Fri Jun 17 18:08:57 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.280631	83.706357	0.000000
-0.067063	83.398336	0.005005
-0.194588	78.814871	0.010010
0.261607	81.382522	0.015014
-0.067646	78.023080	0.020019
0.018794	74.737217	0.025024
-0.078793	79.360345	0.030029
-0.044165	65.226784	0.035034
-0.602109	61.825634	0.040038
-1.108646	41.804523	0.045043
-1.022402	36.900400	0.050048
-1.478799	28.983660	0.055053
-1.636408	28.820854	0.060058
-1.679090	18.224095	0.065062
-2.690651	19.258738	0.070067
-2.670241	4.330780	0.075072
-2.898119	2.783747	0.080077
-3.619088	-0.895955	0.085082
-3.859050	-2.640282	0.090086
-4.100879	-1.554993	0.095091
-3.956910	-6.173295	0.100096
-4.393403	-2.753808	0.105101
-4.769783	-1.064627	0.110106
-5.384567	5.733960	0.115110
-5.640655	-3.481528	0.120115
-5.731668	-13.600785	0.125120
-5.741749	2.672487	0.130125
-5.977471	-1.982162	0.135130
-5.790379	4.322428	0.140134
-6.520476	-0.823293	0.145139
-6.804760	-0.182634	0.150144
-7.378905	-2.295082	0.155149
-7.319514	3.804594	0.160154
-7.273991	-1.948566	0.165158
-7.613955	1.372395	0.170163
-7.762517	3.464939	0.175168
-8.703885	7.011559	0.180173
-8.610314	-3.257768	0.185178
-8.603199	4.509542	0.190182
-9.003700	-1.912428	0.195187
-9.291327	-0.667584	0.200192
-9.825449	6.151933	0.205197
-10.345877	3.073707	0.210202
-10.412227	-2.289483	0.215206
-10.428057	-2.194463	0.220211
-10.570514	2.457214	0.225216
-10.276006	-3.071131	0.230221
-10.664627	6.016573	0.235226
-11.063189	-3.655334	0.240230
-12.108158	2.774512	0.245235
-12.061673	1.305801	0.250240
-11.839584	-3.946284	0.255245
-11.858465	5.876978	0.260250
-12.157489	-7.509617	0.265254
-12.830823	8.591916	0.270259
-13.177977	2.721296	0.275264
-13.330580	-0.223498	0.280269
-13.077744	-4.202593	0.285274
-13.675577	-9.000498	0.290278
-14.776889	4.009969	0.295283
-15.401578	-4.119915	0.300288
-15.223857	-2.777781	0.305293
-14.507501	3.111863	0.310298
-14.792859	-5.129871	0.315302
-15.327189	-7.540980	0.320307
-15.372292	0.533960	0.325312
-15.068870	10.522097	0.330317
-15.766422	6.221258	0.335322
-16.519735	6.005523	0.340326
-16.781253	0.895187	0.345331
-16.935481	-1.497407	0.350336
-16.589800	-0.661712	0.355341
-17.585128	3.673130	0.360346
-18.240999	-6.331129	0.365350
-18.479604	2.024609	0.370355
-18.356044	3.741199	0.375360
-18.447679	1.595913	0.380365
-18.764319	2.155323	0.385370
-18.173318	0.769756	0.390374
-18.566147	-0.969881	0.395379
-19.035484	-2.289316	0.400384
-19.547563	-5.530143	0.405389
-19.886063	4.543374	0.410394
-19.786584	-0.009126	0.415398
-20.097757	1.842670	0.420403
-21.007886	-4.187348	0.425408
-21.248030	-1.790100	0.430413
-21.397128	-3.333650	0.435418
-21.528038	-4.676579	0.440422
-21.771926	4.990501	0.445427
-21.543089	-4.442926	0.450432
-21.643862	-4.225650	0.455437
-22.347440	-2.864112	0.460442
-22.618168	-7.087892	0.465446
-23.258786	9.600586	0.470451
-22.977812	4.761982	0.475456
-23.304455	-1.524659	0.480461
-23.420546	-0.430867	0.485466
-23.315040	-1.036997	0.490470
-24.204549	0.002227	0.495475
-24.337839	-7.302998	0.500480
-24.954880	-5.907892	0.505485
-24.719486	-2.311191	0.510490
-24.789658	-12.722010	0.515494
-25.571368	0.157782	0.520499
-25.757238	3.925735	0.525504
-25.973679	5.515915	0.530509
-26.134259	-9.253680	0.535514
-26.229320	-0.139590	0.540518
-26.592858	2.265736	0.545523
-26.538300	-2.508001	0.550528
-27.223551	0.469380	0.555533
-27.739278	3.750689	0.560538
-28.004544	0.517973	0.565542
-28.167410	3.572309	0.570547
-27.937852	1.648713	0.575552
-27.722727	-4.250441	0.580557
-28.524196	9.235879	0.585562
-29.075298	-12.044795	0.590566
-29.269805	0.985833	0.595571
-29.218101	-4.568852	0.600576
-29.490653	1.006637	0.605581
-29.475963	8.782160	0.610586
-30.024424	-7.243096	0.615590
-30.715203	1.579893	0.620595
-31.241372	-1.953598	0.625600
-31.230493	-3.718897	0.630605
-31.346916	0.756579	0.635610
-31.230776	-4.483223	0.640614
-31.609292	3.084748	0.645619
-31.315191	-0.925675	0.650624
-32.154180	-5.539838	0.655629
-32.682134	0.338379	0.660634
-32.843638	-8.554600	0.665638
-33.166033	-1.466391	0.670643
-32.906387	1.419643	0.675648
-32.902032	1.562615	0.680653
-33.363973	0.903794	0.685658
-33.805811	-6.605094	0.690662
-34.523762	-1.254329	0.695667
-34.507130	-11.735815	0.700672
-34.618370	-1.392441	0.705677
-34.421328	0.314697	0.710682
-34.843381	-4.304438	0.715686
-35.928860	-8.054569	0.720691
-35.957802	-3.083540	0.725696
-35.966322	-3.851076	0.730701
-36.092462	1.952461	0.735706
-35.663052	-9.281975	0.740710
-36.646301	0.213384	0.745715
-36.989099	-5.163447	0.750720
-37.298896	-5.348708	0.755725
-37.494373	-1.043412	0.760730
-37.499165	-10.968618	0.765734
-37.948564	0.333744	0.770739
-37.695290	-9.148929	0.775744
-38.079575	2.714866	0.780749
-38.579793	-12.346554	0.785754
-38.882805	-9.088370	0.790758
-39.075147	-2.512733	0.795763
-39.204420	-0.252113	0.800768
-40.446380	-5.179743	0.805773
-40.647795	3.660965	0.810778
-39.851919	-10.606948	0.815782
-40.430874	-4.621393	0.820787
-40.547817	3.840808	0.825792
-41.017528	-6.387376	0.830797
-40.918126	-6.056757	0.835802
-40.642850	-15.066140	0.840806
-41.705614	-1.493773	0.845811
-42.084667	-12.218505	0.850816
-42.080137	-12.021495	0.855821
-42.612514	-5.136363	0.860826
-42.130913	-7.742975	0.865830
-43.493079	-5.329126	0.870835
-43.761137	-9.078770	0.875840
-43.678824	-10.293159	0.880845
-43.727811	-6.532176	0.885850
-43.749942	-13.155354	0.890854
-43.993919	-7.453197	0.895859
-44.026428	1.648916	0.900864
-44.154899	-9.105629	0.905869
-45.453784	1.771799	0.910874
-45.640197	-8.599769	0.915878
-45.926659	-9.662088	0.920883
-45.911398	-3.075180	0.925888
-45.793797	0.940493	0.930893
-45.974293	-5.953345	0.935898
-45.846167	-4.804837	0.940902
-45.673988	-11.703621	0.945907
-46.641429	4.872237	0.950912
-46.934075	1.060374	0.955917
-47.860254	-1.166806	0.960922
-48.223408	-4.056668	0.965926
-48.138304	-1.528388	0.970931
-48.388344	-3.218348	0.975936
-48.802776	-3.380494	0.980941
-48.886193	0.549603	0.985946
-48.784812	-0.847526	0.990950
-48.746300	4.006327	0.995955
-49.236346	-1.855531	1.000960
-49.038672	-10.063885	1.005965
-49.955455	4.753048	1.010970
-49.961264	-1.715577	1.015974
-50.580145	3.566234	1.020979
-50.414745	-4.871185	1.025984
-51.190771	1.809959	1.030989
-51.786248	-0.608544	1.035994
-51.809799	-4.121387	1.040998
-51.752669	-2.594440	1.046003
-51.742375	4.498459	1.051008
-51.547998	5.746658	1.056013
-51.768537	5.622533	1.061018
-52.556055	-3.452122	1.066022
-53.097463	0.897258	1.071027
-53.217411	-1.385791	1.076032
-53.285285	4.838041	1.081037
-53.455863	-0.801843	1.086042
-53.930727	-11.142431	1.091046
-54.553799	-6.186702	1.096051
-54.800378	-3.855870	1.101056
-54.630143	-11.650007	1.106061
-54.750341	-1.112158	1.111066
-54.729115	-2.925943	1.116070
-55.614451	-5.722099	1.121075
-56.043536	-4.710069	1.126080
-56.543748	-7.575766	1.131085
-56.660653	0.845381	1.136090
-56.559551	-4.603260	1.141094
-56.764880	-0.968033	1.146099
-56.997350	-6.928941	1.151104
-57.009177	-9.383286	1.156109
-57.085712	2.627669	1.161114
-56.952239	-2.743673	1.166118
-57.724611	-0.914074	1.171123
-57.911792	5.529484	1.176128
-58.171435	-4.873718	1.181133
-59.101044	-0.213346	1.186138
-59.218166	-7.729634	1.191142
-59.924041	-2.328186	1.196147
-59.756603	-1.745838	1.201152
-59.745116	1.306156	1.206157
-60.095922	-3.985870	1.211162
-59.787113	-1.966786	1.216166
-60.010777	5.211966	1.221171
-60.589201	-0.030189	1.226176
-60.885675	-2.790043	1.231181
-61.456859	4.608877	1.236186
-61.311447	-3.225734	1.241190
-61.400512	4.806588	1.246195
-61.564956	1.049389	1.251200
-62.064708	-0.254921	1.256205
-62.821248	-5.154108	1.261210
-62.911292	-4.250134	1.266214
-63.112344	-5.488459	1.271219
-62.981246	1.983751	1.276224
-62.829674	-8.488394	1.281229
-63.560394	4.275977	1.286234
-63.766907	-2.722857	1.291238
-64.152907	1.941085	1.296243
-64.264651	4.146697	1.301248
-64.960335	-2.991043	1.306253
-65.678467	1.559785	1.311258
-65.614506	-5.995285	1.316262
-65.647293	2.575860	1.321267
-66.062148	1.524425	1.326272
-65.588470	-8.318109	1.331277
-66.134483	6.899537	1.336282
-66.008182	-3.881769	1.341286
-66.409539	1.409666	1.346291
-67.018810	-2.991473	1.351296
-67.262324	6.844062	1.356301
-67.708362	6.476820	1.361306
-67.830684	-3.677091	1.366310
-68.071537	5.000272	1.371315
-67.865852	2.163654	1.376320
-68.536164	-0.331204	1.381325
-69.113219	-2.498409	1.386330
-69.032227	-5.238918	1.391334
-69.208299	-1.252770	1.396339
-69.089009	-0.141076	1.401344
-69.303149	-6.735495	1.406349
-70.022162	3.642999	1.411354
-70.262585	0.509953	1.416358
-70.454697	-0.226275	1.421363
-70.888632	-1.057081	1.426368
-70.802771	-1.926735	1.431373
-71.003516	3.082521	1.436378
-71.586260	-4.485223	1.441382
-72.330300	-1.784388	1.446387
-72.725864	-6.202500	1.451392
-72.622553	-3.530238	1.456397
-72.341074	2.544157	1.461402
-72.271810	-1.884526	1.466406
-72.708292	-4.591310	1.471411
-72.989146	-3.554782	1.476416
-73.135447	0.302494	1.481421
-73.955970	-2.625197	1.486426
-73.922786	-2.466890	1.491430
-74.180381	-1.581831	1.496435
-74.130384	-7.441300	1.501440
-75.026635	-0.878693	1.506445
-75.551806	-3.159698	1.511450
-75.682873	-16.958191	1.516454
-75.939714	-4.134271	1.521459
-75.884179	-4.669542	1.526464
-75.985660	-9.392276	1.531469
-76.252989	-1.408862	1.536474
-75.935090	-3.638994	1.541478
-75.976033	-6.628785	1.546483
-76.601925	1.446595	1.551488
-76.989354	-8.903195	1.556493
-77.175752	-3.931252	1.561498
-78.146925	5.175936	1.566502
-78.535420	-0.363786	1.571507
-78.542546	-0.688550	1.576512
-78.841085	-4.098652	1.581517
-79.212546	-6.419809	1.586522
-79.041283	-6.241635	1.591526
-79.262093	9.729031	1.596531
-79.508347	-1.135778	1.601536
-79.105743	-4.772540	1.606541
-79.574195	6.860165	1.611546
-80.057144	-2.917874	1.616550
-80.675352	-1.039701	1.621555
-81.126323	8.672655	1.626560
-80.982833	-4.886348	1.631565
-80.830307	-1.518395	1.636570
-81.590414	-2.477706	1.641574
-82.082924	3.516179	1.646579
-82.194512	-1.194418	1.651584
-82.278170	-5.165924	1.656589
-82.743906	5.871777	1.661594
-82.664780	0.208740	1.666598
-82.582539	5.452742	1.671603
-83.175120	-0.544206	1.676608
-83.489006	-1.419830	1.681613
-83.910287	4.460789	1.686618
-83.789206	-0.026630	1.691622
-83.891541	5.165176	1.696627
-84.424414	7.899189	1.701632
-84.965083	4.267281	1.706637
-85.701755	1.637237	1.711642
-85.490346	-0.335834	1.716646
-85.694480	-6.431687	1.721651
-85.580725	-2.692231	1.726656
-85.518428	-7.098640	1.731661
-85.733656	-0.530841	1.736666
-86.268738	-4.329234	1.741670
-87.000698	-8.987022	1.746675
-87.273777	-5.979682	1.751680
-87.024747	-10.419302	1.756685
-87.569838	6.376229	1.761690
-87.350154	-5.587404	1.766694
-88.032246	-8.295387	1.771699
-88.638622	-4.842523	1.776704
-88.706624	-9.567072	1.781709
-88.879000	2.243341	1.786714
-88.823962	-10.940037	1.791718
-89.010920	3.510101	1.796723
-89.577791	0.053635	1.801728
-90.004442	-4.402325	1.806733
-90.484750	6.103630	1.811738
-90.425701	-5.184877	1.816742
-90.496521	3.290965	1.821747
-90.822689	9.563259	1.826752
-90.652871	-1.800297	1.831757
-91.201497	3.785764	1.836762
-91.800168	-3.782683	1.841766
-92.192660	6.031639	1.846771
-92.248841	-0.655736	1.851776
-92.055624	-1.229878	1.856781
-92.537980	0.587431	1.861786
-92.351969	-4.376673	1.866790
-92.959886	-4.944720	1.871795
-93.318578	-2.647344	1.876800
-93.644831	-4.209786	1.881805
-93.534021	0.475365	1.886810
-93.371565	-9.304383	1.891814
-94.548710	-3.708956	1.896819
-95.210798	-5.426318	1.901824
-95.183831	-0.000270	1.906829
-95.434289	-9.879305	1.911834
-95.290732	-6.017133	1.916838
-95.337191	-12.123801	1.921843
-95.736456	-3.198509	1.926848
-95.150751	-11.961332	1.931853
-96.316251	4.711586	1.936858
-96.597895	-9.259209	1.941862
-96.950296	-8.189278	1.946867
-96.913736	-13.152018	1.951872
-97.124350	3.667037	1.956877
-97.240030	4.852521	1.961882
-97.977271	-7.356363	1.966886
-98.326926	-5.021419	1.971891
-98.667987	-9.645915	1.976896
-98.388871	-8.670703	1.981901
-98.597143	-3.050648	1.986906
-98.568351	-10.275657	1.991910
-99.092752	-6.913575	1.996915
-99.860810	-9.683018	2.006912
-99.620017	-5.622954	2.016909
-98.946365	-4.715734	2.026906
-98.053895	-2.612375	2.036902
-97.393059	-9.101267	2.046899
-97.467237	-0.089611	2.056896
-97.055196	-4.182961	2.066893
-96.102286	-6.142639	2.076890
-95.802015	-5.654658	2.086886
-95.465989	-4.736164	2.096883
-94.551629	-0.962531	2.106880
-94.374822	-8.196852	2.116877
-93.804783	-6.102527	2.126874
-92.855771	-8.834890	2.136870
-92.964675	-7.565819	2.146867
-92.394655	-13.418218	2.156864
-91.729901	-0.901604	2.166861
-91.255916	-4.622930	2.176858
-90.841887	-8.192426	2.186854
-90.054216	-8.502489	2.196851
-89.960074	-13.425391	2.206848
-89.529171	-4.554206	2.216845
-88.587264	-9.577925	2.226842
-88.201657	-0.410739	2.236838
-87.905750	-5.743773	2.246835
-87.103094	0.961178	2.256832
-86.971893	-5.182026	2.266829
-85.863321	3.629862	2.276826
-85.564070	0.261220	2.286822
-85.500782	-6.768900	2.296819
-84.787606	-9.136245	2.306816
-83.931138	-5.061753	2.316813
-83.804007	1.992195	2.326810
-83.598565	1.207116	2.336806
-82.678704	1.853899	2.346803
-82.387240	4.544405	2.356800
-81.685222	1.859028	2.366797
-80.917537	4.111761	2.376794
-80.680682	3.640752	2.386790
-80.670555	3.387230	2.396787
-79.526746	-3.762243	2.406784
-79.253621	0.855163	2.416781
-78.899341	-2.838954	2.426778
-78.205257	-2.422955	2.436774
-77.977686	-8.621693	2.446771
-76.727188	-2.382001	2.456768
-76.312183	-6.417951	2.466765
-76.728559	-2.696956	2.476762
-75.810022	-6.375012	2.486758
-74.832562	-7.344140	2.496755
-74.848974	-4.112455	2.506752
-74.430238	-9.322856	2.516749
-73.462861	-5.862307	2.526746
-73.129352	-4.254820	2.536742
-73.026374	-9.776283	2.546739
-72.239290	-7.473230	2.556736
-71.656935	-0.930423	2.566733
-71.142952	-5.126467	2.576730
-70.128732	-0.749614	2.586726
-70.407734	-1.752118	2.596723
-70.126517	-0.429346	2.606720
-68.832180	-3.034763	2.616717
-68.436698	-4.927856	2.626714
-68.445480	-4.314605	2.636710
-67.871651	-12.299540	2.646707
-67.200427	-13.908901	2.656704
-66.670495	-5.519280	2.666701
-66.407491	-8.211697	2.676698
-65.587040	-3.399765	2.686694
-65.235233	0.849707	2.696691
-64.584295	-4.500257	2.706688
-63.945659	-9.412508	2.716685
-63.592034	-5.996540	2.726682
-63.457456	-4.772289	2.736678
-62.591632	-8.958256	2.746675
-62.152854	-6.801405	2.756672
-61.738952	-4.001637	2.766669
-60.823121	2.614171	2.776666
-60.692858	-0.479996	2.786662
-60.623680	-8.117671	2.796659
-59.647128	-13.006661	2.806656
-59.152829	-10.319049	2.816653
-58.801858	-11.491274	2.826650
-57.901168	-8.102226	2.836646
-57.345081	-4.481431	2.846643
-57.275594	-4.600584	2.856640
-56.805443	-5.240182	2.866637
-56.295509	-1.636412	2.876634
-55.855542	-0.936131	2.886630
-54.751649	-1.969738	2.896627
-54.419015	-0.257385	2.906624
-54.371028	-1.016883	2.916621
-54.149631	-1.006383	2.926618
-52.995951	-1.438133	2.936614
-52.899831	-8.049701	2.946611
-51.569141	2.820039	2.956608
-51.403726	1.415675	2.966605
-51.740295	-0.249237	2.976602
-50.812339	-3.617663	2.986598
-50.236641	-4.761646	2.996595
-49.620411	-5.667957	3.006592
-48.654366	-3.483951	3.016589
-48.892597	-2.750169	3.026586
-48.580119	0.453128	3.036582
-47.305322	-4.874871	3.046579
-47.008375	-1.454616	3.056576
-46.896567	0.749869	3.066573
-45.990087	-10.285104	3.076570
-45.478840	-3.190087	3.086566
-44.816566	-5.795547	3.096563
-44.880516	-9.119621	3.106560
-44.231385	-2.348833	3.116557
-43.659272	-10.802739	3.126554
-43.429236	-6.293753	3.136550
-42.197040	-7.706503	3.146547
-41.736847	-7.569529	3.156544
-41.432526	-10.834687	3.166541
-41.629073	-6.832128	3.176538
-40.599388	-7.408640	3.186534
-39.961974	-10.010757	3.196531
-39.824822	-2.435671	3.206528
-38.741123	-1.781533	3.216525
-38.429106	-11.268828	3.226522
-38.517536	-8.809768	3.236518
-37.391171	-9.858762	3.246515
-37.081669	-7.225587	3.256512
-36.957228	-3.387620	3.266509
-36.211270	-3.361568	3.276506
-35.867034	-5.437201	3.286502
-34.802327	-13.981676	3.296499
-34.065098	-17.965473	3.306496
-34.026207	-11.323041	3.316493
-33.936258	-11.764492	3.326490
-33.487508	-7.351332	3.336486
-32.276588	-7.085248	3.346483
-32.331227	-9.829979	3.356480
-31.527129	-10.014728	3.366477
-30.770558	-9.101520	3.376474
-30.616705	-10.846369	3.386470
-30.337570	-12.657090	3.396467
-29.348476	-10.407560	3.406464
-28.806672	-11.198161	3.416461
-28.718955	-7.613516	3.426458
-28.260525	-6.664976	3.436454
-27.491623	-6.842689	3.446451
-27.415143	-5.080051	3.456448
-26.528924	-5.063875	3.466445
-25.950373	-2.098826	3.476442
-25.805882	-8.181803	3.486438
-25.039039	-7.139897	3.496435
-24.497532	2.763662	3.506432
-24.181179	-8.781577	3.516429
-23.072134	-4.526177	3.526426
-22.851946	-0.065341	3.536422
-22.399270	-5.710134	3.546419
-22.684655	0.601708	3.556416
-22.002360	-4.727580	3.566413
-20.977575	-2.807815	3.576410
-20.254796	-3.015400	3.586406
-20.275615	-8.130214	3.596403
-20.069001	-1.947174	3.606400
-18.821907	-2.670264	3.616397
-18.448264	-8.674361	3.626394
-18.256037	-2.732943	3.636390
-17.039463	2.870668	3.646387
-16.584149	-9.622152	3.656384
-16.646995	-3.453204	3.666381
-16.780159	-5.756330	3.676378
-15.907269	-2.073784	3.686374
-14.863409	1.032256	3.696371
-14.183370	-3.387188	3.706368
-13.956767	4.149524	3.716365
-13.519698	0.784059	3.726362
-13.406142	2.929970	3.736358
-12.333010	-1.232357	3.746355
-11.797581	-5.379798	3.756352
-11.504961	-3.613963	3.766349
-11.258219	2.489898	3.776346
-10.198604	1.895182	3.786342
-10.099199	-1.990308	3.796339
-9.835459	-5.343757	3.806336
-8.995765	-5.624317	3.816333
-8.614340	2.173353	3.826330
-7.949567	3.350779	3.836326
-6.967341	-7.754278	3.846323
-7.240221	-3.814311	3.856320
-6.786235	-3.392178	3.866317
-6.006440	-1.714428	3.876314
-5.281335	-2.792744	3.886310
-5.205414	-0.485872	3.896307
-4.494656	-8.256860	3.906304
-4.115777	-6.171053	3.916301
-3.735320	-1.681729	3.926298
-2.992032	-0.900859	3.936294
-2.925299	4.784807	3.946291
-2.354512	22.512305	3.956288
-2.000643	34.382789	3.966285
-1.690769	50.610370	3.976282
-1.396443	66.113647	3.986278
-0.599400	88.664347	3.996275
-0.113356	107.000753	4.006272
0.000000	120.769558	4.011277
0.723994	136.244709	4.016282
0.925966	149.691844	4.021286
1.086171	158.772284	4.026291
0.741272	162.843760	4.031296
0.764208	161.639029	4.036301
0.899285	157.734917	4.041306
0.848050	162.329843	4.046310
1.374867	169.903708	4.051315
1.214792	180.175403	4.056320
1.412289	183.809035	4.061325
1.498600	168.273432	4.066330
1.429321	160.958670	4.071334
1.500976	164.756279	4.076339
1.221518	154.235682	4.081344
1.125019	162.634783	4.086349
1.495658	145.495396	4.091354
1.250169	154.986422	4.096358
1.433907	154.897711	4.101363
1.275136	155.213821	4.106368
0.697774	161.443072	4.111373
1.600193	177.184212	4.116378
1.926589	190.704238	4.121382
1.751473	186.747286	4.126387
1.457101	178.080713	4.131392
1.469674	171.836480	4.136397
1.429031	154.958431	4.141402
1.273050	177.214749	4.146406
1.563765	171.081559	4.151411
1.640828	178.812073	4.156416
1.249695	186.877335	4.161421
1.457719	185.412540	4.166426
1.469931	194.074195	4.171430
1.839760	192.204222	4.176435
1.854020	195.211001	4.181440
1.783903	188.846122	4.186445
1.697755	166.882497	4.191450
1.059260	171.279431	4.196454
1.631489	176.422720	4.201459
1.671312	191.754519	4.206464
1.624722	189.631319	4.211469
2.057377	193.089315	4.216474
1.545896	191.716284	4.221478
1.638138	184.426760	4.226483
1.255563	184.311998	4.231488
1.535753	195.721355	4.236493
1.582521	181.703081	4.241498
1.414317	195.354847	4.246502
1.784943	184.299156	4.251507
1.912920	196.259700	4.256512
2.174606	197.095160	4.261517
2.184579	196.066431	4.266522
1.682297	201.817122	4.271526
1.542187	196.196960	4.276531
1.653131	198.224889	4.281536
1.696813	207.708732	4.286541
2.076551	194.655113	4.291546
1.974935	197.085803	4.296550
2.091603	197.142227	4.301555
2.180464	203.591689	4.306560
1.972738	201.177170	4.311565
2.053054	203.341021	4.316570
1.859071	197.973912	4.321574
2.106173	190.910639	4.326579
1.906539	195.380860	4.331584
1.491933	196.250779	4.336589
1.945358	194.087490	4.341594
1.756199	199.918744	4.346598
2.115586	188.343172	4.351603
2.151809	188.387116	4.356608
1.888195	202.044287	4.361613
1.979143	202.140111	4.366618
1.872712	203.249479	4.371622
1.868491	205.537295	4.376627
1.883267	193.722210	4.381632
1.820999	201.630206	4.386637
1.841486	191.373291	4.391642
1.615628	206.858980	4.396646
1.884315	213.998424	4.401651
2.238968	222.359276	4.406656
2.247834	219.180009	4.411661
2.306721	224.453627	4.416666
2.138865	230.237741	4.421670
2.259766	221.328273	4.426675
2.251804	229.923050	4.431680
2.224634	226.456733	4.436685
2.566608	221.481434	4.441690
2.178794	233.130110	4.446694
2.408397	219.074311	4.451699
2.279061	216.276369	4.456704
1.927572	211.500198	4.461709
2.201012	212.077766	4.466714
2.237699	220.992096	4.471718
2.231560	221.719535	4.476723
2.598477	230.646867	4.481728
2.232381	231.088605	4.486733
2.537853	215.683471	4.491738
2.426752	232.802373	4.496742
2.674520	225.368975	4.501747
2.443628	226.461341	4.506752
2.573961	220.493908	4.511757
2.556191	205.656164	4.516762
2.037994	204.245768	4.521766
2.526591	216.762263	4.526771
2.217755	217.564481	4.531776
2.344109	236.451678	4.536781
2.624436	230.105692	4.541786
2.769137	231.086891	4.546790
2.433378	225.133580	4.551795
2.409648	225.071063	4.556800
2.397086	232.657845	4.561805
2.724128	225.734399	4.566810
2.770337	240.326177	4.571814
2.700031	228.821994	4.576819
2.668169	226.082243	4.581824
2.152579	224.868941	4.586829
2.217546	226.994301	4.591834
2.204372	241.252790	4.596838
2.422690	245.252382	4.601843
2.696982	235.286548	4.606848
2.550545	235.421827	4.611853
2.659628	226.228978	4.616858
2.380529	241.966665	4.621862
2.760964	233.603090	4.626867
2.366279	240.984227	4.631872
2.440605	234.673268	4.636877
2.626135	225.168953	4.641882
2.051226	243.949334	4.646886
2.695780	261.413112	4.651891
2.932635	259.027896	4.656896
2.939229	260.886106	4.661901
3.347130	258.136404	4.666906
2.753189	268.094484	4.671910
2.802954	260.705622	4.676915
2.681556	255.451932	4.681920
2.921652	270.812289	4.686925
2.789996	266.422249	4.691930
2.684917	276.650531	4.696934
2.651115	273.977201	4.701939
2.732566	263.253478	4.706944
2.498277	269.493633	4.711949
2.834047	268.812124	4.716954
2.855422	269.974649	4.721958
2.628022	266.094446	4.726963
2.780364	265.710809	4.731968
2.966715	263.580061	4.736973
3.001863	256.956122	4.741978
2.804871	264.763803	4.746982
2.886619	266.992150	4.751987
3.006780	271.330900	4.756992
2.890300	271.390555	4.761997
3.374086	280.989155	4.767002
2.919030	278.042875	4.772006
3.118753	268.734692	4.777011
3.074220	265.408002	4.782016
2.819361	272.498726	4.787021
3.151823	285.126869	4.792026
3.265987	288.659924	4.797030
3.354005	287.453050	4.802035
3.412887	270.716989	4.807040
3.131480	273.993740	4.812045
3.505814	263.707171	4.817050
3.204458	268.809997	4.822054
2.980980	264.731416	4.827059
3.277278	266.099451	4.832064
2.904246	272.900201	4.837069
3.225388	263.110673	4.842074
3.117591	271.394100	4.847078
2.766503	279.730006	4.852083
2.965669	292.326438	4.857088
3.271657	296.563467	4.862093
3.249713	296.028040	4.867098
3.274693	297.152672	4.872102
2.989364	292.331341	4.877107
3.238001	297.304679	4.882112
3.283618	306.091281	4.887117
3.678011	306.579092	4.892122
3.615891	302.137623	4.897126
3.702121	304.277812	4.902131
3.542151	299.067617	4.907136
3.404980	297.926980	4.912141
3.718772	298.638544	4.917146
3.477940	303.939706	4.922150
3.535921	301.972763	4.927155
3.973979	296.294554	4.932160
3.447019	287.731303	4.937165
3.066917	275.565611	4.942170
3.448272	283.682300	4.947174
3.318268	297.530073	4.952179
3.469749	287.601785	4.957184
3.610115	297.705815	4.962189
3.693258	288.567561	4.967194
3.560159	305.828529	4.972198
3.728522	300.957245	4.977203
3.510945	296.234171	4.982208
3.201957	302.368157	4.987213
3.762979	300.889279	4.992218
3.783601	299.042406	4.997222
3.751020	293.881883	5.002227
3.464957	293.044035	5.007232
3.442771	304.043943	5.012237
3.462328	294.876590	5.017242
3.646249	302.810221	5.022246
3.476626	300.100853	5.027251
3.520076	306.426876	5.032256
3.673050	307.640742	5.037261
3.480464	300.153219	5.042266
3.197049	298.815086	5.047270
3.290942	308.171259	5.052275
3.488088	316.489078	5.057280
3.635914	333.160324	5.062285
4.047321	333.400023	5.067290
3.908644	328.477543	5.072294
3.940264	335.815694	5.077299
3.961109	330.441248	5.082304
3.459165	337.903800	5.087309
3.662611	330.614076	5.092314
3.694474	334.075178	5.097318
4.064077	328.725647	5.102323
4.050371	336.130532	5.107328
3.721437	333.553801	5.112333
4.010634	335.471215	5.117338
3.861952	336.772714	5.122342
3.909572	334.228315	5.127347
3.894269	324.907095	5.132352
4.052401	335.218159	5.137357
4.137292	334.281951	5.142362
3.868284	344.299540	5.147366
3.876382	341.005724	5.152371
3.874940	330.786500	5.157376
3.868022	334.609247	5.162381
3.685601	329.591029	5.167386
3.889137	336.206586	5.172390
3.881784	331.114278	5.177395
3.975930	326.046542	5.182400
3.994064	338.820509	5.187405
4.257908	341.178244	5.192410
3.907807	336.845014	5.197414
3.964753	353.359115	5.202419
4.331013	352.118817	5.207424
4.142501	358.242471	5.212429
4.559859	355.849736	5.217434
4.108222	338.144297	5.222438
4.240531	346.735361	5.227443
4.005456	341.398909	5.232448
4.296731	354.209582	5.237453
4.236879	365.476669	5.242458
4.431191	360.220593	5.247462
4.207159	357.298455	5.252467
4.478356	354.259670	5.257472
4.285907	347.521969	5.262477
4.318105	336.432632	5.267482
4.064240	337.546583	5.272486
4.305375	345.911373	5.277491
4.690188	354.535066	5.282496
4.421932	346.180976	5.287501
4.361534	338.170631	5.292506
4.456168	335.236380	5.297510
3.995140	328.890042	5.302515
4.422653	335.680900	5.307520
4.357136	365.424083	5.312525
4.199233	351.976224	5.317530
4.490272	361.953429	5.322534
4.465577	357.927821	5.327539
4.553180	360.221118	5.332544
4.287726	365.810357	5.337549
4.612837	356.394454	5.342554
4.793360	362.458154	5.347558
4.560388	362.230712	5.352563
4.386813	355.615375	5.357568
4.287531	355.144304	5.362573
4.790018	353.008557	5.367578
4.716286	359.776570	5.372582
4.695613	353.486482	5.377587
4.818128	354.260230	5.382592
4.396496	355.232951	5.387597
4.231434	349.442635	5.392602
4.478081	361.262223	5.397606
4.395742	352.033233	5.402611
4.449238	359.095044	5.407616
4.371596	354.236806	5.412621
4.664426	354.799515	5.417626
4.635232	355.356941	5.422630
4.309117	360.951524	5.427635
4.660749	354.431626	5.432640
4.499365	353.916610	5.437645
4.903805	354.184304	5.442650
4.652090	365.442037	5.447654
4.741400	347.599713	5.452659
4.556747	348.514498	5.457664
4.651354	356.151411	5.462669
4.640982	370.950840	5.467674
5.089740	392.145741	5.472678
4.880507	384.668837	5.477683
4.904774	368.685135	5.482688
4.538182	368.594947	5.487693
4.832281	379.043085	5.492698
4.843924	392.397746	5.497702
4.892977	388.958978	5.502707
4.981318	391.730298	5.507712
4.623980	398.998742	5.512717
4.604710	391.539200	5.517722
4.986009	389.852990	5.522726
4.686179	388.809237	5.527731
4.785692	382.630981	5.532736
4.787968	397.094641	5.537741
4.877675	389.818268	5.542746
4.898384	393.584934	5.547750
4.739634	396.736935	5.552755
5.113605	387.006432	5.557760
4.954625	394.336823	5.562765
4.982054	391.432479	5.567770
5.014351	395.830267	5.572774
4.970011	397.954678	5.577779
5.034462	396.715008	5.582784
4.656096	402.657310	5.587789
5.100289	406.516000	5.592794
5.113473	416.258615	5.597798
5.256791	429.870650	5.602803
5.455952	413.121382	5.607808
5.153243	416.757694	5.612813
5.164927	418.561008	5.617818
5.151052	421.436149	5.622822
5.123936	420.439420	5.627827
5.334307	419.254232	5.632832
5.317042	429.180109	5.637837
5.487874	409.401336	5.642842
5.169747	407.996541	5.647846
4.867501	411.251328	5.652851
5.393762	414.263037	5.657856
4.983824	426.874778	5.662861
5.243579	421.388566	5.667866
5.386921	426.028783	5.672870
5.141413	424.050895	5.677875
4.953200	423.019768	5.682880
4.943318	424.950395	5.687885
5.163581	422.499635	5.692890
5.625018	418.422418	5.697894
5.123362	426.718307	5.702899
5.292078	426.738455	5.707904
5.215579	421.106060	5.712909
5.581260	418.512335	5.717914
5.300688	427.858989	5.722918
5.189145	427.775349	5.727923
5.585911	424.035666	5.732928
5.330613	432.423220	5.737933
5.442105	435.540772	5.742938
5.733379	447.079503	5.747942
5.412171	438.854932	5.752947
5.733166	433.444180	5.757952
5.500793	427.520573	5.762957
5.166694	426.702345	5.767962
5.595967	438.170772	5.772966
5.831825	451.024283	5.777971
5.594734	444.270279	5.782976
5.852921	445.629865	5.787981
5.769769	425.504338	5.792986
5.418831	432.967095	5.797990
5.646470	434.657162	5.802995
5.885621	420.820805	5.808000
5.377226	425.604075	5.813005
5.813182	425.353069	5.818010
5.613558	423.101745	5.823014
5.376440	429.791173	5.828019
5.946997	441.320382	5.833024
5.521707	452.299383	5.838029
5.957538	460.854469	5.843034
5.482025	459.852935	5.848038
5.294502	458.414391	5.853043
5.994085	458.257702	5.858048
5.881343	456.799033	5.863053
6.097864	463.210020	5.868058
5.771334	463.686628	5.873062
5.866392	465.535290	5.878067
5.877756	457.613202	5.883072
5.686678	466.026411	5.888077
5.872275	449.405849	5.893082
6.214807	453.169756	5.898086
5.674832	462.719387	5.903091
5.726106	457.830415	5.908096
5.414820	456.910515	5.913101
5.813215	461.873026	5.918106
5.790268	468.281389	5.923110
5.694275	473.356267	5.928115
5.687791	456.097276	5.933120
5.718458	465.519701	5.938125
5.939567	458.596788	5.943130
5.879106	470.148215	5.948134
5.740784	465.323313	5.953139
5.981815	470.339214	5.958144
6.163050	482.027291	5.963149
6.292433	481.652201	5.968154
6.249970	472.634369	5.973158
6.234533	473.088280	5.978163
6.204665	470.517074	5.983168
5.817626	468.216183	5.988173
5.924192	462.202682	5.993178
6.096916	466.682725	5.998182
6.092107	482.944970	6.003187
6.628959	473.744222	6.008192
6.291518	477.347249	6.013197
6.254692	460.108293	6.018202
6.140355	460.428272	6.023206
6.069889	467.353657	6.028211
6.179774	455.353251	6.033216
6.068461	463.217436	6.038221
6.214731	461.507529	6.043226
6.016866	458.185365	6.048230
6.235720	465.210466	6.053235
6.396179	461.149321	6.058240
6.268843	459.783260	6.063245
6.297793	458.403655	6.068250
6.412803	465.126333	6.073254
6.280662	460.828869	6.078259
6.218554	459.876039	6.083264
6.245321	458.613816	6.088269
6.257472	461.943246	6.093274
6.045547	459.501954	6.098278
5.935629	469.400829	6.103283
6.282232	456.463992	6.108288
6.002870	468.761615	6.113293
6.387045	454.743847	6.118298
6.345702	462.858859	6.123302
6.216158	464.198825	6.128307
6.213805	454.402362	6.133312
6.012573	472.457668	6.138317
6.117611	463.652917	6.143322
6.276354	462.830721	6.148326
6.353939	463.391518	6.153331
6.209371	449.840519	6.158336
6.052207	466.862748	6.163341
5.940128	469.504196	6.168346
6.116724	465.565479	6.173350
5.998876	458.119921	6.178355
6.114148	462.530184	6.183360
6.342774	466.876615	6.188365
6.292781	456.822850	6.193370
5.918357	467.319014	6.198374
5.893741	460.937777	6.203379
6.048448	459.848073	6.208384
5.977746	462.025023	6.213389
6.175892	459.578328	6.218394
5.972154	469.303157	6.223398
6.086148	466.077753	6.228403
6.247764	466.325621	6.233408
6.219895	465.512141	6.238413
6.220939	466.205837	6.243418
6.128977	463.896554	6.248422
6.027421	470.061448	6.253427
6.186966	472.490609	6.258432
6.085418	467.473705	6.263437
6.102905	466.867782	6.268442
6.279474	475.095963	6.273446
6.153801	480.464478	6.278451
6.171181	470.766156	6.283456
6.156603	470.876363	6.288461
6.183844	474.320505	6.293466
6.285245	472.940894	6.298470
5.986217	467.169050	6.303475
6.154977	466.803992	6.308480
6.105464	473.256240	6.313485
5.924128	479.355266	6.318490
6.361111	482.335453	6.323494
6.132472	487.666619	6.328499
6.241987	487.714958	6.333504
6.204778	489.565084	6.338509
6.187286	490.262257	6.343514
6.313740	487.622244	6.348518
6.079643	469.310395	6.353523
5.991719	458.330921	6.358528
6.146697	474.062014	6.363533
6.339062	475.269741	6.368538
6.503103	478.865590	6.373542
5.795804	476.750537	6.378547
6.076442	464.198805	6.383552
6.064311	479.747713	6.388557
6.094003	482.669103	6.393562
6.328403	486.243985	6.398566
6.193497	488.688541	6.403571
6.490214	484.323738	6.408576
6.152064	481.023701	6.413581
6.017433	459.119027	6.418586
6.050255	463.360853	6.423590
5.991537	466.846117	6.428595
6.243849	478.064955	6.433600
6.365680	479.557912	6.438605
6.301907	483.362124	6.443610
6.035347	462.541036	6.448614
6.090036	465.880959	6.453619
6.053780	461.181965	6.458624
6.124000	471.945224	6.463629
6.402651	475.167807	6.468634
6.417517	478.532507	6.473638
6.063240	468.076622	6.478643
6.165482	468.933468	6.483648
5.889545	464.872038	6.488653
6.443519	475.681586	6.493658
6.303479	463.566817	6.498662
5.997689	458.147159	6.503667
6.581618	457.076890	6.508672
6.392671	467.366598	6.513677
6.305095	472.772389	6.518682
6.431292	470.521962	6.523686
6.109183	468.766567	6.528691
6.505453	469.291762	6.533696
6.514808	464.732990	6.538701
6.100612	464.964081	6.543706
6.321488	470.201782	6.548710
6.264450	470.185254	6.553715
6.369247	455.682299	6.558720
5.887814	465.883274	6.563725
6.485752	458.585546	6.568730
6.194809	462.900719	6.573734
5.969812	462.075209	6.578739
6.467741	468.767002	6.583744
6.184397	466.993522	6.588749
6.080384	470.498353	6.593754
6.125648	461.632694	6.598758
5.987698	470.284928	6.603763
6.023112	451.771819	6.608768
6.105191	466.584390	6.613773
6.149031	469.768841	6.618778
6.214017	471.867987	6.623782
5.716614	472.439497	6.628787
6.071339	459.643191	6.633792
5.965986	467.412062	6.638797
5.970026	463.885644	6.643802
6.074604	465.670563	6.648806
5.885602	459.450837	6.653811
6.116441	461.719751	6.658816
6.222860	461.354004	6.663821
6.199544	455.876347	6.668826
6.303929	463.698368	6.673830
6.135519	464.891070	6.678835
6.496506	463.349519	6.683840
6.098770	465.127349	6.688845
5.850460	454.630576	6.693850
6.188006	458.608040	6.698854
6.265394	468.722057	6.703859
6.509222	457.693956	6.708864
6.555529	461.288452	6.713869
6.416769	468.934410	6.718874
6.471518	455.589449	6.723878
6.254807	465.823188	6.728883
6.451727	452.789674	6.733888
6.185937	463.350858	6.738893
6.391774	458.507237	6.743898
5.981779	451.097413	6.748902
6.130287	460.037696	6.753907
6.239209	460.347208	6.758912
6.220576	444.581707	6.763917
5.958893	439.347126	6.768922
6.034015	448.108777	6.773926
5.876389	456.895501	6.778931
6.435503	458.321105	6.783936
6.307458	469.516129	6.788941
6.363551	464.347717	6.793946
6.376681	447.366086	6.798950
5.859344	448.464043	6.803955
6.145393	443.029693	6.808960
6.164317	452.373945	6.813965
6.225831	456.861418	6.818970
6.011414	457.556194	6.823974
5.874570	461.661050	6.828979
5.908974	457.761952	6.833984
5.944704	463.979210	6.838989
5.955758	461.951768	6.843994
6.344785	463.239683	6.848998
6.152022	464.313887	6.854003
6.379518	457.288088	6.859008
6.346150	470.869536	6.864013
6.290199	461.227611	6.869018
6.460313	466.151302	6.874022
6.279937	468.241895	6.879027
6.278314	462.765958	6.884032
5.766737	469.176206	6.889037
6.206493	463.807669	6.894042
6.268035	461.231927	6.899046
5.961628	466.959039	6.904051
6.162707	457.835025	6.909056
6.035963	476.633354	6.914061
6.040610	468.038872	6.919066
5.784608	467.918856	6.924070
5.760111	473.165965	6.929075
5.809532	469.489922	6.934080
5.668434	468.870692	6.939085
6.039869	467.773580	6.944090
6.086999	462.781891	6.949094
6.128497	470.151419	6.954099
6.335004	475.142671	6.959104
5.892205	467.972330	6.964109
6.119996	472.944454	6.969114
6.214662	478.898741	6.974118
6.096880	487.628540	6.979123
6.323861	482.978733	6.984128
6.050891	489.739858	6.989133
6.261260	483.134060	6.994138
6.273606	482.659233	6.999142
6.242025	477.897296	7.004147
6.394573	459.655384	7.009152
6.153265	465.991900	7.014157
6.053167	460.054189	7.019162
6.204869	455.538262	7.024166
6.191144	464.887948	7.029171
6.260335	462.529976	7.034176
6.129797	468.568656	7.039181
6.151320	466.315103	7.044186
6.487809	465.832381	7.049190
6.394364	466.407594	7.054195
6.424418	461.440056	7.059200
6.131547	474.102038	7.064205
6.211353	460.447432	7.069210
6.332578	455.838891	7.074214
6.645444	471.682466	7.079219
6.396019	460.958543	7.084224
6.011879	467.347018	7.089229
5.970735	472.925456	7.094234
6.303474	465.040132	7.099238
6.112690	471.412061	7.104243
6.174737	462.646819	7.109248
6.335481	474.747766	7.114253
6.056949	465.364243	7.119258
5.869115	464.714103	7.124262
6.116102	468.365034	7.129267
6.394506	465.898684	7.134272
5.932480	470.629071	7.139277
5.888353	467.324372	7.144282
6.306378	469.033318	7.149286
6.181115	461.335218	7.154291
6.133681	468.465161	7.159296
5.881379	470.717881	7.164301
6.318555	469.894991	7.169306
6.358748	466.159506	7.174310
6.625728	470.472331	7.179315
6.739887	462.847707	7.184320
6.484290	467.219563	7.189325
6.183198	448.617346	7.194330
6.168884	439.073891	7.199334
5.537417	434.712411	7.204339
6.167510	445.387530	7.209344
6.293763	461.880164	7.214349
6.215924	470.721321	7.219354
6.129196	463.035168	7.224358
5.837606	466.735357	7.229363
6.527360	469.668398	7.234368
6.359844	470.463716	7.239373
6.406138	455.249818	7.244378
6.134529	446.864854	7.249382
5.676535	440.381606	7.254387
6.204864	453.984334	7.259392
6.167476	472.381424	7.264397
6.034328	471.524071	7.269402
6.302588	469.428817	7.274406
6.280737	471.624882	7.279411
6.407475	457.385471	7.284416
6.356342	465.334771	7.289421
6.212921	443.982933	7.294426
6.169674	438.067552	7.299430
5.468564	441.577291	7.304435
6.283634	451.208356	7.309440
6.396031	465.080519	7.314445
6.262447	475.095812	7.319450
6.395289	467.565565	7.324454
6.078851	447.961661	7.329459
5.890573	440.645035	7.334464
6.122676	459.188734	7.339469
5.855261	465.511433	7.344474
5.932163	468.703019	7.349478
5.881035	468.985260	7.354483
5.996335	465.056138	7.359488
6.082564	471.346703	7.364493
6.129486	474.967740	7.369498
6.300382	470.409547	7.374502
6.001894	479.137012	7.379507
6.607164	467.430973	7.384512
6.174893	471.753852	7.389517
6.141869	477.155906	7.394522
6.107533	469.546290	7.399526
5.915249	462.873829	7.404531
6.390891	469.188865	7.409536
6.091003	468.867758	7.414541
6.130131	468.660210	7.419546
5.742526	470.407546	7.424550
5.673799	471.827192	7.429555
5.986015	462.805670	7.434560
5.973973	458.754055	7.439565
6.016338	470.236690	7.444570
6.313243	463.353470	7.449574
5.944471	464.966053	7.454579
6.268187	471.071118	7.459584
6.216806	472.055322	7.464589
6.372508	478.073860	7.469594
6.531561	459.868361	7.474598
6.321848	477.688873	7.479603
6.480355	464.777766	7.484608
6.439670	472.533523	7.489613
6.090310	466.114300	7.494618
6.468986	462.343476	7.499622
6.126171	468.982802	7.504627
6.443509	468.158321	7.509632
6.276073	463.407720	7.514637
6.134552	469.492428	7.519642
6.156155	466.480899	7.524646
5.966461	475.030635	7.529651
6.264033	464.903311	7.534656
6.284596	467.933960	7.539661
5.941324	471.118815	7.544666
6.332619	466.097353	7.549670
5.987826	465.205123	7.554675
6.473286	464.303168	7.559680
6.182168	471.117424	7.564685
6.353152	466.745502	7.569690
6.331196	460.802893	7.574694
5.929813	468.427183	7.579699
6.188079	459.135401	7.584704
6.131799	471.372662	7.589709
6.212180	466.101940	7.594714
6.219549	472.209855	7.599718
5.894322	464.647998	7.604723
6.276435	464.604657	7.609728
6.073938	460.323227	7.614733
6.320941	468.417549	7.619738
6.135845	470.000393	7.624742
5.992671	480.823595	7.629747
6.411966	458.589264	7.634752
6.121434	469.940549	7.639757
6.251934	468.509926	7.644762
6.182992	471.212286	7.649766
6.077856	478.332682	7.654771
6.332797	468.974155	7.659776
6.280756	472.554611	7.664781
6.080693	473.201614	7.669786
6.478440	465.106374	7.674790
5.970337	474.231378	7.679795
6.515640	451.906059	7.684800
6.013319	457.696514	7.689805
5.601625	442.968415	7.694810
6.231302	455.551444	7.699814
6.086359	466.502803	7.704819
6.366263	463.359936	7.709824
5.882221	476.874608	7.714829
6.031292	466.773149	7.719834
6.628949	471.070086	7.724838
6.324732	466.775763	7.729843
6.235760	469.510658	7.734848
6.185653	473.670562	7.739853
5.983767	477.398271	7.744858
5.927748	468.497544	7.749862
6.192767	466.845255	7.754867
6.235821	472.497513	7.759872
6.406792	467.507933	7.764877
6.076911	469.548979	7.769882
6.255059	461.343225	7.774886
6.198106	468.537306	7.779891
6.287748	465.828033	7.784896
6.200557	462.672574	7.789901
5.768378	459.836515	7.794906
6.089027	461.333722	7.799910
5.987711	473.196824	7.804915
6.290816	462.662861	7.809920
6.212421	466.603293	7.814925
6.239931	468.044437	7.819930
6.025149	472.164617	7.824934
5.660830	472.136803	7.829939
6.113494	463.803330	7.834944
6.442584	467.510471	7.839949
6.052327	468.488641	7.844954
5.940755	469.405099	7.849958
6.142295	482.238883	7.854963
6.289201	469.674051	7.859968
6.221013	468.998500	7.864973
6.063182	477.776785	7.869978
6.331912	470.184484	7.874982
6.156042	474.063566	7.879987
6.346473	467.351568	7.884992
6.733904	467.867774	7.889997
6.396171	471.594775	7.895002
5.994681	452.574708	7.900006
5.804338	458.598460	7.905011
6.479520	456.165226	7.910016
6.005718	461.505754	7.915021
5.830213	469.618993	7.920026
6.011157	463.239504	7.925030
6.153033	473.930865	7.930035
6.340561	461.087558	7.935040
