509	27530.612043	31.397146
534.925719	27586.644699	31.402164
535.593977	27644.826602	31.407181
535.945524	27703.506088	31.412199
536.666978	27759.685861	31.417216
536.867929	27822.431762	31.422234
537.998387	27881.256948	31.427252
538.135439	27951.689052	31.432269
539.102500	28003.153702	31.437287
539.942685	28052.939232	31.442304
540.369625	28122.320717	31.447322
541.161423	28173.225059	31.452340
541.536555	28225.902257	31.457357
541.770709	28272.536606	31.462375
542.503917	28327.082147	31.467392
542.952186	28391.953136	31.472410
543.617673	28429.945002	31.477428
544.573031	28480.823084	31.482445
545.239953	28538.695887	31.487463
546.140913	28576.639507	31.492480
546.199610	28633.055195	31.497498
547.153318	28669.841938	31.502516
547.549507	28723.066067	31.507533
547.924607	28770.385006	31.512551
548.469024	28816.442444	31.517568
548.514180	28871.810616	31.522586
550.703314	28884.760281	31.527604
552.825093	28869.287163	31.532621
553.656834	28888.841190	31.537639
554.854047	28904.854828	31.542656
554.618750	28909.723917	31.547674
555.185076	28907.923189	31.552692
555.697217	28921.605653	31.557709
555.821107	28916.953912	31.562727
556.227804	28913.551825	31.567744
555.941667	28922.599979	31.572762
556.604520	28946.131903	31.577780
557.027318	28960.993349	31.582797
557.152346	28986.889241	31.587815
557.605649	29008.254001	31.592832
557.448147	29047.655266	31.597850
557.621606	29086.121469	31.602868
557.761089	29134.370180	31.607885
558.200834	29181.711050	31.612903
558.776305	29246.911132	31.617920
558.799261	29296.782300	31.622938
559.181046	29363.248523	31.627956
559.749434	29431.198351	31.632973
560.297344	29503.180632	31.637991
561.096181	29552.677607	31.643008
561.219566	29638.902732	31.648026
561.674043	29700.363942	31.653044
562.243861	29770.794618	31.658061
562.647746	29841.814712	31.663079
563.691070	29919.187113	31.668096
563.971419	29994.459141	31.673114
564.407502	30059.518179	31.678132
565.117713	30133.571007	31.683149
565.287468	30212.973300	31.688167
566.355440	30283.064599	31.693184
567.106103	30367.895579	31.698202
567.679528	30432.734426	31.703220
568.465193	30512.152531	31.708237
568.858866	30583.174162	31.713255
569.904865	30638.984338	31.718272
570.636346	30708.489574	31.723290
571.175576	30773.871724	31.728308
572.343253	30829.242670	31.733325
572.849017	30880.631496	31.738343
573.718441	30943.107205	31.743360
574.216955	30991.588517	31.748378
574.624752	31035.481647	31.753396
575.530392	31096.304893	31.758413
576.111456	31144.343814	31.763431
577.015689	31198.844669	31.768448
577.432012	31257.471677	31.773466
578.181381	31284.589312	31.778484
579.005785	31318.815838	31.783501
579.554068	31359.821517	31.788519
580.177572	31403.496742	31.793536
580.718043	31453.947531	31.798554
581.233260	31498.085860	31.803572
581.962789	31538.355084	31.808589
582.157268	31577.933896	31.813607
582.693313	31621.040461	31.818624
583.254317	31668.834877	31.823642
583.903281	31716.460208	31.828660
584.759667	31766.348277	31.833677
584.596713	31824.682102	31.838695
585.556576	31869.747757	31.843712
585.930704	31929.706078	31.848730
586.126055	31981.234849	31.853748
586.793626	32040.154044	31.858765
586.695686	32092.975044	31.863783
587.744649	32151.664047	31.868800
588.292936	32234.893671	31.873818
588.448877	32294.207894	31.878836
589.388861	32356.806263	31.883853
589.573475	32435.155865	31.888871
590.081449	32490.474338	31.893888
590.885548	32547.889504	31.898906
591.654511	32607.894997	31.903924
592.048321	32654.034830	31.908941
592.916670	32722.297795	31.913959
593.893275	32772.276024	31.918976
594.275440	32830.636232	31.923994
594.916732	32880.847152	31.929012
595.883727	32927.507841	31.934029
596.002211	32991.494437	31.939047
596.933625	33041.739681	31.944064
597.332065	33096.226240	31.949082
597.855045	33150.099045	31.954100
598.520666	33202.941709	31.959117
598.638522	33274.916115	31.964135
599.212325	33335.846340	31.969152
599.433613	33402.117750	31.974170
600.216532	33461.495848	31.979188
600.698563	33536.837813	31.984205
601.776640	33594.864082	31.989223
603.741026	33615.598543	31.994240
605.008610	33660.106449	31.999258
605.506580	33701.734938	32.004276
606.725083	33725.704837	32.009293
607.021460	33766.275100	32.014311
607.661039	33786.242025	32.019328
607.823341	33827.162875	32.024346
608.148341	33871.032596	32.029364
608.847520	33905.537376	32.034381
609.368528	33958.302158	32.039399
609.641699	34007.352979	32.044416
609.911742	34052.674420	32.049434
610.457812	34104.709664	32.054452
611.405286	34153.920314	32.059469
611.995293	34202.837014	32.064487
612.547147	34251.072234	32.069504
613.110931	34303.130360	32.074522
613.567077	34351.911908	32.079540
614.313169	34401.832011	32.084557
614.520390	34470.274569	32.089575
615.072318	34519.211081	32.094592
615.796834	34586.649860	32.099610
616.044269	34643.230102	32.104628
616.883539	34708.927220	32.109645
617.577150	34778.135951	32.114663
618.130975	34829.809096	32.119680
618.848481	34897.502676	32.124698
619.327381	34959.460913	32.129716
620.299980	35003.768689	32.134733
620.829209	35067.470447	32.139751
621.572103	35122.767547	32.144768
622.336389	35177.142900	32.149786
623.456866	35222.610125	32.154804
624.635901	35259.436332	32.159821
625.240513	35313.469370	32.164839
625.879434	35348.927408	32.169856
626.514508	35389.097959	32.174874
626.871839	35430.870594	32.179892
627.742761	35466.599626	32.184909
627.937833	35509.049508	32.189927
628.898856	35548.759179	32.194944
629.594770	35580.676694	32.199962
630.189022	35627.579920	32.204980
631.145633	35654.016540	32.209997
631.355432	35705.326428	32.215015
631.896533	35754.454312	32.220032
632.370979	35790.937827	32.225050
632.285024	35849.388767	32.230068
633.183734	35883.337181	32.235085
633.570576	35958.897655	32.240103
633.783900	36002.955246	32.245120
634.347384	36054.624000	32.250138
635.406605	36099.368262	32.255156
636.415971	36139.102774	32.260173
636.921545	36177.513414	32.265191
638.389431	36204.879057	32.270208
639.182421	36240.979207	32.275226
639.965724	36262.193785	32.280244
641.005615	36287.689626	32.285261
641.431091	36323.765749	32.290279
641.893254	36354.767155	32.295296
642.267498	36385.353982	32.300314
642.803670	36422.986821	32.305332
643.120012	36466.182603	32.310349
643.583684	36528.151928	32.315367
643.573525	36565.582253	32.320384
643.916079	36623.730997	32.325402
643.873414	36694.429650	32.330420
644.705199	36754.590119	32.335437
645.096196	36815.909700	32.340455
645.450415	36897.949689	32.345472
646.478888	36968.452628	32.350490
646.682810	37064.986386	32.355508
647.363019	37140.638808	32.360525
647.873591	37226.356589	32.365543
648.287825	37314.502158	32.370560
648.844781	37397.883722	32.375578
649.366411	37499.944192	32.380596
650.050221	37581.187659	32.385613
650.554480	37670.891853	32.390631
651.645042	37760.227699	32.395648
653.034969	37818.638794	32.400666
654.402410	37881.564258	32.405684
655.505325	37938.795569	32.410701
655.993515	38016.427848	32.415719
656.743256	38087.660041	32.420736
657.383017	38148.093746	32.425754
657.997382	38221.113371	32.430772
658.752269	38278.968537	32.435789
659.104251	38343.348867	32.440807
659.363765	38414.831022	32.445824
660.111084	38487.040524	32.450842
660.192705	38569.250100	32.455860
661.120161	38642.209959	32.460877
662.014582	38720.311237	32.465895
662.460461	38786.309455	32.470912
663.389244	38859.197362	32.475930
663.922354	38939.149319	32.480948
665.115548	39010.286237	32.485965
665.737522	39083.336458	32.490983
665.790563	39148.586809	32.496000
666.723497	39226.087261	32.501018
667.176359	39304.867259	32.506036
667.979871	39380.401187	32.511053
668.512090	39455.652179	32.516071
669.194821	39544.098545	32.521088
669.986165	39614.262837	32.526106
670.453186	39700.381429	32.531124
671.181879	39781.551479	32.536141
672.114927	39845.019879	32.541159
672.506500	39933.235514	32.546176
673.098762	39998.591921	32.551194
673.728961	40088.646939	32.556212
674.317234	40175.082240	32.561229
675.053831	40255.495450	32.566247
675.906200	40331.568147	32.571264
676.766848	40403.734823	32.576282
677.108858	40497.520517	32.581300
677.981197	40561.418172	32.586317
678.645592	40642.378562	32.591335
679.183464	40715.998532	32.596352
680.138679	40777.929087	32.601370
680.572233	40845.259479	32.606388
681.036643	40913.323705	32.611405
681.928192	40983.801746	32.616423
682.390252	41060.229532	32.621440
683.618674	41126.971233	32.626458
684.318930	41209.913866	32.631476
684.520066	41286.780525	32.636493
685.724322	41353.710162	32.641511
686.303053	41420.140912	32.646528
687.217454	41482.421563	32.651546
687.959671	41560.809591	32.656564
688.886056	41624.294703	32.661581
690.550194	41657.217600	32.666599
690.961681	41723.812959	32.671616
693.476981	41734.902778	32.676634
695.015982	41748.197289	32.681652
696.460638	41756.238388	32.686669
697.611278	41772.943847	32.691687
697.811601	41788.553748	32.696704
698.791239	41788.545855	32.701722
698.849301	41808.002563	32.706740
698.897895	41813.023710	32.711757
699.238861	41819.729536	32.716775
699.330619	41861.845122	32.721792
700.196068	41879.601968	32.726810
700.276269	41938.909803	32.731828
700.555065	41969.780701	32.736845
700.909212	42022.558709	32.741863
700.494416	42089.295720	32.746880
701.144644	42149.175736	32.751898
701.423527	42236.682325	32.756916
701.784474	42316.576497	32.761933
702.304176	42408.416534	32.766951
702.762004	42504.463158	32.771968
703.247451	42586.487845	32.776986
703.478987	42690.734289	32.782004
704.345957	42771.623007	32.787021
705.385347	42868.228499	32.792039
705.936917	42972.246583	32.797056
706.814613	43071.285787	32.802074
707.567687	43169.184331	32.807092
708.266518	43277.798757	32.812109
709.077043	43367.656664	32.817127
709.935728	43466.745326	32.822144
710.761964	43549.121807	32.827162
711.687340	43651.758696	32.832180
713.328007	43714.523006	32.837197
714.878695	43779.957818	32.842215
715.818846	43841.853754	32.847232
716.886713	43888.873158	32.852250
717.645372	43958.557325	32.857268
717.994040	44012.822700	32.862285
718.740923	44075.569265	32.867303
719.435300	44144.156539	32.872320
720.225815	44186.221361	32.877338
721.004448	44250.453555	32.882356
721.506738	44314.886562	32.887373
722.128544	44378.305344	32.892391
722.469872	44451.704354	32.897408
722.997194	44515.638169	32.902426
723.785650	44584.359838	32.907444
724.029359	44659.184113	32.912461
724.609301	44730.555361	32.917479
724.743630	44819.503138	32.922496
725.614075	44898.828027	32.927514
725.712223	44986.304860	32.932532
726.184322	45072.996930	32.937549
727.234399	45155.873790	32.942567
727.570074	45253.208365	32.947584
728.393171	45346.243921	32.952602
729.097209	45429.526772	32.957620
729.933939	45517.271846	32.962637
731.091784	45596.990880	32.967655
732.334318	45694.101398	32.972672
733.473534	45760.650321	32.977690
734.709097	45818.133471	32.982708
736.059850	45880.223742	32.987725
737.054083	45929.622470	32.992743
737.668837	45999.344408	32.997760
738.661735	46044.862791	33.002778
739.384134	46097.676409	33.007796
739.985711	46158.429922	33.012813
740.766325	46213.094127	33.017831
741.182865	46274.481867	33.022848
742.223133	46321.193014	33.027866
743.012359	46376.099411	33.032884
743.593007	46445.073940	33.037901
744.211687	46494.492282	33.042919
744.837025	46572.052306	33.047936
745.787831	46618.235891	33.052954
746.456369	46677.694712	33.057972
747.466204	46751.692736	33.062989
747.717861	46813.899064	33.068007
747.884384	46882.899722	33.073024
748.815781	46956.118934	33.078042
749.575039	47032.171235	33.083060
750.243790	47098.850342	33.088077
751.234285	47175.158516	33.093095
751.774593	47246.119525	33.098112
752.165571	47326.131053	33.103130
752.789023	47400.041006	33.108148
753.606396	47500.834628	33.113165
754.009831	47583.573677	33.118183
754.762091	47670.587986	33.123200
755.547662	47759.921479	33.128218
756.146343	47837.633203	33.133236
756.407809	47934.106443	33.138253
757.151800	48025.671361	33.143271
757.859364	48124.446386	33.148288
759.021094	48214.426977	33.153306
760.497879	48300.057481	33.158324
761.263924	48391.986838	33.163341
761.775406	48478.526864	33.168359
762.471509	48568.308499	33.173376
763.105014	48652.324624	33.178394
763.895908	48751.253279	33.183412
764.471209	48849.725551	33.188429
765.956170	48928.324164	33.193447
766.439624	49014.966012	33.198464
767.381966	49095.607183	33.203482
768.393280	49181.009392	33.208500
769.254718	49255.638683	33.213517
770.014484	49331.235789	33.218535
770.454229	49427.655369	33.223552
770.980025	49502.792976	33.228570
772.247708	49588.836640	33.233588
772.797857	49681.635501	33.238605
773.342536	49766.729298	33.243623
773.902487	49853.482243	33.248640
774.420460	49945.450744	33.253658
775.048877	50044.773087	33.258676
775.365412	50146.810268	33.263693
776.912724	50236.196247	33.268711
777.302631	50327.053943	33.273728
778.338894	50399.870963	33.278746
779.749432	50478.807283	33.283764
780.392988	50562.583721	33.288781
781.221233	50630.815261	33.293799
782.114544	50706.534570	33.298816
782.784508	50792.708099	33.303834
783.624453	50868.828561	33.308852
784.210682	50955.180957	33.313869
785.597188	51029.493067	33.318887
786.384317	51105.989624	33.323904
787.026128	51181.253483	33.328922
787.856434	51244.496259	33.333940
788.645908	51321.776614	33.338957
789.505502	51398.571843	33.343975
789.934607	51476.165322	33.348992
790.724086	51566.573993	33.354010
792.027267	51645.311792	33.359028
792.661056	51732.607356	33.364045
793.523875	51803.749601	33.369063
794.381624	51878.260134	33.374080
795.171254	51959.194472	33.379098
796.073245	52024.443159	33.384116
796.594257	52122.006133	33.389133
797.180118	52199.393270	33.394151
797.479181	52286.702658	33.399168
798.686769	52375.169370	33.404186
799.311173	52477.846841	33.409204
799.643847	52581.116595	33.414221
800.710208	52667.592745	33.419239
801.843970	52772.916457	33.424256
802.012635	52864.217595	33.429274
802.792874	52960.402366	33.434292
803.370017	53072.314757	33.439309
803.930571	53179.605877	33.444327
804.348803	53293.580254	33.449344
805.106524	53406.620751	33.454362
806.119145	53516.340571	33.459380
807.015706	53635.835246	33.464397
808.160438	53737.889607	33.469415
809.908180	53826.336406	33.474432
811.447386	53914.919309	33.479450
812.877105	53978.684312	33.484468
813.663969	54064.916076	33.489485
814.406136	54134.709482	33.494503
815.529415	54213.026276	33.499520
816.243021	54284.505589	33.504538
816.853571	54370.205638	33.509556
817.597679	54453.242860	33.514573
817.980763	54528.366689	33.519591
818.875252	54620.383202	33.524608
819.412663	54705.224920	33.529626
820.435906	54783.952328	33.534644
820.817702	54880.079947	33.539661
821.568504	54963.566812	33.544679
822.170225	55060.435969	33.549696
823.068925	55159.391952	33.554714
823.578271	55255.576046	33.559732
823.671102	55359.892202	33.564749
825.002334	55460.553408	33.569767
825.590510	55567.246361	33.574784
826.505697	55679.818816	33.579802
827.070850	55785.878583	33.584820
828.192793	55903.485570	33.589837
828.731447	56006.018749	33.594855
829.528588	56112.970612	33.599872
830.247666	56229.546930	33.604890
830.895390	56323.501642	33.609908
831.219516	56445.282003	33.614925
832.630868	56543.711157	33.619943
834.165924	56632.041543	33.624960
834.714416	56728.024060	33.629978
835.459370	56821.276214	33.634996
836.766586	56931.275718	33.640013
837.238177	57025.686352	33.645031
838.258162	57123.292341	33.650048
839.346184	57232.407299	33.655066
840.248750	57323.101663	33.660084
841.014828	57408.555204	33.665101
841.939425	57515.335454	33.670119
842.762216	57610.575248	33.675136
843.316329	57711.534810	33.680154
844.339705	57812.385395	33.685172
844.963813	57918.048592	33.690189
845.410800	58032.494095	33.695207
846.400079	58139.898876	33.700224
846.823140	58249.951270	33.705242
847.922555	58352.940567	33.710260
848.905831	58476.026801	33.715277
849.818053	58591.068134	33.720295
850.616984	58690.677512	33.725312
851.608647	58813.726500	33.730330
853.084954	58904.446537	33.735348
854.194479	58989.464304	33.740365
855.246725	59084.616124	33.745383
856.267737	59181.328235	33.750400
857.080928	59283.390238	33.755418
857.938345	59385.192624	33.760436
858.639809	59479.052085	33.765453
859.545374	59575.298616	33.770471
860.437187	59668.381618	33.775488
860.889192	59773.059280	33.780506
861.660876	59873.064530	33.785524
862.461110	59980.719051	33.790541
863.157741	60091.216393	33.795559
864.128628	60193.850897	33.800576
864.686499	60313.087849	33.805594
866.050000	60414.052997	33.810612
867.306600	60516.142420	33.815629
868.178467	60620.628363	33.820647
869.286843	60706.911258	33.825664
870.145495	60815.110367	33.830682
871.806716	60891.151957	33.835700
872.707392	60977.476793	33.840717
873.322650	61078.322938	33.845735
874.090704	61161.036368	33.850752
874.536571	61262.113787	33.855770
875.657955	61351.165588	33.860788
876.299768	61440.449064	33.865805
877.210404	61540.856602	33.870823
878.401080	61630.757709	33.875840
879.181517	61725.480344	33.880858
