Fri Jun 17 18:03:05 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.108033	85.192601	0.000000
0.195727	89.079660	0.005005
0.353107	78.315997	0.010010
-0.180043	87.382963	0.015014
-0.328615	65.098523	0.020019
-0.517526	73.303355	0.025024
-0.844809	58.248219	0.030029
-1.021064	52.700996	0.035034
-1.505871	50.744762	0.040038
-1.515630	47.224464	0.045043
-1.973056	39.198554	0.050048
-2.363867	32.023907	0.055053
-2.215778	34.695625	0.060058
-2.506009	34.974369	0.065062
-2.725464	21.182805	0.070067
-3.180956	18.528091	0.075072
-3.021229	5.799279	0.080077
-3.774742	3.547717	0.085082
-4.233445	5.123882	0.090086
-4.292794	-0.153075	0.095091
-4.556729	-3.018406	0.100096
-5.316712	-2.795173	0.105101
-5.447560	-2.473659	0.110106
-5.825291	-6.802411	0.115110
-5.497443	2.354834	0.120115
-5.706389	-3.105438	0.125120
-6.393832	0.160787	0.130125
-6.939362	-5.800795	0.135130
-7.211257	-5.215490	0.140134
-6.646993	-8.737654	0.145139
-6.989377	-10.145890	0.150144
-6.963833	-8.450519	0.155149
-7.418643	-17.864648	0.160154
-8.289678	3.558936	0.165158
-8.472244	-9.322531	0.170163
-8.936559	-3.051568	0.175168
-8.763411	-5.814321	0.180173
-8.621725	-14.507302	0.185178
-9.066634	-3.181430	0.190182
-9.462744	-5.174500	0.195187
-10.131474	-0.566587	0.200192
-10.359706	-4.871645	0.205197
-9.968326	-10.953437	0.210202
-10.391824	0.797674	0.215206
-10.319570	-11.809630	0.220211
-11.239047	-13.316706	0.225216
-11.688242	-8.567887	0.230221
-11.723602	-8.073994	0.235226
-12.085302	-6.042336	0.240230
-12.060962	-4.437536	0.245235
-12.219339	-2.916619	0.250240
-12.023178	-6.095812	0.255245
-12.289774	-16.078552	0.260250
-13.279734	3.082295	0.265254
-13.497211	-12.088304	0.270259
-13.637909	-7.042675	0.275264
-13.707453	-11.541640	0.280269
-13.454977	-4.976417	0.285274
-14.659766	-5.184015	0.290278
-14.778242	-6.689259	0.295283
-15.005482	2.826251	0.300288
-15.002230	-8.283896	0.305293
-15.092456	-5.055373	0.310298
-15.373471	4.903398	0.315302
-15.216413	-9.860209	0.320307
-16.234534	-5.430622	0.325312
-16.573798	6.966164	0.330317
-16.476893	3.584629	0.335322
-16.905295	6.837990	0.340326
-16.620713	-13.235825	0.345331
-17.177699	1.081441	0.350336
-18.328640	1.954347	0.355341
-18.226874	-0.818445	0.360346
-18.324326	-5.779851	0.365350
-18.391413	-0.919513	0.370355
-18.570042	-6.030222	0.375360
-18.718297	1.538926	0.380365
-18.526517	-8.413254	0.385370
-19.038526	1.571676	0.390374
-19.487043	-6.478182	0.395379
-19.861945	-8.665395	0.400384
-20.092836	-4.455064	0.405389
-19.792263	-13.035339	0.410394
-20.648457	-2.517440	0.415398
-21.015951	4.493796	0.420403
-21.349565	-10.796418	0.425408
-21.703704	-6.789372	0.430413
-21.543400	-4.149292	0.435418
-21.819098	-1.592036	0.440422
-21.943266	1.387378	0.445427
-21.946055	-5.672966	0.450432
-22.164087	-3.076160	0.455437
-22.270231	-2.202877	0.460442
-22.767958	-4.588314	0.465446
-23.380240	-5.991545	0.470451
-24.330580	3.003630	0.475456
-24.439131	-5.233370	0.480461
-23.794310	1.492185	0.485466
-24.557371	0.450856	0.490470
-24.627387	-6.198524	0.495475
-24.678862	-7.122917	0.500480
-24.678434	-3.744694	0.505485
-24.830082	-14.953206	0.510490
-25.913317	-2.058233	0.515494
-26.183247	-7.274529	0.520499
-26.219225	-10.943385	0.525504
-26.516340	1.744554	0.530509
-26.364342	-6.324611	0.535514
-26.206017	-8.030374	0.540518
-26.954032	-9.521350	0.545523
-27.431744	-3.928944	0.550528
-27.924637	-6.596772	0.555533
-27.599391	-1.860059	0.560538
-27.953638	2.330524	0.565542
-28.170820	2.055261	0.570547
-29.188290	-3.953372	0.575552
-29.364853	-1.648994	0.580557
-28.653694	-6.779539	0.585562
-29.393960	0.420936	0.590566
-29.539678	-5.090492	0.595571
-29.604905	-5.593276	0.600576
-29.860802	-1.755883	0.605581
-29.830284	-5.050409	0.610586
-30.486687	2.375685	0.615590
-30.910022	1.196784	0.620595
-31.183988	7.214315	0.625600
-31.091321	-0.605434	0.630605
-31.898910	-5.268043	0.635610
-32.426390	0.785113	0.640614
-32.697484	-4.245500	0.645619
-32.269059	4.923833	0.650624
-32.263822	3.566741	0.655629
-32.362447	-3.113403	0.660634
-32.797411	-3.253603	0.665638
-32.977994	-10.483495	0.670643
-33.703256	4.316786	0.675648
-34.138754	-3.301703	0.680653
-34.154224	-6.460123	0.685658
-34.594861	1.045344	0.690662
-34.282484	-5.681214	0.695667
-34.623876	-0.213090	0.700672
-35.175823	-2.690742	0.705677
-35.356877	-4.419813	0.710682
-35.669123	-2.595676	0.715686
-36.042096	-6.054796	0.720691
-35.523135	-5.200963	0.725696
-36.365460	-4.729018	0.730701
-36.884090	-4.089476	0.735706
-37.550790	-4.625081	0.740710
-37.582855	0.455574	0.745715
-37.464032	-6.169746	0.750720
-37.492487	-0.818167	0.755725
-37.272023	-11.836742	0.760730
-37.524316	2.507822	0.765734
-38.038293	-21.121122	0.770739
-38.356058	-2.634404	0.775744
-38.995059	-0.790286	0.780749
-39.220374	-10.731344	0.785754
-39.143399	-1.480310	0.790758
-39.396212	-3.250337	0.795763
-40.140861	-7.837567	0.800768
-40.598877	1.141877	0.805773
-40.465748	-4.513383	0.810778
-40.440044	-1.473636	0.815782
-40.463600	-2.905465	0.820787
-40.764581	-3.780885	0.825792
-41.457915	-1.578463	0.830797
-41.538431	-1.238478	0.835802
-42.155291	-3.576088	0.840806
-42.060975	-14.860411	0.845811
-42.115340	-7.252216	0.850816
-42.974111	1.282171	0.855821
-43.194679	-13.290196	0.860826
-43.827426	-3.350514	0.865830
-43.173346	-11.724145	0.870835
-43.437567	-15.976447	0.875840
-43.899577	4.172086	0.880845
-43.780728	-6.964377	0.885850
-44.352663	-9.734303	0.890854
-44.241733	-2.492593	0.895859
-44.775693	-6.338158	0.900864
-45.334193	-2.027785	0.905869
-45.459496	-12.930671	0.910874
-45.480072	-1.970933	0.915878
-45.710516	-4.127101	0.920883
-46.430180	-5.061582	0.925888
-46.996680	-4.249706	0.930893
-47.005818	-4.241259	0.935898
-47.068326	0.078227	0.940902
-47.033048	-4.053568	0.945907
-47.251317	-4.558537	0.950912
-47.304175	-1.144224	0.955917
-47.004803	-9.891439	0.960922
-48.121366	2.361053	0.965926
-48.390715	3.657902	0.970931
-48.611803	-0.547703	0.975936
-48.846506	-8.045056	0.980941
-48.783449	0.596572	0.985946
-49.497787	5.327904	0.990950
-49.783502	-8.127805	0.995955
-49.944805	-9.135565	1.000960
-50.272950	1.827351	1.005965
-50.018601	-2.505828	1.010970
-50.361637	2.632045	1.015974
-51.267469	-2.630685	1.020979
-51.468329	-2.073168	1.025984
-51.741661	-4.621995	1.030989
-51.959711	-1.939545	1.035994
-52.071186	-9.865062	1.040998
-51.781460	-6.242291	1.046003
-51.960717	-3.647392	1.051008
-52.406535	5.718371	1.056013
-53.138620	7.060765	1.061018
-54.070289	3.013536	1.066022
-53.754153	-3.721344	1.071027
-53.610220	-0.564108	1.076032
-53.709670	8.058756	1.081037
-53.472934	1.698382	1.086042
-53.826716	0.481481	1.091046
-54.600275	-1.987942	1.096051
-54.686941	0.981686	1.101056
-55.316290	4.245168	1.106061
-54.807818	-6.849898	1.111066
-55.864068	2.449804	1.116070
-56.161763	-4.001891	1.121075
-56.508346	-1.444887	1.126080
-56.867381	-0.114975	1.131085
-56.681517	-2.124468	1.136090
-56.865047	4.399766	1.141094
-57.036426	-3.978137	1.146099
-56.840360	-4.221653	1.151104
-57.240360	3.360137	1.156109
-57.852285	-4.771476	1.161114
-58.363790	10.052477	1.166118
-58.521277	-4.379820	1.171123
-58.300622	3.089326	1.176128
-58.783785	-1.743828	1.181133
-59.274808	-8.060969	1.186138
-59.552745	-2.974569	1.191142
-59.730440	-11.026813	1.196147
-59.721349	-2.595450	1.201152
-59.884737	-0.749881	1.206157
-60.332889	1.340551	1.211162
-61.236726	4.938751	1.216166
-61.535429	-0.927104	1.221171
-61.582717	5.217910	1.226176
-61.577526	7.757089	1.231181
-61.489832	-9.775547	1.236186
-61.593077	6.836809	1.241190
-61.803255	-7.811088	1.246195
-61.654347	-2.314950	1.251200
-62.595502	5.211762	1.256205
-62.818457	-0.919463	1.261210
-63.248328	1.869831	1.266214
-63.410387	-7.541651	1.271219
-64.314068	-4.791993	1.276224
-64.306087	0.218464	1.281229
-63.918230	-6.136442	1.286234
-64.753115	-2.687442	1.291238
-64.591948	-12.262366	1.296243
-64.929155	-12.402828	1.301248
-64.944411	-7.268930	1.306253
-64.593846	-12.300069	1.311258
-65.846174	-2.111958	1.316262
-66.358732	-8.938573	1.321267
-66.402031	-11.069609	1.326272
-66.788381	-8.186914	1.331277
-66.354061	-12.869089	1.336282
-66.628327	-2.483637	1.341286
-66.846461	-6.662498	1.346291
-67.480278	-3.257577	1.351296
-68.079234	-0.364599	1.356301
-68.205107	-12.292314	1.361306
-68.168595	-2.990554	1.366310
-68.129559	-7.081336	1.371315
-68.165110	-15.846672	1.376320
-69.025092	-13.888859	1.381325
-69.359644	-19.314622	1.386330
-69.390220	0.101330	1.391334
-69.354014	-15.967832	1.396339
-69.673868	-13.683245	1.401344
-70.644300	-8.930653	1.406349
-70.961120	-10.283538	1.411354
-71.191130	-6.025599	1.416358
-71.202810	-7.903983	1.421363
-71.185493	-13.852556	1.426368
-71.391007	-3.973435	1.431373
-71.354810	-19.072720	1.436378
-71.309724	-5.222775	1.441382
-71.912994	-5.978087	1.446387
-72.465335	-9.904652	1.451392
-72.708706	-10.594882	1.456397
-72.765330	-18.047634	1.461402
-73.061906	-0.953240	1.466406
-73.426954	-16.609582	1.471411
-73.721023	-10.647125	1.476416
-73.886385	-18.227429	1.481421
-74.039661	-19.242442	1.486426
-74.256318	-9.379824	1.491430
-74.434444	-11.014068	1.496435
-75.463627	-13.835648	1.501440
-75.810291	-1.208937	1.506445
-75.368194	-14.520414	1.511450
-75.737064	2.408998	1.516454
-75.871033	-15.100792	1.521459
-75.895144	-12.493797	1.526464
-76.227015	-7.929642	1.531469
-76.598235	-11.673594	1.536474
-77.015150	-4.860749	1.541478
-77.331412	-10.230751	1.546483
-77.268863	-14.868488	1.551488
-77.480352	-6.132093	1.556493
-77.370742	-14.464744	1.561498
-78.343799	-6.624504	1.566502
-78.523540	-0.703347	1.571507
-78.694219	-19.672984	1.576512
-78.932681	0.594663	1.581517
-78.943091	-12.136233	1.586522
-79.881833	-12.584181	1.591526
-80.399074	-9.058929	1.596531
-80.302663	-15.256063	1.601536
-80.947777	-2.630453	1.606541
-80.310252	-15.798201	1.611546
-80.130402	-2.357423	1.616550
-80.428969	-1.680656	1.621555
-80.922431	-7.712050	1.626560
-81.917882	-3.540967	1.631565
-82.024490	-7.646805	1.636570
-82.375343	-3.962145	1.641574
-82.324121	-2.284660	1.646579
-81.760537	-4.202238	1.651584
-82.389247	10.046053	1.656589
-82.540020	-6.231196	1.661594
-83.238218	4.240520	1.666598
-83.625450	7.241368	1.671603
-83.578582	-8.082681	1.676608
-84.182897	-3.999115	1.681613
-83.888794	-4.860585	1.686618
-84.649560	-9.282131	1.691622
-85.115874	-2.854348	1.696627
-85.344300	-16.912342	1.701632
-85.604284	4.088609	1.706637
-85.506092	-15.016304	1.711642
-85.721377	-6.252837	1.716646
-85.892206	-2.661248	1.721651
-85.533895	-14.072135	1.726656
-85.949194	-15.096670	1.731661
-86.726009	-2.521585	1.736666
-86.944352	-10.807217	1.741670
-86.981549	-4.635866	1.746675
-87.223936	-8.698610	1.751680
-88.349258	-10.831707	1.756685
-88.307495	-12.364374	1.761690
-88.682434	-16.809999	1.766694
-88.520748	-3.925038	1.771699
-88.495976	-10.645223	1.776704
-88.861017	-9.997068	1.781709
-88.906379	-14.095524	1.786714
-89.819399	-13.569389	1.791718
-90.190983	-7.786440	1.796723
-90.153916	-8.900582	1.801728
-90.687202	-3.021290	1.806733
-90.550792	-7.966512	1.811738
-90.465549	-4.584828	1.816742
-90.791147	-14.902282	1.821747
-90.448601	-4.356530	1.826752
-91.033963	-5.991548	1.831757
-91.618770	-17.711935	1.836762
-91.818429	-3.274309	1.841766
-92.594376	-0.265080	1.846771
-92.550956	-11.006573	1.851776
-93.398861	-8.660051	1.856781
-93.424079	-6.286706	1.861786
-93.611797	-1.966534	1.866790
-93.355791	-8.589595	1.871795
-93.521220	-11.572915	1.876800
-94.217860	-0.522696	1.881805
-93.944735	-10.443994	1.886810
-93.968744	-5.756579	1.891814
-94.646014	-8.745779	1.896819
-95.224145	-12.065606	1.901824
-95.545075	-2.336410	1.906829
-95.452533	-9.061941	1.911834
-95.493420	-11.327363	1.916838
-95.777948	-3.180875	1.921843
-96.080737	-14.239933	1.926848
-96.873009	-5.597016	1.931853
-96.950443	-13.075316	1.936858
-97.155128	-9.508095	1.941862
-97.444995	-12.399886	1.946867
-97.445850	-10.268374	1.951872
-97.577289	-7.666822	1.956877
-97.232719	-6.905365	1.961882
-97.933357	-11.456878	1.966886
-98.266087	-2.337242	1.971891
-98.458085	-10.018689	1.976896
-99.130354	-0.467879	1.981901
-99.676016	-13.738478	1.986906
-99.778757	-6.785861	1.991910
-99.939806	-5.236476	1.996915
-99.976453	-4.571290	2.006912
-99.880732	-5.531204	2.016909
-99.162146	-10.899768	2.026906
-99.212890	-11.524142	2.036902
-98.302127	-6.024874	2.046899
-97.555752	-7.511432	2.056896
-97.306347	-12.395967	2.066893
-96.205065	-9.782633	2.076890
-96.042044	-11.814944	2.086886
-95.977220	-14.169784	2.096883
-95.931184	-12.005183	2.106880
-94.827068	-15.587881	2.116877
-93.726854	-18.357474	2.126874
-93.767995	-16.611085	2.136870
-93.352953	-15.422433	2.146867
-92.864319	-16.535588	2.156864
-91.765270	-11.772789	2.166861
-91.606942	-16.586069	2.176858
-91.533773	-13.382749	2.186854
-90.815973	-8.566250	2.196851
-90.019583	-15.856778	2.206848
-89.820066	-19.852990	2.216845
-89.139449	-11.690987	2.226842
-88.442696	-19.352604	2.236838
-88.399168	-9.553435	2.246835
-87.863746	-16.398698	2.256832
-87.044471	-14.915671	2.266829
-86.911427	-11.108418	2.276826
-86.414495	-5.607528	2.286822
-85.791854	-5.056207	2.296819
-85.170236	-2.949551	2.306816
-84.161975	-5.519119	2.316813
-83.968270	-5.489434	2.326810
-83.688709	-4.944305	2.336806
-83.587651	-9.506227	2.346803
-82.605928	-8.254107	2.356800
-82.473815	-3.348144	2.366797
-81.471448	-6.862160	2.376794
-81.008583	-4.961468	2.386790
-80.827271	-11.055936	2.396787
-80.589576	-4.227472	2.406784
-79.268912	-7.180711	2.416781
-79.219693	-3.125387	2.426778
-78.990567	-7.259694	2.436774
-78.114249	-5.922280	2.446771
-77.676742	-6.142165	2.456768
-76.690199	-2.239694	2.466765
-76.690406	-6.639363	2.476762
-75.915672	-6.242937	2.486758
-75.919019	-10.356183	2.496755
-75.518367	-9.329128	2.506752
-74.982471	-6.612117	2.516749
-73.709367	-13.438937	2.526746
-73.487655	-17.185342	2.536742
-73.412481	-9.024639	2.546739
-73.020063	-11.480566	2.556736
-71.956790	-14.583063	2.566733
-71.790561	-9.304601	2.576730
-71.363357	-13.686606	2.586726
-70.435259	-1.008712	2.596723
-70.409050	-12.860412	2.606720
-69.410420	-7.089445	2.616717
-68.830129	-7.740478	2.626714
-68.817350	-11.058570	2.636710
-68.380573	-9.175669	2.646707
-67.352572	-5.416420	2.656704
-67.189918	-9.722044	2.666701
-67.014938	-10.032247	2.676698
-65.881139	-7.844564	2.686694
-65.709362	-7.450251	2.696691
-65.280866	-7.058899	2.706688
-64.258727	-8.759434	2.716685
-63.746095	-6.185554	2.726682
-63.975241	-5.732103	2.736678
-63.223530	-10.280870	2.746675
-62.418934	-6.173883	2.756672
-62.424119	-7.501714	2.766669
-61.643453	-14.076948	2.776666
-60.881873	-6.736502	2.786662
-60.659297	-9.851384	2.796659
-60.578613	-7.155514	2.806656
-59.423250	-14.260908	2.816653
-59.040303	-12.536410	2.826650
-58.687900	-11.477821	2.836646
-57.863990	-8.178399	2.846643
-57.852456	-16.635182	2.856640
-57.250214	-12.479739	2.866637
-56.368170	-13.577081	2.876634
-56.249023	-5.920998	2.886630
-55.800297	-8.041109	2.896627
-54.753067	-7.748064	2.906624
-54.417167	-5.623742	2.916621
-54.467860	-7.304990	2.926618
-53.683422	-12.511610	2.936614
-52.893801	-8.960498	2.946611
-52.746360	-10.316663	2.956608
-51.677721	-11.773205	2.966605
-51.200321	-12.288583	2.976602
-51.278710	-2.346835	2.986598
-50.882729	-6.610040	2.996595
-50.335991	-12.534279	3.006592
-49.617006	-11.799805	3.016589
-49.340233	-3.111081	3.026586
-48.409099	-8.899464	3.036582
-48.315104	-11.672099	3.046579
-47.095591	-7.576386	3.056576
-46.986636	-14.489261	3.066573
-46.584273	-14.353383	3.076570
-46.455521	-9.101883	3.086566
-45.165515	-9.909612	3.096563
-44.882337	-15.706067	3.106560
-44.837046	-13.666805	3.116557
-44.274308	-8.672974	3.126554
-43.286012	-13.196257	3.136550
-43.255719	-10.470870	3.146547
-42.707800	-1.858632	3.156544
-41.811000	-7.951312	3.166541
-41.630333	-9.810511	3.176538
-41.245233	-5.856660	3.186534
-40.292058	-8.560899	3.196531
-40.085434	-10.460767	3.206528
-39.882290	-14.754351	3.216525
-38.981810	-4.679538	3.226522
-38.627154	-6.651433	3.236518
-38.238691	-8.102195	3.246515
-37.288408	-3.844954	3.256512
-36.983663	-4.927536	3.266509
-36.795685	-6.676712	3.276506
-36.171068	-4.685933	3.286502
-35.689859	-7.073040	3.296499
-35.290276	-7.475504	3.306496
-34.414087	-4.636832	3.316493
-34.228761	-0.447644	3.326490
-32.989785	-4.284706	3.336486
-32.739235	-3.733367	3.346483
-32.514003	-4.747805	3.356480
-32.383346	-3.324169	3.366477
-31.672850	-2.067257	3.376474
-31.037704	0.608568	3.386470
-30.627591	-7.106762	3.396467
-29.723018	-6.352946	3.406464
-29.261735	-7.906502	3.416461
-28.926275	-6.953961	3.426458
-29.130125	-7.208304	3.436454
-27.966592	-4.645008	3.446451
-27.437415	-8.444103	3.456448
-27.267888	-6.497805	3.466445
-26.206924	-2.786896	3.476442
-25.855924	-6.844053	3.486438
-25.891726	-3.948623	3.496435
-25.468274	-9.496129	3.506432
-24.860868	-7.238123	3.516429
-23.748357	-6.859698	3.526426
-23.474348	-6.695172	3.536422
-23.315006	1.427249	3.546419
-22.363269	-3.098452	3.556416
-21.776335	-12.288283	3.566413
-21.687093	-7.835358	3.576410
-21.156717	-10.866651	3.586406
-20.320095	-10.895421	3.596403
-20.234325	-9.805548	3.606400
-19.356489	-11.579888	3.616397
-18.627579	-10.347570	3.626394
-18.547481	-5.774575	3.636390
-18.545783	-13.061823	3.646387
-17.472239	-5.647952	3.656384
-17.141320	-10.556903	3.666381
-16.373867	-12.125191	3.676378
-15.502902	-6.013299	3.686374
-15.166806	-10.455632	3.696371
-15.191780	-10.552797	3.706368
-15.000137	-11.430060	3.716365
-13.761460	-6.612790	3.726362
-13.389434	-9.265474	3.736358
-13.219288	-9.833307	3.746355
-12.240363	-10.103662	3.756352
-11.799058	-15.495869	3.766349
-12.161943	-16.961430	3.776346
-11.022288	-19.568032	3.786342
-10.507383	-15.718541	3.796339
-9.770248	-5.167266	3.806336
-9.140403	-9.347828	3.816333
-9.384993	-5.094489	3.826330
-8.626799	-8.553280	3.836326
-7.597833	-1.544544	3.846323
-7.485056	-3.988958	3.856320
-7.191725	-6.543798	3.866317
-6.763483	-9.694444	3.876314
-6.112823	2.523389	3.886310
-5.546769	-0.821470	3.896307
-4.967190	4.416354	3.906304
-4.759518	8.340827	3.916301
-4.095333	20.204928	3.926298
-3.833343	30.004176	3.936294
-2.961938	37.146605	3.946291
-2.766835	43.188295	3.956288
-2.555561	45.493584	3.966285
-2.165827	55.022266	3.976282
-1.538924	73.552125	3.986278
-0.964294	99.087507	3.996275
-0.173905	113.037137	4.006272
0.000000	118.040488	4.011277
-0.054615	123.775729	4.016282
0.328251	138.607038	4.021286
0.604103	138.183122	4.026291
0.540472	147.369216	4.031296
0.715949	135.029382	4.036301
0.791722	153.151725	4.041306
0.914130	137.624932	4.046310
0.770022	149.415359	4.051315
0.560566	148.544841	4.056320
1.063823	141.776033	4.061325
0.797947	144.071992	4.066330
0.977578	135.011503	4.071334
0.975799	144.925135	4.076339
0.909290	143.155102	4.081344
0.948304	144.544558	4.086349
0.908314	147.583218	4.091354
1.153269	153.772464	4.096358
1.113002	142.552226	4.101363
1.341955	152.567025	4.106368
1.107332	133.353053	4.111373
0.423256	142.005485	4.116378
0.980117	139.847682	4.121382
0.767019	155.980995	4.126387
0.797801	150.698477	4.131392
1.108681	150.486988	4.136397
1.036031	151.641040	4.141402
0.931246	152.985925	4.146406
1.291102	149.721082	4.151411
1.058210	156.918986	4.156416
0.889431	140.362177	4.161421
0.836344	154.948655	4.166426
1.029707	143.906648	4.171430
1.134030	149.081898	4.176435
0.997104	148.712582	4.181440
1.149552	148.294378	4.186445
1.032707	158.978582	4.191450
1.144008	145.923424	4.196454
1.329733	151.879600	4.201459
1.431907	153.292105	4.206464
1.203083	150.816360	4.211469
0.699613	163.726394	4.216474
0.910625	160.720916	4.221478
0.952135	143.014031	4.226483
1.096455	152.676256	4.231488
0.823237	146.952718	4.236493
1.138333	169.706915	4.241498
1.425578	165.104786	4.246502
1.431832	171.142501	4.251507
1.443650	179.917464	4.256512
1.626687	171.121207	4.261517
1.092127	167.960429	4.266522
1.452303	173.782242	4.271526
1.390608	181.628548	4.276531
1.350119	172.980344	4.281536
1.637225	166.036310	4.286541
1.357958	162.137309	4.291546
0.985826	158.555267	4.296550
1.561577	165.109652	4.301555
1.661092	176.293265	4.306560
1.632356	167.066113	4.311565
1.398684	174.168450	4.316570
1.617954	164.077009	4.321574
1.290528	162.952597	4.326579
1.447317	172.866924	4.331584
1.741649	172.843085	4.336589
1.550830	176.277408	4.341594
1.256174	166.021764	4.346598
1.564453	167.519793	4.351603
1.188918	170.050257	4.356608
1.926919	171.666890	4.361613
1.602784	172.255556	4.366618
1.869581	172.790992	4.371622
1.680698	181.587475	4.376627
1.201425	166.768246	4.381632
1.838946	165.880476	4.386637
1.693938	181.584945	4.391642
1.844909	181.171920	4.396646
1.822126	178.559113	4.401651
1.538264	171.730897	4.406656
1.502610	171.071444	4.411661
1.415248	173.137048	4.416666
1.383998	175.376450	4.421670
1.525454	175.979684	4.426675
1.306619	174.959962	4.431680
1.720973	171.760450	4.436685
1.790635	179.040682	4.441690
1.663417	181.511720	4.446694
1.546854	180.280824	4.451699
1.490464	176.261895	4.456704
1.765848	173.359180	4.461709
1.770693	190.466048	4.466714
2.198755	186.918924	4.471718
1.960379	187.428611	4.476723
1.673449	191.629563	4.481728
1.941808	179.588999	4.486733
1.866115	185.990800	4.491738
1.591892	183.701970	4.496742
2.169682	193.870156	4.501747
1.866804	196.389731	4.506752
2.315397	188.537365	4.511757
1.810633	182.982932	4.516762
1.820159	190.125167	4.521766
2.231843	194.164415	4.526771
1.880873	200.632501	4.531776
1.983120	184.066904	4.536781
1.712795	194.696724	4.541786
2.328111	200.652947	4.546790
2.425291	198.146293	4.551795
2.092067	189.531542	4.556800
1.783950	182.121673	4.561805
2.045569	196.885970	4.566810
2.100201	197.902641	4.571814
2.454100	211.644237	4.576819
2.232907	203.985873	4.581824
2.131832	187.584702	4.586829
2.089608	185.392482	4.591834
1.804841	189.824543	4.596838
1.900901	196.354088	4.601843
2.581200	205.955279	4.606848
2.685072	195.222924	4.611853
1.986919	191.373019	4.616858
2.193988	190.516539	4.621862
1.898085	184.381176	4.626867
1.909222	213.012767	4.631872
2.317549	203.952705	4.636877
2.515020	208.384930	4.641882
2.529949	200.640554	4.646886
2.550184	207.829560	4.651891
2.260839	207.711127	4.656896
2.385879	211.171891	4.661901
1.764612	206.650508	4.666906
2.267366	208.946194	4.671910
2.543772	208.963616	4.676915
2.165433	213.506351	4.681920
2.745175	209.551779	4.686925
2.771538	215.433039	4.691930
2.493006	204.036084	4.696934
2.413700	203.150244	4.701939
2.189346	206.024793	4.706944
2.430990	205.746668	4.711949
2.181088	200.746401	4.716954
2.032470	209.476219	4.721958
2.566116	205.489054	4.726963
2.286109	213.237478	4.731968
2.239250	203.710412	4.736973
2.553253	213.767354	4.741978
2.270666	208.195519	4.746982
2.734357	204.908669	4.751987
2.923803	224.053915	4.756992
2.618509	210.131213	4.761997
2.632979	216.802791	4.767002
2.698729	204.166001	4.772006
2.524469	220.479208	4.777011
2.680330	211.380988	4.782016
2.691420	209.134517	4.787021
2.591827	213.779117	4.792026
3.050603	218.259474	4.797030
3.187120	206.564625	4.802035
2.848109	221.073582	4.807040
2.968080	206.689875	4.812045
2.772556	217.570518	4.817050
2.750845	208.547399	4.822054
2.707639	204.013998	4.827059
2.645012	210.719897	4.832064
2.808914	204.116594	4.837069
2.660784	208.916469	4.842074
2.541793	210.406194	4.847078
3.247184	208.157193	4.852083
2.695075	210.200595	4.857088
2.605375	200.812667	4.862093
2.897965	212.364403	4.867098
2.861280	207.524052	4.872102
2.794835	215.228495	4.877107
2.949676	207.357852	4.882112
2.657410	200.177994	4.887117
2.627237	211.314319	4.892122
2.891157	207.277858	4.897126
2.954442	203.801229	4.902131
2.730746	209.506196	4.907136
2.776555	204.747643	4.912141
2.505219	207.335582	4.917146
2.645235	215.225338	4.922150
2.897177	215.299120	4.927155
2.666573	224.451445	4.932160
3.214977	228.737533	4.937165
3.108170	244.949176	4.942170
3.056476	234.771698	4.947174
2.869825	232.527307	4.952179
3.068952	237.323738	4.957184
3.460153	235.389212	4.962189
3.052992	223.294544	4.967194
2.811287	220.549203	4.972198
3.333948	227.147959	4.977203
3.201713	228.922071	4.982208
3.115223	229.666400	4.987213
2.897057	225.396110	4.992218
2.847639	228.361564	4.997222
3.174473	235.889944	5.002227
2.951711	243.370364	5.007232
3.302195	233.571220	5.012237
3.273475	241.549617	5.017242
3.405459	237.041551	5.022246
3.430996	233.644794	5.027251
3.083245	239.380061	5.032256
3.385014	232.239582	5.037261
3.230914	248.317404	5.042266
3.063223	229.788968	5.047270
2.994426	233.717862	5.052275
2.819785	237.526611	5.057280
3.142009	238.319630	5.062285
3.062863	235.595020	5.067290
3.045110	232.060617	5.072294
3.372509	244.476233	5.077299
3.344781	239.783764	5.082304
3.481865	231.378923	5.087309
3.432544	230.366738	5.092314
3.541085	241.278553	5.097318
3.519514	228.214430	5.102323
3.424874	232.372183	5.107328
3.557927	229.756356	5.112333
3.461821	228.478249	5.117338
3.323682	228.030397	5.122342
3.429461	234.192489	5.127347
3.508595	238.607885	5.132352
3.903765	242.148668	5.137357
3.646625	235.349725	5.142362
3.602474	230.651701	5.147366
3.624027	224.358378	5.152371
3.224406	246.146160	5.157376
3.282013	222.554626	5.162381
3.049051	248.360805	5.167386
3.555159	248.771219	5.172390
3.649921	258.225669	5.177395
3.424866	254.183645	5.182400
3.854123	260.000323	5.187405
3.922640	260.081308	5.192410
3.922478	272.330972	5.197414
3.991166	259.711013	5.202419
3.696146	254.148924	5.207424
3.743307	253.405452	5.212429
3.386504	257.219621	5.217434
3.716657	247.914614	5.222438
3.937268	250.473676	5.227443
3.877496	265.934171	5.232448
4.106151	257.261904	5.237453
3.767525	249.808135	5.242458
3.688652	241.881799	5.247462
3.628447	234.069974	5.252467
3.673412	251.968056	5.257472
3.877215	254.148075	5.262477
4.126759	256.901832	5.267482
4.124126	256.622474	5.272486
3.717421	241.280415	5.277491
3.392875	246.314455	5.282496
3.952533	236.742205	5.287501
3.666743	256.759758	5.292506
4.155231	253.558366	5.297510
4.087666	259.130051	5.302515
3.678679	267.985861	5.307520
4.057621	248.575043	5.312525
4.138175	261.368154	5.317530
3.839010	263.043526	5.322534
4.138462	251.120282	5.327539
3.800088	264.022099	5.332544
4.202525	254.001386	5.337549
4.114990	257.286150	5.342554
4.025239	254.994274	5.347558
4.479468	256.798190	5.352563
4.095267	261.280740	5.357568
4.218721	242.577603	5.362573
3.728363	243.585012	5.367578
3.989607	256.049324	5.372582
4.034524	257.111422	5.377587
4.097952	261.394263	5.382592
4.361524	257.570770	5.387597
4.007052	254.022276	5.392602
4.192179	259.931628	5.397606
4.166488	262.681209	5.402611
3.883296	262.807629	5.407616
4.055917	260.226266	5.412621
4.432857	269.373144	5.417626
4.407706	257.585150	5.422630
4.416988	266.054323	5.427635
4.307583	262.272300	5.432640
4.508311	259.860115	5.437645
4.291048	257.729736	5.442650
4.097611	254.597684	5.447654
4.371393	250.937662	5.452659
4.152476	252.590223	5.457664
4.513789	253.189280	5.462669
4.373836	258.359388	5.467674
4.202519	256.171644	5.472678
4.524111	257.608270	5.477683
4.111056	257.628798	5.482688
4.070232	245.657136	5.487693
4.224428	253.123448	5.492698
4.041732	252.862179	5.497702
4.027178	257.561921	5.502707
3.931415	251.297559	5.507712
3.931970	268.204145	5.512717
4.403496	281.450088	5.517722
4.360979	286.402533	5.522726
4.796250	284.066997	5.527731
4.615003	288.947585	5.532736
4.944271	286.731294	5.537741
4.815533	287.034110	5.542746
4.445147	273.456057	5.547750
4.569695	256.923380	5.552755
4.071280	271.413098	5.557760
4.487297	273.681377	5.562765
4.750659	290.915685	5.567770
4.578594	288.903491	5.572774
4.735240	288.829524	5.577779
4.506822	296.261180	5.582784
4.793509	293.470426	5.587789
4.956464	299.791760	5.592794
4.605649	290.381664	5.597798
4.897338	291.818330	5.602803
4.813367	285.235078	5.607808
4.702960	274.354369	5.612813
4.166648	278.938378	5.617818
4.425037	286.159271	5.622822
4.933041	279.236091	5.627827
4.726889	293.772366	5.632832
5.035698	293.518003	5.637837
5.104511	287.091296	5.642842
4.459242	293.394428	5.647846
5.140332	288.093954	5.652851
4.992852	302.116102	5.657856
5.042203	276.038871	5.662861
4.547084	269.896726	5.667866
4.703879	276.617094	5.672870
4.744759	283.795995	5.677875
4.721685	293.109028	5.682880
4.999568	290.577257	5.687885
4.964828	299.379563	5.692890
4.903042	297.470791	5.697894
4.729650	298.426506	5.702899
4.561822	303.713742	5.707904
4.875177	295.615230	5.712909
4.737841	292.354065	5.717914
4.727834	299.737383	5.722918
4.905487	297.508206	5.727923
4.808955	298.789966	5.732928
5.034986	288.352185	5.737933
4.799439	294.459936	5.742938
4.872380	291.668005	5.747942
4.849741	292.666348	5.752947
4.952594	306.134812	5.757952
5.427858	314.359615	5.762957
4.834057	305.218607	5.767962
4.883637	315.168014	5.772966
5.123368	315.560941	5.777971
5.092732	318.464485	5.782976
5.276055	318.175924	5.787981
5.171277	315.676574	5.792986
5.352400	320.635468	5.797990
5.456955	315.573091	5.802995
5.460280	305.946255	5.808000
5.189443	301.070993	5.813005
5.267082	300.415199	5.818010
5.153767	296.812995	5.823014
4.975606	293.825015	5.828019
5.113503	314.501957	5.833024
5.277772	314.683848	5.838029
5.102249	312.806016	5.843034
5.310603	325.642466	5.848038
5.317715	319.530684	5.853043
5.175682	325.619746	5.858048
5.285187	318.161511	5.863053
5.452844	318.954375	5.868058
5.393936	321.618714	5.873062
5.402332	318.029428	5.878067
5.362334	321.717152	5.883072
5.255572	317.438185	5.888077
5.331209	319.177559	5.893082
5.104424	314.561370	5.898086
5.652591	320.494861	5.903091
5.208131	319.915191	5.908096
5.392219	315.595380	5.913101
5.840566	308.129570	5.918106
5.651408	324.037277	5.923110
5.895042	323.943523	5.928115
5.714738	324.839610	5.933120
5.496808	311.912049	5.938125
5.279195	319.881824	5.943130
5.407505	323.496582	5.948134
5.698868	317.451810	5.953139
5.118555	322.012557	5.958144
5.296170	319.522903	5.963149
5.439746	323.618985	5.968154
5.475979	329.223367	5.973158
5.414885	324.990285	5.978163
5.472338	327.159515	5.983168
5.415079	318.073766	5.988173
5.735210	324.279396	5.993178
5.550525	327.984461	5.998182
5.806281	323.881248	6.003187
5.456050	328.261083	6.008192
5.682283	338.897068	6.013197
5.578569	342.125537	6.018202
5.537445	351.346688	6.023206
5.866357	344.887183	6.028211
5.766038	354.776086	6.033216
5.970054	346.108259	6.038221
5.879707	342.164195	6.043226
5.216004	339.700318	6.048230
5.558332	342.586274	6.053235
5.680108	352.272697	6.058240
5.929783	346.215701	6.063245
5.671945	353.868948	6.068250
5.510181	355.072558	6.073254
6.064131	355.755632	6.078259
5.754021	353.269487	6.083264
5.964770	350.990599	6.088269
5.484621	346.731654	6.093274
5.784215	354.061959	6.098278
5.958914	332.379337	6.103283
5.475968	337.464600	6.108288
5.798877	320.315961	6.113293
5.857084	334.107012	6.118298
5.437320	331.525038	6.123302
5.863636	332.233469	6.128307
5.626223	342.442927	6.133312
5.801518	328.474178	6.138317
5.690605	328.250113	6.143322
5.346435	337.486304	6.148326
5.873857	334.329731	6.153331
5.946095	348.558121	6.158336
5.855934	342.100588	6.163341
5.889396	324.143628	6.168346
5.456652	328.466335	6.173350
5.634190	316.840952	6.178355
5.278661	330.842849	6.183360
5.952517	339.699079	6.188365
5.964036	352.117952	6.193370
5.657169	334.825730	6.198374
5.765437	330.200219	6.203379
5.440957	323.322248	6.208384
5.657636	331.841642	6.213389
5.452930	328.232520	6.218394
6.125765	348.207083	6.223398
5.975801	337.913264	6.228403
5.476606	326.775092	6.233408
5.528245	332.968324	6.238413
5.941419	346.888247	6.243418
5.633100	333.392177	6.248422
5.689333	334.858511	6.253427
5.457370	340.639887	6.258432
5.909951	336.331880	6.263437
5.527586	347.918747	6.268442
5.587419	352.863674	6.273446
6.121404	356.357730	6.278451
5.529031	351.110838	6.283456
5.785216	346.676027	6.288461
5.991176	349.740742	6.293466
5.327196	344.823462	6.298470
5.731128	337.967479	6.303475
5.909852	349.752746	6.308480
6.034708	341.371189	6.313485
5.644530	328.102836	6.318490
5.273454	330.562926	6.323494
5.609220	339.562375	6.328499
5.377414	348.296626	6.333504
5.953834	348.436060	6.338509
6.025079	354.915333	6.343514
6.029777	350.548172	6.348518
5.726093	331.305965	6.353523
5.377917	337.358059	6.358528
5.665459	331.677996	6.363533
5.765293	342.383340	6.368538
5.550533	337.734361	6.373542
5.972204	344.204322	6.378547
5.489816	337.914006	6.383552
5.763219	348.552814	6.388557
5.874799	350.075860	6.393562
5.646480	330.234455	6.398566
5.536712	330.509847	6.403571
5.941724	342.757144	6.408576
5.546368	338.291708	6.413581
5.719577	342.797663	6.418586
5.979409	347.196673	6.423590
6.175370	334.780065	6.428595
5.762942	322.677511	6.433600
5.627306	324.496008	6.438605
5.754245	330.188717	6.443610
5.236732	330.215557	6.448614
5.476596	328.174355	6.453619
5.631364	336.371140	6.458624
5.923113	339.952026	6.463629
5.947380	334.014197	6.468634
5.819207	338.563931	6.473638
5.517329	316.905094	6.478643
5.439360	335.048666	6.483648
5.655735	318.821523	6.488653
5.839739	329.625348	6.493658
5.882438	334.367298	6.498662
5.669328	329.451252	6.503667
5.761681	323.732201	6.508672
5.707688	321.183561	6.513677
5.625339	326.501195	6.518682
5.437865	334.114123	6.523686
5.936992	331.072365	6.528691
5.646635	333.436750	6.533696
5.897120	336.363230	6.538701
6.010044	330.425664	6.543706
5.791103	323.813917	6.548710
5.776757	325.009400	6.553715
5.834325	336.577797	6.558720
5.914280	321.564629	6.563725
6.049533	328.698462	6.568730
5.711043	325.817637	6.573734
5.684935	326.646062	6.578739
5.592331	327.718393	6.583744
5.440056	324.436616	6.588749
5.564021	322.829079	6.593754
5.495044	326.710863	6.598758
5.695156	318.213802	6.603763
5.709013	333.471503	6.608768
5.675295	323.495811	6.613773
5.520310	329.424820	6.618778
5.276066	330.841050	6.623782
5.955011	327.837485	6.628787
5.805470	328.070154	6.633792
5.862555	328.883765	6.638797
5.799636	320.713596	6.643802
5.597695	323.444334	6.648806
5.735136	317.053173	6.653811
5.636670	325.731307	6.658816
5.641932	327.848235	6.663821
5.688859	317.887164	6.668826
5.881995	329.532281	6.673830
5.908009	318.075149	6.678835
5.538820	323.101045	6.683840
5.765531	328.226019	6.688845
5.709387	317.449135	6.693850
5.523133	329.914875	6.698854
5.638213	321.986057	6.703859
5.659150	322.688658	6.708864
5.575814	318.651477	6.713869
5.625300	325.554871	6.718874
5.741102	337.591136	6.723878
6.055311	334.263788	6.728883
5.237185	330.297628	6.733888
5.516026	349.287274	6.738893
6.012497	348.676908	6.743898
5.678996	354.190019	6.748902
6.082675	337.826743	6.753907
5.576891	337.629436	6.758912
5.887258	330.550827	6.763917
5.753105	325.656389	6.768922
5.521427	328.453245	6.773926
5.515547	324.796670	6.778931
5.552891	322.975414	6.783936
6.019002	340.604094	6.788941
5.622575	326.912711	6.793946
5.515072	325.671220	6.798950
5.806665	329.489719	6.803955
5.764594	353.866633	6.808960
5.854549	343.484190	6.813965
5.955754	332.647991	6.818970
5.535301	331.110618	6.823974
5.512135	327.163284	6.828979
5.485058	335.841398	6.833984
6.156223	345.584106	6.838989
5.952896	341.480036	6.843994
5.592358	338.502035	6.848998
5.763421	321.053232	6.854003
5.884363	332.321604	6.859008
5.577404	322.508151	6.864013
5.735505	324.379648	6.869018
5.379141	334.860670	6.874022
5.735401	328.124504	6.879027
5.702823	325.993215	6.884032
5.376141	327.557925	6.889037
5.799981	337.441982	6.894042
5.952884	346.231280	6.899046
5.949630	333.810094	6.904051
5.697409	335.826162	6.909056
5.818389	329.488249	6.914061
5.534638	326.628319	6.919066
5.485017	325.750957	6.924070
5.933022	324.867250	6.929075
5.840687	333.508257	6.934080
5.863244	336.541096	6.939085
5.895090	333.796837	6.944090
5.694423	336.192688	6.949094
5.677657	323.504593	6.954099
5.583887	336.553083	6.959104
5.567380	337.831609	6.964109
5.606262	325.064013	6.969114
5.581886	334.117400	6.974118
5.838773	330.533773	6.979123
5.635070	333.061947	6.984128
5.716494	329.224903	6.989133
5.717703	325.356991	6.994138
5.456646	332.784815	6.999142
5.712468	327.304400	7.004147
5.587587	328.463398	7.009152
5.841881	329.764992	7.014157
5.676528	335.129972	7.019162
5.927575	336.566688	7.024166
5.910597	331.858986	7.029171
5.629286	331.365269	7.034176
5.932846	328.218675	7.039181
5.557424	328.647742	7.044186
5.545340	333.116019	7.049190
5.436305	331.643507	7.054195
5.634568	332.967834	7.059200
5.957260	342.312620	7.064205
6.023409	333.860511	7.069210
5.629068	330.089522	7.074214
5.869719	328.452920	7.079219
5.667168	321.258487	7.084224
5.480558	324.052389	7.089229
5.639927	318.258462	7.094234
5.549309	328.765757	7.099238
5.659683	319.034097	7.104243
5.415944	336.275783	7.109248
5.992088	342.896879	7.114253
6.100726	339.944297	7.119258
5.296085	331.498201	7.124262
5.857228	331.811459	7.129267
5.532577	324.874120	7.134272
5.954264	326.214195	7.139277
5.805302	320.783500	7.144282
5.684855	326.073130	7.149286
5.649122	321.702633	7.154291
5.679311	323.381679	7.159296
5.194426	327.896376	7.164301
5.941366	333.225355	7.169306
5.806318	345.320884	7.174310
6.193002	336.522061	7.179315
6.098501	327.066971	7.184320
5.937665	323.672756	7.189325
6.199051	319.655434	7.194330
5.585862	328.717492	7.199334
5.927053	323.753715	7.204339
5.595991	338.654352	7.209344
5.534434	325.869705	7.214349
5.944341	323.681249	7.219354
5.952240	323.078486	7.224358
5.655314	327.099785	7.229363
5.522344	327.431919	7.234368
5.595751	320.744941	7.239373
5.588242	324.343202	7.244378
5.789018	323.774684	7.249382
5.966662	322.518555	7.254387
5.971795	316.215690	7.259392
5.954236	321.639768	7.264397
6.083352	313.185294	7.269402
6.002859	316.646698	7.274406
5.223867	304.439722	7.279411
5.553341	322.971593	7.284416
5.444056	327.939096	7.289421
5.810229	329.794164	7.294426
5.636166	322.512116	7.299430
5.725625	326.601406	7.304435
5.925122	335.309743	7.309440
5.693771	334.420751	7.314445
5.845436	329.132091	7.319450
5.809704	332.418324	7.324454
6.052934	325.916434	7.329459
5.718017	316.026133	7.334464
5.521013	313.508961	7.339469
5.487369	312.354650	7.344474
5.705809	324.269061	7.349478
5.818859	322.606703	7.354483
5.908957	329.238133	7.359488
5.563797	323.700928	7.364493
5.836354	316.477059	7.369498
5.558937	319.974154	7.374502
6.045139	315.139211	7.379507
5.204498	315.294746	7.384512
5.325196	320.551396	7.389517
5.705531	326.793196	7.394522
5.616192	332.171193	7.399526
6.064376	321.444470	7.404531
5.839827	326.840401	7.409536
5.579416	327.544181	7.414541
5.989343	322.134255	7.419546
5.625829	338.663352	7.424550
6.015727	327.544344	7.429555
5.679559	316.358758	7.434560
5.465287	314.480460	7.439565
5.893587	304.526061	7.444570
5.662028	321.180811	7.449574
5.476274	306.724494	7.454579
5.537969	325.121106	7.459584
5.896167	325.977809	7.464589
5.974086	331.918624	7.469594
5.513953	333.706599	7.474598
5.805494	322.286434	7.479603
5.581312	327.127008	7.484608
5.658275	328.133661	7.489613
5.914866	325.000202	7.494618
5.635233	336.959521	7.499622
5.456151	328.986256	7.504627
5.425196	328.224585	7.509632
5.750029	330.496386	7.514637
5.552151	332.814024	7.519642
5.687544	324.101770	7.524646
5.752351	331.401628	7.529651
5.702115	341.986481	7.534656
5.440614	335.408246	7.539661
5.982391	320.713181	7.544666
5.966809	327.609237	7.549670
6.252715	326.004382	7.554675
5.974930	322.082598	7.559680
5.797847	313.631264	7.564685
5.693973	304.657660	7.569690
5.467752	295.997043	7.574694
5.609563	300.213192	7.579699
5.394910	315.185033	7.584704
5.576667	322.055587	7.589709
5.870158	319.805771	7.594714
5.520805	326.684093	7.599718
5.616769	327.937412	7.604723
5.456220	328.577037	7.609728
5.842963	326.067817	7.614733
5.662253	318.645387	7.619738
5.649340	332.985004	7.624742
5.723744	322.553458	7.629747
5.639120	330.040164	7.634752
6.109226	328.215647	7.639757
5.957558	327.841870	7.644762
5.919021	326.444863	7.649766
5.989816	320.204884	7.654771
5.488269	307.207450	7.659776
5.384454	318.883959	7.664781
5.595258	316.202506	7.669786
5.487148	331.516195	7.674790
5.569832	327.682692	7.679795
5.630251	333.016459	7.684800
5.561051	331.812212	7.689805
5.847215	328.540242	7.694810
5.531760	332.238036	7.699814
5.686090	331.845760	7.704819
5.970674	326.818970	7.709824
5.692530	323.122205	7.714829
5.652812	327.661970	7.719834
5.664353	328.241614	7.724838
5.716244	328.309774	7.729843
5.954533	328.655383	7.734848
5.642806	327.661154	7.739853
5.906107	327.761268	7.744858
5.725027	329.514502	7.749862
5.836582	312.569525	7.754867
5.776631	327.343392	7.759872
5.886498	319.017619	7.764877
5.982833	315.880606	7.769882
5.457490	313.091817	7.774886
5.964901	324.941029	7.779891
5.702154	315.782877	7.784896
5.631399	313.742789	7.789901
5.619290	306.443103	7.794906
5.866547	312.665380	7.799910
5.591415	306.956505	7.804915
5.492498	315.998196	7.809920
5.689952	321.739763	7.814925
6.000319	318.809894	7.819930
5.892865	324.832233	7.824934
5.816373	311.063809	7.829939
5.548975	311.825977	7.834944
5.278962	296.767008	7.839949
5.590225	315.131598	7.844954
5.815567	326.798987	7.849958
5.787950	334.699104	7.854963
5.648938	324.723548	7.859968
5.693010	330.894356	7.864973
5.965012	332.169525	7.869978
5.820646	334.771112	7.874982
6.067413	318.444198	7.879987
5.565758	311.989559	7.884992
5.214430	307.184505	7.889997
5.215012	312.244051	7.895002
5.625190	334.531388	7.900006
5.867143	327.091587	7.905011