6.343178	466.418366	7.940045
6.175775	470.233287	7.945050
6.471166	463.409717	7.950054
6.018351	467.586627	7.955059
6.071777	469.011229	7.960064
6.254530	472.656458	7.965069
6.242145	474.230923	7.970074
6.248521	468.121985	7.975078
6.180607	477.563171	7.980083
6.253473	476.337883	7.985088
6.061026	488.102872	7.990093
5.926512	478.466298	7.995098
6.167580	476.404769	8.000102
6.082248	479.687257	8.005107
6.094727	471.351165	8.010112
5.964120	477.830774	8.015130
6.225166	477.677594	8.020147
6.078189	480.149470	8.025165
6.034535	474.717514	8.030182
6.249284	478.505910	8.035200
6.499647	475.762427	8.040218
6.428828	478.704473	8.045235
6.194495	473.480177	8.050253
6.285696	482.394925	8.055270
6.290672	480.947227	8.060288
6.268763	471.215410	8.065306
5.972172	479.474599	8.070323
6.416257	469.681669	8.075341
6.085727	476.525373	8.080358
5.936086	478.259177	8.085376
6.109060	474.679622	8.090394
6.219576	478.839048	8.095411
6.351468	463.341665	8.100429
6.025421	477.079637	8.105446
6.438856	473.938220	8.110464
6.026347	474.490437	8.115482
6.271311	479.925623	8.120499
6.346162	469.368353	8.125517
6.202081	470.954200	8.130534
6.302794	475.323306	8.135552
6.380345	467.042735	8.140570
6.247814	476.273773	8.145587
6.543108	470.384537	8.150605
6.216174	475.598663	8.155622
6.561015	468.484773	8.160640
6.352491	475.085384	8.165658
5.966014	478.209015	8.170675
6.050742	467.011583	8.175693
6.439805	469.922856	8.180710
6.279862	467.530615	8.185728
6.267007	472.409297	8.190746
6.005125	473.914339	8.195763
6.327319	465.463593	8.200781
6.075105	470.144875	8.205798
5.940675	466.975041	8.210816
6.157499	466.663873	8.215834
6.200335	482.334444	8.220851
6.721385	492.479601	8.225869
6.247371	496.777716	8.230886
6.328836	494.979933	8.235904
6.333957	495.858173	8.240922
6.539983	503.314613	8.245939
6.330250	494.876874	8.250957
6.352080	497.492726	8.255974
6.191096	494.769385	8.260992
6.875348	493.500687	8.266010
6.264428	501.834964	8.271027
6.793006	496.755882	8.276045
6.511058	490.784841	8.281062
6.326240	483.111400	8.286080
6.526030	469.777323	8.291098
6.130632	483.872859	8.296115
6.649522	490.605898	8.301133
6.318287	497.243251	8.306150
6.181694	492.575880	8.311168
6.528571	486.514891	8.316186
6.582916	499.707422	8.321203
7.028193	491.931415	8.326221
6.581201	489.342217	8.331238
6.454099	480.798635	8.336256
6.670062	473.518188	8.341274
6.509595	474.147007	8.346291
6.451317	471.773691	8.351309
6.431901	474.179683	8.356326
6.562736	473.335220	8.361344
6.560146	469.026256	8.366362
6.221258	473.892401	8.371379
6.493841	483.315141	8.376397
6.691973	493.820633	8.381414
6.464142	487.658726	8.386432
6.739338	488.985339	8.391450
6.696133	488.284751	8.396467
6.459849	472.965666	8.401485
6.405519	481.481807	8.406502
6.429748	492.240984	8.411520
6.674781	493.752909	8.416538
6.437216	494.381355	8.421555
6.740576	485.821140	8.426573
6.839383	488.622603	8.431590
6.356600	483.924593	8.436608
6.551523	491.334845	8.441626
6.433537	496.669746	8.446643
6.807536	494.078333	8.451661
6.646204	496.017607	8.456678
6.401761	490.196617	8.461696
6.503905	488.580224	8.466714
6.283383	494.260876	8.471731
6.381632	492.495930	8.476749
6.725555	487.410735	8.481766
6.541431	492.689705	8.486784
6.659045	491.824606	8.491802
6.356550	499.161054	8.496819
6.694065	495.826562	8.501837
6.797977	492.484838	8.506854
6.453649	498.271101	8.511872
6.579612	490.802474	8.516890
6.155525	507.939917	8.521907
6.115833	506.372486	8.526925
6.845408	523.011339	8.531942
7.334712	522.055527	8.536960
7.139447	508.883132	8.541978
6.633681	505.584082	8.546995
6.548820	504.974464	8.552013
6.487509	497.330287	8.557030
6.489547	494.921747	8.562048
7.059855	510.966053	8.567066
6.562261	511.200357	8.572083
6.409589	516.253065	8.577101
6.488761	518.566307	8.582119
6.592450	524.475539	8.587136
7.012418	522.897057	8.592154
6.569239	534.266184	8.597171
6.849725	528.533114	8.602189
6.901139	527.706179	8.607207
6.666211	538.980072	8.612224
6.914723	527.581571	8.617242
6.681534	541.313221	8.622259
6.755221	524.882425	8.627277
6.866389	529.963129	8.632295
6.672204	530.751674	8.637312
6.495616	530.660602	8.642330
6.617881	526.885544	8.647347
6.541417	530.105087	8.652365
7.086886	530.628190	8.657383
6.961963	536.606720	8.662400
7.150613	525.193763	8.667418
7.172059	530.620649	8.672435
7.222895	525.893377	8.677453
6.937607	528.165631	8.682471
7.067227	532.982270	8.687488
7.029725	528.412974	8.692506
7.012341	535.061756	8.697523
7.319475	521.739122	8.702541
7.200112	521.840293	8.707559
6.816618	511.847514	8.712576
6.748729	502.711455	8.717594
6.906298	507.831876	8.722611
6.928045	505.801127	8.727629
6.694854	507.440760	8.732647
6.718456	520.423084	8.737664
7.025489	528.260939	8.742682
6.678159	530.001231	8.747699
7.028033	527.358119	8.752717
6.953225	522.019703	8.757735
6.830589	531.536503	8.762752
7.260645	532.816714	8.767770
7.089791	532.949275	8.772787
6.833595	536.660067	8.777805
7.025970	532.016347	8.782823
6.922004	533.615412	8.787840
7.186268	528.272011	8.792858
7.156306	531.059652	8.797875
7.006340	530.419126	8.802893
7.085934	523.818151	8.807911
7.147781	528.827730	8.812928
7.176859	525.236649	8.817946
6.761284	533.614059	8.822963
6.894856	529.576711	8.827981
7.012469	525.848683	8.832999
6.853730	525.450341	8.838016
7.017679	524.407477	8.843034
6.966492	534.526127	8.848051
6.604142	530.694225	8.853069
7.018349	528.614581	8.858087
7.248520	534.502204	8.863104
7.100197	532.645767	8.868122
7.107683	531.531869	8.873139
7.368472	525.725112	8.878157
7.415228	528.453942	8.883175
7.214076	536.614629	8.888192
7.252429	524.701503	8.893210
6.924644	534.385658	8.898227
6.979985	532.381799	8.903245
7.009544	520.105998	8.908263
7.104207	535.234593	8.913280
7.331869	527.736645	8.918298
6.938924	531.108780	8.923315
7.140069	531.638723	8.928333
7.109299	526.737630	8.933351
6.956282	533.266645	8.938368
7.211473	522.890369	8.943386
6.867422	527.936310	8.948403
6.728521	522.627048	8.953421
6.985514	522.889071	8.958439
7.310849	536.418841	8.963456
7.534770	538.727712	8.968474
7.331090	539.578066	8.973491
6.921839	525.639326	8.978509
7.399665	530.934656	8.983527
7.116450	533.566966	8.988544
7.139150	531.364416	8.993562
7.158066	538.714976	8.998579
7.080897	550.641533	9.003597
7.189244	551.084547	9.008615
7.140272	569.625329	9.013632
7.452590	562.135930	9.018650
7.424899	563.391641	9.023667
7.160752	553.365615	9.028685
7.465748	554.425100	9.033703
7.372923	572.564549	9.038720
7.467081	561.085387	9.043738
7.411662	542.921265	9.048755
7.242046	534.813027	9.053773
7.352865	530.237975	9.058791
6.973635	529.381443	9.063808
7.227110	549.296212	9.068826
7.364587	551.758219	9.073843
7.231927	565.639309	9.078861
7.604677	561.122673	9.083879
7.522014	563.866130	9.088896
7.450348	558.860023	9.093914
7.621338	544.921472	9.098931
6.968000	546.221922	9.103949
7.509147	547.566340	9.108967
7.259697	551.558076	9.113984
7.387656	556.344882	9.119002
7.520543	554.302347	9.124019
7.272798	557.301370	9.129037
7.465166	550.758798	9.134055
7.470469	559.319593	9.139072
7.396958	556.471870	9.144090
7.673026	561.892467	9.149107
7.358808	562.478739	9.154125
7.887650	552.547469	9.159143
7.240650	550.929214	9.164160
7.247044	530.780403	9.169178
7.522219	540.417492	9.174195
7.224373	556.940556	9.179213
7.809825	567.549819	9.184231
7.515008	564.840442	9.189248
7.709220	556.779193	9.194266
7.511152	549.125242	9.199283
7.270534	543.236279	9.204301
7.572200	542.974979	9.209319
7.471929	555.845846	9.214336
7.550757	554.542348	9.219354
7.750120	541.858813	9.224371
7.468180	542.557623	9.229389
7.489112	533.166056	9.234407
7.460799	548.734751	9.239424
7.498884	546.139717	9.244442
7.918082	555.917430	9.249459
7.564375	548.216519	9.254477
7.661527	536.976620	9.259495
7.615098	536.702906	9.264512
7.354045	532.810864	9.269530
7.376874	546.009854	9.274547
7.473492	548.946325	9.279565
7.876552	560.257885	9.284583
7.507740	562.393054	9.289600
7.664298	554.724841	9.294618
7.600579	559.003594	9.299635
7.580792	563.244341	9.304653
7.531798	558.263401	9.309671
7.633110	564.910773	9.314688
7.674626	558.390712	9.319706
7.248492	561.755772	9.324723
7.333951	562.183301	9.329741
7.424333	541.782743	9.334759
7.568664	564.735085	9.339776
7.415102	562.539585	9.344794
7.606904	558.445902	9.349811
7.434382	564.925421	9.354829
7.583360	558.873479	9.359847
7.418538	561.008206	9.364864
7.529588	579.000795	9.369882
8.017965	587.091980	9.374899
7.864784	593.550974	9.379917
7.875127	575.375490	9.384935
7.875652	566.983861	9.389952
8.034278	568.596367	9.394970
7.745532	552.550554	9.399987
7.388468	564.261658	9.405005
7.905431	550.685246	9.410023
7.653998	562.773244	9.415040
7.942050	566.906140	9.420058
7.831638	558.218414	9.425075
7.598859	566.870157	9.430093
7.524411	555.257424	9.435111
7.922242	575.446041	9.440128
7.581430	591.816259	9.445146
7.977328	591.697747	9.450163
7.795965	602.342168	9.455181
7.975307	598.030487	9.460199
7.973100	593.777325	9.465216
7.720549	585.597615	9.470234
7.805831	576.744295	9.475251
7.541200	593.551222	9.480269
7.872864	590.808970	9.485287
8.301514	598.044218	9.490304
7.810489	589.275062	9.495322
8.064628	590.999638	9.500339
7.765039	592.017891	9.505357
8.099307	587.878477	9.510375
7.990306	587.875375	9.515392
7.679882	582.393241	9.520410
7.847552	583.988893	9.525427
7.750744	583.017904	9.530445
7.888272	592.723568	9.535463
8.049332	594.149074	9.540480
8.111338	599.235611	9.545498
8.571053	589.643337	9.550515
7.904115	585.443381	9.555533
7.809577	573.712330	9.560551
7.851524	568.130693	9.565568
8.008659	588.552820	9.570586
7.936646	588.211119	9.575603
7.767867	596.021605	9.580621
8.315725	593.249324	9.585639
8.143212	599.076746	9.590656
7.992502	589.058022	9.595674
8.108812	589.851455	9.600691
7.882086	594.106921	9.605709
8.025209	598.199942	9.610727
8.266157	602.084792	9.615744
7.997915	603.672786	9.620762
8.160676	596.791248	9.625779
7.976015	597.152266	9.630797
7.970743	585.131000	9.635815
7.909166	603.033814	9.640832
7.809475	609.296343	9.645850
8.013064	596.575450	9.650867
8.113490	600.109672	9.655885
7.872673	594.202417	9.660903
7.941627	595.128317	9.665920
8.186944	601.942305	9.670938
8.334748	583.982920	9.675955
7.975312	591.646564	9.680973
8.216609	593.412641	9.685991
8.313036	592.819145	9.691008
8.094937	601.509803	9.696026
8.338905	594.771054	9.701043
8.189346	595.423063	9.706061
8.026812	595.680018	9.711079
7.920182	590.175228	9.716096
7.988579	595.445724	9.721114
8.043342	594.000763	9.726131
8.063158	592.666522	9.731149
7.895078	599.418324	9.736167
8.344062	597.488783	9.741184
8.071271	599.284404	9.746202
8.038415	595.315249	9.751219
8.152661	601.145203	9.756237
8.238192	604.966917	9.761255
8.316328	608.850485	9.766272
8.482822	617.003648	9.771290
8.071375	608.298415	9.776307
8.079189	605.414333	9.781325
8.060709	613.723424	9.786343
8.405476	614.366101	9.791360
8.261398	625.492292	9.796378
8.503808	619.841888	9.801395
8.335452	622.236637	9.806413
8.751865	623.505345	9.811431
8.644478	614.370273	9.816448
8.130456	600.656932	9.821466
8.277150	597.110848	9.826483
8.277028	600.204341	9.831501
8.371664	593.730747	9.836519
8.391788	597.659187	9.841536
8.575364	595.209240	9.846554
8.419498	600.960674	9.851571
8.022977	590.967057	9.856589
8.261086	608.066000	9.861607
8.350119	609.762512	9.866624
8.363683	627.450916	9.871642
8.535588	619.447667	9.876659
8.643942	625.929736	9.881677
8.231045	619.421795	9.886695
8.383665	620.903033	9.891712
8.154465	620.630564	9.896730
8.217556	616.753124	9.901747
8.487983	630.084837	9.906765
8.468994	627.069194	9.911783
8.504702	628.394682	9.916800
8.563460	631.400842	9.921818
8.509684	620.613097	9.926835
8.515123	623.237797	9.931853
8.298400	623.477186	9.936871
8.361401	624.511155	9.941888
8.215710	629.487352	9.946906
8.042563	633.411313	9.951923
8.442610	629.555615	9.956941
8.305211	628.334896	9.961959
8.277373	625.038661	9.966976
8.453391	637.859542	9.971994
8.811753	645.280102	9.977011
8.620334	643.147767	9.982029
8.466386	638.034258	9.987047
8.728039	631.875970	9.992064
8.618895	632.407099	9.997082
8.945885	621.152558	10.002099
8.564762	625.068371	10.007117
8.325753	621.514346	10.012135
8.573932	619.855362	10.017152
8.523555	639.888263	10.022170
8.663566	643.922566	10.027187
8.534748	662.166519	10.032205
8.612024	660.987473	10.037223
9.187728	655.180685	10.042240
8.683231	644.220219	10.047258
8.846195	635.440364	10.052275
8.494409	621.327040	10.057293
7.994508	628.552276	10.062311
8.478855	641.477806	10.067328
8.510683	656.639403	10.072346
9.071036	655.947934	10.077363
8.906797	661.651967	10.082381
8.957525	666.321143	10.087399
9.121614	658.702410	10.092416
8.740793	651.655703	10.097434
8.952322	634.863326	10.102451
8.701463	626.981516	10.107469
8.283419	633.046003	10.112487
8.565725	641.429909	10.117504
8.699023	660.411135	10.122522
8.517888	661.159135	10.127539
9.024749	660.346645	10.132557
8.793492	663.190007	10.137575
8.980608	662.379878	10.142592
8.811964	664.572926	10.147610
8.655736	665.459884	10.152627
8.696359	662.203637	10.157645
8.800949	660.065208	10.162663
9.138942	658.241107	10.167680
8.777746	661.248180	10.172698
9.072124	657.710014	10.177715
9.098526	666.451205	10.182733
8.824557	663.662957	10.187751
8.875843	656.027150	10.192768
9.019158	657.602647	10.197786
9.120835	662.105887	10.202803
8.990537	652.352407	10.207821
9.169281	661.363723	10.212839
9.061388	637.716145	10.217856
8.922232	631.836070	10.222874
9.139665	632.200725	10.227891
9.002287	626.171747	10.232909
8.755009	631.962399	10.237927
9.144693	618.346065	10.242944
8.784185	624.766112	10.247962
8.656598	626.821043	10.252979
8.984467	635.881174	10.257997
9.175303	656.808770	10.263015
9.202141	651.202058	10.268032
8.901090	649.340876	10.273050
9.194016	648.957612	10.278067
9.142950	625.151408	10.283085
8.588805	623.207896	10.288103
8.780447	654.373465	10.293120
8.902103	659.162532	10.298138
8.830719	663.278034	10.303155
9.017147	662.554232	10.308173
9.110516	663.094613	10.313191
9.136614	666.884885	10.318208
9.187872	665.658002	10.323226
9.351282	661.295806	10.328243
9.393764	662.544390	10.333261
9.247831	666.613037	10.338279
8.939010	660.926293	10.343296
9.170335	663.797488	10.348314
9.376731	658.921104	10.353331
9.161188	666.920485	10.358349
8.933036	668.559101	10.363367
9.217503	661.257733	10.368384
9.049575	658.863836	10.373402
9.276696	659.828406	10.378419
9.242587	654.893579	10.383437
8.753949	665.740282	10.388455
9.090635	662.713544	10.393472
9.181181	663.393557	10.398490
9.100268	658.708810	10.403507
9.418637	661.474600	10.408525
9.254814	661.135756	10.413543
9.408079	658.458376	10.418560
9.236698	667.027141	10.423578
8.900732	662.044262	10.428595
9.377758	658.374369	10.433613
9.517497	663.140945	10.438631
9.593261	654.704482	10.443648
9.298277	656.382746	10.448666
9.368250	656.401861	10.453683
9.427289	651.025211	10.458701
9.334817	661.627145	10.463719
9.370910	658.549392	10.468736
8.908693	657.055912	10.473754
9.351961	663.154406	10.478771
9.609608	660.840355	10.483789
9.006977	663.922002	10.488807
9.110158	668.374407	10.493824
9.419779	665.295675	10.498842
9.594515	662.236214	10.503859
9.328261	668.447716	10.508877
9.121233	660.679460	10.513895
9.445857	657.469704	10.518912
9.134879	658.551856	10.523930
9.035587	668.665402	10.528947
9.355963	661.386410	10.533965
9.228832	659.885264	10.538983
9.516567	671.823503	10.544000
9.440956	679.477219	10.549018
9.488796	684.385050	10.554035
9.528220	671.485099	10.559053
9.204070	680.748893	10.564071
9.403238	679.184852	10.569088
9.598473	689.629153	10.574106
9.579284	692.645131	10.579123
9.833719	686.603957	10.584141
9.391447	697.860266	10.589159
9.692710	687.391781	10.594176
9.673384	683.613055	10.599194
9.490588	679.874098	10.604211
9.961887	681.063615	10.609229
9.479696	677.682465	10.614247
9.802775	667.900862	10.619264
9.680357	668.172015	10.624282
9.541155	672.863116	10.629299
9.381966	661.685218	10.634317
9.348165	662.967542	10.639335
9.643861	664.754505	10.644352
9.835424	667.074481	10.649370
9.386777	673.984749	10.654387
9.636954	679.486457	10.659405
9.280187	683.738563	10.664423
9.716937	691.757682	10.669440
9.633988	693.978417	10.674458
9.615710	696.250604	10.679475
10.116009	684.060003	10.684493
9.889691	693.421708	10.689511
9.630834	691.609212	10.694528
9.789893	695.431915	10.699546
9.703079	689.501783	10.704563
9.763824	682.177358	10.709581
9.697332	693.521392	10.714599
9.749408	687.873073	10.719616
9.968736	681.229321	10.724634
9.653618	692.084995	10.729651
9.945290	685.326666	10.734669
9.842105	672.371682	10.739687
9.185169	676.247136	10.744704
9.431818	686.457317	10.749722
9.255028	692.079006	10.754739
9.552778	688.524919	10.759757
9.741648	685.377284	10.764775
9.676760	693.017611	10.769792
9.840290	681.153239	10.774810
9.589000	694.613055	10.779827
9.859885	691.021507	10.784845
9.861839	688.104134	10.789863
9.763161	692.191703	10.794880
9.773083	695.028055	10.799898
9.683389	700.782699	10.804915
10.185472	704.033079	10.809933
9.766020	701.721134	10.814951
9.705343	712.847894	10.819968
9.843309	719.664227	10.824986
9.955008	729.673853	10.830003
9.952753	719.446132	10.835021
10.159811	718.980493	10.840039
10.180972	721.657513	10.845056
10.449445	718.857242	10.850074
9.856645	703.219654	10.855091
9.784197	695.895511	10.860109
10.085445	697.228639	10.865127
9.905652	690.847659	10.870144
9.995691	698.661829	10.875162
9.754188	717.026339	10.880179
10.128475	715.282413	10.885197
10.136992	728.203840	10.890215
9.739978	727.864189	10.895232
10.172791	723.069041	10.900250
9.846928	732.061124	10.905267
10.518842	723.726903	10.910285
10.472246	722.432427	10.915303
10.289930	714.144330	10.920320
10.270646	693.430132	10.925338
9.915856	693.730065	10.930355
10.193451	679.336308	10.935373
10.025038	696.455478	10.940391
9.868952	692.353248	10.945408
9.899661	708.255573	10.950426
9.801466	716.704927	10.955443
9.902275	721.888196	10.960461
10.135931	716.773029	10.965479
9.876755	720.852441	10.970496
10.289804	720.220882	10.975514
9.951995	722.803247	10.980531
10.329159	714.791620	10.985549
10.209545	729.591481	10.990567
10.139062	713.242514	10.995584
10.132034	717.568380	11.000602
10.218828	715.974591	11.005619
10.141715	719.856040	11.010637
10.054847	708.915478	11.015655
10.280588	719.931061	11.020672
10.184911	729.021882	11.025690
10.184842	732.989340	11.030707
10.422891	736.497571	11.035725
10.604140	735.984059	11.040743
10.034907	732.384113	11.045760
10.480661	726.127479	11.050778
10.161235	728.866225	11.055795
10.385790	748.682522	11.060813
10.353314	749.866609	11.065831
10.451152	755.095458	11.070848
10.663554	735.074138	11.075866
10.284900	725.693360	11.080883
10.282474	725.275135	11.085901
10.293808	730.426431	11.090919
10.486770	746.544526	11.095936
10.655845	742.195735	11.100954
10.525125	732.761935	11.105971
10.159531	727.149165	11.110989
10.600045	729.468125	11.116007
10.380357	748.200277	11.121024
10.615529	742.700037	11.126042
10.494369	752.839711	11.131059
10.472028	743.442808	11.136077
10.580488	740.853564	11.141095
10.253334	741.296727	11.146112
10.279226	746.036783	11.151130
10.466233	743.802564	11.156147
10.543934	753.439735	11.161165
10.798415	746.374790	11.166183
10.474804	759.593355	11.171200
11.007724	740.952308	11.176218
10.741426	756.776104	11.181235
10.631465	734.669155	11.186253
10.704136	724.236080	11.191271
10.241986	724.862888	11.196288
10.657088	735.764733	11.201306
10.419425	735.896589	11.206323
10.427971	752.275244	11.211341
10.942545	758.248745	11.216359
10.456048	747.381662	11.221376
10.899838	743.783016	11.226394
10.338098	752.702120	11.231411
10.567687	746.746738	11.236429
10.616611	741.735095	11.241447
10.379966	752.419907	11.246464
10.880165	749.614185	11.251482
10.475678	743.087276	11.256499
10.552734	754.339587	11.261517
10.705225	748.379501	11.266535
10.400882	754.048394	11.271552
10.638346	747.620873	11.276570
10.551056	757.690753	11.281587
10.600968	749.910651	11.286605
10.788127	754.130439	11.291623
10.780379	755.408244	11.296640
11.059648	769.993237	11.301658
10.847654	757.333018	11.306675
10.786974	750.320648	11.311693
10.641206	756.365124	11.316711
10.795085	770.903444	11.321728
11.161282	773.781768	11.326746
11.064222	778.918421	11.331763
10.611877	758.959330	11.336781
11.276666	758.560318	11.341799
10.994441	759.681592	11.346816
10.862824	759.882824	11.351834
10.836540	761.553444	11.356851
10.660646	748.308733	11.361869
11.073042	753.444162	11.366887
11.068352	762.185063	11.371904
11.001304	756.545101	11.376922
10.970305	747.852731	11.381939
10.735439	751.702144	11.386957
11.203287	758.763840	11.391975
10.767179	759.720351	11.396992
10.870071	758.883076	11.402010
11.159480	774.657046	11.407027
11.292631	769.353463	11.412045
11.275413	757.605288	11.417063
11.096718	759.426230	11.422080
11.195341	752.007687	11.427098
10.993541	746.500354	11.432115
10.948744	751.710786	11.437133
11.372202	751.227287	11.442151
10.888675	753.684281	11.447168
11.066208	744.796833	11.452186
11.174357	744.908415	11.457203
11.210234	749.160432	11.462221
11.406288	741.496585	11.467239
11.164122	747.175809	11.472256
11.043314	745.323631	11.477274
11.202018	745.866737	11.482291
10.906933	736.870064	11.487309
11.074701	741.186765	11.492327
10.729430	753.799721	11.497344
10.925589	757.434398	11.502362
11.065309	775.919066	11.507379
10.961924	782.682044	11.512397
10.796660	773.385250	11.517415
10.848361	782.945861	11.522432
11.392885	777.919351	11.527450
11.565026	773.384031	11.532467
11.315344	770.397254	11.537485
11.390599	769.736213	11.542503
11.231555	779.342675	11.547520
11.589838	776.705801	11.552538
11.430151	776.147189	11.557555
11.344074	780.876929	11.562573
11.543528	769.334644	11.567591
11.009938	786.528780	11.572608
11.021915	780.201710	11.577626
11.060540	776.153113	11.582643
11.100191	779.462850	11.587661
11.507982	778.526083	11.592679
11.505083	780.097944	11.597696
11.346930	784.535357	11.602714
11.372145	781.705039	11.607731
11.050470	786.577475	11.612749
11.650296	775.747126	11.617767
11.302520	780.375885	11.622784
11.527392	789.845322	11.627802
11.263090	788.000848	11.632819
11.286152	804.031895	11.637837
11.792267	802.453634	11.642855
11.710129	810.127395	11.647872
11.462402	806.087804	11.652890
11.498093	793.116723	11.657907
11.300343	807.574554	11.662925
11.386230	806.083655	11.667943
11.353553	815.529580	11.672960
11.610531	806.275178	11.677978
11.952377	809.763615	11.682995
11.680008	810.592921	11.688013
11.884856	813.479174	11.693031
11.764193	799.309755	11.698048
11.913908	796.921306	11.703066
11.910126	777.230525	11.708083
11.548598	790.279841	11.713101
11.382759	771.031326	11.718119
11.371655	776.121018	11.723136
11.368367	782.101077	11.728154
11.585218	799.903517	11.733171
11.708417	807.450636	11.738189
11.787753	808.247273	11.743207
11.765728	805.692105	11.748224
11.897144	797.606919	11.753242
11.902853	802.368848	11.758259
11.749973	804.864982	11.763277
12.132445	796.774287	11.768295
11.627921	790.933619	11.773312
11.359648	786.512043	11.778330
11.608668	787.405271	11.783347
12.008839	801.835367	11.788365
12.068857	802.616121	11.793383
11.986186	799.957657	11.798400
11.968142	780.548552	11.803418
12.195237	775.509451	11.808435
11.631502	775.349465	11.813453
11.816062	767.593427	11.818471
11.529141	768.189145	11.823488
12.055888	778.641395	11.828506
11.706149	766.508748	11.833523
11.739051	790.229101	11.838541
11.928928	782.693810	11.843559
11.979909	800.350603	11.848576
12.004818	798.939913	11.853594
11.962537	792.699410	11.858611
11.710315	800.562840	11.863629
12.002369	803.098598	11.868647
11.877974	809.227331	11.873664
11.678536	807.780114	11.878682
11.700586	802.743196	11.883699
11.816205	807.452807	11.888717
12.153935	805.400404	11.893735
12.140135	802.478935	11.898752
12.082931	795.612217	11.903770
12.311710	790.568304	11.908787
11.905143	807.877561	11.913805
12.179643	794.039684	11.918823
12.236377	796.931655	11.923840
12.090862	802.273599	11.928858
11.954434	793.528456	11.933875
12.199772	805.095330	11.938893
12.308991	801.039520	11.943911
12.451280	798.762337	11.948928
12.158428	805.477686	11.953946
12.143624	793.573582	11.958963
12.370146	795.133295	11.963981
12.094024	798.464812	11.968999
12.176954	794.769647	11.974016
11.997857	796.242654	11.979034
12.154632	795.254897	11.984051
12.117826	799.179663	11.989069
12.270094	791.649437	11.994087
12.248559	795.991712	11.999104
12.209122	802.630692	12.004122
12.608157	795.865691	12.009139
12.158249	810.086123	12.014157
12.149886	801.792096	12.019175
12.270991	800.418564	12.024192
12.345174	797.880476	12.029210
12.226601	789.775823	12.034227
11.823788	805.534766	12.039245
11.902553	801.147429	12.044263
11.816310	809.312584	12.049280
12.454351	822.391450	12.054298
12.709503	822.271922	12.059315
12.374193	829.017368	12.064333
12.630419	829.498997	12.069351
12.123788	816.663699	12.074368
12.256413	824.254729	12.079386
12.646695	831.070905	12.084403
12.545510	827.496287	12.089421
12.728091	835.155195	12.094439
12.497724	817.223947	12.099456
12.327134	828.407441	12.104474
12.533398	821.828787	12.109491
12.819941	843.858563	12.114509
12.747118	813.544730	12.119527
12.236055	797.237603	12.124544
12.126220	817.910098	12.129562
12.649398	816.266406	12.134579
12.538758	833.383211	12.139597
12.350148	833.990542	12.144615
12.619529	834.913850	12.149632
12.892219	839.735151	12.154650
13.136912	830.316646	12.159667
12.679316	814.485816	12.164685
12.339361	806.942124	12.169703
12.749559	813.822693	12.174720
12.503698	824.778555	12.179738
12.489366	825.847435	12.184755
12.736333	831.763875	12.189773
12.603231	831.348076	12.194791
12.782167	827.022424	12.199808
12.468724	835.332630	12.204826
12.626700	824.565844	12.209843
12.433700	834.054370	12.214861
12.495643	827.461514	12.219879
13.070352	830.184337	12.224896
12.575424	838.449123	12.229914
12.649739	827.753322	12.234931
12.723468	840.546690	12.239949
12.826162	836.191978	12.244967
12.878315	832.973342	12.249984
12.569706	834.596215	12.255002
12.718023	830.825218	12.260019
12.660441	838.536641	12.265037
12.804859	831.124622	12.270055
12.625941	833.280231	12.275072
12.591782	838.287363	12.280090
12.847444	848.218615	12.285107
12.866371	858.101627	12.290125
13.003626	860.587144	12.295143
13.710426	854.801209	12.300160
12.941918	847.216724	12.305178
13.157010	832.674366	12.310195
13.172620	824.981811	12.315213
12.932709	829.787525	12.320231
12.963349	824.149609	12.325248
12.836133	832.958942	12.330266
13.206682	828.931340	12.335283
13.167318	827.182339	12.340301
13.033256	834.906275	12.345319
13.100014	827.066842	12.350336
12.790292	826.236532	12.355354
13.015899	830.775912	12.360371
13.039192	836.907470	12.365389
12.916029	832.253903	12.370407
13.095602	839.377918	12.375424
13.273094	851.884188	12.380442
13.558207	851.254007	12.385459
13.255821	836.123685	12.390477
12.799905	838.118458	12.395495
13.013401	833.633527	12.400512
13.231097	855.252548	12.405530
13.330054	847.010340	12.410547
13.353089	856.716106	12.415565
13.367034	856.639030	12.420583
13.268465	837.322957	12.425600
12.773921	842.775283	12.430618
13.352210	845.488459	12.435635
13.168178	843.613708	12.440653
13.264788	861.529308	12.445671
13.347480	854.693835	12.450688
13.273079	862.423026	12.455706
13.663909	852.495607	12.460723
13.447879	860.269397	12.465741
13.389845	865.481083	12.470759
13.452371	862.461884	12.475776
13.423237	860.492494	12.480794
13.583390	848.021118	12.485811
13.332846	836.468344	12.490829
13.427511	835.366113	12.495847
13.301854	819.849569	12.500864
13.502170	835.652384	12.505882
13.768810	836.909786	12.510899
13.554486	834.459011	12.515917
13.503359	827.614298	12.520935
13.407817	822.809894	12.525952
13.366043	826.622705	12.530970
13.394557	828.026960	12.535987
13.296576	826.919153	12.541005
13.298628	850.909273	12.546023
13.567498	846.241329	12.551040
13.690683	848.719144	12.556058
13.697057	845.789788	12.561075
13.495716	859.955962	12.566093
13.616912	854.942506	12.571111
13.924247	851.202747	12.576128
13.517461	861.516137	12.581146
13.673165	856.104256	12.586163
13.608018	849.173681	12.591181
13.598878	852.880098	12.596199
13.657389	848.305379	12.601216
13.505962	856.873295	12.606234
13.636671	859.409699	12.611251
13.772540	854.130044	12.616269
13.721379	854.021075	12.621287
13.748062	849.923070	12.626304
13.770348	863.310596	12.631322
13.832738	858.269907	12.636339
13.770844	850.866580	12.641357
13.589171	855.922643	12.646375
13.908513	852.451933	12.651392
13.521044	857.053258	12.656410
13.766178	856.518693	12.661427
13.877516	855.300705	12.666445
13.784096	857.785784	12.671463
13.751315	847.335509	12.676480
13.925568	857.109836	12.681498
13.886189	849.017973	12.686515
13.538656	847.860505	12.691533
13.342254	856.452430	12.696551
13.538958	848.761849	12.701568
13.729350	868.143458	12.706586
14.094916	882.172125	12.711603
14.202846	879.753997	12.716621
14.050885	882.125786	12.721639
14.304573	883.910506	12.726656
14.365266	867.117949	12.731674
13.680534	856.420144	12.736691
14.124539	847.416306	12.741709
13.822917	852.773584	12.746727
14.246971	855.535623	12.751744
13.890696	851.706173	12.756762
14.075657	873.905029	12.761779
13.963171	875.356737	12.766797
14.137733	891.984897	12.771815
14.255135	884.444280	12.776832
14.198870	885.066032	12.781850
14.095392	884.963790	12.786867
14.303784	868.160265	12.791885
14.203442	892.273366	12.796903
14.235544	876.783298	12.801920
14.155560	866.867788	12.806938
14.061341	864.515541	12.811955
14.305482	875.989366	12.816973
14.346540	880.988932	12.821991
14.149925	889.266168	12.827008
14.377758	884.706207	12.832026
13.854494	887.195414	12.837043
14.313977	880.204793	12.842061
14.463898	887.375882	12.847079
14.357989	882.044872	12.852096
14.483029	883.304160	12.857114
14.262187	879.586830	12.862131
14.114577	879.824578	12.867149
14.215386	882.145892	12.872167
14.214198	873.167020	12.877184
14.338363	881.163590	12.882202
14.350223	880.426276	12.887219
14.485902	880.527182	12.892237
14.209435	881.510509	12.897255
14.461400	878.585797	12.902272
14.474653	879.556402	12.907290
14.159206	884.851229	12.912307
14.460938	880.051837	12.917325
14.146072	879.052903	12.922343
14.481338	882.652482	12.927360
14.573305	879.908880	12.932378
14.412516	886.744825	12.937395
14.527880	882.929689	12.942413
14.456690	885.155583	12.947431
14.393680	873.713729	12.952448
14.346679	894.040866	12.957466
14.454661	915.416412	12.962483
14.681292	904.719059	12.967501
14.641531	918.533256	12.972519
14.681922	906.715948	12.977536
14.844633	912.334239	12.982554
14.835790	914.953685	12.987571
14.854002	897.907149	12.992589
14.896706	922.058722	12.997607
14.812967	898.414605	13.002624
14.840610	890.316502	13.007642
14.523058	882.882427	13.012659
14.736781	880.283734	13.017677
14.583057	901.243733	13.022695
14.892980	907.272565	13.027712
15.132482	905.087272	13.032730
14.730321	896.293329	13.037747
14.947381	883.864234	13.042765
14.683724	901.408094	13.047783
14.792925	901.201217	13.052800
14.901204	897.616570	13.057818
14.924450	903.502509	13.062835
14.818016	904.376874	13.067853
15.100798	905.054276	13.072871
14.903696	902.608893	13.077888
14.714870	903.539469	13.082906
15.236940	910.589862	13.087923
15.405242	895.641470	13.092941
14.893978	885.037837	13.097959
14.693997	878.995938	13.102976
15.000275	901.689400	13.107994
14.735971	907.160368	13.113011
14.967024	914.593951	13.118029
14.867646	906.368731	13.123047
14.726592	915.134351	13.128064
15.066631	901.953551	13.133082
14.927739	904.577289	13.138099
15.292562	901.593267	13.143117
14.930368	908.001703	13.148135
14.912661	897.949846	13.153152
15.113538	897.308666	13.158170
14.697954	901.531632	13.163187
15.358054	895.846745	13.168205
15.286480	906.293414	13.173223
15.229754	906.975278	13.178240
15.426371	895.282397	13.183258
15.035157	907.461607	13.188275
15.388273	897.386502	13.193293
15.206303	906.392366	13.198311
15.344558	905.137226	13.203328
15.296410	890.913744	13.208346
14.964215	905.027302	13.213363
15.284166	893.954038	13.218381
15.230794	900.377281	13.223399
15.497460	892.368772	13.228416
15.432493	892.803990	13.233434
15.487650	895.540937	13.238451
15.163190	889.977566	13.243469
15.358892	899.405662	13.248487
15.629154	900.591410	13.253504
15.420548	889.791811	13.258522
14.983764	898.759318	13.263539
14.985869	904.206871	13.268557
15.381307	916.908451	13.273575
15.542856	923.651864	13.278592
15.878505	925.401512	13.283610
15.473814	929.987415	13.288627
15.204368	931.471514	13.293645
15.383122	930.290344	13.298663
15.819610	934.910447	13.303680
15.783798	924.277368	13.308698
15.882407	936.619663	13.313715
15.951583	924.163346	13.318733
15.911860	928.367351	13.323751
15.750698	908.391360	13.328768
15.658336	893.037702	13.333786
15.612893	888.084213	13.338803
15.411672	892.515036	13.343821
15.569016	900.854110	13.348839
15.505301	923.267782	13.353856
16.067456	923.700733	13.358874
15.857170	932.315478	13.363891
15.955315	921.804221	13.368909
15.931134	907.236212	13.373927
15.543212	893.418389	13.378944
15.903007	900.281982	13.383962
15.464542	898.107016	13.388979
15.866241	899.413428	13.393997
15.861238	915.632117	13.399015
15.483622	919.940307	13.404032
15.946359	929.035082	13.409050
15.609430	923.900908	13.414067
15.661452	926.294113	13.419085
16.034113	925.441322	13.424103
15.733268	926.114551	13.429120
15.863131	924.524999	13.434138
15.964758	932.611950	13.439155
15.972929	931.097738	13.444173
16.159265	937.210898	13.449191
15.950147	925.912178	13.454208
16.236971	927.153045	13.459226
15.882894	930.492035	13.464243
16.063251	919.879917	13.469261
15.983102	923.901086	13.474279
15.900848	922.199161	13.479296
16.078401	925.386015	13.484314
16.107068	932.925287	13.489331
16.290199	921.930645	13.494349
16.134618	926.921178	13.499367
16.231829	928.012469	13.504384
16.156420	914.027733	13.509402
15.856353	921.479322	13.514419
15.868243	923.880771	13.519437
16.255621	928.105911	13.524455
16.035501	925.201389	13.529472
16.347554	922.275737	13.534490
16.135881	927.899962	13.539507
16.100375	924.441956	13.544525
16.062454	920.187357	13.549543
16.330869	940.408592	13.554560
16.367434	935.981186	13.559578
16.030043	944.913501	13.564595
16.222000	943.147496	13.569613
16.263979	937.201965	13.574631
16.391537	947.700600	13.579648
16.400172	941.344494	13.584666
16.225855	946.392475	13.589683
16.072135	936.465948	13.594701
16.283440	950.904742	13.599719
16.415434	947.678718	13.604736
16.711383	938.278202	13.609754
16.424365	945.692400	13.614771
16.472330	944.364868	13.619789
16.446570	937.918817	13.624807
16.291543	954.165236	13.629824
16.318662	934.129378	13.634842
16.410598	949.896980	13.639859
16.365194	943.610481	13.644877
16.667340	956.333897	13.649895
16.523596	963.124329	13.654912
16.836392	966.396581	13.659930
16.564286	955.356325	13.664947
16.576766	968.640067	13.669965
16.887464	977.956388	13.674983
16.436408	978.619940	13.680000
16.826918	978.421226	13.685018
16.398994	975.550838	13.690035
16.535364	977.153309	13.695053
16.828500	979.018683	13.700071
16.791642	987.477477	13.705088
16.765383	980.513412	13.710106
16.745188	976.776883	13.715123
16.839701	970.496644	13.720141
17.320409	977.517134	13.725159
17.188610	975.120725	13.730176
16.855167	976.796556	13.735194
17.230217	970.100422	13.740211
16.551644	952.281304	13.745229
17.011989	959.276825	13.750247
17.116581	969.875742	13.755264
16.809729	948.133278	13.760282
16.882276	951.260824	13.765299
16.940965	963.288535	13.770317
17.132646	977.221198	13.775335
16.883051	971.543392	13.780352
17.072275	975.193249	13.785370
16.907971	967.933256	13.790387
17.092562	973.508172	13.795405
17.145936	967.486724	13.800423
17.153810	972.152880	13.805440
17.017822	970.056362	13.810458
17.016282	971.158951	13.815475
16.886016	961.984761	13.820493
16.836408	969.707916	13.825511
16.929951	972.854809	13.830528
17.007438	970.725567	13.835546
17.018054	962.961337	13.840563
16.680358	975.537192	13.845581
16.953256	969.230848	13.850599
16.994039	967.962378	13.855616
17.124380	973.290026	13.860634
17.359145	991.338907	13.865651
17.109812	995.131339	13.870669
17.542070	997.254284	13.875687
17.381722	998.960793	13.880704
17.534800	995.622994	13.885722
17.282412	996.722791	13.890739
17.453936	993.767335	13.895757
17.586094	986.155324	13.900775
17.308687	988.237565	13.905792
17.439965	975.911034	13.910810
17.136929	976.715329	13.915827
17.157627	983.278451	13.920845
17.675011	991.073118	13.925863
17.391555	996.272317	13.930880
17.668185	996.091349	13.935898
17.876453	994.123821	13.940915
17.812525	986.937288	13.945933
17.770898	971.425522	13.950951
17.629304	960.632845	13.955968
17.488968	960.666839	13.960986
17.674483	961.023422	13.966003
17.423558	958.951520	13.971021
17.577649	959.171603	13.976039
17.420977	984.275251	13.981056
17.471702	979.721865	13.986074
17.546409	986.579537	13.991091
17.627548	997.381178	13.996109
17.737518	990.601148	14.001127
17.853289	991.903125	14.006144
17.675446	993.695214	14.011162
17.806262	1005.625149	14.016179
17.843110	995.995238	14.021197
17.927527	984.003240	14.026215
17.680984	1000.756227	14.031232
17.368006	999.117836	14.036250
17.620654	992.298345	14.041267
17.631378	991.373036	14.046285
18.105764	990.467117	14.051303
17.611307	992.584646	14.056320
17.901168	992.410533	14.061338
18.134825	988.583387	14.066355
17.955038	989.821108	14.071373
18.083145	992.167428	14.076391
17.558206	999.406247	14.081408
17.728366	994.060612	14.086426
17.719966	997.600022	14.091443
17.619442	1011.799378	14.096461
18.073238	1025.538135	14.101479
18.268833	1032.587928	14.106496
18.230807	1035.176027	14.111514
18.169571	1025.500591	14.116531
17.923413	1017.160150	14.121549
18.654450	1013.835337	14.126567
18.049793	1021.847606	14.131584
18.343316	1020.584760	14.136602
18.536815	1015.211225	14.141619
18.039817	1004.624035	14.146637
18.306976	1006.060685	14.151655
18.353527	1001.465863	14.156672
18.577376	994.992869	14.161690
18.321552	988.880685	14.166707
18.164588	988.643049	14.171725
18.627169	986.207296	14.176743
18.225382	991.476551	14.181760
18.308507	993.538632	14.186778
18.372053	982.293367	14.191795
18.148261	993.859815	14.196813
18.071973	984.708135	14.201831
18.469853	996.586197	14.206848
18.403814	1010.422362	14.211866
18.891584	1004.203119	14.216883
18.230630	1007.426210	14.221901
18.775543	991.978346	14.226919
18.501419	990.674816	14.231936
18.286754	988.094159	14.236954
18.512963	999.690932	14.241971
18.156591	1006.181309	14.246989
18.722530	1009.171355	14.252007
18.800789	1019.879401	14.257024
18.448752	1024.893957	14.262042
18.762740	1023.818642	14.267059
18.757690	1021.009452	14.272077
18.756199	1019.173627	14.277095
18.702772	1018.038520	14.282112
18.531550	1031.763454	14.287130
18.819659	1018.648269	14.292147
18.680131	1025.415588	14.297165
18.713338	1007.614317	14.302183
19.021057	1022.722939	14.307200
18.831136	1007.798349	14.312218
19.026649	1009.880728	14.317235
18.715128	1006.028841	14.322253
18.913698	1008.254403	14.327271
18.616521	1006.544885	14.332288
18.626974	1015.261563	14.337306
19.138232	1014.199917	14.342323
18.770096	1016.866104	14.347341
19.225379	1009.256673	14.352359
18.888915	1016.140178	14.357376
19.046326	1015.470787	14.362394
18.847052	1012.171075	14.367411
18.771042	1018.513292	14.372429
19.031627	1012.087331	14.377447
18.963940	1009.640106	14.382464
18.953167	1007.542850	14.387482
19.302896	1012.161255	14.392499
18.806149	1021.880290	14.397517
19.180418	1009.371229	14.402535
19.308298	1006.653326	14.407552
19.069455	1018.103010	14.412570
18.863267	1010.635404	14.417587
18.843229	1021.939676	14.422605
18.786488	1009.592795	14.427623
18.993945	1010.766550	14.432640
18.973019	1021.824134	14.437658
19.194155	1008.003203	14.442675
19.245442	1019.788503	14.447693
19.167065	1020.486174	14.452711
19.358065	1041.820934	14.457728
19.408702	1040.901980	14.462746
19.744112	1037.932664	14.467763
19.353102	1021.456928	14.472781
19.430397	1011.663208	14.477799
19.089187	1014.913073	14.482816
19.312851	1021.454683	14.487834
19.580877	1033.996050	14.492851
19.435268	1028.648164	14.497869
19.572352	1032.037424	14.502887
19.623085	1023.653146	14.507904
19.590856	1024.779736	14.512922
19.112485	1007.609128	14.517939
18.977971	1022.058223	14.522957
19.433012	1028.186993	14.527975
19.661662	1035.132480	14.532992
19.619247	1032.592080	14.538010
19.760596	1027.611437	14.543027
19.584313	1035.949738	14.548045
19.718848	1027.286191	14.553063
20.104924	1029.996311	14.558080
19.734065	1031.692931	14.563098
19.838662	1029.553664	14.568115
19.512455	1032.671914	14.573133
19.756935	1031.868766	14.578151
19.721489	1034.048192	14.583168
19.386985	1035.096289	14.588186
19.647989	1028.672220	14.593203
19.518193	1031.834987	14.598221
19.700961	1029.671310	14.603239
19.943447	1035.390948	14.608256
20.102718	1031.268299	14.613274
20.140593	1019.763115	14.618291
19.447077	1024.567118	14.623309
19.535821	1026.711729	14.628327
19.788052	1033.900132	14.633344
19.520362	1029.211082	14.638362
20.017959	1046.307342	14.643379
20.058285	1059.738887	14.648397
20.008758	1057.150456	14.653415
20.261703	1049.888002	14.658432
20.076203	1047.999691	14.663450
