Fri Jun 17 17:57:26 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.171738	79.571263	0.000000
0.968129	88.832893	0.005005
1.065545	92.490435	0.010010
1.137177	74.276641	0.015014
0.674104	69.562481	0.020019
0.629893	60.006868	0.025024
0.264412	55.784022	0.030029
-0.052381	44.155000	0.035034
-0.319146	38.082559	0.040038
-1.077500	33.472745	0.045043
-1.201815	22.774317	0.050048
-1.083719	14.878525	0.055053
-1.641268	23.469225	0.060058
-1.705642	9.051447	0.065062
-1.968388	14.760284	0.070067
-1.947595	12.955052	0.075072
-2.618660	1.163745	0.080077
-3.245204	1.680149	0.085082
-3.143743	3.032391	0.090086
-3.567523	3.567187	0.095091
-3.582033	-8.236754	0.100096
-4.222997	3.604983	0.105101
-4.830325	-7.437195	0.110106
-4.989831	-0.543200	0.115110
-5.308270	5.012685	0.120115
-4.988743	-0.856663	0.125120
-5.206602	1.294561	0.130125
-4.910764	13.451413	0.135130
-5.601610	2.617480	0.140134
-6.399491	8.483740	0.145139
-6.637938	10.885246	0.150144
-6.620252	8.044949	0.155149
-7.213389	9.329923	0.160154
-6.494435	8.570910	0.165158
-7.243178	8.264046	0.170163
-7.863610	9.435555	0.175168
-8.164652	11.610277	0.180173
-8.348472	5.581880	0.185178
-8.447005	-5.249076	0.190182
-8.532383	9.928312	0.195187
-8.614381	-0.114107	0.200192
-8.534444	2.900658	0.205197
-9.676726	-3.762862	0.210202
-9.867993	4.684066	0.215206
-10.035458	6.737919	0.220211
-10.153444	9.750657	0.225216
-10.255522	-2.726226	0.230221
-10.402182	3.216483	0.235226
-11.128365	-0.938692	0.240230
-11.929743	6.756205	0.245235
-11.884218	-0.301891	0.250240
-11.293691	3.038445	0.255245
-11.770320	10.303647	0.260250
-11.581167	7.666710	0.265254
-12.107900	6.306895	0.270259
-12.280220	-1.189171	0.275264
-12.820818	-4.825434	0.280269
-13.330892	8.776825	0.285274
-13.176924	2.023730	0.290278
-13.288934	6.833142	0.295283
-13.811863	11.840506	0.300288
-14.326385	-2.268400	0.305293
-14.874041	3.841405	0.310298
-14.497165	-5.045361	0.315302
-14.628323	2.297384	0.320307
-14.803082	-5.326341	0.325312
-15.389736	-7.439856	0.330317
-16.276122	7.222453	0.335322
-16.177588	-2.951597	0.340326
-16.332265	-1.761803	0.345331
-16.476079	4.661126	0.350336
-16.421805	-2.575033	0.355341
-16.634808	6.595957	0.360346
-16.415299	-2.165002	0.365350
-17.271981	-0.280342	0.370355
-17.528931	3.381225	0.375360
-17.657704	-4.369528	0.380365
-18.162959	5.461563	0.385370
-18.949038	-3.593001	0.390374
-19.562951	1.484342	0.395379
-18.535846	2.054617	0.400384
-18.824835	5.456893	0.405389
-19.432545	4.643329	0.410394
-19.439495	-5.532325	0.415398
-19.390922	5.120140	0.420403
-20.182481	1.825533	0.425408
-20.463694	1.742672	0.430413
-21.211161	3.426057	0.435418
-21.132515	-6.286881	0.440422
-21.432430	8.570382	0.445427
-21.071978	-1.612279	0.450432
-21.149025	-0.643374	0.455437
-21.941479	2.533968	0.460442
-22.333644	-6.161224	0.465446
-22.681877	0.883132	0.470451
-22.728521	4.914265	0.475456
-22.676609	-0.660780	0.480461
-22.873075	-3.454623	0.485466
-23.080380	-7.051175	0.490470
-23.749181	-1.088962	0.495475
-24.031739	0.557002	0.500480
-23.987838	-2.449855	0.505485
-24.152013	-2.489223	0.510490
-24.449229	-9.895260	0.515494
-25.703218	-4.723161	0.520499
-25.926701	-0.390517	0.525504
-25.066264	-7.335634	0.530509
-25.596498	2.415546	0.535514
-25.567743	-5.394740	0.540518
-26.011419	-2.701014	0.545523
-25.973577	-2.908739	0.550528
-26.735898	-6.114866	0.555533
-27.209658	-1.854872	0.560538
-27.165927	-4.286684	0.565542
-27.461422	4.528814	0.570547
-27.469614	1.020718	0.575552
-27.304031	3.127344	0.580557
-28.574091	-0.174149	0.585562
-28.692944	-7.949635	0.590566
-29.029547	1.908474	0.595571
-28.740278	-1.566585	0.600576
-28.645243	-0.069226	0.605581
-29.361982	5.191363	0.610586
-29.826291	2.161046	0.615590
-30.564819	0.251559	0.620595
-30.668936	-1.777396	0.625600
-30.617417	0.576303	0.630605
-30.850499	2.237920	0.635610
-30.674855	-2.929093	0.640614
-30.822155	-0.456112	0.645619
-31.074501	2.641711	0.650624
-31.501534	-10.607756	0.655629
-32.097153	7.330816	0.660634
-32.194022	2.933693	0.665638
-32.040561	-0.205038	0.670643
-32.158403	3.890222	0.675648
-32.906728	4.718725	0.680653
-33.595149	9.207196	0.685658
-33.598739	9.253020	0.690662
-34.272901	4.900950	0.695667
-34.068388	7.023995	0.700672
-33.956506	3.086086	0.705677
-34.140475	12.955927	0.710682
-34.121931	2.751563	0.715686
-34.713848	9.035867	0.720691
-35.228309	0.037778	0.725696
-35.432703	4.492949	0.730701
-35.567369	-5.790526	0.735706
-36.178198	1.405027	0.740710
-36.737071	2.290046	0.745715
-36.977038	2.913280	0.750720
-36.664213	-2.781108	0.755725
-37.112729	1.869349	0.760730
-36.959237	-6.745264	0.765734
-37.299784	-5.559105	0.770739
-37.197603	11.576967	0.775744
-37.667014	-0.276660	0.780749
-38.197708	9.274115	0.785754
-38.480018	-5.366903	0.790758
-38.734320	4.857780	0.795763
-38.922373	-2.041904	0.800768
-38.745922	4.952924	0.805773
-39.549811	8.038835	0.810778
-39.757199	2.685082	0.815782
-40.105236	4.703044	0.820787
-40.055569	2.522037	0.825792
-40.019308	-4.862082	0.830797
-40.762385	10.395824	0.835802
-41.084706	-0.711485	0.840806
-41.557219	9.375035	0.845811
-41.888568	4.294272	0.850816
-41.638899	-1.730207	0.855821
-41.940741	1.748993	0.860826
-42.214958	-0.585567	0.865830
-42.109811	10.776364	0.870835
-42.600605	3.591939	0.875840
-43.073913	-1.377609	0.880845
-43.571242	5.172756	0.885850
-43.363186	3.823405	0.890854
-43.494240	-5.862170	0.895859
-43.640053	0.434207	0.900864
-44.336598	-3.113969	0.905869
-44.731158	1.149240	0.910874
-44.917844	-7.810387	0.915878
-44.906079	6.289215	0.920883
-45.265342	3.642213	0.925888
-44.857903	5.756585	0.930893
-45.780263	4.670726	0.935898
-46.525591	-4.052382	0.940902
-46.788349	-12.893000	0.945907
-46.776979	4.994195	0.950912
-46.681002	-5.476997	0.955917
-46.867969	-1.569945	0.960922
-46.690323	-10.432469	0.965926
-46.905590	-2.877825	0.970931
-47.567059	1.049106	0.975936
-47.973671	-0.654487	0.980941
-48.402762	3.952093	0.985946
-48.371959	0.369239	0.990950
-48.134107	2.665916	0.995955
-48.942420	7.100715	1.000960
-49.375794	-0.616568	1.005965
-49.719850	6.562662	1.010970
-49.622088	-1.513256	1.015974
-50.017454	4.308394	1.020979
-49.958359	1.554947	1.025984
-50.125894	-1.010067	1.030989
-51.031426	11.680761	1.035994
-51.209037	1.739290	1.040998
-51.426013	-0.865653	1.046003
-51.394576	-1.582803	1.051008
-51.377022	5.977344	1.056013
-51.644863	15.056420	1.061018
-51.921145	4.075443	1.066022
-52.550689	11.012059	1.071027
-52.895230	8.090888	1.076032
-52.509461	4.418439	1.081037
-53.736189	16.446362	1.086042
-54.295658	14.494878	1.091046
-53.853231	8.535832	1.096051
-54.026311	19.482072	1.101056
-54.191818	8.428805	1.106061
-54.488520	10.532559	1.111066
-54.792645	0.919559	1.116070
-54.894586	8.054989	1.121075
-54.947406	7.742359	1.126080
-55.406805	5.353338	1.131085
-56.154034	3.084980	1.136090
-55.867635	-2.808461	1.141094
-56.295060	5.045679	1.146099
-56.628194	7.178774	1.151104
-56.260265	5.008596	1.156109
-56.507218	2.225515	1.161114
-57.104089	-7.464907	1.166118
-57.394659	0.664447	1.171123
-57.830089	-3.905490	1.176128
-57.732438	-5.759014	1.181133
-58.546263	1.676496	1.186138
-58.824636	-1.335393	1.191142
-59.393754	3.704909	1.196147
-59.307847	0.506764	1.201152
-59.204844	-2.441444	1.206157
-59.741673	6.621171	1.211162
-59.827098	6.915223	1.216166
-59.449530	4.482179	1.221171
-60.024483	13.902185	1.226176
-60.034030	-0.944012	1.231181
-60.937840	13.682526	1.236186
-61.030437	7.304695	1.241190
-61.227709	-2.810113	1.246195
-61.390623	2.948031	1.251200
-62.054909	2.301151	1.256205
-62.472809	-2.019315	1.261210
-62.878557	8.097940	1.266214
-62.448318	9.408350	1.271219
-62.793858	8.351712	1.276224
-62.817444	-8.187200	1.281229
-63.079953	8.469005	1.286234
-62.657625	-0.559701	1.291238
-63.354266	2.535616	1.296243
-63.737920	2.143011	1.301248
-64.081142	-4.334637	1.306253
-64.358482	2.264009	1.311258
-64.940773	-3.641897	1.316262
-65.629203	2.654308	1.321267
-65.494074	-1.137692	1.326272
-65.713244	4.712880	1.331277
-65.623401	4.156907	1.336282
-65.599969	8.548355	1.341286
-65.413963	3.572605	1.346291
-66.668193	0.325918	1.351296
-66.907462	-5.784613	1.356301
-67.362899	0.544489	1.361306
-67.402147	2.317540	1.366310
-67.427805	7.098191	1.371315
-67.564575	-2.508291	1.376320
-67.935108	1.153019	1.381325
-68.797027	7.225486	1.386330
-68.828680	-6.974131	1.391334
-69.265012	2.626270	1.396339
-69.303770	-0.807481	1.401344
-69.297472	4.030607	1.406349
-69.277239	5.613215	1.411354
-69.610097	-5.069064	1.416358
-69.666178	-2.348996	1.421363
-70.458885	1.241998	1.426368
-70.464697	-3.317070	1.431373
-70.986489	3.108704	1.436378
-70.864147	-3.639721	1.441382
-70.712284	0.054325	1.446387
-71.029633	6.378825	1.451392
-72.006477	4.509163	1.456397
-72.237440	15.485544	1.461402
-72.313968	1.351986	1.466406
-72.506331	2.953952	1.471411
-72.481758	2.106916	1.476416
-73.283681	9.477505	1.481421
-73.723351	1.508888	1.486426
-73.879404	3.907552	1.491430
-73.939163	0.723164	1.496435
-74.418308	8.879530	1.501440
-74.087810	-2.010311	1.506445
-74.237975	12.832911	1.511450
-74.140186	0.231446	1.516454
-74.845246	2.761633	1.521459
-75.780631	5.716678	1.526464
-75.563460	-4.400722	1.531469
-75.542377	4.183761	1.536474
-75.765997	3.404033	1.541478
-76.026145	0.884806	1.546483
-76.789938	5.995559	1.551488
-76.783063	-6.623346	1.556493
-77.453633	9.359728	1.561498
-77.281378	3.513675	1.566502
-77.222672	-7.913691	1.571507
-77.312167	12.592648	1.576512
-77.584099	-7.783478	1.581517
-78.497247	0.406358	1.586522
-78.623316	0.432682	1.591526
-78.693016	13.588192	1.596531
-79.121205	9.612788	1.601536
-79.661015	-9.238439	1.606541
-80.223974	4.435160	1.611546
-80.219151	-3.160989	1.616550
-80.240000	-2.793610	1.621555
-80.259370	3.942904	1.626560
-80.310541	-6.828428	1.631565
-80.445452	2.130666	1.636570
-80.532273	-4.373028	1.641574
-81.270376	-5.308756	1.646579
-81.345926	6.825754	1.651584
-81.239934	2.517846	1.656589
-82.053141	0.898822	1.661594
-82.285851	-4.911082	1.666598
-82.948955	-1.163246	1.671603
-83.505035	2.741828	1.676608
-83.535832	-10.516666	1.681613
-83.509811	2.064479	1.686618
-83.622284	-1.921376	1.691622
-83.461812	-2.998199	1.696627
-83.652889	2.734238	1.701632
-83.541340	-8.082496	1.706637
-84.380059	6.009703	1.711642
-84.732198	2.266347	1.716646
-85.110893	5.914215	1.721651
-85.350984	6.192146	1.726656
-85.146577	-9.476950	1.731661
-86.031763	4.242128	1.736666
-86.338311	4.448821	1.741670
-86.726950	-2.660027	1.746675
-86.919831	8.042242	1.751680
-86.857115	-0.854261	1.756685
-87.217166	2.932979	1.761690
-86.935992	2.962245	1.766694
-87.087044	3.541692	1.771699
-88.079355	9.305709	1.776704
-88.053026	2.604816	1.781709
-88.650689	6.723606	1.786714
-88.286823	-5.660034	1.791718
-88.431485	10.111687	1.796723
-88.972312	4.964921	1.801728
-89.203697	-1.561113	1.806733
-89.858115	-0.411568	1.811738
-89.685110	1.516422	1.816742
-89.888016	-0.965750	1.821747
-90.147981	-0.537900	1.826752
-90.543598	-7.902112	1.831757
-90.991185	-1.253458	1.836762
-91.469950	-2.846977	1.841766
-91.554063	8.557656	1.846771
-91.603196	2.356909	1.851776
-91.773379	-3.784049	1.856781
-91.656840	12.267869	1.861786
-92.123459	3.434699	1.866790
-92.696915	1.189358	1.871795
-93.215315	-6.666708	1.876800
-92.933841	0.225997	1.881805
-92.841115	10.904860	1.886810
-93.637110	7.208063	1.891814
-94.406353	5.073808	1.896819
-94.690159	5.602708	1.901824
-94.355452	10.595960	1.906829
-94.659439	9.178013	1.911834
-94.505988	11.070775	1.916838
-94.782064	0.844557	1.921843
-95.033459	-3.731105	1.926848
-95.616477	-0.081630	1.931853
-96.040735	9.184466	1.936858
-96.301316	-0.281650	1.941862
-96.377324	3.310569	1.946867
-96.440695	-6.824320	1.951872
-96.448792	-5.686717	1.956877
-97.459950	0.659395	1.961882
-97.411399	0.783178	1.966886
-97.811257	-3.636184	1.971891
-98.067762	4.002671	1.976896
-98.097790	-13.285797	1.981901
-98.328479	3.066156	1.986906
-98.146209	-3.317504	1.991910
-98.491170	-0.993992	1.996915
-99.135656	0.650423	2.006912
-98.970200	-4.469670	2.016909
-98.357397	3.181033	2.026906
-98.311839	-9.597734	2.036902
-97.301823	-2.283757	2.046899
-96.833442	-2.801760	2.056896
-95.990836	0.528160	2.066893
-95.543122	2.594007	2.076890
-95.519600	2.132179	2.086886
-95.167601	2.359242	2.096883
-94.264732	-2.914466	2.106880
-94.073434	7.732299	2.116877
-92.852814	5.686606	2.126874
-92.459214	8.661237	2.136870
-92.556251	6.003772	2.146867
-92.154076	6.522027	2.156864
-90.959385	1.320526	2.166861
-91.191451	6.894430	2.176858
-90.521669	2.009982	2.186854
-89.610378	7.001804	2.196851
-89.360548	6.877955	2.206848
-88.742278	-2.321210	2.216845
-88.051202	3.330987	2.226842
-87.900754	-0.106181	2.236838
-87.344069	-3.790486	2.246835
-86.534430	4.860453	2.256832
-86.604414	0.800996	2.266829
-85.788845	-1.122823	2.276826
-85.054081	-4.175229	2.286822
-85.050212	-7.106719	2.296819
-84.204728	4.085679	2.306816
-83.407233	2.744372	2.316813
-83.370514	4.958963	2.326810
-83.036553	1.583162	2.336806
-82.058032	-1.992657	2.346803
-81.769964	4.143436	2.356800
-81.391806	5.010662	2.366797
-80.480794	2.198259	2.376794
-79.936751	7.488631	2.386790
-80.069221	5.183416	2.396787
-79.624237	-5.471369	2.406784
-78.839581	-7.443197	2.416781
-78.426692	1.158312	2.426778
-77.599939	4.062714	2.436774
-77.372593	-2.838987	2.446771
-76.849473	2.238115	2.456768
-76.128490	3.521755	2.466765
-75.874237	2.793362	2.476762
-75.420733	-0.318386	2.486758
-74.242501	3.313169	2.496755
-74.016493	0.043635	2.506752
-74.040088	3.599557	2.516749
-73.165871	4.869578	2.526746
-72.669720	2.931289	2.536742
-72.686123	4.531540	2.546739
-71.690586	0.492529	2.556736
-71.247274	3.899703	2.566733
-70.956188	4.532255	2.576730
-69.864963	3.371907	2.586726
-69.553287	3.147879	2.596723
-69.223762	0.467513	2.606720
-68.985236	-0.365946	2.616717
-67.832804	-4.195125	2.626714
-67.449339	-5.893585	2.636710
-67.405689	-2.997503	2.646707
-67.242382	-4.177068	2.656704
-66.259750	-2.026666	2.666701
-65.782284	-3.723958	2.676698
-64.571361	2.210709	2.686694
-64.821206	2.735011	2.696691
-64.471015	-1.546237	2.706688
-63.988386	2.671797	2.716685
-63.149650	0.301350	2.726682
-63.213414	5.323487	2.736678
-61.819959	0.088359	2.746675
-61.388964	-5.265753	2.756672
-61.330687	3.251860	2.766669
-60.760852	-4.575739	2.776666
-59.941780	-3.632634	2.786662
-59.722601	2.833810	2.796659
-59.557819	-2.164461	2.806656
-58.612730	-0.542866	2.816653
-58.123288	-1.192991	2.826650
-57.967350	6.572200	2.836646
-57.150461	3.498440	2.846643
-57.007480	4.709237	2.856640
-55.900336	1.601847	2.866637
-55.340498	3.839134	2.876634
-54.996049	2.221055	2.886630
-55.103950	2.897806	2.896627
-54.557509	1.167511	2.906624
-53.809549	-0.274225	2.916621
-53.380918	5.330721	2.926618
-52.514975	1.097697	2.936614
-52.260559	2.093573	2.946611
-51.560789	4.702171	2.956608
-50.952279	9.222921	2.966605
-50.924687	4.200429	2.976602
-50.457420	4.926986	2.986598
-49.414863	4.257031	2.996595
-49.056246	0.671056	3.006592
-48.904263	3.582918	3.016589
-48.148537	8.935712	3.026586
-47.701400	1.212875	3.036582
-47.161786	2.837664	3.046579
-46.429832	5.258149	3.056576
-46.135305	3.937234	3.066573
-46.076406	11.521770	3.076570
-45.331496	0.067497	3.086566
-44.635507	-6.242306	3.096563
-44.016967	-0.591873	3.106560
-43.385619	1.624836	3.116557
-43.038283	5.570375	3.126554
-42.764139	-0.629591	3.136550
-42.371226	3.246133	3.146547
-41.624442	1.433140	3.156544
-41.583810	6.356915	3.166541
-40.496255	2.742629	3.176538
-39.954606	0.042019	3.186534
-39.842475	-0.207518	3.196531
-38.896109	-0.032229	3.206528
-38.246860	4.153567	3.216525
-38.378543	5.715485	3.226522
-37.981319	4.671501	3.236518
-37.033848	6.701701	3.246515
-36.553268	3.925294	3.256512
-36.503542	0.181626	3.266509
-35.265433	2.295497	3.276506
-34.997174	5.670724	3.286502
-35.130943	3.681655	3.296499
-33.829997	0.671273	3.306496
-33.571334	7.092433	3.316493
-33.514632	8.750476	3.326490
-32.436128	11.264706	3.336486
-31.889569	8.508154	3.346483
-31.934015	5.641595	3.356480
-31.122537	9.362388	3.366477
-30.261498	11.456749	3.376474
-30.074561	7.426498	3.386470
-29.913574	0.236292	3.396467
-29.299779	-0.894470	3.406464
-29.052465	5.165421	3.416461
-27.977507	2.555960	3.426458
-26.972040	9.106676	3.436454
-27.275241	-0.960808	3.446451
-26.939083	-4.302986	3.456448
-26.085159	4.132755	3.466445
-25.556999	4.371638	3.476442
-25.417087	1.971154	3.486438
-24.578106	1.757081	3.496435
-24.409058	4.080279	3.506432
-23.572669	5.565444	3.516429
-22.903823	6.342272	3.526426
-22.902450	5.277154	3.536422
-21.581169	11.206735	3.546419
-21.491166	3.938229	3.556416
-21.452076	7.052611	3.566413
-20.758248	4.167456	3.576410
-19.490647	4.255169	3.586406
-19.271513	6.399727	3.596403
-19.272042	1.508756	3.606400
-19.088149	1.152650	3.616397
-18.003548	0.319230	3.626394
-17.472822	0.223380	3.636390
-17.312400	2.530822	3.646387
-16.187008	5.072629	3.656384
-15.828750	3.415902	3.666381
-15.868105	6.243197	3.676378
-15.681204	4.210110	3.686374
-14.836857	10.952199	3.696371
-13.565626	5.289484	3.706368
-13.300532	2.972713	3.716365
-12.797337	-1.384152	3.726362
-12.724519	2.378025	3.736358
-12.615952	-1.387674	3.746355
-11.653780	-6.081046	3.756352
-11.161431	-1.025688	3.766349
-10.406077	-3.474731	3.776346
-10.028961	-3.977750	3.786342
-9.833099	-2.330787	3.796339
-8.909155	-3.701989	3.806336
-8.205750	-0.255649	3.816333
-8.109503	2.509786	3.826330
-7.800999	5.669087	3.836326
-7.208834	6.128307	3.846323
-6.521891	2.901889	3.856320
-6.119985	5.420516	3.866317
-5.185022	6.231354	3.876314
-4.983605	10.969945	3.886310
-4.652222	5.986458	3.896307
-4.430103	9.068243	3.906304
-4.025313	4.668461	3.916301
-3.547558	17.815844	3.926298
-2.987929	37.247756	3.936294
-2.409744	51.248033	3.946291
-2.039786	64.172521	3.956288
-1.750132	74.505834	3.966285
-1.172142	97.752266	3.976282
-0.908237	117.712576	3.986278
0.000000	125.282729	3.991283
-0.193000	139.529566	3.996288
0.196043	141.608344	4.001293
0.333866	152.317709	4.006298
0.622955	167.378150	4.011302
0.937944	171.591736	4.016307
0.326474	163.286120	4.021312
0.608886	162.939864	4.026317
0.958515	175.606885	4.031322
0.813227	178.179804	4.036326
0.618357	180.900873	4.041331
0.614985	176.787312	4.046336
0.886156	180.073425	4.051341
1.037443	189.207847	4.056346
0.646126	183.610703	4.061350
0.957265	169.728863	4.066355
0.852271	171.870032	4.071360
0.430817	163.441072	4.076365
0.707538	176.184148	4.081370
0.831400	177.736919	4.086374
0.847414	184.131975	4.091379
0.903769	186.192257	4.096384
0.948154	186.291477	4.101389
0.908982	177.395620	4.106394
0.806704	188.820780	4.111398
1.092173	171.081429	4.116403
0.906270	179.359829	4.121408
0.925331	182.094277	4.126413
0.916823	184.485807	4.131418
1.066647	191.050232	4.136422
0.873748	182.172426	4.141427
0.779175	185.751200	4.146432
0.949171	191.742182	4.151437
0.886647	181.539331	4.156442
0.715760	176.318762	4.161446
0.964344	183.516974	4.166451
1.056988	190.896016	4.171456
0.587417	180.075296	4.176461
1.062321	189.574071	4.181466
1.149077	194.386811	4.186470
1.014224	181.788342	4.191475
0.797324	188.855351	4.196480
0.942659	186.588362	4.201485
1.246158	199.597351	4.206490
1.128679	218.101371	4.211494
1.166370	211.114336	4.216499
1.126770	218.819263	4.221504
1.555100	209.872910	4.226509
1.318804	190.493417	4.231514
1.130491	185.193848	4.236518
1.214297	181.714817	4.241523
1.232122	196.850766	4.246528
1.126616	199.767143	4.251533
1.445290	201.907748	4.256538
1.046089	200.279459	4.261542
1.553790	199.010327	4.266547
0.975150	207.001786	4.271552
1.324515	210.498880	4.276557
1.359274	206.358252	4.281562
1.364555	214.018619	4.286566
1.476408	208.245082	4.291571
1.494830	209.715337	4.296576
1.407045	216.089969	4.301581
1.722607	208.909931	4.306586
1.165013	215.002723	4.311590
1.327199	198.690611	4.316595
1.379967	215.120198	4.321600
1.309086	218.854486	4.326605
1.732225	220.006857	4.331610
1.660298	218.306208	4.336614
1.780742	209.407481	4.341619
1.399672	195.619563	4.346624
1.390504	196.777685	4.351629
1.508702	184.580949	4.356634
1.333470	204.766148	4.361638
1.513268	209.945658	4.366643
1.783249	208.974150	4.371648
1.539913	214.618857	4.376653
1.462795	202.278750	4.381658
1.598544	216.132195	4.386662
1.996526	203.717061	4.391667
1.519816	207.538931	4.396672
1.341164	216.314210	4.401677
1.565115	219.999293	4.406682
1.561661	218.881034	4.411686
2.069407	214.357498	4.416691
1.579203	219.798945	4.421696
1.566674	207.864862	4.426701
1.658992	219.884227	4.431706
1.330675	222.522110	4.436710
1.866254	209.005090	4.441715
1.501759	228.170593	4.446720
1.506499	221.975792	4.451725
1.553875	224.241811	4.456730
1.362731	223.550400	4.461734
1.549131	214.578941	4.466739
1.281322	218.379509	4.471744
1.798725	243.570388	4.476749
1.976912	239.705658	4.481754
1.833340	249.566569	4.486758
2.050367	246.834580	4.491763
1.987908	246.104215	4.496768
1.652896	237.506927	4.501773
1.886301	236.440462	4.506778
1.742678	247.655670	4.511782
2.227326	246.543102	4.516787
1.719078	254.120327	4.521792
1.584249	258.712401	4.526797
1.848121	251.045040	4.531802
1.571428	254.586417	4.536806
1.612342	246.863174	4.541811
1.594691	255.450888	4.546816
1.838754	256.102600	4.551821
1.607559	252.921789	4.556826
1.859105	266.483317	4.561830
2.181851	270.432399	4.566835
1.997313	277.917545	4.571840
2.138765	271.644944	4.576845
2.082403	282.093638	4.581850
1.999644	279.258345	4.586854
2.372875	270.845428	4.591859
2.194108	273.732358	4.596864
2.109655	272.825681	4.601869
2.298534	269.989242	4.606874
2.340450	263.938218	4.611878
2.234821	253.001501	4.616883
1.888243	255.548298	4.621888
2.117610	263.790078	4.626893
2.268554	265.788670	4.631898
2.079174	282.842486	4.636902
2.189605	276.990227	4.641907
2.293063	274.684208	4.646912
2.506958	281.166390	4.651917
2.351557	277.363415	4.656922
1.920902	279.998585	4.661926
2.127236	275.283203	4.666931
2.240569	287.047528	4.671936
2.194918	275.526193	4.676941
2.310445	277.905211	4.681946
2.253334	293.637618	4.686950
2.044482	279.575912	4.691955
2.297975	276.148968	4.696960
2.001586	284.965563	4.701965
2.262904	286.592980	4.706970
2.369085	283.352927	4.711974
2.578512	278.736879	4.716979
2.527729	278.499482	4.721984
2.444988	282.336001	4.726989
2.207869	276.964397	4.731994
2.513794	279.601451	4.736998
2.613365	284.461027	4.742003
2.089081	275.494790	4.747008
2.135522	284.282420	4.752013
2.763414	299.999243	4.757018
2.342889	304.193242	4.762022
2.789910	307.770029	4.767027
2.691920	305.358371	4.772032
2.362072	298.188091	4.777037
2.760775	302.229537	4.782042
2.529239	296.693211	4.787046
2.736770	289.526160	4.792051
2.386059	285.569958	4.797056
2.660005	312.413823	4.802061
2.740612	315.698095	4.807066
2.444172	323.313751	4.812070
2.438303	322.982061	4.817075
2.566001	325.426749	4.822080
2.219781	329.662670	4.827085
2.626590	318.231854	4.832090
2.557581	320.724235	4.837094
2.604126	319.145765	4.842099
2.421283	321.188994	4.847104
2.570455	316.939532	4.852109
2.792141	312.893111	4.857114
2.499035	316.734019	4.862118
2.543231	314.246826	4.867123
3.013424	327.701814	4.872128
3.014618	323.050116	4.877133
2.882406	320.802799	4.882138
2.904446	317.749194	4.887142
3.095622	319.728673	4.892147
3.217164	320.972624	4.897152
2.803995	314.019637	4.902157
3.054576	322.346131	4.907162
2.896492	321.012820	4.912166
2.765987	325.752195	4.917171
2.910461	320.964202	4.922176
2.810756	326.575011	4.927181
3.006769	318.036422	4.932186
3.022345	323.498815	4.937190
3.349691	316.654209	4.942195
3.290170	321.360668	4.947200
3.276973	320.965866	4.952205
3.244495	313.093964	4.957210
2.845251	323.329136	4.962214
3.133670	316.758584	4.967219
3.224447	320.267705	4.972224
3.148882	324.717142	4.977229
3.319203	314.267116	4.982234
3.254791	318.408832	4.987238
3.321513	310.187146	4.992243
2.993243	315.299987	4.997248
2.871789	319.725675	5.002253
3.139876	315.565572	5.007258
2.815885	323.129568	5.012262
3.034568	324.909116	5.017267
2.757554	312.344037	5.022272
2.745804	311.990828	5.027277
2.851215	315.339846	5.032282
3.016544	331.916016	5.037286
3.200839	336.027051	5.042291
3.392952	346.479281	5.047296
3.322046	340.679637	5.052301
3.442478	348.710071	5.057306
3.266749	345.077008	5.062310
3.744671	340.443347	5.067315
3.463767	328.984560	5.072320
3.131558	325.708044	5.077325
3.419066	313.818332	5.082330
2.974800	322.075226	5.087334
3.573860	325.966553	5.092339
3.101340	330.771660	5.097344
3.428856	335.154888	5.102349
3.748531	339.933694	5.107354
3.254913	338.418171	5.112358
3.845740	337.875212	5.117363
3.540038	332.402508	5.122368
3.338060	330.893565	5.127373
3.461695	320.351247	5.132378
3.342595	324.719121	5.137382
3.165616	330.957469	5.142387
3.318446	344.456541	5.147392
3.303524	346.357407	5.152397
3.493155	355.464440	5.157402
3.461959	347.245986	5.162406
3.356829	345.761003	5.167411
3.289931	345.055446	5.172416
3.801170	354.070144	5.177421
3.762594	346.184636	5.182426
3.370990	350.584197	5.187430
3.412892	349.659867	5.192435
3.484786	344.130906	5.197440
3.534972	350.436089	5.202445
3.442138	343.721106	5.207450
3.437582	348.420213	5.212454
3.545928	343.177247	5.217459
3.695079	344.385235	5.222464
3.357540	349.820690	5.227469
3.498788	363.959486	5.232474
3.819599	368.293914	5.237478
3.830246	378.354035	5.242483
3.942842	374.009997	5.247488
3.568485	386.415693	5.252493
4.049241	380.359167	5.257498
3.631595	376.996399	5.262502
3.872490	378.303988	5.267507
3.965674	380.400404	5.272512
3.776115	371.560612	5.277517
3.641660	372.073176	5.282522
3.824523	382.503091	5.287526
3.750596	373.302492	5.292531
3.681707	380.080361	5.297536
3.312461	387.613430	5.302541
3.749185	378.400171	5.307546
3.703288	380.012952	5.312550
3.776291	380.460249	5.317555
3.856052	380.560693	5.322560
3.891592	371.090694	5.327565
4.316221	377.970641	5.332570
3.798996	382.229475	5.337574
4.060167	372.917923	5.342579
3.936239	385.237788	5.347584
4.234751	377.097518	5.352589
4.242259	376.917721	5.357594
3.831268	389.313130	5.362598
4.053992	373.485488	5.367603
4.095029	384.082835	5.372608
3.887595	386.371696	5.377613
4.268819	369.682989	5.382618
4.168790	384.079766	5.387622
4.279088	388.959102	5.392627
4.313300	379.905101	5.397632
4.102790	380.793599	5.402637
4.201826	378.171777	5.407642
3.798766	384.931588	5.412646
4.036575	382.620784	5.417651
4.168934	391.722952	5.422656
3.844402	390.212865	5.427661
3.931602	384.784749	5.432666
4.005133	396.557944	5.437670
4.190747	406.328716	5.442675
4.216079	412.963460	5.447680
4.017364	416.079878	5.452685
4.255741	420.886430	5.457690
4.064058	415.581620	5.462694
3.878785	420.986658	5.467699
4.258841	412.766905	5.472704
4.500970	411.250241	5.477709
4.419914	415.722324	5.482714
4.097247	412.980756	5.487718
4.279383	408.879710	5.492723
4.362951	416.292731	5.497728
4.237317	418.435194	5.502733
4.376109	411.729633	5.507738
4.450916	414.549970	5.512742
4.317129	412.135563	5.517747
4.299423	412.191430	5.522752
4.429590	420.788211	5.527757
4.562103	421.043675	5.532762
4.003595	422.445271	5.537766
4.792028	422.095017	5.542771
4.495577	418.236518	5.547776
4.119426	419.318905	5.552781
4.350712	433.274275	5.557786
4.846768	443.283551	5.562790
4.848692	441.992700	5.567795
4.412861	429.168776	5.572800
4.122912	431.093858	5.577805
4.651991	440.202928	5.582810
4.732837	445.359499	5.587814
4.643622	452.622472	5.592819
4.667506	446.135896	5.597824
4.681876	457.573636	5.602829
4.948398	443.666012	5.607834
4.834466	451.686912	5.612838
4.685947	442.559647	5.617843
4.539945	433.127679	5.622848
4.651773	435.052480	5.627853
4.899448	447.786401	5.632858
4.721120	444.580383	5.637862
4.790685	443.219681	5.642867
4.806484	439.092009	5.647872
4.289178	455.594904	5.652877
4.814821	443.429300	5.657882
4.740802	451.916380	5.662886
4.533453	444.184972	5.667891
4.562927	446.138855	5.672896
4.565171	442.130061	5.677901
4.875718	442.556227	5.682906
4.775736	439.013756	5.687910
4.672213	442.749774	5.692915
4.653329	445.228909	5.697920
4.783378	449.857327	5.702925
5.043394	436.235150	5.707930
4.872378	446.516532	5.712934
4.928922	442.869701	5.717939
5.000768	445.710467	5.722944
4.627786	450.924519	5.727949
4.734781	444.858462	5.732954
4.622390	451.501512	5.737958
4.905580	464.663483	5.742963
5.111828	462.636747	5.747968
4.956391	475.475782	5.752973
5.380735	462.692174	5.757978
5.100554	475.977202	5.762982
4.935643	467.437153	5.767987
5.134322	470.816484	5.772992
4.786723	467.880728	5.777997
5.263382	463.252175	5.783002
5.186399	470.486286	5.788006
5.409864	476.192814	5.793011
5.289297	464.914081	5.798016
4.779552	461.024919	5.803021
5.372686	461.143237	5.808026
5.286334	468.533615	5.813030
4.935213	461.043954	5.818035
5.122484	463.840279	5.823040
5.099217	468.493397	5.828045
5.316474	469.886028	5.833050
5.306994	472.154232	5.838054
5.692832	471.451560	5.843059
5.597542	454.098016	5.848064
4.984423	457.198273	5.853069
5.076221	451.823636	5.858074
4.778257	466.529067	5.863078
4.984495	463.558282	5.868083
5.251096	470.907556	5.873088
5.399783	473.140787	5.878093
5.322941	475.055908	5.883098
5.452985	476.182821	5.888102
5.401473	477.686827	5.893107
5.374040	479.718057	5.898112
5.448304	469.324741	5.903117
5.816241	473.411209	5.908122
5.214233	477.541685	5.913126
5.287274	470.276729	5.918131
5.192262	468.774659	5.923136
4.942524	474.221019	5.928141
5.373847	464.901256	5.933146
5.325855	472.876870	5.938150
5.127527	473.172725	5.943155
5.475791	482.817448	5.948160
5.270209	483.575089	5.953165
5.813541	490.556323	5.958170
5.204439	491.398600	5.963174
5.720192	489.115581	5.968179
5.586930	503.452675	5.973184
5.575503	505.799352	5.978189
5.738967	500.638143	5.983194
5.581188	497.882965	5.988198
5.506518	493.955812	5.993203
5.610796	492.962694	5.998208
5.612128	510.116682	6.003213
5.656526	498.711244	6.008218
5.698548	514.516593	6.013222
5.778005	505.506305	6.018227
5.476585	483.011080	6.023232
5.459782	488.398598	6.028237
5.873164	492.864491	6.033242
5.453290	486.808442	6.038246
5.663069	491.873741	6.043251
5.770280	488.671756	6.048256
5.666544	496.877072	6.053261
5.594957	479.345510	6.058266
4.988600	484.962645	6.063270
5.504952	495.810414	6.068275
5.534201	511.185718	6.073280
5.632409	517.475685	6.078285
5.808255	509.187803	6.083290
5.386863	506.069141	6.088294
5.519828	498.621937	6.093299
5.632089	506.272954	6.098304
5.498107	511.172213	6.103309
5.801457	503.362991	6.108314
5.497185	510.712454	6.113318
5.481705	517.924918	6.118323
5.489724	508.037506	6.123328
5.565455	510.734768	6.128333
5.713371	505.521479	6.133338
5.600159	508.304611	6.138342
5.680389	514.714191	6.143347
5.729878	508.994125	6.148352
5.522034	519.560315	6.153357
6.091233	505.536020	6.158362
5.619301	519.967706	6.163366
5.694819	509.586982	6.168371
5.420725	505.671464	6.173376
5.341953	513.702142	6.178381
5.638117	501.147011	6.183386
5.355961	516.147048	6.188390
5.386537	511.963620	6.193395
5.588082	511.319601	6.198400
5.637886	510.866962	6.203405
5.580905	508.852598	6.208410
5.440366	510.285367	6.213414
5.624707	515.926583	6.218419
5.727770	511.989221	6.223424
5.463658	510.497298	6.228429
5.745439	503.143559	6.233434
5.578632	515.662861	6.238438
5.545093	510.354622	6.243443
5.555109	514.032909	6.248448
5.283738	514.287230	6.253453
5.469557	504.287780	6.258458
5.652858	504.486456	6.263462
5.717309	507.046076	6.268467
5.644211	505.521021	6.273472
5.357386	515.790717	6.278477
5.669095	508.716559	6.283482
5.432373	507.201336	6.288486
5.502785	507.429828	6.293491
5.701766	518.009301	6.298496
5.663221	517.733556	6.303501
5.874205	506.298449	6.308506
5.618680	511.895364	6.313510
5.440249	512.354266	6.318515
5.651518	506.866806	6.323520
5.381843	510.932973	6.328525
5.712410	507.829625	6.333530
5.492257	508.330193	6.338534
5.370347	528.120171	6.343539
5.655411	524.087433	6.348544
5.946662	531.419417	6.353549
5.778396	524.452859	6.358554
5.436911	518.313121	6.363558
5.573521	513.319568	6.368563
5.378928	516.570890	6.373568
5.418610	534.324548	6.378573
5.800446	531.709959	6.383578
5.823017	536.784092	6.388582
5.668501	530.679971	6.393587
6.034377	532.146374	6.398592
5.723074	513.459160	6.403597
5.696548	514.434103	6.408602
5.520080	517.342601	6.413606
5.796336	510.064568	6.418611
5.625118	505.018583	6.423616
5.422263	508.662791	6.428621
5.495653	509.802280	6.433626
5.531250	510.775186	6.438630
5.416547	517.729846	6.443635
5.755184	503.037614	6.448640
5.790007	514.755172	6.453645
5.958866	510.033319	6.458650
5.646727	515.903286	6.463654
5.204722	514.664710	6.468659
5.486502	503.801358	6.473664
5.345785	513.162111	6.478669
5.624267	517.506182	6.483674
5.965605	531.584641	6.488678
5.880427	529.539836	6.493683
5.911315	519.779646	6.498688
5.584500	515.980042	6.503693
5.629602	515.312693	6.508698
5.403885	514.991100	6.513702
5.502351	522.486550	6.518707
5.566462	503.545924	6.523712
5.413914	514.879631	6.528717
5.472119	506.163551	6.533722
5.577202	511.609553	6.538726
5.492080	515.860930	6.543731
5.805891	522.192812	6.548736
5.533254	531.383891	6.553741
5.837721	526.667513	6.558746
5.440495	528.410538	6.563750
5.439937	536.305680	6.568755
6.061192	537.848629	6.573760
5.549946	533.997191	6.578765
5.500348	509.948082	6.583770
5.587026	518.393489	6.588774
5.798353	527.815517	6.593779
5.639168	516.021805	6.598784
5.515239	521.003461	6.603789
5.839526	510.186714	6.608794
5.677230	515.551065	6.613798
5.821897	513.345906	6.618803
5.913874	505.467032	6.623808
5.537727	509.731261	6.628813
5.505308	512.298104	6.633818
5.604219	512.418060	6.638822
5.635837	513.356698	6.643827
5.552849	507.992940	6.648832
5.317227	515.660150	6.653837
5.709094	516.990214	6.658842
5.687096	509.509760	6.663846
5.615013	516.020040	6.668851
5.641951	510.650046	6.673856
5.592388	520.687510	6.678861
5.562328	519.041438	6.683866
5.683573	515.314175	6.688870
5.455087	518.230530	6.693875
6.172392	518.776358	6.698880
5.510537	511.804036	6.703885
5.547520	509.399708	6.708890
5.825001	513.027419	6.713894
5.325441	511.891355	6.718899
5.818260	519.152532	6.723904
5.506455	512.391387	6.728909
5.768555	519.862793	6.733914
5.433983	505.802242	6.738918
5.352589	516.210065	6.743923
5.654793	508.541533	6.748928
5.487888	519.931306	6.753933
5.670340	511.524317	6.758938
5.842099	514.534182	6.763942
5.875052	517.598693	6.768947
5.987786	518.471160	6.773952
5.685859	515.247586	6.778957
5.594842	509.925418	6.783962
5.528751	509.590711	6.788966
5.461714	513.561035	6.793971
5.512471	504.005346	6.798976
5.614220	515.459981	6.803981
5.664542	506.244373	6.808986
5.688701	516.251622	6.813990
5.680020	514.119116	6.818995
5.716766	518.454825	6.824000
5.718292	511.067549	6.829005
5.678152	508.103965	6.834010
5.738529	504.074638	6.839014
5.854140	509.201771	6.844019
5.876920	515.236689	6.849024
5.367699	513.102923	6.854029
5.976494	505.766855	6.859034
5.851102	522.536594	6.864038
5.710389	508.918211	6.869043
5.877569	518.227985	6.874048
5.545570	515.263776	6.879053
5.731034	511.226482	6.884058
5.880742	512.551609	6.889062
5.787221	492.198622	6.894067
5.717475	481.767075	6.899072
5.460008	479.460438	6.904077
5.314105	482.002133	6.909082
5.261452	490.339456	6.914086
5.630853	501.779586	6.919091
5.698345	511.218014	6.924096
5.610632	520.032813	6.929101
5.929084	511.994535	6.934106
5.626795	504.535414	6.939110
5.618249	489.436178	6.944115
5.693271	481.402661	6.949120
5.445954	484.454946	6.954125
5.322645	494.879589	6.959130
5.535334	505.426780	6.964134
5.486701	512.140758	6.969139
5.970309	512.301949	6.974144
5.808948	516.249670	6.979149
5.820941	499.064528	6.984154
5.606984	488.263066	6.989158
5.155125	488.235203	6.994163
5.723757	495.486727	6.999168
5.312097	509.529304	7.004173
5.709576	511.608507	7.009178
6.044353	512.974307	7.014182
5.560571	502.288134	7.019187
5.753294	504.482674	7.024192
5.560946	504.649859	7.029197
5.816768	493.237304	7.034202
5.604651	490.495303	7.039206
5.355262	482.967212	7.044211
5.482157	497.478915	7.049216
5.584399	502.762782	7.054221
5.713775	511.920574	7.059226
5.671085	509.309854	7.064230
5.691399	512.061320	7.069235
5.515284	518.901671	7.074240
5.314480	521.991619	7.079245
5.276965	512.817840	7.084250
5.555419	508.269975	7.089254
5.434627	515.518690	7.094259
5.696784	504.716616	7.099264
5.821235	511.444842	7.104269
5.812057	510.066636	7.109274
5.384395	512.300558	7.114278
5.375584	518.022031	7.119283
5.952939	516.525412	7.124288
5.456094	517.974586	7.129293
5.565305	516.526774	7.134298
5.431378	517.194559	7.139302
5.223862	516.735949	7.144307
5.629094	521.424023	7.149312
5.533220	517.718050	7.154317
5.827777	522.594033	7.159322
5.926990	514.918786	7.164326
5.813294	519.072496	7.169331
5.756855	515.598942	7.174336
5.063837	515.006923	7.179341
5.708485	520.667534	7.184346
5.830236	517.767812	7.189350
5.711920	523.177741	7.194355
5.797965	512.801777	7.199360
5.506804	523.897259	7.204365
5.614170	516.948825	7.209370
5.734213	513.128028	7.214374
5.396761	515.555145	7.219379
5.715405	508.820238	7.224384
5.408434	523.452233	7.229389
5.788340	522.802838	7.234394
5.638698	515.057067	7.239398
5.743415	514.995496	7.244403
5.837198	512.356171	7.249408
5.183952	520.418997	7.254413
5.351753	516.343394	7.259418
5.569720	515.384855	7.264422
5.608792	514.920580	7.269427
5.976350	503.947657	7.274432
5.604099	509.327763	7.279437
6.008238	518.226370	7.284442
5.979742	521.549541	7.289446
5.499656	526.639733	7.294451
5.917530	521.108454	7.299456
5.718846	518.113797	7.304461
5.686141	503.885853	7.309466
5.758229	496.469095	7.314470
5.577621	489.059415	7.319475
5.598475	479.824646	7.324480
5.415007	486.639761	7.329485
5.704167	493.630093	7.334490
5.735016	487.756449	7.339494
5.760995	497.239854	7.344499
5.828235	480.896656	7.349504
5.852140	483.630944	7.354509
5.424759	482.567542	7.359514
5.188592	483.404465	7.364518
5.352915	479.173160	7.369523
5.782850	496.845923	7.374528
5.572079	507.698333	7.379533
5.435325	508.819866	7.384538
5.662206	511.904041	7.389542
5.454317	522.857215	7.394547
5.839597	514.065648	7.399552
5.764638	510.575834	7.404557
5.690535	497.494390	7.409562
5.782240	489.070530	7.414566
5.573917	482.812964	7.419571
5.607737	492.539363	7.424576
5.512268	481.838388	7.429581
5.327825	482.155023	7.434586
5.344496	499.358941	7.439590
5.651442	510.987061	7.444595
5.877340	511.412105	7.449600
5.549575	526.919190	7.454605
5.649339	522.237629	7.459610
5.682209	518.726338	7.464614
5.651429	517.214771	7.469619
5.804138	520.053358	7.474624
5.732333	502.213371	7.479629
5.576135	499.933311	7.484634
5.767146	490.045488	7.489638
5.364704	498.734791	7.494643
5.664710	498.544459	7.499648
5.577961	495.688476	7.504653
5.399314	499.027523	7.509658
5.884300	520.709702	7.514662
5.555864	512.666666	7.519667
5.778804	496.515627	7.524672
5.459010	496.435817	7.529677
5.563250	499.648120	7.534682
5.453233	516.413915	7.539686
5.553978	517.584971	7.544691
5.716473	513.890911	7.549696
5.714771	516.818509	7.554701
5.930376	513.376302	7.559706
5.603948	498.461321	7.564710
5.355354	480.477090	7.569715
5.305997	500.731538	7.574720
5.409797	503.653832	7.579725
5.941015	516.866183	7.584730
5.834549	509.745698	7.589734
5.994781	504.696519	7.594739
5.703850	493.746231	7.599744
5.258758	495.271062	7.604749
5.478585	496.278464	7.609754
5.376602	492.257973	7.614758
5.569099	515.213622	7.619763
5.696485	520.366626	7.624768
5.542998	514.617347	7.629773
5.680773	513.602676	7.634778
5.946129	512.949431	7.639782
5.917599	508.346624	7.644787
5.956955	487.989317	7.649792
5.145444	485.390363	7.654797
5.458529	481.015929	7.659802
5.768500	497.631776	7.664806
5.545171	493.053657	7.669811
5.820151	480.371823	7.674816
5.707143	486.034826	7.679821
5.647172	488.550991	7.684826
5.645879	479.053698	7.689830
5.596856	479.976928	7.694835
5.758320	482.951003	7.699840
5.319203	483.397588	7.704845
5.378437	475.038135	7.709850
5.763873	497.915906	7.714854
5.752650	487.191846	7.719859
5.684735	487.387682	7.724864
5.485701	486.199693	7.729869
5.280916	487.026072	7.734874
5.198575	492.488816	7.739878
4.977187	501.879942	7.744883
5.606614	513.053869	7.749888
5.147593	515.901390	7.754893
5.623026	511.217773	7.759898
5.691206	506.531402	7.764902
5.670861	513.139248	7.769907
5.579653	511.615230	7.774912
5.559566	513.045540	7.779917
5.258649	516.909502	7.784922
5.677636	521.177136	7.789926
5.394725	518.815324	7.794931
5.708937	513.691608	7.799936
5.781140	519.182546	7.804941
5.645655	524.443775	7.809946
5.998282	518.547023	7.814950
5.623699	526.182279	7.819955
5.785814	521.789515	7.824960
6.029623	524.748925	7.829965
5.568441	512.364270	7.834970
5.781504	515.645709	7.839974
5.586485	522.412834	7.844979
5.491576	514.372618	7.849984
5.583684	519.376380	7.854989
5.596020	517.306685	7.859994
5.937374	521.149730	7.864998
5.610864	521.993976	7.870003
5.624480	512.240806	7.875008
5.566615	524.328193	7.880013
5.503491	522.687813	7.885018
5.790590	514.932988	7.890022
5.331322	523.897759	7.895027
5.429158	515.117661	7.900032
5.468440	522.630645	7.905037
5.438508	520.790175	7.910042
5.447224	519.419452	7.915046
5.486758	519.211834	7.920051
5.820652	510.747508	7.925056
5.565544	517.947707	7.930061
5.661050	518.760680	7.935066
6.397894	515.227490	7.940070
5.830900	523.095615	7.945075
6.017238	517.735433	7.950080
5.672394	519.556578	7.955085
5.728678	512.475936	7.960090
6.030733	515.243916	7.965094
