Fri Jun 17 17:51:21 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.281957	79.799173	0.000000
0.044009	82.410185	0.005005
0.195427	84.821503	0.010010
-0.157692	72.692548	0.015014
-0.126122	81.490248	0.020019
0.194672	87.041747	0.025024
-0.015625	88.925737	0.030029
-0.089116	64.154329	0.035034
-0.634442	58.268493	0.040038
-0.790042	53.871062	0.045043
-0.828204	49.608424	0.050048
-1.325146	50.199003	0.055053
-1.744145	25.241780	0.060058
-2.141885	16.583222	0.065062
-2.620765	18.214275	0.070067
-2.588964	15.492210	0.075072
-2.896559	13.858000	0.080077
-3.277852	9.324249	0.085082
-3.464340	6.413909	0.090086
-3.848052	13.525157	0.095091
-4.441541	9.470472	0.100096
-4.989761	11.501395	0.105101
-5.293021	3.306453	0.110106
-4.689430	0.639317	0.115110
-5.306636	13.376752	0.120115
-5.268756	2.400186	0.125120
-5.457799	3.364435	0.130125
-5.489277	0.784114	0.135130
-6.185900	1.421302	0.140134
-6.722574	0.966128	0.145139
-6.834488	7.610898	0.150144
-7.033831	12.377026	0.155149
-7.135290	7.330868	0.160154
-6.898336	7.138602	0.165158
-7.260062	13.499897	0.170163
-8.047855	7.406737	0.175168
-8.152618	11.833918	0.180173
-8.753904	9.723631	0.185178
-8.517896	9.684649	0.190182
-8.613294	9.815798	0.195187
-9.051876	6.582302	0.200192
-9.735386	18.965310	0.205197
-10.133300	8.684147	0.210202
-10.055505	14.134130	0.215206
-10.084355	3.106102	0.220211
-9.975577	6.606648	0.225216
-10.402980	10.372930	0.230221
-11.267102	16.244494	0.235226
-11.294101	4.644890	0.240230
-11.693160	11.740534	0.245235
-11.514530	7.369255	0.250240
-11.708921	20.276170	0.255245
-11.684131	4.242847	0.260250
-12.184642	10.927546	0.265254
-12.667937	2.698596	0.270259
-13.013025	3.652277	0.275264
-13.233288	8.855019	0.280269
-13.419608	4.431729	0.285274
-13.504255	8.699676	0.290278
-14.353850	6.305861	0.295283
-14.606302	4.439505	0.300288
-14.747884	-0.437382	0.305293
-14.570925	2.504044	0.310298
-14.560539	0.954125	0.315302
-14.650182	5.772660	0.320307
-14.792542	-3.349830	0.325312
-15.998513	17.611685	0.330317
-16.141911	1.447670	0.335322
-16.103275	11.021433	0.340326
-16.337208	10.457726	0.345331
-16.307842	4.082123	0.350336
-17.597816	11.615538	0.355341
-17.801524	10.251372	0.360346
-18.057131	3.600900	0.365350
-17.473982	19.073097	0.370355
-17.660221	10.385703	0.375360
-17.787312	10.361691	0.380365
-17.777761	6.247814	0.385370
-18.260461	13.415970	0.390374
-19.241008	6.209357	0.395379
-19.152078	-0.112605	0.400384
-19.318162	6.932077	0.405389
-19.550315	8.463710	0.410394
-20.456808	2.342730	0.415398
-20.841918	12.586614	0.420403
-20.588695	4.628317	0.425408
-20.767148	20.524684	0.430413
-21.106713	4.202655	0.435418
-20.997932	11.516193	0.440422
-21.133808	16.829424	0.445427
-20.990838	14.780520	0.450432
-21.804728	10.356765	0.455437
-22.333801	9.627818	0.460442
-22.287683	13.925927	0.465446
-22.704553	15.820963	0.470451
-22.839635	2.701146	0.475456
-23.450729	9.149868	0.480461
-24.047539	10.869987	0.485466
-23.816715	13.230008	0.490470
-24.357559	17.901947	0.495475
-23.890673	9.752242	0.500480
-24.375114	10.331668	0.505485
-24.489139	13.809854	0.510490
-24.442019	6.060059	0.515494
-25.645110	12.550160	0.520499
-25.761945	4.333901	0.525504
-25.956163	13.493303	0.530509
-26.146623	5.153915	0.535514
-26.307353	4.097938	0.540518
-26.328022	9.395766	0.545523
-25.981803	7.297291	0.550528
-26.679135	9.138506	0.555533
-27.124113	8.328094	0.560538
-27.249403	8.456911	0.565542
-27.531064	18.650649	0.570547
-28.094634	7.998027	0.575552
-28.636259	6.536511	0.580557
-28.801434	11.261637	0.585562
-28.952177	5.926694	0.590566
-29.133000	11.069207	0.595571
-28.946520	12.324649	0.600576
-29.499878	5.351311	0.605581
-29.315620	8.058873	0.610586
-29.741789	1.095771	0.615590
-30.361277	5.304033	0.620595
-30.639468	-4.750357	0.625600
-30.664251	14.440717	0.630605
-30.645159	6.398798	0.635610
-31.271385	8.695074	0.640614
-31.755188	13.445145	0.645619
-32.014604	7.493260	0.650624
-32.137309	4.988092	0.655629
-32.410882	9.638689	0.660634
-32.313427	3.153499	0.665638
-32.874955	1.237292	0.670643
-32.223035	3.685374	0.675648
-32.790075	9.483680	0.680653
-33.225269	4.721508	0.685658
-33.388979	8.191179	0.690662
-34.481342	8.454901	0.695667
-34.693314	3.050415	0.700672
-34.681148	2.631290	0.705677
-34.876631	10.532533	0.710682
-35.158176	-0.808479	0.715686
-35.732431	13.063366	0.720691
-35.572998	10.301735	0.725696
-35.213947	14.893743	0.730701
-35.261726	11.815704	0.735706
-35.986576	5.634934	0.740710
-36.466023	11.463671	0.745715
-36.641380	10.888057	0.750720
-36.931188	4.733241	0.755725
-37.229811	3.319934	0.760730
-37.659864	5.145333	0.765734
-38.380246	5.611643	0.770739
-38.102078	10.228145	0.775744
-38.984769	2.015866	0.780749
-38.409364	1.670844	0.785754
-38.191597	4.320739	0.790758
-38.359310	9.396151	0.795763
-38.857070	7.566627	0.800768
-39.556633	9.678754	0.805773
-39.536924	8.358159	0.810778
-39.703540	11.453191	0.815782
-40.301639	7.557143	0.820787
-40.771640	6.429247	0.825792
-41.157464	15.911364	0.830797
-41.398495	7.012074	0.835802
-41.500832	-0.819430	0.840806
-41.586221	5.231309	0.845811
-41.756691	8.427816	0.850816
-41.699760	13.881462	0.855821
-41.710887	20.038062	0.860826
-41.845700	4.303392	0.865830
-42.962977	8.261510	0.870835
-42.834603	11.390384	0.875840
-43.365203	8.929144	0.880845
-43.400617	5.623899	0.885850
-43.922981	9.829437	0.890854
-44.481496	13.936993	0.895859
-44.737596	6.499656	0.900864
-44.529941	5.954501	0.905869
-44.783151	17.110815	0.910874
-44.775414	9.362633	0.915878
-44.878684	9.328347	0.920883
-45.189832	13.515154	0.925888
-46.004058	0.527379	0.930893
-46.293670	8.138605	0.935898
-46.180227	-1.527028	0.940902
-46.356026	18.044737	0.945907
-46.312191	7.286415	0.950912
-47.182421	8.016404	0.955917
-47.820371	7.113559	0.960922
-48.025117	8.973729	0.965926
-47.816099	7.633308	0.970931
-47.789331	-1.831836	0.975936
-47.756301	8.565913	0.980941
-48.000089	15.024818	0.985946
-48.474169	7.349233	0.990950
-49.258929	15.460517	0.995955
-49.167606	3.895515	1.000960
-49.507184	8.099280	1.005965
-49.620939	9.919067	1.010970
-50.326278	-1.801403	1.015974
-50.599354	-2.962822	1.020979
-50.761135	9.413962	1.025984
-50.901236	0.107386	1.030989
-51.263269	8.990202	1.035994
-50.845930	-4.278463	1.040998
-51.337065	5.924237	1.046003
-51.400804	-2.954197	1.051008
-52.258192	-0.906211	1.056013
-52.241999	3.737063	1.061018
-52.509622	-2.811950	1.066022
-52.887797	0.545571	1.071027
-52.865436	3.818159	1.076032
-53.025194	15.046550	1.081037
-54.199763	5.110779	1.086042
-54.194589	-0.029465	1.091046
-54.399680	2.682434	1.096051
-54.595970	-0.919686	1.101056
-54.408033	5.741736	1.106061
-54.514703	2.253573	1.111066
-54.435434	2.886108	1.116070
-55.233406	2.028217	1.121075
-55.781081	-5.127794	1.126080
-56.204352	10.738612	1.131085
-56.159587	7.499957	1.136090
-55.993021	-5.461809	1.141094
-56.411645	-1.101447	1.146099
-56.363509	5.227824	1.151104
-57.117205	-1.769426	1.156109
-57.722192	-1.196005	1.161114
-57.623512	-4.135195	1.166118
-57.890929	4.330720	1.171123
-57.745581	-4.558791	1.176128
-57.544014	-0.051708	1.181133
-58.169027	6.622313	1.186138
-58.560272	5.554734	1.191142
-59.026671	5.747557	1.196147
-59.520929	5.723608	1.201152
-59.763357	2.172373	1.206157
-60.317878	11.472967	1.211162
-60.221915	5.310659	1.216166
-60.789165	12.845104	1.221171
-60.728287	10.712365	1.226176
-61.124773	6.749063	1.231181
-61.140167	9.483694	1.236186
-61.129633	1.964349	1.241190
-61.330120	8.559511	1.246195
-61.159681	1.845720	1.251200
-62.065876	-4.703695	1.256205
-62.639264	7.994092	1.261210
-62.455462	-3.339024	1.266214
-62.923756	11.544868	1.271219
-62.586831	5.230617	1.276224
-62.928893	-3.986142	1.281229
-63.985034	-0.891632	1.286234
-64.117018	-8.442336	1.291238
-64.267637	7.777346	1.296243
-64.385185	3.873642	1.301248
-64.571761	4.392506	1.306253
-64.600294	1.514126	1.311258
-64.521151	9.029124	1.316262
-65.420307	8.749852	1.321267
-65.573976	13.960863	1.326272
-65.687681	3.917808	1.331277
-65.786931	15.357148	1.336282
-65.867711	6.467927	1.341286
-66.773937	9.256719	1.346291
-67.312592	2.527411	1.351296
-67.299722	6.779737	1.356301
-67.479818	11.201286	1.361306
-67.358630	4.136148	1.366310
-67.279505	10.719165	1.371315
-67.674127	5.868560	1.376320
-68.156456	0.570590	1.381325
-68.807204	4.188119	1.386330
-68.489155	6.040115	1.391334
-69.017324	11.823083	1.396339
-69.579939	3.447692	1.401344
-70.088285	6.952554	1.406349
-70.371154	1.857234	1.411354
-70.434850	4.728356	1.416358
-70.780901	11.468680	1.421363
-70.610321	9.630077	1.426368
-70.609609	10.611722	1.431373
-70.758164	17.968431	1.436378
-70.739083	5.472797	1.441382
-71.413883	2.803081	1.446387
-72.195357	8.969931	1.451392
-71.687655	7.040753	1.456397
-72.404811	15.282879	1.461402
-72.224955	1.938251	1.466406
-73.092027	12.123730	1.471411
-73.419619	5.577384	1.476416
-73.537868	9.445404	1.481421
-73.674147	16.070151	1.486426
-74.027789	4.657067	1.491430
-73.778817	6.527452	1.496435
-73.818249	5.492753	1.501440
-74.562817	-1.817394	1.506445
-75.305979	16.499150	1.511450
-74.988644	2.827583	1.516454
-75.573319	9.087810	1.521459
-75.432949	-1.213356	1.526464
-75.328505	10.065236	1.531469
-75.956831	4.633080	1.536474
-76.374626	-2.395140	1.541478
-76.762906	3.912947	1.546483
-76.656462	4.503866	1.551488
-76.768794	3.238176	1.556493
-76.928429	-1.954587	1.561498
-77.829627	2.556250	1.566502
-78.405741	13.722827	1.571507
-78.716019	-6.600353	1.576512
-78.563381	6.293056	1.581517
-78.603896	9.133487	1.586522
-78.329306	3.439346	1.591526
-78.413770	8.116126	1.596531
-79.005715	3.720019	1.601536
-79.549151	1.106215	1.606541
-79.675641	4.707829	1.611546
-79.906555	-1.572207	1.616550
-80.356272	4.375708	1.621555
-81.228971	0.502430	1.626560
-81.505543	7.903305	1.631565
-81.726434	8.132079	1.636570
-80.724759	10.810701	1.641574
-81.127695	8.399480	1.646579
-81.384303	-0.093868	1.651584
-81.697066	0.581539	1.656589
-82.770488	0.055968	1.661594
-83.218180	-0.879683	1.666598
-83.457375	11.455309	1.671603
-83.350804	-1.549960	1.676608
-83.111428	-2.383558	1.681613
-83.336800	5.275199	1.686618
-82.976999	0.918794	1.691622
-84.240649	6.663995	1.696627
-84.928608	5.515508	1.701632
-84.503825	5.405477	1.706637
-85.070535	17.349154	1.711642
-84.925123	8.009518	1.716646
-84.854824	14.556707	1.721651
-85.905166	8.117293	1.726656
-86.241331	6.945251	1.731661
-86.825100	8.382213	1.736666
-86.765084	-1.388789	1.741670
-86.776487	2.319785	1.746675
-87.169870	3.638075	1.751680
-86.833572	0.751534	1.756685
-86.892627	2.978788	1.761690
-87.002766	3.824155	1.766694
-87.574206	5.723975	1.771699
-88.241323	4.594125	1.776704
-88.328223	5.313876	1.781709
-88.515671	4.642993	1.786714
-88.315129	10.327116	1.791718
-88.944964	9.169559	1.796723
-89.542638	6.811828	1.801728
-89.578823	-2.965280	1.806733
-90.064241	5.443934	1.811738
-90.191536	3.259996	1.816742
-90.368827	12.400202	1.821747
-90.882976	15.224655	1.826752
-90.739762	4.742655	1.831757
-91.190841	14.392298	1.836762
-91.098303	2.867946	1.841766
-91.281359	9.261500	1.846771
-91.791504	6.980582	1.851776
-92.350603	-1.819642	1.856781
-92.729321	17.485120	1.861786
-92.819097	9.490508	1.866790
-93.140365	10.964540	1.871795
-92.998038	12.349464	1.876800
-92.658804	8.505388	1.881805
-93.244305	20.575720	1.886810
-93.924049	7.675117	1.891814
-94.404214	9.736966	1.896819
-94.870164	4.935321	1.901824
-94.489320	7.252636	1.906829
-94.846823	15.472664	1.911834
-94.727516	6.443625	1.916838
-95.757074	14.217332	1.921843
-96.158108	9.937683	1.926848
-96.362488	7.822600	1.931853
-96.425968	12.933569	1.936858
-95.981404	11.510969	1.941862
-96.340710	10.028823	1.946867
-96.062104	14.152713	1.951872
-97.147221	15.859895	1.956877
-97.563415	17.331160	1.961882
-97.786730	13.929284	1.966886
-98.096269	9.765649	1.971891
-97.648756	16.627617	1.976896
-98.271295	-0.316092	1.981901
-98.980586	12.446521	1.986906
-99.092110	7.747370	1.991910
-99.479632	9.797567	1.996915
-99.340550	9.178157	2.006912
-99.324636	14.415481	2.016909
-98.434013	17.072786	2.026906
-98.154294	7.102251	2.036902
-97.995411	6.491097	2.046899
-96.826379	8.550074	2.056896
-96.787137	8.144340	2.066893
-95.949760	7.507326	2.076890
-95.339574	10.675174	2.086886
-95.275974	7.852522	2.096883
-94.767782	10.992080	2.106880
-94.121678	9.245633	2.116877
-93.607349	8.840148	2.126874
-93.186136	3.256709	2.136870
-92.279666	15.166503	2.146867
-92.066168	14.847385	2.156864
-91.859577	12.538581	2.166861
-91.097083	12.663839	2.176858
-90.799165	6.753943	2.186854
-90.255919	6.941731	2.196851
-89.022196	6.556737	2.206848
-89.002764	5.508204	2.216845
-89.013776	13.221949	2.226842
-88.135828	2.910716	2.236838
-87.533425	9.610051	2.246835
-87.286697	11.009903	2.256832
-86.451608	16.785392	2.266829
-86.013757	16.998606	2.276826
-85.823081	15.501545	2.286822
-84.799477	6.169417	2.296819
-84.473255	5.936278	2.306816
-84.358018	11.112832	2.316813
-83.478660	11.477298	2.326810
-83.154975	11.898182	2.336806
-82.739979	10.663759	2.346803
-81.756602	10.251628	2.356800
-81.775283	14.254681	2.366797
-81.258572	9.339195	2.376794
-79.995884	10.521745	2.386790
-79.797833	6.801850	2.396787
-79.706619	11.973309	2.406784
-79.375637	9.971615	2.416781
-78.319799	10.308523	2.426778
-77.994875	12.699684	2.436774
-78.014938	14.962469	2.446771
-76.946436	8.580480	2.456768
-76.620328	5.667560	2.466765
-76.158240	12.954123	2.476762
-75.545728	8.235113	2.486758
-75.123466	5.282301	2.496755
-74.393343	12.091207	2.506752
-73.788725	10.080182	2.516749
-73.644508	11.923260	2.526746
-73.479769	5.030010	2.536742
-72.451386	3.581393	2.546739
-72.231050	2.842267	2.556736
-71.162182	16.720845	2.566733
-70.921969	12.057995	2.576730
-71.072367	14.088357	2.586726
-69.833946	14.785139	2.596723
-69.173574	8.493128	2.606720
-69.263196	12.661298	2.616717
-68.725573	11.253760	2.626714
-67.906596	12.836877	2.636710
-67.733274	12.750867	2.646707
-66.784980	10.370729	2.656704
-66.292181	9.175734	2.666701
-66.145708	7.290267	2.676698
-66.116785	8.793899	2.686694
-64.930830	8.548642	2.696691
-64.608355	4.468618	2.706688
-63.690524	4.830646	2.716685
-63.236288	2.667194	2.726682
-62.905337	5.872773	2.736678
-62.934454	6.838950	2.746675
-62.210193	11.430782	2.756672
-61.999366	9.786928	2.766669
-60.625248	6.537972	2.776666
-60.156200	-2.723495	2.786662
-59.949474	-0.705676	2.796659
-59.970212	3.535210	2.806656
-58.947463	6.277255	2.816653
-58.318698	-2.847165	2.826650
-58.312657	6.814862	2.836646
-57.294062	0.216527	2.846643
-56.899466	-2.913260	2.856640
-56.701491	2.148377	2.866637
-55.936033	2.816104	2.876634
-55.128186	9.538199	2.886630
-55.257827	8.845791	2.896627
-54.991285	4.573532	2.906624
-53.853761	3.078721	2.916621
-53.565318	2.359887	2.926618
-52.733475	10.436763	2.936614
-52.185585	4.414580	2.946611
-51.823965	4.947709	2.956608
-51.843862	6.635305	2.966605
-50.977623	5.732695	2.976602
-50.432824	3.764417	2.986598
-50.265911	6.708007	2.996595
-49.061290	0.390731	3.006592
-48.677808	4.227546	3.016589
-48.784020	8.597438	3.026586
-48.271909	9.527783	3.036582
-47.712983	8.209176	3.046579
-46.986544	13.115397	3.056576
-46.031805	7.217039	3.066573
-45.594793	10.778421	3.076570
-45.571441	4.116727	3.086566
-45.493108	13.819103	3.096563
-44.248534	3.563307	3.106560
-43.994093	-0.877056	3.116557
-43.504285	5.436554	3.126554
-42.669467	10.677641	3.136550
-42.609731	7.350810	3.146547
-42.041565	6.116813	3.156544
-41.420963	8.495972	3.166541
-41.194610	7.005826	3.176538
-40.695613	6.118031	3.186534
-39.550401	-0.168028	3.196531
-39.856452	6.049278	3.206528
-39.331416	4.049512	3.216525
-38.308197	3.396239	3.226522
-37.905069	9.768915	3.236518
-37.057150	7.342441	3.246515
-36.598082	7.869648	3.256512
-36.299219	6.423957	3.266509
-36.262266	4.713180	3.276506
-35.838106	6.381692	3.286502
-34.600322	7.480276	3.296499
-34.533230	8.665386	3.306496
-34.359553	4.259193	3.316493
-33.277289	6.198061	3.326490
-32.962962	8.803784	3.336486
-32.225164	11.610789	3.346483
-31.432712	4.774817	3.356480
-31.600949	5.666712	3.366477
-31.595408	9.701501	3.376474
-30.305531	6.995288	3.386470
-29.670050	3.189246	3.396467
-29.552216	-0.941520	3.406464
-28.680191	3.302116	3.416461
-28.440686	8.109087	3.426458
-28.396454	10.388649	3.436454
-27.438000	5.411595	3.446451
-26.704705	14.759112	3.456448
-26.493694	7.790990	3.466445
-25.816953	3.473071	3.476442
-25.561671	4.827642	3.486438
-25.028935	8.161899	3.496435
-23.784526	13.720587	3.506432
-23.662184	7.238635	3.516429
-23.423977	8.910792	3.526426
-23.419288	9.125282	3.536422
-22.549064	5.601685	3.546419
-21.902474	10.568407	3.556416
-21.366455	10.223738	3.566413
-20.671749	9.389165	3.576410
-20.511589	10.148427	3.586406
-20.176096	8.517442	3.596403
-19.251415	6.218693	3.606400
-18.868431	4.203816	3.616397
-18.519439	3.851905	3.626394
-17.617249	2.734681	3.636390
-16.992465	2.748687	3.646387
-17.020184	1.584503	3.656384
-16.906465	-0.770702	3.666381
-15.955572	3.569683	3.676378
-15.784439	-2.065637	3.686374
-14.814228	7.202192	3.696371
-14.453183	9.368434	3.706368
-13.666584	3.857829	3.716365
-13.111553	1.267448	3.726362
-13.014866	3.313837	3.736358
-12.562573	2.384809	3.746355
-12.075350	2.851028	3.756352
-11.189690	7.660254	3.766349
-11.198708	12.029007	3.776346
-10.209584	5.782137	3.786342
-9.735818	3.960421	3.796339
-9.389700	3.199007	3.806336
-8.777527	4.793592	3.816333
-8.021675	6.607716	3.826330
-7.922351	4.344408	3.836326
-7.757544	7.668499	3.846323
-6.574307	4.816421	3.856320
-6.680109	2.774714	3.866317
-6.161072	5.868424	3.876314
-5.373379	9.302169	3.886310
-4.926600	8.132218	3.896307
-4.577293	18.849588	3.906304
-4.220964	26.596335	3.916301
-3.479003	36.708063	3.926298
-3.246905	45.444611	3.936294
-2.398613	55.818652	3.946291
-2.231332	63.069692	3.956288
-2.027782	78.955790	3.966285
-1.449127	90.155323	3.976282
-0.973697	108.219463	3.986278
0.000000	119.897235	3.991283
-0.260646	132.328639	3.996288
-0.387313	129.408135	4.001293
-0.201831	137.967561	4.006298
0.160569	156.111159	4.011302
0.415772	158.922396	4.016307
0.454596	163.430339	4.021312
0.431559	162.100260	4.026317
0.862127	159.935059	4.031322
0.492384	167.566983	4.036326
0.572112	156.692673	4.041331
0.348699	154.833902	4.046336
0.648618	161.697597	4.051341
0.540197	150.277569	4.056346
0.341742	156.239419	4.061350
0.659655	148.922081	4.066355
0.455518	156.152333	4.071360
0.295528	156.488985	4.076365
0.774605	156.458934	4.081370
0.612220	156.274832	4.086374
0.394855	139.827559	4.091379
0.351164	150.962366	4.096384
0.860664	152.066451	4.101389
1.082227	159.574827	4.106394
0.650013	151.121029	4.111398
0.046798	142.950414	4.116403
0.507281	148.114443	4.121408
0.690532	160.693689	4.126413
0.611322	158.948686	4.131418
0.761712	165.470596	4.136422
1.179449	157.216308	4.141427
0.527764	158.656272	4.146432
0.522585	146.225919	4.151437
0.926301	160.491613	4.156442
0.683405	157.514450	4.161446
0.773454	165.468358	4.166451
0.735036	168.295646	4.171456
0.858483	156.920345	4.176461
0.894750	155.730381	4.181466
0.528921	160.623880	4.186470
0.675675	160.209216	4.191475
0.630713	170.077975	4.196480
0.855130	168.155618	4.201485
0.930437	168.129733	4.206490
0.909244	178.365726	4.211494
1.142972	177.973703	4.216499
0.758044	174.783742	4.221504
0.686519	170.010200	4.226509
0.829055	174.072107	4.231514
0.556898	178.731990	4.236518
1.252480	165.644847	4.241523
0.869954	165.197590	4.246528
0.731038	166.154701	4.251533
0.789695	175.398656	4.256538
0.642835	172.117423	4.261542
1.017580	173.155307	4.266547
0.890404	177.386364	4.271552
1.108078	171.000900	4.276557
1.275824	168.141365	4.281562
1.119799	184.807910	4.286566
0.803671	168.967044	4.291571
0.952711	174.982238	4.296576
1.305000	169.196783	4.301581
1.131174	172.944633	4.306586
0.980629	174.607163	4.311590
0.995578	169.974152	4.316595
0.981992	181.130222	4.321600
0.963353	168.348865	4.326605
1.076179	182.002857	4.331610
0.981934	177.187506	4.336614
1.124928	176.407615	4.341619
1.042776	193.479049	4.346624
1.394597	195.743609	4.351629
1.624960	193.110458	4.356634
1.081357	178.862562	4.361638
1.377992	181.130175	4.366643
0.876764	176.716752	4.371648
0.860175	187.955810	4.376653
1.076209	195.544252	4.381658
1.067940	199.283139	4.386662
1.316835	197.291788	4.391667
1.416773	205.262425	4.396672
1.865830	200.936125	4.401677
1.696509	200.091720	4.406682
1.483132	196.107592	4.411686
1.413069	178.906060	4.416691
1.225184	187.040561	4.421696
1.207592	191.183551	4.426701
1.750814	200.237656	4.431706
1.314742	199.860274	4.436710
1.462183	198.087459	4.441715
1.644983	201.778604	4.446720
1.294813	195.070752	4.451725
1.709646	199.835094	4.456730
1.626349	187.366583	4.461734
1.172864	165.823569	4.466739
1.062167	192.637653	4.471744
1.477835	189.434789	4.476749
1.784157	205.427579	4.481754
1.432581	197.658117	4.486758
1.437486	200.266275	4.491763
1.548819	201.821738	4.496768
1.574592	206.957207	4.501773
1.943702	202.493829	4.506778
1.479882	209.373790	4.511782
1.513398	203.735633	4.516787
1.315112	212.311530	4.521792
1.812682	205.007519	4.526797
1.611078	215.418563	4.531802
1.382317	207.299335	4.536806
1.801749	201.906053	4.541811
2.035778	200.101875	4.546816
2.005067	213.908809	4.551821
1.875563	204.114708	4.556826
1.903314	205.295320	4.561830
1.806931	202.442189	4.566835
1.317765	204.644075	4.571840
1.143216	210.443120	4.576845
1.626919	208.194687	4.581850
1.702920	206.478540	4.586854
1.736773	214.052084	4.591859
1.733619	213.870719	4.596864
1.789723	208.154806	4.601869
1.975257	204.832721	4.606874
1.556462	206.041580	4.611878
1.867503	196.376522	4.616883
1.686408	203.477463	4.621888
1.754462	202.313390	4.626893
1.818054	196.421203	4.631898
1.366921	212.163197	4.636902
2.044390	207.696119	4.641907
2.082078	226.054006	4.646912
1.974644	226.540776	4.651917
2.238077	217.204085	4.656922
1.765845	227.573492	4.661926
2.218117	216.144675	4.666931
1.963811	229.495459	4.671936
2.073564	225.467875	4.676941
2.336313	222.273650	4.681946
2.007125	216.642891	4.686950
1.925096	200.339606	4.691955
1.409674	208.174941	4.696960
1.778273	214.058542	4.701965
2.268999	224.787066	4.706970
1.946455	222.173788	4.711974
2.179826	213.708976	4.716979
1.797861	230.599211	4.721984
1.900237	222.429867	4.726989
1.938601	222.212002	4.731994
1.848370	230.142827	4.736998
2.224270	226.880460	4.742003
2.199566	233.820050	4.747008
2.061155	227.308456	4.752013
2.173790	231.360943	4.757018
2.063262	244.194906	4.762022
2.360824	248.251586	4.767027
2.014092	241.755866	4.772032
2.262773	255.090554	4.777037
2.626091	251.109616	4.782042
2.483097	248.668754	4.787046
2.450957	241.981821	4.792051
2.324661	238.177778	4.797056
1.835648	234.719960	4.802061
2.617611	238.198055	4.807066
2.018060	244.569572	4.812070
2.601582	253.203402	4.817075
2.392550	261.781902	4.822080
2.466369	268.160493	4.827085
2.633493	249.012042	4.832090
2.056143	237.062900	4.837094
2.367147	249.475155	4.842099
2.453028	256.086562	4.847104
2.227132	257.665919	4.852109
2.546461	256.826720	4.857114
2.407247	262.701410	4.862118
2.680360	253.699146	4.867123
2.600211	252.097353	4.872128
2.481442	256.673156	4.877133
2.755386	257.581577	4.882138
2.373414	262.993026	4.887142
2.812667	260.440780	4.892147
2.590897	252.896577	4.897152
2.635950	261.372065	4.902157
2.977545	255.518894	4.907162
2.376571	246.492809	4.912166
2.608738	246.873206	4.917171
2.755100	248.012006	4.922176
2.564401	250.514947	4.927181
2.804720	248.757275	4.932186
2.237828	252.237579	4.937190
2.912998	256.365288	4.942195
2.818434	255.541605	4.947200
2.575479	265.415116	4.952205
2.916508	259.144087	4.957210
2.631994	271.351059	4.962214
2.670172	262.796911	4.967219
2.772448	255.738351	4.972224
2.866499	262.736556	4.977229
2.827874	254.067899	4.982234
2.500765	266.347264	4.987238
2.332934	254.308135	4.992243
2.060219	259.170203	4.997248
2.300677	254.965387	5.002253
2.780830	258.099778	5.007258
2.814037	264.419604	5.012262
2.786589	254.771899	5.017267
2.764220	258.173534	5.022272
2.697799	273.750215	5.027277
3.129962	276.835558	5.032282
2.825259	279.420994	5.037286
2.696955	285.039122	5.042291
2.761473	285.404763	5.047296
2.925910	279.902288	5.052301
3.253158	277.916649	5.057306
3.375775	292.055734	5.062310
3.306785	283.440060	5.067315
2.937703	271.871461	5.072320
2.968126	267.728391	5.077325
3.196576	267.997519	5.082330
2.953099	273.235583	5.087334
3.186988	263.029592	5.092339
2.898423	273.077238	5.097344
3.100202	273.225690	5.102349
3.168433	282.326828	5.107354
3.292310	283.387474	5.112358
3.267594	268.644373	5.117363
3.018062	269.334730	5.122368
3.012320	257.755081	5.127373
3.147953	269.088282	5.132378
3.268881	283.872129	5.137382
3.357293	281.862450	5.142387
2.979405	275.020445	5.147392
3.219015	283.911157	5.152397
3.635200	268.762264	5.157402
2.950308	271.355245	5.162406
2.936152	267.419286	5.167411
2.915785	286.934976	5.172416
3.137905	289.454159	5.177421
3.314252	280.587350	5.182426
2.705866	290.767100	5.187430
3.075540	290.240986	5.192435
3.004147	291.966739	5.197440
2.779395	289.578533	5.202445
3.070073	299.599376	5.207450
3.381976	315.119331	5.212454
3.276959	315.453557	5.217459
3.104165	318.273213	5.222464
3.369518	320.391732	5.227469
3.685285	322.079381	5.232474
3.490714	327.894822	5.237478
3.568140	326.573684	5.242483
3.797238	315.649965	5.247488
3.594051	322.711416	5.252493
3.516081	290.362796	5.257498
3.042487	305.662645	5.262502
3.433067	300.268797	5.267507
3.762454	309.403699	5.272512
3.570047	313.536116	5.277517
3.712837	314.343995	5.282522
3.446728	321.641062	5.287526
3.777540	322.233971	5.292531
3.854153	312.891769	5.297536
3.308593	300.001540	5.302541
3.608286	304.342830	5.307546
3.632810	313.605171	5.312550
3.685907	305.106141	5.317555
3.451745	303.570989	5.322560
3.785047	315.711218	5.327565
3.833205	311.823695	5.332570
3.446764	304.854240	5.337574
4.104118	302.792811	5.342579
3.442210	297.365128	5.347584
3.401041	302.444466	5.352589
3.741974	311.639216	5.357594
3.554187	307.812816	5.362598
3.851251	315.180451	5.367603
3.695320	318.618509	5.372608
3.591045	313.678291	5.377613
3.856150	309.792201	5.382618
3.449005	323.659830	5.387622
4.261147	308.233740	5.392627
3.951974	313.757425	5.397632
3.953255	324.728200	5.402637
3.926005	309.994557	5.407642
3.656561	318.513077	5.412646
3.718550	318.561629	5.417651
3.861736	323.876533	5.422656
3.665026	326.230710	5.427661
3.845142	321.546520	5.432666
3.493300	312.258171	5.437670
4.023972	316.403994	5.442675
4.024684	316.427607	5.447680
3.958502	317.918263	5.452685
3.910003	317.507831	5.457690
3.890241	324.938001	5.462694
3.968432	323.734148	5.467699
4.166715	318.650695	5.472704
3.908215	322.076794	5.477709
3.943706	322.700833	5.482714
3.858996	320.670198	5.487718
3.744555	328.898729	5.492723
3.910236	324.066570	5.497728
4.117776	333.040390	5.502733
4.271039	336.172893	5.507738
4.231727	330.779056	5.512742
3.838460	323.938006	5.517747
4.227608	329.971565	5.522752
4.070599	339.189503	5.527757
4.210950	336.354224	5.532762
4.169616	337.852986	5.537766
4.002699	339.105630	5.542771
4.026968	343.967891	5.547776
3.986098	351.785790	5.552781
4.124634	335.743674	5.557786
4.350087	344.384384	5.562790
4.387821	344.482355	5.567795
4.001714	348.813133	5.572800
3.961512	346.364248	5.577805
4.382086	336.058112	5.582810
4.204419	347.215330	5.587814
4.374834	347.337226	5.592819
4.461257	338.449219	5.597824
4.162494	345.434018	5.602829
4.309974	346.157844	5.607834
4.289734	353.354858	5.612838
4.307209	340.426261	5.617843
4.305227	341.660371	5.622848
4.436183	351.145396	5.627853
4.297699	346.656827	5.632858
3.884127	352.070402	5.637862
4.290275	343.836294	5.642867
4.353086	350.299037	5.647872
4.735216	362.817961	5.652877
4.182379	348.503165	5.657882
4.467143	358.553445	5.662886
4.970449	357.253670	5.667891
4.749741	353.840620	5.672896
4.359661	337.063289	5.677901
4.557063	340.655149	5.682906
4.336071	347.246366	5.687910
4.283760	349.101759	5.692915
4.651521	362.328934	5.697920
4.344452	372.005574	5.702925
4.648546	377.341308	5.707930
4.569539	383.902033	5.712934
4.538942	380.621164	5.717939
4.460776	377.929351	5.722944
4.699677	380.556661	5.727949
4.658442	378.713757	5.732954
4.624179	382.264411	5.737958
4.874871	376.283435	5.742963
4.915797	379.522827	5.747968
4.988273	380.278263	5.752973
5.064693	369.632471	5.757978
4.415549	373.901008	5.762982
4.635257	373.694635	5.767987
4.846320	382.759462	5.772992
4.561017	373.817190	5.777997
4.504947	369.559808	5.783002
4.680557	381.597244	5.788006
4.758311	389.034520	5.793011
4.975766	389.370598	5.798016
4.684073	382.769766	5.803021
4.764209	385.323418	5.808026
4.953366	384.174722	5.813030
4.958068	378.154910	5.818035
4.736964	371.830654	5.823040
4.815159	383.387989	5.828045
4.534294	374.423272	5.833050
4.503927	383.559605	5.838054
4.638192	388.668616	5.843059
4.813742	382.927062	5.848064
5.028962	396.223428	5.853069
5.098617	403.806309	5.858074
4.891356	397.251821	5.863078
5.265728	394.081434	5.868083
4.887928	382.950506	5.873088
4.869956	395.326392	5.878093
5.377314	393.315340	5.883098
4.782209	398.680565	5.888102
5.406413	406.004919	5.893107
5.255111	388.065406	5.898112
4.577930	384.388413	5.903117
5.319286	381.118155	5.908122
5.242192	401.374541	5.913126
4.856819	396.292369	5.918131
4.919011	400.501680	5.923136
4.980605	407.533367	5.928141
5.448359	396.275499	5.933146
5.129970	414.164730	5.938150
5.102199	408.198453	5.943155
5.288837	413.739810	5.948160
5.217989	408.895435	5.953165
5.433365	404.403681	5.958170
5.156093	416.163193	5.963174
5.260821	405.071037	5.968179
4.999566	405.648105	5.973184
5.205381	415.961371	5.978189
5.312446	413.776104	5.983194
5.157117	416.617541	5.988198
5.216128	411.286069	5.993203
5.538913	406.494470	5.998208
4.919161	414.416317	6.003213
5.399286	405.478421	6.008218
5.384827	407.425407	6.013222
5.491363	412.424187	6.018227
5.576670	402.992870	6.023232
5.509227	415.009953	6.028237
5.517959	400.967425	6.033242
5.630702	412.517855	6.038246
5.431066	404.303106	6.043251
5.657759	383.622350	6.048256
5.066718	381.871228	6.053261
5.171189	382.657261	6.058266
5.256352	388.125886	6.063270
5.218336	389.064659	6.068275
5.615520	397.607196	6.073280
5.297345	390.598728	6.078285
5.487538	385.648416	6.083290
5.117938	393.048164	6.088294
5.202549	389.778730	6.093299
5.383216	377.559823	6.098304
4.718926	386.584658	6.103309
5.159103	390.619644	6.108314
5.090163	408.096812	6.113318
5.356245	402.413808	6.118323
5.355136	411.898523	6.123328
5.546473	412.874359	6.128333
5.189117	410.019970	6.133338
5.439799	411.074940	6.138342
5.437311	412.437999	6.143347
5.475183	408.497894	6.148352
5.531751	410.698095	6.153357
5.351259	411.772046	6.158362
5.420088	415.820023	6.163366
5.325644	404.600145	6.168371
5.398390	388.990021	6.173376
4.989171	397.378488	6.178381
5.668751	398.352300	6.183386
5.243427	399.227185	6.188390
4.992922	402.663812	6.193395
5.282327	410.151957	6.198400
5.360865	420.870592	6.203405
5.245668	415.563338	6.208410
5.460111	416.316294	6.213414
5.567406	417.292089	6.218419
5.611537	407.060713	6.223424
5.259167	397.609599	6.228429
5.093762	387.953167	6.233434
5.165204	398.571339	6.238438
5.387435	399.971045	6.243443
5.435305	403.540414	6.248448
5.382654	401.761960	6.253453
5.244044	384.696111	6.258458
5.140620	392.828520	6.263462
5.309844	396.351471	6.268467
5.207156	406.238658	6.273472
4.967842	412.187467	6.278477
5.483314	412.242734	6.283482
5.667660	414.875369	6.288486
5.414856	414.774175	6.293491
5.315652	394.808645	6.298496
5.267362	396.953457	6.303501
5.171578	389.679117	6.308506
5.314019	398.997488	6.313510
5.094121	407.121835	6.318515
5.415094	419.436666	6.323520
5.497034	419.575044	6.328525
5.522429	414.433864	6.333530
5.372096	388.961738	6.338534
5.564228	390.010061	6.343539
5.265387	387.535881	6.348544
5.026894	388.729979	6.353549
5.392710	385.758152	6.358554
5.425546	389.767704	6.363558
4.981799	379.303876	6.368563
5.381726	395.178888	6.373568
5.370379	407.091920	6.378573
5.141153	390.414286	6.383578
5.151392	400.896210	6.388582
5.321320	411.332260	6.393587
5.489468	402.762549	6.398592
5.522822	416.519154	6.403597
5.187436	391.866726	6.408602
5.404131	401.013705	6.413606
5.162492	401.229745	6.418611
5.393107	406.201387	6.423616
5.101376	412.421560	6.428621
5.408549	402.243948	6.433626
5.482396	410.814978	6.438630
5.578702	394.293588	6.443635
5.132670	389.844485	6.448640
4.858079	396.265847	6.453645
4.992440	400.593008	6.458650
5.317600	409.754326	6.463654
5.231564	420.262330	6.468659
5.799119	409.383717	6.473664
5.408196	418.452919	6.478669
5.564287	409.642288	6.483674
5.439545	407.308480	6.488678
4.904615	396.176626	6.493683
5.486466	400.654959	6.498688
5.191767	418.393835	6.503693
5.527250	412.553856	6.508698
5.419221	406.599342	6.513702
4.963596	406.473056	6.518707
5.266038	407.292291	6.523712
5.500517	419.494415	6.528717
5.380698	415.764830	6.533722
5.389760	420.052439	6.538726
5.150917	403.903272	6.543731
5.701519	400.518294	6.548736
5.168000	400.013049	6.553741
5.227279	381.510673	6.558746
5.202410	393.805810	6.563750
5.518090	403.927350	6.568755
5.642597	402.441696	6.573760
5.442711	392.052174	6.578765
5.253679	385.960960	6.583770
5.128571	386.097050	6.588774
4.955916	388.382709	6.593779
5.426442	400.690426	6.598784
5.121280	403.963866	6.603789
5.369316	411.900916	6.608794
5.368787	419.868828	6.613798
5.302190	426.774619	6.618803
5.722482	410.198374	6.623808
5.437232	404.684168	6.628813
5.447103	388.597474	6.633818
5.612024	387.789458	6.638822
5.171555	391.506892	6.643827
5.403287	383.616108	6.648832
5.166447	391.560926	6.653837
5.658146	389.020860	6.658842
5.173511	383.701616	6.663846
5.032812	389.588638	6.668851
5.317641	382.628537	6.673856
5.186668	383.353459	6.678861
5.416804	390.646218	6.683866
5.375230	389.316438	6.688870
5.446978	379.048324	6.693875
5.189528	386.304910	6.698880
5.205242	393.279293	6.703885
5.175728	374.634211	6.708890
5.414724	387.969835	6.713894
5.103443	387.750489	6.718899
5.389345	387.460692	6.723904
5.708565	386.476661	6.728909
5.598936	381.988614	6.733914
5.418223	391.057392	6.738918
5.396175	395.887507	6.743923
5.428193	380.392695	6.748928
5.223866	387.581645	6.753933
5.263142	385.024823	6.758938
5.304701	386.987162	6.763942
5.016331	379.180462	6.768947
5.229997	392.918718	6.773952
5.147629	387.975625	6.778957
5.365101	384.456582	6.783962
5.367310	387.000888	6.788966
5.356314	384.658438	6.793971
5.576657	383.811611	6.798976
5.122951	391.948173	6.803981
4.838730	389.982264	6.808986
5.125049	385.230279	6.813990
5.184941	386.542119	6.818995
4.944330	398.285656	6.824000
5.389670	408.861420	6.829005
5.738818	414.549814	6.834010
5.264119	406.622518	6.839014
5.092169	404.010818	6.844019
5.414096	405.626018	6.849024
5.457261	420.154545	6.854029
5.344363	412.322017	6.859034
5.632962	400.924809	6.864038
5.151548	394.236316	6.869043
5.148745	389.694004	6.874048
5.057339	402.593000	6.879053
5.393496	406.583515	6.884058
5.418251	414.539131	6.889062
5.510990	414.591847	6.894067
5.495446	398.077600	6.899072
5.223301	400.153455	6.904077
5.088154	386.778363	6.909082
5.446107	407.210296	6.914086
5.183885	397.122594	6.919091
5.498351	393.448307	6.924096
5.261524	398.499222	6.929101
5.292236	396.152995	6.934106
5.168594	396.301865	6.939110
5.153022	411.424454	6.944115
5.614273	412.573086	6.949120
5.375854	413.973190	6.954125
5.171041	391.261747	6.959130
5.029143	395.775328	6.964134
5.155440	410.085788	6.969139
5.234141	419.918166	6.974144
5.227667	418.384426	6.979149
5.315430	415.126895	6.984154
5.604932	421.509561	6.989158
5.303698	418.194340	6.994163
5.743095	421.180435	6.999168
5.476232	416.530059	7.004173
5.283130	394.265207	7.009178
5.167995	388.864416	7.014182
5.375851	386.831910	7.019187
5.806953	382.280625	7.024192
5.605248	393.795099	7.029197
5.518622	385.409629	7.034202
5.540652	382.494946	7.039206
5.122765	387.102943	7.044211
5.146477	384.192717	7.049216
5.381084	394.923872	7.054221
5.056509	386.762262	7.059226
5.147819	388.660092	7.064230
5.084721	392.817411	7.069235
5.384874	386.891553	7.074240
5.061286	386.490733	7.079245
5.449755	390.683893	7.084250
5.727163	384.116733	7.089254
5.257536	393.716214	7.094259
5.384135	376.933076	7.099264
5.146248	391.250575	7.104269
5.361209	378.451922	7.109274
5.482628	380.048350	7.114278
4.920799	385.417709	7.119283
5.338365	387.332745	7.124288
5.284247	387.457034	7.129293
5.220135	383.256633	7.134298
5.345594	387.348272	7.139302
4.991000	384.140201	7.144307
5.446864	398.237016	7.149312
5.206763	413.036003	7.154317
5.406881	412.514783	7.159322
5.524136	410.846220	7.164326
5.571927	398.898419	7.169331
5.195515	393.641696	7.174336
4.992255	389.003252	7.179341
5.145993	398.438343	7.184346
5.558364	402.479337	7.189350
5.081092	401.961388	7.194355
5.517045	411.440943	7.199360
5.079991	419.240665	7.204365
5.708211	418.885877	7.209370
5.357702	395.444631	7.214374
5.003391	397.870993	7.219379
5.635056	402.828857	7.224384
5.342331	403.853185	7.229389
5.128203	392.384638	7.234394
5.278701	395.557671	7.239398
5.303420	406.440149	7.244403
5.311551	403.840745	7.249408
5.134724	417.872245	7.254413
5.216433	412.297831	7.259418
5.240553	415.152854	7.264422
5.427171	416.256361	7.269427
5.711692	407.848654	7.274432
5.324593	411.761857	7.279437
5.138239	391.401940	7.284442
5.283895	393.294881	7.289446
4.876340	417.034700	7.294451
5.499278	406.491627	7.299456
5.197684	415.848690	7.304461
5.675500	416.153727	7.309466
5.533000	409.770411	7.314470
5.407845	402.318214	7.319475
5.451381	395.540689	7.324480
5.109872	395.482854	7.329485
5.126789	384.359132	7.334490
5.630922	393.297897	7.339494
5.318233	394.892286	7.344499
5.671335	382.461982	7.349504
5.420442	385.209185	7.354509
5.385435	379.036132	7.359514
5.582843	377.515670	7.364518
5.318398	384.519449	7.369523
5.498163	370.477134	7.374528
5.473953	384.327145	7.379533
5.620680	382.363014	7.384538
5.617413	383.310417	7.389542
5.494204	383.122168	7.394547
5.728853	381.663793	7.399552
5.314389	388.424530	7.404557
5.408669	381.034931	7.409562
5.235598	380.441556	7.414566
4.946164	387.012000	7.419571
5.246616	379.038360	7.424576
5.120481	386.793884	7.429581
5.395635	389.386556	7.434586
5.141760	394.417412	7.439590
4.913480	387.796170	7.444595
5.100683	375.886387	7.449600
5.127107	390.886931	7.454605
5.002925	375.579506	7.459610
5.383860	381.294966	7.464614
5.151340	384.287756	7.469619
5.233935	378.008330	7.474624
5.319628	381.078467	7.479629
5.292934	384.648978	7.484634
5.216373	381.439488	7.489638
4.897769	386.252193	7.494643
5.611979	389.326790	7.499648
5.222278	392.077728	7.504653
5.010344	387.497361	7.509658
5.207941	397.816520	7.514662
5.557400	407.821940	7.519667
5.611489	398.458172	7.524672
4.971309	395.205610	7.529677
5.098871	402.812215	7.534682
5.579431	402.788826	7.539686
5.229945	405.882758	7.544691
5.569066	406.977295	7.549696
5.232681	392.454798	7.554701
5.246910	399.764110	7.559706
5.413096	399.592682	7.564710
5.191309	405.153773	7.569715
5.374291	401.874103	7.574720
5.368938	404.067033	7.579725
5.258150	407.718029	7.584730
5.530161	394.965330	7.589734
5.351421	394.343888	7.594739
5.272441	380.757000	7.599744
5.113583	391.498893	7.604749
4.873633	398.091900	7.609754
5.416334	406.037985	7.614758
5.356958	420.831805	7.619763
5.503497	408.941385	7.624768
5.481169	415.790874	7.629773
5.701920	405.389245	7.634778
5.645305	391.425668	7.639782
5.344958	386.766659	7.644787
5.600336	377.833970	7.649792
5.250612	384.479949	7.654797
5.085511	383.618256	7.659802
5.269587	378.680803	7.664806
5.300561	386.467636	7.669811
5.277021	378.877595	7.674816
5.221199	389.881390	7.679821
5.231741	381.394720	7.684826
5.357110	378.921860	7.689830
5.358901	384.331722	7.694835
5.486764	377.122827	7.699840
5.039022	380.052526	7.704845
5.297145	383.237070	7.709850
5.276213	385.736481	7.714854
5.284431	382.367069	7.719859
5.373454	387.411178	7.724864
5.215377	389.310599	7.729869
5.351446	386.901080	7.734874
5.053420	392.129505	7.739878
5.117952	384.495419	7.744883
5.384115	392.094175	7.749888
5.283496	411.293616	7.754893
5.492583	401.012527	7.759898
5.240600	400.943165	7.764902
4.987122	412.075143	7.769907
5.166012	408.612828	7.774912
5.172817	411.852175	7.779917
5.578200	410.204591	7.784922
5.683244	406.613654	7.789926
5.285393	412.138103	7.794931
5.631305	409.007569	7.799936
5.217662	398.567930	7.804941
5.309662	387.293592	7.809946
5.367512	390.423613	7.814950
5.405854	392.473512	7.819955
5.204920	385.586455	7.824960
5.413000	388.001230	7.829965
4.937882	387.410897	7.834970
5.307594	392.897346	7.839974
5.472079	407.111669	7.844979
5.261757	392.748976	7.849984
4.907523	396.015969	7.854989
5.247994	409.743818	7.859994
5.594852	412.839816	7.864998
5.452041	421.607099	7.870003
5.495254	407.021690	7.875008
5.400312	405.810892	7.880013
5.437094	393.949384	7.885018
5.271045	386.863929	7.890022
4.968118	390.900678	7.895027
5.337140	400.942704	7.900032
5.004657	411.147318	7.905037
5.665625	415.426221	7.910042
5.465779	410.082917	7.915046
5.111437	390.535131	7.920051
5.153065	391.435802	7.925056
5.369755	408.250798	7.930061
5.211850	414.676057	7.935066
5.777476	409.272218	7.940070
5.241556	406.660038	7.945075
5.246064	385.295744	7.950080
5.139759	406.088610	7.955085
