Fri Jun 17 18:00:19 2022

Number of Points = 9932

Depth (nm)	Load (N)	Time (s)
-0.547250	94.537743	0.000000
-0.209248	100.056380	0.005005
-0.198496	101.354052	0.010010
-0.657115	83.368489	0.015014
-0.615706	75.872971	0.020019
-1.382136	64.109300	0.025024
-1.678398	45.849936	0.030029
-2.158006	37.652507	0.035034
-2.180592	30.108646	0.040038
-2.710448	18.270564	0.045043
-3.010365	17.997425	0.050048
-3.240663	13.081399	0.055053
-3.768412	20.074495	0.060058
-4.554232	15.692228	0.065062
-4.817141	8.175102	0.070067
-4.883963	13.728040	0.075072
-4.919118	0.657120	0.080077
-4.871479	14.992896	0.085082
-4.937312	9.792217	0.090086
-5.697500	6.790746	0.095091
-6.382244	8.829347	0.100096
-6.326198	15.212351	0.105101
-6.482488	3.791305	0.110106
-7.154718	10.168868	0.115110
-6.152084	5.844335	0.120115
-6.708501	8.740510	0.125120
-7.108321	7.635462	0.130125
-7.768667	14.837466	0.135130
-8.117967	18.241872	0.140134
-7.826969	15.498224	0.145139
-8.156219	19.476289	0.150144
-9.056982	7.396374	0.155149
-9.342003	2.759394	0.160154
-9.972658	4.875039	0.165158
-9.460098	8.499276	0.170163
-9.455613	11.313864	0.175168
-9.372209	5.921639	0.180173
-9.355828	15.282617	0.185178
-10.202681	15.346062	0.190182
-10.628098	9.000852	0.195187
-11.329827	10.000971	0.200192
-11.233593	3.993512	0.205197
-11.183047	9.454717	0.210202
-11.665676	14.173198	0.215206
-12.001991	1.106161	0.220211
-12.392199	6.198016	0.225216
-12.527460	4.725770	0.230221
-12.862376	5.495413	0.235226
-12.820290	12.286642	0.240230
-12.797655	-3.781441	0.245235
-12.865641	9.919403	0.250240
-13.823841	1.304473	0.255245
-14.136646	9.100683	0.260250
-14.305446	2.287579	0.265254
-13.862921	9.896281	0.270259
-14.546047	14.958289	0.275264
-14.734652	8.796503	0.280269
-15.240765	4.760237	0.285274
-15.677997	11.231939	0.290278
-15.189760	0.628451	0.295283
-15.536970	14.609150	0.300288
-16.422861	5.265303	0.305293
-16.487771	6.011971	0.310298
-17.086489	8.279581	0.315302
-17.154164	14.174237	0.320307
-17.314967	10.565215	0.325312
-17.007028	9.569850	0.330317
-17.042394	9.907280	0.335322
-17.972812	15.072749	0.340326
-18.318895	5.976215	0.345331
-18.318882	14.290517	0.350336
-18.693593	3.582618	0.355341
-18.544580	13.642983	0.360346
-19.174631	9.791101	0.365350
-19.814687	12.167010	0.370355
-20.116273	11.597170	0.375360
-20.170325	13.444512	0.380365
-20.176784	9.868048	0.385370
-20.394781	5.813888	0.390374
-20.079490	9.943712	0.395379
-20.860609	7.490352	0.400384
-21.517783	8.691644	0.405389
-21.924310	8.866997	0.410394
-22.212514	11.319987	0.415398
-21.986013	7.987772	0.420403
-22.112746	14.026822	0.425408
-22.085567	5.430043	0.430413
-22.001868	5.642704	0.435418
-22.469485	15.743012	0.440422
-23.037398	6.146221	0.445427
-23.576901	9.026760	0.450432
-23.542276	13.716687	0.455437
-23.519528	1.942069	0.460442
-24.448706	11.027273	0.465446
-24.825562	14.118757	0.470451
-25.258134	13.566940	0.475456
-24.799460	9.105889	0.480461
-24.749642	4.495934	0.485466
-25.230209	8.064236	0.490470
-25.458328	12.336283	0.495475
-26.148150	9.747180	0.500480
-26.286654	10.333813	0.505485
-26.573235	24.378046	0.510490
-26.673508	13.941435	0.515494
-26.522923	3.741368	0.520499
-27.168012	11.232686	0.525504
-27.867105	8.024722	0.530509
-28.149313	-0.505433	0.535514
-28.003420	6.293598	0.540518
-28.290783	0.786394	0.545523
-28.234967	3.678089	0.550528
-28.199895	6.094710	0.555533
-28.429253	4.273639	0.560538
-29.358881	8.018010	0.565542
-29.321754	3.171989	0.570547
-29.679746	1.947119	0.575552
-30.050650	4.333148	0.580557
-30.206668	5.935582	0.585562
-30.956118	5.662576	0.590566
-31.087723	4.416455	0.595571
-31.617294	13.025977	0.600576
-31.498966	0.006903	0.605581
-31.619565	10.163780	0.610586
-31.760034	12.138555	0.615590
-31.801030	5.375641	0.620595
-32.003366	9.840731	0.625600
-32.115792	8.889585	0.630605
-32.477702	3.398718	0.635610
-33.250637	13.200502	0.640614
-32.955974	9.304829	0.645619
-33.435179	7.336444	0.650624
-33.301112	4.607042	0.655629
-33.862908	5.262062	0.660634
-34.718890	14.557689	0.665638
-34.873081	6.061307	0.670643
-35.254579	11.754755	0.675648
-35.015438	5.515557	0.680653
-34.937969	4.311444	0.685658
-35.627584	12.634803	0.690662
-35.081730	0.149479	0.695667
-35.577553	15.392527	0.700672
-36.135536	7.409820	0.705677
-36.723123	11.741815	0.710682
-36.665653	15.313825	0.715686
-36.626690	6.725941	0.720691
-37.347802	12.056318	0.725696
-37.499051	15.057221	0.730701
-37.959818	8.142875	0.735706
-38.400204	7.995502	0.740710
-38.435499	0.894013	0.745715
-38.449328	17.100223	0.750720
-38.553827	15.630954	0.755725
-38.238098	15.854379	0.760730
-38.880683	25.044095	0.765734
-39.259518	20.974242	0.770739
-39.453924	15.988317	0.775744
-39.621295	14.706504	0.780749
-40.339077	14.690290	0.785754
-41.063063	19.293398	0.790758
-40.605319	11.071998	0.795763
-41.138082	23.605157	0.800768
-40.839440	13.341995	0.805773
-41.042224	7.333526	0.810778
-41.982458	16.088468	0.815782
-42.055713	11.309533	0.820787
-42.484293	13.710282	0.825792
-42.673062	8.484458	0.830797
-42.726558	10.776684	0.835802
-42.595399	8.933377	0.840806
-42.861909	16.535026	0.845811
-43.864054	4.577156	0.850816
-44.185652	15.571759	0.855821
-44.313373	4.309358	0.860826
-44.271627	10.006254	0.865830
-44.136536	4.118627	0.870835
-44.290315	5.539147	0.875840
-44.789944	13.189608	0.880845
-45.306755	9.549388	0.885850
-45.606811	23.639864	0.890854
-45.656630	1.539237	0.895859
-45.652526	9.716104	0.900864
-46.399911	9.609305	0.905869
-46.796600	6.774349	0.910874
-47.205584	12.043570	0.915878
-47.456270	8.760877	0.920883
-47.466900	18.524948	0.925888
-47.112394	18.670492	0.930893
-47.343611	10.771994	0.935898
-47.616977	16.969997	0.940902
-48.122269	11.203418	0.945907
-48.690989	14.129862	0.950912
-48.849506	8.060757	0.955917
-49.041889	2.259730	0.960922
-49.124678	6.827094	0.965926
-48.838291	-0.841710	0.970931
-49.892241	8.962189	0.975936
-50.028621	0.299069	0.980941
-50.561348	9.952590	0.985946
-50.764467	7.023301	0.990950
-50.666485	3.757834	0.995955
-50.709984	12.918802	1.000960
-51.236165	8.827469	1.005965
-51.793071	10.140363	1.010970
-52.085669	6.887133	1.015974
-52.027834	1.283677	1.020979
-52.175188	3.188558	1.025984
-52.117598	5.931763	1.030989
-52.128883	5.522444	1.035994
-53.177518	6.667653	1.040998
-53.505093	12.389630	1.046003
-53.482247	3.652879	1.051008
-53.671313	4.000072	1.056013
-53.847997	5.366385	1.061018
-54.486131	11.411115	1.066022
-54.741571	11.520313	1.071027
-55.043233	10.842154	1.076032
-55.220374	21.835047	1.081037
-55.192556	4.608568	1.086042
-55.738498	11.020594	1.091046
-55.624612	8.536274	1.096051
-55.452954	17.412450	1.101056
-56.175970	7.246305	1.106061
-56.563443	14.728351	1.111066
-57.075836	13.381349	1.116070
-57.040837	8.561532	1.121075
-57.172109	15.136690	1.126080
-57.393803	11.013686	1.131085
-58.039086	13.875308	1.136090
-58.465255	15.556394	1.141094
-58.456863	9.259846	1.146099
-58.722907	20.658819	1.151104
-58.423715	16.852175	1.156109
-58.682927	5.139228	1.161114
-59.209954	17.681099	1.166118
-59.557867	6.704725	1.171123
-60.140850	16.308591	1.176128
-60.464227	10.584984	1.181133
-60.772796	14.328540	1.186138
-60.703248	13.303141	1.191142
-60.391304	10.904690	1.196147
-60.553625	9.021567	1.201152
-60.865647	14.167324	1.206157
-61.222846	14.076770	1.211162
-61.923201	16.506122	1.216166
-61.665072	11.426231	1.221171
-61.811387	12.089938	1.226176
-62.926808	4.143662	1.231181
-63.263491	10.616609	1.236186
-63.839107	14.179206	1.241190
-63.332665	5.768368	1.246195
-63.605157	22.482483	1.251200
-63.915968	12.404891	1.256205
-63.796322	14.582695	1.261210
-64.316178	15.007174	1.266214
-63.849945	8.821984	1.271219
-64.475906	17.214487	1.276224
-64.792534	10.210870	1.281229
-64.909023	4.605016	1.286234
-65.771898	14.058275	1.291238
-65.999863	7.333743	1.296243
-66.659512	11.595830	1.301248
-66.704656	17.194298	1.306253
-66.403901	7.488441	1.311258
-66.661693	17.249393	1.316262
-66.552072	0.482320	1.321267
-66.617645	18.850381	1.326272
-67.393913	7.144650	1.331277
-67.825787	10.487997	1.336282
-68.514654	11.820659	1.341286
-67.999812	12.989142	1.346291
-68.256789	6.208262	1.351296
-69.134269	12.296727	1.356301
-69.520949	8.096765	1.361306
-69.911115	10.136333	1.366310
-69.888253	11.261885	1.371315
-70.136259	15.772653	1.376320
-70.011246	17.785980	1.381325
-70.043395	12.946145	1.386330
-70.259934	16.032492	1.391334
-70.034881	15.752603	1.396339
-70.497815	11.939846	1.401344
-71.135519	14.239796	1.406349
-71.221517	2.632046	1.411354
-72.242672	14.633678	1.416358
-72.515758	10.898881	1.421363
-72.806923	11.908905	1.426368
-72.694652	22.061609	1.431373
-72.800727	14.718116	1.436378
-73.276227	19.430683	1.441382
-72.749247	13.031946	1.446387
-72.872453	4.851473	1.451392
-73.824576	14.983384	1.456397
-74.106181	4.383547	1.461402
-74.645385	15.671245	1.466406
-74.714215	5.486737	1.471411
-74.886901	17.414815	1.476416
-74.857484	17.538623	1.481421
-74.474444	12.320754	1.486426
-75.860503	17.124893	1.491430
-75.962106	13.216750	1.496435
-75.842985	17.772259	1.501440
-76.058893	13.853912	1.506445
-76.568127	11.638930	1.511450
-77.457005	15.287741	1.516454
-77.430523	16.987117	1.521459
-77.701841	14.412518	1.526464
-77.741720	13.951516	1.531469
-77.475507	13.811795	1.536474
-77.710958	14.626477	1.541478
-77.689533	13.462660	1.546483
-78.469322	9.402637	1.551488
-78.925304	20.928493	1.556493
-79.148936	13.088528	1.561498
-79.618257	17.077053	1.566502
-79.041667	7.248978	1.571507
-79.635665	23.755275	1.576512
-80.388446	13.555010	1.581517
-80.755994	12.620623	1.586522
-80.875743	19.626609	1.591526
-80.757121	7.707595	1.596531
-80.740689	5.176921	1.601536
-81.230956	10.606863	1.606541
-80.971915	7.609432	1.611546
-82.092328	14.121497	1.616550
-82.006311	11.732579	1.621555
-82.458062	9.526000	1.626560
-82.270738	8.337763	1.631565
-82.431196	16.741092	1.636570
-83.561013	9.129121	1.641574
-83.822210	7.820285	1.646579
-83.764136	17.150252	1.651584
-84.009602	14.972526	1.656589
-83.918120	19.931036	1.661594
-84.239401	14.931281	1.666598
-83.885260	9.771890	1.671603
-85.177030	19.824504	1.676608
-85.732967	9.953423	1.681613
-85.598139	13.663527	1.686618
-85.675723	10.051332	1.691622
-85.766804	14.450768	1.696627
-85.774581	17.661459	1.701632
-85.963275	13.992749	1.706637
-86.574646	13.161843	1.711642
-87.236082	7.177331	1.716646
-87.290934	15.053995	1.721651
-87.320470	12.320412	1.726656
-87.520175	8.432723	1.731661
-87.394770	13.979947	1.736666
-88.108504	15.477372	1.741670
-88.266023	14.332646	1.746675
-88.811157	16.813552	1.751680
-88.750480	10.713340	1.756685
-88.801864	11.741322	1.761690
-89.292323	19.731446	1.766694
-89.422057	13.806936	1.771699
-90.168074	24.043710	1.776704
-90.342435	15.250349	1.781709
-90.169389	13.993248	1.786714
-90.221681	8.742177	1.791718
-90.343793	12.002460	1.796723
-91.162184	8.153684	1.801728
-91.521880	9.712429	1.806733
-91.742773	8.911724	1.811738
-92.205775	19.327192	1.816742
-91.845843	10.788762	1.821747
-92.115396	12.912866	1.826752
-93.039636	9.028605	1.831757
-93.487584	8.440874	1.836762
-93.521645	11.928248	1.841766
-93.696894	5.123919	1.846771
-93.633645	18.725591	1.851776
-93.591902	12.607411	1.856781
-93.537244	6.694085	1.861786
-93.906664	17.570544	1.866790
-94.413582	10.654409	1.871795
-94.761155	17.136668	1.876800
-95.315503	10.328463	1.881805
-95.193835	13.872432	1.886810
-95.393196	16.494372	1.891814
-95.931292	13.769557	1.896819
-96.503184	14.093370	1.901824
-96.851064	16.263055	1.906829
-97.024218	8.204154	1.911834
-97.123876	18.909676	1.916838
-96.920791	15.822683	1.921843
-97.012704	12.880238	1.926848
-97.329853	11.545382	1.931853
-97.560305	6.423580	1.936858
-98.342473	9.617966	1.941862
-98.707015	1.637849	1.946867
-98.627898	10.010621	1.951872
-99.175629	7.548081	1.956877
-98.792315	10.122883	1.961882
-99.391555	15.860623	1.966886
-99.852853	13.839148	1.971891
-100.271689	16.050228	1.976896
-100.489448	11.157979	1.981901
-100.027678	7.754486	1.986906
-100.321103	20.235819	1.991910
-100.411084	14.050147	1.996915
-101.209140	17.481458	2.006912
-100.856549	8.626983	2.016909
-100.583390	5.166060	2.026906
-99.914415	10.950565	2.036902
-99.415294	13.197750	2.046899
-99.093492	16.830614	2.056896
-98.039665	13.040749	2.066893
-97.384785	11.775911	2.076890
-97.437102	10.008033	2.086886
-97.216216	10.711730	2.096883
-96.433598	10.706381	2.106880
-95.959851	11.817937	2.116877
-95.059603	9.869972	2.126874
-94.793577	13.078416	2.136870
-94.775423	19.818149	2.146867
-93.466555	18.606413	2.156864
-93.014588	16.643465	2.166861
-93.037818	17.426074	2.176858
-92.890643	14.219832	2.186854
-91.992697	16.423441	2.196851
-91.143703	13.605549	2.206848
-90.478498	12.067716	2.216845
-90.616906	9.163434	2.226842
-90.146595	14.228379	2.236838
-89.532653	8.292998	2.246835
-88.944028	12.615917	2.256832
-87.682423	8.993642	2.266829
-87.444465	11.955033	2.276826
-87.190309	11.450916	2.286822
-87.563039	4.939416	2.296819
-86.432202	13.919691	2.306816
-85.649847	10.236801	2.316813
-85.219028	6.815859	2.326810
-84.255987	7.859514	2.336806
-84.425563	13.210038	2.346803
-84.061422	10.222016	2.356800
-83.461281	10.219738	2.366797
-82.783152	7.667944	2.376794
-82.609370	9.192125	2.386790
-81.358527	12.366473	2.396787
-81.111137	19.573119	2.406784
-80.889756	13.172487	2.416781
-80.456734	10.902289	2.426778
-79.349712	10.049332	2.436774
-79.187375	14.228346	2.446771
-79.176215	12.404471	2.456768
-78.160893	4.868346	2.466765
-77.743697	12.536369	2.476762
-77.754457	10.071429	2.486758
-76.749261	13.099899	2.496755
-76.315586	19.119726	2.506752
-75.751271	17.550259	2.516749
-74.760344	8.044545	2.526746
-74.504871	7.809118	2.536742
-74.806940	11.086313	2.546739
-74.267945	10.839716	2.556736
-73.421888	18.038127	2.566733
-72.409683	13.361921	2.576730
-71.847914	16.628295	2.586726
-71.763380	14.140994	2.596723
-71.659387	13.150102	2.606720
-70.813598	11.512113	2.616717
-70.085948	7.465484	2.626714
-69.870756	13.339063	2.636710
-69.432903	9.861234	2.646707
-68.434113	16.923612	2.656704
-68.373579	10.877705	2.666701
-68.089046	10.702649	2.676698
-67.231126	18.499740	2.686694
-66.780390	23.619318	2.696691
-65.911494	11.921366	2.706688
-65.498451	16.345398	2.716685
-65.501774	10.915495	2.726682
-65.213339	12.821315	2.736678
-64.228690	12.601405	2.746675
-63.983610	19.834321	2.756672
-62.778590	14.396001	2.766669
-62.563762	15.723880	2.776666
-62.513075	16.615320	2.786662
-61.992609	13.521293	2.796659
-61.335135	12.054299	2.806656
-60.782469	11.282827	2.816653
-60.096560	11.774674	2.826650
-59.436313	12.184443	2.836646
-59.331539	11.300314	2.846643
-59.043642	12.121501	2.856640
-57.916450	11.265395	2.866637
-57.214337	14.055980	2.876634
-57.664848	12.219342	2.886630
-57.017759	17.887171	2.896627
-56.493392	14.657548	2.906624
-55.526946	10.473423	2.916621
-54.609194	16.192878	2.926618
-54.826470	13.598272	2.936614
-54.405089	7.667045	2.946611
-53.918314	18.925227	2.956608
-53.030112	10.336970	2.966605
-52.873774	15.657820	2.976602
-52.370252	14.645764	2.986598
-51.514051	17.503008	2.996595
-51.472880	16.846792	3.006592
-50.490522	15.109838	3.016589
-49.802086	9.920002	3.026586
-49.871509	11.047166	3.036582
-49.640914	17.580681	3.046579
-48.680588	13.464356	3.056576
-48.147127	7.037932	3.066573
-47.755588	11.208683	3.076570
-46.661657	10.712374	3.086566
-46.527305	9.746074	3.096563
-46.608257	14.604708	3.106560
-46.042578	8.565325	3.116557
-45.476303	14.083386	3.126554
-44.537696	13.523786	3.136550
-43.488400	12.646846	3.146547
-43.770800	6.801979	3.156544
-43.389342	18.915614	3.166541
-42.886150	10.779012	3.176538
-41.828949	11.039224	3.186534
-41.812253	15.206490	3.196531
-41.507141	7.878126	3.206528
-40.698756	9.795916	3.216525
-40.360383	5.104286	3.226522
-39.769288	10.740524	3.236518
-38.975699	11.768890	3.246515
-38.766461	11.071697	3.256512
-38.514103	5.416730	3.266509
-37.576901	6.725697	3.276506
-37.309196	9.126944	3.286502
-36.366413	18.281550	3.296499
-35.776917	15.500283	3.306496
-35.616368	14.786683	3.316493
-35.418257	8.591848	3.326490
-34.701994	5.738931	3.336486
-33.891590	11.036220	3.346483
-33.657684	8.112527	3.356480
-33.583051	8.835797	3.366477
-32.894376	15.847585	3.376474
-32.101785	14.285624	3.386470
-31.049505	13.798020	3.396467
-31.679813	9.855010	3.406464
-30.863336	14.279363	3.416461
-29.599505	9.544351	3.426458
-29.660508	13.555995	3.436454
-29.323885	16.661034	3.446451
-28.953139	12.150537	3.456448
-27.787897	7.621591	3.466445
-27.609884	14.003609	3.476442
-27.411147	12.305631	3.486438
-26.212064	10.828638	3.496435
-26.239942	11.611625	3.506432
-26.004739	14.406919	3.516429
-25.272317	13.328169	3.526426
-24.716836	13.903348	3.536422
-24.074940	19.007359	3.546419
-23.164452	12.672182	3.556416
-22.996970	11.375947	3.566413
-22.786130	14.669640	3.576410
-22.523860	12.563568	3.586406
-21.741912	2.920706	3.596403
-21.472404	12.531609	3.606400
-20.636565	12.616221	3.616397
-20.179095	15.391563	3.626394
-19.539223	10.169496	3.636390
-18.579424	12.544817	3.646387
-18.740192	18.828639	3.656384
-18.682112	15.568447	3.666381
-17.483082	11.070637	3.676378
-16.641215	12.274932	3.686374
-16.418694	12.581026	3.696371
-16.584898	7.607935	3.706368
-15.760112	12.974562	3.716365
-15.470471	8.390414	3.726362
-14.371303	15.934230	3.736358
-14.024705	18.668531	3.746355
-13.923008	19.933221	3.756352
-13.061306	20.824413	3.766349
-12.269105	14.243744	3.776346
-12.525708	11.724232	3.786342
-11.511041	12.499901	3.796339
-10.794991	19.068712	3.806336
-10.484188	19.177567	3.816333
-10.597689	14.219029	3.826330
-9.731172	24.135950	3.836326
-9.188542	23.172523	3.846323
-8.703245	21.534597	3.856320
-7.749445	19.993463	3.866317
-7.230731	20.770362	3.876314
-7.427694	21.810451	3.886310
-6.711425	19.448328	3.896307
-6.004131	12.796615	3.906304
-5.817336	12.936553	3.916301
-4.721848	23.596064	3.926298
-4.473607	22.338172	3.936294
-4.479857	24.214539	3.946291
-3.725842	26.346863	3.956288
-3.341409	26.746176	3.966285
-2.961344	28.652778	3.976282
-2.163138	49.150924	3.986278
-1.646995	55.126447	3.996275
-1.201693	72.581831	4.006272
-0.968162	76.367701	4.016269
-0.785065	86.591297	4.026266
-0.198044	116.506264	4.036262
0.000000	127.493608	4.041267
0.388078	135.960935	4.046272
0.090803	149.547872	4.051277
0.176634	163.140407	4.056282
0.624470	173.929683	4.061286
0.806005	190.267197	4.066291
0.946038	176.625927	4.071296
1.035636	192.489935	4.076301
0.611975	191.100138	4.081306
1.081611	191.517815	4.086310
0.852843	196.719254	4.091315
1.121814	205.353625	4.096320
1.274835	210.964812	4.101325
1.401370	212.669091	4.106330
1.786718	215.066795	4.111334
1.307619	207.999505	4.116339
1.185451	191.139319	4.121344
1.069248	205.131325	4.126349
1.364363	206.066208	4.131354
1.393330	217.103326	4.136358
1.155019	210.596297	4.141363
1.524117	211.127378	4.146368
1.326114	216.305950	4.151373
1.467514	218.462411	4.156378
1.510780	210.388535	4.161382
1.400961	216.302112	4.166387
1.454324	199.948892	4.171392
1.221639	197.683168	4.176397
1.687001	201.706804	4.181402
1.351870	192.228670	4.186406
1.176691	206.864703	4.191411
1.584446	210.732157	4.196416
1.300785	231.771110	4.201421
1.602842	218.359207	4.206426
1.764288	224.608551	4.211430
1.600664	210.566622	4.216435
1.478860	200.493788	4.221440
1.395469	194.768694	4.226445
1.713717	213.627113	4.231450
1.397076	208.366033	4.236454
1.210496	214.106877	4.241459
1.791218	220.453474	4.246464
1.618489	224.675130	4.251469
1.828603	224.199604	4.256474
1.875680	220.243405	4.261478
1.490438	213.933265	4.266483
1.571342	214.888361	4.271488
1.508267	226.247438	4.276493
1.995961	215.902793	4.281498
2.104298	223.478943	4.286502
1.755735	212.332813	4.291507
1.613228	185.123995	4.296512
1.310906	185.930063	4.301517
1.805503	211.396410	4.306522
1.846869	213.859772	4.311526
1.788259	219.730307	4.316531
2.124610	223.608252	4.321536
1.754387	212.091383	4.326541
1.589961	204.051833	4.331546
1.641294	198.751893	4.336550
1.575605	232.261694	4.341555
1.775260	229.763477	4.346560
1.580358	233.114640	4.351565
1.847531	228.201304	4.356570
2.029770	233.263007	4.361574
1.681963	234.373819	4.366579
1.949427	223.594151	4.371584
1.760585	228.294845	4.376589
1.819237	220.204001	4.381594
1.796294	224.368595	4.386598
1.974505	224.683555	4.391603
2.355654	219.403973	4.396608
1.952420	228.544156	4.401613
1.691272	221.214493	4.406618
2.212068	226.135464	4.411622
1.812444	228.849724	4.416627
2.051446	218.752428	4.421632
2.073466	228.827335	4.426637
1.959381	215.675028	4.431642
1.900663	219.475373	4.436646
1.673945	234.971880	4.441651
2.235356	231.009518	4.446656
1.770077	224.380961	4.451661
1.924377	235.396274	4.456666
1.951483	231.063331	4.461670
1.514088	255.585322	4.466675
1.907159	250.110954	4.471680
1.876661	258.382508	4.476685
2.251389	247.832844	4.481690
2.586244	252.382566	4.486694
2.196922	240.763277	4.491699
2.379421	235.858289	4.496704
2.193186	246.181927	4.501709
2.172363	254.474170	4.506714
2.253612	252.673269	4.511718
2.463180	250.793814	4.516723
2.314131	245.940575	4.521728
2.196835	252.013473	4.526733
2.124391	253.952699	4.531738
2.216379	255.028697	4.536742
2.416519	254.987577	4.541747
2.504329	243.565445	4.546752
2.178517	244.857502	4.551757
2.202382	248.306887	4.556762
2.418258	249.634216	4.561766
2.353401	259.224924	4.566771
2.483901	245.668453	4.571776
2.568003	251.352677	4.576781
2.433616	243.111571	4.581786
2.408670	239.143462	4.586790
2.309197	250.123018	4.591795
2.744039	249.016367	4.596800
2.452171	252.488632	4.601805
2.652622	236.341409	4.606810
2.726505	247.295900	4.611814
2.276024	240.902266	4.616819
2.521248	241.482354	4.621824
2.397066	256.712017	4.626829
2.411342	245.333284	4.631834
2.413867	251.119472	4.636838
2.329197	250.520276	4.641843
2.337224	241.906617	4.646848
2.135081	256.229473	4.651853
2.709377	267.529804	4.656858
2.729293	276.005712	4.661862
2.348169	274.621862	4.666867
2.994828	276.486363	4.671872
2.713337	281.787959	4.676877
2.278838	288.516247	4.681882
2.563250	279.503008	4.686886
2.551143	292.460738	4.691891
2.868447	278.926270	4.696896
2.625908	286.799938	4.701901
2.741547	277.570454	4.706906
2.680666	277.307110	4.711910
2.308407	287.064566	4.716915
2.594467	279.702530	4.721920
2.767682	280.248806	4.726925
2.672224	277.807132	4.731930
2.990344	280.269102	4.736934
2.676383	286.579927	4.741939
2.955494	287.833603	4.746944
2.599347	283.708201	4.751949
2.939201	286.110912	4.756954
2.926414	274.888010	4.761958
2.584690	291.989650	4.766963
2.722101	285.194195	4.771968
3.062807	280.561067	4.776973
2.923817	279.613529	4.781978
2.928436	271.376732	4.786982
2.674152	279.494870	4.791987
2.854727	272.718294	4.796992
2.853078	291.531509	4.801997
3.017859	298.155459	4.807002
3.021142	313.961122	4.812006
2.907315	304.247224	4.817011
3.306328	309.880115	4.822016
2.999354	317.091405	4.827021
3.075804	310.436508	4.832026
3.422354	305.885676	4.837030
3.044241	299.935631	4.842035
3.157007	296.654819	4.847040
2.781174	298.741171	4.852045
3.018256	291.554017	4.857050
3.325909	307.006178	4.862054
3.242274	306.434828	4.867059
3.404371	307.233369	4.872064
3.412101	300.026513	4.877069
3.038980	285.876861	4.882074
3.052662	283.373830	4.887078
2.976049	291.949263	4.892083
2.995726	295.361861	4.897088
3.112938	314.385044	4.902093
3.160511	316.698997	4.907098
3.692701	309.148630	4.912102
3.188413	308.645619	4.917107
2.983428	307.805544	4.922112
3.270105	315.148449	4.927117
3.287933	306.044134	4.932122
3.659001	305.193166	4.937126
3.420371	312.887019	4.942131
3.320308	309.122987	4.947136
3.259896	309.427093	4.952141
3.330513	308.417877	4.957146
3.372800	306.613185	4.962150
3.037301	305.667326	4.967155
3.442964	306.329282	4.972160
3.417362	309.736780	4.977165
3.187432	306.162462	4.982170
3.457865	309.716905	4.987174
3.263657	310.737468	4.992179
3.133938	306.591593	4.997184
3.259052	309.174842	5.002189
3.180725	309.496924	5.007194
3.390112	307.892969	5.012198
3.263733	320.068346	5.017203
3.734444	327.803160	5.022208
3.768518	336.209852	5.027213
3.691747	319.175037	5.032218
3.546454	307.672214	5.037222
3.435546	313.957194	5.042227
3.467482	309.328018	5.047232
3.468685	329.562590	5.052237
3.628177	328.245561	5.057242
3.760138	341.836112	5.062246
3.344285	349.986271	5.067251
3.584681	350.862968	5.072256
3.558347	347.081147	5.077261
3.791709	350.000230	5.082266
3.698215	336.603453	5.087270
3.930410	348.949543	5.092275
3.869139	342.895117	5.097280
3.676065	346.344667	5.102285
3.719990	352.589522	5.107290
4.061506	347.052255	5.112294
3.770740	352.681608	5.117299
3.938057	343.337725	5.122304
3.645213	345.733522	5.127309
3.652130	345.502321	5.132314
3.891969	340.204351	5.137318
3.763691	353.660172	5.142323
4.136372	348.452994	5.147328
3.982222	354.516270	5.152333
3.530625	338.639724	5.157338
3.784202	337.097488	5.162342
3.737833	344.524179	5.167347
3.462659	336.103762	5.172352
3.595948	347.681495	5.177357
3.441941	347.147889	5.182362
3.829800	352.768640	5.187366
3.237939	351.876438	5.192371
3.860625	359.434061	5.197376
4.003274	378.531041	5.202381
3.880665	376.378025	5.207386
3.922805	374.158159	5.212390
3.922216	383.066340	5.217395
4.129785	376.879404	5.222400
4.149114	378.585536	5.227405
3.991775	374.802592	5.232410
4.199900	372.240193	5.237414
4.029965	377.011395	5.242419
4.006455	375.971249	5.247424
3.999998	376.538314	5.252429
3.857144	373.466522	5.257434
4.224181	372.341532	5.262438
4.107662	383.938712	5.267443
4.307943	372.198238	5.272448
4.402065	381.530731	5.277453
4.299784	379.212916	5.282458
4.185221	377.313912	5.287462
4.276363	383.182509	5.292467
4.431093	373.443664	5.297472
4.218104	381.218537	5.302477
4.118324	382.132635	5.307482
4.228046	378.997351	5.312486
4.116904	377.339315	5.317491
4.569752	381.507356	5.322496
4.011274	378.218905	5.327501
4.348404	375.817794	5.332506
4.479654	374.211231	5.337510
4.058184	385.125410	5.342515
4.252413	387.022698	5.347520
4.524195	389.173299	5.352525
4.375699	377.415410	5.357530
4.176305	377.038333	5.362534
4.132268	384.123268	5.367539
4.248512	373.977603	5.372544
4.433180	380.789499	5.377549
4.225804	380.377242	5.382554
4.509698	375.664531	5.387558
4.170639	386.171530	5.392563
4.171451	383.065793	5.397568
4.308654	388.393935	5.402573
4.567299	409.173482	5.407578
4.719219	406.245287	5.412582
4.615134	401.874506	5.417587
4.315238	391.017934	5.422592
4.774415	391.342439	5.427597
4.409129	386.377491	5.432602
4.779334	388.433589	5.437606
4.275890	397.177112	5.442611
4.737346	390.856409	5.447616
4.288560	403.587457	5.452621
4.687695	408.082141	5.457626
4.638825	404.937494	5.462630
4.670943	412.797345	5.467635
4.521663	412.758852	5.472640
4.559486	412.612103	5.477645
4.771819	415.802082	5.482650
4.836674	406.611154	5.487654
4.640296	423.682270	5.492659
4.833767	403.752541	5.497664
4.761015	410.944875	5.502669
4.483707	411.499141	5.507674
4.473674	420.036347	5.512678
4.279816	415.100912	5.517683
4.743347	410.422665	5.522688
4.779320	410.207945	5.527693
4.331648	416.781399	5.532698
4.489209	416.476417	5.537702
4.588875	417.727369	5.542707
4.603237	436.215852	5.547712
4.884059	439.668945	5.552717
4.583988	443.437631	5.557722
5.076834	439.980542	5.562726
4.938341	444.340621	5.567731
5.297584	443.220869	5.572736
4.969595	449.398719	5.577741
5.034117	442.946635	5.582746
4.974208	430.359581	5.587750
4.911361	448.711529	5.592755
5.130807	432.827545	5.597760
4.930995	424.145320	5.602765
4.997734	435.714644	5.607770
5.117972	439.305922	5.612774
4.467067	431.811636	5.617779
5.038211	438.006982	5.622784
4.739730	449.898291	5.627789
4.620685	456.704658	5.632794
4.679107	445.771915	5.637798
4.835458	448.576931	5.642803
5.022128	450.440752	5.647808
4.802365	437.203404	5.652813
4.568208	450.243955	5.657818
5.205103	457.342040	5.662822
5.251055	466.260688	5.667827
5.420133	467.654621	5.672832
5.203064	479.375342	5.677837
5.254247	471.752306	5.682842
5.330165	451.862182	5.687846
4.900105	456.639939	5.692851
5.210356	460.820455	5.697856
5.359615	472.775892	5.702861
5.208704	475.207910	5.707866
5.421547	472.839874	5.712870
5.507496	476.047123	5.717875
5.274316	465.584736	5.722880
5.046112	461.307385	5.727885
4.569063	468.032166	5.732890
4.906464	481.177842	5.737894
5.479264	477.209777	5.742899
5.639569	475.300595	5.747904
5.656241	483.268229	5.752909
5.392048	475.437719	5.757914
5.484294	478.357390	5.762918
5.537514	484.881364	5.767923
5.531715	484.451190	5.772928
5.196095	481.446936	5.777933
5.016008	476.386056	5.782938
5.592904	477.061790	5.787942
5.300586	482.166141	5.792947
5.858802	485.617145	5.797952
5.521205	472.841776	5.802957
5.595226	484.228773	5.807962
5.618471	470.747553	5.812966
5.191113	480.686759	5.817971
5.609778	473.465393	5.822976
5.516036	480.546794	5.827981
5.051566	486.401020	5.832986
5.564199	482.643644	5.837990
5.447721	485.240635	5.842995
5.433871	478.180351	5.848000
5.393942	479.997774	5.853005
5.457624	478.647323	5.858010
5.256979	482.077836	5.863014
4.973878	489.811728	5.868019
5.686754	511.994548	5.873024
5.481103	507.371651	5.878029
5.461687	512.575103	5.883034
5.949902	510.712845	5.888038
5.653186	513.543054	5.893043
5.540978	507.756527	5.898048
5.901930	508.837171	5.903053
5.502369	511.122659	5.908058
6.213446	514.013680	5.913062
5.790405	513.579249	5.918067
6.120021	521.610922	5.923072
6.161784	509.112677	5.928077
5.845274	510.979231	5.933082
5.857526	504.261907	5.938086
5.951900	513.850974	5.943091
5.925699	510.505992	5.948096
6.030137	504.209260	5.953101
5.914458	498.893366	5.958106
5.807686	490.931701	5.963110
5.252393	490.789996	5.968115
5.770902	503.660103	5.973120
5.848574	506.643180	5.978125
5.211331	513.867817	5.983130
5.926232	506.814267	5.988134
5.701735	506.173576	5.993139
5.489295	504.177553	5.998144
5.852204	509.633195	6.003149
5.894325	522.122312	6.008154
6.320590	535.940585	6.013158
6.251605	521.466856	6.018163
6.078281	518.923039	6.023168
6.119186	512.192661	6.028173
5.836814	517.543619	6.033178
5.759320	515.964040	6.038182
5.795767	527.157215	6.043187
6.229626	542.871615	6.048192
6.178234	536.207480	6.053197
6.257523	541.209435	6.058202
6.263577	537.181237	6.063206
6.139821	524.954397	6.068211
5.973594	515.487457	6.073216
6.013487	519.864282	6.078221
5.595428	532.944941	6.083226
6.178747	537.295384	6.088230
6.223305	552.155309	6.093235
6.156411	538.982845	6.098240
6.173571	542.061235	6.103245
6.225787	550.425561	6.108250
6.202831	533.546143	6.113254
5.756441	519.024242	6.118259
5.895972	533.275173	6.123264
6.125403	538.324791	6.128269
6.170578	550.974450	6.133274
6.365985	542.794797	6.138278
6.155062	542.328660	6.143283
5.929691	519.396471	6.148288
5.962320	529.035474	6.153293
5.999315	539.080073	6.158298
6.257112	539.127643	6.163302
6.090483	548.458781	6.168307
6.045760	550.519930	6.173312
6.129756	553.813755	6.178317
6.151025	549.071431	6.183322
6.575592	538.975448	6.188326
5.977194	521.804909	6.193331
5.871333	521.398666	6.198336
6.078014	516.878914	6.203341
6.020708	528.112142	6.208346
6.112306	532.333953	6.213350
6.074024	536.124269	6.218355
6.030236	538.362666	6.223360
6.415616	536.580251	6.228365
5.909278	535.020246	6.233370
6.245898	518.717684	6.238374
6.036219	526.580092	6.243379
6.239831	519.690255	6.248384
6.229495	515.603021	6.253389
5.905713	522.105409	6.258394
6.398581	517.342727	6.263398
6.086707	522.077378	6.268403
5.970537	517.825593	6.273408
6.144746	510.168671	6.278413
5.740572	519.762657	6.283418
5.948827	515.091880	6.288422
6.010274	521.595952	6.293427
6.374491	523.156568	6.298432
5.984564	520.416882	6.303437
6.046431	519.583551	6.308442
5.983223	515.505697	6.313446
6.161720	526.881872	6.318451
6.082416	531.555177	6.323456
6.280889	523.196830	6.328461
6.117604	521.717351	6.333466
5.928630	518.313778	6.338470
5.766069	524.992627	6.343475
6.350818	535.793541	6.348480
6.204266	538.639447	6.353485
6.114320	534.224246	6.358490
6.128943	515.618228	6.363494
6.113348	527.476983	6.368499
6.075211	517.962507	6.373504
5.983060	520.398973	6.378509
5.674722	532.861889	6.383514
5.899162	533.666459	6.388518
5.770612	559.021266	6.393523
6.230996	551.459827	6.398528
5.912738	563.953622	6.403533
6.025609	555.410374	6.408538
6.406266	553.443048	6.413542
6.580883	556.657875	6.418547
6.506332	542.959201	6.423552
6.221128	527.069999	6.428557
5.927567	523.205269	6.433562
5.954528	520.050363	6.438566
5.905026	524.247080	6.443571
5.890453	538.387664	6.448576
6.310306	539.579685	6.453581
6.127965	547.826113	6.458586
6.283545	523.398927	6.463590
6.006977	524.424312	6.468595
6.036854	520.681058	6.473600
6.050948	521.065335	6.478605
5.886731	526.423693	6.483610
6.248849	534.354854	6.488614
6.165681	548.073301	6.493619
5.598181	538.340532	6.498624
5.850186	541.099869	6.503629
6.093606	549.846820	6.508634
6.274385	545.640393	6.513638
6.094333	544.035035	6.518643
6.241025	550.946856	6.523648
6.537024	548.322067	6.528653
5.980123	541.357935	6.533658
6.011634	531.947118	6.538662
6.407821	541.234237	6.543667
6.186011	535.244308	6.548672
6.068604	522.015528	6.553677
5.628521	528.574152	6.558682
6.009099	526.405757	6.563686
6.036176	548.925015	6.568691
6.292547	550.813968	6.573696
6.371403	543.388172	6.578701
5.865857	535.521771	6.583706
6.220275	522.249893	6.588710
5.870225	523.236183	6.593715
5.727757	533.617858	6.598720
6.196581	551.564244	6.603725
6.252413	548.066892	6.608730
6.125645	550.616270	6.613734
5.981852	557.261821	6.618739
6.048180	553.178411	6.623744
6.024219	552.503202	6.628749
5.787060	549.665105	6.633754
6.394115	547.730402	6.638758
5.999867	559.198443	6.643763
5.972494	545.820292	6.648768
6.510631	555.124083	6.653773
6.224119	562.279396	6.658778
6.123171	545.494428	6.663782
6.017217	545.547796	6.668787
5.719915	546.395276	6.673792
6.171815	553.920800	6.678797
5.954007	551.441401	6.683802
6.237830	550.351147	6.688806
6.155586	557.882374	6.693811
6.025617	561.453896	6.698816
6.466873	553.833276	6.703821
6.220487	538.806481	6.708826
5.834376	527.094484	6.713830
5.806106	536.139964	6.718835
5.990275	538.921823	6.723840
6.282147	546.379220	6.728845
6.158160	559.395631	6.733850
6.497900	545.067859	6.738854
6.136747	534.792260	6.743859
5.952607	525.978710	6.748864
6.247623	521.332977	6.753869
5.804383	521.504566	6.758874
6.265777	521.986377	6.763878
6.092183	526.235095	6.768883
6.041378	529.212298	6.773888
6.023585	517.595774	6.778893
5.948917	535.030009	6.783898
6.475639	539.609298	6.788902
6.342805	535.072956	6.793907
6.016544	529.055990	6.798912
6.017318	522.496462	6.803917
5.768877	528.135419	6.808922
5.958271	525.873690	6.813926
5.932318	542.897075	6.818931
6.058238	544.260891	6.823936
6.270779	553.840209	6.828941
6.212369	558.129585	6.833946
6.173360	553.128112	6.838950
6.281111	530.961060	6.843955
6.126976	530.298214	6.848960
6.286437	532.542492	6.853965
5.865852	524.556599	6.858970
6.263906	523.674495	6.863974
5.935410	526.788429	6.868979
6.190831	534.265100	6.873984
6.319099	526.009590	6.878989
6.139432	524.777924	6.883994
6.121566	523.164359	6.888998
6.224626	527.252838	6.894003
6.061821	532.706276	6.899008
6.264071	525.008178	6.904013
6.089322	527.495079	6.909018
6.126432	515.664794	6.914022
5.935460	525.500605	6.919027
5.996631	525.721162	6.924032
6.054422	521.169915	6.929037
5.631487	522.489582	6.934042
5.930767	518.722667	6.939046
6.374133	527.371843	6.944051
5.979086	527.285003	6.949056
6.282102	524.240306	6.954061
5.412644	529.073949	6.959066
6.121552	527.272097	6.964070
6.169725	549.739503	6.969075
5.923523	551.348495	6.974080
6.269742	551.137067	6.979085
5.865417	553.618913	6.984090
6.062361	547.897021	6.989094
6.111867	553.026278	6.994099
6.232177	565.126312	6.999104
6.217348	557.315487	7.004109
6.046856	553.671636	7.009114
6.293738	543.770156	7.014118
5.907315	540.190614	7.019123
6.016333	533.655319	7.024128
6.051412	542.134971	7.029133
5.928543	554.733629	7.034138
6.242400	558.240064	7.039142
5.949458	554.395154	7.044147
6.016506	562.945281	7.049152
6.203420	557.101519	7.054157
6.121921	560.950332	7.059162
6.154428	557.370816	7.064166
6.206824	555.887849	7.069171
6.110470	548.417762	7.074176
6.298907	532.288213	7.079181
5.759608	535.035213	7.084186
5.981322	539.970081	7.089190
6.119190	555.144445	7.094195
5.910447	563.184317	7.099200
6.427627	565.306194	7.104205
6.214413	559.057895	7.109210
6.018575	540.523335	7.114214
5.840011	540.494445	7.119219
6.109213	560.599328	7.124224
6.504265	562.351764	7.129229
6.376266	549.533207	7.134234
6.379894	540.882815	7.139238
6.267363	539.733133	7.144243
6.093841	533.339915	7.149248
5.853177	531.344830	7.154253
5.814082	537.324921	7.159258
5.801704	523.885293	7.164262
5.816959	537.829109	7.169267
6.044653	544.234715	7.174272
6.162443	546.428694	7.179277
6.019971	554.901751	7.184282
6.138289	565.231024	7.189286
6.014088	557.827723	7.194291
6.120998	556.722276	7.199296
6.084749	552.963759	7.204301
5.759924	559.770629	7.209306
6.252173	562.965816	7.214310
6.196899	567.609286	7.219315
6.302828	557.138821	7.224320
5.985074	544.933554	7.229325
6.020753	548.037678	7.234330
5.866611	553.448243	7.239334
5.834319	559.012608	7.244339
5.897006	567.787241	7.249344
6.163327	551.089817	7.254349
6.180462	564.099747	7.259354
6.054759	559.930048	7.264358
6.187231	568.919033	7.269363
6.199699	562.194347	7.274368
6.255619	553.776796	7.279373
6.263450	566.840766	7.284378
6.458323	560.747037	7.289382
6.317089	546.280557	7.294387
6.351403	535.176919	7.299392
6.073860	524.913478	7.304397
5.693564	542.367932	7.309402
6.278524	535.296303	7.314406
6.186362	527.218131	7.319411
5.929254	538.649351	7.324416
6.253466	518.169279	7.329421
5.801068	533.812326	7.334426
6.055914	523.651222	7.339430
5.988744	530.043671	7.344435
6.071188	528.669180	7.349440
6.330757	526.989768	7.354445
6.165486	527.243818	7.359450
6.258811	524.380397	7.364454
6.290786	530.223364	7.369459
5.970594	531.924376	7.374464
6.239207	526.754170	7.379469
6.146860	532.359685	7.384474
6.151993	525.898099	7.389478
6.304228	532.388270	7.394483
6.210234	528.043995	7.399488
6.136081	523.315961	7.404493
6.069125	532.894163	7.409498
6.185623	526.833997	7.414502
6.134083	529.329033	7.419507
5.811262	522.568133	7.424512
6.476702	520.889935	7.429517
6.297978	532.590905	7.434522
6.197813	524.831577	7.439526
6.480342	523.149139	7.444531
6.068915	527.455938	7.449536
6.183006	531.105091	7.454541
5.963438	533.846704	7.459546
5.742559	529.636986	7.464550
6.243694	536.603357	7.469555
5.757650	532.060011	7.474560
5.702213	529.929749	7.479565
5.792509	536.444228	7.484570
6.024633	534.860546	7.489574
6.079267	531.582440	7.494579
6.043132	538.821633	7.499584
6.127750	532.237903	7.504589
6.284465	542.791070	7.509594
5.921464	534.997476	7.514598
6.070504	533.244081	7.519603
5.769799	531.908014	7.524608
6.044214	523.689190	7.529613
5.646989	529.776360	7.534618
5.687747	534.437801	7.539622
5.840071	544.303392	7.544627
5.916803	551.264137	7.549632
6.228516	562.167678	7.554637
5.923868	567.442632	7.559642
5.866689	563.164453	7.564646
6.171001	563.900100	7.569651
6.106811	572.797255	7.574656
6.531204	562.326346	7.579661
6.143254	568.717860	7.584666
6.505866	555.158849	7.589670
6.093910	545.268402	7.594675
5.825356	546.596353	7.599680
6.146559	545.992832	7.604685
5.962075	563.550531	7.609690
6.136147	558.016748	7.614694
6.155525	562.520527	7.619699
5.944713	564.759456	7.624704
6.314143	570.229230	7.629709
6.079321	564.488518	7.634714
6.094148	568.548062	7.639718
6.082789	561.862659	7.644723
6.195760	564.976831	7.649728
5.892450	556.417507	7.654733
5.950144	554.247126	7.659738
6.094283	548.749501	7.664742
6.322712	554.042014	7.669747
6.024354	560.319177	7.674752
6.253106	549.803241	7.679757
6.157374	554.794033	7.684762
5.912127	536.765372	7.689766
6.124500	543.087289	7.694771
6.085595	553.566219	7.699776
6.007836	548.238874	7.704781
5.898246	560.822898	7.709786
6.120764	557.517672	7.714790
6.357782	562.881183	7.719795
5.964535	564.854430	7.724800
6.167947	561.458249	7.729805
5.945056	563.170127	7.734810
6.210777	562.061175	7.739814
6.151120	560.899544	7.744819
5.987691	567.297944	7.749824
6.258313	555.254767	7.754829
6.351079	544.304603	7.759834
6.157232	539.346828	7.764838
5.928716	535.221654	7.769843
5.721373	542.097199	7.774848
6.231494	543.106482	7.779853
6.252522	559.791143	7.784858
6.184583	538.308636	7.789862
6.305520	536.691337	7.794867
6.176477	528.328421	7.799872
6.063380	529.631125	7.804877
6.025625	525.282042	7.809882
5.735016	527.796488	7.814886
5.874043	524.939284	7.819891
5.917322	539.822497	7.824896
6.368897	557.415171	7.829901
6.004094	557.139978	7.834906
5.984610	559.254752	7.839910
6.055352	555.823988	7.844915
6.042199	574.195847	7.849920
6.255573	552.515008	7.854925
6.083675	564.403915	7.859930
6.343838	567.569794	7.864934
5.977979	544.639408	7.869939
6.126200	553.381661	7.874944
6.042507	546.514504	7.879949
5.994162	546.723072	7.884954
6.122891	555.957170	7.889958
6.327147	560.537571	7.894963
6.279253	550.170625	7.899968
6.050940	535.204964	7.904973
5.494440	535.613828	7.909978
5.640743	546.305088	7.914982
6.216346	559.791703	7.919987
6.089886	562.513701	7.924992
6.107320	556.242263	7.929997
5.919141	559.611520	7.935002
6.247153	560.180820	7.940006
6.442352	561.570419	7.945011
6.065159	565.385302	7.950016
5.939224	553.270889	7.955021
5.784929	563.062344	7.960026
6.132503	557.606877	7.965030
6.310664	559.919685	7.970035