879.780943	61812.579253	33.885876
880.713237	61916.859551	33.890893
881.809393	62009.786618	33.895911
883.215644	62097.429140	33.900928
883.810384	62184.928612	33.905946
884.897602	62286.947562	33.910964
885.685142	62361.995595	33.915981
886.618397	62440.862741	33.920999
887.463631	62520.876219	33.926016
888.152900	62618.854357	33.931034
888.904097	62702.246821	33.936052
889.832536	62804.288375	33.941069
890.344064	62898.643881	33.946087
891.408718	62982.573304	33.951104
891.942095	63070.086729	33.956122
892.825496	63155.228956	33.961140
893.997720	63241.410813	33.966157
894.773545	63335.079712	33.971175
895.855526	63417.295032	33.976192
896.373596	63507.853286	33.981210
896.849553	63597.704639	33.986228
897.975192	63690.318358	33.991245
898.697622	63793.517841	33.996263
899.704351	63898.699763	34.001280
900.062302	63998.945546	34.006298
900.851242	64106.250676	34.011316
902.022368	64218.682722	34.016333
903.172379	64308.526435	34.021351
904.182309	64414.987358	34.026368
905.125799	64520.461073	34.031386
905.773560	64623.177690	34.036404
906.730974	64726.943359	34.041421
907.494076	64839.667739	34.046439
908.369584	64951.634457	34.051456
909.034648	65071.544976	34.056474
910.100896	65169.744461	34.061492
911.233590	65287.517776	34.066509
911.753825	65405.779023	34.071527
912.958536	65522.207842	34.076544
913.406539	65651.134531	34.081562
914.293452	65768.129523	34.086580
915.369556	65890.517886	34.091597
915.679169	66024.198555	34.096615
916.971989	66146.792681	34.101632
917.514847	66291.651380	34.106650
918.186803	66424.079620	34.111668
919.369056	66547.073756	34.116685
920.108691	66682.805130	34.121703
921.144088	66812.817382	34.126720
922.095446	66951.524668	34.131738
923.347414	67086.143114	34.136756
924.630627	67212.664808	34.141773
925.835582	67338.485837	34.146791
927.190258	67451.233582	34.151808
927.803268	67573.765511	34.156826
928.895748	67696.149034	34.161844
930.005459	67809.249143	34.166861
930.938063	67928.739604	34.171879
931.899065	68051.810863	34.176896
932.266246	68168.943402	34.181914
933.120219	68298.868475	34.186932
934.144946	68427.729106	34.191949
934.906868	68555.748969	34.196967
935.395409	68685.174342	34.201984
936.408847	68826.520178	34.207002
936.898977	68958.830100	34.212020
938.232243	69098.562956	34.217037
939.103355	69241.964782	34.222055
940.224376	69369.910986	34.227072
941.701021	69499.499799	34.232090
943.131853	69622.299858	34.237108
944.032725	69737.310163	34.242125
945.809112	69843.734601	34.247143
947.049614	69929.243430	34.252160
947.880607	70052.638707	34.257178
948.698315	70162.701508	34.262196
950.031709	70260.115267	34.267213
950.705736	70377.303875	34.272231
951.581455	70476.685193	34.277248
952.425417	70588.155893	34.282266
953.285228	70688.912972	34.287284
954.174052	70785.435441	34.292301
954.866544	70895.655576	34.297319
955.831006	70989.213428	34.302336
956.561001	71092.909000	34.307354
957.177193	71198.318626	34.312372
958.456867	71303.087497	34.317389
958.974120	71415.400811	34.322407
960.444678	71518.608780	34.327424
961.519448	71617.892787	34.332442
962.219891	71742.223700	34.337460
963.151425	71849.866984	34.342477
963.512596	71970.309596	34.347495
964.380256	72084.414738	34.352512
964.907988	72214.676995	34.357530
965.428512	72351.859387	34.362548
966.674469	72483.635597	34.367565
967.275032	72621.919399	34.372583
968.278017	72763.254959	34.377600
969.578002	72900.975481	34.382618
970.156728	73047.859784	34.387636
971.114353	73187.801721	34.392653
971.836140	73341.848299	34.397671
972.666549	73491.647146	34.402688
973.601528	73651.029658	34.407706
974.575889	73801.205161	34.412724
976.217907	73944.851851	34.417741
977.243788	74096.437454	34.422759
978.381728	74233.453355	34.427776
978.986863	74389.714881	34.432794
980.335146	74542.812183	34.437812
982.552518	74671.581821	34.442829
983.338474	74794.164121	34.447847
984.425505	74926.373586	34.452864
985.944148	75049.196223	34.457882
986.773758	75170.375662	34.462900
989.173785	75259.760853	34.467917
990.952937	75358.287285	34.472935
992.481372	75449.708938	34.477952
993.566094	75537.137852	34.482970
994.676874	75607.682241	34.487988
995.392399	75704.116164	34.493005
995.936457	75799.086327	34.498023
996.498000	75894.477755	34.503040
997.249790	75994.126226	34.508058
998.091652	76099.718170	34.513076
998.975935	76203.197408	34.518093
999.690561	76314.801116	34.523111
999.970885	76425.731114	34.528128
1000.742729	76550.128119	34.533146
1001.350880	76672.168469	34.538164
1002.869756	76802.097456	34.543181
1003.413077	76940.196593	34.548199
1004.152594	77073.393715	34.553216
1005.142037	77213.355998	34.558234
1005.438620	77344.844556	34.563252
1006.206657	77486.268455	34.568269
1007.017370	77638.173427	34.573287
1007.641723	77807.795874	34.578304
1009.018543	77944.314435	34.583322
1010.172093	78116.356246	34.588340
1011.632405	78260.016892	34.593357
1012.507146	78396.659481	34.598375
1013.919736	78537.843924	34.603392
1015.650630	78663.295430	34.608410
1016.547442	78807.065741	34.613428
1017.786868	78948.249875	34.618445
1018.817620	79094.011345	34.623463
1019.585600	79216.083351	34.628480
1020.464715	79327.586271	34.633498
1021.188300	79455.094411	34.638516
1022.753193	79564.624942	34.643533
1023.865805	79692.069873	34.648551
1024.506443	79825.919700	34.653568
1025.537229	79941.259266	34.658586
1025.950407	80083.296114	34.663604
1027.027370	80215.203371	34.668621
1027.742378	80364.890613	34.673639
1028.320294	80512.406449	34.678656
1029.195272	80661.018976	34.683674
1030.074537	80811.314518	34.688692
1031.503404	80968.940471	34.693709
1032.256171	81118.651722	34.698727
1033.521404	81280.374747	34.703744
1034.889980	81423.811390	34.708762
1035.481749	81586.597281	34.713780
1036.660941	81734.521055	34.718797
1037.623949	81891.794173	34.723815
1038.552292	82052.888994	34.728832
1039.916877	82219.106644	34.733850
1041.147535	82373.067847	34.738868
1041.907761	82535.269473	34.743885
1042.917117	82693.514707	34.748903
1043.936161	82861.129271	34.753920
1045.419996	83010.662013	34.758938
1047.473384	83142.683590	34.763956
1049.233570	83280.727093	34.768973
1050.412683	83423.005603	34.773991
1051.416250	83562.226593	34.779008
1052.932452	83695.998125	34.784026
1053.774346	83816.760183	34.789044
1054.609160	83941.206360	34.794061
1055.858464	84071.905144	34.799079
1056.275185	84215.447573	34.804096
1057.191526	84340.261994	34.809114
1057.866866	84482.655924	34.814132
1058.879009	84631.075272	34.819149
1060.296713	84768.368285	34.824167
1061.339092	84917.474116	34.829184
1062.768997	85050.578123	34.834202
1063.320051	85208.726803	34.839220
1064.612675	85352.744681	34.844237
1065.818865	85494.405006	34.849255
1066.643957	85641.697590	34.854272
1067.890826	85777.038075	34.859290
1069.411760	85901.482150	34.864308
1070.752878	86036.207384	34.869325
1072.434731	86171.857641	34.874343
1073.623014	86301.478073	34.879360
1074.735381	86427.859393	34.884378
1075.211447	86556.580646	34.889396
1076.214483	86686.442756	34.894413
1077.305096	86822.574539	34.899431
1078.500450	86943.142289	34.904448
1079.740059	87067.189958	34.909466
1080.564441	87192.756258	34.914484
1081.572937	87334.112473	34.919501
1082.382877	87473.243397	34.924519
1083.321625	87603.456612	34.929536
1084.429657	87743.887536	34.934554
1085.382410	87889.122746	34.939572
1086.495735	88016.107269	34.944589
1087.588443	88153.505678	34.949607
1088.648609	88295.985480	34.954624
1090.068938	88431.641523	34.959642
1091.339605	88556.938520	34.964660
1094.145797	88638.715018	34.969677
1095.750226	88734.733662	34.974695
1097.709621	88802.906174	34.979712
1099.017758	88873.446145	34.984730
1099.879016	88959.729464	34.989748
1100.531640	89038.181540	34.994765
1101.315336	89117.289267	34.999783
1101.846989	89209.931257	35.004800
1102.455090	89297.751308	35.009818
1102.822323	89411.102717	35.014836
1103.318308	89529.584703	35.019853
1104.325695	89639.749009	35.024871
1104.594299	89786.412993	35.029888
1105.780683	89917.363562	35.034906
1106.120565	90055.739552	35.039924
1106.699669	90212.607031	35.044941
1107.374772	90367.333156	35.049959
1108.282316	90527.989740	35.054976
1108.938672	90705.200939	35.059994
1109.900464	90881.862788	35.065012
1110.750564	91070.588372	35.070029
1112.089593	91258.240670	35.075047
1113.180495	91444.182456	35.080064
1114.474505	91633.712196	35.085082
1115.352014	91825.597326	35.090100
1116.563190	92017.865329	35.095117
1117.489141	92206.188447	35.100135
1118.301792	92409.804315	35.105152
1119.748688	92602.373288	35.110170
1121.126915	92810.835542	35.115188
1122.225901	92998.661380	35.120205
1123.221951	93198.259550	35.125223
1124.301953	93405.656043	35.130240
1125.544994	93597.051416	35.135258
1126.943630	93807.139149	35.140276
1128.088496	93995.015659	35.145293
1129.216036	94193.365833	35.150311
1130.462107	94393.862724	35.155328
1131.763362	94587.237373	35.160346
1133.181584	94789.943355	35.165364
1134.185775	94989.750954	35.170381
1135.274892	95181.538663	35.175399
1136.740164	95376.898887	35.180416
1137.968980	95566.279981	35.185434
1138.927235	95757.897628	35.190452
1140.360364	95959.287718	35.195469
1142.088242	96136.987173	35.200487
1143.126896	96324.835704	35.205504
1144.025927	96507.954750	35.210522
1145.867260	96700.768853	35.215540
1147.072318	96879.604847	35.220557
1148.582382	97046.958732	35.225575
1150.071558	97218.647258	35.230592
1151.993429	97366.107877	35.235610
1153.711107	97519.534979	35.240628
1155.664991	97654.634726	35.245645
1157.156205	97790.065180	35.250663
1158.011163	97935.863929	35.255680
1159.103453	98064.904760	35.260698
1161.190747	98168.021440	35.265716
1162.536113	98270.432295	35.270733
1164.246624	98391.275209	35.275751
1165.345103	98504.268731	35.280768
1166.337272	98601.396318	35.285786
1167.497239	98711.050545	35.290804
1168.359089	98810.815203	35.295821
1169.506641	98919.016288	35.300839
1170.056041	99050.254082	35.305856
1170.840376	99163.815472	35.310874
1171.672956	99278.692547	35.315892
1172.388998	99397.679324	35.320909
1173.003435	99532.143980	35.325927
1173.585811	99665.076207	35.330944
1174.701627	99797.046941	35.335962
1175.571915	99949.439128	35.340980
1175.957666	100089.319827	35.345997
1177.485052	100245.853023	35.351015
1178.350587	100392.322596	35.356032
1179.603633	100556.576721	35.361050
1180.427384	100727.082527	35.366068
1181.336362	100898.847941	35.371085
1182.422096	101069.027648	35.376103
1183.516831	101251.401445	35.381120
1184.393134	101418.977977	35.386138
1186.092174	101599.905384	35.391156
1187.142727	101785.994273	35.396173
1188.623654	101951.023629	35.401191
1189.889503	102127.524784	35.406208
1190.903884	102309.121597	35.411226
1192.309048	102493.491506	35.416244
1193.600532	102670.973544	35.421261
1194.778706	102841.326894	35.426279
1195.975880	103029.337956	35.431296
1197.468126	103201.566476	35.436314
1198.924753	103382.875822	35.441332
1199.958442	103555.442362	35.446349
1202.279658	103708.255617	35.451367
1203.530246	103881.028951	35.456384
1204.933988	104041.746886	35.461402
1206.156804	104207.789551	35.466420
1207.188790	104380.767083	35.471437
1208.132373	104528.823838	35.476455
1208.749450	104704.113955	35.481472
1210.243220	104873.902626	35.486490
1211.550861	105058.338489	35.491508
1212.632866	105229.210941	35.496525
1214.055842	105399.572000	35.501543
1214.973637	105583.480946	35.506560
1215.974009	105769.403900	35.511578
1217.346783	105943.614342	35.516596
1218.498772	106126.816954	35.521613
1219.351447	106311.906968	35.526631
1220.282489	106508.840206	35.531648
1221.030569	106707.654431	35.536666
1222.098397	106904.365254	35.541684
1223.133935	107111.836160	35.546701
1224.325049	107318.282262	35.551719
1225.637080	107522.164033	35.556736
1226.582137	107735.544478	35.561754
1227.883025	107950.564869	35.566772
1229.352971	108143.988212	35.571789
1230.864859	108347.678439	35.576807
1232.301417	108558.285943	35.581824
1233.566397	108763.299582	35.586842
1235.091354	108968.106988	35.591860
1236.028860	109182.918814	35.596877
1237.572973	109365.799843	35.601895
1239.310765	109569.613813	35.606912
1240.172054	109770.559936	35.611930
1241.864315	109949.392197	35.616948
1243.055881	110142.711330	35.621965
1244.693569	110344.356277	35.626983
1245.757211	110539.092843	35.632000
1246.940196	110722.359572	35.637018
1248.112588	110907.250736	35.642036
1248.785738	111112.329567	35.647053
1250.186474	111297.337498	35.652071
1251.401761	111487.710603	35.657088
1252.511164	111686.830804	35.662106
1253.287862	111855.705686	35.667124
1254.573155	112066.960768	35.672141
1255.847367	112253.946999	35.677159
1257.174614	112450.844976	35.682176
1258.025059	112643.680873	35.687194
1259.540188	112842.982803	35.692212
1260.592425	113051.154929	35.697229
1261.437754	113247.923125	35.702247
1263.024437	113460.646399	35.707264
1263.957426	113660.924885	35.712282
1265.533342	113878.049218	35.717300
1266.727291	114080.086412	35.722317
1268.023941	114293.890325	35.727335
1269.361306	114497.287674	35.732352
1270.013637	114728.216538	35.737370
1271.826565	114934.933557	35.742388
1273.527363	115142.126793	35.747405
1274.999201	115354.389363	35.752423
1276.512946	115553.001302	35.757440
1277.602531	115768.561154	35.762458
1279.156417	115970.020065	35.767476
1280.184842	116188.494654	35.772493
1281.642926	116399.310279	35.777511
1282.875651	116619.021295	35.782528
1283.778928	116836.672708	35.787546
1284.809917	117048.666282	35.792564
1285.981048	117275.969444	35.797581
1286.877763	117503.674697	35.802599
1288.611996	117729.076163	35.807616
1289.562125	117958.283968	35.812634
1290.810492	118196.123677	35.817652
1292.013687	118439.193281	35.822669
1293.563639	118678.380750	35.827687
1294.760764	118918.566380	35.832704
1295.869367	119152.065566	35.837722
1297.260131	119379.019408	35.842740
1298.214511	119626.511855	35.847757
1299.331180	119872.306833	35.852775
1300.765870	120129.290943	35.857792
1301.552694	120387.309803	35.862810
1303.100710	120637.690228	35.867828
1304.113489	120911.756908	35.872845
1305.659227	121172.051807	35.877863
1308.129730	121401.541414	35.882880
1309.866228	121642.268204	35.887898
1312.550161	121858.888867	35.892916
1313.916642	122081.064760	35.897933
1315.767523	122282.606952	35.902951
1317.434236	122496.701711	35.907968
1318.448839	122707.890029	35.912986
1319.781907	122905.416324	35.918004
1321.046458	123119.937097	35.923021
1322.078945	123327.983930	35.928039
1323.503658	123537.183783	35.933056
1324.452162	123750.354762	35.938074
1325.599423	123960.224565	35.943092
1326.554734	124180.760681	35.948109
1327.807067	124403.771182	35.953127
1328.922953	124624.220538	35.958144
1329.864902	124860.060898	35.963162
1330.722594	125094.434228	35.968180
1332.176312	125328.520410	35.973197
1333.151305	125572.117258	35.978215
1334.463828	125816.547263	35.983232
1335.261051	126066.577972	35.988250
1336.804192	126304.902682	35.993268
1338.018814	126540.241867	35.998285
1338.962230	126785.513960	36.003303
1340.761613	127008.807683	36.008320
1341.975620	127254.279452	36.013338
1343.141173	127490.508594	36.018356
1344.833899	127722.570793	36.023373
1346.507464	127954.156260	36.028391
1348.629316	128178.558383	36.033408
1349.704055	128422.668247	36.038426
1351.502447	128630.560803	36.043444
1352.915468	128860.561117	36.048461
1354.300475	129088.957986	36.053479
1355.857422	129301.851157	36.058496
1357.253691	129517.801898	36.063514
1358.688527	129726.231025	36.068532
1360.427428	129950.329111	36.073549
1361.437889	130163.686346	36.078567
1363.704839	130374.947933	36.083584
1365.254103	130586.786289	36.088602
1366.706319	130790.351955	36.093620
1368.044980	130990.502502	36.098637
1368.894698	131220.220495	36.103655
1370.094522	131442.022713	36.108672
1370.803717	131664.947307	36.113690
1371.880993	131903.303205	36.118708
1372.917082	132139.449287	36.123725
1373.912254	132379.559046	36.128743
1375.669853	132623.283842	36.133760
1376.610809	132876.767730	36.138778
1377.865073	133131.393297	36.143796
1379.147054	133385.547217	36.148813
1380.363028	133651.896936	36.153831
1381.658231	133906.204871	36.158848
1382.332022	134190.815598	36.163866
1383.597390	134453.423828	36.168884
1385.211759	134744.133453	36.173901
1386.773950	135020.794620	36.178919
1388.030779	135287.328394	36.183936
1389.413162	135584.524310	36.188954
1390.868663	135854.617609	36.193972
1393.641701	136098.656409	36.198989
1395.409432	136350.191784	36.204007
1397.692152	136603.773642	36.209024
1399.151755	136848.745759	36.214042
1400.744732	137096.651674	36.219060
1402.015543	137342.989981	36.224077
1403.109295	137597.778178	36.229095
1404.718648	137829.369208	36.234112
1405.943866	138091.442386	36.239130
1406.830031	138343.303776	36.244148
1408.615024	138593.737404	36.249165
1409.286372	138847.096274	36.254183
1410.441739	139113.969048	36.259200
1411.947655	139379.467125	36.264218
1413.459089	139646.906332	36.269236
1414.676983	139908.791902	36.274253
1415.952542	140180.167051	36.279271
1417.313028	140438.279819	36.284288
1418.865336	140716.549199	36.289306