20.156461	1032.442411	14.668467
19.887087	1042.081938	14.673485
19.934570	1048.490645	14.678503
20.142988	1056.168203	14.683520
20.070698	1063.877458	14.688538
20.214312	1062.786366	14.693555
20.218260	1051.118304	14.698573
20.093339	1050.075781	14.703591
20.369847	1051.678195	14.708608
20.181525	1058.520169	14.713626
20.388042	1058.894130	14.718643
20.442810	1059.674786	14.723661
20.455810	1062.304406	14.728679
20.565173	1055.810259	14.733696
20.108394	1057.808547	14.738714
20.414440	1058.266748	14.743731
20.216501	1054.851850	14.748749
20.026359	1061.269349	14.753767
20.731486	1058.698791	14.758784
20.251138	1051.841660	14.763802
20.329474	1050.656306	14.768819
20.591397	1063.534913	14.773837
20.073827	1055.138384	14.778855
20.566585	1048.691143	14.783872
20.799485	1057.157106	14.788890
20.783544	1058.116040	14.793907
20.828605	1065.966020	14.798925
20.544469	1061.680457	14.803943
20.816574	1059.132658	14.808960
20.203288	1066.201556	14.813978
20.462480	1053.293106	14.818995
20.370303	1051.342830	14.824013
20.511830	1060.417254	14.829031
20.543089	1053.526270	14.834048
20.595021	1055.421507	14.839066
20.667404	1047.658385	14.844083
20.874813	1060.686593	14.849101
20.963574	1058.669238	14.854119
20.980171	1055.529296	14.859136
20.676418	1053.591745	14.864154
20.938600	1053.663557	14.869171
20.659579	1052.769867	14.874189
20.538679	1058.368816	14.879207
21.120167	1068.052367	14.884224
21.270906	1083.543419	14.889242
20.974834	1061.371861	14.894259
20.955196	1054.243681	14.899277
20.880398	1061.931306	14.904295
21.171915	1048.752541	14.909312
20.764417	1064.894984	14.914330
20.929230	1066.064414	14.919347
20.976167	1081.894351	14.924365
20.911263	1082.231538	14.929383
21.502635	1084.899673	14.934400
21.423875	1086.812305	14.939418
21.209034	1074.943592	14.944435
21.325092	1063.080126	14.949453
21.227347	1062.881069	14.954471
21.229784	1051.909674	14.959488
21.091665	1053.991606	14.964506
21.181355	1069.347917	14.969523
20.986235	1085.534606	14.974541
21.194101	1074.951470	14.979559
21.233591	1068.959454	14.984576
21.263588	1074.484514	14.989594
21.237265	1071.118250	14.994611
21.349759	1069.748882	14.999629
21.300625	1076.752366	15.004647
21.523254	1076.589821	15.009664
20.963986	1079.799174	15.014682
21.163807	1072.810485	15.019699
21.474458	1065.021927	15.024717
21.176483	1078.840011	15.029735
21.533350	1079.016553	15.034752
21.347756	1085.545111	15.039770
21.176366	1085.194917	15.044787
21.559348	1098.965194	15.049805
21.682219	1102.564301	15.054823
22.044422	1102.616341	15.059840
22.167979	1093.718374	15.064858
22.054478	1080.145505	15.069875
22.151027	1065.690541	15.074893
21.707815	1076.413647	15.079911
22.046120	1060.468194	15.084928
21.540637	1061.765957	15.089946
21.623164	1059.961831	15.094963
21.524392	1059.726726	15.099981
21.641392	1062.033960	15.104999
21.843015	1070.461430	15.110016
21.632850	1066.786372	15.115034
21.642286	1063.673995	15.120051
22.071416	1067.053699	15.125069
21.978106	1077.959977	15.130087
21.950720	1061.242671	15.135104
21.961750	1073.222881	15.140122
21.931787	1062.956037	15.145139
21.948401	1071.888246	15.150157
21.965135	1084.459216	15.155175
22.305762	1098.102287	15.160192
21.985862	1087.837947	15.165210
22.165082	1090.418687	15.170227
22.081262	1083.126367	15.175245
21.988071	1082.710816	15.180263
22.293853	1094.079093	15.185280
22.095352	1099.152795	15.190298
22.199982	1095.055745	15.195315
21.881182	1098.404260	15.200333
22.016759	1103.444879	15.205351
22.397837	1093.999414	15.210368
22.076205	1102.911484	15.215386
21.745626	1102.461769	15.220403
22.217278	1095.530641	15.225421
21.947450	1100.441405	15.230439
22.369753	1103.341569	15.235456
22.469542	1103.397067	15.240474
22.097915	1103.702165	15.245491
21.881148	1099.524680	15.250509
21.946557	1115.698414	15.255527
22.182605	1118.126020	15.260544
22.110868	1120.856343	15.265562
21.996122	1131.454426	15.270579
22.770719	1127.415301	15.275597
22.603726	1131.861368	15.280615
22.838706	1122.855500	15.285632
22.686265	1125.625220	15.290650
22.806261	1128.490204	15.295667
22.648512	1124.658790	15.300685
22.557181	1136.704484	15.305703
22.576037	1126.005491	15.310720
22.464181	1128.401949	15.315738
22.208113	1126.471816	15.320755
22.620068	1125.952625	15.325773
22.551841	1127.185200	15.330791
22.786996	1122.371604	15.335808
22.656879	1128.879937	15.340826
22.975708	1137.354102	15.345843
22.992920	1143.470651	15.350861
23.059675	1131.185034	15.355879
23.357870	1115.533184	15.360896
22.969942	1116.976759	15.365914
22.870913	1108.853534	15.370931
23.248813	1101.678943	15.375949
22.977534	1110.696029	15.380967
23.088511	1114.174682	15.385984
23.244434	1106.215766	15.391002
23.062932	1109.405645	15.396019
23.223340	1114.705906	15.401037
22.873694	1108.442741	15.406055
23.408050	1114.106812	15.411072
23.179629	1112.303575	15.416090
22.942526	1119.835931	15.421107
23.484207	1111.537324	15.426125
23.342455	1117.529503	15.431143
23.343815	1105.324456	15.436160
23.479690	1111.506305	15.441178
23.249827	1108.386843	15.446195
23.205243	1110.724089	15.451213
23.303195	1114.517489	15.456231
23.321207	1112.100884	15.461248
23.434312	1116.809826	15.466266
23.495592	1113.457339	15.471283
23.864590	1108.630951	15.476301
23.249150	1113.217290	15.481319
23.530708	1110.677754	15.486336
23.376853	1111.450963	15.491354
23.306485	1123.249081	15.496371
23.678692	1104.965394	15.501389
23.414634	1107.180070	15.506407
23.535653	1108.811482	15.511424
23.591492	1110.519866	15.516442
23.218644	1105.984482	15.521459
23.283761	1114.008309	15.526477
23.198863	1120.763047	15.531495
23.468548	1121.887100	15.536512
23.432165	1124.849330	15.541530
23.332494	1139.663197	15.546547
23.493389	1140.723447	15.551565
23.678985	1139.695054	15.556583
24.050464	1135.249329	15.561600
24.237911	1139.375480	15.566618
23.858771	1127.819058	15.571635
24.280984	1132.136098	15.576653
24.027627	1143.920552	15.581671
24.167435	1128.863095	15.586688
24.404228	1119.979755	15.591706
24.046488	1112.607363	15.596723
24.211922	1105.519655	15.601741
23.917035	1111.785301	15.606759
24.336901	1100.876771	15.611776
23.956368	1098.753560	15.616794
23.830161	1095.517272	15.621811
23.795587	1086.506228	15.626829
23.834482	1101.471428	15.631847
23.960377	1097.944434	15.636864
24.175757	1104.633118	15.641882
24.001239	1116.339097	15.646899
24.325762	1124.785146	15.651917
24.222245	1136.830110	15.656935
24.150347	1128.025235	15.661952
24.535920	1134.378574	15.666970
24.187755	1134.144762	15.671987
24.598157	1133.120343	15.677005
24.426935	1133.466540	15.682023
24.491655	1122.991016	15.687040
23.853874	1113.035383	15.692058
23.801940	1129.373508	15.697075
24.136956	1121.282856	15.702093
24.010058	1137.875169	15.707111
24.166291	1136.452071	15.712128
24.144772	1128.033290	15.717146
24.050616	1147.860947	15.722163
24.225361	1154.041865	15.727181
24.456153	1163.482203	15.732199
24.457665	1162.506843	15.737216
24.706969	1168.093120	15.742234
24.401816	1165.082218	15.747251
24.830140	1162.053344	15.752269
24.644347	1168.558743	15.757287
24.650127	1167.803529	15.762304
24.715935	1169.367749	15.767322
24.442848	1162.976883	15.772339
24.713894	1168.089491	15.777357
24.835278	1166.624547	15.782375
24.842337	1167.114728	15.787392
24.911966	1165.117861	15.792410
25.056137	1163.826286	15.797427
24.782945	1156.318173	15.802445
24.687751	1164.029710	15.807463
24.694283	1161.496507	15.812480
24.882295	1163.176237	15.817498
25.094130	1173.646059	15.822515
25.402368	1174.934961	15.827533
25.057775	1168.649673	15.832551
24.827295	1166.142476	15.837568
25.305980	1160.029008	15.842586
25.077765	1160.456721	15.847603
25.066718	1147.632080	15.852621
25.206917	1160.953419	15.857639
25.471798	1172.545076	15.862656
25.485453	1155.400790	15.867674
25.094186	1160.622686	15.872691
25.029150	1154.472427	15.877709
25.146993	1154.870577	15.882727
24.821899	1171.567122	15.887744
25.412140	1180.108008	15.892762
25.440564	1181.015877	15.897779
25.645364	1182.726676	15.902797
25.735052	1186.310846	15.907815
25.420485	1169.228575	15.912832
25.596333	1145.090762	15.917850
25.622738	1152.240773	15.922867
25.566434	1145.911123	15.927885
25.666228	1151.373825	15.932903
25.363513	1147.849949	15.937920
25.855469	1147.096999	15.942938
25.242402	1152.213637	15.947955
25.617432	1145.894972	15.952973
25.619150	1152.566827	15.957991
25.237851	1153.826635	15.963008
25.653227	1165.007073	15.968026
25.544272	1182.425544	15.973043
25.841083	1173.971548	15.978061
25.721732	1182.946102	15.983079
25.822197	1190.893625	15.988096
26.077905	1185.506543	15.993114
26.059435	1182.019271	15.998131
25.858492	1180.916149	16.003149
25.929548	1180.260710	16.008167
25.815468	1193.665675	16.013184
26.031909	1178.056876	16.018202
25.808233	1184.020966	16.023219
26.000854	1179.992731	16.028237
25.822555	1179.916897	16.033255
25.807700	1180.502054	16.038272
25.999319	1182.765804	16.043290
25.840188	1182.935198	16.048307
26.140218	1178.517869	16.053325
25.821761	1180.062496	16.058343
25.997900	1178.403026	16.063360
26.112719	1180.202004	16.068378
26.399657	1181.931826	16.073395
26.064929	1189.029676	16.078413
25.639032	1193.555796	16.083431
26.037996	1199.998665	16.088448
26.294798	1199.321015	16.093466
25.741885	1211.024211	16.098483
26.361741	1210.033870	16.103501
26.457717	1206.957079	16.108519
25.973660	1215.562760	16.113536
26.329264	1200.796911	16.118554
26.410455	1204.203766	16.123571
26.506580	1197.717272	16.128589
26.851661	1195.395894	16.133607
26.684166	1197.094557	16.138624
26.489502	1192.843691	16.143642
26.333685	1206.455201	16.148659
26.321533	1195.622342	16.153677
26.485135	1218.053974	16.158695
26.521239	1228.971918	16.163712
26.890277	1231.100287	16.168730
26.727457	1228.260983	16.173747
26.985279	1224.447480	16.178765
27.238568	1225.594345	16.183783
26.828692	1219.530112	16.188800
26.903477	1195.398781	16.193818
26.540079	1211.233666	16.198835
26.506379	1215.859957	16.203853
27.160125	1227.831887	16.208871
27.336781	1234.942005	16.213888
27.413665	1218.772528	16.218906
26.724648	1210.983121	16.223923
26.649089	1203.267736	16.228941
27.068578	1223.819927	16.233959
27.095915	1233.377583	16.238976
27.345771	1228.902441	16.243994
27.058712	1225.527906	16.249011
27.144818	1229.765802	16.254029
27.470098	1228.478372	16.259047
26.998935	1214.677834	16.264064
27.136640	1219.365004	16.269082
26.913128	1229.536370	16.274099
26.927999	1234.105383	16.279117
27.057607	1227.185378	16.284135
26.915502	1234.663026	16.289152
27.235919	1224.827582	16.294170
27.240955	1228.064038	16.299187
26.966911	1233.302300	16.304205
27.159105	1232.468071	16.309223
26.977292	1241.535321	16.314240
27.159769	1259.244796	16.319258
27.469675	1257.057202	16.324275
27.422779	1263.213192	16.329293
27.527096	1254.502575	16.334311
27.577295	1258.391344	16.339328
27.521860	1251.380040	16.344346
27.434868	1255.893552	16.349363
27.651341	1260.296002	16.354381
28.065364	1251.888621	16.359399
27.443767	1259.730212	16.364416
27.930563	1254.071245	16.369434
27.827167	1258.288678	16.374451
27.640361	1247.860385	16.379469
27.627525	1253.662694	16.384487
27.796785	1251.607527	16.389504
27.762141	1251.614900	16.394522
27.967503	1244.520099	16.399539
27.528146	1254.153758	16.404557
27.942423	1253.318443	16.409575
28.066266	1265.957582	16.414592
28.496562	1273.007846	16.419610
28.376452	1244.928687	16.424627
28.272702	1247.136029	16.429645
28.223822	1239.426035	16.434663
28.152581	1243.629458	16.439680
28.192074	1244.002445	16.444698
28.448794	1240.907593	16.449715
28.326018	1242.971647	16.454733
28.652805	1244.499587	16.459751
28.473258	1244.718041	16.464768
28.358002	1238.891436	16.469786
28.452766	1242.425960	16.474803
28.333688	1243.027654	16.479821
28.288362	1236.617406	16.484839
28.381897	1241.059967	16.489856
28.439748	1242.268447	16.494874
28.075883	1239.705457	16.499891
28.090759	1247.769592	16.504909
28.395067	1235.285756	16.509927
28.412602	1241.231038	16.514944
28.385206	1244.264235	16.519962
28.333497	1247.206202	16.524979
28.542644	1256.981284	16.529997
28.494204	1266.112598	16.535015
28.707799	1282.199281	16.540032
28.641552	1273.743763	16.545050
29.038421	1262.042520	16.550067
28.903804	1278.546506	16.555085
28.687618	1269.017137	16.560103
28.783881	1269.964523	16.565120
28.913906	1268.780797	16.570138
28.975273	1265.299135	16.575155
28.693201	1277.602614	16.580173
29.057233	1271.723897	16.585191
28.871138	1271.040329	16.590208
28.855951	1270.537009	16.595226
29.240075	1264.458114	16.600243
28.831528	1275.793284	16.605261
29.114777	1270.705520	16.610279
28.882442	1279.596157	16.615296
28.737733	1268.414822	16.620314
29.229500	1280.378677	16.625331
29.015273	1270.427346	16.630349
29.131331	1269.396724	16.635367
29.242278	1264.967491	16.640384
29.395778	1271.511814	16.645402
29.515348	1273.436386	16.650419
29.359206	1275.437882	16.655437
29.247965	1266.711117	16.660455
28.983184	1273.189138	16.665472
29.242338	1265.453919	16.670490
29.126784	1277.267538	16.675507
28.928653	1269.670125	16.680525
29.234651	1278.821670	16.685543
29.536785	1287.461285	16.690560
29.824964	1293.369873	16.695578
29.641403	1294.574781	16.700595
29.574369	1296.543361	16.705613
29.571476	1289.827232	16.710631
29.816242	1295.615876	16.715648
29.852368	1288.674768	16.720666
29.901507	1297.671778	16.725683
29.385907	1305.028077	16.730701
29.665158	1286.899384	16.735719
29.885649	1298.906765	16.740736
29.749877	1294.238619	16.745754
29.750073	1293.029621	16.750771
29.465960	1302.375708	16.755789
29.805357	1298.171086	16.760807
29.728953	1295.553618	16.765824
29.782229	1290.641070	16.770842
30.109232	1284.841334	16.775859
30.114815	1290.113846	16.780877
29.901689	1289.000143	16.785895
29.732154	1293.465576	16.790912
29.934646	1297.090077	16.795930
30.151897	1309.549561	16.800947
29.772620	1318.554796	16.805965
30.098674	1319.922636	16.810983
30.082533	1322.775244	16.816000
30.197890	1320.578639	16.821018
30.699664	1307.836739	16.826035
30.302605	1316.403607	16.831053
30.746431	1304.234311	16.836071
31.087130	1303.472637	16.841088
31.357761	1280.579832	16.846106
31.370074	1265.150534	16.851123
31.020279	1263.863099	16.856141
31.107432	1261.106254	16.861159
30.834303	1247.121204	16.866176
30.807202	1240.155587	16.871194
30.845844	1233.223534	16.876211
30.762995	1239.733112	16.881229
31.222065	1228.982142	16.886247
30.952209	1234.868892	16.891264
30.870427	1232.122019	16.896282
31.098556	1244.337134	16.901299
30.748721	1238.973906	16.906317
30.942792	1234.347805	16.911335
30.970641	1232.943279	16.916352
30.544267	1235.945545	16.921370
30.967154	1224.941942	16.926387
30.822404	1240.243690	16.931405
30.931257	1225.617248	16.936423
30.716099	1233.627879	16.941440
30.753557	1231.991059	16.946458
30.980471	1224.400976	16.951475
30.733501	1233.495584	16.956493
30.876876	1235.327616	16.961511
30.390079	1231.829984	16.966528
30.665969	1233.120724	16.971546
30.851230	1241.205748	16.976563
30.939210	1255.977516	16.981581
31.036391	1252.669817	16.986599
31.257021	1259.376986	16.991616
31.155366	1258.725446	16.996634
31.190093	1256.450522	17.001651
30.862448	1260.441064	17.006669
31.319383	1267.250295	17.011687
30.837370	1253.955833	17.016704
31.099783	1283.944427	17.021722
31.363951	1283.897019	17.026739
31.287286	1295.043980	17.031757
31.312338	1290.238875	17.036775
31.113291	1299.942855	17.041792
31.298331	1294.037581	17.046810
31.671347	1285.697232	17.051827
31.678492	1291.787955	17.056845
31.534005	1290.133731	17.061863
31.544597	1295.458954	17.066880
31.746433	1312.813320	17.071898
31.802415	1309.533322	17.076915
31.871688	1314.766912	17.081933
32.088428	1313.360906	17.086951
32.244836	1312.001540	17.091968
31.897596	1298.562204	17.096986
32.307333	1283.293600	17.102003
31.749773	1277.174758	17.107021
31.809259	1287.368022	17.112039
31.881187	1293.991264	17.117056
31.904900	1305.857346	17.122074
32.020091	1297.865734	17.127091
31.915301	1308.331187	17.132109
32.116188	1310.889072	17.137127
32.323995	1301.052612	17.142144
32.261307	1312.032702	17.147162
32.524281	1305.837711	17.152179
32.174874	1302.049129	17.157197
32.226851	1307.701322	17.162215
32.455089	1307.657917	17.167232
32.402048	1305.932591	17.172250
32.395786	1299.546532	17.177267
32.423240	1309.564433	17.182285
32.259629	1308.553518	17.187303
32.778279	1305.588342	17.192320
32.704637	1304.514051	17.197338
32.813120	1307.322717	17.202355
32.618670	1299.235722	17.207373
32.358261	1309.269971	17.212391
32.534284	1297.928227	17.217408
32.320491	1306.414633	17.222426
32.569639	1299.839674	17.227443
32.594550	1305.753048	17.232461
32.559938	1301.891282	17.237479
32.778218	1305.475368	17.242496
32.145960	1309.706304	17.247514
32.845697	1314.743384	17.252531
33.003429	1331.117345	17.257549
32.723096	1335.364993	17.262567
32.834876	1337.317244	17.267584
32.667837	1340.862626	17.272602
32.760094	1323.686586	17.277619
32.795665	1339.236011	17.282637
32.831267	1328.949825	17.287655
32.920700	1326.242194	17.292672
32.987633	1340.432918	17.297690
33.126891	1341.182618	17.302707
33.605279	1346.377357	17.307725
33.516510	1346.893312	17.312743
33.768027	1326.543676	17.317760
33.128129	1324.516686	17.322778
33.546735	1327.649783	17.327795
33.309664	1321.741821	17.332813
33.520378	1322.783569	17.337831
33.562747	1318.799954	17.342848
33.412408	1317.416375	17.347866
33.561393	1321.892655	17.352883
33.662980	1322.099030	17.357901
33.365904	1317.649410	17.362919
33.771718	1319.472480	17.367936
33.560837	1327.364737	17.372954
33.569468	1321.971429	17.377971
33.567871	1336.531005	17.382989
33.406758	1346.377522	17.388007
33.716468	1345.459586	17.393024
33.599986	1351.672450	17.398042
33.916715	1356.356679	17.403059
34.093689	1347.715821	17.408077
34.259786	1343.776594	17.413095
34.261140	1348.453789	17.418112
33.898361	1357.596456	17.423130
34.043427	1351.458443	17.428147
34.137823	1351.418386	17.433165
34.025368	1350.891073	17.438183
34.319331	1350.276923	17.443200
33.916985	1356.016847	17.448218
33.905552	1352.054369	17.453235
34.064329	1358.249046	17.458253
34.120969	1354.291395	17.463271
34.026131	1348.083416	17.468288
34.045249	1351.313621	17.473306
33.842754	1340.133570	17.478323
34.055047	1363.297056	17.483341
34.265629	1376.001393	17.488359
34.651426	1368.043902	17.493376
34.794581	1377.535157	17.498394
34.920119	1374.243584	17.503411
34.571567	1357.691142	17.508429
34.365137	1351.515094	17.513447
34.663055	1361.145178	17.518464
34.518961	1368.125208	17.523482
34.830321	1372.669395	17.528499
34.768200	1375.785945	17.533517
34.747858	1377.362143	17.538535
35.247215	1365.754809	17.543552
34.754820	1369.764885	17.548570
34.841144	1364.764148	17.553587
35.101097	1373.977731	17.558605
35.186369	1369.616513	17.563623
34.731109	1351.423999	17.568640
34.559035	1359.411787	17.573658
35.255226	1373.657008	17.578675
35.125684	1372.913645	17.583693
35.257251	1381.818661	17.588711
35.398753	1372.486071	17.593728
34.939537	1370.793599	17.598746
34.971721	1362.503555	17.603763
35.313542	1361.645634	17.608781
35.192064	1373.515427	17.613799
35.348124	1373.324969	17.618816
34.693962	1371.571198	17.623834
35.187731	1373.843419	17.628851
35.238897	1368.946945	17.633869
35.265643	1378.766198	17.638887
35.223696	1374.237153	17.643904
35.204717	1372.156564	17.648922
35.028921	1375.594752	17.653939
35.439931	1373.689935	17.658957
35.690849	1396.593517	17.663975
35.730970	1398.882085	17.668992
35.397739	1409.412736	17.674010
35.970833	1400.695384	17.679027
35.921342	1400.593417	17.684045
35.787557	1400.547584	17.689063
35.645055	1400.019357	17.694080
35.642616	1408.852176	17.699098
35.605769	1398.824039	17.704115
35.650056	1409.126993	17.709133
35.744495	1405.839402	17.714151
36.197691	1404.644869	17.719168
35.820028	1405.134432	17.724186
35.912981	1401.552217	17.729203
36.022220	1400.353040	17.734221
35.612413	1404.658050	17.739239
35.930358	1401.458112	17.744256
36.089601	1413.318287	17.749274
36.146665	1424.954516	17.754291
36.374376	1425.717865	17.759309
36.471225	1428.648168	17.764327
36.404108	1421.505662	17.769344
36.586208	1426.750066	17.774362
36.584975	1424.840531	17.779379
36.837755	1427.098877	17.784397
36.570124	1419.731831	17.789415
36.601902	1390.091388	17.794432
36.561564	1394.266489	17.799450
36.329474	1393.855904	17.804467
36.305245	1401.957327	17.809485
36.749953	1416.173520	17.814503
36.833805	1414.284097	17.819520
36.889737	1415.538971	17.824538
36.498598	1417.024048	17.829555
36.852984	1420.691837	17.834573
36.742051	1426.451855	17.839591
37.208223	1426.612993	17.844608
36.941051	1415.684573	17.849626
36.601542	1411.528582	17.854643
36.786313	1414.636784	17.859661
37.135059	1417.300818	17.864679
37.034636	1417.005354	17.869696
36.916929	1425.388063	17.874714
36.909799	1419.680816	17.879731
37.401652	1414.359523	17.884749
37.344562	1417.810274	17.889767
37.053467	1416.705582	17.894784
36.927996	1416.476483	17.899802
36.992227	1416.937091	17.904819
37.347754	1408.052358	17.909837
37.000527	1419.410118	17.914855
37.163398	1425.456115	17.919872
37.034385	1436.006779	17.924890
37.195881	1437.770078	17.929907
37.378663	1436.570487	17.934925
37.157621	1444.888493	17.939943
37.662833	1433.653352	17.944960
37.788218	1447.151804	17.949978
37.722097	1445.185337	17.954995
37.849806	1446.565682	17.960013
37.496772	1447.300751	17.965031
37.646804	1439.372565	17.970048
37.892860	1442.588299	17.975066
37.590755	1443.199553	17.980083
37.707798	1441.321145	17.985101
37.565113	1457.305813	17.990119
37.789305	1456.717035	17.995136
37.794305	1478.156144	18.000154
37.773452	1477.321879	18.005171
38.290762	1465.906362	18.010189
37.951822	1476.165969	18.015207
38.183168	1471.106844	18.020224
38.109484	1470.410096	18.025242
37.894626	1468.719912	18.030259
37.989784	1470.712344	18.035277
38.032310	1482.728580	18.040295
38.247249	1471.011355	18.045312
38.217124	1472.447067	18.050330
38.005463	1487.879467	18.055347
38.674970	1489.728810	18.060365
38.496428	1489.363652	18.065383
38.857712	1487.363153	18.070400
38.868045	1489.896834	18.075418
38.715270	1495.379982	18.080435
38.687414	1472.364066	18.085453
38.549749	1468.324903	18.090471
38.693327	1466.355864	18.095488
38.513220	1485.554950	18.100506
38.713161	1491.149156	18.105523
39.129105	1486.558545	18.110541
39.172736	1486.395038	18.115559
39.226309	1482.310703	18.120576
39.246268	1459.117573	18.125594
38.708405	1459.412903	18.130611
38.922390	1451.370148	18.135629
38.675342	1476.802990	18.140647
38.678179	1475.731330	18.145664
39.011260	1481.123489	18.150682
39.091757	1478.588177	18.155699
39.150779	1474.526166	18.160717
39.109469	1492.906549	18.165735
39.231869	1479.730724	18.170752
39.220751	1479.745209	18.175770
39.534269	1486.764589	18.180787
39.435015	1476.099549	18.185805
39.405517	1482.951927	18.190823
39.302942	1490.372342	18.195840
39.202217	1480.345321	18.200858
39.190450	1484.846003	18.205875
39.588307	1488.240449	18.210893
39.656447	1493.921519	18.215911
39.799574	1496.778005	18.220928
40.038941	1498.352390	18.225946
39.731561	1498.355485	18.230963
40.177736	1489.669020	18.235981
40.240209	1486.109173	18.240999
40.247737	1470.607634	18.246016
40.449901	1464.560477	18.251034
40.112516	1467.044074	18.256051
40.168311	1459.274842	18.261069
39.802364	1466.833109	18.266087
40.025067	1453.861102	18.271104
40.258569	1454.771911	18.276122
39.928989	1461.668246	18.281139
40.299038	1461.352856	18.286157
39.997785	1458.121174	18.291175
40.322306	1464.389526	18.296192
40.369079	1451.824700	18.301210
40.025007	1464.440984	18.306227
40.053604	1462.862303	18.311245
40.296294	1464.814861	18.316263
40.131959	1470.937303	18.321280
40.429018	1460.235935	18.326298
40.081559	1476.392053	18.331315
40.535213	1482.799576	18.336333
40.602183	1492.801581	18.341351
40.459952	1496.949944	18.346368
40.697096	1496.802306	18.351386
40.401230	1507.691371	18.356403
40.741497	1495.833223	18.361421
40.530002	1501.459986	18.366439
40.831274	1499.021046	18.371456
40.835059	1489.826625	18.376474
40.570417	1498.297572	18.381491
40.658715	1489.673734	18.386509
40.825898	1500.653549	18.391527
40.918940	1522.726888	18.396544
40.554447	1520.119073	18.401562
40.920473	1531.314674	18.406579
40.880323	1524.379444	18.411597
41.049513	1509.714360	18.416615
41.372453	1522.837929	18.421632
41.555418	1507.361132	18.426650
41.398270	1505.138532	18.431667
41.915625	1504.495912	18.436685
41.471779	1499.864731	18.441703
41.470474	1509.526135	18.446720
41.697382	1502.920536	18.451738
41.522381	1505.462976	18.456755
41.684190	1502.300384	18.461773
41.821104	1500.564726	18.466791
41.812738	1508.189171	18.471808
41.955620	1505.052165	18.476826
41.399796	1506.442182	18.481843
41.693840	1504.450100	18.486861
41.860734	1502.179945	18.491879
41.426137	1506.138719	18.496896
41.776539	1500.576740	18.501914
41.507233	1501.147507	18.506931
42.362654	1493.217805	18.511949
41.908330	1498.729023	18.516967
41.494385	1495.592832	18.521984
42.345154	1504.581534	18.527002
42.124126	1513.186181	18.532019
41.844666	1499.216127	18.537037
42.446190	1520.043965	18.542055
42.283034	1523.102535	18.547072
42.703930	1513.250211	18.552090
42.442323	1513.933868	18.557107
42.494978	1493.732415	18.562125
42.548952	1496.364747	18.567143
42.083438	1493.677666	18.572160
42.467936	1498.221152	18.577178
42.569535	1514.018434	18.582195
43.081875	1510.155475	18.587213
42.879933	1505.123075	18.592231
42.434875	1499.775974	18.597248
42.532753	1497.969640	18.602266
42.593380	1517.900390	18.607283
42.816824	1514.636216	18.612301
42.841058	1502.157377	18.617319
42.926761	1522.300494	18.622336
42.964791	1514.706229	18.627354
42.701421	1524.428519	18.632371
43.255791	1522.150657	18.637389
43.152192	1504.693195	18.642407
43.215350	1516.970983	18.647424
43.139951	1520.143704	18.652442
42.970349	1515.457885	18.657459
42.989932	1518.622695	18.662477
42.827075	1523.774860	18.667495
42.842093	1526.533747	18.672512
43.133835	1519.437458	18.677530
42.807662	1531.669335	18.682547
43.191926	1530.202399	18.687565
43.361465	1540.481868	18.692583
43.285854	1544.931369	18.697600
43.002641	1542.055324	18.702618
43.239039	1545.907708	18.707635
43.425407	1551.064046	18.712653
43.406654	1549.275515	18.717671
43.297524	1559.619814	18.722688
44.013261	1555.449819	18.727706
44.194372	1566.662006	18.732723
44.235032	1554.128821	18.737741
44.380485	1541.686889	18.742759
43.758841	1547.280261	18.747776
44.116828	1528.960252	18.752794
44.152176	1530.524848	18.757811
44.109108	1525.142424	18.762829
44.156241	1529.544750	18.767847
43.836742	1531.662008	18.772864
44.242987	1530.322517	18.777882
44.006608	1531.620864	18.782899
44.269873	1552.392761	18.787917
44.584616	1551.839717	18.792935
44.487989	1557.247021	18.797952
44.535177	1531.957182	18.802970
44.423911	1534.712256	18.807987
44.611577	1536.313741	18.813005
44.760663	1528.554166	18.818023
44.685457	1532.070943	18.823040
44.572682	1519.283373	18.828058
44.617583	1531.525231	18.833075
44.371165	1547.394164	18.838093
44.530638	1554.461224	18.843111
44.409022	1557.299123	18.848128
44.790363	1563.132099	18.853146
44.852284	1559.136511	18.858163
44.893700	1560.739471	18.863181
44.979380	1554.175038	18.868199
44.569802	1566.697569	18.873216
44.454305	1555.168266	18.878234
44.738810	1576.871682	18.883251
44.720790	1573.335035	18.888269
45.098740	1578.258365	18.893287
44.924747	1574.492528	18.898304
45.312356	1574.650191	18.903322
45.596334	1578.370270	18.908339
45.197206	1575.692612	18.913357
45.311155	1576.599677	18.918375
45.010753	1579.705477	18.923392
45.457773	1583.131143	18.928410
45.799989	1592.213866	18.933427
45.414299	1587.321424	18.938445
45.806996	1594.100534	18.943463
45.546180	1608.859743	18.948480
45.678940	1599.412724	18.953498
45.980419	1606.862104	18.958515
45.574931	1606.178369	18.963533
46.284795	1598.505478	18.968551
45.969428	1604.223555	18.973568
46.135018	1592.473496	18.978586
45.921968	1587.710626	18.983603
46.089421	1595.742105	18.988621
46.450438	1596.080168	18.993639
45.688865	1575.849365	18.998656
45.904827	1582.653118	19.003674
46.081012	1587.006454	19.008691
45.978154	1598.670180	19.013709
46.127387	1588.143682	19.018727
45.886791	1598.055536	19.023744
46.193031	1597.655082	19.028762
46.031167	1600.025278	19.033779
46.015378	1613.484741	19.038797
46.468561	1609.486712	19.043815
46.400374	1625.926092	19.048832
46.649002	1622.717158	19.053850
46.361730	1621.843700	19.058867
46.422640	1626.066995	19.063885
46.802488	1624.618107	19.068903
46.318704	1623.489125	19.073920
46.774557	1622.769323	19.078938
46.610000	1636.542501	19.083955
46.605451	1650.163117	19.088973
47.130440	1646.256686	19.093991
46.836279	1654.865298	19.099008
47.278550	1664.221193	19.104026
47.575162	1658.353537	19.109043
47.546541	1658.144164	19.114061
47.488670	1651.312608	19.119079
47.312555	1656.489067	19.124096
47.599295	1648.068771	19.129114
47.604732	1642.103059	19.134131
47.549527	1621.361107	19.139149
47.813237	1622.047620	19.144167
47.519584	1613.327353	19.149184
47.633986	1611.959589	19.154202
47.656845	1609.206281	19.159219
47.283165	1611.898684	19.164237
47.681450	1630.274674	19.169255
47.851795	1648.255112	19.174272
47.963638	1646.307860	19.179290
48.086588	1652.683017	19.184307
47.723796	1653.522470	19.189325
47.636030	1643.593187	19.194343
47.610284	1644.121117	19.199360
47.801715	1646.070801	19.204378
47.844217	1652.078625	19.209395
47.522734	1654.006469	19.214413
47.966067	1645.200314	19.219431
48.108672	1657.453986	19.224448
47.950044	1675.295432	19.229466
48.010867	1673.601927	19.234483
48.167911	1676.077005	19.239501
47.980548	1669.958682	19.244519
48.426379	1679.019905	19.249536
48.318647	1674.506430	19.254554
48.337948	1669.820271	19.259571
47.892972	1674.196158	19.264589
48.661019	1691.724955	19.269607
48.482091	1706.893476	19.274624
48.444607	1704.511198	19.279642
48.923860	1707.189421	19.284659
49.075703	1706.083533	19.289677
48.931778	1691.139612	19.294695
48.793486	1695.359813	19.299712
48.595804	1698.188332	19.304730
48.858678	1700.780076	19.309747
48.632324	1707.572751	19.314765
48.651041	1694.539958	19.319783
48.679305	1715.752699	19.324800
48.610109	1717.802005	19.329818
49.102704	1727.964918	19.334835
49.085980	1733.288926	19.339853
49.500283	1732.177211	19.344871
49.337863	1727.743673	19.349888
49.365884	1721.308830	19.354906
49.652446	1723.351373	19.359923
49.679602	1730.644438	19.364941
49.615297	1718.276988	19.369959
49.813090	1711.864720	19.374976
49.629103	1722.596760	19.379994
49.929992	1725.219985	19.385011
49.660747	1721.540414	19.390029
49.902480	1717.959777	19.395047
49.611979	1728.019769	19.400064
49.212678	1725.908641	19.405082
50.077239	1740.486455	19.410099
50.476007	1746.042198	19.415117
50.887814	1732.480270	19.420135
50.677781	1720.907500	19.425152
50.359950	1722.705612	19.430170
50.616656	1709.494673	19.435187
50.401430	1714.706391	19.440205
50.610291	1712.220967	19.445223
50.351918	1703.527855	19.450240
50.502119	1703.958044	19.455258
50.293261	1705.888829	19.460275
49.934294	1720.984136	19.465293
50.080658	1710.989521	19.470311
50.528872	1721.859403	19.475328
50.337156	1738.252897	19.480346
50.320752	1739.271004	19.485363
50.353983	1746.272913	19.490381
50.668928	1742.247432	19.495399
50.875541	1746.671739	19.500416
50.346681	1742.820745	19.505434
50.764777	1744.245769	19.510451
50.549887	1771.552860	19.515469
51.054162	1761.799120	19.520487
51.194466	1768.627340	19.525504
51.227154	1768.493996	19.530522
51.622208	1760.259574	19.535539
51.628338	1765.978609	19.540557
51.882075	1755.996041	19.545575
51.891706	1759.277120	19.550592
51.810550	1756.839100	19.555610
52.180685	1734.464910	19.560627
51.584542	1730.031407	19.565645
51.858179	1723.008899	19.570663
51.697759	1728.595367	19.575680
51.798073	1727.881894	19.580698
51.524874	1731.461148	19.585715
51.067673	1725.056944	19.590733
51.394931	1731.986360	19.595751
51.762733	1754.218301	19.600768
51.675940	1754.909529	19.605786
51.911682	1752.133414	19.610803
51.644533	1760.554526	19.615821
52.080853	1754.749442	19.620839
52.145243	1745.106219	19.625856
51.897666	1753.801630	19.630874
52.025522	1755.931577	19.635891
51.619417	1759.980952	19.640909
51.989758	1771.681518	19.645927
52.410512	1773.861214	19.650944
52.520918	1783.646741	19.655962
52.161124	1786.297496	19.660979
52.127251	1783.537838	19.665997
52.357958	1778.201557	19.671015
52.480123	1773.992361	19.676032
52.382746	1787.534432	19.681050
52.550407	1789.849105	19.686067
52.506698	1811.860545	19.691085
52.628342	1808.121895	19.696103
52.910696	1811.773404	19.701120
52.717872	1817.106235	19.706138
52.748034	1816.022530	19.711155
52.737829	1814.335303	19.716173
52.601656	1813.430028	19.721191
53.138079	1826.932547	19.726208
53.152967	1840.713485	19.731226
53.451501	1841.183986	19.736243
53.901910	1821.999459	19.741261
54.177413	1802.921975	19.746279
54.317493	1788.444142	19.751296
54.218057	1783.454457	19.756314
54.228692	1775.025256	19.761331
54.045647	1769.040032	19.766349
53.936774	1748.738321	19.771367
53.975717	1738.808784	19.776384
54.139385	1739.533975	19.781402
53.844202	1742.349573	19.786419
54.165044	1742.771482	19.791437
54.016046	1738.371143	19.796455
54.234157	1733.339330	19.801472
54.202272	1746.033877	19.806490
54.435512	1741.640877	19.811507
54.220158	1743.854633	19.816525
54.258178	1750.925826	19.821543
54.645115	1742.901027	19.826560
54.265214	1738.439852	19.831578
54.391651	1740.175943	19.836595
54.313474	1744.685375	19.841613
53.931120	1742.667883	19.846631
54.384029	1743.576498	19.851648
54.106590	1744.659248	19.856666
54.413365	1733.600963	19.861683
54.149895	1748.859165	19.866701
54.289046	1763.489845	19.871719
54.605239	1765.544005	19.876736
54.472198	1774.535350	19.881754
54.545623	1760.439482	19.886771
54.546605	1769.182962	19.891789
54.364631	1784.180019	19.896807
54.722884	1794.783410	19.901824
54.720730	1803.819948	19.906842
54.615808	1802.365784	19.911859
54.817861	1802.881058	19.916877
54.629069	1811.971059	19.921895
55.336490	1823.338875	19.926912
55.092562	1828.409339	19.931930
55.609661	1823.762056	19.936947
55.355508	1827.129113	19.941965
55.232961	1833.913252	19.946983
55.859128	1829.258471	19.952000
55.571860	1830.265695	19.957018
55.459311	1829.858458	19.962035
55.670347	1823.451817	19.967053
55.314843	1833.919921	19.972071
55.645388	1827.286332	19.977088
55.725069	1850.833610	19.982106
55.777762	1855.094160	19.987123
55.893247	1859.735613	19.992141
55.763715	1860.226075	19.997159
55.900828	1850.563615	20.002176
55.781280	1869.359019	20.007194
56.281325	1856.486253	20.012211
56.113722	1859.576730	20.017229
55.909086	1861.785964	20.022247
56.457597	1863.993653	20.027264
56.169285	1881.864763	20.032282
56.319653	1889.689392	20.037299
56.435109	1881.958065	20.042317
56.608646	1887.475308	20.047335
56.867536	1884.340994	20.052352
56.378533	1888.845910	20.057370
56.831955	1882.300143	20.062387
57.225161	1877.204145	20.067405
56.600988	1877.642168	20.072423
56.788908	1876.331061	20.077440
56.934747	1873.508056	20.082458
57.189253	1877.337830	20.087475
57.233292	1874.652609	20.092493
56.699875	1878.312544	20.097511
57.337158	1885.798771	20.102528
57.000964	1914.445953	20.107546
57.320726	1904.732632	20.112563
57.606705	1902.585149	20.117581
57.301809	1902.595703	20.122599
57.512496	1899.586325	20.127616
57.415161	1904.782845	20.132634
57.336908	1903.991166	20.137651
57.713362	1914.090829	20.142669
57.709346	1912.576184	20.147687
58.072925	1895.698513	20.152704
57.940139	1905.254849	20.157722
58.228132	1896.237757	20.162739
58.292479	1899.081426	20.167757
58.045398	1900.325281	20.172775
58.333293	1904.192427	20.177792
58.230204	1902.504485	20.182810
58.136001	1901.043806	20.187827
58.076023	1898.034923	20.192845
58.078381	1901.828262	20.197863
58.015615	1899.541888	20.202880
57.954390	1902.242254	20.207898
58.580678	1913.659448	20.212915
58.575941	1913.875629	20.217933
58.463621	1923.943930	20.222951
59.008797	1922.621871	20.227968
58.290307	1926.176748	20.232986
58.417567	1917.755646	20.238003
59.019388	1924.535188	20.243021
58.504042	1917.043717	20.248039
58.892935	1905.435051	20.253056
58.748721	1912.883453	20.258074
58.926412	1937.264179	20.263091
58.857112	1935.642665	20.268109
59.192635	1946.312931	20.273127
59.170091	1944.214747	20.278144
59.278360	1948.648371	20.283162
59.288748	1940.912035	20.288179
59.456485	1941.211757	20.293197
59.166929	1943.128817	20.298215
59.562111	1937.276959	20.303232
59.579121	1943.704488	20.308250
59.603441	1941.924501	20.313267
59.753029	1942.658736	20.318285
59.506545	1942.356825	20.323303
59.604092	1940.111913	20.328320
59.402338	1949.728952	20.333338
59.684754	1961.582070	20.338355
59.933989	1970.857242	20.343373
59.794708	1976.879262	20.348391
60.338222	1965.027138	20.353408
60.141556	1968.525222	20.358426
60.153043	1962.307987	20.363443
60.371490	1958.372505	20.368461
60.363056	1957.184574	20.373479
60.504755	1959.046894	20.378496
60.495304	1959.718190	20.383514
60.680269	1962.255211	20.388531
60.999454	1956.928182	20.393549
60.719411	1965.760209	20.398567
60.950385	1960.676185	20.403584
60.816190	1956.443796	20.408602
60.998929	1953.119762	20.413619
60.993893	1957.609226	20.418637
60.896290	1955.886114	20.423655
60.973266	1957.427300	20.428672
61.115703	1956.897762	20.433690
60.778379	1956.679058	20.438707
60.837034	1953.184307	20.443725
60.771359	1959.759836	20.448743
61.203697	1969.257727	20.453760
61.021715	1986.167188	20.458778
61.127864	1983.944462	20.463795
61.006833	1986.513049	20.468813
60.961806	1995.237925	20.473831
61.311238	1998.212974	20.478848
61.418546	2015.248800	20.483866
61.637308	2018.478641	20.488883
62.158342	2011.721978	20.493901
61.833340	2023.079238	20.498919
62.108466	2018.282347	20.503936
62.310597	2005.002275	20.508954
61.662799	2010.639525	20.513971
62.058327	2002.997420	20.518989
61.701754	2009.970923	20.524007
62.207871	2005.437618	20.529024
62.030774	2011.759638	20.534042
62.202019	2025.216328	20.539059
62.406639	2031.725707	20.544077
62.197526	2041.980644	20.549095
62.610665	2038.542710	20.554112
62.653163	2042.334531	20.559130
62.787608	2042.453960	20.564147
63.155439	2027.746321	20.569165
62.693838	2041.014495	20.574183
62.718398	2033.138355	20.579200
63.017117	2034.309624	20.584218
62.663016	2038.808304	20.589235
63.238439	2035.618994	20.594253
62.707663	2039.386794	20.599271
62.880448	2035.864789	20.604288
63.425725	2030.590319	20.609306
63.005908	2026.397111	20.614323
63.068973	2042.011964	20.619341
63.066316	2051.812514	20.624359
63.454846	2061.147663	20.629376
63.255857	2062.109520	20.634394
63.057664	2064.095269	20.639411
63.336269	2058.808808	20.644429
63.754660	2068.750814	20.649447
63.394995	2064.483425	20.654464
63.461728	2074.541358	20.659482
63.371715	2096.339241	20.664499
63.866849	2096.354633	20.669517
63.825141	2108.008972	20.674535
63.971915	2099.002240	20.679552
64.314142	2095.391825	20.684570
63.838245	2105.160426	20.689587
64.364515	2092.389408	20.694605
63.829007	2099.183630	20.699623
64.229908	2112.702624	20.704640
64.035063	2114.707902	20.709658
64.206943	2123.384203	20.714675
64.541368	2127.138160	20.719693
64.622451	2126.916060	20.724711
64.846168	2111.820083	20.729728
65.115167	2117.907771	20.734746
65.045143	2108.781155	20.739763
65.491033	2099.991251	20.744781
65.332745	2109.970460	20.749799
65.363585	2109.455919	20.754816
65.328141	2102.385395	20.759834
65.102161	2112.717591	20.764851
65.195833	2109.342971	20.769869
65.455884	2105.107227	20.774887
65.403276	2107.484933	20.779904
65.462923	2099.623795	20.784922
65.397198	2113.278213	20.789939
65.193915	2109.598609	20.794957
65.223924	2110.024374	20.799975
65.329324	2103.209973	20.804992
65.405016	2109.565220	20.810010
65.514142	2124.806355	20.815027
65.642394	2119.666122	20.820045
65.567111	2132.518199	20.825063
65.548492	2134.026471	20.830080
66.171465	2123.443715	20.835098
66.094316	2134.665376	20.840115
66.058944	2144.679299	20.845133
66.235813	2148.028730	20.850151
66.324474	2148.109312	20.855168
66.507193	2161.700043	20.860186
66.207617	2152.988327	20.865203
66.632918	2156.612226	20.870221
66.671240	2158.135053	20.875239
66.425584	2157.200707	20.880256
66.789360	2156.927690	20.885274
66.465630	2165.070229	20.890291
66.632097	2154.250323	20.895309
66.556332	2160.190991	20.900327
66.664084	2182.610469	20.905344
67.248867	2182.453481	20.910362
67.002411	2186.550449	20.915379
67.098532	2195.387808	20.920397
67.251988	2190.591401	20.925415
67.148031	2188.935067	20.930432
67.479706	2185.400796	20.935450
67.175822	2187.989962	20.940467
67.462343	2188.550662	20.945485
67.276958	2192.138262	20.950503
67.354404	2198.703887	20.955520
67.714354	2195.314523	20.960538
67.924466	2206.887715	20.965555
67.715620	2198.259323	20.970573
67.907784	2209.005958	20.975591
68.359265	2204.174979	20.980608
68.187745	2203.310594	20.985626
68.018513	2207.895924	20.990643
68.101136	2203.752240	20.995661
67.949991	2204.814818	21.000679
68.046255	2204.201999	21.005696
68.353015	2201.802986	21.010714
68.384911	2214.018017	21.015731
68.136164	2207.573455	21.020749
68.435343	2222.073640	21.025767
68.547024	2225.485892	21.030784
68.713980	2231.440974	21.035802
68.278805	2235.850426	21.040819
68.301947	2242.224302	21.045837