5.981029	563.801058	7.975040
6.090302	565.815301	7.980045
5.809666	567.899087	7.985050
5.848537	563.930943	7.990054
5.974266	567.500420	7.995059
5.652033	573.251511	8.000064
6.138165	567.525748	8.005069
5.957180	570.525385	8.010074
5.942972	564.646179	8.015078
6.314111	564.973481	8.020083
5.842510	567.906768	8.025088
6.456780	560.466368	8.030093
5.948202	563.896970	8.035098
6.288085	566.583688	8.040102
6.186341	565.496840	8.045120
5.915831	562.866883	8.050138
6.236130	562.396597	8.055155
6.338992	572.106625	8.060173
5.827719	559.615994	8.065190
5.816523	562.933345	8.070208
5.772796	566.518089	8.075226
5.972990	563.402255	8.080243
6.121608	568.404703	8.085261
6.236507	563.696693	8.090278
6.235805	567.665590	8.095296
6.342735	568.348581	8.100314
6.381120	567.206712	8.105331
6.197798	567.120302	8.110349
5.983289	569.405401	8.115366
6.335859	564.921644	8.120384
6.144438	567.874892	8.125402
6.122295	568.360852	8.130419
6.543275	566.540683	8.135437
5.934571	554.294576	8.140454
6.362233	561.448476	8.145472
6.147089	566.924339	8.150490
6.685783	563.731970	8.155507
6.236040	568.785450	8.160525
6.394584	559.385173	8.165542
6.286715	564.342069	8.170560
5.951214	567.555464	8.175578
6.356263	555.814422	8.180595
6.202055	568.911954	8.185613
5.912775	568.621325	8.190630
6.248985	568.233623	8.195648
6.388708	561.564969	8.200666
6.173926	563.627298	8.205683
6.012768	570.066543	8.210701
6.189182	565.102268	8.215718
6.569208	560.080335	8.220736
6.053018	571.591725	8.225754
6.429489	559.858973	8.230771
6.254975	561.069802	8.235789
6.286448	556.078050	8.240806
6.121162	559.221423	8.245824
6.206443	560.238298	8.250842
6.062162	560.524303	8.255859
6.120565	565.021515	8.260877
6.089301	568.822081	8.265894
6.282823	562.447215	8.270912
6.236483	566.489635	8.275930
6.448527	564.201285	8.280947
6.280152	563.112678	8.285965
6.295356	569.720230	8.290982
6.358674	569.318048	8.296000
6.029318	578.499185	8.301018
6.372179	585.860087	8.306035
6.586211	584.378616	8.311053
6.033854	594.027891	8.316070
6.575025	590.266651	8.321088
6.463379	598.082203	8.326106
6.715331	585.302702	8.331123
6.449488	574.326837	8.336141
5.948228	579.132411	8.341158
6.530750	580.200290	8.346176
6.400330	596.407199	8.351194
6.476626	587.163870	8.356211
6.617857	591.581384	8.361229
6.115766	577.273624	8.366246
6.702248	580.299530	8.371264
6.648870	578.770782	8.376282
6.658671	563.324896	8.381299
6.610247	561.293796	8.386317
6.559598	562.635403	8.391334
6.469352	561.263755	8.396352
6.287694	566.295902	8.401370
6.279221	566.123350	8.406387
6.249295	572.670497	8.411405
6.045440	569.636188	8.416422
6.675594	580.340373	8.421440
6.417861	604.824811	8.426458
6.287786	598.864117	8.431475
6.656629	599.009526	8.436493
6.404599	601.484314	8.441510
6.502057	607.288122	8.446528
6.648725	603.465688	8.451546
6.773185	598.598218	8.456563
7.026516	578.953542	8.461581
6.343609	580.773629	8.466598
6.295380	569.217946	8.471616
6.235597	581.213670	8.476634
6.339658	590.064334	8.481651
6.550175	595.817656	8.486669
6.301201	602.893701	8.491686
6.734684	596.773005	8.496704
6.237048	603.726221	8.501722
6.463866	604.198753	8.506739
6.599478	602.168553	8.511757
6.482744	609.099009	8.516774
6.800529	597.796223	8.521792
6.806092	609.143368	8.526810
6.699413	599.565711	8.531827
6.568642	605.481658	8.536845
6.562931	603.988485	8.541862
6.882267	589.061746	8.546880
6.887309	605.018610	8.551898
6.803741	608.171047	8.556915
6.806283	584.623507	8.561933
6.399052	588.926686	8.566951
6.470357	584.381414	8.571968
6.828509	601.680249	8.576986
6.636973	605.444870	8.582003
6.771472	598.097994	8.587021
6.276101	601.618259	8.592039
6.782065	591.994680	8.597056
6.807803	592.191605	8.602074
6.944391	593.138936	8.607091
6.788480	582.396347	8.612109
6.825051	578.910694	8.617127
6.770475	564.238039	8.622144
6.854311	571.264264	8.627162
6.568001	569.972049	8.632179
6.525341	570.030553	8.637197
6.278878	576.485554	8.642215
6.374079	593.029138	8.647232
6.427345	597.034147	8.652250
6.496032	607.595866	8.657267
6.523176	600.567988	8.662285
6.098892	602.381703	8.667303
6.414822	598.343358	8.672320
6.441803	605.886682	8.677338
6.714702	638.082499	8.682355
6.790742	630.181986	8.687373
6.774892	639.276605	8.692391
7.126751	628.869434	8.697408
6.668345	629.857792	8.702426
6.731306	639.544969	8.707443
6.799412	635.707831	8.712461
6.511390	639.876457	8.717479
7.007578	634.242723	8.722496
6.706992	637.710347	8.727514
6.965080	634.096926	8.732531
6.782820	640.994787	8.737549
6.853685	635.842342	8.742567
6.900549	625.038070	8.747584
6.775201	636.742988	8.752602
7.005535	633.800069	8.757619
6.944608	633.205365	8.762637
6.998041	643.642293	8.767655
7.276772	626.896043	8.772672
6.594905	615.042527	8.777690
6.458135	606.493795	8.782707
6.819762	620.436852	8.787725
6.838674	635.113205	8.792743
7.160864	633.371648	8.797760
6.795822	632.957598	8.802778
6.499938	638.531938	8.807795
6.774480	644.045719	8.812813
6.439833	644.054140	8.817831
6.345706	637.103877	8.822848
6.349772	640.532675	8.827866
6.458867	650.986338	8.832883
6.902863	642.943172	8.837901
6.933198	664.186786	8.842919
7.204652	661.011259	8.847936
7.369982	665.522025	8.852954
7.423664	661.893560	8.857971
7.526795	641.914153	8.862989
7.073985	642.698646	8.868007
7.016155	633.591548	8.873024
6.796603	633.330467	8.878042
6.892372	640.102006	8.883059
7.143905	626.046467	8.888077
6.868331	640.000577	8.893095
7.118411	640.562740	8.898112
7.065070	638.660389	8.903130
6.863459	641.137039	8.908147
6.884027	636.115580	8.913165
6.774845	636.059167	8.918183
6.815258	637.257505	8.923200
7.066307	637.623066	8.928218
6.816875	642.208274	8.933235
7.123592	642.582889	8.938253
6.969855	663.560468	8.943271
6.920308	662.276921	8.948288
7.313237	667.946806	8.953306
7.144497	667.729440	8.958323
7.229686	669.521470	8.963341
7.153616	657.493419	8.968359
7.113214	654.767528	8.973376
6.864671	646.865252	8.978394
7.066771	666.328105	8.983411
7.204535	654.671569	8.988429
6.964083	668.251000	8.993447
7.434138	656.695911	8.998464
7.497095	658.752047	9.003482
7.370930	651.003823	9.008499
7.502762	640.378315	9.013517
6.790384	639.736783	9.018535
7.107304	627.835941	9.023552
7.295258	634.991334	9.028570
7.079616	629.760143	9.033587
7.493248	643.853028	9.038605
6.912220	637.094707	9.043623
6.923627	632.266685	9.048640
7.176129	639.343444	9.053658
7.230515	661.706978	9.058675
7.236629	654.393619	9.063693
7.341967	655.260722	9.068711
7.252296	649.834979	9.073728
7.036400	645.624802	9.078746
6.990832	661.866688	9.083763
7.326002	650.961727	9.088781
7.229265	663.245326	9.093799
7.438029	666.882606	9.098816
7.322528	661.438910	9.103834
7.291170	671.430146	9.108851
7.283486	667.197757	9.113869
6.973284	674.092491	9.118887
7.209236	665.183573	9.123904
7.222343	660.325931	9.128922
7.224034	667.990015	9.133939
7.427217	671.489062	9.138957
7.328099	666.370567	9.143975
7.517451	671.089923	9.148992
7.608869	665.672852	9.154010
6.893829	672.248684	9.159027
7.424129	658.224730	9.164045
7.290148	667.093547	9.169063
7.536949	669.123261	9.174080
7.673130	666.231809	9.179098
7.229803	668.881501	9.184115
7.677631	665.859123	9.189133
7.460365	657.675287	9.194151
7.194434	643.329788	9.199168
7.533131	657.640439	9.204186
6.930698	657.213487	9.209203
7.052859	661.559000	9.214221
7.255578	666.396989	9.219239
7.152702	665.698438	9.224256
7.279412	663.787810	9.229274
7.189152	668.484353	9.234291
7.133142	660.122940	9.239309
7.503623	663.836088	9.244327
7.275658	661.678137	9.249344
7.639624	666.987118	9.254362
7.305489	669.719047	9.259379
7.698773	652.571281	9.264397
7.249251	662.378491	9.269415
7.396394	661.976349	9.274432
7.682088	657.280472	9.279450
7.494684	667.515536	9.284467
7.568470	662.712764	9.289485
7.523969	669.697772	9.294503
7.462882	671.573952	9.299520
7.479186	662.509236	9.304538
7.175029	676.160477	9.309555
7.204240	669.820356	9.314573
7.517544	687.272595	9.319591
7.703467	706.419316	9.324608
7.670992	699.958737	9.329626
7.026680	699.002370	9.334643
7.141107	698.194281	9.339661
7.511800	703.498221	9.344679
7.316604	696.253140	9.349696
7.508643	697.220196	9.354714
7.406654	706.319724	9.359731
7.642875	697.004476	9.364749
7.497797	700.723212	9.369767
7.363187	698.450141	9.374784
7.728527	689.581903	9.379802
7.478189	701.267097	9.384819
7.814771	690.452614	9.389837
7.582816	695.294951	9.394855
7.587589	699.244862	9.399872
7.720755	704.423334	9.404890
7.669417	699.803735	9.409907
7.554043	697.988453	9.414925
7.566288	698.892093	9.419943
7.553848	700.591897	9.424960
7.512275	698.684434	9.429978
7.574948	700.851440	9.434995
7.775487	707.084180	9.440013
7.782809	697.621952	9.445031
7.800294	701.410118	9.450048
7.933484	693.182384	9.455066
7.639487	702.580336	9.460083
7.849543	703.307016	9.465101
7.898968	700.400254	9.470119
7.670883	705.743485	9.475136
7.951262	693.503812	9.480154
7.812307	703.861152	9.485171
7.842629	697.112404	9.490189
7.924068	700.449818	9.495207
7.763277	702.510277	9.500224
7.562586	701.044778	9.505242
7.726699	691.802143	9.510259
7.700972	705.039052	9.515277
7.690964	696.687097	9.520295
7.264237	709.518650	9.525312
7.828881	714.124662	9.530330
7.971712	721.530095	9.535347
7.789975	718.403702	9.540365
7.764829	709.114567	9.545383
7.806670	716.425572	9.550400
8.026579	713.681402	9.555418
7.819614	713.764459	9.560435
7.817779	711.491953	9.565453
8.012186	715.873895	9.570471
7.580995	716.049925	9.575488
7.834452	719.135345	9.580506
7.836367	730.280445	9.585523
7.853713	734.596553	9.590541
8.035171	730.905303	9.595559
7.929805	739.709765	9.600576
8.136471	726.792017	9.605594
8.235935	741.334618	9.610611
7.966776	720.100753	9.615629
8.081646	702.706907	9.620647
7.718304	704.170570	9.625664
7.758492	709.211163	9.630682
7.979520	727.691695	9.635699
8.089713	737.118938	9.640717
8.190864	713.773299	9.645735
7.908200	707.908587	9.650752
8.025727	698.584722	9.655770
8.271097	698.964417	9.660787
7.801518	696.823787	9.665805
7.941987	697.622066	9.670823
7.793617	705.055618	9.675840
8.019628	709.617723	9.680858
7.928721	728.982124	9.685875
7.998475	730.289363	9.690893
8.200316	727.227943	9.695911
7.991734	742.811039	9.700928
8.195311	731.072449	9.705946
8.170810	736.721393	9.710963
7.881649	737.836340	9.715981
8.338045	741.569673	9.720999
7.770529	727.067939	9.726016
8.282916	726.182091	9.731034
8.254417	727.067113	9.736051
8.032766	722.980302	9.741069
8.276397	721.218921	9.746087
7.679918	727.682559	9.751104
7.685758	726.831891	9.756122
7.755920	732.931796	9.761139
7.929249	732.325316	9.766157
8.119291	726.134017	9.771175
7.838636	736.642677	9.776192
7.989436	731.654852	9.781210
8.084517	725.464181	9.786227
7.725779	731.093092	9.791245
7.964268	737.759659	9.796263
7.923709	748.321720	9.801280
8.452196	762.832008	9.806298
8.350722	757.780798	9.811315
8.189204	766.990838	9.816333
8.304700	748.012116	9.821351
8.268544	745.855340	9.826368
8.260346	731.259851	9.831386
8.202681	741.956827	9.836403
8.143714	743.803532	9.841421
8.302308	754.065391	9.846439
8.274670	768.287438	9.851456
8.383311	753.009961	9.856474
8.274211	740.096460	9.861491
7.990541	744.668099	9.866509
8.348203	755.075598	9.871527
8.323686	769.026478	9.876544
8.643096	753.992687	9.881562
8.267793	742.382191	9.886579
8.224032	763.206794	9.891597
8.310173	760.374622	9.896615
8.291221	770.986056	9.901632
8.642666	762.484035	9.906650
8.356877	755.305162	9.911667
7.908564	742.906665	9.916685
8.632920	758.909079	9.921703
8.476033	761.419255	9.926720
8.414100	759.484265	9.931738
8.562269	748.617010	9.936755
8.177087	749.746736	9.941773
8.554483	737.257259	9.946791
8.390076	735.882372	9.951808
8.250519	740.785541	9.956826
8.343981	746.914646	9.961843
8.271452	768.674281	9.966861
8.549426	775.995669	9.971879
8.331830	770.538985	9.976896
8.356960	768.473587	9.981914
8.559033	771.428789	9.986931
8.472622	775.067325	9.991949
8.736361	768.943675	9.996967
8.809519	773.050139	10.001984
8.228818	753.376556	10.007002
8.651163	752.044094	10.012019
8.330793	766.701575	10.017037
8.708853	767.530442	10.022055
8.574802	763.772932	10.027072
8.376586	757.601078	10.032090
8.590067	756.957414	10.037107
8.303328	765.224560	10.042125
8.640571	763.916280	10.047143
8.511117	763.060344	10.052160
8.203722	761.560806	10.057178
8.710760	764.325566	10.062195
8.600050	774.223175	10.067213
8.631243	773.794046	10.072231
8.665587	768.271474	10.077248
8.902430	775.841806	10.082266
8.795514	766.939821	10.087283
8.341061	776.892597	10.092301
8.516833	772.586580	10.097319
8.460390	765.834705	10.102336
8.472376	770.633174	10.107354
8.497148	765.607431	10.112371
8.215115	768.336426	10.117389
8.419859	763.741366	10.122407
8.668599	763.790606	10.127424
8.416813	770.983524	10.132442
8.973665	766.711604	10.137459
8.579000	768.838500	10.142477
8.669362	756.428603	10.147495
8.612180	770.214061	10.152512
8.546630	768.983161	10.157530
8.498631	766.307918	10.162547
8.477903	774.198598	10.167565
8.633742	776.856981	10.172583
8.746947	774.400397	10.177600
8.898708	796.926668	10.182618
8.939496	778.457139	10.187635
8.656743	774.954049	10.192653
8.649715	767.180651	10.197671
8.507273	779.637280	10.202688
8.693245	781.204123	10.207706
9.103438	791.918050	10.212723
8.788684	787.243986	10.217741
9.020418	790.777683	10.222759
8.975669	794.000274	10.227776
8.580222	781.396911	10.232794
9.074884	786.679684	10.237811
8.776139	776.210879	10.242829
8.688228	788.807260	10.247847
8.865519	788.247950	10.252864
8.532852	797.346504	10.257882
8.993701	790.197836	10.262899
8.530755	793.600163	10.267917
8.722748	793.683244	10.272935
8.868911	787.129360	10.277952
8.577666	801.267898	10.282970
8.976649	794.906815	10.287987
8.912200	799.329246	10.293005
8.990102	793.703566	10.298023
9.148580	793.318630	10.303040
9.044614	789.176811	10.308058
9.051327	793.370500	10.313075
8.812338	796.451964	10.318093
8.682880	800.695254	10.323111
8.836383	799.572223	10.328128
8.873138	801.856338	10.333146
9.102806	788.148751	10.338163
8.604372	796.300126	10.343181
8.997898	802.345722	10.348199
9.035555	794.986898	10.353216
8.649266	800.657812	10.358234
9.169765	787.803788	10.363251
8.557561	799.624786	10.368269
9.114200	816.048806	10.373287
9.207485	823.720576	10.378304
9.142886	826.142004	10.383322
9.298962	818.575115	10.388339
9.340871	815.278272	10.393357
9.257185	800.145895	10.398375
9.152385	803.316270	10.403392
9.034066	801.185543	10.408410
8.883780	799.106977	10.413427
9.154876	794.568591	10.418445
8.810091	793.695691	10.423463
8.946895	803.231928	10.428480
8.701505	828.108535	10.433498
8.902585	819.835791	10.438515
9.003857	828.457150	10.443533
9.171242	826.672803	10.448551
9.456120	831.495023	10.453568
9.246453	834.395058	10.458586
9.409716	827.716474	10.463603
9.425807	826.613721	10.468621
9.158547	820.961942	10.473639
9.247859	827.014412	10.478656
9.492691	831.393911	10.483674
9.449878	821.178579	10.488691
9.280993	830.408187	10.493709
9.058505	826.314402	10.498727
9.225694	825.145988	10.503744
9.309170	827.307979	10.508762
9.525684	815.387464	10.513779
9.181578	828.126254	10.518797
9.226366	831.927433	10.523815
9.483814	822.285377	10.528832
9.099338	828.708701	10.533850
9.420999	825.546447	10.538867
9.288937	834.051682	10.543885
9.321192	827.239765	10.548903
9.576003	828.914651	10.553920
9.270505	841.408666	10.558938
9.374569	828.293533	10.563955
9.361551	836.279806	10.568973
9.325789	831.615259	10.573991
9.566490	828.886116	10.579008
9.378168	838.597861	10.584026
9.680837	828.878212	10.589043
9.577338	814.160896	10.594061
9.359235	802.786412	10.599079
9.781871	807.064506	10.604096
9.087088	796.302681	10.609114
9.361696	788.355306	10.614131
8.978612	803.491911	10.619149
8.904847	817.573255	10.624167
9.549858	821.381157	10.629184
9.464022	829.242138	10.634202
9.746005	827.309225	10.639219
9.888337	829.744485	10.644237
9.561255	834.832186	10.649255
9.588692	828.316521	10.654272
9.297022	826.862391	10.659290
9.726575	831.801893	10.664307
9.678046	826.427711	10.669325
9.742677	828.494220	10.674343
9.857597	814.846229	10.679360
9.151965	802.059382	10.684378
9.379519	807.789678	10.689395
9.602439	823.724726	10.694413
9.228230	816.500092	10.699431
9.274692	821.904219	10.704448
9.020305	834.309030	10.709466
9.459818	825.749230	10.714483
9.509359	828.396749	10.719501
9.240794	835.862938	10.724519
9.475874	821.595997	10.729536
9.401523	833.062880	10.734554
9.869911	847.600952	10.739571
10.033942	850.901051	10.744589
9.719779	840.234188	10.749607
9.682147	831.081692	10.754624
9.515985	825.999679	10.759642
9.561826	828.523609	10.764659
9.588023	826.750721	10.769677
9.683015	851.891044	10.774695
9.955105	852.215912	10.779712
9.615058	843.206185	10.784730
9.573368	838.929996	10.789747
9.848358	846.319231	10.794765
9.718971	853.637896	10.799783
10.005413	855.454368	10.804800
9.968854	846.267434	10.809818
9.910851	833.920518	10.814835
9.609178	816.107821	10.819853
9.606582	822.627895	10.824871
10.153816	825.294456	10.829888
9.914829	835.055759	10.834906
9.545565	825.750724	10.839923
9.631703	825.788608	10.844941
9.565683	849.144993	10.849959
9.909339	851.173986	10.854976
9.998001	855.348166	10.859994
10.089133	855.459033	10.865011
10.239840	861.758382	10.870029
10.027023	849.375378	10.875047
9.906670	835.046840	10.880064
9.885436	828.424115	10.885082
9.848435	825.000238	10.890099
9.710721	819.150759	10.895117
9.894820	837.881441	10.900135
9.841910	838.827215	10.905152
9.600907	857.055388	10.910170
10.074401	840.938498	10.915187
10.126017	852.539368	10.920205
9.786770	859.187848	10.925223
10.036935	854.214962	10.930240
10.054983	851.738555	10.935258
10.183967	851.478787	10.940275
10.307765	853.664787	10.945293
9.986307	857.871899	10.950311
10.547376	855.812287	10.955328
9.900053	841.575660	10.960346
9.937844	841.972933	10.965363
9.540826	833.336435	10.970381
9.687748	857.146773	10.975399
10.214741	850.373868	10.980416
10.122849	856.905452	10.985434
10.018593	864.343952	10.990451
10.144748	854.363487	10.995469
9.880661	855.999237	11.000487
10.171856	854.752733	11.005504
10.422868	855.500957	11.010522
10.211133	864.716449	11.015539
10.449617	856.752210	11.020557
10.257419	855.783871	11.025575
10.321248	856.837793	11.030592
10.184773	865.344566	11.035610
9.898853	863.770981	11.040627
10.198832	854.945007	11.045645
10.161107	866.943387	11.050663
10.129064	857.916906	11.055680
10.173915	866.716944	11.060698
10.167493	854.204756	11.065715
10.399406	853.649948	11.070733
9.817077	853.941643	11.075751
10.603973	851.597074	11.080768
10.439565	861.680817	11.085786
10.132221	861.054034	11.090803
10.391388	863.771434	11.095821
10.464880	862.280622	11.100839
10.333356	857.873699	11.105856
10.266314	860.177043	11.110874
10.052932	867.112261	11.115891
9.683740	855.787455	11.120909
9.917344	863.811486	11.125927
10.045988	865.021947	11.130944
9.899397	868.801601	11.135962
10.126058	880.024210	11.140979
10.426310	892.750240	11.145997
10.400471	889.603214	11.151015
10.654483	895.357096	11.156032
10.668216	890.824059	11.161050
10.324932	889.262762	11.166067
10.597065	880.293774	11.171085
10.124423	880.872336	11.176103
10.366213	891.137780	11.181120
10.493537	895.303379	11.186138
10.671258	895.050273	11.191155
10.449102	891.722505	11.196173
10.232603	900.198309	11.201191
10.367381	889.567417	11.206208
10.392578	894.085401	11.211226
10.438499	906.356504	11.216243
10.346022	896.902475	11.221261
10.099285	888.165383	11.226279
10.453700	890.767751	11.231296
10.155183	892.046062	11.236314
10.572365	891.538997	11.241331
10.734670	891.089057	11.246349
10.457753	892.107694	11.251367
10.098281	901.387130	11.256384
10.788082	897.819799	11.261402
10.126325	900.676296	11.266419
10.747314	911.921570	11.271437
10.705782	914.090179	11.276455
10.818713	907.595111	11.281472
10.784266	904.121385	11.286490
10.633282	898.321323	11.291507
10.806236	889.375900	11.296525
10.676686	889.936411	11.301543
10.624543	887.809043	11.306560
10.785337	889.646993	11.311578
10.292039	888.099016	11.316595
11.115419	890.641547	11.321613
10.684315	895.766438	11.326631
10.646824	893.403579	11.331648
10.757043	882.422073	11.336666
10.358772	888.096782	11.341683
10.638013	893.504367	11.346701
10.823894	910.809741	11.351719
10.965279	910.542991	11.356736
10.831647	910.603821	11.361754
10.683530	915.102982	11.366771
11.260292	907.414951	11.371789
10.856199	897.715688	11.376807
10.744305	890.623982	11.381824
10.930888	889.359236	11.386842
10.554440	900.802172	11.391859
11.263784	907.418110	11.396877
11.023602	912.620125	11.401895
10.608662	898.985723	11.406912
10.737359	901.070922	11.411930
10.844413	913.347026	11.416947
10.853606	919.195345	11.421965
10.556338	915.396230	11.426983
10.344184	916.651135	11.432000
11.095118	922.323221	11.437018
10.492008	931.814025	11.442035
11.100649	924.527746	11.447053
11.123638	919.021180	11.452071
10.912708	920.967174	11.457088
11.320611	917.333512	11.462106
11.202871	925.147879	11.467123
11.436726	919.105904	11.472141
11.167490	922.810686	11.477159
11.183904	915.807282	11.482176
11.167589	913.191310	11.487194
11.097305	920.087612	11.492211
11.354266	909.595640	11.497229
11.154508	901.935698	11.502247
10.929535	896.827415	11.507264
11.055656	899.632678	11.512282
10.762150	916.236294	11.517299
10.875150	908.044673	11.522317
10.929943	922.790723	11.527335
10.705211	921.456552	11.532352
10.741834	921.712889	11.537370
10.799158	927.212091	11.542387
11.160240	913.666200	11.547405
10.933871	918.312415	11.552423
10.725979	923.294907	11.557440
11.250617	929.009136	11.562458
11.135047	947.858652	11.567475
11.484515	946.816812	11.572493
11.652148	936.703031	11.577511
11.190979	930.718700	11.582528
10.854187	914.226011	11.587546
11.032274	934.428380	11.592563
11.547209	926.514607	11.597581
11.419370	943.580448	11.602599
11.338208	921.439132	11.607616
11.323741	912.202230	11.612634
10.914032	917.378687	11.617651
11.491015	923.364313	11.622669
11.212660	932.290150	11.627687
11.275773	951.935902	11.632704
11.658865	954.064647	11.637722
11.414861	952.006558	11.642739
11.557173	941.104120	11.647757
11.504406	930.053614	11.652775
11.037804	926.890082	11.657792
11.660164	914.734920	11.662810
11.107287	920.691226	11.667827
11.341420	935.555895	11.672845
11.405236	953.500463	11.677863
11.502491	946.565886	11.682880
11.789043	944.718415	11.687898
11.370684	948.037778	11.692915
11.394458	927.018309	11.697933
11.406300	931.398769	11.702951
11.518375	946.254801	11.707968
11.725860	942.607991	11.712986
11.357527	943.981370	11.718003
11.334196	946.902027	11.723021
11.671486	943.621411	11.728039
11.557544	954.593619	11.733056
11.956400	956.394175	11.738074
11.277260	945.790066	11.743091
11.067155	946.485614	11.748109
11.311786	941.624834	11.753127
11.312757	954.836850	11.758144
11.439757	953.764274	11.763162
11.168242	957.420627	11.768179
11.576901	954.870226	11.773197
11.706749	955.531317	11.778215
11.738231	950.526838	11.783232
11.781012	945.274437	11.788250
11.707148	957.276138	11.793267
12.047058	950.026443	11.798285
11.818873	951.056864	11.803303
11.790027	960.425271	11.808320
11.900726	943.306044	11.813338
11.679532	961.120443	11.818355
11.619915	962.676750	11.823373
11.560150	959.046403	11.828391
11.137613	959.784346	11.833408
11.599185	950.277171	11.838426
11.575167	957.105173	11.843443
11.745276	949.923855	11.848461
11.930915	957.730725	11.853479
11.593473	947.950475	11.858496
11.768410	952.873875	11.863514
11.497107	965.755588	11.868531
12.005676	969.081513	11.873549
12.316423	975.778297	11.878567
11.802845	973.119382	11.883584
11.758184	948.831544	11.888602
11.916427	951.353936	11.893619
11.854274	957.071420	11.898637
11.899329	948.690887	11.903655
11.482379	960.061863	11.908672
12.140752	970.060101	11.913690
11.717104	984.575317	11.918707
12.094697	977.847660	11.923725
12.115113	980.059521	11.928743
11.670282	986.880319	11.933760
12.139940	971.491838	11.938778
12.065644	979.373023	11.943795
12.176693	978.595204	11.948813
11.964645	987.007918	11.953831
11.972784	984.265436	11.958848
11.940929	982.593315	11.963866
12.431639	974.462299	11.968883
12.176026	972.166782	11.973901
11.974817	963.519711	11.978919
11.920050	976.827225	11.983936
12.474643	969.946932	11.988954
11.947081	961.098609	11.993971
11.729551	978.454181	11.998989
12.050941	974.118001	12.004007
12.216065	987.542904	12.009024
12.114215	980.193008	12.014042
12.380486	985.519716	12.019059
12.011888	980.607707	12.024077
12.135722	978.921914	12.029095
11.787937	980.674534	12.034112
12.340304	979.396225	12.039130
12.501301	979.655315	12.044147
12.065223	976.076488	12.049165
12.141349	972.187740	12.054183
12.158942	977.723090	12.059200
12.229861	980.450540	12.064218
12.089587	977.840201	12.069235
11.908555	984.460863	12.074253
12.181147	975.435054	12.079271
12.182646	977.661083	12.084288
12.260928	974.006214	12.089306
12.335621	970.697196	12.094323
12.031582	975.880123	12.099341
12.185888	968.451832	12.104359
11.968115	981.082157	12.109376
12.325637	992.670475	12.114394
12.747418	1008.124263	12.119411
12.612919	996.125345	12.124429
12.573230	993.273102	12.129447
12.098065	989.390158	12.134464
12.500512	983.523274	12.139482
12.121340	988.264784	12.144499
12.103874	1002.036170	12.149517
12.634468	1007.327220	12.154535
12.447776	1006.287881	12.159552
12.593902	1011.572366	12.164570
12.649388	1007.441780	12.169587
12.657485	1015.904528	12.174605
12.754881	998.570928	12.179623
12.311830	999.826030	12.184640
12.570770	999.072051	12.189658
12.710747	1001.576623	12.194675
12.490158	997.463581	12.199693
12.524440	996.174536	12.204711
12.573755	1008.397915	12.209728
12.584829	1010.121993	12.214746
12.847819	1011.508944	12.219763
12.073431	1000.378142	12.224781
12.362378	999.360530	12.229799
11.957966	1005.101849	12.234816
12.131920	1011.831620	12.239834
12.728835	1006.722909	12.244851
12.746332	1012.721644	12.249869
12.842822	1000.898097	12.254887
12.495909	1005.147272	12.259904
12.500586	1006.059077	12.264922
12.679318	1001.730459	12.269939
12.383359	1005.811727	12.274957
12.715209	1010.777565	12.279975
12.800650	1028.428485	12.284992
13.208786	1026.676931	12.290010
12.929820	1019.652499	12.295027
12.688208	1016.196844	12.300045
12.662361	1011.469575	12.305063
12.797395	1006.183710	12.310080
12.830968	1012.655336	12.315098
12.658372	1014.450884	12.320115
12.688467	1028.418313	12.325133
12.991118	1036.243174	12.330151
12.830794	1041.091624	12.335168
12.593113	1042.820439	12.340186
13.266003	1035.923998	12.345203
12.800085	1046.040258	12.350221
13.036897	1039.978061	12.355239
12.973220	1035.908609	12.360256
13.267520	1041.425154	12.365274
13.325547	1028.988723	12.370291
12.890410	1027.800531	12.375309
12.894249	1014.384200	12.380327
12.670115	1024.237439	12.385344
13.108748	1026.573879	12.390362
13.525028	1031.265076	12.395379
12.927795	1027.383514	12.400397
13.027553	1011.562803	12.405415
12.758259	1012.168198	12.410432
12.855161	1024.549418	12.415450
13.461373	1032.732853	12.420467
13.188829	1042.399673	12.425485
13.230174	1029.136141	12.430503
13.018712	1015.013119	12.435520
12.903288	1019.315156	12.440538
13.303851	1023.627491	12.445555
12.730378	1034.359615	12.450573
13.039003	1030.268440	12.455591
13.234640	1036.615901	12.460608
13.194232	1041.218843	12.465626
13.179149	1039.281739	12.470643
12.992973	1032.049372	12.475661
13.413578	1035.281276	12.480679
12.617988	1041.946236	12.485696
12.571557	1033.391504	12.490714
13.160831	1035.404107	12.495731
12.904879	1037.440664	12.500749
13.087201	1048.045605	12.505767
13.404643	1060.200839	12.510784
13.260513	1062.157400	12.515802
13.851264	1053.343218	12.520819
13.654162	1047.701149	12.525837
13.463031	1038.105960	12.530855
13.233104	1033.497245	12.535872
13.296036	1044.187771	12.540890
13.779768	1031.038100	12.545907
13.311508	1038.652531	12.550925
13.519425	1036.581519	12.555943
13.479741	1029.581088	12.560960
13.220007	1040.529953	12.565978
13.682601	1031.393009	12.570995
13.129701	1037.692453	12.576013
13.236205	1025.339300	12.581031
13.373270	1038.942523	12.586048
13.327166	1034.029256	12.591066
13.019469	1044.753432	12.596083
13.503156	1061.273299	12.601101
13.625737	1055.757611	12.606119
13.710760	1067.038935	12.611136
13.927244	1070.770889	12.616154
13.642279	1052.461076	12.621171
13.579961	1064.475507	12.626189
13.822252	1059.346197	12.631207
13.684941	1044.604166	12.636224
13.696450	1034.209989	12.641242
13.631707	1028.570336	12.646259
13.640118	1033.693477	12.651277
13.686913	1032.226376	12.656295
13.485094	1035.323952	12.661312
13.855275	1054.476303	12.666330
13.909078	1042.073239	12.671347
13.830062	1038.641338	12.676365
13.314299	1032.919569	12.681383
13.420023	1044.985972	12.686400
13.576808	1058.631995	12.691418
14.020803	1056.032007	12.696435
13.545143	1057.985799	12.701453
13.759773	1063.571497	12.706471
13.900352	1067.394014	12.711488
14.042310	1070.081329	12.716506
13.974084	1067.491281	12.721523
14.054572	1066.863017	12.726541
14.021370	1060.865374	12.731559
13.796791	1053.880310	12.736576
13.948265	1055.201946	12.741594
13.845772	1032.908906	12.746611
13.797054	1058.060065	12.751629
13.772348	1063.381622	12.756647
14.122249	1066.148934	12.761664
13.708820	1067.402267	12.766682
13.709838	1071.947942	12.771699
13.816933	1067.612709	12.776717
13.640522	1072.322513	12.781735
13.838497	1065.579792	12.786752
14.049936	1071.861652	12.791770
13.935913	1057.487371	12.796787
14.028780	1074.391876	12.801805
14.205665	1061.723865	12.806823
14.024946	1060.544168	12.811840
14.124001	1065.208184	12.816858
14.518384	1054.696029	12.821875
14.050751	1062.631215	12.826893
14.262217	1065.688844	12.831911
14.242895	1063.808738	12.836928
13.920022	1070.146335	12.841946
14.222322	1067.365183	12.846963
14.333555	1070.132009	12.851981
13.917054	1070.626053	12.856999
13.611428	1063.566271	12.862016
13.680511	1065.575579	12.867034
13.883362	1063.540442	12.872051
13.891516	1069.052198	12.877069
14.136013	1086.366529	12.882087
14.482710	1085.712128	12.887104
14.297195	1083.524227	12.892122
14.529320	1091.252577	12.897139
14.591849	1079.952695	12.902157
14.153066	1059.772876	12.907175
14.425853	1060.008268	12.912192
14.623437	1067.866356	12.917210
14.270527	1057.639419	12.922227
14.015351	1059.769940	12.927245
14.121711	1068.327795	12.932263
14.619801	1064.303934	12.937280
14.608483	1081.492284	12.942298
14.569150	1061.864146	12.947315
14.381829	1057.318417	12.952333
14.643302	1059.733912	12.957351
15.003419	1047.662586	12.962368
14.603600	1058.531210	12.967386
14.677911	1051.346477	12.972403
14.707713	1055.254329	12.977421
14.722905	1056.151398	12.982439
14.777577	1056.120698	12.987456
14.589791	1043.683775	12.992474
14.579374	1052.503537	12.997491
14.785243	1050.036823	13.002509
14.801664	1057.347490	13.007527
15.162057	1052.180444	13.012544
14.968068	1036.088864	13.017562
14.801274	1020.177809	13.022579
14.931917	1025.049543	13.027597
14.561268	1026.737861	13.032615
14.632016	1013.491502	13.037632
14.531259	1029.948643	13.042650
14.634093	1015.836370	13.047667
14.445176	1009.888248	13.052685
14.490856	1017.434570	13.057703
14.836876	1022.263026	13.062720
14.590884	1030.213716	13.067738
14.943472	1037.825566	13.072755
14.795461	1045.024982	13.077773
14.775988	1038.279441	13.082791
14.880978	1032.997380	13.087808
14.806667	1039.307824	13.092826
14.628285	1042.864077	13.097843
14.675548	1044.190435	13.102861
14.610717	1054.282554	13.107879
15.074055	1058.986410	13.112896
14.541338	1053.796948	13.117914
14.474523	1050.022879	13.122931
14.937553	1055.512172	13.127949
14.549135	1050.699099	13.132967
14.874745	1054.937685	13.137984
14.645139	1046.337411	13.143002
14.769477	1053.758478	13.148019
14.611608	1062.205532	13.153037
14.541370	1063.937226	13.158055
14.750424	1071.924897	13.163072
14.974564	1085.066863	13.168090
14.921833	1079.372049	13.173107
15.170359	1089.946725	13.178125
14.900971	1086.231117	13.183143
14.963169	1084.348482	13.188160
15.012541	1092.665837	13.193178
15.546546	1092.802699	13.198195
15.342378	1088.314876	13.203213
15.389445	1088.983039	13.208231
15.383280	1092.952781	13.213248
15.384869	1083.582605	13.218266
15.279618	1065.465728	13.223283
15.242054	1059.390863	13.228301
14.731926	1061.994442	13.233319
15.101653	1060.829156	13.238336
14.965697	1080.958133	13.243354
15.070892	1087.143491	13.248371
15.264626	1077.597296	13.253389
15.276452	1084.867403	13.258407
15.445749	1080.515137	13.263424
15.304441	1088.698443	13.268442
15.137455	1094.722755	13.273459
15.333038	1084.285747	13.278477
15.183895	1084.922352	13.283495
15.217310	1081.446559	13.288512
15.340107	1090.248925	13.293530
15.114946	1090.829271	13.298547
15.261648	1089.831753	13.303565
15.256923	1087.481527	13.308583
15.381737	1080.811980	13.313600
15.416522	1084.174160	13.318618
15.161140	1077.383170	13.323635
15.392071	1084.375535	13.328653
15.677524	1089.296751	13.333671
15.585867	1092.284695	13.338688
15.354702	1086.680161	13.343706
14.945638	1094.684758	13.348723
15.447048	1096.776143	13.353741
15.613127	1112.579606	13.358759
15.994914	1116.699428	13.363776
15.700813	1121.459121	13.368794
15.738145	1115.549334	13.373811
15.608738	1096.469559	13.378829
15.570755	1095.486202	13.383847
15.779090	1098.516801	13.388864
15.893168	1096.973160	13.393882
15.651000	1094.034480	13.398899
15.989118	1085.055982	13.403917
15.587972	1093.793867	13.408935
15.618823	1089.428390	13.413952
15.630301	1086.720767	13.418970
15.720421	1087.097538	13.423987
15.677561	1090.638363	13.429005
15.323100	1116.184901	13.434023
15.564613	1119.876489	13.439040
15.528789	1116.896816	13.444058
15.678573	1119.825345	13.449075
15.821780	1117.440291	13.454093
15.646858	1117.344214	13.459111
15.708003	1116.101873	13.464128
15.644195	1118.912367	13.469146
15.653732	1125.830925	13.474163
15.909807	1119.876119	13.479181
15.578083	1112.561217	13.484199
16.245763	1130.767022	13.489216
16.249720	1124.174627	13.494234
16.113144	1128.690435	13.499251
16.362049	1121.502240	13.504269
16.009320	1130.415553	13.509287
16.127488	1120.446481	13.514304
15.870898	1118.985705	13.519322
15.786961	1125.873344	13.524339
16.043316	1114.401466	13.529357
15.849430	1120.435376	13.534375
15.985114	1115.443052	13.539392
15.794041	1115.624054	13.544410
15.844995	1129.504647	13.549427
16.194260	1138.653632	13.554445
15.949793	1145.245930	13.559463
16.159897	1140.184539	13.564480
16.614284	1146.359518	13.569498
16.612279	1148.801890	13.574515
16.594011	1121.767410	13.579533
16.190871	1128.430166	13.584551
16.292699	1114.251439	13.589568
16.282867	1120.275230	13.594586
15.909410	1113.481016	13.599603
16.394469	1116.157373	13.604621
15.767425	1114.134187	13.609639
16.485191	1122.985314	13.614656
16.365998	1131.720843	13.619674
16.191590	1137.212182	13.624691
16.621988	1139.625595	13.629709
16.273053	1136.102715	13.634727
16.595760	1141.562609	13.639744
16.493493	1137.067677	13.644762
16.371355	1142.944404	13.649779
16.617474	1137.433744	13.654797
16.513607	1134.408293	13.659815
16.248514	1122.272723	13.664832
16.255444	1117.541548	13.669850
16.169350	1137.884740	13.674867
16.681550	1137.640208	13.679885
16.242459	1139.883192	13.684903
16.331533	1138.661797	13.689920
16.403636	1148.192663	13.694938
15.914736	1152.053294	13.699955
16.573116	1138.510745	13.704973
16.693952	1135.960911	13.709991
16.635165	1137.848970	13.715008
16.671227	1137.684756	13.720026
16.306351	1144.946246	13.725043
16.661600	1138.663549	13.730061
16.513743	1147.854221	13.735079
16.640243	1159.324772	13.740096
16.893841	1159.671224	13.745114
16.632785	1181.846611	13.750131
17.077519	1172.726333	13.755149
17.268486	1158.462675	13.760167
16.908412	1140.937642	13.765184
16.918033	1140.724676	13.770202
17.113963	1144.090792	13.775219
16.981124	1140.713087	13.780237
16.746837	1137.927017	13.785255
16.459737	1138.761741	13.790272
17.108914	1145.852327	13.795290
16.649785	1148.531298	13.800307
16.629608	1138.713942	13.805325
16.598170	1144.368124	13.810343
16.535953	1153.044198	13.815360
16.933036	1163.916658	13.820378
17.078442	1176.663541	13.825395
17.295955	1168.337687	13.830413
16.574195	1170.707574	13.835431
16.759928	1183.472168	13.840448
17.243098	1173.417989	13.845466
17.124400	1180.447643	13.850483
17.267292	1172.811320	13.855501
17.166155	1176.153987	13.860519
16.915908	1174.629162	13.865536
17.164607	1175.077999	13.870554
16.995299	1179.206761	13.875571
17.173675	1171.605484	13.880589
17.228858	1162.843644	13.885607
17.109172	1171.689902	13.890624
17.231127	1170.946086	13.895642
17.123823	1170.581696	13.900659
17.101035	1164.401583	13.905677
16.981168	1164.290449	13.910695
17.305390	1166.501840	13.915712
17.495239	1163.164587	13.920730
17.252112	1171.861292	13.925747
17.309964	1166.695282	13.930765
17.315049	1161.259713	13.935783
17.252945	1172.947437	13.940800
17.608507	1164.601396	13.945818
17.546858	1162.549188	13.950835
17.604215	1160.998040	13.955853
17.631626	1157.388589	13.960871
17.380637	1166.218874	13.965888
17.307288	1161.838807	13.970906
17.406176	1164.849029	13.975923
17.157374	1162.088594	13.980941
17.411095	1162.886972	13.985959
17.166420	1156.420923	13.990976
17.696958	1161.503780	13.995994
17.519013	1160.255113	14.001011
17.474767	1166.532661	14.006029
17.082920	1158.310453	14.011047
17.309202	1167.257073	14.016064
17.637478	1169.057575	14.021082
17.673437	1184.011128	14.026099
17.728675	1195.858098	14.031117
17.566149	1192.894351	14.036135
17.751630	1192.036437	14.041152
17.885297	1200.606756	14.046170
17.327845	1189.587390	14.051187
17.946708	1187.541752	14.056205
17.951513	1194.945355	14.061223
17.511199	1189.804265	14.066240
17.915488	1179.575800	14.071258
17.918666	1196.446529	14.076275
17.863353	1187.340459	14.081293
17.813836	1191.417821	14.086311
17.512660	1193.203659	14.091328
17.715002	1196.085280	14.096346
17.963775	1191.967399	14.101363
17.981633	1192.644752	14.106381
17.828894	1187.584600	14.111399
17.981262	1195.197918	14.116416
18.064675	1188.230496	14.121434
17.964042	1197.811755	14.126451
17.939830	1190.607115	14.131469
18.022426	1193.790514	14.136487
17.834675	1185.432800	14.141504
17.794431	1191.377032	14.146522
17.871981	1190.108731	14.151539
18.070859	1190.918982	14.156557
18.335955	1190.400968	14.161575
18.150913	1190.672301	14.166592
18.175866	1189.195825	14.171610
18.154837	1190.218994	14.176627
18.089519	1189.587402	14.181645
18.338986	1188.237381	14.186663
18.081017	1192.043498	14.191680
18.200434	1185.596445	14.196698
17.979051	1189.042168	14.201715
18.253137	1187.636876	14.206733
18.396653	1190.198762	14.211751
17.774989	1190.198194	14.216768
18.080219	1184.898548	14.221786
18.059874	1199.210718	14.226803
18.165010	1188.298145	14.231821
18.198376	1195.402527	14.236839
17.977374	1195.086954	14.241856
18.104599	1201.321843	14.246874
18.075738	1219.941934	14.251891
18.217834	1217.014162	14.256909
18.281050	1219.002813	14.261927
17.963810	1219.659094	14.266944
18.808372	1211.175063	14.271962
18.165298	1221.647637	14.276979
18.659437	1210.577484	14.281997
18.510918	1209.626664	14.287015
18.473083	1217.013744	14.292032
18.641080	1221.002601	14.297050
18.754177	1210.125695	14.302067
18.720232	1211.618313	14.307085
18.838519	1206.248161	14.312103
18.765383	1215.231976	14.317120
18.507460	1216.738594	14.322138
18.470805	1213.106315	14.327155
18.478841	1214.021904	14.332173
18.727098	1221.511035	14.337191
18.424567	1217.389112	14.342208
18.794464	1213.749495	14.347226
18.655430	1213.389590	14.352243
18.667980	1216.061826	14.357261
19.047578	1208.548341	14.362279
18.566258	1217.782668	14.367296
18.721756	1214.923139	14.372314
18.775913	1202.941520	14.377331
18.485470	1209.790688	14.382349
19.301658	1220.427003	14.387367
18.684379	1219.508032	14.392384
18.748983	1206.022384	14.397402
19.036508	1219.592885	14.402419
18.852995	1226.777815	14.407437
19.155739	1217.288215	14.412455
18.626643	1224.739233	14.417472
19.158580	1221.977758	14.422490
19.446243	1221.333164	14.427507
18.833159	1224.243631	14.432525
19.045929	1215.149678	14.437543
19.061605	1226.136753	14.442560
19.156013	1217.471901	14.447578
19.126766	1219.487336	14.452595
19.159189	1218.788318	14.457613
19.051506	1218.359426	14.462631
18.930511	1231.414793	14.467648
19.154084	1233.010668	14.472666
19.273289	1229.433186	14.477683
19.218684	1238.671796	14.482701
19.170869	1238.258936	14.487719
18.920773	1233.317701	14.492736
19.158054	1228.150588	14.497754
19.248809	1232.661317	14.502771
19.304392	1232.845417	14.507789
19.682200	1239.824070	14.512807
19.469596	1236.013559	14.517824
19.535414	1233.102793	14.522842
19.574298	1237.895755	14.527859
19.262130	1237.867367	14.532877
19.369508	1230.244792	14.537895
19.439668	1237.627711	14.542912
19.546867	1239.826367	14.547930
19.281114	1237.914761	14.552947
19.012816	1236.994476	14.557965
19.235868	1226.010706	14.562983
19.098919	1226.310659	14.568000
19.156808	1230.639458	14.573018
19.291541	1226.455487	14.578035
19.052978	1239.374502	14.583053
19.587431	1242.353682	14.588071
19.838142	1256.632271	14.593088
19.877732	1253.032978	14.598106
20.332984	1237.539942	14.603123
19.877981	1242.867728	14.608141
19.857319	1219.140805	14.613159
19.956591	1222.845036	14.618176
19.721737	1212.316891	14.623194
19.910265	1214.805162	14.628211
19.586633	1213.362999	14.633229
19.898650	1219.431362	14.638247
19.886645	1215.695384	14.643264
19.678930	1220.393506	14.648282
