Fri Jun 17 17:54:23 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.939217	80.485746	0.000000
1.508192	86.404356	0.005005
1.662050	79.941754	0.010010
1.525838	84.373418	0.015014
1.686543	75.513500	0.020019
1.369569	76.177195	0.025024
1.220292	65.618289	0.030029
1.150551	58.377296	0.035034
0.582614	60.152823	0.040038
0.301348	40.544425	0.045043
0.024507	44.549935	0.050048
-0.028722	34.631602	0.055053
-0.356805	30.111521	0.060058
-0.750054	28.268390	0.065062
-0.420021	27.411467	0.070067
-1.019387	14.901820	0.075072
-1.529143	11.830343	0.080077
-1.600695	0.313554	0.085082
-1.998605	9.686995	0.090086
-2.483412	-6.609479	0.095091
-2.982244	-2.611285	0.100096
-3.066756	9.658951	0.105101
-2.836853	5.090138	0.110106
-3.381187	9.420702	0.115110
-4.352712	6.160175	0.120115
-4.384083	-0.493799	0.125120
-4.586918	3.087574	0.130125
-4.520525	4.997615	0.135130
-5.011574	12.212958	0.140134
-4.844072	8.044241	0.145139
-4.710598	12.671012	0.150144
-5.121808	4.868173	0.155149
-5.470411	2.413206	0.160154
-6.122454	2.411157	0.165158
-6.037590	6.012198	0.170163
-6.072774	8.326677	0.175168
-6.875393	11.173041	0.180173
-7.328956	1.172486	0.185178
-7.751238	12.707773	0.190182
-7.879115	8.351554	0.195187
-8.404891	15.542084	0.200192
-8.438225	11.545273	0.205197
-7.916304	1.390867	0.210202
-8.014604	12.216974	0.215206
-7.628686	13.146065	0.220211
-8.785097	10.185229	0.225216
-9.382349	14.304963	0.230221
-9.070830	11.158153	0.235226
-9.956840	10.813555	0.240230
-10.678716	5.592904	0.245235
-10.633228	6.943242	0.250240
-10.690920	14.321970	0.255245
-10.618680	8.007542	0.260250
-11.042282	16.450904	0.265254
-10.789583	11.790883	0.270259
-10.951861	4.034679	0.275264
-11.947643	4.087791	0.280269
-12.021717	7.249948	0.285274
-12.385589	14.549922	0.290278
-12.361440	7.065236	0.295283
-12.207740	6.884665	0.300288
-13.296479	12.490088	0.305293
-13.647474	-0.035765	0.310298
-13.991768	9.834321	0.315302
-14.065827	3.083449	0.320307
-14.085086	2.971093	0.325312
-14.097915	18.006629	0.330317
-14.200195	-1.510104	0.335322
-14.507513	12.329821	0.340326
-14.883695	9.249760	0.345331
-14.846546	4.724826	0.350336
-15.281602	10.753004	0.355341
-15.534361	3.199697	0.360346
-16.437239	12.190982	0.365350
-16.870696	12.612182	0.370355
-16.873086	4.172099	0.375360
-17.218021	6.408418	0.380365
-16.860386	5.802646	0.385370
-17.210535	14.662397	0.390374
-17.246497	8.586371	0.395379
-17.131391	2.098473	0.400384
-17.930214	10.441205	0.405389
-18.389165	-5.072417	0.410394
-18.876013	11.475300	0.415398
-18.488960	2.987456	0.420403
-18.750714	8.433321	0.425408
-19.613056	5.811560	0.430413
-20.024496	-3.820080	0.435418
-20.617972	8.998475	0.440422
-20.111493	4.951998	0.445427
-20.088723	12.958276	0.450432
-20.590684	3.907223	0.455437
-20.365082	-0.243720	0.460442
-20.672462	12.432369	0.465446
-21.070735	4.233119	0.470451
-21.622710	5.870623	0.475456
-21.729267	15.178867	0.480461
-21.792999	9.377600	0.485466
-22.104600	10.583452	0.490470
-22.708346	12.808130	0.495475
-23.420520	8.925537	0.500480
-23.570848	8.610011	0.505485
-23.555113	6.215252	0.510490
-23.782379	15.257432	0.515494
-23.461839	12.122737	0.520499
-23.622194	13.917932	0.525504
-24.103341	11.956811	0.530509
-24.018073	10.145441	0.535514
-24.774013	14.828289	0.540518
-24.989862	19.339672	0.545523
-24.894392	12.600478	0.550528
-25.901807	9.026250	0.555533
-26.058332	12.360568	0.560538
-26.586732	12.444133	0.565542
-26.698666	13.311924	0.570547
-26.573955	11.085328	0.575552
-26.514228	18.296346	0.580557
-26.585430	3.395896	0.585562
-26.887989	16.440783	0.590566
-27.742799	10.129689	0.595571
-28.082166	11.302071	0.600576
-28.237405	7.585210	0.605581
-28.168475	3.084396	0.610586
-28.158590	6.679153	0.615590
-28.512359	4.786843	0.620595
-29.320917	-0.437153	0.625600
-29.754894	7.203418	0.630605
-29.610604	-0.758839	0.635610
-29.888412	9.891288	0.640614
-29.966982	2.328171	0.645619
-29.513489	2.899122	0.650624
-30.897391	6.949718	0.655629
-31.065387	-0.089226	0.660634
-31.491462	5.157811	0.665638
-31.519247	12.543603	0.670643
-31.544105	-3.650537	0.675648
-31.638236	2.791403	0.680653
-31.574847	5.088510	0.685658
-31.914105	3.875364	0.690662
-32.686349	6.832515	0.695667
-32.940232	1.022802	0.700672
-33.381451	10.715222	0.705677
-32.878855	-0.267122	0.710682
-33.831543	12.224577	0.715686
-34.806330	16.089960	0.720691
-33.967993	-0.104403	0.725696
-34.386393	8.839899	0.730701
-34.235755	6.569726	0.735706
-34.494488	7.792838	0.740710
-34.818568	10.073446	0.745715
-35.570643	-3.469069	0.750720
-36.187480	3.986807	0.755725
-36.331756	-3.885057	0.760730
-35.992408	2.734254	0.765734
-36.490926	5.131668	0.770739
-36.416774	-2.180176	0.775744
-36.748940	7.890352	0.780749
-36.601633	3.961591	0.785754
-37.104912	11.023670	0.790758
-37.755754	7.155157	0.795763
-37.783625	13.076584	0.800768
-38.300120	8.579544	0.805773
-38.054882	0.167961	0.810778
-37.815586	6.501991	0.815782
-38.822337	9.378345	0.820787
-39.247559	4.109181	0.825792
-39.418795	1.674068	0.830797
-39.624519	0.125762	0.835802
-39.836894	7.696545	0.840806
-40.030684	-1.404343	0.845811
-40.680953	4.724924	0.850816
-41.227900	3.307927	0.855821
-40.843843	9.493775	0.860826
-40.871976	11.664018	0.865830
-40.887637	-2.508237	0.870835
-41.072428	7.938964	0.875840
-41.858454	7.594528	0.880845
-42.260383	6.288004	0.885850
-42.658059	7.474224	0.890854
-42.971795	5.911510	0.895859
-42.854398	5.497218	0.900864
-42.969268	15.613918	0.905869
-42.913635	-4.163284	0.910874
-43.525029	4.977668	0.915878
-43.954738	13.544191	0.920883
-43.732386	-1.043343	0.925888
-44.206081	13.550999	0.930893
-44.041710	8.325908	0.935898
-45.327401	11.153715	0.940902
-45.534970	1.882256	0.945907
-45.821701	13.967661	0.950912
-45.911593	14.000440	0.955917
-45.756635	12.186957	0.960922
-46.225696	4.453534	0.965926
-46.044365	12.452791	0.970931
-46.108765	13.740687	0.975936
-46.995391	8.566176	0.980941
-47.119985	1.515874	0.985946
-47.276924	14.120583	0.990950
-47.495137	14.918623	0.995955
-47.688092	9.672417	1.000960
-48.809380	9.109621	1.005965
-48.850225	9.805955	1.010970
-48.925645	2.589221	1.015974
-49.300416	8.336645	1.020979
-49.151654	8.249441	1.025984
-49.276151	5.841289	1.030989
-48.841083	-1.801875	1.035994
-49.228398	4.766153	1.040998
-49.780032	6.346181	1.046003
-50.079177	5.028887	1.051008
-50.497124	11.751388	1.056013
-50.774387	5.675812	1.061018
-51.813926	17.830906	1.066022
-52.069623	8.754512	1.071027
-51.714249	8.910014	1.076032
-51.865190	8.924131	1.081037
-51.556873	3.171332	1.086042
-52.111443	14.953960	1.091046
-52.443077	-2.215098	1.096051
-52.540822	-0.169639	1.101056
-53.553346	18.607470	1.106061
-53.285995	-0.692068	1.111066
-53.881231	3.804429	1.116070
-53.851913	4.751153	1.121075
-53.686195	5.446698	1.126080
-54.260413	10.641208	1.131085
-54.836976	7.267882	1.136090
-55.223211	8.391226	1.141094
-55.367057	7.550124	1.146099
-55.587452	2.418789	1.151104
-55.596633	8.419392	1.156109
-55.563580	8.492907	1.161114
-56.353165	4.072839	1.166118
-56.914787	9.337281	1.171123
-56.786976	3.657110	1.176128
-57.163873	5.314650	1.181133
-56.960499	8.928747	1.186138
-57.477816	14.381181	1.191142
-57.768765	15.022398	1.196147
-57.438166	6.438957	1.201152
-58.203538	9.689387	1.206157
-58.546673	2.947530	1.211162
-58.883102	3.591176	1.216166
-59.451363	3.295397	1.221171
-59.130301	3.094108	1.226176
-59.255336	7.893490	1.231181
-59.350346	1.972716	1.236186
-59.428824	7.372526	1.241190
-60.411073	8.413797	1.246195
-60.441565	9.698227	1.251200
-61.036210	12.699072	1.256205
-60.659092	9.229970	1.261210
-60.946349	11.941740	1.266214
-61.085213	2.602624	1.271219
-61.499338	4.853209	1.276224
-62.243678	17.418616	1.281229
-61.993973	10.161648	1.286234
-62.177325	5.384281	1.291238
-62.699532	8.062094	1.296243
-62.602527	5.984550	1.301248
-63.074906	11.007624	1.306253
-63.354721	1.493031	1.311258
-63.680279	9.288047	1.316262
-63.453761	9.404980	1.321267
-64.034058	6.312878	1.326272
-64.705272	12.097149	1.331277
-64.807363	1.598730	1.336282
-64.969386	10.446150	1.341286
-65.068283	0.530900	1.346291
-64.839311	2.669651	1.351296
-65.943892	9.188590	1.356301
-65.808372	2.983821	1.361306
-66.168908	0.299379	1.366310
-66.521387	15.076229	1.371315
-66.174726	6.375668	1.376320
-66.842430	4.939282	1.381325
-67.520696	0.052186	1.386330
-67.673003	4.710865	1.391334
-67.916561	7.902576	1.396339
-67.814414	6.003944	1.401344
-68.452325	11.754855	1.406349
-67.964312	5.164517	1.411354
-68.220437	20.379805	1.416358
-69.213868	4.947338	1.421363
-69.244159	10.394785	1.426368
-69.913468	7.582297	1.431373
-69.480693	14.497659	1.436378
-69.463433	11.061144	1.441382
-69.653622	10.275104	1.446387
-70.540501	5.355395	1.451392
-71.166434	17.536258	1.456397
-71.198969	5.010755	1.461402
-71.198489	14.557730	1.466406
-71.423794	7.008351	1.471411
-71.735531	14.620912	1.476416
-71.844529	20.974361	1.481421
-71.913785	6.667158	1.486426
-72.760140	12.458443	1.491430
-72.931614	17.135507	1.496435
-72.879961	10.076034	1.501440
-73.488216	14.305741	1.506445
-73.104999	9.528319	1.511450
-73.241321	11.346159	1.516454
-73.902142	15.794760	1.521459
-74.079419	7.893256	1.526464
-74.476347	9.337066	1.531469
-74.553061	9.521967	1.536474
-74.771420	8.999901	1.541478
-75.089854	17.199446	1.546483
-75.633466	6.753305	1.551488
-76.223714	13.382105	1.556493
-76.200424	8.464225	1.561498
-76.192525	1.027436	1.566502
-76.088977	12.310740	1.571507
-76.473207	2.816466	1.576512
-76.512881	8.766293	1.581517
-77.317458	1.053724	1.586522
-77.637374	4.168145	1.591526
-77.886254	8.428094	1.596531
-77.797625	0.846266	1.601536
-78.110317	4.820039	1.606541
-78.094643	11.759348	1.611546
-79.058815	7.269248	1.616550
-79.196541	13.136909	1.621555
-79.310992	10.214230	1.626560
-79.513119	9.669536	1.631565
-79.439485	4.072370	1.636570
-79.461112	7.878769	1.641574
-80.418933	6.218300	1.646579
-80.462282	3.062991	1.651584
-80.746966	0.334369	1.656589
-80.720007	8.038423	1.661594
-80.932152	1.941965	1.666598
-81.266835	12.767500	1.671603
-81.740993	0.789202	1.676608
-82.390957	17.227288	1.681613
-82.260224	6.133500	1.686618
-82.448951	6.345111	1.691622
-82.418311	11.979956	1.696627
-82.599266	7.752543	1.701632
-83.692225	8.323044	1.706637
-83.833068	2.969517	1.711642
-83.869891	5.557962	1.716646
-83.968268	1.252692	1.721651
-83.938508	5.350488	1.726656
-84.550981	5.506644	1.731661
-84.323919	2.841541	1.736666
-84.979199	-0.401873	1.741670
-85.522608	3.569010	1.746675
-85.538252	-1.051334	1.751680
-85.900729	5.330629	1.756685
-85.865115	3.428652	1.761690
-85.644127	6.775396	1.766694
-86.273618	1.466396	1.771699
-86.851267	-0.412961	1.776704
-87.446275	9.341728	1.781709
-87.207634	-5.130700	1.786714
-87.646397	8.072581	1.791718
-87.502296	-1.909304	1.796723
-87.428378	2.902388	1.801728
-88.066029	9.967666	1.806733
-88.413851	2.765041	1.811738
-88.738674	9.518236	1.816742
-88.911778	6.483359	1.821747
-88.728006	2.099021	1.826752
-89.836141	4.354277	1.831757
-89.628854	1.340426	1.836762
-90.125176	-1.899615	1.841766
-90.676606	0.214554	1.846771
-90.449372	3.975043	1.851776
-90.709825	13.041088	1.856781
-90.675486	2.224197	1.861786
-91.403805	-0.676548	1.866790
-91.901640	7.633522	1.871795
-91.658944	-5.974489	1.876800
-91.848176	8.095419	1.881805
-91.779949	7.810261	1.886810
-92.211446	9.704205	1.891814
-92.769694	16.099181	1.896819
-92.912939	11.207998	1.901824
-93.251985	5.396070	1.906829
-93.476659	5.229458	1.911834
-93.311231	14.598646	1.916838
-94.334751	10.535767	1.921843
-94.393417	5.398072	1.926848
-95.116352	12.863505	1.931853
-95.062424	13.191064	1.936858
-94.967807	5.773798	1.941862
-94.893781	12.967038	1.946867
-94.890003	3.162986	1.951872
-95.404909	9.606204	1.956877
-95.745317	17.347652	1.961882
-96.406500	11.315973	1.966886
-96.874729	12.109008	1.971891
-96.780567	6.654453	1.976896
-96.988783	8.669537	1.981901
-96.853354	4.798988	1.986906
-97.713384	0.561530	1.991910
-98.036523	4.472316	1.996915
-98.172426	4.539002	2.006912
-97.658461	4.207924	2.016909
-97.462111	11.822835	2.026906
-96.864456	7.964646	2.036902
-95.919371	6.243636	2.046899
-95.647148	8.124167	2.056896
-95.742196	1.845567	2.066893
-94.899815	4.048214	2.076890
-94.124276	7.252054	2.086886
-93.162859	2.206786	2.096883
-93.239421	8.475694	2.106880
-92.737004	7.141834	2.116877
-92.466577	7.280389	2.126874
-91.960332	3.981932	2.136870
-91.478423	1.149467	2.146867
-90.373906	6.062629	2.156864
-89.999746	8.403770	2.166861
-89.993286	3.215937	2.176858
-89.172559	6.653119	2.186854
-88.984494	8.312914	2.196851
-88.014649	-0.515269	2.206848
-87.154290	-0.581277	2.216845
-87.370288	-3.101131	2.226842
-87.054606	6.731751	2.236838
-86.050991	7.754906	2.246835
-85.856398	-0.790091	2.256832
-85.346229	1.492876	2.266829
-84.392412	4.525811	2.276826
-83.922854	8.302529	2.286822
-83.879921	14.285237	2.296819
-83.399478	1.891840	2.306816
-82.518252	4.418389	2.316813
-82.321295	4.435593	2.326810
-81.202948	2.858867	2.336806
-81.105180	7.522292	2.346803
-80.727494	6.787885	2.356800
-80.642592	-1.951278	2.366797
-79.448537	3.467432	2.376794
-79.510528	3.938849	2.386790
-78.511496	7.823356	2.396787
-78.041251	-0.913279	2.406784
-77.786314	5.164982	2.416781
-77.146235	2.290024	2.426778
-76.658271	-3.903123	2.436774
-76.264014	-5.135621	2.446771
-75.400327	0.068309	2.456768
-74.748643	2.940849	2.466765
-74.862918	-2.333212	2.476762
-74.609582	4.581085	2.486758
-73.701985	4.913456	2.496755
-73.253250	5.789780	2.506752
-72.152487	3.478011	2.516749
-71.829220	0.264308	2.526746
-71.903749	7.591719	2.536742
-71.645833	4.699477	2.546739
-70.458902	1.525365	2.556736
-70.457893	6.194601	2.566733
-69.086970	6.619085	2.576730
-68.785646	13.025133	2.586726
-68.770629	13.398394	2.596723
-68.604840	11.153726	2.606720
-67.803624	7.261110	2.616717
-67.261497	1.452343	2.626714
-66.388259	3.115410	2.636710
-65.818287	10.065594	2.646707
-65.355133	11.167531	2.656704
-65.715069	8.211037	2.666701
-64.627185	9.515378	2.676698
-64.282710	6.133563	2.686694
-63.648528	4.286418	2.696691
-62.722299	4.586057	2.706688
-62.445746	4.779710	2.716685
-62.203941	7.473805	2.726682
-61.864955	8.263260	2.736678
-61.144404	7.810516	2.746675
-60.865549	7.076337	2.756672
-59.553608	6.587527	2.766669
-59.485543	11.234949	2.776666
-59.432108	8.662598	2.786662
-59.049658	12.922070	2.796659
-57.891880	5.501045	2.806656
-57.517434	4.323805	2.816653
-57.212006	11.891941	2.826650
-56.075637	9.135626	2.836646
-56.040566	17.138533	2.846643
-55.826985	13.736786	2.856640
-55.116037	9.346056	2.866637
-54.514745	3.398632	2.876634
-54.331191	10.356147	2.886630
-53.417179	12.633440	2.896627
-52.925474	10.459074	2.906624
-52.768173	8.960109	2.916621
-52.182082	10.405559	2.926618
-51.646105	10.157567	2.936614
-51.280943	7.097731	2.946611
-50.319688	10.654219	2.956608
-49.631225	10.338598	2.966605
-49.591004	15.332269	2.976602
-49.580427	10.935260	2.986598
-48.405623	11.996359	2.996595
-48.105307	5.612122	3.006592
-47.842962	5.646713	3.016589
-46.832935	5.936379	3.026586
-46.565948	15.233425	3.036582
-46.356736	4.731316	3.046579
-45.329227	5.381824	3.056576
-45.004957	7.434694	3.066573
-44.884185	7.625198	3.076570
-43.867277	10.294185	3.086566
-43.626913	13.933556	3.096563
-43.214773	4.252456	3.106560
-42.462077	2.816540	3.116557
-42.422527	5.634748	3.126554
-41.531212	6.300783	3.136550
-40.819721	1.497614	3.146547
-40.613257	7.310683	3.156544
-40.329108	7.552273	3.166541
-39.406030	10.265113	3.176538
-38.845769	6.511542	3.186534
-38.822169	6.981574	3.196531
-38.053551	10.204362	3.206528
-37.358721	2.874126	3.216525
-37.260045	6.840336	3.226522
-36.471328	10.929143	3.236518
-36.019257	8.180872	3.246515
-35.958654	0.188256	3.256512
-34.870972	7.523821	3.266509
-34.481146	9.958391	3.276506
-34.193609	7.956469	3.286502
-33.111853	7.035289	3.296499
-32.777368	4.189991	3.306496
-32.687856	-2.235271	3.316493
-32.407080	1.860117	3.326490
-31.102288	6.469521	3.336486
-30.938815	4.595509	3.346483
-30.757719	-0.338416	3.356480
-30.053719	2.763721	3.366477
-29.580742	1.273338	3.376474
-29.250813	3.104767	3.386470
-28.228856	10.088501	3.396467
-28.006984	6.957053	3.406464
-27.838430	2.500395	3.416461
-26.633903	4.764377	3.426458
-26.381986	6.273280	3.436454
-26.262728	10.694855	3.446451
-25.787529	10.006680	3.456448
-24.875067	7.839635	3.466445
-24.874791	6.910516	3.476442
-23.856971	4.228251	3.486438
-23.209423	-1.025244	3.496435
-23.114494	-0.954130	3.506432
-22.639718	6.361407	3.516429
-21.871061	0.370954	3.526426
-21.619011	-0.866748	3.536422
-20.994869	-2.274771	3.546419
-20.259570	4.268188	3.556416
-19.866695	2.134162	3.566413
-19.870464	-0.973413	3.576410
-19.035384	-3.426139	3.586406
-18.497264	6.340738	3.596403
-18.008798	3.476170	3.606400
-17.444068	2.324999	3.616397
-16.581153	-1.705894	3.626394
-17.051989	2.812577	3.636390
-16.199633	-2.468637	3.646387
-15.410561	-2.602602	3.656384
-14.982762	4.990444	3.666381
-14.104499	-1.186170	3.676378
-13.742366	-1.772170	3.686374
-13.665478	4.554417	3.696371
-13.276806	1.144119	3.706368
-12.437583	2.369479	3.716365
-12.102404	3.966298	3.726362
-11.671411	2.260024	3.736358
-10.717954	3.277707	3.746355
-10.624215	7.080549	3.756352
-9.830926	6.348989	3.766349
-9.091361	5.223490	3.776346
-9.174690	-3.551731	3.786342
-9.032401	-2.374326	3.796339
-7.913529	0.785311	3.806336
-7.694181	2.796349	3.816333
-6.352599	3.398617	3.826330
-6.494202	4.948231	3.836326
-5.865075	5.019072	3.846323
-5.613392	9.806491	3.856320
-5.082710	16.848182	3.866317
-4.547286	8.080360	3.876314
-4.337935	10.865409	3.886310
-3.528817	26.456430	3.896307
-3.498163	26.471642	3.906304
-2.638602	31.786146	3.916301
-2.393346	42.164441	3.926298
-1.648014	60.790295	3.936294
-1.278940	69.540695	3.946291
-0.776230	80.640277	3.956288
-0.069981	100.337646	3.966285
0.000000	102.159101	3.971290
0.402329	107.930327	3.976294
-0.306268	121.457186	3.981299
0.413501	116.346153	3.986304
0.568914	132.098367	3.991309
0.717103	132.626537	3.996314
0.948507	126.747360	4.001318
0.726226	132.019567	4.006323
0.966288	127.702797	4.011328
0.980726	128.870843	4.016333
0.951986	129.079145	4.021338
1.158094	124.190235	4.026342
0.775670	135.621705	4.031347
1.302709	115.200439	4.036352
0.740893	130.680951	4.041357
0.928388	132.291854	4.046362
0.901788	118.725329	4.051366
1.037105	137.480709	4.056371
1.155054	129.254984	4.061376
0.880754	135.153878	4.066381
1.096768	127.383673	4.071386
0.909186	125.716108	4.076390
0.777644	128.180608	4.081395
1.380484	127.905257	4.086400
1.281365	128.157028	4.091405
0.998458	118.692986	4.096410
0.913348	102.504797	4.101414
0.874528	122.454141	4.106419
0.984518	120.224058	4.111424
1.026086	127.517869	4.116429
1.207925	130.358490	4.121434
1.299131	125.314237	4.126438
0.927448	139.936932	4.131443
1.068707	128.626604	4.136448
0.934034	133.919573	4.141453
1.189775	130.741360	4.146458
1.447901	129.054966	4.151462
1.078662	133.593455	4.156467
1.498189	131.500175	4.161472
1.386117	132.228481	4.166477
1.209655	121.054043	4.171482
0.951501	120.360788	4.176486
1.160507	128.951450	4.181491
1.543520	134.632757	4.186496
1.430744	135.789388	4.191501
1.157885	118.759593	4.196506
1.114877	116.971308	4.201510
0.882363	132.320129	4.206515
1.226051	121.628536	4.211520
1.157515	138.093442	4.216525
1.269257	139.592421	4.221530
1.271535	129.823652	4.226534
1.075128	128.443486	4.231539
1.359380	125.469509	4.236544
0.975336	139.353084	4.241549
0.942500	135.555265	4.246554
1.660924	128.340115	4.251558
1.327749	135.680430	4.256563
0.998471	130.094141	4.261568
1.575020	134.549430	4.266573
1.414747	140.652752	4.271578
1.704446	140.914882	4.276582
1.179235	142.738964	4.281587
1.682853	144.402306	4.286592
1.520233	139.700574	4.291597
1.220956	137.485234	4.296602
1.405308	147.688448	4.301606
1.639426	157.486959	4.306611
1.796572	156.572137	4.311616
1.548139	171.467809	4.316621
1.903845	170.014026	4.321626
1.707011	148.855036	4.326630
1.273417	147.498899	4.331635
1.859750	145.110115	4.336640
1.542123	149.954576	4.341645
1.570648	147.331329	4.346650
1.950759	155.813845	4.351654
1.526142	147.238045	4.356659
1.603907	146.282152	4.361664
1.470534	144.818693	4.366669
1.419774	166.901450	4.371674
1.632855	162.298092	4.376678
1.881828	165.865382	4.381683
1.752519	156.327245	4.386688
1.647882	176.107829	4.391693
1.538449	165.179143	4.396698
1.886529	161.238086	4.401702
1.901374	172.321763	4.406707
2.174928	171.835140	4.411712
1.787014	165.092554	4.416717
1.664068	172.721764	4.421722
2.072132	161.511907	4.426726
1.471752	166.485459	4.431731
1.861980	160.277757	4.436736
2.104345	165.240685	4.441741
1.907045	156.913819	4.446746
1.851132	166.060411	4.451750
1.849911	161.273437	4.456755
1.599864	165.529871	4.461760
2.106163	164.091118	4.466765
1.698938	170.969767	4.471770
1.952227	162.572150	4.476774
1.604950	174.999656	4.481779
1.820452	163.537449	4.486784
1.555231	168.764316	4.491789
1.749675	170.378212	4.496794
2.249416	175.685726	4.501798
1.776797	183.031480	4.506803
2.566430	182.180644	4.511808
2.160138	175.197799	4.516813
1.868024	172.661388	4.521818
2.016207	177.029431	4.526822
1.987444	174.399916	4.531827
2.257843	183.482810	4.536832
2.293213	182.934741	4.541837
1.907237	172.296706	4.546842
2.463770	182.829983	4.551846
2.125820	198.040305	4.556851
2.323711	172.731897	4.561856
2.324429	169.156607	4.566861
2.228207	169.803940	4.571866
2.365906	174.419994	4.576870
2.464200	168.849450	4.581875
2.535318	162.647032	4.586880
2.461887	170.251830	4.591885
2.182782	163.640737	4.596890
2.063644	168.053603	4.601894
1.670313	172.709770	4.606899
2.323714	172.744311	4.611904
2.306112	173.629977	4.616909
2.303295	185.622350	4.621914
2.696565	178.959089	4.626918
2.001579	183.338024	4.631923
2.456969	176.698577	4.636928
2.706099	179.071004	4.641933
2.289719	169.500258	4.646938
2.511802	169.131709	4.651942
2.166996	168.879484	4.656947
2.454003	175.456861	4.661952
2.822399	181.268486	4.666957
2.374544	165.451122	4.671962
2.555132	164.126494	4.676966
2.432143	168.310110	4.681971
2.402203	160.761523	4.686976
2.648607	171.413234	4.691981
2.302652	165.881010	4.696986
2.550839	173.511483	4.701990
2.515861	183.490699	4.706995
2.591953	191.772366	4.712000
2.614284	175.875658	4.717005
2.604742	188.802528	4.722010
2.771310	186.380106	4.727014
2.584290	182.901530	4.732019
2.749802	184.312644	4.737024
2.885692	170.287699	4.742029
2.312980	177.695473	4.747034
2.488113	164.849381	4.752038
2.522964	187.427250	4.757043
2.797382	185.313485	4.762048
2.990778	185.646284	4.767053
2.611585	187.707368	4.772058
2.891791	177.463574	4.777062
2.521731	178.773082	4.782067
2.761053	174.942647	4.787072
2.543195	181.169614	4.792077
2.531694	183.660346	4.797082
2.698991	183.644457	4.802086
2.552934	186.715805	4.807091
2.812193	183.953958	4.812096
2.580714	180.499941	4.817101
2.288573	183.747514	4.822106
2.669708	182.702914	4.827110
2.280814	186.697682	4.832115
2.681309	202.916376	4.837120
2.866343	207.619094	4.842125
2.730008	213.833314	4.847130
3.021272	204.707324	4.852134
3.165934	210.582787	4.857139
3.440404	209.988267	4.862144
3.099737	203.141908	4.867149
2.849464	190.823324	4.872154
2.918919	188.736127	4.877158
3.037465	187.267298	4.882163
2.700701	189.828670	4.887168
2.884105	206.256509	4.892173
3.005044	216.800248	4.897178
3.096521	212.942873	4.902182
3.136922	215.941401	4.907187
3.329266	215.953909	4.912192
3.036951	203.187057	4.917197
2.938620	198.412660	4.922202
3.413971	198.232301	4.927206
3.033783	196.055264	4.932211
3.075688	202.839544	4.937216
3.117659	201.864536	4.942221
3.297967	212.772742	4.947226
3.070986	188.140144	4.952230
2.738209	197.425715	4.957235
3.054009	208.887804	4.962240
3.033204	214.945873	4.967245
2.764213	221.732108	4.972250
2.990135	212.674595	4.977254
2.796572	234.109664	4.982259
2.763174	215.205761	4.987264
3.067714	225.218950	4.992269
2.925114	239.008809	4.997274
3.486227	243.246671	5.002278
3.391102	250.209640	5.007283
3.730549	241.164223	5.012288
3.790381	227.169234	5.017293
3.359341	225.126345	5.022298
3.460277	223.531976	5.027302
3.229253	225.130558	5.032307
3.114900	219.101024	5.037312
3.486704	219.750488	5.042317
3.212869	225.577905	5.047322
3.007850	213.945402	5.052326
3.296646	229.623057	5.057331
3.758409	236.309151	5.062336
3.952901	242.961331	5.067341
3.471153	234.771290	5.072346
3.312105	218.270657	5.077350
3.513987	218.830556	5.082355
3.378713	216.415477	5.087360
3.797963	221.771906	5.092365
3.555059	222.541695	5.097370
3.945214	217.409441	5.102374
3.537818	215.604552	5.107379
3.379427	208.640280	5.112384
3.749338	216.308755	5.117389
3.364712	214.151594	5.122394
3.635685	224.601927	5.127398
3.664128	219.231032	5.132403
3.238136	229.326968	5.137408
3.274132	221.447912	5.142413
3.530609	247.796750	5.147418
4.056839	238.827046	5.152422
3.946214	242.785839	5.157427
3.760127	236.296005	5.162432
3.676119	225.457375	5.167437
3.597936	229.090897	5.172442
3.698951	228.972164	5.177446
3.568808	237.612153	5.182451
3.557694	244.623118	5.187456
3.888348	240.922328	5.192461
3.621748	247.914192	5.197466
3.851459	242.053999	5.202470
3.662140	245.566483	5.207475
3.657446	249.234168	5.212480
3.709073	244.161330	5.217485
3.857771	250.943668	5.222490
3.794755	241.171277	5.227494
3.285124	247.781244	5.232499
3.358924	244.218259	5.237504
3.597014	251.512024	5.242509
3.622148	244.772974	5.247514
4.005334	256.901537	5.252518
3.803224	272.454616	5.257523
3.892507	272.559635	5.262528
3.874161	276.806793	5.267533
4.133000	275.961692	5.272538
4.438366	275.153060	5.277542
3.930957	266.905501	5.282547
3.947793	250.715999	5.287552
4.020758	246.822423	5.292557
3.846950	260.026479	5.297562
4.004092	267.738237	5.302566
3.918811	265.530723	5.307571
3.730470	277.135461	5.312576
3.959426	274.016332	5.317581
3.831652	282.894330	5.322586
3.965801	278.849681	5.327590
4.104345	278.357869	5.332595
4.048117	280.640761	5.337600
4.341659	276.364197	5.342605
4.148638	279.421465	5.347610
4.197171	269.142709	5.352614
4.306158	274.819492	5.357619
4.217666	275.880930	5.362624
4.179015	277.700326	5.367629
3.963616	283.388996	5.372634
4.327688	276.289705	5.377638
4.294097	277.783254	5.382643
3.882058	280.139690	5.387648
4.218163	274.882018	5.392653
4.419235	281.458727	5.397658
4.478084	268.315354	5.402662
4.474092	277.940202	5.407667
4.388316	264.674647	5.412672
4.508322	274.718738	5.417677
4.321442	283.471190	5.422682
4.791030	278.944549	5.427686
4.409755	282.240307	5.432691
4.375652	283.233111	5.437696
4.965632	281.718082	5.442701
4.817233	275.250185	5.447706
4.544004	250.475004	5.452710
3.943373	247.517445	5.457715
4.470832	258.390086	5.462720
4.383242	279.786094	5.467725
4.331977	278.697128	5.472730
4.603652	277.872389	5.477734
4.381980	275.192632	5.482739
4.306920	275.051858	5.487744
4.458950	274.233192	5.492749
4.292836	282.799265	5.497754
4.117763	277.812047	5.502758
3.917835	279.209120	5.507763
4.369880	283.708037	5.512768
4.383019	277.589013	5.517773
4.069396	294.230585	5.522778
4.500369	298.424578	5.527782
4.804657	307.548484	5.532787
4.776401	304.150447	5.537792
4.776127	313.885995	5.542797
4.481544	308.380701	5.547802
4.776010	305.577659	5.552806
4.553278	306.736989	5.557811
4.688535	316.332993	5.562816
4.558580	305.217587	5.567821
4.340017	320.486724	5.572826
4.563766	301.959110	5.577830
4.540734	316.816075	5.582835
4.536314	314.322991	5.587840
4.422939	301.704114	5.592845
4.751866	310.516679	5.597850
4.997996	301.163308	5.602854
4.575769	308.740899	5.607859
4.762739	308.281688	5.612864
4.707197	311.119174	5.617869
4.873141	326.559629	5.622874
5.016562	311.659513	5.627878
4.700356	313.383953	5.632883
4.859825	313.103754	5.637888
4.853265	306.512025	5.642893
4.990896	314.107072	5.647898
5.183107	300.919799	5.652902
4.980227	311.893738	5.657907
4.780381	302.632647	5.662912
5.026810	302.721216	5.667917
4.768791	305.643266	5.672922
5.049919	303.582242	5.677926
4.812347	305.525280	5.682931
5.037305	308.463749	5.687936
5.303387	308.455910	5.692941
5.058161	314.016349	5.697946
5.269561	309.413621	5.702950
4.778576	315.213425	5.707955
5.033994	309.341633	5.712960
5.178408	305.382887	5.717965
4.871305	315.653887	5.722970
5.158449	302.562919	5.727974
5.163637	312.321041	5.732979
5.238276	301.743503	5.737984
5.116871	305.438888	5.742989
4.860262	307.182232	5.747994
4.992940	317.494787	5.752998
5.253961	323.558942	5.758003
5.584849	328.764335	5.763008
5.430428	313.867348	5.768013
5.300192	307.963949	5.773018
5.252268	307.238703	5.778022
5.175606	314.949090	5.783027
5.099251	312.620501	5.788032
5.169574	304.113111	5.793037
5.159312	330.578254	5.798042
5.450070	324.778332	5.803046
5.294008	332.154421	5.808051
5.213773	336.982176	5.813056
5.530505	332.677075	5.818061
5.465426	330.498161	5.823066
5.252118	317.058399	5.828070
5.327524	317.444950	5.833075
5.474011	325.984546	5.838080
5.465097	330.620477	5.843085
5.343341	328.464402	5.848090
5.741603	319.992086	5.853094
5.151595	320.080954	5.858099
5.365942	327.927288	5.863104
5.371712	330.101019	5.868109
5.177285	339.756373	5.873114
5.305464	331.035310	5.878118
5.232863	336.741705	5.883123
5.026234	338.395049	5.888128
5.441248	336.453848	5.893133
5.128054	344.465228	5.898138
5.161980	339.723663	5.903142
5.117315	349.059907	5.908147
5.325304	361.752052	5.913152
5.909948	363.539887	5.918157
5.621976	365.568862	5.923162
6.081774	360.880432	5.928166
5.618708	355.012404	5.933171
5.239865	343.449543	5.938176
5.351059	360.783470	5.943181
5.309022	366.456972	5.948186
5.595743	362.624730	5.953190
6.048312	373.995735	5.958195
5.801931	376.836141	5.963200
5.913773	366.060173	5.968205
6.189004	371.979905	5.973210
6.039493	354.429502	5.978214
5.784440	345.196110	5.983219
6.060503	343.791465	5.988224
5.909333	345.668643	5.993229
5.457443	344.889966	5.998234
5.452996	332.863706	6.003238
5.653060	338.416249	6.008243
5.581554	344.059910	6.013248
5.642154	332.094471	6.018253
5.290683	340.653496	6.023258
5.809095	354.708131	6.028262
5.879132	357.805164	6.033267
5.664832	356.399338	6.038272
5.885322	353.025067	6.043277
5.691573	339.630380	6.048282
5.800928	335.814009	6.053286
5.730275	345.589690	6.058291
5.525285	336.143743	6.063296
5.521605	345.932762	6.068301
5.603870	357.631112	6.073306
5.663980	360.130888	6.078310
5.842910	368.982033	6.083315
5.776824	372.157144	6.088320
6.166377	358.050994	6.093325
5.666976	356.811152	6.098330
5.645900	345.724388	6.103334
5.912237	347.565522	6.108339
5.686667	352.705150	6.113344
5.773664	341.912410	6.118349
5.307861	336.683613	6.123354
5.873075	342.377733	6.128358
5.621286	333.626089	6.133363
5.284243	341.387857	6.138368
5.694867	359.504170	6.143373
5.510485	365.108386	6.148378
5.720894	363.603947	6.153382
5.558624	367.939186	6.158387
5.925571	374.680567	6.163392
6.015900	369.371756	6.168397
5.850819	377.967113	6.173402
6.020179	367.488635	6.178406
5.552798	351.881723	6.183411
5.519128	367.538128	6.188416
6.076098	361.789257	6.193421
5.259443	355.496926	6.198426
5.841608	363.592746	6.203430
5.867379	366.101388	6.208435
5.849135	369.553695	6.213440
5.773417	357.322589	6.218445
5.560213	358.725625	6.223450
5.670402	347.581719	6.228454
5.570711	361.780338	6.233459
5.573150	371.236244	6.238464
5.961746	363.686074	6.243469
5.774546	380.581020	6.248474
5.814394	370.375865	6.253478
5.761345	376.457709	6.258483
5.552932	365.813706	6.263488
5.723627	360.653552	6.268493
5.632906	374.345911	6.273498
6.170652	372.193288	6.278502
5.780488	346.505775	6.283507
5.523930	346.255651	6.288512
5.688344	349.653322	6.293517
5.146832	352.859893	6.298522
5.858700	359.752717	6.303526
5.937120	369.616314	6.308531
5.833305	367.724245	6.313536
5.889977	365.858584	6.318541
5.925912	344.668332	6.323546
5.837863	342.503298	6.328550
5.912743	341.134854	6.333555
5.457180	344.645437	6.338560
5.813651	339.172619	6.343565
5.432704	341.330116	6.348570
5.437406	335.229046	6.353574
5.472953	343.988174	6.358579
5.813213	367.226339	6.363584
6.007667	357.664062	6.368589
5.666640	357.099615	6.373594
5.656158	345.601031	6.378598
6.119058	348.978493	6.383603
5.712488	349.744312	6.388608
5.839552	345.904472	6.393613
5.291152	356.354527	6.398618
5.556329	340.802481	6.403622
5.774799	357.084152	6.408627
5.933053	367.263630	6.413632
5.955640	349.063422	6.418637
5.630392	348.848593	6.423642
5.875062	340.112898	6.428646
5.691202	341.415941	6.433651
5.806251	339.823359	6.438656
5.697768	345.322996	6.443661
5.372361	341.198820	6.448666
5.754530	345.940053	6.453670
5.736509	343.309907	6.458675
5.573064	344.957653	6.463680
5.884284	342.942140	6.468685
5.691299	347.859086	6.473690
5.851500	343.916650	6.478694
5.852619	351.223802	6.483699
5.181150	344.207402	6.488704
6.023669	354.845014	6.493709
5.990924	350.589707	6.498714
6.088457	347.451362	6.503718
5.953537	339.707805	6.508723
5.818048	338.890946	6.513728
5.726049	339.839898	6.518733
5.573994	341.143969	6.523738
6.002601	349.567226	6.528742
5.614161	341.373458	6.533747
5.710237	344.272577	6.538752
5.717585	340.544987	6.543757
5.414380	351.611406	6.548762
5.456074	340.845338	6.553766
5.629643	339.307953	6.558771
5.198479	347.339731	6.563776
5.780032	348.064253	6.568781
5.612576	354.513595	6.573786
5.194879	359.373964	6.578790
5.977154	361.398509	6.583795
5.828885	369.094382	6.588800
6.063543	369.465516	6.593805
5.443846	362.835170	6.598810
5.666937	358.392101	6.603814
5.783417	362.289892	6.608819
5.675183	365.815763	6.613824
5.706030	359.995288	6.618829
5.749778	380.264735	6.623834
6.152331	369.121555	6.628838
5.823582	360.804389	6.633843
5.467261	355.330059	6.638848
5.694070	348.443780	6.643853
5.478610	350.393014	6.648858
5.578607	356.924789	6.653862
5.643382	367.036925	6.658867
5.749649	373.963714	6.663872
5.987027	366.384804	6.668877
5.715017	371.035665	6.673882
5.813803	370.467775	6.678886
5.504406	358.363124	6.683891
5.561740	365.388224	6.688896
5.835324	360.397448	6.693901
5.790191	365.335410	6.698906
5.931786	366.606857	6.703910
5.944010	350.385259	6.708915
5.133514	347.209976	6.713920
5.491568	354.018933	6.718925
5.515712	374.948160	6.723930
6.070158	367.597751	6.728934
5.883127	380.087784	6.733939
5.575882	368.232987	6.738944
6.056640	370.723628	6.743949
5.796481	384.866257	6.748954
5.844321	365.744426	6.753958
5.519265	358.854752	6.758963
5.635917	357.386222	6.763968
5.713836	365.136654	6.768973
5.638538	376.206254	6.773978
5.761034	375.457218	6.778982
6.130252	366.630359	6.783987
5.467832	358.347934	6.788992
5.661347	354.994130	6.793997
5.649235	363.837361	6.799002
5.673788	363.083094	6.804006
6.088559	375.236496	6.809011
5.694313	365.945912	6.814016
5.989632	348.449256	6.819021
5.483183	343.208268	6.824026
5.561803	344.471039	6.829030
5.765245	345.862050	6.834035
5.718641	352.710440	6.839040
5.725227	335.777223	6.844045
5.715850	350.688389	6.849050
5.687713	347.427865	6.854054
5.690443	347.506225	6.859059
5.845913	353.606287	6.864064
5.620865	348.698590	6.869069
5.407054	351.020906	6.874074
5.587646	365.012707	6.879078
5.938580	368.249535	6.884083
5.808434	369.550756	6.889088
6.241662	362.993058	6.894093
5.644410	355.545181	6.899098
5.489721	347.436879	6.904102
5.629870	340.047795	6.909107
5.637798	350.760777	6.914112
5.582078	349.081137	6.919117
5.480862	359.207438	6.924122
5.527205	362.778262	6.929126
6.106027	366.367736	6.934131
5.778875	371.589374	6.939136
5.808335	369.465190	6.944141
5.615796	370.833219	6.949146
5.634940	362.955707	6.954150
6.114385	378.286684	6.959155
5.493414	352.841368	6.964160
6.021448	357.743459	6.969165
5.937834	355.880988	6.974170
5.617824	351.877470	6.979174
5.414348	341.412829	6.984179
5.510815	349.463669	6.989184
5.812465	355.565089	6.994189
6.083147	371.887430	6.999194
5.847690	359.133101	7.004198
5.873484	357.138978	7.009203
5.765754	350.965027	7.014208
5.301463	338.975528	7.019213
5.519691	346.049456	7.024218
5.752106	344.393953	7.029222
5.705544	337.774918	7.034227
5.738395	342.639329	7.039232
6.152897	347.540159	7.044237
5.647016	341.756410	7.049242
5.980948	340.436274	7.054246
5.971286	341.736214	7.059251
5.474781	343.768864	7.064256
5.905278	338.157055	7.069261
5.768885	341.582225	7.074266
5.665229	335.299267	7.079270
5.645476	335.614217	7.084275
5.469766	340.845602	7.089280
5.420729	339.251877	7.094285
5.546772	346.852813	7.099290
5.892291	341.059372	7.104294
5.612963	341.161919	7.109299
5.810319	351.136568	7.114304
5.740970	342.979156	7.119309
5.447589	346.182174	7.124314
5.841531	344.894096	7.129318
5.956064	343.444469	7.134323
5.519549	344.901196	7.139328
5.704582	343.866486	7.144333
5.447553	351.034208	7.149338
5.573475	360.093663	7.154342
5.969266	370.683584	7.159347
5.703317	366.790463	7.164352
6.022824	364.027648	7.169357
5.805717	350.279858	7.174362
5.737817	342.800244	7.179366
5.874062	343.879586	7.184371
4.984306	349.731868	7.189376
5.602303	355.556932	7.194381
5.616020	369.306916	7.199386
5.978738	371.604451	7.204390
6.103486	369.677549	7.209395
5.901722	358.853070	7.214400
6.111716	342.658796	7.219405
5.867768	348.833334	7.224410
5.529752	349.134878	7.229414
5.706605	344.217215	7.234419
5.751875	342.712401	7.239424
5.996798	337.425464	7.244429
5.676339	340.165301	7.249434
5.731720	338.341890	7.254438
5.894859	343.352775	7.259443
5.553742	341.330049	7.264448
6.125915	339.672934	7.269453
5.973315	354.569034	7.274458
5.793193	344.463998	7.279462
5.995841	347.379346	7.284467
5.445407	347.825124	7.289472
5.545254	342.775812	7.294477
5.467660	344.876969	7.299482
5.339017	341.986378	7.304486
5.421908	350.181159	7.309491
5.637384	352.169078	7.314496
5.681468	349.589585	7.319501
5.872171	346.348336	7.324506
5.379452	351.261033	7.329510
5.697492	344.018204	7.334515
5.435861	344.434333	7.339520
5.791066	349.178469	7.344525
5.918148	360.311510	7.349530
5.837017	347.984222	7.354534
6.050026	340.945136	7.359539
5.617617	349.903405	7.364544
5.503483	340.028743	7.369549
6.089980	346.669291	7.374554
5.736474	334.693547	7.379558
6.010537	338.870612	7.384563
5.573213	342.830451	7.389568
5.839511	341.539119	7.394573
5.687527	346.884371	7.399578
5.527217	345.697295	7.404582
5.745302	345.329209	7.409587
5.343721	351.303015	7.414592
5.784502	348.937998	7.419597
5.810166	345.543620	7.424602
5.663147	347.197121	7.429606
5.770918	340.993868	7.434611
5.833614	340.533013	7.439616
5.778343	333.705266	7.444621
5.491305	355.062700	7.449626
5.783781	341.553255	7.454630
5.696232	344.695620	7.459635
5.409289	346.442233	7.464640
5.587080	348.082991	7.469645
5.962197	340.528955	7.474650
5.717758	348.726637	7.479654
5.635856	350.971183	7.484659
5.803227	347.337171	7.489664
5.841470	349.138862	7.494669
5.700915	350.253160	7.499674
6.021215	355.224706	7.504678
6.066735	348.873140	7.509683
5.701144	350.740570	7.514688
5.840109	338.762496	7.519693
5.615525	354.216384	7.524698
5.663192	344.292133	7.529702
6.078660	345.814453	7.534707
5.755552	346.504042	7.539712
5.745224	340.517160	7.544717
5.578816	349.845618	7.549722
5.601842	344.065916	7.554726
5.633649	347.002949	7.559731
5.645661	353.122317	7.564736
5.763337	338.932316	7.569741
5.476977	345.222041	7.574746
5.604585	344.385921	7.579750
5.688411	348.931259	7.584755
5.453198	347.936798	7.589760
6.009677	337.824185	7.594765
5.767141	343.457003	7.599770
5.545423	350.737651	7.604774
5.629587	342.962809	7.609779
5.318856	353.305477	7.614784
5.528841	354.356974	7.619789
5.702505	358.101797	7.624794
5.802101	372.263553	7.629798
6.057267	369.008230	7.634803
5.757579	358.469980	7.639808
5.835282	355.377159	7.644813
5.641187	355.910724	7.649818
5.595526	346.649632	7.654822
5.818000	347.928552	7.659827
5.594105	352.445315	7.664832
5.426523	341.213198	7.669837
5.769623	357.276426	7.674842
5.709477	371.238587	7.679846
5.510875	354.984538	7.684851
5.569926	381.110871	7.689856
5.565145	380.440412	7.694861
5.916511	376.959135	7.699866
5.653525	378.789387	7.704870
5.933767	382.540972	7.709875
5.579587	392.331642	7.714880
5.905835	373.929775	7.719885
6.022239	378.263099	7.724890
5.640006	369.282501	7.729894
5.735431	350.827661	7.734899
5.464516	359.884599	7.739904
5.406045	367.799189	7.744909
5.582647	376.985009	7.749914
5.675699	383.189389	7.754918
5.746094	371.381737	7.759923
5.621089	381.808402	7.764928
5.996419	376.486160	7.769933
5.933827	384.579439	7.774938
6.033203	385.032062	7.779942
6.033265	361.386798	7.784947
5.775214	361.164351	7.789952
5.597910	349.662708	7.794957
5.802037	352.889992	7.799962
5.700031	355.276211	7.804966
5.569551	351.658157	7.809971
5.141935	359.420386	7.814976
5.787696	365.306551	7.819981
5.582396	374.839611	7.824986
5.626643	376.480072	7.829990
5.956882	381.074053	7.834995
5.854925	383.705751	7.840000
6.225253	378.941414	7.845005
5.536107	362.324099	7.850010
5.275690	362.496714	7.855014
5.872061	358.643395	7.860019
5.488709	377.528096	7.865024
5.735917	380.267717	7.870029
5.807549	381.586117	7.875034
5.516447	376.229010	7.880038
5.618394	384.593901	7.885043
5.651497	384.290897	7.890048
5.942311	380.959790	7.895053
6.252096	374.417672	7.900058
5.771625	366.516639	7.905062
5.781141	355.036628	7.910067
5.463761	361.090965	7.915072
5.699862	355.446538	7.920077
5.745165	362.827850	7.925082
5.424963	361.988805	7.930086
5.801373	363.007116	7.935091
5.739101	385.617007	7.940096
5.979013	373.559572	7.945101
