Fri Jun 17 18:11:43 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.255308	94.139296	0.000000
1.183991	100.782664	0.005005
1.761378	96.306990	0.010010
1.670267	97.527860	0.015014
1.397837	97.194900	0.020019
1.458881	102.047796	0.025024
1.137022	94.617393	0.030029
1.239593	80.575750	0.035034
0.771546	73.236748	0.040038
0.914573	64.573722	0.045043
0.523773	56.960822	0.050048
0.018585	59.002144	0.055053
0.196692	44.402756	0.060058
-0.443442	40.991209	0.065062
-0.590257	30.586997	0.070067
-1.389279	22.907389	0.075072
-1.496602	19.345520	0.080077
-1.637353	10.602022	0.085082
-1.846409	17.301399	0.090086
-1.819349	7.284468	0.095091
-2.349932	8.255550	0.100096
-2.747475	4.809411	0.105101
-2.663915	-3.400689	0.110106
-3.511878	1.834735	0.115110
-3.419763	2.993570	0.120115
-3.924466	-0.466723	0.125120
-4.254527	-1.514100	0.130125
-4.051090	-5.369937	0.135130
-4.168086	2.217108	0.140134
-4.849258	-1.836818	0.145139
-5.281957	-4.008879	0.150144
-5.822211	3.657400	0.155149
-5.498647	-11.856854	0.160154
-5.748595	-3.167535	0.165158
-5.953285	-3.395525	0.170163
-6.567327	-0.686509	0.175168
-7.464971	-0.536475	0.180173
-7.328203	-11.529462	0.185178
-7.127212	-17.106385	0.190182
-7.280115	-8.387222	0.195187
-7.510900	-15.012413	0.200192
-7.880001	-13.044236	0.205197
-7.600469	-11.614642	0.210202
-8.230389	-9.082754	0.215206
-8.783371	-13.062873	0.220211
-9.195352	-7.051801	0.225216
-9.106273	-7.359799	0.230221
-9.173126	-11.619827	0.235226
-9.710121	-2.174976	0.240230
-9.765451	-2.521524	0.245235
-10.361431	-6.741947	0.250240
-10.812744	2.724381	0.255245
-10.854996	-5.951812	0.260250
-10.969708	-13.302537	0.265254
-10.885640	0.041104	0.270259
-11.083355	-7.874197	0.275264
-11.263146	3.309341	0.280269
-11.901664	-6.312991	0.285274
-12.195677	-4.534099	0.290278
-11.960047	-11.563793	0.295283
-12.419959	-1.503855	0.300288
-12.905576	-3.216420	0.305293
-13.462934	-7.879753	0.310298
-13.611280	-7.331345	0.315302
-13.671835	-10.605973	0.320307
-13.850565	-6.767584	0.325312
-14.124686	1.242406	0.330317
-13.910960	-12.477235	0.335322
-14.649453	-6.500293	0.340326
-15.000908	0.015946	0.345331
-15.469326	-7.648149	0.350336
-15.737157	-8.206429	0.355341
-15.554129	0.019026	0.360346
-15.441768	-9.410613	0.365350
-15.413263	6.133998	0.370355
-16.183804	1.663567	0.375360
-16.516128	0.571773	0.380365
-16.784282	-0.452347	0.385370
-17.658497	0.009324	0.390374
-17.780093	5.647133	0.395379
-17.850317	9.690076	0.400384
-17.928136	2.909413	0.405389
-17.967709	4.532548	0.410394
-18.177937	-10.568373	0.415398
-18.356696	-2.850693	0.420403
-18.558000	-5.314191	0.425408
-19.878124	3.454750	0.430413
-20.123386	-0.348013	0.435418
-19.686518	8.922535	0.440422
-20.201790	2.729614	0.445427
-20.016342	-5.796965	0.450432
-20.279348	6.760397	0.455437
-20.347616	6.563405	0.460442
-20.564340	2.267904	0.465446
-21.103512	-2.158501	0.470451
-21.609902	-0.111063	0.475456
-21.716203	-2.969027	0.480461
-21.602627	4.574365	0.485466
-21.906130	-1.571665	0.490470
-22.257253	-0.001525	0.495475
-22.774669	-1.337628	0.500480
-23.320507	3.390172	0.505485
-23.287436	-1.384131	0.510490
-23.601712	2.736082	0.515494
-23.558382	-0.674411	0.520499
-23.317415	1.092119	0.525504
-24.401095	-0.004228	0.530509
-24.493096	-8.577037	0.535514
-24.900003	0.331757	0.540518
-24.857917	3.269143	0.545523
-24.851395	-4.659782	0.550528
-25.034243	6.074356	0.555533
-25.765493	-1.400817	0.560538
-26.570048	0.761696	0.565542
-26.657856	-1.402967	0.570547
-26.162648	4.934059	0.575552
-26.355584	-2.219362	0.580557
-26.144015	-0.573249	0.585562
-27.017942	0.801811	0.590566
-27.518916	-2.777494	0.595571
-27.826305	-6.846582	0.600576
-28.100305	0.695126	0.605581
-27.890638	-3.393016	0.610586
-28.175161	-7.018758	0.615590
-28.845594	-7.419936	0.620595
-29.192454	-2.397844	0.625600
-29.536546	4.172425	0.630605
-29.522455	-14.585970	0.635610
-29.723620	0.941756	0.640614
-29.714934	-0.697478	0.645619
-29.770644	-1.095859	0.650624
-30.898373	1.775309	0.655629
-30.722816	-5.179086	0.660634
-30.910513	-3.037021	0.665638
-31.279855	-6.686946	0.670643
-31.026793	-7.633724	0.675648
-31.341711	-1.880511	0.680653
-31.593989	-4.275743	0.685658
-32.326441	0.001989	0.690662
-32.550895	-1.489959	0.695667
-32.500292	0.662813	0.700672
-32.897133	-1.824814	0.705677
-33.435000	-11.356915	0.710682
-34.134522	-3.376063	0.715686
-34.375388	-9.022800	0.720691
-33.780752	-5.689665	0.725696
-34.153160	-1.813555	0.730701
-33.964049	-7.299906	0.735706
-34.640854	-4.071346	0.740710
-34.852566	-8.915658	0.745715
-34.918380	-5.803659	0.750720
-35.552846	-4.841353	0.755725
-35.490545	-8.294463	0.760730
-35.887606	-1.187733	0.765734
-36.079503	-2.243077	0.770739
-36.190135	-13.834676	0.775744
-37.064347	1.766450	0.780749
-37.386241	-9.961315	0.785754
-37.523155	-4.056347	0.790758
-37.536660	-1.736437	0.795763
-37.498497	-10.401721	0.800768
-37.905514	0.315607	0.805773
-37.736692	-11.755780	0.810778
-38.108330	-8.712920	0.815782
-38.869936	-3.598010	0.820787
-39.203927	-10.068110	0.825792
-39.477670	-1.931302	0.830797
-39.394842	-5.550424	0.835802
-39.352455	-11.685274	0.840806
-39.878010	-2.841414	0.845811
-40.182262	-7.483867	0.850816
-40.869224	-1.585537	0.855821
-40.491199	-4.030291	0.860826
-40.904290	-7.381881	0.865830
-41.039972	-6.848996	0.870835
-41.853309	-2.750410	0.875840
-42.220073	0.575794	0.880845
-42.106007	-7.956085	0.885850
-42.329151	-5.989670	0.890854
-42.173332	0.996543	0.895859
-42.261330	-1.186637	0.900864
-42.412857	1.030320	0.905869
-42.751859	-4.217089	0.910874
-43.750694	-2.907692	0.915878
-44.078800	-5.522377	0.920883
-44.087989	-1.129655	0.925888
-43.893932	0.544231	0.930893
-44.420951	-3.363043	0.935898
-45.148446	-0.132172	0.940902
-45.216272	-0.664499	0.945907
-45.339277	-7.213479	0.950912
-45.607312	2.815356	0.955917
-45.131756	-4.215547	0.960922
-45.817322	4.382800	0.965926
-46.372260	1.322957	0.970931
-46.863924	-10.532080	0.975936
-47.384309	5.502371	0.980941
-47.332205	-10.255054	0.985946
-47.299378	-7.328366	0.990950
-47.216058	-7.871807	0.995955
-47.115752	-6.083674	1.000960
-47.485452	-6.264893	1.005965
-48.071985	-2.588207	1.010970
-48.729781	1.905428	1.015974
-48.740126	-14.594026	1.020979
-48.535341	-7.176112	1.025984
-49.086006	-2.024239	1.030989
-49.972409	5.358601	1.035994
-50.477629	-2.843999	1.040998
-50.513238	1.712754	1.046003
-49.966916	-0.295860	1.051008
-50.116056	4.693170	1.056013
-50.307549	-1.094972	1.061018
-50.313269	9.205001	1.066022
-51.291210	0.612127	1.071027
-51.799840	-10.072889	1.076032
-51.988237	5.602883	1.081037
-51.755784	-2.117924	1.086042
-52.162046	-1.423635	1.091046
-52.357460	-2.224233	1.096051
-53.047058	-6.927735	1.101056
-53.603144	2.314678	1.106061
-53.297640	-6.382616	1.111066
-53.543946	-3.106232	1.116070
-53.575593	6.611588	1.121075
-53.653734	-10.177526	1.126080
-53.726090	1.262435	1.131085
-54.105475	-13.244416	1.136090
-54.922315	-5.336213	1.141094
-54.919706	-1.278346	1.146099
-54.869820	-5.066627	1.151104
-55.952924	-8.638942	1.156109
-56.219883	-3.722284	1.161114
-56.058194	-6.606639	1.166118
-56.548522	-4.177866	1.171123
-56.262181	-11.912954	1.176128
-56.924218	-0.945250	1.181133
-56.770630	-4.313095	1.186138
-56.961300	-5.277278	1.191142
-57.536063	0.390868	1.196147
-57.831165	0.113582	1.201152
-58.409660	-3.230442	1.206157
-58.515508	2.828411	1.211162
-58.559007	4.353928	1.216166
-59.185499	-1.207393	1.221171
-58.439154	-5.586814	1.226176
-58.765517	0.362671	1.231181
-59.459802	-8.040948	1.236186
-59.773476	0.690933	1.241190
-60.386674	-4.594364	1.246195
-60.326049	-2.971113	1.251200
-60.331834	-2.777717	1.256205
-60.272003	-9.517516	1.261210
-61.017658	-6.093400	1.266214
-61.622748	-0.696275	1.271219
-61.687961	-6.771406	1.276224
-61.966710	-6.620642	1.281229
-61.620559	-13.145194	1.286234
-61.863263	-10.842832	1.291238
-62.780973	-0.249777	1.296243
-62.722054	-11.986969	1.301248
-63.589683	-5.833255	1.306253
-63.427264	-14.617657	1.311258
-63.844547	-11.851559	1.316262
-63.601015	-4.172509	1.321267
-63.478520	-19.117382	1.326272
-64.068085	-12.036473	1.331277
-64.842007	-3.069433	1.336282
-65.006262	0.285267	1.341286
-65.427785	-9.333852	1.346291
-65.359597	-9.924307	1.351296
-65.526596	-4.004670	1.356301
-65.194769	-11.798624	1.361306
-65.402557	-12.004192	1.366310
-66.735917	3.665371	1.371315
-66.507611	-15.023253	1.376320
-67.177285	-5.178659	1.381325
-66.934955	-11.631490	1.386330
-66.987625	-6.412037	1.391334
-67.388222	2.018568	1.396339
-67.776735	-3.393468	1.401344
-68.095858	-4.239408	1.406349
-67.875713	-6.738823	1.411354
-68.227893	-4.376625	1.416358
-68.825257	-1.397665	1.421363
-69.179015	-5.570333	1.426368
-69.510167	-7.639684	1.431373
-69.333809	-12.679134	1.436378
-69.837824	-6.991967	1.441382
-69.935964	1.110717	1.446387
-70.153110	-12.332663	1.451392
-70.774259	-7.427573	1.456397
-70.747226	-9.760702	1.461402
-71.024516	-7.972550	1.466406
-71.565350	-8.038099	1.471411
-71.589738	-8.357625	1.476416
-71.533666	-4.623978	1.481421
-71.788807	-8.011688	1.486426
-72.261423	-13.534450	1.491430
-72.731590	-5.227453	1.496435
-72.789727	-14.043663	1.501440
-72.863493	-9.704342	1.506445
-73.272354	-7.545046	1.511450
-73.547358	-4.110567	1.516454
-74.209520	-13.259699	1.521459
-74.444019	-9.330345	1.526464
-75.092965	-16.175691	1.531469
-74.575976	-16.593304	1.536474
-74.407655	-6.592419	1.541478
-74.810713	-4.609907	1.546483
-74.686202	-12.416559	1.551488
-75.354425	-0.576620	1.556493
-75.837724	-11.581960	1.561498
-76.251135	-4.112783	1.566502
-76.369928	-9.673053	1.571507
-76.080785	-12.138158	1.576512
-76.455445	-16.505860	1.581517
-77.548887	-21.100580	1.586522
-77.930754	-14.224295	1.591526
-78.026879	-18.733412	1.596531
-77.783376	-9.767584	1.601536
-77.878073	-6.555277	1.606541
-77.940093	-0.237910	1.611546
-77.825620	-6.232801	1.616550
-78.744633	-3.417233	1.621555
-79.104806	-7.086632	1.626560
-79.343294	-5.074450	1.631565
-79.301351	-11.825876	1.636570
-79.576887	-5.656927	1.641574
-80.623957	-4.590898	1.646579
-80.631770	-7.701826	1.651584
-80.914288	-10.401240	1.656589
-80.992908	-12.731604	1.661594
-80.927482	-5.639798	1.666598
-80.712659	-0.418439	1.671603
-80.676878	-12.184145	1.676608
-81.790807	-6.422422	1.681613
-81.863815	-13.748301	1.686618
-82.015583	-10.474216	1.691622
-82.956479	-9.544036	1.696627
-83.332184	-14.217621	1.701632
-83.342440	-10.756708	1.706637
-83.422536	-12.442944	1.711642
-83.669070	-15.769726	1.716646
-84.016953	-6.475499	1.721651
-84.037587	-8.652905	1.726656
-84.423641	-7.527652	1.731661
-84.139393	-9.292809	1.736666
-84.365263	-6.619898	1.741670
-85.462525	-3.436081	1.746675
-85.653838	-14.854423	1.751680
-86.045337	-10.893444	1.756685
-86.195221	-10.788372	1.761690
-86.279894	-6.175318	1.766694
-85.985024	-5.863582	1.771699
-85.628218	-9.794445	1.776704
-86.637450	-7.649003	1.781709
-87.193718	-6.572017	1.786714
-87.665804	-8.367723	1.791718
-87.826348	-5.181962	1.796723
-87.486909	-8.311744	1.801728
-87.953326	-3.709423	1.806733
-88.139810	-16.381602	1.811738
-88.592214	-9.093999	1.816742
-89.013787	-9.936126	1.821747
-88.646199	-9.805195	1.826752
-88.995256	-12.108755	1.831757
-89.878136	-11.655690	1.836762
-90.309689	-14.270141	1.841766
-90.480714	6.712652	1.846771
-90.611702	-9.371100	1.851776
-90.771596	-3.976156	1.856781
-90.745076	-8.407592	1.861786
-90.765260	-12.222898	1.866790
-90.978295	-4.750131	1.871795
-91.187231	-10.501425	1.876800
-92.163289	-8.190610	1.881805
-92.067198	-12.174624	1.886810
-92.397356	-9.302440	1.891814
-92.431427	-4.831586	1.896819
-92.555418	-20.354103	1.901824
-93.384172	-6.864849	1.906829
-93.282413	-7.001702	1.911834
-93.446758	1.313657	1.916838
-93.840327	-2.721167	1.921843
-93.772472	-8.245176	1.926848
-94.359935	-1.636225	1.931853
-94.924999	-6.325097	1.936858
-94.994264	-8.470343	1.941862
-95.366061	-11.691055	1.946867
-95.287597	-9.695058	1.951872
-95.698294	-9.134606	1.956877
-95.643554	-4.353122	1.961882
-95.530526	-7.218732	1.966886
-96.397912	-11.377046	1.971891
-96.739381	-11.123503	1.976896
-97.127659	-5.628039	1.981901
-97.323745	-8.837312	1.986906
-96.861530	-10.541679	1.991910
-97.454169	-8.509889	1.996915
-98.267480	-7.811745	2.006912
-97.360575	-8.747030	2.016909
-97.147346	-8.025466	2.026906
-96.476108	-7.845347	2.036902
-95.604797	-1.766311	2.046899
-95.488084	-6.131632	2.056896
-95.620125	-5.845832	2.066893
-95.083486	-12.744206	2.076890
-94.098353	-5.436565	2.086886
-92.940617	-2.637573	2.096883
-92.929405	-9.332224	2.106880
-92.678637	-7.693999	2.116877
-92.705719	-9.685779	2.126874
-92.197741	-2.197453	2.136870
-90.724567	-2.252008	2.146867
-89.930728	-8.685358	2.156864
-89.940125	-10.015612	2.166861
-89.961313	-5.613064	2.176858
-89.109620	-3.918450	2.186854
-88.630893	-4.453381	2.196851
-88.307287	-9.723639	2.206848
-87.397584	-8.111379	2.216845
-87.135377	-7.830659	2.226842
-86.491442	-8.044521	2.236838
-85.629782	-5.781345	2.246835
-85.186029	-10.778760	2.256832
-85.476749	-7.302713	2.266829
-84.809264	-9.346338	2.276826
-84.344546	-10.348194	2.286822
-83.301020	-12.556086	2.296819
-82.627118	-6.430399	2.306816
-82.201003	-4.167723	2.316813
-82.114524	-5.814043	2.326810
-81.832409	-7.586340	2.336806
-81.531525	-9.060248	2.346803
-80.578319	-6.896261	2.356800
-79.504720	-10.253739	2.366797
-79.292632	-7.130978	2.376794
-79.193477	-6.268542	2.386790
-78.764702	-5.468804	2.396787
-78.075983	-3.246820	2.406784
-77.553911	-8.743700	2.416781
-77.184575	-5.363747	2.426778
-75.918749	-3.640568	2.436774
-75.813090	-0.815254	2.446771
-75.949058	3.481507	2.456768
-75.093896	1.305917	2.466765
-74.544165	-3.299333	2.476762
-74.258340	-2.691590	2.486758
-73.318934	-0.628641	2.496755
-72.855455	1.253211	2.506752
-72.832969	1.744097	2.516749
-71.649702	-1.347094	2.526746
-71.323092	-5.692579	2.536742
-71.631196	-3.052177	2.546739
-70.175253	-3.546442	2.556736
-69.625696	-1.159062	2.566733
-69.576368	-3.020694	2.576730
-69.520370	-6.049362	2.586726
-68.809127	-9.158305	2.596723
-68.105205	2.340362	2.606720
-67.115266	-3.137678	2.616717
-67.104881	1.000596	2.626714
-66.619387	-2.348423	2.636710
-65.856080	-3.539012	2.646707
-65.916723	-0.347793	2.656704
-64.682843	-4.055946	2.666701
-63.945225	-0.796289	2.676698
-64.333676	-3.205750	2.686694
-64.008595	-1.700399	2.696691
-63.095336	-6.232119	2.706688
-62.503722	3.037141	2.716685
-61.342927	-5.490121	2.726682
-61.535032	0.183431	2.736678
-60.913365	-1.907106	2.746675
-60.820449	-4.028295	2.756672
-59.793812	-5.650509	2.766669
-59.137176	-6.110095	2.776666
-59.070636	-6.265707	2.786662
-59.098724	-5.783010	2.796659
-57.897498	-3.686722	2.806656
-57.438586	-4.398549	2.816653
-56.418336	-5.893446	2.826650
-56.161916	-7.946185	2.836646
-56.157543	-4.596447	2.846643
-55.793726	-7.791079	2.856640
-54.633667	-7.468549	2.866637
-54.363852	-5.543239	2.876634
-54.259299	-12.518760	2.886630
-53.720828	-9.220268	2.896627
-52.854402	-10.089143	2.906624
-52.640984	-8.611267	2.916621
-51.740891	-6.513919	2.926618
-51.573406	-0.581443	2.936614
-51.038359	-9.646623	2.946611
-50.380766	-12.142046	2.956608
-49.674642	-8.650724	2.966605
-49.638742	-6.126387	2.976602
-48.855738	-2.873876	2.986598
-47.848432	-1.921352	2.996595
-47.946358	-5.480032	3.006592
-48.111129	-6.116832	3.016589
-46.833408	-1.004926	3.026586
-46.454880	-4.741401	3.036582
-46.061658	-7.748871	3.046579
-45.171109	-0.079918	3.056576
-44.838560	-0.570984	3.066573
-44.690145	-1.183381	3.076570
-43.861569	2.674849	3.086566
-43.515095	-13.801082	3.096563
-43.218484	-6.143257	3.106560
-42.408691	-7.347100	3.116557
-42.080725	-3.121730	3.126554
-41.254389	-3.834765	3.136550
-40.272920	-4.223868	3.146547
-40.343767	2.279129	3.156544
-40.194597	-4.261231	3.166541
-39.891954	-3.816321	3.176538
-39.049929	-0.499921	3.186534
-38.433684	4.155481	3.196531
-37.471808	-1.970895	3.206528
-37.079347	0.677528	3.216525
-37.042193	-2.206540	3.226522
-36.895826	1.572453	3.236518
-35.734436	1.353197	3.246515
-35.550980	-1.558549	3.256512
-34.626238	-3.454461	3.266509
-34.046190	-3.972836	3.276506
-34.138105	-2.919782	3.286502
-33.805106	-0.865875	3.296499
-32.737448	3.316364	3.306496
-32.291005	-0.436537	3.316493
-32.355033	-4.909925	3.326490
-31.231282	-3.303000	3.336486
-31.177369	-3.792995	3.346483
-30.245214	4.514350	3.356480
-29.475264	-1.379181	3.366477
-29.199194	-1.204887	3.376474
-29.527935	-1.906703	3.386470
-28.785529	-4.708445	3.396467
-27.887126	-0.494316	3.406464
-26.846021	-6.804173	3.416461
-26.741291	-8.592820	3.426458
-26.352882	1.830117	3.436454
-26.332503	-5.974496	3.446451
-25.011878	-2.696748	3.456448
-24.654175	-8.023253	3.466445
-24.267076	-9.661848	3.476442
-24.296230	-3.420466	3.486438
-23.152206	-1.787666	3.496435
-22.773622	-1.057623	3.506432
-22.680141	-2.088059	3.516429
-21.700836	-7.655603	3.526426
-21.183606	-7.787339	3.536422
-21.127815	-1.855065	3.546419
-20.251189	-3.869427	3.556416
-19.663500	-2.793798	3.566413
-19.648972	-1.733344	3.576410
-18.967303	-7.622669	3.586406
-18.571778	-2.524152	3.596403
-18.122058	-1.603214	3.606400
-17.082052	-4.241232	3.616397
-16.721300	-2.662378	3.626394
-16.838634	2.714230	3.636390
-15.839239	-1.621770	3.646387
-15.421488	1.114920	3.656384
-14.993337	2.149299	3.666381
-13.726992	1.565454	3.676378
-13.414864	-0.470463	3.686374
-13.632145	-0.812636	3.696371
-13.334249	-5.240676	3.706368
-12.538936	-0.255832	3.716365
-11.751418	3.767100	3.726362
-10.916165	2.547373	3.736358
-10.884335	6.779296	3.746355
-10.373503	9.366162	3.756352
-10.038800	2.201820	3.766349
-9.186801	6.285757	3.776346
-9.242931	4.205740	3.786342
-8.374042	12.411584	3.796339
-7.439077	6.433128	3.806336
-7.126836	11.590347	3.816333
-6.966270	5.075947	3.826330
-6.531750	8.311908	3.836326
-5.933224	10.608967	3.846323
-5.785845	12.578344	3.856320
-4.813407	20.756510	3.866317
-4.530089	25.663661	3.876314
-3.759411	38.010563	3.886310
-3.655448	37.405752	3.896307
-3.181017	51.735839	3.906304
-2.720640	60.849535	3.916301
-2.095650	63.957626	3.926298
-1.695188	78.247674	3.936294
-0.947791	92.986869	3.946291
-0.709098	91.089600	3.956288
-0.254404	109.782487	3.966285
0.000000	130.998456	3.971290
0.702335	129.254765	3.976294
0.534786	136.228096	3.981299
0.821050	143.430874	3.986304
0.569913	148.483475	3.991309
0.861137	137.324997	3.996314
0.699270	143.983435	4.001318
0.850126	140.366192	4.006323
0.904673	134.325558	4.011328
0.912822	141.796165	4.016333
0.498437	144.076370	4.021338
0.853215	153.706377	4.026342
0.967024	160.601577	4.031347
1.312653	170.696251	4.036352
1.109727	158.530431	4.041357
1.242114	159.610558	4.046362
1.063056	144.779577	4.051366
1.085120	153.499940	4.056371
1.004708	146.168103	4.061376
1.190560	151.738286	4.066381
1.180844	144.804358	4.071386
1.151171	136.844473	4.076390
0.939715	142.387947	4.081395
0.952290	145.706379	4.086400
0.897690	157.967168	4.091405
1.187189	162.502492	4.096410
1.706356	163.289623	4.101414
1.344826	163.964441	4.106419
1.119317	150.604582	4.111424
0.960871	146.655138	4.116429
0.881772	163.494130	4.121434
0.952544	162.220672	4.126438
0.995086	172.773017	4.131443
1.675861	164.463166	4.136448
1.070535	170.831841	4.141453
1.175993	173.153316	4.146458
1.483938	166.329967	4.151462
1.148587	172.961606	4.156467
1.747806	167.628037	4.161472
1.703001	169.513720	4.166477
1.768668	167.042127	4.171482
1.494216	157.969519	4.176486
1.322122	153.961564	4.181491
1.359692	151.950280	4.186496
1.341784	153.599035	4.191501
1.093024	148.669463	4.196506
1.244511	153.029604	4.201510
0.939222	171.857803	4.206515
1.587616	170.816693	4.211520
1.564260	178.168038	4.216525
1.715400	172.210000	4.221530
1.714953	176.116084	4.226534
1.102571	178.818933	4.231539
1.805136	167.164051	4.236544
1.815751	183.980261	4.241549
1.512988	167.714700	4.246554
1.393160	166.187582	4.251558
1.575245	171.086683	4.256563
1.584518	174.621353	4.261568
1.389526	177.552399	4.266573
1.222156	173.406509	4.271578
1.500225	161.443117	4.276582
1.367444	172.841751	4.281587
1.367806	166.590482	4.286592
1.448184	166.393446	4.291597
1.274190	175.156079	4.296602
1.388002	174.071021	4.301606
0.958458	183.684206	4.306611
1.519118	192.427941	4.311616
1.652922	196.784126	4.316621
1.751127	201.799003	4.321626
2.097959	198.906924	4.326630
1.821577	202.967018	4.331635
1.917427	201.341691	4.336640
2.039223	201.559862	4.341645
1.820033	207.336311	4.346650
1.916931	203.167206	4.351654
1.915021	198.761942	4.356659
2.299131	194.261733	4.361664
1.765095	177.155887	4.366669
1.740119	176.115013	4.371674
1.913369	167.921486	4.376678
1.179549	171.178891	4.381683
1.720242	182.740077	4.386688
1.999305	196.388717	4.391693
1.787814	199.113733	4.396698
2.436136	198.505578	4.401702
2.169678	205.713037	4.406707
2.055489	194.046092	4.411712
1.643162	185.865827	4.416717
1.848258	195.141075	4.421722
2.212749	189.100997	4.426726
2.143163	191.844456	4.431731
1.818986	188.882368	4.436736
2.017363	199.085403	4.441741
2.158205	199.797289	4.446746
2.317527	186.226421	4.451750
1.783880	187.353913	4.456755
2.189517	189.478484	4.461760
1.773667	197.801223	4.466765
1.853459	202.641957	4.471770
2.412214	199.599806	4.476774
1.939740	205.663638	4.481779
2.410532	199.673374	4.486784
2.451790	192.391936	4.491789
2.224654	194.575708	4.496794
2.165832	180.371954	4.501798
1.941377	195.082456	4.506803
2.341788	201.935167	4.511808
1.975792	195.337292	4.516813
1.848375	198.608360	4.521818
2.268817	188.828038	4.526822
1.968804	204.765091	4.531827
2.086437	197.252904	4.536832
1.809328	196.990773	4.541837
2.088457	198.098804	4.546842
2.088564	196.379477	4.551846
2.162325	205.572174	4.556851
2.007707	197.735441	4.561856
2.296690	207.521654	4.566861
2.504707	220.666695	4.571866
2.583730	211.678761	4.576870
2.200141	209.403392	4.581875
2.491025	200.996121	4.586880
2.445730	205.219873	4.591885
2.576922	212.576330	4.596890
2.733680	205.763491	4.601894
2.256842	207.272850	4.606899
2.343602	206.341074	4.611904
2.610283	208.125063	4.616909
2.543230	203.841526	4.621914
2.680376	202.496648	4.626918
2.484009	211.655513	4.631923
2.336548	202.227688	4.636928
2.424532	207.735621	4.641933
2.621507	200.283849	4.646938
2.401745	208.202821	4.651942
2.249435	209.630217	4.656947
2.512856	206.145010	4.661952
2.746596	227.852929	4.666957
2.746544	230.522283	4.671962
2.469721	223.124391	4.676966
2.643040	229.503377	4.681971
2.830653	228.579305	4.686976
2.480253	229.295688	4.691981
2.450156	236.653313	4.696986
2.768716	231.297110	4.701990
2.802224	225.548831	4.706995
2.986515	228.064409	4.712000
2.674522	230.886253	4.717005
2.991648	217.812649	4.722010
2.878115	201.323595	4.727014
2.752325	208.827746	4.732019
2.461243	188.579848	4.737024
2.885191	207.625895	4.742029
2.478629	219.103025	4.747034
2.902867	218.567832	4.752038
2.693586	228.471412	4.757043
2.669116	236.234013	4.762048
2.931368	234.521428	4.767053
2.794628	232.138130	4.772058
2.977447	225.398502	4.777062
2.704247	239.948233	4.782067
2.831103	221.972956	4.787072
2.719687	237.049308	4.792077
2.838713	236.361792	4.797082
3.055105	235.223173	4.802086
3.060394	229.161485	4.807091
3.053132	237.332662	4.812096
3.305286	225.079504	4.817101
3.070777	237.473860	4.822106
3.295628	227.346951	4.827110
2.856099	224.326873	4.832115
3.068794	223.047382	4.837120
3.101427	222.773626	4.842125
3.045081	228.426718	4.847130
3.309274	226.326450	4.852134
2.805688	212.846999	4.857139
2.585384	207.548602	4.862144
2.717658	229.857490	4.867149
2.725484	232.075027	4.872154
3.218519	233.860860	4.877158
3.145902	230.988176	4.882163
3.217739	230.654822	4.887168
3.054424	233.759791	4.892173
3.161981	234.816226	4.897178
3.099861	231.671650	4.902182
2.846853	241.468843	4.907187
2.879308	238.592112	4.912192
2.890316	237.585113	4.917197
2.847905	238.395539	4.922202
2.733978	260.467354	4.927206
3.276187	263.677649	4.932211
3.122373	269.934415	4.937216
3.327002	264.925695	4.942221
3.264935	262.337581	4.947226
3.916803	261.470527	4.952230
3.477613	265.270974	4.957235
3.383610	260.025763	4.962240
3.553593	259.655176	4.967245
3.566018	254.267563	4.972250
3.673088	239.473192	4.977254
3.194703	243.959563	4.982259
3.061731	233.313746	4.987264
3.200524	245.107343	4.992269
3.091538	261.287980	4.997274
3.388096	263.109633	5.002278
3.488549	274.291383	5.007283
3.239304	272.005711	5.012288
3.326628	262.882379	5.017293
3.294210	265.778526	5.022298
3.679779	258.754177	5.027302
3.642713	267.417143	5.032307
3.292024	269.525755	5.037312
3.529387	267.560180	5.042317
3.350221	265.651605	5.047322
3.716911	266.813957	5.052326
3.564335	272.150949	5.057331
3.544815	269.544119	5.062336
3.646529	265.096551	5.067341
3.241490	270.114981	5.072346
3.357708	259.005633	5.077350
3.442167	267.304054	5.082355
3.795495	281.693248	5.087360
3.429684	271.939175	5.092365
3.306051	270.112734	5.097370
3.413221	263.142945	5.102374
3.537349	281.203516	5.107379
3.685077	286.797055	5.112384
3.797082	285.901532	5.117389
3.748197	295.563599	5.122394
4.035765	293.779115	5.127398
3.858455	288.418883	5.132403
3.544892	271.601884	5.137408
3.630706	278.167114	5.142413
3.514680	285.552858	5.147418
4.271428	283.698876	5.152422
4.109754	297.078096	5.157427
4.048343	289.030465	5.162432
4.030281	274.641658	5.167437
3.461117	273.743326	5.172442
3.788723	271.912526	5.177446
3.800963	273.186481	5.182451
4.421367	286.176009	5.187456
3.846370	272.418888	5.192461
3.854104	268.077319	5.197466
3.591894	263.101797	5.202470
3.644865	270.615336	5.207475
3.836362	287.736860	5.212480
3.968186	283.292373	5.217485
3.633631	286.477319	5.222490
4.098776	277.245398	5.227494
3.794546	296.056799	5.232499
3.970101	290.754142	5.237504
4.106766	296.521006	5.242509
4.000067	294.879805	5.247514
4.267081	287.231253	5.252518
4.023434	296.240357	5.257523
3.949530	292.445543	5.262528
3.944979	290.766250	5.267533
4.251922	292.807192	5.272538
4.221838	288.658382	5.277542
4.379166	286.406952	5.282547
4.236487	291.104527	5.287552
4.277858	288.758510	5.292557
4.274351	293.472223	5.297562
4.094406	289.232685	5.302566
4.042692	290.419001	5.307571
4.375341	290.519443	5.312576
4.396942	284.628872	5.317581
4.072265	293.582969	5.322586
4.141765	286.261865	5.327590
4.121784	295.200837	5.332595
4.191276	289.805896	5.337600
4.244605	292.950050	5.342605
3.788745	296.802610	5.347610
4.302556	289.128229	5.352614
4.148463	294.849688	5.357619
4.066096	290.797183	5.362624
4.200430	298.820538	5.367629
4.085787	291.028420	5.372634
4.144835	304.329914	5.377638
4.158130	313.576335	5.382643
4.298893	317.601458	5.387648
4.658917	321.208298	5.392653
4.389018	329.795546	5.397658
4.411371	324.041981	5.402662
4.418785	326.564874	5.407667
4.391041	316.956451	5.412672
4.414826	321.793310	5.417677
4.440500	318.982811	5.422682
4.614669	325.353013	5.427686
4.264231	325.164437	5.432691
4.654882	327.670990	5.437696
4.644624	323.152428	5.442701
4.561428	334.711264	5.447706
4.474077	323.854351	5.452710
4.593086	333.083608	5.457715
4.605978	331.453506	5.462720
4.775909	331.164228	5.467725
4.315267	330.137940	5.472730
4.863246	322.061817	5.477734
4.815323	321.970366	5.482739
4.595419	328.504539	5.487744
4.876804	324.924363	5.492749
4.757474	322.320695	5.497754
4.915029	313.983872	5.502758
4.482023	322.768131	5.507763
4.839615	318.576384	5.512768
4.794470	319.062065	5.517773
4.597196	320.977253	5.522778
4.934008	323.067304	5.527782
4.363541	328.604805	5.532787
4.446247	314.674982	5.537792
4.712215	329.350271	5.542797
4.777313	326.784619	5.547802
4.762951	318.913658	5.552806
4.626625	325.472222	5.557811
4.650162	318.561499	5.562816
4.535257	318.824935	5.567821
4.301620	327.023131	5.572826
4.395199	327.247573	5.577830
4.447262	351.770233	5.582835
4.819718	358.236546	5.587840
4.989080	361.043523	5.592845
4.996035	365.857145	5.597850
5.221677	354.217461	5.602854
4.800229	357.611632	5.607859
5.199001	359.939438	5.612864
5.304006	352.740273	5.617869
5.058089	346.684378	5.622874
5.048682	328.752938	5.627878
4.834007	329.916023	5.632883
4.981844	335.027280	5.637888
5.126867	340.255038	5.642893
4.935516	327.773203	5.647898
5.168325	341.005195	5.652902
5.016443	351.033499	5.657907
5.215661	351.355033	5.662912
5.210156	343.781745	5.667917
4.808585	338.435486	5.672922
5.130697	351.632121	5.677926
5.298714	349.457247	5.682931
5.123208	358.271344	5.687936
5.377728	352.327232	5.692941
5.065333	342.351115	5.697946
5.000546	340.054703	5.702950
4.850652	351.855913	5.707955
4.993943	357.793970	5.712960
5.515192	358.316143	5.717965
4.941153	358.097047	5.722970
5.295846	355.428002	5.727974
4.893699	352.867786	5.732979
5.331963	355.337816	5.737984
5.351524	355.089121	5.742989
4.861650	365.171838	5.747994
5.285812	353.276959	5.752998
5.273123	366.160836	5.758003
5.321801	358.166502	5.763008
5.075106	360.306976	5.768013
4.960605	362.190059	5.773018
5.342022	353.805151	5.778022
5.098079	359.752320	5.783027
5.358550	368.401407	5.788032
5.369031	379.359415	5.793037
5.217577	389.375635	5.798042
5.431269	384.037402	5.803046
5.327100	395.151230	5.808051
5.257599	386.279051	5.813056
5.132646	389.641904	5.818061
5.194817	394.702497	5.823066
5.266207	389.942423	5.828070
5.298141	392.960703	5.833075
5.354114	393.056618	5.838080
5.535727	378.895992	5.843085
5.289708	389.263990	5.848090
5.476799	385.308949	5.853094
5.322776	390.923674	5.858099
5.305689	400.579535	5.863104
5.929367	405.108521	5.868109
5.730035	412.055488	5.873114
5.634354	405.203812	5.878118
5.572406	404.349035	5.883123
5.546332	409.437127	5.888128
6.161636	412.937029	5.893133
5.668358	406.158544	5.898138
5.605096	399.000547	5.903142
5.400512	400.186430	5.908147
5.505892	405.181236	5.913152
5.726066	408.846270	5.918157
5.848455	418.060413	5.923162
6.069487	415.959795	5.928166
5.708843	408.577522	5.933171
5.707890	413.569482	5.938176
6.092973	410.799867	5.943181
5.460987	408.087811	5.948186
5.672099	405.702512	5.953190
5.822309	415.514490	5.958195
5.938698	418.824408	5.963200
6.043893	421.867615	5.968205
6.003898	415.824826	5.973210
5.596220	402.818852	5.978214
5.701689	403.213592	5.983219
5.715541	422.144153	5.988224
6.112166	415.286025	5.993229
5.735062	424.229375	5.998234
6.066059	421.733175	6.003238
5.960332	435.526498	6.008243
6.105324	424.531636	6.013248
5.675595	407.289401	6.018253
5.464022	400.559604	6.023258
5.769822	411.674762	6.028262
5.667691	415.871708	6.033267
5.842369	424.343277	6.038272
5.806499	424.175033	6.043277
5.782779	435.267032	6.048282
6.289035	414.483942	6.053286
5.878046	426.910743	6.058291
5.810878	418.970364	6.063296
6.040565	428.002101	6.068301
5.621774	428.006630	6.073306
5.678530	415.110523	6.078310
5.920813	426.751686	6.083315
5.749948	426.298630	6.088320
6.050381	428.317585	6.093325
5.714395	423.136022	6.098330
6.211474	425.508474	6.103334
6.038724	426.316303	6.108339
5.984489	412.179259	6.113344
5.738970	403.602925	6.118349
5.826786	407.774217	6.123354
5.834394	412.874866	6.128358
6.043341	413.452305	6.133363
6.151681	415.239944	6.138368
5.974507	404.564454	6.143373
5.602710	399.406415	6.148378
5.848859	396.576028	6.153382
5.818347	394.669763	6.158387
5.832317	390.452035	6.163392
5.628514	394.600360	6.168397
5.445199	406.950427	6.173402
6.139415	413.077936	6.178406
6.338249	416.853474	6.183411
5.845188	404.961237	6.188416
5.863587	398.816791	6.193421
5.857184	390.372795	6.198426
5.704928	392.669848	6.203430
5.674361	396.909358	6.208435
5.835712	401.008238	6.213440
5.960836	411.821117	6.218445
5.821804	413.862402	6.223450
5.732990	410.644279	6.228454
5.906257	409.129988	6.233459
6.012252	419.894745	6.238464
6.104637	414.270402	6.243469
5.986920	397.417161	6.248474
6.027775	397.128814	6.253478
5.715628	397.940473	6.258483
5.529560	396.594049	6.263488
5.826611	387.467358	6.268493
5.736951	400.843380	6.273498
5.928169	391.272911	6.278502
5.957276	403.361523	6.283507
6.040342	398.458609	6.288512
6.093957	390.960128	6.293517
5.981895	395.526944	6.298522
5.753485	392.933107	6.303526
5.742704	394.949519	6.308531
5.922640	384.925877	6.313536
5.967986	391.871830	6.318541
5.993630	390.383459	6.323546
5.808784	385.590201	6.328550
5.701839	394.528096	6.333555
5.490075	390.002357	6.338560
5.616824	389.420901	6.343565
5.966198	399.597391	6.348570
5.948867	408.029630	6.353574
5.831008	402.557651	6.358579
5.634968	402.921205	6.363584
5.836895	410.305071	6.368589
5.540483	418.860860	6.373594
6.146249	421.817905	6.378598
6.150992	422.007781	6.383603
5.790830	416.448199	6.388608
5.760705	398.004291	6.393613
5.617122	405.665809	6.398618
5.777174	414.922037	6.403622
5.779986	423.142747	6.408627
5.933533	428.217566	6.413632
6.190770	426.134806	6.418637
5.892981	421.462924	6.423642
5.913652	408.687077	6.428646
5.782137	399.658647	6.433651
5.617958	405.984087	6.438656
5.949747	407.073909	6.443661
5.835801	421.833746	6.448666
5.921423	420.076303	6.453670
6.223119	418.267554	6.458675
5.885537	404.976422	6.463680
5.896847	404.787904	6.468685
5.561872	396.798711	6.473690
5.487088	405.821251	6.478694
5.674113	402.922744	6.483699
5.734753	429.765144	6.488704
5.989108	428.539689	6.493709
6.070387	425.066948	6.498714
5.931999	419.753283	6.503718
6.178930	425.628753	6.508723
5.773667	409.281899	6.513728
5.881349	395.475921	6.518733
5.780986	402.418076	6.523738
5.547777	399.118383	6.528742
5.882984	414.171189	6.533747
5.610253	429.598565	6.538752
6.125905	418.186502	6.543757
6.170140	417.562519	6.548762
6.279999	407.795402	6.553766
5.878286	404.254552	6.558771
5.878286	394.404274	6.563776
6.005348	386.009334	6.568781
5.663670	389.771304	6.573786
5.735838	396.913884	6.578790
5.757941	388.028648	6.583795
5.519567	403.402729	6.588800
5.972076	392.268963	6.593805
5.409225	414.336286	6.598810
5.723868	416.519625	6.603814
5.956934	422.345697	6.608819
5.829430	425.424820	6.613824
6.127336	423.935987	6.618829
5.983021	431.110224	6.623834
6.147462	421.913991	6.628838
6.265282	407.423739	6.633843
5.922996	394.558653	6.638848
6.081739	390.803486	6.643853
5.692703	391.028030	6.648858
5.596455	397.796043	6.653862
5.580661	392.732752	6.658867
5.642848	393.621508	6.663872
5.634582	400.760488	6.668877
5.910758	417.838481	6.673882
5.766283	418.875648	6.678886
5.733700	422.660448	6.683891
5.516314	429.843673	6.688896
6.076237	424.731249	6.693901
5.742018	425.168090	6.698906
5.503541	427.298722	6.703910
5.639649	424.339804	6.708915
5.685174	426.227080	6.713920
5.860120	418.341376	6.718925
5.818756	429.688497	6.723930
5.883890	430.578541	6.728934
5.686892	429.840537	6.733939
5.758310	430.143059	6.738944
6.105185	418.266897	6.743949
5.706174	429.455410	6.748954
5.620019	426.992830	6.753958
6.293205	429.252144	6.758963
6.122311	433.628258	6.763968
6.464594	425.200286	6.768973
5.893599	431.848311	6.773978
5.934995	429.465170	6.778982
6.159814	422.264212	6.783987
5.832766	432.253209	6.788992
6.159839	423.259838	6.793997
5.856999	417.308689	6.799002
5.754014	403.657502	6.804006
5.642158	405.679666	6.809011
5.640115	413.279379	6.814016
5.974634	425.547532	6.819021
5.714170	433.235004	6.824026
5.841934	422.818631	6.829030
5.878679	425.249049	6.834035
5.813376	430.753729	6.839040
6.067158	422.738886	6.844045
6.129890	433.331467	6.849050
5.622262	414.477913	6.854054
5.867424	410.590766	6.859059
5.608455	423.671717	6.864064
5.814438	418.847231	6.869069
5.797716	430.185521	6.874074
6.113636	424.053575	6.879078
5.998344	418.838488	6.884083
5.643009	433.083752	6.889088
5.866222	425.764067	6.894093
5.929739	427.828913	6.899098
5.634215	420.044496	6.904102
6.117639	426.833979	6.909107
5.872869	427.333308	6.914112
5.939076	426.917018	6.919117
5.685897	434.732928	6.924122
5.918273	425.971376	6.929126
5.909275	427.201317	6.934131
5.978776	423.708236	6.939136
5.763819	430.401865	6.944141
5.943914	429.071340	6.949146
5.983498	428.474770	6.954150
5.878665	417.622670	6.959155
5.929534	425.132885	6.964160
5.883592	407.045218	6.969165
5.711759	410.291350	6.974170
5.790501	397.263533	6.979174
5.769392	403.762919	6.984179
5.981415	421.692618	6.989184
6.148463	418.116230	6.994189
5.849497	401.828084	6.999194
5.776504	401.436511	7.004198
5.930353	392.017095	7.009203
5.626068	398.782589	7.014208
5.933788	391.994502	7.019213
6.024518	395.578830	7.024218
5.902379	399.781268	7.029222
6.143746	395.582770	7.034227
5.654572	393.754716	7.039232
5.643113	391.374446	7.044237
5.538192	395.013790	7.049242
5.709996	413.262346	7.054246
6.069644	419.678718	7.059251
5.998643	428.393393	7.064256
5.967110	419.419374	7.069261
5.854078	405.677108	7.074266
5.939504	399.111461	7.079270
5.803201	404.356401	7.084275
5.802449	406.174012	7.089280
5.477294	392.238701	7.094285
5.664051	413.674673	7.099290
5.879001	432.592739	7.104294
5.999571	422.868233	7.109299
5.679806	432.670525	7.114304
5.753717	430.153514	7.119309
5.965708	428.668897	7.124314
5.726052	430.352565	7.129318
5.800853	429.995626	7.134323
5.780903	435.058634	7.139328
5.772132	433.072974	7.144333
6.010272	425.148938	7.149338
6.127640	426.977110	7.154342
5.918454	431.944487	7.159347
5.631827	437.159172	7.164352
5.879281	429.161559	7.169357
5.973265	428.454123	7.174362
6.248346	417.520523	7.179366
5.949781	414.342000	7.184371
5.859311	406.613096	7.189376
6.012440	395.731948	7.194381
5.698894	400.896828	7.199386
5.427620	394.655688	7.204390
5.796507	416.104607	7.209395
5.815968	424.941392	7.214400
5.998089	424.689159	7.219405
5.931699	431.202398	7.224410
6.132590	424.522827	7.229414
6.055922	416.619746	7.234419
5.792090	403.887442	7.239424
5.605962	393.380393	7.244429
5.816303	407.796234	7.249434
5.600053	420.275909	7.254438
5.977535	415.941118	7.259443
5.893086	427.484050	7.264448
5.962279	424.458702	7.269453
5.683868	425.521289	7.274458
6.020736	433.590378	7.279462
6.170737	425.215481	7.284467
5.717167	411.873372	7.289472
5.775139	407.343641	7.294477
6.088130	405.968334	7.299482
5.923579	405.839042	7.304486
5.750662	395.414254	7.309491
5.588942	403.119437	7.314496
5.771940	404.409223	7.319501
5.736785	418.470423	7.324506
5.986657	424.037956	7.329510
5.928947	421.227287	7.334515
6.088937	435.045707	7.339520
6.049688	414.473071	7.344525
5.481932	413.345588	7.349530
5.455079	412.595880	7.354534
5.988595	421.015104	7.359539
5.777610	435.088179	7.364544
6.210024	430.154420	7.369549
6.082094	427.817579	7.374554
5.941072	422.346681	7.379558
5.956251	403.534706	7.384563
5.454618	403.993454	7.389568
5.983078	402.844590	7.394573
5.788751	417.522274	7.399578
5.571057	426.448403	7.404582
6.153238	427.492464	7.409587
5.869999	426.616847	7.414592
5.865847	419.865786	7.419597
5.841918	415.323026	7.424602
6.021395	424.819936	7.429606
5.835894	404.429096	7.434611
5.636170	419.945954	7.439616
6.008096	413.819700	7.444621
5.659612	422.788879	7.449626
5.595638	423.089633	7.454630
5.849622	424.340193	7.459635
5.945777	428.000192	7.464640
5.784989	425.677298	7.469645
5.701813	440.396715	7.474650
6.118337	434.333686	7.479654
5.932875	429.517824	7.484659
5.799922	439.257890	7.489664
5.969175	425.321672	7.494669
6.004190	432.924707	7.499674
5.900054	424.207448	7.504678
5.880237	401.630038	7.509683
5.541617	410.011686	7.514688
6.214077	418.155818	7.519693
5.374285	417.963923	7.524698
5.916048	428.561732	7.529702
5.914699	432.559002	7.534707
5.617976	430.738816	7.539712
6.127305	433.692158	7.544717
6.257963	434.525135	7.549722
5.781122	420.071158	7.554726
5.775573	403.631823	7.559731
5.896454	419.598593	7.564736
6.015290	410.906045	7.569741
5.589007	400.246903	7.574746
5.931490	414.803193	7.579750
5.952407	420.795951	7.584755
5.900136	416.126675	7.589760
5.951439	408.622057	7.594765
5.569354	406.290759	7.599770
5.863560	411.043428	7.604774
6.034306	413.669230	7.609779
5.938652	410.923478	7.614784
5.796846	405.044037	7.619789
5.529194	400.653089	7.624794
5.652132	426.901613	7.629798
6.260671	424.060517	7.634803
5.806876	429.243587	7.639808
6.039350	411.721176	7.644813
5.725266	408.449132	7.649818
5.814191	414.129846	7.654822
5.969135	407.836407	7.659827
5.763461	413.544381	7.664832
5.861462	411.215770	7.669837
5.431825	426.696653	7.674842
5.729622	428.880228	7.679846
5.825070	435.524041	7.684851
5.847880	427.483652	7.689856
6.126993	434.367482	7.694861
5.614666	436.353995	7.699866
5.628462	430.165309	7.704870
5.811924	429.475165	7.709875
5.773351	432.126883	7.714880
5.895589	436.464141	7.719885
5.571293	434.308728	7.724890
5.953279	437.187925	7.729894
6.031328	428.719215	7.734899
5.868907	438.124172	7.739904
6.047511	430.438345	7.744909
6.155130	433.636059	7.749914
5.756436	426.479932	7.754918
5.918860	435.333413	7.759923
5.838607	429.670667	7.764928
5.846689	434.692706	7.769933
5.659180	428.511038	7.774938
5.462113	432.982671	7.779942
5.684289	427.551845	7.784947
5.700285	439.087365	7.789952
5.644564	426.563764	7.794957
5.565875	428.741443	7.799962
5.586944	437.694394	7.804966
5.841673	432.711432	7.809971
5.757210	432.470555	7.814976
5.652219	428.877222	7.819981
5.984920	424.437983	7.824986
5.376247	435.535450	7.829990
5.719820	446.207851	7.834995
5.785246	467.711228	7.840000
6.325433	454.539373	7.845005
6.176503	453.712076	7.850010
5.576033	445.041980	7.855014
5.853365	439.311111	7.860019
5.638664	444.021691	7.865024
5.847318	453.654468	7.870029
5.845427	465.172852	7.875034
6.222800	462.598489	7.880038
6.153901	443.881348	7.885043
5.847150	446.726039	7.890048
5.981694	442.947847	7.895053
5.811083	430.942990	7.900058
6.130605	427.010130	7.905062