5.730903	503.739599	7.970099
5.860389	488.481851	7.975104
5.525384	487.839599	7.980109
5.174905	480.333049	7.985114
5.230765	494.632187	7.990118
5.256948	518.778857	7.995136
5.540295	514.667408	8.000154
5.458422	520.998977	8.005171
5.724860	522.775032	8.010189
5.554677	518.109696	8.015206
5.208788	531.120763	8.020224
5.683551	528.173448	8.025242
5.795409	514.343960	8.030259
5.665003	521.014470	8.035277
5.847971	523.236644	8.040294
5.957716	528.201644	8.045312
5.761956	518.689627	8.050330
5.804375	528.918879	8.055347
5.723146	529.182199	8.060365
6.102687	529.532891	8.065382
5.518167	526.350271	8.070400
5.901767	519.914496	8.075418
5.942049	525.425047	8.080435
5.845290	506.256525	8.085453
5.890517	484.224338	8.090470
5.467065	491.275011	8.095488
5.427553	480.523183	8.100506
5.713085	502.060345	8.105523
5.992202	508.814143	8.110541
5.911538	494.219110	8.115558
5.564629	498.908662	8.120576
5.529375	489.661097	8.125594
5.699629	502.553673	8.130611
6.068043	508.625170	8.135629
6.017833	508.035381	8.140646
5.601974	486.714420	8.145664
5.865128	484.238269	8.150682
5.869124	490.944295	8.155699
5.634768	481.992404	8.160717
5.545289	489.982744	8.165734
5.722536	510.738386	8.170752
5.853933	515.358674	8.175770
6.168964	508.112919	8.180787
5.782166	500.998786	8.185805
6.033878	488.490437	8.190822
5.491057	489.913649	8.195840
6.057515	496.019342	8.200858
5.535166	503.021701	8.205875
5.757025	514.423563	8.210893
5.963655	513.892254	8.215910
5.846065	517.375101	8.220928
6.002459	519.445406	8.225946
5.741191	515.624269	8.230963
5.650258	521.363107	8.235981
5.818561	520.346088	8.240998
5.544849	523.924171	8.246016
5.649816	524.353375	8.251034
5.732351	525.990723	8.256051
5.470615	522.561752	8.261069
5.794255	509.272997	8.266086
5.468061	520.765174	8.271104
5.796569	521.104666	8.276122
5.770460	515.505034	8.281139
5.801113	519.374226	8.286157
6.300228	521.859371	8.291174
5.844911	521.497141	8.296192
5.900169	509.090715	8.301210
6.096548	517.088863	8.306227
5.529681	522.486182	8.311245
5.701255	523.513903	8.316262
5.992227	549.857266	8.321280
6.062919	547.161938	8.326298
6.038486	547.615013	8.331315
6.058097	551.348659	8.336333
5.950775	537.999637	8.341350
5.744851	541.024971	8.346368
5.930029	537.352434	8.351386
6.204339	543.115403	8.356403
5.902610	554.453552	8.361421
6.459276	548.348217	8.366438
6.027655	545.497036	8.371456
5.890755	522.863629	8.376474
5.953240	521.465614	8.381491
5.827518	520.403185	8.386509
6.159805	536.020964	8.391526
6.320555	541.357180	8.396544
6.198833	539.961832	8.401562
6.299464	521.819832	8.406579
6.007981	530.046114	8.411597
6.183126	517.389066	8.416614
6.014160	519.790593	8.421632
5.698324	525.135556	8.426650
5.832233	516.401146	8.431667
5.930431	534.087961	8.436685
6.271362	542.656923	8.441702
5.837755	536.451260	8.446720
6.174891	547.268485	8.451738
6.196969	551.400898	8.456755
6.189584	547.664312	8.461773
6.167860	542.738880	8.466790
5.920525	544.540895	8.471808
5.948949	546.376790	8.476826
6.400220	543.383774	8.481843
6.146096	549.424330	8.486861
6.240209	551.023540	8.491878
6.064013	543.375607	8.496896
6.069516	552.254046	8.501914
6.413943	548.206839	8.506931
5.992490	548.726497	8.511949
6.446029	547.390238	8.516966
5.912070	533.793070	8.521984
6.035065	543.822144	8.527002
6.462588	553.580743	8.532019
6.147005	550.902972	8.537037
6.189137	545.972633	8.542054
6.111449	554.237990	8.547072
6.457242	554.484853	8.552090
6.495192	527.248969	8.557107
5.891295	534.011771	8.562125
6.041226	530.916892	8.567143
6.118948	538.893440	8.572160
6.088357	549.949137	8.577178
6.452981	549.352789	8.582195
6.010708	555.003006	8.587213
6.245592	553.671795	8.592231
6.260184	552.916129	8.597248
6.003311	545.936270	8.602266
6.475283	556.450997	8.607283
6.387157	550.616406	8.612301
6.475715	551.085342	8.617319
6.359029	553.197304	8.622336
6.092906	554.186572	8.627354
6.090204	551.310743	8.632371
6.161958	560.373039	8.637389
6.433562	553.686795	8.642407
6.134922	556.526774	8.647424
6.000372	556.746404	8.652442
6.082810	548.347471	8.657459
5.814874	559.721144	8.662477
5.860865	563.901549	8.667495
5.926137	557.325381	8.672512
6.253682	570.582778	8.677530
6.565258	582.575826	8.682547
6.560205	583.897848	8.687565
6.361441	575.436005	8.692583
6.347585	584.049988	8.697600
6.185105	581.396168	8.702618
6.372924	586.771991	8.707635
6.267633	586.259263	8.712653
6.161034	583.590248	8.717671
6.199400	583.729369	8.722688
6.343736	599.932933	8.727706
6.344633	588.421623	8.732723
6.242108	594.536988	8.737741
6.291723	587.179817	8.742759
6.319054	592.580744	8.747776
6.198093	593.533090	8.752794
6.471803	588.430595	8.757811
6.420951	593.587847	8.762829
6.637700	586.954798	8.767847
6.619158	588.347560	8.772864
6.368486	587.883404	8.777882
6.658276	588.650950	8.782899
6.276865	588.329184	8.787917
6.246655	585.124486	8.792935
6.368272	584.831105	8.797952
6.193073	594.447614	8.802970
6.864573	587.159301	8.807987
6.489615	598.062843	8.813005
6.362802	595.471393	8.818023
6.223271	596.872457	8.823040
6.345236	587.458555	8.828058
6.451637	600.036657	8.833075
6.572618	606.755175	8.838093
6.557637	608.479995	8.843111
6.557692	602.381931	8.848128
6.240703	616.155127	8.853146
6.865347	614.936866	8.858163
6.508078	627.682802	8.863181
6.680376	613.931360	8.868199
6.730840	613.244132	8.873216
6.508905	600.745531	8.878234
6.498243	598.472146	8.883251
6.240266	606.530708	8.888269
6.710712	615.222854	8.893287
6.892033	619.624066	8.898304
6.584050	622.615203	8.903322
6.822412	607.741070	8.908339
6.634508	602.873750	8.913357
6.773719	597.245034	8.918375
6.886571	592.412168	8.923392
6.251474	602.527136	8.928410
6.822307	581.640802	8.933427
6.629684	589.651291	8.938445
6.678259	591.506674	8.943463
6.716257	594.114145	8.948480
6.909592	593.360456	8.953498
6.826317	588.766866	8.958515
6.842354	588.368210	8.963533
6.484491	588.011234	8.968551
6.820366	588.010950	8.973568
6.901251	588.650242	8.978586
6.919600	579.337026	8.983603
6.726961	596.601628	8.988621
6.708933	582.894053	8.993639
6.978500	579.614136	8.998656
6.506709	587.979859	9.003674
6.798546	584.054957	9.008691
6.785495	586.674848	9.013709
6.622058	593.745530	9.018727
6.728414	588.570664	9.023744
6.735658	589.082445	9.028762
6.931630	585.925183	9.033779
6.771433	594.132432	9.038797
6.766688	593.079021	9.043815
6.749891	589.600266	9.048832
6.792844	587.562240	9.053850
6.646905	588.171131	9.058867
6.624568	587.993599	9.063885
6.511306	592.555373	9.068903
6.715835	587.252584	9.073920
6.411874	598.789742	9.078938
6.727003	609.538431	9.083955
6.888647	614.793035	9.088973
6.930292	624.604207	9.093991
6.922130	621.406466	9.099008
6.786580	620.276575	9.104026
6.771059	624.411714	9.109043
6.490847	618.423216	9.114061
6.543750	625.814221	9.119079
6.587933	620.640428	9.124096
6.463654	621.527979	9.129114
6.860665	614.187847	9.134131
6.538622	617.159669	9.139149
6.736310	625.723552	9.144167
6.785366	620.485766	9.149184
6.859693	634.878718	9.154202
7.182166	634.182099	9.159219
7.334875	633.563103	9.164237
6.812580	620.748302	9.169255
7.171731	615.397363	9.174272
7.127208	623.375772	9.179290
6.963710	619.400377	9.184307
6.691532	616.831905	9.189325
6.456188	619.876316	9.194343
6.896129	629.279977	9.199360
6.916917	645.231116	9.204378
6.765425	654.252826	9.209395
7.205665	653.656896	9.214413
6.921587	658.298850	9.219431
7.277981	646.306197	9.224448
7.227252	643.000773	9.229466
6.921307	639.401974	9.234483
6.935814	642.276130	9.239501
7.087625	645.881337	9.244519
7.244961	641.434729	9.249536
6.969816	647.815993	9.254554
6.458668	640.390406	9.259571
6.830252	647.071025	9.264589
6.653257	652.725209	9.269607
6.935866	651.643516	9.274624
6.792579	649.505348	9.279642
7.100753	657.745595	9.284659
7.614330	655.191574	9.289677
7.334298	656.247327	9.294695
7.423064	656.401494	9.299712
7.315785	657.626351	9.304730
7.181910	654.913043	9.309747
7.459588	653.983929	9.314765
7.110661	662.998307	9.319783
7.113872	654.345185	9.324800
7.015187	654.324228	9.329818
7.033271	658.462057	9.334835
7.142620	661.481462	9.339853
6.810940	656.459496	9.344871
7.236050	659.374844	9.349888
7.380239	659.252498	9.354906
7.276817	658.771738	9.359923
7.258516	662.981358	9.364941
7.477823	663.294717	9.369959
7.435752	661.192672	9.374976
7.514174	657.925221	9.379994
7.184391	639.524340	9.385011
7.443063	626.021894	9.390029
7.040035	625.990113	9.395047
6.938362	628.269064	9.400064
7.296386	641.175028	9.405082
7.430256	641.731505	9.410099
7.093723	638.649558	9.415117
7.067839	655.622750	9.420135
7.271148	648.350820	9.425152
7.219061	660.788007	9.430170
7.308998	658.532140	9.435187
7.244535	654.076927	9.440205
7.049154	655.446141	9.445223
7.346111	657.130730	9.450240
7.393568	656.226498	9.455258
7.430255	659.863835	9.460275
7.461168	656.656246	9.465293
7.221818	655.267842	9.470311
7.338854	652.686829	9.475328
7.271063	659.321796	9.480346
7.501399	661.382980	9.485363
7.340963	653.721940	9.490381
7.299672	661.894894	9.495399
7.440743	655.996185	9.500416
7.478957	663.048340	9.505434
6.984769	659.838079	9.510451
7.619701	652.584356	9.515469
7.186325	662.572336	9.520487
7.891631	664.216804	9.525504
7.322858	664.534396	9.530522
7.670423	662.737830	9.535539
7.563909	666.304689	9.540557
7.160278	663.366950	9.545575
7.386305	662.408825	9.550592
7.397771	659.069636	9.555610
7.425692	665.169448	9.560627
7.539395	657.456146	9.565645
7.018531	666.974657	9.570663
7.322434	655.590476	9.575680
7.707310	665.048584	9.580698
7.362641	654.562498	9.585715
7.901858	661.216835	9.590733
7.323579	665.436472	9.595751
7.486882	664.359059	9.600768
7.433513	659.008964	9.605786
7.295047	666.432586	9.610803
7.392161	661.895203	9.615821
7.314530	662.433692	9.620839
7.402387	652.509125	9.625856
7.418603	657.567266	9.630874
7.087422	654.333651	9.635891
7.518353	648.430658	9.640909
7.382362	662.606255	9.645927
7.823009	674.443679	9.650944
7.519494	664.298552	9.655962
7.333652	674.763463	9.660979
7.620311	679.003690	9.665997
7.730913	694.446487	9.671015
7.965585	685.165552	9.676032
7.683625	660.499924	9.681050
7.624596	665.315872	9.686067
7.667032	658.969619	9.691085
7.627987	653.875391	9.696103
7.608436	655.523424	9.701120
8.036202	663.646560	9.706138
7.463383	654.817751	9.711155
7.728025	658.047543	9.716173
7.556293	656.362884	9.721191
7.976575	648.137839	9.726208
7.658670	659.794869	9.731226
7.379495	658.597321	9.736243
7.815421	653.719001	9.741261
7.476595	650.292185	9.746279
7.279474	660.024967	9.751296
7.615299	671.560549	9.756314
7.845754	678.853372	9.761331
8.231834	674.076630	9.766349
7.903129	675.363488	9.771367
8.088346	665.271758	9.776384
7.682899	653.626581	9.781402
7.607465	654.656199	9.786419
7.795748	649.465923	9.791437
7.565139	655.836441	9.796455
7.727327	656.131541	9.801472
8.011443	666.771852	9.806490
7.641782	671.874455	9.811507
7.805332	671.379237	9.816525
7.825567	681.487680	9.821543
7.819692	680.871816	9.826560
7.517755	690.294311	9.831578
7.796436	690.075009	9.836595
8.007041	683.842907	9.841613
7.974319	686.988089	9.846631
8.124115	688.238518	9.851648
7.927050	670.833764	9.856666
7.623858	671.018833	9.861683
8.221905	677.328583	9.866701
7.784764	671.058694	9.871719
7.592106	674.347575	9.876736
7.652583	682.039095	9.881754
7.397966	679.912932	9.886771
7.719491	677.472714	9.891789
7.585295	684.472834	9.896807
7.863279	688.492477	9.901824
8.005959	683.338508	9.906842
7.705252	692.805678	9.911859
7.919604	691.080263	9.916877
7.845145	688.405297	9.921895
7.908691	688.900834	9.926912
7.840116	694.494889	9.931930
7.626270	688.832510	9.936947
7.381836	705.648596	9.941965
7.529651	723.264786	9.946983
7.783951	718.614652	9.952000
8.050183	716.889074	9.957018
8.147229	719.775901	9.962035
8.091568	716.304562	9.967053
8.155076	729.906944	9.972071
8.017385	723.107179	9.977088
8.295591	716.607155	9.982106
7.944337	726.280565	9.987123
8.380636	726.250205	9.992141
8.418557	724.519273	9.997159
7.969931	730.876852	10.002176
8.269015	720.112864	10.007194
8.187110	724.262607	10.012211
8.397617	714.043816	10.017229
8.029140	729.125568	10.022247
7.882356	717.327317	10.027264
8.154561	715.464537	10.032282
8.363158	721.505405	10.037299
8.443942	711.158584	10.042317
8.102699	737.488860	10.047335
7.956826	730.356423	10.052352
8.480570	722.587136	10.057370
8.283643	715.156720	10.062387
8.397584	707.082950	10.067405
7.997938	695.558617	10.072423
7.800681	708.360889	10.077440
8.535105	706.307510	10.082458
8.276342	714.598720	10.087475
8.333655	714.037111	10.092493
7.824868	703.980601	10.097511
7.863071	716.779566	10.102528
7.933116	707.428549	10.107546
7.997262	715.926104	10.112563
8.046800	714.732767	10.117581
7.968641	717.662297	10.122599
7.886539	712.882466	10.127616
8.062736	718.366361	10.132634
7.797766	731.289938	10.137651
8.395349	744.669121	10.142669
8.407777	749.101789	10.147687
8.191212	756.467968	10.152704
8.320224	754.519939	10.157722
8.214951	756.842613	10.162739
8.409637	756.590426	10.167757
8.356782	755.869975	10.172775
8.599326	753.440315	10.177792
8.339033	745.271459	10.182810
8.556343	750.841241	10.187827
8.475800	752.291367	10.192845
8.240307	744.101068	10.197863
8.297074	746.274769	10.202880
8.597532	743.614044	10.207898
8.403226	745.897190	10.212915
8.716223	750.969608	10.217933
8.301898	736.225690	10.222951
8.366461	741.227992	10.227968
8.556017	732.199981	10.232986
8.362756	741.175145	10.238003
8.555518	727.607588	10.243021
8.382431	729.565773	10.248039
8.027014	741.728666	10.253056
8.733535	750.765281	10.258074
8.490185	756.070323	10.263091
8.499365	760.969050	10.268109
8.657920	754.676483	10.273127
8.602016	764.622847	10.278144
8.612715	744.305348	10.283162
8.354124	746.924548	10.288179
8.702461	751.600178	10.293197
8.142098	748.401488	10.298215
8.309893	743.384652	10.303232
8.605898	749.378524	10.308250
8.140814	740.255599	10.313267
8.239862	751.246981	10.318285
8.378947	751.540017	10.323303
8.386916	750.953737	10.328320
8.570066	745.903248	10.333338
8.523799	739.021356	10.338355
8.395898	753.667897	10.343373
8.317365	750.163151	10.348391
8.167280	763.415860	10.353408
8.396685	763.389576	10.358426
8.746153	782.898940	10.363443
8.980602	774.912970	10.368461
8.567674	780.328092	10.373479
8.447971	778.734763	10.378496
8.757508	776.957102	10.383514
8.750959	777.363317	10.388531
8.915711	784.914533	10.393549
9.159265	777.135104	10.398567
9.052484	783.969307	10.403584
8.917949	757.429356	10.408602
8.663457	762.111497	10.413619
8.861167	753.460830	10.418637
8.866245	748.661970	10.423655
8.570163	760.030036	10.428672
9.004781	749.500960	10.433690
8.670674	751.968749	10.438707
8.316759	755.807836	10.443725
8.681453	747.791963	10.448743
8.396508	755.334652	10.453760
8.948730	765.522034	10.458778
8.800035	789.715829	10.463795
8.845707	780.376692	10.468813
8.935220	787.993759	10.473831
8.836361	790.780298	10.478848
8.660856	779.852260	10.483866
9.041667	777.016965	10.488883
8.562400	785.879865	10.493901
8.969386	772.025892	10.498919
8.759998	783.793707	10.503936
8.787879	783.270843	10.508954
8.900463	784.255832	10.513971
8.995899	781.307354	10.518989
8.854026	785.616479	10.524007
8.915038	790.589074	10.529024
9.253579	784.648241	10.534042
8.914799	793.877331	10.539059
8.878651	784.392552	10.544077
9.061696	784.912714	10.549095
9.254024	787.281391	10.554112
9.192808	768.040302	10.559130
8.933454	767.358112	10.564147
8.805984	764.167575	10.569165
9.103843	760.034951	10.574183
8.852173	766.806229	10.579200
9.106931	777.694391	10.584218
9.070088	777.218504	10.589235
8.826508	762.503459	10.594253
9.260055	778.421950	10.599271
9.208476	772.902634	10.604288
8.962126	757.929018	10.609306
8.980083	762.577683	10.614323
8.934585	769.804616	10.619341
9.111997	775.359190	10.624359
8.840053	785.796955	10.629376
9.139267	783.432077	10.634394
9.241896	790.907015	10.639411
8.960208	790.330103	10.644429
8.969626	789.776846	10.649447
8.837649	790.867245	10.654464
8.850157	781.812537	10.659482
9.058624	785.188101	10.664499
9.061465	793.325641	10.669517
9.509694	791.454852	10.674535
9.134411	803.161287	10.679552
9.114449	788.563760	10.684570
9.185399	791.209681	10.689587
9.038463	791.734105	10.694605
9.094210	785.269849	10.699623
9.135194	789.717465	10.704640
8.830959	780.977395	10.709658
8.836250	790.813021	10.714675
8.851283	796.390262	10.719693
8.977251	801.602242	10.724711
9.009931	829.134009	10.729728
9.163636	830.827666	10.734746
9.456982	821.122557	10.739763
9.080683	833.095502	10.744781
9.373651	816.961592	10.749799
9.599046	831.604596	10.754816
9.250468	819.398109	10.759834
9.381312	819.767709	10.764851
9.181030	823.148433	10.769869
9.394333	816.967794	10.774887
9.386162	821.422409	10.779904
9.310931	816.415633	10.784922
9.729688	816.236822	10.789939
9.278413	823.419818	10.794957
9.439460	823.219084	10.799975
9.361034	820.505978	10.804992
9.227762	824.832384	10.810010
9.344072	825.582522	10.815027
9.058096	821.635896	10.820045
9.365930	817.985422	10.825063
9.273620	828.989574	10.830080
9.244110	830.450121	10.835098
9.544017	832.127940	10.840115
9.311848	829.401021	10.845133
9.271507	826.586512	10.850151
9.232463	827.853973	10.855168
9.164254	817.298793	10.860186
9.103729	825.335080	10.865203
9.230800	850.834610	10.870221
9.586652	844.762146	10.875239
9.416613	863.423384	10.880256
9.186210	859.294099	10.885274
9.579515	853.122697	10.890291
9.344250	862.725144	10.895309
9.376615	859.545419	10.900327
9.651778	859.250918	10.905344
9.552620	857.079994	10.910362
9.815456	859.550144	10.915379
9.189202	862.296218	10.920397
9.505230	859.279761	10.925415
9.501286	855.737988	10.930432
9.324050	869.390745	10.935450
9.537469	858.899347	10.940467
9.340606	864.736425	10.945485
9.558954	860.141828	10.950503
9.658044	863.114162	10.955520
9.645068	859.573692	10.960538
9.588092	863.504974	10.965555
9.271921	873.166739	10.970573
9.989059	881.084224	10.975591
10.066855	880.358191	10.980608
9.753208	877.601502	10.985626
9.852447	858.706046	10.990643
9.656591	860.790267	10.995661
9.656174	858.906255	11.000679
9.732286	862.960679	11.005696
9.838288	859.279772	11.010714
9.767396	855.971946	11.015731
9.619444	871.400026	11.020749
9.805344	871.097136	11.025767
10.031432	876.099796	11.030784
9.696278	872.511701	11.035802
10.038705	863.232039	11.040819
9.856729	858.924638	11.045837
9.673876	856.899899	11.050855
9.716983	860.041567	11.055872
9.835530	873.315461	11.060890
9.972509	876.802330	11.065907
9.667574	881.212990	11.070925
10.331543	885.992092	11.075943
9.615788	868.400122	11.080960
9.681939	869.405235	11.085978
10.019374	882.647478	11.090995
9.872381	887.394066	11.096013
10.002411	889.951449	11.101031
9.839500	876.808014	11.106048
9.932184	891.714063	11.111066
10.297197	888.312909	11.116083
9.637162	887.501855	11.121101
10.085688	883.273491	11.126119
9.891834	880.414218	11.131136
10.068407	889.150643	11.136154
10.350396	887.425578	11.141171
9.756040	885.122016	11.146189
9.684909	876.765753	11.151207
9.787725	885.550063	11.156224
10.007127	892.089758	11.161242
10.053179	888.540454	11.166259
10.129581	896.610313	11.171277
10.167966	880.809382	11.176295
10.200837	892.139400	11.181312
9.811432	893.415500	11.186330
10.101590	878.676583	11.191347
10.253031	885.075416	11.196365
10.042632	888.824740	11.201383
10.064759	887.791643	11.206400
10.215786	895.136154	11.211418
10.462942	889.221494	11.216435
10.108320	905.901005	11.221453
10.410164	890.642846	11.226471
10.289720	895.581073	11.231488
9.801164	894.007707	11.236506
10.252381	891.112267	11.241523
9.962060	900.749085	11.246541
10.189118	891.552948	11.251559
10.228186	892.857230	11.256576
10.229373	894.272132	11.261594
10.166201	897.088780	11.266611
10.093991	892.277527	11.271629
9.958078	897.740338	11.276647
9.872804	890.125935	11.281664
9.736971	892.285808	11.286682
9.944890	893.309088	11.291699
9.988934	904.260118	11.296717
10.414434	916.780516	11.301735
10.491238	916.603035	11.306752
10.673552	930.327569	11.311770
10.485090	899.883996	11.316787
10.124947	902.969283	11.321805
10.280257	900.322423	11.326823
10.297785	891.617776	11.331840
10.454337	909.687027	11.336858
10.496875	902.869428	11.341875
10.311498	900.531542	11.346893
10.338120	901.916825	11.351911
10.295552	910.750708	11.356928
10.379051	914.113610	11.361946
10.867122	916.805171	11.366963
10.878919	911.692566	11.371981
10.350827	893.638300	11.376999
10.466978	887.310604	11.382016
10.007195	888.605685	11.387034
10.696814	893.668695	11.392051
10.539304	895.890238	11.397069
10.244833	887.627781	11.402087
10.604987	905.274628	11.407104
10.456380	914.375531	11.412122
10.523045	910.783231	11.417139
10.458061	920.165100	11.422157
10.563979	924.886393	11.427175
10.752274	919.046659	11.432192
10.466266	915.463376	11.437210
10.735924	906.962859	11.442227
10.540053	908.750455	11.447245
10.644166	916.206704	11.452263
10.708288	909.465628	11.457280
10.409097	908.354649	11.462298
10.575890	914.406478	11.467315
10.463801	915.914418	11.472333
10.466128	920.375978	11.477351
10.808616	919.917343	11.482368
10.302317	927.720910	11.487386
10.266449	930.221825	11.492403
10.430561	924.742187	11.497421
10.188509	928.395017	11.502439
10.342688	923.642968	11.507456
10.201350	929.368092	11.512474
10.666933	941.625958	11.517491
10.779661	948.441462	11.522509
10.834975	955.046842	11.527527
11.140393	954.424890	11.532544
10.690620	955.507893	11.537562
10.891183	957.177241	11.542579
10.958205	941.587615	11.547597
10.849218	943.169054	11.552615
10.712252	919.036554	11.557632
10.251729	929.408916	11.562650
10.791322	946.010498	11.567667
10.877230	957.499454	11.572685
10.730171	960.434775	11.577703
10.799931	956.927771	11.582720
10.652134	957.481476	11.587738
10.869218	952.258756	11.592755
10.902021	954.144165	11.597773
10.989231	963.343292	11.602791
11.172242	950.234220	11.607808
11.088961	952.010980	11.612826
11.028531	948.127613	11.617843
11.258860	945.751328	11.622861
10.802501	960.632570	11.627879
11.005864	944.692347	11.632896
11.020199	954.192146	11.637914
11.383600	951.964991	11.642931
11.414838	938.399297	11.647949
10.724782	935.966170	11.652967
10.666271	931.721095	11.657984
10.741393	945.230994	11.663002
10.526771	946.785506	11.668019
10.467270	955.178753	11.673037
10.508966	955.366336	11.678055
11.227463	945.320420	11.683072
11.050962	948.627538	11.688090
10.760474	948.331395	11.693107
10.895115	945.496243	11.698125
11.394927	976.546652	11.703143
11.552736	961.205286	11.708160
11.325836	963.857440	11.713178
11.474864	954.181354	11.718195
11.481292	947.337851	11.723213
11.102801	956.578165	11.728231
11.162649	955.040400	11.733248
11.212001	949.674706	11.738266
11.105564	950.256573	11.743283
11.052329	952.020859	11.748301
11.096805	958.179645	11.753319
11.395412	945.917841	11.758336
11.122721	958.756085	11.763354
11.358963	954.104552	11.768371
11.443569	945.608396	11.773389
11.033016	956.326779	11.778407
11.501801	951.960195	11.783424
11.118675	959.630515	11.788442
11.086744	950.757296	11.793459
11.492710	953.415270	11.798477
11.181586	952.242299	11.803495
11.195020	960.879316	11.808512
10.978814	960.377137	11.813530
11.037711	959.644203	11.818547
11.213618	978.621675	11.823565
11.232314	987.560962	11.828583
11.791282	982.767594	11.833600
11.759919	985.444333	11.838618
11.355290	984.002667	11.843635
11.627936	973.524181	11.848653
11.650454	968.079481	11.853671
11.537929	948.606161	11.858688
11.433295	955.047981	11.863706
11.178103	944.872592	11.868723
11.451082	957.120953	11.873741
11.279751	961.187795	11.878759
11.509832	977.010792	11.883776
11.520108	977.703173	11.888794
11.453692	983.206821	11.893811
11.758535	975.501943	11.898829
11.679759	985.410127	11.903847
11.704145	964.405856	11.908864
11.657063	962.893738	11.913882
11.360145	951.332848	11.918899
11.604359	954.654282	11.923917
11.466996	970.266713	11.928935
11.983540	977.560743	11.933952
11.882005	959.574859	11.938970
11.795605	951.119722	11.943987
11.897149	941.146833	11.949005
11.581892	953.554381	11.954023
11.524699	940.947024	11.959040
11.596117	942.246917	11.964058
11.587528	943.197927	11.969075
11.724632	948.088638	11.974093
11.395751	943.584189	11.979111
11.664752	944.357571	11.984128
11.752926	964.825892	11.989146
11.850842	977.216747	11.994163
11.982495	964.906306	11.999181
11.986799	961.598359	12.004199
11.985854	943.966616	12.009216
11.915826	954.624852	12.014234
11.610754	951.917115	12.019251
11.812319	943.159016	12.024269
11.259030	949.912008	12.029287
11.801346	960.801121	12.034304
11.832731	969.610738	12.039322
12.022800	982.089028	12.044339
12.269470	975.325258	12.049357
11.840706	965.575924	12.054375
11.866153	957.285646	12.059392
11.725837	948.411154	12.064410
11.453819	948.134774	12.069427
11.837430	961.116276	12.074445
11.506542	978.429279	12.079463
11.570282	976.405857	12.084480
11.268916	984.314946	12.089498
11.639841	987.555880	12.094515
11.866413	984.189724	12.099533
11.786060	985.349898	12.104551
12.222801	997.077007	12.109568
12.073603	992.113963	12.114586
11.913278	995.733736	12.119603
11.839684	993.017828	12.124621
11.622939	1012.745212	12.129639
12.026520	1004.062549	12.134656
12.294637	1013.176520	12.139674
12.303981	1016.872421	12.144691
12.403006	1004.033547	12.149709
12.264829	1008.149217	12.154727
12.465196	991.341387	12.159744
12.410342	986.646110	12.164762
11.786015	990.594173	12.169779
12.230592	981.219317	12.174797
12.207884	986.377534	12.179815
12.060803	991.254475	12.184832
12.435880	985.660621	12.189850
11.991737	980.117512	12.194867
12.204805	987.665127	12.199885
12.363877	995.235499	12.204903
12.373660	986.172267	12.209920
12.265914	988.099545	12.214938
11.930877	991.647970	12.219955
11.848905	985.395486	12.224973
12.525569	1009.779185	12.229991
12.218978	1003.325462	12.235008
12.244325	1001.551710	12.240026
11.917542	1014.552918	12.245043
12.456608	1005.864661	12.250061
12.314507	1006.059963	12.255079
12.202419	1014.248216	12.260096
12.342299	1004.113018	12.265114
12.141883	1017.875461	12.270131
12.236160	1010.002428	12.275149
12.395378	1017.349966	12.280167
12.552932	1008.442462	12.285184
12.571075	1014.400935	12.290202
12.056302	1016.895843	12.295219
12.570539	1014.320791	12.300237
12.134165	1010.372740	12.305255
12.288744	1018.702092	12.310272
12.668759	1008.173848	12.315290
12.462919	1012.966868	12.320307
12.537490	1011.401062	12.325325
12.550946	1016.186370	12.330343
12.366539	1013.647924	12.335360
12.605486	1009.675411	12.340378
12.504620	1010.088648	12.345395
12.104068	1006.604694	12.350413
12.133251	1017.795662	12.355431
12.494423	1034.225236	12.360448
13.021220	1039.036242	12.365466
12.713939	1028.535223	12.370483
12.401458	1019.229098	12.375501
12.393116	1026.806842	12.380519
12.549602	1043.069674	12.385536
12.982146	1035.379758	12.390554
12.743364	1047.438862	12.395571
12.653029	1037.625356	12.400589
12.471682	1044.135867	12.405607
12.780724	1044.710484	12.410624
12.885706	1037.485226	12.415642
12.737172	1048.701033	12.420659
12.854842	1041.665779	12.425677
12.648000	1044.476021	12.430695
12.711663	1046.389381	12.435712
12.792156	1043.488413	12.440730
12.522397	1050.606894	12.445747
12.651922	1045.022734	12.450765
12.826089	1039.269748	12.455783
12.941373	1048.579607	12.460800
12.918198	1044.578219	12.465818
12.361127	1045.280660	12.470835
12.727579	1049.254985	12.475853
12.660695	1039.872988	12.480871
12.673339	1035.067270	12.485888
12.773552	1033.158636	12.490906
12.793994	1048.044956	12.495923
13.224998	1039.507706	12.500941
12.999516	1051.464608	12.505959
12.938401	1048.618277	12.510976
12.933814	1038.413768	12.515994
12.788737	1044.072237	12.521011
12.904506	1045.963157	12.526029
12.635130	1041.043694	12.531047
12.700595	1043.727969	12.536064
12.923966	1051.261304	12.541082
12.955694	1067.825591	12.546099
13.249975	1073.262231	12.551117
13.417355	1078.429824	12.556135
13.478285	1060.932931	12.561152
13.541222	1045.169481	12.566170
13.043400	1047.117906	12.571187
12.978427	1049.798274	12.576205
13.007814	1040.311697	12.581223
12.798323	1048.409472	12.586240
13.367181	1044.232909	12.591258
13.031933	1049.371841	12.596275
13.102174	1042.272821	12.601293
13.217262	1035.329333	12.606311
12.959306	1039.523186	12.611328
13.267618	1045.978289	12.616346
13.170111	1066.445327	12.621363
13.238428	1071.809689	12.626381
13.815584	1073.521958	12.631399
13.134331	1063.782250	12.636416
13.255693	1035.240935	12.641434
13.027285	1048.130549	12.646451
13.498120	1063.900232	12.651469
13.389315	1065.839900	12.656487
13.189117	1065.902347	12.661504
13.086126	1060.625319	12.666522
13.095478	1063.035082	12.671539
13.060658	1073.495432	12.676557
13.191610	1071.159662	12.681575
13.084642	1082.729587	12.686592
13.173831	1074.290863	12.691610
12.973179	1077.269757	12.696627
12.934000	1071.420339	12.701645
13.474867	1090.242802	12.706663
13.559590	1102.893416	12.711680
13.723288	1101.546632	12.716698
13.547264	1094.897948	12.721715
13.166603	1091.505545	12.726733
13.619596	1090.390581	12.731751
13.702994	1096.455949	12.736768
13.783323	1092.531040	12.741786
13.816664	1091.057113	12.746803
13.684117	1076.137891	12.751821
13.532229	1072.383862	12.756839
13.435467	1072.626349	12.761856
13.701125	1063.510698	12.766874
13.671759	1065.707225	12.771891
13.652512	1072.303001	12.776909
13.490923	1068.289970	12.781927
13.408814	1067.016722	12.786944
13.330467	1073.092038	12.791962
13.580137	1087.245844	12.796979
13.672482	1102.032867	12.801997
13.990887	1098.609299	12.807015
13.955238	1105.870379	12.812032
13.822488	1084.575545	12.817050
13.695133	1073.247783	12.822067
13.702770	1077.620321	12.827085
13.820339	1089.834387	12.832103
13.734008	1090.820768	12.837120
13.931670	1087.343261	12.842138
13.504445	1084.803827	12.847155
13.837685	1098.365832	12.852173
13.997726	1094.921740	12.857191
13.989652	1113.233934	12.862208
14.074736	1087.782638	12.867226
13.894471	1087.241018	12.872243
13.698458	1068.550280	12.877261
14.134850	1076.676531	12.882279
14.092383	1077.082031	12.887296
13.832645	1062.330018	12.892314
13.728725	1062.596922	12.897331
13.629619	1073.073469	12.902349
14.179638	1084.397979	12.907367
13.956363	1106.057168	12.912384
14.009803	1096.726786	12.917402
13.970288	1093.931972	12.922419
13.747801	1104.215280	12.927437
13.983107	1095.577071	12.932455
13.779376	1097.491185	12.937472
14.295550	1102.173275	12.942490
13.924453	1094.153549	12.947507
13.985098	1092.683352	12.952525
14.092089	1088.780782	12.957543
13.974641	1104.133751	12.962560
14.218086	1093.031333	12.967578
14.306903	1102.979447	12.972595
14.149938	1094.504861	12.977613
14.416456	1085.042223	12.982631
14.236409	1095.944815	12.987648
14.029042	1097.957953	12.992666
14.074273	1096.928088	12.997683
13.959798	1090.271538	13.002701
14.083393	1086.035519	13.007719
13.971119	1106.596791	13.012736
14.126811	1096.693931	13.017754
13.915229	1092.680936	13.022771
14.030826	1102.473426	13.027789
14.760733	1102.850538	13.032807
14.438734	1114.007040	13.037824
14.525777	1092.272141	13.042842
14.241081	1100.695419	13.047859
14.347819	1097.176332	13.052877
14.396805	1095.549026	13.057895
14.285621	1095.364407	13.062912
14.428998	1101.255643	13.067930
14.426040	1102.267535	13.072947
14.479749	1103.032620	13.077965
14.546917	1087.541636	13.082983
14.542951	1105.675983	13.088000
14.716990	1094.708322	13.093018
14.386542	1091.933128	13.098035
13.960688	1092.406291	13.103053
14.580289	1100.465883	13.108071
14.449023	1117.022672	13.113088
14.503679	1123.036532	13.118106
14.619079	1119.440807	13.123123
14.609853	1127.086461	13.128141
14.906936	1113.324465	13.133159
14.732937	1122.383256	13.138176
14.601113	1111.778611	13.143194
14.303145	1111.347888	13.148211
14.458717	1123.906038	13.153229
15.380945	1119.643556	13.158247
14.445595	1104.066844	13.163264
14.524584	1116.495600	13.168282
14.722319	1120.546017	13.173299
14.714641	1125.845869	13.178317
14.651186	1127.815799	13.183335
14.506268	1122.729174	13.188352
14.712961	1122.437783	13.193370
14.636521	1122.121804	13.198387
14.598545	1119.541679	13.203405
14.834582	1110.752954	13.208423
14.682004	1119.817631	13.213440
14.656443	1123.250869	13.218458
14.762298	1122.342021	13.223475
14.463814	1131.605752	13.228493
14.838543	1122.727435	13.233511
14.567904	1128.948115	13.238528
14.841268	1125.026936	13.243546
14.603755	1122.110312	13.248563
14.624742	1144.764332	13.253581
14.996184	1142.141739	13.258599
15.058140	1149.823994	13.263616
15.148261	1146.659215	13.268634
15.625745	1137.723655	13.273651
15.524839	1134.694956	13.278669
15.595659	1111.443515	13.283687
15.481524	1113.500604	13.288704
14.910213	1113.487342	13.293722
15.385373	1111.254186	13.298739
14.943538	1117.478909	13.303757
15.069732	1120.126726	13.308775
15.167639	1113.439195	13.313792
15.074960	1115.450988	13.318810
15.717883	1114.913869	13.323827
15.154251	1113.130135	13.328845
15.341793	1103.665259	13.333863
15.205515	1115.084971	13.338880
15.052978	1107.218663	13.343898
15.052019	1109.340006	13.348915
14.456917	1114.186343	13.353933
14.746253	1107.706352	13.358951
15.099992	1122.039338	13.363968
15.008838	1125.559460	13.368986
15.294162	1120.067874	13.374003
14.881732	1124.066965	13.379021
15.460953	1129.661763	13.384039
15.127190	1128.088231	13.389056
15.021263	1135.849169	13.394074
15.519584	1146.582744	13.399091
15.264555	1155.564870	13.404109
15.257069	1142.431791	13.409127
15.388748	1156.819435	13.414144
15.253697	1146.011770	13.419162
15.742905	1145.411228	13.424179
15.323404	1156.303273	13.429197
15.772466	1149.058171	13.434215
15.415272	1151.796184	13.439232
15.291692	1144.293923	13.444250
15.546125	1141.369537	13.449267
15.770518	1155.316201	13.454285
15.760205	1141.375366	13.459303
15.587515	1145.583812	13.464320
15.690764	1154.037119	13.469338
16.052042	1138.172412	13.474355
15.740032	1133.554478	13.479373
15.510288	1111.226573	13.484391
15.517022	1112.194731	13.489408
15.267351	1112.421298	13.494426
15.892279	1124.192023	13.499443
15.495859	1128.120347	13.504461
15.514984	1126.862943	13.509479
15.477826	1141.182972	13.514496
15.477243	1147.190670	13.519514
15.920834	1139.960260	13.524531
15.783312	1149.126384	13.529549
15.847820	1139.894918	13.534567
15.831102	1144.887633	13.539584
15.965002	1142.543488	13.544602
15.982588	1139.163220	13.549619
15.699136	1147.607575	13.554637
15.734863	1147.610336	13.559655
15.986519	1148.894067	13.564672
15.687166	1151.195715	13.569690
15.553849	1143.807273	13.574707
15.284819	1146.949900	13.579725
15.690758	1151.894016	13.584743
15.777508	1140.469989	13.589760
15.568613	1143.202641	13.594778
15.580381	1140.043014	13.599795
15.604202	1148.855958	13.604813
16.144069	1168.888858	13.609831
16.263513	1176.037581	13.614848
15.804010	1175.928573	13.619866
16.053908	1177.330309	13.624883
16.351497	1174.899506	13.629901
16.211430	1172.962687	13.634919
15.799550	1154.802976	13.639936
15.618972	1170.008638	13.644954
16.128152	1164.291648	13.649971
15.970366	1174.243399	13.654989
15.940729	1174.304660	13.660007
16.029985	1173.087560	13.665024
16.005474	1173.338117	13.670042
16.205047	1173.334115	13.675059
16.228668	1170.992549	13.680077
16.133053	1173.632364	13.685095
16.446057	1170.760438	13.690112
16.425529	1176.433290	13.695130
16.547758	1169.496035	13.700147
16.613161	1164.001227	13.705165
16.484751	1169.544378	13.710183
16.423661	1166.975960	13.715200
16.368802	1176.289375	13.720218
16.740951	1177.056255	13.725235
16.608983	1175.577909	13.730253
16.683936	1152.430046	13.735271
16.361101	1132.704458	13.740288
16.241805	1138.123255	13.745306
16.381191	1135.743161	13.750323
16.366720	1143.379065	13.755341
16.302239	1159.951962	13.760359
16.820580	1161.044523	13.765376
16.691764	1157.337029	13.770394
16.918297	1140.673893	13.775411
16.436291	1140.285570	13.780429
16.452718	1124.656928	13.785447
16.303301	1127.974935	13.790464
16.186507	1132.150072	13.795482
16.602407	1150.648125	13.800499
16.234406	1160.845033	13.805517
16.373943	1169.693084	13.810535
16.353733	1162.154736	13.815552
16.319838	1168.984079	13.820570
16.756351	1166.436489	13.825587
16.809640	1169.110212	13.830605
16.252419	1170.656341	13.835623
16.758427	1169.430203	13.840640
16.357487	1169.064623	13.845658
16.675862	1165.057216	13.850675
16.182546	1175.760373	13.855693
16.527752	1182.339711	13.860711
16.741161	1190.334984	13.865728
16.753680	1201.633180	13.870746
16.876031	1199.284648	13.875763
17.227633	1209.543465	13.880781
17.391060	1196.198869	13.885799
17.114675	1179.292136	13.890816
16.997465	1168.820448	13.895834
16.960977	1157.936945	13.900851
17.236386	1157.926243	13.905869
17.111768	1158.359573	13.910887
17.075448	1154.541434	13.915904
16.882743	1163.614775	13.920922
17.008798	1152.789293	13.925939
16.985944	1158.485753	13.930957
16.697387	1147.927999	13.935975
17.163246	1150.885093	13.940992
16.778029	1160.113259	13.946010
17.017923	1151.531734	13.951027
16.964168	1153.442971	13.956045
16.933147	1166.103034	13.961063
17.118133	1168.470235	13.966080
17.187203	1182.243145	13.971098
17.282476	1176.366614	13.976115
17.170856	1174.928979	13.981133
17.312832	1182.312138	13.986151
17.340973	1156.571783	13.991168
17.025038	1162.035478	13.996186
17.499633	1158.439879	14.001203
17.289470	1149.724511	14.006221
17.043057	1159.651222	14.011239
17.095630	1164.047417	14.016256
17.130172	1180.804654	14.021274
16.923724	1186.511169	14.026291
16.992035	1182.975223	14.031309
17.188606	1186.885701	14.036327
17.363311	1175.550173	14.041344
17.138163	1182.854991	14.046362
17.437198	1173.781757	14.051379
17.349735	1185.072939	14.056397
17.213560	1182.330394	14.061415
17.323633	1187.764624	14.066432
17.065078	1191.900745	14.071450
17.426025	1200.093930	14.076467
17.542766	1214.521512	14.081485
17.448480	1214.509270	14.086503
17.663278	1212.128441	14.091520
17.366610	1224.042980	14.096538
17.593382	1221.022394	14.101555
17.610970	1222.093080	14.106573
17.213178	1229.367170	14.111591
17.277620	1219.599473	14.116608
17.205248	1220.121359	14.121626
17.647649	1215.019753	14.126643
17.577728	1211.507958	14.131661
17.681249	1218.277477	14.136679
17.983954	1210.009479	14.141696
17.850943	1212.655911	14.146714
17.945484	1207.888492	14.151731
17.759582	1220.019251	14.156749
17.822347	1217.248357	14.161767
18.303228	1211.770688	14.166784
18.257524	1217.396955	14.171802
18.036499	1207.631835	14.176819
18.074735	1214.019702	14.181837
18.008378	1215.610616	14.186855
17.903361	1192.392218	14.191872
17.864516	1199.083428	14.196890
17.922368	1194.527614	14.201907
18.193005	1193.473661	14.206925
17.723015	1187.923355	14.211943
17.757562	1192.579628	14.216960
17.709845	1201.256075	14.221978
17.643448	1202.908016	14.226995
18.158653	1208.121377	14.232013
17.744953	1216.263024	14.237031
18.084616	1205.784659	14.242048
17.829743	1214.206190	14.247066
17.892066	1212.423119	14.252083
17.921718	1214.948424	14.257101
17.860450	1215.195642	14.262119
18.056080	1222.441955	14.267136
17.911653	1216.925315	14.272154
17.925463	1217.354927	14.277171
18.599682	1225.750768	14.282189
18.405703	1237.387237	14.287207
18.223484	1216.564596	14.292224
18.179225	1219.365560	14.297242
18.053072	1212.576259	14.302259
18.239390	1227.567063	14.307277
18.117131	1241.293091	14.312295
18.428308	1236.740038	14.317312
18.730246	1245.549327	14.322330
18.574442	1227.988668	14.327347
18.332056	1220.353763	14.332365
18.311453	1216.273166	14.337383
18.306672	1223.229972	14.342400
18.225486	1233.605228	14.347418
18.291216	1241.936085	14.352435
18.527784	1237.761164	14.357453
18.457860	1244.120566	14.362471
18.816050	1240.900581	14.367488
18.876024	1249.043037	14.372506
18.434916	1237.283862	14.377523
18.932715	1225.590277	14.382541
18.166954	1227.694278	14.387559
18.479761	1228.945805	14.392576
18.976719	1237.303402	14.397594
18.759491	1236.743512	14.402611
18.565443	1216.657056	14.407629
18.544776	1241.000738	14.412647
18.745891	1231.345349	14.417664
18.591270	1242.544591	14.422682
18.352216	1245.775164	14.427699
18.639699	1237.974621	14.432717
18.457908	1250.877127	14.437735
18.732027	1246.776667	14.442752
19.064099	1239.210040	14.447770
18.587980	1245.168870	14.452787
18.686367	1235.529373	14.457805
18.475336	1246.904916	14.462823
18.596902	1234.926238	14.467840
18.662484	1233.617404	14.472858
18.828078	1241.499397	14.477875
19.001448	1239.191195	14.482893
18.698348	1234.113109	14.487911
18.807173	1238.256679	14.492928
19.017862	1250.377838	14.497946
18.846371	1261.040158	14.502963
19.156432	1264.545194	14.507981
19.219221	1266.194172	14.512999
19.124630	1242.455484	14.518016
19.066683	1235.122577	14.523034
18.855692	1237.524506	14.528051
18.457449	1241.658270	14.533069
18.670047	1264.571548	14.538087
19.099061	1258.116701	14.543104
19.411561	1261.746917	14.548122
19.080647	1266.665130	14.553139
19.446366	1266.680360	14.558157
19.208357	1260.368272	14.563175
19.500893	1265.602129	14.568192
19.407465	1264.605930	14.573210
19.422297	1268.580887	14.578227
19.607116	1261.021010	14.583245
19.513620	1269.994069	14.588263
19.592929	1255.206381	14.593280
19.610785	1240.913939	14.598298
19.319933	1244.011396	14.603315
19.587149	1226.501286	14.608333
18.981531	1227.842876	14.613351
19.164921	1235.495541	14.618368
19.515084	1255.261674	14.623386
19.269022	1264.652591	14.628403
19.391432	1261.898938	14.633421
19.569345	1257.800688	14.638439
19.262645	1257.539120	14.643456