5.409884	408.960955	7.960090
5.223187	413.693332	7.965094
5.577381	420.671654	7.970099
5.536778	414.361778	7.975104
5.288774	401.881004	7.980109
4.999227	385.644774	7.985114
5.309904	403.347734	7.990118
5.426415	411.098762	7.995136
5.492740	406.888598	8.000154
5.414173	401.931335	8.005171
5.320016	392.582221	8.010189
5.376336	383.475397	8.015206
4.923510	384.693908	8.020224
5.690285	394.489333	8.025242
5.285088	392.616771	8.030259
5.421025	386.705840	8.035277
5.517769	382.880548	8.040294
5.293609	381.741008	8.045312
5.448073	383.411080	8.050330
5.322444	380.047905	8.055347
5.364127	386.752755	8.060365
5.433870	385.321080	8.065382
5.177924	391.277845	8.070400
5.380883	387.273692	8.075418
5.601469	390.942219	8.080435
5.571620	399.389106	8.085453
5.635163	385.388064	8.090470
5.392774	387.356164	8.095488
5.436554	379.741828	8.100506
5.298421	381.954383	8.105523
5.469588	388.239916	8.110541
5.509423	380.872668	8.115558
5.286216	392.295293	8.120576
5.391237	386.752259	8.125594
5.098603	383.359761	8.130611
4.764373	406.066651	8.135629
5.524530	409.017999	8.140646
5.352107	422.757369	8.145664
5.238495	416.783979	8.150682
5.462701	416.876475	8.155699
5.386343	420.987241	8.160717
5.656822	417.497987	8.165734
5.762381	420.371744	8.170752
5.660423	414.566086	8.175770
5.440124	419.672335	8.180787
5.315841	417.770595	8.185805
5.695551	417.810475	8.190822
5.639645	414.169981	8.195840
5.871446	409.121957	8.200858
5.766492	415.177834	8.205875
5.228038	423.897642	8.210893
5.434631	425.210466	8.215910
5.414202	426.707074	8.220928
5.710817	425.001291	8.225946
5.496115	414.623878	8.230963
5.363107	420.848578	8.235981
5.735367	416.578898	8.240998
5.696435	425.419200	8.246016
5.356121	413.413221	8.251034
5.761675	419.498407	8.256051
5.793558	417.494930	8.261069
5.920309	414.681471	8.266086
5.809333	422.220883	8.271104
5.716163	411.376268	8.276122
5.449707	396.967907	8.281139
5.259912	395.965160	8.286157
5.629596	397.189856	8.291174
5.479188	412.907447	8.296192
5.559149	416.366306	8.301210
5.724701	417.152933	8.306227
5.505602	422.669180	8.311245
5.593947	418.518534	8.316262
5.787350	423.582199	8.321280
5.686308	424.028727	8.326298
5.784974	420.157441	8.331315
5.403543	422.383673	8.336333
5.716249	421.762708	8.341350
5.566674	417.117607	8.346368
5.366866	419.190630	8.351386
5.555516	416.811523	8.356403
5.697965	426.818804	8.361421
5.578634	415.503974	8.366438
5.515503	422.174889	8.371456
5.439386	418.280101	8.376474
5.936490	422.532533	8.381491
5.565643	415.725608	8.386509
5.922261	420.193891	8.391526
5.820196	419.007482	8.396544
5.837898	411.434076	8.401562
5.579285	420.475440	8.406579
5.654764	416.082470	8.411597
5.406686	416.804202	8.416614
5.443685	422.966002	8.421632
5.558026	416.989364	8.426650
5.660212	415.741055	8.431667
5.625182	443.816830	8.436685
5.897602	442.164079	8.441702
5.785848	449.609154	8.446720
5.833738	452.321063	8.451738
5.877721	451.721144	8.456755
5.940644	452.663991	8.461773
5.671003	429.075715	8.466790
5.845749	451.584105	8.471808
5.852375	449.968840	8.476826
5.913302	455.210228	8.481843
5.418538	455.666695	8.486861
5.767211	447.026938	8.491878
5.819795	455.677456	8.496896
5.757423	452.920817	8.501914
5.989898	453.538069	8.506931
5.473430	461.094511	8.511949
5.633269	458.758766	8.516966
5.439210	457.531351	8.521984
5.656767	454.010535	8.527002
5.871048	454.817802	8.532019
5.697151	467.605776	8.537037
5.774759	453.939506	8.542054
5.893449	451.561591	8.547072
5.761546	461.522969	8.552090
6.286519	451.244611	8.557107
5.884903	461.769471	8.562125
5.907990	452.084328	8.567143
6.078466	455.597829	8.572160
6.017942	449.724057	8.577178
6.165896	451.390101	8.582195
5.880212	456.247019	8.587213
6.098746	456.657947	8.592231
6.222972	453.212678	8.597248
6.011575	447.695251	8.602266
5.993809	455.979546	8.607283
5.737414	454.977236	8.612301
5.873466	455.894937	8.617319
5.746836	451.820170	8.622336
5.965809	458.886883	8.627354
6.123929	447.697156	8.632371
5.416741	459.642754	8.637389
5.810975	452.956651	8.642407
5.707416	452.759762	8.647424
6.003822	464.740695	8.652442
6.441799	467.858588	8.657459
5.944737	464.791952	8.662477
6.084597	456.757513	8.667495
6.312598	461.925075	8.672512
6.041886	454.919616	8.677530
6.260445	452.745355	8.682547
5.557060	451.924222	8.687565
6.287985	455.243789	8.692583
6.380332	450.123075	8.697600
6.450776	457.179440	8.702618
6.626148	443.088898	8.707635
6.318834	452.386384	8.712653
6.205186	450.604514	8.717671
6.081163	448.944830	8.722688
5.898321	452.684365	8.727706
6.285685	449.088479	8.732723
6.045857	444.628040	8.737741
5.801650	443.621540	8.742759
6.027177	446.487171	8.747776
6.003183	452.112913	8.752794
6.147940	436.340423	8.757811
6.070514	450.663576	8.762829
5.937496	442.897315	8.767847
6.171193	447.073863	8.772864
6.005523	448.351724	8.777882
5.901453	443.199887	8.782899
6.036993	451.578765	8.787917
6.129102	455.412940	8.792935
6.143551	443.536535	8.797952
6.057907	462.671427	8.802970
6.722092	457.929632	8.807987
6.118137	453.200416	8.813005
6.225645	445.163487	8.818023
5.976150	449.939001	8.823040
6.090188	460.020507	8.828058
6.007180	474.524317	8.833075
6.249040	479.383704	8.838093
5.971181	487.981695	8.843111
6.295885	478.097006	8.848128
6.414165	483.343240	8.853146
6.718554	476.227221	8.858163
6.505350	474.083388	8.863181
6.562472	468.219579	8.868199
6.333161	455.782557	8.873216
5.892625	464.795137	8.878234
6.597648	450.699417	8.883251
6.234736	459.561703	8.888269
6.186961	446.784898	8.893287
5.966696	448.655046	8.898304
6.130337	460.932623	8.903322
6.463719	471.007006	8.908339
6.196485	481.012345	8.913357
6.130719	474.486543	8.918375
6.368541	479.733573	8.923392
6.304067	487.165690	8.928410
6.559183	470.350116	8.933427
6.475341	480.386384	8.938445
6.074419	477.446272	8.943463
5.980440	471.009799	8.948480
5.879527	485.267012	8.953498
6.352437	475.565348	8.958515
6.233486	477.998329	8.963533
6.054052	475.937851	8.968551
6.406443	479.174293	8.973568
5.969286	488.161130	8.978586
6.413915	490.431545	8.983603
6.318408	479.943733	8.988621
5.817313	479.168691	8.993639
6.397149	505.772821	8.998656
6.577959	498.086246	9.003674
6.501305	499.779000	9.008691
6.551334	505.298176	9.013709
6.628365	506.513262	9.018727
6.702908	500.674298	9.023744
6.526343	479.941860	9.028762
6.576457	478.010731	9.033779
6.324906	477.306405	9.038797
6.145367	480.499386	9.043815
6.600009	484.469944	9.048832
6.548440	506.409987	9.053850
6.599182	496.842255	9.058867
6.910393	484.166365	9.063885
6.405068	480.564930	9.068903
6.202106	474.998654	9.073920
6.221354	489.275265	9.078938
6.733737	495.210846	9.083955
6.703643	503.711566	9.088973
6.813246	496.957411	9.093991
7.039865	474.296327	9.099008
6.535545	485.088251	9.104026
6.725005	474.483004	9.109043
6.436762	475.575356	9.114061
6.843902	476.395642	9.119079
6.742372	469.939756	9.124096
6.575312	477.779632	9.129114
6.641648	470.051473	9.134131
6.710879	471.306433	9.139149
6.402365	475.099536	9.144167
6.210769	470.138993	9.149184
6.444892	475.580712	9.154202
6.506659	474.774903	9.159219
6.353735	475.840038	9.164237
6.449398	487.978162	9.169255
6.494418	492.491961	9.174272
7.006437	505.665121	9.179290
6.978791	487.536221	9.184307
6.746193	486.126644	9.189325
6.611609	481.368019	9.194343
6.673085	474.318555	9.199360
6.633681	483.237308	9.204378
6.651052	479.667485	9.209395
6.463968	474.555024	9.214413
6.196473	495.780225	9.219431
6.677870	495.501853	9.224448
6.579325	506.490100	9.229466
6.774512	502.167160	9.234483
7.029751	506.175001	9.239501
6.413202	507.157964	9.244519
6.925279	511.329199	9.249536
6.906620	513.962818	9.254554
6.860776	515.132193	9.259571
7.003021	513.034776	9.264589
6.865523	512.054624	9.269607
6.941960	497.934615	9.274624
6.660566	489.286188	9.279642
7.027526	484.455809	9.284659
6.945224	475.606399	9.289677
6.209542	481.697462	9.294695
7.316072	489.545709	9.299712
6.771855	489.481114	9.304730
6.863413	482.691583	9.309747
6.639637	474.920117	9.314765
6.572345	487.894306	9.319783
6.700431	491.969731	9.324800
6.658267	507.617463	9.329818
6.784663	506.933771	9.334835
6.718817	500.209564	9.339853
6.677070	505.673922	9.344871
7.017158	510.045776	9.349888
6.717107	509.291838	9.354906
6.842197	505.810787	9.359923
7.073338	501.765112	9.364941
6.907684	509.066237	9.369959
6.870543	499.276913	9.374976
7.040338	513.373419	9.379994
6.868537	503.566714	9.385011
6.858717	509.680431	9.390029
7.186380	518.234872	9.395047
7.234881	507.287515	9.400064
7.158231	509.293035	9.405082
7.129657	504.986424	9.410099
7.237912	502.502568	9.415117
6.762570	491.989112	9.420135
6.650895	491.355621	9.425152
6.963433	496.404821	9.430170
6.991077	512.921582	9.435187
7.176768	507.071423	9.440205
6.591841	513.937956	9.445223
6.906607	504.787315	9.450240
6.843492	514.616833	9.455258
7.159843	517.071945	9.460275
7.034017	522.281608	9.465293
6.911313	516.711228	9.470311
7.241323	519.799838	9.475328
7.090983	519.814053	9.480346
7.362246	516.733861	9.485363
7.276660	511.585818	9.490381
6.957658	516.944310	9.495399
7.028267	506.243059	9.500416
6.998860	501.606696	9.505434
7.231688	508.694552	9.510451
7.030897	504.930298	9.515469
7.011408	511.687886	9.520487
6.981943	514.779361	9.525504
7.002458	517.585981	9.530522
6.816799	515.087793	9.535539
7.092608	515.624427	9.540557
6.903876	518.100703	9.545575
7.051433	517.506398	9.550592
6.823706	521.766945	9.555610
6.828356	521.236548	9.560627
7.473826	514.295292	9.565645
7.103908	510.531986	9.570663
7.345113	513.202324	9.575680
7.364673	515.864627	9.580698
7.365826	517.449577	9.585715
7.454759	508.271714	9.590733
7.447924	520.048786	9.595751
7.534708	503.939242	9.600768
7.310460	509.295563	9.605786
7.118708	518.257570	9.610803
7.316812	505.378239	9.615821
7.053470	519.673112	9.620839
7.176318	517.361025	9.625856
7.070696	516.469070	9.630874
6.803156	512.932030	9.635891
7.232922	513.533420	9.640909
6.913420	516.146578	9.645927
7.054887	518.412472	9.650944
7.188556	516.258808	9.655962
6.942657	517.813569	9.660979
7.165422	529.959534	9.665997
7.000824	547.121221	9.671015
7.414601	529.928454	9.676032
7.266848	538.437334	9.681050
7.322770	543.941765	9.686067
7.478611	538.434912	9.691085
7.227129	544.945471	9.696103
7.076159	536.046225	9.701120
7.338423	535.141344	9.706138
7.415316	534.337741	9.711155
7.323093	540.201411	9.716173
6.945517	541.992412	9.721191
7.038748	539.990926	9.726208
7.260305	533.595277	9.731226
7.257102	543.690027	9.736243
7.601877	544.461632	9.741261
7.680951	541.307878	9.746279
7.180001	538.078110	9.751296
7.061341	541.024982	9.756314
7.017744	545.473808	9.761331
7.234954	546.301654	9.766349
7.291986	555.852982	9.771367
7.583247	570.859583	9.776384
7.929480	571.970878	9.781402
7.496241	558.461863	9.786419
7.354708	544.494173	9.791437
7.433707	543.046774	9.796455
7.294360	550.914557	9.801472
7.143459	553.688854	9.806490
7.343912	572.267318	9.811507
7.801760	565.337149	9.816525
7.776672	576.757094	9.821543
7.848453	567.782619	9.826560
7.607549	555.719065	9.831578
7.621826	549.196854	9.836595
7.477123	538.121761	9.841613
7.476547	549.329559	9.846631
7.367519	543.093177	9.851648
7.769530	541.182479	9.856666
7.643923	548.288597	9.861683
7.249726	538.336373	9.866701
7.289302	559.693085	9.871719
7.744112	567.871924	9.876736
7.852597	567.587432	9.881754
7.641072	571.809673	9.886771
7.920130	563.286925	9.891789
7.463757	546.949340	9.896807
7.153002	556.364378	9.901824
7.579143	568.188012	9.906842
7.638280	569.775927	9.911859
7.861972	566.831770	9.916877
7.585820	569.974890	9.921895
7.377883	569.080058	9.926912
7.803257	568.698409	9.931930
7.445298	577.054274	9.936947
7.690254	565.765981	9.941965
7.552658	574.484197	9.946983
7.658327	574.327326	9.952000
7.785381	565.007081	9.957018
7.928428	566.152937	9.962035
7.769738	564.811770	9.967053
7.679662	572.834352	9.972071
7.482284	574.403296	9.977088
7.587817	563.947753	9.982106
7.804697	574.190373	9.987123
7.875319	566.653169	9.992141
7.745735	564.503889	9.997159
7.774577	573.795174	10.002176
7.763541	570.927628	10.007194
7.455722	574.937550	10.012211
7.854636	579.949194	10.017229
7.860026	578.297707	10.022247
7.756783	577.620492	10.027264
7.734827	576.018428	10.032282
7.797550	572.491828	10.037299
7.980038	566.721110	10.042317
7.721833	573.867388	10.047335
7.738204	574.994933	10.052352
7.855736	569.597577	10.057370
7.813923	575.480437	10.062387
7.922187	569.164427	10.067405
8.013600	569.917129	10.072423
7.892177	569.408670	10.077440
7.978022	571.595439	10.082458
7.629825	575.665217	10.087475
7.846608	571.729185	10.092493
7.974360	576.950847	10.097511
7.700798	571.712189	10.102528
8.109425	569.328382	10.107546
7.942243	572.258327	10.112563
7.883633	569.849043	10.117581
8.068979	581.077137	10.122599
7.899625	579.657827	10.127616
7.887040	574.681078	10.132634
7.763276	586.632346	10.137651
8.129987	588.550405	10.142669
8.145735	599.853156	10.147687
8.150607	602.168733	10.152704
8.186711	578.173534	10.157722
8.010163	585.425526	10.162739
8.105011	566.331176	10.167757
8.133396	562.943935	10.172775
7.917363	558.398413	10.177792
8.223285	569.655469	10.182810
8.172305	566.826056	10.187827
7.842250	562.189849	10.192845
8.292062	567.437299	10.197863
7.910455	580.745675	10.202880
7.898823	573.688044	10.207898
8.253769	582.607836	10.212915
7.964913	576.985728	10.217933
8.065707	584.215437	10.222951
8.377856	593.996802	10.227968
8.390701	582.322311	10.232986
8.139140	577.490194	10.238003
8.416239	575.438851	10.243021
8.545407	582.652230	10.248039
7.933206	573.855806	10.253056
8.318443	570.623797	10.258074
7.934881	571.612717	10.263091
8.044710	582.344355	10.268109
8.401256	566.557394	10.273127
7.856105	580.636589	10.278144
8.188798	566.293231	10.283162
7.968370	577.000238	10.288179
8.228922	593.334683	10.293197
8.407871	604.386708	10.298215
8.256052	605.047766	10.303232
8.305472	594.938901	10.308250
8.451741	599.479402	10.313267
8.272633	585.143741	10.318285
8.087311	583.725904	10.323303
8.260786	595.430940	10.328320
8.391162	611.002267	10.333338
8.350045	596.731643	10.338355
8.344405	596.828686	10.343373
8.208349	582.838991	10.348391
8.300196	593.120712	10.353408
8.320811	594.821716	10.358426
8.451655	610.319545	10.363443
8.501309	603.038937	10.368461
8.217869	589.845516	10.373479
8.304752	594.915330	10.378496
8.212713	607.502821	10.383514
8.584900	611.948496	10.388531
8.532073	607.460863	10.393549
8.578221	600.717998	10.398567
8.182412	599.571739	10.403584
8.310753	596.578865	10.408602
8.642479	603.118286	10.413619
8.386273	599.276613	10.418637
8.620122	580.307554	10.423655
8.414219	589.063114	10.428672
8.596902	585.225259	10.433690
8.192074	580.554825	10.438707
8.209654	589.719656	10.443725
8.743816	599.272800	10.448743
8.540840	613.778375	10.453760
8.423083	601.666759	10.458778
8.423139	611.599017	10.463795
8.713210	603.899149	10.468813
8.657830	596.276782	10.473831
8.064942	594.507039	10.478848
8.062221	600.369240	10.483866
8.669206	611.954008	10.488883
8.386669	611.717187	10.493901
8.557011	608.753153	10.498919
8.551971	613.353844	10.503936
8.217041	598.593519	10.508954
8.569245	607.531102	10.513971
8.538149	612.138683	10.518989
8.553904	608.469501	10.524007
8.546609	612.029908	10.529024
8.219383	610.427405	10.534042
8.244288	603.399708	10.539059
8.311601	620.294996	10.544077
8.060065	631.341828	10.549095
8.273516	635.638515	10.554112
8.820064	635.021387	10.559130
8.678544	631.855860	10.564147
8.443411	648.290076	10.569165
9.091719	639.923215	10.574183
8.731272	644.724514	10.579200
8.851775	651.061486	10.584218
8.805326	640.730357	10.589235
8.494174	640.556556	10.594253
9.018203	643.181679	10.599271
8.807198	645.658527	10.604288
8.780367	643.485661	10.609306
8.825301	643.037336	10.614323
8.615387	649.911274	10.619341
9.222801	639.520869	10.624359
8.801425	645.913068	10.629376
8.993290	646.628213	10.634394
8.841249	639.986771	10.639411
8.598007	648.333645	10.644429
9.117413	636.953819	10.649447
8.829862	643.675909	10.654464
9.004785	642.684368	10.659482
8.834107	626.080725	10.664499
8.351151	630.597684	10.669517
9.025580	637.086652	10.674535
8.712229	636.424674	10.679552
8.877103	650.021771	10.684570
9.104480	646.908300	10.689587
8.977840	642.525438	10.694605
9.325930	635.097384	10.699623
8.857766	624.204132	10.704640
8.750200	612.249659	10.709658
9.256972	628.288315	10.714675
9.192076	629.355363	10.719693
8.708612	613.312343	10.724711
8.794681	611.339988	10.729728
8.726064	614.542116	10.734746
9.049181	629.352944	10.739763
9.034748	634.496692	10.744781
9.180953	634.997988	10.749799
8.675908	627.779059	10.754816
8.798452	633.889326	10.759834
9.005967	638.268490	10.764851
8.970136	629.358122	10.769869
9.431434	634.079124	10.774887
8.929624	637.874477	10.779904
9.056949	633.237808	10.784922
9.329097	635.825079	10.789939
9.341455	638.894668	10.794957
8.988088	607.501994	10.799975
8.571307	616.164482	10.804992
8.543628	628.327549	10.810010
8.978266	640.016175	10.815027
8.682975	641.277018	10.820045
8.998846	638.098451	10.825063
8.877546	642.496840	10.830080
8.947575	641.906560	10.835098
9.385492	633.667382	10.840115
9.146112	646.348287	10.845133
8.926048	642.815530	10.850151
9.050883	640.679261	10.855168
8.752717	639.610462	10.860186
9.142887	650.872273	10.865203
9.198637	665.232735	10.870221
9.229210	671.581514	10.875239
9.166244	672.270912	10.880256
9.234981	677.458129	10.885274
9.247645	672.743862	10.890291
9.147619	679.923734	10.895309
9.219445	675.020513	10.900327
9.549524	679.602723	10.905344
9.251569	675.028857	10.910362
9.613711	669.549276	10.915379
9.183124	669.523662	10.920397
9.256303	672.756362	10.925415
9.318140	675.666172	10.930432
9.166358	669.585259	10.935450
9.415909	672.985871	10.940467
9.446151	681.109957	10.945485
9.727871	670.786461	10.950503
9.255498	655.444449	10.955520
8.983187	653.401550	10.960538
9.292084	660.472306	10.965555
9.241249	674.613307	10.970573
9.283247	669.700873	10.975591
9.351260	674.393959	10.980608
9.195737	682.575890	10.985626
9.585594	676.168349	10.990643
9.358657	682.411522	10.995661
9.519112	673.100029	11.000679
9.542978	675.606341	11.005696
9.295417	684.765304	11.010714
9.352128	674.750246	11.015731
9.603021	681.211608	11.020749
9.868945	673.174606	11.025767
9.576602	682.699052	11.030784
9.219482	682.775784	11.035802
9.623786	672.623825	11.040819
9.611596	675.324501	11.045837
9.636523	673.674874	11.050855
9.699431	672.416145	11.055872
9.656264	683.851575	11.060890
9.894672	673.258921	11.065907
9.896987	668.306630	11.070925
9.687406	651.116956	11.075943
9.677948	648.087730	11.080960
9.660910	641.898414	11.085978
9.463624	647.145585	11.090995
9.381028	642.877439	11.096013
9.416164	639.131019	11.101031
9.557054	650.868677	11.106048
9.695435	666.090135	11.111066
9.726151	662.035808	11.116083
9.650608	656.951199	11.121101
9.617181	665.407880	11.126119
9.455034	668.982820	11.131136
9.850357	671.165403	11.136154
9.807287	672.586867	11.141171
9.678390	677.671316	11.146189
9.926059	667.370409	11.151207
9.381255	662.452176	11.156224
9.353840	670.077024	11.161242
9.702902	668.817382	11.166259
9.691908	678.301950	11.171277
9.716843	679.823323	11.176295
9.680887	675.240354	11.181312
9.678610	683.295247	11.186330
10.128777	669.231850	11.191347
9.771152	686.943450	11.196365
9.576112	673.825414	11.201383
9.847067	678.856589	11.206400
9.555261	675.472155	11.211418
9.912232	675.599077	11.216435
9.807442	679.173146	11.221453
9.852346	675.905960	11.226471
10.164125	665.879414	11.231488
9.855323	673.601031	11.236506
10.073243	673.359365	11.241523
9.726775	679.260032	11.246541
9.480847	680.851819	11.251559
10.151044	669.885846	11.256576
9.689224	683.118870	11.261594
9.913482	673.272996	11.266611
9.712166	678.258467	11.271629
9.698426	676.305253	11.276647
10.068231	669.083989	11.281664
9.777004	674.689472	11.286682
9.592535	674.522170	11.291699
9.944890	684.509490	11.296717
9.951813	698.041946	11.301735
10.340931	695.940475	11.306752
10.136822	690.194996	11.311770
10.100486	682.367468	11.316787
9.951679	675.280234	11.321805
9.874662	674.337653	11.326823
10.090993	679.049588	11.331840
10.000464	694.759677	11.336858
10.094542	697.843448	11.341875
10.387700	700.113483	11.346893
9.989080	693.033515	11.351911
10.106451	686.926753	11.356928
9.805569	701.113080	11.361946
10.156081	705.615530	11.366963
9.990761	699.991346	11.371981
10.051804	710.789642	11.376999
10.461739	705.477484	11.382016
9.966023	715.633935	11.387034
10.296161	702.301426	11.392051
10.479977	712.031762	11.397069
10.257759	705.392705	11.402087
10.132714	702.092546	11.407104
10.082720	707.956739	11.412122
10.332226	705.378906	11.417139
10.261902	699.707045	11.422157
10.172015	708.077866	11.427175
10.457347	698.968222	11.432192
10.405070	704.789096	11.437210
10.375671	689.952704	11.442227
10.353244	685.880238	11.447245
10.224943	683.056963	11.452263
10.336060	676.558757	11.457280
10.039000	680.496647	11.462298
10.251777	689.319275	11.467315
9.977876	702.734252	11.472333
10.224723	701.956324	11.477351
10.170068	704.058600	11.482368
10.040773	704.652144	11.487386
10.295720	700.197573	11.492403
10.179036	706.511989	11.497421
10.020990	700.372463	11.502439
10.064227	701.540824	11.507456
9.675753	708.374985	11.512474
9.774314	711.032260	11.517491
10.623627	724.093053	11.522509
10.560979	728.117770	11.527527
10.410208	722.413803	11.532544
10.198658	728.579639	11.537562
10.312284	724.328852	11.542579
10.335942	730.332374	11.547597
10.482346	729.896312	11.552615
10.561985	730.027209	11.557632
10.314925	732.696270	11.562650
10.531543	738.247086	11.567667
10.763021	727.651414	11.572685
10.591876	730.533626	11.577703
10.507352	727.913090	11.582720
10.429084	734.595905	11.587738
10.788215	734.636452	11.592755
10.288601	730.004560	11.597773
10.676543	728.411705	11.602791
10.438225	725.475027	11.607808
10.583920	728.342367	11.612826
10.567126	729.424653	11.617843
10.816722	728.939157	11.622861
10.474896	729.076925	11.627879
10.706227	722.204218	11.632896
10.536785	733.329990	11.637914
10.215891	727.539150	11.642931
10.458169	747.372585	11.647949
10.536276	756.828022	11.652967
10.878967	753.446170	11.657984
10.953100	760.965214	11.663002
11.024645	761.900349	11.668019
10.804773	766.348619	11.673037
11.061770	771.840574	11.678055
11.175005	754.812072	11.683072
10.960392	737.286550	11.688090
10.876070	735.951509	11.693107
10.899659	730.600221	11.698125
10.887383	734.385089	11.703143
11.313694	729.096380	11.708160
11.110627	731.001691	11.713178
10.525294	739.417679	11.718195
10.683791	725.116120	11.723213
10.852044	727.866727	11.728231
10.741659	725.911265	11.733248
10.796886	734.062129	11.738266
10.485037	727.299192	11.743283
10.535915	730.260239	11.748301
10.369434	741.356394	11.753319
10.721820	762.758432	11.758336
10.656714	762.549439	11.763354
10.427714	756.000458	11.768371
10.835971	758.325971	11.773389
10.984170	759.310171	11.778407
11.149104	755.948810	11.783424
10.642014	769.008145	11.788442
10.936019	762.038987	11.793459
10.739798	758.666400	11.798477
10.914084	756.414817	11.803495
10.949050	754.517075	11.808512
11.012133	761.588975	11.813530
10.864812	771.984578	11.818547
11.232636	770.633824	11.823565
11.311425	788.924527	11.828583
11.456001	770.569243	11.833600
11.128291	765.552495	11.838618
11.131514	769.730434	11.843635
11.019329	755.859046	11.848653
11.106125	759.788463	11.853671
11.222070	759.665117	11.858688
11.226866	754.774587	11.863706
10.892724	757.911438	11.868723
11.301050	763.000116	11.873741
10.849016	756.626384	11.878759
11.254172	769.382921	11.883776
11.215826	776.378386	11.888794
11.183477	791.160862	11.893811
11.397194	786.783586	11.898829
10.995347	776.631116	11.903847
11.158825	786.935112	11.908864
11.474320	786.562274	11.913882
11.269416	795.071739	11.918899
11.616402	789.640498	11.923917
11.324325	774.246944	11.928935
11.114937	763.127524	11.933952
11.631328	767.470147	11.938970
11.741947	762.046119	11.943987
11.818654	756.115170	11.949005
11.448259	763.245934	11.954023
11.314905	751.843432	11.959040
11.359746	755.038146	11.964058
11.278488	760.520578	11.969075
11.577142	754.786383	11.974093
11.364948	753.966651	11.979111
11.420547	753.595087	11.984128
11.383141	759.804228	11.989146
11.158313	759.345821	11.994163
11.562728	750.624393	11.999181
11.296790	757.700786	12.004199
11.264770	760.840960	12.009216
11.148282	758.582988	12.014234
10.988503	771.301154	12.019251
11.270018	780.391521	12.024269
11.162781	788.309792	12.029287
11.567145	792.398425	12.034304
11.819108	791.512564	12.039322
11.637919	795.922723	12.044339
11.792873	794.950238	12.049357
11.625872	799.192106	12.054375
11.611024	785.546227	12.059392
11.817177	790.721664	12.064410
11.519377	792.273268	12.069427
11.924425	787.368952	12.074445
11.627729	797.116419	12.079463
11.708853	793.726070	12.084480
11.817263	786.236609	12.089498
11.390129	792.430430	12.094515
11.864031	787.933338	12.099533
11.615971	796.570638	12.104551
11.661904	793.018828	12.109568
11.844824	790.738051	12.114586
11.404500	793.360709	12.119603
11.603724	795.982371	12.124621
11.802571	794.718752	12.129639
11.634152	786.146254	12.134656
11.714531	781.655327	12.139674
11.753623	783.693215	12.144691
11.688493	785.431326	12.149709
11.688437	794.576574	12.154727
11.913769	795.204082	12.159744
11.761811	787.476423	12.164762
11.715800	791.124206	12.169779
11.780381	782.874175	12.174797
11.847455	787.082842	12.179815
11.629795	782.766246	12.184832
11.804334	782.997503	12.189850
11.677392	787.027804	12.194867
11.627384	780.178411	12.199885
11.243226	792.564626	12.204903
11.410047	814.357790	12.209920
11.857142	819.598102	12.214938
11.577975	824.116673	12.219955
11.922947	826.514129	12.224973
11.779910	819.593968	12.229991
11.765862	822.882731	12.235008
12.151196	816.651659	12.240026
12.352223	819.725158	12.245043
12.335171	808.783170	12.250061
12.060962	820.430909	12.255079
12.001145	823.349354	12.260096
12.245575	813.504959	12.265114
11.978149	820.605642	12.270131
12.272606	818.366357	12.275149
12.093543	811.278184	12.280167
12.520224	823.576497	12.285184
12.086197	816.336620	12.290202
12.093894	826.152203	12.295219
12.175974	819.083018	12.300237
12.297856	811.237591	12.305255
12.054641	816.035793	12.310272
11.961584	818.384410	12.315290
12.005722	821.690468	12.320307
12.327352	813.615593	12.325325
12.309544	825.783473	12.330343
12.358714	818.917972	12.335360
12.447087	816.640112	12.340378
12.328283	824.255818	12.345395
12.329634	816.944755	12.350413
12.359700	824.701453	12.355431
12.243527	820.690593	12.360448
12.340224	812.803882	12.365466
12.285465	816.017330	12.370483
12.509920	815.110254	12.375501
12.360122	812.067711	12.380519
12.392900	820.807546	12.385536
12.560395	810.383857	12.390554
12.612014	816.998863	12.395571
12.495464	815.150115	12.400589
12.468524	808.683461	12.405607
12.252195	808.080146	12.410624
12.304653	808.967279	12.415642
12.314985	825.293367	12.420659
12.565584	822.338588	12.425677
12.545419	824.388300	12.430695
12.498746	817.261192	12.435712
12.752302	818.420979	12.440730
12.277187	819.635747	12.445747
12.367614	812.016595	12.450765
12.592322	808.180163	12.455783
12.262276	815.293811	12.460800
12.226473	810.160227	12.465818
12.322336	817.226703	12.470835
12.279102	816.984352	12.475853
12.346253	815.664282	12.480871
12.395958	815.947388	12.485888
12.541253	807.963633	12.490906
12.422683	816.178465	12.495923
12.415107	813.481152	12.500941
12.476007	809.534359	12.505959
11.906848	818.585253	12.510976
12.841611	826.345306	12.515994
12.417493	837.832949	12.521011
12.570307	840.103697	12.526029
12.606816	837.142378	12.531047
12.674421	843.411849	12.536064
12.811156	836.300305	12.541082
12.829430	842.503768	12.546099
12.686574	845.177967	12.551117
12.720008	848.467504	12.556135
12.445710	850.062055	12.561152
12.996828	843.814440	12.566170
12.733486	852.046662	12.571187
12.459837	841.198281	12.576205
12.818553	844.421350	12.581223
12.367369	840.891532	12.586240
12.681127	844.426579	12.591258
12.601177	851.428600	12.596275
12.748800	865.702525	12.601293
13.356352	873.908892	12.606311
12.711172	868.893504	12.611328
12.889815	855.586439	12.616346
12.942303	875.210065	12.621363
13.087305	872.763938	12.626381
12.947446	860.072565	12.631399
13.134329	861.340676	12.636416
12.941669	843.653914	12.641434
12.417065	858.094091	12.646451
12.928052	869.675918	12.651469
13.126947	868.659710	12.656487
13.245562	878.816510	12.661504
13.199856	867.359200	12.666522
13.275021	876.180991	12.671539
13.296067	861.948803	12.676557
13.220460	847.407913	12.681575
12.778516	840.063836	12.686592
13.155654	843.388953	12.691610
13.533636	859.444928	12.696627
13.201125	848.643134	12.701645
13.413434	834.307335	12.706663
13.341326	842.160153	12.711680
13.187140	829.529057	12.716698
13.210408	839.308794	12.721715
13.169282	837.783113	12.726733
13.473615	837.773521	12.731751
13.328573	843.439800	12.736768
13.107608	841.581831	12.741786
13.303184	836.362735	12.746803
13.226212	839.489335	12.751821
13.281631	837.798995	12.756839
12.999757	836.546778	12.761856
13.132012	835.586921	12.766874
13.360455	838.188774	12.771891
13.399051	840.342493	12.776909
13.394595	825.594535	12.781927
13.098366	839.088335	12.786944
13.006979	831.266734	12.791962
13.212559	851.637270	12.796979
13.611270	864.934880	12.801997
13.649119	861.535963	12.807015
13.196236	858.348132	12.812032
13.725897	855.646548	12.817050
13.482588	850.713571	12.822067
13.200221	836.836737	12.827085
13.325392	845.019535	12.832103
13.664577	866.059567	12.837120
13.675022	855.793636	12.842138
13.426932	842.189034	12.847155
13.246107	848.909810	12.852173
13.479986	849.642586	12.857191
13.608145	866.032000	12.862208
13.750258	864.781350	12.867226
13.793599	867.703128	12.872243
13.683596	861.345921	12.877261
13.721246	837.874043	12.882279
13.361696	837.799417	12.887296
13.812268	849.876670	12.892314
13.444432	848.031696	12.897331
13.443783	861.896239	12.902349
13.865794	872.362817	12.907367
13.717381	865.309680	12.912384
13.262078	878.204998	12.917402
13.337824	867.681765	12.922419
13.429085	875.353913	12.927437
13.647128	860.607716	12.932455
13.644923	871.417620	12.937472
13.926377	872.013365	12.942490
13.808214	870.060752	12.947507
13.735811	875.494511	12.952525
13.646066	866.458135	12.957543
13.764017	869.982037	12.962560
13.628336	866.558422	12.967578
14.029676	867.597199	12.972595
13.705871	863.660207	12.977613
14.043474	864.814886	12.982631
13.601104	870.208964	12.987648
13.681411	861.054371	12.992666
13.775940	861.227673	12.997683
13.614462	875.244148	13.002701
14.081257	874.839862	13.007719
14.069450	891.922207	13.012736
14.141305	892.388432	13.017754
14.115987	885.693539	13.022771
13.752969	874.636186	13.027789
13.782569	883.415952	13.032807
13.684067	896.561210	13.037824
13.871250	895.782758	13.042842
13.870144	894.104563	13.047859
13.737780	894.887588	13.052877
13.955805	894.812032	13.057895
14.175502	900.798193	13.062912
13.879883	889.490863	13.067930
14.144777	899.578090	13.072947
13.997304	895.238774	13.077965
14.253879	891.190150	13.082983
13.576654	903.844442	13.088000
13.906248	905.673836	13.093018
14.118478	914.060492	13.098035
14.170675	931.260383	13.103053
14.548032	928.847472	13.108071
14.515241	908.962355	13.113088
14.130933	900.874269	13.118106
14.136737	900.185803	13.123123
14.066437	908.482812	13.128141
14.543529	909.986529	13.133159
14.531440	908.714265	13.138176
14.428406	901.983467	13.143194
14.356604	887.088781	13.148211
14.281145	895.878930	13.153229
14.424247	891.219682	13.158247
14.304382	891.846309	13.163264
14.531678	886.639245	13.168282
14.479442	891.440370	13.173299
14.296722	894.027509	13.178317
14.587925	890.676035	13.183335
14.492848	892.263239	13.188352
14.530538	889.741054	13.193370
14.286948	886.507604	13.198387
13.987635	900.214357	13.203405
14.497799	900.952390	13.208423
14.762606	909.263971	13.213440
14.369132	901.692532	13.218458
14.493099	906.287811	13.223475
14.794598	926.811783	13.228493
14.674588	913.969045	13.233511
14.530319	900.317216	13.238528
14.674265	893.742995	13.243546
14.928051	890.102681	13.248563
14.631798	885.164911	13.253581
14.622062	884.784323	13.258599
14.653427	887.069950	13.263616
14.571347	890.611554	13.268634
14.564517	887.738329	13.273651
14.621308	897.023194	13.278669
14.778295	905.070233	13.283687
14.743877	918.848123	13.288704
14.757899	922.262154	13.293722
15.031300	906.410918	13.298739
14.600928	912.087642	13.303757
14.731908	913.380599	13.308775
14.496626	917.930877	13.313792
14.776947	927.884465	13.318810
14.884116	931.829044	13.323827
14.689737	930.115454	13.328845
14.793467	930.675785	13.333863
14.670703	927.735017	13.338880
14.811607	927.998637	13.343898
14.976624	916.558033	13.348915
14.898512	924.910874	13.353933
14.817583	915.885404	13.358951
15.141227	915.908821	13.363968
14.570820	923.653769	13.368986
14.547998	914.132454	13.374003
14.876495	918.580756	13.379021
14.709600	920.427916	13.384039
14.840942	929.767334	13.389056
14.786789	919.965021	13.394074
15.226861	933.632563	13.399091
15.200531	947.252254	13.404109
15.489401	936.614422	13.409127
14.988419	925.121332	13.414144
14.974439	924.166683	13.419162
15.264609	918.244283	13.424179
15.169531	920.150564	13.429197
14.930076	924.656462	13.434215
15.392672	924.571749	13.439232
14.844089	927.580509	13.444250
15.493568	926.391181	13.449267
14.894044	933.682146	13.454285
14.933628	938.478062	13.459303
15.312022	956.142823	13.464320
15.170378	950.611653	13.469338
15.210578	949.697994	13.474355
15.222768	951.113251	13.479373
15.278758	948.560458	13.484391
15.296120	945.004308	13.489408
15.304509	960.455523	13.494426
15.769876	940.892066	13.499443
15.446604	946.648239	13.504461
15.185232	949.980106	13.509479
15.586928	940.617529	13.514496
15.435557	944.091338	13.519514
15.191101	948.534101	13.524531
15.414816	950.664152	13.529549
15.169731	944.917908	13.534567
15.375199	950.501165	13.539584
15.254995	956.414127	13.544602
15.287013	950.707251	13.549619
15.184895	957.551007	13.554637
15.261003	946.480845	13.559655
15.143539	950.153730	13.564672
14.979065	967.751660	13.569690
15.529048	968.966907	13.574707
15.803028	980.254177	13.579725
15.917743	973.084031	13.584743
16.198514	973.128353	13.589760
16.041079	962.233210	13.594778
15.960853	947.046775	13.599795
16.081886	944.631193	13.604813
16.013201	945.067042	13.609831
16.034644	938.192318	13.614848
16.250233	938.310463	13.619866
16.431679	932.541750	13.624883
15.962933	926.318550	13.629901
15.980802	919.448562	13.634919
15.383447	911.035473	13.639936
15.714891	911.658735	13.644954
16.027508	906.744746	13.649971
15.535232	902.750712	13.654989
15.575580	911.481270	13.660007
15.474793	917.900012	13.665024
15.415129	931.089628	13.670042
15.757633	933.737299	13.675059
15.656942	939.054924	13.680077
15.653584	944.290629	13.685095
16.147274	938.480644	13.690112
15.524329	941.145096	13.695130
15.519343	940.569635	13.700147
15.621961	943.452837	13.705165
16.021928	962.497002	13.710183
16.150593	962.841392	13.715200
16.220648	965.718987	13.720218
16.231436	962.255652	13.725235
16.132689	952.530608	13.730253
16.243317	941.365741	13.735271
16.369552	939.027243	13.740288
15.715649	931.293971	13.745306
16.021658	933.846140	13.750323
16.153392	932.406670	13.755341
15.887665	939.470119	13.760359
16.311334	947.434667	13.765376
16.236667	969.030801	13.770394
16.241481	969.206025	13.775411
16.289327	967.214390	13.780429
16.351070	957.855162	13.785447
16.220630	938.528919	13.790464
16.343636	939.808441	13.795482
16.109673	942.675151	13.800499
16.013767	957.296115	13.805517
16.090153	958.540083	13.810535
16.475674	965.092567	13.815552
16.364721	969.403704	13.820570
16.469600	973.636057	13.825587
16.407037	967.661448	13.830605
16.066576	975.583346	13.835623
16.231930	970.956200	13.840640
15.892736	976.321354	13.845658
16.195524	971.338708	13.850675
16.357461	973.162121	13.855693
16.488150	983.493350	13.860711
16.863851	979.141062	13.865728
16.418269	976.657460	13.870746
16.299586	965.621630	13.875763
16.439870	967.143936	13.880781
16.373278	969.184456	13.885799
16.273885	974.444008	13.890816
16.400606	989.514189	13.895834
16.780333	992.113559	13.900851
16.706626	984.558610	13.905869
16.356467	984.571590	13.910887
16.392996	979.989080	13.915904
16.279063	1009.188966	13.920922
16.158301	1002.577599	13.925939
16.596685	993.340775	13.930957
16.657357	1006.613794	13.935975
16.709486	996.858920	13.940992
16.496913	1010.929677	13.946010
16.610510	1003.227057	13.951027
16.805739	1006.180305	13.956045
16.847178	1000.526172	13.961063
16.924833	993.798369	13.966080
16.599385	1012.078578	13.971098
16.712330	1001.225076	13.976115
17.174458	1001.538448	13.981133
16.638937	1002.575485	13.986151
16.823222	998.235718	13.991168
17.199974	1004.388519	13.996186
17.344004	1006.604259	14.001203
17.440659	1000.695687	14.006221
17.413660	1001.957630	14.011239
17.467821	995.810075	14.016256
17.211240	1000.790663	14.021274
17.375540	996.171164	14.026291
17.302784	989.722679	14.031309
17.102286	989.634410	14.036327
17.282203	976.314826	14.041344
17.291111	969.651214	14.046362
17.396872	965.225694	14.051379
17.163015	965.701990	14.056397
17.032473	966.902799	14.061415
16.926717	957.290327	14.066432
17.037904	959.288699	14.071450
17.265491	959.693807	14.076467
17.275315	958.009261	14.081485
16.946940	956.529738	14.086503
17.382701	975.145555	14.091520
17.355140	975.667478	14.096538
17.182430	963.082459	14.101555
17.592056	965.588278	14.106573
17.102466	963.882810	14.111591
17.251501	963.926983	14.116608
17.665328	984.580581	14.121626
17.303280	966.948210	14.126643
17.401802	963.623432	14.131661
17.278605	968.657031	14.136679
17.417161	969.298577	14.141696
17.458587	974.805966	14.146714
17.465009	973.818790	14.151731
17.683789	972.925444	14.156749
17.144568	976.062963	14.161767
17.015633	974.192830	14.166784
17.350418	988.540675	14.171802
17.462934	993.300472	14.176819
17.896110	979.544720	14.181837
17.414268	988.064103	14.186855
17.464857	986.692050	14.191872
17.558062	986.647083	14.196890
17.416755	989.514541	14.201907
17.314792	987.208061	14.206925
17.421990	985.699441	14.211943
17.401895	985.731964	14.216960
17.678698	990.836872	14.221978
17.481251	986.126725	14.226995
17.520597	982.051984	14.232013
17.327822	1002.415511	14.237031
17.864926	1007.237015	14.242048
18.345825	1019.544188	14.247066
17.746673	1007.793748	14.252083
18.202569	997.178503	14.257101
17.700150	994.535457	14.262119
17.920322	988.667773	14.267136
17.993184	988.248259	14.272154
17.541980	984.090496	14.277171
17.857467	992.980473	14.282189
17.632113	1006.040420	14.287207
17.795856	1022.637458	14.292224
17.756838	1021.418477	14.297242
17.479461	1032.441544	14.302259
17.990209	1021.486476	14.307277
17.898401	1028.941505	14.312295
17.678562	1021.548614	14.317312
18.048896	1023.738946	14.322330
17.758278	1019.805254	14.327347
18.116460	1022.262156	14.332365
18.042350	1025.505437	14.337383
17.888252	1018.783470	14.342400
18.146497	1021.128250	14.347418
18.020144	1014.706773	14.352435
18.071289	1013.129913	14.357453
17.935308	1027.982395	14.362471
18.166733	1041.038491	14.367488
18.488889	1041.098768	14.372506
18.565111	1049.595501	14.377523
18.460133	1026.706066	14.382541
18.306752	1030.357383	14.387559
18.244882	1013.144328	14.392576
18.229105	1004.088097	14.397594
18.021458	1021.517291	14.402611
18.277385	1022.916844	14.407629
18.563760	1045.674656	14.412647
18.733403	1031.050509	14.417664
18.594181	1026.936542	14.422682
18.448860	1018.057731	14.427699
18.441187	1018.052759	14.432717
18.336366	1023.894691	14.437735
18.506400	1019.820263	14.442752
18.840989	1014.095353	14.447770
18.608630	1018.346373	14.452787
18.725242	1014.354443	14.457805
18.479047	1018.241249	14.462823
18.451676	1018.793455	14.467840
18.619643	1018.487258	14.472858
18.355585	1016.012452	14.477875
18.736761	1017.059316	14.482893
18.810491	1017.872654	14.487911
18.675434	1016.680265	14.492928
18.543643	1007.994081	14.497946
18.434794	1020.893739	14.502963
18.716121	1006.731337	14.507981
18.923651	1019.066233	14.512999
18.946295	1016.420945	14.518016
18.758640	1012.152838	14.523034
18.614592	1015.668749	14.528051
18.770121	1017.973519	14.533069
18.654558	1013.350142	14.538087
18.471771	1023.990968	14.543104
18.726223	1033.356834	14.548122
18.446758	1042.128419	14.553139
18.433550	1037.776194	14.558157
18.766793	1053.827406	14.563175
18.707531	1042.212386	14.568192
18.539617	1039.549952	14.573210
18.377119	1050.329541	14.578227
18.926574	1059.683789	14.583245
18.915258	1072.519643	14.588263
18.786218	1076.217708	14.593280
19.160533	1061.558332	14.598298
19.002648	1079.036009	14.603315
19.296985	1081.136624	14.608333
19.379549	1063.788489	14.613351
19.379369	1064.527505	14.618368
19.530216	1059.601973	14.623386
19.403577	1039.923811	14.628403
19.675539	1033.586112	14.633421
19.164509	1028.064739	14.638439
18.774550	1023.747188	14.643456
19.223153	1023.868726	14.648474
19.303867	1032.245813	14.653491
19.398290	1027.491078	14.658509
19.364328	1036.120285	14.663527
19.301300	1026.073134	14.668544
19.255791	1028.956958	14.673562
19.253829	1031.759533	14.678579
19.184742	1025.479705	14.683597
19.337028	1035.564481	14.688615