19.650890	1214.211884	14.653299
19.579017	1219.373626	14.658317
19.796039	1207.338952	14.663335
19.635083	1210.269147	14.668352
19.291318	1213.229334	14.673370
19.952631	1236.329004	14.678387
19.601138	1242.084053	14.683405
20.106851	1244.998722	14.688423
19.998939	1248.735820	14.693440
20.154373	1247.567557	14.698458
20.155611	1253.052970	14.703475
19.987487	1257.613033	14.708493
20.279928	1244.317426	14.713511
20.054596	1251.195159	14.718528
20.025137	1253.850369	14.723546
20.368822	1245.045255	14.728563
20.301243	1252.294389	14.733581
20.445443	1241.407174	14.738599
20.091691	1236.575288	14.743616
20.302616	1242.056159	14.748634
20.211703	1234.999980	14.753651
20.037148	1240.070926	14.758669
20.500051	1245.774079	14.763687
20.386618	1256.285019	14.768704
20.268227	1246.929173	14.773722
20.670944	1227.949368	14.778739
20.182387	1237.636857	14.783757
19.878292	1232.060139	14.788775
20.092255	1240.260458	14.793792
20.240590	1256.532744	14.798810
20.405939	1244.162551	14.803827
20.168392	1254.267759	14.808845
20.227990	1247.729840	14.813863
20.421761	1248.005534	14.818880
19.971679	1252.880163	14.823898
20.529023	1246.329986	14.828915
20.057861	1249.716453	14.833933
20.229487	1260.305602	14.838951
20.626212	1266.958697	14.843968
20.414043	1283.815710	14.848986
20.620896	1281.460996	14.854003
20.469115	1284.494401	14.859021
20.578795	1277.842245	14.864039
20.816756	1265.598936	14.869056
20.699792	1278.593439	14.874074
21.181179	1269.346940	14.879091
21.158430	1280.933721	14.884109
20.866883	1260.799636	14.889127
20.821310	1250.304570	14.894144
20.818268	1247.950103	14.899162
20.884030	1239.714390	14.904179
20.757134	1252.476674	14.909197
20.803001	1243.188802	14.914215
20.680444	1236.325274	14.919232
20.445703	1242.814033	14.924250
20.863102	1250.931335	14.929267
20.525510	1275.414749	14.934285
20.792017	1274.992951	14.939303
20.693553	1274.600712	14.944320
20.819042	1268.506538	14.949338
21.121011	1275.795437	14.954355
20.879517	1275.961987	14.959373
20.935231	1281.996206	14.964391
21.071949	1273.214059	14.969408
21.147718	1278.785514	14.974426
21.344376	1271.822854	14.979443
21.181455	1274.862833	14.984461
20.749686	1275.227141	14.989479
21.059447	1277.076402	14.994496
20.891234	1279.858217	14.999514
21.024823	1274.226060	15.004531
20.802551	1286.970761	15.009549
20.985737	1292.460985	15.014567
20.968687	1303.690552	15.019584
21.301943	1308.462561	15.024602
21.584261	1304.779608	15.029619
21.640710	1301.103489	15.034637
21.801112	1310.237512	15.039655
21.567509	1283.485379	15.044672
21.234674	1276.562692	15.049690
21.684215	1273.229889	15.054707
21.409845	1265.587678	15.059725
21.366500	1267.951511	15.064743
21.429313	1271.825586	15.069760
21.447551	1278.612850	15.074778
21.730808	1270.005159	15.079795
21.512928	1271.956682	15.084813
21.421887	1268.593655	15.089831
21.454705	1277.165030	15.094848
21.462674	1293.463441	15.099866
21.694079	1298.478743	15.104883
21.899236	1303.471246	15.109901
21.728264	1296.105917	15.114919
21.638085	1286.026098	15.119936
21.648981	1300.435921	15.124954
21.558280	1297.830672	15.129971
21.573131	1309.431697	15.134989
21.463062	1304.338431	15.140007
21.712678	1303.407650	15.145024
21.594878	1304.934292	15.150042
21.652504	1296.611322	15.155059
21.418380	1302.163429	15.160077
21.447395	1298.352899	15.165095
21.593094	1301.113646	15.170112
21.581621	1309.940816	15.175130
21.704514	1312.237657	15.180147
22.322322	1329.005982	15.185165
22.223635	1318.764177	15.190183
22.368127	1300.432688	15.195200
21.953546	1300.215818	15.200218
22.280492	1290.356419	15.205235
22.329426	1291.701418	15.210253
21.948311	1293.943055	15.215271
22.129397	1293.703163	15.220288
21.941147	1291.507813	15.225306
22.078960	1290.618055	15.230323
22.033151	1289.074199	15.235341
21.862944	1292.012247	15.240359
21.976586	1298.457692	15.245376
21.960176	1318.266726	15.250394
22.264257	1322.995953	15.255411
22.385663	1314.495057	15.260429
22.186761	1330.029496	15.265447
22.520916	1315.296638	15.270464
22.337098	1327.077146	15.275482
22.798002	1326.587605	15.280499
22.644570	1308.244997	15.285517
22.653685	1300.841861	15.290535
22.728509	1290.655089	15.295552
21.885920	1301.293154	15.300570
22.166761	1293.482276	15.305587
22.337639	1291.837841	15.310605
22.037016	1304.233784	15.315623
22.370833	1314.843255	15.320640
22.586144	1329.919496	15.325658
22.605483	1318.484892	15.330675
22.501226	1318.592413	15.335693
22.386307	1313.841669	15.340711
22.857565	1309.762366	15.345728
22.863107	1315.731318	15.350746
22.740874	1317.924812	15.355763
22.550549	1315.368795	15.360781
22.642663	1321.643820	15.365799
22.985856	1317.412972	15.370816
22.723972	1313.132306	15.375834
23.202183	1310.298646	15.380851
23.129844	1313.933394	15.385869
22.813200	1313.673082	15.390887
22.717072	1318.017662	15.395904
22.800499	1318.990016	15.400922
23.119463	1312.313690	15.405939
23.014550	1315.642448	15.410957
22.703968	1314.793751	15.415975
23.062221	1317.668773	15.420992
22.886190	1318.285447	15.426010
22.718736	1316.413395	15.431027
23.375740	1322.506347	15.436045
22.871085	1319.325828	15.441063
23.190747	1316.367738	15.446080
22.961179	1318.834181	15.451098
22.901605	1329.869661	15.456115
23.113722	1316.996775	15.461133
22.643901	1325.662742	15.466151
22.986367	1319.667913	15.471168
22.761779	1320.319428	15.476186
22.572577	1321.475278	15.481203
23.391493	1330.555374	15.486221
22.895107	1344.451937	15.491239
23.455206	1347.431600	15.496256
23.558465	1354.966548	15.501274
23.547875	1339.853580	15.506291
23.342170	1341.817654	15.511309
23.550395	1342.801155	15.516327
23.769223	1326.445786	15.521344
23.379991	1319.651740	15.526362
23.375452	1309.696248	15.531379
23.642358	1297.217011	15.536397
23.640561	1306.347283	15.541415
23.331597	1306.864009	15.546432
23.558965	1307.812832	15.551450
24.093363	1310.577870	15.556467
23.717709	1307.403865	15.561485
23.383493	1311.164024	15.566503
23.445885	1305.808245	15.571520
23.355890	1320.276980	15.576538
23.397893	1303.791188	15.581555
23.827891	1314.798042	15.586573
23.572956	1320.360307	15.591591
23.579464	1321.364735	15.596608
23.934556	1333.169454	15.601626
23.824438	1334.514514	15.606643
23.912257	1323.423236	15.611661
23.256058	1323.828390	15.616679
23.674399	1322.889248	15.621696
24.010956	1337.947708	15.626714
23.592715	1337.540508	15.631731
24.069234	1334.407925	15.636749
23.756071	1340.012550	15.641767
23.703715	1337.565482	15.646784
23.975486	1339.999388	15.651802
23.556605	1340.244238	15.656819
24.189860	1330.752784	15.661837
23.948061	1334.238938	15.666855
23.832319	1338.058064	15.671872
24.005680	1341.567733	15.676890
23.816581	1337.470624	15.681907
23.921496	1339.949584	15.686925
24.141343	1349.748133	15.691943
24.292138	1360.070745	15.696960
24.048662	1370.554952	15.701978
23.791544	1373.377543	15.706995
24.376633	1365.237725	15.712013
24.053676	1378.041754	15.717031
24.319326	1373.833622	15.722048
24.460940	1382.787353	15.727066
24.417965	1377.267966	15.732083
24.349299	1377.247529	15.737101
23.970897	1373.141324	15.742119
24.206075	1373.399902	15.747136
24.562230	1370.545575	15.752154
24.600007	1377.334753	15.757171
24.581261	1370.124003	15.762189
24.330583	1368.917327	15.767207
24.304078	1367.411986	15.772224
24.469146	1365.342147	15.777242
24.219682	1375.348631	15.782259
24.497017	1367.443026	15.787277
24.683063	1392.164384	15.792295
24.652198	1383.577345	15.797312
24.639270	1378.693492	15.802330
24.918694	1400.095527	15.807347
25.183916	1386.987387	15.812365
24.704312	1374.495159	15.817383
24.780211	1377.008080	15.822400
25.001137	1358.430758	15.827418
24.842159	1363.132239	15.832435
25.119957	1354.845870	15.837453
24.478356	1356.046992	15.842471
24.750478	1363.682220	15.847488
25.025216	1355.574699	15.852506
24.743907	1356.845856	15.857523
25.309877	1364.946005	15.862541
25.143223	1363.448604	15.867559
24.828085	1360.264529	15.872576
25.031381	1362.351959	15.877594
24.559900	1365.248758	15.882611
25.455762	1382.869321	15.887629
24.834246	1395.021436	15.892647
25.100264	1395.989431	15.897664
25.297015	1389.210554	15.902682
25.566113	1401.429603	15.907699
25.855592	1374.809263	15.912717
25.072914	1363.094161	15.917735
25.245209	1352.940360	15.922752
25.559580	1345.908498	15.927770
25.131700	1354.050601	15.932787
25.248623	1349.479808	15.937805
25.289879	1353.864159	15.942823
25.144239	1352.044775	15.947840
25.348552	1358.958622	15.952858
25.165231	1380.169047	15.957875
25.883689	1384.848712	15.962893
25.384644	1376.341853	15.967911
25.321100	1375.563506	15.972928
25.397481	1377.982651	15.977946
25.240756	1382.452276	15.982963
25.502316	1380.625050	15.987981
25.389412	1393.829597	15.992999
25.484613	1376.329016	15.998016
25.245672	1382.168162	16.003034
25.363436	1382.371849	16.008051
25.861919	1381.623314	16.013069
25.759205	1385.437530	16.018087
25.528427	1387.822298	16.023104
25.774561	1389.310901	16.028122
25.784674	1392.174510	16.033139
25.854910	1390.851900	16.038157
25.923322	1385.925786	16.043175
25.645577	1392.300105	16.048192
25.880730	1383.686569	16.053210
25.557636	1392.554555	16.058227
25.891145	1394.090446	16.063245
25.860190	1418.747916	16.068263
26.015732	1415.514734	16.073280
26.134406	1415.613549	16.078298
26.177474	1405.791023	16.083315
26.239625	1405.258310	16.088333
26.305299	1408.938643	16.093351
26.369274	1403.412888	16.098368
25.914104	1387.958818	16.103386
25.862648	1402.292489	16.108403
26.052365	1407.126967	16.113421
26.139682	1413.670140	16.118439
26.000096	1411.272203	16.123456
26.232086	1406.177955	16.128474
26.129613	1412.173164	16.133491
26.611407	1398.832175	16.138509
26.197638	1410.102953	16.143527
26.283558	1411.758733	16.148544
26.166691	1400.087267	16.153562
26.138846	1413.665475	16.158579
26.167338	1405.554368	16.163597
26.342229	1405.157243	16.168615
26.145064	1413.596452	16.173632
26.436979	1418.306472	16.178650
26.577104	1437.476670	16.183667
26.720215	1432.386163	16.188685
26.686294	1435.750784	16.193703
26.490335	1434.720829	16.198720
27.133746	1427.049223	16.203738
26.700207	1439.304377	16.208755
26.963298	1424.654484	16.213773
26.915448	1417.605630	16.218791
26.638273	1401.147981	16.223808
26.984910	1394.575679	16.228826
26.720281	1394.763396	16.233843
26.993688	1396.954529	16.238861
27.029499	1393.671568	16.243879
26.723424	1390.439919	16.248896
27.040991	1396.714509	16.253914
27.047431	1394.000189	16.258931
26.814880	1400.660298	16.263949
26.747236	1390.176285	16.268967
26.750476	1401.543491	16.273984
26.805434	1412.546609	16.279002
27.010842	1430.856766	16.284019
27.045302	1427.709845	16.289037
27.262437	1424.751453	16.294055
26.789245	1434.051877	16.299072
27.366944	1425.345165	16.304090
27.030098	1429.259722	16.309107
26.799095	1430.071751	16.314125
27.343195	1424.520518	16.319143
27.085054	1433.023414	16.324160
27.305209	1433.128984	16.329178
26.727087	1436.506497	16.334195
27.094321	1429.607539	16.339213
27.415105	1424.643011	16.344231
27.101525	1436.919563	16.349248
27.031125	1438.887931	16.354266
27.261461	1459.222652	16.359283
27.459473	1464.545125	16.364301
27.988101	1443.282784	16.369319
27.796933	1451.864319	16.374336
28.113725	1438.305059	16.379354
28.151554	1429.101085	16.384371
28.338383	1417.941710	16.389389
28.197018	1414.098448	16.394407
28.124042	1412.328788	16.399424
28.375329	1396.147079	16.404442
27.783605	1400.708692	16.409459
27.843630	1383.660390	16.414477
28.070029	1372.714935	16.419495
27.554553	1376.996163	16.424512
27.851090	1368.976346	16.429530
27.858363	1377.416202	16.434547
27.825841	1373.247785	16.439565
27.772599	1371.185097	16.444583
27.641962	1395.340220	16.449600
28.199602	1401.430823	16.454618
27.978087	1401.554290	16.459635
28.047943	1400.808886	16.464653
28.285587	1404.661023	16.469671
27.858486	1404.291119	16.474688
28.051204	1398.217216	16.479706
28.034801	1403.371767	16.484723
28.008508	1400.271562	16.489741
28.100852	1403.338034	16.494759
28.049205	1405.543824	16.499776
28.432374	1397.108428	16.504794
28.208783	1408.018081	16.509811
28.330664	1411.854815	16.514829
28.251126	1405.702541	16.519847
28.055979	1410.125019	16.524864
28.405125	1408.352522	16.529882
28.028012	1408.009347	16.534899
28.114792	1414.094752	16.539917
28.410601	1407.815528	16.544935
28.221035	1413.333103	16.549952
28.669168	1421.712702	16.554970
28.491195	1425.900448	16.559987
28.097049	1442.769769	16.565005
28.603890	1425.549524	16.570023
28.596456	1442.901798	16.575040
28.590229	1438.051457	16.580058
28.494386	1440.048856	16.585075
28.276711	1428.940168	16.590093
28.664074	1431.024573	16.595111
28.544814	1440.167360	16.600128
28.829872	1436.808320	16.605146
28.632574	1437.804111	16.610163
28.682935	1438.263482	16.615181
28.830690	1431.869490	16.620199
28.458109	1439.621356	16.625216
28.970820	1439.614919	16.630234
28.624762	1446.338398	16.635251
29.143097	1454.683513	16.640269
29.097788	1461.612518	16.645287
28.522613	1473.568808	16.650304
28.901992	1454.322929	16.655322
29.177315	1467.625608	16.660339
28.683648	1467.826984	16.665357
29.040184	1463.135233	16.670375
29.187207	1454.668190	16.675392
29.173100	1464.620653	16.680410
28.999800	1466.503375	16.685427
28.640539	1462.669152	16.690445
29.181832	1466.791693	16.695463
29.245598	1484.826253	16.700480
29.573446	1486.991422	16.705498
29.751150	1479.473568	16.710515
29.607486	1470.833183	16.715533
29.847832	1460.090066	16.720551
29.733489	1462.418880	16.725568
29.825508	1460.248575	16.730586
29.841128	1447.764527	16.735603
29.864890	1451.595926	16.740621
29.903854	1447.357736	16.745639
29.350384	1456.030591	16.750656
29.450464	1460.429999	16.755674
29.881412	1451.237050	16.760691
29.649536	1461.324127	16.765709
29.961478	1451.299409	16.770727
29.845142	1461.104693	16.775744
29.707715	1452.565641	16.780762
29.929291	1454.025656	16.785779
29.715687	1460.941294	16.790797
29.116530	1457.021751	16.795815
29.244649	1455.228111	16.800832
29.752566	1451.028511	16.805850
29.708841	1463.834624	16.810867
29.614003	1482.772286	16.815885
29.868416	1479.685645	16.820903
29.696808	1488.871806	16.825920
29.771002	1488.877623	16.830938
29.649496	1479.136733	16.835955
29.658847	1488.567612	16.840973
29.942940	1493.676581	16.845991
30.374325	1511.202841	16.851008
30.219249	1513.486071	16.856026
30.760356	1508.986065	16.861043
29.840236	1498.866492	16.866061
30.485644	1505.061443	16.871079
30.479784	1516.526699	16.876096
30.424695	1502.936673	16.881114
30.476643	1484.436495	16.886131
30.297695	1492.008572	16.891149
30.498284	1501.709635	16.896167
30.334306	1514.615695	16.901184
30.407021	1511.450195	16.906202
30.773597	1513.519563	16.911219
30.662889	1510.340061	16.916237
31.074533	1508.114658	16.921255
30.712321	1496.966559	16.926272
30.868809	1487.530237	16.931290
30.750893	1483.173627	16.936307
30.813195	1475.093084	16.941325
30.966203	1474.431098	16.946343
30.796693	1472.797551	16.951360
31.004912	1475.395186	16.956378
31.009916	1462.441645	16.961395
31.141280	1475.154496	16.966413
30.767988	1465.831041	16.971431
30.732024	1472.607714	16.976448
30.934653	1465.209737	16.981466
31.017884	1465.532153	16.986483
30.802308	1473.205974	16.991501
31.245795	1473.672839	16.996519
30.795664	1478.257790	17.001536
30.827728	1481.609486	17.006554
31.221741	1476.492224	17.011571
31.042947	1479.371499	17.016589
31.251931	1469.350496	17.021607
30.895863	1475.316620	17.026624
30.887729	1494.365866	17.031642
31.120059	1500.227513	17.036659
31.352295	1514.509806	17.041677
31.655395	1507.380536	17.046695
31.513534	1505.238073	17.051712
31.365961	1499.654139	17.056730
31.447704	1488.858625	17.061747
31.683772	1503.703247	17.066765
31.688308	1503.556080	17.071783
31.626978	1500.375853	17.076800
31.925176	1491.759652	17.081818
32.222483	1479.081915	17.086835
31.886084	1465.431200	17.091853
31.911029	1454.099497	17.096871
31.986776	1452.388970	17.101888
31.507218	1456.669760	17.106906
31.643847	1445.807282	17.111923
31.522536	1455.189781	17.116941
31.864224	1455.175943	17.121959
31.758107	1444.721515	17.126976
31.308382	1446.780881	17.131994
31.575258	1463.017542	17.137011
31.712686	1478.322615	17.142029
31.767540	1495.534284	17.147047
31.995298	1485.085360	17.152064
31.841562	1493.613455	17.157082
32.102086	1485.411381	17.162099
32.175792	1490.614369	17.167117
32.285109	1480.383159	17.172135
32.115679	1490.087053	17.177152
31.612193	1488.597985	17.182170
31.914604	1479.329929	17.187187
31.918379	1493.706078	17.192205
31.949339	1493.954507	17.197223
32.118983	1504.383135	17.202240
32.282705	1517.097729	17.207258
32.651388	1512.797241	17.212275
32.512050	1517.019534	17.217293
32.588848	1521.677152	17.222311
32.561474	1515.756315	17.227328
32.626215	1517.670343	17.232346
32.833777	1507.259799	17.237363
32.418778	1503.180112	17.242381
32.578715	1495.524657	17.247399
32.492358	1503.838809	17.252416
32.455706	1513.249791	17.257434
32.796416	1511.536557	17.262451
32.638336	1512.638036	17.267469
32.736392	1519.151517	17.272487
32.790944	1514.217824	17.277504
32.394511	1520.848923	17.282522
32.728228	1505.853760	17.287539
32.765793	1521.245549	17.292557
32.890631	1517.742653	17.297575
33.098036	1512.983156	17.302592
32.763325	1514.280523	17.307610
32.760390	1514.629465	17.312627
32.391338	1516.384889	17.317645
32.419152	1518.853859	17.322663
32.557706	1528.314862	17.327680
33.063733	1538.772642	17.332698
33.177499	1540.267906	17.337715
33.065750	1550.759868	17.342733
33.030827	1546.726446	17.347751
32.837206	1547.874779	17.352768
32.848903	1551.839701	17.357786
33.089691	1542.344454	17.362803
32.812277	1551.382099	17.367821
33.060153	1559.163183	17.372839
33.806310	1565.541803	17.377856
33.425029	1567.994524	17.382874
33.800990	1558.400818	17.387891
33.782607	1558.914924	17.392909
33.794796	1551.947760	17.397927
33.895296	1558.260856	17.402944
33.552293	1547.925255	17.407962
34.003466	1531.345232	17.412979
33.705752	1530.069197	17.417997
33.762545	1532.883737	17.423015
33.887583	1525.258083	17.428032
33.722929	1532.498285	17.433050
33.639911	1523.335993	17.438067
33.885870	1536.569598	17.443085
33.560770	1527.442420	17.448103
33.643112	1544.394070	17.453120
33.650192	1555.037935	17.458138
33.750336	1552.657217	17.463155
33.909458	1556.107887	17.468173
33.906449	1561.025625	17.473191
34.190587	1560.029251	17.478208
34.315035	1554.254028	17.483226
34.030058	1563.605528	17.488243
34.039789	1562.273274	17.493261
34.013874	1559.553280	17.498279
34.261640	1552.221379	17.503296
33.882341	1562.494044	17.508314
33.846489	1557.958423	17.513331
34.152921	1569.346619	17.518349
34.315263	1578.425362	17.523367
34.437146	1593.091415	17.528384
34.563099	1592.039048	17.533402
34.504347	1580.175114	17.538419
34.726206	1573.575051	17.543437
34.698159	1585.548365	17.548455
34.822709	1582.484075	17.553472
34.521126	1581.655518	17.558490
34.667588	1575.954579	17.563507
34.568056	1572.393294	17.568525
34.626818	1585.596244	17.573543
34.873457	1572.650875	17.578560
34.797215	1580.918900	17.583578
34.721995	1574.585923	17.588595
34.646613	1581.551868	17.593613
34.309969	1577.495358	17.598631
34.706301	1573.333562	17.603648
34.543413	1577.577895	17.608666
34.866069	1583.487946	17.613683
34.568706	1579.131213	17.618701
34.529778	1595.491671	17.623719
34.983513	1600.503192	17.628736
35.048743	1609.954779	17.633754
35.280988	1604.175006	17.638771
35.061115	1598.294399	17.643789
35.199653	1613.196279	17.648807
35.601093	1603.526660	17.653824
35.462636	1607.046484	17.658842
35.745256	1600.713077	17.663859
35.477390	1601.963515	17.668877
35.209405	1599.893574	17.673895
35.663606	1602.928685	17.678912
35.204459	1603.010547	17.683930
35.474039	1598.605643	17.688947
35.443780	1601.512221	17.693965
35.521713	1607.317288	17.698983
35.494844	1603.815178	17.704000
35.639027	1611.119833	17.709018
35.305656	1602.102645	17.714035
35.593622	1611.864450	17.719053
35.489545	1606.273642	17.724071
35.597054	1605.153475	17.729088
35.304137	1598.196449	17.734106
35.471280	1608.916895	17.739123
35.437220	1622.676631	17.744141
35.558957	1634.064075	17.749159
36.166695	1634.012713	17.754176
35.775465	1640.070568	17.759194
35.974910	1632.731307	17.764211
35.832624	1632.502244	17.769229
35.750546	1629.236071	17.774247
35.867264	1635.492961	17.779264
35.914063	1631.164444	17.784282
35.890079	1650.671232	17.789299
36.550090	1658.017734	17.794317
36.427569	1660.313291	17.799335
36.766199	1660.491691	17.804352
36.141182	1648.595443	17.809370
36.804125	1645.451107	17.814387
36.409028	1622.981836	17.819405
35.984053	1630.502746	17.824423
36.220455	1631.478828	17.829440
36.188104	1646.150487	17.834458
36.722639	1649.726575	17.839475
36.662976	1651.338862	17.844493
36.346056	1657.825704	17.849511
36.998541	1652.063075	17.854528
36.877646	1651.577706	17.859546
36.919996	1655.900151	17.864563
36.942976	1650.730722	17.869581
36.735103	1641.309589	17.874599
36.709336	1647.280329	17.879616
36.634164	1647.877103	17.884634
36.939598	1646.776793	17.889651
36.816106	1648.315831	17.894669
36.691441	1659.272602	17.899687
37.024353	1634.367795	17.904704
37.041482	1639.973142	17.909722
36.827185	1647.925178	17.914739
36.938542	1659.760421	17.919757
37.075191	1653.648100	17.924775
37.024121	1642.559992	17.929792
37.103620	1645.674710	17.934810
37.604153	1658.110612	17.939827
37.365671	1655.906235	17.944845
37.212033	1647.086309	17.949863
37.460484	1637.131472	17.954880
37.392444	1645.706823	17.959898
37.214951	1641.512036	17.964915
37.602690	1640.828747	17.969933
37.434900	1658.226417	17.974951
37.182841	1660.992707	17.979968
37.601016	1658.766987	17.984986
37.381242	1671.834023	17.990003
37.866969	1661.177149	17.995021
37.792657	1677.662470	18.000039
37.844154	1675.448871	18.005056
38.108130	1663.305256	18.010074
37.843626	1665.504334	18.015091
37.920638	1665.384489	18.020109
37.784656	1673.430213	18.025127
38.003354	1664.620834	18.030144
37.836972	1668.742546	18.035162
38.079204	1673.306181	18.040179
38.082850	1653.813453	18.045197
37.797770	1651.850675	18.050215
37.975505	1666.901208	18.055232
38.052729	1666.460074	18.060250
37.944370	1665.762782	18.065267
38.292556	1664.839614	18.070285
38.131684	1664.750250	18.075303
38.153492	1661.675462	18.080320
38.315642	1672.642840	18.085338
38.027423	1664.290934	18.090355
38.200476	1666.379889	18.095373
38.006490	1664.887788	18.100391
38.454031	1687.576431	18.105408
38.896923	1686.746575	18.110426
38.823028	1688.591542	18.115443
38.719082	1688.847830	18.120461
38.608228	1684.607310	18.125479
38.757335	1681.271600	18.130496
38.577498	1680.307845	18.135514
38.162836	1694.798212	18.140531
38.703474	1687.544343	18.145549
38.515837	1695.534491	18.150567
38.468403	1696.446336	18.155584
38.683057	1685.170335	18.160602
38.386870	1689.528584	18.165619
38.718553	1701.829988	18.170637
38.913728	1714.972976	18.175655
39.078758	1715.211725	18.180672
39.404664	1719.076437	18.185690
39.484545	1718.749032	18.190707
39.655328	1708.679107	18.195725
39.165206	1692.955739	18.200743
38.899033	1691.315005	18.205760
39.343493	1697.344224	18.210778
39.717672	1710.210217	18.215795
39.437509	1697.289308	18.220813
39.283251	1686.541541	18.225831
39.405713	1686.328317	18.230848
39.420873	1707.334157	18.235866
39.286579	1707.088804	18.240883
39.689592	1703.966005	18.245901
39.819358	1713.379370	18.250919
39.648571	1716.212870	18.255936
39.655680	1716.306215	18.260954
39.600152	1723.114595	18.265971
39.696581	1715.862494	18.270989
39.806025	1717.544712	18.276007
39.518718	1718.950750	18.281024
39.906410	1716.118285	18.286042
39.825323	1713.257829	18.291059
40.024034	1707.993033	18.296077
39.786343	1703.948782	18.301095
39.728545	1709.737865	18.306112
40.132227	1711.332992	18.311130
39.697036	1719.354453	18.316147
40.021950	1706.575882	18.321165
39.882745	1709.313188	18.326183
39.816647	1710.805292	18.331200
40.244502	1727.033980	18.336218
40.145396	1727.597728	18.341235
39.849083	1736.916570	18.346253
40.257594	1731.196037	18.351271
40.051398	1737.693249	18.356288
40.456986	1733.218460	18.361306
40.120613	1729.052416	18.366323
40.598308	1728.667161	18.371341
40.073551	1732.305940	18.376359
40.199050	1732.267405	18.381376
40.507635	1743.912455	18.386394
40.432609	1759.249966	18.391411
40.742288	1760.961507	18.396429
41.017868	1763.715711	18.401447
40.675310	1760.642013	18.406464
40.792927	1754.717459	18.411482
40.635304	1758.935376	18.416499
40.909999	1759.846442	18.421517
41.025225	1754.360469	18.426535
41.228600	1750.627542	18.431552
41.148789	1752.838062	18.436570
40.878079	1757.429099	18.441587
40.992719	1748.055873	18.446605
40.860199	1755.309341	18.451623
41.030852	1752.761758	18.456640
40.942642	1749.867834	18.461658
41.047352	1751.083525	18.466675
41.042492	1767.083389	18.471693
41.253670	1778.908433	18.476711
41.326674	1784.225415	18.481728
41.541475	1770.821792	18.486746
41.420873	1783.577955	18.491763
41.573963	1776.121529	18.496781
41.737948	1775.399834	18.501799
41.728821	1778.124194	18.506816
41.771330	1770.111353	18.511834
41.321752	1774.135280	18.516851
41.738575	1768.877914	18.521869
41.879342	1778.182799	18.526887
41.918073	1778.440965	18.531904
42.240365	1765.820653	18.536922
41.839376	1779.958044	18.541939
42.315710	1772.727815	18.546957
42.245615	1768.492702	18.551975
42.177051	1763.849861	18.556992
42.667816	1769.141500	18.562010
42.199539	1758.512014	18.567027
42.114780	1744.021601	18.572045
42.041026	1746.287018	18.577063
42.005669	1764.239167	18.582080
42.325288	1763.310899	18.587098
42.134206	1773.649269	18.592115
42.371830	1772.786990	18.597133
42.287834	1766.054611	18.602151
42.286653	1770.750067	18.607168
42.441156	1764.337101	18.612186
42.236899	1765.663592	18.617203
42.315129	1761.790440	18.622221
42.878018	1757.139896	18.627239
42.491952	1763.944963	18.632256
42.805817	1757.090951	18.637274
42.818470	1766.296257	18.642291
42.947917	1761.552792	18.647309
43.006175	1756.739270	18.652327
42.677457	1767.392240	18.657344
42.802509	1752.434276	18.662362
42.748685	1756.021562	18.667379
42.613000	1755.969350	18.672397
42.970309	1755.245840	18.677415
42.471692	1768.617172	18.682432
42.912813	1767.939967	18.687450
43.099276	1784.740719	18.692467
43.298495	1788.580836	18.697485
43.277013	1789.650577	18.702503
42.750620	1788.431423	18.707520
43.400086	1790.146337	18.712538
43.166202	1792.743096	18.717555
43.137850	1791.804156	18.722573
43.537526	1777.830436	18.727591
43.454920	1786.183879	18.732608
43.940425	1766.338880	18.737626
44.120253	1778.548657	18.742643
43.886710	1776.168246	18.747661
44.167261	1770.444163	18.752679
43.773302	1773.604918	18.757696
43.946581	1765.171925	18.762714
43.949906	1752.850696	18.767731
43.683986	1746.357613	18.772749
43.918354	1752.024533	18.777767
43.987523	1764.745598	18.782784
43.956904	1767.878248	18.787802
43.992875	1755.761431	18.792819
43.830806	1761.935575	18.797837
44.059583	1769.705768	18.802855
44.071342	1779.947439	18.807872
43.929616	1772.810483	18.812890
44.027125	1772.521091	18.817907
43.620544	1774.110340	18.822925
44.300101	1766.533743	18.827943
44.069874	1778.551832	18.832960
44.026574	1769.058781	18.837978
43.938093	1778.672237	18.842995
44.134369	1795.889082	18.848013
44.435152	1800.263892	18.853031
44.226908	1794.892688	18.858048
44.686508	1793.604543	18.863066
44.400742	1794.892615	18.868083
44.242578	1796.741365	18.873101
44.627304	1796.827067	18.878119
44.647546	1811.089751	18.883136
44.860663	1819.666502	18.888154
44.833549	1827.357206	18.893171
44.609963	1829.629033	18.898189
45.078907	1825.010619	18.903207
44.867329	1826.282033	18.908224
45.125507	1825.166731	18.913242
45.243317	1818.954721	18.918259
44.960627	1837.231129	18.923277
45.368476	1814.065142	18.928295
45.287111	1829.451413	18.933312
45.400291	1823.568121	18.938330
45.327460	1831.755398	18.943347
45.057348	1818.556735	18.948365
45.236748	1819.317502	18.953383
45.324952	1817.846989	18.958400
45.345682	1825.001792	18.963418
45.497928	1826.789112	18.968435
45.188940	1821.551571	18.973453
45.238810	1824.035428	18.978471
45.340403	1833.160244	18.983488
45.951155	1841.651235	18.988506
45.698975	1850.630529	18.993523
45.894356	1851.376438	18.998541
45.903623	1848.838733	19.003559
45.850756	1855.751059	19.008576
45.888257	1849.912618	19.013594
46.100118	1847.340061	19.018611
45.782666	1845.054687	19.023629
46.481887	1844.311749	19.028647
45.925982	1851.815943	19.033664
45.907588	1844.384835	19.038682
45.993657	1844.875291	19.043699
46.155904	1849.658176	19.048717
46.403142	1834.556598	19.053735
46.291534	1850.873107	19.058752
46.339014	1839.148404	19.063770
46.310559	1845.050376	19.068787
46.059397	1841.980762	19.073805
46.411496	1838.974272	19.078823
46.123741	1849.000809	19.083840
46.537669	1853.880842	19.088858
46.752283	1856.053467	19.093875
46.771507	1870.903773	19.098893
46.797972	1873.827353	19.103911
46.567062	1877.960238	19.108928
46.499026	1876.652299	19.113946
46.496633	1867.582702	19.118963
46.684492	1885.139627	19.123981
46.969393	1876.334480	19.128999
46.781736	1873.833436	19.134016
46.909947	1863.007499	19.139034
47.083216	1874.015692	19.144051
46.852425	1874.464323	19.149069
47.304074	1882.369577	19.154087
47.139186	1883.576150	19.159104
47.071841	1896.504656	19.164122
47.051631	1890.232879	19.169139
47.115630	1902.831295	19.174157
47.510767	1885.561787	19.179175
47.593797	1889.383444	19.184192
47.459132	1891.601526	19.189210
47.415971	1887.627257	19.194227
47.310265	1893.408229	19.199245
47.323534	1891.173000	19.204263
47.517083	1897.563684	19.209280
48.072618	1907.265460	19.214298
47.968629	1902.484371	19.219315
48.049907	1893.678411	19.224333
48.018159	1879.417248	19.229351
47.838649	1891.633292	19.234368
48.108158	1895.008213	19.239386
48.078671	1889.100969	19.244403
47.911767	1910.235768	19.249421
48.176301	1914.144195	19.254439
48.175784	1920.698244	19.259456
48.105476	1917.419818	19.264474
48.367924	1915.573486	19.269491
48.315033	1921.566556	19.274509
48.299800	1912.847885	19.279527
48.356078	1911.037394	19.284544
48.425210	1911.719643	19.289562
48.721866	1908.350702	19.294579
48.034458	1917.050007	19.299597
48.625879	1909.314763	19.304615
48.724219	1913.502385	19.309632
48.093573	1916.432821	19.314650
48.491365	1909.153379	19.319667
48.446955	1921.399749	19.324685
48.824217	1924.530784	19.329703
48.953757	1936.847075	19.334720
48.463390	1949.470340	19.339738
48.987326	1938.280550	19.344755
48.976547	1938.733955	19.349773
48.819389	1933.319173	19.354791
49.104694	1931.230853	19.359808
49.118827	1942.970267	19.364826
49.256413	1933.860831	19.369843
48.799247	1933.749843	19.374861
49.036179	1929.175864	19.379879
48.969553	1946.425941	19.384896
49.131568	1953.476613	19.389914
49.486645	1963.796386	19.394931
49.055674	1966.023960	19.399949
49.739230	1958.472198	19.404967
49.982453	1954.873545	19.409984
49.995873	1947.953636	19.415002
50.021475	1949.001389	19.420019
50.012083	1948.308107	19.425037
50.442387	1943.990568	19.430055
50.316318	1926.813543	19.435072
49.835491	1924.659246	19.440090
50.184846	1918.179974	19.445107
50.054477	1922.163091	19.450125
49.939633	1912.495228	19.455143
49.938943	1918.037497	19.460160
50.107938	1923.428731	19.465178
50.559615	1926.529289	19.470195
50.090036	1929.937288	19.475213
50.348870	1934.845092	19.480231
50.428668	1941.018873	19.485248
50.255699	1947.461043	19.490266
50.236636	1943.908346	19.495283
49.925160	1947.520387	19.500301
50.346277	1949.163036	19.505319
50.206206	1952.244230	19.510336
50.348120	1955.365566	19.515354
50.876466	1950.238424	19.520371
50.445768	1957.459260	19.525389
50.571267	1966.346717	19.530407
50.766242	1977.269880	19.535424
50.861491	1969.585967	19.540442
50.884565	1981.469200	19.545459
50.821753	1983.069839	19.550477
50.835487	1972.808128	19.555495
50.965017	1970.495297	19.560512
50.916306	1981.933374	19.565530
51.148097	1973.053535	19.570547
50.941748	1974.349288	19.575565
51.093732	1988.640241	19.580583
51.551934	1989.818856	19.585600
51.510796	2001.245452	19.590618
51.443549	1997.466891	19.595635
51.529236	1999.813721	19.600653
51.918436	1997.285682	19.605671
51.438151	1997.805309	19.610688
51.613696	2004.098635	19.615706
51.986773	1996.707512	19.620723
51.884810	1994.265435	19.625741
52.051218	2001.350832	19.630759
52.159435	1989.621040	19.635776
51.628464	2003.893227	19.640794
52.046933	1990.450841	19.645811
51.755511	1992.965069	19.650829
52.173144	1981.744884	19.655847
52.207722	1987.343126	19.660864
52.025348	1990.520728	19.665882
52.094860	1991.903313	19.670899
52.108057	1992.644074	19.675917
52.093846	1988.424417	19.680935
52.255417	1988.510596	19.685952
52.356040	1988.605330	19.690970
52.587455	1995.899606	19.695987
52.235932	1987.268673	19.701005
52.224073	1994.769917	19.706023
52.569818	1987.399876	19.711040
52.266052	2002.247689	19.716058
52.456712	1999.651465	19.721075
52.400759	2021.425064	19.726093
52.250367	2008.939414	19.731111
52.942589	2016.614992	19.736128
52.758500	2016.338145	19.741146
52.695539	2024.850262	19.746163
52.551515	2035.510514	19.751181
53.219168	2041.568919	19.756199
53.367786	2053.002599	19.761216
53.508314	2051.222579	19.766234
53.710394	2047.882318	19.771251
53.394534	2031.062706	19.776269
53.287669	2022.037547	19.781287
53.619358	2008.904452	19.786304
53.421239	2022.242593	19.791322
53.454292	2021.874146	19.796339
53.670790	2032.986292	19.801357
53.654451	2035.811503	19.806375
54.025305	2050.263382	19.811392
53.548626	2057.090328	19.816410
53.680353	2044.764850	19.821427
53.824588	2044.055874	19.826445
54.015640	2052.011614	19.831463
54.044010	2046.958087	19.836480
54.002157	2040.361498	19.841498
54.035243	2047.265924	19.846515
54.040953	2045.660279	19.851533
54.189701	2046.072214	19.856551
53.847680	2040.870009	19.861568
54.049211	2051.734261	19.866586
54.069666	2041.478867	19.871603
54.055720	2043.545016	19.876621
53.846011	2048.016945	19.881639
53.953269	2062.894930	19.886656
53.962539	2072.132869	19.891674
54.545343	2064.750166	19.896691
54.591003	2071.388337	19.901709
54.882199	2068.985238	19.906727
54.634531	2062.829935	19.911744
54.292423	2065.398267	19.916762
54.845413	2088.225095	19.921779
55.174386	2083.032226	19.926797
54.963916	2086.425542	19.931815
55.719356	2076.024351	19.936832
55.554512	2057.728419	19.941850
55.554839	2044.218078	19.946867
55.321152	2042.350644	19.951885
55.464092	2045.515136	19.956903
55.639916	2035.155578	19.961920
55.318347	2042.900444	19.966938
55.908294	2039.983522	19.971955
55.817289	2044.179026	19.976973
55.750466	2040.709835	19.981991
55.817484	2036.639657	19.987008
55.684273	2036.644907	19.992026
55.610724	2036.680004	19.997043
55.898277	2044.576002	20.002061
55.639188	2035.026130	20.007079
56.202680	2036.533710	20.012096
55.693259	2042.971600	20.017114
55.871401	2042.472345	20.022131
55.886547	2031.662718	20.027149
55.599615	2039.782144	20.032167
55.761194	2031.581661	20.037184
55.771285	2034.164290	20.042202
55.970228	2032.397004	20.047219
55.768553	2032.652215	20.052237
55.697774	2057.146060	20.057255
56.072964	2062.169214	20.062272
56.011613	2072.061416	20.067290
56.186369	2064.274871	20.072307
56.040724	2067.833788	20.077325
55.934045	2084.632798	20.082343
56.270415	2098.803837	20.087360
56.293546	2097.547264	20.092378
56.471877	2099.627922	20.097395
56.665383	2096.866641	20.102413
56.496237	2105.466530	20.107431
56.712123	2116.875692	20.112448
56.935384	2126.343850	20.117466
57.232422	2117.960965	20.122483
57.482755	2119.209572	20.127501
57.403988	2131.289769	20.132519
57.429962	2122.541690	20.137536
57.271515	2121.616477	20.142554
57.604099	2125.288056	20.147571
57.573923	2122.651348	20.152589
57.604359	2136.436254	20.157607
57.831510	2117.087296	20.162624
57.467055	2104.153676	20.167642
57.421250	2093.354924	20.172659
57.777930	2104.140671	20.177677
57.556531	2118.356395	20.182695
58.022894	2126.619178	20.187712
57.266502	2125.472865	20.192730
57.152861	2125.753605	20.197747
57.565781	2122.013717	20.202765
57.630539	2126.782970	20.207783
58.013343	2133.648210	20.212800
58.004863	2141.443061	20.217818
58.285429	2142.735464	20.222835
58.468641	2136.469939	20.227853
58.269826	2144.168075	20.232871
58.418528	2140.517372	20.237888
58.390673	2138.820838	20.242906
58.024711	2151.092090	20.247923
58.335778	2138.650904	20.252941
57.925070	2133.704574	20.257959
58.474761	2144.352759	20.262976
58.556536	2160.274063	20.267994
58.722862	2171.315118	20.273011
58.972268	2165.692526	20.278029
58.968927	2164.108059	20.283047
58.938497	2159.625692	20.288064
59.090957	2161.107107	20.293082
59.141070	2166.732361	20.298099
59.019209	2156.542276	20.303117
59.084976	2163.922038	20.308135
59.369084	2155.712543	20.313152
59.366772	2157.662993	20.318170
59.063336	2159.893807	20.323187
59.143728	2163.900619	20.328205
58.958439	2167.344099	20.333223
59.286252	2149.909894	20.338240
59.251351	2163.664737	20.343258
59.497857	2183.135509	20.348275
59.886784	2186.780416	20.353293
59.492784	2186.443962	20.358311
59.964236	2177.770243	20.363328
60.020390	2177.427086	20.368346
59.930421	2190.874566	20.373363
59.988742	2179.287570	20.378381
59.895521	2178.240882	20.383399
60.250473	2176.049615	20.388416
60.056289	2174.816948	20.393434
60.161159	2171.987706	20.398451
60.321450	2176.571409	20.403469
60.281890	2183.057254	20.408487
60.462014	2172.875633	20.413504
60.343551	2169.951617	20.418522
60.381601	2180.799428	20.423539
60.511776	2169.559952	20.428557
60.506373	2180.334275	20.433575
60.470957	2170.033751	20.438592
60.532153	2180.200540	20.443610
60.507055	2197.888490	20.448627
60.789481	2204.968085	20.453645
60.413381	2204.890865	20.458663
61.055423	2207.768895	20.463680
60.959353	2210.400693	20.468698
61.096284	2206.757442	20.473715
60.604200	2194.226853	20.478733
61.063465	2209.118920	20.483751
60.901631	2216.503461	20.488768
61.309662	2220.184965	20.493786
61.336791	2225.291216	20.498803
61.685154	2222.580163	20.503821
61.112103	2222.233306	20.508839
61.581745	2227.136485	20.513856
61.794575	2219.622280	20.518874
61.483088	2227.039178	20.523891
61.657928	2216.587535	20.528909
61.240406	2241.694031	20.533927
61.568793	2243.776149	20.538944
61.683570	2253.001780	20.543962
61.622481	2262.812955	20.548979
61.575776	2253.694196	20.553997
61.966756	2269.520916	20.559015
61.728838	2290.926307	20.564032
62.325179	2283.770391	20.569050
62.077144	2290.890547	20.574067
62.422633	2284.575944	20.579085
62.051419	2292.374461	20.584103
62.408002	2289.949044	20.589120
62.721674	2285.034642	20.594138
62.312384	2285.883035	20.599155
62.917222	2280.184795	20.604173
62.503498	2278.516942	20.609191
62.646079	2305.480103	20.614208
62.741693	2305.532757	20.619226
62.590992	2314.833649	20.624243
63.047565	2307.383620	20.629261
62.951556	2313.741496	20.634279
63.203259	2305.285335	20.639296
63.199017	2309.840909	20.644314
63.032875	2320.247545	20.649331
63.507817	2305.983673	20.654349
63.130166	2309.838690	20.659367
63.509447	2309.961919	20.664384
63.494380	2308.949872	20.669402
63.284600	2314.146707	20.674419
63.828539	2316.343016	20.679437
64.049277	2329.331487	20.684455
64.091572	2331.202102	20.689472
63.921067	2313.510760	20.694490
63.634000	2309.713143	20.699507
63.910303	2307.609734	20.704525
64.174553	2324.087114	20.709543
64.104076	2322.009839	20.714560
64.022150	2315.943822	20.719578
64.187954	2323.644837	20.724595
64.360182	2326.069068	20.729613
64.210526	2329.964153	20.734631
64.114698	2326.494206	20.739648
64.437855	2326.957087	20.744666
64.252092	2334.292903	20.749683
64.067684	2319.514961	20.754701
64.363612	2327.481367	20.759719
64.259137	2322.146671	20.764736
64.459148	2331.512911	20.769754
64.359984	2345.516397	20.774771
64.540853	2352.681838	20.779789
64.762610	2348.205144	20.784807
64.656184	2349.647317	20.789824
65.018089	2362.411956	20.794842
65.349288	2379.351115	20.799859
65.269531	2381.142805	20.804877
65.507807	2371.700623	20.809895
65.349848	2366.521655	20.814912
65.950421	2359.978404	20.819930
66.273744	2362.106263	20.824947
66.306698	2345.650002	20.829965
66.033173	2332.155789	20.834983
65.840223	2334.775361	20.840000
66.128763	2333.560489	20.845018
65.625454	2325.914457	20.850035
65.712596	2331.799765	20.855053
65.733064	2331.078275	20.860071
65.346294	2339.508943	20.865088
65.879103	2330.876126	20.870106
65.929178	2348.024968	20.875123
65.946645	2355.353791	20.880141
66.066495	2366.450349	20.885159
66.082269	2374.751930	20.890176
66.343964	2374.089956	20.895194
66.088311	2373.000956	20.900211
66.326198	2362.877330	20.905229
66.381145	2373.280723	20.910247
65.847887	2393.180571	20.915264
66.506424	2385.109129	20.920282
66.569937	2389.223139	20.925299
66.489314	2394.874534	20.930317
66.525916	2393.270019	20.935335
66.760741	2414.215505	20.940352
66.845823	2419.084623	20.945370
67.295601	2426.086506	20.950387
67.653194	2404.951679	20.955405
67.820019	2414.295138	20.960423
67.498618	2423.979592	20.965440
67.773145	2419.800023	20.970458
67.421339	2426.513851	20.975475
67.538336	2419.645418	20.980493
67.440579	2410.498043	20.985511
67.588419	2416.761889	20.990528
67.818904	2416.900401	20.995546
67.777423	2411.009519	21.000563
68.079325	2403.565072	21.005581
68.313455	2392.132170	21.010599
67.747344	2401.615146	21.015616
68.193988	2392.991103	21.020634
68.054539	2401.475586	21.025651
68.129625	2405.249872	21.030669
68.311480	2395.642244	21.035687