6.106282	335.722492	7.910016
5.727458	327.585685	7.915021
5.608010	326.256590	7.920026
5.720636	332.575253	7.925030
5.868730	338.441457	7.930035
5.693405	333.389481	7.935040
5.748404	343.107520	7.940045
6.044613	322.062626	7.945050
5.695163	322.387526	7.950054
5.351412	306.419652	7.955059
5.670304	319.607132	7.960064
5.824469	320.103081	7.965069
5.806929	329.966763	7.970074
5.442192	325.375276	7.975078
6.077451	324.109981	7.980083
5.236041	318.409977	7.985088
5.504447	323.536701	7.990093
5.757348	328.225950	7.995098
5.371034	327.929063	8.000102
5.708108	326.012402	8.005107
5.508299	326.469704	8.010112
5.580126	344.297053	8.015130
6.018766	327.866803	8.020147
5.755195	332.135983	8.025165
5.560761	321.402316	8.030182
5.647855	326.810329	8.035200
5.920144	331.689187	8.040218
5.968029	328.078868	8.045235
5.973264	329.892988	8.050253
6.154620	323.604659	8.055270
5.766087	321.479725	8.060288
5.592185	334.695470	8.065306
5.782201	334.698354	8.070323
5.937867	340.917329	8.075341
5.829191	333.597984	8.080358
5.759460	323.285078	8.085376
5.669958	339.108573	8.090394
5.870488	325.726450	8.095411
6.024644	339.008328	8.100429
5.401144	326.260167	8.105446
5.723446	326.968546	8.110464
5.480832	335.767828	8.115482
6.004463	324.549883	8.120499
5.818261	338.261326	8.125517
5.728458	324.625721	8.130534
5.777862	333.672103	8.135552
5.407413	318.470326	8.140570
6.202143	332.832807	8.145587
5.600979	330.797539	8.150605
5.757519	326.460966	8.155622
5.931603	327.689402	8.160640
5.586926	330.407855	8.165658
5.913375	332.790765	8.170675
5.674291	328.602421	8.175693
5.728361	331.533111	8.180710
6.178709	323.143395	8.185728
6.058495	332.987968	8.190746
6.200595	318.387148	8.195763
5.648492	334.630800	8.200781
5.775058	328.290755	8.205798
6.131278	331.713490	8.210816
5.686514	333.313264	8.215834
5.734452	333.442902	8.220851
5.730243	327.288357	8.225869
5.947137	340.352743	8.230886
5.837363	327.059003	8.235904
5.671624	334.907415	8.240922
5.572761	321.949627	8.245939
5.593577	341.530773	8.250957
5.719832	342.026488	8.255974
6.147127	353.288576	8.260992
6.248751	355.141397	8.266010
6.602052	357.579291	8.271027
6.073960	339.349283	8.276045
5.648812	328.414024	8.281062
5.884510	330.491579	8.286080
5.728612	338.390123	8.291098
6.208107	347.261887	8.296115
6.027993	346.657266	8.301133
5.913990	349.635972	8.306150
6.261382	346.385273	8.311168
6.163760	343.640978	8.316186
5.770375	339.320027	8.321203
5.771000	339.526616	8.326221
6.280882	350.415169	8.331238
6.151642	339.881853	8.336256
5.760988	336.197391	8.341274
6.163694	342.704995	8.346291
6.361176	348.583003	8.351309
6.376377	343.253683	8.356326
6.104505	340.367306	8.361344
6.050105	336.742296	8.366362
6.212904	329.289453	8.371379
5.829280	336.595599	8.376397
5.976047	338.156692	8.381414
6.078764	328.486703	8.386432
5.928472	342.211076	8.391450
5.664324	334.307005	8.396467
5.829354	345.751641	8.401485
5.964777	354.633753	8.406502
6.142751	355.697389	8.411520
6.222770	362.914476	8.416538
6.281070	364.529052	8.421555
6.472768	356.254743	8.426573
6.223754	362.337664	8.431590
6.341874	342.378361	8.436608
5.928863	344.560594	8.441626
6.078166	348.963691	8.446643
6.361697	360.043008	8.451661
6.057084	361.252794	8.456678
6.395402	355.201525	8.461696
6.129222	353.875260	8.466714
6.094810	338.742006	8.471731
6.069349	349.829175	8.476749
6.119820	351.212791	8.481766
6.566502	350.606339	8.486784
6.327656	361.015277	8.491802
5.685034	341.274538	8.496819
5.865121	352.183267	8.501837
5.766834	353.947479	8.506854
5.785505	358.638406	8.511872
6.070607	355.559853	8.516890
6.587035	359.397653	8.521907
6.238941	359.651576	8.526925
6.318945	361.799300	8.531942
6.803849	355.795312	8.536960
6.253353	359.735654	8.541978
6.528158	351.892174	8.546995
6.385008	358.295652	8.552013
6.026971	369.479645	8.557030
6.299940	361.871284	8.562048
6.327153	370.487167	8.567066
6.354629	355.470566	8.572083
6.309581	366.636388	8.577101
6.341956	362.339536	8.582119
6.399101	354.565103	8.587136
6.020226	362.949692	8.592154
6.407934	360.039104	8.597171
6.527148	358.153949	8.602189
6.609266	361.554738	8.607207
6.539098	355.722137	8.612224
6.474909	363.109635	8.617242
6.749675	360.417012	8.622259
6.299062	350.826384	8.627277
6.193394	354.226300	8.632295
6.458530	352.757202	8.637312
6.155323	358.201558	8.642330
6.373554	360.330243	8.647347
6.357844	357.279644	8.652365
5.972106	361.740774	8.657383
6.154123	359.224575	8.662400
6.108718	365.520087	8.667418
6.059473	365.223207	8.672435
6.105384	361.103220	8.677453
5.867302	368.127341	8.682471
6.619437	368.738100	8.687488
6.204492	360.482346	8.692506
6.378461	381.935728	8.697523
6.824749	389.247248	8.702541
6.407760	378.040939	8.707559
6.344106	364.885156	8.712576
6.493690	366.315679	8.717594
6.347329	362.626625	8.722611
6.436406	366.622064	8.727629
6.359295	386.903923	8.732647
6.612051	382.552523	8.737664
6.524908	383.661998	8.742682
6.589385	377.510188	8.747699
6.633597	372.144346	8.752717
6.451549	361.739071	8.757735
6.293134	361.673701	8.762752
6.444374	365.368679	8.767770
6.663028	377.996825	8.772787
6.585331	377.523983	8.777805
6.335857	381.119838	8.782823
6.927215	378.682039	8.787840
6.346515	370.461311	8.792858
6.373965	375.854256	8.797875
6.677361	384.842311	8.802893
6.368116	390.205406	8.807911
6.871466	392.217618	8.812928
6.647049	382.671648	8.817946
6.409970	378.308369	8.822963
6.606446	383.164022	8.827981
6.509044	382.631863	8.832999
6.927516	388.488310	8.838016
6.782402	375.271656	8.843034
6.612869	371.680930	8.848051
6.409589	365.437817	8.853069
6.723518	381.701138	8.858087
6.894384	373.164955	8.863104
6.336827	370.298501	8.868122
6.433032	377.178883	8.873139
6.901056	378.292725	8.878157
6.572130	385.786435	8.883175
6.741085	383.009831	8.888192
6.773113	381.784180	8.893210
6.399724	382.492262	8.898227
6.788226	383.471896	8.903245
6.890575	389.636570	8.908263
6.537482	376.460192	8.913280
6.622493	381.524313	8.918298
6.683848	380.419759	8.923315
7.082657	382.333609	8.928333
6.436483	383.883605	8.933351
6.804400	373.723687	8.938368
6.737509	391.888123	8.943386
6.968435	387.195306	8.948403
6.763330	376.396058	8.953421
6.656726	365.935528	8.958439
6.502600	359.371090	8.963456
6.588728	373.246332	8.968474
6.700066	380.431059	8.973491
6.758278	378.678077	8.978509
6.793027	383.195687	8.983527
6.999581	380.422282	8.988544
6.899235	383.394591	8.993562
6.632701	385.468042	8.998579
7.134325	384.049584	9.003597
6.687768	388.043713	9.008615
6.670832	387.805039	9.013632
6.748282	379.500499	9.018650
6.213902	381.936744	9.023667
6.734944	379.419697	9.028685
6.536812	374.288408	9.033703
6.935895	381.196788	9.038720
6.605885	382.374777	9.043738
6.662597	386.396465	9.048755
6.695113	382.840454	9.053773
6.317397	393.285880	9.058791
6.498119	385.412159	9.063808
6.820462	402.293136	9.068826
6.595840	408.654277	9.073843
7.624377	407.721212	9.078861
7.035546	402.905615	9.083879
6.774234	397.384072	9.088896
6.650767	397.197550	9.093914
6.622673	406.864275	9.098931
6.920224	405.295108	9.103949
6.958285	414.025540	9.108967
7.193467	409.885301	9.113984
7.024144	411.705809	9.119002
7.250829	422.669435	9.124019
7.084130	404.600126	9.129037
6.777515	384.335223	9.134055
7.011451	394.177460	9.139072
7.304667	382.947186	9.144090
6.767172	393.601238	9.149107
6.966690	381.755106	9.154125
6.756878	393.682513	9.159143
7.077146	405.752901	9.164160
7.238279	406.872483	9.169178
6.935648	401.576486	9.174195
6.815445	386.578298	9.179213
7.165789	408.137230	9.184231
7.065402	412.127168	9.189248
6.951145	415.491127	9.194266
6.889279	424.131688	9.199283
7.096566	409.744138	9.204301
6.903019	414.531767	9.209319
7.483613	422.995273	9.214336
7.313049	412.374297	9.219354
6.893188	403.926442	9.224371
6.891359	404.031876	9.229389
6.583890	415.614937	9.234407
7.217232	417.673846	9.239424
7.680661	423.524605	9.244442
7.172152	418.266167	9.249459
7.214211	399.614582	9.254477
7.008080	401.826208	9.259495
7.060122	406.877315	9.264512
6.953622	411.536313	9.269530
6.996801	422.695582	9.274547
7.170337	421.890064	9.279565
7.257918	426.562275	9.284583
6.899572	431.527287	9.289600
7.405966	422.246398	9.294618
6.986290	428.475811	9.299635
7.320489	425.166271	9.304653
7.098860	426.991342	9.309671
7.151456	432.475984	9.314688
7.064436	419.075834	9.319706
6.807138	429.433560	9.324723
7.190737	421.293642	9.329741
7.230686	429.071893	9.334759
6.926052	427.765989	9.339776
7.132261	415.965761	9.344794
6.870401	424.005965	9.349811
7.251521	429.489146	9.354829
7.291061	431.203098	9.359847
7.262759	427.499326	9.364864
7.215157	422.484522	9.369882
7.298847	438.462188	9.374899
7.513916	426.923446	9.379917
7.626525	430.592384	9.384935
7.443516	423.551073	9.389952
7.481025	425.159269	9.394970
7.217186	435.561389	9.399987
7.318151	426.318558	9.405005
7.133621	428.901758	9.410023
7.187123	432.693895	9.415040
7.239396	423.390859	9.420058
7.265402	424.287848	9.425075
7.249284	424.083089	9.430093
7.066865	427.605610	9.435111
7.027027	432.468474	9.440128
7.299921	422.430607	9.445146
7.159983	429.058952	9.450163
7.479524	436.184692	9.455181
7.378443	438.042085	9.460199
7.292190	446.077716	9.465216
7.810278	448.997437	9.470234
7.542918	441.817003	9.475251
7.130414	425.404119	9.480269
7.169160	437.231982	9.485287
7.553622	434.151465	9.490304
7.536371	429.935079	9.495322
7.376316	432.988969	9.500339
7.438255	434.819855	9.505357
7.279319	452.092269	9.510375
7.439224	451.253979	9.515392
7.547788	445.138511	9.520410
7.665824	453.951923	9.525427
7.694297	439.653706	9.530445
7.564971	429.566165	9.535463
7.067044	429.915262	9.540480
7.286501	435.916803	9.545498
7.314159	444.813926	9.550515
7.683154	452.756177	9.555533
7.747139	451.486826	9.560551
7.252535	464.306818	9.565568
7.561082	452.443297	9.570586
7.693719	454.410846	9.575603
8.041341	454.637313	9.580621
7.982353	448.095799	9.585639
7.319154	437.243726	9.590656
7.167221	423.536086	9.595674
7.567304	444.209721	9.600691
7.624988	451.532520	9.605709
7.908726	448.298285	9.610727
7.316413	442.391234	9.615744
7.098977	442.954708	9.620762
6.983920	444.984290	9.625779
7.385437	444.704996	9.630797
7.344303	448.985066	9.635815
7.551325	458.552514	9.640832
7.916197	443.779521	9.645850
7.381857	457.288723	9.650867
7.664681	456.076886	9.655885
7.536356	448.609979	9.660903
7.283706	451.605451	9.665920
7.842191	438.828631	9.670938
7.704598	452.086665	9.675955
7.670010	446.767553	9.680973
7.916037	454.523965	9.685991
7.992882	455.411522	9.691008
7.786205	447.947009	9.696026
7.527975	448.258037	9.701043
8.010678	447.503876	9.706061
7.934049	452.732669	9.711079
7.612990	452.121946	9.716096
7.816147	442.720204	9.721114
7.913485	441.839169	9.726131
8.096721	437.477658	9.731149
8.429689	446.858629	9.736167
7.779789	446.408066	9.741184
8.020156	448.735821	9.746202
7.753157	445.783463	9.751219
7.624186	447.887595	9.756237
8.010069	450.293713	9.761255
7.865106	451.167944	9.766272
7.670168	445.013364	9.771290
7.678645	440.642320	9.776307
7.792216	444.764010	9.781325
7.997506	443.270405	9.786343
7.685994	451.109447	9.791360
7.939267	439.930649	9.796378
7.681740	449.996131	9.801395
7.640167	444.439425	9.806413
7.920273	442.252939	9.811431
7.767886	447.692335	9.816448
7.915567	440.869646	9.821466
8.045775	444.289032	9.826483
7.813476	458.777854	9.831501
8.298621	447.642392	9.836519
7.898794	446.071626	9.841536
8.375135	447.002416	9.846554
8.118960	450.245497	9.851571
7.387374	431.298489	9.856589
8.012882	436.639880	9.861607
7.989991	441.604644	9.866624
7.883258	438.023148	9.871642
8.530034	446.151289	9.876659
8.021452	440.681065	9.881677
7.644623	424.317955	9.886695
7.736614	439.812399	9.891712
7.978032	437.683717	9.896730
7.722113	442.766733	9.901747
7.679640	453.850112	9.906765
8.111431	439.212247	9.911783
8.133571	454.878537	9.916800
8.235294	452.446135	9.921818
8.317209	447.562143	9.926835
7.944190	448.340238	9.931853
8.122583	446.543062	9.936871
7.802876	458.204559	9.941888
8.379726	451.658728	9.946906
8.480468	444.984377	9.951923
8.122095	446.485362	9.956941
8.004821	424.183419	9.961959
7.863033	443.799201	9.966976
8.001749	444.512316	9.971994
7.972956	437.415447	9.977011
7.909924	447.502926	9.982029
8.357807	443.812513	9.987047
8.307207	451.296407	9.992064
8.002875	445.072813	9.997082
7.723514	445.255082	10.002099
7.872691	455.580103	10.007117
8.053559	438.893593	10.012135
7.686959	453.179557	10.017152
7.925367	441.607991	10.022170
8.192958	456.156621	10.027187
7.969669	449.355633	10.032205
8.092644	448.139266	10.037223
8.217104	457.404325	10.042240
8.495380	457.674599	10.047258
8.370294	450.710057	10.052275
8.122986	449.109807	10.057293
8.023821	444.563955	10.062311
8.164271	452.834717	10.067328
8.002453	457.286999	10.072346
8.441349	463.393796	10.077363
8.085518	475.365415	10.082381
8.528508	473.677589	10.087399
8.657185	476.554571	10.092416
8.415318	463.528316	10.097434
8.380644	450.382405	10.102451
8.004327	456.792793	10.107469
8.453313	449.202963	10.112487
8.034310	449.316915	10.117504
8.337974	447.719172	10.122522
8.525035	450.294741	10.127539
8.254643	457.572477	10.132557
8.403311	447.983154	10.137575
8.021885	452.587280	10.142592
8.183926	458.060432	10.147610
8.566290	469.619613	10.152627
8.497384	473.331525	10.157645
8.742309	473.529004	10.162663
8.335232	471.804731	10.167680
8.062392	451.601835	10.172698
8.392031	474.619476	10.177715
8.258511	476.932616	10.182733
8.919245	470.599584	10.187751
8.414656	475.626906	10.192768
8.312456	461.356687	10.197786
8.712246	467.200917	10.202803
8.238320	461.097622	10.207821
8.790965	467.039859	10.212839
8.443826	463.614053	10.217856
8.220749	458.081014	10.222874
8.337759	463.995077	10.227891
8.409340	472.221790	10.232909
8.830116	470.140056	10.237927
8.678173	478.723776	10.242944
8.717973	464.449044	10.247962
8.400481	451.111975	10.252979
8.198793	452.956764	10.257997
8.626685	455.049630	10.263015
8.648655	478.610692	10.268032
8.469718	468.898069	10.273050
8.753349	478.240611	10.278067
8.474252	476.748192	10.283085
8.420681	486.505020	10.288103
8.463816	480.226414	10.293120
8.778529	486.714851	10.298138
9.009016	482.373226	10.303155
8.384326	478.094618	10.308173
8.840755	477.051150	10.313191
8.520499	476.813879	10.318208
8.676231	474.342577	10.323226
8.732381	477.943949	10.328243
8.547525	487.382868	10.333261
9.101431	470.092837	10.338279
8.404949	461.605700	10.343296
8.477424	474.206849	10.348314
8.735790	470.589462	10.353331
8.278546	489.178309	10.358349
8.731080	485.125927	10.363367
8.628626	484.607004	10.368384
8.629541	484.692496	10.373402
8.566976	481.660486	10.378419
8.557937	486.325549	10.383437
8.767931	484.708138	10.388455
8.525530	475.672532	10.393472
8.797452	488.115357	10.398490
8.744076	480.709395	10.403507
8.491830	483.727442	10.408525
8.677886	478.913917	10.413543
8.641619	479.320323	10.418560
8.628199	488.076478	10.423578
8.859591	478.544443	10.428595
8.535803	487.158896	10.433613
8.700367	480.854201	10.438631
8.859560	481.733583	10.443648
8.898060	485.978578	10.448666
8.983657	484.428493	10.453683
8.679953	482.026469	10.458701
8.868945	479.766154	10.463719
8.901306	478.672316	10.468736
8.642958	481.704761	10.473754
9.267084	486.601954	10.478771
8.774017	487.536803	10.483789
8.843958	492.838483	10.488807
9.004405	487.362739	10.493824
9.007921	503.239832	10.498842
9.315368	490.502727	10.503859
8.781022	487.783362	10.508877
8.518897	487.308891	10.513895
8.828506	497.075433	10.518912
8.860386	496.073792	10.523930
9.146806	487.825201	10.528947
9.245548	498.821170	10.533965
9.283660	492.832539	10.538983
8.951644	489.087511	10.544000
9.020104	482.630104	10.549018
8.949546	476.750676	10.554035
8.779646	479.124189	10.559053
9.226936	491.612270	10.564071
9.343013	486.527133	10.569088
8.678892	491.704981	10.574106
8.987763	480.629500	10.579123
9.040409	492.722000	10.584141
9.155082	500.903774	10.589159
9.716539	495.408220	10.594176
9.088686	487.643649	10.599194
9.146129	476.872535	10.604211
8.402279	486.367361	10.609229
8.792478	487.647677	10.614247
9.126603	492.095285	10.619264
8.921457	496.948641	10.624282
9.456411	495.962979	10.629299
9.400234	509.986395	10.634317
9.458986	498.187978	10.639335
9.260891	489.174919	10.644352
8.636229	491.217563	10.649370
9.361725	497.837708	10.654387
9.347993	494.654089	10.659405
9.352052	501.751201	10.664423
9.164367	496.062478	10.669440
9.106974	497.606345	10.674458
9.121576	504.006889	10.679475
9.269265	503.539294	10.684493
9.076465	500.826144	10.689511
9.008242	506.685192	10.694528
9.165851	494.687293	10.699546
9.319575	495.578214	10.704563
9.139044	502.283016	10.709581
9.110840	500.976627	10.714599
9.435558	498.354411	10.719616
9.296506	502.046890	10.724634
9.405074	501.337198	10.729651
9.026447	504.879358	10.734669
9.338320	506.123879	10.739687
9.454848	500.992801	10.744704
8.969525	495.604510	10.749722
9.225285	491.798592	10.754739
9.006021	501.494002	10.759757
8.985376	503.373857	10.764775
9.640033	500.523981	10.769792
9.473858	506.800651	10.774810
9.284842	502.809037	10.779827
9.185084	503.615527	10.784845
9.780933	508.393029	10.789863
10.020103	495.989286	10.794880
9.504305	503.991825	10.799898
9.751164	499.033555	10.804915
9.235081	503.331368	10.809933
9.247977	500.858215	10.814951
9.511148	489.962355	10.819968
9.378993	504.209595	10.824986
9.471775	503.867650	10.830003
9.267874	503.015228	10.835021
9.431220	499.512241	10.840039
9.833161	498.600257	10.845056
9.213760	501.897817	10.850074
9.184341	500.203674	10.855091
9.259181	507.631513	10.860109
9.676348	522.160068	10.865127
9.563566	517.556817	10.870144
9.511984	530.982693	10.875162
10.041066	520.120166	10.880179
9.466901	507.708700	10.885197
9.471283	503.177506	10.890215
9.524718	500.390164	10.895232
9.697079	509.645324	10.900250
9.860926	512.385574	10.905267
9.545585	505.970102	10.910285
9.602085	495.992760	10.915303
9.863997	495.279626	10.920320
9.337916	504.858728	10.925338
9.528599	519.452482	10.930355
9.754297	519.185089	10.935373
9.830888	529.370860	10.940391
9.912848	527.603284	10.945408
9.342524	520.194455	10.950426
9.942602	515.064095	10.955443
9.817656	519.660449	10.960461
9.313099	519.543566	10.965479
9.527971	524.540485	10.970496
9.941307	527.050113	10.975514
9.810766	521.983910	10.980531
9.708904	529.478922	10.985549
9.607762	531.746338	10.990567
9.904486	526.346739	10.995584
9.933802	527.639605	11.000602
9.667011	523.730197	11.005619
10.085522	532.085481	11.010637
9.584680	530.475989	11.015655
10.061980	517.548047	11.020672
9.920640	524.069786	11.025690
9.728235	519.483116	11.030707
10.033263	526.327674	11.035725
9.678824	529.819564	11.040743
9.806998	518.182806	11.045760
9.843316	530.826031	11.050778
9.558927	528.118848	11.055795
9.955346	527.936455	11.060813
9.758625	520.341917	11.065831
9.833753	521.286451	11.070848
9.853259	525.029739	11.075866
9.552806	524.700994	11.080883
9.864411	520.625182	11.085901
9.672842	532.914196	11.090919
9.946166	526.367607	11.095936
9.894096	523.983785	11.100954
9.735024	521.407532	11.105971
10.262296	518.379829	11.110989
9.515948	528.469135	11.116007
10.052924	524.741260	11.121024
9.624498	534.670060	11.126042
10.067715	538.055746	11.131059
10.374676	551.520068	11.136077
10.253667	552.697383	11.141095
10.206721	535.866368	11.146112
9.956726	534.832645	11.151130
9.591207	528.060774	11.156147
10.387424	546.883827	11.161165
10.528540	545.873081	11.166183
10.040256	530.963884	11.171200
10.010750	537.357207	11.176218
10.090639	533.634640	11.181235
10.193474	522.517202	11.186253
9.855614	527.942182	11.191271
10.388421	534.987643	11.196288
10.103461	543.965916	11.201306
10.151695	539.827977	11.206323
10.276240	545.466434	11.211341
9.999850	542.413068	11.216359
10.502534	541.950831	11.221376
10.194976	535.516141	11.226394
9.966364	537.412852	11.231411
10.431494	542.289447	11.236429
10.300170	542.546511	11.241447
10.002444	541.903758	11.246464
9.767704	549.583646	11.251482
10.212318	550.853544	11.256499
10.100822	540.163218	11.261517
10.136817	556.479809	11.266535
10.550270	550.858653	11.271552
10.389619	552.583453	11.276570
10.821083	551.183139	11.281587
10.466016	546.713056	11.286605
10.530634	554.352046	11.291623
10.486290	545.673602	11.296640
10.306721	544.235493	11.301658
10.194846	555.762134	11.306675
10.547379	538.688355	11.311693
10.261312	551.570007	11.316711
10.461105	549.816109	11.321728
10.447377	557.129570	11.326746
10.071175	555.402911	11.331763
10.167689	547.177783	11.336781
10.033311	557.790532	11.341799
10.321754	542.660103	11.346816
10.095826	545.899751	11.351834
10.229331	551.329850	11.356851
10.128425	545.282621	11.361869
10.052508	553.567945	11.366887
10.616014	564.388688	11.371904
10.762010	568.716026	11.376922
10.238643	566.858919	11.381939
10.652938	567.282556	11.386957
10.375894	578.586689	11.391975
10.711397	584.452081	11.396992
10.725755	583.265175	11.402010
10.570745	577.079300	11.407027
10.664769	559.579413	11.412045
10.444723	558.044102	11.417063
10.663720	563.476332	11.422080
10.345211	559.312346	11.427098
10.603140	571.319413	11.432115
10.911715	576.293097	11.437133
10.447531	576.107107	11.442151
10.579880	580.424317	11.447168
10.668799	586.253536	11.452186
10.648043	591.484309	11.457203
10.945946	579.846063	11.462221
10.472445	571.179493	11.467239
10.437953	576.853646	11.472256
10.907146	589.261204	11.477274
10.473458	576.605290	11.482291
10.850016	578.511054	11.487309
11.066300	587.736522	11.492327
10.726352	568.313654	11.497344
10.790231	567.844438	11.502362
10.833418	571.672769	11.507379
10.779991	562.113620	11.512397
10.461455	566.585093	11.517415
10.659931	575.101174	11.522432
10.772779	572.682060	11.527450
10.885335	584.073593	11.532467
11.231014	579.933248	11.537485
10.858579	581.725534	11.542503
10.834679	575.489327	11.547520
10.754222	563.281754	11.552538
10.779065	578.673336	11.557555
11.170265	573.671564	11.562573
10.765324	581.749213	11.567591
10.502940	573.706155	11.572608
11.030149	570.139523	11.577626
10.664146	593.697143	11.582643
10.807350	580.611705	11.587661
10.853405	581.368572	11.592679
10.914103	581.899009	11.597696
11.367312	580.016183	11.602714
11.139839	584.957718	11.607731
11.370614	577.001572	11.612749
11.071203	584.957163	11.617767
10.888241	569.244490	11.622784
11.168968	568.670930	11.627802
10.786463	574.582044	11.632819
11.245299	574.676259	11.637837
11.246700	580.708983	11.642855
10.982888	558.915018	11.647872
10.947672	561.867088	11.652890
10.754526	571.450730	11.657907
11.144534	574.619304	11.662925
10.980769	582.335438	11.667943
11.139177	589.499842	11.672960
11.197268	579.339520	11.677978
10.952615	583.259001	11.682995
11.238908	581.572998	11.688013
11.070792	582.195005	11.693031
11.190789	580.084910	11.698048
11.059291	591.107207	11.703066
10.872071	584.074199	11.708083
11.431212	578.914208	11.713101
11.095936	585.512298	11.718119
11.080248	582.428189	11.723136
11.217571	595.122783	11.728154
10.896271	591.366697	11.733171
10.958005	592.236696	11.738189
10.791520	584.977229	11.743207
10.794556	586.942323	11.748224
11.424583	586.092416	11.753242
10.840334	594.044966	11.758259
11.314440	603.786006	11.763277
11.228734	599.850220	11.768295
11.450536	610.262871	11.773312
11.656615	599.942516	11.778330
11.314291	599.713241	11.783347
11.382036	588.929905	11.788365
11.307187	590.505815	11.793383
11.348806	595.436876	11.798400
11.066193	593.217139	11.803418
11.345232	613.662127	11.808435
11.530884	611.374397	11.813453
11.515383	609.916491	11.818471
11.442497	611.381258	11.823488
11.654562	598.038122	11.828506
11.160792	605.438875	11.833523
11.316820	603.160007	11.838541
11.618810	605.381096	11.843559
11.424165	600.366857	11.848576
11.432425	602.055321	11.853594
11.352920	609.092954	11.858611
11.434680	608.266267	11.863629
11.472415	611.443208	11.868647
11.714782	610.430785	11.873664
11.676238	599.964295	11.878682
11.202923	607.881486	11.883699
11.331183	599.298525	11.888717
11.527349	603.360077	11.893735
11.479567	604.981681	11.898752
11.530733	613.271897	11.903770
11.433456	618.592162	11.908787
11.574452	610.763313	11.913805
11.582045	608.050887	11.918823
11.434336	613.717103	11.923840
11.849293	609.960084	11.928858
11.578203	618.924678	11.933875
11.662430	604.493036	11.938893
11.838091	612.569859	11.943911
11.267574	621.038797	11.948928
11.576924	614.654869	11.953946
11.559430	618.126401	11.958963
11.546187	615.155846	11.963981
11.491153	611.533829	11.968999
11.859538	628.370987	11.974016
11.930222	630.959237	11.979034
11.499740	620.444109	11.984051
11.709643	629.472254	11.989069
12.196597	632.161379	11.994087
11.699074	624.240835	11.999104
11.804384	611.601790	12.004122
11.425182	629.692245	12.009139
12.016026	639.200143	12.014157
12.299710	637.332693	12.019175
11.794271	623.582459	12.024192
11.803229	616.574108	12.029210
11.488101	628.925464	12.034227
11.761146	631.082278	12.039245
11.489353	643.022540	12.044263
11.487365	650.370705	12.049280
11.546395	652.792210	12.054298
11.335973	647.812269	12.059315
11.800870	640.953695	12.064333
12.070607	650.032926	12.069351
11.698999	651.206038	12.074368
12.212586	651.098059	12.079386
12.339547	659.443412	12.084403
12.208464	647.557547	12.089421
12.012837	638.937461	12.094439
11.933997	645.285490	12.099456
12.212580	634.596596	12.104474
12.053972	640.861433	12.109491
11.860745	645.474685	12.114509
12.125947	652.513699	12.119527
12.192663	643.925393	12.124544
11.926636	649.356388	12.129562
11.994384	644.934099	12.134579
11.656728	643.997019	12.139597
12.098828	654.812811	12.144615
12.212634	664.629326	12.149632
12.514818	667.195441	12.154650
12.263707	662.437595	12.159667
12.488425	653.794481	12.164685
12.240888	642.347429	12.169703
11.974416	642.723210	12.174720
12.159989	641.193891	12.179738
12.035713	646.682419	12.184755
12.008062	648.038499	12.189773
12.478173	657.470618	12.194791
12.227897	665.133658	12.199808
12.082255	653.981841	12.204826
12.301646	661.365847	12.209843
12.470052	675.981167	12.214861
12.515838	668.552531	12.219879
12.118855	661.067188	12.224896
12.324054	653.353423	12.229914
12.491369	659.118069	12.234931
12.307668	648.660123	12.239949
12.571113	649.450933	12.244967
12.329125	649.010114	12.249984
12.176687	653.248509	12.255002
12.338614	659.220333	12.260019
12.344968	663.477019	12.265037
12.544552	667.772252	12.270055
12.163098	670.812204	12.275072
12.908286	675.946206	12.280090
12.281013	669.511258	12.285107
12.135728	678.505169	12.290125
12.429978	672.086526	12.295143
12.299484	675.221369	12.300160
12.703826	672.272923	12.305178
12.533585	671.337540	12.310195
12.376697	672.450558	12.315213
12.271827	674.635944	12.320231
12.131168	667.390648	12.325248
12.340948	662.921520	12.330266
12.535743	674.791340	12.335283
12.508200	667.071177	12.340301
12.749793	665.960462	12.345319
12.546841	671.940187	12.350336
12.369062	667.466779	12.355354
12.683924	664.510572	12.360371
12.293347	668.324417	12.365389
12.346875	674.946103	12.370407
12.547808	690.882694	12.375424
12.913008	700.136622	12.380442
12.923003	702.697180	12.385459
12.590806	695.396115	12.390477
12.814814	684.964268	12.395495
12.615937	691.134646	12.400512
12.978106	690.659544	12.405530
12.697640	677.862734	12.410547
12.718843	678.080276	12.415565
12.804955	682.754581	12.420583
12.551279	693.976771	12.425600
12.811635	691.491195	12.430618
12.778845	701.905479	12.435635
12.689150	710.060116	12.440653
12.709811	705.689137	12.445671
12.675352	713.539540	12.450688
12.770634	704.638603	12.455706
13.073752	696.560537	12.460723
12.957964	700.009451	12.465741
13.116260	701.618071	12.470759
12.957270	699.867889	12.475776
12.600128	697.897120	12.480794
13.334531	701.550758	12.485811
13.307382	711.694250	12.490829
13.179539	699.988107	12.495847
13.049578	689.265710	12.500864
12.659680	679.953540	12.505882
12.765427	680.021214	12.510899
12.822708	692.414848	12.515917
13.191353	705.362202	12.520935
13.119472	710.395426	12.525952
13.048177	704.992373	12.530970
13.295037	705.452505	12.535987
12.955815	700.199490	12.541005
12.732054	701.104745	12.546023
12.537854	707.509963	12.551040
12.721925	700.617929	12.556058
12.974995	705.352475	12.561075
13.029818	700.463262	12.566093
12.928169	702.859910	12.571111
12.978163	710.696668	12.576128
13.048091	698.199447	12.581146
12.805700	708.235417	12.586163
13.078865	720.398324	12.591181
13.161189	719.353444	12.596199
12.997824	735.689582	12.601216
13.221172	731.034335	12.606234
13.496678	731.057457	12.611251
13.418361	739.158845	12.616269
13.107425	730.196878	12.621287
13.082124	734.356096	12.626304
13.256221	735.256833	12.631322
13.300891	733.657231	12.636339
13.388337	743.631119	12.641357
13.469825	732.395040	12.646375
13.797036	735.556567	12.651392
13.491841	727.125693	12.656410
13.715087	726.762256	12.661427
13.120862	721.174089	12.666445
13.685781	722.548800	12.671463
13.399039	728.169471	12.676480
13.138556	709.600866	12.681498
13.264233	718.302145	12.686515
13.337234	726.609459	12.691533
13.724880	734.640482	12.696551
13.593779	729.461912	12.701568
13.677011	723.860347	12.706586
13.343336	725.479684	12.711603
13.214879	727.117663	12.716621
13.507788	728.462198	12.721639
13.501518	726.703556	12.726656
13.571235	730.757421	12.731674
13.710325	730.275305	12.736691
13.409839	736.032702	12.741709
13.809202	731.721005	12.746727
13.907227	737.761351	12.751744
13.684551	736.383926	12.756762
13.819450	723.473948	12.761779
13.075452	715.338045	12.766797
13.363959	731.308936	12.771815
13.390755	734.829427	12.776832
13.271029	729.922567	12.781850
13.478471	723.904718	12.786867
13.440794	734.403885	12.791885
13.447952	722.166074	12.796903
13.326014	727.612316	12.801920
13.602905	746.861277	12.806938
14.099488	757.249810	12.811955
13.535563	763.994633	12.816973
13.892436	760.408047	12.821991
13.909195	762.585432	12.827008
13.628082	764.132852	12.832026
14.032304	761.053514	12.837043
13.904720	755.958399	12.842061
13.790187	754.321678	12.847079
13.857720	753.090096	12.852096
13.899666	767.076571	12.857114
13.747035	757.918013	12.862131
13.847319	762.125061	12.867149
13.977108	761.095319	12.872167
14.104905	766.903973	12.877184
13.677780	770.071604	12.882202
13.801351	766.367113	12.887219
13.587140	772.853631	12.892237
13.788674	762.420350	12.897255
14.109731	764.086563	12.902272
13.666525	757.245816	12.907290
13.990495	762.453401	12.912307
14.046389	760.080139	12.917325
13.846936	765.529043	12.922343
13.719228	761.574609	12.927360
13.550249	771.775964	12.932378
14.105839	766.281882	12.937395
14.257659	774.520417	12.942413
14.044927	769.853001	12.947431
14.130589	772.663573	12.952448
13.964813	785.331148	12.957466
14.338799	783.187865	12.962483
14.199244	791.773439	12.967501
14.292707	777.353486	12.972519
14.244503	778.657486	12.977536
13.875306	767.259498	12.982554
14.259801	778.793362	12.987571
14.200885	794.736442	12.992589
14.282907	792.240337	12.997607
14.279513	785.805573	13.002624
14.205988	794.603385	13.007642
14.567200	788.898511	13.012659
14.597431	796.764187	13.017677
14.151407	791.962325	13.022695
14.549015	780.764803	13.027712
14.060876	789.168175	13.032730
14.426510	786.630442	13.037747
14.387015	788.425872	13.042765
14.469574	790.210070	13.047783
14.496026	794.570136	13.052800
14.365947	794.844319	13.057818
14.694554	784.118466	13.062835
14.318452	795.592557	13.067853
14.353179	792.825790	13.072871
14.346339	785.245621	13.077888
14.198599	796.366228	13.082906
14.634402	782.676910	13.087923
14.175771	795.067996	13.092941
14.732483	782.784461	13.097959
14.568425	791.256793	13.102976
14.469202	790.611545	13.107994
14.742044	787.354644	13.113011
14.443338	794.550242	13.118029
14.461056	787.636020	13.123047
14.822773	794.535641	13.128064
14.696352	790.223531	13.133082
14.779037	788.314871	13.138099
14.885823	794.767335	13.143117
14.729884	791.892702	13.148135
14.722943	787.967397	13.153152
14.703242	795.418765	13.158170
14.880307	786.096146	13.163187
14.688298	788.857801	13.168205
14.949830	794.461770	13.173223
14.848252	790.383899	13.178240
14.525653	784.447040	13.183258
14.883307	785.090320	13.188275
14.803434	788.546275	13.193293
14.756761	786.257178	13.198311
14.873140	785.495785	13.203328
14.567135	790.700814	13.208346
14.856282	784.064289	13.213363
14.667187	792.276629	13.218381
14.669921	790.562150	13.223399
14.731790	791.548075	13.228416
14.538649	796.661910	13.233434
14.496050	789.473481	13.238451
14.818552	797.227000	13.243469
15.000490	796.436208	13.248487
15.186543	801.186844	13.253504
14.686913	800.263488	13.258522
14.721817	793.726693	13.263539
15.158560	789.755986	13.268557
14.842794	789.060909	13.273575
15.088728	788.062251	13.278592
14.560575	789.617272	13.283610
15.289328	806.936419	13.288627
15.167004	816.785586	13.293645
15.153811	821.695911	13.298663
15.402240	811.188863	13.303680
15.209279	800.115863	13.308698
14.942798	792.539085	13.313715
15.035409	787.687064	13.318733
14.647493	801.782811	13.323751
15.278360	810.185228	13.328768
15.468348	821.069613	13.333786
15.180293	819.127302	13.338803
15.185072	816.859371	13.343821
14.840503	828.613854	13.348839
14.944052	817.690953	13.353856
15.121374	823.895107	13.358874
15.359763	819.688090	13.363891
15.451832	821.385087	13.368909
15.557644	815.946259	13.373927
15.430061	818.166737	13.378944
15.127598	823.097192	13.383962
15.415531	826.575677	13.388979
15.291610	821.656888	13.393997
15.228782	832.068575	13.399015
15.428623	811.154404	13.404032
15.337950	829.064466	13.409050
15.367657	822.763939	13.414067
15.377264	817.318269	13.419085
15.144446	828.121961	13.424103
15.295199	815.700575	13.429120
15.283019	823.850458	13.434138
15.139770	818.935275	13.439155
15.516585	829.060123	13.444173
15.632897	841.768253	13.449191
15.751685	842.448088	13.454208
15.465418	834.296272	13.459226
15.503149	846.392906	13.464243
15.770782	835.753525	13.469261
15.692092	842.189989	13.474279
15.592560	822.916198	13.479296
15.255568	829.554436	13.484314
15.784892	831.082702	13.489331
15.862375	841.832072	13.494349
15.606933	845.219394	13.499367
15.421703	842.164594	13.504384
15.690675	861.005200	13.509402
15.862205	846.384819	13.514419
15.835528	846.901050	13.519437
15.840091	847.506176	13.524455
15.902283	836.545848	13.529472
15.963788	851.133435	13.534490
15.814450	844.302855	13.539507
15.795203	824.011458	13.544525
15.198081	835.213675	13.549543
15.640741	832.782219	13.554560
15.527167	840.194884	13.559578
15.829761	850.424398	13.564595
15.765836	840.855799	13.569613
15.449875	854.141658	13.574631
15.634875	851.894156	13.579648
15.652482	854.697355	13.584666
15.465758	856.453489	13.589683
16.074439	859.327724	13.594701
16.029203	875.550089	13.599719
16.331882	861.144297	13.604736
16.250219	858.080547	13.609754
16.019155	853.813369	13.614771
16.113169	838.242168	13.619789
15.897054	845.060702	13.624807
15.776913	847.146295	13.629824
16.119030	853.510262	13.634842
15.968399	867.416442	13.639859
16.284856	868.419501	13.644877
16.110832	869.391690	13.649895
16.209910	874.793375	13.654912
16.363879	881.370110	13.659930
16.240902	872.473859	13.664947
16.249473	871.462683	13.669965
16.310831	882.135240	13.674983
16.428086	871.136209	13.680000
16.129890	853.365378	13.685018
16.197457	860.359783	13.690035
16.664566	860.991762	13.695053
15.918621	868.518209	13.700071
16.257583	861.202748	13.705088
16.273854	866.666616	13.710106
16.107259	876.433815	13.715123
16.310135	872.247252	13.720141
16.402345	881.689174	13.725159
16.350486	869.116001	13.730176
16.333077	880.415386	13.735194
16.411744	872.182029	13.740211
16.670214	868.425566	13.745229
16.299517	872.022785	13.750247
16.493874	867.375860	13.755264
16.486157	865.899511	13.760282
16.465244	872.004360	13.765299
16.513669	861.851364	13.770317
16.487870	875.040394	13.775335
16.514384	872.622986	13.780352
16.117048	882.526959	13.785370
16.570543	870.048518	13.790387
16.829276	870.666907	13.795405
16.483126	868.898998	13.800423
16.708298	872.944383	13.805440
16.539432	872.148710	13.810458
16.489694	875.776633	13.815475
16.448429	871.976885	13.820493
16.594146	876.099056	13.825511
16.660831	869.788426	13.830528
16.678956	868.305616	13.835546
16.892363	871.718158	13.840563
16.585659	864.290343	13.845581
16.589003	876.609827	13.850599
16.702882	878.364028	13.855616
17.017342	876.665242	13.860634
16.826435	881.573433	13.865651
16.955479	874.992219	13.870669
16.650809	875.304083	13.875687
16.576725	887.493541	13.880704
16.787803	889.658724	13.885722
16.901338	895.434956	13.890739
17.267292	897.515938	13.895757
17.299052	894.152245	13.900775
16.984978	885.159609	13.905792
16.951118	876.823110	13.910810
16.545850	876.463356	13.915827
17.357444	877.769328	13.920845
16.941882	890.459217	13.925863
17.151692	887.862925	13.930880
17.075437	875.332578	13.935898
16.994697	874.370890	13.940915
16.994015	874.965866	13.945933
17.142954	897.441968	13.950951
17.166477	894.782747	13.955968
17.190179	896.307467	13.960986
16.913404	900.823270	13.966003
17.096609	893.660053	13.971021
17.409766	899.983384	13.976039
17.434883	904.140567	13.981056
17.147404	899.729023	13.986074
16.866850	900.739785	13.991091
17.317498	896.078991	13.996109
17.162261	902.958883	14.001127
17.548527	897.816697	14.006144
17.308948	896.898730	14.011162
17.092032	902.701348	14.016179
17.487104	896.629611	14.021197
17.639406	904.779362	14.026215
17.717950	891.323530	14.031232
17.241137	881.917029	14.036250
17.196421	884.301290	14.041267
17.606649	885.820618	14.046285
17.299425	898.913147	14.051303
17.199128	896.709910	14.056320
17.380738	903.102938	14.061338
17.281357	904.285935	14.066355
17.577595	897.734792	14.071373
17.494150	898.006540	14.076391
17.475329	895.847630	14.081408
17.951601	890.877875	14.086426
17.347100	904.973102	14.091443
17.549438	898.421228	14.096461
17.402199	902.413764	14.101479
17.343659	894.233120	14.106496
17.676142	904.377590	14.111514
17.263444	899.676447	14.116531
17.388373	898.376262	14.121549
17.433102	898.278698	14.126567
17.388382	899.395527	14.131584
17.620297	896.409562	14.136602
17.772166	922.721374	14.141619
17.968296	919.210679	14.146637
17.843591	914.203216	14.151655
17.420081	908.060852	14.156672
17.867391	916.097407	14.161690
17.753709	921.442745	14.166707
17.904906	918.218240	14.171725
18.085718	922.003707	14.176743
18.120258	915.065569	14.181760
18.106893	897.000905	14.186778
17.777315	900.675345	14.191795
17.980293	896.018318	14.196813
17.831233	894.175327	14.201831
17.838526	895.099665	14.206848
17.996524	900.349056	14.211866
18.079362	912.216015	14.216883
18.039960	898.910087	14.221901
17.624081	901.255458	14.226919
17.908397	915.951142	14.231936
18.198800	927.788730	14.236954
18.235329	920.383952	14.241971
18.232269	917.262444	14.246989
18.298430	923.841390	14.252007
17.920843	931.187949	14.257024
18.169980	923.115589	14.262042
18.229576	922.773837	14.267059
18.543124	918.960376	14.272077
18.127730	906.883000	14.277095
17.783795	914.167268	14.282112
18.068243	917.522936	14.287130
18.177530	932.602823	14.292147
18.217040	927.363153	14.297165
18.600710	920.428988	14.302183
18.234037	927.470994	14.307200
18.637249	917.027710	14.312218
18.147286	924.675404	14.317235
18.298931	927.774033	14.322253
18.437048	932.273639	14.327271
18.277162	924.234225	14.332288
18.302608	923.753671	14.337306
18.321658	925.962980	14.342323
18.271423	932.570922	14.347341
18.315675	930.333025	14.352359
18.182413	932.243656	14.357376
18.286311	920.158693	14.362394
17.989394	935.137801	14.367411
18.266114	931.742440	14.372429
18.784777	937.661377	14.377447
18.567775	944.228543	14.382464
18.901289	947.404815	14.387482
18.446779	939.528135	14.392499
18.584884	937.043944	14.397517
18.491329	939.584156	14.402535
18.719781	940.574093	14.407552
19.011576	941.711759	14.412570
18.643615	950.386169	14.417587
18.658335	942.603533	14.422605
18.665799	957.911181	14.427623
18.365776	952.769667	14.432640
19.021901	939.155986	14.437658
18.731281	950.003620	14.442675
18.839999	945.574830	14.447693
18.986941	950.708366	14.452711
18.658738	945.613268	14.457728
18.826031	940.280312	14.462746
18.612347	935.136658	14.467763
18.615208	940.231544	14.472781
18.805546	946.133407	14.477799
18.379093	949.857227	14.482816
18.524024	943.713078	14.487834
18.832289	949.496923	14.492851
18.848147	961.953756	14.497869
19.186403	966.220906	14.502887
19.034321	972.772963	14.507904
19.025827	961.969955	14.512922
19.208610	962.451375	14.517939
19.177736	953.410644	14.522957
18.922625	951.514215	14.527975
18.875094	968.667512	14.532992
19.178888	968.176910	14.538010
19.560031	966.347157	14.543027
19.391903	963.155247	14.548045
19.287426	952.005623	14.553063
18.983489	951.519189	14.558080
19.059390	943.023673	14.563098
19.025825	949.836712	14.568115
19.434769	959.992524	14.573133
19.706098	967.633973	14.578151
19.193552	958.249702	14.583168
19.247080	940.365589	14.588186
19.297730	962.172339	14.593203
19.354673	964.577312	14.598221
19.428045	967.871231	14.603239
19.613871	973.291601	14.608256
19.722099	959.422534	14.613274
19.197062	947.320832	14.618291
18.883433	950.060213	14.623309
19.467846	950.256387	14.628327
19.417462	957.726515	14.633344
19.560336	961.704112	14.638362
19.585741	971.789830	14.643379
19.513856	967.594976	14.648397
19.432244	969.226571	14.653415
19.477044	967.749160	14.658432
19.356183	966.146931	14.663450
