Fri Jun 17 17:45:11 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.912492	78.691365	0.000000
-0.596185	96.936962	0.005005
-0.182676	95.904755	0.010010
-0.428509	82.985027	0.015014
-0.599280	69.969559	0.020019
-0.792416	69.773836	0.025024
-0.902171	58.154019	0.030029
-1.196767	57.516367	0.035034
-1.530616	50.600271	0.040038
-1.537968	42.142830	0.045043
-1.865480	25.625980	0.050048
-2.119395	24.318342	0.055053
-2.534234	11.801889	0.060058
-3.080936	3.417147	0.065062
-3.032883	-0.890165	0.070067
-3.331623	-10.563829	0.075072
-3.547222	-9.276439	0.080077
-3.887850	-16.448892	0.085082
-4.691252	-12.527919	0.090086
-5.064832	-19.242221	0.095091
-5.188029	-18.470222	0.100096
-5.289835	-12.127026	0.105101
-5.248019	-16.558997	0.110106
-6.430410	-14.847672	0.115110
-6.489784	-22.363852	0.120115
-6.813539	-13.596081	0.125120
-6.272780	-14.668376	0.130125
-6.873579	-16.078189	0.135130
-6.531245	-18.453816	0.140134
-6.456451	-19.868971	0.145139
-7.596454	-14.383072	0.150144
-8.032231	-8.879450	0.155149
-8.181295	-10.724672	0.160154
-8.329400	0.340424	0.165158
-8.144024	-18.611823	0.170163
-8.543144	-14.066606	0.175168
-9.398010	-6.504637	0.180173
-9.176047	-14.502301	0.185178
-9.479726	-7.101212	0.190182
-9.553764	-5.482552	0.195187
-9.838688	-14.687878	0.200192
-10.802735	-2.234513	0.205197
-10.689846	-10.944364	0.210202
-11.122880	-10.860653	0.215206
-11.355995	-18.446422	0.220211
-11.668505	-8.511539	0.225216
-11.508006	-17.543055	0.230221
-11.534037	-14.293950	0.235226
-11.590183	-15.206844	0.240230
-12.138320	-9.882466	0.245235
-12.502875	-13.647404	0.250240
-12.848855	-9.490878	0.255245
-12.773874	-18.853505	0.260250
-13.492294	-17.876800	0.265254
-13.737642	-19.370360	0.270259
-14.219740	-12.279812	0.275264
-14.687676	-16.750383	0.280269
-14.336744	-23.240769	0.285274
-14.648622	-10.105508	0.290278
-14.578750	-19.708618	0.295283
-14.316185	-22.847872	0.300288
-15.245944	-16.986276	0.305293
-15.701741	-18.780710	0.310298
-15.826180	-19.307129	0.315302
-15.789847	-18.947623	0.320307
-16.135816	-22.136486	0.325312
-16.646271	-15.158045	0.330317
-17.110716	-17.248416	0.335322
-17.347790	-9.248652	0.340326
-17.768990	-10.152961	0.345331
-17.619701	-9.869062	0.350336
-17.575442	-13.538958	0.355341
-17.409995	-14.118692	0.360346
-18.340314	-11.531286	0.365350
-18.888265	-20.498122	0.370355
-18.990160	-16.560358	0.375360
-19.461491	-3.100620	0.380365
-19.450802	-13.676400	0.385370
-19.545426	-3.839890	0.390374
-19.430806	-8.477544	0.395379
-19.966072	-19.105240	0.400384
-20.515612	-10.017165	0.405389
-20.810763	-12.953212	0.410394
-21.357543	-8.043845	0.415398
-21.058426	-11.687434	0.420403
-20.915437	-16.223835	0.425408
-21.240391	-4.322665	0.430413
-21.536146	-16.235520	0.435418
-22.295770	-1.600321	0.440422
-22.734590	-13.130456	0.445427
-22.489328	-6.668340	0.450432
-22.605850	-7.693345	0.455437
-22.713429	-17.481654	0.460442
-23.735645	-17.314608	0.465446
-24.354667	-10.486046	0.470451
-24.253860	-20.689837	0.475456
-24.415035	-7.353683	0.480461
-24.206959	-4.234262	0.485466
-24.617174	-4.203674	0.490470
-24.544046	-10.129109	0.495475
-24.228139	-17.518431	0.500480
-24.922595	-10.647335	0.505485
-25.536289	-21.140832	0.510490
-25.532113	-15.464666	0.515494
-25.840454	-6.381951	0.520499
-26.531585	-21.453641	0.525504
-26.631414	-12.979817	0.530509
-26.508447	-17.825065	0.535514
-26.698571	-15.517769	0.540518
-27.517492	-10.257700	0.545523
-28.192932	-11.115999	0.550528
-28.244785	-7.993430	0.555533
-28.195979	-17.599749	0.560538
-28.661444	-5.648189	0.565542
-28.672689	-6.926305	0.570547
-28.726207	-14.045644	0.575552
-28.386903	-13.812273	0.580557
-29.147987	-21.493203	0.585562
-30.208429	-14.410513	0.590566
-30.081196	-15.191289	0.595571
-30.143754	-9.890794	0.600576
-30.388858	-11.716894	0.605581
-30.367117	-13.506839	0.610586
-30.393716	-12.264874	0.615590
-30.940065	-14.663473	0.620595
-31.437365	-9.038329	0.625600
-31.897105	-12.450009	0.630605
-31.515389	-5.001038	0.635610
-31.754678	-11.485868	0.640614
-32.294823	-8.917535	0.645619
-32.850482	-13.155867	0.650624
-33.592168	-7.433663	0.655629
-33.400432	-14.997110	0.660634
-33.604575	-2.606911	0.665638
-33.561508	-10.540306	0.670643
-33.293879	-6.079868	0.675648
-33.740797	-5.933266	0.680653
-34.156680	-10.363549	0.685658
-34.973039	-16.270970	0.690662
-35.271688	-9.400547	0.695667
-35.429695	-13.615194	0.700672
-35.316597	-7.346396	0.705677
-35.114409	-15.750033	0.710682
-35.807494	-8.336113	0.715686
-36.509692	-7.534171	0.720691
-36.828339	-8.017257	0.725696
-37.058306	-11.700571	0.730701
-36.755054	-13.673270	0.735706
-36.803306	-12.173743	0.740710
-36.787417	-17.862139	0.745715
-37.282398	-17.639468	0.750720
-38.097617	-19.186888	0.755725
-38.071997	-7.708857	0.760730
-38.090468	-13.993990	0.765734
-38.295677	-18.488889	0.770739
-38.972891	-17.869486	0.775744
-39.273881	-9.036629	0.780749
-39.502994	-11.137306	0.785754
-39.280649	-15.306645	0.790758
-39.672724	-15.579405	0.795763
-40.246830	-17.040613	0.800768
-40.965460	-6.951199	0.805773
-40.963664	-6.923978	0.810778
-41.391613	-8.363109	0.815782
-41.338306	-20.646748	0.820787
-41.036877	-26.568884	0.825792
-41.406679	-13.035655	0.830797
-41.356222	-18.765513	0.835802
-42.187287	-18.931361	0.840806
-42.594857	-13.906412	0.845811
-42.898766	-17.234672	0.850816
-43.018669	-14.391854	0.855821
-42.767709	-26.501345	0.860826
-43.191894	-13.852386	0.865830
-43.722800	-21.395358	0.870835
-44.092740	-25.194518	0.875840
-44.473779	-15.684741	0.880845
-44.402803	-21.552390	0.885850
-44.743820	-15.242643	0.890854
-44.931597	-16.459446	0.895859
-45.131901	-14.651279	0.900864
-45.266289	0.567290	0.905869
-45.338805	-18.604727	0.910874
-45.856581	-16.354260	0.915878
-46.216304	-19.031724	0.920883
-46.165393	-14.284066	0.925888
-46.559242	-9.930145	0.930893
-47.224079	-13.015682	0.935898
-47.552017	-16.940026	0.940902
-47.991276	-14.618153	0.945907
-47.880273	-20.187582	0.950912
-47.904555	-2.986007	0.955917
-47.770569	-15.933458	0.960922
-47.745225	-10.422422	0.965926
-48.254476	-8.952032	0.970931
-48.865462	-15.119333	0.975936
-49.235530	-6.580655	0.980941
-49.022667	-13.314687	0.985946
-49.430545	-10.031708	0.990950
-50.237501	-8.372713	0.995955
-50.559983	-10.982765	1.000960
-51.146889	-15.650023	1.005965
-50.813497	-23.439275	1.010970
-50.795031	-14.527906	1.015974
-50.827979	-17.382822	1.020979
-50.931205	-17.142392	1.025984
-51.336275	-13.639267	1.030989
-52.124827	-12.728841	1.035994
-52.410764	-6.884078	1.040998
-52.338467	-8.376566	1.046003
-51.964371	-10.832660	1.051008
-52.879270	-3.877753	1.056013
-53.342209	-15.754327	1.061018
-53.676163	-0.972230	1.066022
-53.871075	-6.998540	1.071027
-54.019382	-1.952158	1.076032
-53.996445	-13.535758	1.081037
-54.284035	-10.924947	1.086042
-54.508522	-11.069082	1.091046
-55.318373	-11.369480	1.096051
-55.695187	-12.053445	1.101056
-56.151077	-9.389794	1.106061
-55.900980	-10.010636	1.111066
-55.756062	-18.789936	1.116070
-55.886302	-12.077747	1.121075
-56.020689	-15.993219	1.126080
-56.407389	-5.204787	1.131085
-57.190918	-8.997555	1.136090
-57.324514	-14.109369	1.141094
-57.690300	-13.307107	1.146099
-57.359411	-16.047276	1.151104
-57.808243	-9.394801	1.156109
-57.769717	-18.113595	1.161114
-58.531127	-13.928858	1.166118
-58.885483	-8.105083	1.171123
-58.820273	-19.923029	1.176128
-59.322836	-8.751070	1.181133
-59.241124	-12.707398	1.186138
-59.269708	-8.132014	1.191142
-60.219519	-5.015080	1.196147
-60.620234	-9.990931	1.201152
-60.584165	-9.244814	1.206157
-60.622336	-20.455756	1.211162
-60.660928	-9.651393	1.216166
-61.098505	-8.550674	1.221171
-61.585195	-17.589646	1.226176
-62.110634	-8.757958	1.231181
-62.224989	-9.196069	1.236186
-62.787902	-8.354130	1.241190
-62.693188	-14.144823	1.246195
-62.404625	-15.628665	1.251200
-62.588250	-15.128405	1.256205
-62.551063	-11.292495	1.261210
-63.404374	-13.328676	1.266214
-64.051945	-2.586859	1.271219
-63.857575	-11.003011	1.276224
-63.911646	-3.546919	1.281229
-64.029190	-2.978120	1.286234
-64.455196	-4.399812	1.291238
-65.498827	0.841974	1.296243
-65.312742	-18.635476	1.301248
-65.787143	-3.520426	1.306253
-65.621860	-8.389680	1.311258
-65.649919	1.774382	1.316262
-65.848770	-3.049143	1.321267
-66.216574	-15.433273	1.326272
-67.016803	-4.063437	1.331277
-67.095574	-13.740699	1.336282
-66.804342	-9.069299	1.341286
-67.295685	-2.737122	1.346291
-68.488826	-8.003727	1.351296
-68.417840	-8.159092	1.356301
-67.940240	-14.022904	1.361306
-68.544345	-6.576018	1.366310
-68.582430	-8.342600	1.371315
-68.634456	-12.596962	1.376320
-69.112161	-4.585413	1.381325
-69.086933	-13.262139	1.386330
-69.722375	-14.484638	1.391334
-70.238474	-9.555504	1.396339
-70.226649	-12.601380	1.401344
-70.629795	-14.494935	1.406349
-70.705281	-10.323384	1.411354
-70.726226	-16.361440	1.416358
-71.688990	-2.454359	1.421363
-71.572230	-15.172212	1.426368
-72.131875	-9.981876	1.431373
-72.136364	-13.515601	1.436378
-71.866625	-3.731574	1.441382
-72.211127	-10.561205	1.446387
-72.026117	-8.319819	1.451392
-73.199256	-4.277381	1.456397
-73.554046	-8.916130	1.461402
-73.828058	-7.685723	1.466406
-74.013194	-10.620320	1.471411
-73.798350	-16.574834	1.476416
-73.818792	-7.103092	1.481421
-73.952282	-10.122049	1.486426
-74.672692	-12.431126	1.491430
-74.748675	-9.735515	1.496435
-75.003943	-6.911238	1.501440
-75.766717	-5.326477	1.506445
-76.293703	-10.993693	1.511450
-76.402432	-3.988096	1.516454
-76.362638	-4.105716	1.521459
-76.192964	-14.687396	1.526464
-76.626484	0.748033	1.531469
-76.357903	-5.591330	1.536474
-77.030899	-8.895922	1.541478
-77.279146	-16.065566	1.546483
-77.761184	-10.067241	1.551488
-78.107142	-6.377596	1.556493
-77.757061	-16.244149	1.561498
-77.914991	-13.812361	1.566502
-79.051690	-12.915883	1.571507
-79.099012	-21.101427	1.576512
-79.621056	1.491048	1.581517
-79.664263	-6.865878	1.586522
-79.833372	-6.637977	1.591526
-79.621764	-5.785278	1.596531
-80.227069	-9.218533	1.601536
-80.883536	4.251070	1.606541
-81.015627	-9.812250	1.611546
-81.382680	-9.244794	1.616550
-81.426617	-1.819789	1.621555
-81.473262	-6.564029	1.626560
-81.837517	-3.853844	1.631565
-81.360623	-12.215138	1.636570
-81.699616	-10.773245	1.641574
-82.568149	-1.719746	1.646579
-82.632932	-6.737232	1.651584
-83.226081	-3.049708	1.656589
-83.112173	-10.182669	1.661594
-83.385420	-11.043881	1.666598
-84.033927	-12.806073	1.671603
-84.289667	-8.926203	1.676608
-84.771996	-11.387925	1.681613
-84.791446	-5.970872	1.686618
-84.698117	-13.508487	1.691622
-84.774315	8.660214	1.696627
-84.793572	-8.866052	1.701632
-85.469553	-4.724122	1.706637
-86.086072	-7.405463	1.711642
-86.237277	-3.347811	1.716646
-86.593169	5.209631	1.721651
-86.590957	-7.517008	1.726656
-86.551487	-2.362922	1.731661
-86.817272	-0.164797	1.736666
-86.654216	-3.605215	1.741670
-87.424611	-0.921639	1.746675
-87.914349	-5.224594	1.751680
-88.175985	6.959879	1.756685
-88.361582	-8.651870	1.761690
-88.062943	-6.965321	1.766694
-88.637570	-5.790510	1.771699
-88.989666	-3.294080	1.776704
-89.215146	-5.053780	1.781709
-89.641083	-4.248224	1.786714
-89.561807	-16.338651	1.791718
-90.095004	1.827415	1.796723
-90.378538	-0.339395	1.801728
-91.180967	2.097124	1.806733
-91.279393	-13.830235	1.811738
-91.014388	-4.577622	1.816742
-91.184785	-6.527825	1.821747
-91.323847	-10.652872	1.826752
-91.320854	0.319021	1.831757
-91.808045	2.063984	1.836762
-92.344154	-5.972429	1.841766
-92.812268	-9.520839	1.846771
-92.665964	-12.790345	1.851776
-92.906285	-6.730379	1.856781
-92.813575	-9.828773	1.861786
-93.496786	-3.297561	1.866790
-94.332085	-4.309630	1.871795
-94.240932	-11.749601	1.876800
-94.507333	-5.090549	1.881805
-94.402442	-4.633317	1.886810
-94.360256	-9.976417	1.891814
-94.873876	-0.713747	1.896819
-95.300472	-14.839198	1.901824
-95.642530	-9.029109	1.906829
-95.756937	-12.223900	1.911834
-95.920785	-15.793486	1.916838
-96.312278	-7.176459	1.921843
-96.201416	-18.320218	1.926848
-96.949064	-6.967607	1.931853
-97.389322	-14.740531	1.936858
-97.418274	-10.875079	1.941862
-97.915282	-9.859983	1.946867
-97.777822	-9.945099	1.951872
-97.929657	-12.573252	1.956877
-98.003721	-13.408377	1.961882
-98.286530	-17.289108	1.966886
-99.118294	-4.163717	1.971891
-99.466416	-22.330485	1.976896
-99.787402	-11.109979	1.981901
-99.888909	-10.559040	1.986906
-99.447342	-16.831452	1.991910
-99.568440	-7.969499	1.996915
-99.915610	-9.689736	2.006912
-99.983327	-11.789459	2.016909
-99.547711	-5.771034	2.026906
-99.273175	-4.513636	2.036902
-98.307208	-8.306582	2.046899
-98.266111	-4.069171	2.056896
-97.652111	-3.206466	2.066893
-96.925052	-4.989408	2.076890
-96.698338	-7.289426	2.086886
-95.969432	-6.753853	2.096883
-95.235339	-4.488325	2.106880
-95.010078	-7.778974	2.116877
-94.612344	-7.588055	2.126874
-93.911460	-6.745128	2.136870
-93.844173	-2.259956	2.146867
-92.838252	-7.448149	2.156864
-92.257150	-8.776492	2.166861
-92.157903	-9.273131	2.176858
-91.806694	-11.730570	2.186854
-90.918396	-11.495935	2.196851
-90.765864	-9.034541	2.206848
-89.693774	-11.593445	2.216845
-89.282687	-8.937737	2.226842
-89.152734	-9.318560	2.236838
-88.454593	-6.839987	2.246835
-87.695414	-6.437479	2.256832
-87.417862	-10.678693	2.266829
-87.364178	-6.023514	2.276826
-86.485853	-2.143017	2.286822
-86.142864	-3.946280	2.296819
-85.253277	-10.090396	2.306816
-84.721713	-6.918281	2.316813
-84.763445	-4.315526	2.326810
-84.108500	3.903468	2.336806
-83.271245	-7.906902	2.346803
-83.008360	-6.205772	2.356800
-82.524027	-2.377932	2.366797
-81.736167	-0.988920	2.376794
-81.443988	-2.140212	2.386790
-81.254688	-3.944994	2.396787
-80.398709	-10.241984	2.406784
-79.942628	-9.596840	2.416781
-79.647309	-12.626274	2.426778
-78.972308	-9.528385	2.436774
-78.413118	-6.974155	2.446771
-78.217563	-5.471862	2.456768
-77.718183	-3.657315	2.466765
-76.894282	-6.685312	2.476762
-75.957850	-8.660528	2.486758
-75.842689	-5.462460	2.496755
-75.617498	-10.523629	2.506752
-75.105338	-10.490234	2.516749
-74.293026	-8.718816	2.526746
-74.128078	-4.922645	2.536742
-73.366454	-6.848846	2.546739
-72.593370	-12.397048	2.556736
-72.279506	-12.518392	2.566733
-72.272480	-3.610801	2.576730
-71.674551	-6.046027	2.586726
-70.852183	-11.180387	2.596723
-70.645617	-10.694310	2.606720
-69.862599	-16.261351	2.616717
-69.209376	-13.649647	2.626714
-69.296710	-3.936833	2.636710
-67.999945	-2.951313	2.646707
-67.645187	1.110471	2.656704
-67.471903	-1.960916	2.666701
-67.381520	0.131849	2.676698
-66.535062	-6.648225	2.686694
-66.088304	-5.557760	2.696691
-65.135609	-9.718959	2.706688
-64.687839	-7.920923	2.716685
-64.588588	-3.925929	2.726682
-64.049724	-8.199716	2.736678
-63.203384	-6.468924	2.746675
-63.015334	-12.418767	2.756672
-62.601973	-7.676968	2.766669
-61.924789	-7.462752	2.776666
-61.527017	-4.016869	2.786662
-60.476773	-6.421379	2.796659
-60.110996	-7.207917	2.806656
-59.645374	-12.309843	2.816653
-59.882631	-6.438588	2.826650
-59.304164	-3.922333	2.836646
-58.386247	-8.047124	2.846643
-57.774620	-10.076816	2.856640
-56.926124	-12.523856	2.866637
-56.750974	-20.323685	2.876634
-56.528256	-7.222907	2.886630
-56.236670	-10.924289	2.896627
-55.353413	-7.878203	2.906624
-54.982377	-2.878832	2.916621
-54.478741	-10.603261	2.926618
-53.794834	-14.454225	2.936614
-53.590202	-9.090119	2.946611
-52.850465	-17.012648	2.956608
-52.083637	-18.690162	2.966605
-52.009176	-14.506508	2.976602
-51.623738	-8.312383	2.986598
-50.627433	-17.400024	2.996595
-50.496913	-16.997725	3.006592
-50.265288	-13.544970	3.016589
-49.454887	-7.737418	3.026586
-48.828148	-11.528496	3.036582
-47.775742	-12.614699	3.046579
-47.637172	-6.831603	3.056576
-47.592748	-11.451950	3.066573
-47.235839	-7.067674	3.076570
-45.945731	-5.962096	3.086566
-45.754746	-7.703535	3.096563
-45.810770	-3.270573	3.106560
-44.496492	-13.528398	3.116557
-44.005972	-13.474607	3.126554
-44.150507	-13.286011	3.136550
-43.827293	-17.270251	3.146547
-42.644576	-13.492109	3.156544
-42.629945	-12.588446	3.166541
-41.732838	-6.773768	3.176538
-40.987627	-10.450182	3.186534
-41.005488	-21.346639	3.196531
-40.507535	-15.284432	3.206528
-39.741893	-15.400059	3.216525
-39.255244	-13.292748	3.226522
-39.097648	-11.723880	3.236518
-38.180874	-16.187130	3.246515
-37.705503	-18.075620	3.256512
-37.835751	-15.258792	3.266509
-36.585315	-17.522502	3.276506
-35.845352	-16.408852	3.286502
-36.244360	-13.150013	3.296499
-35.448793	-10.965622	3.306496
-34.719081	-22.112006	3.316493
-34.283536	-11.255174	3.326490
-34.045482	-15.272876	3.336486
-32.925472	-14.477674	3.346483
-32.834745	-11.279296	3.356480
-32.431238	-10.986983	3.366477
-31.981519	-14.885754	3.376474
-31.143040	-12.822303	3.386470
-31.063003	-11.319970	3.396467
-30.050160	-18.119195	3.406464
-29.647277	-13.995465	3.416461
-29.774849	-14.284479	3.426458
-29.190285	-14.775640	3.436454
-28.430474	-19.399314	3.446451
-27.465432	-18.618856	3.456448
-26.974190	-13.191942	3.466445
-27.327664	-11.531404	3.476442
-26.425402	-12.124177	3.486438
-25.708717	-12.741623	3.496435
-25.535038	-10.596315	3.506432
-24.722025	-14.317387	3.516429
-23.951201	-13.547915	3.526426
-23.767577	-16.560162	3.536422
-23.409633	-12.709330	3.546419
-23.143593	-11.173503	3.556416
-22.149562	-15.602370	3.566413
-21.900252	-13.641727	3.576410
-21.010158	-7.577715	3.586406
-20.850464	-13.955352	3.596403
-20.706310	-7.332075	3.606400
-19.649387	-11.479765	3.616397
-19.236042	-11.026278	3.626394
-18.774580	-9.654128	3.636390
-18.139772	-12.395406	3.646387
-17.448790	-12.043587	3.656384
-17.166701	-12.760887	3.666381
-17.190334	-8.204485	3.676378
-16.793536	-14.307971	3.686374
-15.943553	-11.664549	3.696371
-14.788223	-9.234886	3.706368
-14.426065	-9.502560	3.716365
-14.264040	-13.650674	3.726362
-14.338490	-7.200892	3.736358
-13.151782	-11.072002	3.746355
-12.667670	-11.396895	3.756352
-12.498501	-4.314444	3.766349
-11.302390	-8.352493	3.776346
-10.873597	-14.334844	3.786342
-10.593679	-6.311740	3.796339
-10.410328	-14.003476	3.806336
-10.097068	-9.199982	3.816333
-9.380847	-13.162807	3.826330
-9.138530	-15.917284	3.836326
-8.177814	-13.527586	3.846323
-8.120092	-15.269990	3.856320
-6.664987	-17.940745	3.866317
-6.638394	-13.745179	3.876314
-6.221308	-14.435917	3.886310
-5.834287	-13.995637	3.896307
-5.490283	-19.645982	3.906304
-4.763252	-9.597690	3.916301
-4.439548	-3.024210	3.926298
-3.912008	-7.428291	3.936294
-3.657529	-3.669914	3.946291
-2.939135	17.560617	3.956288
-2.633451	25.236058	3.966285
-2.559755	46.912446	3.976282
-1.988934	66.428054	3.986278
-1.433972	85.364836	3.996275
-0.754478	98.113175	4.006272
-0.487946	118.134067	4.016269
0.000000	144.649514	4.021274
0.533494	153.021320	4.026278
0.375081	153.837660	4.031283
0.451539	167.460855	4.036288
0.518434	179.294470	4.041293
0.569693	194.071730	4.046298
0.731536	186.850196	4.051302
0.863424	196.606956	4.056307
0.898511	176.835263	4.061312
0.792912	176.471662	4.066317
0.580589	185.236612	4.071322
0.888592	198.192451	4.076326
1.375450	211.153895	4.081331
1.088591	210.598422	4.086336
1.223261	203.692590	4.091341
1.001944	205.973529	4.096346
1.302643	209.887846	4.101350
1.087723	195.774353	4.106355
1.145707	208.022882	4.111360
1.286038	207.859542	4.116365
1.030315	203.858407	4.121370
0.997584	209.914934	4.126374
1.150328	218.076954	4.131379
1.215424	206.142620	4.136384
1.139881	215.461062	4.141389
1.039245	215.558392	4.146394
1.142438	216.444522	4.151398
0.974584	219.436247	4.156403
1.250657	223.635466	4.161408
1.406937	218.779081	4.166413
1.326064	226.597704	4.171418
1.462155	216.579894	4.176422
1.202760	220.696238	4.181427
1.489066	220.882186	4.186432
1.707555	217.210309	4.191437
1.561417	231.346525	4.196442
1.587984	213.950703	4.201446
1.371569	220.615554	4.206451
1.448911	213.108897	4.211456
1.457990	209.123736	4.216461
1.085729	199.113868	4.221466
1.333850	211.510961	4.226470
1.000100	219.440086	4.231475
1.574713	216.267862	4.236480
1.327199	217.382779	4.241485
1.461121	226.612145	4.246490
1.504054	208.997530	4.251494
1.136449	217.150333	4.256499
1.372560	211.994155	4.261504
1.455113	220.851995	4.266509
1.602436	218.076588	4.271514
1.527529	215.896965	4.276518
1.726474	216.619969	4.281523
1.407782	215.458649	4.286528
1.690519	221.052885	4.291533
1.635741	229.232631	4.296538
1.684973	226.333421	4.301542
1.493490	212.457552	4.306547
1.456565	216.889550	4.311552
1.588851	220.298671	4.316557
1.627213	220.781968	4.321562
1.980543	215.815872	4.326566
1.847339	214.186038	4.331571
1.399482	214.017653	4.336576
1.910465	220.432939	4.341581
1.762383	229.854615	4.346586
1.889726	214.898831	4.351590
1.687181	220.975497	4.356595
1.250373	229.921838	4.361600
1.524625	222.836509	4.366605
1.288936	226.464858	4.371610
1.949431	241.596934	4.376614
1.796285	249.753378	4.381619
1.748283	244.474312	4.386624
2.093835	252.569572	4.391629
2.086396	250.309861	4.396634
1.978587	232.226745	4.401638
1.804248	236.425057	4.406643
1.609214	226.971791	4.411648
1.466304	233.026512	4.416653
1.825050	248.900994	4.421658
2.107949	243.717295	4.426662
2.162365	253.710941	4.431667
2.083090	249.850764	4.436672
2.112268	250.842931	4.441677
1.880926	255.225559	4.446682
1.814858	256.890675	4.451686
2.010121	260.958099	4.456691
1.913786	252.304581	4.461696
1.721655	255.370402	4.466701
1.384715	252.810062	4.471706
1.926224	250.001493	4.476710
1.923161	256.751073	4.481715
1.781976	254.126425	4.486720
1.931317	254.358226	4.491725
1.696926	254.103843	4.496730
2.082345	263.081072	4.501734
2.235900	279.590767	4.506739
2.418379	278.452305	4.511744
1.964145	264.960855	4.516749
1.960096	272.248338	4.521754
2.469793	273.274498	4.526758
2.118294	279.364697	4.531763
2.063509	280.531253	4.536768
2.696940	276.344815	4.541773
2.025095	270.176255	4.546778
2.592591	269.173499	4.551782
2.453442	262.825035	4.556787
2.085897	254.924429	4.561792
2.366132	255.053962	4.566797
1.621493	249.696313	4.571802
2.123445	260.539685	4.576806
2.258591	276.852736	4.581811
2.428999	287.938900	4.586816
2.314122	281.841150	4.591821
2.106419	290.944016	4.596826
2.403016	286.073957	4.601830
2.475545	286.818766	4.606835
2.388791	287.906375	4.611840
2.575583	291.723221	4.616845
2.002301	292.943794	4.621850
2.396699	287.360103	4.626854
2.375544	288.326303	4.631859
2.462177	291.640612	4.636864
2.509774	287.388943	4.641869
2.211057	295.541190	4.646874
2.456019	298.043797	4.651878
2.443769	288.070529	4.656883
2.760239	290.117052	4.661888
2.670047	285.241822	4.666893
2.492977	294.533774	4.671898
2.620167	291.620608	4.676902
2.572306	292.830019	4.681907
2.428447	297.448337	4.686912
2.412081	283.497713	4.691917
2.390744	301.018825	4.696922
2.486833	299.902022	4.701926
2.339823	296.845582	4.706931
2.209729	295.290406	4.711936
2.730602	303.324190	4.716941
2.743106	322.238598	4.721946
2.800939	312.373249	4.726950
2.649155	306.015027	4.731955
2.533753	310.608491	4.736960
2.880342	310.114077	4.741965
2.686431	319.067062	4.746970
2.731482	315.480033	4.751974
2.824822	312.463561	4.756979
2.611936	311.863228	4.761984
2.908010	323.108300	4.766989
2.802998	331.111351	4.771994
2.869473	328.580046	4.776998
2.760452	327.654805	4.782003
2.839410	319.296531	4.787008
2.998044	330.986155	4.792013
2.777504	325.702982	4.797018
3.105919	327.208212	4.802022
2.822089	314.398798	4.807027
2.509419	298.363050	4.812032
2.625814	308.613816	4.817037
2.865635	329.759194	4.822042
3.004284	315.549724	4.827046
2.684169	323.562475	4.832051
2.961394	328.574349	4.837056
3.123465	322.606967	4.842061
2.943250	332.832458	4.847066
2.893264	321.303346	4.852070
3.060581	329.410907	4.857075
3.037435	324.137549	4.862080
3.096654	316.639577	4.867085
2.921496	324.948903	4.872090
2.938576	324.481829	4.877094
3.181403	319.688186	4.882099
2.927413	324.547409	4.887104
3.111031	306.361303	4.892109
2.897567	327.704169	4.897114
3.309521	317.547103	4.902118
3.189919	321.801262	4.907123
2.941784	330.237766	4.912128
3.476642	319.320466	4.917133
2.956840	324.413706	4.922138
3.188798	324.914753	4.927142
3.249318	319.596114	4.932147
2.843408	328.963222	4.937152
3.075856	323.295140	4.942157
3.198140	326.220309	4.947162
3.014091	325.338521	4.952166
3.083434	327.718772	4.957171
3.121256	325.190651	4.962176
3.200734	321.470816	4.967181
3.352942	344.174123	4.972186
3.436101	336.154555	4.977190
3.463240	332.576420	4.982195
3.245734	325.567059	4.987200
3.344810	335.246480	4.992205
3.320038	336.905136	4.997210
3.218810	339.812600	5.002214
3.779379	340.374271	5.007219
3.466343	336.062552	5.012224
3.534538	325.499278	5.017229
3.198894	330.227232	5.022234
3.298442	329.934707	5.027238
3.208176	328.043163	5.032243
3.104746	351.842931	5.037248
3.373663	343.588244	5.042253
3.534980	353.447167	5.047258
3.517614	343.883391	5.052262
3.543025	353.136592	5.057267
3.191162	355.625535	5.062272
3.684028	343.534745	5.067277
3.396781	356.329176	5.072282
3.598490	349.676563	5.077286
3.282160	358.975717	5.082291
3.392395	361.642414	5.087296
3.967896	358.732666	5.092301
3.470501	363.070549	5.097306
3.334777	359.510992	5.102310
3.321435	357.895753	5.107315
3.364986	369.031279	5.112320
3.586769	360.052306	5.117325
3.363924	366.878721	5.122330
3.233256	372.577444	5.127334
3.713153	385.562689	5.132339
3.638520	399.885099	5.137344
3.970944	389.255170	5.142349
4.014799	386.203298	5.147354
3.789990	387.705373	5.152358
3.644880	383.684226	5.157363
3.885857	402.442356	5.162368
3.810386	393.456335	5.167373
3.773791	392.597986	5.172378
3.682861	392.988916	5.177382
4.088049	394.045677	5.182387
4.040162	385.718514	5.187392
3.569668	363.340752	5.192397
3.588635	379.485952	5.197402
4.014237	379.616583	5.202406
3.900256	387.801320	5.207411
3.940181	394.535329	5.212416
4.128859	381.452354	5.217421
3.750072	388.662860	5.222426
3.563825	393.344689	5.227430
3.839263	381.594300	5.232435
3.669481	388.461830	5.237440
3.963418	391.137268	5.242445
3.816690	387.332471	5.247450
3.830320	394.644699	5.252454
4.128018	394.176762	5.257459
4.132329	381.454178	5.262464
4.563058	387.225355	5.267469
3.893370	388.949179	5.272474
3.817331	386.887331	5.277478
4.347349	397.352779	5.282483
3.804785	388.729151	5.287488
3.861829	383.890197	5.292493
3.733293	386.357022	5.297498
4.016606	387.254465	5.302502
3.804460	384.572522	5.307507
3.525190	389.429653	5.312512
4.267946	403.787887	5.317517
4.385839	413.048248	5.322522
4.260108	404.561346	5.327526
4.025263	399.562714	5.332531
4.068800	413.911870	5.337536
4.107576	421.747999	5.342541
4.289379	415.890375	5.347546
4.597445	423.654712	5.352550
4.471712	421.553561	5.357555
4.063603	410.626973	5.362560
4.242762	420.267089	5.367565
4.474377	419.056316	5.372570
4.561182	416.047619	5.377574
4.335887	403.601561	5.382579
4.097374	403.204201	5.387584
4.406202	400.874139	5.392589
4.203409	408.918544	5.397594
4.727888	408.625245	5.402598
4.391233	405.304698	5.407603
4.294028	401.158367	5.412608
4.534305	384.589777	5.417613
4.186500	393.374798	5.422618
4.280522	412.628601	5.427622
4.697989	411.999859	5.432627
4.494297	417.894850	5.437632
4.688079	395.802877	5.442637
4.241826	399.258273	5.447642
4.316398	405.207056	5.452646
4.510826	414.695051	5.457651
4.372092	429.101947	5.462656
4.584526	426.629049	5.467661
4.530387	430.009213	5.472666
4.416684	426.280417	5.477670
4.529747	428.813257	5.482675
4.451359	426.161566	5.487680
4.587759	416.318415	5.492685
4.490135	424.616485	5.497690
4.452029	427.644504	5.502694
4.543461	425.923634	5.507699
4.344867	426.967879	5.512704
4.550004	418.953055	5.517709
4.596052	431.093238	5.522714
4.574534	420.479888	5.527718
4.654524	422.369782	5.532723
4.504955	416.484158	5.537728
4.883408	417.831501	5.542733
4.387448	419.671097	5.547738
4.391749	421.648165	5.552742
5.094990	431.084158	5.557747
4.982609	429.821632	5.562752
4.936990	417.419699	5.567757
4.792048	423.993625	5.572762
4.595880	415.615316	5.577766
4.860738	415.429895	5.582771
4.659703	420.490311	5.587776
4.867598	423.300036	5.592781
4.879245	430.425340	5.597786
4.903474	430.617752	5.602790
5.036370	419.700495	5.607795
4.992364	425.921189	5.612800
5.223893	421.969645	5.617805
4.997470	424.958318	5.622810
4.917590	418.501271	5.627814
5.053342	424.323859	5.632819
4.696257	419.078348	5.637824
4.776696	425.714862	5.642829
4.696103	431.829949	5.647834
5.203328	440.443476	5.652838
5.030613	433.876939	5.657843
4.898901	434.451659	5.662848
5.176922	448.796801	5.667853
5.026395	456.491350	5.672858
4.953751	453.115662	5.677862
5.156102	453.154345	5.682867
5.117962	455.594315	5.687872
5.199740	452.541454	5.692877
4.973592	458.624702	5.697882
5.086399	452.289535	5.702886
5.294735	463.049442	5.707891
4.933725	464.389456	5.712896
5.265080	458.573855	5.717901
4.984522	461.868326	5.722906
5.024695	454.182629	5.727910
5.221852	452.513251	5.732915
5.307114	464.291935	5.737920
5.297813	461.022540	5.742925
5.158213	453.757646	5.747930
5.202776	456.656883	5.752934
5.470281	460.122911	5.757939
5.385142	458.761331	5.762944
5.450011	456.111674	5.767949
5.149399	455.635241	5.772954
5.018956	462.905538	5.777958
5.415726	456.291302	5.782963
4.832704	463.636430	5.787968
5.270066	461.595010	5.792973
5.322071	453.537146	5.797978
5.077507	465.497539	5.802982
5.392313	459.539252	5.807987
4.796243	472.929558	5.812992
5.138850	456.449259	5.817997
5.302796	464.561003	5.823002
5.598317	457.499660	5.828006
5.337724	456.397928	5.833011
5.280288	470.199935	5.838016
5.460525	472.781805	5.843021
5.300308	477.602203	5.848026
5.444356	480.430642	5.853030
5.754846	475.268921	5.858035
5.547277	485.120570	5.863040
5.197939	480.584553	5.868045
5.468935	478.760225	5.873050
5.400906	479.884399	5.878054
5.460251	475.708279	5.883059
5.221478	489.746265	5.888064
5.409521	483.055018	5.893069
5.668884	491.515199	5.898074
5.585367	482.907966	5.903078
5.343972	479.850405	5.908083
5.543127	480.901556	5.913088
5.565857	479.215188	5.918093
5.459512	478.063741	5.923098
5.767626	486.395836	5.928102
5.648818	479.227918	5.933107
5.452975	489.189312	5.938112
5.706451	490.289452	5.943117
5.709323	507.838940	5.948122
5.874347	506.657778	5.953126
6.017168	498.578284	5.958131
5.655253	491.711647	5.963136
5.522075	486.526182	5.968141
5.761586	501.125430	5.973146
5.820857	507.915671	5.978150
5.793067	508.400697	5.983155
6.028144	520.780868	5.988160
6.049058	510.035293	5.993165
5.927867	506.798299	5.998170
5.594480	491.500279	6.003174
5.802266	500.222021	6.008179
5.750472	519.200638	6.013184
5.865688	513.685372	6.018189
5.933790	518.904341	6.023194
5.837749	515.865237	6.028198
6.072369	517.127764	6.033203
5.865176	522.260079	6.038208
6.224564	523.769653	6.043213
5.679636	519.039001	6.048218
5.536660	526.464544	6.053222
5.738694	515.492708	6.058227
6.206537	523.450962	6.063232
6.103398	518.397840	6.068237
6.204337	520.150273	6.073242
6.152587	520.548705	6.078246
6.185090	521.610193	6.083251
5.793030	508.067545	6.088256
6.113660	507.331561	6.093261
6.118950	488.338966	6.098266
5.692204	487.130266	6.103270
5.671672	486.831847	6.108275
5.578016	510.504531	6.113280
6.092175	509.894248	6.118285
5.807940	523.545149	6.123290
5.599201	526.230556	6.128294
6.072951	523.004390	6.133299
5.930135	522.846078	6.138304
6.262899	517.451928	6.143309
6.353461	519.605297	6.148314
6.202153	507.734525	6.153318
5.966647	497.030790	6.158323
5.569852	496.088250	6.163328
6.172019	489.176022	6.168333
5.749642	486.773503	6.173338
5.771412	496.438446	6.178342
6.075328	484.956160	6.183347
5.725312	502.833463	6.188352
6.124946	501.779069	6.193357
5.629522	490.670390	6.198362
5.659843	510.680241	6.203366
6.237168	523.852467	6.208371
5.917977	525.029048	6.213376
6.013078	506.578584	6.218381
5.811007	507.461202	6.223386
5.893670	502.430483	6.228390
6.065384	501.326946	6.233395
5.776490	513.099579	6.238400
5.850424	512.037554	6.243405
6.195676	515.494027	6.248410
5.905834	503.485060	6.253414
5.947364	501.723142	6.258419
5.445816	504.683756	6.263424
5.949316	510.007956	6.268429
5.905227	523.375823	6.273434
5.853208	524.819984	6.278438
6.423393	525.508333	6.283443
6.117317	514.794017	6.288448
6.158553	493.048523	6.293453
6.096548	494.940321	6.298458
5.828760	489.416499	6.303462
5.827670	486.793785	6.308467
5.794344	488.324031	6.313472
5.842976	495.592601	6.318477
6.384474	491.546302	6.323482
5.859570	493.502015	6.328486
6.007677	483.799352	6.333491
5.796957	493.955624	6.338496
5.663313	489.476698	6.343501
5.509403	492.720919	6.348506
5.762086	509.068552	6.353510
5.976914	505.525287	6.358515
5.989390	524.163874	6.363520
6.087368	519.548759	6.368525
5.744491	519.585910	6.373530
5.589475	515.887639	6.378534
6.304898	511.023673	6.383539
5.928676	521.363170	6.388544
6.066617	515.572197	6.393549
6.191051	510.134335	6.398554
5.699391	496.515306	6.403558
5.676813	487.507809	6.408563
6.014271	506.282589	6.413568
6.163514	511.776772	6.418573
5.475515	502.929794	6.423578
5.374349	515.317896	6.428582
5.896415	516.130868	6.433587
5.851331	524.943595	6.438592
5.771925	524.151358	6.443597
6.008517	525.936695	6.448602
5.937108	525.797694	6.453606
6.233900	525.429361	6.458611
6.145492	530.935622	6.463616
6.213703	524.179421	6.468621
6.264306	531.334409	6.473626
6.137151	515.427443	6.478630
5.994948	497.421761	6.483635
5.742191	496.896326	6.488640
5.767792	485.752949	6.493645
5.910024	495.483710	6.498650
5.895572	501.296168	6.503654
5.739475	490.297048	6.508659
5.730356	514.203738	6.513664
5.827017	520.840557	6.518669
5.930545	522.500404	6.523674
5.475877	530.402030	6.528678
6.053584	521.924437	6.533683
6.005468	523.838794	6.538688
5.754810	526.197670	6.543693
5.920623	531.801588	6.548698
5.794037	522.693350	6.553702
6.192302	517.967742	6.558707
6.325023	533.172043	6.563712
6.113741	517.685373	6.568717
6.185902	522.182208	6.573722
5.827636	498.932510	6.578726
6.282640	488.677600	6.583731
5.911972	490.602941	6.588736
5.806951	480.421189	6.593741
6.064949	493.824661	6.598746
5.701135	486.641814	6.603750
6.137812	485.641056	6.608755
5.703676	495.629433	6.613760
5.360436	498.452435	6.618765
5.597779	505.803704	6.623770
5.632033	520.492538	6.628774
5.902068	520.764668	6.633779
5.766978	524.222047	6.638784
5.909639	519.895707	6.643789
5.933644	530.323004	6.648794
5.750856	532.632120	6.653798
6.014379	515.000027	6.658803
5.954167	519.920245	6.663808
6.045392	525.537545	6.668813
5.973112	513.310465	6.673818
5.648239	529.801083	6.678822
6.131607	516.789782	6.683827
6.332444	526.146539	6.688832
5.925136	527.086162	6.693837
6.330840	515.239821	6.698842
6.059940	532.944758	6.703846
6.320390	521.245891	6.708851
5.727561	515.994143	6.713856
5.745031	495.464832	6.718861
5.907337	514.043772	6.723866
5.889427	526.371867	6.728870
5.993519	529.091514	6.733875
6.004096	527.624625	6.738880
5.937473	526.297258	6.743885
6.203962	525.238747	6.748890
5.803080	503.357154	6.753894
6.163322	492.398703	6.758899
5.682090	495.858750	6.763904
5.639856	506.099310	6.768909
5.790816	511.224189	6.773914
5.849836	523.182909	6.778918
6.236966	526.708003	6.783923
5.907841	527.296397	6.788928
6.089249	515.656256	6.793933
5.963506	506.546507	6.798938
5.731037	506.883610	6.803942
6.037559	507.413118	6.808947
6.134823	515.691671	6.813952
6.130801	503.146396	6.818957
6.274192	498.353241	6.823962
5.788495	496.128784	6.828966
6.099132	493.617254	6.833971
5.750120	496.246642	6.838976
5.874056	491.883561	6.843981
5.830563	505.627041	6.848986
5.535172	497.238933	6.853990
5.815094	499.447653	6.858995
5.709192	521.244737	6.864000
5.835349	524.051096	6.869005
6.082161	527.587673	6.874010
5.995544	524.635211	6.879014
6.223930	527.681312	6.884019
6.467908	512.532594	6.889024
5.869581	503.160795	6.894029
6.059388	497.946901	6.899034
5.981925	505.382068	6.904038
6.236493	501.319126	6.909043
5.900619	498.726993	6.914048
5.812259	500.009852	6.919053
5.914634	498.628349	6.924058
5.617165	493.069992	6.929062
5.926825	492.037460	6.934067
5.864694	494.756510	6.939072
5.690680	494.625880	6.944077
6.250261	496.696947	6.949082
5.617755	493.784707	6.954086
5.845446	493.735705	6.959091
6.031635	494.322313	6.964096
6.038766	494.884021	6.969101
5.946979	487.952357	6.974106
5.859615	487.089615	6.979110
5.820616	490.511282	6.984115
5.403631	493.347725	6.989120
5.734075	505.512723	6.994125
6.204372	515.178902	6.999130
5.976253	519.777152	7.004134
6.015597	507.282287	7.009139
5.912069	495.159281	7.014144
5.455993	487.956249	7.019149
6.051750	514.376113	7.024154
6.079037	523.661072	7.029158
6.240690	509.074636	7.034163
6.211523	507.175480	7.039168
5.843266	496.829676	7.044173
5.870398	494.219634	7.049178
5.709385	500.564000	7.054182
5.658929	496.767249	7.059187
5.713147	513.129127	7.064192
5.879281	520.480398	7.069197
5.845801	528.309056	7.074202
6.000088	529.670974	7.079206
6.069327	520.399552	7.084211
6.013753	532.976242	7.089216
6.038325	521.476226	7.094221
5.652470	516.088448	7.099226
5.692767	533.432040	7.104230
6.258992	522.882351	7.109235
5.662406	531.302090	7.114240
5.757213	530.853467	7.119245
5.926461	516.888752	7.124250
6.008281	529.413791	7.129254
6.266043	525.618689	7.134259
6.062622	524.396744	7.139264
5.751349	518.365881	7.144269
5.975691	527.859038	7.149274
5.829908	528.045571	7.154278
5.797294	527.220494	7.159283
5.842071	530.116355	7.164288
5.569922	532.159909	7.169293
5.596115	533.205674	7.174298
5.638141	532.927442	7.179302
5.764966	523.867267	7.184307
5.639609	535.241347	7.189312
5.577844	535.171981	7.194317
5.638754	527.987983	7.199322
5.432789	537.323955	7.204326
5.742923	541.957660	7.209331
5.709194	563.570138	7.214336
5.756775	570.515286	7.219341
5.869473	557.643115	7.224346
5.945841	563.425898	7.229350
6.069862	566.914023	7.234355
6.093350	567.909721	7.239360
5.942748	566.781016	7.244365
6.301108	565.058586	7.249370
6.030193	566.189652	7.254374
6.089801	557.465643	7.259379
5.963503	558.135767	7.264384
5.891972	546.688608	7.269389
5.987153	535.140141	7.274394
5.640412	535.606746	7.279398
6.128886	545.183885	7.284403
5.464792	547.679565	7.289408
6.180535	561.162907	7.294413
6.254217	554.736125	7.299418
5.926007	549.149508	7.304422
5.822484	530.314071	7.309427
5.530436	535.695522	7.314432
5.640322	551.022038	7.319437
5.624448	551.965866	7.324442
5.767371	571.504192	7.329446
5.862924	563.221567	7.334451
5.924517	566.173051	7.339456
6.204474	565.138940	7.344461
6.563887	562.462014	7.349466
5.977528	562.407617	7.354470
6.248344	558.305057	7.359475
6.201679	547.167925	7.364480
5.913815	532.801422	7.369485
5.698226	532.779133	7.374490
6.057631	536.496307	7.379494
5.983418	531.346809	7.384499
6.023895	535.968500	7.389504
5.928528	537.654698	7.394509
5.998711	517.376686	7.399514
6.189312	535.539502	7.404518
6.301106	523.717537	7.409523
6.019767	527.872537	7.414528
6.095074	529.518131	7.419533
6.401051	520.979932	7.424538
6.048870	532.879725	7.429542
6.441199	525.656626	7.434547
5.935434	528.301220	7.439552
5.678851	527.827136	7.444557
5.969361	525.803998	7.449562
5.599651	529.152177	7.454566
6.046208	526.906950	7.459571
6.169118	532.396440	7.464576
5.842018	528.959428	7.469581
6.093600	531.015190	7.474586
5.645500	530.241216	7.479590
5.895635	532.255187	7.484595
5.975188	534.490506	7.489600
5.644111	531.652281	7.494605
5.958664	531.824263	7.499610
5.865653	535.048109	7.504614
5.932536	522.963259	7.509619
6.249558	535.356066	7.514624
6.058196	530.545725	7.519629
6.332565	526.806077	7.524634
5.962088	521.417911	7.529638
6.164464	501.629048	7.534643
5.904792	500.727061	7.539648
5.532650	511.590787	7.544653
5.819095	508.385101	7.549658
5.903224	526.030033	7.554662
6.146762	521.123333	7.559667
5.900312	517.104788	7.564672
5.928066	512.595477	7.569677
5.709234	503.442198	7.574682
5.750325	522.774596	7.579686
6.250040	527.449011	7.584691
6.182006	519.004355	7.589696
5.587620	508.769538	7.594701
6.042688	507.035184	7.599706
5.300735	519.929008	7.604710
6.275947	518.535036	7.609715
6.131438	533.389757	7.614720
5.977596	524.401293	7.619725
6.124513	506.604675	7.624730
5.792212	503.386786	7.629734
5.790341	505.778507	7.634739
5.776869	504.358439	7.639744
5.581995	528.812455	7.644749
5.726309	535.068986	7.649754
5.960061	531.581771	7.654758
6.215546	534.108125	7.659763
6.127648	535.329143	7.664768
6.176144	536.419943	7.669773
6.011057	518.294311	7.674778
6.001178	518.135018	7.679782
5.939136	501.249310	7.684787
5.677273	503.347786	7.689792
5.586292	505.411545	7.694797
6.058279	536.136973	7.699802
5.972167	527.630394	7.704806
6.203181	525.099336	7.709811
5.871011	523.598642	7.714816
5.578971	520.347221	7.719821
6.053053	528.108288	7.724826
5.888966	538.792606	7.729830
6.215415	530.198508	7.734835
5.986191	520.828890	7.739840
6.137505	509.458187	7.744845
6.044462	507.942415	7.749850
5.995788	511.978621	7.754854
5.657240	501.308981	7.759859
5.671272	503.863820	7.764864
5.790848	518.554454	7.769869
6.176800	514.289109	7.774874
5.931143	511.623961	7.779878
6.234425	506.849023	7.784883
5.670778	505.264457	7.789888
5.598473	509.354121	7.794893
5.992792	517.947780	7.799898
6.155179	519.484573	7.804902
6.117545	502.006745	7.809907
5.707027	500.469347	7.814912
5.812596	500.314151	7.819917
5.890235	491.402673	7.824922
5.887742	515.164800	7.829926
5.940321	510.388511	7.834931
6.078380	512.397033	7.839936
5.884976	502.064196	7.844941
6.126945	494.744938	7.849946
5.536581	501.081339	7.854950
5.569667	517.540074	7.859955
5.646839	519.231730	7.864960
5.965201	530.870882	7.869965
6.184315	532.962629	7.874970
5.982387	537.140348	7.879974