68.396295	2239.102696	21.050855
68.359205	2242.166046	21.055872
68.864158	2244.839309	21.060890
69.247949	2263.923202	21.065907
69.500912	2258.974013	21.070925
69.433413	2262.258960	21.075943
69.462482	2265.384943	21.080960
69.646305	2252.471096	21.085978
69.696531	2261.114542	21.090995
69.624175	2245.329828	21.096013
69.396911	2243.270351	21.101031
69.357350	2256.765032	21.106048
70.001058	2249.494957	21.111066
69.640069	2253.263725	21.116083
69.822473	2244.410440	21.121101
69.918913	2246.398823	21.126119
69.784072	2247.593342	21.131136
70.035558	2244.245616	21.136154
69.900265	2267.459561	21.141171
70.017933	2275.813454	21.146189
70.372292	2283.451623	21.151207
70.113043	2286.228666	21.156224
70.298341	2281.271424	21.161242
70.167425	2282.249540	21.166259
70.250274	2275.216759	21.171277
70.800462	2285.783867	21.176295
70.728019	2305.793652	21.181312
70.757968	2302.809116	21.186330
70.691375	2308.860524	21.191347
71.011737	2298.914570	21.196365
70.928050	2297.430845	21.201383
70.746053	2311.481934	21.206400
70.805750	2295.267734	21.211418
70.733485	2306.728082	21.216435
70.720720	2311.146097	21.221453
71.260418	2323.279579	21.226471
71.263621	2333.118310	21.231488
71.418939	2322.001314	21.236506
71.421585	2330.136157	21.241523
71.151848	2327.784507	21.246541
71.347815	2321.312448	21.251559
71.413928	2339.319673	21.256576
72.065227	2335.208615	21.261594
72.353951	2341.678951	21.266611
72.271467	2333.595246	21.271629
72.463591	2340.907640	21.276647
72.298369	2339.410295	21.281664
72.793688	2327.085975	21.286682
72.415701	2320.933716	21.291699
72.638201	2305.149154	21.296717
72.760877	2297.003419	21.301735
72.452373	2298.935480	21.306752
72.625099	2294.561045	21.311770
72.689816	2297.490161	21.316787
72.895307	2298.878919	21.321805
72.636918	2300.029012	21.326823
72.458170	2297.372474	21.331840
72.756741	2312.804758	21.336858
72.821868	2334.536247	21.341875
73.069964	2333.148565	21.346893
73.195069	2325.779597	21.351911
72.809450	2342.018150	21.356928
73.355066	2334.687171	21.361946
72.868530	2336.972060	21.366963
72.916021	2334.158624	21.371981
73.260562	2342.989824	21.376999
73.271976	2360.448275	21.382016
73.457172	2362.019549	21.387034
73.660184	2366.847402	21.392051
73.646456	2374.317254	21.397069
73.782789	2362.673448	21.402087
73.542499	2368.559645	21.407104
73.729346	2363.808818	21.412122
73.589565	2376.303694	21.417139
73.728803	2386.369859	21.422157
74.052443	2396.940440	21.427175
73.651626	2399.265425	21.432192
74.085842	2395.459729	21.437210
74.397595	2398.568289	21.442227
74.289912	2413.059888	21.447245
74.690456	2417.605709	21.452263
75.544608	2384.153357	21.457280
75.914914	2377.201109	21.462298
76.020542	2354.447928	21.467315
75.736316	2363.530093	21.472333
75.970553	2344.297383	21.477351
75.599418	2330.620164	21.482368
75.981632	2317.726049	21.487386
75.703374	2321.905111	21.492403
75.425315	2318.777660	21.497421
75.641894	2314.199470	21.502439
75.736479	2308.813583	21.507456
75.888297	2308.737997	21.512474
75.593812	2292.286196	21.517491
75.413206	2291.485522	21.522509
75.554227	2305.859312	21.527527
75.240672	2313.207699	21.532544
75.727853	2310.040874	21.537562
75.708556	2316.712392	21.542579
75.669761	2310.575817	21.547597
75.815812	2310.959075	21.552615
75.612877	2337.939181	21.557632
75.683896	2341.512157	21.562650
76.213136	2344.995991	21.567667
76.148094	2347.419502	21.572685
76.098776	2350.221512	21.577703
75.915379	2367.341077	21.582720
76.144151	2374.539914	21.587738
76.283284	2369.165501	21.592755
76.168726	2384.201145	21.597773
76.549553	2386.147797	21.602791
76.860658	2397.568912	21.607808
76.826088	2397.766828	21.612826
76.586438	2398.535850	21.617843
76.792631	2397.914598	21.622861
77.190746	2410.607521	21.627879
77.443810	2419.852799	21.632896
77.715430	2421.681773	21.637914
77.751707	2413.888535	21.642931
77.420299	2415.163372	21.647949
77.860403	2416.144636	21.652967
78.231585	2424.113949	21.657984
78.161896	2399.187012	21.663002
77.667230	2389.887093	21.668019
77.794075	2389.757781	21.673037
78.128603	2387.345859	21.678055
77.938996	2397.630859	21.683072
78.032395	2397.228752	21.688090
78.097578	2409.325409	21.693107
77.657107	2430.958375	21.698125
78.530949	2427.560728	21.703143
78.046215	2431.869805	21.708160
78.167611	2424.394710	21.713178
78.015471	2426.950821	21.718195
77.741746	2440.496782	21.723213
78.447284	2442.131990	21.728231
77.924488	2458.256842	21.733248
78.531291	2472.880950	21.738266
78.827315	2485.821224	21.743283
78.964607	2476.871757	21.748301
79.597584	2484.643652	21.753319
79.445466	2469.013703	21.758336
79.234306	2478.834212	21.763354
79.228844	2477.599683	21.768371
79.257917	2483.906530	21.773389
79.510390	2469.532224	21.778407
79.436564	2470.934344	21.783424
79.260042	2476.676121	21.788442
79.791313	2475.508700	21.793459
79.855685	2498.070494	21.798477
80.116518	2496.825569	21.803495
79.940514	2511.971158	21.808512
79.715173	2495.193860	21.813530
80.399470	2496.543223	21.818547
79.842786	2496.175523	21.823565
80.101134	2493.282527	21.828583
79.999111	2500.147800	21.833600
80.035838	2519.059362	21.838618
80.645058	2517.296678	21.843635
80.451965	2528.719000	21.848653
80.843184	2533.087659	21.853671
80.956044	2529.631410	21.858688
80.474866	2530.770904	21.863706
80.609018	2531.038030	21.868723
80.475612	2543.102044	21.873741
81.115057	2553.502135	21.878759
80.779312	2560.064136	21.883776
80.892666	2562.547013	21.888794
81.096090	2561.350995	21.893811
81.185640	2558.822272	21.898829
81.590338	2573.659991	21.903847
81.611450	2582.475390	21.908864
81.229395	2582.457816	21.913882
81.615983	2580.151785	21.918899
81.482399	2581.656369	21.923917
82.074638	2574.102955	21.928935
81.974106	2579.664418	21.933952
82.065793	2575.808905	21.938970
82.233417	2585.231086	21.943987
82.205145	2593.399946	21.949005
82.543238	2598.655836	21.954023
82.386067	2604.052303	21.959040
82.402557	2602.994439	21.964058
82.663483	2599.702159	21.969075
82.690714	2605.935736	21.974093
82.767044	2588.408961	21.979111
82.600632	2594.749913	21.984128
83.016523	2599.320012	21.989146
83.190120	2590.459726	21.994163
83.077323	2598.043398	21.999181
83.251775	2591.388969	22.004199
83.053990	2594.950766	22.009216
82.807404	2608.444722	22.014234
83.192768	2617.551985	22.019251
83.147083	2620.577466	22.024269
83.619596	2629.479693	22.029287
83.541386	2633.381093	22.034304
83.328466	2633.124378	22.039322
83.656142	2629.646581	22.044339
83.563434	2631.312495	22.049357
83.564266	2632.324646	22.054375
83.730358	2652.986999	22.059392
83.910866	2647.667035	22.064410
83.889000	2645.811568	22.069427
83.876210	2655.360628	22.074445
84.188044	2644.680799	22.079463
84.111233	2662.065270	22.084480
84.432313	2680.049417	22.089498
84.426159	2680.499713	22.094515
84.448237	2683.712773	22.099533
85.112140	2669.180931	22.104551
85.412918	2662.516109	22.109568
85.420933	2659.969816	22.114586
85.292557	2654.214544	22.119603
85.393864	2665.721119	22.124621
85.054703	2649.422433	22.129639
85.646622	2653.836911	22.134656
85.615175	2652.485815	22.139674
86.018968	2645.781832	22.144691
85.717043	2652.039418	22.149709
85.817278	2657.208079	22.154727
85.962854	2655.777168	22.159744
85.735729	2651.561213	22.164762
86.106753	2649.605806	22.169779
86.008813	2667.478069	22.174797
85.897810	2648.455515	22.179815
86.125241	2655.161376	22.184832
85.744034	2656.389387	22.189850
86.099150	2656.563888	22.194867
86.275983	2676.561465	22.199885
86.550640	2682.090930	22.204903
86.991133	2680.289731	22.209920
86.661271	2680.469004	22.214938
86.794449	2670.755506	22.219955
86.541469	2682.145371	22.224973
86.675956	2678.411073	22.229991
87.011062	2681.518960	22.235008
86.458853	2682.935635	22.240026
87.241696	2696.153468	22.245043
86.838112	2707.400261	22.250061
86.741695	2710.224731	22.255079
87.143769	2707.721611	22.260096
86.909292	2729.610534	22.265114
87.203960	2735.074091	22.270131
87.247673	2739.265114	22.275149
87.504777	2744.960519	22.280167
87.467494	2762.959038	22.285184
87.742941	2773.345357	22.290202
87.935785	2761.125297	22.295219
87.641353	2766.532819	22.300237
88.081216	2768.558298	22.305255
87.871056	2779.713546	22.310272
88.053198	2798.676089	22.315290
88.369629	2778.492914	22.320307
88.578552	2792.545616	22.325325
88.759608	2788.315337	22.330343
89.060785	2781.055878	22.335360
89.107496	2788.665500	22.340378
89.003926	2788.952057	22.345395
88.934075	2790.374412	22.350413
88.903302	2785.453706	22.355431
89.334145	2774.080746	22.360448
89.610672	2777.740544	22.365466
89.894018	2765.655054	22.370483
89.817512	2771.110619	22.375501
89.588617	2773.071635	22.380519
89.903567	2767.238710	22.385536
89.752648	2774.298066	22.390554
90.179918	2766.751109	22.395571
89.711494	2765.402932	22.400589
89.834196	2774.751193	22.405607
90.317860	2769.653264	22.410624
89.754803	2776.025952	22.415642
89.973051	2790.920063	22.420659
90.308672	2803.129573	22.425677
90.190444	2806.197462	22.430695
90.423801	2795.333317	22.435712
90.264305	2804.879682	22.440730
90.469417	2804.964540	22.445747
90.463413	2827.162501	22.450765
90.635999	2831.945553	22.455783
90.630077	2831.725698	22.460800
90.622074	2837.844350	22.465818
90.906812	2834.161034	22.470835
90.785407	2850.321165	22.475853
90.945690	2854.637737	22.480871
91.094020	2865.282264	22.485888
91.298424	2867.398857	22.490906
91.179899	2865.818892	22.495923
91.445196	2873.123316	22.500941
91.718841	2879.880259	22.505959
91.783927	2892.134011	22.510976
91.862407	2887.277798	22.515994
91.904864	2884.456831	22.521011
91.978287	2888.537045	22.526029
91.991062	2888.331012	22.531047
92.081202	2908.165724	22.536064
92.152941	2913.205339	22.541082
92.249254	2912.858250	22.546099
92.661102	2919.769421	22.551117
92.440557	2907.162404	22.556135
92.702488	2913.836659	22.561152
92.884243	2922.884625	22.566170
92.970913	2921.861143	22.571187
93.170500	2930.324224	22.576205
93.187304	2943.121900	22.581223
93.190642	2924.095363	22.586240
93.264838	2934.649101	22.591258
93.597632	2931.089281	22.596275
93.629699	2930.317408	22.601293
93.468627	2926.639648	22.606311
93.400719	2928.938126	22.611328
93.711478	2946.345520	22.616346
93.793652	2959.142582	22.621363
93.841656	2959.381905	22.626381
93.804109	2965.040131	22.631399
94.271845	2953.840057	22.636416
94.321315	2960.774851	22.641434
94.352338	2954.577597	22.646451
94.338488	2963.503753	22.651469
94.228777	2979.457335	22.656487
94.544437	2979.569496	22.661504
94.190992	2994.755671	22.666522
94.606159	2989.003655	22.671539
94.967515	2991.535551	22.676557
94.749300	2990.043011	22.681575
95.499242	3006.037239	22.686592
95.446240	3011.864992	22.691610
95.555873	3014.269027	22.696627
95.468473	3005.016023	22.701645
95.678292	3015.496487	22.706663
95.903576	2998.403979	22.711680
95.652609	3000.037565	22.716698
95.668397	2996.858780	22.721715
96.014802	3007.079910	22.726733
95.899205	3011.250627	22.731751
96.417484	2994.497649	22.736768
96.333962	2996.883777	22.741786
96.306036	2994.334346	22.746803
96.637708	2991.211344	22.751821
96.544904	2996.833486	22.756839
96.760689	2991.270125	22.761856
96.790653	2989.224889	22.766874
96.462640	2987.846271	22.771891
96.967255	2989.250743	22.776909
96.443620	2986.812827	22.781927
96.632445	2992.797642	22.786944
96.886069	2992.642535	22.791962
96.794208	3008.618774	22.796979
96.782866	3010.560596	22.801997
96.963615	3008.718269	22.807015
97.196982	3015.052015	22.812032
96.960863	3032.400769	22.817050
97.563330	3033.002315	22.822067
97.577608	3029.883227	22.827085
97.422659	3032.847018	22.832103
97.928089	3034.932509	22.837120
98.216947	3044.134414	22.842138
98.382067	3041.452888	22.847155
98.307537	3051.232545	22.852173
98.418287	3050.355457	22.857191
98.776592	3048.924596	22.862208
98.724982	3049.454903	22.867226
98.669604	3048.052627	22.872243
98.797535	3038.022034	22.877261
98.523070	3054.868489	22.882279
99.096552	3045.891095	22.887296
98.759143	3058.741430	22.892314
98.968907	3058.800712	22.897331
98.920257	3077.458617	22.902349
98.987596	3087.577346	22.907367
99.503804	3077.481023	22.912384
99.235827	3088.953602	22.917402
99.455019	3102.118199	22.922419
100.084564	3103.745246	22.927437
99.590940	3110.601054	22.932455
99.942756	3106.584457	22.937472
99.763198	3108.613305	22.942490
100.112039	3104.009363	22.947507
100.270154	3094.745429	22.952525
100.107527	3116.027633	22.957543
100.534703	3118.535621	22.962560
100.512480	3128.044802	22.967578
100.716810	3124.876001	22.972595
101.118344	3124.517953	22.977613
100.939652	3127.780218	22.982631
101.012927	3119.352872	22.987648
101.275434	3135.684951	22.992666
101.258298	3131.753283	22.997683
101.317286	3116.308878	23.002701
100.858591	3122.467496	23.007719
100.882749	3126.035841	23.012736
101.069044	3140.958040	23.017754
101.434275	3156.112350	23.022771
101.687095	3151.453479	23.027789
101.097634	3151.591636	23.032807
101.624778	3168.249091	23.037824
101.638373	3179.541470	23.042842
101.693325	3175.945478	23.047859
102.087265	3182.318362	23.052877
102.041936	3190.529742	23.057895
102.273476	3202.508419	23.062912
102.287174	3208.231058	23.067930
102.147974	3219.811083	23.072947
102.718486	3210.573832	23.077965
102.744449	3210.134876	23.082983
102.617778	3207.508505	23.088000
102.921878	3232.166345	23.093018
102.795883	3246.351499	23.098035
103.292069	3249.091368	23.103053
102.955509	3248.540987	23.108071
103.390860	3235.488458	23.113088
103.486513	3239.335917	23.118106
103.682069	3241.823749	23.123123
103.768331	3247.796965	23.128141
103.853132	3262.355012	23.133159
103.979547	3258.449068	23.138176
104.076478	3255.902864	23.143194
103.991806	3256.523325	23.148211
103.823612	3251.519000	23.153229
104.033778	3263.718616	23.158247
104.372656	3275.498394	23.163264
104.730123	3283.636587	23.168282
104.440177	3286.979977	23.173299
104.623308	3291.096401	23.178317
104.919941	3286.625503	23.183335
105.019133	3289.889658	23.188352
105.238971	3291.896650	23.193370
105.048525	3314.872477	23.198387
105.313455	3315.123005	23.203405
105.450437	3316.229515	23.208423
105.584464	3310.665454	23.213440
105.551861	3313.288466	23.218458
105.158103	3311.808921	23.223475
105.724343	3318.616656	23.228493
105.695176	3331.321099	23.233511
105.927574	3328.631495	23.238528
106.050770	3334.381657	23.243546
106.051289	3340.327027	23.248563
106.339126	3342.817259	23.253581
106.424226	3349.280121	23.258599
106.357920	3359.335400	23.263616
106.797454	3362.571363	23.268634
106.736758	3370.815316	23.273651
107.285371	3361.977715	23.278669
107.130665	3366.470409	23.283687
107.134399	3364.996858	23.288704
107.282275	3360.109280	23.293722
107.197138	3362.386273	23.298739
107.684231	3361.406074	23.303757
107.650953	3383.842845	23.308775
107.583145	3386.937117	23.313792
107.753534	3387.113585	23.318810
107.589148	3398.311277	23.323827
107.858888	3387.457608	23.328845
107.898520	3389.558344	23.333863
107.995657	3402.308792	23.338880
108.052227	3406.138376	23.343898
107.929898	3419.540327	23.348915
108.558891	3408.674584	23.353933
108.640606	3411.350669	23.358951
108.535548	3420.241451	23.363968
108.165133	3421.603169	23.368986
108.253376	3443.370163	23.374003
108.482974	3429.004686	23.379021
108.638350	3437.279309	23.384039
108.626293	3461.323056	23.389056
109.060205	3462.576710	23.394074
108.888400	3475.458138	23.399091
109.195787	3473.813632	23.404109
109.445344	3492.270494	23.409127
109.669979	3511.861160	23.414144
109.857796	3490.095917	23.419162
109.919238	3501.830622	23.424179
110.226587	3490.693045	23.429197
110.128719	3495.058995	23.434215
110.583596	3497.039949	23.439232
110.745823	3507.359346	23.444250
110.775243	3516.334538	23.449267
111.029344	3510.392148	23.454285
110.878483	3504.596198	23.459303
110.991983	3514.533894	23.464320
111.199662	3507.583762	23.469338
111.351291	3511.985036	23.474355
111.464106	3510.539412	23.479373
111.137748	3512.978178	23.484391
111.392373	3514.842791	23.489408
111.570838	3499.286806	23.494426
111.153913	3513.459125	23.499443
111.356190	3511.826963	23.504461
111.552818	3536.592130	23.509479
111.490676	3542.246384	23.514496
111.612980	3540.437726	23.519514
111.589021	3555.761442	23.524531
112.358727	3568.682572	23.529549
112.334326	3573.528907	23.534567
112.216939	3566.061449	23.539584
113.061436	3562.175092	23.544602
113.972337	3551.642761	23.549619
113.984670	3538.095258	23.554637
114.221533	3528.338799	23.559655
114.268796	3517.924413	23.564672
114.002184	3502.451048	23.569690
113.853254	3499.138887	23.574707
113.788090	3493.763390	23.579725
113.838128	3499.528527	23.584743
113.741601	3489.437691	23.589760
114.315222	3490.201943	23.594778
113.804950	3488.774816	23.599795
113.966209	3486.233241	23.604813
113.971349	3495.368771	23.609831
113.810148	3514.152605	23.614848
114.361281	3509.812992	23.619866
114.056027	3525.177516	23.624883
114.222510	3516.631701	23.629901
114.635321	3530.448808	23.634919
114.383149	3561.256922	23.639936
114.823664	3555.394967	23.644954
114.708861	3567.260595	23.649971
115.265479	3566.718091	23.654989
115.088732	3569.241858	23.660007
114.975955	3584.406720	23.665024
115.230468	3592.183799	23.670042
115.565102	3600.873256	23.675059
115.660052	3595.604595	23.680077
115.533770	3596.196153	23.685095
116.067072	3617.926051	23.690112
115.932316	3619.253743	23.695130
115.803412	3632.099034	23.700147
115.933454	3629.082650	23.705165
115.579211	3635.218202	23.710183
116.014933	3656.052064	23.715200
116.359706	3658.300971	23.720218
116.357008	3660.839141	23.725235
116.688248	3675.947633	23.730253
116.550617	3677.171858	23.735271
116.881103	3690.875608	23.740288
117.051453	3677.112729	23.745306
117.079836	3687.024517	23.750323
117.257439	3698.264030	23.755341
117.478977	3712.370986	23.760359
117.415753	3710.424616	23.765376
117.944106	3717.685726	23.770394
117.334227	3717.140582	23.775411
117.705000	3720.132113	23.780429
117.964291	3731.823089	23.785447
117.701780	3746.118399	23.790464
118.379981	3741.335906	23.795482
118.419904	3745.867239	23.800499
118.413182	3752.910159	23.805517
118.605710	3762.878980	23.810535
118.659129	3768.938177	23.815552
118.829742	3767.838873	23.820570
118.731345	3781.916371	23.825587
119.013236	3791.857366	23.830605
119.136706	3805.489700	23.835623
119.110146	3810.420728	23.840640
119.412462	3806.296026	23.845658
119.243499	3811.670060	23.850675
119.787442	3817.296934	23.855693
120.109841	3819.375153	23.860711
119.773429	3825.874395	23.865728
119.993269	3821.855924	23.870746
119.966446	3823.044029	23.875763
120.213471	3845.681370	23.880781
120.484358	3844.586660	23.885799
120.024368	3862.818913	23.890816
120.495653	3851.766845	23.895834
120.343792	3877.412610	23.900851
120.703832	3886.483486	23.905869
120.939374	3879.699449	23.910887
121.002155	3890.368736	23.915904
121.335777	3910.483593	23.920922
121.456516	3904.367523	23.925939
121.154015	3914.586833	23.930957
121.330412	3911.415429	23.935975
121.635778	3927.521110	23.940992
121.659753	3937.105793	23.946010
121.877032	3938.245862	23.951027
122.451730	3921.494730	23.956045
122.913602	3910.381579	23.961063
122.965504	3916.193810	23.966080
123.119092	3910.954674	23.971098
122.877599	3914.732325	23.976115
123.069403	3913.066427	23.981133
123.092022	3915.468524	23.986151
123.152989	3912.005633	23.991168
123.421663	3929.561297	23.996186
123.553250	3942.367098	24.001203
123.436125	3950.735709	24.006221
124.046178	3936.166370	24.011239
123.508825	3960.754139	24.016256
123.853799	3945.839027	24.021274
123.889961	3958.300416	24.026291
123.682542	3945.170624	24.031309
123.787770	3952.046980	24.036327
123.966306	3973.350832	24.041344
124.222961	3968.985611	24.046362
124.244123	3976.142911	24.051379
124.274023	3984.077211	24.056397
124.570125	3998.301186	24.061415
124.313108	4006.168593	24.066432
124.618170	4000.764475	24.071450
124.985216	4018.028658	24.076467
124.876946	4034.638675	24.081485
124.981769	4035.122544	24.086503
125.090354	4038.508148	24.091520
125.246768	4043.322612	24.096538
125.618888	4066.278507	24.101555
125.493066	4069.028568	24.106573
126.014399	4065.305652	24.111591
125.843399	4073.756125	24.116608
126.012973	4081.886192	24.121626
126.041057	4099.261523	24.126643
126.037030	4097.124140	24.131661
126.380761	4100.346256	24.136679
126.419204	4119.226789	24.141696
127.058676	4119.984466	24.146714
127.116049	4120.058055	24.151731
126.905270	4133.671797	24.156749
127.577608	4123.815043	24.161767
127.251411	4115.769729	24.166784
127.473119	4133.143636	24.171802
127.729134	4136.763460	24.176819
127.713734	4141.665175	24.181837
127.729019	4129.696815	24.186855
127.942232	4143.380682	24.191872
128.284549	4135.054954	24.196890
128.415667	4149.852229	24.201907
128.567076	4162.893140	24.206925
128.676087	4171.688136	24.211943
128.769454	4173.607977	24.216960
128.724410	4158.761412	24.221978
129.045323	4169.169854	24.226995
129.023823	4156.557099	24.232013
129.356862	4165.795642	24.237031
129.465979	4176.342054	24.242048
129.553735	4182.303566	24.247066
129.569814	4183.786187	24.252083
129.543967	4188.907401	24.257101
129.611165	4179.510277	24.262119
129.580992	4196.920598	24.267136
129.510016	4209.897700	24.272154
130.152979	4214.939680	24.277171
129.893409	4226.661727	24.282189
130.345312	4235.780938	24.287207
130.079564	4241.573229	24.292224
130.371906	4247.812234	24.297242
130.741381	4256.000919	24.302259
130.916064	4273.280812	24.307277
131.525087	4273.374167	24.312295
131.390691	4280.507842	24.317312
131.538745	4268.056221	24.322330
131.493339	4272.232145	24.327347
131.439638	4277.190669	24.332365
131.458341	4289.350846	24.337383
131.796834	4295.748368	24.342400
131.941383	4302.304123	24.347418
132.633999	4291.378774	24.352435
132.375671	4292.613259	24.357453
132.633568	4294.984194	24.362471
132.248982	4300.852168	24.367488
132.653192	4316.941038	24.372506
132.813621	4311.224576	24.377523
132.794798	4331.824591	24.382541
132.938523	4315.421078	24.387559
133.084275	4332.899574	24.392576
133.281480	4339.631663	24.397594
133.394657	4349.445121	24.402611
133.184662	4358.675180	24.407629
133.464639	4355.944815	24.412647
133.315539	4354.137851	24.417664
133.803567	4373.518088	24.422682
133.916023	4386.655830	24.427699
134.175038	4387.337352	24.432717
134.120166	4381.009296	24.437735
134.578467	4396.697860	24.442752
134.374073	4403.171462	24.447770
134.921945	4406.425085	24.452787
134.754913	4400.249538	24.457805
135.314236	4397.941325	24.462823
135.604629	4393.131730	24.467840
135.763478	4398.096711	24.472858
135.699726	4395.027331	24.477875
135.527215	4406.390109	24.482893
136.292546	4405.405357	24.487911
136.219226	4420.336482	24.492928
136.505533	4414.713257	24.497946
136.541447	4412.265209	24.502963
136.367875	4416.950736	24.507981
136.611975	4415.072126	24.512999
136.309602	4412.312517	24.518016
136.471958	4420.884581	24.523034
136.897277	4415.835989	24.528051
136.717688	4435.691866	24.533069
136.962653	4434.094258	24.538087
136.988473	4444.073496	24.543104
137.078312	4443.062385	24.548122
137.356856	4456.530912	24.553139
137.368323	4475.514799	24.558157
137.383657	4475.896604	24.563175
137.789799	4485.892212	24.568192
137.864679	4489.389831	24.573210
138.134481	4486.161053	24.578227
138.348240	4493.941024	24.583245
138.366341	4491.725095	24.588263
138.790638	4513.080984	24.593280
138.538304	4519.234199	24.598298
138.774196	4523.105924	24.603315
138.987759	4533.415500	24.608333
139.149238	4528.346924	24.613351
139.173018	4539.505499	24.618368
139.236304	4557.704366	24.623386
139.441243	4550.499071	24.628403
139.599363	4556.892022	24.633421
139.666569	4570.424904	24.638439
140.139125	4584.926049	24.643456
139.877567	4592.310956	24.648474
140.389385	4581.092562	24.653491
140.454574	4592.584508	24.658509
140.575630	4608.627801	24.663527
140.700095	4621.417229	24.668544
140.951346	4622.409554	24.673562
141.023897	4618.289746	24.678579
140.835196	4628.370902	24.683597
141.089972	4633.260952	24.688615
141.324981	4646.760504	24.693632
141.220528	4654.385521	24.698650
141.405633	4637.415644	24.703667
141.733466	4650.758806	24.708685
142.025077	4656.544474	24.713703
142.057776	4656.101996	24.718720
142.112883	4667.263331	24.723738
142.085224	4657.924604	24.728755
142.250712	4688.200090	24.733773
142.545427	4684.507209	24.738791
142.588324	4695.371327	24.743808
142.575319	4705.561944	24.748826
142.908321	4703.111737	24.753843
142.653203	4718.890034	24.758861
142.536625	4727.684238	24.763879
143.060816	4739.782032	24.768896
142.814410	4748.411173	24.773914
143.722567	4756.619292	24.778931
143.372618	4784.511663	24.783949
143.649256	4782.407880	24.788967
143.799305	4780.329856	24.793984
143.696608	4808.229224	24.799002
144.074567	4811.253640	24.804019
144.250336	4815.124403	24.809037
144.734468	4831.220211	24.814055
145.294087	4831.064256	24.819072
145.077383	4824.951136	24.824090
145.551946	4824.328911	24.829107
145.445380	4832.923836	24.834125
145.135361	4836.945418	24.839143
145.469882	4852.270686	24.844160
145.936142	4869.648482	24.849178
146.017371	4868.628536	24.854195
146.038507	4865.956059	24.859213
146.455737	4884.670615	24.864231
146.279963	4895.544431	24.869248
146.382151	4884.749863	24.874266
146.899585	4884.486723	24.879283
146.892048	4888.940037	24.884301
146.952775	4887.765986	24.889319
147.090368	4906.793227	24.894336
146.945205	4917.480047	24.899354
147.245236	4909.249146	24.904371
147.289102	4922.152231	24.909389
147.303766	4937.886705	24.914407
147.524763	4934.082370	24.919424
147.504218	4946.777238	24.924442
148.108752	4962.048295	24.929459
148.274342	4980.072354	24.934477
148.353841	4979.128293	24.939495
148.643855	4981.937392	24.944512
148.294201	4999.172903	24.949530
148.804425	5001.239762	24.954547
148.997951	4998.920582	24.959565
148.934431	5021.296990	24.964583
149.226737	5025.094099	24.969600
149.403048	5031.656696	24.974618
149.894680	5024.624850	24.979635
149.745734	5033.074140	24.984653
149.913001	5035.500415	24.989671
150.294249	5041.846249	24.994688
150.223013	5050.744932	24.999706
150.805890	5045.642397	25.004723
150.953799	5048.408178	25.009741
150.678105	5045.009249	25.014759
151.011418	5056.130144	25.019776
150.928943	5078.871273	25.024794
151.437291	5085.704769	25.029811
151.285734	5086.638837	25.034829
151.351243	5083.637626	25.039847
151.598729	5076.023366	25.044864
151.545828	5088.362235	25.049882
152.065068	5097.810202	25.054899
151.839603	5094.126482	25.059917
151.412859	5101.360297	25.064935
151.948542	5118.388970	25.069952
152.144674	5125.189307	25.074970
152.557880	5121.352989	25.079987
152.401943	5137.204218	25.085005
152.519080	5158.880586	25.090023
152.868854	5158.128661	25.095040
152.928837	5165.729752	25.100058
153.437386	5173.224020	25.105075
153.905337	5176.923462	25.110093
153.804405	5179.521910	25.115111
154.246878	5177.542520	25.120128
154.309905	5185.311653	25.125146
154.597550	5175.158651	25.130163
154.486682	5179.112574	25.135181
154.278707	5174.728146	25.140199
154.414294	5176.735210	25.145216
154.482630	5199.398686	25.150234
154.820514	5203.605676	25.155251
155.180902	5208.123954	25.160269
155.018874	5208.669923	25.165287
155.317100	5224.860033	25.170304
155.236919	5240.937411	25.175322
155.330401	5240.792756	25.180339
155.603311	5249.465039	25.185357
155.495427	5267.373417	25.190375
155.859878	5261.914899	25.195392
155.964769	5281.760799	25.200410
155.997310	5291.756785	25.205427
156.519921	5292.615070	25.210445
156.260863	5313.057032	25.215463
156.828166	5319.157845	25.220480
156.913430	5326.050723	25.225498
156.937176	5343.319859	25.230515
157.016276	5356.367084	25.235533
157.128844	5356.298014	25.240551
157.549839	5362.342822	25.245568
158.156076	5380.505978	25.250586
158.386832	5373.088099	25.255603
158.453507	5378.519201	25.260621
158.269402	5373.960634	25.265639
158.525427	5384.646476	25.270656
158.880756	5409.267732	25.275674
158.977664	5414.449674	25.280691
159.067205	5412.952616	25.285709
158.740253	5421.247398	25.290727
159.388251	5423.614331	25.295744
159.484627	5436.930466	25.300762
159.628398	5440.244371	25.305779
159.808570	5440.972910	25.310797
159.711853	5456.294817	25.315815
160.226381	5456.992213	25.320832
160.006575	5473.389158	25.325850
160.054541	5477.220678	25.330867
160.463267	5482.112980	25.335885
160.709496	5491.398630	25.340903
161.089264	5494.927720	25.345920
160.694730	5497.927055	25.350938
160.793438	5519.181688	25.355955
161.344401	5524.256715	25.360973
161.374627	5530.754011	25.365991
161.881430	5535.198438	25.371008
161.806637	5545.656617	25.376026
161.795040	5541.287498	25.381043
162.046218	5549.768238	25.386061
162.417329	5565.782772	25.391079
163.092648	5556.405461	25.396096
163.000777	5572.984447	25.401114
163.146059	5567.004633	25.406131
163.614756	5568.340507	25.411149
163.379600	5569.757106	25.416167
163.909693	5562.180713	25.421184
163.649244	5563.686573	25.426202
163.594981	5570.755534	25.431219
163.700492	5551.756482	25.436237
163.706373	5586.856602	25.441255
163.712348	5586.767440	25.446272
163.552592	5601.700656	25.451290
163.881756	5610.226752	25.456307
164.331576	5623.281118	25.461325
164.021516	5631.773251	25.466343
164.348706	5644.247869	25.471360
164.379034	5661.105138	25.476378
164.760090	5677.989207	25.481395
164.819892	5683.641294	25.486413
165.146164	5702.925616	25.491431
165.290636	5715.062059	25.496448
165.562295	5724.698825	25.501466
165.769669	5737.429704	25.506483
165.938146	5748.880129	25.511501
166.201281	5756.776963	25.516519
166.270809	5766.173259	25.521536
166.521957	5776.304136	25.526554
166.512868	5790.435927	25.531571
166.931958	5798.448635	25.536589
167.375483	5794.928459	25.541607
167.816154	5795.097068	25.546624
167.928816	5792.029606	25.551642
167.981550	5805.844764	25.556659
168.229179	5806.336072	25.561677
168.353547	5814.526138	25.566695
168.885038	5826.522750	25.571712
168.632475	5824.032631	25.576730
168.689782	5809.891302	25.581747
169.081402	5809.511231	25.586765
168.931132	5817.390940	25.591783
169.166077	5835.191803	25.596800
169.440379	5844.656508	25.601818
169.252166	5845.030426	25.606835
169.718242	5842.079077	25.611853
170.120059	5857.477631	25.616871
170.234582	5857.327112	25.621888
170.872770	5870.484277	25.626906
170.317516	5865.893513	25.631923
170.427188	5863.854351	25.636941
170.526268	5863.525250	25.641959
170.948098	5879.827814	25.646976
171.003257	5896.024350	25.651994
171.086943	5890.981656	25.657011
171.471184	5885.859093	25.662029
171.366077	5898.590831	25.667047
171.397961	5918.189755	25.672064
171.720313	5919.538163	25.677082
171.869638	5925.603917	25.682100
172.380411	5931.092947	25.687117
172.431035	5948.426013	25.692135
172.754168	5960.064335	25.697152
172.616185	5961.112762	25.702170
172.682420	5960.845825	25.707188
172.741277	5971.120619	25.712205
172.600342	5987.156868	25.717223
173.060418	5993.312782	25.722240
173.466378	6003.718948	25.727258
173.369326	6015.397200	25.732276
173.939575	6025.408270	25.737293
173.681878	6038.970409	25.742311
174.005028	6033.061680	25.747328
174.147626	6052.191074	25.752346
174.129226	6063.862593	25.757364
174.424060	6067.403566	25.762381
174.583906	6080.793185	25.767399
174.937365	6080.899892	25.772416
175.518288	6079.527478	25.777434
175.471666	6074.057439	25.782452
175.798206	6078.313021	25.787469
175.759172	6101.493403	25.792487
176.263017	6107.619249	25.797504
176.057451	6112.606733	25.802522
176.263867	6113.746016	25.807540
177.030558	6112.263183	25.812557
176.534782	6121.076275	25.817575
176.978919	6126.225960	25.822592
177.308142	6129.606860	25.827610
177.175389	6142.161449	25.832628
176.976933	6133.824504	25.837645
177.275770	6155.524822	25.842663
177.495319	6153.017638	25.847680
177.503462	6179.914921	25.852698
177.644501	6186.435818	25.857716
177.990709	6189.573687	25.862733
177.935061	6209.886918	25.867751
178.820892	6219.079326	25.872768
178.534757	6230.153547	25.877786
178.423852	6245.610107	25.882804
178.641352	6248.122739	25.887821
179.180095	6256.828596	25.892839
179.503521	6268.361557	25.897856
179.809787	6283.273116	25.902874
179.756469	6284.123193	25.907892
180.141552	6279.985678	25.912909
180.184220	6304.279078	25.917927
180.383575	6311.983583	25.922944
180.820099	6307.972984	25.927962
180.949875	6317.544689	25.932980
180.934952	6326.177968	25.937997
181.240665	6346.710150	25.943015
181.164548	6343.229730	25.948032
181.243189	6355.079883	25.953050
181.424797	6362.909443	25.958068
181.766712	6378.936745	25.963085
181.777322	6390.944727	25.968103
182.076691	6412.806773	25.973120
181.898586	6420.466145	25.978138
181.713608	6430.254042	25.983156
182.371463	6429.932115	25.988173
182.258535	6453.229257	25.993191
182.440619	6469.579356	25.998208
182.990540	6479.531872	26.003226
183.652249	6482.937943	26.008244
183.610466	6492.755645	26.013261
183.557531	6508.955805	26.018279
183.645382	6535.212704	26.023296
184.345620	6518.800288	26.028314
184.772611	6543.589416	26.033332
185.329375	6538.087484	26.038349
185.242465	6543.309792	26.043367
185.175778	6544.020330	26.048384
185.511731	6547.107204	26.053402
185.484036	6540.996664	26.058420
185.696275	6538.429200	26.063437
185.857443	6561.304469	26.068455
185.617157	6573.949728	26.073472
185.731443	6577.042722	26.078490
185.995745	6593.418671	26.083508
186.523143	6594.814985	26.088525
186.527172	6608.827970	26.093543
186.680808	6610.614833	26.098560
187.019949	6625.444852	26.103578
186.967100	6638.326815	26.108596
187.410938	6633.777753	26.113613
187.426012	6639.339946	26.118631
187.366923	6657.534791	26.123648
187.695519	6662.215515	26.128666
187.558153	6672.187835	26.133684
187.930257	6681.688777	26.138701
187.993262	6700.984196	26.143719
188.115183	6709.082192	26.148736
188.404183	6721.500212	26.153754
188.686982	6731.843048	26.158772
189.496868	6737.017229	26.163789
189.722894	6741.292056	26.168807
189.714103	6747.006330	26.173824
190.212298	6735.629584	26.178842
190.142123	6746.082274	26.183860
190.526843	6764.838341	26.188877
190.932607	6764.136907	26.193895
190.732419	6771.781213	26.198912
190.968174	6764.504420	26.203930
190.917920	6767.399524	26.208948
191.055185	6776.150325	26.213965
190.953027	6794.912498	26.218983
190.963120	6807.385592	26.224000
191.279847	6821.776076	26.229018
191.502299	6836.249975	26.234036
191.739627	6839.654963	26.239053
191.787284	6869.142937	26.244071
192.109269	6870.470226	26.249088
192.608252	6891.050555	26.254106
192.079334	6904.440317	26.259124
192.832554	6921.249706	26.264141
192.879572	6934.498115	26.269159
192.922852	6947.673116	26.274176
193.217721	6959.179822	26.279194
193.133943	6976.221283	26.284212
193.467899	6997.334845	26.289229
193.761122	7007.194084	26.294247
194.012492	7021.195479	26.299264
194.652571	7030.991587	26.304282
194.614451	7053.420209	26.309300
195.087470	7054.081265	26.314317
195.188227	7050.596505	26.319335
195.065320	7072.750171	26.324352
195.402412	7084.338958	26.329370
195.642428	7091.648772	26.334388
195.943727	7109.352616	26.339405
196.275297	7120.387833	26.344423
196.193186	7124.386296	26.349440
196.211242	7132.760906	26.354458
196.702215	7140.641847	26.359476
197.413750	7140.974993	26.364493
197.328359	7170.654980	26.369511
197.608475	7162.142667	26.374528
197.676407	7165.056803	26.379546
197.950000	7167.384615	26.384564
198.172391	7171.130853	26.389581
198.788210	7185.523959	26.394599
198.610890	7193.877503	26.399616
198.758684	7191.467937	26.404634
198.836296	7188.957395	26.409652
199.025791	7196.020449	26.414669
198.991698	7206.610014	26.419687
199.112311	7229.130659	26.424704
199.591320	7216.910806	26.429722
199.637992	7238.654508	26.434740
200.008367	7240.618890	26.439757
200.147674	7248.837937	26.444775
200.045119	7251.941099	26.449792
200.785822	7262.914739	26.454810
201.158840	7266.934500	26.459828
201.211576	7262.599901	26.464845
201.106720	7258.671932	26.469863
201.220306	7274.315891	26.474880
201.752782	7264.587180	26.479898
201.906288	7279.020953	26.484916
201.823539	7290.990779	26.489933
201.914431	7297.679576	26.494951
202.015837	7306.603615	26.499968
202.158326	7318.607715	26.504986
202.235209	7325.808476	26.510004
202.341437	7335.711593	26.515021
202.599075	7338.006636	26.520039
202.792315	7372.862973	26.525056
202.765875	7375.044537	26.530074
203.097594	7396.073146	26.535092
203.305107	7414.085930	26.540109
203.602423	7434.023073	26.545127
203.487411	7454.402897	26.550144
204.222338	7473.834158	26.555162
204.235225	7485.262070	26.560180
204.495502	7512.882980	26.565197
205.294736	7510.413177	26.570215
205.153407	7527.005572	26.575232
205.529867	7532.837285	26.580250
205.361819	7538.923308	26.585268
205.770220	7558.184436	26.590285
206.023410	7573.280897	26.595303
205.972326	7577.426341	26.600320
206.507261	7600.007852	26.605338
206.413071	7614.012836	26.610356
206.387331	7629.473132	26.615373
207.139075	7637.784395	26.620391
207.281055	7658.216303	26.625408
207.857378	7657.931541	26.630426
208.151615	7666.293629	26.635444
207.857699	7667.409821	26.640461
208.246517	7674.284008	26.645479
208.208141	7691.042211	26.650496
208.443985	7691.634792	26.655514
208.780009	7708.390672	26.660532
208.612633	7722.377192	26.665549
208.972056	7741.605720	26.670567
209.283495	7755.456788	26.675584
209.346723	7769.967447	26.680602
209.726976	7780.264057	26.685620
209.950855	7794.208475	26.690637
210.139594	7816.778499	26.695655
210.311904	7825.679232	26.700672
210.833408	7836.124915	26.705690
211.170111	7849.310989	26.710708
210.859187	7849.418615	26.715725
211.154239	7857.508913	26.720743
211.222832	7878.233717	26.725760
211.480005	7883.485153	26.730778
211.517704	7900.664959	26.735796
211.656242	7913.570507	26.740813
212.667266	7921.069258	26.745831
212.839323	7918.245947	26.750848
213.345134	7924.755793	26.755866
213.542223	7934.043170	26.760884
213.491540	7954.786316	26.765901
213.921527	7947.428665	26.770919
214.119456	7949.708514	26.775936
214.184058	7950.347674	26.780954
214.014818	7966.832522	26.785972
214.061352	7980.824688	26.790989
214.789652	7985.509504	26.796007
214.930378	7988.412484	26.801024
215.078915	7989.359084	26.806042
215.011862	8013.233788	26.811060
215.387023	8016.924125	26.816077
215.358887	8017.529072	26.821095
215.463016	8041.461236	26.826112
215.776743	8049.316943	26.831130
215.614197	8061.392767	26.836148
215.314761	8078.820193	26.841165
215.670013	8102.159328	26.846183
216.249560	8126.674307	26.851200
216.865896	8139.432122	26.856218
216.799211	8159.561414	26.861236
217.002998	8168.906107	26.866253
217.214154	8190.987705	26.871271
217.455871	8200.868062	26.876288
217.858400	8216.643751	26.881306
218.526618	8217.094409	26.886324
218.990296	8230.099797	26.891341
219.131229	8241.936283	26.896359
219.185669	8257.019940	26.901376
219.655045	8254.064462	26.906394
219.856894	8246.908425	26.911412
219.615451	8267.289812	26.916429
220.370358	8276.638315	26.921447
219.996897	8290.519358	26.926464
220.349888	8301.683390	26.931482
220.335200	8309.956931	26.936500
220.425837	8326.928320	26.941517
221.337505	8337.802625	26.946535
221.221288	8354.255430	26.951552
221.363380	8351.589841	26.956570
221.489841	8370.377326	26.961588
221.454400	8385.235783	26.966605
221.970727	8399.436204	26.971623
221.969455	8418.298534	26.976640
222.416677	8433.943341	26.981658
222.489064	8439.684908	26.986676
222.780586	8475.467087	26.991693
222.736047	8466.182485	26.996711
223.316707	8496.059914	27.001728
222.938148	8512.556470	27.006746
223.736139	8542.704305	27.011764
223.493049	8556.648204	27.016781
224.400116	8571.968609	27.021799
224.229828	8576.003353	27.026816
224.395738	8592.392987	27.031834
224.635792	8602.259690	27.036852
224.817638	8627.652885	27.041869
225.480027	8642.395639	27.046887
225.505417	8674.087650	27.051904
225.611624	8673.847902	27.056922
226.221473	8685.334251	27.061940
226.109755	8702.295545	27.066957
226.651422	8705.854400	27.071975
226.947698	8733.490352	27.076992
227.105562	8736.578104	27.082010
227.546525	8753.121503	27.087028
227.396879	8758.703139	27.092045
227.833493	8764.626145	27.097063
227.988089	8787.646715	27.102080
228.267531	8804.776301	27.107098
228.578656	8800.037569	27.112116
228.265798	8823.741631	27.117133
228.936174	8817.799400	27.122151
228.563986	8837.372163	27.127168
228.920443	8857.338289	27.132186
229.155591	8859.667228	27.137204
229.089052	8886.582280	27.142221
229.311158	8898.154473	27.147239
229.730186	8920.531823	27.152256
229.789900	8935.280450	27.157274
230.295038	8947.988858	27.162292
229.935220	8977.819418	27.167309
230.663423	8988.177954	27.172327
230.744974	9010.000990	27.177344
230.890092	9015.194219	27.182362
231.292868	9054.552161	27.187380
231.486892	9068.518411	27.192397
231.809177	9084.490265	27.197415
231.926233	9098.098294	27.202432
232.546219	9113.067527	27.207450
232.915038	9126.428147	27.212468
232.924011	9150.485705	27.217485
233.238897	9167.792552	27.222503
233.785577	9183.873748	27.227520
233.910390	9186.049335	27.232538
234.488726	9192.738295	27.237556
234.670833	9213.927296	27.242573
234.755905	9204.282780	27.247591
234.993386	9223.172563	27.252608
235.395562	9240.186905	27.257626
235.872565	9237.858622	27.262644
235.676449	9254.551715	27.267661
235.848569	9269.201622	27.272679
235.945439	9277.381502	27.277696
236.473319	9294.866585	27.282714
236.971014	9301.991234	27.287732
