Fri Jun 17 18:05:57 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
0.960116	89.033743	0.000000
1.198100	96.348314	0.005005
1.291216	98.838370	0.010010
1.180272	109.926077	0.015014
1.377051	89.049231	0.020019
1.147423	85.636329	0.025024
0.518074	86.693873	0.030029
0.855981	74.392046	0.035034
0.223997	78.169232	0.040038
0.207673	64.595893	0.045043
0.356880	63.146998	0.050048
-0.749827	48.792137	0.055053
-0.989559	41.546025	0.060058
-1.353203	48.144022	0.065062
-1.001081	40.144403	0.070067
-1.415073	38.471224	0.075072
-1.465860	29.569495	0.080077
-1.783537	21.086070	0.085082
-2.381097	23.135432	0.090086
-3.005530	23.466972	0.095091
-3.212065	29.424562	0.100096
-3.254183	31.003520	0.105101
-3.334123	30.219039	0.110106
-4.275311	20.697504	0.115110
-4.760672	31.127926	0.120115
-4.437375	27.864466	0.125120
-4.613117	21.949171	0.130125
-4.614110	22.798674	0.135130
-5.024951	21.787604	0.140134
-4.751486	23.191763	0.145139
-5.089041	18.032299	0.150144
-5.980486	29.839692	0.155149
-6.018699	12.419356	0.160154
-6.552061	19.007072	0.165158
-6.419451	25.786010	0.170163
-6.514412	24.470447	0.175168
-7.307616	19.534715	0.180173
-7.898632	14.889195	0.185178
-7.925591	18.708276	0.190182
-7.702826	13.643932	0.195187
-8.199095	16.685203	0.200192
-8.017003	16.451523	0.205197
-7.693149	22.545118	0.210202
-8.400124	25.445593	0.215206
-8.582242	19.305615	0.220211
-9.020503	24.757092	0.225216
-9.885205	16.814702	0.230221
-10.330458	11.806339	0.235226
-10.600797	25.750175	0.240230
-10.798560	22.578850	0.245235
-10.467847	14.442896	0.250240
-11.177280	19.172229	0.255245
-10.878672	16.924582	0.260250
-10.901607	29.642536	0.265254
-11.158559	19.155996	0.270259
-12.086071	19.930599	0.275264
-12.668888	15.011995	0.280269
-12.234724	14.125684	0.285274
-12.389642	28.041458	0.290278
-12.368626	24.899281	0.295283
-13.481874	23.453824	0.300288
-13.879826	24.325303	0.305293
-13.077413	17.141396	0.310298
-13.488657	27.940538	0.315302
-13.666392	19.316840	0.320307
-14.138016	26.520817	0.325312
-15.034589	19.049225	0.330317
-14.949645	18.592925	0.335322
-15.700240	24.137756	0.340326
-15.676265	19.382516	0.345331
-15.568620	13.245880	0.350336
-15.808264	18.342103	0.355341
-15.758906	22.667475	0.360346
-15.871935	30.230779	0.365350
-16.433306	11.663308	0.370355
-17.087809	26.367570	0.375360
-17.200175	22.079771	0.380365
-16.946807	24.867586	0.385370
-17.558225	33.957786	0.390374
-17.865836	26.221750	0.395379
-18.142559	27.840887	0.400384
-18.690098	31.400188	0.405389
-18.389849	23.455177	0.410394
-18.574912	25.303963	0.415398
-18.735380	22.750000	0.420403
-19.672919	27.933419	0.425408
-19.947391	24.232782	0.430413
-19.689925	21.443594	0.435418
-20.050316	20.302981	0.440422
-19.915174	23.546149	0.445427
-20.386595	17.071245	0.450432
-21.569047	26.761915	0.455437
-21.072934	19.398043	0.460442
-21.858104	21.218709	0.465446
-21.605492	22.590616	0.470451
-21.794047	21.758873	0.475456
-21.872819	18.900468	0.480461
-21.805377	19.112470	0.485466
-22.702550	27.608057	0.490470
-22.987514	19.392895	0.495475
-23.224488	32.265417	0.500480
-23.586719	31.052492	0.505485
-23.246875	18.933903	0.510490
-23.795682	32.734201	0.515494
-24.251050	27.795003	0.520499
-24.656952	23.202579	0.525504
-25.100510	22.705270	0.530509
-25.272022	18.070730	0.535514
-25.165909	21.583341	0.540518
-25.116077	26.143653	0.545523
-25.412874	26.930636	0.550528
-25.385257	31.968627	0.555533
-26.040386	21.511964	0.560538
-26.396813	27.466448	0.565542
-26.656544	21.865846	0.570547
-27.063122	19.900971	0.575552
-27.130387	30.875590	0.580557
-27.165786	17.178782	0.585562
-28.134339	24.120624	0.590566
-28.220967	18.811712	0.595571
-28.465460	17.246128	0.600576
-28.841058	14.928017	0.605581
-29.007780	15.802501	0.610586
-28.735843	25.842226	0.615590
-28.892417	25.698582	0.620595
-28.835184	23.190916	0.625600
-29.062198	29.598268	0.630605
-29.661178	22.461413	0.635610
-30.798481	30.202076	0.640614
-30.320964	29.917316	0.645619
-30.513037	22.626592	0.650624
-30.758186	28.758922	0.655629
-30.747540	24.098049	0.660634
-31.666525	29.983838	0.665638
-31.916526	31.345756	0.670643
-32.092953	32.893563	0.675648
-32.239531	27.498711	0.680653
-31.675833	29.027683	0.685658
-32.354474	34.453805	0.690662
-32.803669	23.066644	0.695667
-33.138388	30.287727	0.700672
-33.361233	23.049280	0.705677
-33.202058	31.655607	0.710682
-33.770467	34.050585	0.715686
-34.126790	23.282992	0.720691
-34.228748	30.678501	0.725696
-34.476794	28.128834	0.730701
-34.560518	29.272690	0.735706
-35.854846	29.015661	0.740710
-36.333238	26.470145	0.745715
-35.929623	27.115249	0.750720
-35.371025	28.057817	0.755725
-36.068418	19.488336	0.760730
-36.536902	25.859261	0.765734
-36.554503	26.670677	0.770739
-36.515244	24.275319	0.775744
-37.348172	33.487389	0.780749
-37.323664	22.496461	0.785754
-37.893268	29.595567	0.790758
-37.820150	29.173396	0.795763
-38.183518	18.885502	0.800768
-38.139176	29.842159	0.805773
-38.282627	21.313599	0.810778
-39.400596	27.283770	0.815782
-39.071098	26.966586	0.820787
-39.124182	26.988861	0.825792
-39.487019	34.721954	0.830797
-39.664018	33.639064	0.835802
-40.614798	40.239542	0.840806
-40.695285	26.274159	0.845811
-40.670803	25.213228	0.850816
-41.289562	32.475804	0.855821
-41.101349	26.741939	0.860826
-41.175205	26.656374	0.865830
-41.440477	19.596460	0.870835
-42.078428	27.870971	0.875840
-42.954691	19.203750	0.880845
-42.515092	24.638162	0.885850
-42.338750	26.998143	0.890854
-42.695176	18.009297	0.895859
-42.655111	23.324238	0.900864
-43.029846	28.040369	0.905869
-43.617293	21.050584	0.910874
-44.306340	19.347754	0.915878
-44.223539	19.564307	0.920883
-44.247452	25.793453	0.925888
-44.454896	14.702562	0.930893
-44.944153	12.707627	0.935898
-45.432845	29.636643	0.940902
-45.661303	13.382383	0.945907
-45.890318	22.536291	0.950912
-46.032083	14.334233	0.955917
-45.864886	15.551619	0.960922
-46.272260	23.477993	0.965926
-46.461263	18.902601	0.970931
-46.857783	24.739234	0.975936
-47.349959	33.238743	0.980941
-47.493560	20.163748	0.985946
-47.382595	18.217037	0.990950
-47.488721	25.878841	0.995955
-48.361470	25.009479	1.000960
-48.832754	21.320645	1.005965
-49.102362	19.572563	1.010970
-49.114854	25.405152	1.015974
-49.142060	17.166882	1.020979
-49.071014	17.005728	1.025984
-49.605122	17.275494	1.030989
-49.810209	10.597872	1.035994
-50.457356	21.368736	1.040998
-50.343980	17.042035	1.046003
-50.617526	25.412848	1.051008
-50.733454	19.219841	1.056013
-50.773826	12.747094	1.061018
-51.908011	15.661362	1.066022
-51.977063	14.364780	1.071027
-52.463186	7.654746	1.076032
-52.510673	20.256990	1.081037
-52.379249	12.187513	1.086042
-52.744255	24.844711	1.091046
-52.755711	24.004449	1.096051
-52.480163	24.365374	1.101056
-53.067647	27.371297	1.106061
-53.505362	17.178446	1.111066
-54.007778	28.462781	1.116070
-53.898454	18.470057	1.121075
-54.585255	15.342339	1.126080
-55.551183	32.582351	1.131085
-55.481893	15.938796	1.136090
-55.379076	28.563618	1.141094
-55.391744	19.989445	1.146099
-55.534069	23.174149	1.151104
-55.754267	29.515249	1.156109
-55.701496	23.228291	1.161114
-56.478462	30.727913	1.166118
-56.884717	26.791080	1.171123
-57.149425	18.595447	1.176128
-57.771099	26.858569	1.181133
-57.166127	20.265719	1.186138
-57.462615	28.006131	1.191142
-57.609091	14.198544	1.196147
-58.110219	23.868906	1.201152
-58.872234	26.275744	1.206157
-58.788570	20.387979	1.211162
-58.962378	24.708612	1.216166
-58.780849	20.778460	1.221171
-58.819222	18.936492	1.226176
-59.848419	19.795496	1.231181
-59.841792	26.963389	1.236186
-60.517412	32.450381	1.241190
-60.521208	30.848338	1.246195
-60.365917	21.695697	1.251200
-60.960067	23.998857	1.256205
-61.575768	29.611650	1.261210
-61.943198	30.341509	1.266214
-62.170203	22.130531	1.271219
-62.169239	20.972280	1.276224
-62.182755	12.408514	1.281229
-62.304016	14.628329	1.286234
-62.413814	25.315004	1.291238
-62.556949	14.426542	1.296243
-62.999547	20.601952	1.301248
-63.464034	27.089230	1.306253
-63.457203	20.232723	1.311258
-63.639226	21.377725	1.316262
-64.407384	30.260936	1.321267
-64.816279	19.507222	1.326272
-65.547200	28.433772	1.331277
-65.272472	20.117488	1.336282
-65.352108	28.169152	1.341286
-65.359910	22.111298	1.346291
-65.028759	21.445157	1.351296
-65.472077	29.996333	1.356301
-65.892938	20.472586	1.361306
-66.421324	21.402653	1.366310
-66.467685	20.821169	1.371315
-66.654032	14.169834	1.376320
-67.613350	25.964834	1.381325
-68.622395	17.105593	1.386330
-67.932216	23.606349	1.391334
-67.698871	22.486625	1.396339
-68.019307	12.318092	1.401344
-68.557298	21.431997	1.406349
-68.331857	25.589965	1.411354
-68.707972	20.363513	1.416358
-69.238726	23.619101	1.421363
-69.618241	16.850103	1.426368
-70.168597	15.682073	1.431373
-70.076331	22.270182	1.436378
-70.316094	20.647576	1.441382
-70.153303	17.339560	1.446387
-70.519026	19.340526	1.451392
-71.273897	25.043347	1.456397
-71.564668	12.677362	1.461402
-71.628878	20.322919	1.466406
-71.446853	26.145865	1.471411
-71.727785	18.647332	1.476416
-72.066078	26.296620	1.481421
-72.098299	20.878621	1.486426
-72.650729	19.676206	1.491430
-73.100331	19.280743	1.496435
-73.087706	13.532264	1.501440
-73.437258	17.512512	1.506445
-73.877531	16.381238	1.511450
-74.148831	23.638346	1.516454
-74.561953	24.428488	1.521459
-74.677109	26.341430	1.526464
-75.048730	19.751281	1.531469
-74.654450	18.450493	1.536474
-74.947049	24.491650	1.541478
-75.185896	22.768254	1.546483
-75.789757	20.088502	1.551488
-76.170571	25.836293	1.556493
-75.948036	13.967494	1.561498
-76.177808	25.924782	1.566502
-76.776666	22.369242	1.571507
-77.140913	20.560134	1.576512
-77.409689	17.941696	1.581517
-77.636803	16.625018	1.586522
-77.888246	16.768079	1.591526
-77.776074	19.341775	1.596531
-77.860035	9.713885	1.601536
-78.873557	17.939138	1.606541
-79.410227	19.044036	1.611546
-79.560061	14.820684	1.616550
-79.576379	12.418978	1.621555
-79.470599	17.658859	1.626560
-79.698780	20.194810	1.631565
-79.345315	9.596161	1.636570
-80.007976	9.599597	1.641574
-80.233702	15.753951	1.646579
-80.626214	14.683211	1.651584
-81.427621	16.970113	1.656589
-81.074048	8.116032	1.661594
-81.268776	22.481019	1.666598
-81.817181	17.776927	1.671603
-82.508167	20.208073	1.676608
-82.552916	19.742745	1.681613
-82.814829	24.598379	1.686618
-82.979368	27.032389	1.691622
-82.857040	14.212744	1.696627
-82.901667	12.605060	1.701632
-82.800392	21.796213	1.706637
-83.270129	12.083271	1.711642
-84.118972	27.581136	1.716646
-84.030106	14.750675	1.721651
-84.268777	22.984662	1.726656
-85.361389	28.952208	1.731661
-85.641549	21.916284	1.736666
-85.483827	22.121565	1.741670
-85.419382	24.284858	1.746675
-85.871271	18.475861	1.751680
-85.826244	31.563749	1.756685
-85.531960	21.633615	1.761690
-86.301173	28.757816	1.766694
-87.172356	22.634123	1.771699
-87.424267	17.129119	1.776704
-87.739407	24.189477	1.781709
-87.349251	20.162880	1.786714
-87.576171	22.399669	1.791718
-87.701942	22.231174	1.796723
-88.064218	16.833315	1.801728
-88.819075	27.099959	1.806733
-88.956782	14.720173	1.811738
-89.028482	27.983746	1.816742
-89.173809	27.150149	1.821747
-88.919944	19.132933	1.826752
-89.528899	21.696664	1.831757
-90.228546	20.077300	1.836762
-90.428401	22.772325	1.841766
-90.495717	17.913276	1.846771
-90.787440	22.349806	1.851776
-91.194675	23.212772	1.856781
-91.101654	22.579110	1.861786
-92.039632	32.866925	1.866790
-92.193318	27.799643	1.871795
-92.353585	22.498636	1.876800
-92.777925	21.219678	1.881805
-92.556498	19.927890	1.886810
-92.519805	32.244818	1.891814
-92.305435	31.759305	1.896819
-92.717114	23.097350	1.901824
-93.584543	22.180151	1.906829
-93.850472	30.913771	1.911834
-93.938428	29.266521	1.916838
-94.240101	26.144641	1.921843
-94.717569	26.600947	1.926848
-95.577513	24.562662	1.931853
-95.251492	21.373139	1.936858
-95.515227	30.932216	1.941862
-95.589231	16.119232	1.946867
-95.594690	16.401959	1.951872
-95.972031	17.912325	1.956877
-95.716851	24.151506	1.961882
-96.135755	23.897558	1.966886
-96.851111	27.943751	1.971891
-96.793700	20.348129	1.976896
-97.556154	32.298861	1.981901
-97.133101	30.375252	1.986906
-98.118276	23.251308	1.991910
-98.265596	13.011971	1.996915
-98.661683	21.713993	2.006912
-97.911102	22.455876	2.016909
-97.466633	18.258133	2.026906
-97.319665	20.979952	2.036902
-96.381924	20.426398	2.046899
-95.863444	23.839639	2.056896
-95.886550	22.733929	2.066893
-94.873915	20.476232	2.076890
-94.360383	26.924951	2.086886
-94.353839	26.236346	2.096883
-93.185514	27.587675	2.106880
-93.027172	21.065728	2.116877
-92.679493	22.400354	2.126874
-91.989628	20.016712	2.136870
-91.695963	22.087615	2.146867
-90.937985	19.011983	2.156864
-90.014142	20.411265	2.166861
-90.039571	25.376436	2.176858
-90.091668	20.934441	2.186854
-88.981187	25.673044	2.196851
-88.559604	25.850597	2.206848
-88.096348	28.990875	2.216845
-87.215429	24.239664	2.226842
-86.962020	23.130862	2.236838
-86.791648	23.296236	2.246835
-85.812413	21.274868	2.256832
-85.244505	23.933432	2.266829
-85.323056	21.249766	2.276826
-84.415527	28.573085	2.286822
-84.015497	25.339814	2.296819
-83.855748	19.252312	2.306816
-83.194020	16.764878	2.316813
-82.408515	23.454880	2.326810
-81.344277	22.012918	2.336806
-81.388720	19.381078	2.346803
-80.983908	22.965356	2.356800
-80.730811	19.468635	2.366797
-80.045892	14.754554	2.376794
-79.329244	18.495244	2.386790
-79.143156	21.685350	2.396787
-78.633713	21.309494	2.406784
-78.131839	28.571623	2.416781
-77.581563	21.580073	2.426778
-76.644496	16.466454	2.436774
-76.311331	24.196245	2.446771
-76.325467	23.226363	2.456768
-75.373879	20.073500	2.466765
-75.252204	18.353348	2.476762
-74.437822	18.711991	2.486758
-73.854829	21.246931	2.496755
-73.459125	20.774398	2.506752
-73.157445	18.733089	2.516749
-72.211370	26.836378	2.526746
-71.800093	16.506085	2.536742
-71.953148	16.199855	2.546739
-70.759106	20.979697	2.556736
-70.389659	12.717532	2.566733
-70.100555	14.728932	2.576730
-69.085047	20.172689	2.586726
-68.860627	20.870849	2.596723
-68.662895	14.741075	2.606720
-67.960490	16.501799	2.616717
-67.260873	16.743585	2.626714
-66.952273	16.051991	2.636710
-66.704741	20.699717	2.646707
-65.779720	21.475638	2.656704
-65.430197	17.546981	2.666701
-65.148088	19.950953	2.676698
-63.912020	18.297868	2.686694
-63.888193	17.293421	2.696691
-63.972098	23.984704	2.706688
-62.661738	16.453468	2.716685
-62.329530	21.841881	2.726682
-62.180557	20.933796	2.736678
-61.541902	22.556538	2.746675
-61.127603	23.656629	2.756672
-60.179473	18.209434	2.766669
-59.546076	16.631044	2.776666
-59.329146	17.199057	2.786662
-59.659026	17.468335	2.796659
-58.563407	16.287305	2.806656
-57.950883	16.321884	2.816653
-57.153053	14.099707	2.826650
-56.502733	11.810569	2.836646
-56.182565	13.742516	2.846643
-56.075920	12.778045	2.856640
-55.825371	13.519083	2.866637
-54.851897	9.959720	2.876634
-54.656852	11.438665	2.886630
-54.054891	18.236635	2.896627
-53.331659	18.558471	2.906624
-53.139097	14.539333	2.916621
-52.054590	18.760254	2.926618
-51.795549	13.989332	2.936614
-51.660956	15.081187	2.946611
-50.634748	11.829190	2.956608
-50.093039	15.397629	2.966605
-49.969146	17.689991	2.976602
-49.672905	14.692107	2.986598
-48.762928	15.725413	2.996595
-48.716289	21.684691	3.006592
-47.916852	20.287348	3.016589
-47.093027	16.440484	3.026586
-46.866109	12.760613	3.036582
-46.603259	22.353040	3.046579
-46.059827	11.512559	3.056576
-45.599355	12.662077	3.066573
-44.526068	17.986975	3.076570
-44.130354	13.451574	3.086566
-43.925087	17.348405	3.096563
-43.573937	16.774019	3.106560
-42.584301	10.873594	3.116557
-42.093353	12.177692	3.126554
-42.109216	15.417571	3.136550
-41.522326	15.094247	3.146547
-40.951221	18.886404	3.156544
-40.681171	18.861735	3.166541
-39.971731	12.378193	3.176538
-38.969513	17.154367	3.186534
-38.816253	15.851791	3.196531
-38.595996	22.280906	3.206528
-37.408848	13.910876	3.216525
-37.395823	7.877800	3.226522
-37.254675	9.276595	3.236518
-36.586025	20.857604	3.246515
-36.063915	15.858215	3.256512
-34.943980	16.720096	3.266509
-34.599978	16.142551	3.276506
-34.745254	19.649734	3.286502
-33.736530	17.491296	3.296499
-33.261193	16.931635	3.306496
-33.008831	15.935237	3.316493
-32.633653	23.389934	3.326490
-31.648067	18.294142	3.336486
-31.493250	15.600925	3.346483
-30.959585	18.354694	3.356480
-29.833716	17.623873	3.366477
-29.869487	13.649604	3.376474
-29.678021	14.846210	3.386470
-28.652868	17.229024	3.396467
-28.381074	17.466849	3.406464
-28.052641	15.901812	3.416461
-27.370409	14.946978	3.426458
-26.633128	14.281934	3.436454
-26.583943	16.072213	3.446451
-25.345926	15.731548	3.456448
-25.024249	9.717703	3.466445
-24.817272	15.531385	3.476442
-24.630177	11.857738	3.486438
-23.852297	13.588144	3.496435
-23.076886	13.634577	3.506432
-23.036942	16.970097	3.516429
-22.357002	11.211843	3.526426
-21.815989	19.487786	3.536422
-21.667151	12.770036	3.546419
-20.294315	13.622683	3.556416
-19.866380	14.662027	3.566413
-20.007702	12.479783	3.576410
-19.814240	13.862376	3.586406
-18.834558	23.256626	3.596403
-18.388410	19.067897	3.606400
-18.160397	14.107712	3.616397
-17.275547	18.969198	3.626394
-16.755953	15.318328	3.636390
-15.808472	16.664899	3.646387
-15.496441	16.987122	3.656384
-15.174983	13.250045	3.666381
-15.166516	12.208437	3.676378
-14.759035	11.033527	3.686374
-13.678811	11.898853	3.696371
-13.532434	15.308557	3.706368
-12.468305	18.528770	3.716365
-11.831952	17.855807	3.726362
-11.869093	13.396109	3.736358
-11.774930	13.177213	3.746355
-10.742132	14.366752	3.756352
-10.706376	14.787651	3.766349
-9.590660	18.463804	3.776346
-9.196277	14.791663	3.786342
-9.077854	20.626390	3.796339
-8.037409	17.602218	3.806336
-7.606786	9.505339	3.816333
-7.426499	10.425016	3.826330
-6.825270	10.284447	3.836326
-6.264408	14.442653	3.846323
-5.896035	12.171936	3.856320
-5.319990	8.983709	3.866317
-4.713374	14.750330	3.876314
-4.586025	11.539867	3.886310
-3.865769	29.792944	3.896307
-3.677776	36.296191	3.906304
-3.050641	49.001655	3.916301
-2.605602	52.628067	3.926298
-1.894803	71.805871	3.936294
-1.781576	77.214903	3.946291
-1.452591	93.104211	3.956288
-0.715263	111.072005	3.966285
0.000000	117.546435	3.971290
-0.337665	130.409333	3.976294
-0.304283	138.846011	3.981299
0.315030	141.468637	3.986304
0.354547	148.905414	3.991309
0.698798	139.436347	3.996314
0.533649	152.562441	4.001318
0.540639	147.698492	4.006323
0.601847	146.203044	4.011328
0.651419	154.359593	4.016333
0.801107	142.609357	4.021338
0.542729	156.911846	4.026342
0.443194	145.928025	4.031347
0.886589	146.423068	4.036352
0.445245	147.574673	4.041357
0.614831	153.540044	4.046362
0.264160	158.983126	4.051366
0.492778	155.917119	4.056371
0.477912	141.091406	4.061376
0.466817	147.675641	4.066381
0.674604	145.856282	4.071386
1.015112	151.632024	4.076390
0.823250	152.581140	4.081395
0.728088	149.649659	4.086400
0.490031	154.541426	4.091405
0.555354	146.810827	4.096410
0.298376	159.629554	4.101414
0.661652	149.094298	4.106419
1.076898	149.482528	4.111424
0.756188	146.864207	4.116429
0.854201	147.677527	4.121434
0.412716	149.999129	4.126438
0.603548	153.448358	4.131443
0.765687	147.722333	4.136448
0.404485	157.954802	4.141453
0.671311	146.775902	4.146458
1.196639	164.807334	4.151462
0.637230	163.280261	4.156467
0.822494	169.423196	4.161472
0.912471	181.774615	4.166477
0.992145	180.379693	4.171482
0.950733	173.229018	4.176486
0.675549	175.021564	4.181491
1.014078	174.222575	4.186496
0.862981	188.075108	4.191501
1.245016	182.622923	4.196506
0.933002	180.868448	4.201510
0.591692	175.637922	4.206515
0.797370	184.034937	4.211520
0.883117	187.798821	4.216525
0.968092	179.967852	4.221530
1.113875	183.068984	4.226534
1.189688	176.675321	4.231539
1.334744	178.646656	4.236544
1.272363	186.673042	4.241549
1.343846	191.945329	4.246554
1.378589	175.984773	4.251558
0.907599	163.657486	4.256563
0.964577	160.594551	4.261568
0.895015	183.330585	4.266573
0.750731	181.434568	4.271578
1.117488	180.944447	4.276582
1.135514	188.715541	4.281587
0.949917	172.834433	4.286592
0.869885	184.630012	4.291597
0.877294	182.004112	4.296602
0.997053	183.373451	4.301606
1.244742	182.044335	4.306611
1.268865	188.556234	4.311616
1.001428	177.973056	4.316621
1.126455	182.847106	4.321626
1.269981	191.283660	4.326630
1.269317	189.721730	4.331635
1.661735	187.685594	4.336640
1.367941	180.658560	4.341645
1.283101	182.508663	4.346650
1.272288	177.178608	4.351654
1.264176	185.304900	4.356659
1.361020	183.103986	4.361664
1.613973	183.691856	4.366669
1.434319	181.778828	4.371674
1.489219	191.118498	4.376678
1.402463	186.616829	4.381683
1.443421	182.299356	4.386688
1.386604	188.915085	4.391693
1.839545	181.333160	4.396698
1.637445	181.519716	4.401702
1.293344	185.941316	4.406707
1.413557	175.774603	4.411712
1.226901	185.109032	4.416717
1.622809	182.252604	4.421722
1.486974	179.679324	4.426726
1.312487	185.893703	4.431731
1.934368	194.525436	4.436736
1.390478	199.476732	4.441741
1.577788	199.012095	4.446746
1.616688	201.321346	4.451750
1.208062	202.355235	4.456755
1.546756	201.627257	4.461760
1.564918	215.575408	4.466765
1.775990	209.419332	4.471770
1.928081	217.006149	4.476774
1.567650	209.472182	4.481779
1.561369	208.762077	4.486784
1.741372	216.177509	4.491789
1.835294	212.341198	4.496794
1.959578	215.150702	4.501798
1.978306	201.756908	4.506803
1.813362	190.638888	4.511808
1.324278	195.833855	4.516813
1.865863	207.425098	4.521818
1.951035	208.550761	4.526822
1.580904	209.013687	4.531827
1.995017	206.654661	4.536832
1.776316	209.975824	4.541837
1.773059	211.704233	4.546842
2.032245	216.890077	4.551846
1.841127	212.563217	4.556851
2.055351	210.247281	4.561856
1.483928	211.284747	4.566861
1.816529	210.216990	4.571866
1.740672	218.876897	4.576870
1.355459	220.176253	4.581875
1.660510	208.199260	4.586880
1.768565	220.282097	4.591885
1.944063	208.358211	4.596890
1.942927	220.273113	4.601894
1.726267	218.589610	4.606899
2.276388	211.504974	4.611904
1.715344	229.044741	4.616909
2.001469	218.940012	4.621914
1.994142	210.241706	4.626918
1.695941	224.250933	4.631923
1.955066	219.637499	4.636928
2.370362	241.653280	4.641933
2.044717	229.595214	4.646938
1.951446	226.989001	4.651942
1.849763	234.574002	4.656947
2.197641	246.736976	4.661952
2.347516	255.127912	4.666957
2.175788	244.076299	4.671962
2.133032	256.511012	4.676966
1.774965	245.714735	4.681971
1.797731	246.303967	4.686976
2.262355	250.378836	4.691981
2.217494	250.047309	4.696986
2.423269	241.708821	4.701990
2.400740	252.852776	4.706995
2.511801	248.576123	4.712000
2.284083	245.456694	4.717005
2.232046	249.298155	4.722010
2.325410	254.285431	4.727014
1.952046	249.115067	4.732019
2.316278	248.623982	4.737024
2.146962	248.596510	4.742029
1.994364	239.194572	4.747034
2.308357	251.323518	4.752038
2.092111	263.370505	4.757043
2.825771	249.109359	4.762048
2.818090	254.030550	4.767053
2.688126	257.558184	4.772058
2.504526	256.517812	4.777062
2.278454	260.157718	4.782067
2.473842	247.134711	4.787072
2.310665	259.184517	4.792077
2.418675	246.129661	4.797082
2.414838	248.736298	4.802086
2.331203	250.674614	4.807091
2.657947	250.504109	4.812096
2.626368	249.515036	4.817101
2.628651	254.017214	4.822106
2.728433	250.555640	4.827110
2.366113	247.159231	4.832115
3.021249	243.064663	4.837120
3.021097	245.511637	4.842125
2.784685	238.971722	4.847130
2.387959	222.928915	4.852134
2.180332	240.105272	4.857139
2.694317	236.081131	4.862144
2.472296	239.008189	4.867149
2.627652	244.520322	4.872154
3.008032	241.900894	4.877158
2.665185	249.842902	4.882163
2.563054	251.724698	4.887168
2.502356	245.712840	4.892173
2.557075	243.201412	4.897178
2.658577	242.877526	4.902182
2.385375	246.131191	4.907187
2.710984	240.981205	4.912192
2.317027	252.971093	4.917197
2.336702	250.267368	4.922202
2.494385	255.762740	4.927206
2.362996	259.855769	4.932211
2.986122	263.098393	4.937216
3.050124	276.833951	4.942221
3.139654	270.080996	4.947226
2.719667	258.647752	4.952230
2.656839	258.097607	4.957235
3.047818	258.885130	4.962240
2.838075	268.734537	4.967245
2.921004	258.899960	4.972250
3.178291	260.264207	4.977254
2.696526	260.108701	4.982259
2.820974	248.950234	4.987264
2.529630	262.459895	4.992269
2.843824	275.883129	4.997274
2.920932	269.761333	5.002278
2.866141	275.222567	5.007283
2.715443	274.745634	5.012288
2.783637	270.006055	5.017293
2.964146	267.402676	5.022298
3.165645	278.625642	5.027302
2.755803	274.477002	5.032307
3.064885	276.499032	5.037312
2.578080	280.789077	5.042317
3.020342	281.094479	5.047322
3.206877	271.914393	5.052326
2.599609	284.816310	5.057331
3.289330	290.226815	5.062336
3.344969	301.637039	5.067341
3.059159	291.125706	5.072346
3.130356	288.216077	5.077350
3.288471	296.568766	5.082355
3.279639	292.703536	5.087360
2.910707	290.068341	5.092365
3.204666	295.221595	5.097370
3.541559	295.951806	5.102374
3.293281	288.561958	5.107379
3.343425	272.560658	5.112384
3.017563	278.378929	5.117389
3.339188	277.989645	5.122394
3.599103	283.989781	5.127398
3.222093	279.234213	5.132403
3.021723	281.583640	5.137408
3.254438	291.780430	5.142413
3.150284	305.022216	5.147418
3.617150	302.514302	5.152422
3.408393	308.636746	5.157427
3.612014	291.757045	5.162432
3.108195	291.508510	5.167437
3.414228	299.109839	5.172442
3.662136	294.901793	5.177446
3.419102	309.879908	5.182451
3.810469	289.979016	5.187456
3.288212	293.096093	5.192461
3.297810	286.195392	5.197466
3.321592	284.290175	5.202470
3.740915	304.676990	5.207475
3.798653	290.889468	5.212480
3.225554	289.989215	5.217485
3.272210	283.101695	5.222490
3.702403	296.591703	5.227494
3.522903	310.397167	5.232499
3.970293	298.469262	5.237504
3.582556	296.882660	5.242509
3.598393	279.891709	5.247514
3.468562	284.813479	5.252518
3.631498	277.564263	5.257523
3.356188	276.988854	5.262528
3.681259	300.737100	5.267533
3.794396	306.718820	5.272538
3.756793	310.387598	5.277542
3.751305	309.752738	5.282547
4.066562	290.295471	5.287552
3.629387	282.246360	5.292557
3.693817	279.379890	5.297562
3.552504	280.318638	5.302566
3.128648	294.529965	5.307571
3.906408	294.508074	5.312576
4.002363	306.419337	5.317581
4.077405	298.005263	5.322586
3.710484	292.959711	5.327590
3.565128	301.299893	5.332595
3.768838	295.455017	5.337600
3.751490	307.682296	5.342605
3.635911	312.708661	5.347610
3.800948	312.807162	5.352614
3.818269	314.309176	5.357619
3.963969	306.052664	5.362624
3.934825	322.113130	5.367629
3.859043	305.770620	5.372634
3.880474	311.893088	5.377638
3.696670	316.903168	5.382643
3.915453	305.451531	5.387648
3.904136	313.328600	5.392653
3.917994	317.203920	5.397658
4.012203	310.701768	5.402662
3.523122	321.944434	5.407667
3.539035	308.348749	5.412672
3.549138	318.872045	5.417677
3.788505	314.522346	5.422682
4.123149	327.596696	5.427686
4.160436	328.842018	5.432691
4.363888	329.130480	5.437696
3.919877	321.864908	5.442701
4.288613	320.938349	5.447706
4.058848	319.640233	5.452710
3.811005	324.991887	5.457715
4.185305	315.954021	5.462720
4.236889	334.146484	5.467725
4.178700	335.821482	5.472730
4.726841	330.791754	5.477734
4.175070	319.590726	5.482739
4.270649	319.307487	5.487744
4.077518	322.494184	5.492749
4.218701	311.509899	5.497754
4.513300	308.995491	5.502758
4.108304	306.432986	5.507763
4.136118	308.948927	5.512768
3.950913	311.293470	5.517773
4.292274	318.339168	5.522778
4.309853	324.236730	5.527782
4.011783	324.638742	5.532787
4.458674	331.020245	5.537792
4.484909	329.865664	5.542797
4.413132	332.023624	5.547802
4.134088	317.638685	5.552806
4.318968	332.027699	5.557811
4.587571	324.866273	5.562816
4.256904	331.259602	5.567821
4.524872	339.738306	5.572826
4.530053	326.128208	5.577830
4.029498	332.099855	5.582835
4.351240	324.836259	5.587840
4.558519	326.027672	5.592845
4.433638	333.978486	5.597850
4.275760	334.805933	5.602854
4.047129	332.747106	5.607859
4.280714	326.628880	5.612864
4.133193	328.677280	5.617869
4.459818	328.693472	5.622874
4.507575	326.519838	5.627878
4.574746	324.926097	5.632883
4.414489	320.422792	5.637888
4.331067	327.781028	5.642893
4.193614	329.251937	5.647898
4.715639	334.435574	5.652902
4.574589	361.460946	5.657907
4.808175	363.638604	5.662912
4.703931	363.295633	5.667917
4.696796	358.454290	5.672922
4.856278	352.292328	5.677926
4.622322	352.237317	5.682931
4.457030	337.175544	5.687936
4.530377	351.432351	5.692941
4.652473	359.476117	5.697946
4.658020	354.247474	5.702950
4.406818	364.686360	5.707955
4.405693	370.842990	5.712960
4.660904	365.145422	5.717965
4.670817	374.360861	5.722970
4.863490	365.137272	5.727974
4.373367	373.168152	5.732979
4.767604	374.450841	5.737984
4.764296	367.320186	5.742989
4.966361	371.946269	5.747994
4.602916	365.780050	5.752998
4.440287	365.509141	5.758003
4.820504	371.120894	5.763008
4.707584	386.156982	5.768013
4.786760	401.473732	5.773018
5.001753	391.298624	5.778022
4.930999	397.332256	5.783027
5.219700	398.968746	5.788032
5.171193	406.395018	5.793037
4.766924	390.922597	5.798042
5.033633	392.057173	5.803046
4.896574	394.524952	5.808051
5.167656	397.330219	5.813056
5.232216	387.886966	5.818061
4.820117	385.873229	5.823066
5.239090	377.757936	5.828070
5.261398	382.872307	5.833075
4.846871	359.967275	5.838080
4.815284	368.879006	5.843085
4.993011	389.958672	5.848090
5.278291	384.973999	5.853094
5.082925	389.948135	5.858099
5.320290	394.060619	5.863104
5.313786	389.220741	5.868109
5.057893	387.302203	5.873114
4.981365	390.276936	5.878118
5.368283	401.373861	5.883123
5.295275	387.527275	5.888128
5.176935	398.010207	5.893133
5.191759	393.403386	5.898138
5.255575	394.978193	5.903142
4.918810	393.697658	5.908147
5.234762	381.168751	5.913152
5.368170	396.963700	5.918157
5.232369	391.463129	5.923162
5.390779	394.586478	5.928166
5.324767	392.795430	5.933171
5.254396	387.716738	5.938176
5.148005	393.818058	5.943181
4.936214	394.003661	5.948186
5.418540	397.755552	5.953190
4.948224	390.133002	5.958195
5.042794	392.019615	5.963200
5.186492	397.009424	5.968205
5.172848	398.520540	5.973210
5.381513	390.274436	5.978214
5.516204	392.319745	5.983219
5.730082	385.110950	5.988224
5.351232	397.176583	5.993229
5.154725	397.817460	5.998234
5.141741	397.052220	6.003238
5.129921	401.542183	6.008243
5.465751	415.696419	6.013248
5.567644	418.293799	6.018253
5.594405	418.575716	6.023258
5.707819	398.930058	6.028262
5.417048	401.033851	6.033267
5.609635	391.621215	6.038272
5.353075	396.775429	6.043277
5.649708	405.222764	6.048282
5.367976	395.865086	6.053286
5.225318	393.094978	6.058291
5.321370	393.692754	6.063296
5.643802	392.089336	6.068301
5.490823	391.874838	6.073306
5.617044	392.392811	6.078310
5.343977	396.072133	6.083315
5.550296	391.062299	6.088320
5.449520	394.080530	6.093325
5.318972	393.704042	6.098330
5.733095	393.258336	6.103334
5.436975	393.255491	6.108339
5.105117	390.282398	6.113344
5.334569	393.939962	6.118349
5.126328	400.872214	6.123354
5.405860	396.299342	6.128358
5.207467	398.839674	6.133363
5.468405	392.763841	6.138368
5.528391	401.099942	6.143373
5.489626	393.445326	6.148378
5.607133	389.616694	6.153382
5.334173	400.472833	6.158387
5.727431	387.606063	6.163392
5.769221	386.496647	6.168397
5.622333	389.496295	6.173402
5.879178	390.580809	6.178406
5.740823	395.011486	6.183411
5.419571	370.543838	6.188416
5.169658	364.031767	6.193421
5.082297	368.104286	6.198426
5.346038	372.458455	6.203430
5.362020	375.032218	6.208435
5.590038	376.394632	6.213440
5.290272	381.278571	6.218445
5.115913	389.206261	6.223450
5.467412	390.467837	6.228454
5.459841	396.178982	6.233459
5.502893	378.477733	6.238464
5.409278	392.024696	6.243469
5.737798	395.236789	6.248474
5.875236	378.441599	6.253478
5.246183	380.620559	6.258483
5.216694	365.613935	6.263488
5.267698	368.731648	6.268493
5.245172	385.613368	6.273498
5.037897	387.572251	6.278502
5.486667	392.068141	6.283507
5.398967	387.399034	6.288512
5.690690	394.670282	6.293517
5.461803	382.784467	6.298522
5.902304	394.705427	6.303526
5.466784	378.716659	6.308531
5.391050	363.574855	6.313536
5.236883	366.756861	6.318541
5.130393	363.433146	6.323546
5.410707	368.205471	6.328550
5.413636	388.641085	6.333555
5.661526	387.656463	6.338560
5.325150	376.850371	6.343565
5.345304	370.550141	6.348570
5.427983	370.348965	6.353574
5.437500	375.697129	6.358579
5.192685	368.162614	6.363584
5.388645	375.018595	6.368589
5.522660	389.894651	6.373594
5.480124	388.273356	6.378598
5.244447	378.061472	6.383603
5.313539	389.511556	6.388608
5.162805	390.682955	6.393613
5.633709	386.850839	6.398618
5.531064	395.572720	6.403622
5.501860	391.938969	6.408627
5.713345	383.252149	6.413632
5.408538	379.499041	6.418637
5.057230	371.852378	6.423642
5.238007	369.165268	6.428646
5.535800	383.512672	6.433651
5.589910	379.372334	6.438656
5.203938	380.530932	6.443661
5.405318	390.981242	6.448666
5.700689	391.767890	6.453670
5.165073	381.292096	6.458675
5.157950	382.815150	6.463680
5.598929	386.031835	6.468685
5.664253	387.237376	6.473690
5.139417	374.788036	6.478694
5.297629	383.953573	6.483699
5.532266	385.179713	6.488704
5.687155	395.870805	6.493709
5.406501	389.346073	6.498714
5.025379	368.798153	6.503718
5.334073	382.582922	6.508723
5.345469	384.126973	6.513728
5.764260	399.264927	6.518733
5.458952	383.187418	6.523738
5.320085	364.782341	6.528742
5.372930	377.236387	6.533747
5.729736	381.626988	6.538752
5.349197	371.999218	6.543757
4.957716	373.847426	6.548762
5.639468	378.263345	6.553766
5.299666	392.112299	6.558771
5.611488	386.162001	6.563776
5.510097	381.495566	6.568781
5.429122	380.676705	6.573786
5.331634	359.566415	6.578790
4.989469	381.147276	6.583795
5.292445	385.088223	6.588800
5.639346	397.145312	6.593805
5.177865	397.516471	6.598810
5.748336	397.590209	6.603814
5.265954	399.314605	6.608819
5.488387	398.927992	6.613824
5.479741	399.247762	6.618829
5.490722	392.804796	6.623834
5.167795	386.830351	6.628838
5.530611	390.091010	6.633843
5.753584	390.801483	6.638848
5.410658	378.431622	6.643853
5.422850	370.472547	6.648858
5.363608	364.168348	6.653862
5.136641	370.754617	6.658867
5.390695	370.322098	6.663872
5.233667	379.753544	6.668877
5.140720	393.563837	6.673882
5.443877	394.040364	6.678886
5.445828	395.854755	6.683891
5.771618	406.394311	6.688896
5.485182	392.676336	6.693901
5.095634	388.403326	6.698906
5.436180	389.347238	6.703910
5.164721	391.868535	6.708915
5.407149	397.563585	6.713920
5.352115	401.476029	6.718925
5.562358	411.581716	6.723930
5.543570	391.529432	6.728934
5.217131	408.746247	6.733939
5.261290	394.792958	6.738944
5.464976	402.387866	6.743949
5.351074	401.680445	6.748954
5.286885	396.488637	6.753958
5.106304	403.633756	6.758963
5.370606	395.970403	6.763968
5.458641	406.800091	6.768973
5.354620	409.629226	6.773978
5.634801	398.010436	6.778982
5.336139	406.006747	6.783987
5.564291	402.699035	6.788992
5.456422	397.317942	6.793997
5.326024	405.010413	6.799002
5.454714	397.958049	6.804006
4.956030	403.004311	6.809011
5.263379	405.425459	6.814016
5.695072	409.630363	6.819021
5.465524	401.938188	6.824026
5.403198	398.391835	6.829030
5.298456	402.950325	6.834035
5.061298	398.492537	6.839040
5.351759	403.206946	6.844045
5.205298	404.923856	6.849050
5.049796	395.130401	6.854054
5.107209	399.386855	6.859059
5.308075	389.236986	6.864064
5.568520	394.118985	6.869069
5.129120	397.411553	6.874074
5.518621	394.383089	6.879078
5.364248	408.406662	6.884083
5.266027	394.789221	6.889088
5.184009	397.784995	6.894093
5.268027	411.829924	6.899098
5.874755	413.129395	6.904102
5.766485	415.376509	6.909107
5.542640	396.807917	6.914112
5.447026	405.087792	6.919117
5.310809	398.622522	6.924122
5.836374	390.470167	6.929126
5.327797	400.611850	6.934131
5.275772	396.775085	6.939136
5.397089	395.150433	6.944141
5.129663	400.813800	6.949146
5.496771	394.380313	6.954150
5.055576	407.731882	6.959155
5.119414	400.657933	6.964160
5.352067	406.485443	6.969165
5.379866	416.362752	6.974170
5.765965	401.259787	6.979174
5.503349	401.867450	6.984179
5.674068	399.422952	6.989184
5.663718	399.133243	6.994189
5.348679	397.801342	6.999194
5.667177	400.561629	7.004198
5.467474	409.553620	7.009203
5.362146	395.535587	7.014208
5.632233	404.954665	7.019213
5.217593	398.493442	7.024218
5.402122	402.886241	7.029222
5.579069	412.384149	7.034227
5.587318	404.976077	7.039232
5.506219	399.240068	7.044237
5.438755	410.817453	7.049242
5.490347	407.619796	7.054246
5.342502	406.327198	7.059251
5.494850	402.680240	7.064256
5.317201	408.253503	7.069261
5.246756	411.902703	7.074266
5.419976	398.010051	7.079270
4.936202	403.440017	7.084275
5.356870	398.182617	7.089280
5.175176	407.012364	7.094285
5.480673	403.305220	7.099290
5.551470	403.557518	7.104294
5.186893	407.400251	7.109299
5.015445	407.407666	7.114304
5.367374	396.210495	7.119309
5.115367	410.741264	7.124314
5.455468	405.340175	7.129318
5.363337	408.341974	7.134323
5.441477	409.913809	7.139328
5.580357	402.100013	7.144333
5.435018	412.646446	7.149338
5.855342	401.530255	7.154342
5.705120	410.859554	7.159347
5.723890	411.122474	7.164352
5.821064	407.148427	7.169357
5.314778	409.033284	7.174362
5.511527	401.292356	7.179366
5.243209	413.092961	7.184371
5.510154	410.679433	7.189376
5.647567	413.705438	7.194381
5.190954	410.529694	7.199386
5.411749	413.582491	7.204390
5.500365	407.576931	7.209395
5.604482	405.527514	7.214400
5.426508	408.722168	7.219405
5.080697	409.340108	7.224410
5.455430	408.266125	7.229414
5.412250	414.959407	7.234419
5.343951	409.933643	7.239424
5.352964	411.259052	7.244429
5.465545	405.639640	7.249434
5.276875	406.212319	7.254438
5.421296	409.150134	7.259443
5.207315	406.910078	7.264448
5.697882	404.558443	7.269453
5.288242	406.795263	7.274458
5.444542	397.159353	7.279462
5.369137	413.749157	7.284467
5.106257	404.865098	7.289472
5.552213	412.029614	7.294477
5.436671	409.020169	7.299482
5.097239	413.055663	7.304486
5.176761	412.532568	7.309491
5.535691	405.727277	7.314496
5.719520	408.627758	7.319501
5.281412	412.194803	7.324506
6.043036	403.451460	7.329510
5.652239	402.983646	7.334515
5.791622	407.811376	7.339520
5.943981	399.998104	7.344525
5.177722	393.716291	7.349530
5.377983	366.932688	7.354534
5.141066	381.574783	7.359539
5.291570	381.996959	7.364544
5.381470	394.468145	7.369549
5.283158	403.964439	7.374554
5.584227	406.966398	7.379558
5.340534	408.897987	7.384563
5.492786	404.120123	7.389568
5.603367	405.997564	7.394573
5.375519	389.985910	7.399578
5.430298	390.576141	7.404582
4.848093	387.509091	7.409587
5.431122	400.463088	7.414592
5.769030	398.705149	7.419597
5.378664	402.690301	7.424602
5.553697	410.941573	7.429606
5.283535	403.199514	7.434611
5.354198	395.037913	7.439616
5.550044	395.685801	7.444621
5.363057	394.028131	7.449626
5.484794	394.639004	7.454630
5.472528	394.062493	7.459635
5.126307	381.260622	7.464640
5.380244	378.452620	7.469645
5.362800	395.294039	7.474650
5.415791	395.401099	7.479654
5.414513	404.023060	7.484659
5.672071	394.771896	7.489664
5.267509	395.696193	7.494669
5.386941	389.589219	7.499674
5.656616	394.206638	7.504678
5.518510	384.541130	7.509683
5.325973	377.251297	7.514688
5.553317	372.295794	7.519693
4.962407	381.142828	7.524698
5.296796	375.779007	7.529702
5.543949	389.313136	7.534707
5.246740	393.513288	7.539712
5.690726	401.749255	7.544717
5.348810	400.613037	7.549722
5.505872	388.546444	7.554726
5.435894	383.510707	7.559731
5.402747	373.407835	7.564736
5.399053	379.945947	7.569741
5.127875	371.190567	7.574746
5.352517	393.622661	7.579750
5.662763	405.695519	7.584755
5.230003	393.822467	7.589760
5.495691	393.951007	7.594765
5.542832	398.135365	7.599770
5.307530	373.633298	7.604774
5.194751	389.094224	7.609779
5.167419	398.579111	7.614784
5.424056	405.402130	7.619789
5.465642	412.259712	7.624794
5.589117	405.131449	7.629798
5.548148	405.284516	7.634803
5.460446	406.361967	7.639808
5.142920	398.906813	7.644813
5.339019	400.446806	7.649818
5.477577	395.993072	7.654822
5.629667	409.010020	7.659827
5.539971	408.323637	7.664832
5.351264	384.381538	7.669837
5.302786	380.594508	7.674842
5.597749	387.742669	7.679846
5.531037	384.460094	7.684851
5.365941	385.054113	7.689856
5.156132	380.321832	7.694861
5.154458	400.711853	7.699866
5.088237	400.514113	7.704870
5.161993	406.813811	7.709875
5.319699	405.577580	7.714880
5.434247	409.422768	7.719885
5.040743	411.781227	7.724890
5.133292	400.775165	7.729894
5.392186	406.730329	7.734899
5.423121	412.493294	7.739904
5.480982	403.946252	7.744909
5.172984	411.729221	7.749914
5.685872	406.829649	7.754918
5.652735	409.794016	7.759923
5.599296	416.077365	7.764928
5.804696	404.801928	7.769933
5.484284	406.185643	7.774938
5.500120	400.682953	7.779942
5.384760	411.756809	7.784947
5.290118	408.991150	7.789952
5.601705	403.396480	7.794957
5.435464	411.787948	7.799962
5.330328	413.113781	7.804966
5.203962	411.187525	7.809971
5.588539	405.410424	7.814976
5.930538	400.964314	7.819981
5.511553	396.617853	7.824986
5.130121	380.048417	7.829990
4.905934	389.761379	7.834995
5.494882	399.172250	7.840000
5.376308	403.309166	7.845005
5.138459	408.194663	7.850010
5.762988	397.839987	7.855014
5.711267	415.240054	7.860019
5.632594	404.552530	7.865024
5.320941	389.474184	7.870029
5.443374	389.349084	7.875034
5.369970	374.508013	7.880038
5.334690	393.163522	7.885043
5.463658	396.539616	7.890048