5.967924	539.456810	7.884979
5.817456	533.974646	7.889984
5.835252	536.572279	7.894989
6.123891	532.277715	7.899994
5.792596	534.877130	7.904998
5.913329	531.536575	7.910003
6.081210	537.517853	7.915008
5.586594	534.125259	7.920013
5.820485	529.788489	7.925018
5.483762	535.824235	7.930022
5.551261	536.532201	7.935027
5.743099	528.877500	7.940032
5.704323	538.028012	7.945037
5.739352	532.709590	7.950042
5.501515	543.733354	7.955046
5.798702	537.657788	7.960051
5.828761	546.574071	7.965056
5.769988	558.888658	7.970061
6.263152	567.106368	7.975066
5.672030	555.756813	7.980070
5.865308	556.135832	7.985075
5.947255	567.511986	7.990080
5.985360	572.216767	7.995085
6.300892	567.076477	8.000090
5.889780	552.713667	8.005094
5.903542	541.951498	8.010099
5.985366	535.955932	8.015104
5.792380	547.333172	8.020109
5.875178	528.085245	8.025126
5.934051	551.156391	8.030144
6.201560	551.987336	8.035162
5.960610	543.787254	8.040179
5.714960	539.525798	8.045197
5.962118	535.530434	8.050214
6.313388	544.448907	8.055232
6.014947	542.803871	8.060250
5.645244	549.475856	8.065267
5.768498	546.955089	8.070285
6.261541	549.293294	8.075302
5.955184	548.180432	8.080320
5.686946	541.209189	8.085338
5.713928	545.419189	8.090355
5.925471	560.044650	8.095373
6.391864	567.420119	8.100390
5.997772	578.568225	8.105408
6.258797	571.393654	8.110426
6.231858	555.735013	8.115443
6.355399	551.188193	8.120461
6.032649	548.166412	8.125478
5.954164	551.705422	8.130496
6.001456	553.479780	8.135514
6.243218	530.915685	8.140531
5.963081	546.431251	8.145549
6.258893	539.401489	8.150566
5.869410	548.342703	8.155584
6.085386	545.744129	8.160602
6.103644	544.068498	8.165619
5.901798	552.080181	8.170637
6.328708	535.540879	8.175654
6.099670	545.907855	8.180672
5.930971	551.137106	8.185690
5.929775	543.276865	8.190707
5.937764	543.469312	8.195725
6.360111	541.804265	8.200742
5.985436	550.276919	8.205760
5.915487	541.518934	8.210778
6.151095	543.244276	8.215795
5.716669	552.781888	8.220813
6.039589	559.761158	8.225830
5.964872	577.648897	8.230848
5.872525	574.809859	8.235866
6.442275	572.998665	8.240883
6.202341	583.319056	8.245901
6.389172	569.480617	8.250918
6.214995	573.456957	8.255936
6.484910	577.009907	8.260954
6.127477	551.398994	8.265971
6.101665	553.454968	8.270989
5.956503	559.636132	8.276006
5.921272	552.720241	8.281024
5.943140	572.637412	8.286042
6.511437	565.388544	8.291059
6.194001	570.235078	8.296077
6.573505	566.622004	8.301094
6.213765	572.206413	8.306112
6.200615	576.090837	8.311130
6.633487	567.394918	8.316147
6.214112	548.713788	8.321165
6.313843	539.170187	8.326182
6.334992	530.884622	8.331200
5.958697	536.400713	8.336218
6.168579	542.717525	8.341235
6.090178	550.267782	8.346253
6.246063	557.209268	8.351270
6.301701	566.397346	8.356288
6.168135	566.151748	8.361306
6.435612	565.439526	8.366323
6.295534	577.289244	8.371341
6.233674	561.370873	8.376358
6.313543	572.368549	8.381376
6.095861	570.624267	8.386394
6.297976	570.560846	8.391411
6.455461	574.759988	8.396429
6.335561	568.455553	8.401446
6.222428	573.548618	8.406464
6.151201	570.547816	8.411482
6.246831	572.948734	8.416499
6.289280	570.597680	8.421517
6.217240	575.196556	8.426534
6.247724	574.099942	8.431552
6.036484	584.881666	8.436570
5.914240	569.711055	8.441587
6.195329	577.985365	8.446605
6.214387	562.679670	8.451622
6.059668	570.923469	8.456640
5.957666	581.757894	8.461658
6.564738	591.216110	8.466675
6.477066	596.893484	8.471693
6.504739	583.181675	8.476710
6.203656	588.404205	8.481728
6.251888	593.848770	8.486746
6.581637	585.069006	8.491763
6.356312	590.127579	8.496781
6.417289	591.862467	8.501798
6.383157	587.102101	8.506816
6.547506	600.959133	8.511834
6.443113	596.630486	8.516851
6.766265	599.439616	8.521869
6.935791	583.166845	8.526886
6.629858	575.359798	8.531904
6.491077	562.001828	8.536922
6.875647	572.683330	8.541939
6.288296	576.721064	8.546957
6.164839	570.075320	8.551974
6.535175	569.526890	8.556992
6.451250	573.029410	8.562010
6.412384	570.029725	8.567027
6.543216	569.718922	8.572045
6.324305	575.885384	8.577063
6.656308	571.968813	8.582080
6.043263	578.641497	8.587098
6.581742	573.587158	8.592115
6.268152	573.563394	8.597133
6.102434	583.507898	8.602151
6.748036	599.222174	8.607168
6.534949	610.573466	8.612186
7.170438	600.223318	8.617203
6.720360	592.400067	8.622221
6.827198	573.998143	8.627239
6.656456	579.137199	8.632256
6.481138	584.205174	8.637274
6.514458	573.399274	8.642291
6.762583	579.403275	8.647309
6.453084	576.363539	8.652327
6.577881	570.550275	8.657344
6.530085	584.582700	8.662362
6.383459	572.603466	8.667379
6.485413	576.567372	8.672397
6.381898	580.778208	8.677415
6.795348	593.549824	8.682432
6.475051	597.000701	8.687450
7.019084	585.762887	8.692467
7.161909	591.161219	8.697485
6.949266	572.545492	8.702503
6.919509	576.757255	8.707520
6.522132	569.638581	8.712538
6.526934	570.520279	8.717555
6.613746	567.496948	8.722573
6.516671	574.049423	8.727591
6.794972	570.946434	8.732608
5.952001	573.214408	8.737626
6.304563	574.762060	8.742643
6.680964	600.049204	8.747661
6.850440	607.411844	8.752679
6.962609	604.814374	8.757696
6.607252	584.970883	8.762714
6.772494	590.470598	8.767731
6.350057	594.259291	8.772749
6.436906	610.283164	8.777767
6.620528	602.899809	8.782784
6.564196	609.487846	8.787802
6.826481	600.405337	8.792819
6.674824	603.371530	8.797837
6.849462	596.865384	8.802855
6.962418	607.084029	8.807872
6.545473	609.872486	8.812890
6.500210	600.962345	8.817907
6.780181	605.199794	8.822925
6.730287	612.860097	8.827943
7.072878	609.776530	8.832960
6.716599	606.612881	8.837978
6.957774	606.908882	8.842995
6.605980	603.000850	8.848013
6.616347	603.091534	8.853031
6.760648	601.158352	8.858048
6.822709	602.206701	8.863066
6.699207	607.089313	8.868083
6.624936	604.243525	8.873101
6.365787	614.384074	8.878119
6.790025	599.030090	8.883136
6.262350	615.809207	8.888154
6.637486	630.594732	8.893171
6.752886	632.651850	8.898189
6.944150	637.569745	8.903207
7.139107	637.529165	8.908224
7.208277	644.680561	8.913242
7.202351	642.713688	8.918259
7.485578	627.691553	8.923277
6.580813	627.744399	8.928295
6.607262	605.380144	8.933312
6.764533	618.818325	8.938330
7.061467	629.194184	8.943347
7.238095	628.587800	8.948365
6.882924	627.247435	8.953383
6.852636	622.392726	8.958400
6.884230	630.121573	8.963418
6.902691	634.506425	8.968435
7.140108	634.129287	8.973453
6.978664	638.870394	8.978471
6.934800	632.936334	8.983488
6.929219	636.495132	8.988506
7.001931	646.239428	8.993523
6.897359	639.316522	8.998541
6.659861	645.943741	9.003559
6.985118	628.050680	9.008576
6.752491	637.487287	9.013594
6.729329	640.302219	9.018611
7.106951	634.449468	9.023629
6.986963	638.784110	9.028647
7.163879	634.874799	9.033664
6.951413	638.916570	9.038682
6.538960	641.267708	9.043699
6.971127	633.321808	9.048717
6.630381	647.696856	9.053735
6.846732	632.115210	9.058752
6.456311	650.753482	9.063770
6.835850	670.013542	9.068787
7.182488	679.584190	9.073805
6.905205	685.041163	9.078823
7.209527	675.946309	9.083840
7.165774	680.986936	9.088858
7.392098	675.448073	9.093875
7.679383	667.014665	9.098893
7.202863	666.776466	9.103911
7.507144	648.828801	9.108928
7.577104	648.732626	9.113946
6.924014	644.436706	9.118963
7.657977	637.714555	9.123981
7.132812	642.407465	9.128999
6.981925	635.930215	9.134016
7.456615	645.703555	9.139034
7.165666	642.892397	9.144051
7.178866	637.417513	9.149069
6.688941	638.071037	9.154087
7.060077	646.820533	9.159104
7.380482	631.504837	9.164122
7.073198	645.165520	9.169139
7.234796	636.448320	9.174157
7.244491	639.468403	9.179175
7.520635	634.223809	9.184192
7.210869	633.496318	9.189210
7.233948	648.713182	9.194227
7.027911	633.143478	9.199245
6.844610	639.800069	9.204263
6.992398	631.629217	9.209280
7.004600	655.048010	9.214298
7.224198	673.709906	9.219315
7.281863	662.950878	9.224333
7.127844	672.362434	9.229351
7.395470	669.515510	9.234368
7.397449	668.626367	9.239386
7.490034	672.458204	9.244403
7.638633	666.242949	9.249421
7.563531	652.874316	9.254439
7.448267	648.776183	9.259456
7.235386	648.033965	9.264474
7.258920	645.367960	9.269491
7.307000	636.397406	9.274509
6.984262	647.365014	9.279527
7.230593	659.907988	9.284544
7.306178	658.931421	9.289562
7.279255	673.813931	9.294579
7.684835	661.897950	9.299597
7.369690	667.728700	9.304615
7.476989	672.191899	9.309632
7.297714	668.607707	9.314650
7.134948	681.401161	9.319667
7.461757	675.168288	9.324685
7.103815	682.482812	9.329703
7.756746	675.956185	9.334720
7.830066	677.773669	9.339738
7.329727	681.466874	9.344755
7.491637	669.729960	9.349773
7.286143	676.897498	9.354791
7.339407	672.807171	9.359808
7.792530	675.460471	9.364826
7.733695	670.238868	9.369843
7.409535	655.341874	9.374861
7.467458	663.933024	9.379879
7.325202	675.580440	9.384896
7.422953	677.314932	9.389914
7.298706	679.506369	9.394931
7.515422	677.699911	9.399949
7.195838	683.570969	9.404967
7.487369	682.075671	9.409984
7.991143	680.261457	9.415002
7.502714	685.647825	9.420019
7.712814	680.175629	9.425037
7.782301	679.205388	9.430055
7.430848	682.737440	9.435072
7.410184	666.484975	9.440090
7.324544	672.584839	9.445107
7.782542	672.946959	9.450125
7.602618	682.126034	9.455143
7.436613	683.907517	9.460160
7.426357	669.079190	9.465178
7.139271	678.563257	9.470195
7.438644	683.334271	9.475213
7.264057	680.926369	9.480231
7.223925	682.708581	9.485248
7.478966	687.787532	9.490266
7.471969	681.074749	9.495283
7.510278	674.809126	9.500301
7.506599	678.989222	9.505319
7.639370	692.935240	9.510336
7.961827	699.028106	9.515354
7.821006	688.759692	9.520371
7.903508	683.672061	9.525389
7.530458	682.673415	9.530407
7.385655	684.806660	9.535424
7.614827	677.500534	9.540442
7.690017	688.584890	9.545459
8.010377	697.219833	9.550477
7.705478	690.391023	9.555495
7.299500	675.286563	9.560512
7.779960	691.601565	9.565530
7.590838	704.848007	9.570547
7.921046	698.560627	9.575565
7.768154	703.397371	9.580583
7.540563	711.569308	9.585600
8.099791	704.695870	9.590618
7.885181	709.117907	9.595635
7.915568	691.930820	9.600653
7.706064	689.254136	9.605671
7.586174	686.434220	9.610688
7.555238	684.154004	9.615706
7.636556	708.241454	9.620723
7.854543	708.331091	9.625741
7.713536	704.394493	9.630759
7.682563	704.399536	9.635776
7.863643	701.824058	9.640794
7.989180	705.397887	9.645811
7.921600	701.328031	9.650829
8.028658	712.841720	9.655847
7.959806	708.151650	9.660864
7.841223	709.083586	9.665882
8.060316	709.726539	9.670899
7.991745	711.296570	9.675917
8.026905	697.067117	9.680935
7.779920	690.365678	9.685952
8.311329	680.430580	9.690970
7.595175	682.531833	9.695987
7.810103	684.390145	9.701005
7.989813	695.034332	9.706023
7.921802	697.986247	9.711040
7.992686	701.266033	9.716058
8.095052	699.831897	9.721075
8.296802	691.409937	9.726093
8.178336	682.612302	9.731111
7.971432	682.682214	9.736128
8.214728	664.484452	9.741146
7.562441	676.479810	9.746163
7.894062	666.140759	9.751181
8.129890	671.993309	9.756199
7.657332	674.030058	9.761216
7.871314	670.317513	9.766234
7.489296	684.498289	9.771251
7.808360	691.911493	9.776269
7.807062	699.489162	9.781287
7.941259	704.907667	9.786304
8.102025	700.953586	9.791322
8.029873	706.676448	9.796339
8.404830	708.047964	9.801357
8.253129	702.802025	9.806375
7.992191	707.052643	9.811392
8.305519	697.687599	9.816410
8.011491	702.723575	9.821427
8.117424	701.294751	9.826445
8.372857	706.736607	9.831463
8.165890	712.314569	9.836480
8.378316	700.454481	9.841498
7.731596	703.376414	9.846515
7.968112	705.957463	9.851533
8.006441	697.750442	9.856551
7.455872	705.592822	9.861568
8.013554	700.106150	9.866586
7.958238	707.382588	9.871603
8.029400	708.013715	9.876621
8.100047	708.151463	9.881639
7.900609	707.416062	9.886656
8.033690	697.969175	9.891674
7.838649	703.307571	9.896691
8.244952	711.312537	9.901709
8.455727	728.379633	9.906727
7.652703	727.101888	9.911744
8.013561	728.502519	9.916762
8.035758	745.693687	9.921779
7.921420	741.784141	9.926797
8.204121	742.844838	9.931815
7.968409	734.346562	9.936832
8.551092	738.740016	9.941850
8.497556	735.678372	9.946867
8.590041	741.891165	9.951885
8.738456	743.280065	9.956903
8.627188	739.813873	9.961920
8.414123	724.064551	9.966938
8.290027	715.518011	9.971955
8.396572	706.476877	9.976973
8.402345	714.484446	9.981991
8.103829	697.665579	9.987008
7.989189	712.361934	9.992026
8.360895	726.620407	9.997043
8.564766	733.134147	10.002061
8.570835	738.147025	10.007079
8.424919	724.771204	10.012096
8.087929	708.933842	10.017114
8.132236	724.146858	10.022131
8.190511	737.298864	10.027149
8.273332	731.409059	10.032167
8.197899	738.281209	10.037184
8.488156	735.216748	10.042202
8.369774	738.390216	10.047219
8.338760	746.735191	10.052237
8.717603	729.802521	10.057255
8.243037	738.698936	10.062272
8.469276	738.385657	10.067290
8.593635	741.835290	10.072307
8.585324	729.473326	10.077325
8.758679	737.012535	10.082343
8.701735	737.203574	10.087360
8.614666	731.139463	10.092378
8.473805	733.985195	10.097395
8.385725	734.548310	10.102413
8.469633	733.380015	10.107431
8.388095	741.223975	10.112448
8.747835	746.232003	10.117466
8.659147	740.074858	10.122483
8.650775	738.948079	10.127501
8.508350	733.974386	10.132519
8.295920	722.675411	10.137536
8.471285	731.626381	10.142554
8.883548	724.872236	10.147571
8.501510	737.170333	10.152589
8.652650	728.379431	10.157607
8.441642	738.487062	10.162624
8.876260	740.845440	10.167642
8.538378	737.503129	10.172659
8.444273	730.000533	10.177677
8.696966	723.037890	10.182695
8.840558	746.061782	10.187712
8.277519	733.311543	10.192730
8.734335	726.234072	10.197747
8.247582	737.675625	10.202765
8.233792	727.564995	10.207783
8.534929	739.218085	10.212800
8.469866	733.881166	10.217818
8.659091	732.657573	10.222835
8.183395	740.718807	10.227853
8.480550	738.665328	10.232871
8.274445	737.841670	10.237888
8.441549	750.393556	10.242906
8.900815	752.976759	10.247923
8.820757	771.632482	10.252941
9.258441	765.208323	10.257959
9.031048	756.202193	10.262976
8.877907	738.172199	10.267994
9.075297	736.994686	10.273011
8.946202	745.892930	10.278029
8.995784	732.098417	10.283047
8.920892	737.513698	10.288064
8.805273	729.178324	10.293082
8.879927	736.299326	10.298099
8.709376	741.464977	10.303117
8.869613	733.855542	10.308135
8.759605	738.668044	10.313152
8.997112	734.975195	10.318170
9.284278	737.550783	10.323187
9.077538	736.096767	10.328205
9.236152	730.628780	10.333223
8.431578	741.882236	10.338240
8.917938	734.935470	10.343258
8.624730	737.134921	10.348275
8.628849	747.966586	10.353293
8.806009	730.318479	10.358311
8.607490	733.920982	10.363328
8.668092	736.223818	10.368346
8.936967	734.990923	10.373363
8.491424	744.169699	10.378381
8.622252	741.319714	10.383399
8.672308	743.045805	10.388416
8.799528	746.300686	10.393434
9.104832	765.014191	10.398451
8.714301	762.160905	10.403469
8.967578	775.646253	10.408487
8.784315	767.276632	10.413504
9.394100	778.690670	10.418522
9.131821	768.731937	10.423539
8.940556	771.531530	10.428557
8.928381	766.296824	10.433575
8.918486	770.662414	10.438592
8.799288	774.752098	10.443610
9.013502	767.189380	10.448627
8.696028	770.176474	10.453645
8.915689	767.413877	10.458663
8.738465	773.455386	10.463680
9.011750	782.097414	10.468698
9.122221	769.974121	10.473715
8.593641	771.876110	10.478733
8.837788	772.131269	10.483751
8.851557	778.848266	10.488768
8.961589	778.852902	10.493786
8.989825	793.898788	10.498803
9.025221	803.191938	10.503821
9.206672	808.652819	10.508839
9.056222	802.784045	10.513856
9.005033	804.124833	10.518874
9.073132	800.801637	10.523891
9.183201	804.570959	10.528909
9.073437	796.914449	10.533927
9.071883	805.198854	10.538944
9.073283	800.727377	10.543962
9.033609	800.860629	10.548979
9.151501	797.234493	10.553997
9.004684	797.323156	10.559015
9.101391	803.188841	10.564032
9.562818	802.500667	10.569050
9.437417	801.024858	10.574067
9.137690	803.230717	10.579085
9.379400	804.950547	10.584103
9.641924	809.839331	10.589120
9.124300	806.601285	10.594138
9.365184	802.249046	10.599155
9.318987	804.941862	10.604173
9.017931	804.704415	10.609191
9.120708	802.965302	10.614208
9.190212	801.970643	10.619226
9.318919	797.240820	10.624243
9.148273	803.822154	10.629261
9.281655	793.919482	10.634279
9.196012	801.934812	10.639296
8.704709	806.258586	10.644314
9.537050	816.693600	10.649331
9.363574	829.473407	10.654349
9.579783	817.932263	10.659367
9.550670	809.067739	10.664384
9.309356	802.686152	10.669402
9.457183	795.732837	10.674419
9.601958	797.543773	10.679437
9.416756	802.617595	10.684455
9.518216	792.048428	10.689472
9.080256	800.242583	10.694490
9.781108	806.768428	10.699507
9.322285	808.681266	10.704525
9.668448	813.567566	10.709543
9.696585	799.470673	10.714560
9.323085	792.462092	10.719578
9.541039	790.695373	10.724595
9.432345	792.879517	10.729613
9.150076	789.647233	10.734631
9.350672	815.771570	10.739648
9.728307	817.230243	10.744666
9.758259	823.309182	10.749683
9.663152	825.920373	10.754701
9.584231	821.203204	10.759719
9.848928	805.924547	10.764736
9.638175	805.136498	10.769754
9.861323	796.773322	10.774771
9.943513	791.523120	10.779789
9.506299	794.445678	10.784807
10.165977	789.807511	10.789824
9.784179	783.907516	10.794842
9.849095	788.272880	10.799859
9.676678	787.029674	10.804877
9.595461	789.928687	10.809895
10.212833	791.762441	10.814912
9.988265	799.488284	10.819930
9.619269	787.245473	10.824947
9.632977	797.877168	10.829965
9.691510	795.038205	10.834983
9.782577	786.524559	10.840000
9.404358	796.217335	10.845018
9.798019	787.404002	10.850035
9.483256	791.058514	10.855053
9.865599	791.432819	10.860071
10.092908	792.367303	10.865088
9.700320	793.901440	10.870106
9.741340	790.533341	10.875123
9.518966	792.706855	10.880141
9.628079	792.512051	10.885159
9.904653	789.486859	10.890176
9.188645	794.858733	10.895194
9.420175	795.763581	10.900211
9.671394	795.176089	10.905229
9.650513	791.032115	10.910247
9.639107	797.050009	10.915264
9.588115	802.232813	10.920282
9.544691	792.763832	10.925299
9.659645	807.280590	10.930317
10.060842	820.163479	10.935335
9.933198	817.946164	10.940352
9.803663	822.096630	10.945370
9.765282	815.175241	10.950387
10.249229	824.944401	10.955405
9.863114	826.858738	10.960423
9.973373	826.838338	10.965440
10.311430	834.138619	10.970458
10.063969	810.959221	10.975475
9.950652	799.133319	10.980493
9.853915	794.664181	10.985511
9.962605	782.374848	10.990528
9.718205	790.856881	10.995546
10.209697	806.069266	11.000563
10.145364	807.266581	11.005581
9.811810	805.958824	11.010599
10.281771	801.577171	11.015616
9.874080	808.163067	11.020634
9.928432	793.827981	11.025651
10.009321	814.427335	11.030669
10.236616	814.747693	11.035687
10.265346	815.990363	11.040704
10.067897	817.013951	11.045722
9.970183	793.010140	11.050739
9.949952	799.981206	11.055757
9.999269	814.289014	11.060775
10.390495	819.355608	11.065792
10.189547	810.079519	11.070810
10.066773	801.438034	11.075827
10.179148	810.629030	11.080845
9.941088	816.191923	11.085863
10.308629	803.652673	11.090880
10.103911	816.644930	11.095898
10.014471	831.048254	11.100915
10.213275	825.820584	11.105933
10.142494	829.464668	11.110951
10.191520	819.697252	11.115968
10.252877	827.226186	11.120986
10.087588	823.779583	11.126003
10.138142	828.890600	11.131021
10.098978	822.201212	11.136039
10.324329	811.455544	11.141056
9.941503	822.714543	11.146074
10.182785	820.945911	11.151091
10.084905	829.669539	11.156109
10.146411	825.509302	11.161127
10.322499	823.497784	11.166144
10.161581	823.934633	11.171162
10.506062	822.774788	11.176179
10.415429	828.797006	11.181197
10.162682	822.861571	11.186215
10.193686	809.515321	11.191232
10.050353	820.562280	11.196250
10.284226	821.422451	11.201267
10.384634	829.004143	11.206285
10.292607	823.128406	11.211303
10.388476	825.489759	11.216320
10.377373	823.406015	11.221338
10.495260	825.838703	11.226355
10.607304	831.074728	11.231373
10.375045	831.029571	11.236391
10.470529	822.193737	11.241408
10.607008	821.292072	11.246426
10.366666	819.803084	11.251443
10.373735	818.843210	11.256461
10.434725	820.559618	11.261479
10.473586	815.368378	11.266496
10.239772	830.098038	11.271514
10.779051	829.901612	11.276531
10.419729	822.739490	11.281549
10.234220	837.830394	11.286567
10.228090	829.486019	11.291584
10.219371	852.127539	11.296602
10.387139	863.358433	11.301619
10.517199	855.624632	11.306637
10.901402	861.782491	11.311655
10.801913	860.207100	11.316672
11.018438	854.877663	11.321690
10.606530	845.243927	11.326707
10.876196	828.807020	11.331725
10.786700	831.513533	11.336743
10.449031	823.384886	11.341760
10.729050	821.509232	11.346778
10.368139	825.351921	11.351795
10.682127	825.499416	11.356813
10.541627	837.666310	11.361831
10.469711	836.980372	11.366848
10.548474	849.977110	11.371866
10.561515	856.524392	11.376883
10.960034	858.502201	11.381901
10.880675	863.680096	11.386919
10.640131	855.491984	11.391936
11.200900	859.353720	11.396954
10.596673	849.774976	11.401971
10.895767	848.611061	11.406989
10.837442	852.167456	11.412007
10.980264	839.425584	11.417024
10.783480	837.847864	11.422042
10.766320	822.654225	11.427059
10.524125	824.292099	11.432077
10.681531	844.536476	11.437095
10.790981	848.926736	11.442112
10.755408	860.038877	11.447130
10.650845	858.828281	11.452147
10.872618	852.233098	11.457165
10.979033	859.629173	11.462183
11.061254	850.830761	11.467200
11.022224	854.444968	11.472218
10.868461	854.865472	11.477235
10.963275	853.094018	11.482253
11.061576	850.497041	11.487271
10.755337	847.601187	11.492288
11.263025	855.153973	11.497306
10.542926	848.247264	11.502323
11.041708	849.870241	11.507341
11.044301	864.925969	11.512359
10.764438	855.179144	11.517376
11.137395	863.410780	11.522394
10.764749	870.068824	11.527411
10.923529	866.262857	11.532429
10.973101	863.945809	11.537447
10.491799	852.155048	11.542464
10.919843	847.287076	11.547482
11.189882	851.937239	11.552499
11.007035	852.168299	11.557517
11.030362	846.633394	11.562535
11.049277	856.061787	11.567552
10.683404	851.184641	11.572570
10.535973	858.887457	11.577587
10.836975	851.329169	11.582605
10.715871	865.947419	11.587623
11.233726	878.472997	11.592640
11.689653	882.623603	11.597658
11.465987	878.472368	11.602675
11.393660	857.076269	11.607693
11.258286	858.927281	11.612711
11.276731	860.790914	11.617728
11.080499	852.644057	11.622746
10.961950	855.430988	11.627763
11.206639	853.278348	11.632781
11.064004	852.759664	11.637799
11.106176	849.555917	11.642816
11.495266	850.539887	11.647834
11.149254	855.685727	11.652851
11.221438	847.765697	11.657869
11.135181	860.848531	11.662887
11.365551	861.923249	11.667904
11.422431	854.902746	11.672922
11.423105	863.950146	11.677939
11.444350	856.156484	11.682957
11.351048	856.033904	11.687975
11.006611	860.704910	11.692992
11.374926	855.912016	11.698010
11.328507	858.940485	11.703027
11.581133	858.135253	11.708045
11.321827	864.681156	11.713063
11.369239	865.638656	11.718080
11.406268	856.217874	11.723098
11.406963	864.915885	11.728115
11.392431	859.749646	11.733133
11.306930	864.363245	11.738151
11.449093	872.679700	11.743168
11.701590	880.349123	11.748186
11.173577	872.463490	11.753203
11.539179	881.015628	11.758221
11.134595	884.162685	11.763239
11.242423	881.141115	11.768256
11.469729	877.625703	11.773274
11.179694	886.474208	11.778291
11.377781	882.653043	11.783309
11.515010	892.077539	11.788327
11.608171	881.348874	11.793344
11.741387	883.481996	11.798362
11.451719	885.405504	11.803379
11.992074	875.943174	11.808397
11.780936	884.330562	11.813415
11.841427	881.073176	11.818432
12.021137	889.495400	11.823450
11.631851	882.198279	11.828467
11.758387	870.572204	11.833485
11.987034	860.887695	11.838503
11.327592	868.100460	11.843520
11.625796	856.822214	11.848538
11.420602	879.130117	11.853555
11.746846	873.447026	11.858573
11.968360	876.479190	11.863591
11.736559	880.832681	11.868608
11.693107	867.903651	11.873626
11.832737	878.785517	11.878643
11.659790	876.114927	11.883661
11.846338	869.080739	11.888679
11.605346	873.033026	11.893696
11.785867	873.857977	11.898714
11.809476	875.538088	11.903731
12.018286	877.122066	11.908749
11.624105	870.237745	11.913767
11.496581	875.159887	11.918784
11.735856	876.752776	11.923802
11.936594	881.652247	11.928819
11.889968	873.213995	11.933837
11.906197	880.343790	11.938855
11.649837	880.834493	11.943872
11.673948	873.157268	11.948890
11.857956	883.026709	11.953907
11.801902	884.734431	11.958925
11.785133	883.275201	11.963943
11.827936	888.986897	11.968960
12.110710	884.533782	11.973978
11.863157	881.868111	11.978995
11.685404	875.970778	11.984013
11.959918	877.026941	11.989031
11.933433	882.966081	11.994048
11.911699	878.204746	11.999066
11.888427	888.510191	12.004083
11.904805	887.772176	12.009101
11.850917	883.331714	12.014119
11.825855	880.110988	12.019136
11.900183	877.221553	12.024154
11.869486	896.865614	12.029171
12.192427	906.377550	12.034189
12.220955	910.474999	12.039207
12.183962	906.543697	12.044224
12.549706	891.003688	12.049242
12.191592	884.871780	12.054259
12.116685	878.527459	12.059277
12.205937	875.950681	12.064295
11.766321	874.545003	12.069312
12.347103	867.191960	12.074330
12.318020	878.342206	12.079347
12.060404	881.371533	12.084365
12.116707	871.085980	12.089383
11.893401	873.711401	12.094400
12.147173	884.863256	12.099418
12.140195	906.458376	12.104435
12.436631	904.230990	12.109453
12.374387	915.317094	12.114471
12.360251	914.963258	12.119488
12.461289	895.164763	12.124506
12.379697	885.257806	12.129523
12.412482	879.721121	12.134541
12.443101	877.784755	12.139559
11.950245	879.671960	12.144576
12.289673	871.846073	12.149594
12.316904	879.181504	12.154611
12.082718	890.332190	12.159629
12.267994	901.148024	12.164647
12.278943	916.277605	12.169664
12.151221	904.306389	12.174682
12.456201	909.509781	12.179699
12.300379	923.874621	12.184717
12.614383	915.406522	12.189735
12.496443	921.408906	12.194752
12.585269	908.970618	12.199770
12.452046	909.154260	12.204787
12.490865	914.216078	12.209805
12.333202	917.678376	12.214823
12.097301	928.243388	12.219840
12.427652	914.111513	12.224858
12.192979	924.407044	12.229875
12.399782	915.660718	12.234893
12.613629	912.480585	12.239911
12.491538	919.358799	12.244928
12.398977	906.330229	12.249946
12.453025	917.292287	12.254963
12.501285	905.183953	12.259981
12.444479	913.762227	12.264999
12.298622	907.616092	12.270016
12.861989	908.503978	12.275034
12.615966	909.567336	12.280051
12.511377	909.987936	12.285069
12.676625	908.483097	12.290087
12.675187	911.178924	12.295104
12.968004	909.022607	12.300122
12.750912	911.464926	12.305139
12.647549	913.210828	12.310157
13.007007	909.425821	12.315175
12.801978	919.063314	12.320192
12.515329	901.444074	12.325210
12.547154	911.371700	12.330227
12.471226	908.166902	12.335245
12.926518	926.020884	12.340263
13.133785	935.995345	12.345280
12.880183	917.657253	12.350298
12.835525	913.560305	12.355315
12.946357	922.863822	12.360333
12.856192	905.886286	12.365351
12.999406	913.568378	12.370368
12.818581	906.910765	12.375386
13.276595	906.950470	12.380403
12.949539	909.798049	12.385421
12.887269	901.181489	12.390439
13.079653	907.596431	12.395456
12.827254	903.038772	12.400474
12.760275	906.969428	12.405491
12.744249	909.479108	12.410509
13.117704	904.865452	12.415527
12.902400	914.150735	12.420544
12.803752	904.294236	12.425562
12.752084	906.042961	12.430579
12.707952	905.923230	12.435597
12.960697	917.358135	12.440615
12.911439	937.106900	12.445632
12.673554	936.347368	12.450650
12.906366	936.909514	12.455667
12.978802	937.206208	12.460685
13.408881	935.632547	12.465703
13.170729	931.775616	12.470720
13.212808	943.043206	12.475738
13.413460	937.249676	12.480755
13.153819	943.026424	12.485773
13.242015	938.866051	12.490791
13.494233	936.771987	12.495808
13.051574	922.458765	12.500826
13.025458	909.371120	12.505843
12.930864	924.258820	12.510861
13.294476	928.826923	12.515879
13.180556	941.154627	12.520896
13.323181	935.082965	12.525914
13.495128	926.294398	12.530931
12.824216	928.908601	12.535949
12.970616	920.300257	12.540967
12.943302	933.225726	12.545984
12.874294	938.639705	12.551002
13.200913	928.571570	12.556019
12.968979	942.358170	12.561037
13.485373	931.316423	12.566055
13.049978	937.838084	12.571072
12.943452	936.098118	12.576090
13.203067	936.806192	12.581107
13.031731	958.118485	12.586125
13.774933	966.411465	12.591143
13.506728	975.611488	12.596160
13.424305	952.314885	12.601178
13.591896	947.261841	12.606195
13.495254	942.644818	12.611213
13.609996	927.876368	12.616231
13.404459	945.924063	12.621248
13.601844	934.892426	12.626266
13.812665	934.706698	12.631283
13.675758	936.012930	12.636301
13.573648	933.948627	12.641319
13.511580	939.035883	12.646336
13.324315	938.952147	12.651354
13.453120	935.988494	12.656371
13.214086	941.427191	12.661389
13.588871	932.570264	12.666407
13.503608	932.681371	12.671424
13.315748	947.826706	12.676442
13.725129	959.466302	12.681459
13.670207	968.691892	12.686477
13.739305	962.264746	12.691495
13.892926	962.777067	12.696512
13.278671	944.180010	12.701530
13.544557	958.312200	12.706547
13.857151	963.764330	12.711565
13.797274	971.262503	12.716583
13.965745	965.831770	12.721600
13.722407	963.781883	12.726618
13.918028	942.367704	12.731635
13.270648	939.253944	12.736653
13.940998	955.722300	12.741671
13.895529	962.086647	12.746688
13.723627	968.973162	12.751706
13.901047	965.584913	12.756723
13.455807	974.920260	12.761741
13.516100	972.918718	12.766759
13.546804	964.486657	12.771776
13.663299	967.120374	12.776794
13.785867	961.509095	12.781811
13.894433	969.787882	12.786829
14.106448	961.426074	12.791847
13.617106	966.897330	12.796864
13.803847	964.032697	12.801882
14.257634	965.069107	12.806899
14.150332	972.463359	12.811917
13.967145	970.657395	12.816935
13.838734	968.641552	12.821952
13.806730	970.843680	12.826970
13.987008	959.941633	12.831987
13.542126	965.870037	12.837005
14.085971	967.685525	12.842023
13.981997	967.172222	12.847040
13.933454	968.961377	12.852058
13.784969	958.833615	12.857075
14.201132	965.931423	12.862093
13.810922	961.300988	12.867111
14.050607	964.824016	12.872128
14.128669	984.616242	12.877146
14.472962	984.072130	12.882163
14.344065	970.374389	12.887181
14.247922	963.091296	12.892199
14.115946	958.517147	12.897216
13.920705	968.924256	12.902234
14.092452	947.704971	12.907251
14.032248	966.204882	12.912269
14.219686	973.747772	12.917287
14.797487	978.885370	12.922304
14.018338	978.641366	12.927322
14.386638	963.055588	12.932339
14.355670	970.372982	12.937357
14.051756	963.626361	12.942375
14.478154	968.909193	12.947392
14.228672	983.488462	12.952410
14.462185	973.439710	12.957427
14.235292	975.127809	12.962445
14.355626	973.538309	12.967463
14.657735	978.640633	12.972480
14.196912	977.197331	12.977498
14.498602	965.740092	12.982515
14.626218	965.854003	12.987533
14.650118	977.283292	12.992551
14.860967	965.912800	12.997568
14.570715	967.439786	13.002586
14.910310	961.278292	13.007603
14.709131	957.118377	13.012621
14.300855	960.436130	13.017639
14.283212	957.436188	13.022656
14.092859	958.207243	13.027674
14.237461	955.509842	13.032691
14.339421	951.510554	13.037709
14.379126	954.912892	13.042727
14.602346	968.420332	13.047744
14.320317	977.866735	13.052762
14.754418	977.527367	13.057779
14.940674	981.767505	13.062797
14.723987	978.816783	13.067815
14.662915	960.105322	13.072832
14.466535	965.233807	13.077850
14.598071	980.104446	13.082867
14.635110	980.221209	13.087885
14.432699	973.473067	13.092903
14.538419	980.333914	13.097920
14.485379	983.522160	13.102938
14.360203	982.019132	13.107955
14.677116	984.749848	13.112973
14.601630	989.788566	13.117991
14.590626	985.645063	13.123008
14.573408	982.955263	13.128026
14.686379	980.740645	13.133043
15.009021	993.898926	13.138061
14.382234	979.954423	13.143079
14.965120	993.626501	13.148096
15.222920	992.313739	13.153114
15.368260	974.806856	13.158131
15.207322	971.446893	13.163149
15.166094	970.112186	13.168167
15.394466	969.446798	13.173184
15.721748	975.256706	13.178202
15.231300	963.928374	13.183219
15.217883	964.713719	13.188237
14.833482	955.735734	13.193255
15.263716	948.204145	13.198272
14.445247	946.398270	13.203290
15.110118	952.388263	13.208307
15.228250	956.364931	13.213325
14.810196	953.161874	13.218343
15.131857	951.885349	13.223360
15.195209	956.076228	13.228378
15.027752	953.360227	13.233395
15.046955	946.432356	13.238413
15.260836	962.308914	13.243431
15.050095	950.030614	13.248448
15.180246	954.901686	13.253466
15.121895	959.450568	13.258483
15.371470	961.365751	13.263501
15.020849	964.885721	13.268519
15.582034	947.441631	13.273536
15.172002	958.829652	13.278554
15.071744	947.271528	13.283571
15.122037	959.149932	13.288589
15.110012	961.009389	13.293607
15.233593	963.734836	13.298624
14.992792	964.524512	13.303642
15.658919	961.927816	13.308659
15.385670	961.252896	13.313677
15.175889	969.808599	13.318695
15.079892	966.759084	13.323712
15.481682	975.578472	13.328730
15.113321	966.176580	13.333747
14.733820	971.108352	13.338765
14.806465	969.496072	13.343783
15.076322	964.561056	13.348800
15.076025	981.447976	13.353818
15.136941	982.643383	13.358835
15.350918	992.643141	13.363853
15.523548	998.744495	13.368871
15.754918	995.448053	13.373888
15.206077	998.086069	13.378906
15.456418	991.835861	13.383923
16.099228	996.233570	13.388941
15.899092	1001.317812	13.393959
16.035773	993.111020	13.398976
15.879865	983.401774	13.403994
15.771343	966.216606	13.409011
15.630175	969.517522	13.414029
15.397068	971.067291	13.419047
15.743102	965.340919	13.424064
15.760089	954.766391	13.429082
15.571935	970.035018	13.434099
15.607990	960.499380	13.439117
15.407015	957.940514	13.444135
15.572846	974.342362	13.449152
15.547333	984.539786	13.454170
15.645442	995.929984	13.459187
15.657902	991.259381	13.464205
15.541315	995.843937	13.469223
16.032919	992.126705	13.474240
15.688126	994.775291	13.479258
15.962131	1002.979751	13.484275
15.975942	986.073029	13.489293
15.538664	1003.079452	13.494311
15.826678	991.013479	13.499328
15.511303	993.032015	13.504346
15.487285	995.550124	13.509363
15.857566	993.206522	13.514381
15.531613	993.101745	13.519399
15.641024	991.505397	13.524416
15.631274	1002.019092	13.529434
15.875271	1013.978720	13.534451
15.962124	1013.128991	13.539469
15.851950	1016.913320	13.544487
16.166376	1009.406855	13.549504
16.561256	1015.963373	13.554522
16.656668	1004.376227	13.559539
16.534163	986.404430	13.564557
16.436112	986.148394	13.569575
16.474390	983.752108	13.574592
16.350357	987.838322	13.579610
16.052147	986.453418	13.584627
16.482133	975.799208	13.589645
16.087841	978.937486	13.594663
16.666013	972.059209	13.599680
16.459155	980.640021	13.604698
16.412726	971.264140	13.609715
16.119805	951.040531	13.614733
16.008171	953.533829	13.619751
16.075974	961.170214	13.624768
16.014132	971.962609	13.629786
15.859186	977.354274	13.634803
16.221009	978.592574	13.639821
16.251621	980.170160	13.644839
16.214655	975.879015	13.649856
16.126855	982.380714	13.654874
16.352932	983.284118	13.659891
16.824847	980.106744	13.664909
16.572712	973.548745	13.669927
16.366746	971.545004	13.674944
16.184412	981.497248	13.679962
16.008454	979.560167	13.684979
16.301549	976.354646	13.689997
16.222025	977.002956	13.695015
16.273961	972.062822	13.700032
16.412793	966.009494	13.705050
16.234497	979.078199	13.710067
16.667322	998.191436	13.715085
16.371269	1003.091239	13.720103
16.410942	1013.865215	13.725120
16.605231	1007.211349	13.730138
16.378191	1010.710000	13.735155
16.466518	1012.402793	13.740173
16.509618	1007.478288	13.745191
16.678927	1009.696959	13.750208
16.950792	1013.504791	13.755226
16.561782	1016.598500	13.760243
16.983220	1004.886303	13.765261
16.565013	1005.412178	13.770279
16.396783	1017.875341	13.775296
16.659718	1005.919424	13.780314
16.261620	1015.460334	13.785331
16.761403	1013.680603	13.790349
16.400434	1017.274347	13.795367
16.587778	1006.495495	13.800384
16.879269	1009.542234	13.805402
16.511667	1012.041079	13.810419
16.748978	1020.124096	13.815437
16.556605	1039.555066	13.820455
16.943027	1034.727811	13.825472
17.531386	1045.216134	13.830490
17.167308	1032.820742	13.835507
17.059045	1011.419970	13.840525
17.255489	1007.869110	13.845543
16.783985	999.035491	13.850560
17.085694	999.019292	13.855578
16.683431	1006.590925	13.860595
16.918785	999.807015	13.865613
17.244162	1005.005869	13.870631
17.121263	1001.640758	13.875648
17.028789	998.347358	13.880666
16.942368	1001.166374	13.885683
16.886100	1001.284867	13.890701
16.945683	995.903716	13.895719
17.055338	996.486727	13.900736
17.165270	1001.745010	13.905754
16.670225	1010.113123	13.910771
17.357291	1014.009809	13.915789
17.293716	1032.203685	13.920807
17.321012	1027.662488	13.925824
17.324153	1033.926271	13.930842
17.340325	1032.228888	13.935859
17.526083	1016.850552	13.940877
17.354745	998.357753	13.945895
16.869397	997.127962	13.950912
17.252766	1003.295859	13.955930
17.120957	1032.854750	13.960947
17.148880	1021.949637	13.965965
17.044672	1029.747710	13.970983
17.357917	1027.536410	13.976000
17.118839	1026.666448	13.981018
16.964350	1039.642670	13.986035
17.275933	1034.854230	13.991053
17.410269	1035.933507	13.996071
16.876489	1035.167642	14.001088
17.358182	1034.054264	14.006106
17.154849	1033.791712	14.011123
17.476839	1050.172015	14.016141
17.573835	1057.518967	14.021159
17.470917	1060.495845	14.026176
17.763941	1051.988248	14.031194
17.338981	1054.145865	14.036211
17.790050	1056.766899	14.041229
17.798918	1058.174889	14.046247
17.822009	1061.278847	14.051264
17.822742	1041.579115	14.056282
17.434264	1044.819977	14.061299
17.618357	1041.833729	14.066317
17.758339	1042.319187	14.071335
17.738058	1048.727806	14.076352
18.363675	1052.441419	14.081370
17.802984	1048.186519	14.086387
17.889456	1034.542289	14.091405
17.602141	1032.566233	14.096423
17.529459	1036.220720	14.101440
17.846509	1032.067164	14.106458
17.737155	1025.053940	14.111475
17.725094	1029.834112	14.116493
17.643815	1036.006815	14.121511
17.485269	1050.989907	14.126528
17.948257	1066.120088	14.131546
17.828034	1061.883306	14.136563
18.059819	1064.012078	14.141581
17.871099	1063.259721	14.146599
17.702116	1068.264008	14.151616
17.563085	1049.221714	14.156634
17.572256	1062.907326	14.161651
18.112381	1060.508320	14.166669
17.701318	1052.753541	14.171687
17.421939	1066.454835	14.176704
17.947563	1063.419691	14.181722
18.108836	1073.677461	14.186739
18.266156	1076.550462	14.191757
18.144564	1067.065369	14.196775
18.263393	1072.535965	14.201792
18.289178	1060.093468	14.206810
18.283378	1061.756244	14.211827
18.417419	1061.373840	14.216845
18.104253	1050.483276	14.221863
18.023618	1060.775340	14.226880
18.288216	1053.625936	14.231898
17.835129	1059.232922	14.236915
18.351094	1056.186787	14.241933
18.490240	1054.756348	14.246951
18.672541	1057.352373	14.251968
18.711067	1055.855985	14.256986
18.411580	1050.350648	14.262003
18.220951	1061.405049	14.267021
18.494232	1054.155388	14.272039
18.349421	1059.789084	14.277056
18.246645	1050.133560	14.282074
18.427645	1057.567331	14.287091
18.194557	1049.846748	14.292109
18.321483	1052.602756	14.297127
18.173936	1060.152549	14.302144
18.597063	1057.987939	14.307162
18.517475	1060.005480	14.312179
18.273393	1060.665005	14.317197
18.611140	1063.363533	14.322215
18.504663	1078.100609	14.327232
18.993975	1075.958852	14.332250
18.567650	1067.442076	14.337267
18.480004	1057.151390	14.342285
18.727368	1068.792016	14.347303
18.251945	1069.074660	14.352320
18.715492	1076.355971	14.357338
18.960134	1087.344736	14.362355
19.105170	1087.180178	14.367373
18.744730	1065.446068	14.372391
18.411721	1061.376930	14.377408
18.800937	1062.830358	14.382426
19.009077	1077.861972	14.387443
18.530827	1075.102335	14.392461
18.768461	1071.555637	14.397479
19.021552	1085.346783	14.402496
18.788292	1072.791041	14.407514
18.986351	1074.757318	14.412531
18.927334	1084.452136	14.417549
19.138690	1081.236952	14.422567
18.886420	1073.922279	14.427584
18.549242	1061.840487	14.432602
18.620250	1081.497403	14.437619
18.495839	1077.556967	14.442637
18.765582	1083.309947	14.447655
18.614168	1094.491704	14.452672
18.897619	1078.838815	14.457690
18.830958	1088.652616	14.462707
19.073635	1089.883959	14.467725
19.128476	1093.916849	14.472743
19.086278	1092.139009	14.477760
19.024862	1092.096161	14.482778
19.299283	1088.852778	14.487795
18.975031	1096.668561	14.492813
19.379340	1087.355875	14.497831
19.185105	1086.677658	14.502848
18.991006	1088.023327	14.507866
19.255177	1093.305215	14.512883
19.008139	1094.938016	14.517901
19.131695	1102.482138	14.522919
19.536726	1101.628730	14.527936
19.595441	1104.568516	14.532954
19.194908	1090.724488	14.537971
18.995325	1085.411971	14.542989
19.655053	1094.445235	14.548007
18.974731	1104.592921	14.553024
19.308639	1104.832380	14.558042
19.546103	1114.599979	14.563059
19.494161	1119.624985	14.568077
19.813388	1108.039142	14.573095
19.580758	1108.536930	14.578112
19.472969	1094.693845	14.583130
19.642925	1085.429166	14.588147
19.173309	1088.372910	14.593165
19.570075	1088.579875	14.598183
19.640044	1105.672957	14.603200
19.872673	1104.934026	14.608218
19.749458	1086.124478	14.613235