68.378444	2402.170714	21.040704
68.302311	2395.285568	21.045722
68.038842	2397.437329	21.050739
68.208442	2404.168828	21.055757
68.279524	2400.317178	21.060775
68.189396	2416.229123	21.065792
68.733414	2420.559357	21.070810
68.336614	2429.209464	21.075827
68.317407	2434.786490	21.080845
68.648214	2430.040067	21.085863
68.517197	2433.391512	21.090880
68.523620	2426.247349	21.095898
68.788641	2451.120666	21.100915
68.721444	2463.177149	21.105933
69.270993	2454.034773	21.110951
69.071042	2465.981821	21.115968
69.366408	2465.259916	21.120986
69.153209	2471.806235	21.126003
69.546146	2483.739018	21.131021
69.755603	2484.854680	21.136039
69.719651	2490.009298	21.141056
69.902867	2481.845536	21.146074
69.818653	2490.705941	21.151091
69.928589	2491.992086	21.156109
70.210855	2486.600934	21.161127
70.066207	2483.536717	21.166144
70.272152	2481.376079	21.171162
70.329582	2475.601416	21.176179
70.168703	2484.711574	21.181197
70.043875	2481.230664	21.186215
69.923050	2487.289574	21.191232
70.282342	2477.918164	21.196250
69.938377	2487.710742	21.201267
70.291261	2500.467940	21.206285
70.766694	2503.641838	21.211303
70.533899	2513.127363	21.216320
70.815055	2509.419520	21.221338
70.824102	2506.260462	21.226355
70.692849	2500.095479	21.231373
71.026776	2504.002762	21.236391
70.941041	2500.837409	21.241408
71.082029	2505.706318	21.246426
70.881651	2508.109035	21.251443
70.908863	2525.829216	21.256461
71.312612	2524.890470	21.261479
71.110359	2538.411243	21.266496
71.426271	2534.268468	21.271514
71.385188	2533.822955	21.276531
71.282987	2542.551334	21.281549
71.552601	2535.315741	21.286567
71.363289	2560.118277	21.291584
71.812892	2567.404517	21.296602
71.984287	2569.830107	21.301619
72.050327	2567.570656	21.306637
72.386947	2559.758146	21.311655
71.840765	2571.505718	21.316672
72.095380	2559.612578	21.321690
72.127386	2563.701161	21.326707
72.104223	2561.579375	21.331725
72.527948	2558.719908	21.336743
72.313242	2562.129779	21.341760
72.354465	2576.454249	21.346778
72.520470	2574.310078	21.351795
72.701068	2588.585411	21.356813
72.875542	2583.481837	21.361831
72.852566	2589.037497	21.366848
72.958964	2592.820405	21.371866
73.192714	2583.565076	21.376883
73.017357	2588.493671	21.381901
73.045280	2579.344208	21.386919
73.046415	2593.905287	21.391936
72.908873	2592.171025	21.396954
73.168528	2591.751124	21.401971
73.430636	2598.758684	21.406989
73.459376	2577.226683	21.412007
73.166299	2584.102873	21.417024
73.310286	2599.715457	21.422042
73.509219	2607.867032	21.427059
73.130464	2604.762954	21.432077
73.719145	2611.185122	21.437095
73.493491	2605.386588	21.442112
73.254049	2620.798732	21.447130
73.528519	2624.680099	21.452147
74.196982	2635.052576	21.457165
74.563704	2633.545149	21.462183
74.422574	2633.424542	21.467200
74.523731	2629.545789	21.472218
75.022639	2625.828897	21.477235
74.577283	2626.504945	21.482253
75.045428	2620.358809	21.487271
74.745722	2623.581629	21.492288
74.807699	2620.473990	21.497306
75.027689	2613.918684	21.502323
74.701725	2620.942487	21.507341
74.733458	2621.623897	21.512359
74.821961	2617.493696	21.517376
74.803284	2623.541982	21.522394
74.806733	2623.769017	21.527411
75.057337	2643.117634	21.532429
75.407511	2637.387177	21.537447
75.368471	2642.761267	21.542464
75.470422	2646.598472	21.547482
75.286823	2642.995003	21.552499
75.486766	2647.072234	21.557517
75.537352	2650.076994	21.562535
75.510214	2644.741933	21.567552
75.761416	2655.861753	21.572570
76.032596	2668.238162	21.577587
75.900235	2675.845590	21.582605
75.921255	2677.156765	21.587623
76.186269	2679.131360	21.592640
76.026984	2677.538110	21.597658
76.186724	2672.470815	21.602675
76.014599	2681.096713	21.607693
76.119482	2668.071628	21.612711
76.176621	2685.670083	21.617728
75.923816	2695.528353	21.622746
76.529153	2692.652067	21.627763
76.471003	2702.778006	21.632781
76.381481	2699.933730	21.637799
76.664162	2717.812864	21.642816
76.981970	2722.277634	21.647834
77.330829	2715.362663	21.652851
77.428156	2714.741773	21.657869
77.972160	2715.318367	21.662887
77.872348	2709.274066	21.667904
77.213610	2694.095832	21.672922
77.445037	2697.286306	21.677939
77.714526	2710.318573	21.682957
77.841401	2711.104259	21.687975
78.000492	2704.794481	21.692992
77.877767	2690.476823	21.698010
78.189890	2678.718530	21.703027
77.566141	2684.087440	21.708045
77.886325	2686.227285	21.713063
77.968236	2691.768700	21.718080
78.025676	2715.280809	21.723098
78.305797	2702.015538	21.728115
77.771646	2715.249086	21.733133
78.442231	2710.331933	21.738151
78.151128	2708.471595	21.743168
78.040591	2715.491924	21.748186
78.449453	2702.056431	21.753203
77.879137	2716.266903	21.758221
78.333706	2726.564354	21.763239
78.779224	2723.827621	21.768256
78.117468	2739.648272	21.773274
78.560994	2731.330877	21.778291
78.704621	2755.140156	21.783309
78.947365	2754.880157	21.788327
79.219155	2762.837807	21.793344
79.201821	2763.982913	21.798362
79.347417	2765.066688	21.803379
79.070678	2767.871131	21.808397
79.207768	2769.104753	21.813415
79.587894	2777.875553	21.818432
79.528507	2788.282083	21.823450
79.921634	2787.228546	21.828467
79.961782	2781.849577	21.833485
79.787992	2784.712509	21.838503
80.157376	2783.329436	21.843520
80.066940	2791.737871	21.848538
80.365218	2778.989625	21.853555
80.382668	2776.793340	21.858573
80.670965	2779.805473	21.863591
80.622627	2785.254783	21.868608
80.495169	2790.524319	21.873626
80.439789	2776.707622	21.878643
80.179569	2788.874393	21.883661
80.599074	2787.662133	21.888679
80.829697	2786.982079	21.893696
80.718682	2805.233845	21.898714
80.993146	2805.959574	21.903731
81.206744	2813.242632	21.908749
81.100930	2815.971431	21.913767
81.113959	2815.059018	21.918784
80.957509	2815.530751	21.923802
81.012684	2811.904884	21.928819
81.236669	2822.556880	21.933837
81.650090	2834.389674	21.938855
81.642520	2839.848370	21.943872
81.434381	2845.710501	21.948890
81.720942	2844.350636	21.953907
81.806603	2842.938721	21.958925
81.930191	2836.608411	21.963943
82.301288	2836.777894	21.968960
82.152862	2837.192386	21.973978
82.441811	2826.483957	21.978995
82.675930	2827.516015	21.984013
82.524718	2830.560253	21.989031
82.374558	2824.047082	21.994048
82.386406	2829.383643	21.999066
82.408690	2831.327727	22.004083
82.347093	2834.253130	22.009101
82.312318	2847.176225	22.014119
82.634424	2853.106546	22.019136
82.440292	2859.398268	22.024154
82.429969	2853.423296	22.029171
82.714780	2864.271916	22.034189
82.981518	2873.205717	22.039207
83.676133	2880.316342	22.044224
83.259350	2888.618425	22.049242
83.669163	2879.174203	22.054259
83.580582	2886.361442	22.059277
83.456501	2884.600499	22.064295
83.843764	2877.796011	22.069312
83.938579	2872.707156	22.074330
84.067987	2872.846329	22.079347
83.848277	2872.988793	22.084365
83.877591	2873.835193	22.089383
83.961281	2870.634520	22.094400
83.719032	2881.359708	22.099418
83.856303	2872.451758	22.104435
83.818622	2875.446820	22.109453
83.994600	2891.965066	22.114471
84.550134	2895.485994	22.119488
84.098690	2906.620397	22.124506
84.542190	2899.959319	22.129523
84.386576	2905.211525	22.134541
84.555634	2898.458647	22.139559
84.580053	2915.639152	22.144576
84.418822	2917.936994	22.149594
84.811617	2925.365138	22.154611
84.968401	2925.745446	22.159629
85.318504	2925.568397	22.164647
85.815433	2913.116970	22.169664
85.820211	2913.878074	22.174682
86.000440	2910.266049	22.179699
86.100716	2898.497914	22.184717
85.699300	2905.162312	22.189735
86.077258	2903.865212	22.194752
85.739026	2912.566483	22.199770
85.855026	2912.641739	22.204787
85.891578	2913.667264	22.209805
86.393106	2914.631264	22.214823
85.917924	2910.771446	22.219840
85.825876	2922.254426	22.224858
86.256910	2936.397903	22.229875
86.213392	2951.421096	22.234893
86.225186	2939.641649	22.239911
86.446951	2941.884506	22.244928
86.301714	2934.277488	22.249946
86.452637	2952.776860	22.254963
86.695910	2968.610338	22.259981
86.309300	2966.852067	22.264999
86.953360	2962.685751	22.270016
86.933225	2975.399419	22.275034
86.930890	2961.779268	22.280051
86.947146	2986.552256	22.285069
87.500012	2992.855726	22.290087
87.946861	2995.145836	22.295104
87.897775	3003.953841	22.300122
87.743806	2999.064962	22.305139
87.726470	2985.563038	22.310157
87.609188	2988.782782	22.315175
87.647409	2993.013762	22.320192
87.611695	2990.158914	22.325210
88.020864	2982.343981	22.330227
87.869965	2992.548518	22.335245
88.071264	3010.837605	22.340263
88.301427	3014.372867	22.345280
88.240251	3022.072579	22.350298
88.109350	3018.855172	22.355315
88.578703	3013.484328	22.360333
88.502205	3025.926677	22.365351
88.494796	3020.632306	22.370368
88.754130	3040.798527	22.375386
88.881706	3036.712907	22.380403
88.878544	3038.040730	22.385421
89.138502	3043.569219	22.390439
89.438387	3030.639780	22.395456
89.200507	3036.643547	22.400474
88.995767	3033.838043	22.405491
89.357830	3025.426938	22.410509
89.454157	3030.791264	22.415527
89.619363	3042.939897	22.420544
89.633482	3046.428387	22.425562
89.829586	3060.170437	22.430579
89.754853	3056.244426	22.435597
89.925004	3062.493015	22.440615
89.870579	3064.103395	22.445632
89.958488	3059.611339	22.450650
90.034436	3067.189852	22.455667
90.306248	3052.849210	22.460685
90.023449	3070.222290	22.465703
90.104020	3086.084896	22.470720
90.188955	3094.061170	22.475738
90.458908	3088.269074	22.480755
90.230058	3093.329168	22.485773
90.097944	3123.476243	22.490791
90.356968	3123.096203	22.495808
90.632563	3126.273127	22.500826
90.901201	3142.539608	22.505843
91.289970	3149.402737	22.510861
91.334760	3152.917653	22.515879
92.011321	3147.626510	22.520896
91.908265	3142.025921	22.525914
92.035783	3132.300484	22.530931
92.583311	3126.334676	22.535949
92.123094	3120.792663	22.540967
92.546796	3096.707505	22.545984
92.413092	3093.911052	22.551002
91.870320	3095.297057	22.556019
92.294563	3093.321335	22.561037
91.943515	3096.898083	22.566055
92.243881	3109.681442	22.571072
92.152828	3125.385194	22.576090
92.040244	3125.939417	22.581107
92.473228	3138.110164	22.586125
92.337397	3127.070517	22.591143
92.482003	3144.958522	22.596160
92.725492	3155.702395	22.601178
92.627583	3156.314421	22.606195
92.725463	3160.283543	22.611213
92.839459	3166.587966	22.616231
93.221702	3184.301475	22.621248
93.227684	3193.749305	22.626266
92.762321	3195.364599	22.631283
93.399926	3187.960063	22.636301
93.466132	3188.964141	22.641319
93.792160	3199.495493	22.646336
94.012637	3221.540604	22.651354
93.806639	3221.587871	22.656371
94.273670	3209.567591	22.661389
94.186157	3215.764960	22.666407
94.285116	3202.178163	22.671424
94.580586	3210.601831	22.676442
94.204983	3223.667713	22.681459
94.765373	3213.513960	22.686477
94.591565	3217.017182	22.691495
94.760929	3203.765168	22.696512
94.932812	3204.533164	22.701530
94.606085	3208.513015	22.706547
94.589487	3198.350032	22.711565
94.809578	3220.663732	22.716583
95.053214	3219.724784	22.721600
95.331663	3231.964991	22.726618
94.999016	3225.486703	22.731635
95.652263	3236.433818	22.736653
95.396490	3239.599063	22.741671
95.337082	3230.283401	22.746688
95.347197	3230.603045	22.751706
95.227638	3232.805417	22.756723
95.927898	3234.307721	22.761741
95.886022	3246.838988	22.766759
96.098262	3243.788544	22.771776
96.058639	3251.630862	22.776794
95.916167	3261.160495	22.781811
95.870398	3250.925547	22.786829
96.081745	3268.973878	22.791847
96.404934	3281.903599	22.796864
96.673725	3284.576131	22.801882
96.617838	3280.434708	22.806899
96.704022	3280.472004	22.811917
96.518121	3287.327145	22.816935
96.798023	3295.140009	22.821952
97.026066	3309.550652	22.826970
96.903983	3313.027975	22.831987
97.235198	3300.423057	22.837005
97.401742	3314.059211	22.842023
97.317373	3309.759901	22.847040
97.420533	3313.376973	22.852058
97.633898	3330.918696	22.857075
98.226517	3338.513456	22.862093
98.330701	3334.848219	22.867111
98.679338	3319.736624	22.872128
98.955718	3301.361570	22.877146
98.405591	3293.477144	22.882163
98.514914	3281.068972	22.887181
98.365076	3287.742121	22.892199
98.693209	3283.314420	22.897216
98.787452	3280.060724	22.902234
98.477805	3281.401309	22.907251
98.588424	3290.916068	22.912269
98.819525	3306.749158	22.917287
98.981348	3315.757742	22.922304
99.037228	3315.211834	22.927322
98.571531	3316.034212	22.932339
98.968160	3315.474987	22.937357
98.837075	3340.869926	22.942375
98.750256	3343.784260	22.947392
99.520553	3341.747062	22.952410
99.351246	3350.527204	22.957427
99.401086	3359.132337	22.962445
99.862910	3375.090555	22.967463
99.868906	3368.593728	22.972480
100.101844	3374.956430	22.977498
99.995642	3372.522713	22.982515
100.413282	3367.842296	22.987533
100.320372	3366.289128	22.992551
100.343169	3389.752889	22.997568
100.863062	3383.659676	23.002586
100.539388	3389.686498	23.007603
100.614707	3386.442619	23.012621
100.842789	3385.832655	23.017639
101.101932	3387.208657	23.022656
100.941052	3388.950945	23.027674
100.775626	3385.795898	23.032691
100.940179	3392.581820	23.037709
101.259431	3410.218252	23.042727
101.425877	3415.728947	23.047744
101.805509	3409.084964	23.052762
101.763598	3411.155547	23.057779
101.935118	3400.062661	23.062797
101.828468	3402.126284	23.067815
101.888195	3413.908448	23.072832
101.983379	3405.409984	23.077850
101.726336	3408.892038	23.082867
102.043045	3418.915985	23.087885
102.482179	3437.095569	23.092903
102.260137	3446.147546	23.097920
102.610695	3430.049999	23.102938
102.295826	3439.610359	23.107955
102.275164	3429.550666	23.112973
102.104587	3440.887219	23.117991
102.020208	3462.397451	23.123008
102.519872	3468.488284	23.128026
102.491106	3479.945801	23.133043
103.025266	3486.643174	23.138061
103.428960	3485.268910	23.143079
103.205065	3501.267977	23.148096
103.645728	3485.605050	23.153114
103.379839	3505.989092	23.158131
103.668876	3507.304620	23.163149
103.821819	3515.760803	23.168167
103.622074	3520.966605	23.173184
104.348773	3514.633049	23.178202
104.166968	3510.172299	23.183219
104.304033	3514.978392	23.188237
104.294453	3516.475056	23.193255
104.185473	3530.984829	23.198272
104.556113	3525.552651	23.203290
104.584260	3533.587412	23.208307
104.955472	3543.532295	23.213325
104.704356	3545.352201	23.218343
105.032608	3550.317891	23.223360
105.133977	3555.383104	23.228378
105.044810	3572.678888	23.233395
105.298554	3567.276359	23.238413
105.471140	3568.905370	23.243431
105.061103	3569.451553	23.248448
105.457228	3563.947009	23.253466
105.437827	3577.456797	23.258483
105.762456	3589.825453	23.263501
105.808406	3595.092823	23.268519
105.763245	3596.990331	23.273536
106.215531	3590.162526	23.278554
105.974959	3604.350499	23.283571
106.053093	3624.236138	23.288589
106.411763	3622.613019	23.293607
106.451397	3618.977342	23.298624
107.075588	3610.635763	23.303642
108.239935	3586.519301	23.308659
108.148143	3574.028166	23.313677
108.243474	3581.235953	23.318695
108.093331	3562.240851	23.323712
108.407600	3548.271480	23.328730
108.103627	3556.275215	23.333747
108.322836	3528.993516	23.338765
108.357277	3504.241638	23.343783
108.027135	3511.445289	23.348800
108.157811	3505.869906	23.353818
108.108310	3511.159016	23.358835
108.179144	3511.849323	23.363853
107.926006	3502.710194	23.368871
107.819224	3505.605825	23.373888
108.462671	3522.242352	23.378906
108.233571	3542.613635	23.383923
108.276926	3542.576939	23.388941
108.519959	3543.218156	23.393959
108.559255	3543.279783	23.398976
108.419661	3543.017558	23.403994
108.596227	3559.643119	23.409011
108.834699	3576.750982	23.414029
109.060638	3576.538653	23.419047
108.711696	3581.647603	23.424064
108.976037	3581.537565	23.429082
108.949858	3584.932862	23.434099
109.360703	3595.359828	23.439117
109.133366	3595.540575	23.444135
109.245841	3615.314186	23.449152
109.775498	3623.134535	23.454170
109.954243	3623.083215	23.459187
110.056975	3623.540643	23.464205
110.228849	3626.892011	23.469223
109.927519	3628.658846	23.474240
110.339033	3635.527470	23.479258
110.318501	3648.201984	23.484275
110.659091	3650.099181	23.489293
110.748919	3652.270752	23.494311
110.430986	3668.360822	23.499328
110.823806	3657.053006	23.504346
110.672604	3681.383219	23.509363
110.699709	3686.221420	23.514381
111.142851	3687.533799	23.519399
111.153977	3694.287076	23.524416
111.275783	3712.346863	23.529434
111.127437	3717.696568	23.534451
111.197003	3722.221783	23.539469
112.142434	3737.441271	23.544487
111.938080	3746.748385	23.549504
111.843307	3741.954564	23.554522
111.567075	3748.050812	23.559539
111.725292	3756.810616	23.564557
112.164592	3767.451891	23.569575
112.450812	3781.022891	23.574592
112.643803	3777.546360	23.579610
112.844100	3778.290370	23.584627
112.697654	3786.811809	23.589645
113.204407	3794.634083	23.594663
113.019567	3806.223693	23.599680
113.186848	3806.347526	23.604698
113.493924	3804.565621	23.609715
113.613505	3806.251109	23.614733
113.808326	3800.323190	23.619751
113.351325	3812.114350	23.624768
114.339494	3813.879934	23.629786
114.111356	3822.907546	23.634803
113.930992	3831.218872	23.639821
114.729060	3817.151934	23.644839
114.679955	3821.200382	23.649856
114.461688	3812.723074	23.654874
114.962106	3807.219621	23.659891
114.780386	3818.219675	23.664909
115.016789	3815.224169	23.669927
114.806659	3818.625673	23.674944
114.871083	3808.009800	23.679962
115.200898	3809.683190	23.684979
115.448622	3809.920442	23.689997
115.534230	3803.201518	23.695015
115.435113	3804.987137	23.700032
115.334679	3795.709061	23.705050
115.638967	3814.719467	23.710067
115.572855	3823.512650	23.715085
115.568655	3825.456928	23.720103
115.497521	3835.171141	23.725120
115.821404	3839.781309	23.730138
116.046703	3845.330808	23.735155
116.070805	3865.232034	23.740173
116.222351	3855.437974	23.745191
116.124509	3863.890741	23.750208
116.218338	3868.287542	23.755226
116.523854	3882.573623	23.760243
116.674084	3897.388341	23.765261
116.674385	3889.965750	23.770279
116.550987	3899.553632	23.775296
116.838595	3919.313881	23.780314
116.924038	3919.853729	23.785331
117.112506	3933.430081	23.790349
117.373473	3939.726538	23.795367
117.439917	3951.215828	23.800384
117.905627	3948.304254	23.805402
118.176036	3940.932828	23.810419
117.879230	3953.023498	23.815437
118.038873	3947.526226	23.820455
118.245924	3952.698826	23.825472
118.453621	3964.218596	23.830490
118.806285	3961.543157	23.835507
118.843367	3965.281612	23.840525
119.074892	3967.775001	23.845543
118.972246	3972.675015	23.850560
119.064248	3962.003661	23.855578
119.195088	3970.207825	23.860595
119.166262	3970.922196	23.865613
119.381215	3966.672189	23.870631
119.215020	3978.033601	23.875648
119.388861	3993.071681	23.880666
119.398034	4001.829222	23.885683
119.146177	4003.145692	23.890701
119.566789	4005.184774	23.895719
119.432844	4025.653877	23.900736
119.802929	4028.757799	23.905754
120.366959	4033.922291	23.910771
120.421375	4056.311576	23.915789
120.614712	4058.057680	23.920807
120.329877	4064.744929	23.925824
120.801241	4063.153834	23.930842
121.180398	4042.323102	23.935859
121.155608	4051.892328	23.940877
121.580687	4045.577974	23.945895
121.655681	4059.723367	23.950912
121.449723	4047.552835	23.955930
121.523926	4059.710296	23.960947
121.395428	4078.295632	23.965965
121.711503	4071.500494	23.970983
121.545600	4084.008548	23.976000
122.024166	4070.872552	23.981018
122.077583	4092.227661	23.986035
122.400327	4115.148109	23.991053
122.369811	4117.466534	23.996071
122.561313	4118.493558	24.001088
122.341340	4117.682397	24.006106
122.736446	4106.774722	24.011123
122.090393	4119.245255	24.016141
122.651267	4114.869998	24.021159
122.782764	4136.736674	24.026176
122.777396	4129.620073	24.031194
123.153157	4146.432480	24.036211
123.165791	4151.220859	24.041229
123.429473	4149.913910	24.046247
123.804064	4153.212018	24.051264
124.007953	4171.149624	24.056282
124.205993	4171.511298	24.061299
123.992623	4175.982073	24.066317
124.475729	4174.772142	24.071335
124.292440	4173.800135	24.076352
124.052547	4177.683895	24.081370
124.331872	4170.197479	24.086387
124.871288	4204.079685	24.091405
124.850546	4199.551808	24.096423
124.784813	4213.500221	24.101440
124.898260	4199.646728	24.106458
125.359928	4194.608704	24.111475
125.337366	4196.023325	24.116493
125.769687	4194.679686	24.121511
125.651058	4187.475565	24.126528
125.419493	4197.214300	24.131546
126.102637	4178.018549	24.136563
126.262152	4193.432879	24.141581
126.326284	4194.413742	24.146599
126.226397	4197.675730	24.151616
126.084700	4204.080552	24.156634
126.473759	4201.712850	24.161651
126.375478	4217.830769	24.166669
126.474546	4203.466989	24.171687
126.790188	4209.447339	24.176704
126.646074	4221.425820	24.181722
126.699143	4226.428008	24.186739
126.544152	4241.506403	24.191757
126.628122	4251.930246	24.196775
126.906684	4271.408938	24.201792
126.921634	4269.503060	24.206810
127.383428	4286.899048	24.211827
127.327387	4294.761548	24.216845
128.155395	4298.182008	24.221863
127.981264	4297.025765	24.226880
127.946894	4319.836541	24.231898
128.264942	4330.139636	24.236915
128.441919	4338.212293	24.241933
128.341846	4333.471541	24.246951
128.416020	4331.662917	24.251968
128.411876	4359.324587	24.256986
128.936973	4353.442773	24.262003
128.717363	4357.802020	24.267021
128.977604	4364.270844	24.272039
129.265720	4381.702887	24.277056
129.243077	4389.292125	24.282074
129.873123	4384.950584	24.287091
129.358580	4395.622036	24.292109
130.001777	4409.263023	24.297127
130.185437	4414.222306	24.302144
129.983784	4422.270510	24.307162
130.289730	4420.335945	24.312179
129.955242	4425.457726	24.317197
130.370140	4428.869687	24.322215
130.845510	4433.993134	24.327232
130.944261	4448.783065	24.332250
130.992016	4444.000389	24.337267
130.936718	4447.868503	24.342285
130.710336	4450.378998	24.347303
131.107192	4452.778052	24.352320
131.245681	4471.707737	24.357338
131.534233	4468.734944	24.362355
131.296191	4477.125497	24.367373
131.587244	4497.122163	24.372391
131.997407	4502.935319	24.377408
131.872843	4506.629101	24.382426
132.425837	4506.916836	24.387443
132.188529	4503.362020	24.392461
132.231654	4534.901033	24.397479
132.390662	4545.678018	24.402496
132.744686	4540.030897	24.407514
132.532051	4541.459415	24.412531
132.767187	4537.555172	24.417549
133.159097	4542.040448	24.422567
133.457310	4544.505523	24.427584
133.658530	4552.171044	24.432602
133.922128	4545.920735	24.437619
133.948695	4551.579507	24.442637
133.726756	4541.936076	24.447655
134.201089	4545.142879	24.452672
133.951170	4548.586589	24.457690
134.405529	4543.830032	24.462707
134.227258	4548.936918	24.467725
134.447342	4565.930790	24.472743
134.467642	4568.342822	24.477760
134.679559	4582.420257	24.482778
134.547249	4569.813385	24.487795
134.547268	4574.284252	24.492813
134.786223	4589.445572	24.497831
135.555984	4591.024285	24.502848
135.696050	4592.597382	24.507866
135.752429	4590.040377	24.512883
136.013069	4581.587023	24.517901
135.841941	4592.433863	24.522919
136.130153	4579.475954	24.527936
135.553394	4596.461305	24.532954
136.141215	4610.260515	24.537971
136.366910	4617.801509	24.542989
136.269309	4624.916621	24.548007
136.574756	4617.384307	24.553024
136.861589	4629.455294	24.558042
136.781819	4637.268355	24.563059
136.707335	4634.206227	24.568077
136.693855	4646.068031	24.573095
136.859001	4663.798823	24.578112
136.852800	4673.871727	24.583130
137.229301	4677.826438	24.588147
137.429005	4695.441268	24.593165
137.563681	4709.007151	24.598183
138.004404	4708.360624	24.603200
138.128607	4707.850174	24.608218
138.662479	4713.886991	24.613235
138.751936	4723.332898	24.618253
138.508388	4737.501122	24.623271
138.863668	4728.059348	24.628288
138.786678	4727.199585	24.633306
139.042904	4737.228133	24.638323
139.171447	4732.691045	24.643341
139.074179	4731.336137	24.648359
139.563232	4739.021649	24.653376
139.612430	4762.639012	24.658394
139.451024	4762.572155	24.663411
139.542626	4753.796342	24.668429
139.506910	4770.998328	24.673447
139.937809	4783.651902	24.678464
139.995244	4786.505122	24.683482
139.929150	4789.523778	24.688499
140.291698	4802.525008	24.693517
140.188656	4815.650870	24.698535
140.570436	4826.910810	24.703552
140.463920	4831.920021	24.708570
140.492308	4844.697235	24.713587
140.799846	4853.441503	24.718605
140.846669	4865.046949	24.723623
141.489992	4862.000167	24.728640
141.501444	4880.368669	24.733658
141.614747	4869.616374	24.738675
141.936703	4888.694061	24.743693
141.852664	4898.830445	24.748711
142.170778	4896.970195	24.753728
142.314052	4900.700679	24.758746
142.618573	4897.136853	24.763763
142.745735	4885.776618	24.768781
142.734518	4902.493484	24.773799
143.349624	4916.723159	24.778816
143.178466	4922.825236	24.783834
143.282811	4929.470623	24.788851
143.404350	4917.391477	24.793869
143.092254	4924.228134	24.798887
143.781045	4913.151789	24.803904
143.542447	4928.410120	24.808922
143.434539	4929.154213	24.813939
143.893639	4943.696506	24.818957
143.843752	4951.783551	24.823975
143.891567	4952.330082	24.828992
143.976589	4958.944828	24.834010
144.221233	4972.198120	24.839027
144.368687	4980.110627	24.844045
144.560729	4990.552443	24.849063
144.836135	5003.711656	24.854080
144.594332	5008.849724	24.859098
145.010343	5010.312430	24.864115
145.569531	5019.760003	24.869133
145.567790	5028.809356	24.874151
145.963199	5017.844695	24.879168
146.211705	5024.932401	24.884186
145.969150	5029.298007	24.889203
146.070785	5027.626501	24.894221
146.147352	5054.381318	24.899239
146.216209	5047.578016	24.904256
146.515961	5061.763358	24.909274
146.283330	5060.967242	24.914291
146.896291	5072.733934	24.919309
147.230155	5079.201060	24.924327
147.193604	5083.011085	24.929344
147.351611	5085.769678	24.934362
147.321804	5104.211453	24.939379
147.878072	5101.209808	24.944397
147.903462	5117.257693	24.949415
147.785728	5115.999872	24.954432
147.520877	5112.090365	24.959450
147.692033	5132.518872	24.964467
148.299436	5129.140934	24.969485
148.010129	5147.310068	24.974503
148.583053	5154.438431	24.979520
148.647270	5158.808226	24.984538
148.362857	5169.880628	24.989555
149.245197	5176.522851	24.994573
149.517514	5188.639210	24.999591
150.215553	5163.589762	25.004608
150.307114	5163.168991	25.009626
150.385908	5168.074272	25.014643
150.718118	5164.634160	25.019661
150.645613	5176.085612	25.024679
150.916167	5161.246308	25.029696
151.035263	5161.160402	25.034714
150.881080	5151.725852	25.039731
151.115005	5145.553481	25.044749
151.014791	5150.881497	25.049767
151.061275	5149.306561	25.054784
150.785825	5159.216600	25.059802
150.866053	5159.401774	25.064819
151.489583	5166.012180	25.069837
151.399012	5182.534613	25.074855
151.432333	5192.620182	25.079872
151.393156	5191.486337	25.084890
151.483443	5208.926973	25.089907
151.754223	5211.270704	25.094925
151.474039	5230.582751	25.099943
151.909990	5249.011093	25.104960
152.472695	5258.262910	25.109978
152.346269	5274.311768	25.114995
152.640073	5266.942533	25.120013
152.791806	5288.455015	25.125031
152.982770	5286.846607	25.130048
152.887157	5284.881009	25.135066
152.950153	5299.069679	25.140083
153.156319	5315.207437	25.145101
153.364097	5324.125273	25.150119
153.840143	5334.379938	25.155136
153.496223	5341.296881	25.160154
153.775237	5350.923524	25.165171
154.396249	5360.729615	25.170189
154.497857	5369.302836	25.175207
154.649908	5376.635913	25.180224
155.022795	5376.889020	25.185242
154.545520	5384.182549	25.190259
155.078719	5389.726721	25.195277
155.258380	5399.513242	25.200295
155.249221	5395.588741	25.205312
155.384633	5403.921666	25.210330
155.451844	5419.369865	25.215347
156.061996	5424.613797	25.220365
156.025368	5427.580423	25.225383
156.016695	5437.894437	25.230400
156.450251	5438.624187	25.235418
156.360637	5454.011845	25.240435
156.430771	5448.784102	25.245453
156.702716	5453.836157	25.250471
156.882629	5477.580149	25.255488
156.731690	5485.524381	25.260506
156.910372	5493.610739	25.265523
157.378571	5501.752953	25.270541
157.491213	5501.575971	25.275559
157.684865	5501.318584	25.280576
157.995701	5514.673171	25.285594
157.997285	5543.854428	25.290611
158.365311	5535.873386	25.295629
158.715260	5546.361791	25.300647
158.997059	5541.585571	25.305664
158.890300	5542.486230	25.310682
158.523474	5564.657830	25.315699
159.031703	5565.361789	25.320717
158.920574	5567.465816	25.325735
159.037210	5583.542330	25.330752
159.337944	5582.576436	25.335770
159.401741	5594.917567	25.340787
159.835842	5603.755425	25.345805
160.190153	5612.100917	25.350823
160.512085	5609.924130	25.355840
160.896499	5602.609779	25.360858
160.684376	5608.943388	25.365875
161.003488	5606.899385	25.370893
161.082167	5610.074497	25.375911
161.349776	5612.150250	25.380928
161.666478	5626.186008	25.385946
161.703336	5640.793599	25.390963
161.790721	5638.743993	25.395981
161.496887	5645.896109	25.400999
161.811999	5635.896558	25.406016
162.112081	5633.059463	25.411034
161.787670	5654.040397	25.416051
161.953216	5651.451692	25.421069
162.175848	5657.635107	25.426087
162.072595	5662.139194	25.431104
162.689753	5690.577338	25.436122
162.755605	5695.984267	25.441139
162.893558	5703.343467	25.446157
162.755784	5716.502627	25.451175
162.752956	5731.023173	25.456192
163.230362	5727.788791	25.461210
163.411032	5749.442011	25.466227
163.739757	5748.453342	25.471245
164.034221	5755.407728	25.476263
164.097123	5766.240900	25.481280
164.262126	5777.542272	25.486298
164.618701	5783.108060	25.491315
164.398749	5779.310638	25.496333
164.449073	5796.137939	25.501351
164.879053	5807.099955	25.506368
165.237233	5800.358516	25.511386
165.457458	5812.106755	25.516403
165.738195	5805.771981	25.521421
165.990453	5815.823932	25.526439
165.522828	5828.838733	25.531456
165.969406	5826.126118	25.536474
165.781927	5822.830502	25.541491
166.142364	5847.401960	25.546509
166.377518	5854.693885	25.551527
166.634873	5869.769113	25.556544
166.396545	5858.762685	25.561562
167.357850	5869.533280	25.566579
167.458327	5876.009590	25.571597
167.518530	5870.542352	25.576615
167.478638	5872.397514	25.581632
167.369808	5876.745857	25.586650
167.501730	5907.904269	25.591667
167.856310	5905.671611	25.596685
168.003162	5914.528235	25.601703
168.118757	5932.829465	25.606720
168.399930	5936.355346	25.611738
168.173340	5947.387178	25.616755
168.575631	5966.860805	25.621773
168.797548	5968.723669	25.626791
168.835830	5982.132607	25.631808
169.239596	5993.956810	25.636826
169.626102	6005.489326	25.641843
169.859018	5998.017243	25.646861
169.769690	6008.819170	25.651879
169.362352	6028.612492	25.656896
170.362374	6022.807100	25.661914
170.317971	6046.471869	25.666931
170.764598	6052.306328	25.671949
170.912916	6053.212675	25.676967
171.139017	6045.236058	25.681984
171.398964	6049.386127	25.687002
171.487058	6057.102687	25.692020
171.831003	6064.304173	25.697037
172.264150	6070.178684	25.702055
172.050544	6081.922814	25.707072
172.284238	6073.914992	25.712090
171.920597	6084.525481	25.717108
172.114558	6073.948779	25.722125
172.235651	6083.924245	25.727143
172.498305	6108.510783	25.732160
172.857488	6094.220596	25.737178
172.873905	6107.939654	25.742196
173.050024	6132.682379	25.747213
173.377650	6132.432651	25.752231
173.382394	6142.172301	25.757248
173.449377	6141.092420	25.762266
173.625612	6161.518268	25.767284
173.386393	6164.272172	25.772301
174.035413	6177.002473	25.777319
173.893992	6197.585115	25.782336
174.247138	6202.643611	25.787354
174.527871	6210.037607	25.792372
174.713680	6222.013190	25.797389
174.922930	6230.336646	25.802407
174.936104	6241.960512	25.807424
175.245539	6240.282705	25.812442
175.428002	6261.790621	25.817460
175.469268	6263.989135	25.822477
175.879306	6257.095541	25.827495
175.958748	6275.695382	25.832512
176.125726	6281.791414	25.837530
176.318447	6277.243222	25.842548
176.414507	6288.189386	25.847565
176.340467	6298.765286	25.852583
176.516074	6309.950285	25.857600
176.391511	6311.042974	25.862618
176.566603	6337.667029	25.867636
176.733768	6366.422966	25.872653
177.385358	6365.401880	25.877671
177.366445	6386.768575	25.882688
177.379520	6387.709229	25.887706
177.493688	6417.742929	25.892724
177.850626	6434.592424	25.897741
178.231799	6440.215006	25.902759
178.362413	6460.625979	25.907776
178.536040	6462.706437	25.912794
178.923605	6480.633093	25.917812
178.958471	6488.706841	25.922829
179.865238	6495.869352	25.927847
179.861359	6496.689172	25.932864
180.525389	6482.253467	25.937882
180.749525	6483.965588	25.942900
181.039223	6471.740745	25.947917
181.582761	6458.564023	25.952935
181.576289	6466.817120	25.957952
181.641821	6466.347082	25.962970
181.965723	6457.107193	25.967988
181.923534	6455.746133	25.973005
182.040121	6432.729655	25.978023
181.911219	6417.127755	25.983040
182.114973	6418.496700	25.988058
182.093959	6434.124378	25.993076
182.196183	6449.121183	25.998093
182.102712	6452.169908	26.003111
182.300288	6443.143986	26.008128
182.228435	6456.775623	26.013146
182.389008	6468.125484	26.018164
182.399570	6474.467330	26.023181
182.907267	6488.516230	26.028199
182.704412	6508.807034	26.033216
183.063219	6521.247944	26.038234
182.897388	6531.964485	26.043252
183.279917	6554.987254	26.048269
183.707603	6566.632272	26.053287
183.697943	6590.230646	26.058304
183.914469	6601.886360	26.063322
184.250266	6614.143709	26.068340
184.424961	6612.704065	26.073357
184.686765	6628.412539	26.078375
184.722217	6628.908412	26.083392
185.060717	6642.171934	26.088410
185.536524	6663.126779	26.093428
185.303671	6661.306683	26.098445
185.587350	6676.058526	26.103463
185.671693	6697.436838	26.108480
185.691640	6702.307480	26.113498
185.932804	6715.194992	26.118516
186.358453	6715.596890	26.123533
187.124092	6716.137630	26.128551
187.291798	6737.081544	26.133568
187.377335	6731.160844	26.138586
187.505018	6738.498606	26.143604
187.597935	6736.373113	26.148621
188.046264	6731.734274	26.153639
187.979612	6736.525586	26.158656
187.767971	6733.791443	26.163674
188.215037	6743.813981	26.168692
188.483371	6762.064800	26.173709
188.403862	6755.107410	26.178727
188.800579	6759.203436	26.183744
189.327908	6771.581098	26.188762
189.861253	6761.779299	26.193780
190.178446	6766.553312	26.198797
190.330662	6766.995919	26.203815
190.302796	6760.181173	26.208832
190.378391	6762.634762	26.213850
190.431189	6762.663048	26.218868
190.171740	6766.077311	26.223885
190.251427	6757.550474	26.228903
190.464336	6771.832129	26.233920
190.829726	6787.072230	26.238938
190.453814	6796.775501	26.243956
190.721173	6818.741081	26.248973
190.986571	6831.886948	26.253991
191.480667	6841.409455	26.259008
191.425218	6866.190230	26.264026
191.777900	6859.262588	26.269044
191.980802	6889.346239	26.274061
192.306823	6888.717911	26.279079
192.459898	6900.608869	26.284096
192.538404	6916.815950	26.289114
193.301050	6912.375306	26.294132
193.117901	6925.097198	26.299149
193.545307	6939.754518	26.304167
193.438609	6951.043591	26.309184
193.445239	6942.631976	26.314202
193.724653	6959.086122	26.319220
193.775070	6975.471214	26.324237
194.240131	6983.747051	26.329255
194.326083	7007.157661	26.334272
194.222162	7018.700733	26.339290
194.743776	7024.467174	26.344308
194.723954	7038.286791	26.349325
194.935675	7050.235068	26.354343
195.104651	7069.586567	26.359360
195.533139	7074.009002	26.364378
195.830796	7080.993377	26.369396
195.482049	7105.289225	26.374413
195.900994	7107.599963	26.379431
196.411998	7123.395910	26.384448
196.385064	7130.782387	26.389466
196.811346	7142.695082	26.394484
196.578229	7154.318794	26.399501
197.009202	7179.199608	26.404519
197.535273	7183.326240	26.409536
197.292953	7201.242589	26.414554
197.572860	7215.049577	26.419572
197.904241	7220.975301	26.424589
198.338430	7234.615680	26.429607
198.523988	7244.145588	26.434624
198.397264	7262.828891	26.439642
198.895373	7259.931828	26.444660
198.891330	7280.756128	26.449677
199.048634	7285.931797	26.454695
199.371510	7298.374565	26.459712
199.166567	7317.974386	26.464730
199.832588	7323.903622	26.469748
199.606531	7332.471702	26.474765
199.987430	7340.498628	26.479783
200.209427	7343.899182	26.484800
200.109891	7357.077765	26.489818
200.311501	7370.016492	26.494836
200.263813	7398.331096	26.499853
200.763529	7397.150874	26.504871
201.037202	7415.312551	26.509888
201.242164	7432.735010	26.514906
201.454357	7442.706437	26.519924
201.460598	7460.696778	26.524941
201.795426	7471.929398	26.529959
202.011537	7485.844107	26.534976
201.864915	7496.747148	26.539994
202.516975	7513.966229	26.545012
202.649865	7532.872947	26.550029
202.846671	7543.216417	26.555047
203.035118	7554.749894	26.560064
203.478040	7572.708764	26.565082
204.748184	7553.123127	26.570100
204.620110	7559.821631	26.575117
204.652008	7552.004923	26.580135
204.967194	7547.751883	26.585152
204.968464	7570.407041	26.590170
205.327297	7574.281149	26.595188
205.054545	7587.936108	26.600205
205.383574	7589.482052	26.605223
205.413263	7591.066705	26.610240
205.332939	7611.783597	26.615258
205.280596	7623.566658	26.620276
205.897872	7641.562802	26.625293
206.143908	7644.245782	26.630311
206.268478	7654.411494	26.635328
206.446055	7678.597920	26.640346
206.749567	7681.839281	26.645364
206.664815	7708.626965	26.650381
206.898076	7707.722576	26.655399
207.357380	7728.921034	26.660416
207.387561	7751.434587	26.665434
207.637807	7753.797872	26.670452
208.029347	7760.709447	26.675469
208.303615	7766.834701	26.680487
208.806645	7781.386502	26.685504
208.961579	7796.541238	26.690522
209.287506	7788.137565	26.695540
209.602670	7804.967105	26.700557
209.821860	7812.958913	26.705575
210.258159	7810.066511	26.710592
210.568500	7809.345446	26.715610
210.537745	7809.772012	26.720628
210.261400	7816.110076	26.725645
210.663241	7816.347399	26.730663
210.723251	7826.811457	26.735680
210.900742	7840.937695	26.740698
211.113394	7839.715343	26.745716
211.322553	7857.172229	26.750733
211.634829	7864.041882	26.755751
211.600778	7870.735134	26.760768
211.826280	7886.377632	26.765786
212.066108	7898.161975	26.770804
212.157937	7905.354996	26.775821
212.574322	7917.028098	26.780839
212.538355	7925.668887	26.785856
212.959396	7943.992581	26.790874
213.272339	7946.669223	26.795892
213.365227	7964.688273	26.800909
213.608239	7966.234369	26.805927
213.847443	7979.286290	26.810944
213.940795	7988.954060	26.815962
213.940248	7992.053018	26.820980
213.991739	8004.909291	26.825997
214.253068	8027.784983	26.831015
214.737952	8032.569329	26.836032
214.190397	8054.297072	26.841050
214.952784	8058.368919	26.846068
215.325154	8077.143545	26.851085
215.540328	8089.319679	26.856103
216.126868	8092.430603	26.861120
215.615342	8101.953178	26.866138
216.400801	8088.925549	26.871156
216.861820	8119.679157	26.876173
216.823569	8125.086095	26.881191
217.186148	8108.979445	26.886208
217.262535	8129.693816	26.891226
217.638241	8138.639696	26.896244
218.080677	8153.570556	26.901261
217.643610	8157.037466	26.906279
218.044274	8172.154096	26.911296
218.143806	8182.341635	26.916314
218.328205	8188.244883	26.921332
218.342210	8208.817693	26.926349
218.365486	8226.179047	26.931367
218.644414	8247.580678	26.936384
218.758399	8265.511489	26.941402
219.069546	8278.894360	26.946420
219.280060	8294.313674	26.951437
219.616800	8314.816455	26.956455
220.213728	8330.896304	26.961472
220.357710	8348.319659	26.966490
221.414147	8342.605700	26.971508
221.701056	8349.053621	26.976525
222.055699	8365.386446	26.981543
221.762842	8364.204721	26.986560
221.764347	8366.425100	26.991578
222.204119	8366.286691	26.996596
222.496327	8368.215363	27.001613
222.221722	8386.867048	27.006631
222.193559	8392.604820	27.011648
222.458906	8407.821354	27.016666
222.827039	8421.565895	27.021684
222.877606	8435.508154	27.026701
223.090317	8453.344000	27.031719
223.713850	8460.368582	27.036736
223.827541	8469.507850	27.041754
224.290324	8489.016283	27.046772
224.341124	8494.957598	27.051789
224.186871	8509.106464	27.056807
225.164033	8501.786051	27.061824
225.207548	8520.676496	27.066842
225.698644	8532.353393	27.071860
225.824975	8537.324293	27.076877
226.353984	8539.051370	27.081895
226.356683	8531.176015	27.086912
226.226693	8543.622533	27.091930
226.301514	8554.603723	27.096948
226.626614	8550.691437	27.101965
226.642560	8573.106898	27.106983
227.067721	8584.289064	27.112000
227.320798	8597.707848	27.117018
227.289607	8611.858415	27.122036
227.599588	8616.195422	27.127053
227.558969	8642.717388	27.132071
228.136797	8660.050882	27.137088
227.872017	8668.264537	27.142106
228.698449	8675.799043	27.147124
228.946586	8685.231981	27.152141
228.898889	8688.373568	27.157159
229.545402	8700.775482	27.162176
229.457936	8704.885509	27.167194
229.342668	8710.640231	27.172212
229.745925	8720.915505	27.177229
229.619818	8737.672831	27.182247
230.051543	8751.671773	27.187264
229.991673	8763.693248	27.192282
230.042236	8785.614855	27.197300
230.475957	8803.921680	27.202317
230.390136	8834.543806	27.207335
231.027379	8846.657483	27.212352
231.316426	8869.654243	27.217370
231.886298	8878.024734	27.222388
231.996601	8901.550670	27.227405
232.140418	8906.490421	27.232423
232.412080	8916.944449	27.237440
232.787706	8937.859079	27.242458
233.075492	8955.121347	27.247476
233.273674	8960.885524	27.252493
233.610074	8973.661366	27.257511
233.966515	8986.355114	27.262528
234.488404	8998.908734	27.267546
234.369494	8999.019909	27.272564
234.687210	9019.707943	27.277581
234.464785	9029.713976	27.282599
234.712295	9035.012299	27.287616
235.023345	9040.300066	27.292634