6.268831	431.691446	7.910067
6.058745	438.022161	7.915072
5.806305	428.128376	7.920077
6.103859	430.681599	7.925082
5.919038	432.230648	7.930086
6.122641	434.523812	7.935091
5.750565	434.573462	7.940096
5.950735	436.004845	7.945101
5.732541	436.437005	7.950106
6.026765	433.506268	7.955110
6.071202	428.428218	7.960115
5.860137	433.372623	7.965120
6.105889	426.039917	7.970125
5.826899	433.426933	7.975142
5.733726	426.028430	7.980160
5.939462	428.117487	7.985178
5.395099	438.296185	7.990195
5.240020	429.227821	7.995213
5.815170	438.354185	8.000230
5.787179	433.389681	8.005248
6.196143	422.233080	8.010266
5.853655	433.307064	8.015283
5.892653	425.494702	8.020301
5.991474	426.962617	8.025318
6.219848	431.347684	8.030336
6.252212	425.948390	8.035354
6.009994	438.800809	8.040371
6.144642	434.674739	8.045389
6.082472	433.444289	8.050406
5.915124	433.099937	8.055424
5.968923	431.501034	8.060442
6.134387	435.417275	8.065459
6.025982	424.366548	8.070477
6.117006	424.282763	8.075494
5.938093	414.410969	8.080512
5.867660	406.607160	8.085530
5.786758	407.028480	8.090547
5.789925	425.182085	8.095565
5.778494	434.587030	8.100582
5.912080	429.205946	8.105600
6.028822	431.842618	8.110618
5.694377	439.005814	8.115635
5.730701	435.562556	8.120653
6.056209	439.793304	8.125670
6.205602	441.966525	8.130688
6.071088	438.014116	8.135706
6.200658	439.354887	8.140723
6.439870	433.364177	8.145741
6.463150	427.727440	8.150758
5.843209	435.628965	8.155776
6.202639	429.831639	8.160794
5.869182	429.451714	8.165811
6.237025	426.501922	8.170829
6.036900	435.403836	8.175846
5.934670	435.680094	8.180864
6.095587	435.348692	8.185882
5.798292	437.140101	8.190899
5.825716	428.724405	8.195917
5.810065	427.020326	8.200934
5.691869	431.122874	8.205952
6.514109	431.512373	8.210970
6.034390	427.756112	8.215987
6.019581	428.594750	8.221005
6.158868	429.531976	8.226022
5.969330	429.712717	8.231040
6.002202	428.316486	8.236058
5.781572	438.056176	8.241075
5.720897	435.834434	8.246093
5.966283	433.217365	8.251110
5.955175	443.723729	8.256128
5.865073	447.583250	8.261146
5.998169	462.355395	8.266163
6.254068	464.176498	8.271181
5.953234	464.965052	8.276198
6.183839	466.287653	8.281216
6.624164	468.078103	8.286234
6.126214	460.438823	8.291251
6.336409	462.773183	8.296269
6.020798	461.765745	8.301286
6.120267	465.115854	8.306304
6.411110	453.453127	8.311322
6.227308	466.899935	8.316339
6.431533	468.732778	8.321357
6.416584	443.689314	8.326374
6.251997	440.114702	8.331392
6.279847	425.961510	8.336410
6.147843	433.481567	8.341427
6.264721	435.276567	8.346445
6.151039	431.902137	8.351462
6.070459	439.472895	8.356480
6.351052	439.202892	8.361498
6.436287	457.119294	8.366515
6.165054	443.606292	8.371533
6.296454	435.809862	8.376550
5.933937	441.590066	8.381568
6.220876	448.569872	8.386586
6.369920	450.635879	8.391603
6.180055	457.993535	8.396621
6.499579	468.747291	8.401638
6.569432	463.509847	8.406656
6.626286	461.100669	8.411674
6.355626	444.491612	8.416691
6.219141	434.933784	8.421709
6.277488	426.762728	8.426726
5.839351	440.195493	8.431744
6.556051	452.203958	8.436762
6.284715	458.257568	8.441779
6.476821	464.451844	8.446797
6.671345	465.071259	8.451814
6.088315	454.277335	8.456832
6.179731	449.463829	8.461850
6.351256	460.109122	8.466867
6.358285	472.730395	8.471885
6.756138	466.636146	8.476902
6.217118	467.124166	8.481920
6.578015	461.016772	8.486938
6.324921	451.841863	8.491955
6.214253	464.267162	8.496973
6.328751	465.531117	8.501990
6.202114	468.420432	8.507008
6.323228	465.388033	8.512026
6.571461	465.779447	8.517043
6.416729	471.775889	8.522061
6.904791	463.930200	8.527078
6.644272	467.914500	8.532096
6.645633	447.117516	8.537114
6.354017	439.030014	8.542131
6.420477	432.886344	8.547149
6.670030	425.867248	8.552166
6.290096	434.487269	8.557184
6.481262	436.693698	8.562202
6.343101	441.132212	8.567219
6.354944	464.280191	8.572237
6.891957	454.821013	8.577255
6.480145	446.504495	8.582272
6.502740	436.494675	8.587290
6.353781	436.608244	8.592307
6.316378	457.679171	8.597325
6.693710	465.493681	8.602343
6.546632	458.937702	8.607360
6.500138	465.460192	8.612378
6.811208	460.066328	8.617395
6.264867	451.598759	8.622413
6.283066	455.569402	8.627431
6.356956	460.761772	8.632448
6.580198	460.830600	8.637466
6.456390	464.206798	8.642483
6.419061	467.980788	8.647501
6.483568	458.113777	8.652519
6.282227	472.039836	8.657536
6.535518	469.221270	8.662554
6.360224	470.412736	8.667571
6.424723	465.649364	8.672589
6.654822	469.012206	8.677607
6.412943	467.031385	8.682624
6.285127	469.160143	8.687642
6.581483	460.283234	8.692659
6.383355	473.159847	8.697677
6.786527	471.735523	8.702695
6.249356	492.653368	8.707712
6.571444	490.610887	8.712730
6.580144	489.243862	8.717747
6.503450	493.154704	8.722765
6.992896	487.030657	8.727783
6.750965	498.809952	8.732800
6.864995	496.010986	8.737818
6.862877	493.531692	8.742835
6.699059	497.065714	8.747853
6.803205	472.009101	8.752871
6.569212	467.308334	8.757888
6.383772	471.461240	8.762906
6.808021	483.609078	8.767923
6.741165	492.979378	8.772941
6.916528	494.627866	8.777959
6.857897	499.809799	8.782976
6.691253	483.121409	8.787994
6.415228	464.140025	8.793011
6.797981	490.471156	8.798029
6.757328	487.825842	8.803047
6.959946	502.915180	8.808064
6.891321	497.779868	8.813082
6.819123	493.287216	8.818099
6.464554	493.387919	8.823117
6.769190	492.012645	8.828135
7.189405	501.045520	8.833152
7.026488	490.484665	8.838170
7.015664	474.783674	8.843187
6.861271	479.629780	8.848205
6.840162	469.329200	8.853223
6.903550	468.158579	8.858240
6.941022	470.295884	8.863258
7.063798	461.245484	8.868275
6.553237	465.392788	8.873293
6.820935	462.386217	8.878311
6.912947	463.351576	8.883328
6.769158	460.405528	8.888346
6.492845	459.044151	8.893363
6.590041	475.703393	8.898381
6.923961	486.285888	8.903399
7.079121	489.268315	8.908416
6.813631	487.419356	8.913434
7.101169	471.536111	8.918451
6.677124	472.206576	8.923469
6.924552	477.000851	8.928487
6.921954	478.431303	8.933504
6.776260	486.326263	8.938522
6.846362	494.076510	8.943539
6.825874	512.431572	8.948557
7.232983	497.088019	8.953575
7.324039	498.866061	8.958592
6.545352	476.794890	8.963610
6.945654	482.901030	8.968627
7.198527	486.764176	8.973645
7.201668	479.818491	8.978663
7.032734	474.873662	8.983680
6.787796	468.934675	8.988698
6.849020	466.269282	8.993715
6.966793	478.163953	8.998733
7.252242	474.039969	9.003751
6.837944	470.124413	9.008768
6.586375	477.414782	9.013786
7.281057	483.327911	9.018803
6.886037	502.392986	9.023821
6.743739	501.005394	9.028839
7.306723	498.977787	9.033856
7.267632	500.011589	9.038874
7.266077	496.679918	9.043891
7.201969	484.701793	9.048909
6.839973	480.143349	9.053927
7.212825	490.291267	9.058944
7.061467	476.537269	9.063962
7.289551	475.953190	9.068979
6.772714	473.378367	9.073997
6.924994	480.725223	9.079015
6.830042	490.978060	9.084032
6.515353	503.846713	9.089050
7.107844	502.616094	9.094067
6.843062	502.558185	9.099085
7.155824	495.553943	9.104103
7.131462	502.275704	9.109120
6.879348	500.526085	9.114138
7.174104	494.073407	9.119155
7.029295	501.264554	9.124173
6.973130	496.026787	9.129191
7.252204	498.060952	9.134208
7.265587	504.236924	9.139226
6.859720	500.276261	9.144243
6.805681	505.500342	9.149261
6.766694	503.831823	9.154279
7.113676	515.625438	9.159296
7.040181	531.553930	9.164314
7.326694	523.908232	9.169331
7.333083	534.953431	9.174349
7.482933	527.207229	9.179367
7.417782	520.627765	9.184384
7.191674	516.070541	9.189402
7.140317	497.501730	9.194419
6.805224	507.551800	9.199437
7.275532	515.469767	9.204455
7.190617	522.925353	9.209472
7.484806	527.833907	9.214490
7.681943	534.044696	9.219507
7.132141	525.087746	9.224525
7.419419	520.102700	9.229543
7.198726	510.522210	9.234560
7.406469	523.255818	9.239578
7.410286	503.829483	9.244595
7.075005	500.799715	9.249613
7.276227	513.548571	9.254631
7.314321	519.198050	9.259648
7.372303	523.990170	9.264666
7.424082	521.315906	9.269683
7.449107	520.354394	9.274701
7.077971	508.321781	9.279719
7.727372	521.746276	9.284736
7.148176	514.683215	9.289754
7.513222	505.156144	9.294771
7.553361	509.616218	9.299789
7.180160	502.622654	9.304807
7.710815	507.892450	9.309824
7.328734	501.941406	9.314842
7.257684	499.843808	9.319859
7.095078	502.495628	9.324877
7.181306	512.543774	9.329895
7.457152	511.513214	9.334912
7.368807	527.984671	9.339930
7.731936	526.771901	9.344947
7.510837	529.898955	9.349965
7.286773	530.836548	9.354983
7.809423	531.368948	9.360000
7.370512	527.512384	9.365018
7.765846	514.418005	9.370035
7.412491	501.220346	9.375053
7.415809	501.326123	9.380071
7.482732	497.663612	9.385088
7.297710	509.774172	9.390106
7.545030	522.052227	9.395123
7.307492	523.037724	9.400141
7.491029	525.033053	9.405159
7.571833	529.615692	9.410176
7.412227	540.768793	9.415194
7.452320	524.294398	9.420211
7.536761	530.368224	9.425229
7.499079	534.994966	9.430247
7.715006	527.373989	9.435264
7.682412	535.748161	9.440282
7.563274	526.318089	9.445299
7.367764	536.500081	9.450317
7.476489	538.238186	9.455335
8.137887	523.941020	9.460352
7.444907	527.298462	9.465370
7.596869	534.172998	9.470387
7.391908	534.170495	9.475405
7.804857	542.121630	9.480423
7.949186	535.740390	9.485440
7.269486	522.478464	9.490458
7.532366	529.319799	9.495475
7.660362	528.909426	9.500493
7.755485	537.255087	9.505511
7.548149	527.803458	9.510528
7.480176	542.364831	9.515546
7.482586	537.163177	9.520563
7.676054	530.156505	9.525581
7.342186	534.212653	9.530599
7.755844	528.996774	9.535616
7.379619	531.358151	9.540634
7.428336	532.686190	9.545651
7.657333	528.492055	9.550669
7.486497	535.975313	9.555687
7.410892	527.414499	9.560704
7.619492	534.076884	9.565722
7.642714	533.938430	9.570739
7.715706	536.354656	9.575757
7.806681	548.758317	9.580775
7.737013	540.431527	9.585792
7.256576	546.985042	9.590810
7.902793	549.322722	9.595827
7.875698	558.593154	9.600845
7.674122	562.052766	9.605863
7.872319	559.019346	9.610880
7.892492	556.180660	9.615898
8.138534	563.077560	9.620915
7.937462	548.271031	9.625933
7.742175	548.884973	9.630951
7.670376	535.194464	9.635968
7.782921	550.556472	9.640986
7.882623	563.102578	9.646003
8.155380	555.934699	9.651021
8.035480	552.750628	9.656039
8.031007	529.336828	9.661056
7.527066	532.676826	9.666074
7.842541	532.067393	9.671091
7.626699	531.366369	9.676109
7.604173	543.897739	9.681127
8.043836	551.151589	9.686144
8.131482	553.324263	9.691162
7.857227	561.570324	9.696179
8.068959	555.851040	9.701197
8.045591	556.291932	9.706215
7.871977	540.616358	9.711232
7.822460	541.216305	9.716250
7.847959	557.676155	9.721267
8.081362	556.672919	9.726285
7.774895	556.761493	9.731303
8.035179	567.219288	9.736320
8.063479	557.794215	9.741338
8.016342	559.561773	9.746355
8.036986	554.737165	9.751373
7.922342	561.410774	9.756391
8.063845	555.492159	9.761408
7.907211	562.141648	9.766426
8.039829	556.955939	9.771443
7.835642	561.825306	9.776461
7.867748	565.409842	9.781479
7.801108	557.904709	9.786496
7.749457	561.738184	9.791514
7.760346	561.192171	9.796531
7.796213	553.986706	9.801549
7.349287	563.545210	9.806567
7.878586	561.005328	9.811584
7.890202	567.312906	9.816602
7.954101	583.189877	9.821619
7.883475	587.770540	9.826637
8.161378	589.671459	9.831655
7.894516	593.079730	9.836672
8.067417	600.688152	9.841690
7.958685	591.085067	9.846707
8.180858	591.504437	9.851725
8.128074	592.281685	9.856743
7.958057	591.203783	9.861760
8.019223	591.808562	9.866778
8.181590	591.510377	9.871795
8.289404	587.310584	9.876813
8.203939	595.598899	9.881831
8.293190	588.337894	9.886848
8.331156	587.817102	9.891866
8.187440	599.078618	9.896883
8.414329	592.671232	9.901901
8.215053	591.372425	9.906919
8.235379	594.029480	9.911936
8.451681	600.798479	9.916954
8.404983	594.582419	9.921971
8.502370	590.906753	9.926989
8.447741	587.477595	9.932007
8.418101	587.238094	9.937024
8.023578	583.270604	9.942042
7.894559	591.994858	9.947059
8.098439	591.171119	9.952077
8.186738	592.353816	9.957095
8.329558	592.078171	9.962112
8.117913	597.745174	9.967130
8.232098	595.667755	9.972147
8.423671	589.942361	9.977165
7.979868	595.722355	9.982183
8.407681	590.701920	9.987200
8.445396	594.060944	9.992218
7.914154	595.804453	9.997235
8.170099	592.788591	10.002253
8.078150	595.943597	10.007271
8.539348	588.710918	10.012288
8.453079	588.986691	10.017306
8.166670	594.644272	10.022323
7.983635	591.332708	10.027341
8.048335	598.676264	10.032359
8.446718	613.425520	10.037376
8.710468	622.451799	10.042394
8.426871	624.483647	10.047411
8.759309	616.950338	10.052429
8.360087	603.870835	10.057447
8.220998	597.938415	10.062464
8.359490	599.763894	10.067482
8.593801	619.343548	10.072499
8.553550	612.587677	10.077517
8.059937	622.235467	10.082535
8.601943	613.811297	10.087552
8.693176	625.507165	10.092570
8.251949	634.701017	10.097587
8.796778	631.548556	10.102605
8.619981	621.011965	10.107623
8.512393	622.721472	10.112640
8.224451	615.744391	10.117658
8.397730	625.964347	10.122675
8.458257	623.400413	10.127693
8.737214	623.706614	10.132711
8.485096	629.914956	10.137728
8.645246	633.293988	10.142746
8.626149	624.399937	10.147763
8.818465	619.141101	10.152781
8.881840	629.130726	10.157799
8.835874	606.211067	10.162816
8.392326	592.509272	10.167834
8.310533	603.506388	10.172851
8.867031	607.495657	10.177869
8.611220	609.114850	10.182887
8.815427	613.844508	10.187904
8.812635	607.294992	10.192922
8.314875	601.266689	10.197939
8.900869	607.344376	10.202957
8.653143	601.806553	10.207975
8.411572	600.627168	10.212992
8.608869	617.416171	10.218010
8.684250	616.214807	10.223027
9.166366	618.023524	10.228045
8.790201	615.196772	10.233063
8.818016	593.459646	10.238080
8.809557	580.857487	10.243098
8.658902	593.403896	10.248115
8.444086	585.736781	10.253133
8.969909	595.151727	10.258151
8.892601	589.488741	10.263168
8.730547	590.345761	10.268186
8.563747	589.166742	10.273203
8.274720	591.790184	10.278221
8.458003	611.354493	10.283239
8.274495	611.305514	10.288256
8.506748	618.091552	10.293274
8.577635	624.653648	10.298291
8.848634	620.469238	10.303309
8.817542	616.065379	10.308327
8.673724	619.524458	10.313344
8.829189	620.137775	10.318362
8.839538	623.910767	10.323379
8.931242	613.888558	10.328397
8.774925	626.420976	10.333415
8.593507	616.521912	10.338432
8.863688	614.530952	10.343450
8.795008	623.799675	10.348467
8.800392	633.820396	10.353485
9.102950	639.102170	10.358503
9.112147	640.482255	10.363520
9.017669	622.010415	10.368538
8.706071	622.551968	10.373555
8.597113	625.701343	10.378573
8.926429	641.355729	10.383591
8.626601	659.069462	10.388608
8.763603	652.016024	10.393626
8.924827	656.632967	10.398643
9.196584	651.300488	10.403661
9.154351	646.274116	10.408679
9.445965	662.092257	10.413696
9.443181	645.983294	10.418714
8.970005	644.710916	10.423731
9.041191	630.134622	10.428749
8.871783	621.132694	10.433767
8.844607	626.388174	10.438784
9.256129	641.916899	10.443802
9.162774	645.610882	10.448819
9.196728	627.301137	10.453837
9.106045	629.492637	10.458855
8.943064	622.525094	10.463872
8.886394	626.325958	10.468890
8.795581	654.172572	10.473907
9.059736	655.585669	10.478925
8.935265	657.099184	10.483943
8.778816	654.874434	10.488960
9.097374	642.594806	10.493978
9.173649	666.769887	10.498995
9.158170	661.304060	10.504013
9.230388	668.713914	10.509031
8.861519	663.743404	10.514048
9.246152	664.003893	10.519066
9.340607	668.590603	10.524083
9.575295	657.687585	10.529101
9.401853	657.978242	10.534119
9.516749	660.870750	10.539136
9.593485	647.114315	10.544154
9.375469	643.021022	10.549171
9.136545	623.826599	10.554189
9.382582	618.004748	10.559207
8.942295	621.316665	10.564224
9.173760	626.752167	10.569242
9.270265	648.917732	10.574259
9.077482	649.871784	10.579277
9.137508	651.568788	10.584295
9.121398	653.424498	10.589312
9.613536	656.599155	10.594330
9.372511	649.498521	10.599347
9.383470	652.027627	10.604365
9.415195	654.280470	10.609383
9.138703	652.865173	10.614400
9.537588	654.764690	10.619418
9.347381	661.999675	10.624435
9.563507	664.263401	10.629453
9.395854	658.965179	10.634471
9.160422	655.165305	10.639488
9.383281	651.364447	10.644506
9.094253	656.532370	10.649523
9.013204	659.718842	10.654541
9.380153	661.634494	10.659559
9.184170	665.210118	10.664576
9.260997	648.134457	10.669594
8.981549	653.425973	10.674611
9.008786	658.340952	10.679629
9.164513	646.466110	10.684647
9.378862	667.334467	10.689664
9.790303	669.621827	10.694682
9.564358	666.403198	10.699699
9.575622	664.334806	10.704717
9.538482	654.773713	10.709735
9.382304	662.321126	10.714752
9.446935	657.995234	10.719770
9.538129	657.975195	10.724787
9.366593	658.878475	10.729805
9.839812	665.260339	10.734823
9.729279	669.522884	10.739840
9.861117	662.019747	10.744858
9.445300	659.441880	10.749875
9.257918	658.896342	10.754893
9.430531	660.579554	10.759911
9.565484	658.539616	10.764928
9.500328	654.831507	10.769946
9.476467	660.792688	10.774963
9.366742	675.286526	10.779981
9.568691	679.301481	10.784999
9.655375	677.840185	10.790016
9.709442	681.883855	10.795034
9.435354	683.507864	10.800051
9.367644	681.123884	10.805069
9.492951	682.880114	10.810087
9.614063	687.174233	10.815104
9.797746	680.994053	10.820122
9.307455	690.695265	10.825139
8.800758	678.157536	10.830157
9.472131	687.577478	10.835175
9.553088	701.158616	10.840192
9.672729	708.953883	10.845210
9.877572	710.494156	10.850227
9.745552	721.535330	10.855245
9.981403	711.416664	10.860263
9.996185	714.836214	10.865280
9.935411	694.304521	10.870298
9.775957	684.221463	10.875315
9.654333	683.011308	10.880333
9.567956	677.085842	10.885351
9.613852	702.102376	10.890368
9.800944	713.352686	10.895386
10.258043	715.201200	10.900403
9.630464	701.239173	10.905421
9.715877	703.295910	10.910439
9.829704	709.398383	10.915456
10.164780	711.238637	10.920474
10.191133	707.945979	10.925491
9.796656	695.946821	10.930509
9.924521	689.372602	10.935527
9.799809	694.431342	10.940544
9.978491	707.286262	10.945562
9.837168	702.827085	10.950579
9.544087	710.953136	10.955597
9.902593	714.206311	10.960615
9.936684	719.556552	10.965632
9.929346	710.030429	10.970650
10.288814	717.237653	10.975667
9.868903	717.996409	10.980685
10.253504	701.124827	10.985703
10.080665	714.821385	10.990720
9.999349	714.594015	10.995738
10.369791	718.857526	11.000755
9.806098	701.340284	11.005773
10.078292	696.938743	11.010791
9.967869	694.986825	11.015808
10.412296	700.762122	11.020826
10.032955	686.512411	11.025843
10.108342	686.257617	11.030861
10.021988	680.615390	11.035879
9.751588	686.197712	11.040896
10.392172	699.631898	11.045914
10.134744	690.651055	11.050931
9.995437	680.272745	11.055949
10.045364	683.587439	11.060967
10.004991	708.521284	11.065984
10.402709	702.326187	11.071002
10.343988	700.959327	11.076019
10.015713	690.486839	11.081037
9.926546	684.651787	11.086055
10.005028	705.483532	11.091072
10.123628	704.673765	11.096090
10.280542	712.641563	11.101107
10.185850	713.904288	11.106125
10.371203	703.924128	11.111143
10.095393	713.883382	11.116160
10.548292	712.550370	11.121178
10.397210	711.738187	11.126195
9.842283	708.625212	11.131213
10.206882	705.511747	11.136231
10.115659	713.610940	11.141248
10.157257	709.497704	11.146266
10.242665	708.061025	11.151283
10.246367	726.360158	11.156301
10.398338	715.086430	11.161319
10.384608	718.108587	11.166336
10.410803	712.829304	11.171354
10.672141	719.785538	11.176371
10.125345	710.397503	11.181389
10.201830	707.524234	11.186407
10.232139	715.422928	11.191424
10.483117	708.481021	11.196442
10.708308	709.105387	11.201459
10.331169	721.432479	11.206477
10.380198	708.923408	11.211495
10.429839	717.128313	11.216512
10.156133	715.943236	11.221530
10.432891	707.175145	11.226547
9.991228	708.430586	11.231565
10.724153	707.975562	11.236583
10.453744	710.386891	11.241600
10.308656	714.496936	11.246618
10.291084	705.837802	11.251635
10.172631	718.280345	11.256653
10.439552	698.000847	11.261671
10.106327	711.258153	11.266688
10.108674	718.881598	11.271706
10.589931	724.543704	11.276723
10.284080	744.377657	11.281741
10.603915	738.442321	11.286759
10.777729	751.992324	11.291776
10.752264	746.381288	11.296794
10.774159	734.568384	11.301811
10.825177	741.322794	11.306829
10.826689	725.070723	11.311847
10.585846	720.236775	11.316864
10.421230	724.018600	11.321882
10.383011	718.638810	11.326899
10.474670	743.692092	11.331917
11.022453	752.940310	11.336935
10.744891	743.913770	11.341952
10.488072	734.326943	11.346970
10.541679	743.523250	11.351987
10.508285	749.289017	11.357005
10.517373	749.880413	11.362023
10.419061	750.900848	11.367040
10.736366	751.662847	11.372058
10.964557	743.605114	11.377075
10.534285	747.330518	11.382093
10.610423	754.529739	11.387111
10.404495	745.485584	11.392128
10.644747	750.021315	11.397146
10.785249	739.576773	11.402163
10.643830	748.627758	11.407181
10.418961	745.050300	11.412199
10.663448	745.715946	11.417216
10.759834	747.376998	11.422234
10.587727	740.869938	11.427251
10.700168	767.213009	11.432269
11.059125	771.696735	11.437287
10.867686	760.746963	11.442304
10.725772	757.499585	11.447322
10.938639	770.434105	11.452339
10.843987	779.591498	11.457357
11.160274	779.350988	11.462375
10.923972	762.226665	11.467392
10.567865	753.825333	11.472410
11.033433	755.256138	11.477427
11.351153	778.623212	11.482445
10.744631	755.980151	11.487463
10.787255	758.268202	11.492480
10.582857	772.363726	11.497498
10.904867	774.908469	11.502515
10.735871	780.235011	11.507533
10.884505	778.473076	11.512551
11.079141	771.930634	11.517568
10.871051	783.981861	11.522586
10.765574	778.354193	11.527603
10.734664	790.540530	11.532621
11.077742	788.532118	11.537639
11.420195	783.335863	11.542656
10.856805	777.445948	11.547674
11.126684	781.327798	11.552691
10.741632	780.502930	11.557709
10.794008	779.152634	11.562727
11.148050	771.989253	11.567744
10.851971	790.699482	11.572762
11.068790	779.506655	11.577779
10.958503	792.305156	11.582797
11.136938	806.172721	11.587815
11.369022	805.901328	11.592832
11.108902	799.404739	11.597850
11.448993	794.923780	11.602867
11.191114	795.533963	11.607885
11.086088	775.538611	11.612903
11.072242	790.191803	11.617920
11.131475	796.274844	11.622938
11.607803	805.592250	11.627955
11.623949	801.853467	11.632973
11.377372	792.021613	11.637991
11.110477	773.833546	11.643008
11.208157	780.853424	11.648026
11.055492	776.393552	11.653043
11.182889	800.126126	11.658061
11.405702	802.445646	11.663079
11.396480	811.047954	11.668096
11.064939	807.749020	11.673114
11.234962	808.584120	11.678131
11.414590	806.006265	11.683149
11.771301	818.032729	11.688167
11.674652	797.437379	11.693184
11.275878	797.033263	11.698202
11.524754	780.867568	11.703219
11.189824	790.975859	11.708237
11.433797	787.649179	11.713255
11.599420	795.471292	11.718272
11.323395	787.932942	11.723290
11.509743	779.309355	11.728307
11.522581	789.494280	11.733325
11.482584	787.444431	11.738343
11.520646	773.412050	11.743360
11.092031	782.580863	11.748378
11.710336	796.999865	11.753395
11.489039	808.694082	11.758413
11.337798	801.756985	11.763431
11.665357	803.852615	11.768448
11.395706	814.661042	11.773466
11.341501	813.770946	11.778483
11.523319	805.327808	11.783501
11.342525	818.665177	11.788519
11.773597	812.538305	11.793536
11.457359	819.147903	11.798554
11.835325	809.470871	11.803571
11.782535	809.619045	11.808589
11.859420	809.958641	11.813607
11.882441	806.624787	11.818624
11.679841	816.720351	11.823642
11.698831	812.492942	11.828659
11.754993	803.814804	11.833677
11.701636	801.958104	11.838695
11.617422	790.526547	11.843712
11.669356	800.985669	11.848730
11.904657	797.114405	11.853747
11.240415	804.322547	11.858765
11.654372	808.853043	11.863783
11.791862	809.018799	11.868800
11.579446	806.302381	11.873818
11.853871	808.708002	11.878835
12.186037	805.734348	11.883853
11.994308	810.814895	11.888871
12.190174	798.591361	11.893888
11.968821	793.821862	11.898906
11.734419	774.452497	11.903923
11.645108	772.016192	11.908941
11.983470	771.110449	11.913959
12.080580	770.721738	11.918976
11.591209	779.654408	11.923994
11.768089	773.602871	11.929011
11.826926	781.239199	11.934029
11.852301	794.705258	11.939047
12.241586	799.384527	11.944064
11.678437	797.581265	11.949082
12.001572	798.743251	11.954099
12.175365	802.460185	11.959117
11.716525	788.047426	11.964135
12.101437	796.169876	11.969152
12.224037	797.575808	11.974170
11.965101	780.691823	11.979187
11.868815	781.185389	11.984205
11.597081	791.331796	11.989223
11.723798	797.637067	11.994240
11.821761	798.818765	11.999258
11.931863	810.251222	12.004275
11.788998	798.578245	12.009293
11.689416	813.932470	12.014311
11.878497	805.306249	12.019328
12.034852	806.166257	12.024346
11.781336	805.256734	12.029363
12.164044	806.535778	12.034381
11.717612	808.009326	12.039399
12.299464	821.655138	12.044416
12.386571	827.829417	12.049434
12.195450	826.260553	12.054451
12.030453	812.478014	12.059469
12.088250	825.829074	12.064487
12.314315	833.406138	12.069504
12.075105	835.323753	12.074522
12.141859	841.149675	12.079539
12.116996	844.172919	12.084557
12.209441	846.078714	12.089575
12.697751	833.746116	12.094592
12.240188	839.035018	12.099610
12.338095	836.802607	12.104627
12.325257	819.378104	12.109645
12.148817	816.887184	12.114663
12.333394	827.178815	12.119680
12.251530	832.236187	12.124698
12.496245	846.244728	12.129715
12.765973	834.129747	12.134733
12.185537	821.281740	12.139751
12.265048	807.460139	12.144768
12.304441	811.780080	12.149786
12.436585	825.456552	12.154803
12.567805	817.939861	12.159821
12.190203	819.823395	12.164839
12.471343	818.422080	12.169856
12.327497	831.466725	12.174874
12.440056	839.494320	12.179891
12.716456	841.138453	12.184909
12.403272	823.069037	12.189927
12.596819	835.363562	12.194944
12.322018	832.332533	12.199962
12.183873	838.649368	12.204979
12.309166	844.248056	12.209997
12.247477	846.741241	12.215015
12.351693	833.358982	12.220032
12.659847	841.308402	12.225050
12.467956	841.541699	12.230067
12.552189	835.523646	12.235085
12.189812	849.664002	12.240103
12.466412	830.319072	12.245120
12.157083	835.050893	12.250138
12.430172	845.528400	12.255155
12.598971	843.129294	12.260173
12.872229	852.080904	12.265191
12.668691	839.727873	12.270208
12.452199	845.413487	12.275226
12.545771	845.292863	12.280243
12.845483	859.670398	12.285261
12.522068	863.783944	12.290279
12.632441	863.986291	12.295296
13.065662	862.246528	12.300314
12.775288	873.897948	12.305331
12.781922	868.979712	12.310349
12.575455	871.566645	12.315367
12.884326	858.701293	12.320384
12.922751	875.626031	12.325402
12.511292	873.433399	12.330419
12.977454	866.017104	12.335437
13.028402	871.923808	12.340455
13.013417	870.483527	12.345472
12.803228	858.343382	12.350490
12.918746	861.887353	12.355507
13.055206	850.886558	12.360525
12.784610	852.621807	12.365543
13.043324	847.648884	12.370560
13.291608	853.068286	12.375578
12.708770	851.813724	12.380595
12.831659	833.370064	12.385613
12.876123	842.416976	12.390631
12.911735	830.189938	12.395648
12.658011	851.868574	12.400666
12.625744	858.790805	12.405683
13.075078	869.872257	12.410701
12.768054	871.745640	12.415719
13.294057	868.815341	12.420736
13.215120	867.208930	12.425754
12.638119	870.794983	12.430771
13.088282	865.343020	12.435789
13.012722	875.804291	12.440807
12.934364	872.365038	12.445824
12.784692	867.823151	12.450842
13.030596	881.304202	12.455859
12.950170	872.406620	12.460877
13.247821	866.357610	12.465895
13.049658	874.183343	12.470912
12.903961	873.482848	12.475930
12.972809	875.500828	12.480947
12.794338	876.085414	12.485965
12.817756	880.742455	12.490983
13.528919	890.046862	12.496000
13.324369	890.047044	12.501018
13.153104	887.032454	12.506035
13.071679	890.468822	12.511053
13.135710	897.556744	12.516071
13.373482	907.765379	12.521088
13.264022	902.442442	12.526106
13.049892	903.909667	12.531123
13.459219	904.641223	12.536141
13.585445	911.693028	12.541159
13.489740	903.031614	12.546176
12.943540	898.772738	12.551194
13.133069	914.292379	12.556211
13.623322	905.065293	12.561229
13.444288	902.047268	12.566247
13.255549	903.551412	12.571264
13.532084	904.038128	12.576282
13.091671	906.569864	12.581299
13.145406	901.252673	12.586317
12.964849	900.542617	12.591335
13.289837	905.265083	12.596352
13.230083	902.598072	12.601370
13.057703	906.683770	12.606387
13.018928	904.690391	12.611405
13.172019	921.318973	12.616423
13.374390	932.021074	12.621440
13.687324	924.138914	12.626458
13.368965	936.502465	12.631475
13.516703	940.238723	12.636493
13.823241	931.545865	12.641511
13.955257	933.008508	12.646528
13.909627	932.490576	12.651546
13.723942	940.185538	12.656563
13.788361	926.954489	12.661581
13.575550	915.285177	12.666599
13.533130	911.812975	12.671616
14.007136	910.974831	12.676634
13.788286	911.635613	12.681651
13.834896	898.974832	12.686669
13.368553	903.242255	12.691687
13.555656	899.206745	12.696704
13.695150	906.522072	12.701722
13.482581	923.446261	12.706739
13.714285	918.982298	12.711757
13.820012	929.405796	12.716775
13.885858	930.244441	12.721792
13.921668	932.355710	12.726810
13.646596	940.232840	12.731827
14.001199	933.820423	12.736845
13.719247	929.527852	12.741863
13.820144	928.812546	12.746880
13.682357	923.127405	12.751898
13.453672	934.554852	12.756915
13.694270	929.662271	12.761933
13.720056	925.003217	12.766951
13.868227	929.674968	12.771968
13.676318	928.979395	12.776986
13.779999	932.319851	12.782003
13.844176	929.003538	12.787021
13.681051	939.113486	12.792039
13.559094	932.357474	12.797056
13.803760	947.398330	12.802074
13.875614	958.226664	12.807091
14.014700	959.478699	12.812109
14.245768	959.480880	12.817127
14.284272	958.782439	12.822144
14.696824	946.676109	12.827162
14.181095	935.704725	12.832179
14.287941	925.339467	12.837197
14.111861	921.664298	12.842215
13.986805	928.194923	12.847232
14.076852	929.279528	12.852250
14.169360	921.544236	12.857267
14.164945	927.956784	12.862285
14.264582	923.103578	12.867303
13.822143	925.520701	12.872320
14.030276	917.309530	12.877338
13.884305	930.707935	12.882355
14.378136	929.110836	12.887373
14.132595	932.978007	12.892391
14.152854	937.330296	12.897408
14.509600	943.583417	12.902426
14.079998	941.188293	12.907443
14.501910	939.403160	12.912461
14.696649	925.074539	12.917479
14.422500	925.822855	12.922496
14.669199	918.373332	12.927514
14.460093	924.638024	12.932531
14.385920	917.083972	12.937549
14.361921	915.297964	12.942567
14.319367	918.711932	12.947584
14.224818	921.664891	12.952602
14.095680	915.922217	12.957619
13.894796	923.096700	12.962637
14.555690	926.784666	12.967655
14.534363	946.408997	12.972672
14.197643	934.716370	12.977690
14.454145	945.509477	12.982707
14.561925	943.913556	12.987725
14.415815	955.611723	12.992743
14.261103	956.794095	12.997760
14.527357	949.947567	13.002778
14.185613	948.412387	13.007795
14.271175	955.975663	13.012813
14.665538	958.381253	13.017831
14.093862	954.208087	13.022848
14.717734	949.071688	13.027866
14.637369	960.447337	13.032883
14.261710	953.651994	13.037901
14.579130	949.159406	13.042919
14.445309	955.603710	13.047936
14.622984	949.307698	13.052954
14.494630	960.834621	13.057971
14.776894	963.146253	13.062989
14.674437	955.485474	13.068007
14.478100	952.267965	13.073024
15.026591	972.875894	13.078042
14.778199	965.148820	13.083059
14.375023	963.765967	13.088077
14.593835	970.246147	13.093095
14.712157	983.865021	13.098112
14.957105	984.796332	13.103130
14.707328	986.169693	13.108147
14.575412	988.456083	13.113165
15.049943	986.188804	13.118183
14.775296	990.556662	13.123200
15.001478	988.097606	13.128218
14.753801	983.744602	13.133235
14.631909	993.435946	13.138253
14.779276	974.504813	13.143271
14.815123	999.154426	13.148288
15.156773	978.638336	13.153306
14.884996	983.430491	13.158323
15.110925	996.630335	13.163341
15.338748	987.866676	13.168359
15.184684	989.655991	13.173376
15.213201	987.861246	13.178394
15.425949	987.298792	13.183411
15.086903	988.357090	13.188429
14.911059	964.590236	13.193447
14.719038	972.019748	13.198464
15.312627	974.897706	13.203482
15.333531	983.364993	13.208499
15.286397	980.669888	13.213517
15.136815	961.029515	13.218535
14.809367	969.020477	13.223552
14.889983	966.255325	13.228570
15.256245	979.733384	13.233587
15.081386	988.209591	13.238605
15.521582	982.912778	13.243623
15.123824	991.139440	13.248640
15.190838	995.935913	13.253658
15.403313	981.149203	13.258675
15.424827	991.237155	13.263693
15.605138	981.584209	13.268711
15.158832	975.851713	13.273728
15.352621	973.464181	13.278746
15.300898	972.630352	13.283763
15.143194	979.617183	13.288781
15.188004	975.412404	13.293799
15.071658	994.522702	13.298816
15.099789	978.672214	13.303834
15.204739	983.592292	13.308851
15.404347	987.346316	13.313869
15.171679	983.481731	13.318887
15.067191	985.898986	13.323904
15.237322	983.077223	13.328922
15.311040	983.126029	13.333939
15.161572	979.862538	13.338957
15.398183	992.154361	13.343975
15.310511	1007.281024	13.348992
15.620952	1016.866667	13.354010
15.535466	1015.951445	13.359027
15.476616	1016.049843	13.364045
15.841261	1006.839049	13.369063
15.782588	1012.717377	13.374080
15.867093	999.286876	13.379098
15.614234	984.643645	13.384115
15.066407	980.609805	13.389133
15.618979	994.401770	13.394151
15.402517	1010.536396	13.399168
15.718151	1012.253943	13.404186
15.772340	1008.796368	13.409203
15.470634	1015.333558	13.414221
15.476490	1008.730274	13.419239
15.568262	1021.205240	13.424256
15.448516	1012.050940	13.429274
15.599131	1007.293953	13.434291
15.384417	1009.005955	13.439309
15.763844	1003.810962	13.444327
15.424903	1007.254530	13.449344
15.559443	1016.988301	13.454362
16.095918	1022.390962	13.459379
15.797231	1023.081947	13.464397
16.079149	1007.145550	13.469415
16.267552	1007.827222	13.474432
15.813296	1002.362950	13.479450
15.750576	1001.006570	13.484467
15.727534	1004.771230	13.489485
16.133641	997.343202	13.494503
16.054252	1011.694132	13.499520
15.905123	1008.870709	13.504538
15.786498	1009.793559	13.509555
15.769708	1008.857864	13.514573
15.932361	1016.731171	13.519591
16.074277	1042.340329	13.524608
16.192594	1037.509571	13.529626
16.244006	1030.303072	13.534643
15.739850	1028.840152	13.539661
15.841092	1022.830026	13.544679
16.181598	1039.056740	13.549696
16.066333	1031.704726	13.554714
16.073811	1027.416379	13.559731
16.202837	1043.595183	13.564749
16.178102	1037.513476	13.569767
16.237840	1042.832796	13.574784
16.303408	1031.363567	13.579802
16.729231	1037.983373	13.584819
16.071151	1038.371911	13.589837
16.469082	1040.151368	13.594855
16.499888	1030.750000	13.599872
16.050573	1023.208646	13.604890
16.273812	1021.392948	13.609907
16.154387	1034.346308	13.614925
16.164083	1042.291505	13.619943
16.151741	1033.026827	13.624960
16.195048	1037.463890	13.629978
16.275326	1039.349686	13.634995
16.396849	1039.209848	13.640013
16.739632	1032.893445	13.645031
16.424657	1037.891997	13.650048
16.387114	1037.213672	13.655066
16.424015	1031.308719	13.660083
16.322975	1047.594661	13.665101
16.541070	1033.204581	13.670119
16.291067	1040.328034	13.675136
16.407577	1040.145332	13.680154
16.257486	1036.232758	13.685171
16.515933	1042.491826	13.690189
16.230135	1039.564349	13.695207
16.289604	1040.200529	13.700224
16.377931	1041.029538	13.705242
16.552815	1040.556047	13.710259
16.470304	1047.861494	13.715277
16.582479	1055.520783	13.720295
16.517860	1058.949867	13.725312
16.533140	1061.935381	13.730330
16.977916	1078.345975	13.735347
16.801278	1078.375374	13.740365
16.917149	1072.161234	13.745383
16.583302	1063.108628	13.750400
16.618524	1062.293018	13.755418
16.769973	1072.503906	13.760435
16.667742	1073.409469	13.765453
16.764308	1078.940384	13.770471
16.942564	1072.721386	13.775488
16.708956	1084.598948	13.780506
17.125714	1073.131155	13.785523
16.955336	1082.133016	13.790541
17.158585	1068.279987	13.795559
16.951960	1046.912472	13.800576
16.573557	1050.631490	13.805594
16.735603	1053.060356	13.810611
16.352587	1066.951991	13.815629
16.660945	1069.194346	13.820647
16.679595	1079.484789	13.825664
16.727659	1077.987160	13.830682
16.899513	1074.149405	13.835699
16.960983	1081.619114	13.840717
16.820488	1075.577498	13.845735
16.879949	1078.453709	13.850752
16.754371	1080.680401	13.855770
17.205548	1081.666018	13.860787
16.848682	1089.349744	13.865805
16.990142	1086.691381	13.870823
17.113280	1100.017447	13.875840
16.830928	1105.870000	13.880858
17.505678	1100.357400	13.885875
17.105967	1104.216972	13.890893
17.358956	1101.244416	13.895911
17.212500	1107.098790	13.900928
17.272636	1100.041587	13.905946
17.343343	1099.562577	13.910963
17.301541	1111.702357	13.915981
17.449354	1107.372554	13.920999
17.345691	1105.673383	13.926016
17.101887	1112.948979	13.931034
17.365188	1094.671227	13.936051
17.342448	1097.978405	13.941069
17.078001	1098.023974	13.946087
17.180737	1089.433796	13.951104
17.213258	1115.305338	13.956122
17.335937	1102.276255	13.961139
17.365480	1101.790702	13.966157
17.242377	1102.813509	13.971175
17.013066	1107.543529	13.976192
17.292441	1097.372893	13.981210
17.533327	1105.736756	13.986227
17.240700	1103.289116	13.991245
17.260416	1102.098149	13.996263
17.578405	1111.392455	14.001280
17.836093	1128.351887	14.006298
18.130700	1111.016105	14.011315
17.687350	1099.202699	14.016333
17.578225	1098.459501	14.021351
17.758895	1096.221760	14.026368
17.350824	1096.835265	14.031386
17.902217	1091.737244	14.036403
17.742278	1092.242187	14.041421
17.817411	1093.013946	14.046439
17.578501	1089.691680	14.051456
17.364663	1095.799361	14.056474
17.904190	1092.770125	14.061491
17.603384	1102.394037	14.066509
17.558391	1101.546484	14.071527
17.640597	1103.056791	14.076544
17.617044	1110.141455	14.081562
17.845238	1123.417405	14.086579
17.907785	1126.391139	14.091597
18.113416	1123.569749	14.096615
18.502419	1117.241692	14.101632
17.847243	1106.855538	14.106650
17.813156	1099.030576	14.111667
18.064745	1097.227085	14.116685
18.047796	1102.580431	14.121703
17.867156	1091.803619	14.126720
17.753000	1095.181499	14.131738
17.931000	1099.535959	14.136755
18.296993	1114.070028	14.141773
18.130309	1116.517718	14.146791
18.117021	1099.774434	14.151808
18.029512	1095.239667	14.156826
17.942602	1090.115858	14.161843
18.071116	1102.616670	14.166861
18.238662	1118.356497	14.171879
18.405375	1116.581284	14.176896
17.769481	1101.484706	14.181914
18.058874	1109.233850	14.186931
18.120854	1117.841619	14.191949
18.094824	1119.130954	14.196967
18.660090	1119.432687	14.201984
18.261303	1119.660418	14.207002
18.465082	1117.416865	14.212019
18.312051	1104.907990	14.217037
18.308876	1105.622691	14.222055
18.490305	1093.961333	14.227072
18.039583	1098.091179	14.232090
18.649593	1097.747715	14.237107
18.441431	1103.847763	14.242125
17.814951	1093.901705	14.247143
18.310686	1101.211847	14.252160
18.243814	1111.554320	14.257178
18.280039	1106.673804	14.262195
18.280166	1110.022062	14.267213
18.409314	1111.380481	14.272231
18.837359	1102.548047	14.277248
18.495631	1114.023941	14.282266
18.509872	1116.991529	14.287283
18.573691	1105.627255	14.292301
18.332644	1115.725467	14.297319
18.507991	1113.915750	14.302336
18.394165	1115.838935	14.307354
18.555530	1118.347842	14.312371
18.348907	1115.114293	14.317389
18.289466	1122.791117	14.322407
18.631656	1116.105507	14.327424
18.593293	1116.986285	14.332442
18.650717	1115.629609	14.337459
18.532346	1124.438215	14.342477
18.394308	1149.679537	14.347495
18.941817	1134.241750	14.352512
18.891055	1144.044193	14.357530
19.004021	1146.688702	14.362547
19.008752	1135.741685	14.367565
18.872168	1133.318494	14.372583
18.974619	1132.799957	14.377600
18.898241	1126.674439	14.382618
19.036970	1130.701202	14.387635
18.740282	1120.081053	14.392653
18.707611	1124.430775	14.397671
18.867776	1132.260069	14.402688
18.797445	1136.704238	14.407706
18.751378	1133.345185	14.412723
18.907632	1140.416906	14.417741
18.840364	1138.947102	14.422759
18.286898	1138.350195	14.427776
18.231938	1148.148221	14.432794
18.896375	1158.270358	14.437811
19.092295	1170.800570	14.442829
18.774001	1190.688732	14.447847
18.977220	1174.338494	14.452864
19.327579	1179.463894	14.457882
19.344362	1181.763390	14.462899
19.159032	1181.273787	14.467917
19.187169	1182.282485	14.472935
19.474702	1171.850220	14.477952
19.233299	1171.027042	14.482970
19.465301	1174.717857	14.487987
19.335449	1170.368836	14.493005
19.823719	1168.630324	14.498023
19.572619	1147.810585	14.503040
19.202899	1146.957164	14.508058
19.248359	1140.176778	14.513075
19.662205	1136.949538	14.518093
19.567703	1146.509266	14.523111
19.478382	1141.217346	14.528128
19.672608	1135.629493	14.533146
19.721923	1139.875833	14.538163
20.123615	1136.925402	14.543181
19.572434	1134.133350	14.548199
19.548017	1130.114042	14.553216
19.744569	1134.686282	14.558234
19.643390	1135.268069	14.563251
19.635524	1130.677536	14.568269
19.450086	1141.172012	14.573287
19.773598	1132.237258	14.578304
19.553737	1139.511249	14.583322
19.520032	1135.245465	14.588339
19.495051	1141.946150	14.593357
19.571794	1146.963483	14.598375
19.530047	1144.060379	14.603392
19.171174	1140.139570	14.608410
19.111259	1137.712296	14.613427
19.604042	1128.816728	14.618445
19.267289	1134.662193	14.623463