1419.988841	140991.024516	36.294324
1421.549186	141266.076267	36.299341
1422.753360	141546.286728	36.304359
1424.366390	141823.312289	36.309376
1425.967199	142090.692257	36.314394
1427.242275	142363.999387	36.319412
1428.954537	142632.975463	36.324429
1429.947536	142922.045059	36.329447
1431.032297	143191.433809	36.334464
1432.179968	143470.806782	36.339482
1433.182356	143737.334788	36.344500
1434.704959	144013.733245	36.349517
1435.574311	144301.236821	36.354535
1437.220563	144568.945127	36.359552
1438.540307	144851.191797	36.364570
1439.691866	145143.322150	36.369588
1440.936657	145459.978438	36.374605
1441.982414	145757.838090	36.379623
1443.271856	146059.641910	36.384640
1444.441564	146377.827865	36.389658
1445.939144	146690.559680	36.394676
1448.481369	146984.414731	36.399693
1450.189839	147289.723017	36.404711
1451.496209	147590.813878	36.409728
1453.098830	147905.872275	36.414746
1454.752429	148210.144695	36.419764
1456.251107	148519.290122	36.424781
1457.045863	148829.911918	36.429799
1458.773917	149132.213760	36.434816
1460.638283	149441.116014	36.439834
1462.648368	149745.265858	36.444852
1464.973320	150028.565452	36.449869
1466.280695	150319.024436	36.454887
1468.226462	150611.092085	36.459904
1469.773099	150905.866357	36.464922
1471.508696	151188.130906	36.469940
1473.006286	151469.549165	36.474957
1474.043499	151760.647501	36.479975
1475.511702	152050.484316	36.484992
1477.163715	152330.640323	36.490010
1478.150079	152639.866580	36.495028
1479.553265	152922.478158	36.500045
1480.773402	153233.496962	36.505063
1482.222028	153523.056420	36.510080
1483.245555	153843.917787	36.515098
1484.307870	154158.724816	36.520116
1486.046763	154479.244500	36.525133
1487.138953	154812.850620	36.530151
1488.558113	155131.170765	36.535168
1489.618150	155456.161935	36.540186
1490.944080	155808.524300	36.545204
1492.511402	156135.327044	36.550221
1494.152997	156483.634542	36.555239
1495.260976	156824.231994	36.560256
1497.123288	157155.167730	36.565274
1498.679708	157506.669671	36.570292
1500.753920	157840.163808	36.575309
1502.179070	158174.529471	36.580327
1504.174211	158499.428440	36.585344
1506.299706	158822.912929	36.590362
1507.831402	159138.671052	36.595380
1509.934790	159445.431054	36.600397
1511.872763	159768.801894	36.605415
1513.546160	160065.970796	36.610432
1515.337152	160364.023091	36.615450
1516.696373	160677.411184	36.620468
1518.278363	160969.286017	36.625485
1519.632594	161271.477009	36.630503
1521.193459	161567.926805	36.635520
1522.845887	161879.232727	36.640538
1523.765860	162175.222152	36.645556
1525.624335	162467.086964	36.650573
1526.892829	162778.069876	36.655591
1528.683830	163071.980016	36.660608
1530.298126	163364.931860	36.665626
1532.028696	163665.846922	36.670644
1534.180812	163942.777978	36.675661
1535.552645	164214.955406	36.680679
1537.234718	164471.109165	36.685696
1538.614303	164729.052834	36.690714
1540.301325	164999.178269	36.695732
1541.900022	165256.086401	36.700749
1543.185917	165529.555148	36.705767
1544.175071	165794.916292	36.710784
1545.861255	166081.276779	36.715802
1547.039957	166353.461549	36.720820
1548.245171	166640.425637	36.725837
1549.713584	166927.297199	36.730855
1551.320166	167212.802721	36.735872
1553.371493	167500.571065	36.740890
1554.779931	167789.780166	36.745908
1556.400864	168072.395774	36.750925
1557.619130	168367.032888	36.755943
1558.748993	168656.864760	36.760960
1560.336599	168948.932021	36.765978
1562.301052	169256.432177	36.770996
1564.049620	169543.235948	36.776013
1565.657996	169848.730786	36.781031
1566.548941	170147.595820	36.786048
1568.048875	170453.226865	36.791066
1569.415008	170781.076225	36.796084
1571.237736	171100.413571	36.801101
1572.484149	171413.453006	36.806119
1574.101881	171741.775029	36.811136
1576.181016	172058.589223	36.816154
1577.400474	172364.748850	36.821172
1579.204683	172678.859062	36.826189
1581.037965	172994.895451	36.831207
1583.195190	173316.692395	36.836224
1584.958338	173618.163420	36.841242
1587.221038	173916.977374	36.846260
1589.247290	174209.690174	36.851277
1590.645447	174510.313594	36.856295
1592.525086	174808.701652	36.861312
1593.700454	175108.883475	36.866330
1594.765365	175415.735457	36.871348
1596.558113	175710.716924	36.876365
1598.225659	176024.110170	36.881383
1599.367962	176328.962550	36.886400
1601.034855	176636.521904	36.891418
1602.414623	176952.925785	36.896436
1604.278007	177262.829705	36.901453
1605.984380	177570.312138	36.906471
1607.817897	177864.715863	36.911488
1609.762429	178182.582258	36.916506
1610.825758	178488.565069	36.921524
1612.463069	178799.620099	36.926541
1613.813593	179116.562785	36.931559
1615.516460	179442.917154	36.936576
1616.971239	179749.807218	36.941594
1618.165812	180069.129642	36.946612
1619.773175	180399.516574	36.951629
1621.017408	180729.750032	36.956647
1622.401922	181077.134945	36.961664
1623.999095	181420.844208	36.966682
1625.669777	181769.455496	36.971700
1626.951465	182108.956880	36.976717
1628.127354	182469.509587	36.981735
1629.561368	182824.627554	36.986752
1631.565025	183173.776701	36.991770
1632.828214	183535.642147	36.996788
1634.397463	183882.583172	37.001805
1635.826080	184261.015683	37.006823
1637.980468	184605.833436	37.011840
1640.213253	184947.111660	37.016858
1641.601291	185292.428844	37.021876
1643.616397	185612.422605	37.026893
1645.132955	185941.068883	37.031911
1646.787002	186259.095257	37.036928
1648.655539	186601.307156	37.041946
1649.892714	186929.447008	37.046964
1651.465337	187272.892525	37.051981
1653.347824	187606.044879	37.056999
1654.550101	187942.650399	37.062016
1655.929016	188288.419006	37.067034
1657.138567	188641.745293	37.072052
1659.181126	188990.645058	37.077069
1660.757637	189337.567705	37.082087
1662.461107	189708.945825	37.087104
1664.349357	190055.986062	37.092122
1665.426696	190432.969141	37.097140
1666.663948	190804.939173	37.102157
1668.318832	191184.090872	37.107175
1669.958556	191568.147591	37.112192
1671.467325	191946.312717	37.117210
1673.035351	192321.829852	37.122228
1674.796942	192714.404481	37.127245
1677.013734	193094.008104	37.132263
1678.764562	193484.063109	37.137280
1680.613266	193863.884778	37.142298
1681.944090	194248.491794	37.147316
1683.703442	194624.841690	37.152333
1685.821707	195032.072833	37.157351
1687.348017	195423.865507	37.162368
1689.149828	195820.489968	37.167386
1690.906066	196208.694561	37.172404
1692.806506	196588.320711	37.177421
1694.830385	196983.430058	37.182439
1696.208608	197388.945067	37.187456
1698.535825	197759.696350	37.192474
1699.747805	198154.617142	37.197492
1701.531885	198545.408103	37.202509
1703.698226	198925.816054	37.207527
1705.584070	199312.531821	37.212544
1707.630927	199686.437993	37.217562
1709.213146	200082.565525	37.222580
1710.788454	200463.105332	37.227597
1712.715556	200841.798708	37.232615
1714.358875	201223.016973	37.237632
1716.177146	201611.724659	37.242650
1717.783676	201995.162365	37.247668
1720.187042	202354.689139	37.252685
1722.430248	202732.705339	37.257703
1724.153383	203101.198200	37.262720
1726.078746	203465.761454	37.267738
1727.811540	203821.597531	37.272756
1729.627023	204183.008296	37.277773
1731.562651	204538.065059	37.282791
1733.271701	204902.137925	37.287808
1735.145586	205254.745053	37.292826
1736.703981	205611.367642	37.297844
1738.160688	205976.287390	37.302861
1740.397285	206322.211320	37.307879
1741.954492	206687.422498	37.312896
1743.939387	207040.946302	37.317914
1745.961916	207383.075761	37.322932
1748.133137	207707.951423	37.327949
1750.469284	208047.555737	37.332967
1752.072507	208387.994024	37.337984
1753.884731	208710.647652	37.343002
1755.723094	209036.040951	37.348020
1757.654202	209370.588022	37.353037
1759.599362	209675.916252	37.358055
1761.123786	209982.293074	37.363072
1762.847181	210287.723790	37.368090
1764.286935	210594.904159	37.373108
1765.464546	210900.681504	37.378125
1767.200120	211204.056422	37.383143
1767.931464	211536.601466	37.388160
1769.877609	211847.943611	37.393178
1771.240348	212190.494316	37.398196
1772.663604	212523.385609	37.403213
1773.934952	212878.373099	37.408231
1775.397537	213237.774763	37.413248
1776.993285	213596.851039	37.418266
1777.829513	213968.803927	37.423284
1779.242462	214369.793301	37.428301
1780.776714	214747.805193	37.433319
1781.856423	215155.939044	37.438336
1783.374791	215576.192777	37.443354
1785.337509	215987.409391	37.448372
1787.007317	216415.210230	37.453389
1789.106146	216820.515597	37.458407
1791.137780	217246.964866	37.463424
1792.947249	217670.151059	37.468442
1794.620799	218106.187646	37.473460
1796.304412	218532.141352	37.478477
1798.100393	219041.029316	37.483495
1800.457738	219463.192501	37.488512
1802.497280	219902.401727	37.493530
1804.352627	220323.559442	37.498548
1806.047459	220755.920901	37.503565
1808.183617	221190.979450	37.508583
1809.918423	221621.661427	37.513600
1812.124985	222045.561557	37.518618
1814.254630	222482.607438	37.523636
1815.976692	222903.289216	37.528653
1818.117526	223324.868333	37.533671
1820.043770	223748.973705	37.538688
1821.812686	224181.717147	37.543706
1823.769276	224609.452745	37.548724
1824.986037	225050.190146	37.553741
1826.676865	225486.761221	37.558759
1828.440243	225933.050007	37.563776
1830.050211	226369.663007	37.568794
1832.162003	226827.530466	37.573812
1833.311944	227289.597584	37.578829
1835.241159	227742.037508	37.583847
1836.883701	228198.996961	37.588864
1838.853288	228662.457110	37.593882
1840.839828	229122.359959	37.598900
1842.701139	229578.119390	37.603917
1844.616922	230038.722822	37.608935
1846.433689	230504.348115	37.613952
1848.417559	230959.685264	37.618970
1849.858339	231435.536195	37.623988
1852.128920	231896.162924	37.629005
1854.714973	232333.268143	37.634023
1856.956280	232795.172490	37.639040
1859.096925	233234.843365	37.644058
1861.156609	233681.260221	37.649076
1862.741051	234128.620697	37.654093
1864.946841	234566.938111	37.659111
1866.581264	235025.951986	37.664128
1868.124129	235479.546315	37.669146
1870.015320	235910.857643	37.674164
1871.190192	236373.329620	37.679181
1873.350221	236825.250203	37.684199
1875.420399	237265.679734	37.689216
1877.409527	237720.374192	37.694234
1879.342262	238166.721813	37.699252
1880.619155	238596.108944	37.704269
1882.984343	239022.014398	37.709287
1884.941574	239443.949387	37.714304
1886.837637	239878.215416	37.719322
1888.942734	240293.904053	37.724340
1890.270772	240731.212554	37.729357
1891.859807	241171.730157	37.734375
1893.438879	241606.509310	37.739392
1894.969987	242063.651341	37.744410
1896.818784	242510.301177	37.749428
1898.345146	242973.897906	37.754445
1899.870672	243431.932446	37.759463
1901.628930	243910.175094	37.764480
1903.626449	244389.191820	37.769498
1905.522312	244867.057675	37.774516
1906.773903	245358.240477	37.779533
1908.688166	245856.223836	37.784551
1910.531359	246357.776151	37.789568
1912.218950	246854.858709	37.794586
1914.142400	247358.101218	37.799604
1916.128203	247879.700422	37.804621
1918.223439	248383.398540	37.809639
1919.962539	248897.723955	37.814656
1922.062227	249425.276053	37.819674
1924.286719	249927.659090	37.824692
1927.136941	250425.950725	37.829709
1929.629341	250919.805805	37.834727
1932.321415	251407.480720	37.839744
1934.112695	251895.305305	37.844762
1937.221207	252373.665310	37.849780
1939.323489	252837.941195	37.854797
1941.619240	253312.346624	37.859815
1943.956617	253776.330142	37.864832
1945.676575	254236.910568	37.869850
1947.624558	254703.804267	37.874868
1949.091728	255175.426638	37.879885
1950.346260	255641.825958	37.884903
1952.736960	256122.593296	37.889920
1954.326696	256616.499962	37.894938
1955.953467	257103.211493	37.899956
1957.456307	257593.754148	37.904973
1959.183653	258085.707670	37.909991
1961.136022	258585.676801	37.915008
1962.608593	259101.221445	37.920026
1964.650811	259609.330146	37.925044
1966.320849	260130.379923	37.930061
1967.791376	260642.266675	37.935079
1969.877498	261159.055774	37.940096
1972.043529	261688.025052	37.945114
1973.846493	262224.167194	37.950132
1975.741558	262770.810783	37.955149
1977.712441	263299.303614	37.960167
1979.347988	263834.812172	37.965184
1980.877684	264380.880242	37.970202
1982.903641	264924.706424	37.975220
1984.523096	265488.083728	37.980237
1987.222618	266036.928819	37.985255
1989.467765	266580.717221	37.990272
1991.907805	267127.927595	37.995290
1994.666804	267657.531013	38.000308
1996.890931	268196.596145	38.005325
1998.852519	268715.483320	38.010343
2000.888323	269247.135237	38.015360
2003.048763	269773.354964	38.020378
2004.863787	270294.728410	38.025396
2007.183612	270820.005717	38.030413
2009.320964	271332.229995	38.035431
2011.607471	271843.920706	38.040448
2013.394123	272338.089294	38.045466
2015.614916	272833.658513	38.050484
2017.155987	273341.862989	38.055501
2018.821220	273839.148266	38.060519
2020.606406	274338.063928	38.065536
2022.549257	274836.571491	38.070554
2024.280910	275344.969213	38.075572
2026.168067	275857.607732	38.080589
2028.054212	276379.923614	38.085607
2029.781676	276906.024145	38.090624
2031.321925	277440.562596	38.095642
2033.447839	277968.194954	38.100660
2035.247215	278517.979915	38.105677
2037.368241	279075.000518	38.110695
2039.142750	279607.564099	38.115712
2041.224481	280176.247624	38.120730
2043.527753	280726.552660	38.125748
2045.370490	281293.849906	38.130765
2047.140330	281857.474218	38.135783
2049.279328	282427.741602	38.140800
2050.895387	283010.997677	38.145818
2052.928016	283592.963470	38.150836
2055.276740	284174.036607	38.155853
2057.390589	284768.456783	38.160871
2059.513292	285349.715475	38.165888
2061.326439	285943.926960	38.170906
2063.546624	286527.070085	38.175924
2065.801638	287109.062098	38.180941
2068.394553	287705.550398	38.185959
2070.757543	288291.177411	38.190976
2073.097039	288886.458025	38.195994
2074.881712	289469.991355	38.201012
2077.556286	290048.650281	38.206029
2079.573714	290621.243256	38.211047
2082.269687	291207.208707	38.216064
2084.339198	291785.909222	38.221082
2086.529543	292367.660395	38.226100
2088.957762	292930.573628	38.231117
2091.069298	293508.700201	38.236135
2093.489626	294072.320514	38.241152
2095.250578	294644.149675	38.246170
2097.999890	295202.503098	38.251188
2100.440717	295773.070982	38.256205
2102.446898	296320.925077	38.261223
2105.228431	296871.035484	38.266240
2107.912349	297407.418560	38.271258
2111.088646	297926.116180	38.276276
2113.359167	298450.752080	38.281293
2114.877132	298980.437215	38.286311
2117.231736	299504.723608	38.291328
2119.065517	300028.991929	38.296346
2121.117781	300567.647286	38.301364
2123.116879	301085.634723	38.306381
2124.752036	301624.581884	38.311399
2126.708731	302159.307564	38.316416
2128.343164	302705.309192	38.321434
2130.238729	303245.499213	38.326452
2132.179373	303794.059605	38.331469
2133.840707	304347.285168	38.336487
2136.256237	304902.972873	38.341504
2138.132524	305464.638395	38.346522
2140.217607	306035.890955	38.351540
2142.324841	306597.104575	38.356557
2144.109862	307163.066137	38.361575
2146.248327	307734.857210	38.366592
2147.957859	308308.264539	38.371610
2149.570030	308896.311816	38.376628
2151.677498	309474.622603	38.381645
2153.815597	310042.918484	38.386663
2156.204908	310615.714405	38.391680
2157.710737	311175.371014	38.396698
2160.001274	311750.003427	38.401716
2162.272050	312319.860685	38.406733
2163.954973	312900.222665	38.411751
2166.018371	313474.244852	38.416768
2167.887011	314061.778994	38.421786
2169.850151	314664.554368	38.426804
2172.305107	315265.034097	38.431821
2174.139869	315867.846148	38.436839
2176.313523	316475.726375	38.441856
2178.583806	317081.122284	38.446874
2180.848717	317690.195766	38.451892
2183.096417	318302.085291	38.456909
2184.685980	318926.799774	38.461927
2186.765461	319555.337718	38.466944
2188.714326	320201.436998	38.471962
2190.986720	320829.575531	38.476980
2193.397991	321474.595537	38.481997
2195.537198	322113.763535	38.487015
2198.152984	322767.191953	38.492032
2200.033498	323406.796155	38.497050
2202.497855	324062.216767	38.502068
2204.897941	324706.621982	38.507085
2207.147859	325363.867072	38.512103
2209.595020	326016.324663	38.517120
2211.823904	326674.244630	38.522138
2214.024748	327340.083315	38.527156
2216.456098	327978.431506	38.532173
2218.921941	328636.899873	38.537191
2222.134980	329264.949375	38.542208
2224.497786	329891.304951	38.547226
2227.067305	330527.698222	38.552244
2229.392998	331171.106179	38.557261
2232.029418	331807.169349	38.562279
2234.274789	332437.527311	38.567296
2236.389891	333067.315791	38.572314
2238.365127	333723.419957	38.577332
2240.726438	334346.578003	38.582349
2242.999316	334993.681798	38.587367
2245.148946	335627.471084	38.592384
2247.384609	336260.603944	38.597402
2249.462871	336911.981208	38.602420
2251.487522	337547.443447	38.607437
2253.536523	338211.044383	38.612455
2255.285127	338849.023900	38.617472
2257.862080	339511.530596	38.622490
2260.189677	340161.023180	38.627508
2262.752463	340812.600526	38.632525
2265.608335	341456.303131	38.637543
2268.725412	342090.968954	38.642560