19.512625	1080.573285	14.618253
19.514554	1082.625703	14.623271
19.294489	1091.470962	14.628288
19.653472	1105.301609	14.633306
19.771235	1111.752660	14.638323
19.784402	1110.151039	14.643341
20.000636	1107.825544	14.648359
19.508639	1113.153205	14.653376
19.775721	1112.433742	14.658394
20.107613	1116.685930	14.663411
20.052019	1104.955707	14.668429
19.987868	1084.217940	14.673447
19.502688	1080.492576	14.678464
19.885359	1082.951371	14.683482
20.178245	1095.357244	14.688499
19.883180	1092.380946	14.693517
19.917872	1085.867740	14.698535
20.104744	1078.675341	14.703552
19.897799	1067.958437	14.708570
19.979127	1076.757530	14.713587
19.901987	1088.437540	14.718605
20.198469	1082.339855	14.723623
19.936733	1085.224638	14.728640
20.110324	1077.458099	14.733658
20.082964	1091.408062	14.738675
19.804531	1095.392415	14.743693
20.051818	1099.192937	14.748711
19.779465	1108.294127	14.753728
19.995401	1109.286228	14.758746
20.176660	1102.956124	14.763763
20.070731	1109.220744	14.768781
20.201137	1100.654720	14.773799
19.879444	1112.233277	14.778816
19.809829	1103.596171	14.783834
19.774937	1102.211977	14.788851
19.837989	1105.586453	14.793869
20.348940	1118.744249	14.798887
20.255122	1138.180614	14.803904
20.222474	1137.217282	14.808922
20.567080	1134.942490	14.813939
20.570844	1130.393364	14.818957
20.917350	1125.559331	14.823975
20.737424	1112.432909	14.828992
20.382089	1096.650753	14.834010
20.496429	1090.457360	14.839027
20.211912	1097.927581	14.844045
20.250478	1090.638967	14.849063
20.410111	1109.433989	14.854080
20.593976	1129.724931	14.859098
20.688845	1119.281039	14.864115
20.584365	1124.941912	14.869133
20.589362	1128.713425	14.874151
20.725424	1133.231620	14.879168
21.010984	1133.492894	14.884186
20.954797	1107.376482	14.889203
20.218145	1099.697448	14.894221
20.558217	1099.834707	14.899239
20.672855	1120.893010	14.904256
20.752014	1134.251321	14.909274
21.074520	1130.119666	14.914291
20.840390	1109.006594	14.919309
20.385864	1107.231147	14.924327
20.712682	1107.072199	14.929344
20.850237	1123.338361	14.934362
21.059429	1120.540437	14.939379
20.776178	1131.185500	14.944397
20.477972	1130.101354	14.949415
20.945184	1129.928520	14.954432
20.683778	1122.441730	14.959450
20.753702	1121.771965	14.964467
20.703845	1126.822609	14.969485
20.799477	1129.232274	14.974503
20.733287	1121.455964	14.979520
20.851725	1123.064634	14.984538
21.407147	1119.793830	14.989555
20.596762	1133.396442	14.994573
21.022891	1124.782434	14.999591
21.405030	1124.867822	15.004608
20.783429	1132.325192	15.009626
21.155470	1134.655060	15.014643
21.080560	1149.644424	15.019661
21.230347	1156.930288	15.024679
21.176678	1154.063849	15.029696
21.357631	1157.114817	15.034714
21.616149	1154.091376	15.039731
21.439306	1149.028982	15.044749
21.304326	1133.395982	15.049767
21.171311	1135.801134	15.054784
21.384289	1145.735020	15.059802
21.318062	1143.746611	15.064819
21.175086	1150.736267	15.069837
21.496254	1141.945610	15.074855
21.725461	1146.714456	15.079872
21.458489	1146.066435	15.084890
21.760209	1129.168787	15.089907
21.634969	1124.888336	15.094925
21.658705	1113.640564	15.099943
21.572453	1105.693196	15.104960
21.566743	1125.050337	15.109978
21.891927	1118.773466	15.114995
21.814575	1114.216568	15.120013
21.753890	1113.063813	15.125031
21.835503	1119.839758	15.130048
21.512482	1120.051011	15.135066
21.533173	1107.686877	15.140083
21.534941	1118.897520	15.145101
21.852481	1116.242209	15.150119
21.597923	1108.883808	15.155136
21.548421	1113.713928	15.160154
21.447407	1106.161906	15.165171
21.792470	1124.214745	15.170189
21.602814	1132.833724	15.175207
22.061800	1132.392979	15.180224
21.586630	1143.103018	15.185242
21.764029	1139.441520	15.190259
21.597498	1145.501671	15.195277
21.958278	1154.706701	15.200295
22.004085	1151.412724	15.205312
21.724988	1148.119997	15.210330
21.966551	1139.582324	15.215347
21.557753	1142.390778	15.220365
21.780987	1141.880167	15.225383
21.944618	1139.335863	15.230400
21.716486	1150.529231	15.235418
21.853297	1144.043120	15.240435
21.549474	1152.739350	15.245453
22.092595	1156.964709	15.250471
22.238067	1172.063915	15.255488
22.041123	1169.118141	15.260506
22.012372	1171.482742	15.265523
22.308762	1170.941862	15.270541
22.337662	1167.473141	15.275559
22.355795	1163.123182	15.280576
22.097057	1177.382534	15.285594
22.375948	1161.324826	15.290611
22.293633	1176.068215	15.295629
22.474235	1162.459012	15.300647
22.651153	1163.665072	15.305664
22.328281	1161.102418	15.310682
22.513253	1165.071574	15.315699
22.430265	1172.555576	15.320717
22.267637	1168.243140	15.325735
22.408388	1162.792931	15.330752
22.124556	1161.579235	15.335770
22.356785	1161.770245	15.340787
22.231279	1161.713248	15.345805
22.183780	1169.557868	15.350823
22.363196	1162.839481	15.355840
22.568992	1171.557707	15.360858
22.898804	1172.600960	15.365875
23.026426	1165.073504	15.370893
22.950608	1165.833011	15.375911
23.178878	1156.740085	15.380928
22.897322	1163.538618	15.385946
23.119510	1150.604764	15.390963
23.055767	1157.588341	15.395981
23.051998	1165.089487	15.400999
22.996469	1164.720873	15.406016
23.024477	1164.515138	15.411034
22.953299	1163.657416	15.416051
23.016875	1161.145486	15.421069
23.040685	1160.929819	15.426087
22.889049	1141.872971	15.431104
22.874479	1146.315424	15.436122
23.177350	1141.688235	15.441139
22.622764	1141.533272	15.446157
22.845083	1159.606160	15.451175
22.901857	1158.801972	15.456192
22.866874	1155.643070	15.461210
22.870701	1158.640019	15.466227
22.831709	1171.109382	15.471245
22.544191	1165.288249	15.476263
23.218598	1158.470664	15.481280
23.055997	1159.848110	15.486298
23.352226	1156.051903	15.491315
23.234608	1158.688740	15.496333
22.917129	1161.326121	15.501351
23.268281	1144.683219	15.506368
23.309791	1164.141611	15.511386
22.680486	1168.931508	15.516403
23.079848	1174.770455	15.521421
23.156141	1200.115746	15.526439
23.717868	1183.164195	15.531456
23.644639	1189.872210	15.536474
23.466476	1194.766257	15.541491
23.571596	1196.176764	15.546509
23.225318	1202.008951	15.551527
23.626132	1188.453671	15.556544
23.434989	1193.273501	15.561562
23.378334	1185.058192	15.566579
23.609001	1179.022587	15.571597
23.284253	1193.309065	15.576615
23.568029	1181.632607	15.581632
23.189720	1181.864074	15.586650
23.213590	1194.932822	15.591667
23.386900	1184.412466	15.596685
22.697364	1194.488122	15.601703
23.244050	1190.133372	15.606720
23.519583	1212.600425	15.611738
23.944468	1217.344643	15.616755
24.169163	1214.625224	15.621773
24.333769	1209.971392	15.626791
24.477796	1196.375718	15.631808
24.099678	1188.035106	15.636826
24.050067	1187.298202	15.641843
24.115107	1176.517120	15.646861
23.833693	1179.594551	15.651879
24.055194	1172.481783	15.656896
23.937045	1177.832363	15.661914
24.261625	1175.025092	15.666931
24.546175	1168.866367	15.671949
23.864531	1177.485258	15.676967
23.979363	1159.405311	15.681984
23.869203	1167.618202	15.687002
23.833507	1165.539680	15.692019
23.973415	1174.105480	15.697037
24.058758	1169.817573	15.702055
24.236317	1167.191033	15.707072
24.491975	1172.647190	15.712090
24.052799	1168.296470	15.717107
24.101409	1173.811843	15.722125
23.948610	1177.212763	15.727143
23.773756	1174.228279	15.732160
24.052386	1181.813985	15.737178
24.239367	1195.160727	15.742195
24.675858	1198.882191	15.747213
23.991873	1206.906632	15.752231
24.203299	1209.326590	15.757248
24.359483	1205.651281	15.762266
24.219932	1203.627022	15.767283
24.483060	1202.539725	15.772301
24.260688	1209.139473	15.777319
24.577312	1203.422234	15.782336
24.444990	1210.504631	15.787354
24.365045	1204.461589	15.792371
24.511229	1200.971399	15.797389
24.223836	1203.554970	15.802407
24.565814	1205.593009	15.807424
24.587120	1206.306850	15.812442
24.910445	1214.000886	15.817459
25.015766	1204.281939	15.822477
24.749872	1199.763046	15.827495
24.901514	1195.328686	15.832512
24.681049	1205.406303	15.837530
24.889437	1202.559681	15.842547
25.099150	1198.979408	15.847565
24.994826	1200.896359	15.852583
24.780126	1192.686056	15.857600
24.703024	1195.071294	15.862618
24.579206	1197.549334	15.867635
24.666737	1201.409897	15.872653
24.641508	1220.410575	15.877671
24.671325	1230.837537	15.882688
24.945303	1223.501859	15.887706
25.185817	1234.072929	15.892723
25.591024	1213.870336	15.897741
25.165898	1226.757057	15.902759
25.326469	1223.122351	15.907776
25.328910	1218.666328	15.912794
24.915143	1224.534148	15.917811
25.150512	1217.426140	15.922829
25.373448	1219.922924	15.927847
25.021951	1221.555777	15.932864
25.037686	1216.062158	15.937882
24.909056	1222.645937	15.942899
25.368524	1223.717248	15.947917
25.210249	1227.452539	15.952935
25.283105	1226.801179	15.957952
25.148161	1223.526600	15.962970
24.909583	1226.340239	15.967987
25.084892	1213.111777	15.973005
25.355590	1229.217344	15.978023
25.392968	1232.646507	15.983040
25.805724	1237.625021	15.988058
25.322624	1232.313121	15.993075
25.617717	1225.149910	15.998093
25.625267	1247.979258	16.003111
25.891175	1235.042398	16.008128
25.719582	1226.157618	16.013146
25.259520	1217.466058	16.018163
25.651218	1228.557248	16.023181
25.849719	1237.827094	16.028199
25.833839	1242.343017	16.033216
25.530005	1229.711872	16.038234
25.320595	1246.920440	16.043251
25.861233	1237.412966	16.048269
26.182852	1244.828573	16.053287
25.586301	1240.416592	16.058304
25.459991	1234.568639	16.063322
25.228116	1245.374524	16.068339
25.847163	1226.922911	16.073357
25.719785	1239.250333	16.078375
25.784548	1249.589219	16.083392
25.691454	1245.316383	16.088410
26.148801	1267.117103	16.093427
26.167197	1276.379900	16.098445
26.369407	1276.528265	16.103463
26.541955	1270.033800	16.108480
26.626801	1250.580440	16.113498
26.221067	1250.958191	16.118515
26.389671	1240.885411	16.123533
26.063421	1244.383675	16.128551
26.236747	1243.396732	16.133568
26.289215	1251.029511	16.138586
26.237994	1249.545265	16.143603
26.351778	1246.430120	16.148621
26.302461	1244.290468	16.153639
26.548884	1243.363813	16.158656
26.446590	1234.879697	16.163674
26.356143	1240.926058	16.168691
26.676624	1238.286380	16.173709
26.422053	1240.489714	16.178727
26.213948	1250.307443	16.183744
26.573205	1247.505026	16.188762
26.776978	1248.788909	16.193779
26.735746	1235.354303	16.198797
26.833108	1248.204984	16.203815
26.380233	1242.310916	16.208832
26.704090	1247.293186	16.213850
26.309588	1247.847803	16.218867
26.602760	1242.640725	16.223885
26.724362	1239.143195	16.228903
26.382808	1245.767886	16.233920
26.590813	1258.789548	16.238938
26.299155	1272.605264	16.243955
26.696927	1273.223467	16.248973
26.951728	1274.889407	16.253991
26.941816	1272.910518	16.259008
26.876655	1268.984199	16.264026
27.060389	1280.250537	16.269043
27.160950	1268.829654	16.274061
26.875845	1272.715952	16.279079
26.762494	1270.475921	16.284096
27.291847	1269.158159	16.289114
26.800239	1283.418518	16.294131
26.651831	1275.068418	16.299149
26.964507	1282.663081	16.304167
27.189215	1284.069468	16.309184
27.135389	1274.113947	16.314202
26.731073	1276.799637	16.319219
27.064091	1275.225542	16.324237
27.392983	1272.580523	16.329255
27.312970	1276.510290	16.334272
27.269533	1267.371912	16.339290
27.048237	1274.246694	16.344307
27.125321	1285.340612	16.349325
27.492031	1301.183063	16.354343
28.202756	1295.729802	16.359360
27.893122	1277.550982	16.364378
27.541905	1277.158679	16.369395
27.498527	1259.652920	16.374413
27.500381	1269.141682	16.379431
27.580227	1269.682810	16.384448
27.550915	1267.802024	16.389466
27.579063	1261.334712	16.394483
27.525448	1270.801987	16.399501
28.030122	1259.750933	16.404519
27.904404	1254.596152	16.409536
27.930104	1260.116545	16.414554
27.898219	1264.999293	16.419571
27.737091	1267.004824	16.424589
27.852491	1253.161507	16.429607
27.561224	1267.019277	16.434624
27.806213	1257.442431	16.439642
27.761899	1264.916901	16.444659
27.471751	1265.934862	16.449677
27.741074	1267.251945	16.454695
27.654821	1270.445770	16.459712
27.468554	1269.462295	16.464730
27.524023	1283.374650	16.469747
27.986205	1296.584010	16.474765
27.891323	1300.113120	16.479783
27.512933	1306.821909	16.484800
27.710160	1289.046607	16.489818
27.912394	1302.853881	16.494835
28.135137	1308.514368	16.499853
28.357681	1303.649311	16.504871
28.418523	1310.377219	16.509888
28.522403	1299.979345	16.514906
28.155341	1297.800375	16.519923
28.216377	1301.685052	16.524941
28.348015	1292.854554	16.529959
27.988640	1299.091693	16.534976
28.355453	1299.176087	16.539994
28.485149	1308.891647	16.545011
28.409822	1318.137764	16.550029
28.770286	1315.744568	16.555047
28.271339	1311.822229	16.560064
28.745901	1307.551873	16.565082
28.963650	1313.455703	16.570099
28.584793	1309.404748	16.575117
28.881865	1289.059800	16.580135
28.115696	1303.441400	16.585152
28.698286	1291.205372	16.590170
28.278480	1296.020327	16.595187
28.571959	1296.403119	16.600205
28.513087	1304.283162	16.605223
28.515289	1310.379503	16.610240
28.742715	1296.843892	16.615258
28.878791	1309.312615	16.620275
28.848049	1309.279628	16.625293
28.841894	1307.020594	16.630311
28.426046	1310.614076	16.635328
28.428597	1309.176791	16.640346
28.732351	1305.455278	16.645363
28.475855	1311.208411	16.650381
28.792437	1326.263975	16.655399
28.760603	1337.756728	16.660416
28.897051	1340.426169	16.665434
29.007658	1340.216151	16.670451
29.131615	1332.834493	16.675469
29.162810	1330.347602	16.680487
29.110776	1335.190415	16.685504
29.490137	1331.551995	16.690522
29.543385	1327.177651	16.695539
29.307659	1330.117995	16.700557
29.628553	1322.402439	16.705575
29.443972	1319.179001	16.710592
29.740420	1315.385475	16.715610
29.459170	1323.614680	16.720627
29.564359	1326.518439	16.725645
29.767014	1319.311889	16.730663
29.365816	1310.894340	16.735680
29.660438	1322.287155	16.740698
29.873324	1309.768085	16.745715
29.459890	1298.236949	16.750733
29.558769	1297.645431	16.755751
29.518184	1299.469914	16.760768
29.825358	1301.716106	16.765786
29.675236	1297.868465	16.770803
29.608020	1294.189322	16.775821
29.883935	1306.859201	16.780839
30.008349	1316.298882	16.785856
29.769108	1296.861142	16.790874
29.951691	1296.820257	16.795891
29.626758	1297.994390	16.800909
29.683649	1298.608624	16.805927
29.794038	1314.014182	16.810944
29.814418	1321.545640	16.815962
30.297858	1314.973500	16.820979
30.072841	1329.071880	16.825997
30.271961	1322.445028	16.831015
30.049320	1328.486230	16.836032
29.906774	1320.165051	16.841050
30.110525	1324.035462	16.846067
30.006340	1325.419354	16.851085
30.324667	1315.225187	16.856103
30.326525	1325.663947	16.861120
30.206011	1321.536980	16.866138
30.078419	1319.218209	16.871155
29.891990	1328.666650	16.876173
30.168770	1316.779845	16.881191
29.800377	1324.255454	16.886208
30.032790	1326.094011	16.891226
30.269228	1321.517180	16.896243
30.012652	1314.650729	16.901261
30.456943	1333.960896	16.906279
30.531582	1349.717695	16.911296
30.460673	1353.225510	16.916314
30.613815	1348.434964	16.921331
30.780573	1352.311531	16.926349
30.663866	1335.409585	16.931367
30.508110	1344.237605	16.936384
30.818172	1343.383829	16.941402
31.113282	1346.079654	16.946419
30.943161	1343.873456	16.951437
30.865149	1316.427295	16.956455
30.688304	1318.039397	16.961472
30.596887	1314.725675	16.966490
30.376784	1322.970701	16.971507
30.716882	1331.060419	16.976525
30.973699	1345.283052	16.981543
30.765439	1342.270230	16.986560
30.704701	1346.289327	16.991578
30.823487	1338.145955	16.996595
30.406124	1350.715357	17.001613
30.531525	1342.737806	17.006631
30.917237	1347.951158	17.011648
31.054715	1362.120023	17.016666
31.272844	1379.552943	17.021683
31.172469	1386.626173	17.026701
31.763373	1365.949226	17.031719
31.505723	1347.649482	17.036736
31.364157	1338.478554	17.041754
31.573240	1328.541504	17.046771
31.203415	1332.448983	17.051789
31.525826	1326.898841	17.056807
31.468656	1324.236094	17.061824
31.554073	1335.446769	17.066842
31.346146	1330.972924	17.071859
31.603962	1330.946306	17.076877
31.455618	1327.268041	17.081895
31.323843	1329.694276	17.086912
31.350525	1329.269476	17.091930
31.364079	1332.494755	17.096947
31.194780	1346.238233	17.101965
31.560325	1345.070915	17.106983
31.603563	1365.098543	17.112000
31.463970	1355.804053	17.117018
31.909858	1360.919222	17.122035
31.793685	1361.994885	17.127053
31.980006	1359.796762	17.132071
31.703408	1365.110752	17.137088
31.810049	1372.185787	17.142106
31.801197	1358.092171	17.147123
31.813965	1367.603587	17.152141
31.560099	1362.358656	17.157159
32.070415	1358.700827	17.162176
31.863209	1360.457344	17.167194
32.151529	1358.796186	17.172211
31.847389	1366.990637	17.177229
32.113653	1376.455989	17.182247
31.996033	1380.997918	17.187264
32.037967	1388.352997	17.192282
32.358144	1381.094997	17.197299
32.410203	1389.349545	17.202317
32.359910	1384.866020	17.207335
32.362784	1374.658105	17.212352
32.306509	1381.466925	17.217370
32.747687	1379.391002	17.222387
32.389332	1378.972324	17.227405
32.624748	1388.686110	17.232423
32.528380	1375.676280	17.237440
32.481170	1378.621519	17.242458
32.496781	1380.004402	17.247475
32.496941	1386.329452	17.252493
32.474768	1374.585594	17.257511
32.471744	1383.186684	17.262528
32.683760	1387.593908	17.267546
32.638542	1379.878546	17.272563
32.530045	1390.658909	17.277581
32.597128	1378.698645	17.282599
32.487832	1383.364777	17.287616
32.147646	1376.753525	17.292634
32.722891	1381.717285	17.297651
32.611423	1398.591643	17.302669
32.704565	1404.147332	17.307687
33.292360	1408.887368	17.312704
33.448044	1405.025093	17.317722
33.848292	1390.454017	17.322739
33.508716	1375.590184	17.327757
33.504377	1364.529567	17.332775
33.701283	1362.537945	17.337792
33.148806	1362.635767	17.342810
33.236310	1356.356181	17.347827
33.482045	1361.900666	17.352845
33.473834	1355.114960	17.357863
33.688133	1353.198792	17.362880
33.282237	1343.287963	17.367898
33.279580	1335.093126	17.372915
33.402265	1340.787578	17.377933
33.431424	1352.533188	17.382951
33.608675	1361.532241	17.387968
33.304486	1362.473411	17.392986
33.593113	1361.305885	17.398003
33.632140	1365.423756	17.403021
33.589129	1361.369327	17.408039
33.464119	1352.268471	17.413056
33.700170	1363.250594	17.418074
33.907821	1354.212946	17.423091
33.364896	1356.715788	17.428109
33.635739	1353.833957	17.433127
33.741309	1348.204104	17.438144
33.525178	1362.206158	17.443162
33.738460	1355.463950	17.448179
33.593571	1353.554334	17.453197
33.282151	1365.769144	17.458215
33.604512	1355.523495	17.463232
33.517714	1384.057895	17.468250
33.624864	1385.905863	17.473267
33.974003	1392.408731	17.478285
33.981341	1394.544147	17.483303
33.925129	1400.618737	17.488320
33.622402	1403.484407	17.493338
33.802090	1395.416313	17.498355
33.907846	1410.840060	17.503373
34.053641	1419.097154	17.508391
33.963174	1414.341566	17.513408
33.771412	1437.275971	17.518426
34.144918	1425.011207	17.523443
33.808325	1427.599448	17.528461
34.094851	1413.694476	17.533479
34.328816	1429.750455	17.538496
34.627051	1449.692111	17.543514
34.683170	1451.160391	17.548531
34.672084	1450.003698	17.553549
34.680249	1451.204759	17.558567
34.936664	1440.890490	17.563584
34.748359	1422.601965	17.568602
34.817800	1417.895780	17.573619
34.671385	1409.699207	17.578637
34.641096	1411.844816	17.583655
34.807066	1404.183708	17.588672
34.427930	1415.181898	17.593690
35.024060	1429.274594	17.598707
34.955188	1440.519257	17.603725
34.941214	1435.459225	17.608743
35.464002	1420.561070	17.613760
34.917171	1421.651230	17.618778
34.885754	1400.665872	17.623795
35.570624	1398.131347	17.628813
34.462084	1400.682930	17.633831
35.280851	1403.853524	17.638848
35.304946	1407.986879	17.643866
35.132083	1404.514633	17.648883
35.317649	1413.974524	17.653901
34.744291	1407.808693	17.658919
34.967746	1412.084106	17.663936
34.819489	1433.110155	17.668954
35.079144	1432.215935	17.673971
35.355001	1443.713137	17.678989
35.083149	1438.644786	17.684007
35.472759	1436.056969	17.689024
35.453243	1444.169117	17.694042
35.183675	1431.180940	17.699059
35.627222	1442.405396	17.704077
35.355645	1465.897975	17.709095
35.639864	1455.810564	17.714112
35.525012	1474.305993	17.719130
35.538845	1466.918953	17.724147
35.685226	1465.374285	17.729165
35.758085	1475.870635	17.734183
35.962488	1473.668703	17.739200
35.746082	1466.111668	17.744218
35.716932	1465.575282	17.749235
36.064872	1456.386702	17.754253
35.891006	1464.623724	17.759271
36.034499	1457.901339	17.764288
35.924119	1457.519394	17.769306
35.977570	1453.159153	17.774323
36.548903	1458.017686	17.779341
35.970197	1464.407483	17.784359
36.074883	1458.845058	17.789376
35.896632	1464.809252	17.794394
35.927827	1463.598287	17.799411
35.906619	1467.587224	17.804429
35.911702	1479.827075	17.809447
36.440001	1492.887037	17.814464
36.413624	1495.473334	17.819482
36.541148	1491.611781	17.824499
36.373735	1491.980634	17.829517
36.304064	1492.653705	17.834535
36.519505	1489.649564	17.839552
36.733451	1495.281269	17.844570
36.412219	1492.421442	17.849587
36.620325	1496.073068	17.854605
36.345994	1496.987237	17.859623
36.438481	1499.717160	17.864640
36.354653	1499.547724	17.869658
36.571448	1496.085495	17.874675
36.698118	1494.791733	17.879693
36.416780	1508.868535	17.884711
36.918470	1520.212514	17.889728
36.827185	1520.833274	17.894746
36.759479	1525.852370	17.899763
37.240891	1511.555873	17.904781
37.297711	1523.427720	17.909799
37.026162	1517.894736	17.914816
37.376376	1524.053002	17.919834
37.229025	1520.136343	17.924851
37.543329	1509.690756	17.929869
37.345413	1515.513360	17.934887
37.380408	1505.360255	17.939904
37.400269	1492.343213	17.944922
37.573096	1480.666075	17.949939
37.581585	1474.051552	17.954957
37.795283	1478.151444	17.959975
37.409343	1478.749918	17.964992
37.709326	1475.671888	17.970010
37.730565	1471.394553	17.975027
37.825891	1473.329140	17.980045
37.632663	1474.595565	17.985063
37.792120	1479.034779	17.990080
37.770219	1479.297952	17.995098
37.562862	1472.356322	18.000115
37.656111	1472.979087	18.005133
37.432890	1473.514296	18.010151
37.780110	1474.338150	18.015168
37.934052	1473.759915	18.020186
37.375488	1480.831391	18.025203
38.119187	1470.064075	18.030221
38.000439	1473.124370	18.035239
37.648647	1468.794865	18.040256
37.741210	1476.188421	18.045274
37.347833	1483.597393	18.050291
37.798330	1481.433690	18.055309
37.718675	1502.010253	18.060327
37.955021	1497.588500	18.065344
38.145342	1504.625279	18.070362
37.945086	1500.935129	18.075379
38.163918	1494.708854	18.080397
38.012096	1503.615837	18.085415
38.241264	1512.936656	18.090432
38.489617	1527.264405	18.095450
38.745420	1530.623080	18.100467
38.754240	1514.909494	18.105485
38.497583	1521.839079	18.110503
38.702484	1500.417862	18.115520
38.375240	1507.615073	18.120538
38.557213	1520.296017	18.125555
38.675613	1526.757373	18.130573
38.651990	1535.042687	18.135591
38.769148	1531.285207	18.140608
38.786793	1532.135101	18.145626
38.460154	1533.957550	18.150643
38.654258	1534.626151	18.155661
38.366162	1536.328023	18.160679
38.613749	1531.435112	18.165696
38.659490	1541.623422	18.170714
38.713256	1538.060724	18.175731
38.830754	1549.073314	18.180749
38.784555	1562.584323	18.185767
39.097670	1563.816991	18.190784
39.247907	1568.534922	18.195802
39.242191	1552.554035	18.200819
39.325935	1554.523234	18.205837
39.010240	1561.417375	18.210855
39.288839	1560.490867	18.215872
39.477422	1551.692883	18.220890
39.290957	1557.677375	18.225907
40.109251	1547.587357	18.230925
39.586317	1551.297114	18.235943
39.823436	1553.033346	18.240960
39.802000	1559.914405	18.245978
39.516694	1558.023376	18.250995
39.704798	1548.359351	18.256013
39.571466	1561.095883	18.261031
39.753051	1561.627987	18.266048
39.594838	1549.962905	18.271066
39.930674	1562.946256	18.276083
39.853324	1551.685440	18.281101
39.477996	1556.899372	18.286119
39.614549	1547.639576	18.291136
39.714948	1557.174732	18.296154
39.343049	1558.783845	18.301171
39.768974	1549.594454	18.306189
39.763919	1556.494836	18.311207
39.482452	1557.385390	18.316224
39.821565	1566.359629	18.321242
40.076727	1581.837453	18.326259
40.132382	1580.508637	18.331277
40.025704	1588.843610	18.336295
39.986088	1586.648756	18.341312
39.875315	1579.215839	18.346330
40.020484	1581.424433	18.351347
40.277556	1588.913926	18.356365
40.609602	1599.045241	18.361383
40.467465	1602.510227	18.366400
40.572807	1591.817825	18.371418
40.630352	1606.731681	18.376435
40.948061	1590.181262	18.381453
40.837506	1584.645117	18.386471
40.778879	1577.499197	18.391488
40.560827	1570.196709	18.396506
40.737535	1570.157195	18.401523
40.866892	1564.797714	18.406541
40.551286	1573.144570	18.411559
40.800115	1584.845578	18.416576
41.217702	1588.293515	18.421594
40.967115	1602.581035	18.426611
41.218889	1603.132970	18.431629
41.369739	1594.824688	18.436647
40.989832	1574.486374	18.441664
41.164138	1558.026357	18.446682
40.888862	1571.186874	18.451699
40.944085	1586.116056	18.456717
41.225492	1592.723179	18.461735
40.941098	1608.554087	18.466752
41.122664	1595.423076	18.471770
40.908023	1604.925191	18.476787
41.189462	1584.733239	18.481805
40.917218	1600.942427	18.486823
41.040440	1609.973439	18.491840
41.570693	1626.466197	18.496858
41.424758	1628.679874	18.501875
41.564835	1623.000093	18.506893
41.720584	1624.466004	18.511911
41.561907	1631.335653	18.516928
41.872666	1610.031335	18.521946
41.808585	1630.573197	18.526963
42.091293	1614.829342	18.531981
41.982181	1624.302513	18.536999
41.949446	1619.643957	18.542016
42.040235	1621.129325	18.547034
42.032173	1617.301694	18.552051
41.709148	1621.919563	18.557069
42.060724	1619.021903	18.562087
42.024625	1625.510947	18.567104
41.970577	1609.831729	18.572122
42.115549	1624.124783	18.577139
42.106079	1620.518246	18.582157
42.110568	1615.507448	18.587175
41.820168	1619.735256	18.592192
42.237889	1608.972420	18.597210
42.419329	1638.071749	18.602227
42.588464	1640.911791	18.607245
42.525741	1634.237777	18.612263
42.498766	1641.231208	18.617280
42.690859	1636.993933	18.622298
42.426863	1645.161779	18.627315
42.631457	1633.127678	18.632333
42.700024	1633.254954	18.637351
42.341250	1642.673176	18.642368
42.829955	1628.815903	18.647386
42.710733	1629.724377	18.652403
42.672909	1624.812339	18.657421
42.940266	1634.241449	18.662439
42.724776	1636.746211	18.667456
42.947583	1636.606910	18.672474
43.107186	1637.330462	18.677491
43.017368	1629.672388	18.682509
42.836300	1629.702573	18.687527
42.659725	1632.160710	18.692544
42.983863	1631.988427	18.697562
42.716364	1646.736269	18.702579
43.007465	1648.214725	18.707597
42.984801	1661.096329	18.712615
43.086082	1672.164063	18.717632
43.591576	1656.755967	18.722650
43.446422	1661.923016	18.727667
43.579014	1658.988912	18.732685
43.395376	1658.453785	18.737703
43.195162	1660.741055	18.742720
43.355245	1659.782665	18.747738
43.625699	1662.928307	18.752755
43.584538	1655.748739	18.757773
43.704675	1672.640806	18.762791
43.576620	1678.014070	18.767808
43.871386	1672.029826	18.772826
44.410339	1678.220170	18.777843
43.965997	1677.796482	18.782861
44.240492	1670.680190	18.787879
43.829544	1673.481219	18.792896
43.982224	1667.498151	18.797914
43.960539	1675.711172	18.802931
44.028747	1682.434081	18.807949
44.326367	1683.909489	18.812967
44.396429	1684.637689	18.817984
44.615756	1670.985385	18.823002
44.466561	1677.816078	18.828019
44.251274	1668.545003	18.833037
44.462445	1673.619369	18.838055
44.369112	1679.565988	18.843072
44.576074	1666.496443	18.848090
44.134861	1676.935852	18.853107
44.153544	1675.576559	18.858125
44.553426	1675.927506	18.863143
44.172093	1675.891765	18.868160
44.349836	1670.150983	18.873178
44.516495	1677.702003	18.878195
44.706692	1692.263584	18.883213
45.049224	1700.212150	18.888231
44.857405	1701.879534	18.893248
45.152938	1701.424607	18.898266
45.126288	1696.779583	18.903283
44.835912	1678.670709	18.908301
44.956869	1684.449039	18.913319
44.841194	1693.037922	18.918336
45.136451	1696.821960	18.923354
45.246192	1705.900937	18.928371
45.287949	1700.472899	18.933389
45.415570	1704.754480	18.938407
45.378103	1699.938420	18.943424
45.085023	1704.713933	18.948442
44.960940	1693.240312	18.953459
44.977637	1699.348176	18.958477
45.259581	1693.688097	18.963495
45.101327	1698.637259	18.968512
45.355697	1703.226903	18.973530
45.670775	1725.068453	18.978547
45.680785	1720.928741	18.983565
45.567809	1719.374399	18.988583
45.383687	1728.805377	18.993600
45.595979	1722.310811	18.998618
45.784992	1731.343951	19.003635
45.622147	1723.503087	19.008653
46.039074	1725.423232	19.013671
45.931264	1727.506966	19.018688
45.904293	1719.208094	19.023706
46.009797	1724.515784	19.028723
45.959588	1731.362726	19.033741
45.971441	1723.474323	19.038759
45.627439	1728.016576	19.043776
46.202614	1743.665783	19.048794
46.486300	1740.781747	19.053811
46.450639	1745.330238	19.058829
46.546010	1744.655824	19.063847
46.578692	1746.609125	19.068864
46.916338	1739.356323	19.073882
47.287884	1734.562431	19.078899
46.734035	1723.296828	19.083917
46.759776	1717.295468	19.088935
46.829382	1707.570725	19.093952
46.877447	1703.412094	19.098970
46.636139	1708.404590	19.103987
46.538747	1709.035034	19.109005
46.844291	1703.287960	19.114023
46.613765	1713.280570	19.119040
46.667056	1710.122631	19.124058
46.668822	1725.479331	19.129075
46.920397	1740.039024	19.134093
47.250038	1738.547336	19.139111
47.065871	1742.947281	19.144128
46.971849	1734.330415	19.149146
47.049439	1736.394360	19.154163
47.003696	1742.842930	19.159181
47.232517	1731.370075	19.164199
46.968112	1738.236478	19.169216
46.954843	1746.756403	19.174234
47.322650	1753.997260	19.179251
47.156215	1762.739892	19.184269
47.019146	1766.798949	19.189287
47.005889	1771.159473	19.194304
47.331962	1765.519593	19.199322
47.586463	1784.566203	19.204339
47.568364	1797.536924	19.209357
47.644849	1801.592780	19.214375
47.705360	1801.190298	19.219392
48.142905	1793.214967	19.224410
47.944653	1796.979872	19.229427
47.722540	1798.046006	19.234445
48.180251	1788.815760	19.239463
47.980555	1795.087972	19.244480
47.931313	1798.239140	19.249498
48.145147	1796.100556	19.254515
47.945070	1796.898856	19.259533
48.297475	1793.721896	19.264551
48.742086	1795.743746	19.269568
48.269155	1795.625197	19.274586
48.924859	1788.318724	19.279603
48.520549	1790.598201	19.284621
49.285242	1788.860187	19.289639
49.025269	1778.496875	19.294656
48.906510	1780.287162	19.299674
48.927968	1767.081830	19.304691
48.747708	1754.732074	19.309709
48.956461	1749.784133	19.314727
49.004353	1739.520071	19.319744
48.660278	1758.814558	19.324762
48.833673	1738.331312	19.329779
48.594970	1746.695793	19.334797
48.664524	1761.254262	19.339815
49.076678	1771.691665	19.344832
48.914111	1784.444263	19.349850
48.796037	1775.324681	19.354867
49.012496	1784.497385	19.359885
49.090348	1778.521986	19.364903
49.053595	1774.214835	19.369920
48.923988	1780.978539	19.374938
49.183927	1783.508636	19.379955
48.744503	1781.663666	19.384973
49.370853	1798.135912	19.389991
49.167459	1802.046160	19.395008
49.323576	1797.552225	19.400026
49.673174	1801.498123	19.405043
49.452870	1810.009578	19.410061
49.758505	1803.497102	19.415079
49.780018	1807.086509	19.420096
49.435956	1800.243042	19.425114
49.568751	1801.786013	19.430131
49.823620	1809.770072	19.435149
49.941608	1815.913115	19.440167
50.033409	1825.427032	19.445184
50.154457	1842.857320	19.450202
50.345009	1833.324601	19.455219
49.712172	1840.766060	19.460237
50.458983	1825.683043	19.465255
50.219041	1834.012738	19.470272
49.928676	1828.292612	19.475290
50.251855	1833.415737	19.480307
50.287318	1835.615043	19.485325
50.355193	1829.469630	19.490343
50.527015	1835.895072	19.495360
50.282587	1834.141308	19.500378
50.549178	1829.461680	19.505395
50.541477	1828.270144	19.510413
50.759425	1829.776524	19.515431
50.558339	1828.277761	19.520448
50.261109	1837.418155	19.525466
50.693967	1842.924629	19.530483
50.649841	1853.291465	19.535501
50.668006	1846.986198	19.540519
50.889340	1848.775481	19.545536
50.808480	1850.786248	19.550554
51.248646	1842.355734	19.555571
50.928813	1851.027455	19.560589
50.958768	1846.603292	19.565607
51.220112	1853.698506	19.570624
51.047469	1871.523306	19.575642
51.389819	1873.399565	19.580659
51.772419	1866.840807	19.585677
52.523149	1854.114981	19.590695
52.617499	1836.520324	19.595712
52.439590	1832.385042	19.600730
52.324657	1807.994131	19.605747
51.628639	1794.589913	19.610765
51.944032	1787.628974	19.615783
52.124113	1783.771606	19.620800
51.680617	1783.627693	19.625818
52.093582	1784.566621	19.630835
52.060392	1785.050572	19.635853
52.073536	1786.990984	19.640871
52.074022	1787.089419	19.645888
52.009097	1787.884941	19.650906
52.421637	1773.544140	19.655923
51.969991	1780.970811	19.660941
52.234148	1786.670655	19.665959
52.586444	1779.532723	19.670976
52.290416	1781.432393	19.675994
52.682778	1787.156206	19.681011
52.225180	1781.622945	19.686029
52.323146	1782.116593	19.691047
52.374492	1780.952254	19.696064
52.436711	1791.658853	19.701082
52.509545	1784.052802	19.706099
52.465444	1787.055476	19.711117
52.211876	1785.451660	19.716135
52.722839	1794.602194	19.721152
52.285872	1814.499587	19.726170
52.727156	1810.432265	19.731187
52.608425	1825.234292	19.736205
52.854189	1820.269153	19.741223
52.920473	1814.624795	19.746240
52.494145	1824.771673	19.751258
52.396687	1825.815516	19.756275
52.662965	1836.902402	19.761293
52.846704	1849.479387	19.766311
53.084963	1847.604059	19.771328
53.132457	1858.008821	19.776346
53.199725	1860.111112	19.781363
53.296537	1877.958853	19.786381
53.279431	1884.647604	19.791399
53.725840	1880.780988	19.796416
53.124410	1884.885757	19.801434
53.410846	1878.809117	19.806451
53.253960	1878.170324	19.811469
53.425003	1883.870326	19.816487
53.305218	1896.446220	19.821504
53.593637	1903.608610	19.826522
54.232910	1898.615841	19.831539
54.178135	1899.638422	19.836557
54.327421	1905.819213	19.841575
54.683634	1896.573883	19.846592
54.681370	1898.290886	19.851610
54.815750	1889.476129	19.856627
54.616212	1876.069245	19.861645
54.615184	1862.536860	19.866663
54.595804	1865.345284	19.871680
54.076724	1865.058813	19.876698
54.332840	1857.788405	19.881715
54.467078	1861.608695	19.886733
54.606553	1856.857666	19.891751
54.550134	1860.052165	19.896768
54.468040	1868.706823	19.901786
54.847311	1885.037158	19.906803
54.717947	1889.833155	19.911821
54.771715	1905.383359	19.916839
55.141884	1890.916815	19.921856
54.889191	1898.491184	19.926874
54.956184	1891.455736	19.931891
55.087541	1890.087934	19.936909
55.094741	1888.294311	19.941927
55.250564	1891.895273	19.946944
55.144169	1903.291783	19.951962
55.245258	1885.998706	19.956979
55.612397	1890.457459	19.961997
55.223344	1886.793475	19.967015
55.365405	1886.088067	19.972032
55.091680	1893.679314	19.977050
55.024601	1892.005910	19.982067
55.194143	1891.381367	19.987085
55.367861	1915.643925	19.992103
55.371072	1917.663957	19.997120
55.289898	1920.783842	20.002138
55.407590	1925.788788	20.007155
55.855667	1929.594730	20.012173
55.476802	1930.558185	20.017191
55.931871	1935.872811	20.022208
55.972184	1958.115477	20.027226
56.134681	1951.607044	20.032243
56.141371	1947.400500	20.037261
56.257402	1951.102184	20.042279
56.536247	1947.296865	20.047296
56.341466	1948.017914	20.052314
56.619647	1949.679257	20.057331
56.433944	1945.563350	20.062349
56.342312	1947.966473	20.067367
56.729424	1942.232527	20.072384
56.766954	1943.849219	20.077402
56.735513	1938.498225	20.082419
56.954139	1940.263559	20.087437
56.806695	1945.378326	20.092455
56.799751	1941.128774	20.097472
56.455534	1938.957723	20.102490
56.419634	1939.406695	20.107507
56.654014	1929.085135	20.112525
56.837793	1947.022833	20.117543
56.851007	1930.702975	20.122560
56.961930	1939.595279	20.127578
56.938972	1947.188576	20.132595
57.079215	1946.054726	20.137613
57.111065	1952.455842	20.142631
57.221841	1947.239475	20.147648
57.078904	1955.081457	20.152666
57.105074	1953.846093	20.157683
57.162415	1966.531582	20.162701
57.177296	1976.350110	20.167719
57.520992	1980.663966	20.172736
57.490600	1989.010884	20.177754
57.658798	1980.872349	20.182771
57.859189	1979.375349	20.187789
57.747306	1993.987814	20.192807
57.991256	1980.635085	20.197824
58.030296	1998.118942	20.202842
57.961526	2002.508049	20.207859
58.274059	2011.045625	20.212877
58.088088	2010.199060	20.217895
58.123850	2013.221181	20.222912
57.800537	2013.132880	20.227930
58.318311	1999.569270	20.232947
58.605187	2009.718994	20.237965
58.449421	2005.464630	20.242983
58.527611	2010.766722	20.248000
58.359631	2004.955323	20.253018
58.685942	2004.084248	20.258035
58.854859	2005.369266	20.263053
58.410629	2019.366907	20.268071
58.586557	2002.703787	20.273088
58.663930	2030.901460	20.278106
58.383775	2029.437078	20.283123
58.970977	2038.714458	20.288141
58.542310	2045.693729	20.293159
58.883131	2040.036339	20.298176
59.249806	2034.699854	20.303194
58.921429	2039.415585	20.308211
59.390730	2049.615331	20.313229
59.256339	2065.844611	20.318247
59.274573	2063.894015	20.323264
59.696023	2059.330315	20.328282
59.372348	2062.970458	20.333299
59.841369	2067.545796	20.338317
59.779333	2057.271448	20.343335
59.562322	2062.686007	20.348352
59.207362	2053.851697	20.353370
59.476988	2065.615363	20.358387
59.895935	2053.378775	20.363405
59.621546	2065.469472	20.368423
59.659293	2053.063954	20.373440
59.783251	2067.052640	20.378458
59.623028	2059.995429	20.383475
59.820212	2082.151176	20.388493
59.864703	2098.064930	20.393511
59.998462	2088.922601	20.398528
60.160146	2083.333551	20.403546
60.032203	2088.200239	20.408563
60.574655	2087.258197	20.413581
60.456059	2110.448368	20.418599
60.768392	2105.282704	20.423616
60.936987	2104.509884	20.428634
60.837046	2105.804555	20.433651
60.838951	2087.510008	20.438669
60.778539	2088.150463	20.443687
61.070081	2095.376991	20.448704
60.863595	2094.079101	20.453722
60.852140	2105.262733	20.458739
61.435708	2100.632314	20.463757
61.170640	2107.513555	20.468775
61.051999	2105.291210	20.473792
61.167268	2110.151341	20.478810
61.141731	2114.008091	20.483827
61.364486	2099.015060	20.488845
61.305018	2105.551103	20.493863
61.152859	2106.657993	20.498880
61.123993	2107.914474	20.503898
61.290795	2112.725884	20.508915
61.397562	2132.378586	20.513933
61.113966	2138.031800	20.518951
61.527260	2137.870681	20.523968
61.915915	2148.289017	20.528986
61.604495	2140.043100	20.534003
61.808284	2138.499457	20.539021
61.981087	2146.004803	20.544039
62.220854	2156.833722	20.549056
62.468422	2157.755676	20.554074
62.198617	2164.805843	20.559091
63.351538	2135.496537	20.564109
63.455691	2118.982231	20.569127
63.320524	2108.354249	20.574144
63.265720	2102.725974	20.579162
63.072259	2086.784400	20.584179
63.139963	2071.668738	20.589197
63.091256	2067.632787	20.594215
62.879804	2065.893200	20.599232
62.954234	2052.370943	20.604250
62.885975	2073.182199	20.609267
63.089336	2059.230630	20.614285
62.835002	2069.592783	20.619303
62.794527	2068.689356	20.624320
62.938385	2059.537491	20.629338
62.819894	2065.686079	20.634355
62.912880	2067.045928	20.639373
63.092053	2080.507334	20.644391
63.497805	2100.697714	20.649408
63.611405	2096.623363	20.654426
63.270144	2101.417632	20.659443
63.612321	2102.638430	20.664461
63.466544	2098.213481	20.669479
63.548429	2102.379544	20.674496
63.349479	2101.760330	20.679514
63.204660	2107.986145	20.684531
63.203785	2100.273290	20.689549
63.761307	2110.275736	20.694567
63.596194	2114.125367	20.699584
63.868113	2123.382364	20.704602
63.618029	2133.353296	20.709619
63.735998	2127.119124	20.714637
63.554852	2131.374186	20.719655
63.344207	2144.971302	20.724672
63.583388	2151.915217	20.729690
63.903814	2166.345363	20.734707
64.373907	2172.500503	20.739725
64.479746	2188.148638	20.744743
64.246714	2189.481183	20.749760
64.551573	2183.228920	20.754778
64.695087	2192.436038	20.759795
64.727476	2191.652779	20.764813
64.706774	2182.449057	20.769831
64.918563	2188.538470	20.774848
65.153919	2185.355294	20.779866
64.982177	2192.558470	20.784883
65.346239	2187.060553	20.789901
65.339446	2193.411104	20.794919
64.843608	2184.930847	20.799936
65.312988	2193.125127	20.804954
65.247707	2215.156573	20.809971
65.149241	2218.989642	20.814989
65.523824	2217.936120	20.820007
65.475300	2214.258375	20.825024
65.820945	2212.778552	20.830042
65.462466	2226.455821	20.835059
65.675776	2217.500594	20.840077
65.624282	2219.915985	20.845095
65.573640	2220.084733	20.850112
65.605468	2210.916359	20.855130
65.667327	2231.411706	20.860147
65.646296	2244.364390	20.865165
65.829989	2233.783331	20.870183
65.330418	2237.009037	20.875200
65.917071	2247.793361	20.880218
66.363114	2257.590016	20.885235
67.374731	2246.855994	20.890253
67.420789	2254.348992	20.895271
66.958753	2235.731762	20.900288
67.200655	2229.959639	20.905306
67.249398	2216.503321	20.910323
67.392763	2218.613093	20.915341
67.519677	2211.252182	20.920359
67.300070	2204.021306	20.925376
67.194828	2192.638279	20.930394
66.798134	2193.504315	20.935411
66.891225	2185.472252	20.940429
67.121676	2199.599267	20.945447
67.269151	2210.770342	20.950464
67.471800	2207.461492	20.955482
67.507194	2210.726238	20.960499
67.417650	2219.511860	20.965517
67.530118	2208.557214	20.970535
67.642235	2224.570885	20.975552
67.716821	2208.905116	20.980570
67.315325	2219.272928	20.985587
67.506694	2216.173830	20.990605
67.470906	2212.946734	20.995623
67.485906	2223.542185	21.000640
67.310331	2225.720319	21.005658
