Fri Jun 17 17:48:17 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.723671	92.519253	0.000000
-0.863229	93.738949	0.005005
-0.520712	104.466629	0.010010
-0.809619	108.845949	0.015014
-0.324494	104.601915	0.020019
-0.616090	105.075713	0.025024
-0.606427	102.689841	0.030029
-0.756881	92.967775	0.035034
-1.016189	80.909653	0.040038
-1.319237	69.050814	0.045043
-1.331180	70.035391	0.050048
-2.011869	47.171271	0.055053
-1.941315	48.608821	0.060058
-2.333914	37.091669	0.065062
-2.400543	21.980643	0.070067
-3.236292	24.985458	0.075072
-3.485597	6.716748	0.080077
-3.453189	-0.125631	0.085082
-3.990416	-0.303439	0.090086
-3.991304	-3.619331	0.095091
-4.813122	-14.687611	0.100096
-4.773294	-15.216675	0.105101
-4.847076	-19.487559	0.110106
-5.252998	-17.191961	0.115110
-5.738219	-13.804777	0.120115
-6.102025	-25.521826	0.125120
-6.508175	-20.002027	0.130125
-6.218902	-25.336672	0.135130
-6.353725	-8.940973	0.140134
-6.898641	-25.861490	0.145139
-7.516780	-13.231804	0.150144
-8.054026	-9.531097	0.155149
-7.791441	-20.716862	0.160154
-8.176694	-12.379513	0.165158
-7.940189	-11.181878	0.170163
-7.826482	-14.805113	0.175168
-8.434054	-14.350232	0.180173
-8.632283	-15.513411	0.185178
-9.484688	-18.505829	0.190182
-9.216636	-12.763023	0.195187
-9.424955	-16.512697	0.200192
-10.256925	-3.539233	0.205197
-10.395769	-16.477064	0.210202
-11.006499	-14.095723	0.215206
-10.961672	-26.349544	0.220211
-11.177680	-16.211481	0.225216
-11.374650	-13.532866	0.230221
-11.217239	-13.474292	0.235226
-11.332279	-15.236576	0.240230
-11.480761	-18.995406	0.245235
-12.167903	-12.547627	0.250240
-12.736759	-8.168378	0.255245
-12.651951	-15.248954	0.260250
-13.160661	-5.604297	0.265254
-13.124220	-8.984604	0.270259
-13.393684	-15.198626	0.275264
-14.184434	-7.837748	0.280269
-13.785041	-16.938973	0.285274
-14.156119	-8.035472	0.290278
-14.227579	-9.115137	0.295283
-14.313736	-21.122038	0.300288
-15.407879	-14.963382	0.305293
-15.696819	-6.984011	0.310298
-15.815354	-5.361120	0.315302
-15.582168	-12.555948	0.320307
-15.567023	-7.289685	0.325312
-16.067004	-8.304636	0.330317
-16.000141	-15.327372	0.335322
-17.225265	-18.799703	0.340326
-17.389238	-22.378755	0.345331
-17.312546	-13.334791	0.350336
-17.947843	-17.100122	0.355341
-17.624864	-18.956128	0.360346
-17.944139	-16.395710	0.365350
-17.628100	-23.694877	0.370355
-17.968184	-22.799222	0.375360
-18.818439	-20.998472	0.380365
-18.596767	-24.159547	0.385370
-19.377928	-15.650034	0.390374
-19.166646	-16.794849	0.395379
-19.956017	-22.014539	0.400384
-20.382460	-23.359806	0.405389
-20.285088	-20.437476	0.410394
-20.642303	-14.643430	0.415398
-20.640628	-16.417616	0.420403
-20.691575	-20.167003	0.425408
-21.230797	-15.323827	0.430413
-21.747309	-15.203161	0.435418
-21.854632	-11.092627	0.440422
-21.867079	-4.873018	0.445427
-21.890367	-20.848007	0.450432
-22.233942	-8.906261	0.455437
-23.099386	-24.911167	0.460442
-23.756958	-6.383458	0.465446
-23.151025	-30.996730	0.470451
-23.620147	-23.517642	0.475456
-23.934248	-13.778059	0.480461
-23.867231	-20.720307	0.485466
-23.866636	-16.708617	0.490470
-23.976274	-15.151930	0.495475
-24.668408	-20.532424	0.500480
-24.996358	-23.319568	0.505485
-24.883093	-20.863802	0.510490
-25.220986	-18.158804	0.515494
-26.037755	-19.165101	0.520499
-26.122202	-23.539979	0.525504
-26.621324	-19.743788	0.530509
-26.540404	-11.050194	0.535514
-26.740958	-2.913836	0.540518
-26.738666	-9.770739	0.545523
-26.539155	-19.903528	0.550528
-27.532028	-16.741375	0.555533
-27.733962	-25.341276	0.560538
-27.999549	-16.011324	0.565542
-28.243653	-20.718014	0.570547
-28.464816	-17.099247	0.575552
-29.040569	-20.059107	0.580557
-29.617784	-15.375766	0.585562
-29.895691	-15.459529	0.590566
-29.582472	-20.434677	0.595571
-29.855270	-27.940051	0.600576
-30.086431	-19.699950	0.605581
-30.032527	-30.395189	0.610586
-29.856706	-20.277859	0.615590
-30.323968	-25.801693	0.620595
-30.981315	-20.339594	0.625600
-31.855812	-22.238878	0.630605
-31.633526	-13.910362	0.635610
-31.604555	-8.531159	0.640614
-31.946714	-14.979954	0.645619
-31.781437	-16.658002	0.650624
-32.673223	-19.482452	0.655629
-32.853181	-30.733372	0.660634
-33.346297	-20.050009	0.665638
-33.089397	-26.192074	0.670643
-33.174830	-17.897460	0.675648
-33.819308	-19.149258	0.680653
-34.478440	-16.385732	0.685658
-34.340619	-5.508871	0.690662
-34.765254	-20.068796	0.695667
-34.682641	-18.733501	0.700672
-34.790861	-16.761474	0.705677
-34.897489	-21.990257	0.710682
-35.746901	-17.186291	0.715686
-36.157899	-21.765785	0.720691
-36.123042	-15.731049	0.725696
-36.451577	-6.747202	0.730701
-36.369896	-20.276374	0.735706
-36.488775	-14.919562	0.740710
-36.594585	-22.341401	0.745715
-37.198847	-13.021061	0.750720
-37.708389	-12.854784	0.755725
-38.174917	-24.245142	0.760730
-38.311051	-19.548687	0.765734
-38.192738	-20.286943	0.770739
-38.114462	-19.084321	0.775744
-38.879618	-10.434597	0.780749
-39.265276	-26.906997	0.785754
-39.834463	-15.506127	0.790758
-39.892689	-22.898185	0.795763
-40.044623	-19.791353	0.800768
-40.047178	-16.751185	0.805773
-39.843328	-16.886214	0.810778
-39.981959	-14.149415	0.815782
-40.313608	-23.414065	0.820787
-40.806083	-17.816770	0.825792
-41.061328	-18.061767	0.830797
-41.304627	-28.109106	0.835802
-42.476532	-23.854179	0.840806
-42.893342	-17.368258	0.845811
-42.236845	-17.851829	0.850816
-42.862626	-17.062600	0.855821
-42.577984	-17.070166	0.860826
-43.166419	-7.443238	0.865830
-43.197843	-18.424241	0.870835
-43.108213	-24.216461	0.875840
-43.478273	-23.459674	0.880845
-44.019714	-19.611654	0.885850
-44.335847	-9.927378	0.890854
-44.527698	-20.052536	0.895859
-44.511529	-18.575762	0.900864
-45.295971	-16.720432	0.905869
-45.771282	-20.194649	0.910874
-46.069104	-13.996872	0.915878
-45.833407	-17.401220	0.920883
-45.883797	-17.196220	0.925888
-46.360128	-13.698427	0.930893
-46.232942	-17.357644	0.935898
-46.457806	-13.838702	0.940902
-46.551462	-13.498839	0.945907
-47.356002	-20.748887	0.950912
-47.380766	-17.884596	0.955917
-47.336088	-21.309089	0.960922
-48.279923	-20.458309	0.965926
-48.721114	-14.666287	0.970931
-48.805037	-21.412162	0.975936
-49.380141	-20.462639	0.980941
-49.098376	-22.511888	0.985946
-49.692940	-12.498559	0.990950
-49.474591	-24.408663	0.995955
-49.073510	-19.917930	1.000960
-49.820937	-11.249051	1.005965
-50.369421	-22.226193	1.010970
-50.496967	-19.996399	1.015974
-50.565897	-21.057342	1.020979
-50.581295	-22.490861	1.025984
-51.575095	-15.155231	1.030989
-51.814969	-22.390212	1.035994
-52.169008	-10.776268	1.040998
-52.248861	-20.495191	1.046003
-52.165244	-26.119470	1.051008
-52.756543	-16.570410	1.056013
-52.375667	-15.303045	1.061018
-53.032049	-22.021250	1.066022
-53.619807	-14.321949	1.071027
-53.317129	-14.879906	1.076032
-53.965666	-18.481415	1.081037
-53.624217	-26.406984	1.086042
-54.108350	-16.797991	1.091046
-54.744710	-24.165183	1.096051
-55.155230	-22.377729	1.101056
-55.641382	-12.255735	1.106061
-55.325412	-25.937506	1.111066
-55.462733	-10.488383	1.116070
-55.361054	-14.122839	1.121075
-55.735378	-18.032771	1.126080
-56.617016	-22.957300	1.131085
-56.673149	-18.195212	1.136090
-56.992952	-14.721858	1.141094
-56.960357	-19.627272	1.146099
-57.113727	-14.639653	1.151104
-57.510293	-17.392696	1.156109
-57.548124	-18.980546	1.161114
-58.273826	-17.323032	1.166118
-58.696362	-15.824443	1.171123
-58.521663	-23.200163	1.176128
-58.956453	-22.598766	1.181133
-58.701352	-19.690226	1.186138
-59.048357	-29.243969	1.191142
-59.502954	-22.241475	1.196147
-59.848063	-23.176985	1.201152
-59.990071	-17.213687	1.206157
-60.138317	-23.176916	1.211162
-60.962550	-28.569577	1.216166
-61.434302	-21.732750	1.221171
-61.099248	-29.884775	1.226176
-62.178575	-20.504807	1.231181
-61.633465	-29.428577	1.236186
-61.767425	-24.170097	1.241190
-61.796821	-26.729024	1.246195
-61.574670	-31.659432	1.251200
-62.372060	-28.252125	1.256205
-62.985683	-27.902590	1.261210
-63.425575	-20.828540	1.266214
-63.573323	-23.712726	1.271219
-63.225954	-18.940950	1.276224
-63.546990	-23.472642	1.281229
-63.661371	-19.796443	1.286234
-64.995237	-18.477090	1.291238
-65.017830	-25.599004	1.296243
-64.739731	-28.195824	1.301248
-65.142122	-17.946272	1.306253
-64.697818	-19.972025	1.311258
-65.361196	-16.335199	1.316262
-66.401683	-17.580560	1.321267
-66.669186	-18.975526	1.326272
-67.216856	-20.253080	1.331277
-66.081892	-24.384492	1.336282
-66.524268	-27.893581	1.341286
-66.837914	-25.744738	1.346291
-66.733204	-23.770812	1.351296
-67.784359	-23.837330	1.356301
-67.941833	-30.485135	1.361306
-68.279364	-24.688640	1.366310
-68.455387	-21.738825	1.371315
-68.559089	-25.622108	1.376320
-68.878606	-19.038895	1.381325
-68.884982	-17.229031	1.386330
-69.988551	-17.308346	1.391334
-70.208295	-17.031782	1.396339
-70.229500	-25.938374	1.401344
-70.786550	-19.047308	1.406349
-69.657558	-28.845022	1.411354
-70.440934	-19.810636	1.416358
-70.370012	-21.529239	1.421363
-70.707931	-19.923160	1.426368
-71.579498	-21.479963	1.431373
-71.616682	-22.128041	1.436378
-71.913679	-27.002344	1.441382
-71.765909	-21.996115	1.446387
-72.098227	-16.109515	1.451392
-72.779323	-13.979706	1.456397
-72.831959	-14.826689	1.461402
-72.845456	-14.670248	1.466406
-72.847806	-25.341335	1.471411
-73.725887	-15.736315	1.476416
-74.672145	-7.797846	1.481421
-74.404719	-19.771757	1.486426
-74.712405	-18.015602	1.491430
-74.866459	-16.434561	1.496435
-74.735724	-20.399833	1.501440
-74.965188	-9.533558	1.506445
-74.863807	-20.710874	1.511450
-75.285606	-10.694097	1.516454
-75.910693	-15.236222	1.521459
-76.146014	-23.890950	1.526464
-76.968794	-20.196645	1.531469
-76.753810	-23.231307	1.536474
-76.470700	-16.219622	1.541478
-76.613356	-17.867400	1.546483
-77.288190	-18.816572	1.551488
-77.820061	-10.159250	1.556493
-77.870124	-22.239824	1.561498
-77.886420	-15.928220	1.566502
-78.261482	-20.558672	1.571507
-78.892961	-23.055402	1.576512
-79.723798	-11.600969	1.581517
-79.503320	-18.179394	1.586522
-79.819465	-10.930554	1.591526
-79.928413	-20.573993	1.596531
-79.755798	-23.868993	1.601536
-80.073007	-10.221578	1.606541
-79.725316	-21.622761	1.611546
-79.899682	-16.380255	1.616550
-80.883215	-16.680204	1.621555
-80.939338	-18.301322	1.626560
-81.206469	-17.672540	1.631565
-81.665226	-20.229752	1.636570
-82.300796	-17.467570	1.641574
-82.547935	-11.711158	1.646579
-82.854777	-17.591783	1.651584
-83.059748	-14.468635	1.656589
-82.865561	-16.952055	1.661594
-82.892256	-12.431259	1.666598
-82.840320	-16.975224	1.671603
-82.978072	-16.793983	1.676608
-83.942207	-4.022709	1.681613
-84.106428	-16.378134	1.686618
-84.271968	-17.162936	1.691622
-84.339867	-16.572996	1.696627
-84.828072	-16.612719	1.701632
-85.452158	-9.217576	1.706637
-85.687848	-16.973410	1.711642
-86.114767	-8.091212	1.716646
-85.971506	-22.751837	1.721651
-85.996860	-18.666772	1.726656
-86.029018	-9.377594	1.731661
-86.324662	-26.791405	1.736666
-87.028034	-16.983564	1.741670
-87.732418	-11.701295	1.746675
-87.666723	-17.633390	1.751680
-87.621300	-21.883631	1.756685
-87.636697	-12.784310	1.761690
-88.057758	-15.321740	1.766694
-87.967102	-20.789326	1.771699
-88.314054	-23.309474	1.776704
-88.927428	-12.662748	1.781709
-89.149691	-20.336354	1.786714
-89.291449	-11.205174	1.791718
-89.987176	-4.667552	1.796723
-90.332772	-34.439279	1.801728
-90.890319	-15.210129	1.806733
-90.118445	-18.831873	1.811738
-90.694344	-17.100196	1.816742
-90.875266	-17.857775	1.821747
-90.648264	-26.367555	1.826752
-91.149844	-18.237799	1.831757
-91.999262	-26.394202	1.836762
-92.365718	-24.234408	1.841766
-92.544652	-14.282278	1.846771
-92.295906	-19.690503	1.851776
-92.525660	-18.559220	1.856781
-92.435435	-21.781720	1.861786
-92.986802	-24.985770	1.866790
-94.010764	-23.571703	1.871795
-93.754622	-21.365436	1.876800
-94.275316	-21.906696	1.881805
-94.013909	-28.634786	1.886810
-94.103775	-24.425534	1.891814
-94.279951	-19.289681	1.896819
-94.622601	-24.798896	1.901824
-95.536800	-16.764528	1.906829
-95.793365	-29.556868	1.911834
-95.685242	-20.659628	1.916838
-96.023012	-13.140800	1.921843
-96.010640	-24.422304	1.926848
-96.107154	-16.519523	1.931853
-96.867237	-35.573075	1.936858
-97.172711	-30.405865	1.941862
-97.535637	-24.644614	1.946867
-97.232678	-38.828976	1.951872
-97.529085	-25.067622	1.956877
-97.606920	-29.194957	1.961882
-98.041250	-17.650946	1.966886
-98.532001	-18.558098	1.971891
-98.556601	-23.588974	1.976896
-98.894007	-10.869991	1.981901
-98.727406	-24.542124	1.986906
-99.560844	-21.759283	1.991910
-100.502450	-18.733898	1.996915
-99.786442	-18.919803	2.006912
-99.360722	-20.692573	2.016909
-99.070526	-21.878124	2.026906
-99.299457	-19.107146	2.036902
-98.324920	-25.416739	2.046899
-98.073717	-28.530923	2.056896
-96.983960	-25.092611	2.066893
-96.887070	-21.194456	2.076890
-95.750843	-21.711156	2.086886
-95.424920	-20.479701	2.096883
-95.220324	-23.884092	2.106880
-94.998149	-23.577856	2.116877
-94.126103	-28.530409	2.126874
-93.787889	-24.513712	2.136870
-93.066101	-21.886750	2.146867
-92.081987	-23.166316	2.156864
-92.389220	-29.226080	2.166861
-92.086012	-25.831874	2.176858
-91.184195	-23.799132	2.186854
-90.536689	-25.202936	2.196851
-90.177429	-24.314295	2.206848
-89.026743	-19.516668	2.216845
-88.854627	-25.129761	2.226842
-88.717149	-26.816875	2.236838
-88.867677	-22.107812	2.246835
-87.408950	-24.655320	2.256832
-86.865760	-25.792632	2.266829
-86.809566	-29.225304	2.276826
-85.978684	-26.689186	2.286822
-85.510403	-22.296575	2.296819
-85.301701	-24.238752	2.306816
-84.620536	-21.661148	2.316813
-84.029373	-24.550686	2.326810
-83.855109	-17.438090	2.336806
-82.903970	-11.481663	2.346803
-82.469419	-18.903383	2.356800
-82.503821	-14.128661	2.366797
-81.705352	-12.285010	2.376794
-81.287066	-20.295585	2.386790
-80.452309	-19.116112	2.396787
-79.529230	-14.701494	2.406784
-79.605852	-18.157930	2.416781
-79.776380	-23.411765	2.426778
-78.788068	-16.876676	2.436774
-77.869383	-19.208551	2.446771
-77.714625	-16.714149	2.456768
-76.681049	-17.084561	2.466765
-76.574931	-17.564770	2.476762
-76.620460	-15.740467	2.486758
-75.608929	-16.244533	2.496755
-75.014385	-17.181339	2.506752
-74.740435	-20.204664	2.516749
-73.513606	-21.673548	2.526746
-73.424569	-24.384777	2.536742
-73.518357	-26.754819	2.546739
-72.885127	-25.275703	2.556736
-72.032453	-15.718575	2.566733
-71.752141	-16.872450	2.576730
-70.941114	-13.531435	2.586726
-70.514412	-19.877794	2.596723
-70.321597	-17.846528	2.606720
-69.415002	-21.278106	2.616717
-69.040849	-19.882177	2.626714
-68.848075	-14.912466	2.636710
-68.041399	-14.863233	2.646707
-67.487092	-12.621369	2.656704
-67.278335	-16.209808	2.666701
-66.137857	-16.793988	2.676698
-65.904726	-14.498934	2.686694
-65.572584	-15.892595	2.696691
-65.468117	-15.778400	2.706688
-64.509680	-24.553898	2.716685
-64.113913	-16.273265	2.726682
-63.363164	-18.353756	2.736678
-62.483283	-19.593068	2.746675
-62.456129	-18.632029	2.756672
-62.525129	-19.909416	2.766669
-62.038642	-18.400767	2.776666
-61.147069	-14.021213	2.786662
-60.508903	-10.364572	2.796659
-59.537705	-17.984956	2.806656
-59.292171	-15.297589	2.816653
-59.431567	-15.354073	2.826650
-58.623392	-19.423089	2.836646
-57.897578	-15.318478	2.846643
-57.760750	-15.662916	2.856640
-56.815336	-16.463425	2.866637
-56.217548	-13.907518	2.876634
-56.253474	-19.931381	2.886630
-55.921996	-14.219885	2.896627
-55.119031	-13.884131	2.906624
-54.718885	-17.315890	2.916621
-53.477998	-17.815793	2.926618
-53.521280	-20.045058	2.936614
-52.970284	-18.785414	2.946611
-52.811046	-15.056276	2.956608
-52.111820	-15.359446	2.966605
-51.588392	-23.127281	2.976602
-51.289533	-13.989232	2.986598
-50.440347	-16.233677	2.996595
-49.878336	-18.866844	3.006592
-49.544873	-13.906488	3.016589
-48.944306	-18.396420	3.026586
-48.630879	-17.904803	3.036582
-48.368847	-18.143007	3.046579
-47.340202	-16.201277	3.056576
-47.115942	-16.722660	3.066573
-46.471384	-19.153986	3.076570
-45.688802	-18.861273	3.086566
-45.749402	-19.139305	3.096563
-45.450991	-16.015969	3.106560
-44.248683	-12.919589	3.116557
-44.053120	-16.605218	3.126554
-43.519057	-14.565075	3.136550
-42.720674	-16.465185	3.146547
-42.162372	-17.593345	3.156544
-42.365039	-16.069920	3.166541
-41.652852	-18.051726	3.176538
-41.118045	-16.488076	3.186534
-40.554020	-17.332868	3.196531
-39.610394	-18.153228	3.206528
-39.382419	-20.772165	3.216525
-39.461047	-23.455130	3.226522
-38.378816	-14.746036	3.236518
-37.681010	-14.725921	3.246515
-37.701744	-22.364776	3.256512
-37.259613	-20.006261	3.266509
-36.328373	-14.495222	3.276506
-36.037552	-12.309730	3.286502
-35.576618	-14.786602	3.296499
-34.547437	-17.373734	3.306496
-34.261975	-13.134672	3.316493
-34.136880	-10.373145	3.326490
-33.735604	-13.524920	3.336486
-33.045312	-21.901777	3.346483
-32.651887	-20.823597	3.356480
-31.358436	-15.717543	3.366477
-31.439966	-12.730610	3.376474
-31.165740	-18.622079	3.386470
-30.585266	-18.134542	3.396467
-29.727716	-22.987268	3.406464
-29.399413	-21.971566	3.416461
-29.281829	-23.483280	3.426458
-28.544485	-16.522161	3.436454
-27.884461	-22.147596	3.446451
-27.795195	-18.458593	3.456448
-26.745272	-23.320374	3.466445
-26.494677	-22.476890	3.476442
-26.105764	-23.166516	3.486438
-25.014769	-23.452013	3.496435
-24.687365	-17.225135	3.506432
-24.590553	-20.813934	3.516429
-24.280884	-19.671843	3.526426
-23.837756	-24.841759	3.536422
-23.057958	-19.853242	3.546419
-21.905622	-25.805309	3.556416
-21.477224	-24.627037	3.566413
-21.673506	-29.300052	3.576410
-21.598106	-23.452139	3.586406
-20.797857	-22.268694	3.596403
-19.804822	-23.001829	3.606400
-18.977478	-24.190117	3.616397
-18.860200	-21.391332	3.626394
-18.652766	-25.441693	3.636390
-18.138381	-22.228196	3.646387
-17.143160	-20.495871	3.656384
-17.125241	-28.862127	3.666381
-16.527612	-25.531470	3.676378
-15.501414	-24.699340	3.686374
-15.403639	-21.110344	3.696371
-15.130833	-30.563382	3.706368
-14.441837	-27.914553	3.716365
-13.738577	-26.418811	3.726362
-13.978592	-22.689105	3.736358
-12.946445	-21.899851	3.746355
-12.166461	-20.630249	3.756352
-11.904882	-21.375370	3.766349
-11.350411	-23.256270	3.776346
-11.087373	-23.653889	3.786342
-10.522917	-19.565522	3.796339
-9.566178	-21.782785	3.806336
-8.918972	-24.813415	3.816333
-9.017521	-18.108521	3.826330
-9.040610	-22.825934	3.836326
-8.182191	-23.076721	3.846323
-7.465721	-24.297949	3.856320
-6.398664	-20.412063	3.866317
-6.403467	-19.917143	3.876314
-6.016413	-21.874340	3.886310
-5.830718	-23.326640	3.896307
-5.110408	-21.403198	3.906304
-4.462398	-19.553292	3.916301
-4.237805	-3.232632	3.926298
-3.931117	7.915919	3.936294
-3.126125	24.412408	3.946291
-2.682492	28.149220	3.956288
-2.220805	44.803164	3.966285
-1.901048	60.446370	3.976282
-1.636781	74.830725	3.986278
-1.304977	96.513073	3.996275
-0.527691	124.645230	4.006272
0.000000	138.176563	4.011277
0.105821	147.467181	4.016282
0.366209	161.334677	4.021286
0.079859	149.070838	4.026291
0.593882	178.931359	4.031296
0.635451	182.150910	4.036301
0.421005	191.495970	4.041306
0.595221	179.515490	4.046310
0.700162	176.414624	4.051315
0.358100	185.357812	4.056320
0.715947	192.651798	4.061325
0.960889	199.917983	4.066330
1.098875	204.844618	4.071334
1.493304	197.571981	4.076339
0.627746	188.257607	4.081344
0.701047	185.533179	4.086349
1.046184	191.974830	4.091354
0.908940	198.944012	4.096358
1.252082	191.171970	4.101363
0.659837	188.466797	4.106368
0.815621	203.136506	4.111373
1.233639	197.789464	4.116378
0.819456	214.177763	4.121382
1.228507	210.605829	4.126387
1.240057	218.768421	4.131392
1.551043	214.390502	4.136397
0.955169	196.113458	4.141402
0.919595	195.873381	4.146406
1.260203	193.537668	4.151411
0.799888	197.786255	4.156416
0.996293	198.151319	4.161421
1.313570	206.905406	4.166426
0.934679	224.404751	4.171430
1.001490	201.189424	4.176435
1.417693	217.107402	4.181440
1.484217	218.267794	4.186445
1.313318	217.813608	4.191450
0.931905	218.705882	4.196454
1.357616	217.344655	4.201459
1.120301	227.821884	4.206464
1.491188	219.510249	4.211469
1.499941	214.991940	4.216474
1.164168	221.427983	4.221478
1.221408	220.056564	4.226483
1.283768	224.013652	4.231488
1.306307	226.381136	4.236493
1.124633	221.184277	4.241498
1.253334	232.519849	4.246502
1.449110	225.220031	4.251507
1.592720	230.884158	4.256512
1.562300	219.324037	4.261517
1.385616	225.080469	4.266522
1.224521	233.075023	4.271526
1.601638	229.049397	4.276531
1.285948	227.081661	4.281536
1.427004	222.888863	4.286541
1.297934	231.517845	4.291546
1.202604	231.480691	4.296550
1.544684	228.191809	4.301555
1.152415	226.698757	4.306560
1.506424	225.125475	4.311565
1.169716	221.166794	4.316570
1.301961	222.342903	4.321574
1.379658	226.685595	4.326579
1.515889	218.950297	4.331584
1.818995	226.513482	4.336589
1.811740	217.520755	4.341594
1.669279	229.202326	4.346598
1.592570	213.719434	4.351603
1.404389	225.084976	4.356608
1.429392	218.291682	4.361613
1.700644	225.277241	4.366618
1.379767	232.764173	4.371622
1.559317	227.067813	4.376627
1.603788	239.934482	4.381632
1.996496	244.529109	4.386637
1.726589	241.821657	4.391642
1.615671	246.569452	4.396646
1.592170	242.083334	4.401651
1.622045	262.382025	4.406656
1.528412	251.474903	4.411661
1.989301	258.103358	4.416666
1.868670	256.180157	4.421670
1.867597	256.973895	4.426675
1.798886	252.676439	4.431680
1.828609	251.500018	4.436685
1.751716	252.895001	4.441690
1.745640	260.631149	4.446694
2.049303	254.901521	4.451699
1.840695	252.525659	4.456704
1.874711	256.336112	4.461709
1.975527	260.444091	4.466714
1.980282	254.642785	4.471718
1.717536	248.428525	4.476723
1.893381	253.452680	4.481728
2.001843	250.763245	4.486733
1.915946	254.628950	4.491738
2.028447	260.185186	4.496742
1.955474	251.809963	4.501747
1.769634	255.159679	4.506752
1.968426	265.956352	4.511757
2.143472	260.381102	4.516762
2.046558	259.550735	4.521766
1.963924	260.387827	4.526771
1.773942	256.604845	4.531776
2.264423	251.597979	4.536781
2.199193	252.239383	4.541786
2.066192	259.801662	4.546790
2.320709	249.689153	4.551795
2.168146	254.968777	4.556800
1.962907	251.640028	4.561805
2.137870	254.169649	4.566810
2.173138	253.848928	4.571814
2.256808	257.442349	4.576819
2.147820	257.349647	4.581824
2.291566	254.508320	4.586829
2.427040	260.371143	4.591834
2.558424	264.769845	4.596838
2.457084	250.535195	4.601843
2.215730	259.150098	4.606848
2.260367	262.828349	4.611853
2.445984	253.686920	4.616858
2.177544	255.458481	4.621862
2.217129	254.023690	4.626867
2.254117	260.353985	4.631872
2.653444	254.922413	4.636877
2.473954	255.033039	4.641882
2.319414	253.412264	4.646886
2.310816	247.413282	4.651891
1.888234	260.882502	4.656896
2.255085	250.387440	4.661901
2.333975	258.988187	4.666906
2.010452	255.159125	4.671910
2.407048	250.671852	4.676915
2.078006	260.631550	4.681920
2.112989	261.700495	4.686925
2.084884	260.039563	4.691930
2.121371	281.494340	4.696934
2.497579	279.806659	4.701939
2.620985	290.228119	4.706944
2.437876	284.330944	4.711949
2.927821	290.352126	4.716954
2.699889	299.379023	4.721958
3.066581	292.960275	4.726963
2.784654	276.859835	4.731968
2.365210	273.441377	4.736973
2.326254	268.430151	4.741978
2.187879	279.346020	4.746982
2.795865	282.403961	4.751987
2.764289	296.535593	4.756992
2.661362	292.047664	4.761997
2.746357	300.975586	4.767002
2.995741	293.854687	4.772006
2.557158	272.828604	4.777011
2.560016	277.244330	4.782016
2.704564	279.572994	4.787021
2.852147	283.048647	4.792026
2.604357	295.668729	4.797030
2.747061	291.215750	4.802035
2.858969	294.159404	4.807040
2.600680	297.469075	4.812045
2.771051	297.382825	4.817050
2.472378	294.206546	4.822054
2.839603	303.897021	4.827059
2.897680	294.235086	4.832064
3.001695	293.815716	4.837069
3.075938	293.496409	4.842074
2.454999	299.143977	4.847078
2.988580	293.317513	4.852083
3.029336	298.726045	4.857088
3.009029	290.996602	4.862093
2.609498	288.688777	4.867098
2.177731	298.197894	4.872102
2.296947	296.771965	4.877107
2.479752	301.467011	4.882112
2.368419	301.096853	4.887117
2.598169	304.889387	4.892122
2.765867	324.493924	4.897126
2.476468	327.697080	4.902131
2.789667	332.098537	4.907136
2.969816	326.773818	4.912141
2.816690	322.052885	4.917146
2.763601	340.050940	4.922150
3.007375	324.192227	4.927155
2.989053	331.329564	4.932160
2.934989	335.482842	4.937165
3.471740	338.900731	4.942170
3.021103	343.479665	4.947174
3.129908	329.738671	4.952179
3.052539	332.172506	4.957184
2.900336	338.502704	4.962189
3.205304	350.588929	4.967194
3.195330	362.315673	4.972198
3.176605	356.657155	4.977203
3.339494	370.142823	4.982208
3.078510	363.488168	4.987213
3.272462	366.937583	4.992218
3.177496	364.750412	4.997222
3.758737	369.391884	5.002227
3.206465	346.328373	5.007232
3.177869	341.581211	5.012237
3.293347	338.158091	5.017242
2.860867	354.490379	5.022246
3.412455	354.899618	5.027251
3.666029	373.353694	5.032256
3.404721	357.613626	5.037261
3.383568	342.865913	5.042266
3.294683	345.830519	5.047270
3.267104	335.072791	5.052275
3.013261	366.119799	5.057280
3.741139	366.288196	5.062285
3.574667	361.994723	5.067290
3.205719	361.230878	5.072294
3.341647	359.383028	5.077299
3.748955	366.123050	5.082304
3.601325	360.095036	5.087309
3.871718	345.405621	5.092314
3.081178	344.028283	5.097318
3.399426	338.229107	5.102323
3.461217	340.816625	5.107328
3.576671	363.606379	5.112333
3.863793	368.578727	5.117338
3.513245	351.107091	5.122342
3.346604	337.175269	5.127347
3.528277	349.331516	5.132352
3.261659	365.260326	5.137357
3.793887	364.359524	5.142362
3.395569	381.599031	5.147366
3.590804	372.889674	5.152371
3.466982	381.226207	5.157376
3.360601	374.308852	5.162381
3.580665	369.478319	5.167386
3.526618	379.030871	5.172390
3.516222	375.118357	5.177395
3.523334	376.279953	5.182400
3.271654	377.873114	5.187405
3.868638	378.772289	5.192410
3.705989	383.370856	5.197414
3.535252	379.156430	5.202419
3.617456	378.906247	5.207424
3.332898	375.728394	5.212429
3.853992	382.442011	5.217434
3.685055	401.036201	5.222438
3.908732	398.073819	5.227443
3.814799	409.006073	5.232448
3.996377	412.050848	5.237453
4.154969	399.487500	5.242458
3.827333	398.054926	5.247462
3.685567	377.077837	5.252467
3.780262	385.673068	5.257472
3.666062	400.497951	5.262477
4.018721	398.425225	5.267482
4.055857	407.086275	5.272486
4.194676	396.071150	5.277491
3.925708	395.128871	5.282496
3.946592	393.298955	5.287501
3.768483	392.273296	5.292506
3.588914	401.759897	5.297510
3.817182	399.820524	5.302515
3.585546	404.880092	5.307520
3.522175	405.577829	5.312525
3.740772	402.012445	5.317530
3.484780	413.329998	5.322534
4.057715	421.300920	5.327539
3.854874	426.464638	5.332544
3.901963	437.921670	5.337549
4.149168	436.019204	5.342554
3.629179	435.863386	5.347558
3.928846	429.809545	5.352563
4.040128	439.129623	5.357568
3.662671	448.383136	5.362573
3.787211	437.614656	5.367578
4.078800	442.842624	5.372582
4.301909	435.313203	5.377587
4.133661	434.988021	5.382592
3.957720	436.422374	5.387597
4.108749	434.998644	5.392602
4.313473	467.776044	5.397606
4.292360	456.159143	5.402611
4.184484	450.868638	5.407616
4.077721	464.959640	5.412621
4.397355	463.446710	5.417626
4.306474	461.773299	5.422630
4.307619	477.721657	5.427635
4.636346	463.710741	5.432640
4.142010	463.628607	5.437645
4.434493	459.840768	5.442650
4.322157	474.396049	5.447654
4.750671	462.735392	5.452659
4.565700	454.866290	5.457664
4.335883	455.572947	5.462669
4.171017	450.122798	5.467674
4.134089	452.573017	5.472678
4.422016	471.329935	5.477683
4.458203	469.936341	5.482688
4.161172	469.694526	5.487693
4.746159	476.964709	5.492698
4.430316	468.196386	5.497702
4.393109	480.007272	5.502707
4.129830	468.847976	5.507712
4.365901	468.812770	5.512717
4.484747	465.076878	5.517722
4.271855	477.488051	5.522726
4.646827	469.381622	5.527731
4.757978	475.071164	5.532736
4.460884	476.520526	5.537741
4.560270	470.985995	5.542746
4.412982	476.570491	5.547750
4.572091	474.715420	5.552755
4.961218	467.827752	5.557760
4.975867	479.596077	5.562765
4.769876	469.419463	5.567770
4.784171	475.020318	5.572774
4.545865	467.839106	5.577779
4.923323	479.589359	5.582784
5.097598	479.655593	5.587789
5.020973	469.789198	5.592794
4.962790	475.394009	5.597798
4.916037	468.468477	5.602803
4.605232	457.173626	5.607808
4.636095	462.570835	5.612813
4.663162	461.268348	5.617818
4.624146	462.093069	5.622822
4.452699	471.403129	5.627827
4.922328	475.016714	5.632832
4.749409	476.978836	5.637837
4.809485	473.865832	5.642842
4.812850	481.981576	5.647846
4.714739	475.940747	5.652851
4.978524	472.221809	5.657856
4.525480	472.461573	5.662861
4.816507	471.200461	5.667866
4.733540	479.242739	5.672870
4.545460	476.403835	5.677875
4.698121	472.827688	5.682880
4.586402	482.935917	5.687885
4.952443	490.916201	5.692890
4.380674	501.536623	5.697894
4.899782	500.090979	5.702899
5.273932	508.554977	5.707904
5.081986	506.785680	5.712909
5.238489	513.988173	5.717914
5.050451	509.169778	5.722918
5.247207	514.756897	5.727923
5.123085	512.692558	5.732928
4.772663	518.329973	5.737933
5.132175	511.941337	5.742938
5.059572	502.684614	5.747942
5.186639	518.096050	5.752947
5.266074	512.785837	5.757952
5.314485	514.897659	5.762957
5.445528	500.343346	5.767962
5.076505	510.859036	5.772966
4.653066	513.165514	5.777971
4.881246	514.234926	5.782976
4.703315	513.577064	5.787981
4.741434	508.617479	5.792986
4.915083	514.420969	5.797990
5.181047	520.809021	5.802995
5.229446	525.812020	5.808000
5.132079	548.967958	5.813005
5.572847	542.366890	5.818010
5.589218	537.160490	5.823014
5.227241	519.761998	5.828019
5.048047	514.631721	5.833024
5.247937	526.963670	5.838029
5.539788	539.138854	5.843034
5.352286	541.169713	5.848038
5.573108	544.132017	5.853043
5.767629	521.185069	5.858048
5.364276	521.785791	5.863053
5.722076	510.013912	5.868058
5.579811	516.604791	5.873062
5.037064	506.551810	5.878067
5.513269	510.420650	5.883072
5.223511	517.671861	5.888077
5.311017	512.261835	5.893082
5.153460	517.762409	5.898086
5.319452	539.635487	5.903091
5.770178	532.631188	5.908096
5.343811	549.267154	5.913101
5.721509	546.610275	5.918106
5.525231	554.915332	5.923110
5.940697	538.449470	5.928115
5.327951	533.900770	5.933120
5.328698	538.002565	5.938125
5.634844	535.542287	5.943130
5.379193	553.681806	5.948134
5.354010	543.442925	5.953139
5.738510	545.483499	5.958144
5.657785	546.936965	5.963149
5.450163	550.083753	5.968154
5.205829	549.161247	5.973158
5.452419	541.172419	5.978163
5.558985	543.275764	5.983168
5.409756	547.967660	5.988173
5.578920	550.351870	5.993178
5.503801	559.910008	5.998182
5.723713	564.889841	6.003187
5.837231	577.209743	6.008192
5.690612	581.139692	6.013197
5.735610	578.846543	6.018202
5.537644	590.985369	6.023206
5.678650	581.446818	6.028211
6.075256	583.341723	6.033216
5.858030	580.290377	6.038221
5.848164	575.892868	6.043226
5.726936	576.465447	6.048230
5.490696	590.412320	6.053235
5.710724	579.574985	6.058240
5.414251	579.760705	6.063245
5.865255	587.977535	6.068250
5.548256	581.275657	6.073254
5.896569	582.283074	6.078259
6.025518	573.456156	6.083264
5.791073	586.917674	6.088269
5.772532	586.405987	6.093274
5.562916	592.894031	6.098278
5.722275	583.000774	6.103283
6.060558	581.647931	6.108288
5.665828	582.909485	6.113293
5.532543	577.809840	6.118298
5.728269	592.938996	6.123302
5.722972	586.087626	6.128307
6.012466	580.447852	6.133312
5.864309	587.665890	6.138317
5.775843	585.843667	6.143322
5.839383	579.399214	6.148326
5.920288	581.118667	6.153331
6.058109	578.002192	6.158336
6.152256	581.684921	6.163341
5.875003	567.432448	6.168346
5.637834	557.888489	6.173350
5.701770	551.799779	6.178355
5.848327	556.835216	6.183360
5.909835	565.917762	6.188365
6.011934	548.612208	6.193370
5.652244	552.966120	6.198374
5.634698	545.520059	6.203379
5.930724	544.988256	6.208384
5.466691	549.103761	6.213389
5.757458	550.791882	6.218394
5.669192	562.074758	6.223398
5.789363	568.782475	6.228403
5.983091	573.212935	6.233408
5.719237	566.751467	6.238413
5.899592	561.118591	6.243418
5.739835	554.949053	6.248422
5.731583	550.340330	6.253427
5.901879	544.306368	6.258432
5.674804	543.089923	6.263437
5.704086	546.413418	6.268442
5.791755	542.990731	6.273446
5.669714	545.435378	6.278451
5.611001	546.735407	6.283456
5.841239	569.905797	6.288461
6.212950	572.491768	6.293466
5.835917	566.730910	6.298470
5.464960	559.744767	6.303475
5.545265	555.669722	6.308480
5.615878	575.536595	6.313485
5.657678	564.362241	6.318490
5.758317	582.467835	6.323494
5.896801	593.350144	6.328499
6.009189	581.525660	6.333504
6.073922	586.360398	6.338509
5.770315	571.178109	6.343514
5.709661	559.777471	6.348518
5.783679	555.332281	6.353523
5.827810	538.710475	6.358528
6.022143	554.994441	6.363533
6.009234	550.418658	6.368538
5.491388	549.879846	6.373542
6.007246	554.321093	6.378547
6.261432	548.870524	6.383552
5.903767	551.431296	6.388557
5.679498	545.005488	6.393562
5.481856	561.761123	6.398566
5.489132	550.863856	6.403571
5.653173	554.306247	6.408576
5.748951	549.133414	6.413581
5.767997	548.173053	6.418586
5.679323	547.625071	6.423590
5.279997	550.424835	6.428595
5.753859	558.481561	6.433600
5.766848	582.660158	6.438605
5.881729	579.826333	6.443610
5.854779	588.225219	6.448614
5.753598	583.323296	6.453619
6.050794	572.718825	6.458624
5.497592	568.928844	6.463629
5.992721	565.513220	6.468634
5.833947	549.873133	6.473638
5.651161	551.780071	6.478643
5.778416	556.693802	6.483648
5.876032	561.502741	6.488653
5.898736	549.255693	6.493658
5.660251	544.897572	6.498662
5.372409	552.117104	6.503667
5.888700	571.543442	6.508672
5.676251	585.196074	6.513677
5.893027	573.220846	6.518682
5.981062	573.713651	6.523686
5.659153	562.960087	6.528691
6.036242	554.843198	6.533696
5.858689	556.482073	6.538701
5.885678	541.253548	6.543706
5.444145	543.520413	6.548710
5.514461	553.941008	6.553715
6.034738	556.475249	6.558720
5.772849	562.039948	6.563725
5.656852	561.391524	6.568730
5.721466	554.275168	6.573734
5.478279	573.961338	6.578739
6.012532	581.813858	6.583744
6.191101	583.356447	6.588749
6.030975	569.126933	6.593754
5.729418	555.627404	6.598758
5.651298	559.517546	6.603763
5.806653	545.476961	6.608768
5.523539	553.194574	6.613773
5.572663	551.033945	6.618778
5.482097	564.524021	6.623782
5.891798	577.860314	6.628787
6.041593	579.905565	6.633792
5.653920	575.900601	6.638797
5.615509	576.765682	6.643802
5.885705	578.021110	6.648806
5.994415	591.558602	6.653811
5.959878	558.782422	6.658816
5.563889	558.759126	6.663821
5.527535	562.893339	6.668826
5.740554	568.739641	6.673830
5.827354	584.829966	6.678835
5.847679	580.018161	6.683840
5.394991	591.205337	6.688845
5.477871	586.101138	6.693850
5.795899	598.518492	6.698854
5.941113	599.204854	6.703859
6.085353	597.853674	6.708864
5.560127	599.878511	6.713869
5.418374	599.308960	6.718874
6.078337	588.752323	6.723878
5.683670	601.409695	6.728883
6.069719	589.613129	6.733888
5.918375	596.551483	6.738893
6.133166	587.585177	6.743898
6.059819	584.561224	6.748902
5.619613	559.917634	6.753907
5.411208	562.656265	6.758912
5.458853	568.482297	6.763917
5.916276	587.721893	6.768922
6.012272	593.709411	6.773926
5.992439	585.897453	6.778931
5.763761	562.531387	6.783936
5.716304	568.164247	6.788941
5.646003	561.803813	6.793946
5.690559	564.647810	6.798950
5.713317	576.260543	6.803955
5.978370	578.285059	6.808960
5.813472	582.458009	6.813965
5.941119	581.987145	6.818970
5.426235	568.023997	6.823974
5.416696	576.538385	6.828979
6.011422	585.019833	6.833984
5.914719	600.785073	6.838989
6.194635	582.205518	6.843994
5.560052	567.967444	6.848998
5.388598	562.601231	6.854003
5.480175	578.157946	6.859008
5.723269	589.830763	6.864013
5.865948	590.844731	6.869018
6.146211	591.531340	6.874022
5.931939	589.111572	6.879027
5.784066	568.128135	6.884032
5.749131	567.556223	6.889037
6.066564	571.299124	6.894042
5.845410	559.515886	6.899046
5.566097	566.900559	6.904051
5.851403	550.368898	6.909056
5.832889	553.008476	6.914061
5.889148	551.209761	6.919066
5.634736	552.788593	6.924070
5.518166	558.754003	6.929075
6.133600	559.164280	6.934080
5.734621	561.116427	6.939085
5.765947	549.532576	6.944090
5.869855	546.404378	6.949094
5.711198	552.932678	6.954099
5.978000	553.903122	6.959104
5.728989	553.363043	6.964109
5.510607	563.554963	6.969114
5.706283	561.842201	6.974118
5.387246	566.848267	6.979123
5.763675	561.965045	6.984128
5.732493	585.394400	6.989133
5.953646	590.089869	6.994138
6.225589	589.337893	6.999142
6.135091	569.205702	7.004147
6.211818	554.910588	7.009152
5.982459	558.430602	7.014157
5.973095	553.911259	7.019162
5.781144	561.405337	7.024166
5.533426	561.779698	7.029171
5.480071	557.834811	7.034176
5.372610	554.786736	7.039181
5.458552	559.089473	7.044186
5.766554	559.882373	7.049190
5.027416	562.968122	7.054195
5.899890	575.179243	7.059200
5.507342	587.499988	7.064205
5.468176	587.914280	7.069210
5.454721	585.762469	7.074214
5.518802	589.030855	7.079219
5.858961	590.261040	7.084224
5.614527	586.615888	7.089229
6.076537	600.183073	7.094234
5.916678	595.762536	7.099238
5.860904	598.356020	7.104243
5.812590	592.199123	7.109248
5.865422	605.490166	7.114253
6.044869	596.125188	7.119258
6.222762	602.842270	7.124262
6.028029	601.143678	7.129267
5.911366	577.242146	7.134272
5.993279	572.647044	7.139277
5.784471	567.055760	7.144282
6.049671	557.365352	7.149286
5.435924	571.252012	7.154291
5.545161	554.943001	7.159296
5.426173	576.064480	7.164301
5.712615	584.305503	7.169306
6.047325	589.323886	7.174310
6.051546	576.030844	7.179315
5.764835	567.491862	7.184320
5.577412	562.698212	7.189325
6.012689	557.075262	7.194330
5.813368	560.732366	7.199334
5.680107	561.661362	7.204339
5.333292	561.830387	7.209344
5.385865	573.598203	7.214349
5.681816	592.011554	7.219354
5.894800	588.334579	7.224358
5.940588	598.570824	7.229363
5.905280	595.692496	7.234368
5.934061	602.647091	7.239373
5.874462	591.563375	7.244378
5.754417	576.297882	7.249382
5.797270	578.851685	7.254387
5.972827	568.357222	7.259392
5.573146	571.056210	7.264397
5.427683	570.042084	7.269402
5.487532	577.488793	7.274406
5.579843	590.336357	7.279411
6.001284	584.609332	7.284416
5.602220	595.628545	7.289421
5.721386	593.963622	7.294426
5.929929	590.630949	7.299430
5.633594	587.096645	7.304435
6.063612	587.846376	7.309440
5.870740	585.244264	7.314445
5.841529	587.811033	7.319450
5.978276	591.429455	7.324454
6.073415	590.416187	7.329459
6.164483	569.077295	7.334464
5.800105	571.593996	7.339469
5.716321	562.997411	7.344474
5.487744	557.673057	7.349478
5.560395	560.087518	7.354483
5.691871	560.838521	7.359488
5.670241	574.265642	7.364493
5.913506	588.871449	7.369498
5.550192	582.435385	7.374502
5.705538	586.603456	7.379507
6.137870	581.931954	7.384512
5.914759	589.712232	7.389517
5.705492	563.749140	7.394522
5.531646	566.158000	7.399526
5.493190	583.371465	7.404531
5.352329	581.770088	7.409536
5.639000	589.026167	7.414541
5.480755	591.737719	7.419546
5.816700	589.456990	7.424550
5.449409	591.919910	7.429555
5.893730	594.620113	7.434560
6.070551	589.233499	7.439565
5.748742	599.078348	7.444570
6.059861	587.487234	7.449574
5.828014	608.504575	7.454579
5.912348	596.410049	7.459584
6.047723	593.169852	7.464589
5.770403	600.088692	7.469594
5.828257	594.914845	7.474598
5.490647	601.886133	7.479603
5.941655	598.923817	7.484608
6.088681	597.503106	7.489613
5.679842	600.668547	7.494618
5.826973	594.938566	7.499622
5.923682	600.484920	7.504627
5.925352	588.503992	7.509632
5.753873	573.279414	7.514637
5.820842	563.553080	7.519642
5.864720	560.403284	7.524646
5.784789	567.994385	7.529651
5.897661	557.031412	7.534656
5.724871	550.817667	7.539661
5.932765	555.490663	7.544666
5.951338	561.632133	7.549670
5.654030	563.722686	7.554675
5.763637	557.706108	7.559680
5.682064	559.805401	7.564685
5.543558	557.827314	7.569690
5.846605	556.871846	7.574694
5.679054	566.340960	7.579699
5.786648	555.713943	7.584704
6.071354	558.606037	7.589709
5.899042	559.966389	7.594714
6.051258	560.576992	7.599718
5.785424	560.308283	7.604723
5.882007	564.766925	7.609728
6.030544	560.418278	7.614733
5.788310	557.589742	7.619738
5.731972	556.569092	7.624742
5.841562	557.281896	7.629747
6.132396	549.932186	7.634752
5.966398	562.156056	7.639757
5.519843	555.113215	7.644762
6.184831	557.690893	7.649766
5.793799	556.860850	7.654771
5.908582	557.366969	7.659776
5.698459	556.643217	7.664781
5.591751	549.900481	7.669786
5.732514	555.732739	7.674790
5.573958	563.385846	7.679795
5.870268	556.994278	7.684800
5.620553	558.798083	7.689805
5.586625	562.128141	7.694810
6.153295	552.468933	7.699814
5.819506	555.883165	7.704819
5.661008	559.298258	7.709824
5.718590	557.410718	7.714829
5.836407	561.619554	7.719834
6.132693	551.116087	7.724838
5.740690	557.822690	7.729843
5.731560	559.331747	7.734848
6.046646	554.819257	7.739853
5.721181	559.349032	7.744858
6.285237	551.415179	7.749862
5.342590	555.438947	7.754867
5.579833	558.099165	7.759872
5.643342	554.254047	7.764877
5.852476	556.730678	7.769882
6.039610	551.678822	7.774886
5.765668	553.799037	7.779891
5.680569	551.026280	7.784896
5.710339	549.779182	7.789901
5.711394	553.734309	7.794906
6.055295	550.253048	7.799910
6.056372	557.365163	7.804915
6.068913	544.236726	7.809920
5.745387	532.102688	7.814925
5.788874	527.628639	7.819930
5.718750	513.976817	7.824934
5.770035	518.439226	7.829939
5.572455	520.415713	7.834944
5.965753	530.833524	7.839949