19.428772	1255.066379	14.648474
19.291430	1265.864752	14.653491
19.657119	1258.288198	14.658509
19.533440	1261.115755	14.663527
19.587978	1261.581117	14.668544
19.725030	1255.421640	14.673562
19.267820	1268.056173	14.678579
19.581992	1247.192713	14.683597
19.416347	1248.041507	14.688615
19.643518	1260.653220	14.693632
19.779718	1259.920808	14.698650
19.289623	1246.632829	14.703667
19.689103	1268.062360	14.708685
20.104650	1282.015553	14.713703
19.826610	1271.110312	14.718720
19.882390	1263.328586	14.723738
19.605396	1275.982381	14.728755
19.903412	1271.004752	14.733773
20.121528	1282.377884	14.738791
19.959954	1275.148793	14.743808
20.251290	1261.197079	14.748826
19.938361	1262.414040	14.753843
19.946690	1244.733171	14.758861
19.784620	1254.805759	14.763879
19.855917	1256.614338	14.768896
20.198465	1272.961440	14.773914
20.194827	1267.682786	14.778931
19.902738	1257.376715	14.783949
19.635665	1272.503157	14.788967
20.084670	1279.365664	14.793984
20.251286	1278.380963	14.799002
20.033535	1292.296129	14.804019
20.318324	1283.489755	14.809037
20.116623	1282.954052	14.814055
19.985019	1285.058160	14.819072
20.392672	1284.239290	14.824090
20.002002	1286.440000	14.829107
20.202065	1279.972021	14.834125
20.052741	1265.958908	14.839143
20.316306	1286.128435	14.844160
20.618439	1282.553207	14.849178
19.962988	1293.829828	14.854195
20.411938	1285.818178	14.859213
20.419312	1288.999139	14.864231
20.522491	1288.012777	14.869248
20.586316	1283.319336	14.874266
20.479229	1285.514246	14.879283
20.698625	1288.901293	14.884301
20.642563	1285.713935	14.889319
20.494099	1284.718616	14.894336
20.590900	1283.530961	14.899354
20.319150	1286.328019	14.904371
20.738078	1277.974135	14.909389
20.667710	1279.912558	14.914407
20.564244	1284.259136	14.919424
20.864158	1277.363555	14.924442
20.557214	1280.968003	14.929459
20.438129	1275.561298	14.934477
20.489643	1274.562659	14.939495
20.889096	1281.713706	14.944512
20.644363	1279.539952	14.949530
20.715938	1290.792572	14.954547
20.802263	1276.833190	14.959565
20.659800	1286.160445	14.964583
20.659688	1290.179622	14.969600
21.212850	1281.182190	14.974618
20.867091	1283.126233	14.979635
20.810321	1274.009330	14.984653
20.419393	1284.556965	14.989671
20.634653	1284.663738	14.994688
20.766861	1275.978394	14.999706
20.298607	1278.288451	15.004723
20.734973	1281.707146	15.009741
20.872541	1280.496181	15.014759
21.056402	1294.758750	15.019776
20.982864	1297.998435	15.024794
20.631529	1300.116627	15.029811
20.827188	1296.821288	15.034829
20.998362	1303.254416	15.039847
21.089348	1296.873849	15.044864
21.232527	1306.893370	15.049882
21.057999	1309.105399	15.054899
21.135649	1302.880583	15.059917
21.316290	1303.880080	15.064935
20.663448	1301.333231	15.069952
21.160625	1306.505136	15.074970
21.243338	1306.930384	15.079987
21.232876	1305.627491	15.085005
21.669850	1300.488966	15.090023
21.289755	1311.171034	15.095040
21.664322	1300.014785	15.100058
21.262060	1307.999860	15.105075
21.384181	1300.277164	15.110093
21.301901	1305.304056	15.115111
21.217137	1309.003071	15.120128
21.642818	1298.697346	15.125146
21.276917	1305.058728	15.130163
20.997089	1307.043387	15.135181
21.313913	1294.897568	15.140199
21.012374	1305.907112	15.145216
21.365657	1315.859828	15.150234
21.631203	1327.301484	15.155251
21.827930	1325.892107	15.160269
22.284388	1315.424175	15.165287
21.685799	1312.147075	15.170304
21.844528	1287.150909	15.175322
21.694283	1293.943349	15.180339
21.753151	1294.215087	15.185357
22.044610	1286.448110	15.190375
21.636243	1280.129685	15.195392
21.825564	1286.756631	15.200410
21.734871	1290.209787	15.205427
21.841313	1295.420652	15.210445
21.866687	1288.833680	15.215463
21.648761	1295.691307	15.220480
21.682630	1286.099114	15.225498
21.807773	1282.708023	15.230515
21.889257	1289.133613	15.235533
21.857951	1288.856583	15.240551
21.644146	1295.199373	15.245568
21.992844	1289.185011	15.250586
22.021008	1298.740201	15.255603
22.002205	1295.751364	15.260621
22.181848	1291.581954	15.265639
21.828797	1295.659796	15.270656
21.988845	1305.902095	15.275674
22.204430	1317.613455	15.280691
22.148137	1321.777406	15.285709
22.394956	1312.263183	15.290727
22.299798	1302.428264	15.295744
22.065998	1291.960518	15.300762
22.131864	1295.951014	15.305779
22.104649	1293.931645	15.310797
22.046948	1302.138175	15.315815
21.959573	1317.750126	15.320832
22.440519	1316.328939	15.325850
22.109467	1314.763991	15.330867
22.372582	1317.796154	15.335885
22.612924	1319.687268	15.340903
22.020024	1329.751203	15.345920
22.350122	1321.364819	15.350938
22.146032	1319.988601	15.355955
22.048988	1325.424236	15.360973
22.462291	1317.962568	15.365991
22.293562	1326.345039	15.371008
22.561455	1319.274848	15.376026
22.503187	1326.429953	15.381043
22.416508	1318.071508	15.386061
22.641458	1315.275214	15.391079
22.512893	1317.864627	15.396096
22.655822	1315.215818	15.401114
22.585324	1315.121673	15.406131
22.557414	1316.383386	15.411149
22.645305	1316.603845	15.416167
22.679047	1317.388794	15.421184
22.627295	1318.490697	15.426202
22.514360	1326.361553	15.431219
22.693515	1343.619711	15.436237
23.004976	1343.740808	15.441255
22.846860	1353.547852	15.446272
22.903858	1342.012878	15.451290
22.953776	1341.841633	15.456307
23.020116	1344.796671	15.461325
23.519987	1333.802634	15.466343
22.891608	1324.094518	15.471360
22.990998	1306.255929	15.476378
22.909146	1314.453094	15.481395
22.574928	1312.272162	15.486413
22.923057	1321.127359	15.491431
22.903370	1336.346204	15.496448
23.319903	1335.132958	15.501466
23.171831	1343.724595	15.506483
22.840333	1343.151018	15.511501
22.911910	1337.853146	15.516519
22.900375	1342.312013	15.521536
23.052851	1341.113919	15.526554
22.827079	1346.806775	15.531571
22.393636	1356.836350	15.536589
22.675020	1337.918302	15.541607
22.977336	1353.806448	15.546624
23.172340	1366.466505	15.551642
23.194968	1369.768958	15.556659
23.057656	1371.924417	15.561677
23.307763	1361.885621	15.566695
24.020563	1355.780794	15.571712
24.183753	1338.349263	15.576730
24.340009	1327.606826	15.581747
24.231691	1317.020571	15.586765
24.462437	1299.399910	15.591783
24.212847	1297.574190	15.596800
24.263715	1283.869503	15.601818
24.271286	1280.704639	15.606835
23.834072	1285.302746	15.611853
24.243690	1260.832611	15.616871
23.891191	1259.611770	15.621888
23.993601	1250.564874	15.626906
23.792875	1248.226730	15.631923
23.834353	1247.157717	15.636941
24.144733	1242.872105	15.641959
24.011632	1251.377348	15.646976
24.011114	1243.599477	15.651994
23.648039	1252.355928	15.657011
23.872995	1245.735014	15.662029
24.046696	1240.068641	15.667047
24.062272	1245.462302	15.672064
23.919289	1242.205940	15.677082
23.954203	1220.845650	15.682099
23.741159	1227.303634	15.687117
23.925880	1219.580021	15.692135
23.856917	1233.392849	15.697152
23.902540	1234.636821	15.702170
24.199272	1246.256297	15.707187
23.760118	1233.425588	15.712205
24.134895	1240.418915	15.717223
24.308728	1236.144190	15.722240
23.902474	1233.617779	15.727258
24.154447	1236.986015	15.732275
24.130755	1241.404750	15.737293
24.120311	1227.023328	15.742311
23.876843	1231.518353	15.747328
23.864492	1230.530332	15.752346
24.321207	1235.277070	15.757363
23.929077	1237.449670	15.762381
24.266702	1229.441594	15.767399
24.057850	1245.460260	15.772416
23.884732	1237.256771	15.777434
24.227136	1245.559752	15.782451
24.129005	1267.281433	15.787469
24.331809	1269.716945	15.792487
24.138446	1274.045393	15.797504
24.306646	1270.984929	15.802522
24.403176	1265.436487	15.807539
24.219927	1282.130040	15.812557
24.363009	1275.751845	15.817575
24.592098	1278.146771	15.822592
24.266107	1272.089448	15.827610
24.137641	1276.118146	15.832627
24.128397	1275.832332	15.837645
24.315702	1292.204078	15.842663
24.377503	1308.402616	15.847680
24.194539	1306.204418	15.852698
24.380943	1302.933056	15.857715
24.037431	1306.556186	15.862733
24.694088	1297.675001	15.867751
24.564633	1315.614714	15.872768
24.609631	1329.263809	15.877786
24.911648	1339.243171	15.882803
24.913952	1340.876227	15.887821
24.733717	1340.908192	15.892839
24.983440	1348.642011	15.897856
24.863110	1349.254546	15.902874
24.791429	1350.315278	15.907891
24.573873	1350.239277	15.912909
24.706347	1345.930454	15.917927
25.160865	1344.460116	15.922944
24.967541	1345.226905	15.927962
25.095059	1351.291340	15.932979
24.964460	1345.819991	15.937997
24.893461	1343.300826	15.943015
24.752095	1348.413534	15.948032
24.685211	1354.618152	15.953050
25.255742	1349.241673	15.958067
24.814466	1369.539094	15.963085
24.778026	1369.402281	15.968103
24.885920	1358.095047	15.973120
24.937131	1379.199170	15.978138
25.241202	1365.061789	15.983155
25.033368	1376.354221	15.988173
25.239161	1372.672551	15.993191
25.228601	1386.793512	15.998208
25.369112	1390.675959	16.003226
25.450377	1398.391742	16.008243
25.511817	1404.635285	16.013261
25.707641	1396.323932	16.018279
26.057080	1388.881507	16.023296
25.518811	1379.170977	16.028314
26.095360	1357.679133	16.033331
25.607287	1369.308680	16.038349
25.659111	1354.791598	16.043367
25.801298	1359.000912	16.048384
25.704816	1354.988794	16.053402
25.814199	1349.700775	16.058419
25.434399	1359.284837	16.063437
25.796878	1358.819129	16.068455
26.272258	1352.481730	16.073472
25.904723	1356.529320	16.078490
26.045462	1354.339906	16.083507
25.885999	1358.543849	16.088525
25.788195	1353.988665	16.093543
25.708800	1356.869901	16.098560
25.892628	1361.325041	16.103578
25.670897	1350.067483	16.108595
25.703128	1359.509835	16.113613
25.846782	1361.177270	16.118631
25.980030	1383.386619	16.123648
25.888926	1385.230080	16.128666
26.416639	1381.397659	16.133683
26.167642	1385.353902	16.138701
26.416351	1384.441767	16.143719
26.437388	1364.374877	16.148736
25.782188	1363.779122	16.153754
26.484275	1367.237131	16.158771
26.180501	1371.435932	16.163789
26.403519	1369.665895	16.168807
26.328853	1364.425785	16.173824
26.262992	1356.985477	16.178842
26.227038	1357.383996	16.183859
26.028037	1371.205963	16.188877
26.075842	1388.560018	16.193895
26.203935	1383.251555	16.198912
26.271318	1388.766177	16.203930
26.741943	1381.039843	16.208947
26.251731	1386.040475	16.213965
26.552838	1384.991682	16.218983
26.696945	1384.065044	16.224000
26.579921	1386.349018	16.229018
26.449150	1385.273588	16.234035
26.205478	1394.210659	16.239053
26.662559	1380.907642	16.244071
26.718373	1382.308195	16.249088
26.483834	1378.678847	16.254106
26.638096	1384.645152	16.259123
26.530943	1381.840662	16.264141
26.681574	1381.533784	16.269159
26.552135	1391.488442	16.274176
26.701848	1397.982655	16.279194
27.180027	1402.366834	16.284211
27.387302	1395.168895	16.289229
26.881768	1385.505673	16.294247
26.957666	1367.934293	16.299264
26.904518	1380.380107	16.304282
26.896275	1373.166427	16.309299
27.096237	1381.505755	16.314317
27.033599	1373.955066	16.319335
27.069648	1380.476431	16.324352
27.251885	1383.206708	16.329370
27.172853	1369.941238	16.334387
26.952241	1379.583889	16.339405
27.000614	1386.210685	16.344423
27.210993	1394.680568	16.349440
26.984065	1402.435374	16.354458
27.368828	1403.222610	16.359475
27.444339	1399.924387	16.364493
27.363857	1405.724607	16.369511
27.446428	1405.732967	16.374528
27.562836	1408.899766	16.379546
27.663322	1392.904138	16.384563
27.022233	1391.609998	16.389581
26.989327	1402.985181	16.394599
27.756299	1404.262412	16.399616
27.347090	1399.835743	16.404634
27.593323	1395.994989	16.409651
27.556607	1391.499322	16.414669
27.115950	1400.028208	16.419687
27.412623	1397.424301	16.424704
27.298200	1403.724239	16.429722
27.486179	1395.208687	16.434739
27.442978	1395.129295	16.439757
27.573930	1390.900631	16.444775
27.530657	1394.749850	16.449792
27.703978	1426.905005	16.454810
27.527751	1423.723813	16.459827
27.787793	1429.196979	16.464845
27.578901	1434.449674	16.469863
28.001332	1423.681037	16.474880
27.797207	1436.988577	16.479898
27.809459	1421.955979	16.484915
28.151565	1427.859190	16.489933
27.796470	1429.921332	16.494951
28.387938	1428.804590	16.499968
28.191388	1430.634876	16.504986
28.305136	1425.100444	16.510003
28.444342	1429.055951	16.515021
27.793022	1427.980036	16.520039
28.186218	1421.085816	16.525056
28.225349	1418.482195	16.530074
28.192583	1427.417298	16.535091
28.236802	1429.518184	16.540109
27.851572	1428.860623	16.545127
28.299405	1430.530262	16.550144
27.863551	1435.280149	16.555162
28.146417	1425.589004	16.560179
28.600415	1426.195055	16.565197
28.243534	1429.370449	16.570215
28.127304	1426.313138	16.575232
28.091867	1431.656683	16.580250
28.472500	1440.934485	16.585267
28.142064	1449.876167	16.590285
28.274935	1460.564804	16.595303
28.840536	1448.353106	16.600320
28.962568	1457.641619	16.605338
28.699498	1453.313475	16.610355
29.133709	1454.938137	16.615373
28.643144	1447.412872	16.620391
28.768293	1429.379314	16.625408
28.660294	1422.445175	16.630426
28.833014	1423.046405	16.635443
29.077114	1427.532883	16.640461
28.792956	1422.053961	16.645479
28.752611	1417.964781	16.650496
28.525645	1424.501143	16.655514
28.447964	1445.472062	16.660531
28.785058	1440.828424	16.665549
28.537859	1445.555225	16.670567
28.895581	1449.126002	16.675584
28.843200	1444.812446	16.680602
29.092999	1447.347652	16.685619
29.150539	1435.312928	16.690637
28.917976	1451.282994	16.695655
29.185265	1440.369271	16.700672
29.122201	1447.787032	16.705690
29.288490	1451.448682	16.710707
29.105509	1447.994600	16.715725
28.934544	1448.932869	16.720743
29.083301	1439.691158	16.725760
29.133982	1464.147738	16.730778
29.119380	1477.072247	16.735795
29.262666	1474.528861	16.740813
29.429856	1476.189641	16.745831
29.752080	1469.889856	16.750848
29.317696	1472.723821	16.755866
29.573620	1474.257651	16.760883
29.846536	1473.598172	16.765901
29.163207	1477.407346	16.770919
29.560300	1470.342383	16.775936
29.306396	1473.767197	16.780954
29.072283	1477.127307	16.785971
29.617154	1471.821191	16.790989
29.599036	1482.752650	16.796007
29.809063	1465.024618	16.801024
29.438612	1468.705016	16.806042
29.594010	1468.180028	16.811059
30.020823	1477.515923	16.816077
29.696652	1490.647011	16.821095
30.257991	1485.536966	16.826112
30.192784	1479.012606	16.831130
29.937774	1468.836445	16.836147
29.860305	1478.026638	16.841165
29.813187	1473.058282	16.846183
29.759896	1469.168479	16.851200
29.822590	1480.517986	16.856218
30.052284	1495.057760	16.861235
30.238360	1497.705139	16.866253
30.155083	1502.963356	16.871271
30.409656	1498.905448	16.876288
30.543273	1504.011082	16.881306
30.485110	1491.588078	16.886323
30.422014	1471.044497	16.891341
29.913986	1480.423182	16.896359
30.102728	1472.346424	16.901376
30.516251	1475.084730	16.906394
30.266338	1479.782466	16.911411
30.506420	1472.536519	16.916429
30.325227	1484.512769	16.921447
30.490974	1496.638050	16.926464
30.465175	1494.698338	16.931482
30.343954	1497.608992	16.936499
30.793280	1504.984525	16.941517
30.840456	1506.743207	16.946535
30.448636	1477.230107	16.951552
30.674098	1485.134164	16.956570
30.681606	1489.385190	16.961587
30.843777	1488.148860	16.966605
30.906085	1487.033457	16.971623
30.690671	1475.425162	16.976640
30.854255	1465.363673	16.981658
30.297208	1470.712437	16.986675
30.921925	1478.116284	16.991693
30.376379	1483.226533	16.996711
30.730046	1484.989386	17.001728
31.097766	1490.924190	17.006746
30.623893	1500.430277	17.011763
30.921616	1493.062538	17.016781
30.682786	1496.244701	17.021799
30.487347	1490.974624	17.026816
30.922367	1501.247330	17.031834
31.038223	1521.805485	17.036851
31.000322	1512.420746	17.041869
31.181514	1532.655072	17.046887
31.196334	1516.279866	17.051904
31.470468	1526.510435	17.056922
31.467986	1516.298174	17.061939
31.745088	1518.213124	17.066957
31.453633	1510.096480	17.071975
31.135884	1494.076959	17.076992
31.320411	1510.214366	17.082010
31.237055	1517.182395	17.087027
31.500502	1512.732075	17.092045
31.337526	1525.434836	17.097063
31.639106	1517.953062	17.102080
31.890604	1512.510268	17.107098
31.856279	1513.940775	17.112115
31.803264	1513.768921	17.117133
31.836404	1516.106299	17.122151
31.279309	1503.698893	17.127168
31.716370	1512.154784	17.132186
31.648421	1508.829597	17.137203
31.947398	1502.110052	17.142221
31.758827	1515.714672	17.147239
32.071405	1512.897478	17.152256
32.074180	1509.360147	17.157274
32.051601	1520.047105	17.162291
32.146251	1503.986980	17.167309
31.700594	1493.017711	17.172327
31.962033	1509.434844	17.177344
31.864620	1509.374305	17.182362
31.926884	1508.006946	17.187379
31.865513	1503.626759	17.192397
31.790918	1514.190472	17.197415
31.962633	1515.046984	17.202432
32.084502	1505.169170	17.207450
31.849412	1514.459203	17.212467
31.767412	1502.504312	17.217485
31.822925	1505.318271	17.222503
31.905597	1512.816167	17.227520
32.042046	1530.182811	17.232538
32.703817	1518.376717	17.237555
32.938633	1524.207249	17.242573
33.030010	1517.243866	17.247591
33.118596	1508.461315	17.252608
32.887170	1492.463274	17.257626
32.671900	1485.088682	17.262643
32.554048	1485.757502	17.267661
32.846844	1489.678835	17.272679
33.025866	1486.466534	17.277696
33.288649	1481.753349	17.282714
32.696429	1485.636748	17.287731
32.860111	1491.344844	17.292749
33.214506	1484.055089	17.297767
32.624575	1471.101609	17.302784
32.629644	1458.359075	17.307802
32.742271	1480.947177	17.312819
32.973991	1482.874783	17.317837
32.883384	1483.959928	17.322855
32.808045	1483.873673	17.327872
33.094998	1483.596889	17.332890
32.879409	1481.162756	17.337907
33.115470	1483.833713	17.342925
32.920630	1480.835125	17.347943
32.742928	1484.018148	17.352960
32.876708	1485.379374	17.357978
32.500772	1488.129613	17.362995
32.615028	1477.693650	17.368013
32.987947	1493.580836	17.373031
32.816107	1504.114644	17.378048
33.226946	1513.156768	17.383066
33.234419	1516.189338	17.388083
33.059745	1511.918529	17.393101
32.882540	1515.939248	17.398119
33.197054	1519.422345	17.403136
33.485078	1529.938396	17.408154
32.996976	1546.988800	17.413171
33.659058	1545.220567	17.418189
33.747091	1556.374192	17.423207
33.808264	1549.022123	17.428224
33.724546	1544.760202	17.433242
33.376457	1542.238244	17.438259
33.718535	1546.290766	17.443277
33.665176	1546.321720	17.448295
33.648747	1553.103056	17.453312
34.000435	1550.871859	17.458330
33.652441	1547.248337	17.463347
33.917490	1540.694648	17.468365
34.072927	1542.664468	17.473383
33.869701	1548.232787	17.478400
34.193312	1534.750648	17.483418
33.962922	1558.876941	17.488435
33.980464	1541.559940	17.493453
33.724338	1545.159937	17.498471
33.771813	1549.649213	17.503488
33.705497	1550.533086	17.508506
33.366613	1554.751550	17.513523
33.938382	1567.279467	17.518541
33.956405	1566.739908	17.523559
34.077637	1579.474606	17.528576
34.445455	1572.220767	17.533594
34.168627	1576.311209	17.538611
34.281687	1580.102995	17.543629
34.181596	1573.592660	17.548647
34.184582	1572.282391	17.553664
34.212785	1568.732946	17.558682
33.897853	1574.537159	17.563699
34.127143	1590.334147	17.568717
34.620465	1595.997333	17.573735
34.538796	1599.770703	17.578752
34.736767	1593.315934	17.583770
34.641513	1600.484399	17.588787
34.828577	1599.096683	17.593805
35.048664	1593.508691	17.598823
34.836322	1594.744389	17.603840
35.218185	1595.816364	17.608858
34.818676	1601.809051	17.613875
35.057227	1595.301081	17.618893
35.230819	1602.866977	17.623911
34.873351	1602.772891	17.628928
35.465019	1594.706656	17.633946
34.794565	1588.204111	17.638963
35.024390	1578.047289	17.643981
35.324064	1592.242854	17.648999
35.153916	1589.388563	17.654016
35.440798	1572.356279	17.659034
35.013397	1570.000251	17.664051
35.399664	1571.719901	17.669069
35.253201	1562.897650	17.674087
35.047082	1562.024096	17.679104
35.201763	1578.509834	17.684122
35.144081	1592.410475	17.689139
35.357753	1593.360408	17.694157
35.328590	1589.195311	17.699175
35.132314	1598.872635	17.704192
35.336388	1586.673678	17.709210
35.395725	1601.201711	17.714227
35.399205	1594.369041	17.719245
35.763970	1596.202109	17.724263
35.059771	1592.443692	17.729280
35.576236	1592.011438	17.734298
35.655823	1617.555164	17.739315
35.509177	1615.695365	17.744333
35.754043	1621.264821	17.749351
35.623949	1620.425870	17.754368
35.816352	1609.357551	17.759386
35.801746	1614.013066	17.764403
35.761829	1621.050298	17.769421
36.097383	1607.303519	17.774439
35.810384	1614.386540	17.779456
36.045054	1601.346677	17.784474
35.967116	1607.424496	17.789491
35.911488	1609.618772	17.794509
36.253030	1609.717157	17.799527
36.350476	1618.069322	17.804544
36.575229	1604.779141	17.809562
36.424567	1611.230459	17.814579
36.274684	1612.680969	17.819597
36.593631	1602.454596	17.824615
36.487722	1603.484813	17.829632
36.485125	1612.860669	17.834650
36.481485	1605.674854	17.839667
36.167734	1610.321036	17.844685
36.594210	1606.186892	17.849703
36.093085	1611.126810	17.854720
36.445886	1605.943911	17.859738
36.346967	1609.751646	17.864755
36.467500	1610.498957	17.869773
36.818475	1633.547654	17.874791
36.713100	1649.683787	17.879808
36.863426	1635.846512	17.884826
36.851859	1642.262125	17.889843
36.765687	1639.489534	17.894861
36.908019	1640.628490	17.899879
36.546540	1650.107719	17.904896
36.768267	1635.672761	17.909914
36.824424	1642.288136	17.914931
36.703637	1635.622163	17.919949
37.064650	1639.642430	17.924967
36.932365	1634.164566	17.929984
36.500867	1634.826077	17.935002
36.976466	1642.525256	17.940019
37.050123	1639.495789	17.945037
37.237074	1651.333814	17.950055
37.092709	1652.063346	17.955072
37.222515	1657.858234	17.960090
37.413300	1661.340670	17.965107
37.177233	1670.188840	17.970125
37.777770	1657.929048	17.975143
37.233631	1668.831929	17.980160
37.594012	1666.491007	17.985178
37.415717	1664.198281	17.990195
37.320471	1659.894151	17.995213
37.525011	1663.863268	18.000231
37.616646	1660.013501	18.005248
37.872398	1658.960813	18.010266
37.975657	1661.371596	18.015283
37.391870	1654.998315	18.020301
37.917698	1658.851825	18.025319
37.816570	1659.958022	18.030336
37.800892	1664.964905	18.035354
37.752513	1652.991317	18.040371
37.612516	1661.106599	18.045389
37.940314	1649.886222	18.050407
37.750928	1664.398176	18.055424
38.173950	1651.817113	18.060442
37.830854	1653.492258	18.065459
37.973442	1660.611376	18.070477
38.156494	1679.949934	18.075495
38.366971	1684.155467	18.080512
38.529169	1680.343178	18.085530
38.295552	1669.881443	18.090547
38.241875	1678.030023	18.095565
38.760196	1667.479135	18.100583
38.232617	1665.381864	18.105600
38.260976	1674.328997	18.110618
38.544543	1676.015337	18.115635
38.080548	1675.615733	18.120653
38.595356	1670.706274	18.125671
38.526242	1672.642963	18.130688
38.788532	1665.823936	18.135706
39.176863	1664.429532	18.140723
38.306263	1670.225747	18.145741
39.309752	1666.859839	18.150759
39.336215	1670.721551	18.155776
38.843126	1651.059816	18.160794
38.769286	1646.151750	18.165811
38.816986	1646.165119	18.170829
38.793421	1644.976972	18.175847
38.539345	1660.100844	18.180864
38.763915	1668.418521	18.185882
39.373928	1665.363679	18.190899
38.842024	1673.316945	18.195917
38.942226	1664.764261	18.200935
39.067190	1673.123694	18.205952
39.227044	1664.905971	18.210970
39.180930	1674.646571	18.215987
39.335159	1671.769450	18.221005
39.380329	1668.294326	18.226023
39.331756	1677.305428	18.231040
39.387597	1676.442656	18.236058
39.532107	1662.190584	18.241075
38.817172	1671.810856	18.246093
39.106228	1664.863761	18.251111
39.212892	1672.302630	18.256128
39.433495	1688.222813	18.261146
39.257221	1687.003352	18.266163
39.271198	1692.595463	18.271181
39.476489	1688.745301	18.276199
39.431213	1692.759885	18.281216
39.464572	1693.175631	18.286234
39.434740	1689.387777	18.291251
39.480590	1705.890953	18.296269
39.711221	1706.936499	18.301287
39.841058	1711.732599	18.306304
39.356758	1720.768119	18.311322
39.925197	1708.451418	18.316339
39.700299	1717.243036	18.321357
39.975055	1705.544828	18.326375
40.016139	1719.083895	18.331392
40.287482	1714.786534	18.336410
40.415955	1709.236562	18.341427
40.480647	1716.609595	18.346445
40.473407	1718.061209	18.351463
40.112210	1715.960291	18.356480
39.984574	1709.163930	18.361498
40.186281	1722.203476	18.366515
40.455945	1739.867107	18.371533
40.569116	1744.451030	18.376551
40.770561	1746.112052	18.381568
40.706901	1752.197397	18.386586
41.103637	1726.616481	18.391603
40.829008	1724.812192	18.396621
40.606467	1712.204130	18.401639
40.573052	1706.523983	18.406656
40.597977	1708.259615	18.411674
40.972832	1720.286930	18.416691
40.668198	1733.706310	18.421709
40.668781	1722.349326	18.426727
40.805906	1732.974847	18.431744
40.615016	1731.617656	18.436762
40.783031	1724.724117	18.441779
40.444293	1737.295637	18.446797
40.757120	1725.847382	18.451815
41.013200	1734.809849	18.456832
40.879918	1759.485659	18.461850
41.210527	1756.748102	18.466867
41.362796	1761.299154	18.471885
41.815130	1764.799558	18.476903
41.259150	1756.380297	18.481920
41.299468	1760.259020	18.486938
41.421696	1759.078521	18.491955
41.121272	1758.478501	18.496973
41.663562	1761.279708	18.501991
41.660699	1770.742710	18.507008
41.899311	1772.431809	18.512026
41.565733	1767.951517	18.517043
41.422128	1768.476993	18.522061
41.347005	1759.464034	18.527079
41.172242	1765.183209	18.532096
41.314011	1763.998280	18.537114
41.725485	1769.882614	18.542131
41.991761	1782.179202	18.547149
42.031906	1792.685452	18.552167
42.068387	1797.603788	18.557184
42.053143	1791.128471	18.562202
42.430597	1782.352083	18.567219
42.019676	1771.869356	18.572237
42.132161	1768.900731	18.577255
42.329872	1757.440878	18.582272
41.561877	1763.085428	18.587290
42.028625	1768.619239	18.592307
42.407938	1784.083620	18.597325
42.513441	1782.462596	18.602343
42.303619	1784.004186	18.607360
42.449368	1785.703210	18.612378
42.767222	1776.194613	18.617395
42.317876	1783.185405	18.622413
42.413367	1781.773129	18.627431
42.755413	1786.857207	18.632448
42.268848	1780.212992	18.637466
42.539033	1773.219380	18.642483
42.414100	1783.651487	18.647501
42.211760	1784.996954	18.652519
42.424616	1780.830948	18.657536
42.450652	1783.429387	18.662554
43.019246	1802.089063	18.667571
42.780262	1809.935051	18.672589
43.163832	1810.674479	18.677607
43.240307	1810.700388	18.682624
42.974949	1808.530772	18.687642
43.002761	1813.214335	18.692659
43.096304	1811.890176	18.697677
43.352298	1806.664641	18.702695
43.515412	1805.290729	18.707712
43.155042	1805.110510	18.712730
43.315195	1804.404014	18.717747
43.426290	1812.454806	18.722765
43.567109	1801.890589	18.727783
43.841201	1801.074999	18.732800
43.381835	1805.100565	18.737818
43.344715	1806.941402	18.742835
43.466777	1808.879796	18.747853
43.403695	1806.449002	18.752871
43.451550	1801.136805	18.757888
43.020487	1804.615939	18.762906
43.274310	1804.270249	18.767923
43.188391	1808.429412	18.772941
43.008463	1829.293042	18.777959
43.633997	1825.662759	18.782976
43.796087	1839.211740	18.787994
43.907752	1828.892507	18.793011
43.685800	1828.755028	18.798029
43.888046	1830.799781	18.803047
43.974735	1829.674002	18.808064
44.021416	1850.333068	18.813082
44.478331	1850.085903	18.818099
44.957222	1848.376434	18.823117
44.652819	1827.055564	18.828135
44.945587	1814.181456	18.833152
44.371545	1823.245335	18.838170
44.890126	1806.599085	18.843187
44.744852	1807.741370	18.848205
44.577203	1811.907425	18.853223
45.158241	1809.812875	18.858240
44.731463	1816.660168	18.863258
45.161237	1793.557882	18.868275
45.174823	1790.830098	18.873293
44.703654	1777.399930	18.878311
44.763299	1767.911815	18.883328
44.827174	1777.798369	18.888346
44.923866	1772.657984	18.893363
44.919452	1772.055219	18.898381
44.612868	1783.324990	18.903399
44.890428	1767.391669	18.908416
44.655715	1778.948307	18.913434
44.931012	1776.310097	18.918451
44.778749	1801.409990	18.923469
44.951438	1797.944744	18.928487
45.122495	1803.001736	18.933504
45.286613	1794.061983	18.938522
44.989922	1804.029744	18.943539
44.889641	1804.163378	18.948557
45.081178	1804.610711	18.953575
45.175488	1800.532907	18.958592
45.036263	1813.518173	18.963610
45.497990	1822.856351	18.968627
45.573299	1830.061138	18.973645
45.402290	1837.726159	18.978663
45.529306	1835.662581	18.983680
45.249597	1834.859115	18.988698
45.269972	1838.077791	18.993715
45.384819	1840.127624	18.998733
45.304564	1836.021739	19.003751
45.494381	1837.484312	19.008768
45.478721	1857.104543	19.013786
45.794029	1869.924546	19.018803
45.687154	1865.405757	19.023821
45.836535	1867.018754	19.028839
46.108710	1857.336205	19.033856
46.088981	1863.703660	19.038874
45.999938	1861.771265	19.043891
45.860958	1862.605028	19.048909
45.596669	1879.818989	19.053927
45.916632	1883.039060	19.058944
45.989223	1894.999823	19.063962
46.468101	1886.632502	19.068979
46.800806	1892.194543	19.073997
46.582845	1889.187907	19.079015
46.462988	1882.375610	19.084032
46.613834	1882.406088	19.089050
46.981882	1887.260681	19.094067
47.250411	1892.972365	19.099085
46.543841	1889.550091	19.104103
46.974436	1877.306563	19.109120
46.721289	1878.272689	19.114138
46.785129	1892.352611	19.119155
46.877050	1883.302367	19.124173
46.742634	1888.680237	19.129191
46.913479	1877.189722	19.134208
46.670650	1893.398954	19.139226
46.700038	1889.965380	19.144243
47.293330	1899.239217	19.149261
47.086588	1903.425180	19.154279
47.535485	1908.019099	19.159296
47.209574	1913.230381	19.164314
47.432893	1895.766971	19.169331
47.295793	1903.300404	19.174349
47.277230	1908.857450	19.179367
47.423506	1898.941865	19.184384
47.417975	1913.399871	19.189402
47.366019	1906.842812	19.194419
47.579627	1902.820350	19.199437
47.352246	1902.306214	19.204455
47.764407	1904.945614	19.209472
47.393786	1898.000581	19.214490
47.822298	1910.243929	19.219507
48.133928	1907.315801	19.224525
48.074892	1909.255568	19.229543
47.903651	1890.529007	19.234560
47.999203	1902.398952	19.239578
48.052069	1911.459471	19.244595
48.555060	1909.858195	19.249613
48.101618	1893.426954	19.254631
48.261359	1892.715012	19.259648
48.066152	1892.155371	19.264666
48.005948	1893.638245	19.269683
48.422471	1903.994612	19.274701
48.352651	1918.773150	19.279719
48.547386	1918.199878	19.284736
48.666276	1930.680137	19.289754
48.513147	1921.753671	19.294771
48.802602	1925.367798	19.299789
48.724046	1914.228944	19.304807
48.912889	1907.622807	19.309824
48.605491	1896.876725	19.314842
48.596754	1894.866411	19.319859
48.682318	1899.269536	19.324877
48.353903	1914.319397	19.329895
48.419985	1916.090338	19.334912
48.221439	1923.135962	19.339930
48.575587	1919.769663	19.344947
48.914758	1933.368822	19.349965
48.880296	1942.641512	19.354983
48.957163	1947.169325	19.360000
49.278772	1948.861184	19.365018
49.159478	1952.333413	19.370035
49.566661	1948.514986	19.375053
49.147029	1949.929653	19.380071
49.568124	1949.543560	19.385088
49.328075	1950.711843	19.390106
49.409918	1943.246704	19.395123
49.634134	1934.295307	19.400141
49.543752	1945.530835	19.405159
49.355725	1946.505038	19.410176
49.417767	1945.482953	19.415194
49.205261	1946.620674	19.420211
49.643150	1950.712499	19.425229
49.800310	1965.691939	19.430247
49.828933	1975.196289	19.435264
50.062709	1973.727154	19.440282
49.888861	1979.955312	19.445299
50.586771	1960.929874	19.450317
50.104456	1966.274256	19.455335
50.572233	1957.235120	19.460352
50.477552	1968.934372	19.465370
50.592969	1960.575847	19.470387
50.632125	1931.839064	19.475405
50.350613	1932.480773	19.480423
50.274183	1920.665971	19.485440
50.257605	1925.123482	19.490458
50.106467	1938.643904	19.495475
50.447842	1955.593108	19.500493
50.411898	1962.971961	19.505511
50.670684	1956.398273	19.510528
50.628968	1964.245803	19.515546
50.265010	1967.885866	19.520563
50.663091	1962.265403	19.525581
50.349938	1960.871032	19.530599
50.715181	1954.389887	19.535616
50.650005	1981.866149	19.540634
50.842571	1987.768055	19.545651
51.392313	1989.513734	19.550669
51.227965	1986.121394	19.555687
51.018938	1983.895539	19.560704
50.924121	1975.108956	19.565722
50.898740	1991.949079	19.570739
51.229252	1976.019343	19.575757
51.481958	1978.658093	19.580775
51.918070	1978.129346	19.585792
51.497236	1977.855235	19.590810
51.130275	1985.088329	19.595827
51.563332	1975.815976	19.600845
51.404009	1978.181082	19.605863
51.234592	1975.147462	19.610880
51.521522	1969.224997	19.615898
51.400381	1988.544423	19.620915
51.998301	1999.427005	19.625933
51.930598	2005.583987	19.630951
52.249731	2007.215241	19.635968
51.868269	1988.030981	19.640986
51.698635	1994.556870	19.646003
52.303935	1989.483060	19.651021
52.133173	2004.084362	19.656039
51.921582	2005.423116	19.661056
52.305203	2000.070005	19.666074
52.288809	2007.112951	19.671091
52.604372	2006.833768	19.676109
52.237149	2009.685010	19.681127
51.923864	2007.850103	19.686144
52.325218	1995.364492	19.691162
52.316849	1999.480895	19.696179
52.435318	1997.006117	19.701197
52.320059	2007.412751	19.706215
52.425759	2003.592451	19.711232
52.569966	1997.137396	19.716250
52.473919	2018.544427	19.721267
52.550656	2018.816358	19.726285
53.019889	2030.819569	19.731303
52.703074	2022.870255	19.736320
52.822805	2027.713803	19.741338
52.402461	2030.831754	19.746355
52.905063	2025.063580	19.751373
52.924013	2029.171514	19.756391
52.834642	2043.646726	19.761408
53.383248	2045.532759	19.766426
53.187769	2057.790567	19.771443
53.249498	2043.875528	19.776461
53.280355	2050.315361	19.781479
53.068278	2053.023501	19.786496
53.383618	2048.946691	19.791514
53.321003	2051.849281	19.796531
53.604802	2044.309975	19.801549
53.581747	2059.536389	19.806567
53.970493	2077.302663	19.811584
53.984765	2069.397903	19.816602
53.518419	2061.990355	19.821619
53.717645	2065.445889	19.826637
53.752736	2078.522484	19.831655
54.024976	2079.583582	19.836672
54.174580	2073.548469	19.841690
53.889670	2084.740444	19.846707
54.120646	2072.878370	19.851725
53.896226	2068.820401	19.856743
53.763920	2073.540892	19.861760
53.944248	2074.114507	19.866778
54.027325	2094.704069	19.871795
54.397401	2101.604477	19.876813
54.529932	2103.928967	19.881831
54.732482	2103.622503	19.886848
54.662962	2095.341889	19.891866
54.627382	2105.032976	19.896883
54.973871	2093.556415	19.901901
55.082709	2101.218753	19.906919
54.731834	2100.939311	19.911936
55.270127	2099.041989	19.916954
55.332390	2101.190362	19.921971
55.246757	2095.993952	19.926989
55.215700	2094.057401	19.932007
55.133498	2100.215256	19.937024
55.218452	2092.177869	19.942042
55.274231	2085.686687	19.947059
55.188357	2073.852472	19.952077
55.112881	2079.687938	19.957095
54.953933	2091.028275	19.962112
55.155763	2088.312066	19.967130
55.128398	2094.152140	19.972147
55.283036	2090.995738	19.977165
55.306748	2092.661930	19.982183
55.015983	2094.260704	19.987200
55.348528	2101.046876	19.992218
55.406033	2121.865923	19.997235
55.369297	2126.940629	20.002253
55.658722	2122.342905	20.007271
55.593829	2138.884239	20.012288
55.900818	2122.635818	20.017306
55.730575	2127.850038	20.022323
55.880971	2137.169679	20.027341
56.042193	2146.959580	20.032359
56.160946	2153.607684	20.037376
56.685166	2157.122610	20.042394
56.522882	2156.325988	20.047411
56.606263	2152.264476	20.052429
56.680707	2136.594462	20.057447
56.704520	2130.150308	20.062464
56.597618	2119.614056	20.067482
56.519667	2119.967212	20.072499
56.558748	2120.314302	20.077517
56.696205	2123.453340	20.082535
56.558573	2141.968995	20.087552
57.115113	2139.811546	20.092570
56.841288	2157.440395	20.097587
56.788101	2150.832650	20.102605
57.170692	2144.509569	20.107623
57.119867	2148.012194	20.112640
57.321525	2134.736424	20.117658
57.352201	2135.403025	20.122675
57.453661	2137.375988	20.127693
57.656276	2129.654463	20.132711
56.921024	2126.328633	20.137728
57.405801	2129.443411	20.142746
56.949913	2136.737418	20.147763
57.445509	2137.465725	20.152781
57.384999	2137.179360	20.157799
57.089970	2147.777779	20.162816
57.304323	2138.507429	20.167834
57.120575	2143.171529	20.172851
57.359299	2156.186785	20.177869
57.581843	2159.971541	20.182887
57.454981	2165.352187	20.187904
57.730684	2155.446030	20.192922
57.509916	2164.948246	20.197939
57.991147	2168.025826	20.202957
58.515140	2185.264226	20.207975
58.330313	2181.692173	20.212992
58.539147	2184.288644	20.218010
58.642084	2174.473789	20.223027
58.283906	2171.876234	20.228045
58.428481	2149.590125	20.233063
58.528095	2157.544579	20.238080
58.599369	2168.325835	20.243098
58.506410	2183.139179	20.248115
59.002422	2181.016983	20.253133
58.804613	2173.876563	20.258151
58.513495	2180.456186	20.263168
58.822303	2182.470678	20.268186
58.705126	2182.725235	20.273203
58.569111	2183.827030	20.278221
58.849350	2171.507080	20.283239
58.819151	2170.816458	20.288256
59.005546	2176.530876	20.293274
58.988571	2177.769581	20.298291
59.173850	2177.217557	20.303309
59.225595	2179.068865	20.308327
58.980705	2176.410353	20.313344
59.102825	2183.690204	20.318362
59.437501	2188.533905	20.323379
59.316383	2200.488516	20.328397
59.414341	2197.263560	20.333415
59.351485	2200.528822	20.338432
59.683689	2196.386179	20.343450
59.675848	2203.521101	20.348467
59.529776	2199.166605	20.353485
59.915792	2198.489484	20.358503
59.293286	2197.499268	20.363520
59.960999	2214.098055	20.368538
59.814750	2221.471742	20.373555
59.895632	2227.884043	20.378573
59.801926	2227.912254	20.383591
59.906605	2230.102021	20.388608
60.099450	2230.186151	20.393626
59.774816	2235.972928	20.398643
59.987977	2233.924508	20.403661
60.683305	2246.887966	20.408679
60.308575	2258.222556	20.413696
60.578030	2244.418878	20.418714
60.737056	2250.538667	20.423731
60.586109	2246.884589	20.428749
60.696202	2249.468348	20.433767
60.373711	2249.777897	20.438784
60.793170	2243.318331	20.443802
60.781361	2250.416926	20.448819
60.878693	2257.691876	20.453837
61.035275	2260.193500	20.458855
61.128757	2268.527384	20.463872
61.488206	2284.867634	20.468890
61.605102	2281.601717	20.473907
61.026256	2286.079160	20.478925
61.426533	2276.532151	20.483943
61.187172	2284.909947	20.488960
61.619222	2278.158505	20.493978
61.803002	2277.017738	20.498995
61.520096	2274.967508	20.504013
61.814515	2274.278835	20.509031
61.636090	2283.604397	20.514048
61.764049	2274.400688	20.519066
61.682995	2269.264484	20.524083
61.836129	2279.218808	20.529101
61.800704	2268.299701	20.534119
61.789077	2279.579468	20.539136
62.212934	2279.833476	20.544154
62.465579	2278.452124	20.549171
62.143257	2288.368546	20.554189
62.710243	2291.741748	20.559207
62.461719	2285.029401	20.564224
62.499431	2281.404589	20.569242
62.521394	2275.854008	20.574259
62.235374	2282.659603	20.579277
62.197735	2289.737705	20.584295
62.276325	2295.803950	20.589312
62.379266	2301.586617	20.594330
62.328557	2296.315043	20.599347
62.357175	2307.423177	20.604365
62.931935	2315.890093	20.609383
63.019168	2326.052649	20.614400
62.578062	2330.981632	20.619418
62.985597	2324.770479	20.624435
62.889829	2327.918794	20.629453
63.301074	2319.270746	20.634471
63.292372	2320.389186	20.639488
63.252069	2328.319344	20.644506
63.462187	2321.975645	20.649523
63.466236	2328.924392	20.654541
63.638849	2323.057016	20.659559
63.284890	2329.013666	20.664576
63.680319	2333.506756	20.669594
63.613930	2323.976649	20.674611
63.560278	2344.812108	20.679629
63.700743	2354.863077	20.684647
63.929796	2352.620264	20.689664
64.268329	2344.313430	20.694682
64.386239	2344.926958	20.699699
64.562033	2343.474120	20.704717
65.010644	2336.475012	20.709735
64.930962	2317.795710	20.714752
64.731462	2304.291581	20.719770
64.627848	2305.000982	20.724787
64.596956	2300.901336	20.729805
64.500271	2290.793988	20.734823
64.752396	2300.074772	20.739840
64.246478	2302.916440	20.744858
64.672858	2290.442970	20.749875
64.250653	2306.203300	20.754893
64.587283	2300.461431	20.759911
64.610789	2304.990738	20.764928
64.949352	2314.785917	20.769946
65.218056	2327.281361	20.774963
64.618770	2334.695358	20.779981
64.553590	2333.519192	20.784999
64.774065	2332.497129	20.790016
65.398633	2328.544841	20.795034
65.633749	2318.711470	20.800051
65.546025	2318.265841	20.805069
65.844557	2310.719234	20.810087
65.861024	2319.546272	20.815104
65.821824	2316.572439	20.820122
65.994893	2307.153334	20.825139
65.861869	2318.040305	20.830157
65.838293	2312.406333	20.835175
65.797625	2311.975325	20.840192
65.788189	2318.661736	20.845210
65.711009	2307.653475	20.850227
66.047825	2313.731929	20.855245
65.966164	2310.786021	20.860263
65.975773	2322.362297	20.865280
65.633234	2341.571711	20.870298
66.283850	2346.229090	20.875315
66.157776	2341.492087	20.880333
66.114137	2349.701164	20.885351
66.136700	2349.609654	20.890368
66.474118	2361.781493	20.895386
66.701900	2362.743700	20.900403
66.388083	2371.223290	20.905421
66.733491	2370.971426	20.910439
66.860114	2364.434888	20.915456
66.757941	2361.367180	20.920474
66.829651	2354.303144	20.925491
66.851949	2367.028556	20.930509
66.975138	2349.139930	20.935527
66.949887	2356.867989	20.940544
66.814562	2367.738054	20.945562
67.227294	2370.221138	20.950579
66.945669	2386.590878	20.955597
66.981150	2384.436534	20.960615
67.403616	2390.957095	20.965632
67.078137	2398.638614	20.970650
67.165669	2386.703290	20.975667
67.458043	2407.912438	20.980685
67.770696	2411.129507	20.985703
67.749093	2413.330052	20.990720
67.897652	2407.622159	20.995738
67.994103	2409.870801	21.000755
67.871030	2408.543616	21.005773
68.246901	2402.571560	21.010791
68.599967	2397.727345	21.015808
68.926023	2399.743330	21.020826