67.543402	2239.062273	21.010675
67.792622	2244.819103	21.015693
67.972723	2252.422896	21.020711
67.881732	2253.528686	21.025728
67.991329	2249.790007	21.030746
68.056554	2258.818439	21.035763
68.196544	2275.599595	21.040781
68.353593	2280.546933	21.045799
67.949659	2279.637756	21.050816
68.632334	2281.906336	21.055834
68.305924	2284.569401	21.060851
68.738360	2286.644526	21.065869
68.584239	2276.380612	21.070887
68.370179	2291.958393	21.075904
68.816000	2304.013832	21.080922
69.234963	2305.482915	21.085939
69.004852	2312.891522	21.090957
69.462921	2311.805615	21.095975
69.108487	2317.111207	21.100992
69.312584	2309.701200	21.106010
68.963732	2308.142692	21.111027
69.242043	2305.180312	21.116045
69.262337	2304.886866	21.121063
69.218022	2313.303990	21.126080
69.766600	2317.141361	21.131098
69.540621	2317.013650	21.136115
69.606511	2331.723268	21.141133
69.705776	2331.538354	21.146151
69.530469	2330.439597	21.151168
69.824829	2328.006450	21.156186
70.005220	2318.930647	21.161203
70.052657	2317.962987	21.166221
70.050271	2326.236139	21.171239
70.258948	2340.553520	21.176256
70.736952	2345.897551	21.181274
70.173196	2351.752526	21.186291
70.180743	2354.848696	21.191309
70.768980	2344.147572	21.196327
70.458615	2349.247814	21.201344
71.029347	2340.864234	21.206362
70.862287	2343.512636	21.211379
70.723425	2338.474640	21.216397
70.688477	2339.388046	21.221415
70.857484	2341.509716	21.226432
70.736694	2344.444138	21.231450
70.892609	2346.974295	21.236467
70.622657	2359.640089	21.241485
71.329395	2355.408037	21.246503
71.397010	2375.787260	21.251520
71.547705	2365.841143	21.256538
71.317973	2370.121668	21.261555
71.198183	2366.762433	21.266573
71.483246	2363.130002	21.271591
71.436548	2365.920615	21.276608
71.185516	2381.771566	21.281626
71.462966	2388.081649	21.286643
71.831639	2399.506657	21.291661
72.072465	2390.918029	21.296679
71.501105	2394.909264	21.301696
71.864514	2399.659347	21.306714
71.970254	2395.398817	21.311731
72.276517	2416.025055	21.316749
72.586702	2409.687169	21.321767
72.531691	2414.880431	21.326784
72.486087	2407.731175	21.331802
72.822406	2411.485338	21.336819
73.203595	2408.092835	21.341837
72.747881	2386.243166	21.346855
72.607852	2376.599697	21.351872
72.961785	2365.452050	21.356890
73.002051	2371.210976	21.361907
72.689585	2378.532510	21.366925
73.109493	2380.177828	21.371943
72.687276	2394.530031	21.376960
73.169276	2396.696150	21.381978
73.228008	2402.187443	21.386995
73.112418	2401.381916	21.392013
73.179704	2400.920023	21.397031
73.195306	2401.048628	21.402048
73.087247	2396.476375	21.407066
73.320334	2414.585165	21.412083
73.314064	2427.467436	21.417101
73.465861	2435.285873	21.422119
73.559036	2431.590432	21.427136
73.486874	2435.056965	21.432154
73.582502	2437.202262	21.437171
73.869156	2467.158133	21.442189
73.971442	2449.658712	21.447207
73.962373	2456.589689	21.452224
74.105023	2454.696322	21.457242
74.424932	2461.979334	21.462259
74.213373	2467.384858	21.467277
74.366302	2460.111635	21.472295
74.172762	2470.704904	21.477312
74.830527	2481.451589	21.482330
74.825748	2479.016164	21.487347
74.683871	2495.740462	21.492365
74.816572	2495.226355	21.497383
74.719101	2493.720146	21.502400
75.095714	2483.253712	21.507418
75.286260	2478.547947	21.512435
75.084063	2487.923329	21.517453
75.489287	2479.338040	21.522471
75.509857	2489.776836	21.527488
75.312314	2486.686412	21.532506
75.464773	2479.488458	21.537523
75.252251	2492.085757	21.542541
75.498069	2483.265925	21.547559
75.071601	2492.901426	21.552576
75.779843	2508.714738	21.557594
75.819352	2513.710821	21.562611
75.803870	2507.424658	21.567629
75.968582	2506.824912	21.572647
76.099018	2511.655877	21.577664
76.129594	2517.445209	21.582682
76.119712	2513.822391	21.587699
75.826259	2514.624038	21.592717
76.357734	2526.252408	21.597735
76.352876	2538.269934	21.602752
76.093803	2541.129339	21.607770
76.525550	2535.679898	21.612787
76.461837	2545.137422	21.617805
76.675465	2535.083489	21.622823
76.922683	2542.301846	21.627840
76.745223	2530.439608	21.632858
76.662157	2550.744100	21.637875
76.952197	2558.378593	21.642893
77.154015	2561.442518	21.647911
77.054023	2568.214633	21.652928
77.076509	2577.980700	21.657946
77.255235	2563.157540	21.662963
77.298067	2558.978684	21.667981
77.349510	2555.766941	21.672999
77.308157	2561.923377	21.678016
77.298050	2574.886726	21.683034
77.456376	2587.787840	21.688051
77.670723	2592.255656	21.693069
77.962036	2586.496452	21.698087
77.741739	2592.394044	21.703104
77.667811	2600.127631	21.708122
77.505750	2595.827692	21.713139
77.615668	2605.628853	21.718157
78.094564	2604.238666	21.723175
78.282358	2610.078679	21.728192
78.199889	2612.278796	21.733210
78.795158	2608.166390	21.738227
78.720645	2611.051830	21.743245
78.860988	2614.252760	21.748263
79.032822	2606.051482	21.753280
78.638301	2601.033841	21.758298
78.964805	2606.618112	21.763315
78.641528	2593.354799	21.768333
78.583043	2605.082063	21.773351
78.658439	2619.091523	21.778368
78.693240	2628.355945	21.783386
79.041515	2630.259270	21.788403
79.030954	2629.894171	21.793421
78.927952	2629.757830	21.798439
79.385731	2664.829191	21.803456
79.284377	2673.342608	21.808474
79.841230	2664.055213	21.813491
79.879878	2666.534830	21.818509
79.997805	2669.617838	21.823527
79.873906	2674.068661	21.828544
79.916413	2666.878657	21.833562
80.099413	2662.146924	21.838579
79.974537	2665.210437	21.843597
80.211574	2665.245942	21.848615
80.310660	2674.898546	21.853632
80.328542	2694.507280	21.858650
80.490971	2684.314509	21.863667
80.205121	2697.793102	21.868685
80.460561	2683.006295	21.873703
80.831760	2691.590406	21.878720
80.771995	2691.560271	21.883738
80.588455	2686.354381	21.888755
80.850220	2690.333613	21.893773
81.170215	2686.994924	21.898791
81.096909	2699.516101	21.903808
81.178312	2706.656182	21.908826
81.385770	2702.775928	21.913843
81.351860	2707.209442	21.918861
81.267422	2710.478460	21.923879
81.173117	2701.939846	21.928896
81.183484	2709.365763	21.933914
81.609160	2696.888567	21.938931
81.507475	2706.859218	21.943949
81.758471	2722.061303	21.948967
82.193650	2724.493140	21.953984
82.137838	2726.754988	21.959002
82.193076	2724.165448	21.964019
81.889936	2728.161010	21.969037
82.456501	2728.380739	21.974055
82.866318	2721.780881	21.979072
82.672333	2716.789720	21.984090
82.615164	2723.973705	21.989107
82.547948	2721.533263	21.994125
82.714839	2725.925537	21.999143
82.985933	2719.916481	22.004160
82.909361	2725.280367	22.009178
83.187187	2719.265862	22.014195
82.861818	2722.217423	22.019213
82.873611	2718.563395	22.024231
83.047513	2717.428228	22.029248
82.877487	2719.456288	22.034266
83.050505	2722.528575	22.039283
83.244940	2734.560379	22.044301
83.483519	2752.972604	22.049319
83.184023	2748.575377	22.054336
82.873232	2755.242047	22.059354
83.288044	2752.543923	22.064371
83.199277	2767.466280	22.069389
83.657776	2782.670949	22.074407
83.653573	2777.450973	22.079424
83.842854	2786.781160	22.084442
84.078732	2778.070300	22.089459
84.018448	2781.372722	22.094477
84.069665	2785.514536	22.099495
84.396939	2807.468587	22.104512
84.357151	2809.339572	22.109530
84.586462	2799.748245	22.114547
84.633271	2806.747262	22.119565
84.656385	2794.541234	22.124583
84.811214	2798.098477	22.129600
84.778533	2806.083594	22.134618
84.636566	2802.546050	22.139635
85.185922	2795.087884	22.144653
84.829906	2807.519116	22.149671
85.444465	2817.856265	22.154688
85.440063	2827.907682	22.159706
85.782137	2815.020245	22.164723
85.478812	2824.701629	22.169741
85.544462	2826.406266	22.174759
85.665746	2823.771873	22.179776
85.694384	2824.538511	22.184794
85.775905	2828.954057	22.189811
85.877450	2816.729859	22.194829
85.678651	2822.530652	22.199847
85.777758	2822.917446	22.204864
85.560668	2837.638349	22.209882
85.956522	2845.199490	22.214899
85.960850	2847.758860	22.219917
86.068694	2863.895954	22.224935
86.549785	2862.720749	22.229952
86.167411	2875.583607	22.234970
86.542040	2880.265830	22.239987
86.995960	2883.947413	22.245005
87.070121	2890.915936	22.250023
87.133003	2879.296971	22.255040
87.207715	2879.378352	22.260058
87.206603	2880.303884	22.265075
87.228880	2867.772720	22.270093
87.124682	2880.590533	22.275111
87.351080	2873.189153	22.280128
87.459673	2874.813426	22.285146
87.213559	2887.955636	22.290163
87.651896	2897.411438	22.295181
87.621009	2907.455496	22.300199
87.612425	2898.361154	22.305216
87.880864	2894.793574	22.310234
87.767859	2903.116521	22.315251
87.678892	2895.722656	22.320269
87.792379	2917.326934	22.325287
88.360879	2924.200717	22.330304
88.312629	2928.698099	22.335322
88.540478	2928.019731	22.340339
88.673054	2938.542975	22.345357
88.762148	2925.434875	22.350375
88.932179	2916.795910	22.355392
89.054871	2927.323152	22.360410
88.945771	2921.443744	22.365427
89.362663	2919.758305	22.370445
88.837341	2920.800487	22.375463
89.136893	2916.603281	22.380480
89.113068	2916.267546	22.385498
89.172534	2919.062268	22.390515
89.281502	2919.483255	22.395533
88.900087	2908.586574	22.400551
89.312909	2919.438059	22.405568
89.652356	2945.900420	22.410586
89.667821	2945.602646	22.415603
89.777887	2954.554340	22.420621
89.299380	2948.053591	22.425639
89.484295	2950.312081	22.430656
89.572709	2966.585591	22.435674
89.959404	2981.667341	22.440691
90.183140	2981.171556	22.445709
89.916913	2985.281529	22.450727
89.974633	2981.484757	22.455744
90.178837	2996.249188	22.460762
90.379053	3001.445900	22.465779
90.588538	3004.704323	22.470797
90.543125	3011.591978	22.475815
90.879625	3009.076523	22.480832
90.805794	3005.185852	22.485850
90.919001	3027.538413	22.490867
91.021097	3031.365122	22.495885
91.073927	3040.075178	22.500903
91.222958	3034.587112	22.505920
91.200914	3035.693704	22.510938
91.250630	3031.919118	22.515955
91.802720	3034.368586	22.520973
91.909394	3055.788348	22.525991
92.426491	3051.371868	22.531008
92.096520	3035.466181	22.536026
91.668132	3028.516485	22.541043
92.273593	3045.030550	22.546061
92.286533	3055.247747	22.551079
92.574846	3049.294764	22.556096
92.632188	3055.628707	22.561114
92.269410	3053.433410	22.566131
92.755709	3045.668654	22.571149
92.680147	3046.948325	22.576167
92.589235	3043.134504	22.581184
92.833038	3048.236582	22.586202
92.628348	3050.209022	22.591219
92.750268	3047.892620	22.596237
92.797918	3066.045587	22.601255
93.383438	3064.041536	22.606272
93.989389	3050.515126	22.611290
93.812282	3054.654403	22.616307
94.069171	3047.258898	22.621325
93.866944	3051.230289	22.626343
93.987658	3029.718986	22.631360
93.592013	3018.066663	22.636378
93.775286	3045.437495	22.641395
93.999451	3049.396690	22.646413
94.000334	3053.034304	22.651431
93.995242	3054.575907	22.656448
94.350334	3050.341481	22.661466
94.174205	3049.493614	22.666483
94.291055	3051.038574	22.671501
94.227572	3053.766346	22.676519
94.310694	3046.843453	22.681536
94.468774	3081.804921	22.686554
94.398463	3084.683844	22.691571
94.207929	3080.177462	22.696589
94.555820	3076.978556	22.701607
94.845380	3101.315453	22.706624
94.814378	3114.081526	22.711642
95.222716	3124.422837	22.716659
95.344235	3112.204537	22.721677
94.814074	3113.223911	22.726695
95.228616	3108.112593	22.731712
95.329519	3116.936366	22.736730
95.137403	3132.983814	22.741747
95.655529	3127.022533	22.746765
95.719642	3136.160723	22.751783
95.702227	3132.480740	22.756800
96.110809	3148.189380	22.761818
96.195142	3155.998918	22.766835
96.083451	3157.861814	22.771853
96.165668	3162.187963	22.776871
96.599521	3156.811194	22.781888
96.735169	3159.503922	22.786906
96.678041	3163.750070	22.791923
96.849505	3158.368084	22.796941
96.679181	3159.233163	22.801959
96.691676	3158.975252	22.806976
96.985747	3173.935170	22.811994
97.089575	3183.745583	22.817011
97.373891	3172.073063	22.822029
97.248535	3182.534212	22.827047
97.340867	3181.091283	22.832064
97.493369	3186.281419	22.837082
97.166498	3185.734603	22.842099
97.613276	3186.262857	22.847117
97.464887	3202.951589	22.852135
97.748179	3208.441284	22.857152
97.932994	3210.865591	22.862170
98.095304	3203.744020	22.867187
97.985094	3210.051143	22.872205
98.196463	3215.566968	22.877223
98.090194	3228.007819	22.882240
98.112776	3231.263490	22.887258
98.593841	3247.064523	22.892275
98.604342	3236.129253	22.897293
98.596532	3242.744990	22.902311
98.984118	3258.419825	22.907328
99.401962	3260.108897	22.912346
99.289233	3263.540225	22.917363
99.767500	3259.056120	22.922381
99.713019	3249.098259	22.927399
99.498400	3236.155737	22.932416
99.519327	3237.139837	22.937434
99.444534	3252.860010	22.942451
100.047189	3252.006339	22.947469
99.444345	3256.090032	22.952487
99.528624	3260.160725	22.957504
99.833082	3253.338371	22.962522
99.923257	3256.122144	22.967539
99.924863	3264.717600	22.972557
99.771703	3279.393251	22.977575
99.916152	3281.496690	22.982592
100.290116	3276.084161	22.987610
99.951335	3302.174759	22.992627
100.262263	3295.106014	22.997645
100.459581	3311.722054	23.002663
100.445681	3312.591070	23.007680
100.631829	3335.300882	23.012698
100.557580	3347.009668	23.017715
101.221565	3337.023698	23.022733
100.909187	3345.087466	23.027751
101.156540	3356.617210	23.032768
101.788903	3354.405715	23.037786
101.430582	3371.870135	23.042803
101.727735	3367.518077	23.047821
102.042545	3365.086887	23.052839
102.011189	3360.546882	23.057856
102.074368	3347.529751	23.062874
102.080075	3361.062438	23.067891
102.613516	3350.406752	23.072909
102.655705	3356.449214	23.077927
102.420768	3358.675955	23.082944
102.624367	3353.355104	23.087962
102.369804	3364.291431	23.092979
102.450845	3354.794885	23.097997
102.612039	3362.114150	23.103015
102.395698	3358.783738	23.108032
102.767088	3372.251332	23.113050
102.432883	3386.941815	23.118067
102.856733	3381.135096	23.123085
103.123658	3403.792210	23.128103
103.034485	3417.723822	23.133120
103.382638	3417.340826	23.138138
103.453202	3423.718002	23.143155
103.618421	3417.932202	23.148173
103.894768	3416.438196	23.153191
103.710371	3434.792375	23.158208
103.955348	3438.459206	23.163226
103.956861	3444.648633	23.168243
104.399866	3450.603260	23.173261
104.200115	3443.478358	23.178279
104.004939	3452.359006	23.183296
104.093047	3449.357545	23.188314
104.333269	3469.787475	23.193331
104.876936	3467.223345	23.198349
105.109709	3471.861207	23.203367
105.054996	3477.225262	23.208384
105.050557	3463.440847	23.213402
104.855548	3469.836977	23.218419
104.862201	3471.740879	23.223437
105.026017	3493.251362	23.228455
105.236435	3488.433714	23.233472
105.601632	3491.224586	23.238490
105.618900	3488.834163	23.243507
105.662360	3503.465930	23.248525
105.698763	3516.364845	23.253543
106.012593	3518.932739	23.258560
106.094928	3517.035488	23.263578
106.165929	3524.025687	23.268595
106.322628	3523.506379	23.273613
106.437252	3522.066802	23.278631
106.141204	3540.098679	23.283648
106.485989	3539.095310	23.288666
106.835165	3553.101453	23.293683
106.831454	3544.267371	23.298701
106.802668	3545.708618	23.303719
106.688928	3546.842296	23.308736
107.133205	3562.988777	23.313754
106.871586	3574.729659	23.318771
107.044763	3572.820061	23.323789
107.253792	3580.944558	23.328807
107.192789	3596.792326	23.333824
107.441783	3602.344167	23.338842
107.447031	3601.599211	23.343859
107.657381	3608.359968	23.348877
108.317351	3616.924562	23.353895
108.082605	3630.000142	23.358912
108.292063	3622.820147	23.363930
108.392360	3626.522485	23.368947
108.461251	3637.031192	23.373965
108.984432	3629.526980	23.378983
108.257319	3631.332346	23.384000
108.324011	3623.509467	23.389018
108.406678	3630.348546	23.394035
108.819035	3649.306244	23.399053
108.887975	3652.731485	23.404071
109.000852	3660.631425	23.409088
109.177468	3647.460926	23.414106
109.121470	3655.724792	23.419123
109.429648	3662.406317	23.424141
109.719681	3671.095811	23.429159
109.793162	3668.596008	23.434176
110.299768	3665.823022	23.439194
110.309253	3668.853377	23.444211
110.270410	3670.239607	23.449229
110.702490	3674.932607	23.454247
110.505800	3665.386741	23.459264
110.752707	3661.047284	23.464282
110.437036	3662.286190	23.469299
110.506203	3673.971386	23.474317
110.964433	3666.442120	23.479335
110.533534	3678.514001	23.484352
110.398629	3669.976878	23.489370
110.537519	3691.986715	23.494387
110.425709	3692.422758	23.499405
111.063343	3705.535730	23.504423
110.636488	3727.727440	23.509440
110.778332	3732.837632	23.514458
111.177764	3748.130633	23.519475
111.231947	3765.952579	23.524493
112.065361	3744.635671	23.529511
111.805877	3746.441298	23.534528
112.107583	3745.732511	23.539546
112.374127	3740.636137	23.544563
112.066405	3740.977165	23.549581
112.354733	3759.583518	23.554599
112.710038	3777.387330	23.559616
113.065515	3771.990698	23.564634
112.900429	3768.717042	23.569651
112.819384	3771.600630	23.574669
113.369211	3766.117759	23.579687
113.250248	3765.919091	23.584704
113.595863	3771.962476	23.589722
113.502524	3768.304411	23.594739
113.036306	3766.336461	23.599757
113.297736	3764.530692	23.604775
113.701028	3790.233000	23.609792
113.787031	3797.437785	23.614810
113.837575	3799.747869	23.619827
113.521284	3800.961688	23.624845
113.960479	3796.479989	23.629863
113.858224	3823.215300	23.634880
114.048169	3817.256325	23.639898
114.322261	3827.808234	23.644915
114.127092	3822.006183	23.649933
114.392145	3834.783888	23.654951
114.307512	3852.022627	23.659968
115.067548	3850.151313	23.664986
115.040140	3853.963521	23.670003
114.839570	3854.112707	23.675021
115.380804	3866.756735	23.680039
115.515409	3864.681050	23.685056
115.687768	3876.450049	23.690074
115.285980	3875.936129	23.695091
115.414721	3877.010240	23.700109
115.853576	3877.511489	23.705127
115.771718	3874.616155	23.710144
116.131800	3889.333084	23.715162
116.257124	3889.532849	23.720179
116.269601	3896.312834	23.725197
116.643745	3895.461672	23.730215
116.410055	3897.043710	23.735232
116.867080	3896.782001	23.740250
116.889327	3889.078594	23.745267
116.868409	3898.667637	23.750285
116.957139	3895.689612	23.755303
116.886566	3898.315940	23.760320
116.674907	3899.332433	23.765338
117.091581	3912.736663	23.770355
116.765556	3922.955633	23.775373
117.356144	3916.586296	23.780391
117.035749	3937.389567	23.785408
117.335830	3954.450692	23.790426
117.583809	3951.689137	23.795443
117.657073	3960.355754	23.800461
117.766306	3974.423808	23.805479
117.880527	3990.809073	23.810496
117.815235	3992.760038	23.815514
118.255083	3995.271239	23.820531
118.289849	4011.611847	23.825549
118.523047	4018.503257	23.830567
118.862368	4023.586633	23.835584
118.872471	4021.221732	23.840602
119.075406	4020.758514	23.845619
118.905336	4040.002479	23.850637
119.466539	4042.164735	23.855655
119.480706	4052.120533	23.860672
119.159578	4048.221479	23.865690
119.440884	4044.034096	23.870707
119.226459	4064.528546	23.875725
119.447779	4059.150962	23.880743
119.721965	4074.354059	23.885760
119.645238	4078.654900	23.890778
120.323890	4100.405116	23.895795
120.263684	4115.676423	23.900813
120.774750	4101.096230	23.905831
120.663970	4103.147301	23.910848
120.781149	4092.433108	23.915866
120.929351	4093.340198	23.920883
120.829484	4119.955916	23.925901
121.582808	4125.113459	23.930919
121.701124	4127.652521	23.935936
121.704900	4117.032365	23.940954
121.401907	4120.058428	23.945971
121.502537	4128.046872	23.950989
121.439152	4120.734802	23.956007
121.566808	4120.910558	23.961024
121.827469	4134.627954	23.966042
122.732160	4142.079185	23.971059
122.515148	4142.911911	23.976077
122.563808	4152.221003	23.981095
122.526498	4142.677891	23.986112
122.292081	4147.896816	23.991130
122.617916	4137.103818	23.996147
122.485547	4145.418434	24.001165
122.781698	4156.342150	24.006183
123.242372	4173.200029	24.011200
123.143389	4177.447107	24.016218
123.040232	4166.988409	24.021235
123.246025	4176.223759	24.026253
123.212619	4185.616598	24.031271
123.226039	4201.484504	24.036288
123.358979	4204.489721	24.041306
123.762885	4206.360772	24.046323
123.738050	4229.530630	24.051341
123.999710	4232.816868	24.056359
124.334655	4244.229155	24.061376
124.106171	4235.358797	24.066394
124.462321	4236.626673	24.071411
124.275459	4245.619789	24.076429
124.197379	4263.437112	24.081447
124.743106	4269.959325	24.086464
124.292370	4271.886570	24.091482
124.638950	4269.813800	24.096499
124.767939	4286.134311	24.101517
125.728480	4282.592374	24.106535
125.801934	4279.507350	24.111552
125.750613	4281.314669	24.116570
126.061139	4284.805429	24.121587
126.027233	4281.572866	24.126605
126.086946	4282.740380	24.131623
126.256960	4297.442028	24.136640
126.505776	4301.078501	24.141658
126.670947	4300.178570	24.146675
126.640013	4309.967196	24.151693
126.736412	4300.156061	24.156711
127.091452	4292.918886	24.161728
126.658339	4306.370959	24.166746
127.040705	4297.876292	24.171763
126.825557	4310.213241	24.176781
127.134123	4317.632499	24.181799
127.161940	4328.894281	24.186816
126.928055	4328.517427	24.191834
127.249123	4329.102057	24.196851
127.150535	4349.634331	24.201869
127.588299	4349.605776	24.206887
127.624136	4362.735046	24.211904
127.828017	4391.443604	24.216922
127.974163	4385.596435	24.221939
127.944765	4393.376666	24.226957
128.260950	4398.495905	24.231975
128.651124	4423.739945	24.236992
128.661876	4418.798871	24.242010
128.809388	4417.574256	24.247027
128.870782	4423.205999	24.252045
129.244499	4434.515116	24.257063
129.731761	4445.528162	24.262080
129.431856	4443.215502	24.267098
129.788727	4439.586418	24.272115
129.801196	4440.645239	24.277133
129.688261	4442.447853	24.282151
129.979952	4451.546630	24.287168
129.911336	4464.580726	24.292186
130.140878	4471.619425	24.297203
129.736737	4470.157291	24.302221
130.246978	4493.830843	24.307239
130.627778	4498.554275	24.312256
130.658516	4496.468598	24.317274
130.919324	4488.636656	24.322291
130.980261	4489.545671	24.327309
131.183471	4510.356402	24.332327
131.387931	4511.111625	24.337344
131.340183	4524.389588	24.342362
131.646949	4511.607437	24.347379
131.724912	4523.361109	24.352397
131.843662	4515.377141	24.357415
131.803471	4510.194856	24.362432
131.796745	4531.416943	24.367450
131.981610	4555.489599	24.372467
132.102172	4557.824386	24.377485
131.991481	4557.816096	24.382503
132.517542	4573.143992	24.387520
132.471398	4578.893679	24.392538
132.422161	4576.901610	24.397555
132.529079	4588.437884	24.402573
132.977443	4593.401341	24.407591
132.868806	4601.432678	24.412608
133.521038	4613.908450	24.417626
133.464627	4611.635630	24.422643
133.285102	4623.835385	24.427661
133.087225	4625.604883	24.432679
133.632705	4625.854544	24.437696
133.816258	4638.535014	24.442714
133.691473	4645.542893	24.447731
133.621670	4657.504717	24.452749
133.689804	4669.814560	24.457767
134.329476	4681.252919	24.462784
134.470675	4709.356617	24.467802
134.625210	4704.509691	24.472819
134.767662	4698.215696	24.477837
134.652116	4709.703973	24.482855
135.278246	4719.997949	24.487872
135.125110	4735.864933	24.492890
135.405387	4728.497439	24.497907
135.538239	4731.969786	24.502925
135.521011	4748.392256	24.507943
135.738888	4746.351051	24.512960
135.817913	4752.995916	24.517978
136.358149	4762.477271	24.522995
136.637310	4766.045019	24.528013
136.347137	4775.097345	24.533031
136.681550	4767.279810	24.538048
136.762758	4771.253752	24.543066
136.938551	4772.438239	24.548083
137.469020	4771.551607	24.553101
137.272875	4770.053304	24.558119
137.324919	4760.222476	24.563136
137.430211	4783.467607	24.568154
137.845073	4789.184076	24.573171
137.922056	4797.331151	24.578189
138.207239	4788.909863	24.583207
138.440890	4796.112623	24.588224
138.180571	4794.978590	24.593242
138.405509	4793.077966	24.598259
138.377148	4789.407288	24.603277
138.320249	4795.834556	24.608295
138.615222	4808.269047	24.613312
138.696307	4812.431244	24.618330
138.674227	4822.184853	24.623347
138.848108	4820.215530	24.628365
138.633379	4836.036935	24.633383
139.075578	4848.772250	24.638400
139.207468	4850.201879	24.643418
139.506721	4850.099475	24.648435
140.271904	4854.945003	24.653453
139.995171	4866.565711	24.658471
140.601365	4858.663591	24.663488
140.595909	4857.887277	24.668506
140.745033	4858.060262	24.673523
141.059588	4853.895494	24.678541
141.037171	4857.468489	24.683559
141.365013	4851.336576	24.688576
141.314194	4844.408373	24.693594
141.567164	4842.740924	24.698611
141.696691	4833.414595	24.703629
141.775111	4852.132736	24.708647
141.978740	4829.630200	24.713664
141.788701	4839.265247	24.718682
141.777054	4841.814209	24.723699
141.966327	4834.053838	24.728717
141.923188	4842.894253	24.733735
142.211873	4836.186853	24.738752
141.993529	4855.249644	24.743770
141.982613	4867.206567	24.748787
141.957790	4864.546500	24.753805
141.921899	4880.566620	24.758823
142.131909	4897.468906	24.763840
142.457812	4914.352738	24.768858
142.843987	4935.513230	24.773875
143.163938	4936.562730	24.778893
142.973256	4943.346213	24.783911
143.455314	4936.494804	24.788928
143.611275	4951.805032	24.793946
143.830759	4951.807241	24.798963
144.198179	4958.050656	24.803981
144.272122	4959.336351	24.808999
144.321310	4965.307391	24.814016
144.289610	4955.858146	24.819034
144.378394	4975.126000	24.824051
144.649860	4982.087082	24.829069
144.853772	4994.213955	24.834087
144.850988	4983.971544	24.839104
144.909026	4994.060046	24.844122
144.667646	5006.276676	24.849139
145.164398	5018.912496	24.854157
145.107698	5036.189238	24.859175
145.403516	5044.176429	24.864192
145.426228	5059.990892	24.869210
145.361526	5061.030289	24.874227
145.933292	5080.146344	24.879245
145.914595	5080.949705	24.884263
146.117341	5091.339485	24.889280
146.337454	5112.380537	24.894298
145.883941	5117.471982	24.899315
146.595779	5132.445080	24.904333
146.793910	5152.059622	24.909351
147.102135	5153.679707	24.914368
147.057614	5144.218304	24.919386
146.970286	5170.298170	24.924403
147.654910	5178.394085	24.929421
147.663853	5180.337192	24.934439
147.973337	5176.865454	24.939456
147.873756	5197.928243	24.944474
148.177689	5197.450967	24.949491
148.682028	5199.882740	24.954509
148.539437	5205.172204	24.959527
148.375973	5200.662282	24.964544
148.387967	5221.564012	24.969562
148.430479	5221.081348	24.974579
148.750934	5232.536931	24.979597
148.968691	5249.505251	24.984615
149.029900	5263.396575	24.989632
149.652087	5272.737825	24.994650
149.329859	5286.348718	24.999667
149.720774	5286.648495	25.004685
149.666697	5299.312282	25.009703
149.766213	5307.104620	25.014720
150.470018	5313.241874	25.019738
150.640555	5317.950880	25.024755
150.633938	5315.746078	25.029773
150.633609	5326.639942	25.034791
150.774522	5345.960230	25.039808
150.810002	5343.386145	25.044826
150.746748	5349.239765	25.049843
151.248854	5358.254488	25.054861
151.051631	5377.802696	25.059879
151.337309	5377.268593	25.064896
151.799787	5390.241190	25.069914
151.890836	5401.623183	25.074931
152.201088	5400.505339	25.079949
152.229204	5400.804763	25.084967
152.448141	5401.015772	25.089984
152.668385	5391.279463	25.095002
152.882745	5398.426638	25.100019
153.273009	5407.692310	25.105037
153.100379	5418.018673	25.110055
153.397548	5425.892423	25.115072
153.599245	5420.039580	25.120090
153.311055	5427.000139	25.125107
153.466546	5424.235193	25.130125
153.473872	5431.497119	25.135143
153.624791	5448.407454	25.140160
153.891193	5445.538228	25.145178
153.582026	5461.336572	25.150195
153.868799	5473.171242	25.155213
153.775353	5484.297273	25.160231
154.100058	5494.110234	25.165248
154.682892	5510.843326	25.170266
154.588767	5527.778714	25.175283
154.783659	5522.678318	25.180301
155.056308	5545.719558	25.185319
155.356130	5556.908666	25.190336
155.377098	5563.577697	25.195354
155.507580	5577.995708	25.200371
156.015066	5575.693626	25.205389
155.962591	5580.827262	25.210407
156.089720	5591.721394	25.215424
156.174038	5587.492308	25.220442
156.392468	5613.973386	25.225459
156.565112	5609.443724	25.230477
156.329680	5619.953135	25.235495
156.536568	5639.066710	25.240512
157.220906	5637.776425	25.245530
157.094779	5653.801299	25.250547
157.370211	5653.829654	25.255565
157.516618	5668.979136	25.260583
157.535143	5665.965190	25.265600
157.769795	5678.068580	25.270618
157.962107	5699.190645	25.275635
158.017886	5697.732298	25.280653
158.506221	5700.556670	25.285671
158.437530	5726.436672	25.290688
158.801667	5724.957798	25.295706
158.675526	5729.528780	25.300723
158.949290	5734.319207	25.305741
159.374294	5757.895420	25.310759
159.044708	5750.120796	25.315776
159.642002	5751.027393	25.320794
159.641230	5754.625347	25.325811
160.153377	5769.818900	25.330829
160.077681	5775.397512	25.335847
160.320707	5781.512285	25.340864
160.629629	5775.103565	25.345882
160.660460	5771.609482	25.350899
160.742006	5774.133658	25.355917
161.081112	5786.049653	25.360935
161.116089	5805.274694	25.365952
161.441134	5805.670491	25.370970
161.544003	5802.977232	25.375987
161.311544	5797.497256	25.381005
161.747626	5813.539920	25.386023
161.662402	5821.445121	25.391040
161.979639	5828.254844	25.396058
161.593947	5831.546607	25.401075
161.915586	5850.807553	25.406093
162.098125	5870.175124	25.411111
161.624176	5881.625358	25.416128
162.373701	5887.403975	25.421146
162.098938	5903.316758	25.426163
162.600050	5922.494412	25.431181
162.480099	5933.617286	25.436199
162.486672	5943.933115	25.441216
163.018496	5958.328100	25.446234
162.655761	5975.272372	25.451251
163.263433	5987.564474	25.456269
163.675526	5999.168424	25.461287
163.868183	6018.506141	25.466304
164.582663	6027.045688	25.471322
164.446930	6025.429320	25.476339
164.651406	6024.629091	25.481357
164.905686	6040.791197	25.486375
165.069723	6036.886629	25.491392
165.439221	6035.912482	25.496410
165.179189	6044.793548	25.501427
165.350517	6040.041089	25.506445
165.807246	6058.917542	25.511463
166.107244	6071.782234	25.516480
166.283824	6067.358902	25.521498
166.442090	6082.717891	25.526515
166.280634	6067.170589	25.531533
166.475091	6075.817053	25.536551
166.485688	6098.521442	25.541568
166.982699	6097.481209	25.546586
167.209541	6102.635547	25.551603
167.296084	6096.318784	25.556621
167.428500	6106.545285	25.561639
167.491799	6120.787504	25.566656
167.749372	6120.492759	25.571674
167.624903	6120.608834	25.576691
167.690516	6135.487862	25.581709
167.934202	6148.584869	25.586727
168.073609	6149.814103	25.591744
168.663011	6164.958972	25.596762
168.517807	6186.930116	25.601779
168.525913	6180.582246	25.606797
168.772794	6193.303067	25.611815
168.953709	6208.132286	25.616832
168.801426	6215.331306	25.621850
169.186331	6236.281103	25.626867
169.026039	6246.054621	25.631885
169.644345	6261.074273	25.636903
169.599690	6267.102356	25.641920
169.991779	6275.256906	25.646938
169.793547	6287.378351	25.651955
169.851652	6303.754477	25.656973
170.542367	6317.746119	25.661991
170.516152	6331.848240	25.667008
170.806772	6331.525947	25.672026
171.163074	6357.895574	25.677044
171.408992	6356.146442	25.682061
171.512960	6365.819412	25.687079
171.477350	6372.802998	25.692096
172.192378	6388.531316	25.697114
172.196847	6389.287574	25.702132
172.534188	6402.956800	25.707149
172.702643	6390.457612	25.712167
172.309569	6409.357551	25.717184
172.735745	6423.562585	25.722202
172.855845	6425.048666	25.727220
172.839754	6426.680247	25.732237
173.119446	6444.834395	25.737255
173.166804	6456.141707	25.742272
173.785929	6462.613269	25.747290
173.794893	6466.120765	25.752308
173.764274	6479.245513	25.757325
174.066998	6488.958781	25.762343
173.956972	6489.494629	25.767360
174.670032	6498.658476	25.772378
175.075671	6510.843575	25.777396
175.041667	6515.711375	25.782413
175.407162	6508.406086	25.787431
175.097324	6507.632223	25.792448
175.448758	6508.244193	25.797466
175.491419	6532.406511	25.802484
175.709839	6526.754479	25.807501
176.313147	6522.146695	25.812519
176.270974	6527.599492	25.817536
176.615365	6515.938943	25.822554
176.503378	6524.542845	25.827572
176.346088	6539.318305	25.832589
176.867309	6541.163066	25.837607
176.915920	6561.092480	25.842624
177.148525	6558.491743	25.847642
177.406649	6557.703840	25.852660
177.187729	6572.473031	25.857677
177.492026	6576.306391	25.862695
177.779501	6588.735662	25.867712
177.812269	6603.348064	25.872730
178.067926	6616.179613	25.877748
177.968071	6620.743332	25.882765
178.443514	6630.441377	25.887783
178.317132	6650.017188	25.892800
178.576389	6662.815096	25.897818
178.945534	6673.576030	25.902836
178.544170	6684.297236	25.907853
179.135676	6689.937796	25.912871
178.939717	6711.029639	25.917888
179.245911	6717.730527	25.922906
179.372558	6741.813833	25.927924
179.760460	6762.086456	25.932941
180.252042	6762.958702	25.937959
180.373964	6777.628126	25.942976
180.674464	6774.155963	25.947994
180.896217	6786.412001	25.953012
181.323317	6795.108419	25.958029
181.508357	6790.002955	25.963047
181.404923	6797.117719	25.968064
181.784391	6816.790052	25.973082
182.121038	6817.198917	25.978100
181.887560	6817.044831	25.983117
182.169418	6816.004075	25.988135
182.210095	6838.076770	25.993152
182.400074	6848.120116	25.998170
182.694194	6855.913964	26.003188
182.615067	6865.401847	26.008205
183.129827	6874.195589	26.013223
183.001301	6883.947679	26.018240
183.537683	6890.263036	26.023258
183.688353	6910.145212	26.028276
183.583823	6917.643799	26.033293
184.027835	6914.112315	26.038311
183.972358	6930.794669	26.043328
184.291513	6940.503123	26.048346
184.742323	6936.236411	26.053364
184.452087	6945.576685	26.058381
185.059630	6955.000144	26.063399
184.735519	6966.898850	26.068416
184.823654	6975.713916	26.073434
185.170470	6989.412007	26.078452
185.118820	7007.306796	26.083469
185.735669	7013.151992	26.088487
185.864416	7025.455176	26.093504
185.923585	7032.580046	26.098522
186.099196	7048.781461	26.103540
185.858449	7051.981646	26.108557
186.538091	7071.060144	26.113575
186.767294	7088.933563	26.118592
186.863744	7097.900909	26.123610
187.063398	7098.074981	26.128628
187.181433	7126.292377	26.133645
187.177018	7124.891949	26.138663
187.272591	7139.650367	26.143680
187.405913	7145.025379	26.148698
188.193452	7149.485118	26.153716
188.086574	7170.097258	26.158733
188.559245	7179.899288	26.163751
188.796666	7178.631958	26.168768
189.070215	7195.618305	26.173786
189.089378	7202.160724	26.178804
189.256054	7223.617543	26.183821
189.518097	7215.008203	26.188839
189.315472	7232.158780	26.193856
189.513259	7244.089910	26.198874
190.012970	7253.407014	26.203892
190.083030	7272.082150	26.208909
190.272265	7273.704118	26.213927
190.734594	7293.128549	26.218944
190.669735	7309.360735	26.223962
190.743685	7303.336236	26.228980
190.690218	7322.706204	26.233997
190.736585	7330.106658	26.239015
191.339019	7356.868697	26.244032
191.336226	7359.703306	26.249050
191.601984	7386.906512	26.254068
191.624752	7407.432039	26.259085
192.038393	7410.107667	26.264103
192.209534	7429.904385	26.269120
192.378634	7444.506723	26.274138
193.019271	7457.381321	26.279156
193.089357	7465.819210	26.284173
193.275079	7465.119701	26.289191
193.535346	7483.435804	26.294208
193.896353	7505.622401	26.299226
194.185072	7498.044279	26.304244
193.881857	7508.537841	26.309261
194.218444	7523.738629	26.314279
194.097627	7531.040927	26.319296
194.418658	7540.486352	26.324314
195.101188	7552.055964	26.329332
195.090846	7562.823848	26.334349
195.494494	7578.421567	26.339367
195.343680	7579.535300	26.344384
195.534750	7591.455203	26.349402
196.093762	7607.532830	26.354420
195.969045	7613.092661	26.359437
196.226942	7616.837102	26.364455
196.685343	7629.169473	26.369472
196.832599	7649.464314	26.374490
197.308683	7650.944136	26.379508
197.315163	7655.667712	26.384525
197.304922	7648.430640	26.389543
197.412864	7663.584484	26.394560
197.264671	7687.180838	26.399578
197.713000	7688.639282	26.404596
197.924032	7700.919076	26.409613
198.047791	7710.595880	26.414631
198.269736	7730.886292	26.419648
198.375903	7740.441582	26.424666
198.425009	7753.576977	26.429684
198.638081	7775.197760	26.434701
199.085139	7776.357887	26.439719
199.477599	7794.579128	26.444736
199.208322	7809.738288	26.449754
199.554430	7808.618267	26.454772
199.635019	7827.285215	26.459789
199.934305	7836.223214	26.464807
200.594867	7840.630998	26.469824
200.833887	7852.587241	26.474842
201.286988	7849.700747	26.479860
201.234093	7851.306294	26.484877
201.329757	7853.509439	26.489895
201.918264	7845.010933	26.494912
201.633189	7855.093680	26.499930
202.225305	7859.617606	26.504948
202.005240	7881.492462	26.509965
201.904232	7886.187493	26.514983
202.525731	7880.937479	26.520000
202.590681	7900.351489	26.525018
202.877995	7906.081633	26.530036
202.599509	7917.015617	26.535053
202.811779	7935.399295	26.540071
203.057622	7938.297459	26.545088
203.321756	7967.674415	26.550106
203.320270	7975.541564	26.555124
203.720653	7999.943638	26.560141
204.069191	8007.587225	26.565159
204.271773	8010.050687	26.570176
203.982671	8032.921856	26.575194
204.418875	8046.405144	26.580212
204.642540	8058.364881	26.585229
204.336326	8077.198795	26.590247
204.617427	8091.390838	26.595264
205.015182	8121.054656	26.600282
205.651518	8127.771395	26.605300
205.946316	8153.409052	26.610317
206.153014	8166.534356	26.615335
206.098332	8170.846032	26.620352
206.463660	8193.224285	26.625370
206.847649	8195.616672	26.630388
206.836814	8217.012163	26.635405
206.996243	8231.947672	26.640423
207.549578	8242.023689	26.645440
207.727436	8262.827820	26.650458
207.932812	8268.396049	26.655476
208.171018	8280.964020	26.660493
208.424018	8284.188751	26.665511
208.591361	8294.466788	26.670528
208.858114	8297.255202	26.675546
209.677549	8297.855657	26.680564
209.915888	8300.025705	26.685581
210.154027	8300.268232	26.690599
210.190920	8297.803716	26.695616
209.840138	8302.222918	26.700634
210.302635	8313.508260	26.705652
210.420543	8320.906740	26.710669
210.758693	8326.779045	26.715687
211.313239	8346.198110	26.720704
211.204024	8361.087789	26.725722
211.459911	8361.856720	26.730740
211.622711	8361.807704	26.735757
211.591773	8363.932703	26.740775
211.393629	8370.747239	26.745792
211.686345	8389.355180	26.750810
211.793010	8407.415077	26.755828
212.155645	8420.185411	26.760845
212.251526	8434.819729	26.765863
212.533138	8447.302635	26.770880
212.735187	8464.615736	26.775898
212.991515	8476.515220	26.780916
213.103912	8498.005619	26.785933
213.348392	8500.443291	26.790951
213.972253	8517.502821	26.795968
213.782530	8517.610846	26.800986
214.045317	8525.465078	26.806004
214.364371	8537.648009	26.811021
214.536197	8541.143869	26.816039
214.777452	8553.569758	26.821056
214.832782	8571.947162	26.826074
215.351524	8568.487982	26.831092
215.726128	8581.944937	26.836109
215.410078	8597.798731	26.841127
215.767005	8598.827381	26.846144
215.785027	8614.437414	26.851162
215.859397	8621.499815	26.856180
216.143201	8641.509340	26.861197
216.297210	8672.639705	26.866215
216.794989	8673.214850	26.871232
216.789444	8694.884234	26.876250
217.310534	8701.903167	26.881268
217.576031	8725.426014	26.886285
217.268066	8738.271004	26.891303
217.835151	8749.883523	26.896320
217.756739	8767.508234	26.901338
218.147834	8786.592633	26.906356
218.325298	8805.778720	26.911373
218.194807	8824.844271	26.916391
218.858960	8844.962582	26.921408
218.999114	8858.834483	26.926426
218.935424	8887.627162	26.931444
219.490985	8895.030390	26.936461
219.667807	8919.656928	26.941479
220.256931	8928.813645	26.946496
220.013119	8958.260280	26.951514
220.462439	8963.094997	26.956532
220.454947	8981.020109	26.961549
220.861059	9000.632427	26.966567
221.317802	8998.049202	26.971584
221.539104	9024.783636	26.976602
221.924212	9032.230217	26.981620
222.479069	9032.746265	26.986637
222.505128	9049.888364	26.991655
222.854774	9064.203016	26.996672
222.485606	9079.543039	27.001690
223.098407	9077.388409	27.006708
223.109248	9096.229133	27.011725
223.509977	9113.169613	27.016743
223.905902	9116.028878	27.021760
223.739241	9142.070142	27.026778
223.919043	9137.001041	27.031796
224.053657	9152.898667	27.036813
224.356733	9165.408504	27.041831
224.616989	9182.544918	27.046848
224.831326	9201.348803	27.051866
225.413052	9215.046809	27.056884
225.767268	9232.012475	27.061901
225.875693	9228.611091	27.066919
225.836232	9234.718208	27.071936
225.815779	9256.021365	27.076954
226.073654	9269.117017	27.081972
226.271190	9284.049542	27.086989
226.366567	9302.968631	27.092007
226.740841	9321.746083	27.097024
227.140429	9332.458864	27.102042
227.172542	9352.864021	27.107060
227.638401	9360.087792	27.112077
227.964348	9380.995605	27.117095
228.234041	9383.204709	27.122112
228.280738	9399.685961	27.127130
229.018521	9414.473700	27.132148
229.475719	9420.481036	27.137165
229.290016	9418.934854	27.142183
229.908656	9415.305283	27.147200
230.362168	9413.509519	27.152218
229.920531	9416.198407	27.157236
230.219074	9426.029187	27.162253
230.037624	9437.167083	27.167271
230.592574	9434.713212	27.172288
230.425577	9448.820210	27.177306
230.179918	9474.668742	27.182324
230.748675	9473.294192	27.187341
230.858582	9499.215244	27.192359
231.477308	9514.274948	27.197376
231.296223	9538.885490	27.202394
231.528078	9545.508547	27.207412
231.746079	9568.658451	27.212429
231.848110	9597.906206	27.217447
231.992175	9608.739620	27.222464
232.618408	9631.560242	27.227482
232.635640	9649.646641	27.232500
233.062275	9669.137414	27.237517
233.008882	9692.526386	27.242535
233.279314	9710.206037	27.247552
233.504105	9739.651083	27.252570
233.912197	9759.822549	27.257588
234.059894	9775.676866	27.262605