5.605630	383.085713	7.895053
5.269018	379.976068	7.900058
5.468778	379.161458	7.905062
5.504714	373.199201	7.910067
5.229704	372.484026	7.915072
5.362885	374.583259	7.920077
4.956182	387.049166	7.925082
5.494193	392.267068	7.930086
5.314148	406.575909	7.935091
5.499882	410.100438	7.940096
5.518399	409.470068	7.945101
5.498600	408.500339	7.950106
5.447654	403.666659	7.955110
5.459039	404.588717	7.960115
5.352592	406.306672	7.965120
5.266953	404.258800	7.970125
5.226164	405.036092	7.975142
5.277883	402.411060	7.980160
5.073991	411.181702	7.985178
5.188228	411.227308	7.990195
5.860228	408.041940	7.995213
5.491619	404.434122	8.000230
5.788540	406.185803	8.005248
5.358588	414.360423	8.010266
5.420966	417.865287	8.015283
5.269259	410.905803	8.020301
5.332914	410.885021	8.025318
5.530361	399.118183	8.030336
5.737058	416.625797	8.035354
5.243360	416.669112	8.040371
5.408090	408.641781	8.045389
5.093524	412.271692	8.050406
5.482564	413.537638	8.055424
5.521787	409.158559	8.060442
5.365244	415.891419	8.065459
5.412254	413.717911	8.070477
5.269083	416.741440	8.075494
5.446474	407.036582	8.080512
5.399490	415.189277	8.085530
5.276572	404.713944	8.090547
5.276289	407.993222	8.095565
5.230034	413.132318	8.100582
5.502368	412.349759	8.105600
5.468864	418.858450	8.110618
5.543159	433.588960	8.115635
5.404473	430.771578	8.120653
5.227504	446.173918	8.125670
5.546232	440.983488	8.130688
5.557555	444.821026	8.135706
5.599458	444.974118	8.140723
5.689707	436.168285	8.145741
5.927316	437.394645	8.150758
6.095067	442.932783	8.155776
5.481161	425.225002	8.160794
5.470479	411.476413	8.165811
5.663703	408.337162	8.170829
5.466107	418.390294	8.175846
5.819901	416.088440	8.180864
5.506301	419.844360	8.185882
5.597301	423.270264	8.190899
5.479375	420.508876	8.195917
5.796666	427.363358	8.200934
5.825708	433.633926	8.205952
5.742668	417.164756	8.210970
5.694500	406.423087	8.215987
5.638130	400.469311	8.221005
5.353628	409.790501	8.226022
5.578432	416.731210	8.231040
5.671258	433.304321	8.236058
5.631539	435.542625	8.241075
5.992947	434.117763	8.246093
5.532879	435.085712	8.251110
5.748371	442.130922	8.256128
5.652809	437.313851	8.261146
5.136280	440.120729	8.266163
5.670104	433.678528	8.271181
5.383718	434.714056	8.276198
5.640380	429.669169	8.281216
5.714295	438.610362	8.286234
5.539469	445.036461	8.291251
5.542733	434.984384	8.296269
5.524843	439.477695	8.301286
5.822349	441.298174	8.306304
5.484747	443.862735	8.311322
5.564210	444.398917	8.316339
5.582329	440.801607	8.321357
5.518527	451.838722	8.326374
5.788561	445.948382	8.331392
5.903493	450.989840	8.336410
5.911115	456.614042	8.341427
6.210859	441.359248	8.346445
5.675106	449.738263	8.351462
5.718856	443.591076	8.356480
5.750760	440.434345	8.361498
5.683177	442.558199	8.366515
6.021154	435.575968	8.371533
5.826458	444.416549	8.376550
5.786400	448.440562	8.381568
5.720601	447.225865	8.386586
5.813877	457.069667	8.391603
5.859381	440.625952	8.396621
5.994439	445.729215	8.401638
6.033125	441.843672	8.406656
5.997032	442.089247	8.411674
5.810157	442.262060	8.416691
5.726520	442.611985	8.421709
5.684645	449.707653	8.426726
5.572707	444.874995	8.431744
6.162786	443.593406	8.436762
5.708087	452.975584	8.441779
5.856255	448.400648	8.446797
5.810670	454.114392	8.451814
6.036769	465.460384	8.456832
6.058095	457.959963	8.461850
5.598987	459.700907	8.466867
5.930432	466.434365	8.471885
5.943479	466.385384	8.476902
5.723288	470.569055	8.481920
5.918289	465.373791	8.486938
6.110846	480.435049	8.491955
6.395345	468.544645	8.496973
5.881671	458.429274	8.501990
6.053914	455.887932	8.507008
5.845896	449.901868	8.512026
5.887204	454.139109	8.517043
6.322474	454.431918	8.522061
5.834155	459.053814	8.527078
5.880420	459.282552	8.532096
6.123081	461.765629	8.537114
5.703416	461.672636	8.542131
5.861353	469.984981	8.547149
6.181318	472.152090	8.552166
6.364198	469.727864	8.557184
6.315068	457.580156	8.562202
5.958556	454.738744	8.567219
5.825980	438.206728	8.572237
5.758829	448.270674	8.577255
5.645371	467.066280	8.582272
6.065994	465.678812	8.587290
6.106849	461.691339	8.592307
6.228262	471.553700	8.597325
6.080053	477.754150	8.602343
6.167595	475.279634	8.607360
6.117980	475.005460	8.612378
6.164553	481.450479	8.617395
6.342392	466.931405	8.622413
5.976875	477.734068	8.627431
5.564364	469.665654	8.632448
5.876068	466.207516	8.637466
5.912437	477.291379	8.642483
5.805087	461.050984	8.647501
5.896604	472.286882	8.652519
6.170133	474.471946	8.657536
5.845778	472.241661	8.662554
6.109271	476.901384	8.667571
5.863711	469.231754	8.672589
6.050226	466.710673	8.677607
5.785740	475.304236	8.682624
6.283944	485.276206	8.687642
6.216815	499.125647	8.692659
6.374114	502.358676	8.697677
6.245588	493.058514	8.702695
6.216863	490.733229	8.707712
6.563943	476.325963	8.712730
6.118044	479.058122	8.717747
6.063492	469.077634	8.722765
6.159443	468.184835	8.727783
6.174996	467.521914	8.732800
6.025816	468.508264	8.737818
6.098960	492.941040	8.742835
6.161669	496.900745	8.747853
6.320310	501.918815	8.752871
6.288032	503.385886	8.757888
6.559221	495.430177	8.762906
6.393789	493.351214	8.767923
6.155638	472.227503	8.772941
6.206583	483.825828	8.777959
6.114467	497.338508	8.782976
6.359206	495.720650	8.787994
6.179504	504.121413	8.793011
6.160009	491.630989	8.798029
6.621764	502.085164	8.803047
6.253273	499.250853	8.808064
6.572315	500.909113	8.813082
6.331134	498.697872	8.818099
6.346252	494.556612	8.823117
6.274360	487.613351	8.828135
6.539714	496.773719	8.833152
6.367627	476.767458	8.838170
6.012148	474.270916	8.843187
6.256116	487.188605	8.848205
6.330482	493.536892	8.853223
6.188539	501.383595	8.858240
6.912818	500.474344	8.863258
6.568694	504.960880	8.868275
6.479797	477.949916	8.873293
6.229755	473.888557	8.878311
5.834310	484.521413	8.883328
5.991802	490.326603	8.888346
6.119221	495.862409	8.893363
6.540956	493.428791	8.898381
6.535187	497.062903	8.903399
6.133289	505.696248	8.908416
6.425448	500.024631	8.913434
6.403162	493.353411	8.918451
6.666613	495.849375	8.923469
6.463368	496.952183	8.928487
6.154595	508.670940	8.933504
6.441340	500.062704	8.938522
6.401580	499.497352	8.943539
6.540986	505.014833	8.948557
6.401308	501.152819	8.953575
6.494051	505.757867	8.958592
6.517084	498.854528	8.963610
6.331661	505.738866	8.968627
6.417600	500.282610	8.973645
6.671797	507.567851	8.978663
6.154642	503.680791	8.983680
6.600896	505.156112	8.988698
6.557073	509.792717	8.993715
6.554464	504.500376	8.998733
6.508566	496.365304	9.003751
6.821601	506.488920	9.008768
6.798124	507.671288	9.013786
6.502001	506.269890	9.018803
6.695502	509.078438	9.023821
6.729252	503.441897	9.028839
6.621098	504.652707	9.033856
6.856777	508.804512	9.038874
6.382447	497.322075	9.043891
6.404449	501.846762	9.048909
6.960553	501.757318	9.053927
6.256224	507.420745	9.058944
6.633086	507.727790	9.063962
6.429720	506.149178	9.068979
6.762509	505.121353	9.073997
6.656461	504.414474	9.079015
6.924853	507.381031	9.084032
6.688278	503.284359	9.089050
6.797310	508.990140	9.094067
6.764575	509.557175	9.099085
6.942645	499.462223	9.104103
6.579700	508.276283	9.109120
6.737574	504.272498	9.114138
6.829994	509.366531	9.119155
6.554380	510.947663	9.124173
6.517292	509.198120	9.129191
6.682560	512.453053	9.134208
6.769040	512.543033	9.139226
6.646878	511.423911	9.144243
6.631554	498.343080	9.149261
6.865094	507.009380	9.154279
6.685305	504.082685	9.159296
6.976772	501.051878	9.164314
6.582157	509.789517	9.169331
6.869953	511.364792	9.174349
6.894308	506.595871	9.179367
6.752008	515.618711	9.184384
6.705324	506.128970	9.189402
6.796221	497.298194	9.194419
6.673481	505.330469	9.199437
6.931255	502.106068	9.204455
6.870437	500.663197	9.209472
6.805185	506.893962	9.214490
6.441718	504.085780	9.219507
6.570951	503.372273	9.224525
6.904380	504.876976	9.229543
6.835039	508.389779	9.234560
6.499373	503.245110	9.239578
6.481488	499.455364	9.244595
6.296614	521.421859	9.249613
6.859776	520.822824	9.254631
6.869632	531.337958	9.259648
7.353101	531.175358	9.264666
7.046027	526.631187	9.269683
6.935691	511.412794	9.274701
7.035896	505.985658	9.279719
6.890585	500.473555	9.284736
6.757333	497.697379	9.289754
6.779202	504.651191	9.294771
6.961361	512.869187	9.299789
7.011002	520.714171	9.304807
6.817699	522.667611	9.309824
6.946296	522.283903	9.314842
6.634940	528.047754	9.319859
6.758814	533.545584	9.324877
7.137651	532.452824	9.329895
7.073989	542.003504	9.334912
7.241747	526.844769	9.339930
7.341427	535.261705	9.344947
7.254676	513.910429	9.349965
7.246231	512.368310	9.354983
6.683070	499.249020	9.360000
6.765397	502.766531	9.365018
6.690635	503.672411	9.370035
6.911598	527.575011	9.375053
7.128034	527.781370	9.380071
7.131931	533.957940	9.385088
7.003776	524.412838	9.390106
7.086277	526.075972	9.395123
6.852825	531.251535	9.400141
7.222309	529.052166	9.405159
7.020315	533.034422	9.410176
6.986265	536.549633	9.415194
7.154120	530.790801	9.420211
6.934845	543.450328	9.425229
7.101078	534.422380	9.430247
7.032231	523.818700	9.435264
6.956710	530.648959	9.440282
7.200386	530.641756	9.445299
6.979007	542.033836	9.450317
7.086993	529.271822	9.455335
7.335885	533.776129	9.460352
7.176569	530.066767	9.465370
7.216138	528.983158	9.470387
7.102625	531.628981	9.475405
7.046983	531.891388	9.480423
6.961418	533.569269	9.485440
7.131972	534.862486	9.490458
7.227282	543.535641	9.495475
7.007638	538.612008	9.500493
7.274370	539.638869	9.505511
7.142313	536.324151	9.510528
7.022840	534.631602	9.515546
7.138972	542.311623	9.520563
7.146196	538.036440	9.525581
7.270363	529.721720	9.530599
6.943721	540.503597	9.535616
7.110088	532.863492	9.540634
7.123475	531.344512	9.545651
7.098071	535.763123	9.550669
7.235378	533.004367	9.555687
6.711269	539.650750	9.560704
7.086649	542.522373	9.565722
7.572280	556.909854	9.570739
7.375430	559.461865	9.575757
7.817173	555.046548	9.580775
7.463572	548.107961	9.585792
7.370051	548.790013	9.590810
7.035519	533.012067	9.595827
7.133940	537.290621	9.600845
7.248299	531.742236	9.605863
7.190827	544.008172	9.610880
7.695972	551.109807	9.615898
7.666781	547.898845	9.620915
7.431435	550.849146	9.625933
7.540534	540.858732	9.630951
7.344245	537.469068	9.635968
7.522769	540.054936	9.640986
7.312131	539.627620	9.646003
7.217720	536.564889	9.651021
7.136482	536.779588	9.656039
7.046560	535.191959	9.661056
7.376975	554.950217	9.666074
7.856854	556.091638	9.671091
7.761619	546.001928	9.676109
7.473480	529.954683	9.681127
7.396715	546.307701	9.686144
7.194153	536.189187	9.691162
7.528543	538.148416	9.696179
7.200388	542.628963	9.701197
7.206111	529.805213	9.706215
7.439577	549.087300	9.711232
7.492910	567.252997	9.716250
7.793348	564.318316	9.721267
7.344523	566.705338	9.726285
7.407080	558.800414	9.731303
7.600120	553.715672	9.736320
7.409125	557.263272	9.741338
7.616571	564.090802	9.746355
7.647546	568.070366	9.751373
7.701967	564.216426	9.756391
7.197338	552.486250	9.761408
7.359170	563.812093	9.766426
7.606477	564.033990	9.771443
7.536579	569.664031	9.776461
7.794485	559.556163	9.781479
7.710807	559.647066	9.786496
7.555575	567.574941	9.791514
7.993676	558.174460	9.796531
7.283306	560.570507	9.801549
7.455390	557.317427	9.806567
7.698138	565.402755	9.811584
7.730543	569.443493	9.816602
7.973120	559.327545	9.821619
7.457902	551.862325	9.826637
7.482316	554.005546	9.831655
7.699438	559.221375	9.836672
7.568880	558.410901	9.841690
7.696773	568.323423	9.846707
7.702417	575.353185	9.851725
7.927754	559.211511	9.856743
8.092646	566.537998	9.861760
7.645499	552.057178	9.866778
7.656120	533.404404	9.871795
7.463703	531.149623	9.876813
7.769859	545.651169	9.881831
8.006546	557.191513	9.886848
7.690280	545.882749	9.891866
7.561269	536.362190	9.896883
7.641763	563.345195	9.901901
7.461196	564.143478	9.906919
7.583565	566.512129	9.911936
7.641130	563.624902	9.916954
8.159490	565.664964	9.921971
7.870468	568.778507	9.926989
7.892050	564.073016	9.932007
7.969830	573.526591	9.937024
7.707858	571.939801	9.942042
7.637817	566.010870	9.947059
7.655134	567.131546	9.952077
7.699088	570.224781	9.957095
7.764976	561.093034	9.962112
7.687574	567.589598	9.967130
8.162755	562.162710	9.972147
7.795162	575.787184	9.977165
7.821961	566.996940	9.982183
7.864590	562.867820	9.987200
7.599929	566.629617	9.992218
7.651948	560.368814	9.997235
7.563993	567.258828	10.002253
7.445522	563.411580	10.007271
7.697004	573.221681	10.012288
7.682270	589.484520	10.017306
7.894095	589.676885	10.022323
7.967297	601.291478	10.027341
8.257533	595.354815	10.032359
8.063022	589.587496	10.037376
7.771188	580.093579	10.042394
7.901449	577.188755	10.047411
7.821805	589.628476	10.052429
8.012385	597.501644	10.057447
7.769604	595.166650	10.062464
7.790654	599.861785	10.067482
8.068571	601.767619	10.072499
7.974562	603.824830	10.077517
7.919804	602.430938	10.082535
8.022007	599.069397	10.087552
7.928634	607.483030	10.092570
8.133845	589.369449	10.097587
8.054571	605.067493	10.102605
7.934826	594.556469	10.107623
8.260514	598.563034	10.112640
8.235015	595.487263	10.117658
8.144785	600.730768	10.122675
8.341241	602.566291	10.127693
8.282796	609.941534	10.132711
8.266707	592.608367	10.137728
8.162577	599.496754	10.142746
8.165395	596.804037	10.147763
8.412870	604.730148	10.152781
7.673993	593.023917	10.157799
8.128900	594.763533	10.162816
8.255975	606.870904	10.167834
7.962678	595.136473	10.172851
8.206764	601.512692	10.177869
8.220140	601.603211	10.182887
8.387677	601.103786	10.187904
7.851796	604.891185	10.192922
8.501987	602.300691	10.197939
8.531828	594.949169	10.202957
7.947150	599.783365	10.207975
7.890967	593.226388	10.212992
7.953735	597.096747	10.218010
8.075227	600.476681	10.223027
7.964885	595.134307	10.228045
7.977824	598.750177	10.233063
8.108349	602.129397	10.238080
7.633094	601.908055	10.243098
7.934995	602.805267	10.248115
8.106929	622.379931	10.253133
8.389109	629.286399	10.258151
8.575332	624.345668	10.263168
8.460826	627.857738	10.268186
8.506251	622.675473	10.273203
8.522823	610.602544	10.278221
8.431122	607.889317	10.283239
8.649575	593.584221	10.288256
8.242982	597.866028	10.293274
8.392576	598.453348	10.298291
8.209581	592.106212	10.303309
8.029584	602.543707	10.308327
8.168811	605.788029	10.313344
8.605986	629.303896	10.318362
8.522341	613.747531	10.323379
8.524350	605.914451	10.328397
8.156055	601.185569	10.333415
8.382227	604.468584	10.338432
8.558644	619.160843	10.343450
8.516946	620.894428	10.348467
8.469749	620.457463	10.353485
8.252953	614.397210	10.358503
8.727262	616.024559	10.363520
8.249926	615.772857	10.368538
8.473975	617.496521	10.373555
8.878704	630.652745	10.378573
8.547042	616.888432	10.383591
8.326695	599.976969	10.388608
8.554567	605.777197	10.393626
8.466717	605.185979	10.398643
8.297291	605.335422	10.403661
8.023293	624.834418	10.408679
8.383325	632.504848	10.413696
8.647373	626.779791	10.418714
8.594009	626.456439	10.423731
8.419154	632.285429	10.428749
8.447824	634.982629	10.433767
8.553867	633.761007	10.438784
8.569246	636.545056	10.443802
8.613964	636.571709	10.448819
8.754281	636.892288	10.453837
8.474444	642.319671	10.458855
9.008097	625.968035	10.463872
8.550117	636.490336	10.468890
8.553558	638.901402	10.473907
8.795671	624.396691	10.478925
8.567190	629.040011	10.483943
8.862340	622.980287	10.488960
8.442049	631.781706	10.493978
8.768939	629.511062	10.498995
8.735290	626.052618	10.504013
8.751811	618.831043	10.509031
8.663292	628.802013	10.514048
8.758083	621.075148	10.519066
8.701447	625.071650	10.524083
8.744936	610.727514	10.529101
8.685316	628.794943	10.534119
8.978549	622.775298	10.539136
8.857316	629.476596	10.544154
9.013548	625.418333	10.549171
9.122258	616.654601	10.554189
8.550788	626.299970	10.559207
8.760543	624.856207	10.564224
8.878448	621.575705	10.569242
8.489045	624.955725	10.574259
8.974820	628.627449	10.579277
8.985897	628.062304	10.584295
8.907307	627.445139	10.589312
8.695424	626.036420	10.594330
8.960591	629.120850	10.599347
9.203166	619.328654	10.604365
8.799461	621.140911	10.609383
8.789488	621.594925	10.614400
8.997165	625.210124	10.619418
8.992341	630.913222	10.624435
8.955026	620.277072	10.629453
8.934104	621.724945	10.634471
8.949349	622.484190	10.639488
8.775861	634.834238	10.644506
8.751439	618.986946	10.649523
8.712839	623.028477	10.654541
8.448677	626.668956	10.659559
8.520525	625.695320	10.664576
8.806043	627.543993	10.669594
8.510441	620.891770	10.674611
8.751641	636.098822	10.679629
8.785926	646.841647	10.684647
9.010981	654.681361	10.689664
9.145311	651.661093	10.694682
8.950859	656.942411	10.699699
9.068317	651.475548	10.704717
9.159977	657.086445	10.709735
9.202316	651.488183	10.714752
9.084566	660.550723	10.719770
8.850426	651.169210	10.724787
9.345925	653.477235	10.729805
9.429835	649.504996	10.734823
8.970618	629.752542	10.739840
9.269582	626.827739	10.744858
8.960048	637.146052	10.749875
9.085686	625.969078	10.754893
8.932568	624.325414	10.759911
9.095577	640.235958	10.764928
9.122726	654.788113	10.769946
9.372512	656.986204	10.774963
8.935076	655.477975	10.779981
8.973418	654.025301	10.784999
9.091054	658.474302	10.790016
9.484395	652.602166	10.795034
9.080281	656.624741	10.800051
9.413428	651.560968	10.805069
9.442653	657.875491	10.810087
9.729262	644.387295	10.815104
9.507765	640.992941	10.820122
8.890243	632.563077	10.825139
9.148553	620.892245	10.830157
8.987209	625.982042	10.835175
9.131551	640.893807	10.840192
8.794872	654.782481	10.845210
9.109164	661.416719	10.850227
9.340481	659.769779	10.855245
9.255717	664.369736	10.860263
9.334295	665.611327	10.865280
9.030753	667.805333	10.870298
9.167384	665.118314	10.875315
9.377661	660.655423	10.880333
9.213506	658.547488	10.885351
9.417344	661.294903	10.890368
9.554882	664.235409	10.895386
9.137654	671.577212	10.900403
9.568221	652.589950	10.905421
9.215368	662.337380	10.910439
9.335260	662.412950	10.915456
9.566158	660.446028	10.920474
9.309384	657.665356	10.925491
9.269803	662.557777	10.930509
9.146825	663.309685	10.935527
9.338527	664.710806	10.940544
9.471394	665.180643	10.945562
9.134630	663.918847	10.950579
9.416624	671.108805	10.955597
9.143754	680.939598	10.960615
9.609720	698.394596	10.965632
9.775716	694.821070	10.970650
9.916703	699.539604	10.975667
9.824645	681.133031	10.980685
9.326344	671.898355	10.985703
9.469193	657.243198	10.990720
9.480775	663.871259	10.995738
9.472623	673.024834	11.000755
10.002614	667.636039	11.005773
9.680423	664.344432	11.010791
9.529410	668.105473	11.015808
9.590338	657.575595	11.020826
9.421795	668.799353	11.025843
9.510176	669.193127	11.030861
9.674212	672.091636	11.035879
9.592432	667.713897	11.040896
9.459842	671.887589	11.045914
9.373201	679.968280	11.050931
9.827744	672.399294	11.055949
9.638244	694.367590	11.060967
9.911496	690.615424	11.065984
9.751687	693.060521	11.071002
9.507003	691.375774	11.076019
9.671446	686.654965	11.081037
9.636178	693.605170	11.086055
9.459275	684.710736	11.091072
9.743283	686.304964	11.096090
9.492468	699.003519	11.101107
9.969198	688.055129	11.106125
9.649204	688.755933	11.111143
9.691813	693.570141	11.116160
9.890012	688.311677	11.121178
9.979906	691.188657	11.126195
10.007522	691.346095	11.131213
10.032601	691.847233	11.136231
9.822947	689.923613	11.141248
10.201487	682.290292	11.146266
9.870137	680.779387	11.151283
10.285465	678.519429	11.156301
9.801387	667.467189	11.161319
9.762308	661.094726	11.166336
9.557949	653.696086	11.171354
9.676065	665.692600	11.176371
10.102055	678.469772	11.181389
10.119170	687.854175	11.186407
9.847912	668.185776	11.191424
10.014884	666.633775	11.196442
9.835920	679.641605	11.201459
9.839586	677.573090	11.206477
9.970269	689.309484	11.211495
9.777429	681.644568	11.216512
9.960555	677.262754	11.221530
9.803127	685.967171	11.226547
10.132045	683.174572	11.231565
10.250049	690.569144	11.236583
9.878817	683.598980	11.241600
9.946025	681.062461	11.246618
9.986618	688.612209	11.251635
10.094812	685.406334	11.256653
9.848178	686.039831	11.261671
10.219962	693.734517	11.266688
10.047771	687.885308	11.271706
10.264626	694.146811	11.276723
10.127487	691.526942	11.281741
10.099856	689.771083	11.286759
9.761893	688.096329	11.291776
10.148860	679.471533	11.296794
9.813440	681.900545	11.301811
10.007734	683.513621	11.306829
10.227317	678.003989	11.311847
9.924077	683.238836	11.316864
10.205943	674.074275	11.321882
9.995601	684.650913	11.326899
10.065821	680.096148	11.331917
10.187419	685.227118	11.336935
10.033091	690.189600	11.341952
10.357111	686.225077	11.346970
10.038478	683.272019	11.351987
9.800599	691.964813	11.357005
10.241137	692.249076	11.362023
10.116008	708.034760	11.367040
10.662104	702.757441	11.372058
10.078641	704.784019	11.377075
10.301841	705.569722	11.382093
10.329326	714.201888	11.387111
10.357405	704.109293	11.392128
10.268417	694.419399	11.397146
10.164986	705.658935	11.402163
10.253156	714.330420	11.407181
10.586084	716.922148	11.412199
10.189385	718.619481	11.417216
10.367359	717.587455	11.422234
10.250170	720.707110	11.427251
10.697024	710.467551	11.432269
10.654649	710.680123	11.437287
10.242089	701.395551	11.442304
10.550872	694.099186	11.447322
10.269057	688.834095	11.452339
10.107506	700.603126	11.457357
10.355507	711.238236	11.462375
10.300588	715.497448	11.467392
10.654007	708.368052	11.472410
10.633590	716.052353	11.477427
10.271426	702.026717	11.482445
10.735770	712.394786	11.487463
10.104030	719.453196	11.492480
10.492438	712.147918	11.497498
10.620912	719.274249	11.502515
10.360021	719.544792	11.507533
10.524495	708.411496	11.512551
10.512976	723.303778	11.517568
10.739320	714.553506	11.522586
10.268941	718.711116	11.527603
10.579860	710.725861	11.532621
10.457950	717.814483	11.537639
10.318741	718.011656	11.542656
10.803270	713.074855	11.547674
10.884042	706.539158	11.552691
10.709374	713.990456	11.557709
10.810543	711.561664	11.562727
10.537961	714.903390	11.567744
10.878639	716.894666	11.572762
10.546813	723.106443	11.577779
10.496262	716.928368	11.582797
10.429681	712.437666	11.587815
10.341814	723.012870	11.592832
10.547423	719.577428	11.597850
10.686132	722.018775	11.602867
10.570050	718.367335	11.607885
10.667351	726.255088	11.612903
10.765709	737.953195	11.617920
11.197953	726.298056	11.622938
10.928529	725.173279	11.627955
11.103785	718.393150	11.632973
11.063385	713.703821	11.637991
10.439282	711.736494	11.643008
10.753822	711.314986	11.648026
10.794490	713.341560	11.653043
10.820256	721.712226	11.658061
10.972849	706.301133	11.663079
10.915708	709.151574	11.668096
10.832641	715.636347	11.673114
10.867193	718.970920	11.678131
10.785929	711.583876	11.683149
10.955434	710.652069	11.688167
10.402361	715.649734	11.693184
10.884172	718.333243	11.698202
11.172064	737.281151	11.703219
11.037169	737.943712	11.708237
11.156887	743.058677	11.713255
10.972689	734.075079	11.718272
10.857130	715.625918	11.723290
10.819641	720.849872	11.728307
10.789979	738.722701	11.733325
11.348548	739.057420	11.738343
11.069407	741.196203	11.743360
11.232759	744.814861	11.748378
11.110832	731.239781	11.753395
10.911582	720.552530	11.758413
11.088904	714.462162	11.763431
10.790963	718.031904	11.768448
11.343391	727.989509	11.773466
11.257519	738.722844	11.778483
10.883887	725.838372	11.783501
11.163587	735.872215	11.788519
11.130414	739.330638	11.793536
11.193925	745.896761	11.798554
11.192579	739.646330	11.803571
11.081425	740.940525	11.808589
11.364962	744.207540	11.813607
10.822234	743.712983	11.818624
11.054120	747.574561	11.823642
11.270306	751.670031	11.828659
11.171138	750.082342	11.833677
11.050375	750.021745	11.838695
11.034868	746.447472	11.843712
10.752199	733.244355	11.848730
10.727193	756.793736	11.853747
11.119604	745.652053	11.858765
11.238560	742.692783	11.863783
11.063959	743.993783	11.868800
11.360646	741.341364	11.873818
10.917335	746.816622	11.878835
10.987802	758.440055	11.883853
11.329024	765.019275	11.888871
11.346203	776.535053	11.893888
11.654129	767.994599	11.898906
11.496524	777.283894	11.903923
11.404815	783.809892	11.908941
11.649395	768.438956	11.913959
11.504743	779.110441	11.918976
11.457050	771.783138	11.923994
11.169723	769.137829	11.929011
10.946643	778.641928	11.934029
11.760100	769.965091	11.939047
11.252561	769.944766	11.944064
11.446655	775.366056	11.949082
11.667017	773.133962	11.954099
11.373848	765.969895	11.959117
11.655606	769.705679	11.964135
11.544527	777.569830	11.969152
11.480190	769.679984	11.974170
11.486556	774.024687	11.979187
11.549223	778.050609	11.984205
11.737134	772.150963	11.989223
11.528692	775.708205	11.994240
11.556548	770.409528	11.999258
11.517335	777.608242	12.004275
11.200290	776.382132	12.009293
11.465841	780.800678	12.014311
11.599688	769.601765	12.019328
11.463359	770.526750	12.024346
11.567548	772.753388	12.029363
11.502679	774.580795	12.034381
11.744432	771.451515	12.039399
11.373537	776.061466	12.044416
11.341457	777.226979	12.049434
11.493914	786.848573	12.054451
11.695778	804.687129	12.059469
11.941409	807.139850	12.064487
11.773166	802.308369	12.069504
11.671636	800.480731	12.074522
11.826230	794.451586	12.079539
11.759173	800.549313	12.084557
12.081461	795.395180	12.089575
11.723934	790.571346	12.094592
11.987516	782.695488	12.099610
11.902693	773.377659	12.104627
11.627252	778.821483	12.109645
11.657269	775.024299	12.114663
12.004116	788.679611	12.119680
12.282862	782.337928	12.124698
11.726895	786.301726	12.129715
11.533317	772.748361	12.134733
12.210379	788.351389	12.139751
11.899663	778.489060	12.144768
11.848472	779.008980	12.149786
11.994273	779.937462	12.154803
11.932945	792.314070	12.159821
12.063817	787.532870	12.164839
11.979744	787.265008	12.169856
11.672496	774.695815	12.174874
11.986246	789.160700	12.179891
11.930197	807.226562	12.184909
12.222511	811.520206	12.189927
12.187007	806.415498	12.194944
12.138436	801.055110	12.199962
12.104232	786.340486	12.204979
11.611474	792.251701	12.209997
12.333641	789.168149	12.215015
11.946957	807.831445	12.220032
12.022350	809.764471	12.225050
12.314025	800.702134	12.230067
12.185830	807.126931	12.235085
12.398769	806.595152	12.240103
12.400323	794.358250	12.245120
11.981950	784.643721	12.250138
12.014250	781.206561	12.255155
12.397680	797.365058	12.260173
12.313108	780.345206	12.265191
11.857202	788.031261	12.270208
11.893040	789.736035	12.275226
12.273725	797.003539	12.280243
12.269075	800.214733	12.285261
12.215746	796.014892	12.290279
12.259889	793.095604	12.295296
12.384955	808.888818	12.300314
12.029106	799.930957	12.305331
12.065537	805.831775	12.310349
12.199996	801.663314	12.315367
12.651735	812.040238	12.320384
12.741136	802.615880	12.325402
12.879685	807.213011	12.330419
12.561535	802.565489	12.335437
12.361185	791.632327	12.340455
12.601471	779.904731	12.345472
12.033090	778.485964	12.350490
12.412270	780.710988	12.355507
12.040250	799.755665	12.360525
12.289512	799.254855	12.365543
12.398798	803.625764	12.370560
11.953411	805.877417	12.375578
12.102430	803.521558	12.380595
12.109109	809.937520	12.385613
12.212738	795.825128	12.390631
12.167295	801.641726	12.395648
12.413001	810.347509	12.400666
12.809646	819.534276	12.405683
12.592208	816.348837	12.410701
12.743129	808.883002	12.415719
12.493752	816.850075	12.420736
12.337894	802.801670	12.425754
12.826634	801.998281	12.430771
12.690790	810.780473	12.435789
12.471472	798.984381	12.440807
12.662319	810.281963	12.445824
12.191638	813.615891	12.450842
12.690318	811.436541	12.455859
12.761887	819.482545	12.460877
12.619349	827.904075	12.465895
12.817774	819.124333	12.470912
12.880115	817.916259	12.475930
13.095279	813.060022	12.480947
12.710542	810.627731	12.485965
12.728773	802.087578	12.490983
12.682999	802.993577	12.496000
12.727117	808.387054	12.501018
12.643564	795.871208	12.506035
12.878041	803.131325	12.511053
12.630199	811.318793	12.516071
12.975779	823.712827	12.521088
12.574533	823.059132	12.526106
13.171413	811.511004	12.531123
12.885494	812.137060	12.536141
13.033839	800.936108	12.541159
13.171516	800.170007	12.546176
12.924334	794.306058	12.551194
12.787197	801.546451	12.556211
12.691915	795.661978	12.561229
12.875746	794.989577	12.566247
13.043174	801.664820	12.571264
12.888438	815.518082	12.576282
12.731799	820.157981	12.581299
12.983139	827.331849	12.586317
13.017772	820.997459	12.591335
13.244706	818.678053	12.596352
13.002905	821.849540	12.601370
13.281768	829.019818	12.606387
12.921098	809.857009	12.611405
13.096229	819.820104	12.616423
13.221163	806.849549	12.621440
12.881803	816.194271	12.626458
13.448842	806.252760	12.631475
12.868781	807.249137	12.636493
12.960821	813.560960	12.641511
13.474903	821.471018	12.646528
12.983854	814.601018	12.651546
13.212534	821.732590	12.656563
13.012652	807.860383	12.661581
13.188267	815.501522	12.666599
13.344902	811.155370	12.671616
13.349782	815.843220	12.676634
13.419927	812.040144	12.681651
12.569858	807.714871	12.686669
13.101937	811.907841	12.691687
13.279638	805.883905	12.696704
13.721018	810.635020	12.701722
13.369219	813.678933	12.706739
13.250503	817.517312	12.711757
13.683210	807.080843	12.716775
13.102367	812.443166	12.721792
13.146381	806.535734	12.726810
13.527362	816.222702	12.731827
13.378724	814.787313	12.736845
13.251183	814.171781	12.741863
13.447092	816.846335	12.746880
13.242751	819.916327	12.751898
13.278565	822.295271	12.756915
13.473273	823.287079	12.761933
12.975861	820.647743	12.766951
13.043865	808.948563	12.771968
12.864433	827.116249	12.776986
13.353486	811.835335	12.782003
13.432631	816.677364	12.787021
13.104801	816.507886	12.792039
13.421764	825.156169	12.797056
13.363988	835.652045	12.802074
13.731651	846.737994	12.807091
13.992876	836.390633	12.812109
13.820181	840.847591	12.817127
13.816048	830.862622	12.822144
13.288119	827.350470	12.827162
13.526961	816.537979	12.832179
13.599419	820.691212	12.837197
13.872220	812.538040	12.842215
13.895735	816.682282	12.847232
13.675049	819.689247	12.852250
13.736074	812.517268	12.857267
13.585312	810.479521	12.862285
13.558772	814.072871	12.867303
13.855356	812.537500	12.872320
13.716737	820.113162	12.877338
13.722231	815.594113	12.882355
13.616449	810.339286	12.887373
13.582492	820.076524	12.892391
13.810326	821.170102	12.897408
13.592455	841.556431	12.902426
13.393139	841.788003	12.907443
13.588963	852.866104	12.912461
13.361992	848.208924	12.917479
14.034745	844.568655	12.922496
13.696757	847.375060	12.927514
13.746535	847.058180	12.932531
13.724499	846.691627	12.937549
13.654613	853.573845	12.942567
14.021004	839.214801	12.947584
13.812843	850.618295	12.952602
13.847754	844.498007	12.957619
13.880209	840.826573	12.962637
13.718963	844.806860	12.967655
14.052404	846.950920	12.972672
14.215195	861.608275	12.977690
14.236219	846.927521	12.982707
14.328626	836.132269	12.987725
13.914565	842.795329	12.992743
14.048125	839.355892	12.997760
13.865003	851.653978	13.002778
14.171591	838.145366	13.007795
14.061214	836.668382	13.012813
14.154687	839.536134	13.017831
14.236179	835.412095	13.022848
14.302967	835.742341	13.027866
14.275013	840.204570	13.032883
14.491482	841.012067	13.037901
14.138840	841.192948	13.042919
14.320147	838.937811	13.047936
14.162395	841.761893	13.052954
14.275176	842.431320	13.057971
14.138547	834.894376	13.062989
13.932374	850.288587	13.068007
14.064060	831.226383	13.073024
14.057804	846.419658	13.078042
14.143455	849.681400	13.083059
14.509687	863.256397	13.088077
14.405791	866.602202	13.093095
14.485373	854.868191	13.098112
14.151319	851.077173	13.103130
14.027539	852.718726	13.108147
14.548497	854.990664	13.113165
14.257972	863.866110	13.118183
14.588858	867.018794	13.123200
14.480151	868.422820	13.128218
14.558696	863.034000	13.133235
14.514742	868.821243	13.138253
14.256292	860.609308	13.143271
14.229475	860.485068	13.148288
14.460909	857.716908	13.153306
14.769932	869.485604	13.158323
15.156469	860.574186	13.163341
14.988254	854.739605	13.168359
14.820661	835.550184	13.173376
14.717128	834.526359	13.178394
14.358806	842.994392	13.183411
14.455409	836.663671	13.188429
14.354226	833.670505	13.193447
14.525080	829.109205	13.198464
14.393743	841.565790	13.203482
14.237470	837.692475	13.208499
14.399531	845.816949	13.213517
14.446433	847.948009	13.218535
14.487082	860.827369	13.223552
14.663405	860.075707	13.228570
14.865281	855.621243	13.233587
14.698338	851.998498	13.238605
14.462208	867.899638	13.243623
14.953632	852.216350	13.248640
14.716952	853.989849	13.253658
14.708256	863.967780	13.258675
14.924714	857.154761	13.263693
14.714336	863.957191	13.268711
14.872735	854.078255	13.273728
14.525168	852.616087	13.278746
14.826984	855.251196	13.283763
14.955902	859.164954	13.288781
14.632632	854.310014	13.293799
14.499519	861.499966	13.298816
14.815530	861.724818	13.303834
14.748348	863.873267	13.308851
15.124679	875.199709	13.313869
15.164471	877.281761	13.318887
15.040728	865.498077	13.323904
14.838035	861.294503	13.328922
14.858920	859.238062	13.333939
14.862294	869.389175	13.338957
14.924286	882.715761	13.343975
15.542836	879.725393	13.348992
15.418158	876.361151	13.354010
15.152112	861.831632	13.359027
15.010359	856.010958	13.364045
14.820991	857.400046	13.369063
14.714797	869.000960	13.374080
15.168692	878.986654	13.379098
15.211480	877.802690	13.384115
15.775834	881.173050	13.389133
14.853427	882.345615	13.394151
15.213123	887.047343	13.399168
15.337752	882.179756	13.404186
15.520186	882.674627	13.409203
15.324509	869.750024	13.414221
15.186040	861.498463	13.419239
15.053228	847.223172	13.424256
15.332434	869.474614	13.429274
15.262002	884.822677	13.434291
15.478405	885.413864	13.439309
15.116782	883.284588	13.444327
15.285022	878.228664	13.449344
15.337217	886.982599	13.454362
15.579040	892.349150	13.459379
15.790434	883.978407	13.464397
15.538151	875.333973	13.469415
15.187444	855.391159	13.474432
14.907185	858.577509	13.479450
15.102567	877.968102	13.484467
15.724065	872.103629	13.489485
15.485154	878.848214	13.494503
15.503583	884.651471	13.499520
15.598314	892.298218	13.504538
15.512532	888.568674	13.509555
15.603762	887.198521	13.514573
15.537692	886.068473	13.519591
15.793284	884.578882	13.524608
15.492452	879.147607	13.529626
15.468797	895.238640	13.534643
15.566191	881.663587	13.539661
15.581988	885.406796	13.544679
15.541523	886.861879	13.549696
15.556273	878.822621	13.554714
15.090288	884.577660	13.559731
15.659913	879.323536	13.564749
15.466506	882.692883	13.569767
15.240054	877.563397	13.574784
15.708216	882.486645	13.579802
15.638376	889.297419	13.584819
15.725996	894.350647	13.589837
15.441474	907.178588	13.594855
16.255898	905.027647	13.599872
16.328273	899.439459	13.604890
16.109923	880.441083	13.609907
16.004406	873.509339	13.614925
15.703536	884.049391	13.619943
15.753409	875.949576	13.624960
15.994669	868.165175	13.629978
16.122999	881.563997	13.634995
16.404649	863.192724	13.640013
16.314396	870.375360	13.645031
15.989743	865.702916	13.650048
16.263937	859.583006	13.655066
15.825704	873.896992	13.660083
15.996055	869.145424	13.665101
15.883453	875.494828	13.670119
16.018089	868.199572	13.675136
15.878105	861.288325	13.680154
15.853824	871.642644	13.685171
15.984908	863.362814	13.690189
15.756177	871.870737	13.695207
16.080616	862.512978	13.700224
15.901132	856.882420	13.705242
16.118703	879.578736	13.710259
16.362763	883.466866	13.715277
16.126983	880.054361	13.720295
16.282032	884.483431	13.725312
16.099211	875.631402	13.730330
16.048551	894.761553	13.735347
16.267507	893.077277	13.740365
16.449023	888.916718	13.745383
16.208165	897.018431	13.750400
16.315348	891.211483	13.755418
16.371433	888.978727	13.760435
16.353362	893.746000	13.765453
16.517940	893.285442	13.770471
16.411136	889.257641	13.775488
16.533952	873.452540	13.780506
16.228996	880.633073	13.785523
16.277336	871.355645	13.790541
16.235325	891.068171	13.795559
16.414633	896.619118	13.800576
16.389420	896.609367	13.805594
16.276451	897.465914	13.810611
16.677761	891.004019	13.815629
16.723680	897.491050	13.820647
16.551866	893.287059	13.825664
16.549337	894.876576	13.830682
16.641874	897.256142	13.835699
16.674536	896.453557	13.840717
16.672378	894.934763	13.845735
16.622390	894.903344	13.850752
16.517882	887.078378	13.855770
16.293376	900.641758	13.860787
16.666415	893.407647	13.865805
16.402367	894.945558	13.870823
16.708771	894.773807	13.875840
16.825043	890.155621	13.880858
16.345013	894.267837	13.885875
16.601989	891.637936	13.890893
16.699988	899.110534	13.895911
16.750042	893.283358	13.900928
16.972934	882.772270	13.905946
16.429077	891.601853	13.910963
16.675428	883.424499	13.915981
16.778753	883.146353	13.920999
16.706512	888.500935	13.926016
16.755054	888.785793	13.931034
16.914025	887.271318	13.936051
16.821649	882.392165	13.941069
16.706049	888.189749	13.946087
16.561397	887.713269	13.951104
16.993368	892.728751	13.956122
17.032638	911.199532	13.961139
17.531075	907.818717	13.966157
17.114696	900.156202	13.971175
16.987990	896.043328	13.976192
17.045004	878.716784	13.981210
16.604242	893.994527	13.986227
16.956815	883.393386	13.991245
17.098555	898.757180	13.996263
17.141100	911.311093	14.001280
17.636328	915.339953	14.006298
17.062310	901.109993	14.011315
16.783861	895.818879	14.016333
17.139959	896.429365	14.021351
17.247614	913.463487	14.026368
17.414994	907.803407	14.031386
17.083018	911.996131	14.036403
17.273091	903.465349	14.041421
17.075473	907.801477	14.046439
16.850522	918.536991	14.051456
17.324640	914.124461	14.056474
17.364073	914.523031	14.061491
17.299515	922.243509	14.066509
17.512005	913.170254	14.071527
17.450332	920.656803	14.076544
17.818135	919.449719	14.081562
17.463170	910.725094	14.086579
17.305635	890.616278	14.091597
17.304216	901.345334	14.096615
17.091409	913.734027	14.101632
17.531224	912.596465	14.106650
17.601079	918.785452	14.111667
17.270272	924.706214	14.116685
17.595004	920.321267	14.121703
17.340125	928.974502	14.126720
17.232702	912.832063	14.131738
17.218204	924.279992	14.136755
17.533938	924.616104	14.141773
17.545980	924.181685	14.146791
17.399474	929.696448	14.151808
17.567676	918.335626	14.156826
17.409799	923.572178	14.161843
17.221454	920.541911	14.166861
17.738354	911.788705	14.171879
17.627676	919.040699	14.176896
17.715405	916.928655	14.181914
17.547278	920.824481	14.186931
17.436514	929.162051	14.191949
17.699692	942.919983	14.196967
17.865798	949.378596	14.201984
17.868270	934.158161	14.207002
17.837885	948.988446	14.212019
17.769113	949.086912	14.217037
17.962755	947.246021	14.222055
17.861880	939.325943	14.227072
18.228087	936.719019	14.232090
18.144368	945.457390	14.237107
18.205482	923.193235	14.242125
17.964462	913.709759	14.247143
17.896887	912.949816	14.252160
17.921911	912.899434	14.257178
17.810818	909.638824	14.262195
17.624035	909.970866	14.267213
18.132948	934.329549	14.272231
17.955651	942.887619	14.277248
18.159392	941.342865	14.282266
18.149468	942.040959	14.287283
17.901891	942.176230	14.292301
18.415565	940.540989	14.297319
18.066439	935.383254	14.302336
18.584633	936.768715	14.307354
17.992254	920.112423	14.312371
18.194708	924.019289	14.317389
18.299881	925.717081	14.322407
18.161523	911.245224	14.327424
18.097890	915.335675	14.332442
18.286999	934.368153	14.337459
18.280375	926.882780	14.342477
18.242249	930.841641	14.347495
18.181096	934.356330	14.352512
18.319789	931.738602	14.357530
18.204387	942.009104	14.362547
18.017290	925.309853	14.367565
18.305735	926.568352	14.372583
18.285850	932.172694	14.377600
18.430447	931.114708	14.382618
18.204465	937.998499	14.387635
18.117486	928.440399	14.392653
18.310669	930.478461	14.397671
18.230683	936.745899	14.402688
18.443374	933.418281	14.407706
18.544656	931.779738	14.412723
18.260108	933.179928	14.417741
18.778304	941.248017	14.422759
18.783317	952.419120	14.427776
18.565723	937.681292	14.432794
18.657291	936.117981	14.437811
18.639007	939.297220	14.442829
19.011999	921.637026	14.447847
18.738353	930.391209	14.452864
18.933734	923.688546	14.457882
18.679378	921.997311	14.462899
18.833380	923.559830	14.467917
19.251653	920.370671	14.472935
18.625208	926.042560	14.477952
18.867649	919.976325	14.482970
18.827125	924.383979	14.487987
18.232001	920.480833	14.493005
18.674396	922.759541	14.498023
18.675106	926.125569	14.503040
18.761402	923.956482	14.508058
18.922336	929.021355	14.513075
18.599408	933.822579	14.518093
18.829831	948.511096	14.523111
19.133906	964.925266	14.528128
19.307568	954.843545	14.533146
19.150932	939.098995	14.538163
18.667676	930.262817	14.543181
19.017018	934.749169	14.548199
19.281639	946.324333	14.553216
19.154942	943.149966	14.558234
19.214345	933.345697	14.563251
18.919597	930.146117	14.568269
18.995135	923.587381	14.573287
19.127099	943.261807	14.578304
19.156249	953.193941	14.583322
19.064855	956.054648	14.588339
18.948770	963.220755	14.593357
19.247017	958.225476	14.598375
19.454810	958.501582	14.603392
19.543091	949.506033	14.608410
19.599606	953.945595	14.613427
19.161841	936.978958	14.618445
19.132310	931.096693	14.623463
18.836960	946.316858	14.628480
18.942596	953.360091	14.633498
19.329654	951.631334	14.638515
18.777018	961.973340	14.643533
19.311641	954.703092	14.648551