68.860092	2397.474733	21.025843
68.724815	2388.848581	21.030861
68.925445	2391.796855	21.035879
68.880018	2374.061425	21.040896
68.632645	2360.816391	21.045914
68.717223	2347.309892	21.050931
69.013764	2348.199644	21.055949
68.981223	2344.368772	21.060967
68.854713	2348.884047	21.065984
68.666981	2351.607089	21.071002
68.957075	2355.579884	21.076019
69.102355	2372.034566	21.081037
69.219441	2373.900629	21.086055
68.956245	2381.762739	21.091072
68.556792	2391.368808	21.096090
68.957032	2379.677587	21.101107
69.036468	2392.107688	21.106125
69.054844	2390.402655	21.111143
69.457983	2403.608910	21.116160
69.277965	2422.339036	21.121178
69.392580	2413.305972	21.126195
69.244677	2415.533021	21.131213
69.289928	2426.910531	21.136231
69.649110	2425.218539	21.141248
69.895591	2440.834007	21.146266
70.267469	2438.691069	21.151283
70.105453	2434.284037	21.156301
70.181645	2436.985671	21.161319
70.619601	2429.280003	21.166336
70.380451	2437.000345	21.171354
70.553271	2430.830522	21.176371
70.505369	2447.407551	21.181389
70.263330	2437.537264	21.186407
70.425685	2441.493910	21.191424
70.103081	2438.124623	21.196442
70.510172	2444.711150	21.201459
70.631018	2457.755701	21.206477
70.815350	2462.478410	21.211495
71.115079	2461.409701	21.216512
70.389887	2469.175012	21.221530
70.834182	2470.331563	21.226547
70.954041	2477.230025	21.231565
70.820673	2471.758342	21.236583
71.208965	2482.317437	21.241600
71.561926	2495.468328	21.246618
71.731309	2492.916109	21.251635
71.611827	2497.922403	21.256653
71.544241	2491.157451	21.261671
71.909318	2495.821782	21.266688
71.807667	2488.774687	21.271706
72.210306	2501.794882	21.276723
71.753614	2496.873008	21.281741
71.887810	2499.243741	21.286759
72.010550	2490.954584	21.291776
72.043623	2495.633148	21.296794
71.716896	2489.912484	21.301811
71.620711	2497.505940	21.306829
71.589662	2502.556594	21.311847
72.153345	2509.390755	21.316864
72.508768	2528.365887	21.321882
72.624553	2526.476927	21.326899
72.654951	2520.246485	21.331917
72.436968	2522.633233	21.336935
72.618451	2513.528759	21.341952
72.561690	2521.242057	21.346970
72.768980	2524.294372	21.351987
72.645126	2529.556530	21.357005
72.720236	2525.303769	21.362023
73.004955	2545.708836	21.367040
73.055973	2550.261989	21.372058
73.175105	2546.166478	21.377075
73.144442	2552.541939	21.382093
73.433303	2546.935091	21.387111
73.458625	2546.804144	21.392128
73.437735	2544.420554	21.397146
73.277940	2543.647908	21.402163
73.510590	2552.847432	21.407181
73.039208	2560.628873	21.412199
73.365253	2560.444402	21.417216
73.681996	2572.128879	21.422234
73.612768	2572.942818	21.427251
73.816704	2564.840922	21.432269
73.604430	2583.089968	21.437287
74.237424	2589.982333	21.442304
74.245482	2595.313931	21.447322
74.214412	2594.345864	21.452339
74.310255	2593.383871	21.457357
73.952586	2595.694630	21.462375
74.602599	2587.944979	21.467392
74.345216	2591.444237	21.472410
74.359359	2600.292688	21.477427
74.494036	2611.487748	21.482445
74.861177	2618.129810	21.487463
75.174101	2617.136855	21.492480
75.300304	2618.887254	21.497498
75.313146	2616.970115	21.502515
75.398419	2611.330148	21.507533
75.322008	2619.205429	21.512551
75.580584	2603.137397	21.517568
75.756004	2612.776015	21.522586
75.274462	2607.923198	21.527603
75.374347	2613.254502	21.532621
75.746617	2607.988902	21.537639
75.907711	2594.441125	21.542656
76.159044	2606.859758	21.547674
76.344522	2601.578747	21.552691
76.285768	2597.345853	21.557709
76.406202	2605.290384	21.562727
76.302365	2606.327408	21.567744
76.276357	2607.558199	21.572762
76.094198	2602.460736	21.577779
76.533468	2597.881672	21.582797
75.932127	2607.710018	21.587815
76.606845	2599.471983	21.592832
76.341152	2600.276448	21.597850
76.218064	2605.010922	21.602867
76.229858	2596.404701	21.607885
76.112114	2621.695858	21.612903
76.309893	2626.429769	21.617920
76.428876	2632.115794	21.622938
76.434284	2634.141401	21.627955
76.494608	2638.604053	21.632973
76.480479	2664.180040	21.637991
76.921410	2658.359680	21.643008
76.982810	2663.420613	21.648026
77.178847	2659.652859	21.653043
77.549958	2670.795279	21.658061
77.272823	2686.705117	21.663079
77.556293	2684.500459	21.668096
77.512384	2681.653329	21.673114
77.712390	2684.607670	21.678131
77.702064	2685.001569	21.683149
77.829242	2693.236376	21.688167
77.874238	2695.771972	21.693184
77.904990	2691.234398	21.698202
78.005634	2686.821830	21.703219
78.112926	2684.752364	21.708237
78.244343	2680.515794	21.713255
78.576844	2690.305526	21.718272
78.695417	2697.889373	21.723290
78.916959	2683.178660	21.728307
78.959336	2673.763338	21.733325
78.876816	2668.924896	21.738343
78.834542	2668.057904	21.743360
79.041965	2667.736054	21.748378
78.985898	2668.026920	21.753395
79.090489	2663.047141	21.758413
79.050661	2672.164064	21.763431
79.077990	2661.033848	21.768448
79.275104	2676.331759	21.773466
78.908292	2692.480533	21.778483
79.437557	2686.232864	21.783501
79.056437	2703.045870	21.788519
79.088479	2697.510000	21.793536
79.080367	2704.418414	21.798554
79.080590	2706.659470	21.803571
79.559388	2716.065438	21.808589
79.757692	2719.692936	21.813607
79.818883	2716.475165	21.818624
79.951257	2709.198514	21.823642
79.939913	2714.000674	21.828659
80.583745	2708.965512	21.833677
80.255148	2706.051120	21.838695
80.441259	2712.869382	21.843712
80.655852	2713.786951	21.848730
80.438232	2707.647264	21.853747
80.677834	2726.070600	21.858765
80.409000	2729.713137	21.863783
80.576721	2737.015199	21.868800
80.566285	2744.262224	21.873818
80.458584	2736.822301	21.878835
80.880596	2733.255960	21.883853
80.422275	2743.820895	21.888871
80.798900	2758.400434	21.893888
81.381230	2753.586121	21.898906
81.175713	2762.219584	21.903923
81.205485	2754.074485	21.908941
80.992094	2765.088122	21.913959
81.204932	2761.023048	21.918976
81.202682	2787.705589	21.923994
81.719724	2788.208310	21.929011
81.573456	2790.170558	21.934029
81.491408	2802.443564	21.939047
81.622529	2795.156845	21.944064
82.110828	2796.229728	21.949082
81.835161	2804.809122	21.954099
82.154252	2816.144555	21.959117
82.577571	2819.518919	21.964135
82.365501	2825.345474	21.969152
83.070531	2819.932369	21.974170
82.646900	2822.820690	21.979187
82.843101	2810.536253	21.984205
82.805501	2825.189818	21.989223
82.807194	2818.517152	21.994240
83.226730	2818.394311	21.999258
82.672887	2817.667454	22.004275
82.892114	2811.885461	22.009293
82.820894	2826.219793	22.014311
83.007253	2805.922371	22.019328
83.078375	2811.539641	22.024346
83.127666	2817.440085	22.029363
82.722298	2809.849588	22.034381
82.789932	2825.527453	22.039399
83.056697	2838.778007	22.044416
83.540155	2842.415231	22.049434
83.235933	2854.458259	22.054451
83.722715	2865.159130	22.059469
83.537899	2866.303336	22.064487
83.666841	2875.374217	22.069504
84.047226	2859.115982	22.074522
83.945776	2864.487527	22.079539
83.979143	2860.447136	22.084557
83.899922	2875.440363	22.089575
84.176088	2884.957281	22.094592
84.407768	2884.826289	22.099610
84.372733	2893.684655	22.104627
84.587903	2885.456310	22.109645
84.778360	2879.330233	22.114663
84.849218	2887.895783	22.119680
84.971570	2883.710668	22.124698
84.907115	2899.255434	22.129715
85.003802	2910.076291	22.134733
85.350508	2913.329936	22.139751
85.338229	2907.448186	22.144768
85.882983	2915.334166	22.149786
85.378997	2918.016947	22.154803
85.821739	2908.850711	22.159821
85.777318	2918.875684	22.164839
85.626322	2911.438148	22.169856
85.665055	2916.780901	22.174874
85.688853	2914.821350	22.179891
85.788289	2907.150844	22.184909
85.853968	2913.375786	22.189927
85.925939	2919.301241	22.194944
86.101618	2928.245480	22.199962
85.833739	2946.984538	22.204979
86.096024	2949.199398	22.209997
85.695207	2958.264666	22.215015
86.170873	2960.347207	22.220032
86.407551	2966.975668	22.225050
86.089307	2981.470497	22.230067
86.214772	2978.619574	22.235085
86.494325	2994.153720	22.240103
86.627317	3002.823975	22.245120
87.001073	3000.439691	22.250138
87.160821	3001.047474	22.255155
87.313639	2994.642943	22.260173
87.549336	2995.436148	22.265191
87.439400	2989.465079	22.270208
87.984613	2990.934845	22.275226
87.649054	2993.769973	22.280243
87.761135	2980.952496	22.285261
87.788376	2990.970724	22.290279
87.817208	2994.122088	22.295296
88.064118	3004.355014	22.300314
88.338728	3015.921230	22.305331
88.093300	3024.518160	22.310349
88.038452	3021.364890	22.315367
88.205736	3016.923830	22.320384
88.625260	3014.929209	22.325402
88.395399	3025.730791	22.330419
88.853073	3025.155911	22.335437
88.775291	3026.504009	22.340455
88.365011	3027.607346	22.345472
88.691938	3003.845909	22.350490
88.356826	3014.916961	22.355507
88.493713	3011.001069	22.360525
88.762386	3037.295680	22.365543
88.826441	3043.752850	22.370560
89.240419	3044.751484	22.375578
88.710878	3050.157230	22.380595
88.976909	3053.392028	22.385613
89.143222	3068.571420	22.390631
88.998689	3077.765828	22.395648
89.187952	3067.725419	22.400666
89.454428	3088.434647	22.405683
89.660822	3103.701907	22.410701
89.771454	3112.186162	22.415719
90.139067	3104.155217	22.420736
90.159494	3106.668584	22.425754
90.063121	3112.301988	22.430771
90.165024	3107.265423	22.435789
90.262727	3108.593812	22.440807
90.295063	3124.266426	22.445824
90.501768	3125.691276	22.450842
90.771498	3130.966969	22.455859
90.880050	3122.861345	22.460877
91.072828	3118.960942	22.465895
90.839689	3123.579994	22.470912
91.046243	3116.001041	22.475930
90.966058	3124.489848	22.480947
91.267012	3116.526673	22.485965
90.990769	3119.269282	22.490983
91.030233	3146.430186	22.496000
91.223019	3148.568430	22.501018
91.353700	3152.149391	22.506035
91.713165	3154.558382	22.511053
91.398397	3145.939985	22.516071
91.468189	3167.269453	22.521088
91.639456	3162.529635	22.526106
91.635882	3174.981638	22.531123
91.955442	3176.718865	22.536141
92.195146	3177.821282	22.541159
92.276850	3194.156287	22.546176
92.653076	3195.690776	22.551194
92.565632	3208.809554	22.556211
92.468288	3201.902770	22.561229
93.213423	3203.612188	22.566247
92.709449	3201.465884	22.571264
93.126795	3200.559879	22.576282
92.814445	3191.457551	22.581299
93.355562	3193.748163	22.586317
93.565526	3186.100886	22.591335
93.177187	3194.700006	22.596352
93.447056	3180.985205	22.601370
93.265910	3191.836290	22.606387
93.518906	3182.989642	22.611405
93.649985	3188.835685	22.616423
93.681525	3207.945011	22.621440
93.870569	3206.204044	22.626458
93.856299	3212.891248	22.631475
93.911736	3218.080922	22.636493
94.116345	3210.589261	22.641511
94.109017	3210.579099	22.646528
94.551134	3199.848892	22.651546
94.486314	3209.254557	22.656563
94.461762	3202.862882	22.661581
94.523507	3204.546103	22.666599
94.347789	3207.170043	22.671616
94.489169	3215.559473	22.676634
94.723685	3235.671010	22.681651
94.651176	3232.208402	22.686669
94.823580	3226.706895	22.691687
94.694699	3240.197577	22.696704
94.795915	3237.798706	22.701722
94.811330	3253.002175	22.706739
95.159202	3255.156395	22.711757
95.648014	3261.562750	22.716775
95.265592	3260.233314	22.721792
95.357867	3259.917991	22.726810
95.644249	3272.134859	22.731827
95.610713	3286.679905	22.736845
96.106230	3280.062383	22.741863
96.063236	3291.422512	22.746880
96.110225	3289.991783	22.751898
96.146428	3288.980994	22.756915
96.371598	3289.824000	22.761933
96.216215	3282.968956	22.766951
96.206471	3301.265895	22.771968
96.408439	3314.656376	22.776986
96.539437	3317.762083	22.782003
96.392958	3321.297405	22.787021
96.437679	3322.666117	22.792039
96.202599	3347.088894	22.797056
96.761788	3350.989664	22.802074
96.701096	3363.374532	22.807091
96.580502	3370.994518	22.812109
97.797711	3370.725327	22.817127
97.854051	3375.185308	22.822144
97.935873	3366.829647	22.827162
98.087622	3375.433994	22.832179
98.016918	3367.960453	22.837197
98.116625	3369.761409	22.842215
98.119318	3372.080109	22.847232
98.230225	3365.191009	22.852250
98.327279	3373.877288	22.857267
98.304309	3363.495156	22.862285
98.452067	3368.276587	22.867303
98.561526	3365.490465	22.872320
98.812525	3363.503336	22.877338
98.840706	3363.184882	22.882355
98.600649	3367.442524	22.887373
99.045007	3365.434284	22.892391
98.938297	3403.280352	22.897408
99.155775	3393.813053	22.902426
99.001945	3399.249003	22.907443
98.805562	3398.468218	22.912461
99.445255	3396.312932	22.917479
98.905976	3394.771736	22.922496
99.148314	3409.728963	22.927514
99.630451	3414.802901	22.932531
99.240929	3423.581098	22.937549
99.466569	3416.076001	22.942567
99.771781	3443.398000	22.947584
99.446203	3444.765659	22.952602
99.689529	3455.998000	22.957619
99.668444	3467.279411	22.962637
100.215372	3470.670389	22.967655
99.998568	3486.499350	22.972672
99.868865	3491.997078	22.977690
100.560949	3501.218457	22.982707
100.348438	3509.268788	22.987725
101.094925	3516.944368	22.992743
100.967115	3519.890746	22.997760
101.140064	3512.297893	23.002778
101.103302	3514.852329	23.007795
101.264798	3509.648235	23.012813
101.575896	3499.716449	23.017831
101.500312	3502.820302	23.022848
101.684933	3504.610312	23.027866
102.345619	3494.864154	23.032883
101.928966	3496.976161	23.037901
102.036666	3486.988413	23.042919
102.029860	3496.057017	23.047936
102.113456	3484.061660	23.052954
102.433636	3487.120211	23.057971
102.581350	3491.016955	23.062989
102.701287	3485.098051	23.068007
103.041355	3490.504317	23.073024
103.104049	3487.570418	23.078042
103.308448	3475.954243	23.083059
103.039008	3479.504917	23.088077
102.975180	3477.212974	23.093095
102.824346	3471.735178	23.098112
103.003459	3472.003116	23.103130
103.494495	3484.945269	23.108147
103.006892	3500.297545	23.113165
103.342100	3499.376039	23.118183
103.233291	3503.780819	23.123200
103.348380	3512.531508	23.128218
103.634112	3499.962333	23.133235
103.379213	3510.456961	23.138253
103.970760	3521.092052	23.143271
104.127595	3530.596913	23.148288
103.942101	3536.237012	23.153306
103.815769	3540.442332	23.158323
103.728485	3540.890779	23.163341
104.016335	3553.135580	23.168359
104.011926	3566.533801	23.173376
103.794642	3574.805061	23.178394
104.214244	3588.991584	23.183411
104.336427	3603.235031	23.188429
104.555052	3600.318508	23.193447
104.566786	3611.229176	23.198464
104.789702	3624.739683	23.203482
105.239483	3625.684372	23.208499
104.913145	3632.327545	23.213517
105.604427	3641.203830	23.218535
105.476110	3660.517067	23.223552
105.515571	3658.712318	23.228570
105.504706	3661.513289	23.233587
105.702831	3661.637110	23.238605
105.927680	3673.176649	23.243623
106.404100	3677.390111	23.248640
106.103885	3684.890873	23.253658
106.341538	3688.175014	23.258675
106.112446	3685.674260	23.263693
106.419802	3684.610506	23.268711
106.584060	3694.016584	23.273728
106.894877	3702.994722	23.278746
107.252802	3709.381279	23.283763
107.614164	3702.919751	23.288781
107.411966	3711.252756	23.293799
107.318621	3705.597982	23.298816
107.325146	3700.836950	23.303834
107.370560	3706.255250	23.308851
107.300975	3710.455121	23.313869
107.319702	3711.088733	23.318887
107.693379	3718.767311	23.323904
107.625765	3718.068663	23.328922
107.923907	3722.373191	23.333939
107.478593	3738.592392	23.338957
107.887990	3745.328325	23.343975
108.097545	3740.877280	23.348992
108.068166	3736.062749	23.354010
108.288180	3755.250488	23.359027
108.321297	3769.428565	23.364045
108.504009	3768.710756	23.369063
108.706677	3768.007743	23.374080
108.963839	3766.577479	23.379098
109.219388	3752.306620	23.384115
108.858416	3764.603111	23.389133
108.984159	3765.495744	23.394151
109.220234	3786.463345	23.399168
109.768170	3782.962076	23.404186
109.805219	3777.171812	23.409203
109.691675	3779.508709	23.414221
109.983020	3784.245537	23.419239
109.901389	3778.672264	23.424256
109.939791	3775.289933	23.429274
110.409082	3763.892545	23.434291
110.438087	3770.925986	23.439309
110.542957	3760.776311	23.444327
110.730695	3763.910478	23.449344
110.327053	3752.963720	23.454362
111.206789	3755.930906	23.459379
111.197879	3767.870824	23.464397
110.922293	3759.377084	23.469415
111.032323	3763.382140	23.474432
111.235549	3780.307870	23.479450
111.609340	3780.183575	23.484467
111.101936	3788.243289	23.489485
111.389946	3780.203576	23.494503
111.346727	3786.168585	23.499520
111.271120	3785.477956	23.504538
111.510925	3789.972141	23.509555
111.772335	3805.677062	23.514573
111.864407	3811.415636	23.519591
111.877759	3815.099329	23.524608
112.053634	3816.148221	23.529626
111.984956	3810.690514	23.534643
112.136286	3849.884315	23.539661
112.221778	3854.447476	23.544679
112.277503	3848.383183	23.549696
112.105479	3859.394650	23.554714
112.565774	3872.782841	23.559731
112.731495	3884.439462	23.564749
112.975647	3884.898199	23.569767
112.942826	3896.761864	23.574784
113.215115	3909.044181	23.579802
113.354896	3901.729522	23.584819
113.496693	3917.154790	23.589837
113.476765	3907.892011	23.594855
113.974937	3920.898311	23.599872
113.742427	3924.832760	23.604890
114.080727	3920.851668	23.609907
114.055164	3929.043608	23.614925
114.061946	3921.983356	23.619943
114.403542	3922.243593	23.624960
115.024157	3923.290637	23.629978
115.015512	3916.994464	23.634995
115.113101	3918.835606	23.640013
114.863605	3921.436487	23.645031
115.211358	3908.231403	23.650048
114.926527	3921.696219	23.655066
115.110923	3939.456065	23.660083
114.866513	3950.589876	23.665101
114.745968	3947.926926	23.670119
115.434352	3949.156041	23.675136
115.533185	3967.900342	23.680154
116.131059	3965.195170	23.685171
115.933917	3970.312095	23.690189
115.978105	3958.484363	23.695207
116.422826	3956.314159	23.700224
116.383526	3956.658568	23.705242
116.162830	3960.521762	23.710259
116.479202	3961.748915	23.715277
116.370506	3964.058652	23.720295
116.801484	3966.472821	23.725312
116.627833	3964.655810	23.730330
116.693434	3976.751242	23.735347
116.679098	3995.954600	23.740365
116.476404	4002.794731	23.745383
116.977256	3992.327884	23.750400
116.935869	4011.120741	23.755418
117.204403	4011.586849	23.760435
117.463645	4018.807365	23.765453
117.537392	4018.559683	23.770471
117.629164	4017.751845	23.775488
117.707099	4039.183920	23.780506
118.005523	4044.362624	23.785523
118.299622	4038.577976	23.790541
117.907226	4037.950615	23.795559
118.034080	4041.949008	23.800576
118.096101	4056.601739	23.805594
118.817938	4059.393627	23.810611
118.735123	4068.346044	23.815629
118.714215	4066.298490	23.820647
118.907981	4068.911174	23.825664
118.716649	4077.958019	23.830682
119.272148	4097.119169	23.835699
119.539790	4098.624548	23.840717
119.706580	4102.941168	23.845735
119.998923	4087.402693	23.850752
119.649517	4089.784347	23.855770
119.586985	4091.569037	23.860787
119.653874	4095.663642	23.865805
119.629761	4119.808827	23.870823
120.108749	4115.416064	23.875840
120.098775	4116.545476	23.880858
120.156544	4127.452790	23.885875
120.613068	4143.722166	23.890893
120.460883	4150.775653	23.895911
120.567153	4145.519889	23.900928
120.638410	4144.906426	23.905946
121.127044	4156.474542	23.910963
121.033060	4170.883583	23.915981
121.274582	4183.305895	23.920999
121.258259	4174.948788	23.926016
121.347462	4179.310612	23.931034
121.537515	4188.190973	23.936051
121.564378	4202.296455	23.941069
121.928951	4205.664354	23.946087
122.043290	4205.380785	23.951104
121.831350	4216.347946	23.956122
121.890791	4207.206466	23.961139
122.290251	4218.862687	23.966157
122.208474	4232.927187	23.971175
122.548092	4233.663814	23.976192
122.250037	4236.893380	23.981210
122.514103	4253.377952	23.986227
122.545363	4261.457457	23.991245
122.569349	4265.909289	23.996263
123.232229	4284.175134	24.001280
123.286374	4282.102873	24.006298
123.992382	4290.760125	24.011315
123.948527	4279.530334	24.016333
123.723598	4288.517912	24.021351
123.955659	4275.793235	24.026368
124.128725	4269.014686	24.031386
124.431726	4278.421685	24.036403
124.294681	4276.862373	24.041421
124.034567	4280.879461	24.046439
124.400225	4294.078201	24.051456
124.186152	4305.405281	24.056474
124.555624	4306.137739	24.061491
124.992789	4306.215542	24.066509
124.775162	4309.234088	24.071527
124.975938	4302.828143	24.076544
124.891159	4314.751947	24.081562
125.139107	4325.410044	24.086579
125.100924	4334.249273	24.091597
124.859055	4336.416604	24.096615
125.665284	4352.150448	24.101632
125.810097	4368.120232	24.106650
125.634479	4368.632208	24.111667
125.899203	4365.019983	24.116685
125.470513	4370.629918	24.121703
125.967598	4384.065200	24.126720
126.436134	4393.306154	24.131738
126.280389	4389.821289	24.136755
126.527557	4403.575330	24.141773
126.928361	4422.129024	24.146791
127.103381	4418.446641	24.151808
127.208729	4420.326323	24.156826
127.122386	4416.463718	24.161843
127.470024	4423.217299	24.166861
127.276670	4429.580397	24.171879
127.807954	4431.972065	24.176896
127.507502	4441.047883	24.181914
127.721921	4449.328579	24.186931
128.084008	4442.153131	24.191949
127.943108	4444.199743	24.196967
128.275052	4465.499229	24.201984
128.387107	4473.459887	24.207002
128.251469	4480.271756	24.212019
128.427054	4477.646917	24.217037
128.455569	4473.645507	24.222055
128.590699	4489.320912	24.227072
128.897707	4506.364061	24.232090
128.753697	4505.797384	24.237107
129.001761	4503.230587	24.242125
128.908920	4535.964830	24.247143
129.435033	4535.371052	24.252160
129.538082	4542.965465	24.257178
129.805767	4554.304804	24.262195
130.142145	4550.737331	24.267213
130.180451	4551.011366	24.272231
130.609655	4557.123786	24.277248
130.540760	4545.612879	24.282266
130.278606	4552.069363	24.287283
130.586979	4547.303983	24.292301
130.527793	4551.657888	24.297319
130.538735	4573.646406	24.302336
131.004497	4577.236587	24.307354
130.910625	4587.327154	24.312371
131.549836	4586.090064	24.317389
130.996078	4600.594808	24.322407
131.298710	4590.835032	24.327424
131.338640	4608.395198	24.332442
131.435879	4608.232595	24.337459
131.742239	4613.845679	24.342477
131.657764	4634.220726	24.347495
132.095562	4634.325204	24.352512
132.047418	4645.197321	24.357530
131.507594	4654.192549	24.362547
132.110320	4664.288681	24.367565
132.130582	4671.837061	24.372583
132.386451	4679.110029	24.377600
132.765452	4696.962037	24.382618
133.270375	4697.282172	24.387635
133.451238	4698.768956	24.392653
133.466107	4703.342134	24.397671
133.570928	4693.286764	24.402688
133.536448	4693.328759	24.407706
133.621013	4695.491504	24.412723
134.137968	4701.153889	24.417741
134.269836	4717.957035	24.422759
134.276379	4729.094974	24.427776
134.334232	4720.772109	24.432794
134.368608	4725.409779	24.437811
134.631004	4713.242800	24.442829
134.990905	4724.371627	24.447847
135.328345	4719.848653	24.452864
135.150958	4714.107855	24.457882
134.739676	4709.548652	24.462899
135.174100	4710.637331	24.467917
135.150178	4729.077688	24.472935
135.404096	4731.351690	24.477952
135.397499	4738.191840	24.482970
135.387771	4750.096414	24.487987
135.947345	4751.705339	24.493005
135.828113	4767.411481	24.498023
135.672561	4766.805760	24.503040
135.966924	4761.625245	24.508058
135.998291	4782.605755	24.513075
136.530678	4779.866444	24.518093
136.902508	4791.718666	24.523111
136.673006	4789.135895	24.528128
136.574976	4795.012346	24.533146
136.852598	4803.414247	24.538163
137.593399	4797.343632	24.543181
137.393659	4804.447447	24.548199
137.519229	4812.961252	24.553216
138.141088	4800.472215	24.558234
137.740061	4809.664977	24.563251
138.304660	4822.463319	24.568269
138.439257	4833.544612	24.573287
138.059336	4835.600281	24.578304
138.425527	4820.330361	24.583322
138.295873	4827.618638	24.588339
138.572568	4835.520618	24.593357
138.730846	4849.896234	24.598375
138.696963	4853.172590	24.603392
139.067152	4860.829869	24.608410
138.887391	4862.182862	24.613427
139.145179	4861.150112	24.618445
139.088874	4890.116115	24.623463
139.311230	4884.482873	24.628480
139.457568	4895.931619	24.633498
139.600905	4919.570588	24.638515
139.986509	4926.806360	24.643533
139.929374	4922.315036	24.648551
140.194839	4921.117983	24.653568
140.627487	4934.791264	24.658586
140.414679	4948.949846	24.663603
140.530984	4954.305605	24.668621
140.721479	4950.448054	24.673639
140.771203	4954.765858	24.678656
141.220580	4973.352299	24.683674
141.251606	4981.794489	24.688691
141.266190	4969.600765	24.693709
141.579691	4980.983991	24.698727
141.350864	4993.931654	24.703744
141.913315	4998.857312	24.708762
141.951345	5012.293031	24.713779
142.327052	5003.000479	24.718797
142.310336	5007.019041	24.723815
142.095584	5010.423144	24.728832
142.382231	5004.847692	24.733850
142.724251	5017.296494	24.738867
142.694326	5024.447792	24.743885
143.196091	5022.909829	24.748903
143.263378	5020.363541	24.753920
143.409959	5016.479406	24.758938
143.379576	5026.234443	24.763955
143.262629	5028.279512	24.768973
143.261709	5045.311416	24.773991
143.257827	5054.727354	24.779008
143.958465	5051.903334	24.784026
144.041267	5079.360446	24.789043
143.948618	5072.936797	24.794061
143.981912	5081.445605	24.799079
144.572664	5085.865700	24.804096
144.536626	5095.270468	24.809114
144.699812	5108.909925	24.814131
145.025653	5109.886731	24.819149
145.101456	5106.862540	24.824167
144.831199	5120.465354	24.829184
145.026488	5124.957480	24.834202
144.856879	5151.371404	24.839219
145.118153	5154.942937	24.844237
145.381147	5173.429067	24.849255
145.449192	5177.061857	24.854272
145.549376	5188.058549	24.859290
145.753068	5200.843147	24.864307
146.090575	5215.043613	24.869325
146.009489	5224.859965	24.874343
146.264306	5235.988506	24.879360
146.415721	5254.405854	24.884378
146.825361	5267.611496	24.889395
146.834259	5268.811885	24.894413
147.320721	5279.968906	24.899431
147.091660	5299.309560	24.904448
147.641286	5303.630230	24.909466
147.551369	5298.160570	24.914483
147.982181	5303.817015	24.919501
148.514227	5313.756777	24.924519
148.799965	5310.848873	24.929536
148.890602	5309.876163	24.934554
148.912936	5314.926333	24.939571
149.245960	5304.396336	24.944589
148.918691	5301.490283	24.949607
149.066297	5306.890578	24.954624
149.142885	5307.455178	24.959642
149.164347	5304.272227	24.964659
150.028502	5301.541490	24.969677
150.402512	5299.626221	24.974695
150.649215	5295.348134	24.979712
150.623001	5274.578804	24.984730
150.337127	5278.385417	24.989747
150.596757	5269.811361	24.994765
150.707165	5266.913700	24.999783
150.618899	5283.146818	25.004800
151.098706	5289.114082	25.009818
150.625754	5310.724891	25.014835
151.004609	5307.842467	25.019853
151.116716	5310.652042	25.024871
150.900190	5313.541433	25.029888
151.164655	5310.701645	25.034906
151.080827	5330.721504	25.039923
151.040782	5343.328565	25.044941
151.619537	5349.083303	25.049959
151.396469	5368.254505	25.054976
151.823095	5368.802680	25.059994
151.725498	5374.009049	25.065011
151.749460	5398.571923	25.070029
151.755643	5403.568100	25.075047
151.665773	5424.777533	25.080064
152.131593	5434.106192	25.085082
152.106145	5453.900709	25.090099
152.270296	5468.956383	25.095117
152.597142	5472.893556	25.100135
152.787800	5499.706564	25.105152
153.149350	5504.257804	25.110170
153.661303	5524.598681	25.115187
153.400260	5531.866588	25.120205
153.804682	5536.122457	25.125223
153.830902	5562.042214	25.130240
154.118448	5562.780477	25.135258
154.163905	5568.790887	25.140275
154.081717	5575.173775	25.145293
154.967821	5582.547203	25.150311
154.597690	5593.283674	25.155328
155.081536	5601.113025	25.160346
155.087415	5621.858675	25.165363
155.233466	5624.844598	25.170381
155.382123	5624.519862	25.175399
155.743949	5637.580183	25.180416
155.798317	5638.053978	25.185434
156.088278	5646.285737	25.190451
156.109525	5648.525295	25.195469
156.359430	5655.017633	25.200487
156.155131	5674.408974	25.205504
156.515407	5672.938570	25.210522
156.684329	5681.726811	25.215539
157.053437	5697.137713	25.220557
157.147978	5711.597955	25.225575
157.027937	5703.026903	25.230592
157.355439	5715.221129	25.235610
157.491290	5726.020097	25.240627
157.705101	5739.741474	25.245645
157.773379	5732.518972	25.250663
157.720866	5771.023704	25.255680
158.209482	5768.772724	25.260698
158.049618	5774.986666	25.265715
158.028273	5793.343567	25.270733
158.428323	5786.084809	25.275751
158.731399	5798.343804	25.280768
158.944638	5817.075237	25.285786
159.113977	5824.280420	25.290803
159.176046	5830.925336	25.295821
159.463694	5852.864143	25.300839
159.583976	5846.801743	25.305856
159.876734	5854.629109	25.310874
160.242836	5850.075851	25.315891
160.136525	5859.877886	25.320909
160.529366	5868.965326	25.325927
160.725689	5879.565326	25.330944
161.035546	5864.355745	25.335962
160.896276	5871.853238	25.340979
160.778816	5875.929718	25.345997
161.182458	5897.960364	25.351015
161.042710	5903.633870	25.356032
161.442694	5905.087509	25.361050
161.503524	5915.522601	25.366067
161.525408	5927.947353	25.371085
161.790628	5931.951591	25.376103
161.989101	5933.563160	25.381120
162.334712	5951.465464	25.386138
162.464938	5956.458530	25.391155
162.580378	5960.602655	25.396173
163.077790	5954.602772	25.401191
162.902940	5960.262442	25.406208
162.966138	5969.976519	25.411226
163.031127	5987.170972	25.416243
162.972804	5986.694750	25.421261
163.214147	5988.974179	25.426279
163.170013	6015.101696	25.431296
163.752275	6016.881054	25.436314
163.826645	6009.032842	25.441331
163.798059	6035.491754	25.446349
164.482756	6028.603017	25.451367
164.112671	6046.246310	25.456384
164.507324	6048.779084	25.461402
164.988170	6071.393362	25.466419
164.977681	6066.292226	25.471437
165.018923	6069.137342	25.476455
165.357467	6078.961677	25.481472
165.508302	6094.781780	25.486490
165.826312	6091.123294	25.491507
165.693239	6098.782901	25.496525
165.852888	6090.099000	25.501543
166.030807	6120.630337	25.506560
166.096860	6121.243187	25.511578
166.584123	6129.681060	25.516595
166.655450	6149.380029	25.521613
166.895236	6148.930662	25.526631
166.876231	6155.775852	25.531648
167.273666	6151.238567	25.536666
167.675293	6162.329979	25.541683
167.581616	6174.006205	25.546701
168.142106	6165.793593	25.551719
168.686331	6159.610217	25.556736
168.645995	6163.096634	25.561754
168.922804	6161.028870	25.566771
168.865070	6166.029608	25.571789
169.105428	6157.389755	25.576807
168.896297	6165.923681	25.581824
168.838455	6159.619822	25.586842
169.224669	6171.133600	25.591859
169.070338	6175.320249	25.596877
169.737517	6180.033555	25.601895
169.696748	6185.769476	25.606912
170.094374	6185.412021	25.611930
170.228026	6179.490618	25.616947
170.202736	6203.503722	25.621965
170.465035	6197.621580	25.626983
170.479032	6200.017581	25.632000
170.556830	6200.358331	25.637018
170.684041	6208.337040	25.642035
170.805191	6229.323458	25.647053
171.289332	6239.007919	25.652071
171.379478	6237.843057	25.657088
170.989723	6246.081756	25.662106
171.171296	6270.130683	25.667123
171.169612	6283.862353	25.672141
171.638916	6292.456097	25.677159
171.355337	6309.934084	25.682176
171.607807	6330.733414	25.687194
171.811844	6336.037260	25.692212
172.212694	6361.066708	25.697229
172.203210	6368.776793	25.702247
172.606862	6382.234046	25.707264
172.885681	6396.562689	25.712282
173.774300	6389.131107	25.717300
173.343743	6391.645905	25.722317
173.895889	6406.936510	25.727335
173.980854	6411.392993	25.732352
174.289724	6410.776190	25.737370
174.708955	6403.504514	25.742388
174.780627	6406.120949	25.747405
174.926468	6410.726416	25.752423
174.849053	6408.590675	25.757440
174.703181	6404.412184	25.762458
175.367306	6411.558257	25.767476
175.154236	6425.728441	25.772493
175.464524	6427.108035	25.777511
175.524714	6435.973050	25.782528
175.680473	6438.295121	25.787546
175.797760	6445.706145	25.792564
175.900990	6461.992139	25.797581
176.090541	6463.768286	25.802599
176.297647	6472.076471	25.807616
176.363869	6487.093470	25.812634
176.732135	6488.557163	25.817652
176.663495	6500.201114	25.822669
177.349332	6516.514008	25.827687
177.379236	6517.429030	25.832704
177.373096	6518.798991	25.837722
177.797068	6525.061920	25.842740
177.731275	6542.905665	25.847757
178.123025	6545.427977	25.852775
178.480790	6546.241261	25.857792
178.402385	6536.682234	25.862810
179.075236	6551.655198	25.867828
179.135308	6558.789084	25.872845
178.947243	6558.323378	25.877863
179.337082	6558.966718	25.882880
179.443086	6567.868301	25.887898
179.525076	6576.198907	25.892916
179.311621	6598.909627	25.897933
179.362884	6605.054941	25.902951
179.565758	6627.427935	25.907968
179.572021	6631.030370	25.912986
179.692492	6648.595964	25.918004
179.725427	6672.634760	25.923021
180.370757	6692.679312	25.928039
180.258515	6706.032749	25.933056
180.376734	6722.552025	25.938074
181.195237	6730.939118	25.943092
181.623536	6740.856072	25.948109
181.724424	6753.369950	25.953127
182.089900	6760.991138	25.958144
181.947577	6765.760377	25.963162
182.091010	6771.795135	25.968180
182.009230	6781.682667	25.973197
182.258736	6787.884113	25.978215
182.447515	6808.999475	25.983232
182.442147	6821.622430	25.988250
183.011619	6835.239976	25.993268
182.680842	6847.104173	25.998285
182.680509	6860.063435	26.003303
183.312817	6871.502176	26.008320
183.534165	6889.786938	26.013338
183.884492	6908.259803	26.018356
184.068337	6915.507971	26.023373
183.884751	6920.671637	26.028391
184.428868	6930.979044	26.033408
184.597765	6947.496434	26.038426
185.113955	6952.650949	26.043444
185.123773	6969.346025	26.048461
185.713372	6977.012779	26.053479
186.001933	6964.191489	26.058496
185.777841	6980.385904	26.063514
186.202811	6976.888242	26.068532
186.494315	6984.458031	26.073549
186.796936	6970.089023	26.078567
187.240199	6967.232624	26.083584
187.297578	6968.575529	26.088602
187.591069	6973.137721	26.093620
187.520888	6962.579113	26.098637
187.692064	6970.552477	26.103655
188.000872	6972.616050	26.108672
187.857359	6974.721705	26.113690
188.056793	6967.278358	26.118708
188.142007	6968.820640	26.123725
188.222697	6974.986413	26.128743
188.373846	6956.913834	26.133760
188.127069	6978.164810	26.138778
188.250488	6991.910961	26.143796
188.372429	6998.338479	26.148813
188.417838	7018.456356	26.153831
188.762853	7024.604217	26.158848
188.790023	7054.195952	26.163866
188.818370	7058.747092	26.168884
188.839514	7084.725323	26.173901
189.040574	7103.812390	26.178919
189.677138	7131.141665	26.183936
189.470635	7147.761027	26.188954
189.939196	7159.791155	26.193972
190.003375	7182.692084	26.198989
190.085908	7194.988814	26.204007
190.900397	7211.125882	26.209024
191.037433	7225.270894	26.214042
191.592275	7242.621612	26.219060
191.727237	7254.176358	26.224077
191.573956	7261.518513	26.229095
192.133005	7268.036553	26.234112
192.407752	7288.268682	26.239130
192.630146	7274.401874	26.244148
192.697340	7285.727665	26.249165
192.504422	7299.599114	26.254183
193.034131	7306.610401	26.259200
193.193730	7323.848083	26.264218
193.439119	7333.446867	26.269236
193.639048	7344.698657	26.274253
193.469480	7356.006341	26.279271
193.781797	7365.516043	26.284288
194.141018	7385.202580	26.289306
194.524042	7383.801501	26.294324
194.565298	7404.797238	26.299341
194.400366	7420.549048	26.304359
195.045082	7421.222541	26.309376
195.192256	7447.731795	26.314394
195.693974	7437.269245	26.319412
195.543884	7427.983100	26.324429
195.371908	7452.176065	26.329447
196.056526	7449.746570	26.334464
196.221015	7464.678850	26.339482
196.196615	7480.014315	26.344500
196.299852	7488.345808	26.349517
196.308308	7496.911243	26.354535
197.040035	7513.915431	26.359552
196.856673	7517.442452	26.364570
197.076555	7541.481430	26.369588
197.320450	7555.582987	26.374605
197.515260	7559.305537	26.379623
197.589681	7572.428611	26.384640
197.786942	7579.446426	26.389658
198.188967	7607.574036	26.394676
198.930607	7608.934837	26.399693
198.647276	7623.099643	26.404711
198.971491	7632.438964	26.409728
199.465756	7633.604567	26.414746
199.583724	7635.868506	26.419764
199.823820	7635.977521	26.424781
199.710712	7634.694308	26.429799
199.772232	7652.391325	26.434816
200.103746	7658.640927	26.439834
200.398093	7666.720205	26.444852
200.361948	7672.767818	26.449869
200.442795	7687.944999	26.454887
200.991792	7687.119686	26.459904
200.991663	7703.594270	26.464922
200.836108	7716.600503	26.469940
201.671259	7723.498208	26.474957
201.163436	7731.774616	26.479975
201.755102	7740.541019	26.484992
201.764488	7760.123100	26.490010
201.913489	7772.722734	26.495028
202.081272	7783.628866	26.500045
202.196085	7798.643758	26.505063
202.774819	7817.768964	26.510080
202.740610	7824.387391	26.515098
203.003972	7840.549730	26.520116
203.084294	7853.657089	26.525133
203.247977	7871.414567	26.530151
203.033982	7886.616512	26.535168
203.612298	7905.105432	26.540186
204.435826	7917.526930	26.545204
204.983695	7925.439757	26.550221
204.940380	7935.976981	26.555239
204.897128	7937.497381	26.560256
205.208175	7950.557029	26.565274
205.673987	7964.591354	26.570292
205.959262	7975.598613	26.575309
205.724126	7979.174511	26.580327
206.205152	7974.939484	26.585344
206.218550	7995.136384	26.590362
206.608278	7997.320559	26.595380
206.944052	7994.905629	26.600397
206.923536	8015.505980	26.605415
206.882323	8029.548993	26.610432
207.253020	8018.192522	26.615450
207.589924	8042.425493	26.620468
208.288382	8043.957354	26.625485
208.245957	8048.047127	26.630503
208.641524	8041.074036	26.635520
208.474555	8047.783146	26.640538
208.570721	8063.017217	26.645556
209.234489	8075.694611	26.650573
209.039331	8080.824339	26.655591
208.930720	8079.088985	26.660608
209.166032	8092.522106	26.665626
209.016882	8106.964373	26.670644
209.010928	8133.858623	26.675661
209.111881	8154.268036	26.680679
209.900099	8163.833840	26.685696
210.327281	8188.304100	26.690714
209.869928	8207.696463	26.695732
210.362128	8211.084599	26.700749
210.568389	8243.045013	26.705767
210.650562	8251.761661	26.710784
210.922566	8280.977849	26.715802
210.868948	8294.059776	26.720820
211.197161	8311.398909	26.725837
211.549231	8330.510408	26.730855
211.805744	8344.965043	26.735872
212.109694	8368.161042	26.740890
212.377068	8379.542574	26.745908
212.801004	8388.231654	26.750925
213.084555	8411.747771	26.755943
213.632060	8404.961962	26.760960
213.569157	8407.575095	26.765978
213.523326	8419.690080	26.770996
214.096458	8419.643724	26.776013
214.009456	8431.685999	26.781031
214.640360	8445.118278	26.786048
214.679446	8449.975245	26.791066
214.819688	8445.275248	26.796084
215.213747	8449.532064	26.801101
215.152913	8472.589534	26.806119
215.395913	8482.352470	26.811136
215.695864	8481.347941	26.816154
215.867778	8499.718393	26.821172
216.269042	8507.720467	26.826189
216.239640	8515.017405	26.831207
216.541195	8516.682224	26.836224
216.761739	8534.982406	26.841242
216.989094	8531.809498	26.846260
217.246176	8547.963358	26.851277
217.574923	8568.337026	26.856295
217.456058	8570.340325	26.861312
217.340003	8581.788077	26.866330
217.787593	8604.047569	26.871348
217.883441	8619.772195	26.876365
218.295250	8639.846205	26.881383
218.456179	8650.967547	26.886400
218.398791	8671.988433	26.891418
218.452803	8687.371109	26.896436
219.029653	8697.969637	26.901453
219.931972	8708.076896	26.906471
220.307412	8710.290330	26.911488
220.679709	8709.937831	26.916506
220.639559	8716.949122	26.921524
220.843059	8707.546759	26.926541
221.082163	8724.501766	26.931559
221.107689	8739.391374	26.936576
221.585468	8736.001149	26.941594
221.558659	8752.433197	26.946612
221.811399	8753.189222	26.951629
221.828334	8761.338786	26.956647
222.050468	8773.735640	26.961664
222.422373	8789.278284	26.966682
222.197140	8803.306864	26.971700
222.557675	8814.410121	26.976717
222.791042	8828.907641	26.981735
222.907568	8835.614876	26.986752
223.367526	8852.222950	26.991770
223.554085	8868.175374	26.996788
223.638462	8866.870274	27.001805
223.734418	8893.910358	27.006823
224.031897	8896.673229	27.011840
224.448787	8918.632617	27.016858
224.540836	8928.648569	27.021876
224.899280	8950.256134	27.026893
224.881135	8956.747896	27.031911
225.104544	8976.141506	27.036928
225.475106	8987.038402	27.041946
225.654219	9005.035632	27.046964
225.761638	9011.203267	27.051981
226.166248	9041.578870	27.056999
226.339006	9053.590267	27.062016
226.576370	9053.755682	27.067034
226.756383	9091.741403	27.072052
227.111537	9080.738107	27.077069
227.192019	9111.469411	27.082087
227.530743	9130.461197	27.087104
227.967652	9123.377575	27.092122
227.686497	9151.698631	27.097140
228.025065	9159.457006	27.102157
228.245613	9182.873654	27.107175
228.096601	9186.882956	27.112192
228.319182	9204.670733	27.117210
228.389504	9230.402441	27.122228
229.050270	9239.464638	27.127245
228.996224	9259.879161	27.132263
229.546090	9277.957679	27.137280
230.272763	9273.531038	27.142298
230.306872	9294.858159	27.147316
230.647646	9302.149091	27.152333
230.712344	9316.964191	27.157351
230.845427	9331.416597	27.162368
231.158666	9342.825859	27.167386
231.137931	9361.525513	27.172404
231.467107	9377.469716	27.177421
231.626533	9387.065118	27.182439
232.015580	9403.119928	27.187456
232.180938	9394.167806	27.192474
232.577072	9429.124879	27.197492
232.861564	9436.292879	27.202509
232.779783	9457.937251	27.207527
232.933065	9470.788029	27.212544
233.623698	9474.461732	27.217562
233.709611	9492.827133	27.222580
234.506238	9494.932095	27.227597
234.810781	9506.461873	27.232615
234.920142	9515.751348	27.237632
235.293021	9519.666927	27.242650
235.320395	9530.167457	27.247668
235.564148	9543.935992	27.252685
235.423061	9549.951333	27.257703
235.369425	9570.061310	27.262720
236.087678	9580.024039	27.267738