19.224854	1148.713422	14.628480
19.424751	1158.083681	14.633498
19.720552	1163.765360	14.638515
19.974955	1171.705381	14.643533
19.974736	1164.440476	14.648551
20.046771	1173.407215	14.653568
19.913171	1171.237447	14.658586
19.743121	1171.462984	14.663603
20.122853	1162.321241	14.668621
19.732790	1177.649898	14.673639
19.963645	1160.163643	14.678656
19.727032	1175.951808	14.683674
19.683495	1174.170986	14.688691
19.815539	1169.868981	14.693709
19.875133	1172.863293	14.698727
19.808130	1166.535817	14.703744
19.747653	1163.687001	14.708762
20.138414	1181.435748	14.713779
19.876019	1183.456466	14.718797
19.657272	1202.410427	14.723815
20.271153	1196.529189	14.728832
20.361156	1198.005534	14.733850
20.112299	1194.472704	14.738867
20.631546	1194.495094	14.743885
20.226366	1198.035142	14.748903
20.627993	1192.321068	14.753920
20.608937	1194.500151	14.758938
20.237797	1184.974562	14.763955
20.460340	1169.900186	14.768973
20.177239	1174.015182	14.773991
20.196494	1168.748905	14.779008
20.073495	1195.071998	14.784026
20.071121	1188.524333	14.789043
20.595610	1199.062652	14.794061
20.307159	1195.370269	14.799079
20.153604	1197.974050	14.804096
20.480457	1186.525841	14.809114
20.349921	1194.987708	14.814131
20.494176	1188.734159	14.819149
20.190591	1200.971455	14.824167
20.466979	1195.332524	14.829184
20.569409	1198.666160	14.834202
19.989652	1203.206832	14.839219
20.380502	1195.996590	14.844237
20.808860	1222.024160	14.849255
20.527584	1203.321859	14.854272
20.571660	1221.554633	14.859290
20.881549	1217.669885	14.864307
21.227116	1213.831960	14.869325
20.496905	1213.367965	14.874343
20.401979	1188.243288	14.879360
20.728627	1207.340843	14.884378
20.689081	1217.652074	14.889395
21.218143	1223.809941	14.894413
20.767693	1215.740753	14.899431
20.738347	1216.962540	14.904448
20.891376	1215.874597	14.909466
21.007850	1222.116000	14.914483
21.234075	1212.921792	14.919501
20.817402	1198.548487	14.924519
20.969507	1197.905559	14.929536
21.154376	1196.313531	14.934554
20.737626	1192.240919	14.939571
21.121241	1198.224141	14.944589
20.850532	1206.475071	14.949607
20.868555	1217.717239	14.954624
21.264819	1227.767466	14.959642
21.193539	1234.284951	14.964659
21.319086	1216.277578	14.969677
20.834712	1217.916319	14.974695
21.132464	1220.647050	14.979712
20.876195	1220.385761	14.984730
21.138342	1222.324024	14.989747
21.407075	1213.965230	14.994765
21.452803	1234.468107	14.999783
21.366995	1226.398933	15.004800
21.475234	1224.751138	15.009818
21.219294	1226.218453	15.014835
21.331548	1222.305926	15.019853
21.040564	1226.905294	15.024871
21.084088	1223.058912	15.029888
21.490102	1218.020052	15.034906
20.960549	1225.733728	15.039923
21.214922	1212.079937	15.044941
21.369895	1223.959945	15.049959
21.267234	1213.418106	15.054976
21.588406	1213.763169	15.059994
21.304548	1224.433107	15.065011
21.639388	1212.661913	15.070029
21.329874	1223.058963	15.075047
21.494783	1225.612571	15.080064
21.681049	1211.083530	15.085082
21.289805	1228.513513	15.090099
21.556021	1218.558360	15.095117
21.741185	1239.434899	15.100135
21.583348	1249.796520	15.105152
21.913550	1237.097775	15.110170
21.612315	1250.544899	15.115187
21.827167	1246.806248	15.120205
21.870990	1242.508652	15.125223
21.853444	1234.761970	15.130240
21.893581	1223.318085	15.135258
21.447178	1221.845152	15.140275
22.251502	1228.812740	15.145293
21.752279	1223.984966	15.150311
21.258894	1226.543665	15.155328
21.574249	1229.656099	15.160346
21.500884	1243.787749	15.165363
21.763687	1234.230773	15.170381
21.481293	1234.088782	15.175399
21.359725	1240.418574	15.180416
21.997882	1248.687352	15.185434
22.098028	1260.892628	15.190451
22.431838	1255.458689	15.195469
22.235081	1247.454399	15.200487
22.220027	1244.843282	15.205504
22.385941	1239.192385	15.210522
22.003081	1237.869510	15.215539
21.829460	1237.775185	15.220557
21.969067	1236.339094	15.225575
22.192950	1238.650237	15.230592
22.221856	1228.947109	15.235610
22.216529	1237.694472	15.240627
22.222447	1241.817351	15.245645
22.288335	1252.780735	15.250663
22.374196	1259.897280	15.255680
22.671591	1263.809127	15.260698
22.478154	1251.409994	15.265715
22.096048	1236.532112	15.270733
22.507497	1230.263269	15.275751
22.318265	1229.315279	15.280768
22.548080	1234.096972	15.285786
22.488297	1244.517878	15.290803
22.805077	1236.563272	15.295821
22.656987	1234.065603	15.300839
22.544461	1236.559820	15.305856
22.614887	1227.917458	15.310874
22.355515	1231.081720	15.315891
22.718568	1229.397477	15.320909
22.579978	1229.692193	15.325927
22.484450	1236.348348	15.330944
22.643876	1226.842809	15.335962
22.387710	1240.744616	15.340979
22.489900	1250.490210	15.345997
22.980400	1260.343307	15.351015
22.578510	1261.756541	15.356032
22.980740	1267.866218	15.361050
22.904519	1264.363730	15.366067
22.905781	1257.718586	15.371085
22.774723	1263.786985	15.376103
22.629820	1263.461518	15.381120
22.900496	1259.800590	15.386138
22.887420	1270.423190	15.391155
23.087845	1264.042564	15.396173
23.186606	1259.570484	15.401191
22.924716	1266.866481	15.406208
22.946692	1262.571329	15.411226
22.929411	1267.153168	15.416243
22.864351	1259.472243	15.421261
23.018240	1264.720874	15.426279
22.761643	1252.860168	15.431296
22.876706	1259.968710	15.436314
22.972119	1254.522035	15.441331
22.700524	1265.066740	15.446349
22.919188	1259.374392	15.451367
22.981903	1260.506475	15.456384
23.285901	1259.188721	15.461402
23.063418	1265.337274	15.466419
23.305521	1266.141129	15.471437
23.269001	1266.456280	15.476455
22.992902	1270.775641	15.481472
23.211724	1280.758943	15.486490
23.210705	1294.754604	15.491507
23.210103	1291.888726	15.496525
23.591862	1294.963760	15.501543
23.445675	1293.082274	15.506560
23.589660	1291.379320	15.511578
23.474792	1292.646823	15.516595
23.726357	1285.164428	15.521613
23.766423	1279.875757	15.526631
23.425669	1267.582983	15.531648
23.460604	1263.066002	15.536666
23.486965	1275.996907	15.541683
23.847474	1277.215709	15.546701
23.737806	1269.968946	15.551719
23.234305	1269.388136	15.556736
23.389558	1283.392850	15.561754
23.547127	1289.751066	15.566771
23.638855	1297.207584	15.571789
23.716996	1292.471611	15.576807
23.213206	1296.784337	15.581824
23.622574	1290.172129	15.586842
23.481787	1294.430425	15.591859
23.660808	1290.244984	15.596877
23.606332	1289.759217	15.601895
23.387107	1294.789178	15.606912
23.642094	1300.579656	15.611930
23.580989	1306.319923	15.616947
23.759356	1319.674793	15.621965
24.123968	1307.041135	15.626983
23.884791	1318.430452	15.632000
24.198751	1315.388274	15.637018
23.937609	1310.728373	15.642035
24.178810	1302.718187	15.647053
24.031519	1314.920540	15.652071
24.100361	1315.362661	15.657088
24.322834	1312.177430	15.662106
24.490926	1305.139197	15.667123
24.047396	1317.123872	15.672141
24.507371	1302.262255	15.677159
24.207898	1321.625825	15.682176
24.265712	1312.041851	15.687194
24.792921	1311.796395	15.692211
24.452515	1302.155393	15.697229
24.378026	1288.708158	15.702247
24.243275	1280.637248	15.707264
24.175264	1292.703577	15.712282
24.294587	1306.407211	15.717299
24.292647	1313.842692	15.722317
24.758167	1307.449481	15.727335
24.515369	1309.048078	15.732352
24.455299	1310.035620	15.737370
24.687665	1306.820006	15.742387
24.242267	1304.765820	15.747405
24.927308	1303.439451	15.752423
24.710761	1311.093270	15.757440
24.521699	1302.245976	15.762458
24.478704	1305.050287	15.767475
24.465388	1301.079087	15.772493
24.579652	1305.263498	15.777511
24.626586	1305.164008	15.782528
24.753599	1313.263854	15.787546
24.452028	1303.978585	15.792563
24.518937	1311.804180	15.797581
24.542490	1305.438368	15.802599
24.510239	1306.287040	15.807616
24.704359	1307.870887	15.812634
24.667978	1309.247782	15.817651
24.425535	1302.033702	15.822669
24.404148	1309.335017	15.827687
24.457723	1331.635856	15.832704
24.656657	1338.337596	15.837722
24.722988	1330.489527	15.842739
25.055067	1329.595823	15.847757
25.061253	1326.310323	15.852775
25.157383	1332.828763	15.857792
24.700949	1330.308710	15.862810
24.663460	1335.591930	15.867827
24.608795	1348.122994	15.872845
25.272274	1353.370024	15.877863
25.185306	1377.607993	15.882880
25.309771	1369.519935	15.887898
25.504441	1365.815713	15.892915
25.380597	1353.629725	15.897933
25.533195	1342.380044	15.902951
25.202261	1338.117939	15.907968
25.298232	1335.647008	15.912986
25.592388	1334.289154	15.918003
25.265604	1335.196229	15.923021
25.298255	1323.957837	15.928039
25.143910	1339.208106	15.933056
25.282205	1352.493290	15.938074
25.688774	1362.223007	15.943091
25.819565	1358.871910	15.948109
25.561872	1334.342531	15.953127
25.085139	1342.844697	15.958144
25.347606	1343.034566	15.963162
25.599234	1366.649727	15.968179
25.407927	1369.477125	15.973197
25.616873	1363.555655	15.978215
25.588138	1363.532912	15.983232
26.089642	1359.909970	15.988250
26.211297	1358.308354	15.993267
25.917113	1359.150173	15.998285
25.911048	1341.009419	16.003303
25.789922	1333.615717	16.008320
25.408733	1325.932187	16.013338
25.720158	1336.601680	16.018355
25.704598	1359.262460	16.023373
25.971163	1359.292207	16.028391
25.542112	1342.331949	16.033408
25.662044	1351.932144	16.038426
25.859059	1354.223755	16.043443
25.952332	1358.704572	16.048461
26.116956	1356.924168	16.053479
25.863065	1355.912511	16.058496
25.667766	1360.331848	16.063514
25.897319	1357.243065	16.068531
25.848622	1358.502724	16.073549
26.540890	1368.515261	16.078567
26.189628	1367.361132	16.083584
26.161369	1360.568100	16.088602
26.200105	1361.114829	16.093619
26.293408	1357.595954	16.098637
26.272940	1357.139177	16.103655
26.118482	1367.150722	16.108672
26.143890	1378.024076	16.113690
26.530994	1379.694355	16.118707
26.243711	1383.446335	16.123725
26.640028	1382.297078	16.128743
26.565736	1391.466212	16.133760
26.496647	1384.794518	16.138778
26.834042	1377.123411	16.143795
26.479719	1357.692147	16.148813
26.684259	1343.171755	16.153831
26.737686	1342.783008	16.158848
26.666869	1348.914259	16.163866
26.765843	1340.939898	16.168883
26.783205	1356.048263	16.173901
26.776562	1341.646828	16.178919
26.991412	1343.651233	16.183936
26.253920	1344.952151	16.188954
26.861084	1341.646677	16.193971
26.609718	1341.900298	16.198989
26.524155	1342.048412	16.204007
26.607570	1345.554131	16.209024
26.417702	1352.246882	16.214042
26.832138	1356.107410	16.219059
26.843447	1375.614660	16.224077
26.841074	1377.340225	16.229095
26.869067	1378.250538	16.234112
26.782803	1368.957789	16.239130
27.255688	1372.421614	16.244147
27.063875	1377.284848	16.249165
27.001567	1369.887651	16.254183
26.863957	1379.512560	16.259200
27.274257	1374.365068	16.264218
26.903418	1368.497837	16.269235
26.583950	1380.594219	16.274253
26.781736	1374.717510	16.279271
26.991699	1385.398783	16.284288
26.968842	1371.375986	16.289306
27.019905	1372.023813	16.294323
27.124505	1395.626842	16.299341
27.341513	1401.045338	16.304359
27.433076	1399.208178	16.309376
27.466688	1408.156638	16.314394
27.452432	1406.244155	16.319411
27.315136	1409.664530	16.324429
27.521882	1412.491128	16.329447
27.647132	1407.352815	16.334464
27.653927	1398.052456	16.339482
27.711268	1404.465566	16.344499
27.365726	1396.231213	16.349517
27.288571	1395.733465	16.354535
27.765831	1404.664088	16.359552
27.571515	1405.362936	16.364570
28.011165	1403.489572	16.369587
28.170151	1402.297087	16.374605
27.818849	1382.420031	16.379623
27.768099	1375.968906	16.384640
27.814731	1370.598800	16.389658
27.637720	1360.036150	16.394675
27.628717	1363.533219	16.399693
27.652780	1391.403795	16.404711
28.171304	1393.829763	16.409728
27.628840	1407.389161	16.414746
27.904099	1399.342952	16.419763
27.975682	1401.361728	16.424781
27.987670	1399.788966	16.429799
27.965354	1399.586422	16.434816
28.124309	1408.625463	16.439834
28.198435	1399.790271	16.444851
27.690627	1408.260631	16.449869
27.647573	1400.651566	16.454887
27.731996	1404.223270	16.459904
27.637937	1404.194063	16.464922
28.107526	1398.014699	16.469939
28.272696	1407.502689	16.474957
28.145405	1403.083494	16.479975
27.963795	1416.674258	16.484992
27.713506	1426.750980	16.490010
27.977341	1427.739415	16.495027
28.313149	1424.387691	16.500045
28.319897	1425.979860	16.505063
28.292959	1425.141886	16.510080
28.147250	1433.351689	16.515098
28.560216	1426.079794	16.520115
28.546029	1427.564029	16.525133
28.163963	1422.471846	16.530151
28.423418	1424.368457	16.535168
28.501904	1434.707063	16.540186
28.744616	1442.559407	16.545203
28.945974	1440.820525	16.550221
28.789955	1432.505441	16.555239
29.032178	1419.456223	16.560256
28.777309	1426.604282	16.565274
28.645668	1417.315503	16.570291
28.944167	1425.937279	16.575309
28.794063	1429.984569	16.580327
29.220158	1415.870576	16.585344
28.615240	1428.570719	16.590362
28.951378	1417.401891	16.595379
28.755571	1421.311898	16.600397
28.856339	1423.034498	16.605415
28.954257	1424.618600	16.610432
29.018535	1423.385558	16.615450
29.109238	1418.715172	16.620467
29.219934	1412.715135	16.625485
28.984445	1419.460377	16.630503
29.382190	1409.156087	16.635520
28.878276	1426.360933	16.640538
28.873105	1412.593811	16.645555
28.913946	1437.323210	16.650573
29.052027	1444.890988	16.655591
29.257428	1456.442331	16.660608
29.107375	1449.271485	16.665626
29.403306	1448.736527	16.670643
29.182037	1449.849685	16.675661
29.137772	1446.939069	16.680679
29.380568	1446.071615	16.685696
29.185960	1444.346185	16.690714
29.261774	1440.591623	16.695731
29.405777	1443.007410	16.700749
29.547515	1440.578066	16.705767
30.030504	1434.791723	16.710784
29.568283	1441.974646	16.715802
29.580210	1444.949768	16.720819
29.755266	1447.419447	16.725837
29.635512	1439.851850	16.730855
29.647552	1432.789499	16.735872
29.666056	1447.442267	16.740890
29.730063	1442.163340	16.745907
29.806604	1440.173952	16.750925
29.778119	1439.451979	16.755943
29.547355	1437.764054	16.760960
29.827022	1449.778623	16.765978
29.864443	1456.138374	16.770995
30.318193	1454.870516	16.776013
30.314702	1442.694768	16.781031
30.253049	1440.031916	16.786048
30.061718	1439.385827	16.791066
30.115331	1426.941160	16.796083
30.118221	1424.512457	16.801101
30.204829	1424.137090	16.806119
30.354547	1425.215356	16.811136
30.021501	1416.180518	16.816154
30.278595	1420.067609	16.821171
30.496319	1420.907808	16.826189
30.091588	1419.912556	16.831207
30.436240	1420.353719	16.836224
30.522403	1431.475271	16.841242
30.302686	1418.778020	16.846259
30.313064	1414.233975	16.851277
30.023610	1427.948181	16.856295
30.438139	1416.406494	16.861312
29.952889	1429.516260	16.866330
30.351883	1422.415187	16.871347
30.382372	1431.958254	16.876365
30.401084	1450.114020	16.881383
30.643165	1449.695489	16.886400
30.728527	1450.890749	16.891418
30.736770	1455.947914	16.896435
30.785238	1464.665204	16.901453
30.539246	1454.221038	16.906471
30.570458	1456.620929	16.911488
30.346131	1458.545987	16.916506
30.601080	1458.682386	16.921523
30.315614	1449.485688	16.926541
30.310826	1462.509719	16.931559
30.441022	1455.291108	16.936576
30.582525	1463.724440	16.941594
30.943157	1480.375820	16.946611
30.946471	1488.761664	16.951629
30.896792	1495.644554	16.956647
31.283050	1482.700080	16.961664
31.118216	1482.008247	16.966682
31.081809	1489.152306	16.971699
31.263634	1485.823801	16.976717
31.501540	1473.909472	16.981735
31.218837	1471.663264	16.986752
31.061089	1470.738766	16.991770
31.606169	1473.683151	16.996787
31.233526	1459.394799	17.001805
31.119647	1461.385750	17.006823
31.376161	1467.107535	17.011840
30.975682	1480.037905	17.016858
31.489275	1478.175470	17.021875
31.610457	1476.977452	17.026893
31.176908	1483.040703	17.031911
31.302668	1477.452691	17.036928
31.280681	1478.342971	17.041946
31.493960	1477.325702	17.046963
31.428607	1474.538661	17.051981
31.317087	1484.412046	17.056999
31.719357	1473.624299	17.062016
31.355647	1482.719941	17.067034
31.256736	1478.264119	17.072051
31.685543	1483.921448	17.077069
31.879216	1498.288465	17.082087
32.165150	1491.901801	17.087104
32.113367	1483.194573	17.092122
31.843675	1481.921762	17.097139
31.837901	1468.112566	17.102157
31.907156	1474.617423	17.107175
31.833082	1468.492567	17.112192
32.063921	1470.469923	17.117210
32.171102	1472.027295	17.122227
32.081431	1466.618789	17.127245
32.149059	1473.042816	17.132263
32.178676	1471.493494	17.137280
32.181607	1473.141025	17.142298
31.987624	1460.913462	17.147315
32.056894	1465.168386	17.152333
32.325032	1479.697413	17.157351
32.505762	1481.212641	17.162368
32.494347	1476.269062	17.167386
32.407019	1471.448336	17.172403
32.649061	1468.229507	17.177421
32.340577	1470.988213	17.182439
32.524061	1465.146524	17.187456
32.539586	1471.265048	17.192474
32.229853	1455.227716	17.197491
32.522365	1460.517152	17.202509
32.281344	1461.316676	17.207527
32.575541	1462.144560	17.212544
32.351207	1468.213188	17.217562
32.260382	1483.331392	17.222579
32.568568	1486.833641	17.227597
32.782119	1489.545740	17.232615
32.800222	1483.481540	17.237632
32.779996	1486.794681	17.242650
32.833919	1494.250885	17.247667
32.697891	1488.741024	17.252685
32.722264	1489.091333	17.257703
32.592657	1487.856259	17.262720
32.322425	1495.675387	17.267738
32.424194	1493.656209	17.272755
32.811309	1494.058428	17.277773
32.638611	1516.101875	17.282791
33.089736	1520.414209	17.287808
33.250014	1514.088183	17.292826
32.986242	1518.483513	17.297843
33.442243	1504.906186	17.302861
33.085815	1515.057691	17.307879
33.294469	1514.686052	17.312896
33.274872	1509.090693	17.317914
32.998019	1520.256111	17.322931
33.110840	1506.584252	17.327949
33.134072	1508.344157	17.332967
33.111913	1515.860259	17.337984
33.124396	1520.858474	17.343002
33.148212	1520.142764	17.348019
33.431055	1518.760004	17.353037
33.357606	1536.195383	17.358055
33.839635	1544.292247	17.363072
33.811375	1529.861160	17.368090
33.383412	1516.631921	17.373107
33.705861	1529.081161	17.378125
33.564826	1537.521731	17.383143
33.737764	1541.297253	17.388160
34.212115	1534.613121	17.393178
34.183523	1523.548931	17.398195
34.200851	1509.428781	17.403213
33.472641	1512.211982	17.408231
33.909692	1506.979294	17.413248
33.792320	1503.119429	17.418266
33.841948	1503.715532	17.423283
34.065858	1507.602650	17.428301
33.650239	1510.042171	17.433319
33.705187	1513.718797	17.438336
34.104026	1529.144624	17.443354
34.374011	1532.605991	17.448371
34.230223	1530.894544	17.453389
34.246240	1537.539375	17.458407
34.362170	1529.980198	17.463424
34.153221	1529.285853	17.468442
34.034631	1537.455377	17.473459
34.459472	1522.716710	17.478477
34.637690	1532.179774	17.483495
34.630473	1532.014482	17.488512
34.589280	1531.130842	17.493530
34.303560	1528.356402	17.498547
34.445868	1522.206584	17.503565
34.313804	1518.645211	17.508583
34.339248	1531.058387	17.513600
34.474722	1527.623800	17.518618
34.454534	1529.924768	17.523635
34.630652	1526.018479	17.528653
34.527148	1530.745825	17.533671
34.285046	1531.267980	17.538688
34.541885	1528.867129	17.543706
34.304999	1524.033450	17.548723
34.588689	1529.964910	17.553741
34.650563	1548.926981	17.558759
34.680573	1556.969063	17.563776
34.702693	1549.593180	17.568794
34.634423	1545.176733	17.573811
35.173737	1540.324664	17.578829
34.974161	1550.890268	17.583847
35.106976	1545.438063	17.588864
35.098367	1551.838968	17.593882
34.962481	1548.656954	17.598899
35.060136	1553.190641	17.603917
35.366450	1549.989852	17.608935
35.006646	1553.791327	17.613952
35.458796	1543.829472	17.618970
35.096009	1546.105104	17.623987
35.169751	1549.950657	17.629005
35.052528	1553.819684	17.634023
35.089883	1549.778976	17.639040
35.326658	1558.682733	17.644058
35.281061	1571.156172	17.649075
35.375880	1568.210605	17.654093
35.436694	1582.414747	17.659111
35.171972	1577.741580	17.664128
35.679464	1568.272860	17.669146
35.317023	1583.071748	17.674163
35.492528	1575.640045	17.679181
35.211782	1582.194852	17.684199
35.500877	1580.576014	17.689216
35.881222	1590.929513	17.694234
35.612952	1604.678935	17.699251
36.045175	1608.043671	17.704269
36.005714	1611.537197	17.709287
35.875258	1618.268611	17.714304
36.257445	1603.553099	17.719322
36.373293	1604.713384	17.724339
36.379561	1585.707714	17.729357
36.396011	1574.510021	17.734375
36.193898	1567.273364	17.739392
36.404891	1563.046317	17.744410
36.211889	1571.287674	17.749427
36.263812	1567.771692	17.754445
35.964994	1568.286740	17.759463
35.986840	1563.871844	17.764480
36.284772	1562.870027	17.769498
36.233081	1567.389172	17.774515
36.224375	1581.893050	17.779533
36.100382	1585.833681	17.784551
36.001497	1599.794311	17.789568
36.587509	1599.309951	17.794586
36.192529	1607.071917	17.799603
36.332934	1597.759860	17.804621
36.795081	1602.574705	17.809639
36.719575	1601.481020	17.814656
36.596369	1600.092122	17.819674
36.578890	1602.426114	17.824691
36.744768	1600.669490	17.829709
36.790369	1605.459870	17.834727
36.550042	1603.924299	17.839744
37.013472	1599.157659	17.844762
36.746764	1603.854674	17.849779
36.702571	1602.423509	17.854797
36.737352	1599.735941	17.859815
36.638371	1627.844318	17.864832
36.961822	1625.099711	17.869850
36.940816	1641.372186	17.874867
36.935348	1628.689545	17.879885
36.891132	1636.524325	17.884903
36.601926	1634.568932	17.889920
36.990750	1631.441419	17.894938
37.044728	1630.223064	17.899955
37.060659	1630.634226	17.904973
37.087203	1644.564600	17.909991
37.102555	1659.219667	17.915008
37.451959	1654.074725	17.920026
37.721145	1659.392910	17.925043
37.354673	1658.012156	17.930061
37.702157	1656.413526	17.935079
37.709386	1658.233194	17.940096
37.914976	1649.463017	17.945114
38.024992	1647.366467	17.950131
37.721771	1630.994412	17.955149
37.485302	1626.794476	17.960167
37.650936	1625.092613	17.965184
37.856913	1637.060128	17.970202
37.664923	1654.269285	17.975219
37.906538	1653.618548	17.980237
37.860878	1655.364331	17.985255
37.761076	1653.205805	17.990272
37.851302	1651.174747	17.995290
37.831867	1647.878477	18.000307
38.004909	1648.638322	18.005325
38.196972	1643.177416	18.010343
37.861221	1648.720155	18.015360
37.886375	1648.206969	18.020378
38.226046	1657.492491	18.025395
38.434607	1651.224526	18.030413
38.209987	1646.257276	18.035431
37.618324	1647.100127	18.040448
38.316192	1650.611267	18.045466
38.292664	1652.244712	18.050483
38.017755	1646.129151	18.055501
38.340445	1659.501666	18.060519
38.568061	1668.604248	18.065536
38.431257	1675.720199	18.070554
38.661728	1668.402542	18.075571
38.542895	1675.663535	18.080589
38.713792	1675.854457	18.085607
38.605173	1674.958787	18.090624
38.728128	1673.311255	18.095642
38.931732	1681.557223	18.100659
38.638953	1679.280376	18.105677
38.765090	1671.219442	18.110695
38.628071	1686.937637	18.115712
38.715664	1674.255632	18.120730
38.581423	1675.897244	18.125747
38.711371	1680.204346	18.130765
38.694577	1668.450703	18.135783
38.444168	1664.998728	18.140800
38.752221	1687.181407	18.145818
39.219959	1691.492603	18.150835
39.475114	1704.386627	18.155853
39.302580	1684.475137	18.160871
39.377052	1698.357437	18.165888
39.360328	1692.227291	18.170906
39.478213	1697.305680	18.175923
39.409794	1697.885585	18.180941
40.004373	1695.580147	18.185959
39.537976	1681.038279	18.190976
39.516548	1664.847695	18.195994
39.424782	1662.607518	18.201011
38.993681	1675.116768	18.206029
39.573056	1675.155548	18.211047
39.628873	1692.476313	18.216064
39.419471	1691.185195	18.221082
39.181453	1696.012507	18.226099
39.600861	1701.302195	18.231117
39.841298	1696.391883	18.236135
39.851435	1699.852383	18.241152
39.752651	1696.469293	18.246170
39.722284	1693.503171	18.251187
39.587819	1689.117369	18.256205
39.979245	1681.740670	18.261223
39.669556	1692.669548	18.266240
39.825821	1708.348073	18.271258
39.968812	1711.036900	18.276275
39.904140	1722.172708	18.281293
40.141860	1717.561261	18.286311
39.976614	1726.073279	18.291328
40.004405	1718.063706	18.296346
40.719310	1716.147708	18.301363
40.183852	1715.846592	18.306381
40.529099	1709.051563	18.311399
40.412837	1721.327029	18.316416
40.380387	1721.199393	18.321434
40.302372	1713.719211	18.326451
40.226894	1715.127442	18.331469
40.260799	1715.996241	18.336487
40.393338	1725.928427	18.341504
40.541472	1720.506685	18.346522
40.739065	1725.449790	18.351539
41.002687	1736.660176	18.356557
41.256619	1719.899366	18.361575
40.979433	1709.270843	18.366592
41.081336	1701.007626	18.371610
41.336089	1703.057415	18.376627
41.199647	1703.255325	18.381645
41.452626	1690.168267	18.386663
41.178134	1705.376661	18.391680
41.258544	1702.943297	18.396698
41.277269	1700.394205	18.401715
41.385156	1704.708917	18.406733
41.419006	1698.658550	18.411751
41.044776	1698.517249	18.416768
41.378336	1703.386568	18.421786
41.622695	1698.266946	18.426803
41.193708	1699.289450	18.431821
41.434883	1700.585602	18.436839
41.267423	1695.900170	18.441856
41.193463	1691.507066	18.446874
41.450829	1694.371759	18.451891
41.352019	1703.755778	18.456909
41.448655	1694.880852	18.461927
41.258600	1707.879190	18.466944
41.190358	1699.277330	18.471962
41.321652	1706.641250	18.476979
41.573278	1716.930009	18.481997
41.816444	1718.075440	18.487015
41.865776	1724.852214	18.492032
41.693879	1729.435085	18.497050
41.942614	1729.782360	18.502067
41.673637	1742.361961	18.507085
41.928480	1737.909864	18.512103
41.495913	1734.168863	18.517120
41.418663	1736.987606	18.522138
41.552801	1738.132263	18.527155
41.879613	1751.000242	18.532173
41.890695	1756.211361	18.537191
41.972886	1757.126862	18.542208
41.916474	1769.432969	18.547226
42.051730	1760.608278	18.552243
41.909157	1771.687779	18.557261
42.249053	1771.097080	18.562279
42.645067	1787.652362	18.567296
42.438564	1790.238663	18.572314
42.721863	1790.100279	18.577331
42.602141	1788.836766	18.582349
43.068962	1785.004142	18.587367
42.696482	1774.567395	18.592384
42.396386	1758.222245	18.597402
42.864929	1767.059255	18.602419
42.637808	1787.515695	18.607437
43.034984	1781.622230	18.612455
43.107288	1792.109739	18.617472
43.184873	1768.175906	18.622490
43.166595	1758.032657	18.627507
42.975139	1760.737317	18.632525
42.881281	1744.474831	18.637543
42.980084	1753.325255	18.642560
42.682800	1749.906642	18.647578
43.205000	1761.794138	18.652595
43.019103	1774.537513	18.657613
43.037658	1778.611191	18.662631
43.233492	1781.449514	18.667648
43.224236	1785.329787	18.672666
43.337682	1777.722083	18.677683
42.919356	1784.865583	18.682701
42.969722	1777.663635	18.687719
43.265922	1783.443116	18.692736
43.369215	1795.357743	18.697754
43.798801	1789.697074	18.702771
43.741412	1798.070734	18.707789
43.822102	1802.854949	18.712807
43.960199	1792.592776	18.717824
44.021428	1786.757507	18.722842
44.047873	1767.418737	18.727859
43.862178	1766.485873	18.732877
44.086978	1761.087594	18.737895
43.888860	1755.104500	18.742912
44.074965	1764.727024	18.747930
44.021346	1763.569455	18.752947
44.002010	1766.170706	18.757965
43.944117	1758.437948	18.762983
44.017330	1776.778344	18.768000
44.204932	1792.091514	18.773018
44.528345	1794.518875	18.778035
44.142084	1801.774375	18.783053
44.029978	1795.334454	18.788071
43.979172	1792.779974	18.793088
44.169578	1802.252990	18.798106
44.486058	1792.268251	18.803123
44.264921	1806.837962	18.808141
44.762510	1799.365218	18.813159
44.592654	1791.302237	18.818176
44.362882	1790.945195	18.823194
44.851637	1792.401385	18.828211
44.170648	1803.141660	18.833229
44.667661	1800.998879	18.838247
44.596325	1813.315375	18.843264
44.544396	1829.967200	18.848282
45.091524	1824.466903	18.853299
45.162202	1827.232729	18.858317
45.013655	1830.488926	18.863335
44.873552	1819.996597	18.868352
44.794728	1828.381709	18.873370
45.209103	1821.264909	18.878387
44.899589	1826.184063	18.883405
45.197005	1831.399192	18.888423
45.060243	1818.710264	18.893440
45.237195	1830.427245	18.898458
45.592705	1821.149381	18.903475
45.270469	1811.285355	18.908493
45.298927	1815.953454	18.913511
45.756178	1817.401497	18.918528
45.438880	1816.608218	18.923546
46.093371	1808.227117	18.928563
45.641261	1810.844794	18.933581
45.485294	1806.564106	18.938599
45.837476	1808.058351	18.943616
45.458821	1812.379157	18.948634
45.752514	1804.138338	18.953651
45.702968	1809.221758	18.958669
45.528088	1810.041801	18.963687
45.907494	1813.577564	18.968704
45.801964	1807.676698	18.973722
45.558670	1820.483980	18.978739
45.704332	1818.497229	18.983757
45.941044	1831.340882	18.988775
46.165419	1823.087953	18.993792
46.361102	1823.933020	18.998810
46.185643	1830.723186	19.003827
46.022006	1835.833845	19.008845
45.986235	1837.235093	19.013863
45.982886	1837.256162	19.018880
45.893048	1841.320706	19.023898
46.468931	1848.278521	19.028915
46.412509	1860.278798	19.033933
46.490476	1870.463059	19.038951
46.924014	1856.917900	19.043968
46.522643	1868.595597	19.048986
46.701024	1865.099869	19.054003
46.969262	1857.870727	19.059021
46.974860	1852.930500	19.064039
46.933645	1846.346887	19.069056
46.532613	1859.102859	19.074074
46.847220	1853.235295	19.079091
47.194083	1854.199331	19.084109
46.989185	1855.619636	19.089127
47.105257	1851.995291	19.094144
46.728828	1854.848426	19.099162
46.759994	1854.139353	19.104179
46.855923	1853.341564	19.109197
47.042900	1852.101087	19.114215
47.024681	1866.695395	19.119232
47.085048	1872.989694	19.124250
47.280331	1882.718246	19.129267
47.272190	1880.769255	19.134285
47.070475	1891.689774	19.139303
47.599283	1878.944507	19.144320
47.200362	1893.593060	19.149338
47.099531	1882.480778	19.154355
46.913323	1906.828587	19.159373
47.271052	1906.607753	19.164391
47.592914	1906.620833	19.169408
47.650454	1916.244741	19.174426
47.792223	1901.378357	19.179443
47.758756	1909.155583	19.184461
47.798664	1910.797409	19.189479
48.100936	1911.527521	19.194496
48.197394	1924.891017	19.199514
48.413133	1926.863463	19.204531
48.289910	1918.802114	19.209549
47.916387	1909.927255	19.214567
48.564738	1915.321092	19.219584
48.471826	1923.402299	19.224602
48.684910	1907.753585	19.229619
48.809689	1903.671089	19.234637
48.290062	1900.989000	19.239655
48.377881	1901.022081	19.244672
48.315452	1907.481685	19.249690
48.123811	1902.181312	19.254707
48.579081	1906.961964	19.259725
48.745925	1925.087368	19.264743
49.132629	1930.944381	19.269760
48.501656	1931.130394	19.274778
48.774977	1920.024009	19.279795
48.635230	1928.085837	19.284813
48.707469	1934.854171	19.289831
49.094472	1937.712718	19.294848
49.049674	1930.508800	19.299866
49.003277	1926.681126	19.304883
48.999797	1937.087628	19.309901
48.731900	1931.142834	19.314919
49.171050	1925.654936	19.319936
49.028658	1929.130996	19.324954
49.438597	1916.018448	19.329971
49.599151	1918.528803	19.334989
49.282321	1920.198425	19.340007
49.843812	1908.554391	19.345024
49.615036	1921.956586	19.350042
49.581029	1915.909145	19.355059
49.668390	1914.409237	19.360077
49.576375	1921.448564	19.365095
49.873273	1910.591811	19.370112
49.569206	1916.476227	19.375130
49.433990	1910.987733	19.380147
49.569596	1916.285296	19.385165
49.360338	1916.665390	19.390183
49.696694	1931.330354	19.395200
49.729652	1942.549306	19.400218
50.037544	1938.270620	19.405235
50.186553	1950.635642	19.410253
49.844373	1949.967357	19.415271
50.067373	1947.946083	19.420288
49.919323	1950.123876	19.425306
50.285103	1939.624157	19.430323
50.315717	1936.889192	19.435341
50.123318	1944.191670	19.440359
50.605496	1949.909595	19.445376
50.321191	1957.363969	19.450394
50.500967	1962.901057	19.455411
50.805826	1970.859878	19.460429
50.915287	1962.613770	19.465447
51.052971	1949.803530	19.470464
50.795568	1931.136535	19.475482
50.846789	1940.468596	19.480499
50.753122	1927.092497	19.485517
50.726109	1931.774968	19.490535
50.573651	1944.450326	19.495552
50.933856	1956.724740	19.500570
51.257619	1956.095378	19.505587
51.394164	1948.512099	19.510605
51.162529	1956.375435	19.515623
51.515230	1952.008588	19.520640
51.471378	1964.060007	19.525658
51.274158	1957.020779	19.530675
51.324564	1944.988040	19.535693
51.129414	1955.821687	19.540711
51.458095	1954.744264	19.545728
51.298146	1958.079547	19.550746
51.054966	1962.426302	19.555763
51.839499	1955.354219	19.560781
51.283818	1963.675746	19.565799
51.397117	1955.982154	19.570816
51.753305	1953.016696	19.575834
51.461483	1954.030984	19.580851
51.563430	1940.618030	19.585869
51.549125	1958.512951	19.590887
51.732963	1980.498193	19.595904
51.953897	1990.204440	19.600922
51.785842	1981.946571	19.605939
51.902885	1980.676763	19.610957
51.945588	1984.134669	19.615975
52.120170	1985.128922	19.620992
52.299019	1984.435062	19.626010
52.171525	1982.202745	19.631027
52.326679	1981.440382	19.636045
52.115972	1984.329383	19.641063
51.901452	1974.854042	19.646080
52.413678	1988.847311	19.651098
52.258856	2000.647122	19.656115
52.463276	2006.408871	19.661133
52.397522	1997.531627	19.666151
52.769995	2001.409533	19.671168
52.810844	1998.763407	19.676186
52.700216	2002.490110	19.681203
52.847587	1995.695561	19.686221
53.212222	1994.897200	19.691239
53.110916	1998.186919	19.696256
53.143918	1994.380284	19.701274
53.034385	1989.125683	19.706291
53.321002	1991.626910	19.711309
53.063239	1998.328859	19.716327
52.934492	1997.995571	19.721344
53.143418	1988.018347	19.726362
53.110602	1995.762044	19.731379
53.272561	2001.879668	19.736397
53.325787	2020.906747	19.741415
53.488847	2029.493893	19.746432
53.804098	2021.716308	19.751450
53.708466	2029.777550	19.756467
53.716089	2026.225126	19.761485
53.484694	2034.673897	19.766503
53.614836	2029.156613	19.771520
53.875950	2031.146334	19.776538
53.827924	2031.058685	19.781555
53.816551	2020.637738	19.786573
53.796759	2034.112776	19.791591
53.757051	2031.290269	19.796608
54.212642	2026.695277	19.801626
54.007888	2020.880899	19.806643
54.113871	2022.363723	19.811661
53.760954	2025.856684	19.816679
53.794474	2033.678351	19.821696
53.838175	2048.357815	19.826714
53.808088	2067.564153	19.831731
53.935855	2059.279124	19.836749
53.731717	2076.086433	19.841767
54.020666	2086.196005	19.846784
54.201848	2098.840053	19.851802
54.311127	2093.738422	19.856819
55.041678	2106.408492	19.861837
55.031450	2101.254673	19.866855
55.375501	2100.456973	19.871872
55.332886	2077.209576	19.876890
54.890963	2085.044540	19.881907
54.883550	2080.401681	19.886925
55.090704	2078.842083	19.891943
55.383468	2079.356067	19.896960
55.447901	2081.723762	19.901978
55.224820	2087.439662	19.906995
55.054488	2079.443933	19.912013
55.104733	2091.529418	19.917031
55.216506	2072.781996	19.922048
55.543000	2082.352252	19.927066
55.479103	2087.212556	19.932083
55.738143	2079.615940	19.937101
55.393994	2074.911332	19.942119
55.555597	2076.797125	19.947136
55.672965	2091.272652	19.952154
55.763051	2098.699908	19.957171
55.923898	2093.771991	19.962189
55.718166	2095.801516	19.967207
56.055844	2098.615536	19.972224
55.945817	2093.788151	19.977242
55.672167	2103.546355	19.982259
56.085186	2084.199634	19.987277
56.124718	2092.464430	19.992295
55.701300	2094.222652	19.997312
56.154704	2088.811070	20.002330
55.982890	2092.928675	20.007347
56.454128	2099.013044	20.012365
56.214199	2098.741934	20.017383
56.314398	2108.035247	20.022400
56.607542	2109.249963	20.027418
56.436806	2119.689897	20.032435
56.919372	2114.344721	20.037453
56.984959	2116.555535	20.042471
56.886200	2116.300332	20.047488
57.031873	2108.900892	20.052506
56.757758	2117.450115	20.057523
56.793274	2117.156060	20.062541
56.592936	2114.194878	20.067559
56.335302	2116.555870	20.072576
56.469604	2110.149274	20.077594
56.898159	2121.700248	20.082611
56.988296	2137.327994	20.087629
57.045320	2138.188644	20.092647
57.189074	2148.020024	20.097664
57.613807	2151.358961	20.102682
57.433152	2141.811354	20.107699
57.807228	2137.229091	20.112717
57.848559	2137.356121	20.117735
57.417535	2149.996447	20.122752
57.468654	2137.839030	20.127770
57.564558	2150.459104	20.132787
57.573624	2141.856354	20.137805
57.709075	2137.848796	20.142823
57.400073	2144.822319	20.147840
57.789424	2152.112066	20.152858
57.767329	2164.939167	20.157875
58.308833	2166.433480	20.162893
58.094611	2173.045195	20.167911
58.294114	2175.764477	20.172928
58.700084	2170.609966	20.177946
58.621637	2165.998573	20.182963
58.956673	2158.816460	20.187981
58.351746	2139.217984	20.192999
58.868079	2150.202416	20.198016
58.827389	2127.219588	20.203034
58.770669	2132.345251	20.208051
58.797280	2122.624229	20.213069
58.888163	2118.023290	20.218087
58.712114	2120.276234	20.223104
58.730549	2113.711726	20.228122
58.662829	2110.674567	20.233139
58.804375	2135.632047	20.238157
59.210822	2146.310327	20.243175
58.922947	2152.784273	20.248192
59.376996	2148.318638	20.253210
59.290542	2150.426772	20.258227
59.230972	2150.320175	20.263245
59.416968	2154.088167	20.268263
58.809087	2150.103361	20.273280
59.747462	2148.418288	20.278298
59.222561	2149.537076	20.283315
59.013258	2152.833358	20.288333
59.503201	2149.054286	20.293351
59.464811	2152.827680	20.298368
59.247048	2143.156710	20.303386
59.478990	2138.108694	20.308403
59.363149	2146.863127	20.313421
59.462310	2162.507509	20.318439
59.412500	2167.986370	20.323456
59.869055	2164.182134	20.328474
59.673463	2168.984822	20.333491
59.412005	2174.586265	20.338509
59.805863	2190.016733	20.343527
59.890641	2208.035239	20.348544
60.264583	2203.029351	20.353562
60.064082	2205.083218	20.358579
60.408039	2206.671392	20.363597
60.200066	2197.128291	20.368615
59.966586	2213.178408	20.373632
60.351742	2219.512963	20.378650
60.737819	2218.084640	20.383667
61.041501	2235.177805	20.388685
60.945570	2229.998029	20.393703
61.102670	2228.846349	20.398720
61.209015	2209.096892	20.403738
61.584787	2197.182326	20.408755
61.402650	2187.008155	20.413773
61.510579	2183.639815	20.418791
61.437873	2178.924312	20.423808
61.673237	2174.108397	20.428826
61.703582	2172.419118	20.433843
61.572326	2175.558731	20.438861
61.633528	2168.817405	20.443879
61.753542	2179.608669	20.448896
61.546444	2169.691811	20.453914
61.679811	2175.530788	20.458931
61.856938	2167.911129	20.463949
62.043052	2167.047548	20.468967
61.750154	2149.927546	20.473984
61.659282	2149.814734	20.479002
61.325949	2157.036404	20.484019
61.108112	2171.985046	20.489037
61.712759	2171.413720	20.494055
61.312340	2173.638213	20.499072
61.534334	2183.349917	20.504090
61.884839	2204.944781	20.509107
61.773472	2202.143207	20.514125
61.913839	2193.556008	20.519143
61.725420	2206.906464	20.524160
62.561373	2209.541627	20.529178
62.244403	2223.163466	20.534195
62.435561	2229.939725	20.539213
62.708499	2227.405382	20.544231
62.554845	2230.098721	20.549248
62.500378	2225.441985	20.554266
62.416420	2236.499476	20.559283
62.150613	2231.175095	20.564301
62.602353	2245.183770	20.569319
62.466685	2261.055078	20.574336
62.770950	2256.896203	20.579354
63.138011	2245.770464	20.584371
63.046576	2253.514189	20.589389
63.340195	2251.479565	20.594407
63.457645	2248.968699	20.599424
63.611517	2240.613880	20.604442
63.400738	2242.955291	20.609459
63.387678	2250.050151	20.614477
63.493491	2245.432519	20.619495
63.330713	2243.805252	20.624512
63.459182	2242.106350	20.629530
63.308261	2249.253256	20.634547
63.263549	2266.425226	20.639565
63.753210	2279.644936	20.644583
63.584561	2279.590326	20.649600
63.974119	2272.582174	20.654618
64.029783	2271.368213	20.659635
63.876836	2280.948983	20.664653
63.879268	2273.484688	20.669671
64.057285	2286.801870	20.674688
64.385338	2291.809698	20.679706
64.676303	2290.616473	20.684723
64.634130	2296.618137	20.689741
64.719255	2279.735565	20.694759
64.380230	2286.020819	20.699776
64.797185	2273.476896	20.704794
64.598450	2277.941157	20.709811
64.217850	2296.284361	20.714829
64.661046	2286.638098	20.719847
64.392941	2304.846078	20.724864
64.836076	2293.381670	20.729882
64.923967	2283.768869	20.734899
64.775651	2296.518630	20.739917
65.055263	2280.376585	20.744935
65.166928	2296.499743	20.749952
65.182454	2310.897517	20.754970
65.330309	2317.073517	20.759987
65.294442	2314.157798	20.765005
65.513648	2318.551821	20.770023
65.582639	2324.523997	20.775040
65.746425	2317.386415	20.780058
65.822191	2321.688921	20.785075
65.889780	2316.733520	20.790093
66.094872	2310.678470	20.795111
65.779978	2323.692164	20.800128
65.900457	2318.821281	20.805146
66.235232	2313.012006	20.810163
65.933694	2320.113897	20.815181
66.032430	2310.305572	20.820199
65.718278	2319.011956	20.825216
65.769703	2323.903562	20.830234
65.865935	2311.203066	20.835251
65.740493	2331.314181	20.840269
66.033099	2334.642441	20.845287
66.372052	2346.697859	20.850304
66.204505	2335.736894	20.855322
66.488169	2336.380750	20.860339
66.417142	2344.395938	20.865357
66.718956	2357.332755	20.870375
66.559956	2355.705634	20.875392
66.777517	2369.917520	20.880410
66.737598	2361.678704	20.885427
66.634142	2380.309813	20.890445
67.237272	2367.741959	20.895463
67.388226	2372.091828	20.900480
67.302049	2374.410188	20.905498
67.152447	2365.229732	20.910515
67.122047	2371.538138	20.915533
67.342491	2367.056541	20.920551
67.542961	2387.426169	20.925568
67.817095	2393.917048	20.930586
68.117695	2386.729923	20.935603
67.563593	2374.431957	20.940621
67.400455	2364.749407	20.945639
67.758876	2383.919914	20.950656
67.748838	2388.983571	20.955674
68.110158	2393.894168	20.960691
67.706989	2397.397136	20.965709
67.966508	2390.059353	20.970727
67.679697	2392.987849	20.975744
67.589503	2393.435567	20.980762
67.681045	2388.480493	20.985779
67.910556	2418.331817	20.990797
68.105916	2420.659300	20.995815
67.992242	2420.391609	21.000832
68.571859	2425.947059	21.005850