5.701666	529.194222	7.844954
5.713957	514.848680	7.849958
5.753583	531.867167	7.854963
5.747790	535.024017	7.859968
5.563418	536.461754	7.864973
5.551504	544.425556	7.869978
5.601309	543.467581	7.874982
5.561196	546.273156	7.879987
5.798393	548.684933	7.884992
5.831029	548.841211	7.889997
5.707346	549.304084	7.895002
5.862684	551.887731	7.900006
5.624245	549.055803	7.905011
5.679871	552.685924	7.910016
5.563983	550.595740	7.915021
5.531602	560.519347	7.920026
5.876581	549.019329	7.925030
5.530685	556.415853	7.930035
5.894115	552.392617	7.935040
6.133018	553.179440	7.940045
5.869822	556.893139	7.945050
5.941924	555.988685	7.950054
5.639561	551.692092	7.955059
5.685858	549.346042	7.960064
6.048666	550.735262	7.965069
5.835678	559.778771	7.970074
5.996481	553.444261	7.975078
5.886429	546.021467	7.980083
6.086283	547.555384	7.985088
5.861868	555.077942	7.990093
5.775694	547.548565	7.995098
6.198833	545.313143	8.000102
5.757424	535.899444	8.005107
5.742260	526.121268	8.010112
5.722769	524.908448	8.015130
5.457051	520.402709	8.020147
6.130290	527.009588	8.025165
5.660625	535.715316	8.030182
5.734250	524.908845	8.035200
5.878254	522.728887	8.040218
5.894498	528.175983	8.045235
5.801425	518.720727	8.050253
5.588195	527.342101	8.055270
5.791339	520.569848	8.060288
5.896740	531.347910	8.065306
5.888201	540.913136	8.070323
5.792488	529.726968	8.075341
5.835353	526.998910	8.080358
5.751013	538.380510	8.085376
5.955607	540.873925	8.090394
5.964289	545.998888	8.095411
5.921314	531.004090	8.100429
5.837365	524.598422	8.105446
5.802551	523.666777	8.110464
5.985008	524.996454	8.115482
5.892201	533.921803	8.120499
5.968352	522.789745	8.125517
5.800225	530.575745	8.130534
5.940194	527.823870	8.135552
6.133942	526.373177	8.140570
5.880641	526.296081	8.145587
5.994011	519.586186	8.150605
5.834045	525.514300	8.155622
6.188523	524.432330	8.160640
6.088219	521.156465	8.165658
5.926918	526.241176	8.170675
6.430007	513.321978	8.175693
6.269324	507.918943	8.180710
5.802766	515.735838	8.185728
6.086416	511.163592	8.190746
5.844575	508.688351	8.195763
5.690007	514.715554	8.200781
5.551370	518.575936	8.205798
5.623031	521.569353	8.210816
5.639620	520.126454	8.215834
5.759768	535.942564	8.220851
6.105720	542.683958	8.225869
6.020123	548.647945	8.230886
5.915367	544.156190	8.235904
6.208110	550.324986	8.240922
5.996879	548.594192	8.245939
6.118206	544.793536	8.250957
6.173019	533.832521	8.255974
5.978106	524.890207	8.260992
6.278183	515.806577	8.266010
5.757301	525.377035	8.271027
5.910751	521.940895	8.276045
6.141502	533.519508	8.281062
6.128053	536.832361	8.286080
6.443508	521.961841	8.291098
5.931955	528.859138	8.296115
6.119458	513.628627	8.301133
6.114076	525.733248	8.306150
5.927330	525.430346	8.311168
6.254152	517.853946	8.316186
6.151068	522.292225	8.321203
6.125649	518.907073	8.326221
6.074327	515.921861	8.331238
5.970856	518.081470	8.336256
6.117734	516.959996	8.341274
5.927419	520.792160	8.346291
6.162260	521.079560	8.351309
5.869131	523.078781	8.356326
6.015312	542.754991	8.361344
6.112333	535.662801	8.366362
6.129223	547.137021	8.371379
6.640726	557.770446	8.376397
5.954140	542.985161	8.381414
5.884493	549.616910	8.386432
6.371175	542.770751	8.391450
6.399107	562.031835	8.396467
6.209735	535.778685	8.401485
6.091922	529.419388	8.406502
5.941090	534.562395	8.411520
6.595592	531.672052	8.416538
5.968112	534.953510	8.421555
6.179663	527.225020	8.426573
6.381514	545.975527	8.431590
6.129452	539.243888	8.436608
6.290984	537.571994	8.441626
6.179090	539.120068	8.446643
5.958024	533.505032	8.451661
5.983371	543.627373	8.456678
6.178487	553.158757	8.461696
6.360795	544.206683	8.466714
6.258603	560.667200	8.471731
6.427596	550.237149	8.476749
6.442363	552.191891	8.481766
6.358864	551.791322	8.486784
6.449376	548.831344	8.491802
6.556431	544.367174	8.496819
6.179596	523.861631	8.501837
6.457913	515.588632	8.506854
6.001367	523.839262	8.511872
6.373418	513.961653	8.516890
6.032390	525.490819	8.521907
6.183560	530.922183	8.526925
6.430088	538.338113	8.531942
6.310980	541.900595	8.536960
6.297829	552.403914	8.541978
6.414010	551.942994	8.546995
6.568449	554.014077	8.552013
6.608594	533.119165	8.557030
6.391338	527.460982	8.562048
6.670482	512.842743	8.567066
6.652490	522.402049	8.572083
6.390665	515.815928	8.577101
5.884020	511.775197	8.582119
6.003883	523.565523	8.587136
6.157095	520.170954	8.592154
6.527549	539.142030	8.597171
6.744394	539.314519	8.602189
6.600912	527.907572	8.607207
6.201969	527.206512	8.612224
6.429774	515.548510	8.617242
6.112601	524.366473	8.622259
6.221562	537.392567	8.627277
6.316886	542.741689	8.632295
6.395336	545.957585	8.637312
6.562675	534.531843	8.642330
6.312699	551.068286	8.647347
6.483002	546.931762	8.652365
6.942978	542.981522	8.657383
6.476116	539.793938	8.662400
6.525227	534.608364	8.667418
6.408652	536.243232	8.672435
6.568971	543.095788	8.677453
6.569749	530.265773	8.682471
5.962682	538.916394	8.687488
6.302057	548.301369	8.692506
6.206186	547.860144	8.697523
5.883959	549.052071	8.702541
6.210937	544.104536	8.707559
6.588094	551.009828	8.712576
6.225442	554.228574	8.717594
6.240719	548.722859	8.722611
6.254152	554.608582	8.727629
6.217172	565.237907	8.732647
6.380234	575.574958	8.737664
6.788919	573.556101	8.742682
6.820980	585.607307	8.747699
6.928973	574.946650	8.752717
6.399602	557.574809	8.757735
6.276028	559.308276	8.762752
6.448184	561.916329	8.767770
6.573185	569.107612	8.772787
6.815532	580.312318	8.777805
6.869757	582.660275	8.782823
6.566542	587.840634	8.787840
6.446047	579.177036	8.792858
6.602787	575.213217	8.797875
6.857664	578.895817	8.802893
6.955023	574.476750	8.807911
6.292590	566.397089	8.812928
6.696772	565.151750	8.817946
6.641909	567.213532	8.822963
6.559243	573.511460	8.827981
6.911713	563.691991	8.832999
6.638216	565.557060	8.838016
6.458502	553.961842	8.843034
6.457099	560.356879	8.848051
6.292925	576.480697	8.853069
6.772143	572.030640	8.858087
6.838984	582.329362	8.863104
6.792849	575.942385	8.868122
7.265662	574.513213	8.873139
6.771469	559.880170	8.878157
7.032258	559.380649	8.883175
6.795280	551.127142	8.888192
6.555523	551.860322	8.893210
6.518337	548.154116	8.898227
6.298118	563.861289	8.903245
6.704185	578.225711	8.908263
6.816989	581.927201	8.913280
6.529365	579.406806	8.918298
6.918590	574.714050	8.923315
6.790415	590.104009	8.928333
6.601164	576.720156	8.933351
6.868600	576.974584	8.938368
6.903408	580.087513	8.943386
7.044142	582.227014	8.948403
6.872000	576.988837	8.953421
6.941928	568.600656	8.958439
6.615516	574.857411	8.963456
6.564041	580.064425	8.968474
6.691879	581.683869	8.973491
6.783435	582.554684	8.978509
7.008643	574.195608	8.983527
6.774791	573.305112	8.988544
6.573029	578.558756	8.993562
6.646360	581.888295	8.998579
6.930890	579.170057	9.003597
6.852200	587.721665	9.008615
6.571874	588.150986	9.013632
6.658438	575.570432	9.018650
7.043397	583.709769	9.023667
6.984041	588.759447	9.028685
6.905681	582.163078	9.033703
6.839301	583.525852	9.038720
6.819355	582.673812	9.043738
6.865931	576.233240	9.048755
6.686149	588.621994	9.053773
7.213527	586.985737	9.058791
6.992957	581.890635	9.063808
6.661362	585.492774	9.068826
6.788382	582.620021	9.073843
6.794659	586.293552	9.078861
7.087068	580.871281	9.083879
7.055809	589.835247	9.088896
6.968457	592.725787	9.093914
7.051793	583.762583	9.098931
6.965858	588.007496	9.103949
7.105620	586.206942	9.108967
6.904122	591.698322	9.113984
6.616720	582.152895	9.119002
7.210220	580.947737	9.124019
6.897557	592.481489	9.129037
6.900872	587.907788	9.134055
6.796078	606.399322	9.139072
7.024591	611.499185	9.144090
7.257715	609.614613	9.149107
7.224433	609.862728	9.154125
7.192132	609.899281	9.159143
7.033244	592.858310	9.164160
6.900966	580.077138	9.169178
7.373484	591.512667	9.174195
6.930473	603.448769	9.179213
7.032993	592.484507	9.184231
7.151759	597.022931	9.189248
7.101242	603.962718	9.194266
7.295990	595.905125	9.199283
6.941395	595.828330	9.204301
7.357378	590.077078	9.209319
6.858539	600.951878	9.214336
7.009530	605.699891	9.219354
7.313903	598.388579	9.224371
7.267448	607.133052	9.229389
7.107176	605.243793	9.234407
7.076198	601.684168	9.239424
7.044076	610.363864	9.244442
7.313732	608.530696	9.249459
7.503772	617.158906	9.254477
7.319878	602.025664	9.259495
7.297135	600.633385	9.264512
6.926784	583.673828	9.269530
6.999066	579.359903	9.274547
6.679713	590.842015	9.279565
7.157708	597.480982	9.284583
7.513118	611.866846	9.289600
7.005768	615.893447	9.294618
7.396412	606.824039	9.299635
7.208014	611.570594	9.304653
7.118217	603.518168	9.309671
7.078311	603.294786	9.314688
7.172503	605.584729	9.319706
7.076191	598.169359	9.324723
6.893647	606.145966	9.329741
6.791177	609.653735	9.334759
7.022566	606.576441	9.339776
6.699939	615.376662	9.344794
7.344852	627.974805	9.349811
7.185122	649.782139	9.354829
7.320333	645.006592	9.359847
7.324233	650.053060	9.364864
7.496812	644.062345	9.369882
7.568195	635.379422	9.374899
7.157757	644.450336	9.379917
7.539578	636.331907	9.384935
7.656685	649.116012	9.389952
7.567564	635.581225	9.394970
7.597035	616.211866	9.399987
7.162152	616.789307	9.405005
7.286920	613.508492	9.410023
7.219526	611.630368	9.415040
7.150471	621.504299	9.420058
7.213964	626.049163	9.425075
7.330766	645.662675	9.430093
7.067625	640.750402	9.435111
7.726638	649.181992	9.440128
7.115371	645.722742	9.445146
7.508243	651.108857	9.450163
7.142395	646.748453	9.455181
7.544323	647.329319	9.460199
7.697517	635.047853	9.465216
7.208522	648.517688	9.470234
7.424077	638.864814	9.475251
7.696687	655.480835	9.480269
7.368140	641.409506	9.485287
7.238221	641.928387	9.490304
7.528298	649.273752	9.495322
7.730726	654.416151	9.500339
7.293589	653.312607	9.505357
7.557160	646.052145	9.510375
7.671524	638.793653	9.515392
7.476433	639.352104	9.520410
7.539666	650.341572	9.525427
7.663613	647.986205	9.530445
7.623561	642.253648	9.535463
7.633358	636.772630	9.540480
7.458125	644.497275	9.545498
7.732266	636.823283	9.550515
7.891294	644.678773	9.555533
7.732864	642.226847	9.560551
7.823352	637.075697	9.565568
7.645926	640.479798	9.570586
7.549604	635.626407	9.575603
7.742748	647.193641	9.580621
7.173210	641.643964	9.585639
7.523478	651.082698	9.590656
7.462382	646.667704	9.595674
7.802530	635.462162	9.600691
7.632742	647.990235	9.605709
7.589284	641.050469	9.610727
7.477352	641.699224	9.615744
7.866604	645.248688	9.620762
7.776006	637.453049	9.625779
7.699275	643.036495	9.630797
7.616820	641.053990	9.635815
8.003097	647.199209	9.640832
7.695533	646.867570	9.645850
7.522921	643.933198	9.650867
7.748526	645.798583	9.655885
7.529845	649.939799	9.660903
7.609040	636.107569	9.665920
7.355710	654.857688	9.670938
7.463970	648.568238	9.675955
7.803394	644.509673	9.680973
7.667010	642.724305	9.685991
7.437883	650.912007	9.691008
7.415165	657.442703	9.696026
7.861657	653.229343	9.701043
7.539731	647.911321	9.706061
7.838787	663.304156	9.711079
7.662011	666.997109	9.716096
7.948475	679.180892	9.721114
7.855589	677.400691	9.726131
7.736328	672.914852	9.731149
8.017794	673.248832	9.736167
7.921342	662.541787	9.741184
7.663551	656.845809	9.746202
7.763185	660.443019	9.751219
8.212160	666.161323	9.756237
8.030613	663.071556	9.761255
8.194694	653.082768	9.766272
7.841233	652.239901	9.771290
7.751840	646.440944	9.776307
7.492258	648.234621	9.781325
7.544354	660.495923	9.786343
8.072592	666.156568	9.791360
8.012253	676.515070	9.796378
8.012994	675.840282	9.801395
8.033109	668.099842	9.806413
7.678959	658.751275	9.811431
7.802479	664.685076	9.816448
8.015802	671.150760	9.821466
7.994684	679.078726	9.826483
8.012172	682.641960	9.831501
7.665608	686.951673	9.836519
7.950115	677.265467	9.841536
7.909412	680.478362	9.846554
7.849939	680.928060	9.851571
7.902119	673.320073	9.856589
7.899750	676.402983	9.861607
8.420783	672.604558	9.866624
8.112723	686.076830	9.871642
8.051556	680.495986	9.876659
7.794091	675.896513	9.881677
7.841295	681.879420	9.886695
8.198276	676.373160	9.891712
7.837499	683.432655	9.896730
8.010835	673.748394	9.901747
8.253786	674.806436	9.906765
7.908205	672.851520	9.911783
8.258893	674.651831	9.916800
8.057399	680.451877	9.921818
8.160394	683.097231	9.926835
8.374701	673.107562	9.931853
7.794073	683.720445	9.936871
8.397818	665.087401	9.941888
8.115520	672.323202	9.946906
8.063561	674.124693	9.951923
8.371494	672.248348	9.956941
8.042062	679.255588	9.961959
8.307219	671.823604	9.966976
8.172441	677.794042	9.971994
8.128876	673.881205	9.977011
8.259825	679.703353	9.982029
7.705581	681.226546	9.987047
8.260027	687.936107	9.992064
7.990916	677.738420	9.997082
8.014660	681.056736	10.002099
8.108199	675.739724	10.007117
8.021175	684.182150	10.012135
8.151770	677.485464	10.017152
8.183205	678.702471	10.022170
7.770623	678.602639	10.027187
8.256611	681.413452	10.032205
7.992137	706.538409	10.037223
8.391435	715.882623	10.042240
8.564528	709.434352	10.047258
8.189586	703.246450	10.052275
8.503333	705.616641	10.057293
8.182951	687.450135	10.062311
8.317223	687.919989	10.067328
8.465378	683.592834	10.072346
8.445095	678.791944	10.077363
8.317430	677.487958	10.082381
8.138814	679.509698	10.087399
8.076949	686.130567	10.092416
8.343211	689.441842	10.097434
8.399090	711.256140	10.102451
8.379085	704.441768	10.107469
8.359818	709.247046	10.112487
8.685141	709.680030	10.117504
8.619685	704.227635	10.122522
8.166173	692.270568	10.127539
8.379082	703.503680	10.132557
8.402316	703.455417	10.137575
8.891479	703.050996	10.142592
8.674519	697.895811	10.147610
8.195186	688.125152	10.152627
8.469824	678.107934	10.157645
8.191223	679.741206	10.162663
8.517387	678.899937	10.167680
8.205582	682.444680	10.172698
8.205691	708.201005	10.177715
8.840769	709.916653	10.182733
8.594433	718.384986	10.187751
8.628225	704.887775	10.192768
8.656196	685.243798	10.197786
8.171442	685.916334	10.202803
8.274144	698.238147	10.207821
8.472502	701.906550	10.212839
8.601066	713.571371	10.217856
8.777665	711.045051	10.222874
8.470536	719.603207	10.227891
8.513727	708.422364	10.232909
8.756766	714.442217	10.237927
8.840995	706.357073	10.242944
8.866348	689.724119	10.247962
8.345991	682.886235	10.252979
8.641575	689.849828	10.257997
8.519828	691.678668	10.263015
8.626671	698.362833	10.268032
8.520644	712.352687	10.273050
8.557521	716.151862	10.278067
8.819343	711.544606	10.283085
8.652311	711.298458	10.288103
8.626956	710.361490	10.293120
8.830511	703.928039	10.298138
8.423668	714.870299	10.303155
8.635190	704.961971	10.308173
8.647542	720.128324	10.313191
8.759622	713.466391	10.318208
8.914991	708.398127	10.323226
8.773073	716.589281	10.328243
8.807292	710.086145	10.333261
8.573262	711.052614	10.338279
8.824405	705.431860	10.343296
8.786724	716.166908	10.348314
8.503984	715.473098	10.353331
8.571688	706.634656	10.358349
8.594417	716.903794	10.363367
8.332208	719.173273	10.368384
8.436530	715.349616	10.373402
8.348688	717.707034	10.378419
8.699576	713.156426	10.383437
8.742173	715.930123	10.388455
8.483675	708.436743	10.393472
8.750176	719.028329	10.398490
8.594484	733.123890	10.403507
8.572117	744.218393	10.408525
8.489732	743.082453	10.413543
8.413316	744.367781	10.418560
8.838320	742.148372	10.423578
8.519453	745.247289	10.428595
8.896824	738.461730	10.433613
8.617447	741.270639	10.438631
8.638092	746.737552	10.443648
8.898764	748.966779	10.448666
8.894970	742.427037	10.453683
8.973243	749.414770	10.458701
8.949815	754.156191	10.463719
8.897750	751.977689	10.468736
8.765387	740.914381	10.473754
8.589879	753.830469	10.478771
9.236220	761.728046	10.483789
9.101464	769.574165	10.488807
9.003789	756.262332	10.493824
9.155447	747.584112	10.498842
8.771288	752.175465	10.503859
9.217794	756.861810	10.508877
9.016675	746.809261	10.513895
8.703470	748.971087	10.518912
9.061432	762.041804	10.523930
8.816107	767.066745	10.528947
9.159047	768.828594	10.533965
9.143638	773.838748	10.538983
8.837718	777.379187	10.544000
9.475293	770.222635	10.549018
9.450944	774.448112	10.554035
9.210703	752.665322	10.559053
9.135750	753.005202	10.564071
8.866658	750.419301	10.569088
9.064153	743.297326	10.574106
8.668473	752.289674	10.579123
9.139449	761.930444	10.584141
9.227905	781.191189	10.589159
9.113970	781.371616	10.594176
9.318667	783.397765	10.599194
9.189464	777.416609	10.604211
8.990083	779.058573	10.609229
9.151123	777.499522	10.614247
9.099642	779.848544	10.619264
9.266918	780.303074	10.624282
9.375459	782.824698	10.629299
9.344148	781.678101	10.634317
9.277211	778.470646	10.639335
9.246867	779.680804	10.644352
9.469191	786.839479	10.649370
8.915166	780.702175	10.654387
8.931875	780.988044	10.659405
9.303437	776.956581	10.664423
9.140289	787.700722	10.669440
9.215411	779.403880	10.674458
9.220437	778.923243	10.679475
9.059544	781.792382	10.684493
9.358351	771.457330	10.689511
9.126949	783.089520	10.694528
9.266490	775.575813	10.699546
9.069634	776.895530	10.704563
9.230380	772.597358	10.709581
9.319989	772.917564	10.714599
9.117839	781.621089	10.719616
9.275285	773.407213	10.724634
9.180766	781.104338	10.729651
9.271780	775.793026	10.734669
9.360531	778.049848	10.739687
9.391818	799.871114	10.744704
9.770312	793.297731	10.749722
9.415585	788.954924	10.754739
9.404068	791.251049	10.759757
9.505165	771.937303	10.764775
9.212600	785.173047	10.769792
9.174769	782.443594	10.774810
9.354617	805.561340	10.779827
9.554380	810.606603	10.784845
9.483483	810.850344	10.789863
9.429162	813.363808	10.794880
9.500707	809.211938	10.799898
9.629444	818.070315	10.804915
8.996242	817.904401	10.809933
9.643570	804.886388	10.814951
9.259962	815.328631	10.819968
9.596854	809.699296	10.824986
9.347269	810.670521	10.830003
9.797980	815.673683	10.835021
9.656655	802.904262	10.840039
9.676534	813.990219	10.845056
9.702174	802.336275	10.850074
9.752447	806.534595	10.855091
9.594462	804.997071	10.860109
9.696108	810.005890	10.865127
9.365485	804.805589	10.870144
9.963970	799.244581	10.875162
9.490786	806.261205	10.880179
9.528575	802.946975	10.885197
10.088492	803.604928	10.890215
9.801321	803.891111	10.895232
10.022496	809.608554	10.900250
9.717592	789.955798	10.905267
9.530961	792.976451	10.910285
9.617675	787.812493	10.915303
9.808571	801.515298	10.920320
9.535915	808.466706	10.925338
9.369511	807.268353	10.930355
9.489420	812.307205	10.935373
9.852882	802.718814	10.940391
9.752293	809.104850	10.945408
9.871798	802.018643	10.950426
10.023270	815.594165	10.955443
9.535623	809.499553	10.960461
10.412501	804.347753	10.965479
10.201800	809.448246	10.970496
9.609482	803.694043	10.975514
9.897906	792.852864	10.980531
9.894522	800.656496	10.985549
9.767123	783.664212	10.990567
9.690997	804.248507	10.995584
9.689629	809.635445	11.000602
9.965935	812.061084	11.005619
9.546728	817.852685	11.010637
9.855029	805.551801	11.015655
9.706452	813.959452	11.020672
9.833390	804.527489	11.025690
9.791689	809.890030	11.030707
9.794355	813.303997	11.035725
10.161166	812.334321	11.040743
9.919400	809.735010	11.045760
9.914684	811.279667	11.050778
9.822611	812.403834	11.055795
9.630082	816.399616	11.060813
10.239217	807.760279	11.065831
9.801207	811.153992	11.070848
9.690295	809.937755	11.075866
9.996181	813.713895	11.080883
10.089371	811.474828	11.085901
9.773826	801.895953	11.090919
9.509135	815.246570	11.095936
9.664024	822.370213	11.100954
9.957706	841.453822	11.105971
10.206304	844.468284	11.110989
10.421255	848.790612	11.116007
10.453762	846.156536	11.121024
10.046668	827.860782	11.126042
9.868842	818.494621	11.131059
10.186543	822.519962	11.136077
10.123417	813.538255	11.141095
10.289527	824.039915	11.146112
10.070944	818.156073	11.151130
10.025971	806.824077	11.156147
10.135630	821.980458	11.161165
10.116300	826.881052	11.166183
10.148417	845.215282	11.171200
10.084610	850.318734	11.176218
10.438294	843.129614	11.181235
10.050282	849.415614	11.186253
10.607135	833.384869	11.191271
10.220005	821.777273	11.196288
10.057976	815.221284	11.201306
10.490926	825.168393	11.206323
10.090609	823.352269	11.211341
10.327416	810.161949	11.216359
10.175787	814.595389	11.221376
10.120896	816.698740	11.226394
10.428697	828.401176	11.231411
10.291946	842.453140	11.236429
10.534011	840.400727	11.241447
10.162087	831.544936	11.246464
10.029271	832.310350	11.251482
10.210890	838.099925	11.256499
10.310067	845.894407	11.261517
10.410796	849.109419	11.266535
10.437960	854.887666	11.271552
10.411148	846.288461	11.276570
10.658155	838.021874	11.281587
10.113142	847.199322	11.286605
10.436286	844.889158	11.291623
10.590585	851.315716	11.296640
10.519078	848.344424	11.301658
10.380665	844.217206	11.306675
10.109430	850.288141	11.311693
10.247266	853.001744	11.316711
10.467337	844.471932	11.321728
10.182628	848.350571	11.326746
10.420154	842.348395	11.331763
10.164677	857.022426	11.336781
10.355649	848.959030	11.341799
10.539271	847.575144	11.346816
10.194926	849.152239	11.351834
10.224895	843.993757	11.356851
10.287744	858.750699	11.361869
10.210092	853.628407	11.366887
10.367252	871.640330	11.371904
10.659865	881.520453	11.376922
10.827307	870.262349	11.381939
10.898023	870.553416	11.386957
10.746341	870.290541	11.391975
10.595608	853.624871	11.396992
10.354161	851.498106	11.402010
10.575400	858.074160	11.407027
10.526924	872.427009	11.412045
10.677937	870.778677	11.417063
11.021027	872.320056	11.422080
10.737599	868.524197	11.427098
10.604893	850.018453	11.432115
10.284026	848.182232	11.437133
10.514638	867.622790	11.442151
10.781963	867.736700	11.447168
10.571916	876.621499	11.452186
10.493604	870.268881	11.457203
10.547686	880.477999	11.462221
10.442199	876.135274	11.467239
10.567101	877.748939	11.472256
10.438916	869.268729	11.477274
10.580190	877.599501	11.482291
10.624823	883.976391	11.487309
10.662042	878.340739	11.492327
10.803171	875.748246	11.497344
10.569582	874.451022	11.502362
10.758908	883.847755	11.507379
10.911958	907.770646	11.512397
10.997174	899.782672	11.517415
11.079624	893.119091	11.522432
10.663039	886.973467	11.527450
10.860831	883.861942	11.532467
10.722228	904.220942	11.537485
11.089542	905.039053	11.542503
11.144058	907.586605	11.547520
11.098094	890.112392	11.552538
10.899959	871.077769	11.557555
10.909373	876.367472	11.562573
10.899201	870.894414	11.567591
10.908533	862.296475	11.572608
10.487266	879.803997	11.577626
11.039350	883.099105	11.582643
11.514085	902.338709	11.587661
11.343876	891.617782	11.592679
11.295583	885.952249	11.597696
11.023691	878.368499	11.602714
11.154271	874.883920	11.607731
11.021060	881.659635	11.612749
10.902573	873.450430	11.617767
11.482360	873.622439	11.622784
11.130673	876.768763	11.627802
11.053761	871.159956	11.632819
11.180692	873.840339	11.637837
11.185069	865.745747	11.642855
11.486241	871.893589	11.647872
11.006834	872.092440	11.652890
11.089576	864.351336	11.657907
11.206726	874.845420	11.662925
11.153484	873.811706	11.667943
11.263289	863.594418	11.672960
11.197106	879.303669	11.677978
11.167712	861.559429	11.682995
11.479986	873.811119	11.688013
10.958838	868.796193	11.693031
10.866603	865.071700	11.698048
10.915771	866.805030	11.703066
10.869431	865.822725	11.708083
10.920624	868.945194	11.713101
10.786180	886.824708	11.718119
11.116730	887.941823	11.723136
11.236814	913.096696	11.728154
11.482928	900.772413	11.733171
11.036471	912.183373	11.738189
10.954114	915.779593	11.743207
11.436316	913.833510	11.748224
11.148264	917.042685	11.753242
11.130069	911.944938	11.758259
11.129513	909.096479	11.763277
10.944539	907.374270	11.768295
11.280454	906.413856	11.773312
11.165027	904.711582	11.778330
11.358374	911.519642	11.783347
11.618981	915.128934	11.788365
11.380864	917.187758	11.793383
11.346751	916.465999	11.798400
11.012252	916.496090	11.803418
11.540948	915.111140	11.808435
11.414947	928.157718	11.813453
11.406345	939.090831	11.818471
11.849853	943.554321	11.823488
11.647526	943.604961	11.828506
11.412328	931.051615	11.833523
11.491785	926.376975	11.838541
11.435168	932.368770	11.843559
11.720240	932.023855	11.848576
11.519556	939.775315	11.853594
11.607829	939.893003	11.858611
11.698210	939.045440	11.863629
11.618984	930.574971	11.868647
11.768302	910.798735	11.873664
11.277151	918.283128	11.878682
11.370073	919.953488	11.883699
11.718863	930.372104	11.888717
11.541074	932.092183	11.893735
12.021066	938.591212	11.898752
11.874732	940.414324	11.903770
11.641563	914.277647	11.908787
11.351180	904.460880	11.913805
11.119870	926.456276	11.918823
11.339679	934.564590	11.923840
11.622366	934.650359	11.928858
11.533845	937.715359	11.933875
11.611501	933.859469	11.938893
11.664424	944.551272	11.943911
11.940066	938.434266	11.948928
11.776440	936.208143	11.953946
11.851838	936.727159	11.958963
11.461626	930.103541	11.963981
11.674012	943.728103	11.968999
11.973547	940.256961	11.974016
11.781591	936.694685	11.979034
11.843414	940.906278	11.984051
11.782535	943.484038	11.989069
11.752677	946.504252	11.994087
11.902816	939.494382	11.999104
11.744890	936.590976	12.004122
11.663513	934.881859	12.009139
11.905439	942.595581	12.014157
11.764472	935.331359	12.019175
11.911020	958.281257	12.024192
11.949114	972.017878	12.029210
11.798375	978.603252	12.034227
12.076352	974.999474	12.039245
11.883139	976.844161	12.044263
12.243982	963.589397	12.049280
12.146070	965.599728	12.054298
11.747502	967.813565	12.059315
12.395486	954.772485	12.064333
11.699009	956.212262	12.069351
11.981691	960.762326	12.074368
12.137188	974.292046	12.079386
12.304764	967.928832	12.084403
12.121883	946.795251	12.089421
11.642913	955.563385	12.094439
12.037709	953.593244	12.099456
11.919685	961.557735	12.104474
11.979615	976.280040	12.109491
12.492603	968.131961	12.114509
12.214366	973.343727	12.119527
12.051950	968.009317	12.124544
11.998121	972.003541	12.129562
12.146168	971.030651	12.134579
12.101757	961.074940	12.139597
11.857053	968.018426	12.144615
12.357268	961.072402	12.149632
12.270453	964.098937	12.154650
12.164564	971.190996	12.159667
12.680277	960.505613	12.164685
12.299480	966.997338	12.169703
12.448874	966.211615	12.174720
12.134099	964.375155	12.179738
12.014976	965.726059	12.184755
12.268613	959.835917	12.189773
12.231086	970.335697	12.194791
12.282362	956.775719	12.199808
12.200421	964.199601	12.204826
12.022785	967.597509	12.209843
11.761364	960.385972	12.214861
11.833887	963.351774	12.219879
12.053595	970.659385	12.224896
12.395458	986.163924	12.229914
12.185595	992.537491	12.234931
12.333394	1000.537343	12.239949
12.169745	1003.439262	12.244967
12.828408	996.826709	12.249984
12.618170	993.897736	12.255002
12.572131	995.005014	12.260019
12.661468	989.053198	12.265037
12.547390	992.949179	12.270055
12.849111	985.531834	12.275072
12.364091	973.214452	12.280090
12.667776	971.417710	12.285107
12.500206	955.424178	12.290125
12.202596	969.291390	12.295143
12.720762	978.453222	12.300160
12.829516	985.112786	12.305178
12.612570	967.829492	12.310195
12.865467	961.151725	12.315213
12.556718	961.963315	12.320231
12.649953	961.249914	12.325248
12.855113	966.720683	12.330266
12.966410	966.025539	12.335283
12.472016	970.457925	12.340301
12.438079	967.876798	12.345319
12.813400	955.931759	12.350336
12.855826	955.463403	12.355354
12.823816	969.067587	12.360371
12.850001	954.677973	12.365389
12.716815	964.279924	12.370407
12.655047	958.650854	12.375424
12.845967	956.083928	12.380442
12.775098	956.922118	12.385459
12.920349	957.638173	12.390477
12.777145	960.447322	12.395495
12.927655	960.201144	12.400512
12.899472	959.090232	12.405530
12.645745	958.688026	12.410547
12.723861	964.644055	12.415565
12.560992	959.994722	12.420583
12.743554	962.767835	12.425600
12.852196	959.407153	12.430618
12.386061	957.323820	12.435635
13.013024	964.355091	12.440653
13.123500	974.455888	12.445671
12.707824	968.198669	12.450688
12.885191	965.150952	12.455706
13.161647	983.914589	12.460723
13.144453	976.662058	12.465741
12.693096	969.699001	12.470759
12.729668	962.496985	12.475776
13.460231	974.954020	12.480794
13.257334	983.189306	12.485811
13.210148	966.610825	12.490829
13.369317	969.803552	12.495847
13.019343	951.880615	12.500864
12.940862	967.116830	12.505882
12.626137	958.514631	12.510899
12.864011	955.175381	12.515917
12.927222	960.470147	12.520935
12.840209	962.204667	12.525952
13.119301	967.102947	12.530970
13.117874	986.907988	12.535987
13.511063	987.695034	12.541005
13.095938	967.227941	12.546023
12.829823	964.897595	12.551040
13.118490	972.164614	12.556058
13.311956	987.711929	12.561075
13.077817	981.192656	12.566093
13.241333	993.081786	12.571111
13.240189	992.398243	12.576128
13.639925	990.907563	12.581146
13.334544	995.213271	12.586163
13.031308	981.621254	12.591181
13.396167	982.346082	12.596199
13.231705	988.707771	12.601216
13.604826	994.426602	12.606234
13.203361	978.418380	12.611251
13.243738	979.780176	12.616269
13.579867	983.596997	12.621287
13.233907	975.830245	12.626304
13.466792	968.270028	12.631322
12.806847	971.029639	12.636339
13.262619	973.474686	12.641357
13.341341	985.198387	12.646375
13.129608	997.269567	12.651392
13.399953	986.127734	12.656410
13.202398	986.907065	12.661427
13.246872	984.290463	12.666445
13.477065	991.635710	12.671463
13.636522	986.748948	12.676480
13.560436	990.396109	12.681498
13.291632	995.322079	12.686515
13.156664	987.563952	12.691533
13.280315	989.165829	12.696551
13.208775	989.745881	12.701568
13.365214	998.347409	12.706586
13.337650	1009.035706	12.711603
13.808902	1019.551739	12.716621
13.628570	1023.846906	12.721639
13.285420	1024.241407	12.726656
13.435631	1015.850860	12.731674
13.475502	1016.388775	12.736691
13.566987	1020.555698	12.741709
13.831360	1014.323613	12.746727
13.705524	1022.977977	12.751744
13.511063	1012.062976	12.756762
13.198519	1017.668625	12.761779
13.431942	1017.254344	12.766797
13.545342	1024.517055	12.771815
13.639507	1027.809569	12.776832
13.837534	1019.887817	12.781850
13.869478	1015.242307	12.786867
13.546491	1014.379197	12.791885
13.645940	1017.626344	12.796903
13.137918	1021.688984	12.801920
13.973303	1025.938949	12.806938
13.568353	1050.234905	12.811955
13.871419	1050.972370	12.816973
14.074057	1047.528726	12.821991
14.065114	1057.386841	12.827008
14.057147	1046.980948	12.832026
14.122152	1035.864547	12.837043
14.056939	1023.037218	12.842061
14.042594	1018.790716	12.847079
13.818570	1018.278459	12.852096
13.984815	1014.888900	12.857114
13.921138	1019.794170	12.862131
13.874145	1009.292825	12.867149
14.105210	1013.406234	12.872167
13.538240	1015.396113	12.877184
14.152807	1024.975783	12.882202
14.280576	1032.121156	12.887219
14.269094	1024.810175	12.892237
14.393336	1021.696872	12.897255
13.815154	1020.293926	12.902272
14.019773	1016.715322	12.907290
13.691041	1016.596825	12.912307
13.694970	1021.281422	12.917325
13.922806	1029.651035	12.922343
13.835154	1043.179104	12.927360
13.970435	1046.585254	12.932378
14.664009	1045.996466	12.937395
14.430635	1045.639297	12.942413
14.584371	1045.600838	12.947431
14.567596	1036.439260	12.952448
14.227389	1017.406418	12.957466
14.114661	1009.065483	12.962483
13.990488	1012.652928	12.967501
14.120689	1018.342069	12.972519
14.237273	1030.015812	12.977536
14.739325	1034.307010	12.982554
14.310462	1021.277146	12.987571
14.116394	1015.815311	12.992589
14.433384	1019.019216	12.997607
14.204950	1030.601100	13.002624
14.090216	1040.584656	13.007642
14.288749	1040.177354	13.012659
14.142845	1042.936575	13.017677
14.097790	1041.280067	13.022695
14.236802	1046.356370	13.027712
14.206396	1040.652769	13.032730
14.432576	1055.034543	13.037747
14.511160	1049.775004	13.042765
14.380465	1052.735625	13.047783
14.334011	1054.788987	13.052800
14.510363	1054.873533	13.057818
14.381706	1044.238896	13.062835
14.481084	1046.956957	13.067853
14.567391	1044.640855	13.072871
14.590033	1055.362569	13.077888
14.687709	1050.787614	13.082906
14.809202	1055.023965	13.087923
14.551263	1047.625597	13.092941
14.730261	1047.842374	13.097959
14.653676	1049.059845	13.102976
14.561165	1045.431412	13.107994
14.497453	1052.935766	13.113011
14.701368	1042.146647	13.118029
14.589682	1040.186664	13.123047
14.592010	1040.609960	13.128064
14.430919	1035.174525	13.133082
14.284642	1044.232276	13.138099
14.257779	1053.539854	13.143117
14.882244	1057.996923	13.148135
14.836211	1075.652523	13.153152
14.802609	1066.831895	13.158170
15.013494	1067.452799	13.163187
14.551934	1052.058786	13.168205
15.047056	1062.394513	13.173223
15.228107	1058.544634	13.178240
14.888088	1051.006766	13.183258
14.865640	1041.842978	13.188275
14.700953	1041.537382	13.193293
14.718544	1035.711639	13.198311
14.542156	1042.626876	13.203328
14.756726	1054.221757	13.208346
15.095272	1069.665912	13.213363
15.058089	1064.359471	13.218381
15.057015	1070.573965	13.223399
15.050174	1063.556667	13.228416
15.062325	1041.772071	13.233434
14.937792	1033.803929	13.238451
14.583533	1038.925602	13.243469
14.973191	1057.486665	13.248487
15.130335	1071.073279	13.253504
15.049096	1067.241404	13.258522
15.007031	1069.650318	13.263539
14.983106	1067.502133	13.268557
15.193011	1061.328686	13.273575
14.799143	1069.148537	13.278592
15.096475	1076.027571	13.283610
15.180028	1075.339002	13.288627
15.104922	1073.678824	13.293645
15.166134	1067.356082	13.298663
15.133967	1077.694028	13.303680
14.945390	1068.688538	13.308698
14.967064	1076.417675	13.313715
15.108653	1078.864961	13.318733
15.379529	1064.693224	13.323751
14.902748	1078.091914	13.328768
14.687703	1067.476737	13.333786
14.952407	1071.890854	13.338803
15.209956	1079.822508	13.343821
15.535482	1088.882179	13.348839
15.545775	1092.522094	13.353856
15.499098	1080.903384	13.358874
15.438463	1075.785079	13.363891
15.195982	1075.851841	13.368909
15.572886	1068.203862	13.373927
15.489817	1074.468598	13.378944
15.133054	1079.561568	13.383962
15.570761	1071.812541	13.388979
15.313053	1073.296719	13.393997
15.081463	1077.877178	13.399015
14.980428	1080.158501	13.404032
15.372215	1100.590029	13.409050
15.449255	1090.663653	13.414067
15.423190	1085.706126	13.419085
15.761871	1089.802456	13.424103
15.843853	1089.584201	13.429120
15.354209	1087.444524	13.434138
15.244472	1085.396814	13.439155
15.530855	1101.543334	13.444173
15.191847	1089.287807	13.449191
15.531538	1088.668864	13.454208
15.431486	1096.464304	13.459226
15.795982	1089.786437	13.464243
15.839936	1092.416872	13.469261
15.573156	1079.306479	13.474279
15.403185	1088.280009	13.479296
15.531475	1102.279299	13.484314
15.800396	1088.523985	13.489331
15.679902	1100.546618	13.494349
15.787324	1087.574408	13.499367
15.342787	1097.969883	13.504384
15.827329	1101.093991	13.509402
15.595569	1105.930773	13.514419
15.848762	1112.822277	13.519437
15.949297	1127.161618	13.524455
16.111036	1118.502972	13.529472
15.984887	1109.797696	13.534490
15.769122	1097.403575	13.539507
15.523634	1102.344206	13.544525
15.661508	1107.872664	13.549543
15.963024	1108.415517	13.554560
15.814101	1122.752223	13.559578
16.164891	1123.469162	13.564595
15.848519	1127.862162	13.569613
16.012457	1113.323134	13.574631
15.917056	1122.351609	13.579648
15.842848	1118.375646	13.584666
15.993015	1118.015749	13.589683
16.039827	1131.599495	13.594701
16.410489	1124.179287	13.599719
16.238838	1129.646997	13.604736
15.744432	1121.983580	13.609754
15.965864	1119.361559	13.614771
15.704875	1113.078964	13.619789
16.214426	1114.931661	13.624807
16.267298	1117.106705	13.629824
16.341001	1124.974456	13.634842
16.439709	1118.518302	13.639859
16.107447	1125.651599	13.644877
16.352616	1116.043702	13.649895
16.053172	1113.575179	13.654912
16.071197	1120.783712	13.659930
16.388277	1110.483192	13.664947
16.300653	1123.331440	13.669965
16.449701	1123.711062	13.674983
16.323536	1121.716075	13.680000
16.077931	1122.055390	13.685018
16.071363	1125.131608	13.690035
15.929395	1120.652759	13.695053
16.282136	1123.826336	13.700071
16.226941	1116.833586	13.705088
15.733280	1116.001592	13.710106
16.072741	1122.100456	13.715123
16.388755	1148.760865	13.720141
16.516364	1144.050993	13.725159
16.625265	1147.625714	13.730176
16.237322	1153.786830	13.735194
16.555165	1141.376029	13.740211
17.017129	1144.961358	13.745229
16.812074	1147.863493	13.750247
16.806260	1137.378051	13.755264
16.527553	1121.001657	13.760282
16.700222	1121.256886	13.765299
16.397902	1122.189063	13.770317
16.488209	1113.178531	13.775335
16.317144	1121.578275	13.780352
16.519324	1138.576582	13.785370
16.581791	1139.586706	13.790387
16.456433	1148.786703	13.795405
16.369798	1152.175825	13.800423
16.245623	1144.936666	13.805440
16.682150	1150.124570	13.810458
16.530069	1142.497942	13.815475
16.659060	1147.159035	13.820493
15.981342	1144.667163	13.825511
16.442072	1157.444377	13.830528
16.531907	1175.258996	13.835546
16.904336	1184.586899	13.840563
17.050548	1183.533596	13.845581
17.001777	1186.231031	13.850599
17.245855	1172.227816	13.855616
16.815576	1168.976343	13.860634
17.060887	1154.376904	13.865651
16.884705	1148.240429	13.870669
16.735418	1137.334760	13.875687
16.818419	1142.260175	13.880704
16.645190	1164.447032	13.885722
16.813561	1169.942098	13.890739
16.897298	1172.160048	13.895757
17.178053	1175.822350	13.900775
17.145407	1170.009237	13.905792
16.866773	1182.497960	13.910810
17.061635	1179.060304	13.915827
16.996145	1186.392192	13.920845
16.764516	1183.067938	13.925863
16.906966	1166.698659	13.930880
16.805425	1185.347815	13.935898
17.150991	1173.602035	13.940915
17.442008	1181.141977	13.945933
16.991181	1171.766254	13.950951
17.171366	1176.555061	13.955968
17.074863	1183.749589	13.960986
17.314460	1180.357251	13.966003
16.894428	1175.906492	13.971021
16.702841	1168.593097	13.976039
17.266432	1179.640716	13.981056
17.155410	1176.672779	13.986074
17.275285	1195.144995	13.991091
17.482689	1196.906195	13.996109
17.332765	1208.617676	14.001127
17.487943	1199.393565	14.006144
17.637509	1190.075122	14.011162
17.774036	1176.949581	14.016179
17.711663	1173.508225	14.021197
17.583148	1180.168334	14.026215
17.636246	1172.447751	14.031232
17.531240	1186.155985	14.036250
17.177278	1178.401878	14.041267
17.238638	1174.402581	14.046285
17.214798	1176.582509	14.051303
17.146034	1177.092818	14.056320
17.029157	1177.901660	14.061338
17.321817	1195.686923	14.066355
17.680710	1194.639607	14.071373
17.622858	1206.319249	14.076391
17.544452	1192.462523	14.081408
17.642852	1198.892808	14.086426
17.637496	1192.171649	14.091443
17.748277	1208.183694	14.096461
17.798406	1201.460002	14.101479
18.016448	1206.845255	14.106496
17.512276	1211.741517	14.111514
17.859427	1210.970943	14.116531
17.784741	1206.444274	14.121549
17.749183	1214.914062	14.126567
18.063728	1202.091181	14.131584
17.938100	1204.693918	14.136602
17.727786	1186.904182	14.141619
17.876789	1180.985287	14.146637
17.744949	1185.996422	14.151655
17.929824	1186.864162	14.156672
17.719863	1189.555319	14.161690
17.653059	1196.648858	14.166707
17.961041	1195.361984	14.171725
17.759923	1202.804607	14.176743
17.951553	1202.037048	14.181760
17.811348	1210.486826	14.186778
18.109247	1214.923418	14.191795
17.958412	1216.234735	14.196813
17.842922	1208.889383	14.201831
18.182940	1209.375843	14.206848
18.086017	1211.473439	14.211866
18.041177	1198.661476	14.216883
18.089072	1204.874971	14.221901
17.877778	1206.401838	14.226919
18.010498	1192.676156	14.231936
17.791774	1203.548713	14.236954
17.536326	1200.966176	14.241971
17.838021	1204.109673	14.246989
17.514222	1213.382058	14.252007
17.831252	1221.631051	14.257024
18.180709	1234.880741	14.262042
18.167389	1243.728722	14.267059
18.399872	1235.513745	14.272077
18.331545	1239.501786	14.277095
18.361660	1239.538596	14.282112
18.129205	1244.784966	14.287130
18.272197	1237.468683	14.292147
18.568472	1235.769990	14.297165
18.320912	1242.887687	14.302183
18.580120	1235.576104	14.307200
18.636481	1244.246370	14.312218
18.364673	1240.021340	14.317235
18.454863	1238.512404	14.322253
18.311205	1242.959403	14.327271
18.396055	1246.676328	14.332288
18.447854	1241.880212	14.337306
18.258064	1241.073293	14.342323
18.310565	1238.716327	14.347341
18.273577	1238.526898	14.352359
18.317762	1241.764381	14.357376
18.399568	1236.082608	14.362394
18.378109	1242.932422	14.367411
18.581802	1237.262672	14.372429
18.258308	1243.523343	14.377447
18.469222	1253.341105	14.382464
18.604387	1262.659279	14.387482
18.891185	1269.588967	14.392499
18.766952	1266.257475	14.397517
18.557334	1271.292587	14.402535
19.203523	1261.328591	14.407552
19.044379	1268.539869	14.412570
18.683610	1254.217047	14.417587
18.635022	1237.849130	14.422605
18.599666	1243.148171	14.427623
18.612756	1258.471811	14.432640
18.696537	1267.628850	14.437658
18.650002	1277.128408	14.442675
18.744076	1259.226977	14.447693
18.869170	1266.291409	14.452711
18.916047	1260.673304	14.457728
19.248748	1263.969922	14.462746
18.943237	1268.456033	14.467763
19.185602	1260.873627	14.472781
18.940025	1275.174178	14.477799
18.670651	1270.125146	14.482816
18.952250	1273.150743	14.487834
18.760351	1268.533699	14.492851
19.349159	1272.910934	14.497869
19.025548	1276.161524	14.502887
19.093128	1269.427422	14.507904
19.046876	1267.351814	14.512922
18.646634	1270.803321	14.517939
18.890052	1262.898705	14.522957
19.123688	1264.083529	14.527975
18.979023	1267.188632	14.532992
18.944897	1274.125601	14.538010
19.019111	1285.679813	14.543027
18.892231	1286.676143	14.548045
19.465685	1315.590023	14.553063
19.393877	1300.332158	14.558080