234.395933	9801.400911	27.267623
234.655331	9821.774415	27.272640
234.595361	9836.636010	27.277658
234.887148	9863.730396	27.282676
235.765518	9877.577423	27.287693
235.825004	9898.598722	27.292711
236.318049	9900.060194	27.297728
236.512102	9916.461559	27.302746
236.773681	9932.899777	27.307764
236.988793	9937.481434	27.312781
236.909646	9964.498968	27.317799
237.391357	9978.036205	27.322816
237.553836	9988.077436	27.327834
237.775703	10001.876089	27.332852
238.435338	10002.818302	27.337869
238.736743	10025.555590	27.342887
238.969619	10031.922642	27.347904
238.565087	10039.573373	27.352922
238.917774	10057.304340	27.357940
239.243031	10059.207305	27.362957
239.209946	10092.634884	27.367975
239.398472	10102.431577	27.372992
239.930609	10119.924816	27.378010
239.987864	10132.532188	27.383028
240.768130	10145.526794	27.388045
241.093529	10152.639547	27.393063
241.411059	10167.213412	27.398080
241.137911	10177.615480	27.403098
241.732386	10184.202975	27.408116
242.331335	10188.159218	27.413133
242.642193	10198.179079	27.418151
243.403753	10195.533208	27.423168
243.574291	10196.563000	27.428186
243.399078	10193.126607	27.433204
243.604872	10193.028693	27.438221
243.748115	10204.485807	27.443239
244.084580	10220.669232	27.448256
244.152464	10220.680891	27.453274
243.947025	10230.198844	27.458292
244.285960	10243.916017	27.463309
244.373233	10265.885651	27.468327
244.293271	10268.624878	27.473344
244.824051	10287.560234	27.478362
244.624089	10299.938676	27.483380
245.073292	10312.706385	27.488397
245.149374	10328.355708	27.493415
245.408235	10344.787710	27.498432
245.607220	10365.532764	27.503450
245.551600	10382.406239	27.508468
246.120069	10405.782737	27.513485
246.053267	10427.800250	27.518503
245.777943	10456.792406	27.523520
246.639600	10483.616683	27.528538
246.866241	10509.012606	27.533556
247.250332	10527.657485	27.538573
247.436640	10554.220655	27.543591
247.888438	10565.299810	27.548608
248.216297	10589.752553	27.553626
248.092568	10604.916160	27.558644
248.502358	10627.035962	27.563661
248.805848	10644.091123	27.568679
249.102979	10671.102472	27.573696
249.666810	10692.278152	27.578714
249.725658	10708.216692	27.583732
250.189431	10731.772567	27.588749
250.402451	10758.045649	27.593767
250.348597	10769.052965	27.598784
250.572030	10787.520787	27.603802
250.432765	10810.278040	27.608820
251.180187	10829.427788	27.613837
251.532627	10840.561458	27.618855
251.774158	10856.163320	27.623872
252.355352	10878.150206	27.628890
252.436266	10906.255165	27.633908
253.114046	10907.535563	27.638925
253.364328	10918.810741	27.643943
253.577178	10920.475648	27.648960
253.913278	10935.010883	27.653978
253.979301	10962.401470	27.658996
254.587377	10958.337638	27.664013
254.864611	10983.625847	27.669031
255.096290	10988.015180	27.674048
255.159958	10984.536564	27.679066
255.508550	10995.774978	27.684084
255.832612	11013.887565	27.689101
255.843574	11029.362454	27.694119
255.728198	11031.223720	27.699136
256.197571	11041.219347	27.704154
256.179352	11064.237323	27.709172
256.547273	11084.457309	27.714189
256.730645	11101.137407	27.719207
256.823199	11117.987032	27.724224
257.256339	11130.910119	27.729242
257.178693	11155.321580	27.734260
257.508747	11179.666916	27.739277
258.065586	11204.147940	27.744295
258.028761	11217.410749	27.749312
258.547217	11234.043191	27.754330
258.536065	11251.775261	27.759348
259.051570	11277.025918	27.764365
259.276995	11288.349605	27.769383
259.452038	11319.887354	27.774400
259.951290	11321.936472	27.779418
260.205451	11342.974583	27.784436
260.553009	11351.969563	27.789453
260.659106	11365.842196	27.794471
260.822458	11377.467772	27.799488
260.946661	11401.852371	27.804506
261.193830	11422.645931	27.809524
261.574516	11440.124016	27.814541
261.880527	11465.516926	27.819559
261.663810	11485.393338	27.824576
262.324833	11498.409646	27.829594
263.351353	11499.433612	27.834612
263.891997	11493.953219	27.839629
264.280015	11509.898528	27.844647
264.626074	11519.902336	27.849664
264.694772	11517.418650	27.854682
264.698070	11528.243653	27.859700
265.089409	11516.519691	27.864717
265.385959	11522.453666	27.869735
265.340393	11523.766056	27.874752
265.746395	11530.964517	27.879770
265.858473	11547.259830	27.884788
265.918183	11551.698375	27.889805
266.220955	11563.513649	27.894823
266.209630	11585.335217	27.899840
266.642020	11591.777682	27.904858
266.567090	11617.490970	27.909876
266.716604	11626.175491	27.914893
266.398823	11652.160820	27.919911
266.526874	11681.885491	27.924928
267.031024	11706.202698	27.929946
267.449878	11736.347160	27.934964
267.173703	11769.129979	27.939981
267.641194	11797.014680	27.944999
267.593420	11831.649044	27.950016
268.311836	11869.036734	27.955034
268.604919	11898.411346	27.960052
268.964461	11911.279528	27.965069
269.483140	11949.311997	27.970087
269.519214	11977.446751	27.975104
269.886222	12000.053801	27.980122
270.551421	12032.624022	27.985140
270.780956	12054.647303	27.990157
271.265281	12071.073546	27.995175
271.139115	12092.456314	28.000192
271.488828	12109.065693	28.005210
271.412378	12129.743740	28.010228
272.366646	12150.715436	28.015245
272.672558	12180.116792	28.020263
272.520836	12205.139376	28.025280
273.098516	12226.824553	28.030298
273.891157	12240.126883	28.035316
273.673849	12260.237563	28.040333
274.285775	12271.180985	28.045351
274.447730	12297.382321	28.050368
274.659120	12309.274780	28.055386
275.629655	12320.935543	28.060404
275.856664	12331.170797	28.065421
276.385499	12327.699707	28.070439
276.539163	12333.936644	28.075456
276.367783	12338.670658	28.080474
276.480625	12349.994885	28.085492
276.749581	12372.894519	28.090509
277.096129	12379.966141	28.095527
277.376873	12388.195911	28.100544
277.827156	12400.422223	28.105562
278.215392	12416.089467	28.110580
278.108048	12436.692669	28.115597
278.567881	12435.089369	28.120615
278.566195	12459.208095	28.125632
279.007219	12464.100417	28.130650
279.187142	12493.063125	28.135668
279.338814	12504.874250	28.140685
279.495703	12521.219828	28.145703
279.791408	12546.015744	28.150720
280.166507	12566.285245	28.155738
279.977665	12586.947877	28.160756
280.358609	12607.292099	28.165773
280.734478	12608.857612	28.170791
280.659099	12642.259661	28.175808
280.913173	12659.972843	28.180826
281.521201	12685.473500	28.185844
281.423634	12709.438332	28.190861
281.893301	12726.118241	28.195879
282.270879	12758.904751	28.200896
282.756402	12773.888005	28.205914
282.708067	12791.828072	28.210932
283.209330	12811.987094	28.215949
283.468400	12838.083342	28.220967
284.107497	12849.693972	28.225984
284.819226	12866.390542	28.231002
285.022429	12878.270596	28.236020
284.839196	12900.313172	28.241037
285.379117	12904.647092	28.246055
285.477425	12927.476578	28.251072
285.683222	12936.384108	28.256090
286.125622	12964.735150	28.261108
286.168267	12978.775719	28.266125
286.846664	12992.409681	28.271143
286.892792	13010.261802	28.276160
287.603513	13020.852079	28.281178
288.017317	13036.564528	28.286196
288.122419	13045.914341	28.291213
288.549980	13070.128129	28.296231
288.282301	13086.001122	28.301248
288.796134	13097.027592	28.306266
289.423784	13123.302603	28.311284
289.339467	13128.621228	28.316301
289.664746	13141.965705	28.321319
289.756025	13156.472698	28.326336
289.852590	13184.498632	28.331354
290.310061	13205.820568	28.336372
290.441847	13222.741506	28.341389
290.651974	13246.148560	28.346407
291.032831	13266.184742	28.351424
291.155414	13299.125020	28.356442
291.691979	13321.332248	28.361460
291.492931	13343.404840	28.366477
292.137313	13360.132021	28.371495
292.475208	13398.543051	28.376512
292.602801	13422.777256	28.381530
292.990365	13439.197325	28.386548
293.737820	13462.583187	28.391565
294.528398	13475.018537	28.396583
294.395172	13487.936744	28.401600
295.124217	13494.573386	28.406618
295.896971	13508.348128	28.411636
295.696523	13509.412192	28.416653
295.937343	13509.927010	28.421671
296.230155	13534.847839	28.426688
296.425404	13553.060314	28.431706
296.480068	13564.204361	28.436724
296.921109	13579.988458	28.441741
297.215048	13595.231239	28.446759
297.350105	13621.239029	28.451776
297.655275	13633.181494	28.456794
298.061451	13636.570193	28.461812
297.977261	13671.033283	28.466829
298.451492	13674.970151	28.471847
298.348729	13721.308194	28.476864
298.612238	13728.118408	28.481882
298.874105	13755.599366	28.486900
299.145503	13781.556393	28.491917
299.636601	13803.798626	28.496935
299.716704	13826.796297	28.501952
299.881786	13848.460785	28.506970
300.442055	13865.259196	28.511988
300.551074	13894.680603	28.517005
301.137318	13906.094320	28.522023
301.547310	13927.477098	28.527040
301.704241	13952.246204	28.532058
302.307640	13959.841630	28.537076
302.822534	13977.780836	28.542093
302.847876	13995.399513	28.547111
303.272193	14013.585478	28.552128
303.354039	14030.436749	28.557146
303.680235	14039.403681	28.562164
303.672913	14081.793189	28.567181
304.252928	14090.063939	28.572199
304.284637	14118.928078	28.577216
304.533045	14147.677468	28.582234
304.842132	14169.175039	28.587252
305.120435	14196.486951	28.592269
305.194826	14225.273266	28.597287
305.525400	14244.040853	28.602304
305.764144	14278.662758	28.607322
306.307767	14294.876522	28.612340
306.421355	14331.098509	28.617357
307.252955	14350.530021	28.622375
307.762587	14376.147392	28.627392
307.868753	14393.474112	28.632410
308.323439	14421.645981	28.637428
308.698954	14448.245554	28.642445
309.173897	14459.764834	28.647463
309.298164	14491.611885	28.652480
309.234310	14505.783358	28.657498
309.771908	14526.516879	28.662516
309.801165	14556.548473	28.667533
310.540230	14577.453476	28.672551
310.823317	14600.724267	28.677568
311.175412	14628.847342	28.682586
311.182131	14636.408247	28.687604
311.931678	14668.076113	28.692621
312.417557	14686.804224	28.697639
312.789475	14703.716747	28.702656
313.139908	14722.563540	28.707674
313.727151	14715.466759	28.712692
313.744386	14741.863127	28.717709
313.952402	14754.642110	28.722727
314.010794	14766.527109	28.727744
314.171919	14781.770999	28.732762
314.916357	14802.859800	28.737780
315.100430	14830.067066	28.742797
315.021668	14848.800904	28.747815
315.623275	14880.399194	28.752832
315.483410	14907.020513	28.757850
315.929926	14927.189676	28.762868
316.077234	14965.922898	28.767885
316.461257	14979.022708	28.772903
316.723339	15011.646953	28.777920
317.098182	15029.725638	28.782938
317.701427	15053.911609	28.787956
317.948894	15080.290761	28.792973
318.289350	15105.499224	28.797991
318.921968	15126.176743	28.803008
318.931255	15150.899688	28.808026
319.415058	15175.835420	28.813044
319.648075	15197.477797	28.818061
320.011698	15225.231170	28.823079
320.159965	15231.575715	28.828096
320.632208	15265.418562	28.833114
320.849802	15268.005169	28.838132
321.165725	15297.854948	28.843149
321.266461	15313.055775	28.848167
321.820955	15332.974233	28.853184
321.837232	15358.591568	28.858202
322.165505	15377.548396	28.863220
322.420137	15397.231468	28.868237
322.732855	15436.726387	28.873255
323.052583	15453.002139	28.878272
323.472807	15477.789702	28.883290
323.562983	15505.005803	28.888308
324.010039	15539.543750	28.893325
324.556647	15566.001656	28.898343
324.820534	15584.427224	28.903360
324.827329	15619.787150	28.908378
325.510344	15642.781776	28.913396
326.084172	15662.936999	28.918413
326.406836	15678.282554	28.923431
327.187070	15706.312709	28.928448
327.283195	15719.574423	28.933466
327.622068	15728.229674	28.938484
327.786016	15759.155263	28.943501
328.125245	15772.696596	28.948519
328.414749	15784.537633	28.953536
328.339144	15809.326106	28.958554
328.820803	15833.405756	28.963572
329.167122	15862.208083	28.968589
329.568026	15889.496141	28.973607
329.990399	15920.784180	28.978624
330.683566	15934.809056	28.983642
331.140299	15946.740643	28.988660
331.266670	15972.398962	28.993677
331.815916	15983.572823	28.998695
331.931332	16002.542091	29.003712
332.325130	16023.380208	29.008730
332.834628	16039.593492	29.013748
332.768060	16060.575910	29.018765
332.686595	16077.172696	29.023783
332.948332	16109.562746	29.028800
333.507683	16133.828531	29.033818
333.557358	16164.835336	29.038836
333.911215	16184.146643	29.043853
334.546400	16213.629805	29.048871
335.206514	16241.715507	29.053888
335.142678	16267.330223	29.058906
335.468197	16293.214456	29.063924
335.770848	16327.426549	29.068941
336.109762	16348.330939	29.073959
336.473849	16369.216987	29.078976
336.927490	16406.276043	29.083994
337.396008	16416.648701	29.089012
337.669874	16452.687957	29.094029
338.128108	16478.008210	29.099047
338.406830	16493.771647	29.104064
338.528501	16528.315282	29.109082
338.865073	16547.831646	29.114100
339.368610	16574.542647	29.119117
339.317610	16602.881077	29.124135
340.070269	16636.257727	29.129152
340.079778	16670.700497	29.134170
340.831560	16688.820847	29.139188
340.938217	16722.826727	29.144205
341.172473	16746.149649	29.149223
341.986921	16773.655776	29.154240
341.948727	16810.187428	29.159258
342.329977	16821.202194	29.164276
342.597333	16857.068447	29.169293
342.730401	16885.197087	29.174311
343.324092	16900.714708	29.179328
343.859685	16924.980877	29.184346
344.196070	16936.980465	29.189364
344.531909	16962.252437	29.194381
344.854858	16981.689610	29.199399
345.302591	16996.151814	29.204416
345.465924	17026.923826	29.209434
345.741022	17043.252701	29.214452
345.955455	17075.884217	29.219469
345.920896	17097.973917	29.224487
346.619643	17117.845356	29.229504
346.308867	17156.604646	29.234522
346.939414	17183.779459	29.239540
347.482953	17222.505749	29.244557
347.531742	17261.404168	29.249575
348.098071	17291.286891	29.254592
348.506346	17324.709531	29.259610
348.734857	17349.257477	29.264628
349.156047	17380.821183	29.269645
349.806176	17406.419940	29.274663
350.784970	17420.288297	29.279680
350.793209	17453.307905	29.284698
351.125796	17469.170516	29.289716
351.479209	17488.894845	29.294733
351.708357	17512.643728	29.299751
351.863407	17533.961634	29.304768
352.156439	17568.600349	29.309786
352.580975	17598.937522	29.314804
353.102829	17628.752579	29.319821
353.181708	17656.841086	29.324839
353.817745	17686.906834	29.329856
353.956301	17719.498625	29.334874
354.742612	17747.778735	29.339892
355.075209	17773.528542	29.344909
355.413538	17805.272338	29.349927
355.782258	17829.737802	29.354944
356.185735	17857.058634	29.359962
356.410489	17876.628245	29.364980
356.852376	17898.242618	29.369997
357.261445	17922.520234	29.375015
357.964478	17950.491368	29.380032
358.150138	17971.705439	29.385050
358.284233	17996.225888	29.390068
358.947773	18020.067281	29.395085
358.707077	18042.430511	29.400103
359.368247	18064.281389	29.405120
359.848829	18081.202978	29.410138
360.252755	18119.666078	29.415156
360.638128	18128.647487	29.420173
360.614568	18161.509838	29.425191
361.187613	18190.860247	29.430208
361.602852	18211.710173	29.435226
362.042274	18246.493082	29.440244
362.455868	18271.593340	29.445261
362.423740	18301.802725	29.450279
362.704632	18309.715443	29.455296
363.049680	18354.916982	29.460314
363.564810	18379.975314	29.465332
364.003904	18402.661195	29.470349
364.505314	18441.652709	29.475367
364.741371	18466.130114	29.480384
364.998930	18491.694870	29.485402
365.630428	18522.327247	29.490420
365.704974	18553.641785	29.495437
365.725180	18584.010088	29.500455
366.155397	18604.678306	29.505472
366.386733	18632.325377	29.510490
366.755112	18665.960704	29.515508
367.451786	18701.876281	29.520525
367.807632	18736.477041	29.525543
368.009941	18756.415575	29.530560
368.317618	18784.706021	29.535578
369.190705	18811.485359	29.540596
369.634285	18840.800092	29.545613
369.568751	18862.271422	29.550631
369.751700	18887.775086	29.555648
370.103951	18919.693682	29.560666
370.639703	18944.812498	29.565684
370.706729	18973.646134	29.570701
370.897287	19012.351678	29.575719
371.283369	19047.741028	29.580736
371.821853	19088.671696	29.585754
372.382983	19116.991546	29.590772
372.858202	19147.203311	29.595789
373.162993	19179.243794	29.600807
373.666544	19213.441073	29.605824
373.965823	19238.519212	29.610842
374.152786	19269.275678	29.615860
374.959923	19299.180344	29.620877
375.307661	19329.817201	29.625895
375.628047	19350.841961	29.630912
376.058665	19377.963716	29.635930
376.669442	19410.541854	29.640948
377.272177	19430.736286	29.645965
377.386840	19469.728234	29.650983
377.908220	19474.697613	29.656000
378.198079	19506.402253	29.661018
378.371651	19537.513001	29.666036
378.587570	19567.804860	29.671053
379.064500	19605.824138	29.676071
379.028879	19626.963561	29.681088
379.992873	19670.544493	29.686106
380.130552	19693.495031	29.691124
380.608404	19718.955705	29.696141
380.898022	19768.266132	29.701159
381.359635	19794.719689	29.706176
381.637123	19814.862985	29.711194
382.307640	19855.883958	29.716212
382.500552	19881.951888	29.721229
383.173939	19917.035222	29.726247
383.632766	19936.391793	29.731264
383.891032	19976.091012	29.736282
383.863009	20006.619679	29.741300
384.416551	20038.204273	29.746317
384.665143	20068.788006	29.751335
384.915090	20104.020897	29.756352
385.573355	20146.077275	29.761370
385.356083	20177.250979	29.766388
385.958959	20211.961956	29.771405
386.286433	20252.437049	29.776423
386.762739	20285.854326	29.781440
387.647660	20320.067771	29.786458
387.703250	20357.305803	29.791476
388.141849	20388.501809	29.796493
388.548616	20420.540340	29.801511
389.015618	20454.979565	29.806528
389.598012	20488.352821	29.811546
390.138224	20510.644806	29.816564
390.542234	20546.549898	29.821581
390.719696	20570.989663	29.826599
391.031672	20598.580864	29.831616
391.606287	20630.986072	29.836634
392.052437	20660.811242	29.841652
392.733608	20677.780982	29.846669
392.875577	20704.301683	29.851687
393.595175	20730.551472	29.856704
394.352383	20747.373062	29.861722
394.860540	20763.524974	29.866740
395.425916	20774.046672	29.871757
395.453936	20796.096174	29.876775
395.644523	20799.222624	29.881792
395.927467	20820.711098	29.886810
395.978633	20831.468027	29.891828
396.737765	20848.741897	29.896845
396.987493	20871.571375	29.901863
397.188739	20908.018602	29.906880
397.623292	20928.151335	29.911898
397.743204	20956.184957	29.916916
398.398228	20980.411975	29.921933
398.632178	21015.662047	29.926951
398.793258	21038.927446	29.931968
399.221178	21072.308602	29.936986
399.154632	21108.225259	29.942004
400.153567	21127.296408	29.947021
400.607799	21165.020268	29.952039
400.786378	21204.860181	29.957056
401.355675	21229.259467	29.962074
401.970059	21262.425556	29.967092
402.243114	21286.467346	29.972109
402.469907	21323.155614	29.977127
402.857879	21354.044907	29.982144
403.474463	21385.321993	29.987162
403.691055	21411.298488	29.992180
404.373657	21435.269310	29.997197
404.757584	21470.219498	30.002215
404.984211	21492.802958	30.007232
405.588555	21519.658085	30.012250
405.772390	21556.172672	30.017268
406.190764	21591.439039	30.022285
406.348921	21638.774352	30.027303
407.131257	21659.425697	30.032320
407.342145	21685.435096	30.037338
407.913396	21724.302816	30.042356
408.364818	21758.659001	30.047373
408.861796	21788.783613	30.052391
409.116329	21823.352380	30.057408
409.845733	21847.941982	30.062426
410.148099	21884.885386	30.067444
410.364590	21906.720553	30.072461
411.017255	21941.463097	30.077479
411.210992	21971.283635	30.082496
411.889392	21993.690236	30.087514
411.840451	22023.833415	30.092532
412.345967	22062.424286	30.097549
412.644859	22098.255539	30.102567
413.120475	22131.722322	30.107584
413.448794	22164.463094	30.112602
413.587772	22206.718098	30.117620
414.704675	22222.097017	30.122637
415.590192	22258.354660	30.127655
415.849932	22285.052226	30.132672
416.461843	22294.759840	30.137690
416.745847	22332.893013	30.142708
417.107876	22365.160269	30.147725
417.073434	22390.571325	30.152743
417.252258	22418.261729	30.157760
418.178319	22448.809784	30.162778
418.578541	22487.051720	30.167796
418.666678	22519.845688	30.172813
419.203656	22551.496092	30.177831
419.577132	22591.964427	30.182848
419.730404	22623.263998	30.187866
419.823651	22663.318619	30.192884
419.922886	22701.003956	30.197901
420.758667	22743.559262	30.202919
420.827895	22788.725502	30.207936
421.628778	22814.898814	30.212954
421.677037	22854.172942	30.217972
422.347166	22886.465703	30.222989
422.581610	22932.196196	30.228007
422.749175	22972.168243	30.233024
423.398758	23008.786783	30.238042
423.639304	23070.173171	30.243060
424.229458	23093.578269	30.248077
424.905004	23133.321249	30.253095
425.177641	23174.816912	30.258112
425.944309	23204.503456	30.263130
426.333122	23240.432566	30.268148
426.431531	23277.621026	30.273165
427.042320	23324.043808	30.278183
427.483020	23356.533259	30.283200
428.055644	23402.532106	30.288218
428.226370	23426.712198	30.293236
429.186014	23464.410849	30.298253
429.597471	23503.709724	30.303271
429.507445	23541.832042	30.308288
430.426362	23571.981203	30.313306
430.789509	23621.437310	30.318324
431.293572	23651.310176	30.323341
431.833918	23691.169954	30.328359
431.935600	23732.025182	30.333376
432.504735	23751.252699	30.338394
432.822749	23789.137489	30.343412
433.543092	23823.948343	30.348429
433.998315	23859.839346	30.353447
434.165763	23907.512167	30.358464
434.787470	23945.099282	30.363482
434.831522	23986.925045	30.368500
435.319351	24027.368339	30.373517
435.853839	24071.178644	30.378535
435.900746	24118.895729	30.383552
436.604494	24158.442455	30.388570
436.925617	24199.768555	30.393588
437.273075	24247.801935	30.398605
437.862225	24291.799270	30.403623
438.148037	24332.522847	30.408640
438.734182	24375.174163	30.413658
439.150888	24425.713393	30.418676
439.838777	24461.377777	30.423693
440.565065	24500.798548	30.428711
440.966130	24543.758576	30.433728
441.547959	24573.331551	30.438746
441.717539	24621.458604	30.443764
441.860815	24658.522765	30.448781
442.531476	24699.397766	30.453799
443.118201	24748.856271	30.458816
443.554983	24774.583706	30.463834
443.922858	24819.798758	30.468852
443.976181	24865.939842	30.473869
444.518438	24894.513807	30.478887
444.836977	24945.367355	30.483904
446.137949	24990.254403	30.488922
446.281208	25037.406081	30.493940
446.115270	25072.894994	30.498957
446.992311	25115.559769	30.503975
447.334973	25151.260853	30.508992
447.864456	25200.802715	30.514010
448.079718	25249.482218	30.519028
448.686729	25281.326348	30.524045
449.374461	25329.104379	30.529063
449.462063	25374.074108	30.534080
449.761017	25396.194961	30.539098
450.642753	25457.475535	30.544116
450.598927	25487.680749	30.549133
451.315980	25520.737167	30.554151
451.453584	25566.569643	30.559168
451.680965	25603.918366	30.564186
452.334452	25656.831686	30.569204
453.125600	25702.625369	30.574221
453.894145	25739.729950	30.579239
454.615973	25762.061764	30.584256
455.137866	25787.224598	30.589274
455.594214	25827.734147	30.594292
456.331558	25849.874246	30.599309
456.801784	25863.296306	30.604327
457.115076	25905.857965	30.609344
457.598571	25942.757991	30.614362
458.081703	25968.876954	30.619380
458.082550	26005.942443	30.624397
458.412714	26036.673193	30.629415
458.703108	26077.696649	30.634432
459.369073	26109.674468	30.639450
459.587136	26148.069982	30.644468
459.723261	26200.465282	30.649485
460.250866	26236.314543	30.654503
460.747501	26285.089030	30.659520
461.148083	26329.021973	30.664538
460.997318	26378.058808	30.669556
461.670210	26432.280331	30.674573
462.333885	26483.071638	30.679591
462.716443	26539.155461	30.684608
463.071185	26597.953677	30.689626
463.645354	26646.441879	30.694644
464.119756	26704.015615	30.699661
464.746587	26745.833307	30.704679
464.901599	26800.432203	30.709696
465.621551	26845.477387	30.714714
466.365940	26893.253505	30.719732
466.616849	26941.285208	30.724749
467.499047	26988.442516	30.729767
467.811924	27048.908448	30.734784
468.556735	27082.811803	30.739802
469.056398	27144.120827	30.744820
469.494949	27179.889050	30.749837
470.173972	27224.878933	30.754855
470.604166	27265.490835	30.759872
471.277785	27301.592497	30.764890
471.922169	27328.992696	30.769908
472.317191	27373.572733	30.774925
472.812411	27406.190133	30.779943
473.582546	27426.983000	30.784960
474.262631	27457.617154	30.789978
474.458815	27492.476769	30.794996
474.475959	27537.422820	30.800013
474.997553	27568.086647	30.805031
475.286062	27615.688113	30.810048
475.903535	27648.922883	30.815066
476.580874	27687.245535	30.820084
476.960427	27738.677620	30.825101
477.619926	27758.697467	30.830119
477.635714	27806.496169	30.835136
478.096472	27859.265283	30.840154
478.633932	27882.671485	30.845172
479.276490	27935.233979	30.850189
479.804601	27965.947902	30.855207
480.302428	28006.944634	30.860224
480.768988	28041.993888	30.865242
481.252677	28089.728277	30.870260
481.695736	28143.305624	30.875277
482.217677	28175.396364	30.880295
482.227933	28212.739461	30.885312
482.666971	28257.405942	30.890330
483.200440	28292.630714	30.895348
483.312095	28338.553703	30.900365
483.807705	28376.381229	30.905383
483.843413	28431.841058	30.910400
484.547526	28482.817640	30.915418
485.183196	28521.745293	30.920436
485.374488	28574.895730	30.925453
485.967988	28619.127373	30.930471
486.246182	28677.601483	30.935488
486.817829	28735.629554	30.940506
487.486954	28786.628610	30.945524
487.984940	28846.902851	30.950541
488.336929	28896.554183	30.955559
489.012941	28947.028872	30.960576
489.383716	28991.531904	30.965594
490.126404	29054.192256	30.970612
490.663590	29102.665068	30.975629
491.179584	29149.081438	30.980647
491.748625	29201.984912	30.985664
492.115844	29245.659463	30.990682
492.864548	29298.744766	30.995700
493.075507	29355.964064	31.000717
493.717591	29405.026027	31.005735
493.979614	29453.375149	31.010752
494.362029	29516.185327	31.015770
495.087221	29562.760500	31.020788
495.187302	29617.771713	31.025805
496.039226	29673.999072	31.030823
496.307847	29729.761909	31.035840
497.109069	29774.999953	31.040858
497.974185	29835.844462	31.045876
498.634812	29885.583006	31.050893
499.256417	29924.831621	31.055911
500.041063	29969.978274	31.060928
500.319008	30013.701116	31.065946
501.069635	30056.108812	31.070964
501.559866	30099.938588	31.075981
501.917876	30140.515545	31.080999
502.183555	30177.599564	31.086016
502.312697	30228.348609	31.091034
503.402371	30275.858978	31.096052
503.662116	30326.409935	31.101069
504.031769	30368.036109	31.106087
504.321270	30419.011475	31.111104
505.003859	30464.737950	31.116122
505.511571	30516.589172	31.121140
505.948364	30565.559121	31.126157
506.784514	30618.308930	31.131175
506.803194	30675.312054	31.136192
507.231062	30731.581681	31.141210
507.739133	30766.295065	31.146228
508.261704	30833.813035	31.151245
509.019154	30872.807732	31.156263
509.693212	30931.810471	31.161280
510.284860	30987.611996	31.166298
510.803671	31025.709585	31.171316
511.588158	31068.309724	31.176333
512.090593	31109.827257	31.181351
512.902611	31156.714072	31.186368
513.175391	31196.004529	31.191386
513.753229	31227.239688	31.196404
513.932190	31263.523202	31.201421
514.263029	31314.494295	31.206439
515.121769	31361.029978	31.211456
515.519701	31407.919970	31.216474
516.259609	31447.357431	31.221492
516.340749	31501.711923	31.226509
516.970350	31542.366907	31.231527
517.628024	31582.809076	31.236544
517.557975	31627.338357	31.241562
518.124691	31658.522488	31.246580
518.535675	31715.031546	31.251597
518.254217	31763.685521	31.256615
519.155969	31816.948650	31.261632
519.623418	31881.968168	31.266650
520.373364	31934.332356	31.271668
520.822904	31991.040988	31.276685
521.273686	32044.433336	31.281703
521.871298	32091.427660	31.286720
522.168216	32159.325796	31.291738
523.325786	32205.899274	31.296756
523.950997	32258.998251	31.301773
525.097750	32290.680382	31.306791
525.701417	32324.529006	31.311808
526.127666	32369.119723	31.316826
526.958609	32411.718548	31.321844
527.359211	32460.198055	31.326861
527.803074	32497.273136	31.331879
528.565901	32530.499348	31.336896
528.731369	32575.597740	31.341914
529.159811	32616.717740	31.346932
529.455518	32654.054410	31.351949
529.902450	32707.408375	31.356967
530.621671	32750.982673	31.361984
530.807336	32815.471807	31.367002
531.417569	32864.797984	31.372020
531.669461	32917.900976	31.377037
533.136985	32939.098947	31.382055
534.059240	32980.910882	31.387072
534.364966	33015.059589	31.392090
535.388849	33040.250501	31.397108
536.579388	33068.159074	31.402125
537.548025	33098.818295	31.407143
538.234027	33096.789061	31.412160
538.636807	33131.631869	31.417178
539.477052	33141.867813	31.422196
539.701527	33152.041934	31.427213
540.018888	33163.626938	31.432231
540.596326	33187.472209	31.437248
540.557620	33213.092271	31.442266
541.231257	33241.156382	31.447284
541.418964	33271.746788	31.452301
541.680473	33306.471400	31.457319
542.201130	33345.921107	31.462336
542.766250	33386.524770	31.467354
543.125290	33410.674833	31.472372
543.653775	33449.451331	31.477389
543.896998	33489.048407	31.482407
544.746745	33523.738868	31.487424
545.058094	33572.558105	31.492442
545.189945	33616.393008	31.497460
545.485234	33669.582550	31.502477
545.808970	33726.948745	31.507495
546.201208	33779.551346	31.512512
546.167230	33840.492697	31.517530
547.022513	33904.669458	31.522548
547.146230	33970.413237	31.527565
547.287338	34044.788341	31.532583
548.043847	34104.179258	31.537600
548.400858	34195.471578	31.542618
549.093638	34263.902122	31.547636
549.825087	34328.375518	31.552653
550.149899	34407.445769	31.557671
550.984756	34486.791426	31.562688
551.371048	34552.578944	31.567706
552.729699	34616.337001	31.572724
553.367314	34677.655666	31.577741
553.701679	34727.089613	31.582759
554.092254	34776.814165	31.587776
554.447190	34832.301008	31.592794
555.414936	34892.587279	31.597812
555.857696	34956.852099	31.602829
555.995614	35024.572949	31.607847
557.001374	35086.059099	31.612864
557.410105	35146.303351	31.617882
557.608220	35208.596242	31.622900
558.105262	35286.944314	31.627917
558.588449	35358.175263	31.632935
559.298944	35409.738840	31.637952
559.885130	35481.454967	31.642970
560.352593	35548.564462	31.647988
561.087546	35610.526589	31.653005
561.498688	35688.379406	31.658023
562.389399	35749.643923	31.663040
563.051274	35819.792926	31.668058
563.888844	35878.522967	31.673076
564.482580	35942.501133	31.678093
565.120179	36020.532389	31.683111
565.577870	36064.934589	31.688128
566.209046	36130.340049	31.693146
566.595942	36195.114068	31.698164
567.361874	36254.750400	31.703181
568.115246	36323.838352	31.708199
568.749944	36370.825156	31.713216
568.952045	36443.397916	31.718234
569.778834	36506.531417	31.723252
570.211722	36562.815458	31.728269
570.896537	36623.018801	31.733287
571.844336	36674.865364	31.738304
572.271973	36731.927218	31.743322
572.728948	36804.923060	31.748340
573.222720	36859.389426	31.753357
574.314122	36919.081217	31.758375
574.846176	36975.618352	31.763392
575.277978	37047.309526	31.768410
575.753556	37096.445619	31.773428
576.700316	37153.905502	31.778445
576.846893	37220.364341	31.783463
577.854697	37261.704947	31.788480
578.207389	37321.637514	31.793498
578.622054	37380.966609	31.798516
579.384937	37440.840925	31.803533
579.626613	37502.840955	31.808551
580.395056	37570.113136	31.813568
580.778546	37634.671928	31.818586
581.003581	37696.328186	31.823604
581.894854	37763.621720	31.828621
581.915951	37834.733995	31.833639
582.799157	37890.454990	31.838656
583.636746	37961.779380	31.843674
584.093785	38024.029499	31.848692
584.839049	38078.208407	31.853709
585.241335	38144.820702	31.858727
586.299684	38207.271457	31.863744
586.618059	38277.054588	31.868762
587.780598	38327.838073	31.873780
588.654336	38386.131502	31.878797
589.041973	38446.516501	31.883815
589.717544	38495.771522	31.888832
590.216645	38561.258186	31.893850
590.572878	38601.971426	31.898868
591.197849	38667.191364	31.903885
591.324239	38723.043735	31.908903
592.100090	38774.388249	31.913920
592.352513	38835.636621	31.918938
592.668101	38896.720039	31.923956
593.413784	38956.078212	31.928973
593.911952	39021.241555	31.933991
594.544018	39065.508505	31.939008
595.132543	39130.695113	31.944026
596.102892	39199.404438	31.949044
596.390945	39252.532697	31.954061
596.878283	39327.408631	31.959079
597.374088	39377.636552	31.964096
598.468514	39440.192865	31.969114
599.322105	39492.195694	31.974132
600.389919	39545.564652	31.979149
600.422691	39608.746073	31.984167
600.952214	39663.824125	31.989184
601.847665	39713.936101	31.994202
602.040876	39787.274944	31.999220
602.763369	39843.012808	32.004237
603.404077	39912.265677	32.009255
603.685173	39961.577523	32.014272
604.271565	40033.882950	32.019290
604.721702	40110.681239	32.024308
605.455444	40175.916900	32.029325
606.298105	40241.343053	32.034343
606.989755	40305.336082	32.039360
607.647188	40366.531785	32.044378
607.872912	40442.869951	32.049396
608.601791	40513.101680	32.054413
609.172814	40586.993398	32.059431
609.383712	40657.037040	32.064448
609.966147	40731.378870	32.069466
610.515771	40804.148015	32.074484
611.421708	40874.727389	32.079501
612.017096	40954.541995	32.084519
612.867479	41018.069178	32.089536
613.230185	41087.085350	32.094554
613.902369	41174.388984	32.099572
614.771304	41244.177213	32.104589
615.629482	41302.788727	32.109607
616.517747	41360.880847	32.114624
617.393572	41427.442213	32.119642
617.791090	41500.296183	32.124660
618.308813	41561.042343	32.129677
618.603230	41615.300253	32.134695
619.293467	41682.477398	32.139712
620.522640	41747.080721	32.144730
621.156282	41806.381463	32.149748
622.069581	41851.997523	32.154765
622.632020	41924.273295	32.159783
623.266877	41970.081104	32.164800
623.836390	42030.845463	32.169818
624.109393	42092.476939	32.174836
625.072685	42137.959121	32.179853
625.319421	42207.753272	32.184871
625.591993	42269.723218	32.189888
626.395220	42322.515897	32.194906
626.501873	42396.501420	32.199924
627.646947	42464.445676	32.204941
628.198959	42542.004337	32.209959
628.519719	42600.005145	32.214976
629.408294	42667.967478	32.219994
630.019411	42743.395538	32.225012
630.567984	42816.589513	32.230029
630.803787	42885.545046	32.235047
631.425281	42953.249675	32.240064
631.942096	43043.887211	32.245082
631.996345	43119.295593	32.250100
632.847290	43180.859970	32.255117
633.324696	43258.184575	32.260135
633.912287	43342.276235	32.265152
634.618500	43414.597069	32.270170
634.533874	43503.701214	32.275188
635.481909	43588.858143	32.280205
636.088194	43671.805225	32.285223
636.826579	43754.367645	32.290240
637.611570	43840.632612	32.295258
638.000172	43925.962899	32.300276
638.863133	44008.846756	32.305293
639.252929	44096.845634	32.310311
639.944774	44187.620681	32.315328
640.541604	44269.100612	32.320346
641.150896	44362.226727	32.325364
642.211085	44445.322892	32.330381
642.575971	44533.362685	32.335399
643.277170	44611.745058	32.340416
644.264152	44694.071418	32.345434
644.811766	44786.698359	32.350452
645.660425	44862.224981	32.355469
646.328519	44952.590873	32.360487
647.298977	45027.220132	32.365504
648.664534	45096.321452	32.370522
649.184568	45176.103496	32.375540
649.875615	45239.068433	32.380557
650.601075	45307.433725	32.385575
651.613852	45382.073154	32.390592
652.209772	45448.540621	32.395610
652.560513	45525.927179	32.400628
653.227893	45586.895251	32.405645
653.327581	45673.550822	32.410663
653.761127	45742.313504	32.415680
654.900261	45818.926192	32.420698
655.210210	45892.440195	32.425716
655.982710	45979.875940	32.430733
657.065051	46046.024761	32.435751
657.392756	46129.243664	32.440768
658.016451	46200.654227	32.445786
658.422587	46282.676616	32.450804
659.226536	46360.528166	32.455821
659.660968	46437.244576	32.460839
660.608866	46531.477789	32.465856
662.004321	46589.820895	32.470874
662.545930	46673.426666	32.475892
663.308632	46736.125753	32.480909
664.173624	46806.560652	32.485927
664.575313	46887.035876	32.490944
665.268024	46946.308337	32.495962
665.659282	47024.692188	32.500980
666.546745	47095.304429	32.505997
667.324869	47167.274051	32.511015
668.280622	47226.500556	32.516032
669.392975	47274.799983	32.521050
670.288856	47340.362169	32.526068
670.851262	47389.466896	32.531085
671.495148	47457.221904	32.536103
671.993158	47514.229451	32.541120
672.523112	47572.071894	32.546138
672.919317	47650.182755	32.551156
673.426146	47697.352165	32.556173
674.283508	47780.550366	32.561191
674.382244	47853.813331	32.566208
675.116861	47915.835678	32.571226
675.595726	47994.196342	32.576244
676.450673	48067.966192	32.581261
676.777529	48148.064407	32.586279
677.268897	48233.545492	32.591296
677.641669	48306.259395	32.596314
678.302953	48379.667836	32.601332
678.937201	48461.434355	32.606349
679.968140	48548.002094	32.611367
680.233857	48616.202982	32.616384
681.268633	48682.103596	32.621402
681.711334	48754.384394	32.626420
682.602810	48828.808021	32.631437
683.373031	48918.790535	32.636455
683.653036	48993.328953	32.641472
684.251876	49074.428104	32.646490
684.872837	49166.454683	32.651508
685.450291	49254.705305	32.656525
686.562876	49342.643249	32.661543
686.519276	49431.920017	32.666560
687.463347	49515.420878	32.671578
687.979666	49619.582334	32.676596
688.955960	49707.348757	32.681613
689.758564	49806.186081	32.686631
690.142545	49902.092946	32.691648
690.804258	49977.332974	32.696666
691.996045	50081.533229	32.701684
692.544909	50158.791979	32.706701
693.286750	50247.089342	32.711719
693.915266	50358.421623	32.716736
694.896078	50443.237486	32.721754
695.047198	50530.841441	32.726772
696.176528	50617.335838	32.731789
696.647028	50717.268954	32.736807
697.083059	50824.826700	32.741824
698.110977	50911.042345	32.746842
699.275741	51004.475089	32.751860
700.196929	51085.996651	32.756877
700.755822	51183.757029	32.761895
701.241369	51267.790117	32.766912
702.351843	51344.233882	32.771930
703.554303	51420.567918	32.776948
704.234410	51509.756233	32.781965
704.923659	51595.329928	32.786983
705.417494	51674.821245	32.792000
706.129596	51752.956318	32.797018
706.797752	51831.332744	32.802036
707.376604	51921.114640	32.807053
708.181289	52012.154538	32.812071
708.460029	52099.877049	32.817088
709.209484	52178.039215	32.822106
709.989251	52272.792849	32.827124
710.737907	52365.606295	32.832141
711.948658	52448.822837	32.837159
712.110802	52530.950295	32.842176
713.144163	52622.182512	32.847194
713.872576	52710.515422	32.852212
714.738924	52793.879060	32.857229
715.407528	52866.358829	32.862247
716.163686	52962.395913	32.867264
716.764898	53038.501272	32.872282
717.425049	53132.116460	32.877300
718.244828	53213.158340	32.882317
718.757151	53302.439568	32.887335
718.991090	53387.566010	32.892352
719.799788	53471.340133	32.897370
720.332055	53574.221800	32.902388
721.245808	53661.125641	32.907405
721.999315	53759.466820	32.912423
721.915405	53871.449208	32.917440
723.105256	53972.555824	32.922458
723.939780	54072.559415	32.927476
724.643983	54165.995311	32.932493
724.911362	54264.748265	32.937511
725.330475	54354.422517	32.942528
726.014132	54453.416900	32.947546
726.959216	54553.663627	32.952564
727.455584	54651.976133	32.957581
728.267219	54743.204477	32.962599
728.512203	54858.151711	32.967616
729.689321	54950.489237	32.972634
730.850130	55062.271741	32.977652
731.283732	55163.920715	32.982669
732.616375	55244.513030	32.987687
733.320811	55351.090664	32.992704
734.081651	55442.893020	32.997722
734.867681	55525.156864	33.002740
735.609542	55630.535575	33.007757
737.008222	55714.429802	33.012775
737.414859	55803.872588	33.017792
738.435591	55889.075079	33.022810
739.280761	55990.988542	33.027828
739.778743	56073.807980	33.032845
740.549712	56160.386357	33.037863
741.196890	56259.427421	33.042880
741.910476	56340.531371	33.047898
742.691061	56443.260368	33.052916
743.381834	56536.071474	33.057933
744.079878	56625.867671	33.062951
744.773628	56729.370831	33.067968
745.626448	56819.426560	33.072986
746.680439	56911.572494	33.078004
747.113612	57013.464800	33.083021
748.119780	57096.204125	33.088039
748.954524	57188.090735	33.093056
750.394562	57255.080971	33.098074
751.424264	57344.894858	33.103092
752.028057	57428.182613	33.108109
753.186328	57499.290006	33.113127
753.540976	57584.092147	33.118144
754.765009	57644.016722	33.123162
755.784829	57701.668840	33.128180
756.281484	57784.343935	33.133197
756.988512	57851.502093	33.138215
757.723839	57932.722650	33.143232
758.112914	58000.566024	33.148250
758.561560	58085.304126	33.153268
758.997958	58180.446397	33.158285
760.107601	58262.617260	33.163303
760.116743	58360.434925	33.168320
760.899660	58448.259851	33.173338
761.595990	58549.092515	33.178356
762.036974	58643.218766	33.183373
762.810043	58749.499808	33.188391
763.111707	58854.001691	33.193408
763.877932	58963.463777	33.198426
764.542992	59076.671880	33.203444
765.033497	59188.544528	33.208461
765.798380	59296.536142	33.213479
766.689358	59416.445532	33.218496
767.791135	59522.296888	33.223514
768.787132	59629.929605	33.228532
769.329163	59750.764726	33.233549
769.988927	59848.841825	33.238567
770.758822	59960.476443	33.243584
771.409143	60072.870967	33.248602
772.382921	60185.256660	33.253620
773.083160	60298.484715	33.258637
774.150970	60397.811311	33.263655
775.195644	60502.773492	33.268672
775.943821	60588.654235	33.273690
777.783214	60677.463742	33.278708