234.878118	9067.534128	27.297652
235.629190	9080.290789	27.302669
235.977744	9101.433855	27.307687
236.511708	9095.384208	27.312704
236.845092	9103.495551	27.317722
236.678815	9117.358632	27.322740
237.349975	9128.483767	27.327757
237.316744	9136.796259	27.332775
238.024681	9147.348898	27.337792
238.168961	9150.957332	27.342810
238.335396	9166.900009	27.347828
238.676180	9152.967008	27.352845
238.486449	9163.156755	27.357863
238.895937	9174.543608	27.362880
239.245644	9192.994821	27.367898
239.044158	9195.811504	27.372916
239.479023	9207.321782	27.377933
239.385646	9218.786701	27.382951
239.619297	9231.386032	27.387968
239.666681	9249.203758	27.392986
239.677846	9271.535125	27.398004
240.321818	9277.652320	27.403021
240.405034	9307.483130	27.408039
240.586402	9314.191613	27.413056
240.907259	9333.964931	27.418074
241.257297	9353.195378	27.423092
241.486038	9373.558335	27.428109
241.393949	9390.400496	27.433127
241.565810	9406.734822	27.438144
242.210484	9434.112414	27.443162
242.856811	9441.776473	27.448180
242.944840	9459.536475	27.453197
243.190867	9468.374668	27.458215
243.720485	9475.958086	27.463232
243.873994	9487.587000	27.468250
244.157781	9505.201876	27.473268
244.126810	9504.352322	27.478285
244.157806	9525.963869	27.483303
244.549666	9519.454767	27.488320
244.829320	9532.175888	27.493338
244.947843	9555.374490	27.498356
245.147465	9552.603824	27.503373
245.287843	9565.641166	27.508391
245.629093	9580.032429	27.513408
245.830561	9591.997711	27.518426
246.026619	9613.437001	27.523444
246.721598	9629.652342	27.528461
246.714636	9643.747013	27.533479
246.811839	9640.597880	27.538496
247.312439	9664.431138	27.543514
247.323173	9680.085869	27.548532
247.511532	9682.908767	27.553549
247.856306	9708.543652	27.558567
248.118750	9716.745873	27.563584
248.389435	9734.141022	27.568602
248.094137	9751.887043	27.573620
248.485798	9767.689699	27.578637
248.591693	9798.867928	27.583655
248.857230	9820.877343	27.588672
249.191815	9833.263430	27.593690
249.444290	9855.299483	27.598708
249.792508	9876.998238	27.603725
250.201282	9898.118960	27.608743
250.497258	9908.441187	27.613760
250.762542	9929.242309	27.618778
251.291596	9958.439343	27.623796
251.427132	9958.738287	27.628813
251.607380	9973.221253	27.633831
251.591741	9988.667171	27.638848
252.025496	10012.430909	27.643866
252.178757	10030.505280	27.648884
252.608359	10036.653660	27.653901
253.045599	10061.836517	27.658919
252.922766	10072.652271	27.663936
253.344572	10090.298431	27.668954
253.556405	10109.846600	27.673972
253.610720	10121.951747	27.678989
253.714197	10151.382127	27.684007
254.011781	10164.059017	27.689024
254.573607	10187.611086	27.694042
254.925354	10199.835467	27.699060
255.352013	10220.657425	27.704077
255.769172	10227.819500	27.709095
256.141191	10243.762969	27.714112
256.518942	10254.530342	27.719130
256.811586	10251.745679	27.724148
257.709821	10254.639027	27.729165
257.757192	10268.978895	27.734183
258.191630	10268.779918	27.739200
258.797555	10253.272767	27.744218
258.830744	10258.178533	27.749236
259.294483	10244.193438	27.754253
258.991195	10249.468654	27.759271
259.424938	10231.837031	27.764288
259.496332	10245.804978	27.769306
259.576144	10248.293858	27.774324
259.842121	10241.289364	27.779341
259.832119	10243.093585	27.784359
259.725274	10264.428081	27.789376
260.078536	10270.548270	27.794394
260.127825	10292.186958	27.799412
260.333350	10302.815173	27.804429
260.360314	10321.615951	27.809447
260.789263	10341.859428	27.814464
261.388738	10355.586111	27.819482
261.162040	10378.708539	27.824500
261.379346	10407.514642	27.829517
262.163315	10413.969058	27.834535
262.204937	10426.821036	27.839552
262.620745	10434.782283	27.844570
262.514972	10445.882221	27.849588
262.800640	10461.016188	27.854605
263.275173	10477.557363	27.859623
263.286194	10495.329728	27.864640
263.632626	10495.551102	27.869658
263.634000	10518.695715	27.874676
263.449781	10534.199314	27.879693
264.083838	10560.263348	27.884711
264.049673	10584.969137	27.889728
264.633799	10612.087791	27.894746
264.759057	10634.352461	27.899764
265.421792	10648.216210	27.904781
265.460841	10675.170271	27.909799
265.846262	10690.288669	27.914816
266.476232	10701.836942	27.919834
266.528425	10725.134913	27.924852
266.980992	10739.267646	27.929869
267.202394	10744.346342	27.934887
267.341834	10772.226142	27.939904
267.650976	10784.644767	27.944922
267.911507	10801.214738	27.949940
268.456596	10819.594397	27.954957
268.770721	10835.305417	27.959975
268.791861	10849.862877	27.964992
269.088604	10860.668540	27.970010
269.183028	10878.963994	27.975028
269.348136	10892.823179	27.980045
269.799061	10909.775250	27.985063
269.729445	10937.500196	27.990080
270.185618	10953.197186	27.995098
270.401730	10979.688234	28.000116
271.052546	10982.952150	28.005133
271.544752	11008.779700	28.010151
271.388769	11025.487644	28.015168
272.310982	11039.356683	28.020186
272.318403	11044.093642	28.025204
272.787831	11066.499482	28.030221
273.204611	11068.247072	28.035239
273.466201	11076.531282	28.040256
273.927324	11093.034351	28.045274
273.796301	11101.251441	28.050292
273.807855	11112.479673	28.055309
274.426125	11123.309306	28.060327
274.263581	11133.375236	28.065344
274.502116	11159.695828	28.070362
274.353783	11165.445099	28.075380
274.982352	11195.745824	28.080397
275.191286	11206.977571	28.085415
274.890616	11241.720307	28.090432
275.910901	11255.601604	28.095450
276.210429	11272.728905	28.100468
276.230801	11295.146637	28.105485
277.225698	11303.190956	28.110503
277.446389	11326.583922	28.115520
277.605094	11324.332657	28.120538
277.937554	11347.045274	28.125556
278.062775	11360.456100	28.130573
278.427880	11369.416589	28.135591
278.547653	11384.068446	28.140608
278.762994	11408.555983	28.145626
279.131955	11424.750101	28.150644
279.064455	11440.657476	28.155661
279.497350	11455.315680	28.160679
279.627255	11477.573651	28.165696
279.879625	11485.813907	28.170714
279.929621	11511.493549	28.175732
279.952934	11524.993927	28.180749
280.672232	11541.569594	28.185767
280.564132	11566.063832	28.190784
281.028224	11581.605696	28.195802
281.502199	11609.277726	28.200820
281.703174	11617.277618	28.205837
281.995864	11630.752240	28.210855
282.348430	11660.639569	28.215872
282.619079	11673.076305	28.220890
282.954209	11697.498682	28.225908
283.028464	11716.395652	28.230925
283.211162	11739.975166	28.235943
283.641927	11770.632867	28.240960
283.897865	11775.708516	28.245978
284.172175	11807.473264	28.250996
284.442420	11825.628699	28.256013
285.338748	11838.336654	28.261031
285.209193	11863.447885	28.266048
285.277527	11875.694627	28.271066
285.810543	11897.150312	28.276084
286.165364	11921.721032	28.281101
286.749268	11942.922500	28.286119
287.255810	11951.248407	28.291136
287.115269	11978.017803	28.296154
287.436557	11992.498062	28.301172
287.992966	12007.218191	28.306189
288.021936	12021.395637	28.311207
288.299117	12040.850199	28.316224
288.714885	12048.335575	28.321242
288.932539	12066.151765	28.326260
289.163278	12084.870315	28.331277
289.567759	12098.299966	28.336295
289.673828	12121.610696	28.341312
290.213214	12129.293036	28.346330
290.699547	12142.108741	28.351348
290.855547	12165.020437	28.356365
291.275535	12174.093594	28.361383
291.288277	12196.279044	28.366400
291.623026	12204.725021	28.371418
291.937236	12224.205169	28.376436
292.046153	12236.826791	28.381453
293.077610	12256.266611	28.386471
293.289105	12255.363235	28.391488
293.632785	12270.054336	28.396506
294.048405	12279.698729	28.401524
294.578472	12279.200993	28.406541
295.020114	12273.016603	28.411559
295.307933	12266.485875	28.416576
295.316960	12288.880078	28.421594
295.323618	12296.052186	28.426612
295.045916	12315.074510	28.431629
295.607975	12324.143060	28.436647
295.478407	12336.828017	28.441664
295.761282	12362.022782	28.446682
296.219441	12379.287215	28.451700
295.930912	12400.363178	28.456717
296.669596	12420.200096	28.461735
296.643816	12449.734140	28.466752
296.937742	12480.190573	28.471770
297.390162	12501.053749	28.476788
297.610052	12529.212379	28.481805
297.870411	12547.713803	28.486823
298.282570	12563.574110	28.491840
298.670920	12589.044814	28.496858
299.066767	12610.171242	28.501876
299.105431	12635.813575	28.506893
299.618731	12651.178102	28.511911
299.651325	12676.132854	28.516928
299.853487	12697.036282	28.521946
300.605161	12713.163385	28.526964
300.645651	12739.227910	28.531981
300.785083	12747.397748	28.536999
301.204923	12768.533004	28.542016
301.309367	12796.552113	28.547034
301.956469	12817.109151	28.552052
301.829291	12838.921601	28.557069
302.384794	12861.148588	28.562087
302.520588	12899.705335	28.567104
302.967626	12913.758951	28.572122
303.401028	12928.066986	28.577140
303.622803	12961.037246	28.582157
303.957979	12976.529380	28.587175
304.100517	13006.465114	28.592192
304.695256	13020.278386	28.597210
305.028767	13033.194255	28.602228
305.636895	13070.095462	28.607245
305.892209	13080.633712	28.612263
305.930812	13103.501622	28.617280
306.103457	13123.858934	28.622298
306.447136	13131.259085	28.627316
306.764912	13168.659461	28.632333
307.281187	13192.948412	28.637351
307.509158	13202.826248	28.642368
307.738141	13244.017445	28.647386
308.126644	13248.562514	28.652404
308.674746	13284.588512	28.657421
308.813180	13295.237722	28.662439
308.933641	13321.638173	28.667456
309.452848	13337.349075	28.672474
309.933323	13350.838060	28.677492
309.898399	13377.642639	28.682509
310.298783	13394.809013	28.687527
310.577446	13424.514878	28.692544
310.918358	13440.906363	28.697562
311.260143	13443.538177	28.702580
311.768924	13478.565686	28.707597
312.225319	13497.295656	28.712615
312.740592	13504.314460	28.717632
313.286377	13521.869711	28.722650
313.958903	13516.737058	28.727668
313.966360	13536.729917	28.732685
314.132739	13551.925996	28.737703
314.321353	13553.522659	28.742720
314.388900	13575.592143	28.747738
314.692504	13588.248663	28.752756
314.743902	13616.928864	28.757773
314.743061	13629.084405	28.762791
315.326770	13657.436702	28.767808
315.293533	13679.133806	28.772826
315.568949	13701.335979	28.777844
315.734137	13741.298746	28.782861
316.234168	13764.092503	28.787879
316.731985	13801.087764	28.792896
316.805570	13817.837658	28.797914
317.610565	13851.201384	28.802932
317.851516	13867.267917	28.807949
318.170442	13895.308443	28.812967
318.519884	13916.976962	28.817984
318.485165	13947.935165	28.823002
319.358627	13961.130855	28.828020
319.263457	13987.686404	28.833037
319.577484	14003.061678	28.838055
320.138808	14034.742123	28.843072
319.881867	14060.836105	28.848090
320.432513	14082.545491	28.853108
320.519083	14112.791992	28.858125
320.912137	14121.013373	28.863143
321.197235	14145.781856	28.868160
321.602141	14180.377391	28.873178
322.483434	14204.697048	28.878196
323.076255	14204.615942	28.883213
323.176685	14214.821327	28.888231
323.902977	14237.040738	28.893248
323.794371	14253.971065	28.898266
324.363196	14262.826822	28.903284
324.329646	14285.634300	28.908301
324.476870	14294.468702	28.913319
325.020724	14324.259808	28.918336
324.959334	14352.570757	28.923354
325.500814	14362.360967	28.928372
325.619064	14397.554616	28.933389
326.322148	14432.310763	28.938407
326.390980	14445.106239	28.943424
326.170115	14472.020724	28.948442
326.491912	14497.491286	28.953460
326.798530	14533.363153	28.958477
327.691561	14547.914623	28.963495
328.206894	14574.371280	28.968512
328.255090	14598.662860	28.973530
329.259998	14616.100470	28.978548
329.613619	14633.230213	28.983565
329.895938	14653.144102	28.988583
330.248511	14665.005294	28.993600
330.236516	14685.931086	28.998618
330.734848	14702.917082	29.003636
330.610709	14724.717354	29.008653
331.190850	14747.721404	29.013671
331.406899	14771.249332	29.018688
331.318565	14800.675082	29.023706
331.946734	14819.485209	29.028724
332.139718	14849.895066	29.033741
332.731749	14887.742402	29.038759
333.297047	14911.080124	29.043776
333.152396	14932.062939	29.048794
333.787702	14958.410452	29.053812
333.652144	14983.954593	29.058829
334.225635	15021.515318	29.063847
334.910732	15038.131777	29.068864
335.064277	15070.893822	29.073882
335.358497	15089.375169	29.078900
335.844291	15129.529207	29.083917
336.223674	15151.662491	29.088935
336.533886	15172.869512	29.093952
336.737110	15201.489438	29.098970
337.305913	15219.219221	29.103988
337.612558	15240.731112	29.109005
338.048296	15266.633134	29.114023
338.242062	15275.296418	29.119040
338.682552	15308.832428	29.124058
339.022679	15332.884312	29.129076
338.925534	15355.081269	29.134093
339.436316	15379.081230	29.139111
340.140867	15403.733077	29.144128
340.348192	15424.391685	29.149146
340.619171	15449.396176	29.154164
340.974377	15475.964426	29.159181
341.567948	15500.365335	29.164199
342.074584	15514.392384	29.169216
342.161864	15541.829568	29.174234
342.446189	15545.981220	29.179252
342.888972	15580.685325	29.184269
343.056474	15602.041124	29.189287
343.534340	15616.605778	29.194304
343.505213	15651.845509	29.199322
344.153361	15656.565636	29.204340
344.339724	15686.664487	29.209357
344.450927	15703.693764	29.214375
344.834298	15720.614802	29.219392
344.866505	15745.058890	29.224410
345.094544	15777.244126	29.229428
345.499358	15800.590860	29.234445
346.111829	15825.089988	29.239463
346.374149	15847.440678	29.244480
346.948882	15884.465697	29.249498
347.399174	15892.183546	29.254516
348.184235	15913.084098	29.259533
348.461644	15934.108411	29.264551
349.121418	15951.544892	29.269568
349.057062	15975.729531	29.274586
349.459314	15978.572385	29.279604
349.633161	16002.446391	29.284621
349.999838	16025.541286	29.289639
350.402712	16044.510039	29.294656
350.464801	16075.834453	29.299674
350.871620	16092.815027	29.304692
351.376676	16125.708349	29.309709
351.668050	16154.928430	29.314727
352.041547	16173.118840	29.319744
351.811719	16203.677092	29.324762
352.127182	16230.371377	29.329780
353.126782	16259.746683	29.334797
353.089816	16280.547823	29.339815
353.465694	16303.269592	29.344832
354.224845	16329.660209	29.349850
354.670086	16354.151653	29.354868
355.367031	16364.591866	29.359885
355.862521	16390.786793	29.364903
356.220449	16399.566838	29.369920
356.308530	16420.382059	29.374938
356.866066	16446.197931	29.379956
356.965237	16465.362632	29.384973
357.072287	16480.883374	29.389991
357.728637	16510.579377	29.395008
357.421000	16525.678837	29.400026
357.955431	16545.516888	29.405044
358.251418	16579.092101	29.410061
358.678003	16618.788313	29.415079
358.996796	16643.808743	29.420096
358.996313	16671.855054	29.425114
359.090548	16714.131854	29.430132
359.750556	16745.474859	29.435149
360.050020	16776.817916	29.440167
360.833878	16798.198980	29.445184
360.820908	16838.785239	29.450202
361.587009	16858.686065	29.455220
362.639721	16871.955229	29.460237
363.104371	16892.117391	29.465255
363.762761	16914.454177	29.470272
363.805356	16921.732676	29.475290
363.995386	16938.497930	29.480308
364.465056	16957.600081	29.485325
364.673248	16975.558751	29.490343
365.115852	16986.066832	29.495360
365.528650	17018.769191	29.500378
365.406051	17035.329540	29.505396
365.809320	17058.864317	29.510413
365.626871	17090.023202	29.515431
366.187580	17115.546405	29.520448
365.975201	17160.632213	29.525466
366.655670	17190.207212	29.530484
366.555468	17219.886720	29.535501
367.187908	17252.054943	29.540519
367.840148	17281.980007	29.545536
368.292030	17314.971228	29.550554
368.797539	17333.864517	29.555572
369.409513	17353.031761	29.560589
369.540937	17376.935291	29.565607
370.179430	17401.225945	29.570624
370.143442	17422.775532	29.575642
370.504175	17437.561450	29.580660
370.991978	17461.598216	29.585677
371.160120	17491.443286	29.590695
371.881393	17524.148998	29.595712
372.081786	17556.012837	29.600730
372.318731	17574.766581	29.605748
372.709828	17605.285749	29.610765
372.904279	17638.180081	29.615783
373.587661	17661.472143	29.620800
373.738875	17692.564123	29.625818
374.270788	17723.957060	29.630836
375.204946	17746.299608	29.635853
375.222666	17782.020031	29.640871
375.689277	17789.696656	29.645888
375.757405	17839.644907	29.650906
376.133203	17860.656904	29.655924
376.412550	17884.404178	29.660941
376.789948	17921.498071	29.665959
377.268057	17948.448706	29.670976
377.501226	17976.125794	29.675994
377.774486	18011.014497	29.681012
378.102548	18034.014573	29.686029
378.284240	18076.838355	29.691047
378.907842	18112.419435	29.696064
378.952994	18151.082359	29.701082
379.847228	18189.293785	29.706100
379.930570	18232.306131	29.711117
380.273777	18257.569284	29.716135
381.117020	18295.683806	29.721152
381.634736	18330.280348	29.726170
381.726979	18357.894777	29.731188
382.258746	18397.684973	29.736205
382.906455	18430.103597	29.741223
383.262949	18455.025914	29.746240
383.520647	18474.265917	29.751258
384.086982	18511.302942	29.756276
384.654228	18529.094878	29.761293
384.835804	18556.953332	29.766311
385.289141	18582.870245	29.771328
385.455680	18616.603503	29.776346
385.851259	18640.062980	29.781364
386.002820	18677.189764	29.786381
386.379822	18707.740097	29.791399
387.024237	18745.016903	29.796416
387.095777	18778.480931	29.801434
387.525103	18815.582378	29.806452
387.791923	18842.706711	29.811469
387.889051	18884.302790	29.816487
388.551095	18915.137213	29.821504
389.048739	18951.787782	29.826522
389.349829	18995.908864	29.831540
390.196175	19020.780614	29.836557
390.547794	19060.613352	29.841575
391.071109	19085.018617	29.846592
391.448527	19117.989528	29.851610
391.854047	19135.343915	29.856628
392.300567	19175.927336	29.861645
392.783439	19202.114615	29.866663
393.226619	19225.109827	29.871680
393.940002	19239.291733	29.876698
394.104847	19260.611696	29.881716
394.448859	19281.194078	29.886733
394.668212	19303.362656	29.891751
394.914820	19320.768857	29.896768
395.392039	19345.960953	29.901786
395.408276	19369.259025	29.906804
396.108283	19400.691843	29.911821
396.132971	19426.979229	29.916839
396.561316	19452.364055	29.921856
397.104914	19485.632850	29.926874
397.219871	19523.997277	29.931892
397.850758	19554.396633	29.936909
397.857816	19576.127878	29.941927
398.463592	19615.862969	29.946944
398.714532	19635.170070	29.951962
399.448854	19666.643409	29.956980
400.149241	19688.273826	29.961997
400.209096	19734.986185	29.967015
400.571944	19764.541277	29.972032
401.107899	19780.693840	29.977050
401.968047	19806.764224	29.982068
402.631581	19828.251172	29.987085
403.321472	19862.615768	29.992103
403.570791	19866.681313	29.997120
404.014523	19883.940270	30.002138
404.271272	19902.436367	30.007156
404.892797	19920.739465	30.012173
405.095379	19954.300743	30.017191
405.129306	19971.219529	30.022208
405.599201	19991.920616	30.027226
405.798044	20016.950280	30.032244
406.266945	20045.222270	30.037261
406.124320	20089.371062	30.042279
406.751051	20111.443090	30.047296
407.036052	20147.767414	30.052314
407.392867	20188.242065	30.057332
407.392048	20217.123673	30.062349
407.942466	20255.912492	30.067367
408.375253	20295.197069	30.072384
408.764195	20330.714652	30.077402
408.892341	20377.827370	30.082420
409.454335	20416.155846	30.087437
410.270057	20446.105169	30.092455
410.705131	20492.784115	30.097472
411.327292	20519.574660	30.102490
411.522346	20560.408164	30.107508
412.613987	20590.018666	30.112525
412.926422	20614.309837	30.117543
413.308398	20643.168011	30.122560
413.947943	20673.470212	30.127578
414.253921	20708.507312	30.132596
414.420083	20725.631929	30.137613
414.772669	20762.168660	30.142631
414.857402	20795.292390	30.147648
415.770541	20825.109540	30.152666
415.620469	20864.895881	30.157684
415.920996	20889.846890	30.162701
416.740902	20927.548759	30.167719
417.339338	20968.144397	30.172736
417.867392	20997.152347	30.177754
418.153841	21031.154345	30.182772
418.704386	21065.978135	30.187789
418.505854	21092.546430	30.192807
419.050975	21128.889582	30.197824
419.620720	21162.389133	30.202842
419.869327	21201.558212	30.207860
420.329623	21228.413039	30.212877
420.677313	21273.984492	30.217895
420.762079	21313.127437	30.222912
421.418842	21346.109937	30.227930
421.493972	21380.865133	30.232948
422.381750	21415.658861	30.237965
422.202954	21455.238508	30.242983
422.371017	21484.335471	30.248000
423.256167	21521.364043	30.253018
423.192610	21574.140788	30.258036
423.885179	21610.648117	30.263053
425.150995	21641.997470	30.268071
425.179185	21682.935512	30.273088
425.588638	21719.513751	30.278106
425.809954	21753.773993	30.283124
426.112742	21788.894281	30.288141
426.486692	21836.823258	30.293159
426.942914	21886.954028	30.298176
427.526074	21925.224085	30.303194
427.976524	21956.499744	30.308212
428.700968	21994.688153	30.313229
429.113352	22025.881966	30.318247
429.756008	22062.898394	30.323264
430.168130	22091.460764	30.328282
430.806262	22127.200910	30.333300
431.254672	22158.709067	30.338317
431.996848	22188.722593	30.343335
432.285497	22213.847824	30.348352
432.562662	22245.364087	30.353370
433.095840	22280.409287	30.358388
433.468541	22314.300205	30.363405
434.168976	22339.276812	30.368423
434.240583	22382.254420	30.373440
434.896875	22402.951171	30.378458
434.987691	22434.695835	30.383476
435.732173	22463.317160	30.388493
436.179061	22482.471994	30.393511
436.711816	22514.985416	30.398528
436.991030	22535.590432	30.403546
437.450274	22579.752984	30.408564
437.958571	22609.435555	30.413581
438.397210	22647.322857	30.418599
439.219690	22671.885483	30.423616
439.621601	22683.882976	30.428634
440.062036	22728.790144	30.433652
440.244644	22756.943940	30.438669
440.709172	22785.295367	30.443687
440.690750	22824.097848	30.448704
441.323030	22848.183006	30.453722
441.670041	22891.507215	30.458740
441.870085	22933.458866	30.463757
442.584690	22969.735253	30.468775
442.767906	23005.909178	30.473792
443.225332	23040.405599	30.478810
443.551814	23075.105177	30.483828
444.136272	23111.184301	30.488845
444.931217	23148.467952	30.493863
444.952716	23189.339780	30.498880
445.784804	23227.643974	30.503898
446.130704	23256.228767	30.508916
446.410503	23302.463470	30.513933
447.014100	23329.029765	30.518951
447.465606	23379.217767	30.523968
447.708125	23405.021021	30.528986
448.267262	23449.645462	30.534004
448.733862	23476.330931	30.539021
448.955080	23521.005376	30.544039
449.288724	23568.969595	30.549056
449.878040	23604.263665	30.554074
450.330337	23638.104583	30.559092
450.367669	23680.525054	30.564109
451.001745	23719.183356	30.569127
451.249305	23772.306327	30.574144
451.546143	23799.283843	30.579162
451.741822	23845.955027	30.584180
451.947224	23906.302992	30.589197
452.709706	23944.158321	30.594215
452.791330	24001.021660	30.599232
453.447002	24049.744291	30.604250
454.163898	24099.387290	30.609268
454.509268	24146.200013	30.614285
455.171909	24194.269042	30.619303
455.387260	24241.305469	30.624320
456.354212	24279.793062	30.629338
456.375311	24322.235167	30.634356
457.168661	24361.392025	30.639373
458.034866	24407.630100	30.644391
458.199018	24461.068690	30.649408
458.914549	24495.895781	30.654426
459.282517	24530.190876	30.659444
459.431158	24577.608322	30.664461
461.257281	24587.631203	30.669479
461.914005	24624.121010	30.674496
462.428897	24644.091757	30.679514
462.908217	24674.391464	30.684532
463.253600	24694.242184	30.689549
463.574710	24723.101644	30.694567
463.951770	24754.329985	30.699584
464.150421	24787.587661	30.704602
464.426567	24812.915932	30.709620
465.099702	24853.926374	30.714637
465.411788	24878.428725	30.719655
465.619670	24918.131970	30.724672
465.968196	24948.233102	30.729690
466.238038	24997.322150	30.734708
466.574215	25041.347509	30.739725
467.558103	25068.003175	30.744743
468.079193	25125.535312	30.749760
469.076773	25140.556575	30.754778
469.504337	25171.099161	30.759796
469.990377	25202.102049	30.764813
470.339929	25229.226040	30.769831
470.415465	25264.848585	30.774848
471.223883	25293.889865	30.779866
471.810255	25341.110559	30.784884
471.575575	25378.466006	30.789901
472.264644	25411.662368	30.794919
472.520381	25459.635363	30.799936
472.978220	25497.150464	30.804954
473.555357	25538.582220	30.809972
473.837120	25587.986392	30.814989
474.258720	25635.724157	30.820007
474.378296	25679.638879	30.825024
474.774521	25731.509949	30.830042
475.223253	25787.144879	30.835060
475.796577	25852.083149	30.840077
476.268509	25884.382840	30.845095
476.835164	25953.366309	30.850112
477.481962	25995.737021	30.855130
478.127736	26042.536571	30.860148
478.164024	26093.099564	30.865165
478.554083	26137.408973	30.870183
479.071411	26192.078076	30.875200
479.337272	26241.650786	30.880218
479.988751	26295.140313	30.885236
480.587397	26355.420537	30.890253
481.477589	26394.083350	30.895271
481.705513	26445.593385	30.900288
482.221347	26486.103924	30.905306
483.194453	26533.711578	30.910324
483.454691	26565.158181	30.915341
484.424905	26587.790392	30.920359
484.706973	26628.781698	30.925376
485.357139	26662.267675	30.930394
485.408788	26687.326863	30.935412
485.755959	26734.073789	30.940429
486.509974	26772.715908	30.945447
486.337837	26822.227387	30.950464
487.017876	26863.616852	30.955482
487.593022	26899.525709	30.960500
487.974007	26962.569607	30.965517
488.771720	26992.643879	30.970535
489.300199	27043.878663	30.975552
489.620195	27081.054191	30.980570
490.153048	27128.380151	30.985588
490.641737	27173.666335	30.990605
491.566124	27202.745210	30.995623
491.714054	27258.955326	31.000640
492.452648	27294.348916	31.005658
492.990229	27333.728529	31.010676
493.328475	27375.188601	31.015693
493.761010	27413.784601	31.020711
494.083953	27471.729706	31.025728
494.343761	27519.180943	31.030746
494.822288	27567.911424	31.035764
495.306935	27621.420147	31.040781
495.651003	27661.409922	31.045799
496.476439	27717.701434	31.050816
497.016537	27764.144654	31.055834
497.607517	27809.961252	31.060852
497.781711	27865.657929	31.065869
498.509160	27910.158751	31.070887
498.718458	27971.414631	31.075904
499.714468	28021.032061	31.080922
500.067923	28065.333558	31.085940
500.295431	28124.385031	31.090957
501.293216	28165.421996	31.095975
501.640477	28205.702720	31.100992
502.116244	28263.281229	31.106010
503.295444	28301.808833	31.111028
503.503946	28343.049853	31.116045
503.973818	28384.184472	31.121063
504.694246	28424.839077	31.126080
504.900560	28464.131155	31.131098
505.715276	28502.735510	31.136116
506.129896	28547.614851	31.141133
506.357152	28586.310642	31.146151
506.978405	28646.658177	31.151168
507.329496	28690.415890	31.156186
508.066056	28734.589219	31.161204
508.305127	28780.930565	31.166221
508.729103	28830.642151	31.171239
509.262260	28876.811877	31.176256
510.174163	28927.524794	31.181274
510.454367	28968.383123	31.186292
510.808114	29023.933802	31.191309
511.556640	29063.093017	31.196327
511.645745	29111.081709	31.201344
512.177430	29167.638071	31.206362
512.787972	29215.035684	31.211380
512.781630	29273.057239	31.216397
513.545334	29321.164781	31.221415
514.339381	29381.574496	31.226432
514.657287	29422.474949	31.231450
515.435021	29477.278362	31.236468
515.545203	29533.407436	31.241485
516.200362	29584.748553	31.246503
516.538510	29636.334916	31.251520
517.225356	29683.736902	31.256538
518.229265	29716.135218	31.261556
518.579318	29765.656671	31.266573
518.888197	29805.401661	31.271591
519.187651	29852.082859	31.276608
519.725438	29902.147720	31.281626
520.422789	29947.223479	31.286644
520.467850	30009.428717	31.291661
520.985248	30055.269746	31.296679
521.552039	30111.372166	31.301696
521.878407	30171.247052	31.306714
522.894176	30216.216990	31.311732
523.365702	30273.616681	31.316749
523.893252	30323.249052	31.321767
523.964678	30373.929061	31.326784
524.887819	30431.695975	31.331802
525.561226	30479.875333	31.336820
526.605713	30510.586743	31.341837
527.492757	30552.177770	31.346855
528.145651	30590.741052	31.351872
528.320389	30635.615103	31.356890
529.042235	30680.199643	31.361908
529.416196	30724.990357	31.366925
530.057647	30766.692090	31.371943
530.624456	30803.500122	31.376960
531.063648	30858.991944	31.381978
531.605430	30886.622912	31.386996
531.964194	30932.893277	31.392013
532.344260	30978.822626	31.397031
532.811059	31023.311564	31.402048
532.988292	31080.380988	31.407066
534.086500	31121.900437	31.412084
534.245728	31177.830996	31.417101
534.775170	31224.174748	31.422119
535.544934	31278.751631	31.427136
535.704107	31317.045113	31.432154
536.978524	31366.565868	31.437172
537.311643	31421.054786	31.442189
538.152941	31454.767501	31.447207
539.211293	31481.042065	31.452224
539.709732	31523.129037	31.457242
540.337056	31553.088034	31.462260
540.608133	31589.817456	31.467277
541.004425	31632.432801	31.472295
541.673209	31678.461170	31.477312
542.146456	31715.617950	31.482330
542.924153	31756.791405	31.487348
543.909652	31780.125174	31.492365
543.993424	31822.975884	31.497383
545.039973	31846.911731	31.502400
545.481415	31886.923385	31.507418
546.018958	31917.219752	31.512436
546.269540	31956.913020	31.517453
546.762188	31999.825628	31.522471
547.203213	32033.769999	31.527488
547.056426	32075.132426	31.532506
547.519717	32115.901406	31.537524
547.978976	32167.093277	31.542541
548.233307	32215.962271	31.547559
548.937976	32266.271194	31.552576
548.883861	32339.200976	31.557594
549.337881	32393.865293	31.562612
549.918292	32450.730194	31.567629
550.109195	32518.738617	31.572647
551.090813	32585.546306	31.577664
551.352421	32656.613746	31.582682
551.932258	32720.427886	31.587700
552.372357	32774.480374	31.592717
552.997699	32833.708792	31.597735
553.700848	32895.934817	31.602752
553.580172	32970.067855	31.607770
554.177337	33022.173318	31.612788
554.853785	33088.613894	31.617805
555.276321	33159.391556	31.622823
556.490485	33228.422407	31.627840
556.531788	33292.997004	31.632858
557.307231	33357.658192	31.637876
557.940414	33410.784371	31.642893
558.576316	33481.035612	31.647911
559.442590	33538.560220	31.652928
559.624623	33602.623451	31.657946
560.394189	33669.505140	31.662964
562.039708	33707.209844	31.667981
563.161020	33748.684301	31.672999
563.845587	33785.157109	31.678016
564.113326	33840.743542	31.683034
564.599693	33880.802719	31.688052
565.300222	33920.570816	31.693069
565.737402	33968.246664	31.698087
567.255163	33988.159426	31.703104
568.277970	34016.838830	31.708122
569.312586	34023.641122	31.713140
569.922822	34039.583322	31.718157
570.183374	34059.282068	31.723175
571.054614	34082.227617	31.728192
570.768569	34105.062421	31.733210
571.733801	34125.824456	31.738228
571.802529	34161.153798	31.743245
572.026544	34201.878937	31.748263
572.389514	34240.485696	31.753280
572.668668	34288.542082	31.758298
573.245240	34332.670810	31.763316
573.482665	34378.635803	31.768333
573.946449	34433.311073	31.773351
574.493624	34477.429261	31.778368
575.041225	34533.681424	31.783386
575.524884	34583.964177	31.788404
575.946025	34636.021539	31.793421
575.896594	34700.256526	31.798439
576.651483	34755.158995	31.803456
577.380692	34825.179125	31.808474
577.850662	34877.847622	31.813492
578.444928	34950.298548	31.818509
578.674747	35022.813439	31.823527
579.219247	35080.753062	31.828544
579.875038	35158.376546	31.833562
580.590034	35222.325517	31.838580
581.482557	35282.906291	31.843597
581.398469	35357.964665	31.848615
582.529211	35415.703878	31.853632
583.294532	35480.245036	31.858650
584.066160	35536.674593	31.863668
584.479946	35602.467510	31.868685
585.103344	35668.194302	31.873703
585.707073	35723.156394	31.878720
586.003651	35800.435176	31.883738
586.570673	35848.088152	31.888756
587.089007	35916.487494	31.893773
587.706085	35985.416692	31.898791
588.528305	36038.856979	31.903808
589.277538	36111.687668	31.908826
589.985967	36170.638765	31.913844
590.690604	36224.638814	31.918861
590.895354	36287.890436	31.923879
591.675144	36339.517603	31.928896
592.067402	36391.960417	31.933914
593.134411	36431.376562	31.938932
594.230628	36476.383729	31.943949
594.503878	36532.810791	31.948967
595.230810	36577.339832	31.953984
595.668273	36630.627989	31.959002
595.908126	36680.957087	31.964020
596.347650	36729.207982	31.969037
596.954690	36784.971268	31.974055
597.192032	36839.426332	31.979072
597.427627	36908.510771	31.984090
598.483696	36964.875476	31.989108
599.143257	37025.254610	31.994125
599.758439	37092.818556	31.999143
600.434863	37134.523073	32.004160
601.239785	37201.816046	32.009178
602.013406	37258.395847	32.014196
602.653797	37306.949491	32.019213
603.001606	37378.223310	32.024231
603.843653	37418.837319	32.029248
604.727289	37479.669986	32.034266
605.316726	37530.685125	32.039284
605.818457	37578.173598	32.044301
606.615954	37632.317092	32.049319
607.393707	37686.350399	32.054336
608.132153	37731.416945	32.059354
608.701917	37783.824848	32.064372
609.281793	37830.660270	32.069389
609.665710	37879.198062	32.074407
610.299606	37929.013836	32.079424
610.737073	37987.633925	32.084442
611.341166	38039.481344	32.089460
611.941968	38086.096159	32.094477
612.574981	38148.446716	32.099495
613.143071	38203.895724	32.104512
613.989681	38257.325892	32.109530
614.665021	38323.451414	32.114548
615.274554	38375.867046	32.119565
615.544696	38423.803362	32.124583
616.389308	38478.844302	32.129600
616.565906	38541.196232	32.134618
616.730519	38600.621151	32.139636
617.749593	38659.399350	32.144653
618.009037	38737.612193	32.149671
618.939233	38806.140284	32.154688
619.431962	38871.647872	32.159706
619.656704	38942.376915	32.164724
620.391112	39010.423765	32.169741
620.740399	39090.545539	32.174759
621.004540	39154.141336	32.179776
621.900741	39230.271385	32.184794
622.677124	39310.462097	32.189812
623.322073	39382.912865	32.194829
624.032913	39466.407493	32.199847
624.564402	39543.028701	32.204864
625.111733	39618.817399	32.209882
625.667995	39682.672722	32.214900
626.568505	39750.079192	32.219917
626.913514	39833.033306	32.224935
627.685912	39913.069481	32.229952
628.127412	39990.420915	32.234970
628.823066	40067.402174	32.239988
629.688778	40141.868005	32.245005
630.657974	40213.081278	32.250023
631.306693	40277.636747	32.255040
631.759726	40355.903266	32.260058
632.226298	40421.805862	32.265076
633.346125	40473.792371	32.270093
633.878065	40545.467819	32.275111
634.844648	40606.941126	32.280128
635.241580	40660.623445	32.285146
636.098832	40714.251591	32.290164
636.927970	40772.616683	32.295181
637.348299	40827.924542	32.300199
638.078546	40889.144444	32.305216
638.508860	40952.494734	32.310234
638.984247	41007.790835	32.315252
639.682913	41063.027931	32.320269
640.034193	41133.333996	32.325287
640.368669	41194.270203	32.330304
641.006753	41265.574095	32.335322
641.522760	41340.822619	32.340340
642.329220	41415.218199	32.345357
642.954335	41485.893701	32.350375
643.773103	41558.270507	32.355392
644.538887	41628.806391	32.360410
644.921149	41702.358027	32.365428
645.673363	41774.768829	32.370445
645.949205	41863.688234	32.375463
646.297168	41936.166785	32.380480
647.399663	42017.442208	32.385498
647.450935	42095.583906	32.390516
648.116706	42174.997240	32.395533
648.816670	42263.324064	32.400551
649.465893	42355.195710	32.405568
650.050798	42444.499107	32.410586
650.519424	42531.823761	32.415604
651.591867	42616.816455	32.420621
652.006040	42712.833212	32.425639
652.823909	42796.233572	32.430656
653.735720	42888.623079	32.435674
654.364675	42967.935411	32.440692
655.166362	43051.424846	32.445709
655.693526	43131.575657	32.450727
656.319395	43212.379766	32.455744
657.337356	43294.972450	32.460762
657.693881	43386.319997	32.465780
658.793373	43453.255443	32.470797
659.503675	43551.083847	32.475815
660.492186	43616.967974	32.480832
660.972420	43693.308611	32.485850
661.322264	43773.861029	32.490868
662.505733	43848.784712	32.495885
663.250986	43936.189992	32.500903
663.899431	44000.894236	32.505920
664.698549	44064.383344	32.510938
665.280952	44138.552324	32.515956
666.645563	44203.855103	32.520973
667.303010	44267.725213	32.525991
668.150638	44326.935135	32.531008
668.729797	44379.991712	32.536026
669.269914	44441.709559	32.541044
670.019624	44492.209000	32.546061
670.676424	44566.828316	32.551079
671.293851	44632.073508	32.556096
672.178481	44689.747042	32.561114
672.284279	44756.571116	32.566132
672.837048	44829.020578	32.571149
673.417836	44910.000534	32.576167
673.662078	44967.781242	32.581184
674.680339	45036.829308	32.586202
675.057759	45108.731124	32.591220
675.844627	45183.836509	32.596237
676.290258	45269.693684	32.601255
677.009297	45355.370079	32.606272
677.782461	45422.328853	32.611290
677.930509	45500.737093	32.616308
678.333902	45577.726522	32.621325
679.147469	45652.838817	32.626343
679.332777	45724.178072	32.631360
680.232082	45817.060906	32.636378
680.588492	45903.557845	32.641396
681.206139	45993.463212	32.646413
682.180538	46077.903710	32.651431
682.634819	46175.456715	32.656448
683.305381	46260.314773	32.661466
683.918841	46346.193184	32.666484
685.013027	46430.719578	32.671501
685.540728	46511.658378	32.676519
686.069544	46606.731813	32.681536
686.762570	46697.692201	32.686554
687.581573	46798.200451	32.691572
688.478161	46891.758478	32.696589
689.871744	46965.096537	32.701607
690.203153	47043.641772	32.706624
691.123017	47127.369684	32.711642
691.797088	47216.238842	32.716660
692.561923	47307.439706	32.721677
693.363547	47387.657804	32.726695
694.572759	47447.603825	32.731712
695.652675	47529.093195	32.736730
696.172309	47608.566384	32.741748
696.506042	47676.101888	32.746765
697.039731	47753.943814	32.751783
697.476894	47841.064618	32.756800
698.323428	47917.847860	32.761818
699.063460	47998.890378	32.766836
699.599821	48079.730197	32.771853
700.670223	48152.671731	32.776871
701.215409	48244.924137	32.781888
702.180826	48309.123107	32.786906
702.916637	48406.498698	32.791924
704.099272	48467.185032	32.796941
705.342164	48527.375199	32.801959
706.015097	48588.973976	32.806976
706.521686	48657.419069	32.811994
707.176423	48722.141575	32.817012
707.748866	48798.705416	32.822029
708.506236	48871.610077	32.827047
708.738370	48942.713595	32.832064
709.397285	49012.148456	32.837082
710.124344	49089.591046	32.842100
710.559680	49161.798610	32.847117
711.434075	49230.364709	32.852135
712.100904	49320.435526	32.857152
712.968334	49396.532730	32.862170
713.476697	49482.306903	32.867188
714.140450	49557.071007	32.872205
714.756143	49644.233539	32.877223
715.452580	49736.941763	32.882240
715.889757	49809.899985	32.887258
716.575850	49899.427076	32.892276
717.044226	49990.977357	32.897293
718.213038	50083.959414	32.902311
719.334442	50153.833284	32.907328
720.324090	50224.329383	32.912346
720.906250	50309.267477	32.917364
722.039184	50371.771567	32.922381
723.119539	50442.016520	32.927399
724.115304	50490.971831	32.932416
725.489666	50538.758945	32.937434
726.324341	50601.613352	32.942452
727.257696	50643.327507	32.947469
728.067383	50685.706619	32.952487
728.413243	50733.860787	32.957504
729.102623	50768.136348	32.962522
729.451405	50820.819570	32.967540
729.846520	50868.365775	32.972557
730.358264	50928.482707	32.977575
730.386531	50986.247998	32.982592
731.282181	51051.235248	32.987610
731.609404	51120.764361	32.992628
731.979232	51195.763648	32.997645
732.163980	51263.428085	33.002663
732.745935	51357.540245	33.007680
733.137507	51461.147735	33.012698
733.707449	51549.166652	33.017716
734.631859	51642.869575	33.022733
735.507228	51739.423904	33.027751
735.793808	51838.894012	33.032768
736.786288	51931.317230	33.037786
738.079417	52028.492243	33.042804
739.158523	52113.428398	33.047821
740.247858	52189.752463	33.052839
740.665299	52285.690596	33.057856
741.611787	52364.231244	33.062874
742.350632	52446.432976	33.067892
742.859061	52540.095558	33.072909
743.824168	52624.181034	33.077927
743.905382	52726.595880	33.082944
745.063491	52818.995814	33.087962
745.717023	52902.742514	33.092980
746.298034	52998.846528	33.097997
747.140623	53080.578826	33.103015
747.751547	53189.725062	33.108032
748.505167	53277.405395	33.113050
749.445885	53377.393897	33.118068
750.300664	53467.383272	33.123085
751.020735	53560.668119	33.128103
751.118072	53660.248405	33.133120
752.133402	53767.447965	33.138138
753.212916	53864.547531	33.143156
753.828896	53963.354590	33.148173
754.515072	54054.619307	33.153191
755.145592	54163.862476	33.158208
756.018833	54261.263606	33.163226
756.591944	54366.682299	33.168244
757.657132	54468.108879	33.173261
758.521770	54553.944190	33.178279
759.277068	54670.504965	33.183296
759.975838	54764.310838	33.188314
760.554626	54860.512778	33.193332
761.259066	54971.321422	33.198349
762.578794	55064.804499	33.203367
762.956216	55166.475207	33.208384
763.704725	55264.736034	33.213402
764.547286	55372.402661	33.218420
764.690170	55480.223931	33.223437
765.637869	55580.342509	33.228455
766.152710	55703.432165	33.233472
767.256958	55808.940981	33.238490
768.201437	55908.846918	33.243508
768.946849	56013.279022	33.248525
770.215196	56117.713331	33.253543
770.968010	56214.783904	33.258560
771.916536	56294.521520	33.263578
772.917619	56398.894253	33.268596
773.840618	56498.459184	33.273613
774.816338	56577.637360	33.278631
775.634933	56664.462574	33.283648
776.539649	56744.740059	33.288666
777.865260	56815.595898	33.293684
778.297173	56898.732841	33.298701
778.759246	56962.560467	33.303719
779.192700	57041.767311	33.308736
779.833952	57118.121665	33.313754