19.497388	1306.662035	14.563098
19.158246	1309.881751	14.568115
19.510551	1300.352780	14.573133
19.512192	1303.726870	14.578151
19.575837	1304.546659	14.583168
19.473295	1289.365169	14.588186
19.312912	1276.162913	14.593203
19.457851	1283.090989	14.598221
19.420449	1279.389959	14.603239
19.179012	1295.378354	14.608256
19.633790	1290.120380	14.613274
19.186887	1307.269270	14.618291
19.259762	1306.522625	14.623309
19.305511	1302.295190	14.628327
19.758638	1308.774433	14.633344
19.705739	1306.579851	14.638362
19.613808	1303.342978	14.643379
19.603935	1293.912395	14.648397
19.070772	1306.107314	14.653415
19.194936	1302.162110	14.658432
19.313027	1304.871989	14.663450
19.354644	1303.401827	14.668467
19.691819	1302.786050	14.673485
19.450765	1324.245460	14.678503
19.493733	1324.231316	14.683520
19.836923	1323.736976	14.688538
20.029154	1332.570135	14.693555
19.879494	1328.912552	14.698573
19.985417	1325.540432	14.703591
20.032939	1334.547638	14.708608
19.873520	1330.073990	14.713626
19.646005	1333.247599	14.718643
19.893866	1333.260817	14.723661
20.019724	1330.571184	14.728679
19.830508	1332.077465	14.733696
19.932935	1319.353913	14.738714
19.793103	1328.508785	14.743731
19.940305	1323.093660	14.748749
19.894611	1333.546620	14.753767
19.834687	1329.578464	14.758784
20.164846	1325.902156	14.763802
19.976769	1337.463781	14.768819
20.118852	1325.476126	14.773837
20.123088	1329.695822	14.778855
20.241441	1335.511059	14.783872
20.297550	1334.694367	14.788890
20.041315	1336.164151	14.793907
19.986959	1330.445922	14.798925
20.016595	1325.158600	14.803943
19.839317	1327.045559	14.808960
20.126727	1325.408957	14.813978
19.784426	1328.318583	14.818995
19.885776	1343.336703	14.824013
20.319641	1360.215647	14.829031
20.053641	1366.291621	14.834048
20.367211	1361.639355	14.839066
20.148719	1365.149647	14.844083
20.483023	1365.385104	14.849101
20.462020	1362.946244	14.854119
20.608638	1358.416606	14.859136
20.776489	1358.017152	14.864154
20.764487	1365.187090	14.869171
20.723919	1363.415239	14.874189
20.661248	1369.339707	14.879207
20.566528	1360.136957	14.884224
20.804211	1352.964719	14.889242
20.544751	1334.801498	14.894259
20.196067	1330.503003	14.899277
20.339700	1352.467392	14.904295
20.338263	1355.729804	14.909312
20.459640	1352.188186	14.914330
20.268076	1362.664622	14.919347
20.957472	1354.116565	14.924365
20.904952	1358.352787	14.929383
20.905628	1366.055639	14.934400
20.946997	1354.454767	14.939418
20.928625	1366.818100	14.944435
20.743712	1361.483750	14.949453
20.963731	1356.237214	14.954471
20.652386	1365.737532	14.959488
20.851627	1356.307981	14.964506
20.787946	1367.903676	14.969523
20.260662	1360.040100	14.974541
20.734846	1361.685722	14.979559
20.607947	1362.070663	14.984576
21.160364	1350.583668	14.989594
20.798497	1364.984728	14.994611
21.048797	1353.981392	14.999629
21.012482	1358.184214	15.004647
20.621678	1365.478919	15.009664
20.447659	1366.885437	15.014682
20.792565	1380.352930	15.019699
20.891512	1380.863322	15.024717
21.148377	1379.337300	15.029735
20.867996	1386.501855	15.034752
21.180185	1388.083462	15.039770
20.824956	1393.700670	15.044787
20.695218	1386.606018	15.049805
20.853548	1387.258898	15.054823
21.056753	1408.761906	15.059840
21.458754	1414.058785	15.064858
21.538559	1420.964285	15.069875
21.514182	1396.570383	15.074893
21.558553	1383.923354	15.079911
21.366806	1393.083350	15.084928
21.295225	1379.708771	15.089946
21.229794	1388.859974	15.094963
21.325080	1376.130870	15.099981
21.360083	1378.951418	15.104999
21.312952	1403.363645	15.110016
21.884036	1405.948254	15.115034
21.521273	1392.726780	15.120051
21.550298	1380.722835	15.125069
21.786854	1387.360544	15.130087
21.343051	1391.843692	15.135104
21.579181	1382.248157	15.140122
21.060259	1392.919567	15.145139
21.126281	1407.333406	15.150157
21.695499	1420.386892	15.155175
21.321069	1435.351111	15.160192
21.599620	1421.348242	15.165210
21.520453	1425.836542	15.170227
21.651234	1422.694120	15.175245
21.820860	1425.339157	15.180263
21.806217	1420.907954	15.185280
21.883911	1420.185305	15.190298
21.815865	1422.789138	15.195315
21.951738	1420.530488	15.200333
22.127350	1414.424017	15.205351
21.555522	1422.459837	15.210368
21.732222	1421.074296	15.215386
21.569890	1414.324408	15.220403
21.724710	1416.156575	15.225421
22.005050	1419.504841	15.230439
21.695462	1422.837774	15.235456
21.705041	1424.057488	15.240474
21.617806	1412.747623	15.245491
21.846488	1435.136168	15.250509
22.224127	1447.732952	15.255527
22.092950	1444.728156	15.260544
22.502486	1448.482501	15.265562
22.042900	1438.346282	15.270579
21.992519	1454.944800	15.275597
22.527987	1445.262075	15.280615
22.114198	1443.115644	15.285632
21.976469	1442.394940	15.290650
22.253207	1451.201524	15.295667
22.255800	1457.593511	15.300685
22.467807	1453.981297	15.305703
21.855546	1457.996807	15.310720
22.146826	1452.413601	15.315738
22.253405	1448.684662	15.320755
22.346449	1451.771947	15.325773
22.307573	1448.710472	15.330791
22.316574	1452.715636	15.335808
22.129976	1441.972642	15.340826
22.500562	1442.647332	15.345843
22.312235	1455.539362	15.350861
22.716483	1450.748774	15.355879
22.358233	1455.524011	15.360896
22.205135	1447.200966	15.365914
22.517407	1437.834467	15.370931
22.134441	1439.936329	15.375949
22.454476	1435.683742	15.380967
22.574823	1456.313607	15.385984
22.790448	1460.276163	15.391002
22.669970	1454.434236	15.396019
22.851012	1452.521214	15.401037
22.989578	1443.954819	15.406055
22.548566	1446.114359	15.411072
22.808262	1449.537320	15.416090
22.986468	1443.960706	15.421107
22.796502	1444.051416	15.426125
23.164744	1436.179508	15.431143
22.703855	1440.751334	15.436160
22.858906	1449.878132	15.441178
22.710211	1435.202581	15.446195
22.845876	1443.131847	15.451213
23.054485	1435.752598	15.456231
22.776667	1449.855130	15.461248
22.711765	1442.600468	15.466266
22.882375	1459.041793	15.471283
22.740479	1458.583191	15.476301
23.084507	1464.153100	15.481319
23.261657	1471.322357	15.486336
23.171442	1472.168908	15.491354
23.232298	1472.439185	15.496371
23.488268	1480.872870	15.501389
23.544715	1463.622321	15.506407
23.200573	1445.108883	15.511424
23.198552	1443.842018	15.516442
23.402769	1430.700288	15.521459
23.123621	1434.399412	15.526477
23.145859	1420.895822	15.531495
23.133531	1428.558741	15.536512
22.894383	1438.843931	15.541530
23.153276	1453.673380	15.546547
23.144040	1465.887247	15.551565
23.700777	1468.883295	15.556583
23.163854	1467.332113	15.561600
23.245687	1461.930560	15.566618
23.180911	1459.898949	15.571635
23.184563	1466.913974	15.576653
23.474061	1470.401276	15.581671
22.978447	1477.592197	15.586688
23.194910	1483.150639	15.591706
23.612824	1474.215760	15.596723
23.695875	1481.936474	15.601741
23.442473	1478.150826	15.606759
23.480702	1477.994954	15.611776
23.307457	1478.543897	15.616794
23.483155	1489.185749	15.621811
23.693677	1499.926936	15.626829
23.676699	1494.892179	15.631847
23.526987	1503.090948	15.636864
23.794142	1499.673489	15.641882
23.890933	1497.402428	15.646899
23.727289	1501.872113	15.651917
23.867033	1505.215814	15.656935
23.562669	1505.085780	15.661952
23.669973	1498.668196	15.666970
23.494275	1497.836874	15.671987
23.265619	1505.916091	15.677005
23.818172	1502.833078	15.682023
23.919310	1507.350488	15.687040
24.026701	1527.869611	15.692058
24.113767	1521.545931	15.697075
24.015048	1532.729473	15.702093
24.458119	1525.804509	15.707111
24.294930	1506.656212	15.712128
24.250911	1504.380206	15.717146
24.153034	1489.766628	15.722163
23.853483	1493.489235	15.727181
24.020298	1493.391517	15.732199
23.890354	1499.023680	15.737216
23.899414	1514.722249	15.742234
24.112270	1521.927326	15.747251
23.886111	1530.997849	15.752269
24.091986	1524.898115	15.757287
24.567665	1529.389501	15.762304
24.492355	1528.348978	15.767322
24.752362	1526.211411	15.772339
24.519510	1530.772527	15.777357
24.422469	1533.363481	15.782375
24.524163	1521.117040	15.787392
24.493374	1530.319654	15.792410
24.322868	1521.939227	15.797427
24.479419	1527.522997	15.802445
24.492312	1525.313511	15.807463
24.452347	1526.128486	15.812480
24.397140	1525.518863	15.817498
24.715546	1522.467675	15.822515
24.400237	1537.964280	15.827533
24.592003	1531.587761	15.832551
24.606500	1525.673768	15.837568
24.478625	1523.395162	15.842586
24.692283	1521.106248	15.847603
24.289813	1521.226766	15.852621
24.474001	1543.208700	15.857639
24.609173	1545.519335	15.862656
25.081804	1546.988074	15.867674
25.004383	1543.414495	15.872691
24.620633	1541.282348	15.877709
24.559141	1545.100437	15.882727
24.952354	1540.159692	15.887744
24.825736	1542.980361	15.892762
25.119067	1543.531285	15.897779
25.361932	1546.986986	15.902797
25.220668	1554.484787	15.907815
25.433383	1537.386133	15.912832
24.916969	1545.512409	15.917850
25.482118	1535.135341	15.922867
25.231795	1535.597492	15.927885
25.073313	1527.467420	15.932903
25.202776	1521.868565	15.937920
24.993826	1516.326744	15.942938
25.577447	1513.627532	15.947955
25.064744	1521.544129	15.952973
25.019083	1515.068893	15.957991
25.123948	1527.632733	15.963008
25.558144	1534.477021	15.968026
25.332163	1540.409012	15.973043
25.276153	1545.793083	15.978061
25.304730	1551.664661	15.983079
25.221091	1540.953303	15.988096
25.144660	1556.897221	15.993114
25.417762	1541.606201	15.998131
25.207544	1544.989965	16.003149
25.202157	1548.187327	16.008167
25.631509	1538.489111	16.013184
25.396336	1543.699026	16.018202
25.445917	1546.725051	16.023219
25.402399	1552.923959	16.028237
25.195692	1543.983801	16.033255
25.699914	1557.138362	16.038272
25.633280	1572.567687	16.043290
25.672057	1574.129796	16.048307
25.736969	1567.619232	16.053325
25.606023	1568.718615	16.058343
26.209296	1562.677225	16.063360
25.909979	1574.320112	16.068378
26.067194	1555.970059	16.073395
25.992040	1546.095064	16.078413
25.970341	1541.844523	16.083431
26.254756	1539.984781	16.088448
25.774800	1536.176538	16.093466
25.928776	1539.611973	16.098483
26.281636	1538.815239	16.103501
25.920641	1542.007531	16.108519
25.889936	1536.116795	16.113536
25.860095	1537.515506	16.118554
26.024901	1537.916535	16.123571
25.964784	1545.699657	16.128589
26.100269	1558.363942	16.133607
26.076839	1559.602539	16.138624
26.258269	1576.213839	16.143642
26.552604	1564.419195	16.148659
26.550981	1563.824680	16.153677
25.903837	1549.340523	16.158695
26.511365	1552.457671	16.163712
26.242696	1560.333335	16.168730
26.387525	1560.751070	16.173747
26.402343	1561.357339	16.178765
26.301772	1568.020449	16.183783
26.346941	1570.088572	16.188800
26.478006	1569.070831	16.193818
26.599869	1561.932313	16.198835
26.527462	1563.817619	16.203853
26.455847	1566.731904	16.208871
26.598431	1552.718051	16.213888
26.509164	1569.957392	16.218906
26.704734	1565.145549	16.223923
26.577592	1560.160576	16.228941
26.422899	1564.120929	16.233959
26.461483	1555.786439	16.238976
26.190408	1566.988809	16.243994
26.182676	1559.090747	16.249011
26.436505	1571.092474	16.254029
26.352022	1563.250865	16.259047
26.470791	1570.990883	16.264064
26.625253	1587.065744	16.269082
26.541356	1588.845484	16.274099
26.648763	1596.924404	16.279117
26.519314	1594.478729	16.284135
26.589109	1589.487786	16.289152
26.910476	1593.101707	16.294170
27.270052	1586.908689	16.299187
27.151109	1589.563921	16.304205
26.749380	1592.372843	16.309223
26.970472	1588.061071	16.314240
26.676115	1588.682508	16.319258
26.937047	1600.113404	16.324275
27.240310	1616.192303	16.329293
27.151871	1611.159937	16.334311
27.862787	1611.763899	16.339328
26.994911	1600.532067	16.344346
27.242501	1585.686969	16.349363
27.451276	1593.667939	16.354381
27.284810	1593.810254	16.359399
27.616650	1588.563953	16.364416
27.377500	1591.836002	16.369434
27.401737	1590.271853	16.374451
27.958255	1588.527114	16.379469
27.099359	1583.430686	16.384487
27.359249	1583.704498	16.389504
27.452526	1576.253803	16.394522
27.459099	1589.988730	16.399539
27.552053	1591.942222	16.404557
27.334503	1607.705713	16.409575
27.731478	1609.176798	16.414592
27.540314	1615.213658	16.419610
27.661130	1617.942036	16.424627
27.661344	1621.569577	16.429645
27.433309	1618.508799	16.434663
27.268965	1624.034129	16.439680
27.325071	1619.720636	16.444698
27.590734	1616.343557	16.449715
28.315508	1613.150405	16.454733
27.663008	1619.189928	16.459751
27.752076	1616.841000	16.464768
27.960384	1618.526510	16.469786
27.810808	1616.959751	16.474803
27.687978	1617.223158	16.479821
27.825161	1621.584220	16.484839
28.040202	1614.977819	16.489856
27.847203	1628.253439	16.494874
27.958745	1643.442200	16.499891
28.469204	1639.516565	16.504909
28.304379	1638.444850	16.509927
28.002059	1626.607988	16.514944
27.939793	1623.316118	16.519962
28.114244	1642.545138	16.524979
28.253569	1644.298414	16.529997
28.332931	1646.784085	16.535015
28.054799	1644.154849	16.540032
27.904879	1639.607487	16.545050
28.131186	1650.324109	16.550067
28.620933	1643.388579	16.555085
28.426836	1643.996897	16.560103
28.672354	1636.751574	16.565120
28.801384	1641.366748	16.570138
28.708780	1637.548824	16.575155
28.756697	1626.218309	16.580173
28.788481	1625.321395	16.585191
28.711571	1615.556881	16.590208
28.235898	1609.387716	16.595226
28.659359	1612.447676	16.600243
28.547199	1617.243477	16.605261
28.528182	1625.804833	16.610279
28.975853	1625.302568	16.615296
28.915353	1626.978819	16.620314
28.551747	1622.335484	16.625331
28.655885	1626.769754	16.630349
28.756551	1628.504257	16.635367
28.972955	1626.203454	16.640384
28.842732	1633.845125	16.645402
28.963953	1637.554131	16.650419
29.102693	1625.227830	16.655437
28.980501	1638.217286	16.660455
28.599381	1632.723329	16.665472
28.762475	1636.995838	16.670490
28.733212	1624.142352	16.675507
29.121132	1631.375864	16.680525
28.650634	1632.650187	16.685543
29.090899	1632.860165	16.690560
28.819671	1631.232916	16.695578
28.970748	1637.473136	16.700595
29.129536	1625.660029	16.705613
28.962708	1639.404922	16.710631
29.164832	1647.277185	16.715648
28.999284	1660.674645	16.720666
29.147152	1667.955552	16.725683
29.308344	1663.009630	16.730701
29.251206	1668.507709	16.735719
29.670558	1663.148414	16.740736
29.521281	1665.904368	16.745754
29.580277	1673.454768	16.750771
29.712920	1662.088098	16.755789
29.193495	1658.197409	16.760807
29.849426	1667.607619	16.765824
29.611820	1659.299686	16.770842
29.500338	1661.473383	16.775859
29.864010	1665.961772	16.780877
29.469340	1665.390847	16.785895
29.381420	1660.843803	16.790912
29.787838	1662.344819	16.795930
29.352035	1664.228330	16.800947
29.781652	1666.562879	16.805965
29.474939	1671.568195	16.810983
29.563195	1664.082465	16.816000
29.562612	1672.419920	16.821018
29.799255	1689.770580	16.826035
30.138643	1695.386621	16.831053
30.030858	1686.227974	16.836071
29.856516	1696.069891	16.841088
30.019373	1686.055644	16.846106
29.809625	1697.317599	16.851123
30.046913	1690.126375	16.856141
30.070446	1687.718644	16.861159
29.925141	1688.594441	16.866176
30.524850	1680.654020	16.871194
29.954869	1694.126994	16.876211
30.175967	1686.945154	16.881229
30.232331	1694.662536	16.886247
29.964287	1693.303251	16.891264
30.198382	1685.535402	16.896282
30.119501	1692.450468	16.901299
30.657620	1674.331453	16.906317
30.436318	1686.220508	16.911335
30.195926	1692.323060	16.916352
30.085673	1686.584461	16.921370
30.281712	1684.889389	16.926387
30.313264	1702.177694	16.931405
30.495149	1713.011583	16.936423
30.805217	1719.745090	16.941440
30.986006	1713.769530	16.946458
30.755453	1719.294480	16.951475
30.546988	1691.033513	16.956493
30.070817	1701.851569	16.961511
30.410516	1705.088065	16.966528
30.864488	1711.924422	16.971546
30.416183	1719.689078	16.976563
30.431049	1717.994192	16.981581
30.657917	1719.584897	16.986599
30.577420	1718.439319	16.991616
30.924523	1709.821584	16.996634
30.728269	1715.604214	17.001651
30.943541	1717.569283	17.006669
31.444646	1724.008839	17.011687
30.885170	1719.014174	17.016704
31.382460	1703.846363	17.021722
30.686538	1704.962885	17.026739
30.917498	1697.807354	17.031757
31.364566	1720.839536	17.036775
31.217505	1722.781756	17.041792
31.758037	1731.902527	17.046810
31.346229	1724.491612	17.051827
31.463825	1705.989307	17.056845
31.245164	1705.278105	17.061863
31.152739	1704.052227	17.066880
31.521253	1692.930188	17.071898
31.500392	1702.056451	17.076915
31.625562	1695.008267	17.081933
31.407297	1698.472927	17.086951
31.227487	1693.032891	17.091968
31.392242	1698.933072	17.096986
31.702785	1711.318784	17.102003
31.750736	1720.956057	17.107021
31.582791	1711.868417	17.112039
31.567670	1706.885250	17.117056
31.539624	1713.842270	17.122074
31.832749	1729.689905	17.127091
32.022314	1724.750272	17.132109
31.978814	1723.912714	17.137127
31.111644	1711.261014	17.142144
31.670624	1712.173301	17.147162
31.334355	1721.510263	17.152179
31.851048	1730.129096	17.157197
31.725437	1725.047753	17.162215
31.622634	1730.310926	17.167232
31.808738	1724.246290	17.172250
31.898153	1735.705400	17.177267
32.058165	1731.597045	17.182285
32.133982	1733.088055	17.187303
31.896468	1736.418523	17.192320
32.233792	1752.493872	17.197338
32.236078	1756.165194	17.202355
32.066280	1760.074958	17.207373
32.379162	1755.862450	17.212391
32.376979	1761.527804	17.217408
32.300409	1757.933955	17.222426
32.202264	1766.967197	17.227443
32.547474	1770.139013	17.232461
32.666209	1756.601376	17.237479
32.397691	1743.851728	17.242496
32.527264	1740.324802	17.247514
32.301175	1746.088387	17.252531
32.143699	1759.988523	17.257549
32.581324	1756.251341	17.262567
32.199656	1759.218375	17.267584
32.506874	1751.486371	17.272602
32.586080	1753.893739	17.277619
32.420700	1754.610673	17.282637
32.654664	1754.371874	17.287655
32.261120	1764.186093	17.292672
32.420852	1755.088061	17.297690
32.602620	1748.588708	17.302707
32.456835	1772.162801	17.307725
32.935111	1771.799146	17.312743
32.767178	1778.932987	17.317760
32.812512	1782.345981	17.322778
33.280525	1785.433217	17.327795
33.251094	1781.750033	17.332813
32.968758	1787.707231	17.337831
33.079974	1787.472691	17.342848
33.296935	1774.782487	17.347866
33.315068	1777.053554	17.352883
33.381753	1771.683151	17.357901
33.429380	1774.806002	17.362919
33.269850	1777.805804	17.367936
33.279845	1769.797601	17.372954
33.253892	1764.665430	17.377971
33.643678	1770.680206	17.382989
33.275883	1760.903710	17.388007
32.999186	1779.015372	17.393024
33.364812	1772.911826	17.398042
33.441813	1771.654241	17.403059
33.572633	1780.887624	17.408077
33.755745	1767.894392	17.413095
33.835492	1776.808311	17.418112
33.719058	1775.972242	17.423130
33.644103	1772.160013	17.428147
33.516454	1775.895454	17.433165
33.343297	1772.155451	17.438183
33.350274	1771.586270	17.443200
33.518506	1767.444257	17.448218
33.532232	1774.164049	17.453235
33.686706	1774.627432	17.458253
33.715349	1776.897933	17.463271
33.649054	1776.204711	17.468288
33.912024	1783.610635	17.473306
34.015215	1798.719835	17.478323
33.764933	1814.067324	17.483341
34.460691	1811.567142	17.488359
34.004214	1803.676607	17.493376
34.733016	1785.185617	17.498394
34.502114	1774.034797	17.503411
34.228556	1763.184773	17.508429
34.220334	1748.703686	17.513447
34.090406	1748.886780	17.518464
34.342360	1754.512649	17.523482
34.569799	1751.744251	17.528499
34.574547	1756.463185	17.533517
34.250234	1747.040492	17.538535
34.425014	1754.952788	17.543552
34.247025	1750.569898	17.548570
34.261116	1747.820030	17.553587
34.076913	1763.680104	17.558605
34.691382	1761.103283	17.563623
34.581744	1768.440420	17.568640
34.654763	1773.217304	17.573658
34.639502	1765.261726	17.578675
34.349086	1777.088322	17.583693
34.313262	1776.403815	17.588711
34.477953	1785.589839	17.593728
34.595057	1787.262574	17.598746
34.794250	1789.394496	17.603763
34.788854	1789.102960	17.608781
34.736178	1788.792510	17.613799
34.622930	1792.045250	17.618816
34.671236	1785.223971	17.623834
34.493901	1788.765312	17.628851
34.671221	1787.734752	17.633869
34.839548	1805.743742	17.638887
34.920400	1810.117369	17.643904
35.116650	1815.117090	17.648922
35.106185	1813.586639	17.653939
35.028396	1822.346846	17.658957
35.220118	1811.915913	17.663975
35.093329	1801.608788	17.668992
35.120215	1805.587449	17.674010
35.191131	1808.773364	17.679027
35.003069	1816.467257	17.684045
35.255125	1813.343577	17.689063
35.149203	1807.405397	17.694080
35.334004	1813.511737	17.699098
35.702001	1825.159651	17.704115
35.690355	1834.018320	17.709133
35.447075	1819.964026	17.714151
35.534270	1834.470805	17.719168
35.533299	1839.257644	17.724186
35.907249	1839.019200	17.729203
35.640120	1838.170772	17.734221
35.798959	1834.251561	17.739239
35.723387	1835.511837	17.744256
35.519511	1835.000926	17.749274
35.952744	1834.110507	17.754291
35.923897	1834.000031	17.759309
36.088911	1840.151797	17.764327
36.120287	1832.549849	17.769344
36.115931	1841.190777	17.774362
36.209387	1831.245452	17.779379
35.904169	1844.158412	17.784397
35.977138	1822.261430	17.789415
36.155911	1836.864408	17.794432
36.110020	1841.878791	17.799450
36.436918	1828.541534	17.804467
35.887770	1826.660455	17.809485
36.245346	1838.177828	17.814503
36.181814	1835.208169	17.819520
36.179460	1830.624414	17.824538
35.790575	1831.456056	17.829555
36.066933	1832.593668	17.834573
36.098168	1836.988541	17.839591
36.366515	1847.717998	17.844608
36.191860	1864.076192	17.849626
36.812276	1853.136975	17.854643
36.464762	1862.938093	17.859661
36.624499	1859.889197	17.864679
36.578404	1860.752845	17.869696
36.829378	1854.175410	17.874714
37.037029	1861.968518	17.879731
37.182611	1859.984570	17.884749
37.080453	1868.087832	17.889767
37.061561	1867.224522	17.894784
36.795248	1850.805924	17.899802
37.051734	1842.564986	17.904819
36.926396	1851.394923	17.909837
37.285272	1844.703103	17.914855
37.227272	1836.536483	17.919872
36.881643	1832.651115	17.924890
36.932569	1820.905786	17.929907
36.801442	1823.221352	17.934925
36.978664	1839.857651	17.939943
37.051987	1857.869893	17.944960
37.003130	1854.637556	17.949978
37.150831	1857.405604	17.954995
37.038813	1853.060540	17.960013
37.301113	1850.979635	17.965031
37.097286	1863.448202	17.970048
37.279432	1857.975510	17.975066
37.356889	1857.941067	17.980083
37.288204	1854.815568	17.985101
37.173463	1853.322523	17.990119
37.354304	1885.175154	17.995136
37.690246	1887.437906	18.000154
37.729627	1886.178297	18.005171
37.741544	1888.316162	18.010189
37.864083	1887.490369	18.015207
37.674497	1887.297947	18.020224
37.536114	1887.867093	18.025242
37.700573	1883.078039	18.030259
37.485852	1897.722063	18.035277
37.805609	1885.972557	18.040295
37.876733	1885.661608	18.045312
37.452186	1889.567681	18.050330
37.556588	1885.329945	18.055347
37.521687	1899.487787	18.060365
37.716942	1910.138884	18.065383
38.295627	1908.935704	18.070400
37.927178	1916.057264	18.075418
38.036673	1905.377729	18.080435
38.033995	1917.844798	18.085453
37.770393	1908.462704	18.090471
38.267890	1909.891128	18.095488
37.881470	1928.000333	18.100506
38.388286	1933.461076	18.105523
38.094341	1944.574604	18.110541
38.408395	1944.015798	18.115559
38.716909	1943.253582	18.120576
38.719970	1936.835427	18.125594
38.979257	1928.814057	18.130611
38.635696	1939.625591	18.135629
38.411435	1938.784205	18.140647
38.938479	1935.893934	18.145664
38.793252	1941.098874	18.150682
38.552670	1929.318447	18.155699
38.612510	1928.270396	18.160717
38.400701	1940.092318	18.165735
38.545839	1941.967891	18.170752
38.772240	1942.374443	18.175770
39.137101	1931.396149	18.180787
38.715835	1931.281995	18.185805
38.937418	1936.757861	18.190823
39.400166	1950.395243	18.195840
38.875141	1948.574707	18.200858
39.438692	1958.524468	18.205875
39.049264	1961.759758	18.210893
38.903081	1961.407364	18.215911
39.043369	1959.167590	18.220928
39.086225	1966.018844	18.225946
39.574609	1955.783392	18.230963
39.129799	1957.899536	18.235981
39.195038	1954.403726	18.240999
39.622857	1949.310252	18.246016
39.412264	1962.154433	18.251034
39.637833	1957.134727	18.256051
39.684760	1954.633303	18.261069
39.445865	1960.358149	18.266087
39.971013	1957.159133	18.271104
39.616391	1964.663063	18.276122
39.830780	1956.836937	18.281139
39.636020	1955.563874	18.286157
39.569048	1955.893200	18.291175
39.833806	1955.508335	18.296192
39.360154	1966.610014	18.301210
39.418536	1958.218475	18.306227
39.977653	1982.532036	18.311245
39.527254	1992.477894	18.316263
40.160653	1995.006975	18.321280
40.156873	2000.227403	18.326298
40.363939	1998.721411	18.331315
40.452282	1993.341033	18.336333
40.237081	2000.425350	18.341351
40.284068	1994.967592	18.346368
39.842335	1989.553660	18.351386
40.242790	1992.165156	18.356403
40.171794	1993.813269	18.361421
40.287272	1987.446882	18.366439
40.219628	1990.387752	18.371456
40.269823	1988.348380	18.376474
40.536457	1987.033671	18.381491
40.192534	1987.242490	18.386509
39.914011	1993.135747	18.391527
40.591653	1998.378751	18.396544
40.738380	2010.271061	18.401562
40.741639	2011.513131	18.406579
40.870857	2009.488970	18.411597
40.736299	2012.220491	18.416615
41.001991	2008.830725	18.421632
40.983787	2010.108647	18.426650
40.990507	2004.833563	18.431667
41.390061	2002.445180	18.436685
40.917958	2013.423799	18.441703
41.341942	2004.275405	18.446720
41.387409	2004.623446	18.451738
41.103358	2000.738037	18.456755
41.295448	2010.778703	18.461773
41.101493	2007.325959	18.466791
41.292141	2008.404601	18.471808
41.335319	2009.673108	18.476826
41.152768	2002.638132	18.481843
40.806360	1999.602462	18.486861
41.079936	2001.146064	18.491879
41.341122	2002.036998	18.496896
40.954373	2005.029330	18.501914
41.542003	2009.396741	18.506931
41.659581	2016.092291	18.511949
41.546568	2036.497143	18.516967
41.748608	2036.558137	18.521984
41.429090	2040.868054	18.527002
41.660294	2030.180411	18.532019
41.968977	2033.948515	18.537037
41.683414	2037.448057	18.542055
41.897229	2028.903874	18.547072
41.744918	2038.786833	18.552090
41.446475	2031.228581	18.557107
42.060056	2038.636987	18.562125
41.729308	2039.261338	18.567143
42.117581	2026.579859	18.572160
41.963922	2027.676749	18.577178
41.689948	2037.183862	18.582195
41.984194	2045.309917	18.587213
41.749703	2062.830243	18.592231
42.057106	2061.212292	18.597248
42.113278	2067.635784	18.602266
41.988481	2069.907420	18.607283
42.171799	2065.213996	18.612301
42.125344	2065.984407	18.617319
42.095456	2063.946131	18.622336
42.584590	2084.117504	18.627354
42.830335	2093.119765	18.632371
43.084548	2084.197180	18.637389
42.676727	2068.154630	18.642407
42.697174	2058.960277	18.647424
42.735022	2056.521370	18.652442
42.556236	2054.924380	18.657459
43.108809	2054.456247	18.662477
42.903793	2066.804700	18.667495
42.832950	2049.430954	18.672512
43.068689	2050.346199	18.677530
42.819002	2052.351184	18.682547
43.153340	2057.697723	18.687565
43.148324	2075.619299	18.692583
43.198828	2074.387354	18.697600
42.916903	2059.633352	18.702618
43.106863	2081.182803	18.707635
43.241167	2081.008990	18.712653
43.221159	2086.294350	18.717671
43.603945	2082.887076	18.722688
43.346124	2086.069810	18.727706
43.485818	2091.105398	18.732723
43.332698	2076.415800	18.737741
43.190064	2083.419196	18.742759
43.343550	2078.704348	18.747776
43.523901	2082.648912	18.752794
43.660545	2080.841621	18.757811
43.299188	2080.065532	18.762829
43.148301	2084.605705	18.767847
43.236684	2079.486317	18.772864
43.815942	2103.556955	18.777882
43.633750	2102.979044	18.782899
44.129630	2092.233983	18.787917
44.134971	2106.247134	18.792935
44.023269	2099.503886	18.797952
44.054090	2108.349748	18.802970
43.938218	2096.142951	18.807987
44.301629	2098.843694	18.813005
44.037944	2114.412607	18.818023
44.251447	2103.160525	18.823040
44.163235	2099.362623	18.828058
44.277680	2108.260336	18.833075
44.317151	2096.676154	18.838093
44.144913	2107.447913	18.843111
44.055669	2101.073771	18.848128
44.307284	2105.007285	18.853146
44.343042	2100.960036	18.858163
44.821423	2102.718039	18.863181
44.131448	2111.619524	18.868199
44.304814	2122.964179	18.873216
44.498231	2138.323679	18.878234
44.565934	2141.608230	18.883251
44.628726	2129.721324	18.888269
44.513586	2136.785923	18.893287
44.390751	2138.630465	18.898304
44.498688	2137.005500	18.903322
44.919189	2156.715533	18.908339
45.224590	2154.955384	18.913357
45.248757	2157.005028	18.918375
45.469268	2158.066906	18.923392
45.653947	2138.896628	18.928410
45.278819	2119.488698	18.933427
45.235479	2119.041648	18.938445
45.271726	2119.029408	18.943463
45.183565	2119.613050	18.948480
45.279581	2116.623120	18.953498
45.302835	2121.011920	18.958515
45.523792	2117.257907	18.963533
45.078274	2122.015170	18.968551
45.318554	2121.151294	18.973568
45.727485	2134.190295	18.978586
45.367901	2142.505383	18.983603
45.751482	2145.862242	18.988621
45.467737	2149.145361	18.993639
45.586773	2153.953691	18.998656
45.774559	2153.324524	19.003674
45.340551	2146.375369	19.008691
45.578005	2145.652514	19.013709
45.546912	2148.305444	19.018727
45.490037	2149.893746	19.023744
45.966510	2158.369503	19.028762
46.101866	2177.943486	19.033779
46.328995	2182.039753	19.038797
46.086424	2180.262797	19.043815
46.167923	2180.798165	19.048832
46.025933	2181.725800	19.053850
46.139975	2183.592791	19.058867
46.431905	2180.271858	19.063885
46.551127	2177.155223	19.068903
46.357500	2180.523373	19.073920
46.484169	2181.092179	19.078938
46.816545	2180.506305	19.083955
46.497538	2173.199042	19.088973
46.697015	2168.871412	19.093991
46.484765	2174.021033	19.099008
46.745667	2179.175878	19.104026
46.437298	2176.133851	19.109043
46.403883	2175.934366	19.114061
46.552292	2186.560762	19.119079
46.741128	2179.883280	19.124096
46.879046	2179.652565	19.129114
46.652622	2197.041384	19.134131
46.803303	2198.173533	19.139149
47.305898	2195.423109	19.144167
46.976025	2206.169952	19.149184
47.246454	2205.171530	19.154202
47.422575	2199.607592	19.159219
47.569476	2193.729215	19.164237
47.409701	2193.258206	19.169255
47.572868	2195.537121	19.174272
47.621940	2186.924166	19.179290
47.637397	2191.023725	19.184307
47.578100	2195.324295	19.189325
47.529189	2195.991575	19.194343
47.544080	2198.719551	19.199360
47.765746	2187.845980	19.204378
47.746966	2193.817405	19.209395
48.040956	2190.881961	19.214413
48.026982	2192.119823	19.219431
47.827814	2190.821882	19.224448
48.025835	2170.550508	19.229466
47.834827	2179.500995	19.234483
47.942822	2171.103851	19.239501
48.130100	2178.573728	19.244519
47.799504	2178.948053	19.249536
47.904718	2190.052898	19.254554
47.906724	2196.059453	19.259571
47.974711	2184.584248	19.264589
47.806828	2180.791299	19.269607
48.245853	2184.868100	19.274624
48.149537	2184.108980	19.279642
48.086476	2187.744414	19.284659
48.274566	2189.525082	19.289677
48.077667	2205.808590	19.294695
48.115776	2221.449501	19.299712
48.655949	2225.782736	19.304730
48.178604	2232.569773	19.309747
48.217593	2220.761558	19.314765
48.232917	2223.469387	19.319783
48.340755	2231.554473	19.324800
48.794857	2247.184936	19.329818
48.617943	2239.557563	19.334835
48.936762	2242.638587	19.339853
49.013464	2242.481432	19.344871
48.939252	2256.641014	19.349888
48.856143	2242.240811	19.354906
49.065575	2241.306463	19.359923
49.123231	2249.942823	19.364941
49.419363	2254.594584	19.369959
49.021889	2249.285410	19.374976
48.959495	2238.213339	19.379994
49.384412	2246.790629	19.385011
48.996214	2238.892065	19.390029
49.601207	2246.615393	19.395047
49.413261	2259.522592	19.400064
50.116680	2257.935265	19.405082
49.957251	2247.699805	19.410099
49.685343	2228.895462	19.415117
49.744826	2218.840966	19.420135
49.646701	2227.191387	19.425152
50.018891	2221.388552	19.430170
50.076165	2223.278368	19.435187
49.912508	2214.990129	19.440205
50.174309	2214.970326	19.445223
49.866483	2223.834346	19.450240
50.449946	2220.550388	19.455258
49.923977	2225.521844	19.460275
49.968618	2220.437240	19.465293
50.058688	2221.046777	19.470311
49.938968	2236.637948	19.475328
50.180955	2243.708599	19.480346
50.390508	2245.777839	19.485363
50.629263	2252.012791	19.490381
51.108779	2246.346444	19.495399
50.911452	2242.571759	19.500416
50.942221	2223.153328	19.505434
50.458428	2219.636105	19.510451
50.631884	2214.293082	19.515469
50.529211	2211.060559	19.520487
50.556797	2221.308232	19.525504
50.939143	2237.382510	19.530522
50.807073	2249.391026	19.535539
50.710211	2246.909909	19.540557
50.720213	2249.083575	19.545575
50.456759	2255.687433	19.550592
50.588159	2255.145195	19.555610
50.776591	2255.457277	19.560627
50.882943	2249.870664	19.565645
51.106341	2253.577011	19.570663
51.259752	2272.235887	19.575680
51.167442	2276.234479	19.580698
51.424494	2270.353514	19.585715
51.214706	2275.905130	19.590733
51.540100	2272.215222	19.595751
51.493335	2274.725894	19.600768
51.352107	2270.670219	19.605786
51.528040	2276.863652	19.610803
51.367517	2274.016724	19.615821
51.733596	2260.916687	19.620839
51.207493	2268.313431	19.625856
51.369573	2263.009684	19.630874
51.514659	2287.275604	19.635891
51.391550	2305.770630	19.640909
51.776955	2289.186953	19.645927
51.783558	2293.643924	19.650944
52.012585	2289.141661	19.655962
52.189965	2284.863342	19.660979
51.833089	2305.616170	19.665997
51.885928	2290.340158	19.671015
51.768912	2298.328786	19.676032
52.368859	2314.668563	19.681050
52.236671	2320.165171	19.686067
52.076227	2327.389752	19.691085
52.567743	2320.746160	19.696103
52.384989	2317.500939	19.701120
52.672317	2305.245078	19.706138
52.417820	2321.205986	19.711155
52.565527	2329.717974	19.716173
52.821529	2316.832646	19.721191
52.761195	2320.155444	19.726208
52.735551	2324.741409	19.731226
53.230510	2317.980708	19.736243
52.998176	2310.550704	19.741261
52.946357	2314.985501	19.746279
53.081484	2318.990793	19.751296
53.206403	2315.531836	19.756314
53.117411	2312.271427	19.761331
53.417594	2320.986815	19.766349
53.186395	2309.926999	19.771367
53.114577	2319.502263	19.776384
53.060115	2312.334043	19.781402
53.477284	2327.251416	19.786419
53.641652	2342.372634	19.791437
53.643517	2344.135450	19.796455
53.733668	2347.810026	19.801472
53.744539	2333.697672	19.806490
53.791800	2318.274916	19.811507
53.478323	2331.551472	19.816525
53.867158	2328.886863	19.821543
53.414413	2341.058195	19.826560
53.385964	2341.294903	19.831578
53.432550	2331.353898	19.836595
53.283779	2344.776718	19.841613
53.532921	2352.797438	19.846631
53.687675	2366.559213	19.851648
53.825843	2373.920020	19.856666
53.726118	2369.404652	19.861683
54.057415	2369.517792	19.866701
54.274304	2379.271102	19.871719
54.642257	2388.503628	19.876736
54.461700	2390.207000	19.881754
54.717818	2396.897801	19.886771
54.538187	2396.879706	19.891789
54.983572	2393.258807	19.896807
54.846301	2386.706696	19.901824
54.473735	2373.576170	19.906842
54.633938	2383.223939	19.911859
54.990167	2393.976968	19.916877
55.066313	2391.799762	19.921895
55.291950	2391.486353	19.926912
54.890290	2383.579322	19.931930
55.408855	2378.643468	19.936947
55.106509	2368.680506	19.941965
55.089119	2359.804084	19.946983
55.181503	2364.238158	19.952000
55.074105	2384.086611	19.957018
55.066398	2386.656953	19.962035
54.860900	2390.477528	19.967053
55.350075	2393.127502	19.972071
55.324705	2394.113723	19.977088
55.206827	2387.797766	19.982106
55.501533	2391.760021	19.987123
55.289195	2388.109453	19.992141
55.494892	2381.380262	19.997159
55.424100	2390.353019	20.002176
55.477096	2408.284630	20.007194
55.507335	2408.142676	20.012211
55.799850	2416.699938	20.017229
56.342696	2405.236206	20.022247
56.120029	2410.862059	20.027264
55.999089	2407.274646	20.032282
56.605116	2403.597519	20.037299
56.593299	2404.431483	20.042317
56.650907	2399.132060	20.047335
56.579945	2384.157248	20.052352
56.179410	2378.362301	20.057370
56.309780	2375.565831	20.062387
56.328081	2390.326320	20.067405
56.315665	2393.025796	20.072423
56.567934	2399.500303	20.077440
56.015099	2395.779939	20.082458
56.560911	2403.392707	20.087475
56.232010	2399.899701	20.092493
56.271078	2397.528651	20.097511
56.494026	2405.750214	20.102528
56.703037	2423.942144	20.107546
56.861781	2423.699303	20.112563
57.054818	2426.599687	20.117581
57.361677	2427.760624	20.122599
57.192426	2433.032715	20.127616
57.145691	2433.265771	20.132634
57.676762	2423.724913	20.137651
57.404561	2435.922221	20.142669
57.137566	2421.122083	20.147687
57.631020	2427.808495	20.152704
57.316607	2427.522238	20.157722
57.610621	2423.620574	20.162739
57.298949	2423.322838	20.167757
57.160940	2420.753253	20.172775
57.263411	2422.646213	20.177792
57.327301	2447.320772	20.182810
57.658696	2437.742223	20.187827
58.103339	2447.679387	20.192845
58.046350	2455.485673	20.197863
57.926300	2453.094993	20.202880
57.830209	2448.802628	20.207898
58.141571	2449.830137	20.212915
58.065749	2450.499539	20.217933
58.085284	2437.274658	20.222951
58.090760	2443.440186	20.227968
57.928415	2450.667895	20.232986
58.211132	2456.560180	20.238003
58.175336	2477.801627	20.243021
58.497394	2469.950264	20.248039
58.550920	2480.390654	20.253056
58.395323	2480.898505	20.258074
58.930371	2473.618458	20.263091
58.618715	2479.663078	20.268109
58.398631	2477.867781	20.273127
58.855212	2472.268159	20.278144
58.493788	2474.411063	20.283162
59.317419	2478.659466	20.288179
58.802540	2478.569129	20.293197
59.331593	2488.974985	20.298215
59.054205	2488.323899	20.303232
59.178161	2500.663694	20.308250
59.231633	2494.942075	20.313267
59.425227	2491.270084	20.318285
59.416480	2510.705044	20.323303
59.632219	2501.188592	20.328320
59.422768	2502.073518	20.333338
59.552215	2502.590299	20.338355
59.369581	2499.788343	20.343373
59.418403	2495.380145	20.348391
59.361697	2505.305388	20.353408
59.502168	2492.622194	20.358426
59.756146	2491.737517	20.363443
60.075424	2489.694307	20.368461
59.985870	2489.190751	20.373479
60.114179	2483.469297	20.378496
60.222908	2487.986914	20.383514
59.920692	2485.138297	20.388531
60.184821	2492.443973	20.393549
59.879722	2494.601142	20.398567
60.226461	2487.261830	20.403584
60.486434	2516.471800	20.408602
60.527182	2512.830324	20.413619
60.514808	2526.293627	20.418637
60.486019	2520.675437	20.423655
60.801296	2521.193225	20.428672
60.449993	2529.652816	20.433690
60.151286	2520.532493	20.438707
60.609667	2519.538250	20.443725
60.674839	2520.934646	20.448743
61.038784	2513.646007	20.453760
60.326093	2521.508935	20.458778
60.696718	2526.394472	20.463795
60.609527	2542.056530	20.468813
60.628949	2542.699869	20.473831
60.924553	2548.500673	20.478848
60.580094	2551.368751	20.483866
60.899351	2567.834189	20.488883
61.155219	2572.052561	20.493901
61.092434	2579.083855	20.498919
61.363063	2566.032105	20.503936
61.328370	2586.238827	20.508954
61.458591	2598.006766	20.513971
61.658605	2599.262250	20.518989
61.491972	2598.650628	20.524007
62.504588	2600.693939	20.529024
62.068080	2601.604794	20.534042
62.362197	2587.686485	20.539059
62.278303	2598.034434	20.544077
62.348094	2596.891373	20.549095
62.420840	2579.806175	20.554112
62.512457	2571.393033	20.559130
62.240440	2556.544780	20.564147
62.385439	2555.478203	20.569165
61.998084	2563.774505	20.574183
62.580623	2562.272992	20.579200
62.437044	2593.617191	20.584218
63.036763	2586.472020	20.589235
63.068643	2580.660647	20.594253
62.723784	2575.209932	20.599271
62.824542	2562.820695	20.604288
62.859942	2573.972065	20.609306
62.946738	2577.324799	20.614323
62.902031	2579.259561	20.619341
62.948568	2584.684038	20.624359
63.006778	2584.527197	20.629376
62.819857	2582.163754	20.634394
63.137552	2577.433277	20.639411
63.264769	2574.007347	20.644429
63.479636	2585.250164	20.649447
63.441435	2575.097888	20.654464
63.148144	2582.924611	20.659482
63.231754	2573.266682	20.664499
63.423288	2578.456813	20.669517
63.446423	2580.481093	20.674535
63.416960	2575.563026	20.679552
63.349990	2597.215740	20.684570
63.246428	2609.650916	20.689587
63.801816	2612.028102	20.694605
63.569000	2619.640453	20.699623
63.555444	2615.782771	20.704640
63.429038	2614.099060	20.709658
63.331394	2633.812346	20.714675
63.971170	2625.543125	20.719693
63.807927	2636.672826	20.724711
64.329344	2633.190820	20.729728
64.351006	2639.357279	20.734746
64.091568	2655.772128	20.739763
64.553860	2662.245700	20.744781
64.339377	2667.239939	20.749799
64.830971	2664.673951	20.754816
64.727452	2659.524846	20.759834
64.838002	2662.561430	20.764851
65.501043	2658.547196	20.769869
65.003179	2652.076555	20.774887
64.826702	2658.411784	20.779904
64.790988	2660.736026	20.784922
64.994631	2661.277098	20.789939
65.184776	2649.461942	20.794957
64.939372	2664.357859	20.799975
65.074247	2654.108260	20.804992
64.878802	2663.701525	20.810010
65.073570	2678.327443	20.815027
65.620339	2673.705725	20.820045
65.350915	2685.817722	20.825063
65.398382	2679.960806	20.830080
65.569223	2689.750313	20.835098
65.710388	2677.616488	20.840115
65.653176	2682.570421	20.845133
65.337607	2682.739491	20.850151
65.861010	2697.278132	20.855168
66.098703	2713.120239	20.860186
66.121054	2719.516942	20.865203
66.313883	2709.052547	20.870221
66.238111	2717.602676	20.875239
66.398933	2717.730765	20.880256
66.148144	2715.301139	20.885274
66.297800	2716.739026	20.890291
66.444650	2711.918787	20.895309
66.216386	2711.671358	20.900327
66.340029	2713.345470	20.905344
66.355893	2717.467542	20.910362
66.516931	2730.327762	20.915379
66.820573	2727.469754	20.920397
66.700475	2736.291841	20.925415
66.852120	2726.753225	20.930432
67.269948	2739.771968	20.935450
66.840817	2735.539203	20.940467
67.152968	2736.353204	20.945485
66.855419	2746.799754	20.950503
67.308424	2732.319449	20.955520
