Fri Jun 17 18:14:43 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.402695	109.445273	0.000000
0.090065	105.786877	0.005005
0.180868	93.942094	0.010010
0.030075	94.603977	0.015014
-0.337980	82.069041	0.020019
-0.283548	70.449554	0.025024
-0.705448	56.536560	0.030029
-1.154585	44.964877	0.035034
-1.612704	40.941348	0.040038
-2.165857	39.557500	0.045043
-1.991016	29.928617	0.050048
-2.819329	33.201294	0.055053
-3.191190	20.060255	0.060058
-3.452095	28.978524	0.065062
-3.606150	26.929845	0.070067
-3.481208	25.896817	0.075072
-3.706329	20.483653	0.080077
-4.509008	24.175733	0.085082
-4.904954	10.838614	0.090086
-5.113654	22.666695	0.095091
-4.910429	23.313343	0.100096
-4.998183	35.678982	0.105101
-5.147911	31.542434	0.110106
-5.878405	17.767592	0.115110
-6.343167	21.914390	0.120115
-6.284613	17.767104	0.125120
-6.375457	22.051054	0.130125
-6.737656	25.553301	0.135130
-7.453900	19.235124	0.140134
-7.935122	23.758992	0.145139
-7.656144	26.405211	0.150144
-8.005268	28.926337	0.155149
-8.275373	23.078633	0.160154
-7.872602	31.197124	0.165158
-8.395375	31.355486	0.170163
-8.505587	23.827589	0.175168
-9.061392	20.432812	0.180173
-9.613634	29.511390	0.185178
-9.848104	22.641915	0.190182
-10.101810	31.835249	0.195187
-10.240171	22.288817	0.200192
-10.020539	26.464136	0.205197
-10.415498	35.264586	0.210202
-11.053225	26.463193	0.215206
-11.346392	30.359477	0.220211
-11.502599	23.286570	0.225216
-11.345304	37.675934	0.230221
-11.351189	23.636402	0.235226
-11.381788	28.854757	0.240230
-12.707548	20.788327	0.245235
-13.077064	16.571892	0.250240
-13.250968	20.999490	0.255245
-13.099417	26.861051	0.260250
-12.620703	14.978295	0.265254
-13.531698	32.253162	0.270259
-13.810584	17.707477	0.275264
-14.279776	25.729959	0.280269
-14.529217	26.237548	0.285274
-14.695313	21.070707	0.290278
-14.690453	22.656460	0.295283
-14.636390	22.756239	0.300288
-15.401290	25.440400	0.305293
-15.814280	24.249729	0.310298
-16.061322	23.679503	0.315302
-16.148773	27.297498	0.320307
-16.232911	20.790985	0.325312
-16.187123	22.260615	0.330317
-16.852886	25.023806	0.335322
-17.016242	16.666493	0.340326
-17.225362	26.279827	0.345331
-17.367257	21.778304	0.350336
-17.397674	29.274198	0.355341
-18.031338	19.463784	0.360346
-18.572024	21.286830	0.365350
-18.923944	36.054850	0.370355
-18.592040	31.224950	0.375360
-19.235824	26.544992	0.380365
-19.173630	26.127207	0.385370
-19.617157	23.999959	0.390374
-20.575500	27.884462	0.395379
-20.476028	22.033740	0.400384
-20.694796	24.895691	0.405389
-20.842023	22.096423	0.410394
-20.690962	22.626832	0.415398
-20.951485	25.263862	0.420403
-20.914575	16.255229	0.425408
-21.450157	22.483187	0.430413
-21.882828	19.549626	0.435418
-22.018798	21.709926	0.440422
-22.313304	36.596864	0.445427
-22.387572	23.755634	0.450432
-23.242668	34.579216	0.455437
-23.854510	28.109503	0.460442
-23.119751	21.613096	0.465446
-23.682249	28.433965	0.470451
-23.852481	22.848094	0.475456
-23.858367	23.486678	0.480461
-24.027691	23.863540	0.485466
-24.345617	16.494688	0.490470
-25.434037	25.125653	0.495475
-25.112679	20.622509	0.500480
-25.678322	22.009464	0.505485
-25.645356	23.123073	0.510490
-25.300207	11.605478	0.515494
-26.043154	28.319818	0.520499
-26.399689	26.494429	0.525504
-26.812855	24.334706	0.530509
-27.196577	29.248868	0.535514
-27.098422	17.411804	0.540518
-27.071565	24.589750	0.545523
-27.262641	19.644914	0.550528
-27.855449	30.617292	0.555533
-28.427357	22.687026	0.560538
-28.317313	25.376123	0.565542
-28.775902	24.411870	0.570547
-28.446657	19.755078	0.575552
-29.048392	18.735885	0.580557
-29.725523	24.125046	0.585562
-29.992322	30.231175	0.590566
-30.393234	26.428034	0.595571
-30.377515	21.449417	0.600576
-30.022074	29.098432	0.605581
-29.948260	32.125459	0.610586
-30.683758	22.589883	0.615590
-31.734077	28.745145	0.620595
-31.504932	19.422773	0.625600
-31.638870	24.576410	0.630605
-31.975992	27.173092	0.635610
-31.889394	17.210798	0.640614
-32.166413	21.259497	0.645619
-32.659387	18.813497	0.650624
-33.195618	27.994985	0.655629
-33.671406	24.398858	0.660634
-33.256355	29.769275	0.665638
-33.441520	24.172270	0.670643
-33.345622	29.147998	0.675648
-34.190818	27.290173	0.680653
-34.757204	27.616808	0.685658
-34.757952	25.574813	0.690662
-35.354636	23.638189	0.695667
-34.991602	29.973507	0.700672
-35.284232	22.911243	0.705677
-35.467134	29.840100	0.710682
-35.591879	30.960981	0.715686
-36.691012	30.094321	0.720691
-36.698159	19.563909	0.725696
-36.660794	24.536932	0.730701
-36.885624	34.063294	0.735706
-36.638598	17.417049	0.740710
-37.331279	28.867382	0.745715
-37.945238	21.216027	0.750720
-38.100419	26.343794	0.755725
-38.635594	25.339192	0.760730
-38.496167	18.909379	0.765734
-38.385754	20.710434	0.770739
-38.429100	14.941667	0.775744
-38.759451	30.907038	0.780749
-39.380386	23.626045	0.785754
-39.400539	18.127116	0.790758
-40.126383	31.989782	0.795763
-39.905658	22.009532	0.800768
-40.487083	28.562616	0.805773
-40.932303	27.171688	0.810778
-41.265575	25.876011	0.815782
-41.757721	20.940572	0.820787
-41.664691	25.150546	0.825792
-41.705200	28.803361	0.830797
-41.836542	40.244655	0.835802
-41.782802	18.490907	0.840806
-41.842660	32.000553	0.845811
-42.346721	24.384012	0.850816
-43.093117	21.554301	0.855821
-42.972681	28.581325	0.860826
-42.934237	20.112526	0.865830
-44.003593	26.520181	0.870835
-44.253201	23.200409	0.875840
-44.251488	26.044656	0.880845
-44.640213	20.734861	0.885850
-44.448355	28.642728	0.890854
-44.737936	24.641317	0.895859
-44.769667	22.651043	0.900864
-45.405202	22.532554	0.905869
-46.091656	27.154672	0.910874
-45.927069	25.977121	0.915878
-46.287025	20.149884	0.920883
-46.382093	20.977336	0.925888
-46.288667	23.626374	0.930893
-47.046346	24.839636	0.935898
-47.302473	23.749580	0.940902
-47.525834	22.458919	0.945907
-47.479642	24.898549	0.950912
-47.452506	16.974878	0.955917
-48.371328	24.381252	0.960922
-48.439516	13.831392	0.965926
-49.097122	24.843940	0.970931
-49.261316	20.676850	0.975936
-49.382896	24.353598	0.980941
-49.507769	33.021736	0.985946
-49.132614	22.539661	0.990950
-49.951417	27.705319	0.995955
-50.234767	24.805547	1.000960
-50.472913	14.022083	1.005965
-50.774246	23.058559	1.010970
-51.120781	21.792714	1.015974
-50.846953	33.089103	1.020979
-51.174895	29.809583	1.025984
-51.906786	23.245186	1.030989
-52.162479	27.887656	1.035994
-52.285966	23.611582	1.040998
-52.439811	18.122840	1.046003
-52.383048	25.278449	1.051008
-52.466148	24.884420	1.056013
-53.494246	26.607935	1.061018
-53.639348	10.425682	1.066022
-54.313156	20.498479	1.071027
-53.993749	32.904172	1.076032
-53.949745	20.794520	1.081037
-53.991374	22.638213	1.086042
-54.361952	23.999259	1.091046
-55.173249	28.039094	1.096051
-55.383786	13.713134	1.101056
-55.370463	20.975414	1.106061
-55.776275	25.326125	1.111066
-55.655337	26.154968	1.116070
-56.381983	27.621771	1.121075
-56.931725	21.344995	1.126080
-57.107620	24.709718	1.131085
-57.174774	27.590670	1.136090
-57.018023	23.916831	1.141094
-57.497330	27.668435	1.146099
-57.488103	20.402477	1.151104
-57.338156	19.062985	1.156109
-57.816957	19.498197	1.161114
-58.518482	21.831834	1.166118
-59.082984	30.272911	1.171123
-58.836667	20.394572	1.176128
-58.965258	22.902326	1.181133
-59.480667	23.309683	1.186138
-59.963145	15.928133	1.191142
-60.448484	25.324340	1.196147
-60.501092	22.754035	1.201152
-60.615973	22.035356	1.206157
-60.959342	14.088818	1.211162
-60.167692	11.419023	1.216166
-60.659720	28.080209	1.221171
-61.056714	31.848915	1.226176
-61.417669	25.669810	1.231181
-61.739516	22.437033	1.236186
-62.875635	18.862471	1.241190
-63.061175	21.859397	1.246195
-62.905455	20.695752	1.251200
-62.881805	18.051402	1.256205
-63.452830	26.828231	1.261210
-63.513494	14.776042	1.266214
-63.908244	26.000833	1.271219
-64.029682	22.142757	1.276224
-63.466558	15.795446	1.281229
-64.296716	21.046856	1.286234
-64.734704	17.725645	1.291238
-65.068615	18.108950	1.296243
-65.303219	17.622104	1.301248
-65.388205	16.905560	1.306253
-65.572450	13.161129	1.311258
-66.142221	12.079010	1.316262
-66.981556	19.454018	1.321267
-66.586893	15.399649	1.326272
-66.667728	18.919455	1.331277
-66.938231	19.562758	1.336282
-66.687350	22.526802	1.341286
-67.099593	31.879488	1.346291
-67.614027	24.468320	1.351296
-68.013301	25.337066	1.356301
-68.297853	23.346984	1.361306
-68.227439	19.379270	1.366310
-68.832042	21.329766	1.371315
-69.449041	24.203256	1.376320
-69.673039	29.026146	1.381325
-69.971685	32.447781	1.386330
-69.808269	18.337892	1.391334
-69.990894	24.903813	1.396339
-70.043210	17.750106	1.401344
-69.930899	19.194665	1.406349
-70.534978	28.333761	1.411354
-71.332568	20.335055	1.416358
-71.957787	24.195372	1.421363
-71.896929	23.540619	1.426368
-71.723867	27.346577	1.431373
-71.924031	29.870769	1.436378
-71.593151	26.115099	1.441382
-72.154713	28.574259	1.446387
-72.643158	24.549079	1.451392
-73.292602	21.106340	1.456397
-73.481615	25.236314	1.461402
-73.272409	12.229977	1.466406
-73.740118	20.806508	1.471411
-73.852998	26.956510	1.476416
-74.476827	23.941466	1.481421
-74.806019	25.497107	1.486426
-75.152036	22.245459	1.491430
-74.973760	24.207105	1.496435
-74.869616	23.986186	1.501440
-75.011803	21.598502	1.506445
-75.676523	25.686394	1.511450
-76.115356	24.009664	1.516454
-76.457268	26.026407	1.521459
-76.473465	14.861319	1.526464
-76.569896	12.677172	1.531469
-76.857603	23.463462	1.536474
-77.315018	19.009461	1.541478
-77.843621	22.588902	1.546483
-78.046185	29.716975	1.551488
-78.443807	23.974934	1.556493
-78.166471	26.696207	1.561498
-77.963986	27.693035	1.566502
-78.453260	32.923108	1.571507
-78.664962	21.047178	1.576512
-79.318296	24.171199	1.581517
-79.691847	25.338571	1.586522
-79.540593	28.048243	1.591526
-80.036272	27.998665	1.596531
-80.193389	32.611136	1.601536
-80.594872	32.087899	1.606541
-81.141186	34.453163	1.611546
-81.107942	24.603532	1.616550
-80.883562	32.605641	1.621555
-81.108738	29.349297	1.626560
-81.908334	24.466945	1.631565
-82.708713	31.939083	1.636570
-82.415634	22.278517	1.641574
-82.487917	30.712560	1.646579
-82.706582	30.671001	1.651584
-82.854371	29.126052	1.656589
-83.100560	25.819331	1.661594
-83.023161	21.783561	1.666598
-84.114898	31.232626	1.671603
-84.270727	31.346772	1.676608
-84.368608	26.901674	1.681613
-84.524788	29.780455	1.686618
-84.366154	17.473567	1.691622
-84.694049	25.066855	1.696627
-85.580480	29.311778	1.701632
-85.974411	29.804911	1.706637
-86.095468	23.162070	1.711642
-86.001088	21.142742	1.716646
-86.146879	19.763020	1.721651
-86.305889	29.803330	1.726656
-86.218974	24.104272	1.731661
-87.369079	26.983903	1.736666
-87.494396	20.099845	1.741670
-87.789440	28.954525	1.746675
-87.783981	27.078044	1.751680
-87.694742	25.828758	1.756685
-88.171521	33.537177	1.761690
-88.633763	25.919416	1.766694
-89.118625	23.555743	1.771699
-89.584670	22.660422	1.776704
-89.316531	18.878677	1.781709
-89.493128	23.039541	1.786714
-89.404748	26.281007	1.791718
-89.520364	28.299992	1.796723
-90.164113	21.431473	1.801728
-90.815444	27.329408	1.806733
-91.377976	29.441828	1.811738
-91.128899	24.241299	1.816742
-91.226970	32.207620	1.821747
-91.046548	26.426122	1.826752
-91.538876	25.498073	1.831757
-92.277855	25.477891	1.836762
-92.208374	25.140983	1.841766
-92.639278	30.651228	1.846771
-92.649253	26.327675	1.851776
-92.690233	29.755020	1.856781
-93.397595	32.543688	1.861786
-93.886527	28.714144	1.866790
-94.067539	38.296565	1.871795
-94.133755	27.021586	1.876800
-93.845736	24.040649	1.881805
-93.944132	35.373255	1.886810
-94.764383	30.626944	1.891814
-95.351144	30.244420	1.896819
-95.619617	27.563780	1.901824
-95.525215	28.691249	1.906829
-95.929025	29.837210	1.911834
-95.575928	25.196971	1.916838
-96.453986	33.106675	1.921843
-96.907530	27.332889	1.926848
-97.279859	33.085782	1.931853
-97.169708	33.948383	1.936858
-97.312481	25.461957	1.941862
-97.578236	29.827474	1.946867
-97.602454	24.442291	1.951872
-97.413682	26.727389	1.956877
-98.411158	30.944402	1.961882
-98.714808	27.994139	1.966886
-99.115216	27.824141	1.971891
-98.953926	29.331991	1.976896
-99.028109	21.841133	1.981901
-99.205828	26.761505	1.986906
-99.895210	22.758683	1.991910
-100.008298	25.105603	1.996915
-100.524097	24.300085	2.006912
-100.236237	31.372545	2.016909
-99.597636	35.790482	2.026906
-99.272797	30.582840	2.036902
-98.315262	26.264844	2.046899
-97.766157	33.142530	2.056896
-97.743541	34.029146	2.066893
-97.362662	31.727305	2.076890
-96.562724	33.430918	2.086886
-96.079600	29.486974	2.096883
-95.191647	34.829040	2.106880
-94.683677	34.117941	2.116877
-94.787496	30.834082	2.126874
-94.438438	31.412737	2.136870
-93.605464	25.872267	2.146867
-93.261575	30.773874	2.156864
-92.437541	27.292305	2.166861
-92.168648	26.401635	2.176858
-91.378851	25.945790	2.186854
-90.738187	27.290202	2.196851
-90.411884	19.569481	2.206848
-90.433958	25.902544	2.216845
-89.213062	27.215309	2.226842
-89.024009	29.472145	2.236838
-88.831430	29.898792	2.246835
-87.949560	29.826954	2.256832
-87.419600	37.023956	2.266829
-87.279461	35.479356	2.276826
-86.315914	35.888882	2.286822
-86.020385	33.295572	2.296819
-85.759457	32.673949	2.306816
-84.497345	35.456391	2.316813
-84.404185	32.287577	2.326810
-84.186210	33.202968	2.336806
-83.579527	36.258555	2.346803
-83.076171	40.356570	2.356800
-82.800457	38.415213	2.366797
-81.992700	28.697517	2.376794
-81.440676	26.762391	2.386790
-80.964297	26.078676	2.396787
-80.018677	32.626285	2.406784
-79.562799	34.908515	2.416781
-79.804105	35.224130	2.426778
-79.488954	28.784400	2.436774
-78.849255	30.702160	2.446771
-77.853089	28.385767	2.456768
-76.927978	26.755531	2.466765
-76.623218	23.293898	2.476762
-76.519075	27.442466	2.486758
-76.321748	24.529989	2.496755
-75.822577	21.907373	2.506752
-75.119831	21.890604	2.516749
-74.507323	23.196825	2.526746
-73.715181	24.743081	2.536742
-73.451792	22.337878	2.546739
-73.166182	22.033816	2.556736
-72.414288	18.464466	2.566733
-72.011739	30.361375	2.576730
-71.430973	35.068510	2.586726
-70.734668	27.272844	2.596723
-70.435142	31.120224	2.606720
-69.948714	34.099778	2.616717
-69.630718	34.875451	2.626714
-68.838237	34.664955	2.636710
-68.358829	28.487972	2.646707
-68.266598	30.572214	2.656704
-67.541483	40.144708	2.666701
-67.064649	30.847153	2.676698
-66.179602	29.330274	2.686694
-65.888805	28.849700	2.696691
-65.913404	38.045948	2.706688
-64.879161	34.044575	2.716685
-64.593220	31.664469	2.726682
-63.882501	32.731890	2.736678
-62.752036	29.232385	2.746675
-63.052444	25.164007	2.756672
-62.808315	27.693836	2.766669
-61.976596	31.955992	2.776666
-61.042845	35.573078	2.786662
-61.161406	24.251286	2.796659
-60.715421	34.254671	2.806656
-59.694082	31.967488	2.816653
-59.633438	27.623333	2.826650
-58.951828	27.476121	2.836646
-58.099820	27.537089	2.846643
-58.108207	27.179551	2.856640
-57.700004	28.966665	2.866637
-56.870138	33.520169	2.876634
-56.649165	28.350738	2.886630
-55.344641	28.210430	2.896627
-55.306858	32.635778	2.906624
-55.191589	35.595628	2.916621
-54.476507	38.737723	2.926618
-53.460062	36.258911	2.936614
-53.217600	37.182880	2.946611
-53.084467	30.965455	2.956608
-52.904128	29.560384	2.966605
-51.826165	36.412016	2.976602
-51.790901	31.560144	2.986598
-50.856757	30.194555	2.996595
-50.088291	32.968968	3.006592
-50.174650	33.850582	3.016589
-49.345117	36.410349	3.026586
-48.706304	37.289180	3.036582
-48.769001	30.106125	3.046579
-47.933615	30.197520	3.056576
-47.243870	37.919027	3.066573
-46.922933	28.234640	3.076570
-46.361926	32.028285	3.086566
-45.497386	29.487987	3.096563
-45.272302	29.291001	3.106560
-45.415701	29.713432	3.116557
-44.891739	33.426892	3.126554
-43.974186	35.220231	3.136550
-43.284462	32.138772	3.146547
-42.814437	31.024401	3.156544
-42.307899	32.723055	3.166541
-41.475591	27.305006	3.176538
-41.455659	38.340452	3.186534
-41.303226	32.280255	3.196531
-40.243087	28.560485	3.206528
-39.754524	31.313853	3.216525
-39.652949	27.250573	3.226522
-38.913024	28.307414	3.236518
-38.114501	27.787892	3.246515
-38.137354	27.626783	3.256512
-37.606538	31.211664	3.266509
-36.467792	33.640806	3.276506
-36.680444	33.889614	3.286502
-35.955396	33.870529	3.296499
-35.133317	27.707719	3.306496
-34.939081	33.383835	3.316493
-34.412573	32.013297	3.326490
-33.154024	32.796825	3.336486
-33.358779	31.934307	3.346483
-32.938589	30.664426	3.356480
-32.746805	32.074177	3.366477
-31.592162	33.466535	3.376474
-31.567770	30.399249	3.386470
-31.093963	32.549090	3.396467
-30.247832	27.353198	3.406464
-29.913531	33.565782	3.416461
-29.201963	34.209256	3.426458
-28.292503	31.145018	3.436454
-28.207188	35.756296	3.446451
-28.442430	31.882959	3.456448
-27.461485	34.554290	3.466445
-26.824582	34.302091	3.476442
-26.399693	34.242209	3.486438
-25.472526	34.718654	3.496435
-25.383618	24.304243	3.506432
-25.115126	31.532468	3.516429
-24.279215	24.299038	3.526426
-23.544945	26.999120	3.536422
-23.425597	30.202701	3.546419
-23.114691	35.145169	3.556416
-22.023866	30.149063	3.566413
-21.752860	30.702170	3.576410
-21.837392	30.388901	3.586406
-20.786227	35.661184	3.596403
-19.919988	33.301199	3.606400
-20.062899	31.033870	3.616397
-19.658041	34.516598	3.626394
-19.197333	35.480362	3.636390
-17.624927	36.893779	3.646387
-17.623819	28.855455	3.656384
-17.564484	34.183926	3.666381
-17.255824	37.753577	3.676378
-15.912236	32.879451	3.686374
-15.655577	25.155287	3.696371
-15.604966	28.048038	3.706368
-14.842876	30.186516	3.716365
-14.275253	36.899325	3.726362
-14.023769	33.823929	3.736358
-13.212859	31.008627	3.746355
-12.718590	34.501984	3.756352
-12.517324	29.567394	3.766349
-11.530903	37.501197	3.776346
-11.423573	34.646355	3.786342
-10.969043	30.629323	3.796339
-10.143597	25.620032	3.806336
-9.560447	30.873687	3.816333
-9.583637	31.217258	3.826330
-9.037129	29.694423	3.836326
-7.852026	27.355732	3.846323
-7.492457	27.937193	3.856320
-7.378598	29.571507	3.866317
-7.018787	28.510629	3.876314
-6.445332	31.539745	3.886310
-5.852611	35.730008	3.896307
-4.892328	24.542256	3.906304
-4.656429	27.211370	3.916301
-4.470817	29.075993	3.926298
-4.300913	31.099711	3.936294
-3.285962	36.456459	3.946291
-2.908645	30.929104	3.956288
-2.107755	40.182772	3.966285
-2.102158	54.415118	3.976282
-1.910621	65.519276	3.986278
-1.294527	73.938467	3.996275
-0.849935	94.924352	4.006272
-0.330834	118.995187	4.016269
0.000000	135.592838	4.021274
0.170301	144.652421	4.026278
0.304255	157.092207	4.031283
0.440479	152.691034	4.036288
0.538600	155.606305	4.041293
0.830326	168.632588	4.046298
1.140200	169.161667	4.051302
0.838418	175.230650	4.056307
0.691589	180.095222	4.061312
0.921242	182.830968	4.066317
0.739527	179.606630	4.071322
0.889667	184.114994	4.076326
0.919235	178.898805	4.081331
1.063055	184.686727	4.086336
1.058451	178.914416	4.091341
0.605732	188.717917	4.096346
0.930680	179.489042	4.101350
0.862767	185.080490	4.106355
0.812815	184.200051	4.111360
1.299510	177.833810	4.116365
1.022552	189.685400	4.121370
1.152767	183.539430	4.126374
1.369927	192.123184	4.131379
0.960100	180.651424	4.136384
1.182629	181.099513	4.141389
0.917705	186.524798	4.146394
1.200750	200.580842	4.151398
1.242595	209.947945	4.156403
1.340278	208.101894	4.161408
1.533897	207.998907	4.166413
0.854049	208.702948	4.171418
1.266521	201.519060	4.176422
1.166031	213.712122	4.181427
1.056729	209.899534	4.186432
1.337140	217.736152	4.191437
1.351573	222.049625	4.196442
1.394197	208.219123	4.201446
1.423667	217.828242	4.206451
1.376559	217.105588	4.211456
1.630217	210.593365	4.216461
1.283766	224.670984	4.221466
1.556955	214.412926	4.226470
1.061932	217.154477	4.231475
1.450447	211.488295	4.236480
1.445447	213.336578	4.241485
1.488213	218.435060	4.246490
1.510264	220.460393	4.251494
1.306997	218.300087	4.256499
1.709269	220.189408	4.261504
1.649520	217.879548	4.266509
1.197835	222.284110	4.271514
1.563786	209.644239	4.276518
1.315762	218.498711	4.281523
1.495345	217.646422	4.286528
1.560568	222.225151	4.291533
1.487409	218.852720	4.296538
1.142907	214.661867	4.301542
1.614533	223.151248	4.306547
1.219961	227.175336	4.311552
1.644692	223.435794	4.316557
1.564205	225.422523	4.321562
1.586922	218.461273	4.326566
1.541642	225.497386	4.331571
1.362027	220.048961	4.336576
1.632703	231.467388	4.341581
1.394886	243.684484	4.346586
1.580171	254.613531	4.351590
1.467771	246.241307	4.356595
1.469583	254.360456	4.361600
1.898518	248.082326	4.366605
1.543479	264.321007	4.371610
1.928028	248.074337	4.376614
1.726640	249.766814	4.381619
1.476784	262.035653	4.386624
1.728926	247.611448	4.391629
1.635625	255.931109	4.396634
1.677967	252.099225	4.401638
1.883726	262.641458	4.406643
2.207313	255.478041	4.411648
2.089654	255.711542	4.416653
1.824718	259.557607	4.421658
1.680457	256.701957	4.426662
1.766749	252.650636	4.431667
1.851227	255.177674	4.436672
2.253441	243.117034	4.441677
2.102933	247.811744	4.446682
2.110610	249.916430	4.451686
1.879440	257.804354	4.456691
1.867440	257.174726	4.461696
2.350674	250.632617	4.466701
1.964845	255.766434	4.471706
2.057525	253.205683	4.476710
2.049971	254.775369	4.481715
1.788064	256.265577	4.486720
1.614366	253.018381	4.491725
1.890663	251.773901	4.496730
2.185607	247.165367	4.501734
1.932420	253.950313	4.506739
1.759204	256.993976	4.511744
2.050432	279.075602	4.516749
2.085101	281.765039	4.521754
2.407196	283.245009	4.526758
2.247557	286.775213	4.531763
2.362539	279.781234	4.536768
2.092488	268.401813	4.541773
2.324045	270.168950	4.546778
2.444523	275.269532	4.551782
2.188160	266.124005	4.556787
2.228486	264.709770	4.561792
1.918866	256.485958	4.566797
1.942481	267.627574	4.571802
2.490752	272.631398	4.576806
2.545922	288.931966	4.581811
2.032277	284.783218	4.586816
2.234771	292.615459	4.591821
2.363085	284.565114	4.596826
2.474606	276.112441	4.601830
2.311021	287.856857	4.606835
2.379943	283.639894	4.611840
2.582145	277.874021	4.616845
2.423827	285.146014	4.621850
2.687049	282.973678	4.626854
2.097215	278.112794	4.631859
2.318500	284.914795	4.636864
2.503041	284.528171	4.641869
2.307397	291.238844	4.646874
2.658476	289.328367	4.651878
2.384395	292.670198	4.656883
2.608180	290.579994	4.661888
2.593436	286.768443	4.666893
2.518002	293.543398	4.671898
2.438778	284.681978	4.676902
2.329238	286.336106	4.681907
2.607514	288.155864	4.686912
2.562028	292.314543	4.691917
2.441823	294.170933	4.696922
2.345764	286.885641	4.701926
2.413014	288.712256	4.706931
2.436525	296.182346	4.711936
2.564931	287.355284	4.716941
2.351060	289.454174	4.721946
2.381654	288.745439	4.726950
2.217044	290.553956	4.731955
2.118880	291.245186	4.736960
2.575905	309.416589	4.741965
2.533953	312.048713	4.746970
2.931649	307.475376	4.751974
3.003511	315.398211	4.756979
2.619932	313.291738	4.761984
3.078548	314.056580	4.766989
3.011048	313.597000	4.771994
3.153288	295.616930	4.776998
2.467544	291.842708	4.782003
2.581521	293.708324	4.787008
2.772093	284.185793	4.792013
2.994247	312.008292	4.797018
2.800614	311.841996	4.802022
2.932233	301.337065	4.807027
2.634786	308.810977	4.812032
2.698646	302.052813	4.817037
2.416095	307.696556	4.822042
2.834104	313.827896	4.827046
2.854714	313.886667	4.832051
2.658592	323.873549	4.837056
2.928339	321.387351	4.842061
2.692764	323.502878	4.847066
3.208396	324.993702	4.852070
2.658864	317.461128	4.857075
2.624550	319.050660	4.862080
3.250720	308.139110	4.867085
2.985462	320.129356	4.872090
3.140918	311.799995	4.877094
2.968948	316.462971	4.882099
2.860588	311.541389	4.887104
3.178161	314.769493	4.892109
2.722839	317.020406	4.897114
2.996756	317.469628	4.902118
3.129080	313.556273	4.907123
2.925571	313.674593	4.912128
3.181771	322.779993	4.917133
2.989867	343.604887	4.922138
3.084250	346.122992	4.927142
3.436268	349.813058	4.932147
2.846455	352.894014	4.937152
3.120073	345.819570	4.942157
2.942619	363.897582	4.947162
3.373726	349.865829	4.952166
3.179904	359.557142	4.957171
3.129987	352.878448	4.962176
3.350313	349.648423	4.967181
3.204314	355.166479	4.972186
3.335681	349.831488	4.977190
3.725804	358.330742	4.982195
3.666857	354.165007	4.987200
3.531058	344.228611	4.992205
3.146328	331.419385	4.997210
3.303662	327.264675	5.002214
3.282189	325.991538	5.007219
3.220118	342.514507	5.012224
3.637952	348.274509	5.017229
3.150809	348.639279	5.022234
3.125754	354.389819	5.027238
3.447229	363.512218	5.032243
3.345274	356.225110	5.037248
3.470933	356.028438	5.042253
3.155957	362.616501	5.047258
3.597273	349.709824	5.052262
3.570925	362.204835	5.057267
3.235425	357.130959	5.062272
3.053062	350.417250	5.067277
3.036885	360.904285	5.072282
3.111719	359.217314	5.077286
3.168776	362.448670	5.082291
3.636233	377.582843	5.087296
3.717761	379.155890	5.092301
3.546508	378.264422	5.097306
3.633778	379.434349	5.102310
3.552998	380.268522	5.107315
3.262478	385.541644	5.112320
3.471868	373.034616	5.117325
3.583535	392.122906	5.122330
3.864497	383.495590	5.127334
3.961559	393.442075	5.132339
3.762145	388.630717	5.137344
4.005039	382.798447	5.142349
3.658342	375.223054	5.147354
3.606386	360.465080	5.152358
3.879598	370.919611	5.157363
4.154778	369.139942	5.162368
4.043174	359.239968	5.167373
3.367316	357.711909	5.172378
3.758691	354.739981	5.177382
3.841266	357.280178	5.182387
3.657807	345.206889	5.187392
3.640041	346.613508	5.192397
3.336822	364.744393	5.197402
3.364369	376.629972	5.202406
3.623219	385.868762	5.207411
3.587633	384.280259	5.212416
3.956052	385.140213	5.217421
3.852865	387.057130	5.222426
3.754190	387.244261	5.227430
3.583326	385.763491	5.232435
3.602006	397.363045	5.237440
3.900115	383.177543	5.242445
3.871617	395.100474	5.247450
3.949618	408.398888	5.252454
3.996577	411.932867	5.257459
3.915557	420.789692	5.262464
4.283446	420.219460	5.267469
3.848796	410.928247	5.272474
4.164442	421.866726	5.277478
3.877821	412.612674	5.282483
4.237042	416.560856	5.287488
4.134026	402.583890	5.292493
3.801956	400.926658	5.297498
3.876007	419.890796	5.302502
3.994919	426.727635	5.307507
4.197710	430.921651	5.312512
4.378494	430.168213	5.317517
3.839040	430.014796	5.322522
4.066720	426.173179	5.327526
4.012148	427.824106	5.332531
3.906408	430.099614	5.337536
4.342478	428.654318	5.342541
4.100454	433.518019	5.347546
4.185470	421.511146	5.352550
4.220031	425.640769	5.357555
4.202137	428.837434	5.362560
4.416193	422.345124	5.367565
4.304632	426.419312	5.372570
4.092461	423.385280	5.377574
4.094153	416.370998	5.382579
4.018066	417.751994	5.387584
3.989149	420.417688	5.392589
3.798563	425.524437	5.397594
3.661951	431.499170	5.402598
4.061722	444.845959	5.407603
4.078905	450.735147	5.412608
4.635604	450.001319	5.417613
4.500288	460.711280	5.422618
4.588904	452.183779	5.427622
4.509795	458.462725	5.432627
4.393347	454.944306	5.437632
4.341224	453.841619	5.442637
4.120631	451.442622	5.447642
4.361683	450.316465	5.452646
4.545926	448.471588	5.457651
4.588302	458.630458	5.462656
4.562433	450.614139	5.467661
4.507589	464.164181	5.472666
4.646078	457.931479	5.477670
4.744957	452.042607	5.482675
4.543040	463.467136	5.487680
4.728102	454.956953	5.492685
4.304204	462.558912	5.497690
4.161742	453.143924	5.502694
4.459646	460.012399	5.507699
4.340211	456.232810	5.512704
4.736377	450.474496	5.517709
4.438010	461.250235	5.522714
4.546329	448.079142	5.527718
4.483237	444.450032	5.532723
4.493391	464.499527	5.537728
4.906399	476.301383	5.542733
4.813333	474.050697	5.547738
4.386118	467.851631	5.552742
4.942245	476.601798	5.557747
4.670844	477.472593	5.562752
4.806014	483.927083	5.567757
4.640265	481.395237	5.572762
4.813987	486.237411	5.577766
4.686387	490.041958	5.582771
4.419527	499.668538	5.587776
5.168790	488.297925	5.592781
4.847241	494.628036	5.597786
4.802912	488.735720	5.602790
4.794170	494.657255	5.607795
4.768061	492.111868	5.612800
4.837526	489.307479	5.617805
4.842873	499.409778	5.622810
5.304588	492.618359	5.627814
4.971502	490.263707	5.632819
5.408640	484.014508	5.637824
5.049644	468.584232	5.642829
4.858371	471.220482	5.647834
4.686361	461.901174	5.652838
4.818841	475.621373	5.657843
4.834244	488.676489	5.662848
4.898511	483.537112	5.667853
4.606450	485.716316	5.672858
4.888197	480.050417	5.677862
5.062506	489.427641	5.682867
4.681369	492.228652	5.687872
5.108286	482.319605	5.692877
4.848315	488.208302	5.697882
4.886882	482.439359	5.702886
4.873750	483.206842	5.707891
4.853766	491.801763	5.712896
5.494051	493.661228	5.717901
5.144808	493.448569	5.722906
5.112624	492.129838	5.727910
5.299364	495.117863	5.732915
5.032335	487.766962	5.737920
5.266063	485.614892	5.742925
5.216404	497.690012	5.747930
4.868535	482.951504	5.752934
5.347091	506.485094	5.757939
5.395341	515.084868	5.762944
5.405301	511.816169	5.767949
4.922030	501.200181	5.772954
5.241595	515.137764	5.777958
5.623025	503.948060	5.782963
5.246399	519.378562	5.787968
5.444516	512.467750	5.792973
5.358306	507.169065	5.797978
5.449444	507.584539	5.802982
5.460788	490.731864	5.807987
5.054165	491.621583	5.812992
5.517455	492.655217	5.817997
5.630072	510.627369	5.823002
5.358668	500.011885	5.828006
5.369853	495.206733	5.833011
5.128732	496.465784	5.838016
5.688776	504.390259	5.843021
5.641455	523.453434	5.848026
5.074121	503.311838	5.853030
5.465615	508.145055	5.858035
5.475859	524.229362	5.863040
5.838351	517.802326	5.868045
5.725948	522.193007	5.873050
5.701856	503.508425	5.878054
5.896122	500.200215	5.883059
5.565479	494.140784	5.888064
5.462990	487.660014	5.893069
5.369274	495.010958	5.898074
5.316845	495.326960	5.903078
5.337547	500.672121	5.908083
5.104236	522.328603	5.913088
5.657821	513.234395	5.918093
5.492655	526.730012	5.923098
5.654617	523.544384	5.928102
5.665035	522.453003	5.933107
5.312055	524.711799	5.938112
5.242803	531.372955	5.943117
5.301257	537.274063	5.948122
5.372634	526.149098	5.953126
5.553090	532.276793	5.958131
5.929137	548.708613	5.963136
5.978162	541.454538	5.968141
5.550985	544.447325	5.973146
5.793368	543.542154	5.978150
6.045762	544.379962	5.983155
6.013815	543.340812	5.988160
5.647740	521.721442	5.993165
5.541882	538.214799	5.998170
5.506303	535.657756	6.003174
5.889833	549.367276	6.008179
5.871944	560.533169	6.013184
5.873020	564.661686	6.018189
5.582873	560.428156	6.023194
5.460390	564.775927	6.028198
5.802901	555.436165	6.033203
5.891735	561.258232	6.038208
5.776769	558.364110	6.043213
5.677135	559.364031	6.048218
5.689628	556.087008	6.053222
5.964820	560.674353	6.058227
5.756139	559.050270	6.063232
6.047727	558.261833	6.068237
5.671455	552.412233	6.073242
5.893554	563.094630	6.078246
6.045464	555.355565	6.083251
5.630410	560.721472	6.088256
5.707081	554.975769	6.093261
5.497635	561.850865	6.098266
6.014753	575.145505	6.103270
6.035771	580.969577	6.108275
5.964175	572.673671	6.113280
6.283406	559.996287	6.118285
5.901143	560.989903	6.123290
6.019726	553.009708	6.128294
5.944145	552.347617	6.133299
5.873747	558.191018	6.138304
6.136925	556.731231	6.143309
5.798065	557.697702	6.148314
5.748918	553.680259	6.153318
6.179626	546.964813	6.158323
5.773421	558.386268	6.163328
5.878622	557.600000	6.168333
5.959877	557.993042	6.173338
5.900535	563.040332	6.178342
6.502002	561.814796	6.183347
6.318130	553.234651	6.188352
6.509941	559.709754	6.193357
6.017842	554.167909	6.198362
6.049864	546.191449	6.203366
5.789796	531.164203	6.208371
5.670864	532.364862	6.213376
5.794266	537.505498	6.218381
5.741692	552.083161	6.223386
5.860204	546.762277	6.228390
6.270141	550.138473	6.233395
5.911192	563.354935	6.238400
6.218025	552.231468	6.243405
5.743913	534.436445	6.248410
5.767105	530.583797	6.253414
5.919241	521.863560	6.258419
5.608561	543.953255	6.263424
5.779411	550.596811	6.268429
5.912803	550.811479	6.273434
5.966373	559.007829	6.278438
5.978451	558.912123	6.283443
5.799144	561.923903	6.288448
6.450076	557.229272	6.293453
6.328886	543.981789	6.298458
5.611438	535.571444	6.303462
5.779939	533.646489	6.308467
5.692237	541.776128	6.313472
5.731664	530.238514	6.318477
5.863674	548.821792	6.323482
5.954695	557.073879	6.328486
6.034042	547.593748	6.333491
5.876174	555.457010	6.338496
5.932442	543.610717	6.343501
5.779440	537.079910	6.348506
5.741741	553.052236	6.353510
6.007290	548.956047	6.358515
5.753603	561.276473	6.363520
5.965759	558.942287	6.368525
5.725871	563.439220	6.373530
6.036082	565.066630	6.378534
6.113030	557.626160	6.383539
5.448098	553.889852	6.388544
5.612972	558.098098	6.393549
5.725682	557.739590	6.398554
5.635588	558.644980	6.403558
5.854017	549.996983	6.408563
5.659325	569.618502	6.413568
5.971897	562.882428	6.418573
6.330859	559.889012	6.423578
6.175461	562.095240	6.428582
6.250235	554.757747	6.433587
6.279819	565.153841	6.438592
5.994001	538.722297	6.443597
5.945710	536.917637	6.448602
5.915203	533.057733	6.453606
5.995783	526.177896	6.458611
5.700228	529.179982	6.463616
5.785536	527.261751	6.468621
5.665516	536.811259	6.473626
5.938252	541.930628	6.478630
5.924618	556.859395	6.483635
6.059718	557.040233	6.488640
5.942632	543.637752	6.493645
5.702024	542.841274	6.498650
5.597919	555.721935	6.503654
5.948086	552.650850	6.508659
6.127810	556.698956	6.513664
6.241127	552.548936	6.518669
6.068386	542.100744	6.523674
5.999911	534.819433	6.528678
5.986701	524.536548	6.533683
5.425352	531.703173	6.538688
5.983508	519.832680	6.543693
5.911351	527.703784	6.548698
5.552027	531.277296	6.553702
6.011427	529.910601	6.558707
5.516679	532.533562	6.563712
5.874760	545.552292	6.568717
5.984194	547.925058	6.573722
6.077522	562.254899	6.578726
5.974418	560.534531	6.583731
5.581715	561.073839	6.588736
5.802223	558.209799	6.593741
5.984666	560.690412	6.598746
6.053993	561.924904	6.603750
6.272674	563.427023	6.608755
5.885661	551.514292	6.613760
5.818149	536.072995	6.618765
5.653016	532.924760	6.623770
5.721966	550.367463	6.628774
6.025260	559.921614	6.633779
6.090553	567.269054	6.638784
6.238553	556.200992	6.643789
6.117599	543.552581	6.648794
5.815710	529.985071	6.653798
5.821304	528.226710	6.658803
5.551358	522.741095	6.663808
5.716341	528.380390	6.668813
5.776949	550.803252	6.673818
6.086045	559.544994	6.678822
6.262940	549.371393	6.683827
6.085662	530.799263	6.688832
5.954413	528.964584	6.693837
5.559858	536.776797	6.698842
5.658475	535.753243	6.703846
5.819585	529.072155	6.708851
5.941014	544.859761	6.713856
5.637947	551.266942	6.718861
5.975607	556.298169	6.723866
6.167697	566.498532	6.728870
5.932559	550.394800	6.733875
5.713669	547.326340	6.738880
6.124172	544.101174	6.743885
5.927619	541.013808	6.748890
5.813707	536.203387	6.753894
5.806191	541.544571	6.758899
5.926143	542.019588	6.763904
6.219181	540.629629	6.768909
5.934696	532.283880	6.773914
5.714141	534.291363	6.778918
5.762457	528.430008	6.783923
5.658812	529.124921	6.788928
5.945477	540.581571	6.793933
5.899188	548.507981	6.798938
5.616420	551.282392	6.803942
6.200133	555.255655	6.808947
5.945458	557.904233	6.813952
6.081707	546.132261	6.818957
5.946946	537.173564	6.823962
5.832679	543.113051	6.828966
5.758863	532.756169	6.833971
5.775210	538.316768	6.838976
6.023468	554.038311	6.843981
5.756365	550.947475	6.848986
5.949426	565.737702	6.853990
6.158888	551.212366	6.858995
5.722769	541.906123	6.864000
5.754285	537.567829	6.869005
6.044786	533.319890	6.874010
6.036471	542.103722	6.879014
5.818523	540.800668	6.884019
5.749829	529.702928	6.889024
6.000778	537.516585	6.894029
5.699266	534.547898	6.899034
6.010624	547.201629	6.904038
5.958866	545.543967	6.909043
5.728839	540.203857	6.914048
6.044209	538.801900	6.919053
5.942669	537.902979	6.924058
6.017924	539.728293	6.929062
5.812687	529.057786	6.934067
5.892857	538.114821	6.939072
5.698168	522.311056	6.944077
5.906857	542.780341	6.949082
5.832078	552.709314	6.954086
5.870273	553.887608	6.959091
5.998000	569.706753	6.964096
6.032477	549.394425	6.969101
5.984863	538.904915	6.974106
5.828309	535.841883	6.979110
5.954991	527.397999	6.984115
5.526693	536.237820	6.989120
5.797851	539.278324	6.994125
5.766701	555.218780	6.999130
5.815885	554.425049	7.004134
6.167393	558.896699	7.009139
6.095598	567.177038	7.014144
6.160475	547.711163	7.019149
5.866430	539.491319	7.024154
5.626029	537.424165	7.029158
6.138612	548.974500	7.034163
5.706337	551.074797	7.039168
5.739217	551.689397	7.044173
6.087336	560.339207	7.049178
5.842456	552.614589	7.054182
6.111507	541.617981	7.059187
5.701844	547.430939	7.064192
5.950016	545.412228	7.069197
6.001261	544.366749	7.074202
6.062972	535.443280	7.079206
6.032972	526.666485	7.084211
5.681828	536.671574	7.089216
5.886717	529.712071	7.094221
5.751480	535.514933	7.099226
5.788874	529.290520	7.104230
6.301103	538.186153	7.109235
6.281989	533.976256	7.114240
6.006037	534.398871	7.119245
5.677618	539.331231	7.124250
5.847663	535.066608	7.129254
5.854302	529.810303	7.134259
5.876281	525.561806	7.139264
5.685438	530.096755	7.144269
6.214767	534.463658	7.149274
5.966073	536.983563	7.154278
5.844825	530.844125	7.159283
5.862255	531.256261	7.164288
6.033945	532.476500	7.169293
6.053901	528.741608	7.174298
5.798769	525.381595	7.179302
5.968767	534.910327	7.184307
5.702996	531.077292	7.189312
5.945227	531.997301	7.194317
6.030883	530.508611	7.199322
5.857721	533.143835	7.204326
5.992093	522.301840	7.209331
5.472118	534.429110	7.214336
5.772548	526.624723	7.219341
5.804779	530.456785	7.224346
6.028345	526.470984	7.229350
6.114139	530.836421	7.234355
5.885209	541.065895	7.239360
6.030217	529.424695	7.244365
6.026303	525.159979	7.249370
5.698858	530.847969	7.254374
5.782520	527.913932	7.259379
5.645914	529.089112	7.264384
5.785060	526.329770	7.269389
5.711135	534.647150	7.274394
5.591078	531.170555	7.279398
6.031668	545.220462	7.284403
5.972644	571.165351	7.289408
5.940977	558.213189	7.294413
5.864152	549.543424	7.299418
5.765155	553.407762	7.304422
5.886301	552.711986	7.309427
5.943169	565.165505	7.314432
5.843691	557.632800	7.319437
6.245555	568.773925	7.324442
5.944471	557.178037	7.329446
6.188581	545.359327	7.334451
5.795226	539.865013	7.339456
6.037320	542.587508	7.344461
5.855411	547.945642	7.349466
5.734329	544.426985	7.354470
5.813546	530.676743	7.359475
5.693964	539.245225	7.364480
6.130574	530.926639	7.369485
5.849867	524.833046	7.374490
5.697221	526.379909	7.379494
5.656734	537.002923	7.384499
5.899557	556.171243	7.389504
6.336331	563.559947	7.394509
5.941777	548.714287	7.399514
5.707455	541.904345	7.404518
5.849799	543.235037	7.409523
5.860269	538.554312	7.414528
5.930572	541.820998	7.419533
5.844391	543.177832	7.424538
5.697127	535.613218	7.429542
6.247402	542.705594	7.434547
6.092926	540.321840	7.439552
6.061083	539.762790	7.444557
6.115981	532.225948	7.449562
5.943745	528.033806	7.454566
6.096997	528.473293	7.459571
5.292419	544.862958	7.464576
5.467009	531.159617	7.469581
5.510158	537.275602	7.474586
5.877034	552.286161	7.479590
6.059418	549.430236	7.484595
5.951717	569.354019	7.489600
5.999364	569.931237	7.494605
6.257352	565.166345	7.499610
6.067791	556.909393	7.504614
6.015109	535.591541	7.509619
5.737258	543.360482	7.514624
5.802515	533.849155	7.519629
5.771092	533.292403	7.524634
5.386859	534.400996	7.529638
6.095992	555.758011	7.534643
6.045461	566.919863	7.539648
6.117051	553.238949	7.544653
5.888043	537.739046	7.549658
5.574797	530.530586	7.554662
6.030100	542.710661	7.559667
5.940597	552.292205	7.564672
6.031328	535.137585	7.569677
6.083224	535.021054	7.574682
5.781227	541.401214	7.579686
5.960352	535.825366	7.584691
5.792348	529.688766	7.589696
5.943517	532.964703	7.594701
5.638681	533.435731	7.599706
5.375837	542.080517	7.604710
6.058245	548.726269	7.609715
6.420851	560.954523	7.614720
6.108020	545.775993	7.619725
5.850853	538.479274	7.624730
5.596108	535.809276	7.629734
5.758919	532.295533	7.634739
5.657211	543.777269	7.639744
6.040198	556.713330	7.644749
6.130159	571.678568	7.649754
5.578201	553.446536	7.654758
6.021613	565.454951	7.659763
5.977795	572.189646	7.664768
6.066045	550.178592	7.669773
5.824400	544.891521	7.674778
5.819433	542.859433	7.679782
5.967583	539.540922	7.684787
5.852682	546.760040	7.689792
6.099942	548.356865	7.694797
5.880452	546.837195	7.699802
5.934144	535.702532	7.704806
5.868420	542.123343	7.709811
5.989467	538.386842	7.714816
6.112654	536.832910	7.719821
5.973015	534.627055	7.724826
5.411391	539.656982	7.729830
5.957670	537.485123	7.734835
5.977928	539.993083	7.739840
5.888737	532.190304	7.744845
5.462937	536.608017	7.749850
6.033192	547.888480	7.754854
6.219764	554.641905	7.759859
6.059243	544.506233	7.764864
6.146618	541.052190	7.769869
6.038826	541.328652	7.774874
5.701558	536.373214	7.779878
6.108614	532.627460	7.784883
5.820855	531.155645	7.789888
5.933945	531.178721	7.794893
6.036041	523.927475	7.799898
5.949558	530.209650	7.804902
6.097018	530.810139	7.809907
5.879425	527.371069	7.814912
6.065374	528.687802	7.819917
5.809833	530.095675	7.824922
6.074887	531.536409	7.829926
5.940772	529.575319	7.834931
5.778598	533.114091	7.839936
6.312200	531.963182	7.844941
6.091634	530.157161	7.849946
5.606946	533.812093	7.854950
5.913254	531.460880	7.859955
5.726601	539.220384	7.864960
6.076961	533.943455	7.869965
6.091742	537.091495	7.874970
5.646274	533.015806	7.879974
5.896510	528.188869	7.884979
5.928229	541.092921	7.889984
5.954108	542.423434	7.894989
6.007096	533.632644	7.899994
5.902026	538.402179	7.904998
6.298350	539.748475	7.910003
5.996813	538.091284	7.915008
5.785262	533.158366	7.920013
5.957583	532.785214	7.925018
6.240408	537.934084	7.930022