780.498124	57199.572027	33.318772
781.077178	57290.856787	33.323789
782.189728	57375.475156	33.328807
782.726054	57471.380823	33.333824
783.376418	57551.861755	33.338842
784.471361	57638.714846	33.343860
784.773581	57726.963755	33.348877
785.627103	57817.244827	33.353895
786.174888	57923.154214	33.358912
787.340467	58010.319477	33.363930
788.355024	58097.630258	33.368948
789.116896	58201.584483	33.373965
789.853040	58275.759938	33.378983
790.581442	58382.141001	33.384000
791.077761	58467.384470	33.389018
792.244806	58572.214964	33.394036
792.707298	58677.055521	33.399053
793.372982	58763.017838	33.404071
793.879209	58872.446502	33.409088
794.659123	58966.701048	33.414106
795.598203	59078.245583	33.419124
796.209700	59195.791981	33.424141
797.210282	59296.211100	33.429159
797.547965	59419.213969	33.434176
798.352347	59518.326960	33.439194
799.160638	59636.633234	33.444212
799.944915	59764.942287	33.449229
800.591384	59878.789699	33.454247
801.413257	59995.888708	33.459264
802.170392	60121.038207	33.464282
803.147748	60227.280225	33.469300
803.953997	60351.759388	33.474317
804.793376	60470.191768	33.479335
805.452018	60589.299495	33.484352
806.192934	60714.265736	33.489370
807.293680	60829.522001	33.494388
807.885549	60959.930939	33.499405
808.576961	61074.352733	33.504423
809.213988	61207.524058	33.509440
810.012411	61334.317460	33.514458
811.168309	61463.618411	33.519476
811.929910	61590.716576	33.524493
813.000022	61697.911583	33.529511
815.021442	61791.277913	33.534528
817.200761	61878.967874	33.539546
818.321089	61945.641043	33.544564
818.971042	62042.977958	33.549581
820.011203	62113.248771	33.554599
820.936412	62204.144277	33.559616
821.548095	62274.866005	33.564634
822.317999	62352.994875	33.569652
822.930647	62432.660801	33.574669
823.486264	62519.883496	33.579687
823.808563	62605.994903	33.584704
824.481825	62690.284909	33.589722
825.502989	62782.677726	33.594740
825.672687	62876.387970	33.599757
826.534710	62988.371245	33.604775
826.821558	63090.937578	33.609792
827.387177	63198.698237	33.614810
828.662812	63300.665347	33.619828
828.792157	63429.769821	33.624845
829.582736	63535.175075	33.629863
830.373348	63656.535348	33.634880
831.198425	63769.831146	33.639898
832.095222	63885.163725	33.644916
832.482745	63993.577566	33.649933
834.326801	64071.155392	33.654951
836.088948	64155.612000	33.659968
837.203260	64236.725057	33.664986
838.527445	64303.966241	33.670004
838.969364	64398.776038	33.675021
839.638618	64480.924765	33.680039
840.412722	64562.108206	33.685056
841.061388	64653.382802	33.690074
842.122478	64728.324271	33.695092
842.527281	64837.472943	33.700109
843.286389	64925.082911	33.705127
843.966114	65029.629159	33.710144
844.162376	65141.203576	33.715162
845.132455	65246.246373	33.720180
845.554351	65360.066607	33.725197
846.090130	65468.198026	33.730215
847.074873	65588.797740	33.735232
847.463743	65708.833268	33.740250
848.407749	65834.536483	33.745268
849.267488	65974.497492	33.750285
850.168716	66085.681784	33.755303
850.439168	66226.608379	33.760320
851.450567	66363.019196	33.765338
852.472725	66487.139197	33.770356
853.217810	66630.151840	33.775373
854.255441	66757.084167	33.780391
854.986287	66885.206156	33.785408
855.302844	67019.169792	33.790426
856.926820	67148.706717	33.795444
858.219775	67269.764400	33.800461
859.310001	67402.976172	33.805479
860.328207	67523.246377	33.810496
860.853279	67653.765406	33.815514
861.741030	67785.476875	33.820532
862.432184	67913.478933	33.825549
863.650083	68039.851667	33.830567
865.236998	68144.876145	33.835584
866.213962	68266.896110	33.840602
867.012314	68378.109587	33.845620
867.262902	68509.830155	33.850637
868.395022	68632.787507	33.855655
869.175899	68751.295818	33.860672
869.708164	68883.288084	33.865690
870.907959	68999.578538	33.870708
871.514309	69135.815270	33.875725
872.133349	69266.587865	33.880743
873.263379	69381.728592	33.885760
873.868690	69525.315125	33.890778
875.267971	69634.140235	33.895796
876.064994	69760.403375	33.900813
877.025461	69886.406186	33.905831
878.410647	69999.029290	33.910848
879.581419	70114.116627	33.915866
880.399785	70233.518510	33.920884
880.900356	70350.071488	33.925901
881.944538	70460.331862	33.930919
882.704661	70585.271811	33.935936
883.468063	70707.651036	33.940954
884.665517	70804.773373	33.945972
886.210219	70910.077762	33.950989
887.469047	71014.412060	33.956007
888.634789	71109.220382	33.961024
889.482472	71208.122545	33.966042
890.278832	71300.141172	33.971060
890.953457	71399.945568	33.976077
891.507144	71486.965493	33.981095
892.136836	71585.728514	33.986112
892.641678	71698.595181	33.991130
893.620680	71793.956041	33.996148
894.054827	71897.603103	34.001165
894.632018	72001.037215	34.006183
895.529382	72114.972839	34.011200
895.784000	72245.798775	34.016218
896.544186	72377.635598	34.021236
897.396814	72502.881176	34.026253
898.157878	72627.959284	34.031271
899.341134	72766.450450	34.036288
899.677579	72911.577654	34.041306
900.589793	73032.187324	34.046324
901.910612	73181.048489	34.051341
902.911524	73308.759420	34.056359
903.736694	73440.294682	34.061376
904.471470	73586.049596	34.066394
905.462549	73722.125004	34.071412
906.688142	73848.891142	34.076429
907.623215	73990.144343	34.081447
909.099011	74107.700394	34.086464
910.881438	74208.965512	34.091482
912.582195	74311.408323	34.096500
914.225117	74418.123798	34.101517
914.966809	74511.227598	34.106535
916.335935	74595.247074	34.111552
917.228898	74698.761766	34.116570
918.127832	74783.796007	34.121588
919.253779	74872.031018	34.126605
919.546657	74968.171081	34.131623
920.401279	75044.498571	34.136640
921.183485	75159.651911	34.141658
921.839299	75255.682405	34.146676
922.385273	75374.892165	34.151693
922.793129	75477.055350	34.156711
923.955890	75586.392369	34.161728
924.520650	75717.965553	34.166746
925.614634	75818.688272	34.171764
926.234101	75954.934078	34.176781
926.527508	76075.745427	34.181799
927.668592	76201.963630	34.186816
928.247931	76335.479791	34.191834
929.054739	76462.400089	34.196852
929.997402	76609.335964	34.201869
930.723021	76752.362044	34.206887
931.933417	76886.137320	34.211904
932.227815	77029.477097	34.216922
933.246118	77180.287784	34.221940
934.098757	77323.125681	34.226957
935.230926	77472.224312	34.231975
936.920208	77602.224194	34.236992
937.531301	77753.315072	34.242010
938.494203	77891.919367	34.247028
939.471547	78036.664032	34.252045
939.889196	78185.215518	34.257063
941.309317	78316.364847	34.262080
942.061691	78472.086321	34.267098
942.923285	78608.478979	34.272116
944.076380	78754.628686	34.277133
944.790834	78900.915393	34.282151
946.420734	79037.967536	34.287168
947.545111	79160.435197	34.292186
948.669072	79287.388512	34.297204
949.797872	79416.947943	34.302221
950.071013	79559.263698	34.307239
951.946150	79679.579027	34.312256
952.412665	79819.625000	34.317274
953.445696	79943.851689	34.322292
954.467551	80061.647461	34.327309
955.188539	80173.939597	34.332327
956.046959	80291.725734	34.337344
956.365119	80424.765588	34.342362
957.203983	80561.787464	34.347380
957.603294	80699.148806	34.352397
958.945986	80849.569716	34.357415
960.067209	80974.559212	34.362432
961.596724	81079.528813	34.367450
963.070383	81218.239626	34.372468
964.017495	81347.561908	34.377485
964.683208	81478.355040	34.382503
965.892922	81590.206155	34.387520
966.337095	81727.034845	34.392538
967.028774	81876.298973	34.397556
968.071832	82016.705666	34.402573
968.689562	82157.791144	34.407591
970.037309	82303.425334	34.412608
971.017346	82441.206926	34.417626
971.765896	82579.907158	34.422644
972.678036	82723.237496	34.427661
973.359026	82882.980566	34.432679
974.994316	83016.013084	34.437696
976.288670	83150.728927	34.442714
977.735777	83287.299274	34.447732
978.292174	83422.588369	34.452749
979.195229	83568.215799	34.457767
980.209799	83704.683242	34.462784
981.251469	83853.579470	34.467802
981.944035	83995.366096	34.472820
983.498430	84139.503434	34.477837
983.976857	84291.931530	34.482855
984.986534	84427.056382	34.487872
986.030473	84575.767066	34.492890
986.593333	84725.014092	34.497908
987.346637	84870.725183	34.502925
988.423915	85047.089727	34.507943
989.830443	85184.633431	34.512960
990.271109	85328.178374	34.517978
991.217155	85492.527100	34.522996
992.390610	85642.184877	34.528013
993.397048	85804.083381	34.533031
994.704195	85955.847021	34.538048
995.811859	86110.112500	34.543066
996.791552	86263.248606	34.548084
998.445356	86405.921811	34.553101
999.695343	86553.402334	34.558119
1001.325947	86679.230413	34.563136
1002.282689	86812.909836	34.568154
1003.973340	86917.778017	34.573172
1005.918752	87030.931807	34.578189
1006.507356	87146.418455	34.583207
1007.493733	87253.341319	34.588224
1007.921009	87371.462926	34.593242
1009.216038	87494.693332	34.598260
1010.345678	87610.699962	34.603277
1011.080548	87731.683202	34.608295
1012.249853	87844.944374	34.613312
1012.612282	87963.332822	34.618330
1013.542339	88085.665005	34.623348
1014.356226	88211.864603	34.628365
1015.082569	88345.318828	34.633383
1016.360536	88486.965901	34.638400
1017.494526	88595.503022	34.643418
1017.904233	88727.638706	34.648436
1019.091890	88865.544027	34.653453
1019.361753	89002.975928	34.658471
1020.231946	89135.360213	34.663488
1021.375725	89267.706167	34.668506
1022.190517	89408.296464	34.673524
1023.176127	89550.011030	34.678541
1023.690390	89701.689813	34.683559
1024.206462	89833.813973	34.688576
1025.256582	89985.272739	34.693594
1025.766708	90140.188903	34.698612
1026.936239	90307.097112	34.703629
1028.243892	90462.060226	34.708647
1029.337699	90605.028826	34.713664
1031.062512	90762.051127	34.718682
1032.181204	90920.681291	34.723700
1033.893373	91059.429908	34.728717
1034.454997	91220.135417	34.733735
1035.371577	91364.378403	34.738752
1036.578599	91523.447232	34.743770
1037.134756	91679.960570	34.748788
1038.144104	91827.184565	34.753805
1038.760890	91996.917694	34.758823
1039.673117	92168.621998	34.763840
1040.783740	92338.136332	34.768858
1041.759336	92507.547666	34.773876
1042.482283	92677.432493	34.778893
1043.767859	92849.396122	34.783911
1045.217636	93022.783153	34.788928
1046.150050	93201.124603	34.793946
1047.557872	93363.792605	34.798964
1048.837140	93525.837408	34.803981
1049.603087	93697.102031	34.808999
1050.611351	93863.561441	34.814016
1051.341819	94038.619446	34.819034
1052.318667	94212.650385	34.824052
1053.527852	94390.600103	34.829069
1054.751034	94579.075246	34.834087
1055.575784	94742.349183	34.839104
1056.969425	94921.993852	34.844122
1057.608429	95095.359141	34.849140
1059.064826	95271.577776	34.854157
1060.231002	95462.233971	34.859175
1061.411737	95632.126571	34.864192
1062.497737	95802.998231	34.869210
1063.728550	95982.588992	34.874228
1064.752645	96143.313356	34.879245
1065.726256	96322.227600	34.884263
1066.974270	96490.696932	34.889280
1067.850866	96664.755407	34.894298
1069.021865	96845.970222	34.899316
1070.380662	97005.549457	34.904333
1071.292724	97178.130635	34.909351
1072.266740	97348.809901	34.914368
1073.409333	97523.773466	34.919386
1074.804531	97710.927053	34.924404
1075.858256	97888.237562	34.929421
1076.622467	98055.949387	34.934439
1077.366470	98223.045269	34.939456
1078.863425	98399.469176	34.944474
1080.328769	98579.913300	34.949492
1082.109815	98716.863997	34.954509
1083.044833	98882.254876	34.959527
1083.779761	99048.091542	34.964544
1085.472372	99208.705625	34.969562
1086.038102	99374.572498	34.974580
1087.150266	99530.593639	34.979597
1087.892524	99700.099029	34.984615
1088.769580	99864.524604	34.989632
1089.608097	100033.357802	34.994650
1090.647895	100218.474285	34.999668
1091.600631	100374.489057	35.004685
1092.846672	100539.870768	35.009703
1093.301613	100705.891305	35.014720
1094.576472	100871.213393	35.019738
1095.925625	101051.687995	35.024756
1096.883539	101207.441061	35.029773
1097.856767	101377.014215	35.034791
1099.234693	101541.177516	35.039808
1100.696154	101703.453855	35.044826
1101.475323	101879.153502	35.049844
1102.488348	102044.077026	35.054861
1104.242397	102201.654178	35.059879
1105.424820	102364.721780	35.064896
1106.559857	102535.022848	35.069914
1107.598501	102707.170927	35.074932
1108.555759	102871.406141	35.079949
1109.434294	103038.751760	35.084967
1110.265774	103217.149199	35.089984
1111.244892	103397.005055	35.095002
1111.938064	103588.516237	35.100020
1113.017567	103769.966351	35.105037
1113.891683	103966.965543	35.110055
1114.752945	104159.092564	35.115072
1116.470362	104345.949847	35.120090
1117.708947	104524.871238	35.125108
1119.173474	104721.879471	35.130125
1120.587891	104907.334586	35.135143
1121.750923	105098.861172	35.140160
1122.756141	105278.231678	35.145178
1123.862080	105462.538711	35.150196
1125.144547	105654.074842	35.155213
1126.009193	105838.133226	35.160231
1127.241976	106024.525551	35.165248
1128.582467	106196.944095	35.170266
1129.607519	106387.844306	35.175284
1130.749129	106579.245838	35.180301
1131.774361	106775.025029	35.185319
1132.948795	106960.471010	35.190336
1134.401817	107145.010788	35.195354
1135.124800	107335.929904	35.200372
1135.952311	107530.670835	35.205389
1137.287958	107723.530300	35.210407
1138.164673	107918.747197	35.215424
1139.396244	108113.703983	35.220442
1140.715431	108313.600193	35.225460
1141.860659	108512.475431	35.230477
1143.233803	108703.258406	35.235495
1144.081850	108901.577818	35.240512
1145.600069	109097.773499	35.245530
1146.671149	109309.840302	35.250548
1147.761730	109502.791151	35.255565
1148.725691	109705.682641	35.260583
1149.325678	109904.759892	35.265600
1150.538820	110112.958598	35.270618
1151.604033	110329.163829	35.275636
1152.743165	110531.639723	35.280653
1153.875146	110741.516115	35.285671
1155.121891	110960.331060	35.290688
1156.619878	111155.138816	35.295706
1157.785749	111365.647748	35.300724
1158.555969	111570.941423	35.305741
1160.136836	111790.581637	35.310759
1161.121247	111994.436790	35.315776
1162.150771	112195.511637	35.320794
1163.403071	112411.790897	35.325812
1164.400365	112625.175090	35.330829
1165.814907	112822.567473	35.335847
1166.959030	113031.838529	35.340864
1168.170584	113219.347940	35.345882
1169.059774	113425.775802	35.350900
1170.653858	113613.059714	35.355917
1171.927570	113811.356617	35.360935
1172.536357	114003.836144	35.365952
1173.758918	114200.307287	35.370970
1175.216548	114399.160621	35.375988
1176.682835	114592.933561	35.381005
1178.128487	114775.511574	35.386023
1178.981833	114981.678117	35.391040
1180.192899	115161.180868	35.396058
1181.282969	115370.364332	35.401076
1182.276250	115566.616983	35.406093
1183.641130	115766.331549	35.411111
1184.330530	115979.754333	35.416128
1185.806747	116180.745674	35.421146
1186.452730	116394.077411	35.426164
1187.703326	116597.630463	35.431181
1188.808448	116821.532155	35.436199
1189.587311	117045.020919	35.441216
1190.956470	117261.444770	35.446234
1192.116175	117485.013169	35.451252
1193.440914	117716.589113	35.456269
1194.587613	117933.599772	35.461287
1195.728923	118174.421451	35.466304
1197.057003	118395.776941	35.471322
1198.121416	118630.406422	35.476340
1199.409192	118842.876956	35.481357
1200.704798	119075.647052	35.486375
1202.518902	119300.223357	35.491392
1204.217403	119510.387825	35.496410
1205.313681	119730.170010	35.501428
1206.754312	119930.965353	35.506445
1208.396346	120154.765808	35.511463
1209.609299	120355.753896	35.516480
1211.043125	120565.158866	35.521498
1212.528507	120769.107835	35.526516
1214.158324	120962.288364	35.531533
1216.023305	121136.321590	35.536551
1217.023465	121326.770401	35.541568
1218.019934	121514.483839	35.546586
1219.117143	121721.228328	35.551604
1220.480066	121902.382518	35.556621
1221.854012	122081.685799	35.561639
1223.180298	122281.185533	35.566656
1224.334396	122457.600178	35.571674
1225.721187	122648.766390	35.576692
1226.755095	122831.640954	35.581709
1228.260444	123024.817568	35.586727
1229.154109	123219.757055	35.591744
1230.626448	123406.617780	35.596762
1231.215035	123609.264951	35.601780
1231.829246	123811.338942	35.606797
1233.275692	124002.833415	35.611815
1234.239862	124213.596665	35.616832
1234.784086	124425.673049	35.621850
1235.825391	124643.308226	35.626868
1237.227694	124854.358136	35.631885
1239.716290	125051.883846	35.636903
1240.996063	125261.803605	35.641920
1242.069772	125457.754277	35.646938
1243.406904	125658.580042	35.651956
1244.127456	125872.424326	35.656973
1245.446797	126072.089745	35.661991
1246.362128	126282.723368	35.667008
1248.041132	126497.528387	35.672026
1248.716042	126711.360751	35.677044
1249.616284	126916.982141	35.682061
1250.651597	127125.738486	35.687079
1251.918687	127337.220891	35.692096
1252.867513	127543.282014	35.697114
1253.881233	127760.893252	35.702132
1254.617984	127983.000877	35.707149
1255.632970	128199.436208	35.712167
1256.434716	128442.653023	35.717184
1257.684979	128672.653088	35.722202
1258.984770	128928.833944	35.727220
1260.166802	129171.625779	35.732237
1262.027240	129405.941101	35.737255
1263.521998	129644.666579	35.742272
1265.055565	129876.022818	35.747290
1266.414999	130106.180083	35.752308
1267.651108	130337.627075	35.757325
1269.162651	130581.566679	35.762343
1270.065818	130813.756882	35.767360
1271.286322	131058.952664	35.772378
1272.538128	131286.410969	35.777396
1274.043082	131544.822750	35.782413
1275.271003	131778.271799	35.787431
1276.692104	132028.550405	35.792448
1278.386133	132267.959789	35.797466
1279.688299	132487.064338	35.802484
1281.225279	132730.673886	35.807501
1282.616553	132952.923375	35.812519
1284.010428	133189.942747	35.817536
1285.541290	133413.693505	35.822554
1286.698119	133649.208945	35.827572
1287.913577	133894.084926	35.832589
1289.647617	134120.393041	35.837607
1290.356248	134361.743531	35.842624
1291.705838	134591.617676	35.847642
1292.817253	134822.864098	35.852660
1294.100886	135071.211296	35.857677
1295.419794	135307.599268	35.862695
1296.791602	135549.685258	35.867712
1298.160154	135789.985958	35.872730
1299.542397	136032.986588	35.877748
1300.737180	136281.040685	35.882765
1301.948713	136514.881420	35.887783
1303.558416	136767.066873	35.892800
1304.733585	137005.582761	35.897818
1306.448908	137246.914179	35.902836
1307.832898	137474.875523	35.907853
1309.842401	137699.881950	35.912871
1310.998863	137930.077561	35.917888
1312.451187	138150.995386	35.922906
1313.857476	138386.249634	35.927924
1314.564263	138617.437413	35.932941
1316.150136	138848.899394	35.937959
1317.092876	139087.950420	35.942976
1317.756753	139319.517805	35.947994
1319.080744	139571.720956	35.953012
1320.463682	139831.625397	35.958029
1321.628832	140068.288013	35.963047
1322.584981	140332.730293	35.968064
1323.820251	140586.008063	35.973082
1325.083248	140837.888304	35.978100
1326.162765	141108.402479	35.983117
1327.657956	141364.571964	35.988135
1328.622517	141638.558357	35.993152
1329.484277	141912.906331	35.998170
1331.236024	142179.487913	36.003188
1332.638904	142439.928598	36.008205
1334.020097	142714.475712	36.013223
1335.240926	142982.888725	36.018240
1336.479154	143248.384310	36.023258
1338.326673	143488.254117	36.028276
1339.505104	143745.622207	36.033293
1341.279082	143981.031159	36.038311
1343.282703	144213.715181	36.043328
1344.971422	144432.655723	36.048346
1346.924788	144664.767702	36.053364
1347.910984	144902.811642	36.058381
1349.173157	145130.590093	36.063399
1350.681317	145348.856045	36.068416
1352.452169	145567.777257	36.073434
1354.343071	145787.871982	36.078452
1355.349265	146011.183774	36.083469
1356.779887	146222.163158	36.088487
1358.146526	146450.262385	36.093504
1359.070604	146691.625796	36.098522
1360.056322	146904.927668	36.103540
1361.208057	147151.658981	36.108557
1362.244831	147383.281024	36.113575
1363.391310	147629.737434	36.118592
1364.270477	147882.466933	36.123610
1365.631253	148142.271282	36.128628
1366.506271	148412.304156	36.133645
1367.836295	148673.474402	36.138663
1369.066799	148953.598499	36.143680
1369.970215	149229.111630	36.148698
1371.246916	149505.237105	36.153716
1372.535792	149804.826424	36.158733
1374.357874	150067.713210	36.163751
1375.595676	150355.646842	36.168768
1376.755334	150643.621011	36.173786
1378.062419	150937.128322	36.178804
1379.251958	151251.851759	36.183821
1380.600522	151539.852180	36.188839
1381.885114	151836.756761	36.193856
1383.219163	152149.358167	36.198874
1384.872882	152436.718635	36.203892
1386.292892	152746.494821	36.208909
1387.885862	153050.346659	36.213927
1389.169003	153370.741912	36.218944
1390.465389	153682.727844	36.223962
1392.156829	153984.097244	36.228980
1393.186435	154289.866141	36.233997
1394.757672	154580.211780	36.239015
1397.413774	154868.375483	36.244032
1399.640843	155151.272105	36.249050
1401.446465	155429.902381	36.254068
1402.820220	155713.451951	36.259085
1404.640043	155972.713572	36.264103
1405.991505	156248.748369	36.269120
1407.131082	156523.551687	36.274138
1408.831981	156785.920889	36.279156
1409.605397	157065.761357	36.284173
1411.358006	157325.524998	36.289191
1413.665156	157587.025112	36.294208
1414.783364	157855.206509	36.299226
1416.372716	158112.604700	36.304244
1417.408951	158376.819797	36.309261
1418.873496	158638.161984	36.314279
1420.425193	158893.034175	36.319296
1421.261676	159158.746382	36.324314
1422.525219	159421.725388	36.329332
1423.969567	159703.553397	36.334349
1425.488669	159961.012983	36.339367
1427.377078	160223.157701	36.344384
1428.848056	160487.593455	36.349402
1430.161664	160754.619703	36.354420
1431.469204	161014.962754	36.359437
1432.963287	161273.195861	36.364455
1434.487074	161513.181864	36.369472
1435.678397	161760.760438	36.374490
1437.312504	162005.691584	36.379508
1438.086132	162257.770131	36.384525
1438.972272	162512.001042	36.389543
1440.671456	162780.828615	36.394560
1441.321223	163046.139871	36.399578
1442.940193	163324.702716	36.404596
1444.216698	163601.738225	36.409613
1445.203961	163881.703576	36.414631
1446.317183	164161.281927	36.419648
1447.421534	164464.513600	36.424666
1449.059190	164756.303329	36.429684
1450.373535	165066.102101	36.434701
1451.647073	165358.819041	36.439719
1452.903645	165685.532293	36.444736
1454.136194	165999.360718	36.449754
1455.256212	166318.780222	36.454772
1457.162297	166640.330250	36.459789
1458.319336	166942.720279	36.464807
1459.918304	167284.970123	36.469824
1461.172835	167613.449025	36.474842
1463.047190	167938.630000	36.479860
1464.524868	168267.838039	36.484877
1466.057920	168591.062799	36.489895
1468.143545	168923.867327	36.494912
1469.460039	169256.065854	36.499930
1471.234484	169562.063713	36.504948
1472.587578	169902.534278	36.509965
1473.904303	170224.651794	36.514983
1475.116270	170565.861288	36.520000
1476.217304	170899.135307	36.525018
1477.960442	171244.106692	36.530036
1479.503011	171586.144478	36.535053
1480.988381	171936.493447	36.540071
1482.775482	172266.262604	36.545088
1484.256826	172607.023615	36.550106
1486.567920	172934.477119	36.555124
1487.909435	173265.900717	36.560141
1489.187374	173604.925988	36.565159
1491.196218	173935.152227	36.570176
1492.234810	174275.135637	36.575194
1493.829865	174591.221605	36.580212
1495.464228	174937.329301	36.585229
1496.154075	175273.506886	36.590247
1498.406746	175611.140949	36.595264
1499.906266	175952.569897	36.600282
1501.560992	176282.071285	36.605300
1503.258920	176603.813432	36.610317
1505.215210	176947.622927	36.615335
1506.823640	177262.302485	36.620352
1508.819885	177593.761187	36.625370
1510.323543	177906.038112	36.630388
1511.621866	178219.962842	36.635405
1513.181095	178537.006478	36.640423
1515.259877	178849.092351	36.645440
1516.430051	179168.082796	36.650458
1518.016322	179477.411208	36.655476
1519.573384	179796.722182	36.660493
1520.968758	180104.067995	36.665511
1522.839793	180413.062898	36.670528
1524.341883	180737.986003	36.675546
1526.087592	181021.646372	36.680564
1528.034430	181329.720303	36.685581
1529.064783	181649.853431	36.690599
1530.683149	181941.053764	36.695616
1531.790146	182250.249621	36.700634
1533.257717	182550.337678	36.705652
1534.892986	182850.704243	36.710669
1535.988310	183165.669805	36.715687
1537.500375	183448.137991	36.720704
1539.087678	183753.290041	36.725722
1540.693544	184049.784140	36.730740
1542.483722	184337.389574	36.735757
1543.770638	184635.234418	36.740775
1545.413741	184925.723267	36.745792
1547.174112	185224.394025	36.750810
1548.327800	185517.924644	36.755828
1549.256007	185830.851558	36.760845
1550.456560	186138.568851	36.765863
1552.167753	186459.099774	36.770880
1553.475382	186789.816200	36.775898
1554.974186	187106.159048	36.780916
1556.516581	187426.139528	36.785933
1557.743207	187766.522291	36.790951
1559.589538	188086.519550	36.795968
1560.641455	188438.715160	36.800986
1562.313341	188780.464514	36.806004
1563.491121	189121.294955	36.811021
1565.224209	189472.774587	36.816039
1567.310199	189806.654385	36.821056
1568.915738	190157.486455	36.826074
1570.338253	190505.380453	36.831092
1571.711492	190837.035745	36.836109
1573.588390	191192.437007	36.841127
1575.581445	191543.441473	36.846144
1576.503921	191897.773724	36.851162
1578.703352	192243.238535	36.856180
1580.612548	192580.260577	36.861197
1582.102058	192938.249826	36.866215
1583.719875	193283.918457	36.871232
1584.892416	193640.809064	36.876250
1586.625968	193996.085296	36.881268
1588.090434	194348.082005	36.886285
1589.802201	194709.865804	36.891303
1591.635030	195057.463616	36.896320
1593.441105	195420.518043	36.901338
1594.643647	195766.078658	36.906356
1596.291028	196125.964111	36.911373
1597.906158	196481.019879	36.916391
1600.113902	196835.484210	36.921408
1601.716623	197197.833232	36.926426
1602.975788	197549.538624	36.931444
1604.923099	197903.328192	36.936461
1605.928786	198281.359918	36.941479
1607.456958	198634.880030	36.946496
1608.726439	198991.936289	36.951514
1610.351156	199374.200864	36.956532
1611.814890	199729.019645	36.961549
1613.351037	200112.153650	36.966567
1615.852508	200477.761149	36.971584
1617.322051	200845.128667	36.976602
1618.710012	201207.280677	36.981620
1620.259566	201575.121202	36.986637
1621.863226	201951.880378	36.991655
1623.688892	202314.663781	36.996672
1625.293388	202700.022390	37.001690
1626.729337	203080.827432	37.006708
1628.490392	203455.511461	37.011725
1629.507127	203831.920588	37.016743
1631.223544	204224.213877	37.021760
1632.638248	204597.513629	37.026778
1634.227156	204980.448879	37.031796
1635.974810	205367.143519	37.036813
1636.946658	205760.850630	37.041831
1639.161062	206137.580629	37.046848
1640.773596	206507.542938	37.051866
1642.275478	206883.442356	37.056884
1644.197011	207246.690785	37.061901
1645.793860	207616.470461	37.066919
1647.820918	207975.666914	37.071936
1649.520519	208337.712743	37.076954
1651.220343	208688.154429	37.081972
1653.391146	209051.928428	37.086989
1655.132044	209403.801231	37.092007
1657.442321	209753.917737	37.097024
1658.605689	210123.412428	37.102042
1660.364472	210469.471118	37.107060
1661.658858	210829.474484	37.112077
1663.047290	211204.752321	37.117095
1664.680547	211560.182076	37.122112
1666.524787	211931.933639	37.127130
1667.814361	212293.772482	37.132148
1669.794201	212661.466626	37.137165
1671.299692	213048.059929	37.142183
1673.880228	213392.267121	37.147200
1676.868772	213733.690536	37.152218
1678.989611	214075.690810	37.157236
1680.973058	214407.149924	37.162253
1682.994753	214747.238962	37.167271
1684.747703	215085.824555	37.172288
1686.301071	215417.409369	37.177306
1687.565846	215761.538766	37.182324
1688.542703	216096.751775	37.187341
1690.071894	216455.545078	37.192359
1691.406794	216803.247685	37.197376
1692.706833	217164.545187	37.202394
1694.238635	217528.421603	37.207412
1695.844656	217895.030052	37.212429
1697.214615	218268.790464	37.217447
1698.659521	218635.733108	37.222464
1700.357266	219040.046963	37.227482
1701.984939	219461.898971	37.232500
1704.424859	219841.380259	37.237517
1706.247983	220216.520386	37.242535
1708.104493	220582.487367	37.247552
1710.130980	220947.386082	37.252570
1711.583479	221342.199494	37.257588
1713.804493	221696.985129	37.262605
1714.768808	222076.998289	37.267623
1716.196627	222465.851044	37.272640
1718.188671	222852.630495	37.277658
1719.400094	223251.630732	37.282676
1720.757166	223644.639350	37.287693
1722.222529	224040.044309	37.292711
1723.674142	224439.135824	37.297728
1725.612408	224843.253370	37.302746
1726.751992	225269.729456	37.307764
1728.580420	225679.989356	37.312781
1729.983200	226109.218737	37.317799
1731.380645	226525.318656	37.322816
1734.010689	226937.075450	37.327834
1735.789409	227356.594723	37.332852
1737.856096	227762.224473	37.337869
1739.823377	228179.149715	37.342887
1741.808693	228582.788842	37.347904
1743.574021	229003.204581	37.352922
1744.960625	229416.318202	37.357940
1746.662200	229830.142877	37.362957
1748.002745	230249.261156	37.367975
1749.721459	230666.920949	37.372992
1751.448190	231079.525841	37.378010
1752.877774	231510.647641	37.383028
1754.765260	231929.857915	37.388045
1756.449241	232344.302265	37.393063
1758.182393	232753.100521	37.398080
1759.899992	233158.930479	37.403098
1761.394095	233571.860075	37.408116
1762.963319	233986.708784	37.413133
1764.332906	234413.809716	37.418151
1765.677636	234844.243457	37.423168
1767.231912	235284.270757	37.428186
1768.895072	235721.309141	37.433204
1770.661821	236165.977351	37.438221
1772.307804	236610.057033	37.443239
1773.947282	237069.456164	37.448256
1775.779536	237523.515484	37.453274
1777.555418	237990.108381	37.458292
1779.405098	238438.095897	37.463309
1780.768437	238909.992141	37.468327
1782.731692	239384.203261	37.473344
1784.546390	239848.711040	37.478362
1786.000827	240322.551338	37.483380
1788.047667	240799.723795	37.488397
1789.529601	241289.615833	37.493415
1791.724834	241775.326320	37.498432
1794.255158	242251.354744	37.503450
1795.697181	242737.750831	37.508468
1798.245866	243201.076784	37.513485
1800.637975	243660.974758	37.518503
1802.798924	244130.514018	37.523520
1805.027369	244588.027429	37.528538
1806.844713	245047.692718	37.533556
1808.579497	245496.601640	37.538573
1810.777530	245946.958626	37.543591
1813.016221	246402.339276	37.548608
1814.480004	246845.376166	37.553626
1816.277174	247302.380782	37.558644
1818.188344	247766.200484	37.563661
1820.229596	248209.930889	37.568679
1822.034444	248665.538768	37.573696
1823.900128	249112.830304	37.578714
1825.620972	249568.986573	37.583732
1828.408996	249995.371927	37.588749
1830.281399	250439.132682	37.593767
1832.048621	250887.458427	37.598784
1834.328784	251310.702901	37.603802
1835.679433	251751.172637	37.608820
1837.924186	252171.832516	37.613837
1839.710327	252606.515020	37.618855
1841.124007	253050.633307	37.623872
1843.193132	253478.359816	37.628890
1844.589249	253934.878317	37.633908
1846.347471	254385.494328	37.638925
1847.812954	254830.240112	37.643943
1849.259758	255288.198879	37.648960
1851.019416	255744.099136	37.653978
1852.624630	256219.611067	37.658996
1854.183275	256669.016287	37.664013
1856.571345	257144.449574	37.669031
1859.111646	257588.713298	37.674048
1861.509238	258038.030584	37.679066
1863.707052	258486.923754	37.684084
1865.787522	258919.375050	37.689101
1867.397007	259362.649977	37.694119
1869.689689	259787.165664	37.699136
1871.998524	260211.704039	37.704154
1874.130441	260640.387001	37.709172
1876.202198	261035.115665	37.714189
1878.665356	261448.831854	37.719207
1880.546629	261857.081031	37.724224
1882.374023	262255.304725	37.729242
1883.928780	262653.497250	37.734260
1886.035527	263035.035259	37.739277
1887.739957	263411.889373	37.744295
1889.758682	263790.774321	37.749312
1891.896008	264156.201148	37.754330
1893.184387	264536.705539	37.759348
1894.640377	264913.777932	37.764365
1896.948649	265302.902429	37.769383
1898.199176	265704.014403	37.774400
1900.100404	266092.062700	37.779418
1901.763304	266501.666658	37.784436
1903.133686	266911.496589	37.789453
1904.581085	267324.742844	37.794471
1905.972591	267757.837790	37.799488
1907.265394	268196.257913	37.804506
1909.080952	268645.184041	37.809524
1910.471364	269097.152271	37.814541
1912.258137	269569.554497	37.819559
1913.352025	270038.463719	37.824576
1915.263062	270518.083987	37.829594
1917.034952	271007.125704	37.834612
1918.600698	271506.006344	37.839629
1920.475763	272005.241413	37.844647
1921.883767	272515.450827	37.849664
1923.738114	273023.578614	37.854682
1925.663374	273554.810149	37.859700
1927.292934	274085.175167	37.864717
1929.340826	274615.190404	37.869735
1931.028085	275159.210264	37.874752
1933.302172	275696.958936	37.879770
1934.994168	276241.610685	37.884788
1936.659645	276791.422233	37.889805
1938.713397	277351.329025	37.894823
1940.500994	277898.704419	37.899840
1943.472701	278460.793283	37.904858
1945.452153	279002.215349	37.909876
1947.664749	279558.127271	37.914893
1950.021362	280102.633722	37.919911
1952.105416	280653.305625	37.924928
1954.567765	281184.734922	37.929946
1956.452114	281735.233480	37.934964
1958.605275	282277.760514	37.939981
1960.361001	282821.647178	37.944999
1961.966478	283368.071742	37.950016
1964.619408	283905.913145	37.955034
1967.126731	284440.881154	37.960052
1969.192000	284974.066317	37.965069
1971.750483	285484.611788	37.970087
1974.358642	286014.960117	37.975104
1976.655185	286507.028213	37.980122
1979.004707	287026.290188	37.985140
1981.241577	287522.200283	37.990157
1983.373331	288005.806749	37.995175
1985.300656	288506.489192	38.000192
1986.962594	289003.098903	38.005210
1988.880585	289500.197787	38.010228
1990.971989	290000.466527	38.015245
1993.273070	290496.405995	38.020263
1995.180772	290992.992925	38.025280
1997.307792	291483.877388	38.030298
1999.065834	291959.123915	38.035316
2000.669352	292467.744137	38.040333
2002.939617	292956.211433	38.045351
2004.556642	293458.881715	38.050368
2006.710285	293943.833734	38.055386
2008.777969	294438.856121	38.060404
2010.754323	294935.059868	38.065421
2012.760582	295419.496685	38.070439
2014.326990	295899.584830	38.075456
2016.034376	296377.768013	38.080474
2018.012098	296853.847011	38.085492
2019.439188	297350.994436	38.090509
2021.367495	297828.448806	38.095527
2022.445845	298350.514492	38.100544
2024.721013	298845.152292	38.105562
2026.728842	299355.731255	38.110580
2028.632823	299862.464329	38.115597
2030.743840	300372.081295	38.120615
2032.682957	300894.346806	38.125632
2034.531951	301414.668818	38.130650
2036.152305	301956.105831	38.135668
2037.581968	302491.653749	38.140685
2040.150274	303031.708486	38.145703
2041.663526	303584.938134	38.150720
2044.031753	304136.803762	38.155738
2045.902535	304686.716668	38.160756
2048.058463	305244.274124	38.165773
2050.919963	305770.727505	38.170791
2053.164829	306323.031689	38.175808
2055.399918	306873.378445	38.180826
2057.618248	307434.162159	38.185844
2059.709811	307974.519512	38.190861
2062.127299	308527.136251	38.195879
2064.472187	309069.552325	38.200896
2066.529397	309602.590776	38.205914
2069.072433	310143.468508	38.210932
2071.343490	310687.130268	38.215949
2073.725387	311214.415681	38.220967
2075.673994	311756.269615	38.225984
2078.065356	312278.314943	38.231002
2080.505325	312803.802274	38.236020
2082.731082	313336.533352	38.241037
2085.641851	313837.354026	38.246055
2087.717487	314364.719119	38.251072
2090.109816	314866.177350	38.256090
2092.143056	315387.015960	38.261108
2094.014608	315901.910196	38.266125
2095.858480	316429.476419	38.271143
2097.078223	316952.393634	38.276160
2098.671185	317485.859259	38.281178
2100.306246	318032.365527	38.286196
2102.065698	318581.513048	38.291213
2103.915619	319136.735255	38.296231
2105.740324	319703.637312	38.301248
2107.643762	320279.967205	38.306266
2109.543666	320844.561881	38.311284
2111.326723	321432.073871	38.316301
2113.569962	322014.476957	38.321319
2115.251737	322607.733428	38.326336
2117.449577	323201.127447	38.331354
2119.457585	323797.441837	38.336372
2121.479277	324403.548822	38.341389
2123.894323	324999.657390	38.346407
2125.689886	325611.020299	38.351424
2127.907553	326222.332577	38.356442
2130.400757	326825.468594	38.361460
2132.393282	327436.348853	38.366477
2134.745907	328032.818747	38.371495
2136.717222	328647.549072	38.376512
2138.438585	329272.697978	38.381530
2140.458236	329882.304296	38.386548
2142.819694	330508.349312	38.391565
2145.013520	331112.912364	38.396583
2147.078882	331740.795294	38.401600
2149.172293	332369.377359	38.406618
2151.689608	332979.604028	38.411636
2153.611509	333577.128023	38.416653
2155.778577	334167.217649	38.421671
2157.926555	334745.956738	38.426688
2159.995289	335342.624614	38.431706
2162.008584	335946.072745	38.436724
2164.202612	336538.873328	38.441741
2167.030675	337131.308378	38.446759
2168.787404	337735.438427	38.451776
2170.882887	338325.874293	38.456794
2173.746486	338920.288272	38.461812
2175.382205	339530.204646	38.466829
2177.589810	340128.215973	38.471847
2179.878795	340738.212602	38.476864
2182.153919	341345.513548	38.481882
2184.022483	341961.326511	38.486900
2185.734399	342585.025955	38.491917
2188.322024	343209.384596	38.496935
2190.291925	343841.121770	38.501952
2192.014069	344463.247061	38.506970
2194.670986	345097.518820	38.511988
2196.678015	345743.818210	38.517005
2199.307815	346365.945821	38.522023
2201.602610	347003.525742	38.527040
2203.989015	347640.320340	38.532058
2206.299879	348276.103480	38.537076
2208.609309	348922.308383	38.542093
2210.731242	349556.480693	38.547111
2212.892135	350207.234397	38.552128
2214.847113	350848.470964	38.557146
2217.222964	351488.867261	38.562164
2219.164063	352151.555819	38.567181
2221.449681	352806.183885	38.572199
2223.683723	353459.338837	38.577216
2225.998694	354119.194884	38.582234
2228.477088	354778.049455	38.587252
2230.764196	355445.349749	38.592269
2233.000941	356100.417615	38.597287
2235.255289	356770.671049	38.602304
2237.477345	357424.426532	38.607322
2239.625159	358094.092642	38.612340
2241.554880	358768.604675	38.617357
2243.851897	359450.047362	38.622375
2245.956947	360133.184885	38.627392
2247.696033	360822.587294	38.632410
2249.851524	361513.405723	38.637428
2252.030178	362213.975776	38.642445
2253.993596	362910.154701	38.647463
2256.309455	363616.004655	38.652480
2258.670879	364325.436610	38.657498
2260.957371	365025.710005	38.662516
2263.307899	365736.360805	38.667533
2265.832783	366426.726374	38.672551
2268.266427	367127.317301	38.677568
2270.816746	367825.694353	38.682586
2273.791696	368529.137323	38.687604
2275.872880	369228.757945	38.692621
2278.148008	369909.816786	38.697639
2280.458309	370616.018700	38.702656
2282.635823	371316.192290	38.707674
2285.206322	372008.627504	38.712692
2287.277670	372700.345784	38.717709
2289.496629	373404.250969	38.722727
2291.905246	374094.263165	38.727744
2294.115031	374802.986223	38.732762
2297.047181	375477.363407	38.737780
2299.480893	376168.953782	38.742797
2302.530927	376843.944333	38.747815
2304.986552	377500.786603	38.752832
2307.486119	378147.871151	38.757850
2310.576016	378772.656946	38.762868
2312.817233	379386.997416	38.767885
2314.840623	380014.954467	38.772903
2316.736472	380641.551608	38.777920
2318.454733	381285.687866	38.782938
2320.419783	381926.525193	38.787956
2322.570134	382568.587204	38.792973
2324.806509	383219.801017	38.797991
2327.090718	383865.289144	38.803008
2328.732433	384541.245132	38.808026
2331.344681	385189.771167	38.813044
2334.122742	385846.166864	38.818061
2336.749902	386496.717636	38.823079
2338.952482	387172.043700	38.828096
2341.125112	387832.808550	38.833114
2343.718445	388505.100667	38.838132
2345.364141	389193.201840	38.843149
2347.240330	389884.747967	38.848167
2349.888182	390571.765502	38.853184
2351.748296	391260.393736	38.858202
2354.030491	391954.133031	38.863220
2356.452280	392655.437741	38.868237
2358.509233	393366.418527	38.873255
2360.837368	394074.397512	38.878272
2363.023089	394811.987293	38.883290
2366.562846	395492.536167	38.888308
2369.570761	396197.412306	38.893325
2372.863692	396890.921042	38.898343
2375.556616	397578.405005	38.903360
2377.478783	398278.494436	38.908378
2380.263502	398971.531184	38.913396
2382.677693	399666.487984	38.918413
2384.959811	400361.551276	38.923431
2387.361568	401052.295414	38.928448
2389.383738	401756.946536	38.933466
2392.113199	402438.683231	38.938484
2394.259382	403147.308203	38.943501
2396.494925	403845.233305	38.948519
2398.900617	404557.555077	38.953536
2401.072354	405254.695425	38.958554
2403.341538	405968.954561	38.963572
2405.405759	406700.913169	38.968589
2407.541678	407437.223289	38.973607
2409.786804	408155.229747	38.978624
2412.150653	408881.962901	38.983642
2414.744760	409617.200827	38.988660
2417.326070	410347.506417	38.993677
2419.716084	411089.172131	38.998695
2422.598007	411818.349195	39.003712
2424.954209	412555.724099	39.008730
2427.472964	413280.361649	39.013748
2429.955321	414024.184137	39.018765
2432.052829	414770.835214	39.023783
2434.378938	415504.940874	39.028800
2436.491937	416254.813890	39.033818
2438.923594	416995.647144	39.038836
2441.052647	417771.406523	39.043853
2443.343030	418524.096189	39.048871
2446.092263	419282.334674	39.053888
2447.998795	420053.148532	39.058906
2450.507472	420819.585079	39.063924
2452.850857	421593.393895	39.068941
2455.041330	422366.874836	39.073959