67.393302	2740.172777	20.960538
67.240869	2734.281736	20.965555
67.391345	2739.256292	20.970573
67.517418	2751.264026	20.975591
67.941069	2761.832869	20.980608
67.809882	2759.742828	20.985626
67.608379	2761.309161	20.990643
68.098967	2754.867129	20.995661
67.709265	2750.135654	21.000679
67.935268	2751.840399	21.005696
68.018809	2756.941839	21.010714
67.397163	2758.045290	21.015731
67.911631	2753.960049	21.020749
67.510517	2763.653307	21.025767
67.822095	2756.738634	21.030784
68.177096	2771.305725	21.035802
68.076662	2787.280484	21.040819
68.301373	2781.706296	21.045837
68.048907	2792.006399	21.050855
68.183298	2786.316898	21.055872
68.471344	2777.471371	21.060890
68.700644	2785.968081	21.065907
68.727215	2790.113591	21.070925
68.674785	2818.080697	21.075943
68.705642	2817.962260	21.080960
69.054452	2811.654404	21.085978
68.899847	2818.925094	21.090995
69.051187	2818.453150	21.096013
69.096788	2821.475755	21.101031
69.058580	2813.243911	21.106048
69.109992	2813.196472	21.111066
68.935085	2825.745651	21.116083
69.361038	2826.779735	21.121101
69.283570	2832.164273	21.126119
69.298173	2830.553961	21.131136
69.884053	2840.910452	21.136154
69.610272	2838.909456	21.141171
69.932420	2833.503713	21.146189
69.725582	2831.364420	21.151207
69.963333	2840.755084	21.156224
70.214221	2854.770231	21.161242
69.988759	2863.966614	21.166259
70.125371	2874.025328	21.171277
69.875860	2873.153829	21.176295
70.047408	2874.555414	21.181312
69.836548	2864.813163	21.186330
70.026815	2873.525869	21.191347
70.320963	2888.566598	21.196365
70.700353	2895.495019	21.201383
70.438951	2891.298513	21.206400
70.682976	2901.060241	21.211418
70.267019	2902.971304	21.216435
70.352494	2901.005483	21.221453
70.720272	2913.422415	21.226471
70.868804	2922.303906	21.231488
71.229498	2924.115428	21.236506
71.391339	2923.342504	21.241523
71.517755	2924.324794	21.246541
71.472790	2928.877925	21.251559
71.532405	2927.870398	21.256576
71.658139	2923.195344	21.261594
71.726246	2921.745039	21.266611
71.489240	2920.398201	21.271629
71.577210	2918.155961	21.276647
71.218983	2915.093722	21.281664
71.706951	2920.600476	21.286682
71.713565	2921.856630	21.291699
71.957905	2916.809481	21.296717
71.823730	2928.798788	21.301735
71.965840	2941.676897	21.306752
72.003580	2942.597936	21.311770
71.843430	2942.340364	21.316787
72.212665	2954.466910	21.321805
72.144428	2955.736687	21.326823
72.340229	2942.373416	21.331840
72.206520	2944.416722	21.336858
72.410927	2940.310911	21.341875
73.013753	2935.838474	21.346893
73.028712	2930.503829	21.351911
73.251188	2932.785991	21.356928
73.718090	2917.342513	21.361946
73.648153	2919.595704	21.366963
73.616577	2915.646842	21.371981
73.601350	2911.453909	21.376999
73.376051	2904.150804	21.382016
73.738155	2881.856227	21.387034
73.531483	2887.739846	21.392051
73.803548	2873.180025	21.397069
73.730817	2875.205708	21.402087
73.480803	2877.957354	21.407104
73.966622	2870.165195	21.412122
73.960694	2875.453995	21.417139
73.852316	2881.799258	21.422157
73.610933	2874.976036	21.427175
73.513548	2877.726334	21.432192
73.785567	2870.880787	21.437210
73.243905	2885.183590	21.442227
73.803354	2901.207078	21.447245
73.862674	2909.886052	21.452263
73.589824	2909.012130	21.457280
74.053213	2906.537805	21.462298
74.259365	2931.642669	21.467315
74.236787	2930.625178	21.472333
74.088770	2931.730247	21.477351
74.138386	2927.080048	21.482368
74.715961	2940.809075	21.487386
74.558997	2965.343983	21.492403
74.958547	2962.763715	21.497421
74.528709	2962.439538	21.502439
74.631139	2960.906354	21.507456
74.852575	2954.892462	21.512474
74.853603	2961.108938	21.517491
74.871632	2968.961679	21.522509
75.427942	2988.475388	21.527527
74.971695	2996.627450	21.532544
75.398345	2991.212161	21.537562
75.532855	2992.995923	21.542579
75.817266	2993.181434	21.547597
75.818028	2993.112095	21.552615
75.589085	2986.866718	21.557632
76.102414	2985.501876	21.562650
75.651202	2985.384414	21.567667
76.061008	2985.426637	21.572685
76.127832	2976.364989	21.577703
76.133384	2988.469320	21.582720
76.391595	2994.586765	21.587738
76.400367	2998.945540	21.592755
76.186486	3007.465625	21.597773
76.117064	3004.475853	21.602791
76.196810	3011.194264	21.607808
76.607790	3003.724736	21.612826
76.496559	3013.436512	21.617843
76.712435	3008.204682	21.622861
76.917835	2995.594547	21.627879
77.091343	3001.998926	21.632896
77.014639	2999.531661	21.637914
77.000970	3000.941203	21.642931
76.919052	3009.240526	21.647949
77.058206	3026.923475	21.652967
76.877028	3038.132432	21.657984
77.051103	3034.441115	21.663002
77.103693	3034.842332	21.668019
76.892490	3037.709611	21.673037
77.346667	3037.420815	21.678055
77.415573	3056.423441	21.683072
77.590328	3052.020144	21.688090
77.714461	3055.831378	21.693107
77.716068	3049.385838	21.698125
78.127264	3037.454119	21.703143
78.128752	3051.574675	21.708160
78.512663	3040.530231	21.713178
78.277500	3043.704272	21.718195
78.622575	3042.128787	21.723213
78.831475	3036.322474	21.728231
78.711708	3039.533639	21.733248
78.633030	3034.640142	21.738266
78.806198	3034.236618	21.743283
78.698099	3029.642521	21.748301
78.748168	3035.456754	21.753319
78.721349	3039.908075	21.758336
78.485736	3033.886638	21.763354
78.738161	3037.629299	21.768371
78.596492	3046.629567	21.773389
78.836453	3050.144365	21.778407
78.952570	3074.701783	21.783424
78.866088	3082.589668	21.788442
78.947917	3081.055959	21.793459
78.873102	3084.963260	21.798477
78.974412	3092.456921	21.803495
78.919125	3109.778153	21.808512
79.214566	3101.224546	21.813530
79.381874	3117.026790	21.818547
79.597061	3128.773531	21.823565
79.650328	3124.009271	21.828583
79.482900	3136.678332	21.833600
79.712619	3131.822537	21.838618
80.013753	3137.578546	21.843635
79.882967	3148.882365	21.848653
80.376062	3148.571351	21.853671
80.548333	3156.219011	21.858688
80.759853	3148.677043	21.863706
80.979584	3148.443744	21.868723
80.880265	3147.747285	21.873741
81.441786	3143.150149	21.878759
81.179326	3152.635549	21.883776
81.131919	3148.142364	21.888794
81.258250	3143.849459	21.893811
81.455019	3152.606521	21.898829
81.432928	3135.238815	21.903847
81.162946	3121.718527	21.908864
81.373496	3122.974666	21.913882
81.075323	3116.171406	21.918899
80.945298	3142.886144	21.923917
81.121568	3141.608803	21.928935
81.227189	3140.979868	21.933952
80.901825	3145.115057	21.938970
81.551519	3163.011765	21.943987
81.573286	3183.039785	21.949005
81.344350	3173.586981	21.954023
81.354360	3191.359301	21.959040
81.886888	3203.299837	21.964058
82.062072	3206.217511	21.969075
82.161457	3204.845453	21.974093
82.361876	3200.428400	21.979111
82.119054	3209.145547	21.984128
82.327598	3207.389963	21.989146
83.007316	3216.757017	21.994163
82.785820	3223.741348	21.999181
82.747896	3219.213887	22.004199
83.021131	3229.023728	22.009216
83.046184	3234.836287	22.014234
83.036311	3219.343782	22.019251
83.126641	3225.638837	22.024269
83.510195	3219.295515	22.029287
83.469066	3212.933787	22.034304
83.357313	3204.634424	22.039322
83.530382	3207.253999	22.044339
83.173142	3210.622784	22.049357
83.617660	3209.703648	22.054375
83.447831	3203.068800	22.059392
83.664111	3216.672668	22.064410
83.585601	3211.520010	22.069427
83.430881	3214.486211	22.074445
83.702077	3204.134063	22.079463
83.892447	3223.865196	22.084480
83.742160	3242.093777	22.089498
84.065879	3237.852696	22.094515
83.798972	3242.602659	22.099533
84.340694	3244.445559	22.104551
84.283481	3246.844727	22.109568
84.198165	3268.888463	22.114586
84.695173	3267.126276	22.119603
84.511162	3269.873320	22.124621
84.747381	3269.832573	22.129639
84.667176	3275.850057	22.134656
84.775041	3270.869574	22.139674
84.792997	3276.922325	22.144691
85.069921	3291.343024	22.149709
85.549728	3306.089894	22.154727
85.305598	3298.624758	22.159744
85.276448	3307.880123	22.164762
85.580164	3293.812335	22.169779
85.278609	3307.731887	22.174797
85.418323	3293.996106	22.179815
85.348608	3299.090514	22.184832
85.403539	3316.654706	22.189850
85.703680	3319.791420	22.194867
85.844484	3333.394545	22.199885
85.888601	3324.339226	22.204903
85.900823	3324.106943	22.209920
85.885063	3349.072178	22.214938
86.544655	3350.727377	22.219955
86.528869	3356.618034	22.224973
86.946473	3344.885037	22.229991
86.832944	3349.784755	22.235008
86.599240	3354.870997	22.240026
87.024736	3339.462729	22.245043
87.089934	3356.126357	22.250061
87.062637	3345.052784	22.255079
87.249944	3343.308984	22.260096
87.150627	3341.328144	22.265114
87.821616	3336.236733	22.270131
87.335378	3331.163607	22.275149
87.593825	3335.358925	22.280167
87.631205	3329.820794	22.285184
87.755339	3330.456214	22.290202
87.936918	3336.437698	22.295219
88.027283	3333.126792	22.300237
88.148396	3331.331390	22.305255
87.943832	3332.720318	22.310272
87.755113	3333.994398	22.315290
87.747968	3328.703059	22.320307
87.688192	3336.896504	22.325325
87.940761	3347.131154	22.330343
88.268010	3349.020735	22.335360
88.013692	3361.127199	22.340378
88.530852	3356.245221	22.345395
88.076755	3368.730593	22.350413
88.263023	3374.933773	22.355431
88.616254	3381.739191	22.360448
88.216245	3388.410315	22.365466
88.668290	3379.291898	22.370483
88.486187	3396.344338	22.375501
88.640179	3401.437826	22.380519
88.914347	3416.220157	22.385536
88.410588	3420.486648	22.390554
88.932622	3431.159296	22.395571
88.716775	3447.093667	22.400589
89.096222	3454.317636	22.405607
89.510153	3449.752815	22.410624
89.451022	3464.294095	22.415642
89.824916	3472.926223	22.420659
89.641622	3480.948519	22.425677
89.595614	3479.110393	22.430695
89.837073	3479.104999	22.435712
89.940429	3482.873330	22.440730
90.327996	3495.319727	22.445747
90.226084	3506.187465	22.450765
90.456914	3506.042484	22.455783
90.789153	3504.520669	22.460800
91.039002	3500.407949	22.465818
91.359796	3492.655510	22.470835
91.284343	3501.979321	22.475853
91.445419	3484.874911	22.480871
91.517653	3480.686584	22.485888
91.270792	3471.291701	22.490906
91.497861	3458.050759	22.495923
90.920688	3464.270995	22.500941
91.095029	3476.125190	22.505959
91.509284	3478.084982	22.510976
91.169871	3475.760916	22.515994
91.118251	3477.964682	22.521011
91.318828	3489.571984	22.526029
91.465356	3508.207500	22.531047
91.913551	3504.299636	22.536064
91.638467	3518.553199	22.541082
91.980087	3515.882855	22.546099
91.863293	3524.450479	22.551117
92.021710	3535.904568	22.556135
92.395646	3540.021294	22.561152
92.347137	3542.926988	22.566170
92.570053	3544.581937	22.571187
92.585735	3548.666066	22.576205
92.348489	3541.904467	22.581223
92.553131	3554.682131	22.586240
92.643861	3567.069636	22.591258
93.396169	3563.362427	22.596275
93.665027	3567.089099	22.601293
93.390082	3570.612805	22.606311
93.314547	3567.000645	22.611328
93.364271	3567.929180	22.616346
93.479626	3564.350266	22.621363
93.682279	3570.904383	22.626381
93.663979	3567.541007	22.631399
93.743834	3562.957254	22.636416
93.543782	3563.234311	22.641434
93.648393	3586.129702	22.646451
93.855698	3596.147998	22.651469
94.022665	3600.066826	22.656487
94.091173	3590.376129	22.661504
93.995790	3606.320961	22.666522
93.845739	3617.490509	22.671539
94.173644	3636.563017	22.676557
94.184586	3638.591823	22.681575
94.353047	3633.556269	22.686592
94.479474	3647.610139	22.691610
94.574196	3665.101960	22.696627
94.792169	3660.232205	22.701645
94.883016	3657.472395	22.706663
95.051981	3664.418020	22.711680
94.989009	3656.742270	22.716698
95.046216	3668.633796	22.721715
95.762046	3677.204095	22.726733
95.749592	3685.372534	22.731751
95.627725	3683.143795	22.736768
95.697348	3683.550860	22.741786
96.102218	3680.634518	22.746803
96.227346	3687.100375	22.751821
96.095766	3681.111009	22.756839
96.247990	3675.514296	22.761856
96.361471	3673.503957	22.766874
96.294204	3671.697297	22.771891
96.483369	3673.844539	22.776909
95.868001	3678.971473	22.781927
96.073726	3681.831400	22.786944
96.244342	3696.472132	22.791962
96.848050	3690.157004	22.796979
97.549150	3696.209001	22.801997
97.049328	3706.576797	22.807015
97.402192	3697.719195	22.812032
97.095685	3700.632356	22.817050
97.435495	3699.447887	22.822067
97.738733	3694.100906	22.827085
97.455174	3698.242678	22.832103
97.404413	3691.497666	22.837120
97.283446	3709.566783	22.842138
97.290795	3714.809561	22.847155
97.541412	3718.786180	22.852173
97.705000	3722.732770	22.857191
97.984696	3721.517339	22.862208
98.085030	3720.313603	22.867226
98.459777	3741.701956	22.872243
98.356407	3743.303657	22.877261
98.548748	3755.614970	22.882279
98.948825	3742.447806	22.887296
98.909352	3745.357941	22.892314
98.794135	3741.334570	22.897331
99.065803	3740.816223	22.902349
99.094268	3738.914110	22.907367
99.322849	3732.636498	22.912384
99.229168	3736.123818	22.917402
99.014372	3737.703479	22.922419
99.255240	3739.569665	22.927437
99.311997	3747.685685	22.932455
99.196877	3756.894966	22.937472
99.006795	3764.355869	22.942490
99.551631	3770.160210	22.947507
99.517109	3765.568237	22.952525
99.630763	3779.229813	22.957543
99.887179	3787.804859	22.962560
99.643334	3791.662463	22.967578
99.673205	3795.276131	22.972595
100.077428	3808.326385	22.977613
100.210499	3820.603105	22.982631
100.415672	3815.387749	22.987648
100.400788	3814.812283	22.992666
100.548667	3821.219290	22.997683
100.970340	3823.763401	23.002701
100.788982	3828.198497	23.007719
101.386199	3835.247068	23.012736
101.110348	3838.214615	23.017754
101.116078	3845.272891	23.022771
101.588822	3836.387021	23.027789
101.602230	3837.546832	23.032807
101.718892	3836.456137	23.037824
101.758418	3832.132976	23.042842
101.750887	3840.486921	23.047859
101.873764	3825.521430	23.052877
101.933450	3842.899574	23.057895
102.206363	3835.406137	23.062912
101.911814	3834.841708	23.067930
102.164495	3834.426920	23.072947
102.352597	3839.151059	23.077965
101.719866	3851.120366	23.082983
102.188141	3865.573192	23.088000
102.261960	3866.955279	23.093018
102.214200	3864.898079	23.098035
102.592111	3876.408474	23.103053
102.244704	3897.630004	23.108071
102.806082	3894.953003	23.113088
103.081811	3893.070812	23.118106
102.531165	3908.099354	23.123123
103.279027	3929.993749	23.128141
102.970670	3932.826540	23.133159
103.203121	3930.888142	23.138176
103.309919	3937.416999	23.143194
103.609487	3954.533327	23.148211
104.309665	3955.334891	23.153229
103.662899	3955.106585	23.158247
104.002471	3953.346078	23.163264
104.099447	3954.049826	23.168282
103.863092	3970.125948	23.173299
104.479093	3975.174741	23.178317
104.352255	3995.442305	23.183335
104.201296	3983.760005	23.188352
104.658828	3982.006274	23.193370
104.576153	3992.707744	23.198387
104.699255	3994.926253	23.203405
105.017105	4010.788256	23.208423
105.398474	4007.830085	23.213440
105.442645	4005.708764	23.218458
105.376663	4011.188661	23.223475
105.669271	4010.819603	23.228493
105.644996	4006.948396	23.233511
105.745821	4011.380750	23.238528
105.663125	4004.271569	23.243546
105.602780	4009.174467	23.248563
105.933609	4026.721564	23.253581
105.689780	4027.673709	23.258599
106.140068	4031.485714	23.263616
106.042642	4029.489903	23.268634
106.021378	4036.349180	23.273651
106.697832	4042.208534	23.278669
107.302394	4046.126420	23.283687
107.544209	4034.470162	23.288704
107.822973	4010.478544	23.293722
107.370167	4014.557172	23.298739
107.637190	4001.026418	23.303757
107.313075	4006.376746	23.308775
107.353463	4013.173398	23.313792
107.991984	4007.060263	23.318810
107.667158	4008.070361	23.323827
107.953557	3998.953914	23.328845
107.590102	4006.243323	23.333863
107.785212	4005.455763	23.338880
108.003461	3996.690059	23.343898
107.814991	4003.606246	23.348915
107.903356	4015.130211	23.353933
107.868780	4020.812794	23.358951
108.118154	4022.236203	23.363968
108.293859	4024.726328	23.368986
108.015802	4041.532387	23.374003
108.087735	4044.500453	23.379021
108.709994	4055.702228	23.384039
108.649133	4060.112246	23.389056
108.351317	4061.613597	23.394074
108.681622	4071.679879	23.399091
108.641064	4084.833022	23.404109
108.686305	4093.198414	23.409127
108.775532	4105.328686	23.414144
109.278548	4111.143256	23.419162
109.087688	4128.686205	23.424179
109.590545	4128.052252	23.429197
109.179830	4130.795773	23.434215
109.371538	4136.121064	23.439232
109.729121	4159.978155	23.444250
109.939065	4159.019989	23.449267
110.179023	4160.378824	23.454285
110.044300	4168.054767	23.459303
110.251473	4180.217866	23.464320
110.655597	4181.032024	23.469338
110.435594	4185.700053	23.474355
110.621680	4186.483506	23.479373
110.700313	4184.718298	23.484391
110.962412	4197.454652	23.489408
110.951312	4202.931401	23.494426
111.155163	4214.076425	23.499443
111.145577	4202.922125	23.504461
111.226185	4206.449493	23.509479
111.294165	4217.639936	23.514496
111.397652	4229.195408	23.519514
111.374193	4237.148608	23.524531
111.675663	4239.299711	23.529549
111.978918	4245.436153	23.534567
111.899174	4259.656351	23.539584
112.452001	4257.877698	23.544602
112.438087	4261.245956	23.549619
112.884489	4260.459940	23.554637
113.019758	4260.819492	23.559655
112.963365	4256.226679	23.564672
113.058414	4249.981684	23.569690
112.735228	4259.643220	23.574707
113.076931	4257.869727	23.579725
112.913811	4262.369246	23.584743
112.956284	4274.612159	23.589760
113.332303	4275.008881	23.594778
113.236891	4286.840793	23.599795
113.079431	4280.217211	23.604813
113.545027	4297.185833	23.609831
113.759139	4299.798774	23.614848
113.985178	4305.366881	23.619866
114.088994	4300.814371	23.624883
114.227093	4299.756701	23.629901
114.279041	4297.006787	23.634919
114.389505	4316.472615	23.639936
114.676800	4315.574432	23.644954
114.891025	4327.575426	23.649971
114.881990	4327.057246	23.654989
115.168337	4315.171692	23.660007
114.713232	4319.517356	23.665024
115.223472	4322.696934	23.670042
115.154745	4321.816175	23.675059
115.252624	4324.985527	23.680077
115.368198	4334.479694	23.685095
115.154871	4356.741538	23.690112
115.366191	4349.250218	23.695130
115.358027	4357.288352	23.700147
115.517477	4363.388887	23.705165
115.862456	4375.457967	23.710183
116.056152	4385.749548	23.715200
116.594451	4373.822081	23.720218
116.574171	4376.641729	23.725235
116.733063	4374.349696	23.730253
116.940612	4369.388527	23.735271
116.659747	4377.364098	23.740288
116.860448	4378.635761	23.745306
116.899852	4374.182924	23.750323
116.598919	4368.914065	23.755341
116.940935	4389.299137	23.760359
116.941953	4395.533116	23.765376
117.183984	4394.721203	23.770394
117.472670	4397.459586	23.775411
117.386004	4392.850499	23.780429
117.191453	4406.414997	23.785447
117.418561	4423.117040	23.790464
117.837608	4420.465182	23.795482
117.761362	4434.478624	23.800499
118.136177	4440.858412	23.805517
118.636021	4449.609942	23.810535
118.636482	4446.173169	23.815552
118.522370	4440.134538	23.820570
118.550282	4444.172373	23.825587
118.533874	4446.221973	23.830605
118.768638	4440.493143	23.835623
118.972797	4466.161134	23.840640
119.407790	4469.624158	23.845658
119.377677	4473.639354	23.850675
119.615789	4471.123872	23.855693
119.755090	4471.119708	23.860711
119.390937	4483.887912	23.865728
119.911938	4465.367675	23.870746
119.654855	4479.680544	23.875763
119.845966	4492.937680	23.880781
120.012397	4493.567697	23.885799
120.241047	4498.060458	23.890816
120.827969	4487.996790	23.895834
120.806039	4493.315572	23.900851
121.148236	4482.533395	23.905869
121.166940	4480.131549	23.910887
121.343249	4483.639139	23.915904
121.486721	4481.459120	23.920922
121.269326	4480.241580	23.925939
121.230247	4482.547750	23.930957
121.585923	4479.383493	23.935975
121.421970	4476.211082	23.940992
121.831270	4473.048152	23.946010
121.637096	4480.936128	23.951027
121.745866	4505.845105	23.956045
122.003969	4506.820578	23.961063
121.539064	4508.461959	23.966080
121.538213	4504.463880	23.971098
121.886582	4529.578001	23.976115
122.033822	4545.586242	23.981133
122.277626	4543.054052	23.986151
122.070495	4558.147013	23.991168
122.659756	4569.402290	23.996186
122.917108	4571.516669	24.001203
122.785684	4569.081481	24.006221
123.085584	4569.818477	24.011239
123.170716	4592.627223	24.016256
123.145632	4593.800968	24.021274
123.275161	4590.126931	24.026291
123.274364	4594.649185	24.031309
123.763683	4612.681322	24.036327
123.579667	4629.708642	24.041344
123.834465	4628.047992	24.046362
123.662722	4628.391632	24.051379
123.773679	4636.288045	24.056397
124.307904	4646.503522	24.061415
124.221916	4657.431625	24.066432
124.201958	4659.441679	24.071450
124.717052	4661.046229	24.076467
124.919864	4663.276002	24.081485
124.737282	4678.449266	24.086503
124.990887	4683.696336	24.091520
125.170332	4684.370663	24.096538
125.455926	4685.121855	24.101555
125.257933	4691.142522	24.106573
125.358495	4687.707175	24.111591
125.525225	4709.240102	24.116608
125.418591	4717.991759	24.121626
125.722013	4700.972234	24.126643
125.742579	4721.559213	24.131661
126.087315	4738.490910	24.136679
125.936500	4751.093932	24.141696
126.055602	4736.455033	24.146714
126.649588	4745.989656	24.151731
126.865897	4765.691255	24.156749
127.445462	4759.799482	24.161767
127.260495	4755.320818	24.166784
127.247165	4757.165973	24.171802
127.497783	4751.969140	24.176819
127.154184	4757.468259	24.181837
127.600968	4744.372829	24.186855
127.645424	4753.298648	24.191872
127.692105	4752.799546	24.196890
128.026519	4771.355337	24.201907
127.671088	4790.956665	24.206925
128.055115	4791.696231	24.211943
128.233319	4789.157578	24.216960
127.991236	4789.644429	24.221978
128.080625	4802.822651	24.226995
128.210838	4817.234489	24.232013
128.564130	4821.210476	24.237031
128.315460	4829.128158	24.242048
128.429472	4858.529789	24.247066
128.917951	4856.827134	24.252083
128.888419	4872.704423	24.257101
129.041695	4879.578774	24.262119
129.018173	4880.296288	24.267136
129.583434	4894.495719	24.272154
129.966469	4913.316091	24.277171
129.747118	4919.505779	24.282189
130.073322	4915.139015	24.287207
130.225929	4906.457744	24.292224
130.119851	4929.338918	24.297242
130.522904	4937.587022	24.302259
130.522542	4950.373116	24.307277
130.608541	4938.736177	24.312295
130.398903	4949.645653	24.317312
130.643061	4962.209199	24.322330
131.110727	4966.560782	24.327347
131.107501	4970.939426	24.332365
131.272556	4968.891214	24.337383
131.485649	4987.739127	24.342400
131.491750	4996.469843	24.347418
131.762159	4994.753796	24.352435
131.609341	4995.088784	24.357453
131.689456	5001.928092	24.362471
132.010075	5022.279740	24.367488
132.228501	5031.774565	24.372506
132.475613	5028.395911	24.377523
132.551759	5032.327437	24.382541
132.498601	5028.237897	24.387559
132.833787	5036.081500	24.392576
133.021688	5042.118506	24.397594
133.642668	5036.602503	24.402611
133.768305	5023.861057	24.407629
133.740165	5030.300173	24.412647
133.679908	5022.627634	24.417664
133.217355	5035.633149	24.422682
133.723429	5028.960418	24.427699
133.712100	5027.136036	24.432717
133.441617	5023.481116	24.437735
133.697152	5039.527781	24.442752
133.786223	5058.608242	24.447770
133.731042	5067.143627	24.452787
133.947887	5082.224915	24.457805
134.076150	5088.446688	24.462823
134.472349	5102.631873	24.467840
134.697521	5115.931131	24.472858
135.083447	5113.501245	24.477875
135.213042	5114.838340	24.482893
135.930302	5103.981602	24.487911
136.063567	5097.847268	24.492928
136.010500	5098.399589	24.497946
136.273288	5095.813753	24.502963
136.219208	5096.626925	24.507981
136.538032	5089.439504	24.512999
136.644078	5093.956749	24.518016
136.622953	5090.722675	24.523034
136.966468	5094.243572	24.528051
136.570147	5088.140540	24.533069
136.854233	5100.766868	24.538087
137.045993	5113.073046	24.543104
136.855678	5118.592497	24.548122
136.890121	5115.608293	24.553139
137.129521	5122.332190	24.558157
137.311345	5125.793330	24.563175
137.327276	5145.760247	24.568192
137.277346	5154.305045	24.573210
137.565783	5148.867891	24.578227
137.833745	5164.896081	24.583245
137.679408	5182.501077	24.588263
138.178038	5187.127952	24.593280
137.885799	5197.307073	24.598298
138.265281	5206.882351	24.603315
138.201793	5225.452819	24.608333
138.502259	5215.813540	24.613351
138.353474	5231.697618	24.618368
138.519575	5249.744822	24.623386
138.824280	5255.990108	24.628403
138.976195	5275.455750	24.633421
138.846890	5286.041805	24.638439
138.873381	5292.557008	24.643456
139.058086	5315.238420	24.648474
139.499729	5308.386474	24.653491
139.812208	5332.492663	24.658509
140.255790	5342.462972	24.663527
140.320370	5345.759351	24.668544
140.475190	5348.398074	24.673562
140.530580	5343.313035	24.678579
140.725977	5360.312748	24.683597
141.007682	5371.140080	24.688615
141.130868	5371.041724	24.693632
140.904614	5376.516043	24.698650
141.465272	5366.523918	24.703667
141.327238	5378.223543	24.708685
141.567914	5382.705110	24.713703
142.153915	5396.776328	24.718720
142.056429	5393.244576	24.723738
142.222947	5383.896804	24.728755
142.256339	5386.650221	24.733773
142.284857	5392.644540	24.738791
142.300445	5384.133841	24.743808
142.522200	5391.792489	24.748826
142.608948	5398.148083	24.753843
142.804146	5405.256697	24.758861
142.893742	5416.858669	24.763879
143.387490	5416.160033	24.768896
142.761383	5415.626219	24.773914
143.317346	5425.821269	24.778931
143.141887	5436.864015	24.783949
143.853850	5444.282928	24.788967
143.911630	5445.456355	24.793984
143.989186	5439.290980	24.799002
143.995745	5448.284134	24.804019
144.315146	5448.212241	24.809037
144.184033	5458.027671	24.814055
144.428299	5457.394905	24.819072
144.338800	5477.769614	24.824090
144.550458	5470.457277	24.829107
144.701571	5496.882393	24.834125
144.782361	5492.192389	24.839143
145.259681	5498.228733	24.844160
145.026797	5521.387014	24.849178
145.377921	5522.648742	24.854195
145.529082	5534.024772	24.859213
145.782775	5543.011567	24.864231
145.976373	5546.813444	24.869248
145.863549	5550.266146	24.874266
146.401423	5542.953124	24.879283
146.500915	5551.672566	24.884301
146.676244	5569.453975	24.889319
146.628385	5572.624957	24.894336
146.621480	5585.129123	24.899354
146.670442	5582.138480	24.904371
147.104153	5587.972608	24.909389
147.323214	5599.404347	24.914407
147.577452	5595.142292	24.919424
147.976334	5615.191085	24.924442
147.916968	5603.929862	24.929459
148.123433	5600.987077	24.934477
148.038920	5630.058486	24.939495
148.428720	5619.891397	24.944512
148.143344	5623.150687	24.949530
148.476697	5613.743554	24.954547
148.586912	5625.658864	24.959565
148.813641	5648.738595	24.964583
148.898433	5652.646000	24.969600
148.837824	5661.433062	24.974618
148.973698	5664.107278	24.979635
148.839488	5672.872710	24.984653
148.886658	5690.443211	24.989671
149.251422	5699.093453	24.994688
149.685447	5715.615996	24.999706
149.728823	5719.815409	25.004723
150.092707	5727.252918	25.009741
149.908288	5749.947462	25.014759
150.186123	5745.949228	25.019776
150.372018	5767.166955	25.024794
150.237604	5776.238853	25.029811
150.247309	5782.697190	25.034829
150.865384	5795.701757	25.039847
151.183210	5802.497976	25.044864
151.677795	5802.162269	25.049882
151.511576	5808.432473	25.054899
151.726662	5804.863653	25.059917
151.671799	5812.908715	25.064935
152.213190	5822.603171	25.069952
152.288869	5820.243636	25.074970
152.629789	5826.791084	25.079987
152.422514	5819.100056	25.085005
152.626381	5828.070092	25.090023
152.948079	5818.807329	25.095040
152.845603	5822.508040	25.100058
152.843764	5825.424120	25.105075
153.093143	5832.041913	25.110093
152.857879	5855.922519	25.115111
153.368936	5850.396153	25.120128
153.439361	5865.877421	25.125146
153.633635	5874.404870	25.130163
154.025604	5874.357937	25.135181
154.098064	5889.624662	25.140199
154.475723	5880.028861	25.145216
154.369780	5886.432423	25.150234
154.382451	5884.254258	25.155251
154.645925	5910.948873	25.160269
154.402338	5908.557315	25.165287
154.650147	5905.767488	25.170304
154.617871	5921.017780	25.175322
154.643019	5927.660273	25.180339
155.200906	5936.595959	25.185357
155.147943	5956.739960	25.190375
155.252460	5971.558803	25.195392
155.668346	5981.171037	25.200410
156.292407	5993.422610	25.205427
156.176515	5997.689517	25.210445
156.228144	5998.947495	25.215463
156.740941	5993.987080	25.220480
156.839919	6008.595013	25.225498
156.977413	6019.661772	25.230515
157.516543	6007.949538	25.235533
157.329225	6020.047692	25.240551
157.270970	6020.481190	25.245568
157.525141	6009.332189	25.250586
157.680874	6037.383066	25.255603
158.011861	6047.204774	25.260621
158.028688	6054.344897	25.265639
158.138687	6044.926579	25.270656
158.332565	6055.974543	25.275674
158.135442	6070.178859	25.280691
158.479694	6066.278200	25.285709
158.392889	6086.704440	25.290727
158.643870	6099.831693	25.295744
158.778653	6107.996614	25.300762
158.909285	6108.109673	25.305779
159.307488	6129.549371	25.310797
158.875011	6143.725913	25.315815
159.493204	6145.128406	25.320832
159.443157	6162.445435	25.325850
159.420084	6172.676543	25.330867
159.934973	6176.670134	25.335885
161.348597	6163.549927	25.340903
162.858716	6132.043377	25.345920
163.457643	6102.104424	25.350938
163.639491	6075.297063	25.355955
163.726814	6048.292012	25.360973
163.035163	6023.931279	25.365991
163.468000	5995.140892	25.371008
163.494854	5975.299063	25.376026
162.942312	5952.744934	25.381043
163.006201	5939.891718	25.386061
162.864377	5924.482267	25.391079
162.293732	5899.402227	25.396096
162.575403	5922.129836	25.401114
162.416109	5920.123585	25.406131
162.703032	5929.795810	25.411149
162.323634	5940.982271	25.416167
162.509579	5938.880058	25.421184
163.034482	5959.266712	25.426202
162.873360	5972.459974	25.431219
162.898315	5964.098626	25.436237
163.225250	5986.769188	25.441255
163.035823	6003.965072	25.446272
163.697909	6014.737520	25.451290
163.195055	6021.113363	25.456307
163.675404	6036.664517	25.461325
163.508573	6055.955682	25.466343
163.861571	6078.021097	25.471360
163.831815	6089.770203	25.476378
163.761259	6115.850411	25.481395
164.511632	6132.773707	25.486413
164.671298	6144.676467	25.491431
164.414353	6163.457398	25.496448
164.413598	6173.335885	25.501466
164.691386	6206.733599	25.506483
164.868556	6219.206105	25.511501
165.055753	6245.488647	25.516519
165.608020	6265.861698	25.521536
165.855681	6276.386565	25.526554
165.829019	6292.371921	25.531571
166.350265	6295.052309	25.536589
166.130512	6304.010307	25.541607
166.937469	6330.192370	25.546624
167.003070	6341.200415	25.551642
166.638090	6347.736995	25.556659
167.312915	6362.497673	25.561677
167.386319	6365.826667	25.566695
167.567313	6376.016123	25.571712
168.109859	6388.820288	25.576730
167.780707	6400.985619	25.581747
168.328003	6399.582575	25.586765
168.347273	6414.816115	25.591783
168.784475	6420.229383	25.596800
169.262723	6418.272294	25.601818
168.896334	6420.560671	25.606835
169.882069	6430.544769	25.611853
170.002618	6440.530075	25.616871
170.059001	6451.483807	25.621888
170.438407	6445.988566	25.626906
170.097248	6436.181067	25.631923
170.325454	6441.135226	25.636941
170.344686	6436.029065	25.641959
170.335670	6442.806622	25.646976
170.526574	6443.723291	25.651994
170.612081	6466.644167	25.657011
170.975980	6468.392185	25.662029
170.936280	6478.315140	25.667047
171.104047	6484.327692	25.672064
171.261536	6495.077198	25.677082
171.120886	6508.155660	25.682100
171.521861	6513.967221	25.687117
171.687188	6531.646621	25.692135
171.742575	6542.835297	25.697152
172.136207	6555.950254	25.702170
172.484340	6567.885028	25.707188
172.205666	6570.169090	25.712205
172.416272	6584.264372	25.717223
172.259332	6598.438067	25.722240
172.367227	6610.388374	25.727258
172.547844	6624.981736	25.732276
172.854774	6644.526491	25.737293
173.040987	6657.653156	25.742311
173.121334	6682.340303	25.747328
173.949034	6691.489149	25.752346
173.643303	6704.168300	25.757364
174.279949	6703.192253	25.762381
174.503432	6721.048873	25.767399
174.615351	6712.879830	25.772416
174.955202	6714.104151	25.777434
175.517295	6735.258307	25.782452
175.505096	6751.640271	25.787469
175.427113	6750.720741	25.792487
176.061440	6745.939179	25.797504
176.466648	6742.804845	25.802522
175.740248	6757.624655	25.807540
176.016865	6753.305014	25.812557
176.212516	6756.600389	25.817575
176.090035	6759.992733	25.822592
176.349434	6769.969353	25.827610
176.642571	6782.693197	25.832628
176.877032	6797.946484	25.837645
176.943486	6808.624688	25.842663
177.362953	6801.420563	25.847680
177.124417	6812.360537	25.852698
177.167288	6834.866851	25.857716
177.479013	6837.598690	25.862733
177.724160	6858.016450	25.867751
177.628033	6870.879872	25.872768
177.644943	6880.449469	25.877786
177.925605	6895.823560	25.882804
178.255179	6922.828687	25.887821
178.542669	6934.554060	25.892839
178.721539	6948.298132	25.897856
178.902923	6960.466488	25.902874
178.955226	6971.869433	25.907892
179.464482	6988.954228	25.912909
179.689728	6998.731089	25.917927
179.513433	7008.433685	25.922944
180.409747	7022.680073	25.927962
180.245125	7033.819797	25.932980
180.085267	7038.379420	25.937997
180.649862	7042.701308	25.943015
180.744334	7051.091596	25.948032
181.194288	7046.796636	25.953050
181.262240	7067.001509	25.958068
181.582047	7079.810954	25.963085
181.901355	7074.253020	25.968103
181.639335	7085.386121	25.973120
182.322538	7094.877430	25.978138
182.510750	7100.212582	25.983156
182.441273	7105.843392	25.988173
182.949320	7105.013143	25.993191
182.911351	7100.197468	25.998208
183.396256	7118.816090	26.003226
183.579098	7127.506800	26.008244
183.649376	7128.571155	26.013261
183.618527	7129.860257	26.018279
183.443572	7132.746267	26.023296
183.563780	7149.957318	26.028314
184.117676	7159.032998	26.033332
184.080539	7162.518369	26.038349
184.173796	7172.434631	26.043367
184.129073	7188.052112	26.048384
184.408421	7189.497620	26.053402
184.654794	7203.611928	26.058420
184.729434	7225.481020	26.063437
185.135335	7220.691590	26.068455
185.547655	7246.659552	26.073472
185.741144	7240.178839	26.078490
185.745644	7238.908452	26.083508
185.741549	7257.992084	26.088525
186.443285	7264.291929	26.093543
186.426070	7267.873260	26.098560
186.830089	7271.042751	26.103578
187.278327	7278.615852	26.108596
187.045041	7283.175143	26.113613
187.374737	7288.030788	26.118631
187.427019	7308.077099	26.123648
187.538556	7308.149232	26.128666
187.710588	7305.494632	26.133684
187.658293	7314.414344	26.138701
188.168024	7321.258103	26.143719
187.962316	7338.856698	26.148736
188.162692	7321.307205	26.153754
188.304027	7345.403160	26.158772
188.415378	7351.813741	26.163789
189.027300	7360.653833	26.168807
189.296634	7379.834748	26.173824
189.662106	7367.786471	26.178842
189.692354	7362.567907	26.183860
189.745260	7370.512357	26.188877
190.017028	7401.626970	26.193895
189.986729	7403.037305	26.198912
190.101997	7408.616258	26.203930
190.414853	7423.696436	26.208948
190.684286	7440.817630	26.213965
190.661505	7435.618093	26.218983
190.744489	7463.656015	26.224000
191.175615	7465.615104	26.229018
191.382556	7467.132534	26.234036
191.209598	7490.886303	26.239053
191.541810	7500.230593	26.244071
191.555740	7519.098081	26.249088
191.772926	7524.857062	26.254106
192.053799	7543.456523	26.259124
192.509141	7556.543155	26.264141
192.853943	7554.467112	26.269159
192.802588	7563.872021	26.274176
193.153203	7589.646000	26.279194
193.576331	7581.100276	26.284212
193.216586	7612.131974	26.289229
193.981251	7613.661511	26.294247
193.946316	7617.952420	26.299264
194.055062	7635.647967	26.304282
194.407619	7645.096088	26.309300
194.294008	7655.748067	26.314317
194.764299	7654.483749	26.319335
194.576045	7688.020310	26.324352
194.801112	7683.119006	26.329370
194.717854	7702.291154	26.334388
195.327115	7705.954386	26.339405
195.568194	7725.565767	26.344423
195.877699	7735.858413	26.349440
195.776911	7752.899674	26.354458
196.153580	7761.522293	26.359476
196.148448	7771.978306	26.364493
196.773373	7784.112195	26.369511
197.119909	7793.765419	26.374528
197.149918	7787.954407	26.379546
197.623816	7786.975414	26.384564
197.765431	7814.165315	26.389581
197.582929	7815.074006	26.394599
197.680903	7824.868586	26.399616
198.005749	7831.049326	26.404634
198.131529	7842.068106	26.409652
198.292387	7861.141594	26.414669
199.120225	7872.506912	26.419687
198.957045	7877.927495	26.424704
199.185309	7875.842418	26.429722
199.587747	7889.742358	26.434740
199.439675	7900.643626	26.439757
199.897243	7914.533640	26.444775
199.909634	7914.695508	26.449792
199.913252	7905.517473	26.454810
200.501798	7923.702340	26.459828
200.211590	7936.697332	26.464845
200.445388	7934.835036	26.469863
200.631324	7940.462301	26.474880
201.050669	7964.455498	26.479898
201.530707	7958.651572	26.484916
201.554049	7966.768226	26.489933
201.712517	7974.168464	26.494951
201.888228	7997.840637	26.499968
201.992614	7992.185762	26.504986
202.311564	7998.068219	26.510004
202.057357	8015.485780	26.515021
202.265773	8021.802521	26.520039
202.744095	8039.963299	26.525056
202.691647	8052.295803	26.530074
203.221288	8053.908550	26.535092
203.550300	8072.282436	26.540109
203.638549	8082.472646	26.545127
203.744156	8086.446513	26.550144
204.091279	8094.914319	26.555162
204.471927	8098.174511	26.560180
204.937443	8105.782951	26.565197
204.836497	8109.031002	26.570215
204.899080	8127.506723	26.575232
204.904247	8136.065240	26.580250
205.470132	8139.835822	26.585268
205.487158	8155.292750	26.590285
205.793819	8160.995347	26.595303
205.876966	8167.123428	26.600320
205.796333	8185.817578	26.605338
206.430476	8188.184150	26.610356
206.752746	8204.670367	26.615373
206.935617	8214.633832	26.620391
206.897238	8219.355569	26.625408
206.847715	8226.298947	26.630426
207.390127	8239.504802	26.635444
207.681379	8259.634702	26.640461
208.022095	8266.028023	26.645479
208.069187	8280.560020	26.650496
207.763864	8285.195368	26.655514
208.352456	8301.440505	26.660532
208.505506	8314.508672	26.665549
208.451548	8327.213444	26.670567
208.799112	8338.854254	26.675584
208.741716	8350.074757	26.680602
209.535520	8369.409981	26.685620
209.149558	8389.425700	26.690637
209.392485	8400.530958	26.695655
209.783348	8411.923583	26.700672
209.627951	8438.053991	26.705690
210.364812	8441.977417	26.710708
210.317873	8467.000422	26.715725
210.611169	8471.608833	26.720743
210.849905	8498.950764	26.725760
211.371244	8508.400504	26.730778
211.562225	8512.778579	26.735796
212.315627	8529.271485	26.740813
212.821586	8528.238285	26.745831
213.479020	8507.791467	26.750848
213.077293	8515.016418	26.755866
213.360781	8504.524864	26.760884
213.318725	8507.484354	26.765901
213.458451	8500.897844	26.770919
213.861537	8506.855525	26.775936
214.143590	8529.783743	26.780954
214.270673	8535.659680	26.785972
214.187368	8536.398320	26.790989
214.360144	8545.410512	26.796007
214.298913	8546.818209	26.801024
214.017604	8552.669843	26.806042
214.255266	8566.342529	26.811060
214.126514	8579.513663	26.816077
214.728219	8601.429412	26.821095
214.980649	8610.901836	26.826112
214.877638	8620.456167	26.831130
215.258171	8643.695884	26.836148
215.233625	8661.567538	26.841165
215.357575	8680.161316	26.846183
215.776743	8692.366327	26.851200
216.138708	8726.207517	26.856218
216.437550	8732.630042	26.861236
216.973514	8748.959217	26.866253
216.990915	8768.950929	26.871271
217.579594	8774.593500	26.876288
218.294221	8778.466352	26.881306
218.423360	8774.854438	26.886324
218.629244	8779.939082	26.891341
218.594157	8779.031211	26.896359
218.915638	8794.835984	26.901376
218.963536	8815.167719	26.906394
219.321142	8801.426019	26.911412
219.475089	8820.803512	26.916429
219.572064	8842.333956	26.921447
219.566835	8846.878640	26.926464
219.742109	8863.911454	26.931482
220.208440	8872.263764	26.936500
220.007691	8876.552626	26.941517
220.261861	8898.064905	26.946535
221.163096	8894.673655	26.951552
221.171894	8924.513090	26.956570
221.687879	8924.909548	26.961588
221.713884	8934.415846	26.966605
221.762572	8951.638364	26.971623
222.238811	8961.884411	26.976640
222.227249	8966.779157	26.981658
222.260938	8975.801309	26.986676
222.437956	8984.139515	26.991693
222.385791	8999.222755	26.996711
222.771229	9011.869245	27.001728
222.882656	9040.518874	27.006746
223.537903	9046.400990	27.011764
223.810725	9054.328648	27.016781
223.777109	9076.697223	27.021799
224.270642	9090.080489	27.026816
224.486744	9092.764804	27.031834
224.692621	9110.304840	27.036852
224.889916	9112.154106	27.041869
224.881562	9128.129811	27.046887
225.191746	9140.346972	27.051904
225.237403	9158.976373	27.056922
225.716150	9170.220234	27.061940
226.035403	9178.582175	27.066957
226.738844	9194.676014	27.071975
227.288325	9187.706824	27.076992
227.085600	9190.831781	27.082010
226.996464	9189.875360	27.087028
227.571047	9197.800219	27.092045
227.311802	9226.302222	27.097063
227.618680	9213.565912	27.102080
227.555604	9237.207909	27.107098
227.887705	9249.066229	27.112116
228.439952	9247.158753	27.117133
228.593842	9268.547970	27.122151
228.771774	9278.062316	27.127168
228.906080	9287.677661	27.132186
228.887052	9286.985306	27.137204
229.391477	9310.352724	27.142221
229.474524	9324.303047	27.147239
229.566037	9323.192924	27.152256
229.762600	9335.087219	27.157274
230.179306	9351.717276	27.162292
230.303319	9370.552905	27.167309
230.271310	9374.542869	27.172327
230.548518	9392.421923	27.177344
230.714981	9405.606132	27.182362
231.299097	9432.265996	27.187380
231.583749	9434.085818	27.192397
231.532319	9448.372128	27.197415
231.925968	9466.784150	27.202432
232.036939	9489.440450	27.207450
232.735107	9500.171482	27.212468
233.011244	9498.316944	27.217485
233.111047	9517.809051	27.222503