236.674746	9303.724747	27.292749
236.648569	9306.135770	27.297767
237.051155	9326.998391	27.302784
236.985806	9343.499691	27.307802
237.291732	9357.500383	27.312820
237.689600	9378.501714	27.317837
237.803193	9395.450728	27.322855
238.158625	9419.232127	27.327872
237.927489	9437.345283	27.332890
238.620822	9452.778468	27.337908
238.825992	9472.820915	27.342925
239.166917	9487.348443	27.347943
239.232771	9504.593043	27.352960
239.234164	9529.938085	27.357978
240.054294	9554.716224	27.362996
240.067046	9557.112152	27.368013
240.689122	9578.523955	27.373031
241.036358	9579.989876	27.378048
241.230572	9599.422983	27.383066
241.626435	9593.514264	27.388084
241.616638	9621.468872	27.393101
241.898700	9613.946762	27.398119
242.022024	9633.051365	27.403136
242.021803	9644.266357	27.408154
242.327403	9658.775488	27.413172
242.292729	9672.147668	27.418189
242.864861	9702.625129	27.423207
242.892378	9712.614487	27.428224
242.988829	9744.386615	27.433242
243.582645	9742.651757	27.438260
243.684518	9766.846060	27.443277
244.118361	9777.670761	27.448295
244.321768	9795.295383	27.453312
244.880986	9805.823545	27.458330
245.066941	9812.914348	27.463348
245.289877	9825.814509	27.468365
245.144766	9842.033362	27.473383
245.939666	9838.780879	27.478400
245.972128	9851.160461	27.483418
246.449285	9855.338476	27.488436
246.550695	9853.779950	27.493453
246.828779	9872.380146	27.498471
247.080752	9876.989478	27.503488
247.305103	9886.792622	27.508506
247.540889	9889.789661	27.513524
247.913929	9907.645409	27.518541
247.753906	9916.810503	27.523559
248.066132	9918.746287	27.528576
248.044752	9946.401658	27.533594
248.677044	9956.526244	27.538612
248.507899	9975.685360	27.543629
248.758881	9990.407120	27.548647
249.415790	9997.663979	27.553664
249.372522	10020.549027	27.558682
249.770467	10031.278239	27.563700
249.772652	10052.236688	27.568717
249.568389	10067.543863	27.573735
250.026971	10079.162707	27.578752
250.160966	10117.173495	27.583770
250.779339	10119.710748	27.588788
250.821493	10159.166767	27.593805
251.151150	10172.953884	27.598823
251.487795	10193.050231	27.603840
251.326230	10212.195763	27.608858
251.959904	10233.634092	27.613876
252.344165	10254.905903	27.618893
252.546679	10276.768863	27.623911
252.704749	10291.375557	27.628928
253.161854	10315.447855	27.633946
253.479027	10321.380260	27.638964
253.929444	10345.387538	27.643981
254.417135	10345.435756	27.648999
254.549583	10351.687992	27.654016
254.431468	10371.303126	27.659034
255.130610	10381.550018	27.664052
255.591125	10399.189311	27.669069
255.675232	10403.773112	27.674087
255.941878	10409.442145	27.679104
256.035730	10430.183386	27.684122
256.436258	10429.373177	27.689140
256.721191	10456.112715	27.694157
256.797589	10466.638808	27.699175
256.839245	10469.236480	27.704192
256.933428	10494.258797	27.709210
257.092025	10509.030258	27.714228
257.438912	10533.073924	27.719245
257.639950	10551.762551	27.724263
257.984205	10563.856108	27.729280
258.043709	10592.331099	27.734298
258.575321	10610.010809	27.739316
258.864116	10627.715910	27.744333
259.232078	10637.367238	27.749351
259.260598	10649.028796	27.754368
259.462705	10679.490804	27.759386
260.003851	10691.339818	27.764404
260.244740	10709.268048	27.769421
260.621877	10719.367756	27.774439
260.921893	10725.177108	27.779456
261.095657	10748.217789	27.784474
261.270235	10761.735737	27.789492
261.550667	10767.891068	27.794509
261.844281	10787.547815	27.799527
261.801327	10799.433285	27.804544
262.194655	10816.249874	27.809562
262.279059	10828.357650	27.814580
262.926093	10838.545740	27.819597
263.008766	10845.947237	27.824615
263.716552	10863.236337	27.829632
263.471085	10878.783539	27.834650
264.266211	10885.204786	27.839668
264.527075	10888.818672	27.844685
264.613212	10900.215577	27.849703
264.844613	10898.418698	27.854720
264.929020	10938.898534	27.859738
265.640969	10921.839971	27.864756
265.826414	10947.592347	27.869773
265.808778	10951.083915	27.874791
266.134118	10950.418533	27.879808
266.450784	10981.388364	27.884826
266.707901	10988.770399	27.889844
266.658944	10997.315735	27.894861
266.733553	11018.851146	27.899879
267.340257	11036.930899	27.904896
267.250577	11059.677015	27.909914
267.659093	11076.453536	27.914932
267.806914	11096.412206	27.919949
268.194538	11111.690579	27.924967
268.551867	11125.369921	27.929984
268.572442	11151.942599	27.935002
269.179918	11171.732030	27.940020
269.238631	11182.604249	27.945037
269.420569	11216.228369	27.950055
269.491881	11230.325612	27.955072
269.907024	11260.025339	27.960090
270.108578	11272.856155	27.965108
270.433597	11301.384406	27.970125
270.741757	11321.661802	27.975143
271.370455	11336.728584	27.980160
271.197956	11352.647021	27.985178
271.992561	11366.611615	27.990196
271.834524	11385.803647	27.995213
271.900015	11417.649610	28.000231
272.445551	11430.881947	28.005248
272.490585	11451.959579	28.010266
273.052824	11479.419771	28.015284
273.276389	11494.613885	28.020301
273.746443	11509.039065	28.025319
274.225315	11540.074414	28.030336
274.188383	11558.135621	28.035354
274.288941	11576.705038	28.040372
274.886803	11592.922761	28.045389
274.996896	11610.754752	28.050407
275.780405	11628.169189	28.055424
275.858231	11639.416723	28.060442
276.186147	11660.384600	28.065460
276.459272	11666.172762	28.070477
276.759815	11677.923811	28.075495
277.046235	11696.727218	28.080512
277.204520	11718.380448	28.085530
277.639793	11725.581951	28.090548
277.861057	11739.809152	28.095565
278.018753	11769.369796	28.100583
278.141769	11780.696589	28.105600
278.678631	11800.088822	28.110618
278.792071	11815.403959	28.115636
279.194853	11831.350205	28.120653
279.320887	11850.539715	28.125671
279.925994	11870.475372	28.130688
280.027993	11872.837908	28.135706
280.099783	11898.654803	28.140724
280.747389	11908.722146	28.145741
280.705594	11916.294511	28.150759
280.924624	11932.318658	28.155776
281.306792	11951.768289	28.160794
280.966293	11957.586010	28.165812
281.495024	11984.529464	28.170829
281.659184	12010.361131	28.175847
281.724661	12026.294271	28.180864
281.782544	12046.083109	28.185882
282.262320	12085.031478	28.190900
282.318700	12095.619476	28.195917
282.779027	12133.750195	28.200935
283.584692	12146.985606	28.205952
283.827132	12172.821861	28.210970
284.205903	12177.341456	28.215988
284.985063	12192.484897	28.221005
285.266234	12188.656258	28.226023
285.913229	12200.955248	28.231040
286.220977	12211.381799	28.236058
286.684657	12214.796831	28.241076
287.201500	12206.853959	28.246093
287.258696	12218.757713	28.251111
287.454893	12224.434366	28.256128
287.700734	12231.735327	28.261146
287.797208	12236.738340	28.266164
288.049895	12240.681662	28.271181
287.849055	12257.746592	28.276199
288.476177	12271.158319	28.281216
288.886741	12291.928914	28.286234
288.569917	12308.723213	28.291252
289.217598	12320.322511	28.296269
289.238728	12340.640992	28.301287
289.478727	12356.477702	28.306304
289.800257	12370.903116	28.311322
289.787032	12395.129146	28.316340
290.018074	12406.046046	28.321357
290.450206	12442.929385	28.326375
290.669784	12444.752444	28.331392
291.126436	12472.863780	28.336410
291.251048	12493.267690	28.341428
292.022068	12510.592183	28.346445
291.949314	12534.459561	28.351463
292.866817	12539.652474	28.356480
293.115931	12556.674485	28.361498
293.413818	12578.236335	28.366516
293.783085	12582.841145	28.371533
294.040514	12602.889046	28.376551
294.317256	12620.142913	28.381568
294.291503	12631.145173	28.386586
294.394089	12648.894457	28.391604
294.706127	12671.977943	28.396621
294.691348	12696.006119	28.401639
295.134973	12720.597983	28.406656
295.481004	12735.862743	28.411674
295.888332	12764.433478	28.416692
296.136385	12778.606715	28.421709
296.228440	12809.125684	28.426727
296.540447	12820.462780	28.431744
296.695995	12855.221440	28.436762
297.042754	12883.099602	28.441780
297.095331	12902.327773	28.446797
297.315903	12928.167288	28.451815
297.769260	12959.389249	28.456832
298.126667	12976.875933	28.461850
298.363444	13014.196452	28.466868
298.937221	13024.952823	28.471885
299.011272	13060.751372	28.476903
299.392157	13088.268061	28.481920
299.914246	13105.599878	28.486938
300.349283	13135.890708	28.491956
300.714273	13150.508161	28.496973
301.018763	13173.566822	28.501991
300.894045	13183.050954	28.507008
301.464900	13205.901516	28.512026
301.508371	13229.362927	28.517044
302.008133	13243.543607	28.522061
302.384616	13270.725666	28.527079
302.645730	13285.532272	28.532096
302.962878	13296.115555	28.537114
302.847508	13321.407922	28.542132
303.703051	13332.563678	28.547149
303.767176	13357.258947	28.552167
304.070792	13380.694695	28.557184
304.842812	13390.857344	28.562202
304.627605	13417.225474	28.567220
305.218641	13419.722900	28.572237
305.172527	13459.021959	28.577255
305.921725	13453.709536	28.582272
306.629579	13473.734116	28.587290
306.738777	13484.985596	28.592308
307.428127	13505.627908	28.597325
307.810879	13507.706076	28.602343
308.026788	13512.254680	28.607360
308.415968	13526.598967	28.612378
308.406747	13526.263285	28.617396
308.851744	13551.704040	28.622413
309.092617	13566.580455	28.627431
309.251367	13579.289406	28.632448
309.591105	13603.497996	28.637466
309.511898	13625.971745	28.642484
309.655968	13641.471054	28.647501
310.122710	13669.366878	28.652519
309.992704	13697.057722	28.657536
310.468357	13726.123106	28.662554
310.612067	13752.692188	28.667572
310.996130	13775.119126	28.672589
311.056332	13815.647975	28.677607
311.329090	13827.821259	28.682624
311.442683	13872.281326	28.687642
311.736460	13909.690561	28.692660
312.441082	13931.780785	28.697677
313.216009	13954.184014	28.702695
313.444878	13988.215832	28.707712
313.761565	14004.950757	28.712730
313.554744	14033.903120	28.717748
313.990612	14060.443079	28.722765
314.575436	14090.261641	28.727783
314.718953	14115.215940	28.732800
314.983908	14149.108137	28.737818
315.067557	14181.859546	28.742836
315.666795	14205.151233	28.747853
316.143050	14227.271915	28.752871
316.347306	14261.610985	28.757888
317.247128	14275.945177	28.762906
317.746844	14299.198371	28.767924
318.381264	14316.717703	28.772941
318.478356	14340.264786	28.777959
318.771028	14337.593698	28.782976
319.191089	14347.602655	28.787994
319.554158	14364.877128	28.793012
319.765824	14374.920721	28.798029
320.094402	14390.560301	28.803047
320.334993	14405.891426	28.808064
320.730197	14421.359213	28.813082
320.790188	14436.703032	28.818100
321.027232	14455.497346	28.823117
321.518139	14475.532408	28.828135
322.009816	14489.939319	28.833152
322.108115	14494.121606	28.838170
321.894907	14515.197244	28.843188
322.120526	14527.065248	28.848205
322.946785	14551.492297	28.853223
322.585783	14588.564258	28.858240
322.825671	14596.037487	28.863258
323.366690	14625.623168	28.868276
323.377927	14660.942349	28.873293
323.779599	14687.670256	28.878311
323.945796	14718.457861	28.883328
324.637960	14739.733274	28.888346
324.788919	14770.331229	28.893364
325.249618	14794.694857	28.898381
325.860946	14818.861708	28.903399
325.510921	14850.455581	28.908416
326.328761	14876.183201	28.913434
326.313076	14907.007678	28.918452
326.976312	14937.046444	28.923469
327.343821	14957.187704	28.928487
327.451420	14989.383541	28.933504
328.211681	15000.948727	28.938522
328.248076	15045.670671	28.943540
329.050555	15049.406720	28.948557
329.664350	15076.555515	28.953575
329.760528	15086.191607	28.958592
330.353723	15102.777703	28.963610
330.728659	15126.349109	28.968628
331.285962	15134.493288	28.973645
331.732830	15147.948377	28.978663
331.512324	15162.521471	28.983680
331.843510	15188.916737	28.988698
332.120011	15208.550156	28.993716
332.784570	15225.140282	28.998733
333.297834	15227.781736	29.003751
333.628174	15251.478939	29.008768
334.078061	15246.176272	29.013786
334.145184	15262.205288	29.018804
334.790768	15277.099566	29.023821
334.863995	15284.676450	29.028839
334.748822	15314.107591	29.033856
335.302755	15321.476973	29.038874
335.563306	15343.917125	29.043892
335.727416	15373.104963	29.048909
336.038999	15395.248276	29.053927
336.213864	15418.027445	29.058944
336.487521	15434.167324	29.063962
336.798304	15465.657334	29.068980
336.876231	15504.070660	29.073997
337.503723	15520.558491	29.079015
337.721875	15560.040920	29.084032
337.812940	15570.256590	29.089050
337.889880	15608.889409	29.094068
338.354043	15636.992342	29.099085
338.912857	15672.229039	29.104103
338.937938	15707.467784	29.109120
339.975820	15731.609259	29.114138
340.189132	15767.108454	29.119156
340.556454	15793.479774	29.124173
340.993987	15808.041851	29.129191
341.275176	15837.499502	29.134208
341.649991	15849.970998	29.139226
341.881670	15880.450430	29.144244
342.094627	15904.212206	29.149261
342.707547	15934.038917	29.154279
342.998895	15958.796506	29.159296
343.542314	15985.647990	29.164314
343.711922	16010.504688	29.169332
344.242947	16031.580003	29.174349
344.479072	16047.674705	29.179367
344.519841	16079.399884	29.184384
345.090193	16088.735554	29.189402
345.199042	16111.562901	29.194420
345.329419	16136.059051	29.199437
345.865755	16158.982529	29.204455
346.163131	16187.531802	29.209472
346.522387	16216.578384	29.214490
346.808062	16242.445415	29.219508
346.892878	16266.282589	29.224525
347.246266	16291.782225	29.229543
347.311738	16330.735457	29.234560
347.784915	16363.245240	29.239578
348.239860	16400.097462	29.244596
348.687249	16428.146212	29.249613
349.223134	16449.377302	29.254631
349.312497	16494.876187	29.259648
349.903549	16524.387626	29.264666
350.622777	16557.137489	29.269684
350.743872	16583.106475	29.274701
351.095340	16600.523939	29.279719
351.183922	16644.975165	29.284736
352.378338	16666.186992	29.289754
352.601083	16683.435199	29.294772
352.777065	16708.537784	29.299789
353.160850	16728.352227	29.304807
353.335010	16760.523127	29.309824
353.950828	16775.021768	29.314842
354.306343	16804.818730	29.319860
354.704538	16820.349759	29.324877
355.584202	16841.785911	29.329895
355.443490	16864.279023	29.334912
355.695786	16888.273698	29.339930
355.864324	16908.393654	29.344948
356.321286	16934.889046	29.349965
356.546458	16959.950740	29.354983
356.637738	17001.754328	29.360000
357.494516	17015.458117	29.365018
357.874925	17050.133137	29.370036
358.225955	17076.373655	29.375053
358.307955	17097.151341	29.380071
358.886789	17136.134687	29.385088
359.063021	17143.964861	29.390106
359.400772	17176.292246	29.395124
359.470116	17214.971062	29.400141
359.566991	17232.032679	29.405159
359.819568	17273.794396	29.410176
360.571708	17309.540001	29.415194
360.568799	17349.077611	29.420212
361.227393	17380.467786	29.425229
361.602324	17415.164972	29.430247
362.113729	17453.616435	29.435264
362.543677	17479.601729	29.440282
362.541053	17514.562031	29.445300
363.028149	17555.878810	29.450317
363.877051	17576.783499	29.455335
363.994445	17618.423515	29.460352
364.290595	17650.958931	29.465370
365.014555	17681.424540	29.470388
364.869577	17705.904120	29.475405
365.425878	17728.504888	29.480423
365.820593	17768.968973	29.485440
365.983649	17796.933285	29.490458
366.689918	17823.751251	29.495476
367.012064	17853.431110	29.500493
367.357324	17887.169477	29.505511
367.773219	17915.328445	29.510528
368.151897	17948.358325	29.515546
368.173829	17962.862078	29.520564
368.614902	17999.289815	29.525581
369.037983	18016.088393	29.530599
369.245749	18047.135401	29.535616
369.857698	18080.826710	29.540634
370.497158	18110.801126	29.545652
370.457035	18143.245181	29.550669
371.042223	18159.112130	29.555687
371.323194	18192.973721	29.560704
372.260943	18208.208347	29.565722
372.335261	18225.645184	29.570740
372.687753	18257.374770	29.575757
373.559661	18275.081157	29.580775
374.132274	18285.295761	29.585792
374.586820	18293.520066	29.590810
375.254975	18319.763474	29.595828
375.784614	18317.736558	29.600845
376.293569	18324.561451	29.605863
376.019855	18345.653585	29.610880
376.806199	18346.120469	29.615898
376.931373	18362.432904	29.620916
376.679145	18386.379554	29.625933
377.225731	18396.166612	29.630951
377.238325	18417.484000	29.635968
377.474579	18457.544145	29.640986
377.980249	18480.200066	29.646004
377.941970	18509.370299	29.651021
378.411531	18545.266399	29.656039
378.546997	18579.006336	29.661056
378.585494	18619.457568	29.666074
379.147452	18650.308142	29.671092
379.456475	18698.316216	29.676109
380.005915	18732.506352	29.681127
380.573419	18774.583687	29.686144
380.552600	18819.568091	29.691162
381.153606	18845.981129	29.696180
381.405418	18882.098568	29.701197
382.259704	18912.858508	29.706215
382.506431	18957.002728	29.711232
382.726511	18983.297963	29.716250
383.374027	19011.992574	29.721268
383.850291	19057.856701	29.726285
384.877097	19080.078475	29.731303
384.920901	19106.590786	29.736320
385.309741	19127.638488	29.741338
385.763691	19154.041759	29.746356
386.583933	19166.867427	29.751373
387.310190	19185.871208	29.756391
387.530557	19205.681073	29.761408
387.855709	19231.829975	29.766426
388.396199	19248.837315	29.771444
388.422630	19271.045789	29.776461
389.155088	19285.771620	29.781479
389.313066	19317.959613	29.786496
389.539927	19339.579958	29.791514
389.808414	19363.852981	29.796532
389.638938	19397.027231	29.801549
390.017756	19424.343596	29.806567
390.726860	19459.788830	29.811584
390.892293	19484.512687	29.816602
391.209622	19506.733063	29.821620
391.444518	19548.884939	29.826637
392.089585	19588.522022	29.831655
392.243294	19620.961974	29.836672
392.652193	19654.237730	29.841690
393.353531	19684.080158	29.846708
393.594040	19728.101323	29.851725
394.066496	19739.902119	29.856743
394.519180	19774.484101	29.861760
394.784618	19792.064247	29.866778
395.334314	19809.676024	29.871796
395.834570	19846.206748	29.876813
395.936489	19870.657946	29.881831
395.965546	19896.388832	29.886848
396.547398	19924.471604	29.891866
397.215138	19951.643094	29.896884
397.415964	19987.202249	29.901901
398.318208	20010.995723	29.906919
398.330708	20035.969668	29.911936
398.469501	20076.183887	29.916954
399.220892	20098.506375	29.921972
399.560756	20135.903109	29.926989
399.657652	20160.629888	29.932007
399.919919	20192.759671	29.937024
400.345139	20241.539588	29.942042
400.740450	20273.579634	29.947060
400.817625	20313.033701	29.952077
401.070300	20355.711233	29.957095
401.480262	20396.026223	29.962112
401.974234	20446.893774	29.967130
402.636526	20469.911075	29.972148
403.061163	20511.132032	29.977165
403.600499	20551.663976	29.982183
404.292055	20588.902400	29.987200
404.511701	20623.242624	29.992218
405.326322	20645.847017	29.997236
405.790597	20689.718442	30.002253
406.486521	20709.983998	30.007271
407.064146	20743.732108	30.012288
407.061662	20766.842891	30.017306
408.104479	20787.364675	30.022324
408.356435	20810.729665	30.027341
408.522916	20834.373760	30.032359
409.174768	20858.254177	30.037376
409.074479	20894.421820	30.042394
409.735311	20909.965078	30.047412
409.851607	20948.225341	30.052429
410.147124	20976.909265	30.057447
410.402028	21012.882574	30.062464
410.468379	21056.461571	30.067482
411.159905	21081.346357	30.072500
411.296201	21133.180398	30.077517
411.594078	21168.662864	30.082535
412.240019	21202.156162	30.087552
412.767737	21241.034610	30.092570
413.227671	21275.724117	30.097588
413.417342	21315.455110	30.102605
414.009869	21364.954691	30.107623
414.601867	21398.506218	30.112640
414.719575	21445.005611	30.117658
415.287816	21479.456811	30.122676
415.288408	21520.563041	30.127693
415.673260	21559.254673	30.132711
416.363796	21605.938444	30.137728
416.714508	21652.803348	30.142746
416.850345	21689.387568	30.147764
417.670110	21730.940062	30.152781
418.229948	21770.640600	30.157799
418.665222	21804.744017	30.162816
419.023880	21838.142813	30.167834
419.757658	21867.674697	30.172852
420.261462	21897.192797	30.177869
420.727583	21931.636654	30.182887
421.772490	21959.817785	30.187904
422.175347	21982.582245	30.192922
422.683818	21995.945943	30.197940
422.674895	22020.197923	30.202957
423.198327	22041.053485	30.207975
423.729708	22055.132425	30.212992
424.099025	22090.269112	30.218010
424.375247	22108.658768	30.223028
424.647225	22126.777945	30.228045
424.671717	22168.212899	30.233063
425.165546	22186.702099	30.238080
425.485562	22228.731439	30.243098
425.488694	22256.576798	30.248116
425.974639	22294.036051	30.253133
426.300638	22330.512810	30.258151
426.985796	22362.917075	30.263168
427.186717	22405.575273	30.268186
428.151225	22433.094109	30.273204
428.320255	22468.548669	30.278221
428.723871	22499.442083	30.283239
429.024139	22541.087585	30.288256
428.946807	22587.773883	30.293274
429.738032	22622.400094	30.298292
430.024951	22668.956736	30.303309
430.588264	22720.852437	30.308327
431.235140	22757.994275	30.313344
431.555379	22812.150792	30.318362
432.178849	22843.594898	30.323380
432.506014	22891.567767	30.328397
432.441210	22928.366166	30.333415
433.263193	22978.329063	30.338432
432.888803	23027.041687	30.343450
433.933562	23061.792257	30.348468
434.556228	23110.424670	30.353485
435.534363	23150.237155	30.358503
436.064833	23174.853755	30.363520
436.898034	23209.762761	30.368538
437.775843	23222.088433	30.373556
438.581339	23247.766421	30.378573
439.087230	23265.437981	30.383591
439.826270	23281.072940	30.388608
439.978337	23296.611447	30.393626
440.396443	23307.671614	30.398644
440.355858	23329.951746	30.403661
440.637258	23354.263062	30.408679
441.358441	23385.794442	30.413696
441.322155	23417.038542	30.418714
441.753464	23439.696162	30.423732
442.068427	23476.028988	30.428749
442.204276	23516.143067	30.433767
442.776938	23537.026989	30.438784
443.144873	23576.400946	30.443802
443.266263	23597.892884	30.448820
443.552445	23651.349702	30.453837
443.914717	23686.861437	30.458855
444.489626	23725.412909	30.463872
444.761372	23767.714263	30.468890
445.239230	23809.856913	30.473908
445.702104	23860.344085	30.478925
446.137838	23894.188280	30.483943
447.090947	23937.397164	30.488960
447.624095	23974.929554	30.493978
447.589418	24014.428159	30.498996
448.540331	24045.178293	30.504013
448.589309	24094.686233	30.509031
449.166018	24124.473645	30.514048
449.550500	24161.301009	30.519066
450.286270	24201.274483	30.524084
450.478200	24234.305135	30.529101
450.634532	24283.133468	30.534119
451.505747	24321.842083	30.539136
451.660607	24355.986158	30.544154
452.062616	24382.545015	30.549172
452.153614	24424.723472	30.554189
452.658140	24465.912396	30.559207
453.157891	24513.063213	30.564224
453.323211	24561.682685	30.569242
453.710753	24603.146841	30.574260
454.073590	24644.381805	30.579277
454.523394	24689.658470	30.584295
455.228153	24729.095842	30.589312
455.736069	24773.464185	30.594330
456.530597	24820.844446	30.599348
456.731828	24864.213669	30.604365
457.054009	24911.682092	30.609383
457.450601	24953.811096	30.614400
458.310465	24996.689627	30.619418
458.916116	25040.130906	30.624436
459.623025	25085.438461	30.629453
460.471079	25115.904820	30.634471
460.827218	25145.449932	30.639488
461.399992	25179.510470	30.644506
461.846395	25210.343343	30.649524
462.630170	25228.898096	30.654541
462.881892	25262.807103	30.659559
463.580265	25287.719014	30.664576
463.705210	25326.351983	30.669594
463.964216	25357.367641	30.674612
464.518497	25387.388077	30.679629
464.955488	25431.057069	30.684647
465.603950	25459.308289	30.689664
465.795239	25495.735337	30.694682
466.264576	25528.545779	30.699700
467.341788	25555.631460	30.704717
468.030377	25584.863476	30.709735
468.604334	25606.478332	30.714752
468.884419	25639.724152	30.719770
469.240093	25661.542501	30.724788
470.225963	25679.105311	30.729805
470.329170	25715.411823	30.734823
471.024506	25724.225897	30.739840
471.186873	25760.913800	30.744858
471.604070	25790.232243	30.749876
471.992924	25816.372847	30.754893
472.346118	25846.108907	30.759911
473.056126	25875.798378	30.764928
473.198130	25911.581569	30.769946
473.371166	25944.236990	30.774964
473.857949	25977.143174	30.779981
474.659361	26015.987079	30.784999
474.706834	26050.716969	30.790016
475.202367	26095.907740	30.795034
475.679579	26139.811577	30.800052
475.917847	26170.198138	30.805069
476.564524	26213.670272	30.810087
477.244591	26237.999910	30.815104
477.491014	26294.338816	30.820122
477.906431	26337.714035	30.825140
478.355928	26380.528545	30.830157
478.750853	26422.872768	30.835175
479.596503	26457.773734	30.840192
479.894576	26506.411355	30.845210
480.405180	26549.701904	30.850228
480.719653	26583.070008	30.855245
480.972870	26640.777902	30.860263
481.229074	26676.083176	30.865280
481.900365	26714.057581	30.870298
482.228862	26764.649742	30.875316
482.953530	26794.221652	30.880333
483.176152	26837.797328	30.885351
483.908200	26871.995644	30.890368
484.590812	26907.359905	30.895386
484.899465	26959.135679	30.900404
485.573186	26991.697314	30.905421
486.160299	27038.168657	30.910439
486.591910	27063.266244	30.915456
487.215012	27097.833244	30.920474
487.553315	27137.254990	30.925492
488.018470	27172.510804	30.930509
488.272288	27216.877177	30.935527
489.070126	27244.008770	30.940544
489.597403	27284.270102	30.945562
490.170086	27321.981472	30.950580
490.467746	27352.281387	30.955597
490.979586	27403.967967	30.960615
491.221235	27452.254850	30.965632
491.698553	27488.730082	30.970650
492.465992	27517.094260	30.975668
493.458746	27563.070634	30.980685
493.643901	27594.481122	30.985703
494.002133	27636.452712	30.990720
494.766126	27673.565261	30.995738
495.005078	27714.295029	31.000756
495.354822	27753.968643	31.005773
495.687422	27804.613633	31.010791
496.082361	27843.813070	31.015808
496.676293	27905.392888	31.020826
497.111215	27945.951853	31.025844
497.626101	27992.418825	31.030861
498.051006	28032.673658	31.035879
498.981837	28081.538700	31.040896
499.405772	28120.396401	31.045914
500.280466	28169.084889	31.050932
500.775070	28196.334584	31.055949
500.961358	28246.793799	31.060967
501.554218	28276.664591	31.065984
502.406266	28330.470991	31.071002
502.629872	28365.258289	31.076020
502.787026	28409.101157	31.081037
503.490158	28452.768289	31.086055
504.222561	28504.610798	31.091072
504.650953	28529.234685	31.096090
505.254577	28582.086233	31.101108
505.641215	28609.796166	31.106125
506.355904	28648.742416	31.111143
507.104128	28686.052189	31.116160
508.269835	28709.418184	31.121178
508.433454	28746.187914	31.126196
509.192237	28778.051049	31.131213
509.576947	28804.225251	31.136231
509.748994	28831.261354	31.141248
510.243518	28873.522463	31.146266
510.355720	28910.616554	31.151284
511.111860	28950.966780	31.156301
511.176678	28997.754096	31.161319
511.982220	29042.282733	31.166336
512.669251	29078.638143	31.171354
512.528838	29114.544245	31.176372
513.125003	29157.830250	31.181389
513.175507	29206.352495	31.186407
514.212224	29248.656975	31.191424
514.238382	29305.969748	31.196442
514.747726	29359.643795	31.201460
515.226106	29415.055167	31.206477
515.265173	29458.557471	31.211495
515.657469	29520.835852	31.216512
516.173087	29576.027018	31.221530
516.606788	29628.736435	31.226548
517.281048	29680.163029	31.231565
517.714754	29741.810646	31.236583
518.309426	29792.181267	31.241600
518.952027	29850.396718	31.246618
520.402653	29882.036559	31.251636
521.227839	29912.997893	31.256653
522.192794	29956.666327	31.261671
522.298163	29986.406469	31.266688
522.924639	30001.067714	31.271706
523.370953	30058.483543	31.276724
523.445587	30084.982484	31.281741
524.049239	30126.408204	31.286759
524.616084	30178.425153	31.291776
525.053299	30209.880521	31.296794
525.269199	30258.791517	31.301812
525.915242	30298.904430	31.306829
526.435360	30350.043087	31.311847
526.781354	30399.819435	31.316864
527.425320	30450.751671	31.321882
527.869038	30505.257283	31.326900
528.241073	30556.774499	31.331917
528.535904	30597.220907	31.336935
528.917982	30647.253835	31.341952
529.872054	30700.618350	31.346970
530.378144	30762.655074	31.351988
531.053145	30801.234101	31.357005
531.617159	30872.906771	31.362023
532.126300	30922.985641	31.367040
533.238953	30968.414720	31.372058
534.076260	31006.339373	31.377076
534.882753	31026.294321	31.382093
535.412805	31068.494878	31.387111
536.046926	31104.860130	31.392128
536.782041	31145.641702	31.397146
537.087677	31186.027721	31.402164
537.435953	31218.013958	31.407181
538.014792	31246.024288	31.412199
538.111409	31290.001155	31.417216
538.788107	31332.127509	31.422234
539.172366	31378.735601	31.427252
539.540902	31411.965134	31.432269
540.402634	31472.329829	31.437287
540.658008	31517.669201	31.442304
541.199924	31560.607293	31.447322
541.359294	31616.327847	31.452340
541.925534	31669.516750	31.457357
542.342001	31724.339875	31.462375
542.838592	31782.150540	31.467392
543.330105	31831.051685	31.472410
543.956279	31889.566901	31.477428
544.464677	31938.916748	31.482445
545.281560	31982.008989	31.487463
546.244112	32041.197730	31.492480
547.275133	32068.509524	31.497498
547.580922	32107.739617	31.502516
548.557998	32147.656629	31.507533
549.223635	32181.380996	31.512551
549.416949	32222.731488	31.517568
550.135208	32252.260084	31.522586
550.648707	32295.188904	31.527604
551.193073	32335.105620	31.532621
551.420439	32367.022509	31.537639
551.903762	32416.876406	31.542656
552.383291	32451.881731	31.547674
552.859624	32507.063367	31.552692
552.846981	32538.875270	31.557709
553.344188	32591.015031	31.562727
553.524645	32643.390558	31.567744
554.081213	32689.266671	31.572762
554.863160	32744.328876	31.577780
555.356083	32789.875029	31.582797
555.751847	32835.882354	31.587815
556.602642	32885.966852	31.592832
556.977873	32943.448046	31.597850
557.694706	33003.933539	31.602868
557.863675	33047.375782	31.607885
558.724271	33101.791778	31.612903
558.757484	33163.931226	31.617920
559.307203	33216.060946	31.622938
560.068449	33281.450030	31.627956
560.561676	33348.597330	31.632973
560.902805	33396.603183	31.637991
561.470588	33465.448864	31.643008
562.632855	33524.328548	31.648026
562.873362	33589.060511	31.653044
563.383580	33652.675012	31.658061
563.609631	33700.984799	31.663079
564.151374	33771.454822	31.668096
565.158362	33822.260753	31.673114
566.133783	33901.741234	31.678132
566.660783	33957.193496	31.683149
566.940173	34026.420575	31.688167
567.621290	34088.392542	31.693184
568.313351	34145.443162	31.698202
568.845287	34203.969027	31.703220
569.946407	34263.271551	31.708237
570.375469	34307.913873	31.713255
571.189047	34353.344509	31.718272
571.843309	34394.068091	31.723290
572.424315	34457.156161	31.728308
572.951225	34501.438742	31.733325
573.540377	34557.302263	31.738343
573.504561	34613.367563	31.743360
574.479088	34666.494482	31.748378
574.953095	34729.617058	31.753396
575.470804	34776.035172	31.758413
575.938303	34840.080716	31.763431
577.067629	34893.135267	31.768448
577.696732	34939.437477	31.773466
578.336730	34979.934385	31.778484
578.912928	35032.617286	31.783501
579.676752	35080.992984	31.788519
580.503572	35135.818434	31.793536
580.997566	35170.763581	31.798554
581.625253	35217.477010	31.803572
581.961119	35261.392393	31.808589
582.411897	35316.782626	31.813607
582.670356	35373.852354	31.818624
583.423821	35416.707817	31.823642
583.893050	35480.723801	31.828660
584.457545	35527.372786	31.833677
585.254536	35585.587740	31.838695
585.511538	35640.559844	31.843712
586.297856	35685.566020	31.848730
586.644057	35738.753111	31.853748
587.166727	35812.213576	31.858765
587.754038	35857.852867	31.863783
587.662868	35925.914804	31.868800
588.350992	35976.770334	31.873818
589.224942	36054.970620	31.878836
589.565002	36118.271804	31.883853
590.342356	36184.558824	31.888871
590.707765	36241.559888	31.893888
591.410576	36305.480051	31.898906
592.074663	36369.141759	31.903924
592.469689	36432.545381	31.908941
593.091792	36481.084091	31.913959
593.349058	36551.807943	31.918976
594.278950	36607.425577	31.923994
595.214653	36676.127803	31.929012
594.979643	36735.477297	31.934029
595.772032	36794.678486	31.939047
596.065299	36869.323875	31.944064
596.596917	36932.312046	31.949082
597.440254	36993.238176	31.954100
598.060645	37073.789003	31.959117
598.731861	37137.076641	31.964135
599.187928	37208.331855	31.969152
599.781283	37275.231019	31.974170
600.545502	37347.761241	31.979188
601.129033	37423.484345	31.984205
602.138746	37482.979953	31.989223
602.163108	37557.123627	31.994240
603.217039	37619.437231	31.999258
604.021725	37682.433169	32.004276
604.933862	37744.922252	32.009293
606.142873	37792.568476	32.014311
607.260203	37829.305923	32.019328
608.036586	37877.551315	32.024346
608.578622	37915.394492	32.029364
608.924141	37970.813491	32.034381
609.544878	38011.137336	32.039399
610.395290	38065.762607	32.044416
610.710031	38106.639337	32.049434
611.368173	38154.037087	32.054452
611.782038	38211.020516	32.059469
612.414121	38258.451272	32.064487
612.643525	38316.655630	32.069504
613.122845	38367.918695	32.074522
613.553855	38436.471501	32.079540
613.668056	38495.907637	32.084557
614.621213	38555.753894	32.089575
614.798157	38632.427040	32.094592
615.465097	38710.928832	32.099610
616.290345	38768.587475	32.104628
616.397277	38849.105159	32.109645
617.302101	38916.713053	32.114663
617.693030	38995.214547	32.119680
618.570445	39060.431702	32.124698
619.179263	39144.115454	32.129716
619.968279	39207.018258	32.134733
620.922029	39268.741768	32.139751
621.595499	39334.675590	32.144768
622.211902	39393.785043	32.149786
623.211005	39462.215807	32.154804
623.251967	39521.765289	32.159821
623.947585	39584.830105	32.164839
624.685933	39660.798797	32.169856
625.446219	39721.264880	32.174874
626.019054	39790.335846	32.179892
626.597231	39850.677915	32.184909
627.349696	39905.915260	32.189927
627.661795	39985.996656	32.194944
628.272940	40053.910050	32.199962
629.003813	40113.757278	32.204980
629.345882	40180.386826	32.209997
629.924974	40247.349761	32.215015
630.339662	40326.329677	32.220032
631.186912	40395.344728	32.225050
631.877188	40462.725624	32.230068
632.881993	40519.734923	32.235085
633.448870	40587.812323	32.240103
634.211483	40649.452258	32.245120
635.179436	40693.623062	32.250138
635.816316	40735.689656	32.255156
636.257212	40809.654219	32.260173
636.809303	40848.868719	32.265191
637.652548	40902.117787	32.270208
638.100152	40960.016497	32.275226
639.079365	41014.322971	32.280244
639.228540	41077.521518	32.285261
639.597348	41136.267287	32.290279
640.225621	41199.232017	32.295296
640.848003	41273.042027	32.300314
641.381036	41329.014604	32.305332
641.840923	41395.161752	32.310349
643.237535	41450.255746	32.315367
643.882235	41518.389955	32.320384
644.472687	41576.213212	32.325402
645.224500	41643.594519	32.330420
645.532894	41710.497215	32.335437
646.140989	41766.045085	32.340455
646.563850	41828.398871	32.345472
647.545439	41910.821009	32.350490
647.970355	41978.055757	32.355508
648.310968	42050.794894	32.360525
648.962935	42118.816452	32.365543
649.614026	42197.436779	32.370560
650.159696	42272.655790	32.375578
650.662138	42355.535152	32.380596
651.297968	42439.393551	32.385613
651.999348	42514.215146	32.390631
652.360394	42603.783839	32.395648
652.936544	42672.782948	32.400666
654.129734	42749.272912	32.405684
655.357608	42823.076968	32.410701
656.172718	42899.933416	32.415719
656.583931	42965.598559	32.420736
657.830143	43021.394694	32.425754
659.199027	43064.866843	32.430772
659.973904	43131.927686	32.435789
660.724885	43175.117495	32.440807
661.116169	43241.276296	32.445824
661.357827	43289.504695	32.450842
662.316095	43344.127737	32.455860
662.282805	43405.795323	32.460877
663.106738	43472.694541	32.465895
663.711862	43533.808219	32.470912
664.439957	43602.274058	32.475930
664.726361	43665.326011	32.480948
665.284391	43740.918310	32.485965
666.148992	43810.461010	32.490983
666.718845	43878.373177	32.496000
667.374712	43950.991615	32.501018
668.247435	44002.334467	32.506036
668.940362	44080.813712	32.511053
669.936477	44142.881157	32.516071
670.371568	44206.462796	32.521088
670.897721	44278.769353	32.526106
672.110329	44338.351323	32.531124
672.455400	44411.613591	32.536141
673.094354	44475.219131	32.541159
673.561585	44542.692909	32.546176
673.961204	44616.729980	32.551194
674.596488	44675.199544	32.556212
675.268875	44756.877279	32.561229
675.729227	44822.638665	32.566247
676.427446	44904.019099	32.571264
676.831457	44982.439567	32.576282
677.588581	45050.485923	32.581300
678.100419	45118.952159	32.586317
678.794833	45198.443101	32.591335
679.352827	45280.401023	32.596352
679.859551	45362.857246	32.601370
680.705693	45432.206936	32.606388
681.107811	45510.478349	32.611405
681.688843	45595.259918	32.616423
682.420195	45668.671354	32.621440
682.585151	45767.647093	32.626458
683.480841	45853.678554	32.631476
683.931829	45942.777763	32.636493
684.656104	46026.609114	32.641511
686.034414	46110.329098	32.646528
686.641166	46195.484863	32.651546
687.677944	46289.768249	32.656564
687.898790	46367.520691	32.661581
688.669329	46457.835552	32.666599
689.205704	46549.114962	32.671616
690.248812	46630.638209	32.676634
691.100926	46702.533636	32.681652
691.416794	46799.658155	32.686669
692.482943	46886.408113	32.691687
693.214728	46961.479226	32.696704
693.778511	47059.362863	32.701722
694.540197	47134.849700	32.706740
695.693956	47227.138307	32.711757
696.304328	47299.837193	32.716775
697.034457	47365.458423	32.721792
698.183308	47448.429768	32.726810
698.931287	47512.911671	32.731828
699.902311	47593.791004	32.736845
700.471656	47656.594571	32.741863
701.037260	47729.864658	32.746880
701.385304	47802.087939	32.751898
702.584001	47885.182393	32.756916
703.787185	47948.548046	32.761933
704.264174	48033.989396	32.766951
704.928123	48089.177196	32.771968
705.206356	48166.813772	32.776986
705.934963	48244.075874	32.782004
706.345295	48330.148603	32.787021
707.127124	48398.866088	32.792039
707.759815	48484.649947	32.797056
708.341722	48562.351407	32.802074
709.601561	48626.414178	32.807092
710.367401	48702.759241	32.812109
711.362398	48780.032975	32.817127
711.785862	48839.678028	32.822144
712.538932	48924.518519	32.827162
713.766134	48986.295046	32.832180
714.544067	49058.413805	32.837197
714.714574	49119.317645	32.842215
715.789906	49197.353500	32.847232
716.455447	49274.020683	32.852250
717.014215	49331.206611	32.857268
717.481311	49413.001614	32.862285
717.878991	49490.800586	32.867303
719.333051	49557.701984	32.872320
719.341777	49640.110961	32.877338
720.167349	49719.858006	32.882356
720.795770	49802.764891	32.887373
721.252936	49876.926586	32.892391
722.148770	49957.970521	32.897408
722.790451	50036.463939	32.902426
723.715238	50124.967083	32.907444
724.251770	50190.945981	32.912461
725.632922	50259.703292	32.917479
726.688415	50330.826899	32.922496
726.707798	50398.531594	32.927514
727.490717	50467.673220	32.932532
728.532781	50529.589677	32.937549
729.247601	50597.858699	32.942567
730.031698	50662.995856	32.947584
729.975031	50734.349793	32.952602
730.532411	50790.036827	32.957620
731.096448	50876.404967	32.962637
731.497659	50958.182714	32.967655
732.309126	51040.537050	32.972672
732.594762	51143.648797	32.977690
733.545409	51228.867776	32.982708
734.230017	51330.480282	32.987725
734.914841	51407.310670	32.992743
736.054441	51505.203503	32.997760
736.415126	51600.926629	33.002778
737.069971	51694.099724	33.007796
737.953729	51793.262046	33.012813
738.709389	51887.006846	33.017831
739.250733	51982.228051	33.022848
739.735920	52083.883916	33.027866
740.710011	52174.416149	33.032884
742.004396	52268.067037	33.037901
742.612324	52370.493714	33.042919
743.554163	52457.962281	33.047936
744.159200	52555.987047	33.052954
745.132691	52644.594688	33.057972
745.727889	52735.792603	33.062989
746.618865	52834.807402	33.068007
747.785025	52915.455554	33.073024
748.515363	53017.265116	33.078042
749.053138	53097.165430	33.083060
749.783535	53188.185067	33.088077
749.969894	53288.930177	33.093095
751.044532	53389.976923	33.098112
751.641624	53488.734238	33.103130
752.591015	53575.397856	33.108148
753.736690	53668.126131	33.113165
754.091703	53760.682829	33.118183
755.252347	53854.249796	33.123200
755.909817	53945.171326	33.128218
756.803660	54037.216571	33.133236
757.507288	54125.363942	33.138253
758.057299	54213.954206	33.143271
758.815225	54303.142175	33.148288
759.773390	54397.844706	33.153306
761.196098	54483.580803	33.158324
761.598570	54569.973137	33.163341
762.485281	54656.405514	33.168359
763.609130	54742.501945	33.173376
764.305471	54827.987335	33.178394
764.805066	54914.497740	33.183412
765.638713	54990.540329	33.188429
766.235875	55085.445092	33.193447
767.070382	55182.421283	33.198464
767.611969	55270.240516	33.203482
768.145277	55365.327821	33.208500
769.239828	55454.945325	33.213517
769.508659	55544.946724	33.218535
770.326187	55626.902316	33.223552
770.875934	55740.432733	33.228570
771.430669	55835.853625	33.233588
772.530226	55927.355402	33.238605
773.136634	56038.995145	33.243623
774.225942	56126.537689	33.248640
775.031182	56217.716851	33.253658
775.966619	56314.391160	33.258676
777.088841	56397.506254	33.263693
777.428779	56493.326132	33.268711
778.603346	56560.149448	33.273728
778.788254	56641.095787	33.278746
779.592302	56724.524138	33.283764
780.438708	56797.348867	33.288781
781.037668	56903.693067	33.293799
782.167277	56985.425525	33.298816