19.030904	964.014932	14.653568
18.813446	965.622661	14.658586
19.261341	965.617144	14.663603
19.609260	975.126452	14.668621
20.274185	963.330895	14.673639
20.042301	953.370513	14.678656
19.915030	938.970011	14.683674
20.062417	934.322429	14.688691
20.037527	942.735294	14.693709
20.160835	933.826839	14.698727
20.347276	936.216393	14.703744
19.906940	912.320161	14.708762
19.607461	890.503361	14.713779
19.908333	896.493521	14.718797
19.873699	898.661366	14.723815
19.583528	899.983950	14.728832
19.353006	907.696968	14.733850
19.424841	902.292518	14.738867
19.818018	914.212408	14.743885
19.659412	903.361002	14.748903
19.624678	912.365603	14.753920
19.694510	921.455186	14.758938
19.987592	931.290686	14.763955
19.919089	933.845440	14.768973
19.930003	937.348150	14.773991
20.085586	942.245227	14.779008
19.991465	926.637928	14.784026
19.869539	909.867235	14.789043
19.816017	919.962882	14.794061
20.210406	939.280124	14.799079
20.259166	935.414238	14.804096
19.526143	914.441262	14.809114
19.695088	919.146163	14.814131
20.162065	932.569250	14.819149
20.270859	939.285399	14.824167
20.155143	942.708771	14.829184
19.987137	949.920311	14.834202
20.338551	940.128916	14.839219
19.938257	948.510484	14.844237
20.226703	945.316917	14.849255
20.337798	950.458186	14.854272
19.903856	945.840691	14.859290
20.124280	939.711577	14.864307
19.973695	946.948367	14.869325
19.889030	944.704747	14.874343
19.992067	950.276855	14.879360
19.675376	951.673924	14.884378
20.288060	946.455728	14.889395
20.001502	954.399920	14.894413
20.375999	963.748909	14.899431
20.374864	975.003525	14.904448
20.465937	974.192803	14.909466
20.533680	976.261365	14.914483
20.113933	973.372298	14.919501
20.433643	974.695483	14.924519
20.553902	975.499885	14.929536
20.389506	972.466021	14.934554
20.870710	971.975471	14.939571
20.439510	970.521680	14.944589
20.727216	972.270630	14.949607
21.049008	972.668331	14.954624
20.815077	966.444656	14.959642
20.661450	960.144648	14.964659
20.475676	965.945657	14.969677
20.845742	967.686035	14.974695
20.747852	965.108805	14.979712
20.602430	965.156629	14.984730
20.650599	963.461364	14.989747
20.633690	969.649242	14.994765
20.603410	972.222647	14.999783
20.694521	976.765907	15.004800
20.476567	973.392541	15.009818
20.706719	961.437766	15.014835
20.675402	967.811097	15.019853
20.773686	967.216092	15.024871
20.679248	968.320335	15.029888
20.740579	971.510756	15.034906
21.195613	968.337327	15.039923
20.454768	971.622889	15.044941
20.592637	975.985554	15.049959
21.054441	986.108971	15.054976
20.986491	1000.875278	15.059994
21.272623	1001.826905	15.065011
21.356987	1013.411018	15.070029
21.273436	989.744128	15.075047
21.272990	986.585380	15.080064
21.209648	981.637594	15.085082
20.933400	973.320689	15.090099
20.877738	978.381619	15.095117
21.419966	993.977153	15.100135
21.261789	997.752848	15.105152
21.030060	998.059884	15.110170
21.366899	992.213744	15.115187
21.258908	1009.714889	15.120205
21.319495	1006.712124	15.125223
21.127634	1004.544970	15.130240
21.240864	1002.950691	15.135258
21.696948	1002.325741	15.140275
21.194931	1002.487161	15.145293
21.303482	1001.934146	15.150311
21.113141	1002.558692	15.155328
21.155335	998.455905	15.160346
21.632122	1001.795771	15.165363
21.140313	1003.680190	15.170381
21.583650	994.994477	15.175399
21.182004	1002.236015	15.180416
21.161294	997.948813	15.185434
21.532332	992.488697	15.190451
21.482777	999.438658	15.195469
21.498453	996.998836	15.200487
21.518197	993.808386	15.205504
21.466694	1012.939808	15.210522
22.014667	1020.471526	15.215539
21.762186	1020.386759	15.220557
21.539861	1021.087877	15.225575
21.786410	1018.670306	15.230592
21.878972	1024.516803	15.235610
22.120768	1009.883840	15.240627
21.778263	1008.687728	15.245645
21.617563	989.865252	15.250663
22.295658	1004.920532	15.255680
22.095285	1010.239368	15.260698
21.908024	999.827866	15.265715
21.546331	985.368848	15.270733
21.413277	1005.830267	15.275751
22.042721	997.510446	15.280768
21.924020	1022.008619	15.285786
22.117857	1018.924260	15.290803
22.063308	1026.754931	15.295821
22.135064	1020.835523	15.300839
22.277129	1022.025650	15.305856
22.215748	1024.293228	15.310874
22.408165	1012.856072	15.315891
21.954710	1005.963792	15.320909
21.856188	1003.707507	15.325927
21.834971	1021.833968	15.330944
22.033140	1017.914687	15.335962
22.284502	1019.347655	15.340979
22.250642	1020.660323	15.345997
21.981565	1028.850647	15.351015
22.603295	1019.490427	15.356032
21.895372	1025.405013	15.361050
21.968621	1016.269019	15.366067
22.067385	1027.043712	15.371085
21.931938	1020.570589	15.376103
21.990647	1030.918898	15.381120
22.127229	1046.464984	15.386138
22.534590	1034.994449	15.391155
22.782184	1045.955823	15.396173
22.688640	1046.978824	15.401191
22.985595	1048.725459	15.406208
22.523632	1031.166319	15.411226
22.722146	1025.452993	15.416243
22.601158	1010.442558	15.421261
22.699818	1012.144198	15.426279
22.470223	1005.711924	15.431296
22.521886	1017.822310	15.436314
22.750688	1023.515855	15.441331
22.874057	1025.660607	15.446349
22.692899	1024.145568	15.451367
22.594605	1011.356029	15.456384
22.645760	1035.376414	15.461402
22.983858	1036.539865	15.466419
23.003365	1035.299723	15.471437
22.410764	1018.637454	15.476455
22.845540	1036.933405	15.481472
22.792441	1034.927817	15.486490
22.833569	1050.268132	15.491507
22.821266	1038.654365	15.496525
22.641480	1043.655244	15.501543
23.200861	1034.225855	15.506560
22.649474	1043.291405	15.511578
22.662803	1037.086837	15.516595
22.806446	1047.665908	15.521613
22.970642	1043.974301	15.526631
23.127085	1032.612397	15.531648
22.787374	1047.869953	15.536666
22.838456	1042.398829	15.541683
22.985267	1044.994778	15.546701
22.563288	1055.345835	15.551719
23.188615	1059.636559	15.556736
23.633625	1065.931156	15.561754
23.641905	1048.277698	15.566771
23.580937	1049.917690	15.571789
23.467850	1038.850170	15.576807
23.476530	1032.369622	15.581824
23.282868	1037.703493	15.586842
23.575563	1032.854773	15.591859
23.393992	1032.920809	15.596877
23.307481	1033.790288	15.601895
23.227147	1030.394036	15.606912
23.401276	1032.663021	15.611930
23.196205	1041.277727	15.616947
23.346125	1035.025262	15.621965
23.407294	1037.189408	15.626983
23.473969	1032.602650	15.632000
23.448010	1050.910631	15.637018
23.678114	1057.497621	15.642035
23.921900	1054.178982	15.647053
23.404335	1047.966196	15.652071
23.803340	1050.432834	15.657088
23.521955	1053.394424	15.662106
23.646947	1052.443422	15.667123
23.922770	1062.336794	15.672141
23.700190	1052.914139	15.677159
24.025305	1056.244583	15.682176
23.789481	1045.242731	15.687194
23.621749	1038.025799	15.692211
23.854185	1035.988501	15.697229
24.046857	1067.141286	15.702247
24.061875	1051.375178	15.707264
23.960258	1047.756489	15.712282
23.635193	1029.997442	15.717299
23.796982	1048.099816	15.722317
23.886154	1057.492348	15.727335
24.174835	1055.544906	15.732352
24.038110	1055.781037	15.737370
23.903234	1050.988023	15.742387
24.238931	1063.432317	15.747405
24.225603	1067.694947	15.752423
24.506164	1050.356842	15.757440
24.120459	1063.039533	15.762458
24.030846	1056.194625	15.767475
24.239317	1065.321286	15.772493
24.169779	1070.077877	15.777511
24.271753	1067.396155	15.782528
24.114973	1066.503796	15.787546
24.076002	1062.827056	15.792563
24.220383	1067.833509	15.797581
24.072086	1066.822029	15.802599
24.127087	1057.323317	15.807616
24.190788	1063.289973	15.812634
24.036350	1065.536018	15.817651
24.081073	1060.467495	15.822669
24.047855	1070.357121	15.827687
24.240154	1073.745075	15.832704
24.564827	1090.478378	15.837722
24.744630	1083.196969	15.842739
24.784578	1089.821483	15.847757
24.796584	1072.571686	15.852775
24.815731	1066.146074	15.857792
24.507484	1067.150828	15.862810
24.308221	1058.049079	15.867827
24.574828	1072.040205	15.872845
24.672529	1084.428014	15.877863
24.988399	1086.488420	15.882880
24.786786	1083.175696	15.887898
24.727125	1076.787586	15.892915
24.795347	1068.265354	15.897933
24.931549	1077.388679	15.902951
24.951017	1063.792955	15.907968
24.587304	1063.843597	15.912986
24.771065	1075.076217	15.918003
24.893953	1086.227629	15.923021
25.035101	1084.990492	15.928039
25.131481	1083.464749	15.933056
25.028294	1083.497286	15.938074
24.956545	1090.967877	15.943091
25.049436	1083.903658	15.948109
25.043941	1083.620369	15.953127
25.008869	1081.675162	15.958144
25.134688	1092.842626	15.963162
25.069872	1090.444512	15.968179
25.232243	1084.427347	15.973197
25.148733	1086.798607	15.978215
25.121852	1083.901698	15.983232
25.080741	1075.191346	15.988250
24.918170	1084.664316	15.993267
25.125091	1078.951148	15.998285
24.977762	1082.837652	16.003303
25.185734	1074.576425	16.008320
25.502789	1083.119333	16.013338
25.026504	1081.837975	16.018355
25.170557	1082.567567	16.023373
25.098066	1096.890651	16.028391
25.204054	1098.315114	16.033408
25.787271	1106.578771	16.038426
25.425164	1108.014109	16.043443
25.685394	1107.158731	16.048461
25.706525	1110.461369	16.053479
25.890899	1101.348978	16.058496
25.857828	1107.512827	16.063514
25.540179	1099.839707	16.068531
25.462742	1093.644691	16.073549
25.945173	1113.918135	16.078567
26.118162	1099.137478	16.083584
26.065214	1087.032427	16.088602
25.949393	1086.152942	16.093619
25.924945	1090.392626	16.098637
25.711304	1084.294263	16.103655
25.661819	1084.131664	16.108672
25.793944	1074.921680	16.113690
25.649802	1080.663847	16.118707
25.908004	1072.378132	16.123725
25.597485	1096.874842	16.128743
26.071237	1099.102699	16.133760
26.537312	1103.414788	16.138778
26.225551	1093.184535	16.143795
26.415279	1081.373387	16.148813
25.866022	1077.645637	16.153831
25.645111	1078.424077	16.158848
26.021054	1090.058205	16.163866
26.019436	1101.725570	16.168883
26.307840	1106.570310	16.173901
25.753357	1111.716553	16.178919
25.903610	1106.554496	16.183936
26.101043	1095.481779	16.188954
25.873426	1101.645679	16.193971
26.327330	1099.885719	16.198989
25.752340	1109.683930	16.204007
25.943318	1107.117322	16.209024
26.066660	1108.351511	16.214042
26.475078	1131.582785	16.219059
26.784725	1121.112233	16.224077
26.903627	1127.481921	16.229095
26.833552	1103.127615	16.234112
26.731784	1085.730580	16.239130
26.813813	1086.849199	16.244147
26.849389	1086.729153	16.249165
26.773300	1091.859260	16.254183
26.875687	1087.600390	16.259200
26.774480	1087.814477	16.264218
26.664924	1100.678847	16.269235
27.019066	1086.776704	16.274253
26.569115	1090.472577	16.279271
26.825828	1093.993522	16.284288
26.700553	1087.702134	16.289306
26.613903	1095.464952	16.294323
26.989354	1086.837712	16.299341
26.688497	1095.420339	16.304359
26.682212	1085.510559	16.309376
27.001964	1089.334787	16.314394
26.638986	1086.036678	16.319411
26.835014	1089.827142	16.324429
26.616088	1090.460773	16.329447
26.606636	1087.577501	16.334464
27.092927	1094.048309	16.339482
27.258810	1114.864496	16.344499
27.069032	1112.715482	16.349517
27.092285	1103.253906	16.354535
27.101831	1113.605324	16.359552
27.369414	1114.027787	16.364570
27.250934	1115.902922	16.369587
27.108143	1101.132230	16.374605
27.091424	1108.623209	16.379623
27.160875	1117.977720	16.384640
27.603901	1116.789614	16.389658
27.428865	1118.088355	16.394675
27.514673	1121.757784	16.399693
27.510189	1119.306728	16.404711
27.120588	1120.692309	16.409728
27.464515	1124.178294	16.414746
27.350243	1123.496571	16.419763
27.393261	1112.737286	16.424781
27.334579	1124.599575	16.429799
27.173898	1121.019030	16.434816
27.721691	1115.801132	16.439834
27.391668	1123.368599	16.444851
27.488408	1118.433530	16.449869
27.493278	1120.908997	16.454887
27.450690	1116.345099	16.459904
27.516489	1122.318121	16.464922
27.414253	1115.496937	16.469939
27.842352	1126.421676	16.474957
27.775574	1140.363557	16.479975
27.612557	1139.368298	16.484992
28.036678	1137.220392	16.490010
28.238427	1135.529502	16.495027
28.255543	1140.141011	16.500045
28.390408	1123.280558	16.505063
27.808032	1111.470162	16.510080
27.721894	1106.360780	16.515098
27.875328	1111.979094	16.520115
28.036762	1113.117193	16.525133
27.798055	1120.162029	16.530151
27.884445	1125.180501	16.535168
27.915640	1128.832239	16.540186
27.884276	1128.589860	16.545203
27.822794	1126.231736	16.550221
27.935703	1121.947093	16.555239
27.924607	1132.058660	16.560256
27.956633	1122.038558	16.565274
28.131483	1138.182281	16.570291
27.999419	1141.220639	16.575309
28.173693	1143.913610	16.580327
28.207673	1143.982007	16.585344
29.060622	1142.764349	16.590362
28.936731	1160.793478	16.595379
28.806060	1133.387937	16.600397
28.973319	1117.105933	16.605415
28.889453	1128.926351	16.610432
28.705964	1113.424655	16.615450
28.584832	1120.270826	16.620467
28.795029	1121.378775	16.625485
28.535025	1110.713160	16.630503
28.508461	1116.249194	16.635520
28.875626	1115.407930	16.640538
28.745449	1114.948524	16.645555
28.587851	1117.837586	16.650573
28.981060	1120.829580	16.655591
28.578261	1124.698716	16.660608
28.559604	1109.022393	16.665626
28.631529	1112.718929	16.670643
28.271106	1121.143369	16.675661
28.820838	1137.821603	16.680679
28.914991	1147.311782	16.685696
29.047519	1148.000775	16.690714
28.912931	1149.130206	16.695731
29.070902	1146.284841	16.700749
29.224726	1145.585328	16.705767
29.002359	1149.516602	16.710784
29.051105	1144.722566	16.715802
29.476103	1153.348355	16.720819
29.139368	1152.617782	16.725837
29.160541	1140.578318	16.730855
28.983535	1151.543413	16.735872
28.986914	1148.318645	16.740890
28.867483	1157.362465	16.745907
29.300763	1148.346465	16.750925
29.410655	1141.630557	16.755943
29.317903	1152.271430	16.760960
29.604951	1144.216302	16.765978
29.060872	1151.409145	16.770995
29.467740	1137.210020	16.776013
29.443323	1137.581415	16.781031
29.185179	1145.742819	16.786048
29.724752	1156.172306	16.791066
29.708083	1161.676398	16.796083
29.819775	1160.829171	16.801101
29.922949	1157.607892	16.806119
29.491984	1145.258946	16.811136
29.679781	1142.744827	16.816154
29.903874	1158.134757	16.821171
29.745697	1150.120162	16.826189
30.030222	1157.986272	16.831207
29.517040	1154.016692	16.836224
30.236857	1156.202480	16.841242
29.924422	1146.345906	16.846259
30.014797	1141.506765	16.851277
29.866772	1137.528464	16.856295
29.740843	1139.546171	16.861312
29.900344	1140.431851	16.866330
29.485072	1158.738527	16.871347
29.903949	1161.043621	16.876365
30.246389	1158.833308	16.881383
30.070996	1162.259954	16.886400
30.364227	1164.575302	16.891418
30.160149	1161.486581	16.896435
30.058296	1163.949873	16.901453
30.233712	1166.825326	16.906471
30.235990	1165.269942	16.911488
30.424504	1163.261974	16.916506
30.182569	1164.369880	16.921523
30.292644	1158.332639	16.926541
30.339085	1152.893347	16.931559
30.316078	1163.226194	16.936576
30.440243	1158.122784	16.941594
30.355486	1169.382386	16.946611
29.839061	1163.321717	16.951629
30.501296	1154.389309	16.956647
30.211407	1167.034901	16.961664
30.371661	1184.288915	16.966682
30.734546	1184.846714	16.971699
30.873465	1208.004399	16.976717
30.510177	1194.340686	16.981735
30.726291	1189.033803	16.986752
30.675917	1193.399865	16.991770
30.741744	1196.786820	16.996787
30.706383	1187.638857	17.001805
31.067169	1190.103996	17.006823
30.952716	1184.280038	17.011840
30.833650	1194.678869	17.016858
30.846054	1193.378874	17.021875
30.689199	1188.771744	17.026893
31.132792	1182.282231	17.031911
30.825465	1178.372914	17.036928
31.064369	1171.959943	17.041946
31.110542	1179.341296	17.046963
31.299064	1177.642365	17.051981
31.215401	1178.329103	17.056999
31.115533	1184.150954	17.062016
31.095157	1176.808682	17.067034
31.343821	1179.166871	17.072051
31.261817	1187.527357	17.077069
31.384642	1179.362111	17.082087
31.275674	1179.871569	17.087104
31.308943	1179.110206	17.092122
31.162414	1181.777373	17.097139
31.386140	1178.626206	17.102157
31.324402	1175.061879	17.107175
31.050422	1183.337347	17.112192
31.216629	1195.074521	17.117210
31.725601	1203.809998	17.122227
31.544247	1196.847999	17.127245
31.755493	1193.506787	17.132263
31.423073	1210.106925	17.137280
31.560223	1200.611005	17.142298
31.825888	1199.176795	17.147315
32.170120	1204.124881	17.152333
32.305691	1200.843487	17.157351
31.734436	1197.311086	17.162368
32.161531	1193.538743	17.167386
32.223044	1189.774803	17.172403
31.757882	1179.250319	17.177421
32.137779	1174.092196	17.182439
31.887627	1173.639342	17.187456
31.729552	1166.740413	17.192474
31.682829	1182.764324	17.197491
32.075372	1199.191993	17.202509
32.300354	1192.548662	17.207527
32.033115	1202.705209	17.212544
31.928792	1197.448826	17.217562
32.112918	1201.137364	17.222579
32.120131	1194.014504	17.227597
32.110456	1194.652334	17.232615
32.142368	1194.991535	17.237632
32.155233	1198.086521	17.242650
32.290638	1195.374812	17.247667
31.960811	1189.580743	17.252685
32.374583	1193.261819	17.257703
32.300708	1189.942013	17.262720
32.197342	1191.193810	17.267738
32.680686	1212.023898	17.272755
32.366074	1213.098612	17.277773
32.725941	1217.280361	17.282791
32.660710	1216.142866	17.287808
32.682308	1205.369755	17.292826
32.894630	1215.043082	17.297843
32.380426	1209.107611	17.302861
32.745687	1211.801920	17.307879
32.451023	1227.856852	17.312896
32.643135	1228.358788	17.317914
32.770297	1224.130013	17.322931
32.854594	1222.772399	17.327949
33.018117	1215.022004	17.332967
32.513369	1233.594809	17.337984
32.617253	1214.020637	17.343002
32.774101	1221.476918	17.348019
32.587483	1221.533951	17.353037
32.942878	1226.124694	17.358055
32.743400	1231.977290	17.363072
32.981132	1241.671213	17.368090
33.242219	1237.307583	17.373107
33.156698	1249.084668	17.378125
33.180157	1248.543032	17.383143
33.416565	1236.049629	17.388160
33.189994	1244.114110	17.393178
33.193145	1240.280727	17.398195
33.363003	1247.443927	17.403213
33.732163	1235.320569	17.408231
33.361789	1246.389520	17.413248
33.651528	1240.953853	17.418266
33.793624	1235.427378	17.423283
33.737351	1236.632771	17.428301
33.582994	1240.970855	17.433319
33.407023	1232.852487	17.438336
33.620939	1240.431176	17.443354
33.660658	1225.759552	17.448371
33.446709	1232.208226	17.453389
33.700571	1229.559497	17.458407
33.549509	1233.998995	17.463424
33.813328	1240.777302	17.468442
34.138817	1237.521813	17.473459
33.855622	1235.558378	17.478477
33.665727	1232.620822	17.483495
33.550263	1229.917340	17.488512
33.660176	1223.492717	17.493530
33.872282	1225.219618	17.498547
33.482136	1244.280057	17.503565
33.974010	1252.192458	17.508583
34.112781	1255.206296	17.513600
33.939073	1257.346521	17.518618
34.292769	1255.285104	17.523635
34.532274	1258.474317	17.528653
34.545774	1248.829242	17.533671
34.612697	1258.835016	17.538688
34.320875	1243.201596	17.543706
34.321414	1228.045954	17.548723
34.002084	1230.534772	17.553741
34.370223	1239.696807	17.558759
34.605128	1254.313813	17.563776
34.503867	1252.693350	17.568794
34.797170	1243.769061	17.573811
34.521114	1232.580463	17.578829
34.638759	1229.403612	17.583847
34.728218	1222.771770	17.588864
34.449132	1216.174413	17.593882
35.056729	1214.607391	17.598899
34.751172	1226.787154	17.603917
34.439437	1205.988824	17.608935
34.806236	1225.777723	17.613952
34.965749	1231.427353	17.618970
35.199930	1227.405189	17.623987
34.947971	1230.321372	17.629005
35.028358	1212.924626	17.634023
34.867439	1210.012177	17.639040
34.721418	1211.267916	17.644058
34.898850	1222.557205	17.649075
34.960973	1241.746006	17.654093
35.119640	1247.085167	17.659111
35.284049	1249.775466	17.664128
34.775728	1250.512710	17.669146
35.293463	1251.081388	17.674163
35.229737	1251.163663	17.679181
35.230307	1252.512752	17.684199
35.158733	1249.843702	17.689216
35.189683	1247.820575	17.694234
35.381976	1248.372873	17.699251
35.013510	1253.679575	17.704269
35.145406	1253.105350	17.709287
35.279161	1244.938647	17.714304
35.338651	1244.878007	17.719322
35.618353	1238.736956	17.724339
35.216255	1252.024859	17.729357
35.493099	1260.720213	17.734375
35.892959	1265.756707	17.739392
35.731557	1272.488777	17.744410
35.925821	1272.601792	17.749427
35.746974	1278.705690	17.754445
35.982446	1273.047545	17.759463
36.023875	1265.653229	17.764480
35.755691	1259.724090	17.769498
35.967831	1250.262131	17.774515
36.118751	1258.109949	17.779533
35.739318	1257.110889	17.784551
36.057798	1264.480487	17.789568
35.633741	1266.788301	17.794586
36.162378	1265.804844	17.799603
36.062368	1267.699761	17.804621
35.908150	1272.459860	17.809639
36.301324	1264.070905	17.814656
36.238157	1264.577871	17.819674
36.445024	1260.240567	17.824691
36.481333	1266.971663	17.829709
36.215381	1264.344365	17.834727
36.226982	1257.575848	17.839744
36.185362	1269.050391	17.844762
36.231034	1247.906394	17.849779
36.321440	1264.036333	17.854797
36.266795	1271.051433	17.859815
36.074553	1255.747103	17.864832
36.343114	1271.900981	17.869850
36.630585	1276.911279	17.874867
36.809149	1281.714098	17.879885
36.925291	1285.909604	17.884903
37.480188	1269.974806	17.889920
36.742993	1266.346744	17.894938
36.902019	1240.266818	17.899955
36.948358	1249.627612	17.904973
36.683459	1248.587864	17.909991
37.078738	1245.924683	17.915008
36.941015	1248.930539	17.920026
36.704097	1246.879888	17.925043
36.936897	1246.227872	17.930061
36.612174	1249.558496	17.935079
36.897114	1260.952380	17.940096
37.028195	1281.987954	17.945114
37.195390	1272.182286	17.950131
37.137288	1275.521355	17.955149
37.120707	1271.340473	17.960167
37.266955	1276.719502	17.965184
37.240064	1280.202197	17.970202
36.775102	1271.900746	17.975219
37.264599	1274.196877	17.980237
37.366065	1278.981408	17.985255
37.525421	1272.775309	17.990272
37.494575	1281.296627	17.995290
37.741877	1281.274455	18.000307
37.691602	1280.394695	18.005325
37.685378	1283.442872	18.010343
37.691804	1272.737193	18.015360
37.495587	1282.873722	18.020378
37.243999	1279.809407	18.025395
37.664929	1274.574749	18.030413
37.914543	1301.613217	18.035431
38.449044	1306.081308	18.040448
37.976674	1287.987404	18.045466
37.997551	1280.853965	18.050483
37.588723	1266.766278	18.055501
37.416268	1265.411571	18.060519
38.530697	1286.391192	18.065536
38.395624	1293.657061	18.070554
38.001295	1267.467885	18.075571
38.221083	1275.071992	18.080589
37.733345	1285.676640	18.085607
38.616766	1284.203921	18.090624
38.672055	1289.555554	18.095642
38.283535	1278.758826	18.100659
38.375956	1281.331967	18.105677
38.137123	1268.172676	18.110695
38.818415	1271.164456	18.115712
38.464642	1266.296343	18.120730
38.544187	1265.457996	18.125747
38.524207	1256.876700	18.130765
38.405570	1262.161172	18.135783
38.992179	1267.267412	18.140800
38.569622	1270.474542	18.145818
38.290810	1275.867133	18.150835
38.504185	1284.275031	18.155853
38.391571	1294.121700	18.160871
38.548534	1287.087289	18.165888
38.474238	1287.901997	18.170906
38.749093	1291.979005	18.175923
38.633629	1287.361029	18.180941
38.844603	1297.816488	18.185959
38.757589	1286.383448	18.190976
38.672498	1305.146421	18.195994
39.250233	1316.377909	18.201011
39.653086	1312.753656	18.206029
39.282540	1299.550878	18.211047
39.442847	1282.993095	18.216064
39.345911	1285.958323	18.221082
39.376065	1279.411900	18.226099
39.331089	1286.101004	18.231117
39.133975	1283.586272	18.236135
39.533610	1271.149174	18.241152
39.448710	1284.847358	18.246170
39.411329	1281.619887	18.251187
39.634909	1285.710927	18.256205
39.286277	1283.556402	18.261223
39.358330	1271.466254	18.266240
39.444183	1290.996040	18.271258
39.311042	1310.613426	18.276275
39.839122	1307.626995	18.281293
39.510738	1316.813899	18.286311
39.776772	1313.565521	18.291328
39.813072	1311.716291	18.296346
39.766349	1317.232127	18.301363
39.734618	1311.811677	18.306381
39.492688	1315.757268	18.311399
39.955035	1307.310338	18.316416
39.745611	1317.713640	18.321434
39.808668	1310.342478	18.326451
39.905409	1305.416405	18.331469
39.687165	1315.495594	18.336487
40.019250	1321.046106	18.341504
40.117470	1326.931540	18.346522
40.318649	1338.222085	18.351539
40.713486	1337.517152	18.356557
40.323857	1334.759222	18.361575
40.641279	1326.872567	18.366592
40.305187	1322.906184	18.371610
40.447532	1327.198523	18.376627
40.459336	1322.351125	18.381645
40.438108	1323.937692	18.386663
40.549158	1325.347950	18.391680
40.564909	1327.891324	18.396698
40.285455	1327.883081	18.401715
40.735482	1323.462829	18.406733
40.716476	1329.005950	18.411751
40.893192	1321.014737	18.416768
40.774568	1324.685122	18.421786
40.618275	1325.259927	18.426803
40.582613	1325.159593	18.431821
40.403810	1323.867745	18.436839
40.879354	1319.622773	18.441856
41.070028	1323.592525	18.446874
40.888738	1325.751341	18.451891
41.201411	1327.607597	18.456909
41.179608	1344.073185	18.461927
41.092621	1347.243456	18.466944
41.442945	1342.035077	18.471962
41.540475	1343.874338	18.476979
41.485049	1333.924142	18.481997
41.106110	1322.608095	18.487015
41.238408	1326.524166	18.492032
41.358147	1337.373147	18.497050
41.269155	1348.354461	18.502067
41.294389	1350.856106	18.507085
41.134071	1352.435479	18.512103
41.613045	1350.957930	18.517120
41.214063	1345.495754	18.522138
41.194957	1359.466916	18.527155
41.543268	1347.759125	18.532173
41.468529	1370.891150	18.537191
41.697715	1365.219057	18.542208
41.831995	1382.051249	18.547226
41.811406	1379.804789	18.552243
41.888858	1371.315106	18.557261
41.655572	1379.668163	18.562279
42.187023	1378.907060	18.567296
42.608948	1372.821449	18.572314
42.426024	1382.226333	18.577331
42.284093	1368.998096	18.582349
41.985915	1358.835483	18.587367
42.189544	1358.778052	18.592384
42.050587	1367.149676	18.597402
42.021449	1366.394345	18.602419
42.341486	1366.648262	18.607437
42.642825	1368.809939	18.612455
42.671388	1365.949823	18.617472
42.684518	1367.688552	18.622490
42.381163	1374.600946	18.627507
42.387774	1362.023592	18.632525
42.492559	1377.384754	18.637543
42.344862	1368.434480	18.642560
42.510050	1365.815820	18.647578
42.523496	1362.300762	18.652595
42.105384	1367.037822	18.657613
42.216007	1373.872358	18.662631
42.087645	1383.381162	18.667648
42.362879	1392.304409	18.672666
42.666701	1401.845328	18.677683
42.936111	1405.587850	18.682701
43.022767	1399.707945	18.687719
43.053637	1400.356368	18.692736
43.242574	1398.365228	18.697754
42.788085	1395.818059	18.702771
43.230185	1395.140307	18.707789
43.085252	1398.238725	18.712807
43.078799	1383.488407	18.717824
43.543783	1405.761127	18.722842
43.179698	1409.498705	18.727859
43.371928	1408.568396	18.732877
43.629098	1411.755494	18.737895
43.495859	1409.868291	18.742912
43.826203	1411.383443	18.747930
43.416733	1413.527441	18.752947
43.573115	1411.199597	18.757965
43.789589	1414.604475	18.762983
44.014636	1407.248075	18.768000
43.953520	1408.147210	18.773018
43.844574	1415.932790	18.778035
43.785446	1395.354810	18.783053
44.041286	1408.834273	18.788071
43.988070	1409.543126	18.793088
44.046650	1402.588004	18.798106
43.709681	1410.126450	18.803123
43.974758	1406.427834	18.808141
43.837695	1406.515605	18.813159
43.984019	1412.741490	18.818176
44.207740	1405.486488	18.823194
43.863504	1403.658762	18.828211
44.170086	1401.700824	18.833229
43.801640	1408.540983	18.838247
44.002292	1398.034424	18.843264
44.031125	1423.737016	18.848282
44.217632	1428.613362	18.853299
44.450646	1436.248028	18.858317
44.691555	1432.876639	18.863335
44.783922	1419.937360	18.868352
44.970288	1429.168302	18.873370
45.105389	1427.568770	18.878387
44.935038	1426.198346	18.883405
44.912406	1420.042513	18.888423
44.902172	1401.468925	18.893440
44.677048	1397.130549	18.898458
44.228959	1396.979079	18.903475
44.839977	1413.841911	18.908493
44.899902	1415.037453	18.913511
45.253073	1421.446672	18.918528
45.005732	1416.067925	18.923546
45.154245	1425.346887	18.928563
45.505470	1418.787199	18.933581
45.264959	1421.843241	18.938599
45.056180	1415.661263	18.943616
45.253941	1418.133852	18.948634
44.961836	1420.409127	18.953651
45.040077	1421.869333	18.958669
45.023791	1422.653148	18.963687
45.045605	1421.424008	18.968704
45.299493	1420.354322	18.973722
45.199705	1444.827189	18.978739
45.971657	1446.439023	18.983757
45.719823	1448.822172	18.988775
45.914659	1454.136104	18.993792
45.903501	1449.059419	18.998810
45.281881	1452.363447	19.003827
45.366048	1443.254125	19.008845
45.628934	1447.335919	19.013863
45.500026	1439.522207	19.018880
45.864623	1445.175626	19.023898
45.748137	1445.600911	19.028915
45.891892	1448.400186	19.033933
45.975401	1450.157542	19.038951
45.726249	1470.124714	19.043968
46.163541	1469.420987	19.048986
46.237587	1474.372730	19.054003
46.595098	1472.937011	19.059021
46.508795	1464.878811	19.064039
46.720650	1460.324882	19.069056
46.872139	1473.374909	19.074074
46.497378	1467.806698	19.079091
46.720076	1461.788022	19.084109
46.591500	1451.240085	19.089127
46.554237	1467.571371	19.094144
46.545332	1464.174962	19.099162
46.534780	1469.642322	19.104179
46.903933	1464.576832	19.109197
46.695579	1457.429049	19.114215
46.760978	1459.565388	19.119232
46.736707	1461.941031	19.124250
46.869413	1460.470237	19.129267
46.903127	1452.353121	19.134285
46.830669	1457.700062	19.139303
46.647274	1465.584258	19.144320
46.931220	1454.952798	19.149338
46.769894	1462.825844	19.154355
46.854928	1479.783647	19.159373
47.187472	1482.749577	19.164391
47.160592	1493.536424	19.169408
47.590956	1488.371780	19.174426
47.510239	1489.358427	19.179443
47.302209	1485.539610	19.184461
47.632932	1489.037717	19.189479
47.283136	1479.070212	19.194496
47.369377	1482.101487	19.199514
47.312341	1491.141824	19.204531
47.276121	1494.430455	19.209549
47.487830	1503.153307	19.214567
47.554367	1513.434105	19.219584
48.134857	1514.806517	19.224602
48.580915	1504.015407	19.229619
48.850243	1480.515879	19.234637
48.842357	1473.348157	19.239655
48.455473	1472.770384	19.244672
48.870661	1458.132196	19.249690
48.461494	1458.842338	19.254707
48.478364	1440.908272	19.259725
48.650266	1434.492156	19.264743
48.229461	1428.642251	19.269760
48.441451	1420.702602	19.274778
48.429640	1433.489589	19.279795
48.095224	1432.690114	19.284813
48.769672	1421.599300	19.289831
48.469197	1422.858679	19.294848
48.758954	1420.298831	19.299866
48.541821	1421.673881	19.304883
48.488946	1424.090886	19.309901
48.473246	1419.529909	19.314919
48.569671	1411.588606	19.319936
48.637271	1418.985804	19.324954
48.549821	1425.397786	19.329971
48.686133	1447.438194	19.334989
49.241320	1447.995146	19.340007
48.881332	1466.835893	19.345024
48.614077	1454.054775	19.350042
48.551456	1457.867454	19.355059
48.954322	1460.307536	19.360077
48.563128	1448.431639	19.365095
48.453294	1466.791848	19.370112
48.786710	1484.359535	19.375130
48.699509	1481.480057	19.380147
48.900685	1488.016531	19.385165
49.111947	1488.823946	19.390183
49.106060	1521.287778	19.395200
49.378391	1512.022737	19.400218
49.165939	1506.304311	19.405235
49.133181	1520.265683	19.410253
49.565479	1511.542937	19.415271
49.420033	1524.642358	19.420288
49.673364	1529.522197	19.425306
49.769569	1541.652362	19.430323
49.628006	1544.093574	19.435341
50.060930	1542.382724	19.440359
50.073546	1550.952477	19.445376
50.166221	1551.239856	19.450394
50.384365	1551.491028	19.455411
50.209105	1548.634833	19.460429
50.594939	1542.185481	19.465447
50.088078	1545.415731	19.470464
50.210130	1534.304444	19.475482
50.038906	1546.664882	19.480499
50.114381	1542.450123	19.485517
50.406523	1544.559812	19.490535
50.364573	1542.838911	19.495552
50.622299	1534.056980	19.500570
50.501710	1537.510819	19.505587
50.642769	1543.764402	19.510605
50.788463	1540.767074	19.515623
50.575679	1543.826799	19.520640
50.652912	1533.764271	19.525658
50.656510	1540.077313	19.530675
50.453371	1539.348924	19.535693
50.619225	1553.242277	19.540711
50.543274	1562.924366	19.545728
50.931035	1565.016197	19.550746
51.167949	1567.393329	19.555763
50.680748	1559.299743	19.560781
50.991292	1562.500442	19.565799
51.123016	1559.657790	19.570816
51.171150	1556.436915	19.575834
51.365857	1564.819724	19.580851
51.480546	1570.277722	19.585869
51.822535	1570.090999	19.590887
51.210745	1570.883638	19.595904
51.645444	1562.670295	19.600922
51.822319	1563.688149	19.605939
51.540745	1565.590837	19.610957
51.667410	1556.088569	19.615975
51.538712	1563.866877	19.620992
51.679807	1567.201642	19.626010
51.662630	1577.613716	19.631027
51.669267	1593.649657	19.636045
51.912498	1582.954406	19.641063
51.809080	1589.361629	19.646080
51.776412	1590.450530	19.651098
51.969856	1582.602068	19.656115
51.971425	1587.214720	19.661133
52.380180	1582.653621	19.666151
51.971515	1590.231628	19.671168
52.034314	1587.714198	19.676186
52.171669	1592.259403	19.681203
52.044526	1603.731085	19.686221
52.715750	1609.647770	19.691239
52.489896	1617.861533	19.696256
52.462120	1616.632746	19.701274
52.756519	1604.821520	19.706291
52.589992	1612.290791	19.711309
52.675958	1596.639498	19.716327
52.721392	1603.240880	19.721344
52.767428	1604.790313	19.726362
52.731800	1597.629506	19.731379
52.680823	1604.174079	19.736397
52.864289	1602.211382	19.741415
52.680379	1607.045807	19.746432
53.030874	1620.399097	19.751450
52.951382	1629.396004	19.756467
53.198813	1619.026401	19.761485
53.388661	1620.448393	19.766503
53.111399	1626.002653	19.771520
53.224611	1626.058672	19.776538
53.314831	1617.971842	19.781555
53.699910	1631.141445	19.786573
53.864504	1617.660086	19.791591
53.575893	1625.443742	19.796608
53.726938	1625.167103	19.801626
54.049971	1624.418189	19.806643
53.922730	1621.072120	19.811661
53.909813	1614.522478	19.816679
53.607259	1616.050715	19.821696
53.901322	1620.035644	19.826714
53.793498	1616.561155	19.831731
53.722225	1613.740420	19.836749
53.863123	1620.560585	19.841767
53.716993	1620.364043	19.846784
53.852034	1636.696004	19.851802
54.295823	1638.915933	19.856819
54.142945	1651.809615	19.861837
54.400427	1642.769794	19.866855
54.326235	1651.375684	19.871872
54.696674	1647.251635	19.876890
54.718504	1650.138926	19.881907
54.511402	1646.810062	19.886925
54.505707	1636.957309	19.891943
54.341654	1638.446388	19.896960
54.703760	1640.262185	19.901978
54.471405	1635.080472	19.906995
54.556282	1646.869697	19.912013
54.527873	1646.599261	19.917031
54.630838	1650.720680	19.922048
54.804468	1659.208223	19.927066
54.867704	1662.397684	19.932083
55.224925	1669.388606	19.937101
55.445943	1662.111889	19.942119
55.300797	1668.381200	19.947136
55.283424	1666.990841	19.952154
55.690463	1666.316937	19.957171
55.452192	1670.414368	19.962189
55.504043	1665.064153	19.967207
55.400860	1654.237453	19.972224
55.680088	1660.327966	19.977242
55.854325	1657.708935	19.982259
55.266162	1659.294879	19.987277
55.470215	1651.614694	19.992295
55.361942	1656.459792	19.997312
55.653289	1662.016412	20.002330
55.620560	1665.425362	20.007347
55.766785	1670.545484	20.012365
55.588910	1666.867276	20.017383
55.779967	1665.188737	20.022400
55.777383	1683.097527	20.027418
55.800708	1689.131765	20.032435
56.017088	1686.336043	20.037453
56.118710	1684.854253	20.042471
55.902921	1686.406658	20.047488
55.987884	1684.694176	20.052506
56.135826	1689.759295	20.057523
56.533796	1710.470786	20.062541
56.864807	1715.153525	20.067559
57.222602	1713.002395	20.072576
56.832953	1698.118223	20.077594
56.774166	1682.427910	20.082611
56.474518	1686.550505	20.087629
56.535127	1684.805063	20.092647
56.618342	1696.566650	20.097664
56.518137	1712.746847	20.102682
57.141178	1716.558230	20.107699
56.725498	1725.513824	20.112717
57.045011	1718.962824	20.117735
56.972108	1722.111933	20.122752
56.663020	1716.022488	20.127770
57.244223	1713.179908	20.132787
57.173083	1730.532045	20.137805
57.465211	1729.497322	20.142823
57.848879	1741.637743	20.147840
57.910733	1724.953334	20.152858
57.892051	1716.949117	20.157875
57.920925	1713.939675	20.162893
58.265440	1700.712196	20.167911
58.012014	1701.020879	20.172928
57.599038	1707.151651	20.177946
58.259059	1691.232417	20.182963
57.871831	1701.331280	20.187981
57.818727	1708.867966	20.192999
57.939222	1696.302515	20.198016
57.721137	1702.602860	20.203034
57.976716	1700.594309	20.208051
57.624950	1713.954160	20.213069
57.740365	1717.045198	20.218087
58.006745	1724.778003	20.223104
58.014879	1718.488200	20.228122
57.973223	1721.095903	20.233139
58.091797	1731.818192	20.238157
58.154955	1748.817326	20.243175
58.317023	1747.129030	20.248192
58.536756	1761.544712	20.253210
58.777300	1747.293936	20.258227
58.410887	1748.777287	20.263245
58.506407	1747.308709	20.268263
58.622012	1752.023716	20.273280
58.889581	1767.826317	20.278298
59.358110	1763.465859	20.283315
59.411071	1772.674691	20.288333
59.174410	1763.499212	20.293351
59.447914	1748.343756	20.298368
59.229236	1743.122332	20.303386
59.745158	1743.369294	20.308403
59.239664	1735.571956	20.313421
59.261745	1737.760020	20.318439
59.360416	1732.791759	20.323456
59.071070	1755.684833	20.328474
59.397489	1754.279060	20.333491
59.565360	1758.763339	20.338509
59.623183	1758.695495	20.343527
59.812753	1765.006854	20.348544
59.693527	1759.061819	20.353562
60.277393	1752.519626	20.358579
60.021123	1768.913218	20.363597
59.869195	1758.390999	20.368615
60.128493	1765.715166	20.373632
59.633156	1771.180919	20.378650
60.158935	1758.086650	20.383667
59.736327	1763.838735	20.388685
60.049863	1782.589579	20.393703
60.552261	1781.044321	20.398720
60.559813	1790.918971	20.403738
60.848209	1778.991683	20.408755
60.730386	1788.113161	20.413773
60.850110	1782.768948	20.418791
61.194836	1785.469138	20.423808
60.627274	1768.229848	20.428826
60.606614	1765.132961	20.433843
60.458462	1773.402788	20.438861
60.714292	1786.939671	20.443879
61.041517	1772.536278	20.448896
61.123304	1779.778931	20.453914
61.248966	1771.805420	20.458931
61.027994	1780.564120	20.463949
61.000370	1778.784119	20.468967
61.299707	1775.115156	20.473984
61.121140	1777.889322	20.479002
60.851186	1781.584177	20.484019
61.304450	1789.854847	20.489037
61.183719	1795.740629	20.494055
61.571697	1791.491976	20.499072
61.626033	1802.121054	20.504090
61.814830	1792.414223	20.509107
61.841865	1796.012480	20.514125
61.638926	1786.999490	20.519143
62.003316	1792.384572	20.524160
61.891286	1799.094097	20.529178
61.881141	1791.845501	20.534195
61.699448	1789.802526	20.539213
61.909964	1816.281078	20.544231
62.106953	1818.678665	20.549248
61.891491	1826.092393	20.554266
62.632401	1822.639792	20.559283
62.350777	1822.680331	20.564301
62.633668	1826.740793	20.569319
62.554773	1825.911032	20.574336
62.272186	1822.316330	20.579354
62.593342	1827.938135	20.584371
62.807339	1822.079821	20.589389
62.550710	1829.461416	20.594407
62.543564	1816.075750	20.599424
62.659421	1823.915511	20.604442
63.203313	1835.608122	20.609459
62.847260	1829.655962	20.614477
62.977618	1841.951553	20.619495
63.212715	1846.789642	20.624512
63.379610	1850.530020	20.629530
63.240367	1838.931631	20.634547
63.062070	1839.382946	20.639565
63.294081	1843.803047	20.644583
63.404096	1846.484382	20.649600
63.278620	1838.543126	20.654618
63.816606	1838.173830	20.659635
63.959669	1840.453218	20.664653
63.371573	1837.436841	20.669671
63.940316	1839.817923	20.674688
63.890904	1840.801751	20.679706
63.594213	1834.694450	20.684723
63.637956	1842.269830	20.689741
63.610928	1842.134199	20.694759
63.759638	1849.548043	20.699776
64.172019	1875.835670	20.704794
63.761106	1866.398539	20.709811
63.831388	1861.464483	20.714829
63.892996	1863.942056	20.719847
64.144160	1867.362530	20.724864
64.182121	1888.474642	20.729882
64.589577	1888.156566	20.734899
64.736121	1898.218419	20.739917
64.987801	1894.491601	20.744935
64.970784	1887.783470	20.749952
64.578085	1887.999161	20.754970
65.094519	1891.952323	20.759987
65.082254	1888.551655	20.765005
64.893445	1893.464541	20.770023
65.295511	1890.172965	20.775040
65.188684	1891.543895	20.780058
65.015440	1886.565658	20.785075
65.342100	1889.268869	20.790093
65.248602	1895.598586	20.795111
65.486848	1885.799227	20.800128
65.083267	1887.854512	20.805146
65.500978	1886.011511	20.810163
65.411876	1879.630323	20.815181
65.294481	1895.104122	20.820199
66.062450	1907.668992	20.825216
65.542937	1903.571129	20.830234
65.569784	1914.777291	20.835251
66.149880	1907.610467	20.840269
66.060881	1916.037862	20.845287
66.326034	1897.949012	20.850304
66.332498	1895.781838	20.855322
66.180052	1896.223741	20.860339
66.319925	1896.653676	20.865357
66.279688	1899.336369	20.870375
66.515781	1892.802312	20.875392
66.105188	1897.836310	20.880410
66.223827	1900.828031	20.885427
66.616531	1886.890026	20.890445
66.492222	1902.966160	20.895463
66.734081	1898.203576	20.900480
66.708366	1906.584228	20.905498
66.352678	1902.297722	20.910515
66.093411	1909.209322	20.915533
66.427641	1927.192339	20.920551
66.947729	1924.981926	20.925568
67.043973	1923.380141	20.930586
66.899254	1923.256195	20.935603
67.020122	1936.881387	20.940621
67.213535	1948.527608	20.945639
67.256442	1943.681145	20.950656
67.543314	1949.044520	20.955674
67.400233	1950.897465	20.960691
67.816367	1953.681880	20.965709
67.647599	1953.697757	20.970727
67.827051	1943.195536	20.975744
67.652494	1949.117093	20.980762
67.811848	1956.331189	20.985779
67.671938	1952.422980	20.990797
67.816322	1966.079329	20.995815
67.670586	1955.397286	21.000832
67.623017	1956.452468	21.005850
67.834383	1961.278002	21.010867
68.267433	1964.223388	21.015885
68.634106	1973.495557	21.020903
68.459241	1971.921501	21.025920
68.529553	1975.223237	21.030938
68.121931	1976.385897	21.035955