779.194632	60750.152244	33.283725
780.102298	60816.585413	33.288743
781.077477	60882.306044	33.293760
781.773201	60948.370329	33.298778
782.770850	61005.334023	33.303796
782.847299	61078.763567	33.308813
783.862623	61139.188245	33.313831
784.566525	61219.915277	33.318848
785.041764	61303.196105	33.323866
785.763596	61371.640221	33.328884
786.331396	61456.088227	33.333901
786.930303	61532.276879	33.338919
787.766204	61623.854814	33.343936
788.420085	61705.856170	33.348954
788.946780	61786.374675	33.353972
789.886151	61888.517227	33.358989
790.498141	61968.579850	33.364007
791.766957	62067.786414	33.369024
791.886982	62157.425040	33.374042
792.252813	62252.945746	33.379060
793.044287	62357.333749	33.384077
793.832309	62464.718897	33.389095
795.456503	62552.769564	33.394112
796.503394	62640.676248	33.399130
797.287399	62725.700397	33.404148
797.915591	62826.211608	33.409165
798.421455	62923.147022	33.414183
799.021163	63018.512366	33.419200
799.588842	63135.855136	33.424218
800.339036	63234.698316	33.429236
801.117919	63352.310668	33.434253
802.127039	63444.873017	33.439271
802.758475	63550.899189	33.444288
803.419591	63659.632741	33.449306
804.404994	63770.076640	33.454324
805.140466	63878.305950	33.459341
805.944167	63989.868429	33.464359
806.575898	64097.553515	33.469376
807.076453	64224.977059	33.474394
808.065791	64328.855457	33.479412
808.591822	64453.362040	33.484429
809.799425	64562.673365	33.489447
810.834961	64686.812313	33.494464
811.408915	64801.919373	33.499482
812.330359	64905.679176	33.504500
812.767489	65028.762659	33.509517
813.512741	65153.274973	33.514535
814.704985	65269.438838	33.519552
815.040851	65403.894970	33.524570
815.980009	65509.968570	33.529588
816.978415	65638.595111	33.534605
817.672264	65747.428980	33.539623
819.060486	65863.810174	33.544640
820.103526	65978.757361	33.549658
821.106393	66089.785970	33.554676
821.800248	66190.802001	33.559693
823.153246	66297.411488	33.564711
823.725468	66405.137341	33.569728
824.493742	66507.173024	33.574746
825.278981	66617.589388	33.579764
826.438567	66729.935646	33.584781
826.713316	66830.480625	33.589799
827.902039	66938.056306	33.594816
828.343635	67050.770017	33.599834
829.523564	67156.009077	33.604852
830.483766	67274.176138	33.609869
830.879805	67369.045171	33.614887
831.719381	67475.107311	33.619904
831.889094	67586.490757	33.624922
833.063191	67677.407031	33.629940
833.850295	67783.947286	33.634957
834.572271	67901.329171	33.639975
835.735167	68002.048439	33.644992
835.859081	68107.789973	33.650010
836.820280	68216.668116	33.655028
837.159232	68346.697830	33.660045
838.152566	68453.782578	33.665063
839.057388	68581.058001	33.670080
840.059352	68697.329304	33.675098
841.256799	68792.166537	33.680116
842.598425	68896.584449	33.685133
843.989631	68988.146851	33.690151
845.223014	69082.505213	33.695168
845.861042	69182.349828	33.700186
847.142911	69269.676356	33.705204
848.394940	69362.224541	33.710221
849.389559	69440.108862	33.715239
850.133921	69532.489136	33.720256
850.878255	69626.678169	33.725274
851.817549	69717.041491	33.730292
852.212792	69803.126321	33.735309
852.823675	69895.656781	33.740327
853.480740	69995.192215	33.745344
853.526557	70109.195563	33.750362
854.262756	70213.176637	33.755380
854.835160	70342.579089	33.760397
855.229670	70461.793606	33.765415
856.034443	70583.027348	33.770432
856.971899	70708.071637	33.775450
857.617337	70850.377089	33.780468
858.639895	70974.359139	33.785485
859.560775	71112.542070	33.790503
861.047644	71221.183896	33.795520
861.853493	71349.959271	33.800538
863.140300	71470.175822	33.805556
863.777683	71580.718382	33.810573
864.642587	71714.620814	33.815591
865.854030	71825.189494	33.820608
866.433248	71958.103788	33.825626
867.239370	72078.188507	33.830644
868.346488	72190.338312	33.835661
869.209532	72319.577931	33.840679
870.010102	72438.495685	33.845696
870.499999	72564.971984	33.850714
871.124938	72689.137385	33.855732
871.860805	72836.006711	33.860749
872.202846	72962.136756	33.865767
873.070909	73101.251806	33.870784
873.403607	73250.024785	33.875802
874.130488	73394.363455	33.880820
875.591083	73544.633438	33.885837
876.611161	73687.926188	33.890855
877.582661	73834.250886	33.895872
878.512579	73993.813684	33.900890
879.143051	74135.257800	33.905908
880.060097	74279.128061	33.910925
880.626143	74425.207792	33.915943
881.844483	74560.896821	33.920960
882.506317	74710.706579	33.925978
883.627485	74863.843677	33.930996
884.324342	75005.737750	33.936013
885.430195	75155.691882	33.941031
886.400790	75296.916274	33.946048
886.966292	75450.902308	33.951066
888.227119	75589.202704	33.956084
889.756246	75721.798836	33.961101
890.050092	75847.074351	33.966119
891.460108	75967.453378	33.971136
892.153088	76100.873636	33.976154
893.044129	76221.523600	33.981172
894.158716	76348.259598	33.986189
894.889892	76482.732074	33.991207
895.835953	76598.637603	33.996224
896.562259	76733.137704	34.001242
897.223259	76869.110540	34.006260
898.525392	76995.218235	34.011277
899.463225	77123.145483	34.016295
901.107994	77236.130040	34.021312
902.084447	77355.829555	34.026330
902.837781	77470.234605	34.031348
904.269721	77580.624954	34.036365
905.205246	77709.542693	34.041383
906.552633	77820.972960	34.046400
907.746569	77934.086486	34.051418
908.046761	78038.284679	34.056436
908.971437	78147.016223	34.061453
909.772168	78252.574532	34.066471
911.287399	78358.046386	34.071488
912.203809	78466.685976	34.076506
913.485769	78572.324065	34.081524
914.066250	78687.295377	34.086541
914.610592	78795.713661	34.091559
915.347016	78908.142648	34.096576
916.356546	79024.290624	34.101594
916.777239	79137.247578	34.106612
917.679286	79266.420212	34.111629
918.494430	79394.716080	34.116647
919.523236	79524.115859	34.121664
919.976668	79655.041503	34.126682
920.681402	79785.590930	34.131700
921.354216	79915.039379	34.136717
922.179530	80069.102726	34.141735
923.194797	80204.005878	34.146752
924.040904	80360.041455	34.151770
924.379007	80492.667478	34.156788
925.284921	80649.833811	34.161805
926.065051	80807.553503	34.166823
927.180906	80958.677311	34.171840
927.909289	81109.164217	34.176858
928.824306	81269.863356	34.181876
929.668449	81424.603362	34.186893
930.822213	81576.288020	34.191911
932.286118	81728.624447	34.196928
933.451680	81885.199500	34.201946
934.300493	82030.984620	34.206964
935.942318	82165.485430	34.211981
936.434647	82323.219082	34.216999
937.422412	82470.483335	34.222016
938.467970	82615.530947	34.227034
938.761637	82764.145965	34.232052
939.874158	82918.067026	34.237069
940.189096	83079.131526	34.242087
941.324551	83230.343018	34.247104
941.987416	83392.788155	34.252122
942.979162	83555.053320	34.257140
943.883941	83709.476008	34.262157
944.945670	83864.038183	34.267175
946.264138	84023.025660	34.272192
947.470457	84180.463731	34.277210
948.384808	84336.597325	34.282228
949.199294	84480.246107	34.287245
950.234734	84644.915980	34.292263
951.392812	84786.788646	34.297280
952.405130	84928.869858	34.302298
953.289872	85058.337490	34.307316
954.573472	85193.086251	34.312333
955.423625	85335.108272	34.317351
956.088192	85473.941304	34.322368
957.660274	85589.731860	34.327386
958.743582	85721.517707	34.332404
960.653401	85820.915821	34.337421
961.868488	85941.867340	34.342439
963.106572	86057.291699	34.347456
963.746130	86175.941788	34.352474
964.356402	86293.648191	34.357492
965.176379	86421.425669	34.362509
966.003008	86550.822631	34.367527
966.893324	86661.397381	34.372544
967.655910	86799.766413	34.377562
968.533578	86930.802218	34.382580
969.397325	87056.354827	34.387597
970.448290	87192.912848	34.392615
971.649259	87314.715395	34.397632
972.669201	87445.293828	34.402650
973.231285	87582.903411	34.407668
974.306067	87704.235327	34.412685
974.785104	87859.585069	34.417703
975.859290	88004.098295	34.422720
976.718402	88140.421524	34.427738
977.467670	88294.564899	34.432756
978.290975	88437.590982	34.437773
979.722612	88594.356857	34.442791
980.503602	88738.897899	34.447808
981.661332	88893.983580	34.452826
982.670873	89035.463557	34.457844
984.223115	89179.803355	34.462861
985.028687	89338.544902	34.467879
985.906600	89471.448951	34.472896
987.199810	89604.550622	34.477914
988.106983	89753.361281	34.482932
989.177149	89892.260554	34.487949
990.138565	90045.551001	34.492967
991.019662	90181.686070	34.497984
992.063947	90333.243207	34.503002
992.833460	90485.024101	34.508020
993.744621	90634.573700	34.513037
994.918484	90785.555254	34.518055
995.597319	90920.348384	34.523072
996.626094	91078.317600	34.528090
997.458443	91239.681115	34.533108
998.363213	91396.875544	34.538125
999.117590	91559.950305	34.543143
1000.217420	91725.943505	34.548160
1001.785194	91878.898165	34.553178
1002.319367	92046.803883	34.558196
1003.454194	92206.098316	34.563213
1004.142024	92374.417515	34.568231
1004.562978	92545.054376	34.573248
1005.654198	92715.828055	34.578266
1006.448625	92890.361194	34.583284
1008.032568	93052.877922	34.588301
1008.707643	93233.509562	34.593319
1009.949657	93399.148793	34.598336
1011.120327	93563.655335	34.603354
1011.799846	93744.144426	34.608372
1013.264494	93899.439186	34.613389
1014.323174	94073.000124	34.618407
1015.199115	94236.553665	34.623424
1016.288313	94407.788894	34.628442
1017.107613	94576.284981	34.633460
1018.380536	94740.212752	34.638477
1019.574114	94893.982638	34.643495
1020.581744	95040.194749	34.648512
1022.042922	95179.730312	34.653530
1022.881216	95324.623920	34.658548
1024.194422	95467.641843	34.663565
1025.457854	95620.891926	34.668583
1027.134547	95738.499148	34.673600
1028.131946	95875.779779	34.678618
1029.028566	96015.337766	34.683636
1030.263276	96148.725450	34.688653
1030.908456	96281.420388	34.693671
1031.986206	96416.829582	34.698688
1033.405185	96548.694888	34.703706
1034.081943	96692.521801	34.708724
1034.961863	96839.974796	34.713741
1035.796032	96973.768867	34.718759
1036.680935	97127.306266	34.723776
1037.751067	97277.363750	34.728794
1038.267610	97433.749566	34.733812
1039.446766	97595.192164	34.738829
1039.696060	97752.295348	34.743847
1040.230053	97927.274372	34.748864
1041.352324	98102.834388	34.753882
1041.745791	98288.550794	34.758900
1043.011575	98462.095311	34.763917
1044.201768	98653.658479	34.768935
1044.827052	98845.595389	34.773952
1046.026331	99038.476788	34.778970
1047.406268	99231.943785	34.783988
1048.716782	99407.405652	34.789005
1049.482718	99594.715899	34.794023
1050.476331	99775.778915	34.799040
1052.033593	99957.636060	34.804058
1052.725973	100155.801601	34.809076
1054.085725	100338.770542	34.814093
1055.469551	100534.310781	34.819111
1056.482658	100719.549591	34.824128
1057.331794	100901.037097	34.829146
1058.415505	101095.327145	34.834164
1059.481004	101278.446592	34.839181
1060.773520	101470.127910	34.844199
1061.700588	101660.642961	34.849216
1063.213041	101835.100245	34.854234
1064.094608	102017.666622	34.859252
1065.226403	102217.535363	34.864269
1066.268569	102395.385953	34.869287
1067.718402	102564.482879	34.874304
1069.097965	102742.482490	34.879322
1070.146232	102922.507510	34.884340
1071.267537	103097.481433	34.889357
1072.946141	103261.992283	34.894375
1073.843968	103437.480470	34.899392
1075.115549	103594.088934	34.904410
1075.984748	103770.508591	34.909428
1077.173447	103941.190163	34.914445
1078.126840	104115.217290	34.919463
1078.739848	104290.581158	34.924480
1079.991973	104470.323407	34.929498
1080.343860	104653.686359	34.934516
1081.336237	104840.313138	34.939533
1082.310459	105016.799739	34.944551
1083.094620	105215.241994	34.949568
1084.283528	105406.690834	34.954586
1085.270755	105613.663928	34.959604
1086.180347	105795.004519	34.964621
1087.003510	105998.651570	34.969639
1088.084201	106196.418719	34.974656
1089.222760	106382.804154	34.979674
1090.311119	106578.913703	34.984692
1090.931781	106771.935880	34.989709
1092.032030	106964.955879	34.994727
1092.804562	107160.590143	34.999744
1094.239283	107355.064703	35.004762
1095.261743	107555.562101	35.009780
1096.182452	107745.641008	35.014797
1097.835899	107945.973309	35.019815
1098.857865	108151.744383	35.024832
1100.270865	108349.890319	35.029850
1101.153980	108552.102901	35.034868
1102.530735	108741.087193	35.039885
1103.956879	108929.469281	35.044903
1105.377219	109117.688977	35.049920
1106.459449	109310.931478	35.054938
1107.845354	109492.699405	35.059956
1108.886152	109671.650395	35.064973
1110.197253	109865.492222	35.069991
1111.355016	110053.660636	35.075008
1112.483010	110238.060441	35.080026
1113.366841	110424.959467	35.085044
1114.363073	110614.273273	35.090061
1116.476333	110782.704329	35.095079
1118.278815	110945.348219	35.100096
1119.360645	111107.365242	35.105114
1120.524840	111285.495604	35.110132
1121.649271	111465.863257	35.115149
1122.528645	111620.569548	35.120167
1123.669811	111807.663325	35.125184
1124.739440	111973.399195	35.130202
1125.661695	112148.281576	35.135220
1126.372456	112328.229439	35.140237
1128.286439	112497.160117	35.145255
1129.075870	112666.937145	35.150272
1130.540303	112843.456870	35.155290
1131.486012	113023.256248	35.160308
1132.727206	113201.652224	35.165325
1134.032655	113384.181353	35.170343
1134.733880	113557.082282	35.175360
1135.520128	113737.267447	35.180378
1136.691238	113915.856981	35.185396
1137.652650	114117.134689	35.190413
1138.851831	114293.618914	35.195431
1139.398092	114496.551856	35.200448
1140.140830	114695.969607	35.205466
1141.245519	114905.920342	35.210484
1142.193268	115099.732404	35.215501
1143.797375	115305.941783	35.220519
1144.423753	115526.352870	35.225536
1145.361207	115738.922152	35.230554
1146.174830	115949.625760	35.235572
1147.202272	116183.544848	35.240589
1148.233200	116410.268678	35.245607
1149.178818	116636.881763	35.250624
1150.408329	116863.994372	35.255642
1151.354611	117091.789290	35.260660
1152.839601	117324.640866	35.265677
1154.237677	117551.401532	35.270695
1155.178750	117776.947393	35.275712
1157.081881	117994.948362	35.280730
1158.754448	118219.932869	35.285748
1159.587777	118431.044263	35.290765
1160.750733	118646.499373	35.295783
1161.649843	118873.403895	35.300800
1162.662223	119090.154398	35.305818
1163.843121	119329.129455	35.310836
1164.635254	119548.834326	35.315853
1165.653479	119763.498085	35.320871
1166.906656	120005.077033	35.325888
1168.037605	120217.330485	35.330906
1169.241756	120434.933518	35.335924
1170.222485	120657.796064	35.340941
1171.701161	120860.505213	35.345959
1172.761446	121079.987005	35.350976
1174.750370	121275.936170	35.355994
1176.118304	121483.267985	35.361012
1177.492315	121688.788097	35.366029
1179.093182	121881.333425	35.371047
1180.388180	122085.703534	35.376064
1181.580270	122279.485132	35.381082
1182.883519	122476.759894	35.386100
1183.688776	122674.904287	35.391117
1185.204874	122873.553049	35.396135
1186.310456	123081.484477	35.401152
1187.517194	123275.434868	35.406170
1188.803349	123478.003745	35.411188
1189.781006	123677.824383	35.416205
1190.837176	123884.983843	35.421223
1191.917992	124099.313781	35.426240
1193.151123	124313.404529	35.431258
1194.314151	124507.116648	35.436276
1195.371634	124729.337890	35.441293
1196.957667	124925.567948	35.446311
1198.080618	125151.342747	35.451328
1199.054524	125351.973533	35.456346
1200.255399	125568.841417	35.461364
1201.314126	125794.378161	35.466381
1202.481505	126011.749040	35.471399
1203.532185	126232.182651	35.476416
1204.788658	126452.837200	35.481434
1206.089040	126666.401026	35.486452
1207.370927	126899.184031	35.491469
1209.135096	127105.576224	35.496487
1209.616864	127341.486508	35.501504
1210.790236	127558.220922	35.506522
1212.363733	127789.656766	35.511540
1213.434331	128011.139145	35.516557
1214.986403	128219.183680	35.521575
1216.310033	128447.864683	35.526592
1217.321186	128671.085449	35.531610
1218.957422	128890.971905	35.536628
1220.014459	129115.836037	35.541645
1221.448485	129329.535467	35.546663
1222.654385	129555.278023	35.551680
1223.983059	129756.854576	35.556698
1225.663735	129976.006081	35.561716
1226.498723	130199.659897	35.566733
1227.717944	130402.957309	35.571751
1228.906859	130627.886425	35.576768
1230.052312	130849.148261	35.581786
1231.320990	131068.667230	35.586804
1232.296299	131295.512593	35.591821
1233.376690	131509.044570	35.596839
1234.403313	131742.780578	35.601856
1235.406281	131979.082892	35.606874
1236.348422	132213.558916	35.611892
1237.368008	132452.536747	35.616909
1238.723643	132696.163739	35.621927
1239.656911	132941.231746	35.626944
1240.723130	133189.398123	35.631962
1241.853357	133424.333489	35.636980
1243.147472	133683.596416	35.641997
1244.170826	133933.867354	35.647015
1245.407742	134183.014530	35.652032
1246.647139	134451.762727	35.657050
1247.984031	134694.406306	35.662068
1249.162956	134946.928509	35.667085
1250.815126	135171.292702	35.672103
1251.890244	135411.081774	35.677120
1253.070306	135643.882265	35.682138
1254.611368	135873.581772	35.687156
1255.876627	136119.632807	35.692173
1257.483828	136348.234314	35.697191
1258.496257	136581.931336	35.702208
1260.308282	136818.058430	35.707226
1261.802148	137035.234792	35.712244
1262.925298	137265.748606	35.717261
1264.106703	137502.910686	35.722279
1265.517576	137739.440480	35.727296
1266.832586	137962.801764	35.732314
1267.991061	138204.752560	35.737332
1268.838403	138451.080270	35.742349
1270.350544	138680.169926	35.747367
1271.332361	138922.446786	35.752384
1273.387678	139148.710798	35.757402
1275.627880	139366.691338	35.762420
1277.048382	139586.394171	35.767437
1278.674862	139794.880846	35.772455
1279.869558	140018.199561	35.777472
1280.896312	140237.578821	35.782490
1282.116404	140444.349011	35.787508
1283.292976	140681.534125	35.792525
1284.530835	140899.284927	35.797543
1286.281667	141122.226944	35.802560
1287.152676	141346.508261	35.807578
1288.644017	141556.131214	35.812596
1289.651536	141784.691333	35.817613
1290.642944	142016.413051	35.822631
1291.758478	142238.034726	35.827648
1292.960605	142487.971875	35.832666
1294.781670	142701.655556	35.837684
1296.193933	142930.675964	35.842701
1297.447211	143162.704232	35.847719
1298.865488	143396.773656	35.852736
1300.163194	143633.654454	35.857754
1301.564568	143857.508854	35.862772
1302.409766	144087.023944	35.867789
1303.302954	144320.945636	35.872807
1304.637530	144561.402639	35.877824
1305.500128	144809.840070	35.882842
1306.867446	145066.438507	35.887860
1307.668079	145313.456706	35.892877
1308.952805	145572.215657	35.897895
1310.311963	145828.389726	35.902912
1311.002795	146098.410932	35.907930
1312.653777	146361.984659	35.912948
1313.919704	146621.451770	35.917965
1315.711375	146881.429607	35.922983
1317.688879	147143.547150	35.928000
1319.556074	147377.517420	35.933018
1321.794672	147596.081888	35.938036
1324.193168	147811.488576	35.943053
1326.329510	148016.400813	35.948071
1328.102414	148209.135747	35.953088
1329.370344	148418.100494	35.958106
1330.564447	148607.889665	35.963124
1331.547574	148812.071750	35.968141
1332.356367	149015.649731	35.973159
1333.219204	149211.584726	35.978176
1334.199885	149441.250754	35.983194
1335.634618	149643.548849	35.988212
1336.238267	149872.037117	35.993229
1336.886762	150098.312459	35.998247
1337.954968	150329.833880	36.003264
1338.908868	150572.841495	36.008282
1340.150573	150799.377822	36.013300
1340.419612	151040.739031	36.018317
1341.402928	151289.606203	36.023335
1342.939092	151534.565521	36.028352
1344.237248	151798.502847	36.033370
1345.447862	152052.233287	36.038388
1346.632264	152312.869859	36.043405
1347.810347	152578.519471	36.048423
1349.280236	152848.955206	36.053440
1350.111061	153123.735371	36.058458
1352.092010	153368.493164	36.063476
1353.832330	153635.870707	36.068493
1355.679983	153885.372494	36.073511
1357.629667	154158.426961	36.078528
1359.004724	154409.596069	36.083546
1360.428668	154655.342292	36.088564
1362.239553	154918.695892	36.093581
1363.670071	155156.376608	36.098599
1365.142435	155397.540202	36.103616
1366.464159	155657.301227	36.108634
1367.865805	155901.384520	36.113652
1369.038336	156163.355464	36.118669
1370.162386	156413.145571	36.123687
1372.080573	156662.450363	36.128704
1373.598940	156896.816084	36.133722
1376.783498	157103.480700	36.138740
1378.371647	157324.745874	36.143757
1380.021934	157541.879115	36.148775
1380.973602	157764.787232	36.153792
1382.041380	157994.413505	36.158810
1383.373436	158224.466640	36.163828
1384.433373	158461.746472	36.168845
1385.407402	158696.339808	36.173863
1386.518988	158920.737414	36.178880
1387.409420	159192.581265	36.183898
1388.220897	159440.602479	36.188916
1389.316549	159697.204797	36.193933
1390.411412	159968.664678	36.198951
1391.328622	160242.287145	36.203968
1392.356697	160540.543143	36.208986
1393.653202	160819.714020	36.214004
1395.318446	161099.713703	36.219021
1396.827957	161386.325584	36.224039
1398.910995	161659.117030	36.229056
1400.179900	161941.256053	36.234074
1402.081868	162227.047387	36.239092
1403.312887	162515.007248	36.244109
1404.647255	162775.661541	36.249127
1406.018527	163058.463485	36.254144
1407.289553	163333.874453	36.259162
1408.785257	163619.196983	36.264180
1410.017774	163910.198369	36.269197
1411.291269	164206.815595	36.274215
1412.636261	164486.497472	36.279232
1413.712143	164782.504350	36.284250
1415.411532	165070.302243	36.289268
1416.372578	165360.153060	36.294285
1417.432641	165668.450643	36.299303
1419.374946	165957.711320	36.304320
1421.027170	166258.936342	36.309338
1422.520322	166555.254012	36.314356
1424.155113	166852.273431	36.319373
1425.676163	167145.075717	36.324391
1427.121504	167438.425412	36.329408
1428.290317	167731.683315	36.334426
1429.682255	168019.741790	36.339444
1431.641718	168307.263901	36.344461
1432.857338	168591.815077	36.349479
1434.556051	168861.949301	36.354496
1435.659429	169137.843208	36.359514
1437.228694	169408.294003	36.364532
1438.440225	169685.302638	36.369549
1439.584296	169979.733955	36.374567
1440.995810	170248.502815	36.379584
1441.951121	170546.763211	36.384602
1443.116963	170843.912008	36.389620
1444.983860	171146.035036	36.394637
1446.172060	171439.706968	36.399655
1448.085025	171723.248282	36.404672
1449.323939	172035.531567	36.409690
1450.727230	172325.099925	36.414708
1452.605443	172617.776529	36.419725
1453.423705	172914.755003	36.424743
1455.241962	173223.955214	36.429760
1456.507641	173529.276981	36.434778
1458.491775	173837.476514	36.439796
1459.864047	174138.038277	36.444813
1461.147789	174444.809598	36.449831
1463.235407	174736.309629	36.454848
1464.678053	175033.045411	36.459866
1466.206837	175338.005057	36.464884
1467.883236	175643.589369	36.469901
1469.442770	175942.976391	36.474919
1471.339760	176229.339041	36.479936
1473.064674	176531.227737	36.484954
1474.334868	176812.925835	36.489972
1476.024101	177118.326791	36.494989
1477.129372	177417.163485	36.500007
1478.668468	177711.602259	36.505024
1479.873849	178021.695937	36.510042
1480.776516	178329.937975	36.515060
1482.286874	178628.460863	36.520077
1483.245202	178952.003581	36.525095
1484.621406	179269.551992	36.530112
1485.815705	179613.227055	36.535130
1487.140466	179931.562294	36.540148
1489.009855	180257.449811	36.545165
1490.296452	180598.869634	36.550183
1491.828334	180937.560277	36.555200
1493.888451	181259.107087	36.560218
1495.914698	181578.351471	36.565236
1497.844401	181896.496859	36.570253
1499.340836	182200.005361	36.575271
1501.259584	182513.929659	36.580288
1502.846366	182822.884546	36.585306
1504.122691	183142.465739	36.590324
1506.032331	183451.929196	36.595341
1507.150762	183771.692607	36.600359
1508.515188	184076.033245	36.605376
1509.671540	184404.615695	36.610394
1511.142070	184721.292661	36.615412
1513.016803	185052.374669	36.620429
1514.100869	185371.226510	36.625447
1515.528018	185691.356102	36.630464
1517.579580	186011.714040	36.635482
1518.872119	186326.424120	36.640500
1520.562874	186635.548247	36.645517
1522.077150	186954.655122	36.650535
1523.874686	187262.025944	36.655552
1525.345639	187581.422782	36.660570
1527.075277	187899.928029	36.665588
1529.244143	188194.104190	36.670605
1531.126726	188494.003514	36.675623
1533.172451	188780.586703	36.680640
1535.012931	189055.641022	36.685658
1536.473974	189321.962504	36.690676
1537.809342	189580.042110	36.695693
1538.952645	189857.094513	36.700711
1540.581326	190105.937155	36.705728
1542.019432	190376.240520	36.710746
1543.347969	190648.886356	36.715764
1544.968281	190917.714803	36.720781
1545.684090	191207.158002	36.725799
1547.042093	191483.509549	36.730816
1548.489579	191776.426746	36.735834
1549.641006	192070.638519	36.740852
1551.517647	192372.868838	36.745869
1552.472984	192678.769853	36.750887
1554.155378	192981.593940	36.755904
1555.390552	193286.575624	36.760922
1556.751074	193604.499653	36.765940
1558.073397	193924.424762	36.770957
1559.285059	194255.160736	36.775975
1560.988718	194585.321766	36.780992
1562.532431	194917.631144	36.786010
1563.412225	195257.783793	36.791028
1565.213693	195606.113658	36.796045
1566.676709	195939.000303	36.801063
1568.650715	196282.201617	36.806080
1570.548901	196618.193492	36.811098
1571.957640	196969.706199	36.816116
1573.758996	197298.316011	36.821133
1575.239082	197660.573876	36.826151
1576.940581	197995.665869	36.831168
1578.716329	198342.033938	36.836186
1579.724215	198702.204700	36.841204
1581.573647	199043.930099	36.846221
1582.937335	199402.141170	36.851239
1584.586320	199758.707091	36.856256
1586.050409	200108.525686	36.861274
1587.799517	200481.888622	36.866292
1589.634525	200817.734084	36.871309
1591.207226	201191.612508	36.876327
1592.769180	201542.653595	36.881344
1594.393753	201891.489519	36.886362
1595.992587	202257.446524	36.891380
1597.697738	202614.398472	36.896397
1599.150590	202989.855148	36.901415
1600.444119	203359.258364	36.906432
1602.119072	203728.003452	36.911450
1603.447798	204111.688647	36.916468
1605.065119	204469.895769	36.921485
1606.367246	204853.411419	36.926503
1608.295060	205238.818754	36.931520
1609.846265	205623.325479	36.936538
1611.074267	206005.424429	36.941556
1612.860631	206386.493107	36.946573
1615.200532	206750.114503	36.951591
1617.748321	207108.624133	36.956608
1620.321386	207444.135947	36.961626
1622.709149	207775.413505	36.966644
1625.145563	208106.481212	36.971661
1626.955750	208438.250879	36.976679
1628.528151	208756.462028	36.981696
1629.720277	209070.559877	36.986714
1631.181121	209402.061234	36.991732
1632.539755	209736.120445	36.996749
1634.074181	210064.767928	37.001767
1635.511790	210389.369389	37.006784
1637.371399	210714.181510	37.011802
1638.482187	211052.172644	37.016820
1640.080660	211368.548217	37.021837
1641.978411	211700.570318	37.026855
1643.476898	212030.272603	37.031872
1645.053671	212344.674415	37.036890
1646.221939	212660.643469	37.041908
1647.517279	212969.608481	37.046925
1649.223128	213298.950987	37.051943
1650.480016	213619.175427	37.056960
1651.827058	213963.411657	37.061978
1653.188114	214297.691190	37.066996
1654.394580	214643.426319	37.072013
1655.860537	214994.757936	37.077031
1657.274925	215354.125012	37.082048
1658.904710	215710.156085	37.087066
1660.169989	216090.503638	37.092084
1661.750373	216466.228888	37.097101
1663.581418	216848.695274	37.102119
1664.407837	217230.694733	37.107136
1666.086634	217635.158636	37.112154
1667.261569	218040.952212	37.117172
1669.164114	218446.652232	37.122189
1670.330899	218851.205915	37.127207
1671.393938	219266.674323	37.132224
1673.077650	219768.218791	37.137242
1674.613090	220207.207922	37.142260
1676.060920	220646.822967	37.147277
1677.405642	221096.108480	37.152295
1679.102049	221539.089421	37.157312
1680.851073	221998.293445	37.162330
1682.850285	222447.958609	37.167348
1685.118791	222885.897273	37.172365
1687.186266	223341.777510	37.177383
1689.060841	223785.372778	37.182400
1691.551797	224217.488566	37.187418
1693.637739	224655.667389	37.192436
1696.129828	225058.957438	37.197453
1698.650009	225460.770989	37.202471
1700.914041	225880.890860	37.207488
1702.876656	226274.544506	37.212506
1704.671291	226676.482257	37.217524
1706.480777	227061.705513	37.222541
1708.080417	227453.797367	37.227559
1709.675343	227859.454952	37.232576
1711.262757	228249.392189	37.237594
1712.513198	228650.715020	37.242612
1713.569641	229068.251340	37.247629
1715.115873	229463.660018	37.252647
1716.985040	229880.810092	37.257664
1718.869231	230294.580609	37.262682
1720.218016	230723.859368	37.267700
1722.231042	231136.442512	37.272717
1724.006076	231551.911164	37.277735
1725.393376	231968.994694	37.282752
1727.243041	232395.629767	37.287770
1728.503905	232812.330129	37.292788
1730.109346	233240.481262	37.297805
1731.963030	233673.215445	37.302823
1733.522192	234111.206881	37.307840
1735.286785	234541.494189	37.312858
1737.017548	234978.621217	37.317876
1738.402529	235412.301248	37.322893
1740.335507	235854.807521	37.327911
1741.767035	236308.092123	37.332928
1743.399451	236737.035062	37.337946
1745.164650	237197.760095	37.342964
1747.158547	237624.028775	37.347981
1749.273760	238065.798890	37.352999
1751.897322	238490.796631	37.358016
1754.309099	238902.468886	37.363034
1756.249500	239320.545213	37.368052
1757.762441	239710.928653	37.373069
1759.521836	240096.115315	37.378087
1761.329152	240491.531825	37.383104
1762.584668	240880.766115	37.388122
1764.107517	241283.064376	37.393140
1765.995664	241680.654159	37.398157
1767.659148	242085.597737	37.403175
1769.376221	242499.932020	37.408192
1771.185910	242885.953248	37.413210
1772.836143	243287.852671	37.418228
1774.418364	243702.414468	37.423245
1776.158769	244105.367092	37.428263
1778.046763	244545.205911	37.433280
1779.844231	244948.709146	37.438298
1781.972260	245367.196573	37.443316
1784.303192	245770.460100	37.448333
1786.370003	246161.244338	37.453351
1788.489514	246569.167227	37.458368
1790.821948	246940.653035	37.463386
1793.030382	247336.724386	37.468404
1794.942904	247718.594181	37.473421
1797.091944	248103.295712	37.478439
1798.728147	248482.951218	37.483456
1800.627347	248866.043717	37.488474
1802.383180	249246.213582	37.493492
1803.843836	249640.988641	37.498509
1805.641892	250029.890840	37.503527
1807.122318	250419.455673	37.508544
1808.743901	250811.359917	37.513562
1810.566139	251204.933221	37.518580
1811.799411	251609.680179	37.523597
1813.887588	252027.114354	37.528615
1815.202241	252434.642747	37.533632
1816.853308	252845.646696	37.538650
1818.319040	253272.355380	37.543668
1819.888021	253692.289948	37.548685
1821.475655	254133.077698	37.553703
1823.019797	254579.131349	37.558720
1824.872192	255028.080906	37.563738
1826.484014	255459.339038	37.568756
1828.310961	255902.882264	37.573773
1831.185723	256327.453580	37.578791
1833.452135	256757.765343	37.583808
1835.244059	257206.928854	37.588826
1837.366159	257642.904234	37.593844
1839.809329	258065.184899	37.598861
1841.580033	258472.462065	37.603879
1843.264372	258911.863324	37.608896
1844.759777	259340.245452	37.613914
1846.550025	259763.116994	37.618932
1848.597828	260185.971223	37.623949
1850.525742	260618.244475	37.628967
1851.767654	261064.272876	37.633984
1853.634563	261509.460914	37.639002
1855.539924	261942.398077	37.644020
1857.022628	262389.910390	37.649037
1858.496039	262843.800284	37.654055
1859.920454	263309.129550	37.659072
1861.785748	263754.062951	37.664090
1863.569282	264229.874557	37.669108
1865.039057	264695.525770	37.674125
1866.876080	265166.983955	37.679143
1868.479672	265639.090149	37.684160
1870.734680	266123.916619	37.689178
1872.780235	266596.228239	37.694196
1874.648614	267077.078826	37.699213
1876.704202	267541.309730	37.704231
1878.167651	268019.559149	37.709248
1880.668229	268461.182899	37.714266
1882.356544	268913.432202	37.719284
1883.784005	269367.705652	37.724301
1885.689428	269811.026928	37.729319
1887.437245	270274.340460	37.734336
1889.575830	270729.180302	37.739354
1891.546787	271182.396132	37.744372
1893.581659	271644.923575	37.749389
1895.197894	272095.859847	37.754407
1896.816585	272556.625902	37.759424
1898.596026	273026.357155	37.764442
1900.785747	273497.416811	37.769460
1902.244098	273988.563276	37.774477
1903.892762	274480.795026	37.779495
1905.762368	274962.650431	37.784512
1907.599676	275459.421501	37.789530
1909.146691	275954.029656	37.794548
1910.664634	276464.213231	37.799565
1912.873952	276963.154941	37.804583
1914.542879	277473.692282	37.809600
1916.550319	277991.818399	37.814618
1918.777946	278501.625694	37.819636
1920.899126	279018.434933	37.824653
1923.339832	279532.649718	37.829671
1925.640735	280029.562231	37.834688
1927.356776	280532.870015	37.839706
1929.570423	281044.044765	37.844724
1931.578674	281561.729555	37.849741
1933.717939	282062.753088	37.854759
1935.538039	282571.042111	37.859776
1938.093201	283079.411065	37.864794
1940.209241	283582.948766	37.869812
1941.955819	284080.272017	37.874829
1943.503880	284580.750979	37.879847
1945.682541	285096.466188	37.884864
1947.419407	285608.493521	37.889882
1949.316924	286105.048723	37.894900
1950.813909	286636.823476	37.899917
1953.658309	287151.735555	37.904935
1956.034318	287659.763599	37.909952
1957.495081	288170.278304	37.914970
1960.100519	288669.552274	37.919988
1961.826760	289174.456569	37.925005
1963.747249	289699.520059	37.930023
1965.637470	290220.852646	37.935040
1967.825932	290724.709246	37.940058
1970.401856	291226.366072	37.945076
1972.078522	291737.872650	37.950093
1973.919657	292243.406315	37.955111
1975.942259	292762.141081	37.960128
1977.809754	293273.889016	37.965146
1979.817561	293780.861791	37.970164
1981.310760	294305.798786	37.975181
1983.227273	294812.248791	37.980199
1985.386904	295336.765861	37.985216
1987.520910	295853.360217	37.990234
1989.388797	296368.929485	37.995252
1991.077896	296894.888635	38.000269
1993.474573	297415.470469	38.005287
1995.632424	297942.083361	38.010304
1996.989519	298456.787398	38.015322
1999.505258	298968.426924	38.020340
2001.372782	299498.762708	38.025357
2003.548574	300022.339549	38.030375
2005.453314	300537.094662	38.035392
2007.637275	301058.607413	38.040410
2009.239265	301581.966193	38.045428
2010.676700	302103.901708	38.050445
2012.665899	302611.622018	38.055463
2015.081450	303126.380154	38.060480
2016.755595	303634.553407	38.065498
2018.657679	304142.838450	38.070516
2020.387501	304662.399931	38.075533
2021.923616	305179.069858	38.080551
2023.698584	305702.757408	38.085568
2025.167372	306243.635038	38.090586
2027.351892	306785.584332	38.095604
2028.735614	307336.881568	38.100621
2030.683128	307898.900422	38.105639
2032.649842	308452.023825	38.110656
2034.739593	309025.820435	38.115674
2036.816854	309586.104775	38.120692
2039.054866	310151.082076	38.125709
2041.612222	310720.497369	38.130727
2043.911449	311286.396034	38.135744
2045.952495	311861.576968	38.140762
2048.169251	312411.101583	38.145780
2049.984183	312982.883311	38.150797
2052.199571	313553.324671	38.155815
2054.536170	314121.481544	38.160832
2056.737490	314702.505612	38.165850
2059.027116	315268.223610	38.170868
2061.245501	315848.575463	38.175885
2063.149362	316409.853788	38.180903
2065.733294	316969.872351	38.185920
2068.004680	317536.362538	38.190938
2070.588146	318104.116822	38.195956
2072.724791	318668.791805	38.200973
2075.149075	319226.253939	38.205991
2077.382484	319782.346543	38.211008
2079.409039	320339.738367	38.216026
2081.635887	320877.210928	38.221044
2083.866860	321423.971562	38.226061
2086.012907	321975.845249	38.231079
2088.702441	322504.594852	38.236096
2090.757493	323057.972381	38.241114
2093.307278	323595.343460	38.246132
2095.050238	324131.396357	38.251149
2097.159428	324675.229452	38.256167
2099.208616	325221.276607	38.261184
2100.777300	325769.531202	38.266202
2102.922771	326315.908097	38.271220
2104.733656	326870.409142	38.276237
2106.765704	327425.909366	38.281255
2108.322846	327988.084049	38.286272
2110.362257	328556.545936	38.291290
2112.075694	329128.280557	38.296308
2113.618556	329715.498894	38.301325
2115.782259	330298.241780	38.306343
2117.682760	330890.034750	38.311360
2119.254301	331492.944699	38.316378
2121.620987	332094.244059	38.321396
2123.560037	332691.799801	38.326413
2126.188140	333297.307724	38.331431
2128.387128	333891.989525	38.336448
2130.448749	334493.008558	38.341466
2132.975189	335091.227691	38.346484
2135.391342	335692.834593	38.351501
2137.965843	336283.061515	38.356519
2140.600752	336869.514931	38.361536
2143.079581	337446.417817	38.366554
2145.622276	338007.083462	38.371572
2148.120051	338579.655315	38.376589
2150.455400	339140.292151	38.381607
2153.253155	339692.444455	38.386624
2155.582289	340228.905671	38.391642
2157.697226	340749.608747	38.396660
2159.493127	341270.511503	38.401677
2162.016157	341771.185889	38.406695
2164.674976	342266.223343	38.411712
2167.426809	342751.544684	38.416730
2169.852964	343231.838882	38.421748
2172.259568	343715.151866	38.426765
2173.739888	344193.055026	38.431783
2176.261931	344683.014232	38.436800
2178.122948	345183.965918	38.441818
2179.929605	345670.581680	38.446836
2181.873864	346180.391923	38.451853
2183.720888	346689.349804	38.456871
2186.118439	347181.613055	38.461888
2187.821937	347686.472334	38.466906
2189.684111	348206.932912	38.471924
2191.277355	348730.122171	38.476941
2193.289577	349273.411413	38.481959
2194.975977	349818.600623	38.486976
2196.306139	350378.028068	38.491994
2198.425046	350933.079925	38.497012
2200.357001	351514.268289	38.502029
2202.125152	352101.160378	38.507047
2204.505990	352696.900816	38.512064
2206.543354	353296.978426	38.517082
2208.839315	353888.123549	38.522100
2211.097428	354480.586279	38.527117
2213.437752	355074.194382	38.532135
2215.936159	355677.714644	38.537152
2217.956063	356290.871391	38.542170
2220.245560	356904.126744	38.547188
2221.951346	357515.059267	38.552205
2224.076376	358143.724912	38.557223
2226.280152	358782.263053	38.562240
2227.881014	359418.480704	38.567258
2230.099557	360067.753852	38.572276
2232.137368	360718.923905	38.577293
2234.057789	361375.202282	38.582311
2236.501927	362021.818542	38.587328
2238.893643	362691.265666	38.592346
2240.770694	363364.820305	38.597364
2243.133668	364035.720585	38.602381
2245.187172	364714.600799	38.607399
2247.691291	365384.135106	38.612416
2250.124764	366059.072667	38.617434
2252.030474	366745.881312	38.622452
2254.425446	367427.370923	38.627469
2257.256834	368096.625498	38.632487
2259.781188	368775.557857	38.637504
2261.999348	369456.659147	38.642522
2264.366543	370141.756153	38.647540
2266.778800	370815.393575	38.652557
2268.841734	371497.750778	38.657575
2271.371272	372181.108461	38.662592
2273.691098	372861.697951	38.667610
2276.319883	373538.444317	38.672628
2278.296379	374220.561050	38.677645
2280.730459	374911.896456	38.682663
2283.986231	375570.011582	38.687680
2286.229677	376228.839825	38.692698
2288.419093	376897.326628	38.697716
2290.524209	377568.046055	38.702733
2292.503682	378252.441624	38.707751
2294.690740	378926.518919	38.712768
2296.481172	379597.073008	38.717786
2298.858415	380291.783631	38.722804
2300.829014	380980.537597	38.727821
2302.772948	381668.318197	38.732839
2305.603216	382317.701165	38.737856
2308.016128	382976.623331	38.742874
2310.253947	383623.847301	38.747892
2312.525480	384294.581653	38.752909
2314.453526	384960.592486	38.757927
2316.580548	385622.829690	38.762944
2318.321197	386301.773946	38.767962
2321.198997	386964.340779	38.772980
2324.996969	387609.476933	38.777997
2327.831828	388264.139287	38.783015
2330.318399	388899.198911	38.788032
2332.860772	389560.017471	38.793050
2335.402616	390186.980376	38.798068
2337.675978	390834.507783	38.803085
2339.617153	391492.494821	38.808103
2342.718914	392124.674113	38.813120
2344.686958	392770.817017	38.818138
2347.112692	393410.559007	38.823156
2349.372254	394054.902652	38.828173
2352.069897	394716.775314	38.833191
2354.865869	395344.198155	38.838208
2356.680116	395998.280909	38.843226
2359.401779	396656.608885	38.848244
2361.218323	397307.874419	38.853261
2363.220488	397989.252987	38.858279
2365.288492	398646.047930	38.863296
2367.339513	399322.242714	38.868314
2369.762748	399993.773298	38.873332
2372.743481	400663.396730	38.878349
2375.322324	401351.265213	38.883367
2377.676713	402020.605762	38.888384
2380.099623	402691.211457	38.893402
2382.597352	403360.572600	38.898420
2384.897170	404035.474173	38.903437
2387.440835	404715.513188	38.908455
2389.992643	405394.596793	38.913472
2392.084362	406076.526857	38.918490
2394.505587	406759.854952	38.923508
2396.551884	407453.919277	38.928525
2398.380579	408156.894186	38.933543
2401.109106	408851.569996	38.938560
2403.202955	409554.059473	38.943578
2405.360743	410267.995397	38.948596
2408.058825	410982.430815	38.953613
2409.813009	411704.906480	38.958631
2412.511134	412424.343958	38.963648
2414.597172	413148.726367	38.968666
2416.529213	413880.560882	38.973684
2419.107160	414618.498638	38.978701
2421.200732	415368.399360	38.983719
2423.740998	416100.779970	38.988736
2426.328020	416858.634875	38.993754
2428.485150	417604.863841	38.998772
2431.595425	418351.267772	39.003789
2434.294671	419105.390791	39.008807
2436.753059	419836.538321	39.013824
2439.661304	420578.022758	39.018842
2442.343768	421315.952366	39.023860
2444.902743	422035.624632	39.028877
2447.406459	422785.997868	39.033895