782.950230	57078.615466	33.303834
783.243176	57167.621784	33.308852
784.028510	57256.572043	33.313869
784.386492	57354.023392	33.318887
785.265900	57460.519898	33.323904
785.825395	57560.965700	33.328922
786.969368	57661.927957	33.333940
788.300674	57746.922385	33.338957
788.700047	57853.159419	33.343975
789.590560	57937.431590	33.348992
790.620751	58021.649333	33.354010
791.270888	58125.678641	33.359028
792.395681	58209.704528	33.364045
792.961624	58314.336496	33.369063
794.437449	58398.254351	33.374080
795.131540	58492.805352	33.379098
795.758913	58579.860250	33.384116
796.930053	58663.760274	33.389133
797.920743	58758.964768	33.394151
798.867683	58832.506967	33.399168
799.393442	58918.897678	33.404186
799.905637	59002.333401	33.409204
801.123827	59092.717715	33.414221
801.887785	59190.527684	33.419239
802.417683	59265.865976	33.424256
803.237997	59361.461823	33.429274
803.689418	59453.036748	33.434292
804.893656	59547.653377	33.439309
805.226284	59651.294553	33.444327
805.679271	59745.784009	33.449344
806.640114	59847.754579	33.454362
807.560175	59952.348901	33.459380
808.215985	60051.735699	33.464397
809.098960	60153.038170	33.469415
810.043255	60265.081409	33.474432
810.651149	60351.357162	33.479450
811.174142	60471.592798	33.484468
812.341279	60562.535686	33.489485
812.931185	60672.402656	33.494503
813.595629	60775.697446	33.499520
814.575952	60887.415804	33.504538
816.324337	60972.127072	33.509556
817.560848	61053.504365	33.514573
818.399771	61140.863816	33.519591
819.416091	61219.838669	33.524608
820.038975	61301.856036	33.529626
820.942025	61390.760731	33.534644
822.006896	61473.135215	33.539661
822.819528	61560.538751	33.544679
823.659257	61639.203233	33.549696
824.341497	61730.642656	33.554714
824.964309	61822.395738	33.559732
825.570028	61900.543858	33.564749
826.346430	61988.966531	33.569767
827.066782	62072.904920	33.574784
827.937390	62152.324726	33.579802
828.738823	62243.468547	33.584820
829.329544	62349.482465	33.589837
830.116866	62443.783556	33.594855
830.780811	62524.117688	33.599872
831.871098	62634.948760	33.604890
832.322112	62726.797611	33.609908
833.125557	62808.689910	33.614925
833.721033	62901.767094	33.619943
834.074634	62995.175607	33.624960
835.091812	63087.406165	33.629978
835.937070	63195.866329	33.634996
836.698610	63291.692621	33.640013
837.219085	63404.050958	33.645031
838.090953	63507.084889	33.650048
838.725557	63617.693472	33.655066
839.307860	63736.844867	33.660084
840.132971	63849.793500	33.665101
840.806520	63964.594735	33.670119
841.796203	64086.714712	33.675136
842.615838	64205.102467	33.680154
843.232150	64332.418745	33.685172
844.353561	64442.622229	33.690189
845.155576	64573.651409	33.695207
846.122843	64681.466971	33.700224
847.177787	64803.624588	33.705242
848.107900	64921.840058	33.710260
849.528865	65034.481317	33.715277
850.714772	65139.500457	33.720295
851.618657	65247.576017	33.725312
852.717817	65354.311149	33.730330
853.409732	65454.811719	33.735348
854.543619	65549.265418	33.740365
855.421114	65647.605706	33.745383
856.339024	65744.713330	33.750400
857.245603	65860.757030	33.755418
858.039781	65954.971823	33.760436
858.803127	66052.871472	33.765453
859.606602	66152.370674	33.770471
861.041624	66249.312634	33.775488
862.249791	66336.898304	33.780506
863.051288	66431.581852	33.785524
864.106904	66513.541749	33.790541
865.037077	66601.908016	33.795559
866.037085	66698.544935	33.800576
866.813678	66781.234968	33.805594
867.370780	66883.225170	33.810612
868.161608	66964.516379	33.815629
868.879092	67073.264520	33.820647
869.183888	67163.317479	33.825664
869.872600	67268.467762	33.830682
870.388772	67389.452816	33.835700
871.147232	67504.291028	33.840717
871.996725	67615.605872	33.845735
872.557761	67733.266236	33.850752
873.272960	67857.508563	33.855770
874.104621	67977.780777	33.860788
875.261442	68098.998658	33.865805
876.004383	68220.589404	33.870823
876.741143	68340.670789	33.875840
878.152776	68455.051701	33.880858
878.935697	68581.051031	33.885876
880.142397	68683.232955	33.890893
881.132939	68803.805946	33.895911
882.405383	68924.168446	33.900928
883.164422	69035.663836	33.905946
883.782998	69149.895591	33.910964
884.878305	69258.819880	33.915981
885.649405	69376.543017	33.920999
886.479985	69492.638278	33.926016
887.372569	69601.041549	33.931034
887.591128	69720.053313	33.936052
888.367564	69838.834047	33.941069
889.353324	69960.015062	33.946087
889.742405	70081.011252	33.951104
890.797177	70189.333685	33.956122
891.622379	70320.502241	33.961140
892.658993	70428.512743	33.966157
893.243333	70553.873788	33.971175
893.916937	70681.288446	33.976192
894.902480	70802.215011	33.981210
895.872207	70921.671555	33.986228
896.967375	71052.224363	33.991245
897.613101	71186.539078	33.996263
898.307546	71309.932340	34.001280
899.595088	71434.043603	34.006298
900.366372	71558.007291	34.011316
901.932608	71677.236243	34.016333
902.950790	71802.399771	34.021351
903.950857	71935.016222	34.026368
905.068732	72032.214279	34.031386
906.121204	72150.424477	34.036404
907.344575	72265.603208	34.041421
907.991325	72380.353377	34.046439
909.536568	72483.654496	34.051456
910.612122	72588.703535	34.056474
911.094097	72688.912692	34.061492
912.563624	72791.114855	34.066509
914.020245	72886.964151	34.071527
914.599488	72977.609460	34.076544
915.366406	73073.257844	34.081562
915.972012	73185.584390	34.086580
917.161398	73272.670470	34.091597
918.395997	73390.654842	34.096615
919.027216	73493.480057	34.101632
919.978675	73594.437604	34.106650
920.429693	73707.829647	34.111668
921.201349	73808.508142	34.116685
922.361500	73924.427118	34.121703
923.768238	74010.208922	34.126720
924.989862	74106.317617	34.131738
926.063141	74211.457089	34.136756
926.458588	74309.044522	34.141773
927.571253	74418.384101	34.146791
927.682393	74528.845405	34.151808
928.956769	74636.786856	34.156826
929.691798	74751.092156	34.161844
930.461511	74868.231971	34.166861
931.187385	74987.137890	34.171879
931.529784	75111.502898	34.176896
932.905785	75225.735923	34.181914
933.323593	75357.818406	34.186932
933.916689	75488.253488	34.191949
934.918946	75623.308014	34.196967
935.460142	75766.124390	34.201984
936.338816	75902.611543	34.207002
937.108565	76043.760004	34.212020
937.966534	76199.947802	34.217037
939.030413	76334.838334	34.222055
940.209854	76487.205195	34.227072
941.158678	76616.209072	34.232090
942.071419	76765.959307	34.237108
942.844548	76915.638844	34.242125
944.088762	77060.351937	34.247143
944.584365	77211.477361	34.252160
945.475106	77340.969470	34.257178
946.712155	77497.691734	34.262196
948.154671	77634.292057	34.267213
949.590653	77764.644936	34.272231
950.351101	77898.222729	34.277248
951.831547	78023.667631	34.282266
952.750643	78160.048092	34.287284
953.550385	78277.017509	34.292301
954.558403	78395.863261	34.297319
954.936855	78519.804921	34.302336
956.535016	78620.159439	34.307354
957.821338	78722.375258	34.312372
958.600954	78832.898869	34.317389
959.935430	78942.382110	34.322407
960.342072	79073.261335	34.327424
961.295499	79188.603294	34.332442
961.955294	79312.610179	34.337460
962.803703	79436.440957	34.342477
963.592624	79561.243804	34.347495
964.088270	79702.966952	34.352512
965.021059	79832.966227	34.357530
966.380248	79972.650017	34.362548
967.557298	80101.914461	34.367565
968.994789	80214.726886	34.372583
969.941340	80342.651897	34.377600
971.097898	80479.310663	34.382618
972.233325	80599.329874	34.387636
973.491750	80707.670315	34.392653
974.925969	80818.158290	34.397671
975.614953	80943.023303	34.402688
976.849585	81050.471015	34.407706
977.802955	81155.650510	34.412724
978.962967	81268.754627	34.417741
979.773323	81389.388668	34.422759
980.504071	81504.804693	34.427776
981.812622	81618.632407	34.432794
982.584712	81746.834678	34.437812
983.213988	81858.789821	34.442829
984.439807	81971.196927	34.447847
985.353852	82097.125395	34.452864
986.408571	82205.576362	34.457882
987.341770	82335.804995	34.462900
988.268943	82458.842043	34.467917
989.131634	82561.582027	34.472935
989.656089	82704.147875	34.477952
990.485925	82832.662979	34.482970
991.388015	82976.762182	34.487988
992.238330	83112.051372	34.493005
993.125004	83249.423168	34.498023
993.891524	83394.642019	34.503040
995.031337	83544.462753	34.508058
996.109455	83687.537547	34.513076
996.714369	83844.661675	34.518093
998.223339	83976.885632	34.523111
999.599865	84121.976205	34.528128
1001.039152	84248.854281	34.533146
1002.297488	84373.700442	34.538164
1003.519275	84497.414457	34.543181
1004.455633	84627.503667	34.548199
1005.108921	84760.228405	34.553216
1006.173020	84882.217999	34.558234
1007.189456	85009.822111	34.563252
1008.148685	85137.480707	34.568269
1009.526957	85260.046559	34.573287
1010.141458	85404.493331	34.578304
1011.155167	85519.135877	34.583322
1012.393605	85650.395548	34.588340
1013.416097	85774.332922	34.593357
1014.071945	85903.881024	34.598375
1014.991520	86044.446657	34.603392
1015.902455	86179.857575	34.608410
1016.915209	86314.581654	34.613428
1017.466335	86464.620133	34.618445
1018.588548	86592.538055	34.623463
1019.313824	86745.365262	34.628480
1020.110720	86882.406405	34.633498
1021.098425	87015.411175	34.638516
1021.901116	87158.742821	34.643533
1022.914865	87284.815787	34.648551
1023.863807	87443.109351	34.653568
1024.704371	87573.281458	34.658586
1026.002842	87730.183750	34.663604
1026.887240	87874.676869	34.668621
1027.913763	88012.515451	34.673639
1029.035099	88156.774808	34.678656
1029.948728	88314.181468	34.683674
1031.093009	88464.058302	34.688692
1032.192755	88608.393599	34.693709
1033.371226	88739.326064	34.698727
1034.099935	88912.372917	34.703744
1035.138488	89054.803593	34.708762
1036.172428	89217.689294	34.713780
1037.370164	89372.334602	34.718797
1038.636996	89516.799566	34.723815
1039.322125	89688.808752	34.728832
1040.647871	89826.361384	34.733850
1041.900733	89970.090963	34.738868
1043.320638	90123.419561	34.743885
1044.399350	90275.255222	34.748903
1045.068996	90425.438301	34.753920
1046.106699	90576.162484	34.758938
1047.639243	90736.355681	34.763956
1048.312878	90892.692618	34.768973
1049.605758	91043.320430	34.773991
1050.544203	91191.995390	34.779008
1051.691029	91351.231386	34.784026
1052.675299	91508.501764	34.789044
1053.438228	91662.208657	34.794061
1054.511902	91805.934627	34.799079
1055.309597	91973.295904	34.804096
1056.448156	92134.221972	34.809114
1057.548662	92290.826238	34.814132
1058.027541	92462.800819	34.819149
1059.155181	92624.605384	34.824167
1059.916224	92803.168663	34.829184
1060.986933	92985.739014	34.834202
1062.208699	93159.063671	34.839220
1063.145736	93352.127836	34.844237
1064.444461	93515.080876	34.849255
1065.171281	93694.441207	34.854272
1066.374672	93884.287927	34.859290
1067.475323	94051.841061	34.864308
1068.038217	94240.910649	34.869325
1069.416778	94419.933947	34.874343
1070.694907	94604.406188	34.879360
1071.994358	94789.110478	34.884378
1073.018809	94958.442126	34.889396
1074.293205	95138.044952	34.894413
1075.744941	95308.814639	34.899431
1077.009303	95480.907920	34.904448
1077.939868	95647.879770	34.909466
1079.779754	95802.529059	34.914484
1080.768992	95974.671411	34.919501
1082.279271	96126.364246	34.924519
1083.386329	96291.760244	34.929536
1084.305327	96444.439349	34.934554
1085.354694	96601.623940	34.939572
1086.349638	96761.173445	34.944589
1087.692771	96911.461799	34.949607
1089.394696	97057.747669	34.954624
1090.845909	97196.124916	34.959642
1093.020226	97295.627628	34.964660
1093.987444	97422.280049	34.969677
1095.078841	97537.675764	34.974695
1095.968478	97660.607230	34.979712
1096.890929	97771.961483	34.984730
1097.844872	97878.550360	34.989748
1098.288058	98007.090572	34.994765
1099.258941	98123.274982	34.999783
1100.049378	98263.882199	35.004800
1100.787079	98392.267892	35.009818
1101.964588	98534.768612	35.014836
1102.422402	98680.903153	35.019853
1103.275368	98829.182460	35.024871
1104.168595	98979.437534	35.029888
1104.488210	99150.712485	35.034906
1105.997426	99308.698719	35.039924
1106.562559	99480.042787	35.044941
1107.822141	99637.983850	35.049959
1109.163642	99809.302634	35.054976
1110.050503	99989.928841	35.059994
1111.472773	100164.205932	35.065012
1112.507791	100346.468863	35.070029
1113.551448	100515.974084	35.075047
1115.042265	100689.958482	35.080064
1115.723140	100866.104474	35.085082
1117.124282	101041.549694	35.090100
1117.875073	101227.152056	35.095117
1118.918534	101410.795085	35.100135
1120.200185	101603.561690	35.105152
1121.092268	101783.433548	35.110170
1122.603797	101964.609525	35.115188
1123.565108	102155.312291	35.120205
1125.047983	102323.534543	35.125223
1126.396199	102511.997633	35.130240
1128.000213	102675.560875	35.135258
1129.169981	102855.438445	35.140276
1130.202548	103042.248146	35.145293
1131.288029	103217.488242	35.150311
1132.253710	103397.010833	35.155328
1133.640200	103575.660680	35.160346
1134.512874	103747.406359	35.165364
1135.693009	103933.932022	35.170381
1136.931461	104112.724080	35.175399
1138.291809	104289.382175	35.180416
1138.758326	104473.965763	35.185434
1140.381891	104643.845048	35.190452
1141.190520	104841.051746	35.195469
1142.041018	105019.863682	35.200487
1143.200864	105214.785910	35.205504
1144.629358	105390.211603	35.210522
1146.001666	105573.538116	35.215540
1147.274228	105772.903868	35.220557
1148.365258	105950.187712	35.225575
1149.838224	106121.456681	35.230592
1151.797344	106283.324371	35.235610
1153.606978	106437.073946	35.240628
1154.706794	106613.296864	35.245645
1155.490715	106775.299176	35.250663
1156.634211	106940.979209	35.255680
1157.542615	107094.223466	35.260698
1158.680756	107263.072834	35.265716
1159.547857	107444.216203	35.270733
1160.404986	107612.025117	35.275751
1161.256164	107789.500313	35.280768
1162.131572	107971.304502	35.285786
1163.320568	108164.938882	35.290804
1164.018985	108348.611595	35.295821
1164.924923	108544.613607	35.300839
1166.369375	108731.762453	35.305856
1167.439810	108934.136619	35.310874
1168.325462	109099.999409	35.315892
1169.594442	109296.111316	35.320909
1170.895935	109466.784098	35.325927
1172.477997	109644.289584	35.330944
1173.207277	109828.879246	35.335962
1174.231312	110011.787202	35.340980
1175.374016	110199.490253	35.345997
1177.527440	110362.414326	35.351015
1179.281443	110527.419747	35.356032
1180.114775	110705.816396	35.361050
1181.622225	110867.710569	35.366068
1183.257862	111032.421984	35.371085
1184.611618	111190.935971	35.376103
1185.677704	111352.893555	35.381120
1186.342289	111526.357765	35.386138
1187.238122	111694.122142	35.391156
1188.308053	111871.283662	35.396173
1189.448672	112050.689515	35.401191
1190.539640	112223.415972	35.406208
1191.357840	112420.752510	35.411226
1192.581545	112609.776091	35.416244
1193.355722	112807.059338	35.421261
1194.375821	113004.163840	35.426279
1195.566492	113208.247193	35.431296
1196.393048	113408.680505	35.436314
1197.774335	113604.221764	35.441332
1198.890332	113805.015313	35.446349
1200.727890	114018.473626	35.451367
1202.093043	114214.553929	35.456384
1203.160219	114411.128450	35.461402
1204.751329	114612.317737	35.466420
1205.841221	114808.574539	35.471437
1206.986757	115009.118419	35.476455
1208.244286	115212.267741	35.481472
1209.228354	115416.667497	35.486490
1210.421835	115615.877422	35.491508
1211.761458	115827.366885	35.496525
1212.926897	116034.224295	35.501543
1214.676688	116240.466815	35.506560
1215.543521	116448.593089	35.511578
1216.777685	116648.614395	35.516596
1218.140458	116862.236301	35.521613
1218.952372	117060.607376	35.526631
1220.335509	117271.226087	35.531648
1220.979472	117482.767196	35.536666
1222.123585	117711.547661	35.541684
1223.322787	117923.899536	35.546701
1224.507206	118148.964269	35.551719
1225.817227	118367.661791	35.556736
1226.923443	118606.617731	35.561754
1227.953580	118825.200413	35.566772
1228.741980	119058.485447	35.571789
1230.075869	119279.884870	35.576807
1231.247510	119509.004444	35.581824
1232.836689	119744.290956	35.586842
1234.148982	119984.516541	35.591860
1235.619296	120220.105379	35.596877
1236.628036	120437.208441	35.601895
1238.197805	120670.161335	35.606912
1239.818326	120898.887874	35.611930
1240.725543	121116.709758	35.616948
1242.275436	121334.781477	35.621965
1243.535224	121573.546120	35.626983
1244.955798	121788.740681	35.632000
1245.561421	122031.533292	35.637018
1246.941566	122250.121469	35.642036
1248.387659	122480.828089	35.647053
1249.317544	122705.285716	35.652071
1250.600490	122917.317733	35.657088
1251.530926	123141.284305	35.662106
1252.670482	123362.594541	35.667124
1253.778739	123582.745672	35.672141
1254.483355	123811.456450	35.677159
1256.267468	124023.945453	35.682176
1257.166934	124260.573521	35.687194
1258.442396	124482.528479	35.692212
1259.639743	124717.323750	35.697229
1260.992671	124946.239769	35.702247
1262.550125	125184.299454	35.707264
1263.264229	125421.081398	35.712282
1265.077367	125649.178624	35.717300
1266.776199	125877.676742	35.722317
1268.032225	126109.000318	35.727335
1270.249884	126329.126822	35.732352
1271.196210	126560.416455	35.737370
1272.617463	126778.764441	35.742388
1274.037242	127008.267864	35.747405
1274.900540	127230.260479	35.752423
1276.252527	127452.477834	35.757440
1277.368556	127687.119271	35.762458
1278.859777	127905.653752	35.767476
1280.204503	128139.411462	35.772493
1281.537812	128360.649775	35.777511
1283.117088	128580.175736	35.782528
1284.370484	128804.713344	35.787546
1286.455339	129015.640701	35.792564
1288.583571	129215.027587	35.797581
1289.849267	129418.995247	35.802599
1292.165518	129594.333158	35.807616
1293.112164	129791.676089	35.812634
1294.395239	129985.732130	35.817652
1295.360754	130173.757610	35.822669
1296.714503	130388.859057	35.827687
1297.583708	130581.339524	35.832704
1298.846010	130798.347651	35.837722
1299.866242	131002.416965	35.842740
1300.952498	131210.659817	35.847757
1301.913653	131427.899656	35.852775
1302.994691	131642.066064	35.857792
1303.704691	131856.358825	35.862810
1304.916156	132093.121599	35.867828
1305.777156	132326.990565	35.872845
1307.205632	132577.741399	35.877863
1308.599569	132806.885750	35.882880
1309.613324	133054.970863	35.887898
1310.724241	133291.581653	35.892916
1311.987023	133539.806665	35.897933
1312.941989	133801.357774	35.902951
1315.005421	134050.962515	35.907968
1316.339818	134293.983675	35.912986
1317.872060	134528.543231	35.918004
1318.993494	134780.604426	35.923021
1320.132240	135016.639963	35.928039
1322.070381	135263.853295	35.933056
1323.364765	135506.788668	35.938074
1324.605638	135753.081718	35.943092
1325.961556	135998.850399	35.948109
1327.410128	136237.429647	35.953127
1328.435821	136483.282044	35.958144
1330.052352	136726.312412	35.963162
1331.271737	136974.925581	35.968180
1332.691926	137216.394591	35.973197
1333.474089	137476.355303	35.978215
1334.896153	137731.064310	35.983232
1336.175248	137976.644781	35.988250
1337.217095	138217.296220	35.993268
1338.678905	138460.542343	35.998285
1339.474444	138715.134473	36.003303
1341.220897	138946.519885	36.008320
1342.301753	139194.158093	36.013338
1343.687482	139429.917610	36.018356
1345.706725	139660.552602	36.023373
1346.821778	139904.411803	36.028391
1348.471733	140147.017504	36.033408
1349.729060	140386.367924	36.038426
1351.047874	140620.434978	36.043444
1352.596400	140863.455644	36.048461
1353.490507	141118.556545	36.053479
1354.585230	141350.865150	36.058496
1356.070861	141604.426003	36.063514
1357.641828	141855.654055	36.068532
1359.409089	142103.021879	36.073549
1360.709363	142345.574216	36.078567
1362.600917	142592.366960	36.083584
1363.515967	142837.421273	36.088602
1364.804094	143089.288424	36.093620
1366.203933	143334.811093	36.098637
1367.594201	143588.757232	36.103655
1368.615014	143842.297265	36.108672
1370.033223	144098.804014	36.113690
1371.301017	144363.352116	36.118708
1372.299005	144631.294806	36.123725
1373.329793	144905.486027	36.128743
1374.900627	145168.036912	36.133760
1376.233880	145444.058977	36.138778
1377.732864	145724.113840	36.143796
1379.169413	146000.643006	36.148813
1380.395450	146278.908581	36.153831
1381.555144	146557.314120	36.158848
1383.493414	146824.102686	36.163866
1384.945835	147102.032675	36.168884
1386.124576	147374.188985	36.173901
1388.565375	147633.760017	36.178919
1391.296054	147867.590098	36.183936
1393.614144	148093.132280	36.188954
1395.501737	148331.074767	36.193972
1397.789372	148546.351843	36.198989
1399.286908	148751.323253	36.204007
1400.646199	148949.710953	36.209024
1402.475499	149158.599346	36.214042
1403.580387	149354.329935	36.219060
1405.034931	149549.077713	36.224077
1406.080932	149768.080994	36.229095
1407.093451	149979.874364	36.234112
1408.463957	150184.494254	36.239130
1409.403138	150413.919323	36.244148
1410.890421	150622.644334	36.249165
1411.800516	150848.563572	36.254183
1412.818767	151075.734589	36.259200
1413.789761	151309.180535	36.264218
1415.727281	151527.006185	36.269236
1417.283521	151753.039315	36.274253
1418.579197	151994.363025	36.279271
1420.071072	152227.817042	36.284288
1420.923687	152459.843715	36.289306
1421.667882	152703.711374	36.294324
1423.060991	152950.314247	36.299341
1424.087401	153212.771445	36.304359
1424.964656	153470.840999	36.309376
1426.450410	153733.098729	36.314394
1427.016358	154008.905635	36.319412
1429.012129	154265.336299	36.324429
1430.491112	154536.391034	36.329447
1431.968980	154808.437254	36.334464
1433.501246	155058.937392	36.339482
1434.821577	155316.197309	36.344500
1436.375983	155564.908425	36.349517
1437.638597	155814.443287	36.354535
1438.640382	156070.543174	36.359552
1440.243933	156334.130750	36.364570
1440.940748	156616.314976	36.369588
1442.636360	156876.859078	36.374605
1443.751882	157165.815240	36.379623
1444.793584	157445.563254	36.384640
1446.036167	157733.271929	36.389658
1447.238569	158023.830950	36.394676
1448.582370	158314.533534	36.399693
1450.710438	158609.015465	36.404711
1452.313212	158904.576146	36.409728
1453.968509	159188.509702	36.414746
1455.779742	159495.305451	36.419764
1457.174528	159762.996989	36.424781
1458.584697	160061.680758	36.429799
1460.166767	160360.642667	36.434816
1461.330343	160662.923910	36.439834
1462.498900	160965.701313	36.444852
1464.021347	161268.511053	36.449869
1465.587201	161569.653806	36.454887
1467.025556	161871.771391	36.459904
1468.436680	162183.131886	36.464922
1469.628195	162499.238048	36.469940
1471.703810	162799.061742	36.474957
1473.210853	163118.215915	36.479975
1474.423574	163438.309404	36.484992
1476.424436	163744.457844	36.490010
1477.566773	164062.106283	36.495028
1479.243056	164370.660229	36.500045
1481.295732	164674.129589	36.505063
1483.067948	164974.957735	36.510080
1484.563852	165279.373741	36.515098
1486.107509	165572.250459	36.520116
1488.116819	165852.592126	36.525133
1489.894469	166154.467950	36.530151
1491.424931	166445.500208	36.535168
1492.758947	166735.450374	36.540186
1494.258150	167033.736801	36.545204
1495.600698	167323.892422	36.550221
1497.091423	167620.052504	36.555239
1499.036721	167906.774861	36.560256
1500.369615	168190.263413	36.565274
1501.475359	168499.651496	36.570292
1503.395488	168790.063463	36.575309
1505.266153	169077.871538	36.580327
1506.510995	169358.323947	36.585344
1508.700894	169629.954634	36.590362
1510.305948	169918.471906	36.595380
1511.691725	170202.636807	36.600397
1512.961063	170480.516085	36.605415
1514.271476	170777.944879	36.610432
1515.948702	171057.206619	36.615450
1517.029988	171353.966476	36.620468
1518.496655	171641.375382	36.625485
1519.565689	171938.737412	36.630503
1521.046283	172244.205447	36.635520
1522.829310	172541.122984	36.640538
1523.932661	172848.231044	36.645556
1525.478051	173144.595331	36.650573
1527.065139	173455.561097	36.655591
1528.099754	173764.932659	36.660608
1529.413243	174069.729487	36.665626
1530.583320	174401.697124	36.670644
1531.769968	174711.544503	36.675661
1533.483315	175019.453704	36.680679
1534.582028	175329.789166	36.685696
1536.050394	175642.781170	36.690714
1537.169847	175961.328206	36.695732
1538.863508	176265.504686	36.700749
1540.882390	176580.810008	36.705767
1542.245663	176898.408911	36.710784
1544.252377	177216.715418	36.715802
1545.725062	177529.985174	36.720820
1546.996699	177845.828506	36.725837
1548.245244	178182.377533	36.730855
1549.782101	178509.831884	36.735872
1551.531931	178836.225017	36.740890
1553.253403	179172.917975	36.745908
1555.425860	179477.821435	36.750925
1557.143146	179798.070557	36.755943
1558.403772	180136.623103	36.760960
1560.188797	180454.199741	36.765978
1561.764429	180780.227941	36.770996
1563.234170	181109.004566	36.776013
1565.223647	181433.622857	36.781031
1566.067539	181789.250234	36.786048
1567.620602	182118.641279	36.791066
1569.323564	182467.809936	36.796084
1570.567035	182802.155866	36.801101
1572.215125	183142.757791	36.806119
1573.754594	183481.882125	36.811136
1575.592268	183822.431528	36.816154
1577.147621	184172.739995	36.821172
1579.056658	184502.416635	36.826189
1580.846065	184848.501923	36.831207
1582.271011	185188.887084	36.836224
1583.974140	185526.219914	36.841242
1585.353244	185873.395092	36.846260
1587.418530	186207.168643	36.851277
1588.868055	186543.927681	36.856295
1590.380545	186886.961625	36.861312
1592.146770	187226.883716	36.866330
1594.198394	187563.904436	36.871348
1596.175551	187894.782983	36.876365
1598.309190	188215.913976	36.881383
1599.914587	188553.585699	36.886400
1601.788931	188865.966366	36.891418
1603.133651	189192.857004	36.896436
1604.421510	189518.362532	36.901453
1605.857665	189849.608469	36.906471
1607.176055	190181.053504	36.911488
1608.879106	190513.172901	36.916506
1610.197969	190849.331198	36.921524
1611.089035	191203.867806	36.926541
1612.839063	191546.902443	36.931559
1614.305320	191915.616623	36.936576
1615.861868	192247.896810	36.941594
1617.453789	192613.611107	36.946612
1618.916932	192961.601450	36.951629
1620.577335	193322.027515	36.956647
1621.956233	193686.755170	36.961664
1623.868618	194048.197352	36.966682
1625.066837	194414.254086	36.971700
1626.396265	194783.515786	36.976717
1628.110713	195151.535142	36.981735
1629.495202	195530.897529	36.986752
1630.923298	195911.892642	36.991770
1632.681355	196294.625376	36.996788
1634.207258	196676.345100	37.001805
1635.995640	197054.671871	37.006823
1637.444256	197435.507414	37.011840
1639.151798	197809.979686	37.016858
1640.879575	198179.829386	37.021876
1642.225315	198551.826587	37.026893
1643.826091	198913.715581	37.031911
1645.232085	199281.123514	37.036928
1647.287289	199644.591561	37.041946
1649.756600	199983.387527	37.046964
1652.041673	200329.592255	37.051981
1654.045910	200673.877313	37.056999
1655.555100	201021.991568	37.062016
1657.669147	201362.808365	37.067034
1659.169788	201711.714616	37.072052
1660.691957	202040.850344	37.077069
1663.372327	202381.019491	37.082087
1664.907392	202715.044391	37.087104
1666.575562	203040.897415	37.092122
1668.349238	203375.799967	37.097140
1669.839051	203717.086858	37.102157
1671.148376	204040.413616	37.107175
1672.568768	204396.557908	37.112192
1674.590953	204742.624232	37.117210
1676.451455	205086.306482	37.122228
1677.630034	205436.490012	37.127245
1679.354413	205795.358501	37.132263
1680.438498	206149.090789	37.137280
1682.129981	206517.211747	37.142298
1683.349724	206871.597802	37.147316
1684.982756	207246.702780	37.152333
1686.865544	207609.616571	37.157351
1688.361355	208006.486123	37.162368
1690.074419	208374.421686	37.167386
1691.721589	208766.520962	37.172404
1692.772556	209146.746904	37.177421
1694.154933	209537.877939	37.182439
1695.475332	209945.782363	37.187456
1697.297656	210344.196381	37.192474
1699.780525	210732.649125	37.197492
1701.160420	211137.743200	37.202509
1702.734862	211532.242073	37.207527
1704.283450	211951.991114	37.212544
1706.289657	212352.669696	37.217562
1708.039893	212766.954366	37.222580
1710.006869	213171.706646	37.227597
1712.923403	213556.646170	37.232615
1715.498528	213926.075548	37.237632
1717.579326	214297.975685	37.242650
1719.841126	214662.888496	37.247668
1721.591022	215029.487618	37.252685
1723.764477	215391.141684	37.257703
1725.218902	215765.437286	37.262720
1727.347229	216103.659651	37.267738
1728.810771	216466.933939	37.272756
1730.375539	216820.186086	37.277773
1732.537669	217172.857961	37.282791
1733.881498	217541.896037	37.287808
1735.208204	217909.109667	37.292826
1736.658586	218256.899945	37.297844
1738.047930	218624.080418	37.302861
1739.744947	218995.173376	37.307879
1741.152217	219440.936376	37.312896
1743.346409	219801.180896	37.317914
1745.661743	220158.028563	37.322932
1747.350283	220519.984863	37.327949
1749.473984	220860.763864	37.332967
1751.371911	221227.056454	37.337984
1752.916378	221595.262983	37.343002
1754.409068	221956.113601	37.348020
1755.782051	222320.947501	37.353037
1757.276255	222686.753074	37.358055
1758.517245	223052.703392	37.363072
1759.702554	223399.462169	37.368090
1761.417123	223770.466977	37.373108
1762.597515	224147.403387	37.378125
1763.977315	224518.770839	37.383143
1765.420275	224918.754464	37.388160
1766.880998	225302.810801	37.393178
1769.022418	225684.723557	37.398196
1770.336065	226087.094642	37.403213
1771.902800	226490.415687	37.408231
1773.471602	226907.326746	37.413248
1774.775528	227334.290741	37.418266
1776.878638	227747.280550	37.423284
1778.419441	228181.218545	37.428301
1780.319125	228596.860958	37.433319
1781.758887	229033.841112	37.438336
1783.545289	229468.123555	37.443354
1785.752524	229902.083612	37.448372
1787.566338	230340.250526	37.453389
1789.119395	230780.773468	37.458407
1790.846615	231230.565623	37.463424
1792.801541	231690.862830	37.468442
1794.859562	232137.097567	37.473460
1796.468429	232591.917422	37.478477
1798.177235	233038.593654	37.483495
1800.210851	233492.939320	37.488512
1802.437999	233956.855918	37.493530
1804.242737	234400.802087	37.498548
1806.010974	234851.588492	37.503565
1808.617580	235283.338400	37.508583
1810.956095	235728.977701	37.513600
1812.688695	236173.575453	37.518618
1814.871447	236601.588568	37.523636
1816.782478	237046.666927	37.528653
1818.479407	237480.198564	37.533671
1820.349911	237926.479597	37.538688
1821.944645	238371.410238	37.543706
1823.697663	238803.131980	37.548724
1825.517620	239250.338829	37.553741
1827.566414	239695.755972	37.558759
1829.339481	240135.834465	37.563776
1830.657372	240581.018916	37.568794
1832.528015	241037.848531	37.573812
1834.132318	241503.131371	37.578829
1835.840502	241957.347870	37.583847
1838.141110	242416.725369	37.588864
1839.528136	242881.488011	37.593882
1841.572000	243341.976645	37.598900
1843.087266	243806.668891	37.603917
1845.239683	244274.888938	37.608935
1847.066731	244739.099252	37.613952
1848.488123	245204.419037	37.618970
1850.344678	245680.412808	37.623988
1851.627559	246164.123204	37.629005
1854.508041	246627.831616	37.634023
1856.761978	247094.921456	37.639040
1858.568223	247562.975206	37.644058
1860.349545	248032.202226	37.649076
1862.128444	248513.166401	37.654093
1863.840474	248976.487160	37.659111
1865.858671	249436.861766	37.664128
1867.448278	249917.528701	37.669146
1869.399879	250379.236276	37.674164
1871.124760	250864.454322	37.679181
1872.849734	251342.915583	37.684199
1874.518357	251828.601095	37.689216
1876.387307	252309.859074	37.694234
1878.014198	252783.358753	37.699252
1879.533862	253257.689435	37.704269
1881.585675	253718.798794	37.709287
1883.260319	254182.206395	37.714304
1884.902417	254658.549886	37.719322
1886.727367	255127.674194	37.724340
1888.580060	255614.119134	37.729357
1890.545054	256083.119010	37.734375
1893.015535	256556.125215	37.739392
1894.577245	257030.730100	37.744410
1896.728400	257503.764036	37.749428
1898.342715	258001.324959	37.754445
1900.875566	258476.251836	37.759463
1902.823121	258958.591855	37.764480
1904.809033	259431.399278	37.769498
1907.174397	259905.744212	37.774516
1909.479487	260361.580076	37.779533
1913.007820	260793.384923	37.784551
1915.254531	261238.992770	37.789568
1917.256485	261689.772513	37.794586
1919.190630	262118.640333	37.799604
1921.078913	262562.249493	37.804621
1922.935156	263001.469022	37.809639
1924.462514	263450.599296	37.814656
1926.391128	263895.979400	37.819674
1927.666060	264347.437309	37.824692
1929.658829	264809.292940	37.829709
1931.465637	265272.423824	37.834727
1933.650672	265740.419922	37.839744
1935.069136	266197.263659	37.844762
1937.085444	266672.603052	37.849780
1938.624626	267146.166632	37.854797
1940.307798	267626.996582	37.859815
1943.069692	268087.528126	37.864832
1944.976650	268550.461693	37.869850
1947.807549	269013.724344	37.874868
1950.265095	269468.055671	37.879885
1952.173089	269930.936675	37.884903
1953.988832	270383.417198	37.889920
1955.837610	270854.918406	37.894938
1957.601909	271315.687567	37.899956
1958.959579	271778.708082	37.904973
1960.496467	272271.698864	37.909991
1962.052795	272748.402499	37.915008
1963.665198	273244.554506	37.920026
1965.456765	273740.650563	37.925044
1967.277311	274242.202473	37.930061
1969.185690	274743.027616	37.935079
1971.520726	275241.596493	37.940096
1972.897741	275757.215680	37.945114
1975.318628	276256.835175	37.950132
1976.678721	276786.324623	37.955149
1978.633519	277297.831147	37.960167
1980.500362	277823.017434	37.965184
1982.276463	278354.644208	37.970202
1985.800171	278857.682249	37.975220
1987.922425	279361.941886	37.980237
1989.818866	279864.027686	37.985255
1992.160866	280377.545423	37.990272
1994.032639	280891.596898	37.995290
1996.019690	281383.858580	38.000308
1998.249984	281893.427959	38.005325
2000.013125	282405.588012	38.010343
2001.750566	282915.413874	38.015360
2003.312264	283429.661762	38.020378
2005.054685	283950.279261	38.025396
2006.961793	284461.850369	38.030413
2008.635322	285009.553595	38.035431
2010.944954	285505.102710	38.040448
2012.414612	286025.987158	38.045466
2014.676897	286529.313479	38.050484
2016.186081	287042.084935	38.055501
2017.784837	287553.772910	38.060519
2020.229369	288063.388498	38.065536
2021.927278	288593.852751	38.070554
2023.786631	289123.373798	38.075572
2025.599494	289651.655851	38.080589
2027.473660	290192.676569	38.085607
2029.278748	290718.695001	38.090624
2031.317861	291273.323748	38.095642
2034.267011	291800.062602	38.100660
2037.449291	292324.195222	38.105677
2039.623361	292863.021220	38.110695
2041.661108	293377.763171	38.115712
2043.646068	293914.507574	38.120730
2045.626151	294429.330664	38.125748
2047.750725	294971.177709	38.130765
2049.484824	295508.235603	38.135783
2051.480482	296035.697562	38.140800
2053.532770	296582.577747	38.145818
2055.299235	297118.708046	38.150836
2057.343440	297673.914806	38.155853
2059.163783	298234.133816	38.160871
2060.960534	298793.566360	38.165888
2062.788477	299354.539968	38.170906
2064.468915	299931.840437	38.175924
2066.409750	300523.749014	38.180941
2068.534385	301098.632480	38.185959
2070.571143	301687.419568	38.190976
2072.522365	302262.781943	38.195994
2075.118069	302849.970777	38.201012
2078.055867	303421.454609	38.206029
2080.478682	303992.690011	38.211047
2084.199951	304519.109952	38.216064
2087.273356	305064.808576	38.221082
2089.644202	305599.420333	38.226100
2091.967045	306136.449421	38.231117
2093.517629	306666.035010	38.236135
2095.823233	307195.263702	38.241152
2097.791287	307731.605036	38.246170
2099.632680	308267.989300	38.251188
2101.822271	308800.503082	38.256205
2103.840874	309321.258259	38.261223
2106.273962	309848.341031	38.266240
2108.322215	310370.709800	38.271258
2110.475157	310901.920600	38.276276
2112.797560	311425.151193	38.281293
2114.811112	311954.651073	38.286311
2117.291961	312472.667847	38.291328
2119.087906	313005.269213	38.296346
2121.091359	313535.496201	38.301364
2122.763369	314061.355791	38.306381
2124.577834	314605.319106	38.311399
2126.527196	315140.825415	38.316416
2128.426104	315692.790956	38.321434
2130.355095	316238.525974	38.326452
2132.795190	316795.370412	38.331469
2134.752786	317346.119939	38.336487
2136.552217	317897.348378	38.341504
2138.949102	318451.850647	38.346522
2140.401225	319003.864116	38.351540
2142.197639	319583.086910	38.356557
2143.772327	320169.603434	38.361575
2146.114886	320737.223388	38.366592
2147.891653	321318.110173	38.371610
2149.917928	321917.358903	38.376628
2152.065136	322498.503879	38.381645
2153.760554	323072.812199	38.386663
2155.616460	323646.174702	38.391680
2157.761774	324220.855119	38.396698
2159.240987	324815.749258	38.401716
2161.563622	325402.957313	38.406733
2163.671271	325995.857158	38.411751
2165.668587	326589.632717	38.416768
2167.950144	327188.839329	38.421786
2169.799339	327796.591295	38.426804
2171.886637	328403.104342	38.431821
2173.957103	329019.159792	38.436839
2176.432364	329650.221985	38.441856
2178.512612	330272.736341	38.446874
2180.330795	330905.848369	38.451892
2182.317370	331536.209039	38.456909
2184.648552	332184.073080	38.461927
2186.711296	332825.525912	38.466944
2188.738638	333477.512331	38.471962
2190.916578	334128.806009	38.476980
2193.173987	334782.642623	38.481997
2195.440171	335443.247637	38.487015
2197.999055	336115.117582	38.492032
2199.945709	336786.572670	38.497050
2202.024330	337450.483602	38.502068
2204.372962	338113.782887	38.507085
2205.852262	338813.058975	38.512103
2208.449603	339492.316161	38.517120
2210.640989	340195.135854	38.522138
2212.500746	340883.989543	38.527156
2216.046187	341560.701150	38.532173
2218.551335	342243.108933	38.537191
2221.043550	342919.646249	38.542208
2223.611726	343585.806115	38.547226
2225.674506	344275.060663	38.552244
2227.984380	344943.985528	38.557261
2229.791135	345626.308695	38.562279
2232.435862	346307.290363	38.567296
2234.750524	346994.153939	38.572314
2237.280590	347676.378093	38.577332
2240.116178	348333.467664	38.582349
2242.516219	349001.557806	38.587367
2244.982840	349658.968438	38.592384
2247.591801	350319.543411	38.597402
2250.308914	350983.973350	38.602420
2252.661942	351622.214265	38.607437
2254.895717	352282.390656	38.612455
2257.556885	352926.854813	38.617472
2260.025965	353572.965214	38.622490
2262.219971	354203.683446	38.627508
2264.658142	354847.445259	38.632525
2266.991032	355496.644831	38.637543
2269.413763	356127.854836	38.642560
2271.969243	356759.439325	38.647578
2274.133607	357374.916320	38.652596
2276.859279	358000.338817	38.657613
2278.843427	358627.244677	38.662631
2280.822909	359245.768942	38.667648
2283.100129	359875.220370	38.672666
2284.756800	360514.329645	38.677684
2287.249454	361139.843816	38.682701
2289.346655	361792.483798	38.687719
2291.427129	362421.927673	38.692736
2294.283382	363055.774176	38.697754
2296.255670	363682.729510	38.702772
2298.713309	364313.425045	38.707789
2300.571196	364958.669499	38.712807
2302.786200	365586.517736	38.717824
2305.259954	366222.684058	38.722842
2307.521613	366836.627948	38.727860
2309.303974	367461.041507	38.732877
2311.283270	368077.320250	38.737895
2313.402190	368703.610534	38.742912
2315.573905	369336.501846	38.747930
2317.242083	369976.263446	38.752948
2319.877289	370608.548815	38.757965
2322.113334	371250.781256	38.762983
2324.222863	371893.987070	38.768000
2326.637810	372547.757966	38.773018
2328.386823	373211.315697	38.778036
2330.566092	373879.076029	38.783053
2332.544307	374547.541813	38.788071
2335.235799	375219.173763	38.793088
2337.495897	375891.320726	38.798106
2340.173911	376581.746284	38.803124
2342.730909	377250.115164	38.808141
2345.327327	377938.929385	38.813159
2347.373951	378620.923182	38.818176
2350.020258	379309.701431	38.823194
2351.851738	380008.439292	38.828212
2354.024107	380708.805110	38.833229
2356.092113	381417.642609	38.838247
2358.953208	382119.031143	38.843264
2361.084269	382836.702419	38.848282
2363.122929	383569.180564	38.853300
2365.304395	384281.005543	38.858317
2367.984983	385003.178031	38.863335
2370.791671	385711.876261	38.868352
2373.742608	386433.312682	38.873370
2376.124019	387155.080578	38.878388
2378.472879	387878.181056	38.883405
2380.747893	388611.392184	38.888423
2383.216880	389337.962965	38.893440
2385.172764	390064.424299	38.898458
2387.701183	390813.258495	38.903476
2390.171726	391533.389566	38.908493
2392.223059	392287.513952	38.913511
2394.436120	393026.359195	38.918528
2397.347767	393759.165008	38.923546
2399.957598	394496.387822	38.928564
2402.926273	395234.318804	38.933581
2405.367874	395974.498412	38.938599
2407.510934	396725.961754	38.943616
2409.448303	397476.122130	38.948634
2411.613527	398232.561304	38.953652
2414.048147	398985.185618	38.958669
2416.621354	399742.937125	38.963687
2419.003482	400500.269557	38.968704
2421.498649	401261.212267	38.973722
2424.211625	402014.547454	38.978740
2426.679569	402771.323942	38.983757
2428.770746	403524.468474	38.988775
2431.226079	404292.811016	38.993792
2433.301994	405056.026525	38.998810
2435.344285	405833.642849	39.003828
2437.954267	406604.581471	39.008845
2440.465072	407388.840895	39.013863
2442.804591	408169.306089	39.018880
2445.685491	408941.805990	39.023898
2448.737745	409705.566432	39.028916
2451.587026	410463.867137	39.033933
2454.242083	411233.653461	39.038951
2456.442298	411998.021486	39.043968
2459.323620	412748.019520	39.048986
2461.362121	413519.006684	39.054004