19.427722	970.944210	14.668467
19.357341	967.972258	14.673485
19.169621	966.455940	14.678503
19.420446	975.244824	14.683520
19.940538	984.096825	14.688538
19.395341	978.668119	14.693555
19.500618	992.186426	14.698573
19.821625	995.217157	14.703591
19.865344	1001.108374	14.708608
19.822228	994.701777	14.713626
20.120215	997.919001	14.718643
19.810525	997.234321	14.723661
20.218235	986.983734	14.728679
19.903776	988.749696	14.733696
19.715501	977.888375	14.738714
19.697783	982.015496	14.743731
19.797120	988.619860	14.748749
19.899265	985.876694	14.753767
20.023989	989.345142	14.758784
19.862356	989.997974	14.763802
20.176138	997.929608	14.768819
19.579955	999.091650	14.773837
19.976126	989.771662	14.778855
19.878021	995.385287	14.783872
20.057651	987.277599	14.788890
20.098180	990.999790	14.793907
19.833960	997.809852	14.798925
20.103738	992.205923	14.803943
20.237731	999.773370	14.808960
20.210522	993.771979	14.813978
20.321027	989.502713	14.818995
19.850736	993.755056	14.824013
20.359402	995.732612	14.829031
20.290034	998.545568	14.834048
20.164514	996.679559	14.839066
19.792189	994.773868	14.844083
20.252073	1013.053040	14.849101
20.725728	1016.196584	14.854119
20.656362	1009.140447	14.859136
20.483111	1002.886178	14.864154
20.284619	997.637621	14.869171
20.201094	999.302213	14.874189
20.683446	994.361728	14.879207
20.368069	994.972402	14.884224
20.390599	997.318930	14.889242
20.386337	991.562137	14.894259
20.324133	1011.848438	14.899277
20.675642	1012.908473	14.904295
20.404877	1036.955628	14.909312
20.647752	1028.827171	14.914330
20.797131	1023.586530	14.919347
20.560269	1031.594744	14.924365
20.753274	1024.229652	14.929383
20.292289	1017.246082	14.934400
20.649720	1023.974876	14.939418
20.760247	1024.128958	14.944435
20.991860	1034.337915	14.949453
20.644098	1024.495531	14.954471
20.842704	1022.331172	14.959488
20.528756	1024.912753	14.964506
20.710084	1026.647493	14.969523
20.695996	1027.821048	14.974541
20.631734	1025.124823	14.979559
20.766071	1028.034234	14.984576
20.596113	1023.157282	14.989594
20.752667	1017.865846	14.994611
20.342387	1023.176664	14.999629
20.790777	1020.042103	15.004647
20.748434	1024.875649	15.009664
20.979220	1041.113921	15.014682
21.417753	1044.003876	15.019699
21.411360	1047.523655	15.024717
21.400986	1028.746176	15.029735
21.052072	1028.923475	15.034752
20.860962	1026.174322	15.039770
21.119162	1024.429560	15.044787
20.930464	1028.847696	15.049805
21.226423	1019.863226	15.054823
21.212174	1024.144891	15.059840
20.785608	1025.801545	15.064858
21.081026	1025.593814	15.069875
20.817408	1044.222002	15.074893
21.319046	1040.301467	15.079911
21.190249	1047.855139	15.084928
21.179029	1047.548382	15.089946
21.330124	1042.572394	15.094963
21.059010	1049.004118	15.099981
21.498779	1050.658900	15.104999
21.302663	1044.991058	15.110016
21.079945	1042.388092	15.115034
21.471793	1045.989703	15.120051
21.269166	1049.551547	15.125069
21.378189	1040.526093	15.130087
21.356846	1046.007299	15.135104
21.290148	1042.227680	15.140122
21.909962	1044.499743	15.145139
21.522677	1049.339451	15.150157
21.621212	1049.839995	15.155175
21.521667	1041.082658	15.160192
21.456616	1047.857275	15.165210
21.613782	1046.098203	15.170227
21.528738	1047.517004	15.175245
21.990287	1048.957154	15.180263
21.499502	1043.831174	15.185280
21.183903	1045.410335	15.190298
21.964252	1042.210754	15.195315
21.859207	1050.380522	15.200333
21.897830	1044.895699	15.205351
21.675622	1033.881326	15.210368
21.680972	1042.525626	15.215386
22.032893	1044.557586	15.220403
21.745115	1052.681747	15.225421
22.266852	1044.730148	15.230439
22.335407	1039.091935	15.235456
21.902652	1043.119168	15.240474
22.163219	1034.606294	15.245491
21.893431	1040.298860	15.250509
22.014112	1036.209375	15.255527
22.085212	1035.309048	15.260544
21.949813	1052.864816	15.265562
22.177004	1040.495108	15.270579
21.797183	1038.799700	15.275597
22.188756	1033.908541	15.280615
21.879885	1030.066821	15.285632
22.141778	1040.235317	15.290650
22.444071	1042.663298	15.295667
22.135144	1041.134443	15.300685
22.127501	1033.817263	15.305703
22.252399	1036.069621	15.310720
21.888117	1034.064562	15.315738
21.879081	1033.313768	15.320755
22.430689	1047.262239	15.325773
22.329139	1051.727703	15.330791
22.385468	1069.706715	15.335808
22.669941	1062.850783	15.340826
22.663427	1051.275773	15.345843
22.172266	1044.170048	15.350861
22.249682	1038.155581	15.355879
22.299059	1053.297705	15.360896
22.100944	1065.298481	15.365914
22.262998	1058.999088	15.370931
22.372953	1071.160857	15.375949
22.356674	1063.558893	15.380967
22.588834	1073.898093	15.385984
22.355103	1071.110743	15.391002
22.473337	1063.726566	15.396019
22.075717	1065.126065	15.401037
22.423050	1070.610959	15.406055
22.710027	1064.735657	15.411072
22.534663	1070.273178	15.416090
22.813776	1066.765192	15.421107
22.788929	1089.332659	15.426125
22.779935	1089.154264	15.431143
23.228912	1075.591036	15.436160
22.704608	1073.501945	15.441178
22.639527	1061.541803	15.446195
22.496879	1065.254696	15.451213
23.020707	1074.827742	15.456231
23.239986	1078.585595	15.461248
22.620378	1068.751360	15.466266
22.988914	1079.351738	15.471283
23.228534	1085.711186	15.476301
22.468370	1079.086352	15.481319
22.749730	1069.308655	15.486336
22.854205	1089.456731	15.491354
23.021600	1083.340682	15.496371
23.072693	1091.427831	15.501389
23.096299	1087.689881	15.506407
23.300489	1090.118822	15.511424
22.880720	1089.425663	15.516442
23.102435	1078.032766	15.521459
23.033836	1093.366576	15.526477
23.252241	1085.716147	15.531495
23.166341	1084.292730	15.536512
22.932205	1092.302884	15.541530
23.357611	1093.129001	15.546547
23.451012	1088.677520	15.551565
23.354576	1094.623168	15.556583
23.194030	1086.303874	15.561600
23.163764	1097.983880	15.566618
23.166572	1085.015245	15.571635
23.163550	1089.156093	15.576653
23.208367	1087.973533	15.581671
23.092068	1083.592733	15.586688
23.610965	1105.732860	15.591706
23.884042	1100.550763	15.596723
23.532347	1095.702419	15.601741
23.161117	1092.126151	15.606759
23.616332	1095.531425	15.611776
23.529990	1108.781698	15.616794
23.812042	1111.008341	15.621811
23.589277	1105.926765	15.626829
23.598293	1105.833167	15.631847
23.884706	1096.996295	15.636864
23.792204	1097.299864	15.641882
23.983476	1075.059472	15.646899
23.524600	1074.733030	15.651917
23.788657	1081.626574	15.656935
23.790809	1075.063216	15.661952
23.663671	1089.331221	15.666970
23.707816	1090.758472	15.671987
24.216058	1101.353361	15.677005
23.863385	1100.532914	15.682023
24.011064	1083.230987	15.687040
23.843791	1088.603005	15.692058
24.192740	1095.145456	15.697075
23.944156	1084.940111	15.702093
23.780372	1087.890423	15.707111
24.183664	1088.804462	15.712128
24.044402	1109.664693	15.717146
24.285660	1097.311105	15.722163
23.855502	1092.621858	15.727181
24.389518	1098.859943	15.732199
24.298426	1086.203749	15.737216
24.019473	1082.224766	15.742234
24.040125	1085.190089	15.747251
24.293896	1100.029798	15.752269
24.229122	1109.565665	15.757287
24.236027	1110.760932	15.762304
24.111481	1113.463401	15.767322
24.061118	1108.168533	15.772339
24.232638	1107.262535	15.777357
24.198346	1104.671152	15.782375
24.465232	1113.326743	15.787392
24.311051	1104.272955	15.792410
24.494573	1107.145862	15.797427
24.258391	1110.614483	15.802445
24.325136	1101.671213	15.807463
24.010232	1100.599226	15.812480
24.252191	1114.875589	15.817498
24.564546	1110.658562	15.822515
24.556389	1104.119345	15.827533
24.306430	1109.364176	15.832551
24.412140	1114.592018	15.837568
24.585663	1128.794340	15.842586
24.986875	1123.949580	15.847603
25.064470	1140.264990	15.852621
24.383431	1117.506565	15.857639
24.804065	1110.289810	15.862656
24.528911	1127.289393	15.867674
24.775969	1117.288639	15.872691
24.830403	1126.045294	15.877709
24.539739	1135.670294	15.882727
24.845342	1128.952545	15.887744
24.921577	1131.732271	15.892762
24.726578	1126.592925	15.897779
24.999814	1129.130863	15.902797
24.830302	1132.482508	15.907815
25.042808	1121.042688	15.912832
24.950390	1133.312154	15.917850
25.033150	1132.889386	15.922867
24.927823	1132.890774	15.927885
24.731620	1139.761242	15.932903
25.166296	1133.231870	15.937920
24.876996	1135.379080	15.942938
25.321461	1134.708408	15.947955
25.551461	1131.457376	15.952973
25.208387	1139.641559	15.957991
25.272501	1124.819095	15.963008
24.916588	1124.447587	15.968026
25.275444	1134.761832	15.973043
25.366475	1123.081584	15.978061
25.247591	1124.205638	15.983079
25.596612	1124.277171	15.988096
25.318600	1120.778705	15.993114
25.453758	1126.905152	15.998131
25.204069	1118.689234	16.003149
25.081667	1134.056829	16.008167
25.008559	1124.072673	16.013184
25.480168	1127.472080	16.018202
25.579566	1136.853518	16.023219
25.786536	1125.526813	16.028237
25.257971	1125.107233	16.033255
25.205810	1130.810509	16.038272
25.874736	1147.497697	16.043290
25.862549	1148.337497	16.048307
26.049665	1136.217275	16.053325
25.610184	1132.277952	16.058343
25.577864	1131.473545	16.063360
25.719456	1132.626350	16.068378
25.546613	1151.529722	16.073395
25.883703	1151.218218	16.078413
25.643656	1151.308528	16.083431
25.685779	1151.345248	16.088448
25.629835	1159.278971	16.093466
25.660784	1156.192114	16.098483
25.919905	1148.923843	16.103501
25.932523	1154.514004	16.108519
26.047031	1147.367009	16.113536
26.094806	1149.024753	16.118554
26.041018	1154.966092	16.123571
26.037088	1154.435691	16.128589
26.118900	1151.630130	16.133607
25.810081	1154.383706	16.138624
25.787403	1150.427855	16.143642
25.730131	1151.143265	16.148659
26.079493	1155.792856	16.153677
25.950500	1162.367138	16.158695
26.592582	1158.935410	16.163712
26.453397	1173.311395	16.168730
26.626509	1164.903926	16.173747
26.323932	1153.106408	16.178765
26.248668	1155.936120	16.183783
26.485307	1141.673124	16.188800
26.097379	1148.426258	16.193818
26.364230	1155.866193	16.198835
26.314221	1141.757135	16.203853
26.027649	1165.867744	16.208871
26.101281	1167.817635	16.213888
26.319697	1161.749371	16.218906
26.369489	1174.673546	16.223923
26.479985	1169.469238	16.228941
26.130286	1169.546674	16.233959
26.420921	1177.872780	16.238976
26.847611	1170.399884	16.243994
26.800327	1179.217962	16.249011
26.748492	1167.875583	16.254029
26.469191	1175.875178	16.259047
26.802635	1172.179800	16.264064
26.608770	1182.507209	16.269082
26.658867	1179.055765	16.274099
26.867776	1169.566411	16.279117
26.688919	1175.617124	16.284135
26.693949	1171.059447	16.289152
26.721154	1181.283973	16.294170
27.100232	1204.891112	16.299187
27.225421	1195.886501	16.304205
26.842201	1185.318446	16.309223
27.018519	1182.876288	16.314240
27.298087	1191.104639	16.319258
26.961555	1180.776847	16.324275
27.112333	1169.287411	16.329293
26.966199	1182.096527	16.334311
27.124665	1187.286099	16.339328
27.031412	1195.091009	16.344346
27.289570	1201.062402	16.349363
27.079620	1190.561997	16.354381
27.304930	1205.561648	16.359399
27.310031	1190.710349	16.364416
27.379674	1203.798171	16.369434
27.139894	1205.072633	16.374451
27.609735	1198.428733	16.379469
27.337802	1198.764884	16.384487
27.425641	1198.287336	16.389504
27.617780	1196.703922	16.394522
27.637653	1203.077503	16.399539
27.806856	1194.230137	16.404557
27.554900	1197.718721	16.409575
27.311957	1181.185512	16.414592
27.556048	1191.602332	16.419610
27.490692	1190.242022	16.424627
27.953881	1190.814240	16.429645
27.702861	1188.746636	16.434663
27.726097	1190.025411	16.439680
27.696387	1189.403629	16.444698
27.507679	1197.009456	16.449715
27.651204	1191.735480	16.454733
27.503407	1190.510127	16.459751
27.309495	1187.222067	16.464768
27.706836	1191.753463	16.469786
27.450788	1191.575187	16.474803
27.909594	1193.059506	16.479821
27.375243	1192.801114	16.484839
27.662095	1204.634389	16.489856
27.982251	1213.435506	16.494874
27.514888	1213.856892	16.499891
27.775804	1221.061243	16.504909
27.937476	1207.709031	16.509927
28.196443	1221.688585	16.514944
28.384592	1222.648627	16.519962
28.148708	1216.107845	16.524979
28.386837	1220.281478	16.529997
28.429431	1212.283847	16.535015
28.207840	1212.098269	16.540032
28.447959	1216.438491	16.545050
27.985588	1229.664757	16.550067
28.132096	1207.776087	16.555085
28.297156	1215.390049	16.560103
28.203366	1218.278361	16.565120
28.524156	1216.571205	16.570138
28.043259	1216.487777	16.575155
28.234515	1214.013211	16.580173
28.246370	1212.483775	16.585191
28.201799	1215.916242	16.590208
28.311307	1209.982984	16.595226
28.158815	1222.555800	16.600243
28.659680	1228.432930	16.605261
28.984590	1230.989854	16.610279
28.762648	1217.011267	16.615296
28.841989	1213.177020	16.620314
28.275997	1215.656829	16.625331
28.530402	1220.952115	16.630349
28.647220	1235.453316	16.635367
28.640359	1231.088535	16.640384
29.433643	1235.397844	16.645402
29.107990	1231.818298	16.650419
29.059727	1216.017226	16.655437
29.193118	1207.636807	16.660455
28.924692	1204.883938	16.665472
28.888672	1206.501287	16.670490
28.573907	1201.067665	16.675507
29.025210	1200.555296	16.680525
28.957944	1221.823376	16.685543
28.814731	1230.203511	16.690560
29.330019	1230.146626	16.695578
29.121071	1229.899894	16.700595
29.216590	1227.019997	16.705613
29.281315	1219.866677	16.710631
29.225561	1236.424421	16.715648
29.427944	1233.327558	16.720666
28.925780	1229.175410	16.725683
29.092150	1238.626090	16.730701
29.217258	1234.521250	16.735719
29.194147	1238.223765	16.740736
29.173945	1240.703017	16.745754
29.149258	1239.472552	16.750771
29.166354	1245.280889	16.755789
29.451151	1239.861769	16.760807
29.419158	1230.602567	16.765824
29.331869	1239.554881	16.770842
29.283838	1231.042012	16.775859
29.081863	1241.238530	16.780877
29.482566	1250.869157	16.785895
29.404101	1267.778726	16.790912
29.776986	1261.944580	16.795930
29.718560	1264.088866	16.800947
29.690080	1264.786111	16.805965
30.097081	1257.236529	16.810983
29.633297	1270.687464	16.816000
29.765598	1261.095045	16.821018
29.755152	1262.161323	16.826035
30.038817	1262.596460	16.831053
30.001119	1261.981121	16.836071
29.992190	1264.886831	16.841088
29.980648	1256.153720	16.846106
29.878802	1261.059431	16.851123
30.086052	1257.593267	16.856141
30.115506	1262.819661	16.861159
30.155591	1266.263264	16.866176
30.155967	1258.253730	16.871194
30.274584	1271.624007	16.876211
30.188528	1260.562827	16.881229
30.202150	1261.130639	16.886247
30.058770	1266.261356	16.891264
30.013864	1253.649314	16.896282
29.759709	1252.507773	16.901299
29.990925	1252.198511	16.906317
29.840311	1253.329029	16.911335
30.000472	1268.051393	16.916352
30.430432	1284.921750	16.921370
30.528617	1284.368467	16.926387
30.308982	1289.491001	16.931405
30.527070	1282.971583	16.936423
30.332130	1283.781138	16.941440
30.480754	1280.970748	16.946458
30.777157	1285.662250	16.951475
30.405768	1288.986461	16.956493
30.792954	1285.680927	16.961511
30.644919	1291.815928	16.966528
30.794427	1284.800448	16.971546
30.793477	1277.525739	16.976563
30.813821	1285.733843	16.981581
30.914015	1276.408551	16.986599
30.652040	1291.568801	16.991616
30.903840	1281.400231	16.996634
30.899417	1277.159042	17.001651
31.032291	1273.066681	17.006669
31.207098	1283.425789	17.011687
30.750300	1284.375320	17.016704
30.974561	1274.871146	17.021722
30.960813	1287.304817	17.026739
30.530618	1285.191392	17.031757
31.027783	1286.818946	17.036775
30.795378	1285.823781	17.041792
31.225090	1284.292994	17.046810
30.978861	1284.190639	17.051827
31.226035	1276.257000	17.056845
31.078496	1282.274990	17.061863
31.254236	1289.311254	17.066880
31.139535	1279.316195	17.071898
31.144285	1284.413243	17.076915
31.237287	1292.987606	17.081933
31.608985	1293.414805	17.086951
31.624062	1298.781390	17.091968
31.633521	1300.563231	17.096986
31.531905	1292.387173	17.102003
31.498716	1290.669948	17.107021
31.727857	1292.234575	17.112039
31.538170	1293.995973	17.117056
31.666814	1288.355556	17.122074
31.789561	1300.880326	17.127091
31.480036	1304.051350	17.132109
31.507162	1294.663391	17.137127
31.547296	1305.353547	17.142144
31.691928	1299.681336	17.147162
31.798320	1301.335260	17.152179
31.558983	1301.928975	17.157197
31.697263	1295.058265	17.162215
31.540314	1301.647488	17.167232
31.626030	1298.979435	17.172250
31.733163	1295.055119	17.177267
31.410218	1299.778702	17.182285
31.708746	1311.121162	17.187303
31.707125	1324.916572	17.192320
31.937831	1322.836597	17.197338
32.188390	1324.736630	17.202355
31.928203	1319.678524	17.207373
32.456223	1317.852272	17.212391
32.304081	1325.433974	17.217408
32.369652	1320.184328	17.222426
32.336815	1322.707818	17.227443
32.309109	1325.095421	17.232461
32.010116	1321.538194	17.237479
31.954804	1329.149078	17.242496
31.751163	1317.673953	17.247514
32.345539	1325.124492	17.252531
32.465417	1339.134356	17.257549
33.177098	1332.784838	17.262567
32.799582	1325.012086	17.267584
32.959835	1306.814153	17.272602
32.918798	1303.617189	17.277619
32.515837	1301.612223	17.282637
32.601989	1286.506032	17.287655
32.431624	1301.325882	17.292672
32.946738	1304.095683	17.297690
33.002646	1294.388780	17.302707
33.248022	1299.688350	17.307725
33.425146	1282.984430	17.312743
33.322180	1296.906103	17.317760
33.431173	1291.757120	17.322778
33.189442	1271.464320	17.327795
33.162769	1267.194550	17.332813
33.047680	1261.606069	17.337831
32.844624	1267.387623	17.342848
32.969012	1274.562330	17.347866
33.298572	1261.173113	17.352883
32.953271	1269.526230	17.357901
33.097107	1259.331527	17.362919
33.086548	1265.342097	17.367936
33.134421	1256.032599	17.372954
33.141028	1269.457317	17.377971
32.810975	1272.214048	17.382989
33.249626	1280.383726	17.388007
33.493508	1286.355951	17.393024
33.054254	1289.362716	17.398042
33.324611	1287.052149	17.403059
33.453293	1285.175349	17.408077
33.484755	1291.499798	17.413095
33.144398	1295.543232	17.418112
33.455843	1296.232404	17.423130
33.644584	1297.578164	17.428147
33.530288	1291.743094	17.433165
33.634094	1288.723232	17.438183
33.595070	1301.576059	17.443200
33.373247	1296.637563	17.448218
33.686669	1299.742842	17.453235
33.369855	1295.808677	17.458253
33.704604	1297.476219	17.463271
33.865108	1322.188721	17.468288
33.771926	1320.650749	17.473306
33.954059	1321.822419	17.478323
33.737268	1331.860836	17.483341
33.874085	1317.022561	17.488359
34.070710	1334.753376	17.493376
33.911598	1320.425683	17.498394
34.110243	1320.454103	17.503411
33.789336	1326.856423	17.508429
33.900627	1310.905512	17.513447
33.874482	1323.979042	17.518464
33.961460	1322.902051	17.523482
33.850101	1323.756375	17.528499
34.001271	1330.781388	17.533517
34.340580	1346.233078	17.538535
34.485025	1357.079941	17.543552
34.325802	1355.970249	17.548570
34.656488	1353.610277	17.553587
34.729078	1358.737412	17.558605
34.564891	1329.495369	17.563623
34.437852	1330.869996	17.568640
34.413318	1321.448876	17.573658
34.511137	1327.183593	17.578675
34.417421	1343.323369	17.583693
34.441481	1340.491548	17.588711
34.557694	1347.641271	17.593728
34.599388	1348.966990	17.598746
34.895143	1346.057334	17.603763
34.639302	1349.367864	17.608781
34.525990	1340.767363	17.613799
34.720886	1347.431193	17.618816
34.726595	1350.758092	17.623834
34.597129	1343.077957	17.628851
34.292268	1346.176563	17.633869
34.796275	1338.726169	17.638887
35.088705	1352.634142	17.643904
34.917923	1358.849325	17.648922
35.257530	1356.344962	17.653939
34.562694	1369.704861	17.658957
34.810952	1364.912221	17.663975
35.514947	1364.174785	17.668992
35.385068	1361.893329	17.674010
35.649317	1364.705231	17.679027
35.588154	1367.490907	17.684045
35.296259	1356.990228	17.689063
35.104096	1360.268130	17.694080
35.087735	1354.697457	17.699098
35.435614	1347.936369	17.704115
35.625008	1350.206794	17.709133
35.877203	1348.999589	17.714151
35.710694	1352.878322	17.719168
35.271941	1365.940547	17.724186
35.909521	1353.788591	17.729203
35.745186	1366.469392	17.734221
35.702019	1353.767219	17.739239
35.968046	1351.973879	17.744256
35.467433	1349.898132	17.749274
36.260948	1340.220174	17.754291
35.964864	1344.341692	17.759309
35.437344	1332.101914	17.764327
35.955194	1342.837495	17.769344
35.689276	1351.547132	17.774362
35.942119	1350.949245	17.779379
35.699649	1362.965891	17.784397
35.922303	1348.902660	17.789415
36.099337	1354.621860	17.794432
36.043359	1361.011656	17.799450
36.018148	1354.206280	17.804467
35.619660	1348.596763	17.809485
35.886720	1349.377957	17.814503
36.259104	1357.057133	17.819520
36.406455	1358.731027	17.824538
36.143760	1353.642225	17.829555
36.224802	1364.107520	17.834573
36.412013	1368.094783	17.839591
36.738549	1382.216003	17.844608
36.526310	1381.849740	17.849626
36.596821	1368.481439	17.854643
36.341004	1372.707291	17.859661
36.611035	1378.219318	17.864679
36.670659	1375.935102	17.869696
36.707832	1385.384512	17.874714
36.627564	1378.282775	17.879731
36.187098	1382.795216	17.884749
36.730237	1384.821031	17.889767
36.834103	1370.891299	17.894784
36.268561	1380.924328	17.899802
36.840195	1382.111972	17.904819
36.832316	1383.425855	17.909837
36.733530	1385.281206	17.914855
36.863358	1378.170927	17.919872
36.692661	1381.709036	17.924890
36.922266	1373.668429	17.929907
36.759672	1374.160419	17.934925
37.142222	1395.726798	17.939943
37.131444	1399.522967	17.944960
36.883852	1413.568386	17.949978
37.304643	1406.478629	17.954995
37.466499	1410.685464	17.960013
37.223545	1406.880721	17.965031
37.621633	1400.130163	17.970048
37.291011	1405.963677	17.975066
37.768130	1398.841335	17.980083
37.449091	1393.490240	17.985101
37.211911	1372.341463	17.990119
37.216820	1384.200871	17.995136
37.257340	1396.219325	18.000154
37.539045	1392.959253	18.005171
37.365714	1401.442513	18.010189
37.290646	1394.100937	18.015207
37.725499	1401.995730	18.020224
37.682279	1400.831716	18.025242
37.780445	1391.718888	18.030259
37.567322	1386.959620	18.035277
37.553867	1395.449374	18.040295
37.712649	1393.491577	18.045312
37.755742	1414.027038	18.050330
38.455368	1418.973207	18.055347
37.984100	1411.895497	18.060365
37.859358	1401.191421	18.065383
38.199046	1417.036413	18.070400
38.073380	1417.280542	18.075418
38.274811	1431.876916	18.080435
38.562393	1427.672977	18.085453
37.801155	1412.383499	18.090471
37.981392	1409.113911	18.095488
38.017350	1419.131634	18.100506
38.552738	1421.769352	18.105523
38.439058	1424.543689	18.110541
38.321843	1426.308410	18.115559
38.593270	1412.521652	18.120576
38.402369	1420.884226	18.125594
38.379999	1423.463077	18.130611
38.477540	1415.616439	18.135629
38.401330	1421.145479	18.140647
38.753312	1411.998328	18.145664
38.514601	1418.950391	18.150682
38.413093	1415.378034	18.155699
38.753003	1418.156111	18.160717
38.414645	1424.247603	18.165735
38.763674	1417.664634	18.170752
38.790589	1438.837441	18.175770
38.709519	1440.587889	18.180787
39.053871	1440.136990	18.185805
38.952647	1445.684762	18.190823
39.141352	1437.228098	18.195840
39.044715	1447.921400	18.200858
39.052703	1447.795689	18.205875
39.019986	1438.038074	18.210893
39.065343	1443.684313	18.215911
39.341119	1434.131718	18.220928
39.528601	1440.579898	18.225946
39.310406	1442.864932	18.230963
39.099645	1445.985319	18.235981
38.687564	1435.175045	18.240999
39.013930	1428.550564	18.246016
39.084817	1442.945426	18.251034
39.194805	1430.882673	18.256051
39.312263	1446.018985	18.261069
39.426794	1463.999019	18.266087
39.849086	1457.510153	18.271104
39.991913	1467.633764	18.276122
39.829782	1461.371947	18.281139
39.596145	1453.630726	18.286157
39.999133	1445.195135	18.291175
40.070466	1445.543526	18.296192
39.967785	1437.699841	18.301210
39.830143	1434.761417	18.306227
40.205579	1424.460398	18.311245
39.950807	1438.236963	18.316263
40.350003	1433.637318	18.321280
40.399697	1448.629389	18.326298
39.927186	1434.512728	18.331315
39.889956	1435.413003	18.336333
39.741919	1438.356433	18.341351
40.009288	1428.492256	18.346368
39.572707	1444.932029	18.351386
40.060062	1454.461378	18.356403
40.375799	1465.219614	18.361421
40.197278	1472.966791	18.366439
40.298589	1455.589480	18.371456
40.323944	1464.483045	18.376474
40.363163	1466.059965	18.381491
40.175462	1469.572575	18.386509
40.186775	1468.546338	18.391527
40.078593	1469.356442	18.396544
40.296960	1478.667135	18.401562
40.204461	1489.139706	18.406579
40.566964	1492.388044	18.411597
40.262697	1493.614587	18.416615
40.859948	1482.750300	18.421632
40.725632	1484.002138	18.426650
40.405751	1486.285181	18.431667
40.981078	1484.127043	18.436685
40.873754	1483.635862	18.441703
41.365487	1490.676390	18.446720
41.210891	1477.770200	18.451738
41.162757	1480.867108	18.456755
41.497710	1465.377668	18.461773
41.177206	1479.426209	18.466791
41.455779	1465.641366	18.471808
41.210833	1463.890814	18.476826
41.640474	1469.829482	18.481843
41.702166	1470.462145	18.486861
41.509544	1478.563232	18.491879
41.647057	1463.316446	18.496896
41.444957	1477.819702	18.501914
41.519102	1477.411349	18.506931
41.637146	1472.880468	18.511949
41.486188	1475.789746	18.516967
41.760559	1471.556496	18.521984
41.302052	1472.505532	18.527002
41.531492	1467.908896	18.532019
41.761145	1466.489687	18.537037
41.581250	1469.314406	18.542055
41.968100	1469.420205	18.547072
41.986076	1470.077456	18.552090
41.784103	1471.972408	18.557107
42.202421	1473.742219	18.562125
42.007480	1469.757438	18.567143
41.927441	1459.439581	18.572160
42.148992	1465.521884	18.577178
41.802526	1464.153156	18.582195
41.955759	1467.424853	18.587213
41.723424	1474.577450	18.592231
41.942138	1484.641611	18.597248
42.454136	1489.630011	18.602266
42.279024	1500.167893	18.607283
42.685003	1501.534258	18.612301
42.502319	1500.306804	18.617319
42.692649	1490.666016	18.622336
42.492917	1476.431934	18.627354
42.307834	1469.925118	18.632371
42.475893	1474.927372	18.637389
42.445029	1494.832338	18.642407
42.367520	1497.232969	18.647424
42.450696	1495.555828	18.652442
42.282479	1495.965687	18.657459
42.387775	1491.332592	18.662477
42.178285	1495.385034	18.667495
42.377337	1495.766921	18.672512
42.791673	1504.209256	18.677530
43.031819	1518.728809	18.682547
42.981928	1513.981346	18.687565
42.879973	1520.315465	18.692583
43.066546	1525.917398	18.697600
43.061819	1523.092297	18.702618
43.006355	1529.016341	18.707635
43.067662	1520.047356	18.712653
42.799065	1524.522610	18.717671
43.214819	1521.267396	18.722688
43.157764	1515.914447	18.727706
43.115658	1521.656352	18.732723
43.201658	1521.749951	18.737741
43.239741	1534.279140	18.742759
43.593024	1545.141032	18.747776
43.869675	1554.648772	18.752794
43.575581	1557.324774	18.757811
43.958949	1544.568087	18.762829
43.483181	1535.372224	18.767847
43.666791	1525.409312	18.772864
43.975252	1540.836798	18.777882
43.833434	1523.845873	18.782899
43.976198	1514.970436	18.787917
43.791948	1524.389411	18.792935
43.746864	1545.147570	18.797952
44.219695	1534.680295	18.802970
44.103746	1545.981977	18.807987
44.172878	1540.436791	18.813005
44.114087	1544.399239	18.818023
44.323172	1546.773111	18.823040
44.063312	1535.141423	18.828058
43.846441	1545.918161	18.833075
44.294403	1537.478194	18.838093
44.061548	1546.049771	18.843111
44.146321	1552.141456	18.848128
44.424749	1546.542191	18.853146
44.263253	1543.768731	18.858163
44.322799	1532.056401	18.863181
44.073298	1540.383110	18.868199
44.105624	1545.400860	18.873216
44.603081	1543.782021	18.878234
44.628939	1557.328196	18.883251
44.729415	1563.501919	18.888269
44.653114	1565.663390	18.893287
44.881461	1568.776172	18.898304
44.589360	1561.426888	18.903322
44.761057	1576.201171	18.908339
45.007963	1572.524021	18.913357
44.864940	1562.451203	18.918375
44.879938	1557.116579	18.923392
45.245497	1558.296758	18.928410
45.013124	1564.863196	18.933427
45.038819	1553.187971	18.938445
45.044692	1555.630264	18.943463
44.866307	1559.025993	18.948480
44.634607	1565.210439	18.953498
45.081518	1582.879075	18.958515
45.777624	1585.884591	18.963533
45.373373	1598.202316	18.968551
45.494352	1589.229673	18.973568
45.631757	1581.153103	18.978586
45.552852	1585.666924	18.983603
46.015170	1579.040256	18.988621
45.879238	1566.817488	18.993639
45.685411	1553.179977	18.998656
45.812179	1542.757615	19.003674
45.379742	1548.120715	19.008691
45.831539	1560.936668	19.013709
45.741399	1565.918875	19.018727
45.596544	1577.402545	19.023744
45.877059	1578.194901	19.028762
46.006841	1585.808218	19.033779
46.257478	1571.705490	19.038797
46.314865	1579.182414	19.043815
46.369568	1581.176054	19.048832
46.373238	1570.721378	19.053850
46.278959	1576.244026	19.058867
46.453177	1575.742269	19.063885
46.263862	1578.824866	19.068903
46.243583	1583.008084	19.073920
46.504293	1575.609039	19.078938
46.285963	1582.543220	19.083955
46.384443	1569.460642	19.088973
46.413413	1578.926494	19.093991
46.337811	1583.529921	19.099008
46.400414	1580.238511	19.104026
46.130163	1577.660281	19.109043
46.600158	1575.321217	19.114061
46.578604	1579.527480	19.119079
46.378055	1596.447069	19.124096
46.666746	1593.448781	19.129114
46.613647	1606.930564	19.134131
46.295016	1603.163940	19.139149
46.533200	1603.791683	19.144167
46.772418	1618.134715	19.149184
47.158074	1610.835751	19.154202
47.132410	1624.771642	19.159219
46.968827	1618.469452	19.164237
47.137921	1626.049878	19.169255
46.590884	1624.865254	19.174272
47.032696	1622.571023	19.179290
46.853291	1624.643735	19.184307
47.568102	1631.472847	19.189325
47.902934	1639.744223	19.194343
47.533131	1633.922749	19.199360
47.561328	1635.010583	19.204378
47.982482	1651.606435	19.209395
47.888622	1635.800701	19.214413
47.826137	1625.621151	19.219431
47.349288	1618.682853	19.224448
47.814463	1623.015314	19.229466
47.948200	1640.555362	19.234483
47.980096	1641.133142	19.239501
48.117854	1637.618997	19.244519
48.085673	1641.054223	19.249536
48.384264	1637.704287	19.254554
48.240352	1628.336679	19.259571
47.951400	1607.931208	19.264589
47.958161	1623.351834	19.269607
47.983737	1632.869463	19.274624
48.227879	1631.794676	19.279642
47.938490	1638.472194	19.284659
48.242492	1635.200099	19.289677
48.112297	1639.431127	19.294695
48.014291	1636.911660	19.299712
48.606371	1629.467357	19.304730
48.340950	1635.800345	19.309747
48.410585	1629.177506	19.314765
48.579089	1645.931482	19.319783
48.805490	1659.960548	19.324800
49.106437	1653.998060	19.329818
48.502502	1649.876093	19.334835
48.621293	1665.232080	19.339853
48.988897	1659.506932	19.344871
48.504851	1663.147576	19.349888
48.653417	1656.948607	19.354906
48.629366	1670.985844	19.359923
48.833462	1664.054426	19.364941
48.853439	1659.452390	19.369959
48.691922	1673.257757	19.374976
49.197271	1679.121720	19.379994
49.199270	1689.661002	19.385011
49.069052	1687.877184	19.390029
49.308231	1692.096835	19.395047
49.377143	1692.936571	19.400064
49.683515	1680.985077	19.405082
49.584345	1687.868005	19.410099
49.558206	1684.694863	19.415117
49.617846	1685.257404	19.420135
49.516537	1688.377757	19.425152
49.626080	1688.141860	19.430170
49.402727	1684.534180	19.435187
49.588123	1692.567827	19.440205
49.802125	1699.281389	19.445223
49.661030	1715.886113	19.450240
49.992255	1707.981591	19.455258
50.069191	1714.492748	19.460275
50.133013	1709.993250	19.465293
50.477129	1706.752268	19.470311
50.425098	1709.381765	19.475328
50.538606	1706.004310	19.480346
50.422831	1712.578596	19.485363
50.739793	1711.324774	19.490381
50.711053	1690.762561	19.495399
50.491108	1676.895427	19.500416
50.435714	1683.666355	19.505434
50.374262	1678.605414	19.510451
50.334477	1686.557194	19.515469
50.721674	1693.490783	19.520487
50.771206	1702.365901	19.525504
50.898326	1700.966863	19.530522
50.549572	1704.309051	19.535539
50.624191	1702.870315	19.540557
50.703686	1699.137102	19.545575
50.597522	1711.522301	19.550592
50.753506	1705.546091	19.555610
50.840584	1708.150106	19.560627
50.476553	1710.763743	19.565645
50.832408	1708.838900	19.570663
51.130546	1728.148548	19.575680
50.944844	1727.975893	19.580698
51.358436	1728.346146	19.585715
51.289478	1737.203575	19.590733
51.623465	1726.075399	19.595751
51.282714	1731.296946	19.600768
51.623194	1722.744431	19.605786
51.456314	1736.393661	19.610803
51.095311	1729.323854	19.615821
51.363067	1732.907279	19.620839
51.206818	1727.267203	19.625856
51.709136	1732.958859	19.630874
52.109953	1740.272878	19.635891
51.947590	1751.534787	19.640909
52.356707	1734.176083	19.645927
51.839774	1733.830136	19.650944
52.082954	1722.444617	19.655962
52.129586	1725.208898	19.660979
52.005287	1718.272982	19.665997
52.229819	1723.679705	19.671015
52.021273	1725.010433	19.676032
52.028591	1731.629622	19.681050
52.243744	1741.061086	19.686067
52.597636	1760.261903	19.691085
52.832802	1757.517359	19.696103
52.212568	1745.598560	19.701120
52.358799	1748.989984	19.706138
52.540886	1752.491591	19.711155
52.226335	1755.896608	19.716173
52.459442	1745.765488	19.721191
52.703223	1745.885621	19.726208
52.440473	1746.889143	19.731226
52.715760	1746.707587	19.736243
52.452012	1749.223067	19.741261
52.744496	1746.223726	19.746279
53.069761	1772.508759	19.751296
52.837678	1777.663441	19.756314
53.398462	1779.142291	19.761331
53.033061	1775.864495	19.766349
53.200471	1773.590260	19.771367
53.376572	1775.340522	19.776384
53.214069	1767.074727	19.781402
53.381532	1766.311885	19.786419
53.072963	1772.111161	19.791437
53.128885	1767.805084	19.796455
52.879143	1769.790687	19.801472
53.080639	1769.355255	19.806490
53.357734	1779.168570	19.811507
53.451239	1791.138761	19.816525
53.487896	1797.875148	19.821543
53.382176	1798.443130	19.826560
53.798779	1803.491977	19.831578
53.969984	1798.972245	19.836595
54.041015	1798.195508	19.841613
53.861652	1794.145062	19.846631
54.199739	1801.960870	19.851648
54.223356	1799.803836	19.856666
54.262903	1793.883559	19.861683
54.080648	1790.713114	19.866701
53.873675	1788.063702	19.871719
54.065687	1804.864337	19.876736
54.155380	1818.153281	19.881754
54.738620	1817.132360	19.886771
54.344362	1822.234090	19.891789
54.945156	1813.400074	19.896807
54.950408	1819.329492	19.901824
54.778925	1817.346612	19.906842
55.108418	1812.399785	19.911859
54.525887	1807.011629	19.916877
54.965129	1800.048943	19.921895
54.784918	1815.109107	19.926912
54.887605	1814.442067	19.931930
55.052409	1815.483194	19.936947
54.795556	1818.051870	19.941965
54.719228	1815.152788	19.946983
55.004888	1813.585267	19.952000
54.793839	1814.882953	19.957018
54.854969	1809.051996	19.962035
54.928102	1814.324072	19.967053
55.138076	1819.828524	19.972071
55.465046	1828.575715	19.977088
55.371674	1833.990431	19.982106
55.586448	1847.504674	19.987123
55.526059	1852.290690	19.992141
55.474860	1840.924484	19.997159
55.902435	1840.817616	20.002176
55.623233	1840.636877	20.007194
56.034637	1840.200415	20.012211
55.674449	1839.202827	20.017229
55.991557	1838.378890	20.022247
55.813696	1840.645466	20.027264
55.780333	1852.236399	20.032282
55.812334	1839.603617	20.037299
55.790099	1841.974642	20.042317
55.928680	1830.856034	20.047335
55.803545	1836.006741	20.052352
55.802652	1835.011642	20.057370
56.110660	1861.985517	20.062387
56.146861	1862.409047	20.067405
56.575146	1859.638689	20.072423
56.466391	1855.250508	20.077440
56.283956	1856.168642	20.082458
56.392832	1851.856497	20.087475
56.445991	1866.700366	20.092493
56.378764	1859.879703	20.097511
56.719633	1879.724956	20.102528
56.837330	1882.421548	20.107546
57.073970	1882.865703	20.112563
57.316542	1888.647044	20.117581
57.392855	1871.910821	20.122599
56.910026	1879.084762	20.127616
57.206221	1879.069808	20.132634
57.341063	1877.757266	20.137651
57.050028	1883.403276	20.142669
57.365735	1886.935461	20.147687
57.484228	1878.239441	20.152704
57.308918	1882.050476	20.157722
57.658862	1866.180589	20.162739
57.527853	1879.911384	20.167757
57.528042	1875.685406	20.172775
57.664627	1877.462721	20.177792
57.903497	1885.990335	20.182810
58.088108	1867.529824	20.187827
57.617717	1877.184757	20.192845
57.549892	1869.678365	20.197863
57.564107	1875.399623	20.202880
57.495746	1875.390140	20.207898
58.117456	1873.402589	20.212915
57.675251	1872.506031	20.217933
58.164996	1884.544691	20.222951
58.393009	1904.109914	20.227968
57.840022	1907.745142	20.232986
58.514222	1900.725646	20.238003
58.724816	1904.024912	20.243021
58.434731	1905.362119	20.248039
58.513236	1903.453035	20.253056
58.873622	1894.688457	20.258074
58.574190	1894.588638	20.263091
58.484278	1902.717363	20.268109
58.358136	1906.844641	20.273127
58.405234	1901.901805	20.278144
58.692865	1900.858356	20.283162
59.024353	1897.358017	20.288179
58.588514	1898.591102	20.293197
58.917806	1894.279320	20.298215
59.160751	1904.274768	20.303232
59.235466	1922.752896	20.308250
59.184454	1917.468488	20.313267
58.935376	1919.071322	20.318285
59.222006	1919.865438	20.323303
59.494175	1924.106048	20.328320
59.294253	1925.408587	20.333338
59.290029	1923.093565	20.338355
59.689707	1920.380706	20.343373
59.802557	1924.376929	20.348391
59.578442	1914.899642	20.353408
59.427259	1924.810213	20.358426
59.406862	1918.664812	20.363443
59.643115	1922.564934	20.368461
59.280528	1927.100805	20.373479
59.576648	1920.202405	20.378496
59.431436	1942.079704	20.383514
60.005720	1941.602390	20.388531
59.920245	1938.231971	20.393549
59.840399	1946.390148	20.398567
60.098022	1938.924516	20.403584
60.173445	1944.551374	20.408602
60.340762	1960.257857	20.413619
60.277601	1968.604218	20.418637
60.522123	1965.709658	20.423655
60.595394	1967.911286	20.428672
60.632290	1973.969362	20.433690
60.968243	1957.342651	20.438707
60.746470	1960.231504	20.443725
60.611093	1970.706408	20.448743
60.822427	1954.741357	20.453760
60.802982	1962.434779	20.458778
61.187631	1948.752745	20.463795
61.177821	1959.040236	20.468813
61.058992	1962.907651	20.473831
60.999015	1950.193609	20.478848
60.779080	1959.849093	20.483866
60.887363	1961.531908	20.488883
61.142004	1968.775450	20.493901
61.088807	1975.078028	20.498919
61.451565	1986.286690	20.503936
61.407473	1985.161753	20.508954
61.318131	1989.241597	20.513971
61.305637	1989.905115	20.518989
61.219157	1994.423857	20.524007
61.936778	1995.816821	20.529024
62.059502	2012.233132	20.534042
62.369487	2000.252841	20.539059
62.004108	1991.181270	20.544077
61.845174	1986.090366	20.549095
62.150968	2004.656172	20.554112
62.096270	2009.412550	20.559130
62.184308	2012.481420	20.564147
61.909109	2015.769321	20.569165
62.242570	2018.522205	20.574183
62.686175	2007.526005	20.579200
62.304840	2018.807964	20.584218
62.670941	2005.217153	20.589235
62.711076	2011.781795	20.594253
62.376783	2012.914940	20.599271
62.578525	2009.894410	20.604288
62.705373	2020.062772	20.609306
62.709773	2007.546251	20.614323
62.804630	2008.880121	20.619341
62.524088	2008.801177	20.624359
62.958594	2015.413663	20.629376
63.123556	2031.508406	20.634394
63.149060	2037.000287	20.639411
63.215177	2034.124342	20.644429
63.231727	2031.214508	20.649447
63.282773	2024.430809	20.654464
62.948717	2031.571432	20.659482
63.212574	2033.132335	20.664499
63.213064	2030.998011	20.669517
63.208614	2035.709825	20.674535
63.413608	2019.486312	20.679552
63.540779	2040.946824	20.684570
63.474212	2056.363139	20.689587
64.138649	2047.933379	20.694605
63.751225	2055.701785	20.699623
63.796301	2061.147901	20.704640
63.802469	2066.328043	20.709658
63.679202	2057.813837	20.714675
64.126624	2063.008044	20.719693
63.922174	2060.656986	20.724711
64.146687	2054.656655	20.729728
64.067324	2059.215572	20.734746
64.338117	2068.417121	20.739763
64.655495	2074.532559	20.744781
64.572828	2082.187335	20.749799
64.935741	2082.347910	20.754816
64.551759	2088.719290	20.759834
64.759063	2079.822569	20.764851
64.860796	2085.385657	20.769869
64.564281	2081.484527	20.774887
64.963892	2076.983842	20.779904
64.733800	2077.824474	20.784922
64.565915	2076.739789	20.789939
64.983996	2073.862034	20.794957
64.896998	2073.432810	20.799975
65.280757	2079.897458	20.804992
64.934776	2097.139401	20.810010
64.992796	2099.528231	20.815027
65.412088	2103.096401	20.820045
65.316805	2113.308828	20.825063
65.611602	2105.884183	20.830080
65.704579	2101.473429	20.835098
65.793025	2108.065909	20.840115
66.078133	2100.996817	20.845133
65.754600	2105.236481	20.850151
65.888840	2099.434603	20.855168
65.979798	2099.674235	20.860186
66.081167	2104.198797	20.865203
66.233697	2092.015467	20.870221
65.975731	2102.294689	20.875239
66.336725	2095.498030	20.880256
66.173483	2087.695182	20.885274
66.161881	2097.194866	20.890291
66.749260	2113.525793	20.895309
66.494928	2116.386620	20.900327
66.754626	2116.299780	20.905344
66.687799	2120.964506	20.910362
66.628990	2116.983703	20.915379
66.636776	2115.255640	20.920397
66.695149	2117.747170	20.925415
66.817896	2125.539877	20.930432
66.953097	2126.878863	20.935450
66.616072	2130.545178	20.940467
66.760424	2118.019089	20.945485
66.792207	2127.688355	20.950503
66.549067	2121.550758	20.955520
67.009982	2147.702465	20.960538
67.427556	2151.650859	20.965555
67.708991	2139.644497	20.970573
67.378614	2156.478789	20.975591
67.311897	2146.331491	20.980608
67.111901	2149.323059	20.985626
67.058504	2149.557943	20.990643
67.677559	2163.428900	20.995661
67.756236	2175.910128	21.000679
67.545154	2172.775104	21.005696
67.665267	2176.600104	21.010714
67.693763	2174.692998	21.015731
67.805464	2166.747564	21.020749
67.622180	2175.938029	21.025767
68.095545	2177.818464	21.030784
68.162988	2187.262545	21.035802
68.012784	2202.684638	21.040819
68.401077	2191.783724	21.045837
68.496550	2198.238459	21.050855