68.772653	2406.036769	21.010867
68.664066	2421.617512	21.015885
68.734990	2417.658010	21.020903
68.941826	2414.379484	21.025920
68.659076	2422.294857	21.030938
69.179318	2434.091859	21.035955
69.088735	2439.901619	21.040973
69.156631	2443.079448	21.045991
69.147754	2433.967298	21.051008
69.250927	2440.040534	21.056026
69.357462	2434.016778	21.061043
69.198340	2446.579082	21.066061
69.059732	2440.475196	21.071079
69.328047	2449.418716	21.076096
69.262265	2443.437770	21.081114
69.740173	2440.429157	21.086131
69.390461	2443.155117	21.091149
69.581486	2445.687267	21.096167
69.816012	2468.899068	21.101184
69.361274	2474.446517	21.106202
70.034540	2467.367110	21.111219
69.856641	2473.358328	21.116237
69.858016	2470.678523	21.121255
69.882753	2476.216759	21.126272
69.729372	2478.804974	21.131290
70.535599	2492.160055	21.136307
70.247933	2496.059217	21.141325
70.670265	2498.311980	21.146343
70.871258	2494.339503	21.151360
71.040276	2490.105009	21.156378
71.211836	2469.923897	21.161395
71.442224	2476.169711	21.166413
71.587769	2454.974403	21.171431
71.584708	2441.507601	21.176448
71.111281	2444.484050	21.181466
71.300831	2424.740177	21.186483
71.235645	2444.596141	21.191501
71.508639	2439.135288	21.196519
71.276610	2429.088151	21.201536
71.518892	2433.550028	21.206554
71.676438	2426.961481	21.211571
71.626705	2436.137779	21.216589
71.782045	2437.030140	21.221607
72.080916	2434.383971	21.226624
71.476852	2437.915612	21.231642
71.791226	2438.521297	21.236659
71.661400	2436.616870	21.241677
71.751797	2436.265261	21.246695
71.579829	2442.819279	21.251712
71.474069	2447.110256	21.256730
72.073123	2453.158958	21.261747
71.678539	2473.247663	21.266765
71.642733	2465.141971	21.271783
71.705745	2462.668467	21.276800
71.908933	2480.839664	21.281818
72.069542	2487.756550	21.286835
71.903977	2495.432792	21.291853
72.093130	2503.033547	21.296871
72.040664	2495.339284	21.301888
71.959771	2515.755055	21.306906
72.564875	2518.051857	21.311923
72.404166	2524.737113	21.316941
72.360033	2519.697455	21.321959
72.708486	2539.344632	21.326976
72.849638	2541.998477	21.331994
72.968848	2539.058910	21.337011
72.583330	2554.638959	21.342029
73.310468	2557.322193	21.347047
73.468237	2553.582485	21.352064
73.194958	2557.642662	21.357082
73.491953	2561.981699	21.362099
73.640490	2576.049334	21.367117
73.668401	2572.321754	21.372135
74.144909	2577.184919	21.377152
74.008820	2569.166709	21.382170
74.014068	2570.169065	21.387187
74.098263	2570.302361	21.392205
73.976457	2566.749277	21.397223
73.961010	2561.542627	21.402240
73.861194	2570.195417	21.407258
74.219752	2561.166619	21.412275
74.229743	2566.443549	21.417293
73.973837	2562.642663	21.422311
74.465760	2577.579250	21.427328
74.373868	2592.371530	21.432346
74.520313	2590.828272	21.437363
74.328668	2609.363283	21.442381
74.107952	2599.361008	21.447399
74.568132	2600.631866	21.452416
74.854264	2607.744882	21.457434
75.280712	2615.875177	21.462451
75.551636	2612.605645	21.467469
76.205075	2591.989154	21.472487
76.646064	2574.273072	21.477504
76.192017	2577.471531	21.482522
76.466800	2567.082583	21.487539
76.424318	2539.802030	21.492557
76.230305	2537.727149	21.497575
76.405755	2523.756575	21.502592
76.037527	2522.678795	21.507610
76.206092	2491.442244	21.512627
76.114299	2498.443606	21.517645
75.933889	2494.542391	21.522663
76.355604	2487.881567	21.527680
75.919039	2493.882711	21.532698
76.052745	2483.307809	21.537715
75.974042	2496.900130	21.542733
75.898024	2515.975282	21.547751
76.339887	2513.806928	21.552768
76.062374	2522.682145	21.557786
76.301049	2518.293149	21.562803
76.348268	2527.015183	21.567821
76.078538	2531.421233	21.572839
76.380577	2544.680623	21.577856
76.411763	2555.729047	21.582874
76.741500	2559.494510	21.587891
76.591012	2556.099744	21.592909
76.581897	2576.317438	21.597927
76.902927	2586.272396	21.602944
76.634851	2587.852483	21.607962
77.122756	2584.374448	21.612979
76.852182	2584.963178	21.617997
76.811699	2604.317189	21.623015
77.330026	2616.189850	21.628032
77.156672	2622.925283	21.633050
77.611045	2615.179404	21.638067
77.563527	2617.176401	21.643085
77.627771	2617.296084	21.648103
77.835368	2612.562999	21.653120
77.544092	2627.005757	21.658138
78.040451	2628.233595	21.663155
78.014388	2640.701497	21.668173
77.831932	2644.035154	21.673191
78.453341	2637.579672	21.678208
78.199205	2646.687698	21.683226
78.465807	2639.784861	21.688243
78.653503	2632.732142	21.693261
78.090390	2644.857001	21.698279
78.537471	2626.196105	21.703296
78.758454	2660.079014	21.708314
78.560275	2667.177662	21.713331
78.616737	2668.264431	21.718349
78.525805	2663.452199	21.723367
78.652026	2665.496315	21.728384
78.756880	2670.942955	21.733402
78.815717	2679.892682	21.738419
79.169136	2685.350775	21.743437
79.084316	2698.976574	21.748455
79.398744	2684.559116	21.753472
79.539548	2690.932509	21.758490
79.610760	2685.589362	21.763507
79.548607	2689.066428	21.768525
79.778180	2694.336830	21.773543
79.879394	2707.210030	21.778560
79.840947	2711.380045	21.783578
79.974114	2715.953844	21.788595
80.046643	2717.849402	21.793613
79.991534	2717.338102	21.798631
80.130243	2721.792472	21.803648
79.795583	2715.368288	21.808666
80.179248	2714.480508	21.813683
80.577610	2719.660265	21.818701
80.541417	2741.110292	21.823719
80.901087	2733.919886	21.828736
80.926678	2744.852045	21.833754
80.961278	2732.900462	21.838771
80.936500	2734.507455	21.843789
81.148303	2728.500344	21.848807
80.958590	2726.906243	21.853824
81.042592	2730.520453	21.858842
80.920639	2733.231444	21.863859
81.281239	2719.220475	21.868877
81.083076	2732.338736	21.873895
81.175806	2730.687062	21.878912
81.159042	2741.165212	21.883930
81.422914	2754.323245	21.888947
81.574558	2764.650974	21.893965
81.511616	2767.093490	21.898983
81.496422	2765.640861	21.904000
81.738971	2772.267077	21.909018
81.563294	2786.973462	21.914035
82.077848	2789.621201	21.919053
81.766312	2803.232798	21.924071
81.888901	2794.546250	21.929088
82.301865	2796.074199	21.934106
81.849418	2796.188017	21.939123
82.487687	2811.009558	21.944141
82.597646	2820.823358	21.949159
82.919241	2822.299956	21.954176
82.842170	2830.867216	21.959194
82.665144	2823.736830	21.964211
82.826956	2815.475665	21.969229
82.999204	2822.922292	21.974247
83.040064	2820.270513	21.979264
82.850959	2819.024745	21.984282
83.016465	2817.266474	21.989299
83.390446	2834.565166	21.994317
83.353301	2838.990524	21.999335
83.734972	2844.957394	22.004352
83.909316	2845.408801	22.009370
83.708796	2850.632618	22.014387
83.893150	2843.876440	22.019405
83.971767	2846.100942	22.024423
84.035939	2839.965560	22.029440
84.168426	2837.614709	22.034458
83.768053	2844.782477	22.039475
83.895353	2825.775649	22.044493
83.791008	2830.457856	22.049511
83.999194	2829.938230	22.054528
83.844658	2844.126953	22.059546
84.194538	2857.193216	22.064563
84.468375	2863.538271	22.069581
84.675419	2872.071722	22.074599
84.759337	2866.582692	22.079616
84.892183	2869.420662	22.084634
84.554001	2866.407042	22.089651
84.633209	2862.642125	22.094669
84.499639	2878.494421	22.099687
84.642580	2879.407374	22.104704
84.935847	2887.197327	22.109722
84.527045	2885.483705	22.114739
84.922711	2898.584521	22.119757
85.166226	2907.894261	22.124775
85.612098	2905.102712	22.129792
85.590522	2912.999336	22.134810
85.463928	2915.733573	22.139827
85.718333	2920.642423	22.144845
85.771148	2934.262089	22.149863
85.822222	2938.423193	22.154880
85.941769	2945.492393	22.159898
85.810147	2945.654867	22.164915
86.275715	2946.772095	22.169933
86.350438	2946.301026	22.174951
86.505999	2959.616219	22.179968
86.910914	2955.845577	22.184986
87.043524	2963.182316	22.190003
86.953792	2941.900638	22.195021
86.873213	2930.627930	22.200039
86.838886	2935.876914	22.205056
87.162284	2945.777376	22.210074
87.205045	2949.162650	22.215091
87.226899	2945.381653	22.220109
87.113113	2957.679730	22.225127
87.435450	2952.313261	22.230144
87.258696	2953.360457	22.235162
87.417366	2960.372765	22.240179
87.597296	2949.501265	22.245197
87.404861	2951.700746	22.250215
87.705054	2955.372786	22.255232
87.605945	2953.073007	22.260250
87.624778	2968.516183	22.265267
87.874140	2975.658317	22.270285
87.833850	2983.256494	22.275303
88.216979	2976.204607	22.280320
88.277888	2978.198985	22.285338
88.215644	2973.850424	22.290355
88.350284	2969.197078	22.295373
88.458719	2991.514415	22.300391
88.400730	2996.000373	22.305408
88.182825	3003.997394	22.310426
88.155959	3011.313806	22.315443
88.464617	3015.215178	22.320461
88.395705	3030.837970	22.325479
88.328061	3040.719617	22.330496
88.803910	3050.148715	22.335514
89.037019	3042.120874	22.340531
89.127254	3043.938721	22.345549
89.318358	3065.490405	22.350567
89.533611	3067.325669	22.355584
89.625427	3071.206002	22.360602
89.530041	3076.316746	22.365619
90.016586	3066.678945	22.370637
89.717752	3076.941974	22.375655
89.928013	3068.194244	22.380672
90.048489	3068.448690	22.385690
90.198236	3072.430033	22.390707
90.124526	3062.209706	22.395725
90.443196	3069.413598	22.400743
89.936782	3067.208661	22.405760
90.325570	3069.100131	22.410778
90.291974	3083.110693	22.415795
90.663262	3084.138869	22.420813
90.808367	3091.652346	22.425831
90.993623	3091.182983	22.430848
90.764817	3084.170144	22.435866
90.317368	3097.369907	22.440883
91.011705	3100.520145	22.445901
91.014123	3115.681922	22.450919
91.237762	3120.098668	22.455936
91.258358	3121.408768	22.460954
90.926754	3125.282313	22.465971
91.302392	3122.587050	22.470989
91.612287	3136.086209	22.476007
91.713918	3141.970198	22.481024
92.009334	3143.977990	22.486042
91.686957	3147.878749	22.491059
91.985551	3145.388427	22.496077
91.887338	3153.508163	22.501095
92.072050	3150.680834	22.506112
92.035650	3146.970498	22.511130
91.778929	3164.420048	22.516147
92.126084	3180.050619	22.521165
92.011148	3181.348994	22.526183
92.298922	3183.473425	22.531200
92.569030	3186.576459	22.536218
92.725630	3203.737266	22.541235
92.882988	3201.922429	22.546253
93.330353	3201.675271	22.551271
93.015988	3202.983955	22.556288
93.069802	3196.947013	22.561306
93.177917	3196.830651	22.566323
93.127657	3196.290181	22.571341
93.548502	3220.306458	22.576359
93.482855	3224.611456	22.581376
94.043173	3211.149580	22.586394
94.107530	3217.794577	22.591411
94.044737	3214.273272	22.596429
94.310587	3217.463248	22.601447
93.803123	3220.968372	22.606464
94.364466	3218.372163	22.611482
94.372836	3214.009830	22.616499
94.401836	3208.317980	22.621517
94.390970	3209.857349	22.626535
94.509656	3218.877367	22.631552
94.767829	3208.229711	22.636570
94.766131	3211.160976	22.641587
94.670740	3198.445932	22.646605
94.676395	3218.572232	22.651623
95.026084	3229.416614	22.656640
95.448125	3227.112474	22.661658
95.297769	3232.087117	22.666675
95.250979	3228.834824	22.671693
95.638306	3229.457557	22.676711
95.151838	3239.352237	22.681728
95.664236	3222.726796	22.686746
95.332097	3227.716293	22.691763
95.565985	3231.577779	22.696781
95.625508	3230.263489	22.701799
95.434032	3233.225510	22.706816
95.568731	3245.686471	22.711834
95.940493	3259.705421	22.716851
95.960135	3254.819113	22.721869
96.305418	3248.144686	22.726887
96.120151	3250.930861	22.731904
96.413408	3255.584522	22.736922
96.879664	3259.205413	22.741939
97.216170	3257.235983	22.746957
97.350731	3258.445258	22.751975
97.147282	3242.929003	22.756992
97.284625	3234.192511	22.762010
97.398377	3225.539084	22.767027
97.988250	3211.892361	22.772045
98.605225	3201.441793	22.777063
98.594954	3204.309122	22.782080
98.578629	3177.184142	22.787098
98.458323	3170.057162	22.792115
98.567081	3163.239388	22.797133
98.479090	3156.820878	22.802151
98.396963	3165.078509	22.807168
98.446423	3138.896280	22.812186
98.207732	3123.601370	22.817203
98.479281	3130.901319	22.822221
98.519158	3123.376845	22.827239
98.302860	3126.690635	22.832256
98.346895	3121.143966	22.837274
98.150583	3141.297828	22.842291
98.225569	3163.680819	22.847309
98.618399	3164.572734	22.852327
98.177443	3161.536368	22.857344
98.855806	3178.432076	22.862362
98.599407	3193.470000	22.867379
98.754024	3206.322139	22.872397
98.827029	3197.637308	22.877415
98.524777	3210.826816	22.882432
98.916430	3204.906180	22.887450
99.160183	3232.673073	22.892467
98.792846	3231.124186	22.897485
99.215666	3251.532411	22.902503
98.884346	3268.644840	22.907520
99.376425	3285.368850	22.912538
99.323782	3295.441095	22.917555
99.334497	3302.171428	22.922573
99.735310	3311.667886	22.927591
99.775226	3328.601745	22.932608
100.185822	3323.278757	22.937626
100.368828	3337.378364	22.942643
100.501220	3343.788466	22.947661
100.877318	3348.388227	22.952679
100.737428	3353.419836	22.957696
100.714990	3346.063105	22.962714
100.882591	3348.162646	22.967731
100.885892	3347.021484	22.972749
101.442446	3348.533109	22.977767
101.253128	3368.275040	22.982784
101.519998	3372.803189	22.987802
101.984659	3363.897650	22.992819
102.103680	3368.598807	22.997837
102.423340	3338.675731	23.002855
101.844108	3335.620573	23.007872
101.836044	3332.275594	23.012890
102.050106	3339.444632	23.017907
101.712129	3342.753096	23.022925
101.956785	3354.511558	23.027943
102.105936	3364.506606	23.032960
102.047960	3368.648150	23.037978
102.280392	3363.902837	23.042995
102.326150	3377.081110	23.048013
102.424208	3389.981780	23.053031
102.262713	3400.362761	23.058048
102.458253	3395.793271	23.063066
102.436105	3409.331313	23.068083
102.750149	3422.624895	23.073101
103.211019	3419.469708	23.078119
103.417495	3426.352224	23.083136
103.760310	3416.754240	23.088154
103.463954	3423.543531	23.093171
103.351106	3425.488490	23.098189
104.021186	3425.036192	23.103207
103.674363	3451.932240	23.108224
103.999832	3441.551615	23.113242
104.046497	3453.993118	23.118259
103.755016	3458.171522	23.123277
104.266181	3447.273372	23.128295
104.093843	3459.114994	23.133312
104.110614	3468.133194	23.138330
104.243817	3471.089731	23.143347
104.234625	3482.829054	23.148365
104.836585	3471.283453	23.153383
104.664303	3488.451588	23.158400
104.943009	3503.711541	23.163418
105.460298	3504.556807	23.168435
105.288625	3509.974494	23.173453
105.648970	3505.344116	23.178471
105.397021	3501.523439	23.183488
105.695741	3503.974476	23.188506
105.640842	3492.943574	23.193523
105.498021	3500.498799	23.198541
105.702222	3489.817398	23.203559
105.737071	3515.387009	23.208576
105.890584	3521.961802	23.213594
105.957548	3529.440047	23.218611
106.097841	3532.802151	23.223629
106.121334	3524.312788	23.228647
106.273549	3532.218249	23.233664
106.521381	3551.912173	23.238682
106.735291	3545.945351	23.243699
106.648821	3551.226438	23.248717
106.683085	3544.566957	23.253735
106.665363	3564.771218	23.258752
106.675599	3562.358285	23.263770
107.152890	3581.463269	23.268787
107.088696	3583.878558	23.273805
107.640746	3572.186831	23.278823
107.399483	3578.598885	23.283840
107.678019	3581.386787	23.288858
108.195628	3594.814815	23.293875
108.300471	3604.128726	23.298893
108.201528	3589.140879	23.303911
108.068797	3584.588090	23.308928
108.031012	3602.076554	23.313946
108.204870	3601.074369	23.318963
107.931235	3610.362197	23.323981
108.294699	3599.105377	23.328999
108.522282	3598.217112	23.334016
108.614016	3612.746353	23.339034
108.669890	3617.604946	23.344051
108.527498	3630.238261	23.349069
109.075688	3622.808619	23.354087
109.369301	3633.963424	23.359104
109.384201	3621.935292	23.364122
109.370322	3619.122378	23.369139
109.362531	3627.783690	23.374157
109.582816	3617.258602	23.379175
109.604945	3627.076088	23.384192
109.942008	3631.942686	23.389210
109.867587	3639.343682	23.394227
110.130419	3644.597069	23.399245
110.205952	3634.318490	23.404263
110.348150	3647.217944	23.409280
110.196713	3642.666672	23.414298
110.255144	3636.327579	23.419315
110.352933	3642.958539	23.424333
110.718033	3659.480410	23.429351
110.440588	3664.663731	23.434368
110.261796	3679.586850	23.439386
110.763092	3666.796673	23.444403
110.698974	3684.697524	23.449421
111.117318	3693.467209	23.454439
110.954852	3693.205239	23.459456
110.989829	3702.343397	23.464474
111.398874	3708.645462	23.469491
111.376668	3721.633723	23.474509
111.891377	3725.781774	23.479527
111.744951	3730.192077	23.484544
111.500459	3732.573171	23.489562
111.957698	3735.272735	23.494579
112.182696	3751.684113	23.499597
112.279999	3749.818163	23.504615
112.250878	3756.406082	23.509632
112.265939	3751.141203	23.514650
112.637310	3756.893973	23.519667
112.618299	3774.594101	23.524685
113.209087	3776.837570	23.529703
113.017020	3776.523425	23.534720
113.095333	3785.598912	23.539738
113.165130	3776.051200	23.544755
113.247719	3778.329513	23.549773
113.303752	3773.716555	23.554791
113.403570	3791.285524	23.559808
113.636409	3806.327385	23.564826
113.600765	3797.323624	23.569843
113.592210	3808.415764	23.574861
114.127070	3807.835520	23.579879
114.309943	3821.842664	23.584896
113.992965	3834.374433	23.589914
114.593538	3835.492134	23.594931
114.509543	3844.022906	23.599949
114.698379	3837.213188	23.604967
114.909964	3833.512663	23.609984
114.859228	3838.140193	23.615002
115.032472	3832.985629	23.620019
115.006879	3841.551188	23.625037
115.127062	3843.550789	23.630055
115.514607	3849.327681	23.635072
115.417986	3855.015725	23.640090
115.746071	3845.799501	23.645107
115.673221	3846.040415	23.650125
115.756891	3852.731692	23.655143
115.818163	3845.277341	23.660160
115.781315	3843.828210	23.665178
116.233973	3855.718252	23.670195
116.022869	3871.506083	23.675213
116.500683	3872.983206	23.680231
116.293534	3877.683991	23.685248
116.432617	3877.479792	23.690266
116.652266	3870.479483	23.695283
116.681412	3870.939696	23.700301
116.524310	3872.732989	23.705319
116.597939	3885.085698	23.710336
116.463944	3902.499530	23.715354
117.093713	3900.156050	23.720371
116.790928	3904.550255	23.725389
116.912085	3928.958418	23.730407
117.398485	3931.443697	23.735424
117.482871	3943.420601	23.740442
118.092504	3940.701673	23.745459
117.676907	3936.738772	23.750477
117.946089	3940.352415	23.755495
118.235419	3954.836537	23.760512
118.100781	3957.618359	23.765530
118.082152	3951.811696	23.770547
118.326795	3968.403525	23.775565
118.655689	3968.162663	23.780583
118.869843	3978.409148	23.785600
118.355497	3990.317850	23.790618
118.874409	3987.810867	23.795635
118.596313	3992.050974	23.800653
118.928046	4010.117938	23.805671
118.911322	4014.161839	23.810688
119.036903	4015.628999	23.815706
119.519861	4023.338388	23.820723
119.519171	4051.173347	23.825741
119.610061	4041.516049	23.830759
119.895811	4043.594869	23.835776
119.789175	4040.888250	23.840794
120.307367	4059.541690	23.845811
120.240782	4067.801544	23.850829
120.400674	4062.504223	23.855847
120.899528	4058.234970	23.860864
120.774461	4065.937930	23.865882
120.615444	4056.615106	23.870899
120.566868	4066.884835	23.875917
121.237222	4081.409706	23.880935
121.372562	4078.284470	23.885952
121.150718	4090.591943	23.890970
121.176373	4088.062965	23.895987
121.368069	4081.709028	23.901005
121.620886	4102.165520	23.906023
121.497612	4099.189966	23.911040
121.475934	4112.650181	23.916058
122.154290	4112.190197	23.921075
121.894703	4114.808927	23.926093
122.102740	4140.698858	23.931111
122.390308	4131.751837	23.936128
122.361505	4139.447104	23.941146
122.443060	4129.923605	23.946163
122.634659	4142.507734	23.951181
122.807948	4149.715028	23.956199
123.101461	4164.881029	23.961216
123.200009	4168.143107	23.966234
123.466780	4158.544710	23.971251
123.431036	4165.930470	23.976269
123.215461	4168.735229	23.981287
123.721401	4161.386778	23.986304
123.480357	4176.029728	23.991322
123.732574	4184.663495	23.996339
124.122534	4197.639569	24.001357
123.936125	4199.561015	24.006375
124.458823	4191.663230	24.011392
124.462679	4197.006700	24.016410
124.302395	4190.871864	24.021427
124.401565	4194.786300	24.026445
124.646839	4217.762275	24.031463
124.865161	4215.336317	24.036480
125.073359	4211.691788	24.041498
124.891828	4215.455604	24.046515
125.149999	4219.210927	24.051533
125.327382	4213.531459	24.056551
125.492763	4207.566939	24.061568
125.709258	4218.102604	24.066586
126.062827	4233.996594	24.071603
125.826416	4234.928964	24.076621
125.842443	4249.537136	24.081639
126.410352	4235.246236	24.086656
126.165326	4236.810051	24.091674
125.697515	4236.136542	24.096691
125.879106	4236.819894	24.101709
125.816897	4259.145351	24.106727
126.292552	4261.072151	24.111744
126.071938	4284.882452	24.116762
126.478086	4296.586043	24.121779
126.374960	4295.878703	24.126797
126.640858	4322.004630	24.131815
126.997824	4327.342228	24.136832
127.067747	4338.948159	24.141850
127.692298	4351.896008	24.146867
127.659308	4358.611220	24.151885
127.745927	4357.022607	24.156903
127.949685	4345.461825	24.161920
128.261171	4356.019598	24.166938
128.750159	4353.997133	24.171955
128.479929	4353.618393	24.176973
128.306435	4360.166374	24.181991
128.748476	4372.590942	24.187008
128.638435	4380.766435	24.192026
128.600638	4380.114386	24.197043
128.943460	4387.461752	24.202061
128.805970	4386.909748	24.207079
129.373336	4398.933923	24.212096
129.056494	4407.395805	24.217114
129.037693	4418.406995	24.222131
129.373951	4426.783979	24.227149
129.777205	4441.613064	24.232167
130.100450	4442.639873	24.237184
130.031522	4438.201841	24.242202
130.163815	4438.429542	24.247219
130.265990	4436.840699	24.252237
130.193248	4449.646198	24.257255
130.492963	4454.160937	24.262272
130.493284	4461.039188	24.267290
130.932808	4473.464254	24.272307
130.914859	4466.942606	24.277325
131.112865	4463.783255	24.282343
131.204656	4471.558267	24.287360
131.335350	4490.134863	24.292378
131.438521	4480.031088	24.297395
131.727846	4491.374651	24.302413
131.380519	4493.791060	24.307431
131.791812	4504.089001	24.312448
131.833946	4510.352351	24.317466
131.802960	4509.572373	24.322483
132.170240	4508.533265	24.327501
131.931761	4525.960819	24.332519
132.244704	4534.641785	24.337536
132.125503	4544.909781	24.342554
132.406918	4544.354309	24.347571
132.592688	4565.788457	24.352589
132.821994	4571.895510	24.357607
132.706042	4565.138098	24.362624
133.092013	4578.777073	24.367642
133.242348	4597.532452	24.372659
133.691301	4590.904811	24.377677
133.370049	4613.679399	24.382695
133.556071	4598.108887	24.387712
133.931807	4603.691534	24.392730
133.930573	4621.207349	24.397747
134.437887	4631.889486	24.402765
134.171899	4639.081407	24.407783
134.257238	4626.380056	24.412800
134.701591	4631.822155	24.417818
134.491447	4629.560661	24.422835
134.520804	4645.630228	24.427853
134.566168	4661.970427	24.432871
134.673444	4665.076801	24.437888
134.897971	4683.843580	24.442906
135.195556	4693.190294	24.447923
135.396832	4690.179988	24.452941
135.338267	4699.018863	24.457959
135.783764	4710.057055	24.462976
135.879355	4727.684479	24.467994
136.126301	4720.128767	24.473011
136.379859	4716.248985	24.478029
135.949082	4725.025298	24.483047
136.254944	4744.765422	24.488064
136.507149	4745.166148	24.493082
136.563399	4747.241463	24.498099
136.986346	4744.042314	24.503117
137.309632	4759.678832	24.508135
137.747553	4755.134432	24.513152
138.073592	4755.455160	24.518170
138.023010	4754.424837	24.523187
138.060509	4749.560297	24.528205
138.200219	4755.440535	24.533223
138.054581	4756.075122	24.538240
138.282223	4750.701733	24.543258
137.942895	4759.448692	24.548275
137.932112	4749.392820	24.553293
137.904975	4759.975637	24.558311
138.230805	4780.359061	24.563328
138.211811	4790.706645	24.568346
138.645662	4801.567279	24.573363
138.941838	4809.875526	24.578381
138.929412	4819.825115	24.583399
139.160868	4816.319128	24.588416
138.926781	4825.484147	24.593434
139.457783	4838.199083	24.598451
139.972888	4831.053170	24.603469
139.999123	4851.217919	24.608487
140.459122	4837.754007	24.613504
140.938985	4833.370363	24.618522
140.516137	4832.343619	24.623539
140.679060	4824.711252	24.628557
141.012035	4820.902515	24.633575
141.246164	4821.311760	24.638592
141.583725	4814.377282	24.643610
141.379960	4816.131181	24.648627
141.652988	4804.421518	24.653645
141.533332	4814.732294	24.658663
141.719267	4818.735242	24.663680
141.730665	4814.562547	24.668698
141.872098	4813.378241	24.673715
141.993872	4829.557859	24.678733
141.798806	4839.470870	24.683751
142.064406	4856.215700	24.688768
141.977169	4843.839757	24.693786
141.893001	4849.108297	24.698803
142.226474	4861.745033	24.703821
141.947654	4880.398807	24.708839
142.082747	4875.443980	24.713856
142.068506	4893.239477	24.718874
142.236273	4909.482413	24.723891
142.578454	4906.379345	24.728909
142.892117	4932.472364	24.733927
142.786417	4935.013283	24.738944
143.590403	4943.711321	24.743962
143.378567	4968.519811	24.748979
143.595946	4965.013768	24.753997
143.622272	4973.575648	24.759015
143.952184	4991.932294	24.764032
144.104104	5000.022048	24.769050
144.107414	4994.728384	24.774067
144.403841	5009.997103	24.779085
144.592918	5025.805825	24.784103
144.657977	5010.716515	24.789120
144.722201	5016.001403	24.794138
145.676655	5034.966265	24.799155
146.089717	5028.308181	24.804173
145.940558	5031.400538	24.809191
146.582293	5027.975961	24.814208
146.353386	5013.034732	24.819226
146.591665	5005.576406	24.824243
146.722037	4991.218137	24.829261
146.419065	4983.710368	24.834279
146.525131	4991.528156	24.839296
146.771548	5000.084978	24.844314
146.670248	5008.375902	24.849331
146.802487	5010.300015	24.854349
147.035406	5015.739583	24.859367
147.061751	5016.631483	24.864384
147.146568	5014.604436	24.869402
146.953082	5043.452517	24.874419
147.474050	5039.560509	24.879437
147.582089	5059.995453	24.884455
147.591998	5060.947578	24.889472
147.984975	5075.809688	24.894490
148.088464	5074.157559	24.899507
147.979130	5078.375816	24.904525
148.271008	5091.948183	24.909543
148.374927	5105.888084	24.914560
148.563573	5093.373167	24.919578
148.468120	5123.378567	24.924595
148.787190	5138.113620	24.929613
149.088514	5139.286670	24.934631
149.010634	5144.895277	24.939648
149.564731	5153.881466	24.944666
149.515973	5167.919249	24.949683
150.076538	5163.922186	24.954701
149.958867	5164.845902	24.959719
149.828202	5173.991573	24.964736
150.031551	5185.384581	24.969754
149.946771	5201.446906	24.974771
150.437790	5195.489330	24.979789
150.352017	5219.108520	24.984807
150.639787	5235.090069	24.989824
150.795349	5221.109376	24.994842
150.861234	5239.488135	24.999859
151.125872	5257.076249	25.004877
151.070449	5258.597627	25.009895
151.422576	5269.436727	25.014912
151.683328	5282.721456	25.019930
151.638830	5295.081910	25.024947
151.958803	5294.442826	25.029965
152.129630	5293.324482	25.034983
152.141964	5310.987661	25.040000
152.407085	5319.883355	25.045018
152.789235	5324.413790	25.050035
153.336790	5304.153950	25.055053
153.318628	5306.550433	25.060071
153.282726	5306.523360	25.065088
153.485401	5295.054996	25.070106
153.143448	5303.593197	25.075123
153.406951	5305.388424	25.080141
153.537859	5309.335274	25.085159
153.442979	5315.856411	25.090176
153.824548	5310.759681	25.095194
153.593229	5341.500037	25.100211
154.154670	5354.987670	25.105229
153.986856	5360.216725	25.110247
154.198829	5369.062998	25.115264
154.517605	5387.444011	25.120282
154.502762	5391.181193	25.125299
154.903057	5383.833591	25.130317
155.438155	5399.022075	25.135335
155.418776	5399.757779	25.140352
156.046790	5396.794563	25.145370
156.183283	5399.607976	25.150387
156.432132	5385.711657	25.155405
156.950339	5391.462294	25.160423
157.144177	5378.738370	25.165440
157.370374	5375.913598	25.170458
157.069716	5376.972481	25.175475
157.225261	5378.315476	25.180493
157.353490	5374.860386	25.185511
157.482056	5377.901147	25.190528
157.412220	5370.680505	25.195546
157.595710	5368.222753	25.200563
157.668618	5366.092105	25.205581
157.731135	5364.097860	25.210599
157.649217	5375.818786	25.215616
158.087150	5359.233009	25.220634
157.516541	5381.672895	25.225651
157.469327	5393.049410	25.230669
158.227887	5402.522355	25.235687
157.877425	5426.485119	25.240704
158.158928	5433.507663	25.245722
158.005320	5446.510127	25.250739
158.444674	5461.535802	25.255757
158.610556	5482.253874	25.260775
158.484404	5504.300318	25.265792
158.904415	5510.094095	25.270810
158.920699	5529.417081	25.275827
159.185479	5543.625982	25.280845
159.632659	5559.539630	25.285863
159.779175	5568.513456	25.290880
159.982862	5584.509333	25.295898
159.705404	5589.588927	25.300915
160.210315	5606.583046	25.305933
160.694203	5620.075920	25.310951
160.474848	5632.993378	25.315968
160.571418	5634.828198	25.320986
160.764650	5656.474455	25.326003
161.123591	5655.746974	25.331021
161.684631	5668.290628	25.336039
161.821572	5686.360393	25.341056
161.818313	5676.685447	25.346074
162.089562	5683.648376	25.351091
162.216911	5691.406269	25.356109
162.562309	5701.965618	25.361127
162.989946	5715.969617	25.366144
163.192491	5699.939259	25.371162
163.415306	5695.879265	25.376179
163.249032	5696.213307	25.381197
163.646185	5695.568472	25.386215
163.716150	5692.167101	25.391232
163.791616	5688.712835	25.396250
163.851610	5693.092927	25.401267
163.831849	5690.902814	25.406285
164.294345	5688.408101	25.411303
164.113924	5692.336687	25.416320
164.227908	5698.049861	25.421338
164.383977	5716.445695	25.426355
164.519339	5717.800737	25.431373
164.702502	5715.848619	25.436391
164.835271	5718.902924	25.441408
164.668097	5740.027945	25.446426
165.024277	5741.903909	25.451443
165.348174	5743.640322	25.456461
165.917736	5749.344755	25.461479
166.140746	5762.833848	25.466496
166.339797	5760.383689	25.471514
166.531604	5757.763039	25.476531
166.671302	5753.822380	25.481549
166.811735	5748.451332	25.486567
166.461329	5759.242907	25.491584
166.791623	5761.167281	25.496602
166.839782	5781.887194	25.501619
166.463776	5782.413608	25.506637
166.852372	5793.789664	25.511655
167.227170	5817.155219	25.516672
166.933290	5814.608179	25.521690
167.141323	5833.908338	25.526707
167.459957	5849.359269	25.531725
167.685503	5860.601010	25.536743
167.867218	5877.731827	25.541760
167.970122	5879.850734	25.546778
168.328164	5896.754584	25.551795
168.383577	5901.070911	25.556813
168.710561	5916.297630	25.561831
168.857058	5932.639670	25.566848
168.974364	5935.554819	25.571866
169.553560	5951.209072	25.576883
169.986969	5968.918794	25.581901
170.123121	5959.207907	25.586919
169.904554	5974.099244	25.591936
170.054085	5965.140655	25.596954
170.139529	5982.886949	25.601971
170.383358	5988.729872	25.606989
170.563293	5983.716054	25.612007
170.962084	5999.092380	25.617024
171.223027	6018.826607	25.622042
171.316419	6014.655721	25.627059
171.254869	6013.664942	25.632077
171.854595	6012.559553	25.637095
171.786015	6026.042980	25.642112
172.034666	6038.919230	25.647130
172.373364	6048.830938	25.652147
172.078294	6048.709099	25.657165
172.625500	6036.400067	25.662183
172.259907	6057.123723	25.667200
172.658318	6060.659287	25.672218
172.711426	6071.973152	25.677236
172.838847	6089.191982	25.682253
173.019410	6092.469187	25.687271
173.133840	6103.568106	25.692288
173.480347	6116.625061	25.697306
173.458535	6131.556311	25.702324
173.444453	6138.279377	25.707341
173.986767	6143.900272	25.712359
174.021585	6167.319690	25.717376
174.069396	6169.139834	25.722394
174.538527	6175.748754	25.727412
174.432599	6186.248744	25.732429
174.962490	6183.303269	25.737447
174.730096	6190.465104	25.742464
174.403725	6210.687034	25.747482
174.938941	6222.925892	25.752500
174.988375	6238.215583	25.757517
175.502537	6231.391340	25.762535
175.516790	6246.150518	25.767552
175.737919	6264.420400	25.772570
176.182694	6270.349754	25.777588
176.467325	6282.876036	25.782605
176.955373	6285.361038	25.787623
177.265685	6284.462035	25.792640
177.560193	6298.272869	25.797658
177.682131	6291.312146	25.802676
177.854918	6292.999695	25.807693
178.231467	6286.674018	25.812711
178.225430	6292.675141	25.817728
177.924494	6282.312078	25.822746
178.267992	6293.254136	25.827764
178.487414	6311.248690	25.832781
178.802893	6321.958351	25.837799
178.630946	6330.544462	25.842816
178.550995	6320.477029	25.847834
178.899609	6320.801135	25.852852
178.747562	6345.108011	25.857869
179.179403	6349.621827	25.862887
179.253540	6363.800925	25.867904
179.254690	6380.256582	25.872922
179.268928	6388.031252	25.877940
179.503290	6406.010829	25.882957
179.454164	6421.231223	25.887975
179.730228	6441.968477	25.892992
180.195537	6465.223862	25.898010
180.751688	6479.221365	25.903028
180.466964	6501.629502	25.908045
180.712742	6504.862089	25.913063
181.020416	6519.120665	25.918080
181.220426	6534.678620	25.923098
181.586659	6542.720954	25.928116
181.494673	6556.938857	25.933133
181.874278	6571.161898	25.938151
182.116939	6572.431448	25.943168
182.442529	6572.609737	25.948186
182.362326	6592.866860	25.953204
182.209404	6602.885814	25.958221
182.768737	6600.922278	25.963239
183.263666	6622.956867	25.968256
183.295862	6627.734080	25.973274
183.570305	6631.186407	25.978292
184.016398	6654.901306	25.983309
184.374952	6646.555037	25.988327
184.150460	6649.052169	25.993344
184.341203	6652.851579	25.998362
184.466412	6659.738391	26.003380
184.201691	6687.189071	26.008397
184.508479	6684.642893	26.013415
184.781708	6702.679360	26.018432
184.857737	6708.581152	26.023450
185.059990	6709.278514	26.028468
185.367123	6735.201537	26.033485
185.471135	6745.852107	26.038503
185.599355	6766.656099	26.043520
185.703350	6768.095209	26.048538
186.276209	6774.646977	26.053556
186.246123	6787.140101	26.058573
187.001923	6789.530286	26.063591
187.097071	6791.949910	26.068608
187.067612	6799.032614	26.073626
187.351229	6788.275142	26.078644
187.635848	6809.450962	26.083661
187.810532	6811.465913	26.088679
188.205042	6815.553651	26.093696
188.074248	6821.346500	26.098714
188.419400	6807.514851	26.103732
188.484427	6818.618543	26.108749
188.822945	6811.653897	26.113767
188.985890	6827.952385	26.118784
188.808119	6842.161168	26.123802
189.544165	6837.543017	26.128820
189.461141	6845.184419	26.133837
189.703193	6834.650426	26.138855
189.715921	6847.901289	26.143872
189.851776	6854.592655	26.148890
190.185459	6857.505102	26.153908
190.015389	6862.275038	26.158925
190.270739	6877.787904	26.163943
190.310845	6888.104199	26.168960
190.429115	6901.051652	26.173978
190.697797	6913.886693	26.178996
190.790759	6920.259916	26.184013
190.740259	6945.205374	26.189031
191.205880	6955.294265	26.194048
191.093739	6969.139388	26.199066
191.534152	6988.112487	26.204084
191.304650	7006.150133	26.209101
191.876126	7025.978948	26.214119
192.347925	7041.047213	26.219136
192.511795	7061.046984	26.224154
192.789251	7064.417778	26.229172
193.064571	7076.759562	26.234189
193.280718	7089.553853	26.239207
193.715928	7092.845666	26.244224
193.559583	7092.424294	26.249242
193.975894	7100.138804	26.254260
194.100397	7110.018247	26.259277
194.185975	7101.139746	26.264295
194.745288	7124.437194	26.269312
194.690432	7133.361092	26.274330
195.202112	7131.982769	26.279348
195.530415	7140.515337	26.284365
195.299523	7155.234179	26.289383
195.456845	7162.222208	26.294400
195.546320	7166.236273	26.299418
196.413058	7164.359434	26.304436
195.782319	7189.139399	26.309453
195.927440	7194.225687	26.314471
196.431825	7200.718122	26.319488
196.496056	7214.946889	26.324506
196.910977	7219.043943	26.329524
197.313904	7219.651272	26.334541
197.531130	7235.916743	26.339559
197.670570	7237.186172	26.344576
197.547307	7249.079975	26.349594
197.857325	7249.641305	26.354612
198.054774	7268.156520	26.359629
198.035599	7273.035409	26.364647
198.629852	7279.098631	26.369664
198.625877	7284.843008	26.374682
198.655661	7309.527582	26.379700
198.563077	7321.770793	26.384717
198.801190	7324.870921	26.389735
198.770471	7345.011294	26.394752
199.321583	7354.315893	26.399770
199.531101	7373.982378	26.404788
199.637530	7382.259717	26.409805
199.885424	7392.844280	26.414823
200.041685	7397.305732	26.419840
200.138942	7408.012220	26.424858
200.367099	7426.519366	26.429876
200.557349	7442.882477	26.434893
200.721225	7452.054559	26.439911
201.136254	7456.005151	26.444928
200.934834	7477.353996	26.449946
201.471402	7488.315214	26.454964
201.820460	7499.510031	26.459981
202.376076	7490.218448	26.464999
203.609465	7493.291864	26.470016
203.420995	7492.785235	26.475034
203.782735	7470.115655	26.480052
204.031611	7460.741939	26.485069
204.027108	7460.595431	26.490087
204.492056	7457.105210	26.495104
204.123865	7465.413408	26.500122
204.322249	7463.405776	26.505140
204.538323	7456.262703	26.510157
204.030832	7468.853806	26.515175
204.468181	7487.426299	26.520192
204.284866	7493.443943	26.525210
204.946492	7498.777694	26.530228
204.730309	7516.043354	26.535245
204.699340	7534.012376	26.540263
205.106451	7539.779121	26.545280
204.843815	7559.881897	26.550298
205.149929	7570.204060	26.555316
205.436814	7590.861465	26.560333
205.622265	7615.144136	26.565351
206.523043	7615.298547	26.570368
206.470478	7632.852220	26.575386
206.747429	7647.538332	26.580404
206.977461	7658.121315	26.585421
206.931304	7666.922762	26.590439
207.255368	7676.815873	26.595456
207.791825	7711.236988	26.600474
207.721264	7712.406656	26.605492
208.314792	7723.126206	26.610509
207.762672	7736.729239	26.615527
208.214442	7742.389389	26.620544
208.364613	7771.702055	26.625562
208.734730	7772.039956	26.630580
209.091017	7780.272047	26.635597
209.396197	7795.524683	26.640615
209.389627	7803.926569	26.645632
209.416935	7831.730846	26.650650
209.321782	7839.574027	26.655668
209.804984	7858.789973	26.660685
209.717447	7875.804638	26.665703
210.185051	7885.519640	26.670720
210.578784	7901.061714	26.675738
210.757359	7925.576797	26.680756
210.902244	7930.721651	26.685773
210.805399	7959.606237	26.690791
211.535643	7971.575377	26.695808
211.597188	7984.466972	26.700826
211.855259	8000.371185	26.705844
212.077336	8008.042795	26.710861
212.183981	8038.629024	26.715879
212.680722	8040.850565	26.720896
212.735581	8059.729896	26.725914
213.237486	8056.041994	26.730932
213.382772	8069.502646	26.735949
213.473856	8084.796647	26.740967
213.591423	8074.620449	26.745984
213.945096	8090.014974	26.751002
214.144165	8100.052001	26.756020
214.612230	8100.803724	26.761037
214.523823	8108.935793	26.766055
215.079232	8122.964027	26.771072
215.273851	8133.053803	26.776090
215.572596	8131.628861	26.781108
215.979705	8125.970089	26.786125
215.690932	8135.305214	26.791143
216.095796	8141.650733	26.796160
216.373081	8151.713395	26.801178
216.574562	8143.125415	26.806196
217.072926	8141.951667	26.811213
216.923187	8153.792253	26.816231
217.069738	8171.715167	26.821248
216.976429	8181.855966	26.826266
217.245152	8196.608545	26.831284
217.300213	8211.680217	26.836301
216.847072	8228.213270	26.841319
217.644574	8244.105293	26.846336
217.875442	8261.092670	26.851354
218.115076	8279.136513	26.856372
218.498547	8306.435015	26.861389
218.437808	8312.790223	26.866407
218.878441	8334.732238	26.871424
218.773509	8350.373364	26.876442
219.003800	8362.183255	26.881460
219.849460	8373.949986	26.886477
220.029042	8386.121220	26.891495
220.586391	8396.601471	26.896512
220.298479	8404.938563	26.901530
220.560809	8424.288784	26.906548
220.745733	8434.103083	26.911565
220.755342	8445.712599	26.916583
221.151484	8463.699137	26.921600
221.466407	8476.652221	26.926618
221.817800	8502.219450	26.931636
222.055732	8506.284022	26.936653
222.326631	8515.840677	26.941671
222.471629	8531.664168	26.946688
222.641326	8534.918482	26.951706
222.795718	8553.716478	26.956724
223.376452	8557.775307	26.961741
223.467891	8565.528760	26.966759
223.856495	8588.892174	26.971776
224.053373	8593.345640	26.976794
223.890202	8597.487909	26.981812
224.508362	8613.355748	26.986829
224.173446	8617.064947	26.991847
224.963331	8634.672737	26.996864
224.789334	8650.117669	27.001882
224.894384	8663.379910	27.006900
225.241169	8681.920009	27.011917
225.503597	8689.981477	27.016935
225.776667	8697.852122	27.021952
226.104946	8717.349289	27.026970
226.001808	8734.728245	27.031988
226.545838	8744.069504	27.037005
226.262648	8758.939515	27.042023
226.415545	8768.853871	27.047040
226.861674	8787.283057	27.052058
226.799296	8815.874362	27.057076
227.443785	8824.686943	27.062093
227.379968	8843.668845	27.067111
228.001396	8857.791530	27.072128
228.045573	8874.702659	27.077146
228.402258	8883.671803	27.082164
228.879976	8896.308289	27.087181
228.841234	8920.951600	27.092199
229.181221	8916.028436	27.097216
229.684615	8921.631594	27.102234
229.393100	8932.855083	27.107252
229.858342	8934.763738	27.112269
229.990028	8959.933367	27.117287
230.458508	8956.938525	27.122304
230.458265	8974.555088	27.127322
230.690835	8992.815968	27.132340
231.567271	8995.008434	27.137357
231.367553	8997.473451	27.142375
231.656062	9007.778993	27.147392
232.007961	9020.505018	27.152410
232.096703	9017.375533	27.157428
232.712937	9026.330779	27.162445
232.809348	9048.867434	27.167463
232.854024	9043.674257	27.172480
232.971803	9038.295630	27.177498
232.935771	9064.567001	27.182516
233.436896	9061.835341	27.187533
233.458786	9083.837724	27.192551
233.824658	9103.441766	27.197568
234.141926	9105.868953	27.202586
234.499173	9129.301389	27.207604
234.416216	9132.029044	27.212621
234.861512	9141.555524	27.217639
235.155127	9164.210037	27.222656
235.172933	9173.279765	27.227674
235.375224	9177.838843	27.232692
235.641915	9195.398693	27.237709
235.654014	9214.073009	27.242727
235.954676	9221.271306	27.247744
236.036316	9229.863316	27.252762