5.620550	522.383323	7.935027
5.670211	526.292210	7.940032
5.605090	527.012689	7.945037
5.820722	534.727823	7.950042
5.415130	539.798713	7.955046
5.863989	535.576944	7.960051
5.879508	536.968181	7.965056
5.807386	538.722875	7.970061
5.818959	537.477972	7.975066
5.570857	536.550723	7.980070
5.589535	533.155065	7.985075
5.328823	540.164967	7.990080
5.715705	546.243360	7.995085
5.998943	548.851470	8.000090
5.913063	562.196989	8.005094
6.246849	552.675749	8.010099
6.091197	540.906911	8.015104
5.803534	536.100307	8.020109
5.707838	521.363557	8.025126
5.731909	534.561700	8.030144
5.762928	532.457959	8.035162
5.980688	564.107451	8.040179
6.070897	559.851741	8.045197
5.919390	544.345717	8.050214
5.640059	550.001110	8.055232
5.750451	559.088258	8.060250
6.061355	567.058129	8.065267
6.130309	566.997104	8.070285
6.113749	568.233638	8.075302
5.800103	567.953553	8.080320
5.923753	554.406720	8.085338
5.684556	570.548777	8.090355
6.203336	572.611015	8.095373
6.187251	574.082489	8.100390
5.936044	569.908521	8.105408
6.152234	554.603159	8.110426
5.919999	554.150305	8.115443
5.777164	544.284249	8.120461
6.385274	555.816783	8.125478
5.992581	553.719296	8.130496
6.011384	542.434969	8.135514
6.214722	542.145721	8.140531
5.906071	545.438489	8.145549
5.862914	538.593580	8.150566
5.671893	539.671529	8.155584
6.193748	547.576409	8.160602
5.749511	571.697286	8.165619
6.186742	571.593552	8.170637
6.603270	564.667897	8.175654
5.940672	553.289553	8.180672
5.885951	548.370597	8.185690
5.956389	549.561964	8.190707
6.153834	567.750344	8.195725
5.775318	557.542188	8.200742
5.760634	575.352683	8.205760
6.228807	567.835228	8.210778
6.163354	572.811833	8.215795
6.292238	582.207310	8.220813
6.350617	574.297967	8.225830
5.854541	573.837592	8.230848
6.306497	576.887029	8.235866
6.226557	571.348495	8.240883
6.088035	577.543632	8.245901
5.943180	575.193748	8.250918
5.765569	582.370689	8.255936
6.027906	569.076752	8.260954
6.226222	572.260463	8.265971
6.365411	571.134709	8.270989
6.498011	574.900748	8.276006
5.661132	573.594541	8.281024
6.079589	579.657737	8.286042
6.107343	575.180929	8.291059
5.712562	569.564028	8.296077
6.422529	575.089249	8.301094
6.402180	576.020537	8.306112
6.623231	570.855362	8.311130
6.427827	570.934330	8.316147
6.350976	582.038653	8.321165
6.277262	561.974226	8.326182
5.683211	568.642084	8.331200
6.435729	572.715678	8.336218
6.507286	570.939219	8.341235
6.272369	572.957254	8.346253
6.326272	561.007888	8.351270
6.180779	564.398924	8.356288
6.212861	546.362022	8.361306
6.214778	546.021811	8.366323
6.151551	560.355445	8.371341
6.501969	560.655868	8.376358
6.015258	551.733692	8.381376
6.270811	555.722378	8.386394
6.509309	565.182296	8.391411
6.123498	570.481806	8.396429
6.400615	566.942796	8.401446
6.270159	562.190937	8.406464
6.339491	556.464817	8.411482
6.167733	554.453826	8.416499
6.061775	560.008957	8.421517
6.138617	564.864673	8.426534
6.208283	571.682232	8.431552
6.321306	565.643954	8.436570
6.432583	565.432600	8.441587
6.430166	564.019191	8.446605
6.821356	563.336942	8.451622
6.177858	567.896677	8.456640
6.365252	570.759004	8.461658
6.579712	562.531624	8.466675
6.421411	554.135518	8.471693
6.571288	537.135250	8.476710
6.037735	539.349361	8.481728
6.044309	548.183901	8.486746
6.445436	561.090875	8.491763
6.373970	566.901471	8.496781
6.425967	559.749032	8.501798
6.422914	570.439740	8.506816
5.880191	568.405570	8.511834
6.391282	566.522004	8.516851
6.363247	567.638607	8.521869
6.338355	567.813631	8.526886
6.099154	574.731342	8.531904
5.920019	575.941361	8.536922
6.422690	572.810291	8.541939
6.310596	572.701608	8.546957
6.163384	566.601672	8.551974
6.168756	569.620422	8.556992
6.293310	581.439626	8.562010
6.514581	589.946604	8.567027
6.400988	600.066781	8.572045
6.553525	599.724367	8.577063
6.462185	604.137619	8.582080
6.253324	602.324897	8.587098
6.552452	601.719754	8.592115
6.622283	601.922535	8.597133
6.360286	601.365975	8.602151
6.537913	601.202051	8.607168
6.508448	605.442238	8.612186
6.483306	599.629649	8.617203
6.363032	606.186299	8.622221
6.488357	595.511535	8.627239
6.471201	611.019736	8.632256
6.549638	600.410827	8.637274
6.404470	605.218227	8.642291
6.026512	605.302145	8.647309
6.284916	595.741775	8.652327
6.686822	600.466316	8.657344
6.538666	599.934137	8.662362
6.559717	597.019321	8.667379
6.514591	608.117012	8.672397
6.566519	599.797543	8.677415
6.762192	602.530165	8.682432
6.655775	603.050010	8.687450
6.857209	596.735632	8.692467
6.552076	597.560331	8.697485
6.304830	591.204397	8.702503
6.585060	597.271877	8.707520
6.639538	604.185076	8.712538
6.641362	603.666745	8.717555
6.671304	615.290302	8.722573
6.819351	601.699613	8.727591
6.548115	604.319305	8.732608
6.635633	601.912883	8.737626
6.630621	601.248851	8.742643
6.834232	604.366537	8.747661
6.908337	602.231415	8.752679
6.607647	609.372531	8.757696
6.566500	608.395636	8.762714
6.708578	600.983345	8.767731
6.836236	605.554275	8.772749
7.078803	605.985606	8.777767
6.779233	602.200146	8.782784
6.458112	609.742851	8.787802
6.810106	599.699444	8.792819
6.228306	610.081881	8.797837
6.710931	600.086441	8.802855
6.779858	609.297233	8.807872
6.291708	598.416979	8.812890
6.641674	602.265980	8.817907
6.490470	605.715646	8.822925
6.707124	620.900572	8.827943
7.132734	628.541594	8.832960
6.668058	619.014785	8.837978
6.910595	600.711759	8.842995
6.566974	604.788629	8.848013
6.793428	607.670847	8.853031
6.781711	615.892576	8.858048
6.742402	624.543268	8.863066
6.895577	629.281996	8.868083
7.021051	632.386889	8.873101
6.879279	624.410008	8.878119
6.686370	612.430567	8.883136
6.722690	622.030414	8.888154
6.999120	632.583578	8.893171
7.018848	628.809011	8.898189
6.816852	608.636527	8.903207
7.094402	602.851572	8.908224
6.900849	600.760150	8.913242
6.933482	596.848615	8.918259
6.704392	604.041996	8.923277
7.185309	602.046917	8.928295
7.046283	598.184187	8.933312
6.965768	592.242431	8.938330
6.619119	591.993221	8.943347
6.244191	609.448511	8.948365
6.888795	617.253308	8.953383
7.043675	628.321117	8.958400
7.016368	635.973648	8.963418
6.716447	637.812552	8.968435
6.804347	637.055524	8.973453
6.733277	639.719899	8.978471
6.869558	633.136044	8.983488
7.077801	637.511125	8.988506
7.060887	633.236392	8.993523
6.954768	647.628018	8.998541
6.983812	639.606794	9.003559
6.889312	633.210497	9.008576
7.211577	638.929106	9.013594
6.853015	637.950640	9.018611
6.936793	643.439229	9.023629
7.003664	636.031154	9.028647
7.189014	639.764625	9.033664
6.735582	645.984573	9.038682
7.102734	633.025689	9.043699
6.829240	629.836032	9.048717
6.852079	640.127440	9.053735
6.901844	639.540712	9.058752
6.967821	641.444381	9.063770
7.153004	633.016730	9.068787
6.758401	636.674560	9.073805
7.074295	640.588284	9.078823
7.100872	640.441396	9.083840
6.694437	635.927691	9.088858
6.866458	631.210175	9.093875
6.732343	642.822834	9.098893
6.784614	640.667322	9.103911
7.286647	649.646913	9.108928
7.262459	654.483823	9.113946
7.405678	652.347442	9.118963
7.151561	651.306737	9.123981
6.819007	638.932609	9.128999
7.005430	643.267030	9.134016
7.008351	656.045600	9.139034
7.310003	662.441799	9.144051
6.894584	662.308734	9.149069
7.098431	666.979608	9.154087
7.613282	670.862830	9.159104
7.321034	674.442245	9.164122
7.418518	651.207978	9.169139
6.771110	642.590191	9.174157
6.887902	650.893917	9.179175
7.509716	664.904357	9.184192
7.370439	664.921637	9.189210
7.288036	643.380329	9.194227
6.715114	648.266713	9.199245
6.981215	666.829788	9.204263
7.479331	662.648563	9.209280
7.404433	667.612005	9.214298
7.654737	658.548964	9.219315
7.412555	648.019097	9.224333
7.083711	645.300014	9.229351
7.487625	634.253554	9.234368
7.037956	640.818120	9.239386
7.368193	639.232496	9.244403
7.382434	634.859876	9.249421
7.320291	637.048990	9.254439
7.308564	636.373869	9.259456
6.999704	641.888547	9.264474
7.643775	637.772629	9.269491
7.376390	641.239645	9.274509
7.280014	638.959246	9.279527
7.068411	640.343942	9.284544
7.087067	643.923245	9.289562
7.314873	659.082538	9.294579
7.143509	666.338985	9.299597
7.717698	661.798296	9.304615
7.333727	667.488641	9.309632
7.566155	670.869442	9.314650
7.318104	660.956435	9.319667
7.602302	657.831349	9.324685
7.148543	646.085182	9.329703
7.424141	644.849357	9.334720
7.715668	661.494389	9.339738
7.525191	637.553344	9.344755
7.513140	635.460291	9.349773
7.193373	646.359583	9.354791
7.271798	627.494483	9.359808
7.355123	645.126971	9.364826
7.485657	654.253541	9.369843
7.253278	653.378106	9.374861
7.343582	659.800378	9.379879
7.443904	659.320788	9.384896
7.566547	673.400030	9.389914
7.518592	672.552007	9.394931
7.588935	665.612790	9.399949
7.344450	667.802886	9.404967
7.424755	670.278341	9.409984
7.427102	673.741474	9.415002
7.400897	654.898652	9.420019
7.061267	670.431575	9.425037
6.960389	661.921938	9.430055
7.316027	667.365743	9.435072
7.147254	673.244320	9.440090
7.437427	667.431852	9.445107
7.497522	659.787511	9.450125
7.377665	662.845792	9.455143
7.509998	664.153249	9.460160
7.387757	676.234983	9.465178
7.856824	676.601311	9.470195
7.909590	678.788455	9.475213
7.550109	673.471923	9.480231
7.673206	662.991560	9.485248
7.623793	665.625768	9.490266
7.305161	676.715231	9.495283
7.543878	659.427842	9.500301
7.453809	667.644119	9.505319
7.929433	671.124644	9.510336
7.464173	675.846697	9.515354
7.642049	673.080196	9.520371
7.520725	664.039356	9.525389
7.583427	682.046149	9.530407
8.113554	679.973398	9.535424
7.723136	676.332732	9.540442
7.639597	673.381156	9.545459
7.415382	669.048357	9.550477
7.335268	674.275441	9.555495
7.862722	682.618007	9.560512
7.708234	701.544114	9.565530
7.780557	699.244722	9.570547
7.616751	695.049697	9.575565
7.672906	699.422123	9.580583
7.741623	693.993078	9.585600
7.664432	704.339734	9.590618
7.925474	696.832435	9.595635
7.928388	696.253689	9.600653
7.841616	699.473394	9.605671
7.705192	680.527019	9.610688
7.458934	682.220800	9.615706
7.679063	698.507494	9.620723
7.902561	698.550298	9.625741
7.463686	707.219223	9.630759
7.734695	710.391865	9.635776
7.577720	710.488655	9.640794
7.357938	698.165415	9.645811
7.872654	708.302286	9.650829
7.655004	707.071870	9.655847
7.602717	709.285927	9.660864
7.634295	705.700105	9.665882
7.543670	707.436913	9.670899
7.746605	712.854741	9.675917
7.191362	706.866461	9.680935
8.182488	715.775232	9.685952
7.751547	729.290487	9.690970
7.654511	723.552591	9.695987
8.080609	732.687360	9.701005
8.126495	730.339605	9.706023
8.084512	722.034302	9.711040
7.796462	721.480099	9.716058
7.978893	724.543854	9.721075
7.976896	722.495570	9.726093
7.503887	727.180741	9.731111
8.116096	725.191775	9.736128
7.876460	734.357478	9.741146
7.941508	725.891875	9.746163
8.156886	739.829986	9.751181
7.812255	740.659092	9.756199
7.941700	730.109722	9.761216
7.730274	733.772166	9.766234
7.934941	728.607891	9.771251
8.057303	728.472245	9.776269
7.845455	736.275370	9.781287
8.331599	719.999460	9.786304
8.119690	734.259549	9.791322
8.051237	728.502138	9.796339
8.377968	720.773296	9.801357
7.841289	731.852784	9.806375
7.860954	724.672378	9.811392
7.794413	733.523310	9.816410
7.793200	734.105785	9.821427
8.116492	725.221897	9.826445
7.668471	734.697410	9.831463
8.168036	719.092838	9.836480
8.049454	729.767231	9.841498
7.849829	730.827135	9.846515
7.859053	718.460305	9.851533
7.856525	739.176998	9.856551
8.244693	727.483141	9.861568
8.273550	731.839643	9.866586
8.176489	726.776893	9.871603
8.277915	722.077381	9.876621
7.882743	731.368335	9.881639
8.084429	735.496325	9.886656
8.015686	733.043026	9.891674
7.902989	733.528292	9.896691
8.196837	737.109118	9.901709
8.382913	734.015285	9.906727
8.389435	731.470545	9.911744
8.235105	732.332779	9.916762
7.842255	728.876349	9.921779
8.469698	730.861694	9.926797
8.053283	729.687342	9.931815
8.234870	723.527773	9.936832
8.255656	727.699607	9.941850
8.003947	735.740440	9.946867
8.274149	741.728154	9.951885
8.164600	732.351682	9.956903
8.375076	733.664855	9.961920
8.048003	727.305206	9.966938
8.095370	740.538035	9.971955
8.518526	752.221132	9.976973
8.046277	749.706953	9.981991
8.184981	755.684641	9.987008
8.299587	766.027411	9.992026
8.142448	760.006404	9.997043
8.238116	763.394996	10.002061
8.100780	761.425299	10.007079
8.260435	757.303651	10.012096
8.303476	765.950576	10.017114
8.157650	764.431468	10.022131
8.844252	765.269673	10.027149
8.533778	766.861153	10.032167
8.646311	753.927757	10.037184
8.381855	761.865219	10.042202
8.568068	770.658416	10.047219
8.622350	760.045146	10.052237
8.599997	751.281088	10.057255
8.200935	737.180868	10.062272
8.196565	736.499206	10.067290
8.243090	763.738555	10.072307
8.522436	755.873291	10.077325
8.424767	769.555020	10.082343
8.338616	768.014577	10.087360
8.711303	761.635647	10.092378
8.247760	765.980109	10.097395
8.507694	767.474421	10.102413
8.534106	770.442079	10.107431
8.486045	769.117531	10.112448
8.102074	769.075096	10.117466
8.130482	766.791259	10.122483
8.392027	760.751643	10.127501
8.393855	770.730907	10.132519
8.422910	767.784613	10.137536
8.307126	761.170951	10.142554
8.294965	765.927163	10.147571
8.506948	761.137813	10.152589
8.340910	765.735362	10.157607
8.544059	757.461142	10.162624
8.433552	760.358452	10.167642
8.412609	758.685921	10.172659
8.874433	760.482870	10.177677
8.358271	767.207545	10.182695
8.588263	765.688369	10.187712
8.482930	770.294530	10.192730
8.615724	793.184892	10.197747
8.606067	794.783262	10.202765
8.695849	790.857653	10.207783
8.786238	788.240504	10.212800
8.555128	779.711506	10.217818
8.523806	794.720709	10.222835
8.916807	782.071357	10.227853
8.513174	784.445782	10.232871
8.660306	784.339875	10.237888
8.862505	790.237540	10.242906
8.897478	786.282856	10.247923
8.715976	778.343008	10.252941
8.434672	772.021202	10.257959
8.928954	787.342613	10.262976
8.649482	772.516043	10.267994
8.916506	785.229368	10.273011
8.685123	762.790482	10.278029
8.485035	774.735440	10.283047
8.583398	789.319178	10.288064
9.002441	785.911241	10.293082
8.444776	794.727705	10.298099
8.633998	788.139315	10.303117
8.750349	795.520429	10.308135
9.014334	796.607408	10.313152
8.992199	795.469282	10.318170
8.610332	804.649809	10.323187
8.931730	791.954283	10.328205
8.881276	790.117572	10.333223
8.860246	793.352352	10.338240
8.768751	798.952207	10.343258
8.590610	800.560866	10.348275
8.657739	795.309989	10.353293
8.297749	801.584148	10.358311
8.404852	799.104563	10.363328
8.711259	791.297180	10.368346
8.712270	798.376034	10.373363
8.714106	787.655329	10.378381
8.773636	810.786617	10.383399
8.358663	822.704340	10.388416
8.791381	827.222073	10.393434
9.225644	835.767402	10.398451
9.262596	826.902703	10.403469
8.861842	834.781957	10.408487
8.855593	839.174440	10.413504
9.197578	822.659214	10.418522
9.080170	835.373488	10.423539
9.007180	818.984124	10.428557
9.087385	826.067937	10.433575
8.968063	820.675809	10.438592
9.195811	816.829421	10.443610
8.868457	809.619257	10.448627
9.141275	804.961307	10.453645
8.974707	804.312112	10.458663
8.966239	801.246073	10.463680
9.396297	812.024004	10.468698
8.967183	814.172569	10.473715
8.946271	809.590601	10.478733
9.053325	795.408963	10.483751
9.134144	800.926837	10.488768
9.111656	803.187132	10.493786
8.873829	801.333338	10.498803
8.956356	818.586462	10.503821
8.874318	827.363651	10.508839
9.140033	825.192911	10.513856
8.883166	828.314742	10.518874
8.846612	826.106256	10.523891
8.827379	830.439088	10.528909
9.129464	835.864887	10.533927
8.951613	830.349423	10.538944
9.163395	829.049788	10.543962
8.764226	829.434059	10.548979
9.034714	830.215061	10.553997
9.124669	833.667212	10.559015
8.704081	830.537392	10.564032
9.195513	847.632040	10.569050
9.106235	854.329104	10.574067
9.076541	861.778024	10.579085
9.236126	861.901919	10.584103
9.208304	863.650155	10.589120
9.575844	849.795225	10.594138
9.566269	857.636242	10.599155
9.416591	867.044533	10.604173
9.587428	851.710592	10.609191
9.450151	844.877255	10.614208
9.093689	833.070486	10.619226
9.317910	840.932474	10.624243
9.202097	837.863208	10.629261
9.293947	835.260769	10.634279
8.996347	833.577130	10.639296
9.314585	849.223313	10.644314
9.712026	861.041860	10.649331
9.582730	856.757006	10.654349
9.583479	846.408068	10.659367
9.085815	834.652520	10.664384
8.988703	826.801370	10.669402
9.233547	847.977253	10.674419
9.392513	850.312506	10.679437
9.357774	861.586395	10.684455
8.841479	870.739701	10.689472
9.636098	863.564866	10.694490
9.281161	867.908233	10.699507
9.372354	861.844336	10.704525
9.407833	865.398455	10.709543
9.202258	869.742193	10.714560
9.678317	864.932343	10.719578
9.422387	869.180126	10.724595
9.402459	869.789928	10.729613
9.647497	860.436130	10.734631
9.489351	871.853560	10.739648
9.427928	868.811072	10.744666
9.052942	875.204280	10.749683
9.128124	863.162174	10.754701
9.336120	854.230451	10.759719
9.188135	864.576776	10.764736
9.523600	880.539987	10.769754
9.437616	892.112552	10.774771
9.459704	896.539905	10.779789
9.873550	898.145450	10.784807
9.767951	888.510961	10.789824
9.619101	868.973156	10.794842
9.462755	871.616116	10.799859
9.813210	880.145480	10.804877
9.989796	868.834887	10.809895
9.646603	869.068724	10.814912
10.103615	868.294034	10.819930
9.695070	867.920667	10.824947
9.799288	865.677164	10.829965
9.764030	865.960994	10.834983
9.725338	861.581165	10.840000
9.813043	858.575305	10.845018
9.739775	860.430103	10.850035
9.586996	849.391378	10.855053
9.728338	854.558095	10.860071
9.209286	858.337637	10.865088
9.957381	852.906044	10.870106
10.023314	866.336667	10.875123
9.843573	863.047133	10.880141
9.733299	863.679627	10.885159
9.696535	863.379891	10.890176
9.769792	867.305657	10.895194
9.727528	867.382398	10.900211
9.546532	868.222696	10.905229
9.827620	867.269977	10.910247
9.307988	870.017803	10.915264
9.363354	863.173697	10.920282
9.486321	873.581679	10.925299
9.858043	889.994156	10.930317
10.050815	895.855242	10.935335
9.780033	904.461497	10.940352
10.010070	899.694299	10.945370
9.821215	900.984496	10.950387
10.256028	898.195130	10.955405
10.193431	882.291339	10.960423
9.613662	873.663557	10.965440
9.860981	866.264552	10.970458
9.748327	871.457744	10.975475
10.149534	888.395201	10.980493
9.997999	879.608451	10.985511
10.019250	877.346455	10.990528
9.972363	871.696422	10.995546
9.740314	871.590549	11.000563
9.753290	891.097082	11.005581
9.658093	889.256182	11.010599
9.843110	903.364830	11.015616
9.855543	907.461334	11.020634
9.938539	903.950773	11.025651
9.861794	908.210120	11.030669
10.220903	894.717550	11.035687
9.891189	905.720638	11.040704
9.816956	905.855052	11.045722
10.086504	899.469982	11.050739
10.145118	897.890308	11.055757
10.232467	899.244235	11.060775
10.012688	907.282211	11.065792
9.996828	904.593536	11.070810
10.091850	901.960048	11.075827
9.797415	909.801394	11.080845
10.083377	897.963778	11.085863
9.890013	907.356718	11.090880
9.927057	901.537617	11.095898
10.228000	901.693919	11.100915
10.088829	908.550864	11.105933
10.139141	900.453338	11.110951
10.181342	899.551147	11.115968
9.883993	894.620443	11.120986
9.876312	904.364579	11.126003
10.025661	923.181406	11.131021
10.637459	923.103968	11.136039
10.500519	924.032215	11.141056
10.295774	905.790968	11.146074
10.517200	906.432501	11.151091
10.216932	894.463206	11.156109
10.490505	894.712634	11.161127
10.303678	901.522776	11.166144
10.229380	899.209143	11.171162
10.288938	889.833600	11.176179
10.090484	905.984587	11.181197
10.179846	900.786077	11.186215
10.286074	901.544388	11.191232
10.257978	897.979266	11.196250
10.434887	896.046686	11.201267
10.106186	896.284216	11.206285
10.295481	890.543743	11.211303
10.263412	903.183067	11.216320
10.336227	917.009217	11.221338
10.774576	921.597100	11.226355
10.254042	914.249125	11.231373
10.331639	908.735268	11.236391
10.550650	906.033143	11.241408
10.227981	901.268642	11.246426
10.575863	911.471562	11.251443
10.382948	920.821132	11.256461
10.810529	906.712094	11.261479
10.370688	916.197183	11.266496
10.371717	901.604359	11.271514
10.504324	897.089363	11.276531
10.242680	906.810558	11.281549
10.573147	905.840772	11.286567
10.392974	923.575637	11.291584
10.549705	937.892547	11.296602
10.443318	922.767594	11.301619
10.292157	944.606829	11.306637
10.922509	934.561427	11.311655
10.748950	947.367207	11.316672
10.561121	927.365563	11.321690
10.650516	920.844887	11.326707
10.098512	927.122075	11.331725
10.827221	924.331689	11.336743
10.845134	941.450816	11.341760
10.767752	934.579730	11.346778
10.542182	907.466363	11.351795
10.178518	916.754159	11.356813
10.689611	921.570093	11.361831
10.733623	924.927545	11.366848
10.548295	935.513967	11.371866
10.560475	937.446297	11.376883
10.492551	933.433289	11.381901
10.869190	934.440732	11.386919
10.707989	942.528042	11.391936
10.578241	934.787569	11.396954
10.413278	932.978140	11.401971
10.608347	941.408176	11.406989
10.669345	935.579175	11.412007
10.354760	939.892235	11.417024
10.463149	936.103644	11.422042
10.707486	934.499003	11.427059
10.388504	938.152601	11.432077
10.404352	937.712239	11.437095
10.523848	948.923353	11.442112
10.405231	965.697901	11.447130
10.750477	963.981019	11.452147
10.451827	981.708084	11.457165
11.032020	965.541082	11.462183
11.088350	966.468309	11.467200
11.149620	963.092833	11.472218
11.056330	958.678746	11.477235
11.100130	970.633905	11.482253
11.045498	967.168053	11.487271
10.687495	970.423053	11.492288
10.845501	969.759074	11.497306
10.995590	961.673474	11.502323
11.100130	973.583897	11.507341
11.138996	963.095287	11.512359
11.033271	961.607680	11.517376
10.611768	957.947705	11.522394
10.990491	959.936431	11.527411
11.022342	970.897580	11.532429
11.091953	967.298486	11.537447
11.038106	960.734086	11.542464
11.029161	970.803650	11.547482
11.363628	970.141836	11.552499
11.059542	949.633339	11.557517
10.939056	938.999785	11.562535
11.060250	938.408850	11.567552
10.763858	938.710101	11.572570
11.182441	958.606163	11.577587
10.965466	975.126024	11.582605
11.096874	965.108023	11.587623
11.315276	975.106143	11.592640
11.114370	972.372823	11.597658
11.327875	959.553961	11.602675
11.163023	939.113668	11.607693
11.097936	937.484476	11.612711
11.184150	940.876253	11.617728
10.918720	957.286440	11.622746
11.140510	956.742167	11.627763
11.225534	968.303688	11.632781
11.181972	964.935202	11.637799
11.264121	973.213562	11.642816
10.994220	965.203868	11.647834
11.170536	964.170925	11.652851
11.060296	967.296364	11.657869
11.324673	963.019864	11.662887
11.434165	961.063641	11.667904
11.056566	964.405749	11.672922
11.401528	961.211649	11.677939
11.281900	962.646436	11.682957
11.349486	963.070251	11.687975
11.681560	959.350769	11.692992
11.402668	974.194811	11.698010
11.536190	964.475456	11.703027
11.451727	967.057669	11.708045
10.937939	948.849627	11.713063
11.140177	948.962891	11.718080
10.861948	968.532880	11.723098
11.572813	958.407354	11.728115
11.111349	966.275505	11.733133
11.172295	969.756128	11.738151
11.391996	964.419406	11.743168
11.091079	965.527065	11.748186
11.372200	972.166948	11.753203
11.093681	963.529397	11.758221
11.024517	972.533450	11.763239
11.295247	974.546624	11.768256
11.452647	984.032088	11.773274
11.543137	988.902597	11.778291
11.546672	1000.115110	11.783309
11.201663	995.138558	11.788327
11.317079	997.255497	11.793344
11.581385	999.772465	11.798362
11.852846	990.174449	11.803379
11.792314	1001.378321	11.808397
11.868911	992.605161	11.813415
11.904700	978.820215	11.818432
11.462562	975.547893	11.823450
11.895248	960.391766	11.828467
11.416599	967.558884	11.833485
11.699820	957.012736	11.838503
11.942720	957.268838	11.843520
11.680401	967.053368	11.848538
11.832249	962.034203	11.853555
11.537173	963.839467	11.858573
11.548365	961.858443	11.863591
11.402401	965.319916	11.868608
11.371470	959.046177	11.873626
11.545302	974.827505	11.878643
11.513208	984.002755	11.883661
11.507248	992.413478	11.888679
11.498408	995.320704	11.893696
11.790607	998.863679	11.898714
11.578847	985.519059	11.903731
11.819922	996.815310	11.908749
11.703530	1000.030945	11.913767
11.822831	992.761221	11.918784
11.701048	990.457632	11.923802
12.106752	990.403229	11.928819
11.887125	993.432885	11.933837
11.872471	992.417313	11.938855
11.753930	989.339219	11.943872
11.424631	999.074472	11.948890
11.928914	988.751583	11.953907
11.752445	987.822351	11.958925
11.749947	995.444362	11.963943
11.848642	999.023436	11.968960
11.737901	996.223160	11.973978
11.868988	989.239256	11.978995
11.730816	993.306487	11.984013
12.272494	993.168465	11.989031
12.004809	991.667422	11.994048
11.793645	992.696193	11.999066
11.989085	991.653181	12.004083
11.969157	997.037683	12.009101
11.736554	996.810649	12.014119
11.736936	994.339126	12.019136
11.899600	1005.079554	12.024154
12.071338	1013.530041	12.029171
11.887869	1024.480759	12.034189
11.754242	1025.163201	12.039207
12.199319	1028.474880	12.044224
11.806651	1023.771578	12.049242
12.187037	1028.975783	12.054259
12.308538	1030.466950	12.059277
12.048178	1031.236200	12.064295
12.176101	1028.727727	12.069312
12.109558	1028.666781	12.074330
12.232660	1022.958519	12.079347
12.290082	1020.957797	12.084365
12.198212	1021.394337	12.089383
12.101037	1023.821793	12.094400
12.124552	1025.132801	12.099418
12.346442	1020.618676	12.104435
12.248448	1032.880308	12.109453
12.068959	1027.614046	12.114471
12.299198	1017.134730	12.119488
11.888879	1023.897825	12.124506
12.221835	1024.890882	12.129523
12.348786	1024.491889	12.134541
12.378648	1027.008855	12.139559
12.643044	1022.069580	12.144576
12.435648	1019.935719	12.149594
12.370778	1019.567427	12.154611
12.612707	1019.705982	12.159629
12.475574	1014.877146	12.164647
12.282233	987.946458	12.169664
12.346878	994.735709	12.174682
12.371669	989.975630	12.179699
12.335583	992.786997	12.184717
11.969427	1000.432842	12.189735
12.533022	1013.560420	12.194752
12.222002	1020.741627	12.199770
12.256951	1015.869623	12.204787
12.605800	1018.566231	12.209805
12.260907	1022.959149	12.214823
12.398332	1014.648278	12.219840
12.750483	1031.122618	12.224858
12.545617	1021.653355	12.229875
12.527024	1016.739072	12.234893
12.329660	1017.229364	12.239911
12.561395	1011.166851	12.244928
12.322463	1015.754741	12.249946
12.433327	1013.628216	12.254963
12.394319	1012.909191	12.259981
12.386357	1019.578639	12.264999
12.455952	1012.821073	12.270016
12.539568	1017.604156	12.275034
12.686662	1019.470178	12.280051
12.814400	1019.789908	12.285069
12.301356	1010.949790	12.290087
12.225397	1013.697713	12.295104
12.185175	1019.591863	12.300122
12.217169	1037.657122	12.305139
12.559534	1036.492450	12.310157
12.550191	1042.389349	12.315175
12.926273	1034.381694	12.320192
12.717069	1050.582450	12.325210
12.685295	1040.813162	12.330227
13.081998	1045.167862	12.335245
12.582254	1044.823820	12.340263
13.160819	1049.595118	12.345280
12.989015	1044.142939	12.350298
12.997057	1036.431084	12.355315
12.954215	1016.056823	12.360333
12.475362	1023.845812	12.365351
12.890491	1024.473265	12.370368
12.693940	1031.052417	12.375386
12.630171	1036.338320	12.380403
12.753512	1035.042344	12.385421
12.572412	1038.263231	12.390439
13.061355	1043.549786	12.395456
13.202369	1041.896169	12.400474
13.245821	1044.511659	12.405491
13.109048	1037.226999	12.410509
12.793456	1027.780072	12.415527
12.989798	1014.550263	12.420544
12.964869	1017.644802	12.425562
13.004498	1025.414935	12.430579
13.254945	1017.104174	12.435597
12.748017	1011.092390	12.440615
12.884633	1019.285349	12.445632
12.935867	1034.617262	12.450650
12.830312	1044.330709	12.455667
13.240646	1040.765908	12.460685
12.957997	1041.245574	12.465703
13.385042	1043.873288	12.470720
13.202863	1038.542512	12.475738
13.189561	1026.565967	12.480755
13.046405	1010.491193	12.485773
12.926978	1018.940081	12.490791
13.039556	1024.086834	12.495808
12.984030	1028.022628	12.500826
13.204875	1040.371421	12.505843
13.235514	1038.527895	12.510861
13.275676	1052.175942	12.515879
12.784472	1044.619498	12.520896
13.037985	1052.669825	12.525914
13.094770	1053.226531	12.530931
13.176684	1043.719825	12.535949
13.099100	1053.385325	12.540967
12.960567	1047.493782	12.545984
13.097811	1043.595258	12.551002
13.029253	1044.359794	12.556019
13.271224	1041.888658	12.561037
13.080940	1051.067013	12.566055
13.156433	1043.967922	12.571072
13.436486	1047.775116	12.576090
13.254469	1043.789900	12.581107
13.295164	1048.673035	12.586125
12.884277	1051.517969	12.591143
13.242857	1062.708522	12.596160
13.174788	1073.236574	12.601178
13.229812	1077.734682	12.606195
13.848091	1077.720534	12.611213
13.533288	1079.172024	12.616231
13.532050	1073.426934	12.621248
13.692022	1060.556260	12.626266
13.173795	1044.923294	12.631283
13.709409	1056.208427	12.636301
13.609540	1056.351040	12.641319
13.623351	1048.810651	12.646336
13.621423	1051.748626	12.651354
13.225746	1047.144630	12.656371
13.443791	1047.821375	12.661389
13.483140	1062.065200	12.666407
13.686848	1076.826570	12.671424
13.528584	1060.405850	12.676442
13.422089	1079.499628	12.681459
13.620031	1079.442751	12.686477
13.465354	1080.505838	12.691495
13.715527	1080.886710	12.696512
13.611338	1078.024311	12.701530
13.335754	1084.349707	12.706547
13.947166	1080.418425	12.711565
13.623811	1084.005071	12.716583
13.550405	1083.520093	12.721600
13.456356	1084.392798	12.726618
13.187468	1080.890882	12.731635
13.478364	1069.225140	12.736653
13.482936	1089.369699	12.741671
13.788589	1075.397302	12.746688
13.845923	1069.712159	12.751706
13.546413	1076.956829	12.756723
13.445071	1072.964102	12.761741
13.430245	1078.256845	12.766759
13.791528	1091.083488	12.771776
14.173983	1094.433148	12.776794
14.065523	1097.723072	12.781811
14.121532	1079.085348	12.786829
14.075420	1079.578453	12.791847
13.947108	1071.250305	12.796864
14.138817	1077.455908	12.801882
13.875752	1074.997846	12.806899
14.088306	1069.036132	12.811917
13.491693	1072.859914	12.816935
13.750834	1070.474498	12.821952
13.831810	1070.028424	12.826970
13.342122	1077.996789	12.831987
13.904973	1084.939088	12.837005
14.123260	1104.667458	12.842023
14.248937	1103.971055	12.847040
14.394798	1100.704907	12.852058
13.780081	1096.625856	12.857075
14.318422	1093.597215	12.862093
13.919318	1094.819032	12.867111
14.322207	1091.398361	12.872128
14.041531	1081.883003	12.877146
13.852265	1081.241702	12.882163
14.237921	1075.920860	12.887181
13.769024	1081.350880	12.892199
13.988990	1093.761669	12.897216
14.129389	1101.317072	12.902234
14.052229	1102.381448	12.907251
14.285519	1102.880475	12.912269
14.078085	1100.481269	12.917287
14.559101	1104.097998	12.922304
14.557378	1093.038716	12.927322
14.425367	1104.320682	12.932339
14.662686	1088.210934	12.937357
14.285266	1091.589258	12.942375
14.057959	1068.692978	12.947392
14.307405	1073.677637	12.952410
14.143360	1067.288388	12.957427
14.296748	1072.034303	12.962445
14.046703	1081.041123	12.967463
13.883658	1085.869555	12.972480
13.963334	1101.080278	12.977498
14.239335	1100.206929	12.982515
14.442245	1096.443927	12.987533
14.349897	1103.650241	12.992551
14.296522	1100.189661	12.997568
14.391399	1098.734247	13.002586
14.063237	1098.780560	13.007603
14.340450	1092.251429	13.012621
14.451331	1102.197427	13.017639
14.707551	1101.057697	13.022656
14.412251	1097.465684	13.027674
14.385189	1107.928679	13.032691
14.555567	1102.210563	13.037709
14.471919	1103.237437	13.042727
14.459062	1101.727492	13.047744
14.505876	1097.020804	13.052762
14.324279	1113.087910	13.057779
14.830651	1121.258441	13.062797
14.494435	1129.049757	13.067815
14.362433	1134.587179	13.072832
14.876860	1136.918905	13.077850
14.643310	1144.487271	13.082867
14.710491	1136.615152	13.087885
14.824707	1145.010315	13.092903
14.913333	1136.474825	13.097920
15.043613	1116.073627	13.102938
14.603611	1114.326818	13.107955
14.544059	1104.627064	13.112973
14.341748	1104.333973	13.117991
14.635412	1127.944901	13.123008
15.041179	1129.715978	13.128026
14.658980	1140.015592	13.133043
14.816759	1137.791100	13.138061
14.767480	1131.306769	13.143079
14.817629	1142.554549	13.148096
14.576179	1141.721536	13.153114
14.823882	1134.069794	13.158131
15.014411	1142.065679	13.163149
15.107585	1144.464666	13.168167
14.803728	1147.151677	13.173184
15.061410	1131.382970	13.178202
14.901520	1133.976764	13.183219
15.030774	1133.910438	13.188237
15.066543	1137.344499	13.193255
14.836837	1133.358525	13.198272
14.978111	1134.815709	13.203290
15.035043	1136.742792	13.208307
15.259641	1131.632155	13.213325
14.983075	1127.345720	13.218343
14.898827	1132.466171	13.223360
15.111995	1126.848409	13.228378
14.909298	1137.006776	13.233395
15.410830	1130.550182	13.238413
14.840925	1128.276174	13.243431
14.570152	1133.674070	13.248448
14.989431	1135.342907	13.253466
14.829738	1138.274445	13.258483
14.984288	1132.666817	13.263501
15.129745	1133.514283	13.268519
15.116580	1138.518991	13.273536
15.611954	1128.341971	13.278554
14.914294	1140.750204	13.283571
15.054066	1126.020336	13.288589
15.030702	1130.880287	13.293607
14.888800	1138.368067	13.298624
14.997919	1137.296482	13.303642
15.024367	1141.485595	13.308659
15.283796	1158.084532	13.313677
15.438751	1163.322314	13.318695
15.339111	1161.205954	13.323712
15.750412	1168.598653	13.328730
15.278747	1157.846161	13.333747
15.153338	1142.252527	13.338765
15.282151	1143.491715	13.343783
15.042796	1157.307960	13.348800
15.377131	1151.130708	13.353818
15.225623	1162.666730	13.358835
15.104206	1160.123303	13.363853
15.623351	1162.949499	13.368871
15.243723	1160.440722	13.373888
15.428129	1159.569996	13.378906
15.106389	1158.477506	13.383923
15.300691	1162.984378	13.388941
15.623381	1156.625211	13.393959
15.543663	1163.792842	13.398976
15.710415	1158.796136	13.403994
15.572142	1165.238893	13.409011
15.691886	1162.077068	13.414029
15.737022	1158.322164	13.419047
15.358779	1165.808296	13.424064
15.284126	1159.572252	13.429082
15.558496	1172.314989	13.434099
15.303756	1167.742647	13.439117
15.812608	1184.574157	13.444135
15.770558	1188.780180	13.449152
15.699148	1185.588313	13.454170
15.772014	1197.430751	13.459187
15.808253	1198.880990	13.464205
16.085272	1196.152050	13.469223
15.312908	1181.370593	13.474240
15.807791	1171.303071	13.479258
15.924161	1187.258528	13.484275
15.848149	1185.627976	13.489293
16.013089	1177.965560	13.494311
15.638289	1170.685361	13.499328
15.592940	1178.936206	13.504346
15.854255	1186.630600	13.509363
15.904108	1189.097814	13.514381
15.991957	1186.516059	13.519399
15.886982	1188.024805	13.524416
16.163130	1188.843467	13.529434
15.992996	1190.085498	13.534451
16.289019	1188.165564	13.539469
16.009394	1168.458378	13.544487
15.988358	1161.833127	13.549504
15.954947	1149.767314	13.554522
16.251305	1155.932722	13.559539
16.240640	1155.875480	13.564557
16.328193	1142.600655	13.569575
15.723465	1156.479594	13.574592
16.137588	1154.506178	13.579610
16.217615	1161.228382	13.584627
16.290447	1150.841670	13.589645
16.233815	1152.633701	13.594663
15.969971	1158.670971	13.599680
15.831906	1149.838524	13.604698
15.925223	1159.024527	13.609715
15.831079	1159.083910	13.614733
16.056390	1170.084892	13.619751
16.167024	1185.817690	13.624768
16.191423	1188.655258	13.629786
16.270145	1179.530082	13.634803
16.346397	1191.336522	13.639821
16.605314	1188.978290	13.644839
16.502858	1190.490161	13.649856
16.194541	1191.655558	13.654874
16.212514	1190.224728	13.659891
16.072139	1189.347748	13.664909
15.898350	1197.084545	13.669927
16.361425	1193.196786	13.674944
16.316530	1188.026596	13.679962
16.619910	1193.420419	13.684979
16.168075	1191.770839	13.689997
16.111002	1197.730452	13.695015
15.972415	1182.368090	13.700032
16.030486	1188.936877	13.705050
16.590745	1194.088803	13.710067
16.286665	1211.433784	13.715085
16.550212	1209.700732	13.720103
16.396338	1216.863784	13.725120
16.702393	1216.296049	13.730138
16.731683	1205.037842	13.735155
16.602880	1215.913076	13.740173
16.656236	1207.023978	13.745191
16.823736	1206.307628	13.750208
16.352191	1200.142258	13.755226
16.504080	1195.703100	13.760243
16.505235	1206.384295	13.765261
16.866835	1207.282058	13.770279
16.519738	1216.912537	13.775296
16.651360	1208.803698	13.780314
16.930423	1214.437778	13.785331
16.858552	1212.580562	13.790349
17.093614	1204.032900	13.795367
16.693356	1214.951283	13.800384
16.775158	1216.439224	13.805402
16.738149	1216.826102	13.810419
16.868372	1208.610414	13.815437
16.984269	1214.141305	13.820455
16.872472	1208.799167	13.825472
16.833102	1207.989253	13.830490
17.117249	1201.464435	13.835507
16.878340	1202.505704	13.840525
16.680027	1192.967927	13.845543
16.785272	1195.858591	13.850560
17.159620	1202.270491	13.855578
17.013571	1204.578152	13.860595
16.695291	1215.108912	13.865613
17.098638	1211.640505	13.870631
16.763330	1207.544510	13.875648
17.122511	1209.244604	13.880666
16.916171	1208.365989	13.885683
16.595484	1212.358106	13.890701
17.176119	1210.194418	13.895719
17.305617	1212.626352	13.900736
17.148760	1199.479498	13.905754
16.939441	1196.748717	13.910771
16.949489	1206.370221	13.915789
16.896669	1194.427278	13.920807
16.890562	1206.562756	13.925824
16.740826	1201.407626	13.930842
17.066871	1198.882337	13.935859
16.929943	1203.286013	13.940877
17.003220	1204.639156	13.945895
16.906575	1235.543893	13.950912
17.007419	1242.237870	13.955930
17.280591	1235.792024	13.960947
17.263239	1245.865722	13.965965
17.361634	1239.719383	13.970983
17.314026	1244.070826	13.976000
17.326906	1240.170483	13.981018
17.063683	1243.354670	13.986035
16.890758	1249.779600	13.991053
17.559377	1241.314576	13.996071
17.194046	1251.831529	14.001088
17.094401	1247.492034	14.006106
17.047095	1252.658744	14.011123
17.062797	1262.943485	14.016141
17.389837	1262.095108	14.021159
17.399643	1270.173063	14.026176
17.649228	1258.084538	14.031194
17.972515	1263.559719	14.036211
17.910349	1263.866925	14.041229
17.897241	1248.731268	14.046247
17.795577	1238.537665	14.051264
17.787294	1232.961395	14.056282
17.700139	1228.477711	14.061299
17.774880	1234.297719	14.066317
17.741554	1235.472136	14.071335
17.897647	1242.490379	14.076352
18.011216	1226.085718	14.081370
17.941043	1227.702064	14.086387
17.687518	1241.975441	14.091405
17.976342	1231.867722	14.096423
17.644288	1233.025257	14.101440
17.814136	1229.070089	14.106458
17.838542	1225.530809	14.111475
17.522740	1227.847002	14.116493
17.963864	1232.715608	14.121511
18.062446	1230.743449	14.126528
18.034886	1226.363241	14.131546
18.086293	1232.525693	14.136563
17.916231	1235.883756	14.141581
17.975611	1237.603367	14.146599
17.788670	1234.705482	14.151616
17.828712	1229.757765	14.156634
18.172996	1225.701562	14.161651
17.928056	1234.922965	14.166669
18.015696	1229.476809	14.171687
17.873142	1230.944170	14.176704
18.014745	1227.768463	14.181722
18.206614	1228.008644	14.186739
18.222872	1231.085750	14.191757
18.285982	1227.155410	14.196775
18.409642	1236.523021	14.201792
18.135474	1237.190643	14.206810
17.919930	1227.656102	14.211827
17.760895	1239.134773	14.216845
17.993767	1231.680715	14.221863
17.973019	1231.303117	14.226880
17.855413	1235.714614	14.231898
18.204026	1226.691002	14.236915
18.040311	1228.708704	14.241933
18.074164	1230.910487	14.246951
17.958637	1230.580923	14.251968
17.886987	1232.525452	14.256986
18.025257	1235.671252	14.262003
18.139074	1262.181430	14.267021
18.157269	1257.549918	14.272039
18.249801	1263.789009	14.277056
18.030165	1260.135171	14.282074
18.285940	1251.084064	14.287091
18.153265	1260.182891	14.292109
18.140052	1253.801172	14.297127
18.315491	1257.290782	14.302144
18.256173	1273.972347	14.307162
18.338229	1267.436604	14.312179
18.477654	1265.332855	14.317197
18.340748	1273.204498	14.322215
18.593319	1286.197004	14.327232
18.361726	1298.431839	14.332250
18.675710	1289.993842	14.337267
18.594700	1290.521887	14.342285
18.808851	1300.929568	14.347303
18.784241	1292.715949	14.352320
18.630630	1280.697964	14.357338
18.846439	1270.768096	14.362355
18.392778	1266.463420	14.367373
18.487840	1280.647401	14.372391
18.455704	1280.016981	14.377408
18.327885	1292.264484	14.382426
18.333120	1280.529532	14.387443
18.469546	1282.969381	14.392461
18.439156	1282.559134	14.397479
18.343888	1278.590146	14.402496
18.765751	1293.546556	14.407514
18.930752	1310.942419	14.412531
18.920813	1317.106046	14.417549
19.068941	1309.456202	14.422567
18.872263	1296.164316	14.427584
18.643011	1297.529169	14.432602
19.196626	1305.759661	14.437619
19.144464	1299.820990	14.442637
18.663661	1291.440685	14.447655
19.380810	1300.810477	14.452672
19.064435	1297.623870	14.457690
18.943069	1293.089556	14.462707
18.747742	1288.890356	14.467725
19.156118	1296.272974	14.472743
19.371178	1299.893011	14.477760
18.955253	1311.304200	14.482778
19.015066	1300.273518	14.487795
19.107078	1302.844369	14.492813
18.845312	1320.688322	14.497831
19.235493	1315.848910	14.502848
19.213009	1323.195677	14.507866
19.395391	1316.167669	14.512883
19.171661	1324.125418	14.517901
19.261460	1321.774802	14.522919
19.638157	1323.999141	14.527936
19.043503	1319.412779	14.532954
19.235261	1292.129774	14.537971
19.042523	1307.562347	14.542989
19.102306	1314.402544	14.548007
19.258978	1309.722805	14.553024
19.098040	1312.943153	14.558042
19.575562	1317.419533	14.563059
19.353301	1320.287098	14.568077
19.205843	1322.181642	14.573095
19.440929	1316.468440	14.578112
19.004738	1322.933219	14.583130
19.442626	1320.296807	14.588147
19.249418	1322.118643	14.593165
19.007436	1320.806988	14.598183
19.383550	1319.457560	14.603200
19.285150	1337.422405	14.608218
19.679529	1344.049530	14.613235