2457.740878	423142.905916	39.078976
2460.033651	423925.233586	39.083994
2462.739296	424697.999201	39.089012
2465.314062	425456.533976	39.094029
2467.648382	426196.401631	39.099047
2470.827889	426937.625713	39.104064
2473.643687	427674.583736	39.109082
2475.986484	428384.612934	39.114100
2478.979102	429124.889120	39.119117
2481.944601	429826.824030	39.124135
2484.361467	430545.028317	39.129152
2486.997661	431255.328121	39.134170
2489.984378	431957.297387	39.139188
2492.592270	432668.773941	39.144205
2495.371747	433367.596773	39.149223
2498.045457	434065.100069	39.154240
2500.217540	434777.393966	39.159258
2502.490594	435478.210748	39.164276
2504.932624	436201.044404	39.169293
2507.135057	436920.554637	39.174311
2509.803752	437639.509469	39.179328
2511.686071	438373.702775	39.184346
2514.087586	439109.759817	39.189364
2516.063626	439845.053517	39.194381
2519.218399	440580.330364	39.199399
2522.403478	441296.552623	39.204416
2524.895504	442038.772400	39.209434
2527.303443	442778.957328	39.214452
2529.766971	443530.542424	39.219469
2531.912465	444274.869077	39.224487
2534.805485	445028.355304	39.229504
2537.035376	445778.333343	39.234522
2539.633643	446523.722178	39.239540
2542.547736	447291.290518	39.244557
2544.725113	448046.813290	39.249575
2547.810826	448806.458485	39.254592
2549.924317	449572.964602	39.259610
2552.386225	450329.826094	39.264628
2555.023008	451100.995181	39.269645
2557.478753	451877.526839	39.274663
2560.191187	452644.277304	39.279680
2562.574329	453441.447032	39.284698
2564.702808	454225.480464	39.289716
2567.344576	455016.074054	39.294733
2569.645719	455808.463447	39.299751
2572.019995	456613.349722	39.304768
2574.423848	457416.834258	39.309786
2576.544475	458231.507439	39.314804
2579.429991	459029.438669	39.319821
2582.264595	459839.581030	39.324839
2585.110972	460646.453410	39.329856
2588.284653	461467.494386	39.334874
2590.903236	462275.652961	39.339892
2593.437745	463086.319877	39.344909
2596.132356	463896.067805	39.349927
2599.017853	464700.646063	39.354944
2601.439056	465509.816773	39.359962
2604.076878	466327.964457	39.364980
2606.745340	467141.019058	39.369997
2609.146832	467968.384824	39.375015
2612.175218	468758.622114	39.380032
2614.698196	469564.574768	39.385050
2617.543959	470376.654979	39.390068
2620.202369	471195.805170	39.395085
2622.493076	472002.602698	39.400103
2624.871447	472818.849288	39.405120
2627.645211	473633.732136	39.410138
2630.470821	474443.923503	39.415156
2633.156159	475259.154433	39.420173
2635.478132	476077.339532	39.425191
2638.588461	476880.306116	39.430208
2641.313744	477676.685003	39.435226
2644.342515	478438.382793	39.440244
2647.235743	479209.919616	39.445261
2649.779882	479968.401743	39.450279
2652.548431	480728.532150	39.455296
2654.690364	481494.289130	39.460314
2657.041601	482253.667175	39.465332
2659.404323	483025.483131	39.470349
2661.964753	483798.798439	39.475367
2665.333322	484561.596439	39.480384
2667.933381	485337.665969	39.485402
2670.116263	486114.426947	39.490420
2672.897212	486896.860356	39.495437
2675.039832	487689.763550	39.500455
2677.706809	488495.012197	39.505472
2680.047751	489309.615702	39.510490
2682.322496	490110.160723	39.515508
2685.177227	490946.760275	39.520525
2687.797823	491770.640262	39.525543
2690.465591	492594.826408	39.530560
2692.299033	493434.351006	39.535578
2694.657165	494278.995607	39.540596
2697.646913	495126.218686	39.545613
2700.503186	495987.044686	39.550631
2703.108907	496851.248793	39.555648
2705.532308	497720.483900	39.560666
2708.465800	498595.038081	39.565684
2711.387337	499464.655442	39.570701
2714.237346	500345.134945	39.575719
2717.070339	501212.960717	39.580736
2720.163413	502087.960988	39.585754
2723.385556	502965.011799	39.590772
2727.530369	503802.122879	39.595789
2730.031022	504655.045897	39.600807
2733.242216	505519.404968	39.605824
2735.688934	506376.986962	39.610842
2738.027099	507234.138212	39.615860
2740.662640	508106.421237	39.620877
2743.310202	508978.705447	39.625895
2745.731518	509852.240002	39.630912
2748.047930	510739.556626	39.635930
2750.165715	511628.671368	39.640948
2753.100288	512514.576905	39.645965
2755.707873	513414.952236	39.650983
2758.400470	514308.206209	39.656000
2761.403116	515221.919650	39.661018
2764.093210	516140.519550	39.666036
2767.049727	517041.737427	39.671053
2769.508910	517957.849489	39.676071
2772.684515	518867.692302	39.681088
2775.089034	519800.885068	39.686106
2777.574384	520725.846516	39.691124
2780.429923	521652.101315	39.696141
2783.062565	522584.179857	39.701159
2785.655954	523513.789995	39.706176
2788.448765	524452.275145	39.711194
2791.234499	525396.394025	39.716212
2794.437793	526332.125548	39.721229
2796.785171	527286.773396	39.726247
2799.450352	528227.561194	39.731264
2802.324005	529190.106753	39.736282
2804.705283	530149.499348	39.741300
2807.649095	531097.761657	39.746317
2810.384579	532067.140023	39.751335
2812.882308	533029.798769	39.756352
2815.887678	533998.299675	39.761370
2818.770803	534974.104425	39.766388
2821.690164	535941.432893	39.771405
2823.629896	536909.965664	39.776423
2826.973591	537839.253413	39.781440
2830.444948	538773.843621	39.786458
2832.948181	539714.670993	39.791476
2835.745478	540634.307618	39.796493
2838.097498	541571.766815	39.801511
2840.897364	542516.031586	39.806528
2843.891160	543448.128950	39.811546
2847.201795	544400.079717	39.816564
2850.038509	545338.062550	39.821581
2852.540849	546301.081837	39.826599
2855.098249	547241.999846	39.831616
2857.964269	548203.569628	39.836634
2860.331676	549179.434134	39.841652
2863.341445	550153.463985	39.846669
2866.527309	551112.263503	39.851687
2869.115820	552100.451272	39.856704
2872.202467	553087.127673	39.861722
2874.919789	554079.472810	39.866740
2877.918860	555055.314465	39.871757
2880.866790	556058.833891	39.876775
2884.003605	557053.051200	39.881792
2886.964115	558046.469975	39.886810
2890.163152	559034.951874	39.891828
2894.193261	560012.220345	39.896845
2897.711441	560991.611098	39.901863
2901.110983	561965.322738	39.906880
2904.160483	562939.070285	39.911898
2907.096989	563905.682484	39.916916
2910.052670	564866.193443	39.921933
2913.281307	565837.886993	39.926951
2916.746633	566784.161277	39.931968
2920.304127	567726.585275	39.936986
2922.624036	568678.935012	39.942004
2925.465535	569639.210271	39.947021
2928.597327	570598.210858	39.952039
2931.513425	571545.831090	39.957056
2934.660249	572495.400290	39.962074
2937.329908	573450.096246	39.967092
2940.417975	574403.145323	39.972109
2943.027802	575365.835680	39.977127
2945.768276	576319.198328	39.982144
2949.074224	577285.138274	39.987162
2951.436641	578251.059066	39.992180
2954.473040	579235.554428	39.997197
2957.237376	580217.006951	40.002215
2959.369479	581189.708798	40.007232
2962.388094	582199.650259	40.012250
2965.046113	583204.152281	40.017268
2967.158003	584209.313940	40.022285
2969.975820	585236.788311	40.027303
2972.282329	586260.951417	40.032320
2975.758231	587283.180166	40.037338
2978.850417	588317.466122	40.042356
2982.186338	589338.490868	40.047373
2985.285487	590383.373804	40.052391
2988.601134	591409.738001	40.057408
2992.505969	592423.890125	40.062426
2995.410466	593439.573999	40.067444
2999.656971	594424.137002	40.072461
3003.498441	595422.861939	40.077479
3006.441051	596418.945658	40.082496
3009.656638	597394.163240	40.087514
3012.633627	598374.046682	40.092532
3016.344008	599338.552331	40.097549
3019.444859	600315.397098	40.102567
3022.053293	601271.761810	40.107584
3025.003341	602237.253116	40.112602
3027.897366	603191.708929	40.117620
3030.573854	604125.346996	40.122637
3033.151845	605048.864172	40.127655
3035.704939	605982.120553	40.132672
3038.391759	606918.681366	40.137690
3041.024286	607878.543442	40.142708
3043.736235	608825.701350	40.147725
3046.657557	609792.958608	40.152743
3049.141429	610755.101962	40.157760
3052.105099	611720.835232	40.162778
3054.768276	612716.446987	40.167796
3057.479332	613714.712712	40.172813
3060.330404	614727.068796	40.177831
3063.072154	615729.949091	40.182848
3066.041822	616755.701624	40.187866
3068.751128	617791.701075	40.192884
3071.472022	618821.751609	40.197901
3075.097482	619870.800948	40.202919
3077.915566	620934.377934	40.207936
3081.189520	621991.878011	40.212954
3083.783430	623067.727503	40.217972
3087.180242	624140.338955	40.222989
3090.194140	625232.642323	40.228007
3093.586882	626309.884306	40.233024
3097.245387	627381.978510	40.238042
3100.412198	628467.532188	40.243060
3103.638055	629546.822224	40.248077
3107.360755	630623.972568	40.253095
3110.638836	631708.776202	40.258112
3113.836395	632790.585556	40.263130
3116.375494	633888.018005	40.268148
3119.547093	634978.541860	40.273165
3122.228323	636083.956439	40.278183
3124.901390	637205.724012	40.283200
3128.220658	638308.001459	40.288218
3130.860388	639438.115508	40.293236
3133.732698	640571.210166	40.298253
3137.109169	641703.048798	40.303271
3140.145081	642845.742053	40.308288
3143.698230	643970.167487	40.313306
3147.487460	645113.778314	40.318324
3150.647552	646254.222724	40.323341
3153.881922	647397.168483	40.328359
3156.960204	648540.708201	40.333376
3160.131442	649679.715842	40.338394
3163.409188	650823.859193	40.343412
3166.545845	651970.535785	40.348429
3170.201106	653110.317360	40.353447
3173.922115	654238.946143	40.358464
3177.715727	655375.753356	40.363482
3180.937665	656498.775933	40.368500
3184.441203	657616.891944	40.373517
3187.883047	658738.675167	40.378535
3190.321247	659873.242581	40.383552
3193.301501	660982.992662	40.388570
3196.222695	662122.096740	40.393588
3199.456589	663253.847063	40.398605
3202.406397	664395.764195	40.403623
3205.604874	665533.672597	40.408640
3209.194223	666666.803358	40.413658
3211.999524	667821.621516	40.418676
3215.239671	668957.323874	40.423693
3218.497330	670109.650098	40.428711
3221.179104	671266.655962	40.433728
3224.277563	672408.383211	40.438746
3227.354403	673575.184772	40.443764
3230.710808	674725.338731	40.448781
3234.717363	675879.767276	40.453799
3238.583000	676978.606019	40.458816
3241.656463	678074.215288	40.463834
3245.150387	679163.215083	40.468852
3248.862599	680243.206094	40.473869
3252.273860	681321.132930	40.478887
3255.325842	682388.858852	40.483904
3258.450259	683464.544431	40.488922
3261.358472	684551.015356	40.493940
3263.935081	685637.113522	40.498957
3266.719918	686735.112723	40.503975
3269.520858	687851.692486	40.508992
3272.605335	688972.008803	40.514010
3275.074527	690116.111277	40.519028
3277.910489	691255.292780	40.524045
3281.336254	692408.075863	40.529063
3284.353634	693570.055300	40.534080
3287.556520	694741.228092	40.539098
3290.644709	695925.954992	40.544116
3293.511871	697121.073634	40.549133
3296.479566	698335.055134	40.554151
3298.750493	699558.850606	40.559168
3302.278902	700791.735823	40.564186
3304.997828	702049.066483	40.569204
3308.331641	703298.234100	40.574221
3312.233105	704544.898277	40.579239
3315.708937	705821.278998	40.584256
3319.290059	707084.028839	40.589274
3322.498624	708367.853579	40.594292
3325.544788	709643.391173	40.599309
3328.752153	710937.081749	40.604327
3332.172544	712235.095263	40.609344
3336.208718	713524.443031	40.614362
3339.608687	714823.795866	40.619380
3342.610861	716121.925608	40.624397
3345.981005	717435.527765	40.629415
3349.118571	718757.916354	40.634432
3352.634169	720067.074270	40.639450
3355.620414	721394.213788	40.644468
3359.004939	722728.492091	40.649485
3363.336001	724044.798986	40.654503
3366.417936	725375.585033	40.659520
3369.809504	726701.903617	40.664538
3373.291045	728026.954928	40.669556
3377.016495	729362.965980	40.674573
3380.554805	730689.106784	40.679591
3383.963329	732035.499459	40.684608
3387.911853	733352.937736	40.689626
3391.175929	734678.864742	40.694644
3394.344120	736004.539490	40.699661
3398.189184	737327.365833	40.704679
3401.135083	738667.887102	40.709696
3404.633664	740000.937012	40.714714
3408.095381	741327.553270	40.719732
3410.984339	742668.542846	40.724749
3414.456846	744003.142214	40.729767
3417.752959	745356.379320	40.734784
3421.001839	746702.291614	40.739802
3424.199374	748052.958757	40.744820
3427.610274	749411.537026	40.749837
3431.673459	750764.103381	40.754855
3434.998157	752115.372976	40.759872
3438.492119	753477.657306	40.764890
3442.125748	754819.387655	40.769908
3445.432033	756168.076708	40.774925
3449.143194	757503.218158	40.779943
3452.850658	758843.146682	40.784960
3456.432747	760179.660710	40.789978
3459.925372	761534.453932	40.794996
3463.183993	762856.015490	40.800000
3466.804922	764128.264919	40.805005
3470.064650	765351.449011	40.810010
3473.453240	766503.770627	40.815015
3477.017880	767588.753762	40.820020
3479.953770	768613.509185	40.825024
3483.295512	769547.240864	40.830029
3485.554848	770437.134131	40.835034
3488.189125	771263.898412	40.840039
3490.991861	772002.170844	40.845044
3493.033469	772684.295144	40.850048
3495.577100	773302.542712	40.855053
3498.038129	773855.844234	40.860058
3500.083450	774349.833953	40.865063
3501.963800	774781.330964	40.870068
3503.790185	775170.023354	40.875072
3506.044485	775496.242291	40.880077
3507.522745	775763.001428	40.885082
3509.306233	775980.615246	40.890087
3510.666352	776160.236457	40.895092
3511.549522	776317.138261	40.900096
3513.092104	776403.332044	40.905101
3513.852413	776466.516137	40.910106
3515.348761	776493.935966	40.915111
3516.163519	776490.946061	40.920116
3516.802337	776447.567641	40.925120
3517.826115	776386.254794	40.930125
3518.231006	776307.812947	40.935130
3518.762290	776184.991830	40.940135
3519.510587	776051.104718	40.945140
3519.783573	775905.674603	40.950144
3520.217487	775733.677577	40.955149
3520.524947	775551.997945	40.960154
3521.059072	775353.437244	40.965159
3521.455718	775135.149195	40.970164
3521.420882	774905.452979	40.975168
3522.003810	774663.287788	40.980173
3521.983554	774422.593089	40.985178
3522.467239	774153.983697	40.990183
3522.321089	773875.028167	40.995188
3522.441597	773607.000494	41.000192
3522.692552	773320.423192	41.005197
3522.888114	773027.736528	41.010202
3523.002238	772724.363385	41.015207
3522.971562	772425.730327	41.020212
3522.525456	772120.405343	41.025216
3523.000530	771799.595328	41.030221
3523.149760	771490.007940	41.035226
3523.077316	771163.644763	41.040231
3522.915690	770842.898390	41.045236
3522.946973	770515.307021	41.050240
3522.995581	770180.061157	41.055245
3523.169635	769862.222377	41.060250
3523.295088	769523.090714	41.065255
3522.942709	769185.697965	41.070260
3522.787582	768855.107287	41.075264
3522.816277	768490.663425	41.080269
3522.549276	768171.691607	41.085274
3522.610388	767830.226146	41.090279
3522.648900	767495.600019	41.095284
3522.516473	767150.192184	41.100288
3523.272362	766804.818734	41.105293
3522.530602	766458.148590	41.110298
3522.341369	766120.195515	41.115303
3521.972324	765770.227423	41.120308
3521.952965	765440.103688	41.125312
3522.049626	765087.512238	41.130317
3521.623327	764746.331403	41.135322
3521.685709	764410.774242	41.140327
3521.535938	764076.321996	41.145332
3521.516683	763742.129169	41.150336
3521.620676	763391.478677	41.155341
3521.496874	763066.939165	41.160346
3521.363061	762729.514536	41.165351
3521.370518	762384.209048	41.170356
3520.819030	762056.244014	41.175360
3520.982959	761719.168874	41.180365
3520.575026	761390.953882	41.185370
3520.579611	761063.051113	41.190375
3520.722470	760737.676643	41.195380
3520.515296	760408.004438	41.200384
3520.334097	760068.988634	41.205389
3520.187862	759753.980711	41.210394
3520.037590	759431.065565	41.215399
3519.843562	759110.512446	41.220404
3519.806509	758795.792110	41.225408
3519.928106	758466.425293	41.230413
3519.760815	758149.725778	41.235418
3519.426983	757831.905484	41.240423
3519.416017	757513.870508	41.245428
3519.454078	757201.144716	41.250432
3519.366839	756885.810780	41.255437
3518.989376	756577.669124	41.260442
3519.123841	756266.320570	41.265447
3518.985729	755950.758980	41.270452
3518.824169	755642.346474	41.275456
3518.861376	755348.205708	41.280461
3518.384598	755033.649646	41.285466
3518.388599	754732.085062	41.290471
3518.415867	754427.887910	41.295476
3518.092245	754138.648479	41.300480
3518.213915	753824.832742	41.305485
3517.912748	753535.171851	41.310490
3517.959070	753247.121632	41.315495
3517.627008	752950.777205	41.320500
3517.542688	752670.826048	41.325504
3517.403932	752373.538521	41.330509
3517.342934	752097.069229	41.335514
3516.779942	751813.017279	41.340519
3517.155331	751521.538969	41.345524
3516.832135	751247.651056	41.350528
3517.005315	750968.978696	41.355533
3516.763072	750680.732170	41.360538
3516.351433	750409.397936	41.365543
3516.445025	750142.367518	41.370548
3516.231169	749869.499626	41.375552
3516.559710	749594.852709	41.380557
3516.067315	749330.410871	41.385562
3516.294149	749070.584457	41.390567
3516.312779	748800.358078	41.395572
3515.812497	748538.410542	41.400576
3515.755216	748267.733491	41.405581
3515.685148	748019.039219	41.410586
3515.096893	747753.719535	41.415591
3515.651285	747493.391014	41.420596
3515.415737	747243.612128	41.425600
3515.297282	746983.427204	41.430605
3515.058555	746742.380563	41.435610
3514.704107	746479.005279	41.440615
3514.991502	746228.860403	41.445620
3514.512580	745995.887059	41.450624
3514.517443	745742.609897	41.455629
3514.505294	745513.153462	41.460634
3514.646635	745266.412766	41.465639
3514.332063	745027.105426	41.470644
3513.923483	744783.455929	41.475648
3514.538023	744550.061171	41.480653
3513.844763	744321.868951	41.485658
3514.042120	744079.630104	41.490663
3513.911960	743849.254601	41.495668
3513.448614	743618.136312	41.500672
3513.507652	743391.721081	41.505677
3513.729412	743158.498288	41.510682
3513.438516	742942.363386	41.515687
3513.286786	742712.057077	41.520692
3513.233667	742497.057461	41.525696
3513.252212	742270.023305	41.530701
3512.998665	742057.319628	41.535706
3512.760749	741840.502897	41.540711
3513.155106	741613.882336	41.545716
3512.881639	741403.637168	41.550720
3512.695287	741193.174182	41.555725
3512.925185	740983.823858	41.560730
3512.526508	740769.873039	41.565735
3512.685245	740554.835076	41.570740
3512.267337	740351.757949	41.575744
3512.274550	740140.591988	41.580749
3512.089691	739939.939077	41.585754
3511.897455	739741.656771	41.590759
3512.070788	739532.228024	41.595764
3511.876076	739339.328222	41.600768
3511.820878	739148.033247	41.605773
3511.899380	738949.538030	41.610778
3511.840993	738754.919456	41.615783
3511.729097	738565.054585	41.620788
3511.695779	738365.722217	41.625792
3512.009421	738166.475964	41.630797
3511.666154	737983.067552	41.635802
3511.356393	737789.011198	41.640807
3511.580216	737587.885101	41.645812
3511.076201	737402.758069	41.650816
3511.025890	737218.739375	41.655821
3510.755476	737040.740456	41.660826
3510.637370	736860.287604	41.665831
3510.931709	736670.063099	41.670836
3510.532507	736506.177319	41.675840
3510.783190	736325.997894	41.680845
3510.370461	736150.972037	41.685850
3510.141385	735976.555393	41.690855
3510.321609	735810.827442	41.695860
3510.064184	735643.485618	41.700864
3510.127634	735464.208643	41.705869
3510.136688	735294.291289	41.710874
3510.275670	735134.297649	41.715879
3510.138820	734970.832089	41.720884
3509.762381	734808.343264	41.725888
3510.310463	734638.421964	41.730893
3509.900599	734471.130399	41.735898
3509.450849	734317.306340	41.740903
3509.569849	734156.603528	41.745908
3509.403208	733991.637914	41.750912
3509.519837	733843.008061	41.755917
3509.598448	733681.856913	41.760922
3508.914078	733529.640743	41.765927
3509.134089	733376.034569	41.770932
3508.986662	733236.100916	41.775936
3508.841749	733084.529817	41.780941
3509.010064	732936.518334	41.785946
3508.783913	732796.491048	41.790951
3508.853122	732647.302384	41.795956
3508.226091	732508.673166	41.800960
3508.400935	732356.639467	41.805965
3508.517828	732235.657940	41.810970
3508.550714	732081.166813	41.815975
3508.836050	731949.259834	41.820980
3508.391933	731817.570282	41.825984
3508.425183	731677.530266	41.830989
3508.098100	731541.706923	41.835994
3508.147907	731404.630559	41.840999
3508.444071	731264.143799	41.846004
3508.460973	731138.111347	41.851008
3508.379945	730999.663172	41.856013
3508.006933	730865.916006	41.861018
3507.938785	730737.960011	41.866023
3507.989392	730604.237575	41.871028
3508.037701	730472.692416	41.876032
3507.902925	730347.514676	41.881037
3508.053927	730212.035794	41.886042
3507.600733	730098.347456	41.891047
3508.136640	729965.772500	41.896052
3507.594061	729846.944497	41.901056
3507.417182	729721.962195	41.906061
3507.439780	729597.737495	41.911066
3507.262295	729482.806261	41.916071
3507.620218	729359.958919	41.921076
3507.589978	729243.712154	41.926080
3507.377821	729121.302146	41.931085
3507.512271	729002.746202	41.936090
3507.323932	728874.582618	41.941095
3507.102292	728765.889933	41.946100
3506.891201	728649.367364	41.951104
3507.105507	728538.320949	41.956109
3506.756721	728431.477676	41.961114
3506.623294	728317.959319	41.966119
3507.211972	728206.202528	41.971124
3506.716122	728097.793949	41.976128
3506.605352	727986.149732	41.981133
3506.470009	727886.298740	41.986138
3506.323333	727783.723629	41.991143
3506.260459	727682.025137	41.996148
3506.379662	727591.789151	42.001152
3506.958787	727491.567561	42.006157
3506.551055	727378.477826	42.011162
3506.486466	727279.053621	42.016167
3506.755150	727175.956352	42.021172
3506.355847	727076.188633	42.026176
3506.270736	726966.111711	42.031181
3506.549643	726875.246883	42.036186
3506.439268	726775.725039	42.041191
3506.328920	726669.314807	42.046196
3505.965734	726578.750989	42.051200
3506.187084	726474.314905	42.056205
3505.828748	726387.167065	42.061210
3505.949865	726293.051577	42.066215
3506.050813	726212.862130	42.071220
3505.458748	726117.177751	42.076224
3505.887243	726031.878167	42.081229
3505.940721	725936.530972	42.086234
3505.730109	725849.947643	42.091239
3505.756462	725752.323354	42.096244
3505.726253	725663.428781	42.101248
3505.910605	725581.782322	42.106253
3505.707639	725496.333757	42.111258
3505.538605	725406.765577	42.116263
3505.894706	725317.654762	42.121268
3505.711943	725233.885041	42.126272
3505.642454	725126.556040	42.131277
3505.518697	725050.902106	42.136282
3505.571836	724969.766834	42.141287
3505.576320	724880.164246	42.146292
3505.411453	724797.328740	42.151296
3505.321989	724723.202467	42.156301
3505.231590	724640.055714	42.161306
3504.863393	724563.942095	42.166311
3505.252557	724485.720170	42.171316
3505.039183	724410.174280	42.176320
3505.658756	724331.169390	42.181325
3505.395517	724255.184261	42.186330
3505.361432	724162.705613	42.191335
3505.170860	724086.855613	42.196340
3505.090007	724012.077193	42.201344
3504.928230	723933.693258	42.206349
3505.175628	723865.451345	42.211354
3504.725774	723796.630175	42.216359
3504.860998	723710.165447	42.221364
3504.783872	723651.591167	42.226368
3504.790152	723571.986436	42.231373
3505.112559	723500.655979	42.236378
3505.011699	723427.164311	42.241383
3505.049859	723345.569428	42.246388
3504.838460	723277.795022	42.251392
3504.974267	723195.339856	42.256397
3504.739920	723146.354777	42.261402
3504.862885	723069.006105	42.266407
3505.132517	722989.253103	42.271412
3505.098090	722925.015614	42.276416
3504.564898	722837.660804	42.281421
3504.471589	722773.927581	42.286426
3504.535724	722707.441397	42.291431
3504.869781	722644.875857	42.296436
3504.657966	722584.581244	42.301440
3504.755169	722509.412794	42.306445
3504.811759	722439.356443	42.311450
3504.552844	722386.504191	42.316455
3504.581108	722311.097464	42.321460
3504.250168	722255.182670	42.326464
3504.457896	722166.161520	42.331469
3504.389141	722113.821429	42.336474
3504.312415	722046.163404	42.341479
3504.215754	721980.986934	42.346484
3503.967874	721930.658335	42.351488
3504.237199	721865.717938	42.356493
3504.161539	721800.685311	42.361498
3503.754555	721752.365013	42.366503
3504.176973	721693.545590	42.371508
3504.067592	721638.184954	42.376512
3504.089366	721579.133458	42.381517
3503.728941	721525.499229	42.386522
3503.489122	721480.570669	42.391527
3504.021589	721425.251285	42.396532
3503.645641	721370.676608	42.401536
3503.689452	721315.090182	42.406541
3503.625525	721269.784353	42.411546
3503.622081	721223.179182	42.416551
3504.046286	721161.975826	42.421556
3503.569712	721120.604700	42.426560
3503.619836	721054.801722	42.431565
3503.787264	721018.033928	42.436570
3503.736909	720963.254022	42.441575
3503.835227	720906.614628	42.446580
3503.780847	720864.131220	42.451584
3504.078846	720808.251485	42.456589
3503.987200	720758.633708	42.461594
3503.427190	720707.357598	42.466599
3503.480733	720650.723861	42.471604
3503.786313	720609.121766	42.476608
3503.664884	720549.838697	42.481613
3503.488931	720505.985175	42.486618
3503.163220	720462.701608	42.491623
3503.358497	720414.720264	42.496628
3503.040035	720379.368753	42.501632
3503.742179	720320.691743	42.506637
3503.725481	720274.926413	42.511642
3503.347653	720235.270081	42.516647
3503.625155	720185.984580	42.521652
3503.117892	720136.977231	42.526656
3503.211384	720095.804319	42.531661
3503.149458	720062.144628	42.536666
3503.154607	720010.671650	42.541671
3503.237660	719972.921426	42.546676
3503.077991	719946.467706	42.551680
3503.475595	719903.061699	42.556685
3503.462911	719860.020799	42.561690
3503.464540	719813.555661	42.566695
3503.257101	719764.248626	42.571700
3503.116763	719734.270186	42.576704
3503.298913	719680.088078	42.581709
3503.189013	719641.822750	42.586714
3503.079760	719614.318251	42.591719
3502.983840	719559.437455	42.596724
3503.028384	719531.113815	42.601728
3502.916806	719485.607782	42.606733
3502.873929	719452.438392	42.611738
3502.685383	719409.077087	42.616743
3503.066832	719372.861766	42.621748
3502.858632	719340.363943	42.626752
3503.038902	719314.794290	42.631757
3502.791026	719271.640442	42.636762
3503.008959	719236.294621	42.641767
3503.159745	719190.495661	42.646772
3502.963067	719165.979700	42.651776
3502.816739	719132.032644	42.656781
3503.013436	719089.399506	42.661786
3502.810752	719061.263907	42.666791
3502.979058	719030.339248	42.671796
3502.838671	719000.110208	42.676800
3502.910884	718965.084884	42.681805
3503.042911	718930.099124	42.686810
3502.963039	718881.559299	42.691815
3502.888715	718845.813770	42.696820
3502.755617	718822.476571	42.701824
3502.642745	718784.802945	42.706829
3503.020748	718744.022705	42.711834
3502.717093	718723.093997	42.716839
3502.886154	718684.827778	42.721844
3502.956974	718649.305403	42.726848
3502.824998	718610.245456	42.731853
3502.907576	718581.366751	42.736858
3502.643682	718552.049235	42.741863
3502.923093	718513.565611	42.746868
3502.698251	718482.803089	42.751872
3502.670617	718443.824316	42.756877
3502.678819	718424.579229	42.761882
3502.884364	718384.520101	42.766887
3502.939858	718360.803263	42.771892
3502.560711	718331.305627	42.776896
3502.575939	718293.261430	42.781901
3502.678223	718270.726962	42.786906
3502.689795	718239.527690	42.791911
3502.865209	718204.680522	42.796916
3502.391914	718184.770470	42.801921
3502.444628	718146.025026	42.806925
3502.761914	718110.162039	42.811930
3502.629382	718093.469009	42.816935
3502.777070	718059.865805	42.821940
3502.638889	718027.599299	42.826945
3502.549289	717984.015845	42.831949
3502.745561	717972.029838	42.836954
3502.669950	717940.843860	42.841959
3502.666350	717909.149861	42.846964
3502.332169	717880.337608	42.851969
3502.834438	717846.625352	42.856973
3502.651640	717824.235995	42.861978
3502.424106	717796.249044	42.866983
3502.619953	717761.099048	42.871988
3502.703934	717737.921354	42.876993
3502.657045	717699.091099	42.881997
3502.282571	717669.689558	42.887002
3502.191539	717646.540532	42.892007
3502.579682	717625.941171	42.897012
3502.498509	717599.268633	42.902017
3502.323382	717564.278320	42.907021
3502.766665	717534.493156	42.912026
3502.888944	717506.447430	42.917031
3502.600784	717475.741270	42.922036
3502.556548	717463.546266	42.927041
3502.544881	717429.074010	42.932045
3502.526969	717400.803081	42.937050
3502.270016	717375.646983	42.942055
3502.776020	717343.122577	42.947060
3502.397120	717325.972690	42.952065
3502.868020	717286.955753	42.957069
3502.431523	717249.775132	42.962074
3502.253792	717231.450908	42.967079
3502.627639	717212.291426	42.972084
3502.492382	717180.814848	42.977089
3502.590769	717159.617366	42.982093
3502.554614	717125.395934	42.987098
3502.299756	717107.828261	42.992103
3502.081253	717069.420291	42.997108
3502.398654	717052.948466	43.002113
3502.662915	717029.590207	43.007117
3502.465388	716994.948459	43.012122
3502.168335	716968.259982	43.017127
3502.639218	716951.117717	43.022132
3502.190785	716929.414743	43.027137
3502.257216	716897.606135	43.032141
3502.294895	716867.290357	43.037146
3502.076494	716850.906680	43.042151
3502.322564	716828.691823	43.047156
3502.393944	716820.693360	43.052161
3502.265115	716780.781042	43.057165
3502.164792	716761.599677	43.062170
3501.927076	716737.629058	43.067175
3502.237326	716706.225901	43.072180
3502.048612	716702.586164	43.077185
3501.872537	716677.513820	43.082189
3502.514945	716656.820462	43.087194
3502.205371	716634.101618	43.092199
3502.318953	716609.774933	43.097204
3502.365484	716602.574099	43.102209
3502.295253	716573.019214	43.107213
3502.333645	716560.213942	43.112218
3502.132398	716519.469006	43.117223
3502.158271	716508.997332	43.122228
3501.941814	716500.103564	43.127233
3501.966694	716465.373267	43.132237
3502.188016	716452.934474	43.137242
3502.009884	716433.914046	43.142247
3502.037939	716407.418105	43.147252
3501.884125	716398.513877	43.152257
3502.188722	716381.546762	43.157261
3502.155128	716361.708533	43.162266
3502.113456	716337.803595	43.167271
3502.257581	716305.682249	43.172276
3501.875444	716300.288342	43.177281
3502.258612	716274.179788	43.182285
3502.169222	716255.392341	43.187290
3502.040157	716236.710630	43.192295
3502.188644	716223.092886	43.197300
3502.082090	716209.765319	43.202305
3502.200412	716181.517381	43.207309
3502.232155	716154.325484	43.212314
3502.244419	716137.406187	43.217319
3502.175479	716098.721004	43.222324
3502.007988	716094.234105	43.227329
3501.965384	716085.112721	43.232333
3501.855600	716047.327054	43.237338
3501.995843	716040.655979	43.242343
3502.317583	716028.696082	43.247348
3502.012259	716000.517545	43.252353
3501.822346	715991.519627	43.257357
3501.620085	715965.358024	43.262362
3502.088880	715948.114844	43.267367
3502.600220	715918.263103	43.272372
3501.966150	715910.082678	43.277377
3502.076659	715888.780765	43.282381
3502.217209	715874.469196	43.287386
3501.830538	715847.246225	43.292391
3501.856671	715822.683652	43.297396
3502.039164	715826.027203	43.302401
3502.213089	715806.153371	43.307405
3502.113426	715799.670589	43.312410
3501.821802	715781.064341	43.317415
3501.775278	715757.009714	43.322420
3501.875397	715750.146588	43.327425
3501.801050	715738.896706	43.332429
3501.962979	715713.716016	43.337434
3501.870915	715704.850460	43.342439
3501.941989	715684.596430	43.347444
3501.877863	715676.123137	43.352449
3501.974065	715643.560662	43.357453
3502.042850	715645.037749	43.362458
3501.796474	715623.099546	43.367463
3502.317145	715589.871352	43.372468
3502.191745	715589.445586	43.377473
3501.894138	715554.467136	43.382477
3502.176578	715544.001478	43.387482
3502.065031	715527.151029	43.392487
3502.315655	715498.035489	43.397492
3501.728155	715497.239549	43.402497
3501.674623	715476.955997	43.407501
3502.074917	715442.506745	43.412506
3502.121879	715437.587134	43.417511
3502.244416	715416.976652	43.422516
3501.948912	715390.878285	43.427521
3502.209102	715389.991867	43.432525
3502.304555	715356.932255	43.437530
3501.973624	715340.812304	43.442535
3502.171415	715319.345681	43.447540
3502.243495	715298.544784	43.452545
3502.025247	715284.539586	43.457549
3502.267691	715255.424561	43.462554
3501.884427	715245.217391	43.467559
3502.293513	715223.864457	43.472564
3502.085442	715202.266141	43.477569
3502.252806	715181.895758	43.482573
3502.096674	715152.697395	43.487578
3501.942323	715138.085992	43.492583
3501.986496	715134.456703	43.497588
3502.309671	715108.255223	43.502593
3501.969235	715089.903596	43.507597
3501.957988	715064.253414	43.512602
3501.797535	715053.016844	43.517607
3502.398382	715037.238506	43.522612
3501.884343	715019.064264	43.527617
3502.009815	715003.463654	43.532621
3501.906033	714990.828344	43.537626
3501.857603	714977.489219	43.542631
3501.958235	714957.129321	43.547636
3502.047608	714939.152900	43.552641
3501.846141	714921.571828	43.557645
3501.710158	714902.937916	43.562650
3501.732682	714893.953334	43.567655
3501.912979	714889.209843	43.572660
3501.846764	714864.659739	43.577665
3501.968965	714845.536469	43.582669
3502.021375	714845.081281	43.587674
3501.829292	714828.937402	43.592679
3502.038122	714799.875981	43.597684
3502.050535	714800.667869	43.602689
3501.871126	714763.036802	43.607693
3501.979480	714745.652260	43.612698
3501.726090	714746.736173	43.617703
3501.926708	714722.290418	43.622708
3501.750341	714712.991176	43.627713
3501.569733	714703.593385	43.632717
3501.760061	714687.237183	43.637722
3501.637487	714676.986242	43.642727
3502.012901	714647.946389	43.647732
3501.613279	714642.306199	43.652737
3501.542369	714641.176702	43.657741
3502.119003	714627.187913	43.662746
3501.617310	714601.071552	43.667751
3501.942171	714592.532887	43.672756
3501.438173	714586.215227	43.677761
3501.886765	714573.488010	43.682765
3502.169278	714545.951763	43.687770
3502.096169	714542.937045	43.692775
3502.157248	714521.193264	43.697780
3501.756464	714501.659436	43.702785
3502.043032	714498.634885	43.707789
3502.024602	714457.452791	43.712794
3501.851912	714448.450374	43.717799
3502.406421	714434.067956	43.722804
3502.047937	714417.950788	43.727809
3502.167189	714387.314878	43.732813
3501.707078	714388.532239	43.737818
3501.727440	714366.844411	43.742823
3501.724183	714344.416108	43.747828
3501.872555	714348.907182	43.752833
3501.563204	714330.747248	43.757837
3502.082950	714311.308966	43.762842
3501.784948	714300.739205	43.767847
3501.937373	714300.068973	43.772852
3501.664906	714271.680732	43.777857
3501.609953	714253.875568	43.782861
3501.972018	714249.300170	43.787866
3501.736285	714251.026314	43.792871
3501.947550	714226.428500	43.797876
3501.902514	714215.122118	43.802881
3501.738066	714205.373745	43.807885
3501.845414	714174.838276	43.812890
3501.783324	714159.366348	43.817895
3501.939805	714151.897140	43.822900
3501.817326	714149.982137	43.827905
3501.767819	714116.098037	43.832909
3502.051508	714108.955129	43.837914
3501.728915	714104.989024	43.842919
3501.837325	714070.235056	43.847924
3501.710647	714064.896733	43.852929
3501.568114	714047.055983	43.857933
3501.765266	714046.775326	43.862938
3501.691563	714046.291312	43.867943
3501.651814	714010.668364	43.872948
3501.678490	714007.785834	43.877953
3501.167484	713991.544184	43.882957
3501.917438	713995.737540	43.887962
3501.512651	713985.532394	43.892967
3501.967775	713953.449948	43.897972
3501.876330	713947.559867	43.902977
3501.736657	713940.387531	43.907981
3501.957438	713935.289451	43.912986
3501.452243	713916.763998	43.917991
3502.042569	713909.421378	43.922996
3501.641039	713907.651681	43.928001
3501.740212	713882.327031	43.933005
3501.796275	713862.964347	43.938010
3501.735942	713861.138257	43.943015
3501.765491	713845.749860	43.948020
3501.383031	713831.719757	43.953025
3501.429740	713814.790109	43.958029
3501.623780	713807.810637	43.963034
3501.552852	713804.100549	43.968039
3501.924295	713800.317356	43.973044
3501.533561	713791.648017	43.978049
3501.661664	713761.951249	43.983053
3501.894049	713754.270647	43.988058
3501.741461	713749.383031	43.993063
3501.533048	713737.110508	43.998068
3501.638450	713718.979968	44.003073
3501.456707	713714.891151	44.008077
3501.387430	713703.786592	44.013082
3501.494208	713704.116362	44.018087
3501.670096	713692.028393	44.023092
3501.333400	713706.822776	44.028097
3501.489239	713670.322444	44.033101
3501.683251	713654.906523	44.038106
3501.740457	713653.706096	44.043111
3501.659594	713640.916100	44.048116
3501.725369	713638.473614	44.053121
3501.658684	713610.396523	44.058125
3501.530243	713610.665916	44.063130
3501.690150	713605.180691	44.068135
3501.868508	713589.022849	44.073140
3501.752861	713579.364941	44.078145
3501.849404	713559.002353	44.083149
3501.542648	713551.261784	44.088154
3501.556544	713548.827846	44.093159
3501.889903	713538.500177	44.098164
3501.433215	713522.794535	44.103169
3501.396242	713506.771373	44.108173
3501.585682	713504.804677	44.113178
3501.670391	713505.634367	44.118183
3501.747818	713493.363880	44.123188
3501.618356	713469.415692	44.128193
3501.517034	713459.904159	44.133197
3501.611855	713457.804208	44.138202
3501.338962	713449.958697	44.143207
3501.720746	713454.312423	44.148212
3501.581509	713440.936250	44.153217
3501.466035	713430.037472	44.158221
3501.663866	713422.858551	44.163226
3501.778477	713411.971354	44.168231
3502.053706	713404.928508	44.173236
3501.770821	713396.240939	44.178241
3501.612060	713364.505846	44.183245
3502.085032	713366.363187	44.188250
3501.793995	713354.699288	44.193255
3501.816666	713322.338528	44.198260
3501.891351	713317.810123	44.203265
3501.553948	713308.238177	44.208269
3501.692576	713293.575165	44.213274
3501.395507	713283.549877	44.218279
3501.529175	713265.314440	44.223284
3501.539879	713265.759360	44.228289
3501.604578	713265.599824	44.233293
3501.542504	713261.193245	44.238298
3501.925622	713239.392953	44.243303
3502.014360	713218.137533	44.248308
3501.845360	713217.569962	44.253313
3501.544496	713195.684075	44.258317
3501.737942	713170.689115	44.263322
3501.142503	713172.474916	44.268327
3501.586699	713163.468442	44.273332
3501.408050	713158.932188	44.278337
3501.678369	713164.545196	44.283341
3501.730470	713142.054930	44.288346
3501.768742	713133.016246	44.293351
3501.613580	713122.570288	44.298356
3501.684760	713130.201373	44.303361
3501.497571	713112.514915	44.308365
3501.835965	713086.403923	44.313370
3501.524291	713087.745817	44.318375
3501.914026	713071.899462	44.323380
3501.417580	713069.797866	44.328385
3501.271156	713058.506692	44.333389
3501.895071	713031.901688	44.338394
3501.444364	713023.439984	44.343399
3501.632311	713018.843074	44.348404
3501.576728	713018.951557	44.353409
3501.545830	713020.792984	44.358413
3501.539824	712991.115676	44.363418
3501.496516	712975.886627	44.368423
3501.408433	712969.796790	44.373428
3501.541403	712965.010418	44.378433
3501.276686	712961.083836	44.383437
3501.719324	712958.678137	44.388442
3501.276943	712956.517948	44.393447
3501.497156	712941.840845	44.398452
3501.576526	712930.214409	44.403457
3501.606426	712926.685792	44.408461
3501.578758	712917.111848	44.413466
3501.340527	712925.886104	44.418471
3501.819208	712915.831445	44.423476
3501.536661	712894.239529	44.428481
3501.594706	712882.963962	44.433485
3501.582400	712870.657773	44.438490
3501.686342	712886.373370	44.443495
3501.717820	712867.409514	44.448500
3501.666519	712852.876387	44.453505
3501.502888	712841.240355	44.458509
3501.943144	712830.050448	44.463514
3501.242244	712829.868530	44.468519
3501.662064	712822.900570	44.473524
3501.684730	712810.439623	44.478529
3501.301248	712794.373113	44.483533
3501.864781	712787.182853	44.488538
3501.673838	712774.856415	44.493543
3501.701156	712762.196106	44.498548
3501.298960	712750.351218	44.503553
3501.849320	712732.790240	44.508557
3501.929181	712727.268047	44.513562
3501.494839	712737.712727	44.518567
3501.963417	712709.047885	44.523572
3501.629694	712697.489395	44.528577
3501.287220	712689.406518	44.533581
3501.481283	712676.520002	44.538586
3501.474949	712681.583474	44.543591
3501.728860	712671.615302	44.548596
3501.669441	712654.055667	44.553601
3501.599412	712653.223545	44.558605
3501.734633	712643.721636	44.563610
3501.558843	712652.138436	44.568615
3501.646464	712622.791787	44.573620
3501.649631	712602.045280	44.578625
3501.546507	712599.828933	44.583629
3501.674231	712595.489906	44.588634
3501.502022	712592.937553	44.593639
3501.496694	712583.756594	44.598644
3501.409928	712551.212447	44.603649
3501.603729	712545.572043	44.608653
3501.478550	712538.942074	44.613658
3501.412845	712536.123943	44.618663
3501.791450	712540.726831	44.623668
3501.858747	712519.671733	44.628673
3501.307215	712501.895312	44.633677
3501.542342	712497.885912	44.638682
3501.427308	712497.408638	44.643687
3501.454546	712492.043885	44.648692
3501.369472	712494.440334	44.653697
3501.262815	712491.380794	44.658701
3501.306067	712483.928831	44.663706
3501.605381	712471.372037	44.668711
3501.806156	712447.664182	44.673716
3501.414503	712448.870492	44.678721
3501.323093	712449.779024	44.683725
3501.810632	712441.955809	44.688730
3501.738563	712433.778370	44.693735
3501.603970	712407.495290	44.698740
3501.620351	712409.775732	44.703745
3501.321075	712403.422591	44.708749
3501.632977	712395.926156	44.713754
3501.361956	712392.744843	44.718759
3501.607660	712385.755668	44.723764
3501.677774	712362.714396	44.728769
3501.661595	712352.691218	44.733773
3501.934229	712351.206842	44.738778
3501.338754	712345.547836	44.743783