236.534483	9262.218388	27.257780
236.774337	9262.766248	27.262797
237.149892	9288.741937	27.267815
237.338588	9297.331950	27.272832
237.409110	9305.241278	27.277850
237.708935	9332.515257	27.282868
238.107572	9338.499920	27.287885
238.279557	9356.478232	27.292903
238.463669	9366.598108	27.297920
238.605911	9389.168590	27.302938
238.859879	9405.620026	27.307956
239.039127	9418.330152	27.312973
239.287813	9437.687019	27.317991
239.999208	9452.597241	27.323008
240.018425	9458.576454	27.328026
240.219916	9475.508558	27.333044
240.629861	9480.622478	27.338061
241.068200	9499.440582	27.343079
240.570397	9509.294927	27.348096
241.698782	9517.661180	27.353114
241.780138	9531.147867	27.358132
242.341451	9522.669525	27.363149
242.569286	9527.735728	27.368167
242.594124	9524.560831	27.373184
243.017037	9532.661447	27.378202
242.898649	9544.130743	27.383220
243.182108	9542.359236	27.388237
243.323171	9559.395215	27.393255
243.478519	9579.005672	27.398272
243.524553	9586.419754	27.403290
243.679568	9599.843054	27.408308
244.152047	9613.793428	27.413325
244.273636	9632.928224	27.418343
244.419106	9656.672345	27.423360
244.609161	9657.161533	27.428378
244.406989	9684.991404	27.433396
244.829809	9696.426032	27.438413
245.236207	9707.568764	27.443431
245.180687	9734.685828	27.448448
245.110902	9743.897265	27.453466
245.142457	9768.787806	27.458484
245.450904	9788.119412	27.463501
245.979823	9820.775380	27.468519
246.266199	9848.373892	27.473536
246.983068	9865.554016	27.478554
246.919669	9887.715837	27.483572
247.187837	9904.345044	27.488589
247.817264	9919.211813	27.493607
247.953379	9948.530017	27.498624
248.454493	9945.565814	27.503642
248.594372	9982.568440	27.508660
248.852644	9976.269639	27.513677
249.466545	9987.899615	27.518695
249.712171	9994.390508	27.523712
250.429374	9999.933317	27.528730
250.307861	10020.591610	27.533748
250.460588	10024.425722	27.538765
250.573565	10025.704503	27.543783
250.718151	10046.972494	27.548800
250.905863	10048.472837	27.553818
250.921419	10077.528486	27.558836
251.169340	10093.291515	27.563853
251.747957	10113.141907	27.568871
251.916358	10135.616920	27.573888
252.064259	10148.358043	27.578906
252.078984	10163.375228	27.583924
252.366937	10192.745855	27.588941
252.555121	10201.819368	27.593959
252.550262	10238.861600	27.598976
253.395992	10247.600575	27.603994
253.515669	10274.105668	27.609012
253.788006	10285.708315	27.614029
254.459132	10299.263888	27.619047
254.857838	10303.294330	27.624064
255.264918	10309.298441	27.629082
255.384841	10323.960324	27.634100
255.948267	10347.727411	27.639117
256.085697	10349.887663	27.644135
256.256583	10349.482733	27.649152
256.654265	10362.401540	27.654170
257.052587	10358.097717	27.659188
257.488501	10356.118807	27.664205
257.702980	10354.682469	27.669223
257.648340	10360.382007	27.674240
258.134450	10371.270887	27.679258
258.176141	10384.952382	27.684276
258.191144	10392.538222	27.689293
258.747559	10395.389903	27.694311
258.726891	10414.633563	27.699328
258.762652	10420.408703	27.704346
258.807586	10427.264001	27.709364
259.431354	10451.411978	27.714381
259.522143	10447.434965	27.719399
259.721333	10464.705685	27.724416
260.237765	10474.919159	27.729434
260.159991	10486.347713	27.734452
260.132491	10507.974218	27.739469
260.602778	10522.451230	27.744487
260.757778	10539.748281	27.749504
260.996581	10557.878343	27.754522
261.302466	10579.226597	27.759540
261.569303	10603.963527	27.764557
261.704220	10613.125695	27.769575
261.622004	10638.613176	27.774592
262.231254	10644.934410	27.779610
262.330881	10668.683704	27.784628
262.239840	10692.561614	27.789645
262.752199	10709.915286	27.794663
262.109754	10735.481819	27.799680
263.091857	10768.742750	27.804698
263.438572	10781.460797	27.809716
263.418494	10806.503332	27.814733
264.382543	10830.797818	27.819751
264.199045	10857.709560	27.824768
264.716141	10872.677817	27.829786
265.179066	10893.548173	27.834804
265.855227	10908.152838	27.839821
266.560651	10912.844690	27.844839
266.539876	10934.480891	27.849856
266.785310	10933.652305	27.854874
266.798178	10947.661296	27.859892
266.662396	10963.150942	27.864909
267.394248	10974.021464	27.869927
267.650892	11001.470114	27.874944
268.008117	10999.872917	27.879962
268.403879	11020.844413	27.884980
268.466846	11026.199263	27.889997
268.888756	11038.153410	27.895015
268.749956	11060.442822	27.900032
269.051702	11068.324843	27.905050
269.137893	11092.039175	27.910068
269.178832	11108.140913	27.915085
269.993586	11121.870286	27.920103
269.659730	11151.243551	27.925120
269.865918	11171.636937	27.930138
270.322217	11199.063782	27.935156
270.799091	11224.643658	27.940173
270.885665	11244.592171	27.945191
271.144435	11264.683853	27.950208
271.932230	11277.521250	27.955226
272.709632	11285.393683	27.960244
273.355944	11279.928863	27.965261
274.147963	11276.181016	27.970279
274.304938	11286.364126	27.975296
274.280856	11280.816871	27.980314
274.655868	11279.703594	27.985332
274.742515	11289.025436	27.990349
274.843605	11278.697105	27.995367
274.748370	11299.359759	28.000384
275.365515	11311.004344	28.005402
275.351974	11312.437398	28.010420
275.411956	11323.593115	28.015437
276.064761	11342.094120	28.020455
275.765585	11356.516153	28.025472
275.993147	11370.036029	28.030490
276.451411	11384.313335	28.035508
276.042554	11410.005997	28.040525
276.498681	11417.320486	28.045543
276.711505	11454.129221	28.050560
277.114186	11468.795592	28.055578
277.153398	11502.179243	28.060596
277.482266	11516.484468	28.065613
277.425563	11540.918106	28.070631
277.800090	11567.007165	28.075648
278.088510	11599.568037	28.080666
278.382188	11626.712203	28.085684
278.253862	11659.578799	28.090701
279.060110	11683.714855	28.095719
279.320886	11703.976935	28.100736
279.300805	11732.848451	28.105754
279.633706	11749.018927	28.110772
280.207727	11772.163142	28.115789
281.052240	11779.457392	28.120807
281.165353	11804.786620	28.125824
281.643497	11813.191224	28.130842
282.126269	11818.410408	28.135860
282.183771	11845.123020	28.140877
282.494449	11845.566240	28.145895
282.733092	11866.538152	28.150912
282.909674	11878.900842	28.155930
283.477573	11903.050039	28.160948
283.472709	11922.891668	28.165965
283.843826	11927.393544	28.170983
283.846777	11945.275192	28.176000
283.972720	11964.876105	28.181018
284.405170	11975.904207	28.186036
284.292267	12005.158790	28.191053
284.805407	12018.248843	28.196071
285.030037	12047.070808	28.201088
285.262087	12063.055075	28.206106
285.890568	12086.595676	28.211124
285.838351	12111.560475	28.216141
286.380651	12121.916466	28.221159
286.432610	12151.930253	28.226176
286.610694	12165.849817	28.231194
287.378966	12198.819099	28.236212
287.367647	12219.834572	28.241229
288.061812	12239.495844	28.246247
288.248210	12262.497153	28.251264
288.517747	12273.013593	28.256282
289.128250	12293.847062	28.261300
289.557878	12315.867268	28.266317
289.883085	12322.368732	28.271335
289.832571	12342.522593	28.276352
290.077732	12360.329790	28.281370
290.632485	12376.385245	28.286388
290.806173	12403.985580	28.291405
290.939012	12404.538731	28.296423
291.251979	12435.967331	28.301440
291.484085	12446.781633	28.306458
291.839630	12467.572589	28.311476
291.703345	12488.256182	28.316493
292.446678	12500.074496	28.321511
292.848063	12524.414598	28.326528
292.843318	12540.251151	28.331546
293.132419	12556.522687	28.336564
293.272473	12590.139232	28.341581
293.675359	12598.181696	28.346599
294.227073	12624.279268	28.351616
294.448659	12645.302297	28.356634
294.888980	12664.530350	28.361652
294.955330	12681.671075	28.366669
295.633292	12696.923174	28.371687
295.790889	12715.760168	28.376704
295.707540	12741.348846	28.381722
296.445036	12752.476509	28.386740
296.300945	12780.201191	28.391757
296.699989	12789.293922	28.396775
296.702675	12820.012090	28.401792
296.941549	12845.131367	28.406810
297.398970	12865.559214	28.411828
297.634413	12895.239745	28.416845
298.093724	12913.125434	28.421863
298.348705	12940.301867	28.426880
298.503363	12960.726554	28.431898
299.071127	12990.903611	28.436916
299.294829	13012.555546	28.441933
299.873737	13029.359340	28.446951
300.031956	13043.115912	28.451968
300.485623	13056.810804	28.456986
300.544495	13058.189432	28.462004
300.900067	13076.738657	28.467021
301.476298	13091.549442	28.472039
301.619275	13114.374790	28.477056
301.817016	13132.967636	28.482074
302.281081	13148.769444	28.487092
302.401413	13165.737817	28.492109
302.766752	13187.984212	28.497127
303.156882	13207.739723	28.502144
303.569995	13221.684183	28.507162
303.705021	13244.126510	28.512180
303.824080	13259.837608	28.517197
304.221877	13275.311727	28.522215
304.762897	13293.439561	28.527232
304.742888	13309.131260	28.532250
305.439298	13322.317999	28.537268
305.505197	13353.220509	28.542285
305.867338	13375.861676	28.547303
306.411971	13373.219799	28.552320
307.270145	13392.223279	28.557338
307.985369	13386.484716	28.562356
308.105910	13396.128357	28.567373
308.799325	13393.471215	28.572391
309.234670	13374.390023	28.577408
309.291424	13372.604558	28.582426
309.516648	13370.613025	28.587444
309.696728	13376.447191	28.592461
309.761780	13394.926850	28.597479
309.866917	13410.697140	28.602496
309.992114	13411.376096	28.607514
310.393951	13433.186534	28.612532
310.110170	13455.115633	28.617549
310.215157	13465.693279	28.622567
310.707767	13492.798064	28.627584
310.743144	13518.621965	28.632602
311.310161	13527.680903	28.637620
311.161899	13555.331950	28.642637
311.799377	13585.478044	28.647655
312.107682	13606.180598	28.652672
312.026893	13640.315090	28.657690
312.524822	13660.964148	28.662708
312.774508	13688.230964	28.667725
312.944949	13722.383776	28.672743
313.424885	13746.706357	28.677760
313.590514	13784.325653	28.682778
314.028522	13806.820858	28.687796
313.960620	13841.833022	28.692813
314.719176	13873.464593	28.697831
314.939934	13896.743029	28.702848
315.290231	13934.811090	28.707866
316.044931	13960.178926	28.712884
316.660161	13971.140202	28.717901
317.607520	13980.396247	28.722919
317.940610	13998.315134	28.727936
318.064667	14010.614102	28.732954
319.104064	13985.964727	28.737972
319.361818	13996.558315	28.742989
319.732405	14018.885351	28.748007
320.266111	14019.797483	28.753024
320.365963	14017.442158	28.758042
320.657850	14019.045349	28.763060
320.828257	14033.177395	28.768077
320.694638	14028.427518	28.773095
321.267236	14016.011304	28.778112
321.233213	14032.210345	28.783130
321.231200	14050.284248	28.788148
321.626081	14051.112277	28.793165
321.888018	14077.055446	28.798183
321.739215	14083.833368	28.803200
321.471539	14104.925379	28.808218
322.041049	14128.437769	28.813236
322.248771	14157.453827	28.818253
322.467790	14186.252145	28.823271
322.899740	14195.962726	28.828288
322.845235	14240.325573	28.833306
323.248932	14261.599390	28.838324
323.501974	14293.052563	28.843341
323.726983	14328.401657	28.848359
323.969970	14347.352432	28.853376
324.259953	14396.488993	28.858394
325.355533	14426.743360	28.863412
325.606489	14447.015220	28.868429
325.552589	14491.098110	28.873447
326.489044	14511.853489	28.878464
326.397424	14540.390404	28.883482
326.845107	14560.076530	28.888500
327.398465	14588.960282	28.893517
327.474831	14624.746057	28.898535
328.013101	14636.956195	28.903552
327.909068	14680.155875	28.908570
328.805801	14697.983471	28.913588
329.724480	14704.568550	28.918605
330.283352	14715.545998	28.923623
330.993691	14732.347059	28.928640
330.851346	14738.254190	28.933658
331.694156	14752.353958	28.938676
332.146096	14753.178852	28.943693
332.942710	14754.698269	28.948711
333.264723	14749.591950	28.953728
333.477522	14748.937244	28.958746
333.557931	14744.167363	28.963764
333.745384	14761.827592	28.968781
333.942267	14782.102547	28.973799
333.994224	14775.162409	28.978816
333.641657	14801.769893	28.983834
334.150139	14814.183698	28.988852
333.901437	14846.356444	28.993869
334.428594	14866.827232	28.998887
334.969866	14892.380129	29.003904
334.990487	14921.441231	29.008922
335.366817	14956.166054	29.013940
335.699443	14977.714242	29.018957
336.114685	15021.403826	29.023975
336.035291	15041.933042	29.028992
336.291263	15075.355770	29.034010
336.754749	15098.882443	29.039028
337.091654	15141.056545	29.044045
337.371740	15174.934115	29.049063
338.012554	15199.868884	29.054080
338.003422	15229.368902	29.059098
338.601723	15261.324520	29.064116
338.982091	15289.308340	29.069133
339.065304	15329.398888	29.074151
339.867543	15347.320125	29.079168
340.080467	15384.753984	29.084186
340.621254	15399.591678	29.089204
341.130086	15430.005275	29.094221
341.460332	15445.930842	29.099239
341.870774	15474.913978	29.104256
341.979507	15494.517261	29.109274
342.627223	15513.804066	29.114292
342.947093	15540.354622	29.119309
343.114330	15570.487932	29.124327
343.308977	15586.195011	29.129344
343.657455	15607.348932	29.134362
343.767388	15634.063758	29.139380
344.260929	15650.033323	29.144397
344.575955	15675.636059	29.149415
345.535359	15693.994957	29.154432
345.609409	15714.173256	29.159450
345.733214	15730.714995	29.164468
346.250570	15750.151404	29.169485
345.839177	15786.129490	29.174503
346.500851	15807.570515	29.179520
346.792934	15843.707693	29.184538
347.162238	15859.466403	29.189556
347.491101	15889.625461	29.194573
347.933796	15915.683367	29.199591
348.462873	15937.461824	29.204608
348.823582	15970.394542	29.209626
348.791825	15999.737351	29.214644
349.428313	16017.582830	29.219661
349.314763	16056.052837	29.224679
349.886134	16081.361430	29.229696
350.272974	16117.757725	29.234714
350.606845	16151.499123	29.239732
351.217519	16172.433680	29.244749
351.231454	16206.209424	29.249767
351.714459	16228.292247	29.254784
351.635280	16263.473789	29.259802
352.232233	16294.679790	29.264820
352.687670	16333.661188	29.269837
352.803026	16376.089622	29.274855
353.397087	16405.625520	29.279872
353.640094	16441.836785	29.284890
353.842975	16477.616604	29.289908
354.189375	16514.390905	29.294925
354.599609	16551.075872	29.299943
355.512052	16579.449521	29.304960
355.914516	16602.398971	29.309978
356.748599	16622.906081	29.314996
357.222487	16636.822874	29.320013
357.430936	16665.769154	29.325031
357.408023	16672.142618	29.330048
358.337555	16706.538071	29.335066
358.837699	16705.554988	29.340084
359.163861	16723.260483	29.345101
359.579637	16737.535366	29.350119
359.863792	16752.875607	29.355136
360.607537	16772.836766	29.360154
360.697322	16785.132470	29.365172
361.094855	16800.266347	29.370189
361.327779	16823.709266	29.375207
361.605312	16839.200433	29.380224
361.893397	16862.304804	29.385242
361.899098	16879.857211	29.390260
362.467883	16905.645110	29.395277
362.567969	16925.615648	29.400295
362.675859	16952.898829	29.405312
363.075107	16981.705205	29.410330
363.328816	17022.137237	29.415348
363.888068	17049.619871	29.420365
363.718388	17073.938658	29.425383
364.279781	17117.633166	29.430400
364.378544	17145.990059	29.435418
364.546320	17198.944691	29.440436
365.347384	17217.244906	29.445453
365.798699	17254.876697	29.450471
366.731326	17270.306735	29.455488
367.022402	17298.460125	29.460506
367.598788	17319.138594	29.465524
367.895354	17326.857427	29.470541
368.074552	17353.900857	29.475559
368.433899	17369.512918	29.480576
368.714737	17388.308007	29.485594
368.901041	17412.560273	29.490612
369.418406	17431.777982	29.495629
369.439569	17473.425679	29.500647
369.925663	17487.402640	29.505664
370.474928	17516.178720	29.510682
370.874241	17537.902034	29.515700
371.532606	17566.269148	29.520717
371.568710	17591.977938	29.525735
371.941469	17614.230682	29.530752
372.257204	17643.788233	29.535770
371.962793	17673.215467	29.540788
372.554451	17702.036848	29.545805
372.633107	17736.947811	29.550823
372.934434	17776.695941	29.555840
373.200590	17812.964684	29.560858
373.848832	17867.689127	29.565876
374.074156	17895.978986	29.570893
374.341518	17945.733623	29.575911
374.637663	17986.641748	29.580928
375.288827	18021.160271	29.585946
375.330457	18073.262178	29.590964
376.061227	18099.915686	29.595981
376.782779	18147.718007	29.600999
377.253513	18169.373534	29.606016
378.016236	18197.861540	29.611034
378.134927	18237.343172	29.616052
379.065705	18250.419302	29.621069
379.256543	18277.071354	29.626087
379.704799	18306.801968	29.631104
380.428599	18335.274607	29.636122
380.430214	18348.495702	29.641140
381.065842	18380.914627	29.646157
380.975998	18416.291669	29.651175
381.432231	18436.176487	29.656192
381.836249	18458.626952	29.661210
382.048219	18489.147517	29.666228
382.670311	18520.236886	29.671245
382.938556	18552.091331	29.676263
383.270574	18594.011785	29.681280
383.661861	18612.953862	29.686298
383.745981	18649.960909	29.691316
384.204373	18674.560774	29.696333
384.451326	18719.222912	29.701351
384.839525	18744.922286	29.706368
385.232957	18781.830952	29.711386
385.483606	18822.490149	29.716404
386.432399	18854.427605	29.721421
386.625157	18888.231118	29.726439
387.058518	18914.088780	29.731456
387.397115	18944.619096	29.736474
387.764139	18981.838425	29.741492
388.074802	19013.390328	29.746509
388.190780	19048.702990	29.751527
389.091652	19094.580170	29.756544
389.754573	19112.971646	29.761562
390.094072	19149.959450	29.766580
390.937717	19167.412912	29.771597
391.293388	19185.005780	29.776615
391.552446	19206.401440	29.781632
391.435801	19229.111268	29.786650
391.958835	19264.891201	29.791668
392.770613	19283.114679	29.796685
392.961639	19313.974447	29.801703
393.428992	19332.532655	29.806720
393.805413	19361.756839	29.811738
394.100825	19382.621710	29.816756
394.748808	19396.882386	29.821773
394.846840	19418.724417	29.826791
395.260341	19452.856578	29.831808
395.430580	19468.803139	29.836826
395.466495	19496.723589	29.841844
396.254494	19521.976235	29.846861
396.211013	19555.039961	29.851879
396.600692	19587.312906	29.856896
396.752160	19613.202710	29.861914
396.767279	19644.880572	29.866932
397.378128	19688.466414	29.871949
397.445109	19728.012183	29.876967
397.834297	19777.141922	29.881984
398.624469	19804.543461	29.887002
398.676963	19857.426360	29.892020
399.458872	19891.611732	29.897037
399.891425	19949.847252	29.902055
400.120088	19980.156507	29.907072
401.097687	20010.368214	29.912090
401.354825	20043.151212	29.917108
402.289359	20076.739317	29.922125
402.930234	20114.101712	29.927143
403.001317	20131.326633	29.932160
403.578161	20164.428835	29.937178
403.719702	20200.266254	29.942196
404.635802	20219.696858	29.947213
405.259061	20240.539873	29.952231
405.750498	20252.011506	29.957248
406.591808	20263.875934	29.962266
407.091137	20292.584703	29.967284
407.332053	20288.872846	29.972301
407.505906	20305.743486	29.977319
408.153099	20327.184892	29.982336
409.129947	20326.388882	29.987354
409.634054	20337.661395	29.992372
410.008657	20338.275570	29.997389
410.276882	20340.406757	30.002407
410.302406	20357.759300	30.007424
410.778105	20374.277165	30.012442
410.966514	20404.351078	30.017460
411.401378	20402.511515	30.022477
411.557667	20428.296146	30.027495
411.514444	20449.801940	30.032512
412.095616	20479.104428	30.037530
412.044161	20506.541285	30.042548
412.761045	20532.956624	30.047565
412.944694	20558.282845	30.052583
413.246834	20601.550262	30.057600
413.731562	20615.087054	30.062618
414.088025	20643.839075	30.067636
414.373413	20681.706393	30.072653
414.627147	20719.042999	30.077671
415.175826	20750.856625	30.082688
415.643756	20778.690105	30.087706
415.836357	20819.967643	30.092724
415.978659	20856.265138	30.097741
416.302901	20906.410139	30.102759
416.437950	20948.593088	30.107776
417.162621	20982.381844	30.112794
417.260267	21047.101667	30.117812
417.682877	21085.388565	30.122829
418.172354	21132.109079	30.127847
418.742793	21176.115434	30.132864
419.091138	21210.167394	30.137882
419.577415	21256.638094	30.142900
419.983111	21297.911363	30.147917
420.512444	21323.813567	30.152935
420.649293	21375.080578	30.157952
421.444411	21411.111587	30.162970
421.695886	21441.202102	30.167988
421.905073	21490.221689	30.173005
422.787967	21517.691045	30.178023
423.285759	21554.549062	30.183040
423.829099	21588.438530	30.188058
424.271285	21618.467726	30.193076
424.755239	21652.851239	30.198093
425.324842	21684.123916	30.203111
425.520177	21722.394825	30.208128
426.509800	21732.390901	30.213146
427.076137	21763.197557	30.218164
427.666457	21778.408003	30.223181
428.506666	21800.408932	30.228199
428.447071	21828.210359	30.233216
429.071017	21837.305430	30.238234
429.395104	21866.831210	30.243252
429.676915	21900.589727	30.248269
430.042430	21912.014038	30.253287
430.008803	21950.241503	30.258304
430.518532	21978.938810	30.263322
430.815963	21999.402950	30.268340
430.999930	22036.087094	30.273357
431.478266	22071.834708	30.278375
431.561578	22123.833460	30.283392
432.213004	22161.982305	30.288410
432.294063	22208.463013	30.293428
432.755649	22251.408589	30.298445
433.197283	22303.051940	30.303463
433.326192	22361.582746	30.308480
433.721748	22394.345749	30.313498
434.482717	22452.385573	30.318516
434.968915	22489.637023	30.323533
435.763952	22526.537666	30.328551
435.873134	22565.668378	30.333568
436.768543	22602.528863	30.338586
437.179685	22651.573457	30.343604
437.545757	22689.938031	30.348621
438.366148	22722.263707	30.353639
438.420204	22768.506027	30.358656
439.004622	22800.858433	30.363674
439.602799	22830.393979	30.368692
439.833924	22890.566876	30.373709
440.488776	22917.991243	30.378727
440.854853	22957.956909	30.383744
441.573193	22976.461689	30.388762
441.800587	23025.539460	30.393780
442.323482	23057.639242	30.398797
442.642789	23082.643957	30.403815
443.213912	23122.082398	30.408832
443.840994	23158.261732	30.413850
444.312361	23188.355096	30.418868
445.012939	23221.988346	30.423885
445.726505	23243.606940	30.428903
445.897549	23280.275419	30.433920
446.463944	23297.859668	30.438938
446.827035	23334.553133	30.443956
447.296059	23357.041926	30.448973
448.393995	23370.808654	30.453991
448.586920	23400.016707	30.459008
449.002333	23415.516290	30.464026
449.412622	23442.608407	30.469044
449.683579	23480.744571	30.474061
450.132557	23493.573712	30.479079
450.334004	23527.422928	30.484096
450.661573	23539.455438	30.489114
451.002292	23585.810056	30.494132
451.213077	23607.746005	30.499149
451.727987	23640.663472	30.504167
451.453572	23675.646967	30.509184
452.166231	23706.978467	30.514202
452.617578	23755.797225	30.519220
452.471191	23795.272825	30.524237
453.176008	23845.833233	30.529255
453.667436	23883.388065	30.534272
453.843379	23919.669182	30.539290
454.609345	23970.765422	30.544308
455.176429	24022.771625	30.549325
455.434410	24056.491077	30.554343
455.844434	24110.975778	30.559360
456.064459	24140.620565	30.564378
456.533365	24185.668731	30.569396
456.726178	24237.878101	30.574413
457.447436	24284.776963	30.579431
457.661899	24342.956589	30.584448
458.011472	24401.129741	30.589466
458.885969	24458.698657	30.594484
458.950905	24517.670123	30.599501
459.851943	24563.432848	30.604519
460.073322	24622.946407	30.609536
460.757807	24672.933886	30.614554
461.601477	24712.613024	30.619572
462.086350	24758.224612	30.624589
462.062388	24806.059259	30.629607
462.422992	24863.330099	30.634624
463.040677	24912.588176	30.639642
464.021704	24968.349621	30.644660
464.403915	25019.536390	30.649677
465.119088	25064.063395	30.654695
465.385561	25124.832832	30.659712
465.776041	25157.753389	30.664730
466.147029	25203.454467	30.669748
466.654192	25254.728424	30.674765
467.703325	25301.793251	30.679783
467.880845	25344.167710	30.684800
468.351081	25391.723197	30.689818
468.877305	25426.892695	30.694836
469.119962	25477.006369	30.699853
469.927658	25512.381625	30.704871
470.279264	25563.530941	30.709888
470.697728	25603.535099	30.714906
470.999206	25653.248400	30.719924
471.219566	25703.164568	30.724941
471.723313	25758.522109	30.729959
472.199366	25811.802654	30.734976
473.262636	25862.875667	30.739994
474.302915	25891.828953	30.745012
474.898555	25934.349908	30.750029
475.824953	25940.551851	30.755047
476.452276	25966.511096	30.760064
477.084458	25987.984250	30.765082
477.599999	26012.896000	30.770100
477.832433	26045.809812	30.775117
478.293696	26058.337614	30.780135
478.370689	26089.006266	30.785152
478.825528	26118.770031	30.790170
479.555135	26149.983335	30.795188
479.778485	26193.153456	30.800205
480.009783	26218.059088	30.805223
480.314705	26259.392655	30.810240
480.138103	26298.500506	30.815258
480.765048	26348.357325	30.820276
480.821560	26397.293340	30.825293
481.277135	26438.400438	30.830311
481.721355	26505.649433	30.835328
481.912025	26544.882948	30.840346
482.566664	26592.206094	30.845364
482.749498	26651.770924	30.850381
483.018562	26699.092159	30.855399
483.271186	26744.353293	30.860416
483.974917	26812.730654	30.865434
484.378201	26873.398366	30.870452
484.872612	26941.852009	30.875469
485.589677	26995.304374	30.880487
486.195301	27049.094009	30.885504
487.053563	27084.426249	30.890522
488.570138	27119.709163	30.895540
489.076639	27157.099890	30.900557
489.580503	27188.273706	30.905575
490.145791	27221.175484	30.910592
490.731724	27244.664126	30.915610
491.364761	27278.015313	30.920628
491.575646	27325.417322	30.925645
492.069534	27348.738433	30.930663
492.604355	27394.623152	30.935680
492.554716	27440.030941	30.940698
493.063660	27469.428436	30.945716
493.223552	27519.889852	30.950733
493.988396	27565.960793	30.955751
494.721183	27611.772199	30.960768
494.441666	27657.896960	30.965786
495.131776	27707.251945	30.970804
495.420247	27755.046024	30.975821
496.174637	27803.087775	30.980839
496.388034	27862.973456	30.985856
496.928609	27921.069983	30.990874
497.726458	27967.590770	30.995892
498.033832	28028.884137	31.000909
498.353023	28078.815983	31.005927
498.905993	28134.740789	31.010944
499.148826	28193.761507	31.015962
499.935215	28249.206267	31.020980
499.972163	28304.021707	31.025997
500.641449	28361.984763	31.031015
501.303013	28418.088034	31.036032
501.593808	28485.042098	31.041050
502.316043	28541.949602	31.046068
502.844166	28599.634042	31.051085
503.506960	28655.961861	31.056103
504.481034	28708.439870	31.061120
504.700971	28763.863619	31.066138
505.364048	28805.411925	31.071156
506.126233	28870.923177	31.076173
506.547167	28908.451768	31.081191
507.533426	28946.965485	31.086208
508.045956	28995.265223	31.091226
508.782835	29041.202755	31.096244
508.763986	29078.580761	31.101261
509.123455	29126.893663	31.106279
509.594194	29168.774485	31.111296
509.953573	29213.715148	31.116314
510.415055	29274.255380	31.121332
510.904039	29319.300984	31.126349
511.507391	29379.877963	31.131367
512.261224	29410.528406	31.136384
512.635015	29459.978754	31.141402
513.195027	29512.972788	31.146420
513.924117	29568.036901	31.151437
514.462059	29601.487213	31.156455
515.010649	29655.837025	31.161472
515.063851	29704.710326	31.166490
515.358494	29753.587835	31.171508
516.066941	29803.393715	31.176525
516.609076	29855.562009	31.181543
517.046770	29900.620782	31.186560
517.074242	29954.322962	31.191578
518.176482	30001.719877	31.196596
518.394168	30049.254356	31.201613
518.641890	30103.633438	31.206631
519.596639	30153.453044	31.211648
520.041156	30204.786742	31.216666
520.960409	30240.086880	31.221684
521.348548	30282.514125	31.226701
521.680349	30328.102695	31.231719
522.502641	30371.142693	31.236736
522.552798	30430.540544	31.241754
523.552667	30469.336161	31.246772
523.924829	30520.818466	31.251789
524.322606	30567.330597	31.256807
524.880352	30618.236541	31.261824
525.466162	30673.233270	31.266842
525.810247	30730.712357	31.271860
526.206565	30777.367264	31.276877
526.237177	30842.758135	31.281895
527.033557	30886.147607	31.286912
526.960709	30960.488247	31.291930
527.980956	31010.271013	31.296948
528.152352	31079.441329	31.301965
528.681357	31144.065879	31.306983
529.484682	31212.548066	31.312000
529.844690	31279.595960	31.317018
531.278554	31321.899376	31.322036
532.585753	31364.107186	31.327053
533.170442	31403.768931	31.332071
533.978205	31446.246038	31.337088
534.580113	31491.111235	31.342106
535.946135	31499.946242	31.347124
537.052840	31513.957882	31.352141
537.953977	31533.594751	31.357159
538.295886	31540.618363	31.362176
538.528300	31565.086559	31.367194
538.922196	31582.895643	31.372212
538.965211	31612.582582	31.377229
539.747962	31632.819789	31.382247
539.796935	31667.207161	31.387264
539.692609	31701.282444	31.392282
539.958709	31732.500705	31.397300
540.514108	31785.612795	31.402317
540.494861	31829.181061	31.407335
541.035708	31882.314790	31.412352
541.379192	31939.640151	31.417370
541.896453	32003.133888	31.422388
542.068379	32064.343944	31.427405
542.593809	32129.830948	31.432423
543.183700	32184.494091	31.437440
543.741128	32265.200866	31.442458
544.038203	32317.025884	31.447476
544.192283	32388.678012	31.452493
544.454617	32455.307985	31.457511
545.415623	32518.395403	31.462528
546.049173	32603.347726	31.467546
546.762457	32659.607422	31.472564
547.059869	32737.910907	31.477581
547.621170	32808.462114	31.482599
548.504261	32866.388750	31.487616
548.722466	32946.732122	31.492634
549.531432	33003.633360	31.497652
550.367642	33072.903009	31.502669
551.455374	33117.729518	31.507687
552.302230	33159.708836	31.512704
553.105413	33218.375662	31.517722
553.426002	33252.960819	31.522740
554.312005	33297.426841	31.527757
554.422205	33342.189051	31.532775
555.359113	33381.055180	31.537792
555.224374	33429.588163	31.542810
555.771676	33474.139273	31.547828
556.514035	33527.922915	31.552845
557.028817	33568.749754	31.557863
558.304313	33604.234144	31.562880
558.747431	33652.113231	31.567898
559.067651	33689.192231	31.572916
559.636317	33735.879959	31.577933
559.932828	33779.668795	31.582951
560.570799	33828.320684	31.587968
560.935859	33880.804809	31.592986
561.388516	33933.561707	31.598004
561.803052	33977.183113	31.603021
562.204354	34034.152190	31.608039
562.755745	34096.174031	31.613056
563.089756	34154.041414	31.618074
563.783030	34208.169765	31.623092
564.514004	34269.682719	31.628109
564.808603	34345.759481	31.633127
565.568380	34394.932318	31.638144
566.141031	34464.677171	31.643162
566.493800	34521.914633	31.648180
567.793074	34573.538764	31.653197
568.159558	34638.102033	31.658215
568.728937	34689.349091	31.663232
569.418599	34759.365994	31.668250
570.110772	34807.541334	31.673268
570.415994	34859.877321	31.678285
570.665615	34930.517079	31.683303
571.433307	34991.691899	31.688320
571.833015	35046.644719	31.693338
572.168657	35113.250348	31.698356
572.922191	35167.785014	31.703373
573.276363	35244.638354	31.708391
573.769872	35305.487378	31.713408
574.315554	35384.528114	31.718426
574.935320	35447.442715	31.723444
575.734154	35512.716848	31.728461
576.691414	35580.817890	31.733479
577.287154	35636.879261	31.738496
577.987973	35702.504891	31.743514
578.662027	35754.880073	31.748532
579.845760	35814.221259	31.753549
580.175011	35878.722580	31.758567
580.437586	35917.627310	31.763584
580.871068	35986.751046	31.768602
581.498946	36039.491354	31.773620
582.107082	36094.204465	31.778637
582.641433	36152.455305	31.783655
583.404518	36221.499960	31.788672
584.174683	36281.738253	31.793690
584.380500	36344.216599	31.798708
585.296070	36394.767192	31.803725
585.394654	36464.835233	31.808743
586.236951	36508.890423	31.813760
586.909460	36565.737277	31.818778
587.855133	36604.870918	31.823796
589.106278	36645.531990	31.828813
589.597264	36700.701941	31.833831
590.519962	36737.624072	31.838848
590.640894	36780.224789	31.843866
591.312481	36831.151674	31.848884
591.746634	36869.925812	31.853901
591.925545	36922.888440	31.858919
592.951113	36958.064349	31.863936
593.323384	37005.014125	31.868954
594.122647	37046.789530	31.873972
594.735577	37082.655976	31.878989
594.961078	37123.958715	31.884007
595.611836	37162.078892	31.889024
596.015415	37202.323309	31.894042
596.177011	37251.827383	31.899060
596.950389	37302.183193	31.904077
597.436669	37365.480149	31.909095
597.856607	37422.305355	31.914112
598.486265	37482.514170	31.919130
599.187700	37533.939926	31.924148
600.065591	37589.651192	31.929165
599.629519	37651.397899	31.934183
600.311428	37711.179006	31.939200
600.863740	37782.237320	31.944218
601.211084	37843.510551	31.949236
601.614559	37926.095872	31.954253
602.014031	38004.206493	31.959271
602.861231	38070.352994	31.964288
603.604331	38154.817822	31.969306
603.998195	38235.685905	31.974324
605.051534	38313.544083	31.979341
604.996860	38405.525430	31.984359
605.641889	38469.478502	31.989376
606.364657	38556.505297	31.994394
606.705881	38635.695182	31.999412
607.548880	38722.620736	32.004429
608.279192	38808.132359	32.009447
609.186518	38887.516577	32.014464
609.514476	38978.193598	32.019482
609.834244	39057.006928	32.024500
610.362511	39133.570065	32.029517
611.349541	39229.075766	32.034535
611.789938	39306.708517	32.039552
612.297737	39394.011739	32.044570
612.945599	39486.781499	32.049588
613.556092	39562.070121	32.054605
614.245070	39656.273341	32.059623
615.402456	39733.744654	32.064640
616.105837	39810.291011	32.069658
616.185963	39895.271708	32.074676
616.846515	39974.748967	32.079693
617.725232	40066.255362	32.084711
618.386085	40141.932592	32.089728
620.528295	40198.250017	32.094746
622.327107	40232.675682	32.099764
624.174291	40256.928603	32.104781
624.862252	40293.489714	32.109799
625.389008	40296.079229	32.114816
626.008743	40322.941509	32.119834
626.522366	40342.557700	32.124852
627.740303	40362.442094	32.129869
627.676028	40393.105172	32.134887
627.839984	40419.923315	32.139904
628.484070	40455.425040	32.144922
628.765940	40490.140954	32.149940
629.126453	40527.890196	32.154957
629.740176	40570.910393	32.159975
629.469862	40609.162304	32.164992
629.916655	40663.609726	32.170010
630.272380	40727.464036	32.175028
631.065682	40774.404102	32.180045
631.235799	40853.707735	32.185063
631.644935	40923.690802	32.190080
632.084523	40983.633331	32.195098
632.297522	41054.189287	32.200116
632.776613	41123.283876	32.205133
633.430661	41205.217295	32.210151
633.957682	41269.900565	32.215168
634.586347	41346.216322	32.220186
634.629472	41429.300278	32.225204
635.709601	41498.511147	32.230221
636.560407	41570.178604	32.235239
637.367021	41649.389435	32.240256
638.244087	41720.576408	32.245274
638.605451	41802.273781	32.250292
639.506898	41864.323983	32.255309
639.778190	41944.171128	32.260327
640.294807	42019.539050	32.265344
641.162632	42097.725061	32.270362
641.613867	42178.559915	32.275380
642.710407	42251.733026	32.280397
643.877407	42306.652924	32.285415
644.372010	42378.818336	32.290432
645.227648	42441.159061	32.295450
646.049169	42502.965789	32.300468
646.940254	42560.015967	32.305485
647.445464	42633.696042	32.310503
648.137675	42688.733792	32.315520
649.480769	42750.224269	32.320538
649.657739	42805.123753	32.325556
650.175929	42863.146050	32.330573
650.945326	42915.948985	32.335591
651.221316	42997.498455	32.340608
652.188706	43035.145732	32.345626
652.741296	43115.819442	32.350644
652.937613	43181.508303	32.355661
653.424934	43256.766130	32.360679
653.869670	43329.934892	32.365696
654.570872	43402.704585	32.370714
654.920006	43487.979137	32.375732
655.963351	43573.839741	32.380749
656.482079	43649.131822	32.385767
656.589733	43727.918186	32.390784
657.399446	43810.424515	32.395802
657.695460	43911.177761	32.400820
658.454119	43995.325749	32.405837
659.331232	44094.101687	32.410855
659.680864	44175.925079	32.415872
660.571551	44255.903457	32.420890
661.111193	44348.415571	32.425908
662.151061	44432.900887	32.430925
663.228786	44510.039146	32.435943
664.302268	44585.312347	32.440960
665.504186	44651.313025	32.445978
665.848994	44728.807529	32.450996
666.675436	44793.870117	32.456013
667.922212	44858.073755	32.461031
668.342233	44919.708858	32.466048
668.789952	44984.272942	32.471066
669.617538	45055.294569	32.476084
670.212272	45104.965639	32.481101
670.714441	45180.020324	32.486119
671.515984	45233.481246	32.491136
672.245811	45311.413127	32.496154
672.855649	45371.284661	32.501172
673.955950	45435.738787	32.506189
674.402650	45497.399771	32.511207
674.797671	45556.840229	32.516224
675.451296	45615.410629	32.521242
676.212012	45698.653341	32.526260
676.569544	45758.984812	32.531277
677.176507	45826.594621	32.536295
677.409477	45900.872708	32.541312
678.352984	45971.594350	32.546330
678.583829	46042.384056	32.551348
679.028485	46125.696914	32.556365
679.483327	46200.128804	32.561383
679.856811	46285.513046	32.566400
680.567210	46359.710509	32.571418
680.793502	46459.453203	32.576436
681.514195	46535.635909	32.581453
682.287570	46635.216066	32.586471
683.244656	46724.395849	32.591488
684.281019	46810.423968	32.596506
684.534970	46902.143411	32.601524
684.901367	46983.426722	32.606541
686.142668	47062.698797	32.611559
687.015649	47153.760887	32.616576
688.093563	47215.379511	32.621594
689.665489	47289.383891	32.626612
691.170066	47355.526949	32.631629
691.589706	47418.319755	32.636647
692.114802	47478.240446	32.641664
693.212323	47542.001145	32.646682
693.734723	47598.985734	32.651700
694.352544	47657.119956	32.656717
694.900073	47713.424901	32.661735
695.254960	47794.612533	32.666752
696.580616	47828.647683	32.671770
697.022735	47903.265210	32.676788
697.597885	47965.831887	32.681805
698.238992	48030.573204	32.686823
699.113462	48105.580820	32.691840
699.739954	48173.461026	32.696858
699.890939	48245.462793	32.701876
700.461931	48313.068479	32.706893
701.145063	48388.617431	32.711911
701.472171	48483.313610	32.716928
701.887635	48556.633799	32.721946
702.041057	48654.508344	32.726964
702.822342	48746.101730	32.731981
703.494409	48849.778030	32.736999
704.063562	48951.990769	32.742016
704.283463	49059.564721	32.747034
705.163551	49155.517822	32.752052
705.891891	49269.028172	32.757069
706.257514	49372.663423	32.762087
706.673490	49486.296396	32.767104
707.809224	49588.996430	32.772122
708.572857	49704.025801	32.777140
709.495782	49804.946270	32.782157
710.103096	49921.127268	32.787175
710.913490	50026.849372	32.792192
711.493412	50118.703817	32.797210
713.209542	50215.085603	32.802228
714.289582	50314.349748	32.807245
715.263905	50399.134620	32.812263
716.116580	50481.586998	32.817280
716.856639	50574.708845	32.822298
717.267527	50654.550590	32.827316
718.041866	50747.680213	32.832333
718.689585	50829.384789	32.837351
719.166492	50934.977718	32.842368
720.076753	51013.474620	32.847386
720.400654	51109.744568	32.852404
721.101578	51203.223378	32.857421
721.960477	51294.515926	32.862439
723.054183	51374.607360	32.867456
724.520867	51437.921734	32.872474
725.302421	51522.734058	32.877492
726.326584	51581.333866	32.882509
727.821228	51634.612366	32.887527
728.335333	51693.480393	32.892544
728.870615	51739.602972	32.897562
729.502758	51805.982034	32.902580
730.124516	51859.810378	32.907597
730.345456	51915.057340	32.912615
730.662885	51995.280212	32.917632
731.303174	52064.830159	32.922650
731.887265	52143.139401	32.927668
732.166473	52230.931621	32.932685
732.785982	52305.287188	32.937703
733.054359	52398.306564	32.942720
733.943743	52485.385827	32.947738
734.848458	52579.292288	32.952756
735.041421	52682.692768	32.957773
735.623756	52781.745757	32.962791
736.038977	52886.430813	32.967808
737.399929	52988.659761	32.972826
738.048646	53093.913670	32.977844
738.303299	53204.546857	32.982861
739.126138	53308.749524	32.987879
739.599351	53423.719626	32.992896
740.578867	53527.575233	32.997914
741.600973	53635.158239	33.002932
742.009257	53751.341452	33.007949
743.011804	53852.130722	33.012967
743.759518	53969.661481	33.017984
744.697405	54068.541900	33.023002
745.867384	54173.493929	33.028020
746.623059	54269.714082	33.033037
747.828106	54372.222536	33.038055
748.692320	54461.608267	33.043072
749.516247	54553.218802	33.048090
750.498468	54641.884434	33.053108
751.244176	54733.420336	33.058125
752.214985	54825.487945	33.063143
752.570518	54922.700191	33.068160
753.619687	55005.227515	33.073178
754.410899	55099.613481	33.078196
755.017719	55190.138332	33.083213
756.237456	55268.891593	33.088231
756.203926	55366.568672	33.093248
757.014361	55451.191010	33.098266
757.809350	55543.878778	33.103284
758.310303	55643.610492	33.108301
759.524525	55728.362860	33.113319
760.091291	55837.246649	33.118336
760.909626	55925.117497	33.123354
762.261858	56012.280868	33.128372
762.929958	56093.132021	33.133389
764.343841	56178.668289	33.138407
765.285825	56245.636472	33.143424
765.818172	56332.690925	33.148442
766.533432	56400.619817	33.153460
767.264487	56481.866506	33.158477
768.168359	56558.010761	33.163495
768.467640	56648.277371	33.168512
769.103584	56724.018094	33.173530
770.160940	56814.134337	33.178548
770.348738	56908.982938	33.183565
771.160562	56992.095047	33.188583
772.122118	57071.517589	33.193600
772.639375	57171.721866	33.198618
773.316863	57252.007446	33.203636
773.985346	57355.852631	33.208653
774.832900	57455.358945	33.213671
775.288790	57538.570328	33.218688
776.069636	57638.764784	33.223706
777.086211	57727.596474	33.228724
777.639487	57820.094828	33.233741
778.122897	57907.985778	33.238759
779.033481	57999.477747	33.243776
780.148641	58075.978197	33.248794
781.079912	58161.084897	33.253812
781.479499	58232.750316	33.258829
782.418049	58319.309948	33.263847
783.043783	58419.723638	33.268864
784.024265	58507.035457	33.273882