236.252392	9600.096986	27.272756
236.348649	9607.891116	27.277773
236.814637	9611.598240	27.282791
236.578621	9624.089209	27.287808
237.331645	9639.377925	27.292826
237.723292	9651.514897	27.297844
238.216500	9659.557422	27.302861
238.529136	9660.111322	27.307879
238.585985	9664.834147	27.312896
238.815872	9653.727592	27.317914
238.829092	9671.969778	27.322932
238.794615	9683.765566	27.327949
239.113071	9683.787530	27.332967
239.278067	9714.592604	27.337984
239.614377	9721.346411	27.343002
239.839835	9732.568075	27.348020
239.827156	9744.160975	27.353037
240.095196	9759.065593	27.358055
240.037588	9777.543399	27.363072
240.440055	9792.737678	27.368090
240.636315	9816.649295	27.373108
240.824699	9827.318640	27.378125
240.967856	9847.554612	27.383143
241.086120	9868.539214	27.388160
241.713288	9882.375896	27.393178
241.426066	9903.283751	27.398196
242.164084	9932.100952	27.403213
242.821066	9932.321917	27.408231
243.204549	9950.793596	27.413248
243.605687	9950.165281	27.418266
244.026683	9971.080810	27.423284
243.929817	9969.682052	27.428301
244.266319	9967.235989	27.433319
244.363239	9986.462769	27.438336
245.008500	9986.607690	27.443354
245.288225	9983.503003	27.448372
245.761620	9976.981741	27.453389
245.721057	9975.687071	27.458407
245.841494	9970.437671	27.463424
246.235237	9967.638617	27.468442
246.131344	9985.170325	27.473460
246.278012	9993.083102	27.478477
246.765536	9998.941381	27.483495
246.402383	10010.906251	27.488512
246.590485	10018.506489	27.493530
247.030302	10040.557358	27.498548
247.273729	10049.109539	27.503565
247.451486	10065.375803	27.508583
247.240979	10076.483436	27.513600
247.763445	10095.376512	27.518618
247.597750	10118.263908	27.523636
247.881501	10130.419173	27.528653
248.165439	10159.502095	27.533671
248.159177	10190.692627	27.538688
248.658280	10204.832118	27.543706
249.139193	10219.762456	27.548724
249.161810	10248.629768	27.553741
249.625700	10258.439023	27.558759
249.744256	10286.958792	27.563776
249.656978	10311.822671	27.568794
250.121905	10335.361113	27.573812
250.357644	10356.845219	27.578829
251.097707	10371.789364	27.583847
251.121780	10396.221266	27.588864
251.502757	10410.552310	27.593882
251.823885	10432.380001	27.598900
251.970193	10449.450731	27.603917
252.610476	10466.747445	27.608935
252.802997	10475.949603	27.613952
253.016931	10490.318715	27.618970
253.097023	10508.916289	27.623988
253.702410	10521.403658	27.629005
253.937816	10530.650718	27.634023
253.984035	10549.575402	27.639040
254.000227	10556.626191	27.644058
254.411309	10574.756024	27.649076
255.030822	10591.345700	27.654093
255.242346	10596.939652	27.659111
255.107477	10619.962872	27.664128
255.760975	10638.609497	27.669146
255.851525	10650.926462	27.674164
255.951873	10666.245037	27.679181
256.500477	10675.220336	27.684199
256.518720	10693.188677	27.689216
256.757172	10714.719293	27.694234
257.151423	10726.807016	27.699252
257.285740	10739.107322	27.704269
257.436315	10750.676972	27.709287
257.759216	10780.036589	27.714304
258.065773	10798.780437	27.719322
258.140407	10812.902752	27.724340
258.220449	10832.855011	27.729357
258.821116	10846.785171	27.734375
258.725256	10873.808460	27.739392
258.962964	10884.679091	27.744410
259.046454	10908.333747	27.749428
259.454276	10925.047180	27.754445
259.696358	10955.428989	27.759463
260.202952	10975.483878	27.764480
260.632838	10987.140438	27.769498
261.061050	11007.391172	27.774516
261.103954	11024.649081	27.779533
261.652455	11037.633198	27.784551
261.577807	11054.507289	27.789568
262.173047	11069.985892	27.794586
262.260694	11073.638045	27.799604
262.512541	11089.868611	27.804621
262.669516	11100.992311	27.809639
262.489490	11118.799467	27.814656
263.159897	11140.239185	27.819674
263.490621	11164.776509	27.824692
263.444056	11175.436151	27.829709
263.801670	11177.718293	27.834727
263.845179	11195.017252	27.839744
264.434096	11225.827266	27.844762
264.571780	11235.903256	27.849780
264.458034	11273.128287	27.854797
264.748421	11285.474774	27.859815
265.103525	11310.688985	27.864832
265.595390	11331.413301	27.869850
266.084922	11350.573324	27.874868
266.026617	11364.996327	27.879885
266.445796	11378.236992	27.884903
266.751420	11409.258302	27.889920
267.009088	11425.923144	27.894938
267.281499	11450.532044	27.899956
267.439670	11471.327741	27.904973
267.973072	11484.270607	27.909991
267.875249	11508.843413	27.915008
268.676678	11526.557283	27.920026
269.046599	11535.072695	27.925044
269.070193	11560.555103	27.930061
269.536713	11569.016664	27.935079
269.569846	11596.301787	27.940096
269.902386	11605.357630	27.945114
270.486269	11621.197926	27.950132
270.693236	11651.259119	27.955149
270.996503	11661.638774	27.960167
270.972197	11682.239725	27.965184
271.076425	11701.895944	27.970202
271.398945	11708.288880	27.975220
271.122643	11745.726369	27.980237
271.937755	11759.308115	27.985255
272.191831	11784.615488	27.990272
272.336906	11796.891964	27.995290
272.955863	11819.210967	28.000308
273.260366	11835.375229	28.005325
273.640922	11840.543646	28.010343
273.976989	11870.405733	28.015360
274.347763	11877.647948	28.020378
274.999137	11885.287918	28.025396
275.466711	11898.872372	28.030413
275.780144	11900.556856	28.035431
276.064138	11903.177524	28.040448
276.026572	11907.209951	28.045466
276.122907	11924.168421	28.050484
275.652236	11935.096000	28.055501
276.270056	11958.838328	28.060519
276.577160	11975.853229	28.065536
276.684919	12000.365835	28.070554
276.895986	12009.883312	28.075572
277.021728	12031.376893	28.080589
277.611963	12054.206827	28.085607
277.659133	12068.196919	28.090624
278.063173	12091.990719	28.095642
278.380536	12126.936798	28.100660
278.964943	12149.679590	28.105677
279.117151	12160.719718	28.110695
279.384815	12184.585163	28.115712
279.345311	12200.160860	28.120730
279.793117	12213.752015	28.125748
279.823989	12232.035918	28.130765
279.864264	12249.462606	28.135783
279.896782	12271.309220	28.140800
280.313282	12295.039792	28.145818
280.571959	12314.990986	28.150836
280.839549	12347.897231	28.155853
281.100579	12365.559985	28.160871
281.289304	12393.956777	28.165888
281.520236	12427.258504	28.170906
282.530579	12432.654979	28.175924
282.446934	12461.554136	28.180941
282.904093	12475.333059	28.185959
283.289891	12499.051696	28.190976
283.498189	12519.473236	28.195994
283.903899	12537.570713	28.201012
283.978054	12563.914591	28.206029
284.661192	12567.479177	28.211047
285.261872	12594.610225	28.216064
285.311273	12605.224921	28.221082
285.725992	12608.403902	28.226100
286.182027	12629.636962	28.231117
286.725836	12632.964695	28.236135
287.158733	12655.468626	28.241152
287.315614	12673.787246	28.246170
287.895340	12662.866346	28.251188
287.946221	12665.502233	28.256205
288.214292	12676.658987	28.261223
288.100045	12681.470217	28.266240
288.400099	12688.480288	28.271258
288.416906	12707.994664	28.276276
288.534645	12733.020451	28.281293
289.012710	12749.579125	28.286311
289.305160	12773.531144	28.291328
289.497715	12786.257485	28.296346
290.152989	12801.470913	28.301364
290.290652	12822.769729	28.306381
290.334520	12831.888405	28.311399
290.714035	12847.620456	28.316416
290.888023	12870.309530	28.321434
291.380045	12892.192524	28.326452
291.568877	12913.750858	28.331469
291.683543	12932.278496	28.336487
292.426330	12932.864278	28.341504
292.473695	12960.275399	28.346522
293.151042	12977.768797	28.351540
293.282272	13001.486338	28.356557
293.224072	13012.549396	28.361575
293.256878	13037.154814	28.366592
293.327045	13071.143298	28.371610
293.964313	13085.606703	28.376628
294.180923	13119.279415	28.381645
294.359599	13145.710879	28.386663
294.564968	13169.955310	28.391680
294.659078	13193.171853	28.396698
295.021683	13202.980039	28.401716
295.376797	13243.904432	28.406733
295.940522	13276.080981	28.411751
296.309932	13301.087892	28.416768
296.486044	13334.914338	28.421786
297.068831	13351.286028	28.426804
296.862925	13377.964571	28.431821
297.233524	13410.099403	28.436839
297.675292	13432.276718	28.441856
297.424072	13473.732655	28.446874
298.065724	13497.200643	28.451892
298.775020	13514.780717	28.456909
298.873601	13527.401903	28.461927
299.593272	13536.282620	28.466944
300.358370	13551.896135	28.471962
300.891870	13565.494677	28.476980
300.898401	13577.946809	28.481997
301.113012	13586.288963	28.487015
301.554186	13592.486428	28.492032
301.578094	13612.404150	28.497050
301.913134	13613.309859	28.502068
302.029320	13643.574208	28.507085
302.306598	13649.425422	28.512103
302.916031	13664.352575	28.517120
302.883074	13686.580740	28.522138
303.101296	13711.134305	28.527156
303.115687	13725.068228	28.532173
303.809372	13737.641138	28.537191
304.287081	13751.301113	28.542208
304.581874	13787.051951	28.547226
304.897900	13786.805640	28.552244
304.971302	13813.671734	28.557261
305.135031	13822.279346	28.562279
305.560300	13844.302367	28.567296
305.686243	13870.947069	28.572314
305.756827	13892.200115	28.577332
306.197720	13921.478050	28.582349
306.499679	13956.580338	28.587367
306.579471	13983.967303	28.592384
306.840604	14007.915308	28.597402
306.899566	14022.228198	28.602420
307.384265	14063.889597	28.607437
307.975864	14089.926181	28.612455
308.595063	14110.174283	28.617472
308.233516	14138.312510	28.622490
308.967150	14157.982177	28.627508
309.427966	14179.407165	28.632525
309.635530	14201.313964	28.637543
309.978468	14222.479638	28.642560
310.329884	14254.075594	28.647578
310.792262	14276.327859	28.652596
311.030303	14285.538018	28.657613
311.155746	14309.439664	28.662631
311.830052	14336.124830	28.667648
312.182315	14359.111019	28.672666
312.622457	14384.452991	28.677684
312.825176	14400.953500	28.682701
312.942515	14419.282226	28.687719
313.787567	14434.054315	28.692736
313.782311	14468.192197	28.697754
314.047171	14481.412183	28.702772
314.400236	14517.537915	28.707789
314.341044	14532.324781	28.712807
314.871514	14545.803292	28.717824
314.782969	14573.818107	28.722842
315.231872	14597.694804	28.727860
315.604130	14621.644160	28.732877
316.162624	14651.335705	28.737895
316.147982	14677.694592	28.742912
316.244256	14706.901951	28.747930
316.520326	14736.940023	28.752948
317.622448	14749.319779	28.757965
317.815286	14765.496052	28.762983
318.227100	14784.362561	28.768000
318.703118	14814.999562	28.773018
319.003709	14818.093926	28.778036
319.335473	14840.915558	28.783053
319.568577	14863.045954	28.788071
319.784237	14880.358052	28.793088
319.661753	14905.589413	28.798106
320.001335	14932.510836	28.803124
320.531178	14946.647011	28.808141
320.433658	14976.140794	28.813159
321.079942	14992.732122	28.818176
320.976842	15029.086070	28.823194
321.522437	15046.781685	28.828212
321.640785	15077.303651	28.833229
322.171584	15099.566159	28.838247
322.539799	15120.738253	28.843264
322.793290	15149.611365	28.848282
323.028051	15172.745881	28.853300
323.496814	15200.366564	28.858317
323.827016	15226.208818	28.863335
324.549188	15237.206776	28.868352
324.598133	15271.171830	28.873370
324.869412	15290.954352	28.878388
325.354658	15313.699132	28.883405
325.641658	15340.912087	28.888423
326.020047	15344.449127	28.893440
326.331407	15375.570031	28.898458
326.820885	15393.820684	28.903476
327.048020	15422.142280	28.908493
327.492250	15446.775959	28.913511
327.864829	15460.716470	28.918528
328.351369	15477.686308	28.923546
328.483106	15501.003897	28.928564
329.012710	15517.779062	28.933581
329.171961	15550.427628	28.938599
329.795529	15563.544763	28.943616
329.786305	15579.783778	28.948634
330.071175	15614.063402	28.953652
330.549132	15630.336590	28.958669
330.793152	15648.070347	28.963687
331.036533	15675.700903	28.968704
331.040002	15695.983913	28.973722
331.346078	15734.170709	28.978740
331.651402	15749.900549	28.983757
331.415341	15790.956316	28.988775
332.442833	15810.698947	28.993792
332.354233	15852.497963	28.998810
332.778423	15885.834522	29.003828
333.225597	15906.349857	29.008845
333.513925	15942.097009	29.013863
333.968839	15977.356319	29.018880
334.390456	16002.798441	29.023898
334.770970	16042.051695	29.028916
335.288873	16062.873865	29.033933
335.384530	16098.456341	29.038951
335.621942	16115.690470	29.043968
336.043940	16152.043197	29.048986
336.513394	16176.762046	29.054004
336.795676	16201.909231	29.059021
336.885803	16238.219557	29.064039
337.658672	16265.927065	29.069056
338.034478	16283.943822	29.074074
338.225126	16314.638910	29.079092
339.016537	16333.715249	29.084109
338.911771	16363.650904	29.089127
339.454566	16390.785271	29.094144
339.992439	16419.003366	29.099162
339.883979	16434.444799	29.104180
340.432788	16466.504001	29.109197
340.150574	16502.533146	29.114215
340.797407	16530.529997	29.119232
341.217785	16559.474006	29.124250
341.233042	16591.555887	29.129268
341.832136	16622.054440	29.134285
341.461390	16657.326268	29.139303
342.238766	16688.444740	29.144320
342.740891	16719.178680	29.149338
343.559428	16739.603411	29.154356
344.247919	16748.831546	29.159373
344.530146	16750.802307	29.164391
345.120521	16772.845970	29.169408
345.986287	16790.291669	29.174426
346.007338	16799.566086	29.179444
346.228916	16796.168724	29.184461
346.241847	16820.614450	29.189479
346.547826	16820.407607	29.194496
346.993669	16855.755420	29.199514
346.560536	16869.455826	29.204532
347.594345	16883.601375	29.209549
347.246338	16914.379180	29.214567
347.912833	16936.229145	29.219584
348.328190	16974.083824	29.224602
348.696463	17004.509514	29.229620
349.289364	17016.688717	29.234637
349.480882	17035.882869	29.239655
349.729787	17065.075354	29.244672
350.007227	17083.243311	29.249690
350.233172	17109.912899	29.254708
350.953771	17128.896315	29.259725
350.662978	17161.313875	29.264743
351.188539	17186.559282	29.269760
351.530212	17211.373420	29.274778
351.555741	17252.770817	29.279796
351.843027	17279.945940	29.284813
352.356397	17320.477462	29.289831
352.910465	17343.040220	29.294848
353.170553	17380.492865	29.299866
353.563396	17410.384000	29.304884
354.037507	17439.927508	29.309901
354.101939	17481.382065	29.314919
354.606966	17510.647859	29.319936
355.104918	17542.024013	29.324954
355.043629	17577.829628	29.329972
355.968883	17610.150086	29.334989
356.102791	17634.044111	29.340007
356.638999	17668.697668	29.345024
356.958546	17712.066663	29.350042
357.350636	17734.822380	29.355060
357.788065	17760.641332	29.360077
357.939684	17789.594308	29.365095
358.325888	17822.228572	29.370112
359.037389	17850.907365	29.375130
359.079103	17876.076565	29.380148
359.707771	17904.606846	29.385165
360.158709	17933.887102	29.390183
360.430364	17951.281398	29.395200
361.002205	17972.632986	29.400218
361.164916	18008.704980	29.405236
361.594021	18035.512555	29.410253
362.111808	18058.556806	29.415271
361.748320	18087.710947	29.420288
362.242891	18117.069403	29.425306
362.544275	18157.516803	29.430324
363.192925	18181.307187	29.435341
363.740645	18218.170083	29.440359
364.232789	18230.324360	29.445376
364.558231	18250.593266	29.450394
365.130810	18278.184515	29.455412
365.879930	18293.923451	29.460429
366.167277	18313.550860	29.465447
366.571631	18330.357580	29.470464
367.350624	18337.044598	29.475482
367.647953	18355.904265	29.480500
367.895505	18370.607345	29.485517
368.001830	18397.079750	29.490535
368.661668	18399.325338	29.495552
368.897529	18398.893668	29.500570
368.899771	18422.796511	29.505588
369.267196	18425.716515	29.510605
369.814271	18448.438007	29.515623
369.394080	18464.128583	29.520640
370.082380	18481.307615	29.525658
369.336094	18522.702389	29.530676
370.017833	18537.383934	29.535693
369.942536	18577.503976	29.540711
370.473833	18616.322105	29.545728
371.192830	18655.094955	29.550746
371.397932	18704.143384	29.555764
371.631081	18730.311490	29.560781
372.179776	18768.294720	29.565799
372.676833	18801.910383	29.570816
372.894373	18837.059145	29.575834
373.298756	18888.455458	29.580852
373.941093	18919.165456	29.585869
374.161518	18952.018650	29.590887
374.441644	18984.365405	29.595904
375.315430	19011.270941	29.600922
375.495283	19048.188903	29.605940
376.246671	19070.133207	29.610957
376.619085	19103.476960	29.615975
376.896689	19127.369750	29.620992
377.452936	19151.227322	29.626010
377.702471	19174.751216	29.631028
378.444114	19198.718365	29.636045
378.746067	19230.858604	29.641063
379.049276	19254.717370	29.646080
379.946111	19273.052835	29.651098
380.276964	19286.130130	29.656116
380.857956	19321.952608	29.661133
381.074479	19325.807482	29.666151
381.348899	19361.075594	29.671168
381.650133	19378.684027	29.676186
381.609646	19403.854998	29.681204
382.223076	19426.421764	29.686221
382.291395	19461.531990	29.691239
382.403096	19487.212244	29.696256
382.854091	19524.480345	29.701274
383.391014	19561.379537	29.706292
383.794844	19588.137055	29.711309
384.021951	19627.317066	29.716327
384.008488	19654.922815	29.721344
384.750710	19687.627715	29.726362
384.793774	19730.543397	29.731380
385.052402	19769.972327	29.736397
385.542474	19811.204310	29.741415
385.339263	19856.448793	29.746432
385.784302	19892.228861	29.751450
386.092838	19950.461380	29.756468
386.626676	19987.746704	29.761485
387.583116	20036.095629	29.766503
387.625861	20081.569453	29.771520
388.196813	20118.133139	29.776538
388.426154	20163.349161	29.781556
388.915576	20199.519810	29.786573
389.232615	20253.332805	29.791591
389.589688	20294.338968	29.796608
390.521374	20322.323275	29.801626
390.877419	20372.226524	29.806644
391.313799	20403.925731	29.811661
391.983737	20431.844917	29.816679
392.352068	20455.801785	29.821696
393.068070	20484.271525	29.826714
393.578097	20510.938776	29.831732
393.738599	20534.783655	29.836749
394.163504	20552.937207	29.841767
394.548129	20586.825817	29.846784
395.302446	20605.107594	29.851802
395.080697	20630.416145	29.856820
395.256806	20654.701633	29.861837
395.549005	20682.371812	29.866855
395.623587	20719.169041	29.871872
396.280254	20753.028562	29.876890
396.496352	20791.054289	29.881908
396.831215	20831.603497	29.886925
397.276183	20869.296550	29.891943
397.353891	20909.174440	29.896960
398.088916	20939.481743	29.901978
398.343530	20987.262572	29.906996
398.858606	21022.893093	29.912013
399.502853	21073.835291	29.917031
399.975069	21095.776604	29.922048
400.763950	21120.585335	29.927066
401.533958	21156.290466	29.932084
401.842648	21182.281148	29.937101
402.297845	21211.993719	29.942119
402.434298	21236.083241	29.947136
402.967953	21263.362667	29.952154
403.047783	21280.891624	29.957172
403.205515	21307.513021	29.962189
403.737064	21338.307353	29.967207
404.309155	21374.670193	29.972224
404.959500	21409.071315	29.977242
404.587481	21454.201492	29.982260
405.147182	21496.102447	29.987277
405.491898	21519.678461	29.992295
405.410191	21568.697755	29.997312
405.947237	21614.462556	30.002330
406.683114	21655.183639	30.007348
406.993886	21689.520332	30.012365
407.646964	21725.060039	30.017383
408.292737	21770.558080	30.022400
408.830894	21802.690807	30.027418
409.183868	21844.393609	30.032436
409.812088	21866.727849	30.037453
410.233167	21893.774718	30.042471
410.348913	21928.194747	30.047488
410.551646	21956.034822	30.052506
411.139332	21993.372411	30.057524
411.361189	22030.680974	30.062541
412.093964	22071.036193	30.067559
412.390693	22100.505450	30.072576
413.276941	22139.633849	30.077594
413.849261	22164.218351	30.082612
414.273553	22196.145263	30.087629
414.715257	22208.709742	30.092647
415.087057	22249.825435	30.097664
415.454174	22258.794682	30.102682
415.903376	22299.246430	30.107700
415.913071	22327.817694	30.112717
416.674564	22357.872448	30.117735
416.995828	22400.270942	30.122752
417.500985	22421.033803	30.127770
417.611954	22448.344360	30.132788
417.880555	22487.107851	30.137805
418.274350	22518.677774	30.142823
418.144465	22555.183410	30.147840
418.853996	22593.476549	30.152858
419.809006	22627.857931	30.157876
420.017277	22671.414329	30.162893
420.412896	22688.105458	30.167911
420.803058	22729.178267	30.172928
420.950151	22766.366839	30.177946
421.665860	22802.975380	30.182964
422.250596	22829.052041	30.187981
422.740550	22850.861815	30.192999
422.653743	22877.128938	30.198016
423.009948	22905.052303	30.203034
423.675045	22941.786236	30.208052
424.020595	22969.903853	30.213069
424.464208	22998.282751	30.218087
425.059484	23038.557469	30.223104
425.308850	23068.039429	30.228122
425.701079	23099.777840	30.233140
426.001850	23135.126734	30.238157
426.854545	23165.224540	30.243175
426.989195	23201.813771	30.248192
427.887999	23234.483790	30.253210
428.224384	23267.887499	30.258228
428.368813	23294.127895	30.263245
428.545030	23327.403792	30.268263
429.106964	23370.359214	30.273280
429.299825	23411.281949	30.278298
429.407965	23438.425840	30.283316
429.980848	23478.197563	30.288333
430.701238	23530.749244	30.293351
431.143774	23564.618434	30.298368
431.613234	23616.243845	30.303386
432.036687	23651.111401	30.308404
432.563524	23685.842011	30.313421
432.565209	23725.278693	30.318439
432.993675	23765.954992	30.323456
433.408211	23806.201626	30.328474
434.504362	23848.306292	30.333492
434.610419	23890.736364	30.338509
434.913117	23931.170601	30.343527
435.177507	23979.712008	30.348544
435.850227	24022.365247	30.353562
436.413684	24064.650391	30.358580
437.173002	24117.774578	30.363597
437.640868	24143.126774	30.368615
437.436066	24198.196460	30.373632
437.881410	24231.030448	30.378650
438.584060	24279.247597	30.383668
438.647827	24326.568050	30.388685
439.214316	24363.318279	30.393703
439.544138	24418.350333	30.398720
439.573133	24463.633181	30.403738
440.317821	24510.869428	30.408756
440.646731	24569.680573	30.413773
441.562235	24619.128071	30.418791
441.810622	24669.758879	30.423808
442.471349	24715.789042	30.428826
443.296066	24746.611832	30.433844
443.107563	24797.239887	30.438861
444.008264	24822.710440	30.443879
444.184929	24876.555106	30.448896
444.508916	24920.821875	30.453914
445.386791	24969.560670	30.458932
445.897807	25003.123280	30.463949
446.524757	25038.451900	30.468967
447.132284	25083.428969	30.473984
447.424134	25120.075045	30.479002
447.832417	25151.667941	30.484020
448.228849	25196.431196	30.489037
448.814331	25231.581011	30.494055
449.038059	25268.216640	30.499072
449.347772	25310.032890	30.504090
449.957621	25341.775595	30.509108
450.237581	25384.000694	30.514125
450.712643	25410.795011	30.519143
450.917236	25456.801995	30.524160
451.888417	25470.966836	30.529178
453.306109	25486.085777	30.534196
453.818148	25508.723250	30.539213
454.298707	25523.215649	30.544231
454.445642	25531.817892	30.549248
454.919891	25566.564214	30.554266
455.455061	25587.671336	30.559284
455.743230	25622.259427	30.564301
456.645253	25620.144595	30.569319
456.906524	25652.888872	30.574336
457.088687	25673.218876	30.579354
457.494625	25693.243631	30.584372
457.545313	25727.688436	30.589389
457.837768	25757.544803	30.594407
457.941075	25789.012893	30.599424
458.236898	25831.318467	30.604442
459.061078	25872.173765	30.609460
459.198511	25919.751327	30.614477
459.918909	25964.998995	30.619495
459.993444	26005.916038	30.624512
460.573476	26045.241487	30.629530
460.614624	26084.886793	30.634548
460.827026	26140.625190	30.639565
461.519240	26183.430403	30.644583
462.282733	26240.468624	30.649600
462.281993	26297.148208	30.654618
462.678556	26347.355596	30.659636
462.886154	26412.930790	30.664653
463.576936	26467.493085	30.669671
463.860976	26518.893070	30.674688
464.459963	26582.498683	30.679706
464.823617	26631.195121	30.684724
465.207294	26690.086433	30.689741
466.111468	26747.664443	30.694759
466.417732	26799.547345	30.699776
466.685246	26864.666378	30.704794
467.158591	26924.616090	30.709812
467.736175	26987.958626	30.714829
468.389857	27048.181638	30.719847
469.061786	27098.635680	30.724864
469.780130	27145.309438	30.729882
470.321660	27195.634008	30.734900
470.936678	27232.593663	30.739917
472.560919	27249.061527	30.744935
473.112031	27274.988101	30.749952
473.497167	27320.531595	30.754970
473.887575	27354.737103	30.759988
474.324655	27385.729962	30.765005
474.952028	27415.164493	30.770023
475.272662	27446.899182	30.775040
475.013363	27487.616506	30.780058
475.734764	27517.890468	30.785076
475.882239	27559.694953	30.790093
476.080942	27602.872715	30.795111
476.590751	27657.408887	30.800128
477.345452	27706.018163	30.805146
477.638496	27753.871449	30.810164
477.812227	27802.015976	30.815181
478.180019	27852.472256	30.820199
478.709224	27903.163704	30.825216
479.085729	27948.880628	30.830234
479.602108	27994.593368	30.835252
480.198859	28053.860869	30.840269
480.548861	28103.831867	30.845287
481.360591	28149.527507	30.850304
481.674539	28206.255700	30.855322
482.039126	28248.177203	30.860340
482.608759	28289.979575	30.865357
483.108593	28337.159725	30.870375
483.833908	28383.264666	30.875392
483.871832	28433.077079	30.880410
484.150437	28467.877502	30.885428
484.558305	28523.865552	30.890445
484.709775	28575.271563	30.895463
485.516817	28627.783410	30.900480
485.444474	28693.218120	30.905498
485.978043	28745.157414	30.910516
486.475927	28817.971461	30.915533
487.060267	28875.817872	30.920551
487.968320	28930.585284	30.925568
488.538334	28987.163071	30.930586
489.359395	29031.553399	30.935604
489.997139	29084.785641	30.940621
490.310246	29139.305493	30.945639
490.875067	29181.741767	30.950656
491.441707	29237.544841	30.955674
491.928132	29289.764901	30.960692
492.213812	29341.478980	30.965709
492.663809	29394.954724	30.970727
493.489219	29444.118677	30.975744
494.016033	29494.045363	30.980762
494.542051	29538.798316	30.985780
494.911283	29585.858409	30.990797
495.780579	29643.398181	30.995815
496.525539	29677.385312	31.000832
496.897025	29720.239902	31.005850
497.224072	29759.246663	31.010868
497.843481	29802.643940	31.015885
498.530237	29851.895168	31.020903
499.279197	29884.948178	31.025920
499.379176	29949.756368	31.030938
500.265127	29971.564615	31.035956
500.455265	30022.346929	31.040973
501.103742	30062.260092	31.045991
501.451112	30105.760090	31.051008
502.057764	30153.668828	31.056026
502.421361	30193.175283	31.061044
502.946845	30237.822843	31.066061
503.441395	30287.365928	31.071079
504.495803	30330.092813	31.076096
504.286265	30380.740621	31.081114
504.890567	30421.851386	31.086132
505.204915	30470.708723	31.091149
505.609491	30527.303189	31.096167
506.038676	30579.492428	31.101184
506.514016	30632.141109	31.106202
507.092786	30682.422230	31.111220
507.497867	30739.856549	31.116237
507.611602	30797.080724	31.121255
508.474990	30857.616505	31.126272
508.606100	30916.608203	31.131290
509.194106	30967.592198	31.136308
509.411938	31023.039251	31.141325
509.875992	31091.526875	31.146343
510.280093	31144.551762	31.151360
510.784062	31226.307084	31.156378
511.370336	31285.675613	31.161396
511.671472	31358.242600	31.166413
512.229289	31427.053561	31.171431
513.699381	31482.666399	31.176448
514.563559	31519.868258	31.181466
515.414930	31565.310666	31.186484
515.863134	31613.148726	31.191501
516.214247	31650.391897	31.196519
516.682743	31689.833805	31.201536
516.919484	31746.816605	31.206554
517.361758	31780.981138	31.211572
517.785138	31834.036447	31.216589
518.376605	31884.299955	31.221607
518.606765	31924.441427	31.226624
518.859822	31985.120306	31.231642
519.496744	32042.179584	31.236660
519.975653	32097.466746	31.241677
520.422343	32161.985675	31.246695
521.064298	32207.120581	31.251712
521.316704	32272.782866	31.256730
521.738267	32322.223885	31.261748
522.170425	32387.219354	31.266765
522.596366	32459.561873	31.271783
523.231127	32507.948807	31.276800
524.241614	32583.425894	31.281818
524.789529	32629.000321	31.286836
525.601857	32678.929639	31.291853
525.808052	32741.032524	31.296871
526.710013	32793.083521	31.301888
527.250650	32842.834384	31.306906
527.469097	32908.406839	31.311924
528.194948	32964.233144	31.316941
528.661086	33023.267728	31.321959
529.526557	33073.482793	31.326976
530.099564	33124.169411	31.331994
530.885340	33180.529194	31.337012
531.580545	33220.874052	31.342029
531.716900	33279.140658	31.347047
532.098721	33323.390720	31.352064
532.932445	33373.365772	31.357082
533.424322	33428.705414	31.362100
533.826200	33473.062963	31.367117
534.440058	33538.663583	31.372135
534.970616	33581.378055	31.377152
535.193821	33637.684401	31.382170
535.910072	33678.418099	31.387188
536.663795	33732.623355	31.392205
537.211980	33793.660158	31.397223
538.016103	33826.266452	31.402240
538.847956	33869.228208	31.407258
539.712315	33916.264941	31.412276
540.316922	33950.419314	31.417293
540.582218	33991.017189	31.422311
542.134880	34015.474639	31.427328
542.149622	34059.102707	31.432346
542.606188	34092.155358	31.437364
543.386013	34123.623872	31.442381
543.674305	34154.451415	31.447399
543.754742	34196.724578	31.452416
544.287328	34234.018767	31.457434
544.327737	34289.205688	31.462452
545.184978	34329.352585	31.467469
544.989574	34383.581746	31.472487
545.333771	34433.003607	31.477504
546.191128	34497.727885	31.482522
546.517026	34561.628638	31.487540
547.282873	34610.791620	31.492557
547.190092	34681.951210	31.497575
547.985469	34727.089122	31.502592
548.401421	34788.817159	31.507610
548.808844	34847.823347	31.512628
549.573078	34914.615884	31.517645
549.958267	34992.946290	31.522663
550.954103	35048.898389	31.527680
551.215797	35115.898211	31.532698
551.853655	35172.863220	31.537716
552.541755	35206.393887	31.542733
553.239948	35270.617200	31.547751
553.908465	35333.507565	31.552768
554.475295	35374.692838	31.557786
554.961564	35413.887571	31.562804
555.594166	35467.982497	31.567821
555.817069	35524.159118	31.572839
556.557973	35576.219736	31.577856
556.570143	35640.832867	31.582874
557.541596	35694.995287	31.587892
557.919517	35746.210913	31.592909
558.471216	35804.915401	31.597927
559.151546	35860.480588	31.602944
559.711271	35923.157538	31.607962
559.780014	35989.391025	31.612980
560.521839	36040.086274	31.617997
560.904076	36113.034695	31.623015
561.431696	36176.945561	31.628032
562.186791	36234.528831	31.633050
562.529056	36309.611874	31.638068
563.527871	36368.676331	31.643085
564.040164	36433.310239	31.648103
564.582295	36493.451429	31.653120
565.309728	36555.929140	31.658138
565.668417	36617.953853	31.663156
566.323248	36685.058338	31.668173
566.743674	36747.751815	31.673191
567.348586	36815.774049	31.678208
568.016281	36886.550928	31.683226
568.496481	36960.076704	31.688244
569.182993	37024.705888	31.693261
569.524731	37090.393077	31.698279
570.045797	37173.700368	31.703296
570.795539	37231.795859	31.708314
571.534245	37297.196939	31.713332
572.087846	37363.793656	31.718349
572.603055	37429.323859	31.723367
573.082317	37501.258065	31.728384
573.733752	37555.993691	31.733402
574.301423	37640.725189	31.738420
575.616999	37692.134654	31.743437
576.232101	37753.233743	31.748455
577.325999	37802.979073	31.753472
577.770181	37859.265074	31.758490
578.303267	37912.269653	31.763508
579.277326	37958.219270	31.768525
579.863679	38017.070373	31.773543
580.432533	38058.687541	31.778560
580.505212	38100.456640	31.783578
580.803630	38167.947751	31.788596
581.237679	38218.046837	31.793613
581.695314	38277.920742	31.798631
582.069826	38341.422765	31.803648
582.629274	38404.648095	31.808666
583.075685	38473.551944	31.813684
583.893622	38532.372569	31.818701
584.665118	38608.230304	31.823719
584.895398	38673.900686	31.828736
585.221826	38735.855915	31.833754
585.714173	38812.300615	31.838772
586.241479	38885.921048	31.843789
586.646971	38962.544938	31.848807
587.299641	39038.013839	31.853824
588.092741	39111.347988	31.858842
588.145145	39194.862297	31.863860
588.944737	39270.822284	31.868877
589.401622	39355.024582	31.873895
589.921366	39425.911663	31.878912
590.833751	39498.665677	31.883930
590.998295	39580.272296	31.888948
591.627350	39641.406956	31.893965
593.082040	39706.151686	31.898983
594.308885	39760.811007	31.904000
595.182850	39807.975134	31.909018
595.440088	39876.104409	31.914036
596.086192	39926.766423	31.919053
596.693625	39978.691371	31.924071
597.330228	40028.105183	31.929088
597.883784	40084.215725	31.934106
598.180061	40138.718184	31.939124
598.986534	40198.742479	31.944141
599.142264	40259.863097	31.949159
599.879753	40329.072834	31.954176
600.320089	40386.819371	31.959194
600.659256	40462.743949	31.964212
601.323642	40525.504597	31.969229
602.230002	40599.984441	31.974247
602.886938	40672.286749	31.979264
603.444227	40728.521753	31.984282
603.662325	40802.636865	31.989300
604.243350	40866.192260	31.994317
604.913705	40940.854731	31.999335
605.453956	41018.124605	32.004352
606.401630	41081.790332	32.009370
606.878669	41150.553927	32.014388
607.955773	41211.856179	32.019405
608.560865	41278.900562	32.024423
609.080069	41342.881423	32.029440
610.620857	41390.017808	32.034458
611.327592	41441.864099	32.039476
612.288518	41490.615531	32.044493
612.861706	41552.359330	32.049511
613.133888	41607.959291	32.054528
613.768934	41650.413384	32.059546
614.114481	41713.685627	32.064564
614.845446	41763.501994	32.069581
615.185380	41814.201098	32.074599
615.457196	41877.868145	32.079616
615.781956	41934.309598	32.084634
616.552349	42007.772717	32.089652
616.926365	42080.468478	32.094669
617.529678	42148.185606	32.099687
617.830923	42222.374680	32.104704
618.585525	42291.989885	32.109722
618.913687	42380.502099	32.114740
619.698889	42451.997628	32.119757
620.249144	42531.122237	32.124775
620.750912	42604.013519	32.129792
621.369377	42681.220513	32.134810
621.731267	42767.676802	32.139828
622.361065	42846.407524	32.144845
623.068379	42930.363534	32.149863
623.679242	43015.270480	32.154880
624.884659	43093.496225	32.159898
625.686300	43149.713792	32.164916
627.372090	43201.977055	32.169933
628.262935	43252.598076	32.174951
628.433193	43320.192470	32.179968
629.288393	43378.507745	32.184986
629.719636	43445.370966	32.190004
630.210191	43495.367664	32.195021
630.888929	43565.969528	32.200039
631.100822	43632.623570	32.205056
632.112281	43686.139965	32.210074
632.525225	43755.662665	32.215092
632.840354	43818.129355	32.220109
633.710041	43871.783489	32.225127
633.741535	43933.195734	32.230144
634.460238	43987.516220	32.235162
635.241791	44050.765051	32.240180
635.528966	44121.569799	32.245197
636.125464	44194.934650	32.250215
636.801377	44264.267174	32.255232
637.368471	44331.714077	32.260250
638.050800	44407.307302	32.265268
638.263288	44467.646121	32.270285
639.385747	44546.179060	32.275303
639.886171	44619.927795	32.280320
640.641161	44689.760278	32.285338
640.901681	44769.340321	32.290356
641.772658	44835.964984	32.295373
642.612227	44905.935789	32.300391
642.876582	44999.519920	32.305408
643.526087	45058.111401	32.310426
644.532434	45144.736896	32.315444
645.258724	45213.518297	32.320461
645.959858	45288.950909	32.325479
646.579640	45358.091546	32.330496
647.342181	45433.625058	32.335514
648.002220	45507.436026	32.340532
648.602926	45576.258550	32.345549
649.294488	45645.928285	32.350567
649.540055	45736.048905	32.355584
650.347309	45800.410868	32.360602
650.718535	45887.852561	32.365620
651.285084	45963.714406	32.370637
652.482074	46049.601917	32.375655
652.178156	46139.960953	32.380672
652.967452	46214.460560	32.385690
653.429200	46316.686527	32.390708
653.981255	46409.093066	32.395725
654.757246	46494.979873	32.400743
655.600318	46589.467342	32.405760
656.329865	46678.318423	32.410778
656.992966	46769.277775	32.415796
657.964342	46849.913801	32.420813
659.026973	46923.619238	32.425831
659.584454	47015.184673	32.430848
660.204634	47090.198963	32.435866
660.879816	47183.011988	32.440884
661.543918	47267.054530	32.445901
662.637434	47325.314048	32.450919
662.981235	47418.252719	32.455936
664.110580	47483.432206	32.460954
664.535496	47569.625330	32.465972
665.158159	47647.938355	32.470989
666.098971	47721.120779	32.476007
667.263465	47789.317707	32.481024
668.050405	47851.687815	32.486042
668.725306	47912.068209	32.491060
669.291790	47985.095893	32.496077
669.965387	48051.613067	32.501095
670.353240	48123.208749	32.506112
671.316229	48183.447427	32.511130
671.598924	48263.872192	32.516148
672.090036	48333.521912	32.521165
672.768891	48414.301563	32.526183
672.967082	48492.069534	32.531200
673.676857	48567.068443	32.536218
674.018801	48655.670972	32.541236
674.659484	48740.614498	32.546253
675.395980	48822.753799	32.551271
675.724289	48916.684528	32.556288
676.802657	48996.929730	32.561306
677.370260	49094.832556	32.566324
677.738096	49169.625304	32.571341
678.445048	49244.782088	32.576359
678.953569	49341.138951	32.581376
679.322373	49426.133810	32.586394
679.922975	49504.413879	32.591412
680.714026	49604.597247	32.596429
681.528195	49694.045234	32.601447
681.920090	49788.326557	32.606464
682.815311	49874.499339	32.611482
683.323245	49960.743125	32.616500
684.345975	50043.560233	32.621517
685.553819	50138.323684	32.626535
686.627672	50204.582888	32.631552
687.646927	50293.816423	32.636570
688.922775	50357.168431	32.641588
689.512372	50432.526212	32.646605
690.479390	50495.471973	32.651623
690.555203	50572.703303	32.656640
691.440885	50632.978300	32.661658
691.854856	50695.770173	32.666676
692.255681	50782.796616	32.671693
693.251815	50857.741120	32.676711
693.363487	50947.279968	32.681728
694.319541	51026.874853	32.686746
695.120449	51117.670872	32.691764
695.409331	51197.105587	32.696781
696.480183	51273.290098	32.701799
696.989350	51353.743855	32.706816
698.011379	51440.316347	32.711834
698.739344	51517.657951	32.716852
699.502902	51605.474378	32.721869
700.287222	51664.556493	32.726887
701.312626	51745.570533	32.731904
702.130679	51822.272975	32.736922
702.913982	51894.262383	32.741940
703.600747	51963.747429	32.746957
704.351057	52031.882874	32.751975
704.779778	52110.255724	32.756992
705.678699	52173.925805	32.762010
706.665333	52236.229583	32.767028
707.265263	52312.976491	32.772045
707.806632	52376.978254	32.777063
708.510036	52455.325841	32.782080
709.059179	52539.037740	32.787098
709.739247	52612.481043	32.792116
710.349749	52687.452412	32.797133
710.837820	52767.820750	32.802151
711.110901	52852.868636	32.807168
711.515327	52950.183108	32.812186
712.593608	53027.106115	32.817204
713.150672	53123.770648	32.822221
714.097330	53213.313953	32.827239
714.918062	53294.052518	32.832256
715.229622	53388.573137	32.837274
715.881743	53477.553714	32.842292
716.408863	53563.352246	32.847309
717.666369	53649.737508	32.852327
718.274580	53745.651094	32.857344
719.002117	53844.085189	32.862362
720.181040	53909.723577	32.867380
720.739592	54001.622054	32.872397
721.680922	54086.684388	32.877415
722.248971	54166.918820	32.882432
723.143663	54243.864448	32.887450
724.047415	54333.622170	32.892468
724.124142	54426.771490	32.897485
724.657217	54498.957345	32.902503
725.489095	54585.910210	32.907520
726.061246	54670.499304	32.912538
727.088132	54741.378314	32.917556
727.477219	54824.924347	32.922573
728.251705	54904.078660	32.927591
729.062266	54991.712920	32.932608
729.341244	55078.911391	32.937626
729.837910	55170.648673	32.942644
730.654124	55262.996771	32.947661
731.538157	55359.845466	32.952679
732.215346	55455.067195	32.957696
732.439770	55560.518517	32.962714
733.736475	55645.092589	32.967732
733.947770	55764.208023	32.972749
734.811307	55847.066692	32.977767
735.501167	55947.729066	32.982784
736.712708	56048.052593	32.987802
737.453460	56142.906903	32.992820
738.136799	56231.888392	32.997837
739.488953	56329.226479	33.002855
740.123554	56422.696967	33.007872
740.741782	56524.195604	33.012890
741.460748	56607.492174	33.017908
742.160728	56708.213588	33.022925
742.875228	56802.923747	33.027943
743.451703	56895.451935	33.032960
744.388130	56999.187647	33.037978
745.317170	57088.549230	33.042996
746.176466	57188.001759	33.048013
746.965671	57268.818661	33.053031
747.758038	57363.872426	33.058048
748.744516	57449.200784	33.063066
749.566327	57537.381531	33.068084
749.972648	57628.159341	33.073101
750.868329	57714.085272	33.078119
751.251517	57821.215754	33.083136
751.782099	57911.234857	33.088154
752.595350	58023.761247	33.093172
753.317224	58126.078646	33.098189
753.857002	58216.723213	33.103207
754.870942	58322.847980	33.108224
755.354734	58427.671030	33.113242
756.071701	58528.651560	33.118260
756.753827	58645.020190	33.123277
757.609663	58745.820767	33.128295
758.675081	58858.392120	33.133312
759.638204	58954.436210	33.138330
761.180550	59031.823683	33.143348
761.938153	59128.509411	33.148365
762.738377	59212.258336	33.153383
764.248833	59295.965541	33.158400
765.134113	59369.481940	33.163418
765.887329	59436.075059	33.168436
766.668402	59524.252325	33.173453
767.702204	59596.575726	33.178471
768.133629	59660.745620	33.183488
768.772129	59746.577570	33.188506
769.813098	59813.977353	33.193524
770.244946	59897.341556	33.198541
770.758001	59974.214644	33.203559
771.542655	60058.443658	33.208576
771.886286	60142.461834	33.213594
772.761440	60225.633715	33.218612
773.155992	60323.472473	33.223629
773.767094	60420.953427	33.228647
774.351497	60504.212636	33.233664
774.691219	60599.761293	33.238682
775.687258	60699.644549	33.243700
776.320204	60803.374391	33.248717
776.939347	60894.447562	33.253735
777.990937	60979.893817	33.258752
779.053098	61068.840131	33.263770
779.820141	61158.714352	33.268788
780.386704	61243.300498	33.273805
781.274058	61341.637494	33.278823