68.454279	2200.082545	21.055872
68.686776	2201.096306	21.060890
68.441139	2200.966677	21.065907
68.741884	2192.179955	21.070925
68.539341	2202.212626	21.075943
68.893914	2198.468617	21.080960
68.688548	2194.629083	21.085978
69.113077	2199.826748	21.090995
69.164275	2197.273730	21.096013
68.893939	2205.273934	21.101031
69.311087	2216.880425	21.106048
69.698664	2221.713760	21.111066
69.532986	2220.462553	21.116083
69.822561	2225.738169	21.121101
69.648309	2215.508695	21.126119
69.238022	2210.459097	21.131136
69.648061	2210.231914	21.136154
69.614408	2219.712109	21.141171
69.504035	2205.982197	21.146189
69.561847	2217.923217	21.151207
69.633823	2211.268638	21.156224
69.791372	2216.318551	21.161242
69.480835	2218.687548	21.166259
70.064573	2228.136794	21.171277
69.838812	2240.870250	21.176295
69.864108	2249.543799	21.181312
70.046855	2251.120568	21.186330
70.215277	2244.155845	21.191347
70.285503	2250.977797	21.196365
70.315628	2275.577268	21.201383
70.384333	2267.828302	21.206400
70.619842	2271.607769	21.211418
70.731429	2269.886059	21.216435
70.901588	2271.434213	21.221453
70.411920	2276.811794	21.226471
70.968748	2269.728570	21.231488
71.140601	2256.611566	21.236506
71.142367	2271.646258	21.241523
71.225641	2258.698307	21.246541
71.422824	2271.198501	21.251559
71.697177	2279.165306	21.256576
71.315366	2274.580650	21.261594
71.168193	2289.862951	21.266611
71.629288	2285.515772	21.271629
71.684678	2293.485904	21.276647
71.958994	2287.181137	21.281664
72.188921	2294.963597	21.286682
72.066146	2300.021936	21.291699
71.609319	2297.025368	21.296717
71.937867	2299.610218	21.301735
72.030805	2298.765641	21.306752
72.285855	2296.499994	21.311770
71.861721	2289.816413	21.316787
71.871733	2286.943052	21.321805
72.002171	2294.231405	21.326823
72.151727	2297.388535	21.331840
72.458624	2290.434243	21.336858
72.554052	2291.866470	21.341875
72.676633	2293.867032	21.346893
72.159138	2302.873740	21.351911
72.514435	2301.227274	21.356928
72.662653	2314.690387	21.361946
72.577189	2313.840418	21.366963
72.772007	2312.095816	21.371981
72.787018	2313.111871	21.376999
72.732597	2313.940643	21.382016
72.608971	2326.974918	21.387034
73.107521	2346.435894	21.392051
73.516870	2338.353895	21.397069
73.383503	2342.585640	21.402087
73.427301	2347.741905	21.407104
73.679733	2336.074473	21.412122
73.381593	2344.482923	21.417139
73.533574	2336.961822	21.422157
73.432246	2336.268429	21.427175
73.494581	2344.860284	21.432192
73.824682	2356.242364	21.437210
73.742234	2365.786664	21.442227
73.898491	2361.020428	21.447245
73.662918	2364.097480	21.452263
73.716332	2360.097176	21.457280
73.906573	2366.563791	21.462298
74.067715	2387.191555	21.467315
74.337411	2380.570581	21.472333
74.491995	2391.394438	21.477351
74.507275	2391.047816	21.482368
74.958293	2389.883085	21.487386
74.675769	2392.457300	21.492403
74.975541	2377.201157	21.497421
75.115012	2390.866583	21.502439
74.610960	2387.133729	21.507456
74.780016	2388.448607	21.512474
74.910053	2398.259196	21.517491
75.528458	2401.379373	21.522509
75.556928	2401.106151	21.527527
75.278574	2409.140471	21.532544
75.725835	2400.298572	21.537562
75.442960	2403.084271	21.542579
75.456641	2402.294594	21.547597
75.688416	2401.872227	21.552615
75.478084	2403.316302	21.557632
75.892596	2394.743243	21.562650
75.670944	2390.414620	21.567667
75.866566	2388.731689	21.572685
75.891364	2393.704507	21.577703
75.738568	2399.669862	21.582720
75.856797	2396.806843	21.587738
75.848811	2406.239971	21.592755
76.061117	2415.574680	21.597773
76.482243	2430.733930	21.602791
76.255387	2420.278410	21.607808
76.404869	2420.687461	21.612826
76.677831	2433.322046	21.617843
76.384882	2417.617896	21.622861
76.292790	2427.126434	21.627879
76.554215	2440.047990	21.632896
77.177493	2452.031831	21.637914
76.930826	2452.169307	21.642931
76.646456	2450.848434	21.647949
77.137717	2454.309449	21.652967
77.036001	2456.111080	21.657984
77.198838	2444.564367	21.663002
77.274098	2452.042285	21.668019
77.590818	2456.644943	21.673037
77.628289	2449.103448	21.678055
77.425411	2464.403053	21.683072
77.585171	2461.020898	21.688090
77.625145	2479.297975	21.693107
77.819145	2473.389961	21.698125
77.986289	2475.059113	21.703143
78.003921	2479.107920	21.708160
78.064273	2464.598593	21.713178
77.768633	2483.853138	21.718195
77.902538	2479.527999	21.723213
78.089212	2472.621954	21.728231
77.914317	2482.137594	21.733248
78.405719	2491.121623	21.738266
78.341950	2493.056327	21.743283
78.290286	2503.078683	21.748301
78.714941	2498.889476	21.753319
78.333176	2499.941170	21.758336
78.847536	2499.932483	21.763354
78.787183	2504.651761	21.768371
79.035122	2505.216111	21.773389
79.142963	2510.772431	21.778407
78.792458	2530.050719	21.783424
79.304052	2522.772530	21.788442
79.083528	2539.015727	21.793459
79.210408	2529.414766	21.798477
79.302064	2527.973123	21.803495
79.317064	2527.413938	21.808512
79.819636	2524.255516	21.813530
79.669340	2530.884704	21.818547
79.523720	2524.381513	21.823565
79.758297	2543.282648	21.828583
79.669526	2549.030325	21.833600
79.791606	2556.573744	21.838618
79.952513	2556.870659	21.843635
79.922885	2552.289202	21.848653
80.043631	2553.258566	21.853671
80.273640	2571.122657	21.858688
80.024997	2570.426964	21.863706
80.426409	2586.815285	21.868723
80.463984	2581.344661	21.873741
80.662003	2585.908421	21.878759
80.701831	2585.939621	21.883776
80.822257	2575.932600	21.888794
80.946631	2584.459550	21.893811
80.864880	2573.519555	21.898829
80.853527	2582.005279	21.903847
81.020310	2609.379139	21.908864
81.540086	2597.356438	21.913882
81.446072	2604.040873	21.918899
81.513677	2610.384658	21.923917
81.497422	2604.644614	21.928935
81.305220	2614.270301	21.933952
81.570152	2600.237894	21.938970
81.475254	2606.033463	21.943987
81.326813	2602.208382	21.949005
82.002016	2606.868836	21.954023
81.812297	2624.194451	21.959040
81.952079	2633.257867	21.964058
82.114586	2633.998239	21.969075
82.012570	2629.246104	21.974093
82.092723	2633.134160	21.979111
82.086990	2640.744927	21.984128
82.411650	2626.009625	21.989146
82.337642	2612.888298	21.994163
82.895926	2641.233022	21.999181
82.732884	2636.922149	22.004199
82.650614	2639.504069	22.009216
83.034643	2638.617396	22.014234
82.950210	2651.162337	22.019251
82.763742	2658.464550	22.024269
83.146295	2661.406646	22.029287
83.190278	2659.283512	22.034304
82.839088	2656.024816	22.039322
83.302768	2656.725372	22.044339
82.785663	2658.086196	22.049357
83.296197	2643.197934	22.054375
83.359412	2680.074998	22.059392
83.536318	2674.922540	22.064410
83.485900	2679.550453	22.069427
83.400934	2683.350997	22.074445
84.005576	2679.351526	22.079463
84.000058	2680.906476	22.084480
84.171036	2684.099104	22.089498
84.270277	2669.894948	22.094515
83.893657	2676.188172	22.099533
84.327483	2677.865785	22.104551
84.167406	2689.121296	22.109568
84.363362	2687.902868	22.114586
84.705350	2692.450214	22.119603
84.484995	2694.734998	22.124621
84.782138	2687.310476	22.129639
84.700449	2700.791659	22.134656
84.774260	2690.091097	22.139674
84.943562	2704.740472	22.144691
84.790567	2720.547811	22.149709
85.206609	2711.921568	22.154727
84.918299	2726.420626	22.159744
85.255323	2714.929020	22.164762
85.399944	2721.441950	22.169779
85.099179	2715.327474	22.174797
85.465053	2730.176106	22.179815
85.385790	2753.991715	22.184832
85.417098	2750.057194	22.189850
85.634814	2751.214796	22.194867
85.677334	2757.358862	22.199885
85.714241	2754.494726	22.204903
85.912846	2775.693975	22.209920
86.338763	2781.721574	22.214938
86.473304	2771.986113	22.219955
86.113446	2773.890134	22.224973
86.485179	2767.446539	22.229991
86.039929	2780.280693	22.235008
86.530693	2771.799882	22.240026
86.733061	2778.701685	22.245043
86.806370	2796.147959	22.250061
86.909097	2799.908284	22.255079
87.210605	2797.975416	22.260096
87.027341	2797.550751	22.265114
87.556448	2794.343376	22.270131
87.399876	2785.635474	22.275149
87.864444	2789.149037	22.280167
87.338699	2789.250607	22.285184
87.300933	2785.533867	22.290202
87.419930	2786.295257	22.295219
87.040912	2787.613062	22.300237
87.541237	2795.536673	22.305255
87.584790	2816.674734	22.310272
88.002297	2815.073000	22.315290
88.041026	2810.403330	22.320307
88.055507	2820.822401	22.325325
88.344646	2811.840400	22.330343
88.432688	2822.568524	22.335360
88.493629	2819.271223	22.340378
88.398436	2821.050552	22.345395
88.218422	2830.027458	22.350413
88.541948	2813.206617	22.355431
88.532381	2823.124933	22.360448
88.723528	2843.846747	22.365466
89.120105	2830.656085	22.370483
89.136893	2846.813703	22.375501
89.039538	2840.086598	22.380519
88.683273	2848.319140	22.385536
89.013972	2841.645705	22.390554
89.095417	2841.990480	22.395571
88.891605	2862.188159	22.400589
89.741091	2863.936881	22.405607
89.504978	2868.434677	22.410624
89.404453	2871.286221	22.415642
89.865517	2874.385793	22.420659
89.566204	2875.612007	22.425677
89.643235	2881.688966	22.430695
89.762098	2880.108115	22.435712
89.668867	2895.152109	22.440730
90.202794	2893.888915	22.445747
90.199888	2901.676122	22.450765
90.331880	2894.213984	22.455783
89.948365	2903.926765	22.460800
90.042210	2912.868443	22.465818
90.625579	2922.032335	22.470835
90.751731	2932.018328	22.475853
90.760631	2929.558446	22.480871
90.637327	2929.028924	22.485888
90.948427	2926.266048	22.490906
91.554891	2926.872019	22.495923
91.053896	2929.894465	22.500941
91.213145	2936.541283	22.505959
91.386862	2950.562164	22.510976
91.363904	2952.110984	22.515994
91.755294	2955.386730	22.521011
91.734077	2958.755459	22.526029
91.693514	2947.494556	22.531047
91.687403	2952.493557	22.536064
91.674931	2955.668300	22.541082
91.934425	2947.034085	22.546099
91.897413	2975.926807	22.551117
92.180067	2971.369317	22.556135
92.289073	2971.033486	22.561152
92.442468	2981.775270	22.566170
92.616023	2968.023092	22.571187
92.551741	2991.424735	22.576205
92.846040	2976.865815	22.581223
92.579347	2979.608371	22.586240
92.668103	2976.838733	22.591258
92.951050	2989.989864	22.596275
92.727779	3000.178864	22.601293
92.929695	2994.721337	22.606311
93.474319	3001.784879	22.611328
93.222692	2995.072715	22.616346
93.360867	2995.441926	22.621363
93.406799	3002.150127	22.626381
93.508711	3019.888375	22.631399
93.595431	3030.713326	22.636416
93.702141	3027.489877	22.641434
93.780314	3026.744179	22.646451
93.756275	3024.836645	22.651469
94.270743	3025.373258	22.656487
94.334769	3028.868790	22.661504
94.125201	3037.716466	22.666522
94.639718	3047.097795	22.671539
94.277894	3050.042407	22.676557
94.235707	3050.792012	22.681575
94.398046	3054.673209	22.686592
94.192521	3051.664256	22.691610
94.787042	3053.825085	22.696627
94.656688	3062.381244	22.701645
94.637024	3077.408462	22.706663
95.169809	3079.491360	22.711680
95.059635	3082.628819	22.716698
95.071506	3088.086326	22.721715
95.075511	3092.725002	22.726733
95.240947	3089.366181	22.731751
95.558436	3086.488427	22.736768
95.392565	3109.690973	22.741786
95.512077	3105.540901	22.746803
95.732184	3111.694180	22.751821
95.975580	3104.215003	22.756839
96.064110	3100.516571	22.761856
96.009843	3103.010837	22.766874
96.164239	3101.414610	22.771891
96.111910	3121.352392	22.776909
96.370403	3123.480880	22.781927
96.674371	3131.220746	22.786944
96.554547	3129.870497	22.791962
96.515379	3125.410151	22.796979
96.825072	3131.800143	22.801997
97.005302	3117.810879	22.807015
97.236848	3122.875959	22.812032
96.742728	3127.556874	22.817050
97.437256	3142.519800	22.822067
96.911206	3149.404230	22.827085
97.111657	3154.135878	22.832103
97.399402	3157.162336	22.837120
97.439733	3159.303856	22.842138
97.653738	3149.550623	22.847155
97.315378	3166.928315	22.852173
97.536461	3176.381718	22.857191
97.817618	3179.519914	22.862208
97.904130	3180.473746	22.867226
97.962637	3181.188512	22.872243
98.032486	3195.606039	22.877261
98.257863	3205.560756	22.882279
99.043213	3199.792795	22.887296
98.738480	3206.657794	22.892314
98.834120	3196.328485	22.897331
98.320267	3205.107523	22.902349
98.815808	3198.996748	22.907367
98.814766	3203.957583	22.912384
98.796624	3218.907119	22.917402
99.187984	3222.574299	22.922419
99.412400	3228.256397	22.927437
99.484417	3229.518966	22.932455
99.514172	3226.350000	22.937472
99.467720	3231.649914	22.942490
99.992801	3231.100036	22.947507
99.801632	3225.753429	22.952525
100.125837	3230.227506	22.957543
100.112170	3225.340024	22.962560
99.798827	3227.415909	22.967578
99.936954	3240.284208	22.972595
100.161466	3252.191230	22.977613
100.122448	3243.680483	22.982631
100.356494	3258.338914	22.987648
100.323758	3258.779452	22.992666
100.349664	3256.028085	22.997683
100.564183	3273.842405	23.002701
100.736278	3276.325460	23.007719
100.819359	3276.747145	23.012736
101.053597	3284.109665	23.017754
100.641020	3281.137045	23.022771
101.057269	3294.865152	23.027789
101.068643	3302.033595	23.032807
101.441792	3296.042739	23.037824
101.185546	3318.600320	23.042842
101.642711	3310.461448	23.047859
101.535904	3305.941813	23.052877
101.264031	3328.294112	23.057895
101.780113	3330.242408	23.062912
101.551192	3345.471998	23.067930
101.938852	3335.011383	23.072947
101.942068	3332.247630	23.077965
102.012947	3351.158052	23.082983
102.566751	3353.912754	23.088000
102.587028	3357.462486	23.093018
103.171711	3360.564846	23.098035
103.042240	3363.952440	23.103053
103.002256	3364.863520	23.108071
103.174685	3355.380479	23.113088
102.920630	3363.151381	23.118106
103.270689	3357.121421	23.123123
103.060107	3349.656544	23.128141
103.025522	3361.496463	23.133159
103.661515	3368.698941	23.138176
103.392909	3385.140001	23.143194
103.599570	3386.206568	23.148211
103.535911	3386.367970	23.153229
103.575222	3383.687588	23.158247
103.893182	3391.904438	23.163264
104.026244	3410.860115	23.168282
104.218286	3406.053755	23.173299
104.441004	3409.223760	23.178317
104.022224	3408.311789	23.183335
104.609296	3401.750645	23.188352
104.455592	3401.410822	23.193370
104.669352	3422.612765	23.198387
104.923404	3430.852461	23.203405
104.729351	3432.096659	23.208423
105.095911	3436.100721	23.213440
105.147228	3434.020362	23.218458
105.138871	3438.282419	23.223475
105.191385	3431.520702	23.228493
105.340131	3451.555817	23.233511
105.921580	3452.247869	23.238528
105.543355	3460.579270	23.243546
105.750115	3456.722510	23.248563
106.342082	3453.581339	23.253581
106.004639	3464.766873	23.258599
106.111104	3456.831498	23.263616
106.138618	3453.556944	23.268634
106.029428	3453.280201	23.273651
106.471530	3476.264919	23.278669
106.390054	3488.453311	23.283687
106.522577	3478.931941	23.288704
106.629278	3486.560658	23.293722
106.840993	3489.847481	23.298739
106.948376	3483.070323	23.303757
106.947198	3510.211448	23.308775
106.773001	3505.250545	23.313792
107.206814	3511.180260	23.318810
107.154879	3516.186663	23.323827
107.214919	3506.304055	23.328845
107.069235	3529.475519	23.333863
107.587963	3528.078178	23.338880
107.719554	3535.894535	23.343898
107.502828	3541.232694	23.348915
107.646043	3549.905483	23.353933
107.825010	3556.317376	23.358951
107.974625	3567.395660	23.363968
108.402073	3565.141347	23.368986
108.439996	3574.119473	23.374003
108.750269	3561.195324	23.379021
108.629199	3568.726094	23.384039
108.655954	3563.736108	23.389056
108.945749	3575.152558	23.394074
108.856702	3586.072072	23.399091
108.935516	3588.506499	23.404109
109.163498	3598.360630	23.409127
109.240121	3595.198370	23.414144
109.316074	3600.057155	23.419162
109.084703	3591.596297	23.424179
109.745116	3598.775533	23.429197
109.463732	3619.913951	23.434215
109.776280	3610.232648	23.439232
109.919882	3613.546566	23.444250
109.675027	3611.502015	23.449267
110.149022	3622.164975	23.454285
110.055807	3643.856864	23.459303
110.088494	3644.846050	23.464320
110.260278	3644.630890	23.469338
110.470588	3643.047366	23.474355
110.687576	3652.045784	23.479373
110.561980	3661.336599	23.484391
110.438811	3668.861859	23.489408
110.810122	3677.152286	23.494426
110.790991	3670.987477	23.499443
111.227126	3683.925921	23.504461
111.540334	3701.592818	23.509479
111.739366	3692.895793	23.514496
111.864789	3701.144803	23.519514
111.628307	3699.785148	23.524531
111.422889	3696.581146	23.529549
111.552981	3691.704276	23.534567
111.778010	3710.496198	23.539584
112.090903	3718.451435	23.544602
112.086520	3732.934162	23.549619
112.599555	3712.481237	23.554637
112.479781	3725.687711	23.559655
112.526667	3734.145088	23.564672
112.598453	3752.327415	23.569690
112.656482	3751.225146	23.574707
113.133423	3745.336965	23.579725
112.913994	3745.205322	23.584743
113.305783	3741.585492	23.589760
113.427793	3755.325499	23.594778
113.279872	3768.502430	23.599795
113.658851	3767.733089	23.604813
114.094977	3770.823998	23.609831
113.781189	3769.073592	23.614848
113.636651	3777.124564	23.619866
113.809487	3772.454371	23.624883
113.746832	3771.726529	23.629901
114.232214	3795.727875	23.634919
114.470645	3804.091640	23.639936
114.471685	3800.167397	23.644954
114.268974	3796.358521	23.649971
114.586139	3793.071985	23.654989
114.890503	3805.359909	23.660007
114.953288	3816.479969	23.665024
115.086961	3826.882265	23.670042
115.009215	3832.457693	23.675059
115.460914	3825.972029	23.680077
115.136901	3819.010481	23.685095
115.224178	3826.141745	23.690112
115.846065	3830.905152	23.695130
115.748753	3857.207238	23.700147
115.974276	3851.693518	23.705165
116.001938	3855.520910	23.710183
116.205893	3854.979889	23.715200
116.208423	3855.484670	23.720218
115.759916	3858.485571	23.725235
116.227527	3841.587316	23.730253
116.037497	3858.689122	23.735271
115.927008	3863.556529	23.740288
116.444282	3875.233858	23.745306
116.445519	3884.703752	23.750323
116.323236	3886.103401	23.755341
116.870849	3902.132159	23.760359
116.791053	3909.857833	23.765376
117.134305	3913.231955	23.770394
117.327917	3926.133336	23.775411
117.657717	3921.545690	23.780429
117.599844	3936.500152	23.785447
117.688647	3933.041667	23.790464
117.613694	3936.932201	23.795482
117.851924	3928.728990	23.800499
118.277339	3943.924839	23.805517
118.419281	3960.911345	23.810535
118.683386	3960.639495	23.815552
118.523891	3951.538069	23.820570
118.193466	3965.427866	23.825587
118.722865	3951.420783	23.830605
118.588378	3953.473338	23.835623
118.789324	3973.100001	23.840640
119.144435	3973.480043	23.845658
118.910620	3991.312200	23.850675
119.225912	3976.226356	23.855693
119.440251	3985.116731	23.860711
119.258647	3989.766044	23.865728
119.709968	4000.748429	23.870746
119.947724	4016.835492	23.875763
119.766959	4008.429785	23.880781
119.917760	4003.715148	23.885799
120.161096	4015.806265	23.890816
120.123591	4021.874746	23.895834
120.210690	4033.102352	23.900851
120.682611	4030.712221	23.905869
120.839546	4041.227739	23.910887
120.403443	4043.568256	23.915904
120.805279	4028.574294	23.920922
120.540826	4058.746742	23.925939
121.164069	4057.663925	23.930957
121.386083	4060.660929	23.935975
121.268196	4061.444425	23.940992
121.591192	4056.350715	23.946010
121.548066	4064.245198	23.951027
121.774868	4080.691282	23.956045
121.692748	4085.882828	23.961063
121.853478	4090.014193	23.966080
122.170588	4085.876308	23.971098
122.031883	4093.678800	23.976115
122.525910	4105.574762	23.981133
122.536538	4108.461609	23.986151
122.499380	4118.142384	23.991168
122.717901	4113.696420	23.996186
122.686991	4120.281238	24.001203
122.801500	4113.549482	24.006221
123.039038	4123.603173	24.011239
123.078338	4138.464109	24.016256
123.480687	4141.175613	24.021274
123.258449	4141.457483	24.026291
123.614605	4133.262525	24.031309
123.380832	4141.786057	24.036327
123.704981	4157.562409	24.041344
123.700559	4170.830414	24.046362
123.937230	4169.462175	24.051379
123.763613	4175.696663	24.056397
123.828610	4170.095712	24.061415
124.123525	4189.401081	24.066432
124.502614	4191.686870	24.071450
124.480801	4197.865032	24.076467
124.581932	4195.161244	24.081485
124.843503	4196.834188	24.086503
124.791205	4221.810317	24.091520
124.900547	4223.227811	24.096538
125.077750	4219.602583	24.101555
125.594170	4213.826978	24.106573
125.699972	4220.927781	24.111591
125.656021	4223.383496	24.116608
126.056276	4223.862753	24.121626
126.162205	4241.281595	24.126643
126.442336	4234.582902	24.131661
126.487485	4234.531320	24.136679
126.407862	4243.579765	24.141696
126.740717	4237.575562	24.146714
126.960270	4238.263615	24.151731
126.741184	4233.763156	24.156749
126.661215	4236.328024	24.161767
126.708301	4235.890236	24.166784
126.747652	4230.610502	24.171802
126.861107	4255.417386	24.176819
127.152975	4263.106277	24.181837
127.105597	4264.702598	24.186855
126.908547	4283.186947	24.191872
127.193567	4291.695224	24.196890
127.133585	4298.694458	24.201907
127.473794	4307.985818	24.206925
128.117938	4315.721721	24.211943
127.926706	4336.537806	24.216960
128.281983	4329.689557	24.221978
128.479612	4342.257886	24.226995
128.481821	4344.524032	24.232013
128.878712	4349.473833	24.237031
128.386273	4348.278326	24.242048
128.840050	4342.520960	24.247066
128.638565	4360.078435	24.252083
129.024939	4373.318682	24.257101
129.207481	4371.165203	24.262119
129.201598	4383.462613	24.267136
129.664064	4390.978313	24.272154
129.952716	4407.367604	24.277171
130.019639	4399.170960	24.282189
130.356748	4397.879333	24.287207
130.109390	4407.224292	24.292224
130.344835	4405.180147	24.297242
130.443192	4399.677130	24.302259
130.222391	4412.737164	24.307277
130.658397	4424.676877	24.312295
130.635537	4430.847035	24.317312
130.856502	4424.624311	24.322330
130.612678	4441.354134	24.327347
130.812614	4440.557816	24.332365
131.097567	4443.764550	24.337383
130.891473	4459.702169	24.342400
131.353186	4466.773864	24.347418
131.721587	4489.419511	24.352435
131.603237	4486.115035	24.357453
131.851305	4483.421431	24.362471
131.779763	4496.146444	24.367488
132.319591	4502.075068	24.372506
132.223270	4501.384681	24.377523
132.546555	4511.172756	24.382541
132.432857	4507.507601	24.387559
132.745214	4527.484222	24.392576
133.343272	4533.414995	24.397594
133.320080	4540.725599	24.402611
133.152757	4542.505687	24.407629
133.763616	4535.414843	24.412647
133.492662	4537.824065	24.417664
133.754124	4527.578942	24.422682
133.396390	4540.122377	24.427699
133.534129	4535.470392	24.432717
133.811311	4528.481466	24.437735
133.794780	4545.127951	24.442752
134.230555	4547.238598	24.447770
134.192899	4562.449001	24.452787
134.430750	4560.269768	24.457805
134.744465	4558.127542	24.462823
134.256288	4573.701060	24.467840
134.447950	4579.715136	24.472858
134.804925	4587.832812	24.477875
134.585227	4600.488025	24.482893
134.725429	4605.482928	24.487911
135.425271	4619.009933	24.492928
135.658754	4614.216008	24.497946
135.730232	4611.859656	24.502963
135.503194	4625.760417	24.507981
135.839062	4642.610694	24.512999
135.705013	4644.296272	24.518016
136.362028	4641.818985	24.523034
136.299114	4652.617160	24.528051
136.389562	4667.385044	24.533069
136.778799	4668.990754	24.538087
137.018473	4667.241199	24.543104
136.986816	4675.589674	24.548122
137.402072	4665.804029	24.553139
137.388023	4667.223168	24.558157
137.489675	4667.563841	24.563175
137.430899	4678.781892	24.568192
137.576636	4689.408388	24.573210
137.894947	4699.103691	24.578227
137.839052	4696.082544	24.583245
138.109645	4696.219521	24.588263
137.999675	4701.552143	24.593280
138.178017	4707.052642	24.598298
138.270209	4715.994052	24.603315
138.526091	4715.490841	24.608333
138.925899	4712.553047	24.613351
138.270131	4732.634895	24.618368
139.088387	4740.043600	24.623386
139.215379	4763.148732	24.628403
138.473824	4754.905906	24.633421
139.097670	4760.656859	24.638439
139.558119	4773.181072	24.643456
139.859414	4765.028769	24.648474
139.641979	4779.659698	24.653491
139.770835	4775.732873	24.658509
140.106708	4786.855493	24.663527
140.329786	4795.288496	24.668544
140.269611	4789.830588	24.673562
140.490586	4800.494272	24.678579
140.485971	4797.493724	24.683597
140.972722	4817.633109	24.688615
140.991308	4831.396365	24.693632
140.941382	4817.736804	24.698650
141.083853	4827.902434	24.703667
141.338344	4829.511651	24.708685
141.527384	4845.245390	24.713703
141.480089	4848.939785	24.718720
141.542055	4859.088098	24.723738
141.871244	4853.589092	24.728755
141.691641	4870.776502	24.733773
142.384009	4875.925450	24.738791
142.154341	4890.612068	24.743808
142.306682	4880.408476	24.748826
142.360216	4888.045926	24.753843
142.334240	4897.978914	24.758861
142.893648	4908.057197	24.763879
142.475840	4926.226950	24.768896
142.694008	4913.755273	24.773914
142.809763	4934.779451	24.778931
142.951937	4946.671522	24.783949
143.446440	4951.573007	24.788967
143.580922	4967.475808	24.793984
143.703131	4972.350172	24.799002
143.759599	4978.408919	24.804019
144.049149	4983.920962	24.809037
144.146303	4993.314550	24.814055
144.173255	4998.544188	24.819072
144.651554	4991.372002	24.824090
145.103049	5008.887057	24.829107
144.749550	5007.013946	24.834125
144.899201	5027.966462	24.839143
144.861889	5028.318421	24.844160
145.249341	5033.295213	24.849178
145.557100	5037.978889	24.854195
145.661536	5059.273672	24.859213
146.105888	5064.364665	24.864231
145.729168	5067.092389	24.869248
145.838993	5070.028295	24.874266
145.962688	5072.655537	24.879283
145.869960	5095.176285	24.884301
145.883727	5088.530946	24.889319
146.701081	5106.284586	24.894336
146.670141	5111.633353	24.899354
146.838892	5111.929808	24.904371
146.654101	5112.125138	24.909389
147.027538	5129.743869	24.914407
147.303293	5138.966891	24.919424
147.232543	5149.846253	24.924442
147.745893	5148.190568	24.929459
147.816673	5169.197330	24.934477
148.443046	5179.455252	24.939495
148.427587	5183.008186	24.944512
148.094153	5182.576113	24.949530
148.627762	5172.207380	24.954547
148.261662	5191.327310	24.959565
148.545041	5196.645926	24.964583
148.681018	5209.333880	24.969600
149.001666	5210.108350	24.974618
149.152990	5212.604226	24.979635
149.057095	5233.549777	24.984653
149.420874	5231.407807	24.989671
149.675659	5233.547840	24.994688
149.557237	5245.622841	24.999706
149.840165	5246.531956	25.004723
149.834731	5268.661987	25.009741
149.953726	5257.071271	25.014759
150.372380	5282.003900	25.019776
150.296178	5293.496996	25.024794
150.736178	5283.858860	25.029811
150.488393	5288.071817	25.034829
150.774040	5309.072988	25.039847
150.974413	5322.623749	25.044864
150.709997	5325.595903	25.049882
150.799042	5324.982573	25.054899
151.180652	5343.930396	25.059917
151.697922	5348.776244	25.064935
151.819972	5365.050885	25.069952
151.700267	5380.023688	25.074970
152.020540	5374.366107	25.079987
151.992957	5385.139223	25.085005
152.156050	5388.601889	25.090023
152.635344	5399.388444	25.095040
153.158946	5401.656309	25.100058
153.519705	5401.874397	25.105075
153.445294	5396.636803	25.110093
153.172433	5393.604322	25.115111
153.311909	5392.395865	25.120128
153.713832	5399.687418	25.125146
153.964152	5411.150755	25.130163
153.748126	5422.982211	25.135181
153.828706	5417.040752	25.140199
153.868731	5426.038490	25.145216
154.078942	5427.238501	25.150234
154.588830	5433.407945	25.155251
154.453917	5451.033541	25.160269
154.714830	5443.581458	25.165287
154.759145	5449.903094	25.170304
154.639668	5462.934557	25.175322
155.281754	5466.943770	25.180339
155.179928	5489.544563	25.185357
155.144989	5491.714661	25.190375
155.757454	5503.336835	25.195392
155.489743	5515.432125	25.200410
155.793767	5511.469709	25.205427
155.669135	5534.857999	25.210445
156.239946	5538.878287	25.215463
155.961557	5548.355877	25.220480
156.268905	5569.302597	25.225498
156.809095	5565.248943	25.230515
156.985431	5569.041021	25.235533
157.292917	5568.438638	25.240551
157.105297	5599.024199	25.245568
157.231990	5601.261964	25.250586
157.656479	5600.180187	25.255603
157.404672	5603.781153	25.260621
157.875113	5613.032747	25.265639
157.856831	5627.233635	25.270656
157.828945	5630.820238	25.275674
158.301592	5649.154735	25.280691
158.468349	5660.455721	25.285709
158.669959	5669.917415	25.290727
158.496643	5667.996166	25.295744
158.706812	5685.514274	25.300762
159.080255	5686.601334	25.305779
158.728056	5702.781861	25.310797
159.058087	5704.659789	25.315815
159.204093	5709.174437	25.320832
159.178513	5731.884194	25.325850
159.633007	5738.866309	25.330867
160.008352	5746.630271	25.335885
160.110112	5764.350778	25.340903
160.790194	5769.439062	25.345920
160.556558	5766.208604	25.350938
160.978456	5765.242236	25.355955
161.055661	5782.895961	25.360973
161.263636	5785.904691	25.365991
161.720487	5791.553039	25.371008
161.188322	5793.058376	25.376026
161.653322	5788.908472	25.381043
161.638605	5806.308929	25.386061
161.081012	5818.946442	25.391079
161.658564	5823.612302	25.396096
161.898987	5839.896904	25.401114
162.360815	5846.608490	25.406131
162.300291	5859.187853	25.411149
162.419597	5860.838547	25.416167
162.752613	5868.080336	25.421184
162.922740	5890.527822	25.426202
163.524480	5884.678371	25.431219
163.389355	5882.862588	25.436237
163.420782	5885.140640	25.441255
163.668713	5896.424369	25.446272
163.706849	5913.067152	25.451290
163.833170	5904.408560	25.456307
164.132908	5903.777524	25.461325
163.836540	5913.715915	25.466343
164.106267	5917.462630	25.471360
164.295498	5931.673415	25.476378
164.292164	5951.577503	25.481395
164.357451	5961.169926	25.486413
164.660598	5963.021638	25.491431
165.636001	5980.694878	25.496448
165.338045	5993.355544	25.501466
165.523024	5996.809195	25.506483
165.627939	5995.099219	25.511501
165.953624	6006.768634	25.516519
166.144561	6018.080823	25.521536
166.226939	6017.705644	25.526554
166.355766	6024.048910	25.531571
166.756957	6039.507582	25.536589
166.555340	6055.923356	25.541607
166.830304	6050.148624	25.546624
166.782062	6061.001244	25.551642
166.888615	6067.323812	25.556659
167.218886	6076.508398	25.561677
167.215585	6091.585398	25.566695
168.116869	6101.800610	25.571712
167.921601	6117.514419	25.576730
167.771007	6116.195012	25.581747
167.981246	6117.697516	25.586765
168.163760	6130.624214	25.591783
168.557474	6128.746517	25.596800
168.856764	6149.833181	25.601818
169.073797	6162.071308	25.606835
169.076121	6162.252094	25.611853
169.160138	6173.415188	25.616871
168.987095	6179.983527	25.621888
169.380265	6195.180622	25.626906
169.664557	6208.092046	25.631923
169.880454	6217.272880	25.636941
169.880621	6225.501894	25.641959
170.309326	6231.780448	25.646976
170.115447	6237.741083	25.651994
170.520777	6247.260636	25.657011
170.748415	6247.255911	25.662029
170.965474	6277.297453	25.667047
171.430341	6274.984176	25.672064
171.133914	6282.762367	25.677082
171.573472	6286.620359	25.682100
171.891187	6297.639165	25.687117
171.934712	6314.721755	25.692135
172.246597	6303.992959	25.697152
172.441526	6310.541952	25.702170
172.614543	6311.424501	25.707188
172.855826	6329.617085	25.712205
172.920217	6339.297314	25.717223
173.303663	6339.931452	25.722240
173.293947	6338.922569	25.727258
173.074220	6343.262673	25.732276
173.348646	6349.788233	25.737293
173.321444	6363.166622	25.742311
173.520083	6366.963852	25.747328
173.261924	6386.205906	25.752346
173.737757	6394.366207	25.757364
174.169662	6399.316361	25.762381
174.207250	6422.847559	25.767399
174.808574	6426.929959	25.772416
174.091170	6436.963054	25.777434
174.642969	6435.799424	25.782452
174.883873	6459.986855	25.787469
175.120595	6469.165162	25.792487
175.460326	6470.413833	25.797504
175.518402	6475.646665	25.802522
175.782696	6491.157671	25.807540
175.735690	6490.895347	25.812557
175.767587	6510.624155	25.817575
175.884475	6516.271761	25.822592
176.195535	6525.281010	25.827610
176.569961	6537.683882	25.832628
176.836126	6543.991146	25.837645
176.831303	6556.913091	25.842663
177.200916	6553.670444	25.847680
177.112063	6582.403942	25.852698
177.289407	6581.197769	25.857716
178.007474	6587.782032	25.862733
177.793824	6604.569774	25.867751
178.146541	6599.211972	25.872768
177.707270	6610.582835	25.877786
178.379986	6627.261910	25.882804
178.583763	6633.160554	25.887821
178.360462	6651.825313	25.892839
178.765369	6660.425226	25.897856
178.904963	6670.858745	25.902874
179.090866	6694.282212	25.907892
179.819296	6700.151199	25.912909
179.752227	6703.840647	25.917927
180.255760	6708.292235	25.922944
180.321130	6724.778544	25.927962
180.583574	6732.909893	25.932980
180.447995	6726.027185	25.937997
180.594866	6743.278948	25.943015
180.934834	6741.000539	25.948032
180.745903	6761.109765	25.953050
180.967907	6761.696711	25.958068
181.242047	6761.666933	25.963085
181.146212	6779.312717	25.968103
181.613153	6779.315489	25.973120
181.984615	6790.492690	25.978138
181.805554	6819.221915	25.983156
181.897013	6813.385246	25.988173
182.260789	6843.535807	25.993191
182.445189	6852.674985	25.998208
182.617381	6856.097869	26.003226
182.668764	6884.857446	26.008244
183.066980	6872.705605	26.013261
182.898381	6902.150002	26.018279
183.081209	6908.255444	26.023296
183.550724	6927.307925	26.028314
183.820186	6942.018261	26.033332
184.209640	6942.192228	26.038349
184.277773	6945.891560	26.043367
184.746410	6955.764919	26.048384
184.981119	6973.114184	26.053402
185.089898	6973.852279	26.058420
184.902016	6972.930458	26.063437
184.982981	6992.235043	26.068455
185.448120	7002.632016	26.073472
185.803471	6998.089656	26.078490
185.609492	7007.677748	26.083508
185.846556	7021.779958	26.088525
185.818230	7037.815080	26.093543
186.330398	7038.133278	26.098560
186.457006	7047.542887	26.103578
186.637996	7065.043744	26.108596
187.068624	7068.475717	26.113613
187.147327	7074.641847	26.118631
187.190736	7075.658612	26.123648
186.999954	7080.083111	26.128666
186.869255	7094.472553	26.133684
187.546413	7103.203906	26.138701
187.856755	7126.718394	26.143719
187.727757	7127.058066	26.148736
187.971333	7139.263396	26.153754
188.133090	7157.549700	26.158772
188.596316	7161.619011	26.163789
188.559304	7184.443022	26.168807
188.765572	7187.223096	26.173824
189.117265	7204.482285	26.178842
189.054186	7213.272899	26.183860
189.361712	7228.632515	26.188877
189.493086	7236.242412	26.193895
189.630275	7245.238430	26.198912
189.949691	7260.744182	26.203930
190.267840	7281.039977	26.208948
190.490834	7285.245334	26.213965
190.906530	7306.218889	26.218983
190.809861	7311.419423	26.224000
191.543137	7322.451813	26.229018
191.240653	7331.387032	26.234036
191.400108	7333.094225	26.239053
191.549784	7340.059178	26.244071
191.846685	7364.513583	26.249088
192.086027	7364.345444	26.254106
192.258644	7381.158827	26.259124
192.880175	7383.719489	26.264141
192.870754	7400.422146	26.269159
192.835772	7391.175162	26.274176
193.404320	7409.335875	26.279194
193.476573	7415.401598	26.284212
193.632540	7425.900635	26.289229
193.980813	7428.285372	26.294247
194.084025	7433.007695	26.299264
194.197857	7442.668567	26.304282
194.007298	7459.805464	26.309300
194.357555	7459.184884	26.314317
194.644515	7479.911462	26.319335
194.863734	7481.880490	26.324352
194.962665	7481.300882	26.329370
194.902595	7505.602934	26.334388
195.498833	7509.221736	26.339405
195.522015	7531.968503	26.344423
195.666002	7546.285141	26.349440
195.844204	7550.499587	26.354458
195.951928	7568.143141	26.359476
196.513763	7579.286118	26.364493
196.814531	7575.273325	26.369511
196.869834	7598.421295	26.374528
197.176785	7596.511376	26.379546
197.172314	7611.451382	26.384564
197.418934	7616.516993	26.389581
197.473860	7631.632254	26.394599
197.691890	7639.231884	26.399616
197.992423	7658.202261	26.404634
197.428755	7676.990942	26.409652
197.976287	7677.949975	26.414669
198.315657	7703.714861	26.419687
198.744503	7699.698085	26.424704
199.191241	7724.015507	26.429722
199.116377	7739.186307	26.434740
199.312824	7731.376805	26.439757
199.626824	7750.020525	26.444775
199.519292	7765.937997	26.449792
200.003699	7760.269634	26.454810
200.010284	7772.158006	26.459828
200.379488	7783.952262	26.464845
200.249643	7785.562639	26.469863
200.148184	7807.571173	26.474880
200.922916	7809.067480	26.479898
200.716442	7823.223621	26.484916
201.157588	7839.453299	26.489933
201.400635	7860.138045	26.494951
201.610641	7863.653328	26.499968
201.824525	7882.958964	26.504986
201.678951	7890.873559	26.510004
202.366298	7904.335378	26.515021
202.678313	7919.942256	26.520039
202.862542	7915.038949	26.525056
202.923099	7923.218635	26.530074
203.535939	7944.745541	26.535092
203.576081	7937.973320	26.540109
203.706952	7940.628207	26.545127
203.562516	7960.517298	26.550144
203.701191	7967.598572	26.555162
203.890037	7984.059369	26.560180
204.509278	8002.584136	26.565197
204.530401	8005.192679	26.570215
204.696241	8024.648257	26.575232
205.002337	8034.253910	26.580250
205.308290	8035.473666	26.585268
205.433078	8043.523010	26.590285
205.323638	8055.633313	26.595303
205.529178	8061.460516	26.600320
206.192493	8077.264394	26.605338
205.978117	8089.682035	26.610356
206.403597	8101.311211	26.615373
206.454987	8111.911575	26.620391
206.406934	8119.595034	26.625408
206.851278	8138.331770	26.630426
207.259722	8155.064251	26.635444
207.246756	8173.314587	26.640461
207.687478	8176.830990	26.645479
207.933364	8205.020263	26.650496
207.962070	8215.258177	26.655514
207.984886	8225.818465	26.660532
208.321055	8231.293185	26.665549
208.636305	8249.663158	26.670567
208.452898	8264.225469	26.675584
209.164473	8276.712325	26.680602
209.148519	8289.293293	26.685620
209.253805	8300.767073	26.690637
209.614100	8312.708932	26.695655
209.414837	8329.306255	26.700672
210.348352	8346.807946	26.705690
210.174873	8360.027203	26.710708
210.415092	8378.326294	26.715725
210.650400	8383.673672	26.720743
211.207396	8392.984207	26.725760
211.714944	8396.917291	26.730778
211.568146	8422.287548	26.735796
211.669069	8416.792957	26.740813
211.786561	8430.168734	26.745831
211.933210	8458.957862	26.750848
212.815396	8470.762710	26.755866
212.742107	8464.737762	26.760884
212.940385	8478.396342	26.765901
212.922692	8488.831984	26.770919
213.306620	8495.890861	26.775936
213.375608	8504.048963	26.780954
213.637896	8526.201282	26.785972
213.403967	8529.354073	26.790989
213.666696	8532.356597	26.796007
213.790075	8546.374282	26.801024
214.140510	8555.745230	26.806042
214.345356	8578.256919	26.811060
214.319620	8585.582413	26.816077
214.815428	8608.275029	26.821095
214.913915	8624.319822	26.826112
215.085465	8623.669029	26.831130
215.301259	8653.812165	26.836148
215.671307	8654.504565	26.841165
216.115539	8673.450701	26.846183
216.116633	8679.639013	26.851200
216.427919	8698.941271	26.856218
216.353709	8711.199824	26.861236
216.768294	8727.267034	26.866253
216.876802	8741.196771	26.871271
217.091441	8762.897294	26.876288
217.689145	8764.419179	26.881306
217.565267	8788.514003	26.886324
218.033151	8796.489390	26.891341
218.681636	8804.567115	26.896359
218.509258	8814.512698	26.901376
218.970621	8831.733377	26.906394
219.013649	8827.604764	26.911412
218.944635	8846.646625	26.916429
219.230559	8865.506645	26.921447
219.367956	8872.633437	26.926464
219.878242	8891.257696	26.931482
220.307640	8904.017230	26.936500
220.304662	8924.344059	26.941517
220.614329	8920.298734	26.946535
220.386082	8938.089430	26.951552
220.770211	8957.297183	26.956570
220.935761	8967.341112	26.961588
220.893219	8992.162428	26.966605
221.601225	8999.623004	26.971623
221.629340	9024.465716	26.976640
221.999480	9030.455776	26.981658
222.105447	9044.416922	26.986676
222.314638	9053.987302	26.991693
222.933753	9061.657254	26.996711
222.705823	9085.656377	27.001728
222.975019	9090.991273	27.006746
223.518250	9103.696604	27.011764
223.548005	9118.087202	27.016781
223.620245	9132.480207	27.021799
223.977831	9148.257963	27.026816
224.654994	9158.810978	27.031834
224.528472	9175.751583	27.036852
224.630916	9182.623571	27.041869
224.835676	9189.670776	27.046887
224.372647	9212.950535	27.051904
224.847178	9230.960374	27.056922
224.910767	9246.988745	27.061940
225.948399	9272.272262	27.066957
226.321436	9278.988256	27.071975
226.149701	9316.628834	27.076992
226.860134	9308.017872	27.082010
226.843180	9320.201993	27.087028
226.874225	9343.792946	27.092045
227.232088	9348.007954	27.097063
227.193508	9372.242311	27.102080
227.616451	9374.097375	27.107098
227.998696	9391.725692	27.112116
228.018946	9392.792146	27.117133
228.523141	9410.809864	27.122151
228.510691	9425.091946	27.127168
228.829311	9424.075580	27.132186
228.975461	9444.086025	27.137204
228.921296	9462.614884	27.142221
229.474121	9470.373251	27.147239
229.625794	9482.972208	27.152256
229.907874	9495.575504	27.157274
230.268258	9499.805102	27.162292
230.142924	9518.445898	27.167309
230.648055	9525.812025	27.172327
230.632239	9526.391330	27.177344
230.501469	9549.443845	27.182362
230.956043	9574.773514	27.187380
230.967881	9597.510136	27.192397
231.332398	9606.636727	27.197415
231.443795	9626.401083	27.202432
231.940617	9643.177164	27.207450
232.223954	9652.606387	27.212468
232.520309	9677.370878	27.217485
233.048618	9681.181882	27.222503
232.929152	9701.764599	27.227520
233.318120	9714.006832	27.232538
233.661295	9730.936155	27.237556
233.488639	9746.697039	27.242573
234.164757	9759.532071	27.247591
234.295081	9779.306864	27.252608
234.266528	9786.116582	27.257626
234.668748	9807.286318	27.262644
235.070775	9820.146457	27.267661
235.439909	9839.500353	27.272679
235.539974	9860.505294	27.277696
235.797276	9859.673193	27.282714
236.164168	9873.823321	27.287732
236.286264	9885.987918	27.292749
236.456466	9899.844601	27.297767