19.380003	1047.638185	14.693632
19.667101	1048.610930	14.698650
19.401854	1039.340253	14.703667
19.358836	1031.127855	14.708685
19.241307	1044.445093	14.713703
19.248186	1058.363675	14.718720
19.602250	1054.014569	14.723738
19.554556	1061.799664	14.728755
19.477604	1057.569046	14.733773
19.617966	1062.480526	14.738791
19.704400	1069.194178	14.743808
19.646576	1062.086131	14.748826
19.220537	1072.320991	14.753843
19.414374	1067.519406	14.758861
19.780390	1061.932948	14.763879
19.453351	1067.972059	14.768896
19.859966	1059.767584	14.773914
19.781233	1065.238680	14.778931
19.453061	1051.028341	14.783949
19.818078	1058.096842	14.788967
19.864291	1071.952603	14.793984
20.129335	1056.359478	14.799002
19.844670	1065.047300	14.804019
19.991244	1059.273314	14.809037
19.728751	1062.701842	14.814055
19.887644	1060.866137	14.819072
19.847456	1064.282911	14.824090
19.875404	1064.107854	14.829107
19.999209	1056.858603	14.834125
19.997865	1054.903477	14.839143
19.699881	1059.261080	14.844160
19.716136	1058.656101	14.849178
19.905410	1061.724123	14.854195
20.034503	1061.107082	14.859213
20.241597	1073.148409	14.864231
20.039779	1063.276656	14.869248
19.905237	1059.394174	14.874266
19.745530	1069.125734	14.879283
19.852521	1077.801610	14.884301
20.279028	1078.933853	14.889319
20.130182	1100.224407	14.894336
20.615790	1094.264929	14.899354
20.141657	1091.730151	14.904371
20.146794	1089.506241	14.909389
20.249736	1086.172042	14.914407
19.992682	1097.594511	14.919424
20.482619	1092.078779	14.924442
20.212368	1093.570520	14.929459
20.277316	1093.046812	14.934477
20.288730	1091.180108	14.939495
20.543146	1089.782040	14.944512
20.478614	1078.828462	14.949530
20.346751	1091.896562	14.954547
20.413589	1092.010693	14.959565
20.430861	1088.592313	14.964583
20.084998	1096.408876	14.969600
20.333942	1081.970701	14.974618
20.450791	1089.399739	14.979635
20.163917	1079.787769	14.984653
20.046050	1087.248339	14.989671
20.331672	1108.604871	14.994688
20.857294	1133.066654	14.999706
20.773197	1120.241593	15.004723
20.781512	1116.703835	15.009741
21.006883	1118.883238	15.014759
20.753357	1103.946701	15.019776
20.977932	1096.189765	15.024794
20.733361	1090.925638	15.029811
20.571279	1082.607813	15.034829
20.263327	1078.824617	15.039847
20.618743	1100.763206	15.044864
20.775950	1110.396843	15.049882
20.867497	1118.278108	15.054899
21.212563	1111.330226	15.059917
21.122177	1108.987947	15.064935
20.792605	1116.951017	15.069952
21.045180	1111.338517	15.074970
21.062418	1112.428952	15.079987
21.010468	1111.700669	15.085005
20.999667	1104.973349	15.090023
21.115548	1113.870984	15.095040
21.261415	1104.393754	15.100058
20.719440	1094.178542	15.105075
20.980975	1102.369321	15.110093
21.310687	1099.584796	15.115111
20.831226	1105.119363	15.120128
21.080503	1110.234004	15.125146
21.342115	1114.169493	15.130163
21.208466	1113.706745	15.135181
21.306034	1114.696037	15.140199
21.014228	1117.010218	15.145216
20.925822	1110.394608	15.150234
21.382208	1116.560201	15.155251
21.336786	1111.671212	15.160269
21.251393	1104.628749	15.165287
21.096380	1117.114529	15.170304
21.134832	1107.073685	15.175322
20.957586	1111.861210	15.180339
20.931956	1109.138502	15.185357
21.176680	1108.736085	15.190375
21.007564	1114.577714	15.195392
20.935508	1120.755163	15.200410
21.436186	1128.575910	15.205427
21.425650	1130.679965	15.210445
21.809625	1138.001637	15.215463
21.671382	1138.131747	15.220480
21.548389	1131.073081	15.225498
21.776512	1132.585528	15.230515
21.589919	1134.025182	15.235533
21.739977	1140.166114	15.240551
21.494925	1132.445881	15.245568
21.739365	1139.160858	15.250586
21.700384	1132.789766	15.255603
21.524032	1140.997446	15.260621
21.773896	1135.673956	15.265639
21.827474	1132.958549	15.270656
21.432705	1132.098674	15.275674
21.447884	1136.945557	15.280691
21.307694	1144.163420	15.285709
21.734786	1135.501194	15.290727
21.900504	1142.428853	15.295744
21.801111	1131.129082	15.300762
21.792970	1135.016898	15.305779
21.678021	1135.189590	15.310797
21.744943	1129.765414	15.315815
21.666110	1136.977407	15.320832
21.771015	1146.269384	15.325850
22.178038	1151.781026	15.330867
21.937122	1167.718746	15.335885
22.170977	1160.229119	15.340903
21.958609	1165.064227	15.345920
22.158432	1160.111627	15.350938
22.041834	1158.644519	15.355955
22.552421	1162.280777	15.360973
22.681624	1157.043867	15.365991
22.409725	1134.285949	15.371008
22.234816	1125.661981	15.376026
22.314423	1124.894903	15.381043
21.901101	1126.993074	15.386061
22.224622	1129.771881	15.391079
22.150085	1126.336077	15.396096
22.342760	1132.214424	15.401114
22.366492	1140.973462	15.406131
22.423892	1152.842105	15.411149
22.491882	1144.844649	15.416167
22.109548	1143.288647	15.421184
22.564087	1151.301710	15.426202
22.778220	1147.909254	15.431219
22.425415	1134.083229	15.436237
22.539467	1126.650930	15.441255
22.484243	1135.658116	15.446272
22.505034	1132.956427	15.451290
22.446521	1139.623732	15.456307
22.169656	1147.312323	15.461325
22.591989	1157.962499	15.466343
22.856227	1154.103469	15.471360
22.288690	1160.325495	15.476378
22.573210	1158.206312	15.481395
22.445802	1165.159476	15.486413
22.602843	1152.442726	15.491431
22.742133	1161.848283	15.496448
22.743344	1162.389444	15.501466
22.799424	1160.659394	15.506483
22.571166	1167.921433	15.511501
22.539480	1149.859551	15.516519
22.558895	1156.565877	15.521536
22.742513	1164.069281	15.526554
22.672499	1146.776333	15.531571
22.312372	1157.097532	15.536589
22.678189	1175.062651	15.541607
22.786029	1181.818461	15.546624
22.729644	1178.577256	15.551642
22.952330	1181.007890	15.556659
22.865922	1187.599541	15.561677
23.137218	1189.282762	15.566695
23.024727	1188.277151	15.571712
22.952884	1183.943292	15.576730
23.177626	1180.712837	15.581747
22.861438	1188.128863	15.586765
22.803738	1180.193223	15.591783
22.780853	1175.539826	15.596800
22.648970	1198.503991	15.601818
23.006802	1201.825900	15.606835
22.914030	1214.876583	15.611853
23.540534	1211.932871	15.616871
23.535683	1216.885071	15.621888
23.612146	1216.106701	15.626906
23.703611	1207.560060	15.631923
23.612520	1206.603251	15.636941
23.627800	1200.472707	15.641959
23.881035	1190.364221	15.646976
23.614397	1178.733963	15.651994
23.731469	1165.135306	15.657011
23.392254	1169.873790	15.662029
23.464321	1166.523839	15.667047
23.813183	1164.337665	15.672064
23.615192	1172.537935	15.677082
23.528388	1173.043728	15.682099
23.526776	1165.445606	15.687117
23.805338	1169.493641	15.692135
23.990088	1164.778178	15.697152
23.498242	1163.915540	15.702170
23.788611	1164.081097	15.707187
23.719319	1168.297179	15.712205
23.610938	1167.431431	15.717223
23.916693	1165.296514	15.722240
23.561106	1177.330665	15.727258
24.017050	1165.392922	15.732275
23.373308	1173.417294	15.737293
23.686639	1158.530573	15.742311
23.700637	1172.806325	15.747328
23.899570	1197.221333	15.752346
23.975538	1191.144482	15.757363
23.873749	1207.031560	15.762381
24.242115	1201.401750	15.767399
24.030145	1204.039272	15.772416
24.066733	1199.688567	15.777434
24.275390	1197.908744	15.782451
24.184265	1195.728377	15.787469
24.268230	1182.946980	15.792487
24.120712	1178.025336	15.797504
23.828741	1176.762564	15.802522
24.303454	1183.505425	15.807539
24.400877	1191.401891	15.812557
24.157729	1188.431479	15.817575
24.105063	1187.195068	15.822592
24.518424	1195.209488	15.827610
24.257862	1188.378376	15.832627
23.956038	1199.815448	15.837645
24.165499	1192.360174	15.842663
24.498802	1194.968477	15.847680
24.254273	1197.273237	15.852698
24.687951	1190.103909	15.857715
24.283136	1195.223758	15.862733
24.291531	1196.659353	15.867751
24.317741	1191.796226	15.872768
24.344663	1190.947355	15.877786
24.557818	1187.447184	15.882803
24.305496	1196.465513	15.887821
24.394359	1188.679515	15.892839
24.204663	1202.139585	15.897856
24.301283	1196.607305	15.902874
24.462790	1195.274669	15.907891
24.417864	1196.953760	15.912909
24.651573	1205.291339	15.917927
24.759264	1225.327671	15.922944
24.563797	1230.657213	15.927962
24.915406	1224.630986	15.932979
24.746686	1227.318800	15.937997
24.472857	1219.577717	15.943015
24.905140	1224.710795	15.948032
24.698229	1227.322677	15.953050
24.900520	1215.452252	15.958067
24.684595	1220.896996	15.963085
24.905860	1223.892807	15.968103
24.764065	1217.939932	15.973120
24.541478	1220.425291	15.978138
24.873389	1219.095431	15.983155
24.747678	1224.109452	15.988173
25.193375	1246.167881	15.993191
25.399991	1241.753078	15.998208
25.365752	1233.926104	16.003226
25.349610	1215.234425	16.008243
25.138800	1226.936691	16.013261
25.198600	1213.204212	16.018279
25.114679	1210.614003	16.023296
25.006022	1213.666224	16.028314
25.247814	1224.401570	16.033331
25.660985	1227.613898	16.038349
25.173997	1227.660642	16.043367
25.342336	1218.525260	16.048384
25.194069	1232.882759	16.053402
25.362766	1245.488846	16.058419
25.612463	1247.113855	16.063437
25.202614	1254.762794	16.068455
25.590364	1241.097428	16.073472
25.634143	1250.046888	16.078490
25.856874	1244.456230	16.083507
25.848269	1235.674643	16.088525
25.930394	1219.314945	16.093543
26.074699	1213.166099	16.098560
25.516038	1218.976850	16.103578
25.567363	1210.125477	16.108595
25.253924	1217.827661	16.113613
25.290544	1213.746619	16.118631
25.717530	1229.136401	16.123648
25.629932	1242.304745	16.128666
25.758289	1235.806196	16.133683
25.937582	1239.362504	16.138701
25.925024	1240.072878	16.143719
26.031202	1239.162408	16.148736
25.973670	1247.843680	16.153754
26.050579	1243.208320	16.158771
26.228203	1228.918471	16.163789
25.822336	1225.756603	16.168807
25.919081	1216.217788	16.173824
25.856782	1234.351374	16.178842
26.248706	1235.693305	16.183859
26.322914	1239.926500	16.188877
26.171974	1227.133719	16.193895
26.341050	1206.057042	16.198912
25.944525	1216.438264	16.203930
25.969447	1214.481902	16.208947
26.128817	1224.348312	16.213965
25.871637	1225.124146	16.218983
26.184815	1232.441884	16.224000
25.851830	1251.609414	16.229018
25.805850	1238.649578	16.234035
25.949143	1242.629962	16.239053
25.967799	1244.118971	16.244071
26.023729	1241.343315	16.249088
26.135362	1244.903391	16.254106
26.344972	1265.879092	16.259123
26.419910	1275.691855	16.264141
26.390030	1284.181157	16.269159
26.511058	1262.682881	16.274176
26.373665	1272.660455	16.279194
26.553397	1275.871044	16.284211
26.672536	1267.422129	16.289229
26.466742	1274.386401	16.294247
26.452403	1274.293958	16.299264
26.645084	1281.124682	16.304282
26.802501	1275.168113	16.309299
26.650784	1272.147843	16.314317
26.560899	1279.229461	16.319335
26.480453	1265.961171	16.324352
26.721463	1263.557881	16.329370
26.640092	1261.242031	16.334387
26.719918	1266.830932	16.339405
26.250298	1270.165985	16.344423
27.119869	1275.901565	16.349440
26.915512	1290.238521	16.354458
27.129408	1300.584478	16.359475
27.361067	1299.616142	16.364493
26.856048	1283.677968	16.369511
27.025414	1272.987331	16.374528
27.057838	1281.631624	16.379546
26.795642	1294.463694	16.384563
27.345854	1293.479811	16.389581
27.497632	1301.797990	16.394599
27.245801	1276.955903	16.399616
26.977314	1276.395093	16.404634
27.063960	1285.022502	16.409651
27.355241	1291.774247	16.414669
27.130946	1288.885323	16.419687
27.394759	1290.137928	16.424704
27.718922	1295.142156	16.429722
27.365395	1294.172663	16.434739
27.807899	1279.693079	16.439757
27.036267	1274.213750	16.444775
27.199932	1274.389739	16.449792
27.074299	1299.978100	16.454810
27.216188	1286.666932	16.459827
27.389736	1289.060870	16.464845
27.307665	1293.216122	16.469863
27.490758	1284.651453	16.474880
27.339965	1289.781471	16.479898
27.201276	1290.260460	16.484915
27.725920	1292.998782	16.489933
27.335060	1299.247400	16.494951
27.511179	1306.024198	16.499968
27.839937	1316.482959	16.504986
27.945344	1312.923113	16.510003
28.020879	1312.917302	16.515021
28.300484	1314.758993	16.520039
28.138542	1291.571953	16.525056
28.034879	1286.100094	16.530074
28.041241	1279.791875	16.535091
28.181053	1275.678705	16.540109
28.094353	1284.300674	16.545127
28.239521	1280.031107	16.550144
28.392651	1283.435876	16.555162
28.210026	1283.946970	16.560179
28.535267	1276.814129	16.565197
28.510751	1279.087450	16.570215
28.245480	1280.018956	16.575232
28.390111	1250.138392	16.580250
28.428403	1251.483987	16.585267
28.174636	1243.581296	16.590285
28.133111	1251.250112	16.595303
28.081147	1245.126790	16.600320
28.088443	1242.180091	16.605338
28.149499	1269.842003	16.610355
28.301960	1276.808933	16.615373
28.249185	1286.559074	16.620391
28.493832	1279.604976	16.625408
28.665519	1277.180136	16.630426
28.408098	1276.086014	16.635443
28.628605	1272.915297	16.640461
28.097105	1271.306912	16.645479
28.321034	1272.183878	16.650496
28.368178	1273.170932	16.655514
28.284543	1279.695629	16.660531
28.362660	1278.324880	16.665549
28.318147	1276.513116	16.670567
28.853299	1282.435381	16.675584
28.547665	1271.616224	16.680602
28.280685	1296.149378	16.685619
28.533006	1289.346749	16.690637
28.426747	1313.277651	16.695655
28.431530	1305.859098	16.700672
28.972097	1310.901769	16.705690
28.828604	1311.335890	16.710707
28.886591	1308.311071	16.715725
28.452091	1307.133785	16.720743
28.428865	1311.909550	16.725760
28.802379	1316.960305	16.730778
28.984669	1329.988594	16.735795
29.230061	1328.910497	16.740813
28.745334	1336.340828	16.745831
28.701121	1322.294844	16.750848
29.170441	1328.952449	16.755866
29.212173	1336.866120	16.760883
29.272010	1320.850557	16.765901
29.161316	1323.483076	16.770919
29.194093	1329.047144	16.775936
29.412032	1324.674528	16.780954
28.995468	1330.068410	16.785971
29.474543	1320.037259	16.790989
29.444360	1324.529156	16.796007
29.251410	1323.488879	16.801024
29.781451	1318.059313	16.806042
29.875899	1329.194010	16.811059
29.855062	1320.799432	16.816077
29.627741	1329.810927	16.821095
29.638275	1322.276061	16.826112
29.651502	1323.713620	16.831130
29.352471	1328.992694	16.836147
29.547817	1315.236413	16.841165
29.421861	1321.574076	16.846183
29.590150	1323.024443	16.851200
29.860535	1325.149546	16.856218
29.763716	1319.175771	16.861235
29.833097	1321.172477	16.866253
29.601199	1322.793687	16.871271
29.927372	1317.436586	16.876288
30.110395	1318.214059	16.881306
29.762008	1320.274692	16.886323
30.007707	1315.868332	16.891341
29.706207	1322.977268	16.896359
29.650071	1316.171174	16.901376
29.991956	1320.436668	16.906394
29.902654	1348.918562	16.911411
29.999066	1357.397937	16.916429
30.060248	1348.258637	16.921447
30.132426	1348.882887	16.926464
30.141850	1341.119071	16.931482
29.958388	1340.666957	16.936499
30.222319	1342.701406	16.941517
30.459229	1343.016791	16.946535
30.592053	1348.856746	16.951552
30.441513	1335.771300	16.956570
30.617468	1348.532164	16.961587
30.646317	1341.263525	16.966605
30.663067	1334.179571	16.971623
30.168709	1324.040538	16.976640
30.518021	1323.740020	16.981658
30.270438	1340.210106	16.986675
30.627648	1342.271569	16.991693
30.278366	1340.273061	16.996711
30.445497	1345.073494	17.001728
30.482872	1339.212441	17.006746
30.481881	1345.001410	17.011763
30.470610	1340.257848	17.016781
30.562726	1342.512186	17.021799
30.635609	1336.975534	17.026816
30.601195	1343.100753	17.031834
30.674578	1348.904133	17.036851
30.646503	1348.291551	17.041869
30.624692	1357.609048	17.046887
31.050540	1367.741089	17.051904
31.433916	1370.910371	17.056922
31.104669	1362.750095	17.061939
30.991079	1346.209808	17.066957
31.036252	1347.319238	17.071975
30.833987	1356.569487	17.076992
31.388763	1370.021314	17.082010
31.346901	1361.645169	17.087027
31.190872	1348.914154	17.092045
30.956946	1345.327240	17.097063
31.180635	1364.084285	17.102080
31.374244	1358.693301	17.107098
31.230891	1363.051663	17.112115
31.259531	1371.699390	17.117133
31.537227	1372.939459	17.122151
31.331058	1365.500430	17.127168
31.282375	1368.094304	17.132186
30.992613	1368.559824	17.137203
31.246700	1365.772863	17.142221
31.488078	1360.275517	17.147239
31.355890	1367.774821	17.152256
31.767037	1360.388303	17.157274
31.693313	1370.040408	17.162291
31.627203	1360.198663	17.167309
31.642861	1356.679314	17.172327
31.377208	1370.916693	17.177344
31.317369	1369.719648	17.182362
31.596122	1363.946413	17.187379
31.707881	1359.361130	17.192397
31.339572	1373.772262	17.197415
31.479693	1382.884519	17.202432
31.795532	1388.414552	17.207450
31.650162	1395.509776	17.212467
31.667865	1394.623057	17.217485
31.825834	1389.747811	17.222503
31.857857	1397.727298	17.227520
32.060796	1385.842856	17.232538
31.813252	1396.519896	17.237555
32.068108	1383.337502	17.242573
32.348741	1383.630660	17.247591
31.798143	1393.430543	17.252608
31.702953	1397.720675	17.257626
31.892682	1403.940549	17.262643
32.157100	1415.431690	17.267661
32.135768	1408.102859	17.272679
32.166361	1420.478902	17.277696
32.551380	1409.382655	17.282714
32.504096	1409.539379	17.287731
32.183191	1413.569404	17.292749
32.807948	1413.007756	17.297767
32.417939	1411.263637	17.302784
32.591521	1405.337008	17.307802
32.732444	1415.145584	17.312819
32.684119	1410.510518	17.317837
32.926775	1419.955350	17.322855
32.739292	1409.351883	17.327872
33.031335	1406.687735	17.332890
32.837007	1401.360821	17.337907
32.620569	1408.842260	17.342925
33.024569	1397.960575	17.347943
32.615402	1409.006995	17.352960
33.095945	1399.313727	17.357978
32.812597	1411.067950	17.362995
32.609715	1409.152183	17.368013
33.203936	1406.784649	17.373031
32.845860	1406.640679	17.378048
33.011089	1402.545298	17.383066
33.057649	1401.554180	17.388083
32.975181	1409.810174	17.393101
32.941761	1411.564539	17.398119
32.975432	1409.087424	17.403136
33.122248	1406.784805	17.408154
32.940444	1402.859698	17.413171
33.139493	1406.422604	17.418189
33.097866	1401.508091	17.423207
33.126839	1398.509730	17.428224
33.453858	1400.158911	17.433242
33.106571	1404.362998	17.438259
32.974235	1413.039866	17.443277
33.314966	1425.431686	17.448295
33.327992	1436.088671	17.453312
33.345178	1432.165915	17.458330
33.204005	1438.949053	17.463347
32.996455	1435.508517	17.468365
33.194861	1436.225173	17.473383
33.455259	1436.934675	17.478400
33.819451	1453.898061	17.483418
33.887663	1466.583626	17.488435
33.842316	1450.751548	17.493453
34.069739	1440.933402	17.498471
33.462054	1434.383490	17.503488
33.674980	1432.202158	17.508506
33.977082	1446.454685	17.513523
34.168712	1465.399066	17.518541
34.344862	1449.534898	17.523559
33.611007	1444.079541	17.528576
33.968924	1449.537250	17.533594
33.978728	1462.211655	17.538611
33.854475	1467.554242	17.543629
34.425868	1467.941985	17.548647
34.003281	1473.528643	17.553664
34.180806	1465.767926	17.558682
34.452620	1463.511449	17.563699
34.143954	1466.183983	17.568717
34.473776	1455.311832	17.573735
34.253796	1459.559732	17.578752
34.290345	1461.319402	17.583770
34.435501	1458.349355	17.588787
34.380587	1456.057818	17.593805
34.578042	1451.848409	17.598823
34.413572	1456.996896	17.603840
34.256189	1461.596193	17.608858
34.808443	1454.054292	17.613875
34.378361	1454.438022	17.618893
34.771774	1452.600692	17.623911
34.346724	1457.140542	17.628928
34.586760	1448.907253	17.633946
34.793766	1447.102088	17.638963
34.423203	1451.546269	17.643981
35.056099	1444.396468	17.648999
34.938822	1459.862377	17.654016
35.013860	1442.467826	17.659034
34.964985	1453.947684	17.664051
34.957863	1452.469438	17.669069
34.854359	1444.838903	17.674087
34.800875	1454.069993	17.679104
34.951109	1449.137355	17.684122
34.980950	1446.096715	17.689139
35.047021	1450.565564	17.694157
35.278079	1447.977685	17.699175
34.965878	1446.454087	17.704192
35.002674	1445.611828	17.709210
35.101410	1439.111818	17.714227
35.088636	1438.238036	17.719245
35.094731	1449.526478	17.724263
35.355396	1455.886153	17.729280
35.242971	1459.543359	17.734298
35.399570	1455.155707	17.739315
35.288521	1467.871856	17.744333
35.804887	1460.267021	17.749351
35.660550	1468.021141	17.754368
35.732914	1469.958711	17.759386
35.715238	1467.597993	17.764403
35.603839	1464.606809	17.769421
35.823023	1464.409804	17.774439
35.830643	1459.379610	17.779456
35.640626	1468.530255	17.784474
35.541314	1464.418986	17.789491
35.581520	1463.503721	17.794509
35.860932	1465.656083	17.799527
35.671403	1467.063578	17.804544
35.548526	1464.270752	17.809562
35.811731	1462.325146	17.814579
35.552253	1464.968245	17.819597
35.702974	1463.756274	17.824615
35.877647	1486.427794	17.829632
35.636891	1491.586217	17.834650
36.017304	1491.939563	17.839667
35.649094	1502.047378	17.844685
35.901267	1486.889807	17.849703
36.072260	1493.804938	17.854720
36.053275	1493.745548	17.859738
36.345171	1498.315849	17.864755
36.340345	1511.188782	17.869773
36.513353	1508.684556	17.874791
36.512176	1512.526429	17.879808
36.154996	1503.692393	17.884826
36.833868	1507.122817	17.889843
36.664028	1505.122414	17.894861
36.516259	1498.334619	17.899879
36.549444	1491.183297	17.904896
36.463565	1496.008901	17.909914
36.983136	1504.885333	17.914931
36.406830	1503.307990	17.919949
36.499186	1507.112269	17.924967
36.716430	1515.906284	17.929984
36.789226	1516.873343	17.935002
36.965838	1515.276365	17.940019
36.686321	1522.808499	17.945037
36.920359	1514.754514	17.950055
37.063085	1517.697691	17.955072
37.126098	1513.748006	17.960090
37.212204	1514.606163	17.965107
36.999240	1517.768690	17.970125
37.532096	1516.707761	17.975143
37.227326	1518.562750	17.980160
37.220372	1523.516185	17.985178
37.026343	1521.550114	17.990195
36.929520	1523.217001	17.995213
37.229236	1520.398808	18.000231
36.927968	1506.124129	18.005248
37.164529	1519.717557	18.010266
37.493146	1513.865116	18.015283
37.045030	1513.864060	18.020301
37.208326	1505.380511	18.025319
37.565611	1521.360108	18.030336
37.351378	1524.534658	18.035354
37.686786	1534.181855	18.040371
37.404310	1538.871255	18.045389
37.578091	1539.655787	18.050407
38.059599	1544.441431	18.055424
37.696899	1548.741422	18.060442
37.860030	1531.912823	18.065459
38.002959	1535.823661	18.070477
38.261279	1535.555193	18.075495
37.886263	1536.228189	18.080512
37.557977	1537.735916	18.085530
38.139790	1533.817710	18.090547
37.948742	1532.109797	18.095565
37.811770	1535.387254	18.100583
37.987971	1532.186448	18.105600
38.194033	1534.047870	18.110618
38.223310	1524.858651	18.115635
38.217425	1527.873774	18.120653
38.129943	1529.394624	18.125671
38.313753	1529.630260	18.130688
37.871950	1527.064836	18.135706
38.057037	1524.091289	18.140723
38.465845	1523.774580	18.145741
38.379784	1531.421017	18.150759
38.220256	1532.897151	18.155776
38.428451	1529.615439	18.160794
38.400417	1545.176046	18.165811
38.276208	1549.492697	18.170829
38.893866	1553.989579	18.175847
38.940977	1553.439294	18.180864
38.698768	1549.331281	18.185882
38.952486	1550.623380	18.190899
38.423972	1559.085870	18.195917
38.701079	1554.232502	18.200935
39.087082	1568.413719	18.205952
38.856316	1555.881171	18.210970
38.900848	1553.190029	18.215987
39.036640	1556.771751	18.221005
39.017855	1563.412558	18.226023
38.917947	1559.245852	18.231040
39.256996	1555.102249	18.236058
39.006766	1550.092442	18.241075
39.020632	1560.752129	18.246093
38.940872	1558.850917	18.251111
38.903904	1556.746535	18.256128
38.789234	1554.249959	18.261146
39.008487	1551.408914	18.266163
38.886388	1565.261990	18.271181
39.013889	1576.630737	18.276199
39.568533	1579.180666	18.281216
39.369767	1582.796742	18.286234
39.435027	1576.398693	18.291251
39.494087	1574.936205	18.296269
39.791948	1566.021212	18.301287
39.843596	1568.467345	18.306304
39.792088	1565.467761	18.311322
39.980312	1568.250634	18.316339
39.994502	1566.639310	18.321357
40.240385	1563.886748	18.326375
40.182906	1559.109067	18.331392
39.833074	1550.909987	18.336410
40.064733	1540.734784	18.341427
39.657498	1543.734336	18.346445
39.645337	1550.845677	18.351463
40.130459	1559.079064	18.356480
39.715744	1567.362413	18.361498
39.736093	1566.287454	18.366515
39.741288	1563.977642	18.371533
39.698842	1564.122540	18.376551
40.203727	1560.243098	18.381568
39.844536	1571.317939	18.386586
39.999680	1586.333193	18.391603
40.383503	1594.588554	18.396621
40.291183	1593.568933	18.401639
40.493446	1585.587908	18.406656
40.437838	1595.805634	18.411674
40.915613	1595.753833	18.416691
40.860303	1586.097940	18.421709
40.752896	1587.241014	18.426727
41.353522	1580.306354	18.431744
40.982495	1569.830524	18.436762
40.833097	1560.092256	18.441779
40.677505	1554.326972	18.446797
40.874159	1553.891198	18.451815
40.705235	1542.536541	18.456832
40.358918	1560.849209	18.461850
40.896143	1567.192097	18.466867
40.899618	1574.173688	18.471885
40.656429	1588.420525	18.476903
40.860358	1581.101415	18.481920
40.946466	1588.964140	18.486938
40.881443	1584.790841	18.491955
40.880689	1582.578863	18.496973
41.010834	1588.670136	18.501991
40.837860	1581.859329	18.507008
41.091919	1603.972959	18.512026
41.137954	1610.149084	18.517043
41.496344	1621.600352	18.522061
41.268492	1622.479595	18.527079
41.404999	1605.240390	18.532096
41.125827	1623.063634	18.537114
41.486473	1619.635702	18.542131
41.618251	1612.429749	18.547149
41.168588	1615.710769	18.552167
41.472080	1602.088225	18.557184
41.459126	1615.814153	18.562202
41.531947	1614.198591	18.567219
41.848662	1634.668814	18.572237
41.703399	1642.544825	18.577255
42.256056	1649.710364	18.582272
41.663480	1634.550536	18.587290
41.496070	1633.318595	18.592307
41.696393	1642.607217	18.597325
41.989093	1641.516907	18.602343
42.156367	1641.023416	18.607360
41.914568	1636.605869	18.612378
41.808731	1643.329287	18.617395
42.052982	1637.003430	18.622413
42.308748	1642.843928	18.627431
42.223966	1632.310638	18.632448
42.178864	1639.344820	18.637466
42.296981	1640.737416	18.642483
42.244935	1645.875941	18.647501
42.112563	1647.273165	18.652519
42.326173	1652.352184	18.657536
42.080679	1672.316304	18.662554
42.324108	1670.740883	18.667571
43.000996	1666.389921	18.672589
42.467265	1669.364852	18.677607
42.732685	1666.310212	18.682624
42.642092	1669.675261	18.687642
42.621600	1665.529972	18.692659
42.632887	1659.719589	18.697677
42.590661	1665.898596	18.702695
42.557101	1654.807968	18.707712
42.701285	1671.788870	18.712730
42.883730	1677.919910	18.717747
42.984407	1673.261968	18.722765
42.984178	1681.398928	18.727783
43.497836	1675.704251	18.732800
43.502391	1680.729838	18.737818
43.546194	1675.960484	18.742835
43.776842	1669.235307	18.747853
43.648158	1660.267929	18.752871
43.637571	1650.665191	18.757888
43.717163	1646.752874	18.762906
43.420409	1645.043226	18.767923
43.850333	1651.914604	18.772941
43.819343	1649.028914	18.777959
43.397993	1641.878267	18.782976
43.495222	1642.127508	18.787994
43.632087	1649.820807	18.793011
43.868697	1636.291238	18.798029
43.558968	1643.413891	18.803047
43.624668	1637.625181	18.808064
43.478279	1641.473899	18.813082
43.495595	1634.488530	18.818099
43.801544	1647.398112	18.823117
43.529667	1662.759212	18.828135
44.016396	1664.117710	18.833152
43.700859	1673.035799	18.838170
43.794746	1670.706506	18.843187
44.177370	1666.781218	18.848205
43.874162	1670.709156	18.853223
43.905450	1665.798975	18.858240
43.663810	1683.105429	18.863258
43.924547	1691.605312	18.868275
44.371681	1693.416843	18.873293
44.527994	1702.211643	18.878311
44.978112	1688.998505	18.883328
44.881720	1692.870815	18.888346
44.329873	1699.088081	18.893363
44.544469	1688.984908	18.898381
44.216395	1698.429890	18.903399
44.436853	1691.544588	18.908416
44.693218	1686.611557	18.913434
44.364047	1697.399612	18.918451
44.726204	1697.104828	18.923469
44.659050	1691.382667	18.928487
44.824055	1692.739129	18.933504
44.933524	1700.232680	18.938522
44.523498	1696.298974	18.943539
44.893494	1701.958700	18.948557
44.907086	1719.401905	18.953575
45.281919	1712.958252	18.958592
45.243546	1712.024537	18.963610
45.217803	1715.833536	18.968627
45.587844	1713.466999	18.973645
45.649280	1716.687107	18.978663
45.733996	1705.966542	18.983680
45.416982	1686.233766	18.988698
44.923280	1689.679993	18.993715
45.210395	1694.194455	18.998733
45.537193	1708.632488	19.003751
45.715257	1716.630780	19.008768
45.598206	1716.779418	19.013786
45.370874	1720.046735	19.018803
45.600120	1715.449693	19.023821
45.495818	1723.664208	19.028839
45.558498	1714.810266	19.033856
45.817112	1716.342508	19.038874
45.616452	1703.394212	19.043891
46.019564	1713.965294	19.048909
45.922731	1709.907484	19.053927
46.046606	1701.306366	19.058944
45.765884	1700.134984	19.063962
45.902000	1716.925941	19.068979
46.370435	1717.676077	19.073997
46.168949	1739.728609	19.079015
46.359132	1730.638902	19.084032
46.381582	1740.711861	19.089050
46.479107	1737.648104	19.094067
46.767636	1738.115154	19.099085
46.319550	1719.881660	19.104103
46.121341	1731.237334	19.109120
46.658454	1724.407260	19.114138
46.441037	1739.393642	19.119155
46.704638	1739.421139	19.124173
46.939445	1741.685678	19.129191
46.862958	1740.868531	19.134208
46.840057	1733.048475	19.139226
46.762749	1746.848600	19.144243
46.951966	1732.856751	19.149261
46.649036	1733.172895	19.154279
46.905790	1736.888097	19.159296
47.240440	1739.116750	19.164314
46.795832	1737.581269	19.169331
47.138135	1732.033555	19.174349
46.941783	1737.072474	19.179367
47.298227	1733.026327	19.184384
47.287649	1733.917101	19.189402
47.159195	1728.417316	19.194419
47.632737	1727.166236	19.199437
47.062818	1732.094411	19.204455
47.190246	1733.076025	19.209472
47.366653	1734.991219	19.214490
47.018963	1746.448519	19.219507
47.472857	1739.940928	19.224525
47.473551	1754.639895	19.229543
47.218137	1761.922470	19.234560
47.700081	1760.677472	19.239578
47.287087	1771.100381	19.244595
47.795435	1762.963668	19.249613
47.626867	1770.162129	19.254631
47.965507	1759.024131	19.259648
47.736793	1759.920454	19.264666
47.418400	1758.189980	19.269683
47.643524	1762.708861	19.274701
47.929445	1778.273819	19.279719
47.909979	1784.035315	19.284736
48.263115	1789.143157	19.289754
48.152080	1790.362439	19.294771
48.273723	1785.783655	19.299789
48.253344	1791.017358	19.304807
48.223167	1786.580735	19.309824
48.704085	1784.028438	19.314842
48.131622	1787.392108	19.319859
48.534052	1781.812729	19.324877
48.525516	1783.431506	19.329895
48.248251	1783.700472	19.334912
48.548376	1782.841200	19.339930
48.257110	1783.946344	19.344947
48.383191	1788.880903	19.349965
48.658509	1795.041828	19.354983
49.000664	1804.371541	19.360000
48.649551	1803.814994	19.365018
48.430751	1804.336446	19.370035
48.674338	1801.579107	19.375053
48.506410	1803.349966	19.380071
48.588163	1815.587902	19.385088
48.978161	1813.880233	19.390106
49.207627	1827.107793	19.395123
49.205965	1825.952223	19.400141
49.462424	1824.390369	19.405159
49.463700	1818.783164	19.410176
49.588194	1821.029829	19.415194
49.723895	1821.260867	19.420211
50.006900	1825.011491	19.425229
50.151476	1818.165123	19.430247
49.727194	1804.925959	19.435264
49.756313	1791.520898	19.440282
49.745970	1792.692342	19.445299
49.610197	1781.084364	19.450317
49.815169	1794.489194	19.455335
49.561649	1795.395153	19.460352
49.922936	1805.034282	19.465370
49.797892	1813.468038	19.470387
49.946458	1805.670627	19.475405
49.883714	1824.465996	19.480423
49.991520	1818.565103	19.485440
50.193697	1814.553630	19.490458
49.855182	1826.429145	19.495475
49.879377	1818.892554	19.500493
50.164194	1816.076785	19.505511
49.867948	1805.619861	19.510528
50.097382	1823.989899	19.515546
49.939596	1839.367251	19.520563
50.027862	1842.693949	19.525581
50.349169	1842.541779	19.530599
50.194592	1844.777351	19.535616
50.612958	1839.257901	19.540634
50.512260	1849.967931	19.545651
50.615375	1865.820446	19.550669
50.883214	1868.989745	19.555687
50.938702	1875.493538	19.560704
50.862774	1875.738098	19.565722
50.904937	1878.549634	19.570739
50.704686	1871.977483	19.575757
51.531266	1866.944111	19.580775
51.239978	1881.448028	19.585792
51.469926	1870.069355	19.590810
51.298914	1869.821453	19.595827
51.559424	1866.901841	19.600845
51.449033	1863.640728	19.605863
51.136909	1856.539542	19.610880
51.365795	1856.322025	19.615898
51.294554	1864.110649	19.620915
51.360209	1869.220630	19.625933
51.426428	1873.474617	19.630951
51.383608	1878.639638	19.635968
51.467242	1877.841540	19.640986
51.402115	1871.273309	19.646003
51.374091	1873.124467	19.651021
51.687112	1865.788666	19.656039
51.269277	1872.386875	19.661056
51.641465	1885.892731	19.666074
51.720652	1895.972503	19.671091
51.681672	1906.781368	19.676109
51.694969	1902.066228	19.681127
51.946872	1902.636221	19.686144
52.382604	1905.519750	19.691162
52.249608	1903.391911	19.696179
52.047874	1906.386902	19.701197
52.241654	1897.589806	19.706215
51.933108	1910.538354	19.711232
52.570883	1913.608777	19.716250
52.429699	1928.344875	19.721267
52.209493	1934.491365	19.726285
52.395298	1933.001086	19.731303
52.157695	1927.615434	19.736320
52.449342	1937.382756	19.741338
52.504530	1929.694897	19.746355
52.451287	1920.403018	19.751373
52.752257	1941.199886	19.756391
52.590933	1956.520854	19.761408
53.192881	1956.244087	19.766426
53.477873	1953.490863	19.771443
53.124846	1955.820063	19.776461
53.483448	1949.160507	19.781479
53.136886	1946.789417	19.786496
53.244799	1942.957752	19.791514
53.353000	1938.689819	19.796531
53.756857	1946.887316	19.801549
53.699441	1936.275255	19.806567
53.161123	1920.038410	19.811584
53.471142	1929.993225	19.816602
53.518279	1937.051187	19.821619
53.746127	1939.684629	19.826637
53.814721	1936.202020	19.831655
53.528072	1938.896170	19.836672
53.632535	1949.208389	19.841690
53.809416	1945.957781	19.846707
53.856112	1950.181569	19.851725
54.279904	1932.951339	19.856743
53.833672	1940.217681	19.861760
54.179628	1945.396454	19.866778
53.877254	1938.162508	19.871795
54.089886	1938.376825	19.876813
53.953256	1943.026750	19.881831
53.935011	1938.022353	19.886848
53.924066	1941.698633	19.891866
54.351154	1942.402110	19.896883
53.972847	1959.468987	19.901901
54.600587	1960.241478	19.906919
54.111745	1975.387766	19.911936
54.386862	1965.946009	19.916954
54.313178	1977.435496	19.921971
54.178679	1974.716557	19.926989
54.150286	1974.898493	19.932007
54.687995	1991.721427	19.937024
54.756487	1990.941982	19.942042
54.982479	1992.568651	19.947059
54.640601	1997.424754	19.952077
55.030238	1988.962378	19.957095
54.745940	2005.603050	19.962112
54.656494	1994.803752	19.967130
54.876140	1999.676371	19.972147
54.756310	1989.697877	19.977165
55.170006	2004.007570	19.982183
55.092813	2023.041408	19.987200
55.537585	2024.339198	19.992218
55.600272	2018.983132	19.997235
55.295816	2025.088148	20.002253
55.759582	2018.623684	20.007271
55.915752	2030.199812	20.012288
55.463846	2025.993844	20.017306
55.512796	2022.664875	20.022323
55.311913	2027.548735	20.027341
55.763940	2022.949616	20.032359
55.745303	2025.543724	20.037376
55.666517	2019.287545	20.042394
56.034344	2026.360752	20.047411
55.576416	2015.040790	20.052429
55.823890	2019.464693	20.057447
55.884166	2040.686740	20.062464
56.197212	2045.744245	20.067482
56.154076	2047.566045	20.072499
56.002369	2053.724031	20.077517
56.499960	2036.132994	20.082535
56.101520	2060.134869	20.087552
56.217427	2042.601749	20.092570
56.009701	2060.082121	20.097587
56.361237	2066.047809	20.102605
56.922247	2059.996303	20.107623
56.834330	2072.033112	20.112640
56.988588	2076.953237	20.117658
57.192283	2070.972925	20.122675
56.938764	2067.403664	20.127693
57.390579	2070.136913	20.132711
57.203461	2064.988100	20.137728
57.225517	2056.554498	20.142746
57.219567	2045.020809	20.147763
56.887491	2063.994697	20.152781
57.407600	2059.733862	20.157799
57.052144	2057.452422	20.162816
57.195003	2060.540565	20.167834
57.766525	2056.396383	20.172851
57.631582	2064.536642	20.177869
57.354397	2056.064979	20.182887
57.482852	2068.876854	20.187904
57.751031	2058.492486	20.192922
57.635067	2064.304376	20.197939
57.261222	2064.092937	20.202957
57.718433	2054.512200	20.207975
57.569249	2058.118963	20.212992
57.696683	2069.612888	20.218010
57.928417	2075.281953	20.223027
58.071616	2087.090596	20.228045
58.176701	2084.682608	20.233063
58.054560	2082.977353	20.238080
57.955654	2083.324554	20.243098
58.066499	2075.373433	20.248115
58.013555	2088.233977	20.253133
58.053684	2082.985971	20.258151
58.181957	2083.336753	20.263168
58.201269	2101.669996	20.268186
58.758579	2106.327077	20.273203
58.339670	2112.615325	20.278221
58.709155	2106.041296	20.283239
58.556198	2120.138974	20.288256
58.569506	2108.083922	20.293274
58.960753	2100.699184	20.298291
58.778388	2100.126388	20.303309
59.221823	2097.733424	20.308327
59.134306	2095.789733	20.313344
59.276812	2103.553582	20.318362
59.508564	2098.053641	20.323379
59.587231	2099.055588	20.328397
59.385560	2097.484811	20.333415
59.594649	2100.530851	20.338432
59.483435	2101.374592	20.343450
59.612771	2093.112118	20.348467
59.412307	2112.637818	20.353485
59.424830	2099.861241	20.358503
59.587896	2101.311371	20.363520
59.888920	2105.171669	20.368538
59.579753	2097.705703	20.373555
59.318432	2103.403576	20.378573
59.572353	2098.386569	20.383591
60.030995	2098.110785	20.388608
59.810606	2102.291996	20.393626
59.526539	2102.967613	20.398643
59.546310	2118.375179	20.403661
59.737882	2117.075265	20.408679
59.834632	2127.617235	20.413696
59.702403	2136.737408	20.418714
59.685990	2142.328841	20.423731
59.758756	2158.959151	20.428749
60.145219	2155.641776	20.433767
60.012412	2158.950560	20.438784
60.162461	2179.170461	20.443802
60.620886	2177.633668	20.448819
60.760029	2186.037497	20.453837
60.940140	2183.637103	20.458855
60.522498	2179.717923	20.463872
60.687376	2182.245728	20.468890
61.014754	2180.249606	20.473907
60.773087	2179.092166	20.478925
61.022271	2180.936658	20.483943
61.098123	2177.926812	20.488960
60.742774	2187.251817	20.493978
61.420292	2191.614138	20.498995
61.258317	2207.590590	20.504013
61.556617	2210.805293	20.509031
61.649916	2208.745314	20.514048
61.306489	2214.653333	20.519066
61.591740	2213.438632	20.524083
61.394051	2209.013587	20.529101
61.553755	2213.969072	20.534119
61.605240	2207.437617	20.539136
61.698667	2220.469222	20.544154
61.638563	2207.556593	20.549171
61.615965	2210.737227	20.554189
61.967132	2204.861490	20.559207
62.086194	2220.129817	20.564224
61.977535	2233.657233	20.569242
62.387885	2220.266001	20.574259
62.247798	2224.094523	20.579277
61.940931	2230.014189	20.584295
62.090707	2230.588571	20.589312
61.928532	2232.855775	20.594330
62.605279	2223.107737	20.599347
62.549980	2232.529753	20.604365
62.434292	2225.818984	20.609383
62.468098	2228.878828	20.614400
62.268733	2244.505620	20.619418
62.882451	2257.019671	20.624435
62.583703	2261.143868	20.629453
62.766287	2260.093080	20.634471
63.064094	2256.097885	20.639488
62.697178	2267.659157	20.644506
62.945779	2248.420646	20.649523
62.966708	2256.023671	20.654541
63.106057	2256.795854	20.659559
63.526485	2257.435886	20.664576
62.743207	2247.376544	20.669594
63.384920	2258.872538	20.674611
63.586021	2277.850986	20.679629
63.660556	2284.479740	20.684647
63.794233	2281.426405	20.689664
63.685178	2293.323587	20.694682
63.719168	2286.551695	20.699699
63.538510	2286.889259	20.704717
63.711577	2280.517492	20.709735
63.735382	2280.261219	20.714752
64.209978	2286.718363	20.719770
63.851077	2271.165124	20.724787
63.697116	2278.816519	20.729805
63.988057	2280.450536	20.734823
63.973902	2289.626372	20.739840
64.096224	2307.281305	20.744858
64.313161	2318.826682	20.749875
64.190181	2321.887798	20.754893
64.238788	2322.265607	20.759911
64.550261	2318.266550	20.764928
63.912981	2316.264986	20.769946
64.636356	2327.273038	20.774963
64.812406	2339.628002	20.779981
64.767001	2336.285907	20.784999
64.968703	2346.714124	20.790016
65.017448	2344.335539	20.795034
64.986872	2338.268467	20.800051
64.925421	2337.903132	20.805069
65.269398	2341.657923	20.810087
65.466614	2332.772213	20.815104
65.119212	2330.998461	20.820122
65.472312	2336.852969	20.825139
65.546813	2332.709037	20.830157
65.052748	2343.619826	20.835175
65.271819	2329.323654	20.840192
64.899438	2337.057050	20.845210
65.683438	2349.834615	20.850227
65.588849	2347.454261	20.855245
65.636357	2360.962919	20.860263
66.205162	2350.153187	20.865280
65.837882	2353.657285	20.870298
66.205088	2352.152960	20.875315
66.324169	2357.843609	20.880333
66.124773	2351.219142	20.885351
66.791741	2343.258924	20.890368
66.894538	2345.600219	20.895386
66.806956	2351.070876	20.900403
66.611042	2340.126429	20.905421
66.394436	2343.974784	20.910439
66.484782	2334.292641	20.915456
66.679350	2343.750757	20.920474
66.988682	2332.174691	20.925491
67.318446	2339.320513	20.930509
67.123539	2345.636586	20.935527
67.329004	2328.714260	20.940544
67.036949	2308.674564	20.945562
67.046628	2302.117734	20.950579
66.833049	2309.340460	20.955597
66.655041	2313.299718	20.960615
67.290963	2317.988289	20.965632
67.165781	2329.160603	20.970650
67.202963	2322.330682	20.975667
67.094364	2326.846532	20.980685
67.142674	2330.859127	20.985703
67.457079	2330.069110	20.990720
67.401437	2333.319830	20.995738
67.406640	2323.992404	21.000755
67.414410	2337.206458	21.005773
67.560650	2353.335382	21.010791
68.056180	2348.153335	21.015808
67.962481	2353.338781	21.020826
67.639712	2353.403500	21.025843
67.852637	2352.563417	21.030861
67.918687	2354.856883	21.035879
68.012871	2354.326700	21.040896
67.912255	2363.941765	21.045914
68.179602	2365.669872	21.050931
68.546102	2379.890906	21.055949