68.433724	1962.778989	21.040973
68.354735	1972.276798	21.045991
68.572740	1954.943356	21.051008
68.802184	1966.767460	21.056026
68.309138	1964.582899	21.061043
68.861441	1968.974215	21.066061
69.143474	1984.857705	21.071079
69.002464	1992.167799	21.076096
69.365823	1997.228321	21.081114
69.236160	1996.897541	21.086131
69.493490	1981.753995	21.091149
68.964880	1990.149372	21.096167
69.431905	1989.701709	21.101184
69.547952	2002.036813	21.106202
69.489440	1994.518601	21.111219
69.478909	1997.722360	21.116237
69.333961	1991.257099	21.121255
69.311317	1996.894765	21.126272
69.608700	1995.572932	21.131290
69.827452	2019.459120	21.136307
69.742571	2020.688618	21.141325
69.955192	2020.430874	21.146343
69.870103	2023.886006	21.151360
69.892624	2015.858645	21.156378
69.429273	2023.125868	21.161395
70.607588	2042.204963	21.166413
70.672085	2052.408506	21.171431
71.023206	2039.400116	21.176448
70.541619	2032.581334	21.181466
70.495708	2025.711410	21.186483
71.030721	2035.930446	21.191501
71.000264	2037.167437	21.196519
70.745402	2016.060921	21.201536
70.946005	2019.685896	21.206554
71.261741	2039.913859	21.211571
71.023744	2026.687244	21.216589
71.064873	2040.137983	21.221607
71.131301	2034.997030	21.226624
71.345897	2032.386584	21.231642
71.171552	2037.027425	21.236659
71.447985	2017.780256	21.241677
71.526474	2032.574785	21.246695
71.708155	2032.075331	21.251712
71.926183	2027.450133	21.256730
71.604184	2031.645431	21.261747
71.890477	2016.882865	21.266765
71.663033	2030.651461	21.271783
71.793049	2027.237352	21.276800
71.670369	2036.382224	21.281818
71.633360	2030.351766	21.286835
71.599802	2030.874308	21.291853
71.631171	2042.873516	21.296871
72.049125	2049.283651	21.301888
71.955371	2052.492984	21.306906
71.730075	2065.235263	21.311923
72.052672	2053.099324	21.316941
72.148122	2063.531197	21.321959
72.349860	2077.857645	21.326976
72.398005	2076.538643	21.331994
72.102168	2078.983136	21.337011
72.583596	2081.882710	21.342029
72.561176	2079.537632	21.347047
72.998763	2096.008382	21.352064
73.420220	2098.708081	21.357082
73.046598	2113.612864	21.362099
73.136001	2096.907335	21.367117
73.634371	2108.847092	21.372135
73.445678	2097.331137	21.377152
73.484834	2092.120682	21.382170
73.426996	2094.722475	21.387187
74.075093	2096.645919	21.392205
73.575371	2094.046696	21.397223
73.787153	2092.838688	21.402240
74.086962	2090.399506	21.407258
74.079756	2095.890153	21.412275
73.961489	2073.191946	21.417293
74.215814	2086.175008	21.422311
74.026781	2076.765440	21.427328
74.103359	2074.716511	21.432346
73.862589	2088.292883	21.437363
74.237106	2087.927129	21.442381
74.040542	2095.341387	21.447399
74.069400	2089.493662	21.452416
73.904753	2095.037640	21.457434
74.265007	2110.551170	21.462451
74.266692	2115.307269	21.467469
74.597526	2123.813824	21.472487
74.419628	2130.647825	21.477504
74.490390	2133.590067	21.482522
74.351798	2134.045028	21.487539
74.804705	2141.637594	21.492557
74.577111	2166.135202	21.497575
75.044848	2149.031303	21.502592
75.414774	2139.385494	21.507610
75.272051	2141.641162	21.512627
75.729098	2134.050586	21.517645
75.566755	2135.145328	21.522663
75.580482	2139.168322	21.527680
76.035950	2134.926078	21.532698
75.512688	2138.053658	21.537715
75.828874	2135.642456	21.542733
75.900279	2136.655831	21.547751
75.750797	2152.971843	21.552768
76.235410	2152.334638	21.557786
76.199957	2167.507291	21.562803
76.408951	2163.524902	21.567821
76.479609	2172.038502	21.572839
76.216141	2166.506263	21.577856
76.368313	2166.781404	21.582874
76.236399	2159.344996	21.587891
76.256593	2161.848792	21.592909
76.178398	2156.128284	21.597927
76.097276	2170.126625	21.602944
76.745393	2178.403313	21.607962
76.303283	2188.166722	21.612979
76.348222	2191.389256	21.617997
76.797490	2184.125150	21.623015
76.652340	2198.334948	21.628032
76.934399	2193.821109	21.633050
76.909295	2217.513874	21.638067
77.243084	2221.870318	21.643085
77.113757	2222.932019	21.648103
77.426449	2214.356324	21.653120
77.780680	2222.131474	21.658138
77.389761	2218.011366	21.663155
77.478726	2219.167893	21.668173
77.700691	2221.326743	21.673191
77.300105	2221.027990	21.678208
77.707440	2224.125735	21.683226
77.635731	2236.915859	21.688243
77.933989	2241.615228	21.693261
78.176824	2237.308686	21.698279
78.297081	2245.185726	21.703296
78.284111	2243.168587	21.708314
78.003026	2242.670442	21.713331
78.090184	2238.287015	21.718349
78.333001	2249.928795	21.723367
78.384913	2259.144784	21.728384
79.040823	2266.774543	21.733402
78.820818	2275.623912	21.738419
78.862793	2270.920813	21.743437
79.076894	2266.846602	21.748455
78.967693	2268.298670	21.753472
79.481830	2263.700572	21.758490
79.299140	2256.133578	21.763507
79.824001	2256.623954	21.768525
79.651702	2251.780877	21.773543
79.524712	2251.208696	21.778560
79.971527	2260.094091	21.783578
79.762389	2257.572140	21.788595
79.510270	2260.947207	21.793613
79.740913	2250.597298	21.798631
79.413083	2255.962543	21.803648
80.040869	2251.440051	21.808666
79.659125	2253.791365	21.813683
79.728001	2252.906707	21.818701
80.181825	2245.759928	21.823719
79.899468	2249.731368	21.828736
80.034315	2262.571045	21.833754
79.885518	2274.978728	21.838771
80.292049	2270.706391	21.843789
80.669864	2257.724093	21.848807
80.752387	2258.772243	21.853824
80.855351	2255.279115	21.858842
81.060415	2267.130336	21.863859
81.081716	2252.673010	21.868877
81.056018	2254.975388	21.873895
81.189676	2255.606765	21.878912
81.368727	2255.923505	21.883930
81.358807	2259.156744	21.888947
80.979934	2265.432067	21.893965
81.286010	2252.881782	21.898983
81.036329	2263.384139	21.904000
81.465089	2264.285770	21.909018
81.338194	2275.986651	21.914035
81.388411	2298.916613	21.919053
81.808152	2292.150684	21.924071
81.570887	2295.622111	21.929088
81.947280	2288.937010	21.934106
81.831299	2292.380800	21.939123
81.691712	2301.338869	21.944141
82.055470	2302.335559	21.949159
82.069608	2313.061828	21.954176
82.145826	2309.971172	21.959194
82.176987	2312.100327	21.964211
82.238815	2323.488377	21.969229
82.337094	2307.988654	21.974247
82.081275	2319.511777	21.979264
82.672109	2330.869398	21.984282
82.772952	2341.419068	21.989299
82.848299	2343.787740	21.994317
83.264179	2335.871224	21.999335
83.213252	2341.053074	22.004352
83.179355	2341.448121	22.009370
83.291870	2334.631259	22.014387
83.502678	2333.962779	22.019405
83.658862	2330.081253	22.024423
83.447872	2331.632528	22.029440
83.439218	2329.126460	22.034458
83.524174	2332.540408	22.039475
83.722584	2329.004235	22.044493
83.760119	2315.425669	22.049511
83.664415	2323.807941	22.054528
83.841021	2324.329819	22.059546
84.030181	2324.300384	22.064563
83.778601	2328.441142	22.069581
83.810455	2347.989898	22.074599
84.037466	2358.436720	22.079616
84.097579	2351.726594	22.084634
84.082727	2357.656804	22.089651
83.971665	2359.376913	22.094669
84.420039	2381.202218	22.099687
84.484690	2386.723153	22.104704
84.499596	2389.598347	22.109722
84.718287	2387.496625	22.114739
84.701192	2386.317184	22.119757
85.053837	2392.061133	22.124775
84.573759	2401.042773	22.129792
84.977141	2398.375696	22.134810
85.069663	2399.881262	22.139827
85.171846	2409.676797	22.144845
85.318038	2399.601462	22.149863
85.095746	2416.680265	22.154880
85.628308	2426.864930	22.159898
85.527022	2427.783004	22.164915
85.408443	2427.834241	22.169933
85.982056	2429.637428	22.174951
86.035622	2432.212102	22.179968
85.938357	2425.125331	22.184986
86.135670	2437.267349	22.190003
86.060471	2446.741589	22.195021
86.567975	2454.774071	22.200039
86.286782	2462.699040	22.205056
86.721756	2451.020511	22.210074
86.692722	2457.102333	22.215091
86.426220	2458.052590	22.220109
86.784169	2451.625218	22.225127
86.691547	2455.654551	22.230144
87.042058	2445.531056	22.235162
86.958298	2452.692477	22.240179
86.919714	2468.466751	22.245197
87.322044	2480.458586	22.250215
87.325159	2482.729438	22.255232
87.345548	2484.621815	22.260250
87.534906	2472.835659	22.265267
87.066574	2483.117405	22.270285
87.465844	2478.728499	22.275303
87.753399	2480.563484	22.280320
87.458823	2474.688654	22.285338
87.787476	2492.272061	22.290355
87.891209	2498.129860	22.295373
88.049064	2492.996398	22.300391
87.967503	2505.740346	22.305408
87.984908	2503.556309	22.310426
88.102441	2495.827882	22.315443
88.261220	2502.988390	22.320461
88.364788	2506.548108	22.325479
88.740738	2525.076876	22.330496
88.661912	2536.225061	22.335514
89.005029	2526.485041	22.340531
88.979502	2533.302951	22.345549
89.774879	2510.560146	22.350567
89.698172	2495.568075	22.355584
89.559095	2468.715125	22.360602
89.636226	2468.385795	22.365619
89.632438	2462.965810	22.370637
89.581124	2460.451061	22.375655
89.757086	2466.735441	22.380672
89.780217	2460.652694	22.385690
89.765631	2462.994203	22.390707
89.406506	2465.749281	22.395725
89.740900	2457.126144	22.400743
89.840123	2459.309364	22.405760
89.724630	2472.513664	22.410778
89.610912	2496.084568	22.415795
89.675937	2495.947019	22.420813
90.114761	2491.824380	22.425831
90.026511	2496.550265	22.430848
90.400777	2504.263172	22.435866
90.689654	2514.293111	22.440883
90.588079	2531.566946	22.445901
90.763444	2526.656162	22.450919
90.706432	2529.589005	22.455936
90.717003	2537.760810	22.460954
90.754441	2536.112829	22.465971
90.805517	2544.054276	22.470989
90.994970	2555.694525	22.476007
91.095780	2561.843790	22.481024
91.175714	2563.955818	22.486042
91.458387	2557.276336	22.491059
91.226202	2567.678347	22.496077
91.570364	2576.424680	22.501095
91.635909	2582.506582	22.506112
91.464252	2595.778983	22.511130
91.927129	2591.841306	22.516147
91.690700	2587.338321	22.521165
91.951787	2580.883292	22.526183
91.866848	2600.335234	22.531200
91.896822	2614.774192	22.536218
92.326451	2621.407440	22.541235
92.589726	2618.963619	22.546253
92.692758	2606.460574	22.551271
92.267086	2608.768449	22.556288
92.620776	2617.730554	22.561306
92.809026	2621.962081	22.566323
93.000688	2634.078814	22.571341
93.170036	2638.926112	22.576359
93.084311	2634.092544	22.581376
93.229956	2636.958262	22.586394
93.369987	2640.686762	22.591411
93.285144	2628.147203	22.596429
93.550364	2639.954853	22.601447
93.350413	2636.543478	22.606464
93.206910	2642.822356	22.611482
93.825482	2647.563504	22.616499
93.766166	2654.304796	22.621517
93.964256	2653.182490	22.626535
94.089938	2644.577794	22.631552
94.458771	2651.301870	22.636570
94.373830	2646.870548	22.641587
94.345258	2649.065977	22.646605
94.355870	2639.341380	22.651623
94.447260	2643.524834	22.656640
94.087449	2652.081888	22.661658
94.503356	2663.274330	22.666675
94.431519	2686.119631	22.671693
94.852189	2678.313963	22.676711
94.859573	2670.932116	22.681728
95.042122	2680.939281	22.686746
95.264351	2669.039241	22.691763
95.009232	2682.974041	22.696781
95.272204	2688.002655	22.701799
95.630400	2699.063763	22.706816
95.677594	2702.697858	22.711834
95.997142	2702.894799	22.716851
95.708007	2697.351673	22.721869
96.177901	2693.626200	22.726887
95.788677	2697.063517	22.731904
95.849771	2697.472315	22.736922
95.723964	2687.764058	22.741939
95.858469	2700.823063	22.746957
96.042127	2711.380876	22.751975
96.665984	2712.270588	22.756992
96.527048	2729.459509	22.762010
96.704745	2726.757439	22.767027
96.435263	2732.835231	22.772045
96.350173	2732.449779	22.777063
96.667162	2731.747495	22.782080
96.747333	2759.937987	22.787098
96.944488	2756.416101	22.792115
97.011109	2767.240660	22.797133
97.100058	2766.844001	22.802151
97.325137	2768.146069	22.807168
97.151935	2782.796516	22.812186
97.145449	2778.597013	22.817203
97.364105	2797.592427	22.822221
97.978422	2780.460331	22.827239
98.022518	2770.637563	22.832256
98.092928	2764.894496	22.837274
98.175122	2765.497830	22.842291
98.111371	2775.454644	22.847309
98.408054	2789.601397	22.852327
98.636678	2794.132578	22.857344
98.524915	2792.123123	22.862362
98.912731	2790.799585	22.867379
99.104816	2790.504297	22.872397
98.887877	2784.798345	22.877415
98.860451	2786.211279	22.882432
98.832320	2787.419200	22.887450
99.036156	2778.236451	22.892467
99.360780	2791.452136	22.897485
99.028069	2784.409840	22.902503
99.155870	2790.115711	22.907520
99.086529	2811.088239	22.912538
99.124715	2800.667976	22.917555
99.193513	2813.926982	22.922573
99.499231	2816.298390	22.927591
100.002919	2819.984216	22.932608
99.997445	2836.863264	22.937626
100.063811	2834.699392	22.942643
100.231226	2845.034786	22.947661
100.279120	2838.693431	22.952679
100.424507	2833.997387	22.957696
100.323462	2843.134805	22.962714
100.634109	2837.722675	22.967731
100.299340	2841.756125	22.972749
100.523362	2854.220428	22.977767
100.794047	2865.090281	22.982784
100.720664	2867.027030	22.987802
100.824457	2866.435766	22.992819
100.820273	2874.672408	22.997837
100.775211	2879.239253	23.002855
101.546043	2886.445478	23.007872
101.667575	2893.054844	23.012890
101.632592	2886.490614	23.017907
101.706760	2889.704498	23.022925
101.587724	2892.659921	23.027943
101.888917	2892.340594	23.032960
101.937525	2889.695778	23.037978
101.890739	2889.868163	23.042995
101.764184	2893.069732	23.048013
102.012215	2903.235854	23.053031
102.568176	2907.350049	23.058048
102.234516	2921.798538	23.063066
102.431252	2911.279013	23.068083
102.292485	2914.510571	23.073101
102.449550	2911.231155	23.078119
102.556022	2920.595959	23.083136
102.685117	2937.721667	23.088154
102.998061	2932.976093	23.093171
102.906037	2945.957981	23.098189
102.728617	2938.329143	23.103207
103.448811	2948.068774	23.108224
103.084078	2966.282943	23.113242
103.560443	2967.435781	23.118259
103.691948	2972.948571	23.123277
103.700502	2962.839837	23.128295
104.047703	2972.754862	23.133312
103.834584	2995.008306	23.138330
104.362905	2992.921196	23.143347
104.475096	2994.259368	23.148365
104.223343	2999.251567	23.153383
104.523876	2996.754250	23.158400
104.538006	2988.069865	23.163418
104.722355	2992.818318	23.168435
104.740204	2980.727581	23.173453
104.919914	2994.096664	23.178471
104.919473	2994.114095	23.183488
104.769001	3018.263193	23.188506
105.210160	3022.764239	23.193523
104.840683	3018.543099	23.198541
105.025322	3020.622434	23.203559
105.773558	3035.024708	23.208576
105.710159	3044.761541	23.213594
105.920383	3045.977513	23.218611
106.282603	3048.428943	23.223629
106.096541	3049.111124	23.228647
106.574490	3037.048221	23.233664
106.264706	3058.622496	23.238682
106.198402	3046.008648	23.243699
106.479866	3040.880451	23.248717
106.151991	3047.826002	23.253735
106.243928	3048.006046	23.258752
106.203702	3041.104410	23.263770
106.591060	3052.922789	23.268787
106.465165	3060.214334	23.273805
106.591441	3072.061940	23.278823
106.506030	3069.288567	23.283840
106.547722	3098.144775	23.288858
106.796409	3101.276941	23.293875
107.223146	3099.929980	23.298893
107.227642	3118.900742	23.303911
107.521709	3125.890226	23.308928
107.479026	3133.538083	23.313946
107.733478	3130.486156	23.318963
108.288481	3124.934493	23.323981
108.107174	3123.185784	23.328999
108.236510	3117.977718	23.334016
108.416861	3119.872332	23.339034
108.394276	3113.311852	23.344051
108.614236	3124.302529	23.349069
108.921886	3139.380132	23.354087
108.932415	3138.062568	23.359104
109.141120	3150.183565	23.364122
109.153965	3127.840799	23.369139
109.274861	3111.854200	23.374157
109.191018	3107.022140	23.379175
108.734897	3125.144586	23.384192
109.122561	3141.286140	23.389210
108.955493	3139.298824	23.394227
109.362883	3135.745460	23.399245
109.421579	3142.661065	23.404263
109.765796	3151.063595	23.409280
109.945041	3152.087858	23.414298
110.109517	3150.012370	23.419315
110.070634	3149.035720	23.424333
110.096710	3147.411217	23.429351
110.205587	3147.088410	23.434368
110.526368	3152.466652	23.439386
110.222215	3170.594606	23.444403
110.170152	3176.847872	23.449421
110.183159	3185.788964	23.454439
110.827195	3186.122162	23.459456
110.699957	3207.865928	23.464474
110.902951	3208.260608	23.469491
111.221168	3206.697009	23.474509
110.979509	3206.889576	23.479527
111.317283	3207.860725	23.484544
111.679937	3232.286328	23.489562
111.792183	3235.140777	23.494579
112.233468	3230.243855	23.499597
111.981386	3234.762523	23.504615
112.064838	3229.649847	23.509632
112.153400	3227.622794	23.514650
112.447456	3231.776665	23.519667
112.581937	3223.555259	23.524685
112.142181	3235.022606	23.529703
112.320724	3229.789394	23.534720
112.384184	3237.770479	23.539738
112.536186	3253.005565	23.544755
112.539652	3256.975431	23.549773
112.329447	3266.834838	23.554791
113.284910	3280.067376	23.559808
113.304814	3284.928687	23.564826
113.295669	3283.801011	23.569843
113.306042	3280.171454	23.574861
113.463664	3292.626669	23.579879
113.844832	3280.726920	23.584896
113.977715	3301.682251	23.589914
114.303166	3303.497653	23.594931
114.441903	3300.297192	23.599949
114.416100	3295.744429	23.604967
114.615235	3293.711987	23.609984
114.673722	3293.940116	23.615002
115.185176	3291.664417	23.620019
115.219793	3288.884445	23.625037
115.075514	3277.202738	23.630055
114.924681	3265.896175	23.635072
115.332001	3272.979514	23.640090
114.975558	3281.461540	23.645107
115.094338	3283.656195	23.650125
114.735720	3292.249227	23.655143
115.066053	3297.499544	23.660160
115.132665	3295.928531	23.665178
115.084042	3312.892043	23.670195
115.386910	3320.264438	23.675213
115.308575	3322.687542	23.680231
115.604332	3338.286652	23.685248
115.884596	3346.466430	23.690266
115.592133	3350.370526	23.695283
115.625035	3348.596824	23.700301
116.028412	3372.169347	23.705319
116.223850	3377.971290	23.710336
116.234244	3378.450742	23.715354
116.405598	3384.754767	23.720371
116.913969	3396.711580	23.725389
116.855035	3406.367180	23.730407
117.140430	3402.634406	23.735424
117.363843	3403.954131	23.740442
117.403360	3408.083413	23.745459
117.568591	3403.282318	23.750477
117.457433	3410.846405	23.755495
117.358079	3432.057060	23.760512
117.741136	3428.456096	23.765530
117.634833	3433.441980	23.770547
117.890933	3435.240967	23.775565
117.803643	3448.046484	23.780583
118.104457	3453.759677	23.785600
118.885318	3443.664823	23.790618
118.706496	3451.508704	23.795635
119.152255	3432.217088	23.800653
119.291662	3451.257576	23.805671
119.196157	3438.924667	23.810688
119.387539	3436.863964	23.815706
119.251576	3440.922407	23.820723
119.341645	3437.255946	23.825741
119.081984	3444.959699	23.830759
119.457238	3444.587895	23.835776
119.818286	3469.245655	23.840794
119.441753	3461.650041	23.845811
119.728050	3473.756822	23.850829
119.819518	3471.475294	23.855847
119.821044	3473.925705	23.860864
119.838222	3483.874246	23.865882
119.945423	3502.025966	23.870899
120.319844	3491.452900	23.875917
120.179040	3511.444841	23.880935
120.470497	3524.972992	23.885952
120.899282	3528.220607	23.890970
120.932108	3539.941172	23.895987
121.064053	3529.520985	23.901005
120.833336	3534.453946	23.906023
121.291069	3540.345446	23.911040
121.916497	3539.953722	23.916058
121.744070	3544.474203	23.921075
122.044085	3543.447116	23.926093
122.088723	3544.915865	23.931111
122.154789	3539.716204	23.936128
122.310753	3540.045474	23.941146
122.305655	3547.436081	23.946163
122.349159	3540.430143	23.951181
122.687309	3544.051521	23.956199
122.497731	3540.159038	23.961216
122.350096	3549.158533	23.966234
122.518708	3571.093035	23.971251
122.670837	3576.275412	23.976269
122.789260	3584.434962	23.981287
122.699878	3601.999323	23.986304
122.799623	3598.643847	23.991322
122.739631	3606.713753	23.996339
123.495557	3616.913276	24.001357
123.489478	3635.982498	24.006375
123.371324	3639.171010	24.011392
123.685123	3630.640034	24.016410
124.006342	3628.387240	24.021427
124.109637	3632.395342	24.026445
124.310769	3635.000029	24.031463
124.589161	3644.446160	24.036480
125.064639	3645.124742	24.041498
125.111141	3652.370982	24.046515
125.015059	3634.217699	24.051533
125.112719	3642.306312	24.056551
124.910833	3647.819226	24.061568
125.328172	3639.443499	24.066586
125.275660	3645.734038	24.071603
125.497916	3636.719399	24.076621
125.095895	3638.101341	24.081639
125.120554	3649.775702	24.086656
125.588224	3653.049957	24.091674
125.440903	3668.577736	24.096691
125.721165	3676.467106	24.101709
125.727757	3675.064709	24.106727
125.734189	3686.325939	24.111744
125.949441	3702.577051	24.116762
125.886692	3703.355314	24.121779
126.345253	3721.072481	24.126797
126.543723	3727.076829	24.131815
126.451347	3732.293984	24.136832
127.157953	3737.616978	24.141850
127.153682	3754.584229	24.146867
127.436183	3739.018612	24.151885
127.650345	3746.731973	24.156903
127.836587	3746.422285	24.161920
128.045778	3735.867063	24.166938
127.707511	3750.849818	24.171955
128.079901	3746.885159	24.176973
128.467289	3738.670279	24.181991
128.525981	3737.958117	24.187008
128.683491	3735.953798	24.192026
128.548430	3735.449050	24.197043
128.832466	3730.939565	24.202061
128.785402	3744.899402	24.207079
128.711151	3761.829860	24.212096
129.040856	3770.622978	24.217114
128.814676	3776.309679	24.222131
128.707687	3770.856777	24.227149
128.828211	3772.017234	24.232167
128.741194	3792.999924	24.237184
128.952705	3806.962128	24.242202
128.827939	3827.807813	24.247219
128.718260	3832.164388	24.252237
129.225500	3849.079027	24.257255
129.817399	3852.711861	24.262272
130.436975	3861.555298	24.267290
130.530186	3878.298978	24.272307
130.870501	3876.437513	24.277325
131.048625	3879.196478	24.282343
131.013380	3882.255106	24.287360
131.410390	3877.946911	24.292378
131.609599	3869.145837	24.297395
131.703741	3871.739601	24.302413
131.669699	3875.524101	24.307431
131.509954	3881.836885	24.312448
131.621241	3872.787395	24.317466
131.667872	3877.292044	24.322483
131.458191	3864.663166	24.327501
131.753299	3868.869010	24.332519
131.832217	3890.706648	24.337536
132.033824	3884.962237	24.342554
131.777158	3902.113340	24.347571
132.266334	3902.773121	24.352589
132.189797	3921.572474	24.357607
132.159690	3931.818171	24.362624
132.385012	3929.639152	24.367642
132.769304	3938.553232	24.372659
133.028023	3944.064520	24.377677
133.215597	3944.931923	24.382695
133.049098	3950.326449	24.387712
133.390444	3944.361920	24.392730
133.118342	3958.460144	24.397747
133.506403	3975.044681	24.402765
133.631998	3972.668028	24.407783
133.614591	3991.701371	24.412800
133.919642	4001.233064	24.417818
134.254640	4011.578398	24.422835
134.131369	4013.588941	24.427853
134.349018	4002.653739	24.432871
134.557747	4039.953936	24.437888
134.816716	4031.394449	24.442906
134.828924	4039.956977	24.447923
134.844826	4046.427279	24.452941
135.467032	4052.271169	24.457959
135.312748	4048.393169	24.462976
135.435827	4049.830424	24.467994
135.863650	4061.920839	24.473011
136.072151	4062.620575	24.478029
136.158635	4050.383336	24.483047
136.261226	4057.380254	24.488064
136.437649	4055.080193	24.493082
136.365337	4043.584798	24.498099
136.446125	4065.462137	24.503117
136.498403	4073.517171	24.508135
136.455286	4079.263730	24.513152
136.539440	4081.388258	24.518170
136.749886	4100.163761	24.523187
137.000374	4099.044856	24.528205
137.395277	4095.719765	24.533223
137.321498	4106.515033	24.538240
137.543014	4102.786804	24.543258
138.035747	4126.434216	24.548275
137.893018	4126.068937	24.553293
138.007232	4131.066435	24.558311
138.247430	4140.762555	24.563328
138.368283	4137.293206	24.568346
138.133181	4136.729073	24.573363
137.999153	4154.714522	24.578381
138.807268	4160.485429	24.583399
138.586793	4162.286522	24.588416
138.600576	4162.093293	24.593434
138.682653	4184.247788	24.598451
138.856456	4195.159084	24.603469
139.307525	4204.215392	24.608487
139.094816	4206.990142	24.613504
139.720897	4212.401104	24.618522
139.968549	4223.548609	24.623539
139.460721	4217.637281	24.628557
140.049275	4228.623794	24.633575
140.335692	4252.073363	24.638592
140.487715	4243.745343	24.643610
140.992351	4255.104928	24.648627
140.754841	4243.849074	24.653645
140.721817	4244.814578	24.658663
140.966524	4251.189060	24.663680
140.979769	4259.138454	24.668698
141.286685	4265.546705	24.673715
141.022611	4270.010959	24.678733
141.387200	4268.671478	24.683751
141.586436	4292.020616	24.688768
141.781841	4287.726125	24.693786
141.630337	4288.545154	24.698803
141.796158	4295.309984	24.703821
142.342635	4287.558222	24.708839
142.185595	4289.757903	24.713856
142.783112	4295.462661	24.718874
143.019451	4305.919482	24.723891
142.909508	4317.351314	24.728909
143.048714	4312.200670	24.733927
142.764319	4318.779656	24.738944
142.739472	4307.993216	24.743962
143.249718	4311.819285	24.748979
143.284070	4328.243651	24.753997
143.715022	4338.493324	24.759015
143.516244	4338.308245	24.764032
143.854680	4337.422780	24.769050
144.010930	4339.577495	24.774067
143.693726	4358.594556	24.779085
144.051487	4357.098699	24.784103
143.965638	4368.976239	24.789120
144.163113	4385.121550	24.794138
144.186065	4401.300604	24.799155
144.089213	4405.637880	24.804173
144.387021	4420.757736	24.809191
144.526144	4438.353182	24.814208
144.715437	4458.295806	24.819226
145.328810	4461.970108	24.824243
145.347099	4474.382480	24.829261
146.060785	4472.606172	24.834279
146.051106	4484.707401	24.839296
146.367777	4479.854825	24.844314
146.261054	4485.767245	24.849331
146.265803	4483.973286	24.854349
146.641629	4473.909256	24.859367
146.948673	4503.074804	24.864384
147.058564	4500.934184	24.869402
147.026577	4505.741889	24.874419
146.797453	4505.658717	24.879437
147.267143	4507.559763	24.884455
147.468970	4512.658592	24.889472
147.529760	4530.758578	24.894490
147.889705	4527.876288	24.899507
147.676469	4540.034223	24.904525
148.064935	4535.670570	24.909543
148.287465	4539.346836	24.914560
148.428210	4553.214756	24.919578
148.882130	4559.585313	24.924595
148.798040	4556.370437	24.929613
149.053409	4563.491431	24.934631
149.150188	4559.557408	24.939648
148.758712	4561.439331	24.944666
149.211417	4554.360611	24.949683
149.062545	4587.816951	24.954701
149.675136	4579.002704	24.959719
149.153050	4584.772336	24.964736
149.660687	4580.477859	24.969754
150.022869	4603.839762	24.974771
149.972389	4615.642308	24.979789
150.063169	4611.559637	24.984807
150.007704	4622.313233	24.989824
150.437013	4635.715093	24.994842
150.435353	4647.772589	24.999859
150.338820	4651.940558	25.004877
150.693931	4661.488751	25.009895
150.810383	4672.985600	25.014912
150.680153	4680.106145	25.019930
151.516909	4674.114148	25.024947
152.319532	4676.519833	25.029965
153.077038	4666.693096	25.034983
152.842043	4664.023048	25.040000
152.398110	4645.341649	25.045018
152.863328	4645.123408	25.050035
152.959471	4643.111847	25.055053
153.029283	4637.669427	25.060071
152.698125	4637.346471	25.065088
152.690553	4634.469317	25.070106
153.245556	4638.382536	25.075123
153.242007	4637.056160	25.080141
153.192022	4630.902815	25.085159
153.645190	4663.600108	25.090176
153.309299	4659.933266	25.095194
153.363625	4662.026210	25.100211
153.340818	4666.622166	25.105229
153.432564	4690.705632	25.110247
153.845515	4695.137832	25.115264
153.674892	4708.344119	25.120282
153.938792	4725.808112	25.125299
154.072779	4728.896667	25.130317
154.635407	4746.433112	25.135335
154.810698	4770.407525	25.140352
154.920848	4764.377939	25.145370
154.755195	4771.326427	25.150387
155.128980	4783.496473	25.155405
155.361765	4778.022199	25.160423
155.551689	4787.791654	25.165440
155.294139	4809.732947	25.170458
155.654874	4817.786329	25.175475
155.705916	4821.989674	25.180493
156.214249	4834.509124	25.185511
157.386324	4820.029098	25.190528
157.268760	4825.472495	25.195546
157.693870	4811.496984	25.200563
157.563262	4823.642983	25.205581
157.701106	4815.795058	25.210599
157.982574	4821.943153	25.215616
157.833518	4813.296292	25.220634
157.864669	4811.322286	25.225651
157.701128	4813.791672	25.230669
157.998619	4820.510437	25.235687
158.193014	4819.685897	25.240704
157.784779	4847.565964	25.245722
158.375426	4845.287132	25.250739
158.540342	4848.032714	25.255757
158.435480	4864.176781	25.260775
159.024390	4875.047138	25.265792
158.988719	4889.573922	25.270810
158.686582	4879.668756	25.275827
158.871351	4900.120663	25.280845
159.200402	4907.767468	25.285863
159.592557	4915.377014	25.290880
159.731991	4937.299771	25.295898
159.597909	4946.742779	25.300915
159.727778	4949.706841	25.305933
159.576681	4957.850859	25.310951
160.333647	4965.776259	25.315968
160.423426	4973.095068	25.320986
160.806646	4995.840556	25.326003
160.757971	4992.159774	25.331021
160.906013	5001.997752	25.336039
161.107566	5006.899899	25.341056
160.949238	5025.997684	25.346074
161.467027	5028.038866	25.351091
161.646065	5042.524600	25.356109
161.953653	5061.035457	25.361127
161.933169	5057.968207	25.366144
161.934467	5063.313966	25.371162
162.421932	5071.801629	25.376179
162.605960	5081.595874	25.381197
162.781843	5092.262520	25.386215
162.662591	5083.691675	25.391232
162.681747	5086.511136	25.396250
163.169439	5103.577661	25.401267
163.085570	5111.803518	25.406285
163.282361	5110.225658	25.411303
163.639669	5113.302383	25.416320
163.635146	5135.433627	25.421338
164.009987	5146.035746	25.426355
163.913230	5142.885859	25.431373
163.940382	5160.032909	25.436391
164.399746	5158.857174	25.441408
164.670163	5176.668688	25.446426
164.935792	5164.459095	25.451443
164.665193	5177.796584	25.456461
165.309985	5197.379361	25.461479
165.424530	5199.993189	25.466496
165.227659	5208.985273	25.471514
165.339648	5208.463444	25.476531
165.425275	5212.837561	25.481549
165.633274	5226.460994	25.486567
166.179984	5235.998179	25.491584
166.108033	5253.563458	25.496602
166.337964	5247.019192	25.501619
166.556152	5253.170885	25.506637
166.020947	5269.499496	25.511655
166.507584	5278.302437	25.516672
166.797295	5297.152047	25.521690
166.978159	5311.748774	25.526707
167.500957	5309.096820	25.531725
167.711247	5321.800860	25.536743
168.311704	5330.201371	25.541760
168.238716	5330.220620	25.546778
168.588759	5327.116951	25.551795
168.767016	5321.772049	25.556813
168.820820	5327.213919	25.561831
169.012733	5326.027484	25.566848
169.031457	5336.194313	25.571866
169.310569	5336.700842	25.576883
169.472473	5343.389595	25.581901
169.302706	5361.965952	25.586919
169.760566	5356.401311	25.591936
169.737891	5354.421218	25.596954
169.859351	5361.218296	25.601971
170.198163	5389.155538	25.606989
169.827484	5388.763522	25.612007
170.296028	5393.775004	25.617024
170.129128	5399.721392	25.622042
170.543142	5424.273019	25.627059
170.328985	5415.799671	25.632077
170.824120	5438.828058	25.637095
171.192623	5444.720939	25.642112
171.331387	5457.480291	25.647130
171.402209	5474.415657	25.652147
171.407823	5482.461447	25.657165
171.627841	5482.665133	25.662183
172.284726	5497.666507	25.667200
172.275765	5499.759053	25.672218
172.446267	5508.399646	25.677236
172.844029	5510.430123	25.682253
173.127870	5524.491708	25.687271
173.037267	5532.399146	25.692288
173.134457	5533.279297	25.697306
173.538881	5517.252591	25.702324
173.488444	5517.511456	25.707341
173.839617	5530.235572	25.712359
174.131195	5540.543063	25.717376
174.352768	5544.448913	25.722394
174.066969	5549.889009	25.727412
174.504050	5540.141760	25.732429
174.881447	5553.282894	25.737447
174.862654	5545.419681	25.742464
174.453779	5546.809217	25.747482
174.604977	5565.902689	25.752500
174.946504	5571.581152	25.757517
175.135385	5575.001778	25.762535
175.244118	5593.121798	25.767552
175.228644	5601.578334	25.772570
175.628984	5618.830054	25.777588
175.802520	5627.339469	25.782605
176.088978	5631.707898	25.787623
176.055982	5633.895815	25.792640
176.062119	5658.673100	25.797658
176.370547	5659.704816	25.802676
176.405242	5674.030034	25.807693
176.567608	5682.579139	25.812711
177.335506	5689.672978	25.817728
177.420055	5696.965428	25.822746
177.442983	5711.915618	25.827764
177.822737	5714.804439	25.832781
178.131806	5731.755625	25.837799
178.597725	5735.045979	25.842816
178.382216	5737.843905	25.847834
178.585771	5738.790667	25.852852
178.781871	5738.924297	25.857869
178.932282	5753.164989	25.862887
179.165232	5753.862713	25.867904
178.852053	5761.903336	25.872922
179.133809	5772.448889	25.877940
179.478689	5786.443859	25.882957
179.260181	5801.431102	25.887975
179.801317	5818.527330	25.892992
179.570841	5830.936427	25.898010
180.198530	5843.705425	25.903028
180.588591	5849.147522	25.908045
180.638028	5863.761873	25.913063
180.857396	5871.340740	25.918080
181.013585	5876.828796	25.923098
181.211383	5881.404201	25.928116
181.318776	5892.004798	25.933133
181.929997	5910.615848	25.938151
181.870162	5905.992373	25.943168
181.760627	5913.582594	25.948186
182.046339	5927.064555	25.953204
182.720016	5923.060325	25.958221
183.325168	5929.846587	25.963239
183.294723	5924.023432	25.968256
183.123033	5926.376204	25.973274
183.260554	5924.467083	25.978292
183.665070	5926.818623	25.983309
183.930093	5949.983659	25.988327
184.070085	5945.923971	25.993344
184.115175	5959.478234	25.998362
184.010975	5950.700427	26.003380
184.433892	5946.841034	26.008397
184.378393	5969.738804	26.013415
184.442907	5970.750427	26.018432
184.289461	5974.453276	26.023450
184.496972	5998.093413	26.028468
185.023887	6002.670087	26.033485
184.642263	6015.624262	26.038503
185.222792	6028.821042	26.043520
185.302408	6049.329720	26.048538
186.593753	6036.068477	26.053556
188.012056	6023.874622	26.058573
188.030327	6009.559254	26.063591
188.161457	5981.969771	26.068608
188.021962	5965.805374	26.073626
188.104304	5958.606426	26.078644
188.070744	5947.306006	26.083661
187.811531	5933.140777	26.088679
187.915770	5910.607562	26.093696
188.107530	5918.608468	26.098714
187.930919	5923.948638	26.103732
188.046708	5913.868623	26.108749
188.153498	5940.682901	26.113767
188.449236	5951.416064	26.118784
188.475395	5943.949222	26.123802
188.029336	5954.787530	26.128820
188.411531	5970.583225	26.133837
188.421533	5994.606660	26.138855
188.522018	6008.670005	26.143872
188.971184	6021.136443	26.148890
188.438881	6046.980436	26.153908
188.684638	6061.749801	26.158925
188.662229	6076.570040	26.163943
189.062981	6098.027259	26.168960
189.498034	6127.418712	26.173978
189.545551	6149.406475	26.178996
190.050705	6172.321645	26.184013
190.247228	6193.822382	26.189031
190.667830	6205.921171	26.194048
191.273981	6211.876458	26.199066
191.316788	6237.178622	26.204084
191.761640	6237.393794	26.209101
192.075283	6252.873514	26.214119
192.437078	6257.851032	26.219136
192.668722	6273.620852	26.224154
192.517778	6272.883551	26.229172
192.809518	6267.700628	26.234189
192.777074	6278.925672	26.239207
193.139818	6285.971327	26.244224
193.365588	6294.392087	26.249242
193.185055	6293.877085	26.254260
193.628094	6310.548296	26.259277
193.598039	6320.701022	26.264295
193.967234	6316.064424	26.269312
194.540396	6340.793456	26.274330
194.293654	6344.042471	26.279348
194.471834	6346.502570	26.284365
194.849201	6353.703350	26.289383
194.972299	6376.848489	26.294400
194.885814	6379.774736	26.299418
195.176876	6394.106055	26.304436
195.598330	6397.605573	26.309453
195.986773	6412.566579	26.314471
196.110393	6409.428652	26.319488
196.493342	6423.156374	26.324506
197.261369	6406.614684	26.329524
198.339022	6388.417174	26.334541
198.336693	6378.228895	26.339559
198.611296	6361.744822	26.344576
198.901013	6348.170879	26.349594
198.794402	6333.151356	26.354612
198.954814	6320.796107	26.359629
198.498721	6318.433450	26.364647
198.939404	6315.754813	26.369664
198.976380	6314.523953	26.374682
198.514946	6314.199758	26.379700
198.998978	6307.977504	26.384717
198.935257	6320.065494	26.389735
198.798034	6336.133741	26.394752
198.849333	6340.606029	26.399770
198.471210	6348.526992	26.404788
198.926394	6360.520916	26.409805
198.895995	6384.577648	26.414823
199.384135	6400.811418	26.419840
199.614591	6415.528524	26.424858
199.230670	6426.815225	26.429876
199.709648	6437.812846	26.434893
200.341222	6459.470070	26.439911
200.732351	6461.455308	26.444928
201.451879	6469.991028	26.449946
201.416342	6485.899183	26.454964
201.406452	6485.573206	26.459981
201.641707	6492.066744	26.464999
201.777377	6507.644023	26.470016
201.989284	6517.329777	26.475034
201.849185	6530.421457	26.480052
201.964132	6543.299853	26.485069
202.234796	6558.921701	26.490087
202.161570	6577.762265	26.495104
202.449387	6600.855159	26.500122
202.785294	6617.049073	26.505140
202.978863	6617.556474	26.510157
203.508051	6633.436317	26.515175
203.729416	6643.455322	26.520192
204.119069	6656.292892	26.525210
204.041977	6676.846539	26.530228
204.419784	6681.503326	26.535245
204.687912	6704.798128	26.540263
204.635194	6707.541606	26.545280
205.078600	6716.693592	26.550298
205.173913	6734.468228	26.555316
205.231898	6743.153399	26.560333
205.578160	6752.271137	26.565351
205.388024	6769.471792	26.570368
206.073096	6792.322527	26.575386
206.103856	6808.161703	26.580404
206.366944	6813.922178	26.585421
206.253618	6841.892224	26.590439
206.475532	6843.117983	26.595456
207.320532	6858.841610	26.600474
207.360129	6882.323510	26.605492
207.975097	6885.209702	26.610509
207.840450	6888.440988	26.615527
208.302512	6894.514997	26.620544
209.016652	6910.309254	26.625562
209.048800	6910.980537	26.630580
209.655522	6894.821163	26.635597
209.923554	6895.649377	26.640615
210.402108	6884.074162	26.645632
210.392850	6883.427499	26.650650
210.278722	6889.982403	26.655668
210.555861	6884.981291	26.660685
210.527321	6880.088468	26.665703
210.271080	6881.121939	26.670720
210.919071	6882.747132	26.675738
211.003363	6890.137845	26.680756
210.990444	6897.905456	26.685773
210.952435	6905.766245	26.690791
210.760589	6919.175601	26.695808
211.461058	6925.743250	26.700826
211.613385	6931.709632	26.705844
211.838928	6944.655046	26.710861
211.914088	6957.916100	26.715879
212.023561	6970.175871	26.720896
212.469941	6993.337511	26.725914
212.165953	6995.325682	26.730932
212.720321	7015.165991	26.735949
212.755242	7030.120161	26.740967
212.719407	7037.554532	26.745984
213.105490	7054.240720	26.751002
213.200898	7075.066318	26.756020
213.479972	7095.183251	26.761037
214.243493	7106.939838	26.766055
213.708655	7110.373140	26.771072
214.246105	7127.172883	26.776090
214.256412	7156.795146	26.781108
214.473114	7162.746981	26.786125
214.912137	7177.943699	26.791143
214.964848	7207.692913	26.796160
215.383102	7210.062062	26.801178
215.463501	7230.047556	26.806196
215.787040	7233.789593	26.811213
215.971201	7255.586051	26.816231
216.172272	7273.752518	26.821248
216.742595	7264.659476	26.826266
216.965231	7280.427859	26.831284
217.039216	7288.143414	26.836301
217.547947	7310.550024	26.841319
217.614426	7316.252768	26.846336
217.578470	7322.912225	26.851354
218.086858	7339.468119	26.856372
218.098489	7340.314542	26.861389
218.441372	7352.362539	26.866407
218.737670	7380.179616	26.871424
219.015820	7371.116943	26.876442
218.926713	7390.108403	26.881460
219.339905	7397.294259	26.886477
219.506276	7410.995812	26.891495
219.387134	7432.467974	26.896512
220.053775	7439.673965	26.901530
220.012448	7455.427304	26.906548
219.941460	7456.524551	26.911565
220.268306	7486.821861	26.916583
220.670071	7501.765934	26.921600
221.069815	7518.180168	26.926618
221.244781	7525.873546	26.931636
221.283934	7533.461889	26.936653
221.555757	7545.784926	26.941671
221.857562	7565.904982	26.946688
222.355020	7563.983123	26.951706
222.691447	7588.376933	26.956724
222.789043	7585.499097	26.961741
223.104523	7603.387785	26.966759
223.012933	7615.938247	26.971776
223.526618	7617.800875	26.976794
223.913846	7629.287185	26.981812
224.036862	7634.426908	26.986829
224.398100	7641.948397	26.991847
224.094564	7662.659095	26.996864
224.730619	7660.462926	27.001882
224.883574	7673.465893	27.006900
225.398054	7683.374629	27.011917
225.749320	7689.437425	27.016935
225.940855	7689.244158	27.021952
226.335414	7690.905249	27.026970
226.099888	7689.198897	27.031988
226.057763	7704.885663	27.037005
226.192575	7706.496177	27.042023
226.219532	7727.467122	27.047040
226.752346	7736.694644	27.052058
227.185762	7743.864696	27.057076
226.999793	7757.584917	27.062093
227.354132	7767.601446	27.067111
227.390700	7783.891190	27.072128
227.985434	7793.963892	27.077146
228.321742	7813.138023	27.082164
228.151570	7819.494670	27.087181
228.732706	7824.358262	27.092199
228.964653	7842.937730	27.097216
229.109015	7839.006806	27.102234
229.484139	7854.828406	27.107252
229.446009	7853.942315	27.112269
230.106757	7855.158259	27.117287
230.122225	7843.819196	27.122304
230.444115	7855.841921	27.127322
230.606776	7864.663127	27.132340
230.844565	7877.263832	27.137357
231.384680	7880.231968	27.142375
231.274935	7880.125780	27.147392
231.350609	7894.216188	27.152410
231.736184	7903.454094	27.157428
231.753662	7902.136554	27.162445
231.825149	7920.976719	27.167463
231.814044	7936.512834	27.172480
232.248642	7961.355650	27.177498
232.308169	7963.577353	27.182516
232.585698	7984.492826	27.187533
232.984894	7985.846762	27.192551
233.105700	8012.830783	27.197568
233.707457	8018.669340	27.202586
234.008697	8028.842946	27.207604
234.142899	8055.930367	27.212621
234.500856	8063.358079	27.217639
234.388730	8073.230170	27.222656
234.664439	8087.030721	27.227674
235.135728	8101.870073	27.232692
234.946037	8127.908638	27.237709
235.620033	8128.210237	27.242727
235.405565	8150.354578	27.247744
235.839130	8158.609473	27.252762
236.072095	8177.891801	27.257780
235.963454	8189.175754	27.262797
236.706331	8198.905866	27.267815
236.608420	8214.648877	27.272832