236.579068	9921.441453	27.302784
237.100993	9930.802050	27.307802
237.283673	9942.644656	27.312820
237.415365	9943.140382	27.317837
237.774210	9964.070163	27.322855
237.718493	9979.209965	27.327872
238.216275	9995.196878	27.332890
238.294419	9998.425726	27.337908
238.521716	10020.752943	27.342925
239.174648	10032.097583	27.347943
238.909058	10049.063789	27.352960
239.346793	10054.048794	27.357978
239.996498	10062.319973	27.362996
239.906036	10074.646867	27.368013
239.840017	10092.327589	27.373031
240.193530	10107.319161	27.378048
240.418275	10122.044592	27.383066
240.740246	10135.110511	27.388084
240.705492	10153.544766	27.393101
241.169294	10155.375805	27.398119
241.590491	10187.021566	27.403136
241.437204	10193.184116	27.408154
241.865817	10215.507304	27.413172
241.854065	10232.237725	27.418189
242.049873	10248.101745	27.423207
242.211924	10267.304639	27.428224
242.403292	10287.027372	27.433242
242.972049	10308.007810	27.438260
242.882043	10334.302851	27.443277
243.291671	10347.788467	27.448295
243.490045	10371.241256	27.453312
243.769826	10384.177307	27.458330
244.051257	10406.407829	27.463348
244.343526	10418.272756	27.468365
245.020241	10433.459887	27.473383
245.188099	10451.199834	27.478400
245.435048	10462.572055	27.483418
245.632913	10469.907739	27.488436
246.120910	10476.853305	27.493453
246.503716	10486.687980	27.498471
246.484240	10494.084997	27.503488
246.273293	10507.922021	27.508506
246.819998	10525.363545	27.513524
247.151647	10541.633864	27.518541
247.245157	10549.953590	27.523559
248.034742	10565.300930	27.528576
248.048677	10583.589717	27.533594
248.419920	10584.177232	27.538612
248.204251	10590.184852	27.543629
248.517813	10605.816946	27.548647
248.745660	10619.046223	27.553664
248.722103	10644.739066	27.558682
249.113427	10655.381537	27.563700
249.178797	10670.958814	27.568717
249.423705	10688.939905	27.573735
249.684331	10710.196598	27.578752
249.665583	10727.009054	27.583770
250.416629	10745.626200	27.588788
250.406294	10769.771304	27.593805
250.869660	10778.678879	27.598823
251.681067	10803.701457	27.603840
251.631505	10813.334000	27.608858
252.023544	10813.023079	27.613876
251.983548	10838.442430	27.618893
252.386104	10847.059190	27.623911
252.568992	10863.075653	27.628928
252.733230	10888.864527	27.633946
253.319862	10885.048447	27.638964
253.480846	10904.292458	27.643981
253.748691	10924.821840	27.648999
253.735419	10933.974141	27.654016
254.214476	10951.953652	27.659034
254.564311	10967.148329	27.664052
254.019182	10975.407357	27.669069
254.859416	10986.419024	27.674087
255.203860	11005.960422	27.679104
255.318878	11022.178980	27.684122
255.585977	11039.700609	27.689140
256.048409	11070.766125	27.694157
256.117483	11073.405016	27.699175
256.223418	11091.594793	27.704192
256.463091	11107.641458	27.709210
256.923788	11118.070230	27.714228
257.288232	11138.234026	27.719245
257.624689	11149.483925	27.724263
257.759178	11163.297995	27.729280
257.713389	11186.336366	27.734298
258.403739	11188.599455	27.739316
258.173941	11213.764149	27.744333
258.752192	11230.326671	27.749351
258.954997	11246.458386	27.754368
259.176007	11271.026703	27.759386
259.488735	11273.929262	27.764404
259.752228	11303.299702	27.769421
259.947180	11314.439290	27.774439
260.144655	11323.030501	27.779456
260.081603	11345.129676	27.784474
260.688997	11368.228388	27.789492
260.648064	11384.547280	27.794509
261.163596	11414.230588	27.799527
261.731693	11420.056298	27.804544
261.846831	11450.764250	27.809562
262.338363	11436.173125	27.814580
262.696220	11451.672621	27.819597
262.643665	11469.978973	27.824615
263.186552	11476.714949	27.829632
263.128691	11486.166484	27.834650
263.414964	11494.738307	27.839668
263.792918	11509.117312	27.844685
264.014681	11529.048454	27.849703
263.883817	11531.169124	27.854720
264.220098	11551.314479	27.859738
264.478942	11566.064718	27.864756
264.801901	11589.184216	27.869773
264.747011	11597.002834	27.874791
265.321475	11612.326255	27.879808
265.546885	11631.516308	27.884826
265.819106	11661.067161	27.889844
266.198034	11684.817259	27.894861
265.973976	11694.255558	27.899879
266.791544	11711.971676	27.904896
266.913441	11734.995574	27.909914
267.161430	11760.144765	27.914932
267.415457	11778.695200	27.919949
267.741611	11793.475434	27.924967
268.310579	11816.503960	27.929984
268.337157	11836.998949	27.935002
268.650969	11850.081012	27.940020
268.871950	11860.370455	27.945037
269.002203	11886.037352	27.950055
269.350314	11900.068686	27.955072
269.730389	11920.500323	27.960090
270.082392	11937.562871	27.965108
270.137968	11956.838256	27.970125
270.628425	11963.994431	27.975143
271.067612	11983.486606	27.980160
271.208332	11998.397111	27.985178
271.517790	12015.852881	27.990196
271.790065	12032.906715	27.995213
272.027784	12047.805878	28.000231
271.996012	12067.773503	28.005248
272.411311	12087.761424	28.010266
272.447106	12085.048257	28.015284
272.671864	12117.994245	28.020301
273.057104	12135.393432	28.025319
273.700912	12157.905750	28.030336
273.989105	12185.273976	28.035354
274.453432	12187.729197	28.040372
274.482093	12206.345929	28.045389
274.806980	12220.516922	28.050407
275.052576	12240.066783	28.055424
275.415828	12257.955108	28.060442
275.563060	12272.250211	28.065460
275.969275	12284.658579	28.070477
275.972677	12309.668039	28.075495
276.653989	12319.047680	28.080512
276.440521	12351.312125	28.085530
276.658883	12358.891883	28.090548
277.222176	12372.077898	28.095565
277.229041	12390.884412	28.100583
277.693715	12410.680156	28.105600
277.594377	12445.352622	28.110618
278.035986	12455.783859	28.115636
278.101778	12491.464319	28.120653
278.393065	12513.202076	28.125671
278.790449	12530.074911	28.130688
278.900023	12558.395315	28.135706
279.452828	12577.283111	28.140724
279.652307	12604.553322	28.145741
279.733447	12626.543612	28.150759
280.468287	12645.064010	28.155776
280.577032	12664.123386	28.160794
281.096579	12665.825700	28.165812
281.500771	12688.334443	28.170829
281.471069	12702.612044	28.175847
281.623279	12709.374049	28.180864
281.755732	12738.738921	28.185882
282.232010	12754.998475	28.190900
282.744893	12773.183989	28.195917
282.961322	12792.630626	28.200935
283.341930	12812.305303	28.205952
283.455083	12828.195044	28.210970
283.565113	12841.483537	28.215988
284.044355	12867.289414	28.221005
283.986796	12892.852003	28.226023
284.351172	12904.286020	28.231040
284.531409	12923.420496	28.236058
284.908381	12950.841451	28.241076
285.377872	12975.167779	28.246093
285.550148	12992.976756	28.251111
286.013178	13008.923587	28.256128
286.314975	13042.813647	28.261146
286.980145	13059.183956	28.266164
287.041956	13070.298020	28.271181
287.257249	13091.475547	28.276199
287.578064	13108.349098	28.281216
287.651237	13130.941815	28.286234
288.028969	13150.845887	28.291252
288.764714	13174.746910	28.296269
288.712016	13187.203846	28.301287
288.731776	13208.153984	28.306304
288.720694	13222.274507	28.311322
289.307302	13250.890357	28.316340
289.937367	13266.269149	28.321357
289.794891	13294.880130	28.326375
290.346265	13310.892953	28.331392
290.669272	13333.063069	28.336410
290.858009	13353.039762	28.341428
291.573932	13370.966856	28.346445
291.583394	13403.057662	28.351463
292.090639	13407.832028	28.356480
292.066329	13439.763043	28.361498
292.398768	13449.242280	28.366516
292.947294	13475.961116	28.371533
292.988353	13493.015499	28.376551
293.219937	13513.752755	28.381568
293.515483	13536.413103	28.386586
293.787231	13559.742488	28.391604
294.466880	13579.726154	28.396621
293.985076	13602.468459	28.401639
294.637426	13618.543609	28.406656
295.216105	13646.772212	28.411674
295.931007	13673.291951	28.416692
296.149244	13682.057474	28.421709
296.013841	13700.580245	28.426727
296.728507	13711.840016	28.431744
297.083667	13730.268714	28.436762
297.283156	13734.284258	28.441780
297.381993	13757.533911	28.446797
297.744565	13789.922983	28.451815
297.959443	13795.491473	28.456832
298.386568	13817.113847	28.461850
298.445696	13829.112997	28.466868
298.854063	13846.319484	28.471885
298.768483	13877.665812	28.476903
299.207022	13890.605876	28.481920
299.413893	13917.237206	28.486938
299.585640	13941.291368	28.491956
300.104311	13959.081676	28.496973
300.231772	13979.775360	28.501991
300.583317	14000.504338	28.507008
300.589538	14028.899627	28.512026
300.965924	14041.006977	28.517044
301.371623	14061.946101	28.522061
301.587032	14091.906387	28.527079
302.251813	14108.643455	28.532096
302.560923	14130.545892	28.537114
302.602008	14162.232628	28.542132
303.093506	14166.686755	28.547149
303.359561	14199.303859	28.552167
303.488953	14211.975606	28.557184
303.614165	14245.008627	28.562202
304.173988	14260.726269	28.567220
304.397714	14281.918125	28.572237
304.594928	14303.741670	28.577255
304.682464	14334.875719	28.582272
305.070497	14361.553325	28.587290
305.356995	14392.536226	28.592308
306.052756	14412.097440	28.597325
306.220395	14444.619483	28.602343
306.702347	14459.089424	28.607360
307.206470	14495.130124	28.612378
307.154388	14515.573778	28.617396
307.390620	14531.214627	28.622413
307.833482	14560.597400	28.627431
308.167771	14586.773663	28.632448
308.587435	14602.525952	28.637466
308.745945	14632.304401	28.642484
309.318570	14647.465518	28.647501
309.443047	14683.851819	28.652519
310.017711	14696.883386	28.657536
310.602791	14726.660487	28.662554
310.945091	14738.794508	28.667572
311.499185	14758.768961	28.672589
311.221065	14771.909163	28.677607
311.521720	14786.560815	28.682624
311.852254	14802.176801	28.687642
312.301258	14819.722724	28.692660
312.783805	14835.551475	28.697677
312.957607	14853.007610	28.702695
313.269727	14877.077653	28.707712
313.683919	14896.038456	28.712730
313.765551	14925.604830	28.717748
314.217596	14928.029423	28.722765
314.405664	14956.077738	28.727783
314.697737	14982.786484	28.732800
315.325665	15002.192609	28.737818
315.431780	15024.000727	28.742836
315.420339	15047.910424	28.747853
315.524400	15070.918354	28.752871
315.834617	15085.762546	28.757888
316.835131	15110.780861	28.762906
316.887318	15149.889524	28.767924
317.453586	15166.436000	28.772941
317.403309	15193.706317	28.777959
317.741562	15207.210997	28.782976
318.511228	15229.668839	28.787994
318.110801	15245.394072	28.793012
318.576056	15267.041977	28.798029
319.044886	15299.219369	28.803047
319.447094	15314.995734	28.808064
319.874064	15332.159718	28.813082
320.019330	15357.470223	28.818100
320.566193	15366.126893	28.823117
320.773791	15393.933140	28.828135
321.160989	15411.094357	28.833152
321.187232	15433.073899	28.838170
321.437884	15451.770929	28.843188
321.870072	15461.354554	28.848205
321.850400	15491.677982	28.853223
322.741315	15508.706760	28.858240
322.924344	15527.824907	28.863258
323.294407	15556.608442	28.868276
323.724390	15562.843187	28.873293
323.779563	15585.632993	28.878311
324.184697	15614.853701	28.883328
324.418160	15636.959857	28.888346
324.556257	15662.297241	28.893364
325.006274	15683.465925	28.898381
325.226878	15711.664587	28.903399
325.702748	15736.712701	28.908416
326.112765	15749.613270	28.913434
326.557062	15783.598817	28.918452
326.715646	15800.858314	28.923469
327.319492	15830.676862	28.928487
327.313303	15843.441744	28.933504
327.639721	15862.793376	28.938522
327.954905	15899.484835	28.943540
328.231826	15920.170322	28.948557
328.365672	15952.592207	28.953575
329.036112	15976.549170	28.958592
329.277874	15995.659680	28.963610
329.772637	16022.714729	28.968628
329.724577	16049.172778	28.973645
330.201286	16078.711844	28.978663
330.395957	16108.266291	28.983680
331.272386	16124.673945	28.988698
331.391831	16154.683885	28.993716
331.749650	16172.073022	28.998733
332.059267	16206.690230	29.003751
332.478419	16219.485621	29.008768
333.045782	16243.067621	29.013786
333.088462	16267.890603	29.018804
333.859327	16284.178824	29.023821
334.076690	16308.060220	29.028839
333.946862	16329.573528	29.033856
334.622783	16353.553773	29.038874
334.616451	16391.409397	29.043892
334.870742	16406.218363	29.048909
335.312221	16429.525212	29.053927
335.824799	16457.361400	29.058944
335.924791	16477.626177	29.063962
336.303395	16512.010317	29.068980
336.631705	16534.902649	29.073997
337.068822	16566.737864	29.079015
337.205231	16595.927718	29.084032
337.471316	16607.543013	29.089050
337.912664	16650.832259	29.094068
338.438119	16673.520223	29.099085
338.724981	16704.685538	29.104103
338.948999	16729.017246	29.109120
339.450250	16755.856474	29.114138
339.641293	16788.056126	29.119156
340.276498	16806.473288	29.124173
340.316136	16829.212221	29.129191
340.904995	16857.580225	29.134208
341.494804	16875.262583	29.139226
341.691604	16899.381538	29.144244
342.210652	16924.143709	29.149261
342.392699	16941.595960	29.154279
342.693760	16960.188599	29.159296
343.223749	16976.032029	29.164314
343.489766	17007.538701	29.169332
343.714076	17012.942788	29.174349
344.431571	17019.280076	29.179367
344.793438	17039.509920	29.184384
345.376890	17055.683447	29.189402
345.578301	17076.652473	29.194420
345.718462	17087.092622	29.199437
346.173404	17086.857864	29.204455
346.844915	17089.850050	29.209472
347.013399	17088.951971	29.214490
347.171501	17124.515249	29.219508
347.375671	17129.186592	29.224525
347.915237	17150.635478	29.229543
348.002220	17166.704008	29.234560
348.439489	17190.384638	29.239578
348.417510	17214.954964	29.244596
348.821812	17242.980706	29.249613
348.755660	17256.023035	29.254631
349.242433	17290.811700	29.259648
349.762206	17307.814157	29.264666
349.954896	17349.340087	29.269684
350.823412	17359.400899	29.274701
350.694657	17377.037649	29.279719
351.383451	17405.698954	29.284736
351.948569	17423.854170	29.289754
351.995275	17455.185323	29.294772
352.347222	17477.715633	29.299789
352.671551	17489.785315	29.304807
352.873778	17529.305022	29.309824
353.263144	17541.706002	29.314842
353.047849	17580.109784	29.319860
353.550461	17594.429310	29.324877
353.930924	17631.804206	29.329895
354.430704	17669.075820	29.334912
355.175554	17695.434732	29.339930
355.314834	17733.535633	29.344948
355.543791	17765.412464	29.349965
355.813142	17792.219385	29.354983
356.130444	17823.400665	29.360000
356.454890	17843.916725	29.365018
356.701004	17889.349237	29.370036
357.176277	17922.782310	29.375053
357.645398	17955.970559	29.380071
357.746542	17993.490404	29.385088
358.889399	18020.439491	29.390106
359.267957	18056.734264	29.395124
359.486737	18073.738642	29.400141
359.709816	18093.959725	29.405159
359.947190	18129.519869	29.410176
360.503908	18154.867195	29.415194
360.974789	18178.226799	29.420212
361.413951	18206.908889	29.425229
361.564724	18229.519354	29.430247
361.816361	18268.670038	29.435264
362.113519	18291.637760	29.440282
362.369562	18320.925852	29.445300
362.704169	18352.538762	29.450317
362.958901	18380.305941	29.455335
363.299336	18423.663872	29.460352
363.970499	18447.865496	29.465370
364.297625	18482.845551	29.470388
364.631785	18511.953902	29.475405
365.089182	18544.120597	29.480423
365.290898	18571.523288	29.485440
365.951655	18605.762432	29.490458
366.348106	18627.891226	29.495476
366.697236	18658.725121	29.500493
366.813346	18674.854903	29.505511
367.376124	18701.583019	29.510528
367.887241	18730.994988	29.515546
368.276996	18751.792962	29.520564
368.697448	18767.229088	29.525581
369.444705	18786.055487	29.530599
369.140532	18813.165839	29.535616
369.591679	18830.263236	29.540634
370.002890	18849.657876	29.545652
370.440658	18883.201581	29.550669
370.833525	18903.122716	29.555687
370.684145	18937.634270	29.560704
371.183352	18957.515734	29.565722
371.581955	18986.611057	29.570740
372.012702	19026.652850	29.575757
372.181044	19042.277722	29.580775
372.149712	19078.147796	29.585792
373.069265	19106.434764	29.590810
373.718103	19138.047413	29.595828
373.980725	19164.892345	29.600845
374.561788	19173.204828	29.605863
374.468590	19210.466464	29.610880
375.207720	19234.311117	29.615898
375.580267	19271.959014	29.620916
375.954682	19289.873643	29.625933
376.474776	19322.948949	29.630951
376.614773	19353.298622	29.635968
377.154447	19381.113149	29.640986
377.468772	19407.940424	29.646004
377.846223	19439.124195	29.651021
378.196753	19459.901192	29.656039
378.058033	19506.163488	29.661056
378.916981	19525.847141	29.666074
379.394879	19554.449443	29.671092
379.509622	19602.331558	29.676109
379.998819	19618.282038	29.681127
380.406885	19647.110506	29.686144
380.809087	19686.099191	29.691162
381.083568	19718.599653	29.696180
381.379624	19755.894012	29.701197
382.021337	19774.909330	29.706215
381.900152	19809.432183	29.711232
382.524511	19830.660768	29.716250
383.150761	19875.665051	29.721268
383.184956	19905.714835	29.726285
383.602932	19942.188466	29.731303
384.148945	19972.876993	29.736320
384.307603	20006.863457	29.741338
384.968477	20044.714295	29.746356
384.884773	20078.271344	29.751373
385.541562	20106.206362	29.756391
386.222854	20138.490288	29.761408
387.068254	20170.951973	29.766426
387.394295	20185.001938	29.771444
387.479721	20219.097167	29.776461
388.322545	20243.987082	29.781479
388.432309	20275.022955	29.786496
389.292770	20292.816932	29.791514
389.551197	20305.482945	29.796532
389.697245	20335.136535	29.801549
390.104079	20359.488901	29.806567
390.082806	20390.005979	29.811584
390.399864	20414.166801	29.816602
391.393128	20441.627113	29.821620
391.236679	20465.929727	29.826637
391.706046	20493.158671	29.831655
392.306670	20527.917839	29.836672
392.501091	20557.816045	29.841690
393.100222	20585.908067	29.846708
393.235808	20624.400863	29.851725
393.819345	20635.770743	29.856743
393.885296	20672.263442	29.861760
394.233716	20692.463696	29.866778
394.804466	20726.722140	29.871796
394.754100	20749.318968	29.876813
395.200908	20782.191753	29.881831
395.267941	20814.493876	29.886848
396.095142	20858.013753	29.891866
396.351227	20888.441516	29.896884
396.632724	20920.244683	29.901901
397.211248	20950.234297	29.906919
397.492720	20990.212554	29.911936
397.789496	21033.641253	29.916954
398.540109	21060.031338	29.921972
398.622748	21093.416148	29.926989
399.516682	21120.712757	29.932007
399.735251	21162.371565	29.937024
400.105179	21194.029696	29.942042
400.737051	21230.621956	29.947060
401.139752	21266.862920	29.952077
401.677549	21291.907545	29.957095
401.910083	21324.057019	29.962112
402.315733	21353.919975	29.967130
403.121974	21381.080211	29.972148
403.381269	21411.446895	29.977165
403.734757	21422.724657	29.982183
403.944097	21463.061314	29.987200
404.480941	21490.362654	29.992218
404.773782	21516.167278	29.997236
405.071183	21555.321188	30.002253
405.850816	21581.182228	30.007271
405.942916	21620.498104	30.012288
406.471167	21650.140977	30.017306
407.121790	21678.940528	30.022324
407.096885	21714.640137	30.027341
407.649863	21750.054625	30.032359
407.625945	21785.695880	30.037376
408.273824	21822.009261	30.042394
408.955750	21845.665317	30.047412
409.005605	21882.789270	30.052429
409.788282	21924.964881	30.057447
409.931838	21960.659101	30.062464
410.240673	21995.267942	30.067482
410.967197	22025.223850	30.072500
411.189490	22061.903291	30.077517
412.023934	22088.992185	30.082535
412.225695	22126.633847	30.087552
412.505205	22153.356181	30.092570
413.031706	22178.984252	30.097588
413.171718	22226.752942	30.102605
413.796833	22250.373277	30.107623
414.045205	22299.073392	30.112640
414.517024	22332.741319	30.117658
415.167142	22374.481227	30.122676
415.243683	22416.641328	30.127693
415.934297	22445.684677	30.132711
415.702129	22475.403271	30.137728
416.470227	22528.073237	30.142746
416.841929	22561.731443	30.147764
417.521471	22597.670683	30.152781
417.483724	22628.420018	30.157799
418.021495	22668.424321	30.162816
418.697132	22702.311420	30.167834
419.423958	22739.525059	30.172852
419.437713	22779.026930	30.177869
420.057526	22797.158409	30.182887
421.086403	22826.776959	30.187904
421.630917	22861.211239	30.192922
422.362592	22875.304877	30.197940
422.290465	22907.730295	30.202957
422.561641	22915.839097	30.207975
423.070929	22938.882012	30.212992
423.211119	22970.283605	30.218010
423.692412	22984.056249	30.223028
424.227487	23022.116010	30.228045
424.535569	23041.636695	30.233063
425.001424	23070.508730	30.238080
425.106358	23108.269569	30.243098
425.692188	23124.954761	30.248116
425.544151	23170.927453	30.253133
426.067918	23192.307873	30.258151
426.359932	23237.775593	30.263168
426.397979	23272.859349	30.268186
426.662326	23329.456732	30.273204
426.932735	23368.731271	30.278221
427.188067	23420.163020	30.283239
428.224289	23462.335039	30.288256
428.297935	23525.008956	30.293274
429.085500	23570.934554	30.298292
429.283895	23624.401113	30.303309
429.800375	23671.201457	30.308327
430.051770	23720.149560	30.313344
430.783006	23760.813412	30.318362
431.401636	23801.065565	30.323380
431.936933	23840.585771	30.328397
432.821873	23880.040109	30.333415
433.415206	23914.279183	30.338432
433.659870	23950.938483	30.343450
434.218039	23985.811161	30.348468
434.524507	24024.240714	30.353485
434.963575	24066.142835	30.358503
435.281995	24100.984606	30.363520
435.481423	24149.868456	30.368538
435.897587	24189.942268	30.373556
436.362924	24226.034072	30.378573
436.982310	24271.716679	30.383591
437.947588	24300.058414	30.388608
438.610248	24336.505611	30.393626
439.144808	24352.927711	30.398644
439.466959	24391.223019	30.403661
439.771676	24416.047625	30.408679
440.755963	24450.716435	30.413696
440.745591	24482.585796	30.418714
441.267989	24506.276798	30.423732
441.575949	24543.105055	30.428749
441.838699	24575.519018	30.433767
442.428912	24608.632457	30.438784
442.330392	24640.989851	30.443802
442.914598	24681.134679	30.448820
443.297166	24730.497563	30.453837
443.842926	24764.757285	30.458855
444.286804	24802.922906	30.463872
444.668859	24845.091882	30.468890
445.239634	24877.676039	30.473908
445.532249	24925.641418	30.478925
446.046661	24962.732767	30.483943
446.255927	24996.096317	30.488960
446.456971	25044.629198	30.493978
447.170075	25074.427128	30.498996
447.343389	25129.396008	30.504013
447.888516	25166.391228	30.509031
448.294117	25214.382805	30.514048
448.767519	25260.650575	30.519066
449.257487	25309.265534	30.524084
449.801920	25349.875882	30.529101
450.094072	25391.376688	30.534119
451.051494	25424.402328	30.539136
451.134647	25458.175681	30.544154
451.697706	25492.276277	30.549172
452.335414	25532.470988	30.554189
452.722512	25563.677050	30.559207
453.284544	25589.927304	30.564224
453.588535	25624.509621	30.569242
454.185984	25657.418865	30.574260
454.809567	25693.020661	30.579277
454.950733	25730.970518	30.584295
455.515414	25761.516606	30.589312
455.700320	25793.034236	30.594330
455.895715	25837.381510	30.599348
456.421482	25886.522064	30.604365
456.775351	25921.815857	30.609383
457.487111	25962.658510	30.614400
458.043347	26010.800775	30.619418
458.114706	26050.642860	30.624436
458.762775	26097.678745	30.629453
459.043536	26146.570542	30.634471
459.593554	26175.899100	30.639488
460.210360	26229.939873	30.644506
460.507682	26256.616780	30.649524
461.053544	26310.600195	30.654541
461.800756	26350.895342	30.659559
462.496773	26383.231293	30.664576
463.072802	26429.179194	30.669594
463.382358	26466.370900	30.674612
464.014685	26504.417527	30.679629
464.330028	26543.217148	30.684647
464.828537	26574.179426	30.689664
465.134046	26613.996539	30.694682
465.580768	26665.022974	30.699700
465.806536	26703.904074	30.704717
466.268152	26748.004439	30.709735
466.666664	26782.396736	30.714752
467.240625	26836.288806	30.719770
467.388595	26878.630974	30.724788
468.448910	26928.423847	30.729805
468.660028	26977.222313	30.734823
469.075385	27020.091368	30.739840
469.461296	27066.725507	30.744858
470.107324	27116.925256	30.749876
470.581906	27159.753276	30.754893
470.652726	27204.891283	30.759911
471.868884	27240.735388	30.764928
472.275654	27287.054364	30.769946
473.454531	27321.472696	30.774964
474.304460	27342.993405	30.779981
474.490360	27385.008754	30.784999
474.996491	27407.823204	30.790016
475.120556	27432.615922	30.795034
475.510938	27467.392626	30.800052
476.187278	27497.715050	30.805069
476.396605	27535.998238	30.810087
477.014621	27573.784618	30.815104
477.087065	27617.585910	30.820122
477.525806	27654.903825	30.825140
477.691204	27690.645779	30.830157
477.706287	27752.415797	30.835175
478.667720	27792.224473	30.840192
479.225811	27840.226417	30.845210
479.547227	27891.258349	30.850228
479.975702	27928.023349	30.855245
480.864488	27986.636457	30.860263
481.358793	28010.642952	30.865280
481.650799	28060.118733	30.870298
482.310378	28094.492360	30.875316
482.821849	28129.682464	30.880333
483.125006	28168.970409	30.885351
483.616661	28203.227027	30.890368
483.995835	28250.868645	30.895386
484.301010	28278.963804	30.900404
484.600357	28328.338180	30.905421
485.382875	28368.935016	30.910439
486.509463	28403.566090	30.915456
487.060975	28436.362074	30.920474
487.474607	28463.887450	30.925492
487.923514	28500.050876	30.930509
488.506374	28534.356094	30.935527
488.665209	28563.782064	30.940544
488.970415	28610.358041	30.945562
489.532305	28647.392639	30.950580
489.810388	28680.802346	30.955597
490.149323	28727.508688	30.960615
490.718868	28762.529538	30.965632
491.260496	28826.922687	30.970650
491.979095	28869.452555	30.975668
492.390602	28912.345850	30.980685
492.600629	28958.222430	30.985703
493.486135	29000.847935	30.990720
493.686078	29047.480418	30.995738
493.850389	29091.601411	31.000756
495.109790	29118.536221	31.005773
495.316451	29175.263318	31.010791
496.208065	29205.146003	31.015808
496.599699	29254.545532	31.020826
497.130782	29301.111079	31.025844
497.576175	29332.427826	31.030861
498.092157	29379.374670	31.035879
499.124145	29412.865638	31.040896
499.420771	29453.958988	31.045914
499.576276	29495.470231	31.050932
500.077006	29533.135224	31.055949
500.855781	29573.773352	31.060967
501.660041	29611.397569	31.065984
501.972609	29656.915069	31.071002
502.132336	29695.227012	31.076020
502.767120	29734.737884	31.081037
502.788807	29780.767787	31.086055
503.523801	29816.413191	31.091072
504.531361	29856.802601	31.096090
504.755906	29895.713120	31.101108
505.412423	29929.605017	31.106125
506.074182	29981.577196	31.111143
506.184345	30018.535131	31.116160
506.493804	30062.233783	31.121178
506.781541	30121.764721	31.126196
507.699074	30165.148104	31.131213
507.705870	30212.194365	31.136231
508.424934	30259.561009	31.141248
508.966525	30305.591130	31.146266
509.053516	30354.517467	31.151284
509.809583	30404.090032	31.156301
509.877485	30456.080209	31.161319
510.118604	30505.647084	31.166336
510.859971	30570.477269	31.171354
511.443508	30626.553318	31.176372
512.204507	30685.111524	31.181389
512.381407	30744.031958	31.186407
512.879252	30802.732067	31.191424
513.268253	30853.953883	31.196442
513.923451	30919.749356	31.201460
514.613707	30977.925895	31.206477
515.031978	31028.064297	31.211495
515.513793	31073.711963	31.216512
516.058534	31134.323726	31.221530
516.254009	31185.061195	31.226548
516.939815	31234.032509	31.231565
517.483312	31295.260293	31.236583
518.067119	31339.790545	31.241600
518.612429	31396.522212	31.246618
518.704699	31451.029137	31.251636
519.356028	31511.548770	31.256653
520.072896	31565.516898	31.261671
520.534016	31620.676177	31.266688
521.127871	31678.416679	31.271706
521.487902	31729.664779	31.276724
522.014615	31788.092020	31.281741
522.487695	31847.168885	31.286759
523.149046	31902.106472	31.291776
524.242132	31951.188838	31.296794
525.497952	31991.734407	31.301812
526.324237	32019.966738	31.306829
526.961605	32065.610068	31.311847
527.260079	32103.030176	31.316864
527.755797	32147.147968	31.321882
527.965145	32181.998812	31.326900
528.576729	32219.944599	31.331917
528.545067	32268.914875	31.336935
529.323661	32318.662632	31.341952
530.017718	32351.069933	31.346970
529.987821	32412.052872	31.351988
530.525203	32465.693841	31.357005
530.850086	32522.178582	31.362023
531.264488	32581.122492	31.367040
531.829320	32633.251115	31.372058
531.917256	32714.615432	31.377076
532.584378	32765.181284	31.382093
533.299619	32838.950935	31.387111
533.206999	32896.146760	31.392128
533.974798	32962.767339	31.397146
534.301958	33037.208115	31.402164
535.183772	33091.213457	31.407181
536.229581	33146.438163	31.412199
537.328733	33209.937470	31.417216
537.901756	33264.057729	31.422234
538.131854	33309.320651	31.427252
538.905930	33368.541931	31.432269
539.489871	33421.935076	31.437287
539.830091	33473.093678	31.442304
540.489713	33513.681792	31.447322
541.405571	33568.844191	31.452340
542.330351	33610.814826	31.457357
542.775627	33662.303643	31.462375
543.006014	33699.637440	31.467392
543.778437	33746.553317	31.472410
543.799181	33811.114278	31.477428
544.147719	33855.434314	31.482445
544.641263	33918.096335	31.487463
545.160898	33971.085257	31.492480
545.717984	34026.725202	31.497498
546.024533	34083.899569	31.502516
546.693652	34136.482319	31.507533
547.056231	34201.846275	31.512551
547.578024	34258.284887	31.517568
547.884513	34316.832747	31.522586
548.260356	34383.978156	31.527604
548.732471	34444.165163	31.532621
549.176492	34525.364993	31.537639
549.651911	34591.566847	31.542656
550.560160	34648.441126	31.547674
551.500510	34723.743309	31.552692
552.313774	34758.659849	31.557709
552.942641	34821.816961	31.562727
553.606751	34869.741548	31.567744
554.095311	34925.632356	31.572762
554.424122	34966.348137	31.577780
555.684015	35006.675860	31.582797
557.188522	35027.983706	31.587815
557.839671	35047.350416	31.592832
558.442641	35083.198779	31.597850
558.631707	35120.905328	31.602868
559.445512	35140.365052	31.607885
559.483925	35184.392732	31.612903
559.879150	35221.897996	31.617920
560.982101	35245.242064	31.622938
561.684128	35263.710598	31.627956
562.256223	35290.952053	31.632973
562.959328	35329.829730	31.637991
563.255468	35344.708048	31.643008
564.072203	35373.976129	31.648026
563.964104	35408.942796	31.653044
564.451512	35447.468368	31.658061
565.046412	35481.529454	31.663079
565.157340	35532.252316	31.668096
565.767443	35574.579640	31.673114
566.015514	35637.547227	31.678132
566.630546	35691.093470	31.683149
566.908586	35755.921676	31.688167
566.942089	35807.712270	31.693184
567.669545	35869.606923	31.698202
567.741452	35939.377610	31.703220
568.364406	35999.614217	31.708237
569.065952	36066.604526	31.713255
569.105315	36140.335913	31.718272
570.274612	36209.202677	31.723290
570.507192	36279.367752	31.728308
570.981361	36349.641319	31.733325
571.357111	36421.809383	31.738343
571.994092	36509.998994	31.743360
572.625610	36582.677550	31.748378
572.933368	36670.521784	31.753396
573.775218	36737.983644	31.758413
574.196835	36814.283382	31.763431
574.757246	36890.118527	31.768448
575.392775	36972.386474	31.773466
575.937386	37055.241166	31.778484
577.043627	37126.309155	31.783501
577.513948	37198.294174	31.788519
578.080479	37280.685446	31.793536
579.003729	37347.659468	31.798554
579.563300	37416.332236	31.803572
580.339774	37487.248086	31.808589
581.180903	37554.429042	31.813607
581.724897	37614.775673	31.818624
582.519038	37680.020609	31.823642
583.435498	37740.075395	31.828660
584.116435	37783.462974	31.833677
584.831201	37840.436277	31.838695
584.959153	37895.575509	31.843712
585.941599	37942.868321	31.848730
585.820147	38007.632041	31.853748
586.608555	38066.263548	31.858765
587.143438	38126.392443	31.863783
587.949307	38196.267725	31.868800
589.212013	38228.745901	31.873818
590.436879	38261.877486	31.878836
591.096436	38300.014405	31.883853
591.919298	38336.826993	31.888871
592.398967	38379.387710	31.893888
593.445240	38402.549598	31.898906
593.891321	38435.959173	31.903924
594.202295	38435.797082	31.908941
595.112631	38471.695830	31.913959
595.344620	38506.886607	31.918976
595.660655	38527.168113	31.923994
596.219156	38558.905257	31.929012
596.340924	38591.810275	31.934029
596.910628	38639.795266	31.939047
597.170527	38686.045250	31.944064
597.531579	38731.075926	31.949082
597.780930	38785.803130	31.954100
598.239037	38829.918328	31.959117
599.207783	38883.080681	31.964135
599.316187	38951.250200	31.969152
600.193292	39007.837200	31.974170
600.181306	39066.762661	31.979188
601.192679	39138.567660	31.984205
602.021166	39198.240983	31.989223
602.120350	39255.469289	31.994240
602.856007	39312.857243	31.999258
603.276010	39383.265168	32.004276
604.247257	39448.496502	32.009293
604.201146	39512.811114	32.014311
604.837560	39596.962659	32.019328
605.869098	39653.753294	32.024346
606.041205	39734.819592	32.029364
606.892186	39793.992367	32.034381
607.569796	39866.054511	32.039399
608.048199	39947.822184	32.044416
608.678130	40003.168522	32.049434
609.338693	40086.058767	32.054452
609.624748	40160.592516	32.059469
610.395359	40244.936250	32.064487
610.808404	40317.934304	32.069504
611.840350	40392.215712	32.074522
612.462051	40468.522757	32.079540
612.903622	40536.481841	32.084557
614.070349	40598.720559	32.089575
614.726146	40668.103011	32.094592
615.429077	40730.444440	32.099610
616.215333	40802.470116	32.104628
617.106255	40864.941786	32.109645
617.860331	40921.046864	32.114663
618.155587	40985.821353	32.119680
618.925625	41044.743260	32.124698
619.526796	41106.995526	32.129716
620.183180	41161.627494	32.134733
620.982565	41214.275427	32.139751
621.043581	41280.800900	32.144768
621.939306	41340.031204	32.149786
622.731044	41393.258639	32.154804
623.066000	41458.435440	32.159821
624.157818	41516.402532	32.164839
624.257441	41591.203475	32.169856
624.630127	41642.828002	32.174874
625.243860	41714.993223	32.179892
625.486086	41781.389381	32.184909
626.657018	41848.420832	32.189927
627.250877	41919.403103	32.194944
627.622494	41975.852709	32.199962
628.524330	42046.967441	32.204980
629.047504	42118.672553	32.209997
630.423124	42185.510228	32.215015
630.997266	42248.850551	32.220032
631.503633	42305.458741	32.225050
631.790918	42363.981970	32.230068
632.547092	42430.595042	32.235085
633.262419	42489.934752	32.240103
633.654272	42542.742532	32.245120
634.634457	42601.432447	32.250138
634.961036	42659.375478	32.255156
635.800920	42715.793784	32.260173
636.383915	42767.667510	32.265191
636.530104	42823.689858	32.270208
637.527122	42883.100869	32.275226
638.321237	42943.549757	32.280244
638.443417	43010.232286	32.285261
639.441463	43067.945125	32.290279
640.031822	43128.330569	32.295296
640.124650	43187.090738	32.300314
640.608325	43252.088118	32.305332
641.248047	43328.587075	32.310349
641.917686	43396.986057	32.315367
641.948163	43475.774783	32.320384
643.167708	43558.161520	32.325402
643.925641	43629.224107	32.330420
644.531060	43706.598576	32.335437
645.960771	43757.507247	32.340455
646.526488	43831.305220	32.345472
647.270545	43887.471451	32.350490
648.364108	43949.282075	32.355508
649.332791	44004.928283	32.360525
649.824047	44058.484784	32.365543
650.180083	44103.639891	32.370560
650.761004	44170.083047	32.375578
651.503431	44235.618696	32.380596
651.930227	44310.644611	32.385613
652.609241	44363.311982	32.390631
652.771411	44432.373667	32.395648
653.622622	44497.178580	32.400666
654.497960	44559.305311	32.405684
655.054504	44634.108897	32.410701
655.709341	44697.706206	32.415719
655.960542	44768.958295	32.420736
656.508520	44841.411767	32.425754
657.207121	44921.630202	32.430772
657.826000	44996.585916	32.435789
658.783815	45060.001529	32.440807
659.486947	45128.417062	32.445824
660.056985	45196.065540	32.450842
661.492400	45267.141845	32.455860
662.215126	45327.297686	32.460877
662.844526	45389.859544	32.465895
663.235850	45458.125957	32.470912
663.940574	45522.402982	32.475930
664.874425	45577.608097	32.480948
665.538860	45647.178174	32.485965
666.169642	45708.304116	32.490983
666.513620	45768.274792	32.496000
667.393849	45837.481341	32.501018
668.124740	45890.899072	32.506036
668.375851	45970.151064	32.511053
669.374193	46033.136934	32.516071
669.975261	46092.813336	32.521088
670.763110	46157.577650	32.526106
671.343917	46221.915526	32.531124
672.071209	46287.846086	32.536141
672.479362	46353.182513	32.541159
673.010965	46422.736448	32.546176
673.567940	46494.594793	32.551194
674.179360	46565.455968	32.556212
674.495468	46652.341977	32.561229
675.199333	46725.509420	32.566247
675.677310	46795.796776	32.571264
676.205686	46883.520173	32.576282
677.071001	46957.672229	32.581300
677.530209	47037.712028	32.586317
678.316629	47094.313427	32.591335
679.435061	47171.345371	32.596352
679.810733	47234.634411	32.601370
680.492856	47307.384542	32.606388
680.942938	47382.093520	32.611405
681.883444	47459.487759	32.616423
682.465792	47535.299620	32.621440
683.147324	47601.292869	32.626458
684.255897	47669.666067	32.631476
684.547463	47752.386280	32.636493
685.598793	47823.611761	32.641511
686.189046	47899.133218	32.646528
686.749734	47960.966514	32.651546
687.775143	48042.887166	32.656564
688.412995	48127.158972	32.661581
689.181897	48187.057263	32.666599
689.905421	48260.903180	32.671616
690.718466	48314.333044	32.676634
692.383906	48369.863813	32.681652
693.004188	48432.045611	32.686669
693.646840	48483.031413	32.691687
694.176346	48549.643758	32.696704
694.516261	48614.910849	32.701722
695.412066	48676.261314	32.706740
696.130957	48752.058497	32.711757
697.145457	48800.580025	32.716775
697.904651	48857.513321	32.721792
698.307034	48921.634130	32.726810
699.313433	48979.894260	32.731828
699.350938	49047.439583	32.736845
700.200746	49108.527462	32.741863
700.726204	49175.076331	32.746880
701.150079	49256.025082	32.751898
702.074883	49318.882448	32.756916
702.366392	49399.348452	32.761933
702.853311	49485.467316	32.766951
703.897121	49563.639348	32.771968
704.277890	49652.543278	32.776986
705.110660	49724.623820	32.782004
705.852230	49807.840381	32.787021
706.508730	49878.358946	32.792039
706.970387	49968.893263	32.797056
707.778395	50051.506069	32.802074
708.435844	50138.818688	32.807092
708.808001	50231.838982	32.812109
709.623779	50314.521111	32.817127
710.357893	50400.918870	32.822144
710.863213	50488.924764	32.827162
711.705370	50584.556594	32.832180
712.146646	50683.780347	32.837197
713.029059	50763.500127	32.842215
714.371720	50852.145658	32.847232
715.328582	50939.112124	32.852250
716.350657	51011.987273	32.857268
716.749416	51089.028106	32.862285
717.452894	51162.758992	32.867303
718.347682	51241.196301	32.872320
718.845418	51330.666553	32.877338
719.526806	51406.556211	32.882356
720.111253	51492.835236	32.887373
720.424377	51566.821982	32.892391
721.452538	51654.822179	32.897408
721.909894	51743.315531	32.902426
722.862784	51825.024266	32.907444
723.663953	51915.571332	32.912461
724.257545	52002.084844	32.917479
726.729666	52030.684208	32.922496
727.722747	52093.738274	32.927514
728.520781	52140.961691	32.932532
729.270050	52185.514694	32.937549
730.148157	52226.192723	32.942567
730.649554	52278.368117	32.947584
731.273281	52327.415105	32.952602
732.108784	52370.482227	32.957620
732.573779	52423.156823	32.962637
732.999081	52486.900276	32.967655
733.654387	52536.068899	32.972672
733.799522	52599.928726	32.977690
733.960196	52662.143589	32.982708
734.665435	52742.437910	32.987725
735.349581	52811.218872	32.992743
736.203622	52891.128992	32.997760
736.870161	52977.167208	33.002778
737.708773	53048.178804	33.007796
738.503633	53136.413961	33.012813
738.836125	53213.246754	33.017831
739.221936	53296.091924	33.022848
740.059557	53385.887937	33.027866
741.102486	53471.373045	33.032884
741.633883	53563.349848	33.037901
742.094771	53657.777528	33.042919
742.958927	53745.119404	33.047936
743.469818	53836.045781	33.052954
744.586937	53933.202645	33.057972
745.406336	54015.486061	33.062989
746.101949	54114.602908	33.068007
747.310629	54183.522745	33.073024
747.646213	54292.948303	33.078042
748.562949	54373.087828	33.083060
749.429277	54454.796652	33.088077
750.788180	54528.741035	33.093095
751.842920	54615.783456	33.098112
752.546438	54701.210213	33.103130
753.333377	54773.430790	33.108148
753.937737	54856.758037	33.113165
754.239523	54936.528061	33.118183
755.078405	55021.662042	33.123200
755.860022	55117.951641	33.128218
756.468001	55205.563667	33.133236
756.765728	55288.615076	33.138253
757.864099	55379.154072	33.143271
758.342426	55473.777109	33.148288
758.921586	55573.735708	33.153306
759.722402	55659.352647	33.158324
760.418806	55752.898241	33.163341
761.090354	55862.207204	33.168359
761.886851	55946.391757	33.173376
762.580298	56066.654864	33.178394
763.428877	56160.189753	33.183412
764.237223	56261.933581	33.188429
765.344530	56342.213739	33.193447
766.607112	56429.292822	33.198464
767.550497	56511.913584	33.203482
768.400638	56590.973660	33.208500
769.512953	56660.992353	33.213517
770.187453	56751.342579	33.218535
770.797402	56824.547856	33.223552
771.297095	56910.845753	33.228570
772.040672	56995.991386	33.233588
773.001478	57085.044425	33.238605
773.982020	57156.034595	33.243623
775.057977	57237.871750	33.248640
775.480469	57327.805123	33.253658
775.921946	57392.812915	33.258676
776.786807	57480.657726	33.263693
777.039747	57557.286766	33.268711
778.083671	57629.494028	33.273728
778.728601	57702.829420	33.278746
779.561149	57782.257333	33.283764
780.082827	57861.831955	33.288781
780.833976	57953.318687	33.293799
781.854223	58031.699016	33.298816
782.110682	58119.799288	33.303834
783.010653	58204.867230	33.308852