2464.485466	414252.432696	39.059021
2467.252512	414992.887439	39.064039
2469.128223	415718.272611	39.069056
2471.503488	416444.390515	39.074074
2473.260614	417177.098844	39.079092
2475.132647	417903.106857	39.084109
2477.910449	418641.099713	39.089127
2480.520845	419380.846113	39.094144
2483.377211	420092.017200	39.099162
2486.001609	420820.323984	39.104180
2489.402027	421527.895264	39.109197
2492.272317	422239.256261	39.114215
2494.744357	422954.182181	39.119232
2497.022107	423681.323185	39.124250
2499.488654	424400.259068	39.129268
2502.157207	425117.823916	39.134285
2504.240476	425854.350586	39.139303
2506.661232	426581.685410	39.144320
2509.373168	427297.912844	39.149338
2511.613075	428030.803173	39.154356
2514.428370	428772.688665	39.159373
2516.447354	429508.304100	39.164391
2518.333857	430267.914253	39.169408
2520.886677	431022.530017	39.174426
2522.857420	431796.959831	39.179444
2525.515870	432561.987027	39.184461
2527.841679	433334.991037	39.189479
2530.535245	434129.419913	39.194496
2533.185576	434916.843976	39.199514
2534.668895	435728.221728	39.204532
2536.671607	436525.769496	39.209549
2538.960865	437354.467138	39.214567
2540.779571	438195.661512	39.219584
2543.254725	439034.185696	39.224602
2545.679678	439886.754364	39.229620
2547.948261	440741.289825	39.234637
2550.818020	441594.984606	39.239655
2553.439624	442462.550998	39.244672
2555.772178	443331.952484	39.249690
2558.274457	444232.102241	39.254708
2560.792553	445107.068849	39.259725
2563.662034	445991.857382	39.264743
2566.184654	446875.655378	39.269760
2569.374535	447760.571251	39.274778
2571.633953	448646.869081	39.279796
2574.290109	449554.510298	39.284813
2576.745688	450447.377153	39.289831
2578.817428	451354.784967	39.294848
2581.454514	452257.913009	39.299866
2584.167626	453174.593113	39.304884
2586.664158	454086.818596	39.309901
2589.619537	454997.360388	39.314919
2592.281516	455916.809849	39.319936
2595.174085	456828.494470	39.324954
2597.682790	457757.139478	39.329972
2600.284333	458658.830000	39.334989
2602.952784	459584.179726	39.340007
2605.353197	460515.547073	39.345024
2608.294406	461431.060359	39.350042
2610.149732	462363.240611	39.355060
2613.043322	463296.317285	39.360077
2615.829145	464233.107935	39.365095
2617.987777	465170.766389	39.370112
2620.672688	466112.841317	39.375130
2623.279075	467061.301777	39.380148
2625.600452	467993.390048	39.385165
2628.258156	468943.366808	39.390183
2630.510977	469894.778389	39.395200
2633.996809	470830.679656	39.400218
2637.005768	471769.443133	39.405236
2639.799669	472660.250876	39.410253
2642.977598	473557.419446	39.415271
2645.694007	474450.630712	39.420288
2648.505007	475333.933392	39.425306
2651.011157	476214.516983	39.430324
2653.603249	477103.631154	39.435341
2656.758189	477961.699083	39.440359
2659.690927	478846.834260	39.445376
2663.279623	479700.355226	39.450394
2665.910731	480570.205171	39.455412
2668.755971	481419.274079	39.460429
2671.386114	482280.558570	39.465447
2673.668027	483145.545504	39.470464
2676.391484	484010.922624	39.475482
2678.907041	484886.490809	39.480500
2681.883329	485752.347527	39.485517
2684.673481	486619.051001	39.490535
2687.172354	487505.901827	39.495552
2689.707245	488370.138450	39.500570
2692.636564	489261.725787	39.505588
2695.232263	490142.269292	39.510605
2697.424040	491020.664852	39.515623
2699.845546	491923.959332	39.520640
2702.769784	492822.783390	39.525658
2705.218719	493720.932628	39.530676
2708.193406	494622.328573	39.535693
2710.656971	495543.792837	39.540711
2712.773665	496460.774102	39.545728
2715.108555	497395.882533	39.550746
2717.704322	498323.479990	39.555764
2720.256517	499277.517410	39.560781
2723.653297	500205.231260	39.565799
2726.563298	501146.189244	39.570816
2729.586648	502074.314477	39.575834
2732.873977	503013.288138	39.580852
2735.425249	503953.641200	39.585869
2738.312284	504897.414757	39.590887
2740.929193	505838.052047	39.595904
2743.693176	506768.021816	39.600922
2746.877585	507715.162624	39.605940
2749.703012	508655.198433	39.610957
2752.421298	509603.364023	39.615975
2754.804955	510555.410444	39.620992
2757.481360	511502.109173	39.626010
2760.362345	512454.665397	39.631028
2762.778870	513423.369667	39.636045
2765.284610	514387.967740	39.641063
2767.850484	515358.040099	39.646080
2770.131922	516331.828364	39.651098
2772.894667	517320.340938	39.656116
2775.089575	518328.383812	39.661133
2777.809181	519331.739684	39.666151
2780.224868	520340.622135	39.671168
2782.979561	521349.936231	39.676186
2786.164430	522356.795281	39.681204
2788.848174	523370.319293	39.686221
2791.959310	524373.480481	39.691239
2794.270635	525398.715699	39.696256
2796.706346	526427.637314	39.701274
2799.637614	527463.758122	39.706292
2802.467904	528503.650354	39.711309
2805.458861	529533.272744	39.716327
2807.670565	530591.447606	39.721344
2809.984094	531620.935685	39.726362
2812.813958	532676.089411	39.731380
2815.333056	533737.812101	39.736397
2818.394701	534803.343672	39.741415
2820.840037	535850.982503	39.746432
2823.661122	536898.432815	39.751450
2826.765374	537933.733608	39.756468
2829.584470	538958.641641	39.761485
2832.381864	539986.397738	39.766503
2835.522599	541012.261908	39.771520
2839.440896	541997.679060	39.776538
2843.506288	543001.614593	39.781556
2846.741776	544006.621613	39.786573
2849.520942	544999.209259	39.791591
2852.159616	546006.937326	39.796608
2854.921474	547012.158173	39.801626
2857.583799	548010.634817	39.806644
2860.355192	549013.093830	39.811661
2863.188248	550012.302149	39.816679
2866.204852	551029.203660	39.821696
2869.138200	552041.921140	39.826714
2872.259268	553043.021476	39.831732
2874.825889	554060.022093	39.836749
2877.884490	555073.497484	39.841767
2880.199923	556109.583294	39.846784
2882.537365	557147.394372	39.851802
2885.463807	558186.384022	39.856820
2887.744835	559230.423469	39.861837
2891.536214	560277.396347	39.866855
2894.387680	561315.399588	39.871872
2897.168501	562378.698705	39.876890
2900.596314	563426.887546	39.881908
2903.518568	564486.626884	39.886925
2906.513404	565533.412233	39.891943
2909.498973	566589.805841	39.896960
2912.560969	567654.334793	39.901978
2915.520626	568712.115358	39.906996
2918.195240	569785.819798	39.912013
2921.568278	570840.846094	39.917031
2924.016843	571919.779420	39.922048
2927.208597	572987.607229	39.927066
2929.601803	574062.251793	39.932084
2932.016961	575161.740445	39.937101
2934.951337	576251.714318	39.942119
2937.738228	577360.682571	39.947136
2940.434297	578467.460169	39.952154
2943.367009	579587.493223	39.957172
2946.102133	580712.774227	39.962189
2949.107122	581823.363542	39.967207
2951.874358	582965.033789	39.972224
2954.731593	584094.297451	39.977242
2957.429066	585241.833731	39.982260
2960.103249	586388.112342	39.987277
2963.253751	587540.419610	39.992295
2966.307594	588692.732941	39.997312
2969.222737	589855.884713	40.002330
2972.079005	591015.926248	40.007348
2975.122821	592180.033093	40.012365
2978.359696	593339.384229	40.017383
2981.563210	594496.222459	40.022400
2984.468640	595656.152433	40.027418
2987.858801	596830.413819	40.032436
2991.222366	597996.297700	40.037453
2994.903455	599114.836920	40.042471
2999.097907	600252.913228	40.047488
3002.194102	601383.398441	40.052506
3005.284779	602499.655262	40.057524
3008.545222	603632.395755	40.062541
3012.119546	604723.025530	40.067559
3015.220102	605840.406744	40.072576
3018.031345	606946.515712	40.077594
3020.904415	608055.058640	40.082612
3023.165929	609154.137067	40.087629
3026.291532	610226.848888	40.092647
3028.968972	611297.481183	40.097664
3032.166245	612365.624042	40.102682
3034.907754	613421.935864	40.107700
3037.288471	614497.661812	40.112717
3040.312307	615579.427919	40.117735
3043.003480	616669.293483	40.122752
3045.801209	617764.233266	40.127770
3048.692842	618847.899878	40.132788
3050.902964	619969.362432	40.137805
3053.838321	621097.437270	40.142823
3056.814553	622220.140587	40.147840
3059.658281	623365.586557	40.152858
3062.586200	624525.037532	40.157876
3065.328950	625689.190365	40.162893
3068.057103	626851.870340	40.167911
3070.827529	628034.796415	40.172928
3073.405648	629236.951336	40.177946
3076.529997	630437.731084	40.182964
3078.926222	631665.808170	40.187981
3082.141913	632876.381669	40.192999
3085.141840	634104.573289	40.198016
3088.445105	635346.097588	40.203034
3091.808910	636577.482019	40.208052
3095.898373	637804.658013	40.213069
3099.678441	639035.731375	40.218087
3103.333300	640266.329159	40.223104
3106.397770	641486.750313	40.228122
3110.492585	642697.727601	40.233140
3113.991481	643911.602201	40.238157
3117.104038	645117.815800	40.243175
3120.690335	646310.544156	40.248192
3123.472505	647517.074743	40.253210
3127.255414	648712.427893	40.258228
3130.597045	649909.157011	40.263245
3133.755020	651120.375844	40.268263
3136.589004	652324.972983	40.273280
3139.631128	653533.574990	40.278298
3142.283042	654752.107748	40.283316
3145.502946	655960.034801	40.288333
3148.719852	657182.855859	40.293351
3151.866415	658401.352608	40.298368
3154.991393	659616.962142	40.303386
3157.861712	660835.598660	40.308404
3161.069321	662074.287897	40.313421
3164.000987	663301.166614	40.318439
3166.959226	664544.059966	40.323456
3169.561287	665784.014834	40.328474
3172.947782	667044.676840	40.333492
3175.821471	668291.973659	40.338509
3179.191338	669545.292538	40.343527
3182.489732	670795.174780	40.348544
3185.370899	672072.561040	40.353562
3188.272482	673342.013648	40.358580
3191.321827	674624.097021	40.363597
3194.381273	675900.733603	40.368615
3197.467387	677190.014298	40.373632
3200.244801	678482.099081	40.378650
3203.774308	679772.537503	40.383668
3206.635712	681090.876968	40.388685
3209.597905	682382.136342	40.393703
3213.037901	683696.876114	40.398720
3216.055712	685003.649839	40.403738
3219.526264	686329.526009	40.408756
3222.606613	687653.684056	40.413773
3225.433444	688957.536361	40.418791
3228.703230	690289.665102	40.423808
3231.855908	691607.720512	40.428826
3235.301493	692890.404034	40.433844
3238.619814	694168.558260	40.438861
3241.895808	695457.051478	40.443879
3245.398559	696712.983023	40.448896
3248.577543	697996.212118	40.453914
3252.325045	699249.163034	40.458932
3256.154756	700506.036022	40.463949
3259.596139	701767.005703	40.468967
3263.516880	703017.851113	40.473984
3266.940084	704255.813818	40.479002
3270.377728	705507.123282	40.484020
3273.933921	706767.396471	40.489037
3276.515622	708030.370386	40.494055
3280.046065	709288.494817	40.499072
3282.802301	710546.512569	40.504090
3286.241213	711804.677420	40.509108
3289.481472	713079.816667	40.514125
3292.840649	714340.786703	40.519143
3296.528828	715610.322848	40.524160
3299.213471	716899.229571	40.529178
3302.954455	718169.953647	40.534196
3306.233319	719445.260219	40.539213
3309.081194	720747.644508	40.544231
3311.910885	722046.811347	40.549248
3315.067348	723357.141532	40.554266
3317.921169	724681.550798	40.559284
3321.544341	726008.437143	40.564301
3324.433949	727331.672104	40.569319
3328.177460	728652.180238	40.574336
3331.577956	729986.511891	40.579354
3335.119547	731323.021459	40.584372
3338.053851	732674.424066	40.589389
3341.329854	734020.803882	40.594407
3344.981269	735382.299515	40.599424
3347.424043	736751.661518	40.604442
3350.877542	738124.323442	40.609460
3353.966637	739511.266790	40.614477
3356.370953	740908.638816	40.619495
3359.627342	742314.748764	40.624512
3362.208735	743738.868390	40.629530
3365.660893	745161.994639	40.634548
3368.606154	746615.314414	40.639565
3371.277779	748078.267029	40.644583
3374.731585	749532.782887	40.649600
3377.974754	751019.185573	40.654618
3381.416916	752490.983899	40.659636
3385.012102	753972.326265	40.664653
3388.572693	755465.600748	40.669671
3392.566436	756928.332588	40.674688
3396.875586	758399.148992	40.679706
3400.965746	759859.578908	40.684724
3404.722927	761323.620256	40.689741
3408.649282	762775.395415	40.694759
3411.886330	764232.119698	40.699776
3415.049657	765693.687562	40.704794
3418.417186	767143.873558	40.709812
3421.798550	768609.013591	40.714829
3425.065166	770063.759279	40.719847
3428.906365	771510.556973	40.724864
3432.222387	772972.043378	40.729882
3436.120582	774417.376283	40.734900
3439.752053	775865.660255	40.739917
3442.630392	777313.241472	40.744935
3446.395907	778756.804870	40.749952
3449.518084	780213.144276	40.754970
3452.536754	781676.813325	40.759988
3455.692891	783139.524826	40.765005
3458.801528	784579.001996	40.770010
3461.991807	785982.073480	40.775015
3464.662442	787353.692416	40.780020
3467.979701	788657.560885	40.785024
3471.036328	789894.307509	40.790029
3473.871520	791079.534421	40.795034
3477.062198	792187.431814	40.800039
3479.411328	793232.918719	40.805044
3482.420748	794219.359316	40.810048
3485.141009	795132.253733	40.815053
3487.700106	795993.898607	40.820058
3489.872992	796760.365474	40.825063
3491.873735	797500.663542	40.830068
3493.656369	798159.495667	40.835072
3495.941323	798766.751183	40.840077
3497.726205	799315.591879	40.845082
3499.808716	799802.023364	40.850087
3501.358812	800259.118678	40.855092
3503.297669	800640.661918	40.860096
3504.474065	800987.134148	40.865101
3505.790253	801287.206379	40.870106
3506.995633	801541.514725	40.875111
3508.168100	801778.502962	40.880116
3509.073725	801961.470876	40.885120
3510.139055	802112.229510	40.890125
3510.556224	802236.702497	40.895130
3511.327767	802326.632290	40.900135
3512.257303	802403.585636	40.905140
3513.047333	802436.808997	40.910144
3514.100968	802441.883253	40.915149
3514.439455	802442.219760	40.920154
3515.133451	802386.727864	40.925159
3515.222750	802332.365499	40.930164
3516.004889	802268.274260	40.935168
3516.687888	802184.431096	40.940173
3517.125338	802074.629845	40.945178
3517.496155	801949.974774	40.950183
3517.969346	801811.467290	40.955188
3518.600609	801646.490159	40.960192
3518.897033	801475.677639	40.965197
3518.935094	801292.442915	40.970202
3519.751714	801092.934224	40.975207
3519.837309	800882.698163	40.980212
3520.277521	800672.151806	40.985216
3520.347710	800440.562763	40.990221
3520.484803	800207.433887	40.995226
3520.517170	799956.159600	41.000231
3520.705336	799708.285292	41.005236
3520.916075	799443.174526	41.010240
3520.930116	799184.760028	41.015245
3520.947168	798920.152013	41.020250
3521.171799	798641.169272	41.025255
3521.332919	798363.805419	41.030260
3521.027766	798084.004443	41.035264
3521.266948	797797.328883	41.040269
3520.993490	797515.831018	41.045274
3521.436688	797208.432899	41.050279
3521.094772	796920.393759	41.055284
3521.289295	796627.001371	41.060288
3521.408659	796324.821449	41.065293
3520.899627	796025.088847	41.070298
3520.993832	795719.597540	41.075303
3521.228099	795415.248129	41.080308
3520.944134	795115.095633	41.085312
3521.182219	794801.045913	41.090317
3520.928723	794495.509539	41.095322
3520.924702	794176.708598	41.100327
3520.879803	793879.066390	41.105332
3520.411194	793559.528421	41.110336
3520.696354	793254.733048	41.115341
3520.485470	792952.167558	41.120346
3520.283104	792635.392348	41.125351
3520.442425	792326.500709	41.130356
3520.624333	792009.486493	41.135360
3520.216683	791714.710917	41.140365
3519.985215	791391.793095	41.145370
3519.925288	791086.911841	41.150375
3519.785634	790793.871319	41.155380
3519.853394	790481.474849	41.160384
3520.042511	790178.331211	41.165389
3519.654765	789881.461290	41.170394
3519.623783	789571.547014	41.175399
3519.275452	789270.418931	41.180404
3519.105144	788962.171874	41.185408
3519.558327	788668.011701	41.190413
3519.162093	788366.066820	41.195418
3519.416462	788058.988254	41.200423
3519.142938	787765.549774	41.205428
3519.202526	787454.446796	41.210432
3519.079152	787152.405312	41.215437
3518.855608	786859.904387	41.220442
3519.004800	786548.747069	41.225447
3518.769908	786262.024490	41.230452
3518.727883	785961.344855	41.235456
3518.554018	785665.345220	41.240461
3518.395920	785380.688763	41.245466
3518.297999	785073.687405	41.250471
3518.290781	784793.998130	41.255476
3518.182771	784502.610953	41.260480
3518.060377	784200.395363	41.265485
3517.735200	783917.380383	41.270490
3517.790439	783630.160182	41.275495
3517.677731	783356.333994	41.280500
3517.455884	783065.841768	41.285504
3517.722628	782784.700937	41.290509
3517.247049	782503.179897	41.295514
3517.152382	782226.159630	41.300519
3517.071007	781946.617699	41.305524
3516.757889	781666.217723	41.310528
3516.899328	781394.537868	41.315533
3516.557563	781136.014314	41.320538
3516.294168	780863.791007	41.325543
3516.293676	780598.057826	41.330548
3516.401701	780335.249158	41.335552
3516.350234	780075.311204	41.340557
3515.759254	779812.402231	41.345562
3515.910919	779547.737107	41.350567
3516.144296	779299.534352	41.355572
3515.394469	779038.198270	41.360576
3515.885276	778780.634105	41.365581
3515.564802	778529.986633	41.370586
3515.658840	778277.933149	41.375591
3515.641934	778025.003314	41.380596
3515.096706	777774.662245	41.385600
3515.371903	777529.640690	41.390605
3515.063146	777286.036436	41.395610
3514.874136	777039.106120	41.400615
3514.559294	776799.178525	41.405620
3515.353897	776558.222819	41.410624
3515.335536	776304.888901	41.415629
3514.643105	776065.885739	41.420634
3514.528291	775823.972970	41.425639
3514.329127	775588.515994	41.430644
3514.486054	775341.323382	41.435648
3514.218463	775113.641905	41.440653
3513.893840	774888.867946	41.445658
3514.206035	774656.940281	41.450663
3513.985980	774424.108360	41.455668
3513.862338	774201.446813	41.460672
3514.162905	773965.608861	41.465677
3513.558878	773742.077068	41.470682
3513.461864	773521.803652	41.475687
3513.391718	773310.729109	41.480692
3513.011598	773082.953931	41.485696
3513.321058	772871.804062	41.490701
3513.116919	772662.161406	41.495706
3513.194555	772442.467119	41.500711
3513.036332	772229.799907	41.505716
3512.687217	772014.744382	41.510720
3513.072522	771807.738543	41.515725
3512.810759	771594.725292	41.520730
3512.899830	771379.233994	41.525735
3512.707811	771181.567576	41.530740
3512.624875	770968.999370	41.535744
3512.348868	770772.025602	41.540749
3512.295615	770572.546319	41.545754
3512.312393	770369.059175	41.550759
3512.164572	770165.100915	41.555764
3511.798172	769975.265282	41.560768
3511.828321	769774.026135	41.565773
3511.785785	769586.689300	41.570778
3511.954771	769385.810879	41.575783
3511.726978	769205.492363	41.580788
3511.216087	769012.452854	41.585792
3511.918420	768821.228362	41.590797
3511.701312	768630.594419	41.595802
3511.609668	768451.122158	41.600807
3511.736455	768254.162756	41.605812
3511.452799	768062.588831	41.610816
3511.338750	767870.094777	41.615821
3511.358407	767687.037012	41.620826
3511.304046	767510.443904	41.625831
3511.126790	767324.994592	41.630836
3511.383352	767145.384011	41.635840
3511.141571	766960.823554	41.640845
3510.946881	766780.588647	41.645850
3511.226552	766599.235796	41.650855
3510.904342	766414.872302	41.655860
3510.992109	766241.479241	41.660864
3511.106403	766066.056513	41.665869
3510.635808	765891.564418	41.670874
3510.654665	765713.634879	41.675879
3510.718869	765535.496405	41.680884
3510.595030	765369.907891	41.685888
3510.482184	765198.101500	41.690893
3510.326758	765031.771154	41.695898
3510.435008	764863.224038	41.700903
3510.304996	764690.028235	41.705908
3510.090615	764526.260429	41.710912
3510.192165	764366.233728	41.715917
3509.926443	764197.733448	41.720922
3509.769154	764022.159784	41.725927
3509.758919	763882.112760	41.730932
3509.820529	763721.930984	41.735936
3509.779578	763556.338033	41.740941
3509.333876	763406.441669	41.745946
3509.566930	763243.854181	41.750951
3509.466581	763091.280634	41.755956
3508.986427	762947.594953	41.760960
3509.748961	762790.384644	41.765965
3509.365865	762641.202491	41.770970
3509.590946	762475.689760	41.775975
3509.219699	762332.368920	41.780980
3509.092884	762187.278605	41.785984
3509.416543	762034.514937	41.790989
3509.053748	761894.045244	41.795994
3509.084552	761732.593071	41.800999
3508.995652	761598.879812	41.806004
3508.788375	761452.407465	41.811008
3508.844010	761306.826106	41.816013
3508.434388	761160.332198	41.821018
3508.574576	761022.328391	41.826023
3509.021044	760893.546057	41.831028
3508.454580	760759.304856	41.836032
3508.622742	760615.122265	41.841037
3508.214883	760488.792947	41.846042
3508.502239	760350.259207	41.851047
3508.358057	760216.481293	41.856052
3507.957299	760076.132086	41.861056
3508.384167	759956.168599	41.866061
3508.038077	759825.624185	41.871066
3508.253338	759690.642773	41.876071
3508.368220	759561.300496	41.881076
3507.936215	759441.224079	41.886080
3507.997852	759308.728378	41.891085
3508.057145	759185.655478	41.896090
3507.852614	759049.054323	41.901095
3507.797083	758931.325529	41.906100
3507.792193	758805.691098	41.911104
3508.001038	758676.515608	41.916109
3507.776716	758563.052874	41.921114
3507.614692	758434.131941	41.926119
3507.291730	758315.845615	41.931124
3507.419624	758195.163474	41.936128
3507.731292	758067.737274	41.941133
3507.251576	757947.546421	41.946138
3507.511414	757829.501695	41.951143
3507.097368	757716.797980	41.956148
3507.041608	757611.485894	41.961152
3506.960194	757495.466554	41.966157
3506.817709	757395.002599	41.971162
3507.230832	757288.029182	41.976167
3507.158413	757175.014218	41.981172
3507.103947	757057.305615	41.986176
3507.285313	756945.627337	41.991181
3506.985589	756836.494888	41.996186
3507.021604	756729.773400	42.001191
3506.824027	756624.717922	42.006196
3506.899539	756514.581012	42.011200
3506.736131	756402.112613	42.016205
3506.769142	756311.033546	42.021210
3506.651691	756205.909704	42.026215
3506.947736	756089.757259	42.031220
3506.727624	755993.730459	42.036224
3506.986995	755890.415874	42.041229
3506.318541	755788.092434	42.046234
3506.290540	755691.931366	42.051239
3506.506138	755589.706022	42.056244
3505.944195	755479.955749	42.061248
3506.255109	755385.956398	42.066253
3505.816890	755303.039655	42.071258
3506.088526	755212.451141	42.076263
3506.191678	755128.603766	42.081268
3505.851283	755026.956489	42.086272
3506.275409	754929.723722	42.091277
3506.217826	754838.592733	42.096282
3506.187974	754741.975697	42.101287
3506.099665	754651.736276	42.106292
3506.126505	754561.526139	42.111296
3506.103751	754461.003846	42.116301
3505.889673	754379.323810	42.121306
3505.903035	754273.658077	42.126311
3505.946997	754193.710956	42.131316
3505.383603	754104.432377	42.136320
3505.488480	754024.819070	42.141325
3505.506449	753951.638430	42.146330
3505.549681	753855.837588	42.151335
3505.503840	753770.074230	42.156340
3505.766971	753688.456127	42.161344
3505.730059	753609.059463	42.166349
3505.290501	753529.481610	42.171354
3505.496159	753450.141984	42.176359
3505.604428	753372.891661	42.181364
3505.207826	753292.810444	42.186368
3505.237138	753206.682710	42.191373
3505.161727	753130.497343	42.196378
3505.040823	753047.898859	42.201383
3505.154602	752974.693093	42.206388
3504.943552	752908.651693	42.211392
3505.148208	752828.219364	42.216397
3504.825240	752762.145816	42.221402
3505.000794	752682.753874	42.226407
3505.269866	752611.049960	42.231412
3505.007849	752537.753982	42.236416
3505.050181	752462.233967	42.241421
3505.148700	752394.210892	42.246426
3505.257369	752321.246705	42.251431
3505.029704	752249.720292	42.256436
3504.887198	752165.930592	42.261440
3504.898544	752091.696193	42.266445
3504.412326	752039.768906	42.271450
3504.313576	751966.983814	42.276455
3504.703781	751897.327660	42.281460
3504.567938	751845.192992	42.286464
3504.739327	751761.347030	42.291469
3504.753735	751705.630371	42.296474
3504.766769	751635.688438	42.301479
3504.754212	751573.208470	42.306484
3504.347367	751501.803519	42.311488
3504.682187	751432.893237	42.316493
3504.645594	751379.109018	42.321498
3504.821241	751299.900419	42.326503
3504.942194	751244.854362	42.331508
3504.600264	751172.941691	42.336512
3504.768060	751099.758615	42.341517
3504.548708	751049.558827	42.346522
3504.516221	750974.876373	42.351527
3504.575138	750916.627427	42.356532
3504.191453	750848.621029	42.361536
3504.703196	750776.810599	42.366541
3504.482901	750726.411277	42.371546
3504.191504	750657.844567	42.376551
3504.336950	750604.173077	42.381556
3504.451184	750542.997618	42.386560
3504.569000	750479.005277	42.391565
3503.834154	750420.883766	42.396570
3503.916032	750364.701695	42.401575
3504.268605	750311.290356	42.406580
3504.224110	750258.388876	42.411584
3504.100473	750199.176670	42.416589
3503.929429	750141.997338	42.421594
3503.968778	750080.781203	42.426599
3504.090545	750032.000528	42.431604
3503.912449	749970.177212	42.436608
3503.993729	749920.118036	42.441613
3503.752392	749863.442302	42.446618
3503.627611	749813.465892	42.451623
3503.319115	749770.485576	42.456628
3503.602159	749720.984630	42.461632
3504.013032	749676.106342	42.466637
3503.947189	749630.763108	42.471642
3503.979458	749584.514091	42.476647
3504.117765	749531.873884	42.481652
3503.507208	749477.874870	42.486656
3503.866254	749419.219233	42.491661
3503.696012	749378.437209	42.496666
3503.643107	749330.125651	42.501671
3504.113714	749288.347923	42.506676
3503.811631	749234.345648	42.511680
3503.948060	749180.962253	42.516685
3503.734421	749129.612687	42.521690
3503.555653	749074.353703	42.526695
3503.782726	749033.010120	42.531700
3504.003157	748986.726452	42.536704
3503.860498	748927.310045	42.541709
3503.721512	748872.438332	42.546714
3503.781778	748825.191962	42.551719
3503.723455	748787.698856	42.556724
3503.256232	748739.946201	42.561728
3503.811916	748687.330129	42.566733
3503.879776	748644.231974	42.571738
3503.715669	748595.785992	42.576743
3503.657366	748553.696426	42.581748
3503.634265	748499.692355	42.586752
3503.665214	748451.855611	42.591757
3503.410813	748409.105883	42.596762
3503.271596	748357.195370	42.601767
3503.520956	748310.458179	42.606772
3503.383507	748263.043412	42.611776
3503.494054	748220.825315	42.616781
3503.266128	748188.842356	42.621786
3503.508958	748144.823059	42.626791
3503.113298	748090.729470	42.631796
3502.987053	748058.630342	42.636800
3503.146470	748018.033783	42.641805
3503.112608	747991.750175	42.646810
3503.086130	747947.428353	42.651815
3503.247981	747903.470491	42.656820
3503.319583	747879.491653	42.661824
3503.615394	747829.235318	42.666829
3503.274098	747795.836384	42.671834
3503.279660	747742.761256	42.676839
3503.473394	747699.093479	42.681844
3502.910761	747671.314796	42.686848
3502.953339	747625.101846	42.691853
3502.932688	747608.154810	42.696858
3503.172114	747559.833374	42.701863
3503.157531	747517.385052	42.706868
3502.841667	747489.812038	42.711872
3502.907379	747440.184249	42.716877
3502.819215	747412.029720	42.721882
3503.107889	747379.760394	42.726887
3503.113850	747339.778702	42.731892
3503.022900	747306.385721	42.736896
3503.333084	747265.661494	42.741901
3502.499294	747239.408691	42.746906
3502.884512	747213.497996	42.751911
3502.946741	747169.799567	42.756916
3502.525860	747139.573924	42.761920
3502.743726	747104.349880	42.766925
3502.778254	747079.139169	42.771930
3503.146858	747046.113931	42.776935
3502.858232	747021.302387	42.781940
3503.017006	746987.224288	42.786945
3503.272333	746943.838644	42.791949
3502.956523	746921.403557	42.796954
3502.940755	746872.922350	42.801959
3502.832383	746832.660416	42.806964
3502.936984	746806.300510	42.811969
3503.026932	746773.764981	42.816973
3503.028771	746745.247208	42.821978
3502.830267	746705.543174	42.826983
3502.679151	746674.925184	42.831988
3502.582763	746640.640616	42.836993
3503.176769	746612.469328	42.841997
3502.865364	746578.467141	42.847002
3502.719390	746542.015639	42.852007
3502.689133	746505.050591	42.857012
3502.650821	746467.246465	42.862017
3503.009195	746437.976697	42.867021
3502.582457	746419.561985	42.872026
3502.699226	746389.442294	42.877031
3502.794738	746376.526329	42.882036
3502.603444	746340.575637	42.887041
3502.912122	746306.370948	42.892045
3502.630459	746285.361762	42.897050
3502.733380	746240.020329	42.902055
3502.644996	746219.374442	42.907060
3502.440850	746188.219608	42.912065
3502.544774	746161.907070	42.917069
3502.727732	746131.627167	42.922074
3502.800180	746099.190580	42.927079
3502.639207	746073.069800	42.932084
3502.597671	746050.586887	42.937089
3502.512545	746012.936585	42.942093
3502.610128	745985.141647	42.947098
3502.905718	745965.222499	42.952103
3502.789630	745934.694678	42.957108
3502.551228	745907.498702	42.962113
3502.789686	745866.185896	42.967117
3502.632401	745836.109363	42.972122
3502.235506	745814.228217	42.977127
3502.533091	745798.460413	42.982132
3502.357003	745775.998945	42.987137
3502.695428	745753.798403	42.992141
3502.647169	745718.018935	42.997146
3502.423786	745688.941364	43.002151
3502.761036	745666.889063	43.007156
3502.534874	745636.477129	43.012161
3502.466122	745611.525909	43.017165
3502.686605	745587.663732	43.022170
3502.569957	745560.594725	43.027175
3502.562922	745522.039395	43.032180
3502.649615	745508.134824	43.037185
3502.390264	745465.715808	43.042189
3502.637073	745461.325053	43.047194
3502.619874	745423.166372	43.052199
3502.665548	745400.963776	43.057204
3502.421725	745381.330011	43.062209
3502.749297	745350.133409	43.067213
3502.482304	745320.270753	43.072218
3502.130594	745297.441470	43.077223
3502.418134	745270.799001	43.082228
3502.277569	745253.224044	43.087233
3502.626636	745220.441510	43.092237
3502.619407	745208.924736	43.097242
3502.331787	745181.289468	43.102247
3502.508021	745154.022357	43.107252
3502.213114	745126.338665	43.112257
3502.614186	745105.757265	43.117261
3502.619876	745082.818863	43.122266
3502.368222	745051.568486	43.127271
3502.850021	745018.911482	43.132276
3502.318315	745002.339856	43.137281
3502.616721	744965.758147	43.142285
3502.270696	744956.818175	43.147290
3502.244224	744915.099224	43.152295
3502.336181	744905.938513	43.157300
3502.352388	744881.415850	43.162305
3502.158209	744851.143888	43.167309
3502.553346	744846.728282	43.172314
3502.628243	744815.472439	43.177319
3502.373250	744784.715910	43.182324
3502.207286	744777.575119	43.187329
3502.420568	744750.597104	43.192333
3502.777658	744728.489455	43.197338
3502.361566	744709.277964	43.202343
3502.406422	744674.615392	43.207348
3502.098192	744660.922891	43.212353
3502.242826	744631.632272	43.217357
3502.270952	744613.187573	43.222362
3502.141936	744591.159865	43.227367
3502.088601	744569.267902	43.232372
3501.947687	744568.203599	43.237377
3502.687491	744533.722195	43.242381
3502.218478	744520.006578	43.247386
3502.215755	744495.139771	43.252391
3502.445059	744470.630050	43.257396
3502.214225	744461.324409	43.262401
3502.029014	744420.074002	43.267405
3502.155725	744423.810429	43.272410
3501.795850	744402.265285	43.277415
3502.294996	744367.130778	43.282420
3502.010831	744357.092243	43.287425
3501.875038	744332.939056	43.292429
3501.729873	744325.596660	43.297434
3501.935923	744312.510714	43.302439
3502.390220	744297.060080	43.307444
3501.972642	744279.775913	43.312449
3501.947546	744264.997705	43.317453
3501.379171	744260.938747	43.322458
3502.042688	744242.239863	43.327463
3502.318812	744218.216016	43.332468
3502.069598	744198.926257	43.337473
3501.836055	744176.766339	43.342477
3501.704225	744164.873102	43.347482
3501.541250	744160.054939	43.352487
3502.090584	744137.913866	43.357492
3501.874760	744134.241546	43.362497
3501.838801	744104.286641	43.367501
3501.915211	744098.786156	43.372506
3501.916976	744095.819471	43.377511
3501.957510	744059.226717	43.382516
3501.653218	744056.854440	43.387521
3502.004545	744039.887653	43.392525
3501.706226	744047.056475	43.397530
3501.973754	744016.161149	43.402535
3502.091985	743999.479998	43.407540
3502.231210	743995.996149	43.412545
3501.971966	743968.747448	43.417549
3501.870464	743960.804198	43.422554
3501.836939	743950.970932	43.427559
3501.896493	743940.677299	43.432564
3501.593959	743913.138908	43.437569
3501.853947	743900.191691	43.442573
3501.676736	743897.699482	43.447578
3501.653258	743884.057452	43.452583
3501.716538	743872.032647	43.457588
3501.775184	743850.070734	43.462593
3501.861737	743847.139387	43.467597
3501.528625	743844.079617	43.472602
3501.446106	743836.726411	43.477607
3501.910156	743817.911158	43.482612
3501.624418	743812.865856	43.487617
3502.100165	743792.960880	43.492621
3501.945015	743795.854219	43.497626
3501.815768	743771.895996	43.502631
3502.045743	743751.586545	43.507636
3501.834973	743734.711985	43.512641
3501.908193	743729.805084	43.517645
3501.719461	743710.850232	43.522650
3501.874301	743695.447904	43.527655
3501.858409	743688.577980	43.532660
3501.771652	743694.822185	43.537665
3502.024663	743654.286434	43.542669
3502.324861	743648.254222	43.547674
3502.049408	743633.170094	43.552679
3502.134088	743597.853430	43.557684
3501.935913	743605.599427	43.562689
3501.871961	743579.899302	43.567693
3501.733690	743559.501876	43.572698
3501.736912	743554.655877	43.577703
3502.059725	743551.537047	43.582708
3501.626633	743544.389829	43.587713
3501.691532	743513.278794	43.592717
3501.841718	743507.864595	43.597722
3501.776824	743506.095365	43.602727
3501.534700	743496.938776	43.607732
3501.692094	743492.017818	43.612737
3501.832333	743463.514687	43.617741
3501.734190	743460.267605	43.622746
3501.326561	743452.374427	43.627751
3502.052794	743451.166679	43.632756
3501.832698	743428.854095	43.637761
3501.914402	743399.025396	43.642765
3502.133201	743400.868187	43.647770
3502.063648	743386.590125	43.652775
3502.126893	743364.181092	43.657780
3501.878921	743361.601514	43.662785
3501.953118	743341.514529	43.667789
3502.095263	743314.691686	43.672794
3501.914394	743308.936492	43.677799
3501.970507	743292.115772	43.682804
3501.808179	743282.401845	43.687809
3502.143035	743264.298863	43.692813
3501.885681	743264.193092	43.697818
3501.954173	743236.442683	43.702823
3501.501914	743218.222432	43.707828
3501.497860	743216.245298	43.712833
3501.380541	743204.545995	43.717837
3501.628092	743198.373802	43.722842
3501.455823	743205.028095	43.727847
3501.811025	743201.755438	43.732852
3501.781742	743173.427610	43.737857
3501.772729	743158.743560	43.742861
3502.068769	743156.074019	43.747866
3501.425159	743153.164177	43.752871
3501.689201	743117.766276	43.757876
3501.542711	743113.735891	43.762881
3501.823214	743105.580313	43.767885
3501.969019	743107.781363	43.772890
3501.990773	743089.531932	43.777895
3501.857195	743066.264533	43.782900
3501.786359	743063.062220	43.787905
3501.671762	743063.872349	43.792909
3501.944676	743043.405639	43.797914
3501.470915	743026.127991	43.802919
3501.873738	743012.018428	43.807924
3501.196988	743012.031403	43.812929
3501.901777	743011.024927	43.817933
3501.823024	743002.533028	43.822938
3501.815462	742980.431289	43.827943
3502.055790	742962.046550	43.832948
3501.846883	742973.009039	43.837953
3502.051121	742942.119963	43.842957
3501.774688	742921.348131	43.847962
3501.820274	742915.258540	43.852967
3501.851141	742899.182873	43.857972
3501.710547	742884.915640	43.862977
3501.947319	742867.025749	43.867981
3502.087788	742870.463955	43.872986
3501.829429	742855.573302	43.877991
3502.117586	742827.340120	43.882996
3501.861849	742816.305943	43.888001
3501.780103	742804.847410	43.893005
3501.868328	742798.404542	43.898010
3501.958478	742773.714745	43.903015
3502.093157	742755.594228	43.908020
3501.556545	742759.836652	43.913025
3501.463496	742728.649723	43.918029
3501.638176	742711.560927	43.923034
3501.891983	742720.370436	43.928039
3502.007835	742716.098700	43.933044
3501.726470	742710.953064	43.938049
3501.598019	742676.656477	43.943053
3501.747289	742675.890108	43.948058
3501.654263	742667.499105	43.953063
3501.841062	742670.534147	43.958068
3501.578192	742663.456892	43.963073
3501.461394	742625.202191	43.968077
3501.997274	742622.789539	43.973082
3501.525721	742616.191774	43.978087
3501.624003	742615.384375	43.983092
3500.947418	742613.518223	43.988097
3501.777731	742616.051349	43.993101
3501.758579	742592.269143	43.998106
3501.696695	742572.894988	44.003111
3501.743127	742570.414849	44.008116
3501.281955	742575.485556	44.013121
3501.452612	742568.732179	44.018125
3501.586620	742561.737601	44.023130
3501.604303	742559.113858	44.028135
3501.744893	742537.579800	44.033140
3501.528610	742529.060666	44.038145
3501.441210	742515.080676	44.043149
3501.524141	742516.006571	44.048154
3501.521667	742511.309223	44.053159
3501.731909	742506.873425	44.058164
3501.604067	742482.416541	44.063169
3501.846977	742482.623694	44.068173
3501.535236	742468.383988	44.073178
3501.327069	742473.660206	44.078183
3501.392817	742471.918604	44.083188
3501.375746	742476.619284	44.088193
3501.730569	742461.527659	44.093197
3501.843792	742440.690170	44.098202
3501.668752	742431.323449	44.103207
3501.650328	742412.634033	44.108212
3501.706048	742414.998518	44.113217
3501.596221	742412.494699	44.118221
3501.689482	742378.852496	44.123226
3501.767132	742386.801364	44.128231
3501.765384	742378.394970	44.133236
3501.929939	742391.324056	44.138241
3501.951486	742358.385934	44.143245
3501.613030	742347.117509	44.148250
3501.533385	742335.410689	44.153255
3501.812159	742326.611724	44.158260
3501.589593	742334.461899	44.163265
3501.702592	742305.810734	44.168269
3501.705960	742295.524239	44.173274
3501.853060	742289.565746	44.178279
3501.936770	742285.397993	44.183284
3502.157897	742272.949052	44.188289
3501.752519	742240.773314	44.193293
3502.040484	742233.703554	44.198298
3501.856600	742219.145556	44.203303
3501.934100	742199.599095	44.208308
3501.453452	742197.651009	44.213313
3501.606932	742190.504528	44.218317
3501.544883	742189.970843	44.223322
3501.467543	742188.796802	44.228327
3501.809810	742169.898852	44.233332
3501.244923	742154.365187	44.238337
3501.484977	742135.088422	44.243341
3501.669381	742140.448349	44.248346
3501.482806	742133.555820	44.253351
3501.650457	742136.248063	44.258356
3501.527682	742132.163803	44.263361
3501.314682	742108.560531	44.268365
3501.462579	742101.068721	44.273370
3501.533185	742103.381387	44.278375
3501.872156	742101.545103	44.283380
3501.551618	742095.416474	44.288385
3501.729827	742093.854019	44.293389
3501.802674	742065.703150	44.298394
3502.018785	742051.721638	44.303399
3501.808392	742032.321243	44.308404
3501.662134	742050.445410	44.313409
3501.554754	742032.165420	44.318413
3501.865156	742007.733555	44.323418
3501.452368	742003.746605	44.328423
3501.768269	741991.528829	44.333428
3501.456436	741995.042159	44.338433
3501.392500	741998.019987	44.343437
3501.692669	741994.310849	44.348442
3501.730792	741975.067062	44.353447
3502.100973	741958.883958	44.358452
3501.945990	741955.002744	44.363457
3501.921840	741934.878978	44.368461
3502.028819	741917.305111	44.373466
3501.542663	741907.395728	44.378471
3501.761182	741890.743002	44.383476
3501.573014	741888.548688	44.388481
3501.417152	741869.039972	44.393485
3501.307657	741868.316287	44.398490
3501.346730	741856.440775	44.403495
3501.600889	741848.733349	44.408500
3501.542378	741857.842707	44.413505
3501.397511	741858.855776	44.418509
3501.516556	741859.528508	44.423514
3501.274867	741859.172849	44.428519
3501.494331	741844.349689	44.433524
3501.341712	741826.126152	44.438529
3501.214787	741810.717256	44.443533
3501.667763	741808.021334	44.448538
3501.558156	741809.424222	44.453543
3501.841576	741811.850172	44.458548
3501.452497	741815.969804	44.463553
3501.499094	741809.978104	44.468557
3501.670059	741802.432746	44.473562
3501.440156	741767.258782	44.478567
3501.876963	741760.361827	44.483572
3501.257303	741762.590835	44.488577
3501.667378	741763.907857	44.493581
3501.766128	741763.693757	44.498586
3501.671224	741756.192289	44.503591
3501.630757	741726.872012	44.508596
3501.527532	741723.822873	44.513601
3501.605314	741716.243375	44.518605
3501.482716	741722.000506	44.523610
3501.670207	741723.008127	44.528615
3501.634158	741703.627570	44.533620
3501.598686	741678.806744	44.538625
3501.728815	741666.272976	44.543629
3501.663459	741664.552862	44.548634
3501.548715	741672.435330	44.553639
3501.638572	741663.518481	44.558644
3501.345289	741650.016082	44.563649
3501.430701	741645.550976	44.568653
3501.611032	741639.141401	44.573658
3501.349255	741643.784100	44.578663
3501.576945	741630.195579	44.583668
3501.360097	741643.732932	44.588673
3501.666259	741641.704142	44.593677
3501.668853	741640.417898	44.598682
3501.824124	741616.208283	44.603687
3501.728912	741597.430715	44.608692
3501.319517	741593.195713	44.613697
3501.454796	741587.535384	44.618701
3501.897092	741588.303093	44.623706
3501.422612	741581.902763	44.628711
3501.625353	741562.086750	44.633716
3501.354912	741542.348878	44.638721
3501.543644	741539.844902	44.643725
3501.592467	741532.764579	44.648730
3501.021251	741547.695982	44.653735
3501.429532	741534.769847	44.658740
3501.430764	741541.743061	44.663745
3501.452105	741531.947168	44.668749
3501.629407	741542.847816	44.673754
3501.221355	741528.424499	44.678759
3501.428236	741500.051641	44.683764
3501.524299	741488.908013	44.688769
3501.695710	741486.555253	44.693773
3501.643469	741481.272033	44.698778
3501.301239	741492.357515	44.703783
3501.481713	741487.035845	44.708788
3501.290638	741492.507717	44.713793