236.735901	8233.116971	27.277850
237.260122	8246.173729	27.282868
237.280973	8267.156640	27.287885
237.978951	8270.021427	27.292903
238.396725	8288.187710	27.297920
239.117772	8290.849376	27.302938
238.866361	8299.478098	27.307956
239.157422	8299.271441	27.312973
239.515984	8311.218311	27.317991
239.137194	8323.834376	27.323008
239.564029	8326.045516	27.328026
239.905720	8336.462306	27.333044
239.726237	8362.326258	27.338061
240.046168	8370.335469	27.343079
240.159684	8384.787102	27.348096
240.409963	8410.995647	27.353114
240.669313	8425.373461	27.358132
240.570722	8437.362508	27.363149
240.974840	8461.885840	27.368167
241.452023	8477.066437	27.373184
241.892386	8493.533224	27.378202
242.473836	8500.864930	27.383220
242.953584	8509.614906	27.388237
244.035535	8500.017094	27.393255
244.372364	8500.284133	27.398272
244.753533	8485.007445	27.403290
245.252531	8472.888885	27.408308
245.315787	8471.699181	27.413325
245.279687	8461.675086	27.418343
245.128528	8461.191362	27.423360
245.100979	8462.756459	27.428378
245.645049	8460.759800	27.433396
245.403697	8466.245487	27.438413
245.720495	8458.935561	27.443431
245.450456	8465.492595	27.448448
245.776306	8464.230905	27.453466
245.985087	8475.872728	27.458484
245.669977	8497.168558	27.463501
246.125607	8494.343719	27.468519
246.030520	8523.013977	27.473536
246.133572	8537.708534	27.478554
246.280921	8562.741807	27.483572
246.604890	8589.195991	27.488589
246.737393	8606.761730	27.493607
247.151414	8621.723730	27.498624
247.147816	8657.441857	27.503642
247.625859	8678.358800	27.508660
247.813536	8702.856233	27.513677
248.037147	8725.500484	27.518695
248.302134	8748.569574	27.523712
248.395360	8767.635572	27.528730
248.956322	8791.700883	27.533748
249.313941	8816.583820	27.538765
250.111736	8818.103992	27.543783
250.207574	8834.807980	27.548800
250.403251	8857.387737	27.553818
250.793951	8872.955686	27.558836
250.802206	8894.858451	27.563853
251.171264	8912.935073	27.568871
251.284594	8915.887666	27.573888
251.685330	8931.872300	27.578906
252.610283	8936.145812	27.583924
252.650520	8948.799094	27.588941
253.022255	8954.539150	27.593959
253.214542	8959.629981	27.598976
253.597068	8976.116332	27.603994
253.697251	8983.371460	27.609012
254.012987	8999.371071	27.614029
254.223481	9004.609352	27.619047
254.261176	9002.625862	27.624064
254.459222	9023.536999	27.629082
254.944756	9026.762570	27.634100
254.994006	9045.525043	27.639117
255.224264	9054.608242	27.644135
255.185269	9074.468575	27.649152
255.102085	9085.733962	27.654170
255.885737	9111.276040	27.659188
255.815993	9134.691984	27.664205
256.104268	9143.214162	27.669223
256.474778	9168.673723	27.674240
256.480154	9197.809031	27.679258
256.994877	9209.734571	27.684276
256.990886	9236.167113	27.689293
257.645189	9243.172743	27.694311
257.922886	9256.889688	27.699328
258.052954	9285.174133	27.704346
258.490666	9277.354545	27.709364
258.389939	9301.172126	27.714381
259.124383	9310.126802	27.719399
259.293592	9331.387387	27.724416
259.411197	9336.478142	27.729434
259.956968	9359.709436	27.734452
260.280312	9364.519446	27.739469
260.911807	9371.993709	27.744487
261.300738	9389.323913	27.749504
261.212494	9392.632283	27.754522
261.435447	9393.670584	27.759540
261.327800	9400.874564	27.764557
261.683944	9418.790048	27.769575
261.893776	9418.989977	27.774592
261.921510	9436.884417	27.779610
262.155712	9443.833102	27.784628
262.330431	9461.211578	27.789645
262.821420	9481.390855	27.794663
263.058182	9474.581401	27.799680
263.341402	9495.883134	27.804698
264.162334	9497.835964	27.809716
263.741671	9514.517759	27.814733
264.378058	9532.133147	27.819751
264.448696	9535.390729	27.824768
264.694527	9555.964543	27.829786
265.110694	9557.864098	27.834804
264.888483	9578.297487	27.839821
265.107856	9595.924719	27.844839
266.461455	9611.378318	27.849856
266.329899	9622.286587	27.854874
266.706402	9618.937435	27.859892
266.566873	9641.288024	27.864909
266.973898	9640.468888	27.869927
267.490504	9661.705284	27.874944
267.480616	9676.670954	27.879962
268.078451	9673.342528	27.884980
268.406835	9687.754127	27.889997
268.295907	9703.748127	27.895015
268.756623	9709.572148	27.900032
268.860634	9727.938731	27.905050
269.214228	9735.078834	27.910068
269.185963	9755.893028	27.915085
269.385968	9769.084472	27.920103
269.575647	9784.211671	27.925120
269.916649	9801.507745	27.930138
269.971600	9823.436320	27.935156
270.520344	9839.349219	27.940173
270.873859	9854.904610	27.945191
271.228556	9878.552060	27.950208
271.208749	9887.188845	27.955226
271.764950	9899.780003	27.960244
272.341553	9926.730131	27.965261
272.712963	9925.698679	27.970279
272.863961	9940.781245	27.975296
272.966042	9954.424764	27.980314
272.898951	9961.697885	27.985332
273.318816	9989.267371	27.990349
273.255360	9998.364453	27.995367
273.880292	10017.771380	28.000384
274.332566	10044.380760	28.005402
274.556848	10045.663892	28.010420
274.432930	10068.582063	28.015437
274.693489	10091.414333	28.020455
274.907334	10107.555668	28.025472
274.875804	10135.547822	28.030490
275.209384	10153.266987	28.035508
275.737507	10184.830351	28.040525
276.196954	10209.823012	28.045543
276.443712	10227.109206	28.050560
276.718539	10242.355043	28.055578
277.500180	10242.729418	28.060596
277.529978	10260.691398	28.065613
278.028261	10275.628346	28.070631
278.579931	10282.048025	28.075648
278.706954	10291.383060	28.080666
279.333746	10313.103854	28.085684
279.346813	10320.708883	28.090701
279.403287	10322.800645	28.095719
279.501199	10335.434409	28.100736
279.419426	10347.734063	28.105754
279.760236	10364.395795	28.110772
280.269030	10386.692493	28.115789
280.255411	10391.370507	28.120807
280.961506	10420.791832	28.125824
280.696211	10435.058510	28.130842
281.257925	10448.910492	28.135860
281.509543	10468.409136	28.140877
281.579994	10486.945241	28.145895
281.641377	10504.555601	28.150912
281.901311	10533.454082	28.155930
282.144484	10560.967244	28.160948
282.624969	10587.590170	28.165965
282.741563	10603.803309	28.170983
283.070531	10624.391467	28.176000
283.198427	10653.768256	28.181018
283.954386	10670.147043	28.186036
284.169696	10693.333545	28.191053
284.352717	10720.808915	28.196071
284.665961	10728.561226	28.201088
284.913035	10753.359180	28.206106
285.473356	10779.547667	28.211124
285.654566	10789.364025	28.216141
285.985634	10818.257502	28.221159
286.451699	10830.081254	28.226176
286.859273	10850.183937	28.231194
287.205650	10863.856972	28.236212
287.444451	10888.442214	28.241229
287.573470	10895.719416	28.246247
287.915892	10919.531159	28.251264
287.774844	10930.450554	28.256282
288.505953	10943.063900	28.261300
289.567998	10955.151142	28.266317
289.893778	10960.186557	28.271335
290.343126	10962.921409	28.276352
290.309339	10977.751233	28.281370
290.858266	10981.695440	28.286388
291.015086	10987.346669	28.291405
290.760287	11003.221682	28.296423
291.425316	11009.804817	28.301440
291.295150	11020.492413	28.306458
291.919876	11036.172494	28.311476
291.899649	11054.370570	28.316493
291.853781	11067.735499	28.321511
292.190839	11086.298121	28.326528
292.208143	11104.702739	28.331546
292.454570	11126.034807	28.336564
292.781447	11158.112534	28.341581
292.658303	11187.490243	28.346599
293.526637	11198.193281	28.351616
293.984757	11219.217704	28.356634
294.765383	11236.559681	28.361652
294.607531	11247.740500	28.366669
294.729222	11277.288845	28.371687
295.527007	11282.668243	28.376704
295.218827	11310.542155	28.381722
295.666786	11327.520352	28.386740
296.189632	11334.661418	28.391757
296.152627	11368.394658	28.396775
296.692833	11380.800553	28.401792
297.042022	11402.360154	28.406810
297.398756	11429.389513	28.411828
297.928939	11432.115746	28.416845
298.063537	11459.330178	28.421863
298.203799	11473.817968	28.426880
298.523131	11489.605955	28.431898
298.801340	11507.119934	28.436916
298.996965	11543.583487	28.441933
299.321436	11538.513989	28.446951
300.510344	11538.644266	28.451968
300.607771	11544.062892	28.456986
301.028850	11545.991029	28.462004
301.685819	11549.225673	28.467021
301.722565	11557.306382	28.472039
301.608438	11558.666344	28.477056
301.854965	11580.826269	28.482074
302.039739	11579.213545	28.487092
302.188876	11595.883972	28.492109
302.210458	11612.273060	28.497127
302.446914	11631.517994	28.502144
302.721928	11650.376785	28.507162
302.785416	11668.318976	28.512180
303.201674	11693.184815	28.517197
303.185026	11722.539500	28.522215
303.639075	11743.078370	28.527232
303.960972	11776.677199	28.532250
304.500590	11797.665202	28.537268
304.928603	11816.207250	28.542285
305.320533	11837.126869	28.547303
305.574074	11854.090646	28.552320
305.845269	11874.597030	28.557338
306.016133	11894.065904	28.562356
306.851818	11913.211624	28.567373
306.920940	11937.925929	28.572391
307.354662	11953.566151	28.577408
307.332103	11971.469396	28.582426
307.494974	12003.051306	28.587444
308.097353	12023.351582	28.592461
308.471027	12045.796728	28.597479
308.701654	12058.264031	28.602496
309.411728	12069.411536	28.607514
309.614609	12085.017748	28.612532
310.001999	12095.615343	28.617549
310.326043	12122.793115	28.622567
310.873867	12137.439134	28.627584
311.228014	12152.492385	28.632602
311.146190	12171.861748	28.637620
311.622346	12180.304695	28.642637
311.365338	12201.394047	28.647655
311.929284	12222.867066	28.652672
312.400656	12234.098463	28.657690
312.815989	12248.605859	28.662708
313.479146	12265.495718	28.667725
313.509876	12276.636461	28.672743
314.284819	12282.960765	28.677760
314.909476	12289.952977	28.682778
314.812161	12295.163105	28.687796
315.153050	12303.530887	28.692813
315.045278	12327.454165	28.697831
315.397166	12331.593755	28.702848
315.700742	12353.767324	28.707866
316.000388	12369.458589	28.712884
316.631062	12378.186410	28.717901
316.899824	12393.799310	28.722919
317.116981	12412.343980	28.727936
317.692121	12413.061601	28.732954
317.774889	12425.719215	28.737972
318.363347	12434.959925	28.742989
318.495813	12445.981454	28.748007
318.932226	12451.851493	28.753024
319.436445	12459.265627	28.758042
319.334184	12464.312743	28.763060
320.095857	12479.941544	28.768077
319.882743	12491.587818	28.773095
320.063925	12507.565215	28.778112
320.501427	12527.417611	28.783130
320.713450	12539.718185	28.788148
321.014034	12551.132610	28.793165
321.341323	12574.385153	28.798183
321.573329	12579.052149	28.803200
321.778369	12594.600187	28.808218
321.652316	12608.587988	28.813236
322.157489	12626.686365	28.818253
322.403379	12654.643882	28.823271
322.500909	12688.628567	28.828288
322.708593	12703.361547	28.833306
322.761540	12730.273353	28.838324
323.205844	12758.007406	28.843341
323.596404	12785.217789	28.848359
324.172674	12804.986014	28.853376
324.769858	12830.381406	28.858394
325.087298	12854.217486	28.863412
325.683899	12882.414975	28.868429
325.882260	12905.858031	28.873447
325.922851	12913.543228	28.878464
326.419970	12950.243521	28.883482
327.141021	12950.617025	28.888500
328.229465	12950.193557	28.893517
328.232351	12964.302073	28.898535
328.511311	12983.946559	28.903552
329.205466	12981.713275	28.908570
329.331570	13005.894966	28.913588
329.673212	13006.470180	28.918605
329.857004	13031.267957	28.923623
329.931322	13042.067894	28.928640
330.508522	13055.677653	28.933658
330.473876	13073.395011	28.938676
330.881446	13091.762267	28.943693
330.527768	13111.302405	28.948711
331.202836	13135.768161	28.953728
331.651575	13152.992416	28.958746
331.698743	13190.897928	28.963764
332.214614	13200.170048	28.968781
332.241346	13233.959612	28.973799
332.477914	13252.149011	28.978816
332.810082	13277.931104	28.983834
332.924932	13304.181143	28.988852
334.495850	13300.889709	28.993869
335.181947	13323.659797	28.998887
335.496334	13328.872779	29.003904
336.137868	13325.724700	29.008922
335.900287	13351.130354	29.013940
336.173184	13351.915569	29.018957
336.151219	13368.597331	29.023975
336.330634	13401.632222	29.028992
337.032954	13417.694144	29.034010
336.556202	13442.222476	29.039028
337.192585	13460.917757	29.044045
337.310382	13495.464945	29.049063
337.526961	13507.912059	29.054080
338.143150	13540.307334	29.059098
337.970087	13576.070788	29.064116
338.524738	13606.985567	29.069133
339.048103	13626.623323	29.074151
339.429324	13657.838074	29.079168
340.222797	13661.786457	29.084186
340.391788	13700.098423	29.089204
340.905761	13715.637190	29.094221
341.218620	13733.070598	29.099239
341.346533	13744.481452	29.104256
341.804827	13756.678999	29.109274
341.467545	13790.252812	29.114292
342.041336	13822.644660	29.119309
342.506028	13849.871302	29.124327
342.610436	13876.484895	29.129344
343.647455	13885.882020	29.134362
343.227673	13929.472582	29.139380
343.550916	13943.616983	29.144397
343.978687	13968.265337	29.149415
344.354588	13998.468262	29.154432
344.635793	14016.509260	29.159450
345.028898	14052.542183	29.164468
345.517571	14072.949025	29.169485
346.099424	14099.686973	29.174503
345.886011	14134.221187	29.179520
346.529430	14155.548029	29.184538
346.759823	14182.328737	29.189556
347.422199	14192.320968	29.194573
348.299579	14201.880334	29.199591
349.137210	14210.912041	29.204608
350.173412	14213.316727	29.209626
350.388633	14206.160581	29.214644
350.453499	14204.026950	29.219661
350.983387	14210.172091	29.224679
350.984878	14231.660830	29.229696
351.298706	14230.111517	29.234714
351.245988	14231.190422	29.239732
351.744591	14252.847196	29.244749
351.663280	14259.930751	29.249767
351.616142	14287.481126	29.254784
352.168354	14305.896648	29.259802
352.013092	14336.836179	29.264820
352.238133	14359.936473	29.269837
352.766692	14392.346423	29.274855
352.847913	14437.837759	29.279872
353.166725	14452.984121	29.284890
353.372893	14496.070320	29.289908
353.957709	14526.494836	29.294925
355.275471	14539.954456	29.299943
355.545958	14555.126277	29.304960
356.034151	14571.204425	29.309978
356.642420	14596.252430	29.314996
356.689295	14613.247115	29.320013
357.022510	14637.043782	29.325031
357.343090	14664.834734	29.330048
357.777474	14670.428536	29.335066
357.883495	14703.227656	29.340084
358.215973	14718.736064	29.345101
358.443361	14743.396811	29.350119
359.084757	14767.068399	29.355136
359.535085	14789.498297	29.360154
359.544886	14812.909220	29.365172
359.809586	14832.873517	29.370189
360.352061	14865.447581	29.375207
360.568155	14893.829970	29.380224
360.729899	14915.408037	29.385242
360.952585	14936.832586	29.390260
361.685850	14967.572122	29.395277
362.199573	14995.076225	29.400295
362.602696	15024.929786	29.405312
363.035128	15047.058824	29.410330
363.022247	15066.880384	29.415348
363.455158	15094.505252	29.420365
364.123679	15122.403097	29.425383
364.076396	15146.979260	29.430400
364.257344	15169.290511	29.435418
364.666892	15210.630001	29.440436
365.146977	15229.146808	29.445453
365.973652	15254.112258	29.450471
366.194842	15276.221532	29.455488
366.705120	15289.828522	29.460506
367.207088	15313.317592	29.465524
367.533738	15319.183268	29.470541
367.811005	15333.683258	29.475559
368.405662	15348.959579	29.480576
368.723064	15368.044178	29.485594
369.431309	15375.183041	29.490612
369.820987	15380.138304	29.495629
370.493117	15394.952603	29.500647
370.659742	15405.961002	29.505664
370.981872	15411.190708	29.510682
370.910044	15437.226148	29.515700
370.893476	15445.248290	29.520717
371.405206	15462.738772	29.525735
371.409589	15499.465177	29.530752
371.635930	15504.051998	29.535770
371.726955	15552.730167	29.540788
372.503071	15570.137444	29.545805
373.107561	15589.521364	29.550823
373.184020	15622.311468	29.555840
373.714107	15645.812105	29.560858
374.189665	15666.284586	29.565876
374.192507	15703.114150	29.570893
374.681053	15735.172465	29.575911
375.250837	15759.305016	29.580928
375.499140	15781.024305	29.585946
376.053788	15803.372065	29.590964
376.470392	15829.122090	29.595981
376.973013	15860.760628	29.600999
377.193007	15896.667169	29.606016
377.522913	15909.273818	29.611034
377.909592	15933.955602	29.616052
377.971144	15961.104563	29.621069
378.963888	15986.565262	29.626087
378.763438	16028.517242	29.631104
379.408980	16056.557623	29.636122
379.775186	16090.254123	29.641140
379.898721	16125.095915	29.646157
380.745158	16143.839771	29.651175
380.767059	16186.566959	29.656192
381.050209	16207.500803	29.661210
381.629155	16237.245398	29.666228
381.846395	16272.549527	29.671245
382.447627	16305.378341	29.676263
382.462528	16340.686277	29.681280
382.785329	16365.350946	29.686298
383.178277	16395.867547	29.691316
383.737151	16432.269064	29.696333
384.341286	16466.292495	29.701351
384.810904	16497.728100	29.706368
385.413476	16517.058267	29.711386
385.759757	16539.175255	29.716404
386.511831	16561.049905	29.721421
386.752284	16577.625132	29.726439
386.980845	16604.879813	29.731456
387.310314	16632.217081	29.736474
387.748996	16661.408836	29.741492
388.120915	16696.051373	29.746509
388.925488	16719.432291	29.751527
388.891551	16750.896853	29.756544
389.078094	16778.494543	29.761562
389.260265	16797.084672	29.766580
389.925785	16824.429489	29.771597
390.128793	16856.431806	29.776615
390.327217	16892.988789	29.781632
390.769888	16925.241463	29.786650
391.154884	16967.677067	29.791668
391.404883	16983.836556	29.796685
392.356416	17010.610849	29.801703
392.788020	17048.793996	29.806720
393.361505	17058.323567	29.811738
393.871724	17069.599144	29.816756
394.350694	17096.638074	29.821773
394.970090	17099.624751	29.826791
395.317024	17125.569647	29.831808
395.672471	17140.531131	29.836826
395.749666	17152.605363	29.841844
395.629158	17180.125468	29.846861
396.274132	17202.269393	29.851879
396.479917	17226.568592	29.856896
396.762504	17257.013690	29.861914
397.044266	17288.072164	29.866932
397.593845	17322.201001	29.871949
397.913041	17347.908101	29.876967
398.245099	17390.500180	29.881984
398.339665	17418.530361	29.887002
398.890944	17453.759457	29.892020
398.991057	17490.294679	29.897037
399.573638	17515.110226	29.902055
399.602106	17556.668645	29.907072
400.991799	17566.351407	29.912090
402.910848	17569.398156	29.917108
404.159182	17563.582244	29.922125
405.068674	17547.442467	29.927143
405.492063	17548.991068	29.932160
405.693960	17525.437131	29.937178
405.842597	17509.677558	29.942196
405.853775	17523.832746	29.947213
405.884583	17504.897529	29.952231
406.207901	17509.069995	29.957248
406.081086	17540.073855	29.962266
406.279772	17544.358458	29.967284
406.424838	17566.872802	29.972301
406.985794	17580.621453	29.977319
406.907780	17617.289005	29.982336
406.985581	17640.897566	29.987354
407.381769	17667.872365	29.992372
407.586843	17709.066072	29.997389
407.792201	17744.085266	30.002407
408.150089	17775.969053	30.007424
408.292441	17816.955908	30.012442
408.979509	17848.465157	30.017460
409.207597	17907.277675	30.022477
409.575803	17944.433017	30.027495
409.757459	17988.248077	30.032512
410.329699	18030.385743	30.037530
410.820198	18066.994536	30.042548
410.860923	18122.690902	30.047565
411.600889	18165.163619	30.052583
411.743236	18210.631546	30.057600
412.074909	18259.116905	30.062618
412.994394	18297.940732	30.067636
413.412414	18346.900690	30.072653
414.350718	18375.090281	30.077671
414.657000	18411.164499	30.082688
414.693914	18462.587400	30.087706
415.513997	18496.333217	30.092724
415.779614	18543.130992	30.097741
415.788068	18567.159102	30.102759
416.296764	18612.758023	30.107776
416.446487	18667.796496	30.112794
417.275750	18696.900163	30.117812
417.514722	18740.679305	30.122829
417.852649	18781.304993	30.127847
418.321570	18821.765564	30.132864
418.710823	18869.185335	30.137882
419.636595	18905.881320	30.142900
420.699289	18919.401137	30.147917
422.629195	18914.324436	30.152935
422.996116	18919.812670	30.157952
423.588369	18923.564052	30.162970
424.038752	18918.108815	30.167988
424.058399	18922.946899	30.173005
424.339042	18924.025913	30.178023
424.204272	18932.922238	30.183040
424.413789	18952.421436	30.188058
424.762277	18963.665267	30.193076
424.783114	18982.975134	30.198093
425.042814	19015.309556	30.203111
425.349766	19040.827405	30.208128
425.378323	19073.488826	30.213146
425.776467	19088.158059	30.218164
426.158887	19135.269156	30.223181
426.411500	19165.260818	30.228199
426.904702	19216.837268	30.233216
427.001983	19250.197040	30.238234
427.589916	19295.776786	30.243252
427.755123	19345.883639	30.248269
428.933118	19374.013046	30.253287
429.537185	19399.786360	30.258304
430.130548	19432.685738	30.263322
430.920141	19459.137757	30.268340
431.058138	19495.431452	30.273357
431.700185	19517.599453	30.278375
432.237243	19552.854280	30.283392
432.553555	19586.548825	30.288410
432.831733	19604.309508	30.293428
432.742845	19640.207656	30.298445
433.384879	19675.011758	30.303463
434.329724	19699.530769	30.308480
434.523124	19737.408086	30.313498
435.171423	19752.678007	30.318516
435.052462	19794.409949	30.323533
435.709417	19820.503049	30.328551
436.362911	19865.086541	30.333568
436.484367	19899.961810	30.338586
437.118867	19931.206262	30.343604
437.147439	19966.722990	30.348621
437.415962	20006.623777	30.353639
437.570374	20038.000193	30.358656
437.764741	20105.213385	30.363674
438.732374	20137.528565	30.368692
438.786283	20192.896975	30.373709
438.959243	20234.786479	30.378727
439.692308	20285.363087	30.383744
440.199570	20331.498246	30.388762
440.877610	20369.238160	30.393780
441.166680	20415.036135	30.398797
441.730984	20462.831802	30.403815
442.398844	20505.473808	30.408832
442.763597	20541.121952	30.413850
443.619550	20581.692773	30.418868
443.891170	20626.013777	30.423885
444.453298	20668.664298	30.428903
444.674746	20704.276678	30.433920
444.661693	20747.335103	30.438938
445.297204	20788.906361	30.443956
445.827699	20827.631983	30.448973
446.348187	20876.099869	30.453991
446.960657	20908.070328	30.459008
447.161295	20944.421390	30.464026
448.039337	20981.719534	30.469044
448.639433	21024.631107	30.474061
449.233183	21057.852097	30.479079
449.754501	21084.333903	30.484096
450.017502	21122.105026	30.489114
450.566665	21146.453804	30.494132
450.934399	21181.604582	30.499149
451.233754	21210.094294	30.504167
451.774945	21241.741395	30.509184
451.666529	21274.343124	30.514202
452.398460	21304.388287	30.519220
452.992263	21344.890970	30.524237
452.933920	21380.773563	30.529255
453.385462	21413.899046	30.534272
453.922396	21457.911711	30.539290
454.506350	21476.802961	30.544308
454.832316	21517.643810	30.549325
455.166125	21562.401578	30.554343
455.973773	21590.889502	30.559360
456.314026	21648.547090	30.564378
456.705195	21687.307290	30.569396
456.983694	21725.074035	30.574413
457.697985	21766.563670	30.579431
458.497230	21808.759864	30.584448
458.512963	21846.824376	30.589466
459.446031	21879.200686	30.594484
459.981488	21920.376672	30.599501
460.018399	21948.854457	30.604519
460.231114	21981.137742	30.609536
460.590433	22037.530515	30.614554
461.263085	22081.492305	30.619572
461.823532	22127.104795	30.624589
462.304996	22166.957985	30.629607
462.781531	22201.034805	30.634624
462.904927	22252.158495	30.639642
463.671235	22294.030250	30.644660
464.283493	22333.765926	30.649677
465.097611	22378.693636	30.654695
465.674133	22400.928367	30.659712
466.195116	22449.225665	30.664730
466.914055	22471.129361	30.669748
467.554490	22506.972392	30.674765
467.643850	22531.312812	30.679783
468.114044	22568.639634	30.684800
468.533513	22606.060109	30.689818
468.826432	22638.608845	30.694836
469.243738	22671.010840	30.699853
469.678424	22706.606215	30.704871
470.362903	22752.975584	30.709888
470.824005	22792.280164	30.714906
471.371770	22819.176583	30.719924
471.763085	22862.721965	30.724941
472.011291	22898.071191	30.729959
472.781285	22938.734498	30.734976
473.038002	22971.725092	30.739994
473.584223	23010.547719	30.745012
473.984245	23044.899124	30.750029
474.299844	23087.946760	30.755047
475.290468	23116.088347	30.760064
475.213574	23157.247622	30.765082
476.151291	23190.229612	30.770100
476.711304	23229.878302	30.775117
476.779356	23268.796703	30.780135
477.346921	23296.846436	30.785152
477.534104	23342.316040	30.790170
477.729064	23378.077210	30.795188
478.703651	23426.240454	30.800205
478.859710	23478.489879	30.805223
479.686884	23514.764477	30.810240
480.034069	23573.493433	30.815258
480.538457	23591.626011	30.820276
481.461163	23635.589726	30.825293
481.967569	23667.430062	30.830311
482.258242	23696.557737	30.835328
482.517224	23732.364209	30.840346
483.261771	23760.109355	30.845364
484.189848	23775.688125	30.850381
484.777235	23796.727584	30.855399
485.309142	23811.493841	30.860416
485.567133	23839.873422	30.865434
486.115170	23869.627265	30.870452
486.392878	23885.530188	30.875469
486.542126	23921.139243	30.880487
487.055333	23956.905544	30.885504
487.467560	23997.715959	30.890522
487.751574	24030.085912	30.895540
488.299938	24065.580099	30.900557
488.448023	24120.032646	30.905575
489.033976	24156.996802	30.910592
489.522599	24182.938534	30.915610
490.008423	24230.680605	30.920628
490.376224	24269.223499	30.925645
490.838538	24315.241362	30.930663
491.261083	24353.043642	30.935680
491.521027	24410.241383	30.940698
492.170445	24458.483631	30.945716
492.598683	24517.514615	30.950733
493.041834	24561.930956	30.955751
493.156476	24612.795094	30.960768
493.527330	24669.070087	30.965786
494.433664	24725.344646	30.970804
495.517273	24772.566316	30.975821
495.968116	24812.843967	30.980839
496.820840	24844.220540	30.985856
498.250009	24869.735868	30.990874
498.937827	24890.167042	30.995892
500.132262	24911.580170	31.000909
500.588037	24916.311267	31.005927
501.562596	24937.432924	31.010944
501.925752	24944.428243	31.015962
502.191891	24956.353682	31.020980
502.719559	24959.271890	31.025997
502.734951	24978.714082	31.031015
503.280280	25010.586734	31.036032
503.338790	25034.774993	31.041050
503.899838	25063.263979	31.046068
504.167011	25085.919475	31.051085
504.113683	25120.093294	31.056103
504.586291	25154.886351	31.061120
504.464141	25210.330314	31.066138
504.761083	25253.489016	31.071156
505.408769	25300.128489	31.076173
505.627777	25349.472969	31.081191
506.377880	25391.150022	31.086208
506.432611	25439.742974	31.091226
507.425703	25482.483843	31.096244
508.705181	25526.148737	31.101261
509.149657	25570.703103	31.106279
509.770542	25611.206725	31.111296
510.012973	25651.889997	31.116314
510.303581	25698.914734	31.121332
511.028483	25736.187264	31.126349
511.002340	25791.746477	31.131367
511.745056	25827.256202	31.136384
512.153666	25874.126190	31.141402
512.543031	25926.850588	31.146420
513.570708	25962.423668	31.151437
513.831286	26015.690174	31.156455
514.251420	26062.987739	31.161472
514.613287	26111.727143	31.166490
515.036688	26158.548135	31.171508
515.666445	26209.908685	31.176525
516.007713	26253.627150	31.181543
516.696958	26296.117695	31.186560
517.186418	26341.833675	31.191578
517.460686	26383.945441	31.196596
518.264897	26425.303741	31.201613
518.538590	26477.228910	31.206631
519.229441	26513.471007	31.211648
519.425977	26571.673777	31.216666
519.614937	26609.904648	31.221684
520.406973	26660.309057	31.226701
520.739740	26719.956480	31.231719
521.555089	26768.092495	31.236736
522.441796	26817.790834	31.241754
522.356884	26870.918626	31.246772
523.384201	26912.562794	31.251789
523.891233	26969.204378	31.256807
524.572991	27018.300138	31.261824
525.087500	27064.736235	31.266842
525.444368	27104.328266	31.271860
526.492555	27148.546715	31.276877
526.894005	27203.291851	31.281895
527.525653	27242.283381	31.286912
528.149731	27282.689459	31.291930
528.569286	27329.965354	31.296948
528.985137	27369.286374	31.301965
529.542422	27423.892766	31.306983
530.005650	27454.496545	31.312000
531.183056	27497.271749	31.317018
531.709281	27527.265838	31.322036
532.490057	27561.454231	31.327053
533.400621	27602.081615	31.332071
533.730428	27635.925493	31.337088
534.208663	27664.883639	31.342106
534.756328	27706.155123	31.347124
535.171492	27727.701196	31.352141
535.609415	27758.833372	31.357159
535.873287	27793.278409	31.362176
536.733058	27824.198693	31.367194
537.457447	27864.188842	31.372212
538.499961	27887.425888	31.377229
538.774314	27937.131345	31.382247
538.997829	27964.078653	31.387264
539.616952	27993.379886	31.392282
540.333656	28026.194969	31.397300
540.736916	28054.623625	31.402317
540.736042	28095.050207	31.407335
541.080767	28131.700187	31.412352
541.927905	28179.090361	31.417370
542.361667	28222.142274	31.422388
543.542827	28251.861663	31.427405
543.674397	28301.254324	31.432423
544.160628	28328.202735	31.437440
544.544903	28361.143058	31.442458
544.999317	28412.353141	31.447476
545.344518	28456.918814	31.452493
545.754040	28513.720443	31.457511
546.324672	28551.709241	31.462528
546.667255	28602.481021	31.467546
546.844768	28655.715805	31.472564
547.259046	28707.394009	31.477581
548.051899	28775.133382	31.482599
548.665879	28837.189461	31.487616
549.070605	28892.011933	31.492634
549.209101	28943.853360	31.497652
550.010473	28998.380000	31.502669
550.600199	29056.800269	31.507687
550.743150	29130.794484	31.512704
551.066990	29184.274738	31.517722
551.592047	29249.192693	31.522740
552.206561	29308.865310	31.527757
552.941235	29373.300930	31.532775
553.301110	29435.420260	31.537792
554.209894	29487.069131	31.542810
554.597425	29554.714782	31.547828
555.568903	29596.652303	31.552845
556.015429	29650.602618	31.557863
556.588546	29706.279897	31.562880
557.243569	29762.890229	31.567898
558.186873	29818.796647	31.572916
559.080002	29851.734158	31.577933
559.293168	29907.020693	31.582951
559.907373	29949.803972	31.587968
560.695015	29995.038356	31.592986
560.921788	30052.547339	31.598004
561.734448	30106.990380	31.603021
561.983563	30149.333131	31.608039
562.871033	30200.937171	31.613056
563.111262	30243.972571	31.618074
563.947289	30297.519457	31.623092
564.844603	30347.797188	31.628109
565.552113	30389.127355	31.633127
566.246495	30429.115753	31.638144
567.080590	30472.838704	31.643162
567.133708	30509.232899	31.648180
568.012213	30552.585843	31.653197
568.831107	30600.832842	31.658215
569.571778	30629.313781	31.663232
570.068467	30680.141718	31.668250
570.035297	30716.809388	31.673268
570.801571	30755.691776	31.678285
571.256708	30797.781022	31.683303
571.833700	30849.589973	31.688320
572.384601	30894.623048	31.693338
572.422661	30943.136319	31.698356
573.105913	30998.436571	31.703373
573.362696	31044.840873	31.708391
573.977350	31107.627412	31.713408
574.802760	31161.699299	31.718426
575.234484	31225.387461	31.723444
575.631237	31278.985041	31.728461
576.461881	31346.538769	31.733479
576.624207	31400.964448	31.738496
577.433698	31457.138103	31.743514
577.637388	31527.465950	31.748532
578.495051	31582.044920	31.753549
579.103292	31636.693873	31.758567
579.784482	31706.981007	31.763584
580.950422	31737.983603	31.768602
581.502599	31803.171534	31.773620
582.215629	31848.069687	31.778637
583.123956	31895.074821	31.783655
583.919573	31941.817972	31.788672
584.417217	31982.804941	31.793690
585.022505	32021.682150	31.798708
585.471125	32066.044183	31.803725
586.307897	32101.554255	31.808743
586.950475	32154.372167	31.813760
587.474121	32188.558676	31.818778
587.576881	32238.390006	31.823796
588.109755	32279.677883	31.828813
588.662122	32324.493488	31.833831
589.021851	32382.177311	31.838848
589.866639	32426.812093	31.843866
590.003591	32479.620273	31.848884
590.656425	32535.129180	31.853901
591.373681	32582.313018	31.858919
591.658530	32631.121256	31.863936
592.761485	32677.348316	31.868954
593.102680	32712.339215	31.873972
593.499578	32764.032225	31.878989
594.494429	32799.186127	31.884007
595.385980	32830.031104	31.889024
596.503920	32865.571755	31.894042
596.730732	32901.067964	31.899060
597.441814	32938.481255	31.904077
598.155928	32980.409635	31.909095
598.397998	33032.722369	31.914112
598.826340	33072.729384	31.919130
599.025408	33115.769146	31.924148
599.451587	33174.069301	31.929165
599.983883	33219.490052	31.934183
599.722278	33285.544334	31.939200
600.405810	33339.804219	31.944218
601.229158	33406.634931	31.949236
602.059547	33466.796981	31.954253
602.178209	33539.510449	31.959271
602.790218	33607.440442	31.964288
603.776864	33670.767554	31.969306
604.382742	33751.668706	31.974324
604.709564	33820.296923	31.979341
605.109115	33885.426329	31.984359
605.719878	33961.969664	31.989376
606.276850	34027.057668	31.994394
607.087908	34109.043481	31.999412
607.425861	34173.594050	32.004429
607.811561	34254.609775	32.009447
608.818477	34324.809003	32.014464
609.611515	34396.423080	32.019482
610.083016	34467.084147	32.024500
610.973199	34532.241737	32.029517
612.258429	34594.171879	32.034535
612.606285	34665.299224	32.039552
613.498247	34728.421748	32.044570
614.122563	34792.788146	32.049588
614.258993	34859.047229	32.054605
615.119369	34918.126741	32.059623
615.635684	34991.837287	32.064640
616.200812	35058.202650	32.069658
616.645425	35120.914833	32.074676
617.318463	35190.071493	32.079693
617.732979	35250.150806	32.084711
618.075974	35338.727422	32.089728
619.197097	35404.512581	32.094746
619.853858	35465.123611	32.099764
620.420575	35531.181176	32.104781
621.432045	35598.758895	32.109799
621.978010	35669.750020	32.114816
623.024863	35725.266543	32.119834
623.355261	35783.587945	32.124852
624.071461	35847.456843	32.129869
625.939958	35903.134156	32.134887
626.381823	35942.258504	32.139904
627.475693	35983.610136	32.144922
628.378546	36029.402556	32.149940
628.821649	36068.258710	32.154957
629.643802	36084.252755	32.159975
629.516534	36134.890581	32.164992
630.250009	36170.870923	32.170010
630.884339	36212.820134	32.175028
631.094157	36269.992232	32.180045
632.095965	36307.743037	32.185063
631.945833	36368.099730	32.190080
632.797849	36424.338792	32.195098
632.997456	36475.579767	32.200116
633.270426	36527.013854	32.205133
633.663625	36577.762182	32.210151
634.054034	36643.603765	32.215168
634.524627	36713.042911	32.220186
634.959448	36771.504819	32.225204
635.871823	36851.021359	32.230221
636.356756	36914.238076	32.235239
636.649958	36988.066424	32.240256
637.675529	37057.443150	32.245274
638.116595	37126.267009	32.250292
638.827857	37195.166205	32.255309
640.413536	37245.547974	32.260327
640.718724	37319.760744	32.265344
641.919396	37372.782300	32.270362
642.611557	37428.631245	32.275380
643.083383	37495.444008	32.280397
643.952037	37548.773709	32.285415
644.548949	37612.034237	32.290432
645.098684	37668.175854	32.295450
645.413402	37729.880237	32.300468
645.785204	37792.648508	32.305485
646.355473	37863.375921	32.310503
646.861886	37927.649980	32.315520
647.804946	37990.658660	32.320538
649.011046	38058.383713	32.325556
649.597325	38127.720687	32.330573
650.897813	38182.827046	32.335591
651.142531	38246.921579	32.340608
651.671581	38306.638510	32.345626
652.650948	38363.569490	32.350644
653.047779	38418.798192	32.355661
653.648240	38485.044011	32.360679
653.796927	38556.443840	32.365696
654.287472	38622.430637	32.370714
655.060916	38700.122333	32.375732
655.789694	38762.092897	32.380749
656.918813	38824.161342	32.385767
658.100542	38874.434793	32.390784
658.946854	38931.705293	32.395802
659.504722	38980.873665	32.400820
660.311802	39044.710333	32.405837
661.163051	39082.693947	32.410855
661.681041	39141.007619	32.415872
662.693735	39177.095934	32.420890
663.675518	39228.552555	32.425908
664.075868	39275.778164	32.430925
664.918141	39325.313758	32.435943
665.544019	39363.026027	32.440960
665.910214	39401.450691	32.445978
666.646127	39452.847754	32.450996
666.718747	39508.019940	32.456013
667.184740	39558.060567	32.461031
668.032659	39626.870517	32.466048
668.587898	39675.918085	32.471066
669.030935	39730.069813	32.476084
669.005987	39802.368259	32.481101
669.765891	39866.332425	32.486119
670.146373	39945.922383	32.491136
670.705660	40023.203845	32.496154
671.566193	40101.054338	32.501172
671.864275	40188.692924	32.506189
672.735437	40257.640278	32.511207
673.083654	40347.458934	32.516224
673.570742	40428.526437	32.521242
674.694026	40514.650052	32.526260
674.975654	40597.188756	32.531277
675.789786	40668.678890	32.536295
676.626883	40753.001230	32.541312
677.169450	40839.513208	32.546330
678.149843	40901.045152	32.551348
678.862161	40978.532512	32.556365
679.792975	41035.460925	32.561383
680.083611	41110.278662	32.566400
680.412605	41182.429047	32.571418
681.454148	41250.736233	32.576436
682.149550	41327.511242	32.581453
683.849127	41368.973457	32.586471
685.052351	41423.739528	32.591488
686.850236	41456.923851	32.596506
688.035163	41480.795905	32.601524
688.453944	41512.978073	32.606541
689.254008	41544.844437	32.611559
689.785942	41594.320868	32.616576
690.151295	41623.241455	32.621594
690.765114	41662.756780	32.626612
691.082090	41711.284226	32.631629
691.810969	41760.093844	32.636647
691.872981	41814.264444	32.641664
692.156396	41868.098526	32.646682
692.716914	41935.329475	32.651700
693.097213	41999.626106	32.656717
693.539143	42071.865394	32.661735
694.175333	42149.262962	32.666752
694.037787	42229.640169	32.671770
695.131065	42317.024231	32.676788
695.574233	42401.940418	32.681805
695.982267	42490.389356	32.686823
697.039598	42589.588392	32.691840
697.354170	42676.778239	32.696858
698.130431	42765.555684	32.701876
698.801314	42858.499617	32.706893
699.651397	42938.520171	32.711911
700.199919	43039.630952	32.716928
700.608063	43148.551377	32.721946
701.594956	43239.774559	32.726964
702.267797	43334.090793	32.731981
703.141674	43430.031713	32.736999
703.931556	43515.318491	32.742016
704.552150	43621.367974	32.747034
705.486029	43710.164795	32.752052
705.763790	43816.079700	32.757069
706.782890	43898.829538	32.762087
707.757168	43999.158103	32.767104
708.229323	44085.605319	32.772122
709.651001	44147.381041	32.777140
710.725627	44243.055999	32.782157
711.702563	44302.632712	32.787175
713.055055	44378.976538	32.792192
713.707872	44438.980075	32.797210
714.794288	44498.772891	32.802228
715.041140	44575.629451	32.807245
715.743684	44638.299769	32.812263
716.287973	44711.713187	32.817280
716.740074	44779.518634	32.822298
717.496755	44848.884107	32.827316
717.909498	44930.135134	32.832333
718.729072	45009.869649	32.837351
719.508320	45092.052008	32.842368
720.624335	45154.690142	32.847386
722.054956	45214.911211	32.852404
722.315917	45283.037547	32.857421
722.919621	45342.707944	32.862439
723.847357	45405.817083	32.867456
724.707038	45468.148319	32.872474
725.596808	45528.854890	32.877492
726.106124	45592.173053	32.882509
726.547861	45645.994883	32.887527
727.237238	45705.358544	32.892544
727.504208	45763.595749	32.897562
728.060083	45818.880084	32.902580
728.643298	45897.479772	32.907597
729.136644	45966.308901	32.912615
730.243693	46041.677129	32.917632
730.380532	46117.901430	32.922650
730.809823	46187.881948	32.927668
731.689876	46270.239016	32.932685
732.149385	46354.864082	32.937703
732.311004	46458.924770	32.942720
732.848630	46553.235393	32.947738
733.787614	46650.385071	32.952756
734.617767	46747.310159	32.957773
735.552983	46841.234109	32.962791
736.198423	46924.229805	32.967808
737.189792	47028.361131	32.972826
738.103633	47111.054140	32.977844
738.620660	47218.224222	32.982861
739.598550	47301.880073	32.987879
740.693101	47402.374151	32.992896
741.180726	47486.645899	32.997914
742.379683	47563.410226	33.002932
743.295668	47644.819897	33.007949
744.042822	47724.344183	33.012967
745.297872	47793.205074	33.017984
746.303987	47864.851881	33.023002
748.396569	47920.177780	33.028020
749.490361	47971.077823	33.033037
749.944193	48027.781399	33.038055
750.729508	48074.153723	33.043072
751.142719	48131.979154	33.048090
751.927471	48193.921247	33.053108
752.059960	48250.555663	33.058125
752.349857	48325.282244	33.063143
752.715395	48396.355234	33.068160
753.262346	48493.756260	33.073178
754.354902	48566.244053	33.078196
754.570209	48649.438679	33.083213
755.250935	48740.486614	33.088231
756.004163	48823.526377	33.093248
756.570104	48914.237316	33.098266
757.165586	49011.512904	33.103284
757.817353	49102.169427	33.108301
758.204836	49212.596772	33.113319
759.088375	49309.096490	33.118336
759.623602	49414.226137	33.123354
760.537002	49506.584518	33.128372
761.281086	49609.116008	33.133389
761.860171	49709.041372	33.138407
763.031324	49798.275820	33.143424
763.502418	49904.031510	33.148442
764.666101	50001.565206	33.153460
765.501690	50099.946622	33.158477
767.623824	50157.248116	33.163495
770.460049	50192.369620	33.168512
770.991648	50258.131567	33.173530
771.928676	50301.998411	33.178548
772.864579	50349.658844	33.183565
773.762507	50396.662423	33.188583
774.457188	50435.519424	33.193600
775.213886	50477.628912	33.198618
776.263414	50503.777464	33.203636
776.833426	50553.100487	33.208653
777.320381	50599.234711	33.213671
778.118726	50637.585345	33.218688
778.461955	50681.475821	33.223706
779.250886	50716.669669	33.228724
779.970538	50764.256479	33.233741
780.093400	50806.099194	33.238759
780.646156	50857.605244	33.243776
781.201077	50903.754181	33.248794
781.434533	50976.305239	33.253812
781.900385	51039.885566	33.258829
782.257241	51110.793141	33.263847
782.990072	51187.842034	33.268864
783.242788	51276.948352	33.273882
783.753311	51365.437416	33.278900
783.965331	51455.284107	33.283917
784.579031	51562.860364	33.288935
785.598484	51667.451255	33.293952