783.310908	58301.763995	33.313869
784.428655	58401.129155	33.318887
785.111221	58494.550863	33.323904
785.848926	58585.341239	33.328922
786.809573	58676.524747	33.333940
787.426217	58784.620167	33.338957
787.860370	58873.730658	33.343975
788.792781	58971.258787	33.348992
789.439870	59086.005380	33.354010
790.513220	59178.834536	33.359028
791.125230	59269.509825	33.364045
791.943873	59383.540777	33.369063
793.245646	59479.689214	33.374080
793.685729	59576.151781	33.379098
794.502585	59675.642691	33.384116
795.701593	59783.292872	33.389133
796.442202	59878.556768	33.394151
797.458293	59975.544980	33.399168
798.475639	60071.440085	33.404186
799.115620	60164.080263	33.409204
800.209893	60249.617538	33.414221
800.951347	60346.033743	33.419239
801.868527	60436.379196	33.424256
802.395737	60541.913917	33.429274
803.303626	60642.671133	33.434292
803.933201	60741.515778	33.439309
804.690355	60845.674018	33.444327
805.632483	60928.957798	33.449344
806.114676	61038.275770	33.454362
806.926463	61139.632867	33.459380
808.219267	61242.686649	33.464397
808.654879	61341.515837	33.469415
809.548572	61430.738250	33.474432
810.700362	61546.622177	33.479450
811.425709	61637.775900	33.484468
812.488480	61731.516000	33.489485
812.794386	61835.943813	33.494503
813.853918	61930.127800	33.499520
814.438129	62025.168556	33.504538
815.398761	62120.968954	33.509556
816.968696	62198.610500	33.514573
817.613467	62300.746917	33.519591
818.692985	62385.650895	33.524608
819.220881	62482.403394	33.529626
820.461792	62564.601323	33.534644
821.031515	62654.445396	33.539661
822.039602	62746.536846	33.544679
823.141414	62831.773975	33.549696
823.201491	62914.472709	33.554714
823.998530	63005.690143	33.559732
824.911916	63090.959623	33.564749
825.479749	63192.329442	33.569767
826.647515	63284.030178	33.574784
827.786574	63373.018044	33.579802
828.266795	63453.291456	33.584820
828.901916	63547.572272	33.589837
829.419643	63646.354673	33.594855
830.117506	63747.143055	33.599872
830.731522	63849.583030	33.604890
831.675036	63943.005350	33.609908
832.484065	64040.274762	33.614925
833.065491	64144.447303	33.619943
834.024588	64234.593937	33.624960
835.055726	64325.158857	33.629978
835.511486	64417.899399	33.634996
836.922472	64508.756069	33.640013
837.531786	64603.488473	33.645031
838.594089	64695.813512	33.650048
839.035906	64802.819249	33.655066
839.806948	64899.163417	33.660084
840.465027	64989.925911	33.665101
841.409891	65096.590479	33.670119
842.278337	65205.803234	33.675136
842.837856	65318.595304	33.680154
843.493744	65409.979511	33.685172
844.399357	65532.475923	33.690189
844.772654	65651.034469	33.695207
845.908045	65762.260391	33.700224
846.699884	65884.253045	33.705242
847.192463	66003.482867	33.710260
848.884616	66102.296945	33.715277
850.665909	66196.924250	33.720295
852.102840	66282.271673	33.725312
852.955310	66381.232764	33.730330
853.566727	66481.517692	33.735348
854.764348	66572.937185	33.740365
855.600500	66656.653622	33.745383
856.539206	66747.358207	33.750400
857.491675	66841.531723	33.755418
858.039758	66941.506935	33.760436
859.152930	67025.438071	33.765453
859.265768	67138.933653	33.770471
860.186474	67226.071265	33.775488
861.153669	67329.961745	33.780506
861.379211	67433.305674	33.785524
862.564678	67535.555086	33.790541
862.871463	67656.102225	33.795559
863.814173	67763.204324	33.800576
864.915191	67860.177513	33.805594
865.812620	67983.593689	33.810612
867.163827	68072.496851	33.815629
867.972309	68182.405232	33.820647
868.930494	68278.266001	33.825664
869.906441	68379.220224	33.830682
870.498177	68486.554948	33.835700
871.691554	68588.125306	33.840717
872.665247	68685.641867	33.845735
874.012099	68787.472226	33.850752
874.942958	68879.198905	33.855770
875.538039	68967.738155	33.860788
876.531361	69051.709884	33.865805
877.634558	69149.997429	33.870823
878.438368	69240.191352	33.875840
879.015038	69336.328875	33.880858
879.270462	69440.044349	33.885876
880.172528	69536.406974	33.890893
880.716559	69649.212138	33.895911
881.323185	69763.651476	33.900928
882.231194	69872.628930	33.905946
883.007561	69999.801151	33.910964
884.070917	70109.089149	33.915981
884.883497	70230.686121	33.920999
885.605117	70347.234056	33.926016
886.364917	70459.855929	33.931034
887.466021	70587.983131	33.936052
888.538485	70688.318930	33.941069
889.200170	70804.506229	33.946087
890.226115	70895.663023	33.951104
891.233417	71001.158258	33.956122
891.992765	71117.229866	33.961140
893.199546	71213.783436	33.966157
893.880398	71309.122105	33.971175
894.814730	71410.331541	33.976192
895.666429	71518.669071	33.981210
895.966900	71639.783579	33.986228
897.014085	71739.628925	33.991245
897.593219	71852.787639	33.996263
899.365116	71950.812647	34.001280
901.238742	72045.140870	34.006298
902.484853	72131.656440	34.011316
903.431522	72214.092695	34.016333
904.201048	72321.878766	34.021351
904.819053	72414.747535	34.026368
905.520456	72505.750000	34.031386
906.358587	72618.414426	34.036404
907.339755	72704.622129	34.041421
907.817315	72820.047714	34.046439
908.663194	72928.032813	34.051456
909.514359	73027.537207	34.056474
910.284621	73149.296791	34.061492
911.087312	73264.013083	34.066509
912.126044	73366.902851	34.071527
913.474539	73475.408036	34.076544
914.606841	73576.246925	34.081562
915.507182	73678.743746	34.086580
916.880830	73774.307144	34.091597
917.357264	73884.925902	34.096615
918.160954	73991.146190	34.101632
919.232725	74093.496350	34.106650
919.632968	74211.389611	34.111668
920.338384	74326.823306	34.116685
921.034324	74439.337346	34.121703
921.820478	74573.757207	34.126720
922.297894	74696.997004	34.131738
923.539774	74829.869219	34.136756
924.861480	74948.068875	34.141773
925.531124	75073.732777	34.146791
926.245153	75207.845941	34.151808
927.265243	75329.696370	34.156826
927.883395	75465.699090	34.161844
928.769594	75601.588595	34.166861
929.651493	75740.319437	34.171879
930.351553	75880.586615	34.176896
931.617571	76019.078370	34.181914
932.088024	76152.921465	34.186932
933.384892	76298.626463	34.191949
934.427888	76432.097936	34.196967
935.199971	76579.466771	34.201984
936.137180	76709.036011	34.207002
936.504255	76859.655380	34.212020
937.823713	76997.600437	34.217037
938.838511	77142.314158	34.222055
939.635048	77283.719047	34.227072
941.017482	77418.474723	34.232090
941.590075	77564.061544	34.237108
942.750733	77713.966751	34.242125
943.991174	77854.238951	34.247143
944.550233	77982.897942	34.252160
945.957281	78119.962522	34.257178
947.167404	78270.679231	34.262196
948.150559	78386.448558	34.267213
949.676636	78513.197974	34.272231
950.972359	78630.618248	34.277248
952.501956	78735.108864	34.282266
953.221645	78851.246919	34.287284
954.349102	78945.152983	34.292301
955.642738	79025.937815	34.297319
956.389538	79138.157294	34.302336
957.255693	79226.085872	34.307354
958.174101	79328.808281	34.312372
959.018220	79434.934084	34.317389
959.468766	79531.213220	34.322407
960.074996	79636.993580	34.327424
960.649720	79754.659570	34.332442
961.157850	79879.428517	34.337460
962.300852	80002.372152	34.342477
963.139612	80130.579515	34.347495
963.590692	80270.890265	34.352512
964.670285	80401.576936	34.357530
965.082875	80542.427139	34.362548
965.736591	80688.988618	34.367565
966.598512	80847.763885	34.372583
967.514239	81006.822338	34.377600
968.594167	81150.171952	34.382618
969.442990	81303.208368	34.387636
970.934839	81454.608140	34.392653
971.936629	81607.051845	34.397671
972.576304	81761.808855	34.402688
973.747632	81916.567259	34.407706
974.889766	82075.551314	34.412724
975.636782	82226.175120	34.417741
976.999965	82384.036477	34.422759
977.464008	82545.439188	34.427776
978.493098	82689.566095	34.432794
979.420303	82856.164228	34.437812
980.831163	83020.443644	34.442829
982.453059	83166.923623	34.447847
983.317024	83320.034276	34.452864
984.665550	83466.751332	34.457882
985.576993	83623.829392	34.462900
986.563122	83758.530391	34.467917
987.700596	83920.084066	34.472935
988.229504	84061.392148	34.477952
989.633273	84209.806730	34.482970
990.592312	84359.979071	34.487988
991.680064	84505.980421	34.493005
992.870434	84652.769214	34.498023
993.390376	84808.813024	34.503040
994.690123	84950.004935	34.508058
995.557453	85091.725025	34.513076
996.683017	85239.888651	34.518093
997.665319	85392.670671	34.523111
998.765141	85540.315306	34.528128
999.950159	85686.175050	34.533146
1000.432533	85828.893635	34.538164
1001.040140	85990.011785	34.543181
1002.664174	86139.344933	34.548199
1003.521856	86308.244672	34.553216
1004.302942	86449.746862	34.558234
1005.462790	86598.584145	34.563252
1007.268280	86748.454233	34.568269
1008.656178	86879.714944	34.573287
1010.196288	87014.463073	34.578304
1011.570705	87129.521875	34.583322
1013.597802	87212.093188	34.588340
1015.398045	87314.970695	34.593357
1016.848656	87397.916749	34.598375
1018.171707	87499.937715	34.603392
1019.612174	87566.585253	34.608410
1020.155080	87640.912219	34.613428
1020.938032	87723.033663	34.618445
1022.343252	87802.451318	34.623463
1023.039831	87879.506230	34.628480
1024.160668	87935.380554	34.633498
1024.952810	88020.102343	34.638516
1025.487401	88088.160959	34.643533
1026.221069	88164.128538	34.648551
1026.531634	88253.601230	34.653568
1027.156655	88342.224731	34.658586
1027.927029	88444.259217	34.663604
1028.602913	88553.669552	34.668621
1028.885629	88671.093927	34.673639
1029.398735	88789.822251	34.678656
1030.667181	88918.051221	34.683674
1030.778245	89052.472214	34.688692
1031.459132	89204.607539	34.693709
1032.455045	89346.724263	34.698727
1032.817759	89503.413809	34.703744
1033.962882	89647.349152	34.708762
1034.919272	89825.674456	34.713780
1035.316636	89999.056267	34.718797
1036.607683	90161.500681	34.723815
1037.130562	90345.698835	34.728832
1037.899592	90524.478115	34.733850
1038.454231	90720.458010	34.738868
1039.783194	90902.849544	34.743885
1041.074655	91090.672550	34.748903
1042.145976	91281.508154	34.753920
1043.161500	91474.740556	34.758938
1044.335030	91673.612788	34.763956
1045.283487	91850.131631	34.768973
1046.607037	92044.342784	34.773991
1047.793206	92236.280787	34.779008
1049.324794	92429.384539	34.784026
1050.406107	92619.589765	34.789044
1050.912560	92814.505955	34.794061
1052.473926	93004.824416	34.799079
1053.403948	93196.546654	34.804096
1054.670978	93369.517143	34.809114
1056.094046	93548.570972	34.814132
1057.343625	93735.845385	34.819149
1058.961035	93909.261591	34.824167
1060.101168	94081.891048	34.829184
1061.611493	94237.730844	34.834202
1062.967943	94406.022479	34.839220
1063.792340	94582.657611	34.844237
1064.807629	94739.000486	34.849255
1065.692784	94895.511530	34.854272
1067.303611	95050.206744	34.859290
1068.597704	95214.228883	34.864308
1069.607957	95381.774379	34.869325
1070.875924	95520.539820	34.874343
1072.217519	95686.798046	34.879360
1073.478962	95831.155778	34.884378
1074.650251	95982.859638	34.889396
1074.897812	96128.558398	34.894413
1076.409751	96291.469054	34.899431
1077.465650	96447.923587	34.904448
1078.470722	96596.341696	34.909466
1079.818012	96751.192527	34.914484
1080.517410	96901.916778	34.919501
1081.667719	97055.536098	34.924519
1082.605625	97214.616821	34.929536
1083.584377	97372.052173	34.934554
1084.991363	97524.308705	34.939572
1086.160555	97678.207255	34.944589
1087.711138	97815.096373	34.949607
1088.791338	97967.694692	34.954624
1089.867299	98106.702619	34.959642
1091.092422	98250.725833	34.964660
1092.035340	98392.372005	34.969677
1092.939108	98526.542452	34.974695
1093.525491	98672.858178	34.979712
1094.425932	98819.932997	34.984730
1095.280845	98949.169377	34.989748
1095.936053	99116.659490	34.994765
1096.954550	99257.424294	34.999783
1098.009507	99421.779569	35.004800
1098.428440	99586.178120	35.009818
1099.395006	99751.664461	35.014836
1100.244826	99926.629991	35.019853
1101.509106	100099.571619	35.024871
1102.329622	100290.600432	35.029888
1103.530464	100468.366830	35.034906
1104.488703	100647.643584	35.039924
1105.320994	100841.846557	35.044941
1106.692704	101025.755244	35.049959
1107.637375	101219.613197	35.054976
1109.635683	101399.925634	35.059994
1111.316193	101557.257843	35.065012
1112.165577	101732.191453	35.070029
1113.746873	101905.624524	35.075047
1114.817018	102088.330841	35.080064
1115.839820	102266.512784	35.085082
1117.203158	102424.960308	35.090100
1118.252559	102601.962438	35.095117
1119.314116	102781.065936	35.100135
1120.184354	102961.329488	35.105152
1121.603459	103143.174866	35.110170
1122.624511	103314.468808	35.115188
1122.956547	103515.315803	35.120205
1124.602336	103694.075378	35.125223
1125.351000	103889.866456	35.130240
1126.771704	104069.045867	35.135258
1128.039029	104248.935830	35.140276
1128.985490	104443.583763	35.145293
1129.961855	104620.333085	35.150311
1131.213391	104818.099333	35.155328
1132.617533	105008.356858	35.160346
1133.432613	105198.447520	35.165364
1134.680370	105382.755867	35.170381
1136.081924	105571.536084	35.175399
1137.247342	105769.425074	35.180416
1138.382922	105959.176738	35.185434
1139.496434	106143.917948	35.190452
1141.011359	106327.491958	35.195469
1142.283326	106500.696497	35.200487
1143.181720	106696.204920	35.205504
1144.314992	106886.799520	35.210522
1145.750004	107076.306832	35.215540
1146.342120	107267.804538	35.220557
1147.621012	107454.465279	35.225575
1148.474681	107648.240186	35.230592
1149.681880	107830.254334	35.235610
1151.005068	108025.005360	35.240628
1152.395399	108218.847351	35.245645
1153.284256	108409.354001	35.250663
1154.422890	108598.997238	35.255680
1155.568764	108791.946586	35.260698
1157.394615	108968.799167	35.265716
1158.268949	109161.644201	35.270733
1160.057957	109346.928764	35.275751
1160.900580	109533.194943	35.280768
1162.305639	109702.939976	35.285786
1163.428672	109882.030503	35.290804
1164.710365	110065.314058	35.295821
1165.861325	110242.666921	35.300839
1167.033636	110412.366319	35.305856
1168.486057	110592.179577	35.310874
1170.160745	110755.641402	35.315892
1170.672957	110909.213658	35.320909
1171.740133	111073.018842	35.325927
1172.687381	111235.983493	35.330944
1173.671613	111397.258159	35.335962
1174.668478	111565.448333	35.340980
1175.252543	111754.673479	35.345997
1176.699011	111926.959035	35.351015
1177.598069	112117.629245	35.356032
1178.349020	112293.566873	35.361050
1179.514086	112474.795610	35.366068
1180.814235	112681.542574	35.371085
1181.940135	112865.162016	35.376103
1183.385646	113062.399023	35.381120
1184.041579	113255.397725	35.386138
1185.765669	113446.459619	35.391156
1187.087112	113644.430779	35.396173
1188.164450	113826.443005	35.401191
1189.526879	114021.736900	35.406208
1190.582604	114223.379570	35.411226
1191.751470	114415.832439	35.416244
1192.773615	114617.002078	35.421261
1194.182409	114813.687414	35.426279
1195.474938	115018.552529	35.431296
1196.250160	115220.540274	35.436314
1197.965896	115413.251322	35.441332
1198.861095	115620.555934	35.446349
1199.907263	115828.369150	35.451367
1201.112042	116037.297869	35.456384
1202.332821	116238.192698	35.461402
1203.949416	116446.561983	35.466420
1205.163292	116661.398035	35.471437
1206.271072	116860.656205	35.476455
1207.865728	117067.703292	35.481472
1208.997273	117273.067506	35.486490
1210.636922	117476.917138	35.491508
1211.523001	117686.379600	35.496525
1212.857264	117897.986620	35.501543
1213.993220	118087.910326	35.506560
1215.903860	118274.526388	35.511578
1218.278507	118441.363344	35.516596
1220.336450	118609.368852	35.521613
1221.562826	118783.506708	35.526631
1223.353436	118928.623719	35.531648
1224.146959	119109.132905	35.536666
1225.293160	119264.584190	35.541684
1226.393458	119435.325617	35.546701
1227.381005	119594.213586	35.551719
1228.412047	119762.168025	35.556736
1229.104755	119950.124667	35.561754
1230.413378	120121.532496	35.566772
1230.929448	120309.533419	35.571789
1231.765100	120490.893175	35.576807
1233.057944	120688.170195	35.581824
1233.618110	120889.865884	35.586842
1234.859149	121093.908408	35.591860
1235.898979	121301.141096	35.596877
1237.444360	121501.473694	35.601895
1238.463795	121711.817357	35.606912
1239.119758	121929.712231	35.611930
1240.312785	122141.550846	35.616948
1241.381460	122368.479382	35.621965
1242.623858	122579.704645	35.626983
1243.694536	122796.649991	35.632000
1244.968397	123034.638300	35.637018
1246.452758	123246.753276	35.642036
1247.812737	123475.847021	35.647053
1248.691386	123691.233893	35.652071
1249.962635	123915.048305	35.657088
1250.787255	124126.848039	35.662106
1252.170990	124340.457545	35.667124
1252.874554	124564.510347	35.672141
1253.964587	124795.788071	35.677159
1255.468092	125009.585218	35.682176
1256.635346	125240.156466	35.687194
1258.335041	125457.346170	35.692212
1259.628134	125689.889768	35.697229
1260.744470	125919.080459	35.702247
1262.321534	126154.318110	35.707264
1263.362945	126384.323193	35.712282
1264.731628	126596.544192	35.717300
1265.965187	126828.688063	35.722317
1267.046406	127069.465020	35.727335
1268.606590	127295.499768	35.732352
1269.652492	127520.937032	35.737370
1271.840736	127753.677335	35.742388
1273.104060	127988.930347	35.747405
1274.073478	128213.624839	35.752423
1275.838763	128433.182255	35.757440
1277.282619	128674.025613	35.762458
1278.854401	128869.661940	35.767476
1280.639397	129097.130188	35.772493
1281.917514	129298.217646	35.777511
1283.651927	129513.364021	35.782528
1285.090713	129724.073707	35.787546
1286.399250	129921.230644	35.792564
1287.432189	130123.200649	35.797581
1288.326122	130344.044132	35.802599
1289.933668	130555.200394	35.807616
1290.807673	130786.051659	35.812634
1291.823710	130990.742696	35.817652
1292.782507	131230.202949	35.822669
1293.691658	131458.758859	35.827687
1295.106833	131693.443958	35.832704
1296.081739	131934.516739	35.837722
1297.369575	132172.256175	35.842740
1298.899721	132402.908902	35.847757
1300.200151	132641.093409	35.852775
1302.011003	132866.353271	35.857792
1303.363873	133117.843405	35.862810
1305.706535	133323.254746	35.867828
1308.401228	133507.869103	35.872845
1309.721056	133714.783677	35.877863
1311.609174	133890.038703	35.882880
1312.908206	134092.331900	35.887898
1314.255963	134286.428605	35.892916
1315.155461	134465.172198	35.897933
1315.863076	134663.941241	35.902951
1317.567948	134868.859606	35.907968
1318.243064	135080.149486	35.912986
1319.396571	135276.021138	35.918004
1320.268502	135479.014960	35.923021
1321.385243	135699.414423	35.928039
1322.860328	135915.686246	35.933056
1323.737555	136147.348569	35.938074
1324.766671	136366.752755	35.943092
1325.761286	136598.335369	35.948109
1326.684139	136844.321576	35.953127
1327.947088	137078.309975	35.958144
1328.789746	137325.339994	35.963162
1329.852896	137577.787137	35.968180
1331.338363	137822.102388	35.973197
1332.426715	138079.874249	35.978215
1333.553446	138343.765701	35.983232
1334.392945	138609.836949	35.988250
1335.474585	138866.664997	35.993268
1336.897104	139126.303991	35.998285
1338.082783	139392.311291	36.003303
1339.735680	139647.655768	36.008320
1341.548780	139879.150565	36.013338
1343.834594	140113.992058	36.018356
1345.115402	140339.847022	36.023373
1346.727574	140583.045320	36.028391
1347.883111	140811.409418	36.033408
1349.489847	141061.205584	36.038426
1350.796563	141300.833111	36.043444
1352.059228	141538.225202	36.048461
1353.299259	141784.815908	36.053479
1354.770580	142025.258048	36.058496
1355.574680	142271.835740	36.063514
1357.047026	142510.759400	36.068532
1358.131472	142772.028981	36.073549
1359.266693	143036.373519	36.078567
1360.662950	143289.466864	36.083584
1361.753309	143549.764823	36.088602
1363.243357	143824.949392	36.093620
1365.051322	144090.179395	36.098637
1366.032704	144367.608336	36.103655
1367.751914	144634.493010	36.108672
1368.412241	144902.924881	36.113690
1369.630811	145183.618020	36.118708
1371.715436	145455.140408	36.123725
1372.851827	145741.634378	36.128743
1374.404915	146004.612802	36.133760
1375.435017	146293.145198	36.138778
1376.796485	146573.914266	36.143796
1378.681942	146846.367911	36.148813
1380.264059	147122.272743	36.153831
1381.893341	147389.573230	36.158848
1383.391653	147674.868380	36.163866
1384.685594	147935.050219	36.168884
1386.771824	148197.562943	36.173901
1388.323562	148461.130064	36.178919
1390.033421	148728.541098	36.183936
1391.468636	148995.771321	36.188954
1392.524562	149248.582424	36.193972
1393.719729	149516.984994	36.198989
1394.854492	149785.437566	36.204007
1396.427815	150062.177599	36.209024
1397.694886	150323.687052	36.214042
1398.591200	150603.409782	36.219060
1400.769718	150860.979495	36.224077
1402.296455	151137.697134	36.229095
1404.057541	151395.961221	36.234112
1405.411152	151660.243331	36.239130
1406.961548	151918.685440	36.244148
1408.450928	152176.581329	36.249165
1409.540549	152449.487046	36.254183
1411.262137	152692.685171	36.259200
1412.675559	152957.143928	36.264218
1414.067882	153222.128061	36.269236
1415.479802	153475.821670	36.274253
1416.991931	153737.187113	36.279271
1418.385365	153986.828113	36.284288
1419.543676	154251.452200	36.289306
1420.943124	154512.486381	36.294324
1422.757141	154773.567729	36.299341
1424.150761	155032.323089	36.304359
1426.090974	155282.858458	36.309376
1427.768203	155521.400929	36.314394
1428.978835	155779.430450	36.319412
1430.340596	156027.148897	36.324429
1431.836005	156286.872384	36.329447
1432.921499	156531.151337	36.334464
1434.276126	156757.145501	36.339482
1435.929031	156989.497670	36.344500
1437.148688	157216.861483	36.349517
1438.610893	157451.544050	36.354535
1440.723891	157665.099828	36.359552
1442.421343	157899.581092	36.364570
1443.693292	158117.477730	36.369588
1445.484646	158325.736911	36.374605
1446.784065	158554.071870	36.379623
1448.168998	158777.370250	36.384640
1449.092663	159019.534522	36.389658
1450.357234	159242.918843	36.394676
1451.221391	159489.129984	36.399693
1452.376701	159731.336181	36.404711
1453.317507	159996.224681	36.409728
1454.905335	160260.385962	36.414746
1455.362483	160536.217796	36.419764
1456.654757	160809.718196	36.424781
1457.892146	161089.966179	36.429799
1459.310662	161380.804928	36.434816
1460.603111	161680.991523	36.439834
1461.840097	161982.217116	36.444852
1463.255960	162289.822217	36.449869
1464.464340	162604.238952	36.454887
1465.594545	162902.317010	36.459904
1467.263001	163218.831555	36.464922
1468.553622	163543.340801	36.469940
1470.210395	163849.508947	36.474957
1471.559771	164188.692915	36.479975
1473.294783	164509.253350	36.484992
1474.354352	164826.870373	36.490010
1475.906675	165156.347428	36.495028
1477.547139	165489.847180	36.500045
1479.124502	165835.236093	36.505063
1480.542014	166162.053199	36.510080
1482.011664	166500.309014	36.515098
1483.383570	166834.764396	36.520116
1485.476014	167153.584711	36.525133
1486.902840	167503.807933	36.530151
1488.897026	167822.865045	36.535168
1490.867271	168132.868563	36.540186
1493.114629	168442.295342	36.545204
1494.803691	168742.858363	36.550221
1496.478150	169061.482407	36.555239
1497.738339	169365.305634	36.560256
1499.388524	169678.760840	36.565274
1500.532032	169995.271516	36.570292
1502.563642	170292.120749	36.575309
1503.773215	170605.261971	36.580327
1505.233002	170919.163279	36.585344
1506.477616	171227.112845	36.590362
1507.844599	171550.284607	36.595380
1509.349287	171856.050636	36.600397
1510.853791	172175.853795	36.605415
1512.482704	172495.511603	36.610432
1513.707110	172812.015346	36.615450
1514.797675	173135.764132	36.620468
1516.560085	173469.911314	36.625485
1517.762782	173799.927728	36.630503
1519.190499	174120.480077	36.635520
1520.947670	174446.906439	36.640538
1522.271201	174777.023741	36.645556
1524.481455	175100.117897	36.650573
1526.189623	175426.114806	36.655591
1527.659439	175753.371736	36.660608
1529.026291	176057.626457	36.665626
1530.334538	176396.640934	36.670644
1532.151305	176696.916158	36.675661
1533.532212	177018.739029	36.680679
1535.060653	177313.354723	36.685696
1536.869775	177617.431471	36.690714
1538.505866	177913.822339	36.695732
1540.223668	178207.485417	36.700749
1542.060926	178507.425439	36.705767
1542.844853	178794.329816	36.710784
1544.862897	179095.525199	36.715802
1545.934927	179418.264938	36.720820
1547.695336	179709.683165	36.725837
1549.401532	180008.003778	36.730855
1550.773648	180319.467010	36.735872
1552.216352	180626.985848	36.740890
1553.277677	180947.477705	36.745908
1555.005010	181253.963057	36.750925
1556.775823	181574.772668	36.755943
1558.360336	181885.550011	36.760960
1560.466683	182192.181064	36.765978
1561.608989	182518.774144	36.770996
1564.012261	182832.226351	36.776013
1565.589805	183149.345863	36.781031
1567.428794	183457.196227	36.786048
1569.014875	183749.871506	36.791066
1570.414105	184077.586503	36.796084
1572.376063	184368.654260	36.801101
1573.450470	184694.434002	36.806119
1574.759105	185002.012914	36.811136
1576.607657	185322.425756	36.816154
1578.224357	185633.701618	36.821172
1579.579260	185952.473639	36.826189
1581.031675	186258.182437	36.831207
1582.768811	186582.378250	36.836224
1584.723474	186898.009768	36.841242
1586.063197	187225.575487	36.846260
1587.601253	187534.564654	36.851277
1589.370329	187860.184170	36.856295
1590.210897	188196.533461	36.861312
1591.971494	188515.404942	36.866330
1593.134627	188857.493049	36.871348
1594.432567	189197.148937	36.876365
1596.150710	189532.052986	36.881383
1598.671475	189869.352048	36.886400
1600.670733	190185.121059	36.891418
1602.454656	190509.064548	36.896436
1604.949415	190816.376478	36.901453
1606.524524	191131.611480	36.906471
1608.317611	191430.245566	36.911488
1610.161383	191734.407592	36.916506
1611.611930	192041.213352	36.921524
1613.692033	192347.865516	36.926541
1615.070031	192636.710493	36.931559
1616.328167	192962.049132	36.936576
1617.878220	193255.045104	36.941594
1618.756721	193564.784255	36.946612
1620.375838	193883.974269	36.951629
1622.311632	194199.711113	36.956647
1623.601232	194515.048845	36.961664
1625.279808	194838.143961	36.966682
1626.658526	195174.976002	36.971700
1627.911597	195489.867581	36.976717
1629.623660	195819.005110	36.981735
1630.771096	196164.513589	36.986752
1632.108214	196499.239280	36.991770
1634.100729	196831.230042	36.996788
1635.929846	197166.055324	37.001805
1637.540098	197501.629546	37.006823
1638.735203	197843.012806	37.011840
1640.840295	198171.271735	37.016858
1641.999453	198500.412735	37.021876
1643.740284	198814.071311	37.026893
1645.413418	199151.763592	37.031911
1646.326178	199478.080848	37.036928
1648.009613	199808.131564	37.041946
1649.100560	200153.746149	37.046964
1650.492048	200489.320605	37.051981
1652.338919	200841.859781	37.056999
1653.548883	201184.082484	37.062016
1655.488045	201541.980475	37.067034
1656.671993	201901.478252	37.072052
1659.039913	202256.185391	37.077069
1660.975548	202612.908531	37.082087
1662.482966	202965.539855	37.087104
1664.480955	203323.398855	37.092122
1666.069671	203691.459579	37.097140
1667.716529	204038.016509	37.102157
1670.767661	204361.144810	37.107175
1672.825433	204700.907285	37.112192
1675.278347	205023.820170	37.117210
1676.862957	205361.302374	37.122228
1678.465295	205684.333655	37.127245
1680.047210	206008.588622	37.132263
1681.420364	206357.296585	37.137280
1682.561930	206695.010438	37.142298
1683.808926	207048.745186	37.147316
1685.277324	207406.723896	37.152333
1686.791399	207761.649230	37.157351
1688.160293	208125.882185	37.162368
1689.665137	208487.846762	37.167386
1691.608322	208863.187236	37.172404
1692.739120	209239.540235	37.177421
1694.638901	209614.980234	37.182439
1695.763011	210015.298781	37.187456
1697.276230	210398.552130	37.192474
1699.035818	210796.140592	37.197492
1700.249640	211204.919528	37.202509
1702.364303	211603.443358	37.207527
1704.014632	212016.191824	37.212544
1705.824222	212405.373206	37.217562
1707.953270	212815.176285	37.222580
1709.056202	213226.852914	37.227597
1710.776451	213625.857638	37.232615
1712.391007	214053.199361	37.237632
1714.146079	214465.002126	37.242650
1715.761345	214881.198239	37.247668
1717.430968	215306.174711	37.252685
1719.103523	215721.272991	37.257703
1720.512113	216156.100002	37.262720
1722.438021	216584.570010	37.267738
1724.056755	217032.496794	37.272756
1725.249755	217454.768044	37.277773
1727.431565	217891.277935	37.282791
1729.135730	218326.548195	37.287808
1731.470487	218753.537573	37.292826
1733.071691	219187.939660	37.297844
1735.548145	219618.083966	37.302861
1737.719536	220015.973573	37.307879
1739.235074	220510.513907	37.312896
1741.047114	220913.977973	37.317914
1742.954853	221337.035659	37.322932
1744.943077	221757.262362	37.327949
1746.576693	222161.979781	37.332967
1748.566622	222581.752150	37.337984
1750.876784	222975.591127	37.343002
1752.755210	223387.968373	37.348020
1754.394702	223779.178132	37.353037
1755.984969	224174.461294	37.358055
1757.901589	224561.690811	37.363072
1759.267925	224944.898028	37.368090
1760.736934	225324.025481	37.373108
1761.952498	225705.024907	37.378125
1763.914237	226094.080642	37.383143
1764.790155	226493.350554	37.388160
1767.116054	226893.651440	37.393178
1768.847650	227290.165841	37.398196
1770.682963	227696.544978	37.403213
1772.503784	228097.466702	37.408231
1773.789023	228505.514314	37.413248
1775.511193	228920.501296	37.418266
1777.366610	229335.289656	37.423284
1778.630427	229750.024896	37.428301
1780.671743	230172.963959	37.433319
1782.672654	230596.266587	37.438336
1784.269498	231017.224332	37.443354
1786.235286	231448.993758	37.448372
1787.625139	231880.478861	37.453389
1789.497033	232305.687443	37.458407
1791.138730	232756.641341	37.463424
1792.686345	233190.796501	37.468442
1794.804478	233625.823552	37.473460
1796.827521	234076.870407	37.478477
1798.779474	234518.607942	37.483495
1800.675800	234959.085784	37.488512
1802.808159	235389.034792	37.493530
1804.829931	235822.813437	37.498548
1806.414097	236262.152429	37.503565
1808.402463	236706.353454	37.508583
1810.434665	237148.592344	37.513600
1812.156317	237577.014303	37.518618
1814.186399	238026.088697	37.523636
1815.633497	238468.148164	37.528653
1817.831663	238905.333963	37.533671
1819.470483	239350.691258	37.538688
1821.117929	239786.369844	37.543706
1822.994959	240233.518479	37.548724
1825.047271	240689.910810	37.553741
1826.929713	241129.261857	37.558759
1828.738019	241573.731903	37.563776
1830.232382	242026.866227	37.568794
1832.019981	242486.481240	37.573812
1833.754633	242948.315892	37.578829
1835.242110	243414.485365	37.583847
1837.351278	243875.649942	37.588864
1839.403738	244335.122719	37.593882
1841.057202	244787.244779	37.598900
1842.903387	245248.429784	37.603917
1845.488783	245697.706130	37.608935
1847.538433	246160.205146	37.613952
1849.727909	246608.100433	37.618970
1851.931583	247049.363823	37.623988
1853.282146	247490.972359	37.629005
1855.332222	247935.158240	37.634023
1856.921585	248394.434136	37.639040
1858.417434	248837.391948	37.644058
1860.955284	249293.336346	37.649076
1862.737025	249748.136364	37.654093
1864.615606	250188.669679	37.659111
1866.355584	250638.523902	37.664128
1868.375285	251076.545141	37.669146
1870.655099	251508.960362	37.674164
1872.484671	251952.958149	37.679181
1874.565883	252382.155335	37.684199
1876.420800	252828.359636	37.689216
1878.186725	253258.828993	37.694234
1880.053967	253683.616900	37.699252
1881.735365	254100.611634	37.704269
1883.820860	254514.542035	37.709287
1885.487429	254952.827536	37.714304
1886.946130	255369.427876	37.719322
1888.396959	255795.657507	37.724340
1890.258415	256225.578924	37.729357
1891.876618	256647.233891	37.734375
1893.551608	257092.606216	37.739392
1894.732421	257537.145987	37.744410
1896.857903	257994.891436	37.749428
1898.017938	258457.979163	37.754445
1899.964386	258927.820908	37.759463
1901.555304	259397.467523	37.764480
1902.929878	259879.038695	37.769498
1904.896204	260371.333567	37.774516
1906.313758	260883.635446	37.779533
1907.961801	261368.336452	37.784551
1910.092013	261880.138925	37.789568
1911.632318	262388.076033	37.794586
1913.908533	262902.648255	37.799604
1915.743752	263420.011426	37.804621
1918.192515	263933.106519	37.809639
1920.440367	264460.612784	37.814656
1922.092279	264976.836777	37.819674
1924.378553	265484.369004	37.824692
1926.466023	266011.443361	37.829709
1928.327754	266514.066030	37.834727
1931.357899	267018.958747	37.839744
1933.550123	267527.393790	37.844762
1936.040832	268016.853572	37.849780
1937.814774	268529.853139	37.854797
1939.918202	269018.715477	37.859815
1942.050138	269510.189001	37.864832
1943.843177	270011.421953	37.869850
1946.203491	270519.393611	37.874868
1947.962964	271002.874128	37.879885
1950.210015	271489.854969	37.884903
1951.915810	271994.325638	37.889920
1953.341050	272509.587319	37.894938
1955.136099	273011.501248	37.899956
1956.879756	273523.355246	37.904973
1958.614219	274051.238855	37.909991
1960.372792	274569.286654	37.915008
1962.263651	275094.398798	37.920026
1964.331759	275625.678673	37.925044
1966.037217	276153.715161	37.930061
1967.829987	276689.458306	37.935079
1969.384382	277225.417505	37.940096
1971.462637	277762.101497	37.945114
1974.729265	278274.353661	37.950132
1977.790289	278792.684330	37.955149
1980.077483	279291.048903	37.960167
1982.378084	279804.498763	37.965184
1984.343755	280306.038476	37.970202
1986.198866	280801.828977	37.975220
1988.067669	281312.628311	37.980237
1990.469935	281803.626152	37.985255
1992.847372	282298.208376	37.990272
1994.686425	282784.572088	37.995290
1997.022074	283266.330694	38.000308
1998.594045	283772.015503	38.005325
2000.816117	284261.054821	38.010343
2002.355975	284744.795206	38.015360
2004.150868	285242.132269	38.020378
2005.585796	285740.187792	38.025396
2006.898201	286265.745822	38.030413
2008.770286	286777.442012	38.035431
2010.378006	287286.665529	38.040448
2012.242858	287791.247120	38.045466
2014.756429	288292.874579	38.050484
2016.089379	288792.587555	38.055501
2018.109456	289299.093791	38.060519
2020.106542	289801.385470	38.065536
2021.930148	290315.007073	38.070554
2023.735556	290822.965433	38.075572
2025.313763	291360.829827	38.080589
2027.309996	291874.467364	38.085607
2030.430868	292392.615437	38.090624
2032.782482	292903.395822	38.095642
2035.301447	293419.607221	38.100660
2037.405910	293924.328267	38.105677
2039.065826	294440.956865	38.110695
2040.971954	294967.346462	38.115712
2042.732069	295497.923252	38.120730
2044.650475	296034.617855	38.125748
2046.161546	296578.717582	38.130765
2048.117149	297111.489298	38.135783
2050.598737	297646.279315	38.140800
2052.615957	298207.837343	38.145818
2054.332568	298755.168256	38.150836
2056.382569	299318.238705	38.155853
2058.088111	299875.445320	38.160871
2059.919000	300445.936566	38.165888
2061.580876	301016.528685	38.170906
2064.131295	301590.754512	38.175924
2065.543440	302186.854863	38.180941
2067.560370	302773.098707	38.185959
2070.027778	303359.772181	38.190976
2072.108035	303956.537835	38.195994
2074.455386	304535.452154	38.201012
2076.534470	305143.410122	38.206029
2078.909704	305747.454585	38.211047
2080.953714	306331.969183	38.216064
2082.923444	306933.685281	38.221082
2085.550661	307525.815532	38.226100
2087.439952	308115.549648	38.231117
2090.112280	308695.702720	38.236135
2092.878401	309276.699591	38.241152
2094.910813	309874.676234	38.246170
2096.935861	310449.641744	38.251188
2098.875717	311043.739495	38.256205
2100.718441	311631.931873	38.261223
2102.875089	312228.397161	38.266240
2104.655626	312833.630316	38.271258
2106.842972	313417.257107	38.276276
2108.307870	314036.474191	38.281293
2110.193411	314632.635197	38.286311
2112.752212	315247.217031	38.291328
2115.059660	315861.987636	38.296346
2117.382040	316467.456660	38.301364
2119.820949	317071.453823	38.306381
2122.293487	317682.169236	38.311399
2124.829242	318270.091894	38.316416
2127.288757	318844.158057	38.321434
2129.695616	319426.353503	38.326452
2132.034587	320001.013834	38.331469
2134.297177	320590.154996	38.336487
2137.740744	321126.916336	38.341504
2140.027059	321685.371140	38.346522
2142.106678	322232.150212	38.351540
2144.396908	322781.073353	38.356557
2146.848707	323327.679881	38.361575
2149.083411	323866.548254	38.366592
2150.863982	324405.842672	38.371610
2152.813770	324951.985006	38.376628
2154.847496	325492.675257	38.381645
2156.166817	326023.221784	38.386663
2158.160573	326547.177777	38.391680
2159.517060	327083.802223	38.396698
2161.159190	327632.154857	38.401716
2162.956619	328183.497918	38.406733
2164.649560	328737.188825	38.411751
2166.633925	329290.166135	38.416768
2168.962720	329862.781921	38.421786
2171.132928	330420.008131	38.426804
2173.312488	331004.569270	38.431821
2174.856824	331583.212882	38.436839
2177.176938	332173.146014	38.441856
2178.909427	332762.890957	38.446874
2181.589843	333350.898682	38.451892
2183.888297	333943.177385	38.456909
2185.516228	334555.132879	38.461927
2187.827479	335165.952858	38.466944
2189.690726	335791.258667	38.471962
2191.204861	336415.320303	38.476980
2193.355347	337054.880489	38.481997
2195.325074	337695.985807	38.487015
2197.487801	338345.656276	38.492032
2199.227695	338999.779857	38.497050
2201.249750	339670.068038	38.502068
2203.343631	340327.771009	38.507085
2205.831351	341011.290081	38.512103
2208.243085	341676.791131	38.517120
2210.700660	342356.996933	38.522138
2212.874250	343031.859460	38.527156
2214.903965	343704.502891	38.532173
2217.051447	344404.832963	38.537191
2219.375763	345082.814292	38.542208
2220.989893	345792.222181	38.547226
2223.725424	346474.582221	38.552244
2226.030657	347177.382881	38.557261
2227.985959	347875.637251	38.562279
2230.091521	348592.864411	38.567296
2232.240432	349310.098448	38.572314
2234.482928	350028.193785	38.577332
2236.886272	350740.287351	38.582349
2239.335977	351464.821734	38.587367
2242.185690	352172.910297	38.592384
2244.506472	352899.650047	38.597402
2246.540938	353616.934634	38.602420
2248.691743	354334.340245	38.607437
2251.059151	355048.348497	38.612455
2253.459832	355768.327491	38.617472
2255.724932	356496.309307	38.622490
2257.766534	357231.825900	38.627508
2260.053718	357945.468203	38.632525
2262.387648	358674.364513	38.637543
2264.747671	359392.638051	38.642560
2267.449776	360114.216613	38.647578
2270.326157	360823.118641	38.652596
2273.525303	361510.567301	38.657613
2275.968049	362206.374568	38.662631
2279.066070	362896.403625	38.667648
2281.870626	363583.754606	38.672666
2284.322035	364251.491138	38.677684
2286.799484	364906.958926	38.682701
2289.206496	365572.447500	38.687719
2291.642494	366223.866111	38.692736
2294.445647	366878.865590	38.697754
2296.839378	367517.306377	38.702772
2299.270971	368168.260886	38.707789
2300.988922	368810.190531	38.712807
2303.177005	369442.620703	38.717824
2305.193666	370091.961358	38.722842
2307.420210	370716.753769	38.727860
2310.006416	371319.231727	38.732877
2312.308378	371933.921209	38.737895
2315.017941	372527.379889	38.742912
2317.040776	373138.823116	38.747930
2319.102355	373742.869024	38.752948
2321.200235	374357.753472	38.757965
2323.098824	374971.037062	38.762983
2325.272398	375601.864860	38.768000
2327.047147	376238.351931	38.773018
2329.437841	376868.715028	38.778036
2331.574817	377504.535542	38.783053
2333.169716	378164.119342	38.788071
2335.506317	378826.635973	38.793088
2337.356228	379493.810042	38.798106
2339.256784	380168.417639	38.803124
2341.677559	380852.358344	38.808141
2343.715589	381536.272320	38.813159
2345.970166	382232.281838	38.818176
2348.968632	382916.084335	38.823194
2351.680735	383620.153166	38.828212
2354.382998	384302.555828	38.833229
2356.462201	385005.938800	38.838247
2358.909533	385705.341087	38.843264
2361.568445	386401.726825	38.848282
2363.862575	387104.723944	38.853300
2366.316721	387800.225629	38.858317
2368.091544	388514.989789	38.863335
2370.408635	389226.250935	38.868352
2372.725657	389956.330790	38.873370
2374.802001	390685.089795	38.878388
2377.311478	391408.994337	38.883405
2379.677968	392148.215664	38.888423
2381.775336	392880.341011	38.893440
2384.208314	393624.255421	38.898458
2386.018019	394371.194818	38.903476
2388.779568	395125.130822	38.908493
2391.052886	395888.658259	38.913511
2393.639085	396645.068557	38.918528
2395.844002	397400.508832	38.923546
2398.188320	398163.179988	38.928564
2400.701678	398930.668929	38.933581
2403.692246	399690.050631	38.938599
2406.975865	400442.876559	38.943616
2409.818226	401188.103026	38.948634
2412.158101	401933.570591	38.953652
2414.511257	402682.082394	38.958669
2416.538473	403432.756727	38.963687
2419.723360	404176.758288	38.968704
2422.319126	404911.766955	38.973722
2424.946941	405665.499683	38.978740
2427.761418	406395.466923	38.983757
2429.960077	407137.601467	38.988775
2432.173465	407874.038608	38.993792
2434.268265	408619.114192	38.998810
2436.457976	409368.840154	39.003828
2438.698054	410120.994151	39.008845
2440.756415	410886.304117	39.013863
2442.990353	411641.253526	39.018880
2445.762306	412395.839126	39.023898
2448.177359	413167.103524	39.028916
2450.472144	413911.897006	39.033933
2452.942615	414674.546904	39.038951
2455.721332	415436.971481	39.043968
2457.869543	416207.151833	39.048986
2460.136985	416972.224357	39.054004
2462.789778	417747.112239	39.059021
2464.832475	418517.848494	39.064039