68.236494	2381.347965	21.060967
68.565533	2377.814098	21.065984
68.468074	2382.326143	21.071002
68.676997	2380.547327	21.076019
68.641006	2377.269015	21.081037
68.515974	2384.709349	21.086055
68.788281	2373.192164	21.091072
68.858787	2380.834257	21.096090
68.842531	2392.237732	21.101107
68.806371	2400.680655	21.106125
68.641077	2402.568076	21.111143
68.920840	2397.587232	21.116160
69.233882	2402.370045	21.121178
69.435352	2405.833173	21.126195
69.411261	2406.498665	21.131213
69.221277	2407.900412	21.136231
69.660891	2416.433567	21.141248
69.579956	2433.805093	21.146266
69.707716	2434.946545	21.151283
70.044272	2424.804122	21.156301
69.905020	2420.350406	21.161319
70.291805	2426.135174	21.166336
70.119766	2430.915937	21.171354
70.144058	2424.828688	21.176371
70.341927	2420.693363	21.181389
70.467229	2419.191835	21.186407
70.420500	2421.356412	21.191424
70.475092	2418.402023	21.196442
70.337828	2414.121212	21.201459
70.509457	2410.892641	21.206477
70.007725	2415.884104	21.211495
70.271092	2413.138332	21.216512
70.753705	2412.891239	21.221530
70.610093	2438.928572	21.226547
71.080973	2437.034557	21.231565
70.920707	2444.356755	21.236583
71.086086	2439.773268	21.241600
70.979910	2436.792444	21.246618
70.845821	2437.254558	21.251635
71.334828	2430.186893	21.256653
71.205138	2433.218831	21.261671
71.315407	2425.516848	21.266688
71.331807	2434.252639	21.271706
71.082785	2434.344866	21.276723
71.291284	2438.944272	21.281741
71.033127	2456.380318	21.286759
71.550614	2467.941605	21.291776
71.578819	2462.613560	21.296794
71.829096	2459.006147	21.301811
72.061216	2457.752225	21.306829
71.935229	2469.182656	21.311847
71.857897	2458.483780	21.316864
72.041428	2460.153779	21.321882
71.815773	2458.913339	21.326899
72.143060	2472.374020	21.331917
72.131815	2485.101973	21.336935
72.212027	2491.095598	21.341952
72.119935	2484.607969	21.346970
72.203869	2500.248959	21.351987
72.768643	2491.122144	21.357005
72.433160	2498.653023	21.362023
72.452615	2494.162278	21.367040
72.461918	2508.557367	21.372058
72.501049	2521.067520	21.377075
72.870597	2517.310345	21.382093
72.723828	2522.969252	21.387111
72.972688	2520.238472	21.392128
72.870929	2521.708639	21.397146
73.263959	2535.237979	21.402163
73.860634	2532.873816	21.407181
73.360200	2534.291736	21.412199
73.670094	2539.079839	21.417216
73.895959	2534.568951	21.422234
73.691042	2534.384941	21.427251
74.121720	2532.592875	21.432269
73.910751	2530.115295	21.437287
73.932758	2520.164857	21.442304
73.977000	2515.696759	21.447322
74.230772	2535.141195	21.452339
74.505205	2528.060329	21.457357
74.049714	2533.985517	21.462375
74.221582	2522.440426	21.467392
74.544498	2518.965814	21.472410
74.282702	2527.895930	21.477427
74.400549	2529.095733	21.482445
74.480731	2539.915157	21.487463
74.473587	2532.734229	21.492480
74.703067	2526.250621	21.497498
74.295716	2538.533013	21.502515
74.450323	2541.356691	21.507533
74.606924	2559.951133	21.512551
74.758567	2557.395172	21.517568
75.041141	2555.812766	21.522586
74.618960	2559.672897	21.527603
75.136493	2556.532483	21.532621
75.019010	2570.362457	21.537639
75.140964	2578.078383	21.542656
75.935138	2573.924231	21.547674
75.914574	2565.421055	21.552691
76.410509	2554.568961	21.557709
76.727270	2540.044147	21.562727
76.444486	2533.000372	21.567744
76.462508	2519.535108	21.572762
76.114096	2523.715266	21.577779
75.984145	2527.772894	21.582797
76.828202	2527.021618	21.587815
76.482459	2522.698257	21.592832
76.556918	2510.344529	21.597850
76.384378	2518.423161	21.602867
76.518315	2501.297173	21.607885
76.585370	2503.663725	21.612903
76.317760	2508.979705	21.617920
76.822847	2515.788586	21.622938
76.496811	2514.725459	21.627955
76.782338	2513.451240	21.632973
76.741658	2523.008014	21.637991
77.045486	2513.430443	21.643008
76.701322	2515.948414	21.648026
76.487150	2525.643084	21.653043
76.394451	2519.434292	21.658061
76.689571	2530.374685	21.663079
76.487600	2546.423883	21.668096
76.722649	2550.931504	21.673114
76.816918	2564.929439	21.678131
77.242180	2574.221791	21.683149
76.874900	2590.427252	21.688167
77.178941	2585.304513	21.693184
77.440078	2581.177924	21.698202
77.275535	2603.889741	21.703219
77.425262	2608.698973	21.708237
77.352757	2614.247141	21.713255
77.704935	2611.030256	21.718272
77.901202	2630.672567	21.723290
78.291372	2636.132429	21.728307
78.239229	2641.083101	21.733325
78.967830	2629.299333	21.738343
78.569087	2631.389367	21.743360
79.121580	2632.304333	21.748378
78.793041	2623.880657	21.753395
78.888911	2604.564724	21.758413
78.960414	2598.918792	21.763431
78.971600	2597.404716	21.768448
79.359797	2603.311370	21.773466
79.100892	2601.161049	21.778483
79.208110	2594.905615	21.783501
79.214255	2587.652372	21.788519
78.915825	2594.755073	21.793536
79.440943	2603.072539	21.798554
79.414898	2612.428896	21.803571
79.275754	2610.348045	21.808589
79.192344	2618.086704	21.813607
79.080529	2616.317859	21.818624
79.517870	2610.500881	21.823642
79.604119	2636.334587	21.828659
79.988728	2644.175798	21.833677
79.907562	2648.833251	21.838695
79.763731	2653.216462	21.843712
79.844875	2638.378730	21.848730
79.765855	2649.974724	21.853747
79.806217	2651.068905	21.858765
80.251770	2670.392658	21.863783
80.344011	2678.230112	21.868800
80.838566	2675.538791	21.873818
81.109689	2670.302592	21.878835
81.737638	2649.896944	21.883853
81.896323	2634.451814	21.888871
81.401082	2619.683514	21.893888
81.991124	2609.260643	21.898906
81.747925	2599.551089	21.903923
81.409916	2592.410161	21.908941
81.317995	2588.841087	21.913959
81.338946	2583.996115	21.918976
81.844322	2571.601038	21.923994
81.179388	2584.647565	21.929011
81.290770	2579.408416	21.934029
81.551469	2584.234633	21.939047
81.666811	2596.243972	21.944064
81.816411	2608.259045	21.949082
81.478193	2610.033884	21.954099
81.628197	2602.646484	21.959117
81.876256	2611.976185	21.964135
81.132410	2605.733838	21.969152
81.677982	2620.013919	21.974170
81.658494	2646.503433	21.979187
81.808326	2652.115454	21.984205
81.499694	2642.821491	21.989223
81.376116	2670.974089	21.994240
82.277322	2677.942417	21.999258
82.249266	2681.426824	22.004275
82.185247	2684.625069	22.009293
82.574695	2701.384834	22.014311
82.533665	2718.159072	22.019328
82.838257	2703.299104	22.024346
83.051398	2709.169141	22.029363
82.853553	2706.533437	22.034381
82.863948	2708.766517	22.039399
82.610454	2719.429307	22.044416
83.151186	2724.808270	22.049434
83.166493	2730.107227	22.054451
83.450546	2730.445522	22.059469
83.378378	2724.333241	22.064487
83.176628	2736.213489	22.069504
83.300585	2742.814539	22.074522
83.811658	2759.695106	22.079539
83.635479	2759.900431	22.084557
84.013836	2764.490209	22.089575
84.073989	2764.262535	22.094592
84.231210	2748.809661	22.099610
84.302560	2760.915025	22.104627
84.299447	2761.639254	22.109645
84.558040	2775.716767	22.114663
84.515648	2783.723509	22.119680
84.814858	2773.521316	22.124698
84.605553	2779.966734	22.129715
84.659265	2774.848134	22.134733
84.880400	2775.296499	22.139751
84.799371	2780.061061	22.144768
84.983954	2769.012126	22.149786
84.890947	2776.002024	22.154803
84.553568	2795.604881	22.159821
84.927311	2796.997622	22.164839
84.963501	2803.140031	22.169856
85.263624	2797.288700	22.174874
85.244360	2814.203920	22.179891
85.217592	2825.927194	22.184909
85.795815	2821.649413	22.189927
85.599860	2829.521454	22.194944
85.899556	2828.777169	22.199962
86.475437	2824.865939	22.204979
86.765484	2815.812551	22.209997
86.779323	2803.910029	22.215015
86.463792	2814.289870	22.220032
86.718958	2802.670881	22.225050
86.665694	2818.552329	22.230067
86.650012	2816.664328	22.235085
86.721246	2810.794337	22.240103
86.790909	2810.808796	22.245120
86.923110	2804.605428	22.250138
87.070430	2808.298525	22.255155
86.959369	2815.251676	22.260173
87.097657	2807.469647	22.265191
86.880476	2809.282664	22.270208
86.980068	2806.307730	22.275226
87.009322	2812.768242	22.280243
87.069976	2825.477437	22.285261
87.268648	2838.628299	22.290279
87.312893	2846.580514	22.295296
87.203521	2843.012707	22.300314
87.203983	2848.510246	22.305331
87.105927	2853.912343	22.310349
87.370035	2872.379443	22.315367
87.489358	2867.216836	22.320384
87.784660	2869.950259	22.325402
87.682860	2882.297106	22.330419
88.021690	2894.879019	22.335437
88.214523	2889.169115	22.340455
88.069614	2893.582495	22.345472
87.961583	2892.441374	22.350490
88.529321	2904.700588	22.355507
88.593452	2910.230483	22.360525
89.163062	2898.319387	22.365543
89.180905	2906.147273	22.370560
89.158538	2905.468715	22.375578
89.478221	2903.432049	22.380595
89.235937	2901.554925	22.385613
89.834376	2886.412862	22.390631
89.561663	2883.503726	22.395648
89.848739	2869.087090	22.400666
89.935791	2860.591459	22.405683
89.586468	2859.421934	22.410701
89.851380	2863.298663	22.415719
89.503263	2860.301664	22.420736
89.848102	2858.369884	22.425754
89.837206	2868.974739	22.430771
89.730446	2888.835860	22.435789
90.084787	2889.706212	22.440807
89.650545	2894.265321	22.445824
90.052319	2888.875045	22.450842
90.601555	2886.501393	22.455859
90.340028	2890.846353	22.460877
90.401108	2898.453257	22.465895
90.148596	2913.980883	22.470912
90.485780	2921.100938	22.475930
90.614074	2911.903894	22.480947
90.471359	2925.730108	22.485965
91.194298	2926.426992	22.490983
90.992844	2938.799895	22.496000
91.167407	2947.083677	22.501018
91.231679	2946.032821	22.506035
91.210937	2948.943595	22.511053
91.474250	2940.915904	22.516071
91.353929	2944.378694	22.521088
91.582173	2941.394952	22.526106
91.544889	2958.540503	22.531123
91.180552	2964.508187	22.536141
91.645700	2973.616187	22.541159
91.613106	2968.369338	22.546176
92.074621	2981.710905	22.551194
92.353911	2990.881696	22.556211
92.370870	3007.374148	22.561229
92.317908	3002.093269	22.566247
92.422835	2999.958020	22.571264
92.554090	3002.520293	22.576282
93.014198	2992.836136	22.581299
93.001033	2999.234873	22.586317
92.987728	2993.107978	22.591335
92.854613	2995.569688	22.596352
92.882963	2991.936828	22.601370
92.918642	2994.399228	22.606387
92.815334	3012.211761	22.611405
93.270922	3016.383634	22.616423
93.093694	3019.755497	22.621440
93.599752	3018.483960	22.626458
93.394800	3020.227641	22.631475
93.289442	3027.770136	22.636493
93.686103	3037.783320	22.641511
93.727580	3050.569120	22.646528
93.967890	3051.604113	22.651546
94.232960	3046.016015	22.656563
93.986415	3048.672581	22.661581
94.227320	3042.118352	22.666599
94.220576	3052.483649	22.671616
94.208375	3043.408702	22.676634
94.592090	3052.975591	22.681651
94.428220	3062.221649	22.686669
94.575208	3067.701607	22.691687
94.936551	3069.443705	22.696704
94.833414	3078.078455	22.701722
95.073304	3068.923013	22.706739
94.708813	3072.563821	22.711757
95.437181	3071.432907	22.716775
95.257679	3073.151496	22.721792
95.202660	3067.801245	22.726810
95.379669	3079.710151	22.731827
95.246189	3097.373848	22.736845
95.310080	3097.220356	22.741863
95.502588	3102.527395	22.746880
95.471698	3104.569347	22.751898
95.636007	3102.597851	22.756915
95.529457	3123.410093	22.761933
95.926079	3132.854010	22.766951
95.741145	3127.832834	22.771968
95.862069	3130.444880	22.776986
96.314240	3142.037217	22.782003
96.298979	3151.611413	22.787021
96.692074	3142.832860	22.792039
96.823822	3150.068666	22.797056
96.737690	3152.364705	22.802074
97.043405	3143.166781	22.807091
97.147074	3138.483495	22.812109
97.200132	3138.501502	22.817127
97.318140	3137.253106	22.822144
97.524259	3156.975554	22.827162
97.838794	3156.393369	22.832179
97.753045	3160.337113	22.837197
98.098871	3148.655160	22.842215
97.616763	3146.400901	22.847232
97.784284	3151.669192	22.852250
97.986491	3153.113313	22.857267
97.788570	3171.587077	22.862285
98.022193	3163.651615	22.867303
98.393857	3171.425951	22.872320
97.922072	3165.313762	22.877338
98.326005	3163.689080	22.882355
98.213293	3170.265467	22.887373
98.800464	3179.888786	22.892391
98.508208	3182.360830	22.897408
98.667023	3189.992975	22.902426
98.878274	3192.067930	22.907443
98.787287	3200.762938	22.912461
99.430495	3190.142646	22.917479
99.451381	3187.946530	22.922496
99.438584	3189.329527	22.927514
99.601527	3180.196651	22.932531
99.257736	3187.175258	22.937549
99.560273	3200.955279	22.942567
99.826004	3211.579754	22.947584
99.633975	3222.714993	22.952602
99.942860	3210.953299	22.957619
99.889855	3205.734174	22.962637
100.075743	3213.115748	22.967655
100.146875	3205.499026	22.972672
100.116960	3210.203251	22.977690
100.350390	3211.801256	22.982707
100.139400	3232.555010	22.987725
100.405470	3238.525911	22.992743
100.349792	3226.209387	22.997760
100.633052	3235.756861	23.002778
100.753394	3226.197537	23.007795
100.622376	3238.531803	23.012813
101.302390	3252.736973	23.017831
101.483721	3261.930505	23.022848
101.717636	3259.930098	23.027866
101.770970	3253.162445	23.032883
101.870798	3260.672134	23.037901
101.542674	3240.720699	23.042919
101.768892	3234.458225	23.047936
101.828035	3248.828392	23.052954
101.802349	3241.073792	23.057971
101.874504	3244.646798	23.062989
102.096325	3243.453982	23.068007
101.821267	3243.748979	23.073024
101.889253	3257.142011	23.078042
102.026959	3255.356429	23.083059
102.245900	3268.401521	23.088077
102.512759	3269.360065	23.093095
102.433814	3270.317805	23.098112
102.470387	3281.938368	23.103130
102.469131	3280.167215	23.108147
102.811924	3300.166369	23.113165
103.011821	3304.801718	23.118183
103.145038	3302.812529	23.123200
102.885858	3310.259453	23.128218
103.044095	3311.129349	23.133235
103.293054	3322.648892	23.138253
103.514555	3323.217697	23.143271
103.676802	3316.737455	23.148288
103.409605	3322.316261	23.153306
103.660231	3339.592745	23.158323
104.178536	3352.301123	23.163341
103.908357	3361.760319	23.168359
104.323158	3346.556987	23.173376
104.153532	3366.423256	23.178394
104.524442	3349.241994	23.183411
104.401692	3361.784845	23.188429
104.446266	3364.469467	23.193447
104.933999	3369.673592	23.198464
105.158566	3384.710944	23.203482
105.498092	3374.315817	23.208499
105.466254	3380.339432	23.213517
105.755396	3366.974455	23.218535
106.160244	3360.805878	23.223552
105.843204	3354.307233	23.228570
106.180522	3337.703666	23.233587
105.796583	3338.604607	23.238605
105.576077	3328.856569	23.243623
105.724243	3331.292846	23.248640
105.827956	3350.119879	23.253658
105.931269	3361.271887	23.258675
105.897577	3355.771524	23.263693
105.940999	3361.475509	23.268711
106.298812	3360.004549	23.273728
106.210812	3378.182312	23.278746
106.404754	3395.031230	23.283763
106.405317	3389.866531	23.288781
106.845403	3390.828974	23.293799
106.739953	3391.490705	23.298816
106.856555	3405.441980	23.303834
107.129987	3407.282594	23.308851
107.331009	3422.644004	23.313869
107.150335	3420.384887	23.318887
107.520423	3407.007211	23.323904
107.380156	3413.280770	23.328922
107.252526	3410.918342	23.333939
107.434666	3429.088280	23.338957
107.280768	3441.363904	23.343975
107.900081	3443.425414	23.348992
107.862947	3450.147641	23.354010
107.866403	3444.421366	23.359027
107.924277	3455.940872	23.364045
108.012074	3474.677777	23.369063
108.240886	3474.053523	23.374080
108.355397	3485.441972	23.379098
108.336610	3472.646635	23.384115
108.656841	3490.220411	23.389133
108.717296	3501.971040	23.394151
109.238714	3496.927641	23.399168
109.595047	3500.894468	23.404186
109.297314	3506.539443	23.409203
109.564196	3506.525853	23.414221
109.030074	3504.992459	23.419239
109.313119	3495.777229	23.424256
109.473090	3511.229415	23.429274
109.399692	3524.480802	23.434291
109.842317	3527.659594	23.439309
109.952785	3527.337318	23.444327
110.114861	3524.312491	23.449344
110.310570	3519.698055	23.454362
110.215337	3529.721646	23.459379
110.459997	3541.719279	23.464397
110.610009	3555.062317	23.469415
110.603553	3540.783226	23.474432
110.709714	3553.358667	23.479450
110.479913	3550.358011	23.484467
110.977991	3551.382488	23.489485
110.960499	3569.432601	23.494503
111.136465	3567.978851	23.499520
111.319791	3575.440559	23.504538
111.243939	3575.526846	23.509555
111.379712	3569.992337	23.514573
111.426447	3591.064797	23.519591
111.751238	3588.680309	23.524608
111.963439	3602.401283	23.529626
112.489801	3590.520084	23.534643
112.630754	3585.101651	23.539661
112.938015	3587.621383	23.544679
113.108153	3578.116962	23.549696
112.969058	3579.423729	23.554714
113.191556	3580.730252	23.559731
113.099053	3580.562586	23.564749
112.778362	3579.574483	23.569767
113.136917	3575.090072	23.574784
113.159731	3578.894606	23.579802
113.478723	3574.790038	23.584819
113.646420	3570.259778	23.589837
113.433022	3577.437382	23.594855
113.534266	3571.983423	23.599872
113.932305	3574.249853	23.604890
113.762699	3572.091640	23.609907
113.757753	3571.770826	23.614925
113.624574	3577.808209	23.619943
113.640575	3579.831011	23.624960
113.611327	3596.263647	23.629978
113.640999	3591.905942	23.634995
114.047160	3614.357043	23.640013
113.693869	3630.589209	23.645031
113.913848	3632.211544	23.650048
114.099372	3647.177283	23.655066
114.208955	3662.215112	23.660083
114.645496	3661.573261	23.665101
114.687125	3689.109228	23.670119
115.298608	3688.105195	23.675136
115.203106	3685.472789	23.680154
115.547238	3688.514422	23.685171
115.775387	3674.576184	23.690189
115.502964	3682.628702	23.695207
115.933234	3700.092685	23.700224
116.374539	3711.031670	23.705242
116.478452	3697.395192	23.710259
116.620869	3689.126552	23.715277
116.543976	3676.771461	23.720295
116.627025	3672.449750	23.725312
116.572736	3667.893749	23.730330
116.235075	3671.265244	23.735347
116.805206	3677.818532	23.740365
116.619581	3686.866976	23.745383
116.775830	3696.821318	23.750400
116.824739	3696.445877	23.755418
116.691670	3698.808858	23.760435
117.001607	3712.256570	23.765453
116.914051	3724.020939	23.770471
117.349473	3721.580248	23.775488
117.647305	3721.198875	23.780506
117.649248	3726.365731	23.785523
118.026894	3735.973820	23.790541
118.087084	3748.449960	23.795559
118.130500	3755.760183	23.800576
118.310043	3744.119598	23.805594
118.080584	3750.458120	23.810611
118.396175	3746.106406	23.815629
118.087495	3757.483876	23.820647
118.374753	3770.576705	23.825664
118.649366	3782.125006	23.830682
118.225795	3782.188756	23.835699
118.736177	3794.230231	23.840717
118.951964	3799.028462	23.845735
119.311953	3796.532570	23.850752
119.439741	3803.424809	23.855770
119.275048	3814.201158	23.860787
119.857793	3816.309748	23.865805
119.743622	3839.730036	23.870823
119.860504	3838.299467	23.875840
119.926793	3841.854291	23.880858
119.819557	3839.795138	23.885875
120.462953	3847.486070	23.890893
120.261895	3859.207190	23.895911
120.562093	3857.796949	23.900928
120.807085	3858.804053	23.905946
120.403865	3863.383481	23.910963
120.846914	3856.407871	23.915981
120.732465	3864.638979	23.920999
120.838749	3877.993498	23.926016
120.878529	3891.770943	23.931034
120.848586	3896.195028	23.936051
121.565817	3901.600202	23.941069
121.445875	3912.738126	23.946087
121.569604	3917.182748	23.951104
121.709784	3908.486751	23.956122
121.891130	3921.832771	23.961139
122.341823	3910.609658	23.966157
122.597158	3916.972813	23.971175
122.641223	3929.355307	23.976192
123.208519	3918.575469	23.981210
122.454381	3916.177298	23.986227
122.769239	3928.237983	23.991245
122.898219	3933.327096	23.996263
122.793265	3935.452339	24.001280
123.020397	3934.537366	24.006298
123.372707	3938.591207	24.011315
123.109994	3929.683377	24.016333
123.017838	3941.406149	24.021351
123.266596	3947.542426	24.026368
123.728290	3959.474390	24.031386
123.337363	3966.122939	24.036403
123.833572	3959.208145	24.041421
123.893948	3973.954412	24.046439
123.980691	3992.391681	24.051456
124.040581	3994.176504	24.056474
124.383909	3996.553284	24.061491
124.300034	3987.444025	24.066509
124.502520	3997.434976	24.071527
124.501179	4014.585161	24.076544
125.102816	4004.664240	24.081562
124.912748	4005.141212	24.086579
125.054323	4001.024674	24.091597
124.981249	4011.865470	24.096615
124.928274	4014.869999	24.101632
125.030218	4035.123932	24.106650
125.484982	4039.725022	24.111667
125.700934	4039.507271	24.116685
125.060081	4047.978337	24.121703
125.535797	4060.015936	24.126720
126.193927	4061.981308	24.131738
125.838241	4080.210276	24.136755
126.408035	4083.184562	24.141773
126.340495	4086.593943	24.146791
126.607497	4090.580493	24.151808
127.121402	4077.255524	24.156826
127.231983	4084.743348	24.161843
127.206241	4078.978380	24.166861
127.117493	4086.169363	24.171879
127.362368	4104.251699	24.176896
127.973181	4103.379663	24.181914
127.904433	4109.573888	24.186931
128.014482	4102.897245	24.191949
128.211590	4108.938613	24.196967
127.612494	4108.279457	24.201984
128.019583	4102.301587	24.207002
127.832818	4107.324313	24.212019
128.585454	4122.845567	24.217037
128.711310	4130.127302	24.222055
128.668308	4134.583944	24.227072
128.710215	4124.118082	24.232090
129.074411	4122.923986	24.237107
129.140336	4122.575632	24.242125
129.390054	4131.095228	24.247143
129.278817	4127.441990	24.252160
129.339466	4122.345816	24.257178
129.013244	4144.663449	24.262195
129.551149	4156.148586	24.267213
129.621824	4147.967622	24.272231
129.453775	4159.353512	24.277248
130.111113	4170.507350	24.282266
129.992283	4181.863027	24.287283
130.298949	4175.138716	24.292301
130.379179	4171.593826	24.297319
130.366794	4181.587920	24.302336
130.692622	4195.527181	24.307354
130.754720	4204.163442	24.312371
130.797294	4208.296390	24.317389
131.474907	4201.799441	24.322407
131.182893	4206.048630	24.327424
131.298834	4197.137573	24.332442
131.174830	4216.649255	24.337459
131.726593	4215.113307	24.342477
132.438111	4219.051614	24.347495
132.111133	4215.428300	24.352512
132.200643	4213.752604	24.357530
132.455060	4214.203361	24.362547
132.836080	4211.105792	24.367565
132.793178	4205.216052	24.372583
132.347597	4210.539734	24.377600
132.469951	4207.522953	24.382618
132.392293	4211.605005	24.387635
132.549582	4215.228269	24.392653
132.599961	4224.738663	24.397671
132.618517	4236.910648	24.402688
133.134663	4236.783974	24.407706
133.214340	4253.829212	24.412723
133.134973	4273.561928	24.417741
133.652948	4275.762857	24.422759
133.539639	4278.112796	24.427776
133.761364	4281.270968	24.432794
133.993322	4294.410047	24.437811
133.893452	4303.157150	24.442829
134.237061	4294.308218	24.447847
134.356797	4302.586476	24.452864
134.491526	4309.810907	24.457882
134.660265	4327.308425	24.462899
134.579929	4326.528004	24.467917
134.995364	4327.362305	24.472935
135.198226	4327.245955	24.477952
135.548662	4336.728603	24.482970
135.722954	4340.398685	24.487987
136.039307	4346.091143	24.493005
136.030213	4339.629505	24.498023
136.094185	4352.757173	24.503040
136.430616	4336.950067	24.508058
136.439269	4345.332649	24.513075
136.239374	4342.838758	24.518093
136.516003	4329.714450	24.523111
136.313490	4338.833015	24.528128
136.844954	4335.583630	24.533146
136.450153	4356.339885	24.538163
136.580948	4368.572072	24.543181
136.727056	4366.522330	24.548199
136.465379	4380.542852	24.553216
137.017128	4384.789687	24.558234
137.003046	4393.210724	24.563251
136.873302	4412.176272	24.568269
137.712311	4415.082260	24.573287
137.453015	4429.315849	24.578304
137.874243	4430.622498	24.583322
137.856979	4446.413774	24.588339
137.821318	4456.630057	24.593357
138.123290	4458.951962	24.598375
138.243257	4486.954737	24.603392
138.491704	4472.891533	24.608410
138.864047	4478.819658	24.613427
139.211175	4493.325818	24.618445
139.809283	4493.610002	24.623463
139.558145	4495.796233	24.628480
139.839501	4492.085149	24.633498
140.137701	4492.162437	24.638515
140.079088	4492.233656	24.643533
140.268590	4489.430896	24.648551
140.165590	4485.392284	24.653568
140.691486	4482.633639	24.658586
140.490418	4487.325344	24.663603
140.382048	4492.060711	24.668621
140.840323	4479.299071	24.673639
140.988689	4479.570578	24.678656
140.985561	4474.581361	24.683674
141.051613	4494.436668	24.688691
140.762848	4508.710665	24.693709
141.306289	4505.177320	24.698727
141.112476	4509.389007	24.703744
141.221648	4515.203374	24.708762
141.479044	4527.409134	24.713779
141.748614	4534.550621	24.718797
142.022426	4531.444032	24.723815
141.801935	4541.349296	24.728832
141.661723	4550.682864	24.733850
141.939452	4562.348175	24.738867
142.185323	4576.407381	24.743885
142.101603	4563.225420	24.748903
142.226267	4602.595679	24.753920
142.133208	4597.192160	24.758938
143.007884	4616.825829	24.763955
142.835857	4641.227959	24.768973
143.335042	4629.891931	24.773991
143.508120	4631.271336	24.779008
143.491927	4633.652442	24.784026
143.872822	4654.358149	24.789043
144.161764	4658.917285	24.794061
144.062846	4659.521278	24.799079
143.992463	4656.078093	24.804096
143.881207	4665.820375	24.809114
144.441301	4678.168111	24.814131
144.331622	4686.794988	24.819149
144.712921	4688.730452	24.824167
145.039041	4697.492824	24.829184
145.188228	4715.004262	24.834202
145.385793	4709.870576	24.839219
145.527474	4716.452194	24.844237
145.579160	4711.564048	24.849255
145.159947	4718.301878	24.854272
145.971607	4730.213292	24.859290
145.894357	4732.076905	24.864307
146.080613	4736.750783	24.869325
146.542279	4737.353765	24.874343
146.267971	4742.134108	24.879360
146.744306	4753.008941	24.884378
146.824442	4764.911213	24.889395
146.900296	4770.557164	24.894413
146.954290	4758.668140	24.899431
146.802347	4774.299416	24.904448
147.114054	4779.417899	24.909466
147.210853	4793.472146	24.914483
147.108316	4802.743687	24.919501
147.488685	4801.320437	24.924519
147.737664	4811.321902	24.929536
147.543570	4813.717634	24.934554
148.291301	4821.194829	24.939571
148.201575	4838.136546	24.944589
148.668972	4836.755534	24.949607
148.554052	4840.573813	24.954624
148.895110	4835.635179	24.959642
149.069509	4854.776745	24.964659
149.378572	4865.820425	24.969677
149.278237	4862.195523	24.974695
149.780736	4864.344771	24.979712
149.540557	4865.833825	24.984730
150.203572	4851.302892	24.989747
149.681224	4858.175264	24.994765
150.309162	4870.667026	24.999783
150.220309	4878.956626	25.004800
150.420029	4876.938863	25.009818
150.986080	4873.285912	25.014835
150.693259	4885.714120	25.019853
150.591898	4871.855175	25.024871
150.993217	4882.350365	25.029888
151.148319	4899.827950	25.034906
151.410182	4906.244766	25.039923
151.566740	4911.322921	25.044941
151.974956	4895.122153	25.049959
151.496154	4904.824066	25.054976
151.377061	4904.131174	25.059994
151.921576	4909.855230	25.065011
151.755930	4926.489125	25.070029
152.185979	4939.337510	25.075047
152.121343	4936.738352	25.080064
152.031617	4939.339637	25.085082
152.669842	4946.773663	25.090099
152.444632	4964.763424	25.095117
152.479299	4959.857553	25.100135
152.889120	4971.496494	25.105152
153.125625	4982.249106	25.110170
153.597777	4984.836570	25.115187
153.333587	4988.925407	25.120205
153.713927	5002.541308	25.125223
153.804957	5010.367929	25.130240
154.304353	5002.266883	25.135258
154.686837	5009.452041	25.140275
154.028314	5002.787753	25.145293
154.699180	5022.588113	25.150311
154.982077	5026.457674	25.155328
154.918986	5032.667861	25.160346
155.370166	5020.840221	25.165363
155.267144	5027.652434	25.170381
155.366910	5025.748919	25.175399
155.807599	5027.269754	25.180416
155.766794	5021.378571	25.185434
156.059964	5031.350782	25.190451
156.228034	5053.084706	25.195469
156.524738	5051.649349	25.200487
156.162254	5052.364885	25.205504
156.511996	5058.824653	25.210522
156.305492	5043.685919	25.215539
156.479255	5066.352172	25.220557
156.638070	5080.123875	25.225575
156.462880	5086.677974	25.230592
156.449347	5092.675183	25.235610
157.039781	5110.415374	25.240627
157.113626	5126.122099	25.245645
157.240728	5147.480994	25.250663
157.766984	5143.621954	25.255680
157.510140	5158.873324	25.260698
158.004440	5160.101741	25.265715
158.399893	5183.654348	25.270733
158.494371	5173.516129	25.275751
158.679135	5186.845727	25.280768
158.691167	5203.174740	25.285786
158.992319	5201.379501	25.290803
158.718521	5201.532159	25.295821
159.005877	5214.587199	25.300839
159.344578	5218.349090	25.305856
159.217848	5232.404646	25.310874
159.810173	5237.099404	25.315891
159.982476	5251.469930	25.320909
159.923920	5253.355700	25.325927
160.234503	5259.258947	25.330944
160.256513	5256.008194	25.335962
160.709412	5269.636686	25.340979
160.216335	5290.415223	25.345997
160.671683	5285.995369	25.351015
161.042474	5304.548035	25.356032
160.875687	5314.294433	25.361050
160.892193	5316.196089	25.366067
161.303291	5329.438580	25.371085
161.589376	5347.930555	25.376103
162.082704	5338.541877	25.381120
162.077609	5339.080687	25.386138
162.040648	5339.472003	25.391155
162.307833	5349.959870	25.396173
162.902553	5362.513465	25.401191
162.710922	5348.405263	25.406208
163.143502	5348.860317	25.411226
163.636653	5336.243408	25.416243
163.694502	5341.460967	25.421261
163.536883	5342.410245	25.426279
163.447609	5339.219710	25.431296
163.926102	5340.208984	25.436314
164.395586	5329.360964	25.441331
164.232858	5339.325647	25.446349
164.441327	5332.680171	25.451367
164.523158	5329.602180	25.456384
164.114270	5346.432876	25.461402
164.765561	5351.664447	25.466419
164.699664	5368.175909	25.471437
164.640329	5369.327803	25.476455
165.234206	5363.735049	25.481472
164.769557	5393.357394	25.486490
165.014407	5388.625171	25.491507
165.176152	5403.387440	25.496525
165.525060	5411.777842	25.501543
165.789432	5412.518388	25.506560
165.720170	5424.567273	25.511578
165.855160	5438.447209	25.516595
166.203774	5450.471565	25.521613
166.289561	5453.827409	25.526631
166.592010	5459.646238	25.531648
166.797838	5468.477864	25.536666
166.930416	5470.081448	25.541683
166.892461	5486.314312	25.546701
167.035300	5500.092976	25.551719
167.620040	5493.062786	25.556736
167.467608	5517.055836	25.561754
167.230373	5525.833530	25.566771
167.766728	5543.046068	25.571789
168.065980	5557.218572	25.576807
168.529710	5564.346381	25.581824
168.976336	5564.891256	25.586842
168.831279	5557.634199	25.591859
169.251992	5567.171288	25.596877
169.060969	5595.782964	25.601895
169.330191	5589.183204	25.606912
169.109627	5600.739134	25.611930
169.574495	5615.707197	25.616947
169.795106	5625.405162	25.621965
169.946929	5621.752359	25.626983
170.052669	5619.732005	25.632000
170.337061	5639.220902	25.637018
170.431781	5632.549310	25.642035
170.895508	5628.539879	25.647053
171.438767	5637.858964	25.652071
171.649399	5626.993898	25.657088
171.343610	5628.426979	25.662106
171.593914	5631.377481	25.667123
171.984272	5634.023542	25.672141
171.845027	5649.819755	25.677159
171.993762	5650.847309	25.682176
172.257173	5661.662861	25.687194
172.509644	5654.002613	25.692212
172.453788	5647.649019	25.697229
172.449665	5662.009070	25.702247
172.862378	5665.200371	25.707264
172.658370	5683.210267	25.712282
172.953630	5681.458485	25.717300
173.137785	5692.549496	25.722317
173.295883	5702.973818	25.727335
173.779215	5709.421108	25.732352
173.544877	5716.664199	25.737370
173.933101	5730.516490	25.742388
173.818086	5740.507363	25.747405
173.990272	5748.066473	25.752423
174.314255	5737.850376	25.757440
174.743813	5755.676314	25.762458
174.824371	5764.411571	25.767476
174.974783	5760.991311	25.772493
174.693951	5779.408666	25.777511
174.736239	5778.576291	25.782528
175.071222	5801.404260	25.787546
174.927660	5802.389034	25.792564
175.389437	5833.217647	25.797581
175.497876	5842.409059	25.802599
175.779942	5849.504179	25.807616
176.040273	5868.818573	25.812634
175.854697	5870.686143	25.817652
176.495207	5878.940917	25.822669
176.420335	5895.022816	25.827687
176.527121	5902.896095	25.832704
177.013853	5919.183984	25.837722
176.665492	5927.747237	25.842740
177.406406	5939.383075	25.847757
177.345290	5964.894305	25.852775
177.727735	5960.430462	25.857792
177.924401	5979.023099	25.862810
178.123493	5983.425070	25.867828
178.539036	5981.075167	25.872845
178.529096	6008.710797	25.877863
179.159433	6010.408149	25.882880
179.075366	6006.324254	25.887898
179.155312	6015.035336	25.892916
179.388677	6020.087698	25.897933
179.041290	6050.748754	25.902951
179.986587	6038.566526	25.907968
180.211514	6061.504522	25.912986
180.376619	6068.331699	25.918004
180.672497	6065.665360	25.923021
180.498387	6069.908839	25.928039
180.865207	6070.329953	25.933056
180.974628	6070.072388	25.938074
181.176855	6076.739817	25.943092
181.664687	6085.646221	25.948109
181.430569	6089.033306	25.953127
181.697715	6078.279833	25.958144
181.520433	6097.206474	25.963162
181.321256	6112.023869	25.968180
181.778194	6115.478065	25.973197
181.759218	6137.684842	25.978215
182.399429	6150.570974	25.983232
182.017891	6164.455469	25.988250
181.873959	6177.780667	25.993268
182.536379	6183.148506	25.998285
182.595948	6205.528203	26.003303
182.828043	6223.665513	26.008320
183.322455	6235.674908	26.013338
183.660648	6246.976210	26.018356
184.387300	6254.775804	26.023373
184.259703	6257.689193	26.028391
184.460294	6262.698248	26.033408
185.191903	6257.575350	26.038426
185.376031	6255.664759	26.043444
185.176130	6253.407633	26.048461
185.086938	6265.369893	26.053479
185.258313	6275.452136	26.058496
185.629920	6280.108279	26.063514
185.521672	6285.570346	26.068532
186.022660	6284.122204	26.073549
185.833908	6300.025744	26.078567
186.102459	6312.009719	26.083584
186.108851	6321.593275	26.088602
186.099342	6332.323107	26.093620
186.602055	6337.188255	26.098637
186.677238	6354.395615	26.103655
186.668036	6351.595619	26.108672
187.222843	6366.124137	26.113690
186.905069	6369.420428	26.118708
187.259979	6376.754147	26.123725
187.397092	6397.005670	26.128743
187.597633	6404.646236	26.133760
188.272085	6406.477288	26.138778
188.267108	6430.418077	26.143796
188.624505	6426.660044	26.148813
188.711746	6434.521871	26.153831
188.994075	6430.736141	26.158848
189.383458	6434.921527	26.163866
189.894342	6451.959716	26.168884
189.969679	6438.024349	26.173901
189.911863	6443.552915	26.178919
190.167417	6431.900871	26.183936
190.048027	6451.371229	26.188954
190.201657	6457.118280	26.193972
190.547481	6457.196339	26.198989
190.537000	6474.180200	26.204007
191.020711	6485.548860	26.209024
191.135449	6498.915622	26.214042
191.458441	6503.316842	26.219060
191.617667	6496.761765	26.224077
191.741782	6499.109597	26.229095
192.197684	6507.363877	26.234112
192.206041	6515.245940	26.239130
192.196780	6512.853131	26.244148
192.206375	6512.485339	26.249165
192.127105	6533.947353	26.254183
192.268253	6543.311743	26.259200
192.940000	6553.730039	26.264218
192.959205	6571.626665	26.269236
193.109755	6576.944224	26.274253
193.385761	6593.586033	26.279271
193.511437	6613.327772	26.284288
194.058854	6619.011024	26.289306
194.118909	6637.793328	26.294324
194.782985	6630.528135	26.299341
194.959994	6635.593999	26.304359
194.815651	6632.318622	26.309376
194.815920	6637.476866	26.314394
195.230347	6663.331589	26.319412
195.525928	6662.429511	26.324429
195.032706	6669.253708	26.329447
195.221630	6676.663195	26.334464
195.527797	6699.876108	26.339482
195.816284	6714.824119	26.344500
195.804230	6731.004335	26.349517
195.780685	6745.473353	26.354535
196.381319	6758.494160	26.359552
196.465010	6770.148460	26.364570
196.425795	6793.062885	26.369588
197.329666	6800.772658	26.374605
197.622460	6809.836332	26.379623
197.747817	6817.639244	26.384640
198.020523	6819.533166	26.389658
197.729000	6843.257544	26.394676
198.269215	6834.058687	26.399693
198.637574	6843.361871	26.404711
198.895827	6865.564560	26.409728
198.955077	6856.568483	26.414746
199.036327	6873.199628	26.419764
199.430567	6868.786347	26.424781
199.483084	6870.949220	26.429799
199.705864	6889.854438	26.434816
200.319706	6887.665218	26.439834
200.010186	6894.352653	26.444852
200.393178	6888.819622	26.449869
200.687856	6891.849632	26.454887
200.541090	6908.809345	26.459904
200.611268	6916.084297	26.464922
200.744642	6928.633894	26.469940
200.959253	6936.971027	26.474957
201.056958	6947.793731	26.479975
201.024741	6961.378278	26.484992
201.704621	6975.146183	26.490010
201.410104	6993.199384	26.495028
201.570807	7002.905002	26.500045
201.853341	7011.590847	26.505063
202.106611	7041.031596	26.510080
202.123291	7046.502308	26.515098
202.826454	7069.299289	26.520116
203.208559	7072.451860	26.525133
203.326017	7083.941673	26.530151
203.323970	7098.664218	26.535168
203.929467	7104.678267	26.540186
204.044575	7124.509828	26.545204
204.307187	7127.372715	26.550221
204.759407	7135.205751	26.555239
204.631194	7144.765698	26.560256
204.582823	7144.899813	26.565274
204.835122	7161.477633	26.570292
204.946980	7182.091956	26.575309
205.544579	7197.531762	26.580327
205.698094	7203.794238	26.585344
205.991862	7214.590847	26.590362
205.959339	7235.014197	26.595380
206.448570	7237.450341	26.600397
206.583875	7252.499930	26.605415
206.612393	7250.871071	26.610432
206.626753	7255.713682	26.615450
207.137656	7279.179349	26.620468
207.359801	7276.434481	26.625485
207.947576	7289.242044	26.630503
207.873733	7297.691886	26.635520
208.551802	7290.981744	26.640538
208.616170	7301.008381	26.645556
208.471631	7300.559846	26.650573
209.110077	7314.686235	26.655591
209.360745	7335.020912	26.660608
209.198625	7331.250534	26.665626
208.982136	7334.959472	26.670644
209.275715	7357.527187	26.675661
209.706860	7358.747382	26.680679
209.801260	7373.310012	26.685696
210.246909	7380.284909	26.690714
210.277942	7396.199498	26.695732
210.284519	7401.999685	26.700749
210.682439	7415.955822	26.705767
210.587218	7427.791567	26.710784
211.449115	7438.341907	26.715802
211.221164	7457.182489	26.720820
211.251642	7455.134239	26.725837
211.505303	7477.632352	26.730855
211.293016	7491.543439	26.735872
211.766685	7504.196848	26.740890
211.725864	7526.354847	26.745908
212.232094	7540.671184	26.750925
213.064007	7550.449139	26.755943
213.131555	7562.354824	26.760960
213.141404	7572.757751	26.765978
213.525153	7571.544020	26.770996
213.675837	7572.543810	26.776013
214.265516	7586.965263	26.781031
214.205786	7595.062399	26.786048
214.540652	7592.698104	26.791066
214.693824	7593.754983	26.796084
215.053479	7590.486246	26.801101
215.213260	7602.565680	26.806119
215.248879	7619.183133	26.811136
215.547192	7625.352400	26.816154
215.527003	7624.535036	26.821172
215.729884	7640.157440	26.826189
216.001733	7646.264947	26.831207
215.684577	7669.578126	26.836224
216.139545	7676.799729	26.841242
216.325543	7689.000115	26.846260
216.479846	7718.943783	26.851277
217.042235	7724.051513	26.856295
216.831768	7740.932111	26.861312
217.040799	7753.294134	26.866330
217.265143	7773.055580	26.871348
217.369356	7781.681681	26.876365
217.836336	7796.210359	26.881383
218.016015	7811.931311	26.886400
218.226906	7829.128748	26.891418
218.657376	7837.781015	26.896436
218.765564	7863.653922	26.901453
219.187731	7876.602909	26.906471
219.274321	7888.347346	26.911488
219.683940	7898.955030	26.916506
220.567750	7886.895058	26.921524
221.317027	7884.567415	26.926541
221.870157	7877.591069	26.931559
221.571608	7885.763480	26.936576
221.708951	7861.089678	26.941594
221.939708	7868.593598	26.946612
221.774393	7867.415152	26.951629
221.690898	7867.210884	26.956647
221.665754	7890.474289	26.961664
222.129593	7888.106640	26.966682
222.470057	7903.101489	26.971700
222.024476	7922.405714	26.976717
222.628871	7923.499495	26.981735
222.580054	7952.988979	26.986752
222.843997	7951.329596	26.991770
222.944836	7970.492674	26.996788
223.013816	7992.346353	27.001805
223.261176	7998.603003	27.006823
223.406449	8026.303003	27.011840
223.630284	8048.760407	27.016858
223.787468	8064.468804	27.021876
223.981821	8085.061138	27.026893
224.301813	8103.350627	27.031911
224.682475	8116.732858	27.036928
225.057506	8147.893904	27.041946
225.689940	8150.827867	27.046964
225.716628	8159.307148	27.051981
226.203839	8176.049438	27.056999
226.233621	8178.885037	27.062016
226.593825	8197.453893	27.067034
226.763193	8206.501067	27.072052
226.975406	8208.962915	27.077069
227.238154	8230.163217	27.082087
227.742180	8223.985748	27.087104
228.351069	8213.839676	27.092122
228.882572	8217.993264	27.097140
228.768590	8227.957956	27.102157
228.823123	8217.516436	27.107175
228.933514	8218.069238	27.112192
229.051190	8216.827202	27.117210
229.344326	8225.778989	27.122228
229.540132	8233.022642	27.127245
229.607156	8243.182556	27.132263
229.627338	8239.207585	27.137280
229.896828	8251.155851	27.142298
230.057661	8268.677170	27.147316
230.278774	8281.248705	27.152333
230.694051	8278.544049	27.157351
230.983494	8284.488973	27.162368
231.010881	8298.605131	27.167386
231.477668	8303.284664	27.172404
231.437333	8317.688581	27.177421
231.888546	8325.565703	27.182439
231.714038	8335.750053	27.187456
231.879964	8343.008174	27.192474
232.319119	8351.307956	27.197492
232.403030	8369.353397	27.202509
232.694028	8372.308687	27.207527
233.077931	8385.911169	27.212544
233.295779	8403.435766	27.217562
233.463986	8408.195662	27.222580
233.188866	8435.345495	27.227597
233.690096	8448.413364	27.232615
233.870404	8461.616490	27.237632
233.724031	8478.576230	27.242650
234.284871	8504.289105	27.247668
234.789453	8520.252171	27.252685
234.931736	8539.749347	27.257703
235.083617	8550.760287	27.262720
235.226040	8577.377010	27.267738
235.763881	8585.029543	27.272756
235.957545	8611.150990	27.277773
236.063438	8619.482654	27.282791
236.716661	8630.508815	27.287808
236.777997	8650.248019	27.292826