19.817424	1351.905459	14.618253
19.722186	1340.568248	14.623271
19.841106	1337.066381	14.628288
19.470710	1327.876006	14.633306
19.976150	1319.974652	14.638323
19.516752	1316.401200	14.643341
19.587884	1312.729730	14.648359
19.713962	1320.982472	14.653376
19.629483	1341.727567	14.658394
20.025720	1348.725236	14.663411
19.941640	1335.124850	14.668429
19.639146	1328.729764	14.673447
19.836127	1315.180710	14.678464
19.988486	1330.724839	14.683482
20.004195	1326.675192	14.688499
19.824227	1325.304018	14.693517
19.581060	1316.875148	14.698535
19.895895	1331.024615	14.703552
19.739076	1340.416860	14.708570
19.915474	1349.777743	14.713587
20.295675	1338.418992	14.718605
20.012920	1350.818664	14.723623
20.117527	1349.905682	14.728640
20.092082	1354.734555	14.733658
20.174792	1332.247757	14.738675
20.306908	1325.305655	14.743693
19.909708	1324.893776	14.748711
19.911357	1324.960072	14.753728
19.717366	1344.836402	14.758746
20.056165	1351.643627	14.763763
19.759283	1355.844413	14.768781
19.908254	1356.786187	14.773799
20.213980	1345.586259	14.778816
20.093268	1353.109595	14.783834
20.061465	1341.153204	14.788851
20.176677	1352.500948	14.793869
20.086820	1351.153770	14.798887
20.216143	1347.487186	14.803904
19.788846	1347.477537	14.808922
20.094429	1353.045452	14.813939
20.146224	1378.992539	14.818957
20.046803	1385.451764	14.823975
20.451585	1375.365622	14.828992
20.347116	1377.058941	14.834010
20.393357	1387.547342	14.839027
20.805598	1378.256779	14.844045
20.446919	1383.141833	14.849063
20.745148	1374.706409	14.854080
20.543101	1385.460476	14.859098
20.650883	1380.373504	14.864115
20.874293	1378.986068	14.869133
20.599038	1381.293183	14.874151
20.699492	1372.984328	14.879168
20.625974	1378.076700	14.884186
20.901966	1366.729342	14.889203
20.758442	1346.107612	14.894221
20.574275	1345.686308	14.899239
20.460133	1333.069620	14.904256
20.468988	1352.457148	14.909274
20.766070	1360.720464	14.914291
20.706893	1360.318148	14.919309
20.760387	1374.459126	14.924327
20.893541	1367.217632	14.929344
20.665406	1375.482033	14.934362
20.806875	1362.643710	14.939379
20.996723	1366.269921	14.944397
20.670780	1371.846747	14.949415
21.173541	1368.329894	14.954432
21.036346	1368.994834	14.959450
20.944098	1367.768913	14.964467
20.937578	1357.292501	14.969485
20.960570	1372.767232	14.974503
21.177617	1365.422823	14.979520
20.977599	1370.555114	14.984538
21.023778	1369.359727	14.989555
21.238337	1369.923686	14.994573
21.177158	1365.550994	14.999591
21.104595	1369.513328	15.004608
21.178335	1367.940147	15.009626
21.047259	1370.475256	15.014643
21.117668	1365.354738	15.019661
20.937290	1371.606949	15.024679
21.398021	1372.565015	15.029696
21.223441	1370.030783	15.034714
20.999235	1373.295909	15.039731
21.385784	1370.149144	15.044749
21.145225	1370.816304	15.049767
21.302093	1371.253242	15.054784
21.101898	1367.104828	15.059802
20.946307	1375.908331	15.064819
21.189711	1370.008695	15.069837
21.046081	1371.830564	15.074855
21.147691	1363.043983	15.079872
21.127456	1369.211311	15.084890
20.972522	1359.829993	15.089907
21.531121	1380.255668	15.094925
21.505800	1397.628932	15.099943
21.632083	1394.114805	15.104960
21.395514	1398.283926	15.109978
21.770145	1402.373510	15.114995
22.139971	1386.686295	15.120013
21.517714	1380.619127	15.125031
21.290703	1369.989202	15.130048
21.462299	1381.534674	15.135066
21.315804	1387.060815	15.140083
21.255970	1401.976136	15.145101
21.339651	1399.983205	15.150119
21.654597	1393.278786	15.155136
21.970505	1399.124519	15.160154
21.634694	1397.686331	15.165171
21.810396	1391.552279	15.170189
21.768289	1399.980255	15.175207
21.600026	1393.605745	15.180224
21.773900	1399.790033	15.185242
21.823785	1397.755084	15.190259
22.027590	1396.469326	15.195277
21.627573	1401.593137	15.200295
21.801101	1388.249090	15.205312
21.967923	1393.977874	15.210330
21.812819	1395.356788	15.215347
21.878342	1391.591746	15.220365
21.767334	1404.783358	15.225383
21.981900	1413.614334	15.230400
22.384302	1423.056198	15.235418
22.267939	1419.214297	15.240435
22.247774	1408.403122	15.245453
21.886887	1404.851070	15.250471
21.928036	1399.499980	15.255488
22.208323	1403.611150	15.260506
21.996394	1400.049694	15.265523
22.233967	1410.310649	15.270541
22.528837	1410.471905	15.275559
22.365250	1409.424368	15.280576
21.830885	1413.427247	15.285594
22.078953	1416.061153	15.290611
22.365246	1412.346418	15.295629
22.664036	1423.120809	15.300647
22.416659	1410.560453	15.305664
22.311760	1405.900933	15.310682
22.399329	1427.621448	15.315699
22.550865	1414.812510	15.320717
22.319953	1415.183984	15.325735
22.535725	1414.230476	15.330752
22.434883	1406.925496	15.335770
22.316258	1419.243222	15.340787
22.754166	1412.769136	15.345805
22.246661	1428.278159	15.350823
22.855329	1418.367938	15.355840
22.659819	1413.802606	15.360858
22.444961	1421.044390	15.365875
22.594042	1411.637708	15.370893
22.596668	1420.089755	15.375911
22.568637	1418.968114	15.380928
22.602436	1416.159879	15.385946
22.541321	1418.055438	15.390963
22.866790	1416.738435	15.395981
22.769541	1424.997643	15.400999
22.900349	1417.492745	15.406016
23.036309	1414.278569	15.411034
22.704358	1414.628255	15.416051
22.729025	1413.877369	15.421069
22.530957	1416.688964	15.426087
22.448009	1417.605510	15.431104
22.660267	1422.295294	15.436122
22.787109	1413.795424	15.441139
23.250839	1405.443103	15.446157
23.075111	1412.603972	15.451175
22.945210	1415.585727	15.456192
23.278855	1406.975508	15.461210
23.055609	1413.238403	15.466227
23.210848	1406.914840	15.471245
23.084462	1418.895285	15.476263
23.307104	1413.582133	15.481280
23.355807	1406.653465	15.486298
23.134350	1411.478714	15.491315
23.444992	1401.115300	15.496333
23.066545	1407.612248	15.501351
23.141426	1396.034525	15.506368
23.258059	1403.004284	15.511386
23.253773	1402.512532	15.516403
23.233998	1407.981006	15.521421
23.270848	1399.913014	15.526439
23.382836	1406.599699	15.531456
23.205693	1400.306580	15.536474
23.212007	1408.583605	15.541491
23.267151	1398.898854	15.546509
23.383670	1406.678445	15.551527
23.310116	1397.817024	15.556544
23.228077	1398.946008	15.561562
23.067540	1410.784885	15.566579
23.424193	1423.338176	15.571597
23.563656	1429.459694	15.576615
23.590400	1429.381667	15.581632
23.834575	1431.234360	15.586650
23.592797	1433.742210	15.591667
23.869164	1432.019602	15.596685
23.571531	1431.301417	15.601703
23.626400	1430.946677	15.606720
23.973456	1429.074924	15.611738
23.541177	1431.504990	15.616755
23.690156	1427.346949	15.621773
23.753511	1430.369419	15.626791
23.753345	1431.911948	15.631808
23.956455	1434.548211	15.636826
23.591914	1425.385150	15.641843
23.720169	1429.388529	15.646861
23.724640	1437.274944	15.651879
23.501297	1436.361348	15.656896
23.888554	1432.468416	15.661914
23.557156	1438.026488	15.666931
23.811143	1437.107176	15.671949
23.980275	1426.925133	15.676967
23.481825	1441.440968	15.681984
23.723884	1439.494934	15.687002
23.716106	1453.526093	15.692019
24.222632	1453.549026	15.697037
24.044713	1458.934751	15.702055
23.850414	1458.898579	15.707072
23.850766	1459.974506	15.712090
23.809160	1459.048418	15.717107
23.763344	1453.360201	15.722125
24.574907	1462.957306	15.727143
24.286094	1458.740134	15.732160
24.368492	1450.736591	15.737178
24.764293	1461.912982	15.742195
24.674168	1456.193152	15.747213
24.778112	1450.876882	15.752231
24.560082	1458.146374	15.757248
24.811302	1447.099128	15.762266
24.743018	1460.491159	15.767283
24.646793	1443.324707	15.772301
24.777151	1429.818908	15.777319
24.531050	1424.550983	15.782336
24.852775	1419.044202	15.787354
24.142289	1423.450751	15.792371
24.531737	1417.195340	15.797389
24.270612	1415.591987	15.802407
24.344796	1435.312055	15.807424
24.751957	1433.096465	15.812442
24.739741	1451.941969	15.817459
25.063918	1448.131169	15.822477
24.850274	1446.209302	15.827495
24.679149	1432.704396	15.832512
24.837589	1420.262010	15.837530
24.455718	1429.076381	15.842547
24.559011	1435.569649	15.847565
24.396796	1441.034251	15.852583
24.613600	1457.938615	15.857600
24.763506	1443.146135	15.862618
24.495119	1451.909768	15.867635
24.918215	1441.148123	15.872653
24.831266	1445.576630	15.877671
24.891739	1442.461606	15.882688
24.954103	1434.571634	15.887706
24.523383	1442.276848	15.892723
24.870034	1445.796311	15.897741
25.151936	1453.835043	15.902759
24.681182	1482.088369	15.907776
25.260346	1473.602262	15.912794
25.037866	1488.887601	15.917811
25.241092	1479.572270	15.922829
25.239612	1481.832322	15.927847
25.098409	1478.378381	15.932864
25.391150	1473.497244	15.937882
25.395114	1477.375629	15.942899
25.613829	1478.973120	15.947917
25.470844	1474.399827	15.952935
25.059971	1459.351727	15.957952
25.694043	1459.351493	15.962970
25.227258	1462.488851	15.967987
25.208845	1458.572001	15.973005
25.333608	1457.682828	15.978023
25.134865	1467.242742	15.983040
25.354884	1467.500295	15.988058
24.954815	1483.195447	15.993075
25.063396	1474.036790	15.998093
25.683415	1473.045224	16.003111
25.288304	1474.223885	16.008128
25.336208	1470.416872	16.013146
25.399806	1473.390493	16.018163
25.627102	1487.133014	16.023181
25.419107	1493.520961	16.028199
25.113869	1508.141355	16.033216
25.584429	1498.363090	16.038234
25.978517	1498.450772	16.043251
25.966681	1501.123166	16.048269
26.162863	1488.794527	16.053287
25.915673	1493.767381	16.058304
26.332702	1491.248577	16.063322
26.187191	1490.820844	16.068339
26.172920	1482.538479	16.073357
26.043922	1480.646238	16.078375
25.676646	1469.571462	16.083392
26.067641	1465.433421	16.088410
25.748312	1466.386501	16.093427
25.947806	1483.099289	16.098445
26.121456	1482.946059	16.103463
25.851174	1493.940668	16.108480
25.980410	1483.409718	16.113498
25.965763	1489.067127	16.118515
25.898707	1491.048718	16.123533
26.262219	1475.073497	16.128551
25.852388	1488.367599	16.133568
26.513451	1484.082702	16.138586
26.051688	1495.524478	16.143603
26.058019	1485.311976	16.148621
26.629266	1487.555578	16.153639
26.645004	1495.561013	16.158656
26.534985	1491.014912	16.163674
26.544091	1490.603606	16.168691
26.488586	1485.588619	16.173709
26.663887	1482.934801	16.178727
26.415270	1484.021795	16.183744
26.729118	1480.586707	16.188762
26.581524	1480.130582	16.193779
26.501702	1481.719425	16.198797
26.623858	1477.459533	16.203815
26.390722	1476.417644	16.208832
26.478600	1478.255771	16.213850
26.693004	1485.113651	16.218867
26.803482	1488.679463	16.223885
26.789189	1473.109152	16.228903
26.480698	1490.107156	16.233920
26.450570	1479.429867	16.238938
26.495016	1478.634353	16.243955
26.462082	1489.080079	16.248973
27.022632	1478.246352	16.253991
26.738395	1489.055488	16.259008
26.722619	1490.056146	16.264026
26.608293	1485.350138	16.269043
26.190284	1486.841258	16.274061
26.890969	1495.739513	16.279079
26.945732	1514.328693	16.284096
27.336019	1512.542262	16.289114
27.032376	1511.688462	16.294131
27.309208	1514.363666	16.299149
27.585064	1519.472817	16.304167
27.040455	1510.003422	16.309184
27.015103	1492.407039	16.314202
26.986371	1495.848750	16.319219
27.091024	1500.920211	16.324237
27.358333	1511.339671	16.329255
26.878537	1514.129212	16.334272
26.924508	1514.843240	16.339290
27.621757	1519.404023	16.344307
27.282506	1511.701230	16.349325
27.173351	1510.938723	16.354343
27.289156	1521.713676	16.359360
27.238443	1515.486108	16.364378
27.153023	1510.911505	16.369395
26.797182	1512.430482	16.374413
27.330442	1503.156737	16.379431
26.930122	1512.859628	16.384448
27.532111	1528.054825	16.389466
27.511039	1532.942473	16.394483
27.585775	1537.822073	16.399501
28.002381	1534.360053	16.404519
27.788089	1531.821765	16.409536
27.734974	1536.554115	16.414554
27.774051	1542.939207	16.419571
27.373293	1545.026266	16.424589
27.618435	1534.598061	16.429607
27.691751	1535.582340	16.434624
27.786333	1541.905846	16.439642
27.848342	1534.556417	16.444659
27.805105	1543.422048	16.449677
27.985610	1529.383039	16.454695
28.162244	1546.676843	16.459712
27.779513	1537.047066	16.464730
27.727226	1542.115885	16.469747
27.961306	1533.487893	16.474765
28.174206	1533.395067	16.479783
27.956517	1526.772817	16.484800
27.716047	1536.203099	16.489818
27.857833	1524.803918	16.494835
27.640264	1541.874661	16.499853
28.024301	1544.147811	16.504871
27.930628	1560.991295	16.509888
28.018508	1561.236562	16.514906
28.318891	1563.564562	16.519923
28.378104	1563.634283	16.524941
28.725230	1558.488576	16.529959
28.585296	1566.796685	16.534976
28.368904	1551.203193	16.539994
28.372311	1550.516069	16.545011
28.445963	1553.855346	16.550029
28.468772	1554.329531	16.555047
28.423404	1555.282358	16.560064
28.621525	1556.255344	16.565082
28.504272	1531.470847	16.570099
28.418907	1539.227762	16.575117
28.797630	1540.961259	16.580135
28.583058	1539.480860	16.585152
28.666012	1536.366805	16.590170
28.869563	1522.427906	16.595187
28.346432	1532.298066	16.600205
28.437021	1540.854059	16.605223
28.653385	1547.928565	16.610240
28.682546	1554.695220	16.615258
28.963729	1559.057851	16.620275
28.593893	1557.581602	16.625293
28.738608	1550.341645	16.630311
28.715262	1556.444212	16.635328
28.781581	1561.345296	16.640346
29.058254	1553.442085	16.645363
28.850552	1558.425325	16.650381
28.962332	1552.064439	16.655399
28.903774	1555.811113	16.660416
29.101553	1563.987503	16.665434
28.928068	1556.917748	16.670451
28.487126	1563.540892	16.675469
28.714344	1557.990716	16.680487
29.119972	1558.751267	16.685504
29.072608	1569.093148	16.690522
29.008272	1573.319907	16.695539
28.979487	1577.159667	16.700557
28.984277	1580.422995	16.705575
28.946257	1586.477227	16.710592
29.224012	1584.256746	16.715610
29.398412	1583.610097	16.720627
29.243005	1584.482004	16.725645
29.264583	1581.092321	16.730663
29.357682	1572.793637	16.735680
29.195265	1583.651094	16.740698
29.464449	1583.276085	16.745715
29.252790	1610.807072	16.750733
29.384918	1610.860738	16.755751
29.445134	1625.964190	16.760768
29.516443	1616.619522	16.765786
29.716857	1613.165071	16.770803
30.037158	1611.104441	16.775821
29.975457	1609.745474	16.780839
29.707509	1605.734238	16.785856
29.641920	1606.127843	16.790874
29.943921	1598.368427	16.795891
29.791255	1605.274771	16.800909
29.995561	1599.742955	16.805927
30.386465	1598.943001	16.810944
29.906846	1598.268046	16.815962
30.176826	1592.231629	16.820979
30.291005	1580.325592	16.825997
29.984013	1562.255086	16.831015
30.205180	1564.284056	16.836032
30.143725	1556.503574	16.841050
30.119499	1555.345858	16.846067
30.075777	1566.219402	16.851085
29.986729	1556.316004	16.856103
30.168843	1554.486610	16.861120
30.044455	1557.384013	16.866138
30.356809	1564.498870	16.871155
30.427546	1570.983433	16.876173
30.443481	1567.230921	16.881191
30.191987	1555.159307	16.886208
30.199720	1566.697508	16.891226
30.189823	1570.568771	16.896243
29.984938	1589.427175	16.901261
30.485096	1592.760533	16.906279
30.631195	1595.521651	16.911296
30.510042	1598.927566	16.916314
30.583748	1597.411059	16.921331
30.624003	1604.878238	16.926349
30.734915	1592.829824	16.931367
30.662729	1596.851994	16.936384
30.413456	1601.788615	16.941402
30.681725	1591.979741	16.946419
30.413046	1592.574812	16.951437
30.278853	1587.726804	16.956455
30.343955	1594.472149	16.961472
30.241383	1589.142911	16.966490
30.257685	1589.608337	16.971507
30.150882	1601.197095	16.976525
30.380571	1617.053062	16.981543
30.845263	1609.503997	16.986560
30.738440	1623.985226	16.991578
30.730624	1618.654796	16.996595
30.849603	1616.985491	17.001613
31.078600	1622.751269	17.006631
31.153026	1614.414722	17.011648
31.080403	1623.237252	17.016666
30.905347	1616.315366	17.021683
30.687700	1636.999526	17.026701
31.042283	1648.257705	17.031719
31.454750	1641.210995	17.036736
31.264826	1645.674390	17.041754
31.806910	1646.609506	17.046771
31.913792	1641.306461	17.051789
31.713473	1626.183440	17.056807
31.598010	1606.642893	17.061824
31.619153	1616.007695	17.066842
31.752905	1614.876473	17.071859
31.259245	1610.958653	17.076877
30.950421	1603.937354	17.081895
31.467136	1603.517268	17.086912
30.980670	1609.390929	17.091930
31.543228	1620.687748	17.096947
31.483982	1641.074334	17.101965
31.751622	1636.996514	17.106983
31.742649	1641.694788	17.112000
31.666776	1648.119500	17.117018
31.692930	1646.073108	17.122035
31.726675	1631.887536	17.127053
31.762086	1641.919653	17.132071
31.934445	1638.637965	17.137088
31.805732	1644.584461	17.142106
31.937802	1625.627539	17.147123
32.367804	1639.447527	17.152141
32.040108	1637.779625	17.157159
31.923413	1639.523034	17.162176
32.144553	1635.547428	17.167194
32.092150	1638.563588	17.172211
32.011137	1640.358939	17.177229
32.087687	1631.988960	17.182247
31.823030	1635.401805	17.187264
31.690080	1644.902469	17.192282
31.974511	1629.072514	17.197299
31.919863	1635.170472	17.202317
32.129086	1637.792370	17.207335
32.218631	1635.518126	17.212352
32.200007	1637.649557	17.217370
32.060310	1635.724823	17.222387
32.420419	1654.531527	17.227405
32.393383	1656.675382	17.232423
32.452276	1653.412550	17.237440
32.485034	1665.552952	17.242458
32.385070	1665.503463	17.247475
32.497999	1661.542292	17.252493
32.708341	1660.558571	17.257511
32.764338	1657.226142	17.262528
32.752683	1660.577258	17.267546
33.099061	1657.534750	17.272563
32.875992	1653.640448	17.277581
32.581033	1656.168195	17.282599
32.636985	1639.851804	17.287616
32.441460	1650.571113	17.292634
32.808245	1657.353745	17.297651
33.097388	1656.352202	17.302669
32.944946	1660.686540	17.307687
33.141940	1655.733861	17.312704
32.712112	1663.328407	17.317722
33.015544	1660.414293	17.322739
32.957136	1656.292627	17.327757
33.070890	1661.586245	17.332775
33.182467	1648.852259	17.337792
32.669118	1664.571932	17.342810
32.909480	1654.076726	17.347827
32.860406	1662.233961	17.352845
32.934106	1665.503571	17.357863
33.193672	1657.108672	17.362880
33.056848	1655.288575	17.367898
33.130410	1671.818958	17.372915
33.098339	1678.407659	17.377933
33.064559	1679.945957	17.382951
33.455274	1688.355697	17.387968
33.285633	1681.503745	17.392986
33.473471	1693.290448	17.398003
33.611779	1690.987226	17.403021
33.769713	1690.146068	17.408039
34.104608	1691.770729	17.413056
33.403290	1691.140883	17.418074
33.692911	1679.548124	17.423091
33.669967	1676.763840	17.428109
33.324970	1686.343471	17.433127
33.615335	1677.761950	17.438144
33.655530	1687.549211	17.443162
33.849177	1682.257716	17.448179
33.600998	1675.660154	17.453197
33.453523	1681.064124	17.458215
33.790585	1689.909151	17.463232
33.710037	1701.822748	17.468250
33.961595	1722.435732	17.473267
34.174982	1713.340223	17.478285
34.308992	1718.824585	17.483303
34.496177	1712.819205	17.488320
34.356610	1697.006895	17.493338
34.178170	1678.017266	17.498355
33.989607	1683.279643	17.503373
33.852301	1682.506059	17.508391
34.125442	1697.794662	17.513408
34.365949	1711.912740	17.518426
34.445503	1708.224029	17.523443
34.499080	1711.105267	17.528461
34.076397	1715.827836	17.533479
34.290663	1715.587541	17.538496
34.321056	1712.530217	17.543514
34.228458	1715.643228	17.548531
34.407630	1702.680250	17.553549
33.987070	1707.686710	17.558567
34.115662	1699.413948	17.563584
34.368974	1715.777498	17.568602
34.596086	1721.860157	17.573619
34.981006	1730.460250	17.578637
34.663075	1742.001526	17.583655
34.847552	1738.828039	17.588672
34.403678	1744.458454	17.593690
34.549665	1737.209144	17.598707
35.065252	1735.330999	17.603725
34.891476	1730.920225	17.608743
35.013483	1736.764851	17.613760
35.307079	1730.296116	17.618778
35.302796	1736.165274	17.623795
34.860596	1719.839862	17.628813
34.706351	1721.809596	17.633831
34.995505	1724.296966	17.638848
34.824038	1737.081592	17.643866
34.717060	1733.648677	17.648883
35.092308	1728.571468	17.653901
35.111510	1741.197245	17.658919
35.257521	1733.912106	17.663936
34.715256	1739.634462	17.668954
34.908541	1731.074164	17.673971
34.942523	1742.316012	17.678989
34.939344	1760.839529	17.684007
35.397606	1759.230353	17.689024
35.789672	1761.463621	17.694042
35.505979	1759.010056	17.699059
36.085767	1749.316629	17.704077
35.560411	1754.564533	17.709095
35.764307	1749.347295	17.714112
35.418731	1755.976323	17.719130
35.585117	1759.522276	17.724147
36.150171	1753.053297	17.729165
36.087722	1754.734161	17.734183
36.169941	1745.418310	17.739200
36.203235	1754.520157	17.744218
35.852016	1747.096395	17.749235
36.116834	1736.161644	17.754253
36.137320	1728.379268	17.759271
36.143198	1720.763100	17.764288
35.819861	1724.575474	17.769306
35.877823	1728.135897	17.774323
35.999979	1715.609543	17.779341
35.772565	1722.751192	17.784359
35.906581	1731.410702	17.789376
36.231016	1746.662482	17.794394
36.507256	1742.298170	17.799411
36.393625	1745.444210	17.804429
36.428428	1753.214723	17.809447
36.381335	1754.231234	17.814464
36.272525	1751.662385	17.819482
36.537098	1746.513015	17.824499
36.828265	1753.596836	17.829517
36.148890	1753.446010	17.834535
36.259889	1752.413440	17.839552
36.458087	1742.459821	17.844570
36.098448	1758.616633	17.849587
36.308359	1751.925974	17.854605
36.495795	1751.275183	17.859623
36.575079	1744.177505	17.864640
36.712949	1749.864383	17.869658
36.289735	1745.832065	17.874675
36.605861	1739.928865	17.879693
36.554282	1763.341455	17.884711
37.045129	1769.352348	17.889728
37.048463	1779.598543	17.894746
37.015954	1775.389472	17.899763
36.923506	1780.820156	17.904781
36.641702	1779.320593	17.909799
36.978583	1771.578522	17.914816
36.973799	1776.297794	17.919834
36.825241	1779.197287	17.924851
37.049373	1779.932110	17.929869
36.830819	1781.285776	17.934887
36.885154	1783.975172	17.939904
37.433794	1776.278613	17.944922
37.184415	1784.225111	17.949939
37.279570	1774.729143	17.954957
37.190949	1776.269872	17.959975
37.318007	1774.782276	17.964992
37.392891	1776.898579	17.970010
37.590619	1783.576689	17.975027
37.167462	1774.042457	17.980045
37.196559	1790.459099	17.985063
37.454234	1796.398914	17.990080
37.443688	1806.347437	17.995098
37.069965	1808.503658	18.000115
37.376301	1799.927289	18.005133
37.102349	1813.271524	18.010151
37.517210	1821.401342	18.015168
37.840005	1827.681918	18.020186
38.042639	1833.294284	18.025203
38.029331	1828.325715	18.030221
38.143672	1834.647632	18.035239
38.096086	1819.536832	18.040256
38.311085	1802.276524	18.045274
37.906145	1802.384412	18.050291
38.111557	1792.009882	18.055309
37.781197	1799.135606	18.060327
38.120547	1810.575173	18.065344
38.626826	1827.274353	18.070362
38.451674	1819.531927	18.075379
38.363699	1797.172034	18.080397
38.474568	1798.567013	18.085415
38.620784	1792.885337	18.090432
38.454849	1790.277158	18.095450
38.199078	1798.992433	18.100467
38.114558	1787.953503	18.105485
38.346528	1798.461708	18.110503
38.353280	1807.030208	18.115520
38.786910	1803.919234	18.120538
38.889583	1814.867438	18.125555
38.837965	1794.086923	18.130573
38.491964	1795.620431	18.135591
38.634024	1783.820233	18.140608
38.656994	1796.786369	18.145626
38.341463	1814.550850	18.150643
38.533240	1810.508427	18.155661
38.525083	1825.432102	18.160679
38.742906	1822.993993	18.165696
38.942403	1817.125108	18.170714
38.814360	1821.730629	18.175731
39.074497	1812.165486	18.180749
38.694625	1818.220718	18.185767
38.853098	1827.712035	18.190784
39.161111	1819.146795	18.195802
39.156014	1847.261974	18.200819
39.620617	1840.838000	18.205837
39.178048	1835.877387	18.210855
39.391656	1822.317647	18.215872
39.396138	1816.180783	18.220890
39.193295	1820.468031	18.225907
39.150780	1815.820065	18.230925
39.569081	1838.483422	18.235943
39.390381	1845.983957	18.240960
39.401177	1849.062488	18.245978
39.390868	1851.965001	18.250995
39.651862	1846.515408	18.256013
39.542816	1848.758352	18.261031
39.361203	1854.941670	18.266048
39.599261	1843.494366	18.271066
39.233372	1846.189048	18.276083
39.654963	1843.494237	18.281101
39.891289	1848.361646	18.286119
39.494761	1840.493405	18.291136
39.638288	1841.432964	18.296154
39.637726	1855.990449	18.301171
39.871631	1857.521677	18.306189
40.034174	1873.263871	18.311207
39.959851	1873.833736	18.316224
40.252912	1876.464182	18.321242
39.929185	1870.986565	18.326259
40.024181	1872.238521	18.331277
39.756695	1869.729882	18.336295
40.089471	1876.812357	18.341312
40.307879	1868.079700	18.346330
40.096141	1882.021523	18.351347
40.494311	1866.109039	18.356365
40.641867	1866.357385	18.361383
40.075878	1874.573477	18.366400
40.255450	1870.562989	18.371418
40.429694	1868.895102	18.376435
40.299639	1881.639893	18.381453
40.608372	1898.092063	18.386471
40.840305	1898.475204	18.391488
41.149769	1889.945510	18.396506
40.954494	1877.987133	18.401523
41.037342	1871.539981	18.406541
40.891205	1864.399792	18.411559
40.864871	1861.658164	18.416576
41.006321	1855.241830	18.421594
40.510005	1857.851105	18.426611
40.745926	1869.383103	18.431629
41.257790	1877.631474	18.436647
41.154809	1879.280111	18.441664
41.398347	1878.952272	18.446682
41.403541	1867.597983	18.451699
41.326470	1848.135001	18.456717
41.153437	1855.323185	18.461735
41.115605	1844.852433	18.466752
41.393889	1848.864845	18.471770
41.524365	1846.341644	18.476787
41.266239	1852.569961	18.481805
41.329969	1843.573657	18.486823
40.947702	1865.983892	18.491840
41.567178	1869.726614	18.496858
41.314698	1894.140501	18.501875
41.533882	1888.055327	18.506893
41.498575	1881.081354	18.511911
41.235347	1883.577879	18.516928
41.794314	1881.266920	18.521946
41.565291	1894.654939	18.526963
41.506412	1881.372323	18.531981
41.625325	1884.272657	18.536999
41.623708	1879.735590	18.542016
42.111893	1897.442572	18.547034
42.052399	1902.919790	18.552051
41.995788	1903.392225	18.557069
42.323319	1897.416598	18.562087
41.845565	1896.410610	18.567104
42.161727	1896.517943	18.572122
42.005427	1906.366740	18.577139
42.258288	1907.833799	18.582157
42.581381	1903.806536	18.587175
42.477527	1902.637619	18.592192
42.292471	1885.380715	18.597210
42.029456	1884.052033	18.602227
42.594906	1902.803259	18.607245
42.610821	1908.631724	18.612263
42.569526	1907.546897	18.617280
42.586204	1891.207636	18.622298
42.311776	1888.706841	18.627315
42.400316	1900.378317	18.632333
42.743658	1896.235486	18.637351
42.593838	1909.953659	18.642368
42.562100	1905.849148	18.647386
42.768612	1903.684559	18.652403
42.664177	1905.622809	18.657421
42.970500	1902.493998	18.662439
42.764597	1905.999104	18.667456
43.282258	1895.923789	18.672474
42.732481	1905.029717	18.677491
42.590789	1907.071010	18.682509
42.952300	1904.050349	18.687527
42.864904	1900.229497	18.692544
42.786593	1899.197673	18.697562
42.351401	1908.196371	18.702579
42.379371	1928.551517	18.707597
42.886656	1926.554652	18.712615
42.651665	1941.023619	18.717632
42.968051	1944.931693	18.722650
42.737154	1961.793694	18.727667
43.063421	1960.599350	18.732685
43.267500	1957.028860	18.737703
43.206315	1963.157167	18.742720
43.782912	1964.706648	18.747738
43.632149	1969.028981	18.752755
43.666984	1978.345270	18.757773
44.243085	1970.462556	18.762791
43.379433	1971.547074	18.767808
44.161728	1960.053328	18.772826
44.226432	1948.627672	18.777843
43.759050	1948.134128	18.782861
44.060756	1941.498605	18.787879
43.978866	1940.158318	18.792896
44.167122	1939.232582	18.797914
44.005108	1943.091424	18.802931
43.758461	1939.561597	18.807949
44.179012	1959.791302	18.812967
44.017280	1967.360334	18.817984
44.283309	1968.937416	18.823002
44.641601	1972.392863	18.828019
44.498845	1963.944980	18.833037
44.484219	1947.919129	18.838055
44.486099	1956.231436	18.843072
44.781163	1950.108823	18.848090
44.149054	1938.782841	18.853107
44.271868	1939.911676	18.858125
44.307918	1950.571837	18.863143
44.400293	1965.349411	18.868160
44.605668	1962.363350	18.873178
44.670381	1962.067199	18.878195
44.554457	1959.128238	18.883213
44.828186	1954.132790	18.888231
44.739917	1967.232912	18.893248
44.419203	1962.905940	18.898266
44.651007	1971.133585	18.903283
44.655921	1982.806029	18.908301
45.062652	1977.496737	18.913319
44.766406	1996.586171	18.918336
45.174901	1994.334063	18.923354
45.180379	1991.145786	18.928371
44.911832	1994.690457	18.933389
45.170480	1992.488450	18.938407
44.853687	2001.004137	18.943424
45.050565	1996.249795	18.948442
45.276265	1996.535156	18.953459
44.973177	1996.381234	18.958477
45.649086	2006.330759	18.963495
45.668760	2019.835820	18.968512
45.866133	2001.916408	18.973530
45.934964	1993.470351	18.978547
45.646328	1999.434899	18.983565
46.085361	1980.843457	18.988583
45.501040	1994.840218	18.993600
45.774903	1980.729380	18.998618
45.803122	1985.427090	19.003635
45.347115	1985.837953	19.008653
45.735088	1993.353828	19.013671
45.797162	2014.247907	19.018688
46.122377	2007.016322	19.023706
46.012497	2018.475981	19.028723
46.229013	2025.992808	19.033741
46.141470	2009.975862	19.038759
46.388475	2021.279753	19.043776
46.217869	2020.325071	19.048794
46.003583	2020.925290	19.053811
45.730470	2024.701042	19.058829
46.464838	2011.980575	19.063847
46.264665	2019.211926	19.068864
45.924743	2016.924358	19.073882
46.346357	2018.996060	19.078899
46.059332	2022.199713	19.083917
46.473206	2032.179419	19.088935
46.535291	2043.187286	19.093952
46.728452	2044.386327	19.098970
47.241493	2042.602272	19.103987
46.877632	2047.930520	19.109005
47.251916	2043.399436	19.114023
46.915321	2048.165275	19.119040
46.936358	2042.732660	19.124058
47.076527	2032.851492	19.129075
46.831476	2045.999784	19.134093
46.691098	2039.993994	19.139111
46.837724	2047.072839	19.144128
46.819407	2042.051097	19.149146
47.168480	2038.789564	19.154163
47.071093	2047.556608	19.159181
47.307874	2029.145967	19.164199
47.419180	2039.119664	19.169216
47.311184	2034.670311	19.174234
47.228571	2038.244326	19.179251
47.081911	2037.300624	19.184269
47.412576	2056.198932	19.189287
47.320088	2071.550247	19.194304
47.263405	2072.128605	19.199322
47.752063	2063.358011	19.204339
47.843007	2069.801236	19.209357
48.127620	2060.739749	19.214375
48.265250	2067.123639	19.219392
47.981035	2061.925608	19.224410
48.158758	2071.236316	19.229427
47.919197	2070.650967	19.234445
48.190601	2064.411375	19.239463
48.272237	2058.532854	19.244480
48.249571	2049.594884	19.249498
48.231170	2046.611746	19.254515
48.248120	2061.697224	19.259533
48.179342	2058.953166	19.264551
48.292494	2054.351698	19.269568
48.154940	2061.258094	19.274586
48.237889	2056.891961	19.279603
47.999133	2066.548657	19.284621
48.376657	2065.707993	19.289639
48.145992	2053.871504	19.294656
48.206484	2058.062294	19.299674
48.314425	2054.989259	19.304691
48.073644	2066.440000	19.309709
48.663675	2081.725924	19.314727
48.507799	2081.690449	19.319744
48.803323	2091.119780	19.324762
48.810134	2087.502519	19.329779
48.581611	2099.799284	19.334797
48.652426	2085.166583	19.339815
48.848175	2090.086876	19.344832
48.649282	2085.825451	19.349850
48.946852	2084.513819	19.354867
49.086081	2086.883646	19.359885
49.216005	2087.116422	19.364903
49.284023	2097.733576	19.369920
49.185971	2099.865672	19.374938
49.184129	2104.901487	19.379955
49.189830	2109.015570	19.384973
49.205274	2109.192569	19.389991
49.103994	2113.986249	19.395008
49.565520	2110.037896	19.400026
49.823667	2100.329993	19.405043
49.337924	2106.620256	19.410061
49.522846	2098.339496	19.415079
49.688868	2097.682408	19.420096
49.633112	2095.899572	19.425114
49.959761	2092.874827	19.430131
49.826111	2093.545900	19.435149
50.285190	2098.721646	19.440167
50.448334	2096.059510	19.445184
49.678424	2100.556827	19.450202
49.853001	2090.122263	19.455219
49.896461	2096.241498	19.460237
50.161100	2099.620413	19.465255
50.310821	2115.704751	19.470272
50.064307	2127.876968	19.475290
50.475127	2122.441356	19.480307
50.322242	2127.103852	19.485325
50.409071	2124.502033	19.490343
50.558955	2132.379989	19.495360
50.193618	2129.427330	19.500378
50.485397	2126.069788	19.505395
50.753046	2133.484468	19.510413
50.503655	2127.729834	19.515431
50.610999	2123.653332	19.520448
50.588109	2130.654876	19.525466
50.907831	2123.163518	19.530483
50.734248	2130.851530	19.535501
50.713431	2128.662093	19.540519
50.759617	2114.735038	19.545536
50.700385	2125.859584	19.550554
51.266271	2137.946792	19.555571
51.030313	2145.584547	19.560589
51.135998	2144.659923	19.565607
51.155925	2150.460647	19.570624
51.139080	2147.346521	19.575642
51.496691	2144.532764	19.580659
51.664215	2137.147404	19.585677
51.546084	2134.040665	19.590695
51.777811	2135.713230	19.595712
51.533224	2139.870099	19.600730
51.839696	2139.405811	19.605747
51.538125	2137.573272	19.610765
51.717953	2133.192592	19.615783
51.250345	2135.556980	19.620800
51.260921	2131.966248	19.625818
51.431880	2135.612317	19.630835
51.561648	2138.948694	19.635853
51.811157	2143.288017	19.640871
52.038643	2138.333267	19.645888
51.911146	2143.050604	19.650906
52.165823	2143.381941	19.655923
51.871045	2146.537694	19.660941
51.889636	2160.412352	19.665959
52.175420	2164.867701	19.670976
52.363832	2170.088849	19.675994
52.816682	2158.287109	19.681011
52.746353	2158.843722	19.686029
52.397668	2152.302029	19.691047
52.727117	2149.182319	19.696064
52.204143	2151.378744	19.701082
52.771265	2151.412875	19.706099
52.471762	2151.538673	19.711117
52.425401	2161.627237	19.716135
52.854106	2152.342535	19.721152
52.417585	2158.858499	19.726170
52.579931	2158.364226	19.731187
52.545830	2161.974302	19.736205
52.695808	2162.389576	19.741223
53.078248	2153.799972	19.746240
52.639656	2166.317138	19.751258
52.716924	2176.612332	19.756275
53.067025	2186.138558	19.761293
53.034772	2178.034009	19.766311
53.584861	2184.139946	19.771328
53.047059	2182.056107	19.776346
53.434060	2186.295819	19.781363
53.567575	2183.001970	19.786381
53.473918	2186.749117	19.791399
53.594901	2181.430947	19.796416
53.621311	2194.601965	19.801434
53.477740	2192.152601	19.806451
53.806111	2191.942550	19.811469
53.391207	2183.212607	19.816487
53.502366	2184.183159	19.821504
53.407405	2192.133335	19.826522
53.541204	2208.468057	19.831539
54.004746	2207.214660	19.836557
53.918895	2216.007440	19.841575
54.311354	2209.115380	19.846592
54.041758	2218.046968	19.851610
54.185406	2206.406424	19.856627
54.143536	2214.146998	19.861645
53.944394	2211.206465	19.866663
54.180143	2205.835748	19.871680
54.405066	2208.271274	19.876698
54.343908	2214.672514	19.881715
54.375522	2222.187096	19.886733
54.746788	2243.268290	19.891751
54.976926	2232.391318	19.896768
54.393259	2235.799041	19.901786
54.988713	2233.351259	19.906803
55.161361	2234.443880	19.911821
55.031389	2213.935278	19.916839
54.868708	2201.596424	19.921856
54.924927	2203.668643	19.926874
55.084071	2199.431935	19.931891
55.092153	2202.167675	19.936909
54.924984	2222.099726	19.941927
55.367358	2220.450627	19.946944
55.084655	2237.458941	19.951962
55.202595	2227.201810	19.956979
55.053956	2229.882104	19.961997
55.317917	2221.884210	19.967015
55.209919	2231.119663	19.972032
55.432199	2227.057104	19.977050
55.288054	2229.613420	19.982067
55.473274	2234.899689	19.987085
55.463771	2234.350902	19.992103
55.833921	2221.468747	19.997120
55.309678	2226.528035	20.002138
55.323253	2226.034863	20.007155
55.245267	2240.739043	20.012173
55.214013	2260.093426	20.017191
55.408745	2255.742913	20.022208
55.558695	2258.751547	20.027226
55.520119	2271.689332	20.032243
56.247250	2278.596215	20.037261
55.974061	2281.187372	20.042279
56.331498	2276.424766	20.047296
56.421180	2281.284006	20.052314
56.080642	2277.668521	20.057331
56.465808	2278.013215	20.062349
56.418756	2277.049006	20.067367
56.560093	2273.051069	20.072384
56.975373	2273.299811	20.077402
56.487347	2269.644271	20.082419
56.985922	2271.041396	20.087437
56.574293	2276.119780	20.092455
56.755352	2266.699787	20.097472
56.344292	2270.600494	20.102490
56.638131	2268.595361	20.107507
56.661665	2277.846778	20.112525
56.741372	2291.134613	20.117543
56.924675	2301.556366	20.122560
56.908097	2307.270300	20.127578
57.058976	2309.191758	20.132595
57.327288	2308.615302	20.137613
57.065436	2310.900637	20.142631
57.544615	2307.302459	20.147648
57.291222	2315.554231	20.152666
57.417277	2302.237763	20.157683
57.487741	2304.378890	20.162701
57.529461	2304.223958	20.167719
57.341497	2310.130553	20.172736
57.522738	2328.770952	20.177754
57.535912	2330.478680	20.182771
57.765173	2333.034768	20.187789
57.491780	2330.836490	20.192807
57.830122	2321.899391	20.197824
57.938422	2329.435139	20.202842
58.011265	2330.517976	20.207859
57.860640	2323.150756	20.212877
58.229213	2334.315379	20.217895
58.578435	2344.235165	20.222912
58.352151	2332.743017	20.227930
58.275400	2323.606393	20.232947
58.267488	2327.968865	20.237965
58.735646	2347.123426	20.242983
58.700738	2338.902301	20.248000
58.947639	2333.836781	20.253018
58.657988	2322.520530	20.258035
58.603600	2310.063590	20.263053
58.561317	2329.254141	20.268071
58.869281	2337.690983	20.273088
58.943896	2354.556967	20.278106
58.614916	2358.893671	20.283123
59.092042	2343.129395	20.288141
58.524149	2358.273775	20.293159
58.980651	2346.376796	20.298176
58.624472	2353.715728	20.303194
58.948481	2349.942536	20.308211
58.974880	2345.301856	20.313229
59.102258	2368.507661	20.318247
59.274828	2360.490239	20.323264
59.557499	2377.006701	20.328282
59.526622	2377.641019	20.333299
59.576577	2380.928901	20.338317
59.396420	2383.599498	20.343335
59.651685	2380.827513	20.348352
59.771105	2382.023482	20.353370
59.476131	2383.228084	20.358387
59.525656	2378.252046	20.363405
59.634958	2375.993309	20.368423
59.593030	2371.402954	20.373440
59.563280	2380.518402	20.378458
59.938157	2389.141401	20.383475
60.441116	2391.869734	20.388493
60.017368	2411.797030	20.393511
60.383083	2391.957407	20.398528
60.557876	2387.261343	20.403546
60.482888	2391.051894	20.408563
60.724449	2384.849419	20.413581
60.322758	2394.916083	20.418599
60.955002	2386.745872	20.423616
60.807584	2391.389427	20.428634
61.036324	2390.920335	20.433651
61.060528	2392.471902	20.438669
60.769498	2393.110086	20.443687
60.898677	2393.847729	20.448704
61.044047	2389.475854	20.453722
60.887434	2395.315458	20.458739
60.886903	2389.769768	20.463757
60.630536	2390.104151	20.468775
60.937425	2388.396448	20.473792
61.016972	2389.512035	20.478810
61.038292	2385.563150	20.483827
61.221616	2384.498834	20.488845
60.916060	2393.455004	20.493863
61.257096	2399.230407	20.498880
61.143551	2417.501389	20.503898
61.305917	2413.487323	20.508915
61.528467	2419.533614	20.513933
61.414333	2420.549104	20.518951
61.684443	2410.572871	20.523968
61.593358	2424.742379	20.528986
61.600037	2442.022910	20.534003
61.876428	2445.134586	20.539021
61.621217	2446.261715	20.544039
61.779875	2447.866141	20.549056
62.500267	2445.603870	20.554074
62.032028	2449.195610	20.559091
62.113033	2436.960562	20.564109
62.220095	2445.421009	20.569127
62.250345	2438.448883	20.574144
62.442428	2457.228584	20.579162
62.324018	2463.448884	20.584179
62.535473	2464.337822	20.589197
62.387728	2469.474384	20.594215
62.956204	2465.600298	20.599232
62.440963	2464.945784	20.604250
62.631638	2463.252663	20.609267
62.664069	2465.712741	20.614285
62.305543	2466.726723	20.619303
62.738253	2476.883908	20.624320
63.018211	2498.474735	20.629338
63.049136	2492.071390	20.634355
63.352929	2495.379710	20.639373
63.429895	2487.991124	20.644391
63.262822	2487.069290	20.649408
63.026514	2483.751404	20.654426
62.904439	2489.792790	20.659443
63.342507	2487.694760	20.664461
63.163043	2494.403581	20.669479
63.093978	2506.731255	20.674496
63.566245	2506.626031	20.679514
63.345044	2521.808230	20.684531
63.718988	2503.202968	20.689549
63.892395	2508.890520	20.694567
64.303337	2506.505648	20.699584
64.041122	2510.598612	20.704602
64.099513	2500.469707	20.709619
64.167462	2504.196765	20.714637
64.094401	2507.293694	20.719655
64.362368	2506.301133	20.724672
64.433688	2510.653244	20.729690
64.198121	2510.984566	20.734707
64.194042	2507.948170	20.739725
64.201509	2511.615988	20.744743
64.463603	2524.935525	20.749760
64.912118	2527.075273	20.754778
64.797932	2533.260252	20.759795
65.325677	2523.928949	20.764813
64.776664	2523.808410	20.769831
64.741317	2513.383646	20.774848
64.935551	2525.406937	20.779866
64.983390	2532.221311	20.784883
65.065755	2527.160631	20.789901
64.997604	2527.912571	20.794919
65.239099	2522.456142	20.799936
65.141733	2520.986089	20.804954
65.440318	2527.097348	20.809971
65.325799	2529.329093	20.814989
65.209718	2527.242048	20.820007
65.383998	2516.325342	20.825024
65.600885	2530.005165	20.830042
65.496682	2533.800212	20.835059
65.583725	2547.442178	20.840077
65.734994	2550.695935	20.845095
65.589707	2553.378483	20.850112
65.530391	2553.797447	20.855130
65.483522	2559.874395	20.860147
65.570287	2555.790571	20.865165
65.710431	2574.308169	20.870183
66.040429	2584.086023	20.875200
66.168953	2577.226642	20.880218
66.010195	2580.577206	20.885235
66.784404	2576.401963	20.890253
66.133978	2572.640264	20.895271
65.919622	2582.541263	20.900288
66.824853	2589.036391	20.905306
66.628446	2609.630908	20.910323
67.004859	2600.031392	20.915341
67.028672	2609.181381	20.920359
66.937342	2609.708428	20.925376
67.132733	2601.833552	20.930394
67.111536	2608.812587	20.935411
67.047293	2597.274021	20.940429
67.431111	2601.611233	20.945447
66.944609	2592.097649	20.950464
67.282145	2596.507907	20.955482
67.037094	2602.289448	20.960499
67.546715	2591.773276	20.965517
67.436070	2588.451413	20.970535
67.524299	2596.159530	20.975552
67.490612	2594.044216	20.980570
67.008441	2598.982845	20.985587
67.452591	2596.920800	20.990605
67.582184	2600.541570	20.995623
67.757432	2618.730146	21.000640
67.930034	2627.234526	21.005658