785.098472	58589.042640	33.278900
785.896758	58689.909320	33.283917
786.868521	58769.355860	33.288935
787.299008	58860.097258	33.293952
787.888374	58937.623577	33.298970
788.559063	59040.946261	33.303988
788.960179	59154.773353	33.309005
790.483824	59241.600052	33.314023
791.008521	59346.781262	33.319040
791.663199	59434.732604	33.324058
793.078934	59518.020357	33.329076
793.746740	59612.795716	33.334093
794.846974	59703.916358	33.339111
795.636608	59798.305809	33.344128
796.578283	59879.303775	33.349146
797.468290	59963.767666	33.354164
797.778465	60062.889437	33.359181
798.393745	60145.345688	33.364199
799.131969	60244.586893	33.369216
799.697109	60351.055896	33.374234
800.481044	60455.397177	33.379252
800.846836	60557.084416	33.384269
801.585957	60663.140644	33.389287
802.669683	60781.439376	33.394304
803.164236	60889.028951	33.399322
803.976789	61001.205402	33.404340
804.664263	61124.299480	33.409357
805.144493	61233.454371	33.414375
805.715842	61366.530082	33.419392
806.282361	61484.861865	33.424410
807.484280	61616.652612	33.429428
807.705340	61749.776321	33.434445
808.454489	61873.951806	33.439463
809.742228	62012.613952	33.444480
810.778469	62129.076437	33.449498
811.687558	62251.596938	33.454516
812.555612	62373.138950	33.459533
813.735692	62490.123192	33.464551
814.623590	62615.677024	33.469568
815.335490	62734.459626	33.474586
816.251819	62853.569271	33.479604
817.153483	62968.522887	33.484621
818.701764	63070.576247	33.489639
819.615716	63174.448388	33.494656
820.609001	63276.942549	33.499674
822.077050	63371.242220	33.504692
822.394016	63489.266677	33.509709
822.975201	63583.240448	33.514727
823.752554	63679.514577	33.519744
824.079123	63782.836204	33.524762
824.918862	63886.300729	33.529780
825.780434	64011.545053	33.534797
826.580113	64124.227433	33.539815
827.247082	64232.817298	33.544832
827.794324	64353.621430	33.549850
828.650246	64469.861580	33.554868
828.997770	64589.107251	33.559885
829.688665	64708.960361	33.564903
830.345133	64835.242487	33.569920
831.030601	64955.331812	33.574938
831.731006	65067.346745	33.579956
832.346791	65203.309813	33.584973
833.155503	65319.954487	33.589991
833.896659	65462.997613	33.595008
834.623937	65589.493815	33.600026
836.000673	65717.280086	33.605044
836.803261	65844.833707	33.610061
837.941245	65969.437046	33.615079
839.148528	66074.457190	33.620096
839.949908	66200.508583	33.625114
840.982789	66308.466916	33.630132
842.091353	66430.353139	33.635149
843.249086	66539.006318	33.640167
844.165879	66644.241909	33.645184
844.992209	66758.122639	33.650202
846.007674	66859.094513	33.655220
846.948798	66972.913100	33.660237
847.534153	67084.388937	33.665255
848.385445	67194.544144	33.670272
849.018008	67306.474841	33.675290
850.078209	67416.798847	33.680308
850.927625	67525.660036	33.685325
852.031124	67645.094780	33.690343
852.954960	67750.296802	33.695360
853.574275	67863.617248	33.700378
854.852350	67968.249447	33.705396
855.802517	68079.967148	33.710413
856.833077	68175.613008	33.715431
857.913032	68285.198546	33.720448
858.210138	68396.501545	33.725466
859.097575	68502.048444	33.730484
859.806273	68618.177961	33.735501
860.632515	68721.927847	33.740519
862.350339	68810.254699	33.745536
863.962023	68895.311739	33.750554
865.464218	68990.168534	33.755572
865.836823	69077.638593	33.760589
866.918892	69169.562619	33.765607
867.874265	69245.833864	33.770624
868.309169	69330.740215	33.775642
869.073939	69421.485045	33.780660
870.008493	69514.124234	33.785677
870.845971	69595.974107	33.790695
871.632942	69694.531516	33.795712
872.299483	69782.486808	33.800730
873.063626	69887.650060	33.805748
873.661676	69984.210486	33.810765
874.426270	70092.220025	33.815783
875.299852	70179.712622	33.820800
875.521799	70303.532447	33.825818
876.555225	70395.356016	33.830836
877.164232	70519.650314	33.835853
877.799395	70636.150803	33.840871
878.620157	70756.832397	33.845888
879.015776	70875.074892	33.850906
879.994515	70995.244714	33.855924
880.684107	71130.879516	33.860941
881.431045	71259.296994	33.865959
882.885194	71384.176889	33.870976
883.363633	71510.692816	33.875994
884.332271	71639.012528	33.881012
885.592733	71763.680154	33.886029
887.031041	71871.346529	33.891047
887.982981	71989.167657	33.896064
888.865752	72109.890808	33.901082
889.589006	72209.785654	33.906100
890.454682	72326.668065	33.911117
891.418915	72425.094754	33.916135
892.408902	72517.307690	33.921152
893.026576	72623.773379	33.926170
894.258933	72729.378716	33.931188
894.957552	72841.200959	33.936205
895.319937	72951.157122	33.941223
896.388307	73059.674973	33.946240
897.042031	73180.340920	33.951258
897.946733	73286.155121	33.956276
898.327330	73425.966180	33.961293
899.356727	73539.330767	33.966311
900.652529	73661.359996	33.971328
901.262352	73777.375685	33.976346
902.081481	73906.169991	33.981364
903.074929	74036.763819	33.986381
903.933140	74163.636926	33.991399
904.945625	74285.084241	33.996416
905.502075	74430.956492	34.001434
906.129952	74562.208613	34.006452
907.405002	74694.650611	34.011469
908.330969	74837.302046	34.016487
909.165499	74954.342858	34.021504
909.811361	75091.489557	34.026522
910.914991	75239.863091	34.031540
911.866809	75384.341579	34.036557
912.580140	75524.724292	34.041575
914.702277	75621.670355	34.046592
915.707839	75759.318087	34.051610
917.443712	75861.382742	34.056628
918.842457	75974.401367	34.061645
919.860183	76081.500561	34.066663
920.669869	76194.358757	34.071680
921.471521	76298.275531	34.076698
921.943711	76404.701522	34.081716
923.063038	76515.024290	34.086733
923.883450	76633.739812	34.091751
925.015802	76750.114559	34.096768
925.296198	76868.086059	34.101786
926.204362	76983.797163	34.106804
926.884378	77103.556829	34.111821
927.192147	77244.068356	34.116839
928.287466	77370.825691	34.121856
928.778036	77518.247301	34.126874
929.852054	77654.573478	34.131892
930.508247	77796.213480	34.136909
931.158078	77935.496095	34.141927
932.173401	78085.250630	34.146944
932.919974	78239.269809	34.151962
933.739168	78393.202090	34.156980
934.461658	78539.877173	34.161997
935.035083	78695.579174	34.167015
936.020922	78848.120609	34.172032
936.860740	79022.200724	34.177050
937.564272	79186.904868	34.182068
938.706508	79356.155179	34.187085
939.495957	79528.482696	34.192103
940.754764	79685.969210	34.197120
941.940035	79847.985683	34.202138
942.903510	80005.839734	34.207156
943.964136	80157.814622	34.212173
945.021227	80316.597872	34.217191
946.319013	80465.827953	34.222208
947.540287	80618.335965	34.227226
949.131324	80752.988312	34.232244
950.659038	80878.940878	34.237261
951.887322	81013.357644	34.242279
952.960856	81132.908993	34.247296
954.129256	81245.094138	34.252314
954.885509	81356.937026	34.257332
956.244748	81464.239336	34.262349
956.907169	81565.900832	34.267367
957.733547	81670.584876	34.272384
958.675315	81787.061614	34.277402
959.848584	81887.134087	34.282420
961.061614	81989.876486	34.287437
962.112117	82097.846681	34.292455
962.773512	82200.301982	34.297472
963.290711	82320.053106	34.302490
964.218491	82429.766050	34.307508
965.023799	82542.587224	34.312525
965.086313	82680.629962	34.317543
966.177330	82809.367139	34.322560
966.669317	82947.650218	34.327578
967.554070	83094.739048	34.332596
968.177400	83239.221278	34.337613
968.559672	83400.017022	34.342631
969.671594	83551.702314	34.347648
970.991580	83705.714016	34.352666
972.502599	83843.048826	34.357684
974.019675	83981.794367	34.362701
974.487704	84135.292307	34.367719
975.163846	84288.320160	34.372736
976.060076	84435.706676	34.377754
977.233552	84587.053211	34.382772
978.715610	84727.865363	34.387789
979.517735	84880.047351	34.392807
980.810633	85033.775004	34.397824
981.964438	85175.764272	34.402842
982.602383	85324.293913	34.407860
983.639612	85471.334576	34.412877
984.076758	85628.776816	34.417895
985.173726	85779.605972	34.422912
986.284770	85933.451995	34.427930
986.850346	86081.688412	34.432948
988.073803	86242.598356	34.437965
988.679973	86413.862631	34.442983
990.053971	86574.661287	34.448000
990.834215	86726.795657	34.453018
991.295913	86901.023528	34.458036
992.677635	87057.521315	34.463053
993.310419	87239.398950	34.468071
994.631395	87415.285150	34.473088
995.552424	87585.474252	34.478106
996.228512	87757.312540	34.483124
997.264818	87934.237013	34.488141
997.956048	88115.004277	34.493159
999.269514	88281.361712	34.498176
1000.238719	88461.851352	34.503194
1001.254123	88636.069733	34.508212
1002.573398	88805.999012	34.513229
1004.512698	88979.478071	34.518247
1005.651624	89139.333306	34.523264
1006.652142	89303.503251	34.528282
1007.198349	89458.162088	34.533300
1008.486502	89613.205089	34.538317
1009.314038	89779.976386	34.543335
1010.465915	89941.397993	34.548352
1011.409518	90095.153302	34.553370
1012.673712	90270.063791	34.558388
1013.705731	90418.439782	34.563405
1014.522759	90576.041721	34.568423
1016.221269	90728.726509	34.573440
1018.431679	90854.828491	34.578458
1020.043035	90997.289401	34.583476
1020.764263	91109.241649	34.588493
1021.501514	91233.748356	34.593511
1022.515209	91355.222562	34.598528
1023.144550	91487.450832	34.603546
1023.766732	91600.428103	34.608564
1024.796418	91731.002688	34.613581
1025.207208	91875.111017	34.618599
1025.805655	92020.701728	34.623616
1026.675446	92168.596411	34.628634
1027.440467	92322.325928	34.633652
1028.491577	92474.439291	34.638669
1028.792502	92649.406592	34.643687
1029.277898	92810.033891	34.648704
1030.289838	92991.252984	34.653722
1030.970275	93177.098283	34.658740
1031.999088	93353.108135	34.663757
1033.333064	93542.012507	34.668775
1034.159131	93717.476304	34.673792
1036.185425	93892.830820	34.678810
1037.939478	94052.844347	34.683828
1039.978817	94197.620296	34.688845
1041.150542	94365.043290	34.693863
1042.321575	94505.027928	34.698880
1043.501453	94646.195571	34.703898
1044.205850	94799.520278	34.708916
1045.404973	94947.902491	34.713933
1046.281234	95098.504003	34.718951
1047.185094	95256.299031	34.723968
1048.140060	95420.422929	34.728986
1048.773153	95580.771637	34.734004
1049.765814	95740.004594	34.739021
1050.372196	95916.014231	34.744039
1051.512596	96078.181018	34.749056
1052.992721	96239.210027	34.754074
1053.435751	96414.838831	34.759092
1054.476595	96577.506490	34.764109
1055.738232	96755.413713	34.769127
1056.950662	96926.056742	34.774144
1058.820771	97087.400016	34.779162
1060.041807	97246.642691	34.784180
1062.185609	97368.275627	34.789197
1063.124910	97527.617479	34.794215
1063.930863	97671.839705	34.799232
1065.013206	97819.789950	34.804250
1065.500364	97981.792596	34.809268
1066.527259	98135.616093	34.814285
1067.503493	98303.585481	34.819303
1068.209158	98472.309928	34.824320
1069.284313	98643.531851	34.829338
1069.669033	98807.012880	34.834356
1070.820720	98977.933148	34.839373
1071.402131	99175.583530	34.844391
1072.037426	99350.377903	34.849408
1073.049502	99543.382376	34.854426
1073.530060	99748.587900	34.859444
1074.483438	99942.934673	34.864461
1075.694600	100147.610665	34.869479
1076.446547	100355.992299	34.874496
1077.514829	100557.105457	34.879514
1078.925330	100762.196488	34.884532
1080.206426	100955.952093	34.889549
1081.138592	101163.607609	34.894567
1082.974968	101354.576896	34.899584
1084.584393	101535.613071	34.904602
1086.268701	101703.968589	34.909620
1087.870525	101879.113736	34.914637
1089.201483	102049.176360	34.919655
1090.347099	102218.637683	34.924672
1091.656552	102372.142246	34.929690
1092.147723	102533.983150	34.934708
1092.947958	102685.357928	34.939725
1094.136867	102852.061869	34.944743
1095.038190	103010.956698	34.949760
1096.019978	103170.649637	34.954778
1096.623067	103348.281583	34.959796
1097.584143	103516.464944	34.964813
1098.537349	103703.950850	34.969831
1099.202828	103873.413975	34.974848
1100.001725	104063.562222	34.979866
1100.580323	104265.994890	34.984884
1103.191611	104423.968735	34.989901
1105.224585	104589.004998	34.994919
1106.272624	104759.119598	34.999936
1107.519292	104928.987044	35.004954
1108.317598	105101.196976	35.009972
1109.646359	105268.621347	35.014989
1110.812303	105444.534004	35.020007
1111.352662	105619.107803	35.025024
1112.526632	105789.930070	35.030042
1113.188292	105993.958041	35.035060
1114.283465	106175.092713	35.040077
1115.108372	106357.843972	35.045095
1115.876952	106552.891380	35.050112
1116.993680	106749.782298	35.055130
1117.851278	106954.000442	35.060148
1119.133384	107158.922334	35.065165
1120.121575	107366.199754	35.070183
1120.873632	107591.453015	35.075200
1122.001403	107780.484105	35.080218
1123.358939	107995.583429	35.085236
1124.505419	108205.323648	35.090253
1126.423904	108395.583179	35.095271
1127.787407	108594.093341	35.100288
1129.238105	108793.654490	35.105306
1130.387652	108988.884409	35.110324
1131.665134	109187.843873	35.115341
1132.788365	109369.780815	35.120359
1134.550935	109544.076089	35.125376
1136.364813	109713.246504	35.130394
1137.063900	109910.901191	35.135412
1138.631386	110084.104926	35.140429
1140.265083	110253.473269	35.145447
1140.434571	110446.165463	35.150464
1141.721598	110607.081059	35.155482
1142.801606	110788.768639	35.160500
1144.114265	110954.622354	35.165517
1145.344821	111139.137488	35.170535
1146.596476	111313.490830	35.175552
1147.657011	111492.209382	35.180570
1148.611447	111674.658393	35.185588
1149.615158	111851.843220	35.190605
1150.576801	112029.162846	35.195623
1151.699443	112218.783017	35.200640
1153.026859	112394.448119	35.205658
1153.738713	112591.638591	35.210676
1154.794975	112771.303585	35.215693
1155.901182	112962.160406	35.220711
1156.525852	113168.718791	35.225728
1157.616732	113361.987930	35.230746
1158.565351	113575.628057	35.235764
1159.611524	113783.134570	35.240781
1160.241518	113992.231940	35.245799
1160.853570	114220.185413	35.250816
1161.864467	114444.628557	35.255834
1162.915102	114669.611681	35.260852
1163.594400	114914.929207	35.265869
1164.709272	115149.496230	35.270887
1165.884388	115376.934898	35.275904
1167.127284	115600.411208	35.280922
1168.039677	115831.862728	35.285940
1169.010873	116061.089150	35.290957
1170.414223	116288.623970	35.295975
1171.092891	116526.784340	35.300992
1172.360437	116774.364335	35.306010
1173.068622	117019.745940	35.311028
1174.372657	117259.987974	35.316045
1175.771918	117513.672333	35.321063
1176.746868	117766.947837	35.326080
1178.146399	118009.841141	35.331098
1179.996198	118245.122637	35.336116
1181.403388	118478.224046	35.341133
1183.535261	118707.228407	35.346151
1184.725097	118944.018893	35.351168
1185.836548	119173.931147	35.356186
1187.624528	119390.985602	35.361204
1188.824958	119621.634247	35.366221
1190.518024	119837.896808	35.371239
1191.596916	120057.582827	35.376256
1193.024918	120268.697174	35.381274
1194.259243	120483.963517	35.386292
1195.786179	120694.126803	35.391309
1197.153353	120903.937936	35.396327
1198.177619	121109.650998	35.401344
1199.526785	121313.360084	35.406362
1200.955520	121511.139425	35.411380
1202.344352	121722.752257	35.416397
1204.060396	121924.389794	35.421415
1205.407875	122108.855196	35.426432
1206.656665	122302.525759	35.431450
1207.918775	122498.552496	35.436468
1209.011263	122694.634008	35.441485
1210.543481	122895.903105	35.446503
1210.977194	123097.229050	35.451520
1211.980349	123293.240601	35.456538
1213.256762	123501.653109	35.461556
1213.657465	123719.184961	35.466573
1214.977081	123930.533467	35.471591
1216.001478	124148.028329	35.476608
1217.172780	124362.978369	35.481626
1218.582365	124591.958085	35.486644
1219.455595	124798.545412	35.491661
1220.621684	125026.085985	35.496679
1221.693516	125250.728912	35.501696
1223.265489	125469.321109	35.506714
1225.228149	125688.686559	35.511732
1226.959675	125894.125044	35.516749
1228.766315	126096.485295	35.521767
1229.687422	126311.832832	35.526784
1231.013947	126494.655553	35.531802
1232.155160	126698.625738	35.536820
1233.340393	126910.384818	35.541837
1234.386238	127108.492554	35.546855
1234.920989	127322.479026	35.551872
1236.175796	127533.635136	35.556890
1237.241913	127745.470406	35.561908
1237.806844	127978.443391	35.566925
1239.190464	128203.702633	35.571943
1240.296785	128439.796069	35.576960
1241.375294	128661.446112	35.581978
1242.756700	128905.343432	35.586996
1243.543014	129141.317801	35.592013
1245.030491	129364.349995	35.597031
1246.814392	129592.924563	35.602048
1247.950606	129822.140607	35.607066
1249.779037	130027.793247	35.612084
1250.964615	130235.163698	35.617101
1252.855223	130434.774957	35.622119
1253.870594	130653.939694	35.627136
1254.939490	130839.720789	35.632154
1256.300336	131047.219604	35.637172
1256.791365	131253.913326	35.642189
1258.238363	131471.693779	35.647207
1259.098684	131690.764618	35.652224
1260.280343	131909.403363	35.657242
1261.414493	132129.724799	35.662260
1262.320908	132359.086006	35.667277
1263.723030	132590.585074	35.672295
1264.624124	132832.120295	35.677312
1265.543424	133059.950451	35.682330
1266.975648	133303.619582	35.687348
1267.531721	133548.855717	35.692365
1269.429000	133789.117262	35.697383
1271.581043	134013.212693	35.702400
1273.423831	134242.457307	35.707418
1275.303358	134460.655287	35.712436
1276.515197	134675.707315	35.717453
1278.528367	134892.098464	35.722471
1279.686345	135109.494978	35.727488
1280.911151	135315.459066	35.732506
1282.636144	135523.446028	35.737524
1283.775104	135751.905135	35.742541
1285.317678	135952.622501	35.747559
1286.313708	136166.325480	35.752576
1287.519127	136370.955483	35.757594
1288.950738	136583.004117	35.762612
1289.880658	136798.116751	35.767629
1291.167244	137021.032315	35.772647
1292.256165	137240.888568	35.777664
1293.220217	137461.096624	35.782682
1294.778416	137681.676702	35.787700
1295.794629	137909.169358	35.792717
1297.527674	138127.834217	35.797735
1298.699605	138348.863110	35.802752
1300.045430	138583.672183	35.807770
1301.089980	138810.633702	35.812788
1302.485036	139043.624675	35.817805
1303.441908	139276.664565	35.822823
1304.482121	139512.963534	35.827840
1305.766916	139754.751870	35.832858
1306.814644	139995.249873	35.837876
1307.783171	140253.425594	35.842893
1309.192325	140501.246825	35.847911
1310.258271	140770.644624	35.852928
1310.895244	141018.635690	35.857946
1312.082138	141292.316037	35.862964
1312.790589	141574.624380	35.867981
1314.184601	141842.099447	35.872999
1315.450020	142126.779892	35.878016
1316.666240	142411.749795	35.883034
1318.165842	142695.432322	35.888052
1319.013878	142986.630767	35.893069
1320.393062	143269.450259	35.898087
1321.959000	143555.030862	35.903104
1323.103783	143853.922654	35.908122
1324.508341	144150.174248	35.913140
1325.818191	144448.612524	35.918157
1327.300387	144739.568071	35.923175
1328.618310	145040.254574	35.928192
1330.119994	145315.524591	35.933210
1331.709257	145608.282924	35.938228
1333.342456	145897.307913	35.943245
1334.745765	146180.767953	35.948263
1336.100670	146455.690589	35.953280
1337.740764	146722.071024	35.958298
1339.609198	146965.866655	35.963316
1340.412900	147230.195515	35.968333
1341.935679	147487.330290	35.973351
1343.272460	147745.296716	35.978368
1344.594086	148013.248620	35.983386
1345.852400	148259.221326	35.988404
1347.078035	148534.269849	35.993421
1348.686669	148784.170335	35.998439
1350.432162	149041.570764	36.003456
1351.478306	149318.443177	36.008474
1353.170323	149568.994648	36.013492
1354.146558	149838.703918	36.018509
1355.640449	150099.958350	36.023527
1356.640701	150375.425702	36.028544
1358.036609	150643.980413	36.033562
1359.611053	150916.667628	36.038580
1360.684927	151177.707495	36.043597
1362.295647	151447.462620	36.048615
1363.926741	151721.998075	36.053632
1365.169200	151991.615202	36.058650
1366.531872	152262.837850	36.063668
1367.564397	152548.500898	36.068685
1369.173026	152820.498497	36.073703
1370.370514	153108.180509	36.078720
1371.831023	153392.193332	36.083738
1372.872501	153670.049681	36.088756
1373.816817	153964.109590	36.093773
1375.116630	154257.047265	36.098791
1376.441512	154559.039879	36.103808
1377.145007	154866.262542	36.108826
1378.868661	155175.576356	36.113844
1380.385202	155489.569673	36.118861
1381.998203	155778.597871	36.123879
1383.973224	156066.616763	36.128896
1385.493410	156375.491701	36.133914
1387.242759	156663.438187	36.138932
1388.826353	156964.962347	36.143949
1390.362783	157240.960524	36.148967
1392.570169	157506.967208	36.153984
1394.068962	157791.982244	36.159002
1395.479244	158057.059150	36.164020
1396.681659	158338.587850	36.169037
1398.057368	158624.149295	36.174055
1399.376187	158907.654348	36.179072
1400.831089	159170.447636	36.184090
1402.988220	159440.128989	36.189108
1404.383197	159728.206856	36.194125
1405.586606	159984.513602	36.199143
1407.611813	160232.769286	36.204160
1408.819579	160501.295638	36.209178
1410.501771	160757.400927	36.214196
1411.781941	161017.621536	36.219213
1413.158441	161273.717267	36.224231
1414.293815	161535.550976	36.229248
1415.450180	161812.061693	36.234266
1417.126003	162068.785069	36.239284
1418.229692	162335.576985	36.244301
1419.689213	162603.301189	36.249319
1421.028918	162879.547456	36.254336
1422.010933	163148.394646	36.259354
1423.195401	163418.542149	36.264372
1424.611779	163695.529563	36.269389
1426.476383	163980.285409	36.274407
1427.526199	164255.941589	36.279424
1428.816927	164537.725861	36.284442
1430.080728	164828.943539	36.289460
1431.499733	165098.364879	36.294477
1432.595918	165374.857911	36.299495
1434.199040	165649.492301	36.304512
1435.175620	165924.714461	36.309530
1436.684773	166203.390074	36.314548
1437.909990	166489.207336	36.319565
1438.747840	166771.588669	36.324583
1439.898632	167061.837560	36.329600
1441.111100	167355.859333	36.334618
1442.491664	167660.818217	36.339636
1443.803466	167971.170635	36.344653
1445.147368	168271.114997	36.349671
1447.396909	168578.296173	36.354688
1448.532553	168895.218999	36.359706
1450.497141	169203.314531	36.364724
1451.671985	169517.798894	36.369741
1453.043454	169826.986756	36.374759
1454.649275	170129.031787	36.379776
1455.798621	170460.530655	36.384794
1456.988712	170777.673237	36.389812
1458.338958	171109.143452	36.394829
1459.861430	171441.716866	36.399847
1461.016760	171768.313161	36.404864
1462.424528	172103.968565	36.409882
1464.267070	172428.044425	36.414900
1465.665724	172774.188085	36.419917
1466.837097	173117.097888	36.424935
1468.776397	173441.735710	36.429952
1470.368592	173787.905429	36.434970
1472.371545	174114.440829	36.439988
1473.999166	174446.015381	36.445005
1475.482804	174771.854530	36.450023
1477.618957	175099.326312	36.455040
1478.526981	175425.836374	36.460058
1480.725424	175731.981512	36.465076
1482.420753	176060.916147	36.470093
1483.583602	176380.270675	36.475111
1485.276095	176705.364688	36.480128
1486.177828	177040.364192	36.485146
1487.661313	177370.649853	36.490164
1488.853662	177703.270419	36.495181
1490.247902	178037.699980	36.500199
1491.709295	178372.057168	36.505216
1493.402374	178724.438377	36.510234
1495.081412	179065.604856	36.515252
1496.560820	179404.382574	36.520269
1497.854735	179744.716314	36.525287
1499.212355	180088.278199	36.530304
1500.818070	180439.149947	36.535322
1502.065904	180786.250366	36.540340
1503.838880	181122.883767	36.545357
1505.500516	181477.281669	36.550375
1507.111015	181812.182192	36.555392
1508.761787	182153.868644	36.560410
1510.450708	182491.667041	36.565428
1512.058672	182842.782904	36.570445
1513.387562	183170.503848	36.575463
1515.118010	183514.051615	36.580480
1516.780033	183862.766226	36.585498
1518.183406	184205.395248	36.590516
1519.645359	184542.089052	36.595533
1520.804597	184893.432217	36.600551
1522.773269	185223.839244	36.605568
1524.726151	185552.270710	36.610586
1526.526916	185877.111729	36.615604
1527.905821	186217.129769	36.620621
1529.437537	186540.318323	36.625639
1531.412279	186857.050410	36.630656
1532.661045	187186.065151	36.635674
1533.931428	187500.658136	36.640692
1535.662099	187784.978010	36.645709
1537.083952	188102.392600	36.650727
1538.484794	188413.833583	36.655744
1539.472484	188718.769247	36.660762
1540.681454	189040.806811	36.665780
1542.149721	189356.570344	36.670797
1543.666234	189693.234933	36.675815
1545.012375	190010.710556	36.680832
1546.463536	190344.673118	36.685850
1548.564710	190680.167374	36.690868
1550.303359	191002.229375	36.695885
1552.025156	191334.997407	36.700903
1553.984647	191651.694559	36.705920
1555.578972	191982.151475	36.710938
1557.142594	192298.346364	36.715956
1558.961467	192624.491397	36.720973
1560.014671	192938.679557	36.725991
1562.097621	193260.874152	36.731008
1563.837229	193581.172305	36.736026
1565.259907	193902.273652	36.741044
1566.665352	194228.622597	36.746061
1568.060714	194552.194649	36.751079
1569.578231	194884.876009	36.756096
1570.918833	195227.033774	36.761114
1572.489574	195564.115135	36.766132
1573.974915	195896.134224	36.771149
1575.160803	196239.554478	36.776167
1576.785577	196584.338390	36.781184
1578.696764	196938.344488	36.786202
1579.876845	197274.801205	36.791220
1581.672671	197618.914698	36.796237
1583.181814	197992.189154	36.801255
1585.127590	198329.590723	36.806272
1586.929830	198674.292593	36.811290
1588.637124	199008.423429	36.816308
1590.477589	199348.704152	36.821325
1592.512845	199701.168024	36.826343
1594.055513	200031.700029	36.831360
1595.898590	200363.148733	36.836378
1597.130596	200706.330201	36.841396
1598.690758	201035.302411	36.846413
1600.278917	201388.572631	36.851431
1601.973424	201723.239201	36.856448
1603.791508	202075.636746	36.861466
1604.834892	202410.909636	36.866484
1607.070633	202746.621265	36.871501
1608.822740	203090.083490	36.876519
1610.479736	203420.790047	36.881536
1612.024834	203762.969266	36.886554
1613.682737	204101.360364	36.891572
1615.467915	204415.048858	36.896589
1617.167363	204769.586732	36.901607
1618.595015	205096.681988	36.906624
1619.936951	205441.048370	36.911642
1621.382245	205779.228301	36.916660
1622.912937	206130.321438	36.921677
1624.274702	206489.672075	36.926695
1625.766099	206824.407943	36.931712
1627.278109	207178.848333	36.936730
1628.728154	207532.932357	36.941748
1630.394890	207885.686884	36.946765
1631.691772	208253.411331	36.951783
1633.171419	208610.936286	36.956800
1634.913486	208978.183908	36.961818
1636.224301	209356.208939	36.966836
1637.935237	209718.081151	36.971853
1639.401355	210092.833147	36.976871
1640.788659	210439.664279	36.981888
1641.927458	210805.788282	36.986906
1643.635574	211166.537081	36.991924
1645.236686	211529.260657	36.996941
1646.299702	211895.935211	37.001959
1647.857844	212272.052945	37.006976
1649.775839	212651.769766	37.011994
1651.467768	213044.224075	37.017012
1653.486366	213389.540170	37.022029
1655.330053	213784.461470	37.027047
1657.080103	214159.691879	37.032064
1658.861911	214539.566253	37.037082
1660.727881	214915.059911	37.042100
1662.444336	215288.040133	37.047117
1663.904271	215662.918377	37.052135
1665.746398	216039.512592	37.057152
1667.049356	216437.582523	37.062170
1668.587726	216818.776341	37.067188
1670.517694	217205.138717	37.072205
1672.129893	217596.355509	37.077223
1673.650384	217993.913178	37.082240
1675.607627	218383.069429	37.087258
1676.999526	218779.051438	37.092276
1679.161071	219164.214697	37.097293
1680.880197	219586.153552	37.102311
1682.424083	220015.260173	37.107328
1684.072481	220414.914132	37.112346
1685.754633	220810.525593	37.117364
1687.642343	221208.136356	37.122381
1689.329650	221623.459484	37.127399
1691.289126	222004.983709	37.132416
1693.458169	222397.650145	37.137434
1694.773039	222791.475503	37.142452
1696.773358	223183.791661	37.147469
1698.388928	223586.332705	37.152487
1700.269099	223968.892680	37.157504
1702.514158	224365.668002	37.162522
1703.875779	224761.879886	37.167540
1705.818623	225139.886723	37.172557
1707.286150	225545.100549	37.177575
1708.763588	225940.789101	37.182592
1711.115048	226325.107257	37.187610
1713.987073	226681.908233	37.192628
1716.193553	227039.963529	37.197645
1718.392407	227416.258446	37.202663
1719.977015	227773.098035	37.207680
1721.637179	228141.051429	37.212698
1722.908099	228499.240389	37.217716
1724.761420	228853.498306	37.222733
1725.814058	229227.803887	37.227751
1727.306915	229604.856997	37.232768
1728.773433	229984.049151	37.237786
1729.926373	230363.726107	37.242804
1731.429875	230757.291029	37.247821
1733.918488	231142.565465	37.252839
1735.636692	231514.633083	37.257856
1737.411043	231907.495771	37.262874
1738.929552	232294.813638	37.267892
1740.649724	232683.496125	37.272909
1742.356594	233081.427834	37.277927
1743.547381	233474.797637	37.282944
1745.589949	233869.297307	37.287962
1746.902476	234275.578168	37.292980
1748.862827	234672.557328	37.297997
1750.170262	235065.251164	37.303015
1751.716511	235467.660533	37.308032
1753.515542	235877.090597	37.313050
1755.400653	236286.507342	37.318068
1757.013151	236666.326334	37.323085
1758.301620	237062.583982	37.328103
1759.750802	237472.939276	37.333120
1761.299604	237856.327502	37.338138
1762.746898	238279.004761	37.343156
1764.547414	238685.722714	37.348173
1766.030600	239113.272977	37.353191
1767.124660	239537.865758	37.358208
1768.769869	239966.508612	37.363226
1770.051931	240408.167639	37.368244
1771.680024	240860.871003	37.373261
1773.313700	241314.234807	37.378279
1774.978427	241759.999037	37.383296
1777.070338	242220.731549	37.388314
1778.530101	242703.898469	37.393332
1780.670230	243159.569637	37.398349
1783.230533	243619.236388	37.403367
1785.509282	244077.782069	37.408384
1787.190302	244519.661814	37.413402
1789.184009	244988.163259	37.418420
1791.430858	245441.712097	37.423437
1793.580890	245882.576271	37.428455
1794.817921	246347.928253	37.433472
1797.174111	246785.787382	37.438490
1799.024495	247255.128855	37.443508
1800.742084	247691.113539	37.448525
1802.618546	248141.653703	37.453543
1804.703518	248599.374293	37.458560
1806.579684	249045.698665	37.463578
1808.530617	249494.475222	37.468596
1810.916867	249930.300760	37.473613
1812.976121	250370.270798	37.478631
1814.769436	250812.012719	37.483648
1816.793011	251255.418879	37.488666
1818.690466	251692.165282	37.493684
1820.323819	252108.226811	37.498701
1822.748123	252546.740982	37.503719
1823.837357	252987.762969	37.508736
1825.802816	253425.642463	37.513754
1827.285638	253865.609045	37.518772
1829.081931	254321.451747	37.523789
1830.860285	254771.962974	37.528807
1832.142632	255233.200560	37.533824
1833.968722	255689.140567	37.538842
1835.192792	256157.932937	37.543860
1836.704382	256639.252436	37.548877
1838.602153	257109.864094	37.553895
1840.193514	257594.930289	37.558912
1842.035762	258074.721907	37.563930
1844.017552	258568.233634	37.568948
1846.229688	259040.114409	37.573965
1848.177599	259520.345837	37.578983
1850.334416	259996.351071	37.584000
1853.011333	260445.850645	37.589018
1855.332212	260911.972079	37.594036
1857.902972	261366.010848	37.599053
1859.516396	261818.582312	37.604071
1861.210817	262270.454320	37.609088
1862.969081	262710.960328	37.614106
1865.078268	263175.972941	37.619124
1866.811462	263613.231096	37.624141
1868.817645	264071.553867	37.629159
1870.787087	264523.633274	37.634176
1872.284341	264973.428141	37.639194
1874.066867	265429.348409	37.644212
1875.967550	265885.934653	37.649229
1877.822277	266342.223316	37.654247
1879.427354	266779.475235	37.659264
1881.458257	267220.466693	37.664282
1882.817285	267646.022405	37.669300
1884.908923	268080.855467	37.674317
1886.429635	268517.510105	37.679335
1888.365737	268959.150662	37.684352
1890.487415	269397.355995	37.689370
1892.155301	269813.662492	37.694388
1893.829257	270264.947308	37.699405
1895.592009	270708.341958	37.704423
1897.868916	271156.477389	37.709440
1900.119337	271601.365048	37.714458
1901.439173	272070.132451	37.719476
1903.256527	272509.679796	37.724493
1905.399441	272976.302621	37.729511
1907.204176	273436.528456	37.734528
1908.676271	273895.716338	37.739546
1909.921393	274377.015869	37.744564
1911.946021	274859.252277	37.749581
1913.992571	275333.710993	37.754599
1915.390554	275829.665084	37.759616
1917.123523	276316.773441	37.764634
1918.932726	276823.046891	37.769652
1920.270320	277325.688624	37.774669
1922.557125	277833.582619	37.779687
1924.924425	278353.299469	37.784704
1927.125885	278854.143379	37.789722
1928.781043	279348.827682	37.794740
1930.964116	279855.717832	37.799757
1933.060874	280374.864661	37.804775
1934.944320	280889.574699	37.809792
1937.628841	281383.498992	37.814810
1939.738754	281899.692783	37.819828
1941.293121	282395.884464	37.824845
1943.414137	282914.613591	37.829863
1945.810349	283423.134973	37.834880
1947.641958	283930.783090	37.839898
1948.838414	284445.901221	37.844916
1951.290095	284969.293734	37.849933
1953.186106	285485.080024	37.854951
1954.596884	286004.501112	37.859968
1956.676562	286530.998054	37.864986
1958.009702	287065.795866	37.870004
1960.146754	287611.025228	37.875021
1961.812484	288146.779944	37.880039
1963.306303	288691.476672	37.885056
1965.209784	289237.627396	37.890074
1966.758398	289803.951752	37.895092
1968.420110	290372.083760	37.900109
1970.386847	290948.976585	37.905127
1972.027197	291535.776063	37.910144
1974.129876	292109.059670	37.915162
1976.250473	292688.077978	37.920180
1977.449987	293275.856573	37.925197
1979.697985	293870.799020	37.930215
1981.344491	294470.689358	37.935232
1983.817782	295064.267583	37.940250
1985.786566	295667.222333	37.945268
1988.347396	296241.781294	37.950285
1991.461445	296820.004616	37.955303
1993.585672	297397.195067	37.960320
1995.989688	297963.338456	37.965338
1998.382767	298527.880490	37.970356
1999.998067	299097.602531	37.975373
2002.683335	299639.714150	37.980391
2004.901417	300208.644313	37.985408
2007.677938	300736.130999	37.990426
2009.454177	301292.200572	37.995444
2011.598936	301813.004864	38.000461
2013.865591	302329.849511	38.005479
2015.593273	302835.047049	38.010496
2017.572088	303336.974802	38.015514
2019.765958	303841.810242	38.020532
2021.506586	304345.778272	38.025549
2024.214360	304833.888087	38.030567
2025.751233	305346.163562	38.035584
2028.198945	305833.117297	38.040602
2029.940375	306335.067532	38.045620
2031.897148	306842.871076	38.050637
2033.879807	307350.895867	38.055655
2035.472271	307866.981920	38.060672
2037.136800	308389.935069	38.065690
2039.164311	308900.685719	38.070708
2040.866120	309439.422018	38.075725
2042.926441	309969.740322	38.080743
2044.784768	310517.509547	38.085760
2046.647634	311050.926142	38.090778
2048.376604	311591.065473	38.095796
2050.332984	312153.078806	38.100813
2052.299589	312711.531124	38.105831
2054.400302	313275.442243	38.110848
2056.158378	313829.476861	38.115866
2058.427874	314408.333875	38.120884
2060.079082	314970.655991	38.125901
2061.876918	315563.446850	38.130919
2063.733052	316158.991022	38.135936
2065.695973	316762.739826	38.140954
2067.602512	317361.236520	38.145972
2069.485784	317972.707477	38.150989
2071.826350	318586.636500	38.156007
2073.861372	319188.981088	38.161024
2075.754170	319794.238534	38.166042
2078.156471	320428.860297	38.171060
2079.925976	321039.839949	38.176077
2082.403118	321659.228102	38.181095
2084.374285	322294.538021	38.186112
2086.465517	322900.673428	38.191130
2089.165508	323518.559520	38.196148
2091.227480	324144.720840	38.201165
2094.053445	324748.380931	38.206183
2096.200389	325355.473638	38.211200
2098.328656	325980.640621	38.216218
2100.876889	326591.589923	38.221236
2102.629164	327202.994919	38.226253
2104.904634	327808.823080	38.231271
2106.600922	328425.378653	38.236288
2109.082404	329034.079749	38.241306
2111.206092	329656.263843	38.246324
2113.685137	330256.853805	38.251341
2115.907956	330859.104673	38.256359
2118.331086	331468.119662	38.261376
2120.614993	332072.251488	38.266394
2123.357713	332660.561226	38.271412
2125.196440	333267.089328	38.276429
2127.057953	333853.526767	38.281447
2128.924857	334460.900068	38.286464
2131.258359	335056.918204	38.291482
2134.038720	335648.743332	38.296500
2136.463155	336220.516134	38.301517
2139.024864	336801.246089	38.306535
2141.435742	337380.547685	38.311552
2143.532572	337958.904862	38.316570
2145.699171	338522.673828	38.321588
2147.472564	339100.589437	38.326605
2149.551721	339666.238614	38.331623
2151.575767	340250.851470	38.336640
2153.516624	340833.186869	38.341658
2155.504117	341386.876690	38.346676
2156.889962	341953.350873	38.351693
2158.524983	342511.223672	38.356711
2160.042501	343086.292661	38.361728
2162.088330	343667.181090	38.366746
2164.317420	344249.301185	38.371764
2166.114586	344846.790052	38.376781
2168.052704	345449.171771	38.381799
2169.946558	346053.989566	38.386816
2171.662175	346669.919830	38.391834
2174.014036	347280.178559	38.396852
2176.168311	347911.805386	38.401869
2178.401133	348523.107848	38.406887
2180.557285	349156.798155	38.411904
2182.582642	349798.545928	38.416922
2184.871741	350431.967863	38.421940
2186.998141	351080.735359	38.426957
2188.734622	351725.370787	38.431975
2190.664720	352390.062571	38.436992
2192.935794	353043.953824	38.442010
2195.241436	353702.270159	38.447028
2197.507506	354370.758318	38.452045
2199.760691	355040.278498	38.457063
2202.122971	355709.186431	38.462080
2204.280545	356382.456541	38.467098
2206.635225	357066.390708	38.472116
2208.312119	357743.727398	38.477133
2210.325244	358433.835758	38.482151
2213.159240	359128.414264	38.487168
2214.890459	359825.497701	38.492186
2217.168357	360518.292332	38.497204
2218.999502	361232.536493	38.502221
2221.349530	361935.544369	38.507239
2223.746290	362647.512920	38.512256
2225.824453	363370.100334	38.517274
2228.306023	364086.442921	38.522292
2230.430619	364803.896839	38.527309
2232.660924	365515.206197	38.532327
2235.479781	366230.945626	38.537344
2237.361891	366949.261897	38.542362
2240.509015	367663.550033	38.547380
2243.190555	368381.452873	38.552397
2245.481831	369072.924870	38.557415
2248.131965	369781.522012	38.562432
2250.565433	370481.136937	38.567450
2253.419363	371167.175135	38.572468
2255.986682	371859.918436	38.577485
2258.427873	372543.893668	38.582503
2260.737481	373231.149405	38.587520
2262.801070	373907.577616	38.592538
2265.330619	374581.125963	38.597556
2267.611253	375266.470213	38.602573
2269.341613	375960.083641	38.607591
2271.671230	376628.654971	38.612608
2273.737004	377335.651589	38.617626
2275.783074	378020.828067	38.622644
2277.930070	378713.201301	38.627661
2280.356754	379412.715814	38.632679
2281.917503	380116.847503	38.637696
2284.508723	380805.452789	38.642714
2286.899090	381501.709437	38.647732
2289.193249	382202.328634	38.652749
2291.851998	382898.993203	38.657767
2294.402698	383590.285624	38.662784
2296.804582	384278.241257	38.667802
2299.663554	384966.436219	38.672820
2302.061054	385642.371201	38.677837
2304.166296	386311.621848	38.682855
2306.747915	386963.362593	38.687872
2309.472796	387596.914392	38.692890
2311.967298	388222.759498	38.697908
2314.044205	388870.767124	38.702925
2316.241781	389507.359109	38.707943
2318.876041	390135.221530	38.712960
2320.445912	390782.690266	38.717978
2323.074071	391420.971425	38.722996
2325.374163	392060.839851	38.728013
2327.555969	392701.348137	38.733031
2329.691666	393361.241033	38.738048
2331.674534	394017.266816	38.743066
2334.067318	394661.019038	38.748084
2336.537740	395322.663742	38.753101
2338.520844	395985.514946	38.758119
2340.650629	396655.524807	38.763136
2342.420049	397342.964853	38.768154
2344.640217	398044.861078	38.773172
2346.814041	398726.854300	38.778189
2348.734040	399431.149007	38.783207
2351.147806	400126.171296	38.788224
2353.188355	400862.999854	38.793242
2355.326137	401577.215479	38.798260
2357.216999	402316.894702	38.803277
2359.953606	403031.025302	38.808295
2362.777970	403761.567620	38.813312
2364.927505	404497.700814	38.818330
2367.384025	405241.440758	38.823348
2369.629968	405989.882780	38.828365
2371.754917	406745.519753	38.833383
2374.265383	407489.114207	38.838400
2376.409543	408259.932292	38.843418
2378.788276	409012.525834	38.848436
2381.127164	409786.232268	38.853453
2383.450787	410556.321882	38.858471
2386.078785	411323.907180	38.863488
2388.158226	412100.705372	38.868506
2390.962601	412886.428730	38.873524
2393.045200	413671.488287	38.878541
2395.505494	414454.739516	38.883559
2397.878667	415235.676875	38.888576
2399.725488	416048.969045	38.893594
2402.192438	416843.088089	38.898612
2404.673436	417647.816684	38.903629
2406.793230	418450.933670	38.908647
2409.372851	419269.598914	38.913664
2412.141066	420073.570099	38.918682
2414.159287	420893.794916	38.923700
2417.185805	421707.014674	38.928717
2419.580430	422525.528381	38.933735
2422.382296	423324.477266	38.938752
2424.733565	424140.817863	38.943770
2427.696696	424934.446876	38.948788
2430.110209	425736.596816	38.953805
2432.266199	426548.129734	38.958823
2434.481223	427368.182079	38.963840
2437.034401	428173.873384	38.968858
2439.895982	428991.079962	38.973876
2442.946850	429795.115396	38.978893
2445.236716	430587.606255	38.983911
2448.065895	431395.521946	38.988928
2449.889622	432203.930614	38.993946
2452.278239	433006.548641	38.998964
2454.543473	433822.319554	39.003981
2456.254901	434630.561277	39.008999
2458.807535	435450.984843	39.014016
2462.595744	436230.837896	39.019034
2465.946753	437010.736672	39.024052