2467.278913	419254.384238	39.069056
2469.457330	420000.185584	39.074074
2471.496600	420754.546593	39.079092
2473.989786	421505.771245	39.084109
2476.389915	422269.420856	39.089127
2478.966085	423031.372071	39.094144
2481.563650	423785.548751	39.099162
2483.673786	424555.176193	39.104180
2486.109812	425327.257188	39.109197
2488.656495	426106.940874	39.114215
2490.831784	426875.572821	39.119232
2494.204705	427633.906852	39.124250
2497.075036	428405.108881	39.129268
2500.261859	429166.817223	39.134285
2503.285126	429914.353442	39.139303
2506.778986	430647.816304	39.144320
2509.370787	431385.354101	39.149338
2511.838578	432137.012111	39.154356
2514.128000	432881.690206	39.159373
2516.502275	433634.378424	39.164391
2518.630473	434383.489287	39.169408
2520.760314	435151.099909	39.174426
2523.231201	435921.108390	39.179444
2525.608593	436682.907674	39.184461
2527.903558	437469.594173	39.189479
2530.238653	438256.651581	39.194496
2532.871476	439041.051447	39.199514
2535.063019	439822.966837	39.204532
2537.866940	440627.321470	39.209549
2540.147224	441426.724422	39.214567
2542.497795	442226.643487	39.219584
2545.070699	443027.508669	39.224602
2547.768515	443845.981065	39.229620
2550.651300	444653.970384	39.234637
2552.453333	445478.803141	39.239655
2554.817875	446316.107738	39.244672
2557.281106	447153.515275	39.249690
2559.065878	447991.154206	39.254708
2561.290733	448847.959104	39.259725
2563.271912	449719.589656	39.264743
2565.287380	450597.854907	39.269760
2567.818680	451488.894923	39.274778
2569.746654	452396.837812	39.279796
2572.508832	453292.668455	39.284813
2574.911055	454208.899262	39.289831
2577.138325	455116.825557	39.294848
2580.138257	456044.910769	39.299866
2582.827745	456975.533422	39.304884
2585.582920	457893.968442	39.309901
2588.380177	458827.572689	39.314919
2591.560788	459743.325562	39.319936
2595.140351	460645.119266	39.324954
2598.099849	461555.113561	39.329972
2600.921502	462464.937460	39.334989
2603.704063	463374.726090	39.340007
2606.019434	464279.344136	39.345024
2608.904583	465193.429069	39.350042
2611.510049	466096.752825	39.355060
2614.213689	466997.390549	39.360077
2617.159019	467891.983426	39.365095
2619.571433	468789.705471	39.370112
2622.252546	469674.506665	39.375130
2624.714174	470585.324690	39.380148
2627.487062	471479.980854	39.385165
2630.088088	472371.440368	39.390183
2632.977360	473271.600566	39.395200
2635.837531	474154.799162	39.400218
2637.976828	475043.429994	39.405236
2640.606832	475908.701470	39.410253
2643.190236	476774.041369	39.415271
2646.320286	477626.522320	39.420288
2649.053543	478458.726193	39.425306
2651.845279	479313.558674	39.430324
2654.846224	480147.257630	39.435341
2657.541602	480984.857375	39.440359
2660.142920	481832.381790	39.445376
2662.588528	482671.914161	39.450394
2665.158406	483526.130366	39.455412
2668.255702	484359.921925	39.460429
2670.464938	485224.012639	39.465447
2672.625530	486087.110232	39.470464
2675.297151	486950.586051	39.475482
2678.435031	487813.538641	39.480500
2681.144210	488676.923618	39.485517
2683.146804	489554.111994	39.490535
2685.801733	490440.132325	39.495552
2688.799695	491312.524948	39.500570
2691.360161	492197.007538	39.505588
2694.287510	493077.700169	39.510605
2697.208961	493974.546761	39.515623
2699.852223	494868.970337	39.520640
2702.466500	495755.278766	39.525658
2704.838698	496656.767499	39.530676
2707.559598	497555.829736	39.535693
2710.233419	498469.179042	39.540711
2713.140367	499377.698185	39.545728
2716.713333	500259.827538	39.550746
2719.501311	501163.325700	39.555764
2722.038304	502066.009166	39.560781
2724.748904	502978.146697	39.565799
2727.494290	503894.968487	39.570816
2730.761514	504802.726758	39.575834
2733.138152	505722.734573	39.580852
2735.532692	506635.275198	39.585869
2738.411412	507551.314592	39.590887
2740.750191	508478.886505	39.595904
2743.361225	509406.662364	39.600922
2745.725301	510354.489136	39.605940
2748.114631	511295.853556	39.610957
2750.601433	512260.887089	39.615975
2753.045026	513226.221771	39.620992
2755.323270	514192.028717	39.626010
2758.189299	515173.150663	39.631028
2760.719352	516161.523254	39.636045
2763.600667	517147.356343	39.641063
2766.107954	518134.448360	39.646080
2769.091676	519121.549689	39.651098
2771.410283	520139.026558	39.656116
2774.243248	521145.217602	39.661133
2776.951148	522159.322050	39.666151
2779.315004	523184.900173	39.671168
2782.203543	524213.545551	39.676186
2784.658702	525243.602683	39.681204
2787.391645	526276.464140	39.686221
2789.787898	527327.438232	39.691239
2792.950501	528363.861009	39.696256
2796.078554	529409.833823	39.701274
2799.264868	530455.420953	39.706292
2802.567596	531488.631191	39.711309
2805.664665	532517.121224	39.716327
2807.968197	533565.149710	39.721344
2810.951203	534588.026103	39.726362
2813.777037	535637.630622	39.731380
2816.255626	536681.580038	39.736397
2818.928462	537725.421579	39.741415
2821.388342	538770.832452	39.746432
2824.247331	539780.932006	39.751450
2827.077012	540806.057481	39.756468
2829.495597	541818.399124	39.761485
2832.232399	542835.897249	39.766503
2835.536340	543852.523751	39.771520
2838.459567	544871.553594	39.776538
2841.221637	545892.044424	39.781556
2843.954553	546912.414894	39.786573
2847.217395	547938.304607	39.791591
2849.460923	548972.683423	39.796608
2852.368726	550008.282285	39.801626
2854.732910	551060.231284	39.806644
2857.247527	552105.137279	39.811661
2860.506539	553158.083226	39.816679
2862.990637	554227.862531	39.821696
2865.900090	555299.999498	39.826714
2868.612372	556378.867657	39.831732
2870.771237	557461.458828	39.836749
2873.853301	558559.284707	39.841767
2876.678782	559665.552910	39.846784
2879.930617	560781.655080	39.851802
2882.390132	561889.455376	39.856820
2885.121223	563006.007579	39.861837
2887.900329	564129.789129	39.866855
2890.401837	565275.816797	39.871872
2893.984765	566403.186026	39.876890
2897.524836	567536.489228	39.881908
2900.693953	568656.550032	39.886925
2903.959004	569776.898807	39.891943
2907.251333	570900.608446	39.896960
2910.458187	572016.202299	39.901978
2913.472304	573147.790028	39.906996
2917.060803	574251.630784	39.912013
2920.029507	575362.151073	39.917031
2922.824073	576488.005424	39.922048
2925.561689	577602.028012	39.927066
2928.712970	578729.427188	39.932084
2931.163055	579866.320276	39.937101
2933.753049	580995.211129	39.942119
2936.669574	582133.372986	39.947136
2940.387341	583254.998959	39.952154
2943.523612	584378.473419	39.957172
2946.609221	585511.880144	39.962189
2949.990610	586625.680437	39.967207
2953.063278	587751.861006	39.972224
2956.137546	588860.492938	39.977242
2959.488504	589971.983841	39.982260
2962.444912	591098.771699	39.987277
2965.895139	592201.468991	39.992295
2968.686925	593313.492301	39.997312
2972.189358	594409.161239	40.002330
2975.053540	595513.199882	40.007348
2977.476906	596628.778703	40.012365
2981.009692	597716.921013	40.017383
2983.666196	598822.685377	40.022400
2986.402952	599922.872943	40.027418
2989.442146	601035.123602	40.032436
2991.871545	602169.247293	40.037453
2994.292800	603297.303163	40.042471
2996.845925	604433.185349	40.047488
2999.524278	605564.429211	40.052506
3002.654475	606716.205495	40.057524
3005.047049	607863.733253	40.062541
3008.265043	609022.316399	40.067559
3010.944167	610190.075341	40.072576
3013.960668	611341.198272	40.077594
3016.847639	612518.085221	40.082612
3019.783368	613678.934726	40.087629
3023.062957	614810.449648	40.092647
3025.961573	615935.961183	40.097664
3029.201360	617061.201459	40.102682
3032.521392	618185.163381	40.107700
3035.210110	619311.463947	40.112717
3038.371359	620437.170326	40.117735
3041.175283	621565.418320	40.122752
3044.064463	622713.974619	40.127770
3047.362348	623845.801353	40.132788
3050.430577	624993.685641	40.137805
3054.302749	626115.985029	40.142823
3057.089215	627269.767158	40.147840
3060.321317	628414.659781	40.152858
3063.510632	629546.151325	40.157876
3066.561347	630687.582410	40.162893
3070.257872	631826.736099	40.167911
3073.417468	632968.751007	40.172928
3076.629506	634109.784246	40.177946
3079.935902	635244.737353	40.182964
3082.920628	636386.158308	40.187981
3086.432027	637521.927101	40.192999
3089.475789	638680.402767	40.198016
3092.096951	639830.136726	40.203034
3094.865316	640992.189895	40.208052
3097.393266	642162.132304	40.213069
3100.353457	643334.063874	40.218087
3103.138557	644519.404572	40.223104
3105.635218	645710.738083	40.228122
3108.545811	646915.773580	40.233140
3111.371696	648135.834408	40.238157
3114.482307	649355.749857	40.243175
3117.224890	650590.430128	40.248192
3119.968734	651838.063955	40.253210
3123.132958	653096.035368	40.258228
3126.191018	654361.786333	40.263245
3129.466855	655603.278096	40.268263
3132.459994	656890.384900	40.273280
3135.933341	658153.238479	40.278298
3139.187169	659424.081937	40.283316
3142.329546	660715.739438	40.288333
3145.438801	662000.410216	40.293351
3148.002244	663289.779109	40.298368
3151.105470	664584.460468	40.303386
3154.582420	665890.201675	40.308404
3157.574446	667211.269253	40.313421
3160.543942	668518.377008	40.318439
3163.420073	669844.670149	40.323456
3166.469160	671173.285414	40.328474
3169.773979	672494.560152	40.333492
3172.524254	673835.430480	40.338509
3175.823464	675175.521001	40.343527
3178.776330	676512.742505	40.348544
3181.765928	677881.275307	40.353562
3184.934790	679234.171785	40.358580
3188.014901	680615.652344	40.363597
3191.595462	681968.774971	40.368615
3196.114600	683295.267122	40.373632
3199.828991	684639.330085	40.378650
3202.937903	685980.662963	40.383668
3206.166360	687333.395508	40.388685
3209.351650	688663.495094	40.393703
3212.936111	690014.873335	40.398720
3215.809410	691353.064450	40.403738
3218.780288	692697.291281	40.408756
3221.801926	694041.207881	40.413773
3224.993009	695381.669001	40.418791
3227.796741	696739.647497	40.423808
3230.262856	698070.447137	40.428826
3233.495171	699401.563357	40.433844
3236.972870	700714.887833	40.438861
3240.080881	702035.015257	40.443879
3243.631045	703342.925827	40.448896
3247.251669	704653.204300	40.453914
3250.407919	705958.456232	40.458932
3253.257606	707282.484064	40.463949
3256.631736	708604.784908	40.468967
3259.799929	709925.281473	40.473984
3262.525156	711262.481478	40.479002
3266.135237	712599.473614	40.484020
3269.885524	713921.382538	40.489037
3273.268383	715253.884731	40.494055
3276.581344	716591.878149	40.499072
3279.823202	717931.500676	40.504090
3283.581253	719262.562645	40.509108
3286.569306	720614.509739	40.514125
3289.749676	721964.029454	40.519143
3292.803286	723313.548155	40.524160
3296.867582	724657.043879	40.529178
3301.266690	725986.524616	40.534196
3304.449118	727328.296087	40.539213
3307.553985	728678.852868	40.544231
3310.493749	730032.720757	40.549248
3313.633385	731400.703506	40.554266
3317.012298	732750.735944	40.559284
3320.073152	734127.851060	40.564301
3323.313086	735499.912256	40.569319
3326.229144	736888.179656	40.574336
3329.388087	738276.610037	40.579354
3332.143546	739673.302729	40.584372
3335.446482	741082.683389	40.589389
3338.834891	742495.301046	40.594407
3342.534146	743902.189664	40.599424
3346.414204	745315.798253	40.604442
3350.605758	746696.908688	40.609460
3354.916813	748087.958068	40.614477
3358.600645	749468.365773	40.619495
3362.530135	750841.934176	40.624512
3365.888592	752240.575765	40.629530
3369.608190	753604.820089	40.634548
3372.024162	754983.515903	40.639565
3375.239221	756364.785824	40.644583
3378.159698	757765.348768	40.649600
3381.238143	759167.252186	40.654618
3384.400514	760570.211419	40.659636
3387.243247	761993.332135	40.664653
3389.884058	763420.792377	40.669671
3393.286502	764837.183274	40.674688
3396.316805	766284.346238	40.679706
3399.932786	767728.624638	40.684724
3402.861937	769186.892232	40.689741
3406.177467	770637.978390	40.694759
3409.555918	772097.269403	40.699776
3412.912946	773574.205060	40.704794
3416.730648	775038.440004	40.709812
3420.658425	776510.367743	40.714829
3424.320843	777972.518081	40.719847
3427.891402	779433.849634	40.724864
3431.184602	780896.061061	40.729882
3434.774527	782355.670521	40.734900
3438.021452	783826.813787	40.739917
3441.719102	785292.627542	40.744935
3445.591534	786740.312604	40.749952
3449.897594	788171.895222	40.754970
3454.433441	789586.633545	40.759988
3458.426406	791005.785471	40.765005
3461.521341	792408.226891	40.770010
3465.517578	793753.483402	40.775015
3468.699001	795046.961704	40.780020
3471.969532	796281.863740	40.785024
3474.660704	797438.500011	40.790029
3477.234664	798544.855798	40.795034
3479.973679	799567.540429	40.800039
3482.414389	800540.030120	40.805044
3484.631490	801437.510680	40.810048
3487.129422	802294.410474	40.815053
3489.212638	803075.890231	40.820058
3491.040585	803805.831629	40.825063
3493.053814	804471.330961	40.830068
3494.904408	805090.066415	40.835072
3496.450240	805666.339385	40.840077
3498.323506	806176.427043	40.845082
3499.704725	806654.793321	40.850087
3500.944777	807068.839963	40.855092
3501.962888	807446.676997	40.860096
3503.209770	807796.910962	40.865101
3504.123451	808102.387767	40.870106
3505.150573	808365.489993	40.875111
3506.563620	808606.220799	40.880116
3507.565523	808797.958069	40.885120
3508.466929	808977.896861	40.890125
3509.425102	809110.975892	40.895130
3510.374058	809220.190358	40.900135
3510.766714	809302.642783	40.905140
3511.417944	809351.486485	40.910144
3512.183270	809402.956968	40.915149
3512.427584	809411.050571	40.920154
3512.973067	809401.895510	40.925159
3513.907457	809383.807203	40.930164
3514.201835	809344.754568	40.935168
3514.564278	809280.210185	40.940173
3514.955116	809211.789411	40.945178
3515.167137	809116.152547	40.950183
3515.560189	809019.259361	40.955188
3516.037146	808886.578499	40.960192
3516.353062	808768.573965	40.965197
3516.317924	808616.174676	40.970202
3516.600162	808462.102314	40.975207
3516.951910	808315.905202	40.980212
3516.947912	808133.938335	40.985216
3517.426308	807955.366617	40.990221
3517.260342	807773.171823	40.995226
3517.718744	807572.048047	41.000231
3517.650778	807370.221088	41.005236
3518.001052	807151.555611	41.010240
3518.118582	806940.078141	41.015245
3517.951728	806731.827343	41.020250
3518.453042	806503.851574	41.025255
3518.248661	806274.170988	41.030260
3518.425760	806033.438285	41.035264
3518.463845	805791.298335	41.040269
3518.573948	805542.470180	41.045274
3518.850856	805292.085511	41.050279
3518.695477	805046.224950	41.055284
3518.428713	804788.409957	41.060288
3518.597908	804535.514770	41.065293
3518.427572	804281.979855	41.070298
3518.576120	804021.223284	41.075303
3518.170823	803758.341521	41.080308
3518.812251	803488.999342	41.085312
3518.455744	803235.701785	41.090317
3518.388707	802962.336359	41.095322
3518.424487	802691.395480	41.100327
3518.273080	802432.344911	41.105332
3518.467533	802147.377246	41.110336
3518.416156	801881.275040	41.115341
3518.279716	801620.425565	41.120346
3518.051381	801337.015013	41.125351
3517.892892	801078.258171	41.130356
3517.888625	800798.517012	41.135360
3517.822039	800538.498250	41.140365
3517.561943	800267.658321	41.145370
3518.196966	800001.811918	41.150375
3517.624778	799734.437392	41.155380
3517.797359	799446.074388	41.160384
3517.741374	799183.696693	41.165389
3517.656750	798914.148918	41.170394
3517.423478	798640.836348	41.175399
3517.115088	798368.801478	41.180404
3517.285666	798099.130837	41.185408
3517.150593	797834.261233	41.190413
3516.815239	797576.335503	41.195418
3517.140394	797309.602865	41.200423
3516.656767	797057.130950	41.205428
3516.851364	796783.036577	41.210432
3516.430647	796509.622212	41.215437
3516.448201	796262.389696	41.220442
3516.441347	795990.163028	41.225447
3516.081325	795741.894390	41.230452
3516.102781	795477.007606	41.235456
3516.046848	795217.819262	41.240461
3515.786776	794967.837213	41.245466
3516.209780	794722.791095	41.250471
3515.485976	794459.118350	41.255476
3515.324433	794211.204584	41.260480
3515.493918	793969.611583	41.265485
3515.378973	793715.681263	41.270490
3515.522876	793475.990847	41.275495
3515.275350	793224.618554	41.280500
3515.300375	792978.791501	41.285504
3514.974283	792732.620934	41.290509
3514.879126	792494.704830	41.295514
3515.113368	792258.396385	41.300519
3514.732105	792018.841361	41.305524
3514.837639	791773.351913	41.310528
3514.536510	791539.269321	41.315533
3514.559466	791301.146041	41.320538
3514.684267	791051.255901	41.325543
3514.589045	790823.551552	41.330548
3514.194695	790591.762130	41.335552
3513.914013	790355.082001	41.340557
3513.903066	790131.468746	41.345562
3513.884987	789892.567765	41.350567
3513.482157	789675.589333	41.355572
3513.791025	789448.855045	41.360576
3513.936607	789231.084413	41.365581
3513.614126	789019.576570	41.370586
3513.678375	788787.062579	41.375591
3513.660850	788575.048790	41.380596
3513.335694	788341.503327	41.385600
3513.508207	788121.089333	41.390605
3513.286719	787908.892775	41.395610
3513.155822	787693.824043	41.400615
3513.143968	787475.829024	41.405620
3513.255286	787256.479766	41.410624
3512.759098	787038.748027	41.415629
3512.453360	786828.302857	41.420634
3512.771478	786622.123665	41.425639
3512.618554	786423.144818	41.430644
3512.479158	786212.801490	41.435648
3512.480874	786002.625306	41.440653
3512.058341	785797.577154	41.445658
3512.271398	785598.908197	41.450663
3512.179461	785405.053495	41.455668
3511.764023	785197.085987	41.460672
3512.055744	784993.716057	41.465677
3511.944905	784815.780104	41.470682
3512.023791	784615.237451	41.475687
3511.543140	784415.076701	41.480692
3511.568426	784217.138074	41.485696
3511.504146	784033.568835	41.490701
3511.455520	783847.484161	41.495706
3511.262346	783648.828265	41.500711
3511.082715	783473.034322	41.505716
3511.035159	783282.065796	41.510720
3510.624295	783106.645381	41.515725
3510.431629	782921.249100	41.520730
3510.644468	782747.044866	41.525735
3510.407467	782571.090787	41.530740
3510.313228	782405.192638	41.535744
3510.250166	782233.481037	41.540749
3510.134369	782065.020709	41.545754
3510.290240	781894.937381	41.550759
3509.969342	781734.226483	41.555764
3510.185087	781574.210446	41.560768
3509.909613	781404.039236	41.565773
3509.852356	781241.797917	41.570778
3510.123380	781068.478260	41.575783
3509.621270	780914.224039	41.580788
3509.687194	780745.063274	41.585792
3509.481067	780584.307810	41.590797
3509.811215	780435.564045	41.595802
3509.609322	780277.851640	41.600807
3509.637578	780123.689724	41.605812
3509.533783	779955.965495	41.610816
3509.434996	779799.898643	41.615821
3509.460481	779648.630290	41.620826
3509.465904	779494.163500	41.625831
3509.322871	779337.946383	41.630836
3509.257237	779173.396398	41.635840
3509.370562	779021.460699	41.640845
3509.096723	778879.477683	41.645850
3508.990071	778720.977455	41.650855
3509.342791	778572.929963	41.655860
3508.905134	778411.377103	41.660864
3508.902274	778265.547633	41.665869
3508.834235	778136.607927	41.670874
3508.837912	777972.068488	41.675879
3508.786561	777829.585212	41.680884
3508.603358	777689.877332	41.685888
3508.658763	777552.637679	41.690893
3508.105831	777414.413053	41.695898
3508.339897	777271.970145	41.700903
3508.087270	777140.582083	41.705908
3508.285113	776998.878200	41.710912
3508.267552	776859.668509	41.715917
3507.737009	776726.989784	41.720922
3508.153612	776593.364472	41.725927
3508.038661	776477.448762	41.730932
3508.217239	776347.648962	41.735936
3508.110249	776215.432478	41.740941
3507.765444	776069.763253	41.745946
3507.799934	775950.515916	41.750951
3507.717308	775828.676586	41.755956
3507.674712	775695.110727	41.760960
3507.860305	775565.443579	41.765965
3507.538573	775441.569409	41.770970
3507.808327	775311.588436	41.775975
3507.392679	775195.308174	41.780980
3507.432686	775076.833491	41.785984
3507.477671	774955.057001	41.790989
3507.207100	774836.186588	41.795994
3507.456468	774712.304183	41.800999
3507.323987	774592.619135	41.806004
3507.477422	774462.100646	41.811008
3507.473847	774349.973775	41.816013
3506.925834	774238.230623	41.821018
3506.885995	774108.968904	41.826023
3507.007122	774003.267285	41.831028
3506.995393	773880.989865	41.836032
3506.929699	773769.701590	41.841037
3506.827948	773660.535274	41.846042
3506.828236	773550.710233	41.851047
3506.716274	773445.925596	41.856052
3506.593829	773328.976275	41.861056
3506.225060	773223.541392	41.866061
3506.365655	773120.631189	41.871066
3506.650873	773016.464328	41.876071
3506.584319	772907.133246	41.881076
3506.174139	772812.584342	41.886080
3506.221266	772703.871758	41.891085
3505.941804	772605.653728	41.896090
3506.352206	772505.547164	41.901095
3506.226483	772406.611486	41.906100
3506.084943	772299.352558	41.911104
3506.106801	772190.439541	41.916109
3506.055938	772105.279773	41.921114
3506.018188	772007.752710	41.926119
3505.779329	771920.750011	41.931124
3505.829629	771818.969526	41.936128
3505.712802	771727.757211	41.941133
3505.681465	771641.061750	41.946138
3505.823897	771546.454534	41.951143
3505.612476	771460.279333	41.956148
3505.366561	771366.029556	41.961152
3505.512695	771274.620396	41.966157
3505.175719	771187.231142	41.971162
3505.511863	771111.898226	41.976167
3505.394042	771029.693041	41.981172
3505.191462	770932.080467	41.986176
3505.445961	770845.426965	41.991181
3505.519991	770769.986077	41.996186
3505.319313	770676.015627	42.001191
3505.363789	770585.994266	42.006196
3505.238968	770501.025290	42.011200
3505.262527	770418.888489	42.016205
3505.014355	770342.412539	42.021210
3505.450217	770256.559774	42.026215
3505.433819	770177.235355	42.031220
3505.500107	770082.868352	42.036224
3505.267095	770001.360585	42.041229
3504.970153	769920.503040	42.046234
3505.151261	769844.591564	42.051239
3504.646046	769766.526097	42.056244
3504.928458	769692.370205	42.061248
3504.994291	769617.608779	42.066253
3504.703135	769538.421473	42.071258
3504.885421	769455.508619	42.076263
3504.694272	769385.912085	42.081268
3504.511704	769316.362757	42.086272
3504.734471	769234.081347	42.091277
3504.615645	769171.665444	42.096282
3504.776595	769096.291704	42.101287
3504.489103	769023.948071	42.106292
3504.539751	768958.496323	42.111296
3504.812251	768887.290818	42.116301
3504.560123	768809.961937	42.121306
3504.710103	768742.077104	42.126311
3504.616473	768671.817099	42.131316
3504.527045	768601.062913	42.136320
3504.682053	768524.255166	42.141325
3504.390719	768463.931694	42.146330
3504.714425	768392.762274	42.151335
3504.272716	768328.716996	42.156340
3504.561999	768250.997124	42.161344
3504.449876	768175.166320	42.166349
3504.239652	768114.580183	42.171354
3504.173228	768050.716921	42.176359
3504.007468	767992.882455	42.181364
3504.430879	767926.867162	42.186368
3504.374218	767856.691917	42.191373
3504.045929	767797.897049	42.196378
3504.063509	767720.906566	42.201383
3503.961887	767664.389726	42.206388
3504.086934	767604.926959	42.211392
3504.077503	767540.162698	42.216397
3503.944306	767471.475147	42.221402
3504.316623	767407.533866	42.226407
3504.210135	767362.302977	42.231412
3504.122759	767292.028905	42.236416
3504.102763	767232.833591	42.241421
3503.640529	767172.823635	42.246426
3504.405771	767111.033009	42.251431
3503.801874	767053.017182	42.256436
3503.713692	766987.225986	42.261440
3503.668240	766926.159310	42.266445
3503.607975	766865.686108	42.271450
3503.725676	766814.746066	42.276455
3503.619415	766763.300446	42.281460
3503.641602	766702.812298	42.286464
3503.974648	766649.124325	42.291469
3503.653940	766597.762295	42.296474
3504.024210	766532.680061	42.301479
3503.685294	766484.770977	42.306484
3503.392826	766423.888899	42.311488
3503.588571	766382.545855	42.316493
3503.509829	766334.740705	42.321498
3503.492710	766267.600395	42.326503
3503.412719	766226.252753	42.331508
3503.517017	766176.050038	42.336512
3503.751302	766120.994238	42.341517
3503.450891	766056.166579	42.346522
3503.513231	766010.505200	42.351527
3503.570134	765954.491499	42.356532
3503.380458	765905.173639	42.361536
3503.621250	765851.347281	42.366541
3503.015057	765811.168905	42.371546
3503.171275	765764.159390	42.376551
3502.964787	765725.640038	42.381556
3503.045715	765676.275951	42.386560
3503.009578	765635.016393	42.391565
3503.004205	765593.455712	42.396570
3503.257504	765539.920860	42.401575
3502.980359	765500.179460	42.406580
3503.141597	765450.455493	42.411584
3503.222541	765410.851657	42.416589
3503.062639	765368.279890	42.421594
3503.454897	765315.213506	42.426599
3503.335652	765270.070655	42.431604
3503.221464	765225.419742	42.436608
3503.235859	765170.541200	42.441613
3502.925521	765124.344339	42.446618
3503.105841	765069.191110	42.451623
3503.316726	765046.327758	42.456628
3503.315318	765006.587476	42.461632
3503.044629	764955.107274	42.466637
3502.748138	764910.435300	42.471642
3502.695813	764865.328256	42.476647
3502.622015	764834.819416	42.481652
3502.918818	764796.902414	42.486656
3503.009623	764759.315107	42.491661
3502.394202	764710.947264	42.496666
3502.696937	764674.803750	42.501671
3502.431286	764640.479782	42.506676
3502.510233	764612.706068	42.511680
3502.678470	764577.817028	42.516685
3502.416494	764536.292883	42.521690
3502.624015	764506.130690	42.526695
3502.626960	764480.341417	42.531700
3502.510149	764446.189201	42.536704
3502.932143	764402.529593	42.541709
3502.669986	764375.304467	42.546714
3502.729373	764335.747822	42.551719
3502.633883	764293.751028	42.556724
3502.299815	764254.160350	42.561728
3502.697244	764231.411623	42.566733
3502.353865	764204.297919	42.571738
3502.486952	764158.416314	42.576743
3502.597733	764144.048344	42.581748
3502.732962	764104.379324	42.586752
3502.709325	764059.509252	42.591757
3502.339986	764029.982907	42.596762
3502.531782	763995.925582	42.601767
3502.729392	763959.253559	42.606772
3502.370634	763919.566567	42.611776
3502.870412	763897.638243	42.616781
3502.590320	763863.017221	42.621786
3502.731040	763821.225317	42.626791
3502.792929	763793.204821	42.631796
3502.894317	763749.693030	42.636800
3503.051544	763708.982688	42.641805
3502.596765	763662.800684	42.646810
3502.772698	763620.163491	42.651815
3503.045169	763600.195153	42.656820
3502.781593	763548.704118	42.661824
3502.515405	763504.758493	42.666829
3502.284017	763483.097734	42.671834
3502.578031	763460.166503	42.676839
3502.462213	763419.943562	42.681844
3502.502419	763381.075490	42.686848
3502.374478	763353.676526	42.691853
3502.256606	763337.766660	42.696858
3502.481830	763294.478356	42.701863
3502.261925	763259.006208	42.706868
3501.975557	763231.287754	42.711872
3502.449341	763206.994469	42.716877
3502.017853	763184.231604	42.721882
3502.310564	763157.403545	42.726887
3502.239460	763133.249382	42.731892
3502.319420	763103.941056	42.736896
3502.351740	763070.497716	42.741901
3502.290055	763040.226173	42.746906
3502.460486	763004.293770	42.751911
3502.517970	762983.274302	42.756916
3502.233735	762949.389542	42.761920
3502.259125	762923.837814	42.766925
3502.493882	762897.412965	42.771930
3502.585909	762845.907671	42.776935
3502.275106	762824.554057	42.781940
3502.182436	762793.941402	42.786945
3502.517872	762764.342934	42.791949
3502.138368	762734.566568	42.796954
3502.281733	762708.008194	42.801959
3502.347510	762688.120917	42.806964
3502.352034	762653.743216	42.811969
3502.280952	762619.772425	42.816973
3502.014224	762593.281414	42.821978
3502.375923	762563.677820	42.826983
3502.142974	762538.512729	42.831988
3501.763746	762503.753858	42.836993
3502.168289	762493.378633	42.841997
3502.088395	762464.932718	42.847002
3501.988354	762434.073204	42.852007
3501.900880	762416.134126	42.857012
3502.005998	762400.234751	42.862017
3502.197589	762366.811291	42.867021
3502.000866	762358.508172	42.872026
3502.139245	762318.631925	42.877031
3502.068577	762301.972213	42.882036
3501.904118	762260.764638	42.887041
3501.995298	762246.741555	42.892045
3502.027907	762218.078821	42.897050
3502.255588	762196.831737	42.902055
3502.172263	762173.909627	42.907060
3502.106215	762146.989286	42.912065
3501.967393	762116.184203	42.917069
3501.753675	762100.040933	42.922074
3501.560589	762072.204141	42.927079
3501.876223	762050.103581	42.932084
3501.763396	762029.158921	42.937089
3501.621477	762009.896083	42.942093
3501.544744	761994.272531	42.947098
3502.069633	761970.164128	42.952103
3501.918571	761953.664908	42.957108
3501.640199	761936.989386	42.962113
3501.911231	761924.415769	42.967117
3501.745890	761913.246051	42.972122
3501.641804	761880.362559	42.977127
3501.966985	761872.169966	42.982132
3501.649198	761843.465057	42.987137
3501.721013	761814.103734	42.992141
3501.441982	761813.755250	42.997146
3501.734357	761789.388731	43.002151
3502.000259	761780.021984	43.007156
3501.835524	761756.520131	43.012161
3501.826890	761731.315274	43.017165
3501.367573	761730.503302	43.022170
3501.516592	761695.702735	43.027175
3501.837664	761682.972465	43.032180
3501.712544	761664.347229	43.037185
3501.985115	761634.113457	43.042189
3501.726797	761629.124695	43.047194
3502.015193	761598.394884	43.052199
3501.601270	761584.897996	43.057204
3501.641494	761573.397834	43.062209
3502.042453	761539.097526	43.067213
3501.559625	761532.813924	43.072218
3501.661799	761508.329944	43.077223
3501.653207	761489.586363	43.082228
3501.616014	761475.040441	43.087233
3501.901990	761444.063757	43.092237
3501.735649	761436.691858	43.097242
3501.921071	761409.678001	43.102247
3501.531529	761386.310803	43.107252
3501.729112	761383.269059	43.112257
3501.605767	761359.019181	43.117261
3502.070382	761342.416884	43.122266
3501.981222	761320.183763	43.127271
3502.017728	761297.683160	43.132276
3501.806620	761280.847078	43.137281
3502.080592	761248.490325	43.142285
3501.855697	761235.257555	43.147290
3501.704303	761205.240121	43.152295
3501.531944	761188.397430	43.157300
3501.608177	761177.778674	43.162305
3501.771818	761150.175516	43.167309
3501.405430	761146.190917	43.172314
3501.709574	761121.277658	43.177319
3501.695392	761103.175350	43.182324
3501.640153	761091.838226	43.187329
3501.836061	761072.418505	43.192333
3501.529487	761052.489785	43.197338
3501.601155	761048.136753	43.202343
3501.312307	761022.877174	43.207348
3501.507266	761013.373207	43.212353
3501.595427	760998.706989	43.217357
3501.713736	760982.062466	43.222362
3501.583241	760962.449738	43.227367
3501.411214	760955.867628	43.232372
3501.201770	760944.013106	43.237377
3501.739536	760909.194011	43.242381
3501.539805	760921.757573	43.247386
3501.453581	760892.468118	43.252391
3501.428251	760873.972440	43.257396
3501.479931	760869.573276	43.262401
3501.656039	760855.040246	43.267405
3501.479267	760834.448169	43.272410
3501.584650	760813.908077	43.277415
3501.507897	760813.970115	43.282420
3501.493819	760788.861681	43.287425
3501.617702	760768.663745	43.292429
3501.507153	760770.359383	43.297434
3501.528544	760746.626293	43.302439
3501.682331	760727.755321	43.307444
3501.446901	760718.420774	43.312449
3501.634777	760697.472062	43.317453
3501.194260	760688.072698	43.322458
3501.538093	760664.335401	43.327463
3501.850931	760655.600858	43.332468
3501.880294	760632.507441	43.337473
3501.847889	760628.319371	43.342477
3501.655970	760608.173192	43.347482
3501.844969	760580.958447	43.352487
3501.888795	760570.196190	43.357492
3501.738642	760539.929232	43.362497
3501.709030	760524.985547	43.367501
3501.655185	760510.884540	43.372506
3501.543536	760483.916470	43.377511
3501.487479	760482.297679	43.382516
3501.623662	760464.662352	43.387521
3501.744779	760436.915614	43.392525
3501.530213	760436.408397	43.397530
3501.509667	760407.402226	43.402535
3501.651956	760402.691801	43.407540
3501.549727	760400.587261	43.412545
3501.665529	760374.370593	43.417549
3501.198914	760354.614486	43.422554
3501.218303	760356.091398	43.427559
3501.158733	760343.816474	43.432564
3501.259372	760334.376579	43.437569
3501.425617	760307.065938	43.442573
3501.277683	760295.940284	43.447578
3501.372437	760291.829688	43.452583
3501.586584	760290.758247	43.457588
3501.190324	760270.398251	43.462593
3501.365664	760250.831812	43.467597
3501.792869	760248.837090	43.472602
3501.744654	760228.814165	43.477607
3501.403432	760215.401480	43.482612
3501.700057	760205.139641	43.487617
3501.491711	760175.966267	43.492621
3501.484623	760171.576409	43.497626
3501.517473	760150.701141	43.502631
3501.308280	760140.424124	43.507636
3501.033634	760120.388992	43.512641
3501.360225	760108.099211	43.517645
3501.233799	760115.915537	43.522650
3501.560441	760115.614891	43.527655
3501.485980	760098.506902	43.532660
3501.281598	760072.786144	43.537665
3501.593675	760067.159364	43.542669
3501.307338	760070.709724	43.547674
3501.062573	760035.078502	43.552679
3502.009203	760011.831616	43.557684
3501.310534	760023.739033	43.562689
3501.355693	760001.825210	43.567693
3501.421831	759987.259351	43.572698
3501.308440	759977.607686	43.577703
3501.379109	759972.810153	43.582708
3501.410352	759968.068470	43.587713
3501.324565	759936.160274	43.592717
3501.440501	759939.742898	43.597722
3501.588446	759922.548419	43.602727
3501.283247	759903.800583	43.607732
3501.392492	759895.345509	43.612737
3501.414591	759879.997290	43.617741
3501.552355	759877.902284	43.622746
3501.675208	759849.807733	43.627751
3501.585532	759849.230497	43.632756
3501.501244	759835.922699	43.637761
3501.658908	759811.177362	43.642765
3501.323136	759793.421104	43.647770
3501.484298	759789.792664	43.652775
3501.438080	759776.527811	43.657780
3501.461273	759752.347245	43.662785
3501.564037	759740.340560	43.667789
3501.123583	759746.827625	43.672794
3501.545645	759717.400288	43.677799
3501.539495	759705.066161	43.682804
3501.614886	759698.984815	43.687809
3501.507930	759685.779181	43.692813
3501.467022	759664.470695	43.697818
3501.505608	759664.908409	43.702823
3501.739696	759656.777826	43.707828
3501.061406	759626.397125	43.712833
3501.669136	759618.303439	43.717837
3501.258602	759615.657531	43.722842
3501.767717	759590.656033	43.727847
3501.337443	759574.543145	43.732852
3501.461255	759567.170812	43.737857
3501.628568	759549.330848	43.742861
3501.577233	759525.556609	43.747866
3501.723109	759520.302284	43.752871
3501.559983	759515.888490	43.757876
3501.182863	759480.227187	43.762881
3501.752037	759474.458802	43.767885
3501.488513	759473.120789	43.772890
3501.459477	759444.260361	43.777895
3501.512057	759432.952276	43.782900
3501.331522	759429.478815	43.787905
3501.644454	759411.466435	43.792909
3501.627396	759390.547980	43.797914
3501.210611	759385.633256	43.802919
3501.421269	759379.085217	43.807924
3501.046139	759364.541738	43.812929
3501.439160	759327.913624	43.817933
3501.335649	759328.078780	43.822938
3501.329708	759330.102853	43.827943
3501.528758	759313.095922	43.832948
3501.411569	759293.871417	43.837953
3501.523629	759282.454593	43.842957
3501.498968	759279.251364	43.847962
3501.327938	759256.482931	43.852967
3501.792045	759247.820465	43.857972
3501.493275	759238.247835	43.862977
3501.383796	759205.057540	43.867981
3501.365861	759202.099887	43.872986
3501.660784	759192.133028	43.877991
3501.281963	759177.639145	43.882996
3501.431412	759157.185972	43.888001
3501.349899	759152.067658	43.893005
3501.113214	759144.310389	43.898010
3501.173636	759139.711400	43.903015
3501.204288	759117.600043	43.908020
3501.220109	759112.416274	43.913025
3501.319526	759100.261096	43.918029
3501.116142	759105.969358	43.923034
3501.567932	759097.703514	43.928039
3501.855484	759066.618169	43.933044
3501.057162	759051.453193	43.938049
3501.212517	759054.338894	43.943053
3500.931535	759056.951283	43.948058
3500.701890	759049.291443	43.953063
3501.107099	759051.593062	43.958068
3501.197289	759028.632743	43.963073
3501.160328	759006.236164	43.968077
3501.261489	759011.005956	43.973082
3501.464294	759013.094309	43.978087
3501.433154	759000.467094	43.983092
3501.034297	758983.064776	43.988097
3501.299806	758965.157868	43.993101
3501.105897	758968.249354	43.998106
3500.892779	758957.724651	44.003111
3501.344713	758950.544227	44.008116
3501.229465	758949.576381	44.013121
3501.384483	758939.928385	44.018125
3500.936733	758934.969136	44.023130
3501.185904	758920.617714	44.028135
3501.282063	758919.269508	44.033140
3500.957711	758918.780325	44.038145
3501.378983	758894.136477	44.043149
3501.173569	758884.005165	44.048154
3501.025751	758875.640783	44.053159
3501.184373	758877.489743	44.058164
3501.150506	758878.778360	44.063169
3501.416537	758861.710005	44.068173
3501.004300	758850.231133	44.073178
3501.146541	758842.657668	44.078183
3501.193850	758830.856095	44.083188
3501.237560	758827.443992	44.088193
3501.273996	758823.638319	44.093197
3501.100097	758800.326179	44.098202
3501.265517	758780.461513	44.103207
3501.506769	758780.717748	44.108212
3501.206884	758778.053256	44.113217
3501.400488	758776.146109	44.118221
3500.929148	758761.271942	44.123226
3501.234717	758745.282424	44.128231
3501.051771	758736.331529	44.133236
3501.067940	758741.707699	44.138241
3501.388816	758735.140894	44.143245
3500.943009	758721.693493	44.148250
3500.943984	758709.652654	44.153255
3501.341221	758696.312631	44.158260
3500.978942	758701.109854	44.163265
3501.113455	758689.589735	44.168269
3501.246204	758696.723176	44.173274
3501.440081	758686.574965	44.178279
3501.399416	758658.700419	44.183284
3500.961533	758663.904939	44.188289
3501.236666	758656.852151	44.193293
3501.347073	758650.221358	44.198298
3501.215831	758641.853978	44.203303
3501.367858	758620.757418	44.208308
3501.018428	758616.521927	44.213313
3501.440241	758621.387021	44.218317
3500.995214	758610.998854	44.223322
3501.283746	758596.689665	44.228327
3501.551695	758579.324274	44.233332
3501.064720	758573.137567	44.238337
3501.051845	758575.557770	44.243341
3501.081008	758571.358388	44.248346
3500.991399	758564.809921	44.253351
3501.158446	758548.349400	44.258356
3500.943185	758526.721094	44.263361
3500.852557	758510.303070	44.268365
3501.095381	758519.589820	44.273370
3500.929730	758512.807132	44.278375
3501.365691	758509.280719	44.283380
3501.001354	758518.174319	44.288385
3501.172034	758508.276446	44.293389
3501.294563	758495.672348	44.298394
3500.920637	758474.415552	44.303399
3501.395412	758470.784010	44.308404
3501.295894	758478.597572	44.313409
3501.101571	758469.598893	44.318413
3501.183645	758459.912994	44.323418
3501.058834	758450.606713	44.328423
3501.219610	758431.580835	44.333428
3501.029734	758427.911059	44.338433
3501.128019	758433.125831	44.343437
3500.949809	758424.173785	44.348442
3501.265581	758423.381390	44.353447
3501.084144	758395.183697	44.358452
3500.914410	758396.544195	44.363457
3501.437616	758388.019039	44.368461
3501.537025	758388.594824	44.373466
3501.056015	758376.633105	44.378471
3501.426979	758351.897118	44.383476
3501.384225	758343.169340	44.388481
3501.308025	758333.262687	44.393485
3501.315611	758332.077065	44.398490
3501.111815	758321.451237	44.403495
3501.248673	758304.748430	44.408500
3501.258818	758298.380648	44.413505
3501.188899	758294.937734	44.418509
3501.114045	758288.534640	44.423514
3501.139725	758285.372024	44.428519
3501.275212	758259.983753	44.433524
3500.865049	758260.693104	44.438529
3500.970608	758243.797935	44.443533
3500.823025	758258.232587	44.448538
3500.809581	758251.079063	44.453543
3500.872233	758246.035014	44.458548
3500.789004	758254.931817	44.463553
3501.028179	758238.113255	44.468557
3500.817346	758251.522017	44.473562
3501.016729	758242.161908	44.478567
3501.409616	758245.847620	44.483572
3501.127939	758227.338498	44.488577
3501.207346	758219.083893	44.493581
3501.308315	758227.407435	44.498586
3500.965539	758215.373266	44.503591
3501.207988	758220.663063	44.508596
3500.950305	758203.630428	44.513601
3500.982180	758182.601859	44.518605
3501.185042	758176.448882	44.523610
3501.056317	758174.051994	44.528615
3501.271505	758171.400871	44.533620
3501.025355	758170.158452	44.538625
3500.939656	758159.315479	44.543629
3500.896464	758164.948621	44.548634
3500.964157	758149.984178	44.553639
3500.840589	758136.186381	44.558644
3500.959878	758133.057584	44.563649
3501.133030	758131.153657	44.568653
3501.022115	758131.122656	44.573658
3500.725992	758131.566419	44.578663
3501.211816	758126.847171	44.583668
3501.030684	758126.235562	44.588673
3500.935140	758120.526659	44.593677
3500.965035	758127.282824	44.598682
3501.055368	758102.148243	44.603687
3501.083789	758084.722605	44.608692
3500.706581	758091.595426	44.613697
3501.244573	758081.537600	44.618701
3501.167623	758087.768592	44.623706
3501.021542	758080.686176	44.628711
3501.306692	758078.023460	44.633716
3500.931715	758076.950367	44.638721
3501.190569	758050.208526	44.643725
3500.906340	758054.154279	44.648730
3501.060783	758043.419513	44.653735
3501.100924	758046.719450	44.658740
3501.039733	758043.423034	44.663745
3501.112073	758038.377248	44.668749
3501.386509	758032.705843	44.673754
3500.963807	758007.408970	44.678759
3501.110256	758009.112101	44.683764
3501.096846	758003.537593	44.688769
3501.298409	757995.114504	44.693773
3501.143551	758000.025943	44.698778
3500.799591	757982.612255	44.703783
3501.234813	757961.615127	44.708788
3501.002544	757951.733768	44.713793
3501.462778	757947.956329	44.718797
3501.386471	757958.431601	44.723802