786.622000	51777.569733	33.298970
787.520140	51866.426316	33.303988
789.178996	51943.141287	33.309005
790.004681	52034.183859	33.314023
791.052210	52121.235289	33.319040
792.229648	52195.200937	33.324058
793.114285	52271.464511	33.329076
794.109412	52343.117181	33.334093
794.798066	52425.781987	33.339111
795.957044	52500.415207	33.344128
796.672617	52572.209888	33.349146
797.213453	52648.102406	33.354164
798.073653	52727.852849	33.359181
798.477492	52805.834602	33.364199
799.730974	52888.761403	33.369216
800.002114	52974.467169	33.374234
800.625035	53053.462291	33.379252
801.248846	53155.738722	33.384269
801.683333	53254.142684	33.389287
802.651656	53350.019826	33.394304
802.770386	53458.124626	33.399322
803.548447	53560.668189	33.404340
804.686753	53665.281651	33.409357
805.021315	53782.368169	33.414375
805.496365	53894.175443	33.419392
806.054379	54014.776999	33.424410
807.024219	54129.188668	33.429428
807.970999	54242.726605	33.434445
808.881537	54369.444668	33.439463
809.720427	54483.185128	33.444480
811.054214	54591.871612	33.449498
812.061942	54683.471246	33.454516
812.995078	54791.820965	33.459533
813.926995	54912.422816	33.464551
815.557907	54983.600505	33.469568
816.748410	55087.631571	33.474586
817.349089	55169.406359	33.479604
818.226860	55261.251392	33.484621
818.937313	55352.960343	33.489639
819.603592	55446.509431	33.494656
820.506379	55533.739036	33.499674
821.394904	55620.674418	33.504692
822.457245	55716.155718	33.509709
823.049204	55806.698534	33.514727
823.842011	55890.099897	33.519744
824.284148	55990.614043	33.524762
824.699489	56081.187426	33.529780
825.560480	56181.569826	33.534797
826.223314	56299.577215	33.539815
827.185081	56401.947067	33.544832
827.651809	56507.603290	33.549850
828.085251	56618.750421	33.554868
828.913340	56728.707892	33.559885
829.525790	56847.263999	33.564903
830.323084	56949.190037	33.569920
830.979770	57056.713346	33.574938
831.759705	57168.798120	33.579956
832.353775	57289.470480	33.584973
833.431523	57390.998351	33.589991
834.340288	57501.926160	33.595008
835.233251	57622.089612	33.600026
835.826542	57732.767739	33.605044
836.698373	57835.058759	33.610061
837.426201	57971.915735	33.615079
838.492730	58082.978559	33.620096
839.384232	58195.796250	33.625114
840.089113	58320.734671	33.630132
841.088209	58435.463284	33.635149
841.762338	58548.944667	33.640167
843.061337	58666.455970	33.645184
843.788377	58780.561833	33.650202
844.663462	58899.908030	33.655220
846.167876	59015.750492	33.660237
846.748805	59130.350242	33.665255
848.062378	59238.642007	33.670272
848.608988	59339.187208	33.675290
849.218048	59454.049556	33.680308
850.714718	59565.377794	33.685325
851.628444	59668.789792	33.690343
852.903934	59756.140260	33.695360
853.846089	59875.367331	33.700378
854.616575	59977.957811	33.705396
855.351124	60077.413729	33.710413
855.782536	60194.648166	33.715431
856.565903	60299.014064	33.720448
857.523637	60422.027489	33.725466
857.783036	60534.501789	33.730484
858.813798	60646.222985	33.735501
859.244821	60759.586471	33.740519
860.471732	60883.044665	33.745536
861.120979	60998.686476	33.750554
861.804176	61131.843269	33.755572
862.885416	61236.398387	33.760589
863.795966	61360.733631	33.765607
865.585736	61466.057188	33.770624
867.350984	61568.888774	33.775642
867.987603	61671.073895	33.780660
869.046485	61776.931198	33.785677
869.589106	61885.560975	33.790695
870.500011	61976.622145	33.795712
871.237237	62082.060367	33.800730
871.567377	62194.266599	33.805748
872.531772	62293.575087	33.810765
873.396171	62427.449761	33.815783
873.982029	62531.550138	33.820800
874.596358	62647.232344	33.825818
875.756200	62764.183642	33.830836
876.791310	62871.264142	33.835853
877.923870	62981.419948	33.840871
879.077358	63080.517552	33.845888
880.002272	63189.798722	33.850906
880.681833	63296.283063	33.855924
882.043424	63389.380591	33.860941
883.396657	63487.479886	33.865959
883.690001	63580.603867	33.870976
884.313864	63684.943967	33.875994
884.875376	63806.798219	33.881012
886.032572	63916.196393	33.886029
886.425202	64030.418708	33.891047
887.239542	64140.582949	33.896064
888.027003	64256.757465	33.901082
888.501913	64390.165886	33.906100
889.657658	64480.685464	33.911117
890.182579	64602.651609	33.916135
890.722912	64714.229794	33.921152
891.953867	64825.706600	33.926170
892.610026	64945.491034	33.931188
893.363979	65065.917367	33.936205
894.232787	65187.539077	33.941223
894.639256	65308.511243	33.946240
895.815362	65437.536596	33.951258
896.611185	65557.914571	33.956276
897.680430	65690.619483	33.961293
898.244330	65825.419430	33.966311
899.579892	65955.793347	33.971328
900.458597	66083.436999	33.976346
901.723765	66209.765557	33.981364
903.422223	66296.005224	33.986381
904.796331	66419.889358	33.991399
905.770856	66525.614260	33.996416
907.035555	66635.116356	34.001434
907.697808	66736.329651	34.006452
908.739399	66847.045781	34.011469
909.509362	66964.142331	34.016487
910.082771	67059.802147	34.021504
911.288229	67170.461175	34.026522
911.576411	67279.180366	34.031540
912.465414	67405.091739	34.036557
913.339520	67526.536483	34.041575
914.187044	67650.818736	34.046592
914.885836	67765.693451	34.051610
915.578428	67896.527533	34.056628
916.674849	68016.269087	34.061645
917.591850	68151.657588	34.066663
919.381192	68252.488795	34.071680
920.121844	68371.191287	34.076698
921.297365	68488.121504	34.081716
922.402058	68604.994572	34.086733
923.154169	68717.241724	34.091751
924.063425	68837.537441	34.096768
925.011271	68947.704782	34.101786
925.893850	69076.270056	34.106804
926.333143	69193.105043	34.111821
927.215855	69314.438477	34.116839
928.121852	69440.991414	34.121856
928.733856	69579.594739	34.126874
929.409906	69710.468035	34.131892
930.581863	69828.746679	34.136909
931.447532	69967.620252	34.141927
932.388989	70102.903305	34.146944
932.702526	70235.857030	34.151962
933.300394	70389.826738	34.156980
934.281250	70533.136349	34.161997
935.414184	70686.273256	34.167015
936.762684	70824.269207	34.172032
937.613181	70963.619675	34.177050
938.802366	71106.310475	34.182068
940.151144	71229.366929	34.187085
941.289660	71367.711066	34.192103
942.245347	71498.656367	34.197120
943.084278	71630.450218	34.202138
944.169428	71746.445769	34.207156
945.789328	71870.301926	34.212173
947.388254	71985.467322	34.217191
948.931409	72085.756758	34.222208
949.509798	72198.436725	34.227226
950.037070	72305.655764	34.232244
951.133357	72402.612358	34.237261
952.082855	72523.181351	34.242279
952.275225	72632.987090	34.247296
953.337842	72727.838582	34.252314
953.949280	72856.420892	34.257332
954.735917	72965.263326	34.262349
955.627794	73074.088840	34.267367
956.124864	73193.168303	34.272384
956.734511	73318.560047	34.277402
957.451964	73451.251522	34.282420
958.673382	73579.920280	34.287437
959.137609	73714.362876	34.292455
959.984002	73846.042472	34.297472
961.071487	73979.175361	34.302490
961.820870	74138.117402	34.307508
962.687221	74268.556684	34.312525
963.635548	74419.347400	34.317543
964.838912	74564.082376	34.322560
965.622125	74703.973979	34.327578
966.891300	74869.722333	34.332596
967.634646	75012.885930	34.337613
968.803505	75149.117746	34.342631
970.414858	75273.513305	34.347648
971.672008	75415.759423	34.352666
972.460641	75550.216363	34.357684
974.048261	75685.654680	34.362701
975.655748	75804.462876	34.367719
976.336243	75930.218311	34.372736
977.382798	76057.026879	34.377754
977.849055	76191.212332	34.382772
979.062429	76322.713056	34.387789
979.716246	76457.216865	34.392807
980.556379	76597.439935	34.397824
981.645858	76731.461993	34.402842
982.497644	76866.694432	34.407860
983.201575	76998.296351	34.412877
984.279451	77150.248052	34.417895
985.823028	77273.034248	34.422912
987.679322	77387.129066	34.427930
988.618138	77518.954424	34.432948
989.802227	77643.244463	34.437965
990.743388	77767.214967	34.442983
991.252382	77896.115703	34.448000
992.639335	78020.475387	34.453018
993.140092	78160.106785	34.458036
993.968691	78283.820518	34.463053
994.890347	78407.924322	34.468071
995.824700	78546.581642	34.473088
996.738733	78685.774536	34.478106
997.531996	78831.516316	34.483124
998.079168	78962.814244	34.488141
999.213501	79116.813122	34.493159
1000.061692	79264.692990	34.498176
1001.207170	79414.637293	34.503194
1001.697457	79572.263262	34.508212
1002.383655	79736.480954	34.513229
1003.417426	79882.297166	34.518247
1004.141398	80061.667720	34.523264
1005.062424	80216.127011	34.528282
1005.948648	80395.783261	34.533300
1006.924808	80551.108677	34.538317
1007.861581	80728.810756	34.543335
1008.804191	80903.445078	34.548352
1009.989366	81074.371300	34.553370
1012.370737	81202.948627	34.558388
1014.996087	81329.733827	34.563405
1015.846112	81460.085014	34.568423
1016.839180	81612.789470	34.573440
1017.864457	81726.791148	34.578458
1018.937158	81871.114331	34.583476
1019.836669	81999.701647	34.588493
1020.818357	82115.724312	34.593511
1021.622317	82236.812959	34.598528
1022.437606	82351.472597	34.603546
1023.206936	82467.715752	34.608564
1024.491404	82591.662079	34.613581
1025.628435	82709.370162	34.618599
1026.301410	82835.348897	34.623616
1027.006722	82958.298788	34.628634
1028.149445	83101.042751	34.633652
1028.931324	83236.109809	34.638669
1029.786942	83372.842034	34.643687
1030.165222	83523.693589	34.648704
1031.017278	83664.072407	34.653722
1032.131901	83823.016065	34.658740
1033.251029	83967.458605	34.663757
1034.919410	84108.811901	34.668775
1035.626399	84260.353985	34.673792
1036.685740	84412.142297	34.678810
1037.679438	84565.068728	34.683828
1038.311614	84732.931390	34.688845
1039.350870	84892.919902	34.693863
1040.635632	85041.935235	34.698880
1042.183104	85192.515073	34.703898
1043.630706	85342.764452	34.708916
1044.208095	85495.981211	34.713933
1045.408531	85650.943213	34.718951
1046.157010	85803.766613	34.723968
1047.467925	85948.638900	34.728986
1048.218645	86101.767596	34.734004
1049.498823	86273.539180	34.739021
1050.443215	86430.029489	34.744039
1051.315523	86591.797450	34.749056
1053.029791	86731.197470	34.754074
1054.851352	86866.467463	34.759092
1055.773677	87013.517957	34.764109
1057.115854	87158.240665	34.769127
1057.812315	87306.361904	34.774144
1058.836576	87444.431553	34.779162
1059.632660	87599.713977	34.784180
1060.841320	87751.372625	34.789197
1061.811281	87899.186427	34.794215
1062.623244	88055.582948	34.799232
1063.275816	88224.112673	34.804250
1064.094508	88387.787629	34.809268
1065.084882	88558.687377	34.814285
1065.903759	88715.049127	34.819303
1066.378047	88899.199752	34.824320
1067.060324	89072.407189	34.829338
1068.472545	89265.416616	34.834356
1070.343456	89431.278339	34.839373
1072.079896	89583.702805	34.844391
1073.071303	89750.877117	34.849408
1074.604405	89911.399978	34.854426
1075.401196	90074.716761	34.859444
1076.163290	90247.039786	34.864461
1077.853975	90404.812149	34.869479
1078.551914	90561.263002	34.874496
1079.857847	90719.721488	34.879514
1081.185105	90880.810278	34.884532
1081.912501	91040.873129	34.889549
1082.991569	91193.556130	34.894567
1083.553082	91369.319100	34.899584
1084.507416	91531.107001	34.904602
1086.329968	91675.378693	34.909620
1087.667000	91829.915302	34.914637
1089.531570	91982.029925	34.919655
1090.588785	92125.614823	34.924672
1091.544679	92272.932623	34.929690
1092.329381	92415.298605	34.934708
1093.424733	92563.772270	34.939725
1094.013166	92697.210204	34.944743
1095.299056	92849.552859	34.949760
1096.189810	92980.904137	34.954778
1097.353579	93129.255969	34.959796
1097.809560	93282.682102	34.964813
1098.918542	93444.210230	34.969831
1099.739517	93613.629521	34.974848
1100.621276	93776.273562	34.979866
1101.372541	93938.617520	34.984884
1101.880313	94122.542851	34.989901
1103.184575	94297.944193	34.994919
1104.185497	94488.677190	34.999936
1105.252239	94665.734653	35.004954
1106.424698	94855.024147	35.009972
1106.844506	95048.567068	35.014989
1108.267193	95241.521013	35.020007
1109.146800	95431.540813	35.025024
1110.356189	95630.458075	35.030042
1111.612969	95823.760583	35.035060
1112.943266	96026.503342	35.040077
1114.462141	96204.553937	35.045095
1115.893251	96397.034375	35.050112
1117.142044	96578.474832	35.055130
1118.644146	96767.262112	35.060148
1119.734896	96955.213815	35.065165
1121.092895	97137.406195	35.070183
1122.026087	97324.715784	35.075200
1123.184928	97506.804620	35.080218
1124.097972	97697.260284	35.085236
1124.812705	97886.623437	35.090253
1125.875231	98087.926971	35.095271
1126.610638	98286.842717	35.100288
1127.689794	98487.488285	35.105306
1128.878975	98687.294185	35.110324
1130.201642	98885.813341	35.115341
1131.447114	99076.800380	35.120359
1132.745958	99296.706296	35.125376
1133.655642	99501.484168	35.130394
1135.043352	99700.714319	35.135412
1135.684065	99905.685680	35.140429
1137.573423	100088.608926	35.145447
1140.179976	100245.481779	35.150464
1141.885370	100423.404623	35.155482
1143.688750	100586.547824	35.160500
1144.993772	100741.487001	35.165517
1146.536761	100891.347853	35.170535
1147.167009	101052.960176	35.175552
1148.236414	101204.826179	35.180570
1149.148875	101366.602595	35.185588
1149.763732	101535.685352	35.190605
1151.059081	101703.598953	35.195623
1151.567273	101874.683415	35.200640
1152.178660	102053.368894	35.205658
1153.693898	102233.691210	35.210676
1154.219620	102426.152303	35.215693
1154.776724	102615.462707	35.220711
1155.627911	102818.054270	35.225728
1156.279805	103021.782226	35.230746
1157.580038	103229.665632	35.235764
1158.910921	103431.517540	35.240781
1160.727345	103613.515452	35.245799
1162.124959	103819.924709	35.250816
1163.164395	104019.290339	35.255834
1164.509065	104217.479720	35.260852
1165.364368	104426.909205	35.265869
1166.893904	104603.325897	35.270887
1167.880682	104789.243663	35.275904
1169.075763	104961.298269	35.280922
1170.471867	105136.296891	35.285940
1171.523271	105332.288988	35.290957
1172.359374	105507.800914	35.295975
1173.338305	105693.004450	35.300992
1174.265312	105891.009747	35.306010
1175.323888	106067.362378	35.311028
1175.938369	106279.594881	35.316045
1177.673038	106475.254116	35.321063
1178.707172	106668.320567	35.326080
1179.804253	106882.719631	35.331098
1181.122724	107076.995778	35.336116
1181.845246	107291.080282	35.341133
1182.972078	107495.865939	35.346151
1184.746238	107695.694679	35.351168
1185.338221	107912.668334	35.356186
1187.014038	108129.615946	35.361204
1187.747752	108358.931967	35.366221
1189.147755	108568.291047	35.371239
1189.961643	108787.882235	35.376256
1191.103063	109011.461545	35.381274
1192.914544	109222.784110	35.386292
1193.565036	109456.328616	35.391309
1194.844840	109678.763124	35.396327
1196.505361	109901.579647	35.401344
1197.373718	110138.425318	35.406362
1198.580470	110357.292669	35.411380
1199.684200	110593.355873	35.416397
1200.923573	110817.896504	35.421415
1202.565719	111041.004062	35.426432
1203.692396	111281.465053	35.431450
1205.182281	111494.834738	35.436468
1206.761664	111715.069917	35.441485
1208.218776	111931.007342	35.446503
1209.675387	112149.568843	35.451520
1211.098016	112357.673753	35.456538
1214.398615	112515.580917	35.461556
1216.477118	112677.086826	35.466573
1217.950450	112840.290285	35.471591
1219.450262	113004.681153	35.476608
1220.383107	113170.573253	35.481626
1221.785113	113321.008757	35.486644
1223.226589	113479.723880	35.491661
1224.021781	113633.188202	35.496679
1224.711490	113799.770485	35.501696
1225.799863	113971.380554	35.506714
1226.711410	114138.257449	35.511732
1227.438688	114321.293684	35.516749
1227.919232	114498.721575	35.521767
1229.458909	114693.217798	35.526784
1229.864669	114885.673640	35.531802
1231.022627	115084.518130	35.536820
1232.102452	115289.357010	35.541837
1233.226282	115491.352075	35.546855
1234.497587	115705.550417	35.551872
1235.866759	115896.396319	35.556890
1237.653026	116084.526311	35.561908
1238.651350	116304.285863	35.566925
1239.566144	116501.166099	35.571943
1240.710173	116704.395443	35.576960
1242.286251	116910.329362	35.581978
1243.298991	117100.520252	35.586996
1244.642497	117318.431167	35.592013
1245.736517	117523.245761	35.597031
1246.686415	117727.705603	35.602048
1247.621825	117952.923957	35.607066
1248.588234	118170.232331	35.612084
1249.811006	118372.776208	35.617101
1251.975793	118562.164809	35.622119
1253.329733	118743.060136	35.627136
1254.494683	118944.426529	35.632154
1256.125301	119126.963629	35.637172
1256.952687	119325.106801	35.642189
1257.548998	119525.519818	35.647207
1258.664762	119733.463633	35.652224
1259.684794	119954.159772	35.657242
1260.703340	120174.072178	35.662260
1261.561063	120394.773219	35.667277
1262.149163	120634.122986	35.672295
1263.196535	120870.610686	35.677312
1264.411278	121117.425638	35.682330
1265.879999	121355.697476	35.687348
1266.974494	121613.852814	35.692365
1268.223798	121859.996608	35.697383
1269.908647	122115.612626	35.702400
1270.770256	122363.155516	35.707418
1272.088583	122617.442652	35.712436
1273.251543	122880.603384	35.717453
1274.949620	123133.108423	35.722471
1276.855703	123367.610680	35.727488
1278.436302	123623.104839	35.732506
1280.329917	123852.264877	35.737524
1281.700394	124092.311143	35.742541
1282.736515	124332.516164	35.747559
1283.889421	124577.760484	35.752576
1285.374060	124816.678302	35.757594
1287.185234	125046.811617	35.762612
1288.677025	125275.985741	35.767629
1289.754960	125513.468312	35.772647
1291.186222	125748.574779	35.777664
1292.249597	125985.049514	35.782682
1293.401399	126215.402418	35.787700
1294.709580	126454.742587	35.792717
1296.022516	126696.441284	35.797735
1297.543701	126927.257926	35.802752
1298.884491	127175.318393	35.807770
1300.580025	127403.574759	35.812788
1302.072750	127628.013297	35.817805
1303.744200	127851.346453	35.822823
1306.891122	128026.588340	35.827840
1309.192418	128203.936106	35.832858
1310.624635	128392.481753	35.837876
1312.575488	128575.238677	35.842893
1313.131286	128760.572971	35.847911
1314.457657	128934.676939	35.852928
1315.408523	129129.631887	35.857946
1316.598582	129298.931145	35.862964
1318.058235	129480.266443	35.867981
1319.107189	129667.020035	35.872999
1320.280528	129849.583788	35.878016
1321.173493	130044.325857	35.883034
1322.288711	130231.388702	35.888052
1323.435787	130432.365591	35.893069
1324.463337	130631.234003	35.898087
1325.485407	130827.505964	35.903104
1326.393600	131035.244647	35.908122
1327.535767	131254.379908	35.913140
1328.542811	131476.099717	35.918157
1329.439192	131699.360598	35.923175
1330.547716	131934.529186	35.928192
1331.601075	132173.232764	35.933210
1332.692882	132418.675779	35.938228
1333.817179	132660.553083	35.943245
1334.229660	132908.254883	35.948263
1335.680956	133153.225539	35.953280
1336.997616	133411.911705	35.958298
1339.874649	133608.476217	35.963316
1341.866341	133809.118716	35.968333
1343.161988	134032.735226	35.973351
1344.803592	134229.622486	35.978368
1347.077478	134430.348798	35.983386
1348.659197	134620.630671	35.988404
1349.993890	134820.640383	35.993421
1350.890714	135026.669810	35.998439
1351.947294	135232.559936	36.003456
1352.850176	135444.676355	36.008474
1353.823609	135674.671137	36.013492
1355.116017	135895.334242	36.018509
1355.990606	136132.296211	36.023527
1357.294846	136356.725859	36.028544
1358.140482	136605.081117	36.033562
1358.834141	136852.550581	36.038580
1360.416306	137092.178644	36.043597
1361.215688	137370.367289	36.048615
1362.181701	137625.417200	36.053632
1363.312656	137904.506203	36.058650
1364.556172	138182.209525	36.063668
1365.612368	138456.243907	36.068685
1366.928056	138738.009825	36.073703
1368.582610	139035.723171	36.078720
1370.396130	139311.591504	36.083738
1372.093692	139578.225265	36.088756
1374.168865	139855.893150	36.093773
1375.591286	140132.061218	36.098791
1377.075514	140400.309061	36.103808
1378.370404	140687.026992	36.108826
1380.126877	140946.155133	36.113844
1381.977585	141209.631554	36.118861
1382.937627	141481.575898	36.123879
1384.097370	141756.228206	36.128896
1385.401523	142026.762967	36.133914
1386.941083	142306.187872	36.138932
1388.632236	142577.930790	36.143949
1390.072006	142857.807798	36.148967
1391.471999	143117.239498	36.153984
1392.705516	143401.808902	36.159002
1393.701923	143685.544934	36.164020
1394.957236	143961.758459	36.169037
1396.299531	144255.637319	36.174055
1397.607203	144543.006159	36.179072
1399.224651	144836.565208	36.184090
1400.285170	145121.874586	36.189108
1401.745177	145414.373883	36.194125
1402.804517	145711.291838	36.199143
1404.189291	145997.911362	36.204160
1405.701389	146291.728071	36.209178
1407.602133	146597.074105	36.214196
1409.169211	146881.083272	36.219213
1410.535645	147186.675056	36.224231
1411.815691	147468.910166	36.229248
1413.298902	147769.858418	36.234266
1414.550198	148071.532458	36.239284
1416.151098	148375.852411	36.244301
1417.074249	148675.011235	36.249319
1418.244051	148967.371620	36.254336
1419.579236	149279.111819	36.259354
1421.436451	149574.356185	36.264372
1423.593026	149868.868365	36.269389
1424.992917	150175.278413	36.274407
1426.336247	150457.678049	36.279424
1427.749912	150762.606661	36.284442
1429.422135	151064.006890	36.289460
1431.144270	151327.058537	36.294477
1432.284408	151614.776938	36.299495
1433.671115	151878.040236	36.304512
1435.005356	152141.745309	36.309530
1436.968238	152413.820894	36.314548
1438.577646	152680.667756	36.319565
1439.458619	152955.425356	36.324583
1440.647563	153237.858587	36.329600
1441.822809	153519.547782	36.334618
1442.879169	153813.676846	36.339636
1445.016770	154084.834686	36.344653
1446.327089	154374.029649	36.349671
1447.855142	154659.131534	36.354688
1449.088829	154950.233505	36.359706
1450.294398	155238.754572	36.364724
1451.742605	155521.262876	36.369741
1452.992731	155826.449005	36.374759
1454.904779	156114.415368	36.379776
1456.904489	156397.257110	36.384794
1458.582969	156692.585829	36.389812
1460.175905	156971.350973	36.394829
1461.904632	157246.327931	36.399847
1463.765058	157534.401928	36.404864
1465.635682	157807.862301	36.409882
1466.773254	158091.632813	36.414900
1468.166885	158357.361518	36.419917
1469.655245	158629.089433	36.424935
1471.363359	158911.058477	36.429952
1472.659225	159184.547332	36.434970
1474.044666	159474.413840	36.439988
1475.726915	159746.992413	36.445005
1476.597979	160023.246812	36.450023
1478.118176	160316.649129	36.455040
1479.821845	160605.506670	36.460058
1480.891853	160893.139182	36.465076
1482.589007	161191.275874	36.470093
1483.822625	161478.453953	36.475111
1484.774123	161780.917849	36.480128
1485.873006	162087.736531	36.485146
1487.037826	162407.170256	36.490164
1488.602194	162721.110001	36.495181
1490.182009	163048.130188	36.500199
1491.441657	163371.222111	36.505216
1492.662465	163698.332190	36.510234
1493.988343	164033.940768	36.515252
1495.958965	164354.524270	36.520269
1497.017358	164689.103848	36.525287
1498.517157	165017.928630	36.530304
1500.804461	165338.073598	36.535322
1502.243344	165677.419170	36.540340
1503.922550	165987.481151	36.545357
1505.655962	166306.113643	36.550375
1507.173886	166629.542327	36.555392
1509.094811	166948.516342	36.560410
1511.310295	167260.147876	36.565428
1513.110670	167555.443951	36.570445
1515.058135	167833.118283	36.575463
1517.415627	168126.980767	36.580480
1518.935872	168402.102868	36.585498
1520.091106	168702.195675	36.590516
1521.752618	168984.200727	36.595533
1523.714469	169262.579399	36.600551
1525.431534	169531.077375	36.605568
1526.788054	169818.328068	36.610586
1528.087415	170094.930949	36.615604
1529.174524	170380.605590	36.620621
1530.127749	170664.159665	36.625639
1531.049986	170963.912585	36.630656
1532.668151	171245.761093	36.635674
1533.602924	171555.464486	36.640692
1535.146391	171831.973834	36.645709
1536.200977	172130.062633	36.650727
1537.385637	172423.309549	36.655744
1538.376447	172728.569888	36.660762
1539.474799	173045.616247	36.665780
1541.102287	173364.175976	36.670797
1542.296980	173685.182683	36.675815
1544.067458	174019.700253	36.680832
1545.735497	174332.891652	36.685850
1547.428788	174672.680442	36.690868
1548.757303	175003.255181	36.695885
1550.524603	175334.597020	36.700903
1551.885831	175666.503374	36.705920
1553.058748	176007.314184	36.710938
1554.888421	176345.137608	36.715956
1556.808913	176691.286372	36.720973
1558.400844	177028.354333	36.725991
1559.885736	177364.300102	36.731008
1561.973404	177702.534186	36.736026
1563.538696	178026.706140	36.741044
1565.500063	178356.893781	36.746061
1567.165901	178692.120388	36.751079
1569.239998	179024.641646	36.756096
1571.090635	179353.953012	36.761114
1572.490202	179684.039325	36.766132
1573.957720	180006.323616	36.771149
1575.877241	180334.284489	36.776167
1577.282058	180655.847077	36.781184
1579.509935	180968.111432	36.786202
1580.966115	181305.877468	36.791220
1582.894821	181621.266845	36.796237
1584.507739	181953.058331	36.801255
1586.123247	182276.372856	36.806272
1587.508933	182597.709321	36.811290
1588.957427	182923.302046	36.816308
1590.357207	183252.979197	36.821325
1591.748889	183589.082282	36.826343
1592.922195	183921.314236	36.831360
1594.269647	184261.312848	36.836378
1595.616020	184613.613343	36.841396
1596.773887	184967.483218	36.846413
1598.119312	185324.192944	36.851431
1599.561693	185692.008243	36.856448
1601.196686	186051.924130	36.861466
1602.499639	186436.890850	36.866484
1603.392042	186800.184164	36.871501
1605.270542	187184.959033	36.876519
1606.812616	187580.048820	36.881536
1608.567801	187961.510915	36.886554
1610.520615	188330.997809	36.891572
1612.540933	188699.587298	36.896589
1614.711949	189079.705753	36.901607
1616.381613	189448.281942	36.906624
1618.001662	189823.025373	36.911642
1619.863451	190183.386534	36.916660
1621.421587	190554.108065	36.921677
1623.292636	190912.682199	36.926695
1624.498201	191295.843875	36.931712
1626.224855	191651.793189	36.936730
1627.660335	192021.477744	36.941748
1629.440544	192395.525180	36.946765
1631.622446	192764.404982	36.951783
1633.085327	193124.608589	36.956800
1635.212289	193474.814806	36.961818
1636.728264	193846.464685	36.966836
1638.591008	194196.388670	36.971853
1640.304297	194536.157808	36.976871
1641.762677	194878.484686	36.981888
1643.497994	195220.183514	36.986906
1644.564118	195553.857325	36.991924
1646.128506	195880.404282	36.996941
1647.777779	196228.724374	37.001959
1649.285006	196559.257928	37.006976
1650.829837	196907.840172	37.011994
1653.226077	197237.391873	37.017012
1655.092704	197569.140505	37.022029
1657.271103	197894.237264	37.027047
1659.094116	198232.014266	37.032064
1660.874999	198561.027016	37.037082
1661.817510	198895.093702	37.042100
1663.414610	199237.724980	37.047117
1665.491028	199571.975224	37.052135
1666.396935	199929.756805	37.057152
1667.792544	200277.365499	37.062170
1669.300392	200631.927635	37.067188
1670.444267	200991.859006	37.072205
1672.371478	201359.305676	37.077223
1673.208296	201742.653338	37.082240
1674.381726	202117.072311	37.087258
1676.791903	202502.232811	37.092276
1677.628328	202892.696826	37.097293
1679.356866	203287.712901	37.102311
1681.069832	203681.349719	37.107328
1682.863270	204090.300555	37.112346
1684.361355	204489.779800	37.117364
1685.859960	204902.808913	37.122381
1687.599026	205304.182500	37.127399
1689.483201	205721.558089	37.132416
1691.197458	206121.594171	37.137434
1693.298576	206549.642135	37.142452
1694.968706	206961.892056	37.147469
1696.645129	207358.969553	37.152487
1698.312725	207782.156748	37.157504
1700.162349	208188.097994	37.162522
1701.799073	208610.685192	37.167540
1703.427362	209022.762220	37.172557
1705.763695	209432.222498	37.177575
1707.471885	209851.248860	37.182592
1709.304099	210267.107678	37.187610
1711.104761	210670.377333	37.192628
1712.765520	211087.589212	37.197645
1714.689541	211484.518632	37.202663
1716.003747	211902.985541	37.207680
1717.969147	212312.279969	37.212698
1719.915627	212737.858716	37.217716
1721.338545	213149.075503	37.222733
1723.371427	213580.815392	37.227751
1724.965723	213997.341020	37.232768
1726.236676	214405.541084	37.237786
1727.973218	214822.859610	37.242804
1729.836505	215249.962400	37.247821
1731.942774	215662.347119	37.252839
1733.799238	216082.495911	37.257856
1735.521668	216496.166953	37.262874
1737.675317	216916.397140	37.267892
1738.975337	217326.992410	37.272909
1740.797304	217745.503276	37.277927
1742.563215	218159.021763	37.282944
1743.990512	218570.490020	37.287962
1745.946682	219052.124162	37.292980
1748.333305	219458.001769	37.297997
1750.247726	219867.007052	37.303015
1751.730694	220283.374855	37.308032
1753.202650	220682.144777	37.313050
1755.074659	221094.743065	37.318068
1756.991048	221483.333563	37.323085
1758.809515	221863.509192	37.328103
1760.801291	222254.071053	37.333120
1762.296146	222636.919075	37.338138
1763.963171	223008.665772	37.343156
1765.462023	223402.081828	37.348173
1767.498763	223793.479730	37.353191
1768.750085	224174.874687	37.358208
1770.840308	224572.133631	37.363226
1772.320868	224964.338790	37.368244
1773.429641	225392.623769	37.373261
1775.262716	225796.126920	37.378279
1776.843367	226222.634805	37.383296
1778.353181	226630.715435	37.388314
1779.502531	227060.675843	37.393332
1781.077557	227508.296517	37.398349
1783.202313	227925.702847	37.403367
1784.894138	228373.459524	37.408384
1786.812227	228803.907871	37.413402
1788.829553	229242.494722	37.418420
1790.717739	229679.250122	37.423437
1792.544018	230130.089150	37.428455
1794.541204	230583.568372	37.433472
1796.033960	231025.321198	37.438490
1797.519605	231476.144678	37.443508
1799.158605	231941.092489	37.448525
1801.429595	232401.288594	37.453543
1802.805613	232862.752032	37.458560
1804.885261	233328.951871	37.463578
1806.700771	233786.280970	37.468596
1808.657536	234259.336824	37.473613
1810.523801	234717.371345	37.478631
1811.989430	235203.821630	37.483648
1813.479593	235680.184777	37.488666
1815.812914	236149.119210	37.493684
1817.525831	236623.365033	37.498701
1819.598134	237097.654138	37.503719
1821.626180	237577.082958	37.508736
1823.142119	238070.568910	37.513754
1824.875005	238545.121055	37.518772
1826.267481	239035.124386	37.523789
1828.354262	239515.869067	37.528807
1830.031238	240010.374530	37.533824
1832.236230	240507.943510	37.538842
1834.058356	240999.734516	37.543860
1835.451578	241499.142151	37.548877
1837.406169	241986.747317	37.553895
1838.973015	242491.996220	37.558912
1840.702660	242987.794840	37.563930
1843.043339	243483.264546	37.568948
1846.943500	243940.957128	37.573965
1850.292404	244376.717730	37.578983
1852.568542	244831.708775	37.584000
1854.530028	245265.287369	37.589018
1857.225074	245688.228302	37.594036
1859.082367	246122.993910	37.599053
1860.936890	246533.018216	37.604071
1863.120342	246948.754979	37.609088
1864.726130	247375.333383	37.614106
1866.601430	247778.420753	37.619124
1867.599350	248207.387121	37.624141
1869.549753	248626.746247	37.629159
1870.986922	249053.786349	37.634176
1872.747043	249466.877927	37.639194
1874.483970	249901.540928	37.644212
1875.629314	250344.812392	37.649229
1877.719422	250785.692259	37.654247
1879.336083	251211.561505	37.659264
1880.776939	251642.617058	37.664282
1882.443001	252058.901798	37.669300
1884.123404	252488.013052	37.674317
1886.349633	252909.921267	37.679335
1888.244937	253331.833766	37.684352
1890.368117	253755.055123	37.689370
1892.120704	254182.504237	37.694388
1894.554224	254612.533486	37.699405
1896.237427	255028.690052	37.704423
1898.184028	255456.793481	37.709440
1899.815894	255878.369764	37.714458
1901.763027	256304.466534	37.719476
1903.102409	256749.589558	37.724493
1905.184646	257187.654511	37.729511
1907.697049	257614.597842	37.734528
1909.342311	258062.261568	37.739546
1911.263301	258494.790094	37.744564
1912.688523	258960.425063	37.749581
1914.203109	259412.632282	37.754599
1916.326828	259877.008345	37.759616
1917.686278	260337.548066	37.764634
1919.440454	260805.719510	37.769652
1921.551696	261270.859510	37.774669
1923.486504	261752.870984	37.779687
1924.906617	262229.505867	37.784704
1926.684366	262731.763999	37.789722
1928.507320	263219.712382	37.794740
1930.662893	263719.544922	37.799757
1932.309821	264215.422325	37.804775
1933.973226	264711.804742	37.809792
1935.895277	265234.410836	37.814810
1937.761062	265738.684754	37.819828
1940.099131	266249.027559	37.824845
1942.372529	266756.383043	37.829863
1944.097441	267270.763939	37.834880
1946.082397	267789.216506	37.839898
1948.648346	268287.783280	37.844916
1950.835900	268800.714056	37.849933
1953.235903	269299.993012	37.854951
1955.458119	269810.300254	37.859968
1956.932190	270311.128449	37.864986
1959.099051	270818.039468	37.870004
1960.553443	271326.185492	37.875021
1963.148596	271840.721064	37.880039
1967.683575	272269.911481	37.885056
1971.582990	272707.157633	37.890074
1973.910541	273139.735421	37.895092
1975.993770	273574.918697	37.900109
1978.070677	274010.534184	37.905127
1979.902535	274430.211363	37.910144
1981.579022	274863.529353	37.915162
1983.136657	275288.610498	37.920180
1984.763076	275725.542450	37.925197
1986.292852	276153.014542	37.930215
1987.704452	276596.280281	37.935232
1989.128948	277057.045196	37.940250
1990.828647	277505.468904	37.945268
1992.536274	277966.261237	37.950285
1994.328903	278433.135003	37.955303
1996.210474	278898.494271	37.960320
1997.403420	279380.452446	37.965338
1999.745800	279857.164062	37.970356
2001.930594	280324.882954	37.975373
2003.547960	280816.826407	37.980391
2005.661236	281299.135359	37.985408
2007.281092	281772.532582	37.990426
2009.505167	282263.355562	37.995444
2011.500933	282739.304287	38.000461
2014.156516	283206.251880	38.005479
2017.108119	283639.720913	38.010496
2018.661619	284080.151753	38.015514
2020.724650	284523.875359	38.020532
2022.488664	284981.084487	38.025549
2023.660587	285441.387687	38.030567
2025.409312	285897.123384	38.035584
2026.808183	286380.678896	38.040602
2028.447324	286870.467047	38.045620
2030.301758	287366.314079	38.050637
2031.582109	287870.966925	38.055655
2033.353343	288379.422942	38.060672
2034.925141	288910.897577	38.065690
2036.620335	289434.653376	38.070708
2038.850940	289978.130665	38.075725
2040.885183	290516.786795	38.080743
2042.857320	291052.987158	38.085760
2044.599951	291604.590255	38.090778
2046.781505	292162.366574	38.095796
2048.665853	292717.802013	38.100813
2050.567813	293288.420950	38.105831
2052.331657	293866.248080	38.110848
2054.601301	294446.934895	38.115866
2057.164050	295003.669542	38.120884
2059.635120	295589.473217	38.125901
2061.554837	296161.878276	38.130919
2064.016338	296741.607068	38.135936
2066.087740	297315.073081	38.140954
2068.322353	297889.220126	38.145972
2070.272266	298466.560583	38.150989
2071.959367	299053.770476	38.156007
2074.207503	299641.874578	38.161024
2076.164798	300226.721663	38.166042
2078.548850	300824.574483	38.171060
2080.675736	301397.906676	38.176077
2082.501197	302003.844994	38.181095
2085.570540	302577.750521	38.186112
2087.191562	303166.318020	38.191130
2089.460386	303766.711075	38.196148
2091.564842	304358.974997	38.201165
2093.359176	304953.826048	38.206183
2096.767115	305530.628278	38.211200
2098.533405	306136.879025	38.216218
2100.640982	306724.631367	38.221236
2103.145244	307306.828423	38.226253
2104.967628	307882.074354	38.231271
2106.914868	308481.421504	38.236288
2108.714850	309075.938148	38.241306
2110.747045	309682.576323	38.246324
2113.000176	310284.576818	38.251341
2114.585440	310895.850918	38.256359
2116.400967	311499.793847	38.261376
2118.626290	312120.856273	38.266394
2120.368417	312726.731733	38.271412
2122.345184	313345.108166	38.276429
2124.373871	313975.126681	38.281447
2126.910476	314601.957695	38.286464
2128.166711	315246.516860	38.291482
2130.695965	315883.749361	38.296500
2132.696013	316496.483440	38.301517
2135.434960	317134.228671	38.306535
2137.903473	317742.303636	38.311552
2140.425155	318374.309399	38.316570
2142.818505	318987.946741	38.321588
2145.280533	319597.783781	38.326605
2147.619150	320207.508768	38.331623
2150.139041	320808.108036	38.336640
2152.221748	321405.879643	38.341658
2154.213038	321979.717284	38.346676
2156.452049	322555.920924	38.351693
2158.349304	323132.049030	38.356711
2160.926879	323691.073176	38.361728
2162.276584	324275.127131	38.366746
2164.094565	324861.332370	38.371764
2166.445385	325438.024298	38.376781
2168.416392	326029.169424	38.381799
2170.721205	326618.298564	38.386816
2172.235026	327214.484073	38.391834
2174.229252	327828.127540	38.396852
2176.109131	328435.131860	38.401869
2178.098687	329053.282451	38.406887
2180.179466	329669.811938	38.411904
2182.167971	330290.818302	38.416922
2184.555163	330920.764336	38.421940
2186.638318	331564.259529	38.426957
2188.788383	332207.736264	38.431975
2191.177910	332842.229930	38.436992
2193.149497	333488.640767	38.442010
2195.008397	334142.652943	38.447028
2197.363508	334796.067350	38.452045
2199.273220	335464.017056	38.457063
2202.243110	336092.766460	38.462080
2204.947179	336742.926107	38.467098
2207.605558	337390.191459	38.472116
2210.300519	338032.365925	38.477133
2212.454682	338669.976760	38.482151
2214.909153	339309.687482	38.487168
2217.334185	339962.847923	38.492186
2219.635317	340600.054789	38.497204
2221.680471	341243.641458	38.502221
2223.545557	341900.727353	38.507239
2225.472256	342550.103653	38.512256
2227.549550	343203.025113	38.517274
2230.095267	343851.545448	38.522292
2232.757460	344500.113871	38.527309
2235.068215	345146.142880	38.532327
2237.648776	345794.123385	38.537344
2240.420173	346436.809791	38.542362
2242.777837	347080.748652	38.547380
2245.304745	347703.611528	38.552397
2247.403079	348352.118353	38.557415
2250.154600	348983.174585	38.562432
2252.160564	349623.075392	38.567450
2254.092009	350260.619332	38.572468
2256.660337	350892.338886	38.577485
2259.141546	351509.218539	38.582503
2262.414761	352130.576880	38.587520
2265.330083	352742.038292	38.592538
2267.810507	353332.095390	38.597556
2270.578785	353929.049560	38.602573
2272.569563	354530.767751	38.607591
2275.080407	355114.070951	38.612608
2277.096345	355716.427915	38.617626
2279.688438	356308.302987	38.622644
2281.369463	356879.565073	38.627661
2283.149209	357494.825235	38.632679
2285.422742	358094.644007	38.637696
2287.664860	358696.032302	38.642714
2289.734265	359305.001168	38.647732
2292.244224	359890.444633	38.652749
2294.668175	360496.013190	38.657767
2298.032607	361059.986348	38.662784
2300.847694	361637.209748	38.667802
2303.372801	362219.369178	38.672820
2305.339219	362789.155983	38.677837
2307.467760	363351.068536	38.682855
2309.411689	363910.542763	38.687872
2311.556159	364460.284903	38.692890
2312.971667	365017.445959	38.697908
2314.617391	365567.610009	38.702925
2316.775175	366151.876760	38.707943
2318.925354	366722.209232	38.712960
2321.436202	367284.660418	38.717978
2323.524871	367884.766009	38.722996
2325.724146	368472.338242	38.728013
2327.440413	369072.156606	38.733031
2329.459291	369673.360945	38.738048
2331.543790	370292.249139	38.743066
2333.694122	370924.305362	38.748084
2335.949620	371534.647122	38.753101
2338.051521	372170.113748	38.758119
2339.698190	372807.977894	38.763136
2342.077787	373469.271035	38.768154
2343.522596	374131.366039	38.773172
2345.130858	374814.294081	38.778189
2347.274005	375509.902225	38.783207
2349.399482	376210.698327	38.788224
2351.057134	376928.320650	38.793242
2352.834422	377662.214333	38.798260
2355.425461	378398.518822	38.803277
2357.319580	379146.055061	38.808295
2359.740188	379904.213946	38.813312
2362.054039	380667.622340	38.818330
2364.392391	381436.283401	38.823348
2367.089532	382208.645307	38.828365
2369.319137	382975.944744	38.833383
2372.018125	383751.718433	38.838400
2374.522113	384528.190493	38.843418
2376.845706	385325.615832	38.848436
2379.959874	386096.422069	38.853453
2382.380452	386892.981085	38.858471
2385.142909	387675.722926	38.863488
2387.802861	388452.175271	38.868506
2389.920113	389232.602213	38.873524
2392.382812	390040.254155	38.878541
2394.454585	390828.405609	38.883559
2397.062658	391617.766246	38.888576
2399.616773	392410.613470	38.893594
2402.015229	393208.383162	38.898612
2404.451715	394010.713241	38.903629
2406.790764	394800.491881	38.908647
2409.388075	395594.338169	38.913664
2412.179494	396386.889248	38.918682
2414.854317	397185.748973	38.923700
2417.357474	397978.710458	38.928717
2420.138632	398765.978391	38.933735
2423.045819	399544.461232	38.938752
2426.096213	400312.940358	38.943770
2428.817031	401087.129718	38.948788
2431.349021	401850.458636	38.953805
2433.676081	402610.506900	38.958823
2436.647532	403373.899407	38.963840
2439.334899	404131.718589	38.968858
2441.574657	404899.599413	38.973876
2444.229367	405645.246482	38.978893
2446.556466	406400.656540	38.983911
2448.741917	407149.938279	38.988928
2451.391924	407898.970618	38.993946
2453.340370	408659.245216	38.998964
2455.993242	409407.551498	39.003981
2458.429356	410171.908080	39.008999
2460.212638	410928.726223	39.014016
2463.181331	411672.788049	39.019034
2465.578930	412425.003800	39.024052
2467.753946	413155.198596	39.029069
2469.964214	413898.056862	39.034087
2472.238784	414636.552360	39.039104
2474.481716	415368.016570	39.044122