782.519006	61423.552009	33.283840
782.933417	61523.320962	33.288858
783.372734	61604.541962	33.293876
784.175754	61718.285153	33.298893
784.250947	61808.719521	33.303911
785.698797	61908.615864	33.308928
786.143535	62014.253992	33.313946
787.095400	62111.951924	33.318964
788.304207	62207.446000	33.323981
788.901165	62298.472225	33.328999
789.775593	62407.675451	33.334016
790.239916	62501.726942	33.339034
791.680987	62603.985448	33.344052
792.839725	62696.727930	33.349069
793.860575	62787.502654	33.354087
794.484172	62878.015037	33.359104
795.221796	62971.169990	33.364122
796.153327	63056.910330	33.369140
796.832536	63153.678736	33.374157
796.978749	63258.367780	33.379175
798.468584	63346.159462	33.384192
799.669145	63431.256205	33.389210
800.959437	63505.775898	33.394228
801.586131	63596.278281	33.399245
802.349193	63675.089635	33.404263
803.291240	63757.594732	33.409280
804.056219	63840.230690	33.414298
804.433542	63931.528155	33.419316
805.292141	64020.078575	33.424333
805.869582	64113.435949	33.429351
806.562790	64204.094303	33.434368
807.047517	64309.048536	33.439386
807.513780	64403.443401	33.444404
808.267015	64502.626908	33.449421
809.029117	64610.608809	33.454439
810.062638	64730.323057	33.459456
810.497476	64836.527240	33.464474
811.436019	64953.521342	33.469492
811.333603	65066.029920	33.474509
812.718533	65162.658959	33.479527
813.805015	65267.733077	33.484544
814.879722	65386.502345	33.489562
815.499949	65491.212471	33.494580
816.071603	65606.994168	33.499597
817.164072	65719.345853	33.504615
818.701546	65816.970408	33.509632
819.433297	65932.000328	33.514650
820.623757	66029.771987	33.519668
821.485641	66123.400928	33.524685
822.063120	66221.597649	33.529703
822.850091	66308.639800	33.534720
823.565509	66415.342801	33.539738
824.708902	66510.431368	33.544756
825.746981	66609.969577	33.549773
826.648105	66698.404206	33.554791
827.512772	66796.505373	33.559808
828.104549	66893.703981	33.564826
828.954476	66981.844843	33.569844
829.717519	67076.088724	33.574861
830.819270	67165.889216	33.579879
832.443190	67222.462457	33.584896
833.191813	67316.829933	33.589914
833.967492	67376.446289	33.594932
834.586723	67448.082106	33.599949
834.952948	67529.610280	33.604967
836.284737	67596.557315	33.609984
836.736826	67690.501514	33.615002
837.107288	67770.898219	33.620020
837.698750	67859.996079	33.625037
837.855966	67966.009302	33.630055
838.425501	68063.703823	33.635072
839.278551	68186.066299	33.640090
839.823619	68290.771239	33.645108
840.485415	68397.436278	33.650125
840.805490	68525.402438	33.655143
841.700492	68651.238056	33.660160
842.409090	68786.968707	33.665178
843.338720	68905.617545	33.670196
844.088416	69033.313127	33.675213
844.786144	69165.058352	33.680231
845.981277	69290.759421	33.685248
846.640718	69424.706622	33.690266
847.375036	69564.851315	33.695284
848.427335	69689.946158	33.700301
849.234370	69820.697238	33.705319
850.252330	69952.735617	33.710336
851.275489	70092.740986	33.715354
851.835030	70233.652549	33.720372
852.818768	70362.385839	33.725389
854.073910	70495.633856	33.730407
855.660914	70603.389383	33.735424
856.975797	70731.734800	33.740442
857.905443	70831.785070	33.745460
858.716766	70953.398918	33.750477
859.262089	71058.471502	33.755495
860.736469	71174.108494	33.760512
861.673416	71284.245429	33.765530
862.611176	71395.078370	33.770548
863.760922	71495.702248	33.775565
864.550048	71609.406521	33.780583
865.331505	71717.459434	33.785600
866.164403	71816.682991	33.790618
866.613825	71923.932046	33.795636
867.392340	72035.180448	33.800653
867.969121	72166.066229	33.805671
868.794616	72272.211188	33.810688
869.684120	72382.001151	33.815706
870.604879	72514.191544	33.820724
871.709599	72628.417932	33.825741
872.102717	72762.613525	33.830759
873.035160	72883.522521	33.835776
874.032126	73002.505339	33.840794
874.764023	73120.135216	33.845812
876.004572	73238.977718	33.850829
876.445007	73369.811177	33.855847
877.366395	73484.635335	33.860864
878.001142	73611.586655	33.865882
878.740889	73747.590066	33.870900
879.775680	73876.032259	33.875917
880.796610	74010.928184	33.880935
881.867667	74132.118343	33.885952
882.885065	74269.508195	33.890970
883.454278	74394.040097	33.895988
884.800950	74504.346723	33.901005
885.377915	74640.502867	33.906023
885.863977	74762.407075	33.911040
886.991178	74891.700013	33.916058
887.755254	75013.470928	33.921076
889.102976	75127.043947	33.926093
889.495271	75256.486305	33.931111
890.379729	75371.712291	33.936128
891.132795	75490.192566	33.941146
892.643452	75595.171106	33.946164
893.682017	75699.324073	33.951181
894.461429	75818.389935	33.956199
895.853075	75919.740418	33.961216
897.061349	76021.988296	33.966234
897.898526	76124.279265	33.971252
899.089445	76230.926727	33.976269
900.004297	76327.545023	33.981287
900.504757	76429.792093	33.986304
901.354685	76526.712980	33.991322
901.967351	76641.200088	33.996340
902.991040	76740.306802	34.001357
903.639642	76862.119733	34.006375
904.794863	76971.559692	34.011392
905.660520	77080.687721	34.016410
906.058024	77201.671328	34.021428
907.243901	77318.135101	34.026445
907.636934	77452.460534	34.031463
908.463155	77572.881640	34.036480
909.342831	77712.004608	34.041498
910.151908	77833.935379	34.046516
911.097518	77958.620972	34.051533
911.627359	78107.456905	34.056551
912.308592	78244.054350	34.061568
913.297672	78374.744180	34.066586
913.921267	78537.078548	34.071604
915.292683	78664.069459	34.076621
915.819731	78818.122804	34.081639
916.904806	78961.021111	34.086656
917.729196	79117.740846	34.091674
918.532229	79263.142233	34.096692
919.724378	79396.018299	34.101709
920.444681	79557.970772	34.106727
921.435123	79693.241579	34.111744
922.641810	79854.533484	34.116762
923.179566	80008.409743	34.121780
924.138497	80164.728545	34.126797
924.936823	80310.757406	34.131815
926.174454	80461.053951	34.136832
927.974319	80597.891213	34.141850
928.635961	80752.289681	34.146868
929.694460	80880.546972	34.151885
931.229726	81025.313100	34.156903
931.881520	81156.568469	34.161920
932.858099	81298.398801	34.166938
933.468747	81441.916604	34.171956
934.296478	81574.037188	34.176973
935.488625	81713.828882	34.181991
937.211294	81844.727028	34.187008
938.054749	81970.818235	34.192026
939.123487	82108.949998	34.197044
939.845149	82225.623718	34.202061
941.075797	82357.561763	34.207079
942.120890	82470.735087	34.212096
943.553189	82586.849851	34.217114
944.272142	82715.983621	34.222132
944.858938	82829.937035	34.227149
945.634881	82973.240884	34.232167
946.407776	83089.961112	34.237184
947.529418	83228.691883	34.242202
948.082244	83365.486978	34.247220
948.615250	83494.864764	34.252237
949.889318	83634.426809	34.257255
950.716309	83773.893067	34.262272
951.450464	83894.932445	34.267290
952.341625	84021.052295	34.272308
953.686927	84153.247348	34.277325
954.658793	84272.028460	34.282343
955.817164	84390.095903	34.287360
956.807959	84516.549909	34.292378
957.286203	84639.318669	34.297396
958.839073	84756.076054	34.302413
959.519695	84869.454510	34.307431
960.103486	85007.424709	34.312448
960.983527	85140.708642	34.317466
961.738977	85277.740822	34.322484
963.027875	85402.365866	34.327501
963.544719	85537.110692	34.332519
964.562886	85690.679542	34.337536
965.357376	85818.210903	34.342554
965.992175	85975.293727	34.347572
967.150643	86116.237640	34.352589
968.001440	86274.368641	34.357607
969.006968	86424.565458	34.362624
970.199387	86572.530182	34.367642
971.110507	86722.206717	34.372660
971.954826	86870.338657	34.377677
972.898962	87020.751964	34.382695
973.735367	87172.886303	34.387712
974.579464	87330.342112	34.392730
975.147398	87494.356255	34.397748
976.502279	87665.334620	34.402765
977.503928	87822.299292	34.407783
978.469816	87989.275629	34.412800
980.290100	88133.412395	34.417818
981.121505	88288.225210	34.422836
983.058782	88422.276227	34.427853
984.217247	88547.097796	34.432871
985.540777	88695.262903	34.437888
986.869837	88821.620689	34.442906
987.696746	88954.327527	34.447924
988.891483	89086.841169	34.452941
989.836639	89216.663095	34.457959
990.467162	89351.739916	34.462976
991.492518	89476.930190	34.467994
992.547306	89610.849575	34.473012
993.316499	89743.481781	34.478029
994.199295	89879.620890	34.483047
994.904745	90028.637293	34.488064
996.073480	90169.097344	34.493082
996.701882	90313.672931	34.498100
997.257962	90463.128184	34.503117
998.545130	90606.526660	34.508135
999.315243	90763.270650	34.513152
1000.528821	90917.651026	34.518170
1001.166410	91078.437879	34.523188
1001.987896	91221.727428	34.528205
1003.184848	91391.727078	34.533223
1004.215568	91542.546938	34.538240
1005.426910	91693.173211	34.543258
1006.014661	91859.859553	34.548276
1006.783530	92012.466295	34.553293
1007.729691	92183.532113	34.558311
1008.606070	92362.990613	34.563328
1009.710966	92529.412188	34.568346
1010.414298	92699.851030	34.573364
1011.376811	92867.152998	34.578381
1011.825477	93043.832947	34.583399
1012.738371	93235.254392	34.588416
1014.586497	93402.197867	34.593434
1015.137137	93577.940647	34.598452
1016.429762	93747.573772	34.603469
1017.602736	93921.259902	34.608487
1018.589596	94087.774972	34.613504
1019.836648	94236.834946	34.618522
1021.256185	94391.336109	34.623540
1022.405506	94536.869458	34.628557
1023.591688	94700.064108	34.633575
1024.038684	94848.114842	34.638592
1026.006601	94980.120971	34.643610
1027.009941	95129.277426	34.648628
1028.084339	95277.587433	34.653645
1029.133134	95425.149305	34.658663
1029.417389	95582.011173	34.663680
1030.533996	95726.284616	34.668698
1031.381590	95888.562127	34.673716
1032.875357	96039.009990	34.678733
1033.866501	96194.707620	34.683751
1034.289397	96375.163197	34.688768
1035.669831	96525.544184	34.693786
1036.473745	96696.880210	34.698804
1036.935125	96864.520330	34.703821
1038.012845	97034.331926	34.708839
1039.493247	97190.397714	34.713856
1041.048645	97358.087505	34.718874
1042.074352	97528.442846	34.723892
1043.234362	97694.219030	34.728909
1044.335282	97861.778690	34.733927
1045.381803	98024.334597	34.738944
1046.391604	98189.689494	34.743962
1047.507933	98347.551173	34.748980
1048.569304	98519.350717	34.753997
1049.849330	98681.612554	34.759015
1050.505627	98850.278155	34.764032
1051.657216	99005.213225	34.769050
1052.645308	99175.820180	34.774068
1054.512680	99330.518184	34.779085
1055.997472	99485.464213	34.784103
1056.896006	99643.661341	34.789120
1058.019342	99794.231141	34.794138
1059.121709	99938.467825	34.799156
1059.916576	100099.369396	34.804173
1061.652945	100239.513934	34.809191
1063.595544	100369.608968	34.814208
1064.499588	100508.316604	34.819226
1065.416640	100645.743905	34.824244
1065.953689	100800.114416	34.829261
1067.198927	100936.988649	34.834279
1067.963424	101090.316475	34.839296
1068.956121	101231.368610	34.844314
1070.163362	101370.752394	34.849332
1070.979186	101524.821414	34.854349
1072.130916	101683.147430	34.859367
1072.727137	101839.363186	34.864384
1073.655906	101994.676267	34.869402
1074.756660	102151.462359	34.874420
1075.331245	102306.842415	34.879437
1076.431230	102483.714928	34.884455
1077.374053	102645.639965	34.889472
1078.667338	102811.895844	34.894490
1079.834447	102982.251468	34.899508
1080.665355	103135.656396	34.904525
1082.234205	103301.071860	34.909543
1082.873115	103480.136209	34.914560
1083.804584	103631.938037	34.919578
1084.776185	103812.646459	34.924596
1085.750198	103982.502432	34.929613
1086.802464	104162.275393	34.934631
1087.551561	104347.748240	34.939648
1088.395002	104524.202248	34.944666
1089.288641	104711.591359	34.949684
1089.852337	104897.339475	34.954701
1090.979843	105078.499344	34.959719
1091.589893	105273.323095	34.964736
1092.245070	105462.251568	34.969754
1093.714793	105663.027425	34.974772
1094.836845	105849.132874	34.979789
1096.302875	106047.214575	34.984807
1097.168349	106235.062452	34.989824
1098.463583	106448.614577	34.994842
1099.472488	106643.926842	34.999860
1100.336137	106843.380977	35.004877
1101.574679	107033.135767	35.009895
1102.634894	107242.376229	35.014912
1103.970260	107444.543077	35.019930
1104.772096	107652.145041	35.024948
1105.496393	107862.370701	35.029965
1107.000840	108076.103781	35.034983
1107.981220	108290.698157	35.040000
1108.942369	108501.117506	35.045018
1110.120379	108711.565851	35.050036
1111.446578	108926.285239	35.055053
1113.137363	109127.987772	35.060071
1114.096379	109345.697425	35.065088
1115.659007	109547.677683	35.070106
1116.917569	109750.077235	35.075124
1117.629720	109972.557671	35.080141
1118.845825	110168.494477	35.085159
1120.006433	110373.549697	35.090176
1121.281783	110592.230223	35.095194
1122.377388	110791.979053	35.100212
1123.437989	111005.200809	35.105229
1124.419146	111217.512661	35.110247
1125.593282	111434.987936	35.115264
1126.368849	111645.094997	35.120282
1127.833006	111868.289474	35.125300
1128.611220	112086.582990	35.130317
1130.491679	112296.752398	35.135335
1131.354262	112521.192093	35.140352
1132.865833	112729.348385	35.145370
1134.408838	112928.037662	35.150388
1135.153579	113154.161597	35.155405
1136.371707	113361.041102	35.160423
1137.633188	113570.512051	35.165440
1138.450000	113781.527934	35.170458
1140.361124	113986.447449	35.175476
1141.514281	114189.758554	35.180493
1142.939619	114379.381305	35.185511
1144.548247	114568.860906	35.190528
1145.813912	114758.157967	35.195546
1147.143273	114948.877376	35.200564
1147.736997	115154.252026	35.205581
1149.297374	115338.233581	35.210599
1149.949500	115532.857494	35.215616
1151.207319	115721.136073	35.220634
1153.036272	115907.053254	35.225652
1153.948957	116093.617788	35.230669
1155.333211	116282.208535	35.235687
1156.260859	116469.203832	35.240704
1157.303035	116656.561460	35.245722
1158.648238	116840.905210	35.250740
1159.698348	117036.461666	35.255757
1160.864853	117222.028531	35.260775
1161.803006	117409.028236	35.265792
1162.938159	117602.217734	35.270810
1164.362549	117788.302987	35.275828
1165.243374	117980.460213	35.280845
1166.755518	118160.552724	35.285863
1167.708330	118352.966578	35.290880
1168.722339	118531.522166	35.295898
1170.040386	118701.234699	35.300916
1171.283532	118873.862344	35.305933
1172.622729	119042.496322	35.310951
1173.184064	119224.996001	35.315968
1174.159982	119410.836649	35.320986
1175.696991	119595.064827	35.326004
1176.316268	119778.267964	35.331021
1177.590370	119960.172489	35.336039
1178.562823	120163.809459	35.341056
1179.434900	120352.929960	35.346074
1180.573806	120547.456318	35.351092
1181.535169	120748.615506	35.356109
1182.399942	120959.650942	35.361127
1183.392550	121168.385700	35.366144
1184.241541	121391.249948	35.371162
1185.393593	121601.101817	35.376180
1186.269367	121836.700663	35.381197
1187.493389	122063.360176	35.386215
1188.863632	122301.795369	35.391232
1189.889639	122530.607623	35.396250
1192.083110	122733.996407	35.401268
1194.358504	122926.715094	35.406285
1195.788575	123138.077792	35.411303
1197.345052	123340.118989	35.416320
1198.659768	123543.481643	35.421338
1199.838111	123734.752692	35.426356
1201.168811	123929.079298	35.431373
1202.172230	124133.257983	35.436391
1203.228224	124344.754602	35.441408
1204.168597	124544.688241	35.446426
1206.068923	124723.400362	35.451444
1207.251490	124931.128691	35.456461
1208.376764	125128.209272	35.461479
1209.237432	125333.294231	35.466496
1210.113603	125533.815368	35.471514
1211.363973	125740.181865	35.476532
1212.330480	125963.364751	35.481549
1213.801100	126182.574650	35.486567
1214.853399	126393.870679	35.491584
1215.713712	126609.496641	35.496602
1216.991241	126817.031942	35.501620
1217.856637	127055.917925	35.506637
1218.991295	127272.656415	35.511655
1219.933294	127500.911744	35.516672
1221.163704	127740.857859	35.521690
1222.014575	127974.138374	35.526708
1222.956670	128226.088580	35.531725
1224.305218	128455.424253	35.536743
1225.662743	128699.957782	35.541760
1226.651516	128952.007518	35.546778
1228.123670	129199.339877	35.551796
1230.044291	129421.603563	35.556813
1231.341973	129656.280225	35.561831
1232.845951	129885.689331	35.566848
1234.277687	130121.564102	35.571866
1235.411833	130339.921141	35.576884
1236.706230	130581.171373	35.581901
1237.900480	130802.132896	35.586919
1239.071108	131035.167634	35.591936
1240.096316	131282.108766	35.596954
1241.532251	131505.316826	35.601972
1242.425754	131740.342183	35.606989
1243.849643	131978.310995	35.612007
1245.188386	132201.235801	35.617024
1246.558380	132427.579700	35.622042
1247.952709	132659.486300	35.627060
1249.243080	132896.989673	35.632077
1250.361553	133109.131193	35.637095
1251.587236	133315.754452	35.642112
1252.698619	133528.001313	35.647130
1254.303606	133730.266732	35.652148
1255.418940	133951.072871	35.657165
1256.011003	134175.833927	35.662183
1257.880866	134385.108151	35.667200
1259.027411	134617.120569	35.672218
1260.111840	134834.134526	35.677236
1260.885516	135069.127868	35.682253
1261.861979	135301.008527	35.687271
1263.097636	135544.308724	35.692288
1263.889774	135781.104361	35.697306
1265.528282	136028.588465	35.702324
1266.834715	136273.593848	35.707341
1267.487433	136523.286359	35.712359
1268.925025	136763.164224	35.717376
1270.253256	137027.873870	35.722394
1271.829818	137265.082482	35.727412
1273.076412	137518.969328	35.732429
1274.380363	137781.153219	35.737447
1275.815990	138027.963134	35.742464
1276.819885	138296.869934	35.747482
1278.237218	138552.029526	35.752500
1279.981718	138795.864955	35.757517
1281.359657	139045.963123	35.762535
1282.931563	139287.041268	35.767552
1284.383054	139533.922944	35.772570
1285.732102	139771.643384	35.777588
1287.608261	140023.517322	35.782605
1288.753195	140260.666396	35.787623
1290.243638	140506.039746	35.792640
1290.913859	140748.241427	35.797658
1292.327720	140982.890975	35.802676
1293.614112	141225.995537	35.807693
1295.072432	141475.286595	35.812711
1296.411874	141715.925842	35.817728
1297.987985	141960.344301	35.822746
1299.449767	142203.173020	35.827764
1301.062699	142432.435526	35.832781
1302.916284	142663.308108	35.837799
1304.674351	142869.064874	35.842816
1305.867037	143111.551438	35.847834
1306.984622	143318.900725	35.852852
1308.335707	143543.268390	35.857869
1309.295016	143777.669758	35.862887
1311.112765	144007.491911	35.867904
1312.049487	144238.767844	35.872922
1313.471694	144451.779801	35.877940
1314.604707	144677.471634	35.882957
1315.368220	144919.762786	35.887975
1317.346105	145141.525680	35.892992
1318.035949	145380.598385	35.898010
1318.994066	145612.336216	35.903028
1320.699556	145854.731099	35.908045
1322.149895	146078.350051	35.913063
1323.440416	146308.870508	35.918080
1324.691103	146551.713284	35.923098
1326.278582	146786.271145	35.928116
1328.048785	147003.260758	35.933133
1328.869653	147242.514295	35.938151
1330.586849	147475.609314	35.943168
1332.133627	147694.440994	35.948186
1333.721815	147924.998429	35.953204
1335.537030	148127.427757	35.958221
1336.983614	148341.955168	35.963239
1338.449393	148547.475917	35.968256
1339.746949	148761.941712	35.973274
1340.704715	148943.096508	35.978292
1342.079864	149142.712712	35.983309
1343.173387	149348.921119	35.988327
1344.272735	149542.066156	35.993344
1345.208766	149758.284520	35.998362
1345.968905	149968.889284	36.003380
1346.887064	150196.160217	36.008397
1347.963670	150419.233429	36.013415
1349.067852	150650.839342	36.018432
1350.195639	150896.115594	36.023450
1351.431252	151138.166609	36.028468
1352.834396	151378.479096	36.033485
1354.446749	151618.656944	36.038503
1356.446845	151855.689837	36.043520
1357.334754	152102.903583	36.048538
1358.606128	152347.911742	36.053556
1359.962168	152593.186481	36.058573
1360.664016	152859.424050	36.063591
1362.254611	153109.191440	36.068608
1363.568837	153360.426931	36.073626
1364.369662	153627.490564	36.078644
1365.423794	153903.837147	36.083661
1367.058375	154172.732370	36.088679
1369.387918	154438.825049	36.093696
1370.986301	154689.616123	36.098714
1372.723292	154950.356114	36.103732
1374.257740	155196.328113	36.108749
1375.816662	155467.109485	36.113767
1377.236149	155702.359509	36.118784
1378.553930	155957.645005	36.123802
1380.144933	156216.159637	36.128820
1382.588307	156431.417151	36.133837
1384.485107	156666.086338	36.138855
1385.844599	156904.575545	36.143872
1386.968043	157129.113158	36.148890
1388.115690	157361.690702	36.153908
1389.799174	157595.233649	36.158925
1390.667644	157847.916399	36.163943
1392.003085	158080.644562	36.168960
1393.315614	158341.045874	36.173978
1394.006177	158590.312196	36.178996
1395.012810	158850.374238	36.184013
1395.741615	159105.993110	36.189031
1397.195497	159379.710800	36.194048
1398.400944	159672.424914	36.199066
1399.429458	159944.085606	36.204084
1400.604191	160236.580476	36.209101
1401.756295	160527.343104	36.214119
1402.885876	160818.860024	36.219136
1404.444243	161114.634079	36.224154
1405.739851	161418.509976	36.229172
1407.330786	161708.725992	36.234189
1408.427282	162022.433632	36.239207
1409.843861	162324.862402	36.244224
1411.200406	162627.100300	36.249242
1412.561655	162938.284148	36.254260
1414.070365	163238.509262	36.259277
1415.208150	163558.527093	36.264295
1416.864107	163860.508422	36.269312
1418.494096	164176.820600	36.274330
1421.054945	164456.554097	36.279348
1423.829213	164723.693034	36.284365
1425.422258	165004.275714	36.289383
1427.692143	165277.147845	36.294400
1429.165916	165533.506911	36.299418
1430.623502	165795.871675	36.304436
1431.746627	166051.137300	36.309453
1432.810857	166310.969284	36.314471
1434.663193	166549.698197	36.319488
1435.644270	166795.399269	36.324506
1436.471299	167038.843314	36.329524
1438.068465	167277.834176	36.334541
1439.509026	167534.426106	36.339559
1440.854017	167785.249292	36.344576
1442.419427	168034.057879	36.349594
1443.238686	168298.167486	36.354612
1444.604132	168546.149225	36.359629
1445.156045	168827.778972	36.364647
1447.282371	169079.482253	36.369664
1448.936156	169351.758322	36.374682
1450.010096	169632.722801	36.379700
1451.582097	169905.815166	36.384717
1452.718025	170185.453072	36.389735
1453.745395	170468.625671	36.394752
1454.786623	170767.342444	36.399770
1456.346670	171066.977601	36.404788
1457.429355	171366.173568	36.409805
1458.644094	171675.158796	36.414823
1459.998405	171989.211578	36.419840
1461.236680	172307.130773	36.424858
1462.947997	172616.687055	36.429876
1464.980580	172930.532134	36.434893
1466.103570	173242.791548	36.439911
1467.678638	173566.665849	36.444928
1469.241330	173875.518943	36.449946
1471.008483	174205.317523	36.454964
1472.621589	174506.729684	36.459981
1473.658787	174845.499015	36.464999
1475.138561	175164.869304	36.470016
1477.026336	175483.844078	36.475034
1478.341262	175805.657156	36.480052
1479.615038	176133.393177	36.485069
1480.945041	176460.182914	36.490087
1482.346897	176789.171162	36.495104
1484.059666	177123.173850	36.500122
1485.362329	177470.737675	36.505140
1487.013792	177792.736301	36.510157
1488.731683	178128.699331	36.515175
1490.503899	178465.734377	36.520192
1492.058801	178783.325968	36.525210
1493.197052	179126.448293	36.530228
1495.220004	179442.049927	36.535245
1496.786479	179779.686213	36.540263
1498.312040	180086.832612	36.545280
1500.384674	180427.003762	36.550298
1501.855296	180745.256053	36.555316
1503.544233	181050.680316	36.560333
1504.976183	181375.377818	36.565351
1506.605866	181677.883633	36.570368
1508.730644	181987.734183	36.575386
1510.564849	182295.553148	36.580404
1512.761841	182580.962070	36.585421
1514.333101	182879.600485	36.590439
1516.020242	183168.130621	36.595456
1517.767096	183451.587975	36.600474
1519.106857	183737.970207	36.605492
1520.774566	184018.841615	36.610509
1521.846256	184312.595147	36.615527
1523.278768	184615.200973	36.620544
1524.593499	184909.310894	36.625562
1525.466723	185220.301399	36.630580
1526.703766	185515.531737	36.635597
1528.193303	185822.171186	36.640615
1529.413461	186139.087881	36.645632
1531.028980	186445.887571	36.650650
1531.969343	186771.041523	36.655668
1533.057407	187065.746208	36.660685
1534.559843	187378.649959	36.665703
1535.742425	187690.339079	36.670720
1537.315886	188000.974971	36.675738
1538.616924	188317.001842	36.680756
1540.003099	188635.783615	36.685773
1541.205343	188960.970045	36.690791
1542.389380	189296.570487	36.695808
1544.335186	189625.445576	36.700826
1545.689612	189968.320769	36.705844
1547.239521	190306.379774	36.710861
1548.758765	190654.537844	36.715879
1549.936164	191002.386474	36.720896
1551.650901	191353.778680	36.725914
1552.576784	191710.902046	36.730932
1554.324475	192067.040722	36.735949
1556.017940	192434.920449	36.740967
1558.134395	192787.891961	36.745984
1560.418496	193131.278418	36.751002
1562.691747	193466.010586	36.756020
1565.337529	193782.884313	36.761037
1567.386730	194098.652511	36.766055
1569.349710	194404.991367	36.771072
1570.938526	194725.066524	36.776090
1572.375612	195040.953602	36.781108
1574.042470	195334.384115	36.786125
1575.583004	195654.383067	36.791143
1576.917523	195977.274247	36.796160
1578.465420	196281.304143	36.801178
1579.505293	196614.124478	36.806196
1581.032521	196936.861508	36.811213
1582.126222	197277.458736	36.816231
1583.215548	197613.691080	36.821248
1584.609266	197967.763157	36.826266
1585.376350	198325.216542	36.831284
1587.248970	198678.692441	36.836301
1589.064482	199038.705439	36.841319
1590.130844	199393.550235	36.846336
1592.043149	199752.598735	36.851354
1593.524399	200131.514071	36.856372
1594.645720	200505.793489	36.861389
1596.611417	200871.022047	36.866407
1599.153103	201213.239866	36.871424
1601.407506	201559.252447	36.876442
1603.121075	201912.606130	36.881460
1604.939622	202266.883708	36.886477
1606.565314	202608.244333	36.891495
1607.853453	202952.811327	36.896512
1610.136197	203294.942335	36.901530
1611.842334	203644.890244	36.906548
1613.164500	203986.917070	36.911565
1614.844688	204329.990761	36.916583
1616.171087	204682.444333	36.921600
1617.814256	205022.314965	36.926618
1619.128699	205385.655252	36.931636
1620.546826	205734.365534	36.936653
1622.232232	206087.108933	36.941671
1623.288169	206442.370788	36.946688
1625.059518	206803.902483	36.951706
1626.278515	207177.272591	36.956724
1627.907266	207543.592885	36.961741
1630.015980	207908.781406	36.966759
1631.496789	208285.617861	36.971776
1633.432608	208651.765349	36.976794
1634.800484	209007.799614	36.981812
1636.157877	209389.385222	36.986829
1638.142416	209751.415455	36.991847
1639.446875	210102.779436	36.996864
1641.318987	210448.793823	37.001882
1642.987449	210803.198710	37.006900
1644.421939	211155.586768	37.011917
1646.312846	211496.853220	37.016935
1647.479174	211851.015534	37.021952
1648.989201	212206.620716	37.026970
1650.144500	212578.895542	37.031988
1651.710225	212944.602342	37.037005
1653.228313	213314.229659	37.042023
1654.603111	213689.825138	37.047040
1656.522145	214067.541513	37.052058
1658.004776	214450.258841	37.057076
1659.497315	214838.487329	37.062093
1661.770954	215203.984308	37.067111
1663.934005	215591.469863	37.072128
1665.937128	215951.096982	37.077146
1667.532617	216330.984178	37.082164
1669.478430	216711.881517	37.087181
1671.437115	217069.056612	37.092199
1673.118052	217439.638380	37.097216
1674.794400	217811.898575	37.102234
1676.165385	218191.754030	37.107252
1677.980903	218562.190686	37.112269
1679.832492	218940.597798	37.117287
1680.707879	219321.149196	37.122304
1682.629421	219761.570736	37.127322
1684.529434	220143.682419	37.132340
1686.082447	220525.827604	37.137357
1687.985826	220912.640269	37.142375
1689.845308	221300.756946	37.147392
1691.348544	221677.529907	37.152410
1693.091093	222073.440807	37.157428
1695.270901	222462.473666	37.162445
1697.652205	222836.234922	37.167463
1698.853101	223210.269258	37.172480
1700.624367	223585.886642	37.177498
1702.425993	223967.723094	37.182516
1703.720780	224366.510131	37.187533
1705.339087	224749.319291	37.192551
1706.663248	225144.471913	37.197568
1707.756069	225530.088426	37.202586
1709.734145	225941.111753	37.207604
1711.188841	226348.184589	37.212621
1713.230059	226758.336545	37.217639
1714.713291	227176.227759	37.222656
1716.777882	227546.703304	37.227674
1719.993200	227931.086360	37.232692
1721.903581	228321.859115	37.237709
1723.676346	228700.717601	37.242727
1725.278832	229080.875397	37.247744
1727.450379	229465.842251	37.252762
1729.532890	229841.528282	37.257780
1731.101878	230204.142841	37.262797
1733.425801	230561.959456	37.267815
1735.308852	230927.343285	37.272832
1737.191564	231281.094458	37.277850
1738.374404	231657.696360	37.282868
1740.323175	232014.486447	37.287885
1741.600324	232370.245632	37.292903
1743.430140	232757.944926	37.297920
1744.886907	233109.586448	37.302938
1746.913114	233479.880530	37.307956
1748.673769	233834.978666	37.312973
1750.445251	234206.078667	37.317991
1752.091146	234569.071846	37.323008
1753.624935	234928.782193	37.328026
1755.633920	235306.576667	37.333044
1756.923661	235670.342460	37.338061
1758.287938	236015.223208	37.343079
1759.807907	236381.136849	37.348096
1761.343611	236733.814294	37.353114
1762.516330	237109.592026	37.358132
1763.769173	237477.685864	37.363149
1765.561530	237850.872994	37.368167
1766.842848	238245.406985	37.373184
1768.410270	238636.439673	37.378202
1770.051042	239024.996962	37.383220
1771.294539	239438.692718	37.388237
1773.716891	239832.532642	37.393255
1775.806915	240230.848351	37.398272
1778.288155	240632.249833	37.403290
1779.919569	241038.543104	37.408308
1781.712131	241440.110954	37.413325
1783.613028	241834.421858	37.418343
1785.497449	242241.767592	37.423360
1787.202793	242633.902191	37.428378
1788.981006	243032.553774	37.433396
1790.328148	243437.272415	37.438413
1792.505734	243858.721377	37.443431
1794.082224	244265.283053	37.448448
1795.807940	244683.632832	37.453466
1797.310166	245108.802779	37.458484
1798.295123	245538.733161	37.463501
1800.373691	245978.212181	37.468519
1801.754534	246430.686664	37.473536
1803.177539	246871.520279	37.478554
1805.223815	247324.596979	37.483572
1806.472801	247787.815133	37.488589
1808.705516	248250.515208	37.493607
1810.374564	248716.230592	37.498624
1811.878628	249194.751568	37.503642
1813.807093	249666.166116	37.508660
1815.739856	250155.210179	37.513677
1817.339038	250622.031524	37.518695
1818.860859	251117.063581	37.523712
1820.669739	251601.887281	37.528730
1822.637374	252092.400802	37.533748
1824.545656	252585.922133	37.538765
1826.580368	253071.192255	37.543783
1828.728991	253563.988589	37.548800
1830.429853	254049.924357	37.553818
1833.246931	254505.394779	37.558836
1836.039439	254966.102565	37.563853
1839.377883	255401.977317	37.568871
1841.734653	255853.739524	37.573888
1843.475604	256285.052677	37.578906
1845.602499	256720.722167	37.583924
1847.415642	257143.107022	37.588941
1849.423045	257566.856945	37.593959
1851.103297	257997.189782	37.598976
1852.751501	258425.165463	37.603994
1854.975284	258844.230847	37.609012
1857.230012	259246.321703	37.614029
1859.706752	259651.068507	37.619047
1862.029308	260043.723459	37.624064
1864.330811	260431.910878	37.629082
1866.453353	260805.165359	37.634100
1868.885668	261183.423699	37.639117
1870.729390	261558.985127	37.644135
1872.340543	261937.099923	37.649152
1874.304989	262293.537898	37.654170
1875.988883	262660.590007	37.659188
1877.731584	263034.059268	37.664205
1879.497340	263407.422954	37.669223
1881.173731	263768.429924	37.674240
1882.737508	264139.642085	37.679258
1884.262748	264493.764103	37.684276
1885.598757	264859.450348	37.689293
1887.310540	265219.561646	37.694311
1888.604679	265590.741511	37.699328
1890.315640	265968.837949	37.704346
1892.412113	266339.706581	37.709364
1893.681330	266730.729680	37.714381
1894.805930	267116.009945	37.719399
1896.757483	267525.107982	37.724416
1898.218265	267938.910335	37.729434
1899.743806	268353.489072	37.734452
1901.331415	268792.266177	37.739469
1902.898780	269211.689111	37.744487
1904.153018	269651.638247	37.749504
1905.715370	270111.375491	37.754522
1907.632247	270560.739848	37.759540
1909.157088	271041.033029	37.764557
1910.765878	271522.607158	37.769575
1912.444049	272001.781213	37.774592
1913.984008	272492.002211	37.779610
1915.932543	272993.357294	37.784628
1917.175289	273512.254652	37.789645
1918.815957	274035.606775	37.794663
1920.903965	274565.183593	37.799680
1922.365519	275101.289953	37.804698
1924.663483	275619.957543	37.809716
1926.108792	276154.463965	37.814733
1929.638067	276668.124239	37.819751
1932.700914	277164.510903	37.824768
1934.991734	277682.006589	37.829786
1937.818424	278192.248858	37.834804
1939.533326	278695.104277	37.839821
1941.131662	279202.702556	37.844839
1943.248658	279707.622624	37.849856
1944.719624	280222.174130	37.854874
1946.767352	280737.060527	37.859892
1948.184318	281260.076957	37.864909
1950.339452	281771.919867	37.869927
1952.457685	282300.634079	37.874944
1954.278095	282824.137917	37.879962
1956.417435	283354.801317	37.884980
1958.216639	283878.051384	37.889997
1960.763820	284406.408517	37.895015
1962.578551	284940.219501	37.900032
1964.323020	285456.081731	37.905050
1966.453728	285982.749873	37.910068
1968.364693	286505.769447	37.915085
1970.494044	287038.657314	37.920103
1972.812851	287566.685697	37.925120
1974.317839	288092.840294	37.930138
1976.430623	288624.150132	37.935156
1978.706957	289156.497638	37.940173
1981.253255	289671.348282	37.945191
1983.394123	290185.883089	37.950208
1985.479810	290709.518260	37.955226
1987.155261	291231.898454	37.960244
1989.122828	291750.037104	37.965261
1991.078942	292272.290263	37.970279
1993.267983	292784.063319	37.975296
1995.146573	293304.546898	37.980314
1997.486216	293817.839955	37.985332
1999.293232	294342.978909	37.990349
2001.695882	294853.717006	37.995367
2004.024545	295354.508592	38.000384
2006.221660	295865.860333	38.005402
2008.890742	296349.497488	38.010420
2010.836700	296833.531674	38.015437
2013.175198	297315.542956	38.020455
2015.465614	297782.041478	38.025472
2016.808211	298256.466873	38.030490
2019.154184	298713.605388	38.035508
2020.897516	299160.098235	38.040525
2022.893745	299611.449063	38.045543
2024.747616	300071.913932	38.050560
2027.069789	300525.670233	38.055578
2029.580612	300970.961119	38.060596
2031.788991	301423.995554	38.065613
2034.045069	301867.318086	38.070631
2036.688959	302306.205949	38.075648
2037.905817	302753.252112	38.080666
2040.503158	303187.495842	38.085684
2042.231627	303654.618272	38.090701
2044.095383	304096.064994	38.095719
2046.106451	304542.894678	38.100736
2047.473364	305016.088998	38.105754
2048.930174	305480.275522	38.110772
2050.397419	305964.597206	38.115789
2052.383009	306456.982522	38.120807
2054.026228	306951.707375	38.125824
2055.603136	307470.439510	38.130842
2057.286996	307980.389176	38.135860
2058.808130	308513.980613	38.140877
2060.654385	309041.242053	38.145895
2062.899676	309572.192485	38.150912
2064.689367	310123.048481	38.155930
2066.828822	310661.957894	38.160948
2068.849409	311211.092014	38.165965
2070.863814	311762.788146	38.170983
2073.630733	312320.577320	38.176000
2075.327466	312882.094878	38.181018
2077.463057	313442.951509	38.186036
2079.174735	314015.834653	38.191053
2081.151525	314589.075749	38.196071
2083.154938	315154.486769	38.201088
2084.960963	315739.834381	38.206106
2087.220644	316324.975112	38.211124
2089.656660	316910.742030	38.216141
2091.672241	317503.048823	38.221159
2093.870981	318078.205765	38.226176
2096.024916	318676.243685	38.231194
2097.878304	319245.861759	38.236212
2100.516821	319839.010097	38.241229
2102.638479	320437.748746	38.246247
2104.968604	321025.833901	38.251264
2107.066344	321624.362613	38.256282
2109.284829	322206.945771	38.261300
2111.756908	322788.389864	38.266317
2113.598049	323373.030788	38.271335
2116.077305	323959.439488	38.276352
2118.022036	324551.517010	38.281370
2120.418121	325133.662952	38.286388
2122.434848	325715.917001	38.291405
2124.783057	326307.352248	38.296423
2127.407747	326891.474693	38.301440
2129.186945	327463.113318	38.306458
2131.524756	328046.332603	38.311476
2133.860534	328620.559046	38.316493
2136.393184	329202.008190	38.321511
2138.482969	329758.594165	38.326528
2140.412953	330345.336090	38.331546
2142.748654	330916.924819	38.336564
2144.644952	331491.626981	38.341581
2146.899449	332059.206452	38.346599
2149.296061	332612.616390	38.351616
2151.048659	333192.554411	38.356634
2153.005712	333762.069629	38.361652
2155.164383	334313.978668	38.366669
2157.515989	334854.274405	38.371687
2159.914813	335392.678386	38.376704
2161.879814	335951.152020	38.381722
2163.653595	336488.810706	38.386740
2165.735448	337035.475065	38.391757
2167.496057	337578.734672	38.396775
2170.134789	338136.159596	38.401792
2172.057324	338700.576015	38.406810
2174.304299	339260.160425	38.411828
2176.307173	339814.397909	38.416845
2178.040867	340392.482789	38.421863
2180.305030	340974.001283	38.426880
2181.759054	341558.946799	38.431898
2183.771790	342137.168218	38.436916
2185.877492	342739.835112	38.441933
2187.455413	343346.896729	38.446951
2189.395836	343967.672443	38.451968
2191.879759	344577.893362	38.456986
2194.752056	345190.427867	38.462004
2196.884415	345790.234786	38.467021
2199.110038	346414.941230	38.472039
2201.807680	347028.165897	38.477056
2204.677736	347629.197436	38.482074
2207.581309	348230.190179	38.487092
2209.962898	348833.900769	38.492109
2211.823316	349427.284728	38.497127
2214.027865	350037.911299	38.502144
2216.108447	350644.794249	38.507162
2218.154939	351257.358944	38.512180
2220.235354	351879.679429	38.517197
2221.831422	352502.934069	38.522215
2224.143928	353115.580994	38.527232
2226.011923	353766.127423	38.532250
2228.156015	354393.527108	38.537268
2230.599613	355041.675091	38.542285
2232.559227	355676.901742	38.547303
2234.715442	356316.552033	38.552320
2237.292977	356962.110888	38.557338
2239.889978	357607.859469	38.562356
2242.981743	358241.184940	38.567373
2245.428688	358874.582030	38.572391
2248.325308	359492.443382	38.577408
2250.359785	360123.402858	38.582426
2252.559993	360743.669172	38.587444
2254.815663	361363.510750	38.592461
2256.454862	362012.975674	38.597479
2259.099152	362644.149454	38.602496
2261.295240	363282.820532	38.607514
2263.092906	363921.318806	38.612532
2265.495930	364561.659706	38.617549
2267.505791	365220.802108	38.622567
2269.671704	365868.973856	38.627584
2271.903759	366522.374634	38.632602
2273.775371	367169.583575	38.637620
2275.796604	367831.063235	38.642637
2277.829354	368495.395630	38.647655
2280.381859	369159.224234	38.652672
2282.760833	369819.087328	38.657690
2285.339934	370492.069617	38.662708
2288.120645	371132.920544	38.667725
2290.691276	371791.448019	38.672743
2293.782909	372435.039742	38.677760
2296.064870	373072.920545	38.682778
2298.462643	373718.759869	38.687796
2300.677750	374361.041656	38.692813
2302.787539	375005.966755	38.697831
2304.748027	375625.493107	38.702848
2306.891083	376256.517218	38.707866
2308.827352	376877.318655	38.712884
2310.844172	377486.861314	38.717901
2313.027945	378119.949428	38.722919
2316.031519	378712.062719	38.727936
2318.101678	379329.906610	38.732954
2320.575033	379961.517736	38.737972
2323.907596	380560.162499	38.742989
2326.594040	381162.174537	38.748007
2329.296372	381755.932249	38.753024
2331.849435	382364.993600	38.758042
2333.565151	382972.661003	38.763060
2335.847226	383576.191942	38.768077
2337.746571	384196.585067	38.773095
2340.064534	384813.017873	38.778112
2341.853362	385451.761492	38.783130
2343.422991	386094.889411	38.788148
2345.687271	386735.328791	38.793165
2347.215464	387407.567015	38.798183
2349.701731	388059.655471	38.803200
2352.297732	388717.035924	38.808218
2354.672819	389390.612635	38.813236
2356.998450	390062.484537	38.818253
2358.898278	390746.808119	38.823271
2361.565170	391441.331748	38.828288
2364.050354	392113.386022	38.833306
2365.968220	392800.575819	38.838324
2368.444350	393489.381223	38.843341
2370.228280	394204.949826	38.848359
2372.794709	394900.145969	38.853376
2375.174881	395606.305859	38.858394
2377.173171	396339.858901	38.863412
2379.800136	397049.643842	38.868429
2382.018639	397773.874241	38.873447
2384.278083	398510.827266	38.878464
2386.629716	399240.599932	38.883482
2388.722645	399983.827929	38.888500
2391.312512	400718.110581	38.893517
2393.443827	401482.680945	38.898535
2396.235804	402228.344982	38.903552
2398.715318	402979.995707	38.908570
2400.836936	403744.506648	38.913588
2403.482469	404500.041965	38.918605
2405.877852	405261.780351	38.923623
2407.691236	406023.518163	38.928640
2410.318250	406808.940660	38.933658
2412.855957	407560.787314	38.938676
2415.160750	408339.378940	38.943693
2417.872934	409112.535542	38.948711
2420.155864	409889.819580	38.953728
2422.598337	410663.634973	38.958746
2424.662127	411458.540572	38.963764
2427.433845	412230.001575	38.968781
2430.280674	413015.130817	38.973799
2433.152540	413785.035360	38.978816
2435.668305	414558.598099	38.983834
2438.581384	415334.250238	38.988852
2441.633522	416086.961158	38.993869
2443.844104	416851.464524	38.998887
2446.396399	417616.521688	39.003904
2448.783566	418369.047866	39.008922
2451.008981	419130.897537	39.013940
2453.970954	419876.598492	39.018957
2456.595524	420631.980831	39.023975
2459.250541	421383.562534	39.028992