233.647094	9521.343868	27.227520
233.725227	9532.219690	27.232538
233.998127	9543.880878	27.237556
234.561707	9553.848101	27.242573
234.347905	9560.032356	27.247591
235.001374	9557.517191	27.252608
234.523170	9569.580490	27.257626
234.451129	9578.426754	27.262644
234.924696	9591.182744	27.267661
234.765767	9611.154385	27.272679
235.207116	9638.611130	27.277696
235.803474	9653.443071	27.282714
235.799949	9669.435057	27.287732
235.555022	9681.963079	27.292749
236.120868	9705.722643	27.297767
236.380010	9722.613238	27.302784
237.112041	9736.587657	27.307802
237.291246	9747.056087	27.312820
238.118414	9749.850906	27.317837
238.261044	9759.620347	27.322855
238.957269	9744.320839	27.327872
239.104722	9737.855435	27.332890
239.383869	9731.774654	27.337908
239.845798	9751.664588	27.342925
240.501953	9759.779427	27.347943
240.284125	9735.384677	27.352960
240.632195	9732.331747	27.357978
240.381670	9723.679385	27.362996
240.921414	9746.517693	27.368013
240.486193	9756.562755	27.373031
240.934869	9758.592490	27.378048
240.974430	9762.552540	27.383066
240.870407	9764.370803	27.388084
241.459877	9775.004276	27.393101
241.547754	9785.790419	27.398119
241.755561	9795.975251	27.403136
242.061118	9815.890457	27.408154
241.736477	9828.019032	27.413172
242.200878	9840.026762	27.418189
242.004169	9862.388078	27.423207
242.233392	9869.779806	27.428224
242.702067	9903.693205	27.433242
242.620291	9918.037756	27.438260
243.003627	9940.000294	27.443277
243.195136	9965.635959	27.448295
243.237119	9990.158917	27.453312
243.438960	10017.359103	27.458330
243.806698	10030.115696	27.463348
244.753734	10041.703060	27.468365
244.601447	10057.656335	27.473383
244.824334	10073.059641	27.478400
245.031644	10084.960586	27.483418
245.621003	10104.075853	27.488436
246.181502	10108.248019	27.493453
246.126203	10112.447654	27.498471
246.512203	10131.024002	27.503488
246.728998	10135.572342	27.508506
246.941859	10161.706608	27.513524
247.603792	10158.241423	27.518541
247.389612	10167.523652	27.523559
247.690639	10188.580039	27.528576
248.079763	10196.050919	27.533594
248.137014	10209.879460	27.538612
248.758486	10220.532337	27.543629
248.552161	10239.913103	27.548647
248.701937	10248.755971	27.553664
248.979225	10261.459236	27.558682
249.122161	10292.143950	27.563700
249.352024	10304.003496	27.568717
249.600401	10318.421966	27.573735
249.828487	10339.670293	27.578752
249.989852	10357.102492	27.583770
250.005769	10376.800231	27.588788
250.182561	10383.933047	27.593805
250.468415	10420.970909	27.598823
251.083326	10447.317733	27.603840
251.393748	10451.917573	27.608858
251.570830	10485.397708	27.613876
252.251681	10495.070299	27.618893
252.305392	10513.945736	27.623911
252.587529	10532.386965	27.628928
253.169060	10540.126203	27.633946
253.103720	10561.447207	27.638964
253.544199	10568.297583	27.643981
253.578425	10588.954484	27.648999
254.015117	10591.339270	27.654016
254.426740	10621.186623	27.659034
254.337807	10626.597367	27.664052
254.804722	10640.591416	27.669069
254.759827	10656.128008	27.674087
255.204957	10669.010911	27.679104
255.414757	10683.856824	27.684122
255.515150	10706.942818	27.689140
255.993478	10716.087461	27.694157
256.414358	10732.236103	27.699175
256.577557	10736.694251	27.704192
257.036409	10753.349489	27.709210
256.955606	10775.138172	27.714228
257.776147	10779.514697	27.719245
257.578003	10796.049870	27.724263
257.468629	10809.787644	27.729280
257.908173	10825.087133	27.734298
257.994515	10844.592539	27.739316
258.332077	10866.128269	27.744333
258.664801	10887.341815	27.749351
259.037907	10909.875417	27.754368
259.127700	10917.775321	27.759386
259.528142	10931.099177	27.764404
260.148304	10940.934177	27.769421
260.574849	10957.762807	27.774439
260.703925	10961.950152	27.779456
261.135859	10971.573784	27.784474
260.737179	10994.097066	27.789492
261.141100	10990.358646	27.794509
261.127415	11023.020710	27.799527
261.267761	11035.007542	27.804544
262.170348	11041.387421	27.809562
262.092564	11058.279460	27.814580
262.486233	11064.019070	27.819597
263.269277	11087.620905	27.824615
263.415783	11086.131233	27.829632
263.521632	11094.261762	27.834650
263.542947	11116.307325	27.839668
263.809471	11109.325241	27.844685
263.874576	11128.164837	27.849703
264.104748	11149.154680	27.854720
264.354768	11158.249267	27.859738
264.538518	11173.996546	27.864756
265.044069	11190.089037	27.869773
265.353431	11203.987634	27.874791
265.770790	11220.086928	27.879808
266.138398	11230.565994	27.884826
266.180190	11245.186645	27.889844
266.406831	11261.007245	27.894861
266.351406	11285.478237	27.899879
266.714332	11293.485793	27.904896
266.925506	11306.910738	27.909914
267.253113	11334.630369	27.914932
267.380764	11342.261042	27.919949
267.729545	11371.066055	27.924967
268.230783	11382.863978	27.929984
268.341521	11411.974911	27.935002
268.331153	11429.089348	27.940020
268.779115	11445.711659	27.945037
269.148577	11460.088976	27.950055
269.603926	11477.641363	27.955072
270.051982	11486.791476	27.960090
270.220478	11506.206821	27.965108
270.394287	11533.200708	27.970125
270.828963	11532.647970	27.975143
270.717846	11560.176148	27.980160
271.388308	11560.835392	27.985178
271.396600	11574.869419	27.990196
271.821854	11587.003148	27.995213
272.702420	11601.324043	28.000231
272.587499	11622.813048	28.005248
272.696735	11631.880867	28.010266
272.898857	11648.827869	28.015284
273.319285	11660.306934	28.020301
273.322825	11675.802579	28.025319
273.701444	11699.601716	28.030336
273.966085	11717.501203	28.035354
274.502014	11733.535614	28.040372
274.541999	11747.389614	28.045389
274.867237	11764.371436	28.050407
274.839110	11784.473730	28.055424
275.267836	11796.781952	28.060442
275.680730	11821.598259	28.065460
275.998830	11843.976848	28.070477
276.231289	11851.642351	28.075495
275.976077	11874.243868	28.080512
276.255422	11892.194682	28.085530
276.805078	11920.611172	28.090548
277.077893	11932.193745	28.095565
277.676741	11951.141026	28.100583
277.725652	11973.159534	28.105600
278.273744	11984.816173	28.110618
278.514542	12004.409200	28.115636
278.609582	12013.624565	28.120653
279.197430	12041.593698	28.125671
279.104776	12053.897338	28.130688
279.611591	12066.867240	28.135706
279.401882	12081.432727	28.140724
279.703504	12102.637280	28.145741
280.057644	12124.480796	28.150759
280.202316	12151.625529	28.155776
280.956119	12154.918335	28.160794
281.249493	12171.719932	28.165812
281.635617	12171.739387	28.170829
282.087336	12181.609440	28.175847
282.112857	12204.306600	28.180864
282.350001	12208.712689	28.185882
282.617631	12230.717272	28.190900
282.894168	12229.818892	28.195917
283.779652	12235.182538	28.200935
284.033318	12247.252297	28.205952
284.297415	12255.796777	28.210970
284.273887	12266.696060	28.215988
284.373186	12276.161425	28.221005
285.145928	12287.145901	28.226023
285.260273	12309.218605	28.231040
285.555545	12307.527615	28.236058
285.574922	12324.384345	28.241076
285.758777	12337.299387	28.246093
286.145444	12357.561977	28.251111
285.720232	12382.403344	28.256128
286.091400	12396.009050	28.261146
286.355964	12418.362659	28.266164
286.721277	12446.424617	28.271181
286.831421	12466.889292	28.276199
287.192917	12499.458908	28.281216
287.548693	12527.620294	28.286234
287.650218	12550.620482	28.291252
288.176808	12564.766242	28.296269
288.352850	12580.114327	28.301287
288.665056	12608.910285	28.306304
289.183052	12626.674135	28.311322
289.955483	12637.528107	28.316340
290.481551	12652.157822	28.321357
291.156604	12654.593939	28.326375
291.007110	12669.443060	28.331392
291.505363	12679.017303	28.336410
291.609588	12693.464997	28.341428
291.739535	12714.230836	28.346445
292.387467	12708.010465	28.351463
292.684939	12735.061451	28.356480
292.613671	12745.731029	28.361498
293.265460	12753.447065	28.366516
292.937872	12771.006433	28.371533
293.478200	12785.096525	28.376551
293.377224	12807.924279	28.381568
293.551644	12820.954736	28.386586
293.912883	12846.123163	28.391604
293.670400	12874.756449	28.396621
294.409051	12901.260076	28.401639
294.187236	12926.965164	28.406656
294.483653	12960.882876	28.411674
294.928409	12982.154627	28.416692
295.345453	13016.709566	28.421709
296.068654	13035.694195	28.426727
296.802474	13062.996298	28.431744
296.873795	13068.772844	28.436762
297.203295	13088.138121	28.441780
297.334864	13112.035533	28.446797
298.042807	13120.022929	28.451815
297.823669	13134.647655	28.456832
298.180666	13148.714939	28.461850
298.503147	13168.032623	28.466868
299.020416	13190.773964	28.471885
299.621872	13203.023046	28.476903
300.003025	13216.221195	28.481920
300.020073	13228.636723	28.486938
300.272744	13240.817702	28.491956
300.426184	13253.910302	28.496973
301.178597	13260.405858	28.501991
301.154832	13274.853268	28.507008
301.450887	13284.937392	28.512026
301.785110	13297.798275	28.517044
302.275313	13310.209330	28.522061
302.524515	13315.210998	28.527079
302.583356	13333.680700	28.532096
302.894122	13348.274320	28.537114
303.139162	13364.049793	28.542132
303.533799	13377.085087	28.547149
303.626807	13387.488252	28.552167
303.889914	13410.339889	28.557184
304.228692	13434.170256	28.562202
304.645008	13442.433196	28.567220
304.913749	13474.136070	28.572237
304.875649	13487.493918	28.577255
305.245789	13515.643598	28.582272
304.932723	13534.610274	28.587290
305.548364	13556.021439	28.592308
305.750388	13583.868215	28.597325
306.012972	13607.837570	28.602343
306.324484	13637.738638	28.607360
306.705267	13672.096117	28.612378
307.004998	13692.417367	28.617396
307.296337	13723.061072	28.622413
308.023693	13746.995972	28.627431
308.508188	13764.575944	28.632448
308.618735	13785.730910	28.637466
308.840427	13807.069164	28.642484
308.463651	13846.955320	28.647501
309.012198	13871.797932	28.652519
309.525915	13903.163082	28.657536
310.032578	13940.592305	28.662554
310.474906	13956.995919	28.667572
310.303285	13988.120483	28.672589
310.671701	14011.563803	28.677607
311.317595	14045.707820	28.682624
312.656486	14057.343331	28.687642
313.343108	14064.879275	28.692660
313.400661	14063.137769	28.697677
314.071893	14081.875370	28.702695
313.682250	14098.653737	28.707712
313.637194	14109.948678	28.712730
314.393096	14115.558287	28.717748
314.545061	14130.427998	28.722765
314.760238	14154.473800	28.727783
315.003848	14168.455210	28.732800
315.022042	14186.155653	28.737818
315.209975	14212.722964	28.742836
315.595571	14232.165388	28.747853
315.823853	14262.833189	28.752871
316.104491	14286.270997	28.757888
316.246970	14328.595281	28.762906
316.684542	14337.874839	28.767924
316.668223	14378.361187	28.772941
316.926562	14403.366294	28.777959
317.509055	14428.498834	28.782976
317.688354	14461.293341	28.787994
318.234829	14482.624229	28.793012
318.303964	14510.869758	28.798029
318.557372	14539.522866	28.803047
319.288251	14562.345690	28.808064
319.748734	14604.554817	28.813082
320.703055	14604.339630	28.818100
321.531819	14628.801146	28.823117
321.768176	14631.617785	28.828135
322.043439	14633.227004	28.833152
322.267192	14639.669099	28.838170
322.600959	14618.195098	28.843188
322.786865	14640.509661	28.848205
322.922137	14648.304533	28.853223
323.056618	14646.610077	28.858240
323.078675	14676.324720	28.863258
323.783959	14682.289672	28.868276
323.866948	14698.960191	28.873293
324.302943	14720.071758	28.878311
324.394724	14735.702225	28.883328
324.600175	14771.474931	28.888346
325.134871	14779.583346	28.893364
324.515041	14802.783767	28.898381
324.937079	14831.965728	28.903399
325.479203	14846.526985	28.908416
325.267297	14890.656311	28.913434
325.624746	14919.125735	28.918452
326.284793	14960.629639	28.923469
326.335589	14992.262911	28.928487
326.909741	15027.213672	28.933504
326.705244	15058.358334	28.938522
327.742086	15089.016299	28.943540
328.011564	15122.854712	28.948557
328.637242	15158.225894	28.953575
329.831542	15156.423104	28.958592
330.338332	15161.218636	28.963610
331.183639	15179.353302	28.968628
331.387709	15183.095850	28.973645
331.644305	15182.545801	28.978663
331.887242	15189.930594	28.983680
331.977846	15214.370608	28.988698
332.371305	15206.008665	28.993716
332.406799	15222.068192	28.998733
332.982011	15238.854507	29.003751
333.558148	15247.864116	29.008768
333.771636	15266.691729	29.013786
333.695872	15265.963623	29.018804
333.695451	15295.763503	29.023821
334.025924	15306.431056	29.028839
334.819188	15321.296189	29.033856
334.322030	15352.551494	29.038874
335.019600	15369.959102	29.043892
335.451949	15395.363948	29.048909
335.577263	15416.029964	29.053927
336.529999	15428.723586	29.058944
336.713737	15437.599892	29.063962
337.482982	15460.641412	29.068980
337.351806	15468.413162	29.073997
337.624567	15486.296530	29.079015
338.002912	15496.068887	29.084032
338.091001	15531.823342	29.089050
338.895931	15534.626073	29.094068
338.936523	15563.700903	29.099085
339.027709	15583.756526	29.104103
339.606950	15593.678403	29.109120
339.693184	15624.427511	29.114138
339.731054	15641.357090	29.119156
340.423373	15665.797119	29.124173
340.374390	15694.997391	29.129191
341.117711	15704.381403	29.134208
341.544508	15734.237202	29.139226
342.269130	15740.535059	29.144244
342.630954	15757.967330	29.149261
343.037582	15778.506688	29.154279
343.318232	15785.407906	29.159296
343.341263	15799.775685	29.164314
343.719561	15813.468178	29.169332
344.196901	15833.915473	29.174349
344.411369	15846.336440	29.179367
345.005615	15841.049043	29.184384
345.024942	15871.398345	29.189402
345.235143	15876.566476	29.194420
345.462041	15897.753699	29.199437
345.333728	15928.460206	29.204455
345.948633	15951.699860	29.209472
346.102904	15974.927798	29.214490
346.097495	16000.322761	29.219508
346.103712	16028.201486	29.224525
346.546366	16072.658698	29.229543
347.098198	16099.740774	29.234560
347.360216	16143.178432	29.239578
348.021477	16175.004167	29.244596
348.383429	16207.259549	29.249613
349.016910	16225.823043	29.254631
349.424041	16238.765553	29.259648
350.062163	16267.693503	29.264666
349.975492	16286.190699	29.269684
350.458938	16319.111773	29.274701
350.594997	16353.030047	29.279719
351.604137	16371.969496	29.284736
351.513475	16395.875508	29.289754
351.642136	16426.965834	29.294772
351.695579	16463.219846	29.299789
351.947857	16489.201672	29.304807
352.887427	16515.288467	29.309824
353.239506	16546.724932	29.314842
353.481683	16575.571028	29.319860
353.814871	16607.554551	29.324877
353.643287	16645.422590	29.329895
354.589779	16673.639579	29.334912
355.063526	16704.846493	29.339930
355.218078	16745.530950	29.344948
355.384358	16760.310817	29.349965
355.697708	16789.014632	29.354983
357.310856	16785.630478	29.360000
358.322243	16799.472408	29.365018
358.920781	16815.997957	29.370036
359.256892	16822.989705	29.375053
358.929249	16843.948700	29.380071
359.389964	16841.153188	29.385088
359.936079	16855.107131	29.390106
360.371271	16869.448359	29.395124
360.756920	16870.309655	29.400141
360.623932	16885.906991	29.405159
361.016663	16907.627543	29.410176
361.347443	16920.149797	29.415194
361.398964	16941.931801	29.420212
361.548338	16954.894047	29.425229
361.315047	16987.807834	29.430247
361.781798	17005.871851	29.435264
362.160489	17054.773272	29.440282
362.390599	17084.534932	29.445300
362.726345	17117.616118	29.450317
362.864847	17153.116652	29.455335
363.237925	17189.626538	29.460352
363.304488	17222.762106	29.465370
363.653481	17259.708055	29.470388
364.547445	17287.670003	29.475405
365.147262	17318.247101	29.480423
365.934755	17337.620140	29.485440
366.415707	17359.714405	29.490458
366.527421	17391.134079	29.495476
367.079559	17410.997127	29.500493
367.237757	17435.329891	29.505511
367.641390	17454.438954	29.510528
367.693110	17489.964082	29.515546
367.716871	17501.956108	29.520564
368.587769	17531.552230	29.525581
368.482347	17561.376787	29.530599
369.011804	17584.662889	29.535616
369.458866	17610.573135	29.540634
369.767807	17648.712015	29.545652
369.930101	17671.788097	29.550669
370.217437	17704.052487	29.555687
370.445981	17740.352718	29.560704
371.349341	17767.059139	29.565722
372.095303	17789.729468	29.570740
372.552558	17812.974289	29.575757
373.262775	17819.606386	29.580775
373.659693	17838.862034	29.585792
374.194090	17848.784848	29.590810
374.259913	17867.094533	29.595828
374.787515	17878.698901	29.600845
374.850298	17896.350201	29.605863
375.276673	17924.591098	29.610880
375.584516	17949.732085	29.615898
375.229927	17965.677787	29.620916
375.711054	17995.847078	29.625933
376.050072	18032.632462	29.630951
376.245304	18063.733716	29.635968
376.731754	18103.075311	29.640986
377.059621	18128.996708	29.646004
377.858122	18158.743125	29.651021
377.973197	18191.785864	29.656039
378.087729	18233.309800	29.661056
378.716343	18261.820347	29.666074
379.025469	18302.739898	29.671092
379.832883	18329.688592	29.676109
380.241782	18364.801565	29.681127
380.476374	18388.930714	29.686144
380.784603	18425.310635	29.691162
380.998073	18459.742152	29.696180
381.295640	18487.705880	29.701197
381.520008	18523.656970	29.706215
382.024055	18563.329357	29.711232
382.608100	18596.203566	29.716250
382.726537	18637.083097	29.721268
383.445735	18666.397463	29.726285
383.678146	18710.751641	29.731303
384.172404	18739.097725	29.736320
384.734258	18775.288096	29.741338
384.957007	18809.394044	29.746356
385.518217	18829.969845	29.751373
385.878033	18857.137200	29.756391
386.434200	18895.252059	29.761408
386.801239	18928.393133	29.766426
387.327557	18945.356879	29.771444
387.411059	18971.356436	29.776461
387.989854	19009.981728	29.781479
388.171443	19036.086482	29.786496
388.594002	19064.101357	29.791514
388.816714	19101.141737	29.796532
389.587079	19123.185549	29.801549
389.927783	19148.526254	29.806567
390.706513	19170.988086	29.811584
391.177564	19193.518396	29.816602
391.605471	19222.536875	29.821620
392.310328	19229.917696	29.826637
392.660017	19261.760129	29.831655
393.013081	19271.097507	29.836672
394.259847	19265.989164	29.841690
394.723613	19282.178548	29.846708
395.276085	19274.874374	29.851725
395.279851	19285.573545	29.856743
395.245221	19283.116886	29.861760
395.514699	19283.625562	29.866778
395.623845	19303.332713	29.871796
396.036481	19314.654498	29.876813
396.951542	19314.114770	29.881831
397.121770	19327.288231	29.886848
397.718128	19332.014944	29.891866
397.772218	19354.075565	29.896884
397.879955	19365.547349	29.901901
397.937328	19381.197375	29.906919
398.333773	19412.113224	29.911936
398.164512	19439.380444	29.916954
398.563648	19455.847164	29.921972
399.078321	19501.045713	29.926989
399.089609	19530.029877	29.932007
399.305816	19566.419689	29.937024
399.922970	19603.482375	29.942042
399.882594	19648.828695	29.947060
400.326144	19675.245656	29.952077
401.002551	19722.278254	29.957095
401.441725	19769.055573	29.962112
402.164873	19804.002715	29.967130
402.516941	19842.967139	29.972148
402.754453	19880.437186	29.977165
403.264201	19910.456993	29.982183
403.441048	19956.542154	29.987200
404.437160	19980.558151	29.992218
404.914546	20007.116637	29.997236
405.403559	20036.646649	30.002253
406.057523	20054.998204	30.007271
406.202826	20087.599804	30.012288
406.962249	20109.749220	30.017306
407.124174	20151.159685	30.022324
407.638824	20160.688292	30.027341
408.082949	20189.939092	30.032359
408.434487	20218.554190	30.037376
409.248955	20242.700061	30.042394
409.340079	20277.600240	30.047412
409.789535	20303.567883	30.052429
410.281303	20328.787536	30.057447
410.658331	20358.847535	30.062464
411.034253	20381.808319	30.067482
410.975711	20403.766052	30.072500
411.689859	20432.147860	30.077517
411.889552	20477.306763	30.082535
412.053380	20504.990216	30.087552
412.802612	20536.557444	30.092570
413.199914	20578.202621	30.097588
413.620533	20601.277682	30.102605
414.162252	20637.811252	30.107623
414.431373	20658.697968	30.112640
414.621782	20688.245615	30.117658
415.075707	20735.872985	30.122676
415.536868	20771.742272	30.127693
415.819790	20797.257464	30.132711
415.856624	20844.995412	30.137728
416.589296	20874.549494	30.142746
417.546154	20908.211415	30.147764
417.972900	20930.160179	30.152781
418.498420	20962.373956	30.157799
418.687205	20988.803769	30.162816
419.258936	21011.491662	30.167834
419.635530	21046.234077	30.172852
419.963023	21073.495538	30.177869
420.363185	21109.717814	30.182887
420.749711	21131.490628	30.187904
421.429193	21153.408743	30.192922
421.455381	21178.177239	30.197940
421.820441	21208.857227	30.202957
422.551816	21228.925257	30.207975
422.873322	21249.307351	30.212992
423.408428	21269.255091	30.218010
423.957471	21298.255468	30.223028
424.289249	21320.475940	30.228045
424.616871	21347.715750	30.233063
424.892463	21377.819645	30.238080
425.211844	21404.460194	30.243098
425.541952	21428.417032	30.248116
426.185050	21462.078570	30.253133
426.705468	21491.848737	30.258151
426.631669	21523.989693	30.263168
427.040310	21553.616134	30.268186
427.479364	21601.166431	30.273204
427.627340	21642.999133	30.278221
428.255418	21667.829203	30.283239
428.339473	21712.022012	30.288256
428.764119	21747.891559	30.293274
429.179806	21796.698213	30.298292
429.653002	21840.730544	30.303309
430.331902	21892.476950	30.308327
430.247058	21929.699207	30.313344
430.977814	21977.899038	30.318362
431.261059	22021.961813	30.323380
431.645412	22081.223666	30.328397
432.355143	22108.137918	30.333415
432.693992	22158.617135	30.338432
433.745377	22184.397830	30.343450
433.800722	22237.779905	30.348468
434.522825	22275.012381	30.353485
435.378656	22310.910844	30.358503
435.427958	22338.334080	30.363520
436.239116	22371.693581	30.368538
436.405856	22405.062418	30.373556
436.774355	22434.255567	30.378573
437.355446	22475.742450	30.383591
437.407873	22516.789011	30.388608
437.867308	22559.523057	30.393626
438.031850	22603.088288	30.398644
438.843853	22640.774952	30.403661
439.237209	22677.805895	30.408679
439.693557	22722.991242	30.413696
439.803546	22768.607944	30.418714
440.646485	22808.916837	30.423732
440.903122	22854.854739	30.428749
441.484810	22891.949480	30.433767
441.893429	22929.968692	30.438784
442.393051	22967.703235	30.443802
443.704710	22993.341022	30.448820
443.779022	23024.537762	30.453837
444.461905	23049.592559	30.458855
445.010743	23081.727662	30.463872
445.544285	23116.290575	30.468890
445.645665	23148.777649	30.473908
446.116569	23179.440477	30.478925
446.876426	23211.275865	30.483943
446.553149	23243.403164	30.488960
446.832406	23277.909296	30.493978
447.774557	23309.227337	30.498996
448.030728	23352.377166	30.504013
448.718052	23389.088035	30.509031
448.904120	23431.505418	30.514048
449.238523	23457.170606	30.519066
449.688107	23499.719428	30.524084
450.171804	23534.323008	30.529101
450.803584	23556.553357	30.534119
451.265217	23586.439470	30.539136
451.589361	23619.037095	30.544154
451.859532	23649.924915	30.549172
452.419101	23693.616559	30.554189
453.480948	23708.211232	30.559207
453.878810	23723.146425	30.564224
454.805882	23744.329791	30.569242
455.202845	23753.447914	30.574260
456.520431	23762.917755	30.579277
457.354756	23755.271562	30.584295
457.481040	23761.853231	30.589312
457.767902	23774.969795	30.594330
458.064153	23784.397969	30.599348
458.196187	23800.785571	30.604365
458.717458	23814.098197	30.609383
459.080702	23830.259773	30.614400
459.521719	23846.878373	30.619418
459.846812	23857.629570	30.624436
460.250028	23888.743306	30.629453
460.673501	23909.119553	30.634471
460.807751	23935.244477	30.639488
461.202315	23965.580785	30.644506
461.324464	23990.085134	30.649524
461.078494	24028.764295	30.654541
461.763906	24069.414581	30.659559
462.170892	24110.467597	30.664576
462.569434	24160.324677	30.669594
463.093325	24192.518064	30.674612
463.953083	24222.217747	30.679629
464.864295	24255.863964	30.684647
465.192005	24289.805854	30.689664
465.340577	24327.921842	30.694682
465.952477	24359.448061	30.699700
466.163884	24407.728430	30.704717
466.740757	24439.487699	30.709735
467.044340	24494.347941	30.714752
467.288492	24525.904003	30.719770
467.634771	24568.280256	30.724788
468.096774	24625.139465	30.729805
468.558026	24652.007560	30.734823
468.985342	24710.818833	30.739840
468.986082	24751.814697	30.744858
469.590452	24809.619158	30.749876
469.739682	24862.550714	30.754893
470.336310	24918.521177	30.759911
471.100830	24977.312056	30.764928
471.003272	25032.975537	30.769946
471.663080	25091.891438	30.774964
472.019169	25148.476643	30.779981
473.023897	25199.198071	30.784999
473.365266	25252.704506	30.790016
474.183034	25293.105470	30.795034
475.175760	25336.328804	30.800052
475.899725	25392.740169	30.805069
476.328041	25422.447358	30.810087
476.686023	25463.887099	30.815104
477.462536	25503.276620	30.820122
478.210335	25535.886393	30.825140
478.460723	25571.912795	30.830157
479.045622	25599.083566	30.835175
479.601134	25636.456728	30.840192
480.222174	25671.781484	30.845210
480.948647	25690.740616	30.850228
481.148818	25725.103957	30.855245
481.809864	25753.949823	30.860263
481.971443	25780.049363	30.865280
482.063241	25813.844196	30.870298
482.776698	25842.637349	30.875316
482.956597	25879.937790	30.880333
483.358662	25913.205002	30.885351
483.640554	25953.721754	30.890368
483.432138	25998.042042	30.895386
483.752522	26039.473643	30.900404
484.492639	26093.506317	30.905421
485.046686	26138.876881	30.910439
485.479731	26188.122194	30.915456
485.576650	26238.271974	30.920474
486.145448	26293.869869	30.925492
486.710715	26347.796744	30.930509
486.962537	26398.277700	30.935527
487.637435	26437.626307	30.940544
488.164100	26509.653337	30.945562
488.621507	26553.933869	30.950580
489.004522	26617.525241	30.955597
489.529926	26672.787738	30.960615
490.287167	26733.491071	30.965632
490.284257	26784.173177	30.970650
491.668429	26829.388768	30.975668
491.945569	26888.945318	30.980685
492.567775	26927.048337	30.985703
493.150750	26966.795102	30.990720
494.032687	27012.637144	30.995738
495.349946	27036.972594	31.000756
496.882789	27046.052099	31.005773
497.625250	27075.391372	31.010791
498.094361	27086.811505	31.015808
498.461233	27099.529332	31.020826
498.755923	27124.050499	31.025844
499.129242	27140.735589	31.030861
499.307508	27163.935504	31.035879
499.752843	27178.173426	31.040896
499.630882	27218.899011	31.045914
500.297913	27244.860043	31.050932
500.596744	27288.821801	31.055949
500.618071	27330.728865	31.060967
501.090732	27372.072129	31.065984
501.235371	27415.886319	31.071002
502.096598	27457.405000	31.076020
502.379516	27514.943855	31.081037
502.904891	27557.865534	31.086055
503.241123	27603.131008	31.091072
503.253369	27655.125433	31.096090
504.143897	27701.289640	31.101108
504.571058	27746.597170	31.106125
505.575261	27792.998264	31.111143
506.369764	27829.459517	31.116160
506.249567	27877.407191	31.121178
506.843981	27931.037630	31.126196
507.248296	27981.109858	31.131213
507.953370	28027.886182	31.136231
508.527636	28084.747616	31.141248
508.686352	28129.122790	31.146266
509.180114	28179.732798	31.151284
509.609675	28238.192932	31.156301
510.347187	28285.182233	31.161319
510.954531	28336.811720	31.166336
511.349000	28396.230925	31.171354
512.101694	28428.533042	31.176372
512.649293	28492.126037	31.181389
512.795546	28542.775883	31.186407
513.471400	28586.593134	31.191424
513.408776	28649.347935	31.196442
514.054022	28696.268491	31.201460
515.110876	28742.196478	31.206477
515.946397	28794.672759	31.211495
516.357167	28839.474787	31.216512
517.363642	28867.057060	31.221530
518.307493	28889.242495	31.226548
518.500730	28924.607084	31.231565
518.629476	28957.875058	31.236583
519.329737	28985.031998	31.241600
519.522764	29031.738316	31.246618
520.315794	29075.486863	31.251636
520.433872	29109.589766	31.256653
520.650364	29156.197875	31.261671
520.866148	29196.373529	31.266688
521.360905	29249.687012	31.271706
521.998029	29287.723332	31.276724
523.039904	29335.665010	31.281741
523.525033	29375.790038	31.286759
524.236369	29414.467366	31.291776
524.816828	29460.599402	31.296794
525.347925	29498.000728	31.301812
525.863447	29550.699634	31.306829
526.185779	29592.988058	31.311847
526.761340	29625.473249	31.316864
526.883231	29682.074284	31.321882
527.764264	29724.301794	31.326900
528.294855	29772.865917	31.331917
528.709180	29816.802254	31.336935
529.310134	29867.522399	31.341952
529.592680	29916.923159	31.346970
530.191198	29979.803248	31.351988
530.911602	30023.793390	31.357005
531.067110	30065.880344	31.362023
531.400900	30115.582343	31.367040
531.682260	30181.957923	31.372058
532.636975	30234.286226	31.377076
533.130736	30300.986656	31.382093
533.647426	30345.566719	31.387111
534.382151	30396.310349	31.392128
536.015664	30422.718247	31.397146
536.982709	30454.647780	31.402164
537.690523	30490.128846	31.407181
538.145458	30521.925844	31.412199
538.848346	30546.989815	31.417216
538.947935	30577.984589	31.422234
539.341235	30615.010488	31.427252
539.689506	30657.972360	31.432269
539.905519	30694.967921	31.437287
540.791915	30743.393614	31.442304
541.045800	30784.822311	31.447322
541.077482	30841.404200	31.452340
541.547384	30885.677891	31.457357
541.887689	30947.746129	31.462375
542.647820	30997.269392	31.467392
542.718322	31055.729147	31.472410
543.117940	31119.293151	31.477428
543.887319	31169.989089	31.482445
544.180441	31240.143461	31.487463
544.571292	31290.164287	31.492480
545.228113	31360.312379	31.497498
545.555747	31420.027434	31.502516
546.312440	31484.211831	31.507533
546.241434	31553.112177	31.512551
547.430591	31614.697878	31.517568
548.501875	31664.975940	31.522586
549.677385	31714.040987	31.527604
550.462499	31758.513794	31.532621
551.085127	31802.240647	31.537639
551.504258	31845.218885	31.542656
552.515053	31880.646135	31.547674
553.141705	31915.572444	31.552692
553.851592	31942.751308	31.557709
554.452022	31976.044479	31.562727
555.059015	31989.972357	31.567744
555.043672	32032.035580	31.572762
555.926681	32057.769127	31.577780
556.099179	32088.053958	31.582797
556.345753	32133.570052	31.587815
556.753911	32165.403027	31.592832
557.142420	32209.277047	31.597850
557.435602	32255.101251	31.602868
557.974644	32294.690729	31.607885
558.453733	32357.709575	31.612903
559.304561	32399.323762	31.617920
559.494567	32454.363614	31.622938
559.567116	32513.253823	31.627956
560.187362	32563.997461	31.632973
560.360593	32626.885037	31.637991
561.179513	32691.461068	31.643008
561.539851	32766.854692	31.648026
562.389856	32830.507827	31.653044
563.179496	32894.417342	31.658061
563.093297	32962.530499	31.663079
563.892480	33015.981536	31.668096
564.355673	33073.082665	31.673114
564.950421	33146.356329	31.678132
566.078897	33197.541203	31.683149
566.384719	33280.951673	31.688167
567.090374	33336.997298	31.693184
567.274592	33401.940062	31.698202
567.683554	33465.028122	31.703220
569.002089	33527.321626	31.708237
569.507416	33601.280998	31.713255
570.382760	33659.199140	31.718272
571.047621	33706.631536	31.723290
571.795237	33764.309312	31.728308
572.818116	33815.491412	31.733325
573.386572	33862.195497	31.738343
574.306385	33905.805607	31.743360
574.542143	33953.379338	31.748378
575.080120	34009.369719	31.753396
576.435671	34044.747210	31.758413
576.744234	34086.177695	31.763431
577.340972	34115.133250	31.768448
577.996476	34161.770019	31.773466
578.439348	34204.674285	31.778484
579.306915	34236.586158	31.783501
580.154693	34275.005341	31.788519
581.064001	34297.686186	31.793536
581.421307	34330.938941	31.798554
581.796554	34375.830343	31.803572
581.929876	34403.531590	31.808589
582.282158	34447.593866	31.813607
582.651834	34487.352045	31.818624
583.198766	34542.916582	31.823642
583.256774	34600.695791	31.828660
583.781680	34650.975215	31.833677
584.221270	34717.729654	31.838695
584.663250	34786.137597	31.843712
585.533436	34835.861587	31.848730
585.946042	34895.100819	31.853748
586.452992	34958.859543	31.858765
586.853859	35019.593855	31.863783
587.585761	35077.231140	31.868800
587.815792	35141.503564	31.873818
588.108979	35207.864402	31.878836
589.056354	35291.165091	31.883853
589.763255	35355.545296	31.888871
590.068559	35424.003610	31.893888
590.560633	35488.274788	31.898906
591.239090	35560.133733	31.903924
591.770704	35613.870516	31.908941
592.390638	35682.220760	31.913959
592.902143	35740.070347	31.918976
593.775840	35812.664788	31.923994
593.985458	35880.720976	31.929012
594.563481	35949.634653	31.934029
595.158199	36013.707613	31.939047
596.160579	36066.300837	31.944064
597.903049	36101.769655	31.949082
598.634417	36153.426602	31.954100
599.460331	36189.499100	31.959117
600.145481	36239.292419	31.964135
600.250958	36289.715504	31.969152
601.108787	36327.935432	31.974170
601.239159	36389.691356	31.979188
601.901471	36430.001745	31.984205
602.295839	36484.666563	31.989223
603.214903	36529.507763	31.994240
604.010669	36585.409718	31.999258
603.861596	36637.242646	32.004276
604.860933	36692.451496	32.009293
605.057918	36759.701962	32.014311
605.622276	36806.562728	32.019328
606.391384	36862.290063	32.024346
607.098064	36928.882100	32.029364
607.370826	36988.700612	32.034381
608.111930	37050.758222	32.039399
608.538012	37116.359143	32.044416
609.277059	37180.263934	32.049434
609.837815	37246.347963	32.054452
610.569263	37307.874650	32.059469
611.390085	37381.797185	32.064487
611.503500	37431.552999	32.069504
612.510305	37497.093593	32.074522
612.611856	37570.738632	32.079540
613.582372	37624.638931	32.084557
613.960341	37696.209068	32.089575
614.947921	37762.618648	32.094592
615.655621	37829.324295	32.099610
615.884557	37906.992835	32.104628
616.481531	37969.213242	32.109645
617.118238	38043.462583	32.114663
617.460438	38111.874433	32.119680
618.138921	38179.081768	32.124698
618.426384	38259.642839	32.129716
619.433128	38332.215825	32.134733
620.007700	38402.992237	32.139751
620.458169	38485.866174	32.144768
621.417380	38537.795111	32.149786
621.796278	38619.974489	32.154804
622.382931	38699.146314	32.159821
622.874108	38767.494851	32.164839
623.343991	38856.124732	32.169856
624.792766	38918.030181	32.174874
625.411101	38997.797783	32.179892
626.339211	39055.825515	32.184909
627.259433	39110.470892	32.189927
627.623210	39179.628111	32.194944
628.226185	39226.911686	32.199962
629.017895	39301.620213	32.204980
629.424105	39360.505779	32.209997
630.271416	39419.378273	32.215015
630.681631	39471.243188	32.220032
631.789629	39527.796811	32.225050
632.507901	39594.425083	32.230068
633.197326	39648.990437	32.235085
634.454655	39674.922156	32.240103
635.813903	39710.575344	32.245120
636.443373	39723.517476	32.250138
636.870521	39761.257413	32.255156
637.170206	39790.757522	32.260173
637.690019	39822.503424	32.265191
638.047435	39871.770807	32.270208
638.426942	39912.180069	32.275226
638.574969	39958.114235	32.280244
639.090211	40009.578116	32.285261
639.485379	40065.418379	32.290279
639.380802	40135.616615	32.295296
640.372816	40195.553501	32.300314
640.614833	40267.209939	32.305332
640.948745	40341.872443	32.310349
641.782282	40422.986874	32.315367
642.044461	40507.571163	32.320384
642.949909	40585.220813	32.325402
643.259843	40664.576498	32.330420
643.526440	40734.320780	32.335437
644.190390	40819.408025	32.340455
645.037729	40919.274164	32.345472
645.746706	41006.312066	32.350490
646.210227	41095.904036	32.355508
646.784568	41182.049614	32.360525
647.660199	41280.306129	32.365543
648.215003	41363.775548	32.370560
649.240951	41440.310168	32.375578
649.765455	41530.061436	32.380596
650.517939	41623.936222	32.385613
651.698331	41709.109141	32.390631
651.918155	41787.092357	32.395648
652.745790	41867.971025	32.400666
653.398621	41946.953260	32.405684
654.722446	42034.446402	32.410701
655.541491	42103.750530	32.415719
656.038365	42183.612081	32.420736
656.779509	42258.593562	32.425754
657.223264	42336.791320	32.430772
657.890337	42413.563188	32.435789
658.367282	42490.546897	32.440807
659.046547	42575.866986	32.445824
659.815896	42653.689988	32.450842
660.401974	42729.005359	32.455860
660.916999	42802.811058	32.460877
661.836939	42886.005696	32.465895
662.635697	42965.485818	32.470912
663.884763	43038.816972	32.475930
664.191648	43114.072908	32.480948
664.851630	43189.807259	32.485965
665.156975	43254.613448	32.490983
665.788147	43335.963670	32.496000
666.574555	43417.882047	32.501018
667.226373	43492.416046	32.506036
667.496792	43576.419371	32.511053
668.289430	43654.987819	32.516071
669.186296	43749.073530	32.521088
670.371645	43799.300032	32.526106
671.839097	43871.287894	32.531124
672.301534	43935.953541	32.536141
673.351997	43990.452811	32.541159
674.028476	44053.242559	32.546176
675.075021	44096.590793	32.551194
675.779073	44149.424085	32.556212
676.182753	44198.591084	32.561229
677.525082	44245.073258	32.566247
677.649473	44305.944218	32.571264
678.110432	44363.605184	32.576282
678.861003	44413.435059	32.581300
679.469516	44459.985921	32.586317
680.096496	44505.896019	32.591335
680.064833	44563.108925	32.596352
680.616437	44622.517525	32.601370
681.473525	44669.397066	32.606388
681.450747	44741.124171	32.611405
681.987110	44799.013928	32.616423
681.683389	44889.569317	32.621440
682.831848	44967.534781	32.626458
683.484805	45048.601484	32.631476
683.744030	45142.102222	32.636493
684.487203	45228.282665	32.641511
685.264641	45319.781578	32.646528
685.878883	45398.456415	32.651546
686.352523	45486.981554	32.656564
686.945479	45592.797671	32.661581
687.885566	45686.791188	32.666599
688.205123	45778.576750	32.671616
689.332247	45865.122650	32.676634
690.095873	45966.078053	32.681652
690.776030	46050.425436	32.686669
692.155324	46117.027323	32.691687
692.975587	46207.010859	32.696704
693.827093	46276.839765	32.701722
695.487013	46351.707198	32.706740
696.165771	46425.739950	32.711757
696.975170	46490.009407	32.716775
697.371468	46561.958051	32.721792
697.666369	46627.664945	32.726810
698.590142	46692.917141	32.731828
699.189029	46774.154961	32.736845
699.991642	46845.213020	32.741863
700.310830	46927.688453	32.746880
700.918178	47012.424839	32.751898
701.910044	47088.849264	32.756916
702.484049	47165.280210	32.761933
703.419738	47238.900844	32.766951
704.153172	47310.085813	32.771968
704.565087	47379.666490	32.776986
705.274668	47460.781497	32.782004
705.807088	47558.189969	32.787021
706.359241	47634.496948	32.792039
707.035699	47724.558921	32.797056
707.520933	47799.939737	32.802074
708.155433	47892.346419	32.807092
708.615945	47997.035762	32.812109
709.745998	48070.895782	32.817127
710.771817	48157.519488	32.822144
711.444771	48246.046508	32.827162
712.917147	48318.350552	32.832180
713.804384	48392.890072	32.837197
714.705396	48459.835397	32.842215
715.331480	48537.220116	32.847232
715.866158	48613.995002	32.852250
716.810694	48677.693576	32.857268
716.820130	48759.299839	32.862285
717.820639	48825.181403	32.867303
718.317518	48900.400398	32.872320
718.741308	48986.906729	32.877338
719.618725	49064.542411	32.882356
720.037660	49163.048543	32.887373
721.177985	49231.703361	32.892391
721.686307	49319.981587	32.897408
722.133692	49400.974645	32.902426
723.366680	49483.397837	32.907444
723.590286	49578.859163	32.912461
724.129068	49653.458273	32.917479
725.021180	49731.422680	32.922496
726.069453	49808.805605	32.927514
726.981032	49870.403818	32.932532
728.085188	49934.771754	32.937549
729.014728	49997.956067	32.942567
729.686839	50056.063532	32.947584
730.509252	50111.275215	32.952602
731.379802	50178.629558	32.957620
731.917431	50238.228570	32.962637
732.221162	50315.130709	32.967655
732.737836	50386.975839	32.972672
733.082378	50458.015973	32.977690
733.881430	50540.654703	32.982708
733.935698	50630.940989	32.987725
734.407887	50713.906352	32.992743
735.217402	50806.929704	32.997760
736.045151	50907.992150	33.002778
736.800407	50994.645135	33.007796
736.929204	51104.422256	33.012813
737.778175	51191.894432	33.017831
738.503622	51310.613585	33.022848
739.250893	51401.710732	33.027866
740.047938	51511.587692	33.032884
741.253021	51605.484170	33.037901
742.328089	51693.129544	33.042919
743.172502	51795.229892	33.047936
743.369712	51889.958382	33.052954
744.141651	51984.655100	33.057972
745.206124	52080.068132	33.062989
746.541427	52164.633722	33.068007
747.124696	52266.950468	33.073024
747.475902	52369.047253	33.078042
748.352819	52454.088200	33.083060
749.175383	52572.552542	33.088077
749.605399	52649.765155	33.093095
750.056468	52758.253515	33.098112
750.816046	52859.097340	33.103130
752.053571	52951.466029	33.108148
752.737032	53075.054946	33.113165
753.477617	53166.793233	33.118183
754.934822	53249.410033	33.123200
755.858192	53340.581774	33.128218
757.114473	53419.947344	33.133236
757.715420	53510.737463	33.138253
758.648474	53582.942254	33.143271
759.347297	53671.467672	33.148288
759.828977	53762.569382	33.153306
760.720789	53840.506102	33.158324
761.338595	53922.247874	33.163341
761.979737	54011.340389	33.168359
762.917806	54096.618409	33.173376
764.969194	54143.733546	33.178394
765.852832	54220.662229	33.183412
766.822754	54278.186341	33.188429
767.672205	54336.874216	33.193447
768.849436	54392.683607	33.198464
768.986686	54459.002448	33.203482
770.437166	54496.361714	33.208500
771.018286	54558.411882	33.213517
771.917808	54615.645391	33.218535
772.595357	54675.234738	33.223552
773.008434	54730.230503	33.228570
773.589967	54789.911955	33.233588
773.916604	54853.679660	33.238605
773.970176	54934.666314	33.243623
774.948604	55001.131673	33.248640