5.673746	358.708531	7.950106
5.656477	360.364740	7.955110
5.675098	357.429739	7.960115
5.830398	373.678907	7.965120
5.989150	374.486137	7.970125
5.218471	363.226232	7.975142
5.755181	365.346720	7.980160
6.054629	377.426111	7.985178
5.665470	372.804140	7.990195
5.867126	359.880477	7.995213
5.392928	361.866656	8.000230
5.767944	370.865882	8.005248
5.940069	368.624583	8.010266
5.766164	378.793679	8.015283
5.914437	368.443780	8.020301
5.786558	358.536597	8.025318
5.388984	361.570956	8.030336
5.614925	358.965238	8.035354
5.709147	369.392292	8.040371
5.968483	380.810310	8.045389
5.819713	384.410344	8.050406
5.790708	388.953173	8.055424
5.877722	386.424867	8.060442
5.870954	380.831947	8.065459
5.814651	383.442695	8.070477
5.979831	384.722470	8.075494
5.777545	383.138812	8.080512
5.865488	362.651151	8.085530
5.485050	375.375576	8.090547
5.891015	376.317328	8.095565
6.133257	380.529469	8.100582
5.902756	378.085235	8.105600
6.013763	362.760541	8.110618
5.829562	365.609648	8.115635
5.788178	364.715318	8.120653
5.981766	365.608322	8.125670
5.519039	368.995799	8.130688
5.915738	372.517766	8.135706
6.287110	376.216958	8.140723
6.343213	360.677202	8.145741
5.895761	352.377705	8.150758
5.594156	361.213233	8.155776
5.466707	354.793026	8.160794
6.064001	361.255558	8.165811
5.981920	373.318249	8.170829
5.988132	360.473325	8.175846
5.921680	365.409536	8.180864
5.989600	353.612915	8.185882
5.739994	361.016324	8.190899
5.737608	371.067153	8.195917
6.379197	380.451364	8.200934
5.773941	366.450320	8.205952
5.632283	372.009797	8.210970
5.787156	382.219910	8.215987
5.960707	380.683026	8.221005
6.155965	371.724977	8.226022
5.983252	383.589376	8.231040
6.223067	373.015028	8.236058
6.152519	380.654604	8.241075
5.938815	381.091538	8.246093
5.813582	369.085695	8.251110
5.924040	384.198167	8.256128
6.197933	377.699238	8.261146
6.275846	388.643333	8.266163
6.292535	378.068866	8.271181
6.189356	363.842853	8.276198
5.841564	361.800754	8.281216
5.894151	350.952060	8.286234
6.061888	366.183917	8.291251
5.916144	367.427780	8.296269
6.289278	359.861879	8.301286
6.119287	368.238179	8.306304
5.876725	360.510073	8.311322
5.793511	360.919610	8.316339
5.857207	374.623848	8.321357
5.874105	375.829262	8.326374
5.982772	389.516984	8.331392
6.024759	384.224984	8.336410
6.047990	377.427594	8.341427
5.722732	386.127711	8.346445
6.110895	385.075970	8.351462
5.873879	390.274963	8.356480
6.139363	384.736781	8.361498
5.975108	380.285476	8.366515
5.848608	382.930724	8.371533
6.261398	374.489416	8.376550
5.975677	388.543838	8.381568
5.859236	380.723900	8.386586
5.850180	388.147374	8.391603
5.984648	397.440902	8.396621
6.488134	409.793854	8.401638
6.127326	406.780584	8.406656
6.478267	390.183430	8.411674
6.337811	377.684490	8.416691
5.913743	381.386772	8.421709
6.246096	377.673514	8.426726
6.201343	388.249650	8.431744
6.206900	374.169515	8.436762
6.198817	382.346685	8.441779
6.011439	384.597958	8.446797
6.307209	379.650354	8.451814
6.259426	384.949375	8.456832
6.291295	384.163919	8.461850
6.242410	385.401723	8.466867
6.473874	386.526401	8.471885
6.363010	379.806607	8.476902
6.098434	379.648317	8.481920
6.209976	379.749529	8.486938
6.255967	389.718911	8.491955
6.340670	384.325529	8.496973
6.321851	374.071502	8.501990
6.019049	386.310442	8.507008
6.471004	377.103053	8.512026
6.256731	374.899011	8.517043
6.343174	388.517598	8.522061
6.703565	386.889823	8.527078
6.191685	387.074182	8.532096
6.306323	380.573968	8.537114
6.109949	384.676944	8.542131
6.119864	381.819755	8.547149
6.480840	380.259986	8.552166
6.440553	386.616121	8.557184
6.141679	377.306187	8.562202
5.982037	390.374399	8.567219
6.113614	408.187838	8.572237
6.777528	412.716871	8.577255
6.393415	418.910109	8.582272
6.509061	413.429692	8.587290
6.765356	403.671204	8.592307
6.306506	398.952945	8.597325
6.110266	379.931645	8.602343
6.306562	392.320682	8.607360
6.588877	402.029949	8.612378
6.523819	386.071177	8.617395
6.110642	380.275164	8.622413
6.710309	397.789750	8.627431
6.535141	393.636485	8.632448
6.467450	375.300447	8.637466
6.446022	378.230365	8.642483
6.013931	387.721980	8.647501
6.337515	396.658714	8.652519
6.332686	410.729455	8.657536
6.431479	417.094766	8.662554
6.504806	411.112969	8.667571
6.456887	412.797420	8.672589
6.699989	412.842320	8.677607
6.259933	421.031471	8.682624
6.374176	417.040511	8.687642
6.509728	412.913738	8.692659
6.390509	410.575596	8.697677
6.657052	410.438468	8.702695
6.340390	415.982761	8.707712
6.594473	418.807845	8.712730
6.512886	420.252444	8.717747
6.551028	429.063231	8.722765
6.750979	413.312722	8.727783
6.448678	415.877757	8.732800
6.441836	413.580182	8.737818
6.584082	410.453971	8.742835
6.196870	417.203573	8.747853
6.659269	424.959885	8.752871
6.322075	422.139517	8.757888
6.202637	412.174603	8.762906
6.292674	422.894288	8.767923
6.224765	418.577929	8.772941
6.244994	420.466584	8.777959
6.557479	420.434800	8.782976
6.319129	420.014696	8.787994
6.694279	425.948092	8.793011
6.646959	432.772888	8.798029
6.579034	434.211281	8.803047
6.496729	440.564580	8.808064
6.630629	441.169900	8.813082
6.913387	429.835102	8.818099
6.799446	437.645485	8.823117
6.807523	418.791536	8.828135
6.719504	422.978667	8.833152
6.591144	416.345419	8.838170
6.709878	420.830043	8.843187
6.448806	423.638792	8.848205
6.617398	405.423666	8.853223
6.722496	418.154622	8.858240
6.261458	433.303670	8.863258
6.831760	434.191343	8.868275
6.645165	439.392601	8.873293
7.048295	441.451452	8.878311
6.842504	435.627642	8.883328
6.886284	427.618861	8.888346
6.891888	414.102799	8.893363
6.477433	419.155918	8.898381
6.254360	426.147114	8.903399
6.607107	432.599146	8.908416
6.855007	441.610486	8.913434
7.259367	435.758484	8.918451
6.957890	439.302425	8.923469
6.871612	421.433746	8.928487
7.118875	422.495571	8.933504
6.723370	420.799156	8.938522
7.277019	409.994292	8.943539
6.877243	416.042508	8.948557
7.022053	410.304121	8.953575
7.053989	417.694420	8.958592
7.113317	415.414978	8.963610
7.011104	412.776795	8.968627
6.576137	417.709712	8.973645
6.749241	426.401421	8.978663
6.778282	420.987360	8.983680
6.614798	424.915999	8.988698
6.705209	407.692706	8.993715
6.720830	418.474161	8.998733
6.912681	411.495399	9.003751
7.005218	408.559125	9.008768
6.828675	420.494063	9.013786
7.053108	414.764485	9.018803
7.021807	419.283887	9.023821
6.835412	404.446336	9.028839
6.984477	406.267320	9.033856
6.752251	406.435314	9.038874
6.846070	405.694279	9.043891
6.818006	414.860123	9.048909
6.944320	403.720227	9.053927
6.966925	406.466078	9.058944
6.706837	410.331644	9.063962
6.892874	397.198952	9.068979
6.673631	407.301201	9.073997
6.863216	404.074415	9.079015
7.087387	407.972276	9.084032
6.818258	411.846234	9.089050
6.913093	402.564145	9.094067
6.776559	400.039137	9.099085
6.785222	408.310181	9.104103
6.350951	411.872054	9.109120
6.625210	422.964033	9.114138
7.056449	429.228231	9.119155
7.073431	441.131414	9.124173
6.692262	435.222591	9.129191
7.044521	427.134588	9.134208
6.930007	440.270137	9.139226
6.810147	429.352225	9.144243
6.604145	439.129097	9.149261
6.716978	434.409500	9.154279
6.843454	434.803082	9.159296
6.976680	433.247308	9.164314
7.076494	429.152846	9.169331
6.780828	433.442597	9.174349
6.910008	459.344683	9.179367
7.326117	461.795241	9.184384
7.265573	467.011380	9.189402
7.343637	459.581278	9.194419
6.662044	447.594034	9.199437
7.224713	455.273267	9.204455
7.279723	463.037867	9.209472
7.341128	465.569228	9.214490
7.280759	447.599765	9.219507
6.820053	452.057096	9.224525
6.899247	454.375282	9.229543
7.271672	459.663930	9.234560
7.189786	467.928995	9.239578
7.297524	468.700854	9.244595
7.251376	471.204428	9.249613
7.021480	461.793223	9.254631
7.303336	466.787114	9.259648
6.898295	473.809166	9.264666
7.624547	473.662159	9.269683
7.275494	455.380664	9.274701
7.166450	458.318073	9.279719
7.200840	442.889708	9.284736
6.782413	463.507356	9.289754
7.208182	466.919799	9.294771
7.552587	479.330151	9.299789
7.615603	474.326329	9.304807
7.396123	462.502598	9.309824
7.147290	458.544023	9.314842
7.222503	444.610892	9.319859
7.217832	440.616660	9.324877
7.161594	445.356139	9.329895
7.244214	445.666862	9.334912
7.114346	454.369578	9.339930
7.389905	472.407167	9.344947
7.334287	481.300293	9.349965
7.261168	478.192149	9.354983
7.546751	462.897194	9.360000
7.426388	468.339004	9.365018
7.768124	457.735651	9.370035
7.571423	449.916028	9.375053
7.261962	459.189292	9.380071
7.537386	447.825782	9.385088
7.078078	453.030053	9.390106
7.214819	438.190331	9.395123
7.096607	447.376491	9.400141
6.985849	443.042446	9.405159
7.197968	458.516600	9.410176
7.294495	467.998545	9.415194
7.517572	475.147477	9.420211
7.596067	482.027163	9.425229
7.494050	478.455166	9.430247
7.438783	471.217872	9.435264
7.699707	461.134200	9.440282
7.543248	452.188308	9.445299
7.095094	443.355858	9.450317
7.089193	449.819481	9.455335
7.378920	452.438470	9.460352
7.170361	479.776317	9.465370
7.540791	469.944098	9.470387
7.489601	482.315686	9.475405
7.035732	482.779156	9.480423
7.863402	471.901936	9.485440
7.504673	482.287629	9.490458
7.419350	471.885747	9.495475
7.379365	479.694684	9.500493
7.149288	477.560176	9.505511
7.483276	479.012867	9.510528
7.311502	476.400406	9.515546
7.398179	482.024521	9.520563
7.337340	475.908517	9.525581
7.183300	483.989736	9.530599
7.092257	472.066901	9.535616
7.492748	488.949798	9.540634
7.613199	497.518815	9.545651
7.700935	507.587624	9.550669
7.715918	501.508414	9.555687
7.646240	492.549059	9.560704
7.515985	492.288135	9.565722
7.387703	496.359549	9.570739
7.549278	498.327467	9.575757
7.764731	503.976638	9.580775
7.959693	504.383247	9.585792
7.686885	496.957906	9.590810
7.508964	482.011205	9.595827
7.652587	480.300956	9.600845
7.318862	486.227995	9.605863
7.528482	491.482499	9.610880
7.711127	500.682854	9.615898
7.734840	510.662906	9.620915
7.881569	505.520959	9.625933
7.666056	503.920985	9.630951
7.741962	499.761194	9.635968
7.974637	500.963822	9.640986
7.731324	487.367033	9.646003
7.424358	477.897769	9.651021
7.070408	494.095512	9.656039
7.512182	497.134274	9.661056
7.782886	509.157921	9.666074
7.778002	518.855160	9.671091
7.485679	510.120775	9.676109
7.783491	506.538216	9.681127
8.007522	504.285122	9.686144
8.124477	512.421304	9.691162
7.901539	506.152917	9.696179
8.296756	495.695557	9.701197
8.101741	493.278080	9.706215
7.975271	481.551659	9.711232
7.535450	475.691148	9.716250
7.728110	478.629001	9.721267
7.829402	473.569413	9.726285
7.507105	482.553711	9.731303
8.106780	482.237208	9.736320
7.743801	489.511504	9.741338
7.862117	483.489332	9.746355
7.854664	486.572838	9.751373
7.554582	487.683125	9.756391
8.023285	499.901000	9.761408
8.150673	500.825092	9.766426
7.730146	488.967636	9.771443
7.764776	488.138019	9.776461
7.778927	496.052523	9.781479
7.651005	507.218691	9.786496
8.123734	500.603206	9.791514
8.253655	503.100746	9.796531
7.799616	488.220600	9.801549
7.624046	501.228173	9.806567
8.176399	504.488298	9.811584
8.182306	500.382067	9.816602
7.854151	502.960467	9.821619
7.961748	496.625533	9.826637
8.223256	504.439879	9.831655
8.195473	494.396494	9.836672
8.160955	485.645650	9.841690
7.775283	486.873499	9.846707
7.904832	488.979404	9.851725
7.528780	483.910183	9.856743
7.989938	487.185266	9.861760
7.979743	503.974445	9.866778
7.813559	516.766515	9.871795
7.904741	505.698325	9.876813
8.047571	519.832607	9.881831
7.730370	511.227740	9.886848
7.968906	508.643327	9.891866
7.977415	519.376039	9.896883
8.315060	509.878151	9.901901
7.954723	514.740432	9.906919
7.926058	509.535912	9.911936
7.941234	503.483635	9.916954
7.567062	518.485073	9.921971
7.875279	504.550953	9.926989
8.012090	517.937288	9.932007
7.934130	507.200922	9.937024
8.152510	512.872443	9.942042
8.199899	517.540984	9.947059
8.671649	519.095573	9.952077
8.041200	518.107230	9.957095
8.077004	513.587993	9.962112
8.146727	513.067080	9.967130
8.122562	514.732044	9.972147
8.255227	505.751845	9.977165
8.177736	504.810166	9.982183
7.861077	503.976737	9.987200
8.249613	514.782097	9.992218
8.103924	522.307077	9.997235
8.323918	527.126248	10.002253
8.389638	529.804526	10.007271
8.608178	520.273480	10.012288
8.417878	520.898636	10.017306
7.866514	508.319673	10.022323
8.114923	504.463856	10.027341
8.008004	508.955305	10.032359
8.653992	515.508423	10.037376
8.170547	510.482237	10.042394
8.008342	515.972353	10.047411
8.527761	518.836418	10.052429
8.348849	519.398466	10.057447
8.387844	518.002426	10.062464
8.247078	505.971502	10.067482
8.230244	510.854634	10.072499
8.387603	511.889089	10.077517
8.435697	517.399955	10.082535
8.298393	498.849968	10.087552
8.294950	504.135559	10.092570
8.221816	516.011065	10.097587
8.380700	521.102767	10.102605
8.291117	538.481505	10.107623
8.212252	531.663618	10.112640
8.260508	529.925124	10.117658
8.342018	530.327561	10.122675
8.505831	528.905656	10.127693
8.506056	529.907573	10.132711
8.806456	533.230249	10.137728
8.470162	530.631739	10.142746
8.650891	530.320701	10.147763
8.692599	515.582913	10.152781
8.617713	513.877091	10.157799
8.219251	510.607287	10.162816
8.472739	507.972363	10.167834
8.309991	504.416358	10.172851
8.553811	494.144187	10.177869
8.633383	506.078745	10.182887
8.350354	503.951656	10.187904
8.392658	506.773968	10.192922
8.184880	524.013687	10.197939
8.651545	520.856562	10.202957
8.239795	538.676606	10.207975
8.392664	538.874483	10.212992
8.783721	533.128583	10.218010
8.392784	534.374633	10.223027
8.785390	531.693749	10.228045
8.647826	539.321512	10.233063
8.846524	530.567309	10.238080
8.755464	531.083460	10.243098
8.329550	543.622291	10.248115
8.815211	540.336229	10.253133
8.517784	535.829068	10.258151
8.627360	541.776731	10.263168
8.771260	533.598709	10.268186
8.784308	551.462129	10.273203
8.442655	536.291430	10.278221
8.280914	539.804098	10.283239
8.312916	538.181483	10.288256
8.833034	540.305148	10.293274
8.499592	539.115287	10.298291
8.653324	531.957784	10.303309
8.380741	541.698743	10.308327
8.470118	536.548014	10.313344
8.764192	529.082566	10.318362
8.421713	537.762994	10.323379
8.788672	533.513681	10.328397
8.492918	539.842266	10.333415
8.582859	540.521820	10.338432
8.838258	530.851976	10.343450
8.649103	544.068123	10.348467
8.713224	539.938034	10.353485
8.689125	540.868214	10.358503
8.870220	547.961171	10.363520
9.250138	533.945822	10.368538
8.606290	540.201567	10.373555
8.591329	534.925279	10.378573
8.974716	537.300389	10.383591
8.823019	530.687898	10.388608
9.047783	529.872539	10.393626
8.683268	531.194307	10.398643
8.930928	531.658294	10.403661
8.655123	535.775102	10.408679
8.850526	540.608796	10.413696
9.300026	525.580405	10.418714
8.939276	538.387313	10.423731
8.957058	531.251225	10.428749
8.840972	534.986400	10.433767
8.690858	530.432711	10.438784
9.242099	527.742979	10.443802
8.668907	543.138905	10.448819
8.719590	530.718692	10.453837
8.962593	540.468042	10.458855
9.123948	538.953247	10.463872
8.926546	532.193051	10.468890
8.681547	537.702643	10.473907
9.104410	536.292205	10.478925
9.068087	540.462706	10.483943
9.276574	539.796101	10.488960
9.178696	528.997092	10.493978
9.302791	548.917453	10.498995
9.172465	535.073319	10.504013
9.128057	533.984421	10.509031
8.930849	536.162947	10.514048
9.148325	530.154784	10.519066
8.915559	531.453473	10.524083
9.000132	540.904579	10.529101
9.166665	536.635433	10.534119
9.086103	533.343098	10.539136
9.129575	537.260987	10.544154
9.079562	531.613002	10.549171
9.298096	533.233299	10.554189
9.056705	530.093276	10.559207
8.985749	542.806553	10.564224
9.112571	529.944985	10.569242
8.890594	535.271436	10.574259
8.979540	538.731808	10.579277
9.074384	536.122656	10.584295
8.851558	531.592468	10.589312
9.096012	527.684157	10.594330
8.795248	534.599150	10.599347
8.948532	536.079519	10.604365
9.136195	548.502988	10.609383
9.115120	563.631592	10.614400
9.344273	553.301589	10.619418
9.291958	570.241332	10.624435
9.111661	564.622075	10.629453
9.263025	560.099757	10.634471
9.325176	559.592502	10.639488
9.547243	560.317216	10.644506
8.840736	550.091750	10.649523
9.082064	554.739682	10.654541
9.220829	555.935877	10.659559
9.101827	564.088866	10.664576
9.002938	556.411972	10.669594
9.201226	561.968750	10.674611
9.085778	555.823606	10.679629
9.547054	556.698112	10.684647
9.408993	557.120313	10.689664
9.391212	564.392972	10.694682
9.419254	556.673526	10.699699
9.133886	560.634464	10.704717
9.863453	555.161004	10.709735
9.449486	561.691120	10.714752
9.870045	554.542402	10.719770
9.231464	560.137693	10.724787
9.596930	571.203597	10.729805
9.809914	550.356155	10.734823
9.320199	547.502852	10.739840
9.285721	544.421536	10.744858
9.344593	544.743295	10.749875
9.320908	544.726051	10.754893
9.316773	552.015136	10.759911
9.351963	557.022892	10.764928
9.370781	561.685763	10.769946
9.419348	563.615785	10.774963
9.469864	558.771283	10.779981
9.758181	560.031788	10.784999
9.275972	561.723089	10.790016
9.491262	554.570697	10.795034
9.314670	564.031566	10.800051
9.548845	555.642483	10.805069
9.408296	558.241872	10.810087
9.141103	560.132650	10.815104
9.569590	563.573401	10.820122
9.574640	562.675475	10.825139
9.626903	563.143399	10.830157
9.756049	557.903185	10.835175
9.388803	565.589410	10.840192
9.574765	551.302569	10.845210
9.599821	563.705443	10.850227
9.476782	565.878929	10.855245
9.615964	553.072369	10.860263
9.532088	556.393178	10.865280
9.459903	554.096208	10.870298
9.609002	562.236719	10.875315
9.473623	561.141286	10.880333
9.428804	553.035759	10.885351
9.441316	560.250434	10.890368
9.946657	577.448845	10.895386
9.850583	563.595057	10.900403
9.336265	561.729414	10.905421
9.460960	571.509864	10.910439
9.635065	584.103120	10.915456
10.108052	577.740489	10.920474
10.138601	580.547053	10.925491
9.848660	576.155948	10.930509
9.954682	555.335725	10.935527
9.651382	557.815721	10.940544
9.858072	550.323846	10.945562
9.929229	558.454477	10.950579
9.750646	564.881894	10.955597
9.830372	549.842308	10.960615
9.509348	559.120703	10.965632
9.590681	556.609257	10.970650
9.567355	565.916516	10.975667
9.810600	592.810211	10.980685
10.170639	592.999834	10.985703
9.741692	591.983506	10.990720
10.137301	586.349616	10.995738
10.184426	578.684462	11.000755
9.366685	573.365621	11.005773
9.476139	570.266480	11.010791
9.509601	584.258974	11.015808
9.898204	588.283868	11.020826
10.399259	587.782395	11.025843
10.132628	595.822352	11.030861
10.267762	587.559743	11.035879
10.114584	589.555580	11.040896
9.820848	578.498563	11.045914
10.159048	574.850816	11.050931
9.932298	571.171390	11.055949
9.959254	550.771169	11.060967
9.939235	561.754496	11.065984
9.946344	574.290665	11.071002
9.879917	572.501352	11.076019
9.773439	595.740319	11.081037
10.052244	581.171704	11.086055
10.175794	594.279626	11.091072
9.941403	590.717597	11.096090
10.069374	588.212960	11.101107
9.691609	594.964218	11.106125
10.170803	587.474272	11.111143
9.821958	593.381229	11.116160
10.217731	595.139580	11.121178
10.041056	584.350676	11.126195
9.932151	590.893086	11.131213
9.998682	583.112510	11.136231
10.078578	590.736238	11.141248
10.043561	581.148291	11.146266
10.179493	584.092051	11.151283
10.054571	590.073196	11.156301
10.211852	586.453155	11.161319
10.298995	584.371016	11.166336
9.972882	577.164321	11.171354
10.116225	586.386808	11.176371
10.033468	581.326086	11.181389
10.204960	579.096475	11.186407
10.249846	584.373667	11.191424
10.117029	590.857263	11.196442
10.222402	584.391375	11.201459
10.392832	591.092064	11.206477
10.334028	582.209977	11.211495
10.455321	587.913999	11.216512
10.266297	592.014824	11.221530
10.480474	584.641362	11.226547
10.381132	584.334948	11.231565
10.262999	578.118594	11.236583
10.512420	585.469283	11.241600
10.007901	580.850675	11.246618
9.951296	580.415318	11.251635
9.777174	590.907002	11.256653
10.340581	598.757234	11.261671
10.305413	605.951117	11.266688
10.562469	610.329742	11.271706
10.447161	606.835704	11.276723
10.099876	608.787632	11.281741
10.567474	611.548723	11.286759
10.596321	610.886188	11.291776
10.537079	609.988907	11.296794
11.022254	604.264146	11.301811
10.568279	600.736446	11.306829
10.694971	576.931324	11.311847
10.409442	575.403013	11.316864
10.220628	584.279364	11.321882
10.376587	577.252561	11.326899
10.300040	587.930960	11.331917
10.486780	600.480007	11.336935
10.362153	610.789674	11.341952
10.634551	607.202262	11.346970
10.921678	614.088076	11.351987
10.422570	603.815701	11.357005
10.397544	599.781508	11.362023
10.695117	608.030622	11.367040
10.688105	607.581903	11.372058
10.550769	597.353726	11.377075
10.349614	609.648381	11.382093
10.416390	604.044142	11.387111
10.413848	607.645906	11.392128
10.547182	612.614928	11.397146
10.759275	603.305553	11.402163
10.620387	618.030797	11.407181
11.016383	616.269926	11.412199
10.822762	613.328030	11.417216
10.814909	618.291586	11.422234
10.779626	613.563288	11.427251
10.723601	606.518363	11.432269
10.745442	606.921468	11.437287
10.918966	605.432594	11.442304
10.627675	596.398605	11.447322
10.505561	588.892666	11.452339
10.655909	601.190501	11.457357
10.806845	603.048597	11.462375
10.861213	605.738814	11.467392
10.596508	606.721586	11.472410
10.830874	607.914297	11.477427
10.641220	611.695180	11.482445
10.732800	600.661105	11.487463
10.679342	607.872595	11.492480
10.329367	613.580355	11.497498
10.708333	599.102547	11.502515
10.691760	608.364421	11.507533
10.611804	595.239162	11.512551
10.994462	607.002173	11.517568
10.687741	607.975985	11.522586
10.958728	607.801506	11.527603
10.772030	607.422413	11.532621
10.735289	600.763622	11.537639
10.862621	600.503186	11.542656
10.533446	605.255797	11.547674
11.091959	618.297350	11.552691
10.947823	635.562046	11.557709
11.176298	637.085434	11.562727
11.117996	620.438741	11.567744
11.121859	619.111911	11.572762
11.277936	611.907135	11.577779
10.903556	611.295480	11.582797
11.229733	604.220689	11.587815
11.153032	613.858277	11.592832
11.011381	621.628085	11.597850
11.298667	606.308495	11.602867
11.085376	620.435334	11.607885
10.791898	612.168169	11.612903
11.158361	605.173683	11.617920
10.813636	612.476889	11.622938
11.045762	601.784579	11.627955
10.894947	612.296811	11.632973
11.074776	610.168755	11.637991
11.250038	612.097802	11.643008
11.332576	622.086061	11.648026
11.099644	610.898649	11.653043
10.836433	620.122003	11.658061
11.184704	629.868873	11.663079
11.394022	635.588004	11.668096
11.406680	616.797220	11.673114
11.212279	619.175471	11.678131
11.132084	606.092954	11.683149
10.985813	609.401312	11.688167
11.124263	617.444418	11.693184
11.115994	636.090152	11.698202
11.521798	635.388190	11.703219
11.195250	644.116812	11.708237
11.301431	638.656195	11.713255
11.605062	643.458942	11.718272
11.178797	626.594683	11.723290
11.629592	622.985097	11.728307
11.910173	617.188833	11.733325
11.281652	610.713822	11.738343
11.471492	603.288102	11.743360
11.355492	608.164127	11.748378
11.128795	605.357444	11.753395
11.398811	610.474205	11.758413
11.441287	611.128583	11.763431
11.579399	602.492275	11.768448
11.014179	610.890501	11.773466
11.138850	602.882554	11.778483
10.820090	604.271323	11.783501
11.016244	621.977040	11.788519
11.377286	627.018250	11.793536
11.577214	630.411579	11.798554
11.483334	635.835464	11.803571
11.330423	639.017974	11.808589
11.504468	641.197796	11.813607
11.723085	638.559788	11.818624
11.402704	641.128652	11.823642
11.779473	640.487022	11.828659
11.674115	642.291469	11.833677
11.247294	642.822685	11.838695
11.830270	632.490902	11.843712
11.377122	635.666428	11.848730
11.468636	635.874505	11.853747
11.491445	646.907856	11.858765
11.635994	639.978779	11.863783
11.816500	638.737146	11.868800
11.731736	642.447064	11.873818
11.752412	632.835853	11.878835
11.394498	648.023477	11.883853
11.564515	648.984584	11.888871
11.560135	654.098940	11.893888
11.571701	646.830772	11.898906
11.734957	647.849887	11.903923
11.573229	650.701215	11.908941
11.619830	658.156509	11.913959
11.801793	646.749929	11.918976
11.584705	651.029040	11.923994
11.649710	652.883512	11.929011
11.845465	650.822679	11.934029
11.527633	646.345450	11.939047
11.829803	648.904535	11.944064
11.685189	648.429477	11.949082
11.633256	648.235644	11.954099
11.690671	638.988174	11.959117
11.663262	651.297879	11.964135
11.825345	644.543823	11.969152
11.576073	653.975689	11.974170
12.118905	656.718182	11.979187
11.693169	660.696570	11.984205
11.752702	674.980655	11.989223
12.075505	664.744059	11.994240
12.038857	668.767613	11.999258
11.870446	670.285520	12.004275
11.931035	653.363933	12.009293
11.940173	658.688624	12.014311
12.467277	669.663763	12.019328
11.752161	660.367726	12.024346
11.840497	646.608990	12.029363
11.758850	645.913642	12.034381
12.150145	663.694837	12.039399
12.148671	659.947831	12.044416
11.874156	659.237889	12.049434
11.978587	657.065670	12.054451
12.298920	660.440174	12.059469
12.090888	667.551016	12.064487
11.735466	652.221087	12.069504
11.950868	650.952001	12.074522
11.751413	663.851091	12.079539
12.230190	657.638635	12.084557
11.890490	666.556252	12.089575
12.131973	662.062820	12.094592
12.228292	667.725161	12.099610
12.185940	663.201745	12.104627
12.022493	668.021704	12.109645
12.280159	670.842696	12.114663
12.300960	665.498811	12.119680
12.430289	668.261416	12.124698
11.722093	659.304753	12.129715
12.129129	666.287186	12.134733
12.006023	664.421660	12.139751
12.297492	666.323329	12.144768
11.993650	659.748273	12.149786
12.163349	666.286335	12.154803
12.307446	664.501584	12.159821
12.158614	660.864890	12.164839
12.448326	661.291185	12.169856
12.564653	658.287530	12.174874
12.169061	664.980762	12.179891
12.479486	656.309092	12.184909
12.200757	676.942777	12.189927
12.094873	663.626509	12.194944
12.293196	667.544282	12.199962
12.217244	661.720851	12.204979
12.175346	667.013873	12.209997
12.047882	682.256724	12.215015
12.256822	659.581020	12.220032
12.445333	670.088266	12.225050
12.248004	680.082924	12.230067
12.436443	684.331648	12.235085
12.345848	699.104056	12.240103
12.754559	699.094663	12.245120
12.608383	687.932143	12.250138
12.213868	685.352927	12.255155
12.573986	682.248319	12.260173
12.577791	702.020184	12.265191
12.873223	690.279185	12.270208
12.684015	679.373016	12.275226
12.472720	674.875118	12.280243
12.774860	662.520477	12.285261
12.643389	667.916766	12.290279
12.457194	655.312024	12.295296
12.495202	667.510878	12.300314
12.394504	667.982576	12.305331
12.561791	665.124176	12.310349
12.658493	666.387013	12.315367
12.723339	678.351905	12.320384
12.751003	687.441527	12.325402
12.790962	678.856527	12.330419
12.636815	662.898694	12.335437
12.267920	669.891010	12.340455
12.365274	686.719004	12.345472
12.585897	685.499831	12.350490
12.574936	701.857104	12.355507
12.770729	696.237686	12.360525
12.464809	700.768959	12.365543
12.824882	700.915866	12.370560
12.786246	698.720966	12.375578
12.752762	701.134290	12.380595
12.760375	693.806132	12.385613
12.797062	699.412259	12.390631
12.665824	698.405491	12.395648
12.872371	698.776915	12.400666
12.837000	700.229212	12.405683
13.150839	691.797880	12.410701
13.016619	697.537719	12.415719
12.939759	699.138435	12.420736
12.667481	699.811473	12.425754
12.649848	701.766096	12.430771
13.018385	691.954523	12.435789
12.759052	700.709798	12.440807
12.955389	702.542054	12.445824
12.868672	696.794408	12.450842
12.983938	695.078614	12.455859
13.339682	696.057276	12.460877
12.562517	714.233704	12.465895
12.604847	701.420680	12.470912
12.859734	705.906181	12.475930
12.932493	702.381060	12.480947
13.238976	702.229025	12.485965
12.889589	701.946059	12.490983
12.724173	707.200968	12.496000
12.920743	706.770768	12.501018
13.197896	718.587421	12.506035
13.208668	719.844073	12.511053
13.340880	725.243796	12.516071
13.155046	724.506711	12.521088
13.652756	715.081692	12.526106
13.077244	709.139715	12.531123
13.470537	698.749068	12.536141
12.993900	696.758454	12.541159
12.970035	693.829269	12.546176
12.915746	703.889728	12.551194
13.051468	714.795118	12.556211
13.404062	714.814538	12.561229
13.185180	725.948348	12.566247
13.646268	709.616579	12.571264
13.452950	708.438647	12.576282
13.017210	703.377503	12.581299
13.399591	714.930423	12.586317
13.180004	717.581751	12.591335
13.286566	725.872715	12.596352
13.247081	716.368097	12.601370
13.213982	731.886628	12.606387
13.212964	714.397110	12.611405
13.141443	727.328332	12.616423
13.521889	723.986890	12.621440
13.636052	723.944176	12.626458
13.342858	734.340599	12.631475
13.630703	713.404714	12.636493
13.275361	732.010029	12.641511
13.100090	722.272681	12.646528
13.596163	720.740029	12.651546
13.173388	730.096062	12.656563
13.586846	723.214765	12.661581
13.494625	726.124431	12.666599
13.685282	736.246554	12.671616
13.559489	726.352369	12.676634
13.211405	727.276177	12.681651
13.584484	710.585442	12.686669
13.358700	721.670991	12.691687
13.267395	721.600620	12.696704
13.461457	724.334564	12.701722
13.263094	725.707466	12.706739
13.409346	725.433452	12.711757
13.622051	735.894599	12.716775
13.789946	739.119668	12.721792
13.740037	721.533157	12.726810
13.281951	721.357226	12.731827
13.750806	737.826113	12.736845
14.111428	742.875304	12.741863
13.830574	728.207067	12.746880
14.085295	719.576507	12.751898
13.772430	721.891595	12.756915
13.825218	716.790387	12.761933
13.738606	722.343203	12.766951
13.396438	723.535101	12.771968
13.919223	719.414551	12.776986
13.754302	722.007191	12.782003
13.670838	721.835722	12.787021
13.560034	712.152425	12.792039
13.469660	719.265583	12.797056
14.110758	729.755910	12.802074
14.030673	738.470784	12.807091
13.924871	730.440846	12.812109
13.731303	723.274645	12.817127
13.850574	721.223760	12.822144
14.286582	728.567519	12.827162
13.736758	726.359161	12.832179
14.036874	721.530993	12.837197
13.774476	712.325808	12.842215
13.789577	722.622758	12.847232
13.965456	733.170333	12.852250
13.876613	744.967135	12.857267
14.433817	744.409874	12.862285
13.982058	750.244238	12.867303
14.113666	738.414299	12.872320
14.090705	729.659034	12.877338
13.934857	717.231664	12.882355
13.660457	738.626855	12.887373
14.044349	740.252563	12.892391
14.014273	747.372246	12.897408
14.352849	747.942183	12.902426
14.257586	742.725624	12.907443
14.311437	743.334813	12.912461
14.454287	743.124155	12.917479
13.975578	743.630535	12.922496
14.234703	738.515497	12.927514
14.073771	751.301179	12.932531
14.484903	748.583914	12.937549
14.659667	742.994350	12.942567
14.140767	731.177268	12.947584
14.028958	722.060032	12.952602
13.803847	725.122483	12.957619
14.435146	743.457535	12.962637
14.273598	742.850260	12.967655
14.201049	750.653133	12.972672
14.579243	747.225060	12.977690
14.508612	745.435637	12.982707
14.179571	750.930929	12.987725
14.277520	745.848188	12.992743
14.394135	750.686383	12.997760
14.335088	741.851288	13.002778
14.367839	754.375271	13.007795
14.688381	756.165632	13.012813
14.359742	756.912404	13.017831
14.368638	754.644838	13.022848
14.587195	746.054917	13.027866
14.459568	749.443861	13.032883
14.524209	754.716647	13.037901
14.559621	747.610203	13.042919
14.155070	746.859079	13.047936
14.998680	744.673038	13.052954
14.960289	744.334247	13.057971
14.743254	726.561155	13.062989
14.349910	716.471110	13.068007
14.136908	716.147760	13.073024
14.336247	733.171830	13.078042
14.734046	748.111319	13.083059
14.540712	744.728045	13.088077
14.495415	737.342918	13.093095
14.412499	747.800062	13.098112
14.577181	753.347930	13.103130
14.774628	744.907570	13.108147
14.702214	747.092743	13.113165
14.803847	749.163169	13.118183
14.811004	753.033020	13.123200
14.845035	741.651940	13.128218
15.069183	743.690980	13.133235
14.693939	748.833348	13.138253
15.016512	753.278285	13.143271
14.788503	757.545069	13.148288
14.748722	753.901053	13.153306
14.760184	758.887230	13.158323
14.800034	754.288122	13.163341
14.786015	757.771365	13.168359
14.284197	757.318472	13.173376
14.670682	746.739963	13.178394
14.259238	745.927982	13.183411
14.451734	752.310335	13.188429
14.760705	756.353233	13.193447
14.856511	767.889263	13.198464
15.087572	776.644563	13.203482
14.965094	784.329580	13.208499
14.886784	779.212546	13.213517
15.164426	774.057609	13.218535
15.010551	772.646559	13.223552
14.887372	773.434178	13.228570
15.340010	776.279276	13.233587
15.001006	777.446638	13.238605
14.846480	762.379841	13.243623
14.767245	784.449297	13.248640
14.943461	784.938158	13.253658
14.688660	789.369234	13.258675
15.047204	788.337744	13.263693
15.257902	779.876267	13.268711
14.947170	783.096650	13.273728
14.790469	771.641746	13.278746
15.298241	786.135467	13.283763
15.163914	786.305104	13.288781
15.197077	779.422625	13.293799
15.049300	790.420656	13.298816
15.248132	773.833415	13.303834
15.564807	782.123145	13.308851
15.335480	783.928922	13.313869
15.250943	779.331782	13.318887
15.028807	777.883852	13.323904
15.210956	776.704922	13.328922
15.374239	783.418103	13.333939
15.053137	768.923236	13.338957
15.068640	765.558393	13.343975
15.018328	788.057267	13.348992
15.539368	797.092311	13.354010
15.344780	810.251718	13.359027
15.570264	808.040265	13.364045
15.720234	808.821066	13.369063
15.225532	803.311453	13.374080
15.499030	801.253229	13.379098
15.921503	795.685267	13.384115
15.530706	792.236581	13.389133
15.460675	768.526259	13.394151
15.287749	768.283642	13.399168
15.561037	770.681025	13.404186
15.832853	780.086788	13.409203
15.308476	786.111174	13.414221
15.635255	776.545053	13.419239
15.606682	788.708418	13.424256
15.606040	782.427772	13.429274
15.692939	784.539232	13.434291
15.479770	786.057896	13.439309
15.836306	779.157889	13.444327
15.558474	780.597543	13.449344
15.484834	785.913794	13.454362
15.622406	796.565015	13.459379
15.273218	803.613560	13.464397
15.661854	800.604378	13.469415
15.904115	807.991794	13.474432
16.115824	807.232328	13.479450
15.887052	798.963362	13.484467
15.835154	807.310822	13.489485
15.985849	797.761160	13.494503
15.794553	803.704211	13.499520
15.747883	799.034831	13.504538
15.686362	805.408444	13.509555
16.000992	806.292380	13.514573
15.912238	798.851458	13.519591
15.806899	800.305158	13.524608
15.723548	799.641974	13.529626
16.222492	806.821975	13.534643
15.722153	800.619454	13.539661
16.003893	794.033030	13.544679
15.812672	800.498272	13.549696
15.997879	799.144240	13.554714
16.017484	795.932437	13.559731
16.023817	797.230579	13.564749
16.222520	799.623042	13.569767
15.578049	799.780625	13.574784
15.722260	810.559680	13.579802
16.152515	801.796364	13.584819
15.691282	802.878933	13.589837
15.992124	794.090481	13.594855
15.704493	801.463807	13.599872
15.775159	802.383961	13.604890
16.045898	802.597288	13.609907
15.797894	819.967045	13.614925
15.964960	827.634665	13.619943
16.289328	832.547797	13.624960
16.145246	836.353834	13.629978
16.171110	823.339327	13.634995
16.129923	833.602993	13.640013
16.110180	820.926555	13.645031
16.194278	836.195218	13.650048
16.157069	818.466929	13.655066
16.198307	827.681927	13.660083
16.065457	838.028149	13.665101
16.427564	825.872846	13.670119
16.373760	824.691794	13.675136
16.065280	834.684161	13.680154
16.075026	826.352902	13.685171
15.771863	837.203971	13.690189
16.176034	841.537543	13.695207
16.853042	849.208404	13.700224
16.786859	848.636846	13.705242
16.722745	837.608205	13.710259
16.407367	833.855854	13.715277
16.431251	814.928918	13.720295
16.439692	816.851862	13.725312
16.660115	839.819555	13.730330
16.812406	833.265456	13.735347
16.775486	834.835534	13.740365
16.703143	825.450279	13.745383
16.442037	810.779073	13.750400
16.826843	811.666502	13.755418
16.985168	812.843524	13.760435
16.874050	817.638494	13.765453
16.924457	814.236345	13.770471
16.548627	810.074000	13.775488
16.579618	810.620854	13.780506
16.832394	812.266197	13.785523
16.689477	815.897246	13.790541
16.804625	816.912755	13.795559
16.554689	820.015963	13.800576
16.697431	822.199636	13.805594
16.982068	819.503384	13.810611
16.871700	829.530138	13.815629
16.800626	822.361837	13.820647
16.838211	815.783704	13.825664
16.633804	822.488925	13.830682
16.776553	815.110298	13.835699
16.678682	822.437923	13.840717
16.658308	822.497485	13.845735
16.885077	825.345097	13.850752
16.637126	819.072865	13.855770
16.799352	824.525898	13.860787
16.865316	838.937600	13.865805
17.080430	840.343160	13.870823
17.120074	849.111027	13.875840
17.175860	851.247153	13.880858
17.035535	838.853520	13.885875
16.853496	837.772712	13.890893
17.089752	844.391710	13.895911
17.106358	849.225693	13.900928
17.266335	847.898880	13.905946
17.094281	839.010470	13.910963
17.249009	846.591180	13.915981
17.367026	832.117357	13.920999
16.912161	822.589986	13.926016
17.094917	834.503515	13.931034
17.255122	844.291818	13.936051
17.663244	845.192301	13.941069
17.248912	831.871646	13.946087
17.044810	819.013269	13.951104
16.792883	825.769693	13.956122
17.101484	840.566629	13.961139
16.981563	844.374558	13.966157
17.139067	846.794347	13.971175
17.004834	850.957781	13.976192
16.847530	844.552568	13.981210
17.394470	853.512480	13.986227
17.244818	853.339609	13.991245
17.601112	856.999499	13.996263
17.402918	846.330909	14.001280
17.258062	843.986726	14.006298
17.512442	849.569323	14.011315
17.290408	852.736989	14.016333
17.160330	855.698440	14.021351
17.660827	851.619550	14.026368
17.202921	858.476754	14.031386
17.548932	867.530498	14.036403
17.664122	875.166807	14.041421
17.396580	871.518299	14.046439
17.755693	862.947863	14.051456
17.840306	875.210192	14.056474
17.918184	854.062575	14.061491
17.602308	854.243491	14.066509
17.379396	851.420386	14.071527
17.658992	843.310980	14.076544
17.434342	851.396252	14.081562
17.854238	863.747717	14.086579
17.745767	866.760103	14.091597
17.791274	865.689305	14.096615
18.102879	865.431110	14.101632
17.579212	854.134571	14.106650
17.653145	847.558256	14.111667
17.466259	860.824292	14.116685
17.351003	867.433224	14.121703
17.957507	872.102049	14.126720
17.619681	876.572144	14.131738
18.065619	870.794757	14.136755
17.702915	872.208174	14.141773
17.421172	866.199593	14.146791
17.651611	868.262405	14.151808
17.504502	884.931457	14.156826
18.116310	870.421980	14.161843
18.087538	873.017409	14.166861
18.178620	871.340258	14.171879
18.594369	868.646614	14.176896
18.209027	867.111242	14.181914
18.386912	873.034492	14.186931
18.133643	866.223398	14.191949
18.298354	877.144359	14.196967
18.268715	870.229367	14.201984
18.038716	877.186486	14.207002
18.244028	864.156094	14.212019
18.074143	870.126515	14.217037
18.085060	872.437216	14.222055
18.599407	866.797663	14.227072
17.924535	873.208882	14.232090
18.004456	869.658913	14.237107
18.003339	877.150588	14.242125
18.133786	869.312004	14.247143
18.306246	868.492724	14.252160
18.016747	873.914365	14.257178
18.258013	867.534624	14.262195
18.114930	869.824861	14.267213
17.972465	874.043012	14.272231
18.302533	867.460336	14.277248
18.317257	880.876135	14.282266
18.155737	871.624169	14.287283
18.380556	878.702729	14.292301
17.824390	877.168978	14.297319
18.311701	890.842830	14.302336
18.230453	905.773516	14.307354
18.478326	900.525265	14.312371
18.587293	911.226003	14.317389
18.508292	906.197224	14.322407
18.694631	901.859139	14.327424
18.980970	906.777434	14.332442
19.119210	895.409826	14.337459
18.776384	885.166598	14.342477
18.364766	880.781850	14.347495
18.533557	883.294644	14.352512
18.276247	897.249338	14.357530
18.223237	899.320489	14.362547
18.436816	899.552373	14.367565
18.585608	903.394783	14.372583
18.620847	891.777189	14.377600
18.568158	906.414959	14.382618
18.690182	899.560175	14.387635
18.556043	899.758519	14.392653
18.682727	893.482845	14.397671
18.825764	898.723754	14.402688
18.680481	902.118224	14.407706
18.701176	905.850438	14.412723
18.762149	898.855811	14.417741
18.597225	909.723518	14.422759
19.035529	916.791612	14.427776
18.663344	924.608745	14.432794
18.978415	919.420180	14.437811
19.241901	922.353237	14.442829
19.185940	931.123262	14.447847
19.257269	906.846354	14.452864
19.300913	913.373782	14.457882
18.985051	899.841833	14.462899
18.763189	897.014214	14.467917
18.697199	904.745016	14.472935
19.404254	909.246953	14.477952
19.222055	912.225148	14.482970
19.009463	892.168404	14.487987
18.787233	892.765813	14.493005
18.833902	914.765123	14.498023
19.478469	914.619883	14.503040
19.640510	923.540075	14.508058
19.505583	916.016423	14.513075
19.160125	893.524640	14.518093
18.809930	900.176572	14.523111
19.189144	907.316288	14.528128
18.842014	921.422735	14.533146
19.467093	924.698029	14.538163
19.654811	924.320472	14.543181
19.428914	928.880240	14.548199
19.569493	916.835499	14.553216
19.125677	902.974049	14.558234
19.052543	917.708136	14.563251
19.365101	923.014179	14.568269
19.213802	926.288993	14.573287
19.560840	919.465891	14.578304
19.475526	924.321364	14.583322
19.391829	924.496759	14.588339
19.415680	924.720810	14.593357
19.528786	921.511157	14.598375
19.757004	919.939153	14.603392
19.593955	922.234684	14.608410
19.475601	921.120255	14.613427
19.524174	912.218951	14.618445
19.701168	921.086856	14.623463
19.439913	923.189276	14.628480
19.402243	926.531418	14.633498
19.839399	920.059456	14.638515
19.630193	916.203223	14.643533
19.764646	929.993628	14.648551
19.993916	924.918527	14.653568
19.695364	923.361048	14.658586
19.623153	928.418269	14.663603
19.700850	923.145738	14.668621
19.640535	931.827123	14.673639
19.786368	913.731710	14.678656
19.798725	915.771528	14.683674