2476.800739	416112.009412	39.049140
2478.981386	416843.822096	39.054157
2481.292473	417601.094481	39.059175
2483.421011	418352.499454	39.064192
2485.977897	419115.029580	39.069210
2488.014174	419886.333874	39.074228
2490.196588	420666.756858	39.079245
2492.653898	421459.137521	39.084263
2494.785105	422256.332503	39.089280
2497.321860	423050.674950	39.094298
2499.203855	423868.924967	39.099316
2501.422625	424682.737363	39.104333
2504.215157	425497.896089	39.109351
2506.345294	426335.567094	39.114368
2508.992115	427168.060581	39.119386
2511.633929	428017.436013	39.124404
2513.883573	428866.036222	39.129421
2516.979772	429713.909243	39.134439
2519.699506	430563.889806	39.139456
2522.596809	431408.343283	39.144474
2525.099703	432251.262471	39.149492
2527.485908	433104.294068	39.154509
2530.138899	433954.365127	39.159527
2533.811504	434787.078126	39.164544
2536.658252	435619.189116	39.169562
2539.841493	436457.641682	39.174580
2543.296957	437269.044144	39.179597
2546.004138	438088.739688	39.184615
2548.301500	438902.501969	39.189632
2551.452767	439720.445328	39.194650
2553.696036	440545.087192	39.199668
2556.489496	441358.728681	39.204685
2559.060295	442169.847311	39.209703
2561.559032	442978.165324	39.214720
2564.396266	443784.677415	39.219738
2567.543118	444583.519789	39.224756
2570.321290	445377.183130	39.229773
2572.984127	446171.595340	39.234791
2575.210486	446978.039471	39.239808
2578.120604	447769.974293	39.244826
2580.026804	448591.029628	39.249844
2582.591245	449387.817586	39.254861
2585.333041	450194.864293	39.259879
2587.728215	451003.657148	39.264896
2590.216517	451815.033387	39.269914
2592.078175	452631.084021	39.274932
2594.328796	453451.741444	39.279949
2597.446124	454268.480946	39.284967
2599.672511	455102.224875	39.289984
2602.870707	455913.728098	39.295002
2605.827099	456747.183361	39.300020
2608.667427	457552.461625	39.305037
2612.234782	458349.902793	39.310055
2614.784055	459158.654019	39.315072
2617.453093	459954.411047	39.320090
2620.375125	460750.549658	39.325108
2623.031910	461547.408184	39.330125
2625.441128	462339.776997	39.335143
2628.123712	463145.261560	39.340160
2631.174005	463934.427706	39.345178
2633.616573	464737.157588	39.350196
2635.302001	465539.878822	39.355213
2637.809462	466346.575179	39.360231
2640.017680	467143.230925	39.365248
2642.553154	467925.902912	39.370266
2644.581678	468719.744089	39.375284
2646.803682	469515.592210	39.380301
2649.357167	470307.259666	39.385319
2651.177059	471115.790187	39.390336
2653.744654	471924.718356	39.395354
2655.348407	472753.575801	39.400372
2657.774719	473593.374905	39.405389
2660.064436	474446.849100	39.410407
2662.867884	475315.353669	39.415424
2664.926372	476181.617461	39.420442
2667.386643	477059.240019	39.425460
2669.442221	477945.726618	39.430477
2671.957294	478848.710542	39.435495
2674.576990	479774.813159	39.440512
2677.581382	480666.061360	39.445530
2680.854599	481582.015464	39.450548
2683.886045	482496.246372	39.455565
2686.546281	483412.108046	39.460583
2689.082324	484330.922388	39.465600
2691.941102	485261.550958	39.470618
2694.520589	486191.419790	39.475636
2697.500421	487121.375495	39.480653
2701.005164	488043.017747	39.485671
2703.269185	488983.392146	39.490688
2706.020685	489910.815090	39.495706
2709.179269	490850.991342	39.500724
2712.312923	491784.055238	39.505741
2714.799184	492718.538408	39.510759
2717.458797	493667.071645	39.515776
2720.123349	494611.767074	39.520794
2722.677881	495561.373177	39.525812
2725.622598	496507.632594	39.530829
2728.702478	497436.814651	39.535847
2731.999269	498382.254893	39.540864
2735.191669	499312.121887	39.545882
2738.514012	500239.645723	39.550900
2741.182224	501165.208506	39.555917
2744.104567	502100.664160	39.560935
2746.607592	503037.245768	39.565952
2750.174406	503950.803032	39.570970
2753.314475	504865.741539	39.575988
2756.226259	505768.060061	39.581005
2759.762180	506671.485841	39.586023
2761.976210	507587.382482	39.591040
2764.461593	508477.066039	39.596058
2767.185995	509397.968326	39.601076
2769.437000	510323.785931	39.606093
2772.283925	511243.150155	39.611111
2774.140309	512171.143678	39.616128
2776.990829	513112.426338	39.621146
2779.562258	514042.863055	39.626164
2782.046594	514986.967047	39.631181
2784.565477	515946.328102	39.636199
2786.882435	516902.740909	39.641216
2789.496947	517851.285950	39.646234
2792.398345	518822.398391	39.651252
2795.456636	519797.353447	39.656269
2798.147931	520749.183814	39.661287
2800.698005	521734.981367	39.666304
2803.417024	522709.756589	39.671322
2806.878441	523691.851297	39.676340
2809.370686	524674.193645	39.681357
2812.528783	525631.180903	39.686375
2815.427686	526609.451698	39.691392
2817.938032	527583.090084	39.696410
2821.283162	528553.253865	39.701428
2824.000802	529509.561774	39.706445
2826.801974	530459.098065	39.711463
2829.369938	531409.115155	39.716480
2831.977973	532330.572244	39.721498
2835.015166	533253.863392	39.726516
2837.318726	534207.064666	39.731533
2840.622929	535133.715616	39.736551
2843.654058	536079.778274	39.741568
2846.664016	537006.508724	39.746586
2849.647196	537947.021714	39.751604
2852.430710	538893.694851	39.756621
2855.643793	539836.812845	39.761639
2858.233001	540792.297306	39.766656
2860.628442	541750.315000	39.771674
2862.909355	542707.280584	39.776692
2865.643692	543679.648543	39.781709
2868.597327	544649.548881	39.786727
2871.484730	545639.861744	39.791744
2874.190763	546623.797783	39.796762
2876.625346	547622.140706	39.801780
2879.695966	548624.680774	39.806797
2882.774502	549626.191250	39.811815
2885.394514	550628.860750	39.816832
2888.208362	551634.943558	39.821850
2891.382601	552661.903833	39.826868
2894.270202	553683.807523	39.831885
2897.337308	554699.271664	39.836903
2899.772275	555727.377836	39.841920
2903.068191	556766.820633	39.846938
2906.528555	557791.885205	39.851956
2908.860599	558837.808049	39.856973
2911.812521	559875.005280	39.861991
2914.725973	560916.950149	39.867008
2917.469005	561962.758888	39.872026
2920.444391	563023.865731	39.877044
2922.904567	564082.058779	39.882061
2925.872301	565159.818137	39.887079
2928.757539	566235.442888	39.892096
2931.064362	567316.346031	39.897114
2934.038717	568406.738024	39.902132
2936.426280	569510.538503	39.907149
2939.474934	570602.990503	39.912167
2942.345836	571713.949914	39.917184
2945.420459	572827.087156	39.922202
2948.825739	573920.951386	39.927220
2952.002089	575038.895322	39.932237
2955.874838	576124.562141	39.937255
2959.525642	577212.880721	39.942272
2963.133613	578305.776925	39.947290
2966.448056	579378.108909	39.952308
2969.559650	580465.278619	39.957325
2972.735162	581534.186151	39.962343
2976.103552	582593.891713	39.967360
2979.287587	583645.262068	39.972378
2982.355602	584713.157759	39.977396
2985.484588	585766.610512	39.982413
2988.550948	586805.293272	39.987431
2991.795089	587849.722318	39.992448
2994.748982	588893.156408	39.997466
2997.941364	589933.703762	40.002484
3000.802256	590974.265515	40.007501
3003.918695	592009.131888	40.012519
3007.073932	593041.596806	40.017536
3009.766437	594081.864122	40.022554
3012.548640	595115.562344	40.027572
3014.994981	596170.264365	40.032589
3017.928788	597203.102566	40.037607
3020.900837	598264.541352	40.042624
3023.830878	599281.720172	40.047642
3027.044269	600293.304811	40.052660
3029.438748	601319.006362	40.057677
3032.219724	602330.083618	40.062695
3034.664321	603360.451545	40.067712
3037.420429	604383.917597	40.072730
3040.784875	605425.360612	40.077748
3043.026469	606474.201129	40.082765
3045.822694	607509.991822	40.087783
3048.703310	608576.647959	40.092800
3051.121354	609644.180347	40.097818
3054.212369	610713.901525	40.102836
3056.573647	611807.102837	40.107853
3059.366007	612915.882094	40.112871
3062.092583	614031.963969	40.117888
3065.053677	615158.296793	40.122906
3067.684476	616304.021216	40.127924
3070.416149	617461.009647	40.132941
3072.992139	618634.149911	40.137959
3075.680354	619810.445097	40.142976
3078.892736	620989.875589	40.147994
3082.272328	622180.045502	40.153012
3085.195293	623385.651390	40.158029
3088.649117	624585.288660	40.163047
3092.351457	625800.038946	40.168064
3094.844567	627007.308204	40.173082
3098.714818	628217.959438	40.178100
3102.314717	629429.016993	40.183117
3105.359905	630626.045239	40.188135
3109.033087	631849.348042	40.193152
3112.264483	633053.010514	40.198170
3115.839646	634250.187984	40.203188
3119.669137	635461.861284	40.208205
3122.926850	636642.444573	40.213223
3126.860804	637840.098328	40.218240
3130.369615	639030.648097	40.223258
3134.035159	640200.528793	40.228276
3137.237705	641385.717843	40.233293
3140.042649	642558.664582	40.238311
3143.509578	643736.603948	40.243328
3145.898577	644916.081196	40.248346
3149.161057	646090.290503	40.253364
3151.893830	647285.191656	40.258381
3154.914058	648485.985412	40.263399
3157.651331	649688.875506	40.268416
3160.345066	650898.904740	40.273434
3163.086163	652114.858980	40.278452
3166.214236	653337.078002	40.283469
3168.945159	654578.392940	40.288487
3171.860494	655811.650550	40.293504
3175.060712	657063.534030	40.298522
3177.962789	658311.422353	40.303540
3181.155019	659579.220737	40.308557
3184.264782	660840.594214	40.313575
3187.405100	662101.251026	40.318592
3190.179656	663383.207641	40.323610
3193.882927	664651.949872	40.328628
3197.471573	665934.924837	40.333645
3200.983741	667199.977443	40.338663
3203.831524	668466.116281	40.343680
3206.865206	669748.968298	40.348698
3210.360494	671016.450439	40.353716
3213.424460	672311.632424	40.358733
3216.624032	673582.846256	40.363751
3220.089272	674866.223026	40.368768
3223.063870	676148.758957	40.373786
3226.540768	677434.067017	40.378804
3229.663782	678707.626836	40.383821
3233.336771	679978.187484	40.388839
3236.676351	681205.802444	40.393856
3240.531914	682436.496294	40.398874
3243.945938	683642.710455	40.403892
3246.932930	684857.477002	40.408909
3249.843966	686077.158792	40.413927
3253.202631	687294.864893	40.418944
3256.056886	688517.156727	40.423962
3259.107401	689743.320468	40.428980
3262.325157	690976.088330	40.433997
3265.005532	692225.497785	40.439015
3268.085221	693465.785417	40.444032
3271.074638	694727.147154	40.449050
3274.429775	695991.344323	40.454068
3277.523653	697270.430693	40.459085
3280.146248	698552.186166	40.464103
3283.502273	699843.350854	40.469120
3286.393734	701156.560325	40.474138
3289.414155	702463.256300	40.479156
3292.823828	703792.438003	40.484173
3295.346429	705123.544497	40.489191
3298.713903	706464.115431	40.494208
3302.079137	707827.065163	40.499226
3304.805246	709183.366771	40.504244
3308.039156	710568.287511	40.509261
3311.153729	711955.428928	40.514279
3314.914087	713337.336506	40.519296
3318.016211	714729.471321	40.524314
3321.421745	716128.847969	40.529332
3326.195118	717501.839918	40.534349
3330.379028	718870.400497	40.539367
3334.380035	720240.844330	40.544384
3338.066761	721611.510049	40.549402
3341.840163	722975.655552	40.554420
3345.028404	724345.753294	40.559437
3348.238888	725713.642462	40.564455
3352.325598	727049.332823	40.569472
3355.828269	728416.376837	40.574490
3359.813252	729762.066362	40.579508
3363.855047	731081.344411	40.584525
3367.438007	732404.582702	40.589543
3371.800680	733719.476044	40.594560
3375.091899	735036.454753	40.599578
3378.513772	736342.533509	40.604596
3382.246617	737644.103262	40.609613
3385.425911	738938.939734	40.614631
3388.665743	740237.107873	40.619648
3391.500238	741557.181343	40.624666
3395.023743	742857.882136	40.629684
3398.632875	744167.822485	40.634701
3401.442385	745470.182098	40.639719
3404.842011	746778.537835	40.644736
3407.856405	748108.524021	40.649754
3411.023245	749423.227132	40.654772
3414.498028	750748.496679	40.659789
3417.860429	752079.321733	40.664807
3421.081378	753399.252088	40.669824
3424.534936	754745.067730	40.674842
3427.952102	756071.696306	40.679860
3431.025401	757404.354421	40.684877
3433.841036	758751.588448	40.689895
3437.702656	760088.469762	40.694912
3440.951893	761452.179921	40.699930
3444.528748	762805.849013	40.704948
3447.703237	764160.472371	40.709965
3450.760760	765525.591082	40.714983
3454.864376	766866.392041	40.720000
3458.670493	768218.061856	40.725018
3462.286670	769535.368974	40.730023
3466.557744	770813.518950	40.735028
3469.513359	772035.361623	40.740032
3472.564668	773189.609597	40.745037
3475.330933	774299.058800	40.750042
3478.346635	775329.076119	40.755047
3481.220438	776308.067197	40.760052
3483.585637	777220.557824	40.765056
3486.246350	778060.435132	40.770061
3488.915326	778839.927338	40.775066
3491.195298	779546.472660	40.780071
3493.655215	780193.086745	40.785076
3495.360590	780785.007632	40.790080
3497.526760	781317.423372	40.795085
3499.523008	781796.502108	40.800090
3501.286812	782233.135926	40.805095
3503.019547	782598.475003	40.810100
3504.230510	782918.729095	40.815104
3505.687518	783199.236786	40.820109
3507.048659	783442.026515	40.825114
3507.850846	783640.588361	40.830119
3509.316284	783815.084545	40.835124
3509.808134	783955.115466	40.840128
3510.607912	784040.898433	40.845133
3511.363614	784128.556410	40.850138
3512.689718	784163.548498	40.855143
3513.063312	784189.845893	40.860148
3513.398130	784180.299370	40.865152
3514.326264	784149.262570	40.870157
3514.869251	784100.929490	40.875162
3515.092125	784021.568251	40.880167
3515.879021	783941.621146	40.885172
3516.273118	783845.853040	40.890176
3517.403181	783721.240676	40.895181
3516.909665	783587.894237	40.900186
3517.190896	783438.383835	40.905191
3517.767919	783273.574549	40.910196
3517.727443	783109.798035	40.915200
3518.221205	782905.105155	40.920205
3518.651445	782712.172759	40.925210
3518.310219	782505.638998	40.930215
3518.407013	782291.107297	40.935220
3518.698380	782080.570782	40.940224
3518.855532	781851.897993	40.945229
3518.931614	781619.492540	40.950234
3519.231377	781376.662178	40.955239
3519.387832	781130.452657	40.960244
3519.244768	780883.005040	40.965248
3519.374929	780629.009190	40.970253
3519.244793	780373.718942	40.975258
3519.495980	780115.109137	40.980263
3519.665840	779846.957395	40.985268
3519.421005	779576.256189	40.990272
3519.456729	779301.266396	40.995277
3519.287918	779015.522425	41.000282
3519.269135	778744.506757	41.005287
3519.221987	778465.906352	41.010292
3518.998742	778186.635310	41.015296
3519.495608	777898.621026	41.020301
3519.264437	777626.466705	41.025306
3519.151526	777332.033459	41.030311
3519.391001	777039.302218	41.035316
3519.220989	776757.013979	41.040320
3519.111791	776460.871185	41.045325
3518.998873	776173.627952	41.050330
3518.853454	775888.003506	41.055335
3518.980683	775592.131058	41.060340
3518.690379	775305.523082	41.065344
3518.948119	775018.714840	41.070349
3518.764865	774731.377342	41.075354
3518.494744	774435.720783	41.080359
3518.267676	774146.594832	41.085364
3517.797136	773861.683744	41.090368
3518.172242	773573.519155	41.095373
3517.905259	773294.314582	41.100378
3518.073241	773008.132102	41.105383
3518.054202	772726.747127	41.110388
3518.158128	772446.611755	41.115392
3518.049519	772146.649569	41.120397
3517.557299	771869.152208	41.125402
3517.359996	771579.624863	41.130407
3517.139890	771294.967114	41.135412
3516.927869	771026.111557	41.140416
3517.495245	770741.499424	41.145421
3516.916081	770470.812144	41.150426
3516.993028	770194.044647	41.155431
3517.365392	769915.247041	41.160436
3517.150056	769651.417265	41.165440
3516.932942	769359.293216	41.170445
3516.979061	769092.049468	41.175450
3516.397473	768815.585717	41.180455
3516.667351	768539.414516	41.185460
3516.349016	768275.404988	41.190464
3516.329677	767994.480728	41.195469
3516.413849	767727.970220	41.200474
3516.013220	767462.417502	41.205479
3515.992750	767197.236122	41.210484
3515.760686	766931.685925	41.215488
3515.818950	766665.289572	41.220493
3515.533957	766412.743582	41.225498
3515.295463	766156.286775	41.230503
3515.390540	765892.173794	41.235508
3515.137760	765649.210229	41.240512
3515.390555	765394.026546	41.245517
3515.112686	765146.021815	41.250522
3514.912683	764901.053029	41.255527
3514.834193	764647.131312	41.260532
3514.343968	764405.793816	41.265536
3514.708762	764156.072204	41.270541
3514.544220	763919.349861	41.275546
3514.295405	763674.299761	41.280551
3514.088902	763431.355286	41.285556
3514.075558	763209.528488	41.290560
3514.098364	762955.434192	41.295565
3514.099890	762732.604484	41.300570
3513.899368	762492.341361	41.305575
3513.325459	762250.603222	41.310580
3513.208810	762030.041178	41.315584
3513.587786	761802.534307	41.320589
3513.187590	761579.736902	41.325594
3512.770678	761351.608027	41.330599
3513.095821	761128.036144	41.335604
3513.307710	760916.562956	41.340608
3513.158274	760692.513956	41.345613
3513.033360	760467.516886	41.350618
3512.485776	760251.463694	41.355623
3512.916480	760021.575839	41.360628
3512.746070	759817.239902	41.365632
3512.739852	759602.558949	41.370637
3512.736479	759390.091883	41.375642
3512.426858	759180.432754	41.380647
3512.439923	758963.608734	41.385652
3512.275247	758757.762946	41.390656
3512.312098	758545.018854	41.395661
3512.111589	758334.430073	41.400666
3512.101060	758131.502842	41.405671
3512.076165	757918.702087	41.410676
3511.708884	757732.158813	41.415680
3511.661880	757518.610226	41.420685
3511.420527	757332.727332	41.425690
3511.102265	757128.343538	41.430695
3511.107008	756929.675882	41.435700
3510.793407	756744.975213	41.440704
3511.049755	756555.832101	41.445709
3510.949694	756375.381637	41.450714
3510.829685	756184.711930	41.455719
3510.798590	756005.771618	41.460724
3510.979382	755824.126342	41.465728
3510.944273	755625.826302	41.470733
3510.888752	755443.124953	41.475738
3510.518916	755259.483791	41.480743
3510.381694	755083.156039	41.485748
3510.440194	754899.583582	41.490752
3510.190471	754722.476171	41.495757
3510.401415	754549.287861	41.500762
3510.304674	754378.812756	41.505767
3510.266615	754188.573572	41.510772
3509.678560	754018.221023	41.515776
3509.755777	753851.951952	41.520781
3509.909470	753686.901143	41.525786
3509.467611	753515.525693	41.530791
3509.676429	753351.100520	41.535796
3509.438082	753194.597619	41.540800
3509.357370	753031.151732	41.545805
3509.422563	752875.925561	41.550810
3509.250404	752710.463195	41.555815
3509.705504	752550.573138	41.560820
3509.279214	752390.183370	41.565824
3509.201913	752225.485129	41.570829
3509.123562	752075.748762	41.575834
3508.873037	751907.368096	41.580839
3509.082653	751759.998187	41.585844
3508.626946	751611.895727	41.590848
3508.615227	751468.508278	41.595853
3508.937727	751315.134557	41.600858
3508.764982	751159.369836	41.605863
3509.022972	751003.283815	41.610868
3508.563747	750858.230105	41.615872
3508.630502	750700.638247	41.620877
3508.501277	750563.082500	41.625882
3508.207867	750413.695276	41.630887
3508.477322	750255.566861	41.635892
3508.109972	750120.364482	41.640896
3507.860308	749988.845555	41.645901
3508.193637	749841.566891	41.650906
3507.705717	749714.232643	41.655911
3507.797045	749574.202048	41.660916
3507.611263	749450.914253	41.665920
3507.913350	749311.832237	41.670925
3507.662280	749181.139784	41.675930
3507.356961	749043.932053	41.680935
3507.796063	748899.137924	41.685940
3507.205155	748788.259139	41.690944
3507.160005	748641.712029	41.695949
3507.370027	748528.621886	41.700954
3507.161992	748409.373088	41.705959
3507.228598	748281.034269	41.710964
3506.874286	748167.834483	41.715968
3506.912942	748039.446887	41.720973
3507.100129	747921.163034	41.725978
3506.990152	747806.632791	41.730983
3507.047691	747683.227353	41.735988
3506.863496	747565.691331	41.740992
3506.917860	747442.529703	41.745997
3506.771806	747326.565202	41.751002
3506.770115	747201.580482	41.756007
3506.854236	747092.691109	41.761012
3506.493800	746975.076470	41.766016
3506.495419	746865.950456	41.771021
3506.144999	746752.729480	41.776026
3506.262192	746646.892714	41.781031
3506.939786	746532.114776	41.786036
3506.410177	746424.256588	41.791040
3506.461910	746311.605305	41.796045
3506.580439	746199.831057	41.801050
3506.197656	746088.681763	41.806055
3506.361616	745979.170552	41.811060
3505.849216	745882.423530	41.816064
3506.166443	745776.492507	41.821069
3505.965150	745670.843461	41.826074
3505.811689	745567.409501	41.831079
3505.814769	745462.267615	41.836084
3505.580500	745369.076832	41.841088
3505.525930	745279.859341	41.846093
3505.853969	745181.679516	41.851098
3505.689695	745081.256394	41.856103
3506.089738	744979.651161	41.861108
3505.690101	744885.888740	41.866112
3505.726776	744784.637643	41.871117
3505.319058	744692.357336	41.876122
3504.943620	744602.048110	41.881127
3505.530930	744501.097867	41.886132
3505.438455	744421.369004	41.891136
3505.548406	744321.286355	41.896141
3505.263047	744233.429969	41.901146
3505.304858	744142.008267	41.906151
3505.405087	744034.804152	41.911156
3505.170892	743952.918548	41.916160
3505.392017	743863.441641	41.921165
3505.098215	743773.702710	41.926170
3505.208646	743695.070136	41.931175
3505.419762	743597.928160	41.936180
3505.121026	743519.905333	41.941184
3505.186324	743419.966931	41.946189
3504.886562	743335.020141	41.951194
3504.504207	743250.629990	41.956199
3504.556812	743168.293259	41.961204
3504.589568	743096.787848	41.966208
3504.895706	743021.676395	41.971213
3504.856193	742942.912750	41.976218
3504.504484	742869.490891	41.981223
3504.709071	742783.218598	41.986228
3504.820097	742700.422288	41.991232
3504.496209	742618.438728	41.996237
3504.953545	742542.209828	42.001242
3504.555373	742467.110584	42.006247
3504.700426	742387.222971	42.011252
3504.614725	742307.669393	42.016256
3504.454088	742231.094543	42.021261
3504.446819	742165.768859	42.026266
3504.257585	742087.515946	42.031271
3504.507066	742011.167912	42.036276
3504.241523	741944.498372	42.041280
3504.080293	741871.431381	42.046285
3503.883272	741807.914463	42.051290
3504.117725	741740.962761	42.056295
3504.379482	741659.713212	42.061300
3504.593292	741588.164220	42.066304
3504.130055	741517.072661	42.071309
3504.324320	741448.394135	42.076314
3504.121858	741388.880791	42.081319
3504.272227	741299.633803	42.086324
3503.933587	741244.246908	42.091328
3504.061676	741161.035985	42.096333
3504.048540	741098.076489	42.101338
3503.998398	741045.855398	42.106343
3503.892052	740969.209895	42.111348
3503.614784	740896.499297	42.116352
3503.408364	740829.612744	42.121357
3504.020931	740775.499757	42.126362
3503.726830	740719.162057	42.131367
3503.869446	740662.207706	42.136372
3503.614797	740599.580931	42.141376
3503.683134	740529.282982	42.146381
3503.998936	740469.528697	42.151386
3503.714672	740416.550733	42.156391
3503.751127	740350.856599	42.161396
3503.700593	740284.879509	42.166400
3503.593872	740220.543499	42.171405
3503.842357	740165.596153	42.176410
3503.477227	740109.908910	42.181415
3503.536775	740036.293845	42.186420
3503.383142	739987.594980	42.191424
3503.354912	739933.483217	42.196429
3503.607162	739877.395520	42.201434
3503.378296	739828.213438	42.206439
3503.898817	739760.604135	42.211444
3503.478613	739712.046566	42.216448
3503.092866	739655.963797	42.221453
3503.482838	739592.431053	42.226458
3503.369703	739544.662688	42.231463
3503.302833	739478.978417	42.236468
3503.370380	739426.183051	42.241472
3503.191780	739367.046346	42.246477
3503.306442	739327.005862	42.251482
3503.105286	739283.455468	42.256487
3503.574320	739224.062266	42.261492
3503.408519	739173.579459	42.266496
3503.138880	739114.752750	42.271501
3503.303923	739066.539768	42.276506
3502.872595	739019.513440	42.281511
3503.022561	738965.118276	42.286516
3503.011067	738920.545097	42.291520
3503.012004	738863.007586	42.296525
3502.937343	738820.868484	42.301530
3502.884395	738775.509764	42.306535
3503.503704	738712.476316	42.311540
3502.993596	738664.471418	42.316544
3502.952574	738617.675063	42.321549
3503.249196	738567.408845	42.326554
3503.140326	738527.203377	42.331559
3502.902979	738471.631960	42.336564
3503.157651	738420.679087	42.341568
3502.681322	738365.195895	42.346573
3502.341904	738336.110293	42.351578
3502.699278	738301.417505	42.356583
3502.955216	738242.349066	42.361588
3502.664325	738212.463357	42.366592
3502.635775	738160.467119	42.371597
3502.594348	738125.047822	42.376602
3502.474524	738081.873236	42.381607
3502.675131	738038.150680	42.386612
3502.468705	738000.630518	42.391616
3502.703893	737957.347114	42.396621
3502.727017	737918.700094	42.401626
3502.113415	737871.944500	42.406631
3502.509139	737838.826712	42.411636
3502.375118	737791.397637	42.416640
3502.161261	737771.987315	42.421645
3502.767192	737730.521665	42.426650
3502.526547	737684.841392	42.431655
3502.569587	737654.502562	42.436660
3502.494904	737620.224580	42.441664
3502.495512	737580.144689	42.446669
3502.410250	737537.109888	42.451674
3502.475516	737512.556198	42.456679
3502.500086	737456.390123	42.461684
3502.757669	737428.093230	42.466688
3502.458743	737379.402417	42.471693
3502.641427	737349.138317	42.476698
3502.339477	737304.703069	42.481703
3502.360988	737256.107002	42.486708
3502.260565	737222.672784	42.491712
3502.280263	737187.585612	42.496717
3502.396221	737150.799921	42.501722
3502.352136	737121.364177	42.506727
3502.775723	737073.096428	42.511732
3502.409022	737037.082756	42.516736
3502.282131	737008.204612	42.521741
3502.347091	736970.090424	42.526746
3502.496848	736924.489743	42.531751
3502.148201	736879.713449	42.536756
3501.902557	736853.675055	42.541760
3501.918652	736822.743691	42.546765
3502.105128	736797.821373	42.551770
3502.178016	736771.829048	42.556775
3502.336002	736736.914992	42.561780
3502.199803	736714.965448	42.566784
3501.875505	736672.757281	42.571789
3502.038481	736645.611458	42.576794
3501.673785	736616.672222	42.581799
3501.857685	736585.217335	42.586804
3501.952553	736563.427142	42.591808
3501.786468	736530.990636	42.596813
3502.011687	736505.417665	42.601818
3501.760920	736471.163853	42.606823
3501.699436	736451.131280	42.611828
3502.048276	736426.428419	42.616832
3501.636551	736389.825407	42.621837
3502.090214	736370.994213	42.626842
3501.669272	736346.071888	42.631847
3501.679663	736317.910900	42.636852
3501.886225	736292.884715	42.641856
3501.506095	736272.656905	42.646861
3501.760993	736236.685375	42.651866
3501.610990	736222.605619	42.656871
3501.665898	736193.199592	42.661876
3501.762986	736162.499742	42.666880
3501.407595	736153.056387	42.671885
3501.706695	736115.988227	42.676890
3501.750324	736106.280918	42.681895
3501.656115	736072.890358	42.686900
3501.861854	736055.633607	42.691904
3501.571068	736027.224422	42.696909
3501.784118	736005.413182	42.701914
3501.579594	735992.084397	42.706919
3501.771162	735977.056923	42.711924
3502.071254	735946.966089	42.716928
3501.716214	735925.248508	42.721933
3501.653465	735887.892649	42.726938
3501.702671	735877.887190	42.731943
3501.749035	735835.662847	42.736948
3501.739885	735825.370013	42.741952
3501.131612	735794.686332	42.746957
3501.488746	735773.395069	42.751962
3501.477784	735755.084645	42.756967
3501.852026	735724.832248	42.761972
3501.597033	735710.026547	42.766976
3501.431373	735680.209651	42.771981
3501.573427	735673.999565	42.776986
3501.568117	735647.125638	42.781991
3501.663240	735625.926775	42.786996
3501.693559	735600.185153	42.792001
3501.611475	735576.144811	42.797005
3501.798284	735558.543664	42.802010
3501.691216	735534.853784	42.807015
3501.544902	735500.182605	42.812020
3501.659400	735490.066885	42.817025
3501.685723	735450.813487	42.822029
3501.883470	735434.249646	42.827034
3501.315416	735414.050717	42.832039
3501.589876	735385.941809	42.837044
3501.528350	735382.932816	42.842049
3501.273681	735347.091002	42.847053
3501.828740	735334.427523	42.852058
3501.515728	735310.672023	42.857063
3501.605173	735286.008522	42.862068
3501.233975	735273.448516	42.867073
3501.612422	735244.975462	42.872077
3501.544660	735229.890454	42.877082
3501.418493	735218.180797	42.882087
3501.796554	735190.945015	42.887092
3501.670178	735172.701831	42.892097
3501.356442	735149.391438	42.897101
3501.332187	735131.329271	42.902106
3501.071827	735110.633260	42.907111
3501.345927	735095.788487	42.912116
3501.438910	735086.962731	42.917121
3501.504182	735055.224472	42.922125
3501.469883	735041.618490	42.927130
3501.319711	735017.686720	42.932135
3501.270956	734998.588861	42.937140
3501.254073	734997.403748	42.942145
3501.212207	734972.760985	42.947149
3501.496754	734948.608680	42.952154
3501.469571	734941.832025	42.957159
3501.488888	734909.605808	42.962164
3501.540776	734899.450194	42.967169
3501.245782	734875.789423	42.972173
3501.156648	734857.539369	42.977178
3501.107881	734855.419037	42.982183
3501.168893	734841.549475	42.987188
3501.233883	734822.630394	42.992193
3501.175832	734799.029239	42.997197
3501.220432	734796.002489	43.002202
3500.958654	734773.870385	43.007207
3500.874504	734761.113644	43.012212
3500.728128	734755.890991	43.017217
3501.196122	734752.843758	43.022221
3501.478094	734744.332887	43.027226
3501.189755	734720.373565	43.032231
3501.403386	734698.657683	43.037236
3500.961400	734691.602868	43.042241
3501.042067	734660.998991	43.047245
3501.431670	734643.015834	43.052250
3500.969405	734640.270783	43.057255
3501.046544	734618.923737	43.062260
3501.298016	734608.685275	43.067265
3501.105719	734595.748144	43.072269
3501.561094	734585.079959	43.077274
3501.139967	734562.726105	43.082279
3501.277621	734547.853372	43.087284
3501.125711	734533.077961	43.092289
3501.274619	734517.460808	43.097293
3501.286235	734505.380840	43.102298
3500.986281	734491.520824	43.107303
3501.431415	734480.062185	43.112308
3501.166575	734465.503314	43.117313
3501.391562	734450.714970	43.122317
3501.548283	734442.174979	43.127322
3501.204404	734425.401561	43.132327
3501.584307	734413.310096	43.137332
3501.313344	734386.178845	43.142337
3501.260200	734377.970472	43.147341
3501.519735	734350.949442	43.152346
3501.269053	734340.051100	43.157351
3501.132881	734322.302618	43.162356
3501.393586	734303.943994	43.167361
3501.054677	734283.555840	43.172365
3501.405077	734270.181991	43.177370
3501.414779	734266.220275	43.182375
3501.504697	734234.969725	43.187380
3501.541581	734231.894536	43.192385
3501.355396	734191.432554	43.197389
3501.346880	734170.395488	43.202394
3501.213808	734167.843384	43.207399
3501.279709	734141.348674	43.212404
3501.242180	734134.919567	43.217409
3501.223667	734121.853949	43.222413
3501.517895	734104.231872	43.227418
3500.850310	734104.391726	43.232423
3501.123336	734076.823016	43.237428
3501.088197	734057.968188	43.242433
3501.316654	734053.574192	43.247437
3501.144629	734037.316099	43.252442
3500.951726	734030.516558	43.257447
3501.339092	734001.245584	43.262452
3501.198194	733991.962242	43.267457
3501.145565	733989.495795	43.272461
3501.414868	733965.937108	43.277466
3501.168237	733956.077153	43.282471
3501.235963	733941.165351	43.287476
3500.990220	733919.523282	43.292481
3501.175998	733914.245192	43.297485
3501.255160	733893.093905	43.302490
3500.936394	733890.126861	43.307495
3500.978818	733863.981647	43.312500
3500.781903	733856.737082	43.317505
3501.327935	733857.092423	43.322509
3501.315455	733840.758064	43.327514
3500.794396	733829.260150	43.332519
3501.002857	733810.810029	43.337524
3501.241990	733809.483425	43.342529
3500.986344	733798.931701	43.347533
3501.020288	733772.589573	43.352538
3500.959208	733763.688817	43.357543
3501.129214	733746.433021	43.362548
3500.993793	733749.722765	43.367553
3501.290361	733738.337133	43.372557
3501.279965	733708.734787	43.377562
3500.967729	733715.766657	43.382567
3501.022666	733703.925854	43.387572
3501.392507	733688.815146	43.392577
3501.338099	733685.457802	43.397581
3501.236292	733673.692363	43.402586
3501.105111	733639.901756	43.407591
3501.259202	733622.301786	43.412596
3501.296367	733628.582912	43.417601
3501.063852	733608.422992	43.422605
3501.473410	733584.988534	43.427610
3501.540683	733578.591170	43.432615
3501.436169	733560.489232	43.437620
3501.389065	733533.021073	43.442625
3501.129897	733517.370406	43.447629
3501.221514	733485.176046	43.452634
3500.981316	733494.919068	43.457639
3501.324741	733482.980762	43.462644
3501.312292	733462.685098	43.467649
3500.838120	733448.307495	43.472653
3500.992085	733437.093525	43.477658
3500.896806	733431.416003	43.482663
3500.960292	733406.949064	43.487668
3501.130217	733391.771823	43.492673
3500.824936	733398.703804	43.497677
3501.183362	733377.406002	43.502682
3501.016110	733368.918413	43.507687
3501.256780	733343.085301	43.512692
3501.316798	733347.679614	43.517697
3501.081438	733339.005218	43.522701
3501.259788	733306.498768	43.527706
3501.144789	733301.022444	43.532711
3501.149284	733288.644781	43.537716
3501.575067	733274.217165	43.542721
3501.198555	733257.644733	43.547725
3501.295326	733246.340934	43.552730
3501.212671	733218.927088	43.557735
3501.066079	733209.792309	43.562740
3500.969475	733209.709289	43.567745
3500.827065	733205.326613	43.572749
3501.128257	733179.433469	43.577754
3501.303469	733172.225809	43.582759
3501.225976	733159.168377	43.587764
3501.024413	733144.943217	43.592769
3501.452381	733115.464289	43.597773
3501.389770	733109.533597	43.602778
3501.039713	733107.017012	43.607783
3501.283257	733072.914561	43.612788
3501.299102	733061.277312	43.617793
3501.077184	733054.085665	43.622797
3501.299068	733017.907171	43.627802
3501.225799	733012.473264	43.632807
3501.310627	733019.588650	43.637812
3501.133136	732989.763731	43.642817
3501.250609	732975.138983	43.647821
3501.254867	732964.097625	43.652826
3500.968496	732956.074874	43.657831
3501.306954	732940.571877	43.662836
3501.419181	732931.938623	43.667841
3501.202475	732920.438620	43.672845
3501.637262	732894.324446	43.677850
3501.367985	732888.774316	43.682855
3501.072453	732867.236666	43.687860
3500.891226	732856.770428	43.692865
3500.953211	732838.490824	43.697869
3501.203058	732833.647039	43.702874
3500.910915	732815.128838	43.707879
3501.538586	732802.994027	43.712884
3501.063765	732806.884857	43.717889
3500.823275	732790.982137	43.722893
3501.305606	732761.641470	43.727898
3500.909473	732761.756475	43.732903
3501.003414	732754.413341	43.737908
3501.006326	732750.303469	43.742913
3500.801787	732728.849435	43.747917
3501.377087	732713.554422	43.752922
3501.265516	732706.146182	43.757927
3501.176745	732692.891814	43.762932
3501.171220	732670.909623	43.767937
3500.953954	732669.064117	43.772941
3501.093153	732656.415668	43.777946
3501.026377	732658.753786	43.782951
3501.404940	732628.142479	43.787956
3501.308645	732621.721875	43.792961
3501.041804	732614.438234	43.797965
3501.055002	732591.809079	43.802970
3500.996871	732577.460190	43.807975
3501.370929	732574.873287	43.812980
3501.329732	732556.065461	43.817985
3500.863172	732529.504911	43.822989
3500.656135	732527.162557	43.827994
3500.570296	732521.532346	43.832999
3500.852472	732515.643266	43.838004
3500.981473	732514.532705	43.843009
3501.029398	732503.533015	43.848013
3501.081299	732470.202382	43.853018
3500.947268	732473.343873	43.858023
3500.879230	732463.898191	43.863028
3501.098739	732462.624127	43.868033
3501.089636	732444.107815	43.873037
3501.192984	732416.313915	43.878042
3500.941584	732423.138796	43.883047
3500.716750	732417.432455	43.888052
3501.207501	732394.575293	43.893057
3501.099307	732388.899170	43.898061
3500.961781	732376.791147	43.903066
3500.851062	732381.463738	43.908071
3501.079848	732359.937116	43.913076
3501.275357	732340.891619	43.918081
3501.104209	732329.828868	43.923085
3501.087116	732325.375489	43.928090
3500.766347	732299.681338	43.933095
3501.030839	732289.932931	43.938100
3501.113931	732287.938674	43.943105
3500.735471	732296.171051	43.948109
3501.024175	732283.002173	43.953114
3500.884937	732262.724445	43.958119
3500.516592	732249.763119	43.963124
3500.945218	732234.937072	43.968129
3501.225574	732244.199460	43.973133
3501.126541	732237.036289	43.978138
3500.997106	732218.539345	43.983143
3500.930736	732204.933873	43.988148
3500.746336	732196.992541	43.993153
3500.711294	732200.167295	43.998157
3500.967511	732196.758000	44.003162
3500.892465	732179.341298	44.008167
3500.969132	732162.295605	44.013172
3500.991431	732153.923956	44.018177
3500.514085	732154.795108	44.023181
3500.474476	732158.366751	44.028186
3500.920883	732154.430862	44.033191
3500.991545	732145.506549	44.038196
3500.964851	732120.704014	44.043201
3500.804900	732108.005113	44.048205
3501.048346	732104.053224	44.053210
3500.705961	732101.980686	44.058215
3500.853435	732100.272835	44.063220
3501.011748	732073.013340	44.068225
3500.989576	732061.578995	44.073229
3501.174151	732053.229941	44.078234
3501.111066	732055.518108	44.083239
3501.016598	732040.134447	44.088244
3501.155685	732027.980190	44.093249
3500.927425	732024.205243	44.098253
3501.151036	732009.214601	44.103258
3500.966918	732005.085740	44.108263
3500.963945	731964.235699	44.113268
3501.079427	731960.453435	44.118273
3500.881951	731973.954438	44.123277
3501.039663	731961.301844	44.128282
3500.995255	731934.966671	44.133287
3500.877413	731929.886013	44.138292
3500.931067	731922.598300	44.143297
3500.658041	731931.209751	44.148301
3501.031796	731911.143466	44.153306
3500.787353	731901.231114	44.158311
3500.672157	731884.315574	44.163316
3500.798924	731879.739144	44.168321
3500.696574	731875.646222	44.173325
3501.053641	731874.993052	44.178330
3500.972977	731877.828855	44.183335
3500.812920	731856.810802	44.188340
3500.777848	731833.939920	44.193345
3500.668092	731831.284185	44.198349
3500.757413	731829.635404	44.203354
3500.501787	731826.558121	44.208359
3500.845351	731826.798481	44.213364
3501.272498	731824.648222	44.218369
3500.453924	731809.977983	44.223373
3500.723329	731794.088071	44.228378
3500.881766	731784.901272	44.233383
3500.863198	731785.944232	44.238388
3501.050374	731787.349328	44.243393
3500.935028	731789.250070	44.248397
3501.131632	731770.500154	44.253402
3501.086174	731758.475023	44.258407
3501.109861	731751.588246	44.263412
3501.040370	731750.213279	44.268417
3501.033662	731731.001696	44.273421
3501.006838	731711.941945	44.278426
3500.614438	731707.055071	44.283431
3500.549123	731700.331509	44.288436
3501.008857	731700.007983	44.293441
3500.494659	731703.559217	44.298445
3500.909127	731690.616185	44.303450
3501.013319	731671.980348	44.308455
3500.673795	731658.072470	44.313460
3500.970014	731648.516123	44.318465
3500.678135	731657.972783	44.323469
3500.763706	731646.024868	44.328474
3500.708840	731644.994092	44.333479
3500.407211	731630.089546	44.338484
3501.021243	731605.674732	44.343489
3500.560684	731619.269318	44.348493
3500.807282	731604.670274	44.353498
3500.724566	731609.635791	44.358503
3500.667889	731611.675433	44.363508
3500.896878	731603.863277	44.368513
3500.280168	731613.373668	44.373517
3500.955080	731603.358543	44.378522
3500.309438	731582.023874	44.383527
3500.570352	731564.649367	44.388532
3500.998960	731566.806901	44.393537
3500.684725	731572.305882	44.398541
3500.784617	731563.772246	44.403546
3500.489475	731565.455159	44.408551
3500.420014	731565.664744	44.413556
3500.572503	731556.033003	44.418561
3500.786257	731555.651084	44.423565
3500.544281	731564.505385	44.428570
3500.717322	731560.911497	44.433575
3500.522803	731554.605313	44.438580
3501.000565	731523.379220	44.443585
3500.363073	731523.286524	44.448589
3500.665210	731516.502088	44.453594
3500.648294	731520.912080	44.458599
3500.871334	731518.201247	44.463604
3500.796230	731509.349841	44.468609
3500.799718	731514.152614	44.473613
3500.654091	731511.057032	44.478618
3500.515519	731492.708494	44.483623
3500.465332	731494.697574	44.488628
3500.940175	731483.873545	44.493633
3500.897615	731488.981056	44.498637
3500.776215	731486.030018	44.503642
3500.552183	731486.611780	44.508647
3500.463361	731492.024047	44.513652
3500.600347	731480.116911	44.518657
3500.648349	731479.762379	44.523661
3500.576115	731480.913284	44.528666
3500.310424	731487.543236	44.533671
3500.611338	731492.395910	44.538676
3500.677986	731480.747992	44.543681
3500.570060	731448.578499	44.548685
3500.759160	731431.413652	44.553690
3500.846800	731442.095346	44.558695
3500.800828	731443.241917	44.563700
3500.886719	731431.788825	44.568705
3500.451506	731442.854036	44.573709
3500.713043	731436.274320	44.578714
3500.600654	731427.825139	44.583719
3500.537877	731402.580694	44.588724
3500.895517	731397.470647	44.593729
3500.721501	731395.320581	44.598733
3500.493193	731384.117421	44.603738
3500.540768	731386.040853	44.608743
3500.181774	731395.112754	44.613748
3500.442544	731391.652852	44.618753
3500.390120	731397.356284	44.623757
3500.716454	731389.131681	44.628762
3500.562112	731391.088478	44.633767
3500.628439	731393.949679	44.638772
3500.470553	731384.319505	44.643777
3500.395442	731399.286828	44.648781
3500.814567	731390.700256	44.653786
3500.784405	731393.329805	44.658791
3500.808903	731384.560842	44.663796
3500.732475	731362.388735	44.668801
3500.747543	731356.493439	44.673805
3500.833487	731349.199874	44.678810
3500.507582	731355.097088	44.683815
3500.642237	731345.418525	44.688820
3500.930597	731344.182432	44.693825
3500.585729	731345.873607	44.698829