2461.640831	422119.188314	39.034010
2464.060502	422875.726705	39.039028
2466.434468	423612.222369	39.044045
2468.655255	424341.632305	39.049063
2470.429209	425069.980532	39.054080
2473.198222	425781.534666	39.059098
2475.714234	426515.488972	39.064116
2478.109655	427230.707857	39.069133
2480.558091	427961.338410	39.074151
2482.447802	428680.445602	39.079168
2485.025285	429407.669230	39.084186
2487.427573	430162.033975	39.089204
2490.159784	430890.603967	39.094221
2491.976251	431639.450017	39.099239
2494.040624	432405.947773	39.104256
2496.361556	433175.465554	39.109274
2498.227986	433953.485895	39.114292
2500.509217	434736.725877	39.119309
2502.791209	435538.918652	39.124327
2505.018683	436345.950974	39.129344
2507.649455	437152.078265	39.134362
2509.466460	437970.254827	39.139380
2512.479565	438794.731838	39.144397
2514.752859	439620.211942	39.149415
2517.315359	440439.238011	39.154432
2520.246339	441267.179674	39.159450
2523.122387	442106.028567	39.164468
2525.788705	442932.889192	39.169485
2528.783264	443765.330867	39.174503
2532.181557	444577.993906	39.179520
2534.890987	445398.733821	39.184538
2537.112647	446231.512722	39.189556
2539.683958	447049.329392	39.194573
2542.779333	447879.117771	39.199591
2545.289548	448704.873679	39.204608
2547.866781	449528.512709	39.209626
2550.029380	450362.607457	39.214644
2552.750894	451191.873187	39.219661
2555.544508	452016.997776	39.224679
2558.213383	452847.774549	39.229696
2561.069923	453674.744961	39.234714
2563.331963	454508.000668	39.239732
2565.874222	455338.445833	39.244749
2568.322083	456181.665759	39.249767
2571.100716	457024.088361	39.254784
2573.674831	457849.269143	39.259802
2576.135023	458695.618901	39.264820
2579.250192	459522.007062	39.269837
2582.063585	460359.330786	39.274855
2584.560008	461198.491839	39.279872
2587.526830	462016.662932	39.284890
2590.200865	462847.081214	39.289908
2592.895059	463673.720990	39.294925
2596.089332	464504.640575	39.299943
2598.554634	465327.154777	39.304960
2601.762835	466136.118688	39.309978
2603.919725	466968.217099	39.314996
2606.149443	467781.570046	39.320013
2608.623959	468615.566455	39.325031
2610.757876	469462.518756	39.330048
2612.878325	470287.961549	39.335066
2615.213097	471141.576968	39.340084
2617.835129	471985.254471	39.345101
2620.742465	472822.380456	39.350119
2623.514041	473665.048796	39.355136
2625.833897	474508.158198	39.360154
2628.633880	475367.314683	39.365172
2631.058506	476221.189900	39.370189
2633.594762	477081.674596	39.375207
2635.698951	477941.079553	39.380224
2638.025520	478790.458124	39.385242
2640.523705	479634.264158	39.390260
2643.202681	480468.153732	39.395277
2646.112522	481287.776948	39.400295
2648.896906	482129.652391	39.405312
2652.175387	482948.179897	39.410330
2654.953774	483766.651894	39.415348
2658.526730	484565.617829	39.420365
2661.567566	485379.630498	39.425383
2664.270274	486174.881745	39.430400
2668.462394	486956.069265	39.435418
2671.263134	487732.757816	39.440436
2673.346322	488520.080586	39.445453
2676.108128	489315.785999	39.450471
2678.776660	490106.625195	39.455488
2681.458385	490885.969449	39.460506
2683.814946	491682.491698	39.465524
2686.665684	492467.893888	39.470541
2689.538192	493265.065141	39.475559
2691.463929	494073.911648	39.480576
2694.243157	494865.473118	39.485594
2696.300463	495699.702550	39.490612
2698.474633	496525.546759	39.495629
2700.992939	497354.371260	39.500647
2703.464158	498207.681004	39.505664
2706.071459	499051.188726	39.510682
2708.185815	499913.702375	39.515700
2710.703471	500778.273651	39.520717
2713.456532	501653.151317	39.525735
2715.606545	502547.449866	39.530752
2718.075564	503433.174376	39.535770
2720.897836	504340.679434	39.540788
2723.657820	505236.798275	39.545805
2726.424073	506140.178398	39.550823
2728.926531	507066.846818	39.555840
2731.581390	507998.680511	39.560858
2734.297207	508915.123757	39.565876
2736.410925	509858.333265	39.570893
2739.379886	510800.438260	39.575911
2741.952463	511744.771025	39.580928
2744.678574	512688.366932	39.585946
2747.415458	513663.808592	39.590964
2750.045010	514614.663786	39.595981
2752.800021	515587.261545	39.600999
2755.483021	516554.116399	39.606016
2758.640947	517510.402161	39.611034
2761.471679	518491.271147	39.616052
2764.778094	519461.267702	39.621069
2767.879801	520422.118325	39.626087
2770.780941	521387.929078	39.631104
2774.070006	522334.372141	39.636122
2777.734637	523278.427511	39.641140
2781.348805	524222.986408	39.646157
2784.202525	525158.596944	39.651175
2786.892930	526104.046883	39.656192
2789.648578	527039.304600	39.661210
2791.795792	527973.698008	39.666228
2794.462091	528911.874202	39.671245
2797.088467	529849.091352	39.676263
2799.418615	530799.941329	39.681280
2802.282501	531743.593814	39.686298
2805.448061	532686.934291	39.691316
2808.329174	533641.284152	39.696333
2811.255402	534582.276522	39.701351
2814.065632	535527.454566	39.706368
2817.317201	536477.429586	39.711386
2819.951336	537421.254538	39.716404
2822.470860	538365.036362	39.721421
2825.229692	539295.332580	39.726439
2827.654714	540223.409568	39.731456
2829.888174	541136.012967	39.736474
2832.303564	542055.016758	39.741492
2835.203368	542986.657145	39.746509
2837.663229	543902.414277	39.751527
2840.650909	544845.736769	39.756544
2843.345533	545782.556368	39.761562
2845.817837	546732.022268	39.766580
2848.448295	547694.470990	39.771597
2851.067173	548649.764930	39.776615
2853.577437	549632.663235	39.781632
2856.092445	550611.367866	39.786650
2859.062061	551608.627787	39.791668
2860.786429	552597.827217	39.796685
2863.266761	553612.614401	39.801703
2866.123850	554646.813895	39.806720
2869.288382	555693.698209	39.811738
2872.052397	556730.768137	39.816756
2874.786799	557789.469378	39.821773
2878.153894	558826.578203	39.826791
2880.559869	559897.525818	39.831808
2883.146659	560953.336487	39.836826
2886.174562	562039.530154	39.841844
2888.934888	563123.267317	39.846861
2891.976927	564195.869289	39.851879
2894.984275	565281.445557	39.856896
2898.200640	566370.461693	39.861914
2901.570248	567455.243540	39.866932
2904.605927	568547.821414	39.871949
2907.730028	569629.046494	39.876967
2910.686965	570722.857568	39.881984
2913.859934	571816.639404	39.887002
2917.464899	572900.017033	39.892020
2920.051343	573982.316083	39.897037
2923.308964	575074.597757	39.902055
2926.613692	576154.784604	39.907072
2929.791938	577225.767893	39.912090
2932.888471	578323.110778	39.917108
2935.897888	579405.071511	39.922125
2938.951312	580480.108850	39.927143
2941.711915	581571.350795	39.932160
2944.722015	582649.516015	39.937178
2947.781323	583730.386295	39.942196
2950.556041	584828.907532	39.947213
2953.391523	585909.370769	39.952231
2956.021060	587011.980010	39.957248
2958.959046	588094.888024	39.962266
2962.489284	589193.840290	39.967284
2965.679653	590284.929629	39.972301
2968.753332	591368.622068	39.977319
2971.498651	592467.653539	39.982336
2974.004314	593553.946509	39.987354
2977.442320	594654.814913	39.992372
2980.939037	595742.896749	39.997389
2984.142967	596850.611555	40.002407
2987.155595	597928.903090	40.007424
2989.707973	599033.263081	40.012442
2992.764697	600121.961241	40.017460
2995.907474	601201.179476	40.022477
2999.540657	602288.676930	40.027495
3002.936303	603366.048388	40.032512
3006.263819	604438.624465	40.037530
3009.875056	605494.936000	40.042548
3012.219404	606556.513983	40.047565
3015.357348	607629.821768	40.052583
3018.330643	608695.198915	40.057600
3021.054062	609769.873023	40.062618
3023.855239	610811.312359	40.067636
3026.715993	611852.094764	40.072653
3030.051669	612870.092707	40.077671
3033.129732	613878.287184	40.082688
3036.025251	614890.871213	40.087706
3039.157631	615903.423419	40.092724
3042.007390	616942.080175	40.097741
3044.910683	617953.081781	40.102759
3047.747404	618979.898668	40.107776
3050.601725	620016.963568	40.112794
3053.730326	621047.286705	40.117812
3056.064628	622102.982217	40.122829
3059.372201	623155.115671	40.127847
3062.109599	624225.529138	40.132864
3064.529534	625299.336081	40.137882
3067.675556	626374.664008	40.142900
3070.206341	627467.718799	40.147917
3073.062692	628571.096690	40.152935
3075.894320	629690.295718	40.157952
3078.418082	630808.528516	40.162970
3081.189619	631940.283202	40.167988
3084.268059	633082.949052	40.173005
3087.159075	634229.365288	40.178023
3090.279863	635392.938404	40.183040
3092.859232	636567.551023	40.188058
3095.988471	637747.578987	40.193076
3098.898742	638938.087005	40.198093
3101.592560	640143.361313	40.203111
3104.431285	641346.424967	40.208128
3107.397858	642562.594411	40.213146
3110.477661	643796.505197	40.218164
3113.488272	645032.821020	40.223181
3116.547984	646274.363058	40.228199
3119.749196	647531.234357	40.233216
3122.798222	648798.940832	40.238234
3126.392050	650047.805321	40.243252
3129.344222	651319.545006	40.248269
3132.737321	652569.522409	40.253287
3136.515447	653838.012783	40.258304
3139.383639	655103.153053	40.263322
3142.418886	656360.830762	40.268340
3145.849075	657639.050984	40.273357
3149.018409	658918.591540	40.278375
3152.734678	660206.388265	40.283392
3155.229386	661486.001641	40.288410
3158.445756	662766.222664	40.293428
3161.756256	664057.656185	40.298445
3164.648263	665346.546940	40.303463
3167.900997	666633.562662	40.308480
3171.477737	667927.465948	40.313498
3175.086559	669219.496640	40.318516
3178.271135	670501.921319	40.323533
3182.324991	671776.419249	40.328551
3186.060898	673029.116958	40.333568
3189.380609	674298.769841	40.338586
3193.062117	675561.628611	40.343604
3196.091519	676820.099775	40.348621
3199.454780	678080.830262	40.353639
3202.847029	679324.886656	40.358656
3206.457701	680565.609123	40.363674
3209.313957	681813.343354	40.368692
3212.656745	683060.976441	40.373709
3215.329499	684313.218532	40.378727
3218.826178	685553.135090	40.383744
3221.627876	686806.849981	40.388762
3225.202304	688040.455403	40.393780
3228.272657	689292.639266	40.398797
3231.305249	690531.354044	40.403815
3234.415885	691767.552482	40.408832
3237.907359	692970.521615	40.413850
3241.022637	694161.285551	40.418868
3244.664285	695357.358489	40.423885
3247.921559	696547.431351	40.428903
3251.578154	697718.383785	40.433920
3255.007747	698894.325118	40.438938
3258.235123	700076.983981	40.443956
3261.238561	701260.759284	40.448973
3264.304082	702442.182900	40.453991
3267.635371	703626.276434	40.459008
3270.564555	704828.856117	40.464026
3274.406936	706014.074668	40.469044
3277.848681	707206.626955	40.474061
3281.020651	708404.258973	40.479079
3285.709773	709568.639189	40.484096
3289.435390	710743.962998	40.489114
3293.252345	711918.317389	40.494132
3296.190228	713088.298500	40.499149
3299.527616	714261.615650	40.504167
3302.520777	715430.917078	40.509184
3305.679637	716611.310610	40.514202
3308.766064	717789.472235	40.519220
3311.745096	718988.311760	40.524237
3314.359318	720199.800258	40.529255
3317.680826	721408.621771	40.534272
3320.487308	722638.515245	40.539290
3323.120134	723858.663517	40.544308
3326.180732	725117.561907	40.549325
3329.002363	726379.074824	40.554343
3331.826545	727652.747222	40.559360
3334.831510	728936.962269	40.564378
3338.376090	730228.987392	40.569396
3341.881540	731520.813472	40.574413
3345.162765	732821.507891	40.579431
3348.797976	734114.774643	40.584448
3351.858488	735437.006590	40.589466
3355.069949	736763.684906	40.594484
3358.215046	738091.585324	40.599501
3361.039429	739436.193135	40.604519
3364.105656	740777.869384	40.609536
3366.774192	742155.836696	40.614554
3369.774573	743534.445765	40.619572
3373.327382	744920.167790	40.624589
3376.849467	746305.945904	40.629607
3380.364489	747698.676201	40.634624
3383.713918	749114.249436	40.639642
3386.750853	750516.460198	40.644660
3390.379662	751918.614799	40.649677
3394.518777	753309.446154	40.654695
3398.185428	754704.339343	40.659712
3401.835474	756109.272294	40.664730
3405.788981	757502.918688	40.669748
3409.412613	758892.279328	40.674765
3412.956093	760288.140929	40.679783
3416.486487	761671.791141	40.684800
3419.973703	763082.644472	40.689818
3423.366851	764468.066557	40.694836
3426.733382	765850.384873	40.699853
3429.623488	767244.522666	40.704871
3432.878107	768652.938784	40.709888
3435.758653	770064.393304	40.714906
3439.174699	771480.502242	40.719924
3442.218373	772897.383487	40.724941
3445.286803	774322.730810	40.729959
3448.564641	775755.476533	40.734976
3451.414692	777201.367052	40.739994
3454.664166	778667.914842	40.745012
3457.539696	780106.608977	40.750016
3460.524437	781511.867942	40.755021
3463.660452	782859.231183	40.760026
3466.643714	784172.730013	40.765031
3470.023921	785410.891365	40.770036
3473.197805	786584.177107	40.775040
3475.965643	787705.923021	40.780045
3479.071186	788748.508481	40.785050
3481.593041	789741.259641	40.790055
3484.145603	790652.994724	40.795060
3486.308633	791506.019525	40.800064
3488.729609	792301.574403	40.805069
3491.142376	793024.840447	40.810074
3493.263700	793696.955443	40.815079
3495.394178	794306.982529	40.820084
3497.545613	794852.038774	40.825088
3499.123466	795352.663076	40.830093
3500.886927	795787.677017	40.835098
3502.822016	796177.616442	40.840103
3504.705504	796516.291132	40.845108
3506.414022	796793.616457	40.850112
3507.812113	797027.931975	40.855117
3509.736931	797229.706398	40.860122
3510.669840	797383.142552	40.865127
3511.900293	797492.497275	40.870132
3512.877955	797570.969076	40.875136
3513.257670	797615.720090	40.880141
3514.738964	797624.899448	40.885146
3515.528929	797617.897211	40.890151
3516.427907	797568.370161	40.895156
3516.635037	797499.519575	40.900160
3517.121887	797421.099557	40.905165
3517.921745	797307.137815	40.910170
3518.381294	797185.278376	40.915175
3518.641622	797029.628181	40.920180
3519.252093	796873.180318	40.925184
3519.480889	796695.830476	40.930189
3520.157294	796504.067403	40.935194
3519.987213	796297.956487	40.940199
3520.415705	796076.373951	40.945204
3520.439265	795846.946806	40.950208
3520.653894	795611.146925	40.955213
3521.104942	795353.106969	40.960218
3521.537237	795106.844974	40.965223
3521.857608	794835.108199	40.970228
3521.941758	794551.712851	40.975232
3521.953213	794275.389521	40.980237
3521.865757	793970.833772	40.985242
3521.797551	793691.259383	40.990247
3522.068059	793389.713301	40.995252
3521.589531	793089.260374	41.000256
3521.576966	792778.550236	41.005261
3522.185334	792476.221522	41.010266
3521.855358	792164.014003	41.015271
3521.656755	791853.686787	41.020276
3521.828590	791531.052219	41.025280
3521.955437	791220.152096	41.030285
3522.030786	790888.120523	41.035290
3521.860160	790580.090989	41.040295
3521.963435	790243.258611	41.045300
3522.173293	789910.962404	41.050304
3521.559223	789586.256046	41.055309
3522.175956	789250.372692	41.060314
3521.812011	788918.861936	41.065319
3521.840685	788588.401195	41.070324
3521.885332	788244.504704	41.075328
3521.681644	787909.922272	41.080333
3522.054670	787565.250556	41.085338
3521.815017	787227.102884	41.090343
3521.690393	786887.543712	41.095348
3521.580452	786541.722496	41.100352
3521.386035	786200.274023	41.105357
3521.562672	785859.927885	41.110362
3521.297525	785530.406343	41.115367
3521.167300	785192.488375	41.120372
3521.067114	784849.828915	41.125376
3520.845544	784510.713722	41.130381
3521.333997	784182.284155	41.135386
3520.686835	783837.945508	41.140391
3520.627699	783501.263912	41.145396
3520.654831	783167.601704	41.150400
3520.415031	782833.279512	41.155405
3520.565037	782498.385483	41.160410
3520.456802	782167.601411	41.165415
3520.280651	781831.106955	41.170420
3520.020319	781501.153721	41.175424
3519.815744	781175.112009	41.180429
3520.108744	780840.461747	41.185434
3519.743757	780519.041739	41.190439
3519.621039	780197.813431	41.195444
3519.726414	779861.721967	41.200448
3519.379993	779549.359061	41.205453
3519.300657	779216.220710	41.210458
3519.405442	778901.245555	41.215463
3518.987942	778577.533485	41.220468
3518.837980	778263.015682	41.225472
3518.522467	777957.321946	41.230477
3518.752160	777636.069638	41.235482
3518.962492	777332.083949	41.240487
3518.398874	777013.199556	41.245492
3518.539831	776702.455104	41.250496
3518.143210	776407.786050	41.255501
3518.123843	776095.663811	41.260506
3517.795815	775804.700727	41.265511
3517.673554	775503.992533	41.270516
3517.576677	775199.722631	41.275520
3517.695286	774903.923034	41.280525
3517.630463	774604.251670	41.285530
3517.129644	774313.848771	41.290535
3517.334943	774019.771959	41.295540
3517.262019	773729.767690	41.300544
3517.171043	773439.065451	41.305549
3517.296948	773149.497921	41.310554
3517.157833	772857.697104	41.315559
3516.656180	772567.914860	41.320564
3516.855574	772285.394028	41.325568
3516.456964	772006.803439	41.330573
3516.708616	771718.488865	41.335578
3516.072107	771448.438737	41.340583
3515.787252	771177.532369	41.345588
3515.987290	770895.992794	41.350592
3516.136949	770632.729571	41.355597
3516.213382	770340.497937	41.360602
3515.954792	770082.308208	41.365607
3515.549413	769809.745655	41.370612
3515.363075	769537.974569	41.375616
3515.111303	769278.918018	41.380621
3515.154762	769015.122074	41.385626
3514.939170	768756.041289	41.390631
3515.102114	768498.416684	41.395636
3515.095558	768239.628328	41.400640
3514.741269	767996.315062	41.405645
3514.781331	767742.233181	41.410650
3514.545277	767480.893382	41.415655
3514.631207	767224.173890	41.420660
3514.434085	766974.294781	41.425664
3514.044947	766740.410503	41.430669
3514.224340	766484.931779	41.435674
3513.993528	766242.723955	41.440679
3513.976680	766005.402866	41.445684
3514.043618	765754.305393	41.450688
3513.761008	765517.850865	41.455693
3513.791610	765276.801111	41.460698
3513.528366	765048.513057	41.465703
3513.314000	764810.742962	41.470708
3513.490349	764585.967605	41.475712
3513.232336	764360.517637	41.480717
3513.051451	764118.331431	41.485722
3512.944184	763905.170833	41.490727
3512.512442	763685.301688	41.495732
3512.945069	763457.392674	41.500736
3512.601144	763233.945040	41.505741
3512.643690	763025.025360	41.510746
3512.667135	762801.997378	41.515751
3512.383118	762579.753428	41.520756
3512.442572	762365.436554	41.525760
3512.032912	762166.580427	41.530765
3512.693157	761939.820990	41.535770
3512.470786	761730.169293	41.540775
3511.947070	761513.014240	41.545780
3511.867349	761304.757692	41.550784
3511.805368	761100.932321	41.555789
3511.854076	760900.289805	41.560794
3511.484238	760701.437832	41.565799
3511.437112	760487.825289	41.570804
3511.476608	760294.617914	41.575808
3511.622586	760100.203896	41.580813
3511.810574	759902.472206	41.585818
3511.598370	759687.532208	41.590823
3511.119168	759496.215804	41.595828
3511.311351	759295.062977	41.600832
3510.936403	759101.350900	41.605837
3511.010195	758913.579926	41.610842
3510.768333	758723.685201	41.615847
3510.699122	758537.014189	41.620852
3510.653894	758358.033158	41.625856
3510.631132	758167.841593	41.630861
3510.621281	757982.874448	41.635866
3510.791781	757798.267832	41.640871
3510.616188	757623.091251	41.645876
3510.614060	757434.901495	41.650880
3510.416502	757258.436919	41.655885
3510.352850	757075.085396	41.660890
3509.551756	756893.726972	41.665895
3509.768780	756723.746255	41.670900
3509.950691	756551.200777	41.675904
3509.487454	756386.261083	41.680909
3509.682706	756217.309305	41.685914
3509.511197	756051.277539	41.690919
3509.342030	755891.807391	41.695924
3509.868133	755716.619194	41.700928
3509.586729	755561.208762	41.705933
3509.546781	755392.820689	41.710938
3509.234496	755227.781692	41.715943
3509.211866	755060.222731	41.720948
3509.469257	754904.413708	41.725952
3508.950476	754750.260342	41.730957
3508.957081	754590.585933	41.735962
3509.040907	754440.770409	41.740967
3508.781709	754286.614202	41.745972
3509.267644	754125.320255	41.750976
3508.864238	753972.465369	41.755981
3508.640687	753814.195428	41.760986
3508.676460	753660.224798	41.765991
3508.180830	753502.635340	41.770996
3508.526941	753363.718011	41.776000
3508.642005	753219.404269	41.781005
3508.496702	753074.982697	41.786010
3508.354714	752929.125717	41.791015
3507.907470	752786.279546	41.796020
3507.960997	752643.891219	41.801024
3508.167909	752506.512414	41.806029
3507.835460	752368.775801	41.811034
3507.938821	752228.495258	41.816039
3507.832373	752094.667521	41.821044
3508.157912	751953.653808	41.826048
3507.668300	751825.762226	41.831053
3507.793486	751676.873912	41.836058
3507.823337	751546.224659	41.841063
3507.128762	751430.165400	41.846068
3507.641232	751295.184254	41.851072
3507.566207	751177.339384	41.856077
3507.583291	751041.250175	41.861082
3507.484842	750909.327051	41.866087
3507.443439	750779.022394	41.871092
3507.516835	750648.597773	41.876096
3507.351793	750529.522936	41.881101
3507.193451	750406.493110	41.886106
3507.179822	750276.175402	41.891111
3506.845534	750157.863842	41.896116
3507.148617	750029.021110	41.901120
3507.199232	749920.720539	41.906125
3507.158949	749785.458613	41.911130
3506.946000	749671.467182	41.916135
3506.939281	749544.050944	41.921140
3506.754109	749425.802386	41.926144
3506.645251	749313.567145	41.931149
3506.791022	749187.947945	41.936154
3506.660706	749078.874997	41.941159
3506.414231	748966.113977	41.946164
3506.614818	748852.338643	41.951168
3506.741579	748744.107903	41.956173
3506.628514	748632.703516	41.961178
3506.676266	748515.044962	41.966183
3506.513988	748401.570065	41.971188
3506.444388	748299.641094	41.976192
3506.158823	748194.583936	41.981197
3506.313463	748080.310763	41.986202
3506.454850	747970.139645	41.991207
3506.290105	747865.947578	41.996212
3506.757032	747746.478557	42.001216
3506.161506	747634.941953	42.006221
3506.042567	747536.025658	42.011226
3506.162229	747440.182108	42.016231
3505.974255	747334.009990	42.021236
3506.070589	747218.399479	42.026240
3505.710823	747128.265306	42.031245
3505.754233	747010.337650	42.036250
3505.964405	746907.800604	42.041255
3505.678279	746811.423319	42.046260
3505.590776	746709.229401	42.051264
3505.342044	746634.788036	42.056269
3505.391879	746539.735768	42.061274
3505.789314	746456.091679	42.066279
3505.632571	746372.389998	42.071284
3505.573434	746263.414165	42.076288
3505.120074	746181.390545	42.081293
3505.496068	746077.727809	42.086298
3505.100111	745990.255604	42.091303
3505.433260	745910.422315	42.096308
3505.394312	745818.143987	42.101312
3505.250462	745735.125374	42.106317
3505.112475	745637.028504	42.111322
3504.921793	745556.487281	42.116327
3504.864509	745475.033410	42.121332
3505.278116	745381.884245	42.126336
3504.695659	745299.477255	42.131341
3504.846727	745219.963624	42.136346
3504.792482	745127.383088	42.141351
3504.623316	745067.397845	42.146356
3505.126899	744979.123044	42.151360
3505.022590	744897.176592	42.156365
3505.056141	744816.689584	42.161370
3504.664810	744740.474073	42.166375
3504.573476	744662.675697	42.171380
3504.754817	744574.795665	42.176384
3504.928359	744498.731646	42.181389
3504.687697	744414.676854	42.186394
3505.049998	744333.388987	42.191399
3504.929953	744270.719826	42.196404
3504.965732	744175.443456	42.201408
3504.627387	744107.321214	42.206413
3504.656445	744020.597285	42.211418
3504.663436	743936.002036	42.216423
3504.415148	743862.523094	42.221428
3504.460481	743792.554804	42.226432
3504.265229	743725.789998	42.231437
3504.705742	743641.762702	42.236442
3504.407346	743574.420335	42.241447
3504.172489	743507.660223	42.246452
3504.363935	743433.165161	42.251456
3503.870655	743367.287125	42.256461
3504.229348	743299.289919	42.261466
3504.333752	743231.779165	42.266471
3503.711954	743159.097069	42.271476
3504.193978	743092.066626	42.276480
3504.109144	743031.161861	42.281485
3503.786748	742955.511018	42.286490
3504.054195	742889.453820	42.291495
3503.914920	742833.748584	42.296500
3503.959206	742769.606306	42.301504
3503.793182	742714.646382	42.306509
3503.859677	742640.658975	42.311514
3504.026285	742574.121306	42.316519
3503.716167	742523.238772	42.321524
3503.824517	742453.989942	42.326528
3503.876243	742397.162138	42.331533
3503.495636	742335.361304	42.336538
3503.850410	742271.015310	42.341543
3503.980261	742209.623656	42.346548
3504.145830	742139.769186	42.351552
3503.735757	742085.438645	42.356557
3503.695500	742020.908631	42.361562
3503.695402	741958.794699	42.366567
3503.424135	741899.593445	42.371572
3503.781843	741840.584535	42.376576
3503.962097	741791.198796	42.381581
3503.318803	741734.134894	42.386586
3503.582699	741682.261882	42.391591
3503.346771	741626.910292	42.396596
3503.499307	741563.432716	42.401600
3503.454976	741519.423693	42.406605
3503.383247	741449.750713	42.411610
3503.484710	741397.457563	42.416615
3503.021334	741342.042650	42.421620
3503.443331	741291.278480	42.426624
3503.297081	741244.515112	42.431629
3502.961553	741193.331456	42.436634
3503.218678	741143.236548	42.441639
3502.947117	741103.071110	42.446644
3503.253773	741046.735526	42.451648
3503.011737	741003.250901	42.456653
3502.542161	740957.231706	42.461658
3503.057337	740903.877723	42.466663
3503.038084	740865.895112	42.471668
3503.159711	740821.854785	42.476672
3502.866872	740767.297963	42.481677
3502.650527	740728.259111	42.486682
3503.108273	740682.678615	42.491687
3502.960334	740647.931253	42.496692
3503.054128	740588.016846	42.501696
3502.705131	740551.373247	42.506701
3502.714536	740500.622738	42.511706
3503.501572	740461.565147	42.516711
3502.562736	740416.312842	42.521716
3502.650617	740363.075301	42.526720
3503.082798	740329.813524	42.531725
3502.959397	740287.888220	42.536730
3502.972836	740234.612656	42.541735
3503.143834	740191.747827	42.546740
3502.997740	740152.249343	42.551744
3502.688225	740109.265615	42.556749
3502.713398	740065.929549	42.561754
3502.698142	740024.825902	42.566759
3502.788206	739985.238094	42.571764
3503.038093	739936.323955	42.576768
3502.728875	739898.434097	42.581773
3503.077668	739853.905656	42.586778
3503.248357	739807.922377	42.591783
3502.711595	739758.048856	42.596788
3502.884004	739722.502485	42.601792
3502.670474	739683.111746	42.606797
3502.275575	739631.235255	42.611802
3502.709825	739597.772202	42.616807
3502.384679	739561.515835	42.621812
3502.507638	739521.326652	42.626816
3502.843478	739485.010173	42.631821
3502.399150	739443.133442	42.636826
3502.522842	739408.682052	42.641831
3502.319150	739376.560241	42.646836
3502.759194	739341.165818	42.651840
3502.470809	739306.930497	42.656845
3502.496467	739272.643130	42.661850
3502.777503	739222.185859	42.666855
3502.585798	739200.598688	42.671860
3502.331490	739155.819709	42.676864
3501.919026	739123.385075	42.681869
3502.280164	739090.476162	42.686874
3502.302746	739053.022155	42.691879
3502.267830	739025.076162	42.696884
3502.282284	738982.329628	42.701888
3502.453279	738945.988461	42.706893
3502.246320	738916.536861	42.711898
3502.278387	738893.081374	42.716903
3502.325362	738857.799235	42.721908
3502.384896	738819.793818	42.726912
3502.368533	738803.519736	42.731917
3502.600950	738762.813898	42.736922
3502.467742	738724.988303	42.741927
3502.316453	738688.798170	42.746932
3502.660979	738640.948868	42.751936
3502.135080	738611.796220	42.756941
3501.901783	738589.966889	42.761946
3502.185740	738557.909609	42.766951
3502.205250	738530.002359	42.771956
3502.311647	738501.536421	42.776960
3502.127007	738473.811138	42.781965
3501.989637	738438.706034	42.786970
3502.266152	738405.857758	42.791975
3501.965945	738372.906748	42.796980
3502.091901	738346.762414	42.801985
3501.946160	738328.579158	42.806989
3502.207960	738296.178152	42.811994
3502.128043	738259.133166	42.816999
3501.998719	738241.837586	42.822004
3502.354621	738208.381652	42.827009
3501.983839	738183.555806	42.832013
3501.986421	738158.470271	42.837018
3502.246020	738129.730301	42.842023
3502.100537	738101.700384	42.847028
3502.270762	738062.287678	42.852033
3502.450968	738035.143792	42.857037
3502.033331	737994.244588	42.862042
3502.184158	737968.243340	42.867047
3501.901740	737948.449000	42.872052
3502.067304	737919.031106	42.877057
3501.977431	737886.637075	42.882061
3502.073356	737855.449197	42.887066
3502.009602	737833.045498	42.892071
3502.049263	737810.476206	42.897076
3502.037733	737790.141908	42.902081
3501.875167	737762.558942	42.907085
3502.101845	737736.742326	42.912090
3502.267647	737705.987640	42.917095
3502.204010	737683.731943	42.922100
3502.223154	737644.639027	42.927105
3502.164626	737621.491657	42.932109
3502.088099	737587.461332	42.937114
3502.334617	737543.975999	42.942119
3501.989771	737532.355384	42.947124
3501.797884	737488.546346	42.952129
3501.899116	737474.427319	42.957133
3501.749843	737442.684567	42.962138
3501.679287	737426.020773	42.967143
3501.602514	737404.756114	42.972148
3502.181139	737374.278306	42.977153
3502.100494	737356.923279	42.982157
3501.731493	737334.618108	42.987162
3501.953377	737302.368117	42.992167
3501.723072	737274.052411	42.997172
3501.823510	737245.484014	43.002177
3501.607727	737226.468602	43.007181
3501.546437	737200.005074	43.012186
3501.896479	737190.100018	43.017191
3501.577942	737163.728365	43.022196
3501.545486	737152.599893	43.027201
3501.789333	737119.355857	43.032205
3501.794891	737113.565332	43.037210
3501.870804	737091.829250	43.042215
3501.691208	737066.572454	43.047220
3502.015439	737033.166322	43.052225
3502.122033	737006.031107	43.057229
3502.014541	736989.570446	43.062234
3502.283288	736959.686606	43.067239
3501.683418	736937.616417	43.072244
3501.697364	736925.638711	43.077249
3501.584375	736901.854947	43.082253
3501.736837	736873.375594	43.087258
3501.827099	736852.725176	43.092263
3501.566862	736831.934682	43.097268
3501.868956	736804.024187	43.102273
3501.642382	736788.968401	43.107277
3501.935363	736762.147961	43.112282
3501.879201	736742.263750	43.117287
3501.768732	736722.487437	43.122292
3501.750601	736691.610787	43.127297
3501.633393	736673.567504	43.132301
3501.658533	736654.411942	43.137306
3501.858273	736630.278767	43.142311
3501.530831	736613.160858	43.147316
3501.577268	736592.714960	43.152321
3501.679910	736566.024293	43.157325
3501.792033	736547.794365	43.162330
3502.029863	736519.101695	43.167335
3501.592813	736505.663768	43.172340
3501.589166	736477.951127	43.177345
3501.619107	736458.695327	43.182349
3501.503967	736440.453223	43.187354
3501.595457	736425.443166	43.192359
3501.417532	736407.112385	43.197364
3501.562781	736384.670085	43.202369
3501.585001	736375.807975	43.207373
3501.455645	736343.562679	43.212378
3501.666858	736343.131901	43.217383
3501.046096	736319.133383	43.222388
3501.457418	736300.507024	43.227393
3501.596621	736296.030030	43.232397
3501.418902	736274.779047	43.237402
3501.649511	736245.938125	43.242407
3501.258591	736237.935969	43.247412
3501.618882	736219.020917	43.252417
3501.173960	736195.339395	43.257421
3501.539991	736181.421778	43.262426
3501.549222	736175.283538	43.267431
3501.490526	736153.369193	43.272436
3501.571336	736129.105694	43.277441
3501.699381	736128.490689	43.282445
3501.704085	736105.081028	43.287450
3501.772747	736088.787363	43.292455
3501.667231	736074.551564	43.297460
3501.725566	736042.274037	43.302465
3501.776706	736029.051575	43.307469
3501.869705	736005.231104	43.312474
3502.169708	735976.575710	43.317479
3501.728925	735954.773456	43.322484
3501.850914	735939.856434	43.327489
3501.835460	735913.727517	43.332493
3501.890728	735895.554993	43.337498
3501.946705	735855.110971	43.342503
3501.556514	735854.482604	43.347508
3501.392184	735823.379308	43.352513
3501.544097	735803.557364	43.357517
3501.475835	735791.245102	43.362522
3501.618565	735764.792605	43.367527
3501.540355	735748.967954	43.372532
3501.628994	735733.709611	43.377537
3501.641765	735712.425656	43.382541
3501.408575	735695.983106	43.387546
3501.593568	735677.887637	43.392551
3501.309738	735649.476037	43.397556
3501.559830	735638.397753	43.402561
3501.642572	735624.575482	43.407565
3501.304797	735599.637155	43.412570
3501.447710	735578.776780	43.417575
3501.342451	735569.043960	43.422580
3501.651275	735554.738764	43.427585
3501.433167	735536.313641	43.432589
3501.545774	735529.415414	43.437594
3501.674097	735502.617977	43.442599
3501.341437	735499.604354	43.447604
3501.488180	735483.049085	43.452609
3501.408484	735460.344409	43.457613
3501.266447	735442.747904	43.462618
3501.664714	735434.119576	43.467623
3501.277044	735413.692917	43.472628
3501.153826	735389.757867	43.477633
3501.711443	735385.557684	43.482637
3501.568002	735375.632960	43.487642
3501.724416	735344.425306	43.492647
3501.552847	735342.226417	43.497652
3501.410070	735321.511577	43.502657
3501.455923	735311.407004	43.507661
3501.374738	735285.088922	43.512666
3501.762258	735274.482381	43.517671
3501.349033	735249.406946	43.522676
3501.498638	735234.385058	43.527681
3501.291870	735208.235964	43.532685
3501.386660	735204.854613	43.537690
3501.508065	735187.560484	43.542695
3501.181206	735177.715321	43.547700
3501.561605	735154.092311	43.552705
3501.466650	735139.506631	43.557709
3501.469494	735141.090082	43.562714
3501.602682	735104.638722	43.567719
3501.219230	735103.910183	43.572724
3501.115472	735093.533082	43.577729
3501.525162	735092.376489	43.582733
3501.303653	735056.280505	43.587738
3501.593855	735036.928786	43.592743
3501.436680	735035.420392	43.597748
3501.635951	734995.690815	43.602753
3501.946531	735001.876176	43.607757
3501.443500	734971.023536	43.612762
3501.474110	734944.883853	43.617767
3501.186422	734932.755028	43.622772
3501.759134	734931.769463	43.627777
3501.346495	734909.068752	43.632781
3501.180909	734900.087555	43.637786
3501.554159	734893.492195	43.642791
3501.608369	734860.616626	43.647796
3501.804742	734839.300015	43.652801
3501.480218	734829.503535	43.657805
3501.416523	734796.251201	43.662810
3501.508820	734793.711564	43.667815
3501.486802	734777.529222	43.672820
3501.504131	734752.925565	43.677825
3501.526185	734747.576094	43.682829
3501.217904	734720.996699	43.687834
3501.502715	734698.724621	43.692839
3501.278969	734690.148793	43.697844
3501.314331	734688.113524	43.702849
3501.409888	734676.069473	43.707853
3501.345093	734656.874505	43.712858
3501.618024	734642.821119	43.717863
3501.123680	734635.329438	43.722868
3501.199289	734614.378685	43.727873
3501.586242	734597.781898	43.732877
3501.341836	734585.942393	43.737882
3501.246991	734568.583671	43.742887
3500.850511	734549.443260	43.747892
3501.077837	734545.792231	43.752897
3501.091887	734530.395431	43.757901
3501.396001	734537.572223	43.762906
3501.208888	734526.317162	43.767911
3501.165895	734510.286249	43.772916
3501.331358	734504.170413	43.777921
3501.436722	734494.549982	43.782925
3501.224340	734484.734549	43.787930
3501.574241	734455.471485	43.792935
3501.032559	734457.095557	43.797940
3501.328501	734448.285086	43.802945
3501.112061	734417.877963	43.807949
3501.093840	734417.138500	43.812954
3501.409737	734395.701962	43.817959
3501.368212	734388.531224	43.822964
3501.379764	734378.876658	43.827969
3501.284506	734357.903973	43.832973
3501.171922	734349.160906	43.837978
3501.471817	734334.360009	43.842983
3501.098679	734327.788533	43.847988
3501.599690	734305.331135	43.852993
3501.405216	734302.294219	43.857997
3501.285194	734300.581539	43.863002
3501.540411	734254.997879	43.868007
3501.535467	734255.988770	43.873012
3501.431314	734243.927575	43.878017
3501.327285	734227.114154	43.883021
3501.188677	734207.583798	43.888026
3501.513960	734191.491389	43.893031
3501.107678	734192.746621	43.898036
3501.382460	734169.039174	43.903041
3501.313970	734158.704538	43.908045
3501.176696	734162.588447	43.913050
3501.589120	734139.353190	43.918055
3501.475886	734118.877878	43.923060
3501.406058	734108.939421	43.928065
3501.199332	734098.380039	43.933069
3500.938641	734072.087648	43.938074
3501.423630	734055.968576	43.943079
3501.304079	734058.760540	43.948084
3501.322442	734047.916379	43.953089
3501.166783	734024.873678	43.958093
3501.149693	734017.203540	43.963098
3501.223795	733992.340659	43.968103
3501.377792	733996.424030	43.973108
3501.409120	733981.914386	43.978113
3501.385636	733960.780295	43.983117
3501.018902	733950.049146	43.988122
3501.121941	733943.299654	43.993127
3501.184397	733951.407975	43.998132
3501.399734	733932.660022	44.003137
3501.322588	733907.722868	44.008141
3501.297856	733908.370544	44.013146
3501.306964	733897.527710	44.018151
3500.800651	733876.869221	44.023156
3501.174171	733867.253232	44.028161
3501.261271	733853.674720	44.033165
3501.367917	733846.677030	44.038170
3501.401354	733834.840005	44.043175
3501.096335	733815.385702	44.048180
3501.154929	733798.693025	44.053185
3501.348431	733799.007617	44.058189
3501.363296	733789.549815	44.063194
3501.232141	733762.640951	44.068199
3501.153942	733755.277690	44.073204
3501.440803	733747.507560	44.078209
3501.473364	733743.195288	44.083213
3501.030081	733729.753722	44.088218
3501.298111	733712.036154	44.093223
3501.202370	733722.448085	44.098228
3501.057386	733711.927497	44.103233
3501.392429	733678.109596	44.108237
3501.117501	733670.778769	44.113242
3501.162291	733671.414975	44.118247
3501.051531	733670.344199	44.123252
3501.053050	733662.522131	44.128257
3501.028964	733627.624742	44.133261
3500.959504	733616.150940	44.138266
3501.274503	733613.029567	44.143271
3500.956338	733616.102034	44.148276
3501.285203	733608.275322	44.153281
3501.403567	733593.305044	44.158285
3501.061484	733576.529604	44.163290
3501.240670	733566.252290	44.168295
3501.009481	733564.062762	44.173300
3500.814039	733554.342402	44.178305
3501.196120	733541.209678	44.183309
3501.145577	733528.792008	44.188314
3501.545303	733515.012744	44.193319
3501.439424	733521.218569	44.198324
3501.353773	733502.321332	44.203329
3501.270480	733465.502276	44.208333
3500.817316	733467.359442	44.213338
3501.572865	733453.471763	44.218343
3501.017839	733451.187201	44.223348
3500.807986	733429.389420	44.228353
3501.018286	733421.532616	44.233357
3501.179252	733423.535836	44.238362
3501.114259	733407.902419	44.243367
3501.029455	733413.807802	44.248372
3500.696894	733408.367524	44.253377
3500.951937	733410.652242	44.258381
3500.489800	733397.411263	44.263386
3500.900451	733362.836941	44.268391
3500.915390	733367.290164	44.273396
3501.117258	733358.840605	44.278401
3501.393096	733355.379054	44.283405
3500.866988	733365.367494	44.288410
3500.911148	733364.023538	44.293415
3500.744324	733375.833866	44.298420
3500.879604	733352.840177	44.303425
3501.028850	733324.992380	44.308429
3501.267898	733319.556593	44.313434
3501.063844	733311.471112	44.318439
3501.194086	733310.459475	44.323444
3501.085081	733309.338852	44.328449
3501.243888	733295.698043	44.333453
3501.078200	733282.308869	44.338458
3501.146164	733263.484701	44.343463
3501.215065	733266.394317	44.348468
3500.799463	733273.295119	44.353473
3501.321839	733266.723303	44.358477
3501.151486	733244.423416	44.363482
3501.247597	733223.713200	44.368487
3501.045732	733227.311182	44.373492
3501.083525	733217.353839	44.378497
3501.111424	733211.952874	44.383501
3501.096198	733195.914756	44.388506
3501.117911	733178.038690	44.393511
3500.959969	733175.737934	44.398516
3501.225355	733169.852118	44.403521
3501.103941	733166.010560	44.408525
3500.875584	733154.314818	44.413530
3501.013031	733121.517412	44.418535
3500.724435	733131.961975	44.423540
3500.586026	733121.588054	44.428545
3500.924563	733123.562005	44.433549
3500.669983	733133.010770	44.438554
3501.120384	733116.796528	44.443559
3500.748014	733118.194840	44.448564
3500.789387	733118.138532	44.453569
3501.087281	733116.802112	44.458573
3501.198150	733117.427443	44.463578
3501.158023	733090.204237	44.468583
3500.788991	733073.828273	44.473588
3500.618704	733075.886323	44.478593
3500.926134	733068.904288	44.483597
3500.756741	733065.367665	44.488602
3501.256690	733055.927858	44.493607
3501.285174	733066.270596	44.498612
3500.997432	733043.791516	44.503617
3501.319896	733032.945245	44.508621
3501.230070	733028.850854	44.513626
3501.039695	733015.366297	44.518631
3500.630456	733030.237264	44.523636
3500.863603	733018.415547	44.528641
3500.935490	733007.016538	44.533645
3501.087146	732991.495038	44.538650
3501.011847	732976.803170	44.543655
3501.118258	732969.507702	44.548660
3501.291920	732973.142757	44.553665
3501.709279	732966.885112	44.558669
3501.085517	732948.422072	44.563674
3501.062243	732941.643109	44.568679
3501.083463	732941.144541	44.573684
3500.936766	732939.089408	44.578689
3501.411575	732926.980072	44.583693
3501.211064	732903.743537	44.588698
3501.284079	732888.680427	44.593703
3501.120343	732888.311442	44.598708
3501.207795	732875.176818	44.603713
3501.215700	732857.351835	44.608717
3501.136854	732851.621697	44.613722
3500.902671	732836.361705	44.618727
3501.330052	732836.439646	44.623732
3500.958516	732829.074505	44.628737
3501.295119	732814.413291	44.633741
3501.293386	732800.105029	44.638746
3501.318101	732786.485522	44.643751
3501.279177	732790.700410	44.648756
3501.404127	732777.163344	44.653761
3501.222776	732752.289347	44.658765
3501.445059	732762.798491	44.663770
3501.090889	732743.795319	44.668775
3501.038925	732726.029451	44.673780
3501.167647	732706.451277	44.678785
3501.322230	732692.364548	44.683789
3501.057835	732700.379608	44.688794