19.529451	921.108136	14.688691
19.740909	923.601248	14.693709
19.579528	934.193402	14.698727
19.921351	942.913657	14.703744
19.850673	958.065457	14.708762
20.069022	959.350813	14.713779
20.308932	952.162652	14.718797
19.924481	951.500296	14.723815
20.266840	946.993363	14.728832
19.939024	935.014845	14.733850
20.009421	938.892733	14.738867
20.143932	952.914826	14.743885
19.782365	949.097294	14.748903
20.216480	952.010461	14.753920
20.279991	944.672893	14.758938
20.194565	950.651353	14.763955
20.207984	951.401121	14.768973
20.115428	949.717084	14.773991
20.305792	942.786359	14.779008
20.363775	946.688752	14.784026
20.184080	949.373250	14.789043
20.371774	947.759949	14.794061
19.959636	944.476380	14.799079
20.073780	941.285249	14.804096
20.510224	953.723795	14.809114
20.179402	956.487740	14.814131
20.482334	947.729757	14.819149
20.265970	955.353105	14.824167
20.371448	940.777924	14.829184
20.086504	941.521773	14.834202
20.105256	954.884018	14.839219
20.495020	949.228333	14.844237
20.305781	947.907194	14.849255
20.476115	951.585416	14.854272
20.377596	950.659802	14.859290
20.067429	949.825661	14.864307
20.691740	955.227135	14.869325
20.423487	951.374802	14.874343
20.886091	962.699235	14.879360
20.574251	950.392086	14.884378
20.554424	947.073231	14.889395
20.966106	955.008310	14.894413
20.641539	961.664275	14.899431
20.435556	955.787546	14.904448
20.383369	956.611599	14.909466
20.496374	965.014802	14.914483
20.492760	974.698731	14.919501
20.693619	971.604198	14.924519
20.793030	978.638494	14.929536
20.896168	972.386779	14.934554
20.858193	976.190175	14.939571
20.792191	967.383665	14.944589
20.698510	977.910859	14.949607
20.733525	973.635698	14.954624
20.859036	969.140786	14.959642
20.722810	978.865654	14.964659
20.945067	968.501091	14.969677
20.734696	979.141375	14.974695
20.991728	967.979349	14.979712
21.289044	965.503786	14.984730
20.961667	968.458093	14.989747
21.152113	968.406046	14.994765
21.043329	978.576718	14.999783
21.215266	975.370464	15.004800
21.422558	966.668915	15.009818
20.965639	979.657120	15.014835
21.232697	969.860270	15.019853
20.997626	977.174553	15.024871
21.446345	988.209599	15.029888
21.446468	974.083761	15.034906
20.841619	974.984317	15.039923
21.106489	978.053564	15.044941
21.472640	995.444071	15.049959
21.633441	991.283030	15.054976
21.780217	973.989310	15.059994
21.602258	963.533797	15.065011
21.445648	962.438321	15.070029
21.495194	957.158450	15.075047
21.618839	956.447470	15.080064
21.733121	958.141830	15.085082
21.791844	965.382476	15.090099
21.845020	951.101394	15.095117
21.577620	960.915765	15.100135
21.791968	963.491075	15.105152
21.630074	960.849725	15.110170
21.544558	966.964811	15.115187
21.347531	956.430194	15.120205
21.173691	958.519270	15.125223
21.575846	963.062451	15.130240
21.948377	955.187722	15.135258
21.358151	961.308744	15.140275
21.709212	953.489549	15.145293
21.487528	964.077770	15.150311
21.444258	963.488227	15.155328
21.822592	962.739640	15.160346
21.613819	961.087121	15.165363
21.604679	957.495245	15.170381
21.317450	963.608425	15.175399
21.634737	977.036418	15.180416
21.961187	979.765923	15.185434
22.091643	993.248997	15.190451
22.134870	990.857390	15.195469
22.047511	991.168426	15.200487
21.822500	979.099169	15.205504
22.092628	973.567290	15.210522
21.943090	986.268993	15.215539
22.237548	986.216194	15.220557
22.128868	969.803073	15.225575
21.944067	962.391421	15.230592
22.159600	969.857959	15.235610
21.936409	983.683249	15.240627
21.713950	984.621819	15.245645
22.102262	992.632057	15.250663
22.200575	985.093816	15.255680
22.258975	993.142353	15.260698
22.045543	991.545327	15.265715
22.271615	992.913256	15.270733
22.455223	992.400956	15.275751
22.032712	987.316062	15.280768
22.145484	989.706697	15.285786
21.982335	995.016244	15.290803
22.349329	987.891585	15.295821
22.376136	992.550700	15.300839
22.041360	988.883419	15.305856
22.595109	987.553348	15.310874
22.105991	986.605649	15.315891
21.978684	987.590999	15.320909
22.633814	980.372394	15.325927
22.470139	987.750402	15.330944
22.551795	982.847839	15.335962
22.437377	994.548892	15.340979
22.582614	991.686028	15.345997
22.307579	1002.243775	15.351015
22.377407	1012.078502	15.356032
22.971448	1007.005344	15.361050
22.905893	1008.344189	15.366067
22.735834	1007.566674	15.371085
22.965374	993.175537	15.376103
22.917942	992.523695	15.381120
23.159774	975.107882	15.386138
23.182173	974.986134	15.391155
22.682893	969.056578	15.396173
22.865778	970.913936	15.401191
22.541765	973.542508	15.406208
22.786822	964.609894	15.411226
22.768560	978.977462	15.416243
22.676046	975.636825	15.421261
23.214445	971.461453	15.426279
23.052874	978.515505	15.431296
23.154824	977.884896	15.436314
23.019291	981.145488	15.441331
23.078049	966.366250	15.446349
23.220040	978.927767	15.451367
23.116801	978.148203	15.456384
22.975883	969.510825	15.461402
22.910068	976.654860	15.466419
23.053843	977.281788	15.471437
23.214295	979.063353	15.476455
23.199483	982.473555	15.481472
23.307233	979.421660	15.486490
23.244449	975.287942	15.491507
22.851209	976.153328	15.496525
23.173066	968.653527	15.501543
22.831948	979.049811	15.506560
23.390744	992.042033	15.511578
23.205126	994.144488	15.516595
23.369252	1005.960661	15.521613
23.232093	1002.452252	15.526631
23.234437	1007.564623	15.531648
23.635623	1003.078210	15.536666
23.396103	1003.438550	15.541683
23.268375	1004.105880	15.546701
23.518207	999.720603	15.551719
23.070157	1005.629834	15.556736
23.357609	1004.414096	15.561754
23.577062	999.895294	15.566771
23.762657	1008.153787	15.571789
23.772876	1009.613102	15.576807
23.515676	1010.654292	15.581824
23.916734	1002.861013	15.586842
23.529266	1002.618421	15.591859
23.961565	1000.338909	15.596877
23.636639	1002.117295	15.601895
23.341567	1001.326308	15.606912
23.711748	992.878363	15.611930
23.511808	1002.035131	15.616947
23.655786	1008.085715	15.621965
23.740119	999.763224	15.626983
23.371460	1007.635518	15.632000
23.787568	1006.326747	15.637018
23.506592	1017.287042	15.642035
23.633588	1022.643252	15.647053
24.054144	1033.061788	15.652071
24.134309	1041.244126	15.657088
24.324562	1034.487778	15.662106
23.771846	1032.154665	15.667123
23.957067	1028.564325	15.672141
24.417147	1027.810022	15.677159
23.931637	1026.162549	15.682176
24.558791	1029.825098	15.687194
24.032377	1010.561850	15.692211
24.080203	1004.705906	15.697229
24.189513	1000.566018	15.702247
24.073402	1019.924388	15.707264
24.171767	1019.313271	15.712282
24.088639	1026.902306	15.717299
24.025024	1022.116783	15.722317
24.277253	1028.427713	15.727335
24.080314	1032.081963	15.732352
24.165858	1024.472995	15.737370
24.453517	1029.632829	15.742387
24.184591	1028.700889	15.747405
24.543930	1022.038877	15.752423
24.491666	1034.120551	15.757440
24.598135	1027.599772	15.762458
24.302892	1033.749742	15.767475
24.474579	1029.653413	15.772493
24.852789	1025.281042	15.777511
24.714326	1028.204355	15.782528
24.495728	1029.016703	15.787546
24.620218	1026.073034	15.792563
24.332343	1037.613983	15.797581
24.394195	1023.241633	15.802599
24.240104	1023.736978	15.807616
24.681112	1020.361986	15.812634
24.437193	1021.973377	15.817651
24.644736	1027.859869	15.822669
25.031137	1027.315438	15.827687
24.513829	1034.684531	15.832704
25.061849	1034.724226	15.837722
24.663230	1033.861476	15.842739
24.849490	1041.432908	15.847757
25.074857	1047.058587	15.852775
24.644948	1038.846345	15.857792
24.962844	1040.218307	15.862810
25.084742	1049.480658	15.867827
24.994720	1046.182503	15.872845
24.941975	1043.710782	15.877863
24.800444	1051.599676	15.882880
25.173075	1043.901647	15.887898
25.398043	1038.034752	15.892915
25.549233	1022.971215	15.897933
25.520415	1013.855366	15.902951
25.098333	1011.611561	15.907968
25.143853	1009.567975	15.912986
25.187402	1005.416182	15.918003
25.211492	1011.010344	15.923021
25.229055	1006.753821	15.928039
25.182726	1019.076608	15.933056
25.317374	1015.068718	15.938074
25.544320	1009.386926	15.943091
25.241072	1009.835412	15.948109
25.469002	1015.079180	15.953127
25.434910	1010.770221	15.958144
25.549427	1011.158328	15.963162
25.583869	1017.621979	15.968179
25.418115	1018.914097	15.973197
25.517775	1012.841279	15.978215
25.403989	1021.671554	15.983232
25.458482	1006.669377	15.988250
25.264816	1006.317414	15.993267
25.272714	1024.027718	15.998285
25.578822	1017.793034	16.003303
25.425270	1029.887209	16.008320
25.595708	1020.999247	16.013338
25.812913	1027.850218	16.018355
25.686249	1018.942742	16.023373
25.827172	1015.615264	16.028391
25.721070	1028.084599	16.033408
25.939453	1023.917916	16.038426
25.726785	1027.523601	16.043443
25.587194	1030.880147	16.048461
25.765875	1024.467046	16.053479
25.783662	1026.239259	16.058496
25.498915	1028.899894	16.063514
25.888058	1028.978199	16.068531
25.579024	1031.505084	16.073549
25.984349	1036.675283	16.078567
26.055673	1052.842097	16.083584
26.147521	1058.604925	16.088602
26.152181	1048.748494	16.093619
25.970998	1066.093838	16.098637
26.274168	1055.716555	16.103655
26.133371	1052.941375	16.108672
26.332966	1056.865139	16.113690
26.396871	1064.215200	16.118707
26.131435	1057.354669	16.123725
26.203543	1049.729419	16.128743
26.189170	1057.247989	16.133760
26.204508	1064.323068	16.138778
26.328183	1054.338984	16.143795
26.246243	1059.489001	16.148813
26.248703	1051.691084	16.153831
26.035877	1056.809314	16.158848
26.308119	1061.454821	16.163866
26.483364	1053.881321	16.168883
26.432133	1060.258053	16.173901
26.768312	1053.991194	16.178919
26.677087	1057.926682	16.183936
26.498076	1048.421231	16.188954
26.522192	1048.564143	16.193971
26.225138	1051.721680	16.198989
26.481365	1050.707180	16.204007
26.288323	1059.914014	16.209024
26.336514	1060.828864	16.214042
26.734530	1057.335820	16.219059
26.856950	1075.995992	16.224077
27.036615	1078.281433	16.229095
26.547431	1074.867734	16.234112
26.434686	1082.755797	16.239130
26.750574	1076.670244	16.244147
26.666981	1084.642828	16.249165
27.026464	1078.724821	16.254183
27.126229	1077.907181	16.259200
27.132333	1079.551822	16.264218
27.306706	1084.762391	16.269235
27.132423	1084.647742	16.274253
27.121680	1082.846555	16.279271
27.233133	1077.053626	16.284288
26.914190	1078.991254	16.289306
27.261456	1070.573059	16.294323
27.004170	1079.696099	16.299341
27.197110	1078.104747	16.304359
27.374516	1080.311435	16.309376
27.427503	1076.506854	16.314394
27.026339	1070.259393	16.319411
27.130028	1082.598240	16.324429
27.194044	1078.002106	16.329447
27.248567	1073.779184	16.334464
26.997294	1079.522280	16.339482
27.080404	1071.146020	16.344499
27.082699	1080.154661	16.349517
27.036892	1074.173709	16.354535
26.879194	1085.862734	16.359552
27.143248	1098.459570	16.364570
27.302422	1105.685161	16.369587
27.425201	1111.704665	16.374605
27.348240	1114.085124	16.379623
27.137109	1118.224798	16.384640
27.343717	1106.750204	16.389658
27.737355	1112.440453	16.394675
27.227391	1114.082685	16.399693
27.772012	1117.693229	16.404711
28.023297	1122.896146	16.409728
28.230159	1119.316360	16.414746
28.251249	1102.394155	16.419763
27.793511	1099.403941	16.424781
28.153232	1100.133165	16.429799
28.127079	1098.758136	16.434816
28.087152	1095.010724	16.439834
27.791224	1088.181229	16.444851
28.051376	1093.321642	16.449869
28.126247	1094.882024	16.454887
27.915412	1094.114037	16.459904
27.798250	1095.003619	16.464922
28.120393	1084.856615	16.469939
28.159855	1099.315089	16.474957
28.200918	1091.928823	16.479975
27.890319	1093.318245	16.484992
27.929799	1095.652578	16.490010
28.083301	1086.640234	16.495027
28.028116	1099.962928	16.500045
28.180175	1092.819223	16.505063
28.395290	1093.608306	16.510080
28.034745	1094.265518	16.515098
28.472528	1093.244462	16.520115
28.259800	1100.755865	16.525133
28.233111	1098.601835	16.530151
28.563682	1111.342736	16.535168
28.338717	1119.884868	16.540186
28.921943	1114.993778	16.545203
28.399968	1111.906763	16.550221
28.417895	1097.229063	16.555239
28.792214	1110.227639	16.560256
28.771395	1105.545208	16.565274
28.266414	1091.673675	16.570291
28.510322	1099.777258	16.575309
28.876581	1112.253975	16.580327
28.388233	1119.981660	16.585344
28.308158	1122.303979	16.590362
28.717978	1123.219749	16.595379
28.586344	1129.161472	16.600397
28.364649	1124.471479	16.605415
28.734193	1115.732644	16.610432
28.726602	1119.661334	16.615450
28.687689	1121.063080	16.620467
28.521127	1130.897805	16.625485
29.019687	1136.489133	16.630503
29.284559	1141.803572	16.635520
28.980683	1124.726308	16.640538
29.250754	1125.346818	16.645555
29.168963	1121.990982	16.650573
28.942701	1117.533234	16.655591
28.580104	1124.798313	16.660608
28.940196	1138.659074	16.665626
29.141997	1152.936294	16.670643
28.892622	1148.159560	16.675661
29.098293	1151.160339	16.680679
29.491712	1138.405918	16.685696
29.382586	1148.449600	16.690714
29.355213	1135.231681	16.695731
29.087626	1139.900008	16.700749
29.213461	1147.339417	16.705767
29.130841	1143.010930	16.710784
29.235773	1147.738205	16.715802
29.627909	1138.518462	16.720819
29.484607	1152.905792	16.725837
29.137746	1149.062537	16.730855
29.439097	1151.954898	16.735872
29.464842	1160.773084	16.740890
29.687894	1171.506810	16.745907
29.934114	1175.792916	16.750925
30.123907	1156.689176	16.755943
30.220677	1146.721315	16.760960
29.758797	1136.308148	16.765978
30.040354	1128.441760	16.770995
29.772319	1135.378151	16.776013
29.700634	1134.857493	16.781031
30.083435	1126.412497	16.786048
29.893914	1134.736553	16.791066
29.944798	1135.074218	16.796083
29.930546	1125.535431	16.801101
30.005109	1131.066526	16.806119
30.291689	1128.008107	16.811136
30.139524	1135.127592	16.816154
30.177795	1138.975833	16.821171
30.040870	1133.513126	16.826189
29.857007	1133.899649	16.831207
30.195823	1129.378687	16.836224
29.782563	1137.627732	16.841242
30.060347	1132.612608	16.846259
30.047787	1133.565511	16.851277
30.287950	1131.110051	16.856295
29.931223	1124.701646	16.861312
29.974801	1142.794325	16.866330
30.326717	1145.805046	16.871347
30.524061	1154.104182	16.876365
30.273597	1157.659095	16.881383
30.886392	1154.777938	16.886400
30.658326	1152.412106	16.891418
30.483531	1151.795204	16.896435
30.542634	1156.552933	16.901453
30.305803	1154.735380	16.906471
30.393494	1163.298009	16.911488
30.185319	1166.137269	16.916506
30.500150	1159.115686	16.921523
30.493391	1161.147887	16.926541
30.406909	1151.845093	16.931559
30.496094	1166.741012	16.936576
30.368286	1163.064486	16.941594
30.572820	1160.149218	16.946611
30.736777	1163.636829	16.951629
30.631034	1180.333574	16.956647
31.122743	1174.029007	16.961664
30.717401	1194.156102	16.966682
30.946050	1183.677740	16.971699
30.978681	1183.654679	16.976717
30.958290	1180.233903	16.981735
31.089917	1176.989428	16.986752
30.992646	1179.895294	16.991770
31.075740	1181.096462	16.996787
31.034279	1186.358685	17.001805
30.854879	1183.165902	17.006823
31.134059	1178.586337	17.011840
30.600160	1189.098262	17.016858
31.011242	1186.199445	17.021875
31.481252	1171.383549	17.026893
31.229788	1178.043596	17.031911
31.370920	1184.595879	17.036928
31.155878	1187.966180	17.041946
31.465935	1199.007103	17.046963
31.431116	1201.209319	17.051981
31.437816	1204.497890	17.056999
31.666685	1202.921420	17.062016
31.803462	1199.833950	17.067034
31.374434	1200.129731	17.072051
31.774567	1194.084459	17.077069
31.822877	1207.555784	17.082087
31.862354	1188.882086	17.087104
31.654619	1181.500122	17.092122
31.487635	1183.691233	17.097139
31.276937	1183.346426	17.102157
31.402236	1197.968276	17.107175
31.815250	1198.830767	17.112192
31.310167	1204.522003	17.117210
31.639457	1208.071118	17.122227
31.752912	1205.297745	17.127245
31.566008	1208.380316	17.132263
31.726852	1207.988324	17.137280
31.811844	1226.374203	17.142298
32.361738	1231.569258	17.147315
32.356685	1236.428221	17.152333
32.169802	1225.787801	17.157351
32.208497	1209.253479	17.162368
32.196855	1210.087342	17.167386
32.466558	1195.672413	17.172403
32.342071	1195.557360	17.177421
31.894222	1195.714938	17.182439
31.863087	1208.253843	17.187456
32.377162	1212.958806	17.192474
32.274020	1228.578843	17.197491
32.308647	1222.347469	17.202509
32.292812	1238.131343	17.207527
32.794761	1222.049124	17.212544
32.689363	1228.670744	17.217562
32.455309	1228.370761	17.222579
33.065356	1218.521080	17.227597
32.866767	1209.059334	17.232615
32.661833	1192.017517	17.237632
32.951265	1199.608492	17.242650
32.613012	1195.127211	17.247667
32.625062	1176.621463	17.252685
32.621138	1183.271472	17.257703
32.615425	1184.355911	17.262720
32.497669	1183.594102	17.267738
32.474793	1186.803730	17.272755
32.861421	1200.268818	17.277773
32.572098	1215.256431	17.282791
32.866817	1222.795361	17.287808
32.464605	1224.802354	17.292826
32.653304	1226.781607	17.297843
32.922122	1213.072288	17.302861
32.668834	1225.676082	17.307879
32.672035	1214.527721	17.312896
32.868215	1228.095742	17.317914
33.312613	1247.318327	17.322931
33.914157	1241.123819	17.327949
33.584674	1233.223113	17.332967
33.893552	1215.172688	17.337984
33.682824	1227.602488	17.343002
33.447143	1218.940171	17.348019
33.446773	1216.704981	17.353037
33.349073	1217.073248	17.358055
33.865375	1222.232547	17.363072
33.733278	1219.637378	17.368090
33.465213	1218.651348	17.373107
33.618208	1215.828096	17.378125
33.280415	1218.926299	17.383143
33.424425	1214.114871	17.388160
33.284952	1217.602927	17.393178
33.318987	1220.547210	17.398195
33.152117	1212.374224	17.403213
33.462532	1213.008111	17.408231
33.656222	1212.202018	17.413248
33.433122	1213.451322	17.418266
33.872281	1230.106768	17.423283
34.091604	1227.715384	17.428301
33.672438	1247.445258	17.433319
34.034877	1234.206953	17.438336
34.183246	1240.304140	17.443354
34.149923	1237.373275	17.448371
34.159852	1236.088689	17.453389
33.768360	1216.436239	17.458407
34.049772	1231.723482	17.463424
34.022642	1229.278968	17.468442
34.150373	1237.672786	17.473459
34.109991	1240.025532	17.478477
33.905297	1237.582183	17.483495
34.015321	1230.141085	17.488512
34.013006	1224.803210	17.493530
33.833529	1227.134585	17.498547
34.256283	1228.531656	17.503565
34.320682	1238.004455	17.508583
34.376827	1242.471376	17.513600
34.297459	1237.668327	17.518618
33.759950	1242.810267	17.523635
34.175071	1258.637886	17.528653
34.360782	1272.151389	17.533671
34.463069	1271.976205	17.538688
34.794406	1270.840946	17.543706
34.377200	1271.043822	17.548723
34.887399	1266.986835	17.553741
34.663865	1274.303277	17.558759
34.832834	1265.745326	17.563776
34.885906	1272.639433	17.568794
34.984360	1267.765484	17.573811
35.016710	1253.523014	17.578829
35.002335	1265.502119	17.583847
35.161436	1272.851025	17.588864
35.170411	1254.227196	17.593882
34.976511	1265.674746	17.598899
35.472116	1251.575748	17.603917
34.780384	1261.463195	17.608935
34.898719	1263.080148	17.613952
35.036017	1249.337540	17.618970
34.939818	1259.529533	17.623987
35.301390	1257.478659	17.629005
35.058415	1267.505690	17.634023
34.835640	1262.527264	17.639040
34.848295	1260.297383	17.644058
35.057807	1258.763493	17.649075
34.970347	1249.983220	17.654093
35.601148	1277.156399	17.659111
35.318794	1281.258742	17.664128
35.434439	1281.222671	17.669146
35.371650	1286.004241	17.674163
35.708293	1280.971020	17.679181
35.642932	1288.375742	17.684199
35.674503	1282.637350	17.689216
35.649581	1285.443419	17.694234
35.486809	1293.345809	17.699251
35.460580	1290.809801	17.704269
35.549876	1288.349471	17.709287
35.722493	1291.140032	17.714304
35.870554	1293.885464	17.719322
35.416951	1287.781663	17.724339
35.291787	1287.097848	17.729357
35.459715	1295.081884	17.734375
35.833561	1319.645592	17.739392
35.795128	1312.996420	17.744410
35.570161	1327.893921	17.749427
36.070555	1319.596200	17.754445
36.044207	1325.517349	17.759463
36.086715	1316.899682	17.764480
36.249914	1315.174279	17.769498
36.113820	1322.135279	17.774515
36.246535	1321.068853	17.779533
36.236127	1311.118700	17.784551
36.058899	1319.271920	17.789568
36.147698	1313.745257	17.794586
36.234754	1325.504802	17.799603
36.555071	1328.335386	17.804621
36.539971	1338.547809	17.809639
36.874663	1336.475410	17.814656
36.766462	1312.953069	17.819674
36.717146	1309.418573	17.824691
36.883626	1298.267029	17.829709
37.057255	1302.710112	17.834727
36.810089	1308.894717	17.839744
36.827544	1304.167678	17.844762
36.756074	1310.639999	17.849779
36.954367	1312.099186	17.854797
36.820966	1311.475004	17.859815
36.585888	1313.354628	17.864832
36.876240	1296.955151	17.869850
36.751313	1306.417728	17.874867
36.773847	1301.954007	17.879885
36.884174	1302.333763	17.884903
36.683714	1299.839703	17.889920
37.268004	1315.028660	17.894938
37.066297	1329.704983	17.899955
37.244953	1320.483214	17.904973
37.298720	1320.594429	17.909991
37.127550	1323.388199	17.915008
37.459117	1318.729023	17.920026
37.428446	1334.067054	17.925043
37.192771	1309.149819	17.930061
37.409060	1310.087137	17.935079
37.147213	1328.964230	17.940096
37.396782	1329.146836	17.945114
36.777437	1330.911201	17.950131
37.408266	1332.261495	17.955149
37.732218	1327.998055	17.960167
37.256295	1323.228211	17.965184
37.617009	1321.210148	17.970202
37.380466	1322.124701	17.975219
37.722462	1327.772436	17.980237
37.564983	1319.691529	17.985255
37.579454	1333.813444	17.990272
37.648513	1320.306910	17.995290
37.799488	1339.653966	18.000307
38.163404	1341.065156	18.005325
37.932143	1339.069103	18.010343
38.310183	1334.680534	18.015360
38.096470	1318.514017	18.020378
38.143805	1318.501504	18.025395
37.814194	1307.916242	18.030413
38.162316	1322.113791	18.035431
38.473849	1332.209721	18.040448
38.332836	1319.556573	18.045466
37.874726	1316.769518	18.050483
38.338250	1326.138636	18.055501
38.700313	1324.626628	18.060519
38.191065	1326.727010	18.065536
38.337440	1311.015989	18.070554
38.485794	1324.145998	18.075571
38.398113	1331.298948	18.080589
38.748478	1338.598381	18.085607
38.715495	1333.558074	18.090624
38.646199	1325.591244	18.095642
38.504321	1322.208738	18.100659
38.573922	1312.022066	18.105677
38.710516	1330.871522	18.110695
38.934048	1336.758232	18.115712
39.087106	1330.981128	18.120730
38.873542	1320.317518	18.125747
38.520478	1316.927595	18.130765
38.627709	1317.862174	18.135783
38.661241	1337.488972	18.140800
39.064144	1332.686052	18.145818
38.902931	1339.813040	18.150835
38.716182	1341.692902	18.155853
38.749128	1341.193822	18.160871
38.605448	1344.680244	18.165888
38.913388	1332.840230	18.170906
38.903164	1338.211481	18.175923
39.085913	1344.760065	18.180941
39.281269	1344.942627	18.185959
38.947587	1362.809298	18.190976
39.161396	1359.229485	18.195994
39.045161	1370.802782	18.201011
39.442321	1362.283622	18.206029
39.183231	1361.696075	18.211047
39.259082	1359.549767	18.216064
39.530345	1353.931742	18.221082
39.417836	1359.221974	18.226099
39.291723	1361.563397	18.231117
39.438906	1353.862923	18.236135
39.523041	1378.328424	18.241152
39.724041	1374.099185	18.246170
39.662221	1379.002666	18.251187
39.730656	1392.870006	18.256205
39.942430	1388.873610	18.261223
39.374289	1391.047960	18.266240
40.178256	1391.487232	18.271258
39.843706	1388.061146	18.276275
39.905283	1387.803754	18.281293
40.126470	1383.554623	18.286311
39.913880	1379.373256	18.291328
39.987118	1382.460655	18.296346
39.792026	1386.154836	18.301363
40.033495	1391.292550	18.306381
40.167998	1381.791084	18.311399
40.104389	1396.727580	18.316416
40.259446	1379.964295	18.321434
40.298509	1386.117894	18.326451
40.210581	1385.047979	18.331469
40.390207	1396.966597	18.336487
40.664878	1405.290811	18.341504
40.714100	1400.191546	18.346522
40.910525	1404.489142	18.351539
40.575032	1390.708456	18.356557
41.006798	1374.336968	18.361575
40.624472	1378.979948	18.366592
40.542362	1373.232859	18.371610
40.646326	1376.889145	18.376627
40.860292	1392.498376	18.381645
40.988223	1383.403499	18.386663
40.654628	1381.073673	18.391680
40.818578	1392.228779	18.396698
41.105134	1398.466836	18.401715
40.752433	1406.618165	18.406733
41.166694	1397.985910	18.411751
41.028199	1399.662885	18.416768
41.043881	1394.756591	18.421786
41.453899	1400.513910	18.426803
41.106424	1398.198985	18.431821
41.370455	1397.812280	18.436839
41.108669	1394.298511	18.441856
41.325336	1395.309392	18.446874
41.344864	1393.490933	18.451891
41.168651	1399.780707	18.456909
41.449757	1397.083764	18.461927
41.291838	1407.813259	18.466944
41.327415	1395.050781	18.471962
41.288670	1393.645930	18.476979
41.179753	1400.496940	18.481997
41.735132	1406.024598	18.487015
41.757443	1426.736014	18.492032
41.689999	1424.239510	18.497050
41.883512	1432.949262	18.502067
41.722712	1432.123730	18.507085
41.558445	1425.406844	18.512103
41.845518	1427.042225	18.517120
41.730526	1424.311899	18.522138
41.741233	1420.575676	18.527155
41.788853	1425.864513	18.532173
42.091870	1417.034208	18.537191
41.823658	1420.390562	18.542208
41.759175	1421.048578	18.547226
42.066185	1420.497648	18.552243
41.871260	1437.307126	18.557261
42.752036	1441.423673	18.562279
43.088941	1431.240134	18.567296
43.119280	1413.997951	18.572314
43.026321	1411.632456	18.577331
42.586551	1402.689398	18.582349
42.861836	1406.267614	18.587367
42.450704	1416.659290	18.592384
42.841055	1400.002149	18.597402
42.763166	1384.674769	18.602419
42.793140	1368.303531	18.607437
42.667531	1364.145112	18.612455
42.967916	1365.355455	18.617472
42.650088	1368.741697	18.622490
43.085186	1366.754178	18.627507
42.641260	1370.474751	18.632525
42.743374	1367.384348	18.637543
42.747089	1380.928983	18.642560
43.004283	1384.536971	18.647578
42.859092	1400.496048	18.652595
43.036582	1408.332103	18.657613
43.520202	1404.467288	18.662631
43.414236	1405.889259	18.667648
43.114139	1405.334508	18.672666
43.114742	1392.708943	18.677683
42.964920	1401.675733	18.682701
42.706686	1395.643350	18.687719
42.867374	1405.375043	18.692736
43.167536	1404.057955	18.697754
43.134169	1400.553857	18.702771
43.211928	1404.753463	18.707789
43.372956	1414.289836	18.712807
43.284516	1431.823318	18.717824
43.335646	1434.023880	18.722842
43.527394	1429.809943	18.727859
43.266681	1437.720023	18.732877
43.641020	1430.679373	18.737895
43.788150	1436.120173	18.742912
43.620836	1436.245299	18.747930
43.821306	1433.463329	18.752947
43.931981	1460.069361	18.757965
44.299062	1454.475925	18.762983
44.025731	1456.030044	18.768000
44.026660	1439.089955	18.773018
43.881166	1446.910420	18.778035
43.771029	1461.019304	18.783053
44.424710	1460.900898	18.788071
44.407509	1464.107279	18.793088
44.100943	1466.027541	18.798106
44.333128	1459.769930	18.803123
44.145496	1455.974146	18.808141
44.165051	1461.120025	18.813159
44.346506	1454.034653	18.818176
44.228378	1456.370826	18.823194
44.403758	1449.575433	18.828211
44.510988	1452.108396	18.833229
44.422661	1451.003504	18.838247
44.595175	1459.057727	18.843264
44.496603	1478.249980	18.848282
45.411055	1474.667471	18.853299
45.438835	1460.029127	18.858317
45.405631	1447.999667	18.863335
45.481261	1445.238050	18.868352
45.382161	1447.718299	18.873370
45.518749	1440.794715	18.878387
45.251225	1449.467719	18.883405
45.334717	1419.193492	18.888423
44.979449	1407.340027	18.893440
45.131113	1407.505049	18.898458
45.079935	1399.465092	18.903475
44.866934	1423.916272	18.908493
45.009710	1435.317834	18.913511
45.154070	1428.081558	18.918528
44.733806	1441.475457	18.923546
45.223340	1438.208844	18.928563
45.278914	1439.726408	18.933581
45.428110	1432.486570	18.938599
45.026500	1441.814117	18.943616
45.010220	1451.584699	18.948634
45.472713	1456.494762	18.953651
45.572255	1478.319361	18.958669
45.647726	1471.660638	18.963687
45.440075	1468.582329	18.968704
45.267186	1473.649571	18.973722
45.411926	1479.528565	18.978739
45.705412	1494.701467	18.983757
45.697343	1496.170954	18.988775
45.918551	1504.001366	18.993792
45.899852	1498.650766	18.998810
46.007996	1497.889978	19.003827
45.994035	1495.230247	19.008845
45.908231	1492.847804	19.013863
46.125291	1505.371291	19.018880
45.776660	1499.381450	19.023898
46.549175	1506.765129	19.028915
46.493641	1516.150554	19.033933
46.634273	1504.374436	19.038951
46.661659	1502.432615	19.043968
46.494035	1506.844286	19.048986
46.443641	1493.476347	19.054003
46.390590	1516.612151	19.059021
46.362302	1523.243521	19.064039
46.886384	1518.902675	19.069056
46.878140	1526.368488	19.074074
46.824007	1517.073483	19.079091
46.780162	1536.767330	19.084109
46.416113	1518.155969	19.089127
46.871983	1525.465908	19.094144
46.638863	1526.266914	19.099162
46.909270	1524.829568	19.104179
46.602206	1522.721682	19.109197
46.764078	1522.705880	19.114215
47.361818	1536.039328	19.119232
46.760731	1557.845447	19.124250
47.305331	1550.120951	19.129267
47.504835	1562.181666	19.134285
47.671279	1545.369460	19.139303
47.651928	1543.235013	19.144320
47.699523	1554.295010	19.149338
47.703062	1536.265038	19.154355
47.428185	1517.865623	19.159373
47.608511	1528.416548	19.164391
47.766122	1533.903671	19.169408
47.416236	1537.768492	19.174426
47.580379	1537.815303	19.179443
47.619443	1541.104078	19.184461
47.914481	1546.290420	19.189479
47.865228	1548.705315	19.194496
47.539740	1543.306083	19.199514
47.796195	1540.084880	19.204531
47.867184	1543.083318	19.209549
47.690798	1545.484697	19.214567
47.881207	1536.939175	19.219584
47.943088	1549.597934	19.224602
48.223190	1547.802291	19.229619
48.041384	1562.238131	19.234637
48.291534	1567.296117	19.239655
48.633265	1565.419365	19.244672
48.139209	1567.380642	19.249690
48.366202	1566.132393	19.254707
48.421424	1565.637477	19.259725
48.469875	1562.664220	19.264743
48.475181	1564.565731	19.269760
48.285043	1567.424506	19.274778
48.181564	1564.755626	19.279795
48.480128	1563.644298	19.284813
48.373236	1564.236142	19.289831
48.753932	1562.228114	19.294848
48.739697	1587.367759	19.299866
48.877210	1593.375161	19.304883
48.994055	1609.366098	19.309901
49.094838	1601.929901	19.314919
49.282829	1595.139042	19.319936
49.105328	1597.317390	19.324954
49.030853	1598.145969	19.329971
49.173270	1602.774637	19.334989
48.642703	1599.872408	19.340007
49.127551	1589.394893	19.345024
48.786964	1601.137141	19.350042
49.077805	1588.167910	19.355059
49.185111	1597.277902	19.360077
49.057190	1617.311407	19.365095
49.427069	1618.322036	19.370112
49.482415	1629.739453	19.375130
49.749632	1618.494955	19.380147
49.664221	1609.463749	19.385165
49.455198	1615.461825	19.390183
49.801612	1613.179179	19.395200
49.643236	1619.814102	19.400218
49.991220	1608.148716	19.405235
49.974685	1609.708201	19.410253
50.201371	1608.929281	19.415271
50.259689	1603.424509	19.420288
50.221733	1609.100457	19.425306
50.366292	1608.893049	19.430323
50.304096	1607.992065	19.435341
50.054793	1607.832399	19.440359
50.271380	1601.976922	19.445376
50.101582	1619.548153	19.450394
50.109126	1606.912597	19.455411
50.204684	1611.534489	19.460429
50.561358	1623.322286	19.465447
51.011256	1628.552995	19.470464
50.604789	1636.303151	19.475482
50.978653	1633.192334	19.480499
51.041699	1608.425752	19.485517
50.829589	1601.903743	19.490535
50.836353	1587.902221	19.495552
50.789468	1600.739725	19.500570
50.734616	1582.341459	19.505587
50.966018	1598.937348	19.510605
51.075764	1609.763833	19.515623
51.051149	1616.879269	19.520640
50.868200	1627.946533	19.525658
51.094190	1621.855238	19.530675
51.408500	1619.183840	19.535693
51.087329	1622.835646	19.540711
51.174733	1624.528249	19.545728
51.030339	1628.762082	19.550746
51.368321	1624.295841	19.555763
51.279283	1616.300252	19.560781
51.251891	1629.851061	19.565799
51.275888	1622.855559	19.570816
51.382234	1617.182568	19.575834
51.483741	1620.751133	19.580851
51.715093	1631.691672	19.585869
51.459359	1640.956118	19.590887
51.948731	1644.651956	19.595904
52.017986	1646.778278	19.600922
51.871247	1645.966538	19.605939
52.146617	1644.026792	19.610957
52.015791	1645.852908	19.615975
52.169404	1650.396661	19.620992
52.003517	1654.397069	19.626010
51.963848	1653.752570	19.631027
52.289250	1635.552063	19.636045
52.066938	1643.529879	19.641063
52.159446	1642.583891	19.646080
52.370665	1640.407567	19.651098
52.331697	1647.617132	19.656115
52.204197	1639.307851	19.661133
52.228169	1650.818292	19.666151
52.129245	1640.924762	19.671168
52.305433	1659.345999	19.676186
52.237793	1664.463526	19.681203
52.590933	1672.059502	19.686221
52.353521	1674.258842	19.691239
52.521256	1675.874321	19.696256
52.488171	1676.080681	19.701274
52.581237	1676.518827	19.706291
52.893247	1684.661400	19.711309
52.904897	1698.920730	19.716327
53.057642	1690.452248	19.721344
53.192533	1688.337815	19.726362
53.174582	1693.634885	19.731379
53.561057	1686.070853	19.736397
53.330868	1691.971297	19.741415
53.270896	1684.194854	19.746432
53.722344	1691.228842	19.751450
53.340362	1698.809213	19.756467
53.423188	1689.289771	19.761485
53.597773	1694.538701	19.766503
53.751494	1682.682714	19.771520
53.667861	1683.053772	19.776538
53.545659	1689.005951	19.781555
53.819903	1680.816096	19.786573
53.316950	1686.681163	19.791591
53.774635	1679.488757	19.796608
53.839749	1697.442681	19.801626
53.873602	1704.808278	19.806643
54.451490	1707.183536	19.811661
53.926541	1711.984173	19.816679
53.964470	1720.180190	19.821696
53.931500	1706.200913	19.826714
54.010215	1713.099223	19.831731
54.188527	1701.239528	19.836749
53.594022	1716.221258	19.841767
54.238799	1723.601865	19.846784
54.249513	1731.637059	19.851802
54.108748	1740.239158	19.856819
54.422260	1733.373047	19.861837
54.651138	1744.885330	19.866855
54.412449	1737.231474	19.871872
54.737779	1739.844378	19.876890
54.591423	1737.175113	19.881907
55.051039	1738.844451	19.886925
55.064951	1735.665880	19.891943
54.922863	1735.445874	19.896960
54.839951	1723.579578	19.901978
54.748718	1742.470943	19.906995
55.531258	1746.827916	19.912013
55.310455	1761.110976	19.917031
55.440744	1741.135707	19.922048
55.598362	1732.611669	19.927066
55.071762	1725.896208	19.932083
55.574205	1715.536549	19.937101
55.564197	1725.036974	19.942119
55.270765	1712.758436	19.947136
55.520555	1726.976638	19.952154
55.643457	1746.534773	19.957171
56.060953	1741.334033	19.962189
55.778768	1740.353463	19.967207
55.888499	1720.321402	19.972224
55.948662	1722.214603	19.977242
55.912038	1712.178786	19.982259
55.901370	1714.719182	19.987277
56.016139	1727.175205	19.992295
55.956269	1738.667362	19.997312
56.275459	1744.856438	20.002330
55.780199	1750.199783	20.007347
56.340622	1739.880472	20.012365
55.787212	1748.627926	20.017383
56.217353	1751.654115	20.022400
56.076945	1748.568905	20.027418
56.132109	1743.070513	20.032435
56.320751	1744.539614	20.037453
56.257530	1752.511910	20.042471
56.324155	1767.540503	20.047488
56.683876	1770.911468	20.052506
56.557452	1778.797826	20.057523
56.593206	1772.458171	20.062541
56.598787	1786.997721	20.067559
56.750094	1772.116113	20.072576
56.769614	1762.989820	20.077594
56.954688	1767.317357	20.082611
57.057935	1766.345562	20.087629
56.789593	1779.414505	20.092647
57.444509	1792.468205	20.097664
57.393330	1796.204706	20.102682
57.160915	1801.011870	20.107699
57.246137	1809.199681	20.112717
57.249161	1804.049300	20.117735
57.420809	1799.107115	20.122752
58.045380	1789.996784	20.127770
57.698155	1799.033224	20.132787
57.734670	1788.674575	20.137805
57.743305	1786.486624	20.142823
57.882289	1784.545906	20.147840
57.651984	1784.243317	20.152858
57.648572	1796.169043	20.157875
57.741152	1782.383002	20.162893
57.961368	1787.282652	20.167911
57.929457	1786.026234	20.172928
58.075567	1795.896815	20.177946
57.865572	1788.385802	20.182963
58.263125	1794.622897	20.187981
58.156914	1815.508160	20.192999
58.420090	1812.634601	20.198016
58.672270	1806.999901	20.203034
58.970824	1818.033734	20.208051
58.745506	1798.072216	20.213069
58.368571	1788.116136	20.218087
58.320019	1783.096773	20.223104
58.537580	1796.160172	20.228122
58.362572	1802.825101	20.233139
58.420575	1802.579714	20.238157
58.247578	1813.841124	20.243175
58.338493	1813.723337	20.248192
58.686533	1821.422990	20.253210
58.814880	1833.690624	20.258227
58.892810	1830.000217	20.263245
58.860445	1837.073734	20.268263
59.026769	1841.793776	20.273280
58.997407	1830.305898	20.278298
59.202249	1838.759275	20.283315
59.198574	1834.206844	20.288333
58.957559	1845.670918	20.293351
59.388376	1853.098958	20.298368
59.934711	1863.187711	20.303386
59.672553	1867.835666	20.308403
59.996746	1862.952754	20.313421
59.797148	1866.750946	20.318439
60.015154	1857.808144	20.323456
60.118700	1843.966683	20.328474
59.642835	1836.464400	20.333491
59.717222	1841.328067	20.338509
59.709942	1860.388692	20.343527
60.096413	1856.037555	20.348544
59.831890	1850.576114	20.353562
60.086830	1852.863336	20.358579
60.018744	1854.830230	20.363597
59.937012	1856.774589	20.368615
60.038169	1851.966543	20.373632
60.547060	1877.713809	20.378650
60.655660	1886.465489	20.383667
60.618758	1887.675632	20.388685
60.753990	1885.691431	20.393703
60.696564	1887.746320	20.398720
61.064549	1878.928974	20.403738
61.112985	1878.213918	20.408755
61.165610	1877.838715	20.413773
60.863364	1865.206404	20.418791
60.744900	1871.854091	20.423808
60.986838	1869.323814	20.428826
60.847944	1879.541419	20.433843
61.032448	1877.098244	20.438861
61.264486	1881.288088	20.443879
61.204376	1882.633583	20.448896
61.319988	1872.802282	20.453914
61.115525	1881.104022	20.458931
61.138970	1881.314769	20.463949
61.246010	1884.152165	20.468967
61.165976	1894.350549	20.473984
61.367130	1894.384912	20.479002
61.795380	1907.622050	20.484019
61.869176	1916.247249	20.489037
61.749537	1907.162502	20.494055
61.777191	1923.286304	20.499072
61.605799	1910.775121	20.504090
61.323906	1918.890931	20.509107
61.655910	1927.334247	20.514125
62.154214	1938.241661	20.519143
61.780641	1946.425478	20.524160
62.227772	1946.024473	20.529178
61.978463	1946.165591	20.534195
62.189781	1939.718343	20.539213
62.469719	1940.118353	20.544231
62.208537	1961.751221	20.549248
62.895055	1958.798224	20.554266
63.021170	1961.076951	20.559283
63.021749	1963.452919	20.564301
63.120542	1938.346798	20.569319
62.834265	1937.178311	20.574336
62.851642	1930.661724	20.579354
63.047582	1944.013093	20.584371
62.818913	1948.544482	20.589389
62.990609	1950.226656	20.594407
62.801737	1948.594736	20.599424
63.168477	1949.949612	20.604442
63.094524	1953.479305	20.609459
63.330128	1951.953218	20.614477
63.224978	1953.393606	20.619495
63.292930	1952.404831	20.624512
63.287570	1942.125479	20.629530
63.136038	1948.880270	20.634547
62.975583	1955.779854	20.639565
63.260750	1966.409718	20.644583
63.642629	1979.219190	20.649600
63.879041	1974.240990	20.654618
63.874086	1984.365538	20.659635
63.635769	1984.407584	20.664653
63.907941	1973.012795	20.669671
63.694086	1979.616932	20.674688
64.198994	1991.992188	20.679706
64.054820	2002.562722	20.684723
64.435152	2010.713405	20.689741
64.632742	2001.823520	20.694759
64.540852	2010.558591	20.699776
64.409391	2010.464767	20.704794
64.468828	2006.776604	20.709811
64.590191	2010.524639	20.714829
64.960001	1999.590376	20.719847
64.598619	2008.401336	20.724864
64.592844	1998.112962	20.729882
64.686223	2005.094004	20.734899
64.495330	2009.068737	20.739917
64.804526	1996.988246	20.744935
64.642435	2010.822798	20.749952
65.444659	2007.081268	20.754970
64.958134	2017.301226	20.759987
65.163351	2028.381429	20.765005
65.223409	2031.394377	20.770023
65.452491	2029.881965	20.775040
65.615373	2032.821132	20.780058
65.947156	2013.589196	20.785075
65.753481	2021.459294	20.790093
65.947477	2011.966455	20.795111
66.103833	2020.336651	20.800128
66.187689	2002.260111	20.805146
66.094285	1996.409154	20.810163
65.619817	1979.759294	20.815181
65.972845	1975.467619	20.820199
65.823378	1990.552814	20.825216
66.186745	2004.671295	20.830234
66.238621	2009.891907	20.835251
66.113728	2012.263539	20.840269
66.197047	2005.509582	20.845287
66.090660	2011.686816	20.850304
66.195738	2008.266266	20.855322
66.200311	2004.273440	20.860339
66.231755	2022.299479	20.865357
66.600490	2009.815380	20.870375
66.510384	2033.997094	20.875392
66.796975	2030.696767	20.880410
66.895103	2037.489239	20.885427
66.653632	2035.296756	20.890445
66.970397	2025.766182	20.895463
66.898548	2032.156583	20.900480
66.686424	2034.223422	20.905498
67.086160	2037.502756	20.910515
67.088864	2028.061383	20.915533
67.283090	2032.234717	20.920551
67.160018	2028.343809	20.925568
67.039078	2045.425902	20.930586
67.205467	2051.651126	20.935603
67.150510	2065.884855	20.940621
67.632046	2061.780069	20.945639
67.626186	2067.224865	20.950656
67.816497	2064.274393	20.955674
67.497364	2057.784150	20.960691
67.738122	2065.972232	20.965709
67.922295	2055.445164	20.970727
67.802760	2068.486075	20.975744
67.511110	2066.848388	20.980762
67.919739	2074.490855	20.985779
67.944202	2087.491315	20.990797
67.935497	2093.743687	20.995815
67.822473	2090.869213	21.000832
68.215616	2084.080661	21.005850
68.414727	2108.559704	21.010867
68.172752	2121.458014	21.015885
68.800468	2120.700613	21.020903
68.846677	2120.178832	21.025920
68.657444	2119.401293	21.030938
68.927880	2111.923272	21.035955
68.716452	2126.305108	21.040973
69.096278	2114.858465	21.045991
68.669791	2112.751838	21.051008
68.948881	2112.542145	21.056026
69.015702	2122.189102	21.061043
68.881061	2118.946557	21.066061
69.513061	2120.299492	21.071079
69.407229	2137.735479	21.076096