3500.568389	731345.381308	44.703834
3500.696113	731328.919662	44.708839
3500.623323	731317.542151	44.713844
3500.649892	731310.852603	44.718849
3500.418330	731317.625613	44.723853
3500.539983	731313.297309	44.728858
3500.647936	731310.159746	44.733863
3500.473309	731315.784389	44.738868
3500.561007	731317.899287	44.743873
3500.455987	731319.154672	44.748877
3500.397671	731304.110277	44.753882
3500.408295	731312.774549	44.758887
3500.392431	731306.785288	44.763892
3500.461918	731307.467118	44.768897
3500.533316	731322.212292	44.773901
3500.572089	731311.707695	44.778906
3500.365098	731314.515050	44.783911
3500.195791	731313.057463	44.788916
3500.893544	731313.437392	44.793921
3500.546749	731312.504334	44.798925
3500.684577	731305.845915	44.803930
3500.530954	731306.713174	44.808935
3500.707099	731303.960500	44.813940
3500.667339	731276.780579	44.818945
3500.580026	731267.188123	44.823949
3500.843707	731257.686215	44.828954
3500.572547	731275.211697	44.833959
3500.644502	731260.739936	44.838964
3500.769294	731265.027609	44.843969
3500.730789	731271.818274	44.848973
3500.408356	731277.021688	44.853978
3500.438019	731277.710101	44.858983
3500.799398	731272.153677	44.863988
3501.016453	731262.857560	44.868993
3500.844802	731239.512368	44.873997
3500.914902	731222.960989	44.879002
3500.739005	731231.160966	44.884007
3500.746945	731224.325863	44.889012
3501.039237	731223.980472	44.894017
3500.878403	731208.705238	44.899021
3501.008038	731192.936290	44.904026
3500.975752	731189.326648	44.909031
3500.444810	731188.572567	44.914036
3500.536360	731188.111785	44.919041
3500.358024	731182.396884	44.924045
3500.717896	731176.840644	44.929050
3500.792636	731185.543978	44.934055
3500.590673	731176.168443	44.939060
3500.650343	731154.220881	44.944065
3500.446481	731145.439875	44.949069
3500.865337	731138.239670	44.954074
3500.839141	731140.076309	44.959079
3500.500420	731136.368719	44.964084
3500.958223	731131.142912	44.969089
3500.639205	731133.126984	44.974093
3500.674369	731137.875225	44.979098
3500.915588	731135.012698	44.984103
3500.446155	731123.898545	44.989108
3501.220474	731103.169818	44.994113
3500.774977	731102.748258	44.999117
3500.861394	731102.238798	45.004122
3501.064697	731097.797844	45.009127
3501.008107	731088.942919	45.014132
3501.249998	731068.104002	45.019137
3500.986861	731067.602783	45.024141
3500.844986	731059.801870	45.029146
3501.014697	731027.337218	45.034151
3500.715526	731018.819433	45.039156
3501.084795	731010.438788	45.044161
3500.535646	731010.529568	45.049165
3500.840383	731015.134290	45.054170
3500.725652	731015.450413	45.059175
3500.526666	731013.304371	45.064180
3500.954891	730982.777692	45.069185
3500.583251	730981.006826	45.074189
3500.715623	730975.438522	45.079194
3501.013798	730962.265940	45.084199
3500.833486	730965.415660	45.089204
3500.723546	730968.256618	45.094209
3500.587074	730968.576335	45.099213
3500.834129	730949.370488	45.104218
3500.572215	730929.406824	45.109223
3500.708511	730935.178439	45.114228
3500.713683	730929.928258	45.119233
3500.844818	730926.885761	45.124237
3501.246897	730924.887980	45.129242
3500.965275	730914.237725	45.134247
3500.657891	730892.399633	45.139252
3500.991487	730869.910811	45.144257
3500.999702	730892.987007	45.149261
3501.101033	730868.902322	45.154266
3501.274850	730874.568734	45.159271
3501.072589	730849.989412	45.164276
3501.273243	730824.452021	45.169281
3501.103324	730830.769542	45.174285
3500.747530	730805.967843	45.179290
3500.968924	730804.445600	45.184295
3500.764269	730797.843361	45.189300
3500.834231	730799.763233	45.194305
3500.907283	730802.871147	45.199309
3500.919455	730787.665576	45.204314
3501.208203	730762.361048	45.209319
3500.758943	730757.532513	45.214324
3500.710817	730754.767192	45.219329
3500.909041	730752.803057	45.224333
3500.798352	730755.148980	45.229338
3500.858781	730723.245928	45.234343
3500.484604	730717.166872	45.239348
3500.644821	730708.869987	45.244353
3500.628644	730720.312644	45.249357
3500.712126	730705.986560	45.254362
3500.893200	730714.029021	45.259367
3500.526258	730715.575399	45.264372
3500.420635	730706.331970	45.269377
3500.388437	730709.110648	45.274381
3500.555534	730711.262107	45.279386
3500.367713	730719.266476	45.284391
3500.424951	730710.788516	45.289396
3500.685258	730711.290293	45.294401
3500.460876	730719.251180	45.299405
3500.753973	730699.096186	45.304410
3500.840756	730679.767616	45.309415
3500.613191	730670.049058	45.314420
3500.976326	730672.267180	45.319425
3501.094482	730677.150548	45.324429
3500.841451	730671.447629	45.329434
3501.064673	730655.414552	45.334439
3501.221914	730639.887588	45.339444
3501.214675	730641.374539	45.344449
3501.078334	730628.124648	45.349453
3500.665882	730611.552717	45.354458
3500.482451	730598.558181	45.359463
3500.602214	730588.286886	45.364468
3500.882823	730583.139537	45.369473
3500.607275	730581.550799	45.374477
3500.689565	730592.184974	45.379482
3500.605993	730593.882645	45.384487
3500.689017	730589.708913	45.389492
3500.608618	730584.967893	45.394497
3500.346400	730598.729501	45.399501
3500.117047	730598.569337	45.404506
3500.790792	730595.536099	45.409511
3500.607278	730594.080728	45.414516
3500.788023	730564.138142	45.419521
3500.652317	730553.512824	45.424525
3500.491289	730551.905156	45.429530
3500.831189	730540.408832	45.434535
3500.670722	730542.515418	45.439540
3500.964038	730541.922209	45.444545
3500.659377	730536.178202	45.449549
3500.721126	730542.061466	45.454554
3500.835461	730507.078128	45.459559
3501.049623	730504.120804	45.464564
3500.828723	730495.391432	45.469569
3500.847201	730499.003731	45.474573
3500.611330	730499.587516	45.479578
3500.859448	730494.098806	45.484583
3500.897764	730484.286563	45.489588
3501.178915	730457.447067	45.494593
3501.111223	730457.260185	45.499597
3500.812449	730458.250569	45.504602
3500.932948	730448.820904	45.509607
3500.875948	730426.890656	45.514612
3501.059387	730405.911126	45.519617
3500.835612	730413.277905	45.524621
3500.989205	730399.038746	45.529626
3500.783522	730399.865176	45.534631
3500.553663	730389.057099	45.539636
3500.826708	730368.954126	45.544641
3500.542942	730370.684925	45.549645
3500.757679	730353.810720	45.554650
3501.244976	730354.770268	45.559655
3500.966196	730372.100852	45.564660
3501.183062	730340.913333	45.569665
3501.128398	730326.857039	45.574669
3500.976931	730308.805107	45.579674
3501.291289	730309.595136	45.584679
3500.972361	730304.596212	45.589684
3501.248925	730270.030781	45.594689
3500.841662	730277.229899	45.599693
3500.661245	730281.519004	45.604698
3500.899313	730274.298388	45.609703
3500.808723	730245.538572	45.614708
3500.941320	730225.607034	45.619713
3500.760071	730231.481153	45.624717
3501.099104	730228.800253	45.629722
3500.844636	730233.101620	45.634727
3500.478731	730214.490596	45.639732
3500.912927	730186.981070	45.644737
3500.835884	730193.135157	45.649741
3500.843283	730190.707155	45.654746
3500.897001	730192.778436	45.659751
3500.919687	730192.626140	45.664756
3500.939730	730179.844942	45.669761
3500.723464	730157.246909	45.674765
3500.655446	730148.095683	45.679770
3500.803529	730136.333327	45.684775
3500.753384	730145.107942	45.689780
3501.014507	730140.458806	45.694785
3500.963486	730141.754974	45.699789
3500.713247	730119.756776	45.704794
3501.151171	730111.710555	45.709799
3500.733570	730114.355015	45.714804
3500.920869	730107.093114	45.719809
3500.969330	730113.870376	45.724813
3500.902789	730081.936262	45.729818
3501.034763	730072.405210	45.734823
3500.801290	730049.463027	45.739828
3500.807492	729977.101818	45.744833
3500.614789	729865.645201	45.749837
3500.155130	729688.406269	45.754842
3500.312766	729469.108663	45.759847
3499.968979	729185.445956	45.764852
3499.862543	728852.298436	45.769857
3499.668416	728455.694711	45.774861
3500.091170	728005.912535	45.779866
3499.610507	727495.911559	45.784871
3498.905582	726935.675796	45.789876
3499.122901	726307.662918	45.794881
3498.877761	725626.704864	45.799885
3498.082078	724885.716175	45.804890
3497.695382	724087.595114	45.809895
3497.244943	723239.640429	45.814900
3496.747771	722332.712485	45.819905
3496.147966	721375.527436	45.824909
3495.732268	720348.434281	45.829914
3494.904855	719271.442123	45.834919
3494.471337	718142.563676	45.839924
3493.801118	716946.455059	45.844929
3493.234243	715694.542179	45.849933
3492.556418	714385.099381	45.854938
3491.696903	713016.722613	45.859943
3490.708972	711591.857133	45.864948
3490.334597	710112.586844	45.869953
3489.529227	708578.113619	45.874957
3488.586584	706975.795162	45.879962
3487.945662	705317.096245	45.884967
3486.984555	703598.362223	45.889972
3485.953781	701831.642795	45.894977
3484.909726	699988.569546	45.899981
3483.942412	698090.558169	45.904986
3483.147029	696147.604059	45.909991
3481.856874	694146.062405	45.914996
3481.078896	692083.888756	45.920001
3479.457680	689980.873401	45.925005
3478.039379	687806.854312	45.930010
3477.188764	685586.217049	45.935015
3475.968384	683316.197352	45.940020
3474.800017	680989.270380	45.945025
3473.510319	678600.741856	45.950029
3472.202347	676172.478683	45.955034
3470.690000	673684.245971	45.960039
3468.761104	671146.855558	45.965044
3467.756581	668545.586718	45.970049
3466.489103	665914.763009	45.975053
3465.125725	663215.462553	45.980058
3463.508980	660468.525184	45.985063
3461.628400	657669.623885	45.990068
3460.084671	654820.718745	45.995073
3458.488788	651920.538321	46.000077
3457.249440	648981.571109	46.005082
3455.411034	645970.854051	46.010087
3453.566765	642937.188649	46.015092
3452.088957	639828.178659	46.020097
3450.529547	636694.925570	46.025101
3448.401718	633499.006802	46.030106
3446.849061	630254.053594	46.035111
3445.069557	626965.071069	46.040116
3443.017387	623630.783523	46.045121
3441.124170	620255.247290	46.050125
3439.380889	616824.249527	46.055130
3437.473088	613349.836348	46.060135
3435.084214	609829.673340	46.065140
3433.418499	606254.498534	46.070145
3431.647268	602645.590962	46.075149
3429.282787	598982.376574	46.080154
3427.500369	595277.631226	46.085159
3425.070555	591528.166707	46.090164
3423.105628	587731.559830	46.095169
3421.030321	583893.003774	46.100173
3418.458925	580018.421700	46.105178
3416.644475	576089.931496	46.110183
3414.120218	572119.214169	46.115188
3412.005928	568115.927480	46.120193
3409.520287	564069.009417	46.125197
3407.112573	559975.894724	46.130202
3404.660309	555842.322639	46.135207
3402.440831	551680.223508	46.140212
3399.872329	547475.923619	46.145217
3397.683251	543224.341593	46.150221
3395.305937	538941.539490	46.155226
3392.457502	534614.790389	46.160231
3389.749455	530256.846071	46.165236
3387.605742	525850.060185	46.170241
3385.248132	521423.126182	46.175245
3382.235207	516945.457193	46.180250
3379.830473	512431.933190	46.185255
3376.980131	507883.985348	46.190260
3374.672524	503289.057724	46.195265
3371.876180	498671.684272	46.200269
3369.137464	494020.499936	46.205274
3366.459216	489322.244339	46.210279
3363.365543	484599.003301	46.215284
3360.964718	479834.398913	46.220289
3357.719900	475052.888317	46.225293
3354.473192	470239.555407	46.230298
3351.902059	465379.699651	46.235303
3349.038764	460504.847695	46.240308
3346.078713	455596.026080	46.245313
3343.176505	450648.042725	46.250317
3340.006273	445683.726936	46.255322
3337.091618	440683.582360	46.260327
3333.717183	435671.379866	46.265332
3330.956856	430611.033290	46.270337
3327.729388	425535.820152	46.275341
3324.560125	420437.197941	46.280346
3321.674645	415305.042338	46.285351
3318.249922	410157.179299	46.290356
3315.210553	404978.113023	46.295361
3312.285691	399773.139041	46.300365
3308.896956	394545.423249	46.305370
3305.409712	389295.335368	46.310375
3301.797375	384023.311035	46.315380
3298.867513	378736.462513	46.320385
3295.420329	373421.083751	46.325389
3292.153928	368095.724351	46.330394
3288.583246	362728.729853	46.335399
3285.042249	357368.881145	46.340404
3281.664373	351984.802725	46.345409
3277.946070	346590.830507	46.350413
3274.815372	341172.315901	46.355418
3271.331275	335736.571347	46.360423
3267.675379	330286.476957	46.365428
3263.958990	324810.366180	46.370433
3260.290754	319335.874839	46.375437
3256.898353	313846.865113	46.380442
3253.414552	308348.730724	46.385447
3249.552598	302838.680681	46.390452
3245.736688	297310.852388	46.395457
3241.933944	291784.159123	46.400461
3238.300151	286253.778090	46.405466
3234.559658	280699.957203	46.410471
3230.707135	275157.780054	46.415476
3226.815752	269587.776368	46.420481
3222.985423	264042.765855	46.425485
3219.323978	258466.004410	46.430490
3215.449636	252881.741049	46.435495
3211.445508	247315.268813	46.440500
3207.493740	241732.014412	46.445505
3203.529725	236151.030205	46.450509
3199.425730	230570.316907	46.455514
3195.457027	224985.491541	46.460519
3191.468176	219414.421920	46.465524
3187.371960	213831.777107	46.470529
3183.540375	208188.949094	46.475533
3179.091151	202597.215001	46.480538
3175.346165	197023.001784	46.485543
3170.987721	191466.629265	46.490548
3166.340324	185902.056767	46.495553
3162.254995	180361.355988	46.500557
3158.166372	174822.376588	46.505562
3153.879131	169293.015984	46.510567
3149.394850	163769.941369	46.515572
3145.077451	158256.731089	46.520577
3140.930770	152774.506218	46.525581
3136.485006	147297.090771	46.530586
3132.255980	141813.733789	46.535591
3127.831773	136348.354373	46.540596
3123.330479	130928.326739	46.545601
3118.727751	125497.814033	46.550605
3114.086763	120098.025493	46.555610
3109.592639	114713.507711	46.560615
3104.845349	109338.121886	46.565620
3100.331094	104003.652141	46.570625
3095.416953	98675.428176	46.575629
3090.598520	93398.571332	46.580634
3086.000325	88115.724786	46.585639
3080.978099	82897.385984	46.590644
3075.944704	77673.481726	46.595649
3070.997750	72507.651554	46.600653
3065.629960	67361.993195	46.605658
3060.601686	62251.837853	46.610663
3055.303407	57196.180029	46.615668
3050.302658	52169.456406	46.620673
3044.696113	47185.672116	46.625677
3039.185972	42254.287638	46.630682
3033.154329	37360.632998	46.635687
3026.992008	32542.318564	46.640692
3020.065962	27781.307936	46.645697
3012.343694	23130.417923	46.650701
2996.993532	18757.880579	46.655706
2979.744211	14606.157420	46.660711
2958.058520	10770.461598	46.665716
2929.456594	7434.377755	46.670721
2898.204919	4574.268482	46.675725
2868.750026	2160.017456	46.680730
2832.468480	496.681723	46.685735
2766.569010	275.620966	46.690740
2726.294672	268.936031	46.695745
2719.223515	265.154740	46.700749
2733.459146	268.973876	46.705754
2755.628612	261.682396	46.710759
2775.197557	266.328043	46.715764
2788.189980	250.279313	46.720769
2793.420516	259.034247	46.725773
2792.586135	260.898299	46.730778
2788.482276	248.960572	46.735783
2783.506647	251.918154	46.740788
2779.298834	251.856472	46.745793
2775.821035	250.796205	46.750797
2773.061683	255.508353	46.755802
2770.714807	251.579080	46.760807
2767.585173	249.877862	46.765812
2765.675263	250.624612	46.770817
2763.077113	247.487411	46.775821
2759.562911	249.698928	46.780826
2756.909023	242.912315	46.785831
2753.440655	251.276347	46.790836
2750.648894	249.281227	46.795841
2747.361114	243.767191	46.800845
2744.205125	245.966985	46.805850
2741.304575	244.720423	46.810855
2738.160067	241.180134	46.815860
2734.657496	240.159918	46.820865
2731.441141	235.719828	46.825869
2727.798553	240.553727	46.830874
2725.052864	240.690140	46.835879
2721.702033	238.716936	46.840884
2718.554709	234.511115	46.845889
2715.386346	233.669439	46.850893
2711.725381	237.413142	46.855898
2708.398895	240.301081	46.860903
2704.946996	236.964441	46.865908
2701.674378	238.274633	46.870913
2698.413846	224.518081	46.875917
2694.733198	232.908603	46.880922
2691.876032	230.819171	46.885927
2688.462928	230.956566	46.890932
2684.563119	221.841853	46.895937
2681.642002	229.740986	46.900941
2677.778382	228.527796	46.905946
2674.726220	230.012271	46.910951
2671.548946	229.292282	46.915956
2668.206101	232.530666	46.920961
2664.840237	223.850131	46.925965
2660.888224	232.869917	46.930970
2657.443735	228.371353	46.935975
2654.007820	230.815282	46.940980
2650.329855	227.707137	46.945985
2646.936292	227.876456	46.950989
2643.275943	236.424291	46.955994
2640.631646	230.623455	46.960999
2637.054276	224.715423	46.966004
2633.429510	229.028631	46.971009
2629.947750	220.959920	46.976013
2626.604905	218.839246	46.981018
2623.660301	218.995630	46.986023
2620.254177	226.215344	46.991028
2616.268769	216.979895	46.996033
2613.051878	223.944505	47.001037
2609.611447	219.643637	47.006042
2606.126300	226.280288	47.011047
2602.244520	219.717008	47.016052
2598.736756	226.749716	47.021057
2596.254886	216.539363	47.026061
2591.891132	220.690782	47.031066
2588.785094	217.604830	47.036071
2585.464332	219.075029	47.041076
2581.978279	213.435309	47.046081
2578.295953	223.684517	47.051085
2574.729572	219.195157	47.056090
2571.043969	216.089731	47.061095
2567.848500	222.282985	47.066100
2564.255162	218.633229	47.071105
2561.392011	217.203985	47.076109
2557.670688	224.833307	47.081114
2554.098316	213.667072	47.086119
2550.464899	219.591455	47.091124
2546.918536	218.834396	47.096129
2544.058913	207.607196	47.101133
2539.871927	216.215655	47.106138
2536.712537	212.972420	47.111143
2533.107732	214.492451	47.116148
2529.513512	218.206106	47.121153
2525.631632	206.268649	47.126157
2522.816497	214.789497	47.131162
2519.669512	202.655381	47.136167
2515.682513	206.111632	47.141172
2512.415548	208.215901	47.146177
2508.695906	208.783280	47.151181
2505.302710	212.923661	47.156186
2502.269405	206.505937	47.161191
2498.136262	209.300262	47.166196
2495.323028	210.631633	47.171201
2491.519361	204.806204	47.176205
2487.720067	212.576558	47.181210
2484.545280	206.774285	47.186215
2480.844506	212.519444	47.191220
2477.435842	205.913078	47.196225
2473.749109	206.655404	47.201229
2470.742735	204.054080	47.206234
2467.341169	195.912063	47.211239
2463.469667	196.985931	47.216244
2460.065309	200.595580	47.221249
2457.038498	190.548198	47.226253
2452.805058	198.558792	47.231258
2449.472953	196.925487	47.236263
2446.037301	199.970026	47.241268
2442.364037	191.878550	47.246273
2439.195597	191.340009	47.251277
2435.901189	194.993630	47.256282
2432.474655	196.488958	47.261287
2428.680982	189.998101	47.266292
2425.206185	199.070465	47.271297
2422.092175	203.765761	47.276301
2418.069167	203.148129	47.281306
2414.754202	198.078555	47.286311
2411.186559	194.084083	47.291316
2407.466642	202.084668	47.296321
2404.177382	197.089979	47.301325
2400.549762	202.280212	47.306330
2397.270121	195.145400	47.311335
2393.806927	195.446631	47.316340
2390.497346	200.300433	47.321345
2387.087068	191.569897	47.326349
2383.153660	194.323358	47.331354
2380.046209	187.718510	47.336359
2376.039530	190.823135	47.341364
2372.823973	196.315943	47.346369
2369.608583	188.340718	47.351373
2365.884303	202.027318	47.356378
2362.473979	186.775241	47.361383
2358.997063	189.851348	47.366388
2355.365108	190.897679	47.371393
2351.975791	192.575956	47.376397
2348.016143	189.807195	47.381402
2344.902664	190.236439	47.386407
2341.454834	189.714447	47.391412
2337.901118	194.274629	47.396417
2334.484020	188.328305	47.401421
2330.834674	197.577648	47.406426
2327.285741	192.085527	47.411431
2323.718762	191.690042	47.416436
2320.179913	196.707767	47.421441
2316.877876	192.843242	47.426445
2313.316743	189.833277	47.431450
2310.012916	187.613063	47.436455
2306.304497	186.348271	47.441460
2302.925954	183.808125	47.446465
2299.952393	183.841656	47.451469
2296.257401	192.844415	47.456474
2292.657680	181.257925	47.461479
2288.964687	191.978759	47.466484
2285.268952	188.538819	47.471489
2282.127189	179.677477	47.476493
2278.350075	192.187488	47.481498
2274.912556	179.291663	47.486503
2271.544425	182.227076	47.491508
2268.055941	181.855737	47.496513
2264.288008	171.150820	47.501517
2260.763124	188.505296	47.506522
2257.520001	181.197024	47.511527
2253.866617	185.300765	47.516532
2250.365572	185.417955	47.521537
2246.956095	180.129946	47.526541
2243.431391	197.264778	47.531546
2240.224798	183.040154	47.536551
2236.538332	186.018458	47.541556
2232.896672	188.336359	47.546561
2229.336513	185.127788	47.551565
2225.721377	188.614858	47.556570
2222.631268	190.778455	47.561575
2219.223770	178.218512	47.566580
2215.309337	183.908298	47.571585
2211.756235	182.032763	47.576589
2208.605750	182.890930	47.581594
2205.066710	181.412677	47.586599
2201.503985	184.844118	47.591604
2197.677469	191.879990	47.596609
2194.537000	181.782394	47.601613
2191.036785	185.940342	47.606618
2187.794805	192.588519	47.611623
2184.297786	181.698689	47.616628
2180.617235	189.359037	47.621633
2177.216953	184.185204	47.626637
2173.000198	186.426149	47.631642
2169.467438	191.307809	47.636647
2166.214405	183.942647	47.641652
2162.602171	183.349963	47.646657
2159.978094	181.021212	47.651661
2156.600666	184.167036	47.656666
2152.722770	164.884314	47.661671
2148.950271	184.890234	47.666676
2145.310896	177.593043	47.671681
2141.751096	178.966626	47.676685
2138.551241	184.684128	47.681690
2135.038531	167.717240	47.686695
2131.679769	181.698647	47.691700
2128.085596	187.236195	47.696705
2124.814467	176.060558	47.701709
2121.025448	184.809468	47.706714
2116.905453	181.941600	47.711719
2114.039964	176.674686	47.716724
2110.739715	176.958627	47.721729
2107.425169	177.790770	47.726733
2103.370964	172.352182	47.731738
2099.661193	168.838770	47.736743
2096.258063	180.007429	47.741748
2093.060255	177.498690	47.746753
2089.847465	170.216919	47.751757
2085.840832	174.406951	47.756762
2082.859063	178.507306	47.761767
2079.275505	178.377038	47.766772
2075.575502	177.557040	47.771777
2072.049686	170.078109	47.776781
2068.179147	176.901152	47.781786
2064.915316	168.033586	47.786791
2061.142331	178.774551	47.791796
2058.005801	169.919051	47.796801
2054.980500	171.658810	47.801805
2050.841384	176.621686	47.806810
2047.602786	170.514820	47.811815
2043.809647	156.875401	47.816820
2040.428573	174.204206	47.821825
2037.230531	164.098143	47.826829
2033.447469	170.327738	47.831834
2030.427736	168.903701	47.836839
2026.807946	162.682416	47.841844
2022.920709	169.131943	47.846849
2019.749368	167.390659	47.851853
2016.149782	175.279848	47.856858
2012.191354	175.654376	47.861863
2008.670515	165.641686	47.866868
2004.963897	164.702869	47.871873
2001.903661	166.397541	47.876877
1998.506235	167.945820	47.881882
1995.228230	164.548432	47.886887
1991.785740	161.504498	47.891892
1987.914710	172.480411	47.896897
1984.787466	161.927935	47.901901
1980.942347	166.323760	47.906906
1977.108609	174.754984	47.911911
1974.590452	162.390890	47.916916
1970.156113	167.942669	47.921921
1967.078779	160.665992	47.926925
1963.248474	158.890486	47.931930
1959.557386	168.348301	47.936935
1956.361839	166.328888	47.941940
1952.586509	162.529096	47.946945
1949.834757	165.348804	47.951949
1946.029605	169.832561	47.956954
1942.634989	166.701012	47.961959
1939.035124	166.298287	47.966964
1935.670955	169.842280	47.971969
1932.466558	159.423999	47.976973
1928.466809	168.168711	47.981978
1924.925233	157.323830	47.986983
1921.489220	160.043827	47.991988
1917.748045	165.532492	47.996993
1914.590829	154.654514	48.001997
1910.650802	166.615374	48.007002
1907.515091	159.993903	48.012007
1903.996013	161.888810	48.017012
1900.230985	159.607236	48.022017
1897.140914	156.282980	48.027021
1893.609835	157.311809	48.032026
1889.867589	160.955395	48.037031
1886.512771	165.273205	48.042036
1882.974161	162.621613	48.047041
1879.561301	154.441570	48.052045
1876.084352	163.031799	48.057050
1872.521618	164.543048	48.062055
1868.909719	165.748685	48.067060
1865.530178	171.747168	48.072065
1862.032234	161.273406	48.077069
1858.229963	160.217770	48.082074
1854.984430	166.041313	48.087079
1851.330899	153.173041	48.092084
1847.960930	162.174566	48.097089
1844.671873	159.002915	48.102093
1840.906796	161.438101	48.107098
1837.326864	162.885531	48.112103
1833.942489	152.952226	48.117108
1830.058676	153.924328	48.122113
1827.152334	160.384907	48.127117
1823.033826	170.351165	48.132122
1819.862595	168.009334	48.137127
1816.701287	159.342663	48.142132
1812.731407	165.413376	48.147137
1809.374039	154.832503	48.152141
1805.621574	163.852070	48.157146
1802.208175	167.115627	48.162151
1798.943837	161.681815	48.167156
1795.452088	156.745688	48.172161
1792.336478	158.227690	48.177165
1788.509474	162.485312	48.182170
1784.801254	157.624542	48.187175
1781.377420	157.226919	48.192180
1777.889421	169.001670	48.197185
1774.688941	150.806322	48.202189
1770.909740	161.731272	48.207194
1767.264536	151.226764	48.212199
1763.697453	160.267338	48.217204
1760.533130	166.277981	48.222209
1757.169847	155.492317	48.227213
1753.356452	157.136385	48.232218
1749.658834	158.617606	48.237223
1746.457456	154.345574	48.242228
1742.360453	162.866018	48.247233
1739.226674	158.653825	48.252237
1735.618887	168.888535	48.257242
1732.644134	155.141223	48.262247
1729.359526	150.618574	48.267252
1725.511193	155.048508	48.272257
1721.937950	157.064041	48.277261
1718.314234	160.294053	48.282266
1714.719068	155.582543	48.287271
1711.553999	152.942397	48.292276
1707.846349	154.163259	48.297281
1704.128667	154.708140	48.302285
1700.763001	148.724274	48.307290
1696.976152	157.140654	48.312295
1693.933792	149.084073	48.317300
1690.208386	153.026766	48.322305
1686.780901	151.892588	48.327309
1682.747685	149.866040	48.332314
1679.853030	151.357871	48.337319
1676.568319	155.858200	48.342324
1673.049489	155.627970	48.347329
1669.979751	150.000003	48.352333
1665.796714	153.938072	48.357338
1662.299278	149.236065	48.362343
1658.440468	148.793047	48.367348
1655.031703	149.444430	48.372353
1651.953681	155.143457	48.377357
1648.446194	152.306359	48.382362
1644.493158	156.566651	48.387367
1641.369958	148.285137	48.392372
1637.569708	145.797915	48.397377
1634.434082	145.252983	48.402381
1630.859865	155.141207	48.407386
1627.374093	155.697439	48.412391
1624.043219	153.000789	48.417396
1620.167044	158.691862	48.422401
1616.873096	152.988431	48.427405
1612.960824	155.070726	48.432410
1609.584329	159.904428	48.437415
1606.059045	147.444554	48.442420
1602.634993	158.430539	48.447425
1599.627525	144.248724	48.452429
1595.968396	149.709456	48.457434
1592.084260	141.651436	48.462439
1588.714630	135.873561	48.467444
1585.008962	143.113088	48.472449
1581.893170	144.656650	48.477453
1578.129926	153.934722	48.482458
1574.639873	145.944974	48.487463
1571.695514	143.433716	48.492468
1568.113184	146.411905	48.497473
1564.410324	147.143503	48.502477
1560.869505	147.011542	48.507482
1557.205688	145.156729	48.512487
1553.507719	138.495397	48.517492
1549.723472	146.532190	48.522497
1546.547035	136.579491	48.527501
1542.971233	144.753209	48.532506
1539.838205	142.854407	48.537511
1536.209421	136.215564	48.542516
1532.539663	147.024083	48.547521
1529.208070	147.600617	48.552525
1525.508272	152.313943	48.557530
1522.125213	142.222264	48.562535
1518.782461	138.834838	48.567540
1515.353298	148.415330	48.572545
1511.692990	147.642749	48.577549
1507.886760	144.052365	48.582554
1504.526044	150.986716	48.587559
1501.249119	146.448390	48.592564
1497.443867	144.368051	48.597569
1494.174319	146.631396	48.602573
1490.566800	144.660750	48.607578
1486.938079	138.153960	48.612583
1483.831435	137.994470	48.617588
1480.101275	139.201709	48.622593
1476.931415	137.492981	48.627597
1473.486268	144.668288	48.632602
1469.875253	136.799936	48.637607
1466.252502	138.619463	48.642612
1462.384829	145.602195	48.647617
1459.147214	140.033424	48.652621
1455.489028	139.077813	48.657626
1452.137363	138.936682	48.662631
1448.978513	136.099376	48.667636
1445.012287	141.421525	48.672641
1441.467402	136.468496	48.677645
1437.774621	150.351226	48.682650
1434.733101	144.993662	48.687655
1431.187906	142.188670	48.692660
1427.624878	138.116403	48.697665
1424.033335	145.265115	48.702669
1420.408954	143.644835	48.707674
1416.830312	149.804353	48.712679
1413.595251	142.102612	48.717684
1409.831069	151.560160	48.722689
1406.458507	145.456148	48.727693
1403.064754	148.314801	48.732698
1399.779487	148.543950	48.737703
1395.844768	144.132373	48.742708
1392.356706	149.458941	48.747713
1389.176628	144.284037	48.752717
1385.473147	150.604590	48.757722
1382.179179	147.542488	48.762727
1378.778511	140.510369	48.767732
1375.378224	146.268168	48.772737
1371.890015	143.177908	48.777741
1367.914240	134.689355	48.782746
1364.472638	140.563928	48.787751
1361.005264	142.572280	48.792756
1357.341508	148.204086	48.797761
1354.028728	141.951483	48.802765
1350.546959	139.225439	48.807770
1346.840405	141.530401	48.812775
1343.547797	147.380874	48.817780
1339.800745	136.743340	48.822785
1336.658382	140.082494	48.827789
1332.772914	145.726625	48.832794
1329.368707	147.662763	48.837799
1326.048578	148.352807	48.842804
1322.713946	152.782757	48.847809
1319.071361	148.753187	48.852813
1315.717487	151.831442	48.857818
1311.822409	147.811793	48.862823
1308.659309	148.917438	48.867828
1305.091573	151.520870	48.872833
1301.808708	142.332358	48.877837
1298.098707	146.257650	48.882842
1294.241269	147.038622	48.887847
1291.070553	142.237184	48.892852
1287.257118	144.330037	48.897857
1283.857259	138.348478	48.902861
1280.109512	143.536271	48.907866
1276.770027	148.831579	48.912871
1273.658749	139.872941	48.917876
1269.985453	147.741008	48.922881
1266.777077	144.726771	48.927885
1263.058784	149.066884	48.932890
1259.138712	148.430573	48.937895
1255.959199	148.188235	48.942900
1252.433784	151.754192	48.947905
1249.191429	139.156392	48.952909
1245.620878	138.356344	48.957914
1242.058128	141.674929	48.962919
1238.386820	147.763930	48.967924
1234.483157	151.777253	48.972929
1231.438502	156.206730	48.977933
1227.730439	147.697790	48.982938
1224.474284	149.065211	48.987943
1221.362898	139.576601	48.992948
1217.366042	143.001953	48.997953
1213.885329	139.452584	49.002957
1210.351962	144.608230	49.007962
1206.783734	141.316501	49.012967
1203.337514	136.267411	49.017972
1199.673701	145.472868	49.022977
1196.123775	136.144849	49.027981
1193.002670	135.554250	49.032986
1189.423635	141.457883	49.037991
1185.890962	141.966239	49.042996
1182.599918	146.439783	49.048001
1179.275400	142.608197	49.053005
1175.491725	137.075215	49.058010
1171.852221	131.204955	49.063015
1168.327115	135.720694	49.068020
1164.708739	145.447692	49.073025
1161.677108	145.057958	49.078029
1157.735948	134.003300	49.083034
1154.208816	144.425765	49.088039
1150.824405	135.141766	49.093044
1147.244188	138.831160	49.098049
1143.949815	133.700299	49.103053
1140.108433	138.378254	49.108058
1136.651570	134.408234	49.113063
1133.260965	128.437124	49.118068
1129.568857	132.448989	49.123073
1126.740188	134.759064	49.128077
1123.156075	133.530799	49.133082
1119.456454	134.152557	49.138087
1115.916125	132.969920	49.143092
1111.907316	141.906499	49.148097
1108.788160	139.017701	49.153101
1105.029892	135.663079	49.158106
1101.460819	135.760389	49.163111
1098.136506	134.903243	49.168116
1094.671497	140.352918	49.173121
1091.379934	137.114257	49.178125
1087.837505	144.465853	49.183130
1084.429012	134.752966	49.188135
1081.115806	138.267282	49.193140
1077.433952	137.873419	49.198145
1073.911861	139.238913	49.203149
1070.420874	138.213495	49.208154
1066.668679	137.337391	49.213159
1063.643603	142.739352	49.218164
1059.553837	139.528975	49.223169
1056.156185	129.635735	49.228173
1052.489095	142.338791	49.233178
1049.002829	140.424611	49.238183
1045.915163	140.475241	49.243188
1042.048119	138.320755	49.248193
1038.926923	136.551232	49.253197
1035.057675	138.772381	49.258202
1031.612334	132.034337	49.263207
1028.271631	129.767859	49.268212
1024.879518	145.625848	49.273217
1021.497872	145.401853	49.278221
1017.684029	148.036315	49.283226
1013.809169	160.594520	49.288231
1010.525682	132.654833	49.293236
1006.903502	137.331268	49.298241
1003.671860	140.965706	49.303245
1000.204787	140.650333	49.308250
997.042338	142.819742	49.313255
993.584730	147.780075	49.318260
989.594108	140.448602	49.323265
986.162321	137.318552	49.328269
982.430137	138.380173	49.333274
979.146420	135.594767	49.338279
975.894842	136.677079	49.343284
972.109017	136.552762	49.348289
968.497016	127.973503	49.353293
965.424918	127.445403	49.358298
961.748146	135.389291	49.363303
958.306390	130.223465	49.368308
954.377510	136.292510	49.373313
951.213878	128.996109	49.378317
947.672143	133.808625	49.383322
943.866832	138.466571	49.388327
941.125958	131.323989	49.393332
937.068471	137.929235	49.398337
933.837676	144.159302	49.403341
930.300791	136.542433	49.408346
926.461131	141.845848	49.413351
923.230312	130.604105	49.418356
919.548687	132.969853	49.423361
916.434855	133.301984	49.428365
912.464193	140.586863	49.433370
908.953824	136.277250	49.438375
905.553987	132.209973	49.443380
901.632129	142.910086	49.448385
898.485834	132.609229	49.453389
895.411888	124.720601	49.458394
891.795275	127.302121	49.463399
888.447656	126.255443	49.468404
884.538794	141.423188	49.473409
881.512601	128.588005	49.478413
877.598174	131.736178	49.483418
873.952205	137.823659	49.488423
870.459789	131.062407	49.493428
866.819679	146.299030	49.498433
863.666435	137.700164	49.503437
860.078546	144.741791	49.508442
856.466951	142.116488	49.513447
852.875240	127.435423	49.518452
849.466815	136.597597	49.523457
846.184354	129.931561	49.528461
842.640524	141.952278	49.533466
838.991277	138.082353	49.538471
835.763127	132.478233	49.543476
832.212307	131.843028	49.548481
828.454567	136.056883	49.553485
825.148764	137.305792	49.558490
821.519473	138.225182	49.563495
818.008926	128.951400	49.568500
814.198456	137.218740	49.573505
810.936198	128.526925	49.578509
807.463826	135.955528	49.583514
804.046848	130.090337	49.588519
800.501747	129.948924	49.593524
796.890176	135.896971	49.598529
793.521393	127.208650	49.603533
790.384196	128.533198	49.608538
786.504879	138.331450	49.613543
783.324694	123.399223	49.618548
779.668886	137.613768	49.623553
776.135144	135.119476	49.628557
772.290056	133.604729	49.633562
768.514369	133.642519	49.638567
765.332333	130.991580	49.643572
761.726506	130.306768	49.648577
758.284988	124.849833	49.653581
754.930621	130.073829	49.658586
751.271621	128.076124	49.663591
747.978587	122.461745	49.668596
744.539694	135.716002	49.673601
741.656530	135.976435	49.678605
737.699824	135.370418	49.683610
734.058716	134.376152	49.688615
730.463694	121.190568	49.693620
727.073534	132.113359	49.698625
723.408557	127.086443	49.703629
719.818178	134.441569	49.708634
715.941451	126.363938	49.713639
713.066128	120.752861	49.718644
709.156592	125.608295	49.723649
705.777560	123.667556	49.728653
702.444230	117.302354	49.733658
698.873118	124.318239	49.738663
695.390830	128.386043	49.743668
692.083748	130.773291	49.748673
688.641189	115.860258	49.753677
685.185915	126.726007	49.758682
681.346827	126.232538	49.763687
677.968073	124.534496	49.768692
674.402499	124.886180	49.773697
670.838393	127.771759	49.778701
667.305907	131.229879	49.783706
663.922346	130.505099	49.788711
660.364973	123.356431	49.793716
656.580449	129.916630	49.798721
653.228070	129.350664	49.803725
649.845340	132.590748	49.808730
646.486648	127.375317	49.813735
643.064719	120.223123	49.818740
639.186905	130.821633	49.823745
636.315007	127.566979	49.828749
632.045817	137.600207	49.833754
628.697865	131.851199	49.838759
625.504421	126.369382	49.843764
621.723679	136.205287	49.848769
618.331142	131.541518	49.853773
615.009115	130.630150	49.858778
611.174793	136.172735	49.863783
607.929761	124.166239	49.868788
604.003626	124.477616	49.873793
600.338571	130.899236	49.878797
597.389436	125.573616	49.883802
593.695129	126.899075	49.888807
590.524404	124.002706	49.893812
586.960381	126.348054	49.898817
583.434592	122.906028	49.903821
580.136322	131.205345	49.908826
576.049421	127.770860	49.913831
572.825605	121.286758	49.918836
568.999691	120.636310	49.923841
565.575795	128.407917	49.928845
562.169572	127.591878	49.933850
558.669651	134.868582	49.938855
555.546244	111.519062	49.943860
551.856091	114.956896	49.948865
548.544314	121.270164	49.953869
544.940841	120.045468	49.958874
541.344111	134.487584	49.963879
537.669393	122.363868	49.968884
533.905598	135.531150	49.973889
530.470223	125.425071	49.978893
527.093655	129.866775	49.983898
523.559557	127.593994	49.988903
520.472518	129.333314	49.993908
516.642184	137.948767	49.998913
513.296483	122.439281	50.003917
509.680331	120.905138	50.008922
505.876543	130.950788	50.013927
502.808697	119.451518	50.018932
499.446765	131.665871	50.023937
496.109622	131.382660	50.028941
492.867756	125.723908	50.033946
488.971312	127.438039	50.038951
485.179634	124.470845	50.043956
481.414108	120.726563	50.048961
478.159572	119.488773	50.053965
474.583913	127.162525	50.058970
470.835229	124.489728	50.063975
467.442802	112.506086	50.068980
464.081789	127.097362	50.073985
460.606541	128.658884	50.078989
457.272004	124.614928	50.083994
453.869108	123.461394	50.088999
450.289430	122.636380	50.094004
446.533344	120.470796	50.099009
443.236420	118.720307	50.104013
439.675896	127.121701	50.109018
436.109966	126.551342	50.114023
432.724599	120.751909	50.119028
429.124626	122.078632	50.124033
425.435676	125.740161	50.129037
422.112830	118.778531	50.134042
418.454216	122.127980	50.139047
415.273353	124.955661	50.144052
411.766395	129.046362	50.149057
408.202421	116.161842	50.154061
404.909748	127.484269	50.159066
401.053431	127.570353	50.164071
397.755841	130.558530	50.169076
393.885938	123.650893	50.174081
390.434357	127.177519	50.179085
387.020273	129.964440	50.184090
383.532878	125.763018	50.189095
380.442241	117.274979	50.194100
376.558384	115.157529	50.199105
373.262534	127.740664	50.204109
369.720252	117.109064	50.209114
365.922760	125.687030	50.214119
362.692704	112.599886	50.219124
358.607175	116.880671	50.224129
355.747758	113.838078	50.229133
352.590895	116.128635	50.234138
348.927097	121.280248	50.239143
345.327067	116.742184	50.244148
341.384221	120.646852	50.249153
337.797292	119.040931	50.254157
334.240061	113.158260	50.259162
330.829239	122.781220	50.264167
327.713256	110.668921	50.269172
323.685555	119.718703	50.274177
320.558642	118.932262	50.279181
317.178394	119.410572	50.284186
313.651856	120.423486	50.289191
310.335649	114.545394	50.294196
306.690435	118.492608	50.299201
303.035405	122.085472	50.304205
299.816255	115.227107	50.309210
295.731837	119.154552	50.314215
292.556523	118.967379	50.319220
288.714374	118.546453	50.324225
285.243329	116.602446	50.329229
281.889339	107.126019	50.334234
278.492459	118.950098	50.339239
275.172300	108.915529	50.344244
271.576980	120.865329	50.349249
267.731007	120.248125	50.354253
264.804692	112.386653	50.359258
261.008524	126.021888	50.364263
257.556261	119.169534	50.369268
253.746698	125.863127	50.374273
250.243245	120.101053	50.379277
247.008255	112.241351	50.384282
243.258662	128.768444	50.389287
240.275521	122.330306	50.394292
236.317359	126.935784	50.399297
232.725926	124.337746	50.404301
229.629315	118.203220	50.409306
225.709937	120.338194	50.414311
222.373249	115.192333	50.419316
219.214249	126.874525	50.424321
215.690523	126.395243	50.429325
212.059771	114.387529	50.434330
208.302891	131.305001	50.439335
204.613926	115.411261	50.444340
201.302224	120.640469	50.449345
198.102990	115.291431	50.454349
194.682119	125.755223	50.459354
190.679673	125.280918	50.464359
187.736890	122.990723	50.469364
183.637324	122.338982	50.474369
180.214357	121.726764	50.479373
177.066834	115.934828	50.484378
173.243427	123.670533	50.489383
169.640958	119.701365	50.494388
166.433358	124.105828	50.499393
163.024366	127.443247	50.504397
159.705150	118.143294	50.509402
155.904796	120.609219	50.514407
152.489153	122.846449	50.519412
148.472373	121.655105	50.524417
145.425896	121.105267	50.529421
142.203656	126.352812	50.534426
138.450894	131.076007	50.539431
135.146857	119.311065	50.544436
131.308197	129.241691	50.549441
127.602425	125.085296	50.554445
124.227579	119.705520	50.559450
120.618127	126.947520	50.564455
117.279498	117.357011	50.569460
113.575722	131.079244	50.574465
110.336312	130.696274	50.579469
107.091663	122.061613	50.584474
103.579064	132.856852	50.589479
100.047897	116.980422	50.594484
96.590923	126.727276	50.599489
92.733818	125.068620	50.604493
89.238898	117.831233	50.609498
85.648857	115.634285	50.614503
82.744821	118.072288	50.619508
78.474603	116.806717	50.624513
74.805281	122.713307	50.629517
71.799190	115.025889	50.634522
68.251968	116.828045	50.639527
65.147660	113.531378	50.644532
61.701908	116.937548	50.649537
57.670602	120.609362	50.654541
54.061543	124.310261	50.659546
50.560538	123.683508	50.664551
47.376965	115.863601	50.669556
44.095382	122.265604	50.674561
40.202176	122.238022	50.679565
36.640231	121.507156	50.684570
33.181248	131.164022	50.689575
30.012443	118.703817	50.694580
26.199149	112.979854	50.699585
22.648744	113.406598	50.704589
19.132042	116.811773	50.709594
15.885194	125.033530	50.714599
12.303680	113.890649	50.719604
8.675317	134.277111	50.724609
5.208344	117.346438	50.729613
2.117352	119.254962	50.734618