67.379212	2623.155067	21.010675
67.661946	2631.955726	21.015693
68.009058	2626.317923	21.020711
67.411071	2628.109143	21.025728
68.103229	2625.996428	21.030746
68.059823	2642.745325	21.035763
67.618853	2642.568637	21.040781
67.928635	2647.641031	21.045799
68.022907	2640.462103	21.050816
68.098716	2658.073919	21.055834
68.874742	2653.389278	21.060851
69.707082	2641.393787	21.065869
69.869700	2626.503183	21.070887
69.925438	2615.302946	21.075904
69.903699	2615.460932	21.080922
69.733453	2604.691582	21.085939
69.986915	2588.435863	21.090957
69.789841	2581.697523	21.095975
69.514107	2583.970636	21.100992
69.915789	2574.304335	21.106010
69.739231	2564.818394	21.111027
69.730273	2548.796887	21.116045
69.489442	2543.720226	21.121063
69.188113	2548.158689	21.126080
69.939365	2538.031151	21.131098
69.438678	2547.771439	21.136115
69.834373	2565.961115	21.141133
69.654466	2574.603581	21.146151
69.962979	2582.879043	21.151168
69.962710	2578.845505	21.156186
69.808561	2582.213414	21.161203
70.043126	2583.126867	21.166221
70.073308	2578.488639	21.171239
70.077215	2582.137773	21.176256
70.157802	2582.322456	21.181274
69.942892	2578.409239	21.186291
70.138892	2581.396503	21.191309
69.979251	2592.129393	21.196327
70.221199	2610.833667	21.201344
70.326431	2603.606870	21.206362
70.399839	2607.664162	21.211379
70.624342	2630.512078	21.216397
70.637516	2630.628434	21.221415
70.334812	2645.106551	21.226432
70.431692	2639.072122	21.231450
70.510171	2647.227967	21.236467
70.299834	2656.125153	21.241485
70.613245	2665.577849	21.246503
70.515962	2668.434336	21.251520
71.056542	2690.948696	21.256538
71.375590	2701.414697	21.261555
71.287509	2700.836037	21.266573
71.648575	2689.351923	21.271591
71.402743	2697.260891	21.276608
71.536936	2692.006103	21.281626
71.738986	2689.333858	21.286643
71.851840	2703.038604	21.291661
72.158089	2706.151671	21.296679
72.080680	2721.881454	21.301696
72.637027	2710.962536	21.306714
72.608164	2698.351429	21.311731
72.644541	2679.233135	21.316749
72.766395	2676.118688	21.321767
72.802847	2680.449081	21.326784
72.839395	2661.070532	21.331802
72.574695	2674.958084	21.336819
72.514393	2677.185170	21.341837
72.841903	2675.470861	21.346855
72.485400	2674.978940	21.351872
72.411268	2671.732884	21.356890
72.295615	2674.720777	21.361907
72.482831	2681.788050	21.366925
72.609476	2678.420039	21.371943
72.762029	2704.574657	21.376960
72.936536	2701.922343	21.381978
72.588298	2705.783186	21.386995
72.752816	2710.306093	21.392013
73.301959	2725.269517	21.397031
73.090109	2731.677902	21.402048
73.604865	2736.972572	21.407066
73.730710	2730.676982	21.412083
73.942143	2732.896320	21.417101
74.013378	2728.784715	21.422119
73.729871	2735.184143	21.427136
73.814032	2724.224785	21.432154
74.027483	2727.206815	21.437171
74.384938	2724.705204	21.442189
74.472304	2720.351932	21.447207
74.011596	2734.136277	21.452224
74.354922	2727.886045	21.457242
74.247691	2732.121428	21.462259
74.462452	2726.432352	21.467277
74.482340	2727.839388	21.472295
74.231155	2725.384593	21.477312
74.539527	2716.055775	21.482330
74.383863	2730.309525	21.487347
74.379777	2745.751149	21.492365
74.615884	2752.935532	21.497383
74.501393	2755.752373	21.502400
74.534742	2760.645931	21.507418
74.639721	2753.488795	21.512435
74.838638	2779.131084	21.517453
74.861919	2790.680604	21.522471
74.668863	2785.805384	21.527488
74.809550	2783.770912	21.532506
74.988466	2797.050568	21.537523
75.342193	2805.611958	21.542541
75.713667	2813.397527	21.547559
75.619507	2808.653116	21.552576
75.494281	2811.494587	21.557594
75.994003	2809.965829	21.562611
75.764100	2809.969819	21.567629
76.085469	2804.832320	21.572647
75.844415	2805.174008	21.577664
75.827059	2806.334077	21.582682
76.225076	2822.939726	21.587699
76.197847	2829.186359	21.592717
76.233315	2835.646209	21.597735
76.110757	2833.170414	21.602752
76.279988	2829.601976	21.607770
76.628086	2831.413555	21.612787
76.145451	2842.427866	21.617805
76.526234	2839.294767	21.622823
76.561382	2857.066330	21.627840
76.523152	2863.740813	21.632858
76.848367	2865.834168	21.637875
76.598210	2870.413832	21.642893
77.181282	2859.782512	21.647911
76.768492	2873.550354	21.652928
77.230892	2871.579736	21.657946
77.704617	2884.928983	21.662963
77.685879	2879.902710	21.667981
77.767318	2859.378987	21.672999
77.489940	2864.123812	21.678016
77.504797	2860.417627	21.683034
77.827981	2871.321663	21.688051
77.688077	2890.032644	21.693069
77.815374	2886.636132	21.698087
77.630595	2891.504560	21.703104
77.613632	2889.520686	21.708122
77.777736	2897.225005	21.713139
77.562480	2894.775630	21.718157
77.933979	2889.793561	21.723175
77.919166	2907.159681	21.728192
78.310539	2919.191856	21.733210
78.464929	2921.875060	21.738227
78.117969	2920.597244	21.743245
78.344500	2914.595496	21.748263
78.356799	2914.765940	21.753280
78.641277	2935.599492	21.758298
79.203126	2936.118004	21.763315
78.809852	2947.693951	21.768333
79.033351	2939.601623	21.773351
79.300652	2944.113424	21.778368
79.023013	2942.244129	21.783386
79.211931	2933.370888	21.788403
79.330055	2932.731571	21.793421
79.720291	2928.660211	21.798439
79.844894	2923.616401	21.803456
80.089583	2912.716065	21.808474
80.440068	2906.145656	21.813491
80.187762	2925.119468	21.818509
80.159140	2896.220174	21.823527
79.989567	2880.273052	21.828544
79.959020	2874.987703	21.833562
79.947274	2883.250011	21.838579
80.036569	2899.224331	21.843597
80.052216	2896.549957	21.848615
80.272918	2905.754413	21.853632
80.661080	2906.102565	21.858650
80.899296	2911.378290	21.863667
80.566214	2908.171282	21.868685
80.515180	2908.134521	21.873703
80.799380	2913.474657	21.878720
80.369914	2917.788447	21.883738
80.771083	2906.071905	21.888755
80.594832	2916.481774	21.893773
81.090214	2926.011088	21.898791
80.851856	2940.726044	21.903808
80.912530	2945.614331	21.908826
81.220419	2937.353639	21.913843
80.727024	2942.361172	21.918861
80.817849	2926.086459	21.923879
80.963251	2961.814148	21.928896
81.130838	2974.755659	21.933914
81.279653	2969.331015	21.938931
81.463760	2983.989977	21.943949
81.613841	2977.602065	21.948967
81.412426	2998.116820	21.953984
81.601301	2997.909866	21.959002
81.888034	3007.057342	21.964019
81.913545	2995.807521	21.969037
81.798780	3000.941925	21.974055
81.917776	3020.636875	21.979072
82.057865	3021.747171	21.984090
82.571031	3024.397541	21.989107
82.273908	3031.026139	21.994125
82.437222	3019.236435	21.999143
82.970430	3026.551111	22.004160
82.736978	3023.319253	22.009178
82.841765	3022.829009	22.014195
82.699397	3047.813843	22.019213
83.049353	3049.060535	22.024231
83.110253	3052.971193	22.029248
82.871429	3056.924575	22.034266
82.989609	3047.605120	22.039283
82.940740	3044.924118	22.044301
83.405597	3044.351198	22.049319
83.547805	3038.749269	22.054336
83.435195	3047.304429	22.059354
83.992042	3060.839635	22.064371
83.453052	3070.594485	22.069389
84.002140	3076.462743	22.074407
84.050844	3068.602167	22.079424
84.129576	3072.881152	22.084442
84.100279	3072.388385	22.089459
84.120527	3068.474941	22.094477
84.303917	3075.628469	22.099495
84.243206	3066.369049	22.104512
84.196761	3063.198630	22.109530
84.217087	3064.263080	22.114547
84.264117	3068.172503	22.119565
84.650810	3084.135387	22.124583
84.697929	3090.139831	22.129600
84.572591	3090.912326	22.134618
84.815211	3090.161361	22.139635
84.812128	3093.257801	22.144653
85.324645	3082.576635	22.149671
85.353115	3090.724882	22.154688
85.151413	3096.700989	22.159706
85.285174	3096.258688	22.164723
85.071805	3117.683131	22.169741
85.123389	3122.017826	22.174759
85.576059	3124.633777	22.179776
85.352372	3117.746465	22.184794
85.582594	3121.136052	22.189811
85.660008	3134.099375	22.194829
86.133338	3141.717385	22.199847
86.116622	3155.598011	22.204864
85.987201	3142.811509	22.209882
86.369573	3137.303895	22.214899
86.560445	3145.862615	22.219917
86.203278	3145.694826	22.224935
86.455307	3138.333929	22.229952
86.742143	3145.427775	22.234970
86.585060	3136.339853	22.239987
86.507705	3140.833786	22.245005
86.648106	3139.567091	22.250023
87.085311	3167.849753	22.255040
87.284907	3170.834173	22.260058
87.556656	3171.491858	22.265075
87.261783	3165.144349	22.270093
87.481818	3162.317056	22.275111
87.514442	3164.809104	22.280128
87.631717	3173.107609	22.285146
87.742407	3159.857535	22.290163
87.410390	3171.573871	22.295181
87.688157	3166.298608	22.300199
87.514472	3159.117513	22.305216
87.427470	3166.763296	22.310234
87.755694	3163.375069	22.315251
87.710304	3161.471480	22.320269
87.697764	3191.951924	22.325287
87.919496	3191.649737	22.330304
87.955218	3189.130256	22.335322
87.979194	3199.632245	22.340339
88.050255	3212.351788	22.345357
88.078119	3223.968195	22.350375
88.227342	3219.844288	22.355392
88.487259	3234.611763	22.360410
88.454352	3227.486382	22.365427
88.546449	3244.954805	22.370445
88.784087	3253.036483	22.375463
88.928842	3255.682366	22.380480
88.887341	3256.484247	22.385498
89.305024	3252.577156	22.390515
89.165707	3246.182106	22.395533
89.294389	3243.885770	22.400551
89.836092	3255.557765	22.405568
89.410628	3270.969140	22.410586
89.432904	3265.257129	22.415603
89.869864	3283.732545	22.420621
89.855493	3277.182849	22.425639
89.617352	3274.353326	22.430656
89.572315	3277.645372	22.435674
89.729633	3273.360250	22.440691
90.460490	3268.481742	22.445709
90.852221	3281.291369	22.450727
91.267567	3265.011195	22.455744
90.936987	3254.478293	22.460762
90.949988	3243.394559	22.465779
90.807666	3252.378818	22.470797
90.915269	3250.813209	22.475815
91.223619	3248.887047	22.480832
90.907003	3251.589916	22.485850
91.215813	3239.413240	22.490867
91.112957	3237.322326	22.495885
90.999688	3246.231670	22.500903
91.198319	3253.868613	22.505920
91.243466	3276.558293	22.510938
91.315126	3270.858154	22.515955
91.362338	3277.362696	22.520973
91.431428	3275.238083	22.525991
91.802442	3264.986644	22.531008
91.753136	3280.159911	22.536026
91.996164	3284.220296	22.541043
92.187590	3305.642692	22.546061
91.780358	3300.745023	22.551079
92.118024	3296.755934	22.556096
92.063104	3302.283282	22.561114
92.114156	3291.823952	22.566131
92.259454	3303.525242	22.571149
92.495675	3327.135685	22.576167
92.588129	3324.323660	22.581184
92.779431	3326.509419	22.586202
92.776823	3321.881144	22.591219
92.971968	3325.249831	22.596237
93.082576	3322.000893	22.601255
93.478043	3308.778965	22.606272
93.447148	3317.073427	22.611290
93.361948	3314.023581	22.616307
93.531152	3318.166328	22.621325
93.881041	3331.966894	22.626343
93.678420	3335.499726	22.631360
93.490972	3355.848441	22.636378
93.551608	3343.606618	22.641395
93.657990	3349.627300	22.646413
93.780485	3341.424768	22.651431
94.020418	3335.211559	22.656448
93.591943	3349.755720	22.661466
93.781920	3362.548545	22.666483
94.351133	3359.311583	22.671501
94.297853	3373.181549	22.676519
94.584042	3365.989295	22.681536
94.507237	3373.784285	22.686554
94.605060	3368.571932	22.691571
94.722276	3390.660773	22.696589
94.838648	3395.558451	22.701607
95.000818	3397.621491	22.706624
95.020417	3396.286654	22.711642
94.990625	3386.030871	22.716659
94.939141	3398.452398	22.721677
94.892025	3400.752600	22.726695
95.353484	3402.511943	22.731712
95.331500	3417.685922	22.736730
95.745596	3413.188389	22.741747
96.037866	3415.257372	22.746765
95.811852	3409.326311	22.751783
95.905816	3412.191312	22.756800
96.122684	3418.638188	22.761818
96.115673	3413.036906	22.766835
96.256866	3407.396822	22.771853
96.346745	3415.814192	22.776871
96.604685	3422.131399	22.781888
96.764200	3432.042857	22.786906
96.986913	3432.501598	22.791923
97.003030	3414.468154	22.796941
96.820590	3421.810995	22.801959
97.250985	3422.876226	22.806976
97.161410	3428.362522	22.811994
97.092340	3427.620424	22.817011
97.249106	3427.684968	22.822029
97.009336	3429.855364	22.827047
97.486833	3424.839763	22.832064
97.091182	3423.073885	22.837082
97.073938	3420.876191	22.842099
97.401977	3436.266454	22.847117
97.207035	3451.405817	22.852135
97.834248	3454.254656	22.857152
97.402331	3464.762106	22.862170
97.926098	3462.887529	22.867187
98.242509	3475.837013	22.872205
98.358098	3472.052519	22.877223
97.994841	3472.155841	22.882240
98.128882	3483.087410	22.887258
98.557214	3473.271628	22.892275
98.743623	3491.480239	22.897293
98.769871	3504.273222	22.902311
98.880162	3504.376596	22.907328
99.020929	3519.448423	22.912346
98.741438	3516.514298	22.917363
98.580079	3506.243288	22.922381
98.993004	3514.358971	22.927399
99.581810	3528.277898	22.932416
99.547798	3538.428298	22.937434
99.036389	3537.845539	22.942451
99.582130	3533.257977	22.947469
99.849875	3538.421519	22.952487
99.737766	3535.692668	22.957504
99.698572	3547.961864	22.962522
99.772131	3556.267837	22.967539
100.398278	3555.651169	22.972557
100.560478	3568.506660	22.977575
100.557357	3554.781414	22.982592
100.622533	3553.497657	22.987610
100.950511	3548.610419	22.992627
101.028494	3556.267167	22.997645
100.758577	3549.967325	23.002663
101.113174	3545.512717	23.007680
100.908999	3548.519423	23.012698
100.910228	3547.630190	23.017715
100.998494	3548.622747	23.022733
101.161970	3551.901067	23.027751
101.195691	3561.335037	23.032768
100.941281	3574.531841	23.037786
101.597051	3573.943324	23.042803
101.521982	3578.465746	23.047821
101.666447	3577.112111	23.052839
101.895052	3570.246295	23.057856
102.017358	3573.802750	23.062874
101.793029	3578.682294	23.067891
102.168055	3585.317152	23.072909
101.888525	3612.687344	23.077927
102.117598	3600.335430	23.082944
102.063001	3608.554057	23.087962
102.039731	3608.477637	23.092979
102.189261	3621.423869	23.097997
102.476293	3631.765885	23.103015
102.636805	3636.353910	23.108032
102.676257	3637.423096	23.113050
102.881637	3639.634123	23.118067
102.867033	3650.950786	23.123085
103.267482	3653.144754	23.128103
103.314381	3651.211594	23.133120
103.271806	3663.506641	23.138138
103.298457	3656.263674	23.143155
103.668917	3665.680727	23.148173
103.595542	3682.605030	23.153191
103.560773	3677.976482	23.158208
103.830612	3688.256819	23.163226
104.032956	3686.472645	23.168243
104.257725	3687.652785	23.173261
103.712307	3683.481971	23.178279
103.996895	3708.039782	23.183296
104.257347	3713.755049	23.188314
104.608689	3712.969453	23.193331
104.900532	3709.022133	23.198349
104.685084	3706.808512	23.203367
105.045623	3708.968564	23.208384
105.455527	3722.960315	23.213402
105.452176	3727.099560	23.218419
105.666698	3723.426926	23.223437
105.579124	3735.748014	23.228455
105.653392	3732.474713	23.233472
105.962836	3726.703393	23.238490
105.718491	3735.148915	23.243507
106.130879	3724.042175	23.248525
105.813397	3732.790434	23.253543
106.077241	3732.096158	23.258560
106.301251	3735.067969	23.263578
106.193158	3723.699652	23.268595
106.518602	3730.312101	23.273613
106.173142	3730.174643	23.278631
106.245860	3725.110455	23.283648
106.404416	3731.712838	23.288666
106.269540	3740.223252	23.293683
106.727708	3739.055294	23.298701
106.582136	3745.299910	23.303719
106.496040	3754.424343	23.308736
106.791777	3769.104868	23.313754
107.032438	3785.067542	23.318771
107.419429	3771.680079	23.323789
106.933717	3786.904310	23.328807
107.378682	3796.507510	23.333824
107.439213	3806.725847	23.338842
107.333950	3812.086916	23.343859
107.877826	3796.672339	23.348877
107.806705	3821.643026	23.353895
108.280239	3824.270595	23.358912
108.110022	3831.547809	23.363930
108.251996	3821.555356	23.368947
108.458275	3832.605890	23.373965
108.418611	3825.202191	23.378983
108.565316	3835.430245	23.384000
108.721557	3816.879685	23.389018
108.784448	3837.535103	23.394035
109.117299	3843.442742	23.399053
109.095911	3854.208645	23.404071
109.384682	3847.283885	23.409088
109.209506	3842.962513	23.414106
109.522392	3848.229694	23.419123
109.766531	3845.869591	23.424141
109.383056	3838.987249	23.429159
109.833374	3837.942258	23.434176
109.675582	3845.181188	23.439194
109.864617	3839.685379	23.444211
109.689534	3851.148161	23.449229
110.025055	3872.758440	23.454247
110.359086	3862.867919	23.459264
110.588049	3869.172406	23.464282
110.305689	3874.695226	23.469299
110.320920	3871.062764	23.474317
110.341321	3875.839911	23.479335
110.404716	3885.540832	23.484352
111.059253	3888.150934	23.489370
111.170034	3888.160517	23.494387
111.543821	3875.366178	23.499405
111.926794	3882.094737	23.504423
111.976312	3871.738437	23.509440
111.990858	3865.958586	23.514458
111.947626	3862.685096	23.519475
112.116445	3869.350801	23.524493
112.217541	3865.882832	23.529511
112.428000	3863.919710	23.534528
112.372310	3856.589927	23.539546
112.592077	3863.774392	23.544563
112.583833	3853.988006	23.549581
112.787601	3853.564764	23.554599
112.548842	3853.850570	23.559616
112.928934	3859.534198	23.564634
112.736831	3858.242771	23.569651
112.771546	3853.434886	23.574669
112.935567	3859.727324	23.579687
112.686793	3850.983394	23.584704
112.864497	3858.837524	23.589722
113.112248	3882.225607	23.594739
113.480491	3876.243650	23.599757
113.259254	3888.837101	23.604775
113.099978	3887.172061	23.609792
113.381731	3896.943014	23.614810
113.421906	3919.852199	23.619827
113.719248	3913.647729	23.624845
113.848066	3907.351567	23.629863
113.544435	3922.163340	23.634880
114.076617	3931.185524	23.639898
113.868270	3942.399932	23.644915
113.940399	3954.158365	23.649933
114.277177	3970.692732	23.654951
114.240566	3972.674302	23.659968
114.674797	3972.137159	23.664986
114.623992	3994.668214	23.670003
115.292031	4002.644109	23.675021
115.355426	4007.252321	23.680039
115.110851	4012.204663	23.685056
115.621069	4005.147353	23.690074
115.535820	4013.619349	23.695091
115.310881	4015.572763	23.700109
115.354293	4030.074965	23.705127
115.293881	4035.951167	23.710144
115.869017	4035.954066	23.715162
115.904729	4055.435393	23.720179
116.471448	4052.588525	23.725197
116.320511	4069.815938	23.730215
116.403669	4070.916084	23.735232
116.755867	4068.235982	23.740250
116.788956	4059.523453	23.745267
116.737222	4062.122196	23.750285
116.771684	4057.698594	23.755303
116.750001	4065.090227	23.760320
116.935481	4078.050552	23.765338
116.848326	4091.321190	23.770355
116.984969	4096.103500	23.775373
117.076027	4103.072031	23.780391
117.242965	4115.462161	23.785408
117.753985	4113.886916	23.790426
117.705414	4121.884307	23.795443
117.499165	4125.455324	23.800461
117.968182	4114.903544	23.805479
117.969349	4134.811240	23.810496
118.353764	4139.059802	23.815514
117.783343	4144.355351	23.820531
118.324074	4139.488490	23.825549
118.597978	4152.883851	23.830567
118.748132	4161.087642	23.835584
119.495945	4159.056844	23.840602
119.149759	4154.565350	23.845619
119.621633	4155.297714	23.850637
119.736241	4152.704332	23.855655
119.450816	4154.247283	23.860672
119.638261	4143.214249	23.865690
119.409717	4151.577830	23.870707
119.276924	4150.865580	23.875725
119.913377	4169.144309	23.880743
119.966420	4180.522171	23.885760
120.082276	4176.354734	23.890778
119.746258	4178.113211	23.895795
120.193609	4188.294292	23.900813
120.350479	4203.841337	23.905831
120.652968	4209.922296	23.910848
120.981435	4207.539070	23.915866
120.732817	4221.154017	23.920883
120.823892	4210.581109	23.925901
121.261065	4209.115779	23.930919
121.120047	4223.728740	23.935936
121.320264	4236.982854	23.940954
121.171242	4236.333148	23.945971
121.935003	4237.865953	23.950989
121.764068	4229.647536	23.956007
121.551904	4241.854273	23.961024
121.790630	4235.301099	23.966042
122.026885	4259.248035	23.971059
121.783328	4253.724742	23.976077
122.427017	4255.002266	23.981095
122.038304	4258.559533	23.986112
122.503230	4258.684702	23.991130
122.625792	4286.722034	23.996147
122.665852	4283.692920	24.001165
123.009486	4279.356482	24.006183
122.797448	4289.459382	24.011200
123.121925	4275.928708	24.016218
123.108527	4302.616020	24.021235
123.687883	4314.739713	24.026253
123.364132	4317.967253	24.031271
123.022948	4325.949584	24.036288
123.162202	4325.192512	24.041306
123.258955	4345.194449	24.046323
123.517486	4347.177816	24.051341
124.246078	4347.867137	24.056359
124.044399	4354.057528	24.061376
124.478400	4364.100370	24.066394
124.370629	4367.830694	24.071411
124.831112	4364.506469	24.076429
125.151064	4358.155527	24.081447
124.814374	4362.189285	24.086464
125.195474	4353.330165	24.091482
125.262186	4357.696947	24.096499
125.158399	4350.932098	24.101517
125.456252	4352.266313	24.106535
125.308757	4358.533542	24.111552
125.820253	4368.377654	24.116570
125.380688	4378.579847	24.121587
125.435468	4382.233549	24.126605
125.580956	4382.863053	24.131623
125.974921	4401.335918	24.136640
126.251645	4400.604824	24.141658
126.253501	4415.327313	24.146675
126.295690	4413.850819	24.151693
126.713294	4417.531651	24.156711
126.531177	4410.321453	24.161728
126.903231	4432.693091	24.166746
126.980293	4445.587078	24.171763
127.072560	4446.271893	24.176781
127.041776	4449.613005	24.181799
127.168608	4442.837356	24.186816
127.520965	4459.379890	24.191834
127.481189	4466.152967	24.196851
127.396507	4472.483042	24.201869
127.748001	4467.719983	24.206887
127.583693	4473.658502	24.211904
127.895403	4484.262775	24.216922
128.247509	4502.781305	24.221939
128.357135	4508.380568	24.226957
128.860102	4500.903704	24.231975
128.540409	4500.195325	24.236992
128.675427	4508.412052	24.242010
128.753137	4521.918692	24.247027
128.891310	4531.406766	24.252045
129.139968	4524.791182	24.257063
129.279038	4528.779786	24.262080
129.434054	4520.712596	24.267098
129.634203	4542.367167	24.272115
129.345573	4548.103502	24.277133
129.821854	4546.344589	24.282151
129.649627	4554.085538	24.287168
129.897025	4543.966429	24.292186
130.131733	4574.734910	24.297203
130.130328	4569.236631	24.302221
130.505400	4568.572666	24.307239
130.278465	4577.024408	24.312256
130.612819	4577.536694	24.317274
131.117395	4584.832064	24.322291
130.910994	4592.429867	24.327309
131.169180	4592.405901	24.332327
131.017990	4588.973791	24.337344
131.150338	4601.876045	24.342362
131.514187	4615.354905	24.347379
131.505688	4630.159644	24.352397
131.714165	4633.467337	24.357415
131.663640	4647.286782	24.362432
132.231627	4641.326867	24.367450
132.113637	4657.668196	24.372467
132.102986	4661.400564	24.377485
132.205758	4661.781229	24.382503
132.341462	4666.732797	24.387520
132.394729	4676.185454	24.392538
132.561404	4685.494840	24.397555
132.861596	4692.543861	24.402573
133.050487	4683.482598	24.407591
132.826072	4690.658959	24.412608
133.001896	4696.937172	24.417626
133.378569	4708.829454	24.422643
133.083764	4714.037649	24.427661
133.606930	4707.829995	24.432679
133.480443	4722.710344	24.437696
133.776435	4731.665139	24.442714
134.214544	4741.575236	24.447731
134.519722	4745.531568	24.452749
134.620948	4738.700981	24.457767
134.033353	4738.715969	24.462784
134.309210	4754.926586	24.467802
134.965170	4755.525620	24.472819
135.064541	4763.291630	24.477837
135.649278	4759.364683	24.482855
135.217965	4769.446050	24.487872
135.534570	4764.374470	24.492890
135.153339	4767.379327	24.497907
135.403082	4775.697623	24.502925
135.790833	4776.546775	24.507943
135.657128	4796.308794	24.512960
135.739196	4787.608592	24.517978
135.803494	4796.275883	24.522995
135.697699	4819.936359	24.528013
136.015797	4815.471712	24.533031
136.208441	4822.390605	24.538048
136.323956	4838.506671	24.543066
136.758394	4844.432464	24.548083
136.819658	4856.105568	24.553101
136.661833	4856.666575	24.558119
136.970404	4865.683148	24.563136
137.148425	4877.240784	24.568154
137.340863	4876.191332	24.573171
137.368195	4902.326335	24.578189
137.410679	4906.460244	24.583207
137.627264	4905.138223	24.588224
138.292452	4910.886301	24.593242
138.811712	4914.762999	24.598259
138.693719	4929.509823	24.603277
139.025430	4918.123472	24.608295
139.175626	4917.054260	24.613312
139.067946	4917.128893	24.618330
139.253155	4911.428586	24.623347
139.023859	4926.943650	24.628365
139.487258	4910.979445	24.633383
139.083170	4917.702997	24.638400
139.568155	4915.859907	24.643418
139.444465	4922.671538	24.648435
139.465862	4947.606590	24.653453
139.589687	4952.091630	24.658471
139.425897	4954.997384	24.663488
139.445052	4962.942209	24.668506
140.089509	4968.576408	24.673523
140.077765	4975.238726	24.678541
140.400563	4991.059824	24.683559
140.461065	5006.756776	24.688576
140.605577	5016.211801	24.693594
140.674042	5012.198110	24.698611
140.654334	5036.660512	24.703629
141.215566	5040.664152	24.708647
141.145717	5044.578922	24.713664
141.164354	5058.724310	24.718682
141.298909	5062.880763	24.723699
141.282705	5077.892756	24.728717
141.888180	5081.121974	24.733735
142.100239	5092.082657	24.738752
142.155116	5088.908378	24.743770
142.696220	5088.056930	24.748787
142.704236	5087.396449	24.753805
142.821972	5079.449365	24.758823
142.782247	5082.636161	24.763840
143.056205	5103.658646	24.768858
143.002361	5103.389621	24.773875
143.121781	5107.863625	24.778893
143.668735	5097.197435	24.783911
143.637158	5108.107258	24.788928
143.643456	5110.049156	24.793946
143.751996	5103.293590	24.798963
143.850549	5124.413767	24.803981
144.210857	5123.549045	24.808999
144.421741	5140.435558	24.814016
144.207397	5141.567497	24.819034
144.710034	5137.848631	24.824051
144.678925	5138.173587	24.829069
144.759369	5149.142004	24.834087
144.994338	5160.118617	24.839104
145.028919	5174.317375	24.844122
144.985535	5173.170843	24.849139
145.010711	5177.410870	24.854157
145.557311	5187.678103	24.859175
145.793753	5196.424906	24.864192
145.366556	5196.089547	24.869210
145.686160	5200.519287	24.874227
145.791512	5217.391129	24.879245
145.930326	5235.487606	24.884263
145.783672	5230.578704	24.889280
145.802237	5257.894739	24.894298
146.286429	5261.743488	24.899315
146.821740	5277.653998	24.904333
146.930102	5283.276587	24.909351
147.112678	5286.675356	24.914368
147.097122	5292.421712	24.919386
147.354367	5292.906673	24.924403
147.343513	5307.457269	24.929421
147.366406	5311.970998	24.934439
147.694681	5316.649777	24.939456
147.666104	5344.355767	24.944474
148.198029	5344.059496	24.949491
148.016707	5349.305745	24.954509
148.478226	5355.342219	24.959527
148.617142	5369.465536	24.964544
148.784985	5374.163903	24.969562
149.249342	5368.257956	24.974579
149.243704	5371.721097	24.979597
149.184870	5379.327834	24.984615
149.527583	5383.797890	24.989632
149.370672	5402.706858	24.994650
149.764674	5400.507099	24.999667
149.470901	5405.382204	25.004685
149.702037	5412.300474	25.009703
150.107764	5426.421248	25.014720
149.931039	5427.885613	25.019738
150.273754	5433.948160	25.024755
150.386387	5447.756159	25.029773
150.635199	5459.114230	25.034791
150.960493	5450.479569	25.039808
151.130367	5449.237723	25.044826
151.280914	5445.103959	25.049843
151.544127	5477.650969	25.054861
151.645388	5473.330857	25.059879
151.527243	5478.101193	25.064896
151.368337	5484.420380	25.069914
152.000299	5479.749029	25.074931
152.123890	5505.947797	25.079949
152.017464	5508.887436	25.084967
152.383638	5499.482792	25.089984
152.527202	5512.620991	25.095002
152.691062	5506.476673	25.100019
152.715026	5510.961928	25.105037
153.017628	5525.245630	25.110055
153.036191	5521.985939	25.115072
153.298927	5537.419842	25.120090
153.827849	5523.224853	25.125107
153.616752	5539.169875	25.130125
152.995208	5542.415639	25.135143
153.271533	5549.685599	25.140160
153.298716	5562.354879	25.145178
153.761520	5579.208666	25.150195
153.684981	5592.614268	25.155213
153.907994	5607.709091	25.160231
154.158202	5621.737745	25.165248
154.449389	5632.297378	25.170266
155.151756	5631.833379	25.175283
155.561550	5635.671744	25.180301
156.112660	5628.009935	25.185319
156.304673	5631.780527	25.190336
156.270858	5632.379234	25.195354
156.311557	5618.834711	25.200371
155.949578	5611.392369	25.205389
156.445039	5621.785737	25.210407
156.692474	5616.767123	25.215424
156.725613	5616.589960	25.220442
156.811827	5616.277964	25.225459
156.889596	5619.520952	25.230477
156.375761	5622.026620	25.235495
156.726350	5617.453177	25.240512
156.947291	5646.843048	25.245530
157.222043	5645.991729	25.250547
157.309096	5654.283972	25.255565
157.108043	5663.288815	25.260583
157.819444	5669.861979	25.265600
158.059539	5668.639164	25.270618
157.960069	5671.229564	25.275635
158.104309	5684.626912	25.280653
158.181115	5697.294356	25.285671
158.304734	5695.741992	25.290688
158.637141	5718.722983	25.295706
158.829243	5728.733656	25.300723
158.966092	5729.118138	25.305741
158.953914	5735.161802	25.310759
159.192835	5756.747809	25.315776
159.045755	5765.846130	25.320794
159.605513	5764.531598	25.325811
159.823520	5783.718963	25.330829
159.714697	5797.931086	25.335847
159.869167	5790.732842	25.340864
160.110174	5805.017582	25.345882
160.475260	5819.907855	25.350899
160.501063	5820.013867	25.355917
160.787765	5825.915755	25.360935
161.524106	5817.345696	25.365952
161.130040	5832.696854	25.370970
161.648055	5826.462847	25.375987
161.805701	5832.295608	25.381005
161.480292	5840.470613	25.386023
161.691072	5836.522851	25.391040
161.743655	5846.391388	25.396058
162.409006	5854.590792	25.401075
162.745339	5847.423737	25.406093
162.536327	5853.503304	25.411111
163.121778	5850.553386	25.416128
162.731703	5852.842411	25.421146
162.938979	5850.065596	25.426163
162.959384	5847.838071	25.431181
163.060282	5863.193648	25.436199
163.224865	5873.172757	25.441216
163.343074	5887.150336	25.446234
163.283417	5884.847111	25.451251
163.442210	5904.873802	25.456269
163.665391	5921.008529	25.461287
163.868848	5914.461311	25.466304
163.928091	5940.364330	25.471322
164.152220	5947.736084	25.476339
164.248242	5944.993491	25.481357
164.296965	5963.260145	25.486375
164.779396	5979.098245	25.491392
164.625319	5983.498229	25.496410
164.825492	6000.088944	25.501427
165.015304	6000.199997	25.506445
165.461802	6030.342281	25.511463
165.781643	6029.375550	25.516480
165.599574	6042.414717	25.521498
165.859136	6039.114087	25.526515
166.360254	6044.805581	25.531533
166.532693	6050.532788	25.536551
166.744725	6045.654604	25.541568
166.827083	6057.562950	25.546586
166.717099	6081.173243	25.551603
167.267213	6078.581216	25.556621
167.719636	6081.914842	25.561639
167.648167	6077.754010	25.566656
167.814859	6077.535747	25.571674
167.708895	6091.549969	25.576691
168.259525	6105.066810	25.581709
168.129908	6112.862085	25.586727
168.477780	6108.938733	25.591744
168.557791	6111.662416	25.596762
168.827669	6129.058435	25.601779
168.884500	6122.298425	25.606797
168.940323	6150.518717	25.611815
169.110352	6136.326897	25.616832
169.309031	6152.002817	25.621850
169.419403	6165.435343	25.626867
169.288228	6165.078335	25.631885
169.572546	6176.526327	25.636903
170.364704	6187.307896	25.641920
170.414313	6182.889846	25.646938
170.534461	6190.432577	25.651955
170.552693	6187.994285	25.656973
170.895661	6207.438641	25.661991
170.821432	6210.961408	25.667008
170.805912	6217.608337	25.672026
170.965542	6213.757982	25.677044
171.348727	6230.891913	25.682061
171.477122	6248.561247	25.687079
171.689261	6247.352487	25.692096
171.578071	6260.997548	25.697114
171.856562	6272.678924	25.702132
172.343496	6277.586818	25.707149
171.961336	6278.683710	25.712167
172.420052	6300.219763	25.717184
172.411498	6315.428567	25.722202
172.446797	6326.321030	25.727220
172.938994	6328.990437	25.732237
173.245679	6325.358995	25.737255
173.766157	6333.611868	25.742272
174.239515	6346.352562	25.747290
174.248944	6350.881427	25.752308
174.679847	6353.077425	25.757325
174.534749	6351.186865	25.762343
174.979760	6354.310699	25.767360
174.868324	6352.394855	25.772378
174.667501	6350.503315	25.777396
175.032212	6341.478838	25.782413
175.085916	6344.876411	25.787431
175.516666	6346.031987	25.792448
175.291537	6344.009015	25.797466
175.249845	6350.483135	25.802484
175.744545	6355.426782	25.807501
175.685624	6370.163559	25.812519
176.204806	6354.903009	25.817536
176.508507	6353.251348	25.822554
176.667193	6382.700979	25.827572
176.859857	6379.466529	25.832589
176.624466	6384.705564	25.837607
176.890281	6373.867854	25.842624
176.989126	6381.834019	25.847642
177.183153	6405.211553	25.852660
177.436677	6410.449694	25.857677
177.197383	6420.007144	25.862695
177.287253	6427.551869	25.867712
177.314360	6443.849670	25.872730
177.808451	6460.877997	25.877748
178.026455	6464.813811	25.882765
178.256640	6480.244596	25.887783
178.477205	6486.675194	25.892800
178.636640	6508.620419	25.897818
178.283944	6514.438992	25.902836
178.732904	6525.614140	25.907853
178.896717	6546.024387	25.912871
179.603367	6554.204698	25.917888
179.710716	6569.998601	25.922906
179.817307	6574.196334	25.927924
180.058330	6583.087285	25.932941
179.946188	6597.848869	25.937959
180.164424	6607.491873	25.942976
179.899407	6623.518618	25.947994
180.344085	6633.860450	25.953012
180.812101	6643.253248	25.958029
181.188181	6661.629355	25.963047
181.294077	6672.618232	25.968064
181.692720	6683.892432	25.973082
181.644660	6694.595789	25.978100
182.340426	6682.961802	25.983117
182.273330	6687.777577	25.988135
182.687660	6686.758090	25.993152
183.001018	6709.683044	25.998170
182.953496	6702.684931	26.003188
183.215810	6699.716092	26.008205
183.273091	6704.070916	26.013223
183.438015	6703.687536	26.018240
183.677954	6709.130458	26.023258
183.527489	6719.502711	26.028276
183.588028	6719.558850	26.033293
183.572997	6735.659167	26.038311
184.273264	6740.476626	26.043328
184.310834	6756.216935	26.048346
184.303461	6761.351256	26.053364
184.788145	6768.130328	26.058381
184.717435	6794.988119	26.063399
184.808557	6788.855393	26.068416
185.197376	6794.316139	26.073434
185.477049	6811.252875	26.078452
185.792076	6807.760926	26.083469
185.530022	6820.559614	26.088487
185.739954	6837.379579	26.093504
185.791067	6848.213851	26.098522
186.163410	6854.744616	26.103540
186.566734	6866.911361	26.108557
186.683387	6876.901432	26.113575
186.656207	6874.128741	26.118592
187.195022	6876.966933	26.123610
187.296012	6891.251506	26.128628
187.548889	6903.229037	26.133645
187.464991	6904.504039	26.138663
187.584799	6908.119955	26.143680
187.925489	6915.139621	26.148698
187.739152	6933.336181	26.153716
188.255275	6927.546299	26.158733
188.561871	6954.680357	26.163751
188.797240	6962.918712	26.168768
189.137118	6959.700643	26.173786
189.111854	6968.045319	26.178804
189.363388	6971.864631	26.183821
189.662287	6980.075111	26.188839
189.734566	6987.519056	26.193856
190.137625	6983.849399	26.198874
190.031818	6989.957934	26.203892
190.067464	7005.748433	26.208909
190.660089	7013.106718	26.213927
190.642507	7019.052527	26.218944
191.012047	7019.013216	26.223962
190.951876	7039.778741	26.228980
191.292493	7040.546857	26.233997
191.001455	7056.780002	26.239015
191.446871	7070.191495	26.244032
191.415580	7075.877313	26.249050
191.162280	7097.067256	26.254068
191.882029	7105.872657	26.259085
191.732517	7126.898103	26.264103
191.836063	7137.315064	26.269120
192.722612	7152.776862	26.274138
192.767305	7165.694205	26.279156
193.271673	7159.575376	26.284173
193.769361	7167.086562	26.289191
193.814283	7181.568964	26.294208
194.347743	7173.437545	26.299226
194.283489	7176.170418	26.304244
195.051832	7163.948243	26.309261
195.373242	7167.064425	26.314279
195.172754	7170.044417	26.319296
195.293242	7158.938099	26.324314
195.216062	7164.047916	26.329332
195.095388	7161.131602	26.334349
195.071853	7182.786798	26.339367
195.511505	7190.928316	26.344384
195.701932	7196.215800	26.349402
195.585514	7221.901201	26.354420
195.863961	7226.065039	26.359437
196.255506	7236.358597	26.364455
196.128889	7247.543253	26.369472
196.870789	7256.280471	26.374490
196.716934	7256.475420	26.379508
196.882520	7280.283523	26.384525
197.557764	7283.269259	26.389543
197.726340	7283.428750	26.394560
197.730781	7285.957249	26.399578
197.716494	7311.764456	26.404596
197.912982	7310.739382	26.409613
198.095002	7323.033045	26.414631
198.367992	7341.208100	26.419648
198.409725	7345.229348	26.424666
198.439418	7359.845984	26.429684
198.815735	7369.640414	26.434701
199.272248	7376.786761	26.439719
199.580425	7396.460486	26.444736
199.779549	7397.181241	26.449754
199.953150	7412.356104	26.454772
200.258597	7403.346391	26.459789
200.076416	7399.930628	26.464807
200.342063	7421.905943	26.469824
200.514252	7426.794033	26.474842
200.308291	7437.739162	26.479860
201.016313	7448.122056	26.484877
200.796212	7459.459449	26.489895
201.029326	7472.096041	26.494912
201.348980	7483.626543	26.499930
201.380200	7497.523903	26.504948
201.566154	7505.136671	26.509965
202.102814	7517.051761	26.514983
202.130110	7528.608031	26.520000
202.430774	7543.422417	26.525018
202.475575	7552.674982	26.530036
202.812297	7558.743289	26.535053
202.991801	7579.957271	26.540071
203.012926	7588.755359	26.545088
203.295924	7598.789138	26.550106
203.546604	7610.629726	26.555124
204.229724	7627.853971	26.560141
204.353927	7630.566636	26.565159
204.219395	7633.658633	26.570176
204.498904	7631.456335	26.575194
204.638117	7654.128026	26.580212
205.033644	7650.772181	26.585229
205.117641	7670.109344	26.590247
205.268959	7689.737817	26.595264
205.417788	7694.016262	26.600282
205.605344	7705.264828	26.605300
205.978239	7717.082825	26.610317
206.467197	7724.494905	26.615335
206.065763	7749.896109	26.620352
206.546686	7744.626148	26.625370
206.880555	7771.282883	26.630388
207.214529	7773.879586	26.635405
207.455959	7784.129128	26.640423
207.334191	7807.075193	26.645440
208.012409	7817.092280	26.650458
208.227477	7826.177291	26.655476
208.276533	7821.655690	26.660493
208.116227	7836.390191	26.665511
208.778502	7845.074015	26.670528
208.770477	7840.996700	26.675546
208.803269	7865.899010	26.680564
209.043902	7868.755424	26.685581
209.440422	7876.021457	26.690599
209.206191	7903.651876	26.695616
209.902148	7897.957801	26.700634
209.819943	7926.924141	26.705652
209.967281	7936.337124	26.710669
210.309530	7938.834018	26.715687
210.467312	7956.961966	26.720704
210.751915	7960.123021	26.725722
210.882844	7977.191270	26.730740
211.380205	7988.783200	26.735757
211.584206	7998.071800	26.740775
211.249756	8016.291053	26.745792
211.539079	8025.051123	26.750810
212.019508	8046.366967	26.755828
212.197469	8056.550035	26.760845
212.227609	8067.943955	26.765863
212.517080	8086.678760	26.770880
213.002889	8087.101424	26.775898
213.525556	8106.889269	26.780916
213.416512	8121.705314	26.785933
213.565398	8114.436845	26.790951
213.770056	8131.656853	26.795968
214.243645	8138.170542	26.800986
214.206983	8144.019902	26.806004
214.815719	8142.399304	26.811021
214.939903	8143.240462	26.816039
214.851531	8164.339039	26.821056
215.105212	8164.647457	26.826074
215.087854	8174.392002	26.831092
215.552354	8180.023407	26.836109
216.071604	8190.978529	26.841127
215.863384	8197.670119	26.846144
215.936542	8205.075892	26.851162
216.028841	8220.766809	26.856180
215.805442	8240.575590	26.861197
216.017930	8247.210691	26.866215
215.991346	8269.659524	26.871232
216.412389	8288.236431	26.876250
216.990916	8310.408333	26.881268
217.191058	8330.335118	26.886285
217.789161	8350.258036	26.891303
217.928599	8359.860848	26.896320
218.474865	8377.061385	26.901338
218.780966	8385.914969	26.906356
218.907632	8386.186992	26.911373
218.982438	8395.878549	26.916391
219.466887	8419.423480	26.921408
219.685101	8414.840521	26.926426
219.787570	8418.313147	26.931444
220.163280	8438.664626	26.936461
220.101935	8437.612215	26.941479
219.777574	8458.685796	26.946496
220.090927	8464.841835	26.951514
220.803483	8468.167418	26.956532
220.448199	8497.530703	26.961549
221.105560	8507.362642	26.966567
221.441635	8531.361703	26.971584
221.931208	8520.065503	26.976602
222.202419	8522.513639	26.981620
222.434752	8533.831761	26.986637
223.043818	8530.481220	26.991655
223.255002	8547.710834	26.996672
223.073626	8543.355715	27.001690
223.333318	8543.818326	27.006708
223.385324	8541.845913	27.011725
223.746733	8553.282031	27.016743
224.090179	8565.165422	27.021760
224.142984	8560.708371	27.026778
224.243067	8575.767372	27.031796
224.392196	8592.685951	27.036813
224.677944	8593.192287	27.041831
224.789274	8618.938988	27.046848
224.867954	8618.303643	27.051866
225.261108	8632.320672	27.056884
225.498797	8648.278527	27.061901
225.982532	8638.834392	27.066919
226.482428	8635.182935	27.071936
226.750468	8633.522795	27.076954
227.177068	8651.052305	27.081972
227.029391	8657.460684	27.086989
227.486774	8662.453017	27.092007
227.901372	8665.979394	27.097024
227.645292	8664.848252	27.102042
228.077550	8666.159734	27.107060
228.034328	8670.152107	27.112077
228.239742	8672.232298	27.117095
228.339803	8693.064732	27.122112
228.360669	8688.876844	27.127130
228.185832	8710.300087	27.132148
228.266538	8721.576578	27.137165
228.611447	8737.312684	27.142183
228.879409	8762.867381	27.147200
229.056526	8763.839208	27.152218
229.013882	8784.485144	27.157236
229.578665	8787.711675	27.162253
230.299841	8807.042819	27.167271
230.405206	8818.248323	27.172288
230.389001	8831.025100	27.177306
230.986084	8842.688529	27.182324
230.617749	8854.821950	27.187341
231.161316	8859.922915	27.192359
231.172142	8879.233527	27.197376
231.259041	8892.921976	27.202394
231.837448	8911.850798	27.207412
231.942397	8930.061891	27.212429
232.100562	8939.357082	27.217447
232.289449	8957.879602	27.222464
232.586365	8972.083075	27.227482
233.087067	8987.320894	27.232500
233.167772	9008.801335	27.237517
233.597755	9009.438909	27.242535
233.983050	9027.428655	27.247552
234.075039	9032.131264	27.252570
234.614431	9044.531523	27.257588
234.317036	9054.985633	27.262605