2271.070705	342721.921749	38.647578
2273.630123	343337.729157	38.652596
2275.770401	343985.146370	38.657613
2278.127718	344608.965880	38.662631
2279.830441	345230.169920	38.667648
2282.203059	345869.832826	38.672666
2284.628490	346508.183901	38.677684
2287.034149	347136.910831	38.682701
2289.347805	347765.492156	38.687719
2291.788055	348378.030163	38.692736
2294.440483	348995.371993	38.697754
2296.576400	349619.947409	38.702772
2299.385917	350240.697519	38.707789
2301.333933	350873.432656	38.712807
2303.794819	351492.091339	38.717824
2305.782841	352092.980121	38.722842
2307.577909	352688.766658	38.727860
2309.901292	353280.854220	38.732877
2312.081358	353884.782221	38.737895
2314.098155	354469.799120	38.742912
2316.582945	355081.500578	38.747930
2318.777311	355693.241279	38.752948
2320.718374	356285.908595	38.757965
2322.519775	356904.395357	38.762983
2324.574213	357525.419062	38.768000
2326.705192	358155.301162	38.773018
2328.654126	358790.658754	38.778036
2330.995000	359434.973913	38.783053
2332.853311	360080.931739	38.788071
2335.125939	360733.939847	38.793088
2337.418448	361401.065399	38.798106
2339.415925	362074.824823	38.803124
2342.416818	362731.155218	38.808141
2345.009243	363415.448443	38.813159
2347.223662	364071.100085	38.818176
2349.487892	364760.142541	38.823194
2351.584786	365433.472235	38.828212
2353.966818	366126.783163	38.833229
2356.170667	366818.791838	38.838247
2358.128454	367524.932346	38.843264
2360.496042	368220.921375	38.848282
2362.303214	368948.240554	38.853300
2364.510111	369663.963512	38.858317
2366.596994	370406.071542	38.863335
2368.474547	371146.778748	38.868352
2370.703501	371903.569203	38.873370
2373.281850	372657.774971	38.878388
2375.678890	373404.487565	38.883405
2378.306765	374155.787477	38.888423
2380.912987	374922.520046	38.893440
2383.226535	375683.806365	38.898458
2385.354150	376448.936220	38.903476
2388.120831	377223.960433	38.908493
2390.836812	378003.007658	38.913511
2393.001029	378769.271678	38.918528
2395.657691	379541.066334	38.923546
2397.833422	380321.037288	38.928564
2400.209235	381103.264420	38.933581
2402.632939	381884.831329	38.938599
2405.206146	382672.262859	38.943616
2407.558885	383441.253595	38.948634
2409.885592	384239.895123	38.953652
2412.110247	385026.921874	38.958669
2415.084589	385808.329032	38.963687
2417.588701	386599.403556	38.968704
2420.548906	387387.137880	38.973722
2422.815562	388178.770074	38.978740
2425.253206	388964.345942	38.983757
2428.083546	389747.302058	38.988775
2430.433929	390533.182354	38.993792
2433.205619	391308.833437	38.998810
2435.880302	392093.023252	39.003828
2438.989287	392847.008333	39.008845
2441.347963	393616.256222	39.013863
2443.868677	394373.722422	39.018880
2446.962045	395136.853458	39.023898
2449.094279	395891.506819	39.028916
2451.593682	396640.909985	39.033933
2453.605022	397399.980088	39.038951
2456.139539	398162.593315	39.043968
2458.960795	398903.801000	39.048986
2461.744241	399662.937819	39.054004
2464.359181	400412.250287	39.059021
2467.017263	401135.156858	39.064039
2469.191875	401853.107904	39.069056
2472.063007	402559.979073	39.074074
2473.964198	403277.052424	39.079092
2476.654752	403962.203357	39.084109
2479.218352	404665.246505	39.089127
2481.503033	405360.717137	39.094144
2483.982672	406066.449715	39.099162
2485.934141	406790.644964	39.104180
2488.165526	407507.377108	39.109197
2490.642198	408228.711259	39.114215
2492.832706	408962.790850	39.119232
2495.870144	409674.493789	39.124250
2497.904236	410421.656434	39.129268
2499.993210	411154.603769	39.134285
2502.808337	411900.177243	39.139303
2505.378487	412636.423665	39.144320
2508.178105	413391.025678	39.149338
2510.211689	414142.896032	39.154356
2512.300273	414903.904181	39.159373
2514.298580	415675.364918	39.164391
2516.324026	416467.210846	39.169408
2519.125101	417244.139487	39.174426
2521.464011	418054.675812	39.179444
2523.420079	418853.322330	39.184461
2526.445311	419664.453420	39.189479
2528.332170	420477.671290	39.194496
2531.381980	421281.250882	39.199514
2533.852718	422085.508128	39.204532
2537.466326	422884.359689	39.209549
2540.871968	423687.726556	39.214567
2543.213978	424489.065875	39.219584
2546.087886	425277.480528	39.224602
2549.077280	426089.647730	39.229620
2551.434505	426889.994141	39.234637
2554.145756	427682.964833	39.239655
2556.873907	428473.628299	39.244672
2559.462387	429274.515076	39.249690
2561.875763	430060.925420	39.254708
2564.576828	430874.344885	39.259725
2567.077039	431672.583367	39.264743
2569.462711	432483.468292	39.269760
2571.900628	433283.130041	39.274778
2574.385216	434099.915072	39.279796
2576.708730	434918.469357	39.284813
2579.175937	435733.579756	39.289831
2580.879476	436563.110071	39.294848
2583.533139	437391.592617	39.299866
2586.071149	438243.140370	39.304884
2588.556142	439087.074151	39.309901
2591.446119	439939.916383	39.314919
2593.697830	440794.602704	39.319936
2596.640955	441624.045008	39.324954
2599.510190	442467.483668	39.329972
2602.514902	443300.242784	39.334989
2605.283551	444139.636970	39.340007
2607.726519	444994.887628	39.345024
2610.785199	445830.627310	39.350042
2613.765620	446661.086637	39.355060
2616.913919	447482.127980	39.360077
2619.850675	448302.565886	39.365095
2622.153398	449128.135256	39.370112
2625.010073	449953.075098	39.375130
2627.243376	450786.380534	39.380148
2629.799468	451609.231740	39.385165
2631.800650	452453.686530	39.390183
2634.184135	453282.973803	39.395200
2636.653138	454108.674024	39.400218
2639.424067	454947.640973	39.405236
2641.428154	455754.592043	39.410253
2644.437973	456559.676387	39.415271
2646.657365	457384.477385	39.420288
2649.197715	458206.512231	39.425306
2651.034320	459034.545306	39.430324
2653.621357	459868.688994	39.435341
2655.960800	460710.775751	39.440359
2658.150994	461566.045382	39.445376
2660.584320	462432.257542	39.450394
2662.823307	463299.677129	39.455412
2664.647451	464194.016446	39.460429
2667.114410	465098.822378	39.465447
2669.203888	466017.799823	39.470464
2672.352851	466923.520203	39.475482
2674.645155	467848.088180	39.480500
2677.487439	468779.140526	39.485517
2680.804198	469702.742523	39.490535
2683.234337	470649.891030	39.495552
2685.750006	471580.204252	39.500570
2688.780590	472529.079659	39.505588
2691.719877	473473.426258	39.510605
2694.838564	474411.583193	39.515623
2697.921959	475361.064570	39.520640
2701.062907	476284.979690	39.525658
2703.697220	477228.580584	39.530676
2706.749305	478181.609815	39.535693
2709.937477	479121.890651	39.540711
2712.272442	480059.941265	39.545728
2715.345209	480984.691866	39.550746
2718.203503	481923.923144	39.555764
2721.126764	482870.719312	39.560781
2723.503948	483808.114210	39.565799
2726.494391	484759.697160	39.570816
2729.477296	485705.475224	39.575834
2731.944904	486646.997115	39.580852
2734.357075	487607.811829	39.585869
2736.971655	488553.851742	39.590887
2739.564858	489515.036912	39.595904
2742.742706	490467.795052	39.600922
2745.848609	491423.591433	39.605940
2748.686585	492380.540044	39.610957
2751.564472	493332.180707	39.615975
2754.446435	494288.107494	39.620992
2757.412902	495241.948496	39.626010
2760.104843	496188.112296	39.631028
2762.652026	497159.321819	39.636045
2765.744524	498125.289859	39.641063
2767.872123	499097.919976	39.646080
2770.439128	500062.501279	39.651098
2773.455172	501033.307915	39.656116
2775.687774	502005.801344	39.661133
2778.926270	502980.744142	39.666151
2781.647903	503966.204377	39.671168
2784.403796	504937.429337	39.676186
2787.793048	505906.222572	39.681204
2789.964697	506881.714373	39.686221
2793.825835	507849.557105	39.691239
2797.026653	508809.838102	39.696256
2800.330483	509758.348752	39.701274
2803.366367	510708.561413	39.706292
2806.160901	511666.167178	39.711309
2809.639079	512596.484600	39.716327
2812.338301	513542.349301	39.721344
2814.977936	514476.827449	39.726362
2818.136129	515417.715523	39.731380
2820.341847	516359.409996	39.736397
2823.005860	517298.200301	39.741415
2825.486637	518234.696721	39.746432
2828.418860	519148.238186	39.751450
2831.360702	520040.010013	39.756468
2833.841482	520944.501317	39.761485
2836.658329	521839.967271	39.766503
2839.071189	522743.809031	39.771520
2841.734760	523663.925158	39.776538
2844.231584	524583.307771	39.781556
2846.448976	525517.587666	39.786573
2849.104659	526450.377236	39.791591
2852.004419	527394.297579	39.796608
2854.316119	528350.239294	39.801626
2857.160439	529316.101201	39.806644
2859.275064	530298.987293	39.811661
2862.001837	531262.727476	39.816679
2864.783462	532253.175755	39.821696
2867.465597	533252.633849	39.826714
2870.804604	534254.733343	39.831732
2873.599811	535250.663169	39.836749
2876.626925	536265.861263	39.841767
2879.337392	537283.556275	39.846784
2882.256087	538305.019173	39.851802
2884.828937	539331.698998	39.856820
2887.705235	540380.793846	39.861837
2890.697549	541414.045830	39.866855
2893.180734	542459.479892	39.871872
2895.805502	543521.160266	39.876890
2898.817274	544572.234746	39.881908
2901.495487	545648.934185	39.886925
2904.666637	546710.834976	39.891943
2908.072983	547803.489943	39.896960
2910.798654	548877.165132	39.901978
2913.756411	549959.868380	39.906996
2916.024114	551059.139728	39.912013
2919.085016	552153.566674	39.917031
2921.809665	553260.778427	39.922048
2924.973842	554365.464718	39.927066
2928.253332	555467.428134	39.932084
2931.272995	556570.952163	39.937101
2934.617961	557675.135328	39.942119
2937.516115	558783.320368	39.947136
2940.379014	559892.323038	39.952154
2943.451261	560997.530939	39.957172
2946.344898	562116.438846	39.962189
2949.693003	563221.163034	39.967207
2952.549404	564349.027550	39.972224
2955.391368	565465.296913	39.977242
2958.361917	566578.536573	39.982260
2960.902243	567712.035926	39.987277
2963.792732	568830.818231	39.992295
2966.904524	569969.747200	39.997312
2970.018357	571114.296580	40.002330
2972.884279	572242.722832	40.007348
2975.631523	573390.490499	40.012365
2978.318987	574546.694674	40.017383
2981.433980	575686.514553	40.022400
2984.484707	576834.770758	40.027418
2987.407527	577991.370746	40.032436
2989.747281	579161.403400	40.037453
2993.326448	580319.734533	40.042471
2996.220187	581497.680488	40.047488
2998.714642	582668.157507	40.052506
3001.524336	583833.155204	40.057524
3004.924339	585017.348032	40.062541
3007.422800	586193.552980	40.067559
3010.390584	587363.650709	40.072576
3013.759743	588563.142212	40.077594
3017.309853	589728.552821	40.082612
3020.009678	590896.796971	40.087629
3023.280607	592032.962102	40.092647
3025.979949	593173.422141	40.097664
3029.383235	594306.741988	40.102682
3032.513442	595428.676393	40.107700
3035.574407	596559.581606	40.112717
3038.378058	597696.230134	40.117735
3041.629664	598819.221967	40.122752
3044.364560	599965.326088	40.127770
3047.618697	601105.322521	40.132788
3050.503112	602249.673346	40.137805
3053.178354	603401.103700	40.142823
3056.391008	604541.817648	40.147840
3059.542692	605710.606684	40.152858
3062.910718	606869.480868	40.157876
3065.638378	608032.946267	40.162893
3069.040901	609194.328931	40.167911
3071.916637	610355.178568	40.172928
3074.714148	611546.686732	40.177946
3077.897120	612723.298214	40.182964
3081.293558	613915.654821	40.187981
3084.425908	615078.971447	40.192999
3088.624281	616242.889492	40.198016
3091.846609	617421.745654	40.203034
3095.194030	618578.057409	40.208052
3098.910332	619745.833258	40.213069
3102.117816	620912.668461	40.218087
3105.642541	622072.478971	40.223104
3108.644536	623234.200597	40.228122
3111.823797	624386.374072	40.233140
3114.688325	625550.916578	40.238157
3117.632771	626729.706692	40.243175
3121.359877	627879.965283	40.248192
3124.684753	629039.605709	40.253210
3128.288681	630186.837991	40.258228
3131.056079	631359.001306	40.263245
3133.936680	632526.322230	40.268263
3136.919834	633695.693073	40.273280
3139.670660	634878.649082	40.278298
3142.946985	636042.267819	40.283316
3146.513308	637210.549267	40.288333
3149.855605	638383.426667	40.293351
3153.137714	639564.812617	40.298368
3155.799334	640756.492593	40.303386
3158.194391	641930.918326	40.308404
3161.090829	643130.414213	40.313421
3163.941474	644334.115289	40.318439
3167.604427	645542.326484	40.323456
3170.617581	646751.747324	40.328474
3174.023664	647965.195729	40.333492
3176.963639	649182.113865	40.338509
3179.624130	650400.176407	40.343527
3182.844603	651636.337212	40.348544
3185.746613	652872.446888	40.353562
3188.975016	654103.814594	40.358580
3191.982612	655346.323934	40.363597
3195.075152	656594.241216	40.368615
3198.456020	657858.586686	40.373632
3201.399772	659092.763165	40.378650
3204.324980	660351.731884	40.383668
3207.791825	661618.413440	40.388685
3210.653345	662887.368863	40.393703
3213.990080	664149.857330	40.398720
3216.806735	665441.527832	40.403738
3220.416543	666701.843827	40.408756
3223.326850	667987.980001	40.413773
3226.802917	669253.503053	40.418791
3230.125495	670533.704602	40.423808
3233.794750	671781.200561	40.428826
3237.513831	673006.643885	40.433844
3241.414680	674203.308774	40.438861
3244.812004	675416.159833	40.443879
3248.266232	676609.706897	40.448896
3251.333732	677804.407143	40.453914
3254.905419	678982.570600	40.458932
3258.305619	680180.387589	40.463949
3261.635083	681378.756002	40.468967
3264.799189	682554.641983	40.473984
3268.170265	683751.153445	40.479002
3271.676873	684951.259833	40.484020
3274.339857	686140.572274	40.489037
3277.122311	687361.682306	40.494055
3280.476203	688556.769115	40.499072
3283.424528	689793.457550	40.504090
3286.802395	691023.651639	40.509108
3289.793889	692248.629619	40.514125
3292.688098	693494.839225	40.519143
3295.987947	694738.624536	40.524160
3298.751832	696001.618418	40.529178
3301.948514	697260.392920	40.534196
3305.224182	698534.197390	40.539213
3308.192752	699825.468255	40.544231
3311.475248	701112.580686	40.549248
3314.300610	702410.730690	40.554266
3317.224548	703732.903695	40.559284
3320.525778	705059.618929	40.564301
3323.303107	706408.114138	40.569319
3326.592482	707750.765871	40.574336
3329.374553	709122.858007	40.579354
3332.293619	710493.618050	40.584372
3335.577941	711880.385853	40.589389
3338.926017	713260.432100	40.594407
3342.860720	714654.410412	40.599424
3346.714489	716033.326314	40.604442
3350.221225	717418.604343	40.609460
3354.466294	718808.824457	40.614477
3357.511549	720198.071659	40.619495
3361.234863	721576.293286	40.624512
3365.032188	722970.342885	40.629530
3368.066210	724356.522182	40.634548
3371.301805	725748.959332	40.639565
3374.602701	727157.062357	40.644583
3378.219598	728553.210089	40.649600
3382.197620	729957.852607	40.654618
3385.431234	731346.372023	40.659636
3389.108118	732736.012346	40.664653
3392.426685	734135.298543	40.669671
3395.827845	735532.204970	40.674688
3399.239266	736928.668960	40.679706
3402.334420	738325.336057	40.684724
3406.313124	739715.444601	40.689741
3409.805252	741124.728678	40.694759
3413.624130	742504.261278	40.699776
3416.751833	743902.258792	40.704794
3419.969573	745291.807949	40.709812
3423.343619	746693.853079	40.714829
3426.621734	748100.196998	40.719847
3429.913751	749504.806181	40.724864
3433.363863	750909.134996	40.729882
3436.705192	752316.084013	40.734900
3440.321766	753731.694857	40.739917
3443.060361	755138.227550	40.744935
3446.758904	756542.176989	40.749952
3450.072537	757958.779807	40.754970
3453.374369	759387.867983	40.759988
3457.072563	760802.892492	40.765005
3460.553705	762201.606030	40.770010
3463.535059	763565.495084	40.775015
3466.909979	764875.721844	40.780020
3470.077046	766135.617440	40.785024
3473.221491	767316.045391	40.790029
3476.136597	768438.860220	40.795034
3478.935706	769482.387339	40.800039
3482.278644	770459.952159	40.805044
3484.922436	771368.682256	40.810048
3487.725072	772210.726912	40.815053
3490.221698	772984.658743	40.820058
3492.694050	773695.919081	40.825063
3494.832826	774331.527526	40.830068
3496.633579	774912.234424	40.835072
3498.966386	775434.068568	40.840077
3500.939807	775919.000091	40.845082
3502.851074	776320.956928	40.850087
3504.580608	776674.924489	40.855092
3505.851679	776979.232571	40.860096
3507.429668	777241.439895	40.865101
3508.801499	777466.213487	40.870106
3510.204015	777633.090776	40.875111
3511.254030	777777.036517	40.880116
3512.226958	777865.816789	40.885120
3513.390267	777923.950018	40.890125
3514.287952	777969.132801	40.895130
3515.360951	777971.908703	40.900135
3516.117448	777942.547469	40.905140
3516.751162	777878.949469	40.910144
3517.931423	777792.323915	40.915149
3518.017778	777703.712366	40.920154
3518.628956	777577.998252	40.925159
3519.164269	777437.675338	40.930164
3519.454668	777273.565845	40.935168
3519.997965	777089.819271	40.940173
3520.068514	776905.063204	40.945178
3520.071961	776701.557775	40.950183
3520.804291	776497.040103	40.955188
3521.046946	776261.680761	40.960192
3521.017516	776022.814064	40.965197
3521.253646	775778.086063	40.970202
3521.700762	775511.306628	40.975207
3521.954542	775250.605639	40.980212
3521.894437	774986.746675	40.985216
3522.001574	774691.730110	40.990221