3501.370772	712316.308582	44.748788
3501.407168	712311.091102	44.753793
3501.307246	712307.285881	44.758797
3501.514028	712296.977625	44.763802
3501.464252	712301.006200	44.768807
3501.825487	712298.663405	44.773812
3501.984331	712299.679498	44.778817
3501.651625	712270.599625	44.783821
3501.929395	712253.181973	44.788826
3501.784538	712247.994406	44.793831
3502.009446	712229.791302	44.798836
3501.960856	712214.412857	44.803841
3501.687510	712203.340053	44.808845
3501.682422	712190.535344	44.813850
3501.665298	712173.464066	44.818855
3501.910496	712165.283573	44.823860
3501.866118	712150.698464	44.828865
3501.839722	712143.108809	44.833869
3501.665035	712113.654844	44.838874
3501.638944	712111.475274	44.843879
3501.795855	712110.853769	44.848884
3501.679592	712091.366614	44.853889
3501.570181	712078.132264	44.858893
3501.655442	712066.056959	44.863898
3501.482034	712076.409692	44.868903
3501.375126	712063.621618	44.873908
3501.634306	712065.564220	44.878913
3501.184076	712042.359894	44.883917
3501.495295	712022.851574	44.888922
3501.422660	712025.643180	44.893927
3501.458055	712014.767284	44.898932
3501.456639	712010.747111	44.903937
3501.271884	712013.507614	44.908941
3501.311055	712005.063203	44.913946
3501.046703	712014.934687	44.918951
3501.590088	712004.024466	44.923956
3501.395067	711990.704857	44.928961
3501.258285	711972.958055	44.933965
3501.577379	711968.587085	44.938970
3501.387046	711964.796650	44.943975
3501.357089	711959.341742	44.948980
3501.373620	711957.155089	44.953985
3501.402602	711964.148936	44.958989
3501.561802	711957.124069	44.963994
3501.674375	711938.889271	44.968999
3501.759353	711910.285131	44.974004
3501.422392	711913.418269	44.979009
3501.484403	711915.046038	44.984013
3501.665386	711913.824913	44.989018
3501.552572	711906.398234	44.994023
3501.163188	711884.275406	44.999028
3501.359538	711885.533530	45.004033
3501.285751	711887.134111	45.009037
3501.407163	711877.683265	45.014042
3501.151955	711885.766495	45.019047
3501.155702	711878.816888	45.024052
3501.406346	711875.102449	45.029057
3501.261578	711873.041701	45.034061
3501.377214	711873.320447	45.039066
3501.151391	711873.407440	45.044071
3501.640912	711874.319303	45.049076
3501.389951	711855.747314	45.054081
3501.435258	711843.876840	45.059085
3501.625578	711833.074382	45.064090
3501.378386	711836.837983	45.069095
3501.284076	711830.400904	45.074100
3501.300119	711829.604112	45.079105
3501.308132	711840.324241	45.084109
3501.400506	711831.821230	45.089114
3501.393572	711836.488216	45.094119
3501.562976	711809.110688	45.099124
3501.403639	711788.686866	45.104129
3501.581392	711794.316084	45.109133
3501.706778	711775.582454	45.114138
3501.359863	711783.035661	45.119143
3501.348592	711778.619914	45.124148
3501.422258	711765.851188	45.129153
3500.991173	711747.556910	45.134157
3501.506027	711729.652279	45.139162
3501.603374	711738.074482	45.144167
3501.481366	711720.771442	45.149172
3501.158872	711739.488206	45.154177
3501.191754	711738.291530	45.159181
3501.503412	711726.922882	45.164186
3501.387680	711737.613953	45.169191
3501.518388	711715.057280	45.174196
3501.264006	711701.995211	45.179201
3500.977999	711689.236170	45.184205
3501.537097	711687.456157	45.189210
3501.166967	711685.730427	45.194215
3501.275871	711675.338321	45.199220
3501.549851	711683.880299	45.204225
3500.998232	711674.391537	45.209229
3501.320740	711675.281386	45.214234
3501.258604	711689.884990	45.219239
3501.562307	711677.524851	45.224244
3501.468626	711687.418147	45.229249
3501.277388	711665.758375	45.234253
3501.330334	711638.399543	45.239258
3501.245135	711632.506818	45.244263
3501.341701	711633.632558	45.249268
3501.412421	711637.393349	45.254273
3501.225247	711635.339550	45.259277
3501.428880	711629.150906	45.264282
3501.116250	711623.792132	45.269287
3501.578778	711624.509936	45.274292
3501.705458	711624.687590	45.279297
3501.628010	711609.660281	45.284301
3501.779761	711591.418264	45.289306
3501.015379	711600.677932	45.294311
3501.087505	711594.808820	45.299316
3501.222575	711598.906456	45.304321
3501.519988	711591.510986	45.309325
3501.480097	711581.540454	45.314330
3501.151133	711591.472742	45.319335
3501.382736	711583.343576	45.324340
3501.357486	711585.432568	45.329345
3501.224568	711552.048380	45.334349
3501.521704	711549.964165	45.339354
3501.661595	711549.692898	45.344359
3501.381695	711536.485877	45.349364
3501.447370	711543.325093	45.354369
3501.452337	711544.962361	45.359373
3501.522815	711535.718104	45.364378
3501.100758	711524.619349	45.369383
3501.298501	711502.894882	45.374388
3501.485244	711501.424556	45.379393
3501.416810	711506.002610	45.384397
3501.567162	711491.185638	45.389402
3501.548772	711500.818518	45.394407
3501.382239	711497.818150	45.399412
3501.146688	711494.382444	45.404417
3501.207727	711487.373412	45.409421
3501.069117	711494.246426	45.414426
3501.032220	711497.677595	45.419431
3501.385824	711500.696765	45.424436
3501.327026	711470.129379	45.429441
3500.765169	711462.131218	45.434445
3501.242836	711456.542463	45.439450
3501.260686	711455.943891	45.444455
3501.025298	711456.826681	45.449460
3501.181362	711451.291068	45.454465
3500.945285	711455.499745	45.459469
3501.186677	711450.148584	45.464474
3501.234963	711452.026903	45.469479
3501.013545	711445.114152	45.474484
3500.958150	711443.634191	45.479489
3500.749243	711447.441275	45.484493
3501.210155	711453.867780	45.489498
3500.889660	711471.840225	45.494503
3501.151852	711473.782468	45.499508
3501.200946	711486.829253	45.504513
3501.132787	711474.033888	45.509517
3501.216266	711462.702596	45.514522
3501.021812	711449.828788	45.519527
3501.157359	711455.812675	45.524532
3501.420540	711447.777438	45.529537
3501.245055	711450.189121	45.534541
3501.380350	711448.727288	45.539546
3501.200438	711452.628854	45.544551
3501.596881	711451.074228	45.549556
3501.281528	711442.340375	45.554561
3500.946785	711449.940775	45.559565
3501.291812	711450.628374	45.564570
3501.284054	711458.174732	45.569575
3501.287211	711452.118365	45.574580
3501.414011	711462.223680	45.579585
3501.001060	711451.024046	45.584589
3501.170820	711450.499648	45.589594
3501.178777	711453.476677	45.594599
3501.338136	711445.557871	45.599604
3501.575296	711424.769822	45.604609
3501.391751	711409.064751	45.609613
3501.290851	711407.393749	45.614618
3501.240546	711411.571749	45.619623
3501.159970	711406.174489	45.624628
3501.079313	711414.924260	45.629633
3500.665004	711415.240957	45.634637
3501.086533	711409.264339	45.639642
3501.456404	711410.791693	45.644647
3501.138168	711406.426480	45.649652
3501.410870	711414.621471	45.654657
3501.434064	711413.426350	45.659661
3501.651306	711406.838187	45.664666
3501.309523	711393.144782	45.669671
3501.327942	711372.442391	45.674676
3501.786115	711366.062576	45.679681
3501.485399	711361.893001	45.684685
3501.560987	711360.887770	45.689690
3501.145539	711364.232632	45.694695
3501.452797	711365.075397	45.699700
3501.433141	711357.384648	45.704705
3500.972645	711350.064576	45.709709
3501.212467	711326.545702	45.714714
3500.968903	711332.641964	45.719719
3501.323426	711325.137547	45.724724
3501.397797	711320.757050	45.729729
3501.140816	711326.309502	45.734733
3501.299276	711320.078460	45.739738
3501.133178	711324.573472	45.744743
3501.472436	711319.652810	45.749748
3501.543979	711329.668135	45.754753
3501.043219	711321.064075	45.759757
3501.339944	711310.144093	45.764762
3501.362359	711329.698265	45.769767
3501.229513	711313.488248	45.774772
3501.698439	711310.382803	45.779777
3501.432963	711290.322798	45.784781
3501.299490	711276.694060	45.789786
3501.362635	711272.365032	45.794791
3501.241913	711268.116026	45.799796
3501.482840	711276.514960	45.804801
3501.278861	711249.048415	45.809805
3501.294502	711193.747181	45.814810
3501.175791	711085.352567	45.819815
3501.060329	710904.529245	45.824820
3500.899179	710675.853980	45.829825
3500.741110	710399.463797	45.834829
3500.960484	710054.391029	45.839834
3500.587641	709660.547865	45.844839
3500.202489	709199.262087	45.849844
3499.868152	708703.383650	45.854849
3499.776076	708133.297855	45.859853
3499.687852	707504.871338	45.864858
3499.096925	706833.273315	45.869863
3498.779032	706099.540852	45.874868
3498.640994	705298.755875	45.879873
3497.973409	704446.566641	45.884877
3497.598763	703540.238624	45.889882
3497.169875	702574.247217	45.894887
3496.547982	701539.700222	45.899892
3496.071250	700453.167751	45.904897
3495.490882	699320.835729	45.909901
3494.823807	698105.646399	45.914906
3493.926808	696837.422947	45.919911
3493.465279	695525.730384	45.924916
3492.792882	694138.327668	45.929921
3492.013841	692690.136232	45.934925
3491.647632	691184.175959	45.939930
3490.606449	689625.176624	45.944935
3489.670418	688008.951251	45.949940
3488.992834	686328.873940	45.954945
3487.770425	684588.379251	45.959949
3487.243796	682778.762965	45.964954
3486.029261	680930.548863	45.969959
3485.192432	679011.903399	45.974964
3484.455638	677036.932819	45.979969
3483.348443	675004.684306	45.984973
3482.176828	672900.216029	45.989978
3480.642970	670760.381162	45.994983
3479.806385	668557.252313	45.999988
3478.875487	666292.964775	46.004993
3477.593805	663974.007733	46.009997
3476.686580	661597.330371	46.015002
3475.209246	659182.071422	46.020007
3474.014002	656694.507478	46.025012
3472.922406	654156.895182	46.030017
3471.549016	651559.571428	46.035021
3470.178259	648906.495434	46.040026
3469.109956	646210.226087	46.045031
3467.359643	643440.294923	46.050036
3465.907597	640614.942039	46.055041
3464.302349	637754.165109	46.060045
3462.922977	634829.953396	46.065050
3461.318741	631860.907119	46.070055
3459.782522	628847.247637	46.075060
3458.269992	625777.581896	46.080065
3456.710309	622652.332377	46.085069
3455.244183	619479.304467	46.090074
3453.358957	616252.985398	46.095079
3451.440826	612974.627674	46.100084
3449.848134	609647.546757	46.105089
3448.256252	606272.415492	46.110093
3446.247856	602849.923044	46.115098
3444.156547	599384.702262	46.120103
3442.601013	595858.393359	46.125108
3440.604302	592295.580239	46.130113
3438.643357	588676.112735	46.135117
3436.857853	585001.487619	46.140122
3434.960257	581289.415391	46.145127
3433.020269	577519.845723	46.150132
3430.724232	573718.502842	46.155137
3428.559922	569868.130035	46.160141
3426.873451	565969.396208	46.165146
3424.572579	562033.331695	46.170151
3422.705476	558034.206010	46.175156
3420.508046	554009.696270	46.180161
3417.918901	549935.562628	46.185165
3415.863589	545816.970115	46.190170
3413.400726	541652.086386	46.195175
3411.531474	537447.585085	46.200180
3409.430995	533188.649868	46.205185
3406.767715	528898.326492	46.210189
3404.587713	524555.530973	46.215194
3402.280481	520182.563927	46.220199
3399.699894	515759.792154	46.225204
3397.313283	511296.771018	46.230209
3394.659438	506800.440886	46.235213
3392.517569	502257.420604	46.240218
3390.014800	497677.753636	46.245223
3387.581904	493058.732718	46.250228
3384.663273	488396.040484	46.255233
3382.094976	483708.107282	46.260237
3379.725990	478963.825361	46.265242
3377.055190	474196.231596	46.270247
3373.982676	469381.694581	46.275252
3371.375784	464538.812328	46.280257
3368.472042	459661.586045	46.285261
3365.903554	454741.347896	46.290266
3362.957344	449801.388784	46.295271
3360.318407	444828.069874	46.300276
3357.471556	439805.706897	46.305281
3354.427049	434763.068061	46.310285
3351.821809	429681.744804	46.315290
3348.436659	424583.014032	46.320295
3345.612808	419436.820464	46.325300
3342.663060	414269.589489	46.330305
3339.575098	409079.821234	46.335309
3336.566547	403848.348050	46.340314
3333.366070	398607.062103	46.345319
3330.117473	393321.359422	46.350324
3327.534523	388013.018360	46.355329
3324.441739	382684.419630	46.360333
3321.038037	377320.176122	46.365338
3317.902994	371934.580234	46.370343
3314.867163	366523.975863	46.375348
3311.622730	361091.977689	46.380353
3308.360738	355636.829492	46.385357
3305.033212	350151.827884	46.390362
3301.692240	344647.222624	46.395367
3298.478745	339133.687249	46.400372
3295.151758	333576.101459	46.405377
3291.707633	328005.878032	46.410381
3288.385526	322402.295312	46.415386
3284.811860	316800.249902	46.420391
3281.199509	311160.771363	46.425396
3277.982394	305532.174621	46.430401
3274.009822	299889.538489	46.435405
3270.697063	294207.078712	46.440410
3267.110972	288531.411759	46.445415
3263.407974	282829.680239	46.450420
3260.029268	277121.488809	46.455425
3256.143941	271405.771862	46.460429
3252.354278	265677.279460	46.465434
3248.659795	259937.381453	46.470439
3244.974674	254179.669131	46.475444
3241.255690	248428.823916	46.480449
3237.177667	242675.471959	46.485453
3233.666586	236894.549354	46.490458
3229.361647	231123.561744	46.495463
3225.569409	225355.616324	46.500468
3221.763423	219570.424953	46.505473
3217.572141	213799.060922	46.510477
3213.915556	207969.835091	46.515482
3209.728470	202145.293220	46.520487
3206.158060	196360.320693	46.525492
3201.809527	190577.386711	46.530497
3197.605484	184792.364336	46.535501
3193.537747	179006.740960	46.540506
3189.268866	173235.149633	46.545511
3184.907906	167476.991420	46.550516
3180.959258	161705.297740	46.555521
3176.246488	155958.799788	46.560525
3172.002886	150218.713914	46.565530
3167.715251	144494.017731	46.570535
3163.507568	138770.543677	46.575540
3159.041176	133077.587549	46.580545
3154.549986	127390.730102	46.585549
3150.344651	121710.712025	46.590554
3145.616061	116044.771524	46.595559
3140.640002	110416.483914	46.600564
3136.189792	104781.277428	46.605569
3131.353661	99202.323010	46.610573
3126.351380	93617.281831	46.615578
3121.350263	88080.602517	46.620583
3116.193755	82567.862362	46.625588
3111.459269	77097.691925	46.630593
3105.753282	71655.154854	46.635597
3100.768795	66241.804300	46.640602
3095.021186	60887.666645	46.645607
3088.413395	55593.840936	46.650612
3077.460437	50476.500842	46.655617
3061.108396	45595.349064	46.660621
3046.744284	40859.304542	46.665626
3032.712093	36302.966125	46.670631
3019.282698	31961.540568	46.675636
3006.433190	27831.481248	46.680641
2994.158768	23931.156297	46.685645
2982.274931	20227.852052	46.690650
2971.037931	16770.037471	46.695655
2960.027438	13514.588448	46.700660
2949.544416	10466.240125	46.705665
2939.037044	7623.421629	46.710669
2928.528044	4974.784960	46.715674
2917.232899	2554.930881	46.720679
2896.506907	595.739465	46.725684
2827.605399	269.267021	46.730689
2771.370102	273.155265	46.735693
2749.568609	255.137762	46.740698
2752.991306	250.056768	46.745703
2770.150478	246.320528	46.750708
2789.652486	243.862712	46.755713
2803.849512	261.092296	46.760717
2811.825528	257.215128	46.765722
2813.684888	251.396167	46.770727
2810.953335	234.307701	46.775732
2806.701210	236.361095	46.780737
2801.893827	240.016228	46.785741
2798.308223	250.611804	46.790746
2794.717731	247.889643	46.795751
2792.024640	234.771980	46.800756
2789.705124	230.161895	46.805761
2787.178824	226.511159	46.810765
2784.433845	228.805705	46.815770
2781.354334	243.884317	46.820775
2778.333283	238.772880	46.825780
2775.808170	236.144755	46.830785
2772.739494	229.428168	46.835789
2769.384099	227.351093	46.840794
2766.145767	230.956921	46.845799
2762.939834	237.494566	46.850804
2759.521715	227.167712	46.855809
2755.934771	242.221594	46.860813
2753.088482	229.286009	46.865818
2750.130100	221.945162	46.870823
2746.760148	226.895938	46.875828
2743.518937	227.914370	46.880833
2739.890174	234.117080	46.885837
2736.846458	231.459379	46.890842
2733.570332	224.389788	46.895847
2730.561543	227.132773	46.900852
2726.882738	215.236661	46.905857
2723.202934	228.617897	46.910861
2720.095215	222.486411	46.915866
2716.434068	223.110828	46.920871
2713.147649	216.216028	46.925876
2710.211389	214.295181	46.930881
2706.385842	217.164104	46.935885
2703.253560	218.212685	46.940890
2700.045633	222.986104	46.945895
2696.284889	221.450588	46.950900
2693.184700	212.276515	46.955905
2689.484847	217.016126	46.960909
2686.513001	224.377433	46.965914
2682.959673	221.610347	46.970919
2679.574181	224.140832	46.975924
2676.041775	217.975688	46.980929
2672.314809	216.278903	46.985933
2669.091860	213.996068	46.990938
2665.983432	215.149657	46.995943
2661.261269	218.191318	47.000948
2658.492968	207.410868	47.005953
2655.218255	217.675630	47.010957
2652.155303	204.204328	47.015962
2647.819717	209.531900	47.020967
2644.351527	212.239102	47.025972
2641.382154	198.467762	47.030977
2637.883119	208.090233	47.035981
2635.190850	204.574228	47.040986
2631.875980	201.236087	47.045991
2627.594604	205.129730	47.050996
2624.503514	197.971989	47.056001
2620.588554	211.510025	47.061005
2617.414570	200.339936	47.066010
2613.794588	204.438653	47.071015
2610.456234	209.647540	47.076020
2607.029351	203.191485	47.081025
2603.398187	206.805823	47.086029
2599.865770	201.447667	47.091034
2596.607573	201.506607	47.096039
2592.935796	206.003854	47.101044
2589.801485	197.683876	47.106049
2586.447984	203.496968	47.111053
2582.994714	206.682657	47.116058
2579.194803	205.542487	47.121063
2575.814021	206.756031	47.126068
2572.038018	200.208621	47.131073
2569.017194	209.549106	47.136077
2565.915518	202.734358	47.141082
2562.181544	195.292972	47.146087
2558.095832	205.975439	47.151092
2554.454336	195.031210	47.156097
2551.222953	207.454831	47.161101
2547.774341	203.107222	47.166106
2544.502012	194.788625	47.171111
2540.796778	206.200025	47.176116
2537.726164	190.822445	47.181121
2534.435438	188.227704	47.186125
2531.063712	200.411123	47.191130
2527.306621	201.858892	47.196135
2523.521275	204.312236	47.201140
2519.881682	186.325368	47.206145
2516.174138	193.879226	47.211149
2513.293612	191.068382	47.216154
2509.578750	193.481255	47.221159
2506.218822	192.430709	47.226164
2502.653862	188.504581	47.231169
2499.329476	192.936684	47.236173
2495.819336	190.944069	47.241178
2492.451830	187.266461	47.246183
2488.639904	194.247588	47.251188
2485.556873	182.479437	47.256193
2482.012086	183.494456	47.261197
2478.265852	183.090635	47.266202
2474.647438	191.508112	47.271207
2471.011403	194.976347	47.276212
2467.704650	189.359732	47.281217
2464.433631	189.150150	47.286221
2460.903161	182.143647	47.291226
2457.503707	181.393718	47.296231
2453.917950	185.834994	47.301236
2450.635559	190.277544	47.306241
2446.870886	197.327646	47.311245
2443.420620	186.511315	47.316250
2439.911095	190.273574	47.321255
2436.655181	192.139467	47.326260
2433.224363	186.962964	47.331265
2429.613206	187.243283	47.336269
2425.834855	185.935105	47.341274
2422.501439	185.698000	47.346279
2418.763870	179.593915	47.351284
2415.491885	180.448570	47.356289
2411.536486	176.374059	47.361293
2408.128103	183.195871	47.366298
2404.644330	186.833715	47.371303
2401.553974	187.946216	47.376308
2398.751753	177.130164	47.381313
2394.544543	189.365986	47.386317
2391.391126	180.669474	47.391322
2387.990058	184.041240	47.396327
2383.794793	184.286509	47.401332
2380.409049	177.547580	47.406337
2377.432443	185.741623	47.411341
2373.578651	182.411645	47.416346
2370.199314	175.020455	47.421351
2366.152307	182.686689	47.426356
2363.229422	171.076837	47.431361
2359.319591	178.070332	47.436365
2355.820446	174.040888	47.441370
2352.528946	189.969204	47.446375
2348.839217	179.279650	47.451380
2345.929382	171.068940	47.456385
2342.340952	180.425998	47.461389
2338.821680	174.594867	47.466394
2335.366074	177.455922	47.471399
2331.650004	171.342246	47.476404
2328.433491	174.055173	47.481409
2324.638377	175.107638	47.486413
2320.902032	179.265523	47.491418
2317.471594	168.342831	47.496423
2314.202486	179.983681	47.501428
2311.229491	168.346060	47.506433
2306.986280	171.964914	47.511437
2303.337963	178.589934	47.516442
2300.206191	178.848588	47.521447
2296.310163	171.584286	47.526452
2293.312915	161.729095	47.531457
2289.653579	162.584066	47.536461
2286.358743	174.022382	47.541466
2282.509206	168.807230	47.546471
2278.917022	174.755383	47.551476
2275.731924	171.499648	47.556481
2271.985440	172.146276	47.561485
2268.848466	176.079423	47.566490
2265.596982	173.222852	47.571495
2261.883240	177.459333	47.576500
2258.605044	169.585581	47.581505
2254.578993	178.877647	47.586509
2251.003852	169.641148	47.591514
2247.744468	167.654771	47.596519
2244.061358	167.816531	47.601524
2240.701635	163.393304	47.606529
2237.182209	176.942068	47.611533
2233.419584	170.260765	47.616538
2230.487691	171.559081	47.621543
2226.929846	165.544804	47.626548
2223.198591	157.640956	47.631553
2219.286678	163.813401	47.636557
2215.869710	163.211615	47.641562
2212.653046	162.894953	47.646567
2209.196127	172.962045	47.651572
2205.998246	168.173605	47.656577
2201.994488	168.971053	47.661581
2198.597679	172.217148	47.666586
2195.497245	172.532652	47.671591
2191.822262	174.922613	47.676596
2188.550727	163.687586	47.681601
2184.638460	173.647985	47.686605
2180.975291	166.664518	47.691610
2177.526166	168.848946	47.696615
2174.029275	170.568867	47.701620
2170.572692	156.082428	47.706625
2167.139073	164.507996	47.711629
2163.847901	169.495669	47.716634
2160.642995	171.636497	47.721639
2156.805207	173.345417	47.726644
2153.436804	166.167709	47.731649
2149.917619	162.280102	47.736653
2146.269364	170.815444	47.741658
2142.605738	166.315955	47.746663
2138.522214	172.131705	47.751668
2135.686370	161.227904	47.756673
2132.427388	172.255449	47.761677
2129.222725	155.405464	47.766682
2125.329376	158.935157	47.771687
2121.432535	164.652109	47.776692
2118.351627	163.076130	47.781697
2114.727444	161.114778	47.786701
2111.178490	156.804710	47.791706
2107.601815	152.524104	47.796711
2104.207144	159.344057	47.801716
2101.017477	160.606234	47.806721
2097.343181	158.037710	47.811725
2093.671861	161.174062	47.816730
2090.356851	162.210343	47.821735
2086.565094	171.738820	47.826740
2083.248874	158.617072	47.831745
2079.530831	168.751790	47.836749
2076.139589	157.592944	47.841754
2073.067153	158.523534	47.846759
2069.067360	161.322617	47.851764
2065.792528	155.040193	47.856769
2062.058082	160.393438	47.861773
2058.781392	162.180769	47.866778
2055.481990	155.960046	47.871783
2051.636880	161.310718	47.876788
2048.473001	154.094290	47.881793
2044.635543	160.160817	47.886797
2040.968783	161.715999	47.891802
2037.652406	154.425586	47.896807
2033.728485	156.319584	47.901812
2030.825128	148.309738	47.906817
2027.305945	154.890881	47.911821
2023.537308	155.417278	47.916826
2020.124661	150.425808	47.921831
2016.488687	156.114031	47.926836
2013.243751	151.478791	47.931841
2009.713516	150.772807	47.936845
2006.292617	150.927641	47.941850
2002.943860	154.200656	47.946855
1999.177197	153.738690	47.951860
1995.913861	150.092599	47.956865
1992.283249	148.929856	47.961869
1988.558495	156.308189	47.966874
1985.074848	148.732964	47.971879
1981.236454	157.426033	47.976884
1977.838128	150.831443	47.981889
1975.193015	158.444897	47.986893
1971.732495	153.085871	47.991898
1967.824471	153.091956	47.996903
1964.009600	166.098643	48.001908
1960.845855	147.863858	48.006913
1957.131835	164.978537	48.011917
1953.395131	154.939903	48.016922
1950.251556	151.441739	48.021927
1946.742230	165.891043	48.026932
1943.441401	157.348215	48.031937
1939.766327	158.480593	48.036941
1936.275403	156.888043	48.041946
1932.585921	148.105541	48.046951
1928.847498	160.249070	48.051956
1925.676138	153.613756	48.056961
1922.306311	157.250857	48.061965
1918.526040	155.446382	48.066970
1915.332550	147.949630	48.071975
1911.615736	157.972777	48.076980
1908.192706	149.499767	48.081985
1904.584045	160.989155	48.086989
1901.002226	147.806227	48.091994
1897.826825	151.857497	48.096999
1894.014539	153.420940	48.102004
1890.922960	147.067651	48.107009
1887.211263	151.441253	48.112013
1883.718131	150.647534	48.117018
1880.270180	145.287498	48.122023
1876.497865	148.454191	48.127028
1873.223530	140.023472	48.132033
1869.246574	148.184295	48.137037
1866.089501	144.072161	48.142042
1862.636028	139.804715	48.147047
1859.091869	147.776602	48.152052
1855.757809	140.934674	48.157057
1851.876681	144.046605	48.162061
1848.959583	156.470054	48.167066
1845.282357	147.400854	48.172071
1841.595586	151.215459	48.177076
1838.184657	140.755917	48.182081
1834.580163	147.386277	48.187085
1831.136643	143.497275	48.192090
1827.841196	140.802672	48.197095
1824.114022	147.237292	48.202100
1820.809288	140.667593	48.207105
1816.828110	145.231750	48.212109
1813.250038	143.686313	48.217114
1809.996768	141.986603	48.222119
1806.464196	151.650336	48.227124
1803.487335	137.795175	48.232129
1799.842935	157.125145	48.237133
1796.331758	142.691160	48.242138
1792.419486	139.419796	48.247143
1788.868265	150.291164	48.252148
1785.489728	142.148340	48.257153
1782.056535	152.758219	48.262157
1778.543577	147.712156	48.267162
1774.852451	143.412349	48.272167
1771.428826	146.720252	48.277172
1767.958596	144.822302	48.282177
1764.469072	147.356729	48.287181
1761.376239	150.941530	48.292186
1757.662776	142.577190	48.297191
1754.058622	142.570802	48.302196
1750.543480	138.432869	48.307201
1747.262130	143.836581	48.312205
1743.489287	152.955883	48.317210
1740.373998	139.215088	48.322215
1736.364305	154.968973	48.327220
1733.170280	146.374104	48.332225
1729.369950	149.803883	48.337229
1726.205996	144.741852	48.342234
1722.504660	141.778954	48.347239
1719.013391	150.097584	48.352244
1715.790552	145.903727	48.357249
1711.926717	154.987031	48.362253
1708.369501	158.477171	48.367258
1705.309747	149.285625	48.372263
1701.495828	148.612926	48.377268
1698.183059	140.694110	48.382273
1694.365537	150.664661	48.387277
1690.774513	144.799066	48.392282
1687.598450	151.174609	48.397287
1683.825729	149.990513	48.402292
1680.476870	147.746522	48.407297
1676.901922	142.471465	48.412301
1673.550166	148.959418	48.417306
1670.021839	144.700803	48.422311
1666.251143	149.624088	48.427316
1662.941187	142.654410	48.432321
1659.509693	150.301120	48.437325
1656.072613	146.133556	48.442330
1652.508319	138.697721	48.447335
1649.035860	145.732190	48.452340
1645.618734	142.882088	48.457345
1642.003938	150.589985	48.462349
1638.476631	141.492986	48.467354
1635.040502	146.399311	48.472359
1631.190334	146.570374	48.477364
1627.701488	144.025416	48.482369
1624.823391	141.547335	48.487373
1621.149168	147.804234	48.492378
1617.745133	136.309534	48.497383
1613.829243	150.219268	48.502388
1610.281308	137.544495	48.507393
1606.665472	145.162606	48.512397
1603.357304	131.509373	48.517402
1600.418711	144.066762	48.522407
1596.844325	140.390096	48.527412
1593.197085	137.948984	48.532417
1588.873762	140.388156	48.537421
1585.506239	141.403554	48.542426
1582.242614	133.632002	48.547431
1579.009746	145.124244	48.552436
1575.651142	132.905337	48.557441
1571.990755	140.651827	48.562445
1568.409678	134.687814	48.567450
1564.912502	130.832025	48.572455
1561.321327	139.577003	48.577460
1558.126891	131.885761	48.582465
1554.031058	134.799727	48.587469
1550.993508	138.569097	48.592474
1547.800242	136.225029	48.597479
1543.885806	145.567674	48.602484
1540.590547	143.571254	48.607489
1537.012921	136.627722	48.612493
1533.179207	139.036090	48.617498
1529.731577	137.693059	48.622503
1526.004831	144.139505	48.627508
1522.870407	130.257051	48.632513
1519.378185	136.177395	48.637517
1515.849352	131.276491	48.642522
1512.610193	126.585475	48.647527
1508.752322	150.290409	48.652532
1505.498926	129.298808	48.657537
1502.185432	132.584918	48.662541
1498.305368	137.546020	48.667546
1495.061133	122.840376	48.672551
1491.244464	135.543429	48.677556
1487.844259	132.688689	48.682561
1484.250277	134.585524	48.687565
1480.877242	137.675705	48.692570
1477.526626	123.951300	48.697575
1473.192472	142.278556	48.702580
1470.229316	129.138538	48.707585
1466.989151	132.934661	48.712589
1463.042852	128.701155	48.717594
1459.908568	134.384786	48.722599
1456.193643	128.983379	48.727604
1453.170464	122.420606	48.732609
1449.420805	133.817675	48.737613
1446.011962	128.846423	48.742618
1442.535739	129.206071	48.747623
1438.581182	137.177674	48.752628
1435.083392	124.663693	48.757633
1431.992394	121.732469	48.762637
1428.377492	129.355893	48.767642
1424.743476	126.475457	48.772647
1421.166266	138.504430	48.777652
1418.001368	125.085343	48.782657
1414.108154	134.800498	48.787661
1410.359556	127.010471	48.792666
1407.331525	123.427687	48.797671
1403.780535	136.953835	48.802676
1400.301239	126.648736	48.807681
1396.668310	136.098147	48.812685
1392.994311	135.666179	48.817690
1389.788131	126.042969	48.822695
1385.888424	132.858026	48.827700
1382.746672	131.881756	48.832705
1379.267936	134.540617	48.837709
1375.913489	130.966803	48.842714
1372.297897	128.731602	48.847719
1368.592623	139.137476	48.852724
1365.491887	120.061492	48.857729
1361.912046	139.805505	48.862733
1358.052196	131.137692	48.867738
1354.899527	125.336280	48.872743
1350.854448	140.414554	48.877748
1347.730675	119.890428	48.882753
1344.178835	135.456202	48.887757
1340.538487	129.899276	48.892762
1337.462381	128.518673	48.897767
1333.614759	137.100747	48.902772
1330.548607	127.895603	48.907777
1326.674912	134.887355	48.912781
1323.302431	133.531451	48.917786
1319.589353	130.374345	48.922791
1316.356048	128.887816	48.927796
1312.619534	132.762243	48.932801
1308.867966	136.814995	48.937805
1305.289937	132.464525	48.942810
1302.474060	131.676988	48.947815
1298.451827	137.497367	48.952820
1295.036427	125.622444	48.957825
1291.724181	128.438072	48.962829
1288.101422	132.342788	48.967834
1285.136375	126.747311	48.972839
1281.294824	126.560110	48.977844
1277.678513	127.770165	48.982849
1274.101508	122.742310	48.987853
1270.856185	134.614322	48.992858
1267.039053	131.894454	48.997863
1263.425817	131.858443	49.002868
1260.028008	124.894438	49.007873
1256.748706	127.483418	49.012877
1253.246755	129.998236	49.017882
1249.770302	129.986514	49.022887
1245.966749	129.236958	49.027892
1242.572709	121.650943	49.032897
1238.996900	127.939198	49.037901
1235.435660	127.448219	49.042906
1232.364175	112.830415	49.047911
1228.108496	128.300893	49.052916
1225.064645	124.231494	49.057921
1221.466762	128.185026	49.062925
1218.223078	135.416711	49.067930
1215.024721	128.693755	49.072935
1210.998894	134.528231	49.077940
1207.924843	131.833939	49.082945
1204.414350	125.779245	49.087949
1200.533359	125.422645	49.092954
1196.861714	125.488145	49.097959
1193.375478	127.677373	49.102964
1190.166917	123.441349	49.107969
1186.429850	127.847005	49.112973
1183.023013	124.435187	49.117978
1179.449818	119.348185	49.122983
1175.633670	128.729701	49.127988
1172.695803	120.313865	49.132993
1169.079224	122.801991	49.137997
1165.453686	119.541322	49.143002
1162.248431	123.113244	49.148007
1158.410952	134.053893	49.153012
1155.444706	114.457547	49.158017
1151.928854	125.654057	49.163021
1147.906845	136.877721	49.168026
1144.482201	117.162667	49.173031
1140.656967	129.570836	49.178036
1137.325199	128.276223	49.183041
1134.332505	122.952647	49.188045
1130.594720	123.811609	49.193050
1127.160483	116.332423	49.198055
1123.057653	124.312926	49.203060
1120.260268	118.294907	49.208065
1116.412050	132.918028	49.213069
1113.028513	124.839822	49.218074
1109.674513	115.145302	49.223079
1106.024640	121.220404	49.228084
1102.564497	107.312493	49.233089
1098.915278	125.947926	49.238093
1095.434389	125.861301	49.243098
1091.924564	118.337661	49.248103
1088.102910	117.734923	49.253108
1084.826132	122.140073	49.258113
1081.487729	116.284669	49.263117
1077.923511	120.308122	49.268122
1074.928433	123.179042	49.273127
1071.239699	129.179127	49.278132
1067.509090	111.082152	49.283137
1063.953225	123.749972	49.288141
1060.530673	113.223081	49.293146
1057.109270	119.359178	49.298151
1053.452238	124.448653	49.303156
1049.948915	118.941112	49.308161
1046.442107	117.536110	49.313165
1042.505064	123.586894	49.318170
1039.397922	111.278460	49.323175
1035.634322	125.414396	49.328180
1032.528514	118.654346	49.333185
1029.066288	115.878986	49.338189
1025.300228	126.053294	49.343194
1022.004205	122.387422	49.348199
1018.287411	115.285368	49.353204
1015.042905	113.534752	49.358209
1011.346297	118.604388	49.363213
1007.628774	111.986722	49.368218
1004.524120	115.464718	49.373223
1001.063904	118.668624	49.378228
997.227373	126.273145	49.383233
993.865023	120.230777	49.388237
990.536274	127.249025	49.393242
987.062936	118.497154	49.398247
983.192061	120.188196	49.403252
979.376460	120.583460	49.408257
976.356396	123.101625	49.413261
972.974478	121.001482	49.418266
969.684786	115.655110	49.423271
965.931759	128.712508	49.428276
962.466340	113.678054	49.433281
958.812154	116.804470	49.438285
955.124129	119.011015	49.443290
951.803824	127.185445	49.448295
948.432354	130.831495	49.453300
944.705811	117.286644	49.458305
941.096856	116.777414	49.463309
937.932965	119.547989	49.468314
934.747852	115.734932	49.473319
930.827076	125.004773	49.478324
927.340504	107.624431	49.483329
923.697469	118.067102	49.488333
920.045373	123.104175	49.493338
917.178025	124.378117	49.498343
913.040905	127.583741	49.503348
910.091939	118.753403	49.508353
906.693020	121.098490	49.513357
902.580601	119.334942	49.518362
899.147325	114.770815	49.523367
895.588929	118.158840	49.528372
892.095321	119.887599	49.533377
889.063949	120.013473	49.538381
885.340597	107.728727	49.543386
882.009285	115.504842	49.548391
878.087366	117.713380	49.553396
874.382224	117.647994	49.558401
871.690451	115.280263	49.563405
867.673497	133.059514	49.568410
864.769692	123.842443	49.573415
860.891311	115.035584	49.578420
857.029999	132.614766	49.583425
853.516659	123.398830	49.588429
849.800440	123.269398	49.593434
847.100288	107.556307	49.598439
843.438635	121.648048	49.603444
839.818975	115.682280	49.608449
836.002009	123.216015	49.613453
832.785771	123.210214	49.618458
829.271279	116.003540	49.623463
825.365576	122.538515	49.628468
822.171831	104.303385	49.633473
818.865811	114.224890	49.638477
815.225050	122.570424	49.643482
811.798429	111.499033	49.648487
808.373557	118.559029	49.653492
804.579085	118.866106	49.658497
801.042543	121.406400	49.663501
797.611495	116.185277	49.668506
794.281183	123.543941	49.673511
790.440190	127.319568	49.678516
787.074323	122.717319	49.683521
783.651562	121.388000	49.688525
780.009860	124.582364	49.693530
776.663802	114.796868	49.698535
773.238123	125.571611	49.703540
769.845263	109.482618	49.708545
766.200083	119.669246	49.713549
762.653907	116.675415	49.718554
759.357156	117.634183	49.723559
755.416701	114.618396	49.728564
752.185047	111.707929	49.733569
748.831423	106.989631	49.738573
744.914135	119.076568	49.743578
741.653724	118.529199	49.748583
737.971576	114.152172	49.753588
734.789057	122.539310	49.758593
731.486207	115.273129	49.763597
727.791061	114.576145	49.768602
724.574742	112.445578	49.773607
720.596401	119.483673	49.778612
717.130555	117.486890	49.783617
713.213518	118.581633	49.788621
709.943382	109.479788	49.793626
706.781204	104.329360	49.798631
703.162674	109.469782	49.803636
699.801260	109.023874	49.808641
696.326500	107.067467	49.813645
692.498813	114.638629	49.818650
688.931051	107.071144	49.823655
685.452721	114.059801	49.828660
681.946147	106.115522	49.833665
678.854021	115.907888	49.838669
674.923775	110.617229	49.843674
671.954557	101.450467	49.848679
668.231627	118.828425	49.853684
664.678190	110.659682	49.858689
660.929636	114.401929	49.863693
657.190646	115.147883	49.868698
653.911304	111.513320	49.873703
650.389213	110.755711	49.878708
647.189740	107.709953	49.883713
643.790713	115.774948	49.888717
639.988416	108.421488	49.893722
636.455824	105.586351	49.898727
632.865348	114.013475	49.903732
629.214700	115.073149	49.908737
626.171969	118.233121	49.913741
622.742937	109.772039	49.918746
619.182527	101.422171	49.923751
615.126139	115.412495	49.928756
611.923664	115.505827	49.933761
608.345372	120.015890	49.938765
604.442570	124.899126	49.943770
601.610126	106.812019	49.948775
598.279574	111.280951	49.953780
594.835288	115.406472	49.958785
591.366257	115.980977	49.963789
587.607070	118.875547	49.968794
584.346213	117.421847	49.973799
580.203672	122.458973	49.978804
576.809435	115.501349	49.983809
573.681170	117.903407	49.988813
569.874196	116.142389	49.993818
566.350060	116.126573	49.998823
562.682120	116.867531	50.003828
559.642433	112.074780	50.008833
556.023554	115.377053	50.013837
552.298454	124.621460	50.018842
549.181981	108.872195	50.023847
545.253065	124.942215	50.028852
541.814439	112.177618	50.033857
538.435008	114.190442	50.038861
534.791376	120.300534	50.043866
531.303225	113.588640	50.048871
527.771143	121.848296	50.053876
524.758088	111.572041	50.058881
521.381021	116.113884	50.063885
517.240248	119.812478	50.068890
514.051755	115.247729	50.073895
510.294626	114.865539	50.078900
507.134959	111.310492	50.083905
503.320749	105.947670	50.088909
499.858342	113.049673	50.093914
496.192424	105.680233	50.098919
492.933433	108.993241	50.103924
489.558540	109.428280	50.108929
485.764158	112.060028	50.113933
482.239621	115.269149	50.118938
478.908796	106.057435	50.123943
475.576070	119.825091	50.128948
471.976138	118.225540	50.133953
468.555863	118.449492	50.138957
464.876716	112.142541	50.143962
461.152993	108.858224	50.148967
457.924351	105.433274	50.153972
454.589352	113.663610	50.158977
450.905408	108.040831	50.163981
446.883413	106.329863	50.168986
444.042731	105.480782	50.173991
440.200409	113.331466	50.178996
437.116267	106.564604	50.184001
433.360100	107.605287	50.189005
429.885741	101.846491	50.194010
426.554772	100.639797	50.199015
422.641992	113.628866	50.204020
419.165798	102.824425	50.209025
415.895540	107.836022	50.214029
412.073825	102.376078	50.219034
408.993061	99.579383	50.224039
405.439716	107.409526	50.229044
401.807825	104.494814	50.234049
398.200632	100.419840	50.239053
394.859873	116.102605	50.244058
391.470743	102.022437	50.249063
387.589228	107.077576	50.254068
384.272289	109.533819	50.259073
380.754817	105.207949	50.264077
377.417228	109.408879	50.269082
374.186210	104.950581	50.274087
370.099293	109.041953	50.279092
366.637803	103.968978	50.284097
363.311400	98.835286	50.289101
359.708498	104.683813	50.294106
356.240060	101.183548	50.299111
352.599953	102.874380	50.304116
349.249168	99.763843	50.309121
345.837239	95.385946	50.314125
342.253219	96.688397	50.319130
338.990299	99.210295	50.324135
335.333740	101.766212	50.329140
331.847247	100.957409	50.334145
328.468557	99.981518	50.339149
324.667008	99.072917	50.344154
321.283387	104.825852	50.349159
317.644327	111.177504	50.354164
314.315905	114.072804	50.359169
310.621539	102.782386	50.364173
307.027136	108.313229	50.369178
303.645976	100.638383	50.374183
299.719563	108.502773	50.379188
296.994597	99.716873	50.384193
293.548019	101.317989	50.389197
289.920214	97.270822	50.394202
286.506150	96.174950	50.399207
282.721047	96.385092	50.404212
279.054803	94.671840	50.409217
275.392985	97.241120	50.414221
271.985757	95.500827	50.419226
269.127650	91.594374	50.424231
265.216613	102.939326	50.429236
261.918114	105.201002	50.434241
258.146760	100.430227	50.439245
254.195768	97.592163	50.444250
251.136178	97.090793	50.449255
247.646502	104.044014	50.454260
244.141956	105.513518	50.459265
240.813534	110.592150	50.464269
237.402427	102.040276	50.469274
233.373970	109.617401	50.474279
230.042018	110.458356	50.479284
226.631436	102.399733	50.484289
223.321584	101.590296	50.489293
219.317910	104.077115	50.494298
216.230843	100.150927	50.499303
212.461568	96.649482	50.504308
209.068345	104.363405	50.509313
205.683125	97.498587	50.514317
201.787938	98.864517	50.519322
198.223961	94.375869	50.524327
194.758051	105.629167	50.529332
192.032446	88.554196	50.534337
188.749680	103.001250	50.539341
184.648226	92.273135	50.544346
181.401316	101.485567	50.549351
177.579885	107.907510	50.554356
174.054507	98.736522	50.559361
170.690958	93.322664	50.564365
166.823589	100.398110	50.569370
163.606749	99.065935	50.574375
160.112952	107.329602	50.579380
156.526061	103.119683	50.584385
153.058334	93.505211	50.589389
149.326909	105.058407	50.594394
146.219585	97.992960	50.599399
142.394262	105.449397	50.604404
139.294733	98.581766	50.609409
135.878385	104.594262	50.614413
131.745467	108.678732	50.619418
128.608020	100.799580	50.624423
124.663332	103.217695	50.629428
121.587701	102.472040	50.634433
118.081153	110.614532	50.639437
114.216962	105.122307	50.644442
111.087778	102.781263	50.649447
107.756204	98.403069	50.654452
103.854067	96.160687	50.659457
100.571807	94.232057	50.664461
96.905340	108.743147	50.669466
93.264212	88.492829	50.674471
89.997588	89.686337	50.679476
86.679181	91.533330	50.684481
83.479525	90.108586	50.689485
79.804432	96.221749	50.694490
76.210358	87.289613	50.699495
72.244671	108.380901	50.704500
68.607258	92.570717	50.709505
65.240844	100.116716	50.714509
61.745850	107.215233	50.719514
58.563025	97.607971	50.724519
54.903044	103.355561	50.729524
51.545090	107.436625	50.734529
47.989946	103.956596	50.739533
44.271483	111.202184	50.744538
41.499726	96.579149	50.749543
37.739626	110.633641	50.754548
33.700425	103.723372	50.759553
30.288386	102.301808	50.764557
26.949794	98.217301	50.769562
23.662554	99.089884	50.774567
19.452484	107.756877	50.779572
16.485956	100.040241	50.784577
12.931707	103.033917	50.789581
9.430162	112.770694	50.794586
6.132347	102.101420	50.799591
2.454830	101.366120	50.804596