234.625314	9068.872990	27.267623
234.878029	9089.814496	27.272640
234.682916	9093.184675	27.277658
235.554771	9113.415984	27.282676
235.879438	9125.422654	27.287693
236.408507	9134.987193	27.292711
236.451076	9141.262535	27.297728
236.823812	9144.187826	27.302746
237.234115	9150.752627	27.307764
237.391402	9160.746835	27.312781
237.850991	9157.023185	27.317799
238.233966	9156.550745	27.322816
238.222338	9160.479697	27.327834
238.711942	9168.016030	27.332852
238.570617	9192.833537	27.337869
238.730903	9190.636660	27.342887
238.718258	9200.250278	27.347904
238.877815	9206.170622	27.352922
239.465858	9215.003822	27.357940
239.508404	9222.271780	27.362957
239.866512	9241.314797	27.367975
239.865546	9252.994387	27.372992
239.956285	9258.004499	27.378010
240.471601	9265.157692	27.383028
240.433024	9284.100448	27.388045
240.462182	9290.618345	27.393063
240.782848	9313.483609	27.398080
240.729218	9333.560159	27.403098
241.557469	9344.046436	27.408116
241.635651	9361.388833	27.413133
241.839831	9369.506791	27.418151
242.149493	9390.881170	27.423168
242.421629	9406.002962	27.428186
242.825838	9411.304509	27.433204
242.672708	9435.197144	27.438221
242.932421	9440.138275	27.443239
243.115300	9446.745710	27.448256
243.331150	9473.204324	27.453274
243.659398	9481.085088	27.458292
243.542773	9508.951611	27.463309
244.264417	9518.107042	27.468327
244.528077	9538.427337	27.473344
244.402106	9558.780093	27.478362
244.798956	9570.457630	27.483380
245.242571	9571.841356	27.488397
245.547951	9582.820371	27.493415
245.776021	9599.056499	27.498432
245.805254	9608.329384	27.503450
246.373254	9629.400405	27.508468
246.543745	9645.541371	27.513485
246.608028	9649.202588	27.518503
247.065601	9673.114644	27.523520
247.064118	9681.434728	27.528538
247.212404	9692.332779	27.533556
247.064286	9713.727713	27.538573
247.881024	9728.636434	27.543591
247.916103	9744.673163	27.548608
248.052592	9776.634776	27.553626
248.267653	9781.666937	27.558644
248.310982	9802.415705	27.563661
248.990076	9827.620979	27.568679
248.906894	9843.382033	27.573696
249.206981	9869.723317	27.578714
249.997521	9876.848392	27.583732
250.235576	9894.858850	27.588749
250.564793	9909.261830	27.593767
251.099812	9930.602639	27.598784
251.418462	9935.835859	27.603802
252.830450	9898.702464	27.608820
253.221431	9892.528184	27.613837
253.890873	9879.156036	27.618855
254.005291	9878.900724	27.623872
253.758716	9875.417919	27.628890
254.384797	9848.055463	27.633908
254.086772	9842.198137	27.638925
254.213259	9838.320122	27.643943
254.339046	9836.141495	27.648960
254.384443	9834.953088	27.653978
254.518884	9834.961512	27.658996
254.337373	9851.158805	27.664013
254.518911	9867.150054	27.669031
254.328490	9874.532642	27.674048
254.524426	9905.047697	27.679066
254.734196	9913.328077	27.684084
254.702670	9939.116392	27.689101
255.281475	9969.682978	27.694119
255.463095	9986.509400	27.699136
255.162002	10001.235404	27.704154
255.838574	10028.711071	27.709172
255.723763	10058.601323	27.714189
256.233353	10090.763913	27.719207
256.548826	10097.320440	27.724224
256.628162	10131.414604	27.729242
256.876496	10151.080403	27.734260
257.034712	10183.924713	27.739277
257.204538	10213.841229	27.744295
257.760321	10238.181350	27.749312
258.034703	10255.679616	27.754330
258.923433	10281.771732	27.759348
259.029466	10308.253120	27.764365
259.529540	10314.046397	27.769383
260.251940	10325.351336	27.774400
260.466024	10328.381201	27.779418
260.762076	10324.847537	27.784436
260.954716	10356.225868	27.789453
261.470898	10359.299300	27.794471
261.463797	10361.786873	27.799488
261.625327	10368.577860	27.804506
261.736468	10390.192175	27.809524
261.868543	10400.170863	27.814541
262.138363	10404.507144	27.819559
262.360494	10412.882632	27.824576
261.914601	10429.576637	27.829594
262.507438	10457.731087	27.834612
262.880502	10467.579967	27.839629
262.960842	10492.508399	27.844647
263.259919	10502.569701	27.849664
263.204618	10526.763619	27.854682
263.467325	10541.880960	27.859700
263.604632	10580.914003	27.864717
264.078920	10589.775535	27.869735
264.955498	10599.584176	27.874752
264.935867	10615.317306	27.879770
265.274723	10636.838972	27.884788
265.691019	10642.402849	27.889805
266.381089	10659.377126	27.894823
266.610612	10671.864011	27.899840
266.676032	10680.828188	27.904858
266.800857	10693.828033	27.909876
267.110059	10716.612117	27.914893
267.277004	10719.032226	27.919911
267.825991	10734.915234	27.924928
267.685549	10748.478378	27.929946
268.182424	10766.490934	27.934964
268.461624	10779.585741	27.939981
268.591780	10801.407014	27.944999
269.111486	10804.596549	27.950016
269.620477	10827.851029	27.955034
270.110210	10828.321193	27.960052
269.988554	10838.284795	27.965069
270.319466	10846.035797	27.970087
270.473054	10853.715420	27.975104
270.726985	10881.192647	27.980122
271.306293	10888.131891	27.985140
271.121716	10902.252412	27.990157
271.556790	10918.598873	27.995175
271.781434	10927.330318	28.000192
272.027380	10953.200212	28.005210
272.233263	10951.465869	28.010228
272.206087	10978.312415	28.015245
272.486615	10999.605538	28.020263
272.675212	11017.367058	28.025280
272.990164	11044.208872	28.030298
273.167588	11060.090904	28.035316
273.643599	11082.325447	28.040333
273.577458	11100.942445	28.045351
273.810232	11130.834449	28.050368
274.321109	11159.222769	28.055386
275.042781	11165.672070	28.060404
275.345391	11178.383565	28.065421
275.814617	11190.186562	28.070439
276.569081	11199.246123	28.075456
276.209416	11212.756261	28.080474
276.781576	11209.514528	28.085492
277.076524	11225.870399	28.090509
277.112429	11237.479123	28.095527
277.440254	11253.117333	28.100544
277.618581	11268.914332	28.105562
277.828925	11284.980204	28.110580
277.967082	11301.385836	28.115597
278.354080	11327.478711	28.120615
278.820505	11328.234821	28.125632
278.689058	11351.747728	28.130650
278.575774	11372.608838	28.135668
279.068299	11395.031733	28.140685
279.361688	11413.756390	28.145703
279.420299	11429.538768	28.150720
279.591408	11450.855393	28.155738
279.885825	11479.819143	28.160756
279.843996	11490.290668	28.165773
280.264174	11525.416843	28.170791
280.893001	11533.577229	28.175808
280.696644	11568.399380	28.180826
281.236111	11580.922145	28.185844
281.754427	11609.235961	28.190861
281.847419	11639.880130	28.195879
282.203623	11650.156419	28.200896
282.387365	11676.885568	28.205914
283.566400	11688.315735	28.210932
284.324766	11688.968212	28.215949
284.844704	11689.332539	28.220967
285.111623	11710.876259	28.225984
285.268995	11715.712976	28.231002
285.401151	11714.759778	28.236020
285.696340	11706.543562	28.241037
285.639853	11715.946144	28.246055
285.901918	11733.368487	28.251072
286.119987	11749.542266	28.256090
286.395294	11756.786094	28.261108
286.408183	11773.939449	28.266125
286.367629	11791.402673	28.271143
286.807961	11809.411611	28.276160
287.016230	11843.305180	28.281178
286.919138	11862.260685	28.286196
287.520413	11879.685136	28.291213
287.429653	11907.221373	28.296231
287.620622	11931.937461	28.301248
287.954825	11957.713936	28.306266
288.795397	11967.114184	28.311284
289.378589	12001.106528	28.316301
289.508985	12020.678381	28.321319
290.150297	12032.294253	28.326336
290.444784	12041.096641	28.331354
290.828416	12062.451253	28.336372
291.448017	12061.695973	28.341389
291.608829	12068.345975	28.346407
292.218787	12077.103853	28.351424
292.372541	12081.375567	28.356442
292.513936	12087.794008	28.361460
293.018707	12095.554551	28.366477
292.780419	12105.252298	28.371495
293.287992	12113.871200	28.376512
294.216154	12134.396391	28.381530
294.063255	12136.512929	28.386548
294.101179	12151.445359	28.391565
294.174168	12148.004303	28.396583
294.462535	12174.059779	28.401600
294.262839	12176.615870	28.406618
294.648719	12209.245260	28.411636
295.286664	12218.978725	28.416653
295.780193	12230.713842	28.421671
296.096774	12237.620108	28.426688
296.184666	12262.297095	28.431706
296.398844	12279.285175	28.436724
296.692562	12288.313170	28.441741
297.068056	12314.370155	28.446759
297.513132	12323.321022	28.451776
297.620035	12345.658023	28.456794
298.173954	12361.877474	28.461812
298.536061	12376.337083	28.466829
298.630512	12385.974991	28.471847
299.341501	12381.353177	28.476864
299.748167	12393.348673	28.481882
299.715344	12403.559278	28.486900
299.752091	12416.133119	28.491917
299.915593	12438.169316	28.496935
300.059386	12446.067214	28.501952
300.093595	12468.864001	28.506970
300.415933	12488.423442	28.511988
300.766156	12499.214993	28.517005
300.954416	12530.932355	28.522023
301.193777	12550.907498	28.527040
301.345198	12579.134260	28.532058
301.687529	12604.117761	28.537076
302.093537	12613.612647	28.542093
302.545048	12645.358988	28.547111
302.743595	12668.188635	28.552128
302.457949	12683.934874	28.557146
303.016194	12726.466192	28.562164
303.846113	12746.704342	28.567181
304.043979	12776.307345	28.572199
304.576528	12785.399949	28.577216
304.982950	12805.757380	28.582234
305.389302	12830.688045	28.587252
306.088636	12833.246170	28.592269
306.120784	12859.168812	28.597287
306.445089	12875.129082	28.602304
306.458936	12887.008976	28.607322
306.761122	12914.801546	28.612340
307.525050	12926.640383	28.617357
307.493147	12946.933706	28.622375
307.544009	12960.126523	28.627392
307.822334	12992.507456	28.632410
308.124032	13005.739011	28.637428
308.601730	13029.402141	28.642445
308.711021	13042.074727	28.647463
308.979619	13076.123167	28.652480
309.083391	13093.332156	28.657498
309.246093	13124.249634	28.662516
310.121121	13149.848334	28.667533
310.062645	13177.241102	28.672551
310.224798	13201.338273	28.677568
310.651272	13232.472162	28.682586
311.085621	13257.094679	28.687604
311.923198	13279.185506	28.692621
312.085585	13295.278675	28.697639
312.323049	13321.981122	28.702656
312.811586	13334.023600	28.707674
313.222869	13357.572168	28.712692
313.635023	13363.857883	28.717709
313.593839	13395.980662	28.722727
314.176175	13406.855606	28.727744
314.517431	13435.424238	28.732762
314.543447	13448.000658	28.737780
314.973719	13453.306317	28.742797
315.855400	13465.365532	28.747815
316.324603	13472.596832	28.752832
316.962809	13479.194899	28.757850
316.877802	13486.195204	28.762868
317.278278	13499.664479	28.767885
317.493876	13506.573881	28.772903
317.613378	13529.296521	28.777920
318.079876	13535.852218	28.782938
318.165709	13545.492245	28.787956
318.547308	13562.376635	28.792973
318.548994	13585.030671	28.797991
318.667657	13603.922417	28.803008
318.860067	13620.138572	28.808026
319.273119	13654.104337	28.813044
319.881067	13664.789237	28.818061
319.411236	13696.156437	28.823079
319.590773	13708.917158	28.828096
320.039017	13746.646973	28.833114
320.376017	13770.840442	28.838132
321.066288	13796.477161	28.843149
321.468310	13821.332843	28.848167
321.677124	13837.891627	28.853184
321.890635	13855.626902	28.858202
322.223900	13887.080116	28.863220
322.978974	13897.455477	28.868237
323.030227	13921.863693	28.873255
323.309417	13945.643085	28.878272
323.370461	13959.681324	28.883290
323.594006	13987.726762	28.888308
324.016604	14011.075821	28.893325
324.488879	14036.969772	28.898343
324.670335	14061.501558	28.903360
325.113280	14077.942892	28.908378
325.341348	14103.923221	28.913396
325.961955	14134.369392	28.918413
326.198852	14162.283680	28.923431
326.568636	14184.661485	28.928448
327.143380	14199.774537	28.933466
327.615010	14218.687160	28.938484
327.808612	14228.966885	28.943501
328.088257	14251.432252	28.948519
328.495015	14263.719106	28.953536
329.654449	14272.505105	28.958554
329.815978	14290.883048	28.963572
329.916042	14296.191831	28.968589
330.685393	14309.865272	28.973607
330.725773	14312.801032	28.978624
331.250766	14326.139986	28.983642
331.319868	14339.455395	28.988660
331.867552	14348.395069	28.993677
331.780098	14361.643516	28.998695
332.114682	14376.779292	29.003712
332.433813	14388.861729	29.008730
332.548708	14414.117467	29.013748
332.678042	14432.166798	29.018765
332.868259	14459.066503	29.023783
333.036158	14498.095997	29.028800
333.462423	14511.779321	29.033818
333.762420	14537.866594	29.038836
334.291777	14554.814149	29.043853
334.347048	14586.855473	29.048871
334.276736	14611.122577	29.053888
335.173156	14636.727952	29.058906
334.963053	14670.922281	29.063924
335.973560	14699.720804	29.068941
336.226416	14732.818647	29.073959
336.092058	14753.982304	29.078976
337.008449	14786.657970	29.083994
337.033736	14809.913413	29.089012
337.353695	14848.184033	29.094029
337.937187	14868.598162	29.099047
338.234464	14893.398801	29.104064
338.718655	14914.059589	29.109082
338.846430	14941.815236	29.114100
339.563958	14957.527826	29.119117
339.961929	14989.550833	29.124135
340.501416	15000.110869	29.129152
340.825624	15023.182992	29.134170
340.576963	15038.447788	29.139188
341.118182	15057.709173	29.144205
341.563261	15081.989076	29.149223
341.785530	15111.373180	29.154240
342.592573	15121.444390	29.159258
342.700587	15146.773323	29.164276
342.851632	15168.938211	29.169293
342.988795	15191.564082	29.174311
343.208554	15218.214252	29.179328
343.661889	15235.257100	29.184346
343.725595	15265.049238	29.189364
344.341243	15278.559895	29.194381
344.638156	15313.498796	29.199399
345.057065	15330.720835	29.204416
345.623194	15354.522383	29.209434
345.746933	15377.877332	29.214452
346.075269	15404.120465	29.219469
346.596806	15424.845044	29.224487
346.380489	15447.224216	29.229504
347.124625	15464.456993	29.234522
347.151783	15504.177385	29.239540
347.905576	15518.423414	29.244557
348.466720	15541.182659	29.249575
348.680451	15557.841663	29.254592
349.169240	15575.730093	29.259610
349.132244	15591.773530	29.264628
349.884897	15616.214335	29.269645
350.073448	15638.175031	29.274663
350.004802	15668.363431	29.279680
350.723574	15682.587051	29.284698
350.712513	15718.022446	29.289716
351.218301	15744.770962	29.294733
351.424618	15776.017195	29.299751
351.766368	15803.803376	29.304768
352.281182	15818.475525	29.309786
352.757679	15863.775850	29.314804
353.203598	15880.136543	29.319821
353.842346	15911.807696	29.324839
353.845228	15939.354075	29.329856
354.474430	15956.149371	29.334874
354.780793	15983.658022	29.339892
355.163901	16000.781108	29.344909
355.744888	16017.913899	29.349927
356.010764	16032.132670	29.354944
356.748758	16045.659892	29.359962
357.015674	16076.326049	29.364980
357.396319	16089.214415	29.369997
357.713546	16097.400510	29.375015
357.882558	16119.477004	29.380032
358.720733	16126.676572	29.385050
359.186179	16142.660726	29.390068
359.850393	16150.138241	29.395085
360.287300	16162.000671	29.400103
360.390590	16170.584866	29.405120
361.011760	16163.863262	29.410138
361.030910	16179.998821	29.415156
361.204315	16199.094099	29.420173
361.593145	16203.901587	29.425191
361.196415	16218.113946	29.430208
361.707508	16241.818743	29.435226
361.987886	16270.123445	29.440244
362.285624	16289.987855	29.445261
362.605539	16312.296464	29.450279
362.633203	16351.418276	29.455296
362.675891	16379.578231	29.460314
362.978949	16414.669766	29.465332
363.346587	16450.477289	29.470349
363.880012	16485.172904	29.475367
363.883205	16521.022203	29.480384
364.346509	16566.269906	29.485402
364.521309	16603.990243	29.490420
364.599015	16633.320689	29.495437
365.186404	16673.660145	29.500455
365.643728	16708.837017	29.505472
366.048725	16750.731192	29.510490
366.708145	16785.132241	29.515508
366.691107	16830.581828	29.520525
367.366476	16856.452801	29.525543
367.899087	16890.648152	29.530560
368.325966	16917.419563	29.535578
368.905174	16948.325499	29.540596
369.265339	16970.596785	29.545613
370.031511	16977.249115	29.550631
370.308418	17010.995392	29.555648
371.038319	17030.345973	29.560666
371.069576	17044.249926	29.565684
371.304642	17067.866201	29.570701
371.850869	17083.366542	29.575719
372.339933	17107.804488	29.580736
372.892659	17131.804720	29.585754
373.353863	17150.449761	29.590772
373.233629	17169.791972	29.595789
373.948119	17181.249635	29.600807
373.832133	17209.145743	29.605824
374.453433	17228.144167	29.610842
374.670491	17266.453260	29.615860
374.799852	17290.259227	29.620877
375.366834	17312.769322	29.625895
375.466087	17338.013223	29.630912
375.943251	17371.246195	29.635930
376.399118	17408.040518	29.640948
376.747406	17429.832044	29.645965
377.029797	17466.612752	29.650983
377.336506	17503.233445	29.656000
377.934636	17531.519052	29.661018
378.012262	17571.031102	29.666036
378.321381	17598.262974	29.671053
378.671113	17638.606428	29.676071
379.121389	17679.100372	29.681088
379.283854	17701.722327	29.686106
379.907905	17730.301896	29.691124
380.455339	17763.317481	29.696141
381.075361	17782.535868	29.701159
381.552035	17811.275624	29.706176
382.407887	17829.203267	29.711194
384.376997	17818.954639	29.716212
384.888043	17815.248900	29.721229
385.436422	17818.783467	29.726247
385.420183	17827.773008	29.731264
385.644423	17822.844364	29.736282
385.924695	17823.302280	29.741300
385.717922	17828.117752	29.746317
385.952616	17841.165723	29.751335
385.917636	17870.575400	29.756352
386.063522	17881.161692	29.761370
386.561537	17902.153399	29.766388
386.523370	17941.335612	29.771405
386.535445	17968.038904	29.776423
386.618273	18002.070079	29.781440
387.052958	18033.839104	29.786458
387.336751	18076.819243	29.791476
387.513901	18115.327666	29.796493
388.296068	18155.778680	29.801511
388.450135	18196.244269	29.806528
388.866158	18237.155126	29.811546
389.407656	18277.138812	29.816564
389.887564	18309.949159	29.821581
391.009781	18332.081510	29.826599
391.277744	18350.725322	29.831616
392.330970	18372.121970	29.836634
392.605365	18394.103595	29.841652
392.782954	18419.834273	29.846669
393.374053	18429.828324	29.851687
393.638911	18456.372180	29.856704
394.386791	18475.600088	29.861722
394.928607	18479.716012	29.866740
394.984154	18492.080134	29.871757
395.151324	18506.162940	29.876775
395.348780	18534.658691	29.881792
395.880365	18554.280466	29.886810
395.844233	18568.206346	29.891828
395.659593	18610.135372	29.896845
396.195886	18628.209973	29.901863
396.390202	18672.470812	29.906880
396.567379	18703.139395	29.911898
397.169865	18733.229777	29.916916
397.080552	18783.383469	29.921933
397.778056	18809.731486	29.926951
398.453920	18844.302761	29.931968
399.316981	18885.900810	29.936986
399.512830	18909.500995	29.942004
399.636451	18946.662898	29.947021
400.102121	18972.218885	29.952039
401.044072	19011.072130	29.957056
401.043852	19051.781397	29.962074
401.477528	19080.037054	29.967092
401.568748	19123.062913	29.972109
402.084050	19162.283755	29.977127
402.514063	19185.244795	29.982144
402.664808	19228.374544	29.987162
403.561623	19261.778067	29.992180
403.731211	19305.393598	29.997197
404.679270	19335.823370	30.002215
404.514837	19371.850112	30.007232
405.061160	19409.390560	30.012250
406.260908	19434.180535	30.017268
406.073231	19470.485662	30.022285
406.771596	19499.096922	30.027303
407.094321	19532.441845	30.032320
407.644537	19553.250398	30.037338
408.551266	19586.351811	30.042356
408.442576	19613.054143	30.047373
408.857356	19650.665855	30.052391
409.035992	19680.743215	30.057408
409.494629	19710.775698	30.062426
409.698203	19744.227543	30.067444
409.839436	19785.987144	30.072461
410.518683	19816.311094	30.077479
410.819908	19862.939483	30.082496
411.067175	19900.229585	30.087514
411.608591	19932.637193	30.092532
411.626639	19983.959061	30.097549
412.421436	20024.122428	30.102567
412.630288	20064.421052	30.107584
412.657437	20105.304906	30.112602
413.202979	20146.146901	30.117620
413.468990	20206.413166	30.122637
414.198140	20240.440868	30.127655
414.715743	20300.011399	30.132672
414.925293	20324.579328	30.137690
415.711230	20360.642681	30.142708
416.244688	20404.175406	30.147725
417.034364	20434.264564	30.152743
417.566354	20461.520849	30.157760
418.110609	20491.256722	30.162778
419.009015	20508.979970	30.167796
419.225516	20537.225285	30.172813
419.948843	20556.663062	30.177831
421.000042	20555.730149	30.182848
421.366487	20564.359618	30.187866
422.380511	20566.956613	30.192884
422.633071	20582.693468	30.197901
423.021882	20582.808660	30.202919
423.391744	20584.833128	30.207936
423.699495	20585.395353	30.212954
424.050623	20576.556896	30.217972
423.941433	20597.143607	30.222989
424.247556	20608.471251	30.228007
424.847558	20611.373513	30.233024
424.993516	20637.062403	30.238042
425.511912	20642.675824	30.243060
425.476587	20660.954784	30.248077
425.972884	20681.545089	30.253095
426.375843	20703.632951	30.258112
426.559421	20726.253919	30.263130
426.772905	20740.258389	30.268148
427.081895	20770.066943	30.273165
427.762109	20792.813628	30.278183
428.254224	20822.144095	30.283200
428.642145	20848.836854	30.288218
429.281934	20877.638365	30.293236
429.626927	20902.684442	30.298253
429.502332	20927.460110	30.303271
430.408667	20952.729933	30.308288
430.351027	20995.246101	30.313306
430.923472	21019.830454	30.318324
431.387582	21065.440258	30.323341
431.821939	21076.196665	30.328359
431.885987	21124.685841	30.333376
432.177433	21163.379372	30.338394
432.998991	21196.018812	30.343412
433.143706	21234.613897	30.348429
433.705443	21275.917918	30.353447
433.918434	21306.479676	30.358464
434.092905	21347.061427	30.363482
435.042246	21390.341585	30.368500
435.373703	21443.733346	30.373517
435.779274	21474.506234	30.378535
436.413311	21513.821649	30.383552
437.014107	21543.032836	30.388570
437.758628	21573.081085	30.393588
438.116489	21604.349337	30.398605
438.887613	21629.041910	30.403623
439.054496	21660.704631	30.408640
439.327732	21698.130002	30.413658
440.092746	21722.036943	30.418676
439.992121	21765.533449	30.423693
440.484736	21801.664385	30.428711
441.209510	21834.053094	30.433728
441.158934	21870.808909	30.438746
441.839579	21907.832811	30.443764
442.431230	21947.580420	30.448781
442.787751	21973.234795	30.453799
443.411911	22005.219553	30.458816
444.098932	22033.395536	30.463834
444.179123	22059.510623	30.468852
444.473429	22115.449250	30.473869
444.945210	22148.861327	30.478887
445.180147	22182.738533	30.483904
445.052350	22233.892797	30.488922
445.727705	22259.489922	30.493940
446.410624	22306.343922	30.498957
446.707909	22346.127168	30.503975
447.461986	22392.723611	30.508992
447.794598	22424.781237	30.514010
448.476146	22462.236667	30.519028
449.338700	22489.696777	30.524045
449.527739	22534.244593	30.529063
450.127385	22557.136344	30.534080
450.196966	22604.279099	30.539098
450.997684	22636.082777	30.544116
451.302621	22662.530438	30.549133
451.745183	22700.352487	30.554151
452.207895	22725.835840	30.559168
452.386478	22760.540351	30.564186
452.938414	22780.415990	30.569204
453.176890	22813.098638	30.574221
453.557528	22847.569512	30.579239
454.394414	22881.250376	30.584256
454.639754	22920.293024	30.589274
455.383928	22957.056379	30.594292
455.590881	22995.378653	30.599309
455.806866	23026.080204	30.604327
456.454610	23066.134916	30.609344
457.161220	23092.962785	30.614362
457.777712	23133.937420	30.619380
458.067845	23170.229478	30.624397
458.506966	23207.868737	30.629415
459.225480	23242.525557	30.634432
459.665453	23269.942009	30.639450
460.475569	23289.013740	30.644468
460.718866	23319.198802	30.649485
460.776544	23353.107784	30.654503
461.511355	23377.132469	30.659520
461.532005	23425.971308	30.664538
461.649153	23460.898754	30.669556
462.303294	23503.744520	30.674573
462.537041	23554.946783	30.679591
462.934947	23588.503271	30.684608
463.727822	23630.372293	30.689626
464.135301	23680.230945	30.694644
464.714216	23732.380902	30.699661
464.931694	23775.683064	30.704679
465.622389	23816.307984	30.709696
465.560515	23874.006738	30.714714
466.279718	23918.202049	30.719732
466.615335	23966.994856	30.724749
466.900136	24014.583578	30.729767
467.759148	24059.211769	30.734784
468.013341	24115.835413	30.739802
468.825799	24163.024681	30.744820
469.455604	24203.529750	30.749837
469.712991	24239.678136	30.754855
470.748962	24280.976950	30.759872
471.337705	24327.689740	30.764890
471.618029	24362.285997	30.769908
472.019838	24399.382147	30.774925
472.738225	24441.986211	30.779943
473.289906	24470.494656	30.784960
473.400303	24522.686993	30.789978
474.088606	24546.564934	30.794996
474.152511	24588.126861	30.800013
474.357158	24636.847135	30.805031
475.087891	24679.433971	30.810048
475.883555	24718.767817	30.815066
476.170046	24765.897866	30.820084
476.701856	24806.975747	30.825101
477.589488	24848.701133	30.830119
478.500109	24872.041119	30.835136
478.967179	24898.224042	30.840154
479.531066	24921.678454	30.845172
480.037526	24954.579330	30.850189
480.436399	24978.439710	30.855207
481.459536	25004.016336	30.860224
481.627398	25027.886764	30.865242
482.088429	25044.879997	30.870260
482.433629	25067.396324	30.875277
483.075023	25100.000667	30.880295
483.356040	25116.979711	30.885312
483.669979	25141.059439	30.890330
484.039879	25172.920490	30.895348
484.251404	25192.566888	30.900365
484.519891	25230.131708	30.905383
484.717457	25257.681505	30.910400
485.283427	25297.960058	30.915418
485.899884	25334.688253	30.920436
486.368884	25372.185388	30.925453
486.582565	25419.852911	30.930471
486.897303	25459.649982	30.935488
487.264587	25500.435129	30.940506
488.017718	25534.236087	30.945524
488.057696	25587.641934	30.950541
488.424833	25628.493646	30.955559
488.856816	25682.345659	30.960576
489.215284	25737.613663	30.965594
489.717776	25791.895895	30.970612
490.194482	25835.612838	30.975629
490.274837	25908.446039	30.980647
491.164725	25955.968049	30.985664
491.675054	26021.371509	30.990682
492.399510	26073.750459	30.995700
493.355040	26120.634327	31.000717
493.828019	26173.367615	31.005735
494.142211	26220.238403	31.010752
494.800718	26264.976617	31.015770
495.154136	26319.458755	31.020788
496.068362	26360.792275	31.025805
496.529052	26408.374197	31.030823
497.321978	26445.633772	31.035840
498.138359	26483.756972	31.040858
498.587610	26523.937918	31.045876
499.167024	26556.056936	31.050893
499.085637	26600.373198	31.055911
499.930291	26640.526602	31.060928
500.332096	26686.519814	31.065946
500.711163	26728.655978	31.070964
501.207788	26773.848237	31.075981
501.783153	26814.989928	31.080999
502.294352	26851.035414	31.086016
502.926849	26889.262601	31.091034
503.308648	26928.067755	31.096052
503.782289	26977.289384	31.101069
504.191474	27013.074562	31.106087
505.742159	27028.608107	31.111104
506.499972	27060.077016	31.116122
507.573206	27075.768756	31.121140
508.210062	27099.920621	31.126157
508.124004	27124.492247	31.131175
508.382023	27149.886856	31.136192
509.075516	27173.474237	31.141210
509.367422	27206.910303	31.146228
509.510803	27222.743980	31.151245
509.936657	27278.791189	31.156263
510.082232	27296.889478	31.161280
510.693021	27352.729564	31.166298
511.003778	27391.131164	31.171316
511.233306	27431.924828	31.176333
511.670294	27475.100486	31.181351
512.001935	27520.653320	31.186368
512.576548	27574.168943	31.191386
513.071542	27634.022790	31.196404
513.514877	27670.781562	31.201421
513.633638	27728.395401	31.206439
514.825098	27781.657808	31.211456
514.816217	27827.217524	31.216474
515.020420	27877.338189	31.221492
516.100580	27919.338740	31.226509
516.524662	27966.924719	31.231527
517.147583	28005.859439	31.236544
517.381453	28065.950569	31.241562
518.095190	28110.009303	31.246580
518.547147	28147.934863	31.251597
518.873049	28202.206671	31.256615
519.869240	28242.802365	31.261632
520.517650	28289.115353	31.266650
520.633291	28337.258312	31.271668
521.230835	28367.573219	31.276685
521.828721	28422.595522	31.281703
522.350584	28475.151042	31.286720
522.934100	28513.001922	31.291738
523.356644	28563.264967	31.296756
524.256334	28607.234142	31.301773
524.376203	28654.881987	31.306791
524.701707	28703.073127	31.311808
525.072811	28752.736399	31.316826
525.510451	28812.704779	31.321844
526.341007	28853.200063	31.326861
526.742798	28918.477900	31.331879
526.922241	28983.310224	31.336896
527.706653	29031.946603	31.341914
528.015460	29097.944069	31.346932
528.960347	29151.541867	31.351949
529.698663	29212.562717	31.356967
530.400982	29253.411483	31.361984
530.809125	29307.805576	31.367002
530.882834	29369.524140	31.372020
531.918267	29411.766033	31.377037
532.480887	29462.809740	31.382055
533.940189	29491.885608	31.387072
534.943795	29531.766927	31.392090
535.393334	29576.624107	31.397108
535.996246	29599.210805	31.402125
536.597172	29626.883549	31.407143
536.725349	29658.928659	31.412160
537.112804	29694.082520	31.417178
537.694594	29737.504754	31.422196
538.620615	29767.246991	31.427213
538.803343	29821.856791	31.432231
539.024675	29853.741661	31.437248
539.561976	29889.861681	31.442266
539.880348	29936.773348	31.447284
540.509745	29979.607766	31.452301
541.028517	30036.304646	31.457319
541.449443	30078.240054	31.462336
541.403497	30127.913388	31.467354
541.561442	30186.232387	31.472372
542.182847	30244.379968	31.477389
542.652203	30307.941755	31.482407
543.408286	30358.586811	31.487424
544.856977	30397.661076	31.492442
545.685409	30450.629107	31.497460
546.604407	30484.696139	31.502477
547.003993	30528.491335	31.507495
547.462172	30558.075980	31.512512
547.934597	30603.121291	31.517530
548.271690	30645.327536	31.522548
548.847884	30688.349205	31.527565
548.935112	30742.378260	31.532583
548.826090	30794.212567	31.537600
549.420355	30852.811538	31.542618
549.788478	30919.698906	31.547636
550.371162	30980.840102	31.552653
550.582690	31048.362904	31.557671
551.201070	31117.058380	31.562688
551.871843	31172.477930	31.567706
552.208567	31239.687243	31.572724
553.101205	31290.918104	31.577741
553.684680	31342.897753	31.582759
553.979095	31399.967581	31.587776
554.941979	31460.387867	31.592794
555.020244	31509.959277	31.597812
556.317776	31558.507997	31.602829
557.503544	31594.855141	31.607847
558.176654	31640.548157	31.612864
558.946692	31673.197126	31.617882
559.197069	31719.881881	31.622900
559.580516	31763.430405	31.627917
560.188178	31800.675413	31.632935
560.738321	31852.258223	31.637952
561.074185	31895.092411	31.642970
561.752741	31940.542342	31.647988
562.078414	31986.205598	31.653005
562.372142	32043.384899	31.658023
562.858702	32103.810757	31.663040
563.881448	32151.059412	31.668058
564.244722	32207.306334	31.673076
564.887772	32270.963102	31.678093
565.292374	32330.706009	31.683111
565.627183	32387.450467	31.688128
565.927267	32447.624478	31.693146
566.609056	32516.153939	31.698164
567.179492	32568.164600	31.703181
567.863324	32629.774330	31.708199
568.512649	32698.000652	31.713216
569.141476	32741.236311	31.718234
569.413814	32813.280661	31.723252
570.243623	32864.520209	31.728269
570.981770	32923.701695	31.733287
571.196930	32992.796425	31.738304
571.908609	33046.255494	31.743322
572.810195	33107.575128	31.748340
573.618474	33167.190706	31.753357
573.991155	33228.863649	31.758375
574.369985	33284.095315	31.763392
575.228318	33343.580107	31.768410
575.740654	33415.479754	31.773428
576.002188	33461.274210	31.778445
577.268154	33515.270609	31.783463
578.328476	33555.555551	31.788480
579.058916	33597.245958	31.793498
579.631133	33648.066668	31.798516
580.523210	33680.901039	31.803533
581.145637	33718.895508	31.808551
581.833245	33759.706680	31.813568
582.406064	33794.298313	31.818586
582.687395	33839.980008	31.823604
583.015852	33875.265592	31.828621
583.329950	33925.442022	31.833639
583.905511	33985.272547	31.838656
584.114364	34035.368935	31.843674
584.710805	34095.669714	31.848692
585.067165	34143.144780	31.853709
585.461479	34210.892244	31.858727
585.860812	34273.274407	31.863744
586.508858	34323.431215	31.868762
586.753876	34399.390146	31.873780
587.151057	34474.140723	31.878797
587.508191	34545.685690	31.883815
588.161463	34622.912668	31.888832
588.825654	34682.961181	31.893850
589.801481	34754.442119	31.898868
590.335394	34815.285881	31.903885
590.685971	34880.329138	31.908903
591.524682	34942.530220	31.913920
592.796736	34994.040135	31.918938
592.927137	35064.318299	31.923956
593.493715	35108.109688	31.928973
594.162503	35173.366262	31.933991
594.255672	35241.284392	31.939008
595.161923	35289.185597	31.944026
595.805187	35362.778672	31.949044
596.324143	35414.373818	31.954061
596.737960	35479.771677	31.959079
596.911642	35551.881311	31.964096
598.370247	35610.055782	31.969114
598.857543	35665.071649	31.974132
599.550418	35716.389463	31.979149
600.135959	35789.144911	31.984167
600.976263	35853.962044	31.989184
602.085983	35892.315745	31.994202
603.152170	35936.745767	31.999220
603.770505	35990.980273	32.004237
604.373446	36035.799905	32.009255
604.797673	36094.561140	32.014272
605.121077	36137.098283	32.019290
605.604993	36203.497065	32.024308
605.784543	36250.921848	32.029325
606.736837	36299.121085	32.034343
607.136415	36365.212546	32.039360
607.892514	36419.343409	32.044378
608.605217	36483.167731	32.049396
608.919243	36529.702988	32.054413
609.600841	36591.465601	32.059431
609.907461	36659.448313	32.064448
610.524199	36719.817653	32.069466
611.096655	36785.149719	32.074484
611.733449	36845.648708	32.079501
612.776865	36908.384396	32.084519
613.040987	36974.639448	32.089536
613.911035	37027.878949	32.094554
614.535266	37094.491265	32.099572
615.332156	37153.323470	32.104589
616.105568	37210.676335	32.109607
616.166435	37285.554386	32.114624
617.163960	37332.088687	32.119642
617.503782	37395.795079	32.124660
617.787578	37470.270750	32.129677
618.530222	37538.159110	32.134695
619.228389	37610.344525	32.139712
619.784718	37675.401567	32.144730
620.421678	37745.129442	32.149748
620.573312	37814.272180	32.154765
621.311998	37893.929362	32.159783
621.513038	37965.532740	32.164800
622.374720	38036.793134	32.169818
622.836189	38123.551855	32.174836
623.415645	38196.879828	32.179853
624.002823	38277.520236	32.184871
624.582156	38370.210412	32.189888
625.537640	38449.695146	32.194906
626.131791	38518.666075	32.199924
627.977640	38571.842782	32.204941
629.192366	38621.358756	32.209959
630.295916	38661.054557	32.214976
631.507813	38696.512226	32.219994
632.233621	38735.055659	32.225012
632.776018	38770.492061	32.230029
633.459875	38811.580451	32.235047
633.634287	38846.235310	32.240064
634.076394	38886.180313	32.245082
635.009526	38919.740285	32.250100
635.431172	38949.477452	32.255117
636.292592	38983.068387	32.260135
636.062039	39013.213817	32.265152
637.251900	39059.597508	32.270170
637.449032	39088.592510	32.275188
638.093383	39126.623152	32.280205
638.407924	39168.638565	32.285223
639.075270	39223.117656	32.290240
639.309663	39266.273500	32.295258
639.250000	39323.777661	32.300276
639.554009	39382.392722	32.305293
640.300199	39453.374797	32.310311
640.091521	39534.402268	32.315328
640.657847	39612.226843	32.320346
641.299430	39704.159011	32.325364
641.478503	39797.270113	32.330381
642.241302	39884.160778	32.335399
642.659541	39978.682013	32.340416
643.656396	40062.273775	32.345434
644.393083	40137.780509	32.350452
645.327895	40223.687729	32.355469
646.542274	40301.091951	32.360487
647.721273	40370.926101	32.365504
648.870595	40434.770699	32.370522
649.532938	40499.775999	32.375540
649.945311	40556.403813	32.380557
651.567471	40607.966280	32.385575
652.094466	40657.734548	32.390592
652.775952	40707.496242	32.395610
653.023419	40772.416702	32.400628
653.330917	40837.614698	32.405645
654.306450	40893.060930	32.410663
654.602078	40970.974083	32.415680
655.129048	41041.727200	32.420698
655.607120	41113.874589	32.425716
655.943765	41190.200246	32.430733
656.670861	41264.671411	32.435751
656.741541	41352.043806	32.440768
657.217443	41430.841323	32.445786
657.828318	41529.306825	32.450804
658.392845	41608.522891	32.455821
659.129397	41696.326201	32.460839
659.865005	41784.287936	32.465856
660.216379	41879.537181	32.470874
661.491470	41954.289513	32.475892
662.053262	42049.334215	32.480909
662.610423	42133.983904	32.485927
663.361353	42234.068421	32.490944
664.259156	42306.561192	32.495962
665.410157	42400.805834	32.500980
665.662833	42473.848363	32.505997
666.921777	42545.969554	32.511015
667.251777	42626.971653	32.516032
668.258363	42708.366923	32.521050
669.356031	42764.739330	32.526068
669.867698	42842.141426	32.531085
670.948638	42900.228225	32.536103
671.785677	42971.376080	32.541120
672.815580	43024.836940	32.546138
673.107569	43087.551208	32.551156
672.909530	43165.034587	32.556173
673.912966	43212.586843	32.561191
674.738898	43294.036770	32.566208
675.340776	43364.217996	32.571226
676.156220	43433.606277	32.576244
677.239986	43492.748996	32.581261
677.997804	43548.311943	32.586279
679.015318	43598.552886	32.591296
679.880362	43642.517235	32.596314
680.462324	43686.175063	32.601332
680.418597	43743.494540	32.606349
681.282362	43784.933555	32.611367
681.852661	43851.383543	32.616384
681.939215	43900.513754	32.621402
682.783085	43955.968906	32.626420
683.115229	44021.155034	32.631437
683.701744	44098.843554	32.636455
684.084426	44173.115171	32.641472
684.628142	44249.336903	32.646490
685.299912	44317.874554	32.651508
685.768442	44410.379767	32.656525
686.070862	44490.090489	32.661543
686.590117	44579.894787	32.666560
687.376749	44656.431482	32.671578
687.893647	44751.892088	32.676596
688.521482	44844.669799	32.681613
689.382395	44936.683034	32.686631
690.178538	45022.644943	32.691648
691.313766	45111.515919	32.696666
691.909619	45196.520393	32.701684
692.602182	45302.321021	32.706701
693.583610	45377.498958	32.711719
693.985573	45469.742560	32.716736
694.576345	45565.498160	32.721754
695.522577	45644.958477	32.726772
696.157897	45741.307531	32.731789
696.860426	45819.094417	32.736807
697.658229	45923.216947	32.741824
698.177667	46010.729215	32.746842
698.650677	46111.376358	32.751860
699.371174	46195.038381	32.756877
700.187606	46285.660379	32.761895
701.115506	46374.249633	32.766912
701.994297	46469.652534	32.771930
702.824304	46539.087760	32.776948
704.028103	46620.899893	32.781965
706.198597	46675.827044	32.786983
708.895781	46700.278925	32.792000
709.789430	46723.527113	32.797018
710.990343	46747.775886	32.802036
711.620625	46775.299389	32.807053
712.992766	46767.413823	32.812071
713.417901	46795.700878	32.817088
713.599848	46823.242039	32.822106
714.110979	46838.232891	32.827124
713.938512	46864.127698	32.832141
714.440952	46904.117803	32.837159
714.878734	46950.330293	32.842176
715.171412	46988.315401	32.847194
715.585580	47038.662555	32.852212
715.634125	47105.141165	32.857229
716.114247	47158.654550	32.862247
716.738005	47229.819201	32.867264
716.961630	47301.947401	32.872282
717.681294	47362.069074	32.877300
718.385938	47443.992895	32.882317
719.389490	47517.381943	32.887335
719.835947	47589.313182	32.892352
720.140068	47676.789935	32.897370
721.078674	47751.577034	32.902388
721.374136	47843.704599	32.907405
722.274358	47916.079659	32.912423
722.950752	48001.519161	32.917440
723.598225	48082.668860	32.922458
724.475333	48178.737506	32.927476
724.656729	48257.006186	32.932493
725.318785	48342.926469	32.937511
725.764796	48436.822554	32.942528
726.430669	48519.363791	32.947546
727.467766	48596.677004	32.952564
728.310018	48688.206243	32.957581
728.885728	48759.836197	32.962599
729.858164	48858.096845	32.967616
730.539891	48940.463565	32.972634
730.901663	49018.152722	32.977652
731.846169	49118.469034	32.982669
732.618791	49206.996184	32.987687
733.452462	49287.753724	32.992704
733.981033	49389.274320	32.997722
735.319381	49466.607360	33.002740
735.857172	49552.250495	33.007757
736.666865	49636.914007	33.012775
737.357613	49730.276776	33.017792
737.744351	49817.803277	33.022810
739.049395	49896.890153	33.027828
739.221840	49978.521530	33.032845
740.376961	50074.566154	33.037863
741.516807	50152.364450	33.042880
741.912158	50248.119153	33.047898
742.869358	50336.020755	33.052916
743.523266	50421.781133	33.057933
744.067228	50514.745676	33.062951
745.237494	50590.298172	33.067968
745.895267	50676.611776	33.072986
746.290992	50767.182727	33.078004
746.756605	50875.120753	33.083021
747.506822	50964.300878	33.088039
748.198945	51053.579497	33.093056
748.815766	51154.001862	33.098074
749.950758	51249.000701	33.103092
750.387396	51354.817314	33.108109
751.251047	51446.893070	33.113127
751.903269	51551.411515	33.118144
752.506973	51653.986523	33.123162
753.325269	51755.168218	33.128180
753.929151	51874.428504	33.133197
754.598937	51969.779744	33.138215
755.742335	52079.128129	33.143232
756.457223	52185.932819	33.148250
757.106900	52280.113862	33.153268
758.025150	52386.247821	33.158285
759.115380	52488.740145	33.163303
760.642341	52562.813339	33.168320
761.165365	52652.746497	33.173338
761.932928	52735.260432	33.178356
763.681976	52813.429474	33.183373
764.903373	52879.524804	33.188391
766.212332	52943.432521	33.193408
766.717980	53013.355632	33.198426
767.477623	53064.580418	33.203444
767.983771	53141.428192	33.208461
768.962316	53204.431305	33.213479
769.620454	53276.440198	33.218496
770.024279	53351.802135	33.223514
770.409883	53422.795403	33.228532
770.703640	53512.075601	33.233549
770.898191	53595.136854	33.238567
771.558427	53686.366119	33.243584
772.420370	53793.363672	33.248602
773.064992	53879.801055	33.253620
773.654052	53985.189624	33.258637
774.578087	54057.928051	33.263655
775.905642	54150.065912	33.268672
776.992627	54222.329313	33.273690
778.216426	54303.971717	33.278708
778.684544	54381.892113	33.283725
779.329576	54444.082659	33.288743