69.372837	2134.819975	21.081114
69.788533	2135.584836	21.086131
69.390873	2136.928577	21.091149
69.737089	2122.271332	21.096167
69.834549	2136.129396	21.101184
70.097555	2119.211545	21.106202
70.087823	2122.243197	21.111219
70.167453	2125.858036	21.116237
70.088755	2125.427486	21.121255
69.825650	2127.346509	21.126272
69.984891	2124.980723	21.131290
70.410068	2126.031020	21.136307
70.182091	2123.449269	21.141325
70.181498	2114.226111	21.146343
70.361717	2133.894501	21.151360
70.110536	2123.160602	21.156378
70.201698	2130.956646	21.161395
70.080715	2149.055015	21.166413
70.633837	2148.596628	21.171431
70.459957	2149.076396	21.176448
70.726251	2157.750053	21.181466
70.573768	2148.101718	21.186483
70.192627	2156.895965	21.191501
70.869001	2174.141367	21.196519
70.797655	2184.544012	21.201536
70.955344	2187.397062	21.206554
71.028550	2179.408864	21.211571
71.148601	2180.376013	21.216589
71.474997	2190.023181	21.221607
71.393784	2200.407003	21.226624
71.985587	2203.446970	21.231642
71.929980	2187.772173	21.236659
71.658236	2178.256239	21.241677
71.746416	2176.559353	21.246695
71.885450	2197.170509	21.251712
71.734329	2197.240191	21.256730
72.214444	2190.212726	21.261747
72.041128	2201.937469	21.266765
72.415486	2205.156095	21.271783
71.769070	2203.792710	21.276800
72.023795	2201.974047	21.281818
72.007155	2202.415480	21.286835
71.836546	2204.943166	21.291853
71.923100	2205.709974	21.296871
72.216821	2218.370515	21.301888
72.359852	2221.463020	21.306906
72.550735	2226.888954	21.311923
72.590401	2240.422458	21.316941
72.505358	2231.132161	21.321959
72.560854	2236.284531	21.326976
72.440224	2247.477707	21.331994
72.636648	2253.425181	21.337011
73.068966	2262.455171	21.342029
73.092546	2252.273170	21.347047
72.910584	2260.534757	21.352064
73.268412	2254.407920	21.357082
73.512832	2251.647638	21.362099
73.477461	2252.125256	21.367117
73.779916	2248.691930	21.372135
73.818509	2242.513032	21.377152
73.620120	2248.913527	21.382170
73.885685	2240.866164	21.387187
73.915491	2245.135387	21.392205
74.046561	2245.971179	21.397223
73.845547	2250.614990	21.402240
74.239502	2263.318360	21.407258
74.389415	2260.443858	21.412275
74.205233	2273.659467	21.417293
74.618587	2270.984101	21.422311
74.654551	2272.293190	21.427328
74.064266	2267.077869	21.432346
74.828513	2262.348477	21.437363
74.773786	2269.542052	21.442381
74.556184	2265.243950	21.447399
74.674481	2261.229796	21.452416
74.912578	2268.369982	21.457434
75.095554	2267.629005	21.462451
74.918493	2273.557847	21.467469
74.788309	2261.644662	21.472487
74.714605	2264.472008	21.477504
74.522259	2260.122858	21.482522
74.672641	2278.511325	21.487539
75.184295	2293.454264	21.492557
75.226417	2296.579696	21.497575
74.978843	2296.610287	21.502592
75.150137	2305.289186	21.507610
75.621687	2322.719191	21.512627
75.460780	2326.781542	21.517645
76.017901	2325.385850	21.522663
76.158830	2321.157678	21.527680
75.983964	2330.128770	21.532698
76.261612	2310.148360	21.537715
76.491556	2317.862378	21.542733
76.666340	2315.842021	21.547751
76.406719	2315.970680	21.552768
76.100375	2307.274610	21.557786
76.535246	2309.583968	21.562803
76.320368	2311.026089	21.567821
76.506537	2310.863334	21.572839
76.872330	2317.201987	21.577856
76.363500	2308.618702	21.582874
76.666667	2309.208963	21.587891
76.362180	2313.303834	21.592909
76.442477	2328.333455	21.597927
76.708070	2334.580496	21.602944
76.827023	2348.681642	21.607962
76.734102	2337.950426	21.612979
76.665163	2353.301337	21.617997
76.952417	2360.169215	21.623015
76.857958	2370.238809	21.628032
77.222747	2378.099742	21.633050
77.273657	2382.240689	21.638067
77.213584	2383.840165	21.643085
77.287963	2380.447471	21.648103
77.299415	2390.553808	21.653120
77.317889	2405.942607	21.658138
77.974349	2404.360315	21.663155
77.512989	2403.782715	21.668173
77.881100	2399.607322	21.673191
77.921043	2395.206931	21.678208
77.849959	2420.813686	21.683226
77.943247	2420.299425	21.688243
78.158429	2421.722054	21.693261
78.147208	2420.321197	21.698279
78.656608	2419.269659	21.703296
78.327720	2414.788822	21.708314
78.560758	2411.131163	21.713331
78.414731	2426.083921	21.718349
78.899492	2437.842786	21.723367
79.079210	2439.178395	21.728384
79.109977	2443.267585	21.733402
79.168357	2440.869301	21.738419
80.230582	2422.275731	21.743437
80.234635	2408.560936	21.748455
80.242775	2388.334655	21.753472
80.238637	2387.029871	21.758490
80.369523	2376.049224	21.763507
80.177484	2370.586181	21.768525
80.192468	2354.958934	21.773543
80.155701	2348.950789	21.778560
80.083974	2356.104314	21.783578
80.517742	2346.086766	21.788595
80.646654	2351.155317	21.793613
80.238296	2347.968449	21.798631
80.313326	2348.050942	21.803648
80.098937	2350.338282	21.808666
80.455889	2345.561198	21.813683
80.444250	2340.015428	21.818701
80.182301	2345.572961	21.823719
80.697671	2339.306914	21.828736
80.483102	2349.827963	21.833754
80.613058	2347.900094	21.838771
80.808459	2351.908749	21.843789
80.446169	2347.075993	21.848807
80.440788	2344.787928	21.853824
80.375663	2363.593818	21.858842
80.629605	2362.343786	21.863859
80.725561	2367.026864	21.868877
80.436135	2374.723678	21.873895
80.936176	2392.640380	21.878912
80.544522	2400.131355	21.883930
80.825214	2408.670474	21.888947
81.200432	2419.533330	21.893965
81.230216	2434.985241	21.898983
81.188945	2435.483138	21.904000
81.213477	2439.147366	21.909018
81.597346	2453.464432	21.914035
81.667839	2462.014496	21.919053
81.567459	2470.859113	21.924071
81.905583	2462.447991	21.929088
81.974280	2471.807835	21.934106
82.330066	2479.315188	21.939123
82.802238	2481.502622	21.944141
82.590364	2479.654774	21.949159
83.146067	2477.895907	21.954176
82.794724	2480.035942	21.959194
82.923443	2474.569951	21.964211
82.905069	2453.432213	21.969229
82.544222	2454.686393	21.974247
83.204596	2459.625317	21.979264
82.937658	2478.784973	21.984282
82.966415	2469.678778	21.989299
83.296815	2475.522968	21.994317
82.858664	2476.384471	21.999335
83.319091	2471.528339	22.004352
83.157444	2476.701126	22.009370
83.180681	2485.513003	22.014387
83.173270	2483.434318	22.019405
83.316145	2503.336557	22.024423
83.460673	2505.767429	22.029440
83.341279	2518.579551	22.034458
83.662147	2512.114256	22.039475
83.782291	2510.725812	22.044493
83.691214	2525.855367	22.049511
83.894368	2530.863606	22.054528
83.973172	2530.325370	22.059546
83.904099	2534.410704	22.064563
84.105248	2535.767169	22.069581
84.257560	2554.431638	22.074599
84.816532	2554.734899	22.079616
84.470776	2565.920440	22.084634
84.580383	2558.203175	22.089651
84.490473	2560.736011	22.094669
84.495822	2566.714180	22.099687
85.377503	2560.885615	22.104704
85.144205	2568.244442	22.109722
85.130667	2583.412350	22.114739
85.446854	2583.407915	22.119757
85.435295	2587.295507	22.124775
85.768833	2581.385581	22.129792
85.907097	2593.628546	22.134810
85.987944	2580.761110	22.139827
85.949484	2587.826139	22.144845
85.751658	2584.753451	22.149863
85.988678	2579.855277	22.154880
85.843519	2588.388492	22.159898
85.674627	2585.745266	22.164915
85.833753	2576.887826	22.169933
85.925737	2580.268425	22.174951
86.007249	2583.591709	22.179968
86.224108	2602.870731	22.184986
86.131540	2610.066814	22.190003
86.472002	2605.771547	22.195021
86.422261	2610.502534	22.200039
86.506364	2613.083629	22.205056
86.381597	2613.650527	22.210074
86.834484	2628.195272	22.215091
86.775046	2638.700183	22.220109
86.733952	2634.469105	22.225127
87.337124	2628.645066	22.230144
87.543530	2620.451427	22.235162
87.651745	2625.357359	22.240179
87.900471	2619.924526	22.245197
87.447422	2620.090843	22.250215
87.566977	2629.789984	22.255232
87.576386	2628.978226	22.260250
87.564189	2624.915584	22.265267
87.771272	2634.487184	22.270285
87.467102	2652.084273	22.275303
88.056788	2661.284419	22.280320
88.009784	2662.822693	22.285338
87.831687	2661.383402	22.290355
88.224128	2660.824931	22.295373
87.677285	2672.203422	22.300391
88.289657	2680.472206	22.305408
88.773138	2690.712114	22.310426
88.548976	2689.317092	22.315443
88.749778	2690.890175	22.320461
88.699560	2684.877049	22.325479
88.712137	2688.502770	22.330496
88.788515	2685.910109	22.335514
88.946213	2689.414857	22.340531
89.373844	2704.017416	22.345549
89.209173	2711.853907	22.350567
89.455573	2714.407653	22.355584
89.003010	2717.970516	22.360602
89.048885	2716.689284	22.365619
89.493373	2708.619033	22.370637
89.307601	2712.436391	22.375655
89.834154	2716.658232	22.380672
89.577283	2732.335251	22.385690
89.548839	2736.326873	22.390707
89.932648	2734.839472	22.395725
89.910167	2736.484314	22.400743
90.015944	2740.626081	22.405760
90.292008	2743.464287	22.410778
90.296639	2759.447105	22.415795
90.752958	2751.291792	22.420813
90.811056	2765.569580	22.425831
90.581791	2757.888846	22.430848
90.801287	2760.762442	22.435866
90.808089	2761.353546	22.440883
91.232928	2757.582039	22.445901
91.083319	2764.251818	22.450919
91.105856	2754.696466	22.455936
91.199554	2758.350850	22.460954
91.109563	2761.002242	22.465971
91.168508	2749.472235	22.470989
91.172702	2774.718618	22.476007
91.521870	2774.763824	22.481024
91.944030	2773.142480	22.486042
91.421377	2786.706914	22.491059
91.729187	2774.890635	22.496077
91.616384	2779.298671	22.501095
91.628711	2801.777063	22.506112
91.951824	2806.903652	22.511130
91.755462	2817.525538	22.516147
92.125297	2805.689479	22.521165
91.847027	2812.696426	22.526183
92.464390	2825.849380	22.531200
92.807578	2828.909137	22.536218
92.433419	2825.775149	22.541235
92.851866	2829.464562	22.546253
92.772780	2832.790571	22.551271
93.255334	2829.484680	22.556288
93.538194	2817.574084	22.561306
93.133335	2830.377994	22.566323
93.381609	2817.362453	22.571341
93.365443	2823.133259	22.576359
93.487719	2842.411761	22.581376
93.944730	2845.642381	22.586394
93.807277	2849.495839	22.591411
94.223363	2845.939165	22.596429
93.714564	2849.012554	22.601447
93.822493	2844.802325	22.606464
94.296684	2841.750198	22.611482
94.157401	2845.510253	22.616499
94.523563	2836.379663	22.621517
94.081371	2843.637107	22.626535
94.424647	2848.161112	22.631552
94.345868	2841.784146	22.636570
94.146274	2852.202644	22.641587
94.312130	2840.804811	22.646605
94.457946	2868.052337	22.651623
94.324364	2876.233370	22.656640
94.259606	2870.907275	22.661658
94.358800	2878.657869	22.666675
94.523610	2890.821849	22.671693
95.100357	2902.465777	22.676711
94.931801	2904.713295	22.681728
95.211191	2906.663916	22.686746
95.172044	2908.717083	22.691763
95.636667	2914.116667	22.696781
95.539157	2937.074165	22.701799
95.579602	2937.334074	22.706816
96.102212	2925.265436	22.711834
95.892996	2933.698060	22.716851
95.754576	2927.867618	22.721869
96.010343	2928.028747	22.726887
96.383234	2935.464184	22.731904
96.444886	2944.041969	22.736922
96.286273	2958.612657	22.741939
96.288299	2952.745480	22.746957
96.195480	2955.536754	22.751975
96.675217	2960.018034	22.756992
96.691878	2956.820252	22.762010
96.440487	2964.814990	22.767027
96.755670	2974.008576	22.772045
97.132268	2983.155344	22.777063
96.912071	2984.016874	22.782080
97.235783	2981.563388	22.787098
97.440272	2989.350874	22.792115
97.536373	2990.644518	22.797133
97.804522	3017.914498	22.802151
97.819749	3009.882752	22.807168
97.855198	3005.290403	22.812186
97.838081	3008.680171	22.817203
97.911883	3009.679471	22.822221
98.001322	3006.732594	22.827239
98.026326	3010.322463	22.832256
98.461283	3005.582221	22.837274
98.124813	3011.891399	22.842291
98.343608	3016.160926	22.847309
98.531515	3029.964203	22.852327
98.275057	3039.899327	22.857344
98.550444	3037.412916	22.862362
98.754581	3045.735566	22.867379
99.124331	3057.939246	22.872397
99.082968	3067.169696	22.877415
99.088298	3072.221223	22.882432
99.088994	3074.739872	22.887450
98.847566	3067.633489	22.892467
99.437095	3068.215173	22.897485
99.352872	3061.483484	22.902503
99.760679	3083.550471	22.907520
100.014876	3087.055810	22.912538
99.822343	3090.587354	22.917555
99.917143	3087.164733	22.922573
100.110887	3089.897778	22.927591
100.029131	3092.168301	22.932608
100.163903	3085.832524	22.937626
100.212933	3086.463083	22.942643
100.487563	3098.824739	22.947661
100.760035	3116.368256	22.952679
100.674935	3114.467764	22.957696
100.861453	3108.721061	22.962714
101.039545	3110.964154	22.967731
100.914147	3111.832379	22.972749
101.252559	3112.280586	22.977767
100.827808	3114.426210	22.982784
101.321880	3102.622435	22.987802
101.000529	3116.911630	22.992819
101.246853	3119.291035	22.997837
101.365286	3131.660956	23.002855
101.099555	3136.209870	23.007872
101.427981	3127.582665	23.012890
101.378260	3142.149208	23.017907
101.754636	3158.654561	23.022925
101.843126	3160.016419	23.027943
101.991020	3172.978768	23.032960
102.131446	3168.908733	23.037978
102.314374	3160.641936	23.042995
102.472156	3167.540353	23.048013
102.695631	3171.734335	23.053031
102.779620	3180.236091	23.058048
102.916248	3181.282840	23.063066
102.741869	3188.201423	23.068083
103.050515	3182.792694	23.073101
103.215054	3180.411303	23.078119
103.057793	3182.095914	23.083136
103.215782	3178.808060	23.088154
102.937515	3188.968967	23.093171
103.415284	3196.779653	23.098189
103.348502	3198.656727	23.103207
103.274016	3209.657082	23.108224
103.824785	3205.603891	23.113242
103.536012	3209.386120	23.118259
103.807363	3221.309406	23.123277
104.040562	3233.068161	23.128295
104.037996	3239.572750	23.133312
104.348922	3233.261974	23.138330
104.217749	3240.966380	23.143347
104.343951	3242.842100	23.148365
104.686686	3253.951119	23.153383
104.836260	3263.417301	23.158400
104.926334	3264.291855	23.163418
105.292865	3260.053502	23.168435
105.029905	3258.483362	23.173453
105.156699	3261.375214	23.178471
105.181637	3265.066343	23.183488
105.466072	3253.665435	23.188506
105.310427	3262.772855	23.193523
105.150416	3274.672189	23.198541
105.718661	3283.966437	23.203559
105.645959	3281.113782	23.208576
105.754703	3276.636350	23.213594
105.933385	3292.326988	23.218611
106.164117	3305.916682	23.223629
106.836371	3307.333130	23.228647
106.340007	3310.299806	23.233664
106.825679	3302.966568	23.238682
106.536388	3314.532268	23.243699
106.700459	3320.828080	23.248717
106.915329	3312.585819	23.253735
106.742576	3322.767471	23.258752
106.665556	3323.909582	23.263770
106.891711	3315.131933	23.268787
107.023146	3317.683624	23.273805
107.401563	3324.746250	23.278823
107.345020	3333.402164	23.283840
107.512988	3329.654311	23.288858
107.477837	3338.388963	23.293875
107.615858	3335.102820	23.298893
107.606064	3337.269285	23.303911
107.746221	3349.539698	23.308928
107.759257	3360.753982	23.313946
108.289384	3354.235456	23.318963
107.943767	3355.263529	23.323981
108.448436	3354.510388	23.328999
108.267834	3356.515067	23.334016
108.479364	3362.573854	23.339034
108.599212	3379.178770	23.344051
108.709785	3386.584782	23.349069
109.220467	3380.866794	23.354087
108.997891	3377.345657	23.359104
109.030790	3388.405859	23.364122
108.873741	3391.035033	23.369139
108.811247	3390.551355	23.374157
109.870427	3400.745677	23.379175
109.349261	3418.662390	23.384192
109.966092	3404.371221	23.389210
110.175480	3399.345482	23.394227
110.402782	3391.705895	23.399245
110.471830	3387.175180	23.404263
110.328872	3388.519216	23.409280
110.107746	3386.302681	23.414298
110.605781	3386.055019	23.419315
110.650802	3396.906107	23.424333
110.837455	3385.875716	23.429351
110.334670	3393.455320	23.434368
110.413027	3389.792036	23.439386
110.438781	3387.470689	23.444403
110.654457	3398.718654	23.449421
110.657772	3396.313231	23.454439
110.968019	3414.302818	23.459456
111.052003	3417.721154	23.464474
110.997022	3423.053315	23.469491
110.801913	3444.485899	23.474509
111.296166	3449.653167	23.479527
111.301529	3458.159479	23.484544
111.502146	3471.203875	23.489562
112.049590	3489.112788	23.494579
111.627119	3494.132384	23.499597
111.989650	3474.632888	23.504615
111.782750	3496.728591	23.509632
112.364147	3507.789863	23.514650
112.889905	3507.912827	23.519667
113.003141	3507.465697	23.524685
113.022625	3505.089464	23.529703
112.942927	3507.735333	23.534720
112.997722	3511.104598	23.539738
113.448982	3508.159711	23.544755
112.791199	3507.211118	23.549773
113.288171	3526.106119	23.554791
113.195907	3536.962006	23.559808
113.390070	3540.677052	23.564826
113.387490	3542.423800	23.569843
113.397125	3542.865629	23.574861
113.918671	3561.799507	23.579879
113.942908	3573.562534	23.584896
113.964169	3573.589790	23.589914
114.011939	3569.447244	23.594931
114.106225	3574.778276	23.599949
114.769197	3575.972648	23.604967
114.531732	3580.346501	23.609984
114.676444	3584.451706	23.615002
115.036069	3583.382072	23.620019
114.866969	3586.422379	23.625037
115.218316	3580.057106	23.630055
115.131155	3585.408450	23.635072
114.849851	3585.169811	23.640090
115.225466	3598.416754	23.645107
114.826570	3610.388721	23.650125
115.061304	3609.335115	23.655143
115.332558	3631.309024	23.660160
115.446413	3629.289964	23.665178
115.663764	3632.596017	23.670195
115.553948	3641.056207	23.675213
116.218247	3653.309056	23.680231
116.441560	3671.155495	23.685248
116.421184	3657.183004	23.690266
116.972424	3662.994096	23.695283
116.835733	3664.709990	23.700301
117.695584	3653.990421	23.705319
117.264901	3645.310715	23.710336
117.411589	3646.424730	23.715354
117.067625	3632.176864	23.720371
117.341726	3640.285822	23.725389
117.879673	3642.990510	23.730407
117.421884	3643.523405	23.735424
117.233498	3650.299228	23.740442
117.472826	3652.801151	23.745459
117.359005	3645.666603	23.750477
117.482830	3646.063472	23.755495
117.947277	3674.123725	23.760512
117.942262	3679.560280	23.765530
117.744637	3678.353690	23.770547
117.886542	3702.643152	23.775565
118.194187	3702.935057	23.780583
117.936820	3712.290377	23.785600
118.143567	3714.785519	23.790618
118.845357	3738.100004	23.795635
118.456737	3742.451771	23.800653
118.704386	3743.499009	23.805671
118.718141	3761.589848	23.810688
119.540562	3772.239954	23.815706
119.496385	3774.577174	23.820723
119.353256	3774.258082	23.825741
119.728996	3761.210734	23.830759
119.878137	3776.131874	23.835776
119.766651	3787.117127	23.840794
120.151250	3790.911231	23.845811
119.797237	3792.517959	23.850829
120.228505	3793.452000	23.855847
120.479759	3788.402644	23.860864
120.521648	3803.049078	23.865882
120.775672	3815.784458	23.870899
120.933047	3814.726763	23.875917
121.371216	3811.262675	23.880935
121.310668	3821.520897	23.885952
121.013145	3824.815690	23.890970
121.603205	3815.155536	23.895987
121.252693	3819.098974	23.901005
121.187840	3818.996035	23.906023
121.269346	3825.859776	23.911040
121.184536	3845.483023	23.916058
121.723132	3844.036346	23.921075
121.347869	3850.439322	23.926093
121.615962	3872.123115	23.931111
121.903805	3879.811359	23.936128
122.150549	3879.051840	23.941146
122.706361	3880.832228	23.946163
123.004941	3900.605639	23.951181
123.617077	3872.480418	23.956199
123.697363	3869.089176	23.961216
123.549988	3859.906703	23.966234
123.915457	3843.321581	23.971251
123.660509	3842.627321	23.976269
123.531340	3831.663669	23.981287
124.092961	3842.169738	23.986304
123.932380	3831.333368	23.991322
124.144608	3841.145832	23.996339
124.130932	3838.042686	24.001357
123.921975	3839.659963	24.006375
123.900101	3832.413975	24.011392
124.061801	3838.187887	24.016410
124.516393	3849.989856	24.021427
124.183747	3870.495367	24.026445
124.376460	3868.463173	24.031463
124.804203	3861.058193	24.036480
124.814201	3866.366319	24.041498
124.768573	3861.980130	24.046515
124.804682	3869.139265	24.051533
124.816669	3886.087487	24.056551
124.909001	3893.751922	24.061568
125.191731	3900.594463	24.066586
125.433934	3892.068976	24.071603
125.189784	3915.468078	24.076621
125.805486	3924.319732	24.081639
125.825321	3920.775512	24.086656
125.243270	3927.972429	24.091674
125.737307	3947.868558	24.096691
126.027817	3949.933624	24.101709
126.048845	3959.872042	24.106727
126.346738	3963.495140	24.111744
126.476406	3976.711219	24.116762
127.042378	3970.445574	24.121779
126.804028	3979.319483	24.126797
126.591841	3981.365320	24.131815
126.707273	3991.304214	24.136832
126.988078	3997.562396	24.141850
127.199663	3992.745187	24.146867
127.441370	4006.637646	24.151885
127.579215	4016.066465	24.156903
127.968609	4018.357267	24.161920
128.099604	4015.865168	24.166938
128.354071	4015.524101	24.171955
128.232232	4018.295972	24.176973
127.984524	4009.171034	24.181991
128.459816	4027.536712	24.187008
128.616141	4048.469536	24.192026
128.812295	4041.867627	24.197043
128.634602	4048.350071	24.202061
128.767683	4045.885185	24.207079
128.779969	4058.877499	24.212096
129.088574	4072.079674	24.217114
129.237692	4078.448366	24.222131
129.218374	4081.982059	24.227149
129.294671	4091.328225	24.232167
129.421153	4095.676785	24.237184
129.422183	4114.254072	24.242202
130.023822	4115.448446	24.247219
130.179523	4118.533714	24.252237
130.550408	4125.621191	24.257255
130.542241	4120.542387	24.262272
130.710711	4126.261729	24.267290
130.871421	4128.448797	24.272307
131.139452	4133.048687	24.277325
131.289290	4126.222911	24.282343
131.476948	4119.755865	24.287360
131.081173	4116.426748	24.292378
131.161264	4128.626248	24.297395
131.423343	4142.244539	24.302413
131.693579	4156.248155	24.307431
131.480901	4149.151854	24.312448
131.598018	4159.727674	24.317466
131.792094	4160.740137	24.322483
131.926076	4176.984053	24.327501
131.492271	4186.993472	24.332519
131.849978	4185.698496	24.337536
132.130392	4208.812412	24.342554
132.217342	4210.619565	24.347571
132.749568	4224.295413	24.352589
132.514090	4238.362664	24.357607
132.911673	4243.873085	24.362624
132.832426	4250.281765	24.367642
132.904106	4240.501559	24.372659
133.099834	4258.128417	24.377677
133.429594	4266.051261	24.382695
133.774778	4266.534216	24.387712
133.828480	4270.933113	24.392730
133.888794	4263.402362	24.397747
134.125313	4260.640684	24.402765
134.420400	4270.129366	24.407783
134.883725	4271.292794	24.412800
134.675283	4284.533424	24.417818
135.070431	4274.944363	24.422835
135.109926	4276.020717	24.427853
135.123948	4283.197493	24.432871
135.586887	4270.931415	24.437888
135.378131	4276.999368	24.442906
135.288166	4269.380971	24.447923
135.645562	4271.437722	24.452941
135.524711	4269.519010	24.457959
135.537938	4271.847159	24.462976
135.753887	4260.115120	24.467994
135.846930	4280.410642	24.473011
136.226751	4289.270203	24.478029
136.153735	4296.429160	24.483047
136.511588	4289.195462	24.488064
136.451775	4293.234432	24.493082
136.526662	4300.898815	24.498099
136.882059	4320.006525	24.503117
136.628542	4322.849157	24.508135
136.833849	4321.826778	24.513152
136.828164	4327.323128	24.518170
137.049057	4346.969048	24.523187
137.156770	4356.189661	24.528205
137.104317	4359.590319	24.533223
137.520889	4359.921235	24.538240
137.818373	4368.973292	24.543258
138.086297	4369.929791	24.548275
137.985868	4370.516724	24.553293
138.263483	4386.418042	24.558311
138.493351	4403.937012	24.563328
138.077423	4397.666624	24.568346
138.318092	4413.793828	24.573363
138.540357	4406.833829	24.578381
138.805940	4436.824468	24.583399
139.204235	4429.810006	24.588416
139.132523	4449.647221	24.593434
139.392717	4461.362648	24.598451
139.538649	4464.608295	24.603469
139.795218	4462.701657	24.608487
139.877434	4468.821347	24.613504
140.092581	4460.541821	24.618522
140.252493	4466.181595	24.623539
140.617078	4471.380208	24.628557
140.648138	4480.460064	24.633575
140.724159	4484.816724	24.638592
140.800235	4483.036155	24.643610
140.918871	4479.534062	24.648627
140.952037	4475.865828	24.653645
140.955307	4477.032481	24.658663
141.134900	4493.314822	24.663680
141.019210	4502.367099	24.668698
141.338061	4516.966209	24.673715
141.944088	4505.206182	24.678733
141.614288	4516.570011	24.683751
142.247730	4530.176545	24.688768
141.997662	4541.480678	24.693786
142.243693	4542.165977	24.698803
142.477410	4534.427511	24.703821
142.145220	4540.171924	24.708839
142.640131	4533.653258	24.713856
142.748142	4543.383466	24.718874
143.139101	4560.241879	24.723891
143.201096	4560.364748	24.728909
142.932395	4567.401201	24.733927
143.007220	4561.783966	24.738944
143.114253	4573.633608	24.743962
143.549670	4581.754054	24.748979
143.775720	4585.954293	24.753997
143.949932	4593.828337	24.759015
144.082067	4584.211917	24.764032
144.220911	4587.689515	24.769050
144.073815	4604.816944	24.774067
144.475130	4605.989128	24.779085
144.446778	4620.023876	24.784103
144.210761	4618.316417	24.789120
144.753036	4624.789715	24.794138
144.412685	4636.520800	24.799155
145.258749	4630.977780	24.804173
145.390973	4643.848663	24.809191
145.732083	4656.595853	24.814208
145.799383	4666.842440	24.819226
146.034018	4663.773865	24.824243
146.017905	4663.405689	24.829261
146.227038	4665.524934	24.834279
146.391752	4659.756483	24.839296
146.357691	4656.633329	24.844314
146.444841	4673.760497	24.849331
146.792295	4680.722178	24.854349
146.768618	4681.937426	24.859367
147.405585	4676.853620	24.864384
147.134543	4676.593959	24.869402
146.955275	4694.354500	24.874419
147.422267	4701.485336	24.879437
147.348607	4713.755730	24.884455
147.610855	4705.811617	24.889472
147.712619	4717.365340	24.894490
147.590306	4743.136797	24.899507
148.268787	4742.700451	24.904525
148.403270	4741.957580	24.909543
148.380374	4746.132289	24.914560
148.350486	4776.828701	24.919578
148.220337	4772.097574	24.924595
148.715258	4778.972578	24.929613
148.800868	4785.373770	24.934631
148.951837	4788.328044	24.939648
149.111465	4793.136336	24.944666
149.460801	4800.441127	24.949683
149.646824	4810.818501	24.954701
149.488125	4828.315097	24.959719
149.871884	4812.776900	24.964736
150.109695	4828.482882	24.969754
150.062351	4846.758780	24.974771
150.216391	4846.335548	24.979789
150.376495	4855.842293	24.984807
150.567052	4858.715185	24.989824
151.040522	4870.064708	24.994842
150.986456	4875.902422	24.999859
151.295444	4870.430453	25.004877
151.468172	4866.864158	25.009895
151.780297	4870.020057	25.014912
151.549436	4880.876276	25.019930
151.766217	4906.465645	25.024947
151.898759	4897.197852	25.029965
151.611458	4906.268639	25.034983
152.034520	4911.478159	25.040000
152.586262	4922.127182	25.045018
152.146613	4936.448709	25.050035
152.635863	4931.223984	25.055053
152.672166	4934.913225	25.060071
152.901874	4926.899590	25.065088
152.740544	4943.917132	25.070106
152.783595	4958.092315	25.075123
153.052622	4956.456830	25.080141
153.036914	4971.723100	25.085159
153.324593	4988.984251	25.090176
153.464842	4996.078949	25.095194
153.486845	5001.681191	25.100211
153.958040	5012.029425	25.105229
154.071836	5025.113960	25.110247
154.196979	5027.696906	25.115264
154.573558	5039.302858	25.120282
154.662634	5051.927651	25.125299
154.918405	5045.530421	25.130317
154.552919	5059.946844	25.135335
154.901852	5073.933480	25.140352
155.363281	5083.791947	25.145370
155.437562	5085.379216	25.150387
155.627682	5095.931723	25.155405
155.665211	5108.916380	25.160423
155.851964	5113.738378	25.165440
156.029214	5107.788116	25.170458
156.459507	5126.911931	25.175475
156.774554	5130.434402	25.180493
156.610932	5137.537916	25.185511
156.513322	5129.376165	25.190528
157.000537	5137.449704	25.195546
157.136004	5159.442023	25.200563
157.516152	5153.862837	25.205581
157.647775	5164.473940	25.210599
157.937601	5166.386892	25.215616
157.919463	5159.844540	25.220634
158.003599	5168.804928	25.225651
158.388612	5175.611739	25.230669
158.395699	5185.333125	25.235687
158.288505	5185.000549	25.240704
158.623366	5184.953646	25.245722
158.368358	5193.191501	25.250739
159.219031	5205.305533	25.255757
159.043957	5219.242336	25.260775
159.021054	5214.183741	25.265792
159.275367	5213.191755	25.270810
159.248209	5226.051008	25.275827
159.636138	5235.772935	25.280845
159.356533	5241.129255	25.285863
159.668880	5243.971742	25.290880
159.843134	5254.675055	25.295898
159.824280	5270.883282	25.300915
160.482519	5282.077180	25.305933
160.529598	5302.259586	25.310951
160.424115	5300.287788	25.315968
160.949594	5306.482213	25.320986
161.192408	5315.588795	25.326003
161.360810	5315.087559	25.331021
161.487360	5314.591703	25.336039
161.378040	5320.981400	25.341056
161.895902	5324.384369	25.346074
161.883549	5332.334677	25.351091
162.086466	5338.486630	25.356109
162.430662	5333.547352	25.361127
162.525650	5342.320168	25.366144
162.738837	5341.196395	25.371162
162.891404	5372.974129	25.376179
163.057837	5374.183830	25.381197
163.238555	5366.177326	25.386215
163.020612	5368.589730	25.391232
163.391795	5358.132154	25.396250
163.214965	5371.536195	25.401267
163.517342	5376.432782	25.406285
163.458709	5397.789037	25.411303
163.587013	5399.416978	25.416320
163.782183	5402.652276	25.421338
164.318510	5426.840278	25.426355
164.563052	5423.458031	25.431373
164.553555	5434.729916	25.436391
164.740807	5433.394650	25.441408
165.088863	5449.062458	25.446426
165.044891	5453.621256	25.451443
165.268578	5442.328886	25.456461
165.520669	5445.991841	25.461479
165.415117	5462.600584	25.466496
165.635392	5447.875722	25.471514
165.918604	5467.797006	25.476531
166.330620	5466.218832	25.481549
166.988535	5479.852846	25.486567
166.839490	5488.116563	25.491584
167.203653	5482.253240	25.496602
167.264132	5487.235737	25.501619
167.307232	5479.993944	25.506637
167.203860	5479.915114	25.511655
166.993122	5489.246014	25.516672
167.225786	5496.857987	25.521690
167.313380	5516.518858	25.526707
167.447139	5519.445415	25.531725
167.590583	5530.003608	25.536743
167.601296	5554.625681	25.541760
168.077416	5551.201778	25.546778
167.785768	5574.464350	25.551795
168.156750	5581.216177	25.556813
168.484602	5607.113503	25.561831
168.917141	5608.544422	25.566848
169.185520	5615.898490	25.571866
169.107848	5626.268239	25.576883
169.246680	5638.080322	25.581901
169.726402	5633.666592	25.586919
169.794983	5642.944082	25.591936
170.597506	5649.715593	25.596954
170.291455	5653.690290	25.601971
170.443864	5652.898719	25.606989
170.635981	5655.673838	25.612007
170.377629	5653.655726	25.617024
170.774583	5677.783789	25.622042
171.084645	5683.802299	25.627059
171.173612	5686.092081	25.632077
171.147892	5704.736335	25.637095
171.231852	5719.072374	25.642112
171.425504	5723.665800	25.647130
171.533233	5744.687719	25.652147
171.749460	5748.535488	25.657165
171.961654	5761.998870	25.662183
172.220077	5775.521528	25.667200
172.183724	5779.686145	25.672218
172.343674	5793.283462	25.677236
172.581784	5808.905315	25.682253
172.575963	5812.695484	25.687271
172.624186	5827.009206	25.692288
172.983996	5837.321364	25.697306
173.218751	5860.896200	25.702324
173.252417	5865.720239	25.707341
173.779470	5874.690917	25.712359
174.351136	5888.084437	25.717376
174.540667	5890.960841	25.722394
175.045205	5896.131952	25.727412
174.958716	5896.595333	25.732429
175.274622	5890.903700	25.737447
175.199860	5888.576241	25.742464
175.400671	5895.394285	25.747482
175.298372	5895.912275	25.752500
175.501931	5896.974080	25.757517
175.510245	5910.894408	25.762535
175.561067	5918.085505	25.767552
176.158491	5926.557783	25.772570
176.178605	5935.663925	25.777588
176.381736	5952.033653	25.782605
176.560207	5935.981084	25.787623
176.477521	5953.625390	25.792640
176.684961	5948.171502	25.797658
176.935524	5971.702921	25.802676
177.207045	5982.918263	25.807693
177.504113	5976.778433	25.812711
177.553332	6002.651036	25.817728
177.750852	6008.087428	25.822746
177.730191	6013.329307	25.827764
177.807948	6021.456377	25.832781
178.264203	6034.472246	25.837799
178.025025	6033.974917	25.842816
178.387486	6056.859360	25.847834
178.679431	6061.351490	25.852852
178.589446	6071.888975	25.857869
178.871980	6083.949239	25.862887
178.964743	6102.162354	25.867904
179.517514	6114.258075	25.872922
179.699885	6117.795729	25.877940
179.772151	6119.901686	25.882957
180.226178	6124.192841	25.887975
180.340646	6145.211023	25.892992
180.559704	6141.282319	25.898010
180.944191	6143.230860	25.903028
180.699110	6143.704060	25.908045
181.183923	6160.306802	25.913063
181.450280	6174.578293	25.918080
181.425768	6168.447717	25.923098
181.621891	6175.370627	25.928116
181.551704	6196.379391	25.933133
182.184887	6204.878171	25.938151
181.903512	6199.475489	25.943168
182.383807	6209.544977	25.948186
183.058024	6225.665014	25.953204
182.518320	6231.492559	25.958221
182.871176	6228.474140	25.963239
182.919361	6246.674351	25.968256
182.803142	6256.485408	25.973274
183.536012	6264.046143	25.978292
183.455848	6274.358447	25.983309
184.080360	6284.216567	25.988327
183.939643	6291.629476	25.993344
184.264968	6286.669412	25.998362
184.321861	6296.458031	26.003380
184.423750	6320.606177	26.008397
184.735146	6318.271198	26.013415
184.342215	6329.240400	26.018432
184.665559	6340.667921	26.023450
184.826069	6350.566950	26.028468
185.020278	6375.693033	26.033485
185.387600	6378.807778	26.038503
185.587426	6397.973010	26.043520
185.897346	6412.216999	26.048538
186.234321	6417.974554	26.053556
186.306359	6418.838502	26.058573
186.760158	6431.469172	26.063591
186.813730	6445.333617	26.068608
186.838403	6442.755627	26.073626
186.951804	6447.233429	26.078644
186.942244	6446.489211	26.083661
187.378712	6459.250378	26.088679
187.313608	6468.412731	26.093696
187.477392	6471.442382	26.098714
187.760654	6483.698951	26.103732
187.812636	6500.292058	26.108749
188.194539	6513.193082	26.113767
188.266744	6530.057744	26.118784
188.488591	6534.664838	26.123802
188.799030	6533.790257	26.128820
189.212619	6542.982595	26.133837
189.730644	6541.808877	26.138855
190.052278	6541.502682	26.143872
190.123365	6547.315492	26.148890
190.457623	6539.038720	26.153908
190.265911	6549.773793	26.158925
190.428842	6557.287597	26.163943
190.479887	6564.786128	26.168960
190.497599	6561.281444	26.173978
190.708984	6580.470969	26.178996
190.431915	6596.565932	26.184013
190.633197	6606.203941	26.189031
190.874610	6619.095315	26.194048
190.922389	6633.772941	26.199066
191.561478	6651.224845	26.204084
191.558133	6679.626155	26.209101
192.399719	6672.626846	26.214119
192.322146	6694.942616	26.219136
192.701368	6685.468961	26.224154
193.192054	6698.327645	26.229172
192.933052	6718.591861	26.234189
193.130864	6714.371969	26.239207
193.379872	6724.366011	26.244224
193.401351	6741.605579	26.249242
193.408586	6742.822938	26.254260
193.604576	6759.529438	26.259277
194.200236	6784.477621	26.264295
193.870577	6779.538808	26.269312
194.331239	6789.452039	26.274330
194.875457	6801.199997	26.279348
194.905921	6806.102045	26.284365
195.703569	6809.612449	26.289383
195.699166	6828.144213	26.294400
195.866034	6822.370682	26.299418
196.237488	6824.679856	26.304436
196.147839	6837.563405	26.309453
196.836551	6820.653266	26.314471
196.831886	6818.866949	26.319488
196.532444	6831.237938	26.324506
196.834247	6839.009992	26.329524
197.202947	6860.153863	26.334541
197.299354	6854.698423	26.339559
197.280335	6869.559861	26.344576
197.161240	6880.847048	26.349594
197.531380	6891.524440	26.354612
197.550452	6898.071447	26.359629
198.063681	6911.534625	26.364647
198.015036	6912.005924	26.369664
198.082912	6937.030229	26.374682
198.071530	6950.838171	26.379700
198.088862	6960.978766	26.384717
198.446080	6968.291926	26.389735
198.739075	7000.569451	26.394752
199.082145	6999.045123	26.399770
199.389952	7018.761065	26.404788
199.579012	7028.131196	26.409805
199.954561	7039.864825	26.414823
200.100932	7038.065991	26.419840
200.336475	7060.509834	26.424858
200.450889	7072.391635	26.429876
200.588483	7079.428639	26.434893
200.861257	7080.201771	26.439911
200.877501	7100.914602	26.444928
200.922107	7105.106285	26.449946
201.497105	7123.795751	26.454964
201.620003	7133.659774	26.459981
201.435064	7141.762542	26.464999
201.875564	7158.672224	26.470016
201.913787	7168.393594	26.475034
202.798985	7184.635517	26.480052
202.810350	7192.979801	26.485069
203.118204	7194.470187	26.490087
202.991818	7210.740800	26.495104
202.979863	7227.647756	26.500122
203.479667	7233.751123	26.505140
203.540686	7256.739376	26.510157
203.736582	7257.352792	26.515175
204.020132	7279.096608	26.520192
204.179960	7286.234769	26.525210
204.666568	7302.456398	26.530228
204.685283	7311.777022	26.535245
205.013791	7317.036144	26.540263
204.870868	7332.546376	26.545280
205.071948	7345.705764	26.550298
206.068312	7350.029236	26.555316
206.151653	7367.883831	26.560333
206.430268	7365.239868	26.565351
206.737709	7367.683425	26.570368
206.628759	7368.051332	26.575386
207.197280	7378.416467	26.580404
206.642982	7401.456756	26.585421
206.835703	7396.368726	26.590439
207.124978	7416.459237	26.595456
207.140451	7434.515800	26.600474
207.676211	7440.659747	26.605492
207.873587	7463.898968	26.610509
208.219237	7465.505978	26.615527
208.689897	7474.994211	26.620544
208.555815	7486.984563	26.625562
208.875984	7486.404486	26.630580
208.999662	7504.657399	26.635597
209.160085	7510.900758	26.640615
209.442249	7512.130783	26.645632
209.544011	7548.610390	26.650650
209.565409	7536.336399	26.655668
210.211415	7561.906015	26.660685
210.197151	7575.619669	26.665703
210.572255	7572.446859	26.670720
210.630778	7582.329734	26.675738
210.765328	7599.092226	26.680756
210.735937	7602.258167	26.685773
211.193706	7626.189271	26.690791
211.053811	7632.321888	26.695808
211.338020	7662.012304	26.700826
211.601017	7668.701843	26.705844
211.749041	7689.273028	26.710861
211.993607	7694.567492	26.715879
212.190493	7716.645321	26.720896
212.425537	7732.861140	26.725914
212.854090	7747.519064	26.730932
213.180869	7759.248728	26.735949
213.367097	7759.229679	26.740967
213.782559	7779.065738	26.745984
213.993436	7787.915967	26.751002
214.053941	7793.204812	26.756020
214.130750	7790.682533	26.761037
214.574724	7796.963963	26.766055
214.973438	7802.655843	26.771072
214.593481	7816.490329	26.776090
215.110081	7822.059441	26.781108
215.202805	7836.860681	26.786125
215.464373	7839.030726	26.791143
215.566730	7851.986382	26.796160
215.615568	7875.589594	26.801178
215.872716	7887.646001	26.806196
216.106222	7901.420381	26.811213
216.285877	7918.695597	26.816231
216.655002	7923.967079	26.821248
216.855352	7938.892318	26.826266
217.166035	7937.411096	26.831284
217.488373	7963.850410	26.836301
217.462927	7967.092963	26.841319
217.807730	7982.763828	26.846336
217.969291	7993.352951	26.851354
218.242222	8000.307224	26.856372
218.522575	8010.678908	26.861389
218.680917	8016.584098	26.866407
219.256782	8022.899633	26.871424
219.105845	8042.246439	26.876442
219.874920	8036.952953	26.881460
220.004107	8050.380087	26.886477
220.106732	8063.252372	26.891495
220.783062	8066.209775	26.896512
220.476032	8079.495155	26.901530
220.578499	8076.989048	26.906548
221.021006	8093.805659	26.911565
220.978038	8099.690764	26.916583
221.277783	8096.305089	26.921600
221.492490	8121.042977	26.926618
221.932303	8123.140123	26.931636
222.249980	8141.356807	26.936653
222.183719	8151.295428	26.941671
222.454436	8145.040992	26.946688
222.489789	8168.042703	26.951706
222.643661	8174.990052	26.956724
222.831202	8190.528133	26.961741
223.322865	8204.913687	26.966759
223.779165	8206.899400	26.971776
223.549310	8219.270139	26.976794
224.041323	8229.622553	26.981812
224.235581	8252.517637	26.986829
223.925018	8259.991188	26.991847
224.505591	8268.126455	26.996864
224.623794	8280.350399	27.001882
224.789164	8317.372601	27.006900
225.130332	8326.142404	27.011917
225.731366	8341.852974	27.016935
225.783637	8352.610950	27.021952
225.901006	8366.419208	27.026970
226.110297	8381.842005	27.031988
226.441856	8385.093858	27.037005
226.293265	8386.215136	27.042023
226.523546	8405.854306	27.047040
226.508162	8432.737284	27.052058
226.692954	8453.405751	27.057076
226.942684	8473.222162	27.062093
226.989255	8478.273293	27.067111
227.983940	8493.950118	27.072128
228.161161	8490.390937	27.077146
228.342562	8505.041786	27.082164
228.618212	8530.535070	27.087181
228.772781	8525.596389	27.092199
229.368288	8536.950345	27.097216
229.199606	8558.307863	27.102234
229.614481	8563.794099	27.107252
229.622485	8579.467157	27.112269
229.834332	8585.606292	27.117287
230.345140	8581.535568	27.122304
230.555719	8602.665495	27.127322
230.604196	8611.843293	27.132340
230.867207	8619.515538	27.137357
230.921107	8643.428625	27.142375
231.393219	8655.915452	27.147392
231.382438	8669.131617	27.152410
231.423838	8687.119908	27.157428
231.787192	8696.086315	27.162445
231.832181	8718.517682	27.167463
232.085040	8732.649563	27.172480
232.192140	8750.868059	27.177498
232.789296	8767.392644	27.182516
233.090383	8786.233564	27.187533
232.726175	8806.426528	27.192551
233.480277	8812.440208	27.197568
233.746751	8830.811133	27.202586
234.087134	8839.206383	27.207604
234.425683	8850.062863	27.212621
234.186575	8869.736478	27.217639
235.041927	8880.462212	27.222656
235.126070	8897.445561	27.227674
235.263779	8910.730208	27.232692
235.821546	8918.415069	27.237709
235.600606	8937.973888	27.242727
235.934448	8940.666175	27.247744
235.913572	8959.932611	27.252762
236.363446	8977.765134	27.257780
236.776926	8984.436529	27.262797
236.547450	9003.219334	27.267815
236.740087	9025.087775	27.272832
236.727005	9045.615003	27.277850
236.922941	9074.600344	27.282868
237.439908	9092.789731	27.287885
237.531736	9108.332004	27.292903
238.050760	9131.058588	27.297920
238.232359	9155.629485	27.302938