775.232195	55090.616978	33.253658
775.781749	55169.494039	33.258676
776.150755	55261.366960	33.263693
776.729937	55348.940407	33.268711
776.973306	55438.433960	33.273728
777.257265	55538.725976	33.278746
778.323042	55628.033321	33.283764
778.976966	55736.738206	33.288781
779.533001	55841.485475	33.293799
779.928408	55959.914734	33.298816
780.252809	56072.682230	33.303834
781.049476	56192.423757	33.308852
781.882144	56295.054929	33.313869
782.573856	56423.630049	33.318887
783.124257	56539.496837	33.323904
783.963977	56666.652476	33.328922
784.679024	56787.080935	33.333940
785.785190	56911.091280	33.338957
786.768632	57028.462466	33.343975
787.475928	57157.456786	33.348992
789.425886	57256.836361	33.354010
790.525890	57367.359201	33.359028
791.286429	57478.577240	33.364045
791.949875	57590.861008	33.369063
793.250940	57697.996780	33.374080
793.517749	57804.811895	33.379098
794.495421	57908.766986	33.384116
795.103287	58022.579040	33.389133
795.848377	58128.286427	33.394151
796.699986	58243.297879	33.399168
797.300845	58347.905499	33.404186
798.775950	58441.935028	33.409204
799.526400	58545.627795	33.414221
800.495770	58659.661511	33.419239
801.731782	58761.966642	33.424256
802.301096	58854.568548	33.429274
803.324138	58966.016675	33.434292
804.338281	59066.160932	33.439309
804.828279	59153.209710	33.444327
805.450885	59252.434002	33.449344
805.928942	59368.777837	33.454362
806.613656	59473.257301	33.459380
807.447752	59582.420812	33.464397
808.220869	59705.271313	33.469415
809.176035	59812.753835	33.474432
809.648285	59907.038818	33.479450
810.679285	60020.905670	33.484468
811.594073	60132.795317	33.489485
812.312649	60250.962387	33.494503
813.352519	60361.657000	33.499520
813.880436	60471.293245	33.504538
814.571594	60579.664231	33.509556
815.512641	60700.761154	33.514573
815.652500	60827.844339	33.519591
816.779101	60944.917513	33.524608
817.194005	61087.890133	33.529626
818.292380	61204.710350	33.534644
819.062636	61311.504645	33.539661
819.533927	61445.533355	33.544679
820.843244	61561.644314	33.549696
821.728345	61691.889509	33.554714
822.954125	61800.841898	33.559732
823.946378	61917.235045	33.564749
825.455481	62008.140467	33.569767
827.072973	62094.205648	33.574784
827.990534	62183.484498	33.579802
829.353644	62266.040405	33.584820
830.740776	62342.619572	33.589837
831.356625	62421.526663	33.594855
832.094413	62499.212871	33.599872
832.952200	62573.497830	33.604890
833.618874	62635.255313	33.609908
834.382605	62697.812260	33.614925
834.984166	62779.030202	33.619943
835.462498	62840.547766	33.624960
836.154913	62922.364319	33.629978
837.066322	62983.443817	33.634996
838.230016	63048.874678	33.640013
839.178649	63131.818912	33.645031
840.019853	63198.005402	33.650048
840.610452	63272.823951	33.655066
841.685605	63357.713931	33.660084
842.313307	63425.131263	33.665101
842.680195	63507.680524	33.670119
843.574208	63590.054130	33.675136
844.802677	63679.989520	33.680154
845.222069	63766.848438	33.685172
845.629358	63851.882906	33.690189
846.372052	63938.562461	33.695207
847.183344	64018.283951	33.700224
848.393335	64113.376106	33.705242
849.005050	64213.858922	33.710260
849.638756	64298.149658	33.715277
850.447253	64414.619028	33.720295
851.369262	64491.928170	33.725312
852.601900	64599.484569	33.730330
853.266320	64693.911369	33.735348
853.711040	64800.682974	33.740365
854.358808	64905.626118	33.745383
855.365017	65013.026272	33.750400
855.791180	65117.198105	33.755418
856.513472	65243.187752	33.760436
857.364286	65352.088382	33.765453
857.920944	65474.756446	33.770471
858.907417	65593.851662	33.775488
859.724994	65720.005381	33.780506
860.792803	65832.709809	33.785524
862.370524	65931.731978	33.790541
863.102558	66053.413416	33.795559
863.705599	66167.132420	33.800576
864.556663	66286.279342	33.805594
865.140636	66406.653478	33.810612
866.383426	66507.801245	33.815629
867.487177	66630.296773	33.820647
868.335948	66741.107905	33.825664
869.044999	66860.205791	33.830682
870.162874	66971.093593	33.835700
871.188005	67088.875890	33.840717
871.555025	67196.627260	33.845735
872.843110	67303.486613	33.850752
873.911152	67415.017248	33.855770
875.194556	67527.878348	33.860788
876.251070	67631.932767	33.865805
876.711679	67734.107701	33.870823
877.515839	67854.011005	33.875840
877.702786	67955.973210	33.880858
878.362735	68089.836419	33.885876
879.265661	68206.399710	33.890893
879.911650	68343.820087	33.895911
880.685154	68456.100581	33.900928
881.244718	68590.830839	33.905946
881.950705	68726.353273	33.910964
882.612948	68867.175929	33.915981
883.108649	69012.889346	33.920999
883.774259	69158.543946	33.926016
885.019251	69296.440120	33.931034
885.828099	69449.167147	33.936052
886.848713	69589.005638	33.941069
887.508974	69741.190353	33.946087
888.707324	69866.091633	33.951104
889.570050	70000.603448	33.956122
890.163601	70133.194306	33.961140
891.218342	70272.911470	33.966157
891.940939	70410.073207	33.971175
892.807111	70551.397948	33.976192
893.896899	70701.431549	33.981210
894.404153	70844.430213	33.986228
895.244595	70978.022337	33.991245
896.096464	71130.324228	33.996263
896.859346	71276.919278	34.001280
897.753142	71431.821588	34.006298
898.351826	71587.102810	34.011316
899.699299	71733.989683	34.016333
900.693472	71897.390169	34.021351
901.324423	72057.266666	34.026368
902.274756	72205.468412	34.031386
903.122929	72362.794291	34.036404
904.385583	72522.683216	34.041421
905.193201	72684.166555	34.046439
906.590894	72831.577424	34.051456
907.431766	72985.917847	34.056474
908.244635	73150.837666	34.061492
909.558166	73277.251030	34.066509
910.914714	73417.425408	34.071527
912.072581	73559.126142	34.076544
913.277101	73689.866690	34.081562
914.288763	73830.271712	34.086580
915.687184	73958.616459	34.091597
916.467153	74089.246455	34.096615
917.544920	74217.095728	34.101632
918.640816	74340.863565	34.106650
919.190461	74481.090144	34.111668
919.953256	74600.468716	34.116685
920.996783	74738.610153	34.121703
921.917444	74869.044368	34.126720
922.602566	74997.583151	34.131738
923.286989	75142.395815	34.136756
924.206780	75271.289375	34.141773
924.850326	75428.418318	34.146791
925.917713	75560.400787	34.151808
927.191190	75695.379371	34.156826
927.805204	75836.274322	34.161844
929.054795	75979.291017	34.166861
930.046753	76111.289299	34.171879
931.050526	76253.735057	34.176896
932.228437	76383.876225	34.181914
932.742301	76513.717238	34.186932
934.566637	76638.717992	34.191949
935.899680	76764.572632	34.196967
936.668908	76888.586093	34.201984
938.110717	77011.546196	34.207002
938.438206	77139.442053	34.212020
939.778915	77258.536689	34.217037
940.295434	77385.036358	34.222055
941.011374	77515.210223	34.227072
942.327311	77629.440546	34.232090
943.046502	77756.946031	34.237108
943.830718	77874.959812	34.242125
944.934991	78006.501621	34.247143
945.668412	78136.802717	34.252160
946.831096	78251.599315	34.257178
947.440738	78394.604918	34.262196
948.578381	78520.141353	34.267213
949.687218	78639.376721	34.272231
951.006835	78755.509849	34.277248
952.331568	78868.233238	34.282266
952.636654	78983.049387	34.287284
954.141205	79084.674186	34.292301
954.834987	79188.154573	34.297319
955.364713	79308.659848	34.302336
956.128960	79407.068977	34.307354
957.120022	79536.373933	34.312372
957.745188	79655.606395	34.317389
958.614475	79769.909100	34.322407
959.240668	79892.077833	34.327424
960.714234	80008.400639	34.332442
961.779755	80133.028136	34.337460
963.120798	80256.250514	34.342477
963.628778	80387.652170	34.347495
964.128669	80508.573661	34.352512
964.929995	80636.543644	34.357530
965.499600	80781.399267	34.362548
966.481345	80915.629054	34.367565
967.245047	81062.832899	34.372583
968.213460	81212.635446	34.377600
969.313779	81353.484374	34.382618
970.189186	81496.731213	34.387636
971.469058	81650.774207	34.392653
972.516754	81802.206002	34.397671
972.720010	81947.269010	34.402688
974.062013	82093.206824	34.407706
975.223506	82240.567361	34.412724
976.444900	82384.945418	34.417741
977.822722	82522.465691	34.422759
978.527901	82669.227759	34.427776
979.913671	82809.949722	34.432794
980.470302	82963.666044	34.437812
981.654059	83089.700948	34.442829
983.561770	83234.995406	34.447847
984.463016	83369.493374	34.452864
985.637393	83495.532059	34.457882
986.368801	83636.563796	34.462900
987.076734	83771.849090	34.467917
988.102660	83910.467349	34.472935
988.620541	84069.290696	34.477952
989.473741	84212.887167	34.482970
990.353651	84371.760075	34.487988
991.264849	84516.228271	34.493005
992.255459	84675.565754	34.498023
992.542694	84847.365493	34.503040
993.588153	85009.302986	34.508058
994.153191	85178.717977	34.513076
995.118428	85337.608635	34.518093
995.726181	85515.352140	34.523111
996.565704	85706.966330	34.528128
998.161925	85879.379037	34.533146
999.623906	86041.697509	34.538164
1000.868175	86205.540221	34.543181
1002.282859	86365.236499	34.548199
1002.949538	86535.758122	34.553216
1004.407321	86683.363509	34.558234
1005.187734	86850.888181	34.563252
1006.006371	87019.451795	34.568269
1007.038296	87177.375706	34.573287
1008.179379	87345.641364	34.578304
1009.151268	87509.013140	34.583322
1010.558214	87659.088330	34.588340
1011.811057	87822.896588	34.593357
1013.031055	87962.316658	34.598375
1013.874069	88116.759782	34.603392
1014.926579	88274.175030	34.608410
1015.664692	88423.220646	34.613428
1016.112849	88597.982687	34.618445
1017.764540	88748.821532	34.623463
1018.301272	88912.578945	34.628480
1019.341655	89058.300308	34.633498
1020.196760	89223.797963	34.638516
1021.166935	89371.146634	34.643533
1022.619130	89514.992519	34.648551
1023.313959	89685.304308	34.653568
1024.483894	89824.306928	34.658586
1025.051641	89972.833581	34.663604
1026.089442	90138.560396	34.668621
1027.204784	90286.137432	34.673639
1028.604304	90449.483745	34.678656
1029.929617	90590.072524	34.683674
1031.121182	90736.430883	34.688692
1032.127352	90882.700646	34.693709
1033.421765	91039.872460	34.698727
1034.060242	91192.635272	34.703744
1035.147367	91338.837409	34.708762
1036.443613	91489.106934	34.713780
1036.742493	91655.606022	34.718797
1037.837518	91816.784293	34.723815
1038.710045	91988.576553	34.728832
1039.447518	92144.468200	34.733850
1040.586376	92315.047680	34.738868
1041.155527	92501.122013	34.743885
1042.213057	92671.578243	34.748903
1042.689765	92869.234398	34.753920
1043.633114	93057.776311	34.758938
1044.506874	93241.375250	34.763956
1044.998113	93449.553268	34.768973
1046.179109	93657.776849	34.773991
1047.073484	93858.232662	34.779008
1048.240066	94060.923632	34.784026
1049.234548	94274.114209	34.789044
1050.132561	94488.316416	34.794061
1051.592475	94692.356472	34.799079
1052.711589	94894.441854	34.804096
1055.144321	95080.574695	34.809114
1057.744345	95236.816308	34.814132
1059.591650	95401.697682	34.819149
1060.703439	95554.402871	34.824167
1061.616491	95712.117435	34.829184
1062.879664	95858.367993	34.834202
1064.434258	96003.748140	34.839220
1065.974321	96133.192071	34.844237
1067.616557	96265.689895	34.849255
1068.511232	96393.305204	34.854272
1069.945157	96507.512731	34.859290
1071.424974	96638.260671	34.864308
1072.455222	96746.383178	34.869325
1073.761643	96864.259787	34.874343
1074.813154	96969.353804	34.879360
1076.056359	97084.646468	34.884378
1077.038478	97186.575025	34.889396
1077.021329	97317.327993	34.894413
1077.875996	97434.813784	34.899431
1078.580731	97586.851955	34.904448
1079.039205	97717.629384	34.909466
1080.045539	97854.533293	34.914484
1080.393377	98010.001138	34.919501
1080.938354	98174.787716	34.924519
1081.437036	98342.735774	34.929536
1082.386126	98506.140669	34.934554
1084.139295	98665.380466	34.939572
1084.861041	98842.335290	34.944589
1085.605534	99011.753761	34.949607
1086.908568	99193.590714	34.954624
1087.982522	99363.545656	34.959642
1089.490756	99537.886756	34.964660
1090.258695	99696.340498	34.969677
1092.013051	99836.290251	34.974695
1093.315085	99988.313399	34.979712
1094.192148	100131.310003	34.984730
1095.614020	100277.287677	34.989748
1096.697269	100435.978611	34.994765
1097.840909	100583.637669	34.999783
1098.720954	100729.049358	35.004800
1099.759387	100882.432152	35.009818
1101.147119	101037.581368	35.014836
1101.798959	101190.283030	35.019853
1102.456913	101353.437915	35.024871
1103.488349	101520.989288	35.029888
1104.259350	101689.503039	35.034906
1105.461383	101855.844278	35.039924
1106.109769	102042.178919	35.044941
1107.077217	102214.639805	35.049959
1107.892182	102394.149070	35.054976
1109.909312	102568.312374	35.059994
1112.215917	102711.687684	35.065012
1113.200010	102879.186065	35.070029
1114.731405	103044.144272	35.075047
1115.686246	103205.336675	35.080064
1117.162765	103354.577350	35.085082
1118.362099	103513.464242	35.090100
1119.322429	103656.118307	35.095117
1120.618259	103812.128910	35.100135
1121.617739	103973.951870	35.105152
1122.478191	104144.056077	35.110170
1123.454534	104297.513712	35.115188
1123.970708	104477.112223	35.120205
1124.773850	104640.377633	35.125223
1125.750125	104834.035984	35.130240
1126.935285	105008.093972	35.135258
1128.478024	105175.153429	35.140276
1128.892512	105369.706803	35.145293
1130.070709	105554.674103	35.150311
1131.245967	105747.153625	35.155328
1131.894946	105945.041260	35.160346
1133.368271	106133.509916	35.165364
1134.140438	106328.238966	35.170381
1135.660163	106520.261658	35.175399
1136.924726	106729.236676	35.180416
1137.977106	106923.619620	35.185434
1139.113207	107107.312812	35.190452
1139.972266	107318.006266	35.195469
1140.756973	107515.034427	35.200487
1142.263482	107722.216499	35.205504
1143.187909	107931.130674	35.210522
1144.248664	108140.391179	35.215540
1145.271724	108349.862227	35.220557
1146.229113	108561.131773	35.225575
1147.656147	108765.447104	35.230592
1148.845163	108989.246833	35.235610
1150.167758	109189.592687	35.240628
1151.175682	109410.360575	35.245645
1152.515162	109620.827661	35.250663
1153.584174	109826.983768	35.255680
1155.147372	110041.546469	35.260698
1156.333496	110234.069010	35.265716
1157.536149	110450.062801	35.270733
1158.564715	110646.769288	35.275751
1159.899187	110848.974832	35.280768
1160.718450	111065.809803	35.285786
1162.040150	111266.234402	35.290804
1163.736460	111454.741224	35.295821
1165.583008	111634.749576	35.300839
1167.445230	111814.452475	35.305856
1168.216358	112003.027850	35.310874
1170.040618	112151.626435	35.315892
1171.502346	112319.440323	35.320909
1172.561086	112476.592021	35.325927
1173.940697	112621.099019	35.330944
1174.624983	112787.613183	35.335962
1175.812441	112943.555341	35.340980
1176.626075	113113.660529	35.345997
1177.419863	113267.579488	35.351015
1178.758235	113432.785488	35.356032
1179.927085	113598.692035	35.361050
1180.982394	113760.893749	35.366068
1181.555044	113950.440088	35.371085
1182.463381	114133.052727	35.376103
1183.756650	114329.944172	35.381120
1184.719074	114520.189854	35.386138
1185.660565	114710.972408	35.391156
1186.510421	114923.702200	35.396173
1187.090049	115135.186132	35.401191
1188.493518	115346.142230	35.406208
1189.356527	115573.368762	35.411226
1190.610643	115777.397183	35.416244
1192.244679	115984.734242	35.421261
1193.444176	116192.094216	35.426279
1194.716350	116399.126895	35.431296
1196.367553	116615.081355	35.436314
1198.013322	116824.221750	35.441332
1198.863347	117041.300611	35.446349
1199.887644	117241.158411	35.451367
1201.158736	117452.962995	35.456384
1201.783863	117680.929986	35.461402
1202.986176	117894.168342	35.466420
1204.335159	118130.254799	35.471437
1205.062370	118358.260899	35.476455
1206.224740	118585.309642	35.481472
1207.444114	118815.417126	35.486490
1208.614090	119044.926411	35.491508
1210.246412	119273.689238	35.496525
1211.415117	119510.931931	35.501543
1212.974358	119744.373671	35.506560
1214.481472	119962.670646	35.511578
1216.143055	120167.967782	35.516596
1217.214616	120383.818475	35.521613
1218.300455	120610.046684	35.526631
1220.235872	120814.491927	35.531648
1221.804739	121023.624707	35.536666
1223.140188	121232.126064	35.541684
1224.634550	121434.291746	35.546701
1225.813452	121651.211073	35.551719
1227.343764	121832.793610	35.556736
1228.439566	122031.772668	35.561754
1230.050523	122210.708259	35.566772
1231.830431	122421.133871	35.571789
1232.565996	122600.698572	35.576807
1233.969467	122795.551080	35.581824
1235.593116	122979.887828	35.586842
1236.806821	123154.396094	35.591860
1237.785907	123345.127815	35.596877
1238.773390	123526.354486	35.601895
1240.561517	123703.710850	35.606912
1241.773440	123883.064830	35.611930
1242.890753	124075.603222	35.616948
1244.069224	124257.626395	35.621965
1244.737161	124453.929717	35.626983
1245.644120	124639.244652	35.632000
1246.349237	124852.298930	35.637018
1247.207799	125057.218020	35.642036
1248.282269	125271.341946	35.647053
1248.655156	125496.014432	35.652071
1250.156776	125698.486497	35.657088
1250.953930	125925.094276	35.662106
1251.543052	126140.039904	35.667124
1252.770046	126375.312284	35.672141
1253.465238	126602.981287	35.677159
1255.028013	126820.279731	35.682176
1256.988441	127049.313829	35.687194
1258.093330	127284.765518	35.692212
1259.564085	127513.694164	35.697229
1260.344031	127757.074406	35.702247
1261.182587	127993.082656	35.707264
1262.165796	128239.994651	35.712282
1262.983255	128496.594609	35.717300
1265.187096	128728.085093	35.722317
1266.846984	128987.274557	35.727335
1268.097403	129219.585938	35.732352
1268.924025	129476.876900	35.737370
1270.108568	129732.095166	35.742388
1272.009642	129971.542030	35.747405
1273.532560	130220.889939	35.752423
1275.301570	130460.577910	35.757440
1276.781340	130699.136792	35.762458
1278.464867	130935.305903	35.767476
1279.820423	131162.911289	35.772493
1280.791620	131396.375156	35.777511
1282.262653	131624.509772	35.782528
1283.830835	131859.754136	35.787546
1285.099909	132089.941144	35.792564
1286.646128	132328.742061	35.797581
1287.384104	132560.858659	35.802599
1288.960098	132794.460593	35.807616
1289.888082	133037.413245	35.812634
1291.010521	133275.873126	35.817652
1292.538165	133506.648555	35.822669
1294.274426	133747.038457	35.827687
1295.632356	133980.178026	35.832704
1296.723560	134220.538961	35.837722
1298.691471	134441.638475	35.842740
1300.261724	134660.612204	35.847757
1301.670728	134891.315703	35.852775
1303.444897	135110.537533	35.857792
1304.316887	135327.666458	35.862810
1305.804081	135557.753132	35.867828
1307.181547	135775.016702	35.872845
1308.201101	135997.209479	35.877863
1309.540363	136216.384013	35.882880
1310.290692	136452.925576	35.887898
1311.338627	136685.032726	35.892916
1312.929324	136922.427176	35.897933
1314.125804	137151.292594	35.902951
1315.226758	137383.598672	35.907968
1316.682571	137622.402447	35.912986
1318.431249	137847.859207	35.918004
1319.937147	138070.771237	35.923021
1320.964286	138306.810883	35.928039
1322.968911	138520.514264	35.933056
1324.940647	138733.210117	35.938074
1326.250713	138947.259611	35.943092
1327.841811	139155.317226	35.948109
1328.911323	139372.743972	35.953127
1330.060800	139571.989083	35.958144
1331.006262	139783.505007	35.963162
1331.947042	140022.347740	35.968180
1333.221499	140247.189049	35.973197
1333.955791	140470.029236	35.978215
1335.117389	140710.602642	35.983232
1336.017250	140949.851692	35.988250
1336.809229	141205.858055	35.993268
1337.833945	141440.220627	35.998285
1338.804767	141697.342184	36.003303
1340.238655	141942.038144	36.008320
1341.494382	142199.547303	36.013338
1342.309499	142446.872841	36.018356
1343.492909	142709.241733	36.023373
1344.709434	142978.277184	36.028391
1345.974714	143240.395539	36.033408
1347.030760	143512.150033	36.038426
1348.329805	143783.980452	36.043444
1350.073376	144064.222940	36.048461
1351.165378	144349.610158	36.053479
1352.101324	144637.409643	36.058496
1353.211468	144927.921762	36.063514
1354.311247	145220.669919	36.068532
1355.932916	145525.673196	36.073549
1357.032077	145828.381537	36.078567
1358.508261	146136.901617	36.083584
1359.810379	146444.134271	36.088602
1360.980425	146754.917061	36.093620
1362.421118	147066.545385	36.098637
1363.854625	147382.261279	36.103655
1365.248600	147695.044132	36.108672
1367.240926	148008.732356	36.113690
1368.117104	148334.847114	36.118708
1369.906493	148641.243812	36.123725
1371.054122	148964.452818	36.128743
1372.561901	149276.304382	36.133760
1374.085680	149594.522823	36.138778
1375.348921	149923.238143	36.143796
1377.290447	150227.009958	36.148813
1378.270070	150560.343896	36.153831
1379.686165	150881.419540	36.158848
1381.459871	151201.043418	36.163866
1383.811727	151490.551729	36.168884
1385.655611	151795.684177	36.173901
1387.436763	152084.467208	36.178919
1389.318739	152367.439111	36.183936
1391.157441	152657.726338	36.188954
1392.387252	152942.675204	36.193972
1394.072606	153210.058990	36.198989
1395.495250	153482.194104	36.204007
1397.147260	153760.089909	36.209024
1398.647173	154036.110244	36.214042
1399.748782	154298.626003	36.219060
1401.459742	154569.173410	36.224077
1402.654689	154837.233237	36.229095
1404.083285	155104.013035	36.234112
1406.131762	155363.385298	36.239130
1407.707285	155617.484593	36.244148
1410.080411	155848.975166	36.249165
1411.602451	156091.111594	36.254183
1412.862952	156341.233877	36.259200
1414.423953	156581.793863	36.264218
1415.684868	156825.627172	36.269236
1416.928347	157068.513446	36.274253
1417.751905	157310.899971	36.279271
1419.670992	157535.663474	36.284288
1422.071652	157768.035959	36.289306
1423.482816	157997.275541	36.294324
1424.938210	158226.813553	36.299341
1426.623938	158441.598940	36.304359
1428.141006	158656.996989	36.309376
1429.237918	158873.899378	36.314394
1431.062785	159083.438412	36.319412
1432.767339	159291.564927	36.324429
1434.097540	159513.455788	36.329447
1435.309901	159720.854174	36.334464
1436.788254	159914.013381	36.339482
1437.881491	160116.828342	36.344500
1439.002237	160316.924815	36.349517
1440.233343	160521.761442	36.354535
1441.507353	160717.102330	36.359552
1443.348274	160922.778643	36.364570
1444.339120	161124.841629	36.369588
1445.340574	161339.032482	36.374605
1446.319487	161563.694894	36.379623
1447.453459	161795.653206	36.384640
1448.511648	162026.635773	36.389658
1449.496002	162271.359347	36.394676
1450.473739	162520.817773	36.399693
1451.450844	162790.120720	36.404711
1452.107738	163063.195874	36.409728
1452.806822	163355.639557	36.414746
1454.000013	163658.584746	36.419764
1455.073897	163960.638350	36.424781
1456.268951	164273.242881	36.429799
1457.577730	164596.513985	36.434816
1458.751323	164910.585792	36.439834
1459.550733	165246.253499	36.444852
1461.024543	165593.497745	36.449869
1462.035528	165925.722492	36.454887
1463.534760	166292.482568	36.459904
1464.935028	166642.386484	36.464922
1466.390250	167008.969488	36.469940
1467.704008	167368.384514	36.474957
1469.356706	167736.298458	36.479975
1470.992690	168103.621825	36.484992
1472.865962	168461.024160	36.490010
1474.524778	168837.193931	36.495028
1476.071393	169202.739225	36.500045
1478.175675	169570.821675	36.505063
1480.273436	169901.436499	36.510080
1482.700123	170233.458462	36.515098
1484.548737	170577.443387	36.520116
1486.170311	170905.657236	36.525133
1487.917885	171234.423557	36.530151
1489.197323	171578.916355	36.535168
1490.875183	171903.790495	36.540186
1492.288612	172232.492346	36.545204
1493.223083	172567.582870	36.550221
1495.702283	172875.478441	36.555239
1498.483380	173179.924977	36.560256
1501.077565	173460.267461	36.565274
1502.899789	173772.770144	36.570292
1504.684252	174038.478641	36.575309
1506.935747	174323.413500	36.580327
1508.817423	174570.732913	36.585344
1511.399773	174811.541329	36.590362
1512.826636	175067.048026	36.595380
1514.068952	175308.728299	36.600397
1515.484551	175540.926347	36.605415
1516.944768	175789.464015	36.610432
1518.303204	176023.869360	36.615450
1518.974106	176286.817768	36.620468
1520.139728	176538.200090	36.625485
1521.426784	176805.034116	36.630503
1522.364857	177081.344346	36.635520
1523.571869	177345.910114	36.640538
1524.307251	177636.712443	36.645556
1525.233788	177920.250625	36.650573
1526.591509	178229.343153	36.655591
1527.427949	178537.445203	36.660608
1528.807854	178847.070870	36.665626
1530.254080	179159.847677	36.670644
1532.174602	179463.993453	36.675661
1534.412954	179733.718599	36.680679
1535.344149	180037.384493	36.685696
1537.027877	180316.622097	36.690714
1538.657056	180622.891811	36.695732
1539.768275	180910.185488	36.700749
1541.094453	181210.112004	36.705767
1542.574856	181510.433514	36.710784
1544.201738	181813.930943	36.715802
1545.238154	182135.475202	36.720820
1546.542362	182447.394112	36.725837
1548.052678	182776.936162	36.730855
1548.937807	183110.125153	36.735872
1550.432125	183450.729363	36.740890
1552.040191	183781.911426	36.745908
1553.396315	184137.304698	36.750925
1554.813664	184469.791858	36.755943
1556.552513	184818.601880	36.760960
1559.047105	185156.258425	36.765978
1560.533125	185485.528952	36.770996
1561.974363	185836.501815	36.776013
1563.682274	186171.642029	36.781031
1564.983795	186532.302126	36.786048
1566.641754	186875.147090	36.791066
1568.305215	187227.005728	36.796084
1569.490457	187582.309663	36.801101
1570.724319	187936.021012	36.806119
1571.736484	188308.494816	36.811136
1573.702188	188680.140167	36.816154
1575.237434	189058.967938	36.821172
1576.717008	189429.860846	36.826189
1578.814253	189788.505314	36.831207
1580.476012	190159.804222	36.836224
1582.904974	190523.374329	36.841242
1584.459888	190889.719298	36.846260
1585.799645	191245.527607	36.851277
1587.740588	191608.321959	36.856295
1589.243655	191982.730551	36.861312
1590.922747	192339.491907	36.866330
1592.681562	192693.296917	36.871348
1595.165501	193045.181079	36.876365
1596.617264	193389.443612	36.881383
1598.326093	193751.324271	36.886400
1600.074999	194096.125414	36.891418
1601.632853	194455.978546	36.896436
1603.034613	194809.664299	36.901453
1604.931101	195150.815871	36.906471
1606.988095	195487.905514	36.911488
1608.821873	195826.151125	36.916506
1610.327467	196169.785035	36.921524
1612.041170	196498.405439	36.926541
1613.830699	196835.495637	36.931559
1615.294761	197180.716004	36.936576
1616.513653	197528.644932	36.941594
1617.940387	197868.961789	36.946612
1618.990382	198238.188003	36.951629
1620.450185	198587.694885	36.956647
1621.617005	198966.795909	36.961664
1622.470486	199322.666242	36.966682
1624.143816	199705.128057	36.971700
1625.324360	200087.889512	36.976717
1627.227478	200469.022438	36.981735
1628.687212	200857.848791	36.986752
1629.959818	201242.175661	36.991770
1631.525070	201636.968864	36.996788
1633.165397	202034.468887	37.001805
1635.508165	202425.836440	37.006823
1636.854668	202831.413879	37.011840
1638.517874	203211.674360	37.016858
1640.267836	203588.608539	37.021876
1641.898647	203941.986119	37.026893
1643.765147	204303.719050	37.031911
1645.513550	204676.722927	37.036928
1647.069974	205045.519623	37.041946
1649.237584	205390.231771	37.046964
1650.990530	205764.014775	37.051981
1652.760967	206123.270947	37.056999
1654.092371	206495.095790	37.062016
1655.950880	206860.575195	37.067034
1657.536231	207220.501975	37.072052
1658.959240	207606.360344	37.077069
1660.662128	207973.622953	37.082087
1662.308549	208344.363071	37.087104
1664.817950	208690.886931	37.092122
1667.099398	209057.944298	37.097140
1668.427162	209426.812099	37.102157
1670.304600	209784.644840	37.107175
1671.642572	210149.234967	37.112192
1673.366207	210505.763005	37.117210
1675.341549	210874.161625	37.122228
1677.112833	211232.437157	37.127245
1679.391646	211594.007785	37.132263
1680.763945	211952.606409	37.137280
1682.273618	212308.948843	37.142298
1683.816304	212669.909447	37.147316
1685.443046	213049.041691	37.152333
1687.432793	213404.877229	37.157351
1689.447533	213756.748106	37.162368
1690.978018	214122.440434	37.167386
1692.920952	214484.688042	37.172404
1694.398523	214860.550961	37.177421
1695.791791	215222.638589	37.182439
1697.065579	215607.757547	37.187456
1698.063311	215987.971296	37.192474
1699.716896	216377.144841	37.197492
1701.057989	216767.413062	37.202509
1703.760481	217137.113504	37.207527
1706.170634	217502.215963	37.212544
1708.448131	217874.300834	37.217562
1710.580589	218239.375838	37.222580
1712.054244	218677.733799	37.227597
1714.015412	219036.744483	37.232615
1715.832548	219396.212069	37.237632
1717.100555	219757.194230	37.242650
1719.591002	220107.688595	37.247668
1720.873880	220473.445700	37.252685
1722.291881	220835.778227	37.257703
1723.978820	221214.373500	37.262720
1725.170512	221591.198043	37.267738
1726.729426	221967.277248	37.272756
1727.937125	222356.877492	37.277773
1729.343002	222739.766245	37.282791
1730.770784	223144.318300	37.287808
1732.244773	223550.591289	37.292826
1734.149139	223944.882006	37.297844
1735.529898	224361.663278	37.302861
1737.006030	224768.168733	37.307879
1738.540783	225197.195458	37.312896
1739.912575	225611.544181	37.317914
1742.156050	226026.359440	37.322932
1744.103064	226446.457622	37.327949
1745.977895	226870.277584	37.332967
1747.326389	227297.208804	37.337984
1749.002600	227717.051240	37.343002
1751.038479	228131.882343	37.348020
1752.646935	228563.143463	37.353037
1754.663195	228974.525967	37.358055
1756.597288	229383.307063	37.363072
1758.114265	229775.978258	37.368090
1760.064415	230170.179012	37.373108
1761.622109	230584.182331	37.378125
1763.095309	230977.219702	37.383143
1764.927385	231391.611661	37.388160
1766.475742	231801.479608	37.393178
1768.046587	232219.752702	37.398196
1769.682045	232640.810358	37.403213
1771.363467	233056.959096	37.408231
1773.752245	233475.582640	37.413248
1775.692881	233881.834869	37.418266
1777.903627	234303.741428	37.423284
1779.753110	234715.472122	37.428301
1781.656857	235130.116004	37.433319
1783.896661	235542.139633	37.438336
1785.292798	235955.040685	37.443354
1787.951687	236343.678003	37.448372
1789.818993	236746.697728	37.453389
1792.150680	237145.678692	37.458407
1794.766890	237529.321418	37.463424
1796.057183	237912.625786	37.468442
1797.791989	238297.914808	37.473460
1799.579362	238703.619106	37.478477
1801.241937	239097.177294	37.483495
1802.875053	239499.098415	37.488512
1804.187781	239907.169916	37.493530
1805.824827	240319.430620	37.498548
1807.721489	240730.353558	37.503565
1810.201743	241122.738454	37.508583
1811.834651	241527.228942	37.513600
1813.722675	241932.465325	37.518618
1815.563158	242338.650156	37.523636
1817.979458	242741.539526	37.528653
1819.829744	243134.565533	37.533671
1821.746272	243539.139328	37.538688
1823.960684	243928.244993	37.543706
1826.107319	244302.578103	37.548724
1827.661252	244709.855586	37.553741
1829.426259	245089.587529	37.558759
1830.992080	245491.681975	37.563776
1832.660646	245891.295856	37.568794
1834.253091	246301.160188	37.573812
1835.593519	246714.013523	37.578829
1837.256421	247127.779240	37.583847
1838.645112	247546.976299	37.588864
1840.364992	247979.353894	37.593882
1842.233999	248403.400508	37.598900
1843.622931	248853.260355	37.603917
1845.345630	249283.759100	37.608935
1846.968495	249726.747713	37.613952
1848.613394	250189.014040	37.618970
1850.962487	250622.077601	37.623988
1853.449314	251052.908648	37.629005
1855.986267	251458.785872	37.634023
1858.430801	251896.076997	37.639040
1859.568447	252331.501928	37.644058
1861.288661	252749.480260	37.649076
1863.976364	253178.907811	37.654093
1865.725112	253597.694828	37.659111
1867.362065	254023.283254	37.664128
1868.961730	254456.143398	37.669146
1870.672972	254886.241705	37.674164
1872.007796	255333.244918	37.679181
1873.513700	255783.166737	37.684199
1875.226139	256235.671023	37.689216
1876.634967	256676.133782	37.694234
1878.262303	257128.754017	37.699252
1879.742706	257568.265180	37.704269
1881.400333	258026.316848	37.709287
1883.342039	258471.238792	37.714304
1884.820066	258925.560588	37.719322
1887.448893	259367.752162	37.724340
1889.387809	259802.462433	37.729357
1891.393019	260258.398826	37.734375
1893.525204	260694.245514	37.739392
1895.870003	261145.425874	37.744410
1897.804037	261579.806402	37.749428
1899.542264	262028.064024	37.754445
1901.351863	262489.239921	37.759463
1903.060125	262941.769911	37.764480
1904.468867	263395.365448	37.769498
1906.613901	263861.921425	37.774516
1908.474677	264327.838344	37.779533
1910.204168	264800.152920	37.784551
1912.116178	265275.155071	37.789568
1914.069890	265756.830985	37.794586
1915.488582	266236.740717	37.799604
1917.305725	266726.262600	37.804621
1918.912145	267223.084212	37.809639
1921.176297	267707.196434	37.814656
1922.591831	268215.835643	37.819674
1924.812424	268718.752223	37.824692
1927.180415	269209.297933	37.829709
1929.250960	269712.974818	37.834727
1931.643703	270199.984156	37.839744
1933.581228	270695.552806	37.844762
1936.011036	271184.637674	37.849780
1937.653475	271679.059834	37.854797
1939.693626	272185.684860	37.859815
1941.690100	272679.843558	37.864832
1943.953556	273174.262030	37.869850
1946.279371	273653.224524	37.874868
1948.485625	274143.586344	37.879885
1949.976545	274639.146273	37.884903
1952.214292	275122.083513	37.889920
1953.906373	275624.136634	37.894938
1955.897556	276126.164570	37.899956
1957.658266	276620.507317	37.904973
1959.829260	277129.057099	37.909991
1961.220702	277618.886435	37.915008
1962.821248	278138.603745	37.920026
1964.646766	278640.145429	37.925044
1966.590900	279171.056370	37.930061
1967.960204	279693.957914	37.935079
1970.194869	280211.685135	37.940096
1972.518029	280749.590727	37.945114
1974.839057	281267.859583	37.950132
1976.908395	281790.639350	37.955149
1978.722391	282308.963800	37.960167
1980.879160	282831.014747	37.965184
1982.826044	283359.042795	37.970202
1984.882291	283880.548309	37.975220
1987.086597	284397.506202	37.980237
1989.396288	284913.962344	37.985255
1992.192180	285407.297445	37.990272
1994.378469	285921.001956	37.995290
1996.072805	286423.076382	38.000308
1998.123038	286934.793271	38.005325
2000.011947	287435.790565	38.010343
2001.929327	287940.032669	38.015360
2003.717348	288451.965361	38.020378
2005.471834	288967.838781	38.025396
2007.868449	289475.602750	38.030413
2009.001770	290002.344853	38.035431
2011.071324	290506.221996	38.040448
2013.093826	290996.084123	38.045466
2014.735707	291493.068602	38.050484
2016.708513	291982.122327	38.055501
2018.170111	292495.413976	38.060519
2020.249607	293006.848524	38.065536
2022.217640	293524.293642	38.070554
2023.680981	294040.118322	38.075572
2025.629002	294556.647803	38.080589
2027.110434	295094.130387	38.085607
2029.361104	295634.734071	38.090624
2031.258755	296175.876175	38.095642
2033.044578	296725.720526	38.100660
2035.332999	297269.611720	38.105677
2037.276294	297818.992590	38.110695
2039.321660	298363.299383	38.115712
2041.679089	298916.618811	38.120730
2043.749012	299478.516638	38.125748
2046.211691	300024.040738	38.130765
2048.110167	300590.456150	38.135783
2050.481134	301139.011610	38.140800
2052.634921	301697.555777	38.145818
2054.622186	302240.073072	38.150836
2057.094842	302790.684767	38.155853
2059.153880	303357.260313	38.160871
2061.869091	303901.399731	38.165888
2064.601109	304443.856905	38.170906
2067.177361	304982.374711	38.175924
2069.265589	305508.779741	38.180941
2071.209046	306049.706906	38.185959
2073.557580	306574.792550	38.190976
2075.935536	307111.196734	38.195994
2078.164998	307642.568329	38.201012
2080.555233	308170.887827	38.206029
2082.317557	308702.025277	38.211047
2084.256275	309210.502763	38.216064
2086.593067	309738.592437	38.221082
2088.271356	310281.059727	38.226100
2090.684726	310807.732911	38.231117
2092.563137	311338.859058	38.236135
2094.254365	311879.941846	38.241152
2095.964604	312416.446696	38.246170
2097.519124	312974.939527	38.251188
2099.497564	313521.143499	38.256205
2101.650614	314085.369550	38.261223
2103.479754	314653.200044	38.266240
2105.185237	315227.420354	38.271258
2107.232671	315798.862401	38.276276
2109.627313	316366.154112	38.281293
2112.388984	316943.766152	38.286311
2115.054916	317502.471819	38.291328
2117.300428	318057.916224	38.296346
2119.303527	318621.115523	38.301364
2121.384709	319172.515368	38.306381
2123.368835	319751.730769	38.311399
2125.667071	320309.687206	38.316416
2127.696290	320877.459166	38.321434
2129.665960	321446.657989	38.326452
2131.837304	322005.509742	38.331469
2133.814180	322580.258030	38.336487
2135.612983	323156.579465	38.341504
2137.735392	323751.808546	38.346522
2138.987017	324331.155143	38.351540
2140.661560	324929.773276	38.356557
2142.304025	325540.044679	38.361575
2144.277711	326156.170825	38.366592
2146.459917	326766.772163	38.371610
2148.069751	327391.832077	38.376628
2150.671485	327989.809437	38.381645
2153.151767	328600.291823	38.386663
2155.385443	329179.353068	38.391680
2157.429443	329769.229693	38.396698
2159.030877	330367.779883	38.401716
2161.196054	330966.230432	38.406733
2162.788274	331576.193612	38.411751
2164.561300	332196.706412	38.416768
2166.319622	332819.245625	38.421786
2168.146278	333456.845766	38.426804
2170.568931	334098.782265	38.431821
2172.807393	334745.184103	38.436839
2174.483604	335392.102820	38.441856
2176.519380	336044.437246	38.446874
2178.499662	336711.394242	38.451892
2181.275092	337375.596505	38.456909
2183.687688	338034.062852	38.461927
2186.435498	338686.855522	38.466944
2190.060697	339311.268493	38.471962
2193.184510	339951.113409	38.476980
2195.948222	340569.840795	38.481997
2198.108639	341199.244786	38.487015
2200.852133	341809.253993	38.492032
2203.513964	342427.518157	38.497050
2205.373106	343045.780496	38.502068
2207.616899	343653.996545	38.507085
2209.753887	344276.334194	38.512103
2211.833581	344876.668525	38.517120
2214.152944	345493.376384	38.522138
2216.181306	346107.916320	38.527156
2218.306315	346743.852266	38.532173
2220.200509	347376.315422	38.537191
2221.680588	348008.939977	38.542208
2223.944245	348646.476291	38.547226
2225.960347	349295.160138	38.552244
2227.926631	349956.582386	38.557261
2230.035728	350617.971207	38.562279
2231.568491	351284.597083	38.567296
2233.248973	351959.968629	38.572314
2235.434214	352646.081693	38.577332
2238.120231	353328.015542	38.582349
2240.265890	354018.528744	38.587367
2242.406284	354709.488426	38.592384
2245.119264	355396.789665	38.597402
2247.458771	356082.745985	38.602420
2249.765556	356774.430893	38.607437
2252.656377	357458.801655	38.612455
2254.851139	358146.397161	38.617472
2257.558515	358832.475422	38.622490
2260.091320	359502.130128	38.627508
2262.881821	360179.875285	38.632525
2264.812208	360860.136294	38.637543
2266.636656	361536.267866	38.642560
2269.233486	362200.158510	38.647578
2271.093353	362896.430145	38.652596
2273.519339	363559.590376	38.657613
2276.908597	364231.864764	38.662631
2279.052216	364897.129099	38.667648
2281.063320	365561.871123	38.672666
2283.723421	366254.651933	38.677684
2285.476875	366920.884174	38.682701
2287.382175	367594.055280	38.687719
2289.326789	368281.260558	38.692736
2291.317111	368967.887533	38.697754
2293.714047	369664.479006	38.702772
2295.578537	370360.029384	38.707789
2297.755349	371060.257890	38.712807
2299.518955	371758.486839	38.717824
2302.383998	372454.211862	38.722842
2304.730643	373135.983660	38.727860
2306.921342	373805.391488	38.732877
2309.418432	374474.862740	38.737895
2311.877738	375153.685796	38.742912
2314.382421	375799.113465	38.747930
2317.071774	376467.880735	38.752948
2319.282786	377133.468221	38.757965
2321.514042	377799.369147	38.762983
2323.952288	378478.536188	38.768000
2326.560230	379133.647303	38.773018
2328.481832	379827.225643	38.778036
2330.590170	380500.472983	38.783053
2332.824403	381165.546418	38.788071
2335.320257	381864.109500	38.793088
2337.649472	382546.762054	38.798106
2339.571381	383244.249912	38.803124
2341.523584	383947.574787	38.808141
2343.274376	384662.682063	38.813159
2345.551226	385384.024796	38.818176
2347.519294	386102.791111	38.823194
2349.814189	386842.301400	38.828212
2352.405507	387583.139746	38.833229
2354.970792	388328.198659	38.838247
2357.206745	389076.843485	38.843264
2359.182781	389829.290523	38.848282
2361.193831	390581.967019	38.853300
2363.362327	391352.774074	38.858317
2365.753151	392125.248622	38.863335
2367.340208	392912.462089	38.868352
2369.948179	393700.981566	38.873370
2372.184078	394503.431622	38.878388
2374.668812	395289.623326	38.883405
2377.171698	396085.143453	38.888423
2379.259147	396897.818162	38.893440
2381.838526	397696.982412	38.898458
2384.643430	398507.491660	38.903476
2387.427716	399323.556947	38.908493
2390.100713	400119.598120	38.913511
2392.193293	400934.845375	38.918528
2394.700885	401742.576148	38.923546
2397.262423	402554.531989	38.928564
2399.787778	403354.890905	38.933581
2402.976994	404157.042786	38.938599
2405.523686	404967.335109	38.943616
2408.609833	405751.240986	38.948634
2410.834038	406539.878347	38.953652
2413.645249	407326.977176	38.958669
2416.453420	408113.597838	38.963687
2419.114513	408887.680166	38.968704
2423.092334	409626.588888	38.973722
2427.558480	410329.399970	38.978740
2430.729553	411038.461125	38.983757
2434.262568	411743.036003	38.988775
2437.358907	412409.821674	38.993792
2440.076896	413084.479868	38.998810
2442.621875	413735.416528	39.003828
2445.302137	414380.590499	39.008845
2447.694085	415022.123771	39.013863
2449.398573	415678.875029	39.018880