780.231034	54524.857027	33.293760
780.401968	54603.427863	33.298778
781.126420	54676.574487	33.303796
781.992550	54752.048281	33.308813
782.533121	54838.696696	33.313831
783.674847	54914.277004	33.318848
784.464461	55008.005631	33.323866
785.520725	55077.655135	33.328884
786.295224	55160.879458	33.333901
786.980795	55241.648367	33.338919
788.292328	55317.764380	33.343936
788.140291	55401.345704	33.348954
788.955645	55481.853947	33.353972
789.277957	55570.304674	33.358989
790.090968	55677.718645	33.364007
791.169184	55756.863782	33.369024
791.684175	55859.134282	33.374042
792.688556	55952.781184	33.379060
793.153194	56060.191865	33.384077
793.393439	56154.667938	33.389095
794.262464	56271.275952	33.394112
794.852247	56380.658014	33.399130
795.824718	56497.578763	33.404148
796.127184	56611.167604	33.409165
797.009091	56733.709648	33.414183
797.721417	56850.776753	33.419200
797.862879	56972.280474	33.424218
798.613759	57100.344072	33.429236
799.798593	57230.251149	33.434253
800.817384	57353.962271	33.439271
802.375633	57462.488083	33.444288
803.086878	57577.714425	33.449306
804.365484	57682.660620	33.454324
805.172305	57803.098416	33.459341
806.500394	57894.507914	33.464359
807.182969	57994.031591	33.469376
808.196779	58108.572510	33.474394
808.886530	58198.515824	33.479412
809.694720	58307.960647	33.484429
810.590973	58417.366171	33.489447
811.505479	58505.839032	33.494464
812.295116	58619.908196	33.499482
813.102382	58710.630558	33.504500
814.037052	58813.516380	33.509517
814.689220	58910.224775	33.514535
815.910687	59005.290822	33.519552
816.924243	59109.751300	33.524570
817.947730	59190.536968	33.529588
818.549638	59293.531032	33.534605
819.116506	59395.400194	33.539623
819.608824	59490.273564	33.544640
820.340209	59597.184931	33.549658
821.092916	59684.590167	33.554676
822.065910	59793.301552	33.559693
822.284845	59902.075482	33.564711
823.138970	60020.085499	33.569728
823.690765	60128.186033	33.574746
824.758578	60239.127678	33.579764
825.770313	60341.319600	33.584781
826.099803	60455.974786	33.589799
827.447210	60565.892191	33.594816
827.799886	60695.808056	33.599834
828.870761	60805.033191	33.604852
829.640461	60916.021693	33.609869
830.613580	61027.507940	33.614887
831.714453	61115.303969	33.619904
832.639821	61210.707608	33.624922
833.623506	61283.980688	33.629940
834.876765	61371.733568	33.634957
835.339740	61478.358081	33.639975
836.685272	61556.369293	33.644992
837.177540	61653.009851	33.650010
837.874181	61737.197127	33.655028
839.150126	61821.661511	33.660045
839.763282	61919.743310	33.665063
840.630754	62014.484014	33.670080
841.300717	62116.400252	33.675098
842.169549	62209.574116	33.680116
842.750834	62303.497727	33.685133
843.575297	62406.483243	33.690151
844.110952	62505.086363	33.695168
844.672665	62609.639809	33.700186
845.511020	62725.026000	33.705204
846.467660	62833.642533	33.710221
846.966416	62957.297181	33.715239
847.871855	63063.041097	33.720256
848.809702	63187.357475	33.725274
849.502475	63301.961979	33.730292
850.389397	63418.349032	33.735309
850.854904	63551.930466	33.740327
851.851783	63672.896124	33.745344
852.758618	63792.088551	33.750362
853.182530	63924.396102	33.755380
853.764968	64051.513743	33.760397
854.520835	64191.979180	33.765415
855.877062	64317.870127	33.770432
856.497582	64466.173022	33.775450
857.221510	64593.460142	33.780468
858.285155	64721.317481	33.785485
859.845652	64839.958623	33.790503
861.980704	64940.621565	33.795520
862.800701	65061.574115	33.800538
863.789729	65177.600098	33.805556
864.933883	65278.732576	33.810573
865.231738	65391.075182	33.815591
866.081253	65487.491064	33.820608
867.042344	65615.320345	33.825626
867.718592	65717.019379	33.830644
868.680695	65842.371763	33.835661
869.206917	65957.650745	33.840679
869.967748	66070.078205	33.845696
871.050929	66183.350476	33.850714
871.788697	66298.899677	33.855732
872.857849	66417.448013	33.860749
873.569365	66544.148510	33.865767
874.347637	66653.864080	33.870784
875.318586	66770.199038	33.875802
876.288745	66877.980995	33.880820
877.035122	67000.044372	33.885837
877.879316	67118.703549	33.890855
879.033728	67234.536468	33.895872
880.762872	67334.450122	33.900890
881.792911	67428.676456	33.905908
883.076169	67524.852703	33.910925
884.201559	67615.915558	33.915943
885.299340	67702.899164	33.920960
886.025165	67794.250385	33.925978
887.066855	67879.518027	33.930996
887.974684	67962.487906	33.936013
888.291154	68061.906068	33.941031
889.111429	68150.499218	33.946048
889.601896	68259.904215	33.951066
890.322215	68349.387290	33.956084
891.037378	68458.370347	33.961101
891.730428	68559.738919	33.966119
892.065275	68656.608819	33.971136
892.737229	68763.387700	33.976154
893.655863	68873.881848	33.981172
894.216636	68979.194436	33.986189
894.750512	69110.542746	33.991207
895.647748	69228.035247	33.996224
896.736692	69354.297944	34.001242
896.814882	69486.906568	34.006260
897.353123	69618.377418	34.011277
898.356948	69746.894873	34.016295
899.547978	69881.249754	34.021312
900.338305	70020.275139	34.026330
901.167387	70164.593718	34.031348
902.453910	70298.796270	34.036365
903.124507	70439.229005	34.041383
904.283038	70582.717981	34.046400
905.068694	70708.855645	34.051418
906.256771	70859.448871	34.056436
907.963161	70974.135620	34.061453
908.996871	71107.088914	34.066471
911.231865	71183.926124	34.071488
913.391249	71272.468097	34.076506
914.623479	71358.179655	34.081524
915.786002	71448.222031	34.086541
916.286961	71527.466601	34.091559
917.547722	71610.474313	34.096576
918.578925	71693.071473	34.101594
919.041416	71785.805104	34.106612
919.709199	71863.562488	34.111629
920.027830	71971.023069	34.116647
920.967890	72056.027061	34.121664
921.610610	72170.011409	34.126682
921.911557	72278.507206	34.131700
922.968695	72381.869675	34.136717
923.557004	72498.286761	34.141735
924.583701	72614.340827	34.146752
925.304818	72716.635025	34.151770
926.113351	72837.728625	34.156788
926.985634	72953.462320	34.161805
927.639027	73084.125772	34.166823
928.541496	73202.631984	34.171840
929.235390	73337.881427	34.176858
930.335938	73448.210809	34.181876
931.538840	73573.922839	34.186893
932.431424	73700.559817	34.191911
933.608584	73830.729764	34.196928
934.395726	73960.775486	34.201946
935.714675	74071.881277	34.206964
936.638925	74179.707614	34.211981
937.858570	74303.656612	34.216999
938.950811	74407.939904	34.222016
939.813529	74532.037968	34.227034
940.874848	74641.899247	34.232052
941.520202	74756.668270	34.237069
942.270724	74867.195721	34.242087
943.031613	74987.309896	34.247104
943.976722	75110.657598	34.252122
944.548667	75247.520212	34.257140
945.478888	75374.072080	34.262157
945.887263	75509.717525	34.267175
946.941271	75641.126664	34.272192
947.961131	75769.221792	34.277210
948.157685	75917.212743	34.282228
949.508547	76051.857603	34.287245
950.328720	76191.372907	34.292263
951.273471	76339.185597	34.297280
952.204134	76462.733005	34.302298
952.848589	76606.796057	34.307316
953.498399	76738.746842	34.312333
954.231369	76887.167578	34.317351
955.063988	77027.875184	34.322368
956.336296	77170.705522	34.327386
957.216560	77313.197028	34.332404
958.559578	77456.649983	34.337421
959.587831	77599.846161	34.342439
960.244025	77750.986265	34.347456
961.855268	77883.315616	34.352474
962.625571	78035.906181	34.357492
963.739680	78169.281175	34.362509
964.154048	78321.066174	34.367527
964.899689	78470.222768	34.372544
966.463704	78620.395793	34.377562
966.864252	78771.521959	34.382580
968.369202	78916.608384	34.387597
969.144648	79064.663333	34.392615
970.164775	79223.324753	34.397632
971.924486	79357.390393	34.402650
972.610738	79506.139900	34.407668
973.395357	79648.175054	34.412685
974.595889	79799.776325	34.417703
976.255258	79935.943260	34.422720
977.410855	80072.251547	34.427738
977.876819	80213.647287	34.432756
978.614481	80353.069399	34.437773
979.911478	80500.901731	34.442791
981.078850	80631.258642	34.447808
983.167319	80745.135803	34.452826
984.412698	80879.017484	34.457844
986.234979	80975.201507	34.462861
987.739035	81077.100682	34.467879
988.543834	81181.798662	34.472896
989.682340	81279.780215	34.477914
990.408968	81393.260316	34.482932
991.382924	81497.855766	34.487949
991.783510	81610.454758	34.492967
992.579988	81716.105526	34.497984
993.405068	81839.427989	34.503002
994.013506	81950.286038	34.508020
995.356991	82073.991903	34.513037
996.051932	82197.420137	34.518055
996.577594	82331.239986	34.523072
997.671502	82461.980185	34.528090
998.373893	82595.272452	34.533108
998.986758	82729.396485	34.538125
1000.310430	82871.982337	34.543143
1001.387643	83014.129140	34.548160
1002.486070	83125.107696	34.553178
1003.808003	83260.926627	34.558196
1005.010808	83392.799207	34.563213
1005.875470	83529.752180	34.568231
1006.421416	83658.995745	34.573248
1007.284017	83792.679615	34.578266
1008.103695	83933.280435	34.583284
1009.131507	84077.346414	34.588301
1010.252531	84218.221643	34.593319
1010.873199	84369.905174	34.598336
1012.342934	84500.632548	34.603354
1013.416695	84633.090409	34.608372
1015.356377	84750.631334	34.613389
1016.724425	84877.600372	34.618407
1017.909605	84994.217406	34.623424
1019.149837	85116.792532	34.628442
1020.108188	85236.985381	34.633460
1021.070891	85348.351459	34.638477
1021.442727	85469.092067	34.643495
1022.379848	85575.192757	34.648512
1023.394036	85695.530565	34.653530
1023.664161	85814.410581	34.658548
1024.582942	85936.632069	34.663565
1025.768017	86063.910020	34.668583
1026.185244	86198.048623	34.673600
1026.870276	86319.899605	34.678618
1027.556516	86477.559249	34.683636
1028.474482	86614.344372	34.688653
1029.247518	86764.138862	34.693671
1029.795828	86929.816366	34.698688
1030.943830	87087.226304	34.703706
1031.936304	87255.768518	34.708724
1033.428481	87398.923688	34.713741
1034.532159	87571.164190	34.718759
1034.814547	87740.365561	34.723776
1036.452996	87894.003953	34.728794
1036.663258	88074.800007	34.733812
1037.547934	88246.417313	34.738829
1038.685213	88424.012053	34.743847
1039.749692	88602.373260	34.748864
1041.410214	88769.416871	34.753882
1042.283244	88945.591194	34.758900
1043.285471	89125.422168	34.763917
1044.238056	89307.604251	34.768935
1045.211817	89479.494121	34.773952
1046.509243	89659.583908	34.778970
1047.325821	89854.070044	34.783988
1048.328392	90044.805673	34.789005
1049.475076	90229.740837	34.794023
1050.664600	90421.055990	34.799040
1052.141572	90591.218552	34.804058
1053.422408	90778.116583	34.809076
1054.664294	90944.763862	34.814093
1056.139367	91100.082856	34.819111
1057.629497	91273.134033	34.824128
1058.681711	91431.689792	34.829146
1059.381867	91602.621283	34.834164
1060.435364	91774.628259	34.839181
1061.576761	91937.444659	34.844199
1062.193073	92107.292355	34.849216
1063.666820	92268.897603	34.854234
1064.385666	92435.736873	34.859252
1065.639484	92613.919220	34.864269
1066.837284	92786.808184	34.869287
1067.709489	92961.587915	34.874304
1068.800311	93137.687123	34.879322
1069.788653	93311.766515	34.884340
1070.755675	93482.116270	34.889357
1072.753221	93643.637402	34.894375
1074.419141	93803.056230	34.899392
1075.666023	93960.317587	34.904410
1076.480686	94117.917509	34.909428
1077.482572	94267.549915	34.914445
1078.622023	94425.186537	34.919463
1079.586543	94572.022913	34.924480
1081.649488	94699.188381	34.929498
1083.432654	94842.909204	34.934516
1084.677515	94966.818978	34.939533
1085.663885	95097.108518	34.944551
1086.822282	95235.744745	34.949568
1089.219064	95320.073848	34.954586
1090.854833	95435.565543	34.959604
1091.901424	95532.507223	34.964621
1092.795253	95628.290905	34.969639
1093.386693	95737.665189	34.974656
1094.344350	95844.415499	34.979674
1095.290895	95943.818812	34.984692
1096.267605	96034.216020	34.989709
1097.111696	96139.872333	34.994727
1097.742435	96242.279106	34.999744
1098.759099	96354.434157	35.004762
1099.213799	96479.406808	35.009780
1099.586964	96594.138507	35.014797
1100.411351	96718.943409	35.019815
1101.069573	96876.181702	35.024832
1101.616128	97024.133793	35.029850
1102.203760	97186.437421	35.034868
1102.753421	97342.348264	35.039885
1104.045740	97508.829147	35.044903
1104.888716	97678.088842	35.049920
1106.086732	97856.419540	35.054938
1107.200523	98029.871865	35.059956
1107.907583	98219.713452	35.064973
1109.056622	98404.032353	35.069991
1109.925328	98593.957562	35.075008
1110.907813	98786.309034	35.080026
1111.840564	98984.804870	35.085044
1113.096625	99176.702411	35.090061
1114.584695	99360.142677	35.095079
1115.533468	99563.724183	35.100096
1116.904428	99764.407273	35.105114
1117.957415	99962.175386	35.110132
1118.748776	100166.022074	35.115149
1119.981752	100352.607774	35.120167
1121.105376	100557.314162	35.125184
1122.895782	100762.392753	35.130202
1123.592585	100964.374747	35.135220
1125.066826	101161.879648	35.140237
1126.257267	101354.184338	35.145255
1127.073874	101558.151877	35.150272
1128.469858	101753.616553	35.155290
1129.663417	101968.801382	35.160308
1130.372702	102166.187625	35.165325
1131.437451	102384.746753	35.170343
1132.395584	102582.012571	35.175360
1133.706716	102787.693340	35.180378
1134.905300	102992.609255	35.185396
1135.950436	103209.367660	35.190413
1137.617541	103417.406833	35.195431
1138.897582	103630.843468	35.200448
1140.226593	103824.587217	35.205466
1142.119179	104013.983707	35.210484
1143.193866	104211.369173	35.215501
1144.515994	104399.735960	35.220519
1145.646074	104587.743358	35.225536
1147.038543	104777.101686	35.230554
1148.347176	104964.651562	35.235572
1149.124125	105156.786995	35.240589
1150.365853	105340.120587	35.245607
1151.672725	105528.941264	35.250624
1152.352833	105718.462524	35.255642
1153.583749	105912.769872	35.260660
1155.009336	106086.363927	35.265677
1156.622756	106254.899809	35.270695
1158.370882	106454.166142	35.275712
1159.833267	106622.400111	35.280730
1161.016270	106775.280097	35.285748
1162.035554	106952.480921	35.290765
1162.979874	107108.961477	35.295783
1164.230499	107274.182239	35.300800
1165.894271	107430.849315	35.305818
1167.580664	107589.172803	35.310836
1168.828651	107752.357731	35.315853
1169.780352	107892.350418	35.320871
1170.547820	108044.052644	35.325888
1171.282190	108198.864458	35.330906
1172.200337	108350.290090	35.335924
1172.866642	108508.382895	35.340941
1174.192642	108668.444502	35.345959
1175.021480	108840.204790	35.350976
1175.847457	109007.089976	35.355994
1176.908921	109186.743211	35.361012
1177.743765	109367.220574	35.366029
1179.120818	109536.715646	35.371047
1179.805691	109725.314427	35.376064
1181.197646	109900.952798	35.381082
1182.789606	110088.402929	35.386100
1183.899030	110275.858391	35.391117
1185.596973	110448.244718	35.396135
1186.395126	110625.481006	35.401152
1187.380207	110816.064320	35.406170
1188.512216	111000.531474	35.411188
1189.212564	111204.871063	35.416205
1190.390345	111404.331885	35.421223
1190.937173	111615.097217	35.426240
1192.160449	111827.728156	35.431258
1193.213298	112032.319444	35.436276
1193.900928	112264.944145	35.441293
1194.957552	112490.770067	35.446311
1195.617467	112720.755523	35.451328
1196.899129	112951.513874	35.456346
1198.007132	113189.143988	35.461364
1199.094669	113432.949184	35.466381
1200.686307	113674.329161	35.471399
1201.558651	113919.808581	35.476416
1203.514190	114167.783645	35.481434
1204.563269	114406.916168	35.486452
1205.899457	114639.833176	35.491469
1208.162496	114873.143156	35.496487
1209.891784	115096.420708	35.501504
1211.434886	115301.613451	35.506522
1213.109141	115507.723484	35.511540
1215.060907	115707.770866	35.516557
1216.465617	115898.179984	35.521575
1217.369087	116110.199692	35.526592
1218.498977	116298.718585	35.531610
1219.559728	116493.078432	35.536628
1220.433227	116710.695090	35.541645
1221.709670	116900.954814	35.546663
1223.409279	117102.016773	35.551680
1225.021949	117294.212591	35.556698
1226.590279	117478.814742	35.561716
1227.732173	117678.997632	35.566733
1229.432790	117852.658188	35.571751
1230.508339	118040.513359	35.576768
1231.932961	118215.805732	35.581786
1233.311285	118399.533013	35.586804
1234.659574	118575.790554	35.591821
1235.954962	118743.542983	35.596839
1236.722963	118934.027208	35.601856
1237.705371	119111.070953	35.606874
1238.546781	119299.467317	35.611892
1239.762636	119505.111928	35.616909
1240.625021	119684.840069	35.621927
1241.759899	119885.077399	35.626944
1242.945544	120079.770169	35.631962
1244.316232	120280.275216	35.636980
1245.542663	120486.406511	35.641997
1246.796342	120670.675685	35.647015
1247.915249	120872.252967	35.652032
1249.552994	121061.897180	35.657050
1251.653755	121236.005789	35.662068
1253.132359	121406.391609	35.667085
1254.373573	121551.587251	35.672103
1255.524747	121721.281532	35.677120
1256.694451	121887.932330	35.682138
1257.837729	122051.496358	35.687156
1258.686620	122231.546445	35.692173
1259.648534	122410.438339	35.697191
1260.695800	122588.721533	35.702208
1261.488556	122780.316439	35.707226
1262.804397	122962.422532	35.712244
1263.822741	123159.862679	35.717261
1264.956526	123361.391054	35.722279
1266.313608	123556.597870	35.727296
1267.159816	123767.896974	35.732314
1268.364368	123974.512369	35.737332
1269.053857	124184.547715	35.742349
1270.789004	124391.521537	35.747367
1271.873675	124610.289708	35.752384
1272.697234	124831.738892	35.757402
1273.668382	125057.892532	35.762420
1275.160497	125304.455098	35.767437
1276.165238	125534.991879	35.772455
1277.248000	125771.233469	35.777472
1277.963623	126018.412214	35.782490
1278.975799	126277.013991	35.787508
1280.080615	126536.895373	35.792525
1281.104977	126795.905084	35.797543
1282.441637	127064.472527	35.802560
1283.455996	127335.618033	35.807578
1284.855563	127611.404391	35.812596
1285.574620	127899.321915	35.817613
1287.237872	128180.722634	35.822631
1288.732072	128454.422085	35.827648
1290.141106	128735.996742	35.832666
1291.653526	128995.210074	35.837684
1293.886955	129261.873247	35.842701
1296.277746	129503.909256	35.847719
1298.262230	129748.346847	35.852736
1300.005309	129992.433428	35.857754
1302.174054	130203.924990	35.862772
1303.520837	130426.734493	35.867789
1305.044945	130645.586580	35.872807
1306.749096	130856.690552	35.877824
1307.972114	131063.908068	35.882842
1309.300884	131264.517720	35.887860
1310.963991	131485.583578	35.892877
1312.624570	131670.079778	35.897895
1314.356608	131861.841527	35.902912
1315.064212	132054.737746	35.907930
1316.327934	132261.030898	35.912948
1317.468133	132477.297133	35.917965
1318.499553	132673.971759	35.922983
1319.627757	132883.409889	35.928000
1320.537736	133095.649161	35.933018
1321.668703	133299.321486	35.938036
1322.826250	133520.573943	35.943053
1323.740795	133754.165171	35.948071
1325.302350	133974.998762	35.953088
1326.419420	134197.378152	35.958106
1328.364831	134400.301123	35.963124
1329.631860	134624.864450	35.968141
1330.724739	134841.991034	35.973159
1332.058268	135065.709630	35.978176
1333.491406	135296.005729	35.983194
1334.859160	135508.260864	35.988212
1335.938721	135731.265431	35.993229
1337.049769	135952.706873	35.998247
1338.714093	136174.248217	36.003264
1339.483506	136390.018689	36.008282
1341.094134	136594.037665	36.013300
1342.026347	136815.565243	36.018317
1343.159911	137033.371448	36.023335
1344.490310	137244.756405	36.028352
1345.926284	137461.475606	36.033370
1347.381047	137687.778259	36.038388
1348.223969	137919.978153	36.043405
1349.058673	138134.950302	36.048423
1350.771565	138368.720681	36.053440
1351.446265	138623.154338	36.058458
1353.303704	138858.603145	36.063476
1354.495017	139101.860405	36.068493
1356.086331	139349.833213	36.073511
1357.253143	139593.098053	36.078528
1358.423154	139845.252497	36.083546
1359.896790	140075.485990	36.088564
1361.016547	140332.001490	36.093581
1362.345792	140587.913574	36.098599
1363.643984	140850.451657	36.103616
1364.707347	141136.209851	36.108634
1366.472138	141384.866028	36.113652
1367.886203	141640.328052	36.118669
1368.859637	141913.059590	36.123687
1370.677127	142165.478695	36.128704
1371.731461	142452.162220	36.133722
1372.649163	142715.893410	36.138740
1373.921810	143004.764376	36.143757
1375.285942	143287.446971	36.148775
1376.966705	143559.934567	36.153792
1378.116879	143855.477649	36.158810
1379.283628	144144.058492	36.163828
1380.719330	144423.910419	36.168845
1382.071132	144722.166444	36.173863
1384.047669	145011.609197	36.178880
1385.069697	145307.997222	36.183898
1386.644942	145600.174416	36.188916
1387.917306	145882.449014	36.193933
1389.681961	146181.739370	36.198951
1391.415345	146471.703451	36.203968
1392.558232	146768.844382	36.208986
1394.220047	147032.788499	36.214004
1396.204502	147318.431142	36.219021
1398.474641	147582.341785	36.224039
1400.178886	147836.354393	36.229056
1402.019071	148089.090650	36.234074
1403.950123	148337.818551	36.239092
1405.492871	148590.696360	36.244109
1406.366031	148828.277325	36.249127
1407.870309	149075.191232	36.254144
1409.165539	149331.057582	36.259162
1410.541905	149583.360983	36.264180
1412.273741	149834.389570	36.269197
1413.064127	150088.049186	36.274215
1414.569597	150339.283585	36.279232
1415.643956	150600.801296	36.284250
1416.880751	150852.603703	36.289268
1418.101473	151113.847041	36.294285
1419.543586	151379.203035	36.299303
1420.868061	151642.855407	36.304320
1421.861383	151921.594879	36.309338
1423.612620	152189.188376	36.314356
1424.599060	152464.901503	36.319373
1425.930041	152738.999342	36.324391
1427.325849	153012.263918	36.329408
1429.163463	153289.401998	36.334426
1430.805439	153551.048818	36.339444
1432.026115	153817.523946	36.344461
1433.551601	154073.574395	36.349479
1435.584260	154306.735459	36.354496
1436.824868	154558.967531	36.359514
1438.539827	154804.653335	36.364532
1439.873751	155045.266488	36.369549
1440.891405	155289.840526	36.374567
1442.128781	155543.588989	36.379584
1443.073555	155806.609685	36.384602
1444.439444	156072.314997	36.389620
1446.251903	156335.791548	36.394637
1447.163597	156609.237685	36.399655
1448.338008	156888.946815	36.404672
1449.824831	157164.178847	36.409690
1450.956123	157453.134159	36.414708
1452.144669	157735.561591	36.419725
1453.369864	158039.550831	36.424743
1454.764924	158324.396512	36.429760
1455.877756	158623.321720	36.434778
1457.493871	158921.645551	36.439796
1459.314971	159224.225516	36.444813
1460.618924	159534.797029	36.449831
1462.394024	159830.056426	36.454848
1464.333365	160134.234682	36.459866
1465.721694	160430.729674	36.464884
1467.714450	160715.949630	36.469901
1469.286300	161017.226638	36.474919
1471.115254	161303.315115	36.479936
1472.806614	161606.327354	36.484954
1474.475923	161863.849813	36.489972
1477.329257	162115.734784	36.494989
1480.333251	162349.567839	36.500007
1482.220569	162578.905754	36.505024
1484.463114	162808.718885	36.510042
1486.486716	163031.515395	36.515060
1487.976543	163246.979431	36.520077
1489.138188	163465.442466	36.525095
1490.405238	163684.422022	36.530112
1491.346011	163904.382991	36.535130
1492.672078	164139.493743	36.540148
1493.502772	164370.551703	36.545165
1494.264420	164617.494818	36.550183
1495.311018	164869.733707	36.555200
1496.400772	165140.034591	36.560218
1497.521148	165398.405305	36.565236
1498.254907	165675.112561	36.570253
1499.326720	165968.539347	36.575271
1500.915650	166258.837169	36.580288
1501.594054	166553.754180	36.585306
1502.817850	166853.861145	36.590324
1504.348416	167163.423019	36.595341
1505.754051	167472.360642	36.600359
1508.130066	167773.310576	36.605376
1509.491097	168072.222959	36.610394
1511.292121	168369.668608	36.615412
1512.842756	168675.786250	36.620429
1514.234118	168970.816743	36.625447
1515.658436	169271.756842	36.630464
1517.205081	169576.764590	36.635482
1518.428028	169889.454330	36.640500
1520.021591	170197.554641	36.645517
1521.562349	170515.893513	36.650535
1522.800152	170831.594617	36.655552
1524.365772	171151.507259	36.660570
1525.567234	171478.614126	36.665588
1527.115053	171788.115800	36.670605
1528.240733	172124.135338	36.675623
1529.623338	172447.450036	36.680640
1531.113533	172788.261478	36.685658
1532.665041	173100.461481	36.690676
1534.434582	173406.853310	36.695693
1535.755278	173723.334222	36.700711
1537.671730	174030.505193	36.705728
1539.164053	174341.796724	36.710746
1540.478106	174665.759674	36.715764
1541.896161	174977.562550	36.720781
1543.258833	175304.859366	36.725799
1545.099907	175619.870454	36.730816
1546.372780	175954.179176	36.735834
1548.015125	176277.298882	36.740852
1549.902754	176606.700220	36.745869
1551.190015	176927.471729	36.750887
1553.115247	177254.028303	36.755904
1555.135543	177574.606313	36.760922
1556.934417	177884.536883	36.765940
1558.999984	178200.149030	36.770957
1560.831061	178513.098713	36.775975
1562.720299	178814.846625	36.780992
1564.064683	179125.570879	36.786010
1565.060359	179448.945130	36.791028
1567.133577	179741.491822	36.796045
1568.712100	180066.867505	36.801063
1570.479251	180383.139139	36.806080
1571.428591	180700.424029	36.811098
1572.469801	181030.095921	36.816116
1574.145833	181362.812343	36.821133
1575.347530	181701.003767	36.826151
1576.914067	182042.474995	36.831168
1578.072553	182394.792038	36.836186
1579.681318	182744.282466	36.841204
1581.444484	183088.939042	36.846221
1582.732955	183443.602285	36.851239
1585.144444	183765.016747	36.856256
1587.702228	184088.693596	36.861274
1590.134227	184401.731082	36.866292
1592.532003	184697.894221	36.871309
1594.570900	185006.748145	36.876327
1596.174230	185312.159977	36.881344
1597.511975	185614.672672	36.886362
1598.607766	185922.545642	36.891380
1600.919257	186220.470226	36.896397
1602.564469	186514.406837	36.901415
1603.899198	186801.529229	36.906432
1605.367467	187105.729270	36.911450
1606.999554	187411.350869	36.916468
1608.487668	187706.868341	36.921485
1609.659498	188030.861273	36.926503
1611.210547	188338.151450	36.931520
1612.000666	188662.579328	36.936538
1613.011628	189003.043082	36.941556
1614.485815	189324.784364	36.946573
1615.412814	189673.148988	36.951591
1616.672868	190023.377299	36.956608
1618.052890	190384.860380	36.961626
1619.258828	190750.373258	36.966644
1621.261910	191104.788179	36.971661
1622.760691	191467.121339	36.976679
1624.045944	191847.391534	36.981696
1625.425390	192222.964133	36.986714
1626.763682	192611.684996	36.991732
1628.501424	192987.037849	36.996749
1629.956328	193379.844673	37.001767
1631.981696	193750.558888	37.006784
1634.694736	194119.955277	37.011802
1637.311015	194475.836793	37.016820
1638.976339	194817.430721	37.021837
1641.233519	195171.649108	37.026855
1643.033374	195485.472315	37.031872
1645.008861	195805.958450	37.036890
1646.732007	196124.545587	37.041908
1648.235637	196432.925334	37.046925
1649.536344	196759.482251	37.051943
1651.144081	197071.745317	37.056960
1652.875027	197392.292471	37.061978
1653.830622	197721.145807	37.066996
1655.691943	198052.973829	37.072013
1656.847601	198379.105710	37.077031
1658.426837	198706.743267	37.082048
1660.462206	199039.880385	37.087066
1662.248619	199382.595200	37.092084
1664.149744	199702.756952	37.097101
1665.429062	200052.262753	37.102119
1667.045140	200378.772232	37.107136
1668.842777	200731.217264	37.112154
1670.345815	201073.454161	37.117172
1672.160867	201417.786715	37.122189
1673.355464	201775.339342	37.127207
1675.164065	202140.359189	37.132224
1676.537243	202489.836111	37.137242
1677.986213	202862.626121	37.142260
1679.745455	203217.299022	37.147277
1681.250860	203590.540480	37.152295
1682.669144	203967.569264	37.157312
1684.536078	204340.551432	37.162330
1685.990645	204714.517998	37.167348
1687.997275	205084.877811	37.172365
1689.506128	205475.066102	37.177383
1691.435700	205850.572089	37.182400
1693.141916	206228.694490	37.187418
1694.833400	206611.823954	37.192436
1696.648819	206986.554433	37.197453
1698.769860	207367.851456	37.202471
1701.151516	207730.365491	37.207488
1703.586509	208080.352467	37.212506
1705.183434	208444.587005	37.217524
1707.272373	208805.795761	37.222541
1708.319265	209173.476935	37.227559
1709.875057	209533.977309	37.232576
1711.977457	209906.096144	37.237594
1713.080372	210279.461619	37.242612
1714.268478	210657.258946	37.247629
1715.885383	211036.967796	37.252647
1717.702976	211426.067102	37.257664
1719.956016	211792.163047	37.262682
1721.605088	212167.427193	37.267700
1723.933785	212523.812215	37.272717
1725.635774	212896.658035	37.277735
1727.376211	213276.584766	37.282752
1729.137026	213640.585855	37.287770
1730.523783	214026.491859	37.292788
1732.370458	214401.732669	37.297805
1733.867248	214772.537687	37.302823
1735.983598	215153.857606	37.307840
1737.500575	215527.633783	37.312858
1738.695499	215888.639055	37.317876
1740.904013	216273.834066	37.322893
1742.999280	216641.448755	37.327911
1744.992080	217022.720470	37.332928
1747.090831	217378.832153	37.337946
1748.649199	217751.010046	37.342964
1750.408491	218109.720427	37.347981
1752.102736	218475.884552	37.352999
1753.971382	218837.449408	37.358016
1755.214786	219242.017072	37.363034
1756.652631	219645.157184	37.368052
1758.246575	220001.564960	37.373069
1759.740767	220353.266323	37.378087
1760.990591	220728.604806	37.383104
1763.089296	221091.841068	37.388122
1764.793801	221453.797736	37.393140
1766.485528	221823.199638	37.398157
1768.209753	222186.552406	37.403175
1769.836188	222570.114928	37.408192
1771.554617	222942.132241	37.413210
1772.784432	223329.191970	37.418228
1774.499259	223706.038249	37.423245
1776.035745	224118.119064	37.428263
1777.288699	224515.999119	37.433280
1778.532144	224919.317622	37.438298
1780.027629	225352.643672	37.443316
1781.548882	225774.308446	37.448333
1782.907416	226213.654611	37.453351
1784.521016	226658.268667	37.458368
1786.556506	227101.747564	37.463386
1787.880405	227556.623622	37.468404
1790.204635	228008.643066	37.473421
1792.639086	228443.932317	37.478439
1794.485552	228891.944467	37.483456
1796.965151	229317.170457	37.488474
1798.723075	229766.139959	37.493492
1800.673715	230201.387967	37.498509
1802.564258	230653.869020	37.503527
1804.163712	231103.758031	37.508544
1806.128775	231543.783061	37.513562
1807.901473	232007.845256	37.518580
1809.386839	232446.225141	37.523597
1811.280847	232902.090784	37.528615
1813.029124	233351.275964	37.533632
1815.334326	233804.129519	37.538650
1817.421392	234250.822538	37.543668
1819.469370	234704.559449	37.548685
1821.102995	235142.896699	37.553703
1823.466306	235600.368576	37.558720
1826.714719	236003.564019	37.563738
1829.536423	236416.382134	37.568756
1832.369637	236795.643527	37.573773
1835.058042	237178.587560	37.578791
1837.253029	237565.653034	37.583808
1839.301963	237938.467605	37.588826
1840.853654	238322.669165	37.593844
1842.114196	238682.279743	37.598861
1843.903373	239057.628860	37.603879
1845.455048	239446.379531	37.608896
1847.097301	239818.807722	37.613914
1848.405016	240215.246279	37.618932
1849.809504	240605.166542	37.623949
1851.562196	241005.724160	37.628967
1852.614748	241419.887138	37.633984
1854.220542	241830.885490	37.639002
1855.350954	242264.266657	37.644020
1857.070285	242684.392522	37.649037
1858.803932	243112.340694	37.654055
1860.229915	243551.822512	37.659072
1861.865732	243998.687848	37.664090
1863.666570	244444.942310	37.669108
1865.217922	244894.922205	37.674125
1867.192451	245354.536519	37.679143
1868.651096	245823.254994	37.684160
1870.353472	246279.410205	37.689178
1872.310396	246746.574119	37.694196
1874.497413	247199.830591	37.699213
1877.535444	247641.058090	37.704231
1879.317243	248083.586595	37.709248
1881.105035	248517.020366	37.714266
1882.816309	248945.259680	37.719284
1884.267535	249388.962158	37.724301
1886.190398	249817.726172	37.729319
1887.490504	250268.110173	37.734336
1889.003543	250705.808584	37.739354
1890.198136	251171.173324	37.744372
1891.993443	251638.877645	37.749389
1894.025477	252108.270548	37.754407
1895.258776	252596.619907	37.759424
1897.526974	253053.704662	37.764442
1899.720692	253538.669376	37.769460
1901.553325	254014.625273	37.774477
1903.688598	254501.251466	37.779495
1905.938350	254977.418213	37.784512
1907.983518	255451.281974	37.789530
1909.954167	255929.883279	37.794548
1912.904314	256398.262772	37.799565
1916.137232	256846.349135	37.804583
1917.955618	257297.845367	37.809600
1920.496756	257747.189673	37.814618
1922.595132	258181.619447	37.819636
1924.892402	258631.766348	37.824653
1926.876536	259063.395332	37.829671
1928.280149	259516.992723	37.834688
1930.029934	259949.346385	37.839706
1931.307534	260417.876303	37.844724
1932.880425	260876.932599	37.849741
1934.703703	261343.238051	37.854759
1936.333628	261819.965345	37.859776
1938.155598	262287.998149	37.864794
1939.819576	262773.432768	37.869812
1941.778601	263259.834414	37.874829
1944.287517	263710.529387	37.879847
1946.412000	264196.395047	37.884864
1948.507633	264652.391026	37.889882
1952.711194	265083.320206	37.894900
1957.573897	265461.885607	37.899917
1960.492694	265865.871129	37.904935
1962.487544	266241.253096	37.909952
1964.920975	266611.252904	37.914970
1967.180939	266992.636374	37.919988
1968.880115	267342.384019	37.925005
1971.488955	267698.128254	37.930023
1972.851851	268062.537833	37.935040
1974.921095	268408.362108	37.940058
1976.666254	268764.705827	37.945076
1978.261692	269135.045676	37.950093
1979.676231	269486.235925	37.955111
1981.371747	269853.814999	37.960128
1983.255187	270218.720679	37.965146
1985.151463	270600.694594	37.970164
1986.553440	270981.505236	37.975181
1988.641746	271344.902437	37.980199
1990.279425	271733.243213	37.985216
1991.970796	272126.680574	37.990234
1993.546741	272516.478563	37.995252
1994.875782	272932.405505	38.000269
1996.192724	273341.652961	38.005287
1997.649750	273773.586552	38.010304
1999.233184	274199.630530	38.015322
2000.593638	274649.258908	38.020340
2001.774676	275100.745206	38.025357
2003.085427	275571.464253	38.030375
2003.970555	276053.633169	38.035392
2005.885631	276553.589940	38.040410
2007.326969	277044.911128	38.045428
2008.927206	277563.385292	38.050445
2010.845717	278055.971515	38.055463
2012.238744	278580.193048	38.060480
2014.015470	279089.921345	38.065498
2015.975430	279602.945663	38.070516
2017.466511	280144.242419	38.075533
2019.566791	280669.052564	38.080551
2021.526952	281220.048254	38.085568
2022.827778	281757.790222	38.090586
2024.919114	282315.619296	38.095604
2026.507513	282883.588893	38.100621
2029.411998	283446.563124	38.105639
2031.519699	284023.485760	38.110656
2033.677386	284590.313776	38.115674
2036.228489	285165.787200	38.120692
2037.857900	285739.277477	38.125709
2040.510919	286301.089405	38.130727
2042.892683	286877.371837	38.135744
2045.111119	287446.998648	38.140762
2047.449542	288014.469662	38.145780
2049.331544	288585.671661	38.150797
2051.834185	289158.876725	38.155815
2053.744809	289741.346938	38.160832
2055.920573	290311.908765	38.165850
2058.182544	290888.956240	38.170868
2059.885312	291465.941331	38.175885
2062.516340	292041.906418	38.180903
2064.752954	292608.155234	38.185920
2067.906990	293156.825289	38.190938
2071.124172	293708.352506	38.195956
2072.874659	294268.781263	38.200973
2075.814608	294800.283693	38.205991
2078.086789	295320.159827	38.211008
2080.474451	295854.517281	38.216026
2083.329447	296370.888503	38.221044
2085.334993	296908.758368	38.226061
2087.304814	297421.486765	38.231079
2089.396165	297937.494366	38.236096
2091.177309	298465.462665	38.241114
2093.367879	298982.693164	38.246132
2094.733296	299512.274225	38.251149
2096.872607	300028.339555	38.256167
2098.709405	300565.405575	38.261184
2102.116936	301065.407139	38.266202
2104.757748	301576.149320	38.271220
2106.707870	302093.352544	38.276237
2108.887539	302604.495745	38.281255
2111.133832	303110.317097	38.286272
2113.142265	303612.873453	38.291290
2114.928858	304125.444781	38.296308
2116.490289	304644.145720	38.301325
2118.449859	305158.053930	38.306343
2120.562515	305685.190763	38.311360
2122.472267	306212.307223	38.316378
2124.452324	306740.577044	38.321396
2125.850375	307289.993286	38.326413
2127.958609	307821.104901	38.331431
2130.157939	308367.435463	38.336448
2132.610703	308906.609689	38.341466
2134.875815	309449.493758	38.346484
2136.784895	309987.049364	38.351501
2139.031086	310533.306800	38.356519
2140.640710	311080.986419	38.361536
2142.884863	311640.670364	38.366554
2144.966524	312178.817271	38.371572
2147.543995	312728.127955	38.376589
2150.176077	313265.566569	38.381607
2152.624550	313793.509021	38.386624
2154.693489	314333.293276	38.391642
2156.824713	314845.282704	38.396660
2158.497973	315370.421975	38.401677
2160.627289	315862.369170	38.406695
2162.616622	316384.122189	38.411712
2164.704282	316897.627812	38.416730
2167.071070	317397.219072	38.421748
2169.828815	317909.209713	38.426765
2172.327052	318405.013870	38.431783
2174.749495	318910.958442	38.436800
2176.561151	319416.721087	38.441818
2178.619015	319927.898385	38.446836
2179.985725	320463.358956	38.451853
2182.037614	320982.984515	38.456871
2184.734593	321507.551967	38.461888
2186.882510	322020.678652	38.466906
2189.061075	322545.653647	38.471924
2191.398028	323078.926193	38.476941
2193.791359	323594.792590	38.481959
2195.799314	324128.542414	38.486976
2197.954198	324661.780945	38.491994
2200.316334	325190.435828	38.497012
2201.996626	325741.643318	38.502029
2203.920265	326280.999567	38.507047
2205.892488	326834.027610	38.512064
2207.847210	327399.620869	38.517082
2209.935974	327963.510921	38.522100
2211.951965	328536.191966	38.527117
2214.028518	329117.793947	38.532135
2215.746662	329714.453591	38.537152
2217.414218	330309.465250	38.542170
2219.494967	330912.957768	38.547188
2221.087618	331538.281249	38.552205
2222.984880	332155.702867	38.557223
2225.215024	332800.378196	38.562240
2226.867308	333432.880238	38.567258
2229.237183	334083.533865	38.572276
2231.039502	334732.928244	38.577293
2233.224478	335389.410018	38.582311
2235.504135	336067.445098	38.587328
2237.197108	336750.696287	38.592346
2240.233325	337408.078179	38.597364
2242.851086	338087.985704	38.602381
2245.977458	338731.679359	38.607399
2248.708561	339384.695203	38.612416
2251.488269	340037.415369	38.617434
2254.223417	340686.200149	38.622452
2256.361456	341335.659145	38.627469
2258.788469	341972.142414	38.632487
2261.495822	342617.226102	38.637504
2263.965424	343247.822584	38.642522
2266.392993	343887.301091	38.647540
2268.674782	344512.404469	38.652557
2270.956973	345131.915938	38.657575
2273.166580	345767.242943	38.662592
2275.536136	346401.900375	38.667610
2277.899195	347024.190596	38.672628
2279.556535	347665.851801	38.677645
2281.735399	348303.509411	38.682663
2284.165156	348948.552339	38.687680
2286.715521	349586.460344	38.692698
2289.523552	350210.384461	38.697716
2291.512704	350846.464139	38.702733
2293.470759	351468.608063	38.707751
2295.964323	352107.529758	38.712768
2298.225663	352742.750307	38.717786
2300.313993	353372.432967	38.722804
2302.209320	354020.002504	38.727821
2304.310031	354655.805103	38.732839
2306.277288	355270.838663	38.737856
2308.466869	355896.153700	38.742874
2310.833213	356518.867424	38.747892
2312.684095	357139.246739	38.752909
2314.646971	357770.635440	38.757927
2317.160875	358413.239370	38.762944
2318.695422	359064.063685	38.767962
2320.795153	359712.652792	38.772980
2322.748519	360383.100384	38.777997
2324.890408	361049.852165	38.783015
2327.212327	361721.510223	38.788032
2329.515465	362401.100805	38.793050
2332.364617	363085.231877	38.798068
2334.960959	363762.314854	38.803085
2338.054338	364416.142156	38.808103
2341.602057	365059.127028	38.813120
2344.233211	365719.249292	38.818138
2347.059175	366351.119357	38.823156
2350.024690	366995.284119	38.828173
2352.472197	367630.391677	38.833191
2355.099304	368270.633410	38.838208
2356.973749	368919.080377	38.843226
2358.984707	369556.535618	38.848244
2361.287755	370201.312603	38.853261
2364.203104	370840.066970	38.858279
2366.458840	371489.318498	38.863296
2368.730623	372140.153605	38.868314
2371.221205	372778.741130	38.873332
2373.597208	373422.231174	38.878349
2375.708244	374068.974410	38.883367
2377.955111	374724.204809	38.888384
2379.959685	375390.393725	38.893402
2382.416720	376053.958977	38.898420
2385.013062	376715.764003	38.903437
2387.799621	377373.949150	38.908455
2390.339964	378027.394925	38.913472
2392.510321	378694.659192	38.918490
2394.784536	379361.056340	38.923508
2397.100564	380032.403516	38.928525
2399.403619	380706.427275	38.933543
2401.638550	381385.114328	38.938560
2403.617812	382063.069153	38.943578
2405.825750	382762.169461	38.948596
2407.843691	383456.975987	38.953613
2409.791772	384158.092561	38.958631
2412.309679	384863.207006	38.963648
2414.576727	385576.764896	38.968666
2416.794691	386293.915148	38.973684
2419.404198	387007.536574	38.978701
2421.935075	387736.087092	38.983719
2424.409114	388465.365381	38.988736
2426.660865	389189.010366	38.993754
2429.840786	389907.212153	38.998772
2431.970358	390624.988149	39.003789
2434.777234	391344.967418	39.008807
2437.451130	392057.043199	39.013824
2439.719660	392772.084435	39.018842
2442.734799	393497.884419	39.023860
2444.846206	394207.873724	39.028877
2447.464574	394932.564224	39.033895
2450.407520	395630.013476	39.038912
2452.514679	396349.938555	39.043930
2455.080645	397051.319815	39.048948
2457.213212	397768.899755	39.053965
2459.845169	398479.587606	39.058983