3522.098276	774414.480209	40.995226
3522.170307	774113.586237	41.000231
3522.378850	773815.365966	41.005236
3522.263883	773513.887344	41.010240
3522.492266	773195.397162	41.015245
3522.557933	772902.187080	41.020250
3522.373429	772570.636673	41.025255
3522.518070	772256.651209	41.030260
3522.310993	771929.607378	41.035264
3522.717811	771600.526380	41.040269
3522.102643	771284.161954	41.045274
3521.956090	770952.877373	41.050279
3521.852465	770624.428421	41.055284
3522.297328	770300.357885	41.060288
3521.985860	769973.540314	41.065293
3521.659275	769648.090517	41.070298
3521.948440	769308.973433	41.075303
3521.886426	768980.789653	41.080308
3521.317586	768648.091914	41.085312
3521.872321	768318.101357	41.090317
3521.669428	767995.170683	41.095322
3521.736189	767652.663297	41.100327
3521.493709	767316.944057	41.105332
3521.089342	766981.433610	41.110336
3521.222338	766643.650289	41.115341
3520.952666	766328.249810	41.120346
3521.076035	765987.431271	41.125351
3520.797374	765654.650467	41.130356
3520.893359	765333.132784	41.135360
3520.806434	765005.172464	41.140365
3520.566082	764669.826945	41.145370
3520.418848	764343.178930	41.150375
3520.227036	764016.524056	41.155380
3520.088565	763694.876221	41.160384
3520.086512	763367.224775	41.165389
3519.880769	763052.218279	41.170394
3519.755431	762737.431908	41.175399
3519.851826	762415.295972	41.180404
3519.238660	762101.500763	41.185408
3519.402285	761779.967789	41.190413
3519.180807	761474.122034	41.195418
3519.060310	761152.658618	41.200423
3518.997202	760839.854667	41.205428
3518.833565	760540.029506	41.210432
3519.253838	760230.031232	41.215437
3518.490827	759926.284502	41.220442
3518.277138	759620.066450	41.225447
3518.511438	759314.798206	41.230452
3518.152722	759018.497768	41.235456
3518.043586	758714.742494	41.240461
3517.672283	758429.030711	41.245466
3517.669182	758134.956442	41.250471
3517.715103	757838.395080	41.255476
3517.447049	757547.006917	41.260480
3517.671748	757262.485426	41.265485
3517.590134	756982.298095	41.270490
3517.374704	756684.599792	41.275495
3517.414845	756403.976231	41.280500
3516.903926	756121.952512	41.285504
3517.145858	755829.920874	41.290509
3517.035471	755557.436426	41.295514
3516.865540	755265.204462	41.300519
3516.844961	755002.509891	41.305524
3516.433067	754725.454171	41.310528
3516.617054	754440.291306	41.315533
3516.324458	754175.984014	41.320538
3516.283782	753897.405143	41.325543
3516.415403	753625.997148	41.330548
3515.920306	753362.436027	41.335552
3516.195170	753080.219945	41.340557
3516.009617	752816.885287	41.345562
3515.810868	752555.272339	41.350567
3516.272250	752282.824162	41.355572
3515.723384	752017.200965	41.360576
3515.892242	751760.834450	41.365581
3515.339140	751491.193120	41.370586
3515.384685	751234.039206	41.375591
3515.075349	750967.698192	41.380596
3514.925085	750725.625729	41.385600
3515.141697	750471.629096	41.390605
3515.022805	750216.938555	41.395610
3514.742027	749960.191460	41.400615
3514.834975	749723.234822	41.405620
3514.434442	749477.607590	41.410624
3514.548026	749229.614869	41.415629
3514.485443	748992.068723	41.420634
3513.703789	748748.309548	41.425639
3514.323486	748511.377136	41.430644
3513.751626	748270.829544	41.435648
3513.941625	748028.764988	41.440653
3513.600408	747801.605781	41.445658
3513.632488	747571.709674	41.450663
3513.850452	747340.787678	41.455668
3513.586702	747115.028843	41.460672
3513.574440	746883.142927	41.465677
3513.362985	746663.639083	41.470682
3513.230251	746431.561975	41.475687
3513.161751	746203.965225	41.480692
3512.910179	745985.536364	41.485696
3513.180342	745767.212912	41.490701
3512.695074	745553.407579	41.495706
3512.564668	745332.814950	41.500711
3513.021889	745115.925420	41.505716
3512.485055	744896.722398	41.510720
3512.364733	744687.282309	41.515725
3512.383770	744480.087747	41.520730
3512.222867	744272.423063	41.525735
3512.129760	744056.336799	41.530740
3512.008488	743856.169530	41.535744
3512.058378	743646.278035	41.540749
3511.821521	743452.547203	41.545754
3511.685295	743250.240887	41.550759
3511.820359	743055.845490	41.555764
3511.367590	742865.251041	41.560768
3511.211860	742664.762494	41.565773
3511.311916	742485.885894	41.570778
3511.255030	742283.442759	41.575783
3511.312469	742096.701564	41.580788
3510.963639	741908.836193	41.585792
3511.072761	741719.159747	41.590797
3511.118386	741522.911541	41.595802
3510.961011	741339.600452	41.600807
3510.733076	741155.851648	41.605812
3510.658122	740976.870905	41.610816
3510.802932	740790.875803	41.615821
3510.600068	740605.032713	41.620826
3510.462827	740430.699369	41.625831
3510.679190	740255.710188	41.630836
3510.089476	740069.671153	41.635840
3510.292788	739903.036020	41.640845
3510.497005	739732.093561	41.645850
3510.418021	739552.042514	41.650855
3510.252813	739374.079368	41.655860
3510.129482	739207.384687	41.660864
3510.394334	739045.717971	41.665869
3510.016554	738872.033299	41.670874
3509.710118	738698.580416	41.675879
3509.514752	738535.643592	41.680884
3509.281824	738368.603127	41.685888
3509.762172	738208.664950	41.690893
3509.386383	738050.893644	41.695898
3509.477664	737885.966526	41.700903
3509.133743	737735.704535	41.705908
3509.248532	737577.249032	41.710912
3509.332512	737419.141851	41.715917
3509.287544	737266.842354	41.720922
3508.921475	737117.512562	41.725927
3509.343875	736951.076392	41.730932
3508.884722	736808.684092	41.735936
3509.092469	736650.986639	41.740941
3509.056013	736511.240963	41.745946
3509.060382	736359.559374	41.750951
3508.825328	736200.639521	41.755956
3508.515319	736056.427565	41.760960
3508.770901	735907.170418	41.765965
3508.376974	735773.954312	41.770970
3508.341938	735634.341582	41.775975
3508.927180	735482.844372	41.780980
3508.496195	735340.520298	41.785984
3508.364035	735200.916077	41.790989
3508.429641	735067.711296	41.795994
3508.088311	734920.712290	41.800999
3508.085711	734785.138219	41.806004
3507.888710	734648.505006	41.811008
3507.972828	734504.546524	41.816013
3508.020000	734385.242961	41.821018
3507.737848	734251.686120	41.826023
3507.846085	734114.250869	41.831028
3507.447481	733983.233436	41.836032
3507.661613	733854.686824	41.841037
3507.531457	733727.383168	41.846042
3507.402025	733601.265514	41.851047
3507.576832	733488.907858	41.856052
3507.387809	733367.598497	41.861056
3507.517443	733228.411860	41.866061
3507.461771	733107.670648	41.871066
3507.355795	732987.777600	41.876071
3507.315914	732865.297327	41.881076
3506.943644	732762.575394	41.886080
3507.119447	732627.826733	41.891085
3506.942451	732509.176102	41.896090
3506.884067	732399.069864	41.901095
3506.740913	732279.717091	41.906100
3506.863284	732176.658400	41.911104
3506.825565	732054.165476	41.916109
3506.530290	731953.549679	41.921114
3506.593060	731845.198442	41.926119
3506.665607	731731.496307	41.931124
3506.526135	731622.878414	41.936128
3506.589324	731522.049464	41.941133
3506.563533	731419.005613	41.946138
3506.725565	731296.963414	41.951143
3506.373912	731196.941765	41.956148
3506.464311	731096.647749	41.961152
3506.138216	730979.435435	41.966157
3506.428448	730876.530553	41.971162
3506.174764	730781.093148	41.976167
3506.370566	730672.159498	41.981172
3506.084759	730578.408814	41.986176
3506.292460	730475.264865	41.991181
3505.799108	730375.256498	41.996186
3506.211990	730282.278392	42.001191
3506.029435	730178.254171	42.006196
3505.651241	730082.234807	42.011200
3505.734086	729986.534343	42.016205
3505.907772	729897.404991	42.021210
3505.555671	729797.415695	42.026215
3505.660534	729709.137643	42.031220
3505.663095	729616.318790	42.036224
3505.221429	729530.011243	42.041229
3505.246738	729439.266889	42.046234
3505.223053	729356.850911	42.051239
3505.371400	729269.898259	42.056244
3505.401176	729193.267033	42.061248
3505.230720	729103.541938	42.066253
3505.376074	729020.797428	42.071258
3505.312689	728927.733958	42.076263
3505.387126	728850.646323	42.081268
3505.369503	728780.904351	42.086272
3505.616819	728680.703215	42.091277
3505.433935	728586.318135	42.096282
3505.075936	728503.750631	42.101287
3505.191177	728420.955477	42.106292
3505.121982	728346.809508	42.111296
3505.275649	728249.838502	42.116301
3505.086864	728177.444594	42.121306
3505.092382	728087.976478	42.126311
3505.244113	728013.840517	42.131316
3504.894421	727935.328137	42.136320
3505.121492	727858.949016	42.141325
3505.067476	727773.549620	42.146330
3505.139652	727698.581749	42.151335
3505.065806	727612.886702	42.156340
3504.394712	727540.765021	42.161344
3504.581274	727457.898781	42.166349
3504.929733	727397.596750	42.171354
3504.677016	727318.319266	42.176359
3504.454849	727239.085508	42.181364
3504.483371	727180.667889	42.186368
3504.505463	727097.082006	42.191373
3504.638378	727032.205201	42.196378
3504.348522	726964.177259	42.201383
3504.365395	726893.719836	42.206388
3504.327171	726831.049761	42.211392
3503.997337	726760.301656	42.216397
3504.391967	726678.978664	42.221402
3504.323643	726627.658423	42.226407
3504.537028	726556.026020	42.231412
3504.514238	726486.612169	42.236416
3504.341179	726419.105436	42.241421
3504.286430	726355.047073	42.246426
3504.194253	726292.233145	42.251431
3504.151475	726223.414971	42.256436
3504.096441	726162.724583	42.261440
3504.196395	726107.656968	42.266445
3503.990099	726050.707083	42.271450
3504.197169	725984.075431	42.276455
3504.069215	725911.849638	42.281460
3503.870933	725846.671321	42.286464
3504.040154	725784.206731	42.291469
3504.043074	725722.165575	42.296474
3503.807067	725665.862125	42.301479
3504.117473	725604.809901	42.306484
3503.966147	725555.924829	42.311488
3503.811539	725491.132909	42.316493
3503.817904	725430.724294	42.321498
3503.828438	725383.248549	42.326503
3503.761992	725312.444431	42.331508
3503.987820	725265.675769	42.336512
3503.722478	725203.575917	42.341517
3503.778848	725149.946229	42.346522
3503.391822	725086.577121	42.351527
3503.781676	725029.125181	42.356532
3503.531882	724981.640579	42.361536
3503.385758	724930.421703	42.366541
3503.415856	724880.709703	42.371546
3503.407422	724836.851713	42.376551
3503.411737	724774.654502	42.381556
3503.562820	724743.258559	42.386560
3503.582031	724695.034018	42.391565
3503.350871	724635.303091	42.396570
3503.184833	724591.420277	42.401575
3503.663057	724528.944657	42.406580
3503.377887	724490.037055	42.411584
3503.513210	724436.191428	42.416589
3503.156171	724390.356656	42.421594
3503.223813	724345.095754	42.426599
3503.633684	724287.982274	42.431604
3503.424878	724250.498222	42.436608
3503.381966	724197.869989	42.441613
3503.314793	724140.239566	42.446618
3503.087823	724101.568326	42.451623
3503.685405	724051.063659	42.456628
3503.021402	724014.545899	42.461632
3503.293846	723961.417970	42.466637
3503.095254	723916.942174	42.471642
3502.902354	723871.672164	42.476647
3502.976924	723828.637691	42.481652
3503.110296	723790.797614	42.486656
3503.062307	723746.841230	42.491661
3503.119103	723709.856047	42.496666
3502.853105	723667.025708	42.501671
3503.160966	723609.825264	42.506676
3503.269430	723578.729331	42.511680
3502.990988	723531.588068	42.516685
3503.053107	723489.148683	42.521690
3503.069021	723448.203731	42.526695
3503.056955	723391.252912	42.531700
3502.781892	723359.872560	42.536704
3503.103906	723311.242918	42.541709
3503.104201	723264.599317	42.546714
3502.599201	723234.148714	42.551719
3503.085620	723196.445848	42.556724
3502.881725	723159.352575	42.561728
3502.392830	723119.183376	42.566733
3503.113056	723087.736657	42.571738
3502.669628	723042.949626	42.576743
3502.783899	722994.897720	42.581748
3502.712597	722971.909097	42.586752
3503.024368	722926.401797	42.591757
3502.806427	722895.258091	42.596762
3502.487425	722858.678194	42.601767
3502.596776	722814.492567	42.606772
3502.785104	722783.430016	42.611776
3502.776703	722750.615291	42.616781
3502.834387	722708.370918	42.621786
3502.569790	722672.227349	42.626791
3502.700258	722639.438807	42.631796
3502.511790	722600.506312	42.636800
3502.738898	722567.453653	42.641805
3502.653170	722536.633755	42.646810
3502.633721	722493.806162	42.651815
3502.529863	722464.030020	42.656820
3502.265764	722423.869865	42.661824
3502.344453	722389.601691	42.666829
3502.285206	722369.881253	42.671834
3502.357454	722346.024418	42.676839
3502.227885	722319.970038	42.681844
3502.288381	722295.321816	42.686848
3502.219708	722263.457027	42.691853
3502.451046	722237.045300	42.696858
3502.604173	722203.854695	42.701863
3502.250171	722177.242058	42.706868
3502.492902	722134.220555	42.711872
3502.444396	722101.162009	42.716877
3502.567609	722074.470181	42.721882
3502.076582	722040.145983	42.726887
3502.545637	722012.107838	42.731892
3502.297826	721990.335475	42.736896
3502.414383	721963.941847	42.741901
3502.482065	721932.648166	42.746906
3502.511318	721897.592908	42.751911
3502.427539	721861.862107	42.756916
3502.405758	721831.376055	42.761920
3502.339504	721801.393009	42.766925
3502.200004	721778.313187	42.771930
3501.809678	721753.886586	42.776935
3502.194695	721721.696855	42.781940
3502.321570	721705.117037	42.786945
3502.063581	721676.255931	42.791949
3502.478935	721638.557730	42.796954
3502.181800	721615.503504	42.801959
3502.411928	721580.810338	42.806964
3502.039038	721563.569150	42.811969
3502.162608	721531.768937	42.816973
3502.271511	721525.454502	42.821978
3501.875879	721488.187108	42.826983
3501.848296	721465.187077	42.831988
3502.186839	721442.076901	42.836993
3501.835103	721416.601765	42.841997
3502.460417	721388.337379	42.847002
3502.098835	721368.317463	42.852007
3502.143359	721336.876623	42.857012
3501.876220	721315.353579	42.862017
3501.916476	721290.705717	42.867021
3502.264808	721261.247169	42.872026
3502.202813	721239.491706	42.877031
3502.177303	721214.656165	42.882036
3501.883904	721184.311782	42.887041
3501.647177	721162.386668	42.892045
3501.992001	721147.703375	42.897050
3502.468152	721128.486481	42.902055
3502.394022	721105.542728	42.907060
3502.039752	721074.117214	42.912065
3501.976059	721053.303590	42.917069
3501.963912	721013.442034	42.922074
3502.002907	721008.973283	42.927079
3501.981723	720972.038345	42.932084
3502.099875	720958.235070	42.937089
3501.941403	720924.099201	42.942093
3501.899345	720905.413668	42.947098
3501.910200	720889.099308	42.952103
3501.943686	720869.161647	42.957108
3501.844082	720848.601358	42.962113
3502.280476	720817.192961	42.967117
3502.109358	720802.544737	42.972122
3501.983017	720769.642498	42.977127
3501.836834	720751.469658	42.982132
3501.679652	720741.479852	42.987137
3501.555963	720716.956547	42.992141
3501.726557	720708.846292	42.997146
3501.729991	720702.796580	43.002151
3502.062525	720669.867700	43.007156
3501.679200	720654.411358	43.012161
3501.483911	720639.518922	43.017165
3501.709609	720611.863365	43.022170
3501.273057	720604.299598	43.027175
3501.814898	720586.359788	43.032180
3501.919038	720554.311126	43.037185
3501.345335	720549.992963	43.042189
3501.874494	720536.914422	43.047194
3501.553103	720518.968364	43.052199
3501.688753	720503.773073	43.057204
3501.726810	720502.031367	43.062209
3501.600961	720474.582202	43.067213
3501.591059	720458.072087	43.072218
3501.314043	720456.084927	43.077223
3501.699128	720436.187297	43.082228
3501.493775	720415.990508	43.087233
3501.881741	720404.125139	43.092237
3502.170609	720379.284736	43.097242
3502.046478	720363.586678	43.102247
3502.292979	720333.447479	43.107252
3501.778157	720313.648683	43.112257
3501.853277	720294.248210	43.117261
3501.536865	720267.127367	43.122266
3501.584385	720255.615563	43.127271
3502.003413	720237.794474	43.132276
3502.303861	720217.265686	43.137281
3501.844471	720206.135101	43.142285
3502.063401	720169.156919	43.147290
3502.092391	720150.160428	43.152295
3501.931445	720121.079529	43.157300
3502.043135	720111.193295	43.162305
3501.928582	720087.509605	43.167309
3501.793083	720050.539879	43.172314
3501.587754	720053.797045	43.177319
3501.751531	720032.199463	43.182324
3501.614715	720022.998828	43.187329
3501.592202	720007.977533	43.192333
3501.840245	719986.266732	43.197338
3501.549123	719964.545797	43.202343
3501.619478	719952.038041	43.207348
3501.572676	719940.541389	43.212353
3501.702290	719928.618862	43.217357
3501.992466	719905.710773	43.222362
3501.535683	719899.438998	43.227367
3501.998583	719872.237674	43.232372
3501.377077	719864.009552	43.237377
3501.636058	719851.172942	43.242381
3502.003886	719817.292679	43.247386
3501.591889	719814.286302	43.252391
3502.061125	719784.009133	43.257396
3502.010157	719761.206610	43.262401
3501.493456	719754.696681	43.267405
3501.821407	719720.227543	43.272410
3501.643366	719715.744375	43.277415
3501.864394	719696.467168	43.282420
3501.860843	719676.532773	43.287425
3501.477068	719658.495985	43.292429
3502.112093	719651.398932	43.297434
3501.762106	719634.695435	43.302439
3501.734718	719604.549273	43.307444
3501.746405	719590.562967	43.312449
3501.619730	719569.260136	43.317453
3501.966432	719555.317589	43.322458
3501.436420	719539.288325	43.327463
3501.895955	719513.921239	43.332468