3501.160983	732685.311140	44.693799
3501.101110	732675.616826	44.698804
3500.806124	732661.505315	44.703809
3501.084468	732647.398055	44.708813
3501.208194	732660.498226	44.713818
3501.150871	732650.852973	44.718823
3500.804008	732649.474495	44.723828
3500.857257	732646.098940	44.728833
3501.507631	732618.413452	44.733837
3501.165223	732602.131152	44.738842
3500.939675	732597.266780	44.743847
3501.173346	732598.020394	44.748852
3501.237974	732591.424658	44.753857
3501.125679	732564.310630	44.758861
3501.031306	732556.998459	44.763866
3501.221644	732551.669233	44.768871
3500.806031	732553.371859	44.773876
3500.876651	732557.915351	44.778881
3501.410986	732548.221711	44.783885
3501.044574	732524.615403	44.788890
3501.149614	732504.396992	44.793895
3500.692205	732507.146297	44.798900
3500.678117	732498.186892	44.803905
3501.138827	732498.308844	44.808909
3500.935819	732507.551764	44.813914
3501.110542	732484.796650	44.818919
3500.920827	732470.964484	44.823924
3501.116770	732455.187074	44.828929
3501.142821	732446.716107	44.833933
3500.851271	732461.964769	44.838938
3500.779640	732436.824104	44.843943
3500.853696	732455.725829	44.848948
3500.726116	732449.161741	44.853953
3500.848718	732445.378539	44.858957
3500.894209	732439.082918	44.863962
3501.042600	732411.875785	44.868967
3500.756886	732405.238768	44.873972
3500.730410	732393.855150	44.878977
3501.063686	732402.167840	44.883981
3500.806896	732406.815038	44.888986
3500.789527	732403.153973	44.893991
3500.662226	732411.493255	44.898996
3500.742234	732395.289269	44.904001
3500.971100	732399.410593	44.909005
3500.913665	732399.717202	44.914010
3501.032991	732392.419080	44.919015
3500.842858	732370.417124	44.924020
3500.633943	732364.807162	44.929025
3500.515872	732358.835590	44.934029
3500.623625	732353.420855	44.939034
3500.769213	732361.764605	44.944039
3501.034167	732351.966709	44.949044
3500.877888	732359.865211	44.954049
3501.046443	732353.301620	44.959053
3500.881595	732356.250194	44.964058
3501.079392	732370.923024	44.969063
3501.060163	732358.993513	44.974068
3500.554447	732322.437105	44.979073
3500.711850	732314.835538	44.984077
3500.768199	732310.023434	44.989082
3500.657836	732305.090336	44.994087
3500.741762	732309.037604	44.999092
3500.776820	732310.071637	45.004097
3500.499512	732304.720504	45.009101
3500.466063	732312.054103	45.014106
3500.903994	732303.316865	45.019111
3500.802045	732312.048169	45.024116
3500.545039	732303.326747	45.029121
3500.673549	732304.939502	45.034125
3500.999696	732308.401118	45.039130
3501.185998	732297.774421	45.044135
3500.919926	732307.027991	45.049140
3500.851572	732308.227655	45.054145
3501.232050	732303.064900	45.059149
3501.100407	732269.070661	45.064154
3500.916728	732267.615634	45.069159
3501.257709	732261.320558	45.074164
3501.049282	732260.513301	45.079169
3501.244793	732246.369518	45.084173
3501.137455	732233.266043	45.089178
3501.096014	732224.013769	45.094183
3501.190794	732213.798202	45.099188
3501.259459	732216.411150	45.104193
3501.221717	732206.118444	45.109197
3501.140051	732197.813561	45.114202
3501.069695	732189.655344	45.119207
3501.101938	732188.758793	45.124212
3501.288038	732187.242642	45.129217
3501.130218	732164.541583	45.134221
3501.112567	732153.156168	45.139226
3501.041825	732127.321189	45.144231
3500.965738	732126.541563	45.149236
3500.812760	732133.350413	45.154241
3500.988163	732127.825319	45.159245
3500.681212	732135.105247	45.164250
3501.097520	732128.153927	45.169255
3500.946084	732110.452658	45.174260
3500.745698	732093.551681	45.179265
3501.049471	732094.392789	45.184269
3500.966808	732085.642320	45.189274
3500.662682	732092.228608	45.194279
3501.026139	732085.137440	45.199284
3500.920520	732092.582195	45.204289
3500.846353	732089.871161	45.209293
3500.659348	732092.476886	45.214298
3500.555861	732082.343433	45.219303
3500.893940	732075.553541	45.224308
3500.410568	732062.858538	45.229313
3500.635143	732057.176724	45.234317
3500.679844	732078.163824	45.239322
3500.987647	732056.920484	45.244327
3500.960895	732038.455724	45.249332
3500.531159	732041.992856	45.254337
3501.185362	732035.893420	45.259341
3500.702363	732031.764467	45.264346
3500.893915	732030.792056	45.269351
3500.786891	732030.908812	45.274356
3500.679230	732033.947082	45.279361
3500.990791	732029.835367	45.284365
3500.852868	732031.442692	45.289370
3501.001361	732025.278274	45.294375
3500.674196	732019.489551	45.299380
3500.648039	732008.600493	45.304385
3500.861711	731992.373612	45.309389
3500.545368	731995.297837	45.314394
3501.114933	731991.242496	45.319399
3500.647233	732002.411330	45.324404
3500.870183	731992.669458	45.329409
3501.338794	731985.709373	45.334413
3500.736103	731994.672318	45.339418
3500.577590	731991.281971	45.344423
3500.613842	731992.464394	45.349428
3500.821172	731985.844582	45.354433
3501.056645	731980.606555	45.359437
3500.823861	731987.032591	45.364442
3500.618772	731952.801581	45.369447
3501.092715	731951.782494	45.374452
3500.707172	731944.121759	45.379457
3501.104182	731936.084113	45.384461
3500.818871	731943.509184	45.389466
3500.840335	731936.771500	45.394471
3500.879849	731932.358082	45.399476
3500.583625	731945.231717	45.404481
3501.168596	731941.966062	45.409485
3500.859365	731942.264782	45.414490
3500.908621	731930.917514	45.419495
3500.870040	731905.918285	45.424500
3500.367006	731905.407259	45.429505
3500.679185	731898.076821	45.434509
3500.537678	731902.507190	45.439514
3501.091364	731896.424261	45.444519
3501.042577	731897.323654	45.449524
3500.802863	731910.336555	45.454529
3500.831936	731904.785975	45.459533
3500.816783	731902.659320	45.464538
3500.784178	731908.062012	45.469543
3500.706830	731908.867092	45.474548
3500.561736	731904.385134	45.479553
3500.963233	731900.308007	45.484557
3500.580359	731900.668416	45.489562
3500.996790	731898.420920	45.494567
3501.036727	731868.258908	45.499572
3500.807309	731869.584287	45.504577
3501.202042	731852.931073	45.509581
3500.957664	731857.031850	45.514586
3500.907883	731846.394061	45.519591
3501.026642	731852.019359	45.524596
3501.044156	731848.005663	45.529601
3501.273266	731823.060974	45.534605
3501.152264	731818.921604	45.539610
3500.900481	731807.178260	45.544615
3500.820407	731802.982601	45.549620
3500.721912	731809.089484	45.554625
3501.148545	731810.950172	45.559629
3500.699169	731815.877116	45.564634
3500.937892	731799.843777	45.569639
3501.210338	731783.260147	45.574644
3500.754698	731776.155522	45.579649
3500.693428	731767.599241	45.584653
3500.224559	731771.737160	45.589658
3500.658853	731765.574831	45.594663
3500.698932	731767.152791	45.599668
3500.366561	731767.950512	45.604673
3500.879636	731754.595182	45.609677
3500.800928	731766.591362	45.614682
3500.914945	731754.292320	45.619687
3500.738397	731756.054633	45.624692
3500.719912	731766.802933	45.629697
3500.494170	731752.777422	45.634701
3500.596688	731758.554021	45.639706
3500.909984	731758.007113	45.644711
3500.893390	731769.151235	45.649716
3500.765030	731766.052911	45.654721
3500.910036	731770.386485	45.659725
3500.952881	731758.643898	45.664730
3501.066967	731748.523588	45.669735
3500.933836	731729.828118	45.674740
3500.471345	731724.952857	45.679745
3500.897612	731713.344910	45.684749
3500.598454	731725.773721	45.689754
3500.856368	731717.511260	45.694759
3500.904804	731722.405510	45.699764
3501.104279	731722.471618	45.704769
3501.331427	731723.325430	45.709773
3500.985848	731705.655359	45.714778
3501.125621	731681.071618	45.719783
3501.068943	731676.971063	45.724788
3500.757059	731676.725536	45.729793
3500.992995	731671.437717	45.734797
3501.137624	731679.930882	45.739802
3500.938305	731669.565160	45.744807
3500.995770	731646.430928	45.749812
3500.675529	731638.957181	45.754817
3500.822340	731622.294949	45.759821
3500.864473	731558.805783	45.764826
3500.652442	731435.638336	45.769831
3500.567290	731274.466252	45.774836
3500.341801	731052.997299	45.779841
3500.712474	730773.779073	45.784845
3500.600580	730429.109396	45.789850
3500.020078	730022.295985	45.794855
3500.123789	729581.817143	45.799860
3499.647181	729059.333682	45.804865
3499.432643	728484.115694	45.809869
3499.077650	727866.721267	45.814874
3498.819651	727178.018820	45.819879
3498.716826	726443.003323	45.824884
3498.333841	725639.781882	45.829889
3497.830968	724771.380826	45.834893
3496.995025	723864.084401	45.839898
3496.936484	722892.762401	45.844903
3496.434045	721858.090180	45.849908
3495.674125	720782.821888	45.854913
3495.491010	719614.536197	45.859917
3494.582741	718401.816989	45.864922
3493.951393	717131.136047	45.869927
3493.171208	715801.992263	45.874932
3492.479557	714421.216703	45.879937
3492.075983	712959.371162	45.884941
3491.115908	711453.882337	45.889946
3490.583104	709882.373003	45.894951
3489.890284	708245.550467	45.899956
3488.638152	706556.010279	45.904961
3487.953993	704801.464977	45.909965
3487.010620	702996.621383	45.914970
3486.240924	701127.214404	45.919975
3485.207982	699199.937661	45.924980
3484.176704	697200.739922	45.929985
3483.242728	695152.286148	45.934989
3482.092583	693052.905228	45.939994
3480.971404	690879.038741	45.944999
3480.198107	688677.563534	45.950004
3479.051403	686385.659654	45.955009
3477.846238	684051.011310	45.960013
3476.108679	681671.924477	45.965018
3475.229861	679225.968959	45.970023
3474.586902	676721.620594	45.975028
3473.140887	674168.628782	45.980033
3471.773759	671539.539078	45.985037
3470.237401	668868.348356	45.990042
3469.021555	666130.799478	45.995047
3467.658903	663354.664742	46.000052
3465.998188	660528.910097	46.005057
3464.829724	657639.287021	46.010061
3463.012883	654697.272416	46.015066
3461.846817	651702.811657	46.020071
3460.571337	648650.293237	46.025076
3458.480282	645553.686970	46.030081
3457.107937	642393.253694	46.035085
3455.670333	639206.640916	46.040090
3454.036444	635943.715198	46.045095
3452.331961	632635.177907	46.050100
3450.407677	629284.525723	46.055105
3448.905730	625859.015938	46.060109
3446.846596	622410.356840	46.065114
3445.289065	618897.565057	46.070119
3443.526099	615337.703834	46.075124
3441.391147	611739.243406	46.080129
3439.735736	608079.091404	46.085133
3437.577540	604377.337416	46.090138
3435.710188	600629.004328	46.095143
3433.913095	596828.774631	46.100148
3431.806214	592988.480582	46.105153
3429.866903	589076.261224	46.110157
3427.724291	585133.393029	46.115162
3426.077323	581139.533258	46.120167
3423.834954	577107.706647	46.125172
3421.471019	573026.997636	46.130177
3419.435719	568894.534375	46.135181
3417.293053	564734.021783	46.140186
3414.737240	560512.815913	46.145191
3412.807728	556241.135487	46.150196
3410.391521	551953.608734	46.155201
3408.342170	547603.770895	46.160205
3405.804900	543215.074802	46.165210
3403.573814	538784.650970	46.170215
3401.472933	534308.929862	46.175220
3398.940011	529786.623189	46.180225
3396.738233	525219.757243	46.185229
3394.209874	520615.597025	46.190234
3391.686415	515969.077803	46.195239
3388.933272	511281.641590	46.200244
3386.452969	506555.571722	46.205249
3384.236412	501785.402049	46.210253
3381.376766	496995.349034	46.215258
3378.885221	492147.512648	46.220263
3376.119373	487264.399662	46.225268
3373.343968	482355.180338	46.230273
3370.890757	477396.313059	46.235277
3368.330111	472408.221574	46.240282
3365.414319	467380.113158	46.245287
3362.667494	462310.837955	46.250292
3359.882084	457219.085764	46.255297
3357.034675	452077.345441	46.260301
3354.105421	446928.725562	46.265306
3351.202124	441730.830018	46.270311
3348.432617	436495.565119	46.275316
3345.361758	431237.730745	46.280321
3342.381271	425942.410229	46.285325
3339.203764	420625.657081	46.290330
3336.131498	415280.792655	46.295335
3333.491873	409903.999390	46.300340
3329.913955	404505.150825	46.305345
3327.086369	399054.014010	46.310349
3323.961584	393609.295349	46.315354
3320.570489	388113.822118	46.320359
3317.538552	382598.772155	46.325364
3314.237603	377069.467624	46.330369
3310.929684	371507.820425	46.335373
3307.686736	365930.427963	46.340378
3304.713769	360327.448457	46.345383
3301.265329	354692.219892	46.350388
3297.617321	349069.405208	46.355393
3294.482939	343382.215771	46.360397
3290.874819	337696.036557	46.365402
3287.549849	331973.730593	46.370407
3284.454531	326244.918871	46.375412
3280.837898	320508.777067	46.380417
3277.247048	314725.212862	46.385421
3273.746161	308946.597830	46.390426
3270.012174	303164.147556	46.395431
3266.422625	297354.037737	46.400436
3262.876176	291530.435820	46.405441
3259.406595	285691.116026	46.410445
3255.442549	279859.165191	46.415450
3251.871743	274012.303554	46.420455
3248.184135	268135.229568	46.425460
3244.077500	262263.518468	46.430465
3240.568130	256377.084698	46.435469
3236.928403	250502.941741	46.440474
3233.027113	244599.979356	46.445479
3229.261170	238711.859528	46.450484
3225.269009	232807.571180	46.455489
3221.294554	226881.167068	46.460493
3217.510692	220973.159809	46.465498
3213.310301	215053.295447	46.470503
3209.506730	209097.928538	46.475508
3205.256158	203142.479682	46.480513
3201.543186	197226.791861	46.485517
3197.432737	191309.799199	46.490522
3192.799986	185399.209058	46.495527
3188.857548	179490.123484	46.500532
3184.147653	173603.114072	46.505537
3180.196680	167709.106237	46.510541
3176.040691	161836.867872	46.515546
3171.600734	155965.697874	46.520551
3167.680440	150100.929800	46.525556
3163.016409	144251.770062	46.530561
3158.616513	138406.946002	46.535565
3154.194067	132598.935869	46.540570
3149.571934	126787.529607	46.545575
3145.196009	120989.372634	46.550580
3140.542752	115229.640994	46.555585
3135.986440	109468.929264	46.560589
3131.499651	103728.633592	46.565594
3126.154494	98018.455815	46.570599
3121.362482	92333.861622	46.575604
3116.744638	86680.486970	46.580609
3111.680602	81044.682128	46.585613
3106.802999	75467.305358	46.590618
3101.437591	69890.274056	46.595623
3096.706669	64349.310875	46.600628
3091.209586	58863.619439	46.605633
3085.997013	53409.644354	46.610637
3080.172665	48007.838444	46.615642
3074.341632	42654.512289	46.620647
3068.017630	37351.070541	46.625652
3061.205822	32121.120133	46.630657
3053.995771	26970.090511	46.635661
3041.724426	22038.840289	46.640666
3025.534180	17343.152899	46.645671
3009.449437	12822.495951	46.650676
2992.939224	8545.440082	46.655681
2977.219539	4528.229957	46.660685
2953.691016	1007.063305	46.665690
2842.083448	274.342335	46.670695
2744.038548	275.792172	46.675700
2702.508380	258.009967	46.680705
2707.678484	239.853716	46.685709
2738.229441	231.139965	46.690714
2774.391781	250.941415	46.695719
2803.257818	247.928880	46.700724
2819.184282	249.004359	46.705729
2824.686971	229.561601	46.710733
2821.762656	227.628658	46.715738
2815.464735	231.712075	46.720743
2808.984923	236.529118	46.725748
2803.105657	247.125079	46.730753
2799.651448	230.449507	46.735757
2797.272995	222.413345	46.740762
2794.832035	224.378748	46.745767
2792.569927	221.480956	46.750772
2790.054450	231.925479	46.755777
2787.650069	234.270036	46.760781
2784.931995	233.451291	46.765786
2781.462750	227.504932	46.770791
2778.858232	219.068705	46.775796
2775.349227	219.171223	46.780801
2771.857074	223.085296	46.785805
2768.992986	219.197461	46.790810
2765.591193	222.155281	46.795815
2763.091126	212.141034	46.800820
2759.628376	218.671880	46.805825
2755.817965	217.330064	46.810829
2753.123201	215.990260	46.815834
2749.261891	225.705420	46.820839
2746.553010	209.122436	46.825844
2743.265647	207.067110	46.830849
2739.856055	202.940637	46.835853
2736.429443	204.768881	46.840858
2732.837169	212.193811	46.845863
2729.680330	209.798978	46.850868
2726.367946	216.454538	46.855873
2723.554537	203.402875	46.860877
2719.630116	200.883706	46.865882
2716.607191	205.850098	46.870887
2712.865066	193.553674	46.875892
2709.083060	205.998320	46.880897
2705.886005	202.133488	46.885901
2702.918662	201.529127	46.890906
2699.084360	198.439753	46.895911
2695.629813	192.779360	46.900916
2692.525568	202.743376	46.905921
2689.596043	195.770017	46.910925
2686.079567	194.239300	46.915930
2682.335128	204.020797	46.920935
2679.302769	201.594938	46.925940
2675.250574	195.768477	46.930945
2671.905693	198.697407	46.935949
2668.530342	192.824221	46.940954
2665.013289	201.427083	46.945959
2661.926764	195.993510	46.950964
2658.193431	201.738232	46.955969
2654.894496	192.995556	46.960973
2651.017276	191.644178	46.965978
2647.220469	195.766845	46.970983
2644.606612	187.050478	46.975988
2641.401863	193.507706	46.980993
2637.780333	196.754984	46.985997
2634.353870	191.778308	46.991002
2630.498669	197.374899	46.996007
2627.129299	188.909526	47.001012
2623.671587	192.557125	47.006017
2620.984521	182.095217	47.011021
2617.437413	186.989398	47.016026
2613.599165	187.904925	47.021031
2610.189160	181.083605	47.026036
2606.319133	194.273040	47.031041
2602.672800	180.679963	47.036045
2599.195080	190.151741	47.041050
2595.785659	185.512882	47.046055
2592.762481	184.728400	47.051060
2589.109509	183.212275	47.056065
2585.792709	179.908665	47.061069
2583.049344	180.060995	47.066074
2579.130887	185.169626	47.071079
2575.463873	176.602821	47.076084
2571.515396	181.953035	47.081089
2567.939011	181.639843	47.086093
2564.414248	181.063937	47.091098
2561.033898	178.491939	47.096103
2557.963643	176.002789	47.101108
2554.606456	175.736591	47.106113
2551.183278	179.739060	47.111117
2547.513362	174.538343	47.116122
2544.122506	183.330355	47.121127
2540.801864	169.091413	47.126132
2536.961060	186.126882	47.131137
2533.312653	189.539525	47.136141
2530.029684	178.466142	47.141146
2526.505655	190.399522	47.146151
2523.233952	167.372980	47.151156
2519.647027	187.661355	47.156161
2516.124255	173.876820	47.161165
2513.183346	180.522906	47.166170
2509.130424	184.148972	47.171175
2505.968451	164.972477	47.176180
2502.508287	172.444560	47.181185
2498.656455	172.025483	47.186189
2495.354811	167.480956	47.191194
2491.569041	178.863909	47.196199
2488.177780	164.647371	47.201204
2484.444053	170.968513	47.206209
2481.282869	179.948683	47.211213
2478.127226	169.937252	47.216218
2474.350305	180.938684	47.221223
2471.227264	171.653978	47.226228
2467.489869	179.636725	47.231233
2463.634869	171.807626	47.236237
2460.113906	177.146538	47.241242
2456.480653	168.605046	47.246247
2453.739532	174.580882	47.251252
2450.177085	173.100605	47.256257
2446.473829	173.951499	47.261261
2443.033805	171.297918	47.266266
2439.360797	169.313216	47.271271
2436.427478	166.934881	47.276276
2432.783633	175.263682	47.281281
2428.806016	164.554673	47.286285
2425.300111	163.601613	47.291290
2421.487690	167.503469	47.296295
2418.938546	173.514429	47.301300
2415.075504	171.752241	47.306305
2411.446562	162.377717	47.311309
2407.913110	163.269591	47.316314
2404.478872	164.775132	47.321319
2401.380809	163.892486	47.326324
2397.516896	166.833181	47.331329
2393.957317	157.747338	47.336333
2390.523028	165.176339	47.341338
2387.002830	164.173976	47.346343
2383.760863	163.079557	47.351348
2380.029685	169.351816	47.356353
2376.549641	161.893271	47.361357
2373.512286	165.411845	47.366362
2369.532424	170.294415	47.371367
2366.489921	169.740236	47.376372
2362.472702	150.454728	47.381377
2359.040250	165.036289	47.386381
2355.772059	165.047568	47.391386
2352.000819	159.030272	47.396391
2348.713645	151.700248	47.401396
2344.955926	159.200608	47.406401
2341.435135	164.849399	47.411405
2338.117034	166.391407	47.416410
2334.812787	163.074482	47.421415
2331.452627	160.832635	47.426420
2327.521993	159.090803	47.431425
2323.861005	156.616796	47.436429
2320.623317	161.015750	47.441434
2316.984268	162.886612	47.446439
2313.889396	162.128417	47.451444
2310.159470	169.801020	47.456449
2306.878670	167.595973	47.461453
2303.322359	155.953384	47.466458
2299.166038	169.261695	47.471463
2296.133656	154.778901	47.476468
2292.738997	168.516755	47.481473
2289.276682	161.307944	47.486477
2285.929765	161.481898	47.491482
2282.057921	171.131659	47.496487
2278.447501	161.234610	47.501492
2274.981287	160.660697	47.506497
2271.611766	162.834263	47.511501
2268.495257	154.783783	47.516506
2264.576513	163.855235	47.521511
2261.237578	153.885216	47.526516
2257.805077	156.427587	47.531521
2254.442162	161.748763	47.536525
2251.129295	158.226924	47.541530
2247.311743	158.273245	47.546535
2243.761469	144.392922	47.551540
2240.023644	154.984492	47.556545
2236.739510	150.932007	47.561549
2233.310860	154.690334	47.566554
2229.680131	163.398368	47.571559
2226.236214	160.799293	47.576564
2222.493998	156.912292	47.581569
2218.876360	151.600023	47.586573
2215.845049	149.673013	47.591578
2212.141918	163.033008	47.596583
2208.664180	158.605513	47.601588
2205.139154	160.259652	47.606593
2201.687565	149.870268	47.611597
2198.359487	151.708461	47.616602
2194.975801	152.909200	47.621607
2191.705412	146.165976	47.626612
2187.886144	155.299153	47.631617
2184.050703	156.086926	47.636621
2180.797188	159.493835	47.641626
2177.386388	148.440786	47.646631
2173.801591	154.772828	47.651636
2169.921399	153.878835	47.656641
2166.420994	154.246443	47.661645
2163.371103	145.925918	47.666650
2159.736692	155.524003	47.671655
2156.370460	152.963033	47.676660
2152.600373	152.508239	47.681665
2149.134128	156.804680	47.686669
2146.317937	149.801736	47.691674
2142.097841	158.516506	47.696679
2138.870174	139.334902	47.701684
2135.131628	162.441103	47.706689
2131.821445	155.043839	47.711693
2128.217400	156.476305	47.716698
2124.575183	158.935916	47.721703
2121.230446	154.799833	47.726708
2117.786782	151.799036	47.731713
2114.216629	147.918956	47.736717
2110.785662	152.511110	47.741722
2107.175894	152.073604	47.746727
2103.663247	155.217436	47.751732
2100.376333	148.110576	47.756737
2096.721966	155.487060	47.761741
2093.201116	153.160936	47.766746
2089.611609	149.848464	47.771751
2086.644299	153.700966	47.776756
2082.897733	158.841338	47.781761
2079.109993	153.256446	47.786765
2075.617580	147.011676	47.791770
2071.977831	152.462329	47.796775
2068.823527	140.833689	47.801780
2065.201187	152.314003	47.806785
2061.570184	143.657290	47.811789
2058.612484	141.573358	47.816794
2054.631199	146.744157	47.821799
2051.048697	144.630754	47.826804
2047.646858	147.726670	47.831809
2044.183364	147.214860	47.836813
2040.927768	157.010555	47.841818
2037.522450	146.961365	47.846823
2033.946366	157.700152	47.851828
2030.309944	142.135460	47.856833
2026.426739	147.577353	47.861837
2023.144904	145.604188	47.866842
2019.655916	148.093750	47.871847
2016.225092	142.379333	47.876852
2012.741386	144.024418	47.881857
2009.146501	153.402947	47.886861
2005.735343	143.580115	47.891866
2001.744704	145.705657	47.896871
1998.442440	142.057562	47.901876
1995.181408	149.279750	47.906881
1991.731872	143.566285	47.911885
1988.632385	138.100292	47.916890
1984.729081	148.955298	47.921895
1981.553224	140.353286	47.926900
1977.754230	142.707772	47.931905
1974.209803	145.627475	47.936909
1971.095201	145.988543	47.941914
1966.674453	153.294797	47.946919
1963.712293	143.731883	47.951924
1960.063975	142.830450	47.956929
1956.561062	138.398675	47.961933
1953.241391	140.768274	47.966938
1949.725365	145.898771	47.971943
1946.377727	140.642854	47.976948
1942.768558	144.646617	47.981953
1938.889587	142.196064	47.986957
1935.785238	133.420036	47.991962
1932.301537	146.496604	47.996967
1928.938355	137.595542	48.001972
1925.428522	141.311521	48.006977
1921.783316	138.670691	48.011981
1918.304795	146.157886	48.016986
1914.490231	138.779885	48.021991
1911.434666	136.190924	48.026996
1908.015334	136.626618	48.032001
1904.111466	142.762912	48.037005
1900.637739	131.725501	48.042010
1896.485143	141.230878	48.047015
1893.340163	138.270961	48.052020
1889.942641	131.292935	48.057025
1886.716583	143.831917	48.062029
1883.421554	139.939604	48.067034
1879.854328	134.024340	48.072039
1876.640743	132.248765	48.077044
1872.991652	142.419798	48.082049
1869.056000	147.180246	48.087053
1865.747376	136.679681	48.092058
1861.554442	143.047840	48.097063
1858.628068	136.879561	48.102068
1855.096330	137.909950	48.107073
1851.568895	138.449251	48.112077
1848.311671	135.698600	48.117082
1844.511974	146.473796	48.122087
1840.993124	138.024860	48.127092
1837.836311	131.758831	48.132097
1834.216051	145.852866	48.137101
1830.501421	142.964131	48.142106
1826.956489	139.786989	48.147111
1823.562850	138.280470	48.152116
1820.224149	141.081348	48.157121
1816.754896	136.016992	48.162125
1813.635628	133.750456	48.167130
1809.617006	139.319178	48.172135
1806.207412	131.168892	48.177140
1802.542092	128.943543	48.182145
1798.758060	127.427757	48.187149
1795.296153	129.304434	48.192154
1792.091344	135.601615	48.197159
1788.693368	129.971948	48.202164
1785.274899	131.474787	48.207169
1781.630287	133.811162	48.212173
1778.274572	133.182850	48.217178
1774.337365	135.031969	48.222183
1770.936345	134.359076	48.227188
1767.465352	140.696059	48.232193
1763.975105	131.427270	48.237197
1760.422619	129.947335	48.242202
1756.758527	135.766955	48.247207
1753.753051	127.136314	48.252212
1750.080757	132.818967	48.257217
1746.487603	131.414852	48.262221
1743.415718	129.403763	48.267226
1739.614883	129.924744	48.272231
1736.074182	124.365357	48.277236
1732.907464	127.787812	48.282241
1729.061146	125.700084	48.287245
1725.646026	124.481768	48.292250
1722.028819	132.265802	48.297255
1718.328921	132.578854	48.302260
1715.102088	129.643505	48.307265
1711.354846	130.416701	48.312269
1708.028255	127.952555	48.317274
1704.467345	131.601208	48.322279
1701.152976	124.342383	48.327284
1697.379742	141.256327	48.332289
1693.926126	137.216222	48.337293
1690.660399	123.079147	48.342298
1687.041634	127.601729	48.347303
1683.601847	126.505939	48.352308
1679.942707	138.700872	48.357313
1676.767740	132.556390	48.362317
1673.377867	126.999683	48.367322
1669.504012	140.211960	48.372327
1665.885924	130.984984	48.377332
1662.895007	139.716832	48.382337
1659.166112	134.627389	48.387341
1655.426184	131.877994	48.392346
1651.575067	117.261602	48.397351
1648.338860	128.168881	48.402356
1645.058432	131.441731	48.407361
1641.237617	131.479097	48.412365
1638.305198	121.845234	48.417370
1634.536621	141.905144	48.422375
1631.425973	122.774326	48.427380
1627.844183	126.617919	48.432385
1623.900097	126.552997	48.437389
1620.037390	128.592377	48.442394
1616.672805	129.896192	48.447399
1613.030524	126.172394	48.452404
1610.257385	126.755562	48.457409
1606.694796	130.079764	48.462413
1603.058003	120.439978	48.467418
1599.414052	133.672402	48.472423
1595.779717	132.525670	48.477428
1592.368612	128.934452	48.482433
1588.722002	133.723599	48.487437
1585.899089	116.838148	48.492442
1582.219645	127.225384	48.497447
1578.777864	118.828264	48.502452
1574.787054	130.423514	48.507457
1571.164107	130.726704	48.512461
1567.968279	120.069000	48.517466
1564.205379	122.086554	48.522471
1561.019270	112.908045	48.527476
1557.402852	127.885098	48.532481
1553.694324	123.748272	48.537485
1550.408563	121.867520	48.542490
1546.958262	114.349785	48.547495
1543.562386	121.927750	48.552500
1540.011905	125.973427	48.557505
1536.615184	125.291734	48.562509
1533.101071	118.541564	48.567514
1529.293582	118.575051	48.572519
1525.990873	118.589365	48.577524
1522.411603	128.159061	48.582529
1518.711240	123.934286	48.587533
1515.396152	123.770298	48.592538
1511.781643	128.074270	48.597543
1508.352620	112.781247	48.602548
1504.896899	111.569659	48.607553
1501.139988	119.231996	48.612557
1497.948330	115.741227	48.617562
1494.349151	123.741890	48.622567
1490.892957	121.485115	48.627572
1487.111572	118.887604	48.632577
1483.533419	122.391105	48.637581
1480.267761	127.480657	48.642586
1476.608904	131.276185	48.647591
1473.384655	131.653846	48.652596
1470.028114	120.841140	48.657601
1466.396524	127.721217	48.662605
1462.805901	118.089705	48.667610
1458.951707	131.715658	48.672615
1455.890653	122.837757	48.677620
1452.210239	123.695424	48.682625
1448.428946	121.717365	48.687629
1445.574954	116.763256	48.692634
1442.025819	120.671645	48.697639
1438.473930	119.771473	48.702644
1434.749453	114.828343	48.707649
1431.394109	123.492309	48.712653
1428.158905	111.790667	48.717658
1423.916006	133.409979	48.722663
1420.403010	119.483887	48.727668
1417.563058	118.624709	48.732673
1413.987421	123.646928	48.737677
1410.772608	119.806647	48.742682
1406.767974	128.426770	48.747687
1403.206524	120.885373	48.752692
1399.702693	128.671784	48.757697
1395.848644	122.913683	48.762701
1392.906941	111.902606	48.767706
1389.078284	124.741948	48.772711
1385.880906	116.073400	48.777716
1382.407564	122.240578	48.782721
1378.810987	135.376516	48.787725
1375.621974	114.956162	48.792730
1371.758039	122.957820	48.797735
1368.230359	121.750986	48.802740
1364.769540	125.063252	48.807745
1361.057718	127.242427	48.812749
1357.963977	117.066253	48.817754
1353.898368	114.402748	48.822759
1350.682213	117.539664	48.827764
1347.314091	118.702209	48.832769
1343.326777	120.767255	48.837773
1340.553422	115.560093	48.842778
1336.732817	123.853358	48.847783
1333.323903	114.639984	48.852788
1330.337919	118.760726	48.857793
1325.997014	121.920441	48.862797
1322.562834	119.391990	48.867802
1318.596774	122.728704	48.872807
1315.844701	123.557024	48.877812
1312.542524	115.579228	48.882817
1308.725079	111.236346	48.887821
1305.269057	117.074519	48.892826
1301.543066	125.409151	48.897831
1298.242553	121.823337	48.902836
1294.737295	114.011855	48.907841
1290.940531	124.239610	48.912845
1288.037092	111.733988	48.917850
1284.228373	118.114745	48.922855
1280.387720	119.727311	48.927860
1277.010767	116.525974	48.932865
1273.587874	116.576025	48.937869
1270.086879	120.482693	48.942874
1266.693474	114.302981	48.947879
1263.177842	111.427964	48.952884
1259.738223	115.130874	48.957889
1256.086352	120.033659	48.962893
1252.583535	108.585754	48.967898
1249.186037	124.542984	48.972903
1245.574551	118.398087	48.977908
1242.395852	116.686515	48.982913
1238.580989	126.311901	48.987917
1235.246212	116.892342	48.992922
1231.277908	134.464940	48.997927
1228.170598	112.218088	49.002932
1224.684331	116.699945	49.007937
1221.069823	117.821579	49.012941
1217.682937	110.262264	49.017946
1214.064391	121.895128	49.022951
1210.538003	125.416525	49.027956
1207.362592	113.093635	49.032961
1203.532872	119.385795	49.037965
1200.260123	110.001370	49.042970
1196.495994	119.792420	49.047975
1193.024724	116.955691	49.052980
1189.841734	110.812774	49.057985
1185.976746	123.893140	49.062989
1182.758316	112.772263	49.067994
1178.934236	113.416035	49.072999
1175.639918	119.736015	49.078004
1171.943468	114.189395	49.083009
1168.736015	113.566803	49.088013
1165.259669	110.417183	49.093018
1161.316111	109.897193	49.098023
1157.711378	117.607198	49.103028
1154.672419	109.403347	49.108033
1150.911246	111.532098	49.113037
1147.480426	112.524655	49.118042
1144.174528	115.440810	49.123047
1140.372485	116.403011	49.128052
1137.031515	107.465086	49.133057
1133.515684	114.347940	49.138061
1130.200908	110.398986	49.143066
1126.548644	119.958021	49.148071
1123.107748	115.098390	49.153076
1119.666641	114.835471	49.158081
1115.924341	109.733807	49.163085
1112.597080	103.208198	49.168090
1108.548400	106.249406	49.173095
1105.270216	115.325276	49.178100
1102.309156	108.632153	49.183105
1098.552213	113.594148	49.188109
1095.444373	102.942029	49.193114
1091.584645	120.016797	49.198119
1087.947986	113.727446	49.203124
1084.060377	115.826132	49.208129
1080.663363	113.805983	49.213133
1077.491702	114.129066	49.218138
1073.823696	113.560875	49.223143
1070.502118	107.661286	49.228148
1067.240973	109.653270	49.233153
1063.258845	113.762693	49.238157
1059.776268	111.017554	49.243162
1056.225168	116.858686	49.248167
1052.667871	114.542324	49.253172
1049.778418	113.695776	49.258177
1046.000764	110.814124	49.263181
1042.888742	107.107672	49.268186
1039.063187	108.017632	49.273191
1035.532759	117.839301	49.278196
1032.407643	111.626536	49.283201
1028.539388	116.597399	49.288205
1024.772918	109.018973	49.293210
1020.966767	114.668819	49.298215
1017.795776	116.416581	49.303220
1014.655373	108.653362	49.308225
1010.667916	117.190288	49.313229
1007.204764	109.384733	49.318234
1004.191316	116.867684	49.323239
1000.576632	116.299002	49.328244
996.941847	108.591797	49.333249
993.479737	109.407544	49.338253
989.979970	114.435885	49.343258
986.427466	117.327583	49.348263
982.611006	119.964131	49.353268
979.402812	109.184125	49.358273
975.465473	115.517639	49.363277
972.152773	117.447612	49.368282
968.729833	113.722967	49.373287
965.428483	108.595635	49.378292
962.148085	105.345408	49.383297
958.325368	116.502454	49.388301
955.041796	105.912385	49.393306
951.675449	97.476529	49.398311
947.863750	114.422866	49.403316
944.440827	107.544475	49.408321
941.065445	110.861863	49.413325
937.608253	96.120738	49.418330
933.932930	105.149378	49.423335
930.198623	105.505386	49.428340
926.849997	99.978250	49.433345
922.881398	108.959083	49.438349
919.643428	96.686923	49.443354
916.032074	102.385042	49.448359
912.669272	105.758973	49.453364
909.422318	105.622672	49.458369
905.962070	120.359793	49.463373
902.371697	106.725735	49.468378
899.031085	116.166729	49.473383
895.388125	109.783310	49.478388
891.958390	110.622387	49.483393
888.380911	113.169039	49.488397
884.691982	108.785726	49.493402
881.333491	110.873941	49.498407
877.748447	113.347069	49.503412
874.439961	119.400869	49.508417
870.401672	117.292983	49.513421
867.242752	106.018482	49.518426
863.748043	108.983771	49.523431
860.168803	110.106791	49.528436
856.826429	112.220175	49.533441
853.071196	123.862012	49.538445
849.580006	112.788112	49.543450
846.546556	111.575101	49.548455
843.165936	114.642830	49.553460
839.526595	110.162334	49.558465
836.023963	107.862759	49.563469
832.229882	101.779574	49.568474
828.424186	110.377467	49.573479
824.964503	111.948547	49.578484
822.037918	101.747294	49.583489
818.394824	111.480292	49.588493
814.790619	105.041980	49.593498
811.479707	110.337094	49.598503
807.518318	102.280960	49.603508
804.310101	114.705809	49.608513
800.383290	114.128551	49.613517
797.308287	106.339675	49.618522
793.793064	111.265967	49.623527
790.305980	119.662612	49.628532
787.167777	90.910603	49.633537
783.092933	105.921710	49.638541
779.616024	106.919283	49.643546
775.935429	106.394908	49.648551
772.259425	115.377235	49.653556
769.505220	107.823230	49.658561
765.776700	109.572785	49.663565
762.284321	106.976171	49.668570
758.745679	107.924220	49.673575
755.079496	102.418195	49.678580
751.935146	103.343216	49.683585
748.077211	106.917493	49.688589
744.612165	95.171209	49.693594
741.353296	102.471903	49.698599
737.787251	101.208089	49.703604
734.052406	102.522423	49.708609
730.537119	105.327066	49.713613
727.193325	106.970357	49.718618
723.377027	102.762079	49.723623
719.722204	108.417073	49.728628
716.470041	109.790602	49.733633
713.147904	103.221696	49.738637
709.710341	102.319202	49.743642
706.542368	102.163252	49.748647
702.479573	112.200464	49.753652
699.335250	104.603548	49.758657
695.277113	113.766604	49.763661
691.822636	100.430685	49.768666
688.476157	104.075005	49.773671
685.090471	106.839423	49.778676
681.762917	114.520190	49.783681
677.949229	118.452255	49.788685
674.444503	113.230298	49.793690
671.302179	109.946354	49.798695
667.555171	113.612009	49.803700
664.368100	106.251719	49.808705
660.314082	108.977555	49.813709
657.122512	106.555459	49.818714
653.530862	107.332835	49.823719
649.836960	111.025208	49.828724
646.859889	110.403084	49.833729
643.221494	106.590400	49.838733
639.371501	109.657902	49.843738
635.815656	101.100097	49.848743
632.565589	108.100459	49.853748
629.418934	97.967890	49.858753
625.464360	104.653284	49.863757
622.169174	98.015859	49.868762
618.668410	113.170169	49.873767
614.627921	116.240322	49.878772
611.234893	100.629309	49.883777
607.858025	111.706112	49.888781
604.730985	99.594424	49.893786
601.292101	103.011839	49.898791
597.518168	109.920442	49.903796
594.420251	99.272866	49.908801
590.276476	106.346490	49.913805
586.787454	105.332085	49.918810
583.560480	101.956112	49.923815
580.203968	100.618975	49.928820
576.733627	98.021840	49.933825
572.661405	115.613019	49.938829
569.593194	89.766990	49.943834
566.053267	100.736909	49.948839
561.897799	108.318661	49.953844
558.995639	94.132818	49.958849
555.804054	97.625826	49.963853
552.639420	103.585543	49.968858
548.877187	99.827267	49.973863
544.820612	107.673809	49.978868
541.272040	96.026658	49.983873
537.719826	100.572149	49.988877
534.542893	98.628825	49.993882
530.949454	98.159282	49.998887
527.392789	99.371608	50.003892
524.039621	96.234700	50.008897
520.295730	98.920028	50.013901
516.984225	105.033813	50.018906
513.555572	98.972763	50.023911
509.743561	106.817399	50.028916
506.825338	98.151263	50.033921
502.997425	97.678067	50.038925
499.501579	104.414674	50.043930
495.815461	99.253020	50.048935
492.277208	96.552792	50.053940
488.901216	86.166601	50.058945
485.284553	94.981448	50.063949
481.664837	108.056208	50.068954
478.386846	94.756525	50.073959
474.789185	97.513117	50.078964
471.389733	103.200116	50.083969
468.020228	106.486345	50.088973
464.465864	102.035925	50.093978
460.978218	104.900550	50.098983
457.510420	104.832103	50.103988
454.124755	100.546663	50.108993
450.126523	104.167624	50.113997
446.752623	100.193599	50.119002
443.096408	101.031627	50.124007
439.663686	112.181971	50.129012
436.497294	101.026343	50.134017
432.763416	102.481311	50.139021
429.117382	99.221656	50.144026
425.891354	96.680775	50.149031
422.086695	104.341541	50.154036
419.002813	88.924876	50.159041
415.578987	93.726597	50.164045
411.697085	99.318161	50.169050
408.821096	109.318353	50.174055
404.985365	98.755431	50.179060
401.612166	96.193040	50.184065
397.846416	97.367405	50.189069
394.498536	92.953599	50.194074
390.746632	92.414613	50.199079
386.839481	104.662823	50.204084
384.061944	96.113728	50.209089
380.357438	112.522757	50.214093
376.960471	94.112527	50.219098
373.412313	95.127832	50.224103
369.515044	96.362552	50.229108
365.920697	97.256088	50.234113
362.817177	100.830132	50.239117
359.550664	99.509029	50.244122
356.182607	97.076263	50.249127
352.227471	92.591306	50.254132
349.061240	94.371580	50.259137
345.299102	101.107172	50.264141
341.853944	91.563382	50.269146
338.553480	97.858008	50.274151
334.550900	102.265386	50.279156
331.143723	91.766134	50.284161
327.588686	99.539829	50.289165
323.905173	98.148721	50.294170
320.502059	95.242297	50.299175
316.900319	94.845578	50.304180
313.608791	94.406992	50.309185
309.958794	99.267497	50.314189
306.883459	94.606032	50.319194
303.734794	99.498689	50.324199
299.828123	89.594334	50.329204
296.260369	97.174219	50.334209
292.534485	97.731326	50.339213
289.297245	95.014438	50.344218
285.753618	83.951047	50.349223
282.103900	97.285506	50.354228
278.426621	95.934650	50.359233
275.113313	94.476755	50.364237
271.700719	96.236065	50.369242
268.590841	93.839022	50.374247
264.824359	100.270930	50.379252
261.509760	87.113520	50.384257
257.780893	101.337498	50.389261
253.766814	89.629482	50.394266
250.678974	89.166779	50.399271
246.632001	97.202050	50.404276
243.710700	94.136712	50.409281
240.168104	97.976403	50.414285
236.916536	95.482559	50.419290
233.041482	88.256333	50.424295
229.421197	98.966777	50.429300
226.423712	90.066414	50.434305
222.849669	105.363042	50.439309
219.292759	86.828222	50.444314
215.554166	94.833593	50.449319
212.273907	95.960426	50.454324
208.734878	93.795570	50.459329
205.019102	99.207789	50.464333
201.459858	100.432691	50.469338
198.093794	89.200767	50.474343
194.305180	100.881468	50.479348
191.263455	87.770545	50.484353
187.669768	94.669702	50.489357
184.377708	97.250480	50.494362
181.032351	90.615306	50.499367
176.675481	99.316041	50.504372
173.798196	94.311184	50.509377
169.755347	96.967010	50.514381
166.491333	89.518947	50.519386
163.423067	93.115114	50.524391
159.327565	95.451737	50.529396
156.254714	92.139340	50.534401
152.570787	92.237926	50.539405
149.000657	99.180959	50.544410
145.817194	85.888018	50.549415
141.688307	101.139572	50.554420
138.788915	88.389052	50.559425
135.187573	98.681246	50.564429
131.498790	95.022105	50.569434
127.966151	95.643955	50.574439
124.376032	99.499742	50.579444
121.465540	94.760924	50.584449
117.879849	94.989638	50.589453
114.143932	89.572834	50.594458
110.512050	90.108977	50.599463
106.689243	93.683972	50.604468
103.427727	90.052912	50.609473
99.595735	89.272583	50.614477
96.490842	93.706836	50.619482
93.131574	83.983277	50.624487
89.514606	99.639574	50.629492
86.256599	84.175227	50.634497
82.227369	96.194577	50.639501
78.840662	92.729384	50.644506
75.583677	90.394650	50.649511
71.984725	97.198688	50.654516
68.832871	87.382071	50.659521
65.141656	95.998339	50.664525
61.632319	93.747196	50.669530
58.260813	87.987703	50.674535
54.310335	95.955035	50.679540
51.240158	93.417793	50.684545
47.416454	92.734807	50.689549
43.849853	91.008034	50.694554
40.402493	85.519276	50.699559
36.785970	98.069169	50.704564
33.163733	88.123376	50.709569
29.561296	90.096991	50.714573
26.859454	79.957183	50.719578
23.554592	92.343788	50.724583
19.557528	85.982462	50.729588
16.166754	79.750848	50.734593
12.632732	98.907278	50.739597
8.555384	98.128164	50.744602
5.286510	90.990478	50.749607
1.499700	96.934466	50.754612