237.204915	8659.577205	27.297844
237.324276	8671.091481	27.302861
237.576375	8684.865002	27.307879
237.979193	8700.109410	27.312896
238.078257	8701.893773	27.317914
238.425170	8719.602085	27.322932
238.266906	8722.059400	27.327949
238.623907	8740.102424	27.332967
239.157160	8759.185937	27.337984
238.842992	8767.388174	27.343002
239.195946	8785.507544	27.348020
239.454251	8808.371494	27.353037
239.944125	8822.417573	27.358055
239.483485	8839.284178	27.363072
239.815494	8854.394765	27.368090
240.413258	8874.242841	27.373108
240.502397	8885.011569	27.378125
240.727473	8907.220260	27.383143
241.223314	8920.838474	27.388160
241.355437	8947.450435	27.393178
242.073736	8947.892806	27.398196
242.547833	8967.685135	27.403213
242.947526	8971.106945	27.408231
243.244810	8977.318663	27.413248
243.117610	8989.443681	27.418266
243.279885	9002.251647	27.423284
243.307874	9005.895926	27.428301
243.702107	9023.968534	27.433319
243.594572	9028.931982	27.438336
243.778687	9042.440605	27.443354
244.196360	9057.196840	27.448372
244.509195	9074.277852	27.453389
244.523650	9084.402133	27.458407
244.671929	9100.884245	27.463424
245.100127	9122.649852	27.468442
245.239060	9124.604097	27.473460
245.208546	9148.669803	27.478477
245.381956	9159.273463	27.483495
245.887706	9182.764857	27.488512
245.605524	9201.777205	27.493530
246.731950	9216.348080	27.498548
246.833330	9230.252674	27.503565
246.772665	9267.486348	27.508583
247.183481	9270.328942	27.513600
247.167368	9292.020502	27.518618
247.909495	9304.536212	27.523636
248.262279	9331.871559	27.528653
248.002846	9326.609869	27.533671
248.756680	9353.272822	27.538688
248.638125	9356.438932	27.543706
249.592304	9369.335405	27.548724
249.957576	9362.772494	27.553741
250.462289	9363.947546	27.558759
250.520384	9360.552101	27.563776
250.690146	9386.574011	27.568794
251.362231	9382.182424	27.573812
251.534021	9385.368835	27.578829
251.514378	9382.441633	27.583847
251.557060	9384.548188	27.588864
251.653568	9410.940747	27.593882
252.228599	9403.132946	27.598900
252.384057	9421.182655	27.603917
252.196359	9432.510589	27.608935
252.596090	9443.243844	27.613952
252.740444	9459.308669	27.618970
252.880436	9473.376432	27.623988
252.934775	9483.961490	27.629005
253.287665	9508.283871	27.634023
253.707619	9519.621982	27.639040
253.586915	9550.267845	27.644058
253.969699	9566.279771	27.649076
254.148729	9573.483493	27.654093
254.576833	9595.749214	27.659111
254.712342	9606.727364	27.664128
255.020593	9637.161109	27.669146
255.612989	9640.681033	27.674164
255.753882	9666.138626	27.679181
256.060115	9671.897727	27.684199
256.544102	9687.607780	27.689216
256.634686	9705.128165	27.694234
256.846619	9709.028797	27.699252
257.213970	9734.089640	27.704269
257.456693	9738.842280	27.709287
257.696428	9754.181754	27.714304
258.037546	9769.257032	27.719322
258.214494	9785.998209	27.724340
258.309995	9799.578129	27.729357
258.447806	9811.855108	27.734375
259.114377	9812.997002	27.739392
259.228208	9835.467317	27.744410
259.493290	9848.750464	27.749428
259.697532	9866.541262	27.754445
259.762365	9878.129278	27.759463
260.184314	9890.296085	27.764480
259.553655	9914.733653	27.769498
259.827146	9927.390743	27.774516
260.442618	9958.461015	27.779533
260.770858	9982.855963	27.784551
261.491960	9991.294893	27.789568
261.924796	10003.871211	27.794586
262.282169	10001.026213	27.799604
262.464751	10022.629812	27.804621
262.840893	10027.694401	27.809639
263.368503	10028.032206	27.814656
263.999438	10030.591785	27.819674
264.996912	10017.561262	27.824692
265.261483	10010.908467	27.829709
265.164262	9994.485575	27.834727
265.208101	9988.467406	27.839744
265.190240	9988.258506	27.844762
265.512067	9985.401297	27.849780
265.822669	9982.972942	27.854797
265.569450	9994.717088	27.859815
265.490416	9995.054845	27.864832
265.596114	10025.073145	27.869850
266.027638	10034.869544	27.874868
266.191678	10050.777282	27.879885
266.482092	10070.012218	27.884903
267.033929	10082.759476	27.889920
267.013918	10103.023697	27.894938
266.823567	10119.304719	27.899956
267.312484	10127.593226	27.904973
267.595461	10158.417399	27.909991
267.536644	10166.700029	27.915008
267.332811	10203.086762	27.920026
267.612745	10225.132180	27.925044
268.234170	10253.922890	27.930061
268.256709	10290.700782	27.935079
268.666113	10311.705371	27.940096
268.505534	10338.669219	27.945114
269.214245	10359.877033	27.950132
269.573338	10391.754140	27.955149
269.751161	10417.710206	27.960167
270.334688	10440.486999	27.965184
270.912219	10465.975731	27.970202
271.265070	10485.954741	27.975220
271.524103	10499.505718	27.980237
271.980653	10527.523879	27.985255
272.118383	10524.320581	27.990272
272.568513	10553.141864	27.995290
272.796807	10572.139555	28.000308
273.227322	10586.364073	28.005325
273.084564	10605.770098	28.010343
273.678364	10606.303335	28.015360
273.735135	10639.043417	28.020378
274.096898	10648.397990	28.025396
274.269945	10658.006092	28.030413
274.474249	10685.616584	28.035431
274.944403	10701.645067	28.040448
275.296383	10718.812719	28.045466
275.200106	10733.470751	28.050484
275.246625	10749.222229	28.055501
275.950755	10774.227955	28.060519
276.844968	10771.729308	28.065536
277.464308	10778.226207	28.070554
277.798190	10770.532665	28.075572
278.033394	10778.752579	28.080589
278.311773	10778.950610	28.085607
278.596969	10769.776925	28.090624
278.533784	10797.106672	28.095642
278.586753	10798.304897	28.100660
278.881372	10808.334083	28.105677
279.296605	10822.780370	28.110695
279.596080	10830.873819	28.115712
279.795744	10839.699218	28.120730
279.915892	10849.754265	28.125748
280.093912	10857.256539	28.130765
280.153823	10873.763033	28.135783
280.608578	10883.176351	28.140800
280.579429	10897.516907	28.145818
280.827374	10907.802869	28.150836
281.241955	10930.896781	28.155853
281.079190	10952.547189	28.160871
281.526995	10968.986184	28.165888
281.707244	10993.839784	28.170906
281.925188	11007.814791	28.175924
282.424240	11036.209674	28.180941
282.372246	11055.509768	28.185959
282.907270	11076.913627	28.190976
283.301657	11089.480642	28.195994
284.151225	11099.206664	28.201012
284.301586	11105.895853	28.206029
284.673624	11128.415678	28.211047
285.290482	11137.761246	28.216064
285.374731	11151.514353	28.221082
285.323381	11144.009908	28.226100
285.686139	11177.405381	28.231117
285.730869	11182.481280	28.236135
286.268837	11204.225175	28.241152
286.481863	11217.050902	28.246170
286.370461	11238.036080	28.251188
286.830709	11252.862905	28.256205
287.175105	11272.313276	28.261223
287.497630	11290.465749	28.266240
287.603626	11299.012300	28.271258
288.065377	11334.208471	28.276276
288.609892	11337.115109	28.281293
288.490485	11355.878405	28.286311
288.916514	11376.325388	28.291328
289.042420	11401.581005	28.296346
289.178230	11422.991771	28.301364
289.735322	11443.517913	28.306381
289.738458	11466.337437	28.311399
290.273002	11483.403877	28.316416
290.556115	11501.013198	28.321434
290.776396	11533.468717	28.326452
291.156949	11547.254872	28.331469
291.277561	11570.012480	28.336487
291.711561	11596.889096	28.341504
292.111005	11614.581638	28.346522
292.534891	11637.972838	28.351540
293.201030	11646.675482	28.356557
293.378350	11669.291444	28.361575
293.673291	11676.322428	28.366592
293.608505	11690.127542	28.371610
293.850655	11717.196961	28.376628
294.298769	11731.627572	28.381645
294.827796	11752.612594	28.386663
294.717973	11760.037048	28.391680
295.227004	11777.199434	28.396698
295.260234	11790.455736	28.401716
295.863412	11799.543961	28.406733
296.170604	11828.837220	28.411751
296.183618	11841.472911	28.416768
296.580030	11861.225780	28.421786
297.117328	11883.084161	28.426804
297.829242	11899.628353	28.431821
297.925319	11907.908989	28.436839
297.945232	11925.398618	28.441856
298.258617	11950.417515	28.446874
298.289997	11963.288194	28.451892
298.909230	11983.146016	28.456909
298.942092	11993.452647	28.461927
298.986041	12021.401709	28.466944
299.563444	12031.296432	28.471962
299.719440	12055.301607	28.476980
299.623368	12062.931921	28.481997
300.194022	12092.623114	28.487015
299.954989	12114.364957	28.492032
300.352511	12143.293948	28.497050
300.654705	12164.547260	28.502068
301.183403	12186.380690	28.507085
301.547479	12219.749732	28.512103
301.711230	12241.892848	28.517120
302.436921	12258.004920	28.522138
302.692963	12294.022118	28.527156
303.050754	12297.057658	28.532173
303.260997	12311.583462	28.537191
303.786680	12331.939460	28.542208
304.622496	12340.978312	28.547226
304.395240	12364.321157	28.552244
305.243082	12368.535966	28.557261
305.407465	12393.555089	28.562279
305.604992	12402.797720	28.567296
305.888959	12411.501241	28.572314
306.303011	12431.351155	28.577332
306.734481	12435.017426	28.582349
306.951022	12457.547603	28.587367
307.392676	12469.704427	28.592384
307.895719	12478.779733	28.597402
307.852563	12499.668532	28.602420
308.081358	12500.765185	28.607437
308.024126	12520.337362	28.612455
308.098840	12534.526588	28.617472
308.498069	12558.985342	28.622490
308.526744	12585.845844	28.627508
309.222292	12606.534839	28.632525
309.584314	12621.358757	28.637543
310.251773	12651.766093	28.642560
310.727089	12648.013838	28.647578
310.634979	12680.886002	28.652596
311.383630	12682.361183	28.657613
311.767240	12710.406285	28.662631
311.873422	12718.696688	28.667648
312.279841	12729.724934	28.672666
312.365134	12740.324320	28.677684
312.597858	12768.006924	28.682701
312.945225	12784.317901	28.687719
312.854618	12811.083553	28.692736
313.345910	12823.638974	28.697754
313.477364	12845.304484	28.702772
314.051021	12856.807740	28.707789
314.146639	12874.408732	28.712807
314.509607	12908.863586	28.717824
315.103151	12929.149178	28.722842
315.354158	12944.444115	28.727860
315.990274	12971.987559	28.732877
315.820481	12984.783732	28.737895
316.348850	13016.122577	28.742912
316.743189	13025.378568	28.747930
316.988382	13044.065905	28.752948
317.383890	13066.541981	28.757965
317.478838	13088.989225	28.762983
317.844304	13109.465798	28.768000
318.242258	13130.154475	28.773018
318.723495	13144.572967	28.778036
319.412336	13157.631640	28.783053
319.740384	13159.224022	28.788071
319.983920	13178.195453	28.793088
320.203609	13183.227153	28.798106
320.624966	13205.461164	28.803124
320.697485	13226.174086	28.808141
321.273120	13222.918786	28.813159
321.233788	13243.111346	28.818176
321.725975	13249.085900	28.823194
321.470978	13270.095980	28.828212
321.894384	13285.721910	28.833229
322.426350	13305.261759	28.838247
322.368197	13330.848806	28.843264
322.530035	13336.788445	28.848282
322.502999	13357.965638	28.853300
322.803965	13385.929504	28.858317
323.471909	13406.118233	28.863335
324.109959	13443.377816	28.868352
324.494004	13459.968625	28.873370
324.646548	13485.892834	28.878388
324.888527	13498.146641	28.883405
325.397332	13519.305942	28.888423
325.510613	13548.268899	28.893440
325.847329	13568.002248	28.898458
326.121627	13594.758994	28.903476
326.567243	13618.852321	28.908493
326.879777	13641.899290	28.913511
326.760802	13672.885187	28.918528
327.489014	13693.641065	28.923546
327.497076	13716.975117	28.928564
327.795811	13749.609571	28.933581
328.698283	13775.532581	28.938599
329.058182	13810.065499	28.943616
329.845351	13823.636328	28.948634
329.955626	13851.579088	28.953652
330.340182	13865.502090	28.958669
330.660330	13884.677526	28.963687
330.795432	13903.231267	28.968704
331.457043	13916.161119	28.973722
331.344594	13950.493854	28.978740
331.523005	13970.726787	28.983757
332.339739	13995.019056	28.988775
332.412437	14020.572836	28.993792
332.634714	14035.265237	28.998810
333.130822	14060.230235	29.003828
333.391181	14085.641045	29.008845
333.585119	14103.085189	29.013863
334.013656	14120.075888	29.018880
334.661454	14132.265908	29.023898
335.133976	14156.774779	29.028916
335.527716	14173.545945	29.033933
335.997113	14191.152456	29.038951
336.255836	14204.058059	29.043968
336.277469	14216.082666	29.048986
336.892833	14242.979241	29.054004
337.203010	14263.089782	29.059021
337.735534	14277.874279	29.064039
337.904845	14295.800255	29.069056
338.965309	14295.974013	29.074074
339.381554	14313.748665	29.079092
339.774201	14310.662247	29.084109
340.592498	14296.286978	29.089127
341.026735	14307.858559	29.094144
341.118194	14294.787632	29.099162
341.268696	14297.676748	29.104180
341.807094	14295.767051	29.109197
341.943522	14299.886229	29.114215
341.671448	14314.348953	29.119232
341.814321	14317.474168	29.124250
342.423380	14320.783560	29.129268
342.177707	14350.425373	29.134285
342.500950	14358.089541	29.139303
342.376180	14387.635686	29.144320
342.667530	14404.709363	29.149338
343.189523	14424.313681	29.154356
343.314475	14446.141577	29.159373
343.731475	14470.124290	29.164391
344.060196	14502.507830	29.169408
344.425428	14514.661549	29.174426
344.702928	14539.646263	29.179444
344.650681	14569.833171	29.184461
345.055313	14590.870903	29.189479
344.926540	14630.148698	29.194496
345.601935	14656.411865	29.199514
345.595015	14683.152493	29.204532
345.797322	14717.444002	29.209549
346.555827	14754.951351	29.214567
347.018090	14795.535633	29.219584
347.692339	14822.592021	29.224602
347.879092	14850.311012	29.229620
348.361143	14882.452331	29.234637
348.696189	14909.413909	29.239655
348.922594	14936.866405	29.244672
349.449018	14971.638895	29.249690
349.759172	15003.623030	29.254708
349.825910	15034.394669	29.259725
350.441981	15069.232855	29.264743
350.835467	15095.857203	29.269760
351.239732	15131.192503	29.274778
351.567805	15160.434698	29.279796
351.978846	15187.897920	29.284813
352.467237	15200.085278	29.289831
353.214445	15236.415101	29.294848
353.575770	15261.059157	29.299866
354.332706	15259.369957	29.304884
354.518648	15287.532709	29.309901
355.010242	15297.590272	29.314919
355.107491	15325.201995	29.319936
355.251002	15338.702918	29.324954
355.732240	15360.148161	29.329972
356.130887	15388.382928	29.334989
356.187637	15404.625021	29.340007
356.651730	15428.604467	29.345024
357.092547	15455.793673	29.350042
357.574762	15477.201080	29.355060
357.719581	15503.558476	29.360077
358.056524	15518.586216	29.365095
358.485381	15557.680598	29.370112
359.017486	15560.605845	29.375130
359.657039	15585.918163	29.380148
359.718437	15613.782205	29.385165
360.050791	15635.290369	29.390183
360.432198	15662.228145	29.395200
360.606771	15674.770610	29.400218
361.054556	15700.351385	29.405236
360.822243	15735.391813	29.410253
361.368318	15757.996318	29.415271
361.292880	15790.616611	29.420288
362.205589	15842.785988	29.425306
362.220806	15859.434200	29.430324
362.484137	15904.500654	29.435341
363.197824	15926.294187	29.440359
363.428324	15956.825985	29.445376
363.876653	15982.711312	29.450394
364.340022	16011.650410	29.455412
365.066841	16033.178680	29.460429
366.246298	16036.445692	29.465447
366.730377	16054.433210	29.470464
367.074616	16065.133592	29.475482
367.399595	16064.501195	29.480500
367.603484	16090.540784	29.485517
368.236106	16093.547156	29.490535
368.326144	16094.771140	29.495552
368.399137	16113.687615	29.500570
368.930882	16121.195033	29.505588
368.777278	16139.531309	29.510605
369.122118	16148.849319	29.515623
369.546095	16169.384631	29.520640
369.537501	16200.736820	29.525658
369.778662	16221.989792	29.530676
369.942104	16247.585553	29.535693
370.710683	16271.279218	29.540711
370.865603	16297.186985	29.545728
371.178282	16327.005978	29.550746
371.754269	16345.337925	29.555764
371.974353	16392.468289	29.560781
372.198489	16413.202606	29.565799
372.267039	16439.492204	29.570816
372.604470	16468.181913	29.575834
373.312508	16503.069337	29.580852
373.254668	16540.763664	29.585869
373.914407	16577.211862	29.590887
374.121552	16611.571139	29.595904
374.555790	16636.359616	29.600922
375.106000	16677.654277	29.605940
375.278069	16709.330499	29.610957
375.586843	16745.876777	29.615975
376.272776	16781.575506	29.620992
376.550216	16822.053625	29.626010
376.925313	16857.017594	29.631028
377.424121	16883.685662	29.636045
378.033639	16922.713864	29.641063
378.218844	16960.493298	29.646080
378.601079	17002.674171	29.651098
378.908175	17021.037350	29.656116
378.868610	17069.168000	29.661133
379.335889	17094.642090	29.666151
379.810456	17146.724442	29.671168
379.995373	17191.164302	29.676186
380.805975	17221.293118	29.681204
381.177294	17260.084255	29.686221
382.437864	17279.099558	29.691239
383.951257	17267.139398	29.696256
384.857779	17274.482632	29.701274
385.086877	17272.092775	29.706292
385.375589	17274.935817	29.711309
385.979471	17275.808138	29.716327
386.120237	17267.189198	29.721344
386.315625	17289.236149	29.726362
386.670150	17300.369112	29.731380
386.559887	17317.304455	29.736397
386.901441	17322.246257	29.741415
387.062332	17345.035150	29.746432
387.008576	17362.500253	29.751450
387.343931	17374.761941	29.756468
387.830307	17403.245679	29.761485
388.270985	17421.524062	29.766503
388.864580	17443.103109	29.771520
388.937186	17479.371819	29.776538
389.409851	17486.520820	29.781556
389.705918	17516.998896	29.786573
389.805805	17544.000696	29.791591
390.221526	17565.322556	29.796608
390.261867	17601.981520	29.801626
390.540037	17626.874648	29.806644
391.102015	17662.070949	29.811661
391.497023	17691.648580	29.816679
391.879682	17723.985354	29.821696
392.075908	17762.322812	29.826714
392.514185	17797.658175	29.831732
392.566019	17837.325016	29.836749
392.786618	17869.047412	29.841767
393.430672	17898.593502	29.846784
393.803211	17939.570872	29.851802
394.802553	17959.995498	29.856820
395.086304	17995.908682	29.861837
395.252764	18016.813801	29.866855
396.082323	18056.624691	29.871872
396.201730	18091.230184	29.876890
396.342335	18101.056140	29.881908
396.699772	18137.006256	29.886925
397.270555	18172.775983	29.891943
397.364417	18194.078025	29.896960
398.101559	18236.885662	29.901978
398.699346	18255.677998	29.906996
399.336824	18283.737744	29.912013
399.593415	18308.963371	29.917031
400.234606	18339.699332	29.922048
400.744881	18364.739452	29.927066
401.173292	18383.949441	29.932084
401.551611	18407.261725	29.937101
401.664387	18444.104410	29.942119
402.239953	18476.642338	29.947136
402.079111	18499.199347	29.952154
402.668903	18528.054063	29.957172
403.330261	18560.800181	29.962189
403.687182	18584.633337	29.967207
404.564182	18614.056880	29.972224
404.227344	18647.837593	29.977242
404.756901	18674.315841	29.982260
405.056569	18708.476492	29.987277
405.333092	18740.533348	29.992295
406.160317	18774.387378	29.997312
406.322318	18811.322013	30.002330
407.085379	18837.418067	30.007348
407.942531	18865.990914	30.012365
408.771720	18875.830643	30.017383
409.365129	18886.638078	30.022400
409.610313	18905.239063	30.027418
409.918287	18912.471217	30.032436
410.323752	18940.157577	30.037453
410.677752	18964.452091	30.042471
411.130788	18979.419556	30.047488
411.321329	19009.178531	30.052506
411.281874	19024.270407	30.057524
411.529779	19060.773560	30.062541
411.962465	19089.344780	30.067559
412.325239	19112.477762	30.072576
412.800201	19162.360866	30.077594
413.060991	19186.843023	30.082612
412.927856	19211.603475	30.087629
413.717692	19246.642316	30.092647
414.118702	19273.436097	30.097664
414.518004	19314.467581	30.102682
415.159491	19350.907568	30.107700
415.481924	19386.030646	30.112717
415.615000	19418.300235	30.117735
416.365363	19457.320459	30.122752
416.257101	19496.248495	30.127770
416.883423	19530.307697	30.132788
417.626608	19566.650860	30.137805
417.816124	19603.879063	30.142823
418.395797	19638.261539	30.147840
418.729302	19666.352036	30.152858
419.470035	19701.636469	30.157876
419.568592	19728.293610	30.162893
419.733178	19768.991556	30.167911
420.475715	19797.722200	30.172928
420.964014	19841.317847	30.177946
421.181613	19867.756791	30.182964
421.662702	19896.270901	30.187981
421.682551	19937.031132	30.192999
422.723732	19961.821505	30.198016
422.855955	20006.403745	30.203034
423.391939	20027.864865	30.208052
423.515119	20055.992528	30.213069
424.147910	20090.666660	30.218087
424.760769	20106.078410	30.223104
425.247962	20154.401629	30.228122
425.744565	20174.748531	30.233140
426.427714	20205.101008	30.238157
426.278061	20227.746771	30.243175
427.231497	20257.234622	30.248192
427.770338	20291.623647	30.253210
427.968688	20312.614632	30.258228
428.200134	20340.587625	30.263245
428.611416	20365.437504	30.268263
428.919476	20398.444564	30.273280
429.399912	20431.016294	30.278298
429.858833	20461.721801	30.283316
429.966153	20492.186210	30.288333
430.050031	20535.988003	30.293351
430.658736	20569.057400	30.298368
431.542461	20616.920356	30.303386
432.019672	20646.093838	30.308404
432.921755	20685.780713	30.313421
433.439177	20717.545927	30.318439
433.996131	20722.129762	30.323456
434.482627	20755.755883	30.328474
435.057495	20780.437309	30.333492
435.833411	20799.073646	30.338509
436.244849	20819.728733	30.343527
436.398729	20835.666736	30.348544
436.643013	20859.845056	30.353562
437.477709	20873.212022	30.358580
437.846277	20889.570069	30.363597
438.173047	20926.330637	30.368615
438.755008	20936.773950	30.373632
438.653064	20966.271224	30.378650
438.990036	20989.333830	30.383668
439.573466	21016.385475	30.388685
440.154114	21056.752553	30.393703
440.623344	21069.970684	30.398720
441.032337	21105.519720	30.403738
441.299860	21133.916895	30.408756
441.783057	21168.266505	30.413773
441.749832	21195.455550	30.418791
442.398453	21223.649252	30.423808
442.712785	21251.504355	30.428826
442.960306	21289.625367	30.433844
443.466314	21330.434357	30.438861
443.579105	21373.211828	30.443879
443.816846	21404.290054	30.448896
444.742129	21443.077726	30.453914
444.951752	21477.184869	30.458932
445.793540	21513.064939	30.463949
446.193180	21550.677224	30.468967
446.725968	21582.047342	30.473984
447.548638	21621.054288	30.479002
447.852484	21651.407737	30.484020
448.223005	21675.375477	30.489037
448.760116	21713.930246	30.494055
449.084025	21740.379704	30.499072
449.548247	21774.631214	30.504090
449.481338	21813.915652	30.509108
450.163886	21852.035053	30.514125
450.307287	21890.575206	30.519143
450.982849	21917.102132	30.524160
451.645571	21941.862122	30.529178
452.239762	21971.832075	30.534196
452.580436	21994.597436	30.539213
452.800442	22037.087576	30.544231
453.499331	22049.990825	30.549248
453.980892	22086.239416	30.554266
454.091621	22127.525944	30.559284
454.652247	22154.583206	30.564301
454.722616	22199.247741	30.569319
455.703273	22229.403092	30.574336
455.645417	22264.063969	30.579354
455.856087	22315.760010	30.584372
456.416053	22347.016660	30.589389
456.535193	22400.461047	30.594407
457.458883	22434.911942	30.599424
457.943616	22474.513099	30.604442
458.229378	22522.401948	30.609460
459.014829	22554.851436	30.614477
459.433552	22597.436120	30.619495
460.259839	22620.052286	30.624512
461.213848	22653.287601	30.629530
461.316181	22693.897296	30.634548
462.312874	22718.809520	30.639565
462.223780	22763.133048	30.644583
462.847432	22790.980310	30.649600
462.882412	22831.815969	30.654618
463.091236	22874.354216	30.659636
463.598059	22909.559662	30.664653
464.128813	22946.973514	30.669671
464.592624	22986.385391	30.674688
465.427116	23033.796639	30.679706
465.520800	23085.123393	30.684724
466.322813	23101.949302	30.689741
466.562019	23155.920138	30.694759
467.297835	23184.151516	30.699776
467.530889	23229.570709	30.704794
468.059864	23270.498828	30.709812
468.959132	23303.269874	30.714829
469.078172	23353.848942	30.719847
469.206998	23394.869051	30.724864
470.027935	23434.446569	30.729882
470.167339	23469.335748	30.734900
470.895720	23508.059944	30.739917
471.273453	23560.927308	30.744935
472.090682	23592.570865	30.749952
472.785829	23627.711830	30.754970
472.696615	23678.116720	30.759988
473.315413	23706.997590	30.765005
473.648518	23752.791056	30.770023
474.108503	23793.414932	30.775040
474.737354	23838.355279	30.780058
475.047336	23874.497417	30.785076
475.277179	23919.532633	30.790093
476.116464	23957.216005	30.795111
476.254457	24004.149558	30.800128
477.314026	24039.763853	30.805146
477.737499	24088.796442	30.810164
478.084170	24127.938682	30.815181
478.587167	24172.047683	30.820199
479.047918	24213.129747	30.825216
479.404501	24250.665279	30.830234
479.836895	24302.311601	30.835252
480.175473	24344.625382	30.840269
480.316032	24384.165144	30.845287
481.235796	24424.297838	30.850304
481.709101	24469.992669	30.855322
482.369235	24494.878249	30.860340
483.646519	24516.740789	30.865357
484.432929	24536.114394	30.870375
485.355645	24554.888206	30.875392
485.560405	24569.472943	30.880410
485.794374	24592.000880	30.885428
486.456017	24599.460607	30.890445
486.813208	24616.786113	30.895463
486.962885	24659.920547	30.900480
487.762038	24669.429643	30.905498
487.982324	24705.670441	30.910516
488.739136	24716.924454	30.915533
488.886583	24753.704170	30.920551
488.970213	24778.786842	30.925568
489.773378	24804.579555	30.930586
490.315184	24842.782666	30.935604
490.755858	24856.230863	30.940621
490.980133	24891.222394	30.945639
491.664657	24908.582146	30.950656
492.013027	24940.408587	30.955674
492.430486	24980.736408	30.960692
492.939808	25023.474542	30.965709
493.171387	25051.236073	30.970727
493.627799	25098.957151	30.975744
494.030420	25138.146030	30.980762
494.164611	25193.582159	30.985780
494.667209	25232.947050	30.990797
495.317707	25283.847284	30.995815
495.294985	25340.451736	31.000832
495.881553	25385.414215	31.005850
496.088734	25446.636329	31.010868
496.717797	25496.979317	31.015885
497.004576	25547.272058	31.020903
497.929244	25601.830684	31.025920
498.775940	25651.453525	31.030938
499.327213	25698.987035	31.035956
499.982412	25745.030406	31.040973
500.378239	25788.473754	31.045991
500.705034	25845.356163	31.051008
501.653059	25888.663896	31.056026
501.805593	25934.040551	31.061044
502.375206	25991.797843	31.066061
502.942733	26027.974298	31.071079
502.817867	26082.891704	31.076096
503.701219	26123.472874	31.081114
503.979542	26183.247446	31.086132
504.751448	26229.058240	31.091149
505.361956	26280.747175	31.096167
506.270770	26312.145568	31.101184
508.437007	26320.621050	31.106202
509.703504	26336.308450	31.111220
510.647073	26342.223832	31.116237
511.128693	26355.022930	31.121255
511.163928	26350.796667	31.126272
511.647858	26352.274575	31.131290
511.826524	26371.164499	31.136308
512.133010	26384.298674	31.141325
512.423370	26400.952599	31.146343
512.764108	26430.045121	31.151360
513.025886	26448.817235	31.156378
513.129429	26476.160725	31.161396
513.397918	26505.041416	31.166413
513.823698	26550.730755	31.171431
513.810322	26597.168180	31.176448
514.324437	26630.834447	31.181466
514.424695	26689.659343	31.186484
514.747609	26731.555767	31.191501
515.328838	26776.734113	31.196519
514.935052	26830.219148	31.201536
515.671502	26882.254881	31.206554
516.258315	26940.053501	31.211572
516.815513	26999.778277	31.216589
517.090712	27052.509393	31.221607
517.647169	27119.909448	31.226624
518.504001	27166.150252	31.231642
518.858728	27220.688793	31.236660
519.409780	27279.043361	31.241677
520.110418	27336.357538	31.246695
520.422913	27392.780554	31.251712
520.801524	27450.094961	31.256730
521.355533	27517.392870	31.261748
521.418164	27575.760152	31.266765
522.347870	27642.062410	31.271783
522.482008	27699.698996	31.276800
523.192690	27775.984447	31.281818
523.977743	27845.128532	31.286836
524.299830	27904.116288	31.291853
525.244186	27962.139696	31.296871
525.911732	28031.632117	31.301888
527.036105	28076.695260	31.306906
527.687178	28135.073951	31.311924
528.126930	28181.689577	31.316941
528.724390	28232.052096	31.321959
529.472153	28276.626240	31.326976
530.090726	28322.789823	31.331994
530.757915	28369.863465	31.337012
531.215383	28410.246281	31.342029
531.763808	28441.673701	31.347047
532.831271	28481.374918	31.352064
533.666624	28507.275105	31.357082
534.287430	28536.826250	31.362100
535.013811	28569.927890	31.367117
535.467538	28599.551056	31.372135
535.669730	28626.430426	31.377152
536.438810	28662.228747	31.382170
537.029214	28700.974942	31.387188
537.423608	28727.254697	31.392205
537.833440	28757.768749	31.397223
538.494342	28796.374105	31.402240
539.312165	28816.463460	31.407258
539.786656	28841.789970	31.412276
540.254433	28884.159674	31.417293
540.988273	28909.033092	31.422311
540.898500	28954.341162	31.427328
541.163423	28987.741067	31.432346
541.680112	29026.746303	31.437364
542.109735	29066.892349	31.442381
542.680232	29118.268292	31.447399
542.788123	29168.440355	31.452416
543.022141	29217.692490	31.457434
543.534250	29274.823531	31.462452
543.798547	29336.964798	31.467469
544.232792	29390.556788	31.472487
544.775159	29462.369287	31.477504
545.423857	29519.989535	31.482522
545.923939	29578.748329	31.487540
546.282026	29636.439305	31.492557
547.062827	29694.479876	31.497575
547.388603	29756.577717	31.502592
548.632323	29817.299223	31.507610
549.096129	29860.776181	31.512628
549.962781	29914.755435	31.517645
550.707519	29961.192658	31.522663
551.061633	30011.187426	31.527680
551.761791	30062.897967	31.532698
552.519733	30109.623650	31.537716
552.635790	30157.654951	31.542733
553.802426	30205.562399	31.547751
553.705130	30240.703309	31.552768
553.910252	30282.501635	31.557786
554.727772	30337.345360	31.562804
554.729200	30383.077367	31.567821
555.503699	30436.357338	31.572839
555.710106	30500.168738	31.577856
556.246420	30550.554406	31.582874
556.974162	30614.484725	31.587892
557.013392	30671.610503	31.592909
558.316925	30733.009906	31.597927
558.320819	30799.919624	31.602944
559.061573	30849.420319	31.607962
559.692140	30916.876367	31.612980
560.106175	30968.898967	31.617997
561.147372	31022.016530	31.623015
561.867234	31082.270951	31.628032
562.386517	31139.968492	31.633050
562.836166	31191.544111	31.638068
563.501287	31263.362519	31.643085
564.343403	31309.124547	31.648103
564.793134	31368.408831	31.653120
565.133625	31413.702268	31.658138
565.795600	31476.889387	31.663156
566.150310	31533.542765	31.668173
566.853292	31591.299622	31.673191
567.319753	31655.431715	31.678208
567.803046	31723.609464	31.683226
568.921086	31781.115011	31.688244
569.102312	31841.265844	31.693261
569.673158	31898.815313	31.698279
570.202006	31955.318068	31.703296
570.503997	32016.481231	31.708314
571.307101	32077.807505	31.713332
571.694025	32141.569616	31.718349
572.279234	32208.675267	31.723367
572.952912	32265.356903	31.728384
573.688008	32335.195939	31.733402
574.353335	32385.054250	31.738420
574.688926	32470.068189	31.743437
575.512185	32521.014516	31.748455
576.163816	32575.984260	31.753472
576.889003	32642.812720	31.758490
577.764979	32699.670412	31.763508
578.248421	32752.819541	31.768525
579.252331	32792.657838	31.773543
579.762871	32845.326269	31.778560
580.398278	32895.676928	31.783578
581.237114	32955.331056	31.788596
581.487516	33000.936974	31.793613
582.135507	33051.399583	31.798631
583.116265	33096.165007	31.803648
583.854568	33149.399222	31.808666
584.508384	33174.916774	31.813684
585.187034	33228.139043	31.818701
585.824036	33256.300694	31.823719
586.732406	33291.624613	31.828736
587.109546	33324.591257	31.833754
587.818203	33355.685306	31.838772
588.124600	33403.359319	31.843789
589.178193	33419.606031	31.848807
589.190229	33461.415530	31.853824
589.478928	33507.477102	31.858842
590.244838	33550.234526	31.863860
590.109173	33601.955379	31.868877
591.066591	33649.733372	31.873895
591.190976	33694.784514	31.878912
591.597308	33753.500186	31.883930
591.958307	33794.488853	31.888948
592.563627	33850.088736	31.893965
592.997248	33899.727856	31.898983
593.605914	33949.306490	31.904000
594.335842	34014.185957	31.909018
594.986495	34073.474312	31.914036
595.145834	34124.191513	31.919053
595.885766	34181.272189	31.924071
596.193857	34233.435560	31.929088
596.400469	34306.932903	31.934106
597.370432	34370.426307	31.939124
597.836059	34436.925913	31.944141
598.758802	34495.943273	31.949159
599.463218	34544.564086	31.954176
600.508913	34617.298527	31.959194
601.071986	34680.892157	31.964212
601.190607	34736.607173	31.969229
601.648802	34795.216666	31.974247
602.515773	34853.947822	31.979264
603.022812	34919.864828	31.984282
603.697834	34991.008677	31.989300
603.942857	35055.047772	31.994317
604.856086	35128.854035	31.999335
605.394987	35193.952539	32.004352
606.095583	35265.980037	32.009370
607.223583	35312.162514	32.014388
607.919861	35385.791257	32.019405
608.490874	35444.425163	32.024423
609.296421	35502.190303	32.029440
609.371581	35565.937517	32.034458
610.149931	35625.459125	32.039476
610.776983	35681.468203	32.044493
611.935422	35732.541628	32.049511
612.985663	35780.783304	32.054528
613.340725	35827.171198	32.059546
614.329008	35875.366608	32.064564
614.505524	35932.524324	32.069581
615.267391	35975.840522	32.074599
615.924364	36026.805534	32.079616
616.303809	36087.221789	32.084634
616.987195	36124.053078	32.089652
617.539075	36191.119257	32.094669
617.810773	36249.925419	32.099687
618.822540	36297.089179	32.104704
619.264911	36359.307488	32.109722
619.890146	36414.132457	32.114740
620.660493	36471.480480	32.119757
621.859077	36507.848274	32.124775
622.445257	36561.313575	32.129792
622.965834	36613.691592	32.134810
623.650477	36657.609296	32.139828
623.823554	36709.770707	32.144845
624.014201	36768.860289	32.149863
624.926339	36827.565144	32.154880
624.900256	36891.355939	32.159898
625.651285	36960.276148	32.164916
626.267119	37017.881965	32.169933
626.726211	37086.431353	32.174951
627.436140	37143.507482	32.179968
628.158112	37209.662295	32.184986
628.944729	37265.106921	32.190004
629.417603	37336.113686	32.195021
630.082698	37403.942004	32.200039
631.084481	37457.246255	32.205056
631.829589	37515.851670	32.210074
632.380192	37576.307602	32.215092
632.720645	37641.703546	32.220109
633.268368	37699.657408	32.225127
633.870189	37755.374098	32.230144
634.246420	37812.422520	32.235162
634.747865	37872.120607	32.240180
635.239361	37938.745612	32.245197
635.761294	38002.237835	32.250215
636.629354	38061.844107	32.255232
637.185779	38129.481700	32.260250
637.657708	38191.095357	32.265268
638.320101	38261.954325	32.270285
639.124353	38322.073916	32.275303
639.846200	38390.578283	32.280320
640.207511	38462.586468	32.285338
641.434035	38507.015247	32.290356
642.559894	38569.604273	32.295373
643.068208	38636.513122	32.300391
644.295522	38680.257236	32.305408
645.313107	38726.372094	32.310426
646.109408	38784.373362	32.315444
646.778766	38824.760398	32.320461
647.326207	38878.425191	32.325479
647.633302	38912.127066	32.330496
648.130537	38968.363568	32.335514
648.967255	39013.404393	32.340532
649.648822	39069.026635	32.345549
649.764241	39122.312489	32.350567
650.870844	39173.101209	32.355584
650.875874	39236.573075	32.360602
651.637272	39292.533125	32.365620
651.826649	39363.354959	32.370637
652.097319	39427.651449	32.375655
652.872620	39503.461862	32.380672
653.187018	39586.517873	32.385690
653.934341	39647.522520	32.390708
654.507336	39721.151446	32.395725
655.108463	39806.329480	32.400743
655.664930	39877.363822	32.405760
656.528104	39966.912162	32.410778
656.903930	40052.305521	32.415796
657.616908	40126.544177	32.420813
658.972843	40196.578908	32.425831
659.987743	40272.794664	32.430848
660.493107	40339.628146	32.435866
661.340989	40416.273140	32.440884
662.206092	40473.864267	32.445901
662.422470	40553.815686	32.450919
663.064057	40619.607915	32.455936
663.728722	40686.233110	32.460954
664.824877	40750.605519	32.465972
665.599738	40824.783052	32.470989
666.007571	40886.965712	32.476007
667.051496	40947.720233	32.481024
667.268567	41010.013903	32.486042
668.089762	41064.027933	32.491060
669.215808	41142.924837	32.496077
670.132549	41192.977233	32.501095
671.244372	41237.832628	32.506112
671.635365	41294.071790	32.511130
672.204919	41346.966675	32.516148
672.796684	41407.125354	32.521165
673.292805	41465.175465	32.526183
673.741670	41519.716724	32.531200
674.475370	41584.572105	32.536218
674.977385	41649.680857	32.541236
675.497376	41716.163313	32.546253
676.033304	41784.711216	32.551271
676.233761	41849.346671	32.556288
676.756312	41924.261903	32.561306
677.613331	41995.510224	32.566324
677.879765	42057.032054	32.571341
678.697527	42134.551064	32.576359
679.564693	42197.154370	32.581376
680.237933	42261.602266	32.586394
680.664660	42320.471641	32.591412
681.779346	42388.909900	32.596429
682.356980	42473.731599	32.601447
683.063735	42528.971782	32.606464
683.365808	42609.230405	32.611482
683.826450	42690.722763	32.616500
684.563122	42761.378354	32.621517
685.389845	42834.803919	32.626535
685.916793	42911.897719	32.631552
686.681501	42992.990464	32.636570
687.526551	43077.982053	32.641588
688.310041	43159.558622	32.646605
688.723168	43246.261308	32.651623
689.473297	43324.532154	32.656640
689.976212	43408.653811	32.661658
690.607264	43493.461812	32.666676
691.190737	43578.919036	32.671693
691.770783	43668.772246	32.676711
693.319579	43736.815025	32.681728
694.840664	43799.075195	32.686746
695.468574	43877.166578	32.691764
696.429107	43945.812970	32.696781
697.127800	44007.932525	32.701799
698.193483	44072.637271	32.706816
698.839370	44120.794409	32.711834
699.915199	44186.606122	32.716852
700.398674	44237.578540	32.721869
701.075596	44305.379782	32.726887
701.505976	44364.877020	32.731904
702.030623	44431.636777	32.736922
702.258225	44499.958525	32.741940
703.173189	44572.337459	32.746957
703.674534	44647.238731	32.751975
704.396357	44725.671699	32.756992
704.830433	44795.409546	32.762010
705.687828	44865.045795	32.767028
706.160537	44925.964995	32.772045
707.090342	45011.538603	32.777063
707.831221	45084.302061	32.782080
708.780466	45160.896108	32.787098
709.226341	45239.948562	32.792116
710.012122	45310.390911	32.797133
710.482446	45398.123435	32.802151
710.956616	45470.279034	32.807168
711.531483	45564.900760	32.812186
712.666037	45634.582258	32.817204
713.553778	45714.093829	32.822221
714.431065	45787.074183	32.827239
714.624512	45869.770966	32.832256
715.761833	45939.449974	32.837274
716.305035	46022.771428	32.842292
717.339810	46098.218298	32.847309
717.988461	46172.520148	32.852327
718.792926	46235.504205	32.857344
719.581236	46310.661274	32.862362
720.389296	46377.001937	32.867380
721.430428	46449.730288	32.872397
721.617938	46524.334283	32.877415
722.331356	46596.609195	32.882432
723.545235	46665.795024	32.887450
723.685438	46747.816068	32.892468
724.882850	46809.356812	32.897485
725.155806	46882.713301	32.902503
725.580366	46949.536478	32.907520
726.714266	47019.084244	32.912538
727.193414	47098.164202	32.917556
727.576688	47164.565512	32.922573
728.508812	47237.709726	32.927591
729.221835	47309.352672	32.932608
730.347944	47371.560776	32.937626
730.748066	47440.742422	32.942644
731.950556	47496.268607	32.947661
732.479912	47567.087201	32.952679
733.119425	47632.951800	32.957696
734.174939	47697.607519	32.962714
734.438328	47782.770593	32.967732
735.205711	47841.635430	32.972749
735.834274	47922.029857	32.977767
736.839652	47995.531159	32.982784
738.184994	48056.271346	32.987802
738.735089	48125.916925	32.992820
739.625567	48188.719488	32.997837
739.851281	48264.312444	33.002855
740.782393	48326.151805	33.007872
741.628490	48406.654275	33.012890
742.334421	48461.315113	33.017908
743.303244	48529.670448	33.022925
743.900052	48611.225776	33.027943
744.618037	48686.969224	33.032960
744.984125	48760.772253	33.037978
745.743565	48833.989160	33.042996
746.838580	48907.194852	33.048013
747.337888	48982.369393	33.053031
748.331269	49057.212706	33.058048
749.081058	49128.129979	33.063066
749.774966	49206.175529	33.068084
750.684593	49274.274897	33.073101
751.467275	49347.496225	33.078119
751.790520	49430.597483	33.083136
752.284503	49514.984616	33.088154
752.828261	49601.824199	33.093172
753.718379	49676.646011	33.098189
754.651897	49774.299018	33.103207
755.011785	49857.853999	33.108224
755.875603	49952.718001	33.113242
756.480916	50050.562704	33.118260
757.066952	50134.927796	33.123277
757.822881	50232.104098	33.128295
758.312691	50321.406826	33.133312
759.354015	50414.857073	33.138330
760.533552	50501.974182	33.143348
761.388512	50582.645382	33.148365
762.813659	50660.139561	33.153383
763.686457	50745.141953	33.158400
764.502859	50813.584412	33.163418
764.975362	50902.279942	33.168436
765.744413	50971.160381	33.173453
766.407283	51053.495251	33.178471
767.194972	51138.279764	33.183488
768.049167	51216.647970	33.188506
768.326822	51293.248621	33.193524
769.145940	51387.675407	33.198541
769.940565	51469.649040	33.203559
770.376042	51556.584870	33.208576
771.354670	51639.135135	33.213594
771.828491	51740.898529	33.218612
772.505788	51821.724412	33.223629
773.313453	51921.866619	33.228647
774.078560	52006.860831	33.233664
774.864271	52092.944918	33.238682
775.864788	52185.229109	33.243700
776.771569	52264.110846	33.248717
777.559932	52353.234379	33.253735
778.021457	52425.525654	33.258752
778.979207	52511.317692	33.263770
779.489938	52598.454161	33.268788
780.438910	52681.089581	33.273805
780.926284	52766.682847	33.278823
781.395629	52866.001587	33.283840
782.141298	52952.203514	33.288858
782.750270	53049.787896	33.293876
783.818917	53145.590646	33.298893