3501.449393	719507.498705	43.337473
3501.351855	719492.290516	43.342477
3501.718862	719467.484078	43.347482
3501.510689	719461.022114	43.352487
3501.804284	719447.286527	43.357492
3502.223712	719431.794434	43.362497
3501.721800	719418.537397	43.367501
3501.813571	719382.717340	43.372506
3501.755442	719373.701350	43.377511
3501.811289	719353.161268	43.382516
3501.711216	719327.439768	43.387521
3501.704631	719313.406425	43.392525
3501.552602	719305.397714	43.397530
3501.256609	719289.428479	43.402535
3501.639008	719258.915798	43.407540
3501.397318	719247.450396	43.412545
3501.266081	719248.067240	43.417549
3501.547418	719238.548675	43.422554
3501.306629	719223.760407	43.427559
3501.551645	719210.875531	43.432564
3501.702004	719205.693116	43.437569
3501.781715	719188.471382	43.442573
3502.293600	719150.993944	43.447578
3501.696697	719151.489376	43.452583
3501.650163	719127.841311	43.457588
3501.731543	719120.488153	43.462593
3501.733540	719112.701769	43.467597
3502.012313	719078.684448	43.472602
3501.781757	719075.796596	43.477607
3501.628569	719036.593599	43.482612
3501.798977	719023.869544	43.487617
3501.497538	719006.363265	43.492621
3501.629637	718986.107242	43.497626
3501.426858	718978.652136	43.502631
3501.836714	718967.872180	43.507636
3501.611017	718957.296425	43.512641
3501.627056	718928.231711	43.517645
3501.849317	718915.895677	43.522650
3501.768095	718906.635026	43.527655
3501.471549	718883.672310	43.532660
3501.733998	718869.494573	43.537665
3501.565084	718854.445799	43.542669
3501.683248	718829.529808	43.547674
3501.486608	718825.495585	43.552679
3501.214259	718812.199643	43.557684
3501.278807	718808.816578	43.562689
3501.177488	718792.814220	43.567693
3501.505413	718773.715600	43.572698
3501.495429	718771.683903	43.577703
3501.317725	718753.313528	43.582708
3501.680733	718760.990435	43.587713
3501.680887	718736.093667	43.592717
3501.910725	718720.433208	43.597722
3501.806489	718704.282377	43.602727
3501.770032	718683.309543	43.607732
3501.897288	718672.675100	43.612737
3501.671954	718651.435824	43.617741
3501.646338	718620.889051	43.622746
3501.463480	718623.051945	43.627751
3501.380971	718599.755501	43.632756
3501.615103	718580.523152	43.637761
3501.208513	718565.413941	43.642765
3501.126293	718568.105777	43.647770
3501.323623	718562.220855	43.652775
3501.707174	718557.693854	43.657780
3501.630362	718534.247497	43.662785
3501.558900	718523.248931	43.667789
3501.763600	718510.766413	43.672794
3501.543712	718484.863730	43.677799
3501.371375	718474.675319	43.682804
3501.598057	718472.604439	43.687809
3501.635634	718460.496641	43.692813
3501.715320	718425.368835	43.697818
3501.226652	718427.284731	43.702823
3501.336471	718425.778720	43.707828
3501.531130	718406.651690	43.712833
3501.468568	718389.997391	43.717837
3501.539880	718385.174714	43.722842
3501.576710	718389.533245	43.727847
3501.481099	718359.989031	43.732852
3501.503199	718347.189262	43.737857
3501.567378	718345.343595	43.742861
3501.915242	718325.397501	43.747866
3501.556562	718304.576160	43.752871
3501.642649	718299.552601	43.757876
3501.758077	718284.654202	43.762881
3501.713920	718255.448303	43.767885
3501.964651	718240.428271	43.772890
3501.523180	718225.968984	43.777895
3501.382095	718206.599389	43.782900
3501.685604	718198.067950	43.787905
3501.542529	718184.650448	43.792909
3501.894369	718160.636222	43.797914
3501.300101	718154.534638	43.802919
3501.225401	718144.528083	43.807924
3501.310243	718141.389388	43.812929
3501.231811	718130.837847	43.817933
3501.215200	718101.329264	43.822938
3501.669779	718100.758204	43.827943
3501.561155	718095.171510	43.832948
3501.736597	718084.280362	43.837953
3501.449972	718064.884891	43.842957
3501.732259	718033.045108	43.847962
3501.569812	718041.801500	43.852967
3501.545320	718008.573937	43.857972
3501.393101	717993.024855	43.862977
3501.058539	717990.798606	43.867981
3501.574040	717979.156732	43.872986
3501.170246	717980.364304	43.877991
3501.575691	717960.606226	43.882996
3501.757801	717944.505806	43.888001
3501.445712	717945.747829	43.893005
3501.541198	717916.368869	43.898010
3501.459358	717897.931172	43.903015
3501.556131	717905.752065	43.908020
3501.448231	717897.437108	43.913025
3501.344482	717886.095838	43.918029
3501.232103	717855.858210	43.923034
3501.352181	717850.878366	43.928039
3501.233133	717840.531572	43.933044
3501.537461	717839.241317	43.938049
3501.241148	717830.610225	43.943053
3501.571146	717818.155571	43.948058
3501.528040	717806.605769	43.953063
3501.683840	717804.596041	43.958068
3501.949090	717775.734144	43.963073
3501.507974	717766.283697	43.968077
3501.734388	717755.482902	43.973082
3501.595253	717731.201375	43.978087
3501.539999	717712.610072	43.983092
3501.612717	717694.890406	43.988097
3501.400180	717697.653658	43.993101
3501.631002	717668.102659	43.998106
3501.908694	717660.517372	44.003111
3501.730161	717646.013628	44.008116
3501.956000	717627.276482	44.013121
3501.614128	717613.940517	44.018125
3501.659079	717593.596323	44.023130
3501.379411	717588.781586	44.028135
3501.513243	717576.011777	44.033140
3501.455374	717568.233848	44.038145
3501.286342	717554.670817	44.043149
3501.460518	717532.321029	44.048154
3501.610536	717530.262589	44.053159
3501.412027	717522.210244	44.058164
3501.805693	717508.554152	44.063169
3501.541953	717483.846075	44.068173
3501.424097	717469.083984	44.073178
3501.733036	717474.836505	44.078183
3501.582473	717457.103632	44.083188
3501.613126	717425.799155	44.088193
3501.719050	717432.478109	44.093197
3501.663809	717411.257176	44.098202
3501.525728	717377.549849	44.103207
3501.142816	717382.027871	44.108212
3501.477524	717376.466642	44.113217
3501.564929	717368.466107	44.118221
3501.670316	717336.156879	44.123226
3501.227382	717337.619024	44.128231
3501.509139	717335.290749	44.133236
3501.766199	717318.184671	44.138241
3501.330789	717305.310104	44.143245
3501.654924	717288.688919	44.148250
3501.631661	717289.486475	44.153255
3501.444805	717265.409899	44.158260
3501.405904	717238.679783	44.163265
3501.114685	717237.339042	44.168269
3501.209635	717243.027877	44.173274
3501.222118	717235.337221	44.178279
3501.434008	717220.768222	44.183284
3501.297760	717190.482533	44.188289
3501.392655	717197.560333	44.193293
3501.746305	717186.787386	44.198298
3501.701116	717167.300329	44.203303
3501.513173	717148.134447	44.208308
3501.569908	717137.013664	44.213313
3501.388317	717142.153010	44.218317
3501.650930	717110.759422	44.223322
3501.856796	717088.353610	44.228327
3501.824008	717076.503466	44.233332
3501.897243	717050.498297	44.238337
3501.520452	717043.417452	44.243341
3501.466939	717037.523312	44.248346
3501.503845	717002.942271	44.253351
3501.450960	716990.549666	44.258356
3501.600051	716988.590459	44.263361
3501.730512	716991.694104	44.268365
3501.766783	716958.402731	44.273370
3501.413045	716944.125146	44.278375
3501.359900	716934.411219	44.283380
3501.729687	716915.499879	44.288385
3501.321367	716907.580826	44.293389
3501.314437	716889.178135	44.298394
3501.256576	716886.608223	44.303399
3501.367762	716877.809592	44.308404
3501.099481	716856.721674	44.313409
3501.283552	716856.244848	44.318413
3501.166536	716842.820887	44.323418
3501.211905	716850.552048	44.328423
3501.102006	716846.899382	44.333428
3501.537517	716839.981768	44.338433
3501.165666	716822.482546	44.343437
3501.308532	716806.138397	44.348442
3501.581767	716800.735768	44.353447
3501.383884	716804.786663	44.358452
3501.546059	716794.094463	44.363457
3501.522375	716776.934465	44.368461
3501.392379	716758.055755	44.373466
3501.327321	716760.844547	44.378471
3501.439512	716757.700818	44.383476
3501.448155	716726.794227	44.388481
3501.009118	716711.587805	44.393485
3501.328791	716702.704931	44.398490
3501.475084	716705.309993	44.403495
3501.153663	716699.162243	44.408500
3501.667376	716689.900039	44.413505
3501.003229	716675.822114	44.418509
3501.528070	716649.046569	44.423514
3501.599838	716658.212166	44.428519
3501.523052	716658.869804	44.433524
3501.711832	716637.556981	44.438529
3501.430282	716622.870057	44.443533
3501.712554	716620.739934	44.448538
3501.377474	716598.422209	44.453543
3501.508785	716570.223207	44.458548
3501.590467	716565.348163	44.463553
3501.487603	716552.665522	44.468557
3501.340167	716538.353153	44.473562
3501.557203	716516.638488	44.478567
3501.235764	716520.957979	44.483572
3501.517836	716512.279552	44.488577
3501.451266	716514.423765	44.493581
3501.457564	716484.459231	44.498586
3501.605278	716471.536623	44.503591
3501.625943	716470.044998	44.508596
3501.562674	716445.003077	44.513601
3501.272516	716430.962155	44.518605
3501.586571	716411.017106	44.523610
3501.781738	716412.324348	44.528615
3501.309101	716394.195968	44.533620
3501.379188	716372.306778	44.538625
3501.209482	716365.637618	44.543629
3501.039614	716353.015357	44.548634
3501.359007	716357.278641	44.553639
3501.270318	716352.481238	44.558644
3501.538698	716325.399780	44.563649
3501.319338	716332.629461	44.568653
3501.510613	716321.237318	44.573658
3501.613205	716304.253925	44.578663
3501.640366	716296.510375	44.583668
3501.580307	716279.653030	44.588673
3501.344866	716274.383736	44.593677
3501.201588	716262.253042	44.598682
3500.973788	716238.229892	44.603687
3501.352156	716230.130583	44.608692
3501.379538	716214.548520	44.613697
3501.297438	716224.236120	44.618701
3501.421227	716214.938613	44.623706
3501.330015	716211.679462	44.628711
3501.300742	716195.809065	44.633716
3501.595381	716171.352118	44.638721
3501.019522	716175.862659	44.643725
3501.265762	716166.991357	44.648730
3501.216834	716164.915852	44.653735
3501.321305	716150.958079	44.658740
3501.650291	716125.354279	44.663745
3501.329587	716130.517229	44.668749
3501.336025	716124.810984	44.673754
3501.572774	716111.724279	44.678759
3501.244769	716100.219207	44.683764
3501.221415	716067.876765	44.688769
3501.086427	716071.570340	44.693773
3501.193895	716070.361966	44.698778
3501.313943	716069.994900	44.703783
3501.430593	716060.748013	44.708788
3501.361839	716048.257417	44.713793
3500.872670	716042.781849	44.718797
3501.061448	716038.434527	44.723802
3501.285894	716034.527809	44.728807
3500.939241	716027.788399	44.733812
3501.527598	716029.725285	44.738817
3501.502066	716024.173088	44.743821
3501.273779	715999.256332	44.748826
3501.281005	715990.722011	44.753831
3501.314840	715999.944207	44.758836
3501.480135	715981.263010	44.763841
3501.228370	715966.470791	44.768845
3501.337300	715946.409705	44.773850
3501.657239	715946.257661	44.778855
3501.289866	715939.918498	44.783860
3501.618235	715937.433305	44.788865
3501.290145	715912.681620	44.793869
3501.095596	715887.213224	44.798874
3501.372150	715893.418699	44.803879
3500.955731	715887.335661	44.808884
3501.340399	715886.329514	44.813889
3501.336277	715896.947235	44.818893
3501.256418	715870.616431	44.823898
3501.523191	715852.166240	44.828903
3501.333337	715855.472077	44.833908
3501.377740	715838.894260	44.838913
3501.012653	715845.404252	44.843917
3501.155055	715837.591623	44.848922
3501.224157	715808.060812	44.853927
3501.228159	715802.453975	44.858932
3501.611191	715806.210900	44.863937
3501.406389	715800.192054	44.868941
3501.387579	715781.193549	44.873946
3501.381224	715759.960364	44.878951
3501.001549	715752.035479	44.883956
3501.397704	715749.935934	44.888961
3501.230633	715751.997723	44.893965
3501.361691	715750.934243	44.898970
3501.013045	715724.052043	44.903975
3500.862387	715723.432019	44.908980
3501.429592	715704.237275	44.913985
3501.105593	715709.500251	44.918989
3500.857104	715700.511762	44.923994
3501.043136	715700.977202	44.928999
3501.216045	715709.581375	44.934004
3501.402723	715707.764502	44.939009
3501.410359	715702.851583	44.944013
3501.441195	715675.509611	44.949018
3501.505526	715656.794767	44.954023
3501.347802	715663.617926	44.959028
3501.715886	715645.001700	44.964033
3501.656174	715625.662309	44.969037
3501.493644	715606.488705	44.974042
3501.836258	715601.669213	44.979047
3501.155442	715584.466532	44.984052
3501.567048	715575.269598	44.989057
3501.259836	715568.473685	44.994061
3501.285568	715558.000921	44.999066
3501.321934	715553.926607	45.004071
3501.524629	715534.692486	45.009076
3501.500354	715511.576296	45.014081
3501.333063	715512.993192	45.019085
3501.482534	715504.583715	45.024090
3501.443606	715480.179887	45.029095
3501.052849	715470.123141	45.034100
3501.444233	715455.025281	45.039105
3501.510385	715457.693591	45.044109
3501.158699	715459.885188	45.049114
3501.239001	715447.964444	45.054119
3500.853901	715428.033378	45.059124
3501.346124	715418.376419	45.064129
3501.097873	715418.814412	45.069133
3501.077353	715421.000908	45.074138
3501.345998	715421.899246	45.079143
3501.450367	715420.492832	45.084148
3501.565145	715400.379866	45.089153
3501.349333	715371.241911	45.094157
3501.213784	715366.650148	45.099162
3501.535268	715380.142010	45.104167
3501.251352	715363.170976	45.109172
3501.118167	715334.118468	45.114177
3501.057377	715334.029333	45.119181
3500.837334	715329.898052	45.124186
3501.229964	715317.478972	45.129191
3501.004807	715328.927784	45.134196
3500.999744	715316.177499	45.139201
3501.113061	715319.483060	45.144205
3500.752563	715315.126905	45.149210
3500.578205	715319.422700	45.154215
3500.488880	715313.632498	45.159220
3501.396574	715313.581781	45.164225
3501.502865	715316.441965	45.169229
3501.285356	715316.626805	45.174234
3501.279370	715289.289665	45.179239
3500.753263	715285.953175	45.184244
3501.010924	715271.522089	45.189249
3501.383423	715280.143336	45.194253
3501.308549	715273.011094	45.199258
3501.092652	715275.974150	45.204263
3501.294343	715277.181263	45.209268
3501.440943	715263.661600	45.214273
3501.295956	715244.335425	45.219277
3501.360433	715238.122828	45.224282
3501.577498	715228.759204	45.229287
3501.429194	715226.203729	45.234292
3501.451086	715200.995184	45.239297
3501.197456	715189.030025	45.244301
3500.899466	715190.121260	45.249306
3501.511126	715183.173188	45.254311
3501.502520	715194.387931	45.259316
3501.438735	715173.063525	45.264321
3501.269920	715154.931874	45.269325
3500.842741	715141.010668	45.274330
3501.235758	715135.835268	45.279335
3500.958972	715141.338876	45.284340
3500.885985	715136.240484	45.289345
3500.765356	715130.901879	45.294349
3500.899935	715133.310902	45.299354
3501.052140	715135.766628	45.304359
3500.986335	715142.624634	45.309364
3500.922712	715140.303221	45.314369
3500.883626	715142.889789	45.319373
3500.845125	715143.938148	45.324378
3501.100255	715134.320046	45.329383
3500.751317	715120.931660	45.334388
3501.234386	715097.085476	45.339393
3501.025458	715095.036147	45.344397
3501.237130	715095.150068	45.349402
3501.267844	715086.263632	45.354407
3500.963399	715090.283339	45.359412
3501.536382	715083.540045	45.364417
3501.192280	715085.333549	45.369421
3501.112787	715069.866264	45.374426
3501.131348	715048.726402	45.379431
3500.789618	715055.084289	45.384436
3501.293875	715042.199806	45.389441
3500.688933	715034.013764	45.394445
3500.821022	715037.911740	45.399450
3501.024918	715039.366609	45.404455
3500.875347	715042.318786	45.409460
3500.959252	715035.705893	45.414465
3500.968390	715040.914231	45.419469
3501.101892	715041.041071	45.424474
3501.348602	715037.328685	45.429479
3500.755367	715039.461070	45.434484
3501.166839	715036.664181	45.439489
3501.143251	715020.989099	45.444493
3500.968234	715004.098579	45.449498
3501.264040	714993.530866	45.454503
3500.811525	714989.288981	45.459508
3500.871186	714985.805952	45.464513
3501.061774	714990.785867	45.469517
3501.234507	714993.784033	45.474522
3500.920790	714989.668064	45.479527
3501.001345	714989.109010	45.484532
3501.074750	714998.077678	45.489537
3501.113177	714994.796631	45.494541
3501.281421	714986.978945	45.499546
3501.217354	714948.139046	45.504551
3501.020357	714953.133414	45.509556
3501.184140	714946.854575	45.514561
3501.018063	714951.000335	45.519565
3501.072952	714943.002870	45.524570
3501.327007	714950.998999	45.529575
3500.995693	714948.424064	45.534580
3501.396455	714935.754993	45.539585
3501.175955	714910.784107	45.544589
3500.969258	714914.490037	45.549594
3501.283002	714901.537587	45.554599
3501.349362	714898.996156	45.559604
3501.174469	714900.513646	45.564609
3501.065678	714903.012570	45.569613
3500.961969	714900.747334	45.574618
3501.135633	714891.241654	45.579623
3501.065564	714875.524365	45.584628
3501.140890	714862.660873	45.589633
3501.330460	714849.282300	45.594637
3501.436032	714860.081673	45.599642
3501.460596	714852.684553	45.604647
3501.231976	714857.634585	45.609652
3501.330790	714822.885501	45.614657
3501.428049	714812.350373	45.619661
3501.220304	714806.877102	45.624666
3501.609512	714806.167794	45.629671
3501.120430	714798.607415	45.634676
3501.270897	714773.029014	45.639681
3501.346034	714767.955540	45.644685
3501.159751	714770.417691	45.649690
3501.486320	714762.176684	45.654695
3501.390625	714761.795598	45.659700
3501.340034	714741.361057	45.664705
3501.298474	714736.604562	45.669709
3501.153363	714722.685669	45.674714
3501.163566	714708.989182	45.679719