2462.492887	399185.136404	39.064000
2464.367518	399917.353772	39.069018
2466.436761	400630.920204	39.074036
2468.789985	401335.882242	39.079053
2471.313973	402034.438370	39.084071
2474.239140	402728.172524	39.089088
2476.038649	403405.758099	39.094106
2478.564005	404106.163124	39.099124
2480.972865	404805.860454	39.104141
2483.814260	405502.630926	39.109159
2486.243864	406202.796344	39.114176
2488.644830	406906.419626	39.119194
2491.829766	407585.320677	39.124212
2494.722843	408283.076184	39.129229
2497.396999	408978.367357	39.134247
2499.610045	409669.613109	39.139264
2501.757897	410381.624029	39.144282
2504.635597	411081.817557	39.149300
2507.654587	411775.813996	39.154317
2510.160499	412468.180108	39.159335
2512.788777	413171.044771	39.164352
2515.056049	413873.545146	39.169370
2517.554625	414580.142154	39.174388
2519.436722	415282.719042	39.179405
2521.812970	416014.345855	39.184423
2525.003667	416704.409573	39.189440
2527.675484	417431.869764	39.194458
2530.675708	418137.273408	39.199476
2533.425241	418843.661301	39.204493
2536.119439	419543.682618	39.209511
2539.154237	420244.666363	39.214528
2541.479217	420957.978321	39.219546
2544.143859	421666.883876	39.224564
2546.202265	422374.046545	39.229581
2548.276388	423112.177309	39.234599
2550.728129	423837.716144	39.239616
2553.215299	424565.911388	39.244634
2555.157099	425299.036095	39.249652
2558.116198	426027.717242	39.254669
2560.414623	426771.421992	39.259687
2563.078701	427508.512117	39.264704
2565.649950	428265.542395	39.269722
2568.227235	429011.561817	39.274740
2570.599785	429768.222944	39.279757
2572.843880	430538.144430	39.284775
2575.270829	431302.340948	39.289792
2577.226140	432088.357154	39.294810
2579.614218	432870.985162	39.299828
2581.997062	433659.104908	39.304845
2584.216400	434466.762132	39.309863
2586.851202	435262.276487	39.314880
2589.202375	436073.195968	39.319898
2592.279052	436873.591728	39.324916
2594.772913	437679.926237	39.329933
2597.573582	438484.511278	39.334951
2600.280273	439301.379875	39.339968
2602.480154	440113.040003	39.344986
2605.815660	440923.167108	39.350004
2608.122479	441733.637316	39.355021
2610.898657	442565.807220	39.360039
2615.794652	443327.066133	39.365056
2620.550348	444076.938434	39.370074
2623.258894	444826.010740	39.375092
2625.862117	445578.565352	39.380109
2627.681572	446324.596549	39.385127
2630.332637	447083.414330	39.390144
2632.443430	447840.018440	39.395162
2634.768741	448603.034844	39.400180
2637.355002	449369.824871	39.405197
2639.051780	450137.139021	39.410215
2641.278868	450911.165441	39.415232
2643.142308	451665.398219	39.420250
2645.476815	452431.764619	39.425268
2647.448630	453196.696353	39.430285
2649.665889	453980.826274	39.435303
2652.000550	454765.261066	39.440320
2653.766821	455561.238452	39.445338
2656.288160	456382.645182	39.450356
2658.729926	457191.695119	39.455373
2661.101207	458021.049471	39.460391
2663.543310	458852.380498	39.465408
2665.896318	459698.555286	39.470426
2667.932475	460564.058164	39.475444
2670.811561	461427.968746	39.480461
2673.023215	462310.048730	39.485479
2675.776164	463200.036823	39.490496
2678.510930	464120.415321	39.495514
2681.005228	465014.761623	39.500532
2683.867676	465917.749474	39.505549
2686.422414	466833.633339	39.510567
2689.184927	467756.817651	39.515584
2692.339399	468666.047199	39.520602
2695.179957	469581.702983	39.525620
2698.798436	470483.998637	39.530637
2701.575606	471405.438676	39.535655
2704.449241	472314.490546	39.540672
2707.209152	473237.663109	39.545690
2709.429276	474167.446964	39.550708
2712.351038	475103.382958	39.555725
2714.477377	476033.140044	39.560743
2717.323132	476956.064239	39.565760
2720.609343	477891.849878	39.570778
2723.462803	478834.376666	39.575796
2726.210386	479765.357992	39.580813
2729.232289	480697.761414	39.585831
2733.550928	481598.089274	39.590848
2737.549038	482506.403477	39.595866
2740.814573	483381.821747	39.600884
2744.288538	484257.061831	39.605901
2747.493709	485143.562142	39.610919
2750.361121	486006.245416	39.615936
2753.516502	486864.951932	39.620954
2755.758093	487725.080342	39.625972
2758.252839	488590.576366	39.630989
2760.914951	489464.027444	39.636007
2762.820335	490330.897672	39.641024
2764.938271	491224.993633	39.646042
2766.740716	492121.972261	39.651060
2769.123307	493022.542646	39.656077
2771.292906	493961.098728	39.661095
2773.454655	494883.760546	39.666112
2775.606237	495838.565113	39.671130
2777.652225	496795.553385	39.676148
2780.512443	497764.561762	39.681165
2782.542436	498744.296101	39.686183
2784.856030	499741.783584	39.691200
2788.121651	500729.772737	39.696218
2791.125027	501727.884639	39.701236
2794.029437	502718.488275	39.706253
2797.294902	503724.707492	39.711271
2800.205830	504715.038453	39.716288
2803.275838	505718.040877	39.721306
2805.750917	506715.987161	39.726324
2809.202633	507719.004506	39.731341
2812.107136	508706.521650	39.736359
2814.974475	509698.622307	39.741376
2818.324794	510681.205195	39.746394
2820.714109	511676.740368	39.751412
2824.024525	512650.034063	39.756429
2826.967033	513598.128066	39.761447
2829.574497	514537.602309	39.766464
2832.820182	515485.885069	39.771482
2835.023510	516440.984867	39.776500
2838.115137	517389.479723	39.781517
2840.907095	518334.691046	39.786535
2843.651357	519279.852431	39.791552
2846.206858	520234.105741	39.796570
2848.097905	521202.515033	39.801588
2851.346840	522162.931193	39.806605
2854.008247	523142.121627	39.811623
2856.869881	524125.496874	39.816640
2859.936126	525107.565503	39.821658
2862.392424	526105.383314	39.826676
2865.301886	527093.693333	39.831693
2867.882458	528101.680557	39.836711
2870.991438	529095.867151	39.841728
2874.227311	530101.394727	39.846746
2877.224809	531114.041938	39.851764
2880.502425	532113.585357	39.856781
2883.164878	533132.139091	39.861799
2885.800104	534139.049638	39.866816
2888.965069	535154.862059	39.871834
2891.615286	536187.044190	39.876852
2894.773057	537195.014466	39.881869
2898.003966	538230.828729	39.886887
2900.979325	539242.207491	39.891904
2904.728966	540255.700730	39.896922
2907.880162	541276.213375	39.901940
2910.469130	542292.570128	39.906957
2913.261275	543326.576059	39.911975
2915.650076	544349.658132	39.916992
2918.013856	545397.111953	39.922010
2920.199164	546453.317169	39.927028
2923.377878	547512.294831	39.932045
2925.378548	548590.392619	39.937063
2928.219110	549681.540367	39.942080
2930.848927	550786.260276	39.947098
2933.319382	551889.409142	39.952116
2936.056589	552992.374208	39.957133
2938.961591	554109.445679	39.962151
2941.752078	555225.237498	39.967168
2945.361667	556352.208640	39.972186
2948.396757	557488.576426	39.977204
2951.997977	558602.244364	39.982221
2955.068041	559725.251443	39.987239
2957.696329	560854.566006	39.992256
2960.974914	561987.192486	39.997274
2963.804276	563113.567409	40.002292
2966.942993	564240.798634	40.007309
2970.253132	565367.803548	40.012327
2974.262190	566474.509373	40.017344
2978.789454	567552.214281	40.022362
2982.474789	568635.992912	40.027380
2985.811365	569709.094973	40.032397
2989.567413	570776.817082	40.037415
2992.825129	571825.207761	40.042432
2995.795985	572880.786511	40.047450
2998.456549	573932.012608	40.052468
3001.106236	574979.539844	40.057485
3004.016897	576030.950688	40.062503
3006.624228	577082.674590	40.067520
3009.820309	578131.051879	40.072538
3012.094268	579192.836783	40.077556
3015.019000	580254.774184	40.082573
3017.970870	581313.155039	40.087591
3021.106345	582379.839785	40.092608
3024.013498	583426.561346	40.097626
3026.916194	584459.053869	40.102644
3029.806311	585456.213901	40.107661
3032.898498	586481.233278	40.112679
3036.320379	587478.941000	40.117696
3040.034642	588477.520295	40.122714
3043.080104	589485.299386	40.127732
3045.775752	590486.185482	40.132749
3048.467713	591497.612216	40.137767
3050.713583	592530.874091	40.142784
3054.174775	593552.922295	40.147802
3057.531380	594579.959506	40.152820
3060.500855	595611.680183	40.157837
3063.184487	596647.715418	40.162855
3065.945073	597695.065984	40.167872
3068.842533	598749.411557	40.172890
3071.606375	599807.589682	40.177908
3074.461461	600868.259912	40.182925
3076.998276	601957.674598	40.187943
3079.675931	603049.215783	40.192960
3083.361803	604133.027697	40.197978
3085.950522	605245.799351	40.202996
3088.746706	606350.620442	40.208013
3091.916911	607474.689291	40.213031
3094.678711	608598.063533	40.218048
3098.001128	609733.641628	40.223066
3100.739945	610876.305594	40.228084
3103.732527	612025.114038	40.233101
3106.653989	613179.568148	40.238119
3109.860193	614350.209711	40.243136
3113.125259	615516.167183	40.248154
3116.142946	616700.243438	40.253172
3119.314759	617871.917506	40.258189
3122.554530	619049.304219	40.263207
3125.359282	620238.782732	40.268224
3128.503204	621430.674271	40.273242
3131.439273	622643.558897	40.278260
3134.893769	623847.427085	40.283277
3138.198503	625064.126235	40.288295
3141.200287	626272.894100	40.293312
3144.718882	627477.094040	40.298330
3147.470059	628693.172255	40.303348
3150.813890	629911.510349	40.308365
3154.035011	631130.877009	40.313383
3157.469114	632364.297491	40.318400
3160.555821	633582.903064	40.323418
3163.631609	634808.107601	40.328436
3167.669600	636025.372622	40.333453
3171.312824	637217.956453	40.338471
3174.652301	638432.958513	40.343488
3178.472512	639641.750755	40.348506
3181.736558	640837.721343	40.353524
3184.964226	642026.275524	40.358541
3188.783941	643216.139826	40.363559
3192.199787	644408.325742	40.368576
3195.538528	645585.324931	40.373594
3198.170419	646776.863205	40.378612
3201.174953	647970.492412	40.383629
3204.075672	649165.990978	40.388647
3206.901826	650367.739023	40.393664
3209.868714	651557.358495	40.398682
3212.541812	652777.380408	40.403700
3216.062918	653972.449188	40.408717
3219.629448	655187.492447	40.413735
3223.262962	656389.523323	40.418752
3227.017480	657569.771316	40.423770
3229.648778	658787.113680	40.428788
3233.000058	659986.060305	40.433805
3236.039795	661168.381164	40.438823
3238.353718	662347.242869	40.443840
3240.864450	663526.625079	40.448858
3244.006821	664699.736381	40.453876
3247.187042	665892.105684	40.458893
3250.229031	667084.050715	40.463911
3252.568582	668279.893217	40.468928
3255.516231	669494.636372	40.473946
3257.863683	670723.498328	40.478964
3260.841709	671967.612364	40.483981
3263.870564	673230.001426	40.488999
3266.427790	674505.921299	40.494016
3269.512374	675777.155652	40.499034
3272.699430	677079.065947	40.504052
3275.531245	678383.486419	40.509069
3278.933412	679715.604262	40.514087
3281.917709	681025.887405	40.519104
3285.666417	682346.686732	40.524122
3289.289661	683692.051222	40.529140
3292.616883	685032.697521	40.534157
3296.229136	686376.823145	40.539175
3299.691005	687728.668069	40.544192
3303.560488	689062.373279	40.549210
3307.143862	690400.196469	40.554228
3310.283176	691753.326640	40.559245
3313.823184	693100.281397	40.564263
3317.203018	694470.573646	40.569280
3320.370568	695835.580537	40.574298
3323.753227	697214.376259	40.579316
3327.141513	698569.352524	40.584333
3331.215345	699925.196369	40.589351
3334.757892	701283.495695	40.594368
3338.263445	702634.948243	40.599386
3342.096723	703985.294131	40.604404
3345.889403	705331.670681	40.609421
3350.029647	706676.987236	40.614439
3353.257943	708022.244212	40.619456
3356.678272	709363.346083	40.624474
3359.758658	710706.422984	40.629492
3362.421602	712068.269485	40.634509
3365.654077	713422.972429	40.639527
3368.699241	714793.277668	40.644544
3371.769701	716166.820065	40.649562
3374.491681	717561.866315	40.654580
3377.338678	718956.461784	40.659597
3380.415790	720361.716927	40.664615
3383.993619	721759.382665	40.669632
3388.246648	723161.793869	40.674650
3392.679244	724533.238415	40.679668
3397.068545	725913.605623	40.684685
3400.671913	727297.329837	40.689703
3403.758515	728678.681987	40.694720
3406.970475	730054.246478	40.699738
3410.575121	731425.413643	40.704756
3414.253335	732793.867311	40.709773
3418.040882	734163.305372	40.714791
3421.883833	735518.875656	40.719808
3425.295951	736865.995607	40.724826
3428.677994	738221.431361	40.729844
3432.127627	739589.059851	40.734861
3435.346852	740935.869179	40.739879
3438.547478	742295.375962	40.744896
3441.828608	743663.117917	40.749914
3445.342779	745020.672514	40.754932
3448.196701	746406.350321	40.759949
3451.311256	747770.593400	40.764967
3454.798160	749151.982280	40.769984
3458.085961	750516.454452	40.775002
3461.413434	751888.737863	40.780007
3464.237367	753218.959820	40.785012
3468.177687	754464.435424	40.790016
3472.745783	755653.721507	40.795021
3476.507633	756757.119074	40.800026
3480.191066	757791.966453	40.805031
3483.019232	758772.680896	40.810036
3485.888638	759665.237569	40.815040
3488.407407	760481.572731	40.820045
3490.988230	761242.115057	40.825050
3492.849542	761940.647284	40.830055
3494.710862	762570.063883	40.835060
3497.135848	763144.542018	40.840064
3499.290251	763656.785455	40.845069
3501.179152	764119.627211	40.850074
3503.017340	764524.313134	40.855079
3504.335502	764880.347837	40.860084
3505.586422	765187.268990	40.865088
3507.094332	765449.910083	40.870093
3508.410458	765665.243905	40.875098
3509.799961	765846.394042	40.880103
3510.523098	765982.688552	40.885108
3512.127390	766093.495259	40.890112
3512.443296	766168.377397	40.895117
3513.343079	766212.203006	40.900122
3514.614185	766229.986878	40.905127
3515.154412	766215.502551	40.910132
3515.934998	766174.110793	40.915136
3516.163774	766115.506066	40.920141
3516.698321	766036.243191	40.925146
3517.428373	765933.776124	40.930151
3517.816834	765821.109516	40.935156
3518.057452	765683.568261	40.940160
3518.165499	765535.199776	40.945165
3518.742598	765372.551341	40.950170
3519.086400	765198.055425	40.955175
3519.361946	765010.204740	40.960180
3519.595005	764803.225035	40.965184
3519.921227	764611.657918	40.970189
3519.917134	764385.623314	40.975194
3520.259552	764150.599193	40.980199
3520.073146	763922.558980	40.985204
3520.456524	763662.658824	40.990208
3520.363678	763426.599045	40.995213
3520.544121	763168.540060	41.000218
3520.884408	762903.146443	41.005223
3520.587371	762638.539292	41.010228
3520.597006	762362.675711	41.015232
3520.781624	762081.002042	41.020237
3520.629418	761796.907147	41.025242
3520.906200	761525.309603	41.030247
3520.971502	761232.623594	41.035252
3521.126073	760942.328813	41.040256
3520.954202	760649.215412	41.045261
3520.808147	760343.406839	41.050266
3520.762681	760049.262581	41.055271
3521.053920	759750.215883	41.060276
3521.226668	759448.364445	41.065280
3521.184375	759147.128671	41.070285
3520.828388	758833.546786	41.075290
3520.747932	758512.504122	41.080295
3520.737292	758215.174067	41.085300
3520.442088	757902.135928	41.090304
3520.235987	757592.722441	41.095309
3520.666346	757285.116130	41.100314
3520.737606	756980.468916	41.105319
3520.230769	756664.848282	41.110324
3520.408540	756358.974010	41.115328
3520.220857	756053.295982	41.120333
3520.046812	755738.371918	41.125338
3520.224104	755430.288453	41.130343
3519.716590	755115.048269	41.135348
3520.071801	754796.048345	41.140352
3519.706481	754489.448535	41.145357
3519.761753	754172.496616	41.150362
3519.543485	753873.698814	41.155367
3519.198831	753573.626383	41.160372
3519.604512	753260.677553	41.165376
3519.453264	752959.166487	41.170381
3519.106656	752651.947065	41.175386
3518.800184	752350.783544	41.180391
3518.915585	752054.280023	41.185396
3518.761578	751751.734385	41.190400
3518.299701	751467.503604	41.195405
3518.229558	751164.772940	41.200410
3518.583070	750879.002698	41.205415
3518.477193	750583.121482	41.210420
3518.269810	750292.630510	41.215424
3517.785306	750000.939355	41.220429
3517.659294	749707.844044	41.225434
3517.855826	749422.144844	41.230439
3517.668557	749139.018415	41.235444
3517.799125	748850.196323	41.240448
3517.213979	748575.317290	41.245453
3516.841086	748302.073551	41.250458
3517.028317	748021.661177	41.255463
3516.855137	747749.155695	41.260468
3516.997209	747475.847302	41.265472
3516.916618	747198.414748	41.270477
3517.033030	746928.106113	41.275482
3516.592297	746659.807752	41.280487
3516.076508	746390.425200	41.285492
3516.629247	746114.925431	41.290496
3516.121605	745854.074118	41.295501
3516.032076	745584.642819	41.300506
3516.124203	745324.712828	41.305511
3516.034169	745063.222412	41.310516
3515.934907	744788.970212	41.315520
3515.849756	744540.957729	41.320525
3515.519870	744283.782090	41.325530
3515.616714	744030.730025	41.330535
3515.249859	743766.621803	41.335540
3515.605571	743503.275316	41.340544
3515.261177	743273.955727	41.345549
3515.075457	743007.418699	41.350554
3515.149164	742766.592843	41.355559
3515.158957	742521.171284	41.360564
3514.889248	742267.084683	41.365568
3514.577790	742020.810514	41.370573
3514.944374	741771.647124	41.375578
3514.585917	741534.613723	41.380583
3514.351596	741295.079788	41.385588
3514.624193	741057.532151	41.390592
3514.204460	740823.653012	41.395597
3514.151894	740581.396546	41.400602
3513.984971	740351.616577	41.405607
3513.517882	740125.243219	41.410612
3513.568658	739894.375256	41.415616
3513.638569	739679.525212	41.420621
3513.825501	739442.289653	41.425626
3513.842705	739214.672509	41.430631
3513.283977	738995.059658	41.435636
3513.545964	738767.389270	41.440640
3513.227168	738545.943310	41.445645
3513.134527	738332.122733	41.450650
3512.831452	738108.386081	41.455655
3513.036846	737899.600910	41.460660
3513.298048	737674.422898	41.465664
3512.952970	737469.972811	41.470669
3512.876237	737244.442663	41.475674
3512.658324	737041.049222	41.480679
3512.718133	736829.439509	41.485684
3512.995936	736612.047632	41.490688
3512.478482	736404.926467	41.495693
3512.503880	736203.055159	41.500698
3512.157346	736008.317471	41.505703
3511.948195	735815.136104	41.510708
3511.928988	735601.923262	41.515712
3511.824067	735404.755290	41.520717
3511.699128	735221.939650	41.525722
3511.705233	735023.209584	41.530727
3511.509129	734833.417743	41.535732
3511.808839	734622.947624	41.540736
3511.418263	734444.068662	41.545741
3511.333732	734261.670011	41.550746
3511.524226	734064.370843	41.555751
3510.863894	733875.128136	41.560756
3511.120386	733698.501886	41.565760
3511.138390	733510.772207	41.570765
3510.888773	733311.398550	41.575770
3511.081506	733129.621568	41.580775
3510.736513	732937.779790	41.585780
3510.885968	732761.893380	41.590784
3510.638805	732581.959165	41.595789
3510.486133	732409.531357	41.600794
3510.913757	732236.805922	41.605799
3510.278379	732067.817570	41.610804
3510.494206	731888.880763	41.615808
3509.877637	731718.792647	41.620813
3510.116455	731545.786564	41.625818
3510.227241	731382.503794	41.630823
3510.165123	731212.461983	41.635828
3510.358456	731029.449223	41.640832
3509.733721	730872.715558	41.645837
3510.004931	730706.074640	41.650842
3509.823707	730552.777689	41.655847
3509.673870	730386.496939	41.660852
3509.948022	730214.744309	41.665856
3509.664516	730063.138930	41.670861
3509.380762	729909.301977	41.675866
3509.483344	729750.296729	41.680871
3509.189103	729593.434230	41.685876
3509.525538	729446.024058	41.690880
3509.137291	729278.967557	41.695885
3509.413073	729137.357116	41.700890
3509.506301	728979.477631	41.705895
3509.238689	728817.493759	41.710900
3509.183541	728664.289001	41.715904
3508.969854	728518.439050	41.720909
3508.977853	728371.311411	41.725914
3508.885145	728224.792228	41.730919
3508.756983	728079.812006	41.735924
3509.018456	727928.572248	41.740928
3508.752780	727776.376432	41.745933
3508.373008	727643.121837	41.750938
3508.329159	727498.563253	41.755943
3508.488137	727366.949143	41.760948
3508.446082	727220.651313	41.765952
3508.221497	727088.055659	41.770957
3507.982128	726943.618675	41.775962
3508.005297	726816.229616	41.780967
3508.094407	726683.179191	41.785972
3508.139016	726551.025843	41.790976
3507.707012	726427.124832	41.795981
3507.572060	726291.132089	41.800986
3507.872059	726164.678174	41.805991
3507.642844	726049.211209	41.810996
3507.480409	725923.226408	41.816000
3507.479841	725797.559800	41.821005
3507.620809	725674.642920	41.826010
3507.652456	725551.692712	41.831015
3507.289074	725428.508609	41.836020
3507.595815	725307.491520	41.841024
3507.398392	725184.623234	41.846029
3507.132145	725071.130931	41.851034
3507.513805	724958.570727	41.856039
3507.229504	724831.994638	41.861044
3507.317462	724715.366219	41.866048
3507.239785	724594.996904	41.871053
3506.975662	724473.070673	41.876058
3506.921510	724369.891999	41.881063
3506.936726	724263.032928	41.886068
3507.284450	724134.706113	41.891072
3507.151681	724029.652760	41.896077
3507.036834	723917.011693	41.901082
3507.016668	723795.927301	41.906087
3506.739606	723696.544022	41.911092
3506.688730	723569.810846	41.916096
3506.522968	723467.134996	41.921101
3506.761283	723365.977277	41.926106
3506.979344	723249.851894	41.931111
3506.805844	723136.069784	41.936116
3506.743153	723025.935990	41.941120
3506.393790	722935.329416	41.946125
3506.627968	722827.721603	41.951130
3506.537829	722724.280459	41.956135
3506.279921	722625.228134	41.961140
3506.462693	722514.303379	41.966144
3506.152331	722417.438457	41.971149
3506.319095	722304.679310	41.976154
3506.453951	722214.827596	41.981159
3506.128272	722113.450321	41.986164
3506.131481	722005.870000	41.991168
3505.862809	721922.477138	41.996173
3506.162550	721821.191245	42.001178
3506.280849	721724.792741	42.006183
3505.771828	721636.726814	42.011188
3506.446772	721522.980651	42.016192
3506.217127	721441.113454	42.021197
3506.302146	721334.155442	42.026202
3506.316435	721251.204875	42.031207
3505.725905	721140.538282	42.036212
3506.082330	721030.655788	42.041216
3506.129918	720951.712878	42.046221
3505.624544	720852.581107	42.051226
3505.828506	720766.619370	42.056231
3505.900239	720666.745427	42.061236
3505.850623	720573.980972	42.066240
3505.494619	720490.836085	42.071245
3505.556454	720401.720605	42.076250
3505.275424	720303.140238	42.081255
3505.424863	720225.760375	42.086260
3505.343408	720137.211198	42.091264
3505.574304	720058.378285	42.096269
3505.399407	719975.743791	42.101274
3505.456022	719891.929675	42.106279
3505.152214	719808.620580	42.111284
3505.242238	719726.039010	42.116288
3505.190756	719650.125112	42.121293
3505.177414	719577.080485	42.126298
3504.895000	719495.599584	42.131303
3504.943824	719416.741102	42.136308
3505.006386	719324.241744	42.141312
3504.910284	719250.712013	42.146317
3504.917547	719176.123096	42.151322
3504.919400	719097.666108	42.156327
3504.679751	719036.507010	42.161332
3504.872381	718950.429231	42.166336
3504.941885	718890.457838	42.171341
3504.512557	718813.408492	42.176346
3504.684172	718737.647809	42.181351
3504.769218	718678.912223	42.186356
3504.681773	718593.571398	42.191360
3504.860947	718531.793831	42.196365
3504.833002	718445.003345	42.201370
3504.978253	718379.510448	42.206375
3504.436954	718303.516457	42.211380
3504.752944	718232.389582	42.216384
3504.496455	718172.615708	42.221389
3504.593671	718100.333486	42.226394
3504.392068	718026.860020	42.231399
3504.459207	717960.037551	42.236404
3504.557633	717894.399796	42.241408
3504.660269	717835.754588	42.246413
3504.467267	717771.751265	42.251418
3504.498204	717699.774148	42.256423
3504.322022	717622.027165	42.261428
3504.301478	717551.743764	42.266432
3504.295112	717495.197501	42.271437
3504.100110	717433.572874	42.276442
3504.191740	717368.775385	42.281447
3504.124529	717317.347173	42.286452
3503.973649	717245.941850	42.291456
3503.834552	717191.250841	42.296461
3504.111905	717138.226840	42.301466
3504.258754	717075.203747	42.306471
3503.974384	717021.478144	42.311476
3503.833762	716944.314271	42.316480
3503.767732	716891.097422	42.321485
3503.759562	716829.784730	42.326490
3503.782470	716779.429684	42.331495
3503.563522	716729.957633	42.336500
3503.774097	716663.646816	42.341504
3503.766517	716621.332356	42.346509
3503.486067	716566.561418	42.351514
3503.564400	716516.691724	42.356519
3503.369662	716473.911361	42.361524
3503.884925	716425.655635	42.366528
3503.605037	716368.402840	42.371533
3503.657341	716302.859479	42.376538
3503.945211	716249.877747	42.381543
3503.876999	716201.270661	42.386548
3503.824950	716148.394073	42.391552
3503.882785	716098.277230	42.396557
3503.971811	716038.728716	42.401562
3503.878376	715975.836311	42.406567
3503.265339	715929.302168	42.411572
3503.976459	715866.375217	42.416576
3503.643498	715828.228391	42.421581
3503.348756	715770.329009	42.426586
3503.700730	715711.528540	42.431591
3503.534295	715666.953302	42.436596
3503.617516	715605.765425	42.441600
3503.426324	715569.677797	42.446605
3503.754398	715523.283574	42.451610
3503.555684	715464.026618	42.456615
3503.265334	715410.887085	42.461620
3503.482169	715359.548801	42.466624
3503.386208	715310.593847	42.471629
3503.323490	715269.968647	42.476634
3503.270309	715217.830645	42.481639
3502.881460	715178.598544	42.486644
3502.956210	715129.267009	42.491648
3503.203977	715093.997911	42.496653
3503.177661	715038.331532	42.501658
3503.050056	715006.994274	42.506663
3502.852204	714974.477676	42.511668
3503.182416	714917.014950	42.516672
3503.373972	714902.345917	42.521677
3503.079204	714855.902095	42.526682
3503.318470	714819.492026	42.531687
3502.913460	714768.550621	42.536692
3503.208863	714719.477942	42.541696
3503.055541	714687.647552	42.546701
3503.143989	714634.192427	42.551706
3503.206070	714604.707887	42.556711
3503.025485	714555.812155	42.561716
3503.282439	714501.732901	42.566720
3503.039553	714453.640805	42.571725
3503.283911	714418.319830	42.576730
3503.011662	714378.518902	42.581735
3502.999402	714344.927157	42.586740
3503.345911	714303.534975	42.591744
3503.287362	714257.247310	42.596749
3502.958573	714220.283443	42.601754
3503.021361	714174.074516	42.606759
3503.043757	714147.324185	42.611764
3503.125651	714096.298259	42.616768
3503.023116	714067.087162	42.621773
3502.643955	714015.789576	42.626778
3502.635206	713977.531170	42.631783
3502.809219	713957.156655	42.636788
3502.872307	713904.296591	42.641792
3502.793479	713869.820722	42.646797
3502.855360	713826.289765	42.651802
3503.047188	713796.532842	42.656807
3502.799561	713753.995532	42.661812
3502.854568	713714.683273	42.666816
3502.529115	713678.212737	42.671821
3502.597360	713646.887691	42.676826
3502.883464	713607.338242	42.681831
3503.168281	713572.999574	42.686836
3502.821063	713531.023489	42.691840
3502.836699	713501.145765	42.696845
3502.913396	713454.732104	42.701850
3503.067261	713434.558170	42.706855
3502.761681	713389.497625	42.711860
3502.560499	713360.399644	42.716864
3502.814259	713322.243778	42.721869
3502.623885	713299.595396	42.726874
3502.497138	713257.829660	42.731879
3502.606381	713212.649996	42.736884
3502.514781	713179.265247	42.741888
3502.491761	713157.085113	42.746893
3502.866601	713113.201002	42.751898
3503.044364	713079.969865	42.756903
3502.640102	713051.053266	42.761908
3502.791684	713010.530678	42.766912
3502.511090	712967.399308	42.771917
3502.550723	712938.011930	42.776922
3502.643316	712909.906081	42.781927
3502.425008	712889.147161	42.786932
3502.509044	712854.441722	42.791937
3502.136599	712821.995322	42.796941
3502.283351	712795.964631	42.801946
3502.579221	712769.661063	42.806951
3502.230700	712753.141953	42.811956
3502.382570	712704.031685	42.816961
3502.609307	712679.426727	42.821965
3502.597115	712663.993387	42.826970
3502.630980	712622.148346	42.831975
3502.187347	712598.100617	42.836980
3502.626584	712566.213953	42.841985
3502.619007	712538.570116	42.846989
3502.495752	712514.667737	42.851994
3502.606570	712464.818383	42.856999
3502.083327	712456.715488	42.862004
3502.402142	712415.864629	42.867009
3502.471638	712399.275750	42.872013
3502.242398	712359.210048	42.877018
3502.540312	712336.329500	42.882023
3501.919952	712315.585980	42.887028
3502.192997	712276.578457	42.892033
3502.252241	712261.827454	42.897037
3502.386079	712238.080346	42.902042
3502.137821	712208.241675	42.907047
3502.067598	712181.599713	42.912052
3502.591638	712151.335413	42.917057
3502.301274	712135.401101	42.922061
3502.322521	712090.825622	42.927066
3502.723718	712071.898085	42.932071
3502.221410	712041.207380	42.937076
3502.323481	712011.459031	42.942081
3502.418195	711987.965866	42.947085
3501.830822	711960.614503	42.952090
3501.783449	711933.918351	42.957095
3501.411758	711901.964662	42.962100
3501.608441	711895.826968	42.967105
3501.756235	711888.108995	42.972109
3501.419032	711872.380472	42.977114
3502.338970	711852.076185	42.982119
3502.091974	711836.630506	42.987124
3502.111263	711812.305502	42.992129
3502.257942	711815.408399	42.997133
3502.000286	711779.265938	43.002138
3502.094654	711755.970736	43.007143
3501.971939	711733.207714	43.012148
3502.059643	711713.487358	43.017153
3501.828843	711702.853556	43.022157
3501.657508	711662.774998	43.027162
3501.962904	711646.493129	43.032167
3501.722430	711642.363356	43.037172
3502.388549	711609.442866	43.042177
3502.160191	711599.999835	43.047181
3501.827858	711568.088022	43.052186
3501.820796	711554.339508	43.057191
3501.859454	711550.560667	43.062196
3501.984708	711514.055972	43.067201
3501.733375	711505.510121	43.072205
3501.638545	711480.607367	43.077210
3501.819407	711454.418017	43.082215
3501.958960	711452.012339	43.087220
3501.841308	711433.318042	43.092225
3502.007270	711409.811508	43.097229
3502.004125	711392.736281	43.102234
3501.933382	711357.752474	43.107239
3502.279037	711351.887607	43.112244
3502.031483	711325.222625	43.117249
3501.927697	711300.519381	43.122253
3502.157593	711279.930653	43.127258
3501.976097	711256.878231	43.132263
3501.854448	711246.523657	43.137268
3501.651888	711213.645912	43.142273
3501.614269	711205.759402	43.147277
3501.661897	711201.432883	43.152282
3501.833184	711181.598203	43.157287
3501.882757	711161.932512	43.162292
3501.769433	711148.746946	43.167297
3501.836516	711109.073143	43.172301
3501.736585	711090.921212	43.177306
3502.049962	711081.785207	43.182311
3501.948738	711068.200390	43.187316
3501.736448	711047.783455	43.192321
3501.629181	711043.681016	43.197325
3501.970173	711024.661825	43.202330
3501.965522	711009.869570	43.207335
3501.954610	710990.213477	43.212340
3501.875010	710957.562630	43.217345
3501.950288	710953.082491	43.222349
3502.011065	710927.854557	43.227354
3502.030557	710903.874415	43.232359
3501.669669	710889.140819	43.237364
3501.670717	710853.646657	43.242369
3501.806067	710856.305000	43.247373
3501.744104	710838.344824	43.252378
3501.666522	710819.592914	43.257383
3501.737704	710804.688487	43.262388
3501.924932	710791.353415	43.267393
3501.587872	710776.714971	43.272397
3501.661801	710756.994678	43.277402
3501.918959	710754.122587	43.282407
3501.829283	710727.280713	43.287412
3501.711866	710711.166217	43.292417
3501.157237	710700.733600	43.297421
3501.590059	710682.145258	43.302426
3501.810657	710662.599082	43.307431
3501.775647	710663.150979	43.312436
3501.743778	710641.660747	43.317441
3501.446401	710619.072537	43.322445
3501.631298	710610.900488	43.327450
3501.707760	710607.561773	43.332455
3501.557026	710588.771800	43.337460
3501.951762	710562.345794	43.342465
3501.586489	710554.909976	43.347469
3501.654659	710549.785431	43.352474
3501.819152	710514.808932	43.357479
3501.808781	710508.356951	43.362484
3502.036201	710491.192173	43.367489
3501.621753	710467.282512	43.372493
3501.656351	710455.957913	43.377498
3502.013219	710441.253863	43.382503
3501.808190	710412.444280	43.387508
3501.798087	710401.673087	43.392513
3501.413558	710380.041894	43.397517
3501.333483	710359.849684	43.402522
3501.581528	710348.936476	43.407527
3501.574232	710353.802930	43.412532
3501.498205	710334.652536	43.417537
3501.423545	710309.842316	43.422541
3501.598411	710311.650330	43.427546
3501.625920	710302.262863	43.432551
3501.457583	710301.992846	43.437556
3501.633959	710261.403424	43.442561
3501.530176	710248.760988	43.447565
3501.192819	710248.270671	43.452570
3501.499858	710244.496547	43.457575
3501.216276	710241.117896	43.462580
3501.837741	710218.128554	43.467585
3501.601378	710214.295277	43.472589
3501.629679	710214.141699	43.477594
3501.658520	710193.931098	43.482599
3501.730501	710182.053853	43.487604
3501.519387	710163.769381	43.492609
3501.524197	710154.534441	43.497613
3500.977507	710123.595910	43.502618
3501.605826	710119.570054	43.507623
3501.449001	710117.510858	43.512628
3501.647079	710109.584384	43.517633
3501.618037	710104.028818	43.522637
3501.176723	710078.434525	43.527642
3501.392096	710069.412930	43.532647
3501.287903	710069.132305	43.537652
3501.522339	710060.901897	43.542657
3501.222599	710060.157119	43.547661
3501.025102	710042.763778	43.552666
3501.228315	710028.034764	43.557671
3501.204582	710028.783425	43.562676
3501.429923	710017.377077	43.567681
3501.635298	710016.002707	43.572685
3501.241661	710022.521896	43.577690
3501.242124	710012.046347	43.582695
3501.306575	709988.751262	43.587700
3501.393433	709961.182744	43.592705
3501.725414	709965.596175	43.597709
3501.435272	709961.722023	43.602714
3501.639097	709951.609973	43.607719
3501.378269	709936.907837	43.612724
3501.321980	709917.852542	43.617729
3501.104797	709917.243050	43.622733
3501.186982	709910.775322	43.627738
3501.319091	709904.646873	43.632743
3501.239288	709914.043491	43.637748
3501.143705	709885.065097	43.642753
3501.099098	709872.114437	43.647757
3501.089696	709866.803711	43.652762
3501.065244	709864.077156	43.657767
3501.060255	709881.752635	43.662772
3501.378103	709860.947361	43.667777
3501.319312	709851.226125	43.672781
3501.657698	709859.957921	43.677786
3501.705886	709845.651394	43.682791
3501.474233	709835.660818	43.687796
3501.492806	709819.919349	43.692801
3501.626049	709810.116684	43.697805
3501.594348	709793.589104	43.702810
3501.921132	709767.072574	43.707815
3501.381604	709770.935047	43.712820
3501.777571	709745.251040	43.717825
3501.580084	709726.864082	43.722829
3501.551700	709713.463663	43.727834
3501.919249	709718.119590	43.732839
3501.581753	709711.969308	43.737844
3501.860086	709689.730336	43.742849
3501.680387	709691.348831	43.747853
3501.584497	709672.944968	43.752858
3501.547691	709643.608499	43.757863
3501.257986	709650.160444	43.762868
3501.269080	709642.165139	43.767873
3501.426027	709646.011872	43.772877
3501.524929	709633.781873	43.777882
3501.733754	709604.355029	43.782887
3501.398113	709593.438015	43.787892
3501.615251	709595.437796	43.792897
3501.468988	709578.680484	43.797901
3501.610075	709563.514092	43.802906
3501.991416	709546.619881	43.807911
3501.537728	709544.013806	43.812916
3501.621285	709520.466038	43.817921
3501.773707	709513.887105	43.822925
3501.565173	709507.020265	43.827930
3501.491525	709486.874578	43.832935
3501.279064	709469.979042	43.837940
3501.503123	709471.928058	43.842945
3501.342370	709464.407836	43.847949
3501.543564	709469.041740	43.852954
3501.518335	709440.099861	43.857959
3500.951026	709427.036303	43.862964
3501.694565	709410.826726	43.867969
3501.538385	709413.335096	43.872973
3501.497256	709410.114648	43.877978
3501.286426	709399.226409	43.882983
3501.174870	709382.711231	43.887988
3501.456181	709367.372367	43.892993
3501.421211	709373.733474	43.897997
3500.992425	709366.009205	43.903002
3501.386360	709367.532967	43.908007
3501.091912	709368.227121	43.913012
3501.432421	709351.239971	43.918017
3501.368685	709325.531371	43.923021
3501.312901	709322.015405	43.928026
3501.467375	709308.087623	43.933031
3501.062092	709315.949850	43.938036
3501.547755	709303.059653	43.943041
3501.416897	709296.874923	43.948045
3501.433458	709272.443824	43.953050
3501.623577	709274.944658	43.958055
3501.485801	709276.308046	43.963060
3501.478398	709255.902612	43.968065
3501.399868	709238.587275	43.973069
3501.481614	709218.762837	43.978074
3501.491060	709211.959041	43.983079
3501.088311	709212.720756	43.988084
3501.475474	709204.613244	43.993089
3501.217236	709188.270884	43.998093
3500.992223	709170.830661	44.003098
3501.552450	709158.772008	44.008103
3501.285388	709164.277890	44.013108
3501.382939	709162.573641	44.018113
3501.109370	709163.264360	44.023117
3501.299165	709157.125844	44.028122
3501.582557	709131.458601	44.033127
3501.175199	709131.376998	44.038132
3501.265113	709129.177483	44.043137
3501.296597	709127.136579	44.048141
3501.057399	709124.991450	44.053146
3501.181454	709108.238197	44.058151
3501.257535	709121.780712	44.063156
3501.191026	709094.731268	44.068161
3501.255955	709085.385934	44.073165
3501.006539	709080.461948	44.078170
3501.402683	709078.311120	44.083175
3501.298422	709075.200283	44.088180
3501.286882	709079.323377	44.093185
3501.306450	709073.163279	44.098189
3501.203045	709057.341259	44.103194
3501.544108	709036.579802	44.108199
3501.306459	709033.391687	44.113204
3501.573072	709018.799419	44.118209
3501.803837	709028.195340	44.123213
3501.525816	709000.088191	44.128218
3501.381298	708986.556865	44.133223
3501.657654	708982.638303	44.138228
3501.796553	708974.372989	44.143233
3501.711680	708954.277556	44.148237
3501.357933	708941.773798	44.153242
3501.625865	708938.551752	44.158247
3501.211313	708932.413639	44.163252
3501.589017	708918.746255	44.168257
3501.675628	708903.289776	44.173261
3501.290955	708891.337242	44.178266
3501.486945	708885.594737	44.183271
3501.324305	708882.890705	44.188276
3501.767426	708854.564600	44.193281
3501.592017	708849.032406	44.198285
3501.354097	708835.168699	44.203290
3501.901267	708828.871585	44.208295
3501.436979	708808.739201	44.213300
3501.743094	708795.927570	44.218305
3501.429543	708792.305020	44.223309
3501.562645	708783.692903	44.228314
3501.644379	708761.930899	44.233319
3501.279143	708752.159745	44.238324
3501.253632	708742.233130	44.243329
3501.134631	708740.912164	44.248333
3501.132885	708743.891751	44.253338
3501.492074	708737.079436	44.258343
3501.280595	708715.763004	44.263348
3501.534887	708703.208071	44.268353
3501.223570	708706.636065	44.273357
3501.256163	708704.545223	44.278362
3501.184779	708688.468957	44.283367
3501.103123	708698.065834	44.288372
3501.132955	708672.439119	44.293377
3501.214039	708659.813436	44.298381
3501.000747	708656.571499	44.303386
3501.461552	708645.472001	44.308391
3501.173043	708635.539068	44.313396
3501.359403	708640.473805	44.318401
3500.969499	708642.971367	44.323405
3501.106185	708645.232942	44.328410
3501.586917	708630.356357	44.333415
3500.944076	708617.601966	44.338420
3501.154458	708602.770008	44.343425
3500.924199	708600.126716	44.348429
3500.815540	708585.744693	44.353434
3501.190941	708591.542013	44.358439
3500.665719	708602.106092	44.363444
3501.059026	708589.577676	44.368449
3501.084656	708598.362451	44.373453
3500.960244	708590.239591	44.378458
3501.490685	708580.916090	44.383463
3501.498888	708595.563072	44.388468
3501.264921	708583.535547	44.393473
3501.292133	708559.597207	44.398477
3501.261023	708556.523748	44.403482
3501.633591	708547.375266	44.408487
3501.506795	708541.884495	44.413492
3501.592910	708528.810888	44.418497
3501.678951	708524.327701	44.423501
3501.131039	708509.918826	44.428506
3501.273931	708499.517200	44.433511
3501.011546	708510.981415	44.438516
3501.128461	708493.632274	44.443521
3501.277413	708502.744359	44.448525
3501.197485	708498.636175	44.453530
3501.592817	708479.453388	44.458535
3501.447487	708463.239951	44.463540
3501.375031	708450.093116	44.468545
3501.224267	708457.765096	44.473549
3501.101273	708460.864129	44.478554
3501.206191	708451.908744	44.483559
3501.123987	708451.574773	44.488564
3501.481957	708418.891569	44.493569
3501.394167	708415.281207	44.498573
3501.328437	708407.595383	44.503578
3501.486206	708403.348561	44.508583
3501.398442	708415.677861	44.513588
3501.491897	708383.981705	44.518593
3501.121763	708364.676874	44.523597
3501.398148	708367.560973	44.528602
3501.619148	708363.055400	44.533607
3501.311768	708363.453827	44.538612
3501.223891	708344.648530	44.543617
3501.385911	708325.156357	44.548621
3501.217390	708312.124499	44.553626
3501.423365	708316.360986	44.558631
3501.425985	708308.812749	44.563636
3501.491746	708304.730053	44.568641
3501.769282	708286.956696	44.573645
3501.876486	708273.233674	44.578650
3501.979229	708265.619196	44.583655
3501.808540	708243.152733	44.588660
3501.760065	708230.845772	44.593665
3501.539292	708223.284718	44.598669
3501.654526	708199.678429	44.603674
3501.680101	708175.937920	44.608679
3501.644930	708181.952341	44.613684
3501.498428	708171.101564	44.618689
3501.361695	708143.166882	44.623693
3501.422970	708144.249265	44.628698
3501.582333	708123.565286	44.633703
3501.768899	708127.209179	44.638708
3501.573033	708093.325154	44.643713
3501.491706	708078.292206	44.648717
3501.414913	708082.476221	44.653722
3501.304305	708073.655375	44.658727
3501.419628	708080.240897	44.663732
3501.535261	708044.616824	44.668737
3501.175850	708031.566426	44.673741
3501.265802	708037.460954	44.678746
3501.565365	708025.443794	44.683751
3501.497701	708032.754811	44.688756
3501.408915	708009.132055	44.693761
3501.425792	707992.046724	44.698765
3501.384766	707981.823841	44.703770
3501.667926	707975.420760	44.708775
3501.221471	707971.968798	44.713780
3501.167629	707949.531915	44.718785
3501.537715	707945.448418	44.723789
3501.475740	707942.181203	44.728794