238.314357	9174.589978	27.307956
239.363410	9183.228463	27.312973
239.841658	9187.732288	27.317991
240.600213	9180.673233	27.323008
240.547954	9190.745667	27.328026
240.768494	9200.949243	27.333044
241.096659	9208.751957	27.338061
241.367711	9207.135411	27.343079
241.581815	9199.356983	27.348096
241.473356	9199.582263	27.353114
241.708436	9221.548694	27.358132
242.352473	9219.057204	27.363149
242.014856	9238.460891	27.368167
242.498295	9234.472542	27.373184
242.346109	9242.611892	27.378202
242.055193	9262.345012	27.383220
242.574071	9279.258900	27.388237
242.694031	9298.724495	27.393255
243.044615	9319.426408	27.398272
243.195393	9327.902260	27.403290
243.417222	9350.183814	27.408308
243.890287	9363.196483	27.413325
243.894511	9375.992431	27.418343
244.089134	9402.198534	27.423360
244.553181	9410.705887	27.428378
244.362434	9435.506872	27.433396
244.719924	9445.432612	27.438413
244.917287	9454.100098	27.443431
245.323681	9452.413776	27.448448
245.919295	9477.086540	27.453466
246.395782	9476.635621	27.458484
246.812234	9484.582146	27.463501
247.086360	9501.276180	27.468519
247.573145	9493.516905	27.473536
247.298743	9492.677897	27.478554
247.232856	9509.369347	27.483572
247.591512	9522.637488	27.488589
247.808628	9546.012748	27.493607
247.946640	9550.885955	27.498624
248.038822	9572.276320	27.503642
248.435535	9589.414083	27.508660
248.935819	9598.826193	27.513677
248.625200	9615.240149	27.518695
249.202578	9629.306303	27.523712
249.464077	9654.936867	27.528730
249.259781	9667.741694	27.533748
249.818508	9687.115956	27.538765
250.197766	9708.391845	27.543783
250.370633	9726.767536	27.548800
250.577784	9738.786384	27.553818
250.701958	9759.528846	27.558836
251.227587	9769.124341	27.563853
251.764166	9799.750515	27.568871
252.053782	9807.334618	27.573888
251.899354	9829.379202	27.578906
252.342001	9840.695678	27.583924
252.661686	9857.557405	27.588941
252.881468	9871.802142	27.593959
252.776070	9883.319993	27.598976
253.146500	9909.374032	27.603994
253.031506	9937.660244	27.609012
253.383496	9950.529646	27.614029
253.462303	9975.612828	27.619047
254.130111	9986.271999	27.624064
254.395236	10008.652841	27.629082
254.550976	10031.307136	27.634100
254.880110	10047.886246	27.639117
255.067574	10076.670764	27.644135
255.198586	10088.971167	27.649152
255.507651	10115.236626	27.654170
255.576567	10122.470733	27.659188
256.349450	10153.112681	27.664205
256.548623	10163.522888	27.669223
257.019723	10189.772578	27.674240
257.283826	10195.218255	27.679258
257.160107	10228.114344	27.684276
257.495918	10224.700965	27.689293
257.433590	10263.412812	27.694311
257.851406	10275.710614	27.699328
258.717964	10298.660794	27.704346
258.759211	10325.183803	27.709364
259.169160	10328.365525	27.714381
259.422809	10341.366601	27.719399
260.032023	10360.497733	27.724416
260.122820	10365.826514	27.729434
260.157811	10383.337200	27.734452
260.329094	10381.813535	27.739469
260.504680	10404.056966	27.744487
260.646018	10428.455301	27.749504
261.107571	10444.002043	27.754522
261.399141	10454.390786	27.759540
262.013002	10448.957664	27.764557
261.745029	10470.223921	27.769575
262.238392	10482.531389	27.774592
262.611494	10483.529107	27.779610
262.498391	10513.406637	27.784628
262.933361	10510.254829	27.789645
262.792682	10535.684179	27.794663
263.054304	10545.222373	27.799680
263.604084	10561.966255	27.804698
263.514222	10575.121493	27.809716
263.725364	10594.829555	27.814733
263.633455	10621.926657	27.819751
264.053722	10646.477516	27.824768
264.828985	10663.690619	27.829786
264.611105	10692.267051	27.834804
265.280990	10704.630450	27.839821
265.333873	10735.207988	27.844839
265.891394	10739.279170	27.849856
266.721109	10742.871032	27.854874
267.283689	10750.762399	27.859892
267.752458	10749.346844	27.864909
267.873447	10757.399817	27.869927
268.096089	10769.576008	27.874944
268.500173	10780.404793	27.879962
268.352213	10787.207252	27.884980
268.790387	10782.413786	27.889997
268.935666	10798.939919	27.895015
268.705608	10822.046253	27.900032
269.204149	10826.542451	27.905050
269.227244	10847.414982	27.910068
269.433695	10857.343846	27.915085
269.546197	10887.822742	27.920103
269.582919	10895.381622	27.925120
270.396135	10915.073562	27.930138
270.338224	10950.276461	27.935156
270.481699	10958.698452	27.940173
270.848602	10989.521321	27.945191
271.074972	11017.737744	27.950208
271.745258	11027.941035	27.955226
272.209260	11048.115020	27.960244
272.685929	11041.446293	27.965261
273.027594	11046.748592	27.970279
273.141374	11066.687703	27.975296
273.743740	11063.751427	27.980314
273.882058	11080.309732	27.985332
274.319231	11090.127925	27.990349
274.711013	11093.791051	27.995367
274.328433	11107.568125	28.000384
274.687158	11119.868515	28.005402
274.882529	11137.668518	28.010420
275.481161	11150.283610	28.015437
275.463840	11160.653222	28.020455
275.264698	11178.993104	28.025472
275.826151	11189.272882	28.030490
275.983424	11220.797552	28.035508
276.183930	11223.805469	28.040525
276.940297	11245.503704	28.045543
276.995151	11264.811528	28.050560
277.712164	11272.169324	28.055578
277.668198	11296.126252	28.060596
278.052617	11314.465458	28.065613
278.015319	11326.086476	28.070631
278.429674	11336.376605	28.075648
279.111305	11346.973727	28.080666
278.767319	11370.175405	28.085684
278.850918	11388.659217	28.090701
279.437468	11406.210166	28.095719
279.400075	11429.773839	28.100736
280.047743	11446.238444	28.105754
280.108698	11462.044180	28.110772
280.493186	11466.576841	28.115789
280.638914	11472.874616	28.120807
281.035108	11498.255680	28.125824
281.479348	11500.901703	28.130842
281.530303	11527.714225	28.135860
281.581174	11539.668991	28.140877
282.197384	11555.661480	28.145895
282.655593	11571.267386	28.150912
282.917907	11586.820761	28.155930
282.719921	11608.816704	28.160948
283.005998	11627.267150	28.165965
283.230940	11645.557590	28.170983
283.137294	11668.576286	28.176000
283.512632	11701.332583	28.181018
283.664792	11712.556824	28.186036
284.021523	11754.693749	28.191053
284.578326	11768.239683	28.196071
285.008655	11800.908257	28.201088
284.943455	11821.320827	28.206106
285.387401	11845.156538	28.211124
285.978145	11877.117876	28.216141
286.507916	11876.147499	28.221159
286.999328	11906.195056	28.226176
287.402227	11913.788126	28.231194
287.732520	11929.352598	28.236212
287.891405	11937.726842	28.241229
288.324342	11965.819207	28.246247
288.370779	11970.145015	28.251264
288.709056	11977.759882	28.256282
289.218870	11991.416238	28.261300
289.233960	11999.551243	28.266317
289.698902	12007.855768	28.271335
289.809792	12032.829663	28.276352
290.202638	12044.505800	28.281370
290.386080	12058.087217	28.286388
290.852732	12074.328833	28.291405
291.100837	12078.268186	28.296423
291.173432	12106.419083	28.301440
291.286327	12116.559666	28.306458
291.517008	12139.884435	28.311476
291.531750	12161.940334	28.316493
292.181293	12190.944172	28.321511
292.033155	12222.538864	28.326528
292.925473	12233.842209	28.331546
293.081941	12270.759952	28.336564
293.268376	12286.189508	28.341581
293.641422	12300.771797	28.346599
293.954614	12320.899941	28.351616
294.569515	12348.515205	28.356634
294.561417	12357.982672	28.361652
294.965609	12372.255715	28.366669
295.751167	12390.359313	28.371687
295.740149	12412.861067	28.376704
296.254223	12417.544238	28.381722
296.465191	12435.352534	28.386740
296.491438	12446.675418	28.391757
296.960639	12463.864086	28.396775
297.224747	12482.475167	28.401792
297.971464	12486.418457	28.406810
298.066379	12500.528678	28.411828
297.832189	12510.705107	28.416845
298.220166	12528.829210	28.421863
298.072620	12553.780654	28.426880
298.486102	12580.459049	28.431898
298.869329	12600.999812	28.436916
298.666888	12622.064956	28.441933
298.965903	12651.570669	28.446951
299.599285	12685.973840	28.451968
299.950759	12703.606229	28.456986
300.074861	12725.796009	28.462004
300.285842	12744.866915	28.467021
301.124316	12752.353352	28.472039
301.371525	12775.214557	28.477056
301.759388	12793.206602	28.482074
301.698817	12814.251577	28.487092
302.445684	12829.159907	28.492109
302.820341	12844.204152	28.497127
302.866748	12868.036497	28.502144
303.686105	12869.429066	28.507162
303.747267	12890.996022	28.512180
303.950314	12898.815017	28.517197
304.436200	12907.340305	28.522215
304.579299	12928.816480	28.527232
304.797374	12953.413105	28.532250
305.298739	12956.985966	28.537268
305.793448	12963.948107	28.542285
306.672101	12980.443673	28.547303
306.712313	12994.528741	28.552320
307.173495	13004.459157	28.557338
307.522788	13004.372842	28.562356
307.344222	13011.572924	28.567373
307.571775	13033.931895	28.572391
307.431524	13046.223670	28.577408
307.604407	13064.992404	28.582426
307.922626	13089.027335	28.587444
308.295883	13114.502994	28.592461
308.805956	13141.892760	28.597479
308.832379	13168.579690	28.602496
308.987121	13191.236214	28.607514
309.505883	13211.843486	28.612532
309.721577	13246.755341	28.617549
310.212652	13252.228964	28.622567
310.557771	13274.740511	28.627584
310.982582	13301.845285	28.632602
311.192418	13325.224073	28.637620
311.306840	13344.234503	28.642637
311.803169	13364.398131	28.647655
312.266105	13393.061626	28.652672
312.406986	13408.342223	28.657690
312.760457	13437.023980	28.662708
313.010424	13458.284532	28.667725
313.535734	13471.222512	28.672743
313.884922	13510.542733	28.677760
313.744883	13527.608379	28.682778
314.127098	13541.446415	28.687796
314.394372	13566.467603	28.692813
314.875669	13592.518621	28.697831
314.959497	13602.713814	28.702848
315.349766	13638.160122	28.707866
315.835369	13654.182694	28.712884
315.972741	13686.903732	28.717901
316.617076	13708.959574	28.722919
316.654307	13741.599648	28.727936
316.936819	13753.585326	28.732954
317.740169	13785.716833	28.737972
317.953332	13800.402679	28.742989
318.395370	13816.903866	28.748007
319.053043	13835.829350	28.753024
319.507485	13843.906475	28.758042
319.628315	13858.320883	28.763060
319.784519	13868.891911	28.768077
320.332691	13892.513168	28.773095
319.933105	13910.848446	28.778112
320.426834	13927.018080	28.783130
321.168767	13939.327877	28.788148
320.980947	13969.137491	28.793165
321.736270	13970.093223	28.798183
321.647989	13994.364074	28.803200
321.770956	14010.486639	28.808218
322.532024	14032.085401	28.813236
322.384123	14049.731289	28.818253
322.664097	14066.853803	28.823271
323.317282	14087.821249	28.828288
323.322668	14111.143718	28.833306
323.777471	14124.911880	28.838324
323.981985	14164.834529	28.843341
324.219590	14181.888554	28.848359
324.414850	14216.058847	28.853376
324.683270	14233.788646	28.858394
325.115920	14256.408361	28.863412
325.114100	14294.477532	28.868429
325.429378	14326.532007	28.873447
325.995090	14357.414929	28.878464
326.230666	14389.030446	28.883482
326.265814	14420.365688	28.888500
326.649650	14451.728171	28.893517
327.121725	14481.920819	28.898535
327.801015	14512.641747	28.903552
327.833612	14546.248733	28.908570
328.054735	14569.148307	28.913588
328.577095	14605.288720	28.918605
328.821420	14629.714873	28.923623
329.145842	14665.149130	28.928640
329.886569	14687.800220	28.933658
330.824606	14699.679275	28.938676
331.614147	14713.767431	28.943693
332.187143	14725.037319	28.948711
331.986089	14735.490160	28.953728
332.672928	14762.300087	28.958746
333.183573	14770.919961	28.963764
333.196225	14792.645635	28.968781
333.402622	14786.356002	28.973799
333.552137	14812.984188	28.978816
333.976447	14835.837774	28.983834
334.356353	14839.372922	28.988852
334.395467	14860.079297	28.993869
334.604068	14871.343624	28.998887
335.084614	14898.147065	29.003904
335.447332	14924.219907	29.008922
335.970711	14939.556602	29.013940
336.013381	14964.762241	29.018957
336.193788	14982.706060	29.023975
336.684045	15004.850719	29.028992
336.653950	15028.189843	29.034010
337.043359	15046.042272	29.039028
337.332928	15086.624454	29.044045
337.938986	15106.521411	29.049063
337.880246	15130.837893	29.054080
338.390787	15152.081003	29.059098
339.135354	15176.951292	29.064116
339.283323	15210.397046	29.069133
339.912659	15215.131241	29.074151
340.207697	15230.688970	29.079168
340.608836	15252.632842	29.084186
341.193313	15270.637518	29.089204
341.218017	15297.548858	29.094221
341.780947	15304.981394	29.099239
341.811806	15328.947571	29.104256
342.075293	15344.149717	29.109274
342.404143	15370.205253	29.114292
342.492587	15398.948662	29.119309
342.832525	15416.021649	29.124327
343.384236	15443.810275	29.129344
343.116871	15466.993995	29.134362
343.770020	15485.750350	29.139380
343.881173	15525.860466	29.144397
344.410744	15533.133154	29.149415
344.515884	15559.866066	29.154432
344.661455	15593.125435	29.159450
345.280004	15607.376743	29.164468
345.596414	15645.434008	29.169485
345.731071	15669.711278	29.174503
345.796452	15696.080619	29.179520
346.203181	15730.469544	29.184538
346.669752	15757.448513	29.189556
347.324414	15797.539933	29.194573
347.589166	15837.314787	29.199591
347.957589	15856.702047	29.204608
348.220120	15900.162514	29.209626
349.338276	15914.271203	29.214644
349.508286	15946.554724	29.219661
349.650171	15971.531063	29.224679
350.224850	15999.167076	29.229696
350.295894	16026.847393	29.234714
350.643818	16048.274720	29.239732
350.882420	16075.364584	29.244749
351.713203	16106.225685	29.249767
351.710563	16129.432558	29.254784
352.087986	16158.165540	29.259802
352.597781	16177.898527	29.264820
353.142951	16207.355578	29.269837
353.455804	16227.540610	29.274855
353.963764	16248.623221	29.279872
353.797957	16275.334523	29.284890
354.602242	16295.166896	29.289908
355.511215	16306.478217	29.294925
355.781265	16330.273715	29.299943
356.284918	16338.433750	29.304960
356.503252	16362.590958	29.309978
356.611633	16377.728404	29.314996
357.065117	16393.319234	29.320013
357.173972	16421.774162	29.325031
357.624673	16429.621490	29.330048
357.469273	16474.056071	29.335066
358.241522	16487.743544	29.340084
358.246577	16536.618684	29.345101
358.493284	16554.794367	29.350119
358.582137	16577.351447	29.355136
358.954480	16617.315221	29.360154
359.691399	16640.998936	29.365172
360.012657	16683.241152	29.370189
360.086192	16711.302078	29.375207
360.833093	16734.864475	29.380224
361.503813	16759.487772	29.385242
361.842127	16763.930295	29.390260
362.112853	16794.373435	29.395277
362.597016	16816.143248	29.400295
363.344053	16835.687870	29.405312
363.753998	16853.630277	29.410330
363.753835	16878.669413	29.415348
364.321135	16891.084541	29.420365
364.071772	16929.851918	29.425383
364.456634	16950.230789	29.430400
364.790521	16985.476163	29.435418
365.274457	17007.282520	29.440436
365.365402	17040.233892	29.445453
365.691994	17070.105526	29.450471
366.009414	17098.243241	29.455488
367.088642	17124.142226	29.460506
367.421875	17144.914529	29.465524
367.650145	17162.814940	29.470541
368.092163	17183.063229	29.475559
368.600479	17190.278713	29.480576
368.812276	17212.403246	29.485594
369.263440	17229.327228	29.490612
369.498218	17248.377353	29.495629
369.440722	17271.913354	29.500647
370.287968	17283.878742	29.505664
370.105402	17326.866763	29.510682
370.757849	17345.578072	29.515700
370.815230	17367.815159	29.520717
371.082431	17395.328041	29.525735
371.484729	17415.955225	29.530752
371.654424	17453.541333	29.535770
372.351934	17487.094302	29.540788
372.647120	17519.747877	29.545805
372.743263	17550.574506	29.550823
373.423110	17581.704623	29.555840
373.689383	17612.545667	29.560858
374.455326	17644.839128	29.565876
374.452755	17670.336998	29.570893
375.075779	17702.228697	29.575911
375.527408	17725.814760	29.580928
375.719674	17759.040778	29.585946
376.096442	17785.505172	29.590964
376.180611	17820.439122	29.595981
376.804652	17856.542982	29.600999
377.479505	17885.535376	29.606016
377.831853	17913.750644	29.611034
378.665346	17922.212941	29.616052
379.408679	17942.697433	29.621069
379.704554	17971.615784	29.626087
380.342278	17976.639453	29.631104
380.702268	17988.659495	29.636122
380.953686	17998.635679	29.641140
381.007347	18015.189838	29.646157
381.215857	18043.117096	29.651175
381.735990	18054.186826	29.656192
381.495993	18105.367821	29.661210
382.008705	18123.852577	29.666228
382.499054	18148.785352	29.671245
382.533401	18187.424984	29.676263
382.748674	18217.552059	29.681280
383.653625	18255.936890	29.686298
383.810616	18289.502448	29.691316
384.395560	18310.548105	29.696333
384.506586	18358.402104	29.701351
384.646036	18382.969462	29.706368
385.255831	18412.471730	29.711386
385.721612	18446.725652	29.716404
386.224002	18485.338676	29.721421
386.702505	18506.222550	29.726439
387.096803	18532.968980	29.731456
387.546938	18562.539022	29.736474
387.995223	18584.544127	29.741492
388.481276	18612.982720	29.746509
388.601845	18640.479457	29.751527
388.925232	18672.569401	29.756544
389.084947	18706.802180	29.761562
389.484386	18735.977382	29.766580
389.851419	18771.498495	29.771597
390.312884	18802.580473	29.776615
390.847559	18836.650344	29.781632
390.933630	18876.055442	29.786650
391.727454	18897.979919	29.791668
392.277781	18939.133594	29.796685
391.909783	18970.771425	29.801703
392.838351	18987.971036	29.806720
393.454951	19027.154368	29.811738
393.614406	19052.534426	29.816756
394.212051	19066.516322	29.821773
394.358136	19098.595548	29.826791
394.264433	19124.013035	29.831808
395.035835	19163.182009	29.836826
395.371093	19184.486226	29.841844
395.898172	19219.401562	29.846861
395.888370	19256.657382	29.851879
396.498824	19289.534796	29.856896
396.696037	19322.487221	29.861914
396.770663	19359.456511	29.866932
397.252471	19396.123350	29.871949
397.747205	19438.573921	29.876967
398.542118	19467.834482	29.881984
398.736362	19510.075021	29.887002
399.146581	19529.656705	29.892020
399.968284	19565.721983	29.897037
400.139685	19599.499033	29.902055
400.645174	19632.689368	29.907072
401.093701	19665.392622	29.912090
401.476981	19702.666122	29.917108
401.692549	19727.601183	29.922125
402.161633	19764.264636	29.927143
402.609456	19784.160410	29.932160
403.088412	19821.347339	29.937178
403.455911	19862.434333	29.942196
403.938933	19894.898977	29.947213
404.177839	19931.227384	29.952231
404.799484	19963.153600	29.957248
405.342779	20001.310863	29.962266
405.325432	20027.820631	29.967284
405.971130	20063.358113	29.972301
405.916584	20098.843287	29.977319
406.723438	20122.039509	29.982336
407.109112	20152.993119	29.987354
407.400704	20202.044245	29.992372
407.934799	20229.104407	29.997389
408.254402	20271.456898	30.002407
408.492937	20305.167460	30.007424
408.935660	20344.307083	30.012442
409.066598	20383.083938	30.017460
409.808137	20416.712753	30.022477
410.342225	20469.804634	30.027495
410.385805	20500.851969	30.032512
410.996499	20541.589639	30.037530
411.372440	20580.446077	30.042548
412.489311	20613.757534	30.047565
412.322069	20657.878848	30.052583
412.787238	20699.087257	30.057600
413.679340	20724.491628	30.062618
413.798690	20766.471856	30.067636
414.285180	20785.274518	30.072653
414.550185	20821.177975	30.077671
415.041562	20863.694201	30.082688
415.180163	20900.124925	30.087706
415.563077	20929.388680	30.092724
416.256799	20974.082041	30.097741
416.390925	21010.592580	30.102759
416.949426	21039.813173	30.107776
417.530016	21084.237089	30.112794
417.776145	21125.930698	30.117812
418.539477	21162.024876	30.122829
418.504924	21189.393887	30.127847
419.078012	21236.256991	30.132864
419.751395	21265.037920	30.137882
419.968087	21305.702559	30.142900
420.562688	21342.637143	30.147917
420.526656	21376.393877	30.152935
420.551122	21406.410166	30.157952
421.300240	21441.403616	30.162970
422.054645	21470.466282	30.167988
422.487036	21504.735157	30.173005
422.593307	21532.715169	30.178023
423.899967	21546.507277	30.183040
424.736522	21584.200020	30.188058
425.281950	21583.168208	30.193076
425.912891	21603.368413	30.198093
425.839489	21628.800498	30.203111
426.416074	21647.587586	30.208128
426.903336	21661.927410	30.213146
426.945049	21692.144739	30.218164
427.273314	21704.360358	30.223181
427.623751	21743.941126	30.228199
428.019815	21765.933860	30.233216
428.103003	21794.745923	30.238234
428.109631	21839.505247	30.243252
429.000481	21869.968159	30.248269
429.501472	21898.465034	30.253287
429.554153	21940.629542	30.258304
430.055105	21973.976624	30.263322
430.521824	22006.373944	30.268340
430.979034	22036.106614	30.273357
431.271827	22081.176970	30.278375
431.535962	22118.442498	30.283392
432.312619	22153.279908	30.288410
432.487974	22203.783135	30.293428
432.976036	22241.834816	30.298445
433.316009	22283.725406	30.303463
433.343609	22324.318256	30.308480
433.797181	22364.682774	30.313498
434.406316	22417.654792	30.318516
435.294147	22440.139100	30.323533
436.532184	22476.830541	30.328551
436.747023	22509.330579	30.333568
437.083059	22533.101872	30.338586
437.460244	22567.776273	30.343604
438.365119	22587.441774	30.348621
438.998109	22617.701307	30.353639
439.105875	22648.863339	30.358656
439.576412	22673.921246	30.363674
440.065872	22703.184571	30.368692
440.661230	22722.969442	30.373709
441.083215	22759.197844	30.378727
441.101816	22793.481292	30.383744
441.766080	22812.920537	30.388762
441.787248	22863.580636	30.393780
441.850311	22889.704673	30.398797
442.501843	22934.344005	30.403815
442.930726	22964.917158	30.408832
443.720100	22997.805220	30.413850
443.776351	23032.336768	30.418868
444.218016	23069.243761	30.423885
444.684953	23106.162406	30.428903
445.145849	23145.534148	30.433920
445.571004	23185.438590	30.438938
446.175535	23227.423180	30.443956
446.672681	23254.169502	30.448973
447.081125	23298.653057	30.453991
447.439440	23340.410750	30.459008
447.874689	23374.764933	30.464026
448.225680	23411.823342	30.469044
448.655392	23444.196443	30.474061
449.355016	23479.372639	30.479079
449.530804	23526.062075	30.484096
450.263822	23553.736329	30.489114
449.921057	23602.655101	30.494132
450.425622	23637.329451	30.499149
451.236078	23680.305944	30.504167
451.411860	23713.762492	30.509184
452.141221	23743.799875	30.514202
452.254940	23784.470211	30.519220
452.610755	23820.139443	30.524237
453.198403	23864.444904	30.529255
453.329191	23916.600619	30.534272
453.658442	23956.292563	30.539290
453.903952	24006.836797	30.544308
454.253342	24062.621454	30.549325
455.081171	24113.141828	30.554343
455.370200	24160.793475	30.559360
456.287454	24211.173131	30.564378
456.603681	24252.414921	30.569396
457.873452	24291.073071	30.574413
458.175021	24322.127126	30.579431
458.412326	24362.931278	30.584448
459.513234	24401.296022	30.589466
459.824399	24439.044530	30.594484
460.375545	24461.128543	30.599501
461.093596	24495.116311	30.604519
461.435855	24525.340793	30.609536
461.661443	24551.982865	30.614554
462.008657	24603.590632	30.619572
462.525915	24638.245984	30.624589
463.205998	24678.542101	30.629607
463.099879	24716.657000	30.634624
463.373158	24756.434217	30.639642
463.930658	24802.746765	30.644660
464.094685	24849.408650	30.649677
464.735492	24898.946812	30.654695
464.782733	24952.412714	30.659712
465.492564	24996.492652	30.664730
465.845824	25060.180833	30.669748
465.898125	25109.173912	30.674765
466.645969	25160.947066	30.679783
467.230629	25221.992139	30.684800
468.049846	25269.224481	30.689818
468.633917	25312.335728	30.694836
469.150369	25361.813874	30.699853
469.514744	25399.098310	30.704871
470.112407	25460.728741	30.709888
470.701197	25485.848421	30.714906
471.452471	25539.483095	30.719924
471.750444	25579.220268	30.724941
472.040687	25620.453894	30.729959
472.327983	25668.709313	30.734976
472.968817	25716.663279	30.739994
473.421972	25766.774478	30.745012
473.915705	25805.369384	30.750029
474.696037	25839.901465	30.755047
474.997886	25889.577636	30.760064
475.746843	25933.826967	30.765082
476.170358	25970.118700	30.770100
477.155466	25998.324392	30.775117
478.050106	26028.888761	30.780135
477.743017	26066.450181	30.785152
478.708263	26090.445242	30.790170
479.506212	26119.391925	30.795188
479.877113	26151.614318	30.800205
480.137801	26176.196497	30.805223
480.802334	26207.127444	30.810240
481.251514	26238.554738	30.815258
481.547007	26276.331967	30.820276
481.853612	26301.903456	30.825293
481.959360	26332.022147	30.830311
482.407190	26372.843424	30.835328
482.833387	26399.354106	30.840346
483.192021	26446.823896	30.845364
483.521074	26480.848664	30.850381
483.744005	26510.768408	30.855399
484.010011	26561.304137	30.860416
484.485043	26612.959794	30.865434
484.825600	26649.194185	30.870452
485.388954	26700.643019	30.875469
485.754304	26749.279641	30.880487
485.841489	26807.368981	30.885504
486.496562	26856.661217	30.890522
487.035450	26911.985190	30.895540
487.782557	26956.729544	30.900557
488.989015	27000.861476	30.905575
489.307533	27049.431013	30.910592
489.893293	27100.161260	30.915610
490.557346	27136.671010	30.920628
490.781069	27189.351158	30.925645
491.417299	27222.367417	30.930663
491.725308	27276.491194	30.935680
492.155263	27317.459623	30.940698
492.469921	27367.418665	30.945716
492.877611	27413.870370	30.950733
493.772065	27461.932177	30.955751
493.800909	27523.339529	30.960768
494.484929	27546.544228	30.965786
495.552118	27599.820549	30.970804
495.741795	27650.299578	30.975821
496.267477	27686.410760	30.980839
496.579749	27744.626740	30.985856
497.481624	27781.637786	30.990874
498.602053	27824.041635	30.995892
498.891224	27858.678259	31.000909
499.486036	27894.791013	31.005927
499.835262	27943.484139	31.010944
500.230405	27982.794295	31.015962
500.476180	28024.596250	31.020980
500.944016	28072.544479	31.025997
501.561871	28113.666552	31.031015
502.035308	28164.469041	31.036032
502.601492	28206.457975	31.041050
503.292639	28246.858397	31.046068
503.732177	28294.591112	31.051085
504.169081	28326.040011	31.056103
504.476679	28373.006187	31.061120
505.940533	28399.483261	31.066138
506.479840	28426.177009	31.071156
506.900190	28452.865317	31.076173
507.762080	28482.215458	31.081191
507.833042	28524.359960	31.086208
508.384529	28555.440074	31.091226
508.727705	28590.820008	31.096244
509.144032	28624.730386	31.101261
509.612492	28656.445948	31.106279
509.870900	28707.869358	31.111296
510.400779	28735.937458	31.116314
510.855034	28780.400753	31.121332
511.022978	28845.319829	31.126349
511.325637	28877.596482	31.131367
511.708816	28939.230756	31.136384
512.365446	28984.572694	31.141402
512.861895	29032.010893	31.146420
513.081620	29089.846081	31.151437
513.519004	29142.162250	31.156455
513.985852	29193.584023	31.161472
514.546779	29258.451989	31.166490
514.797699	29308.143252	31.171508
515.679511	29366.288996	31.176525
516.527009	29419.272968	31.181543
516.863808	29464.344314	31.186560
517.307554	29508.953179	31.191578
518.118440	29552.920688	31.196596
518.473278	29607.706459	31.201613
519.019877	29635.871033	31.206631
519.717508	29680.289892	31.211648
520.421757	29716.280985	31.216666
521.114625	29750.362160	31.221684
521.373525	29806.499017	31.226701
522.281798	29829.877755	31.231719
522.312841	29880.307551	31.236736
522.529780	29926.419040	31.241754
523.486033	29963.012402	31.246772
524.176898	30019.627170	31.251789
524.437310	30051.767878	31.256807
525.005985	30097.291368	31.261824
525.457204	30144.184818	31.266842
526.132499	30188.479323	31.271860
526.693093	30243.381197	31.276877
527.386427	30278.394052	31.281895
527.885428	30318.846958	31.286912
528.362608	30367.774840	31.291930
529.033072	30412.540813	31.296948
529.064694	30465.609806	31.301965
529.624180	30497.458726	31.306983
530.107415	30566.121038	31.312000
530.574164	30616.972783	31.317018
531.123779	30661.390315	31.322036
531.774614	30725.217067	31.327053
532.505973	30763.168281	31.332071
532.769060	30826.406685	31.337088
532.655902	30874.175119	31.342106
533.273228	30923.633421	31.347124
533.543030	30982.927357	31.352141
534.334609	31042.702772	31.357159
534.886831	31116.404019	31.362176
535.223227	31177.476529	31.367194
535.745725	31241.768190	31.372212
536.058352	31313.629556	31.377229
537.059765	31371.982954	31.382247
537.664911	31430.982911	31.387264
537.919374	31501.393832	31.392282
539.028716	31552.728441	31.397300
539.806353	31623.930129	31.402317
540.410101	31667.337836	31.407335
541.231909	31722.245119	31.412352
542.452715	31757.230122	31.417370
543.246512	31795.668573	31.422388
543.809680	31835.268691	31.427405
544.306119	31865.950478	31.432423
545.033709	31896.606554	31.437440
545.498891	31947.825258	31.442458
545.995849	31963.516235	31.447476
546.097071	32010.469620	31.452493
546.775523	32043.409101	31.457511
547.792384	32066.482507	31.462528
548.142543	32097.005977	31.467546
548.488225	32134.793853	31.472564
548.812806	32189.860888	31.477581
549.485573	32218.655502	31.482599
549.931639	32259.254179	31.487616
550.322628	32296.750893	31.492634
551.374177	32324.791753	31.497652
552.363141	32361.750709	31.502669
552.874591	32390.010731	31.507687
553.591119	32410.976174	31.512704
553.818153	32451.286658	31.517722
554.491821	32464.853550	31.522740
554.867275	32493.644342	31.527757
555.268683	32520.004356	31.532775
555.558994	32546.051538	31.537792
556.005056	32585.404573	31.542810
556.230941	32625.545251	31.547828
556.316969	32669.341158	31.552845
556.994836	32707.223399	31.557863
557.357674	32754.820045	31.562880
557.527290	32817.935939	31.567898
558.111934	32857.175056	31.572916
558.556333	32921.258596	31.577933
558.902050	32977.075571	31.582951
559.736549	33044.840354	31.587968
559.981567	33111.097121	31.592986
560.421578	33160.117798	31.598004
561.253371	33237.744799	31.603021
561.640546	33296.395880	31.608039
561.919075	33360.435967	31.613056
562.456234	33435.872306	31.618074
562.613487	33489.781502	31.623092
563.321681	33570.554510	31.628109
564.001760	33638.192570	31.633127
564.699445	33707.270084	31.638144
565.136094	33792.548089	31.643162
566.010995	33857.923592	31.648180
566.702142	33926.220438	31.653197
567.116434	33994.913798	31.658215
567.910833	34062.973124	31.663232
568.524380	34133.066611	31.668250
569.073194	34185.290855	31.673268
569.842337	34270.550642	31.678285
570.750891	34329.058581	31.683303
571.451893	34390.760079	31.688320
571.971027	34458.901335	31.693338
572.790228	34505.552727	31.698356
573.529754	34567.355734	31.703373
574.301679	34617.448756	31.708391
574.907562	34660.061853	31.713408
575.468132	34710.960247	31.718426
576.143355	34752.337599	31.723444
576.706046	34816.319936	31.728461
576.981415	34862.832190	31.733479
577.496423	34913.135961	31.738496
577.889343	34970.494532	31.743514
578.684469	35024.599081	31.748532
579.211141	35092.378571	31.753549
579.712247	35153.216466	31.758567
580.456066	35208.245295	31.763584
580.536869	35261.740163	31.768602
581.452036	35321.982840	31.773620
581.912328	35375.670661	31.778637
582.305524	35446.844175	31.783655
582.931754	35504.197268	31.788672
583.376438	35567.643275	31.793690
584.132281	35622.371561	31.798708
584.821592	35687.983392	31.803725
585.746341	35730.391443	31.808743
586.586266	35787.760453	31.813760
586.960126	35844.004598	31.818778
587.783655	35891.084940	31.823796
588.175741	35950.226764	31.828813
588.599581	36003.587974	31.833831
589.437969	36057.398097	31.838848
590.044766	36104.786406	31.843866
590.902535	36153.682790	31.848884
591.260584	36201.472447	31.853901
592.141675	36254.019954	31.858919
592.450337	36301.726552	31.863936
592.852077	36362.553473	31.868954
593.161756	36400.574116	31.873972
593.798799	36443.050558	31.878989
594.360460	36504.700397	31.884007
595.016470	36544.002029	31.889024
595.630293	36585.090810	31.894042
596.515982	36634.861269	31.899060
597.076137	36680.437743	31.904077
597.490699	36730.801146	31.909095
598.225341	36787.404939	31.914112
598.378616	36843.890821	31.919130
598.820954	36904.252022	31.924148
599.102835	36966.678971	31.929165
599.638069	37036.130820	31.934183
599.991315	37096.980888	31.939200
600.354113	37157.895855	31.944218
601.137673	37228.901107	31.949236
601.934402	37309.193314	31.954253
602.429692	37374.644645	31.959271
603.036559	37451.396111	31.964288
603.388740	37525.854532	31.969306
604.084972	37608.907572	31.974324
604.354143	37683.740242	31.979341
605.157927	37771.898881	31.984359
605.831224	37837.476984	31.989376
606.352547	37919.736680	31.994394
607.342590	37991.528127	31.999412
607.800266	38075.178430	32.004429
608.187540	38147.124236	32.009447
609.085746	38222.770032	32.014464
609.543189	38305.184114	32.019482
610.251102	38386.398565	32.024500
610.758403	38463.249742	32.029517
611.355502	38543.672084	32.034535
612.623975	38610.612437	32.039552
613.131685	38679.188160	32.044570
614.092546	38749.570177	32.049588
614.709314	38818.901660	32.054605
614.969316	38894.877169	32.059623
615.736039	38959.395829	32.064640
616.130003	39033.379987	32.069658
616.970642	39102.539643	32.074676
617.253210	39177.720281	32.079693
618.059728	39246.504201	32.084711
619.133326	39325.853384	32.089728
619.508656	39397.730340	32.094746
620.224547	39472.360432	32.099764
621.150044	39541.431899	32.104781
621.140691	39611.586904	32.109799
622.081651	39676.091788	32.114816
622.492350	39762.450248	32.119834
622.954030	39827.006832	32.124852
623.191805	39902.813434	32.129869
623.614917	39982.352383	32.134887
624.837498	40070.089554	32.139904
625.133555	40147.225942	32.144922
625.854111	40235.119862	32.149940
626.745010	40310.491397	32.154957
627.227267	40391.821659	32.159975
628.092278	40459.776495	32.164992
628.534517	40535.122428	32.170010
629.016041	40609.584548	32.175028
629.706619	40683.172539	32.180045
630.199611	40771.100488	32.185063
631.396631	40849.236160	32.190080
632.165693	40917.366460	32.195098
632.511617	40991.189691	32.200116
633.149295	41045.890769	32.205133
633.789045	41109.601490	32.210151
635.341910	41165.025434	32.215168
635.470130	41231.419655	32.220186
636.304121	41295.313438	32.225204
636.820986	41348.223386	32.230221
637.375133	41407.921079	32.235239
638.271181	41462.170088	32.240256
638.972339	41523.627436	32.245274
639.526342	41580.999016	32.250292
640.350987	41636.396910	32.255309
640.905652	41698.365339	32.260327
641.582478	41744.935841	32.265344
642.335038	41814.979034	32.270362
642.756018	41874.823468	32.275380
643.241201	41937.419857	32.280397
643.418992	42006.855182	32.285415
644.114088	42079.769217	32.290432
644.810423	42147.935072	32.295450
645.464767	42223.322124	32.300468
646.302165	42295.079979	32.305485
646.762180	42369.303343	32.310503
647.212184	42429.934030	32.315520
647.680877	42515.459089	32.320538
648.388385	42582.541781	32.325556
649.126120	42662.952446	32.330573
649.447463	42740.843698	32.335591
650.524307	42811.133585	32.340608
651.517445	42880.424171	32.345626
652.369949	42959.225827	32.350644
653.285493	43016.346070	32.355661
653.451879	43100.686373	32.360679
654.655889	43154.917622	32.365696
654.994359	43225.574777	32.370714
655.710271	43293.877345	32.375732
656.199588	43366.413829	32.380749
656.651378	43432.850594	32.385767
657.602941	43502.551376	32.390784
658.381651	43574.481776	32.395802
658.888448	43646.435497	32.400820
660.009342	43704.253102	32.405837
660.699907	43777.117707	32.410855
661.458156	43841.399082	32.415872
661.952430	43901.020001	32.420890
662.128644	43980.235047	32.425908
662.622321	44040.285915	32.430925
663.502830	44111.907843	32.435943
665.001793	44168.259064	32.440960
666.414806	44224.454225	32.445978
666.783313	44288.956561	32.450996
667.836413	44332.436761	32.456013
667.879050	44395.430624	32.461031
668.446475	44445.249824	32.466048
669.109587	44501.115643	32.471066
669.404023	44560.235066	32.476084
670.189376	44626.503861	32.481101
670.564398	44697.930937	32.486119
671.385166	44762.489272	32.491136
672.199667	44821.368455	32.496154
673.011489	44874.084730	32.501172
674.019437	44931.861734	32.506189
674.600603	44988.544629	32.511207
675.168462	45034.866738	32.516224
675.864455	45100.567891	32.521242
676.473142	45151.522005	32.526260
677.351955	45213.846151	32.531277
677.583792	45276.420010	32.536295
678.171291	45337.750918	32.541312
678.270858	45396.005397	32.546330
678.426204	45459.565114	32.551348
679.501339	45533.386298	32.556365
679.729868	45597.461658	32.561383
680.378034	45665.657810	32.566400
681.069020	45750.169220	32.571418
681.349440	45819.055362	32.576436
681.897033	45905.072236	32.581453
682.425014	45990.600151	32.586471
683.555141	46072.883365	32.591488
684.104956	46148.354097	32.596506
684.691436	46235.082828	32.601524
685.550607	46312.214370	32.606541
686.267351	46402.967372	32.611559
687.067373	46476.231619	32.616576
688.035073	46555.970282	32.621594
687.993313	46648.877715	32.626612
689.118610	46728.151998	32.631629
689.509799	46817.672628	32.636647
690.158304	46904.599387	32.641664
691.266822	46985.983845	32.646682
691.653502	47079.469624	32.651700
692.341329	47165.011037	32.656717
693.165420	47256.520835	32.661735
693.612534	47347.155744	32.666752
694.456459	47427.644950	32.671770
695.192171	47523.610818	32.676788
696.164312	47607.726978	32.681805
696.619367	47708.562645	32.686823
697.273311	47797.526346	32.691840
698.746167	47878.576233	32.696858
698.942694	47965.614454	32.701876
699.766599	48055.381712	32.706893
700.542483	48135.755724	32.711911
701.070833	48219.708246	32.716928
701.698957	48306.423719	32.721946
702.331958	48409.409488	32.726964
703.440947	48491.653002	32.731981
704.083269	48573.333236	32.736999
704.925684	48664.830958	32.742016
705.605083	48738.458704	32.747034
706.062193	48833.991046	32.752052
707.014940	48916.906601	32.757069
707.762573	49008.971232	32.762087
708.721908	49082.080090	32.767104
709.907936	49163.881024	32.772122
710.358364	49250.374450	32.777140
711.339087	49322.593199	32.782157
711.989763	49390.230630	32.787175
712.831842	49477.667558	32.792192
713.875756	49539.530005	32.797210
714.537328	49606.019916	32.802228
715.551252	49665.061038	32.807245
716.436744	49736.946581	32.812263
717.165602	49799.178003	32.817280
717.605613	49854.970277	32.822298
718.201049	49929.450341	32.827316
718.999475	50001.231307	32.832333
719.747445	50067.616877	32.837351
720.383046	50138.964259	32.842368
720.993126	50209.978189	32.847386
721.264095	50279.396810	32.852404
722.016047	50359.269283	32.857421
722.532957	50439.730680	32.862439
722.915113	50518.938754	32.867456
724.038994	50583.318069	32.872474
724.640753	50668.080833	32.877492
725.410132	50746.833904	32.882509
725.687110	50834.658225	32.887527
726.121769	50911.547144	32.892544
726.955471	50987.176188	32.897562
727.943166	51057.783104	32.902580
728.855035	51124.663105	32.907597
729.738771	51204.921492	32.912615
730.468526	51281.238563	32.917632
731.211112	51339.878179	32.922650
731.847597	51424.189963	32.927668
732.732139	51498.934466	32.932685
733.365884	51570.619094	32.937703
733.941877	51647.474833	32.942720
734.788689	51720.571313	32.947738
735.309235	51806.142204	32.952756
736.078483	51872.385135	32.957773
736.435336	51951.135771	32.962791
737.261056	52043.100824	32.967808
738.183576	52119.187029	32.972826
738.802889	52213.252969	32.977844
739.684282	52292.031621	32.982861
740.201109	52382.305913	32.987879
740.750963	52479.619264	32.992896
741.408909	52566.010924	32.997914
742.144731	52666.478421	33.002932
742.918805	52754.399463	33.007949
743.946415	52856.139896	33.012967
744.313488	52941.501171	33.017984
745.680161	53021.819556	33.023002
746.340942	53118.498532	33.028020
747.290896	53215.458509	33.033037
748.307100	53299.829091	33.038055
748.914739	53376.471580	33.043072
749.641912	53465.635595	33.048090
750.349516	53544.801952	33.053108
751.067691	53633.058436	33.058125
751.809597	53714.146765	33.063143
752.646438	53799.781285	33.068160
753.760848	53885.711277	33.073178
754.482056	53973.235893	33.078196
755.325211	54061.637828	33.083213
755.714535	54145.629617	33.088231
756.700293	54239.278007	33.093248
757.173487	54320.122807	33.098266
757.753030	54420.682097	33.103284
758.541626	54499.194395	33.108301
758.955803	54597.191553	33.113319
759.671014	54690.962820	33.118336
760.907721	54778.759269	33.123354
761.515613	54873.484333	33.128372
762.272708	54971.293738	33.133389
763.158491	55060.735615	33.138407
763.924860	55162.095383	33.143424
764.528919	55247.616877	33.148442
765.253912	55345.635654	33.153460
766.113024	55435.058377	33.158477
767.268463	55519.737611	33.163495
767.630977	55616.257209	33.168512
768.530348	55711.544487	33.173530
769.583277	55810.206176	33.178548
770.104787	55898.663408	33.183565
770.748043	55998.234424	33.188583
771.334803	56087.781126	33.193600
772.016542	56186.462070	33.198618
772.386359	56286.168381	33.203636
773.287656	56394.892436	33.208653
774.234686	56497.979363	33.213671
774.784277	56601.006419	33.218688
776.006278	56687.600539	33.223706
776.909182	56778.570185	33.228724
777.630848	56862.372984	33.233741
778.547864	56943.009470	33.238759
779.579019	57031.589346	33.243776
780.689453	57106.728405	33.248794
781.338901	57178.437164	33.253812
782.425829	57267.779763	33.258829
783.126398	57334.968739	33.263847
783.201991	57417.528814	33.268864
783.968974	57500.682214	33.273882
785.006198	57588.277757	33.278900
785.665441	57664.043581	33.283917
786.508785	57749.226459	33.288935
787.338351	57843.935190	33.293952
787.928600	57921.419654	33.298970
789.309916	58014.356661	33.303988