3501.311024	714725.487996	45.684724
3501.396268	714705.427873	45.689729
3501.507305	714683.477910	45.694733
3501.450865	714671.578667	45.699738
3501.554949	714669.626364	45.704743
3501.249581	714672.108222	45.709748
3501.459175	714634.263659	45.714753
3501.079966	714630.853008	45.719757
3501.335550	714619.894520	45.724762
3501.638433	714618.504789	45.729767
3501.072354	714619.293059	45.734772
3501.271414	714592.515212	45.739777
3501.293748	714581.644839	45.744781
3501.047964	714581.933604	45.749786
3501.323664	714571.815267	45.754791
3500.946796	714582.148902	45.759796
3501.199305	714574.217671	45.764801
3501.255696	714578.624568	45.769805
3500.836617	714575.270103	45.774810
3501.110470	714531.410456	45.779815
3500.857371	714480.144984	45.784820
3500.756033	714355.861739	45.789825
3500.869443	714196.557687	45.794829
3500.540568	713968.446703	45.799834
3500.767691	713682.523898	45.804839
3499.962083	713353.636324	45.809844
3500.068178	712951.928215	45.814849
3499.875577	712503.646115	45.819853
3499.498097	711992.285051	45.824858
3499.364043	711429.527161	45.829863
3498.760056	710824.862493	45.834868
3498.548219	710142.791994	45.839873
3498.443985	709404.693778	45.844877
3497.679335	708618.724420	45.849882
3497.382525	707770.829407	45.854887
3496.861330	706877.643330	45.859892
3496.736138	705901.201058	45.864897
3496.329505	704883.712030	45.869901
3495.579732	703791.437937	45.874906
3495.184909	702652.011655	45.879911
3494.772255	701436.851921	45.884916
3494.036578	700176.793957	45.889921
3493.399668	698840.829264	45.894925
3492.376981	697456.547998	45.899930
3491.818207	696007.129301	45.904935
3490.811682	694503.485213	45.909940
3490.134978	692946.057539	45.914945
3489.299769	691322.511454	45.919949
3488.440295	689648.664104	45.924954
3487.717740	687908.634710	45.929959
3486.809497	686118.569058	45.934964
3485.938373	684250.767948	45.939969
3485.343864	682327.905492	45.944973
3484.188821	680359.003938	45.949978
3483.361127	678316.884626	45.954983
3482.114439	676223.054021	45.959988
3480.986173	674067.920126	45.964993
3479.975794	671856.529100	45.969997
3478.911344	669597.300904	45.975002
3477.983538	667265.132071	45.980007
3476.260886	664896.001095	45.985012
3475.120926	662453.573547	45.990017
3473.803818	659969.123818	45.995021
3472.342358	657420.697886	46.000026
3470.905139	654824.854790	46.005031
3469.720074	652190.117470	46.010036
3468.331230	649479.055534	46.015041
3467.008674	646726.009031	46.020045
3465.560406	643912.730854	46.025050
3464.217689	641044.290529	46.030055
3462.668594	638135.458528	46.035060
3461.144344	635157.444449	46.040065
3459.835741	632144.304342	46.045069
3457.583428	629067.666013	46.050074
3456.591434	625945.099169	46.055079
3454.530467	622779.312025	46.060084
3453.300228	619549.012451	46.065089
3451.775611	616280.306756	46.070093
3449.515054	612941.901603	46.075098
3447.847536	609558.354888	46.080103
3445.897247	606144.633804	46.085108
3444.174074	602675.792590	46.090113
3442.424430	599149.374437	46.095117
3440.583704	595585.036929	46.100122
3438.600042	591967.142310	46.105127
3436.732685	588289.229352	46.110132
3434.914386	584574.290868	46.115137
3432.912023	580811.735296	46.120141
3430.620481	577001.450089	46.125146
3428.938368	573139.282856	46.130151
3426.919929	569230.743284	46.135156
3424.612136	565283.902861	46.140161
3422.481361	561284.816431	46.145165
3420.183571	557253.107012	46.150170
3418.303426	553171.230039	46.155175
3416.106322	549047.294456	46.160180
3413.888914	544866.962168	46.165185
3411.540206	540647.520304	46.170189
3409.200848	536390.645864	46.175194
3407.136454	532081.545347	46.180199
3404.555726	527741.224315	46.185204
3402.460894	523339.969988	46.190209
3400.189611	518909.229107	46.195213
3397.406944	514437.736258	46.200218
3394.915046	509914.834527	46.205223
3392.767534	505363.194804	46.210228
3390.299131	500774.836310	46.215233
3387.647203	496127.878624	46.220237
3384.845299	491470.563680	46.225242
3382.538106	486746.017040	46.230247
3379.789990	482011.622740	46.235252
3377.253960	477226.225123	46.240257
3374.539822	472402.590257	46.245261
3371.711250	467536.299080	46.250266
3369.083990	462643.462188	46.255271
3366.264349	457714.675957	46.260276
3363.023711	452747.497905	46.265281
3360.388993	447747.086558	46.270285
3357.637764	442724.627673	46.275290
3354.700248	437656.557213	46.280295
3351.884192	432569.722486	46.285300
3348.732373	427445.743782	46.290305
3346.312101	422295.242947	46.295309
3343.265022	417109.093397	46.300314
3340.417945	411889.380822	46.305319
3337.154795	406645.849210	46.310324
3333.780780	401371.356988	46.315329
3331.177733	396055.080203	46.320333
3328.089485	390724.205305	46.325338
3324.600789	385365.327491	46.330343
3321.387059	379981.892773	46.335348
3318.585555	374577.515731	46.340353
3315.250655	369135.648974	46.345357
3311.517758	363683.024033	46.350362
3308.551833	358201.448660	46.355367
3305.264016	352700.748306	46.360372
3301.697185	347181.763683	46.365377
3298.584771	341639.675096	46.370381
3294.864586	336086.755175	46.375386
3291.594159	330490.746996	46.380391
3288.061779	324898.354589	46.385396
3284.516745	319270.860929	46.390401
3281.422230	313646.234031	46.395405
3277.232693	307989.154340	46.400410
3274.129312	302330.897237	46.405415
3270.329950	296659.197044	46.410420
3266.959170	290960.566510	46.415425
3263.317216	285260.934341	46.420429
3259.357146	279546.550412	46.425434
3256.015190	273814.910113	46.430439
3252.538687	268084.341322	46.435444
3248.242788	262335.825774	46.440449
3244.715252	256581.779089	46.445453
3240.595533	250818.754466	46.450458
3237.153456	245048.804568	46.455463
3233.155646	239281.883598	46.460468
3229.199817	233505.333566	46.465473
3225.707465	227723.232722	46.470477
3221.263257	221940.955885	46.475482
3216.843770	216146.472381	46.480487
3212.993623	210351.708502	46.485492
3209.268148	204500.864408	46.490497
3205.503930	198714.211456	46.495501
3200.961898	192937.646836	46.500506
3196.560212	187159.037106	46.505511
3192.448871	181383.406314	46.510516
3188.296738	175623.413656	46.515521
3184.075343	169868.228370	46.520525
3179.562769	164122.486230	46.525530
3175.343562	158383.373791	46.530535
3170.873007	152662.470077	46.535540
3166.250919	146951.456139	46.540545
3161.993733	141250.783958	46.545549
3157.219782	135572.499250	46.550554
3152.541224	129909.024391	46.555559
3147.807299	124266.774715	46.560564
3142.953779	118647.851975	46.565569
3138.525976	113056.223245	46.570573
3133.306962	107490.923751	46.575578
3128.839838	101941.917871	46.580583
3123.792300	96419.536843	46.585588
3118.992848	90929.810795	46.590593
3114.002479	85467.700091	46.595597
3108.584241	80039.741453	46.600602
3103.410612	74654.564779	46.605607
3098.095968	69304.965204	46.610612
3092.561371	63997.844589	46.615617
3087.026470	58724.796564	46.620621
3081.167601	53516.264776	46.625626
3075.137783	48360.519716	46.630631
3068.391524	43270.167276	46.635636
3058.652093	38322.683121	46.640641
3043.520635	33622.994093	46.645645
3028.557216	29088.568849	46.650650
3014.151724	24718.494047	46.655655
3000.101076	20591.484355	46.660660
2986.280540	16699.115141	46.665665
2972.731936	13042.632966	46.670669
2958.837534	9645.789507	46.675674
2939.878199	6634.873251	46.680679
2915.767460	4085.370270	46.685684
2892.315451	1884.002633	46.690689
2860.130733	356.894778	46.695693
2795.381444	230.393522	46.700698
2757.044175	232.773289	46.705703
2748.767642	233.259008	46.710708
2760.596395	250.279401	46.715713
2780.229132	224.418643	46.720717
2798.023640	221.779541	46.725722
2809.703219	217.724134	46.730727
2814.402242	215.519308	46.735732
2813.750101	232.506244	46.740737
2809.806829	228.564106	46.745741
2805.277330	225.928880	46.750746
2801.210020	227.695168	46.755751
2797.546464	217.283381	46.760756
2794.777417	223.530268	46.765761
2792.188211	213.771664	46.770765
2789.201124	218.366016	46.775770
2787.177696	218.249855	46.780775
2784.572569	212.343372	46.785780
2781.342067	208.897804	46.790785
2778.737044	201.495883	46.795789
2775.436401	217.900342	46.800794
2771.888563	214.731481	46.805799
2768.396948	209.481661	46.810804
2765.570952	208.386151	46.815809
2762.791519	198.893699	46.820813
2759.670791	210.762758	46.825818
2756.487453	213.012477	46.830823
2753.236975	204.650401	46.835828
2749.594876	210.628788	46.840833
2746.410024	201.162801	46.845837
2743.006282	205.560726	46.850842
2739.590441	208.119097	46.855847
2736.558106	205.609102	46.860852
2733.319254	206.409106	46.865857
2730.098543	188.314550	46.870861
2726.810035	202.439734	46.875866
2723.123159	193.154750	46.880871
2719.805593	204.650289	46.885876
2715.967240	203.121888	46.890881
2713.145964	200.838842	46.895885
2709.772779	202.140631	46.900890
2706.496094	192.727180	46.905895
2703.445008	193.256951	46.910900
2699.183022	194.534387	46.915905
2696.139740	193.467197	46.920909
2692.824234	198.341528	46.925914
2689.273639	199.262040	46.930919
2686.059959	195.149132	46.935924
2682.087620	195.193821	46.940929
2678.862952	189.603889	46.945933
2675.427288	192.919222	46.950938
2672.717660	192.202741	46.955943
2668.608052	195.034868	46.960948
2665.113114	204.185042	46.965953
2661.994628	186.245314	46.970957
2658.001704	196.857120	46.975962
2654.573268	188.983011	46.980967
2651.774412	188.466417	46.985972
2648.141040	190.493522	46.990977
2645.191052	188.482846	46.995981
2641.952849	184.997031	47.000986
2638.107217	189.600005	47.005991
2634.511507	189.799064	47.010996
2630.841563	180.429676	47.016001
2627.022171	180.770361	47.021005
2623.420548	185.064769	47.026010
2620.772608	183.780827	47.031015
2617.477665	188.171288	47.036020
2613.691868	192.610652	47.041025
2610.381480	182.524819	47.046029
2607.013034	184.443962	47.051034
2603.514059	175.032090	47.056039
2599.687502	179.536622	47.061044
2595.975752	179.062666	47.066049
2593.021423	169.235622	47.071053
2589.093102	181.510200	47.076058
2585.808119	176.345138	47.081063
2582.173018	185.182304	47.086068
2578.783789	184.129258	47.091073
2575.898429	175.644146	47.096077
2572.119735	183.136162	47.101082
2568.351557	179.830110	47.106087
2565.394946	175.171730	47.111092
2561.392408	178.259737	47.116097
2558.396914	178.674831	47.121101
2554.734048	175.321559	47.126106
2550.527231	171.933832	47.131111
2548.183543	178.784128	47.136116
2544.444686	178.574006	47.141121
2540.787836	174.372582	47.146125
2537.293706	172.035500	47.151130
2533.692545	180.330323	47.156135
2530.372683	172.728443	47.161140
2526.399952	177.278946	47.166145
2523.055521	172.205873	47.171149
2519.981080	172.786410	47.176154
2516.687162	170.198533	47.181159
2513.074853	169.754164	47.186164
2509.178799	173.546249	47.191169
2506.332863	159.727950	47.196173
2502.647964	173.488686	47.201178
2499.136391	168.302214	47.206183
2495.082005	161.995754	47.211188
2491.341206	177.822996	47.216193
2488.513025	164.789931	47.221197
2485.073838	164.288702	47.226202
2481.495370	164.238365	47.231207
2478.257889	157.774950	47.236212
2474.551243	168.008551	47.241217
2471.607524	158.356866	47.246221
2467.641077	169.756537	47.251226
2463.711529	154.832059	47.256231
2460.736057	163.444044	47.261236
2456.698457	162.743160	47.266241
2453.398309	158.250883	47.271245
2450.221197	160.508075	47.276250
2446.625501	166.529520	47.281255
2443.393053	157.561884	47.286260
2439.697577	165.913830	47.291265
2436.383010	150.626866	47.296269
2432.673976	170.182297	47.301274
2429.328666	162.988870	47.306279
2425.587927	158.862818	47.311284
2422.027397	165.557495	47.316289
2418.588179	152.065051	47.321293
2415.314784	163.558577	47.326298
2411.694783	158.473221	47.331303
2408.446775	157.046459	47.336308
2404.561790	171.713023	47.341313
2401.606776	162.116543	47.346317
2397.631292	167.162930	47.351322
2394.172096	155.053594	47.356327
2390.681278	166.886845	47.361332
2387.395078	159.974542	47.366337
2383.988958	149.195361	47.371341
2380.382806	166.515326	47.376346
2376.554384	157.190401	47.381351
2373.349356	158.828490	47.386356
2369.627882	161.507023	47.391361
2366.445935	155.289267	47.396365
2362.792541	165.878614	47.401370
2359.007682	159.806100	47.406375
2355.944979	160.835330	47.411380
2352.202555	166.989686	47.416385
2348.885731	152.789714	47.421389
2345.530036	169.188104	47.426394
2341.818384	156.450670	47.431399
2338.306884	158.400224	47.436404
2334.727609	151.614455	47.441409
2331.676249	157.371391	47.446413
2327.903659	148.872796	47.451418
2323.902161	159.927322	47.456423
2321.082552	159.385576	47.461428
2317.706344	155.340544	47.466433
2314.397202	144.827166	47.471437
2310.502781	156.777634	47.476442
2306.662074	153.123705	47.481447
2303.162404	144.539876	47.486452
2299.820298	150.688745	47.491457
2296.388593	144.152083	47.496461
2292.876000	152.976857	47.501466
2289.310139	155.287897	47.506471
2285.780301	152.120439	47.511476
2282.614358	152.567511	47.516481
2278.803951	146.403406	47.521485
2275.555141	148.286807	47.526490
2271.565918	149.073309	47.531495
2268.504495	156.000381	47.536500
2265.064867	156.323088	47.541505
2261.508070	156.381831	47.546509
2258.041653	147.126129	47.551514
2254.249266	153.184840	47.556519
2251.101775	144.718355	47.561524
2247.301034	148.937109	47.566529
2243.960870	152.653726	47.571533
2240.307069	159.289595	47.576538
2236.782578	156.058145	47.581543
2233.552533	152.931060	47.586548
2229.569674	168.720629	47.591553
2226.581634	156.882694	47.596557
2223.292459	155.516771	47.601562
2219.663023	158.504213	47.606567
2216.013278	151.798703	47.611572
2211.976896	164.029900	47.616577
2208.695280	155.119356	47.621581
2205.383489	157.427847	47.626586
2201.516920	164.898601	47.631591
2198.530107	149.462063	47.636596
2195.132154	153.013844	47.641601
2191.765002	142.678713	47.646605
2187.995748	157.011507	47.651610
2184.267186	158.551362	47.656615
2180.605183	149.679192	47.661620
2177.501705	161.975510	47.666625
2174.034436	154.717264	47.671629
2170.794689	149.546250	47.676634
2167.076515	157.406459	47.681639
2163.611391	154.123207	47.686644
2159.714185	151.301475	47.691649
2156.292125	154.706318	47.696653
2152.877198	144.348549	47.701658
2149.609225	156.309427	47.706663
2146.391665	153.353605	47.711668
2142.442464	151.316823	47.716673
2138.913188	152.241364	47.721677
2135.470664	148.498152	47.726682
2131.919710	157.085103	47.731687
2128.787475	147.539723	47.736692
2124.497459	148.895980	47.741697
2121.372083	149.244100	47.746701
2117.888220	143.706076	47.751706
2114.397405	152.517706	47.756711
2110.980246	143.204255	47.761716
2107.695020	149.207482	47.766721
2103.908482	139.737180	47.771725
2100.521338	139.963711	47.776730
2096.643342	147.994901	47.781735
2093.224385	142.854829	47.786740
2090.206532	148.013574	47.791745
2086.692265	149.013422	47.796749
2082.970236	149.466738	47.801754
2079.237872	150.973570	47.806759
2076.088103	145.510670	47.811764
2072.348353	143.015181	47.816769
2068.633662	142.843910	47.821773
2066.022383	144.553170	47.826778
2061.788979	151.850381	47.831783
2058.548824	141.774154	47.836788
2054.916486	142.602176	47.841793
2051.521204	145.117612	47.846797
2047.641959	136.616651	47.851802
2044.241078	143.973667	47.856807
2041.155327	143.270192	47.861812
2037.304524	144.137781	47.866817
2033.821909	137.907769	47.871821
2030.239465	143.568980	47.876826
2027.022923	147.467745	47.881831
2023.491667	135.273041	47.886836
2019.571328	144.716341	47.891841
2016.291515	141.802516	47.896845
2013.279333	139.809715	47.901850
2009.572214	150.514193	47.906855
2006.478354	140.203216	47.911860
2002.220862	142.902801	47.916865
1998.758177	138.286290	47.921869
1995.307152	133.656209	47.926874
1992.091527	141.340336	47.931879
1988.562853	144.243391	47.936884
1984.758713	145.245773	47.941889
1981.458831	136.466343	47.946893
1977.721088	139.710315	47.951898
1974.177377	145.970778	47.956903
1971.270378	143.850662	47.961908
1967.321605	145.393454	47.966913
1963.982781	144.459650	47.971917
1960.593232	138.089764	47.976922
1956.993858	140.380586	47.981927
1953.397192	134.620855	47.986932
1949.772489	143.401510	47.991937
1946.566506	133.567187	47.996941
1942.877269	138.972657	48.001946
1939.129934	135.012349	48.006951
1935.737641	146.146999	48.011956
1932.540300	144.534029	48.016961
1929.333831	149.107861	48.021965
1925.569360	144.257656	48.026970
1921.896783	140.048171	48.031975
1918.333652	132.312324	48.036980
1914.754667	132.141398	48.041985
1911.403157	124.143951	48.046989
1908.002167	136.672256	48.051994
1904.501469	144.985039	48.056999
1900.884625	134.932707	48.062004
1897.065041	140.047239	48.067009
1894.036586	135.774449	48.072013
1890.552381	138.179245	48.077018
1886.851892	139.350627	48.082023
1883.259952	149.576916	48.087028
1879.809778	133.201389	48.092033
1876.467913	141.633700	48.097037
1872.790501	135.618458	48.102042
1869.090498	134.904235	48.107047
1865.788730	123.576841	48.112052
1862.215351	136.839222	48.117057
1859.337003	142.715997	48.122061
1855.860397	136.304986	48.127066
1851.734429	143.020998	48.132071
1848.434345	130.828217	48.137076
1844.706910	140.444330	48.142081
1841.343111	142.190240	48.147085