2449.845284	423512.559384	39.038912
2452.274577	424244.822923	39.043930
2454.238281	424984.027963	39.048948
2456.753991	425726.359757	39.053965
2459.061958	426478.323240	39.058983
2461.924487	427206.628609	39.064000
2465.280848	427929.615464	39.069018
2468.013807	428624.788231	39.074036
2470.869860	429323.008527	39.079053
2473.147745	430001.611254	39.084071
2475.749067	430672.800711	39.089088
2478.057014	431356.421806	39.094106
2480.249686	432029.968760	39.099124
2482.476400	432706.882106	39.104141
2484.558791	433407.538922	39.109159
2487.403620	434084.967850	39.114176
2490.865834	434734.184081	39.119194
2493.694773	435422.053412	39.124212
2496.173538	436084.199169	39.129229
2498.357135	436766.365276	39.134247
2500.809695	437448.618240	39.139264
2502.917765	438135.057399	39.144282
2504.631783	438837.531999	39.149300
2506.868938	439533.926910	39.154317
2509.255015	440260.231614	39.159335
2511.488896	440971.408513	39.164352
2513.679041	441698.052945	39.169370
2515.944927	442446.721063	39.174388
2517.849623	443184.393871	39.179405
2520.142854	443945.756324	39.184423
2522.603780	444698.261621	39.189440
2525.162750	445459.071949	39.194458
2527.598436	446225.137102	39.199476
2530.465414	446993.835327	39.204493
2533.257093	447781.133466	39.209511
2535.556360	448567.725411	39.214528
2538.091597	449339.479813	39.219546
2540.333071	450130.069978	39.224564
2543.220130	450916.224720	39.229581
2545.925336	451702.481342	39.234599
2548.508457	452493.128508	39.239616
2551.499649	453282.869056	39.244634
2553.732630	454078.267665	39.249652
2556.944265	454878.227044	39.254669
2558.728966	455683.397467	39.259687
2561.202916	456487.866054	39.264704
2564.065260	457298.558834	39.269722
2566.201283	458121.574805	39.274740
2568.961914	458926.961299	39.279757
2571.709176	459740.962764	39.284775
2574.683363	460563.234935	39.289792
2577.116726	461376.918653	39.294810
2579.185367	462202.306275	39.299828
2581.909591	463020.070203	39.304845
2584.520801	463849.393702	39.309863
2587.175306	464667.960130	39.314880
2589.897876	465497.701062	39.319898
2592.489341	466339.304886	39.324916
2594.957983	467182.964591	39.329933
2597.591116	468028.733277	39.334951
2599.634044	468857.432393	39.339968
2602.468553	469705.165891	39.344986
2606.101971	470533.226186	39.350004
2609.118377	471357.815853	39.355021
2612.566573	472165.322614	39.360039
2615.701427	472963.247822	39.365056
2618.757630	473753.422912	39.370074
2621.231879	474563.766501	39.375092
2623.997269	475352.659318	39.380109
2626.409110	476154.306228	39.385127
2628.852423	476955.913287	39.390144
2631.527635	477742.345433	39.395162
2633.507276	478550.273382	39.400180
2636.345321	479340.650609	39.405197
2638.850744	480136.149291	39.410215
2640.967049	480945.312276	39.415232
2643.274594	481716.434115	39.420250
2645.536052	482493.034576	39.425268
2648.572031	483272.957351	39.430285
2650.924323	484053.363276	39.435303
2653.322430	484838.220978	39.440320
2655.969436	485623.305835	39.445338
2657.683540	486433.398623	39.450356
2660.054712	487233.198916	39.455373
2662.539349	488047.936313	39.460391
2665.390452	488868.026713	39.465408
2668.249957	489681.465190	39.470426
2670.790021	490508.444948	39.475444
2673.365848	491331.493287	39.480461
2675.820485	492175.718560	39.485479
2678.180422	493024.611338	39.490496
2681.084851	493859.596017	39.495514
2684.382326	494711.227390	39.500532
2687.389380	495560.089147	39.505549
2690.062523	496411.990981	39.510567
2692.202876	497264.694862	39.515584
2694.949321	498123.056985	39.520602
2697.176426	499003.102707	39.525620
2699.919238	499873.281178	39.530637
2702.569843	500758.914917	39.535655
2705.292339	501646.607953	39.540672
2708.213723	502524.637670	39.545690
2710.741561	503419.732094	39.550708
2713.954252	504303.771485	39.555725
2717.131679	505187.113378	39.560743
2720.254661	506077.929698	39.565760
2723.232984	506951.628009	39.570778
2725.692467	507843.213419	39.575796
2728.735086	508714.083098	39.580813
2731.769566	509603.862487	39.585831
2734.894756	510480.672181	39.590848
2737.676315	511351.139071	39.595866
2740.314711	512234.888997	39.600884
2743.233918	513114.460516	39.605901
2746.004230	513994.461221	39.610919
2748.247780	514887.552621	39.615936
2751.021609	515771.132067	39.620954
2753.404924	516671.556758	39.625972
2756.223361	517573.066640	39.630989
2758.413400	518482.085053	39.636007
2760.687578	519394.058964	39.641024
2763.920917	520306.928465	39.646042
2766.928677	521218.168855	39.651060
2770.144458	522118.993910	39.656077
2773.271356	523025.673655	39.661095
2775.917532	523923.514046	39.666112
2779.216479	524829.855751	39.671130
2781.876745	525737.306124	39.676148
2784.729564	526626.037185	39.681165
2787.589995	527529.568951	39.686183
2790.141606	528433.600521	39.691200
2793.024964	529333.192128	39.696218
2795.513522	530246.740192	39.701236
2798.229307	531159.841651	39.706253
2801.444597	532073.558811	39.711271
2804.089592	532973.571367	39.716288
2808.000448	533861.389922	39.721306
2811.246314	534740.305413	39.726324
2814.321454	535619.598443	39.731341
2817.557689	536497.452519	39.736359
2820.452873	537381.800920	39.741376
2823.531229	538235.470984	39.746394
2826.175911	539113.615050	39.751412
2828.989653	539960.584112	39.756429
2831.476245	540797.947732	39.761447
2833.947691	541629.328210	39.766464
2836.507424	542449.025055	39.771482
2839.160069	543280.177605	39.776500
2841.793093	544104.192236	39.781517
2844.869322	544951.773716	39.786535
2846.988293	545800.819904	39.791552
2849.224446	546648.034786	39.796570
2852.128970	547511.983159	39.801588
2855.126587	548392.656295	39.806605
2857.650319	549254.396420	39.811623
2860.502775	550128.798101	39.816640
2862.936484	551009.597785	39.821658
2865.962891	551897.581866	39.826676
2868.518225	552796.845428	39.831693
2871.262863	553691.042060	39.836711
2873.768029	554611.856441	39.841728
2876.265360	555528.086183	39.846746
2878.770466	556479.127073	39.851764
2881.221627	557416.190484	39.856781
2884.165182	558367.778145	39.861799
2886.294233	559330.284536	39.866816
2889.116925	560310.541102	39.871834
2891.716362	561295.081932	39.876852
2894.248927	562287.496511	39.881869
2897.653497	563285.065960	39.886887
2900.361139	564286.993646	39.891904
2903.543780	565291.979669	39.896922
2906.839910	566299.881964	39.901940
2909.863603	567310.060456	39.906957
2913.293409	568309.549195	39.911975
2916.882452	569310.590503	39.916992
2920.240969	570318.167691	39.922010
2923.854171	571298.768889	39.927028
2926.571939	572296.557696	39.932045
2930.306340	573283.309571	39.937063
2933.307231	574294.795755	39.942080
2937.428746	575236.667679	39.947098
2941.024478	576197.070597	39.952116
2944.147254	577148.447081	39.957133
2947.735173	578083.168803	39.962151
2950.705182	579018.474215	39.967168
2953.976932	579961.433960	39.972186
2956.778798	580893.716094	39.977204
2959.265799	581837.916056	39.982221
2962.168198	582769.186751	39.987239
2964.410466	583720.453458	39.992256
2967.021974	584682.515678	39.997274
2969.763342	585639.266074	40.002292
2972.184389	586618.754341	40.007309
2974.999042	587586.267713	40.012327
2977.181429	588573.156163	40.017344
2979.933994	589568.740601	40.022362
2981.931293	590582.058270	40.027380
2984.967794	591602.534644	40.032397
2987.483430	592629.573727	40.037415
2990.204644	593658.243466	40.042432
2993.516434	594687.677869	40.047450
2997.008689	595721.651242	40.052468
2999.673702	596760.679361	40.057485
3002.599580	597797.568645	40.062503
3005.979773	598846.460366	40.067520
3008.745600	599885.343672	40.072538
3011.843196	600932.941758	40.077556
3014.610955	601979.798405	40.082573
3017.928623	603018.608985	40.087591
3020.783531	604065.511529	40.092608
3024.238798	605100.155923	40.097626
3028.239762	606095.427287	40.102644
3031.754422	607087.088612	40.107661
3035.201443	608051.251824	40.112679
3038.782037	609011.257652	40.117696
3041.825165	609978.575262	40.122714
3045.584894	610933.834345	40.127732
3047.969636	611898.493715	40.132749
3051.179617	612853.779681	40.137767
3053.642536	613818.109956	40.142784
3056.449348	614777.448521	40.147802
3059.274728	615748.502422	40.152820
3061.633545	616743.749061	40.157837
3064.452124	617723.980367	40.162855
3067.150302	618740.039019	40.167872
3069.801931	619746.713139	40.172890
3072.655820	620775.303696	40.177908
3075.236493	621804.141976	40.182925
3078.121976	622848.823913	40.187943
3080.948627	623907.605825	40.192960
3083.869176	624963.620017	40.197978
3087.296692	626034.334394	40.202996
3090.459071	627109.281552	40.208013
3093.570778	628180.782175	40.213031
3096.354687	629275.303251	40.218048
3099.465750	630360.818038	40.223066
3102.895397	631448.066129	40.228084
3105.733147	632547.831960	40.233101
3109.301588	633633.932397	40.238119
3112.098321	634748.501109	40.243136
3115.377489	635866.215165	40.248154
3119.089187	636960.630424	40.253172
3122.049204	638076.811789	40.258189
3124.866497	639190.850446	40.263207
3127.860687	640320.554946	40.268224
3130.841119	641451.733793	40.273242
3133.714189	642586.596294	40.278260
3136.279535	643742.181186	40.283277
3139.556003	644900.958172	40.288295
3142.275888	646065.778026	40.293312
3145.149656	647238.465207	40.298330
3148.526712	648409.486936	40.303348
3151.176264	649604.866865	40.308365
3155.104827	650774.075538	40.313383
3158.221300	651968.497297	40.318400
3161.190649	653158.315335	40.323418
3165.100122	654337.571730	40.328436
3168.323104	655529.952152	40.333453
3171.764865	656718.814671	40.338471
3174.813454	657910.187891	40.343488
3177.958960	659093.183293	40.348506
3182.635930	660253.524975	40.353524
3186.573547	661413.003880	40.358541
3190.141208	662563.992283	40.363559
3193.632941	663719.086777	40.368576
3196.448111	664862.309674	40.373594
3200.154629	666005.995414	40.378612
3203.894007	667119.535922	40.383629
3208.062710	668240.188702	40.388647
3212.045602	669337.210834	40.393664
3215.536454	670432.943833	40.398682
3219.151763	671516.145626	40.403700
3221.987988	672600.694324	40.408717
3225.019400	673672.555678	40.413735
3228.391590	674758.705456	40.418752
3231.145547	675841.997660	40.423770
3234.400937	676924.882184	40.428788
3237.237203	677993.148010	40.433805
3240.342277	679068.302610	40.438823
3243.429341	680119.683881	40.443840
3246.026606	681155.127956	40.448858
3249.130664	682183.565910	40.453876
3251.633448	683238.710550	40.458893
3255.273491	684294.687630	40.463911
3258.112336	685347.397249	40.468928
3260.223405	686416.639718	40.473946
3263.697819	687490.942215	40.478964
3266.633758	688577.169528	40.483981
3270.072242	689659.857255	40.488999
3273.294670	690747.512406	40.494016
3276.303164	691854.771288	40.499034
3279.337592	692966.552655	40.504052
3282.148688	694098.671807	40.509069
3284.912825	695246.627026	40.514087
3287.763050	696399.924602	40.519104
3290.573113	697553.722904	40.524122
3294.861840	698705.836406	40.529140
3298.320115	699868.198642	40.534157
3301.806337	701035.805208	40.539175
3304.690728	702213.961936	40.544192
3307.795832	703403.965314	40.549210
3311.101680	704580.343885	40.554228
3314.845008	705783.095583	40.559245
3318.200742	706971.922606	40.564263
3321.351259	708179.589449	40.569280
3324.046626	709399.888985	40.574298
3327.384042	710629.514394	40.579316
3330.262930	711877.851669	40.584333
3333.597751	713118.158345	40.589351
3337.116490	714369.587245	40.594368
3340.298606	715622.420380	40.599386
3343.742722	716872.104406	40.604404
3346.932103	718131.736797	40.609421
3350.686464	719394.746533	40.614439
3354.110090	720664.840410	40.619456
3357.320612	721943.231383	40.624474
3361.201255	723199.708108	40.629492
3364.110506	724485.815112	40.634509
3367.210988	725756.713321	40.639527
3370.651668	727052.364747	40.644544
3373.574390	728354.171919	40.649562
3376.830492	729660.508439	40.654580
3380.109515	730987.525623	40.659597
3383.540078	732295.138289	40.664615
3386.732777	733617.935676	40.669632
3389.945045	734943.079953	40.674650
3393.567153	736274.700578	40.679668
3396.700112	737602.873773	40.684685
3400.186822	738945.127295	40.689703
3403.411741	740286.753556	40.694720
3406.283750	741638.619734	40.699738
3409.640778	743001.814381	40.704756
3413.083935	744358.890740	40.709773
3416.535655	745739.890177	40.714791
3419.648603	747111.631650	40.719808
3422.828236	748494.999054	40.724826
3426.164108	749876.616279	40.729844
3429.575707	751265.611479	40.734861
3432.729150	752662.379824	40.739879
3436.434274	754065.255628	40.744896
3439.476542	755470.692945	40.749914
3442.824394	756867.698230	40.754932
3446.446712	758280.350881	40.759949
3449.654900	759700.240922	40.764967
3453.146893	761109.927744	40.769984
3456.261591	762535.747013	40.775002
3460.044309	763933.283536	40.780007
3464.532218	765261.998469	40.785012
3468.479502	766548.912001	40.790016
3472.202487	767760.920867	40.795021
3474.803788	768909.790161	40.800026
3478.082861	769987.614092	40.805031
3480.979930	771001.052183	40.810036
3483.662304	771946.457713	40.815040
3486.237727	772813.889460	40.820045
3488.554644	773623.197764	40.825050
3491.498084	774364.455944	40.830055
3494.069648	775047.106386	40.835060
3495.976193	775643.199173	40.840064
3498.419001	776190.563575	40.845069
3499.950567	776681.179372	40.850074
3501.900751	777119.268501	40.855079
3503.630469	777496.332073	40.860084
3504.884151	777830.584071	40.865088
3506.411103	778123.727650	40.870093
3507.259782	778389.754838	40.875098
3508.961341	778572.704221	40.880103
3510.513208	778738.104318	40.885108
3511.256072	778871.498195	40.890112
3512.464457	778956.682944	40.895117
3513.150447	779026.500425	40.900122
3514.175347	779047.443122	40.905127
3515.117697	779051.864207	40.910132
3515.552303	779015.769256	40.915136
3516.103500	778958.985612	40.920141
3516.511932	778901.536134	40.925146
3517.112157	778801.140349	40.930151
3517.818338	778688.668153	40.935156
3518.105899	778565.731341	40.940160
3518.861587	778424.259050	40.945165
3519.012546	778261.622100	40.950170
3519.690835	778079.502305	40.955175
3519.678108	777887.205205	40.960180
3519.668832	777688.700589	40.965184
3520.257784	777457.260221	40.970189
3519.933118	777251.756955	40.975194
3520.320342	777025.455515	40.980199
3520.563832	776790.162226	40.985204
3520.533202	776540.482587	40.990208
3520.821362	776290.692497	40.995213
3520.764655	776026.033454	41.000218
3520.995062	775754.769233	41.005223
3521.419512	775492.620782	41.010228
3521.330917	775208.735367	41.015232
3521.110290	774923.580522	41.020237
3521.014278	774642.776493	41.025242
3521.014772	774343.331661	41.030247
3521.261367	774059.937266	41.035252
3521.121299	773769.208694	41.040256
3521.110776	773478.299455	41.045261
3521.202407	773175.196699	41.050266
3521.291763	772869.668401	41.055271
3521.103039	772569.788508	41.060276
3520.830788	772265.624789	41.065280
3521.126709	771967.856896	41.070285
3520.864201	771658.395727	41.075290
3520.871504	771341.783006	41.080295
3520.877633	771035.108610	41.085300
3520.434198	770726.032378	41.090304
3520.750634	770414.797588	41.095309
3520.438920	770112.029751	41.100314
3520.780492	769796.970889	41.105319
3520.652716	769492.521287	41.110324
3520.430304	769178.761248	41.115328
3520.588053	768846.937797	41.120333
3519.698239	768552.185196	41.125338
3519.681689	768241.702733	41.130343
3519.896781	767936.541250	41.135348
3519.832856	767630.624746	41.140352
3519.692287	767316.526114	41.145357
3519.224925	767011.094443	41.150362
3519.534350	766707.542971	41.155367
3519.266140	766402.497117	41.160372
3519.125706	766117.235688	41.165376
3519.444434	765805.462465	41.170381
3518.935830	765506.730220	41.175386
3519.414523	765208.710376	41.180391
3519.123236	764901.437688	41.185396
3518.691061	764602.410189	41.190400
3518.787177	764305.896912	41.195405
3518.392528	764012.658316	41.200410
3518.601013	763711.960771	41.205415
3518.539004	763419.137174	41.210420
3518.149567	763116.048780	41.215424
3518.081529	762826.162179	41.220429
3518.110417	762543.745337	41.225434
3518.074292	762257.382746	41.230439
3518.032647	761965.683012	41.235444
3517.718003	761677.174077	41.240448
3517.690137	761395.266201	41.245453
3517.722555	761109.785987	41.250458
3517.654921	760822.880862	41.255463
3517.387435	760531.113704	41.260468
3516.894121	760255.900486	41.265472
3517.153115	759978.184688	41.270477
3516.934818	759700.636267	41.275482
3516.442958	759415.721539	41.280487
3516.719645	759155.242484	41.285492
3516.402161	758882.466888	41.290496
3516.267004	758617.941757	41.295501
3515.903666	758352.655536	41.300506
3516.088883	758092.105807	41.305511
3515.994541	757830.014072	41.310516
3515.687114	757579.201311	41.315520
3516.008498	757312.334409	41.320525
3515.589993	757061.473606	41.325530
3515.225832	756806.251955	41.330535
3515.586279	756548.384620	41.335540
3515.193724	756300.949793	41.340544
3515.521609	756047.069287	41.345549
3515.216151	755798.172228	41.350554
3515.174198	755546.755156	41.355559
3515.055125	755300.279472	41.360564
3514.645038	755058.534150	41.365568
3514.541897	754809.127167	41.370573
3514.430088	754573.834389	41.375578
3514.578210	754344.367088	41.380583
3514.277817	754092.698153	41.385588
3513.925354	753858.262612	41.390592
3514.427868	753623.629256	41.395597
3513.940558	753395.473113	41.400602
3513.956355	753166.832001	41.405607
3513.964104	752937.987892	41.410612
3513.573530	752701.597411	41.415616
3514.002111	752481.757173	41.420621
3513.702864	752250.869129	41.425626
3513.294403	752022.659283	41.430631
3513.381129	751803.350107	41.435636
3513.028564	751587.021474	41.440640
3513.481802	751372.233026	41.445645
3512.924557	751159.680209	41.450650
3512.812057	750940.774640	41.455655
3512.943058	750731.702306	41.460660
3512.545335	750520.834511	41.465664
3512.801107	750311.285611	41.470669
3512.761211	750096.889076	41.475674
3512.442410	749890.091464	41.480679
3512.533474	749682.479532	41.485684
3512.352210	749480.984023	41.490688
3512.618393	749264.142395	41.495693
3512.163355	749059.864962	41.500698
3511.942186	748860.435122	41.505703
3511.963676	748660.367129	41.510708
3511.643506	748475.223675	41.515712
3511.683995	748263.332698	41.520717
3511.275355	748085.656106	41.525722
3511.434345	747890.289449	41.530727
3511.272118	747690.622226	41.535732
3511.168348	747516.242667	41.540736
3511.477529	747342.235747	41.545741
3511.208066	747143.560636	41.550746
3511.072551	746966.060497	41.555751
3511.055691	746777.119912	41.560756
3510.834085	746596.956746	41.565760
3510.947278	746410.951291	41.570765
3510.820748	746241.044757	41.575770
3510.713849	746061.295134	41.580775
3510.698355	745879.746830	41.585780
3510.512667	745711.716884	41.590784
3511.097757	745531.049856	41.595789
3510.426990	745357.753895	41.600794
3510.227803	745184.079570	41.605799
3510.065742	745018.749702	41.610804
3509.919455	744843.872672	41.615808
3509.779612	744678.482526	41.620813
3509.845099	744517.454920	41.625818
3509.738547	744347.948983	41.630823
3509.874590	744197.136967	41.635828
3509.610493	744032.099823	41.640832
3509.804232	743876.080838	41.645837
3509.620277	743717.500710	41.650842
3509.878060	743560.031037	41.655847
3509.866187	743388.659363	41.660852
3509.293421	743245.016830	41.665856
3509.384457	743074.313549	41.670861
3509.286599	742932.416366	41.675866
3508.998937	742774.378308	41.680871
3509.082554	742631.555646	41.685876
3508.958848	742490.000919	41.690880
3509.181965	742331.226722	41.695885
3508.646078	742184.888396	41.700890
3509.037776	742039.828217	41.705895
3508.994645	741901.464085	41.710900
3508.599846	741746.884944	41.715904
3508.945919	741597.224862	41.720909
3508.681466	741461.115116	41.725914
3508.387610	741316.056036	41.730919
3508.457440	741179.441083	41.735924
3508.001893	741046.768429	41.740928
3508.134852	740910.088937	41.745933
3508.052706	740774.728623	41.750938
3507.695349	740647.918933	41.755943
3507.758186	740523.857149	41.760948
3507.833824	740404.539802	41.765952
3507.929568	740272.702888	41.770957
3507.836122	740149.897689	41.775962
3507.856080	740025.884670	41.780967
3508.120264	739883.180433	41.785972
3507.438976	739770.557705	41.790976
3507.443805	739636.845495	41.795981
3507.292612	739524.873706	41.800986
3507.505959	739400.472683	41.805991
3507.785501	739285.062397	41.810996
3507.457270	739158.817744	41.816000
3507.705034	739035.444222	41.821005
3507.577438	738920.343287	41.826010
3507.428568	738808.113659	41.831015
3507.676332	738680.826243	41.836020
3507.280162	738563.241343	41.841024
3507.443646	738439.031436	41.846029
3506.996504	738313.535159	41.851034
3506.885438	738197.530468	41.856039
3507.156710	738091.059613	41.861044
3506.845227	737980.873794	41.866048
3506.901566	737867.310562	41.871053
3507.019278	737759.277322	41.876058
3506.889762	737646.434378	41.881063
3506.931429	737532.918293	41.886068
3506.669886	737428.951240	41.891072
3506.854094	737319.664016	41.896077
3506.671656	737216.868712	41.901082
3506.719317	737102.751726	41.906087
3506.817100	736997.185672	41.911092
3506.569134	736892.219697	41.916096
3506.495393	736785.887434	41.921101
3506.338697	736680.953089	41.926106
3506.225621	736594.419385	41.931111
3506.282459	736477.817611	41.936116
3505.899444	736387.614690	41.941120
3506.267687	736287.537277	41.946125
3506.283830	736186.922925	41.951130
3506.096113	736097.674257	41.956135
3506.210290	735990.755986	41.961140
3505.918812	735902.462615	41.966144
3506.211930	735808.231616	41.971149
3506.004529	735719.773862	41.976154
3505.782392	735621.023006	41.981159
3505.984351	735525.615917	41.986164
3505.442560	735440.130464	41.991168
3505.912526	735329.135547	41.996173
3505.808815	735252.880745	42.001178
3505.660863	735156.883658	42.006183
3505.454401	735076.140021	42.011188
3504.997932	734988.606301	42.016192
3505.399205	734905.681646	42.021197
3505.269959	734827.991600	42.026202
3505.242496	734753.649880	42.031207
3505.371970	734655.522020	42.036212
3505.067805	734589.391848	42.041216
3505.567155	734495.853868	42.046221
3505.474449	734415.975800	42.051226
3505.301935	734335.664618	42.056231
3505.276639	734249.883136	42.061236
3504.821071	734176.646360	42.066240
3504.723439	734092.162202	42.071245
3504.671823	734018.857235	42.076250
3504.691868	733949.846557	42.081255
3504.711916	733884.746089	42.086260
3504.611358	733811.546330	42.091264
3505.171526	733742.642639	42.096269
3504.814204	733667.998867	42.101274
3505.061409	733608.749741	42.106279
3504.986326	733517.176536	42.111284
3504.776228	733450.427386	42.116288
3505.046175	733365.528320	42.121293
3505.183178	733296.443214	42.126298
3504.697725	733223.796798	42.131303
3504.744253	733143.041464	42.136308
3504.333435	733077.362070	42.141312
3504.787348	733011.885806	42.146317
3505.038803	732935.104769	42.151322
3504.756370	732876.828969	42.156327
3504.407123	732798.759623	42.161332
3504.158902	732728.446042	42.166336
3504.343538	732662.219270	42.171341
3504.472935	732599.763973	42.176346
3504.189179	732535.990130	42.181351
3504.489343	732478.704446	42.186356
3504.283438	732420.610755	42.191360
3504.791519	732342.543862	42.196365
3504.585264	732282.369678	42.201370
3504.202803	732216.133939	42.206375
3504.408898	732141.531479	42.211380
3504.025212	732075.195759	42.216384
3504.435697	732016.799246	42.221389
3504.585517	731952.107387	42.226394
3504.279584	731889.966128	42.231399
3504.272140	731831.290730	42.236404
3503.837853	731777.686635	42.241408
3503.956410	731704.580116	42.246413
3504.196499	731654.478515	42.251418
3504.232770	731586.980006	42.256423
3504.195047	731526.227650	42.261428
3504.028475	731466.932171	42.266432
3504.353959	731399.334788	42.271437
3504.218716	731342.806289	42.276442
3504.019136	731293.072227	42.281447
3504.042833	731217.550526	42.286452
3503.629922	731166.464376	42.291456
3503.828676	731102.005246	42.296461
3503.877880	731067.431575	42.301466
3503.437610	731012.783459	42.306471
3503.642945	730950.748588	42.311476
3503.514765	730915.163624	42.316480
3503.914741	730861.267029	42.321485
3503.588955	730804.419607	42.326490
3503.828322	730754.758273	42.331495
3504.365087	730692.270475	42.336500
3503.867641	730646.939726	42.341504
3503.949818	730591.112912	42.346509
3503.543411	730529.522582	42.351514
3503.516120	730469.602500	42.356519
3503.350078	730422.878566	42.361524
3503.140251	730384.432316	42.366528
3503.729377	730322.527325	42.371533
3503.467186	730285.129296	42.376538
3503.611931	730239.541568	42.381543
3503.722120	730189.551445	42.386548
3503.437697	730144.083630	42.391552
3503.757418	730081.627007	42.396557
3503.242864	730045.260118	42.401562
3503.137229	729990.846980	42.406567
3503.052911	729951.436915	42.411572
3502.981554	729914.897146	42.416576
3503.140219	729864.203618	42.421581
3502.894190	729814.715813	42.426586
3502.773269	729788.683746	42.431591
3502.974072	729741.994331	42.436596
3503.251063	729708.070641	42.441600
3503.254507	729671.715536	42.446605
3503.151610	729621.311368	42.451610
3502.881540	729584.109532	42.456615
3503.072398	729534.547825	42.461620
3503.191646	729503.125869	42.466624
3503.497113	729454.436286	42.471629
3503.563146	729426.985302	42.476634
3503.117158	729385.898676	42.481639
3503.535869	729333.623402	42.486644
3503.325472	729290.169373	42.491648
3503.093878	729254.693289	42.496653
3503.333289	729209.529938	42.501658
3503.139739	729162.407046	42.506663
3503.356536	729103.229085	42.511668
3502.970521	729075.009556	42.516672
3502.939898	729027.314092	42.521677
3502.802554	728994.198905	42.526682
3502.905324	728947.620206	42.531687
3503.155754	728912.508781	42.536692
3502.999575	728873.353041	42.541696
3503.119293	728825.235276	42.546701
3503.373381	728787.844113	42.551706
3502.909801	728749.927418	42.556711
3503.089666	728710.170475	42.561716
3503.059422	728667.773134	42.566720
3503.150738	728633.330766	42.571725
3502.911922	728589.877697	42.576730
3502.817580	728555.217999	42.581735
3502.889132	728520.382130	42.586740
3502.844272	728482.840825	42.591744
3502.953908	728440.865021	42.596749
3503.007200	728408.904842	42.601754
3503.107994	728367.276881	42.606759
3503.291709	728328.210967	42.611764
3502.771715	728288.022708	42.616768
3502.774043	728250.422999	42.621773
3502.879971	728214.391226	42.626778
3502.860183	728179.965306	42.631783
3502.878567	728139.241497	42.636788
3502.820567	728106.604982	42.641792
3502.824616	728066.725344	42.646797
3502.933876	728036.736033	42.651802
3502.712655	728001.203238	42.656807
3502.918854	727966.887694	42.661812
3502.644228	727926.805726	42.666816
3502.747754	727896.370985	42.671821
3502.983681	727865.617009	42.676826
3502.687454	727832.820606	42.681831
3502.751365	727791.294887	42.686836
3502.621520	727763.127560	42.691840
3502.727128	727728.233144	42.696845
3503.001595	727691.279470	42.701850
3502.777391	727661.244804	42.706855
3502.920028	727621.785970	42.711860
3502.605313	727600.039550	42.716864
3502.551875	727558.532042	42.721869
3502.692033	727527.396281	42.726874
3502.632666	727497.482402	42.731879
3502.369632	727456.801698	42.736884
3502.249852	727439.481507	42.741888
3502.324888	727402.955832	42.746893
3502.828567	727373.295257	42.751898
3502.469063	727345.362617	42.756903
3502.582327	727312.892805	42.761908
3502.385512	727289.639758	42.766912
3502.556800	727267.118521	42.771917
3502.160035	727233.989518	42.776922
3502.281561	727204.986018	42.781927
3502.275101	727173.526329	42.786932
3501.963837	727157.971251	42.791937
3502.068118	727116.930887	42.796941
3502.287852	727110.057442	42.801946
3502.167964	727091.596994	42.806951
3502.216291	727069.442350	42.811956
3501.970718	727046.345304	42.816961
3501.903032	727021.534244	42.821965
3502.343718	727005.111428	42.826970
3501.891090	726976.053361	42.831975
3502.084004	726955.014071	42.836980
3502.066076	726934.405938	42.841985
3501.802051	726915.126626	42.846989
3502.080901	726887.186021	42.851994
3502.001821	726872.137040	42.856999
3502.243871	726844.499651	42.862004
3502.227606	726820.719967	42.867009
3502.678205	726799.389960	42.872013
3502.528772	726769.587398	42.877018
3502.010519	726744.057200	42.882023
3502.224292	726719.793282	42.887028
3501.998573	726701.844919	42.892033
3502.201482	726673.817043	42.897037
3502.368052	726647.677897	42.902042
3501.992612	726630.844174	42.907047
3502.372785	726595.850012	42.912052
3502.119407	726581.968911	42.917057
3502.153327	726556.198233	42.922061
3502.124143	726524.591162	42.927066
3502.050272	726500.671423	42.932071
3502.528047	726475.025336	42.937076
3502.253766	726463.129445	42.942081
3501.812247	726433.225280	42.947085
3501.999586	726422.590874	42.952090
3502.090972	726388.039945	42.957095
3502.388022	726371.342303	42.962100
3502.151398	726354.584170	42.967105
3501.827074	726326.196287	42.972109
3501.627968	726313.594057	42.977114
3501.748762	726293.853288	42.982119
3502.029908	726278.743688	42.987124
3501.590135	726267.073061	42.992129
3501.574836	726232.043602	42.997133
3502.159412	726234.424610	43.002138
3501.834378	726213.964518	43.007143
3501.912178	726192.496342	43.012148
3501.539698	726186.512803	43.017153
3501.676954	726170.534870	43.022157
3502.003053	726141.791109	43.027162
3501.726353	726133.561909	43.032167
3501.596588	726108.213281	43.037172
3501.637453	726092.796189	43.042177
3501.912154	726077.340426	43.047181
3501.924401	726066.139877	43.052186
3501.349481	726055.036345	43.057191
3501.630463	726028.430358	43.062196
3501.557263	726021.108896	43.067201
3501.592423	726030.319788	43.072205
3501.630104	726000.483507	43.077210
3501.386997	725986.698801	43.082215
3501.823163	725968.639452	43.087220
3501.403332	725978.619319	43.092225
3501.660657	725951.323264	43.097229
3501.499151	725925.136930	43.102234
3501.542777	725924.782945	43.107239
3501.903279	725919.916889	43.112244
3501.720590	725895.815159	43.117249
3501.715806	725882.040445	43.122253
3501.969179	725869.214100	43.127258
3501.940666	725854.204446	43.132263
3501.994896	725826.693776	43.137268
3501.627614	725830.124157	43.142273
3501.491409	725793.328903	43.147277
3501.765679	725770.043245	43.152282
3501.583867	725767.447060	43.157287
3501.811303	725750.858770	43.162292
3501.780758	725730.447911	43.167297
3501.724866	725721.042076	43.172301
3501.865966	725701.197421	43.177306
3501.512285	725687.281823	43.182311
3501.990332	725666.439882	43.187316
3501.635532	725673.138817	43.192321
3501.778531	725642.590079	43.197325
3501.439887	725626.441963	43.202330
3501.335561	725624.526685	43.207335
3501.320499	725619.474746	43.212340
3501.548481	725608.584801	43.217345
3501.768074	725588.875567	43.222349
3501.798054	725578.860727	43.227354
3501.534381	725577.318651	43.232359
3501.946171	725536.170010	43.237364
3501.698897	725532.940358	43.242369
3501.658055	725520.954965	43.247373
3501.953990	725495.831426	43.252378
3501.601274	725494.155384	43.257383
3501.803003	725489.117094	43.262388
3501.716008	725464.205403	43.267393
3501.716564	725445.275348	43.272397
3501.515500	725434.010078	43.277402
3501.327789	725435.131404	43.282407
3501.599336	725413.034511	43.287412
3501.317755	725399.156064	43.292417
3501.461003	725386.495833	43.297421
3501.935491	725377.893957	43.302426
3501.786048	725368.007622	43.307431
3501.997201	725343.145406	43.312436
3501.879441	725337.119149	43.317441
3501.891017	725314.866731	43.322445
3502.035528	725292.790509	43.327450
3501.672177	725290.917957	43.332455
3501.817903	725249.712741	43.337460
3501.925696	725247.712764	43.342465
3501.495522	725236.831979	43.347469
3501.892981	725205.000655	43.352474
3501.421836	725198.784911	43.357479
3501.777523	725174.790322	43.362484
3501.462867	725168.945149	43.367489
3501.450281	725151.007724	43.372493
3501.704177	725141.302248	43.377498
3501.511986	725141.383656	43.382503
3501.754326	725128.310196	43.387508
3501.931488	725112.868743	43.392513
3501.343776	725104.838575	43.397517
3501.588163	725088.989510	43.402522
3501.452142	725071.815670	43.407527
3501.860676	725053.213752	43.412532
3501.737746	725048.823535	43.417537
3501.740151	725032.964793	43.422541
3502.058453	725008.529880	43.427546
3501.847235	725001.230317	43.432551
3501.797624	724982.307486	43.437556
3501.745584	724968.043471	43.442561
3501.623820	724946.555463	43.447565
3501.751403	724948.169890	43.452570
3501.849185	724925.456149	43.457575
3501.669766	724901.945661	43.462580
3501.639485	724902.991484	43.467585
3501.346608	724883.067898	43.472589
3501.610327	724863.696547	43.477594
3501.443149	724858.173691	43.482599
3501.577577	724852.353196	43.487604
3501.652054	724847.335544	43.492609
3501.720595	724815.755308	43.497613
3502.259328	724802.781030	43.502618
3501.785050	724786.306760	43.507623
3501.850702	724761.714630	43.512628
3501.696993	724762.533071	43.517633
3502.047939	724748.003842	43.522637
3502.147946	724729.749537	43.527642
3501.486643	724717.419471	43.532647
3502.039610	724687.443715	43.537652
3501.853207	724676.472340	43.542657
3501.704192	724668.220565	43.547661
3502.056730	724635.948430	43.552666
3502.066778	724636.888501	43.557671
3501.913231	724605.492840	43.562676
3501.727696	724587.334967	43.567681
3501.692177	724580.005994	43.572685
3501.974924	724564.100021	43.577690
3501.546942	724539.787046	43.582695
3501.688271	724527.423177	43.587700
3501.806076	724524.281475	43.592705
3501.633673	724503.841454	43.597709
3501.719036	724479.393907	43.602714
3501.825821	724475.659276	43.607719
3501.718653	724454.564059	43.612724
3501.421576	724445.246182	43.617729
3501.667578	724434.450834	43.622733
3501.718019	724414.964991	43.627738
3501.538504	724401.712288	43.632743
3501.695222	724387.561453	43.637748
3501.717787	724379.974896	43.642753
3501.578833	724368.549215	43.647757
3501.483135	724344.428559	43.652762
3501.309283	724338.906456	43.657767
3501.730289	724322.283304	43.662772
3501.464942	724330.455398	43.667777
3501.358242	724303.759222	43.672781
3501.765742	724294.225616	43.677786
3501.634160	724286.961819	43.682791
3501.720153	724278.522130	43.687796
3501.795423	724261.212557	43.692801
3501.603126	724244.492351	43.697805
3501.698642	724237.934418	43.702810
3501.626281	724221.838658	43.707815
3501.612289	724199.835265	43.712820
3501.771834	724181.074280	43.717825
3501.887584	724177.784098	43.722829
3501.835189	724154.597424	43.727834
3501.641764	724155.571175	43.732839
3501.727649	724128.049597	43.737844
3501.767785	724120.261645	43.742849
3501.429929	724096.725476	43.747853
3501.832936	724092.693904	43.752858
3501.511121	724074.210476	43.757863
3501.499802	724056.964347	43.762868
3501.662057	724061.497468	43.767873
3501.322268	724046.436829	43.772877
3501.424412	724040.274152	43.777882
3501.466375	724025.150388	43.782887
3501.430032	724012.220344	43.787892
3501.481704	723997.392307	43.792897
3501.232826	723988.115510	43.797901
3501.425229	723987.092526	43.802906
3501.368018	723982.294367	43.807911
3501.530968	723964.573171	43.812916
3501.437798	723963.696505	43.817921
3500.919776	723958.379714	43.822925
3501.370417	723958.503591	43.827930
3501.372294	723960.733756	43.832935
3501.232567	723947.870260	43.837940
3501.178908	723923.989247	43.842945
3501.529423	723913.374205	43.847949
3501.700640	723905.960904	43.852954
3501.331087	723910.879378	43.857959
3501.223940	723900.191257	43.862964
3501.386387	723903.782708	43.867969
3501.519714	723879.077634	43.872973
3501.578487	723859.688232	43.877978
3501.472243	723861.985857	43.882983
3501.550510	723864.599942	43.887988
3501.386025	723836.077908	43.892993
3501.213434	723822.773563	43.897997
3501.617272	723817.155643	43.903002
3501.325240	723810.958805	43.908007
3501.459998	723817.033120	43.913012
3501.110927	723811.143098	43.918017
3501.042205	723786.272875	43.923021
3501.221127	723775.339057	43.928026
3501.166855	723769.350723	43.933031
3501.467687	723767.467185	43.938036
3501.443825	723775.748615	43.943041
3501.462227	723771.532620	43.948045
3501.440943	723758.946647	43.953050
3501.099724	723741.159592	43.958055
3501.388824	723722.475287	43.963060
3501.576731	723718.479081	43.968065
3501.405963	723721.332629	43.973069
3501.693462	723717.468661	43.978074
3501.521299	723695.688324	43.983079
3501.324468	723679.314680	43.988084
3501.369135	723670.534239	43.993089
3501.474600	723671.409086	43.998093
3501.628568	723659.140961	44.003098
3501.364544	723647.041024	44.008103
3501.597143	723637.634699	44.013108
3501.429148	723633.350305	44.018113
3501.182399	723623.130989	44.023117
3501.129701	723623.238920	44.028122
3501.288703	723622.915339	44.033127
3501.424600	723612.583209	44.038132
3501.460662	723592.701272	44.043137
3501.401011	723591.273797	44.048141
3501.750270	723578.973280	44.053146
3501.230876	723588.129849	44.058151
3500.984602	723575.233811	44.063156
3501.225637	723548.477726	44.068161
3501.183528	723541.347184	44.073165
3501.391806	723533.233493	44.078170
3501.249074	723533.405871	44.083175
3501.408712	723537.989280	44.088180
3501.209749	723532.024684	44.093185
3501.386080	723542.305498	44.098189
3501.854447	723512.636865	44.103194
3501.324475	723498.350153	44.108199
3501.662721	723482.185094	44.113204
3501.713213	723480.888100	44.118209
3501.368069	723465.133343	44.123213
3501.451932	723451.439049	44.128218
3501.531233	723438.786399	44.133223
3501.568304	723440.862187	44.138228
3501.605745	723433.569705	44.143233
3501.726307	723417.440494	44.148237
3501.930252	723399.909583	44.153242
3501.544520	723407.160698	44.158247
3501.727394	723377.191786	44.163252
3501.325252	723360.702735	44.168257
3501.291465	723352.381030	44.173261
3501.671642	723347.708492	44.178266
3501.306961	723336.764792	44.183271
3501.561184	723316.449595	44.188276
3501.761258	723309.675376	44.193281
3501.546781	723302.424408	44.198285
3501.669899	723290.904356	44.203290
3501.383498	723278.460599	44.208295
3501.269612	723267.871908	44.213300
3501.307811	723260.083465	44.218305
3501.444255	723253.815398	44.223309
3501.346393	723250.262739	44.228314
3501.317660	723250.267578	44.233319
3501.233868	723235.510128	44.238324
3501.266109	723224.351980	44.243329
3501.265801	723222.716360	44.248333
3501.135883	723226.306854	44.253338
3501.120933	723224.673654	44.258343
3501.223272	723222.128838	44.263348
3501.403650	723210.946192	44.268353
3501.222122	723214.446083	44.273357
3501.487650	723201.464883	44.278362
3501.161773	723180.005998	44.283367
3501.083349	723169.510459	44.288372
3501.379453	723172.832298	44.293377
3501.335504	723169.468970	44.298381
3501.420002	723168.513289	44.303386
3501.321076	723168.529728	44.308391
3501.275734	723146.726984	44.313396
3501.207519	723126.960297	44.318401
3501.264154	723127.446719	44.323405
3501.655103	723129.612814	44.328410
3501.405407	723135.602457	44.333415
3501.436976	723125.138253	44.338420
3501.327310	723101.958086	44.343425
3501.260870	723088.635014	44.348429
3501.307564	723080.696290	44.353434
3501.219513	723081.851028	44.358439
3501.246151	723084.077339	44.363444
3501.163006	723081.711839	44.368449
3501.171008	723081.512330	44.373453
3501.425156	723072.399220	44.378458
3501.475415	723056.776618	44.383463
3501.274041	723035.544631	44.388468
3501.298880	723036.581580	44.393473
3500.981336	723041.640679	44.398477
3501.678945	723040.087968	44.403482
3501.235731	723033.965096	44.408487
3501.289970	723021.117669	44.413492
3501.371665	722995.377522	44.418497
3501.322967	722988.445872	44.423501
3501.007639	722991.125279	44.428506
3500.923766	723004.870088	44.433511
3501.647051	722985.616671	44.438516
3501.357301	722990.968628	44.443521
3501.127856	722994.327820	44.448525
3501.541820	722961.295449	44.453530
3501.373090	722949.971862	44.458535
3501.317482	722946.659940	44.463540
3501.814011	722939.885999	44.468545
3501.207201	722935.029343	44.473549
3501.225831	722907.960948	44.478554
3500.843215	722901.034836	44.483559
3500.809184	722887.210379	44.488564
3500.845047	722899.597171	44.493569
3500.858986	722902.470045	44.498573
3501.055162	722886.922150	44.503578
3501.050985	722898.324149	44.508583
3500.950464	722893.582084	44.513588
3501.157560	722892.804394	44.518593
3500.982341	722890.007921	44.523597
3501.044567	722893.765088	44.528602
3500.706322	722894.961197	44.533607
3501.286267	722874.987654	44.538612
3501.305780	722887.030172	44.543617
3500.544429	722898.755580	44.548621
3500.796440	722891.575873	44.553626
3501.104232	722896.432580	44.558631
3501.132490	722894.246899	44.563636
3501.044539	722887.420791	44.568641
3500.945021	722893.881497	44.573645
3501.226560	722884.367089	44.578650
3500.977351	722895.165169	44.583655
3501.037305	722896.493755	44.588660
3500.710471	722897.687978	44.593665
3500.459689	722902.389136	44.598669
3501.052647	722894.012967	44.603674
3500.926416	722900.825075	44.608679
3500.976113	722895.512912	44.613684
3501.219090	722893.539600	44.618689
3501.057296	722902.042980	44.623693
3501.203525	722893.344071	44.628698
3501.216397	722901.422024	44.633703
3501.300173	722889.164358	44.638708
3501.421599	722869.117862	44.643713
3501.187948	722864.496922	44.648717
3501.292871	722861.951568	44.653722
3501.025739	722862.392369	44.658727
3500.858056	722859.594640	44.663732
3501.242850	722852.492098	44.668737
3501.192326	722855.177359	44.673741
3501.501052	722856.663124	44.678746
3501.353481	722858.620860	44.683751
3501.072402	722834.526425	44.688756
3501.493184	722814.975608	44.693761
3501.148499	722812.554110	44.698765
3501.358014	722805.827490	44.703770
3501.127261	722821.282292	44.708775