789.608947	58099.675615	33.309005
790.227315	58195.981956	33.314023
790.517352	58294.131664	33.319040
791.142365	58396.529818	33.324058
791.863862	58504.201916	33.329076
791.933470	58614.232560	33.334093
793.060985	58727.759882	33.339111
793.637048	58838.289084	33.344128
794.727103	58945.257761	33.349146
795.722018	59071.960249	33.354164
796.174085	59186.607106	33.359181
797.220330	59292.649577	33.364199
797.799015	59418.582801	33.369216
798.758999	59525.468707	33.374234
799.657438	59646.281761	33.379252
800.183236	59762.954647	33.384269
804.186056	59799.862231	33.389287
806.120704	59860.775039	33.394304
807.461087	59916.010226	33.399322
808.208483	59970.964794	33.404340
808.659279	60021.058106	33.409357
809.399263	60075.255788	33.414375
809.895346	60138.632863	33.419392
810.703424	60198.754084	33.424410
811.029185	60258.519456	33.429428
811.775978	60326.089949	33.434445
812.349886	60396.166848	33.439463
812.340656	60480.118677	33.444480
813.078127	60549.347337	33.449498
813.410782	60640.422781	33.454516
813.751546	60745.446008	33.459533
814.232107	60832.844675	33.464551
814.821622	60929.996780	33.469568
815.833229	61045.844288	33.474586
816.713048	61150.394587	33.479604
816.993738	61261.674946	33.484621
818.036574	61364.619190	33.489639
818.732617	61475.225011	33.494656
819.944199	61569.653924	33.499674
820.760191	61683.609777	33.504692
821.108296	61789.376654	33.509709
822.100435	61897.034480	33.514727
822.996287	62001.504307	33.519744
823.881172	62107.240614	33.524762
825.077787	62212.091398	33.529780
826.388510	62316.348594	33.534797
827.355383	62406.511267	33.539815
828.392148	62497.326416	33.544832
829.753289	62573.866357	33.549850
830.534739	62659.453068	33.554868
831.153761	62760.148618	33.559885
831.953117	62840.853423	33.564903
832.315563	62928.773672	33.569920
833.082931	63008.681691	33.574938
833.855618	63083.576631	33.579956
834.178195	63176.561308	33.584973
834.554188	63272.761246	33.589991
835.296970	63371.700970	33.595008
835.979917	63481.637103	33.600026
837.170889	63581.900399	33.605044
837.744715	63674.327286	33.610061
838.855997	63777.449264	33.615079
839.502599	63880.086299	33.620096
840.003399	63981.584938	33.625114
840.687863	64111.492898	33.630132
841.857307	64222.192948	33.635149
843.318318	64321.018005	33.640167
843.865656	64429.458245	33.645184
844.396732	64539.501060	33.650202
845.049687	64654.948007	33.655220
845.592479	64778.764525	33.660237
846.676943	64880.531010	33.665255
847.431233	65007.563031	33.670272
848.272174	65128.904680	33.675290
849.080340	65250.796133	33.680308
849.927542	65390.344484	33.685325
851.053058	65513.954865	33.690343
851.518850	65640.077727	33.695360
852.196260	65761.880077	33.700378
853.162355	65888.509325	33.705396
854.156563	66013.832377	33.710413
855.427275	66132.693590	33.715431
856.353443	66257.612152	33.720448
857.278611	66384.213261	33.725466
858.660046	66496.951170	33.730484
859.375010	66610.223877	33.735501
860.333697	66726.067748	33.740519
860.992333	66837.656722	33.745536
861.950816	66951.586280	33.750554
863.226484	67066.077062	33.755572
864.198116	67187.465854	33.760589
865.144751	67283.216580	33.765607
865.937091	67400.425763	33.770624
866.772122	67509.441157	33.775642
867.887055	67621.274667	33.780660
868.352241	67736.403072	33.785677
869.183475	67848.632602	33.790695
869.585032	67956.647443	33.795712
870.990209	68078.544748	33.800730
871.758634	68190.274397	33.805748
872.567554	68316.659840	33.810765
873.675311	68426.949787	33.815783
874.418407	68544.274647	33.820800
874.918771	68671.263480	33.825818
876.273782	68769.393699	33.830836
876.721883	68893.167977	33.835853
877.867096	69004.681315	33.840871
878.834254	69121.953212	33.845888
879.857983	69233.532173	33.850906
880.665923	69346.108603	33.855924
881.194422	69475.468628	33.860941
882.372677	69590.096725	33.865959
882.912556	69704.464657	33.870976
883.774088	69840.043971	33.875994
884.997391	69940.857105	33.881012
885.420248	70068.518398	33.886029
886.614712	70180.560853	33.891047
887.242500	70308.505720	33.896064
887.930912	70436.295857	33.901082
889.432760	70550.565569	33.906100
889.898147	70662.459650	33.911117
890.804674	70771.694891	33.916135
891.409785	70886.336533	33.921152
892.181021	70999.730815	33.926170
893.786492	71115.333207	33.931188
894.146543	71224.092343	33.936205
895.119597	71342.513645	33.941223
896.186993	71452.914454	33.946240
897.502552	71571.254880	33.951258
898.600540	71670.376958	33.956276
899.013709	71790.537756	33.961293
900.150091	71895.680841	33.966311
900.619593	72012.595853	33.971328
900.913898	72151.059956	33.976346
901.860208	72281.581682	33.981364
902.445618	72405.018275	33.986381
903.465529	72541.992207	33.991399
904.330481	72672.574057	33.996416
905.055408	72818.945279	34.001434
905.844323	72949.193601	34.006452
906.541106	73100.289009	34.011469
907.545368	73233.007569	34.016487
908.459436	73371.793982	34.021504
909.658508	73516.345784	34.026522
911.582893	73640.547411	34.031540
912.981337	73757.709746	34.036557
913.938179	73877.994241	34.041575
914.840726	73998.123981	34.046592
916.241404	74110.664860	34.051610
917.414023	74213.119037	34.056628
917.970032	74341.504407	34.061645
919.181642	74450.366056	34.066663
920.338938	74571.588724	34.071680
921.013879	74679.535002	34.076698
921.668068	74780.831969	34.081716
922.623934	74907.800873	34.086733
923.515007	75024.586190	34.091751
925.165767	75116.884018	34.096768
925.893475	75226.867049	34.101786
927.176566	75330.762765	34.106804
927.673032	75436.414939	34.111821
928.635579	75553.159580	34.116839
929.755439	75666.223073	34.121856
930.328144	75778.188904	34.126874
931.214557	75888.338642	34.131892
932.169545	76003.284371	34.136909
932.828800	76118.431572	34.141927
933.424350	76240.623159	34.146944
934.104529	76367.456480	34.151962
935.098392	76491.082344	34.156980
935.478660	76621.401313	34.161997
936.321408	76765.900810	34.167015
937.143627	76892.049437	34.172032
938.036107	77029.565900	34.177050
938.997706	77177.944591	34.182068
939.697419	77323.565693	34.187085
940.383165	77473.706246	34.192103
941.581814	77608.240591	34.197120
942.476427	77761.618564	34.202138
943.501729	77901.408115	34.207156
944.707809	78042.490540	34.212173
945.423380	78197.906355	34.217191
947.255703	78327.475655	34.222208
947.912569	78472.763464	34.227226
948.836027	78601.226405	34.232244
949.734297	78747.209691	34.237261
950.361254	78873.794105	34.242279
951.500558	79008.713608	34.247296
951.956255	79142.007807	34.252314
953.158068	79271.889621	34.257332
953.927867	79414.368823	34.262349
954.675510	79543.195263	34.267367
955.863036	79675.384355	34.272384
956.321393	79832.207879	34.277402
957.628713	79966.225945	34.282420
958.326004	80113.415402	34.287437
959.148595	80250.716513	34.292455
959.823550	80395.899856	34.297472
960.396399	80555.062664	34.302490
961.664831	80709.632286	34.307508
962.804087	80863.648718	34.312525
963.462740	81013.545365	34.317543
964.883692	81171.458349	34.322560
966.311412	81323.139935	34.327578
967.089544	81471.514121	34.332596
968.416265	81620.468832	34.337613
969.883554	81760.120379	34.342631
970.544161	81901.981711	34.347648
971.763035	82050.432033	34.352666
972.944858	82190.987660	34.357684
973.558495	82324.141482	34.362701
974.642530	82473.262229	34.367719
975.885603	82613.437018	34.372736
976.705012	82761.154754	34.377754
977.814211	82892.198782	34.382772
978.686909	83038.770655	34.387789
979.373653	83185.608409	34.392807
980.568071	83328.630034	34.397824
981.291330	83488.047703	34.402842
982.520915	83638.334980	34.407860
983.786857	83779.829080	34.412877
984.396397	83928.228147	34.417895
985.712651	84073.258807	34.422912
986.577241	84222.901828	34.427930
987.772223	84366.277777	34.432948
988.898751	84515.385709	34.437965
989.725718	84670.340008	34.442983
991.019155	84805.015109	34.448000
992.767233	84932.067134	34.453018
994.439317	85048.743055	34.458036
995.443978	85177.919207	34.463053
996.029585	85305.007983	34.468071
997.129022	85429.120571	34.473088
997.989198	85567.617799	34.478106
998.529838	85696.557450	34.483124
999.403425	85830.922180	34.488141
999.896285	85981.979629	34.493159
1000.995597	86107.285421	34.498176
1001.241705	86263.890622	34.503194
1002.141220	86416.648801	34.508212
1003.054792	86581.105560	34.513229
1003.997490	86738.275403	34.518247
1005.260181	86899.063317	34.523264
1006.040334	87056.547009	34.528282
1007.693102	87183.013291	34.533300
1009.301596	87322.776190	34.538317
1010.685588	87465.760124	34.543335
1011.940966	87599.116102	34.548352
1012.914871	87734.392630	34.553370
1013.901262	87866.295010	34.558388
1015.562062	87984.721317	34.563405
1016.205117	88121.149713	34.568423
1017.382622	88238.670298	34.573440
1018.342782	88371.124065	34.578458
1019.497362	88491.212621	34.583476
1020.116949	88627.989549	34.588493
1020.798405	88751.271423	34.593511
1021.745208	88866.517246	34.598528
1022.211528	89000.733467	34.603546
1023.000360	89131.593514	34.608564
1023.580179	89271.791737	34.613581
1024.084617	89412.167830	34.618599
1024.854202	89556.671232	34.623616
1026.012032	89722.045888	34.628634
1027.176033	89874.560986	34.633652
1028.069706	90026.001744	34.638669
1028.874233	90195.437980	34.643687
1029.788205	90351.858087	34.648704
1030.852178	90513.583129	34.653722
1032.250601	90676.006893	34.658740
1033.361192	90834.878406	34.663757
1034.349454	90993.467478	34.668775
1035.462620	91151.024243	34.673792
1036.056313	91331.148695	34.678810
1037.322509	91498.732733	34.683828
1038.548277	91651.502009	34.688845
1039.532793	91823.027395	34.693863
1040.865279	91978.958234	34.698880
1042.143633	92135.069947	34.703898
1043.297131	92308.336568	34.708916
1044.367400	92461.953221	34.713933
1045.331231	92639.570226	34.718951
1046.330246	92789.839911	34.723968
1047.208590	92965.808861	34.728986
1048.252192	93129.276348	34.734004
1049.382519	93298.958742	34.739021
1050.203825	93461.579209	34.744039
1051.781589	93618.309017	34.749056
1053.159222	93785.137099	34.754074
1054.609091	93927.439634	34.759092
1055.762423	94075.634485	34.764109
1056.335968	94240.124170	34.769127
1057.669733	94396.266464	34.774144
1058.785325	94558.585852	34.779162
1059.548672	94718.591063	34.784180
1060.732205	94877.476835	34.789197
1061.590149	95041.076474	34.794215
1063.438999	95197.853666	34.799232
1064.608519	95333.001014	34.804250
1066.175302	95466.703242	34.809268
1068.133395	95594.701182	34.814285
1068.869471	95725.928320	34.819303
1069.979916	95867.817284	34.824320
1071.144856	96005.171947	34.829338
1071.962509	96145.477891	34.834356
1073.400687	96275.483659	34.839373
1074.078332	96409.408121	34.844391
1075.136266	96540.795058	34.849408
1076.157918	96675.815991	34.854426
1076.717656	96814.731508	34.859444
1077.686252	96956.137447	34.864461
1078.867470	97108.815089	34.869479
1080.449362	97238.270275	34.874496
1081.586069	97374.143167	34.879514
1082.321254	97522.206420	34.884532
1083.583069	97649.437836	34.889549
1084.444150	97793.265630	34.894567
1085.262594	97943.381334	34.899584
1085.985589	98100.490197	34.904602
1086.902556	98243.944114	34.909620
1087.805788	98394.599213	34.914637
1088.749601	98553.155661	34.919655
1089.844142	98703.021162	34.924672
1090.904699	98877.792581	34.929690
1091.671689	99035.583697	34.934708
1092.714163	99179.287999	34.939725
1093.421013	99346.815398	34.944743
1094.269460	99503.627265	34.949760
1095.277334	99657.963519	34.954778
1096.243628	99833.808120	34.959796
1097.349022	99992.473379	34.964813
1098.379540	100173.102362	34.969831
1099.493518	100343.943313	34.974848
1100.398377	100511.002327	34.979866
1101.072714	100697.246655	34.984884
1102.313870	100869.640191	34.989901
1103.109708	101080.603888	34.994919
1104.237070	101247.567473	34.999936
1105.171228	101437.743906	35.004954
1106.106567	101631.587530	35.009972
1107.545479	101831.484410	35.014989
1108.800642	102033.217851	35.020007
1110.474530	102221.029594	35.025024
1111.803925	102398.148520	35.030042
1112.802962	102584.327294	35.035060
1114.007185	102762.830819	35.040077
1114.886520	102966.299157	35.045095
1116.081473	103159.515955	35.050112
1117.220368	103346.658442	35.055130
1117.736509	103542.428512	35.060148
1118.886064	103748.055344	35.065165
1120.209982	103945.448415	35.070183
1121.617287	104149.693232	35.075200
1122.513063	104350.440459	35.080218
1123.310187	104550.179757	35.085236
1124.657450	104752.970143	35.090253
1125.769011	104967.047509	35.095271
1126.468677	105170.721099	35.100288
1127.919217	105377.665904	35.105306
1128.900468	105590.807412	35.110324
1130.264190	105801.594791	35.115341
1132.230991	105993.931831	35.120359
1133.922789	106182.896245	35.125376
1135.237998	106367.086283	35.130394
1136.216211	106564.391664	35.135412
1138.092989	106746.426687	35.140429
1139.312522	106917.920133	35.145447
1140.313165	107109.171624	35.150464
1141.547280	107290.734352	35.155482
1142.276764	107481.970163	35.160500
1143.499762	107661.890678	35.165517
1144.409530	107843.333635	35.170535
1145.307902	108033.316744	35.175552
1146.841759	108232.999505	35.180570
1147.372151	108418.980493	35.185588
1148.712667	108604.841038	35.190605
1149.676392	108807.168599	35.195623
1151.213064	109002.815953	35.200640
1152.409026	109180.534431	35.205658
1153.560843	109384.279117	35.210676
1154.801098	109573.861677	35.215693
1155.809480	109767.499477	35.220711
1157.166377	109955.747980	35.225728
1158.403239	110145.791108	35.230746
1158.994663	110344.607067	35.235764
1160.147964	110531.436579	35.240781
1160.980061	110736.549162	35.245799
1161.991421	110936.883199	35.250816
1163.520308	111142.997982	35.255834
1164.380102	111341.282616	35.260852
1165.444273	111552.291312	35.265869
1166.472877	111742.177375	35.270887
1167.865507	111942.645513	35.275904
1168.773035	112130.527446	35.280922
1169.728072	112325.547650	35.285940
1171.325017	112513.634527	35.290957
1172.811000	112702.741893	35.295975
1174.048482	112891.727080	35.300992
1175.378038	113066.268791	35.306010
1176.766449	113256.422266	35.311028
1177.910059	113426.968457	35.316045
1178.956577	113617.662523	35.321063
1180.550667	113810.142056	35.326080
1181.688939	113991.866549	35.331098
1182.665393	114172.846253	35.336116
1184.372779	114343.709928	35.341133
1186.150959	114520.048671	35.346151
1187.500790	114688.883340	35.351168
1189.093899	114854.447981	35.356186
1189.907418	115032.977059	35.361204
1190.668425	115202.495277	35.366221
1191.785947	115380.824092	35.371239
1193.240761	115565.597630	35.376256
1194.492189	115725.535373	35.381274
1196.121825	115889.098203	35.386292
1198.126914	116034.583104	35.391309
1199.680784	116190.659668	35.396327
1201.266873	116344.603179	35.401344
1202.351751	116487.531659	35.406362
1203.250571	116645.163766	35.411380
1204.747310	116809.792896	35.416397
1205.382933	116954.382016	35.421415
1206.233624	117125.797380	35.426432
1206.791661	117290.939758	35.431450
1207.871359	117472.164149	35.436468
1210.370197	117626.469994	35.441485
1212.090264	117768.564623	35.446503
1212.888299	117922.647354	35.451520
1214.364088	118076.187682	35.456538
1215.090045	118233.502414	35.461556
1216.018123	118392.786485	35.466573
1216.894596	118561.393185	35.471591
1217.479157	118744.785759	35.476608
1218.696526	118919.749572	35.481626
1219.311161	119115.557248	35.486644
1220.318108	119303.077474	35.491661
1221.261156	119507.804621	35.496679
1221.879393	119709.077076	35.501696
1222.855662	119915.765661	35.506714
1223.978741	120139.208676	35.511732
1225.235838	120352.367019	35.516749
1226.342460	120575.195173	35.521767
1227.201900	120811.726416	35.526784
1228.594354	121025.437434	35.531802
1229.312504	121262.933470	35.536820
1231.072163	121491.869615	35.541837
1231.969071	121724.600282	35.546855
1232.887155	121959.496259	35.551872
1234.619181	122186.262694	35.556890
1235.812773	122416.719209	35.561908
1237.236905	122652.563216	35.566925
1238.757021	122868.496766	35.571943
1240.098142	123107.386954	35.576960
1241.480016	123323.524145	35.581978
1242.574466	123569.720599	35.586996
1243.823345	123787.720805	35.592013
1245.306705	124021.436670	35.597031
1246.195727	124253.187158	35.602048
1247.647392	124485.644537	35.607066
1249.126344	124695.945658	35.612084
1250.383843	124912.038843	35.617101
1251.647306	125119.514387	35.622119
1253.136498	125335.293335	35.627136
1254.390531	125533.432607	35.632154
1255.336480	125747.428832	35.637172
1256.631182	125953.751543	35.642189
1257.785675	126159.199032	35.647207
1258.895799	126372.297879	35.652224
1260.542520	126588.186302	35.657242
1261.555798	126808.503314	35.662260
1262.842032	127011.779997	35.667277
1264.248630	127226.394571	35.672295
1265.296328	127454.112507	35.677312
1266.238913	127681.177787	35.682330
1267.347104	127908.293313	35.687348
1268.867760	128129.498893	35.692365
1270.076082	128366.145477	35.697383
1270.948240	128595.700779	35.702400
1272.810394	128826.500534	35.707418
1274.963181	129033.905664	35.712436
1276.485992	129243.863028	35.717453
1278.334009	129461.854890	35.722471
1279.799836	129672.458357	35.727488
1281.269018	129872.947423	35.732506
1282.268076	130093.619624	35.737524
1282.968020	130305.723343	35.742541
1284.280467	130523.393079	35.747559
1284.898378	130752.080955	35.752576
1286.634679	130953.483284	35.757594
1288.028577	131185.201953	35.762612
1289.175551	131418.066107	35.767629
1289.997496	131631.235939	35.772647
1291.016898	131868.104943	35.777664
1292.197358	132115.888937	35.782682
1293.279366	132358.278203	35.787700
1294.156440	132608.284039	35.792717
1295.572514	132847.186160	35.797735
1296.862460	133108.752159	35.802752
1298.190645	133354.594279	35.807770
1299.548005	133605.986056	35.812788
1300.651809	133855.710392	35.817805
1302.239308	134119.922799	35.822823
1303.342235	134386.651801	35.827840
1304.557005	134631.787091	35.832858
1306.618867	134875.604702	35.837876
1307.847360	135125.178616	35.842893
1309.505911	135369.624613	35.847911
1310.416141	135633.175525	35.852928
1312.179735	135861.151682	35.857946
1313.506801	136111.794363	35.862964
1314.734248	136366.816798	35.867981
1315.965355	136622.728075	35.872999
1316.848152	136875.681603	35.878016
1318.238888	137129.085313	35.883034
1319.554712	137391.872923	35.888052
1320.743995	137652.249254	35.893069
1321.587631	137912.355278	35.898087
1323.031311	138190.558151	35.903104
1324.697988	138449.834490	35.908122
1325.770863	138713.509543	35.913140
1327.245175	138972.162474	35.918157
1328.775007	139230.643340	35.923175
1330.249950	139499.139385	35.928192
1331.607998	139749.474417	35.933210
1333.156614	140001.149086	35.938228
1334.848532	140245.067189	35.943245
1337.014723	140480.133922	35.948263
1338.622700	140709.195793	35.953280
1340.219622	140924.300330	35.958298
1341.454916	141147.885762	35.963316
1342.605442	141367.606566	35.968333
1344.038870	141570.987729	35.973351
1345.143018	141807.406223	35.978368
1345.925790	142025.074566	35.983386
1347.194086	142244.071287	35.988404
1348.035775	142479.777043	35.993421
1349.473072	142705.063558	35.998439
1350.463070	142957.461050	36.003456
1351.884800	143182.778580	36.008474
1353.533103	143423.771636	36.013492
1354.736273	143672.372677	36.018509
1356.111053	143911.271335	36.023527
1357.559873	144150.197372	36.028544
1359.257108	144385.761334	36.033562
1360.355768	144635.172705	36.038580
1361.752639	144883.775483	36.043597
1363.042733	145126.855873	36.048615
1364.169940	145382.494362	36.053632
1365.497000	145640.625193	36.058650
1366.870381	145904.672598	36.063668
1368.015829	146151.499684	36.068685
1370.007037	146392.392545	36.073703
1371.396030	146644.889505	36.078720
1373.005745	146897.973047	36.083738
1374.594186	147147.041612	36.088756
1375.887643	147411.366906	36.093773
1377.282776	147651.517254	36.098791
1378.559372	147906.273706	36.103808
1380.377779	148146.103458	36.108826
1381.503962	148387.292468	36.113844
1382.849523	148654.877534	36.118861
1384.814527	148882.157214	36.123879
1386.148539	149143.850220	36.128896
1387.217524	149388.378176	36.133914
1388.983840	149632.728691	36.138932
1390.303631	149882.316907	36.143949
1392.650558	150104.099656	36.148967
1394.723456	150327.590679	36.153984
1397.106692	150525.043295	36.159002
1399.519844	150719.283077	36.164020
1400.978596	150910.739547	36.169037
1402.694250	151098.197112	36.174055
1403.922624	151296.555565	36.179072
1404.885133	151496.468506	36.184090
1406.100744	151680.156025	36.189108
1406.888715	151883.892401	36.194125
1408.303056	152096.430115	36.199143
1409.677822	152308.100382	36.204160
1410.505513	152513.419036	36.209178
1412.580555	152704.642843	36.214196
1413.765157	152908.838970	36.219213
1415.017814	153106.911087	36.224231
1416.040483	153336.124324	36.229248
1417.245427	153535.069089	36.234266
1418.117382	153750.458421	36.239284
1419.375519	153988.934200	36.244301
1420.691993	154227.668149	36.249319
1421.845135	154456.752222	36.254336
1422.899511	154696.686814	36.259354
1424.344322	154925.991660	36.264372
1425.088396	155183.714113	36.269389
1426.734971	155423.669129	36.274407
1428.398312	155669.800467	36.279424
1429.771792	155910.602894	36.284442
1431.745586	156151.662436	36.289460
1433.040380	156391.542131	36.294477
1434.235091	156616.483790	36.299495
1435.546597	156837.982281	36.304512
1436.598690	157072.299348	36.309530
1437.914741	157310.709529	36.314548
1438.914173	157554.349388	36.319565
1440.235415	157798.977598	36.324583
1441.290081	158053.216620	36.329600
1442.334783	158320.639573	36.334618
1443.397542	158578.940055	36.339636
1444.481917	158869.461278	36.344653
1445.519516	159143.107013	36.349671
1447.074340	159442.295095	36.354688
1448.553023	159739.404737	36.359706
1449.688449	160020.728056	36.364724
1451.056705	160328.935544	36.369741
1452.190482	160631.741638	36.374759
1453.557082	160938.241240	36.379776
1454.716406	161251.273127	36.384794
1456.392425	161569.423332	36.389812
1457.478271	161897.544317	36.394829
1459.594034	162211.947250	36.399847
1461.515879	162517.554381	36.404864
1463.489293	162825.045583	36.409882
1465.471661	163127.843194	36.414900
1466.950662	163433.517670	36.419917
1468.967566	163726.138446	36.424935
1471.789807	163997.731126	36.429952
1473.678501	164261.613917	36.434970
1475.167847	164539.292752	36.439988
1476.544979	164826.799724	36.445005
1477.916624	165092.283181	36.450023
1479.547552	165370.019998	36.455040
1480.773315	165642.471370	36.460058
1482.409520	165903.830331	36.465076
1483.701655	166190.281899	36.470093
1485.053536	166474.010115	36.475111
1486.670784	166752.519269	36.480128
1487.482531	167042.050494	36.485146
1489.429449	167321.307946	36.490164
1490.302891	167629.992592	36.495181
1491.969399	167918.689924	36.500199
1493.148913	168211.746009	36.505216
1494.391170	168514.246874	36.510234
1495.962288	168812.533240	36.515252
1497.464079	169107.533895	36.520269
1498.981633	169407.431889	36.525287
1500.414244	169715.974659	36.530304
1502.233037	170023.998669	36.535322
1504.177212	170307.069174	36.540340
1505.317289	170613.128592	36.545357
1506.479118	170913.958307	36.550375
1507.970049	171229.277818	36.555392
1508.978761	171545.580390	36.560410
1510.629881	171842.984890	36.565428
1511.953112	172159.112571	36.570445
1513.718778	172481.184110	36.575463
1515.386716	172803.235980	36.580480
1516.486406	173121.069577	36.585498
1517.897195	173434.754753	36.590516
1519.467840	173765.001828	36.595533
1520.766884	174079.027020	36.600551
1522.696032	174399.625033	36.605568
1524.006049	174739.325716	36.610586
1525.357542	175056.851195	36.615604
1527.063620	175393.546547	36.620621
1528.384111	175707.401069	36.625639
1530.033883	176048.082513	36.630656
1531.010893	176373.953149	36.635674
1532.858702	176687.053872	36.640692
1534.435244	177004.605402	36.645709
1535.742693	177308.763470	36.650727
1537.639724	177618.638303	36.655744
1539.106354	177941.480935	36.660762
1541.111265	178234.792012	36.665780
1542.941223	178555.852294	36.670797
1545.167986	178841.388220	36.675815
1547.080529	179142.728324	36.680832
1548.564309	179437.160771	36.685850
1550.348046	179731.215193	36.690868
1551.050477	180030.831954	36.695885
1552.814435	180332.685964	36.700903
1554.418143	180631.027191	36.705920
1555.778300	180939.411963	36.710938
1557.059699	181239.993162	36.715956
1558.325936	181562.320604	36.720973
1559.518703	181880.600616	36.725991
1561.462394	182205.142389	36.731008
1562.793423	182537.276339	36.736026
1564.560496	182873.642885	36.741044
1565.630513	183208.603965	36.746061
1567.277724	183537.277341	36.751079
1568.742621	183876.035719	36.756096
1570.253298	184204.837318	36.761114
1571.609686	184540.063777	36.766132
1573.122870	184886.448949	36.771149
1574.419336	185238.177992	36.776167
1576.456461	185588.250598	36.781184
1577.973073	185942.219709	36.786202
1579.682256	186286.550187	36.791220
1581.722074	186618.591397	36.796237
1584.003934	186947.268713	36.801255
1586.123689	187265.489828	36.806272
1587.791861	187584.866549	36.811290
1590.104676	187906.042267	36.816308
1591.862926	188226.677017	36.821325
1593.233024	188539.241061	36.826343
1595.520038	188845.066595	36.831360
1596.701200	189164.063111	36.836378
1598.538310	189470.499656	36.841396
1600.164130	189784.944802	36.846413
1601.239060	190096.982164	36.851431
1602.985074	190406.383748	36.856448
1604.600088	190721.444982	36.861466
1606.057742	191036.648211	36.866484
1607.688684	191348.447614	36.871501
1608.680738	191674.826410	36.876519
1610.804325	192003.215578	36.881536
1611.511597	192326.839548	36.886554
1613.062563	192659.478350	36.891572
1614.084840	193002.743358	36.896589
1615.715641	193336.159655	36.901607
1617.463835	193683.040418	36.906624
1619.615733	194017.846608	36.911642
1621.694008	194348.096520	36.916660
1623.418792	194671.233940	36.921677
1624.876460	195001.666303	36.926695
1627.234258	195320.080997	36.931712
1629.124721	195638.231960	36.936730
1631.132742	195949.204746	36.941748
1632.658501	196256.412210	36.946765
1634.238557	196571.534188	36.951783
1635.805205	196881.353112	36.956800
1637.225049	197210.482657	36.961818
1638.555147	197522.629036	36.966836
1640.200240	197835.499115	36.971853
1641.358581	198155.535665	36.976871
1643.230846	198458.810973	36.981888
1644.669629	198764.787575	36.986906
1646.134713	199060.642411	36.991924
1647.680712	199371.999811	36.996941
1648.988545	199688.730510	37.001959
1650.819185	199990.584860	37.006976
1651.401045	200322.877451	37.011994
1653.217539	200643.921132	37.017012
1655.378439	200948.721240	37.022029
1657.634936	201269.123511	37.027047
1659.420415	201587.789698	37.032064
1660.860147	201906.044843	37.037082
1662.393703	202244.740180	37.042100
1663.789888	202568.922127	37.047117
1665.401695	202897.932653	37.052135
1666.983055	203223.331112	37.057152
1668.876845	203564.245626	37.062170
1669.871069	203901.946122	37.067188
1671.322250	204256.992719	37.072205
1672.706216	204616.953214	37.077223
1674.330292	204954.427100	37.082240
1675.474856	205336.790363	37.087258
1677.400434	205713.223448	37.092276
1679.047638	206081.273496	37.097293
1679.826520	206464.490217	37.102311
1681.602888	206846.197568	37.107328
1682.592906	207250.651369	37.112346
1683.969699	207660.096768	37.117364
1686.069690	208060.815407	37.122381
1687.471369	208483.352160	37.127399
1689.178596	208895.263232	37.132416
1690.697684	209312.654934	37.137434
1691.799248	209740.288969	37.142452
1693.786871	210173.847976	37.147469
1695.320096	210617.871528	37.152487
1696.951820	211052.814643	37.157504
1698.463392	211488.567173	37.162522
1700.251962	211938.853563	37.167540
1702.137462	212375.894598	37.172557
1704.180280	212817.737111	37.177575
1706.335808	213253.925051	37.182592
1708.491765	213692.248391	37.187610
1710.186912	214135.653455	37.192628
1712.544359	214544.486909	37.197645
1715.166857	214959.322811	37.202663
1717.713582	215354.998074	37.207680
1719.377467	215770.656790	37.212698
1720.845234	216180.584570	37.217716
1722.525625	216585.932671	37.222733
1723.857423	217012.344271	37.227751
1725.530238	217411.652388	37.232768
1726.751299	217844.943412	37.237786
1728.273721	218257.410667	37.242804
1730.552875	218668.890661	37.247821
1731.990449	219158.942026	37.252839
1734.122790	219562.398659	37.257856
1736.272430	219967.504903	37.262874
1739.023197	220372.843272	37.267892
1741.605321	220756.088797	37.272909
1743.278465	221121.859518	37.277927
1745.517316	221493.684272	37.282944
1747.779094	221866.903442	37.287962
1749.760514	222232.474401	37.292980
1751.579044	222584.840567	37.297997
1753.247800	222952.853221	37.303015
1754.898281	223294.886539	37.308032
1756.672347	223662.147446	37.313050
1758.347580	224008.369687	37.318068
1760.463383	224324.116627	37.323085
1761.990739	224654.973128	37.328103
1763.417603	224982.799233	37.333120
1764.676064	225313.295717	37.338138
1766.044425	225674.813530	37.343156
1767.760371	226001.095878	37.348173
1768.845736	226370.612806	37.353191
1770.203023	226726.064908	37.358208
1771.772170	227096.773792	37.363226
1773.425888	227462.211883	37.368244
1774.931797	227832.298351	37.373261
1775.957846	228226.367138	37.378279
1777.626727	228617.587313	37.383296
1779.485004	229012.866721	37.388314
1781.080866	229408.978177	37.393332
1782.679801	229813.396277	37.398349
1784.279950	230229.220276	37.403367
1786.858636	230614.910363	37.408384
1789.087750	231020.319696	37.413402
1790.523862	231429.290691	37.418420
1792.831867	231820.972633	37.423437
1794.827611	232232.240778	37.428455
1796.594403	232627.062614	37.433472
1798.621590	233032.053594	37.438490
1800.226328	233426.116858	37.443508
1802.984211	233817.830889	37.448525
1804.347741	234220.953540	37.453543
1805.988380	234624.539281	37.458560
1807.887078	235036.440332	37.463578
1809.017151	235451.314719	37.468596
1810.992235	235852.206166	37.473613
1812.689325	236271.764040	37.478631
1815.023574	236675.849237	37.483648
1816.611681	237097.992650	37.488666
1819.237969	237498.881420	37.493684
1821.535244	237892.484394	37.498701
1822.857263	238298.264905	37.503719
1825.096892	238697.264264	37.508736
1826.836381	239106.025479	37.513754
1828.333635	239507.054588	37.518772
1830.625170	239909.959619	37.523789
1832.371445	240318.442636	37.528807
1834.002129	240733.372340	37.533824
1835.657265	241146.698411	37.538842
1837.130311	241550.326289	37.543860
1839.279388	241965.121510	37.548877
1841.180363	242386.613997	37.553895
1842.688231	242802.812412	37.558912
1844.656588	243220.103723	37.563930
1846.182635	243646.309088	37.568948
1847.872074	244063.368517	37.573965
1849.945239	244486.207605	37.578983
1851.713810	244920.630616	37.584000
1853.107706	245353.033330	37.589018
1855.128706	245786.602893	37.594036
1857.405028	246216.853792	37.599053
1858.928277	246655.054117	37.604071
1860.431560	247087.237845	37.609088
1862.882177	247526.606583	37.614106
1864.081516	247976.750803	37.619124
1866.465852	248412.295742	37.624141
1868.164575	248857.582499	37.629159
1870.155165	249281.736881	37.634176
1872.395338	249716.545012	37.639194
1874.252937	250142.525884	37.644212
1876.058228	250584.113304	37.649229
1877.914897	251023.863584	37.654247
1880.038655	251438.370080	37.659264
1881.788922	251856.977872	37.664282
1883.130306	252270.954126	37.669300
1885.043352	252676.529101	37.674317
1886.562346	253102.034912	37.679335
1888.449486	253527.073530	37.684352
1890.380594	253938.666797	37.689370
1892.640929	254356.759755	37.694388
1894.868640	254761.724834	37.699405
1896.524598	255187.132816	37.704423
1899.004499	255593.707645	37.709440
1901.034804	256018.418825	37.714458
1902.301851	256433.527132	37.719476
1904.509032	256851.528174	37.724493
1906.287131	257279.583886	37.729511
1907.851676	257704.880688	37.734528
1909.396575	258156.625628	37.739546
1911.492087	258596.212812	37.744564
1913.053304	259047.421628	37.749581
1914.194863	259513.408470	37.754599
1915.526410	259978.322266	37.759616
1917.240614	260446.475034	37.764634
1919.226361	260935.896083	37.769652
1920.809882	261404.857803	37.774669
1922.321391	261910.437427	37.779687
1923.774798	262419.989394	37.784704
1926.079431	262916.241228	37.789722
1927.699066	263429.804292	37.794740
1929.424685	263950.919661	37.799757
1931.207398	264463.184920	37.804775
1933.026619	265013.497735	37.809792
1934.871431	265543.559538	37.814810
1936.238726	266093.235003	37.819828
1937.696972	266638.500128	37.824845
1940.033816	267195.253740	37.829863
1942.210453	267743.345418	37.834880
1944.611106	268284.134068	37.839898
1947.342941	268846.459717	37.844916
1949.658196	269378.649498	37.849933
1951.983755	269910.963858	37.854951
1954.347696	270433.160748	37.859968
1956.629969	270971.196365	37.864986
1958.529223	271509.446995	37.870004
1960.736517	272040.685341	37.875021
1962.991708	272562.541242	37.880039
1965.027235	273085.423324	37.885056
1967.605129	273598.968051	37.890074
1969.444958	274129.501405	37.895092
1971.121967	274635.166209	37.900109
1973.204180	275156.537834	37.905127
1975.343731	275679.600838	37.910144
1977.024663	276198.166267	37.915162
1978.593284	276723.912609	37.920180
1980.515987	277245.128291	37.925197
1982.569687	277767.667367	37.930215
1984.363527	278311.662215	37.935232
1986.268944	278832.064064	37.940250
1987.883024	279373.139267	37.945268
1990.743590	279908.316482	37.950285
1992.841208	280446.971653	37.955303
1994.573903	280977.328557	37.960320
1996.784081	281495.335820	37.965338
1998.904626	282019.681450	37.970356
2001.689422	282537.895319	37.975373
2003.964024	283056.522365	37.980391
2006.100214	283563.232090	37.985408
2008.997453	284052.642899	37.990426
2010.726025	284552.939747	37.995444
2012.724794	285038.787801	38.000461
2014.678860	285508.385052	38.005479
2016.152864	286001.200705	38.010496
2017.780727	286472.373071	38.015514
2019.675422	286950.002353	38.020532
2021.454666	287440.984589	38.025549
2023.090303	287925.257749	38.030567
2024.135758	288440.209299	38.035584
2026.464790	288932.898691	38.040602
2028.055678	289447.959308	38.045620
2029.933886	289969.345817	38.050637
2031.728022	290489.956777	38.055655
2033.681258	291014.501698	38.060672
2036.381830	291531.173668	38.065690
2038.753882	292049.015515	38.070708
2040.876890	292575.938750	38.075725
2043.492955	293090.611590	38.080743
2045.388271	293617.694973	38.085760
2047.425381	294141.348982	38.090778
2048.973305	294672.523650	38.095796
2050.888427	295196.980433	38.100813
2053.213362	295742.498915	38.105831
2054.816501	296283.257669	38.110848
2056.642382	296824.307035	38.115866
2058.419589	297385.401305	38.120884
2060.223048	297954.031625	38.125901
2062.217222	298509.089909	38.130919
2063.791968	299094.210030	38.135936
2066.350503	299643.708051	38.140954
2069.005064	300230.725366	38.145972
2070.703319	300795.903069	38.150989
2073.410924	301370.713816	38.156007
2075.053635	301948.592821	38.161024
2077.760607	302510.545657	38.166042
2079.699051	303087.962329	38.171060
2081.567893	303668.256786	38.176077
2083.831038	304238.983802	38.181095
2085.582745	304823.353761	38.186112
2088.025885	305397.827679	38.191130
2089.731884	305986.438736	38.196148
2092.011114	306581.376096	38.201165
2094.412096	307152.620041	38.206183
2097.022578	307730.047417	38.211200
2100.544643	308284.133547	38.216218
2103.148690	308833.542855	38.221236
2105.654337	309382.025136	38.226253
2108.088162	309926.757102	38.231271
2109.891903	310480.147832	38.236288
2111.844427	311014.362341	38.241306
2113.551798	311568.548618	38.246324
2115.419056	312121.891826	38.251341
2117.380330	312669.501752	38.256359
2118.931494	313244.779042	38.261376
2121.168550	313787.434120	38.266394
2123.787861	314340.027055	38.271412
2125.973265	314891.671962	38.276429
2128.143167	315456.697549	38.281447
2130.177738	316019.252595	38.286464
2132.364333	316569.894136	38.291482
2135.038733	317119.333321	38.296500
2137.519562	317659.074909	38.301517
2140.123331	318183.861237	38.306535
2141.834344	318735.224647	38.311552
2143.752367	319274.792843	38.316570
2145.875815	319833.087206	38.321588
2147.753831	320360.414500	38.326605
2149.703280	320921.293109	38.331623
2151.252122	321482.131715	38.336640
2153.138448	322025.212155	38.341658
2154.989977	322578.069203	38.346676
2156.726006	323118.727798	38.351693
2159.192916	323653.090921	38.356711
2160.816279	324204.879815	38.361728
2162.922615	324760.798555	38.366746
2164.694979	325325.730129	38.371764
2166.728217	325890.664081	38.376781
2168.206163	326467.084451	38.381799
2169.601053	327063.062477	38.386816
2171.293255	327666.068745	38.391834
2173.233980	328277.482034	38.396852
2174.895970	328900.486686	38.401869
2177.095450	329524.385788	38.406887
2178.815018	330155.212247	38.411904
2180.977655	330794.056901	38.416922
2183.304102	331444.265957	38.421940
2185.987833	332088.721722	38.426957
2188.395372	332739.663895	38.431975
2190.943201	333395.398507	38.436992
2192.884558	334043.330734	38.442010
2195.205757	334705.154301	38.447028
2197.075698	335355.545001	38.452045
2199.971804	336003.397054	38.457063
2202.281632	336666.340478	38.462080
2204.711690	337332.377860	38.467098
2207.188054	337993.550728	38.472116
2209.589117	338644.675717	38.477133
2211.664463	339297.978536	38.482151
2213.868524	339964.069960	38.487168
2216.134844	340620.243073	38.492186
2219.021873	341274.629546	38.497204
2221.197249	341936.359030	38.502221
2223.931533	342581.844412	38.507239
2225.976967	343243.856914	38.512256
2228.384975	343901.510953	38.517274
2231.132649	344548.389171	38.522292
2233.452152	345189.948908	38.527309
2236.111508	345851.366773	38.532327
2238.251274	346494.689682	38.537344
2240.758235	347132.790943	38.542362
2243.315030	347775.671712	38.547380
2245.280160	348414.555521	38.552397
2247.511495	349056.634668	38.557415
2249.374808	349693.969259	38.562432
2251.757811	350342.653897	38.567450
2253.815518	350982.374154	38.572468
2256.388758	351636.870447	38.577485
2259.067846	352271.977455	38.582503
2261.202267	352922.187869	38.587520
2263.659337	353557.997998	38.592538
2265.772370	354205.375962	38.597556
2268.219656	354844.594264	38.602573
2270.499139	355486.139784	38.607591
2272.825910	356118.812232	38.612608
2275.186334	356754.311385	38.617626
2278.083434	357388.976153	38.622644
2280.133728	358020.371446	38.627661
2282.659628	358652.743925	38.632679
2284.351405	359285.422321	38.637696
2286.977998	359928.084684	38.642714
2289.686688	360538.375014	38.647732
2292.163598	361166.859877	38.652749
2294.528222	361772.367875	38.657767
2296.890129	362402.881838	38.662784
2298.697359	363027.617167	38.667802
2300.858987	363657.027868	38.672820
2302.630800	364291.997931	38.677837
2304.902644	364910.080948	38.682855
2306.695856	365531.201309	38.687872
2308.755650	366135.398045	38.692890
2310.955339	366759.627370	38.697908
2312.714951	367392.873662	38.702925
2314.904246	368016.804821	38.707943
2316.930760	368646.916385	38.712960
2319.053239	369292.017653	38.717978
2321.221954	369934.614217	38.722996
2323.259731	370598.755625	38.728013
2325.308015	371247.512606	38.733031
2327.488783	371923.679383	38.738048
2329.093509	372605.838424	38.743066
2331.729543	373290.502154	38.748084
2333.561336	373977.441631	38.753101
2336.223154	374668.389645	38.758119
2338.313076	375374.280343	38.763136
2341.009966	376084.824072	38.768154
2343.248884	376785.285067	38.773172
2345.665873	377505.736377	38.778189
2348.033632	378203.459063	38.783207
2350.480461	378927.121438	38.788224
2353.274994	379631.413428	38.793242
2356.041898	380344.139275	38.798260
2357.985634	381070.678921	38.803277
2360.587751	381791.033568	38.808295
2363.721713	382504.438440	38.813312
2366.279673	383202.862217	38.818330
2369.493163	383905.396786	38.823348
2371.776513	384611.391549	38.828365
2374.497303	385304.418885	38.833383
2376.883384	386015.538030	38.838400
2378.736855	386715.929403	38.843418
2381.848141	387410.519719	38.848436
2384.178677	388126.519128	38.853453
2387.090064	388807.219263	38.858471
2389.446207	389512.991789	38.863488
2391.734363	390216.427401	38.868506
2393.881837	390908.361857	38.873524
2395.991704	391621.706434	38.878541
2398.099822	392336.302077	38.883559
2400.088339	393048.796932	38.888576
2402.067209	393776.763434	38.893594
2404.987715	394497.789080	38.898612
2406.776531	395235.940800	38.903629
2408.807532	395967.723299	38.908647
2411.411705	396712.394405	38.913664
2413.696628	397455.654968	38.918682
2416.475878	398198.409375	38.923700
2418.724591	398947.466871	38.928717
2421.257992	399685.991832	38.933735
2423.888460	400429.245911	38.938752
2426.395917	401160.692540	38.943770
2429.036987	401919.465083	38.948788
2431.337093	402668.467629	38.953805
2433.727315	403423.516577	38.958823
2436.497377	404168.702059	38.963840
2438.841372	404924.529017	38.968858
2441.255346	405667.554403	38.973876
2443.364178	406426.799735	38.978893
2445.618754	407172.775223	38.983911
2448.473422	407931.146111	38.988928
2450.625578	408693.614845	38.993946
2453.514953	409443.197749	38.998964
2457.121495	410167.993053	39.003981
2459.712366	410902.816105	39.008999
2462.253715	411641.553375	39.014016
2464.717488	412373.291885	39.019034
2467.491237	413090.419855	39.024052
2470.144615	413784.499218	39.029069
2472.924792	414448.652265	39.034087
2475.615379	415134.356729	39.039104
2478.167723	415807.427993	39.044122