784.410113	53241.011919	33.303911
785.229544	53345.013363	33.308928
786.274467	53440.164432	33.313946
786.858635	53535.695711	33.318964
787.926565	53626.231765	33.323981
788.810171	53720.185285	33.328999
789.424523	53824.052725	33.334016
790.155644	53916.206583	33.339034
790.898822	54008.807456	33.344052
792.037439	54105.993266	33.349069
793.407070	54197.018911	33.354087
794.237277	54285.247111	33.359104
795.615529	54354.922916	33.364122
796.056926	54435.887213	33.369140
796.743054	54530.686122	33.374157
797.633943	54603.128971	33.379175
798.118475	54700.792756	33.384192
799.259003	54779.329904	33.389210
800.024018	54878.255905	33.394228
800.893681	54954.898973	33.399245
802.004990	55036.632788	33.404263
802.437674	55136.746248	33.409280
803.273577	55219.777593	33.414298
803.795626	55319.643360	33.419316
804.855619	55403.510233	33.424333
805.567480	55499.206751	33.429351
806.084452	55587.745512	33.434368
807.282886	55678.439936	33.439386
808.099699	55761.325074	33.444404
808.585495	55854.249030	33.449421
809.224799	55953.864735	33.454439
810.021280	56056.216144	33.459456
811.018532	56157.315228	33.464474
811.378379	56255.386500	33.469492
812.005121	56346.703338	33.474509
812.858401	56456.750053	33.479527
813.176344	56570.494338	33.484544
814.160578	56689.430271	33.489562
814.573013	56789.410083	33.494580
815.277452	56914.820213	33.499597
816.314305	57022.191905	33.504615
817.141005	57141.997121	33.509632
817.868123	57252.258738	33.514650
818.532481	57378.916982	33.519668
819.255332	57502.052838	33.524685
820.761444	57617.792302	33.529703
821.180012	57727.545341	33.534720
822.360382	57842.430199	33.539738
823.479723	57955.581705	33.544756
824.124008	58071.744900	33.549773
824.848412	58179.452718	33.554791
825.792902	58294.739527	33.559808
827.324235	58381.321256	33.564826
828.489826	58486.518168	33.569844
829.066365	58566.509937	33.574861
830.451453	58673.485103	33.579879
830.858951	58773.981196	33.584896
832.130028	58859.363225	33.589914
832.775240	58942.985202	33.594932
833.389183	59034.796713	33.599949
834.205450	59114.725589	33.604967
834.693311	59215.532848	33.609984
835.616804	59298.579249	33.615002
836.083513	59393.368164	33.620020
836.640570	59498.924162	33.625037
837.342066	59596.961374	33.630055
837.974769	59719.727610	33.635072
838.821139	59819.833742	33.640090
839.509221	59936.291123	33.645108
840.112380	60048.484624	33.650125
841.037678	60157.161892	33.655143
842.119074	60275.382427	33.660160
842.645926	60393.303849	33.665178
843.479892	60510.163755	33.670196
844.639796	60616.807376	33.675213
845.739364	60738.250882	33.680231
846.357332	60859.402156	33.685248
847.161271	60975.075187	33.690266
848.399469	61085.841744	33.695284
848.852360	61207.231056	33.700301
850.199431	61310.484809	33.705319
851.062911	61436.926859	33.710336
851.818543	61542.637480	33.715354
852.984325	61658.709401	33.720372
854.019496	61772.382894	33.725389
854.786301	61884.066338	33.730407
855.339090	62001.638798	33.735424
856.266090	62104.201494	33.740442
857.265835	62221.347072	33.745460
858.407649	62337.799744	33.750477
859.480536	62439.183212	33.755495
860.112302	62545.918248	33.760512
861.045065	62662.672933	33.765530
862.175979	62771.683958	33.770548
862.883247	62875.399449	33.775565
863.944928	62977.969441	33.780583
864.377756	63094.474548	33.785600
865.318243	63204.366479	33.790618
866.449612	63320.895984	33.795636
866.900219	63429.037327	33.800653
868.678968	63514.809733	33.805671
870.298649	63604.015973	33.810688
871.056376	63690.540119	33.815706
872.143097	63785.657366	33.820724
873.331229	63870.821315	33.825741
874.065070	63957.394792	33.830759
874.785244	64049.002606	33.835776
875.640714	64127.794129	33.840794
876.699333	64215.774994	33.845812
877.394114	64306.831889	33.850829
878.298218	64382.683220	33.855847
879.399755	64465.190063	33.860864
880.433168	64538.915489	33.865882
880.957441	64636.317200	33.870900
881.460170	64730.201896	33.875917
882.160253	64825.900132	33.880935
883.124327	64920.063117	33.885952
883.551089	65019.126396	33.890970
884.355515	65124.765106	33.895988
884.529851	65228.011900	33.901005
885.424192	65329.281144	33.906023
885.897361	65464.296285	33.911040
886.884600	65582.126760	33.916058
887.427005	65697.218556	33.921076
888.240069	65813.486167	33.926093
889.471584	65918.558591	33.931111
890.188062	66044.364158	33.936128
890.630063	66154.778006	33.941146
891.887521	66266.820907	33.946164
892.556778	66383.216701	33.951181
893.392413	66496.373961	33.956199
894.103874	66620.527460	33.961216
895.183702	66737.539855	33.966234
896.458216	66839.480349	33.971252
897.029448	66967.123673	33.976269
898.223267	67086.850251	33.981287
898.982245	67200.017702	33.986304
899.906612	67326.340156	33.991322
901.102185	67450.165316	33.996340
902.031947	67577.936182	34.001357
902.627712	67686.846813	34.006375
903.140076	67822.420653	34.011392
904.071760	67943.618140	34.016410
905.129857	68074.620432	34.021428
905.691862	68215.176965	34.026445
907.042171	68335.725552	34.031463
907.612655	68473.690155	34.036480
908.416801	68595.317186	34.041498
909.810447	68728.341646	34.046516
910.807957	68863.019681	34.051533
911.522702	68992.731577	34.056551
912.508216	69132.477815	34.061568
913.475642	69261.548750	34.066586
914.581005	69391.299411	34.071604
915.396357	69519.372847	34.076621
916.613335	69650.807420	34.081639
918.006956	69764.939167	34.086656
919.306641	69887.610505	34.091674
920.739350	69988.009749	34.096692
921.445429	70102.915005	34.101709
922.597241	70211.354261	34.106727
923.718329	70320.260754	34.111744
924.142264	70435.960752	34.116762
925.290619	70549.188922	34.121780
925.896177	70663.734479	34.126797
926.546248	70782.547780	34.131815
927.385145	70890.574486	34.136832
928.374141	71020.082444	34.141850
929.196693	71138.963940	34.146868
930.261293	71271.426521	34.151885
930.803696	71391.576323	34.156903
931.776803	71517.662611	34.161920
932.607820	71646.157181	34.166938
933.554716	71759.791927	34.171956
934.081840	71905.032630	34.176973
934.910393	72044.963027	34.181991
935.672252	72182.546670	34.187008
936.557023	72329.033540	34.192026
937.899965	72459.560106	34.197044
938.766983	72596.629352	34.202061
941.156588	72686.543011	34.207079
943.525676	72791.106467	34.212096
945.209272	72877.976171	34.217114
946.410347	72959.588936	34.222132
946.916227	73050.487062	34.227149
947.852848	73129.399773	34.232167
948.574900	73220.781299	34.237184
948.921118	73318.119544	34.242202
949.634601	73420.412226	34.247220
950.344342	73524.698087	34.252237
951.012648	73625.494104	34.257255
951.823874	73730.668453	34.262272
952.412310	73840.427344	34.267290
953.237614	73929.246074	34.272308
954.067172	74044.284604	34.277325
954.711716	74157.735439	34.282343
955.136774	74267.877747	34.287360
955.986261	74381.232486	34.292378
957.030094	74498.862434	34.297396
957.694885	74628.724011	34.302413
958.269655	74761.308145	34.307431
959.501922	74887.870605	34.312448
959.863119	75019.068737	34.317466
961.122244	75151.225430	34.322484
962.053839	75296.801078	34.327501
962.493596	75445.223165	34.332519
963.606336	75577.311841	34.337536
964.519480	75731.817506	34.342554
965.659053	75864.257631	34.347572
966.462224	76021.945942	34.352589
967.542369	76160.077352	34.357607
968.423938	76315.711832	34.362624
969.625859	76472.369477	34.367642
970.763015	76608.691630	34.372660
972.258826	76741.811587	34.377677
973.443757	76871.422950	34.382695
974.277540	77016.096376	34.387712
975.230895	77153.167108	34.392730
976.291404	77297.931245	34.397748
977.164175	77447.762322	34.402765
977.899798	77591.171765	34.407783
978.717831	77735.251581	34.412800
979.412467	77883.293470	34.417818
980.358513	78029.567799	34.422836
981.281677	78181.381597	34.427853
982.483105	78348.552678	34.432871
984.198008	78489.502920	34.437888
985.729066	78624.500622	34.442906
986.902033	78763.752403	34.447924
988.127425	78891.319309	34.452941
989.024336	79029.663387	34.457959
990.143373	79156.193068	34.462976
990.829672	79293.732407	34.467994
992.101531	79413.551910	34.473012
993.425323	79548.697103	34.478029
994.383689	79668.114529	34.483047
995.568690	79795.161898	34.488064
996.213855	79928.770938	34.493082
997.334690	80045.291450	34.498100
998.258711	80184.757807	34.503117
999.368941	80322.334283	34.508135
1000.374608	80443.323129	34.513152
1000.854803	80587.837873	34.518170
1002.144687	80704.333727	34.523188
1002.923288	80848.155349	34.528205
1003.570922	80986.400949	34.533223
1004.393448	81125.814022	34.538240
1004.965457	81283.210777	34.543258
1005.986316	81424.958791	34.548276
1007.394093	81546.260038	34.553293
1008.509569	81695.047891	34.558311
1010.069107	81835.627262	34.563328
1010.915069	81984.588254	34.568346
1011.917684	82118.327992	34.573364
1012.770001	82254.314063	34.578381
1013.803562	82397.236413	34.583399
1014.513020	82538.454640	34.588416
1015.385532	82687.105792	34.593434
1016.674169	82822.655887	34.598452
1017.807418	82962.237382	34.603469
1019.086769	83106.122985	34.608487
1020.250418	83226.417083	34.613504
1021.096218	83363.062463	34.618522
1021.972106	83483.114618	34.623540
1022.699403	83622.672578	34.628557
1023.346911	83752.918713	34.633575
1024.177948	83889.057176	34.638592
1024.912149	84041.232508	34.643610
1025.683563	84187.803222	34.648628
1026.788459	84332.490995	34.653645
1027.447046	84485.219595	34.658663
1028.703071	84627.093863	34.663680
1029.623138	84803.444820	34.668698
1030.795319	84961.709907	34.673716
1031.731854	85121.938675	34.678733
1032.263672	85289.151501	34.683751
1033.462719	85451.749701	34.688768
1034.289220	85628.324905	34.693786
1035.339428	85787.419425	34.698804
1036.445167	85968.740779	34.703821
1037.318067	86146.318275	34.708839
1038.521165	86305.884504	34.713856
1039.745848	86488.822676	34.718874
1040.778594	86661.941850	34.723892
1042.265124	86826.988700	34.728909
1043.139779	87000.680789	34.733927
1044.582762	87165.268980	34.738944
1045.743306	87332.537596	34.743962
1046.778694	87486.659702	34.748980
1048.410016	87649.302655	34.753997
1049.328094	87812.362494	34.759015
1050.865386	87961.335662	34.764032
1051.985277	88117.548783	34.769050
1053.587292	88245.547961	34.774068
1055.258223	88392.660180	34.779085
1056.305016	88542.737233	34.784103
1057.136825	88677.992132	34.789120
1058.627615	88814.081376	34.794138
1059.896453	88939.981635	34.799156
1061.008152	89074.907577	34.804173
1061.670096	89206.934556	34.809191
1062.982415	89335.557236	34.814208
1064.127494	89491.711925	34.819226
1064.603105	89609.393741	34.824244
1065.926460	89739.276140	34.829261
1066.591454	89887.703647	34.834279
1067.637236	90023.253429	34.839296
1068.446737	90175.905249	34.844314
1069.508641	90320.852104	34.849332
1070.755508	90458.231619	34.854349
1071.547519	90612.256122	34.859367
1072.992260	90746.876753	34.864384
1074.084408	90902.441848	34.869402
1075.018853	91048.477485	34.874420
1076.053626	91185.738123	34.879437
1076.942432	91334.295647	34.884455
1078.333449	91469.005175	34.889472
1079.194411	91623.562663	34.894490
1080.359705	91776.513689	34.899508
1081.377995	91918.698921	34.904525
1082.269923	92076.032642	34.909543
1083.321028	92222.271201	34.914560
1084.305348	92370.534419	34.919578
1084.825814	92526.103537	34.924596
1086.404501	92686.922297	34.929613
1087.131678	92849.269530	34.934631
1088.570832	93003.474032	34.939648
1089.156985	93161.125005	34.944666
1090.668833	93319.458899	34.949684
1091.787634	93461.275685	34.954701
1092.812474	93605.431830	34.959719
1093.541732	93748.492208	34.964736
1094.681309	93902.606507	34.969754
1095.325769	94067.931488	34.974772
1096.666018	94211.880625	34.979789
1097.475290	94374.420567	34.984807
1098.761985	94521.349057	34.989824
1099.847497	94680.047310	34.994842
1100.360350	94846.602023	34.999860
1101.855301	95010.197092	35.004877
1102.513543	95174.881560	35.009895
1103.417105	95346.514745	35.014912
1105.324522	95517.672395	35.019930
1105.868252	95687.791462	35.024948
1107.314043	95861.699376	35.029965
1108.326509	96028.293084	35.034983
1109.561653	96194.179959	35.040000
1110.212693	96373.838219	35.045018
1111.067777	96553.615847	35.050036
1112.478525	96733.422856	35.055053
1113.125156	96917.219480	35.060071
1114.103503	97108.970438	35.065088
1115.180418	97298.016049	35.070106
1116.792146	97486.657828	35.075124
1118.745422	97655.094088	35.080141
1119.512957	97843.884942	35.085159
1121.087973	98005.530231	35.090176
1122.344233	98203.688073	35.095194
1123.525544	98371.029044	35.100212
1125.185707	98544.913710	35.105229
1126.130436	98716.892395	35.110247
1127.043674	98895.404630	35.115264
1128.630458	99064.499893	35.120282
1129.417277	99223.194247	35.125300
1131.051276	99393.708344	35.130317
1132.346741	99556.473547	35.135335
1133.755360	99713.206472	35.140352
1135.038064	99873.544679	35.145370
1136.278336	100027.831995	35.150388
1137.705151	100167.628794	35.155405
1139.504203	100303.122667	35.160423
1141.146829	100431.558507	35.165440
1142.812195	100573.647869	35.170458
1143.453728	100706.562803	35.175476
1144.821306	100841.966504	35.180493
1145.356484	100979.446431	35.185511
1146.333285	101119.215459	35.190528
1147.289611	101262.610255	35.195546
1147.945629	101413.678826	35.200564
1149.040856	101553.316601	35.205581
1149.872148	101708.429016	35.210599
1150.802775	101874.365644	35.215616
1152.126267	102035.875637	35.220634
1153.024527	102201.509485	35.225652
1154.107322	102365.891751	35.230669
1155.443233	102522.894516	35.235687
1156.402569	102685.621367	35.240704
1157.479571	102845.353736	35.245722
1158.247064	103007.842162	35.250740
1159.234614	103186.916478	35.255757
1160.339866	103373.767194	35.260775
1161.558832	103551.596214	35.265792
1162.520961	103729.950294	35.270810
1163.318139	103923.403434	35.275828
1164.492106	104096.836464	35.280845
1165.535276	104277.143805	35.285863
1166.872870	104456.441038	35.290880
1168.382125	104616.676110	35.295898
1169.412626	104785.844197	35.300916
1170.957245	104938.945151	35.305933
1172.078178	105111.228525	35.310951
1172.767640	105278.809926	35.315968
1174.559129	105438.407931	35.320986
1175.036272	105617.184569	35.326004
1176.258855	105779.057405	35.331021
1177.242070	105959.918147	35.336039
1177.992731	106144.225677	35.341056
1179.161378	106335.595781	35.346074
1179.877795	106527.878208	35.351092
1181.528298	106718.461863	35.356109
1182.504085	106916.884890	35.361127
1183.572427	107115.040722	35.366144
1185.235402	107309.552931	35.371162
1186.029810	107502.272747	35.376180
1187.234489	107701.030936	35.381197
1188.321250	107901.634088	35.386215
1189.107126	108111.395697	35.391232
1190.302189	108308.652692	35.396250
1191.365187	108539.043172	35.401268
1192.638603	108755.252149	35.406285
1193.825761	108968.538498	35.411303
1194.793027	109195.074451	35.416320
1195.962944	109410.140487	35.421338
1196.818256	109650.885724	35.426356
1197.860130	109867.344655	35.431373
1198.974683	110107.734251	35.436391
1199.994956	110346.203507	35.441408
1201.228407	110581.877984	35.446426
1202.231974	110830.133482	35.451444
1203.805560	111067.009798	35.456461
1204.794707	111310.686350	35.461479
1206.465358	111541.318120	35.466496
1207.939637	111785.222429	35.471514
1209.530952	112017.138142	35.476532
1210.553216	112252.709959	35.481549
1212.186390	112482.418367	35.486567
1213.666747	112715.840534	35.491584
1215.199164	112937.512326	35.496602
1216.378790	113166.908913	35.501620
1218.076760	113381.120308	35.506637
1219.470222	113599.488553	35.511655
1220.445516	113828.405056	35.516672
1221.798893	114036.344187	35.521690
1222.887526	114262.977692	35.526708
1223.959727	114476.997226	35.531725
1225.678078	114688.846114	35.536743
1227.159257	114898.379432	35.541760
1228.747916	115091.096752	35.546778
1229.880649	115316.261766	35.551796
1231.499982	115521.963259	35.556813
1233.059919	115715.690510	35.561831
1234.331208	115916.840814	35.566848
1235.428537	116109.595895	35.571866
1236.869923	116303.954985	35.576884
1237.902837	116498.915302	35.581901
1239.332727	116692.607437	35.586919
1240.061835	116891.801996	35.591936
1241.353250	117095.427992	35.596954
1242.563031	117290.769828	35.601972
1243.732600	117483.864311	35.606989
1245.122002	117683.094223	35.612007
1245.750496	117899.101054	35.617024
1247.052117	118097.524800	35.622042
1248.199883	118303.261199	35.627060
1249.328699	118514.146630	35.632077
1250.049711	118717.270512	35.637095
1251.377050	118918.888746	35.642112
1252.462120	119125.122891	35.647130
1253.245023	119323.032861	35.652148
1254.425775	119530.913961	35.657165
1255.624612	119747.093395	35.662183
1257.127386	119969.116323	35.667200
1258.165167	120174.250635	35.672218
1259.414825	120396.559555	35.677236
1260.884233	120616.907581	35.682253
1261.866521	120835.107788	35.687271
1263.463907	121064.891260	35.692288
1264.774883	121272.319596	35.697306
1265.474148	121515.257215	35.702324
1267.063332	121725.607906	35.707341
1268.295559	121964.101510	35.712359
1270.131393	122190.888829	35.717376
1271.816513	122398.478435	35.722394
1272.843195	122621.956289	35.727412
1274.345019	122833.736000	35.732429
1275.539509	123052.665040	35.737447
1277.097341	123280.685354	35.742464
1278.503462	123496.933877	35.747482
1280.060060	123695.669957	35.752500
1281.461198	123909.083477	35.757517
1283.146425	124115.100823	35.762535
1284.316671	124340.151855	35.767552
1285.414352	124539.210419	35.772570
1286.933397	124742.978374	35.777588
1288.081617	124951.156301	35.782605
1289.524119	125163.938144	35.787623
1290.893207	125372.627305	35.792640
1292.518162	125575.394721	35.797658
1294.008219	125775.384889	35.802676
1294.994790	125988.729736	35.807693
1296.357836	126181.544699	35.812711
1297.108357	126398.974646	35.817728
1298.245120	126601.855196	35.822746
1299.704724	126833.796911	35.827764
1300.594220	127062.970467	35.832781
1301.817218	127278.743944	35.837799
1302.799352	127506.194342	35.842816
1304.289686	127736.008380	35.847834
1305.146537	127958.134074	35.852852
1306.418917	128214.022235	35.857869
1307.982916	128442.663182	35.862887
1308.915474	128679.433986	35.867904
1310.551493	128910.183189	35.872922
1312.263266	129144.267856	35.877940
1313.510463	129370.699234	35.882957
1315.295409	129587.751809	35.887975
1316.470755	129830.347197	35.892992
1317.742401	130053.965429	35.898010
1318.660578	130283.905777	35.903028
1319.802146	130527.500851	35.908045
1321.463086	130751.642553	35.913063
1322.715016	130990.279197	35.918080
1324.458140	131219.037388	35.923098
1326.003156	131437.739676	35.928116
1327.260186	131665.098553	35.933133
1328.772416	131886.826359	35.938151
1330.086014	132114.762176	35.943168
1331.775231	132318.779693	35.948186
1333.956990	132529.143967	35.953204
1335.550624	132735.309690	35.958221
1337.283572	132932.693836	35.963239
1338.952386	133120.404560	35.968256
1340.588637	133307.893589	35.973274
1341.796215	133469.872224	35.978292
1342.751811	133652.823607	35.983309
1344.362936	133811.605742	35.988327
1344.868027	133992.161674	35.993344
1346.031386	134169.997879	35.998362
1347.368198	134342.773311	36.003380
1348.043029	134541.711911	36.008397
1349.843524	134730.931421	36.013415
1350.629996	134930.208843	36.018432
1351.888458	135125.466394	36.023450
1352.827878	135327.091615	36.028468
1353.575741	135551.912526	36.033485
1354.902693	135771.428242	36.038503
1355.417953	136008.778750	36.043520
1356.651165	136227.514317	36.048538
1358.156982	136470.168183	36.053556
1359.031445	136709.771596	36.058573
1360.361885	136954.093597	36.063591
1361.868960	137211.269580	36.068608
1362.532992	137467.129298	36.073626
1364.381705	137723.593269	36.078644
1365.073923	137991.015397	36.083661
1366.543642	138251.502075	36.088679
1367.723334	138526.277516	36.093696
1368.674796	138799.863155	36.098714
1370.296678	139079.121597	36.103732
1371.686442	139364.532319	36.108749
1373.343470	139633.607904	36.113767
1374.826972	139922.697504	36.118784
1376.359172	140194.448257	36.123802
1378.304784	140461.504465	36.128820
1380.151741	140741.880373	36.133837
1381.481969	140993.243558	36.138855
1382.909922	141272.082902	36.143872
1384.427347	141530.152106	36.148890
1386.416417	141782.730518	36.153908
1387.680704	142054.553039	36.158925
1389.239754	142308.221016	36.163943
1390.366629	142572.056274	36.168960
1392.035611	142822.057737	36.173978
1394.213895	143069.668622	36.178996
1396.084462	143300.289181	36.184013
1398.036635	143540.700105	36.189031
1400.589475	143753.343020	36.194048
1402.341027	143954.263254	36.199066
1403.916993	144164.952899	36.204084
1404.951336	144386.068844	36.209101
1406.366127	144593.934479	36.214119
1407.379787	144816.793876	36.219136
1408.713122	145027.465462	36.224154
1409.620987	145257.649696	36.229172
1410.618483	145490.268106	36.234189
1411.489262	145721.514046	36.239207
1412.562638	145967.299292	36.244224
1413.133603	146214.133353	36.249242
1414.634350	146465.038024	36.254260
1416.020293	146722.215743	36.259277
1417.583055	146973.367293	36.264295
1419.085546	147230.047361	36.269312
1420.069243	147475.489921	36.274330
1421.921135	147716.833243	36.279348
1423.343119	147971.210986	36.284365
1424.978441	148230.552066	36.289383
1426.348025	148483.445497	36.294400
1428.054556	148731.845816	36.299418
1429.883606	148984.666495	36.304436
1430.777817	149239.203923	36.309453
1431.878566	149473.124266	36.314471
1433.046382	149720.085893	36.319488
1434.482280	149961.335308	36.324506
1436.032017	150208.756850	36.329524
1436.792527	150460.242742	36.334541
1438.065963	150713.268749	36.339559
1439.295077	150966.747730	36.344576
1440.442979	151228.080366	36.349594
1442.064999	151488.600536	36.354612
1443.241746	151765.596497	36.359629
1444.215202	152036.451126	36.364647
1445.872388	152314.411498	36.369664
1447.005011	152608.049621	36.374682
1448.589889	152876.462264	36.379700
1450.000170	153177.960957	36.384717
1451.958631	153447.901180	36.389735
1454.049682	153729.605170	36.394752
1455.766215	153990.481859	36.399770
1458.035188	154253.932473	36.404788
1459.540783	154517.790517	36.409805
1460.985375	154766.502122	36.414823
1462.506238	155039.151724	36.419840
1463.781365	155310.359827	36.424858
1465.113404	155580.393339	36.429876
1466.389536	155857.503600	36.434893
1467.659149	156124.354527	36.439911
1469.288436	156404.276923	36.444928
1470.516823	156678.863780	36.449946
1471.977763	156952.120049	36.454964
1473.303295	157245.380443	36.459981
1474.627128	157533.124994	36.464999
1475.648331	157825.374490	36.470016
1476.981691	158123.130758	36.475034
1478.475666	158421.040191	36.480052
1479.834950	158737.622655	36.485069
1481.028168	159029.903068	36.490087
1482.759062	159347.164451	36.495104
1483.643968	159669.820714	36.500122
1485.502870	159976.206228	36.505140
1486.940714	160292.724264	36.510157
1488.526566	160606.188078	36.515175
1489.741546	160923.356848	36.520192
1491.244677	161254.423092	36.525210
1492.925365	161574.056969	36.530228
1494.557074	161899.423259	36.535245
1496.064022	162205.109648	36.540263
1498.379794	162521.879651	36.545280
1500.172694	162846.313051	36.550298
1502.221497	163131.147169	36.555316
1504.614508	163409.024135	36.560333
1506.234762	163694.516702	36.565351
1508.199534	163976.033569	36.570368
1509.490099	164257.334187	36.575386
1511.305898	164535.872430	36.580404
1512.309428	164813.633615	36.585421
1513.957010	165096.085855	36.590439
1515.349093	165379.242073	36.595456
1516.327549	165675.600942	36.600474
1518.272791	165948.036472	36.605492
1519.293256	166244.557175	36.610509
1520.711384	166530.584082	36.615527
1522.079857	166829.855162	36.620544
1523.364627	167129.129453	36.625562
1524.601764	167432.715113	36.630580
1525.402277	167739.725058	36.635597
1526.804950	168051.192564	36.640615
1528.720110	168351.347576	36.645632
1530.351159	168667.171855	36.650650
1532.011181	168950.534855	36.655668
1534.000191	169242.930525	36.660685
1535.835632	169514.187882	36.665703
1537.480955	169790.351072	36.670720
1539.044822	170068.331328	36.675738
1540.598165	170338.663265	36.680756
1541.648116	170626.756783	36.685773
1543.010079	170912.503547	36.690791
1544.652926	171194.309768	36.695808
1545.572142	171489.485800	36.700826
1546.850576	171789.933887	36.705844
1548.318475	172088.867769	36.710861
1549.483849	172401.660458	36.715879
1551.089586	172717.795857	36.720896
1552.465120	173046.471382	36.725914
1554.213717	173358.996048	36.730932
1555.678658	173672.851518	36.735949
1557.052717	173996.280025	36.740967
1558.805487	174311.284862	36.745984
1560.103616	174646.557911	36.751002
1562.333338	174959.292427	36.756020
1563.889147	175277.978446	36.761037
1565.432628	175601.186543	36.766055
1567.979780	175913.227324	36.771072
1569.652404	176229.780788	36.776090
1571.472984	176537.453357	36.781108
1573.097742	176854.513714	36.786125
1574.809250	177163.388531	36.791143
1576.573147	177465.517468	36.796160
1577.971650	177780.666754	36.801178
1579.533369	178089.813257	36.806196
1580.898733	178401.900579	36.811213
1582.282592	178724.076633	36.816231
1584.229293	179028.418359	36.821248
1586.077443	179345.305067	36.826266
1588.140061	179639.033543	36.831284
1590.201142	179943.450590	36.836301
1591.575422	180244.556437	36.841319
1593.758423	180534.449750	36.846336
1595.927770	180821.491201	36.851354
1597.675496	181094.503035	36.856372
1599.178018	181389.349652	36.861389
1600.456132	181672.824663	36.866407
1601.688680	181962.629593	36.871424
1603.447961	182274.014939	36.876442
1605.172481	182561.025377	36.881460
1606.700815	182847.866798	36.886477
1607.683660	183146.947131	36.891495
1609.380910	183435.489900	36.896512
1610.527035	183746.287336	36.901530
1611.895454	184060.552956	36.906548
1613.813328	184370.388291	36.911565
1614.911232	184688.840296	36.916583
1616.525038	184995.315124	36.921600
1617.998243	185318.811212	36.926618
1619.577777	185635.589491	36.931636
1620.951957	185960.311595	36.936653
1623.018549	186268.774722	36.941671
1625.458081	186581.633152	36.946688
1626.749077	186887.994182	36.951706
1629.009077	187188.611027	36.956724
1630.644130	187486.362724	36.961741
1632.244618	187794.594088	36.966759
1633.426677	188096.574923	36.971776
1634.796060	188418.239971	36.976794
1636.387287	188727.150637	36.981812
1637.919786	189043.155974	36.986829
1638.772415	189382.645639	36.991847
1639.945835	189690.970563	36.996864
1641.304890	190019.983398	37.001882
1643.017360	190333.858585	37.006900
1645.133918	190642.133680	37.011917
1646.350125	190958.988747	37.016935
1647.537324	191282.591101	37.021952
1648.969939	191618.239789	37.026970
1649.984147	191957.019110	37.031988
1651.748785	192297.085042	37.037005
1653.298363	192650.581562	37.042023
1654.725345	192998.755874	37.047040
1655.881619	193352.765928	37.052058
1657.928546	193708.141072	37.057076
1659.866093	194075.444394	37.062093
1661.154845	194448.367119	37.067111
1662.988098	194805.967455	37.072128
1664.434336	195181.077356	37.077146
1665.936687	195563.975143	37.082164
1667.094977	195943.542535	37.087181
1668.556477	196336.925457	37.092199
1670.316106	196733.701855	37.097216
1671.862339	197135.441965	37.102234
1673.711240	197528.082240	37.107252
1675.928546	197928.547910	37.112269
1677.266052	198337.071387	37.117287
1678.973877	198733.246198	37.122304
1680.336686	199149.070603	37.127322
1681.956951	199551.308035	37.132340
1683.924632	199973.131348	37.137357
1685.092134	200401.907793	37.142375
1686.979358	200819.216981	37.147392
1688.803298	201245.121964	37.152410
1690.507232	201674.210845	37.157428
1692.716999	202086.141482	37.162445
1695.013255	202495.101811	37.167463
1697.311889	202891.989417	37.172480
1699.456770	203283.089512	37.177498
1701.813278	203671.566445	37.182516
1704.156052	204048.341079	37.187533
1706.050266	204425.407818	37.192551
1708.061925	204795.384699	37.197568
1710.097925	205162.058097	37.202586
1712.235838	205520.653633	37.207604
1713.978481	205878.821170	37.212621
1715.868126	206235.340748	37.217639
1717.744703	206582.302987	37.222656
1719.520806	206938.374804	37.227674
1721.506258	207294.413537	37.232692
1723.578398	207619.203476	37.237709
1724.903836	207978.008459	37.242727
1726.370566	208321.579805	37.247744
1728.369699	208662.664502	37.252762
1729.658490	209008.376076	37.257780
1731.245793	209360.769492	37.262797
1733.191907	209699.200751	37.267815
1735.161393	210034.150279	37.272832
1737.106949	210381.549155	37.277850
1738.632387	210731.761872	37.282868
1740.311545	211069.531815	37.287885
1741.225378	211430.997707	37.292903
1742.718120	211777.309099	37.297920
1744.465256	212146.512766	37.302938
1745.193911	212504.763068	37.307956
1747.559078	212880.445122	37.312973
1748.761598	213251.927804	37.317991
1750.476781	213620.914352	37.323008
1751.812590	214012.289289	37.328026
1753.273302	214391.860926	37.333044
1755.193388	214769.199234	37.338061
1757.150475	215138.481986	37.343079
1758.322983	215509.775638	37.348096
1760.097051	215877.390002	37.353114
1761.921352	216251.448470	37.358132
1764.057214	216596.782701	37.363149
1765.772277	216967.280975	37.368167
1767.668884	217337.648980	37.373184
1769.682301	217702.817824	37.378202
1771.496729	218075.869012	37.383220
1773.388533	218439.409833	37.388237
1774.719555	218837.358026	37.393255
1776.038408	219267.362601	37.398272
1778.288944	219633.286475	37.403290
1780.179109	220018.879086	37.408308
1782.399009	220387.325140	37.413325
1784.262567	220758.701593	37.418343
1786.444209	221126.470777	37.423360
1787.884601	221506.250768	37.428378
1789.557497	221886.806318	37.433396
1791.811669	222274.150017	37.438413
1793.076955	222655.563125	37.443431
1794.401733	223043.495288	37.448448
1795.962693	223433.904171	37.453466
1797.687016	223839.425398	37.458484
1799.286916	224245.425848	37.463501
1800.478263	224658.429508	37.468519
1801.860332	225072.469780	37.473536
1803.845578	225505.258195	37.478554
1805.353938	225938.050969	37.483572
1807.314611	226371.151298	37.488589
1809.243135	226792.447398	37.493607
1810.855217	227235.082691	37.498624
1812.912408	227671.524273	37.503642
1814.569666	228108.770196	37.508660
1816.346911	228557.554877	37.513677
1818.034491	229006.787721	37.518695
1819.919113	229455.354373	37.523712
1821.875175	229902.716802	37.528730
1824.109418	230354.936904	37.533748
1825.825525	230798.455598	37.538765
1827.658856	231257.857202	37.543783
1829.495572	231704.863980	37.548800
1831.587897	232158.230802	37.553818
1833.159615	232604.039489	37.558836
1835.105871	233059.643068	37.563853
1837.343776	233514.386788	37.568871
1838.936744	233954.582070	37.573888
1840.982264	234398.996387	37.578906
1842.971873	234856.934754	37.583924
1845.079559	235301.239544	37.588941
1847.054795	235729.005553	37.593959
1849.926760	236170.086908	37.598976
1852.999283	236573.211287	37.603994
1854.775015	236997.634942	37.609012
1856.826467	237398.288528	37.614029
1859.122427	237806.700833	37.619047
1861.006457	238214.801226	37.624064
1863.125981	238602.440212	37.629082
1864.374287	239009.987118	37.634100
1866.564927	239397.844454	37.639117
1868.594881	239798.531827	37.644135
1870.260486	240198.797679	37.649152
1872.200428	240585.301585	37.654170
1873.517012	240989.868879	37.659188
1875.367225	241385.356036	37.664205
1877.169971	241787.659569	37.669223
1878.689682	242191.077579	37.674240
1880.503087	242584.261197	37.679258
1882.058755	242979.850570	37.684276
1884.231045	243364.923334	37.689293
1886.031569	243745.968444	37.694311
1887.478475	244132.839080	37.699328
1889.473875	244529.831243	37.704346
1890.825571	244930.944243	37.709364
1892.518798	245330.527844	37.714381
1894.198926	245734.686641	37.719399
1895.839223	246153.357560	37.724416
1897.482030	246562.654964	37.729434
1898.734180	247005.879614	37.734452
1900.836324	247443.400765	37.739469
1902.096519	247881.214370	37.744487
1903.644851	248329.522975	37.749504
1905.672569	248773.662789	37.754522
1906.979374	249250.336778	37.759540
1908.298396	249715.704924	37.764557
1910.525493	250207.824944	37.769575
1911.942563	250688.445073	37.774592
1914.082955	251172.248223	37.779610
1915.751068	251672.692910	37.784628
1917.725567	252164.805844	37.789645
1919.949303	252662.974642	37.794663
1921.927249	253159.152286	37.799680
1924.189679	253652.692011	37.804698
1926.114275	254154.848908	37.809716
1928.664583	254651.262907	37.814733
1931.186966	255141.432586	37.819751
1933.545713	255626.980799	37.824768
1935.930583	256100.128073	37.829786
1937.786856	256582.406645	37.834804
1940.010059	257058.299136	37.839821
1941.781182	257535.740017	37.844839
1943.485582	258028.383198	37.849856
1945.292180	258509.298576	37.854874
1947.703476	258990.189999	37.859892
1949.649941	259471.564879	37.864909
1951.998297	259951.298138	37.869927
1953.401204	260448.538419	37.874944
1955.460419	260933.628713	37.879962
1957.281357	261428.259190	37.884980
1959.281955	261928.981935	37.889997
1961.099216	262420.411871	37.895015
1962.437097	262918.500457	37.900032
1964.245072	263423.090351	37.905050
1965.736624	263940.002137	37.910068
1967.494172	264460.984841	37.915085
1969.922090	264970.323068	37.920103
1971.976525	265494.736050	37.925120
1974.050471	266001.718800	37.930138
1975.700212	266529.093870	37.935156
1977.906691	267046.519786	37.940173
1980.246454	267569.435548	37.945191
1981.998607	268101.110509	37.950208
1983.997243	268611.456282	37.955226
1985.922561	269154.024543	37.960244
1987.725114	269681.091209	37.965261
1989.746765	270209.467195	37.970279
1991.383850	270746.974934	37.975296
1993.945663	271264.107996	37.980314
1996.071175	271802.498441	37.985332
1998.437618	272323.548793	37.990349
2000.485448	272843.863550	37.995367
2002.072034	273379.673193	38.000384
2004.350886	273892.733425	38.005402
2006.449198	274426.474864	38.010420
2008.384883	274940.453618	38.015437
2010.427370	275450.781090	38.020455
2012.476265	275962.706792	38.025472
2014.936411	276435.316666	38.030490
2017.858348	276899.694947	38.035508
2020.171312	277369.456821	38.040525
2022.658541	277835.937348	38.045543
2024.506234	278308.314490	38.050560
2026.569022	278769.808258	38.055578
2028.591108	279236.184915	38.060596
2030.027067	279713.809034	38.065613
2031.593055	280183.256445	38.070631
2033.140943	280688.014228	38.075648
2035.039903	281176.938010	38.080666
2036.355216	281687.777208	38.085684
2038.086553	282195.142218	38.090701
2039.598452	282722.736321	38.095719
2041.177055	283264.517156	38.100736
2043.026192	283797.818171	38.105754
2044.676960	284342.428476	38.110772
2046.971731	284885.812600	38.115789
2049.570649	285430.820934	38.120807
2052.100279	285969.234550	38.125824
2054.365205	286511.779637	38.130842
2056.055293	287064.451276	38.135860
2058.264506	287609.922612	38.140877
2060.605997	288145.285892	38.145895
2062.906050	288700.009184	38.150912
2065.213558	289241.215967	38.155930
2068.027853	289782.362026	38.160948
2069.858417	290330.984077	38.165965
2072.296757	290859.310048	38.170983
2074.416180	291411.080061	38.176000
2076.496308	291941.950046	38.181018
2078.474203	292485.610771	38.186036
2079.976607	293029.297024	38.191053
2082.551703	293584.867909	38.196071
2083.938474	294145.585889	38.201088
2086.689583	294701.655688	38.206106
2088.707372	295242.579332	38.211124
2090.594551	295802.596692	38.216141
2092.251711	296370.116597	38.221159
2094.262186	296938.133796	38.226176
2096.138408	297504.595507	38.231194
2098.083184	298080.338682	38.236212
2099.676203	298671.706136	38.241229
2101.969124	299252.185409	38.246247
2104.123594	299832.836668	38.251264
2106.317647	300412.462070	38.256282
2108.700980	301010.440691	38.261300
2110.827191	301593.194241	38.266317
2112.986103	302183.939020	38.271335
2114.895543	302776.753199	38.276352
2116.943969	303359.229341	38.281370
2119.528035	303946.082936	38.286388
2121.310778	304547.084486	38.291405
2123.341845	305139.685372	38.296423
2125.915262	305734.833683	38.301440
2128.121529	306337.657621	38.306458
2130.484011	306918.864767	38.311476
2132.655600	307501.648704	38.316493
2135.021203	308087.520140	38.321511
2137.327567	308671.035458	38.326528
2139.852291	309247.095000	38.331546
2142.385288	309813.067172	38.336564
2144.708908	310397.760771	38.341581
2146.498634	310964.431950	38.346599
2148.834063	311532.913250	38.351616
2151.118999	312091.063188	38.356634
2153.566547	312637.856273	38.361652
2156.533764	313159.596929	38.366669
2159.195513	313669.424002	38.371687
2160.911739	314194.513475	38.376704
2163.114029	314703.850863	38.381722
2165.866386	315200.422282	38.386740
2168.164047	315698.335264	38.391757
2170.479504	316191.925022	38.396775
2172.766051	316678.558491	38.401792
2176.266002	317144.978180	38.406810
2178.312331	317630.121280	38.411828
2180.265357	318101.767696	38.416845
2182.441116	318584.927449	38.421863
2184.398812	319067.815195	38.426880
2185.968710	319565.440206	38.431898
2187.915754	320050.912649	38.436916
2189.603064	320553.614592	38.441933
2191.037823	321068.136086	38.446951
2192.575977	321596.474549	38.451968
2194.335199	322126.117825	38.456986
2196.386321	322677.899826	38.462004
2197.671088	323242.245279	38.467021
2199.812023	323793.393367	38.472039
2201.542706	324372.355781	38.477056
2203.476872	324960.698699	38.482074
2206.092121	325530.414295	38.487092
2207.995193	326118.573552	38.492109
2210.390973	326694.890412	38.497127
2212.857937	327286.651702	38.502144
2214.791125	327889.514113	38.507162
2217.144940	328492.681541	38.512180
2219.111512	329090.321537	38.517197
2221.543417	329696.027774	38.522215
2223.912230	330316.183530	38.527232
2226.020783	330926.423887	38.532250
2228.434379	331533.230697	38.537268
2230.478070	332157.253538	38.542285
2232.856074	332773.445811	38.547303
2235.258203	333399.705457	38.552320
2237.613641	334027.057254	38.557338
2239.628549	334641.206992	38.562356
2241.861149	335273.717899	38.567373
2244.450913	335901.542127	38.572391
2246.873994	336520.374999	38.577408
2248.968779	337154.891630	38.582426
2251.272471	337772.967923	38.587444
2253.983883	338399.853576	38.592461
2256.316928	339024.788935	38.597479
2258.317763	339650.000074	38.602496
2260.762006	340278.988212	38.607514
2262.880263	340910.636812	38.612532
2264.705903	341542.224309	38.617549
2266.970355	342178.680489	38.622567
2269.194043	342830.795446	38.627584
2271.221647	343476.360429	38.632602
2273.694014	344117.249211	38.637620
2276.120689	344765.370368	38.642637
2278.638286	345388.874395	38.647655
2281.135153	346040.062816	38.652672
2283.752207	346672.746131	38.657690
2286.448715	347288.759061	38.662708
2288.903698	347920.563879	38.667725
2291.807654	348540.763895	38.672743
2294.461189	349147.292825	38.677760
2296.447359	349768.719243	38.682778
2299.007244	350367.456306	38.687796
2301.297926	350981.024628	38.692813
2303.175636	351593.383991	38.697831
2305.722406	352196.843878	38.702848
2307.685986	352785.750120	38.707866
2309.944880	353368.433224	38.712884
2311.813172	353953.431515	38.717901
2314.058754	354542.825320	38.722919
2316.064920	355139.812197	38.727936
2318.062244	355737.324973	38.732954
2320.270317	356331.394285	38.737972
2322.914109	356935.024893	38.742989
2324.467020	357553.061601	38.748007
2326.841864	358155.221945	38.753024
2328.714192	358788.080947	38.758042
2331.509691	359402.458807	38.763060
2333.438901	360038.612630	38.768077
2335.495751	360677.373858	38.773095
2337.792867	361318.469948	38.778112
2339.685264	361970.252831	38.783130
2342.532938	362625.012654	38.788148
2344.961031	363270.190657	38.793165
2347.294668	363923.136528	38.798183
2349.771799	364587.970847	38.803200
2352.051422	365250.289583	38.808218
2354.339030	365915.588918	38.813236
2356.450425	366575.401109	38.818253
2358.485834	367254.543826	38.823271
2361.056143	367935.741841	38.828288
2363.170713	368627.732615	38.833306
2365.779208	369308.949898	38.838324
2367.808989	369999.102742	38.843341
2370.069752	370708.075441	38.848359
2372.584876	371405.629200	38.853376
2374.654478	372116.533683	38.858394
2377.396460	372806.464492	38.863412
2380.188842	373518.159930	38.868429
2382.942453	374226.093959	38.873447
2385.373892	374926.103644	38.878464
2387.493273	375647.910638	38.883482
2390.432878	376348.872857	38.888500
2392.603448	377064.809060	38.893517
2394.856520	377766.211200	38.898535
2397.485385	378476.133376	38.903552
2399.790782	379185.536405	38.908570
2402.340425	379891.891906	38.913588
2404.719301	380621.919071	38.918605
2407.022123	381334.446816	38.923623
2409.694449	382048.673031	38.928640
2411.899385	382771.835603	38.933658
2414.468106	383493.096466	38.938676
2417.060522	384215.123451	38.943693
2419.280450	384923.352838	38.948711
2422.422733	385626.216565	38.953728
2425.675891	386333.508614	38.958746
2428.439303	387028.392785	38.963764
2431.406375	387717.016874	38.968781
2434.288977	388395.727647	38.973799
2437.192194	389076.499072	38.978816
2439.716107	389751.158398	38.983834
2442.289502	390417.328169	38.988852
2444.436312	391081.120702	38.993869
2446.732243	391753.822179	38.998887
2449.259104	392398.993641	39.003904
2451.658395	393077.782983	39.008922
2453.639260	393745.017603	39.013940
2456.155456	394410.906875	39.018957
2458.309514	395096.864272	39.023975
2460.751383	395766.740248	39.028992
2462.732709	396459.183140	39.034010
2465.167743	397136.708590	39.039028
2467.596159	397800.812961	39.044045
2469.537066	398465.363087	39.049063