3501.559358	741485.242644	44.718797
3501.518215	741464.774291	44.723802
3501.427926	741451.584208	44.728807
3501.599205	741440.625911	44.733812
3501.337748	741444.131158	44.738817
3501.144230	741441.888144	44.743821
3501.757073	741438.967854	44.748826
3501.573572	741443.399906	44.753831
3501.478857	741434.958414	44.758836
3501.491520	741438.962396	44.763841
3501.453843	741405.090401	44.768845
3501.448099	741392.628110	44.773850
3501.211576	741393.903671	44.778855
3501.922629	741395.467766	44.783860
3501.167171	741391.784415	44.788865
3501.627004	741387.504580	44.793869
3501.703972	741388.332678	44.798874
3501.250915	741383.066169	44.803879
3501.605412	741354.767313	44.808884
3501.511676	741358.541629	44.813889
3501.296263	741349.031920	44.818893
3501.452750	741344.505442	44.823898
3501.711939	741348.419275	44.828903
3501.922643	741333.497692	44.833908
3501.438771	741335.457088	44.838913
3501.825163	741317.538972	44.843917
3501.742949	741307.116958	44.848922
3501.548396	741302.203342	44.853927
3501.601161	741302.194662	44.858932
3501.283813	741312.435496	44.863937
3501.247621	741293.597996	44.868941
3501.876996	741287.806348	44.873946
3501.652104	741277.655164	44.878951
3501.747960	741263.889967	44.883956
3501.617570	741263.515887	44.888961
3501.268730	741253.632445	44.893965
3501.483349	741260.174979	44.898970
3501.202271	741248.400917	44.903975
3501.735110	741219.280773	44.908980
3501.466218	741208.938937	44.913985
3501.341680	741207.525254	44.918989
3501.453501	741211.315131	44.923994
3501.717162	741210.084595	44.928999
3501.855372	741202.593538	44.934004
3501.486255	741195.384142	44.939009
3501.397039	741178.286184	44.944013
3501.821822	741160.905418	44.949018
3501.505093	741170.206613	44.954023
3501.690910	741165.922481	44.959028
3501.354239	741174.781836	44.964033
3501.292111	741164.257397	44.969037
3501.723322	741143.660701	44.974042
3501.539531	741129.941482	44.979047
3501.593095	741114.699240	44.984052
3501.394617	741116.710446	44.989057
3501.441684	741112.943806	44.994061
3501.560731	741108.720137	44.999066
3501.268978	741113.120801	45.004071
3501.472924	741108.437969	45.009076
3501.507368	741114.664183	45.014081
3501.496097	741106.010714	45.019085
3501.188803	741069.708872	45.024090
3501.261669	741078.055524	45.029095
3501.436269	741066.304810	45.034100
3501.465331	741062.095985	45.039105
3501.467765	741066.596441	45.044109
3501.440453	741067.243968	45.049114
3500.956365	741074.099953	45.054119
3501.400257	741074.076101	45.059124
3501.635496	741081.011053	45.064129
3501.579359	741066.627657	45.069133
3501.763438	741055.518335	45.074138
3501.402817	741046.526852	45.079143
3501.340498	741028.138174	45.084148
3501.242075	741026.621225	45.089153
3501.444782	741020.553671	45.094157
3501.378759	741021.801116	45.099162
3501.278573	741022.955286	45.104167
3501.498618	741018.665420	45.109172
3501.485825	741025.690866	45.114177
3501.237765	741022.269710	45.119181
3501.330379	741028.090701	45.124186
3501.078598	741007.804352	45.129191
3501.394955	740996.524710	45.134196
3501.343416	740984.959623	45.139201
3501.508753	740972.567321	45.144205
3501.971140	740973.875836	45.149210
3501.457547	740976.186449	45.154215
3501.646123	740972.940420	45.159220
3501.718656	740970.702768	45.164225
3501.785649	740950.116295	45.169229
3501.608058	740933.527015	45.174234
3501.323028	740931.002214	45.179239
3501.409116	740920.947564	45.184244
3501.388498	740942.763037	45.189249
3501.575186	740932.592857	45.194253
3501.746755	740938.153565	45.199258
3501.267626	740909.446810	45.204263
3501.404419	740902.796533	45.209268
3501.159847	740903.875659	45.214273
3501.377004	740897.113176	45.219277
3501.605301	740894.998145	45.224282
3501.250460	740896.491178	45.229287
3501.390885	740892.164939	45.234292
3501.577203	740890.056844	45.239297
3501.507892	740892.046762	45.244301
3501.412527	740891.765796	45.249306
3501.163578	740892.301579	45.254311
3501.714655	740877.619658	45.259316
3501.492568	740859.306450	45.264321
3501.502124	740844.862335	45.269325
3501.258097	740838.917925	45.274330
3501.467553	740847.736859	45.279335
3501.744777	740844.871817	45.284340
3501.355674	740848.052191	45.289345
3501.329007	740839.895584	45.294349
3501.339602	740844.098052	45.299354
3501.267030	740844.505771	45.304359
3501.502945	740821.714770	45.309364
3501.595941	740811.955607	45.314369
3501.627397	740808.686013	45.319373
3501.726302	740800.409693	45.324378
3501.500899	740807.668311	45.329383
3501.526812	740799.750280	45.334388
3501.247688	740805.237174	45.339393
3501.242229	740786.146082	45.344397
3501.525412	740756.966575	45.349402
3501.516290	740754.841279	45.354407
3501.628583	740755.960376	45.359412
3501.673766	740749.176724	45.364417
3501.604199	740752.205411	45.369421
3501.349591	740747.944372	45.374426
3501.525885	740750.586201	45.379431
3501.581459	740734.254743	45.384436
3501.625978	740725.542178	45.389441
3501.196182	740716.017670	45.394445
3501.684037	740705.154431	45.399450
3501.430173	740719.985482	45.404455
3501.615425	740699.922896	45.409460
3501.711485	740704.111315	45.414465
3501.411836	740701.885627	45.419469
3501.500945	740669.968009	45.424474
3501.323196	740676.773713	45.429479
3501.713753	740664.937258	45.434484
3501.235862	740661.751771	45.439489
3501.152771	740667.008517	45.444493
3501.525137	740659.577179	45.449498
3501.330821	740662.131894	45.454503
3501.488549	740664.529510	45.459508
3501.471328	740667.500117	45.464513
3501.441543	740660.481467	45.469517
3501.715289	740647.229888	45.474522
3501.697543	740635.015699	45.479527
3501.760747	740623.431124	45.484532
3501.678594	740621.070548	45.489537
3501.893221	740612.923297	45.494541
3501.751854	740588.413325	45.499546
3501.780167	740582.077481	45.504551
3501.720342	740573.283066	45.509556
3501.493647	740578.909839	45.514561
3501.493364	740578.069061	45.519565
3501.702633	740563.690357	45.524570
3501.558251	740551.249652	45.529575
3501.675141	740534.314097	45.534580
3501.604749	740532.396716	45.539585
3501.470200	740538.651308	45.544589
3501.672435	740536.886730	45.549594
3501.411119	740513.435066	45.554599
3501.479722	740496.606336	45.559604
3501.586456	740498.319946	45.564609
3501.599774	740496.438187	45.569613
3501.574009	740487.242344	45.574618
3501.497594	740489.233536	45.579623
3501.811222	740471.325537	45.584628
3501.796177	740457.626730	45.589633
3501.420405	740445.174631	45.594637
3501.092136	740437.067448	45.599642
3501.417052	740444.779556	45.604647
3501.726873	740444.382155	45.609652
3501.642491	740437.570183	45.614657
3501.392201	740432.962015	45.619661
3501.488893	740418.255407	45.624666
3501.417818	740403.675421	45.629671
3501.353731	740397.750408	45.634676
3501.495723	740403.118526	45.639681
3501.228719	740410.137062	45.644685
3501.814594	740392.629071	45.649690
3501.648029	740396.514805	45.654695
3501.553595	740400.042372	45.659700
3501.508794	740379.571819	45.664705
3501.790840	740364.834483	45.669709
3501.804277	740342.227261	45.674714
3501.439002	740348.767449	45.679719
3501.426864	740349.907166	45.684724
3501.619197	740346.511870	45.689729
3501.565928	740327.130789	45.694733
3501.710792	740308.904063	45.699738
3501.297981	740314.413384	45.704743
3501.355892	740306.934752	45.709748
3501.249087	740305.072798	45.714753
3501.139973	740300.836938	45.719757
3501.389003	740295.354750	45.724762
3501.156850	740310.232442	45.729767
3501.511625	740297.164747	45.734772
3501.361808	740306.983475	45.739777
3501.418624	740299.208231	45.744781
3501.557270	740302.796254	45.749786
3501.371202	740281.112183	45.754791
3501.396680	740270.918332	45.759796
3501.563055	740257.931169	45.764801
3501.242793	740255.956082	45.769805
3501.334444	740247.581456	45.774810
3501.379340	740241.885641	45.779815
3501.136614	740184.398158	45.784820
3501.570664	740072.089506	45.789825
3500.826127	739902.493816	45.794829
3501.040323	739669.961120	45.799834
3500.940931	739400.519497	45.804839
3500.958900	739051.102849	45.809844
3500.886813	738654.190306	45.814849
3500.588676	738194.063452	45.819853
3500.342374	737674.970259	45.824858
3499.891335	737116.141513	45.829863
3499.528435	736486.392640	45.834868
3499.278507	735814.952777	45.839873
3499.009685	735069.413038	45.844877
3498.760895	734277.219910	45.849882
3497.995754	733422.705231	45.854887
3497.849630	732512.147852	45.859892
3497.668848	731530.831099	45.864897
3496.881889	730504.923527	45.869901
3496.542876	729411.152737	45.874906
3495.775144	728254.392336	45.879911
3495.492609	727041.153624	45.884916
3494.804785	725765.959663	45.889921
3493.814292	724436.397678	45.894925
3493.491397	723050.199748	45.899930
3492.737813	721605.982779	45.904935
3492.194448	720084.916941	45.909940
3491.510921	718522.530426	45.914945
3490.655532	716880.113439	45.919949
3489.862322	715168.298770	45.924954
3489.011025	713434.955444	45.929959
3488.035277	711607.810928	45.934964
3487.469220	709735.175149	45.939969
3486.248079	707793.061587	45.944973
3485.576071	705791.458399	45.949978
3484.354229	703749.735489	45.954983
3483.384117	701623.704812	45.959988
3482.328840	699454.918600	45.964993
3480.904316	697231.014794	45.969997
3480.288900	694955.390599	45.975002
3478.925007	692618.865181	45.980007
3478.140092	690216.049713	45.985012
3476.788510	687764.803452	45.990017
3475.290711	685250.533828	45.995021
3474.309705	682677.117382	46.000026
3472.911014	680054.228074	46.005031
3471.824136	677367.805915	46.010036
3470.509965	674631.996246	46.015041
3468.980249	671844.665565	46.020045
3467.841386	668997.594563	46.025050
3466.327566	666097.996781	46.030055
3464.854962	663139.624357	46.035060
3463.678804	660137.064772	46.040065
3461.927886	657084.186922	46.045069
3460.470109	653958.230454	46.050074
3458.915867	650780.335173	46.055079
3457.309204	647566.897688	46.060084
3455.471618	644296.323182	46.065089
3453.786767	640974.054568	46.070093
3452.301696	637593.339848	46.075098
3450.196220	634178.491604	46.080103
3448.584477	630694.958807	46.085108
3447.266608	627172.717231	46.090113
3445.536303	623597.880111	46.095117
3443.746161	619962.932412	46.100122
3441.977291	616293.280846	46.105127
3439.904848	612548.588420	46.110132
3437.742835	608776.817231	46.115137
3435.866644	604949.690303	46.120141
3434.296160	601082.023071	46.125146
3432.161968	597145.712732	46.130151
3430.385350	593169.790009	46.135156
3428.465568	589144.867861	46.140161
3426.087721	585074.133485	46.145165
3424.290495	580956.884488	46.150170
3422.106731	576787.468353	46.155175
3419.947467	572580.628118	46.160180
3417.912720	568323.947626	46.165185
3415.587607	564027.637563	46.170189
3413.584637	559670.726233	46.175194
3411.094896	555274.672654	46.180199
3408.749266	550837.391020	46.185204
3406.619644	546353.205663	46.190209
3404.087354	541842.118675	46.195213
3401.994253	537264.083287	46.200218
3399.580206	532657.843412	46.205223
3397.252864	527999.452606	46.210228
3394.886760	523286.333569	46.215233
3392.541768	518561.490227	46.220237
3389.940402	513768.342248	46.225242
3387.431354	508953.804349	46.230247
3384.660242	504089.075394	46.235252
3382.186852	499180.470724	46.240257
3379.725003	494240.626275	46.245261
3376.972868	489258.058200	46.250266
3374.561470	484247.336618	46.255271
3371.889450	479185.936852	46.260276
3368.873010	474092.754781	46.265281
3365.875183	468963.381366	46.270285
3363.447960	463785.923708	46.275290
3360.483520	458599.236291	46.280295
3357.819359	453365.539186	46.285300
3355.142135	448098.526453	46.290305
3351.870235	442783.291901	46.295309
3349.277115	437455.549423	46.300314
3346.203289	432076.900333	46.305319
3343.355222	426677.839982	46.310324
3340.369677	421249.594618	46.315329
3337.061246	415792.672858	46.320333
3334.215981	410302.624281	46.325338
3331.233829	404796.359436	46.330343
3328.256961	399228.231094	46.335348
3325.161003	393652.596286	46.340353
3321.889900	388046.349248	46.345357
3319.171342	382406.346377	46.350362
3315.509794	376749.006619	46.355367
3312.473336	371068.715962	46.360372
3309.131591	365355.235238	46.365377
3305.826637	359627.565283	46.370381
3302.784399	353863.092841	46.375386
3298.943106	348087.367088	46.380391
3295.486710	342297.665253	46.385396
3292.515642	336474.341054	46.390401
3288.942237	330620.334742	46.395405
3285.465643	324764.359367	46.400410
3282.058246	318879.432962	46.405415
3278.489128	312998.732645	46.410420
3275.041001	307085.267830	46.415425
3271.346485	301163.001150	46.420429
3268.173387	295211.483500	46.425434
3264.145006	289258.771808	46.430439
3260.615964	283300.160489	46.435444
3257.130215	277323.220682	46.440449
3252.985023	271330.844119	46.445453
3249.667190	265327.216992	46.450458
3245.940897	259320.287499	46.455463
3241.692333	253298.844979	46.460468
3238.061616	247266.905665	46.465473
3234.191186	241253.137877	46.470477
3230.546670	235208.391618	46.475482
3226.404368	229183.036014	46.480487
3222.352314	223130.043329	46.485492
3218.705107	217089.651160	46.490497
3214.454854	211022.765849	46.495501
3210.572949	204907.544477	46.500506
3206.192340	198867.575460	46.505511
3202.222853	192823.973569	46.510516
3198.455112	186777.312196	46.515521
3193.978705	180747.227748	46.520525
3189.898497	174706.969072	46.525530
3185.526573	168677.291258	46.530535
3181.200001	162658.252120	46.535540
3176.768226	156654.377258	46.540545
3172.437914	150657.197775	46.545549
3168.100911	144671.180813	46.550554
3163.419589	138705.061159	46.555559
3158.690257	132746.796447	46.560564
3154.109268	126817.775799	46.565569
3149.344537	120898.715065	46.570573
3144.682958	115007.827293	46.575578
3139.688890	109140.176753	46.580583
3134.937388	103300.135253	46.585588
3130.092854	97481.608271	46.590593
3125.078903	91696.572543	46.595597
3120.184994	85933.428007	46.600602
3114.748229	80227.230769	46.605607
3109.073423	74543.962137	46.610612
3103.495299	68896.115283	46.615617
3097.531143	63324.828421	46.620621
3091.297935	57789.479670	46.625626
3084.667544	52331.008233	46.630631
3076.836417	46968.771715	46.635636
3066.186219	41756.384330	46.640641
3051.249177	36779.855339	46.645645
3036.133449	31963.239076	46.650650
3021.551492	27365.165203	46.655655
3007.022270	22985.130914	46.660660
2993.106468	18843.368705	46.665665
2979.567602	14971.620565	46.670669
2966.062708	11338.078954	46.675674
2950.801383	8023.522865	46.680679
2927.534242	5197.602617	46.685684
2902.872681	2766.183420	46.690689
2876.818536	782.655588	46.695693
2815.616504	244.961051	46.700698
2762.527369	254.915691	46.705703
2743.219968	256.207923	46.710708
2750.363402	239.196698	46.715713
2769.034994	248.591872	46.720717
2789.358176	234.037535	46.725722
2804.256209	239.322882	46.730727
2811.757199	232.222105	46.735732
2813.087028	241.526382	46.740737
2810.351587	238.344179	46.745741
2806.563274	235.332682	46.750746
2801.653900	222.857297	46.755751
2797.795368	226.825832	46.760756
2794.382896	216.565886	46.765761
2790.627074	232.313502	46.770765
2789.196452	214.780632	46.775770
2786.849352	219.724487	46.780775
2784.277935	214.932904	46.785780
2781.786879	209.737491	46.790785
2778.305391	219.404124	46.795789
2775.530438	216.401356	46.800794
2771.958416	214.001563	46.805799
2769.061342	218.564224	46.810804
2765.982250	209.154319	46.815809
2762.568220	210.631527	46.820813
2759.567361	201.138826	46.825818
2756.242261	209.511492	46.830823
2753.022586	205.123237	46.835828
2750.295374	206.099597	46.840833
2746.471617	217.296620	46.845837
2743.327684	202.827271	46.850842
2739.644961	204.376993	46.855847
2736.194303	200.098223	46.860852
2733.595693	202.068807	46.865857
2730.148110	208.042207	46.870861
2726.869483	200.489557	46.875866
2723.012757	210.348971	46.880871
2719.466571	207.000686	46.885876
2716.873299	205.120339	46.890881
2713.294740	204.744982	46.895885
2710.432838	198.201817	46.900890
2706.735600	206.595660	46.905895
2702.897093	209.234848	46.910900
2699.796078	202.522683	46.915905
2696.456790	204.662267	46.920909
2692.864233	202.918735	46.925914
2689.553358	196.938512	46.930919
2686.195967	204.266339	46.935924
2682.707895	194.335948	46.940929
2679.258512	190.026432	46.945933
2675.756657	200.932420	46.950938
2672.490755	202.177184	46.955943
2668.460945	198.195233	46.960948
2665.680696	182.583374	46.965953
2662.229648	195.603517	46.970957
2658.829367	197.228110	46.975962
2655.234003	192.483970	46.980967
2651.663867	196.016324	46.985972
2648.317601	192.366631	46.990977
2645.213570	185.190682	46.995981
2642.116655	184.232048	47.000986
2638.284083	188.615952	47.005991
2634.392138	198.223931	47.010996
2631.113990	190.609915	47.016001
2627.779135	195.243553	47.021005
2624.298867	177.559346	47.026010
2620.684325	184.089322	47.031015
2617.490549	188.333945	47.036020
2614.184553	186.281571	47.041025
2610.496288	194.785294	47.046029
2606.679206	186.309160	47.051034
2603.040040	187.430864	47.056039
2599.354319	183.263554	47.061044
2596.780831	185.726359	47.066049
2593.300581	191.715723	47.071053
2589.985564	183.011839	47.076058
2586.484621	180.476318	47.081063
2582.826099	196.298711	47.086068
2579.348699	187.596459	47.091073
2575.920410	191.999918	47.096077
2572.042423	189.452236	47.101082
2568.796635	188.850224	47.106087
2565.512357	190.641773	47.111092
2562.020579	190.856224	47.116097
2558.158739	182.570678	47.121101
2554.964002	181.546212	47.126106
2551.480550	189.756769	47.131111
2548.007785	190.613376	47.136116
2544.540514	172.802978	47.141121
2540.450690	184.358349	47.146125
2537.383309	175.336849	47.151130
2534.395816	177.258661	47.156135
2530.699895	177.561008	47.161140
2527.363145	178.540351	47.166145
2523.552868	181.576993	47.171149
2520.060931	176.419997	47.176154
2516.639604	173.290000	47.181159
2512.822134	179.223167	47.186164
2510.088161	182.120291	47.191169
2506.223079	179.238419	47.196173
2502.757544	181.416219	47.201178
2499.160880	187.135631	47.206183
2495.627537	184.642453	47.211188
2492.413815	170.148013	47.216193
2488.994722	185.435896	47.221197
2485.220951	178.395444	47.226202
2481.474265	179.946106	47.231207
2478.311840	172.719187	47.236212
2475.272925	165.719283	47.241217
2471.426750	171.807802	47.246221
2467.655171	167.485914	47.251226
2464.543492	166.076378	47.256231
2460.742748	186.013971	47.261236
2457.574105	168.800100	47.266241
2453.911595	181.892486	47.271245
2450.398188	165.737198	47.276250
2446.838581	163.061932	47.281255
2443.569240	167.181247	47.286260
2440.247194	162.593531	47.291265
2436.176308	174.986698	47.296269
2432.831061	165.959205	47.301274
2429.392634	173.002443	47.306279
2425.757495	174.736754	47.311284
2422.651687	164.641103	47.316289
2419.229078	177.965714	47.321293
2415.872608	162.707814	47.326298
2412.276685	167.775363	47.331303
2408.476683	163.003772	47.336308
2404.981621	161.152588	47.341313
2401.465296	166.467843	47.346317
2398.280432	162.546741	47.351322
2394.281592	154.984804	47.356327
2391.174801	155.827897	47.361332
2387.808949	158.586221	47.366337
2383.801407	160.709223	47.371341
2380.511286	151.734423	47.376346
2377.140946	156.772927	47.381351
2373.646786	149.151709	47.386356
2370.485902	154.089423	47.391361
2366.724947	165.267030	47.396365
2363.471377	157.400546	47.401370
2359.388277	164.925535	47.406375
2355.893073	161.088818	47.411380
2352.731852	151.633099	47.416385
2349.156252	159.162848	47.421389
2345.665245	157.262103	47.426394
2342.319413	156.802737	47.431399
2338.257148	152.621667	47.436404
2335.007862	146.257219	47.441409
2331.730199	149.789928	47.446413
2328.362298	154.977448	47.451418
2324.700268	151.338691	47.456423
2321.354010	159.493331	47.461428
2317.889454	154.276535	47.466433
2314.056828	149.603782	47.471437
2310.576002	153.485104	47.476442
2307.496546	158.516333	47.481447
2303.648155	174.217212	47.486452
2300.371603	155.041305	47.491457
2296.382367	159.844338	47.496461
2293.376728	147.907253	47.501466
2289.715263	159.936124	47.506471
2285.906427	157.033902	47.511476
2282.737132	157.822701	47.516481
2278.769414	158.436294	47.521485
2275.633482	158.801614	47.526490
2272.658610	153.529801	47.531495
2269.035806	157.620168	47.536500
2265.406443	152.101165	47.541505
2261.576944	165.708953	47.546509
2258.265378	151.749552	47.551514
2254.874076	152.496603	47.556519
2251.005689	161.300183	47.561524
2247.602788	156.814036	47.566529
2244.085127	159.655829	47.571533
2240.619729	152.695186	47.576538
2237.378371	159.214158	47.581543
2233.564315	153.471213	47.586548
2230.398469	155.643791	47.591553
2226.741649	158.921870	47.596557
2223.253161	155.346616	47.601562
2219.475880	153.321716	47.606567
2215.970028	152.310370	47.611572
2213.034259	153.873365	47.616577
2209.209854	154.556624	47.621581
2205.862748	152.025553	47.626586
2202.676171	155.893937	47.631591
2198.774278	162.247267	47.636596
2195.275270	145.927860	47.641601
2191.815210	152.966562	47.646605
2188.182646	155.181751	47.651610
2184.991173	151.643764	47.656615
2181.021202	151.014015	47.661620
2178.001644	151.666593	47.666625
2174.377557	154.311371	47.671629
2170.809577	148.298225	47.676634
2167.122042	153.723915	47.681639
2163.200495	155.560752	47.686644
2159.933972	147.104193	47.691649
2156.998614	152.362466	47.696653
2153.780983	150.279254	47.701658
2150.247264	146.169478	47.706663
2146.339327	160.542588	47.711668
2142.790426	147.784727	47.716673
2139.334156	149.239821	47.721677
2135.509923	149.101216	47.726682
2132.032834	150.006633	47.731687
2128.477100	149.211617	47.736692
2125.359623	152.692487	47.741697
2121.457463	157.456586	47.746701
2118.507963	151.300572	47.751706
2114.776232	145.885893	47.756711
2111.193885	154.693309	47.761716
2107.651901	143.988998	47.766721
2104.252211	156.723525	47.771725
2100.781061	152.271507	47.776730
2097.697433	147.366541	47.781735
2094.059816	147.903321	47.786740
2090.538024	140.650240	47.791745
2086.411241	146.994744	47.796749
2082.917253	152.783109	47.801754
2079.872489	144.542669	47.806759
2076.098503	147.905011	47.811764
2072.923219	139.993060	47.816769
2069.272265	149.377435	47.821773
2065.942966	146.501944	47.826778
2062.355149	148.726205	47.831783
2058.731942	148.927329	47.836788
2055.310922	151.005954	47.841793
2051.515258	151.132846	47.846797
2047.946180	139.419966	47.851802
2044.872519	147.510491	47.856807
2041.266671	147.396767	47.861812
2037.625548	138.692965	47.866817
2034.310688	145.595639	47.871821
2030.733823	140.703384	47.876826
2027.272235	139.950677	47.881831
2023.727254	147.301945	47.886836
2020.441125	142.617669	47.891841
2017.004939	143.094107	47.896845
2012.717920	141.249372	47.901850
2009.854888	140.344618	47.906855
2006.218498	148.738966	47.911860
2003.041926	130.619534	47.916865
1999.306200	143.293177	47.921869
1995.382772	142.229850	47.926874
1992.584679	147.854038	47.931879
1988.836267	137.569843	47.936884
1985.184815	132.810169	47.941889
1981.705848	136.763468	47.946893
1977.997961	142.547691	47.951898
1974.580058	140.251141	47.956903
1971.127496	150.002914	47.961908
1967.739800	140.254131	47.966913
1964.149873	143.672702	47.971917
1960.812317	136.382506	47.976922
1957.395318	139.093002	47.981927
1953.581918	136.144497	47.986932
1950.321569	143.114172	47.991937
1946.543211	146.303106	47.996941
1943.200277	140.248738	48.001946
1940.172211	137.253779	48.006951
1936.551323	145.572400	48.011956
1933.162283	140.223854	48.016961
1929.659596	142.656122	48.021965
1925.672442	139.530023	48.026970
1921.799615	139.064792	48.031975
1918.145729	142.097160	48.036980
1915.264592	127.116216	48.041985
1911.661917	148.429109	48.046989
1908.389290	131.946991	48.051994
1904.872786	134.724537	48.056999
1900.996475	130.851930	48.062004
1897.827862	132.147860	48.067009
1894.162597	140.469526	48.072013
1890.873673	143.795256	48.077018
1887.158398	139.434802	48.082023
1883.288262	143.833864	48.087028
1880.438209	135.188956	48.092033
1876.618527	139.681881	48.097037
1873.572627	137.485583	48.102042
1869.482733	139.851033	48.107047
1865.928135	134.478284	48.112052
1862.308517	134.477508	48.117057
1859.022606	131.771618	48.122061
1855.726508	124.635282	48.127066
1852.337660	124.522467	48.132071
1848.770834	136.130446	48.137076
1845.518985	132.334371	48.142081
1841.712423	139.301704	48.147085
1838.459402	131.587548	48.152090
1834.740342	140.149453	48.157095
1831.048911	140.538898	48.162100
1827.692648	139.235706	48.167105
1823.920443	143.202214	48.172109
1820.587224	135.053612	48.177114
1817.194905	128.577159	48.182119
1813.619800	132.289992	48.187124
1810.548601	125.811236	48.192129
1806.456940	134.132797	48.197133
1802.893164	141.715866	48.202138
1799.803682	138.992465	48.207143
1796.113479	140.977781	48.212148
1792.632505	128.471287	48.217153
1789.179397	137.881890	48.222157
1785.464900	139.445196	48.227162
1782.463451	136.086798	48.232167
1778.491752	141.756653	48.237172
1775.087338	140.535684	48.242177
1771.345139	140.345737	48.247181
1768.081896	137.946573	48.252186
1764.667422	130.426189	48.257191
1761.001602	132.894319	48.262196
1757.678951	138.794841	48.267201
1753.960125	132.341977	48.272205
1750.718552	139.688750	48.277210
1747.286539	132.566747	48.282215
1743.351412	137.214890	48.287220
1740.042384	133.439628	48.292225
1736.634207	130.233342	48.297229
1733.429106	138.183254	48.302234
1729.783326	127.038321	48.307239
1725.670676	130.401459	48.312244
1722.767116	128.677784	48.317249
1719.151281	135.934866	48.322253
1715.771681	134.862178	48.327258
1712.267230	134.050542	48.332263
1708.396865	137.557057	48.337268
1705.044969	124.420480	48.342273
1701.933121	136.164889	48.347277
1697.844271	138.745627	48.352282
1694.425761	123.321945	48.357287
1691.052274	135.437702	48.362292
1688.020234	124.901280	48.367297
1684.257480	126.928914	48.372301
1680.338743	126.381937	48.377306
1677.184172	132.217951	48.382311
1673.340660	138.787019	48.387316
1670.311268	129.321500	48.392321
1666.291282	126.668003	48.397325
1662.878876	122.235658	48.402330
1659.350038	124.209933	48.407335
1655.962746	132.503072	48.412340
1652.459791	133.158816	48.417345
1649.087294	128.089579	48.422349
1645.725942	133.773021	48.427354
1642.255630	124.167701	48.432359
1638.572971	135.537323	48.437364
1635.091874	123.639392	48.442369
1631.519620	132.066419	48.447373
1627.862770	130.111114	48.452378
1624.563591	123.844556	48.457383
1620.375264	123.671485	48.462388
1617.478804	121.328266	48.467393
1614.324881	116.856664	48.472397
1610.596527	127.228659	48.477402
1607.015278	121.033943	48.482407
1603.228594	128.548548	48.487412
1600.269491	123.151127	48.492417
1596.718835	131.460541	48.497421
1592.851776	127.033187	48.502426
1589.621243	123.601232	48.507431
1586.014106	113.711212	48.512436
1582.398272	126.768247	48.517441
1578.786878	126.848453	48.522445
1575.599935	124.653277	48.527450
1572.440285	124.257607	48.532455
1568.555502	123.729974	48.537460
1565.109844	126.605972	48.542465
1561.486229	120.373333	48.547469
1558.242402	130.213141	48.552474
1554.507396	124.571837	48.557479
1550.677172	136.545369	48.562484
1547.365346	120.039336	48.567489
1543.817662	122.853532	48.572493
1540.362975	115.016799	48.577498
1537.022459	119.732890	48.582503
1533.493290	125.549026	48.587508
1530.080440	117.401076	48.592513
1526.453795	127.538024	48.597517
1522.643402	126.547390	48.602522
1519.583577	121.417152	48.607527
1515.840780	126.388024	48.612532
1512.538958	115.821311	48.617537
1508.995622	116.955503	48.622541
1505.384675	124.633649	48.627546
1501.830007	109.674980	48.632551
1498.254987	115.360611	48.637556
1494.833524	116.373966	48.642561
1491.355214	114.624211	48.647565
1488.077114	120.860118	48.652570
1484.831184	114.170655	48.657575
1480.880115	113.965295	48.662580
1477.470538	118.230729	48.667585
1473.481748	110.416522	48.672589
1469.881814	120.997621	48.677594
1466.698571	108.005005	48.682599
1463.452814	124.893563	48.687604
1460.153527	110.264168	48.692609
1456.342664	123.871244	48.697613
1453.001020	113.121160	48.702618
1449.464104	113.474872	48.707623
1445.623241	116.971012	48.712628
1441.980605	119.979431	48.717633
1438.813739	123.069978	48.722637
1435.608933	125.732292	48.727642
1431.745183	126.391228	48.732647
1428.078253	120.386323	48.737652
1424.948580	115.598085	48.742657
1421.527971	113.099612	48.747661
1418.170857	121.551905	48.752666
1414.798180	116.842849	48.757671
1410.400684	119.628976	48.762676
1407.117286	122.065571	48.767681
1403.529742	125.630446	48.772685
1400.131213	120.378483	48.777690
1396.829928	123.021306	48.782695
1393.387590	127.885823	48.787700
1389.935535	122.644522	48.792705
1386.312113	126.167212	48.797709
1382.937663	133.261008	48.802714
1379.444866	130.067691	48.807719
1375.586755	126.520170	48.812724
1372.299064	121.396666	48.817729
1368.932641	129.436538	48.822733
1365.008812	136.793736	48.827738
1361.696339	137.514638	48.832743
1358.246485	128.985418	48.837748
1354.948024	134.233402	48.842753
1351.200567	134.124049	48.847757
1347.833866	124.374157	48.852762
1344.313551	123.238498	48.857767
1340.769345	130.669504	48.862772
1337.552725	127.614533	48.867777
1333.518615	114.509192	48.872781
1330.310307	128.482932	48.877786
1327.049880	122.552390	48.882791
1322.953906	119.133965	48.887796
1319.575134	117.633860	48.892801
1316.300161	122.948621	48.897805
1312.659474	119.612953	48.902810
1309.481028	115.518636	48.907815
1305.746731	123.851438	48.912820
1301.939997	118.271620	48.917825
1298.449836	114.782931	48.922829
1295.193748	119.240318	48.927834
1292.094515	118.493465	48.932839
1288.643074	124.708153	48.937844
1284.788496	112.527988	48.942849
1281.426770	122.549358	48.947853
1277.189429	121.944727	48.952858
1273.902470	115.823670	48.957863
1270.543860	121.275475	48.962868
1267.483065	122.812714	48.967873
1263.947126	119.959169	48.972877
1260.312355	122.390429	48.977882
1257.053366	125.632952	48.982887
1253.011005	121.381448	48.987892
1249.121448	122.314399	48.992897
1245.770147	111.056209	48.997901
1242.588054	121.536604	49.002906
1239.416048	111.838789	49.007911
1236.085497	121.406088	49.012916
1232.206269	119.306303	49.017921
1228.189791	116.871327	49.022925
1224.751092	121.734786	49.027930
1221.999318	117.588510	49.032935
1218.382282	111.886538	49.037940
1214.866936	116.596564	49.042945
1211.162785	116.978428	49.047949
1207.444192	122.006140	49.052954
1204.286584	111.373372	49.057959
1200.501951	119.478010	49.062964
1196.898973	115.155454	49.067969
1193.574034	117.028819	49.072973
1190.548560	126.349592	49.077978
1187.237311	114.569574	49.082983
1183.036338	123.972488	49.087988
1179.494411	114.115674	49.092993
1175.883822	129.845822	49.097997
1172.235480	119.838538	49.103002
1169.399580	121.187779	49.108007
1165.587089	124.923380	49.113012
1161.725446	119.086810	49.118017
1158.724010	112.087126	49.123021
1154.820776	119.219290	49.128026
1151.564836	107.619774	49.133031
1147.987845	122.457350	49.138036
1145.077219	118.601715	49.143041
1141.401174	115.879866	49.148045
1137.660943	115.765178	49.153050
1134.480562	114.231137	49.158055
1130.599657	115.004903	49.163060
1126.687771	109.207888	49.168065
1123.196736	107.473207	49.173069
1119.874034	114.967488	49.178074
1116.903119	109.217815	49.183079
1112.956022	123.188767	49.188084
1109.567106	115.359098	49.193089
1106.009406	116.067819	49.198093
1102.247596	122.007962	49.203098
1099.494501	115.537415	49.208103
1095.670972	120.144164	49.213108
1092.411954	121.371658	49.218113
1088.744410	114.663508	49.223117
1084.712489	121.473138	49.228122
1081.230717	114.510198	49.233127
1077.897544	117.716431	49.238132
1074.397155	112.515812	49.243137
1071.259857	119.204838	49.248141
1067.645872	123.365209	49.253146
1064.002119	111.575168	49.258151
1060.612531	120.805482	49.263156
1057.281000	106.384110	49.268161
1053.355003	114.970737	49.273165
1049.479765	120.787274	49.278170
1046.458350	115.503454	49.283175
1042.929083	130.125998	49.288180
1039.694375	118.315464	49.293185
1036.241502	120.608801	49.298189
1032.465278	118.708602	49.303194
1028.929306	118.717004	49.308199
1025.275518	118.858821	49.313204
1021.789414	118.644652	49.318209
1018.517365	117.618658	49.323213
1015.010041	113.006113	49.328218
1011.657057	117.479999	49.333223
1007.703739	113.316995	49.338228
1004.325082	119.828859	49.343233
1000.990568	107.861082	49.348237
997.455799	120.970629	49.353242
994.315491	103.490111	49.358247
990.405980	121.327978	49.363252
987.061214	122.086324	49.368257
983.596457	115.874466	49.373261
979.814764	114.354106	49.378266
976.318057	107.507020	49.383271
973.057600	115.238343	49.388276
969.469939	116.597043	49.393281
965.733076	117.412583	49.398285
962.035611	116.737055	49.403290
958.915769	112.052959	49.408295
955.510282	117.482406	49.413300
952.388525	121.012211	49.418305
948.341091	109.225551	49.423309
944.760787	117.694525	49.428314
941.635196	102.135415	49.433319
937.719062	119.113855	49.438324
934.397562	112.137287	49.443329
931.105140	113.977848	49.448333
927.251779	111.115931	49.453338
924.012516	101.755767	49.458343
920.032742	107.637722	49.463348
916.610272	112.677919	49.468353
913.509660	102.226197	49.473357
909.712949	116.136051	49.478362
906.294945	96.750691	49.483367
903.223526	105.700592	49.488372
899.795843	110.638463	49.493377
895.755173	112.108527	49.498381
892.440649	110.370810	49.503386
889.285318	111.306577	49.508391
885.233610	108.219118	49.513396
881.442897	115.094877	49.518401
878.097552	107.384496	49.523405
874.636050	116.520921	49.528410
871.480486	112.203948	49.533415
867.469285	111.714376	49.538420
864.297861	109.495516	49.543425
861.167707	111.222573	49.548429
857.220339	104.492635	49.553434
853.663513	102.667891	49.558439
850.366115	115.641258	49.563444
846.724342	103.077190	49.568449
843.103930	110.214596	49.573453
840.054121	115.045989	49.578458
836.614610	110.445646	49.583463
832.578772	104.892509	49.588468
829.221333	104.587303	49.593473
826.198220	110.219981	49.598477
822.001255	112.212751	49.603482
818.678504	102.463985	49.608487
815.238975	110.877730	49.613492
811.496577	111.622903	49.618497
808.192555	101.535180	49.623501
804.705864	114.393185	49.628506
801.611121	108.175537	49.633511
797.799773	109.321308	49.638516
794.493377	105.150407	49.643521
791.073585	102.976982	49.648525
787.187436	103.203575	49.653530
783.382640	104.840419	49.658535
780.008059	109.989797	49.663540
776.634726	109.022463	49.668545
773.150046	102.641852	49.673549
769.547020	107.715695	49.678554
766.575069	103.755107	49.683559
763.069641	101.713534	49.688564
758.945100	96.930398	49.693569
755.799021	104.347489	49.698573
752.193771	107.088265	49.703578
749.035039	107.740157	49.708583
745.098566	106.319136	49.713588
741.436257	108.836345	49.718593
738.279107	104.504954	49.723597
734.408071	107.021104	49.728602
731.468511	97.361548	49.733607
727.485359	103.659042	49.738612
724.009373	103.072086	49.743617
720.846845	95.515820	49.748621
717.075857	100.208326	49.753626
713.747881	101.429626	49.758631
710.607167	105.165225	49.763636
706.841036	91.783108	49.768641
703.155700	95.330102	49.773645
699.445003	97.530377	49.778650
696.308003	95.392576	49.783655
692.729385	107.398256	49.788660
689.061962	93.552220	49.793665
685.843564	100.811269	49.798669
682.131024	102.363434	49.803674
678.807093	94.951416	49.808679
674.918700	96.310984	49.813684
671.490742	103.525510	49.818689
668.413513	91.843328	49.823693
664.517875	104.213448	49.828698
660.819021	91.810226	49.833703
657.417124	108.333907	49.838708
654.106693	105.855136	49.843713
650.566367	100.085945	49.848717
647.098069	106.532664	49.853722
643.657259	112.595157	49.858727
640.038522	109.685702	49.863732
636.222497	108.095811	49.868737
633.357271	99.967922	49.873741
629.613301	101.687957	49.878746
625.973907	98.015710	49.883751
622.435931	108.138470	49.888756
619.402622	106.182821	49.893761
615.621195	106.670241	49.898765
611.705108	106.512056	49.903770
608.972641	99.446482	49.908775
605.271226	97.377613	49.913780
601.529720	95.330008	49.918785
598.087763	99.545899	49.923789
594.239024	103.462302	49.928794
591.350989	105.817340	49.933799
587.473829	100.991545	49.938804
583.701676	107.861137	49.943809
580.553466	93.241503	49.948813
576.867636	105.467739	49.953818
573.798642	99.885572	49.958823
569.977079	110.515645	49.963828
566.595323	106.596829	49.968833
563.044880	98.715589	49.973837
559.554177	96.956909	49.978842
556.049347	86.778076	49.983847
552.319816	105.826432	49.988852
548.905355	101.887807	49.993857
545.353829	90.920306	49.998861
541.775124	100.438361	50.003866
538.801284	93.606117	50.008871
535.116823	97.751038	50.013876
531.581830	95.777149	50.018881
528.120193	100.724325	50.023885
524.291414	108.141697	50.028890
520.985791	96.982028	50.033895
517.514766	104.473784	50.038900
514.007202	108.221918	50.043905
510.692699	100.576037	50.048909
507.200550	108.224046	50.053914
503.836849	107.149983	50.058919
499.699064	103.196949	50.063924
496.339393	99.759574	50.068929
493.043998	96.963907	50.073933
489.142029	103.173365	50.078938
486.018244	96.906361	50.083943
482.491241	100.683009	50.088948
478.985085	104.984652	50.093953
475.655194	95.922944	50.098957
471.813912	93.179478	50.103962
468.596493	89.588268	50.108967
464.886784	92.837419	50.113972
461.267531	98.979031	50.118977
458.297144	98.316242	50.123981
454.497479	95.659812	50.128986
450.788204	97.114177	50.133991
447.493790	104.080173	50.138996
443.986040	99.245669	50.144001
440.292295	92.233136	50.149005
436.424656	98.955725	50.154010
433.079010	93.910397	50.159015
429.749726	101.921542	50.164020
426.575650	105.038551	50.169025
423.396198	98.477551	50.174029
419.418463	100.330548	50.179034
415.763370	96.017821	50.184039
412.202258	103.930934	50.189044
408.920871	102.361995	50.194049
405.797258	96.298681	50.199053
401.968779	100.207171	50.204058
398.197736	94.466297	50.209063
394.510143	98.665939	50.214068
391.292014	88.924892	50.219073
387.855210	96.045218	50.224077
384.369746	103.918361	50.229082
381.201196	93.386667	50.234087
377.461248	91.119402	50.239092
373.644514	91.308448	50.244097
370.202089	92.454733	50.249101
366.504293	97.841267	50.254106
363.253694	89.332054	50.259111
360.111458	98.684620	50.264116
356.539842	97.250765	50.269121
352.973975	100.808831	50.274125
349.252677	98.563557	50.279130
345.868091	94.999435	50.284135
342.139065	95.745216	50.289140
338.610293	94.555069	50.294145
335.198250	87.190781	50.299149
331.396637	95.001241	50.304154
328.270236	103.632721	50.309159
324.974048	100.404394	50.314164
321.553427	99.099604	50.319169
318.169357	101.982624	50.324173
314.215108	101.865820	50.329178
310.802702	100.270191	50.334183
307.229352	96.479355	50.339188
303.791208	93.495050	50.344193
300.302363	90.075374	50.349197
296.772779	93.510642	50.354202
293.336956	92.444413	50.359207
290.102712	91.006474	50.364212
286.364531	97.570556	50.369217
282.921113	83.080981	50.374221
279.295789	92.126697	50.379226
275.468671	83.900421	50.384231
271.984161	85.984005	50.389236
268.128089	101.104817	50.394241
265.301969	95.977874	50.399245
261.607994	100.308941	50.404250
258.896629	95.652517	50.409255
254.664355	101.504461	50.414260
251.122351	95.155603	50.419265
247.801409	96.872824	50.424269
244.042989	101.958157	50.429274
240.320742	103.810730	50.434279
236.944470	95.735726	50.439284
233.692503	107.442231	50.444289
230.276240	97.210735	50.449293
226.702832	97.998263	50.454298
223.368069	100.613289	50.459303
219.810896	96.833272	50.464308
216.145488	99.321499	50.469313
212.920991	92.696943	50.474317
209.079888	100.267813	50.479322
205.835879	99.768892	50.484327
202.113772	102.043372	50.489332
198.063368	97.731235	50.494337
195.433689	93.528963	50.499341
191.738389	99.620309	50.504346
188.349025	90.171545	50.509351
184.770459	98.519513	50.514356
181.132164	94.299350	50.519361
177.535467	99.364190	50.524365
174.127135	98.324091	50.529370
170.685980	89.944801	50.534375
167.153264	103.492923	50.539380
163.665678	103.393851	50.544385
160.264846	100.038815	50.549389
156.376854	97.741914	50.554394
153.019710	91.656070	50.559399
149.668047	97.485721	50.564404
146.167757	99.297755	50.569409
143.123595	86.860922	50.574413
138.933871	91.074586	50.579418
135.625363	91.981770	50.584423
132.032333	103.178685	50.589428
128.339496	98.059721	50.594433
125.264247	94.892741	50.599437
121.528999	100.930211	50.604442
118.275917	91.181622	50.609447
114.817683	99.870376	50.614452
110.692922	98.361937	50.619457
107.454135	92.816690	50.624461
104.261073	96.633498	50.629466
100.562685	99.570719	50.634471
97.179547	91.771485	50.639476
93.605808	92.219590	50.644481
89.977822	92.604886	50.649485
86.326236	93.428628	50.654490
83.395160	88.799780	50.659495
79.338229	97.424274	50.664500
75.872495	96.660203	50.669505
73.076040	92.328665	50.674509
69.351223	94.210249	50.679514
65.698935	83.687827	50.684519
61.950079	92.552791	50.689524
57.992022	97.709369	50.694529
54.793110	94.574250	50.699533
51.281344	94.418922	50.704538
48.167009	83.345756	50.709543
44.752797	87.203115	50.714548
40.784258	90.982308	50.719553
37.491507	84.982372	50.724557
33.671856	96.742127	50.729562
30.679641	90.713163	50.734567
26.876629	92.814982	50.739572
23.558925	91.847577	50.744577
20.379452	83.231767	50.749581
16.700395	89.674585	50.754586
13.219180	86.561957	50.759591
9.507751	78.147842	50.764596
5.947372	93.730620	50.769601
2.180909	75.447702	50.774605