3501.014908	757953.163000	44.728807
3501.049478	757940.769927	44.733812
3500.965191	757931.703074	44.738817
3501.399625	757912.877440	44.743821
3501.227613	757911.820135	44.748826
3501.274037	757917.339946	44.753831
3501.424455	757914.008505	44.758836
3501.328573	757894.135355	44.763841
3501.218506	757885.319470	44.768845
3501.130308	757873.045279	44.773850
3501.029870	757874.098302	44.778855
3501.334382	757871.777784	44.783860
3500.886129	757848.014533	44.788865
3501.175875	757825.017606	44.793869
3501.187339	757828.717201	44.798874
3501.204597	757824.618080	44.803879
3501.287058	757824.456416	44.808884
3501.156487	757830.400362	44.813889
3501.062723	757799.817034	44.818893
3501.295130	757793.905633	44.823898
3500.881671	757783.955290	44.828903
3501.332094	757781.018395	44.833908
3500.822785	757782.583175	44.838913
3501.078670	757777.951064	44.843917
3501.069238	757778.742296	44.848922
3500.803606	757755.491462	44.853927
3501.089011	757738.417393	44.858932
3501.181158	757736.625462	44.863937
3501.148327	757737.321858	44.868941
3501.146023	757743.294028	44.873946
3501.010721	757739.121365	44.878951
3501.027405	757728.063445	44.883956
3501.330152	757721.893597	44.888961
3501.203940	757696.447987	44.893965
3501.330191	757704.619862	44.898970
3501.248946	757690.616849	44.903975
3501.290226	757683.058917	44.908980
3500.997543	757669.485635	44.913985
3501.118243	757653.129547	44.918989
3500.864093	757647.051665	44.923994
3501.146973	757645.869798	44.928999
3500.956253	757645.111670	44.934004
3500.849657	757653.864973	44.939009
3500.926692	757648.225905	44.944013
3501.107594	757646.320578	44.949018
3500.805397	757636.401009	44.954023
3500.927836	757607.952765	44.959028
3500.933294	757613.578275	44.964033
3501.101103	757594.006246	44.969037
3500.873708	757601.200230	44.974042
3500.818508	757608.069627	44.979047
3501.019900	757599.251295	44.984052
3500.902020	757601.294325	44.989057
3501.225476	757600.599289	44.994061
3501.129332	757603.625814	44.999066
3500.887415	757600.211008	45.004071
3501.585750	757575.171634	45.009076
3500.705633	757567.519075	45.014081
3500.978592	757567.671409	45.019085
3500.907087	757570.545812	45.024090
3500.743384	757567.660965	45.029095
3500.924154	757564.324358	45.034100
3500.742839	757571.165273	45.039105
3501.215557	757558.254983	45.044109
3501.206063	757562.402362	45.049114
3500.704968	757556.414570	45.054119
3500.897658	757539.256667	45.059124
3500.635334	757541.323582	45.064129
3501.277990	757545.856750	45.069133
3501.131726	757538.724504	45.074138
3500.811198	757527.228470	45.079143
3501.413428	757538.875416	45.084148
3501.007519	757539.337352	45.089153
3501.166633	757537.830437	45.094157
3501.349530	757500.290518	45.099162
3501.120577	757492.234147	45.104167
3501.238447	757485.058203	45.109172
3501.146594	757494.302803	45.114177
3501.085320	757501.568140	45.119181
3500.955485	757488.461174	45.124186
3501.096831	757471.805155	45.129191
3501.384975	757444.710865	45.134196
3500.791282	757446.289654	45.139201
3500.733688	757444.719822	45.144205
3500.666558	757454.009741	45.149210
3501.137121	757446.972900	45.154215
3501.110076	757455.861350	45.159220
3501.168526	757457.184306	45.164225
3501.048750	757437.313912	45.169229
3501.032305	757419.055124	45.174234
3501.154452	757409.311913	45.179239
3501.104053	757408.579929	45.184244
3501.173201	757409.999836	45.189249
3501.180436	757402.496608	45.194253
3500.949943	757418.624642	45.199258
3500.892535	757396.226701	45.204263
3501.318287	757376.858270	45.209268
3500.680426	757370.350016	45.214273
3500.815320	757361.838534	45.219277
3500.972224	757361.072289	45.224282
3500.710096	757364.471828	45.229287
3501.017192	757372.910312	45.234292
3500.608465	757373.076587	45.239297
3500.767057	757363.228583	45.244301
3500.958762	757378.546595	45.249306
3500.927642	757373.714889	45.254311
3500.788878	757370.875203	45.259316
3500.997778	757377.750520	45.264321
3501.030909	757368.515525	45.269325
3501.183318	757341.295231	45.274330
3500.806483	757324.773876	45.279335
3500.910584	757327.372570	45.284340
3501.009929	757322.173780	45.289345
3501.145807	757311.194271	45.294349
3500.671620	757320.206125	45.299354
3500.716842	757323.308112	45.304359
3501.098336	757325.663544	45.309364
3500.917577	757325.792148	45.314369
3501.050555	757326.707962	45.319373
3500.763964	757337.169480	45.324378
3500.754088	757327.546694	45.329383
3500.724395	757310.770519	45.334388
3501.017503	757318.224250	45.339393
3501.089416	757292.300343	45.344397
3501.344384	757284.163784	45.349402
3500.976488	757287.037915	45.354407
3501.337859	757279.772184	45.359412
3501.135965	757290.071701	45.364417
3501.421264	757269.245515	45.369421
3501.036503	757251.688825	45.374426
3501.098168	757235.094813	45.379431
3501.202596	757238.828689	45.384436
3501.237754	757236.305708	45.389441
3501.411075	757233.167614	45.394445
3501.598515	757206.681402	45.399450
3501.201878	757193.420589	45.404455
3501.210565	757189.914828	45.409460
3501.107945	757203.406262	45.414465
3501.194417	757176.294989	45.419469
3501.258881	757152.198050	45.424474
3500.816437	757153.554474	45.429479
3501.355842	757141.027321	45.434484
3501.022476	757156.481905	45.439489
3501.190823	757148.162087	45.444493
3501.137104	757139.089238	45.449498
3500.998777	757111.126449	45.454503
3501.501634	757108.970357	45.459508
3501.469898	757108.333975	45.464513
3501.174658	757110.702589	45.469517
3501.339791	757097.792995	45.474522
3500.812073	757078.334580	45.479527
3501.343037	757057.072359	45.484532
3501.394493	757057.902961	45.489537
3501.400843	757061.850562	45.494541
3501.448180	757049.355215	45.499546
3500.921537	757028.267682	45.504551
3501.043336	757015.463826	45.509556
3501.136698	757024.875821	45.514561
3501.365362	757012.893389	45.519565
3501.232150	757012.076335	45.524570
3500.714498	756993.998069	45.529575
3501.245844	756968.243932	45.534580
3501.046755	756977.556237	45.539585
3501.036923	756965.909293	45.544589
3500.997433	756967.890179	45.549594
3500.911731	756977.924123	45.554599
3501.231775	756977.180241	45.559604
3501.031549	756965.712834	45.564609
3501.091637	756942.701843	45.569613
3501.004938	756943.160419	45.574618
3500.688501	756940.794159	45.579623
3501.369286	756931.254177	45.584628
3500.748218	756944.634307	45.589633
3501.057553	756939.894142	45.594637
3500.899957	756947.323998	45.599642
3501.139545	756940.966526	45.604647
3501.193502	756917.462886	45.609652
3501.274190	756902.049617	45.614657
3500.937379	756897.613637	45.619661
3500.955336	756895.389540	45.624666
3500.972783	756890.352066	45.629671
3501.121099	756894.769884	45.634676
3500.893097	756900.928088	45.639681
3500.958737	756896.573678	45.644685
3500.967131	756875.249230	45.649690
3501.076565	756865.852941	45.654695
3501.143178	756853.502165	45.659700
3501.009116	756858.213463	45.664705
3501.216529	756848.751603	45.669709
3501.115809	756855.777275	45.674714
3500.885133	756853.594252	45.679719
3501.217444	756840.459161	45.684724
3500.870761	756823.586219	45.689729
3500.995649	756814.582189	45.694733
3501.275973	756814.338449	45.699738
3501.051986	756816.695378	45.704743
3501.392881	756811.752482	45.709748
3501.043099	756822.077067	45.714753
3501.103327	756792.007201	45.719757
3501.041737	756776.271673	45.724762
3500.749155	756773.309102	45.729767
3501.184392	756764.352446	45.734772
3500.779982	756770.046309	45.739777
3501.047310	756768.620082	45.744781
3501.227494	756766.171700	45.749786
3501.246264	756770.216120	45.754791
3500.939205	756736.356668	45.759796
3500.998495	756728.251855	45.764801
3500.979398	756730.969832	45.769805
3501.064072	756734.954020	45.774810
3500.740694	756703.318316	45.779815
3501.059500	756651.289220	45.784820
3500.735623	756531.050263	45.789825
3500.799416	756353.386420	45.794829
3500.282103	756132.275676	45.799834
3499.887104	755847.160640	45.804839
3500.368340	755518.693459	45.809844
3499.944387	755116.997703	45.814849
3499.789471	754677.169754	45.819853
3499.543494	754163.662187	45.824858
3499.203953	753603.422272	45.829863
3499.417477	752974.850901	45.834868
3498.975068	752306.974132	45.839873
3498.302982	751571.952471	45.844877
3498.110756	750770.588168	45.849882
3497.690513	749919.132795	45.854887
3497.188250	749000.203162	45.859892
3496.593030	748048.961340	45.864897
3495.964940	747024.266754	45.869901
3495.401726	745943.028773	45.874906
3494.952805	744812.878768	45.879911
3494.414996	743607.080668	45.884916
3493.739912	742366.999134	45.889921
3493.029837	741048.533250	45.894925
3492.534009	739682.323125	45.899930
3491.256543	738250.846191	45.904935
3490.733198	736755.496820	45.909940
3489.871708	735213.595831	45.914945
3488.950917	733600.813599	45.919949
3488.575988	731942.608570	45.924954
3487.491269	730215.983390	45.929959
3486.519839	728440.673872	45.934964
3485.442583	726608.907045	45.939969
3484.490184	724706.038169	45.944973
3483.588511	722760.585484	45.949978
3482.395074	720760.975236	45.954983
3481.248561	718689.012270	45.959988
3480.185325	716580.258183	45.964993
3479.139764	714410.533507	45.969997
3478.213382	712176.352728	45.975002
3476.877549	709898.458613	45.980007
3475.752317	707540.514313	45.985012
3474.126480	705154.088230	45.990017
3472.916902	702702.040783	45.995021
3471.776118	700194.070355	46.000026
3470.327363	697637.355099	46.005031
3469.199026	695022.304429	46.010036
3467.744733	692375.344836	46.015041
3466.229925	689659.436225	46.020045
3464.410484	686884.567504	46.025050
3463.032414	684070.534306	46.030055
3461.718270	681198.840562	46.035060
3460.274413	678280.581886	46.040065
3458.631266	675308.406414	46.045069
3457.125572	672284.856888	46.050074
3455.494621	669202.803385	46.055079
3453.833312	666074.603906	46.060084
3451.919309	662894.569480	46.065089
3450.091648	659671.188562	46.070093
3448.421157	656396.875214	46.075098
3446.677933	653080.668459	46.080103
3445.076526	649710.707655	46.085108
3443.090034	646294.984728	46.090113
3441.186049	642826.086219	46.095117
3439.195013	639310.950942	46.100122
3437.468813	635742.579962	46.105127
3435.360214	632130.148849	46.110132
3433.175944	628487.996379	46.115137
3431.251425	624784.341417	46.120141
3429.523015	621045.853713	46.125146
3427.315621	617252.973515	46.130151
3425.270697	613411.721277	46.135156
3423.076189	609539.369934	46.140161
3420.851560	605610.191680	46.145165
3418.887325	601632.679949	46.150170
3416.318517	597613.774103	46.155175
3414.283032	593541.255518	46.160180
3411.911320	589447.289992	46.165185
3409.624411	585309.084261	46.170189
3407.546827	581131.318373	46.175194
3405.107372	576901.289824	46.180199
3403.067209	572623.217587	46.185204
3400.147503	568321.999865	46.190209
3397.585084	563960.169986	46.195213
3395.365950	559577.633926	46.200218
3392.807348	555151.178252	46.205223
3390.451229	550675.804008	46.210228
3387.756299	546186.667590	46.215233
3385.134359	541648.256107	46.220237
3382.756786	537067.480556	46.225242
3379.966158	532451.953981	46.230247
3377.440050	527786.816225	46.235252
3374.718725	523107.017793	46.240257
3372.187836	518373.410274	46.245261
3369.776341	513596.897893	46.250266
3366.560659	508818.109130	46.255271
3364.144286	503962.229405	46.260276
3361.160008	499102.374759	46.265281
3358.501485	494197.446299	46.270285
3355.215458	489262.521334	46.275290
3352.567996	484304.280036	46.280295
3349.956043	479300.809092	46.285300
3346.994524	474254.091492	46.290305
3343.782670	469189.792928	46.295309
3340.993204	464092.011498	46.300314
3337.860392	458980.699644	46.305319
3335.188766	453814.023079	46.310324
3331.783842	448632.082327	46.315329
3328.832019	443431.915511	46.320333
3325.635379	438189.459902	46.325338
3322.430110	432938.937280	46.330343
3319.345345	427639.293909	46.335348
3315.915485	422333.333795	46.340353
3313.156091	416995.227787	46.345357
3310.265422	411638.611253	46.350362
3306.607713	406247.411077	46.355367
3303.374603	400839.867545	46.360372
3299.837447	395400.046779	46.365377
3296.600441	389940.730753	46.370381
3293.610496	384471.541263	46.375386
3289.899155	378974.979567	46.380391
3286.710007	373456.614168	46.385396
3283.198707	367929.916459	46.390401
3279.552049	362372.511002	46.395405
3276.543048	356802.563750	46.400410
3272.946512	351225.148767	46.405415
3269.768068	345609.478780	46.410420
3265.793721	339981.079043	46.415425
3262.215229	334349.259501	46.420429
3258.855448	328687.824836	46.425434
3255.188132	323024.873173	46.430439
3251.530377	317344.281629	46.435444
3247.684882	311653.430185	46.440449
3244.050229	305962.276563	46.445453
3240.551631	300243.938530	46.450458
3236.562208	294529.397716	46.455463
3232.714493	288795.880643	46.460468
3228.670044	283068.418395	46.465473
3224.768250	277337.120232	46.470477
3221.129494	271592.537936	46.475482
3217.382258	265858.642031	46.480487
3213.805805	260113.020794	46.485492
3209.628129	254348.334923	46.490497
3205.744723	248591.937716	46.495501
3201.790665	242833.825300	46.500506
3197.680863	237086.078856	46.505511
3193.709983	231322.872785	46.510516
3189.650167	225558.375255	46.515521
3185.471047	219789.862787	46.520525
3181.853230	214040.619134	46.525530
3177.237713	208244.964698	46.530535
3173.334857	202446.245815	46.535540
3169.103153	196718.430193	46.540545
3164.846761	190967.430650	46.545549
3161.102804	185239.711264	46.550554
3156.436737	179521.971630	46.555559
3152.302342	173811.507697	46.560564
3147.987082	168106.228952	46.565569
3143.546360	162414.654160	46.570573
3139.243301	156734.477992	46.575578
3134.616422	151072.289835	46.580583
3130.515246	145421.692729	46.585588
3125.619188	139787.876756	46.590593
3121.249284	134171.752794	46.595597
3117.000447	128564.502047	46.600602
3112.179796	122983.252806	46.605607
3107.459869	117430.209538	46.610612
3102.514701	111887.900719	46.615617
3098.054688	106366.936803	46.620621
3093.336607	100876.724736	46.625626
3087.966811	95418.049969	46.630631
3083.347687	89982.788984	46.635636
3078.128937	84590.962431	46.640641
3073.347530	79228.171019	46.645645
3068.404445	73894.830454	46.650650
3063.109109	68593.702613	46.655655
3058.032822	63322.932724	46.660660
3052.559962	58106.142403	46.665665
3047.017939	52935.532253	46.670669
3041.384973	47803.699570	46.675674
3035.804084	42723.596105	46.680679
3029.775282	37706.286827	46.685684
3023.432509	32732.610232	46.690689
3016.911152	27841.374706	46.695693
3010.019817	23031.198329	46.700698
3000.094913	18360.689055	46.705703
2979.680387	14084.366432	46.710708
2948.918898	10317.178018	46.715713
2916.641196	6931.327475	46.720717
2886.979003	3989.340771	46.725722
2859.417263	1529.220231	46.730727
2808.367342	270.546967	46.735732
2739.445645	267.266966	46.740737
2707.726133	255.745375	46.745741
2709.416533	246.034392	46.750746
2729.011994	249.897869	46.755751
2753.359402	247.717783	46.760756
2773.135278	250.955047	46.765761
2784.591220	247.370079	46.770765
2788.115958	234.416356	46.775770
2786.116396	237.247612	46.780775
2781.808180	234.230633	46.785780
2776.721164	239.240035	46.790785
2772.236855	243.771189	46.795789
2769.163417	239.821663	46.800794
2766.385593	237.930387	46.805799
2763.907736	232.207674	46.810804
2761.173964	222.422500	46.815809
2758.379306	245.240935	46.820813
2756.024836	232.736210	46.825818
2753.140711	234.309639	46.830823
2750.450322	228.047271	46.835828
2747.306647	224.124587	46.840833
2743.701913	225.684887	46.845837
2740.758241	223.313726	46.850842
2736.965394	237.991438	46.855847
2733.769352	223.840723	46.860852
2731.384689	215.833226	46.865857
2727.974099	215.131288	46.870861
2724.813074	225.670633	46.875866
2721.303089	232.059715	46.880871
2718.068865	218.169905	46.885876
2714.723529	222.879426	46.890881
2711.628556	218.878260	46.895885
2708.664991	208.692490	46.900890
2704.904015	208.533233	46.905895
2701.625549	210.434824	46.910900
2698.025702	216.519896	46.915905
2695.022228	219.669126	46.920909
2691.616565	205.695644	46.925914
2688.134161	214.960124	46.930919
2684.648110	212.518354	46.935924
2681.256256	217.586267	46.940929
2677.846695	221.314824	46.945933
2674.740454	210.931680	46.950938
2671.086645	210.643413	46.955943
2668.298032	208.661836	46.960948
2664.896051	206.361471	46.965953
2660.466198	209.247391	46.970957
2657.408336	208.181639	46.975962
2654.198607	205.321185	46.980967
2651.228628	206.305236	46.985972
2647.545606	212.269728	46.990977
2643.976728	207.973708	46.995981
2640.776141	202.537287	47.000986
2636.742743	204.212645	47.005991
2633.701696	201.570559	47.010996
2630.454289	201.925067	47.016001
2627.070768	204.751068	47.021005
2623.648290	206.303592	47.026010
2619.944183	209.009017	47.031015
2616.043126	200.674845	47.036020
2612.638739	203.210872	47.041025
2609.234419	202.337690	47.046029
2606.014677	202.293948	47.051034
2602.957583	208.450064	47.056039
2599.798676	206.810254	47.061044
2595.888812	202.419375	47.066049
2592.260679	193.231950	47.071053
2589.111293	189.175168	47.076058
2584.791973	192.000237	47.081063
2581.674292	189.306350	47.086068
2578.749842	184.635126	47.091073
2575.109803	191.886886	47.096077
2571.921252	191.765584	47.101082
2568.261886	194.185397	47.106087
2564.878751	193.591923	47.111092
2561.253582	187.864150	47.116097
2557.909678	190.011118	47.121101
2554.108702	179.521317	47.126106
2550.439554	190.897719	47.131111
2546.765030	188.434390	47.136116
2543.496932	185.357345	47.141121
2540.571348	183.875697	47.146125
2537.140593	192.994768	47.151130
2533.670257	184.986218	47.156135
2529.744670	189.112311	47.161140
2526.216162	191.450897	47.166145
2522.955740	187.482015	47.171149
2519.822089	180.526568	47.176154
2516.184442	192.035521	47.181159
2512.499251	171.235476	47.186164
2509.125578	181.861248	47.191169
2505.337584	189.491188	47.196173
2502.263981	177.961411	47.201178
2498.716862	182.343561	47.206183
2494.685270	180.652974	47.211188
2491.201185	185.692087	47.216193
2487.785971	189.499864	47.221197
2484.850184	180.002938	47.226202
2481.245047	194.325886	47.231207
2477.956459	181.924962	47.236212
2474.334232	176.721505	47.241217
2470.876257	183.218179	47.246221
2467.685465	173.370206	47.251226
2464.037289	174.420314	47.256231
2460.024187	176.381374	47.261236
2456.683436	173.255851	47.266241
2453.232416	176.666421	47.271245
2450.346656	168.101753	47.276250
2446.313992	184.701736	47.281255
2442.446329	174.811947	47.286260
2439.634057	171.898283	47.291265
2436.223838	168.556160	47.296269
2432.584414	165.567143	47.301274
2428.597435	169.569891	47.306279
2425.381149	167.261871	47.311284
2421.964394	171.913563	47.316289
2418.351386	168.582146	47.321293
2414.860009	162.528661	47.326298
2411.510627	168.573251	47.331303
2407.759861	158.616789	47.336308
2404.497007	166.645282	47.341313
2401.038888	171.439410	47.346317
2397.559364	167.606576	47.351322
2394.271094	161.332596	47.356327
2390.566638	174.961824	47.361332
2387.288261	163.789898	47.366337
2383.716656	174.303488	47.371341
2380.427769	158.704095	47.376346
2376.454547	162.109050	47.381351
2372.609413	167.097140	47.386356
2369.492097	159.880018	47.391361
2365.831083	171.047598	47.396365
2363.008762	165.267764	47.401370
2359.076291	166.425824	47.406375
2355.450863	165.738065	47.411380
2351.801384	165.180193	47.416385
2348.474042	165.660440	47.421389
2345.298825	163.365810	47.426394
2341.476061	166.677995	47.431399
2338.072369	163.852488	47.436404
2334.857311	166.259095	47.441409
2331.023438	170.238744	47.446413
2327.749025	168.397460	47.451418
2324.227539	168.960201	47.456423
2320.660206	168.044991	47.461428
2317.359509	171.833533	47.466433
2313.398689	175.383311	47.471437
2310.359384	159.814477	47.476442
2306.378235	162.793379	47.481447
2303.004768	160.568126	47.486452
2300.014221	162.137374	47.491457
2296.222980	163.102392	47.496461
2292.502979	160.492117	47.501466
2289.258358	172.199964	47.506471
2285.797343	160.125969	47.511476
2282.129750	169.192480	47.516481
2278.614709	170.090058	47.521485
2275.393788	161.489678	47.526490
2271.612694	162.529998	47.531495
2268.353762	165.265776	47.536500
2264.642505	153.730543	47.541505
2261.394805	167.750509	47.546509
2257.924819	151.638564	47.551514
2253.871841	163.518608	47.556519
2250.883943	158.478865	47.561524
2246.987797	159.303237	47.566529
2243.345978	160.576062	47.571533
2240.409971	159.051365	47.576538
2236.938881	153.834149	47.581543
2233.518680	153.953154	47.586548
2229.588087	159.862675	47.591553
2225.958557	167.250107	47.596557
2222.863289	154.766701	47.601562
2219.050903	163.386399	47.606567
2215.755317	156.340031	47.611572
2212.628028	159.555672	47.616577
2208.695842	157.101590	47.621581
2205.227822	162.394202	47.626586
2201.887527	152.526246	47.631591
2198.374361	162.142273	47.636596
2194.626406	156.209044	47.641601
2190.827377	166.372089	47.646605
2187.964551	158.310197	47.651610
2184.416050	161.332783	47.656615
2180.725854	152.753199	47.661620
2177.120681	148.333584	47.666625
2173.731066	161.613420	47.671629
2170.580179	156.790973	47.676634
2166.558652	162.012901	47.681639
2163.291559	149.134338	47.686644
2160.099668	155.139204	47.691649
2156.405675	149.821644	47.696653
2153.117585	155.614726	47.701658
2148.997816	155.119552	47.706663
2145.974081	160.484832	47.711668
2142.837595	156.798452	47.716673
2138.471710	167.589045	47.721677
2135.497475	152.394993	47.726682
2131.747782	157.463975	47.731687
2128.063897	151.580780	47.736692
2124.910162	155.428787	47.741697
2120.820805	154.357118	47.746701
2118.072853	147.247344	47.751706
2114.259249	159.571514	47.756711
2110.692583	160.365501	47.761716
2106.879776	157.035107	47.766721
2103.537892	163.538867	47.771725
2100.479843	146.512464	47.776730
2097.364436	160.410165	47.781735
2093.383341	152.772597	47.786740
2089.514982	138.011690	47.791745
2085.840016	150.362043	47.796749
2082.973675	142.627611	47.801754
2079.212026	158.873532	47.806759
2075.482167	147.648238	47.811764
2072.227878	154.211110	47.816769
2068.741700	147.898770	47.821773
2065.365095	151.114185	47.826778
2061.865014	155.038566	47.831783
2058.417924	145.460171	47.836788
2054.762441	149.762351	47.841793
2051.123103	155.569109	47.846797
2048.046604	150.739372	47.851802
2044.503855	157.793473	47.856807
2040.907619	161.862073	47.861812
2037.404730	154.809755	47.866817
2033.701340	154.882705	47.871821
2029.898931	143.566276	47.876826
2026.496459	153.216379	47.881831
2023.027239	150.400027	47.886836
2019.914687	153.134628	47.891841
2016.280816	152.522173	47.896845
2013.186556	146.475481	47.901850
2009.258188	154.588470	47.906855
2005.511416	153.081268	47.911860
2002.323288	150.214016	47.916865
1998.718864	151.625305	47.921869
1995.607406	148.911116	47.926874
1991.858406	145.874948	47.931879
1988.448124	142.108164	47.936884
1984.831941	148.639699	47.941889
1981.158499	157.308200	47.946893
1977.593928	146.686894	47.951898
1974.092455	157.539625	47.956903
1970.817128	149.355439	47.961908
1967.353408	153.602631	47.966913
1963.642972	150.649688	47.971917
1960.297530	147.266261	47.976922
1956.538694	148.777373	47.981927
1953.281776	144.878842	47.986932
1950.123578	133.415099	47.991937
1946.228892	156.852345	47.996941
1943.040955	138.164944	48.001946
1939.370489	140.975876	48.006951
1935.756925	140.434130	48.011956
1932.200999	142.921007	48.016961
1928.619778	146.900775	48.021965
1925.345938	147.442152	48.026970
1921.636502	152.254223	48.031975
1918.216699	158.250461	48.036980
1914.896297	147.706561	48.041985
1911.179966	158.207577	48.046989
1908.011734	142.411059	48.051994
1904.190953	146.189997	48.056999
1900.405376	145.176150	48.062004
1897.411542	141.204664	48.067009
1893.650679	149.161329	48.072013
1890.418875	134.880446	48.077018
1886.540458	151.357594	48.082023
1882.873268	152.460098	48.087028
1879.797734	141.811914	48.092033
1876.182774	150.578548	48.097037
1873.056848	139.858605	48.102042
1868.998657	146.286479	48.107047
1865.968139	153.813100	48.112052
1862.659167	141.912061	48.117057
1858.524259	142.144699	48.122061
1854.951621	144.747286	48.127066
1851.581403	146.579480	48.132071
1847.513619	144.366087	48.137076
1844.424451	138.797625	48.142081
1841.331650	148.771274	48.147085
1837.901103	141.367546	48.152090
1834.484211	141.446867	48.157095
1830.846236	133.811916	48.162100
1827.475700	142.527220	48.167105
1823.818948	145.420834	48.172109
1820.251339	144.016719	48.177114
1816.425403	139.097082	48.182119
1813.094760	128.999781	48.187124
1809.754625	144.339717	48.192129
1805.996389	148.806746	48.197133
1802.905839	135.324433	48.202138
1798.898995	140.393103	48.207143
1795.521728	139.331805	48.212148
1792.416849	143.155969	48.217153
1788.808604	141.037360	48.222157
1785.450233	128.956532	48.227162
1781.650263	138.673679	48.232167
1778.031593	137.606234	48.237172
1774.598713	132.955972	48.242177
1770.984795	147.143102	48.247181
1767.846944	132.707052	48.252186
1764.258752	141.114920	48.257191
1760.450942	134.939261	48.262196
1757.260271	131.234949	48.267201
1753.648379	146.783759	48.272205
1749.960829	133.051569	48.277210
1746.627082	138.095144	48.282215
1743.089915	135.654191	48.287220
1739.880872	137.410226	48.292225
1736.124731	139.891977	48.297229
1732.825739	138.462950	48.302234
1729.309322	144.064495	48.307239
1725.712245	140.345483	48.312244
1722.213602	140.897056	48.317249
1718.442286	143.687011	48.322253
1714.947141	133.311988	48.327258
1711.713871	135.275908	48.332263
1707.687491	129.383008	48.337268
1704.668319	134.636330	48.342273
1700.735935	138.883676	48.347277
1697.683970	147.602705	48.352282
1694.013282	145.900451	48.357287
1690.643413	144.130176	48.362292
1687.456937	130.623422	48.367297
1683.624549	146.021171	48.372301
1680.276343	139.508127	48.377306
1676.450154	142.039630	48.382311
1672.864977	141.699826	48.387316
1669.852412	138.348097	48.392321
1666.161387	142.105540	48.397325
1662.536957	128.587352	48.402330
1658.819296	144.985134	48.407335
1655.475670	136.419864	48.412340
1652.299622	125.856241	48.417345
1648.424186	141.494793	48.422349
1645.084010	136.049215	48.427354
1641.381961	139.000028	48.432359
1638.234717	144.755536	48.437364
1634.645466	135.879359	48.442369
1630.684673	145.507068	48.447373
1627.582241	135.101160	48.452378
1624.123223	137.760489	48.457383
1620.721686	139.014742	48.462388
1617.328534	137.967083	48.467393
1613.369198	137.992867	48.472397
1610.081490	135.593554	48.477402
1606.821868	139.919874	48.482407
1603.022698	134.310476	48.487412
1599.496297	132.708906	48.492417
1595.570857	133.416008	48.497421
1592.370178	134.003539	48.502426
1589.335175	127.247634	48.507431
1585.652665	130.345427	48.512436
1582.127525	127.109738	48.517441
1578.617616	131.410087	48.522445
1575.013754	126.920374	48.527450
1571.222844	133.641647	48.532455
1568.160112	129.759793	48.537460
1564.577727	133.693092	48.542465
1560.719825	137.940454	48.547469
1557.653923	130.359709	48.552474
1553.794251	137.111146	48.557479
1550.407456	136.157014	48.562484
1546.710940	122.571578	48.567489
1543.579862	138.135528	48.572493
1540.308658	133.672975	48.577498
1536.643991	132.586540	48.582503
1533.022485	136.392562	48.587508
1529.401067	134.220926	48.592513
1525.757994	145.979943	48.597517
1522.729588	126.673333	48.602522
1519.195839	136.104622	48.607527
1515.286878	132.933033	48.612532
1511.576309	126.453595	48.617537
1508.349979	125.613986	48.622541
1505.004239	125.231275	48.627546
1501.617536	131.328309	48.632551
1497.721746	135.655814	48.637556
1494.575049	122.352221	48.642561
1490.718044	135.246080	48.647565
1487.492436	133.562567	48.652570
1483.329581	139.288874	48.657575
1480.484898	136.917832	48.662580
1476.886316	130.960946	48.667585
1473.345852	140.915731	48.672589
1470.083439	131.918426	48.677594
1466.464781	142.782278	48.682599
1462.959579	136.625805	48.687604
1459.360441	130.116691	48.692609
1455.652736	128.299638	48.697613
1452.290955	120.333921	48.702618
1449.007406	132.844408	48.707623
1445.214402	131.494984	48.712628
1442.270773	126.896892	48.717633
1438.443717	130.708272	48.722637
1435.303784	123.864720	48.727642
1431.126862	133.525878	48.732647
1427.805551	130.813601	48.737652
1424.501766	129.949806	48.742657
1420.678441	135.280450	48.747661
1417.417347	127.917297	48.752666
1413.887372	127.141936	48.757671
1410.148355	132.301529	48.762676
1406.484709	123.019577	48.767681
1403.134807	133.524154	48.772685
1399.948643	118.783701	48.777690
1396.546532	123.580574	48.782695
1392.755522	124.602428	48.787700
1389.741145	127.678582	48.792705
1385.839526	131.671492	48.797709
1382.530426	118.732383	48.802714
1378.783296	129.381790	48.807719
1375.450679	130.887272	48.812724
1371.784720	124.585084	48.817729
1368.074714	131.187542	48.822733
1365.140276	117.491499	48.827738
1361.353503	133.448669	48.832743
1357.816552	117.674197	48.837748
1354.448713	117.829461	48.842753
1350.574820	124.880027	48.847757
1347.121386	124.459467	48.852762
1343.783810	126.339745	48.857767
1340.272739	123.333024	48.862772
1337.029560	117.750873	48.867777
1333.405078	132.604296	48.872781
1329.915361	126.974240	48.877786
1326.547480	128.800556	48.882791
1322.525241	133.019155	48.887796
1319.261200	130.522236	48.892801
1315.717032	122.696220	48.897805
1312.386787	121.998329	48.902810
1308.755328	128.973991	48.907815
1305.086899	119.018453	48.912820
1302.147243	127.832181	48.917825
1298.421326	131.488979	48.922829
1294.601231	123.092876	48.927834
1291.298038	125.324075	48.932839
1287.685002	126.818128	48.937844
1284.154702	129.878313	48.942849
1280.613277	129.007490	48.947853
1277.390925	123.740628	48.952858
1273.420150	124.315460	48.957863
1270.319388	128.196549	48.962868
1267.066712	120.704464	48.967873
1263.201407	124.622596	48.972877
1259.475617	123.222738	48.977882
1256.258871	122.016680	48.982887
1252.313954	124.466844	48.987892
1249.476985	121.713055	48.992897
1245.324927	128.592598	48.997901
1242.050530	123.617180	49.002906
1239.048809	125.132806	49.007911
1235.592001	123.234285	49.012916
1232.076868	126.580895	49.017921
1228.090979	127.012844	49.022925
1224.554693	125.680643	49.027930
1221.446543	124.377271	49.032935
1217.488224	124.049660	49.037940
1214.036722	119.089442	49.042945
1210.241272	123.992173	49.047949
1207.023683	131.447060	49.052954
1204.051982	128.703421	49.057959
1200.271996	122.066504	49.062964
1196.751553	121.188922	49.067969
1193.079465	126.729508	49.072973
1189.658939	121.662940	49.077978
1186.713326	121.279436	49.082983
1182.491930	126.059867	49.087988
1179.176067	129.456935	49.092993
1175.480777	130.550140	49.097997
1172.385664	123.253605	49.103002
1168.622996	117.748516	49.108007
1164.827070	119.872917	49.113012
1161.516034	120.475748	49.118017
1158.024547	120.583813	49.123021
1154.628799	117.231743	49.128026
1151.058137	121.071101	49.133031
1147.660435	124.416060	49.138036
1144.262735	108.264708	49.143041
1140.662764	126.317118	49.148045
1137.370104	113.897868	49.153050
1133.508725	120.021259	49.158055
1130.199927	124.710318	49.163060
1126.897137	118.141317	49.168065
1122.955369	127.586940	49.173069
1119.528788	125.893273	49.178074
1115.939758	112.716521	49.183079
1112.392819	119.533678	49.188084
1109.126109	125.120148	49.193089
1105.669735	129.637762	49.198093
1101.969096	125.437278	49.203098
1098.567807	117.831282	49.208103
1095.006195	123.648438	49.213108
1091.731101	121.555913	49.218113
1087.891986	127.090562	49.223117
1084.555646	124.559272	49.228122
1080.819636	120.524913	49.233127
1077.418041	120.425932	49.238132
1073.844610	120.238843	49.243137
1070.470846	119.754594	49.248141
1067.366660	122.186597	49.253146
1063.709817	117.382545	49.258151
1059.749038	122.945498	49.263156
1056.758723	121.835432	49.268161
1052.921948	118.402915	49.273165
1049.400016	115.260333	49.278170
1046.118165	112.015362	49.283175
1042.462294	115.399894	49.288180
1039.284688	110.893842	49.293185
1035.774252	127.341956	49.298189
1032.118763	117.795208	49.303194
1028.363057	121.221973	49.308199
1024.912532	111.421395	49.313204
1021.499220	110.498570	49.318209
1017.979615	111.206977	49.323213
1014.399208	117.167820	49.328218
1010.816919	114.696356	49.333223
1007.324853	120.059427	49.338228
1004.339979	111.902929	49.343233
1000.635752	120.713690	49.348237
997.181294	116.097921	49.353242
993.827190	122.881599	49.358247
989.677259	121.710257	49.363252
986.489950	120.682863	49.368257
982.708125	125.857639	49.373261
979.599872	116.750166	49.378266
975.637039	118.037142	49.383271
972.171233	117.726713	49.388276
969.050825	117.694825	49.393281
965.679671	117.438944	49.398285
961.802789	119.403715	49.403290
958.380605	122.399671	49.408295
954.971559	118.263422	49.413300
951.795135	112.771967	49.418305
947.912019	123.687614	49.423309
944.866674	113.568665	49.428314
941.294144	116.116382	49.433319
936.963195	114.402087	49.438324
934.030857	105.946066	49.443329
930.387208	108.797253	49.448333
927.095943	118.069572	49.453338
923.118665	110.487123	49.458343
919.657836	111.434503	49.463348
916.815739	110.879710	49.468353
912.655443	116.959185	49.473357
909.454448	107.045087	49.478362
905.921402	120.953032	49.483367
902.225412	116.754544	49.488372
899.062160	99.979258	49.493377
895.240026	117.459153	49.498381
892.170180	106.248732	49.503386
888.359126	113.742167	49.508391
884.784462	114.864364	49.513396
881.348738	109.234466	49.518401
877.579555	115.862960	49.523405
874.678960	112.620768	49.528410
870.888559	114.096493	49.533415
867.126608	118.768232	49.538420
863.779437	108.730637	49.543425
859.825443	113.599228	49.548429
856.862047	109.117966	49.553434
853.737128	116.804987	49.558439
850.161212	118.336692	49.563444
846.606255	108.905868	49.568449
842.770612	105.946981	49.573453
839.559510	112.336254	49.578458
835.848061	110.613568	49.583463
832.133622	111.776381	49.588468
828.761331	105.234196	49.593473
825.171642	113.985837	49.598477
821.850864	110.711219	49.603482
818.503480	104.243054	49.608487
814.436014	115.733264	49.613492
811.302715	103.771750	49.618497
807.895342	109.644057	49.623501
804.406448	103.212420	49.628506
801.017522	114.998876	49.633511
797.613138	111.999821	49.638516
793.895510	107.054188	49.643521
789.802750	115.268959	49.648525
786.592918	111.280358	49.653530
783.188861	111.580460	49.658535
779.899295	111.914641	49.663540
776.501996	110.990167	49.668545
772.795522	108.100287	49.673549
769.284272	111.133093	49.678554
765.705739	109.169964	49.683559
762.078720	119.248800	49.688564
758.904400	105.819678	49.693569
755.304708	113.486922	49.698573
752.008582	106.777852	49.703578
748.401154	107.156147	49.708583
744.993927	114.840387	49.713588
741.556602	112.468843	49.718593
737.843213	111.097236	49.723597
733.977902	97.617696	49.728602
730.528644	108.532933	49.733607
726.686887	109.279697	49.738612
723.957381	105.534441	49.743617
720.017383	108.283472	49.748621
716.372851	114.144713	49.753626
713.415597	105.678810	49.758631
709.643248	106.128331	49.763636
706.104101	111.239784	49.768641
702.930858	115.841759	49.773645
699.419928	109.483540	49.778650
695.444531	121.543275	49.783655
691.925015	119.135497	49.788660
688.711574	113.598524	49.793665
684.739433	110.206430	49.798669
681.759500	121.228098	49.803674
678.433110	115.412902	49.808679
674.280186	112.729656	49.813684
671.091516	111.641780	49.818689
667.526569	115.399711	49.823693
663.992505	114.597699	49.828698
660.680579	111.248941	49.833703
657.264789	107.940323	49.838708
654.314116	110.098916	49.843713
650.437315	114.628115	49.848717
646.483337	104.750298	49.853722
643.220566	115.829212	49.858727
639.556319	113.824987	49.863732
636.048026	108.632626	49.868737
632.820701	116.104553	49.873741
629.319610	107.734748	49.878746
625.687398	101.993871	49.883751
621.482655	107.381480	49.888756
618.460074	104.619534	49.893761
615.168532	108.538915	49.898765
611.703769	115.478615	49.903770
608.248175	109.751641	49.908775
604.836604	106.910640	49.913780
601.507852	98.602629	49.918785
597.411421	112.716641	49.923789
594.008916	99.188236	49.928794
590.269532	109.361251	49.933799
586.715127	113.767515	49.938804
583.480278	111.148390	49.943809
580.223675	103.164275	49.948813
576.574551	115.817380	49.953818
573.294693	97.646724	49.958823
569.143444	108.119030	49.963828
566.169922	103.808609	49.968833
562.574072	110.624092	49.973837
559.268911	102.067313	49.978842
556.077574	107.290251	49.983847
551.939402	108.182320	49.988852
548.763945	103.315426	49.993857
544.902797	113.177977	49.998861
541.378436	109.174539	50.003866
538.028767	100.819347	50.008871
534.416015	106.609958	50.013876
531.006202	95.329259	50.018881
527.452983	111.480949	50.023885
524.101838	109.774907	50.028890
520.627028	110.713917	50.033895
516.908730	107.839284	50.038900
513.701692	98.042405	50.043905
510.111266	110.144729	50.048909
506.292738	106.832496	50.053914
503.024956	99.290164	50.058919
499.463612	114.708366	50.063924
496.205451	103.668119	50.068929
492.179843	110.272461	50.073933
489.088686	101.912269	50.078938
485.607378	103.374925	50.083943
481.931565	115.995838	50.088948
478.337053	103.300804	50.093953
474.949659	105.502466	50.098957
471.604591	98.226376	50.103962
468.268655	105.530185	50.108967
464.464453	103.843010	50.113972
460.872777	104.686243	50.118977
457.622579	110.049473	50.123981
454.146723	109.021717	50.128986
450.337153	108.905812	50.133991
446.700720	115.310784	50.138996
443.419890	105.115577	50.144001
439.795275	109.032215	50.149005
436.002480	103.339714	50.154010
432.979228	103.673769	50.159015
429.232905	103.448714	50.164020
426.096781	102.734947	50.169025
422.754101	109.767203	50.174029
418.949038	109.801737	50.179034
415.369455	107.845635	50.184039
411.677424	104.307463	50.189044
408.721514	98.252209	50.194049
405.236274	103.517375	50.199053
401.311134	103.463341	50.204058
397.888129	93.815718	50.209063
394.117880	108.144304	50.214068
391.063826	97.111307	50.219073
387.613808	100.723316	50.224077
383.699288	103.900612	50.229082
380.115601	100.333031	50.234087
376.778298	114.972147	50.239092
373.335023	104.009144	50.244097
370.155321	106.929613	50.249101
366.519141	108.345091	50.254106
363.163621	101.748082	50.259111
358.930362	103.669256	50.264116
355.923251	94.889516	50.269121
352.327762	114.085687	50.274125
348.840857	102.839684	50.279130
345.392854	105.334898	50.284135
342.122915	101.579864	50.289140
338.433313	100.125775	50.294145
334.647687	103.618947	50.299149
331.039852	99.363978	50.304154
327.859883	100.370413	50.309159
324.142764	110.708290	50.314164
321.027713	98.262732	50.319169
317.298108	101.534089	50.324173
314.047818	99.515489	50.329178
310.526351	94.521200	50.334183
306.718682	103.586546	50.339188
303.097838	104.918632	50.344193
300.082792	108.703543	50.349197
296.127925	103.991426	50.354202
292.709890	98.177621	50.359207
289.313663	100.017234	50.364212
285.795513	93.653337	50.369217
281.931331	106.089827	50.374221
278.702079	110.935083	50.379226
275.258611	99.448107	50.384231
271.453881	106.536335	50.389236
268.587921	100.035877	50.394241
265.075707	104.502907	50.399245
261.137481	101.061442	50.404250
257.726998	105.647735	50.409255
254.182898	104.764903	50.414260
250.917171	102.088655	50.419265
247.522718	102.828285	50.424269
244.048237	95.199189	50.429274
240.169340	102.935371	50.434279
236.781416	103.056083	50.439284
233.262488	97.927066	50.444289
229.289819	107.536909	50.449293
225.861602	103.223589	50.454298
222.682407	98.379320	50.459303
219.102379	103.208513	50.464308
216.025161	85.571518	50.469313
212.448508	86.139190	50.474317
208.768283	95.840362	50.479322
205.593812	89.437399	50.484327
201.649939	104.637007	50.489332
198.388066	105.325645	50.494337
194.797410	101.482356	50.499341
191.159499	101.954260	50.504346
187.395069	106.104522	50.509351
183.717223	105.040929	50.514356
180.579310	105.605385	50.519361
177.305663	109.101057	50.524365
173.612294	98.992039	50.529370
170.616648	96.039320	50.534375
166.543256	103.036132	50.539380
163.493390	94.597162	50.544385
159.746814	109.996088	50.549389
156.307095	100.021551	50.554394
152.926241	90.382570	50.559399
149.171242	112.510897	50.564404
145.819492	100.505819	50.569409
142.367283	104.778681	50.574413
138.225705	97.651067	50.579418
134.719317	97.074854	50.584423
130.919297	97.984599	50.589428
128.245387	100.750175	50.594433
124.846757	99.103897	50.599437
121.167750	98.674979	50.604442
117.935353	86.755284	50.609447
114.076822	99.307803	50.614452
110.759309	93.319019	50.619457
107.247839	91.732161	50.624461
103.617402	105.771758	50.629466
100.235490	93.596122	50.634471
96.596906	99.776611	50.639476
93.461996	94.739611	50.644481
89.385208	103.002548	50.649485
85.771081	94.827721	50.654490
82.687872	100.504884	50.659495
78.695804	106.568318	50.664500
75.556924	95.285492	50.669505
71.819800	96.129198	50.674509
68.838421	94.413628	50.679514
65.308689	102.673087	50.684519
61.699504	102.797977	50.689524
57.655898	103.763871	50.694529
54.735771	104.416359	50.699533
51.308153	106.812746	50.704538
48.000261	93.234669	50.709543
43.869836	103.372721	50.714548
40.624129	101.431947	50.719553
36.564416	111.615288	50.724557
33.394378	102.782209	50.729562
30.025044	107.204195	50.734567
26.329700	101.166994	50.739572
23.304820	100.214467	50.744577
19.873936	101.195184	50.749581
16.262947	100.109993	50.754586
12.671750	100.107821	50.759591
8.530738	101.757922	50.764596
5.572967	90.866169	50.769601
1.693304	99.140039	50.774605