2469.450333	437754.955952	39.029069
2472.044679	438492.520105	39.034087
2474.699982	439217.955688	39.039104
2477.098754	439951.253648	39.044122
2479.337682	440662.340318	39.049140
2481.882010	441392.834369	39.054157
2484.299144	442130.105458	39.059175
2486.762776	442845.638688	39.064192
2488.901233	443580.478797	39.069210
2491.291718	444309.839167	39.074228
2493.542367	445043.296146	39.079245
2495.753163	445791.456342	39.084263
2498.003536	446524.559745	39.089280
2500.238419	447295.579837	39.094298
2502.235888	448052.852811	39.099316
2504.434871	448827.870394	39.104333
2506.688934	449606.290086	39.109351
2509.289360	450388.771273	39.114368
2511.478014	451178.169970	39.119386
2513.837310	451978.940562	39.124404
2516.189947	452789.543220	39.129421
2518.441043	453603.569947	39.134439
2522.695422	454375.716607	39.139456
2525.657562	455177.781354	39.144474
2527.939955	455978.663246	39.149492
2530.430706	456779.631060	39.154509
2532.444152	457591.668633	39.159527
2534.590856	458408.454776	39.164544
2537.373359	459229.046146	39.169562
2539.991273	460048.519163	39.174580
2542.675365	460864.965203	39.179597
2544.869281	461700.213137	39.184615
2547.570852	462520.885290	39.189632
2549.964956	463367.251685	39.194650
2552.302938	464199.691572	39.199668
2554.856519	465037.872824	39.204685
2558.433548	465842.796014	39.209703
2562.122598	466656.309329	39.214720
2564.915202	467501.117160	39.219738
2567.509383	468314.287265	39.224756
2570.363841	469125.055555	39.229773
2573.194819	469929.527905	39.234791
2575.870037	470733.436382	39.239808
2578.749427	471525.050187	39.244826
2581.659611	472338.097893	39.249844
2583.987537	473122.359896	39.254861
2585.922431	473934.085636	39.259879
2588.481596	474742.237850	39.264896
2590.627140	475557.697531	39.269914
2593.418741	476377.207020	39.274932
2596.061767	477195.745186	39.279949
2597.666404	478031.136727	39.284967
2600.168707	478864.018568	39.289984
2601.992746	479698.944385	39.295002
2604.167987	480558.720916	39.300020
2606.320460	481414.723730	39.305037
2608.551635	482307.130579	39.310055
2611.242816	483182.502103	39.315072
2612.989502	484069.953434	39.320090
2615.105422	484967.750589	39.325108
2617.632593	485868.059670	39.330125
2620.061592	486799.840375	39.335143
2622.772735	487715.624115	39.340160
2625.282463	488651.331988	39.345178
2627.701991	489571.408212	39.350196
2630.161631	490504.299586	39.355213
2632.254729	491451.938487	39.360231
2635.186292	492394.491521	39.365248
2637.538945	493322.202052	39.370266
2639.795998	494241.552220	39.375284
2642.623838	495164.542844	39.380301
2644.981939	496111.073324	39.385319
2647.777389	497031.546004	39.390336
2650.805526	497957.176772	39.395354
2653.575256	498885.019010	39.400372
2656.112369	499819.658302	39.405389
2659.101342	500762.695044	39.410407
2661.924504	501705.957884	39.415424
2665.177159	502644.304508	39.420442
2667.198757	503592.635777	39.425460
2670.342019	504528.976538	39.430477
2672.608936	505478.872655	39.435495
2675.799884	506430.375740	39.440512
2678.293229	507384.762006	39.445530
2681.051551	508332.897066	39.450548
2683.950235	509288.364043	39.455565
2686.681415	510248.842975	39.460583
2690.174138	511202.887416	39.465600
2693.785164	512129.938266	39.470618
2696.605688	513079.646190	39.475636
2699.482843	514015.982009	39.480653
2701.722484	514967.234635	39.485671
2704.057651	515917.204233	39.490688
2706.621653	516867.833992	39.495706
2709.241923	517825.702508	39.500724
2712.556915	518770.750292	39.505741
2715.142620	519734.401197	39.510759
2717.912394	520695.039269	39.515776
2720.284963	521662.936778	39.520794
2722.460633	522641.131660	39.525812
2725.313599	523618.244856	39.530829
2727.443613	524616.064335	39.535847
2730.088209	525612.523938	39.540864
2732.398136	526615.972615	39.545882
2734.580280	527637.956158	39.550900
2737.524794	528639.955244	39.555917
2740.046961	529674.129073	39.560935
2742.516729	530692.430968	39.565952
2745.153323	531738.423167	39.570970
2747.735124	532785.608250	39.575988
2751.079442	533829.219716	39.581005
2753.315440	534889.447996	39.586023
2756.068287	535945.185101	39.591040
2758.841720	537016.290683	39.596058
2761.537730	538074.145636	39.601076
2764.439822	539147.536408	39.606093
2767.244233	540230.924837	39.611111
2770.289198	541296.583109	39.616128
2773.457887	542365.460677	39.621146
2776.228398	543438.347022	39.626164
2779.539271	544497.331058	39.631181
2782.617556	545569.299079	39.636199
2785.225653	546633.869927	39.641216
2788.477124	547697.548642	39.646234
2791.166622	548760.584773	39.651252
2794.044929	549814.055488	39.656269
2797.109235	550863.694271	39.661287
2800.167814	551918.883489	39.666304
2803.395487	552956.520812	39.671322
2806.044904	554004.176408	39.676340
2809.646667	555034.606108	39.681357
2812.980411	556055.050959	39.686375
2816.059036	557073.148833	39.691392
2820.178653	558049.794949	39.696410
2823.541952	559048.852473	39.701428
2827.023796	560003.504444	39.706445
2829.572315	560952.916919	39.711463
2832.046577	561873.842090	39.716480
2835.473828	562788.768798	39.721498
2838.064249	563703.619316	39.726516
2840.729677	564614.727152	39.731533
2843.427128	565532.796382	39.736551
2845.895673	566451.290423	39.741568
2848.574954	567369.031623	39.746586
2850.902643	568294.397108	39.751604
2853.041831	569232.478796	39.756621
2855.363422	570181.957336	39.761639
2857.613283	571141.366114	39.766656
2860.247039	572118.908966	39.771674
2862.448349	573117.025124	39.776692
2865.245993	574095.090933	39.781709
2868.093969	575104.886728	39.786727
2870.438514	576120.956599	39.791744
2873.093736	577130.871954	39.796762
2875.398648	578172.469578	39.801780
2878.050210	579223.253014	39.806797
2880.237177	580293.184998	39.811815
2882.638466	581369.308313	39.816832
2885.543004	582461.553127	39.821850
2888.163633	583566.835627	39.826868
2890.650427	584661.911677	39.831885
2892.928400	585803.350337	39.836903
2895.358395	586942.350324	39.841920
2898.486344	588087.242980	39.846938
2901.132472	589263.382723	39.851956
2904.291089	590418.423366	39.856973
2907.208527	591591.081910	39.861991
2910.542990	592766.111389	39.867008
2913.267710	593942.528101	39.872026
2916.093941	595137.346922	39.877044
2919.285767	596318.008150	39.882061
2922.317492	597519.012556	39.887079
2925.521520	598707.845211	39.892096
2928.908120	599896.676399	39.897114
2931.802918	601110.202471	39.902132
2934.613053	602299.432833	39.907149
2937.903513	603496.370517	39.912167
2941.002941	604704.577525	39.917184
2943.960072	605911.629143	39.922202
2946.673067	607120.094419	39.927220
2949.620390	608324.388867	39.932237
2952.917690	609537.503251	39.937255
2955.605784	610763.745282	39.942272
2958.694353	611977.581087	39.947290
2961.297672	613208.621544	39.952308
2964.058942	614428.846916	39.957325
2966.887516	615664.729142	39.962343
2969.701906	616909.075682	39.967360
2972.837888	618145.328914	39.972378
2976.008497	619384.686343	39.977396
2979.342838	620607.930886	39.982413
2982.472059	621856.261264	39.987431
2985.764768	623089.828628	39.992448
2989.256012	624322.023023	39.997466
2992.474922	625540.881427	40.002484
2996.384379	626753.092655	40.007501
2999.608896	627972.322613	40.012519
3002.505508	629173.187317	40.017536
3005.881865	630374.535893	40.022554
3008.562934	631567.673795	40.027572
3011.481735	632765.729905	40.032589
3014.524924	633981.051568	40.037607
3017.070401	635174.950123	40.042624
3020.047348	636357.061314	40.047642
3022.812202	637528.343477	40.052660
3025.470184	638704.500775	40.057677
3028.683590	639868.906716	40.062695
3031.542501	641031.293809	40.067712
3035.013740	642185.117460	40.072730
3038.000145	643348.367587	40.077748
3040.872817	644513.099533	40.082765
3043.999295	645673.566899	40.087783
3046.558003	646859.573058	40.092800
3049.725656	648036.863908	40.097818
3052.657336	649219.339752	40.102836
3055.446961	650413.262851	40.107853
3058.500529	651601.218567	40.112871
3061.247043	652813.948413	40.117888
3064.345616	654019.097836	40.122906
3067.191123	655239.884586	40.127924
3069.919955	656458.297841	40.132941
3072.946804	657673.821146	40.137959
3076.463658	658899.122075	40.142976
3079.944485	660142.001249	40.147994
3083.690549	661372.031874	40.153012
3086.686151	662592.572154	40.158029
3089.809661	663831.801280	40.163047
3092.648217	665064.348643	40.168064
3096.284882	666282.871604	40.173082
3099.362287	667529.045029	40.178100
3102.701207	668762.027963	40.183117
3105.956907	669996.456284	40.188135
3109.070449	671247.955446	40.193152
3112.224037	672476.058727	40.198170
3115.250284	673721.972294	40.203188
3118.532142	674975.035820	40.208205
3121.531368	676225.939899	40.213223
3124.176812	677480.064415	40.218240
3127.598470	678732.151757	40.223258
3130.911809	679993.677340	40.228276
3134.025247	681267.881154	40.233293
3137.456907	682531.672299	40.238311
3140.190678	683784.129765	40.243328
3143.337031	685053.778169	40.248346
3146.536781	686352.685329	40.253364
3149.016228	687630.971678	40.258381
3152.328410	688912.166118	40.263399
3154.920514	690219.106328	40.268416
3157.945825	691513.179770	40.273434
3161.141117	692818.946283	40.278452
3164.350904	694128.686469	40.283469
3168.101208	695439.979563	40.288487
3170.482409	696758.744247	40.293504
3173.745175	698076.571109	40.298522
3176.673622	699403.031703	40.303540
3179.933645	700728.840205	40.308557
3183.621638	702045.801813	40.313575
3186.895172	703369.273632	40.318592
3190.591805	704692.771000	40.323610
3194.251091	706003.042061	40.328628
3197.095296	707328.010488	40.333645
3200.398634	708629.271787	40.338663
3203.906425	709950.159495	40.343680
3206.861592	711268.260477	40.348698
3209.874189	712598.177651	40.353716
3212.911362	713920.853569	40.358733
3216.356943	715229.694772	40.363751
3219.527299	716555.746466	40.368768
3222.779021	717879.942702	40.373786
3225.851330	719200.051282	40.378804
3229.155272	720526.738058	40.383821
3232.409650	721829.435513	40.388839
3235.562346	723127.989639	40.393856
3238.181536	724411.646720	40.398874
3241.366271	725701.188828	40.403892
3244.029861	726988.094202	40.408909
3247.373943	728286.543791	40.413927
3249.916107	729592.626456	40.418944
3253.129518	730892.460978	40.423962
3256.382779	732214.552341	40.428980
3259.333173	733542.995782	40.433997
3263.114315	734854.740783	40.439015
3266.038728	736199.733918	40.444032
3269.425369	737536.774669	40.449050
3272.295601	738874.269021	40.454068
3275.661173	740217.180055	40.459085
3279.069063	741567.749655	40.464103
3282.848104	742923.206051	40.469120
3286.304869	744268.570551	40.474138
3289.888971	745630.546013	40.479156
3293.306027	746990.882629	40.484173
3296.495461	748338.993554	40.489191
3299.544067	749717.348919	40.494208
3302.278169	751102.655606	40.499226
3305.733254	752474.786923	40.504244
3308.665149	753873.554019	40.509261
3312.384244	755256.523022	40.514279
3315.960174	756647.783573	40.519296
3319.401350	758023.208164	40.524314
3323.289171	759424.149282	40.529332
3326.849956	760816.077443	40.534349
3330.228279	762207.238300	40.539367
3333.434593	763600.138380	40.544384
3336.445808	765012.681415	40.549402
3339.697141	766417.739320	40.554420
3343.150069	767812.273715	40.559437
3347.110828	769211.722152	40.564455
3350.278214	770623.814937	40.569472
3353.295144	772028.833253	40.574490
3356.945437	773441.338994	40.579508
3360.201194	774874.168468	40.584525
3363.625131	776285.869034	40.589543
3366.656883	777715.428728	40.594560
3370.188589	779140.796196	40.599578
3373.343396	780563.933669	40.604596
3376.596217	782009.689077	40.609613
3380.027333	783442.909760	40.614631
3383.109072	784906.605766	40.619648
3386.410846	786343.289994	40.624666
3389.792438	787799.625936	40.629684
3393.154483	789258.411937	40.634701
3396.596204	790706.838213	40.639719
3399.884262	792176.894734	40.644736
3403.884969	793611.354225	40.649754
3407.762427	795075.367941	40.654772
3411.019841	796535.407519	40.659789
3414.957865	797992.532380	40.664807
3417.854959	799458.040594	40.669824
3421.508451	800908.580218	40.674842
3424.841052	802354.122679	40.679860
3427.997473	803820.571206	40.684877
3431.451749	805288.858128	40.689895
3434.815334	806751.613481	40.694912
3437.775149	808225.609674	40.699930
3441.618769	809673.873151	40.704948
3444.742172	811152.974020	40.709965
3448.743774	812618.807009	40.714983
3452.292978	814089.866074	40.720000
3455.389824	815559.212831	40.725018
3459.193870	817000.736938	40.730023
3462.469958	818412.150759	40.735028
3465.790767	819754.959647	40.740032
3468.932061	821056.829431	40.745037
3471.634267	822293.275745	40.750042
3474.224398	823468.730267	40.755047
3477.065422	824582.431741	40.760052
3480.136433	825607.041122	40.765056
3482.962006	826589.108551	40.770061
3485.267115	827498.498580	40.775066
3487.821191	828326.221514	40.780071
3490.035151	829111.294167	40.785076
3492.090622	829835.187887	40.790080
3494.471971	830493.300405	40.795085
3496.109785	831091.444923	40.800090
3498.147222	831635.358240	40.805095
3499.557496	832133.427416	40.810100
3501.433135	832571.273320	40.815104
3503.205154	832958.376746	40.820109
3504.601047	833312.612328	40.825114
3506.466387	833599.475837	40.830119
3507.477337	833856.248794	40.835124
3508.983980	834059.376978	40.840128
3510.045458	834244.510353	40.845133
3510.982932	834377.134017	40.850138
3512.408303	834461.738674	40.855143
3513.372378	834535.484125	40.860148
3514.300209	834554.221815	40.865152
3514.926140	834573.058148	40.870157
3515.172371	834550.026234	40.875162
3516.452580	834501.342432	40.880167
3516.783606	834444.760699	40.885172
3517.694102	834342.342864	40.890176
3518.060255	834240.696775	40.895181
3518.348211	834114.653495	40.900186
3519.189461	833957.321504	40.905191
3519.005729	833795.028994	40.910196
3519.729801	833610.710654	40.915200
3519.943017	833433.501875	40.920205
3519.869845	833231.240166	40.925210
3520.421980	833014.172353	40.930215
3520.806954	832795.611228	40.935220
3521.297857	832550.950606	40.940224
3521.131615	832314.202233	40.945229
3521.427242	832051.927080	40.950234
3521.359102	831781.692510	40.955239
3521.109229	831520.951016	40.960244
3521.747638	831252.433406	40.965248
3521.873861	830966.943861	40.970253
3521.572392	830682.928866	40.975258
3521.747378	830395.647769	40.980263
3521.986646	830098.720404	40.985268
3522.115680	829793.639786	40.990272
3522.511372	829484.788035	40.995277
3522.006061	829170.696522	41.000282
3522.250975	828852.166483	41.005287
3522.054589	828543.661052	41.010292
3522.110133	828220.098915	41.015296
3522.427852	827909.670658	41.020301
3522.173126	827579.629129	41.025306
3522.351554	827258.100245	41.030311
3522.244870	826925.899869	41.035316
3522.383329	826582.401150	41.040320
3522.162745	826266.852061	41.045325
3522.061220	825934.013962	41.050330
3522.207361	825594.861249	41.055335
3521.832406	825262.034210	41.060340
3521.670921	824915.662434	41.065344
3522.073781	824587.463514	41.070349
3521.354875	824255.815627	41.075354
3521.896983	823911.376976	41.080359
3521.695724	823590.366598	41.085364
3521.479058	823236.923372	41.090368
3521.306907	822904.432457	41.095373
3521.223372	822576.311458	41.100378
3521.325553	822236.895067	41.105383
3520.878730	821905.328414	41.110388
3520.594413	821558.164553	41.115392
3520.389759	821240.023964	41.120397
3520.086695	820908.872721	41.125402
3520.250872	820593.281567	41.130407
3520.693544	820277.825052	41.135412
3520.005762	819953.196055	41.140416
3520.131729	819623.083841	41.145421
3519.983336	819297.012636	41.150426
3519.743470	818972.212731	41.155431
3519.733037	818662.185603	41.160436
3519.695389	818338.593591	41.165440
3519.753897	818026.861702	41.170445
3519.614795	817703.353474	41.175450
3519.328454	817385.041717	41.180455
3519.052671	817078.459621	41.185460
3519.152518	816755.306439	41.190464
3519.152854	816452.125167	41.195469
3519.167823	816136.885799	41.200474
3519.076901	815827.474516	41.205479
3519.035228	815522.055146	41.210484
3518.899976	815203.810383	41.215488
3518.946200	814899.278309	41.220493
3518.006162	814590.586701	41.225498
3518.338156	814288.525727	41.230503
3518.142895	813994.666764	41.235508
3518.052274	813693.285437	41.240512
3517.855849	813395.972680	41.245517
3517.860310	813100.572519	41.250522
3517.830574	812812.952118	41.255527
3517.593342	812519.084628	41.260532
3517.290686	812227.468196	41.265536
3517.441978	811929.445518	41.270541
3517.045218	811657.118728	41.275546
3517.451488	811357.657148	41.280551
3517.165424	811080.047327	41.285556
3516.490461	810776.182794	41.290560
3516.696257	810512.675498	41.295565
3516.337210	810235.728982	41.300570
3516.567663	809959.653653	41.305575
3516.039910	809696.627804	41.310580
3516.108980	809417.176212	41.315584
3516.166264	809144.820328	41.320589
3515.838492	808883.444979	41.325594
3516.023918	808607.420107	41.330599
3515.595618	808354.519002	41.335604
3515.870330	808080.859378	41.340608
3515.391882	807825.986536	41.345613
3515.104217	807571.366706	41.350618
3515.485313	807309.715743	41.355623
3515.179197	807065.765338	41.360628
3515.097270	806809.612562	41.365632
3515.017863	806557.469432	41.370637
3514.789168	806304.508286	41.375642
3514.956969	806050.295679	41.380647
3514.533166	805795.485019	41.385652
3514.628149	805554.404935	41.390656
3514.506712	805305.605487	41.395661
3514.457455	805067.473856	41.400666
3514.656877	804823.408921	41.405671
3514.194350	804586.505657	41.410676
3513.831569	804339.378184	41.415680
3514.059484	804107.591171	41.420685
3514.091551	803875.730619	41.425690
3513.792722	803640.974446	41.430695
3513.637592	803408.981954	41.435700
3513.706157	803170.421740	41.440704
3513.799469	802941.658425	41.445709
3513.525890	802710.397644	41.450714
3513.355995	802482.839728	41.455719
3513.198316	802259.932135	41.460724
3513.019477	802031.575979	41.465728
3513.080169	801813.425034	41.470733
3513.116786	801600.765424	41.475738
3513.270954	801371.449393	41.480743
3512.774052	801156.313270	41.485748
3512.534119	800933.768907	41.490752
3512.557781	800728.345540	41.495757
3512.228454	800519.589023	41.500762
3512.383113	800304.858434	41.505767
3512.299368	800100.072012	41.510772
3512.255198	799900.228850	41.515776
3512.108919	799690.386660	41.520781
3512.221632	799488.003153	41.525786
3511.958693	799285.970250	41.530791
3511.927777	799082.028324	41.535796
3511.692729	798884.052221	41.540800
3511.386010	798683.775724	41.545805
3511.430249	798497.079093	41.550810
3511.982191	798294.882702	41.555815
3511.444625	798097.670371	41.560820
3511.427881	797897.372381	41.565824
3511.521691	797706.670703	41.570829
3511.187447	797522.660968	41.575834
3511.136783	797328.095109	41.580839
3510.648252	797154.114671	41.585844
3510.834870	796960.431997	41.590848
3510.920958	796784.040208	41.595853
3510.838287	796602.419097	41.600858
3510.671388	796407.846772	41.605863
3510.548643	796233.782933	41.610868
3510.716294	796061.335998	41.615872
3510.651258	795879.742275	41.620877
3510.141125	795707.840483	41.625882
3510.210430	795522.631173	41.630887
3510.020511	795357.394374	41.635892
3509.941703	795183.297120	41.640896
3509.914683	795023.033819	41.645901
3509.887434	794855.941521	41.650906
3510.011224	794677.869955	41.655911
3509.904738	794518.639447	41.660916
3510.009047	794346.602692	41.665920
3509.937812	794185.492731	41.670925
3509.726921	794013.549003	41.675930
3509.785045	793843.324587	41.680935
3509.315781	793683.545747	41.685940
3509.522050	793519.771737	41.690944
3509.662456	793364.796175	41.695949
3509.758653	793206.681149	41.700954
3509.622723	793041.184401	41.705959
3509.272066	792887.605604	41.710964
3509.162113	792727.107123	41.715968
3509.186006	792577.438242	41.720973
3509.311905	792426.177473	41.725978
3509.279384	792257.943601	41.730983
3509.073439	792108.843082	41.735988
3509.084178	791954.643867	41.740992
3508.944866	791789.707751	41.745997
3508.625748	791651.620211	41.751002
3508.562878	791501.648072	41.756007
3508.342652	791355.923742	41.761012
3508.828082	791224.474534	41.766016
3508.917861	791078.693259	41.771021
3508.205800	790930.977983	41.776026
3508.427874	790776.521589	41.781031
3508.374820	790642.988750	41.786036
3508.244445	790511.480649	41.791040
3508.203827	790377.695078	41.796045
3508.186144	790237.859512	41.801050
3508.423252	790099.109221	41.806055
3508.039109	789954.857193	41.811060
3508.022321	789824.103750	41.816064
3508.312510	789689.071181	41.821069
3507.714221	789554.231998	41.826074
3508.000069	789414.035171	41.831079
3507.668421	789291.677953	41.836084
3507.873874	789166.969291	41.841088
3508.161260	789035.856192	41.846093
3507.554760	788911.178919	41.851098
3507.765266	788771.964756	41.856103
3507.797475	788656.662592	41.861108
3507.469008	788518.073127	41.866112
3507.339873	788395.126364	41.871117
3507.436674	788281.429334	41.876122
3507.414516	788150.006995	41.881127
3507.548919	788035.759173	41.886132
3507.343893	787902.887961	41.891136
3507.198268	787789.272275	41.896141
3507.353274	787672.508437	41.901146
3507.435084	787539.779660	41.906151
3507.011256	787435.445295	41.911156
3506.993317	787307.742483	41.916160
3507.021728	787196.890470	41.921165
3506.615013	787084.240654	41.926170
3506.997616	786963.445835	41.931175
3506.716986	786851.852991	41.936180
3506.708933	786738.197807	41.941184
3506.822885	786638.629725	41.946189
3506.382211	786528.188954	41.951194
3506.737385	786419.925575	41.956199
3506.232502	786314.801603	41.961204
3506.396857	786207.353138	41.966208
3506.499919	786101.781424	41.971213
3505.904523	785998.781813	41.976218
3506.336253	785886.712008	41.981223
3506.246928	785794.442262	41.986228
3505.905708	785697.689590	41.991232
3505.900046	785597.045082	41.996237
3505.940688	785500.275804	42.001242
3506.013589	785403.549056	42.006247
3505.951492	785313.727056	42.011252
3506.341536	785219.158042	42.016256
3506.571231	785122.942467	42.021261
3505.970418	785027.502068	42.026266
3506.569209	784911.799869	42.031271
3506.059774	784821.406373	42.036276
3505.859456	784712.717224	42.041280
3506.101705	784610.198448	42.046285
3505.759755	784525.969521	42.051290
3506.391192	784417.876082	42.056295
3505.871207	784323.248924	42.061300
3505.618310	784222.478425	42.066304
3505.757021	784131.378991	42.071309
3505.253825	784044.908880	42.076314
3505.730078	783948.538445	42.081319
3505.573448	783867.910406	42.086324
3505.297970	783780.809327	42.091328
3505.523023	783694.558913	42.096333
3505.589574	783602.235172	42.101338
3505.638029	783513.847792	42.106343
3505.692888	783428.802680	42.111348
3505.365877	783338.901351	42.116352
3505.563485	783259.339155	42.121357
3505.251452	783171.203865	42.126362
3505.192698	783073.385395	42.131367
3505.111279	782989.685601	42.136372
3504.929962	782907.329366	42.141376
3505.059311	782827.478556	42.146381
3504.872002	782756.483689	42.151386
3504.839678	782676.018482	42.156391
3505.173545	782601.984707	42.161396
3504.941886	782526.764717	42.166400
3504.748987	782448.586182	42.171405
3504.903751	782371.972610	42.176410
3504.869095	782285.256321	42.181415
3504.798168	782213.056294	42.186420
3504.668635	782138.012129	42.191424
3504.881444	782056.614051	42.196429
3504.820679	781987.607559	42.201434
3504.910514	781898.160460	42.206439
3504.469461	781837.233822	42.211444
3504.879787	781756.931171	42.216448
3504.602229	781690.269773	42.221453
3504.269768	781623.961194	42.226458
3504.544462	781547.614215	42.231463
3504.328581	781486.647404	42.236468
3504.484790	781413.713097	42.241472
3504.554816	781329.821405	42.246477
3504.382668	781277.602636	42.251482
3504.596530	781204.066320	42.256487
3504.324085	781135.529436	42.261492
3504.297760	781074.675415	42.266496
3504.553075	781009.100434	42.271501
3504.349672	780939.664699	42.276506
3504.558845	780868.339720	42.281511
3504.232629	780805.614188	42.286516
3504.153462	780738.074803	42.291520
3504.496114	780668.989042	42.296525
3504.365960	780607.607030	42.301530
3504.469201	780528.177904	42.306535
3504.354306	780464.873269	42.311540
3504.207906	780402.016115	42.316544
3504.221336	780329.192868	42.321549
3503.837271	780280.741390	42.326554
3504.114942	780204.773373	42.331559
3504.098691	780159.310981	42.336564
3504.167579	780096.710827	42.341568
3504.203867	780028.063218	42.346573
3503.930939	779967.437454	42.351578
3504.098527	779913.135234	42.356583
3503.837676	779855.409718	42.361588
3503.668332	779792.747890	42.366592
3503.927398	779727.357508	42.371597
3504.028199	779676.410679	42.376602
3503.705177	779614.067949	42.381607
3503.704620	779557.871720	42.386612
3503.617372	779497.358963	42.391616
3503.984531	779452.124031	42.396621
3503.812113	779399.990167	42.401626
3503.704233	779339.430291	42.406631
3503.479088	779286.959855	42.411636
3503.325769	779231.327657	42.416640
3503.462902	779176.532843	42.421645
3503.681067	779136.586195	42.426650
3503.829660	779085.627319	42.431655
3503.925974	779024.194463	42.436660
3503.597549	778973.953391	42.441664
3503.705300	778908.236142	42.446669
3503.396143	778852.282296	42.451674
3503.711598	778796.027947	42.456679
3503.638696	778761.393239	42.461684
3503.315792	778706.375611	42.466688
3503.320451	778649.777770	42.471693
3503.206600	778616.527159	42.476698
3503.384214	778562.360821	42.481703
3503.629220	778520.880668	42.486708
3503.392318	778465.354842	42.491712
3503.523513	778415.969066	42.496717
3503.228728	778379.006799	42.501722
3503.233716	778313.104281	42.506727
3503.596756	778270.520413	42.511732
3503.492649	778220.876889	42.516736
3503.177746	778165.804625	42.521741
3503.222895	778123.518520	42.526746
3503.296396	778064.689908	42.531751
3503.355160	778022.647062	42.536756
3503.214395	777978.323623	42.541760
3503.740731	777928.672364	42.546765
3503.235444	777885.835976	42.551770
3503.703488	777835.799955	42.556775
3503.301215	777793.093659	42.561780
3502.977575	777743.433932	42.566784
3503.244495	777697.121783	42.571789
3503.254663	777660.548462	42.576794
3503.153146	777607.307132	42.581799
3503.539343	777558.660953	42.586804
3503.362935	777510.944207	42.591808
3503.316555	777453.410257	42.596813
3503.074534	777419.338556	42.601818
3503.324303	777371.944261	42.606823
3503.382297	777326.501085	42.611828
3503.157513	777275.443555	42.616832
3503.094133	777227.361701	42.621837
3503.183373	777194.907848	42.626842
3502.998199	777138.624970	42.631847
3502.895206	777107.186999	42.636852
3502.942483	777061.350137	42.641856
3503.037805	777016.095761	42.646861
3502.730903	776998.474317	42.651866
3502.951746	776949.900629	42.656871
3503.059440	776908.729346	42.661876
3502.809773	776870.915100	42.666880
3503.000395	776827.366753	42.671885
3502.744783	776798.561722	42.676890
3503.155818	776748.478438	42.681895
3503.110034	776719.392280	42.686900
3503.064547	776657.569053	42.691904
3503.148571	776619.649133	42.696909
3502.744818	776587.667876	42.701914
3503.076657	776548.328222	42.706919
3503.133493	776502.683188	42.711924
3502.868586	776455.023380	42.716928
3503.368261	776416.738342	42.721933
3502.615180	776377.577050	42.726938
3502.740060	776332.215088	42.731943
3502.703111	776301.156573	42.736948
3502.639007	776262.323888	42.741952
3502.814481	776225.420665	42.746957
3502.581759	776192.917097	42.751962
3502.894638	776162.735588	42.756967
3502.515989	776125.332644	42.761972
3502.741867	776090.980483	42.766976
3502.805499	776054.931831	42.771981
3502.491311	776014.760642	42.776986
3502.688576	775973.864684	42.781991
3502.852395	775934.401793	42.786996
3502.575910	775904.612011	42.792001
3502.887057	775864.336659	42.797005
3502.444414	775844.322391	42.802010
3502.639527	775803.425835	42.807015
3502.696097	775767.967747	42.812020
3502.633703	775742.523797	42.817025
3502.839629	775695.027395	42.822029
3502.645643	775668.078646	42.827034
3502.730210	775627.051667	42.832039
3502.731766	775597.657806	42.837044
3502.429400	775554.577225	42.842049
3502.785796	775524.336657	42.847053
3502.800243	775493.020034	42.852058
3502.576164	775448.399563	42.857063
3502.648298	775415.448264	42.862068
3502.601945	775389.508066	42.867073
3502.745173	775353.196617	42.872077
3502.485465	775342.013453	42.877082
3502.586443	775294.384082	42.882087
3502.394268	775271.864965	42.887092
3502.183276	775230.244510	42.892097
3502.429185	775205.978700	42.897101
3502.121399	775190.027130	42.902106
3502.482899	775144.224791	42.907111
3502.432465	775116.314749	42.912116
3502.098362	775088.057564	42.917121
3502.511233	775062.581951	42.922125
3502.422350	775025.420926	42.927130
3502.436904	774999.813958	42.932135
3502.330644	774971.370952	42.937140
3502.186716	774937.714609	42.942145
3502.768360	774907.631237	42.947149
3502.405300	774875.635750	42.952154
3502.680373	774842.402135	42.957159
3502.471717	774825.940980	42.962164
3502.518684	774791.661530	42.967169
3502.324788	774754.467241	42.972173
3502.285727	774724.978105	42.977178
3502.257085	774693.074282	42.982183
3502.041755	774667.159448	42.987188
3502.245088	774642.504875	42.992193
3502.558840	774605.127455	42.997197
3502.390048	774589.250089	43.002202
3502.063538	774562.860832	43.007207
3502.144265	774529.608673	43.012212
3502.536893	774506.104190	43.017217
3502.283970	774477.141827	43.022221
3502.191817	774455.046857	43.027226
3502.449544	774423.636217	43.032231
3502.318995	774407.210456	43.037236
3502.128337	774373.263779	43.042241
3502.112043	774340.913187	43.047245
3502.114159	774326.976774	43.052250
3502.027967	774292.913974	43.057255
3502.106311	774273.055525	43.062260
3502.033979	774249.627056	43.067265
3502.098358	774218.641447	43.072269
3501.802978	774206.723764	43.077274
3502.221224	774172.774028	43.082279
3502.015962	774153.454574	43.087284
3502.287670	774131.840201	43.092289
3502.002495	774092.392340	43.097293
3502.129148	774083.802675	43.102298
3502.079853	774044.709546	43.107303
3502.018223	774023.002198	43.112308
3501.649273	774009.717456	43.117313
3501.914513	773983.228324	43.122317
3501.700761	773970.902796	43.127322
3502.134152	773939.116329	43.132327
3502.047858	773938.145691	43.137332
3501.829646	773899.966147	43.142337
3501.537549	773873.617966	43.147341
3501.906386	773870.503724	43.152346
3501.793388	773843.140893	43.157351
3502.019234	773833.943576	43.162356
3502.189264	773810.178168	43.167361
3501.981292	773783.224789	43.172365
3501.703190	773770.564822	43.177370
3501.723734	773744.361505	43.182375
3501.869509	773746.258132	43.187380
3501.930364	773716.699183	43.192385
3502.073972	773697.419373	43.197389
3501.908016	773685.725696	43.202394
3502.088023	773654.669351	43.207399
3501.564468	773648.008827	43.212404
3501.651556	773608.053606	43.217409
3501.460699	773597.890624	43.222413
3501.464288	773589.222220	43.227418
3501.829348	773573.894673	43.232423
3501.660952	773546.983136	43.237428
3501.760373	773536.279605	43.242433
3501.983172	773520.285963	43.247437
3501.803296	773499.680099	43.252442
3501.551287	773496.077298	43.257447
3501.736417	773474.869301	43.262452
3501.546045	773447.665531	43.267457
3501.813411	773427.084058	43.272461
3501.708745	773433.405424	43.277466
3501.843283	773396.888728	43.282471
3501.801842	773390.246800	43.287476
3501.900012	773370.678139	43.292481
3501.963563	773344.860296	43.297485
3501.862357	773340.395234	43.302490
3501.680235	773312.106080	43.307495
3502.055337	773289.388625	43.312500
3501.764620	773270.080964	43.317505
3501.991312	773244.925330	43.322509
3501.844087	773237.463469	43.327514
3502.190440	773210.367134	43.332519
3501.998537	773183.852164	43.337524
3501.993916	773172.623527	43.342529
3502.016676	773142.083523	43.347533
3501.659118	773137.956212	43.352538
3501.793828	773108.678127	43.357543
3501.634791	773083.240915	43.362548
3501.441898	773087.902569	43.367553
3501.790785	773059.573947	43.372557
3501.718499	773040.968378	43.377562
3501.574427	773028.728256	43.382567
3501.590391	773013.703498	43.387572
3501.640797	772986.605992	43.392577
3501.688584	772976.845992	43.397581
3501.590018	772983.708521	43.402586
3501.397816	772947.539108	43.407591
3501.553022	772934.165796	43.412596
3501.688659	772926.312101	43.417601
3501.986394	772925.918164	43.422605
3501.721839	772893.060431	43.427610
3501.784690	772884.282895	43.432615
3502.012813	772859.568994	43.437620
3501.438441	772847.399676	43.442625
3501.639215	772829.881296	43.447629
3501.810587	772814.190145	43.452634
3501.850840	772785.517436	43.457639
3501.481359	772781.194874	43.462644
3501.327534	772774.275433	43.467649
3501.792899	772741.000874	43.472653
3501.492982	772726.175493	43.477658
3501.624411	772727.631462	43.482663
3502.146670	772703.705767	43.487668
3501.724263	772688.260234	43.492673
3502.087685	772666.281618	43.497677
3501.768033	772643.529215	43.502682
3501.985346	772633.888513	43.507687
3501.861799	772600.661383	43.512692
3501.716383	772588.174469	43.517697
3501.944821	772570.158342	43.522701
3501.737786	772555.809828	43.527706
3501.799738	772541.219812	43.532711
3501.962687	772508.289715	43.537716
3501.763101	772493.742823	43.542721
3501.981173	772485.234701	43.547725
3501.709778	772456.218157	43.552730
3501.880547	772429.049453	43.557735
3501.953980	772427.067079	43.562740
3501.604631	772395.501815	43.567745
3502.125624	772377.732417	43.572749
3502.049669	772373.164079	43.577754
3501.812102	772344.092245	43.582759
3502.086352	772329.713016	43.587764
3502.012573	772308.150384	43.592769
3502.113957	772277.840092	43.597773
3501.809291	772259.123173	43.602778
3501.861508	772236.455833	43.607783
3502.025568	772226.626367	43.612788
3501.735947	772196.528128	43.617793
3502.146571	772175.426905	43.622797
3501.785554	772163.171932	43.627802
3501.820924	772148.092943	43.632807
3501.830066	772132.968998	43.637812
3501.495894	772106.128839	43.642817
3501.751540	772095.151105	43.647821
3501.518001	772089.327892	43.652826
3501.277039	772073.555526	43.657831
3501.363681	772042.754110	43.662836
3501.246246	772047.551727	43.667841
3501.645703	772029.998616	43.672845
3501.803986	772031.203989	43.677850
3501.745010	772006.780972	43.682855
3501.666671	771994.084926	43.687860
3501.465200	771991.852305	43.692865
3501.502249	771965.098067	43.697869
3501.556084	771958.242061	43.702874
3501.797679	771943.768957	43.707879
3501.641432	771932.366444	43.712884
3501.174079	771913.281446	43.717889
3501.512807	771889.580487	43.722893
3501.492968	771880.864682	43.727898
3501.407705	771892.356523	43.732903
3501.445958	771863.779079	43.737908
3501.630478	771839.906400	43.742913
3501.639768	771836.949250	43.747917
3501.805018	771828.252059	43.752922
3501.403986	771811.077014	43.757927
3501.701676	771792.160845	43.762932
3501.810390	771792.487748	43.767937
3501.940051	771771.185494	43.772941
3501.743739	771749.395169	43.777946
3501.551869	771740.116488	43.782951
3501.917122	771713.405626	43.787956
3501.468872	771696.681472	43.792961
3501.929095	771691.088132	43.797965
3501.706448	771671.370926	43.802970
3501.602681	771650.895091	43.807975
3501.479456	771637.072818	43.812980
3501.425048	771639.643484	43.817985
3501.851367	771599.325735	43.822989
3501.653943	771594.875510	43.827994
3501.532364	771585.732807	43.832999
3501.730302	771558.162306	43.838004
3501.686911	771554.474808	43.843009
3501.792571	771537.905073	43.848013
3501.567153	771521.734852	43.853018
3501.590593	771489.512944	43.858023
3502.144713	771483.509827	43.863028
3501.645767	771469.897118	43.868033
3501.460111	771452.833435	43.873037
3501.589281	771453.797398	43.878042
3501.707920	771432.890098	43.883047
3501.677259	771404.371527	43.888052
3501.398169	771397.126641	43.893057
3501.589004	771390.099677	43.898061
3501.444539	771382.044308	43.903066
3501.257470	771358.970439	43.908071
3501.583806	771355.024687	43.913076
3500.952760	771355.030478	43.918081
3501.408159	771351.851623	43.923085
3501.336319	771356.050984	43.928090
3501.254569	771320.150910	43.933095
3501.442651	771312.730213	43.938100
3501.404946	771304.016679	43.943105
3501.327890	771293.289793	43.948109
3501.560532	771296.946226	43.953114
3501.061522	771262.888348	43.958119
3501.544616	771252.315161	43.963124
3501.444114	771249.720773	43.968129
3501.650948	771241.607199	43.973133
3501.301731	771224.520750	43.978138
3501.376240	771206.231145	43.983143
3501.138257	771198.338824	43.988148
3500.983660	771202.699742	43.993153
3501.031841	771196.582941	43.998157
3501.264120	771201.766702	44.003162
3501.252372	771200.684850	44.008167
3501.452596	771188.236975	44.013172
3501.351537	771164.310775	44.018177
3501.518663	771154.725706	44.023181
3501.420184	771149.716940	44.028186
3501.312186	771143.478107	44.033191
3501.494250	771134.087604	44.038196
3501.163163	771118.229553	44.043201
3501.666897	771101.494527	44.048205
3501.552819	771088.162372	44.053210
3501.273047	771088.799834	44.058215
3501.554401	771064.957916	44.063220
3501.027810	771059.970569	44.068225
3501.271507	771056.333913	44.073229
3501.282914	771038.103585	44.078234
3500.964929	771044.462245	44.083239
3500.967906	771038.352782	44.088244
3500.985464	771039.827907	44.093249
3501.084627	771033.751812	44.098253
3501.071231	771030.601023	44.103258
3501.268875	771019.779079	44.108263
3501.523697	770994.069196	44.113268
3501.341417	770991.783830	44.118273
3501.485895	770978.359484	44.123277
3501.310180	770980.802624	44.128282
3501.371504	770967.490532	44.133287
3501.333725	770937.690401	44.138292
3501.467546	770938.456597	44.143297
3501.264625	770938.096033	44.148301
3501.248492	770940.069414	44.153306
3501.023365	770931.287878	44.158311
3501.343418	770924.140586	44.163316
3501.304532	770901.237866	44.168321
3501.396158	770893.537086	44.173325
3501.252524	770889.767285	44.178330
3501.289665	770885.376403	44.183335
3501.354868	770884.774461	44.188340
3501.109624	770876.143985	44.193345
3501.363537	770835.505692	44.198349
3501.223053	770841.638123	44.203354
3501.093482	770841.019095	44.208359
3501.473377	770827.013630	44.213364
3501.079888	770843.090656	44.218369
3501.377075	770830.478355	44.223373
3501.539676	770815.030746	44.228378
3501.550627	770793.252613	44.233383
3501.665359	770779.241608	44.238388
3501.253211	770790.000892	44.243393
3501.205963	770771.286920	44.248397
3501.216155	770755.223887	44.253402
3501.373885	770750.418853	44.258407
3501.620920	770746.288812	44.263412
3501.209418	770750.199768	44.268417
3501.537604	770728.122680	44.273421
3501.216921	770715.415213	44.278426
3501.181268	770691.525941	44.283431
3501.282882	770690.868697	44.288436
3501.040881	770692.978005	44.293441
3501.271809	770674.119282	44.298445
3501.366648	770681.444675	44.303450
3501.074488	770677.699309	44.308455
3501.202789	770657.477981	44.313460
3500.876415	770660.241734	44.318465
3501.025994	770640.066111	44.323469
3501.274854	770641.650899	44.328474
3501.497076	770647.723553	44.333479
3501.397678	770625.519742	44.338484
3501.356193	770635.577501	44.343489
3501.428670	770607.974922	44.348493
3501.408445	770594.626367	44.353498
3501.298101	770592.920218	44.358503
3501.558728	770593.961111	44.363508
3501.446049	770592.206079	44.368513
3501.466861	770562.985986	44.373517
3501.409759	770561.812996	44.378522
3501.193466	770557.907224	44.383527
3501.321893	770552.170785	44.388532
3501.104877	770562.405458	44.393537
3501.256833	770547.106857	44.398541
3501.594787	770523.598731	44.403546
3501.376385	770521.910422	44.408551
3501.375994	770504.271964	44.413556
3501.079503	770510.676797	44.418561
3501.439834	770509.681167	44.423565
3501.432930	770483.322984	44.428570
3501.406623	770465.491636	44.433575
3501.191303	770458.481637	44.438580
3501.248554	770457.536084	44.443585
3501.046480	770455.894332	44.448589
3501.452206	770466.666741	44.453594
3500.987740	770436.688750	44.458599
3501.275439	770411.710466	44.463604
3500.872004	770414.487044	44.468609
3501.030170	770406.084976	44.473613
3501.004693	770406.237036	44.478618
3501.156469	770406.211995	44.483623
3501.349584	770404.209304	44.488628
3500.902000	770402.460299	44.493633
3501.067857	770401.644602	44.498637
3501.429035	770417.302220	44.503642
3501.098504	770391.144999	44.508647
3501.175174	770362.407589	44.513652
3501.148110	770368.226044	44.518657
3501.158296	770355.758904	44.523661
3501.311390	770359.281140	44.528666
3501.096017	770358.873332	44.533671
3501.254520	770356.482182	44.538676
3501.316033	770353.318726	44.543681
3501.205032	770331.411574	44.548685
3500.768497	770321.728098	44.553690
3501.006162	770312.228825	44.558695
3501.306676	770310.553259	44.563700
3500.930016	770311.896589	44.568705
3501.343618	770307.147528	44.573709
3501.195425	770307.024242	44.578714
3501.254750	770315.981812	44.583719
3501.300498	770309.963222	44.588724
3500.907839	770291.847098	44.593729
3501.187966	770263.666938	44.598733
3501.218315	770261.740377	44.603738
3501.094134	770272.846993	44.608743
3501.163751	770260.665501	44.613748
3500.969952	770268.334629	44.618753
3501.098658	770262.499377	44.623757
3501.252012	770272.476161	44.628762
3500.744187	770269.061853	44.633767
3501.015330	770264.927562	44.638772
3500.837594	770260.325461	44.643777
3501.130738	770262.642085	44.648781
3501.308890	770267.983265	44.653786
3501.378203	770236.043941	44.658791
3501.381473	770222.641561	44.663796
3500.778520	770220.524012	44.668801
3501.088236	770214.363180	44.673805
3501.012868	770215.755282	44.678810
3500.496986	770218.353427	44.683815
3500.994025	770215.019398	44.688820