2480.418559	416476.403507	39.049140
2482.100156	417172.959098	39.054157
2484.059581	417865.803036	39.059175
2486.199702	418554.698374	39.064192
2488.326265	419269.685476	39.069210
2490.516727	419977.627466	39.074228
2493.028848	420700.436133	39.079245
2496.184277	421399.467648	39.084263
2498.892099	422105.263539	39.089280
2500.976883	422832.942648	39.094298
2503.737828	423544.157789	39.099316
2506.241879	424265.420867	39.104333
2508.605177	424990.736790	39.109351
2511.545396	425726.821797	39.114368
2513.724159	426464.630737	39.119386
2515.897811	427188.899785	39.124404
2518.478468	427938.495212	39.129421
2520.963498	428675.578169	39.134439
2522.840206	429431.267927	39.139456
2524.907375	430197.381239	39.144474
2527.960180	430958.497509	39.149492
2530.318380	431738.939889	39.154509
2532.673449	432511.257802	39.159527
2535.423518	433286.825499	39.164544
2537.995512	434072.519831	39.169562
2540.593007	434842.695471	39.174580
2542.676616	435637.375939	39.179597
2545.501397	436440.256848	39.184615
2547.820620	437233.830616	39.189632
2550.256304	438048.865152	39.194650
2552.704899	438846.105899	39.199668
2555.235588	439664.659232	39.204685
2557.793703	440471.084451	39.209703
2560.623566	441288.263751	39.214720
2563.207026	442110.867643	39.219738
2566.004034	442924.551352	39.224756
2568.499634	443729.704509	39.229773
2571.212904	444552.043801	39.234791
2574.141562	445370.218638	39.239808
2576.539968	446205.043183	39.244826
2579.130015	447031.406482	39.249844
2581.775955	447862.281319	39.254861
2584.284376	448682.676184	39.259879
2586.790098	449515.077954	39.264896
2588.947773	450355.192517	39.269914
2591.774391	451193.746830	39.274932
2593.438698	452046.013864	39.279949
2595.880027	452899.584197	39.284967
2598.525030	453761.682721	39.289984
2600.792006	454641.860621	39.295002
2602.801499	455511.778816	39.300020
2605.706803	456393.748280	39.305037
2608.368262	457271.826862	39.310055
2610.940991	458155.898783	39.315072
2613.029390	459036.827224	39.320090
2616.380244	459922.412096	39.325108
2619.528412	460808.800299	39.330125
2622.075844	461696.512373	39.335143
2625.848003	462553.148026	39.340160
2628.626421	463417.240214	39.345178
2631.374248	464293.632233	39.350196
2634.362818	465155.642178	39.355213
2636.929836	466007.323413	39.360231
2640.329663	466833.914967	39.365248
2643.032743	467659.222161	39.370266
2646.042681	468451.546630	39.375284
2648.846907	469245.135789	39.380301
2651.585518	470036.934467	39.385319
2654.161569	470812.811421	39.390336
2656.143015	471619.574943	39.395354
2658.278877	472417.033047	39.400372
2660.758892	473213.693255	39.405389
2663.133378	474034.383665	39.410407
2665.814929	474862.918267	39.415424
2667.980274	475683.924514	39.420442
2670.886477	476497.195264	39.425460
2673.732813	477321.804700	39.430477
2675.611505	478168.204700	39.435495
2678.405894	478999.010429	39.440512
2681.181147	479853.719519	39.445530
2683.720554	480701.862630	39.450548
2686.305948	481555.664703	39.455565
2689.189577	482421.546367	39.460583
2691.919353	483283.675443	39.465600
2694.050367	484155.758189	39.470618
2697.013089	485036.243634	39.475636
2699.423082	485910.012015	39.480653
2701.623625	486811.941149	39.485671
2704.563531	487693.913838	39.490688
2707.060331	488588.534924	39.495706
2709.916674	489489.006849	39.500724
2712.667861	490394.143600	39.505741
2715.331875	491317.971755	39.510759
2718.211495	492227.483345	39.515776
2720.490132	493157.131033	39.520794
2723.421420	494084.046889	39.525812
2726.427533	495017.005586	39.530829
2728.549644	495951.724463	39.535847
2731.865015	496865.559175	39.540864
2734.924759	497810.968529	39.545882
2737.943243	498741.449631	39.550900
2740.931870	499661.088871	39.555917
2743.911716	500591.221211	39.560935
2747.061460	501517.591356	39.565952
2749.697972	502448.382519	39.570970
2752.183622	503375.968820	39.575988
2755.110424	504303.631488	39.581005
2757.735010	505240.116375	39.586023
2760.745613	506157.423094	39.591040
2763.690194	507090.823872	39.596058
2766.796172	508024.950778	39.601076
2769.831369	508942.549223	39.606093
2772.686003	509860.477965	39.611111
2775.499563	510779.520236	39.616128
2778.071513	511700.515331	39.621146
2780.988998	512612.075012	39.626164
2784.293647	513539.092110	39.631181
2786.851110	514458.820076	39.636199
2790.637218	515358.334255	39.641216
2793.357726	516273.342691	39.646234
2795.885862	517177.848155	39.651252
2798.528427	518076.689049	39.656269
2801.225169	518992.649598	39.661287
2804.453452	519890.028397	39.666304
2807.023288	520800.360381	39.671322
2809.632252	521710.933967	39.676340
2811.907365	522629.819725	39.681357
2814.612247	523554.119351	39.686375
2817.311229	524469.952432	39.691392
2820.326271	525388.094999	39.696410
2823.119616	526300.930373	39.701428
2826.750532	527196.702111	39.706445
2829.264252	528070.751434	39.711463
2832.248889	528941.247631	39.716480
2834.651263	529818.434882	39.721498
2837.488403	530701.338080	39.726516
2840.606257	531562.897718	39.731533
2843.028141	532445.915785	39.736551
2845.796239	533317.699088	39.741568
2848.713466	534195.948790	39.746586
2851.244411	535085.533402	39.751604
2853.774623	535977.277819	39.756621
2856.384177	536875.747619	39.761639
2859.135746	537779.320742	39.766656
2862.086197	538691.609427	39.771674
2864.742665	539614.202737	39.776692
2867.439339	540538.993541	39.781709
2869.900010	541481.169294	39.786727
2872.226154	542425.668755	39.791744
2874.965636	543370.589806	39.796762
2877.811619	544340.427114	39.801780
2880.274952	545316.798569	39.806797
2882.834924	546308.876582	39.811815
2885.223040	547305.538447	39.816832
2887.645432	548312.732423	39.821850
2890.848549	549312.181861	39.826868
2894.563977	550314.238938	39.831885
2897.885639	551317.946696	39.836903
2901.352684	552313.815286	39.841920
2904.059300	553320.493120	39.846938
2906.997410	554330.324713	39.851956
2909.985829	555330.322631	39.856973
2913.600701	556344.514786	39.861991
2916.854431	557343.916685	39.867008
2919.818278	558353.441182	39.872026
2922.932108	559354.323210	39.877044
2926.644351	560336.593480	39.882061
2929.862826	561335.750883	39.887079
2932.907588	562332.701256	39.892096
2935.991905	563311.487872	39.897114
2938.606333	564314.184747	39.902132
2941.653298	565302.269966	39.907149
2943.924797	566318.126697	39.912167
2946.661623	567323.031406	39.917184
2949.129093	568338.947806	39.922202
2951.924085	569364.519230	39.927220
2955.285133	570374.604264	39.932237
2958.178898	571403.609997	39.937255
2961.051854	572422.899277	39.942272
2963.701426	573463.773901	39.947290
2966.370404	574503.706402	39.952308
2969.150041	575551.011198	39.957325
2971.910440	576609.721526	39.962343
2974.236845	577673.129861	39.967360
2977.207833	578738.698537	39.972378
2979.929036	579816.857568	39.977396
2982.889380	580893.729406	39.982413
2985.528450	581980.741123	39.987431
2988.707483	583065.059880	39.992448
2991.771795	584156.772810	39.997466
2994.713448	585259.789712	40.002484
2997.888953	586344.769824	40.007501
3001.342184	587438.830572	40.012519
3004.419253	588532.753981	40.017536
3007.825285	589625.119998	40.022554
3011.343448	590696.770085	40.027572
3014.831404	591765.021522	40.032589
3017.486127	592855.612390	40.037607
3020.574098	593919.326634	40.042624
3024.353852	594971.758989	40.047642
3027.330303	596004.693549	40.052660
3030.053984	597021.049498	40.057677
3032.834777	598043.418014	40.062695
3035.729487	599059.217624	40.067712
3038.496437	600097.233399	40.072730
3040.924884	601116.485332	40.077748
3044.283294	602149.261962	40.082765
3046.905657	603211.804760	40.087783
3049.933934	604259.314798	40.092800
3052.915440	605304.634331	40.097818
3055.549413	606363.328485	40.102836
3058.658657	607438.209742	40.107853
3061.504285	608504.926163	40.112871
3064.312107	609589.760519	40.117888
3067.073799	610667.843913	40.122906
3069.869889	611789.789625	40.127924
3072.872485	612888.879599	40.132941
3075.494122	614009.580406	40.137959
3078.361703	615141.779575	40.142976
3081.527059	616274.463634	40.147994
3084.288048	617427.047799	40.153012
3087.660039	618562.961966	40.158029
3091.060970	619723.147927	40.163047
3094.073650	620885.124038	40.168064
3097.158625	622039.417291	40.173082
3100.360481	623202.213471	40.178100
3104.086131	624366.996333	40.183117
3107.512132	625539.346748	40.188135
3110.572294	626709.331439	40.193152
3114.161619	627843.835149	40.198170
3117.372914	629009.846082	40.203188
3120.973528	630164.527879	40.208205
3124.102532	631334.890957	40.213223
3126.869603	632498.842931	40.218240
3130.303177	633667.448237	40.223258
3133.210375	634847.990399	40.228276
3136.174474	636013.515738	40.233293
3139.152376	637207.903875	40.238311
3141.980039	638386.560248	40.243328
3145.467896	639578.394737	40.248346
3148.276166	640777.237950	40.253364
3151.519967	641962.999125	40.258381
3154.490981	643166.923071	40.263399
3157.172984	644365.516014	40.268416
3160.797100	645582.860444	40.273434
3163.813506	646803.250183	40.278452
3166.980342	648014.344144	40.283469
3170.088395	649233.775984	40.288487
3173.223172	650456.344485	40.293504
3177.137037	651667.222120	40.298522
3180.412714	652889.418953	40.303540
3183.871576	654089.911181	40.308557
3187.397244	655298.267083	40.313575
3190.750686	656523.189892	40.318592
3194.016468	657722.424433	40.323610
3196.684956	658939.886858	40.328628
3199.651405	660158.044296	40.333645
3202.623498	661388.544454	40.338663
3205.651125	662606.135465	40.343680
3208.660782	663830.444638	40.348698
3212.026185	665066.035445	40.353716
3215.469175	666286.675257	40.358733
3218.704666	667521.572508	40.363751
3221.873908	668758.559285	40.368768
3225.360636	669971.307271	40.373786
3228.174672	671215.990714	40.378804
3231.594087	672448.972297	40.383821
3234.403324	673662.004224	40.388839
3237.313487	674877.000231	40.393856
3240.518348	676058.136331	40.398874
3243.626011	677264.685992	40.403892
3247.147704	678455.405683	40.408909
3250.068709	679654.916262	40.413927
3253.147825	680860.405482	40.418944
3256.902631	682047.393468	40.423962
3259.768357	683277.886105	40.428980
3262.691855	684484.464181	40.433997
3265.873046	685715.916727	40.439015
3268.757657	686953.854769	40.444032
3272.290373	688172.453193	40.449050
3275.833858	689410.293246	40.454068
3278.804094	690650.439891	40.459085
3282.315673	691901.639554	40.464103
3285.196883	693151.974335	40.469120
3288.623329	694413.503180	40.474138
3292.117770	695680.843355	40.479156
3295.539954	696945.534210	40.484173
3299.848659	698186.491721	40.489191
3303.468261	699440.130228	40.494208
3307.508128	700685.984728	40.499226
3310.798772	701936.097682	40.504244
3314.388023	703166.306678	40.509261
3318.232621	704404.970849	40.514279
3321.870781	705647.505036	40.519296
3325.142010	706882.737866	40.524314
3328.319620	708121.325504	40.529332
3331.288013	709370.366969	40.534349
3335.018537	710599.788424	40.539367
3338.113768	711856.466826	40.544384
3341.085866	713108.375998	40.549402
3343.839487	714376.123094	40.554420
3346.430229	715652.812459	40.559437
3349.722724	716927.658339	40.564455
3352.724248	718217.497119	40.569472
3355.651307	719527.627618	40.574490
3358.895621	720830.823164	40.579508
3361.866149	722157.891764	40.584525
3365.742318	723474.067185	40.589543
3368.568436	724803.998142	40.594560
3371.760269	726143.983597	40.599578
3374.913294	727504.857567	40.604596
3378.262554	728859.840060	40.609613
3381.509996	730218.368536	40.614631
3384.489888	731600.372775	40.619648
3387.573048	732961.284258	40.624666
3391.130163	734347.167988	40.629684
3394.622615	735737.858999	40.634701
3398.349645	737127.381552	40.639719
3401.571523	738524.148334	40.644736
3404.827356	739918.049488	40.649754
3408.159599	741335.816536	40.654772
3410.919832	742750.513988	40.659789
3414.260044	744174.675301	40.664807
3417.385297	745605.319535	40.669824
3420.954204	747030.896713	40.674842
3424.659617	748476.152201	40.679860
3428.123575	749909.500239	40.684877
3431.735086	751325.955334	40.689895
3434.800066	752784.210330	40.694912
3438.253025	754219.371505	40.699930
3441.792594	755661.685440	40.704948
3445.361341	757111.008926	40.709965
3449.068424	758549.303575	40.714983
3452.483388	760005.878364	40.720000
3455.969122	761442.873550	40.725018
3459.137076	762870.282048	40.730023
3462.709010	764254.473293	40.735028
3466.113385	765579.274220	40.740032
3469.439522	766844.355775	40.745037
3473.435648	768035.380343	40.750042
3476.391578	769163.358918	40.755047
3479.632300	770199.474068	40.760052
3482.720048	771182.410997	40.765056
3485.462872	772099.316478	40.770061
3488.303408	772936.104542	40.775066
3490.787662	773703.810457	40.780071
3492.972875	774392.006633	40.785076
3495.784482	775029.515237	40.790080
3497.277263	775601.457066	40.795085
3499.665346	776112.257128	40.800090
3501.387958	776587.538997	40.805095
3503.043334	776978.132348	40.810100
3504.605329	777329.193520	40.815104
3505.943328	777640.602136	40.820109
3507.353216	777895.628814	40.825114
3508.696216	778112.070336	40.830119
3509.335168	778294.268123	40.835124
3510.910766	778438.213205	40.840128
3511.882882	778555.383499	40.845133
3513.069562	778615.623948	40.850138
3513.520954	778653.691081	40.855143
3514.313380	778664.387486	40.860148
3515.299043	778642.963858	40.865152
3516.081483	778605.185098	40.870157
3516.603787	778536.148018	40.875162
3517.279453	778453.648919	40.880167
3517.887004	778355.607614	40.885172
3518.311799	778211.822702	40.890176
3518.428766	778074.779576	40.895181
3519.102625	777906.288808	40.900186
3519.483637	777723.469961	40.905191
3519.879078	777532.817772	40.910196
3520.317072	777331.521224	40.915200
3520.551491	777109.824272	40.920205
3520.784381	776864.344236	40.925210
3521.464102	776637.390510	40.930215
3521.082262	776379.836298	40.935220
3521.502114	776113.377224	40.940224
3521.734804	775847.973274	40.945229
3521.764497	775566.837815	40.950234
3521.902851	775282.226961	40.955239
3521.945890	775000.772122	40.960244
3521.966666	774709.658819	40.965248
3522.052056	774407.098785	40.970253
3521.875995	774105.603627	40.975258
3522.077267	773797.434552	40.980263
3522.206665	773492.465652	40.985268
3521.863480	773161.015469	40.990272
3521.905767	772864.062947	40.995277
3521.718417	772543.789072	41.000282
3521.632863	772227.178807	41.005287
3521.678736	771906.198318	41.010292
3521.883465	771584.635723	41.015296
3521.823545	771274.532222	41.020301
3521.588965	770947.201244	41.025306
3521.903785	770622.277694	41.030311
3521.543092	770296.810973	41.035316
3521.569796	769965.402411	41.040320
3521.434962	769637.011516	41.045325
3521.567517	769307.034282	41.050330
3521.413879	768976.793984	41.055335
3521.110889	768650.358384	41.060340
3521.007078	768308.893138	41.065344
3520.660766	767995.249801	41.070349
3520.764459	767663.331448	41.075354
3520.572408	767336.819854	41.080359
3520.480601	767024.473701	41.085364
3520.769841	766684.150602	41.090368
3520.531841	766371.801279	41.095373
3520.390478	766049.070104	41.100378
3520.488218	765724.214828	41.105383
3520.055277	765402.539249	41.110388
3520.316841	765066.633681	41.115392
3520.219370	764754.390800	41.120397
3519.905766	764428.068026	41.125402
3519.927111	764111.636717	41.130407
3519.567160	763794.860564	41.135412
3519.698886	763471.036234	41.140416
3519.303711	763157.395255	41.145421
3519.511927	762840.337034	41.150426
3519.393361	762528.744916	41.155431
3518.893128	762220.310408	41.160436
3519.101311	761908.194720	41.165440
3518.775057	761590.284354	41.170445
3518.653625	761289.888391	41.175450
3518.615601	760980.882868	41.180455
3518.336605	760679.452697	41.185460
3518.149570	760368.522734	41.190464
3517.902470	760091.189320	41.195469
3517.816764	759789.839797	41.200474
3517.831860	759506.372811	41.205479
3517.590856	759216.868256	41.210484
3517.425924	758909.970354	41.215488
3517.532830	758627.343600	41.220493
3517.329619	758333.752624	41.225498
3517.055838	758048.897193	41.230503
3517.205068	757773.585092	41.235508
3517.446937	757482.848945	41.240512
3517.104030	757201.280027	41.245517
3516.713910	756912.304691	41.250522
3516.877717	756636.110009	41.255527
3516.942385	756352.566721	41.260532
3516.699343	756067.138553	41.265536
3516.269796	755791.258205	41.270541
3516.399588	755513.103294	41.275546
3516.372077	755250.811919	41.280551
3515.715955	754972.125421	41.285556
3516.047994	754706.892477	41.290560
3515.824332	754443.322185	41.295565
3515.450548	754172.015538	41.300570
3516.011145	753908.544177	41.305575
3515.489321	753651.464516	41.310580
3515.395206	753381.466378	41.315584
3515.428308	753130.746596	41.320589
3515.565225	752879.310108	41.325594
3515.180269	752614.172829	41.330599
3514.837522	752363.045689	41.335604
3515.077152	752102.775811	41.340608
3514.989666	751851.441666	41.345613
3514.629608	751601.428599	41.350618
3514.833688	751357.834301	41.355623
3514.406938	751118.189466	41.360628
3514.645337	750862.718836	41.365632
3514.304409	750616.671976	41.370637
3514.146250	750369.994283	41.375642
3514.196318	750140.219340	41.380647
3513.948313	749897.888869	41.385652
3514.031476	749665.920635	41.390656
3513.820153	749433.253028	41.395661
3513.461735	749191.857483	41.400666
3513.511932	748965.802783	41.405671
3513.300103	748738.796583	41.410676
3513.169604	748521.652846	41.415680
3513.154991	748291.043283	41.420685
3512.909197	748064.615996	41.425690
3512.512364	747846.855045	41.430695
3512.474519	747626.656608	41.435700
3512.816103	747410.886445	41.440704
3512.767201	747206.788775	41.445709
3512.779157	746980.287407	41.450714
3512.377877	746766.006004	41.455719
3512.211369	746559.390237	41.460724
3512.252449	746350.411667	41.465728
3511.873151	746144.907489	41.470733
3512.049898	745932.287112	41.475738
3512.033338	745738.229264	41.480743
3512.102879	745538.319466	41.485748
3511.975810	745321.531042	41.490752
3511.486643	745134.407499	41.495757
3511.522183	744938.393312	41.500762
3511.602502	744743.355559	41.505767
3511.482525	744540.287707	41.510772
3511.387769	744336.518291	41.515776
3511.273651	744137.295300	41.520781
3511.065521	743957.216657	41.525786
3511.023094	743758.318309	41.530791
3510.825611	743580.701421	41.535796
3510.817772	743396.918015	41.540800
3510.533972	743212.434230	41.545805
3510.484690	743029.143553	41.550810
3510.817562	742837.329781	41.555815
3510.511394	742666.187982	41.560820
3510.490287	742499.248117	41.565824
3510.364588	742318.228275	41.570829
3510.164022	742143.002637	41.575834
3510.462995	741962.102269	41.580839
3510.311364	741794.278900	41.585844
3510.498984	741613.784605	41.590848
3510.481318	741443.261018	41.595853
3510.093688	741265.079398	41.600858
3510.350368	741086.935674	41.605863
3510.113643	740912.677939	41.610868
3509.913204	740737.915757	41.615872
3509.883309	740584.291544	41.620877
3509.809797	740403.466580	41.625882
3510.129762	740238.054945	41.630887
3509.482494	740075.223517	41.635892
3509.399057	739899.978345	41.640896
3509.594966	739747.042611	41.645901
3509.425189	739584.864237	41.650906
3509.286374	739430.246311	41.655911
3508.811502	739274.988321	41.660916
3509.119976	739122.417737	41.665920
3509.084628	738971.187333	41.670925
3509.111715	738816.035327	41.675930
3509.274304	738654.871486	41.680935
3508.759769	738500.347051	41.685940
3509.138947	738341.763289	41.690944
3508.804475	738203.085278	41.695949
3508.888096	738051.322979	41.700954
3508.912603	737898.775893	41.705959
3508.376544	737759.579208	41.710964
3508.692915	737610.046141	41.715968
3508.481357	737462.576794	41.720973
3508.259847	737320.401034	41.725978
3508.602578	737182.137685	41.730983
3508.297942	737044.572736	41.735988
3508.192648	736894.947516	41.740992
3508.047136	736764.180441	41.745997
3508.112009	736615.709549	41.751002
3508.072791	736479.476662	41.756007
3507.855436	736360.690965	41.761012
3508.264132	736219.678207	41.766016
3507.752718	736090.445280	41.771021
3507.651522	735952.877436	41.776026
3507.859962	735824.659567	41.781031
3507.531713	735688.955921	41.786036
3507.522059	735562.403167	41.791040
3507.492389	735442.038533	41.796045
3507.065114	735308.621560	41.801050
3507.462340	735183.678438	41.806055
3507.242825	735060.666672	41.811060
3507.521795	734930.937971	41.816064
3507.253254	734819.909031	41.821069
3507.340951	734698.177402	41.826074
3507.615428	734582.105540	41.831079
3507.340983	734444.144475	41.836084
3507.308101	734318.862988	41.841088
3507.051550	734208.912659	41.846093
3507.044403	734083.128229	41.851098
3506.769220	733963.574074	41.856103
3506.753138	733854.915768	41.861108
3507.074478	733739.269551	41.866112
3506.669243	733628.890326	41.871117
3506.910432	733511.719416	41.876122
3506.969780	733390.863824	41.881127
3506.525252	733277.070285	41.886132
3506.976380	733162.434015	41.891136
3506.924264	733055.206634	41.896141
3506.844074	732943.873154	41.901146
3506.749230	732823.430624	41.906151
3506.651665	732720.810792	41.911156
3506.701482	732585.041832	41.916160
3506.462989	732496.008714	41.921165
3506.501643	732382.370278	41.926170
3506.449337	732277.063616	41.931175
3506.031618	732178.104311	41.936180
3506.400782	732065.991278	41.941184
3506.130921	731965.123356	41.946189
3506.010418	731863.338199	41.951194
3506.091360	731760.973786	41.956199
3506.128375	731654.059710	41.961204
3506.030870	731568.310767	41.966208
3505.909726	731470.432717	41.971213
3505.875358	731358.822250	41.976218
3505.867576	731266.617747	41.981223
3505.502585	731166.052710	41.986228
3505.560729	731069.526770	41.991232
3505.591865	730977.064938	41.996237
3505.669179	730885.089645	42.001242
3505.621352	730805.613768	42.006247
3505.081751	730718.789867	42.011252
3505.363461	730623.063571	42.016256
3505.588511	730551.216329	42.021261
3505.619057	730458.996315	42.026266
3505.912255	730356.628629	42.031271
3505.419179	730256.717318	42.036276
3505.689405	730155.886214	42.041280
3505.801409	730079.843703	42.046285
3505.407541	729988.134226	42.051290
3505.646250	729902.114006	42.056295
3505.582384	729811.388099	42.061300
3505.307944	729716.485968	42.066304
3505.503345	729628.241180	42.071309
3505.430876	729538.157539	42.076314
3505.365564	729452.232335	42.081319
3505.466138	729365.783495	42.086324
3505.192304	729265.724712	42.091328
3505.173712	729193.162757	42.096333
3505.236734	729103.596778	42.101338
3504.994681	729020.618689	42.106343
3504.825090	728946.246737	42.111348
3505.230321	728852.212901	42.116352
3505.219838	728776.822416	42.121357
3504.666830	728694.338206	42.126362
3505.062114	728608.526136	42.131367
3504.662100	728526.460771	42.136372
3504.717907	728456.307265	42.141376
3504.729326	728381.652567	42.146381
3504.895392	728313.064814	42.151386
3504.820743	728238.026721	42.156391
3504.300746	728159.346108	42.161396
3504.713218	728084.671961	42.166400
3504.759723	728007.085213	42.171405
3504.660048	727933.435574	42.176410
3504.797829	727864.650571	42.181415
3504.682485	727790.605909	42.186420
3504.417966	727709.054888	42.191424
3504.440939	727644.943929	42.196429
3504.404357	727576.482568	42.201434
3504.290716	727507.686567	42.206439
3504.200830	727441.710032	42.211444
3504.316551	727368.515144	42.216448
3504.307669	727305.050855	42.221453
3504.528952	727240.210336	42.226458
3504.652247	727155.864762	42.231463
3504.212297	727090.934149	42.236468
3504.316629	727006.292895	42.241472
3504.363800	726944.005648	42.246477
3504.269250	726868.462812	42.251482
3504.410009	726812.451543	42.256487
3504.137100	726750.463453	42.261492
3504.299035	726676.065601	42.266496
3503.846852	726617.277197	42.271501
3503.974747	726553.685388	42.276506
3504.011674	726489.959470	42.281511
3503.965674	726431.201708	42.286516
3503.849457	726358.482071	42.291520
3503.835694	726302.740605	42.296525
3504.003674	726242.013668	42.301530
3504.218590	726183.557871	42.306535
3503.995515	726117.493580	42.311540
3503.957399	726054.619056	42.316544
3504.053331	726004.555884	42.321549
3503.811154	725943.299893	42.326554
3503.778462	725879.382529	42.331559
3503.636557	725835.799490	42.336564
3503.755512	725768.139722	42.341568
3503.977379	725708.936098	42.346573
3503.963027	725637.778964	42.351578
3503.987973	725574.593019	42.356583
3503.582560	725527.137071	42.361588
3503.813492	725462.677353	42.366592
3503.564839	725408.950847	42.371597
3503.694067	725343.664558	42.376602
3503.662285	725287.175837	42.381607
3503.652412	725246.739461	42.386612
3503.731942	725185.325542	42.391616
3503.408248	725134.731732	42.396621
3503.391104	725086.069256	42.401626
3503.369388	725023.134573	42.406631
3503.325661	724988.005217	42.411636
3503.089057	724929.069976	42.416640
3503.396400	724874.405604	42.421645
3502.751007	724834.072219	42.426650
3503.426402	724783.063351	42.431655
3503.358425	724745.211200	42.436660
3503.291082	724689.765007	42.441664
3503.325916	724634.103314	42.446669
3503.079415	724593.752393	42.451674
3503.291581	724536.524361	42.456679
3503.035872	724498.057805	42.461684
3503.029100	724447.704765	42.466688
3503.388819	724412.506286	42.471693
3503.170876	724367.044686	42.476698
3502.951310	724311.323729	42.481703
3503.137408	724267.826865	42.486708
3503.097033	724221.096055	42.491712
3503.049390	724184.724852	42.496717
3502.887828	724142.226473	42.501722
3502.898505	724090.877106	42.506727
3502.889101	724046.469674	42.511732
3502.978388	723998.972721	42.516736
3502.762720	723966.048242	42.521741
3502.942849	723925.722677	42.526746
3503.151547	723875.380101	42.531751
3503.046136	723829.996073	42.536756
3503.109485	723785.922173	42.541760
3503.046660	723747.767198	42.546765
3502.397328	723700.687979	42.551770
3503.036234	723650.818167	42.556775
3502.970974	723616.677850	42.561780
3502.800468	723581.860850	42.566784
3502.913744	723551.507388	42.571789
3502.530523	723504.680476	42.576794
3503.252648	723457.224532	42.581799
3502.792102	723419.926843	42.586804
3502.919977	723376.583610	42.591808
3502.671540	723325.470572	42.596813
3502.571763	723298.621158	42.601818
3502.866779	723250.887633	42.606823
3502.662896	723220.981917	42.611828
3502.950538	723180.833226	42.616832
3503.018998	723156.087015	42.621837
3502.721258	723106.616552	42.626842
3502.808177	723054.554170	42.631847
3502.570993	723033.030563	42.636852
3502.797567	722977.127732	42.641856
3502.648130	722967.139310	42.646861
3502.485156	722925.477595	42.651866
3502.712699	722887.022809	42.656871
3502.648274	722851.292927	42.661876
3502.760079	722813.055207	42.666880
3502.685050	722778.714757	42.671885
3502.489469	722734.925899	42.676890
3502.599477	722701.694701	42.681895
3502.278527	722675.325958	42.686900
3502.607151	722626.244833	42.691904
3502.549208	722595.370862	42.696909
3502.531445	722567.216633	42.701914
3502.570233	722518.281911	42.706919
3502.235019	722497.219264	42.711924
3502.125707	722454.158260	42.716928
3502.291975	722415.265250	42.721933
3502.335290	722385.563529	42.726938
3502.485050	722344.937834	42.731943
3502.265901	722329.358294	42.736948
3502.554801	722290.890603	42.741952
3502.463086	722253.130099	42.746957
3502.288402	722231.494927	42.751962
3502.572048	722200.662186	42.756967
3502.476262	722169.396280	42.761972
3502.089315	722136.046635	42.766976
3502.357906	722107.149469	42.771981
3502.333657	722071.211279	42.776986
3502.367058	722044.137482	42.781991
3502.063185	722026.142156	42.786996
3502.246166	721987.690562	42.792001
3502.238892	721957.995669	42.797005
3501.707097	721947.771741	42.802010
3502.268790	721906.927100	42.807015
3502.002185	721896.064365	42.812020
3501.925196	721858.497936	42.817025
3502.192517	721846.852828	42.822029
3502.192427	721810.512899	42.827034
3502.110915	721783.060622	42.832039
3502.195610	721763.066995	42.837044
3502.101330	721733.435253	42.842049
3502.027101	721713.864390	42.847053
3501.911823	721686.367795	42.852058
3502.004106	721648.028771	42.857063
3501.802303	721633.238305	42.862068
3502.108612	721599.375310	42.867073
3502.136401	721576.564664	42.872077
3501.994732	721547.634190	42.877082
3502.146594	721531.545629	42.882087
3502.107314	721502.399762	42.887092
3501.841198	721473.836649	42.892097
3502.144704	721433.131504	42.897101
3502.254081	721418.140492	42.902106
3502.060185	721385.499616	42.907111
3502.004938	721364.239080	42.912116
3502.311125	721341.976742	42.917121
3502.017689	721315.995760	42.922125
3502.004565	721298.099545	42.927130
3502.200429	721269.806448	42.932135
3501.722226	721249.160896	42.937140
3502.010497	721221.100267	42.942145
3501.926061	721198.406288	42.947149
3502.151957	721177.445881	42.952154
3501.999717	721141.376071	42.957159
3501.757089	721130.062136	42.962164
3501.745420	721097.241269	42.967169
3501.844985	721085.374911	42.972173
3501.828943	721056.570710	42.977178
3501.719148	721031.203051	42.982183
3501.872834	721034.202225	42.987188
3501.706554	720998.530769	42.992193
3501.807785	720977.292966	42.997197
3501.615391	720956.401125	43.002202
3501.641787	720941.571714	43.007207
3501.676050	720933.087533	43.012212
3501.976819	720900.115092	43.017217
3501.754237	720889.739587	43.022221
3501.757892	720865.988906	43.027226
3501.825521	720838.260944	43.032231
3501.610102	720824.859609	43.037236
3501.635977	720792.229666	43.042241
3502.333937	720777.784819	43.047245
3501.938603	720763.669366	43.052250
3502.102093	720720.504699	43.057255
3501.631333	720709.128721	43.062260
3501.758117	720673.308272	43.067265
3501.748441	720674.648716	43.072269
3501.805999	720648.805979	43.077274
3501.790227	720622.529021	43.082279
3501.783237	720609.687907	43.087284
3501.720449	720583.220257	43.092289
3501.656293	720584.916809	43.097293
3501.341474	720551.548869	43.102298
3501.558511	720522.158868	43.107303
3501.543238	720531.979274	43.112308
3501.560320	720499.300050	43.117313
3501.757064	720483.697897	43.122317
3501.339057	720469.040251	43.127322
3501.520873	720456.812309	43.132327
3501.682849	720440.075358	43.137332
3501.367410	720426.888251	43.142337
3501.679929	720413.944450	43.147341
3501.403797	720385.230489	43.152346
3501.646423	720383.603729	43.157351
3501.699089	720369.413571	43.162356
3501.416126	720350.072332	43.167361
3501.469115	720328.543330	43.172365
3501.224014	720324.567438	43.177370
3501.734517	720314.962621	43.182375
3501.502948	720292.439240	43.187380
3501.608751	720277.645110	43.192385
3501.559245	720265.950978	43.197389
3501.383579	720245.153756	43.202394
3501.664922	720226.611535	43.207399
3501.321778	720221.808822	43.212404
3501.529079	720188.253969	43.217409
3501.738355	720178.450839	43.222413
3501.582837	720182.245223	43.227418
3501.600948	720147.680145	43.232423
3501.247697	720135.688914	43.237428
3501.078329	720128.179720	43.242433
3501.300411	720129.630715	43.247437
3501.205296	720104.852851	43.252442
3501.408337	720085.579445	43.257447
3501.337949	720073.888494	43.262452
3501.248702	720073.159505	43.267457
3501.452986	720066.679436	43.272461
3501.581338	720044.790134	43.277466
3501.521891	720032.502263	43.282471
3501.540529	720016.383203	43.287476
3501.486781	719993.829628	43.292481
3501.408861	719978.222331	43.297485
3501.039472	719988.399425	43.302490
3500.960065	719966.891367	43.307495
3500.941528	719966.001919	43.312500
3501.304273	719944.470326	43.317505
3501.438330	719932.199919	43.322509
3501.179594	719916.919917	43.327514
3501.425446	719902.250743	43.332519
3501.088434	719914.902006	43.337524
3500.995237	719879.064905	43.342529
3501.191707	719877.247320	43.347533
3500.657040	719869.104015	43.352538
3501.131046	719866.199200	43.357543
3501.469617	719866.292095	43.362548
3501.338751	719848.065095	43.367553
3501.504914	719845.855800	43.372557
3501.109519	719831.837948	43.377562
3501.445675	719809.169852	43.382567
3501.162222	719813.729382	43.387572
3501.004299	719808.449517	43.392577
3501.111073	719807.836880	43.397581
3501.271468	719775.230310	43.402586
3501.278624	719756.286050	43.407591
3501.317168	719753.056442	43.412596
3501.494431	719757.837404	43.417601
3501.259750	719741.660494	43.422605
3501.343189	719721.612580	43.427610
3501.553338	719709.180502	43.432615
3501.228986	719714.391510	43.437620
3501.233312	719697.778301	43.442625
3501.260103	719665.391740	43.447629
3501.108685	719659.713986	43.452634
3501.562019	719662.366600	43.457639
3501.451323	719658.913668	43.462644
3501.322264	719640.884276	43.467649
3501.133779	719623.856470	43.472653
3501.338713	719626.500555	43.477658
3501.468687	719600.196286	43.482663
3501.375874	719581.714463	43.487668
3501.489357	719566.372307	43.492673
3501.689625	719558.801516	43.497677
3501.253518	719560.807694	43.502682
3501.188440	719535.527267	43.507687
3501.414412	719530.431741	43.512692
3501.091361	719517.690764	43.517697
3501.308002	719515.968950	43.522701
3501.113019	719519.224656	43.527706
3501.054300	719483.330565	43.532711
3501.372766	719485.509614	43.537716
3501.531801	719473.879090	43.542721
3501.495616	719473.637191	43.547725
3501.423512	719462.590350	43.552730
3501.415990	719440.771508	43.557735
3501.277247	719429.586862	43.562740
3501.273684	719422.644727	43.567745
3501.456382	719396.033554	43.572749
3501.165124	719393.502998	43.577754
3501.189668	719368.108069	43.582759
3501.619344	719371.706932	43.587764
3501.531475	719354.215623	43.592769
3501.801826	719338.301615	43.597773
3501.217056	719333.339945	43.602778
3501.447039	719320.209724	43.607783
3501.286279	719295.093156	43.612788
3501.465377	719282.417614	43.617793
3501.500499	719269.369106	43.622797
3501.397961	719267.253656	43.627802
3501.620898	719248.818102	43.632807
3501.619375	719242.371405	43.637812
3501.419716	719219.443107	43.642817
3501.429131	719194.794042	43.647821
3501.092026	719180.517493	43.652826
3501.143469	719179.269247	43.657831
3501.348372	719175.763960	43.662836
3501.328998	719167.336438	43.667841
3501.415732	719136.425707	43.672845
3501.357831	719133.211797	43.677850
3501.474614	719126.894241	43.682855
3501.359036	719121.706128	43.687860
3501.518608	719089.692137	43.692865
3501.344926	719089.373761	43.697869
3501.341232	719074.149251	43.702874
3501.335683	719065.322594	43.707879
3501.206153	719039.852941	43.712884
3501.228108	719039.254265	43.717889
3501.477437	719024.533384	43.722893
3501.346338	719022.968123	43.727898
3501.550560	718995.707399	43.732903
3501.497155	718989.269080	43.737908
3501.377730	718974.906613	43.742913
3501.308634	718960.932557	43.747917
3501.231570	718950.877742	43.752922
3501.388845	718938.651634	43.757927
3501.302617	718936.285433	43.762932
3501.383959	718934.089916	43.767937
3501.489972	718897.124601	43.772941
3501.431997	718895.001692	43.777946
3501.259578	718893.096072	43.782951
3501.353409	718884.699153	43.787956
3501.058207	718864.662157	43.792961
3501.509113	718842.617212	43.797965
3501.613947	718845.922822	43.802970
3501.701562	718826.070447	43.807975
3501.364462	718801.675863	43.812980
3501.663177	718802.469694	43.817985
3501.503769	718791.287606	43.822989
3501.558940	718777.540685	43.827994
3501.522693	718751.955548	43.832999
3501.308972	718758.487941	43.838004
3500.832610	718741.257927	43.843009
3501.360294	718715.728276	43.848013
3501.140916	718703.762450	43.853018
3501.625372	718709.485167	43.858023
3501.671473	718704.914821	43.863028
3501.390514	718678.625963	43.868033
3501.722296	718663.890823	43.873037
3501.515541	718654.650618	43.878042
3501.463241	718630.555642	43.883047
3501.474610	718618.601159	43.888052
3501.445569	718612.753678	43.893057
3501.536677	718597.066267	43.898061
3501.499583	718581.895977	43.903066
3501.706391	718578.439723	43.908071
3501.504182	718563.941439	43.913076
3501.253836	718538.886996	43.918081
3501.360040	718528.702193	43.923085
3501.245038	718522.968049	43.928090
3501.319556	718507.630389	43.933095
3501.300997	718486.554832	43.938100
3501.453146	718471.005888	43.943105
3501.455804	718446.157343	43.948109
3501.176811	718451.460830	43.953114
3501.327483	718429.018037	43.958119
3501.266647	718412.313844	43.963124
3501.498454	718405.877541	43.968129
3501.246410	718394.809425	43.973133
3501.100894	718396.172682	43.978138
3501.145961	718371.316906	43.983143
3501.236587	718353.099635	43.988148
3501.311435	718354.872863	43.993153
3501.601524	718342.971123	43.998157
3501.107114	718341.019389	44.003162
3501.383764	718312.950906	44.008167
3501.652114	718312.460255	44.013172
3501.212077	718300.530315	44.018177
3501.282286	718299.874014	44.023181
3501.156276	718279.510065	44.028186
3501.445894	718262.450070	44.033191
3501.503959	718260.952602	44.038196
3501.398315	718251.149658	44.043201
3501.320410	718219.865959	44.048205
3501.431027	718210.820808	44.053210
3501.219983	718203.515159	44.058215
3501.251105	718202.071730	44.063220
3501.445955	718187.705573	44.068225
3501.326470	718161.041210	44.073229
3501.322931	718165.803368	44.078234
3501.522711	718155.057060	44.083239
3501.726485	718138.258994	44.088244
3501.252979	718121.920010	44.093249
3501.341754	718110.745596	44.098253
3501.310857	718106.733240	44.103258
3501.332245	718094.925151	44.108263
3501.450296	718076.901144	44.113268
3501.343361	718067.098198	44.118273
3501.608741	718059.366496	44.123277
3501.132886	718043.325343	44.128282
3501.641228	718015.465575	44.133287
3501.722474	718017.981815	44.138292
3501.795059	718001.006754	44.143297
3501.748624	717983.356927	44.148301
3501.345079	717979.406090	44.153306
3501.127216	717948.838906	44.158311
3501.442441	717938.966047	44.163316
3501.406449	717927.018402	44.168321
3501.628423	717921.128958	44.173325
3501.286230	717908.041477	44.178330
3501.330902	717885.416343	44.183335
3501.611171	717884.477295	44.188340
3501.225862	717872.140892	44.193345
3501.439981	717850.430074	44.198349
3501.376256	717839.082096	44.203354
3501.575727	717829.129036	44.208359
3501.591771	717815.635005	44.213364
3501.243915	717802.647497	44.218369
3501.391690	717788.834048	44.223373
3501.261376	717783.796342	44.228378
3501.412336	717777.224115	44.233383
3501.648431	717751.243705	44.238388
3501.620270	717743.411416	44.243393
3501.606876	717728.533270	44.248397
3501.108742	717702.872447	44.253402
3501.197561	717692.937511	44.258407
3501.182376	717695.122572	44.263412
3501.078819	717693.899719	44.268417
3501.514841	717678.748812	44.273421
3501.160067	717659.611600	44.278426
3501.048721	717642.467800	44.283431
3501.017865	717637.413569	44.288436
3501.152496	717641.557968	44.293441
3501.248087	717633.754729	44.298445
3500.913550	717629.941127	44.303450
3501.359556	717618.905433	44.308455
3501.379333	717602.037495	44.313460
3501.107922	717593.898048	44.318465
3501.044642	717582.202433	44.323469
3501.199152	717582.970614	44.328474
3501.625844	717573.475726	44.333479
3501.294515	717551.755067	44.338484
3501.125826	717548.112431	44.343489
3501.339223	717546.737974	44.348493
3500.988498	717528.641447	44.353498
3501.421669	717524.006494	44.358503
3501.775413	717496.864992	44.363508
3501.432346	717497.169775	44.368513
3501.404417	717469.744037	44.373517
3501.054814	717462.014207	44.378522
3501.453670	717441.859103	44.383527
3501.455064	717435.559341	44.388532
3501.292017	717440.001048	44.393537
3501.225593	717406.976302	44.398541
3500.957966	717401.911453	44.403546
3501.156657	717398.356851	44.408551
3501.299260	717394.662706	44.413556
3501.276920	717396.601010	44.418561
3501.345834	717384.536049	44.423565
3500.862279	717368.098041	44.428570
3501.145414	717347.813023	44.433575
3500.939442	717349.781683	44.438580
3501.030086	717340.342065	44.443585
3501.268838	717337.078441	44.448589
3501.071743	717350.057673	44.453594
3500.532437	717347.319457	44.458599
3500.643430	717339.662211	44.463604
3500.819132	717346.478574	44.468609
3501.101521	717345.588722	44.473613
3500.761725	717329.523712	44.478618
3501.297169	717307.559975	44.483623
3501.399969	717304.814844	44.488628
3501.018274	717303.637897	44.493633
3500.939095	717304.940762	44.498637
3501.040560	717298.673965	44.503642
3501.403807	717290.726968	44.508647
3501.347350	717266.083107	44.513652
3500.946253	717270.167407	44.518657
3501.187251	717276.873829	44.523661
3501.282224	717283.703584	44.528666
3501.331474	717275.014795	44.533671
3501.409823	717277.680549	44.538676
3501.034300	717260.629227	44.543681
3500.966361	717256.969815	44.548685
3500.934224	717253.205275	44.553690
3500.891280	717245.920612	44.558695
3501.231242	717246.509366	44.563700
3500.929499	717245.517615	44.568705
3501.139823	717236.405334	44.573709
3500.987917	717220.705900	44.578714
3500.980558	717195.706487	44.583719
3501.080876	717201.940170	44.588724
3501.151142	717191.412450	44.593729
3501.195686	717186.593511	44.598733
3501.052550	717198.373548	44.603738
3500.977646	717188.961117	44.608743
3501.349037	717184.981049	44.613748
3501.024982	717163.655018	44.618753
3501.439711	717151.086131	44.623757
3501.144252	717146.769800	44.628762
3501.228931	717143.432352	44.633767
3501.648322	717131.953975	44.638772
3501.235594	717117.785601	44.643777
3501.107133	717097.220760	44.648781
3501.172519	717100.285556	44.653786
3501.105667	717097.915629	44.658791
3500.911481	717103.553184	44.663796
3501.023579	717084.436715	44.668801
3501.234152	717064.510242	44.673805
3501.248063	717068.922902	44.678810
3501.022153	717048.919705	44.683815
3500.788749	717053.968508	44.688820
3500.906777	717050.327879	44.693825