3501.196539	707942.277037	44.733799
3501.293257	707949.660278	44.738804
3501.581080	707927.713125	44.743809
3501.498695	707905.479480	44.748813
3501.357996	707903.119125	44.753818
3501.525497	707900.757498	44.758823
3501.090888	707903.163339	44.763828
3501.061975	707894.477785	44.768833
3501.285026	707877.407815	44.773837
3501.274866	707872.592570	44.778842
3501.498449	707865.801978	44.783847
3501.245091	707867.830260	44.788852
3501.367805	707858.325062	44.793857
3501.338556	707868.410801	44.798861
3501.401617	707834.830582	44.803866
3501.499055	707814.056772	44.808871
3501.351375	707812.492101	44.813876
3501.291373	707804.606150	44.818881
3501.644162	707813.685284	44.823885
3501.332889	707786.721819	44.828890
3501.249057	707766.027509	44.833895
3501.195342	707772.094941	44.838900
3501.456418	707768.823935	44.843905
3501.115179	707761.828639	44.848909
3501.268105	707766.223147	44.853914
3501.454701	707757.104561	44.858919
3501.371737	707739.985568	44.863924
3501.113629	707725.080535	44.868929
3501.070755	707723.200567	44.873933
3501.392427	707721.707298	44.878938
3501.477222	707709.327906	44.883943
3501.584737	707712.091154	44.888948
3501.402413	707697.471512	44.893953
3501.383373	707681.980633	44.898957
3501.250361	707682.648236	44.903962
3501.394058	707671.351587	44.908967
3501.159534	707674.518994	44.913972
3501.532526	707676.791438	44.918977
3501.525595	707642.626107	44.923981
3501.314809	707635.261525	44.928986
3501.315667	707624.187061	44.933991
3501.267279	707627.075422	44.938996
3501.568968	707620.966982	44.944001
3501.811822	707594.109984	44.949005
3501.634382	707591.656292	44.954010
3501.735642	707582.700607	44.959015
3501.388498	707574.216301	44.964020
3501.650583	707538.764574	44.969025
3501.534810	707529.944022	44.974029
3501.437541	707525.043654	44.979034
3501.650747	707516.367369	44.984039
3501.593793	707496.363227	44.989044
3501.914807	707483.149889	44.994049
3501.754482	707484.765592	44.999053
3501.764260	707463.111511	45.004058
3501.911921	707450.373725	45.009063
3501.486749	707435.545458	45.014068
3501.699461	707414.900620	45.019073
3501.617777	707405.627348	45.024077
3501.477646	707408.928239	45.029082
3501.420960	707386.887653	45.034087
3501.289611	707366.448542	45.039092
3501.780514	707344.962968	45.044097
3501.689556	707352.675712	45.049101
3501.375351	707350.045901	45.054106
3501.506606	707312.926341	45.059111
3501.496927	707310.643496	45.064116
3501.445555	707300.769150	45.069121
3501.519214	707306.567548	45.074125
3501.173553	707282.140976	45.079130
3501.530806	707263.259750	45.084135
3501.554344	707261.517694	45.089140
3501.252354	707248.208297	45.094145
3501.282024	707252.176470	45.099149
3501.515435	707251.690968	45.104154
3501.541406	707225.067311	45.109159
3501.112650	707221.214812	45.114164
3501.303420	707219.792755	45.119169
3501.211319	707220.105990	45.124173
3501.108661	707213.915093	45.129178
3501.428246	707219.821899	45.134183
3501.243968	707204.903761	45.139188
3501.239656	707175.901120	45.144193
3501.277575	707180.414261	45.149197
3501.446408	707171.794625	45.154202
3501.593761	707167.350263	45.159207
3501.281296	707167.302608	45.164212
3501.222748	707144.169111	45.169217
3501.148992	707132.013743	45.174221
3501.152695	707122.825383	45.179226
3501.047362	707130.143391	45.184231
3501.214244	707121.871674	45.189236
3500.891699	707124.706180	45.194241
3500.933697	707122.712727	45.199245
3500.765890	707124.578052	45.204250
3501.140409	707122.579313	45.209255
3501.115008	707119.007758	45.214260
3501.305332	707120.217937	45.219265
3501.342348	707115.990437	45.224269
3501.337820	707096.771322	45.229274
3501.289262	707076.764816	45.234279
3500.979941	707078.802528	45.239284
3501.558509	707073.839883	45.244289
3501.481149	707079.862046	45.249293
3500.949211	707086.257310	45.254298
3501.358783	707074.518630	45.259303
3501.077372	707061.006885	45.264308
3501.125885	707040.338620	45.269313
3501.126060	707038.451387	45.274317
3501.171552	707038.990212	45.279322
3501.101596	707042.925281	45.284327
3500.883015	707028.459483	45.289332
3501.216393	707036.946679	45.294337
3501.102487	707037.362852	45.299341
3500.633794	707043.151725	45.304346
3500.950999	707027.554437	45.309351
3500.883882	707035.015204	45.314356
3500.937208	707043.250687	45.319361
3501.177219	707037.003036	45.324365
3500.892040	707036.702549	45.329370
3501.564245	707030.085486	45.334375
3500.858054	707016.147224	45.339380
3501.021149	706991.437093	45.344385
3501.073887	706988.498209	45.349389
3500.959312	706987.970870	45.354394
3501.142508	706990.523187	45.359399
3500.834710	706997.427785	45.364404
3501.401102	706969.174433	45.369409
3501.172725	706990.418974	45.374413
3501.104566	706985.761810	45.379418
3501.354869	706978.270802	45.384423
3501.236498	706972.082327	45.389428
3501.202386	706973.230286	45.394433
3501.046230	706951.900327	45.399437
3500.783374	706937.342362	45.404442
3501.417388	706936.740978	45.409447
3501.148119	706933.855288	45.414452
3501.340977	706930.247586	45.419457
3501.274031	706931.251982	45.424461
3501.294936	706936.761359	45.429466
3501.606375	706932.836074	45.434471
3501.491202	706914.628133	45.439476
3501.542465	706896.640974	45.444481
3501.505692	706888.452353	45.449485
3501.391209	706891.699538	45.454490
3501.279277	706867.928473	45.459495
3501.193369	706848.424260	45.464500
3501.199920	706849.267524	45.469505
3501.242606	706848.515527	45.474509
3500.935179	706851.595950	45.479514
3501.067821	706845.961887	45.484519
3500.961342	706845.234540	45.489524
3501.160747	706847.684890	45.494529
3501.170051	706846.640417	45.499533
3501.272170	706839.968422	45.504538
3501.258869	706830.782560	45.509543
3500.969156	706813.546891	45.514548
3501.148748	706809.494342	45.519553
3501.050530	706803.749404	45.524557
3501.084445	706806.177449	45.529562
3501.505253	706783.609419	45.534567
3501.009519	706796.455449	45.539572
3500.761462	706793.715203	45.544577
3500.949089	706805.206652	45.549581
3501.077044	706811.890392	45.554586
3500.952204	706793.981786	45.559591
3500.938121	706801.632653	45.564596
3501.391553	706794.852902	45.569601
3501.148699	706797.922673	45.574605
3501.404149	706797.632168	45.579610
3501.364418	706775.338884	45.584615
3501.055568	706771.118704	45.589620
3501.005488	706746.244435	45.594625
3501.141001	706751.585994	45.599629
3501.194381	706763.000352	45.604634
3501.125713	706756.505513	45.609639
3500.954076	706762.543478	45.614644
3501.231943	706747.200514	45.619649
3501.125103	706756.803719	45.624653
3500.937850	706740.196626	45.629658
3501.077982	706720.605103	45.634663
3501.083213	706714.644347	45.639668
3501.347716	706716.289321	45.644673
3501.184793	706720.537896	45.649677
3500.965567	706706.071661	45.654682
3501.169495	706711.451605	45.659687
3501.074690	706710.970647	45.664692
3501.015499	706710.334806	45.669697
3501.295723	706705.768917	45.674701
3501.123020	706710.813772	45.679706
3501.428205	706702.667796	45.684711
3501.790552	706695.307027	45.689716
3501.590161	706669.911048	45.694721
3501.129652	706674.059824	45.699725
3501.037994	706671.095028	45.704730
3501.332922	706661.858049	45.709735
3501.090736	706653.156819	45.714740
3501.230529	706629.840163	45.719745
3500.934121	706634.160505	45.724749
3500.865944	706621.705495	45.729754
3501.194068	706619.565310	45.734759
3501.147137	706625.135763	45.739764
3500.930574	706617.721594	45.744769
3501.003194	706621.831960	45.749773
3501.180245	706619.021408	45.754778
3501.480836	706617.183772	45.759783
3501.125658	706627.722158	45.764788
3500.826822	706617.788589	45.769793
3500.996014	706618.406332	45.774797
3501.039420	706616.561530	45.779802
3501.285141	706602.316287	45.784807
3501.259353	706587.917220	45.789812
3501.321261	706507.496076	45.794817
3501.525540	706403.756452	45.799821
3501.168597	706215.770841	45.804826
3501.456357	705989.130550	45.809831
3500.738219	705699.815770	45.814836
3500.885247	705354.117623	45.819841
3500.850187	704952.351458	45.824845
3499.839694	704502.092403	45.829850
3500.070430	703986.521928	45.834855
3499.724987	703414.275879	45.839860
3499.538973	702791.233840	45.844865
3498.907823	702109.931615	45.849869
3498.709168	701373.987516	45.854874
3498.888073	700572.065046	45.859879
3498.135972	699717.633996	45.864884
3497.785715	698803.151318	45.869889
3497.007352	697832.016946	45.874893
3496.068028	696810.333815	45.879898
3495.935413	695711.220469	45.884903
3495.659580	694585.535336	45.889908
3494.779221	693374.450846	45.894913
3494.076302	692112.677377	45.899917
3493.455287	690772.147319	45.904922
3493.205073	689401.945117	45.909927
3492.040248	687959.068550	45.914932
3491.366834	686451.813377	45.919937
3491.081721	684887.384891	45.924941
3490.090393	683262.250587	45.929946
3488.911621	681586.304651	45.934951
3487.664737	679851.231394	45.939956
3487.061479	678057.827977	45.944961
3486.049368	676192.730682	45.949965
3485.151877	674297.782001	45.954970
3484.239597	672314.755076	45.959975
3483.218416	670293.977795	45.964980
3482.066541	668191.539271	45.969985
3481.013261	666073.104216	45.974989
3479.855230	663857.510255	45.979994
3478.936575	661609.522641	45.984999
3477.740072	659305.942932	45.990004
3476.671879	656942.972703	45.995009
3475.479198	654519.615550	46.000013
3474.000262	652041.703149	46.005018
3472.925455	649509.634552	46.010023
3471.256433	646918.589587	46.015028
3470.520727	644279.025043	46.020033
3468.836709	641581.116756	46.025037
3467.120065	638829.074914	46.030042
3466.199665	636028.179345	46.035047
3464.680066	633170.718992	46.040052
3463.243777	630267.956539	46.045057
3461.360521	627290.551466	46.050061
3459.791777	624281.304468	46.055066
3458.334886	621216.427967	46.060071
3456.951315	618107.367531	46.065076
3455.258149	614938.514039	46.070081
3453.690899	611713.915487	46.075085
3451.994412	608451.886066	46.080090
3450.325801	605115.141841	46.085095
3448.398260	601758.088099	46.090100
3446.473830	598335.835308	46.095105
3445.060149	594876.831787	46.100109
3443.267046	591355.731293	46.105114
3441.319701	587780.393725	46.110119
3439.386190	584157.843568	46.115124
3437.567811	580492.962867	46.120129
3435.391980	576783.944137	46.125133
3433.229356	573028.033669	46.130138
3431.789131	569215.674660	46.135143
3429.366156	565371.833572	46.140148
3427.209642	561467.534615	46.145153
3425.410537	557531.439363	46.150157
3422.859561	553532.980548	46.155162
3421.067982	549497.677905	46.160167
3418.983913	545436.077108	46.165172
3416.445552	541307.497783	46.170177
3414.685428	537148.474503	46.175181
3412.229860	532935.726606	46.180186
3410.167588	528655.164978	46.185191
3407.764554	524376.908763	46.190196
3405.218868	520031.447641	46.195201
3402.961978	515639.186823	46.200205
3400.415565	511219.863505	46.205210
3398.171074	506748.002910	46.210215
3395.528395	502256.112793	46.215220
3393.104922	497702.168066	46.220225
3390.717549	493105.802853	46.225229
3388.121391	488493.819273	46.230234
3385.334232	483817.480621	46.235239
3382.772972	479124.136501	46.240244
3379.895430	474389.225543	46.245249
3377.551805	469610.373613	46.250253
3374.489472	464815.702426	46.255258
3372.424788	459954.159841	46.260263
3369.511238	455088.133761	46.265268
3366.798353	450164.994465	46.270273
3364.248926	445205.279452	46.275277
3361.284709	440217.612738	46.280282
3358.560929	435185.001318	46.285287
3356.031532	430121.361505	46.290292
3352.908808	425016.632593	46.295297
3350.075605	419899.845841	46.300301
3346.997850	414744.707844	46.305306
3344.238343	409550.070110	46.310311
3341.143688	404325.146577	46.315316
3338.296956	399079.208939	46.320321
3335.157695	393790.212329	46.325325
3331.797309	388485.734824	46.330330
3329.096325	383144.256381	46.335335
3325.856555	377781.554099	46.340340
3322.778090	372391.869860	46.345345
3319.589156	366973.672797	46.350349
3316.059133	361529.189831	46.355354
3313.134305	356060.226647	46.360359
3309.915760	350571.796456	46.365364
3306.707234	345057.648370	46.370369
3303.545173	339520.963957	46.375373
3299.628981	333955.979746	46.380378
3296.768851	328365.687773	46.385383
3293.091092	322768.532170	46.390388
3289.616177	317131.545017	46.395393
3286.528286	311494.930430	46.400397
3282.910513	305844.702078	46.405402
3279.512411	300172.705650	46.410407
3275.694095	294477.814432	46.415412
3272.497820	288775.355121	46.420417
3269.041909	283050.339870	46.425421
3265.255985	277330.251801	46.430426
3261.972942	271573.104938	46.435431
3257.905925	265809.845352	46.440436
3254.373283	260036.583195	46.445441
3251.097442	254244.548282	46.450445
3247.000555	248449.705662	46.455450
3243.231688	242643.330430	46.460455
3239.052276	236842.146632	46.465460
3235.417498	231022.920594	46.470465
3231.417482	225203.347183	46.475469
3227.099590	219373.994430	46.480474
3223.446605	213556.086919	46.485479
3219.491574	207651.910823	46.490484
3215.603884	201816.195580	46.495489
3211.447754	195984.765839	46.500493
3207.049366	190164.320973	46.505498
3203.346003	184342.483896	46.510503
3199.448813	178514.615325	46.515508
3195.139134	172690.140528	46.520513
3190.657438	166875.275062	46.525517
3186.338609	161076.762321	46.530522
3182.323585	155265.281250	46.535527
3177.967927	149478.096489	46.540532
3173.864690	143704.912530	46.545537
3169.701729	137930.593697	46.550541
3164.816619	132179.064117	46.555546
3160.529565	126425.997744	46.560551
3155.923479	120711.575409	46.565556
3151.193340	114992.691648	46.570561
3146.658706	109301.383434	46.575565
3141.823434	103616.063388	46.580570
3137.011664	97971.234771	46.585575
3131.874921	92355.209204	46.590580
3126.860942	86769.130374	46.595585
3122.106986	81192.074698	46.600589
3116.955711	75663.850759	46.605594
3111.731867	70164.189169	46.610599
3106.409305	64717.134793	46.615604
3100.903416	59292.270146	46.620609
3095.116978	53925.239797	46.625613
3089.000652	48611.631121	46.630618
3083.007471	43338.626282	46.635623
3075.506440	38163.916326	46.640628
3063.515200	33190.014362	46.645633
3047.852462	28430.147574	46.650637
3032.253099	23839.785564	46.655642
3017.594082	19469.051546	46.660647
3000.425253	15403.901335	46.665652
2975.008791	11824.659956	46.670657
2946.829954	8708.414276	46.675661
2920.819122	5982.105388	46.680666
2897.566543	3653.838904	46.685671
2875.923452	1770.567604	46.690676
2851.857505	446.988885	46.695681
2803.743646	273.345158	46.700685
2774.210523	267.095716	46.705690
2768.434007	264.837025	46.710695
2777.925291	268.725067	46.715700
2793.926605	265.846590	46.720705
2808.377133	264.787952	46.725709
2817.365492	268.426608	46.730714
2820.534404	249.359908	46.735719
2819.861731	256.815795	46.740724
2816.409841	253.186998	46.745729
2812.453854	253.920315	46.750733
2808.313275	263.953936	46.755738
2805.073960	252.500250	46.760743
2802.168311	248.859007	46.765748
2799.501626	237.507307	46.770753
2796.936344	250.520488	46.775757
2794.106744	246.263403	46.780762
2791.688795	246.433541	46.785767
2788.806433	248.742725	46.790772
2785.303238	247.537466	46.795777
2782.429675	232.771548	46.800781
2779.308367	255.886522	46.805786
2776.536193	242.478472	46.810791
2772.808841	248.727458	46.815796
2769.793767	239.298679	46.820801
2767.225559	230.697776	46.825805
2763.573663	233.407855	46.830810
2760.314312	238.809769	46.835815
2756.553312	239.082837	46.840820
2753.376265	241.891735	46.845825
2750.161736	236.357686	46.850829
2747.113762	242.487925	46.855834
2743.885547	239.218818	46.860839
2740.528280	249.778783	46.865844
2736.868431	242.394411	46.870849
2733.885350	235.747168	46.875853
2730.293025	246.380185	46.880858
2727.126684	230.639779	46.885863
2723.686333	237.281751	46.890868
2719.797132	237.042076	46.895873
2717.195506	226.483827	46.900877
2713.169328	230.923598	46.905882
2710.264632	229.114546	46.910887
2706.954952	235.946050	46.915892
2703.482687	235.532194	46.920897
2700.122154	229.854225	46.925901
2696.233839	234.919839	46.930906
2692.781391	226.727623	46.935911
2689.450565	235.124958	46.940916
2686.524538	226.180777	46.945921
2682.775521	227.854402	46.950925
2678.956982	227.998334	46.955930
2676.619525	222.223256	46.960935
2672.358806	228.644279	46.965940
2668.524784	222.684579	46.970945
2665.518088	221.308628	46.975949
2661.774209	219.393831	46.980954
2658.583686	218.962776	46.985959
2655.545695	222.894658	46.990964
2652.274688	227.807993	46.995969
2648.739833	218.247905	47.000973
2644.593752	221.478569	47.005978
2641.693772	217.767838	47.010983
2638.403640	216.640309	47.015988
2634.213990	217.570339	47.020993
2630.966282	213.327736	47.025997
2627.608561	210.693688	47.031002
2624.378939	206.908485	47.036007
2620.485551	214.983596	47.041012
2617.720061	214.019452	47.046017
2613.864720	221.892120	47.051021
2610.386611	213.746660	47.056026
2606.541959	212.694383	47.061031
2603.286699	215.437792	47.066036
2599.519135	217.287425	47.071041
2596.287320	208.409144	47.076045
2593.374860	212.676673	47.081050
2589.625649	207.742388	47.086055
2586.256520	211.370772	47.091060
2582.525331	211.641623	47.096065
2579.461343	205.911512	47.101069
2575.513877	211.616914	47.106074
2572.375539	207.422558	47.111079
2568.490858	206.282814	47.116084
2564.819085	201.398289	47.121089
2561.698034	206.570232	47.126093
2558.050867	208.712547	47.131098
2555.231081	208.860547	47.136103
2551.870396	214.550518	47.141108
2548.013164	211.472939	47.146113
2544.254492	205.009720	47.151117
2540.679054	212.036689	47.156122
2537.332229	212.901269	47.161127
2534.114146	216.080016	47.166132
2530.360454	202.655526	47.171137
2527.110834	215.281269	47.176141
2523.440139	207.564030	47.181146
2520.187430	204.176223	47.186151
2516.576534	200.648613	47.191156
2512.894657	204.281473	47.196161
2509.728062	199.181336	47.201165
2505.861796	205.282431	47.206170
2502.619354	197.642508	47.211175
2498.498502	201.272879	47.216180
2495.723322	204.124739	47.221185
2492.207634	202.522980	47.226189
2488.629682	204.224883	47.231194
2485.381550	190.936177	47.236199
2481.226538	205.841907	47.241204
2478.212919	200.006645	47.246209
2475.065946	193.450498	47.251213
2471.380725	203.427522	47.256218
2467.895826	197.772526	47.261223
2463.950737	202.910485	47.266228
2460.738653	205.180344	47.271233
2457.250880	194.069089	47.276237
2453.507581	199.354401	47.281242
2450.355541	200.459710	47.286247
2446.870994	195.878383	47.291252
2443.252304	199.392105	47.296257
2439.941105	194.091599	47.301261
2436.616732	198.973661	47.306266
2432.989740	184.999446	47.311271
2429.128830	196.225917	47.316276
2425.779802	187.240122	47.321281
2422.564319	186.151712	47.326285
2418.475239	197.693037	47.331290
2415.083890	188.342082	47.336295
2411.875528	196.678659	47.341300
2408.478771	189.841484	47.346305
2405.142852	177.244067	47.351309
2401.288668	182.225530	47.356314
2398.031716	184.893589	47.361319
2393.793948	189.695663	47.366324
2390.671667	187.024600	47.371329
2387.446269	184.332530	47.376333
2383.798355	192.837427	47.381338
2380.908355	181.304614	47.386343
2377.466837	178.260184	47.391348
2373.319511	185.480254	47.396353
2369.828647	182.950958	47.401357
2365.881020	185.254884	47.406362
2362.772295	189.918551	47.411367
2359.235647	192.222896	47.416372
2355.909450	189.640884	47.421377
2352.442267	180.062984	47.426381
2349.086320	193.032036	47.431386
2345.963029	183.691809	47.436391
2342.212801	191.422759	47.441396
2338.483909	190.949290	47.446401
2335.210405	183.905090	47.451405
2331.129148	196.560141	47.456410
2327.680566	185.610062	47.461415
2324.361690	183.865542	47.466420
2321.016978	178.153328	47.471425
2317.867061	178.511269	47.476429
2313.760657	186.240648	47.481434
2310.272346	178.429485	47.486439
2307.149202	183.112350	47.491444
2303.174218	182.412676	47.496449
2300.309609	174.884409	47.501453
2296.639478	181.536315	47.506458
2292.959262	175.373529	47.511463
2289.657657	173.899882	47.516468
2286.273103	180.167645	47.521473
2282.704934	176.354339	47.526477
2278.916087	186.794840	47.531482
2275.369343	171.544556	47.536487
2271.507755	180.971751	47.541492
2268.175599	178.974914	47.546497
2265.386244	177.938591	47.551501
2261.858547	178.724810	47.556506
2258.334506	178.435539	47.561511
2254.613553	175.561229	47.566516
2250.742985	178.565864	47.571521
2247.653791	183.908367	47.576525
2243.749049	180.315619	47.581530
2240.370558	175.172267	47.586535
2237.313873	175.249408	47.591540
2233.767976	174.671524	47.596545
2230.302942	172.233583	47.601549
2226.611977	175.087325	47.606554
2222.951992	177.121141	47.611559
2219.562428	186.727323	47.616564
2216.437640	181.595639	47.621569
2212.710288	179.213201	47.626573
2208.850835	175.793746	47.631578
2205.539922	175.814947	47.636583
2201.913295	177.433981	47.641588
2198.193026	179.283034	47.646593
2195.250655	175.286420	47.651597
2191.501764	179.348996	47.656602
2187.889022	163.237716	47.661607
2184.423206	174.032468	47.666612
2181.130399	183.508784	47.671617
2177.610568	176.125263	47.676621
2173.937084	183.102442	47.681626
2170.560759	176.212569	47.686631
2166.935863	178.088868	47.691636
2163.431403	175.488201	47.696641
2159.828514	175.838418	47.701645
2156.392939	189.470414	47.706650
2153.432710	177.524757	47.711655
2149.829817	180.571178	47.716660
2145.989782	181.188615	47.721665
2142.489130	172.746601	47.726669
2138.731759	182.108097	47.731674
2135.779073	182.420871	47.736679
2132.535649	183.794144	47.741684
2128.444210	178.671515	47.746689
2125.083062	172.669349	47.751693
2121.167424	175.965730	47.756698
2117.995448	176.787859	47.761703
2114.706540	179.357034	47.766708
2110.692979	188.108016	47.771713
2107.383263	174.965838	47.776717
2104.140084	179.184470	47.781722
2100.877075	168.494746	47.786727
2096.930145	172.337623	47.791732
2093.712579	177.205791	47.796737
2090.083781	168.282051	47.801741
2086.129651	169.499204	47.806746
2082.928220	170.877397	47.811751
2079.267886	179.328342	47.816756
2075.888375	177.634723	47.821761
2072.911176	170.799186	47.826765
2069.368406	176.286222	47.831770
2065.728708	171.808300	47.836775
2062.043813	179.510692	47.841780
2058.413407	177.013667	47.846785
2055.010512	178.822496	47.851789
2051.397513	177.170148	47.856794
2047.952028	168.071036	47.861799
2044.350385	183.523803	47.866804
2040.800234	174.954515	47.871809
2037.772183	176.484379	47.876813
2034.093468	178.849827	47.881818
2030.522541	163.132966	47.886823
2027.165898	170.769548	47.891828
2023.696285	177.533689	47.896833
2020.447841	164.778489	47.901837
2016.453708	180.691961	47.906842
2012.847290	174.003748	47.911847
2009.099501	182.050891	47.916852
2005.686507	173.101537	47.921857
2002.335197	174.778724	47.926861
1998.947012	177.409628	47.931866
1996.046638	162.948831	47.936871
1992.464175	170.261932	47.941876
1988.876127	172.826897	47.946881
1985.026855	163.062050	47.951885
1981.440518	171.787733	47.956890
1977.735279	165.996046	47.961895
1974.156401	161.194373	47.966900
1970.899598	170.448780	47.971905
1967.721558	167.990348	47.976909
1964.106093	163.318869	47.981914
1960.781595	153.478738	47.986919
1956.665136	172.899229	47.991924
1953.334137	164.866185	47.996929
1950.006902	167.112484	48.001933
1946.508488	174.155159	48.006938
1943.096582	158.941294	48.011943
1939.414539	163.164097	48.016948
1936.258316	170.909221	48.021953
1933.057350	156.310829	48.026957
1928.993090	171.569190	48.031962
1925.398974	160.718221	48.036967
1921.804661	157.630838	48.041972
1918.351260	163.204610	48.046977
1915.241585	164.706649	48.051981
1911.318475	163.686970	48.056986
1907.975135	161.313799	48.061991
1904.597516	170.085071	48.066996
1901.114126	165.501679	48.072001
1897.732936	157.093190	48.077005
1894.123290	159.620176	48.082010
1890.353045	152.458207	48.087015
1886.862642	161.657055	48.092020
1883.328610	161.946373	48.097025
1880.004014	164.327464	48.102029
1876.484896	165.526004	48.107034
1872.979774	156.385245	48.112039
1869.355963	160.557016	48.117044
1865.882395	158.602896	48.122049
1862.558267	159.872139	48.127053
1858.607081	166.790018	48.132058
1855.526478	168.985454	48.137063
1851.685551	160.242940	48.142068
1848.563162	163.647665	48.147073
1845.106592	155.526803	48.152077
1841.712207	163.532080	48.157082
1837.785159	151.171522	48.162087
1834.473656	156.782422	48.167092
1830.656576	160.467860	48.172097
1827.455392	159.120227	48.177101
1823.548160	155.009719	48.182106
1820.484922	155.734921	48.187111
1817.508877	155.414996	48.192116
1813.400890	167.073818	48.197121
1809.911271	154.467132	48.202125
1806.241374	154.281753	48.207130
1803.233280	159.472585	48.212135
1799.593854	158.056715	48.217140
1795.804805	165.959510	48.222145
1792.719623	158.613443	48.227149
1788.887990	155.656882	48.232154
1785.308948	157.682593	48.237159
1781.457178	161.379153	48.242164
1778.007988	159.207553	48.247169
1774.887512	151.640617	48.252173
1771.330690	168.166145	48.257178
1768.317631	154.518307	48.262183
1764.709213	147.474881	48.267188
1761.135581	149.442093	48.272193
1757.556218	157.940644	48.277197
1753.762576	160.073585	48.282202
1749.994909	157.739706	48.287207
1746.528323	156.406531	48.292212
1742.929075	159.777896	48.297217
1739.852909	151.417465	48.302221
1736.377858	145.760532	48.307226
1733.024285	149.032177	48.312231
1729.782890	156.580408	48.317236
1725.892770	157.772296	48.322241
1722.348740	158.828082	48.327245
1718.776950	160.156848	48.332250
1715.647579	158.635390	48.337255
1711.895075	157.330499	48.342260
1708.183938	155.697298	48.347265
1704.908879	146.813979	48.352269
1701.212754	163.776059	48.357274
1697.944104	156.208490	48.362279
1694.429611	156.156701	48.367284
1690.629432	156.023414	48.372289
1687.381299	152.940230	48.377293
1683.743832	149.915474	48.382298
1680.467010	149.449559	48.387303
1676.781931	160.339432	48.392308
1673.247371	162.804828	48.397313
1670.085916	155.798887	48.402317
1666.299408	155.059712	48.407322
1662.588289	157.800856	48.412327
1659.297279	155.536439	48.417332
1655.626354	163.232303	48.422337
1652.305614	145.484265	48.427341
1648.729349	153.641393	48.432346
1645.352267	148.975100	48.437351
1641.856261	157.414535	48.442356
1638.127379	146.118921	48.447361
1634.975670	146.783943	48.452365
1631.296140	152.081865	48.457370
1627.788414	150.349502	48.462375
1624.247584	153.623863	48.467380
1620.677340	157.043409	48.472385
1617.410617	144.263613	48.477389
1613.780104	160.622282	48.482394
1610.730139	144.650197	48.487399
1607.040281	151.695073	48.492404
1603.180692	147.435205	48.497409
1599.663900	146.340969	48.502413
1596.061992	146.629360	48.507418
1592.425354	152.791828	48.512423
1589.479952	150.661189	48.517428
1585.902862	149.559203	48.522433
1582.431805	145.453190	48.527437
1578.110435	154.672433	48.532442
1575.062081	141.849567	48.537447
1572.075124	148.615523	48.542452
1568.241821	149.860301	48.547457
1564.953054	146.976162	48.552461
1561.256408	148.743325	48.557466
1557.541876	153.661524	48.562471
1553.794738	140.889420	48.567476
1550.480016	154.953861	48.572481
1547.517336	148.494444	48.577485
1543.656309	156.240664	48.582490
1540.132615	142.261138	48.587495
1536.671493	154.464339	48.592500
1533.121520	151.295766	48.597505
1529.996470	144.780210	48.602509
1526.144903	151.077432	48.607514
1522.766831	147.061826	48.612519
1519.091737	147.993296	48.617524
1515.735929	145.933529	48.622529
1512.333323	149.210718	48.627533
1508.615795	146.442123	48.632538
1505.249467	150.239789	48.637543
1501.849851	149.529956	48.642548
1498.108999	156.118858	48.647553
1494.871764	143.811443	48.652557
1491.132221	147.109592	48.657562
1487.377097	143.879375	48.662567
1483.999365	145.043953	48.667572
1480.871273	144.680228	48.672577
1477.605793	137.667046	48.677581
1473.665769	151.293941	48.682586
1470.395442	140.642736	48.687591
1466.657009	143.597560	48.692596
1462.760991	142.479902	48.697601
1459.664031	136.618253	48.702605
1456.232779	137.774758	48.707610
1452.572931	136.501323	48.712615
1448.999518	145.877064	48.717620
1445.254056	144.554487	48.722625
1442.064774	144.300199	48.727629
1438.318869	153.763364	48.732634
1434.867732	151.000785	48.737639
1431.549394	142.986849	48.742644
1428.628521	146.632954	48.747649
1425.426893	140.117559	48.752653
1421.203681	149.190633	48.757658
1417.648924	148.784644	48.762663
1414.343428	138.689885	48.767668
1410.308839	149.242669	48.772673
1406.990821	137.416223	48.777677
1403.515165	144.898358	48.782682
1400.069452	141.292102	48.787687
1396.260842	144.483786	48.792692
1392.802048	151.259050	48.797697
1389.645180	136.526800	48.802701
1386.100680	143.808627	48.807706
1382.715911	139.561603	48.812711
1378.829119	138.744616	48.817716
1375.548525	146.850753	48.822721
1372.215274	143.088132	48.827725
1368.457471	148.437544	48.832730
1364.965870	139.806338	48.837735
1361.519105	144.634910	48.842740
1358.148661	150.830583	48.847745
1354.847053	149.545379	48.852749
1350.939426	147.935042	48.857754
1347.322388	144.327452	48.862759
1343.807050	144.958687	48.867764
1340.615563	143.642997	48.872769
1337.079333	142.765933	48.877773
1333.315185	152.904921	48.882778
1330.110625	147.645331	48.887783
1326.826653	133.693564	48.892788
1323.029741	142.516843	48.897793
1319.328132	144.681097	48.902797
1315.967319	148.265670	48.907802
1312.217309	138.624802	48.912807
1308.909196	150.257755	48.917812
1305.269049	146.150443	48.922817
1302.035121	144.200096	48.927821
1298.357361	140.309782	48.932826
1294.860190	153.141530	48.937831
1291.745765	148.998729	48.942836
1287.877351	153.731939	48.947841
1284.838356	136.751160	48.952845
1281.208217	146.277933	48.957850
1277.600816	142.036950	48.962855
1274.089423	150.275972	48.967860
1270.449075	147.315232	48.972865
1267.057493	143.474764	48.977869
1262.855406	145.760568	48.982874
1259.485753	138.325204	48.987879
1256.457272	137.976511	48.992884
1252.772563	145.165871	48.997889
1249.567473	139.382524	49.002893
1245.935026	155.910302	49.007898
1241.881121	140.369928	49.012903
1238.850105	143.193797	49.017908
1235.578436	137.354216	49.022913
1232.331597	149.262205	49.027917
1228.522444	144.665991	49.032922
1225.446526	142.117034	49.037927
1221.691857	141.156728	49.042932
1217.895990	146.503512	49.047937
1214.311292	141.313402	49.052941
1210.532811	139.676851	49.057946
1207.545129	141.280943	49.062951
1203.934768	135.931119	49.067956
1200.159281	146.964041	49.072961
1196.924585	138.164681	49.077965
1193.584739	147.558515	49.082970
1189.804292	144.914135	49.087975
1186.263011	144.527235	49.092980
1183.012419	138.832401	49.097985
1179.710098	138.515384	49.102989
1175.552056	143.795011	49.107994
1172.205041	143.460354	49.112999
1168.787430	138.224612	49.118004
1165.263493	143.358990	49.123009
1161.961165	138.898196	49.128013
1158.213599	139.262258	49.133018
1154.696217	136.712996	49.138023
1151.208490	141.056586	49.143028
1147.656159	138.189700	49.148033
1144.682454	134.683956	49.153037
1140.851280	138.214889	49.158042
1137.511980	132.649861	49.163047
1133.831873	137.346049	49.168052
1130.285568	141.939332	49.173057
1126.929727	132.992800	49.178061
1122.975041	136.841229	49.183066
1119.809558	141.427577	49.188071
1116.239269	129.956048	49.193076
1112.925612	142.769119	49.198081
1109.543437	131.512063	49.203085
1105.891442	140.584792	49.208090
1102.612577	138.551693	49.213095
1098.891092	141.214358	49.218100
1095.340454	147.336733	49.223105
1091.744837	138.387195	49.228109
1088.321956	132.267960	49.233114
1085.054809	133.527597	49.238119
1081.506690	136.577884	49.243124
1077.512727	141.760923	49.248129
1074.307319	131.338298	49.253133
1070.571827	135.422529	49.258138
1066.966708	135.058171	49.263143
1063.632648	127.854285	49.268148
1060.376261	142.243457	49.273153
1057.142243	137.117265	49.278157
1053.386134	140.886241	49.283162
1049.519922	140.964624	49.288167
1046.148933	142.704863	49.293172
1042.405058	140.975514	49.298177
1039.137267	131.663994	49.303181
1035.978719	142.957575	49.308186
1032.511664	139.770190	49.313191
1028.951153	137.363966	49.318196
1025.047286	138.015361	49.323201
1021.673012	139.506737	49.328205
1018.158722	137.377407	49.333210
1015.163158	135.168711	49.338215
1011.445049	134.561887	49.343220
1007.401870	138.092608	49.348225
1004.014885	131.435488	49.353229
1000.218729	131.971157	49.358234
997.409817	139.965360	49.363239
994.065574	134.312089	49.368244
990.234107	139.413389	49.373249
986.972914	133.457448	49.378253
982.933493	142.420725	49.383258
979.500345	132.615548	49.388263
976.202063	136.306644	49.393268
972.365178	145.234151	49.398273
969.266950	139.317088	49.403277
965.443974	139.595579	49.408282
962.316912	132.787422	49.413287
958.822292	132.505466	49.418292
954.822568	140.704425	49.423297
951.732619	132.340664	49.428301
948.369475	137.720859	49.433306
944.760138	138.094944	49.438311
941.595744	139.804536	49.443316
937.704075	132.467166	49.448321
934.208944	132.422117	49.453325
930.284341	139.141070	49.458330
927.540497	129.489524	49.463335
923.572720	139.775129	49.468340
919.882769	136.027912	49.473345
916.657590	124.495372	49.478349
912.990360	138.034050	49.483354
909.330134	135.140109	49.488359
905.965337	131.912783	49.493364
902.340492	150.055113	49.498369
899.574332	133.344370	49.503373
895.819853	136.079990	49.508378
892.576566	135.179578	49.513383
888.779461	131.841093	49.518388
884.980139	130.385135	49.523393
881.449972	135.634057	49.528397
877.774274	139.388074	49.533402
874.354178	124.012126	49.538407
870.893827	122.264899	49.543412
867.425822	133.822678	49.548417
864.337640	135.877249	49.553421
860.629514	125.812563	49.558426
856.694358	133.712789	49.563431
853.853938	125.917063	49.568436
850.164838	130.016094	49.573441
846.898935	126.191266	49.578445
842.946551	131.163194	49.583450
839.619085	131.196960	49.588455
836.018714	119.475379	49.593460
832.617848	132.966353	49.598465
829.214892	122.950108	49.603469
825.566474	130.969709	49.608474
822.007959	128.733059	49.613479
818.615629	123.933111	49.618484
814.727912	129.205919	49.623489
811.451171	124.858019	49.628493
807.844244	134.856896	49.633498
804.591214	132.449574	49.638503
801.403916	136.175276	49.643508
797.233684	136.339307	49.648513
794.232698	127.741291	49.653517
790.197028	127.844513	49.658522
786.975111	132.492579	49.663527
783.522265	127.782430	49.668532
779.954715	129.964397	49.673537
776.433302	124.219385	49.678541
773.009675	130.687589	49.683546
769.660697	126.723491	49.688551
766.147595	115.272645	49.693556
762.386968	130.888665	49.698561
758.974850	127.870807	49.703565
755.555423	136.191079	49.708570
752.054138	127.620704	49.713575
748.482311	125.567879	49.718580
744.932129	129.609412	49.723585
741.857154	118.638384	49.728589
737.892657	136.133325	49.733594
733.939654	128.980015	49.738599
730.962236	127.516819	49.743604
727.552826	126.784826	49.748609
724.105610	123.992655	49.753613
720.584455	124.545696	49.758618
716.771751	122.670235	49.763623
713.426436	122.977024	49.768628
709.646841	121.802127	49.773633
706.600371	118.740387	49.778637
702.777858	124.824757	49.783642
699.874112	124.210906	49.788647
696.088798	121.255856	49.793652
692.329789	129.193097	49.798657
688.922713	118.069663	49.803661
685.165476	123.397496	49.808666
681.744231	117.777633	49.813671
678.245184	126.187352	49.818676
674.879187	124.683934	49.823681
671.444330	124.462176	49.828685
667.505953	119.878338	49.833690
664.114892	121.912116	49.838695
661.093695	114.449080	49.843700
657.393709	128.765752	49.848705
654.339336	116.654756	49.853709
650.905207	126.198438	49.858714
647.026423	119.797369	49.863719
643.191354	125.604459	49.868724
639.919208	126.909699	49.873729
636.400223	124.212998	49.878733
632.783377	126.259035	49.883738
629.323214	122.573810	49.888743
625.972446	116.578617	49.893748
621.909163	118.514879	49.898753
618.777652	108.625461	49.903757
615.248909	128.575564	49.908762
611.725626	123.389869	49.913767
608.395893	124.950573	49.918772
604.728813	129.867863	49.923777
601.547020	122.348071	49.928781
597.849259	130.423029	49.933786
594.349545	131.373209	49.938791
591.081438	124.441993	49.943796
586.999588	136.708326	49.948801
584.003356	121.650851	49.953805
580.322983	120.120593	49.958810
576.596802	128.083863	49.963815
573.067343	121.130156	49.968820
569.562237	135.818285	49.973825
566.501151	128.562438	49.978829
562.855116	136.561354	49.983834
559.322964	136.197199	49.988839
556.133439	132.224381	49.993844
552.229287	134.846461	49.998849
548.707533	125.302114	50.003853
545.013601	128.017753	50.008858
541.240103	123.684909	50.013863
538.480325	124.652367	50.018868
534.879558	121.299998	50.023873
531.666274	117.685953	50.028877
527.786567	131.645811	50.033882
523.938179	129.813375	50.038887
520.693643	119.929591	50.043892
517.378979	127.257640	50.048897
513.672025	127.201191	50.053901
510.448035	139.770113	50.058906
506.709756	124.994203	50.063911
503.262594	127.704617	50.068916
499.580225	127.664029	50.073921
496.213251	128.140957	50.078925
492.652103	127.229943	50.083930
489.203099	120.678342	50.088935
485.872878	115.539249	50.093940
482.172534	135.461914	50.098945
479.026896	122.207900	50.103949
475.123094	132.722065	50.108954
471.467429	120.175940	50.113959
467.739764	118.288981	50.118964
464.407704	125.050463	50.123969
461.356140	123.175932	50.128973
458.038568	125.290234	50.133978
454.422429	123.478299	50.138983
450.776025	117.727931	50.143988
446.822403	126.480333	50.148993
443.563450	120.505386	50.153997
439.988333	129.465470	50.159002
436.683390	126.028938	50.164007
433.314311	127.094122	50.169012
429.996391	127.681557	50.174017
426.415662	123.820997	50.179021
422.793489	125.929486	50.184026
419.106993	119.893956	50.189031
415.678949	123.021784	50.194036
411.844571	126.175668	50.199041
408.565472	118.154226	50.204045
404.975158	126.618799	50.209050
401.305305	114.662371	50.214055
398.029045	117.518930	50.219060
394.565754	118.403255	50.224065
391.330435	129.305704	50.229069
387.238522	131.718987	50.234074
384.316163	121.180946	50.239079
380.873417	125.417287	50.244084
377.000819	130.102331	50.249089
373.665123	117.550922	50.254093
369.885600	126.483451	50.259098
366.272960	127.639275	50.264103
363.307063	128.773903	50.269108
360.019267	121.117435	50.274113
356.196048	125.409106	50.279117
352.358576	116.573146	50.284122
348.813971	118.007761	50.289127
345.539707	121.446948	50.294132
341.843242	115.946543	50.299137
338.395506	112.578818	50.304141
334.954950	119.860240	50.309146
331.637858	113.144018	50.314151
328.147094	117.736471	50.319156
324.144366	124.152464	50.324161
320.997255	120.757308	50.329165
317.571899	116.730351	50.334170
314.174847	119.792736	50.339175
310.736304	124.125724	50.344180
307.164257	126.576849	50.349185
303.771803	114.996340	50.354189
300.106058	123.144978	50.359194
296.436129	118.894051	50.364199
292.923714	124.463765	50.369204
289.411400	119.763583	50.374209
286.374890	116.932407	50.379213
282.440109	123.208296	50.384218
278.786434	123.994711	50.389223
275.623956	116.393084	50.394228
271.903780	123.878289	50.399233
268.562175	115.583804	50.404237
265.106197	122.486606	50.409242
261.496974	129.031263	50.414247
258.249869	125.189047	50.419252
254.439470	129.982869	50.424257
250.930140	126.125027	50.429261
247.347208	121.732023	50.434266
243.942877	119.099337	50.439271
240.569385	118.415695	50.444276
237.012817	132.565433	50.449281
233.447273	108.983295	50.454285
229.938614	129.691249	50.459290
226.301713	121.794549	50.464295
222.717647	120.869253	50.469300
219.404094	120.427860	50.474305
215.799639	119.305076	50.479309
212.614492	124.194947	50.484314
209.159772	113.029016	50.489319
205.485978	119.538075	50.494324
201.569217	119.885806	50.499329
198.165456	113.314944	50.504333
195.028769	115.243922	50.509338
191.638872	116.616669	50.514343
188.048147	116.671470	50.519348
184.123768	116.716202	50.524353
181.085480	117.844847	50.529357
177.033363	116.831413	50.534362
174.044635	117.485735	50.539367
170.558995	126.897672	50.544372
167.037237	118.638353	50.549377
163.670705	111.651287	50.554381
159.936925	117.284934	50.559386
156.278277	118.755059	50.564391
152.647895	120.633108	50.569396
148.846346	130.951804	50.574401
146.066031	121.576528	50.579405
142.446281	122.688560	50.584410
138.698004	121.938434	50.589415
135.529690	118.214663	50.594420
132.085942	127.308481	50.599425
128.548685	121.718105	50.604429
124.991507	120.558744	50.609434
121.114850	123.003240	50.614439
118.105342	118.648277	50.619444
114.129436	127.706423	50.624449
110.541845	119.447644	50.629453
107.093090	124.129416	50.634458
104.039275	120.874445	50.639463
100.908552	117.057238	50.644468
96.914682	122.340891	50.649473
93.408066	121.250314	50.654477
89.302492	120.463517	50.659482
85.928339	126.423056	50.664487
82.887876	118.524873	50.669492
79.383972	121.110912	50.674497
76.091428	116.090266	50.679501
72.283700	119.231377	50.684506
68.749861	121.223899	50.689511
65.142627	119.936166	50.694516
61.529132	121.229767	50.699521
58.016401	126.374694	50.704525
55.161636	121.321959	50.709530
51.565308	123.741249	50.714535
48.198457	121.379769	50.719540
43.944857	128.876093	50.724545
41.139197	117.448152	50.729549
37.040634	131.272159	50.734554
33.653698	116.699091	50.739559
30.373243	120.891403	50.744564
26.583728	120.665646	50.749569
23.228857	127.082604	50.754573
19.795518	121.011144	50.759578
16.201556	124.824607	50.764583
13.021387	121.821987	50.769588
8.832702	121.340749	50.774593
5.351493	118.048962	50.779597
2.386697	121.206326	50.784602