2472.074115	399122.652903	39.054080
2474.220435	399786.226481	39.059098
2476.488279	400439.957744	39.064116
2479.023222	401102.169584	39.069133
2481.278098	401781.085957	39.074151
2483.999411	402448.759697	39.079168
2486.463717	403120.742424	39.084186
2488.547317	403795.888688	39.089204
2490.906881	404482.273433	39.094221
2492.684266	405178.998991	39.099239
2495.613618	405864.469882	39.104256
2497.790310	406578.702646	39.109274
2500.062186	407291.913042	39.114292
2502.745514	407998.145880	39.119309
2504.761677	408709.182832	39.124327
2507.457380	409440.456140	39.129344
2509.628991	410182.005154	39.134362
2512.125891	410918.641550	39.139380
2515.202814	411655.896198	39.144397
2517.088622	412401.534415	39.149415
2520.109496	413153.068055	39.154432
2522.325632	413907.828813	39.159450
2524.922039	414668.583513	39.164468
2527.467936	415418.560389	39.169485
2529.927812	416189.651868	39.174503
2532.811606	416940.744310	39.179520
2535.397573	417714.555008	39.184538
2537.830369	418482.112594	39.189556
2540.471683	419253.866778	39.194573
2542.796548	420017.344033	39.199591
2545.528771	420794.606959	39.204608
2548.129012	421578.375057	39.209626
2550.912655	422353.732538	39.214644
2553.770822	423136.244106	39.219661
2556.182898	423907.006299	39.224679
2559.312750	424682.638405	39.229696
2562.274411	425462.881397	39.234714
2564.670049	426241.319659	39.239732
2567.142653	427012.125595	39.244749
2569.857293	427789.043537	39.249767
2572.472099	428557.852493	39.254784
2575.508202	429336.843952	39.259802
2578.021512	430102.481074	39.264820
2580.736470	430861.377909	39.269837
2583.713073	431637.721719	39.274855
2586.603363	432393.553436	39.279872
2589.551897	433159.322644	39.284890
2591.962823	433922.624807	39.289908
2595.021711	434674.861934	39.294925
2597.178995	435439.117594	39.299943
2599.841879	436194.761531	39.304960
2602.134838	436969.268199	39.309978
2604.145702	437730.637298	39.314996
2606.866722	438501.124068	39.320013
2609.241343	439280.446870	39.325031
2611.654376	440064.239821	39.330048
2613.768879	440847.396873	39.335066
2616.376347	441633.885460	39.340084
2619.114868	442410.103909	39.345101
2621.458987	443222.636755	39.350119
2623.988321	444014.821124	39.355136
2627.079729	444809.312128	39.360154
2629.744333	445600.708214	39.365172
2632.690529	446394.659330	39.370189
2634.943020	447184.446832	39.375207
2637.961392	447981.008511	39.380224
2640.610650	448752.057799	39.385242
2643.631860	449502.279817	39.390260
2645.898414	450254.218680	39.395277
2648.363076	451012.015437	39.400295
2650.827710	451761.187223	39.405312
2653.379697	452518.358845	39.410330
2655.827630	453282.296722	39.415348
2658.850597	454033.115118	39.420365
2661.513064	454802.574681	39.425383
2664.374821	455547.347230	39.430400
2667.171842	456324.919202	39.435418
2669.981061	457084.257442	39.440436
2672.773152	457836.137946	39.445453
2675.139697	458614.856656	39.450471
2677.612586	459378.967701	39.455488
2680.427684	460160.636450	39.460506
2683.325692	460938.469628	39.465524
2686.755188	461703.951485	39.470541
2689.395625	462471.202548	39.475559
2692.661978	463236.955608	39.480576
2695.382797	464003.325231	39.485594
2697.367030	464793.339515	39.490612
2700.025193	465569.817333	39.495629
2702.679304	466361.577971	39.500647
2705.010173	467162.304727	39.505664
2707.162799	467962.370944	39.510682
2709.157503	468771.930094	39.515700
2711.564806	469598.011115	39.520717
2713.827397	470437.369133	39.525735
2716.057457	471265.377957	39.530752
2718.722396	472124.754489	39.535770
2721.252640	472984.821545	39.540788
2724.250765	473855.431255	39.545805
2726.542911	474737.281363	39.550823
2729.694509	475591.973434	39.555840
2732.735715	476466.394357	39.560858
2735.243847	477347.428338	39.565876
2738.315959	478241.913124	39.570893
2740.876221	479126.691801	39.575911
2744.252720	479998.919791	39.580928
2746.811102	480876.846768	39.585946
2749.965759	481764.529936	39.590964
2752.822273	482656.712794	39.595981
2755.763606	483544.495117	39.600999
2758.944528	484412.452607	39.606016
2762.711903	485271.637649	39.611034
2765.575645	486143.400266	39.616052
2768.329274	486995.399848	39.621069
2771.304705	487855.347799	39.626087
2774.031398	488711.256682	39.631104
2777.354370	489576.918040	39.636122
2779.921198	490420.352976	39.641140
2783.293111	491271.991695	39.646157
2785.907092	492118.162542	39.651175
2789.072357	492953.249878	39.656192
2792.144753	493797.496069	39.661210
2794.903537	494631.660600	39.666228
2798.026786	495461.081986	39.671245
2801.318316	496281.807303	39.676263
2803.639591	497124.196419	39.681280
2806.519148	497937.038981	39.686298
2809.123923	498765.778571	39.691316
2811.924329	499590.207445	39.696333
2814.243412	500429.404348	39.701351
2816.647021	501278.431094	39.706368
2819.270486	502116.735767	39.711386
2821.862409	502967.763020	39.716404
2824.627708	503820.684417	39.721421
2827.136917	504665.182132	39.726439
2829.814853	505486.714591	39.731456
2832.165200	506305.436037	39.736474
2834.609150	507139.529685	39.741492
2837.126658	507973.366462	39.746509
2840.032901	508814.254896	39.751527
2842.043468	509657.717729	39.756544
2844.749532	510508.532289	39.761562
2847.452095	511383.850833	39.766580
2849.743558	512251.779563	39.771597
2852.531761	513137.471476	39.776615
2854.986070	514027.251274	39.781632
2857.788850	514918.082186	39.786650
2860.703718	515832.781025	39.791668
2863.981988	516729.678872	39.796685
2867.436270	517650.027091	39.801703
2870.439752	518538.199093	39.806720
2873.409252	519459.325948	39.811738
2875.993375	520373.861702	39.816756
2879.076424	521295.212244	39.821773
2881.823315	522232.279170	39.826791
2884.472874	523150.818691	39.831808
2886.824436	524097.053614	39.836826
2889.629191	525044.413367	39.841844
2892.380482	526005.621786	39.846861
2895.038465	526969.906134	39.851879
2897.832707	527939.946719	39.856896
2900.890275	528904.895769	39.861914
2903.245751	529893.964134	39.866932
2906.366942	530881.983734	39.871949
2909.497792	531885.138181	39.876967
2912.481042	532876.721164	39.881984
2915.516658	533881.767852	39.887002
2918.504708	534892.540888	39.892020
2921.281186	535894.320245	39.897037
2923.939058	536914.467910	39.902055
2926.574389	537928.659526	39.907072
2930.381995	538932.673173	39.912090
2933.208941	539966.814810	39.917108
2936.723745	540967.211523	39.922125
2940.196305	541994.306851	39.927143
2943.206448	543000.830559	39.932160
2946.908945	543998.969091	39.937178
2949.768948	545007.234651	39.942196
2952.918282	546007.936455	39.947213
2955.824246	547003.829178	39.952231
2958.419691	548023.033129	39.957248
2961.715424	549018.012278	39.962266
2964.524717	550033.411927	39.967284
2967.429918	551038.314070	39.972301
2970.712402	552049.815802	39.977319
2973.874702	553043.468394	39.982336
2977.551232	554033.092941	39.987354
2980.760572	555018.299535	39.992372
2983.960513	556004.892892	39.997389
2987.418627	556985.843421	40.002407
2989.836237	557968.200409	40.007424
2993.100037	558953.711240	40.012442
2995.804921	559937.482934	40.017460
2998.908956	560913.781070	40.022477
3001.856096	561903.645567	40.027495
3004.451339	562887.767685	40.032512
3007.509166	563876.008340	40.037530
3010.085889	564871.987580	40.042548
3013.404351	565867.868269	40.047565
3016.470029	566843.880276	40.052583
3019.632550	567833.660062	40.057600
3022.755959	568820.859931	40.062618
3025.221245	569804.829576	40.067636
3028.057263	570763.664011	40.072653
3031.259595	571719.655251	40.077671
3033.206852	572685.769793	40.082688
3036.089172	573640.564921	40.087706
3038.834615	574622.810102	40.092724
3041.256502	575600.516051	40.097741
3044.327781	576596.602719	40.102759
3047.037952	577594.927319	40.107776
3050.438733	578580.867344	40.112794
3053.368264	579600.315097	40.117812
3056.274042	580619.030698	40.122829
3059.486160	581626.276742	40.127847
3062.369973	582654.958442	40.132864
3065.473348	583684.921475	40.137882
3068.079433	584725.960946	40.142900
3070.930877	585771.533438	40.147917
3073.784922	586817.967818	40.152935
3076.450167	587891.311534	40.157952
3079.251808	588975.965100	40.162970
3082.040990	590066.937848	40.167988
3084.520650	591170.591189	40.173005
3087.465272	592284.688584	40.178023
3090.360670	593418.631174	40.183040
3093.496064	594549.569672	40.188058
3096.048352	595694.272150	40.193076
3098.699894	596851.419209	40.198093
3101.926101	598018.373787	40.203111
3104.721036	599198.604089	40.208128
3107.527115	600386.874788	40.213146
3110.808269	601576.396911	40.218164
3114.134386	602789.118818	40.223181
3117.328577	603987.818051	40.228199
3120.368554	605201.383262	40.233216
3124.201455	606406.280013	40.238234
3127.352779	607606.857882	40.243252
3131.081376	608816.569959	40.248269
3134.892566	610027.889661	40.253287
3137.739557	611240.738919	40.258304
3141.145069	612448.812398	40.263322
3144.677990	613663.936199	40.268340
3147.411905	614859.855058	40.273357
3151.859382	616065.462421	40.278375
3155.252704	617252.962281	40.283392
3159.081704	618418.714113	40.288410
3162.466573	619601.611505	40.293428
3166.063783	620780.096904	40.298445
3169.971856	621943.059786	40.303463
3173.255671	623098.005332	40.308480
3176.676066	624251.005905	40.313498
3180.475479	625394.327400	40.318516
3184.417922	626516.071731	40.323533
3188.700849	627616.612238	40.328551
3192.134491	628727.568370	40.333568
3195.081744	629821.308772	40.338586
3198.447897	630919.011631	40.343604
3201.319445	632013.536386	40.348621
3204.152931	633106.405831	40.353639
3207.274379	634206.002834	40.358656
3210.899255	635279.943943	40.363674
3214.500447	636364.259457	40.368692
3217.664858	637438.752530	40.373709
3221.182340	638505.490901	40.378727
3224.504756	639575.793607	40.383744
3227.242650	640643.437468	40.388762
3230.847692	641704.391764	40.393780
3234.383957	642755.371232	40.398797
3237.967119	643805.586257	40.403815
3241.202375	644839.842022	40.408832
3244.091637	645857.644140	40.413850
3246.745650	646863.316734	40.418868
3249.241417	647880.331810	40.423885
3251.902723	648890.387292	40.428903
3254.699493	649918.112986	40.433920
3257.598718	650968.542320	40.438938
3259.983412	652014.660308	40.443956
3262.840436	653083.411493	40.448973
3265.594588	654169.253298	40.453991
3268.214721	655274.376841	40.459008
3270.900566	656382.354224	40.464026
3274.075092	657509.052069	40.469044
3276.644152	658643.588735	40.474061
3279.637191	659805.559239	40.479079
3281.975285	660970.536291	40.484096
3285.658896	662138.386817	40.489114
3289.025775	663327.850970	40.494132
3292.345416	664533.948524	40.499149
3296.107216	665711.456203	40.504167
3299.230113	666928.531602	40.509184
3302.338786	668150.379453	40.514202
3306.119204	669354.697872	40.519220
3309.385956	670588.791154	40.524237
3312.812545	671811.059577	40.529255
3316.572258	673035.501095	40.534272
3320.190854	674253.591332	40.539290
3323.852914	675481.855943	40.544308
3326.855029	676702.761098	40.549325
3330.418720	677946.622598	40.554343
3333.634127	679186.647726	40.559360
3336.509560	680436.052524	40.564378
3340.153767	681690.277605	40.569396
3343.059610	682957.864726	40.574413
3346.422357	684219.389788	40.579431
3349.402408	685495.998929	40.584448
3352.826301	686770.120998	40.589466
3355.675978	688060.044830	40.594484
3358.960358	689367.035768	40.599501
3362.527479	690668.975935	40.604519
3365.945705	691967.823853	40.609536
3369.567869	693266.300363	40.614554
3373.554816	694556.887537	40.619572
3377.311030	695866.967081	40.624589
3380.936637	697150.787919	40.629607
3384.484440	698448.616339	40.634624
3387.829107	699744.551358	40.639642
3391.433260	701038.566281	40.644660
3394.803042	702334.113286	40.649677
3398.950487	703623.590238	40.654695
3402.475774	704914.662934	40.659712
3405.291544	706208.929838	40.664730
3408.318791	707502.818793	40.669748
3411.052944	708825.039374	40.674765
3414.056542	710142.950627	40.679783
3417.059682	711464.272759	40.684800
3420.429178	712808.447413	40.689818
3423.166268	714143.554630	40.694836
3427.313444	715483.265630	40.699853
3430.868043	716809.501660	40.704871
3434.516574	718151.937465	40.709888
3438.039877	719490.122419	40.714906
3441.718292	720826.286511	40.719924
3445.046646	722174.606319	40.724941
3448.558903	723513.381428	40.729959
3452.012453	724852.789495	40.734976
3455.582814	726177.973096	40.739994
3459.430213	727524.590675	40.745012
3462.965060	728830.600247	40.750016
3466.408742	730082.029600	40.755021
3469.756032	731307.135700	40.760026
3472.499332	732460.709713	40.765031
3475.786311	733544.918906	40.770036
3478.514994	734571.803371	40.775040
3482.188884	735513.865113	40.780045
3485.164124	736398.277653	40.785050
3487.735350	737211.997050	40.790055
3490.603684	737947.754418	40.795060
3493.145283	738626.156839	40.800064
3495.195110	739227.507242	40.805069
3497.797688	739780.044862	40.810074
3499.501956	740275.907439	40.815079
3501.416771	740709.481545	40.820084
3503.112568	741095.933477	40.825088
3504.718581	741425.357310	40.830093
3505.846637	741707.913238	40.835098
3507.350508	741948.163334	40.840103
3508.562462	742147.013035	40.845108
3509.215874	742313.757010	40.850112
3510.631572	742439.426217	40.855117
3511.896598	742527.239407	40.860122
3512.564875	742577.864962	40.865127
3513.699815	742605.765054	40.870132
3514.611702	742603.043019	40.875136
3515.105937	742563.796968	40.880141
3515.915574	742521.927181	40.885146
3516.627644	742434.133480	40.890151
3517.386648	742328.726289	40.895156
3517.643559	742210.345250	40.900160
3518.431384	742062.252237	40.905165
3518.398645	741901.928486	40.910170
3519.016754	741734.372363	40.915175
3519.882371	741538.878339	40.920180
3519.824248	741341.009791	40.925184
3520.205170	741124.763879	40.930189
3520.453807	740889.095922	40.935194
3520.584962	740650.719957	40.940199
3520.886994	740400.041606	40.945204
3521.059973	740140.373984	40.950208
3521.145032	739858.650124	40.955213
3521.445369	739589.989921	40.960218
3521.413352	739305.594490	40.965223
3522.108579	739013.697342	40.970228
3521.946613	738719.061648	40.975232
3521.911130	738410.887201	40.980237
3522.014043	738108.961667	40.985242
3522.146599	737789.850298	40.990247
3522.470461	737465.647407	40.995252
3522.204020	737150.881365	41.000256
3522.086766	736820.143827	41.005261
3522.144545	736501.141814	41.010266
3522.105252	736170.364540	41.015271
3522.062471	735824.974044	41.020276
3522.069157	735492.379481	41.025280
3522.156788	735153.917211	41.030285
3521.968815	734820.733039	41.035290
3521.660302	734484.584956	41.040295
3522.070912	734151.917662	41.045300
3521.767774	733816.433815	41.050304
3521.570303	733470.571673	41.055309
3521.415876	733125.380704	41.060314
3521.153248	732795.392646	41.065319
3521.124462	732451.637430	41.070324
3520.768819	732113.516791	41.075328
3521.359123	731784.534876	41.080333
3521.081142	731453.999447	41.085338
3520.609122	731124.225411	41.090343
3520.491627	730776.253962	41.095348
3520.255817	730455.872613	41.100352
3519.950803	730123.900749	41.105357
3520.165562	729799.952189	41.110362
3519.616582	729468.390109	41.115367
3520.090361	729139.815621	41.120372
3519.970031	728815.387938	41.125376
3519.745511	728499.435377	41.130381
3519.635508	728166.212135	41.135386
3519.320888	727853.370409	41.140391
3519.473577	727532.463104	41.145396
3519.399974	727219.111397	41.150400
3519.349262	726901.086537	41.155405
3519.195625	726586.683380	41.160410
3518.838537	726266.107988	41.165415
3518.769705	725948.792438	41.170420
3518.858447	725639.317708	41.175424
3518.449924	725321.984526	41.180429
3518.095291	725013.352397	41.185434
3517.857540	724708.654160	41.190439
3518.368639	724400.500270	41.195444
3517.845643	724108.861694	41.200448
3518.126620	723802.656468	41.205453
3517.878052	723499.997091	41.210458
3517.687396	723210.056245	41.215463
3517.678338	722901.337533	41.220468
3517.217124	722613.948596	41.225472
3517.243696	722308.324932	41.230477
3517.196063	722018.913603	41.235482
3516.642910	721731.558817	41.240487
3516.980287	721440.030979	41.245492
3516.812467	721157.897642	41.250496
3516.481949	720876.674098	41.255501
3516.258189	720584.713153	41.260506
3516.165183	720313.496959	41.265511
3516.161811	720027.479960	41.270516
3516.102444	719761.397358	41.275520
3515.987179	719498.142186	41.280525
3515.696114	719214.227647	41.285530
3515.873268	718949.865409	41.290535
3515.720671	718675.332559	41.295540
3515.445979	718409.341631	41.300544
3515.233910	718145.663046	41.305549
3515.230706	717881.247228	41.310554
3515.040937	717606.288634	41.315559
3515.071777	717359.112253	41.320564
3515.138104	717104.481954	41.325568
3515.216417	716835.604825	41.330573
3514.856096	716582.269358	41.335578
3514.462806	716335.182522	41.340583
3514.630762	716068.448853	41.345588
3514.276260	715824.565333	41.350592
3513.843668	715567.887189	41.355597
3514.012931	715323.307220	41.360602
3513.997237	715083.365110	41.365607
3513.951295	714843.917357	41.370612
3513.847825	714599.659185	41.375616
3513.681249	714362.301739	41.380621
3513.510513	714132.877941	41.385626
3513.144673	713897.376401	41.390631
3513.281424	713663.571759	41.395636
3512.900165	713440.019748	41.400640
3512.930940	713210.885028	41.405645
3512.976994	712985.017126	41.410650
3512.682471	712772.252356	41.415655
3512.848409	712541.191233	41.420660
3512.769358	712319.296835	41.425664
3512.605234	712098.453023	41.430669
3512.605112	711875.690204	41.435674
3512.157135	711668.432705	41.440679
3512.251536	711434.871461	41.445684
3512.115497	711230.182569	41.450688
3512.294012	711017.246032	41.455693
3511.901161	710800.179013	41.460698
3511.800237	710597.405155	41.465703
3511.828553	710385.371233	41.470708
3511.487922	710183.768977	41.475712
3511.325571	709976.224512	41.480717
3511.465076	709779.994537	41.485722
3511.042176	709584.001945	41.490727
3511.004819	709379.500578	41.495732
3511.138279	709196.018344	41.500736
3511.110469	708994.336327	41.505741
3510.954623	708811.837067	41.510746
3510.984644	708614.506071	41.515751
3511.051526	708423.619717	41.520756
3510.572705	708229.194328	41.525760
3510.426557	708036.894513	41.530765
3510.487811	707852.253302	41.535770
3510.298267	707672.218315	41.540775
3510.298413	707491.452948	41.545780
3510.198002	707306.826729	41.550784
3510.316316	707127.375062	41.555789
3510.211682	706946.863878	41.560794
3509.768275	706769.235826	41.565799
3509.529587	706597.132925	41.570804
3509.417797	706424.856611	41.575808
3509.483752	706261.140123	41.580813
3509.475103	706089.138063	41.585818
3509.076900	705928.472129	41.590823
3509.578951	705766.064946	41.595828
3509.358776	705596.571586	41.600832
3509.380677	705430.462347	41.605837
3509.128910	705258.285212	41.610842
3508.816924	705111.796641	41.615847
3509.125431	704946.177154	41.620852
3509.113418	704791.337683	41.625856
3508.959382	704624.695589	41.630861
3508.756853	704476.737513	41.635866
3508.590975	704326.733989	41.640871
3508.919295	704168.597964	41.645876
3508.973120	704006.629269	41.650880
3508.347403	703848.247610	41.655885
3508.508056	703696.291284	41.660890
3508.288513	703555.524346	41.665895
3508.397368	703403.124291	41.670900
3508.115058	703255.705089	41.675904
3508.277403	703121.078707	41.680909
3508.189680	702972.678501	41.685914
3508.162710	702826.153872	41.690919
3508.285664	702691.527347	41.695924
3507.952753	702543.160329	41.700928
3507.797981	702398.835970	41.705933
3507.951889	702256.445862	41.710938
3507.497402	702130.850539	41.715943
3507.663964	701985.919617	41.720948
3507.507779	701849.934805	41.725952
3507.569875	701723.701610	41.730957
3507.426249	701577.821276	41.735962
3507.076468	701461.541706	41.740967
3507.442011	701332.121851	41.745972
3507.322458	701200.643256	41.750976
3506.944885	701072.336305	41.755981
3506.934302	700947.296644	41.760986
3506.839486	700825.300788	41.765991
3506.704599	700692.922490	41.770996
3506.495544	700576.061163	41.776000
3506.329898	700470.721874	41.781005
3506.732071	700348.090509	41.786010
3506.630671	700231.505001	41.791015
3506.470547	700119.102745	41.796020
3506.587075	699998.452128	41.801024
3506.309369	699883.531361	41.806029
3506.719684	699770.085962	41.811034
3506.425548	699656.904631	41.816039
3506.095524	699534.830239	41.821044
3506.192468	699440.917448	41.826048
3506.204972	699324.599289	41.831053
3506.324826	699215.867282	41.836058
3506.030116	699110.731799	41.841063
3505.882805	699004.029690	41.846068
3505.928768	698904.850336	41.851072
3505.867687	698807.079461	41.856077
3506.161078	698689.463691	41.861082
3505.793050	698597.905459	41.866087
3505.898122	698489.067472	41.871092
3505.852462	698380.650755	41.876096
3505.729925	698275.874529	41.881101
3505.749851	698177.337551	41.886106
3505.250958	698084.801307	41.891111
3505.442027	697976.439916	41.896116
3505.655019	697881.496965	41.901120
3505.202668	697773.885723	41.906125
3505.288623	697690.098270	41.911130
3505.021318	697601.496055	41.916135
3505.317405	697506.535331	41.921140
3505.506823	697420.242297	41.926144
3505.495793	697322.297493	41.931149
3505.339902	697223.381141	41.936154
3505.330335	697128.765182	41.941159
3505.172585	697031.686644	41.946164
3505.094608	696944.190116	41.951168
3505.220805	696863.023396	41.956173
3505.232196	696772.527078	41.961178
3504.957418	696684.811889	41.966183
3504.793853	696586.436617	41.971188
3504.888634	696501.343603	41.976192
3504.880580	696412.587150	41.981197
3505.047820	696321.414036	41.986202
3504.617729	696245.306075	41.991207
3504.734357	696152.548367	41.996212
3504.681574	696073.840549	42.001216
3504.750017	695992.128384	42.006221
3504.653491	695905.668900	42.011226
3504.444104	695836.283864	42.016231
3504.529073	695757.252097	42.021236
3504.722698	695691.976496	42.026240
3504.346000	695613.566757	42.031245
3504.396602	695521.708471	42.036250
3504.296897	695448.870932	42.041255
3504.265784	695371.247343	42.046260
3504.331547	695294.900066	42.051264
3504.504187	695225.546570	42.056269
3504.714662	695133.110793	42.061274
3504.156006	695071.784287	42.066279
3503.957743	694992.394649	42.071284
3504.295173	694925.448466	42.076288
3504.063740	694856.855124	42.081293
3503.999090	694774.606659	42.086298
3503.828625	694708.538514	42.091303
3504.139702	694637.168177	42.096308
3503.784560	694576.650097	42.101312
3503.810807	694504.082390	42.106317
3504.321644	694432.030835	42.111322
3503.696222	694363.598261	42.116327
3503.982838	694297.003892	42.121332
3504.009322	694239.404628	42.126336
3503.921888	694165.261365	42.131341
3503.780473	694099.532047	42.136346
3503.630298	694036.638749	42.141351
3503.522328	693958.717079	42.146356
3503.512391	693902.166153	42.151360
3503.494037	693841.736621	42.156365
3503.607167	693782.976085	42.161370
3503.349482	693729.051443	42.166375
3503.633631	693667.824644	42.171380
3503.347035	693599.330185	42.176384
3503.319821	693544.172567	42.181389
3503.544380	693486.485952	42.186394
3503.339482	693432.152859	42.191399
3503.388671	693374.395018	42.196404
3503.453460	693308.327326	42.201408
3503.081931	693253.075580	42.206413
3503.053088	693196.473552	42.211418
3502.950043	693147.941768	42.216423
3502.912381	693089.699006	42.221428
3503.057228	693052.019476	42.226432
3502.895092	692987.031514	42.231437
3502.820564	692930.186626	42.236442
3503.041791	692883.092131	42.241447
3502.957171	692836.644868	42.246452
3502.989007	692793.113060	42.251456
3502.670250	692737.152964	42.256461
3502.637319	692677.613355	42.261466
3502.706037	692655.813516	42.266471
3502.974742	692606.570657	42.271476
3502.899310	692559.573228	42.276480
3503.015915	692514.135698	42.281485
3502.905408	692466.148646	42.286490
3502.888356	692412.226009	42.291495
3502.674395	692355.649237	42.296500
3502.728159	692321.613224	42.301504
3502.781387	692277.627640	42.306509
3503.074658	692227.035442	42.311514
3502.716598	692180.729449	42.316519
3502.373250	692123.874101	42.321524
3502.778446	692098.385652	42.326528
3502.688664	692054.870344	42.331533
3502.812367	691999.329987	42.336538
3502.702621	691959.648204	42.341543
3502.781696	691900.632147	42.346548
3502.465325	691856.058822	42.351552
3502.373760	691822.094674	42.356557
3502.682624	691776.571871	42.361562
3502.246971	691750.325883	42.366567
3502.522117	691697.843164	42.371572
3502.440560	691659.150406	42.376576
3502.287494	691615.643417	42.381581
3502.727712	691578.505876	42.386586
3502.529044	691540.826991	42.391591
3502.673438	691495.678204	42.396596
3502.385589	691452.242446	42.401600
3502.105769	691426.318018	42.406605
3502.571633	691376.737291	42.411610
3502.510184	691333.014776	42.416615
3502.330139	691291.252021	42.421620
3502.170295	691249.535485	42.426624
3502.238262	691214.199322	42.431629
3502.365571	691175.370448	42.436634
3502.326577	691138.061508	42.441639
3502.230836	691103.249503	42.446644
3502.298732	691054.976621	42.451648
3501.502611	691040.729184	42.456653
3502.168468	691006.736277	42.461658
3502.112929	690974.603883	42.466663
3502.116231	690944.302589	42.471668
3502.035352	690904.909886	42.476672
3501.924462	690876.418425	42.481677
3502.395062	690832.705051	42.486682
3502.204740	690806.515257	42.491687
3502.516039	690769.694209	42.496692
3502.281736	690728.286087	42.501696
3501.920596	690701.328113	42.506701
3502.505506	690650.081735	42.511706
3502.318478	690623.791348	42.516711
3502.239497	690577.281657	42.521716
3502.461927	690549.231642	42.526720
3502.235483	690515.483856	42.531725
3502.426007	690469.575915	42.536730
3502.342103	690437.048221	42.541735
3502.224443	690393.380168	42.546740
3502.455727	690349.305928	42.551744
3502.203233	690320.786344	42.556749
3502.342565	690284.937140	42.561754
3502.054859	690245.525963	42.566759
3501.921659	690209.422943	42.571764
3502.202429	690194.399072	42.576768
3502.138293	690158.334192	42.581773
3502.402986	690116.144146	42.586778
3502.129159	690077.227532	42.591783
3502.186521	690052.089318	42.596788
3501.901893	690006.058492	42.601792
3501.777186	689981.547294	42.606797
3501.949178	689947.084637	42.611802
3501.723257	689920.699095	42.616807
3501.829687	689893.611659	42.621812
3502.110189	689865.948002	42.626816
3501.920156	689828.559055	42.631821
3502.199255	689795.521194	42.636826
3501.830290	689775.528329	42.641831
3501.565056	689742.182137	42.646836
3501.616164	689705.648538	42.651840
3501.650515	689684.394531	42.656845
3502.138051	689661.323902	42.661850
3502.000897	689631.539010	42.666855
3502.156720	689601.357264	42.671860
3502.329873	689551.765078	42.676864
3501.996924	689525.794165	42.681869
3502.118370	689488.999248	42.686874
3501.906306	689465.098235	42.691879
3501.861321	689436.541547	42.696884
3502.137526	689410.171050	42.701888
3501.837364	689372.350532	42.706893
3501.867280	689333.032149	42.711898
3501.700686	689312.308112	42.716903
3501.757603	689290.452275	42.721908
3501.621366	689258.625661	42.726912
3501.760272	689241.682833	42.731917
3501.628608	689207.167997	42.736922
3501.530680	689186.432321	42.741927
3501.691296	689160.727139	42.746932
3501.399793	689137.833682	42.751936
3501.471103	689116.671757	42.756941
3501.879198	689085.152694	42.761946
3501.635211	689064.291578	42.766951
3501.552726	689036.137941	42.771956
3501.251925	689011.354603	42.776960
3501.574637	689002.890898	42.781965
3501.800471	688967.071914	42.786970
3501.747715	688955.833551	42.791975
3501.921039	688919.027732	42.796980
3501.781460	688890.634243	42.801985
3501.682960	688868.156102	42.806989
3501.679675	688837.400892	42.811994
3501.669644	688805.452284	42.816999
3501.600686	688783.217884	42.822004
3501.603439	688754.402307	42.827009
3501.417980	688732.585172	42.832013
3501.730799	688697.696323	42.837018
3501.469851	688691.120414	42.842023
3501.719598	688652.658548	42.847028
3501.654359	688638.485552	42.852033
3501.175186	688614.925029	42.857037
3501.521982	688604.864397	42.862042
3501.608450	688575.735806	42.867047
3501.610578	688563.193909	42.872052
3501.470565	688527.632713	42.877057
3501.156691	688519.721677	42.882061
3501.326892	688493.515324	42.887066
3501.169204	688468.756609	42.892071
3501.294241	688456.194251	42.897076
3501.580462	688435.841282	42.902081
3501.397283	688421.986050	42.907085
3501.474079	688395.446466	42.912090
3501.455927	688377.433049	42.917095
3501.302637	688357.749769	42.922100
3501.582138	688325.403226	42.927105
3501.197231	688308.047516	42.932109
3501.584084	688289.469295	42.937114
3501.448972	688266.050076	42.942119
3501.324434	688247.805132	42.947124
3501.278481	688220.389458	42.952129
3501.281126	688211.629519	42.957133
3501.457448	688190.497836	42.962138
3501.623578	688164.589823	42.967143
3501.149294	688147.646738	42.972148
3501.491289	688122.356558	42.977153
3501.310659	688102.030219	42.982157
3501.676590	688081.563738	42.987162
3501.772595	688055.268834	42.992167
3501.474651	688025.505201	42.997172
3501.438957	688002.765666	43.002177
3501.165246	688002.810950	43.007181
3501.147022	687964.689068	43.012186
3501.352091	687950.221461	43.017191
3501.082578	687945.537743	43.022196
3501.345315	687914.785196	43.027201
3501.045944	687909.359816	43.032205
3501.342211	687894.329557	43.037210
3501.244032	687878.866740	43.042215
3501.243182	687860.401483	43.047220
3501.607594	687843.866714	43.052225
3501.079926	687829.868414	43.057229
3501.109992	687811.845899	43.062234
3501.186925	687792.272655	43.067239
3501.121621	687768.741064	43.072244
3501.075653	687757.002357	43.077249
3500.786798	687761.081734	43.082253
3501.380706	687732.712699	43.087258
3501.323580	687724.509666	43.092263
3500.976471	687706.300409	43.097268
3501.009568	687672.598608	43.102273
3500.978881	687666.730493	43.107277
3501.213450	687651.262069	43.112282
3501.103747	687645.108358	43.117287
3501.016992	687629.294812	43.122292
3501.314455	687615.060267	43.127297
3501.001155	687602.370069	43.132301
3501.320778	687579.670296	43.137306
3501.254755	687567.337373	43.142311
3501.157136	687557.548120	43.147316
3501.050178	687528.647213	43.152321
3500.972775	687521.492601	43.157325
3501.155528	687511.159222	43.162330
3501.156840	687488.113632	43.167335
3501.037529	687477.929683	43.172340
3501.160699	687465.913776	43.177345
3501.225381	687456.097590	43.182349
3501.102733	687425.207971	43.187354
3501.488880	687420.415623	43.192359
3501.270750	687400.492097	43.197364
3501.030879	687380.572121	43.202369
3500.706254	687371.019280	43.207373
3501.283749	687357.733550	43.212378
3501.215123	687332.061048	43.217383
3501.020248	687319.948182	43.222388
3501.092538	687298.931160	43.227393
3500.955803	687287.754372	43.232397
3501.171027	687268.007813	43.237402
3501.066074	687273.898705	43.242407
3500.979811	687260.274548	43.247412
3500.746309	687235.923183	43.252417
3500.588303	687228.930986	43.257421
3501.089863	687209.385858	43.262426
3501.136539	687213.808234	43.267431
3500.817076	687187.629243	43.272436
3501.140034	687172.593378	43.277441
3500.870297	687172.488678	43.282445
3500.952023	687157.393101	43.287450
3500.967512	687137.977924	43.292455
3500.662893	687113.438878	43.297460
3500.988984	687118.113781	43.302465
3500.830614	687127.000170	43.307469
3500.831564	687097.980501	43.312474
3501.000334	687095.463843	43.317479
3500.786586	687067.923073	43.322484
3501.094122	687061.252022	43.327489
3501.045453	687071.215419	43.332493
3500.764096	687039.803170	43.337498
3500.910169	687031.565927	43.342503
3500.904125	687020.317433	43.347508
3500.912980	687011.605081	43.352513
3501.050446	687004.016334	43.357517
3500.911816	686988.210239	43.362522
3500.997346	686984.960653	43.367527
3500.623724	686984.425125	43.372532
3500.858938	686971.892276	43.377537
3500.735815	686954.440917	43.382541
3500.788773	686931.733814	43.387546
3500.699996	686928.114795	43.392551
3500.517056	686924.660669	43.397556
3500.971897	686919.159825	43.402561
3500.452739	686919.992332	43.407565
3500.668562	686916.621634	43.412570
3500.709373	686898.296860	43.417575
3500.390677	686882.371006	43.422580
3500.723968	686864.396047	43.427585
3500.598367	686873.526157	43.432589
3500.486099	686861.150135	43.437594
3500.671217	686856.689381	43.442599
3500.973838	686860.074079	43.447604
3500.629852	686858.986091	43.452609
3500.584969	686855.061124	43.457613
3500.872583	686828.681211	43.462618
3500.989446	686823.285942	43.467623
3501.001250	686827.714270	43.472628
3500.980748	686825.328373	43.477633
3500.815362	686800.168132	43.482637
3500.808435	686781.452786	43.487642
3500.758910	686773.148078	43.492647
3500.834409	686764.225362	43.497652
3500.776794	686766.873177	43.502657
3500.935139	686759.280775	43.507661
3500.935326	686726.526676	43.512666
3500.874657	686721.409577	43.517671
3500.682322	686726.319697	43.522676
3501.155733	686712.900893	43.527681
3500.741444	686702.565706	43.532685
3500.996629	686680.969460	43.537690
3500.866888	686680.393608	43.542695
3500.394158	686674.797016	43.547700
3500.830207	686675.919693	43.552705
3500.683514	686663.200639	43.557709
3500.893339	686643.154940	43.562714
3500.947614	686638.018799	43.567719
3500.610824	686626.028013	43.572724
3501.127104	686625.594289	43.577729
3500.628048	686610.643562	43.582733
3500.942059	686591.227658	43.587738
3500.860034	686583.575275	43.592743
3500.668979	686589.480840	43.597748
3500.892028	686581.031351	43.602753
3500.581400	686569.185503	43.607757
3500.810851	686546.796723	43.612762
3500.662188	686540.648698	43.617767
3500.637792	686534.380573	43.622772
3501.017442	686531.928468	43.627777
3500.554204	686530.213014	43.632781
3500.379033	686524.119137	43.637786
3501.123301	686530.766198	43.642791
3501.031378	686498.325173	43.647796
3501.090127	686484.128306	43.652801
3501.008309	686484.639675	43.657805
3500.947771	686472.802151	43.662810
3500.844586	686449.273387	43.667815
3501.024236	686443.967077	43.672820
3500.818654	686435.687849	43.677825
3500.675568	686432.177167	43.682829
3500.981200	686425.456185	43.687834
3501.105224	686396.165028	43.692839
3500.795831	686389.296760	43.697844
3500.966029	686390.811870	43.702849
3500.790648	686388.949256	43.707853
3500.681254	686365.371520	43.712858
3501.070643	686337.728853	43.717863
3500.501411	686347.579953	43.722868
3500.587802	686337.808750	43.727873
3500.684239	686343.467841	43.732877
3500.688350	686339.335430	43.737882
3500.581475	686325.962175	43.742887
3500.529675	686306.755460	43.747892
3500.794134	686285.455425	43.752897
3500.731684	686297.711867	43.757901
3500.573521	686292.262173	43.762906
3500.581339	686287.730880	43.767911
3500.782743	686291.530767	43.772916
3500.981999	686295.978157	43.777921
3500.477369	686281.973640	43.782925
3500.636026	686264.125917	43.787930
3500.582724	686255.672015	43.792935
3500.481451	686262.508793	43.797940
3500.315155	686253.077944	43.802945
3500.547468	686256.026461	43.807949
3500.433898	686260.625128	43.812954
3500.827166	686253.192604	43.817959
3500.452131	686257.734921	43.822964
3500.693140	686248.485660	43.827969
3500.862600	686228.943527	43.832973
3500.839985	686205.301253	43.837978
3500.709526	686203.530739	43.842983
3500.375958	686209.161415	43.847988
3500.860296	686199.075391	43.852993
3500.475831	686201.926730	43.857997
3500.765209	686202.874583	43.863002
3500.904881	686183.138150	43.868007
3500.587098	686180.502524	43.873012
3500.886677	686159.146608	43.878017
3500.623173	686160.036491	43.883021
3500.664596	686160.676856	43.888026
3500.658363	686157.541702	43.893031
3500.591406	686156.407843	43.898036
3500.556438	686126.046896	43.903041
3500.250339	686122.015435	43.908045
3500.381249	686114.576374	43.913050
3500.716976	686113.127053	43.918055
3500.769973	686117.100884	43.923060
3500.467803	686107.443429	43.928065
3500.482790	686115.854121	43.933069
3500.568046	686104.539620	43.938074
3500.696203	686109.098416	43.943079
3500.615809	686115.931854	43.948084
3500.642242	686099.499547	43.953089
3500.402770	686078.979255	43.958093
3500.614470	686066.200133	43.963098
3500.585002	686068.594590	43.968103
3500.558901	686072.083694	43.973108
3500.441491	686064.237592	43.978113
3500.436763	686064.039296	43.983117
3500.361291	686065.047459	43.988122
3500.547014	686062.278806	43.993127
3500.365445	686067.834667	43.998132
3500.741207	686062.794417	44.003137
3500.676458	686069.077702	44.008141
3500.748638	686052.139929	44.013146
3500.462043	686031.926010	44.018151
3500.478883	686027.094403	44.023156
3500.627538	686028.314443	44.028161
3500.557615	686026.782800	44.033165
3500.793140	686019.973542	44.038170
3500.701017	686019.142519	44.043175
3500.506379	686026.890984	44.048180
3501.019698	686020.832333	44.053185
3500.586069	686000.343950	44.058189
3500.754188	685977.615426	44.063194
3500.931050	685974.250820	44.068199
3500.717076	685976.078403	44.073204
3500.520179	685969.639265	44.078209
3500.584085	685982.522424	44.083213
3500.634261	685959.464869	44.088218
3500.928037	685949.509628	44.093223
3500.686268	685933.121344	44.098228
3500.807087	685924.339661	44.103233
3500.465686	685942.815746	44.108237
3500.819375	685931.108188	44.113242
3501.086064	685918.170423	44.118247
3500.732117	685898.913212	44.123252
3500.665742	685888.420028	44.128257
3500.556067	685887.442544	44.133261
3500.422817	685886.966786	44.138266
3500.658718	685879.261267	44.143271
3500.449817	685882.531738	44.148276
3500.764116	685877.352194	44.153281
3500.668143	685884.636428	44.158285
3500.579331	685867.376436	44.163290
3500.794784	685843.693876	44.168295
3500.469797	685834.039899	44.173300
3500.829742	685837.963126	44.178305
3500.605858	685841.435221	44.183309
3500.787794	685839.513441	44.188314
3500.958596	685836.199569	44.193319
3500.640860	685816.537932	44.198324
3500.583829	685803.952204	44.203329
3500.333998	685800.757617	44.208333
3500.814291	685802.669632	44.213338
3501.051364	685787.645671	44.218343
3500.842603	685795.595801	44.223348
3500.828990	685770.706320	44.228353
3500.812894	685755.773929	44.233357
3500.820947	685748.603791	44.238362
3500.894605	685751.927180	44.243367
3500.706644	685744.341379	44.248372
3501.008815	685727.862831	44.253377
3500.782079	685714.458698	44.258381
3500.700969	685701.179832	44.263386
3500.804135	685698.275360	44.268391
3500.446214	685704.607347	44.273396
3500.776240	685699.076615	44.278401
3500.885283	685696.071604	44.283405
3500.521534	685657.100996	44.288410
3500.864331	685655.700221	44.293415
3500.762509	685658.803722	44.298420
3500.986985	685647.863919	44.303425
3500.795464	685653.172756	44.308429
3500.720923	685632.225921	44.313434
3500.414365	685612.910485	44.318439
3500.384406	685619.636392	44.323444
3500.609030	685605.211600	44.328449
3500.526904	685603.582334	44.333453
3500.557098	685603.627179	44.338458
3500.731554	685609.124482	44.343463
3500.846575	685615.975785	44.348468
3501.008739	685603.901184	44.353473
3500.846092	685579.483869	44.358477
3500.806472	685565.301822	44.363482
3500.723263	685562.378323	44.368487
3501.024162	685569.348297	44.373492
3500.752093	685556.150561	44.378497
3500.561989	685543.984743	44.383501
3500.622203	685540.937965	44.388506
3500.547893	685529.748688	44.393511
3500.213834	685533.189323	44.398516
3500.412275	685524.195286	44.403521
3500.667378	685535.006298	44.408525
3500.530200	685530.697729	44.413530
3500.681920	685529.228943	44.418535
3500.637209	685539.392508	44.423540
3500.706024	685524.943554	44.428545
3500.732125	685511.298197	44.433549
3500.696365	685497.463902	44.438554
3500.955587	685481.489857	44.443559
3500.676574	685483.378071	44.448564
3500.850269	685485.788892	44.453569
3501.041699	685481.874060	44.458573
3501.030979	685452.602129	44.463578
3500.871674	685440.729795	44.468583
3500.596980	685445.206145	44.473588
3500.757916	685442.491186	44.478593
3500.804459	685427.547904	44.483597
3500.815752	685419.381261	44.488602
3500.731977	685396.443985	44.493607
3500.751189	685405.302708	44.498612
3500.940308	685396.409658	44.503617
3500.791893	685393.148380	44.508621
3500.370195	685367.628235	44.513626
3501.036326	685355.370447	44.518631
3500.775166	685354.666869	44.523636
3500.778447	685359.943682	44.528641
3500.818708	685356.800568	44.533645
3500.858120	685352.661875	44.538650
3500.860275	685322.142748	44.543655
3500.549412	685312.286736	44.548660
3500.827256	685314.730176	44.553665
3500.887527	685306.704696	44.558669
3500.657274	685308.087025	44.563674
3500.823768	685304.126453	44.568679
3500.439780	685283.429098	44.573684
3500.764782	685273.119454	44.578689
3500.814779	685266.639014	44.583693
3500.836747	685264.146114	44.588698
3501.028428	685254.306560	44.593703
3500.610809	685242.825161	44.598708
3500.775173	685223.829363	44.603713
3500.992347	685222.648431	44.608717
3500.626099	685212.901036	44.613722
3500.743168	685209.147737	44.618727
3500.671747	685219.017354	44.623732
3500.615218	685210.563012	44.628737
3500.722073	685180.872482	44.633741
3500.916716	685170.783413	44.638746
3500.970884	685163.854128	44.643751
3500.968341	685170.127753	44.648756
3500.793737	685151.436758	44.653761
3500.880123	685137.432368	44.658765
3500.664967	685125.070979	44.663770
3501.035291	685109.028134	44.668775
3500.721967	685110.075711	44.673780
3500.997706	685105.599126	44.678785
3500.845888	685094.123399	44.683789
3500.604691	685075.891339	44.688794
3501.213028	685071.957221	44.693799
3500.830596	685074.011971	44.698804