3500.600366	770219.617485	44.693825
3500.824183	770206.966977	44.698829
3500.889876	770214.100563	44.703834
3500.959158	770211.231393	44.708839
3500.998473	770218.221519	44.713844
3500.793744	770213.426762	44.718849
3500.990657	770209.255435	44.723853
3501.150606	770212.825880	44.728858
3500.751265	770217.227820	44.733863
3501.138662	770200.657805	44.738868
3501.197855	770205.575242	44.743873
3500.950143	770209.163782	44.748877
3500.952049	770208.917147	44.753882
3501.235130	770215.719178	44.758887
3501.094003	770191.845722	44.763892
3501.087502	770185.096587	44.768897
3501.260589	770171.370420	44.773901
3501.139078	770173.213602	44.778906
3500.956580	770165.064644	44.783911
3501.002707	770163.036906	44.788916
3501.258617	770164.374274	44.793921
3500.971369	770153.187745	44.798925
3501.204541	770169.409035	44.803930
3501.032128	770161.307679	44.808935
3500.769453	770140.607555	44.813940
3500.517235	770154.938198	44.818945
3501.104543	770151.145776	44.823949
3501.045410	770162.833074	44.828954
3500.917858	770142.849708	44.833959
3501.148562	770125.960515	44.838964
3500.903540	770127.429940	44.843969
3500.920624	770112.990360	44.848973
3501.158662	770117.927573	44.853978
3500.935535	770100.571321	44.858983
3501.442572	770106.548085	44.863988
3501.040988	770104.889950	44.868993
3501.010716	770108.393334	44.873997
3501.063549	770106.315200	44.879002
3500.949073	770102.392360	44.884007
3501.311562	770111.497170	44.889012
3501.176462	770112.406438	44.894017
3501.250240	770092.291121	44.899021
3501.294844	770071.047300	44.904026
3500.824613	770065.458685	44.909031
3501.283941	770064.151003	44.914036
3500.927748	770068.398082	44.919041
3501.074723	770068.472379	44.924045
3501.055089	770071.185660	44.929050
3500.881139	770071.608625	44.934055
3501.474970	770056.630174	44.939060
3500.846712	770063.829307	44.944065
3501.056469	770045.415938	44.949069
3501.024036	770030.343832	44.954074
3500.952663	770040.358065	44.959079
3501.186423	770028.296885	44.964084
3501.031867	770033.249758	44.969089
3501.036092	770031.770911	44.974093
3501.140221	770029.585733	44.979098
3500.977993	770034.096417	44.984103
3500.920934	770017.205256	44.989108
3500.963006	770030.452775	44.994113
3501.098436	770027.474057	44.999117
3501.327029	770029.111602	45.004122
3501.418581	770023.479394	45.009127
3501.388090	770003.183974	45.014132
3501.392209	769996.974917	45.019137
3501.059729	769984.859417	45.024141
3501.342452	769981.117242	45.029146
3501.097077	769982.143295	45.034151
3501.112446	769982.042247	45.039156
3500.830313	769985.932222	45.044161
3501.002419	769988.367482	45.049165
3500.936225	769984.338054	45.054170
3501.093385	769961.153661	45.059175
3501.596328	769936.483122	45.064180
3501.077826	769937.505041	45.069185
3501.386495	769925.431315	45.074189
3501.233766	769930.876690	45.079194
3501.172879	769935.764876	45.084199
3501.323249	769930.369245	45.089204
3501.141416	769911.428970	45.094209
3500.943274	769902.198285	45.099213
3501.288665	769896.770403	45.104218
3501.279910	769895.392222	45.109223
3501.641948	769886.266043	45.114228
3500.970536	769890.368216	45.119233
3501.177845	769881.858887	45.124237
3501.578600	769867.552523	45.129242
3501.017939	769853.207909	45.134247
3501.196134	769847.068508	45.139252
3501.307066	769851.534163	45.144257
3501.159908	769846.581831	45.149261
3501.130678	769841.659282	45.154266
3500.849790	769848.554847	45.159271
3501.086750	769842.405732	45.164276
3500.731696	769844.928153	45.169281
3501.111716	769842.795878	45.174285
3501.107230	769828.753502	45.179290
3500.960047	769813.404271	45.184295
3501.302749	769810.095569	45.189300
3501.091191	769819.886894	45.194305
3501.158520	769811.499164	45.199309
3501.063923	769809.740957	45.204314
3500.950284	769817.594401	45.209319
3501.302076	769806.055373	45.214324
3501.141051	769815.591981	45.219329
3501.220999	769799.170426	45.224333
3501.372136	769777.612512	45.229338
3500.934612	769772.363190	45.234343
3501.161621	769760.746163	45.239348
3500.918079	769772.366001	45.244353
3501.300188	769767.720352	45.249357
3500.820373	769767.848955	45.254362
3500.754555	769761.946906	45.259367
3500.943729	769760.043244	45.264372
3501.359301	769766.331048	45.269377
3501.166217	769761.829721	45.274381
3501.171696	769757.147754	45.279386
3500.990058	769737.911354	45.284391
3501.296200	769731.947815	45.289396
3501.251832	769717.024869	45.294401
3501.021706	769720.709287	45.299405
3501.221446	769721.711094	45.304410
3501.218968	769724.520216	45.309415
3501.230843	769725.799442	45.314420
3500.942442	769726.142789	45.319425
3501.209966	769729.449317	45.324429
3501.389561	769707.492297	45.329434
3501.352868	769687.788339	45.334439
3501.463690	769685.897606	45.339444
3501.146883	769680.036967	45.344449
3501.098373	769675.955174	45.349453
3501.351919	769676.307517	45.354458
3501.212965	769666.426178	45.359463
3501.327714	769646.844911	45.364468
3501.062154	769642.256936	45.369473
3500.927116	769644.053209	45.374477
3501.357159	769637.872018	45.379482
3500.877140	769633.418028	45.384487
3501.218701	769634.445687	45.389492
3501.064854	769641.911756	45.394497
3501.228755	769638.189046	45.399501
3501.292934	769615.659520	45.404506
3500.794114	769595.341822	45.409511
3501.133387	769590.703143	45.414516
3501.064651	769598.352295	45.419521
3500.891848	769590.841687	45.424525
3500.816993	769590.804820	45.429530
3501.091975	769585.092692	45.434535
3501.046428	769578.152352	45.439540
3500.769035	769587.905585	45.444545
3501.176461	769580.446912	45.449549
3501.114731	769588.242744	45.454554
3500.867589	769585.425622	45.459559
3500.855507	769584.195760	45.464564
3500.650197	769588.763108	45.469569
3500.747261	769582.932552	45.474573
3500.915477	769577.238061	45.479578
3501.016439	769584.415702	45.484583
3501.073062	769586.377420	45.489588
3501.150708	769587.793628	45.494593
3500.869458	769578.280616	45.499597
3501.201062	769570.588083	45.504602
3500.862783	769571.826646	45.509607
3501.054215	769552.478838	45.514612
3501.036271	769537.304783	45.519617
3501.037916	769537.452379	45.524621
3501.026882	769531.048330	45.529626
3501.014487	769536.815738	45.534631
3501.338127	769529.124477	45.539636
3500.928157	769539.195340	45.544641
3501.232942	769540.179814	45.549645
3501.471554	769535.114248	45.554650
3501.336181	769532.525017	45.559655
3501.299568	769498.678246	45.564660
3500.642718	769507.459483	45.569665
3501.329895	769498.771865	45.574669
3501.125935	769499.988244	45.579674
3500.923194	769493.812948	45.584679
3501.027678	769493.697168	45.589684
3500.977120	769485.870593	45.594689
3500.867275	769492.541117	45.599693
3501.434975	769488.455945	45.604698
3500.959332	769498.242056	45.609703
3501.370960	769476.590945	45.614708
3501.024905	769463.195640	45.619713
3500.977576	769448.519026	45.624717
3501.240412	769446.208898	45.629722
3501.134187	769445.438061	45.634727
3501.212880	769448.529536	45.639732
3500.978555	769445.858072	45.644737
3500.695176	769449.354316	45.649741
3501.150288	769458.346075	45.654746
3500.977259	769448.568628	45.659751
3501.311173	769448.464212	45.664756
3501.287957	769454.972623	45.669761
3501.259999	769438.666655	45.674765
3501.132541	769419.519028	45.679770
3500.981455	769416.932352	45.684775
3501.331513	769405.737930	45.689780
3501.005004	769405.446985	45.694785
3501.175025	769409.410372	45.699789
3501.287271	769397.861019	45.704794
3501.050914	769408.051201	45.709799
3501.214671	769396.394780	45.714804
3500.665654	769369.629446	45.719809
3500.703407	769383.223778	45.724813
3501.317870	769383.615050	45.729818
3501.101037	769382.813207	45.734823
3501.180378	769347.418990	45.739828
3501.108730	769298.498170	45.744833
3500.762588	769176.641120	45.749837
3500.923099	769002.609810	45.754842
3500.907445	768780.800884	45.759847
3500.730088	768501.696039	45.764852
3500.405587	768162.477154	45.769857
3500.315255	767759.672126	45.774861
3500.189638	767313.475213	45.779866
3500.078152	766792.716482	45.784871
3499.751989	766225.468866	45.789876
3499.503593	765602.355374	45.794881
3499.035670	764919.565318	45.799885
3498.719336	764174.062438	45.804890
3497.905391	763376.735859	45.809895
3498.101293	762526.235011	45.814900
3497.264547	761618.686737	45.819905
3496.866661	760637.744321	45.824909
3496.579491	759609.387415	45.829914
3495.809867	758518.002254	45.834919
3495.304982	757372.470722	45.839924
3494.931062	756167.755880	45.844929
3494.264851	754891.359734	45.849933
3493.735692	753547.867287	45.854938
3492.897927	752168.186259	45.859943
3492.251962	750707.262500	45.864948
3491.563101	749210.594982	45.869953
3490.676703	747639.248061	45.874957
3490.109789	745996.008569	45.879962
3489.497341	744307.985732	45.884967
3488.532291	742540.587630	45.889972
3487.620962	740726.389706	45.894977
3486.713041	738850.330021	45.899981
3485.423466	736904.710701	45.904986
3484.472526	734927.625959	45.909991
3483.572448	732874.493792	45.914996
3482.381087	730770.423627	45.920001
3481.541601	728594.268873	45.925005
3480.630912	726376.716322	45.930010
3478.993970	724100.248860	45.935015
3478.050480	721763.941984	45.940020
3476.864978	719364.680140	45.945025
3475.577929	716911.666275	45.950029
3474.358488	714397.684225	45.955034
3473.263349	711847.344121	45.960039
3471.869567	709226.329368	45.965044
3470.610848	706565.699410	45.970049
3469.453508	703828.464951	45.975053
3467.943707	701049.324033	45.980058
3466.354685	698217.857172	45.985063
3464.900936	695320.060415	45.990068
3463.551391	692373.988955	45.995073
3461.970906	689382.195859	46.000077
3460.232221	686333.579980	46.005082
3458.737971	683242.616377	46.010087
3457.136010	680079.290686	46.015092
3455.327337	676881.824868	46.020097
3453.629271	673628.356597	46.025101
3452.546941	670324.987370	46.030106
3450.476897	666966.552871	46.035111
3449.340257	663545.552111	46.040116
3447.471462	660093.954476	46.045121
3445.570299	656576.816695	46.050125
3443.734552	653011.049547	46.055130
3441.952459	649398.014679	46.060135
3440.408505	645731.594746	46.065140
3438.507014	642017.195250	46.070145
3435.949912	638259.730385	46.075149
3434.203689	634443.661202	46.080154
3432.217987	630599.402487	46.085159
3430.191410	626694.552385	46.090164
3427.964618	622741.162008	46.095169
3426.008637	618745.482731	46.100173
3424.447569	614708.267700	46.105178
3421.937059	610619.329367	46.110183
3419.569095	606464.650878	46.115188
3417.514332	602289.125739	46.120193
3415.220591	598066.029157	46.125197
3412.928832	593798.103059	46.130202
3410.570306	589495.531995	46.135207
3408.394546	585138.252738	46.140212
3406.120735	580737.539136	46.145217
3403.875759	576295.459450	46.150221
3401.874897	571828.664300	46.155226
3399.145963	567291.453690	46.160231
3396.501941	562726.648255	46.165236
3394.256914	558122.808210	46.170241
3391.770826	553475.842440	46.175245
3389.543727	548775.417435	46.180250
3386.904727	544055.604059	46.185255
3384.658382	539271.786735	46.190260
3382.066602	534466.589655	46.195265
3379.321955	529614.346817	46.200269
3376.669276	524724.140574	46.205274
3373.595210	519803.171288	46.210279
3370.877021	514837.265800	46.215284
3368.079073	509839.120703	46.220289
3365.252055	504810.094879	46.225293
3362.655263	499753.234858	46.230298
3359.935351	494661.474303	46.235303
3357.037614	489514.836668	46.240308
3354.242622	484359.982426	46.245313
3351.652016	479155.859960	46.250317
3348.816654	473916.262743	46.255322
3345.804327	468660.589671	46.260327
3342.936850	463353.085728	46.265332
3339.918240	458026.033646	46.270337
3336.960317	452664.160267	46.275341
3334.403522	447268.182121	46.280346
3330.988200	441854.148267	46.285351
3328.213516	436405.854681	46.290356
3324.826135	430911.801126	46.295361
3321.850305	425415.179269	46.300365
3318.633921	419865.845067	46.305370
3315.254337	414314.553385	46.310375
3312.311478	408717.282724	46.315380
3309.090529	403105.996520	46.320385
3305.593120	397470.465252	46.325389
3302.435348	391805.534880	46.330394
3299.029512	386132.580419	46.335399
3295.866376	380425.122859	46.340404
3292.783280	374710.143747	46.345409
3289.095560	368967.047709	46.350413
3286.068729	363200.923844	46.355418
3282.390576	357414.722563	46.360423
3279.197477	351612.747370	46.365428
3275.523988	345783.240741	46.370433
3272.022344	339932.545858	46.375437
3268.523257	334062.132175	46.380442
3264.787726	328207.589581	46.385447
3261.359574	322309.748955	46.390452
3257.708088	316396.714210	46.395457
3254.036951	310494.060145	46.400461
3250.938974	304565.178618	46.405466
3246.978708	298632.225499	46.410471
3243.526723	292677.020985	46.415476
3239.546010	286717.457965	46.420481
3235.907003	280756.474224	46.425485
3232.340161	274764.139857	46.430490
3228.345864	268783.984867	46.435495
3224.667495	262785.657583	46.440500
3220.581117	256776.613837	46.445505
3216.629679	250781.418979	46.450509
3212.916578	244772.272111	46.455514
3208.650986	238767.923205	46.460519
3205.106564	232765.642103	46.465524
3201.030771	226742.871884	46.470529
3196.846973	220721.421069	46.475533
3193.247163	214724.017162	46.480538
3189.013679	208630.660073	46.485543
3184.871906	202596.296571	46.490548
3180.763033	196597.900273	46.495553
3176.484469	190592.620352	46.500557
3172.537549	184588.204382	46.505562
3168.121503	178602.524300	46.510567
3163.962955	172617.771028	46.515572
3160.115868	166639.852428	46.520577
3155.436864	160687.730234	46.525581
3151.375715	154719.226156	46.530586
3146.658285	148773.659463	46.535591
3142.018813	142841.465961	46.540596
3137.492615	136930.184471	46.545601
3132.964321	131028.970410	46.550605
3128.783566	125145.918228	46.555610
3123.914801	119308.603746	46.560615
3119.005922	113458.783426	46.565620
3114.955399	107644.532026	46.570625
3109.836763	101851.943714	46.575629
3105.524792	96083.529058	46.580634
3100.450034	90336.057933	46.585639
3095.797940	84613.110045	46.590644
3090.646265	78930.791890	46.595649
3085.582981	73282.206681	46.600653
3080.419415	67653.720524	46.605658
3075.019350	62086.182493	46.610663
3069.536836	56539.853429	46.615668
3063.934691	51052.424126	46.620673
3056.812637	45644.070419	46.625677
3045.546812	40400.134371	46.630682
3027.712127	35447.808420	46.635687
3010.355619	30673.145533	46.640692
2994.094625	26118.865227	46.645697
2978.475050	21829.596993	46.650701
2963.487144	17812.132356	46.655706
2944.770087	14170.300368	46.660711
2919.820442	11025.770126	46.665716
2893.750188	8310.530502	46.670721
2870.089199	5979.483921	46.675725
2849.779779	4045.074593	46.680730
2831.579756	2493.858905	46.685735
2816.757410	1286.232650	46.690740
2803.638434	402.264657	46.695745
2776.666962	253.522276	46.700749
2758.249801	266.577198	46.705754
2754.901035	265.318400	46.710759
2761.086820	258.865372	46.715764
2770.574684	252.172055	46.720769
2778.558232	258.477564	46.725773
2782.879007	244.741280	46.730778
2783.810262	253.646766	46.735783
2783.164451	258.546054	46.740788
2780.829599	240.440411	46.745793
2776.819350	244.699132	46.750797
2773.173813	241.285575	46.755802
2769.831284	236.333546	46.760807
2767.182225	239.933218	46.765812
2764.750938	229.720698	46.770817
2761.917043	232.395260	46.775821
2759.682871	236.061043	46.780826
2756.475898	235.151549	46.785831
2753.515631	229.087412	46.790836
2750.659765	228.774374	46.795841
2747.053985	229.472502	46.800845
2744.215272	227.537473	46.805850
2740.957466	232.525947	46.810855
2737.702909	234.378782	46.815860
2734.573561	228.759425	46.820865
2731.033934	231.580427	46.825869
2728.206886	232.016858	46.830874
2725.010136	231.735794	46.835879
2721.564461	222.867946	46.840884
2718.324446	224.653858	46.845889
2714.867974	234.923033	46.850893
2711.727747	215.182842	46.855898
2708.388995	220.330764	46.860903
2705.527637	224.838041	46.865908
2702.311186	225.513593	46.870913
2698.086985	221.378724	46.875917
2695.001970	232.424907	46.880922
2691.437589	217.437570	46.885927
2688.544255	220.336719	46.890932
2685.392131	222.449500	46.895937
2681.715576	228.548881	46.900941
2678.473507	219.748799	46.905946
2674.383667	215.914558	46.910951
2671.642949	218.569014	46.915956
2668.149138	211.894700	46.920961
2664.655363	219.918656	46.925965
2661.125705	213.185753	46.930970
2657.394625	223.679604	46.935975
2653.813559	213.276456	46.940980
2650.535616	214.225079	46.945985
2647.240769	208.085587	46.950989
2644.879099	219.332122	46.955994
2640.956247	217.950601	46.960999
2636.985382	218.686172	46.966004
2633.398122	207.653185	46.971009
2630.262512	219.332742	46.976013
2627.584972	204.216816	46.981018
2623.495408	207.309509	46.986023
2619.847254	209.201148	46.991028
2616.798361	209.386268	46.996033
2613.074386	209.233029	47.001037
2610.030655	211.395209	47.006042
2606.285275	204.296888	47.011047
2602.664176	209.976091	47.016052
2599.730012	212.949545	47.021057
2596.120988	206.755550	47.026061
2592.088427	202.455470	47.031066
2588.500446	206.605957	47.036071
2585.286940	206.661273	47.041076
2582.354837	207.569857	47.046081
2578.356563	214.244537	47.051085
2575.525487	207.589245	47.056090
2571.690036	210.230439	47.061095
2567.756078	202.664707	47.066100
2564.657667	199.857950	47.071105
2561.247635	217.347786	47.076109
2557.833713	206.678874	47.081114
2554.506115	204.241794	47.086119
2551.242725	215.383497	47.091124
2547.322675	201.718363	47.096129
2543.885511	202.618245	47.101133
2540.452954	204.643568	47.106138
2536.799810	197.934782	47.111143
2533.084688	199.155980	47.116148
2529.955261	192.352003	47.121153
2526.658843	194.516413	47.126157
2523.288538	196.021720	47.131162
2520.175323	194.918295	47.136167
2516.376844	190.908693	47.141172
2512.609701	194.103009	47.146177
2509.018539	192.394367	47.151181
2505.482207	193.019234	47.156186
2502.106047	191.191722	47.161191
2498.608992	200.534345	47.166196
2495.312788	190.714685	47.171201
2491.794712	196.264430	47.176205
2488.448234	184.298782	47.181210
2485.110828	191.720346	47.186215
2481.484242	191.465256	47.191220
2477.865685	186.351993	47.196225
2474.215418	190.810069	47.201229
2470.683823	186.387299	47.206234
2467.471972	192.905793	47.211239
2463.838303	184.412106	47.216244
2459.922902	188.163430	47.221249
2456.552741	188.687213	47.226253
2453.719530	185.599430	47.231258
2450.093162	182.016647	47.236263
2446.971142	189.432565	47.241268
2443.606919	172.378625	47.246273
2439.571315	187.623796	47.251277
2435.831800	181.267256	47.256282
2432.134353	185.030858	47.261287
2428.922359	186.870162	47.266292
2425.644779	185.593336	47.271297
2421.794927	187.909662	47.276301
2418.578813	181.220777	47.281306
2415.218766	185.462314	47.286311
2411.314134	187.623932	47.291316
2408.003225	176.312761	47.296321
2404.029445	184.147217	47.301325
2401.211371	176.678665	47.306330
2397.674887	176.791559	47.311335
2394.321742	183.517418	47.316340
2391.109261	184.010996	47.321345
2387.049767	195.376989	47.326349
2383.506183	184.383007	47.331354
2380.015704	186.036991	47.336359
2376.494784	184.803859	47.341364
2373.581921	176.443872	47.346369
2369.663763	185.712463	47.351373
2366.342912	186.913500	47.356378
2362.500741	185.392982	47.361383
2359.073431	187.436720	47.366388
2355.568134	184.916754	47.371393
2351.999893	179.419152	47.376397
2348.980011	183.171839	47.381402
2345.380560	180.982820	47.386407
2341.675276	196.193694	47.391412
2338.581495	193.441994	47.396417
2334.631366	197.228981	47.401421
2331.480287	182.182467	47.406426
2327.927223	188.698567	47.411431
2324.045102	188.342670	47.416436
2320.708147	183.138708	47.421441
2316.888061	190.116606	47.426445
2313.873898	183.484936	47.431450
2310.457626	181.357961	47.436455
2306.410566	185.260681	47.441460
2303.357529	179.081440	47.446465
2299.937757	180.491514	47.451469
2296.402221	185.203253	47.456474
2292.837311	181.839145	47.461479
2289.274293	195.490231	47.466484
2286.119587	189.757638	47.471489
2282.300153	183.476050	47.476493
2278.782710	191.219441	47.481498
2275.621991	176.247991	47.486503
2271.930152	185.698614	47.491508
2268.531170	173.172757	47.496513
2264.576369	187.695064	47.501517
2261.273012	180.956825	47.506522
2257.776600	167.882544	47.511527
2254.015134	177.296954	47.516532
2251.205694	169.821168	47.521537
2247.556377	178.352874	47.526541
2244.010392	169.675172	47.531546
2239.827568	175.516571	47.536551
2236.486705	180.071393	47.541556
2233.364292	171.690779	47.546561
2229.723864	176.332721	47.551565
2226.636285	165.386703	47.556570
2223.168314	166.736543	47.561575
2219.550974	178.500267	47.566580
2216.089038	164.526781	47.571585
2212.215677	174.063360	47.576589
2208.699787	170.831910	47.581594
2205.399429	171.304272	47.586599
2201.745878	177.746732	47.591604
2198.490792	167.597897	47.596609
2194.776277	173.381887	47.601613
2191.542017	174.980556	47.606618
2187.825434	171.228252	47.611623
2184.353159	169.070406	47.616628
2181.160206	170.186266	47.621633
2177.303287	170.234226	47.626637
2173.482679	176.627028	47.631642
2170.303763	175.726562	47.636647
2166.842602	177.044340	47.641652
2163.517908	173.749089	47.646657
2159.896383	179.787660	47.651661
2156.799742	169.875266	47.656666
2153.051178	173.828132	47.661671
2149.128292	177.599325	47.666676
2145.897288	170.827498	47.671681
2142.404162	180.470262	47.676685
2138.883919	178.463666	47.681690
2135.556862	168.256756	47.686695
2131.608032	183.671316	47.691700
2128.189383	170.638149	47.696705
2124.994820	174.237984	47.701709
2121.397955	175.081390	47.706714
2118.241098	176.214603	47.711719
2114.260239	178.249999	47.716724
2111.132579	170.945047	47.721729
2107.448972	175.597599	47.726733
2103.878219	161.502344	47.731738
2100.249133	174.975051	47.736743
2096.623427	175.969285	47.741748
2093.502575	167.855725	47.746753
2089.831953	188.546169	47.751757
2086.685352	165.684664	47.756762
2082.817502	171.669583	47.761767
2079.278513	174.137374	47.766772
2075.695675	168.543583	47.771777
2072.198336	172.578032	47.776781
2068.708709	176.213575	47.781786
2065.366211	164.789362	47.786791
2062.085333	171.623268	47.791796
2058.510486	165.375977	47.796801
2055.067048	189.797712	47.801805
2051.791316	172.469016	47.806810
2048.059934	168.191818	47.811815
2044.253250	170.943164	47.816820
2040.891778	167.158010	47.821825
2037.211020	170.271919	47.826829
2034.028502	162.177115	47.831834
2030.614752	160.082721	47.836839
2026.663524	170.291651	47.841844
2023.109093	165.991473	47.846849
2019.564784	168.263254	47.851853
2016.132693	168.286949	47.856858
2012.892108	161.635821	47.861863
2009.584975	160.621948	47.866868
2006.471329	158.060877	47.871873
2002.364968	162.483222	47.876877
1999.004954	159.290660	47.881882
1995.660131	150.821213	47.886887
1991.912181	160.537482	47.891892
1988.662224	150.284988	47.896897
1984.489396	153.151522	47.901901
1981.291059	160.012060	47.906906
1977.648901	164.617594	47.911911
1974.199580	160.502905	47.916916
1970.919296	165.544579	47.921921
1967.345538	163.981733	47.926925
1963.988854	167.630061	47.931930
1960.787876	155.203127	47.936935
1956.602721	161.599293	47.941940
1953.447261	157.224778	47.946945
1949.931450	161.213444	47.951949
1946.493719	164.950795	47.956954
1943.343034	161.592166	47.961959
1939.527254	155.562519	47.966964
1936.070995	155.512931	47.971969
1931.751648	162.768652	47.976973
1928.304676	160.665445	47.981978
1925.264243	159.071284	47.986983
1921.685731	157.441385	47.991988
1918.881119	157.469511	47.996993
1914.988172	166.688911	48.001997
1911.282634	161.239340	48.007002
1907.606392	165.460253	48.012007
1903.964405	174.496784	48.017012
1900.722378	166.725126	48.022017
1897.453820	163.318580	48.027021
1894.567216	168.775381	48.032026
1890.972912	162.154564	48.037031
1886.899308	165.670164	48.042036
1883.435819	160.776852	48.047041
1879.612209	167.428515	48.052045
1876.183587	165.221868	48.057050
1872.920186	156.969324	48.062055
1869.234038	155.528203	48.067060
1865.548427	158.262602	48.072065
1862.064314	165.687805	48.077069
1858.894451	161.094935	48.082074
1855.660649	162.073563	48.087079
1851.620080	162.763017	48.092084
1848.749807	155.742027	48.097089
1844.934529	155.468648	48.102093
1841.364497	166.640696	48.107098
1838.009748	161.163839	48.112103
1834.084816	163.152737	48.117108
1830.918600	158.471473	48.122113
1826.976998	164.753198	48.127117
1823.534949	160.542125	48.132122
1820.401558	160.968176	48.137127
1816.390240	160.839403	48.142132
1813.460808	163.547377	48.147137
1809.589068	150.943063	48.152141
1806.106491	155.129396	48.157146
1803.023159	150.597812	48.162151
1799.340496	160.937058	48.167156
1796.115747	150.492896	48.172161
1792.335414	159.066207	48.177165
1788.690256	157.226853	48.182170
1785.771801	150.468660	48.187175
1781.608138	154.134265	48.192180
1778.146152	154.283293	48.197185
1774.682409	158.324646	48.202189
1771.369948	144.269816	48.207194
1767.978801	146.115830	48.212199
1763.669601	149.185353	48.217204
1760.671872	140.285630	48.222209
1757.014196	144.966931	48.227213
1754.053673	147.495590	48.232218
1750.462588	144.212492	48.237223
1746.433552	156.321859	48.242228
1743.581286	147.546626	48.247233
1739.946868	158.155175	48.252237
1736.226953	148.538483	48.257242
1733.003109	152.247849	48.262247
1729.128393	159.214769	48.267252
1725.946389	153.972821	48.272257
1722.152486	158.464406	48.277261
1718.689329	161.108975	48.282266
1715.350194	152.500706	48.287271
1711.637192	155.974062	48.292276
1708.081724	152.277009	48.297281
1704.490534	156.662385	48.302285
1701.378687	150.968181	48.307290
1697.838505	143.829462	48.312295
1694.214254	151.581128	48.317300
1691.061375	152.918050	48.322305
1687.311843	152.658982	48.327309
1683.972312	154.955509	48.332314
1680.372532	155.768604	48.337319
1676.459942	158.656633	48.342324
1673.180578	150.544461	48.347329
1669.802294	155.907882	48.352333
1666.069056	151.280703	48.357338
1662.644771	147.792036	48.362343
1659.064313	143.084087	48.367348
1655.788490	140.717525	48.372353
1652.054906	144.865871	48.377357
1648.600642	143.966083	48.382362
1645.213541	144.144645	48.387367
1641.497958	149.048176	48.392372
1638.423099	149.510247	48.397377
1634.758742	155.107210	48.402381
1631.317829	146.801242	48.407386
1627.622182	155.746636	48.412391
1623.789476	162.510536	48.417396
1620.689593	140.162762	48.422401
1617.149427	146.115857	48.427405
1613.730018	150.418759	48.432410
1610.366565	149.491318	48.437415
1606.797790	146.130456	48.442420
1603.513507	150.136470	48.447425
1599.452005	146.858296	48.452429
1595.777940	145.105415	48.457434
1592.843575	137.450374	48.462439
1589.523981	150.994869	48.467444
1586.297943	146.753132	48.472449
1582.171030	145.059561	48.477453
1578.338723	139.488276	48.482458
1574.895967	143.986690	48.487463
1571.161723	141.862561	48.492468
1567.963324	141.396191	48.497473
1564.588184	142.737109	48.502477
1561.059283	138.608957	48.507482
1557.814447	130.389154	48.512487
1554.170515	148.734514	48.517492
1550.967094	133.079605	48.522497
1547.048965	140.985492	48.527501
1543.290768	130.164321	48.532506
1540.227728	141.020647	48.537511
1536.600226	149.818061	48.542516
1533.040183	148.085206	48.547521
1529.447609	148.035088	48.552525
1525.980052	142.772979	48.557530
1522.585462	143.163442	48.562535
1518.773824	150.370306	48.567540
1515.745837	129.990189	48.572545
1511.968197	144.718913	48.577549
1508.462497	139.274101	48.582554
1504.800566	140.950930	48.587559
1501.509443	142.947521	48.592564
1497.957157	145.565612	48.597569
1494.623553	147.599249	48.602573
1491.316996	140.038372	48.607578
1487.889703	133.456763	48.612583
1483.893312	148.687496	48.617588
1480.615999	145.224546	48.622593
1477.033096	141.932059	48.627597
1473.706969	141.190748	48.632602
1470.226786	133.051689	48.637607
1466.347833	139.858120	48.642612
1462.809286	148.457912	48.647617
1459.166655	140.168593	48.652621
1455.869967	145.677502	48.657626
1452.698980	141.145945	48.662631
1449.145332	141.267044	48.667636
1445.751092	139.478556	48.672641
1442.121765	143.167969	48.677645
1438.710920	138.189775	48.682650
1435.332187	137.334283	48.687655
1431.279925	145.147278	48.692660
1427.789106	143.684635	48.697665
1424.430687	144.288223	48.702669
1421.004702	145.637101	48.707674
1417.544285	140.954070	48.712679
1413.954503	146.870176	48.717684
1410.469501	145.470520	48.722689
1406.828212	144.490468	48.727693
1403.242242	148.495168	48.732698
1399.756571	144.649287	48.737703
1396.031283	143.188264	48.742708
1393.344203	139.147387	48.747713
1389.814844	130.794365	48.752717
1386.298408	136.816528	48.757722
1382.447612	140.871088	48.762727
1378.585909	141.881420	48.767732
1375.523999	136.727406	48.772737
1371.817182	137.876631	48.777741
1368.487619	135.752672	48.782746
1364.976832	136.024408	48.787751
1361.311704	142.511310	48.792756
1357.789010	139.495872	48.797761
1354.785363	138.971522	48.802765
1351.263356	135.672606	48.807770
1347.518124	135.185622	48.812775
1343.747693	147.678288	48.817780
1340.614081	147.904851	48.822785
1336.922525	146.405729	48.827789
1333.245440	147.050410	48.832794
1329.899891	142.354327	48.837799
1326.045013	144.801350	48.842804
1323.025081	148.708482	48.847809
1319.108038	137.153369	48.852813
1315.743018	141.629628	48.857818
1312.895758	141.993221	48.862823
1308.921628	141.488988	48.867828
1305.540570	130.938612	48.872833
1301.940358	143.146935	48.877837
1298.652575	136.041134	48.882842
1294.992752	132.547079	48.887847
1291.109098	147.440974	48.892852
1287.672718	133.882166	48.897857
1284.392611	132.501720	48.902861
1280.664712	130.231979	48.907866
1277.363642	141.768309	48.912871
1273.690282	140.569729	48.917876
1270.390774	135.473964	48.922881
1267.081848	137.349181	48.927885
1263.186353	130.776977	48.932890
1260.108746	129.935029	48.937895
1256.462882	130.359904	48.942900
1252.465311	127.285604	48.947905
1249.061786	136.105291	48.952909
1245.955655	130.653054	48.957914
1242.637436	127.539080	48.962919
1239.133696	139.388876	48.967924
1235.787648	130.917191	48.972929
1231.953434	136.809863	48.977933
1227.609907	139.513670	48.982938
1224.691464	128.024480	48.987943
1221.497826	141.907078	48.992948
1217.952074	134.991950	48.997953
1214.457098	138.800763	49.002957
1210.776562	136.803642	49.007962
1207.459237	136.067808	49.012967
1203.589700	145.010431	49.017972
1200.404179	138.818179	49.022977
1196.396205	133.030162	49.027981
1192.955250	136.108580	49.032986
1190.207890	132.022995	49.037991
1186.666724	138.066398	49.042996
1183.000859	124.356141	49.048001
1179.579880	137.877080	49.053005
1175.856723	128.323881	49.058010
1172.198349	132.674087	49.063015
1168.549801	134.619742	49.068020
1164.991756	122.570923	49.073025
1161.564413	126.510045	49.078029
1158.315165	128.739726	49.083034
1154.978407	127.950922	49.088039
1151.118390	139.468586	49.093044
1147.573614	134.828813	49.098049
1144.147539	137.201115	49.103053
1140.662375	130.126829	49.108058
1137.309859	126.906751	49.113063
1133.569356	137.123514	49.118068
1130.274331	133.224745	49.123073
1126.897620	134.852029	49.128077
1122.933207	124.204846	49.133082
1119.567669	126.617443	49.138087
1116.452353	132.602084	49.143092
1112.766299	127.621710	49.148097
1109.617386	127.859679	49.153101
1105.312150	133.146271	49.158106
1102.359268	122.974774	49.163111
1098.649118	133.761556	49.168116
1095.079566	127.008566	49.173121
1091.690757	128.886329	49.178125
1088.223075	135.110217	49.183130
1084.907931	113.222624	49.188135
1081.350846	132.309288	49.193140
1077.891582	128.494652	49.198145
1074.155290	130.393977	49.203149
1070.268928	124.481927	49.208154
1067.148898	129.784813	49.213159
1063.375661	127.818610	49.218164
1060.304813	123.151393	49.223169
1056.522270	127.482641	49.228173
1053.192940	137.149554	49.233178
1050.006865	125.179629	49.238183
1045.932549	131.866717	49.243188
1042.638845	121.561010	49.248193
1039.300798	124.935055	49.253197
1035.576852	130.398169	49.258202
1032.479030	128.022141	49.263207
1028.484163	140.438644	49.268212
1025.098731	131.769258	49.273217
1021.702825	125.430537	49.278221
1018.115074	121.190520	49.283226
1014.643056	122.548570	49.288231
1011.016091	131.731316	49.293236
1007.561012	125.287582	49.298241
1004.325025	127.466841	49.303245
1000.556262	131.043427	49.308250
997.233649	125.725602	49.313255
993.761344	128.949301	49.318260
990.189205	130.160597	49.323265
986.665697	130.637444	49.328269
982.735327	139.805056	49.333274
979.542163	135.551091	49.338279
975.854102	134.451535	49.343284
972.945259	119.905875	49.348289
969.063159	128.431256	49.353293
965.292956	128.284251	49.358298
962.162466	128.848827	49.363303
958.478085	134.759509	49.368308
954.921263	132.464852	49.373313
951.517263	132.278396	49.378317
948.085134	127.815680	49.383322
944.599401	124.795287	49.388327
941.177963	127.595795	49.393332
937.943718	128.357973	49.398337
934.363603	128.310084	49.403341
930.429472	123.307527	49.408346
926.877307	119.955412	49.413351
923.279555	129.333674	49.418356
919.933005	129.319059	49.423361
916.652714	125.872495	49.428365
912.948259	127.092010	49.433370
909.498465	125.849570	49.438375
905.754168	129.614977	49.443380
902.377879	120.648398	49.448385
899.156352	125.201027	49.453389
895.478708	134.146210	49.458394
892.519285	120.666917	49.463399
888.841412	126.965323	49.468404
885.119183	119.292469	49.473409
881.340522	129.902745	49.478413
877.686158	128.835185	49.483418
874.413537	117.381419	49.488423
871.157276	127.086457	49.493428
867.549753	119.183239	49.498433
863.946835	122.050838	49.503437
860.152350	124.146899	49.508442
857.026886	122.044767	49.513447
853.684928	120.371858	49.518452
850.296270	128.474253	49.523457
846.585331	125.467656	49.528461
842.882953	137.343824	49.533466
839.503178	126.374168	49.538471
835.811251	129.696422	49.543476
832.024914	124.546303	49.548481
828.917984	124.783451	49.553485
825.418011	124.359269	49.558490
822.210206	115.891286	49.563495
818.212579	122.950070	49.568500
815.024301	113.146664	49.573505
811.258095	117.929884	49.578509
807.574319	111.576606	49.583514
804.731106	118.222161	49.588519
801.200683	114.352312	49.593524
797.615685	124.849011	49.598529
793.944350	112.423155	49.603533
790.349095	120.258960	49.608538
787.331989	114.534828	49.613543
783.607333	125.220680	49.618548
779.480109	118.623735	49.623553
776.453373	111.592309	49.628557
772.833395	117.378007	49.633562
769.557828	106.821517	49.638567
765.852876	120.919135	49.643572
762.208959	116.685736	49.648577
759.130940	117.796860	49.653581
755.168362	109.842399	49.658586
751.959783	115.578760	49.663591
748.575146	125.405051	49.668596
745.058560	124.896481	49.673601
741.281466	122.208022	49.678605
737.535703	126.963252	49.683610
734.381230	112.572459	49.688615
730.588311	126.685899	49.693620
727.540298	115.706671	49.698625
724.214626	119.255535	49.703629
720.277201	122.784019	49.708634
717.080664	119.263544	49.713639
713.020406	124.137709	49.718644
709.698928	123.677290	49.723649
706.248883	117.571243	49.728653
702.503309	128.156843	49.733658
699.388057	123.546243	49.738663
695.760595	122.772957	49.743668
692.486594	118.630943	49.748673
689.060852	115.143813	49.753677
685.031347	120.705930	49.758682
681.936061	121.716779	49.763687
678.145198	122.125425	49.768692
674.942772	116.701911	49.773697
671.292930	114.264320	49.778701
667.859992	120.398722	49.783706
664.348890	119.837813	49.788711
660.729356	121.782279	49.793716
657.555910	114.414198	49.798721
653.674711	121.044939	49.803725
650.102338	126.490143	49.808730
647.253294	119.632968	49.813735
643.318114	118.258843	49.818740
639.691233	116.633042	49.823745
636.274445	115.261450	49.828749
632.989236	127.734709	49.833754
629.422527	113.561851	49.838759
625.496522	118.116630	49.843764
621.965374	118.980469	49.848769
618.903933	114.613789	49.853773
614.817551	130.555401	49.858778
611.479848	111.123927	49.863783
608.072024	122.634259	49.868788
604.546751	122.982104	49.873793
601.277944	117.283943	49.878797
598.157057	124.948990	49.883802
594.604951	116.160306	49.888807
591.128070	127.002709	49.893812
587.424922	124.153931	49.898817
583.438106	122.901318	49.903821
579.669776	123.831421	49.908826
576.699890	117.455536	49.913831
573.190299	125.750902	49.918836
569.823222	121.966826	49.923841
566.391443	119.327366	49.928845
562.280637	119.109453	49.933850
559.434379	112.483164	49.938855
555.582059	116.000639	49.943860
552.450843	123.289939	49.948865
548.678860	122.304984	49.953869
545.102927	129.569877	49.958874
541.809903	113.314214	49.963879
538.133431	129.429748	49.968884
534.748101	125.221709	49.973889
531.060118	121.243511	49.978893
527.644355	129.917207	49.983898
524.011573	122.857000	49.988903
520.588839	129.345033	49.993908
517.343698	122.697207	49.998913
513.748323	123.770330	50.003917
510.156424	126.089224	50.008922
506.924819	121.311640	50.013927
502.806860	124.334965	50.018932
499.623437	122.436542	50.023937
496.216585	117.117787	50.028941
492.639147	122.562985	50.033946
489.327820	124.056235	50.038951
485.418781	123.118182	50.043956
482.106815	118.113421	50.048961
478.733186	123.772432	50.053965
474.978161	113.952777	50.058970
471.470911	116.416893	50.063975
467.891045	117.686787	50.068980
464.582416	122.057096	50.073985
461.114224	105.333149	50.078989
457.442907	106.022697	50.083994
454.423008	112.108209	50.088999
450.816739	112.341583	50.094004
447.255190	114.503549	50.099009
443.833830	105.882947	50.104013
439.825400	110.303996	50.109018
436.419873	110.385839	50.114023
432.852508	106.622140	50.119028
429.268319	114.709791	50.124033
426.059111	109.502131	50.129037
422.407139	123.442449	50.134042
418.956299	102.997750	50.139047
415.844575	108.847932	50.144052
411.993141	108.567961	50.149057
408.836868	116.870483	50.154061
405.096870	114.279809	50.159066
401.727955	121.658040	50.164071
397.806300	116.176652	50.169076
394.300844	124.562450	50.174081
391.044677	112.682764	50.179085
387.444444	119.231963	50.184090
384.200968	108.146607	50.189095
380.467116	114.969998	50.194100
377.252292	121.584633	50.199105
373.531979	117.077991	50.204109
370.257272	117.905583	50.209114
366.349879	110.938722	50.214119
362.683268	116.864944	50.219124
359.238427	117.147759	50.224129
355.954042	110.359401	50.229133
352.411319	112.417886	50.234138
349.205722	113.686693	50.239143
345.794246	109.866005	50.244148
342.290617	107.035643	50.249153
338.684113	113.141733	50.254157
334.843903	110.972112	50.259162
331.322763	105.288699	50.264167
328.006835	110.352963	50.269172
324.321963	113.874619	50.274177
321.135729	115.057749	50.279181
317.117623	112.625847	50.284186
313.968619	102.351885	50.289191
310.239571	117.336346	50.294196
306.750007	115.404101	50.299201
303.727461	107.494867	50.304205
299.784169	119.532868	50.309210
296.572330	118.662308	50.314215
292.840280	121.517159	50.319220
289.438845	115.065815	50.324225
286.224773	107.651158	50.329229
282.396174	114.935165	50.334234
279.064511	110.775882	50.339239
275.080059	108.076382	50.344244
271.678848	109.176675	50.349249
268.661067	104.902700	50.354253
264.650831	102.020032	50.359258
261.455603	111.180815	50.364263
257.780781	107.738640	50.369268
254.294987	114.831730	50.374273
251.001467	106.756422	50.379277
247.516013	115.142767	50.384282
243.996346	110.620093	50.389287
240.086941	114.949713	50.394292
236.821654	114.674159	50.399297
233.600893	112.521105	50.404301
229.987218	111.270417	50.409306
226.609630	112.452862	50.414311
222.932691	106.658103	50.419316
218.998399	108.226092	50.424321
215.773073	100.408255	50.429325
212.432264	117.208455	50.434330
209.176246	101.144143	50.439335
205.513919	115.947702	50.444340
201.942307	113.841531	50.449345
198.544955	109.408097	50.454349
194.581526	110.948985	50.459354
191.129344	105.498551	50.464359
188.089468	113.569571	50.469364
184.318871	109.151207	50.474369
180.742611	102.951813	50.479373
176.847739	111.750394	50.484378
174.177752	97.244741	50.489383
170.558538	115.257454	50.494388
166.769933	108.382376	50.499393
163.271236	106.892625	50.504397
159.636515	110.115041	50.509402
156.093758	109.509358	50.514407
152.897060	108.676862	50.519412
149.404475	104.430981	50.524417
146.012571	106.440916	50.529421
142.030917	111.923408	50.534426
139.070369	100.757937	50.539431
135.313166	108.999505	50.544436
131.555635	105.094653	50.549441
128.449511	95.761132	50.554445
124.393660	112.769609	50.559450
121.283492	101.463458	50.564455
117.826079	110.047712	50.569460
114.326052	115.308117	50.574465
111.162527	100.852371	50.579469
107.296701	108.299805	50.584474
103.772029	102.711535	50.589479
99.950544	113.140770	50.594484
96.632324	116.740434	50.599489
93.288461	102.155233	50.604493
89.436995	106.343558	50.609498
86.239292	105.123929	50.614503
82.767691	105.974235	50.619508
79.365355	110.186987	50.624513
75.589282	106.270871	50.629517
71.725118	112.438773	50.634522
68.762344	108.761830	50.639527
65.307005	105.307253	50.644532
61.767038	111.464696	50.649537
58.597000	112.211033	50.654541
54.905263	115.255563	50.659546
51.378870	109.156348	50.664551
47.621442	118.792771	50.669556
43.591631	108.867330	50.674561
40.299751	109.346423	50.679565
37.167374	111.082643	50.684570
34.123221	104.316829	50.689575
30.396778	104.285839	50.694580
26.570045	101.901586	50.699585
23.343346	97.297293	50.704589
19.449445	102.166820	50.709594
16.421545	97.108190	50.714599
12.633112	107.688098	50.719604
9.200511	99.293979	50.724609
5.974336	102.058316	50.729613
2.234452	104.200615	50.734618