3501.288633	717050.711303	44.698829
3500.814131	717053.170856	44.703834
3501.167525	717027.863300	44.708839
3500.957776	717012.073824	44.713844
3500.963931	717011.279192	44.718849
3500.879833	717010.251445	44.723853
3501.047990	717011.215848	44.728858
3500.894535	717007.322430	44.733863
3501.087167	717008.382000	44.738868
3501.204628	717015.059441	44.743873
3501.538796	716987.572289	44.748877
3501.211469	716978.052517	44.753882
3501.596357	716958.841077	44.758887
3501.362002	716963.046789	44.763892
3501.591159	716941.380742	44.768897
3501.343449	716920.487931	44.773901
3500.988304	716906.805746	44.778906
3501.222475	716906.568700	44.783911
3501.343707	716882.092773	44.788916
3501.225192	716860.483971	44.793921
3501.208784	716843.322847	44.798925
3501.096286	716833.469769	44.803930
3501.125479	716826.470461	44.808935
3501.231196	716828.437341	44.813940
3501.026236	716817.458566	44.818945
3501.393813	716786.641575	44.823949
3501.312650	716786.059779	44.828954
3501.310118	716781.794065	44.833959
3501.309676	716771.426326	44.838964
3500.956612	716763.398777	44.843969
3501.371960	716740.758908	44.848973
3501.254136	716747.128192	44.853978
3501.239099	716740.284944	44.858983
3501.294790	716738.142701	44.863988
3501.032032	716722.113401	44.868993
3501.369656	716700.478417	44.873997
3501.170008	716688.952913	44.879002
3501.316794	716686.745997	44.884007
3500.893339	716679.374898	44.889012
3501.062852	716677.957947	44.894017
3501.544499	716665.426886	44.899021
3500.873303	716646.290038	44.904026
3501.136915	716645.800081	44.909031
3501.186230	716647.776324	44.914036
3500.971382	716638.733657	44.919041
3501.176145	716625.652997	44.924045
3500.934710	716628.520628	44.929050
3501.017346	716617.841322	44.934055
3501.072083	716601.164027	44.939060
3500.991125	716594.728419	44.944065
3500.972224	716578.410505	44.949069
3501.045457	716579.043388	44.954074
3501.086071	716582.459725	44.959079
3501.145876	716576.695357	44.964084
3500.824783	716576.649278	44.969089
3501.203863	716562.646765	44.974093
3501.194985	716557.885902	44.979098
3501.048983	716543.027568	44.984103
3501.154122	716540.976321	44.989108
3500.876876	716542.659294	44.994113
3501.242676	716530.841697	44.999117
3500.985759	716549.338601	45.004122
3501.272624	716527.314692	45.009127
3501.172459	716503.667986	45.014132
3501.056589	716501.206774	45.019137
3501.391494	716479.125192	45.024141
3501.239923	716483.466287	45.029146
3501.219384	716484.958024	45.034151
3501.045812	716468.169367	45.039156
3500.922921	716463.625727	45.044161
3501.408955	716457.493189	45.049165
3501.422035	716450.446622	45.054170
3500.707042	716453.640613	45.059175
3501.169021	716450.687023	45.064180
3501.097162	716447.424776	45.069185
3501.242435	716424.679862	45.074189
3501.255523	716412.077028	45.079194
3500.853417	716400.733412	45.084199
3501.155574	716403.808945	45.089204
3501.207061	716410.646598	45.094209
3501.296361	716398.676071	45.099213
3501.019212	716378.034819	45.104218
3501.256085	716369.462918	45.109223
3501.255201	716366.288130	45.114228
3501.196713	716368.530301	45.119233
3501.093548	716362.147794	45.124237
3501.127723	716345.969486	45.129242
3501.338854	716327.479856	45.134247
3501.400088	716311.396231	45.139252
3501.324734	716317.014674	45.144257
3501.432995	716311.539776	45.149261
3501.228521	716294.607049	45.154266
3501.223375	716279.625751	45.159271
3501.303289	716274.701225	45.164276
3500.961856	716271.880338	45.169281
3501.348292	716266.954764	45.174285
3501.482957	716244.955269	45.179290
3501.341187	716220.421656	45.184295
3500.915169	716215.630312	45.189300
3501.157230	716214.201295	45.194305
3501.616104	716218.888144	45.199309
3501.326642	716201.572390	45.204314
3501.353914	716185.742189	45.209319
3500.993255	716178.459491	45.214324
3500.967198	716177.223608	45.219329
3501.128244	716175.262255	45.224333
3501.029297	716170.317614	45.229338
3500.976521	716143.685421	45.234343
3501.056428	716131.269568	45.239348
3500.987541	716131.330640	45.244353
3501.386475	716119.209326	45.249357
3501.193682	716120.779203	45.254362
3501.202206	716122.266201	45.259367
3501.304108	716103.595686	45.264372
3501.182072	716091.560424	45.269377
3501.263570	716072.496322	45.274381
3501.065730	716083.344345	45.279386
3501.025118	716077.745064	45.284391
3501.030111	716072.187853	45.289396
3500.966534	716064.855963	45.294401
3501.221740	716043.183300	45.299405
3501.233154	716039.311796	45.304410
3501.355501	716033.040606	45.309415
3501.202733	716041.152601	45.314420
3500.886760	716021.608341	45.319425
3501.342095	716004.913276	45.324429
3501.228848	715989.998938	45.329434
3501.085905	715987.790107	45.334439
3501.200137	715983.703139	45.339444
3501.019022	715985.519171	45.344449
3501.208040	715983.900434	45.349453
3500.995215	715955.160785	45.354458
3501.104536	715943.186302	45.359463
3501.196843	715939.053324	45.364468
3500.980219	715935.963637	45.369473
3501.059896	715934.660633	45.374477
3501.180106	715937.171061	45.379482
3500.766606	715943.093693	45.384487
3500.988598	715939.782690	45.389492
3501.154636	715932.214291	45.394497
3501.521736	715914.839060	45.399501
3501.388603	715895.810027	45.404506
3501.145468	715895.056485	45.409511
3501.349757	715893.782494	45.414516
3501.090535	715883.158749	45.419521
3501.600071	715857.722650	45.424525
3501.305282	715852.065996	45.429530
3501.141083	715848.471488	45.434535
3501.566178	715840.413684	45.439540
3501.252009	715829.550888	45.444545
3501.551009	715822.406933	45.449549
3501.164998	715808.529603	45.454554
3501.305235	715796.351351	45.459559
3501.197428	715769.280551	45.464564
3500.928999	715752.059620	45.469569
3501.579542	715753.341362	45.474573
3501.574738	715757.410511	45.479578
3501.292336	715745.053962	45.484583
3501.579377	715730.916440	45.489588
3501.308006	715718.806096	45.494593
3501.592972	715714.988465	45.499597
3501.015156	715688.739275	45.504602
3501.240507	715676.100263	45.509607
3501.311394	715673.111808	45.514612
3500.945033	715671.535176	45.519617
3501.221585	715674.267916	45.524621
3501.087867	715656.776461	45.529626
3501.222350	715632.443550	45.534631
3501.074020	715625.026054	45.539636
3501.002487	715616.702809	45.544641
3500.734919	715614.812157	45.549645
3500.992187	715605.343058	45.554650
3500.870490	715618.560569	45.559655
3501.283661	715614.870548	45.564660
3501.268766	715615.964594	45.569665
3501.315088	715587.577776	45.574669
3501.058432	715578.937787	45.579674
3501.406151	715583.097607	45.584679
3501.347233	715563.162502	45.589684
3500.918298	715568.988716	45.594689
3501.172888	715553.467061	45.599693
3500.985627	715528.393189	45.604698
3501.018279	715525.609458	45.609703
3501.228582	715524.681721	45.614708
3501.119126	715531.745143	45.619713
3500.926897	715520.067963	45.624717
3501.065317	715521.732060	45.629722
3501.011122	715511.272421	45.634727
3501.338651	715481.449567	45.639732
3500.816941	715484.016595	45.644737
3500.955058	715474.070891	45.649741
3500.794787	715477.570489	45.654746
3500.677780	715469.006539	45.659751
3500.984983	715465.085891	45.664756
3500.998909	715473.716648	45.669761
3500.820773	715464.170499	45.674765
3501.017147	715463.145827	45.679770
3500.860597	715468.182874	45.684775
3501.384262	715467.649881	45.689780
3501.388470	715445.669857	45.694785
3501.513740	715427.142826	45.699789
3501.249499	715427.385030	45.704794
3501.027874	715428.612492	45.709799
3501.539818	715417.463800	45.714804
3501.252947	715398.508662	45.719809
3501.201591	715375.594948	45.724813
3501.179802	715376.045163	45.729818
3501.105485	715367.374824	45.734823
3501.408949	715337.158513	45.739828
3501.262334	715266.480272	45.744833
3501.347474	715146.990031	45.749837
3501.193164	714978.713967	45.754842
3501.122790	714740.011428	45.759847
3500.966435	714441.771499	45.764852
3500.485173	714096.383476	45.769857
3500.637704	713694.105482	45.774861
3500.209339	713234.981283	45.779866
3499.925893	712723.596643	45.784871
3500.106192	712149.118824	45.789876
3499.680009	711522.979774	45.794881
3498.816521	710832.481475	45.799885
3498.737709	710090.959866	45.804890
3498.392956	709278.516425	45.809895
3498.250341	708417.448619	45.814900
3497.379480	707501.390105	45.819905
3497.171873	706523.239480	45.824909
3496.923267	705488.506619	45.829914
3496.382387	704398.305957	45.834919
3495.519611	703239.156937	45.839924
3494.856180	702027.792081	45.844929
3494.131306	700747.136424	45.849933
3493.570398	699418.298290	45.854938
3493.016801	698023.285363	45.859943
3492.267203	696564.586718	45.864948
3491.514485	695060.093113	45.869953
3490.713527	693478.054963	45.874957
3489.789827	691841.030930	45.879962
3488.880045	690144.142786	45.884967
3488.463252	688396.535891	45.889972
3487.194247	686588.548372	45.894977
3486.435690	684710.560074	45.899981
3485.717281	682791.989334	45.904986
3484.396732	680802.335074	45.909991
3483.873319	678749.791791	45.914996
3482.048279	676660.530378	45.920001
3481.330186	674488.273570	45.925005
3480.154138	672269.769980	45.930010
3478.901943	670010.512123	45.935015
3478.271367	667668.608772	45.940020
3476.858795	665285.645953	45.945025
3475.781217	662829.472532	45.950029
3474.239638	660331.717519	45.955034
3472.672870	657776.352473	45.960039
3471.889690	655177.187898	45.965044
3470.283366	652528.015124	45.970049
3469.353725	649797.468792	45.975053
3467.699544	647041.003996	45.980058
3466.351117	644200.185439	45.985063
3464.959802	641324.020093	45.990068
3462.888758	638387.375964	45.995073
3461.733622	635393.147428	46.000077
3460.309405	632367.918444	46.005082
3458.895721	629280.529271	46.010087
3457.593645	626126.809941	46.015092
3455.854633	622943.174780	46.020097
3453.789329	619685.235068	46.025101
3452.208958	616395.762272	46.030106
3450.558110	613054.119382	46.035111
3448.797245	609654.708205	46.040116
3446.718202	606218.294782	46.045121
3445.347400	602709.200996	46.050125
3443.450226	599173.817572	46.055130
3441.243557	595577.894728	46.060135
3439.445509	591940.512151	46.065140
3436.968439	588255.643415	46.070145
3435.098379	584497.257350	46.075149
3433.372534	580736.731603	46.080154
3431.601753	576909.674959	46.085159
3430.008099	573035.325913	46.090164
3427.408160	569125.227176	46.095169
3425.620686	565151.370345	46.100173
3423.305355	561139.368360	46.105178
3420.860235	557079.011724	46.110183
3418.824287	552973.662135	46.115188
3416.730410	548838.144066	46.120193
3414.707116	544638.542965	46.125197
3412.520123	540401.087546	46.130202
3409.875553	536117.235274	46.135207
3407.733864	531805.833483	46.140212
3405.195389	527440.018748	46.145217
3403.094416	523024.323337	46.150221
3400.797215	518567.014083	46.155226
3398.448348	514091.448598	46.160231
3396.276989	509542.758119	46.165236
3393.258111	504976.585512	46.170241
3390.907503	500348.794490	46.175245
3388.471117	495700.710673	46.180250
3385.851929	490998.913499	46.185255
3383.407622	486273.086900	46.190260
3380.779172	481512.211034	46.195265
3378.423432	476692.409759	46.200269
3375.212766	471849.055374	46.205274
3372.350159	466965.189598	46.210279
3369.899816	462046.882165	46.215284
3366.912006	457103.013497	46.220289
3364.371149	452106.965961	46.225293
3361.813560	447081.175454	46.230298
3358.736748	442031.417575	46.235303
3356.143270	436940.900455	46.240308
3352.938076	431824.984904	46.245313
3349.959233	426655.072698	46.250317
3347.279180	421476.185581	46.255322
3344.362323	416257.896337	46.260327
3341.405560	411017.529169	46.265332
3337.965073	405740.498668	46.270337
3335.191076	400441.162063	46.275341
3332.312728	395103.459769	46.280346
3328.399466	389740.295367	46.285351
3325.769959	384359.876616	46.290356
3322.362395	378959.549148	46.295361
3319.556739	373510.762879	46.300365
3316.188810	368056.960309	46.305370
3312.632413	362577.312033	46.310375
3309.550231	357065.734691	46.315380
3306.455363	351540.858453	46.320385
3303.112068	345981.741607	46.325389
3299.718755	340412.556177	46.330394
3296.339851	334824.855669	46.335399
3293.164280	329190.087777	46.340404
3289.430438	323561.456697	46.345409
3285.914070	317898.682539	46.350413
3282.618208	312232.275397	46.355418
3279.060166	306533.893331	46.360423
3275.520822	300840.780437	46.365428
3271.833275	295124.745332	46.370433
3268.149124	289396.678586	46.375437
3264.660836	283657.713186	46.380442
3260.845565	277909.610451	46.385447
3257.321829	272135.912486	46.390452
3253.279827	266369.575919	46.395457
3249.661098	260586.348335	46.400461
3246.056812	254794.188487	46.405466
3242.026973	248984.302874	46.410471
3238.604633	243181.731020	46.415476
3234.668735	237377.741345	46.420481
3230.798817	231557.006330	46.425485
3226.861041	225731.108203	46.430490
3222.692537	219913.873285	46.435495
3219.082019	214080.290603	46.440500
3214.788558	208220.891032	46.445505
3210.785892	202331.851183	46.450509
3206.882160	196506.493162	46.455514
3202.486860	190680.841336	46.460519
3198.590789	184856.218486	46.465524
3193.946806	179037.345320	46.470529
3190.087942	173223.633220	46.475533
3186.035041	167430.874100	46.480538
3181.462123	161628.609713	46.485543
3176.889950	155836.492945	46.490548
3172.324176	150081.053525	46.495553
3168.023237	144309.491822	46.500557
3163.840497	138565.539201	46.505562
3159.439766	132837.668129	46.510567
3155.015800	127120.344433	46.515572
3150.172732	121421.055874	46.520577
3145.628875	115740.748533	46.525581
3140.832458	110075.878058	46.530586
3136.010540	104433.324800	46.535591
3131.539123	98812.207000	46.540596
3126.102755	93234.925809	46.545601
3121.314156	87673.225198	46.550605
3116.435679	82133.932302	46.555610
3111.045044	76645.616093	46.560615
3105.463992	71196.366664	46.565620
3099.782959	65787.873289	46.570625
3094.079513	60421.805148	46.575629
3087.952633	55124.011009	46.580634
3081.430560	49901.794550	46.585639
3070.568448	44824.457645	46.590644
3056.056768	39969.448288	46.595649
3041.772951	35262.996425	46.600653
3027.801068	30744.436280	46.605658
3014.032849	26429.956976	46.610663
3001.159264	22340.755391	46.615668
2988.313844	18488.913189	46.620673
2975.754461	14854.872413	46.625677
2963.236841	11487.369225	46.630682
2947.980795	8399.922057	46.635687
2927.126784	5743.964825	46.640692
2904.385768	3450.227992	46.645697
2882.993157	1516.094354	46.650701
2851.023238	266.401248	46.655706
2791.748346	250.079472	46.660711
2761.109975	242.352302	46.665716
2756.595969	245.974355	46.670721
2768.326100	256.714620	46.675725
2786.410361	233.996741	46.680730
2802.130114	228.547435	46.685735
2811.695641	227.973722	46.690740
2814.750145	230.522853	46.695745
2813.289208	237.413439	46.700749
2809.321408	229.761494	46.705754
2804.990840	224.328080	46.710759
2801.433644	225.594564	46.715764
2798.108514	232.672332	46.720769
2794.827879	225.828830	46.725773
2792.205200	229.116498	46.730778
2789.444218	239.080902	46.735783
2786.992523	225.073987	46.740788
2784.430697	221.738003	46.745793
2781.565606	220.247794	46.750797
2778.612455	226.963460	46.755802
2775.099135	229.192816	46.760807
2772.307680	220.554095	46.765812
2768.925790	221.461048	46.770817
2766.192232	222.637806	46.775821
2762.904410	213.098117	46.780826
2759.508433	230.823946	46.785831
2756.213078	214.399600	46.790836
2752.924659	221.100520	46.795841
2749.280372	215.549826	46.800845
2746.546749	205.020537	46.805850
2743.171747	214.256781	46.810855
2739.706926	202.087883	46.815860
2736.167095	218.599428	46.820865
2732.893640	216.602397	46.825869
2730.032029	210.048161	46.830874
2726.564015	209.484437	46.835879
2723.348733	205.309045	46.840884
2720.062653	208.356879	46.845889
2716.404656	212.389818	46.850893
2713.012690	209.661748	46.855898
2709.732256	213.743099	46.860903
2706.024558	208.570188	46.865908
2702.490463	213.617073	46.870913
2699.639915	215.866034	46.875917
2696.151551	207.128627	46.880922
2692.408824	217.120603	46.885927
2689.340936	212.843481	46.890932
2686.418880	206.860513	46.895937
2682.958732	206.444315	46.900941
2679.036110	196.771013	46.905946
2674.889198	204.221103	46.910951
2672.010199	188.088873	46.915956
2669.015134	199.348118	46.920961
2665.352871	200.812865	46.925965
2661.677700	202.181676	46.930970
2657.958608	204.447160	46.935975
2654.904483	197.091104	46.940980
2651.225155	202.962467	46.945985
2648.111329	190.590517	46.950989
2644.910545	191.498369	46.955994
2641.565820	192.426698	46.960999
2638.185597	198.158174	46.966004
2633.974957	207.895334	46.971009
2630.743177	193.456673	46.976013
2627.573985	191.640396	46.981018
2623.894477	193.572367	46.986023
2620.570839	189.998132	46.991028
2617.274194	191.522371	46.996033
2613.175129	194.439651	47.001037
2610.229766	195.200457	47.006042
2606.226424	191.518335	47.011047
2603.431104	184.186772	47.016052
2599.877108	180.280884	47.021057
2595.868292	195.506738	47.026061
2592.743885	187.929712	47.031066
2588.975433	191.271018	47.036071
2585.658426	186.843021	47.041076
2582.438626	192.510087	47.046081
2578.795831	193.337837	47.051085
2575.820359	190.587894	47.056090
2572.077727	194.825982	47.061095
2568.405114	180.993382	47.066100
2565.159628	190.086534	47.071105
2561.173514	180.535173	47.076109
2558.129774	183.949908	47.081114
2554.449400	177.840405	47.086119
2551.176238	187.143772	47.091124
2547.985618	185.429181	47.096129
2544.387302	198.547044	47.101133
2540.814604	184.122492	47.106138
2537.075989	189.319591	47.111143
2533.636951	186.411997	47.116148
2529.592266	187.471303	47.121153
2526.317197	190.690321	47.126157
2523.527208	180.486289	47.131162
2519.719589	189.437912	47.136167
2516.354006	183.669613	47.141172
2512.928601	188.439340	47.146177
2509.386852	184.353504	47.151181
2506.007558	182.486268	47.156186
2501.919391	192.718110	47.161191
2498.793215	181.213663	47.166196
2495.466619	185.721160	47.171201
2491.769295	184.826974	47.176205
2488.730173	182.627155	47.181210
2484.727613	186.867701	47.186215
2481.309825	184.370645	47.191220
2478.085454	185.273252	47.196225
2474.104744	178.030719	47.201229
2471.141934	176.618872	47.206234
2467.795253	185.079013	47.211239
2464.512000	182.514110	47.216244
2460.477761	178.543811	47.221249
2456.873338	170.896019	47.226253
2453.479043	169.128797	47.231258
2449.956477	173.521167	47.236263
2446.410600	169.895277	47.241268
2442.568687	171.623408	47.246273
2439.236427	175.995719	47.251277
2436.744389	174.076142	47.256282
2432.704873	171.205122	47.261287
2429.009634	160.702141	47.266292
2425.652879	172.020812	47.271297
2422.301135	171.995759	47.276301
2418.372435	167.947840	47.281306
2415.023855	176.349325	47.286311
2411.587232	170.030674	47.291316
2407.775807	175.702293	47.296321
2404.745428	165.279661	47.301325
2401.604522	165.785078	47.306330
2397.835943	177.004037	47.311335
2394.331330	169.979737	47.316340
2390.781972	172.420790	47.321345
2387.124717	174.851495	47.326349
2383.735236	178.751627	47.331354
2380.049557	171.370348	47.336359
2376.884582	166.924852	47.341364
2372.947947	166.647613	47.346369
2369.809620	167.372657	47.351373
2366.191704	168.474514	47.356378
2362.591913	170.033955	47.361383
2359.465461	178.904663	47.366388
2355.613194	167.825485	47.371393
2352.095653	177.470786	47.376397
2348.611762	166.753105	47.381402
2345.151811	168.736367	47.386407
2342.154130	154.380205	47.391412
2338.370877	162.773410	47.396417
2334.738224	164.815870	47.401421
2331.535700	157.961435	47.406426
2327.940213	167.599331	47.411431
2324.305623	157.972056	47.416436
2320.698513	161.422632	47.421441
2317.161162	162.917107	47.426445
2313.971638	153.840504	47.431450
2309.999686	167.666075	47.436455
2306.797319	160.169303	47.441460
2303.092632	164.664176	47.446465
2299.429213	166.597899	47.451469
2296.406095	161.635831	47.456474
2292.749242	166.591858	47.461479
2289.373303	157.226859	47.466484
2285.866927	159.086038	47.471489
2282.565386	166.099652	47.476493
2279.415488	156.158496	47.481498
2275.327762	175.221037	47.486503
2271.997174	154.641235	47.491508
2268.298415	164.500522	47.496513
2264.418256	169.864552	47.501517
2261.193726	161.223191	47.506522
2257.863196	158.518289	47.511527
2254.692587	162.493362	47.516532
2250.779024	165.346705	47.521537
2247.173353	164.296659	47.526541
2243.626535	167.250485	47.531546
2240.121757	166.403763	47.536551
2236.689837	161.159184	47.541556
2233.392514	163.329115	47.546561
2229.937601	166.832110	47.551565
2226.725940	161.216176	47.556570
2222.663128	156.891506	47.561575
2219.169266	171.476440	47.566580
2215.886545	173.749345	47.571585
2212.460021	163.394469	47.576589
2209.173189	155.937624	47.581594
2205.293829	169.421155	47.586599
2201.857894	164.414073	47.591604
2198.111034	161.076458	47.596609
2194.259591	160.664704	47.601613
2191.082679	153.928889	47.606618
2187.760474	155.874067	47.611623
2184.560322	154.167855	47.616628
2181.142200	156.662720	47.621633
2177.424146	154.926865	47.626637
2174.156230	148.390650	47.631642
2170.225950	157.062316	47.636647
2166.871836	155.098051	47.641652
2163.502809	161.362396	47.646657
2159.990277	159.363994	47.651661
2156.210075	166.220191	47.656666
2152.860321	161.023643	47.661671
2149.342667	149.606874	47.666676
2145.834081	158.675993	47.671681
2142.059600	153.788990	47.676685
2139.207916	145.272065	47.681690
2135.495669	150.738429	47.686695
2131.741920	150.758106	47.691700
2128.367613	149.793369	47.696705
2124.860054	157.870920	47.701709
2121.396208	147.902983	47.706714
2117.890496	166.534929	47.711719
2114.324801	154.885991	47.716724
2110.921833	152.894938	47.721729
2106.979360	151.247831	47.726733
2103.760118	152.715041	47.731738
2100.183126	152.270338	47.736743
2096.691877	152.929537	47.741748
2093.438522	152.321898	47.746753
2089.996116	159.422724	47.751757
2086.899030	155.278797	47.756762
2082.809044	159.392106	47.761767
2079.275729	153.969106	47.766772
2075.766115	150.246570	47.771777
2072.217897	153.143736	47.776781
2069.170782	151.527899	47.781786
2065.500119	158.240514	47.786791
2062.039817	147.912304	47.791796
2058.277952	159.281760	47.796801
2054.775776	150.332961	47.801805
2051.270717	153.395268	47.806810
2047.733978	152.662344	47.811815
2044.565338	142.401863	47.816820
2040.726862	149.983343	47.821825
2036.887652	158.221289	47.826829
2033.549874	152.058880	47.831834
2030.565868	151.294576	47.836839
2026.995800	146.715602	47.841844
2023.480769	152.476368	47.846849
2019.979341	152.084533	47.851853
2016.377206	147.397414	47.856858
2012.660526	147.042041	47.861863
2009.218336	149.925045	47.866868
2005.708958	142.350748	47.871873
2002.372250	149.248628	47.876877
1999.305217	139.730501	47.881882
1995.270863	147.609299	47.886887
1991.829033	143.604470	47.891892
1988.261598	137.856479	47.896897
1984.388468	149.043536	47.901901
1981.219426	139.738676	47.906906
1977.887871	143.538149	47.911911
1974.584009	141.216042	47.916916
1971.050242	146.837279	47.921921
1967.268390	143.237506	47.926925
1963.824409	138.629411	47.931930
1960.123725	145.197108	47.936935
1957.085029	147.512061	47.941940
1953.498042	139.540020	47.946945
1949.919809	143.340529	47.951949
1946.530117	138.193017	47.956954
1942.543975	151.384423	47.961959
1939.185965	143.354123	47.966964
1935.624177	148.275547	47.971969
1932.123446	151.946210	47.976973
1928.961689	133.160807	47.981978
1925.150385	141.466440	47.986983
1921.701099	142.612563	47.991988
1918.448820	146.051044	47.996993
1914.851530	135.866453	48.001997
1911.501176	137.275419	48.007002
1907.689474	140.020234	48.012007
1904.428211	136.297744	48.017012
1900.934982	140.598659	48.022017
1897.009136	139.247177	48.027021
1894.084209	140.287087	48.032026
1890.220704	141.826301	48.037031
1886.611375	123.529726	48.042036
1883.364488	142.973164	48.047041
1879.373006	132.168792	48.052045
1876.447411	133.621057	48.057050
1872.817158	146.958567	48.062055
1869.524943	132.714604	48.067060
1865.961142	130.448890	48.072065
1862.138620	142.101654	48.077069
1859.259033	137.441950	48.082074
1854.936637	139.697207	48.087079
1851.721639	138.285383	48.092084
1848.287424	139.082945	48.097089
1844.644824	135.209993	48.102093
1840.911039	139.714810	48.107098
1837.375487	141.453690	48.112103
1834.320722	130.741972	48.117108
1830.911987	132.008336	48.122113
1827.370987	137.500643	48.127117
1824.110709	140.776140	48.132122
1820.369446	140.641889	48.137127
1816.700359	140.263217	48.142132
1813.185603	138.857496	48.147137
1809.350392	145.133064	48.152141
1806.294979	135.715201	48.157146
1802.876472	140.715597	48.162151
1799.029097	144.591627	48.167156
1795.663756	138.788218	48.172161
1791.884541	141.871116	48.177165
1788.800911	132.852222	48.182170
1785.362603	138.065087	48.187175
1781.606033	140.572562	48.192180
1778.160604	139.494797	48.197185
1774.598702	141.460099	48.202189
1771.198549	132.672075	48.207194
1767.383559	140.643377	48.212199
1764.371507	141.229939	48.217204
1760.942555	139.255136	48.222209
1757.443598	137.834414	48.227213
1753.707008	132.946054	48.232218
1750.073321	134.483812	48.237223
1746.646222	132.610935	48.242228
1743.081697	132.679524	48.247233
1739.596184	151.782941	48.252237
1736.306049	142.411146	48.257242
1732.802896	142.588761	48.262247
1729.048103	138.253215	48.267252
1725.726303	132.911915	48.272257
1722.201552	143.522841	48.277261
1718.894629	140.770477	48.282266
1714.959915	137.911824	48.287271
1711.536362	142.066959	48.292276
1708.391719	139.385185	48.297281
1704.684499	132.904843	48.302285
1701.022115	128.860667	48.307290
1697.243771	135.306675	48.312295
1693.945387	133.641019	48.317300
1690.779760	127.811706	48.322305
1687.133132	138.869497	48.327309
1683.941184	120.052849	48.332314
1680.066908	134.682046	48.337319
1676.443028	120.299481	48.342324
1672.861863	125.285895	48.347329
1669.355204	126.959743	48.352333
1666.633430	128.803030	48.357338
1662.891811	126.527512	48.362343
1659.531371	133.491144	48.367348
1655.806875	130.262234	48.372353
1652.184929	132.537346	48.377357
1648.465549	132.017192	48.382362
1644.850311	133.614144	48.387367
1641.428161	137.214592	48.392372
1638.029716	133.587098	48.397377
1634.437081	132.181621	48.402381
1631.095657	132.718892	48.407386
1627.716698	132.720706	48.412391
1624.252052	123.649095	48.417396
1620.837858	128.592085	48.422401
1617.040088	129.609363	48.427405
1613.590022	130.245963	48.432410
1609.714870	140.514676	48.437415
1606.493896	141.552369	48.442420
1602.878175	131.066464	48.447425
1599.511270	137.603000	48.452429
1596.299760	128.442873	48.457434
1592.651445	134.560756	48.462439
1589.055208	130.401921	48.467444
1585.445210	134.724031	48.472449
1581.899598	127.185554	48.477453
1578.645512	122.307947	48.482458
1575.361358	129.584396	48.487463
1571.665698	127.651811	48.492468
1568.462176	118.093158	48.497473
1564.438758	124.156038	48.502477
1561.207040	120.482619	48.507482
1557.447529	129.921944	48.512487
1553.840765	121.771836	48.517492
1550.421105	119.955915	48.522497
1547.092958	133.329802	48.527501
1543.486496	126.568095	48.532506
1540.040993	126.938586	48.537511
1536.805709	125.470196	48.542516
1533.003709	124.881562	48.547521
1529.428135	132.519340	48.552525
1525.659370	127.045526	48.557530
1522.190494	132.682807	48.562535
1519.108109	135.695398	48.567540
1515.575548	121.961100	48.572545
1512.193369	128.040444	48.577549
1508.831859	123.905912	48.582554
1505.005165	122.197386	48.587559
1501.661495	130.268359	48.592564
1498.102476	123.023650	48.597569
1494.311706	125.011950	48.602573
1491.115761	117.174836	48.607578
1487.370334	124.638937	48.612583
1483.575667	127.645544	48.617588
1480.452212	117.369015	48.622593
1476.936328	127.804008	48.627597
1473.305429	122.311531	48.632602
1470.118127	125.605390	48.637607
1466.507352	125.878242	48.642612
1463.072748	118.978795	48.647617
1459.342078	122.189707	48.652621
1455.982051	123.508099	48.657626
1452.627842	123.749862	48.662631
1448.771503	122.680734	48.667636
1445.529970	111.701185	48.672641
1442.037027	128.399126	48.677645
1438.509273	124.253351	48.682650
1434.669027	127.017540	48.687655
1431.366480	118.531365	48.692660
1427.658752	113.243683	48.697665
1424.347414	125.996616	48.702669
1421.130899	116.556482	48.707674
1417.308226	117.391992	48.712679
1413.660694	118.830915	48.717684
1410.333151	117.518828	48.722689
1406.922547	121.660218	48.727693
1403.380345	122.844092	48.732698
1399.559873	129.526844	48.737703
1396.535072	119.833527	48.742708
1393.257735	120.468901	48.747713
1389.452258	132.427259	48.752717
1385.985599	121.575080	48.757722
1382.346669	114.166930	48.762727
1378.861979	123.285937	48.767732
1375.306181	111.172600	48.772737
1371.843320	122.166605	48.777741
1368.670495	117.365689	48.782746
1364.880810	116.806551	48.787751
1361.383330	116.952767	48.792756
1357.566414	124.032789	48.797761
1354.148778	126.930214	48.802765
1350.809718	110.981890	48.807770
1347.588720	123.857827	48.812775
1344.178125	119.352309	48.817780
1340.733549	117.305287	48.822785
1336.670550	125.647243	48.827789
1333.376773	115.073892	48.832794
1329.283627	112.666577	48.837799
1325.920368	119.540351	48.842804
1322.605454	117.094734	48.847809
1319.134310	125.467200	48.852813
1315.807620	111.471644	48.857818
1312.513741	118.602294	48.862823
1308.839512	106.264572	48.867828
1305.220454	109.406789	48.872833
1301.609142	123.755077	48.877837
1298.568078	118.722995	48.882842
1294.984475	121.195710	48.887847
1291.201128	131.981279	48.892852
1287.722661	111.624031	48.897857
1284.263487	129.818978	48.902861
1280.983061	110.941253	48.907866
1277.466208	127.268341	48.912871
1273.503956	118.253567	48.917876
1270.376748	120.781233	48.922881
1266.990056	117.993555	48.927885
1263.436327	118.682185	48.932890
1259.907019	120.009482	48.937895
1256.168094	127.227224	48.942900
1252.724205	119.414283	48.947905
1248.762323	131.010153	48.952909
1246.179954	116.634263	48.957914
1242.337227	115.060870	48.962919
1238.920546	116.817252	48.967924
1235.351059	124.076167	48.972929
1231.471942	123.113055	48.977933
1228.119161	122.381523	48.982938
1224.510938	118.673961	48.987943
1221.112144	121.811091	48.992948
1217.934154	121.290333	48.997953
1214.017364	125.520392	49.002957
1210.974513	114.469819	49.007962
1207.177369	121.637863	49.012967
1203.608203	115.399161	49.017972
1200.151984	114.243972	49.022977
1196.584074	123.189067	49.027981
1193.356571	120.348208	49.032986
1189.428074	117.994633	49.037991
1186.001990	118.034242	49.042996
1182.745772	113.204699	49.048001
1178.743210	118.197504	49.053005
1175.828338	116.752628	49.058010
1172.407749	118.022894	49.063015
1169.020123	120.698034	49.068020
1165.302027	113.641466	49.073025
1161.747653	127.078803	49.078029
1158.604719	119.959969	49.083034
1154.708571	109.122058	49.088039
1150.870397	112.579992	49.093044
1147.389364	109.625740	49.098049
1143.927159	116.960268	49.103053
1140.736769	109.945034	49.108058
1137.321646	116.171229	49.113063
1133.526848	105.639367	49.118068
1130.419832	101.400403	49.123073
1126.225202	117.807483	49.128077
1123.186787	110.045009	49.133082
1119.879023	115.371328	49.138087
1116.012971	115.641863	49.143092
1112.931169	113.978855	49.148097
1109.103140	118.057535	49.153101
1105.673503	105.449557	49.158106
1102.022352	115.096438	49.163111
1098.570850	114.469015	49.168116
1095.469326	107.983519	49.173121
1091.168954	115.808610	49.178125
1087.819166	109.926317	49.183130
1084.628731	111.267004	49.188135
1081.157647	114.973710	49.193140
1077.836698	108.396766	49.198145
1073.721950	115.170864	49.203149
1070.883545	104.383685	49.208154
1067.444019	123.143831	49.213159
1063.544106	114.651354	49.218164
1060.073282	115.544069	49.223169
1056.435561	110.289544	49.228173
1052.925180	110.964856	49.233178
1049.473054	122.535907	49.238183
1045.986490	112.700879	49.243188
1042.589863	111.508318	49.248193
1039.148363	114.028720	49.253197
1035.602997	109.803372	49.258202
1032.440290	115.355119	49.263207
1028.497245	116.889213	49.268212
1025.400272	111.645823	49.273217
1021.611735	122.822801	49.278221
1017.825805	118.775915	49.283226
1014.167398	119.385448	49.288231
1011.145176	121.326982	49.293236
1007.897598	121.316012	49.298241
1003.967916	120.773551	49.303245
1000.306054	119.994251	49.308250
997.202269	123.259423	49.313255
993.023592	120.623350	49.318260
990.138124	114.760391	49.323265
986.264914	120.895195	49.328269
982.761257	126.831136	49.333274
979.388481	113.502459	49.338279
975.898326	120.371125	49.343284
972.855562	116.565231	49.348289
969.185786	123.628683	49.353293
965.396650	113.000945	49.358298
961.847678	123.560822	49.363303
958.250370	114.080319	49.368308
954.874239	112.810434	49.373313
951.265019	115.338619	49.378317
948.179245	113.810788	49.383322
944.611862	98.244935	49.388327
941.119352	118.075209	49.393332
937.603503	115.455685	49.398337
933.673149	116.078459	49.403341
930.590398	113.007789	49.408346
927.259668	114.830291	49.413351
923.457768	106.311839	49.418356
919.888636	113.572732	49.423361
916.336417	115.212766	49.428365
912.755602	112.323244	49.433370
909.573093	116.428174	49.438375
905.826421	114.004066	49.443380
902.590559	104.658010	49.448385
898.776006	109.709471	49.453389
895.686585	105.811341	49.458394
891.693714	112.443833	49.463399
888.252168	108.462073	49.468404
884.839294	104.448721	49.473409
881.445835	112.018124	49.478413
877.605646	111.063117	49.483418
874.428199	107.347742	49.488423
871.059954	116.314030	49.493428
867.577062	107.597452	49.498433
863.859601	113.441500	49.503437
860.741941	105.317873	49.508442
857.080045	106.574199	49.513447
853.313956	101.765057	49.518452
849.963279	105.738500	49.523457
846.239361	115.360182	49.528461
842.357885	114.959464	49.533466
838.998037	111.019639	49.538471
835.852059	119.218143	49.543476
832.908075	108.788495	49.548481
829.146798	120.411424	49.553485
825.387188	114.878797	49.558490
822.103717	112.917392	49.563495
818.122025	120.396632	49.568500
814.991440	116.105013	49.573505
811.248414	116.692475	49.578509
807.504403	120.980085	49.583514
804.147680	115.890114	49.588519
801.066792	116.840283	49.593524
797.368147	119.412461	49.598529
793.892115	109.114777	49.603533
790.468089	114.704562	49.608538
786.646451	113.694275	49.613543
782.979141	110.930926	49.618548
780.185838	114.963455	49.623553
776.428008	111.066075	49.628557
772.554432	109.715541	49.633562
769.506064	116.739352	49.638567
765.748967	104.870432	49.643572
762.607393	106.160645	49.648577
758.718648	109.028447	49.653581
755.127620	113.548818	49.658586
751.603292	105.110766	49.663591
748.109363	112.423848	49.668596
744.774195	104.305652	49.673601
741.300369	118.708308	49.678605
738.216451	105.267798	49.683610
734.198605	110.344087	49.688615
730.627222	106.862167	49.693620
727.671167	100.608589	49.698625
723.612301	105.712615	49.703629
720.165843	96.436035	49.708634
716.793221	105.344360	49.713639
712.975455	104.134003	49.718644
709.567681	94.890281	49.723649
706.149636	109.002102	49.728653
702.609964	107.380916	49.733658
699.266374	103.740441	49.738663
695.868032	114.743197	49.743668
692.447622	108.655540	49.748673
688.569112	111.860136	49.753677
685.229950	106.567466	49.758682
681.764738	103.958526	49.763687
678.615737	110.642135	49.768692
675.025368	102.904605	49.773697
671.260269	103.870799	49.778701
667.653242	103.824487	49.783706
664.032153	108.378346	49.788711
660.397167	110.235213	49.793716
657.088025	103.214484	49.798721
653.378609	102.578194	49.803725
650.388112	99.897567	49.808730
647.071555	94.631574	49.813735
642.948801	101.861092	49.818740
639.812500	94.056695	49.823745
635.799305	107.722160	49.828749
632.472871	96.546351	49.833754
629.138917	104.230393	49.838759
625.653992	107.732197	49.843764
622.229052	100.850314	49.848769
618.871004	106.584387	49.853773
615.357104	106.420444	49.858778
611.880252	103.878030	49.863783
607.705187	102.925230	49.868788
604.181222	104.264071	49.873793
600.833562	105.519965	49.878797
597.532025	113.371319	49.883802
593.986960	104.723358	49.888807
590.824020	113.335504	49.893812
587.630127	105.367257	49.898817
583.901751	109.785086	49.903821
580.380034	100.131806	49.908826
576.979929	106.940660	49.913831
572.703644	112.378127	49.918836
569.295244	105.089214	49.923841
565.963992	107.808391	49.928845
562.568102	107.380603	49.933850
559.220781	108.389615	49.938855
555.605653	108.963588	49.943860
552.044368	107.153143	49.948865
548.509382	114.594375	49.953869
544.907611	103.435957	49.958874
541.812539	101.825155	49.963879
538.120942	108.687776	49.968884
534.731019	104.376918	49.973889
531.152827	117.315106	49.978893
527.698442	106.522747	49.983898
524.200101	101.453800	49.988903
520.435145	103.679884	49.993908
516.750824	93.652899	49.998913
513.379817	100.213266	50.003917
510.152586	99.650760	50.008922
506.514526	97.966577	50.013927
502.920080	102.494450	50.018932
500.006749	101.286840	50.023937
496.293735	100.994659	50.028941
491.939914	107.093322	50.033946
488.644946	107.038965	50.038951
485.288979	112.290725	50.043956
481.932968	99.306303	50.048961
478.612139	104.003057	50.053965
475.447892	100.048255	50.058970
472.047769	103.631619	50.063975
467.936488	105.271381	50.068980
464.494347	102.182852	50.073985
460.554797	112.055380	50.078989
457.454810	98.761868	50.083994
454.031339	96.983883	50.088999
450.703894	100.524608	50.094004
447.296193	94.416141	50.099009
443.169750	98.011830	50.104013
439.794819	96.392739	50.109018
436.466727	100.213793	50.114023
432.994593	100.017036	50.119028
429.523058	94.540585	50.124033
425.621368	102.657512	50.129037
422.364446	109.917886	50.134042
419.089312	103.116695	50.139047
415.363344	108.156270	50.144052
412.228492	99.189360	50.149057
408.508902	108.706907	50.154061
404.907074	97.627390	50.159066
401.412023	105.136899	50.164071
397.798213	102.682558	50.169076
394.617620	102.253892	50.174081
390.939526	107.536544	50.179085
387.173304	108.286339	50.184090
384.029237	102.871960	50.189095
380.325008	107.797847	50.194100
376.909368	103.854501	50.199105
373.419886	93.877990	50.204109
369.950440	104.826305	50.209114
366.429257	100.880769	50.214119
362.826807	103.127372	50.219124
359.344635	104.421017	50.224129
355.623208	102.317296	50.229133
352.130685	100.169633	50.234138
349.072598	100.893197	50.239143
345.375905	108.023633	50.244148
342.152231	101.282835	50.249153
338.379995	107.184218	50.254157
335.081371	102.927648	50.259162
331.379223	111.268249	50.264167
327.774291	101.133164	50.269172
324.554156	108.241282	50.274177
320.961297	108.967671	50.279181
317.658739	115.501049	50.284186
313.678311	107.873683	50.289191
310.016505	102.953660	50.294196
306.835340	92.128979	50.299201
303.063155	109.208004	50.304205
300.005442	93.119141	50.309210
296.907032	105.528481	50.314215
292.881666	99.594606	50.319220
289.920873	97.732806	50.324225
285.968402	111.707395	50.329229
281.926962	108.783131	50.334234
278.823920	100.579467	50.339239
274.781916	108.997103	50.344244
271.736436	99.759735	50.349249
268.198650	105.196788	50.354253
264.620258	95.559178	50.359258
261.393633	99.610779	50.364263
257.839046	107.179637	50.369268
254.180974	98.746759	50.374273
250.953057	100.902234	50.379277
247.603621	107.655388	50.384282
243.975918	91.576826	50.389287
240.046120	98.382995	50.394292
236.817149	98.707624	50.399297
233.139075	108.487985	50.404301
229.208858	101.929805	50.409306
226.514936	96.528986	50.414311
222.698686	110.534278	50.419316
219.264398	97.790266	50.424321
215.703585	104.946786	50.429325
212.105523	105.706112	50.434330
208.849739	95.060471	50.439335
205.081064	99.253094	50.444340
202.009918	93.103946	50.449345
198.580207	100.581458	50.454349
195.147366	98.209927	50.459354
191.174917	96.594447	50.464359
187.521267	96.746573	50.469364
184.093718	95.004645	50.474369
180.577341	102.084154	50.479373
176.973241	94.594909	50.484378
174.112106	89.840946	50.489383
170.301817	96.603251	50.494388
166.789589	89.524594	50.499393
163.064521	92.632586	50.504397
159.831639	96.957232	50.509402
156.089439	94.632212	50.514407
152.688490	99.548960	50.519412
149.612263	97.114071	50.524417
145.728136	107.671304	50.529421
141.961428	102.709098	50.534426
138.444615	100.278562	50.539431
135.183200	108.943920	50.544436
131.398374	94.743545	50.549441
127.790380	100.178378	50.554445
124.424061	96.922870	50.559450
121.281910	99.027105	50.564455
117.765904	99.859515	50.569460
114.358547	90.427287	50.574465
110.700186	102.472595	50.579469
107.059068	102.243645	50.584474
103.572838	100.881343	50.589479
100.134064	102.765138	50.594484
96.765797	103.937091	50.599489
93.505715	98.713147	50.604493
89.528953	103.428070	50.609498
86.466476	104.895923	50.614503
82.643714	100.027357	50.619508
79.296117	97.231521	50.624513
75.482490	91.540553	50.629517
71.856536	101.417372	50.634522
68.627583	97.329046	50.639527
64.813757	104.758231	50.644532
61.777967	99.992931	50.649537
57.921843	99.278022	50.654541
54.612383	97.544218	50.659546
51.503095	106.098124	50.664551
47.770162	93.698943	50.669556
44.240131	93.211048	50.674561
40.416953	98.410594	50.679565
36.931615	102.577209	50.684570
33.694472	94.041266	50.689575
29.906052	99.606026	50.694580
26.527468	100.666885	50.699585
23.145641	100.999741	50.704589
19.418093	96.400366	50.709594
15.925931	97.206414	50.714599
12.296373	103.635143	50.719604
9.223939	89.131614	50.724609
5.574511	94.931206	50.729613
2.253969	100.382905	50.734618