1837.778471	137.047507	48.152090
1834.314442	134.544237	48.157095
1830.875505	125.173692	48.162100
1827.221461	140.996279	48.167105
1823.395677	135.882437	48.172109
1820.085993	136.776576	48.177114
1816.801834	134.450711	48.182119
1813.745956	131.711484	48.187124
1809.974565	134.367991	48.192129
1806.176184	135.578165	48.197133
1802.812321	145.272387	48.202138
1798.930233	148.226679	48.207143
1795.883518	141.091091	48.212148
1792.392687	141.901611	48.217153
1788.838671	136.991006	48.222157
1785.501521	132.134839	48.227162
1781.850898	134.113043	48.232167
1778.386780	132.188227	48.237172
1774.636391	139.889907	48.242177
1771.329585	136.377311	48.247181
1767.936914	132.765877	48.252186
1764.096395	136.428058	48.257191
1761.176079	134.451203	48.262196
1757.368230	134.580412	48.267201
1753.648056	127.995173	48.272205
1749.910303	135.623933	48.277210
1746.711583	135.776899	48.282215
1743.335934	144.919197	48.287220
1739.720788	137.291204	48.292225
1736.352087	145.091069	48.297229
1733.069892	125.538191	48.302234
1729.098505	138.290428	48.307239
1725.849857	136.137736	48.312244
1722.540882	134.436288	48.317249
1718.801961	132.109521	48.322253
1715.152531	132.215272	48.327258
1711.523531	136.013723	48.332263
1708.372133	129.607354	48.337268
1704.996916	129.542942	48.342273
1701.278643	126.662798	48.347277
1697.706237	127.337737	48.352282
1693.916809	122.247011	48.357287
1690.937234	122.838678	48.362292
1687.194464	130.797475	48.367297
1683.646656	126.373952	48.372301
1680.246330	116.540522	48.377306
1676.348279	129.520994	48.382311
1673.292173	128.776379	48.387316
1669.871711	130.247461	48.392321
1665.985404	127.422439	48.397325
1662.884566	127.759539	48.402330
1659.191094	132.043314	48.407335
1655.896748	130.327854	48.412340
1652.523723	132.413481	48.417345
1648.670242	141.490614	48.422349
1645.063697	132.498495	48.427354
1641.638275	122.150268	48.432359
1638.435928	124.169918	48.437364
1634.894472	125.994386	48.442369
1631.316814	124.890887	48.447373
1627.551864	132.352381	48.452378
1623.810539	135.152072	48.457383
1620.569068	129.218922	48.462388
1616.998246	134.903407	48.467393
1613.994993	130.636925	48.472397
1610.280056	126.020953	48.477402
1606.537577	140.093994	48.482407
1603.496875	126.499005	48.487412
1599.745409	129.832807	48.492417
1596.200495	137.199832	48.497421
1592.962979	121.355115	48.502426
1588.872098	125.255114	48.507431
1585.492772	128.030734	48.512436
1581.868405	127.985239	48.517441
1578.386889	119.399694	48.522445
1575.207354	126.205512	48.527450
1571.672618	129.351260	48.532455
1568.309145	111.737045	48.537460
1564.945135	119.756080	48.542465
1561.284467	115.261205	48.547469
1557.464010	123.474725	48.552474
1553.742934	121.190152	48.557479
1550.921662	118.596940	48.562484
1547.325288	126.714115	48.567489
1543.595787	120.522936	48.572493
1539.796170	126.312907	48.577498
1536.460291	124.401378	48.582503
1533.151797	124.329402	48.587508
1529.479861	117.677389	48.592513
1526.087776	122.552443	48.597517
1522.549766	119.801831	48.602522
1519.074450	121.919327	48.607527
1515.766721	119.885537	48.612532
1512.111066	114.224422	48.617537
1508.334715	119.180968	48.622541
1505.305276	122.559705	48.627546
1501.692981	116.491215	48.632551
1498.322088	125.552186	48.637556
1494.741166	118.692319	48.642561
1490.865082	120.510043	48.647565
1487.646458	112.087013	48.652570
1483.583676	118.173062	48.657575
1480.238445	113.820530	48.662580
1477.009103	120.155746	48.667585
1473.347771	127.995448	48.672589
1470.133524	121.063945	48.677594
1466.513669	122.855779	48.682599
1463.296864	118.216746	48.687604
1460.175696	117.658517	48.692609
1456.338677	121.379794	48.697613
1452.662768	114.680368	48.702618
1448.893357	123.329914	48.707623
1445.532596	109.527088	48.712628
1441.995164	120.539131	48.717633
1438.369236	118.309536	48.722637
1434.857074	121.346280	48.727642
1431.474099	130.013454	48.732647
1428.067670	116.453435	48.737652
1424.576994	127.155625	48.742657
1420.960380	115.935138	48.747661
1417.772177	124.560547	48.752666
1413.659964	132.140397	48.757671
1410.408078	124.641142	48.762676
1407.117366	116.436944	48.767681
1402.955767	125.272341	48.772685
1399.933929	126.508424	48.777690
1396.796806	120.742479	48.782695
1393.353488	120.793423	48.787700
1389.750973	117.811304	48.792705
1385.806511	130.451619	48.797709
1382.370740	113.274643	48.802714
1378.375592	118.405332	48.807719
1375.296281	118.456108	48.812724
1371.869746	113.817801	48.817729
1368.258685	131.843139	48.822733
1365.479079	120.820931	48.827738
1361.506950	129.776892	48.832743
1357.930506	120.282794	48.837748
1354.314662	123.054813	48.842753
1350.844536	126.032166	48.847757
1347.412100	117.291494	48.852762
1343.784907	126.805152	48.857767
1340.723318	119.568428	48.862772
1337.116356	117.857533	48.867777
1333.258176	122.008676	48.872781
1329.973220	113.433792	48.877786
1326.432335	123.003002	48.882791
1323.194183	122.278593	48.887796
1319.549129	117.538050	48.892801
1315.627839	115.107539	48.897805
1312.167804	122.755132	48.902810
1308.689178	120.152931	48.907815
1305.627648	120.819453	48.912820
1301.988710	110.653797	48.917825
1298.191528	121.399027	48.922829
1295.106274	112.368559	48.927834
1291.371459	120.026620	48.932839
1287.980962	109.304333	48.937844
1284.162821	114.305900	48.942849
1280.588493	122.697480	48.947853
1277.438314	108.297689	48.952858
1273.950068	110.607570	48.957863
1270.492709	112.772620	48.962868
1267.070744	112.949978	48.967873
1263.471406	117.867119	48.972877
1260.174333	119.716890	48.977882
1256.305648	118.755152	48.982887
1252.770736	111.441919	48.987892
1249.332437	112.365161	48.992897
1245.399055	117.177101	48.997901
1242.270091	112.018911	49.002906
1238.736443	115.915814	49.007911
1235.554318	115.357417	49.012916
1232.088537	114.856537	49.017921
1228.182679	114.957913	49.022925
1224.598814	114.583978	49.027930
1221.253933	117.944999	49.032935
1218.095356	113.689610	49.037940
1214.608891	112.895189	49.042945
1210.953292	106.530674	49.047949
1207.573382	116.016043	49.052954
1203.509708	111.724338	49.057959
1200.014400	105.393034	49.062964
1196.771701	115.049627	49.067969
1192.912457	108.869676	49.072973
1189.899994	110.944607	49.077978
1186.218142	107.680635	49.082983
1182.648903	111.744712	49.087988
1179.430149	112.762029	49.092993
1176.114974	117.647693	49.097997
1172.442848	112.455354	49.103002
1168.890657	116.181740	49.108007
1165.384433	114.972689	49.113012
1162.081300	120.651818	49.118017
1158.044171	109.700683	49.123021
1154.541231	115.251744	49.128026
1150.802776	119.321034	49.133031
1147.872179	110.925909	49.138036
1144.201735	116.850893	49.143041
1140.620472	108.601023	49.148045
1137.538867	109.210425	49.153050
1134.077506	118.735809	49.158055
1130.134229	115.904208	49.163060
1126.592940	115.805289	49.168065
1123.110915	114.710464	49.173069
1120.064145	118.591810	49.178074
1116.345498	108.936262	49.183079
1112.786132	108.691170	49.188084
1109.038766	109.045004	49.193089
1105.825766	107.953116	49.198093
1102.113755	103.479053	49.203098
1098.554661	112.735728	49.208103
1095.112143	104.185041	49.213108
1091.447769	121.206501	49.218113
1088.247831	113.016745	49.223117
1085.071180	108.023878	49.228122
1081.415390	109.303033	49.233127
1077.623306	111.439330	49.238132
1074.052168	112.064889	49.243137
1070.481005	107.778039	49.248141
1067.416500	109.067827	49.253146
1063.606828	120.321291	49.258151
1060.392317	112.975211	49.263156
1056.638458	122.605433	49.268161
1053.091024	109.320207	49.273165
1050.282906	109.492590	49.278170
1045.926266	115.257033	49.283175
1042.551615	116.248038	49.288180
1039.258904	112.024137	49.293185
1035.174590	118.457750	49.298189
1031.718659	114.767298	49.303194
1028.569437	111.512183	49.308199
1025.275126	120.546594	49.313204
1021.935926	115.634231	49.318209
1017.889768	117.852016	49.323213
1014.884995	112.559354	49.328218
1010.767664	117.370075	49.333223
1007.219537	116.977781	49.338228
1004.008158	106.288410	49.343233
1000.509958	118.761263	49.348237
997.577302	119.445908	49.353242
993.750119	116.329574	49.358247
989.999942	115.307589	49.363252
986.871627	111.530053	49.368257
982.833120	112.049934	49.373261
979.655471	99.093161	49.378266
976.181053	116.882380	49.383271
972.466689	115.623392	49.388276
969.440193	104.129038	49.393281
965.692503	109.277072	49.398285
962.326095	118.573516	49.403290
958.816958	109.384789	49.408295
955.009246	104.051979	49.413300
951.361098	105.231123	49.418305
947.906759	112.543580	49.423309
944.544688	103.907465	49.428314
940.958949	117.269076	49.433319
937.404535	118.268891	49.438324
933.965547	108.836879	49.443329
930.834653	114.977581	49.448333
927.333256	99.833478	49.453338
923.503570	110.698673	49.458343
919.933396	101.449475	49.463348
916.519497	104.594282	49.468353
912.597384	120.736321	49.473357
909.616977	101.317964	49.478362
905.690331	106.910942	49.483367
902.648235	114.227437	49.488372
899.132496	112.845176	49.493377
895.648956	113.970609	49.498381
892.213843	107.936662	49.503386
888.512749	105.957855	49.508391
884.779635	107.364481	49.513396
881.645205	100.300093	49.518401
877.895983	115.265773	49.523405
874.651330	104.522652	49.528410
871.393666	109.092949	49.533415
868.065153	110.882946	49.538420
864.239235	104.363532	49.543425
860.356280	112.679206	49.548429
856.916027	100.405498	49.553434
853.380635	110.785801	49.558439
849.712470	106.360953	49.563444
846.226712	109.292197	49.568449
842.368839	106.038641	49.573453
839.492392	102.246067	49.578458
836.046230	117.514309	49.583463
832.622116	110.227502	49.588468
829.172195	107.176983	49.593473
825.521165	107.075442	49.598477
821.988097	103.027403	49.603482
818.276776	109.497585	49.608487
814.923272	105.297991	49.613492
811.553528	105.434719	49.618497
807.638892	102.904573	49.623501
804.663574	104.163776	49.628506
801.088747	107.255081	49.633511
797.428529	105.288325	49.638516
793.981229	106.700478	49.643521
790.390361	107.487440	49.648525
787.066151	99.166651	49.653530
783.089213	113.453891	49.658535
779.984775	103.005489	49.663540
776.225800	110.074828	49.668545
772.960290	115.687636	49.673549
769.693391	104.094055	49.678554
765.682415	119.406782	49.683559
762.425152	117.632459	49.688564
759.066382	106.048220	49.693569
755.240292	103.099489	49.698573
751.890955	96.031825	49.703578
747.958628	113.523868	49.708583
744.828693	109.794564	49.713588
741.473685	105.531549	49.718593
737.911978	111.392072	49.723597
734.470863	95.119496	49.728602
731.154869	109.799262	49.733607
727.282857	110.033066	49.738612
723.885628	105.653941	49.743617
720.249811	110.856642	49.748621
717.033542	98.916879	49.753626
713.269222	107.168986	49.758631
709.598028	102.676112	49.763636
706.424070	105.307468	49.768641
702.486037	94.853094	49.773645
699.425233	95.651789	49.778650
695.765615	104.356375	49.783655
692.371493	99.412790	49.788660
689.078691	97.636344	49.793665
685.242035	101.978307	49.798669
682.024143	98.611363	49.803674
678.103923	99.990843	49.808679
674.792534	105.633838	49.813684
671.399505	101.420023	49.818689
667.702993	106.826431	49.823693
664.376980	100.636263	49.828698
660.821653	105.957075	49.833703
657.401208	99.951904	49.838708
653.977904	99.501721	49.843713
650.310909	102.889862	49.848717
646.747463	103.165852	49.853722
643.131754	104.706742	49.858727
639.573007	96.324006	49.863732
636.094699	101.240346	49.868737
632.418597	105.542479	49.873741
629.599537	106.106324	49.878746
625.727355	101.866342	49.883751
622.113213	100.578825	49.888756
619.119144	97.578909	49.893761
615.320096	99.351941	49.898765
611.575796	95.835276	49.903770
608.026373	94.657005	49.908775
604.556991	101.908106	49.913780
601.074380	105.440511	49.918785
597.828434	96.176687	49.923789
594.140379	106.207816	49.928794
590.972858	102.132453	49.933799
587.193720	104.951422	49.938804
584.205328	97.151276	49.943809
580.334947	99.413139	49.948813
576.726408	97.483802	49.953818
573.411493	98.916397	49.958823
569.214625	103.895879	49.963828
566.201775	101.115006	49.968833
562.460743	96.666442	49.973837
559.292852	97.717463	49.978842
555.443611	93.460331	49.983847
552.036152	104.415969	49.988852
548.946642	94.932631	49.993857
545.295470	105.108833	49.998861
541.748970	95.322317	50.003866
538.171124	93.590581	50.008871
534.760863	97.137076	50.013876
531.407429	98.910780	50.018881
527.628346	102.022835	50.023885
524.337691	95.990715	50.028890
520.536275	95.548985	50.033895
517.073563	103.364605	50.038900
513.667264	93.216215	50.043905
510.029206	103.547542	50.048909
506.424033	100.351237	50.053914
503.254420	100.292401	50.058919
499.361968	110.895290	50.063924
496.493663	97.157091	50.068929
492.491111	97.434325	50.073933
489.071146	92.884170	50.078938
485.849862	94.599261	50.083943
482.169779	99.862411	50.088948
478.824082	93.066725	50.093953
475.092159	106.030095	50.098957
471.580848	94.106033	50.103962
467.957027	105.342956	50.108967
463.955171	94.527487	50.113972
460.772866	91.518909	50.118977
457.364124	91.568895	50.123981
454.460307	88.048958	50.128986
450.926494	96.616434	50.133991
446.982473	99.124303	50.138996
444.108509	102.813274	50.144001
440.327477	103.304579	50.149005
436.350669	89.764964	50.154010
432.724207	104.207811	50.159015
429.584496	95.952038	50.164020
426.367362	102.834216	50.169025
422.363385	102.947975	50.174029
419.051317	99.455422	50.179034
415.588588	95.352883	50.184039
411.968937	110.061413	50.189044
408.487974	96.680802	50.194049
405.020573	102.701971	50.199053
401.292141	92.484266	50.204058
398.241665	94.378652	50.209063
394.476368	104.721939	50.214068
391.638946	92.936440	50.219073
387.548911	105.960948	50.224077
384.139443	102.118752	50.229082
380.541140	100.524949	50.234087
376.885670	99.434765	50.239092
373.671289	94.205493	50.244097
369.570443	103.624197	50.249101
366.461740	93.335552	50.254106
363.054204	91.204910	50.259111
359.234012	93.117472	50.264116
355.954537	91.363976	50.269121
352.440539	96.978335	50.274125
349.170529	97.716952	50.279130
345.623419	99.650073	50.284135
341.926713	98.830211	50.289140
338.568599	91.655677	50.294145
335.003658	98.706209	50.299149
331.326214	103.279191	50.304154
328.260197	101.662528	50.309159
324.336287	88.539118	50.314164
321.046436	86.251228	50.319169
317.166611	89.103959	50.324173
313.552833	86.550607	50.329178
310.384745	95.507755	50.334183
306.864194	87.525330	50.339188
303.789378	82.957286	50.344193
300.092314	89.492659	50.349197
296.436451	91.768700	50.354202
293.222226	91.161769	50.359207
289.251012	89.694340	50.364212
285.931771	80.999480	50.369217
282.165244	91.197827	50.374221
278.886357	80.248271	50.379226
275.619586	91.486806	50.384231
271.914184	82.962870	50.389236
268.146454	78.187145	50.394241
264.695239	89.419628	50.399245
261.718066	91.699369	50.404250
257.804008	83.400737	50.409255
253.989202	94.315158	50.414260
250.737134	89.114364	50.419265
247.449867	102.811925	50.424269
243.864435	84.010406	50.429274
240.549823	95.860753	50.434279
236.858785	95.665793	50.439284
233.429156	95.611317	50.444289
229.653731	90.201895	50.449293
226.354225	93.969227	50.454298
223.127838	87.102860	50.459303
219.494947	101.351787	50.464308
215.933324	91.486041	50.469313
212.270742	86.705137	50.474317
208.714394	100.722908	50.479322
205.121648	94.886128	50.484327
201.518068	103.023588	50.489332
198.471126	98.584396	50.494337
194.767112	105.691512	50.499341
191.763138	94.184081	50.504346
188.054838	87.553714	50.509351
184.417366	103.805555	50.514356
180.519477	90.332465	50.519361
177.113238	105.141879	50.524365
173.929428	96.225509	50.529370
170.287186	97.473681	50.534375
166.750817	102.044688	50.539380
163.646138	90.805222	50.544385
159.313913	104.712600	50.549389
156.305386	98.501342	50.554394
152.809670	101.351981	50.559399
149.444963	97.211906	50.564404
146.156131	94.199997	50.569409
142.419504	95.259051	50.574413
138.689320	89.555291	50.579418
135.183148	93.145307	50.584423
131.648209	98.575681	50.589428
128.363796	95.142936	50.594433
124.712141	94.567405	50.599437
121.050740	96.737977	50.604442
118.010632	93.726004	50.609447
113.992678	95.495265	50.614452
110.880780	90.595917	50.619457
106.997049	94.980209	50.624461
103.777022	92.149698	50.629466
100.527105	103.395441	50.634471
96.478456	101.192811	50.639476
93.732984	92.601099	50.644481
89.789485	102.535806	50.649485
86.424743	92.686221	50.654490
82.769179	94.935187	50.659495
79.023393	90.915739	50.664500
75.798697	94.051937	50.669505
71.886722	96.461531	50.674509
68.617193	90.762786	50.679514
65.140412	92.582462	50.684519
61.447806	102.472144	50.689524
58.417235	86.637257	50.694529
54.669683	98.248512	50.699533
51.084301	92.284574	50.704538
47.658674	99.854671	50.709543
44.268232	105.312615	50.714548
40.900839	99.580233	50.719553
37.004851	97.513714	50.724557
33.399009	97.577116	50.729562
30.106606	97.335053	50.734567
26.408291	102.029599	50.739572
23.230612	88.136661	50.744577
19.562068	93.929145	50.749581
16.222887	84.834126	50.754586
12.557395	90.704251	50.759591
9.337734	90.054469	50.764596
5.724232	96.555707	50.769601
2.133211	94.012304	50.774605