2451.486142	416334.178599	39.023898
2453.516322	416978.686374	39.028916
2455.417851	417647.384401	39.033933
2457.391000	418318.990662	39.038951
2459.289113	418993.681067	39.043968
2461.431162	419664.160193	39.048986
2463.090494	420352.274900	39.054004
2464.777652	421051.532863	39.059021
2467.093490	421741.425178	39.064039
2469.133807	422439.496994	39.069056
2471.275449	423118.846791	39.074074
2472.988505	423807.084994	39.079092
2475.210707	424520.486823	39.084109
2477.636950	425220.010965	39.089127
2479.642176	425940.141564	39.094144
2481.601630	426657.321757	39.099162
2483.527014	427402.484464	39.104180
2485.724077	428154.818915	39.109197
2488.579459	428893.857893	39.114215
2490.244617	429656.813985	39.119232
2492.954468	430430.152871	39.124250
2495.026473	431223.213123	39.129268
2497.357757	432013.166521	39.134285
2500.182381	432806.301760	39.139303
2502.491313	433613.769121	39.144320
2504.959881	434416.322937	39.149338
2507.131199	435237.169217	39.154356
2509.291217	436061.935672	39.159373
2511.285578	436894.544178	39.164391
2513.594093	437735.622820	39.169408
2515.853035	438606.839129	39.174426
2519.684999	439433.432917	39.179444
2523.279763	440269.042526	39.184461
2527.114005	441080.192199	39.189479
2530.500595	441904.238143	39.194496
2533.351594	442704.966719	39.199514
2536.261410	443514.358597	39.204532
2538.336444	444323.555176	39.209549
2541.100409	445130.331160	39.214567
2543.237933	445949.372643	39.219584
2545.261303	446775.079404	39.224602
2548.215704	447594.631439	39.229620
2551.025182	448400.215318	39.234637
2553.744466	449233.198411	39.239655
2555.927674	450050.558172	39.244672
2558.450299	450878.855892	39.249690
2560.777472	451707.911991	39.254708
2563.147770	452550.633356	39.259725
2565.528958	453370.612678	39.264743
2567.717664	454227.759426	39.269760
2570.113446	455080.437108	39.274778
2572.166340	455947.901027	39.279796
2574.121881	456827.277034	39.284813
2576.582023	457710.677569	39.289831
2579.025774	458589.947226	39.294848
2581.702316	459483.902357	39.299866
2584.278590	460370.504156	39.304884
2586.923970	461259.582852	39.309901
2589.744654	462160.926823	39.314919
2592.499601	463064.565903	39.319936
2595.339784	463965.672912	39.324954
2598.014326	464852.007847	39.329972
2600.431944	465769.477575	39.334989
2603.229556	466668.850044	39.340007
2606.380806	467555.134879	39.345024
2609.051904	468448.330964	39.350042
2611.372421	469345.282854	39.355060
2614.038779	470253.100074	39.360077
2616.757746	471159.450690	39.365095
2619.389832	472066.126105	39.370112
2621.733196	472966.945456	39.375130
2624.017650	473866.468522	39.380148
2626.675570	474780.031038	39.385165
2629.443584	475689.186505	39.390183
2632.274647	476592.074257	39.395200
2635.425138	477487.036329	39.400218
2637.959113	478378.521553	39.405236
2640.540598	479256.521717	39.410253
2642.844008	480116.193855	39.415271
2645.981213	480987.807118	39.420288
2648.290364	481846.537973	39.425306
2651.412873	482698.529223	39.430324
2653.690910	483566.676133	39.435341
2656.570596	484420.645503	39.440359
2659.058633	485296.095606	39.445376
2661.390007	486159.715264	39.450394
2664.636343	487020.415411	39.455412
2666.796820	487883.322876	39.460429
2670.020374	488751.867366	39.465447
2673.011570	489627.625000	39.470464
2676.307250	490481.484532	39.475482
2679.816775	491329.715090	39.480500
2682.293115	492192.155211	39.485517
2685.412218	493043.696976	39.490535
2688.128577	493891.024372	39.495552
2690.622873	494745.764041	39.500570
2692.800930	495619.131654	39.505588
2694.861608	496497.821896	39.510605
2696.820511	497377.290569	39.515623
2699.520505	498273.743275	39.520640
2701.689961	499174.473349	39.525658
2704.454273	500081.462776	39.530676
2706.694104	500995.349491	39.535693
2709.790552	501903.142948	39.540711
2712.725168	502824.379416	39.545728
2715.778202	503744.082215	39.550746
2718.973417	504651.354761	39.555764
2721.748272	505574.984606	39.560781
2724.777916	506476.030992	39.565799
2727.485704	507402.038793	39.570816
2729.625027	508323.902878	39.575834
2732.185698	509253.710821	39.580852
2734.759896	510190.469843	39.585869
2737.243255	511141.706703	39.590887
2739.448017	512089.706785	39.595904
2741.773932	513055.019083	39.600922
2744.586684	514030.977327	39.605940
2747.009853	515006.989817	39.610957
2749.766153	515986.061132	39.615975
2752.853518	516965.520102	39.620992
2756.322363	517928.125675	39.626010
2760.039505	518888.312601	39.631028
2763.209888	519843.089012	39.636045
2766.595718	520804.722518	39.641063
2769.198537	521750.355613	39.646080
2771.664486	522703.407636	39.651098
2775.430023	523633.015422	39.656116
2778.629454	524574.948812	39.661133
2781.947097	525502.954195	39.666151
2785.356394	526419.858429	39.671168
2787.643675	527353.308085	39.676186
2790.478461	528265.309520	39.681204
2792.962047	529195.338223	39.686221
2795.035606	530119.586480	39.691239
2797.784852	531039.939642	39.696256
2800.473517	531982.344497	39.701274
2802.933832	532917.477970	39.706292
2805.235002	533856.302531	39.711309
2807.726228	534814.412212	39.716327
2810.865964	535767.620515	39.721344
2813.169263	536735.850345	39.726362
2815.523930	537692.583814	39.731380
2818.047124	538677.101060	39.736397
2820.348740	539656.354495	39.741415
2822.744696	540632.405714	39.746432
2825.052365	541601.814194	39.751450
2827.580944	542557.085066	39.756468
2830.225517	543547.984581	39.761485
2832.822011	544517.345660	39.766503
2835.562594	545517.696383	39.771520
2838.325823	546505.701016	39.776538
2841.499154	547495.025710	39.781556
2844.449929	548489.947936	39.786573
2847.046572	549501.498853	39.791591
2849.782661	550499.076456	39.796608
2852.742412	551507.754608	39.801626
2855.712905	552523.594709	39.806644
2858.606726	553553.445096	39.811661
2861.403495	554568.858998	39.816679
2864.268273	555599.311991	39.821696
2866.791869	556651.501192	39.826714
2869.867874	557691.607618	39.831732
2872.662773	558731.629117	39.836749
2875.292594	559792.998513	39.841767
2878.093811	560857.670424	39.846784
2880.574740	561927.935228	39.851802
2883.732908	562992.375335	39.856820
2886.489975	564085.974823	39.861837
2889.073520	565169.768792	39.866855
2892.432211	566254.750109	39.871872
2896.142466	567340.034163	39.876890
2898.849330	568419.819876	39.881908
2901.698541	569518.919429	39.886925
2904.601216	570614.602670	39.891943
2907.718419	571710.557784	39.896960
2910.280162	572824.979718	39.901978
2913.293392	573937.472360	39.906996
2915.524369	575064.096779	39.912013
2918.155150	576184.583117	39.917031
2920.946581	577310.461342	39.922048
2923.618292	578459.585047	39.927066
2926.335959	579610.350460	39.932084
2929.445338	580775.088301	39.937101
2932.315262	581947.980600	39.942119
2935.442613	583088.473412	39.947136
2938.579322	584256.737690	39.952154
2941.699383	585413.862319	39.957172
2945.046895	586581.768018	39.962189
2947.669549	587758.352950	39.967207
2951.062426	588917.603485	39.972224
2954.801471	590081.646487	39.977242
2958.474572	591222.835390	39.982260
2962.232579	592345.811535	39.987277
2965.199881	593491.509369	39.992295
2969.305129	594600.335430	39.997312
2972.903195	595701.576668	40.002330
2976.540997	596784.926030	40.007348
2980.175612	597870.980375	40.012365
2983.281786	598950.109779	40.017383
2986.848771	600010.935161	40.022400
2989.953896	601080.702567	40.027418
2992.982276	602115.036164	40.032436
2995.974475	603165.853480	40.037453
2998.800753	604209.443656	40.042471
3003.352421	605211.809550	40.047488
3006.696442	606222.094613	40.052506
3010.244532	607217.743090	40.057524
3013.451154	608214.211172	40.062541
3016.515566	609204.660536	40.067559
3019.444350	610175.532843	40.072576
3022.106519	611162.724171	40.077594
3024.542816	612152.016741	40.082612
3027.558221	613119.767954	40.087629
3029.938754	614062.132743	40.092647
3032.697092	615010.706263	40.097664
3035.454218	615957.148390	40.102682
3038.326812	616908.340328	40.107700
3041.235229	617859.544054	40.112717
3043.730084	618823.631752	40.117735
3046.176027	619794.240976	40.122752
3048.594494	620784.811795	40.127770
3051.048261	621782.983291	40.132788
3053.678689	622787.630275	40.137805
3056.380516	623816.757140	40.142823
3059.137067	624850.523308	40.147840
3061.344520	625905.613681	40.152858
3064.049853	626957.270699	40.157876
3067.173882	628036.577032	40.162893
3069.695302	629125.113320	40.167911
3072.630190	630206.228277	40.172928
3074.867533	631329.692508	40.177946
3077.938228	632459.539769	40.182964
3080.871776	633603.516420	40.187981
3083.627024	634749.793629	40.192999
3086.569482	635909.040996	40.198016
3089.374151	637075.418452	40.203034
3091.784570	638262.239304	40.208052
3094.860098	639464.930101	40.213069
3097.734674	640685.074755	40.218087
3100.905149	641893.951220	40.223104
3104.103146	643122.282132	40.228122
3107.035234	644354.797882	40.233140
3110.581580	645593.844173	40.238157
3113.458187	646839.231453	40.243175
3117.262209	648089.097482	40.248192
3120.395035	649321.023907	40.253210
3124.216679	650568.683791	40.258228
3127.576696	651811.529680	40.263245
3130.965373	653057.354667	40.268263
3134.732009	654286.220289	40.273280
3138.117804	655538.807943	40.278298
3141.361651	656772.481436	40.283316
3144.415680	658010.563237	40.288333
3147.395463	659245.164105	40.293351
3151.548030	660470.153546	40.298368
3154.867177	661709.115601	40.303386
3157.792445	662940.467658	40.308404
3161.457428	664171.241580	40.313421
3164.325590	665392.086330	40.318439
3167.163606	666633.380695	40.323456
3170.346973	667873.760074	40.328474
3173.465343	669118.067691	40.333492
3176.553202	670354.159336	40.338509
3179.631577	671601.977077	40.343527
3182.743023	672839.430216	40.348544
3185.943876	674088.837118	40.353562
3188.925116	675344.675663	40.358580
3192.147875	676603.685252	40.363597
3194.894599	677867.026311	40.368615
3197.995053	679129.838521	40.373632
3201.391194	680396.453750	40.378650
3204.361949	681664.852816	40.383668
3207.743305	682928.140784	40.388685
3210.669888	684204.739031	40.393703
3214.326860	685473.340699	40.398720
3217.976120	686738.837027	40.403738
3221.520900	687991.415101	40.408756
3225.447946	689243.905029	40.413773
3228.443255	690499.203514	40.418791
3231.594401	691746.906571	40.423808
3234.424470	692993.843510	40.428826
3237.571872	694216.095783	40.433844
3240.609773	695421.283249	40.438861
3243.460354	696656.145093	40.443879
3246.653788	697848.477645	40.448896
3250.044189	699059.804636	40.453914
3252.923246	700288.896204	40.458932
3256.570993	701486.856079	40.463949
3260.113211	702723.971534	40.468967
3263.223445	703933.479256	40.473984
3266.478819	705157.014476	40.479002
3270.103915	706373.775853	40.484020
3273.843309	707608.277734	40.489037
3276.979854	708820.513669	40.494055
3280.869405	710040.030008	40.499072
3284.402147	711267.798684	40.504090
3287.356351	712485.634164	40.509108
3290.799664	713702.421973	40.514125
3293.973175	714939.073813	40.519143
3296.738662	716173.731307	40.524160
3299.726486	717416.482808	40.529178
3302.605667	718683.209009	40.534196
3305.779874	719946.083668	40.539213
3308.550946	721228.763506	40.544231
3311.731459	722510.435810	40.549248
3314.738162	723795.844024	40.554266
3317.686052	725115.861129	40.559284
3320.755068	726427.689250	40.564301
3323.724606	727752.517718	40.569319
3327.376411	729085.022569	40.574336
3330.604593	730416.144458	40.579354
3333.431064	731763.364054	40.584372
3336.918272	733124.274794	40.589389
3340.033976	734484.770460	40.594407
3343.825697	735843.344497	40.599424
3347.743252	737207.491564	40.604442
3351.294028	738568.604036	40.609460
3354.826168	739925.589018	40.614477
3357.938588	741305.400004	40.619495
3360.846719	742683.672381	40.624512
3364.320124	744058.848832	40.629530
3367.305434	745457.975910	40.634548
3370.578517	746858.580259	40.639565
3373.836393	748259.921658	40.644583
3376.799764	749665.987334	40.649600
3379.914684	751075.074228	40.654618
3382.924689	752519.340422	40.659636
3386.261990	753955.007556	40.664653
3389.681846	755388.669186	40.669671
3393.452092	756819.444257	40.674688
3397.052806	758270.800789	40.679706
3400.195513	759715.016718	40.684724
3404.937528	761132.368274	40.689741
3408.927936	762563.648116	40.694759
3412.505239	763972.098173	40.699776
3416.329926	765393.619312	40.704794
3419.531719	766815.415743	40.709812
3423.552797	768215.224925	40.714829
3427.281241	769612.607054	40.719847
3430.657887	771027.228563	40.724864
3434.403827	772405.898102	40.729882
3438.194055	773809.698097	40.734900
3442.303745	775173.395654	40.739917
3445.764002	776551.088069	40.744935
3449.279834	777918.250391	40.749952
3452.759065	779277.897121	40.754970
3455.965441	780667.171876	40.759988
3459.366601	782014.588291	40.765005
3462.783878	783359.477227	40.770010
3465.998854	784672.494199	40.775015
3468.837217	785910.012102	40.780020
3471.895046	787113.606972	40.785024
3474.830567	788240.985498	40.790029
3477.328383	789321.425703	40.795034
3479.662569	790331.122246	40.800039
3482.734266	791277.570980	40.805044
3484.713961	792169.400882	40.810048
3487.116247	792984.771179	40.815053
3489.423758	793759.791934	40.820058
3491.764757	794451.831427	40.825063
3493.926988	795104.502114	40.830068
3495.839950	795700.298935	40.835072
3498.326614	796215.191905	40.840077
3500.533907	796685.862964	40.845082
3502.369566	797095.793896	40.850087
3504.180582	797447.490477	40.855092
3505.287950	797747.454458	40.860096
3507.097401	798013.472920	40.865101
3508.697818	798229.798634	40.870106
3509.765418	798419.409160	40.875111
3511.092140	798553.171410	40.880116
3512.307249	798661.577175	40.885120
3513.537847	798712.265744	40.890125
3514.500672	798742.190154	40.895130
3515.374357	798744.352427	40.900135
3516.256448	798707.350881	40.905140
3516.875187	798655.277192	40.910144
3517.271537	798576.640293	40.915149
3518.254557	798472.876077	40.920154
3518.099125	798345.299126	40.925159
3519.039740	798204.630853	40.930164
3519.604128	798046.303861	40.935168
3520.178307	797871.185710	40.940173
3520.424547	797673.440964	40.945178
3520.610311	797479.872783	40.950183
3521.443299	797241.229468	40.955188
3521.277006	797012.953379	40.960192
3521.507910	796761.433943	40.965197
3521.855156	796510.180768	40.970202
3522.039037	796243.432107	40.975207
3521.915410	795957.036914	40.980212
3522.245928	795683.811186	40.985216
3522.070477	795394.357483	40.990221
3522.431242	795109.566019	40.995226
3522.420237	794816.673276	41.000231
3522.643716	794499.717021	41.005236
3522.520443	794201.366411	41.010240
3522.779880	793874.308906	41.015245
3522.771615	793560.295102	41.020250
3522.496496	793236.832309	41.025255
3522.501266	792925.587508	41.030260
3522.478357	792594.931628	41.035264
3522.518101	792275.400342	41.040269
3522.457176	791948.502714	41.045274
3522.316200	791612.367548	41.050279
3522.632954	791273.193058	41.055284
3522.358817	790939.111211	41.060288
3522.451120	790599.990621	41.065293
3522.291936	790253.918153	41.070298
3522.055661	789922.189621	41.075303
3522.214656	789576.326280	41.080308
3522.048008	789239.935161	41.085312
3521.875158	788911.637936	41.090317
3522.061165	788573.142016	41.095322
3521.676660	788236.935946	41.100327
3521.665661	787890.527068	41.105332
3521.547468	787573.070574	41.110336
3521.531579	787219.060163	41.115341
3521.563036	786871.955685	41.120346
3521.294867	786539.287933	41.125351
3521.161000	786204.468467	41.130356
3520.680729	785878.933621	41.135360
3521.133523	785533.661059	41.140365
3520.631155	785193.643346	41.145370
3520.466918	784873.517542	41.150375
3520.664762	784540.581418	41.155380
3520.192428	784212.166480	41.160384
3520.056657	783883.828423	41.165389
3519.949296	783568.897116	41.170394
3519.938643	783253.296637	41.175399
3520.026992	782933.878663	41.180404
3519.781311	782607.615424	41.185408
3519.560460	782292.351832	41.190413
3520.148213	781964.150890	41.195418
3519.424116	781645.547898	41.200423
3519.269009	781326.935199	41.205428
3519.027986	781014.177268	41.210432
3519.025015	780707.172141	41.215437
3518.785933	780380.708671	41.220442
3518.703599	780086.925894	41.225447
3518.592098	779778.275517	41.230452
3518.455663	779470.206618	41.235456
3518.132551	779169.586356	41.240461
3518.448132	778867.420914	41.245466
3517.909896	778572.323324	41.250471
3518.005165	778265.592233	41.255476
3517.771005	777974.751241	41.260480
3517.499557	777676.127827	41.265485
3517.585899	777379.008181	41.270490
3517.511816	777104.054255	41.275495
3517.415426	776803.840167	41.280500
3517.427427	776522.450553	41.285504
3517.158465	776229.527237	41.290509
3517.344311	775953.600840	41.295514
3516.847642	775653.947159	41.300519
3517.030008	775376.768692	41.305524
3516.907003	775090.127127	41.310528
3516.588944	774816.456836	41.315533
3516.878011	774543.365391	41.320538
3516.650162	774262.223894	41.325543
3516.668861	773975.909280	41.330548
3516.460908	773707.694974	41.335552
3516.265762	773427.254803	41.340557
3516.359697	773149.957521	41.345562
3516.303889	772877.993910	41.350567
3516.046429	772609.747716	41.355572
3515.691392	772333.380442	41.360576
3515.542463	772062.535005	41.365581
3515.237136	771814.611688	41.370586
3514.912142	771554.072127	41.375591
3515.141538	771292.101626	41.380596
3514.659281	771044.378718	41.385600
3514.835874	770801.071232	41.390605
3514.918003	770552.105412	41.395610
3514.979723	770297.517721	41.400615
3514.936103	770047.225381	41.405620
3514.628277	769803.423141	41.410624
3514.644722	769548.915743	41.415629
3514.405140	769292.421539	41.420634
3514.234612	769057.244889	41.425639
3514.370097	768812.597627	41.430644
3513.799884	768578.408181	41.435648
3513.745935	768344.421742	41.440653
3513.684793	768106.979156	41.445658
3513.731824	767876.608421	41.450663
3513.344714	767647.879520	41.455668
3513.206022	767419.940468	41.460672
3513.086388	767200.321526	41.465677
3513.452372	766974.799320	41.470682
3512.765212	766755.655396	41.475687
3512.811574	766529.235944	41.480692
3513.025481	766323.683935	41.485696
3512.748732	766101.002170	41.490701
3512.677923	765888.977834	41.495706
3512.312280	765675.369258	41.500711
3512.365595	765445.267507	41.505716
3512.361689	765242.482724	41.510720
3512.324715	765037.922913	41.515725
3512.225249	764828.535762	41.520730
3511.989669	764633.859117	41.525735
3512.172575	764406.761158	41.530740
3512.049305	764211.907071	41.535744
3511.530887	764013.464108	41.540749
3511.666255	763809.779246	41.545754
3511.733279	763615.026161	41.550759
3511.619266	763417.240340	41.555764
3511.401519	763227.850428	41.560768
3511.392117	763031.763291	41.565773
3511.457239	762830.430804	41.570778
3510.963827	762645.658551	41.575783
3510.928540	762453.555651	41.580788
3510.666871	762277.860740	41.585792
3511.096239	762088.433879	41.590797
3510.810532	761897.936595	41.595802
3510.561727	761716.455312	41.600807
3510.705279	761530.711902	41.605812
3510.517302	761352.664819	41.610816
3510.468570	761180.608896	41.615821
3510.208981	761006.659950	41.620826
3510.059692	760832.639440	41.625831
3510.318343	760659.780873	41.630836
3509.944689	760485.740122	41.635840
3509.646764	760320.612757	41.640845
3509.692989	760148.567000	41.645850
3509.525567	760001.369967	41.650855
3509.796705	759821.336106	41.655860
3509.348625	759663.817545	41.660864
3509.388023	759509.619738	41.665869
3509.367507	759344.079857	41.670874
3509.270606	759188.565792	41.675879
3509.199966	759025.889195	41.680884
3509.168479	758869.469576	41.685888
3509.106606	758727.115617	41.690893
3508.819260	758570.436038	41.695898
3508.956623	758424.737186	41.700903
3508.587979	758277.046469	41.705908
3508.569737	758126.333937	41.710912
3508.954692	757991.788488	41.715917
3508.937860	757837.960864	41.720922
3508.631315	757693.407121	41.725927
3508.861107	757526.749881	41.730932
3508.809501	757400.162859	41.735936
3508.281578	757236.388381	41.740941
3508.627967	757095.022277	41.745946
3508.384719	756961.253450	41.750951
3508.638420	756808.939819	41.755956
3508.656180	756662.733445	41.760960
3508.540737	756519.656035	41.765965
3508.528097	756387.862858	41.770970
3507.767877	756251.106568	41.775975
3508.041365	756104.699167	41.780980
3507.881096	755966.900737	41.785984
3507.878011	755843.143030	41.790989
3508.026192	755707.806604	41.795994
3507.484287	755580.233736	41.800999
3507.909305	755446.969741	41.806004
3507.642095	755319.495238	41.811008
3507.555485	755185.916295	41.816013
3507.759970	755064.777671	41.821018
3507.335662	754943.691667	41.826023
3507.622155	754817.055362	41.831028
3507.552022	754683.958669	41.836032
3507.222743	754573.861282	41.841037
3507.447412	754443.674126	41.846042
3507.325219	754316.702101	41.851047
3507.076718	754194.488956	41.856052
3507.224501	754078.676753	41.861056
3507.163637	753963.835457	41.866061
3507.316743	753840.612143	41.871066
3506.867274	753728.942389	41.876071
3506.893290	753602.526616	41.881076
3506.614074	753497.491651	41.886080
3506.625823	753373.444738	41.891085
3506.876350	753269.652422	41.896090
3506.508990	753158.207717	41.901095
3506.503409	753053.565918	41.906100
3506.814797	752947.932021	41.911104
3506.508344	752845.016165	41.916109
3506.658237	752731.553803	41.921114
3506.378806	752624.235220	41.926119
3506.338430	752521.419231	41.931124
3506.371482	752417.947699	41.936128
3506.121269	752306.817027	41.941133
3506.264058	752202.484871	41.946138
3505.910539	752103.024103	41.951143
3506.127327	752001.739156	41.956148
3505.927359	751901.262609	41.961152
3505.734992	751808.192215	41.966157
3505.976329	751712.776998	41.971162
3505.830384	751612.337156	41.976167
3505.874564	751523.323831	41.981172
3506.041266	751422.237136	41.986176
3505.906325	751320.458046	41.991181
3506.153752	751235.063012	41.996186
3505.197184	751130.601671	42.001191
3505.613354	751033.568517	42.006196
3505.689132	750949.532397	42.011200
3505.700492	750856.416875	42.016205
3505.757646	750768.627657	42.021210
3505.858295	750683.448384	42.026215
3505.778567	750581.205855	42.031220
3505.428701	750499.705150	42.036224
3505.344866	750400.424900	42.041229
3505.338636	750303.946411	42.046234
3504.815172	750224.151125	42.051239
3505.282761	750139.251044	42.056244
3505.672324	750069.480113	42.061248
3505.312018	749979.330212	42.066253
3505.537025	749895.603822	42.071258
3505.272205	749808.894412	42.076263
3505.248406	749710.978728	42.081268
3505.110848	749634.374315	42.086272
3504.893260	749540.045676	42.091277
3505.057978	749469.367795	42.096282
3504.998592	749394.378505	42.101287
3505.254281	749312.122958	42.106292
3505.135680	749229.631942	42.111296
3504.817343	749142.775709	42.116301
3504.916341	749063.359700	42.121306
3504.858618	748994.987072	42.126311
3504.981987	748906.375287	42.131316
3504.860846	748827.734397	42.136320
3504.499417	748760.496922	42.141325
3504.863146	748676.685063	42.146330
3504.361934	748610.161144	42.151335
3504.625793	748539.013717	42.156340
3504.968749	748464.492505	42.161344
3504.555308	748403.634777	42.166349
3504.752148	748319.846655	42.171354
3504.708982	748257.147702	42.176359
3504.526206	748179.894041	42.181364
3504.638818	748107.581718	42.186368
3504.327300	748031.929142	42.191373
3504.438483	747957.540212	42.196378
3504.228193	747894.569461	42.201383
3504.463696	747823.321352	42.206388
3504.467497	747757.645609	42.211392
3504.138776	747693.704461	42.216397
3504.653482	747619.295041	42.221402
3504.388125	747558.850999	42.226407
3504.814294	747491.027641	42.231412
3504.517431	747417.639947	42.236416
3504.426157	747349.208992	42.241421
3504.299585	747266.401967	42.246426
3504.162719	747207.021212	42.251431
3504.005597	747139.834817	42.256436
3504.065131	747077.801304	42.261440
3504.013397	747009.163146	42.266445
3504.052736	746954.891236	42.271450
3503.703747	746890.996276	42.276455
3504.024499	746834.453006	42.281460
3504.109021	746779.579335	42.286464
3504.049713	746710.346722	42.291469
3504.029415	746650.843626	42.296474
3504.195657	746589.925364	42.301479
3504.154407	746530.523664	42.306484
3504.153132	746460.142470	42.311488
3504.125494	746395.448972	42.316493
3504.213803	746331.576025	42.321498
3503.903358	746281.706750	42.326503
3503.911096	746213.002345	42.331508
3503.524512	746162.354057	42.336512
3503.821357	746100.273573	42.341517
3503.815883	746045.063627	42.346522
3503.666300	745988.641395	42.351527
3503.598370	745934.429556	42.356532
3503.879777	745878.775602	42.361536
3503.703029	745817.512572	42.366541
3503.985272	745777.230313	42.371546
3503.702798	745713.364162	42.376551
3503.624547	745652.281283	42.381556
3503.691234	745594.090401	42.386560
3503.832494	745543.944056	42.391565
3503.867173	745482.050289	42.396570
3503.262369	745431.235601	42.401575
3503.567876	745373.646233	42.406580
3503.628006	745325.390322	42.411584
3503.279654	745279.129497	42.416589
3503.508722	745225.456870	42.421594
3503.168123	745180.825479	42.426599
3503.616401	745132.998580	42.431604
3503.696441	745078.064292	42.436608
3502.955747	745029.246814	42.441613
3503.358902	744971.490056	42.446618
3502.946245	744928.055568	42.451623
3502.879364	744888.567965	42.456628
3503.495960	744831.368131	42.461632
3503.418927	744780.511442	42.466637
3503.352145	744731.086384	42.471642
3503.091904	744681.495236	42.476647
3503.216010	744646.572462	42.481652
3502.816445	744597.003803	42.486656
3502.315559	744567.523168	42.491661
3503.273890	744524.304829	42.496666
3503.390396	744478.061336	42.501671
3503.008750	744428.093145	42.506676
3503.460534	744386.045394	42.511680
3503.333946	744350.569469	42.516685
3503.028056	744296.088994	42.521690
3502.977034	744255.409048	42.526695
3502.987998	744211.505075	42.531700
3503.315506	744160.379764	42.536704
3503.070045	744125.911266	42.541709
3503.500076	744068.538956	42.546714
3503.029268	744018.928978	42.551719
3502.526748	743974.960213	42.556724
3503.142351	743940.793585	42.561728
3502.480460	743901.448783	42.566733
3502.797454	743857.442822	42.571738
3502.880021	743827.714666	42.576743
3502.855952	743780.452018	42.581748
3503.159308	743742.430185	42.586752
3502.939912	743710.229914	42.591757
3502.905938	743661.336576	42.596762
3502.371035	743613.910125	42.601767
3502.571561	743589.452015	42.606772
3502.677550	743552.945188	42.611776
3502.543159	743528.641120	42.616781
3502.830314	743485.478558	42.621786
3502.313556	743453.623038	42.626791
3502.247705	743417.143977	42.631796
3502.327043	743382.519657	42.636800
3502.481964	743356.041122	42.641805
3502.411440	743322.726873	42.646810
3502.705137	743296.076869	42.651815
3502.898077	743258.318174	42.656820
3502.772580	743212.057786	42.661824
3502.465106	743177.595377	42.666829
3502.652604	743143.842166	42.671834
3502.527169	743110.536094	42.676839
3502.549261	743077.502183	42.681844
3502.537845	743046.303208	42.686848
3502.166397	743013.185717	42.691853
3502.617659	742971.921664	42.696858
3502.513332	742950.676582	42.701863
3502.332616	742915.005337	42.706868
3502.492661	742882.392842	42.711872
3502.187596	742855.049124	42.716877
3502.390129	742819.066874	42.721882
3502.536291	742801.290828	42.726887
3502.829039	742762.375952	42.731892
3502.515767	742722.670946	42.736896
3502.460038	742692.714117	42.741901
3502.583784	742656.051855	42.746906
3502.377507	742628.443780	42.751911
3502.464096	742596.534535	42.756916
3502.188689	742571.558520	42.761920
3502.415572	742547.290624	42.766925
3502.377204	742505.709446	42.771930
3502.713154	742477.022233	42.776935
3502.427503	742447.992578	42.781940
3502.916699	742405.037974	42.786945
3502.322503	742372.745814	42.791949
3502.370644	742345.589217	42.796954
3502.662337	742302.073275	42.801959
3502.560814	742269.402569	42.806964
3502.340371	742243.031779	42.811969
3502.410761	742204.348707	42.816973
3502.201485	742174.761450	42.821978
3501.956160	742151.509966	42.826983
3501.895634	742127.189369	42.831988
3502.108430	742102.081739	42.836993
3501.831311	742089.813849	42.841997
3501.736927	742060.355536	42.847002
3502.051998	742044.379641	42.852007
3501.888131	742017.108589	42.857012
3502.117779	741999.415851	42.862017
3501.897248	741967.307548	42.867021
3502.064936	741935.184417	42.872026
3501.895914	741929.426324	42.877031
3501.682027	741897.366093	42.882036
3501.853323	741885.221601	42.887041
3501.610324	741857.468533	42.892045
3501.641945	741829.571077	42.897050
3501.532225	741825.632927	42.902055
3501.534834	741798.630338	42.907060
3501.917793	741785.164893	42.912065
3501.659226	741772.843989	42.917069
3502.297289	741738.565226	42.922074
3501.887954	741724.686596	42.927079
3502.127056	741694.627805	42.932084
3502.420923	741669.999962	42.937089
3502.125329	741643.639588	42.942093
3501.933343	741625.372764	42.947098
3501.660085	741603.014484	42.952103
3501.805050	741577.916400	42.957108
3502.216705	741554.900787	42.962113
3501.947111	741542.976995	42.967117
3502.221560	741514.494282	42.972122
3501.715148	741484.261147	42.977127
3501.624602	741474.434303	42.982132
3502.063989	741434.845725	42.987137
3501.933172	741416.222110	42.992141
3501.997411	741395.340643	42.997146
3502.065288	741382.322240	43.002151
3502.005040	741353.993172	43.007156
3502.117875	741329.295270	43.012161
3501.712665	741316.997886	43.017165
3502.127552	741289.084649	43.022170
3501.805667	741270.591180	43.027175
3501.931277	741249.699187	43.032180
3502.047176	741230.144117	43.037185
3501.531641	741206.885043	43.042189
3501.723372	741185.635746	43.047194
3501.967909	741176.049911	43.052199
3501.947878	741144.201883	43.057204
3502.146894	741132.793541	43.062209
3501.501356	741107.181628	43.067213
3502.000781	741090.480922	43.072218
3502.274146	741064.618107	43.077223
3501.822841	741038.973876	43.082228
3501.758291	741016.183771	43.087233
3501.471179	740999.810685	43.092237
3502.120540	740974.182201	43.097242
3501.792280	740955.886888	43.102247
3501.589828	740941.082411	43.107252
3501.887784	740921.348115	43.112257
3501.650365	740899.822746	43.117261
3502.015179	740883.836295	43.122266
3501.966149	740869.500936	43.127271
3501.742235	740838.278895	43.132276
3501.927377	740830.928192	43.137281
3501.508454	740801.568280	43.142285
3501.543857	740782.618940	43.147290
3501.782864	740778.474257	43.152295
3501.672266	740754.009328	43.157300
3501.981356	740732.739424	43.162305
3501.430563	740716.903939	43.167309
3501.706482	740699.893116	43.172314
3501.830184	740687.111654	43.177319
3501.755617	740668.081289	43.182324
3501.900316	740642.732979	43.187329
3501.771798	740638.896266	43.192333
3501.871750	740604.355294	43.197338
3502.178414	740580.562811	43.202343
3501.653709	740552.604401	43.207348
3501.814999	740533.435813	43.212353
3501.892129	740523.035989	43.217357
3501.566313	740500.386499	43.222362
3501.901342	740491.032199	43.227367
3501.500625	740477.149948	43.232372
3501.597034	740442.757246	43.237377
3501.805441	740431.148492	43.242381
3501.666073	740422.218747	43.247386
3501.647394	740392.890106	43.252391
3501.699852	740395.404160	43.257396
3501.901950	740366.929283	43.262401
3501.794780	740352.602596	43.267405
3501.923069	740327.651701	43.272410
3501.677449	740319.530821	43.277415
3501.521324	740299.128056	43.282420
3501.718568	740280.942199	43.287425
3501.475776	740256.794365	43.292429
3501.540373	740240.262659	43.297434
3501.642366	740240.146959	43.302439
3501.376552	740216.299593	43.307444
3501.504839	740194.612945	43.312449
3501.546170	740185.603608	43.317453
3501.448290	740179.387297	43.322458
3501.494340	740154.746238	43.327463
3501.545432	740146.279359	43.332468
3501.649157	740140.277028	43.337473
3501.405881	740119.146225	43.342477
3501.431513	740095.101937	43.347482
3501.912232	740086.514535	43.352487
3501.444335	740078.182810	43.357492
3501.753168	740047.512669	43.362497
3501.381583	740043.320107	43.367501
3501.526464	740022.916356	43.372506
3501.561565	740010.296844	43.377511
3501.480569	739997.745963	43.382516
3501.675776	739982.972913	43.387521
3501.438541	739976.828937	43.392525
3501.502536	739940.658637	43.397530
3501.774232	739939.179299	43.402535
3501.610654	739922.239439	43.407540
3501.836569	739895.193463	43.412545
3501.547333	739891.828144	43.417549
3501.540978	739869.272458	43.422554
3501.675746	739844.615776	43.427559
3501.986552	739838.034862	43.432564
3501.792916	739825.205519	43.437569
3501.590435	739805.551150	43.442573
3501.533892	739788.247046	43.447578
3501.622434	739777.844361	43.452583
3501.307635	739756.773878	43.457588
3501.674458	739729.258845	43.462593
3501.508579	739733.095348	43.467597
3501.416868	739708.723008	43.472602
3501.621512	739703.791963	43.477607
3501.458684	739687.346155	43.482612
3501.814936	739673.238469	43.487617
3501.175286	739656.327242	43.492621
3501.231580	739635.739264	43.497626
3501.467437	739626.251935	43.502631
3501.375653	739628.740599	43.507636
3501.530471	739609.917131	43.512641
3501.341036	739589.419108	43.517645
3501.471310	739586.577957	43.522650
3501.877704	739579.684224	43.527655
3501.706797	739554.928750	43.532660
3501.543266	739535.959839	43.537665
3501.174503	739539.236334	43.542669
3501.532860	739516.718317	43.547674
3501.225813	739509.348790	43.552679
3501.582128	739496.774321	43.557684
3501.839379	739491.735513	43.562689
3501.570800	739469.469370	43.567693
3501.463328	739449.402664	43.572698
3501.300132	739451.457960	43.577703
3501.414110	739429.919998	43.582708
3501.705700	739407.758993	43.587713
3501.244826	739400.860010	43.592717
3501.227050	739394.629847	43.597722
3501.421624	739381.141998	43.602727
3501.181267	739360.157099	43.607732
3501.395614	739354.877946	43.612737
3501.417785	739349.778956	43.617741
3501.385797	739345.183612	43.622746
3501.623120	739326.296370	43.627751
3501.265328	739304.143445	43.632756
3501.172479	739287.042130	43.637761
3501.398964	739303.824707	43.642765
3501.293396	739276.633523	43.647770
3501.510066	739259.678884	43.652775
3501.089916	739243.274678	43.657780
3501.436629	739246.878297	43.662785
3501.342279	739252.929389	43.667789
3500.995167	739225.035884	43.672794
3501.152975	739203.638480	43.677799
3500.826927	739196.024445	43.682804
3500.951675	739192.095707	43.687809
3501.087149	739190.836628	43.692813
3501.164122	739181.325554	43.697818
3501.335474	739187.035963	43.702823
3501.175359	739187.359331	43.707828
3501.293329	739169.233505	43.712833
3501.372910	739151.856049	43.717837
3501.318844	739140.585615	43.722842
3501.383850	739142.355924	43.727847
3501.191095	739143.525699	43.732852
3501.427165	739116.425927	43.737857
3501.430427	739108.658447	43.742861
3501.318440	739102.938339	43.747866
3501.492889	739091.234301	43.752871
3501.116538	739083.826357	43.757876
3501.374675	739057.217453	43.762881
3501.160539	739044.786010	43.767885
3501.460878	739047.210059	43.772890
3501.539375	739042.893115	43.777895
3501.625425	739033.330892	43.782900
3501.582645	739015.725999	43.787905
3501.094995	739004.378604	43.792909
3501.257799	738997.920401	43.797914
3501.425559	738988.196205	43.802919
3501.164205	738964.443282	43.807924
3501.320360	738948.487429	43.812929
3501.396091	738954.560115	43.817933
3501.335735	738942.053627	43.822938
3501.458849	738942.231256	43.827943
3501.236420	738928.663133	43.832948
3501.440421	738918.833918	43.837953
3501.262931	738915.796024	43.842957
3501.358331	738919.144486	43.847962
3501.313923	738895.850236	43.852967
3501.118568	738869.315644	43.857972
3500.995606	738862.607715	43.862977
3500.875907	738866.288583	43.867981
3500.869799	738860.649749	43.872986
3501.154951	738865.203705	43.877991
3500.940732	738871.819097	43.882996
3501.121709	738855.116861	43.888001
3501.080776	738869.619311	43.893005
3501.167412	738841.553837	43.898010
3501.108182	738823.753346	43.903015
3500.951784	738817.793004	43.908020
3501.251274	738809.432075	43.913025
3501.177434	738814.094856	43.918029
3501.298046	738819.368654	43.923034
3501.445898	738806.530707	43.928039
3501.246129	738796.471224	43.933044
3501.177699	738767.491118	43.938049
3501.151005	738770.859819	43.943053
3501.146945	738764.725843	43.948058
3501.583564	738755.748514	43.953063
3501.079013	738747.174070	43.958068
3501.387611	738719.467278	43.963073
3501.461183	738724.897334	43.968077
3501.106272	738721.542366	43.973082
3501.256130	738715.778709	43.978087
3500.957526	738700.837513	43.983092
3501.556644	738669.767779	43.988097
3501.109275	738670.138635	43.993101
3501.125102	738668.453978	43.998106
3501.083693	738671.280936	44.003111
3501.005837	738680.397139	44.008116
3501.060650	738671.185962	44.013121
3501.069777	738666.929752	44.018125
3500.969711	738651.955657	44.023130
3501.212571	738629.899491	44.028135
3501.111758	738628.778320	44.033140
3501.645191	738612.413129	44.038145
3501.061318	738625.175183	44.043149
3501.106055	738618.835133	44.048154
3501.382131	738623.440202	44.053159
3501.368336	738596.825224	44.058164
3501.410335	738586.478150	44.063169
3501.040611	738573.923255	44.068173
3501.293048	738574.871121	44.073178
3501.256954	738584.326856	44.078183
3501.199483	738561.578009	44.083188
3501.512491	738535.997272	44.088193
3501.037846	738536.916865	44.093197
3501.214283	738539.163646	44.098202
3501.000563	738530.343006	44.103207
3500.626671	738537.479812	44.108212
3501.118248	738523.199307	44.113217
3500.861408	738517.403763	44.118221
3501.138241	738490.196176	44.123226
3501.066684	738494.660865	44.128231
3501.002204	738483.836499	44.133236
3501.315856	738471.960123	44.138241
3501.114236	738470.905064	44.143245
3501.406581	738482.829894	44.148250
3501.350578	738471.558832	44.153255
3501.202842	738460.302913	44.158260
3501.286730	738434.116529	44.163265
3501.205098	738429.380433	44.168269
3501.076435	738430.985001	44.173274
3501.429871	738418.854594	44.178279
3501.046389	738412.139859	44.183284
3501.306757	738388.348478	44.188289
3501.017544	738383.646657	44.193293
3501.223633	738384.354825	44.198298
3501.252481	738377.621401	44.203303
3500.843482	738385.753663	44.208308
3501.172507	738375.705217	44.213313
3501.091070	738370.672197	44.218317
3501.213943	738350.663607	44.223322
3501.207480	738347.844613	44.228327
3500.847849	738340.878495	44.233332
3501.245978	738336.063064	44.238337
3501.082181	738340.988368	44.243341
3501.310140	738333.677765	44.248346
3501.461306	738334.741348	44.253351
3501.104546	738316.246743	44.258356
3501.371913	738286.417774	44.263361
3501.237150	738294.653241	44.268365
3501.152749	738284.326662	44.273370
3501.092578	738291.114985	44.278375
3500.970625	738268.524386	44.283380
3501.333631	738250.702316	44.288385
3501.296566	738246.948283	44.293389
3501.433565	738247.618404	44.298394
3501.380911	738243.669039	44.303399
3501.306931	738242.345471	44.308404
3501.433354	738210.758342	44.313409
3501.180673	738201.597436	44.318413
3501.503399	738203.374844	44.323418
3501.606944	738202.863045	44.328423
3501.323780	738188.017288	44.333428
3501.415522	738165.588993	44.338433
3501.329449	738167.582395	44.343437
3501.074730	738170.642688	44.348442
3501.494347	738155.779692	44.353447
3501.316529	738137.255101	44.358452
3501.553448	738110.498114	44.363457
3501.489233	738113.625904	44.368461
3500.926068	738105.456270	44.373466
3501.196244	738080.178018	44.378471
3501.039132	738079.214506	44.383476
3500.962592	738062.850033	44.388481
3501.126709	738063.862034	44.393485
3501.236558	738062.607015	44.398490
3501.288990	738064.181731	44.403495
3501.182798	738066.970130	44.408500
3501.356763	738037.403055	44.413505
3501.110197	738026.806070	44.418509
3501.237142	738015.306218	44.423514
3501.377235	738015.530543	44.428519
3501.216485	738020.406062	44.433524
3501.047021	737999.010028	44.438529
3501.159625	737996.517583	44.443533
3501.443410	737975.739287	44.448538
3501.373040	737972.534893	44.453543
3500.795940	737969.166840	44.458548
3501.382928	737965.606423	44.463553
3501.308225	737963.095441	44.468557
3500.874994	737939.763690	44.473562
3501.248890	737922.730751	44.478567
3501.156829	737939.667805	44.483572
3501.114745	737918.398942	44.488577
3501.117677	737928.096400	44.493581
3500.871195	737919.329975	44.498586
3501.186087	737926.452461	44.503591
3501.082074	737921.373408	44.508596
3501.221737	737890.277612	44.513601
3501.201139	737890.281099	44.518605
3500.984622	737879.827389	44.523610
3501.274164	737875.771815	44.528615
3500.860699	737889.694378	44.533620
3501.082348	737873.676074	44.538625
3501.307748	737868.938387	44.543629
3501.062595	737853.590932	44.548634
3501.036108	737838.702107	44.553639
3500.990220	737826.785229	44.558644
3501.070862	737825.089685	44.563649
3501.111329	737822.609106	44.568653
3500.707290	737831.384343	44.573658
3500.890405	737828.731756	44.578663
3500.911687	737836.397636	44.583668
3501.003456	737832.523159	44.588673
3500.962465	737835.696700	44.593677
3500.903071	737840.654538	44.598682
3501.080777	737828.255400	44.603687
3500.814943	737825.973876	44.608692
3501.001678	737787.497455	44.613697
3501.111769	737785.549637	44.618701
3500.779195	737782.932772	44.623706
3501.116775	737770.358686	44.628711
3500.871040	737786.232904	44.633716
3500.819648	737779.066916	44.638721
3501.129167	737780.302326	44.643725
3501.245814	737779.837816	44.648730
3501.582411	737775.279618	44.653735
3500.870166	737773.764565	44.658740
3501.047283	737753.448636	44.663745
3500.939623	737756.831144	44.668749
3501.163599	737745.116949	44.673754
3501.205440	737737.292278	44.678759
3501.040011	737743.059379	44.683764
3500.782981	737738.203416	44.688769
3500.873557	737742.988092	44.693773
3500.914655	737733.679140	44.698778