3501.214009	722813.981115	44.713780
3501.388693	722811.424218	44.718785
3501.214003	722808.478917	44.723789
3501.367047	722778.364053	44.728794
3501.163529	722766.252823	44.733799
3501.222306	722765.450061	44.738804
3501.407997	722759.917052	44.743809
3501.401935	722767.651265	44.748813
3501.266830	722764.748978	44.753818
3501.305039	722768.361457	44.758823
3501.432271	722745.388997	44.763828
3501.627973	722732.517746	44.768833
3501.148484	722721.988772	44.773837
3501.312519	722723.498473	44.778842
3501.366493	722726.711793	44.783847
3501.575343	722709.575182	44.788852
3501.750185	722693.733021	44.793857
3500.967953	722689.797498	44.798861
3501.668514	722682.791345	44.803866
3501.582345	722689.250003	44.808871
3501.372298	722662.565598	44.813876
3501.609655	722645.622432	44.818881
3501.667155	722640.556676	44.823885
3501.406506	722635.741780	44.828890
3501.754353	722631.123758	44.833895
3501.667681	722604.418777	44.838900
3501.681746	722586.223511	44.843905
3501.173202	722593.297339	44.848909
3501.478953	722571.236770	44.853914
3501.510387	722556.409493	44.858919
3501.313604	722553.666041	44.863924
3501.624174	722549.748150	44.868929
3501.500336	722547.389222	44.873933
3501.411951	722536.002217	44.878938
3501.670066	722523.814345	44.883943
3501.423040	722505.860340	44.888948
3501.776159	722507.933708	44.893953
3501.680002	722500.166753	44.898957
3501.888543	722465.233011	44.903962
3501.689672	722468.587361	44.908967
3501.403276	722460.703088	44.913972
3501.615814	722436.674640	44.918977
3501.190333	722431.738144	44.923981
3501.507981	722418.400094	44.928986
3501.064807	722412.871630	44.933991
3501.444008	722422.723728	44.938996
3501.492153	722413.891806	44.944001
3500.994030	722390.823412	44.949005
3501.440175	722373.944335	44.954010
3501.041666	722376.092373	44.959015
3501.395341	722367.209911	44.964020
3501.566278	722366.091133	44.969025
3501.184596	722368.186818	44.974029
3501.571171	722358.059568	44.979034
3501.473743	722336.560739	44.984039
3501.720531	722324.572742	44.989044
3501.620656	722319.830240	44.994049
3501.462365	722319.112880	44.999053
3501.145182	722303.400856	45.004058
3501.358723	722280.462419	45.009063
3501.605523	722272.043684	45.014068
3501.175668	722275.039689	45.019073
3501.284281	722280.276696	45.024077
3501.131332	722270.486369	45.029082
3500.792300	722286.901969	45.034087
3500.820064	722276.982638	45.039092
3501.098341	722273.714418	45.044097
3501.276383	722288.904359	45.049101
3501.328530	722269.115731	45.054106
3501.221381	722241.471052	45.059111
3501.427303	722236.925840	45.064116
3501.790279	722229.281055	45.069121
3501.558837	722239.581305	45.074125
3501.273540	722201.654446	45.079130
3501.352935	722194.403514	45.084135
3501.490234	722191.406434	45.089140
3501.563670	722194.815043	45.094145
3501.384398	722192.613898	45.099149
3501.696575	722174.517188	45.104154
3501.454925	722163.749896	45.109159
3501.443801	722157.951562	45.114164
3501.671969	722145.470635	45.119169
3501.534134	722147.030328	45.124173
3501.576383	722101.463907	45.129178
3501.383814	722105.709716	45.134183
3501.615361	722099.524213	45.139188
3501.843687	722096.264179	45.144193
3501.413515	722084.734734	45.149197
3501.479041	722060.332888	45.154202
3501.294808	722059.124036	45.159207
3501.268922	722054.815335	45.164212
3501.425752	722060.391542	45.169217
3501.280327	722036.916846	45.174221
3501.191777	722023.496562	45.179226
3501.250529	722009.357852	45.184231
3501.154703	722009.572082	45.189236
3501.145385	721997.774664	45.194241
3501.282704	722013.665901	45.199245
3501.143543	722012.994928	45.204250
3501.177976	722006.346171	45.209255
3500.945984	722008.020602	45.214260
3501.103333	722008.242569	45.219265
3501.054487	721997.294471	45.224269
3501.466890	721975.760029	45.229274
3501.303601	721971.523567	45.234279
3500.859510	721971.299590	45.239284
3501.099410	721967.789713	45.244289
3501.088920	721970.815676	45.249293
3501.351043	721960.708509	45.254298
3501.026152	721966.463538	45.259303
3501.171543	721962.622245	45.264308
3501.469261	721960.887550	45.269313
3501.261687	721954.923234	45.274317
3501.207161	721929.747625	45.279322
3501.282051	721920.514147	45.284327
3501.057557	721921.592439	45.289332
3501.226768	721922.109907	45.294337
3501.003297	721920.659637	45.299341
3501.275843	721915.310019	45.304346
3501.328503	721909.748853	45.309351
3501.126647	721912.409850	45.314356
3501.366648	721907.115182	45.319361
3501.400434	721894.269389	45.324365
3501.317564	721882.682267	45.329370
3501.130088	721875.623888	45.334375
3500.816110	721872.998729	45.339380
3501.324247	721874.402146	45.344385
3500.918313	721873.775247	45.349389
3501.000010	721876.736433	45.354394
3500.988491	721869.252358	45.359399
3501.296624	721879.463887	45.364404
3501.531340	721867.824262	45.369409
3501.117602	721848.359503	45.374413
3501.224131	721829.354067	45.379418
3501.402412	721835.373073	45.384423
3501.468265	721832.982592	45.389428
3501.450958	721838.835610	45.394433
3501.187537	721837.243197	45.399437
3501.098983	721829.375202	45.404442
3501.050001	721811.783577	45.409447
3501.179865	721807.002816	45.414452
3501.533831	721793.112414	45.419457
3501.262916	721802.874380	45.424461
3501.209749	721802.387486	45.429466
3500.977435	721805.202282	45.434471
3501.190469	721797.383572	45.439476
3501.515721	721792.421782	45.444481
3501.216700	721781.812204	45.449485
3501.127046	721756.691452	45.454490
3501.182755	721759.557820	45.459495
3501.227411	721759.600108	45.464500
3501.638340	721744.212893	45.469505
3501.435050	721751.980647	45.474509
3501.143351	721747.566981	45.479514
3501.339590	721739.750992	45.484519
3501.263864	721718.643592	45.489524
3501.181756	721711.121462	45.494529
3500.728019	721705.941309	45.499533
3501.211296	721701.300395	45.504538
3501.304002	721709.762938	45.509543
3501.004045	721710.357951	45.514548
3501.396893	721708.012553	45.519553
3501.127971	721710.188921	45.524557
3501.566992	721705.406589	45.529562
3501.359198	721698.797616	45.534567
3500.969150	721673.775831	45.539572
3501.239369	721667.385305	45.544577
3501.223998	721660.843657	45.549581
3501.425187	721660.860079	45.554586
3501.351428	721663.847031	45.559591
3500.916609	721657.077229	45.564596
3501.328908	721657.554543	45.569601
3501.393346	721654.370998	45.574605
3501.033824	721627.460068	45.579610
3501.163899	721628.231912	45.584615
3501.049861	721623.094727	45.589620
3501.122154	721620.405652	45.594625
3500.974018	721628.114829	45.599629
3501.067322	721624.579457	45.604634
3500.931364	721624.602015	45.609639
3501.050630	721624.136194	45.614644
3501.268962	721622.315393	45.619649
3501.147953	721627.739493	45.624653
3501.336817	721627.510061	45.629658
3501.323584	721619.034482	45.634663
3501.175369	721598.484115	45.639668
3501.385569	721588.434655	45.644673
3501.032189	721585.815914	45.649677
3500.971027	721583.743822	45.654682
3501.165475	721583.860514	45.659687
3500.884135	721586.584328	45.664692
3500.962383	721572.590388	45.669697
3501.186816	721573.594536	45.674701
3501.029492	721581.850637	45.679706
3501.388751	721585.708048	45.684711
3501.229561	721578.198536	45.689716
3501.282609	721577.594920	45.694721
3500.891332	721560.307219	45.699725
3501.092862	721543.169411	45.704730
3501.463240	721543.554502	45.709735
3501.040708	721536.435520	45.714740
3501.455019	721531.905066	45.719745
3501.582787	721538.130951	45.724749
3501.195817	721529.320413	45.729754
3501.331206	721538.023972	45.734759
3501.303181	721527.170969	45.739764
3501.624711	721491.966565	45.744769
3501.241246	721498.723173	45.749773
3501.246527	721491.880507	45.754778
3500.948321	721497.978500	45.759783
3500.965942	721493.315265	45.764788
3501.061165	721495.679406	45.769793
3501.132489	721498.047496	45.774797
3501.406109	721494.333534	45.779802
3501.302399	721476.155294	45.784807
3501.457811	721447.671315	45.789812
3501.398074	721371.676080	45.794817
3501.064804	721256.061206	45.799821
3500.905986	721092.718839	45.804826
3501.006056	720860.708359	45.809831
3500.715401	720578.428016	45.814836
3500.715741	720240.156779	45.819841
3500.659689	719840.540075	45.824845
3500.232746	719387.357333	45.829850
3499.963045	718878.925540	45.834855
3499.660991	718303.064911	45.839860
3499.590188	717686.056458	45.844865
3499.065586	716994.322226	45.849869
3498.886757	716265.365685	45.854874
3498.667104	715462.576016	45.859879
3497.926918	714609.531279	45.864884
3497.479810	713687.224420	45.869889
3497.050811	712737.814985	45.874893
3496.780798	711701.806277	45.879898
3496.047162	710609.254311	45.884903
3494.822865	709476.675508	45.889908
3494.542353	708271.341907	45.894913
3493.948244	707022.881897	45.899917
3493.186118	705697.625637	45.904922
3492.810546	704323.565323	45.909927
3491.898904	702885.676258	45.914932
3491.218660	701396.622342	45.919937
3490.470066	699835.352982	45.924941
3489.521259	698219.998105	45.929946
3488.552113	696551.344673	45.934951
3487.566252	694808.574689	45.939956
3486.992447	693030.524195	45.944961
3485.775522	691190.779779	45.949965
3484.406314	689289.920700	45.954970
3483.344795	687326.340904	45.959975
3482.263127	685321.911947	45.964980
3481.441876	683255.598168	45.969985
3480.188633	681151.831020	45.974989
3479.003873	678956.748555	45.979994
3478.035281	676725.080160	45.984999
3476.858759	674439.676408	45.990004
3475.564640	672102.929361	45.995009
3474.026629	669704.352626	46.000013
3473.028155	667253.051809	46.005018
3471.974368	664732.024469	46.010023
3470.297715	662177.847434	46.015028
3469.194164	659554.307403	46.020033
3467.450960	656892.763987	46.025037
3466.105165	654175.337890	46.030042
3464.646466	651404.071600	46.035047
3463.015290	648589.681236	46.040052
3461.910993	645704.825472	46.045057
3460.026127	642778.420707	46.050061
3458.333352	639803.324433	46.055066
3456.780453	636768.002199	46.060071
3455.322701	633701.745996	46.065076
3453.637332	630569.994938	46.070081
3451.664262	627393.392389	46.075085
3449.733518	624158.978037	46.080090
3448.092404	620887.814970	46.085095
3446.004461	617581.806029	46.090100
3444.403469	614208.033201	46.095105
3442.753327	610797.029005	46.100109
3440.915477	607333.490842	46.105114
3439.153499	603811.516524	46.110119
3436.895326	600260.477128	46.115124
3434.999652	596654.504356	46.120129
3433.038249	593010.057539	46.125133
3430.893416	589296.230255	46.130138
3428.871271	585547.252388	46.135143
3426.896006	581765.531679	46.140148
3424.797531	577925.882125	46.145153
3422.953366	574046.868611	46.150157
3420.655341	570120.434487	46.155162
3418.486185	566146.556487	46.160167
3415.829937	562137.546654	46.165172
3413.735874	558082.033438	46.170177
3411.251553	553998.844078	46.175181
3409.118187	549850.902325	46.180186
3406.764933	545676.077657	46.185191
3404.001653	541466.780867	46.190196
3402.284530	537209.592546	46.195201
3399.705011	532914.697153	46.200205
3397.249923	528573.387785	46.205210
3394.606298	524188.726504	46.210215
3392.440633	519770.487176	46.215220
3389.923285	515304.249581	46.220225
3387.326105	510816.180185	46.225229
3384.571711	506270.909936	46.230234
3382.143730	501701.405722	46.235239
3379.409200	497094.120039	46.240244
3376.595724	492438.131594	46.245249
3374.274577	487770.175098	46.250253
3371.480310	483043.247598	46.255258
3368.895296	478294.635745	46.260263
3365.651330	473499.169734	46.265268
3362.832839	468680.624904	46.270273
3359.954153	463832.403887	46.275277
3357.154784	458941.312310	46.280282
3354.661986	454027.438135	46.285287
3351.596233	449081.001490	46.290292
3348.748482	444094.879730	46.295297
3345.621244	439092.090505	46.300301
3342.653614	434057.815025	46.305306
3339.857395	428988.154609	46.310311
3336.579501	423891.400567	46.315316
3333.230564	418762.296618	46.320321
3330.322890	413615.474811	46.325325
3327.370232	408435.698670	46.330330
3324.299776	403231.404290	46.335335
3320.724445	398008.800339	46.340340
3318.135417	392755.798329	46.345345
3314.768774	387469.177164	46.350349
3311.087507	382171.021246	46.355354
3308.167901	376841.734014	46.360359
3304.655725	371497.099126	46.365364
3301.580443	366120.369956	46.370369
3298.262171	360739.968058	46.375373
3294.514770	355337.238017	46.380378
3291.143404	349908.667558	46.385383
3287.798475	344477.677651	46.390388
3284.479786	339002.419350	46.395393
3281.223013	333520.605023	46.400397
3277.100981	328011.452982	46.405402
3273.663763	322491.769771	46.410407
3270.109441	316974.200744	46.415412
3266.652470	311426.825876	46.420417
3263.140261	305880.895639	46.425421
3259.442937	300303.677458	46.430426
3255.871804	294725.509994	46.435431
3251.842926	289148.543924	46.440436
3248.268792	283552.017759	46.445441
3244.527593	277938.061424	46.450445
3240.495815	272328.282689	46.455450
3236.854088	266722.892587	46.460455
3232.950876	261081.522130	46.465460
3229.068677	255452.022520	46.470465
3225.194131	249826.009637	46.475469
3221.109265	244190.319803	46.480474
3217.484762	238556.117278	46.485479
3213.231566	232909.084576	46.490484
3209.159013	227270.447496	46.495489
3205.264291	221626.549722	46.500493
3201.457364	215991.684483	46.505498
3197.336221	210350.352971	46.510503
3193.453171	204639.739333	46.515508
3189.053166	198992.559053	46.520513
3184.942538	193370.385487	46.525517
3180.578124	187738.233709	46.530522
3176.371752	182122.639442	46.535527
3172.011735	176514.251794	46.540532
3167.871061	170914.029745	46.545537
3163.621326	165324.815659	46.550541
3159.066374	159753.918023	46.555546
3154.880960	154183.138771	46.560551
3150.092352	148634.996809	46.565556
3145.637208	143087.502642	46.570561
3141.446751	137561.937516	46.575565
3136.408310	132068.340989	46.580570
3132.043539	126584.668731	46.585575
3127.507888	121117.359656	46.590580
3122.673391	115676.438113	46.595585
3117.600928	110262.960829	46.600589
3112.881031	104866.873795	46.605594
3108.185658	99495.242222	46.610599
3103.033148	94163.171434	46.615604
3098.170273	88854.606888	46.620609
3093.110429	83585.008173	46.625613
3087.938723	78337.357174	46.630618
3083.148785	73130.588987	46.635623
3078.317458	67970.986152	46.640628
3072.952050	62823.016360	46.645633
3067.488600	57722.550018	46.650637
3061.840434	52672.982054	46.655642
3056.556784	47662.095708	46.660647
3050.346409	42721.861454	46.665652
3044.742551	37817.796341	46.670657
3038.110123	32984.475836	46.675661
3031.101946	28217.687633	46.680666
3021.265181	23606.438058	46.685671
3006.315311	19235.898942	46.690676
2991.895768	15020.218851	46.695681
2977.670727	11010.194233	46.700685
2961.351727	7263.841311	46.705690
2939.050450	3960.985322	46.710695
2910.886294	1138.802943	46.715700
2829.386464	237.135610	46.720705
2747.022603	244.856814	46.725709
2710.762584	242.876890	46.730714
2714.424360	228.408404	46.735719
2739.061707	226.172606	46.740724
2768.471327	224.430128	46.745729
2791.151379	214.799515	46.750733
2804.374770	225.520424	46.755738
2808.208875	223.342737	46.760743
2805.889017	225.264059	46.765748
2800.790632	224.711633	46.770753
2795.432749	213.072677	46.775757
2790.371535	224.061955	46.780762
2786.735331	219.741095	46.785767
2783.756726	223.794576	46.790772
2781.016928	215.336551	46.795777
2779.277647	215.782791	46.800781
2776.419153	210.011051	46.805786
2774.220683	204.796875	46.810791
2771.057737	210.707434	46.815796
2768.333986	202.689005	46.820801
2765.121900	207.508922	46.825805
2761.811669	205.351819	46.830810
2758.786485	192.968055	46.835815
2755.445953	198.963861	46.840820
2752.197292	202.884651	46.845825
2749.157616	197.132271	46.850829
2745.590656	210.566335	46.855834
2742.698742	200.693155	46.860839
2739.208047	208.638865	46.865844
2736.038183	200.390799	46.870849
2732.997183	203.194632	46.875853
2729.481419	207.015991	46.880858
2726.079073	198.874892	46.885863
2722.982771	208.737787	46.890868
2719.620208	200.374615	46.895873
2716.176728	204.268675	46.900877
2712.936883	202.576532	46.905882
2709.850412	199.327068	46.910887
2705.853799	204.410095	46.915892
2702.625388	192.304324	46.920897
2699.665977	191.476089	46.925901
2695.538584	188.693970	46.930906
2692.473723	193.478907	46.935911
2688.614900	186.876080	46.940916
2685.675744	201.136502	46.945921
2682.641197	197.172783	46.950925
2679.057689	197.637824	46.955930
2675.471685	195.102956	46.960935
2671.617968	195.303900	46.965940
2668.093476	182.242930	46.970945
2665.327994	192.316701	46.975949
2662.208865	189.752313	46.980954
2658.676263	185.277080	46.985959
2654.850415	185.890795	46.990964
2651.337435	195.549985	46.995969
2648.092452	192.232089	47.000973
2644.473989	194.088058	47.005978
2641.211918	192.380311	47.010983
2637.891406	186.088224	47.015988
2634.656629	179.561719	47.020993
2630.823594	183.946581	47.025997
2626.936870	181.442993	47.031002
2624.058481	183.069302	47.036007
2620.744875	188.231334	47.041012
2617.094469	185.996872	47.046017
2614.093037	180.011728	47.051021
2610.438262	188.236883	47.056026
2606.819306	189.102725	47.061031
2603.441858	169.424438	47.066036
2599.660814	177.617220	47.071041
2596.058885	176.073722	47.076045
2592.877309	182.739924	47.081050
2589.281922	180.875069	47.086055
2585.837266	190.393143	47.091060
2582.195874	183.137349	47.096065
2579.062097	175.867771	47.101069
2575.286939	191.509684	47.106074
2571.760438	182.770831	47.111079
2568.477008	185.217277	47.116084
2564.824629	193.904238	47.121089
2561.693370	178.481851	47.126093
2558.172752	185.179544	47.131098
2554.923790	176.480205	47.136103
2551.400546	183.624123	47.141108
2548.007643	179.243669	47.146113
2544.562465	171.269682	47.151117
2540.911920	176.991358	47.156122
2537.339623	175.319669	47.161127
2533.500245	175.157236	47.166132
2530.242680	167.676130	47.171137
2526.944528	171.673745	47.176141
2523.193430	179.395521	47.181146
2519.974008	167.327122	47.186151
2516.658999	169.700688	47.191156
2512.913764	171.925068	47.196161
2509.572194	165.524892	47.201165
2505.739668	174.294012	47.206170
2502.525585	166.326003	47.211175
2498.720274	175.998965	47.216180
2495.567741	168.345587	47.221185
2492.184061	168.517407	47.226189
2488.482470	170.418645	47.231194
2484.978466	158.715119	47.236199
2481.388776	166.643054	47.241204
2478.169622	163.351216	47.246209
2474.657989	163.742364	47.251213
2470.901489	160.518002	47.256218
2468.082517	162.724611	47.261223
2464.195191	158.225021	47.266228
2460.455763	156.072539	47.271233
2456.989951	156.478019	47.276237
2453.454531	165.841098	47.281242
2450.282123	158.795694	47.286247
2446.577039	167.001275	47.291252
2443.084121	172.824010	47.296257
2439.593431	157.489100	47.301261
2436.045633	158.314885	47.306266
2433.041366	163.080085	47.311271
2429.460924	165.824857	47.316276
2425.979470	166.288996	47.321281
2422.431676	162.929080	47.326285
2418.560008	160.533708	47.331290
2415.612809	158.776171	47.336295
2412.149491	157.593109	47.341300
2408.370243	154.095710	47.346305
2404.619440	156.149421	47.351309
2401.028047	156.454579	47.356314
2398.013365	157.914755	47.361319
2394.266295	157.013135	47.366324
2390.761700	156.286459	47.371329
2387.181276	156.066870	47.376333
2383.635701	156.205994	47.381338
2380.460217	156.226798	47.386343
2376.826267	162.231201	47.391348
2373.550180	164.308740	47.396353
2370.235484	157.198363	47.401357
2366.465379	162.001047	47.406362
2363.186541	149.758724	47.411367
2359.334986	152.112338	47.416372
2355.730278	153.857534	47.421377
2352.437842	159.030060	47.426381
2348.604299	160.667922	47.431386
2345.526144	150.702203	47.436391
2341.892064	160.725611	47.441396
2338.528249	153.491972	47.446401
2335.230594	152.395598	47.451405
2331.470335	154.066724	47.456410
2327.942680	148.874250	47.461415
2324.343539	154.789849	47.466420
2320.908111	151.516002	47.471425
2317.599324	144.071003	47.476429
2313.444363	150.480642	47.481434
2310.188735	144.308347	47.486439
2306.967457	143.861409	47.491444
2303.390589	152.174523	47.496449
2300.288377	145.476973	47.501453
2296.507487	150.657031	47.506458
2293.218067	138.861330	47.511463
2289.695932	153.891597	47.516468
2286.353547	145.612720	47.521473
2283.110067	141.438441	47.526477
2278.679960	153.449295	47.531482
2275.145661	149.982689	47.536487
2271.601304	152.562361	47.541492
2268.459059	147.957115	47.546497
2265.288038	146.741548	47.551501
2261.403711	145.565201	47.556506
2258.061602	146.128352	47.561511
2254.341092	145.868539	47.566516
2250.958571	148.490291	47.571521
2248.036320	139.100517	47.576525
2244.129928	146.527753	47.581530
2240.427491	145.734913	47.586535
2236.530805	150.821524	47.591540
2233.415592	151.053276	47.596545
2230.302355	140.490215	47.601549
2226.460507	148.915361	47.606554
2223.139300	143.773837	47.611559
2219.631892	149.915270	47.616564
2215.885648	149.595225	47.621569
2212.863376	137.224511	47.626573
2208.794752	140.585110	47.631578
2205.559745	133.975551	47.636583
2202.041608	149.383110	47.641588
2198.423546	153.242148	47.646593
2195.172053	148.454564	47.651597
2191.489149	148.759077	47.656602
2187.922356	141.157426	47.661607
2184.415315	141.594430	47.666612
2181.168043	149.446721	47.671617
2177.816963	145.698838	47.676621
2174.088912	149.978485	47.681626
2170.639320	148.917280	47.686631
2166.879840	143.315009	47.691636
2163.166926	152.519837	47.696641
2160.064905	143.885516	47.701645
2156.333707	148.546558	47.706650
2152.822731	143.898890	47.711655
2149.649725	147.440330	47.716660
2145.723646	141.476336	47.721665
2142.696443	138.097721	47.726669
2139.339832	148.777627	47.731674
2135.840105	139.489532	47.736679
2132.396846	139.467863	47.741684
2128.400146	154.154169	47.746689
2125.049175	136.671532	47.751693
2121.433848	145.031608	47.756698
2118.283404	144.180384	47.761703
2114.532102	138.808483	47.766708
2110.880115	149.320869	47.771713
2107.596567	138.100982	47.776717
2103.699979	135.104026	47.781722
2100.561239	138.823937	47.786727
2097.298669	138.454453	47.791732
2093.550010	147.028255	47.796737
2090.016053	133.519141	47.801741
2086.311711	143.635678	47.806746
2083.266295	139.607930	47.811751
2079.818483	140.332791	47.816756
2076.062139	139.751104	47.821761
2072.342351	136.836775	47.826765
2068.624215	134.337370	47.831770
2065.228704	138.933593	47.836775
2062.182748	140.117984	47.841780
2058.876655	140.670196	47.846785
2055.195144	136.428180	47.851789
2051.313288	140.764001	47.856794
2048.003716	137.881182	47.861799
2044.721328	145.180926	47.866804
2040.927398	139.433723	47.871809
2037.845756	135.187643	47.876813
2033.961128	139.701540	47.881818
2030.625990	134.178083	47.886823
2027.259706	133.791109	47.891828
2023.135131	145.953841	47.896833
2020.198434	129.543867	47.901837
2016.554372	139.720127	47.906842
2013.022862	137.925517	47.911847
2009.192777	138.587090	47.916852
2005.417252	133.258187	47.921857
2002.462264	126.752972	47.926861
1999.337302	139.856937	47.931866
1995.614297	139.783661	47.936871
1992.331875	128.825565	47.941876
1988.531011	133.391729	47.946881
1985.327856	132.661626	47.951885
1981.483677	133.529408	47.956890
1978.047230	135.697164	47.961895
1974.846015	133.888310	47.966900
1971.021574	139.955779	47.971905
1967.739024	134.570677	47.976909
1964.040678	141.037780	47.981914
1960.262210	140.570965	47.986919
1957.014357	134.328620	47.991924
1953.583422	144.697142	47.996929
1949.797785	129.497668	48.001933
1946.381038	142.235815	48.006938
1942.874939	130.489967	48.011943
1939.589551	137.357721	48.016948
1935.878487	137.008422	48.021953
1932.737562	129.987652	48.026957
1928.962965	135.507973	48.031962
1925.663772	128.609342	48.036967
1922.070361	124.629323	48.041972
1918.375895	134.481894	48.046977
1914.936276	132.299180	48.051981
1911.248170	135.617523	48.056986
1907.918661	124.921677	48.061991
1904.853151	133.759717	48.066996
1901.006820	143.689375	48.072001
1897.710523	128.773341	48.077005
1893.894892	137.849766	48.082010
1890.185728	137.883222	48.087015
1886.682738	133.874236	48.092020
1883.307929	120.909068	48.097025
1880.145452	129.424566	48.102029
1876.842887	135.648939	48.107034
1873.359768	123.638282	48.112039
1869.924453	131.908924	48.117044
1865.785684	129.003056	48.122049
1862.404981	129.769862	48.127053
1858.671394	129.429695	48.132058
1855.632019	129.056565	48.137063
1852.117407	124.933309	48.142068
1848.701263	134.661268	48.147073
1844.843919	133.029938	48.152077
1841.148763	132.544691	48.157082
1837.810137	122.585101	48.162087
1834.581376	116.083170	48.167092
1830.781924	129.920630	48.172097
1827.530824	120.846195	48.177101
1823.779122	127.306071	48.182106
1820.486883	130.358190	48.187111
1817.043220	122.570140	48.192116
1813.476902	128.659488	48.197121
1809.824942	125.209255	48.202125
1806.417677	123.331879	48.207130
1802.865008	125.624812	48.212135
1799.201768	117.256899	48.217140
1795.732398	124.038031	48.222145
1792.415023	134.663519	48.227149
1788.895816	123.352561	48.232154
1785.843763	129.160736	48.237159
1782.145076	123.024652	48.242164
1778.347302	122.111679	48.247169
1775.130827	116.712839	48.252173
1770.970434	125.275223	48.257178
1767.689479	121.585537	48.262183
1764.180526	121.663671	48.267188
1760.638925	131.612192	48.272193
1757.603492	124.687357	48.277197
1753.987039	123.227531	48.282202
1750.609700	127.729422	48.287207
1746.890862	115.493936	48.292212
1742.970961	125.398417	48.297217
1740.321753	116.727495	48.302221
1736.406169	121.112600	48.307226
1732.911440	120.744401	48.312231
1729.805186	117.300281	48.317236
1725.848185	118.416899	48.322241
1722.344443	123.108880	48.327245
1718.519316	125.444881	48.332250
1715.249370	120.255249	48.337255
1711.554638	123.526713	48.342260
1708.180875	127.273436	48.347265
1705.182458	123.654971	48.352269
1701.706230	123.646828	48.357274
1697.927203	125.165738	48.362279
1694.133851	113.819617	48.367284
1690.622834	126.757673	48.372289
1687.351072	124.037813	48.377293
1683.854983	126.078155	48.382298
1680.487203	126.174004	48.387303
1677.119303	127.714958	48.392308
1673.330954	131.809274	48.397313
1670.430741	113.287035	48.402317
1666.278118	123.665680	48.407322
1662.619018	131.300470	48.412327
1659.217076	121.081197	48.417332
1655.787509	130.782908	48.422337
1652.154473	130.706872	48.427341
1648.688254	119.816474	48.432346
1644.975507	124.813716	48.437351
1641.746919	115.930095	48.442356
1638.429187	123.145013	48.447361
1634.920312	118.686722	48.452365
1631.036231	124.506653	48.457370
1628.046246	122.136374	48.462375
1624.617086	111.375431	48.467380
1620.926858	121.101040	48.472385
1617.402345	116.488083	48.477389
1613.209035	121.618307	48.482394
1610.049631	116.372157	48.487399
1606.973922	113.099688	48.492404
1603.331687	117.337178	48.497409
1599.963847	111.426047	48.502413
1596.187524	107.644595	48.507418
1592.668171	123.490837	48.512423
1589.491482	108.903785	48.517428
1585.491405	120.192378	48.522433
1582.397460	110.235683	48.527437
1579.011866	117.324156	48.532442
1575.545095	113.272750	48.537447
1571.781414	126.462750	48.542452
1568.421560	120.619583	48.547457
1564.682722	120.388700	48.552461
1560.944770	115.632598	48.557466
1557.745284	114.778502	48.562471
1554.400945	110.624725	48.567476
1550.208487	120.389069	48.572481
1547.010515	113.425061	48.577485
1543.610213	126.577721	48.582490
1540.206353	115.591844	48.587495
1536.873958	119.275208	48.592500
1533.145252	122.881026	48.597505
1530.205291	113.959317	48.602509
1526.156249	117.066707	48.607514
1522.553234	117.488817	48.612519
1519.078873	109.443295	48.617524
1515.720583	116.329165	48.622529
1512.539985	108.766359	48.627533
1508.479706	121.212699	48.632538
1505.058663	117.149038	48.637543
1501.765510	108.404127	48.642548
1497.620289	119.689830	48.647553
1494.762629	112.592870	48.652557
1491.251298	125.723524	48.657562
1487.668026	120.472976	48.662567
1484.178517	121.273335	48.667572
1480.820841	124.918707	48.672577
1477.260997	113.540412	48.677581
1473.843777	111.590977	48.682586
1470.144246	121.020475	48.687591
1466.742007	113.397769	48.692596
1463.031315	120.163731	48.697601
1459.864357	113.873683	48.702605
1456.167759	119.376151	48.707610
1452.384669	115.547417	48.712615
1449.178347	115.674701	48.717620
1445.456554	123.959626	48.722625
1442.075099	120.478893	48.727629
1438.324219	125.587819	48.732634
1434.766106	121.800329	48.737639
1431.447829	118.245390	48.742644
1428.140761	127.569386	48.747649
1424.851160	113.416799	48.752653
1421.221606	128.252939	48.757658
1417.346034	126.567232	48.762663
1414.238456	113.352589	48.767668
1410.552608	118.155738	48.772673
1407.233498	115.176188	48.777677
1403.579936	121.799526	48.782682
1399.779365	120.240520	48.787687
1396.854091	114.269986	48.792692
1392.944573	114.062047	48.797697
1390.031846	112.176818	48.802701
1386.330824	108.711448	48.807706
1382.753098	116.827686	48.812711
1379.284665	108.342248	48.817716
1375.353128	112.237393	48.822721
1371.836528	104.723733	48.827725
1368.352314	109.935107	48.832730
1364.723792	114.247292	48.837735
1361.813876	105.905644	48.842740
1358.125623	118.243840	48.847745
1354.809038	109.380012	48.852749
1351.295991	110.286017	48.857754
1347.492173	117.105017	48.862759
1343.794256	105.772261	48.867764
1340.242175	118.462820	48.872769
1337.139626	108.676097	48.877773
1333.874188	114.582336	48.882778
1329.925494	118.569764	48.887783
1326.526081	113.051288	48.892788
1322.760188	119.577097	48.897793
1319.717680	116.656527	48.902797
1316.085700	110.260811	48.907802
1312.575944	111.117563	48.912807
1309.149336	107.827173	48.917812
1305.036976	119.903846	48.922817
1302.112839	111.997552	48.927821
1298.552226	117.166406	48.932826
1294.961293	119.822905	48.937831
1291.553619	108.458634	48.942836
1287.872892	110.309914	48.947841
1284.319668	112.592929	48.952845
1280.782802	111.100212	48.957850
1277.384770	113.998824	48.962855
1274.160258	102.564133	48.967860
1270.669198	110.190706	48.972865
1266.752943	110.964561	48.977869
1263.449784	115.371061	48.982874
1260.279057	112.694599	48.987879
1256.755799	104.332437	48.992884
1253.117964	111.090635	48.997889
1249.367414	110.067529	49.002893
1245.553655	113.789340	49.007898
1242.230321	112.874154	49.012903
1238.976736	98.637844	49.017908
1235.535326	113.822570	49.022913
1232.073366	110.253559	49.027917
1228.447988	109.754545	49.032922
1224.943026	120.920869	49.037927
1221.739304	110.855821	49.042932
1217.604937	108.550011	49.047937
1214.622110	101.350713	49.052941
1210.956944	108.641150	49.057946
1207.352192	105.429938	49.062951
1203.740026	107.376284	49.067956
1199.895043	114.977370	49.072961
1196.704413	110.272123	49.077965
1193.549695	112.710316	49.082970
1189.963985	114.931710	49.087975
1186.758899	109.903467	49.092980
1182.893297	114.997908	49.097985
1179.791350	108.877881	49.102989
1175.980273	110.725829	49.107994
1172.054341	113.343887	49.112999
1168.527774	113.382056	49.118004
1165.095839	110.735790	49.123009
1162.170162	105.455395	49.128013
1158.591907	107.627430	49.133018
1154.707276	114.610181	49.138023
1151.696609	111.759452	49.143028
1147.682805	117.718958	49.148033
1144.121630	117.430582	49.153037
1141.004616	113.726476	49.158042
1137.617729	112.234068	49.163047
1133.958418	103.671219	49.168052
1130.353747	112.196272	49.173057
1127.198881	117.216057	49.178061
1123.046751	109.513466	49.183066
1119.704259	107.781447	49.188071
1116.574752	102.938061	49.193076
1112.676646	116.638142	49.198081
1109.297453	107.365009	49.203085
1105.787657	110.315066	49.208090
1102.330696	114.187773	49.213095
1099.111612	107.084800	49.218100
1095.024624	110.741582	49.223105
1091.851033	110.719082	49.228109
1088.579556	109.410426	49.233114
1084.708423	117.225723	49.238119
1081.465019	102.170520	49.243124
1077.643005	119.470982	49.248129
1074.231014	105.828643	49.253133
1070.746688	115.488177	49.258138
1066.850580	114.526302	49.263143
1063.781811	109.810027	49.268148
1060.369264	110.906419	49.273153
1056.604879	110.471087	49.278157
1053.257977	109.464466	49.283162
1049.574749	117.479493	49.288167
1046.403244	104.298702	49.293172
1042.708671	109.971692	49.298177
1039.315740	105.088416	49.303181
1035.596415	105.781871	49.308186
1032.122692	107.919702	49.313191
1028.767813	110.234557	49.318196
1024.940171	118.687971	49.323201
1021.394282	113.450027	49.328205
1018.549977	110.671649	49.333210
1014.863248	103.260177	49.338215
1011.385522	96.994080	49.343220
1007.645319	110.791968	49.348225
1004.275695	105.495193	49.353229
1000.641960	107.015511	49.358234
997.037674	108.975734	49.363239
993.917741	105.778595	49.368244
989.889295	114.167288	49.373249
986.835796	115.642634	49.378253
983.233361	107.523380	49.383258
979.886099	110.305678	49.388263
976.423213	96.089762	49.393268
972.791521	107.106218	49.398273
969.243624	99.929274	49.403277
965.737741	110.254321	49.408282
961.737115	104.113924	49.413287
958.784231	107.792786	49.418292
955.169193	115.632791	49.423297
951.643406	109.680787	49.428301
948.215212	112.433327	49.433306
944.644298	114.409570	49.438311
941.507907	112.209172	49.443316
937.346312	108.012606	49.448321
933.979000	103.830444	49.453325
930.835040	103.119400	49.458330
927.089031	113.230169	49.463335
923.501839	110.838996	49.468340
919.827769	96.908803	49.473345
916.537865	95.648150	49.478349
913.120029	109.743073	49.483354
909.341247	105.908256	49.488359
906.353184	112.726049	49.493364
902.850759	108.326976	49.498369
899.276167	99.791357	49.503373
896.360664	102.492984	49.508378
891.992917	104.902266	49.513383
888.363559	99.310483	49.518388
884.924564	110.685156	49.523393
881.459137	104.940270	49.528397
878.017247	112.242876	49.533402
874.700533	112.695217	49.538407
871.504055	105.109575	49.543412
867.557538	106.876109	49.548417
864.073275	106.294224	49.553421
860.677013	106.896335	49.558426
857.139826	111.647083	49.563431
853.605430	102.331885	49.568436
850.055119	102.966679	49.573441
846.579229	103.541369	49.578445
843.065966	106.317395	49.583450
839.265882	102.095467	49.588455
836.111273	105.351078	49.593460
832.723521	106.554257	49.598465
829.083520	111.743796	49.603469
825.331319	105.835618	49.608474
821.841439	101.575240	49.613479
818.719623	99.238145	49.618484
815.420836	100.537669	49.623489
811.539839	109.345264	49.628493
808.160130	109.508962	49.633498
804.280626	104.434358	49.638503
801.185246	91.703726	49.643508
797.649657	106.124144	49.648513
794.374253	101.621384	49.653517
790.457648	99.996212	49.658522
786.627028	106.266648	49.663527
783.482176	106.284032	49.668532
780.182069	108.511664	49.673537
776.622982	108.681094	49.678541
772.868681	112.000790	49.683546
769.243881	101.666072	49.688551
766.238869	108.944194	49.693556
762.012868	107.363903	49.698561
759.090386	104.082878	49.703565
755.668221	101.831809	49.708570
751.635139	104.888981	49.713575
748.885433	97.043793	49.718580
745.131132	108.165053	49.723585
741.530652	104.657782	49.728589
738.300447	93.864112	49.733594
734.562951	95.417493	49.738599
730.837631	87.299968	49.743604
727.328389	101.309162	49.748609
723.731849	91.272714	49.753613
720.477230	88.804622	49.758618
716.885393	95.897621	49.763623
713.672788	92.950343	49.768628
709.716370	96.556436	49.773633
706.209754	98.580630	49.778637
702.939591	97.087192	49.783642
699.649296	96.384653	49.788647
696.036802	94.726849	49.793652
692.497994	102.200995	49.798657
688.804462	103.054880	49.803661
685.666516	102.186162	49.808666
681.796946	100.794829	49.813671
678.476965	91.363312	49.818676
675.010412	99.497984	49.823681
671.347903	101.019046	49.828685
667.658498	95.983871	49.833690
664.137821	100.416904	49.838695
660.958285	88.582259	49.843700
657.163319	101.398915	49.848705
653.843636	92.232587	49.853709
650.630975	94.189867	49.858714
647.001414	102.962767	49.863719
643.729856	99.032757	49.868724
639.757480	104.731123	49.873729
636.174809	99.030809	49.878733
632.747828	99.431024	49.883738
629.309654	106.802480	49.888743
626.025975	93.873980	49.893748
622.331272	101.699276	49.898753
618.650729	105.806658	49.903757
615.608530	95.542113	49.908762
611.622448	101.843855	49.913767
608.328283	94.584495	49.918772
605.081684	105.201450	49.923777
601.518352	96.117266	49.928781
597.878815	99.146147	49.933786
594.233442	102.486206	49.938791
591.209466	100.497924	49.943796
587.286504	101.537610	49.948801
583.481570	105.643975	49.953805
580.499017	89.861232	49.958810
576.726706	98.730317	49.963815
573.123150	97.036418	49.968820
569.798756	95.543618	49.973825
566.056002	97.132964	49.978829
562.764331	99.267421	49.983834
559.034740	104.683027	49.988839
556.385911	104.757346	49.993844
552.560228	98.105091	49.998849
548.766271	113.799770	50.003853
545.032569	104.449514	50.008858
541.525075	113.991963	50.013863
538.333606	100.619035	50.018868
534.533186	109.130530	50.023873
531.059066	108.774793	50.028877
527.856602	93.465709	50.033882
524.108777	103.801493	50.038887
520.573974	90.055625	50.043892
517.037144	100.620796	50.048897
513.595840	94.460436	50.053901
510.624106	92.941680	50.058906
506.980695	97.228884	50.063911
503.835650	91.964946	50.068916
500.059091	97.811682	50.073921
496.293016	96.542079	50.078925
492.806418	98.017913	50.083930
489.237430	92.710537	50.088935
485.782993	91.610988	50.093940
482.103230	95.439931	50.098945
478.583279	96.354581	50.103949
474.921164	96.723741	50.108954
471.606757	97.862764	50.113959
468.184101	89.956321	50.118964
465.015286	96.501343	50.123969
461.370749	105.243544	50.128973
457.884919	99.750312	50.133978
454.032012	107.912639	50.138983
450.683578	93.373005	50.143988
447.282462	98.747771	50.148993
443.472471	91.850314	50.153997
440.188730	94.810181	50.159002
436.311494	95.956288	50.164007
433.254475	93.687692	50.169012
429.571897	90.211144	50.174017
426.195197	92.027140	50.179021
422.666128	97.617750	50.184026
418.931297	106.783661	50.189031
415.840799	94.276952	50.194036
412.536158	93.711432	50.199041
408.855312	93.246293	50.204045
405.199824	90.474085	50.209050
401.350842	100.564920	50.214055
398.044976	82.123349	50.219060
394.840829	102.097578	50.224065
391.186483	101.889913	50.229069
387.981372	89.766942	50.234074
384.126422	104.047938	50.239079
380.711547	95.325109	50.244084
376.594967	97.276486	50.249089
373.242372	95.185108	50.254093
370.165520	93.647619	50.259098
366.651845	93.020961	50.264103
363.515272	88.907369	50.269108
359.761642	84.692641	50.274113
356.230185	92.622279	50.279117
352.774825	83.717365	50.284122
348.861394	97.612255	50.289127
345.515205	99.274466	50.294132
341.853993	101.155166	50.299137
338.419668	95.042560	50.304141
335.325860	84.169405	50.309146
331.373222	103.708389	50.314151
328.209165	94.410757	50.319156
324.567467	92.552944	50.324161
320.907204	88.241444	50.329165
317.774292	82.098523	50.334170
314.013179	96.664324	50.339175
310.575818	87.209852	50.344180
306.729384	90.435979	50.349185
303.379020	97.278870	50.354189
300.230547	100.333402	50.359194
296.280812	98.637890	50.364199
293.097562	86.158950	50.369204
289.454900	98.410921	50.374209
286.199096	97.261192	50.379213
282.649712	83.505779	50.384218
279.086151	99.015777	50.389223
275.595085	85.684416	50.394228
272.054581	86.944254	50.399233
268.095496	101.047688	50.404237
264.878177	87.921860	50.409242
261.109319	97.610769	50.414247
258.468957	88.332953	50.419252
254.895093	89.532639	50.424257
250.926723	99.129598	50.429261
247.444881	93.158374	50.434266
243.718640	97.996129	50.439271
240.345482	93.790335	50.444276
237.028484	90.575091	50.449281
233.450240	99.096318	50.454285
230.039390	86.786285	50.459290
225.883274	89.919896	50.464295
222.799019	82.224861	50.469300
219.234473	80.352955	50.474305
216.028013	87.338749	50.479309
212.917088	88.048146	50.484314
208.944298	95.920414	50.489319
205.895258	84.872212	50.494324
201.998581	88.561443	50.499329
198.559966	87.006068	50.504333
195.066014	87.914296	50.509338
191.189215	98.290946	50.514343
187.587856	84.821919	50.519348
184.365866	96.433592	50.524353
180.794762	94.219456	50.529357
177.419843	85.316155	50.534362
173.892655	91.551944	50.539367
170.202038	92.789267	50.544372
166.993639	94.532535	50.549377
163.433771	89.908124	50.554381
159.989818	88.682229	50.559386
156.338998	99.089243	50.564391
152.972920	93.822884	50.569396
149.072066	89.394467	50.574401
145.954632	84.259662	50.579405
142.715662	81.587621	50.584410
138.815136	84.367859	50.589415
135.592970	81.679811	50.594420
131.843652	89.112856	50.599425
128.400950	87.606376	50.604429
124.911222	82.395130	50.609434
121.151690	86.818218	50.614439
117.880402	83.367574	50.619444
114.760656	80.053956	50.624449
111.234917	86.713820	50.629453
107.230069	81.299701	50.634458
103.489160	92.915975	50.639463
100.574200	82.812119	50.644468
96.990658	86.799087	50.649473
92.933873	88.096945	50.654477
89.905269	82.157316	50.659482
86.255146	88.051511	50.664487
82.715771	78.911021	50.669492
79.254557	90.367958	50.674497
75.597398	87.473823	50.679501
72.308260	85.586285	50.684506
68.877054	88.621691	50.689511
65.452670	76.637713	50.694516
61.678053	83.891509	50.699521
58.418957	86.708882	50.704525
55.317311	87.334187	50.709530
51.075979	94.867239	50.714535
47.710183	96.830943	50.719540
44.417236	97.070894	50.724545
40.533504	91.578703	50.729549
37.083477	88.674058	50.734554
33.649481	89.681794	50.739559
30.341341	79.837724	50.744564
26.684586	88.158863	50.749569
23.224959	87.781068	50.754573
20.253681	90.420201	50.759578
16.428571	95.272832	50.764583
13.008148	89.761483	50.769588
9.419704	95.380288	50.774593
5.345765	95.224397	50.779597
2.240684	84.024880	50.784602