3500.999610	685064.275533	44.703809
3500.556298	685043.786586	44.708813
3500.815272	685040.905943	44.713818
3500.825855	685023.378983	44.718823
3500.653521	685027.987983	44.723828
3500.758131	685019.307682	44.728833
3500.801749	684995.750890	44.733837
3500.584309	684980.004105	44.738842
3500.975264	684983.574066	44.743847
3500.520766	684987.532687	44.748852
3500.517485	684991.665676	44.753857
3500.559890	684983.642864	44.758861
3500.549939	684981.901981	44.763866
3500.941244	684985.919975	44.768871
3500.658637	684958.035659	44.773876
3500.689607	684947.774241	44.778881
3500.827023	684943.519589	44.783885
3500.534749	684939.087006	44.788890
3500.894599	684940.869750	44.793895
3500.647014	684936.230627	44.798900
3500.803280	684920.372191	44.803905
3500.893548	684907.661302	44.808909
3500.829616	684899.008740	44.813914
3500.937959	684901.629670	44.818919
3500.532174	684905.480699	44.823924
3500.739348	684884.883892	44.828929
3500.786899	684862.869548	44.833933
3500.690005	684854.919432	44.838938
3500.838930	684854.098253	44.843943
3500.730217	684856.555913	44.848948
3500.886175	684845.078796	44.853953
3500.692112	684842.173385	44.858957
3500.928832	684832.574876	44.863962
3501.046050	684812.291504	44.868967
3500.737871	684822.499411	44.873972
3500.701207	684803.187437	44.878977
3501.089975	684803.222817	44.883981
3500.780644	684781.914513	44.888986
3500.972657	684765.701377	44.893991
3500.622643	684770.489238	44.898996
3500.224119	684756.166086	44.904001
3500.613065	684768.648725	44.909005
3500.548899	684762.634895	44.914010
3500.764338	684745.820382	44.919015
3500.708322	684733.979843	44.924020
3500.738783	684721.228788	44.929025
3500.901641	684718.861824	44.934029
3500.628045	684717.761933	44.939034
3500.882364	684714.433854	44.944039
3500.779899	684718.185044	44.949044
3501.143898	684695.420947	44.954049
3500.868382	684681.575244	44.959053
3500.971622	684683.450238	44.964058
3501.060844	684660.582096	44.969063
3501.074190	684648.978932	44.974068
3500.746594	684643.606035	44.979073
3500.899604	684638.552028	44.984077
3500.444382	684640.021425	44.989082
3500.859403	684622.128115	44.994087
3500.862180	684603.058148	44.999092
3501.106979	684590.022537	45.004097
3500.935084	684586.466108	45.009101
3500.661348	684587.208459	45.014106
3501.224230	684559.531724	45.019111
3501.149152	684559.942504	45.024116
3500.845914	684545.055579	45.029121
3500.997020	684526.906956	45.034125
3500.761584	684521.468966	45.039130
3500.872928	684495.410163	45.044135
3500.965822	684501.220361	45.049140
3500.813092	684485.910141	45.054145
3501.032982	684488.114432	45.059149
3500.689748	684461.433588	45.064154
3501.142761	684451.848726	45.069159
3501.004430	684455.157833	45.074164
3501.003927	684442.361714	45.079169
3500.856248	684423.963518	45.084173
3500.385238	684413.485711	45.089178
3500.615884	684401.348409	45.094183
3500.589568	684408.423146	45.099188
3500.750911	684397.591861	45.104193
3500.927954	684407.321712	45.109197
3500.646884	684398.306230	45.114202
3501.088688	684365.918759	45.119207
3500.748314	684358.058238	45.124212
3500.666689	684360.561345	45.129217
3500.774415	684352.377809	45.134221
3501.050036	684354.274174	45.139226
3501.246053	684330.690476	45.144231
3500.523129	684322.644188	45.149236
3500.240403	684313.529311	45.154241
3500.623118	684311.972366	45.159245
3500.541156	684306.508882	45.164250
3500.541386	684301.081604	45.169255
3500.851482	684310.092488	45.174260
3501.037428	684289.049719	45.179265
3500.733961	684274.510931	45.184269
3500.450837	684271.869013	45.189274
3500.918780	684271.293812	45.194279
3500.721522	684268.338951	45.199284
3500.789472	684262.701292	45.204289
3501.079542	684233.574899	45.209293
3500.658597	684222.242132	45.214298
3500.612065	684219.511306	45.219303
3500.512677	684222.515309	45.224308
3500.822663	684216.040947	45.229313
3500.829199	684219.973496	45.234317
3500.487678	684197.872469	45.239322
3500.862913	684180.582377	45.244327
3500.759557	684181.445978	45.249332
3500.368038	684173.792919	45.254337
3500.698143	684167.813122	45.259341
3500.457460	684175.869521	45.264346
3500.641791	684169.664854	45.269351
3500.589429	684179.681824	45.274356
3500.769749	684169.444640	45.279361
3500.578253	684143.086332	45.284365
3500.656694	684132.965529	45.289370
3500.919462	684124.009276	45.294375
3500.435110	684130.811376	45.299380
3500.746270	684130.710211	45.304385
3500.721510	684124.340898	45.309389
3500.375421	684125.792338	45.314394
3500.626276	684112.057948	45.319399
3500.391018	684098.852009	45.324404
3500.503721	684092.908092	45.329409
3500.688281	684099.400498	45.334413
3500.545249	684089.615004	45.339418
3500.563189	684082.790470	45.344423
3500.412688	684092.475204	45.349428
3500.591426	684090.503796	45.354433
3500.751067	684077.033392	45.359437
3500.621429	684093.586094	45.364442
3500.568670	684083.984847	45.369447
3500.421462	684089.984367	45.374452
3500.488121	684071.301072	45.379457
3500.328515	684051.410308	45.384461
3500.623886	684042.946517	45.389466
3500.564660	684037.927253	45.394471
3500.408573	684053.139985	45.399476
3500.474808	684042.274203	45.404481
3500.618245	684036.723515	45.409485
3500.613444	684041.853049	45.414490
3500.533137	684049.534504	45.419495
3500.515909	684056.209667	45.424500
3500.667955	684047.072465	45.429505
3500.594630	684050.370975	45.434509
3500.726395	684045.220565	45.439514
3500.753956	684015.340171	45.444519
3500.276486	684020.846590	45.449524
3500.215820	684009.205050	45.454529
3500.160742	684009.313789	45.459533
3500.148107	684010.660346	45.464538
3500.547754	684007.905514	45.469543
3500.358919	684013.712790	45.474548
3500.305796	684004.011932	45.479553
3500.484367	684001.642187	45.484557
3500.814414	684007.164542	45.489562
3500.655699	684006.792476	45.494567
3500.333078	684005.949565	45.499572
3500.444651	684005.632417	45.504577
3500.775732	683992.631489	45.509581
3500.332596	684003.509925	45.514586
3500.340695	683998.877860	45.519591
3500.422260	684004.242108	45.524596
3500.833623	683989.933283	45.529601
3500.511071	683966.484138	45.534605
3500.297037	683966.121213	45.539610
3500.431563	683946.679545	45.544615
3500.453595	683963.655559	45.549620
3500.254961	683956.916516	45.554625
3500.920849	683956.109411	45.559629
3500.569368	683962.142773	45.564634
3500.592141	683951.582827	45.569639
3500.604599	683954.369259	45.574644
3500.083108	683961.028241	45.579649
3500.708814	683957.837686	45.584653
3500.819018	683965.139173	45.589658
3500.847533	683937.399486	45.594663
3500.375296	683919.651433	45.599668
3500.271541	683926.988309	45.604673
3500.326609	683921.302774	45.609677
3500.450239	683921.630950	45.614682
3500.447963	683915.108394	45.619687
3500.510431	683919.081622	45.624692
3500.268141	683913.594606	45.629697
3500.668253	683914.375027	45.634701
3500.224575	683912.705619	45.639706
3500.603558	683920.062310	45.644711
3500.664596	683922.940310	45.649716
3500.784806	683921.277302	45.654721
3500.846206	683917.084530	45.659725
3500.699841	683899.631139	45.664730
3500.820786	683872.722477	45.669735
3500.858348	683879.538096	45.674740
3500.470288	683878.058666	45.679745
3500.676898	683873.642700	45.684749
3500.229522	683874.314213	45.689754
3500.377652	683866.870474	45.694759
3500.810437	683868.691175	45.699764
3500.402538	683849.986267	45.704769
3500.687160	683834.005143	45.709773
3500.154443	683830.607636	45.714778
3500.524592	683822.977787	45.719783
3500.204274	683832.342300	45.724788
3500.356538	683823.852164	45.729793
3500.627370	683828.438323	45.734797
3500.447670	683833.447495	45.739802
3500.446716	683826.227538	45.744807
3500.642265	683831.722434	45.749812
3500.645313	683823.655311	45.754817
3500.950910	683790.242631	45.759821
3500.670420	683734.369686	45.764826
3500.384288	683605.846035	45.769831
3500.269389	683452.344361	45.774836
3500.180440	683225.285149	45.779841
3500.031729	682948.879454	45.784845
3499.858277	682609.521384	45.789850
3499.534634	682217.284900	45.794855
3499.066543	681760.208961	45.799860
3499.113954	681251.872114	45.804865
3498.847944	680692.751570	45.809869
3498.425740	680087.245624	45.814874
3498.005163	679408.516936	45.819879
3497.513446	678675.842667	45.824884
3497.269196	677891.050851	45.829889
3496.496230	677042.895218	45.834893
3495.965687	676150.268380	45.839898
3496.016981	675192.916141	45.844903
3495.515011	674187.555406	45.849908
3494.860605	673111.870779	45.854913
3494.574088	671978.017483	45.859917
3493.747769	670791.759594	45.864922
3493.128283	669541.583867	45.869927
3492.207881	668240.318153	45.874932
3491.551159	666873.781263	45.879937
3491.213459	665433.105802	45.884941
3489.920627	663953.749103	45.889946
3489.477179	662398.464058	45.894951
3488.666806	660811.592058	45.899956
3487.628319	659149.112169	45.904961
3486.712040	657426.708055	45.909965
3485.394650	655655.423378	45.914970
3484.569200	653814.705326	45.919975
3483.558690	651930.658682	45.924980
3482.644445	649995.668552	45.929985
3481.631469	647992.846032	45.934989
3480.236922	645938.646646	45.939994
3479.197859	643825.469395	45.944999
3478.253429	641663.825846	45.950004
3476.802159	639438.830627	45.955009
3476.223492	637160.274522	45.960013
3474.301745	634832.895761	45.965018
3473.315792	632446.176931	45.970023
3472.042461	630009.195752	45.975028
3470.689793	627517.429959	45.980033
3469.645317	624960.712846	45.985037
3467.665014	622359.951330	45.990042
3466.425373	619701.710848	45.995047
3465.161286	617011.145394	46.000052
3463.669504	614249.059911	46.005057
3462.150331	611444.462746	46.010061
3460.470826	608581.697979	46.015066
3458.692452	605674.567050	46.020071
3457.304310	602719.950276	46.025076
3455.504309	599712.478261	46.030081
3454.285522	596648.437746	46.035085
3451.873710	593555.512042	46.040090
3450.298861	590393.004021	46.045095
3448.416876	587195.684306	46.050100
3446.640973	583940.089243	46.055105
3445.068223	580643.061341	46.060109
3443.073005	577285.415849	46.065114
3441.240408	573890.563533	46.070119
3439.099010	570454.536669	46.075124
3437.339787	566971.912863	46.080129
3435.224912	563443.845084	46.085133
3432.866022	559871.649611	46.090138
3431.107892	556246.850230	46.095143
3429.074329	552584.629803	46.100148
3426.840196	548884.656194	46.105153
3425.015888	545132.794047	46.110157
3422.965723	541348.588683	46.115162
3420.766662	537498.214620	46.120167
3418.304281	533627.674545	46.125172
3416.533652	529694.258178	46.130177
3414.048724	525722.550229	46.135181
3411.693662	521714.720151	46.140186
3409.424948	517653.133136	46.145191
3406.918616	513568.337829	46.150196
3404.578542	509426.807695	46.155201
3402.281723	505246.484758	46.160205
3399.738419	501044.700535	46.165210
3397.386008	496785.169025	46.170215
3394.390189	492505.140680	46.175220
3391.923146	488188.637176	46.180225
3389.714097	483812.361398	46.185229
3386.877238	479417.601025	46.190234
3384.576235	474969.379577	46.195239
3381.920003	470504.807451	46.200244
3379.052075	466000.716910	46.205249
3376.338126	461451.164373	46.210253
3373.742325	456874.599985	46.215258
3371.412288	452253.969433	46.220263
3368.586216	447610.136136	46.225268
3365.518934	442919.481218	46.230273
3362.896153	438204.565831	46.235277
3360.169500	433449.811389	46.240282
3357.370261	428673.436536	46.245287
3354.155362	423862.617721	46.250292
3351.167973	419010.502888	46.255297
3348.400203	414132.765412	46.260301
3345.053067	409233.971170	46.265306
3342.283184	404294.742716	46.270311
3339.351904	399335.357979	46.275316
3336.333383	394358.391123	46.280321
3333.279822	389340.422724	46.285325
3329.790852	384302.195974	46.290330
3326.706839	379234.670633	46.295335
3323.658570	374141.460971	46.300340
3320.629701	369029.101280	46.305345
3317.375709	363890.230320	46.310349
3313.685944	358729.026507	46.315354
3310.726841	353544.660796	46.320359
3307.594487	348348.783390	46.325364
3304.150874	343125.671112	46.330369
3301.010735	337862.549405	46.335373
3297.152111	332607.942419	46.340378
3293.465166	327320.251818	46.345383
3290.226585	322018.169026	46.350388
3287.239881	316690.736244	46.355393
3283.528668	311339.444468	46.360397
3280.090681	305990.182524	46.365402
3276.430347	300625.220879	46.370407
3272.993097	295250.072110	46.375412
3269.127662	289849.575758	46.380417
3265.969510	284439.088104	46.385421
3261.773253	279029.173136	46.390426
3258.511728	273589.695370	46.395431
3254.580070	268140.771581	46.400436
3250.662034	262707.261166	46.405441
3247.142028	257246.582709	46.410445
3243.245065	251787.199114	46.415450
3239.182650	246305.939459	46.420455
3235.767891	240841.165970	46.425460
3231.782709	235359.197492	46.430465
3228.227062	229870.351298	46.435469
3224.147392	224381.879949	46.440474
3220.430055	218882.320612	46.445479
3216.428176	213379.461202	46.450484
3212.507817	207858.222817	46.455489
3208.905534	202278.768753	46.460493
3204.592244	196778.203284	46.465498
3200.575361	191275.832130	46.470503
3196.534936	185767.817272	46.475508
3192.205129	180268.038781	46.480513
3187.775692	174770.523786	46.485517
3183.971924	169279.123491	46.490522
3179.436851	163804.836769	46.495527
3175.366181	158325.662398	46.500532
3171.135484	152863.072100	46.505537
3166.770117	147402.066155	46.510541
3162.106819	141971.836535	46.515546
3157.784498	136534.678939	46.520551
3153.152406	131124.981700	46.525556
3149.009807	125721.278518	46.530561
3144.466730	120332.544140	46.535565
3139.971643	114974.435009	46.540570
3135.212492	109617.992984	46.545575
3130.561180	104281.426935	46.550580
3125.502435	98986.606498	46.555585
3121.339226	93690.981893	46.560589
3116.111540	88443.716834	46.565594
3111.493606	83209.405191	46.570599
3106.646381	78005.703428	46.575604
3101.545821	72829.783508	46.580609
3096.664021	67689.791531	46.585613
3091.267241	62587.765066	46.590618
3085.967748	57504.710153	46.595623
3080.472229	52472.636389	46.600628
3074.646034	47495.093321	46.605633
3068.299810	42566.018193	46.610637
3061.553272	37731.886060	46.615642
3049.442103	33100.964454	46.620647
3033.883525	28652.734814	46.625652
3018.776865	24379.844558	46.630657
3003.470489	20336.313132	46.635661
2985.187898	16601.020865	46.640666
2961.608461	13303.997347	46.645671
2935.680832	10434.085343	46.650676
2910.751827	7960.504694	46.655681
2889.000278	5862.557434	46.660685
2869.129104	4161.405019	46.665690
2852.936440	2805.363805	46.670695
2838.770452	1772.177566	46.675700
2828.076706	1010.031404	46.680705
2819.271526	483.686572	46.685709
2811.844278	168.777771	46.690714
2797.432019	237.109001	46.695719
2793.770385	240.839966	46.700724
2795.589369	232.667717	46.705729
2800.109665	225.701263	46.710733
2803.408285	239.663832	46.715738
2805.654912	241.377501	46.720743
2806.350818	232.699274	46.725748
2805.144201	216.589448	46.730753
2802.263504	207.307747	46.735757
2798.607886	222.773785	46.740762
2795.201953	219.292938	46.745767
2792.160899	218.025823	46.750772
2789.306302	222.901761	46.755777
2786.594136	216.255642	46.760781
2783.053608	225.220293	46.765786
2780.845111	223.551540	46.770791
2778.125681	217.965740	46.775796
2775.054199	216.216644	46.780801
2772.055065	213.588670	46.785805
2768.723622	213.356524	46.790810
2765.582738	215.138245	46.795815
2762.607164	211.234537	46.800820
2758.903390	213.067994	46.805825
2755.740723	207.669642	46.810829
2752.456217	210.649502	46.815834
2749.084320	210.655742	46.820839
2746.076668	208.593979	46.825844
2742.828319	214.810514	46.830849
2740.066371	214.197390	46.835853
2735.988637	213.917909	46.840858
2732.635415	211.430867	46.845863
2729.543854	199.097179	46.850868
2726.222252	208.823656	46.855873
2722.875616	204.074044	46.860877
2719.518728	205.307434	46.865882
2716.148597	210.089964	46.870887
2712.990566	206.691291	46.875892
2709.448559	210.662607	46.880897
2705.630901	206.875842	46.885901
2702.255796	200.696119	46.890906
2698.834129	192.498245	46.895911
2695.815886	205.104391	46.900916
2692.016480	209.476498	46.905921
2689.436106	202.813371	46.910925
2686.004675	209.275941	46.915930
2682.633567	201.055103	46.920935
2678.382006	200.616984	46.925940
2674.475948	195.901217	46.930945
2672.026251	193.188481	46.935949
2669.064181	186.446087	46.940954
2664.378922	198.373497	46.945959
2660.984906	191.516328	46.950964
2657.775083	196.884894	46.955969
2655.051146	196.199426	46.960973
2651.033372	191.343125	46.965978
2648.054177	189.669622	46.970983
2645.106360	186.276462	46.975988
2641.031506	185.794327	46.980993
2637.859358	186.904840	46.985997
2633.974270	194.928694	46.991002
2629.711678	188.333161	46.996007
2627.095219	183.469065	47.001012
2623.953744	195.950012	47.006017
2620.405866	191.836276	47.011021
2616.871932	193.819731	47.016026
2612.879373	198.711303	47.021031
2609.584651	186.523451	47.026036
2606.224148	194.507640	47.031041
2602.547973	188.964339	47.036045
2599.482006	192.174532	47.041050
2596.003066	186.961092	47.046055
2592.659687	190.173211	47.051060
2588.944552	189.823380	47.056065
2585.664613	182.831557	47.061069
2581.832766	187.830734	47.066074
2578.730120	188.519520	47.071079
2575.156449	182.039488	47.076084
2571.436853	184.035563	47.081089
2567.959947	181.629129	47.086093
2564.611493	181.548556	47.091098
2560.790569	180.524402	47.096103
2557.925823	181.468635	47.101108
2553.942234	184.539323	47.106113
2551.219760	193.546875	47.111117
2547.131695	181.522211	47.116122
2543.865619	184.094825	47.121127
2540.084979	169.695438	47.126132
2536.477805	178.675226	47.131137
2533.318373	172.499023	47.136141
2529.974683	178.438828	47.141146
2526.666798	183.549420	47.146151
2523.247751	185.047620	47.151156
2519.604314	189.659657	47.156161
2516.068105	178.623678	47.161165
2512.194338	183.905731	47.166170
2508.408673	181.651904	47.171175
2505.577748	179.335106	47.176180
2502.084854	177.837743	47.181185
2498.590598	174.782636	47.186189
2495.385698	177.296610	47.191194
2491.662663	178.323018	47.196199
2487.913208	178.875065	47.201204
2484.437936	182.490557	47.206209
2481.262467	170.714268	47.211213
2477.040343	176.508895	47.216218
2473.888771	180.009815	47.221223
2470.752792	174.527561	47.226228
2466.958999	182.137019	47.231233
2463.806293	175.315453	47.236237
2460.313943	177.251101	47.241242
2456.500537	174.288347	47.246247
2453.481653	173.442480	47.251252
2449.848279	172.872029	47.256257
2446.422857	178.550737	47.261261
2443.030904	172.564864	47.266266
2439.250013	169.849728	47.271271
2435.635764	176.191585	47.276276
2431.801643	173.387786	47.281281
2428.640557	175.068897	47.286285
2425.279834	173.332247	47.291290
2421.750041	172.510034	47.296295
2418.262862	167.236948	47.301300
2414.721436	169.200098	47.306305
2411.672321	169.323849	47.311309
2407.622980	170.787596	47.316314
2404.246738	178.095096	47.321319
2400.624122	165.468017	47.326324
2397.194228	170.517997	47.331329
2394.074228	168.576731	47.336333
2390.587172	171.502582	47.341338
2386.768793	171.564702	47.346343
2383.645377	162.407221	47.351348
2379.594434	168.799143	47.356353
2376.432699	164.678316	47.361357
2373.113402	158.809929	47.366362
2369.527775	163.871117	47.371367
2366.103947	164.720602	47.376372
2361.825169	169.296496	47.381377
2358.558044	164.941929	47.386381
2355.416830	164.227888	47.391386
2351.759943	176.914526	47.396391
2348.773980	168.009789	47.401396
2344.971722	168.915651	47.406401
2341.173350	167.852839	47.411405
2338.002172	171.671656	47.416410
2334.282007	168.136889	47.421415
2331.061557	163.320347	47.426420
2327.542747	161.661466	47.431425
2324.086481	166.348034	47.436429
2320.644372	164.596337	47.441434
2316.795786	170.728455	47.446439
2313.397976	160.382342	47.451444
2309.554468	163.535623	47.456449
2306.552346	164.867257	47.461453
2303.331814	162.196980	47.466458
2299.419851	170.934777	47.471463
2296.152819	169.033332	47.476468
2292.089963	165.202529	47.481473
2288.871760	162.698429	47.486477
2285.267577	162.369958	47.491482
2281.739640	156.135814	47.496487
2278.665729	158.783552	47.501492
2274.814081	163.963669	47.506497
2271.469888	161.355538	47.511501
2267.982704	159.150573	47.516506
2264.525305	158.708216	47.521511
2261.415865	164.467329	47.526516
2256.976573	164.703852	47.531521
2253.824954	167.571881	47.536525
2250.755048	161.400225	47.541530
2246.649131	157.839258	47.546535
2243.679366	155.605439	47.551540
2239.920104	160.746207	47.556545
2236.468138	151.452655	47.561549
2233.014843	166.387640	47.566554
2229.294162	163.273581	47.571559
2225.997272	152.170235	47.576564
2222.462061	156.507845	47.581569
2219.069187	155.693121	47.586573
2215.790384	150.546531	47.591578
2211.980692	157.375399	47.596583
2208.916671	145.985052	47.601588
2205.046229	165.783232	47.606593
2201.623158	148.311866	47.611597
2198.136248	158.696349	47.616602
2194.116858	154.915084	47.621607
2191.079373	145.977582	47.626612
2187.242448	160.388280	47.631617
2183.753394	148.744141	47.636621
2180.171934	155.054713	47.641626
2177.020562	151.696022	47.646631
2173.737180	149.874348	47.651636
2169.778140	150.388187	47.656641
2166.524767	153.169336	47.661645
2163.415086	155.851892	47.666650
2159.552364	158.284069	47.671655
2156.121934	162.858741	47.676660
2152.256964	152.514005	47.681665
2149.100004	146.271414	47.686669
2145.688507	143.855893	47.691674
2141.537923	152.328266	47.696679
2138.455953	149.548735	47.701684
2134.934481	146.259682	47.706689
2131.528897	144.538012	47.711693
2128.158131	152.611840	47.716698
2124.107234	161.745763	47.721703
2120.964496	165.795839	47.726708
2117.354633	157.507143	47.731713
2114.115736	151.908641	47.736717
2110.726577	147.555756	47.741722
2107.174853	154.611729	47.746727
2103.356454	144.389378	47.751732
2099.862964	155.310392	47.756737
2096.447472	153.639922	47.761741
2093.070035	153.585841	47.766746
2089.345525	151.248671	47.771751
2085.980360	154.011501	47.776756
2082.471223	156.482648	47.781761
2079.043642	156.377883	47.786765
2075.289996	151.776589	47.791770
2071.632825	155.758011	47.796775
2068.667964	149.926873	47.801780
2064.970247	150.168999	47.806785
2061.523602	157.784607	47.811789
2058.231221	150.788604	47.816794
2054.600196	160.844038	47.821799
2051.217888	153.414791	47.826804
2047.347510	154.992298	47.831809
2043.785362	146.805688	47.836813
2040.360913	143.911299	47.841818
2036.610488	147.107809	47.846823
2033.537162	149.001408	47.851828
2030.364513	161.956925	47.856833
2026.667240	151.603281	47.861837
2023.050433	153.277915	47.866842
2019.189341	155.750009	47.871847
2016.013523	148.811098	47.876852
2012.264307	157.849150	47.881857
2009.086036	147.093790	47.886861
2006.080065	153.028924	47.891866
2001.605107	148.637211	47.896871
1998.538054	148.716284	47.901876
1994.723112	147.590237	47.906881
1991.298042	158.506506	47.911885
1987.858120	147.156735	47.916890
1984.585881	142.368407	47.921895
1981.390860	140.132250	47.926900
1977.528270	144.167721	47.931905
1973.985415	150.698994	47.936909
1970.412599	151.008125	47.941914
1966.790337	142.530419	47.946919
1963.690235	147.700521	47.951924
1959.888598	147.989760	47.956929
1956.391587	148.139523	47.961933
1953.166608	145.510722	47.966938
1949.449453	147.531006	47.971943
1946.015131	139.480982	47.976948
1942.211189	140.432482	47.981953
1938.776237	141.892740	47.986957
1935.466862	146.101591	47.991962
1931.928355	141.546876	47.996967
1928.369503	135.636887	48.001972
1925.068698	136.463384	48.006977
1921.233603	145.934481	48.011981
1917.897232	141.941245	48.016986
1914.473872	144.619922	48.021991
1911.120763	130.484478	48.026996
1907.468630	141.547947	48.032001
1904.138155	135.213750	48.037005
1900.519100	134.096966	48.042010
1896.680509	137.386749	48.047015
1893.449464	139.823409	48.052020
1889.897085	143.106612	48.057025
1886.334432	136.478203	48.062029
1882.804730	136.177999	48.067034
1879.211485	143.733182	48.072039
1875.675490	136.283398	48.077044
1871.917906	138.285783	48.082049
1868.762224	135.297273	48.087053
1865.794679	138.033249	48.092058
1862.103549	137.268059	48.097063
1858.532980	130.777546	48.102068
1855.169392	142.309264	48.107073
1851.640745	147.696104	48.112077
1847.520286	138.152403	48.117082
1843.617123	145.286562	48.122087
1841.273155	128.818968	48.127092
1837.858416	137.104531	48.132097
1834.469243	141.620121	48.137101
1830.629153	138.508079	48.142106
1826.458331	143.796543	48.147111
1823.044512	145.626160	48.152116
1819.874809	140.821768	48.157121
1816.114058	138.728453	48.162125
1813.213005	140.571557	48.167130
1809.267331	141.647905	48.172135
1806.154022	142.832366	48.177140
1802.325662	138.774357	48.182145
1798.906797	140.715140	48.187149
1795.746210	134.787608	48.192154
1791.668750	138.271199	48.197159
1788.458568	134.330569	48.202164
1784.813475	139.459311	48.207169
1781.255694	137.821578	48.212173
1777.791088	137.210332	48.217178
1773.869131	142.165145	48.222183
1771.067335	131.291169	48.227188
1767.352583	140.018226	48.232193
1763.638410	130.092726	48.237197
1760.311162	139.830633	48.242202
1756.870160	140.490274	48.247207
1753.531058	128.285360	48.252212
1749.867704	138.090631	48.257217
1746.231691	139.985362	48.262221
1743.009139	132.114338	48.267226
1738.976200	142.420745	48.272231
1735.413190	136.331459	48.277236
1732.230896	132.460650	48.282241
1728.464976	141.358825	48.287245
1725.395619	133.668832	48.292250
1721.581488	131.669114	48.297255
1718.024761	133.984664	48.302260
1714.800934	143.270142	48.307265
1711.352480	142.673246	48.312269
1708.235664	132.443941	48.317274
1704.499509	132.972981	48.322279
1701.503275	133.819812	48.327284
1697.252501	137.217180	48.332289
1693.371549	133.921225	48.337293
1690.323543	132.569462	48.342298
1686.678110	136.854540	48.347303
1683.139951	133.504530	48.352308
1679.775862	127.836784	48.357313
1676.404135	130.091310	48.362317
1672.990864	129.778302	48.367322
1669.093747	135.414237	48.372327
1665.704044	128.275873	48.377332
1661.996040	122.562351	48.382337
1659.002751	129.400189	48.387341
1655.682939	130.584269	48.392346
1651.843628	138.362370	48.397351
1648.153926	132.292397	48.402356
1644.564767	131.774536	48.407361
1640.647446	132.470029	48.412365
1637.980971	133.726365	48.417370
1634.344401	129.808607	48.422375
1630.815072	126.113426	48.427380
1627.250350	121.870004	48.432385
1623.177579	137.612173	48.437389
1620.448222	128.481008	48.442394
1616.663075	135.452929	48.447399
1613.089769	132.882163	48.452404
1610.198027	143.267258	48.457409
1606.645019	139.688108	48.462413
1602.572160	127.281764	48.467418
1599.022064	132.242174	48.472423
1595.318093	126.003336	48.477428
1592.280330	122.232608	48.482433
1588.629990	129.871092	48.487437
1585.117540	123.295826	48.492442
1581.504143	128.236750	48.497447
1578.624345	132.965663	48.502452
1574.693607	136.922814	48.507457
1570.758384	133.313734	48.512461
1567.946009	120.516493	48.517466
1564.380359	129.067437	48.522471
1561.050489	121.972532	48.527476
1557.334114	122.029958	48.532481
1553.485079	128.397434	48.537485
1549.896549	123.670418	48.542490
1546.448793	133.239610	48.547495
1542.990035	123.757235	48.552500
1539.699473	127.572942	48.557505
1536.126788	113.344249	48.562509
1532.804964	118.033807	48.567514
1528.772425	130.946518	48.572519
1525.495471	123.955350	48.577524
1522.165086	127.749258	48.582529
1518.484482	124.727903	48.587533
1515.502272	125.274572	48.592538
1511.933857	139.028536	48.597543
1508.481023	126.813119	48.602548
1504.765394	123.689446	48.607553
1500.950352	128.223033	48.612557
1497.668270	123.417426	48.617562
1493.829474	134.074088	48.622567
1490.696672	121.921260	48.627572
1486.913331	129.090325	48.632577
1483.358934	123.593241	48.637581
1480.151913	126.648430	48.642586
1476.473417	130.914504	48.647591
1473.323329	123.689422	48.652596
1469.845899	122.515604	48.657601
1465.989888	129.182882	48.662605
1462.624326	115.780489	48.667610
1458.663448	130.155262	48.672615
1455.592319	116.085800	48.677620
1451.938757	126.058994	48.682625
1448.447793	124.138164	48.687629
1445.276486	125.516631	48.692634
1441.778716	122.360836	48.697639
1438.137631	113.696564	48.702644
1434.676983	125.379050	48.707649
1430.552466	120.268425	48.712653
1427.384902	128.364317	48.717658
1423.984106	119.739729	48.722663
1420.992587	123.827785	48.727668
1417.283848	122.833865	48.732673
1413.548949	125.636844	48.737677
1410.452315	114.231913	48.742682
1406.593338	127.091472	48.747687
1402.872255	121.045305	48.752692
1399.568907	120.226492	48.757697
1395.710485	124.157608	48.762701
1392.596753	116.849807	48.767706
1388.717761	128.612173	48.772711
1385.253586	115.802822	48.777716
1381.738555	120.478960	48.782721
1378.701839	123.270561	48.787725
1375.488452	125.387381	48.792730
1371.478173	125.057620	48.797735
1368.131248	125.849595	48.802740
1364.065095	126.155643	48.807745
1360.534913	129.090674	48.812749
1357.498048	125.821410	48.817754
1353.581986	127.040106	48.822759
1350.811820	123.585322	48.827764
1347.377115	125.779721	48.832769
1343.575701	127.059134	48.837773
1339.945529	125.085320	48.842778
1336.291433	127.070044	48.847783
1332.790071	120.056680	48.852788
1329.225239	120.315327	48.857793
1325.636630	126.559101	48.862797
1322.558430	120.496166	48.867802
1318.934022	129.492570	48.872807
1315.731255	124.228387	48.877812
1312.002803	116.472062	48.882817
1308.345180	120.250761	48.887821
1305.077196	122.610533	48.892826
1301.033021	131.429916	48.897831
1297.725816	115.447541	48.902836
1294.582163	118.780665	48.907841
1290.919651	112.103101	48.912845
1287.367721	109.519625	48.917850
1283.538538	115.112671	48.922855
1280.487692	116.616522	48.927860
1277.458031	112.382553	48.932865
1273.366123	125.599359	48.937869
1270.291321	119.702059	48.942874
1266.218279	122.023927	48.947879
1262.831961	124.106772	48.952884
1259.249852	119.239654	48.957889
1255.601678	117.580694	48.962893
1252.382991	114.786470	48.967898
1248.716352	116.568916	48.972903
1245.459601	121.734925	48.977908
1242.268328	116.416807	48.982913
1238.513524	119.110571	48.987917
1234.756313	115.525987	48.992922
1231.222072	121.113172	48.997927
1227.236288	112.470582	49.002932
1224.061528	115.816419	49.007937
1220.949203	120.102653	49.012941
1217.784020	111.760241	49.017946
1214.534908	117.542264	49.022951
1210.748922	108.918249	49.027956
1207.037455	112.681698	49.032961
1203.129158	111.908557	49.037965
1199.919972	117.616875	49.042970
1195.948360	108.415096	49.047975
1192.528569	109.669227	49.052980
1189.138861	108.340411	49.057985
1185.598850	117.302000	49.062989
1182.483919	111.460966	49.067994
1179.062819	115.574683	49.072999
1175.652035	118.455925	49.078004
1171.827733	112.601957	49.083009
1168.263056	111.428482	49.088013
1164.765347	109.299463	49.093018
1161.067084	113.798592	49.098023
1157.756156	107.431844	49.103028
1154.609076	114.100374	49.108033
1150.376076	107.172471	49.113037
1147.312136	114.325873	49.118042
1143.721065	115.343644	49.123047
1140.340957	106.993748	49.128052
1136.689767	118.122977	49.133057
1132.945957	122.333691	49.138061
1130.201658	115.757313	49.143066
1126.247034	119.495865	49.148071
1123.213765	110.683903	49.153076
1119.409534	110.353760	49.158081
1115.804517	118.587575	49.163085
1111.968328	114.565708	49.168090
1108.505968	121.919237	49.173095
1105.241499	116.355470	49.178100
1101.836652	102.448087	49.183105
1098.080379	109.161894	49.188109
1094.798822	104.090362	49.193114
1091.142761	111.422170	49.198119
1087.768179	109.881366	49.203124
1084.437143	108.133244	49.208129
1080.756817	119.961769	49.213133
1077.179771	105.638391	49.218138
1073.707071	115.405266	49.223143
1069.996707	117.371153	49.228148
1066.672334	112.139213	49.233153
1063.082290	118.750287	49.238157
1060.168982	114.625849	49.243162
1055.947804	113.780457	49.248167
1052.463313	112.026056	49.253172
1049.182107	104.342215	49.258177
1045.214756	115.514904	49.263181
1042.187275	102.465322	49.268186
1038.900650	114.201115	49.273191
1035.358666	102.950556	49.278196
1031.608328	103.624663	49.283201
1028.172491	110.588066	49.288205
1025.087438	112.500546	49.293210
1021.394698	100.555546	49.298215
1017.595108	103.434744	49.303220
1014.255111	109.899973	49.308225
1010.276374	104.528632	49.313229
1007.444416	105.755622	49.318234
1003.558297	105.378799	49.323239
1000.254322	108.705208	49.328244
996.854106	101.146938	49.333249
992.831449	106.107347	49.338253
989.349845	102.521477	49.343258
986.084058	114.032049	49.348263
982.538705	102.926946	49.353268
979.294758	113.632925	49.358273
975.490705	113.584882	49.363277
972.205655	102.519865	49.368282
969.002599	110.129822	49.373287
964.836730	111.769241	49.378292
961.798327	112.725647	49.383297
958.101996	111.778457	49.388301
954.432685	103.704857	49.393306
951.030761	110.353672	49.398311
947.535722	105.602257	49.403316
944.206043	112.414319	49.408321
940.447719	113.386233	49.413325
936.756119	100.499859	49.418330
933.525584	113.507304	49.423335
930.397065	109.364621	49.428340
927.013847	101.053142	49.433345
922.876221	109.384394	49.438349
919.367202	103.407327	49.443354
915.824365	111.237703	49.448359
912.415730	108.500558	49.453364
909.271841	98.382262	49.458369
905.560849	99.998536	49.463373
902.370237	102.954760	49.468378
898.289919	101.851732	49.473383
894.796205	105.032516	49.478388
891.857095	96.613616	49.483393
887.954019	102.246521	49.488397
884.403539	100.330564	49.493402
881.215447	103.903445	49.498407
877.643066	107.150187	49.503412
874.061811	97.492476	49.508417
870.239845	116.350768	49.513421
867.221947	102.845301	49.518426
863.545029	108.236255	49.523431
859.891226	108.710393	49.528436
856.505174	112.061201	49.533441
852.571579	109.969898	49.538445
849.466336	106.116264	49.543450
846.262963	114.408743	49.548455
842.612964	107.102635	49.553460
839.416135	111.282416	49.558465
835.500780	110.200615	49.563469
832.249994	108.785911	49.568474
828.443497	109.280887	49.573479
825.046128	110.663631	49.578484
821.467672	105.943550	49.583489
817.625282	115.165399	49.588493
814.737522	112.687405	49.593498
811.080858	107.505930	49.598503
807.413734	109.634197	49.603508
803.824397	105.117416	49.608513
800.047653	119.188283	49.613517
797.178857	112.786162	49.618522
793.421791	109.121885	49.623527
790.115904	109.832160	49.628532
786.640339	101.307243	49.633537
783.062398	110.952107	49.638541
779.173368	108.615500	49.643546
775.699661	107.387825	49.648551
772.617688	106.745329	49.653556
769.059883	101.385476	49.658561
765.104453	108.772398	49.663565
761.949115	104.175123	49.668570
758.497645	110.006683	49.673575
754.977008	99.254889	49.678580
751.594756	104.752916	49.683585
747.832664	96.741116	49.688589
744.312900	100.541834	49.693594
740.267829	103.737529	49.698599
737.604934	99.999794	49.703604
734.183899	98.110244	49.708609
730.292662	100.940011	49.713613
726.869165	96.108657	49.718618
723.387558	96.902627	49.723623
720.115400	94.519908	49.728628
716.803600	91.404963	49.733633
712.655272	99.805881	49.738637
708.950274	97.580282	49.743642
705.361468	97.754685	49.748647
702.045414	101.835180	49.753652
699.170307	96.241874	49.758657
695.419881	103.044266	49.763661
692.069158	94.574693	49.768666
688.720936	98.757626	49.773671
684.819414	97.092347	49.778676
681.323333	94.024607	49.783681
677.779301	99.157457	49.788685
674.399281	93.786929	49.793690
670.843151	107.694380	49.798695
667.168183	98.009625	49.803700
663.713622	102.736520	49.808705
660.143922	111.587240	49.813709
656.969629	101.452914	49.818714
653.545518	105.521793	49.823719
649.707644	107.771899	49.828724
646.727281	96.724692	49.833729
643.002353	102.014495	49.838733
639.423954	103.872051	49.843738
635.817828	111.497489	49.848743
632.330112	104.947865	49.853748
628.636984	105.286477	49.858753
625.383401	106.468121	49.863757
621.788693	100.761517	49.868762
618.153450	100.375792	49.873767
614.526346	102.345650	49.878772
611.255644	102.165598	49.883777
607.719548	98.095221	49.888781
604.330184	106.401793	49.893786
600.772537	102.054197	49.898791
597.136673	106.482700	49.903796
594.031342	97.222216	49.908801
589.933264	104.883999	49.913805
586.982115	108.626151	49.918810
583.397379	101.034201	49.923815
579.239842	104.066207	49.928820
576.201747	95.569693	49.933825
572.647482	109.072186	49.938829
569.434742	96.721587	49.943834
565.679115	96.465227	49.948839
562.193284	100.421495	49.953844
558.847573	99.496785	49.958849
554.949358	101.599337	49.963853
551.845530	96.180493	49.968858
548.238972	97.312683	49.973863
544.761096	98.556901	49.978868
541.460468	95.786971	49.983873
537.657983	101.666947	49.988877
534.056833	96.817331	49.993882
530.425184	91.073940	49.998887
526.974610	97.755253	50.003892
523.834224	89.915330	50.008897
520.063577	104.003957	50.013901
516.817234	93.486284	50.018906
513.327775	98.201345	50.023911
509.599500	100.452331	50.028916
506.241382	88.351299	50.033921
502.625154	98.706632	50.038925
499.209112	97.281581	50.043930
495.688864	102.460568	50.048935
492.112675	110.095959	50.053940
488.884630	102.581812	50.058945
484.937805	103.136156	50.063949
481.848262	97.997382	50.068954
477.852961	101.201065	50.073959
474.351136	105.053115	50.078964
471.279843	98.952879	50.083969
467.479648	101.637549	50.088973
464.172803	102.864090	50.093978
460.604186	94.742719	50.098983
457.081878	101.205722	50.103988
453.651593	100.660414	50.108993
450.177581	98.157939	50.113997
446.834453	94.711204	50.119002
443.493013	96.806242	50.124007
439.313000	96.956950	50.129012
435.955561	94.399409	50.134017
432.449052	97.050131	50.139021
429.302806	97.998626	50.144026
425.784229	97.386117	50.149031
421.665386	101.645975	50.154036
418.386593	99.141097	50.159041
414.935235	106.908751	50.164045
411.462707	103.512154	50.169050
408.049201	94.285868	50.174055
404.623366	101.445849	50.179060
401.860514	91.018866	50.184065
397.644258	104.924103	50.189069
393.992022	98.940763	50.194074
390.485201	100.329642	50.199079
386.684225	96.685319	50.204084
383.150130	90.689473	50.209089
380.030211	105.581400	50.214093
376.899415	92.581977	50.219098
373.125190	96.997755	50.224103
369.578334	97.971410	50.229108
366.066148	101.694446	50.234113
362.741429	96.359627	50.239117
359.097626	97.121874	50.244122
355.419568	99.056436	50.249127
351.931242	100.966785	50.254132
348.788888	96.031470	50.259137
344.848082	99.246761	50.264141
341.593791	98.790916	50.269146
337.934375	87.121356	50.274151
334.277236	99.142000	50.279156
331.079536	98.781940	50.284161
327.538424	95.096088	50.289165
324.214652	102.418753	50.294170
320.638922	98.007349	50.299175
316.863575	91.145112	50.304180
313.399683	96.557613	50.309185
309.732145	100.833384	50.314189
306.663406	94.081483	50.319194
302.993327	89.320515	50.324199
298.933912	99.144636	50.329204
295.909691	88.214169	50.334209
292.301347	95.121197	50.339213
289.005699	90.922193	50.344218
285.621337	89.854970	50.349223
281.905401	96.767058	50.354228
278.490740	90.038124	50.359233
275.116431	96.111436	50.364237
271.570012	90.410195	50.369242
267.969047	96.827823	50.374247
264.300726	88.753813	50.379252
261.107985	87.031605	50.384257
257.356142	91.631043	50.389261
254.060185	94.043496	50.394266
250.640397	95.295501	50.399271
247.206792	96.491791	50.404276
243.911769	90.118336	50.409281
239.665099	94.346937	50.414285
236.245822	86.955190	50.419290
232.929036	92.149145	50.424295
229.042038	99.875082	50.429300
225.914389	89.689029	50.434305
222.261505	87.408105	50.439309
218.756587	90.482228	50.444314
215.412103	86.398165	50.449319
211.768339	93.327529	50.454324
208.605643	93.594205	50.459329
204.848256	99.407609	50.464333
200.972005	94.382048	50.469338
197.606004	89.247041	50.474343
194.180386	101.377333	50.479348
191.096912	86.259782	50.484353
187.315892	102.593673	50.489357
183.965720	92.735105	50.494362
180.184471	89.849029	50.499367
176.555402	106.011460	50.504372
173.390005	93.478360	50.509377
169.649095	100.747925	50.514381
166.700473	90.263414	50.519386
163.586415	84.554177	50.524391
159.605395	93.728621	50.529396
155.644047	83.778070	50.534401
152.142575	98.417032	50.539405
148.899983	86.958429	50.544410
145.215733	90.008353	50.549415
141.438054	98.360493	50.554420
138.317663	93.053501	50.559425
134.576006	104.227806	50.564429
131.364479	99.230381	50.569434
128.154472	96.492933	50.574439
123.572305	105.358649	50.579444
120.803576	97.534292	50.584449
117.699261	101.341519	50.589453
114.129581	96.611026	50.594458
110.446673	95.904969	50.599463
106.583542	101.430178	50.604468
103.605709	100.157629	50.609473
99.652730	99.641504	50.614477
95.900530	94.242617	50.619482
92.568995	93.705901	50.624487
89.079442	94.180130	50.629492
85.961759	78.257942	50.634497
81.964275	90.566828	50.639501
79.014136	86.945413	50.644506
75.328403	90.405703	50.649511
71.938865	88.659540	50.654516
68.446093	87.954880	50.659521
64.708792	92.323579	50.664525
61.359382	90.435781	50.669530
57.665381	86.260975	50.674535
54.078629	94.005060	50.679540
50.866177	84.757964	50.684545
46.812691	93.801696	50.689549
43.643164	86.440462	50.694554
40.224042	87.713861	50.699559
36.288516	94.611567	50.704564
33.332672	92.549060	50.709569
29.920758	95.028933	50.714573
26.390426	94.467897	50.719578
22.842402	99.122683	50.724583
19.130732	97.789253	50.729588
15.468698	89.671449	50.734593
11.949651	99.920479	50.739597
8.760879	84.101742	50.744602
5.479253	92.898820	50.749607
1.554981	85.892772	50.754612