3500.985473	737737.081644	44.703783
3500.828871	737735.672684	44.708788
3501.395073	737727.068633	44.713793
3500.996039	737725.650253	44.718797
3500.830511	737705.143422	44.723802
3500.884237	737693.011962	44.728807
3500.922880	737695.578635	44.733812
3501.122029	737689.509213	44.738817
3501.075469	737687.092454	44.743821
3501.129997	737686.143400	44.748826
3501.414504	737678.624934	44.753831
3501.142510	737704.597646	44.758836
3501.339032	737669.236292	44.763841
3501.363901	737660.375261	44.768845
3501.214444	737649.118479	44.773850
3501.452547	737647.644279	44.778855
3501.207153	737650.604268	44.783860
3501.051722	737625.889715	44.788865
3501.372065	737619.206443	44.793869
3501.369137	737601.245475	44.798874
3501.338878	737597.292088	44.803879
3501.153272	737604.596530	44.808884
3501.096017	737592.285334	44.813889
3501.119603	737563.186682	44.818893
3501.103478	737558.043393	44.823898
3501.418091	737561.999459	44.828903
3501.190095	737553.279056	44.833908
3501.295987	737555.735699	44.838913
3501.173383	737551.748068	44.843917
3501.103305	737551.363882	44.848922
3500.971582	737514.868538	44.853927
3500.692367	737519.813419	44.858932
3501.172832	737512.905674	44.863937
3501.296184	737508.481527	44.868941
3501.197204	737518.938544	44.873946
3501.391615	737516.135544	44.878951
3501.168520	737505.533986	44.883956
3500.937714	737485.086857	44.888961
3501.044797	737464.534359	44.893965
3501.281209	737471.818666	44.898970
3501.150028	737471.691982	44.903975
3500.827924	737465.609563	44.908980
3500.951383	737467.222141	44.913985
3501.101744	737469.176645	44.918989
3500.950810	737471.576791	44.923994
3501.232722	737452.331376	44.928999
3501.014956	737455.187907	44.934004
3500.838252	737442.153991	44.939009
3501.100709	737436.073915	44.944013
3501.202052	737430.416314	44.949018
3501.094197	737423.655193	44.954023
3500.883084	737431.112454	44.959028
3500.857582	737436.262870	44.964033
3501.524745	737431.600371	44.969037
3501.007096	737421.344267	44.974042
3500.982323	737393.094180	44.979047
3501.360028	737388.232078	44.984052
3501.340384	737385.810779	44.989057
3501.068243	737389.171140	44.994061
3500.984547	737388.541786	44.999066
3501.351126	737384.225824	45.004071
3501.349802	737378.189294	45.009076
3501.348561	737345.927088	45.014081
3501.164811	737349.767684	45.019085
3501.377537	737346.615221	45.024090
3501.508325	737336.796161	45.029095
3500.962139	737321.497426	45.034100
3501.112719	737309.745241	45.039105
3501.423783	737293.958415	45.044109
3500.802140	737304.254668	45.049114
3501.115375	737292.030234	45.054119
3501.299590	737291.950393	45.059124
3501.060955	737296.740257	45.064129
3501.496638	737290.482998	45.069133
3501.056010	737257.154937	45.074138
3501.200924	737248.768442	45.079143
3501.074865	737257.844750	45.084148
3501.047816	737246.418723	45.089153
3501.326037	737241.572972	45.094157
3501.057602	737237.361866	45.099162
3501.137247	737215.972049	45.104167
3501.129960	737208.204462	45.109172
3501.146882	737208.449166	45.114177
3501.277590	737200.708251	45.119181
3500.997413	737200.259799	45.124186
3501.169980	737201.517933	45.129191
3500.820019	737206.326247	45.134196
3501.211969	737199.779244	45.139201
3501.427801	737179.851328	45.144205
3501.327387	737169.971302	45.149210
3501.357451	737153.240963	45.154215
3501.314827	737166.064343	45.159220
3501.299316	737152.162096	45.164225
3501.081002	737137.254178	45.169229
3500.920456	737123.227396	45.174234
3501.144279	737114.679269	45.179239
3500.965666	737115.302675	45.184244
3501.184013	737117.988290	45.189249
3501.416694	737114.288116	45.194253
3501.232025	737115.605297	45.199258
3501.348956	737085.351351	45.204263
3501.529989	737074.435017	45.209268
3501.102755	737072.031493	45.214273
3501.369620	737069.711207	45.219277
3501.079440	737060.604666	45.224282
3501.047954	737040.568819	45.229287
3501.284411	737029.841203	45.234292
3501.060303	737024.039157	45.239297
3501.144990	737031.546879	45.244301
3500.677915	737019.698396	45.249306
3501.211659	737010.356678	45.254311
3500.826061	737019.575113	45.259316
3500.836930	737015.614642	45.264321
3500.840445	737022.146095	45.269325
3500.737421	737030.575557	45.274330
3500.949358	737026.334442	45.279335
3500.984793	737034.741019	45.284340
3500.797551	737021.361766	45.289345
3500.884790	737020.110321	45.294349
3500.972313	737022.669134	45.299354
3501.061605	736989.598779	45.304359
3500.979346	736977.983552	45.309364
3501.179181	736970.874293	45.314369
3500.889292	736975.029516	45.319373
3500.847928	736979.094183	45.324378
3500.825765	736969.398917	45.329383
3500.722931	736976.888192	45.334388
3501.031004	736972.482709	45.339393
3501.201965	736982.697881	45.344397
3501.046136	736978.814423	45.349402
3501.203704	736975.720415	45.354407
3501.202896	736961.073134	45.359412
3500.979868	736941.563539	45.364417
3501.252327	736936.965982	45.369421
3501.175852	736930.941532	45.374426
3501.102121	736929.568219	45.379431
3500.810764	736932.684519	45.384436
3500.786700	736934.024674	45.389441
3501.001555	736928.298476	45.394445
3501.303101	736927.259029	45.399450
3501.286972	736919.839018	45.404455
3500.812799	736905.368827	45.409460
3501.102239	736897.551905	45.414465
3501.323257	736888.360693	45.419469
3500.967575	736890.745360	45.424474
3501.173142	736880.171104	45.429479
3501.089350	736894.040916	45.434484
3501.008847	736882.375775	45.439489
3501.226512	736881.201727	45.444493
3501.092421	736855.145158	45.449498
3501.289592	736851.747645	45.454503
3501.176302	736844.739504	45.459508
3501.233570	736844.532182	45.464513
3501.183059	736837.662117	45.469517
3501.248244	736833.940008	45.474522
3501.320083	736808.393599	45.479527
3501.296895	736798.945725	45.484532
3501.304264	736799.637392	45.489537
3501.593470	736800.331972	45.494541
3501.071651	736783.345656	45.499546
3500.820704	736762.751547	45.504551
3501.337055	736758.558960	45.509556
3501.377694	736753.207829	45.514561
3501.183027	736748.143008	45.519565
3500.854219	736754.828568	45.524570
3501.501632	736754.969098	45.529575
3501.283677	736741.149076	45.534580
3501.382058	736726.930351	45.539585
3501.242879	736716.412848	45.544589
3501.505964	736717.210726	45.549594
3501.549444	736700.378250	45.554599
3501.387188	736678.829026	45.559604
3501.220148	736666.485057	45.564609
3501.422012	736660.216462	45.569613
3501.116967	736660.910280	45.574618
3501.562214	736648.316645	45.579623
3501.157431	736623.640195	45.584628
3501.139643	736626.562946	45.589633
3501.089300	736614.546022	45.594637
3500.935094	736621.252327	45.599642
3501.108638	736615.483246	45.604647
3501.350749	736617.719721	45.609652
3501.232291	736603.536610	45.614657
3501.254646	736582.500977	45.619661
3501.424859	736581.780112	45.624666
3501.388110	736583.419345	45.629671
3501.034421	736573.976333	45.634676
3501.045444	736558.039691	45.639681
3501.093302	736541.750519	45.644685
3500.956524	736539.991657	45.649690
3500.895255	736532.133358	45.654695
3501.106047	736540.066090	45.659700
3500.962972	736530.885147	45.664705
3500.910387	736539.554227	45.669709
3500.665151	736534.448140	45.674714
3500.938796	736530.988368	45.679719
3500.717594	736524.047264	45.684724
3501.039356	736536.415540	45.689729
3500.943635	736526.929843	45.694733
3500.843818	736531.152859	45.699738
3501.170590	736521.250926	45.704743
3501.031887	736511.970264	45.709748
3501.070893	736484.300279	45.714753
3501.261321	736475.460064	45.719757
3501.358226	736478.809307	45.724762
3501.022581	736468.125991	45.729767
3501.328578	736480.892861	45.734772
3501.136259	736478.796749	45.739777
3501.070300	736460.101315	45.744781
3500.843213	736450.983651	45.749786
3501.009183	736442.988738	45.754791
3500.441132	736439.618527	45.759796
3500.744735	736442.636700	45.764801
3501.163411	736437.024935	45.769805
3501.147015	736445.341721	45.774810
3501.224886	736416.526854	45.779815
3501.294615	736361.880254	45.784820
3500.710666	736241.669290	45.789825
3500.968799	736066.630702	45.794829
3500.829580	735850.328492	45.799834
3500.534854	735556.143729	45.804839
3500.325755	735215.408284	45.809844
3500.290407	734817.261609	45.814849
3500.439508	734362.782446	45.819853
3499.759138	733854.653531	45.824858
3499.679266	733270.498565	45.829863
3499.030990	732660.253294	45.834868
3498.496959	731981.958577	45.839873
3498.433312	731240.787660	45.844877
3497.863283	730458.180525	45.849882
3497.914259	729602.388461	45.854887
3497.332470	728697.670057	45.859892
3496.901552	727724.211802	45.864897
3496.396770	726695.008034	45.869901
3495.668048	725610.409736	45.874906
3495.086573	724459.628794	45.879911
3494.540712	723258.815656	45.884916
3493.896144	721981.844724	45.889921
3493.205598	720666.257288	45.894925
3492.230905	719293.230113	45.899930
3491.654809	717848.635398	45.904935
3490.826266	716355.662592	45.909940
3489.976999	714794.301924	45.914945
3489.422982	713171.164100	45.919949
3488.340890	711504.667317	45.924954
3487.695982	709766.179643	45.929959
3486.223105	707978.511986	45.934964
3485.558443	706120.305142	45.939969
3484.889310	704211.819847	45.944973
3483.427256	702250.024645	45.949978
3482.807536	700223.034618	45.954983
3481.475408	698152.540589	45.959988
3480.272899	696008.340369	45.964993
3479.416711	693813.674957	45.969997
3477.657519	691572.447925	45.975002
3476.648029	689260.865616	45.980007
3475.641282	686904.735744	45.985012
3474.107488	684495.700299	45.990017
3473.141604	682020.043465	45.995021
3471.704021	679502.547216	46.000026
3470.386530	676916.324610	46.005031
3469.038795	674298.383293	46.010036
3467.604562	671614.607168	46.015041
3466.426567	668875.611771	46.020045
3464.637294	666079.702579	46.025050
3463.203758	663222.284480	46.030055
3461.725541	660339.716329	46.035060
3459.965246	657396.169650	46.040065
3458.722875	654392.513324	46.045069
3456.333346	651352.958197	46.050074
3455.041182	648250.819030	46.055079
3453.673530	645106.638261	46.060084
3451.722011	641908.516954	46.065089
3449.852463	638659.355156	46.070093
3447.892176	635376.307422	46.075098
3446.190594	632026.455559	46.080103
3444.353680	628649.971157	46.085108
3442.446296	625212.166226	46.090113
3440.959814	621716.719946	46.095117
3438.793277	618202.716043	46.100122
3437.112860	614615.705309	46.105127
3434.987095	610994.252876	46.110132
3432.656256	607324.451212	46.115137
3431.120999	603601.684863	46.120141
3428.869328	599845.495149	46.125146
3426.571926	596030.341262	46.130151
3424.491112	592164.577272	46.135156
3422.268669	588271.395769	46.140161
3420.351834	584330.905775	46.145165
3417.936434	580341.601687	46.150170
3415.898033	576313.167846	46.155175
3413.671153	572245.224706	46.160180
3411.237854	568140.372702	46.165185
3409.294654	563981.259628	46.170189
3406.391223	559788.592160	46.175194
3404.078491	555552.830988	46.180199
3401.842600	551275.955733	46.185204
3399.505935	546953.843747	46.190209
3396.938671	542603.188166	46.195213
3394.534227	538205.960211	46.200218
3391.950307	533766.131920	46.205223
3389.817894	529283.481947	46.210228
3386.773600	524781.851091	46.215233
3384.297541	520220.999137	46.220237
3381.537676	515638.678451	46.225242
3379.307162	511006.307995	46.230247
3376.399891	506345.503497	46.235252
3373.599433	501650.018482	46.240257
3371.071888	496925.032605	46.245261
3368.588207	492156.470096	46.250266
3365.953720	487350.680964	46.255271
3362.850190	482517.081067	46.260276
3359.741981	477646.738715	46.265281
3357.000497	472740.555188	46.270285
3354.113898	467808.293898	46.275290
3351.132379	462842.153012	46.280295
3348.537019	457849.915286	46.285300
3345.192351	452828.688027	46.290305
3342.250253	447766.272760	46.295309
3339.103015	442701.222980	46.300314
3336.256753	437583.764321	46.305319
3333.271220	432448.222423	46.310324
3329.909291	427286.283382	46.315329
3327.195210	422090.763674	46.320333
3323.776552	416881.959101	46.325338
3320.465850	411625.199664	46.330343
3317.389957	406363.982467	46.335348
3314.024813	401080.695399	46.340353
3311.129224	395752.546594	46.345357
3307.770049	390427.710799	46.350362
3304.208286	385067.904092	46.355367
3301.161809	379685.536183	46.360372
3297.995088	374289.740892	46.365377
3294.940072	368859.634193	46.370381
3291.109086	363422.474337	46.375386
3287.858126	357957.672938	46.380391
3284.669396	352472.010159	46.385396
3280.686808	346967.492165	46.390401
3277.470294	341451.300216	46.395405
3273.874923	335905.362676	46.400410
3270.208515	330357.149342	46.405415
3266.960632	324781.267762	46.410420
3262.903949	319203.387072	46.415425
3259.651888	313617.376084	46.420429
3256.022081	308016.647721	46.425434
3252.618061	302399.741658	46.430439
3248.948940	296784.247510	46.435444
3244.986216	291142.151186	46.440449
3241.301598	285503.015193	46.445453
3237.496500	279846.143257	46.450458
3233.534565	274186.635195	46.455463
3229.930358	268516.249349	46.460468
3226.267804	262844.267081	46.465473
3222.354217	257165.696626	46.470477
3218.349461	251491.558490	46.475482
3214.491382	245798.096489	46.480487
3210.715247	240122.880440	46.485492
3206.540388	234424.446612	46.490497
3203.047625	228712.136742	46.495501
3198.809923	223026.289380	46.500506
3194.885996	217332.930520	46.505511
3190.817663	211643.258024	46.510516
3186.932083	205861.024811	46.515521
3182.864541	200158.744373	46.520525
3178.525523	194473.596091	46.525530
3174.326396	188787.659118	46.530535
3170.441126	183104.373137	46.535540
3165.789100	177433.058756	46.540545
3161.674291	171760.462692	46.545549
3157.319782	166117.555913	46.550554
3152.644791	160463.454851	46.555559
3148.838665	154844.175886	46.560564
3144.198570	149225.507335	46.565569
3140.041117	143623.078036	46.570573
3135.624738	138043.465984	46.575578
3131.303210	132464.771949	46.580583
3126.589037	126905.862226	46.585588
3121.934140	121373.364421	46.590593
3117.121129	115848.822155	46.595597
3112.369263	110357.445992	46.600602
3107.520077	104877.622421	46.605607
3102.992999	99434.496046	46.610612
3097.661116	94011.269877	46.615617
3093.033905	88624.141165	46.620621
3087.635587	83268.986256	46.625626
3082.730204	77952.170278	46.630631
3077.167951	72660.022455	46.635636
3071.732076	67432.803359	46.640641
3066.253636	62234.485099	46.645645
3059.860229	57098.119450	46.650650
3050.713373	52105.285903	46.655655
3035.175565	47354.390151	46.660660
3020.199209	42754.881969	46.665665
3005.684206	38344.199087	46.670669
2991.094995	34161.311735	46.675674
2977.162316	30200.311029	46.680679
2963.038760	26503.092229	46.685684
2946.945770	23116.501041	46.690689
2927.436367	20110.743759	46.695693
2905.911540	17487.571648	46.700698
2885.562721	15190.318117	46.705703
2867.425636	13225.117991	46.710708
2851.414000	11588.196811	46.715713
2838.151981	10219.591632	46.720717
2827.166404	9135.234904	46.725722
2818.035523	8260.426702	46.730727
2810.688578	7571.314740	46.735732
2804.688676	7042.308321	46.740737
2800.302865	6629.465826	46.745741
2796.606482	6317.529731	46.750746
2793.467427	6065.993593	46.755751
2791.045211	5869.980554	46.760756
2789.121057	5724.128433	46.765761
2787.497700	5588.070523	46.770765
2785.599314	5452.274871	46.775770
2784.507377	5346.451599	46.780775
2783.213094	5215.706261	46.785780
2781.308969	5088.759840	46.790785
2779.931630	4944.318337	46.795789
2778.093482	4786.113816	46.800794
2776.237145	4624.860605	46.805799
2774.333891	4452.618146	46.810804
2772.126141	4266.240409	46.815809
2770.027616	4059.737032	46.820813
2767.768391	3849.233962	46.825818
2765.230627	3627.930552	46.830823
2762.784231	3394.437286	46.835828
2759.672751	3159.280414	46.840833
2757.018948	2906.017017	46.845837
2753.473075	2654.917356	46.850842
2750.451696	2399.470239	46.855847
2747.427171	2143.926381	46.860852
2744.413522	1892.083429	46.865857
2741.197259	1637.264852	46.870861
2737.565266	1363.500764	46.875866
2733.903235	1105.383255	46.880871
2730.300038	839.596169	46.885876
2726.412422	596.225193	46.890881
2722.703424	348.773542	46.895885
2716.691530	164.068530	46.900890
2704.407502	205.709642	46.905895
2695.812981	196.989618	46.910900
2690.199804	206.351909	46.915905
2687.923195	189.684384	46.920909
2686.293301	195.397243	46.925914
2684.006386	207.701810	46.930919
2682.181864	194.600333	46.935924
2679.060458	199.989789	46.940929
2675.975710	195.116348	46.945933
2672.756181	202.788476	46.950938
2669.374157	202.877567	46.955943
2666.140020	193.647371	46.960948
2662.477967	208.084292	46.965953
2659.591208	191.194156	46.970957
2656.173079	196.447643	46.975962
2652.646900	195.005392	46.980967
2649.622909	190.904359	46.985972
2645.986346	195.553455	46.990977
2643.169908	201.523931	46.995981
2639.654824	186.878158	47.000986
2636.087346	196.077089	47.005991
2632.270585	188.899980	47.010996
2628.708504	193.209968	47.016001
2625.316141	191.693688	47.021005
2622.810263	194.549685	47.026010
2619.303007	192.916267	47.031015
2616.016998	187.782160	47.036020
2612.188932	200.862073	47.041025
2608.628940	182.498231	47.046029
2605.105959	191.809599	47.051034
2601.456677	195.811991	47.056039
2598.590647	187.883531	47.061044
2595.674888	188.241223	47.066049
2591.785073	188.378923	47.071053
2587.939029	191.061744	47.076058
2584.384205	189.531939	47.081063
2581.668557	190.572254	47.086068
2577.706323	186.467754	47.091073
2574.763418	185.615738	47.096077
2571.138806	195.069070	47.101082
2568.057990	189.992989	47.106087
2564.424287	179.412356	47.111092
2560.408693	183.279076	47.116097
2557.189408	174.623935	47.121101
2553.953543	184.777199	47.126106
2550.049754	176.469239	47.131111
2546.782097	173.535427	47.136116
2543.489349	185.390283	47.141121
2540.436599	174.743682	47.146125
2536.935034	186.889261	47.151130
2533.102588	182.972099	47.156135
2529.649236	180.474573	47.161140
2526.051752	179.523964	47.166145
2522.494873	183.852117	47.171149
2519.089058	182.632579	47.176154
2515.477009	183.013259	47.181159
2512.163771	174.214857	47.186164
2508.553867	180.369670	47.191169
2505.084655	171.992170	47.196173
2501.767182	182.757700	47.201178
2498.446650	176.070446	47.206183
2495.465694	179.963050	47.211188
2491.394075	188.399573	47.216193
2488.232934	178.903479	47.221197
2484.461434	179.079112	47.226202
2480.780538	185.327795	47.231207
2477.488191	174.939372	47.236212
2474.029624	178.334258	47.241217
2470.572794	167.542492	47.246221
2466.973579	177.001357	47.251226
2463.209325	176.313840	47.256231
2460.370409	167.808333	47.261236
2456.600892	169.146175	47.266241
2453.224943	167.698361	47.271245
2449.754298	169.034868	47.276250
2446.305768	171.510693	47.281255
2442.724125	168.320916	47.286260
2438.961340	169.464267	47.291265
2435.526775	177.376791	47.296269
2432.434358	166.354415	47.301274
2428.838397	174.702946	47.306279
2425.380641	164.843006	47.311284
2421.618546	176.673436	47.316289
2418.336528	164.917592	47.321293
2414.847064	169.214930	47.326298
2411.590412	171.220919	47.331303
2408.082608	163.374819	47.336308
2404.239961	174.785841	47.341313
2400.703626	164.269767	47.346317
2397.386615	154.484234	47.351322
2393.849253	166.187279	47.356327
2390.535444	160.105822	47.361332
2386.934113	163.859691	47.366337
2383.481844	168.295935	47.371341
2380.003260	164.658558	47.376346
2376.523947	163.920972	47.381351
2373.195055	159.728371	47.386356
2369.305241	164.877050	47.391361
2366.140103	161.052798	47.396365
2362.811930	159.569519	47.401370
2359.053503	159.744480	47.406375
2355.603385	162.391137	47.411380
2352.164860	159.013359	47.416385
2348.241300	156.317197	47.421389
2344.867754	166.932857	47.426394
2341.514019	162.626192	47.431399
2338.329082	156.645787	47.436404
2334.801146	161.339099	47.441409
2331.439970	160.293085	47.446413
2327.303194	156.425937	47.451418
2323.783434	158.792292	47.456423
2320.524098	161.694109	47.461428
2317.093537	164.696118	47.466433
2313.586267	155.343553	47.471437
2310.050614	153.400551	47.476442
2306.507978	153.529163	47.481447
2303.039733	148.855707	47.486452
2299.647044	158.268049	47.491457
2296.236355	156.846247	47.496461
2292.934942	152.039986	47.501466
2288.797648	148.517910	47.506471
2285.515196	147.641826	47.511476
2281.995891	148.011292	47.516481
2278.691644	151.803263	47.521485
2275.396304	155.204615	47.526490
2271.786334	152.786534	47.531495
2268.673926	154.760055	47.536500
2264.413835	155.801224	47.541505
2261.199310	149.733038	47.546509
2257.545289	166.304847	47.551514
2253.959908	157.426845	47.556519
2250.609207	153.636383	47.561524
2247.152431	164.044484	47.566529
2243.839407	153.382057	47.571533
2240.570300	161.656654	47.576538
2236.786703	159.100811	47.581543
2233.859413	149.109779	47.586548
2230.063270	157.930685	47.591553
2226.215815	149.659520	47.596557
2222.654685	158.252455	47.601562
2218.786179	160.492351	47.606567
2215.525281	154.209091	47.611572
2212.451991	153.415833	47.616577
2208.753528	148.796776	47.621581
2205.251884	152.371476	47.626586
2201.639397	155.332077	47.631591
2198.358742	145.829804	47.636596
2194.548405	146.189535	47.641601
2191.027173	155.933064	47.646605
2187.715352	148.751110	47.651610
2184.099590	154.103391	47.656615
2180.896918	141.867149	47.661620
2177.281069	154.701645	47.666625
2174.075798	152.803292	47.671629
2170.493463	148.791182	47.676634
2166.419341	145.656006	47.681639
2163.278190	145.451827	47.686644
2159.659059	150.128019	47.691649
2156.709263	146.625049	47.696653
2152.893756	147.638068	47.701658
2149.305584	148.669473	47.706663
2146.050707	148.815080	47.711668
2142.138239	139.496858	47.716673
2138.803460	143.469619	47.721677
2135.265126	146.261700	47.726682
2131.277654	149.179499	47.731687
2128.249976	133.618216	47.736692
2124.583899	150.695306	47.741697
2121.254292	144.809502	47.746701
2118.064501	147.865710	47.751706
2114.493076	151.001525	47.756711
2110.989335	149.332837	47.761716
2107.242430	149.211691	47.766721
2103.256531	145.172570	47.771725
2100.180586	147.234498	47.776730
2096.624022	146.274920	47.781735
2093.708271	141.040458	47.786740
2090.081739	148.136087	47.791745
2086.297320	146.297248	47.796749
2082.673139	144.014895	47.801754
2079.291839	143.330192	47.806759
2075.901472	150.583253	47.811764
2071.726763	148.339825	47.816769
2068.496063	139.768912	47.821773
2065.841116	142.680500	47.826778
2061.960486	154.904191	47.831783
2058.549422	141.719854	47.836788
2054.617399	150.620245	47.841793
2051.563865	144.733161	47.846797
2047.862095	143.941148	47.851802
2044.070783	151.818927	47.856807
2040.638271	133.404031	47.861812
2037.169299	151.221883	47.866817
2033.562335	147.177471	47.871821
2030.432299	149.305048	47.876826
2026.497312	143.632311	47.881831
2023.510392	142.310233	47.886836
2020.199665	144.107618	47.891841
2015.976457	142.663602	47.896845
2012.849068	138.638417	47.901850
2009.454829	140.182060	47.906855
2006.138801	140.814870	47.911860
2002.574604	141.779873	47.916865
1998.623457	147.871249	47.921869
1995.159905	137.125075	47.926874
1991.441323	147.768738	47.931879
1988.120511	139.588159	47.936884
1984.955181	147.699901	47.941889
1981.147618	149.223847	47.946893
1978.028209	142.547740	47.951898
1974.078124	152.197715	47.956903
1970.748094	139.526924	47.961908
1967.259449	144.943564	47.966913
1964.103686	140.133185	47.971917
1960.481073	140.221276	47.976922
1956.825009	141.654426	47.981927
1953.288907	132.791059	47.986932
1949.632155	133.831632	47.991937
1946.100381	140.852668	47.996941
1942.834901	130.783147	48.001946
1939.132457	140.107551	48.006951
1936.158121	136.245324	48.011956
1932.464175	145.892155	48.016961
1928.386109	141.921371	48.021965
1925.394058	137.753455	48.026970
1921.431658	139.192211	48.031975
1918.461460	139.017117	48.036980
1914.915366	134.963718	48.041985
1911.083835	142.730459	48.046989
1907.582712	144.130083	48.051994
1904.222853	151.467215	48.056999
1901.287950	135.631068	48.062004
1897.452941	144.541365	48.067009
1893.664951	143.459883	48.072013
1890.541177	133.490851	48.077018
1886.797080	141.019147	48.082023
1883.391549	139.045287	48.087028
1879.570691	142.773397	48.092033
1876.016595	137.471239	48.097037
1872.710623	134.577488	48.102042
1868.911386	136.293347	48.107047
1865.780288	139.415988	48.112052
1862.503132	140.587511	48.117057
1858.665736	131.504412	48.122061
1855.850509	142.164226	48.127066
1851.998873	141.279617	48.132071
1848.311188	130.645328	48.137076
1844.590924	128.072854	48.142081
1840.793880	134.572372	48.147085
1837.996597	127.533580	48.152090
1834.003733	139.095437	48.157095
1830.662955	128.807815	48.162100
1827.208265	136.824550	48.167105
1823.680163	142.229096	48.172109
1820.415557	126.642051	48.177114
1816.630666	135.447411	48.182119
1813.539451	136.690768	48.187124
1809.619308	126.889521	48.192129
1806.301045	138.399384	48.197133
1802.946372	136.793679	48.202138
1799.333534	139.636868	48.207143
1795.845769	134.289060	48.212148
1792.310965	144.924718	48.217153
1788.494174	131.113479	48.222157
1785.099217	138.359225	48.227162
1781.748115	141.852482	48.232167
1778.150811	135.623985	48.237172
1774.774128	138.367470	48.242177
1770.731303	135.062148	48.247181
1767.679597	131.917758	48.252186
1764.037552	137.252634	48.257191
1760.962734	134.111488	48.262196
1756.913872	122.403475	48.267201
1753.733769	126.099881	48.272205
1750.417186	130.279098	48.277210
1746.863972	133.956450	48.282215
1743.470946	122.970128	48.287220
1739.583377	134.498033	48.292225
1735.497001	141.626757	48.297229
1732.684423	136.528604	48.302234
1729.132108	139.489891	48.307239
1725.716841	125.391943	48.312244
1722.413387	130.845170	48.317249
1718.463444	133.198282	48.322253
1715.122088	124.676225	48.327258
1711.506251	133.221187	48.332263
1708.119319	128.390934	48.337268
1704.452010	124.034392	48.342273
1701.363401	127.528992	48.347277
1698.032192	117.689642	48.352282
1694.259360	139.120167	48.357287
1690.981439	127.826306	48.362292
1687.213647	136.242559	48.367297
1683.203971	145.418795	48.372301
1680.227732	129.553197	48.377306
1676.320636	135.012993	48.382311
1673.202960	127.319798	48.387316
1669.678044	128.845520	48.392321
1666.133391	139.434359	48.397325
1662.812663	137.418214	48.402330
1659.157933	141.137137	48.407335
1655.615472	128.736110	48.412340
1652.635036	125.882906	48.417345
1648.424666	137.679499	48.422349
1645.053168	124.389369	48.427354
1641.742273	134.889149	48.432359
1638.003018	131.143311	48.437364
1634.480377	135.902017	48.442369
1630.926839	127.889605	48.447373
1627.727629	124.057206	48.452378
1623.913667	130.681867	48.457383
1620.840985	138.264439	48.462388
1617.295043	131.877410	48.467393
1613.270663	130.564447	48.472397
1609.752520	112.447004	48.477402
1606.218174	129.373347	48.482407
1603.530296	126.646910	48.487412
1599.713567	133.647579	48.492417
1596.320433	135.515204	48.497421
1592.866961	128.636502	48.502426
1588.867257	130.705735	48.507431
1585.702712	123.557533	48.512436
1581.930531	130.714816	48.517441
1578.344533	132.187202	48.522445
1575.227805	123.813921	48.527450
1571.679858	127.987632	48.532455
1568.060340	127.330819	48.537460
1564.444497	130.798680	48.542465
1560.524439	127.246289	48.547469
1557.529105	117.544176	48.552474
1554.177868	134.755738	48.557479
1551.166628	124.917537	48.562484
1547.143371	123.499276	48.567489
1543.461309	131.562808	48.572493
1540.288273	124.725473	48.577498
1536.232850	128.453318	48.582503
1533.079987	124.978185	48.587508
1529.731209	116.286840	48.592513
1525.742760	123.154032	48.597517
1522.446089	123.630498	48.602522
1518.815132	129.008931	48.607527
1515.513058	123.775835	48.612532
1512.035196	123.363171	48.617537
1508.748886	122.689444	48.622541
1505.156464	122.100421	48.627546
1501.440890	126.621075	48.632551
1498.190371	122.642781	48.637556
1494.605940	119.200961	48.642561
1490.508965	132.555989	48.647565
1487.544544	124.473460	48.652570
1483.915815	123.360042	48.657575
1480.558270	113.812189	48.662580
1476.574869	124.745254	48.667585
1473.129458	123.308800	48.672589
1470.205131	124.204863	48.677594
1466.453974	117.584430	48.682599
1463.237008	115.556976	48.687604
1459.368782	121.078206	48.692609
1455.940079	116.636360	48.697613
1452.514785	123.061739	48.702618
1448.913374	120.741860	48.707623
1445.540555	121.653313	48.712628
1441.964681	121.970919	48.717633
1438.201550	127.791464	48.722637
1434.920293	118.777813	48.727642
1431.352411	122.596983	48.732647
1427.666903	117.996271	48.737652
1424.385742	124.257860	48.742657
1420.959023	126.274069	48.747661
1417.441180	119.705174	48.752666
1414.286798	121.780614	48.757671
1410.235863	126.807677	48.762676
1406.698424	119.760744	48.767681
1403.382024	121.187982	48.772685
1400.291778	125.172660	48.777690
1396.589710	132.234215	48.782695
1393.166245	119.750582	48.787700
1389.600756	132.468373	48.792705
1385.665679	124.166450	48.797709
1382.153278	121.186984	48.802714
1378.608219	122.586057	48.807719
1375.449885	121.311844	48.812724
1372.120698	118.862627	48.817729
1368.805709	121.539376	48.822733
1364.918061	126.927558	48.827738
1361.080817	117.762679	48.832743
1357.717171	122.971803	48.837748
1354.236140	112.704944	48.842753
1350.923919	124.238584	48.847757
1347.667141	109.442033	48.852762
1343.838020	129.389694	48.857767
1340.265185	116.608447	48.862772
1336.736871	113.521551	48.867777
1333.183014	109.515965	48.872781
1329.925352	116.094788	48.877786
1326.372714	116.721221	48.882791
1323.003625	118.946007	48.887796
1319.336710	117.792900	48.892801
1315.525186	125.264582	48.897805
1312.365223	113.921925	48.902810
1308.800051	121.446286	48.907815
1305.352602	120.365717	48.912820
1301.848407	115.392681	48.917825
1297.999267	121.008969	48.922829
1295.120967	115.448457	48.927834
1291.286790	125.386644	48.932839
1287.835250	118.638748	48.937844
1284.662037	118.953444	48.942849
1280.759511	125.064638	48.947853
1277.567976	113.616545	48.952858
1273.689679	123.931672	48.957863
1270.001173	112.819597	48.962868
1266.695061	121.486207	48.967873
1263.058732	117.551592	48.972877
1259.920955	117.015052	48.977882
1256.138578	119.632078	48.982887
1252.892893	120.006971	48.987892
1249.702033	109.502446	48.992897
1245.485710	119.043090	48.997901
1242.328160	117.269207	49.002906
1239.008444	117.266855	49.007911
1235.264908	126.651335	49.012916
1231.772184	111.539033	49.017921
1227.911628	125.018660	49.022925
1224.767506	108.759257	49.027930
1220.828497	126.090833	49.032935
1217.338745	116.875567	49.037940
1214.166463	119.778789	49.042945
1210.804619	119.072457	49.047949
1207.400883	117.083896	49.052954
1203.754773	124.670513	49.057959
1200.323561	121.044897	49.062964
1197.082718	123.828082	49.067969
1193.515842	127.313403	49.072973
1190.298770	109.937583	49.077978
1185.849537	123.697043	49.082983
1182.655110	116.254405	49.087988
1179.302675	111.840615	49.092993
1175.496804	116.184336	49.097997
1172.181095	115.625092	49.103002
1168.700081	110.934867	49.108007
1165.286728	116.310454	49.113012
1161.824261	110.557280	49.118017
1158.120026	118.538969	49.123021
1155.035311	116.663288	49.128026
1151.284829	107.365254	49.133031
1147.604663	112.790844	49.138036
1144.291121	116.972005	49.143041
1140.505247	116.017193	49.148045
1137.221377	113.196584	49.153050
1133.438861	112.362977	49.158055
1130.080072	114.817096	49.163060
1126.687249	110.296588	49.168065
1122.741159	118.767566	49.173069
1119.596949	109.659450	49.178074
1116.134193	123.214261	49.183079
1112.930732	120.368885	49.188084
1109.251809	119.338935	49.193089
1105.159129	117.594816	49.198093
1102.476241	110.158548	49.203098
1098.647698	120.520824	49.208103
1095.306627	112.711286	49.213108
1091.848347	109.444477	49.218113
1088.096179	122.085526	49.223117
1084.554284	102.298628	49.228122
1081.036508	114.654119	49.233127
1077.298347	112.844498	49.238132
1074.214630	100.679368	49.243137
1070.456870	112.403753	49.248141
1067.084469	108.393373	49.253146
1063.694908	118.595618	49.258151
1059.705525	103.100013	49.263156
1056.739748	115.363536	49.268161
1053.173594	119.320879	49.273165
1049.549157	116.311769	49.278170
1046.292258	117.748571	49.283175
1042.667489	120.275710	49.288180
1039.267544	119.464947	49.293185
1035.173342	115.588378	49.298189
1032.190329	107.707253	49.303194
1028.473413	117.991274	49.308199
1025.332620	108.992395	49.313204
1021.819760	107.982924	49.318209
1017.920391	114.885931	49.323213
1014.627512	107.828405	49.328218
1010.783501	114.418142	49.333223
1007.242450	113.056782	49.338228
1004.552089	109.577966	49.343233
1000.563662	113.778095	49.348237
996.909770	102.946117	49.353242
993.679623	117.658844	49.358247
989.974577	113.920604	49.363252
986.895718	110.847264	49.368257
982.770279	117.787426	49.373261
979.178525	105.825878	49.378266
975.947408	111.748379	49.383271
972.741000	106.646321	49.388276
969.005975	109.999309	49.393281
965.157172	114.608857	49.398285
962.406491	103.191903	49.403290
958.799929	111.892420	49.408295
954.861062	104.045674	49.413300
951.447454	112.393312	49.418305
947.744912	104.930238	49.423309
944.322041	110.832688	49.428314
940.964740	113.775117	49.433319
937.458328	111.495013	49.438324
934.246522	104.890209	49.443329
930.465971	111.067520	49.448333
927.007468	110.813584	49.453338
923.461230	103.029582	49.458343
919.855704	106.881489	49.463348
916.725964	99.334632	49.468353
912.924880	109.759206	49.473357
909.717431	102.529933	49.478362
906.017641	108.763322	49.483367
902.440380	99.696500	49.488372
898.948671	104.067267	49.493377
895.366849	105.337899	49.498381
892.201979	99.382464	49.503386
888.136321	100.942973	49.508391
885.050108	102.905294	49.513396
881.712598	101.649981	49.518401
877.761382	110.496571	49.523405
874.365457	104.916938	49.528410
870.710496	110.131391	49.533415
867.195492	103.597496	49.538420
864.078682	103.876138	49.543425
860.377318	105.457906	49.548429
857.151111	102.932854	49.553434
853.592352	105.526955	49.558439
849.777561	109.607047	49.563444
846.835379	98.065890	49.568449
842.729236	115.896544	49.573453
839.127729	107.683324	49.578458
835.514852	104.621200	49.583463
832.181386	113.750685	49.588468
829.153645	97.580703	49.593473
825.235015	99.591457	49.598477
822.084726	98.169750	49.603482
818.476248	113.675722	49.608487
814.390685	108.550822	49.613492
811.546131	99.613673	49.618497
807.942953	107.418259	49.623501
804.303041	96.590287	49.628506
800.897536	108.500722	49.633511
797.562251	107.919005	49.638516
793.893532	111.244575	49.643521
790.661491	108.683054	49.648525
787.123150	104.845124	49.653530
783.289301	102.488493	49.658535
779.666701	109.664272	49.663540
776.720145	107.193111	49.668545
772.492250	109.187178	49.673549
769.151971	102.408494	49.678554
765.737857	103.393687	49.683559
762.400666	110.410017	49.688564
759.319699	102.668723	49.693569
755.373988	108.659111	49.698573
751.653883	104.147110	49.703578
748.476723	106.987375	49.708583
744.772992	105.781732	49.713588
741.254873	101.897077	49.718593
737.415672	113.031231	49.723597
734.046274	111.645182	49.728602
730.639803	104.180149	49.733607
727.167503	114.493276	49.738612
724.030549	104.216902	49.743617
720.533499	104.307386	49.748621
717.094999	102.500668	49.753626
713.654316	99.777312	49.758631
710.110340	105.575741	49.763636
706.468550	99.746616	49.768641
702.824679	103.436365	49.773645
699.480847	100.391867	49.778650
695.504360	93.216474	49.783655
691.950927	94.676360	49.788660
688.735741	89.166556	49.793665
684.734697	92.493921	49.798669
681.416136	91.909136	49.803674
678.027308	111.038865	49.808679
674.645054	102.522031	49.813684
671.142151	103.859883	49.818689
667.791055	98.328852	49.823693
664.483606	90.213618	49.828698
660.815941	97.165902	49.833703
657.194691	102.164197	49.838708
653.615641	99.730664	49.843713
649.925588	108.911996	49.848717
646.684283	102.347873	49.853722
643.465308	103.535995	49.858727
640.059319	100.767678	49.863732
636.472222	99.853181	49.868737
632.662357	96.004840	49.873741
629.215187	95.244913	49.878746
625.274884	97.690046	49.883751
621.908795	102.929571	49.888756
619.027490	94.562469	49.893761
615.401756	99.671657	49.898765
612.060474	97.089166	49.903770
608.432315	96.964133	49.908775
604.387537	103.060507	49.913780
601.052536	92.246852	49.918785
597.353927	103.759745	49.923789
593.951862	102.512448	49.928794
590.748382	104.774488	49.933799
587.158982	99.614622	49.938804
583.842832	97.737786	49.943809
580.113310	105.720427	49.948813
576.731305	98.297266	49.953818
572.876375	101.476757	49.958823
569.343542	95.884436	49.963828
566.428459	101.438253	49.968833
562.609186	104.423578	49.973837
559.403272	105.172709	49.978842
555.855762	98.379309	49.983847
552.160314	109.613482	49.988852
548.715306	92.965276	49.993857
544.744396	104.064044	49.998861
541.705241	93.295643	50.003866
538.491885	91.982724	50.008871
534.252418	95.677804	50.013876
531.268498	90.518086	50.018881
527.251559	102.325634	50.023885
523.969861	96.746511	50.028890
520.467585	100.969389	50.033895
516.860403	98.080879	50.038900
513.800837	93.854686	50.043905
510.276077	96.760762	50.048909
506.838215	99.695823	50.053914
503.322384	99.214996	50.058919
499.463686	101.311439	50.063924
496.251113	104.170812	50.068929
492.203311	104.114598	50.073933
488.929762	104.330779	50.078938
485.382489	89.463384	50.083943
481.886190	103.108689	50.088948
478.446484	96.415075	50.093953
474.795831	107.113220	50.098957
471.587847	101.958795	50.103962
468.219638	101.839070	50.108967
464.529872	103.953271	50.113972
461.255015	98.790822	50.118977
457.698717	105.667371	50.123981
453.814663	92.047631	50.128986
450.427360	90.663435	50.133991
446.951243	90.489626	50.138996
443.773841	102.037046	50.144001
440.098366	102.178145	50.149005
436.827333	95.609884	50.154010
433.230343	95.305797	50.159015
429.225888	94.390373	50.164020
425.826912	91.109413	50.169025
422.312666	102.104818	50.174029
419.138785	95.408551	50.179034
415.483380	92.820597	50.184039
412.012551	105.388442	50.189044
408.861553	104.307206	50.194049
405.205233	104.558030	50.199053
401.614205	103.107867	50.204058
398.049338	92.369104	50.209063
394.164490	100.406719	50.214068
390.678086	94.196519	50.219073
387.059893	95.976466	50.224077
383.892962	94.778710	50.229082
380.423559	99.758348	50.234087
376.831923	83.543174	50.239092
373.754182	92.094181	50.244097
369.687274	98.345229	50.249101
366.617284	99.026755	50.254106
363.218255	99.473259	50.259111
359.160003	100.666061	50.264116
355.643067	100.378153	50.269121
352.329135	98.887928	50.274125
348.941677	91.029798	50.279130
345.688277	89.020607	50.284135
341.620223	89.704362	50.289140
338.682255	86.058800	50.294145
335.100844	94.228396	50.299149
331.519980	92.246976	50.304154
327.935066	88.679689	50.309159
324.525284	94.434848	50.314164
321.107067	88.608649	50.319169
317.424413	89.875455	50.324173
313.971827	84.373664	50.329178
310.625429	85.495422	50.334183
306.726495	105.256554	50.339188
303.151391	93.213061	50.344193
299.321000	96.835900	50.349197
296.409716	92.876325	50.354202
292.968925	97.489577	50.359207
289.299155	92.787560	50.364212
286.168299	97.717154	50.369217
282.222683	91.376157	50.374221
278.744675	93.023793	50.379226
275.261594	97.989219	50.384231
271.357805	99.154480	50.389236
268.308294	97.387946	50.394241
264.775931	95.503514	50.399245
261.258572	90.497969	50.404250
257.987489	99.279702	50.409255
254.482020	88.620421	50.414260
250.938352	88.956478	50.419265
247.143283	91.830745	50.424269
243.840745	92.741432	50.429274
240.351235	93.507563	50.434279
236.867784	92.235047	50.439284
233.499528	86.580403	50.444289
229.719027	95.460608	50.449293
226.522620	89.822605	50.454298
223.012943	95.156177	50.459303
219.142225	93.739049	50.464308
215.940432	90.171561	50.469313
212.135356	95.968816	50.474317
208.860885	98.852131	50.479322
205.202795	106.853635	50.484327
201.444261	98.104588	50.489332
198.533229	91.995129	50.494337
194.926303	86.088128	50.499341
191.274232	95.652686	50.504346
188.194684	95.242929	50.509351
184.072187	92.737755	50.514356
180.226006	86.168224	50.519361
176.976729	86.961786	50.524365
173.890431	89.824320	50.529370
170.513515	91.203267	50.534375
166.822706	98.910689	50.539380
163.359647	93.634953	50.544385
159.687304	92.769222	50.549389
156.290427	97.025429	50.554394
152.854692	88.375143	50.559399
149.087526	90.956176	50.564404
145.635959	84.471871	50.569409
142.052554	90.960509	50.574413
138.688978	90.022180	50.579418
135.429562	84.387038	50.584423
131.821144	100.670621	50.589428
128.795421	89.348244	50.594433
125.135723	92.184745	50.599437
121.116379	92.876828	50.604442
117.603750	91.937437	50.609447
113.471100	94.327841	50.614452
110.516040	83.443263	50.619457
106.930981	79.191882	50.624461
103.502668	84.775670	50.629466
100.227216	85.942658	50.634471
96.364204	91.481283	50.639476
93.236925	84.891241	50.644481
89.901045	86.259099	50.649485
86.236312	84.588450	50.654490
83.031774	93.148313	50.659495
79.238760	75.936494	50.664500
75.715313	73.869027	50.669505
72.102402	84.200909	50.674509
68.697596	91.004867	50.679514
65.102839	91.940006	50.684519
61.416923	91.569958	50.689524
58.233323	81.254232	50.694529
54.694164	89.608856	50.699533
51.155170	83.457472	50.704538
47.633017	80.958452	50.709543
43.868128	96.100698	50.714548
40.514881	79.925819	50.719553
37.015947	79.939312	50.724557
33.550541	81.940078	50.729562
30.347846	86.032500	50.734567
26.405157	86.380627	50.739572
22.972417	82.636611	50.744577
19.804998	73.489791	50.749581
16.199756	88.063057	50.754586
13.001180	87.690992	50.759591
8.998865	92.172274	50.764596
5.450142	74.770169	50.769601
1.669572	90.518884	50.774605