Fri Jun 17 18:17:42 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.050106	80.850102	0.000000
0.126967	80.531501	0.005005
0.214248	78.145325	0.010010
0.348057	66.199678	0.015014
-0.079488	58.672408	0.020019
-0.476180	53.850924	0.025024
-0.625131	46.952813	0.030029
-1.445537	37.098038	0.035034
-1.016799	32.610587	0.040038
-1.742151	33.156034	0.045043
-1.806343	28.964814	0.050048
-1.518982	18.861598	0.055053
-2.464879	9.957512	0.060058
-2.430985	6.144850	0.065062
-3.332879	11.615366	0.070067
-4.201643	9.328513	0.075072
-4.565956	22.461940	0.080077
-4.619742	13.990707	0.085082
-4.118809	7.941640	0.090086
-4.337218	16.318277	0.095091
-4.841413	11.366284	0.100096
-4.557304	8.736064	0.105101
-5.497262	13.193112	0.110106
-6.017396	8.468922	0.115110
-6.570682	10.269196	0.120115
-5.708963	10.139618	0.125120
-6.031846	9.956132	0.130125
-6.404522	15.986715	0.135130
-6.553443	19.260720	0.140134
-6.854015	21.325837	0.145139
-7.695810	15.212635	0.150144
-7.814588	10.462384	0.155149
-8.231498	18.755986	0.160154
-8.049281	11.300645	0.165158
-8.361662	18.181561	0.170163
-8.411553	7.639507	0.175168
-8.353579	17.428860	0.180173
-9.178784	9.798404	0.185178
-9.445734	6.549788	0.190182
-9.749754	15.443645	0.195187
-9.840953	12.296645	0.200192
-9.320989	13.759484	0.205197
-10.249508	16.238977	0.210202
-10.849239	15.693233	0.215206
-11.416312	14.161140	0.220211
-11.410499	23.224511	0.225216
-11.371314	15.220294	0.230221
-11.409840	21.915195	0.235226
-11.325008	8.872692	0.240230
-12.142356	14.564768	0.245235
-12.452522	20.973109	0.250240
-12.382809	11.058215	0.255245
-12.857836	14.908160	0.260250
-12.610579	19.282133	0.265254
-13.544936	19.148978	0.270259
-14.217173	20.012769	0.275264
-14.482078	13.997064	0.280269
-14.567145	20.386934	0.285274
-14.364670	14.766146	0.290278
-14.236274	15.472392	0.295283
-14.368690	15.761028	0.300288
-14.589085	13.129021	0.305293
-15.331247	19.772752	0.310298
-15.150541	7.257956	0.315302
-15.371396	13.300204	0.320307
-16.169650	19.122108	0.325312
-16.732288	14.088271	0.330317
-17.326517	10.345677	0.335322
-17.424111	13.386787	0.340326
-17.568089	19.394355	0.345331
-17.282438	14.712644	0.350336
-17.372506	14.644377	0.355341
-17.384940	11.794683	0.360346
-17.462372	14.274002	0.365350
-18.446345	17.581037	0.370355
-18.966286	6.564989	0.375360
-18.945611	12.886171	0.380365
-19.231478	13.760925	0.385370
-19.167501	17.956390	0.390374
-19.242633	15.357464	0.395379
-20.022378	13.898017	0.400384
-20.110947	12.199171	0.405389
-20.601192	11.704887	0.410394
-20.611625	8.057062	0.415398
-20.658768	13.454968	0.420403
-20.834383	14.445777	0.425408
-21.386884	7.794529	0.430413
-21.772358	13.169148	0.435418
-21.937976	14.646092	0.440422
-22.106201	16.564302	0.445427
-22.425574	12.386298	0.450432
-22.282558	15.175286	0.455437
-23.287132	24.855918	0.460442
-23.504671	10.896565	0.465446
-23.690711	18.755951	0.470451
-23.650391	4.563124	0.475456
-23.624860	10.863567	0.480461
-23.810756	18.184419	0.485466
-23.808538	15.146998	0.490470
-24.635745	22.151179	0.495475
-25.038142	12.026461	0.500480
-24.900527	14.063735	0.505485
-25.201919	10.404481	0.510490
-25.459019	12.368049	0.515494
-26.182134	8.727588	0.520499
-26.504374	9.544256	0.525504
-26.137935	9.714849	0.530509
-26.913032	13.702878	0.535514
-26.815208	8.080346	0.540518
-26.719018	10.357945	0.545523
-27.310585	9.015810	0.550528
-27.654289	1.206271	0.555533
-28.136066	16.305666	0.560538
-28.175301	1.749562	0.565542
-28.501813	10.640445	0.570547
-28.669077	19.406199	0.575552
-28.297739	9.276007	0.580557
-29.433778	25.846322	0.585562
-29.427359	11.021950	0.590566
-29.630950	17.091521	0.595571
-29.760010	16.142151	0.600576
-29.621615	12.206153	0.605581
-31.045919	19.608930	0.610586
-31.356410	10.613050	0.615590
-31.099007	12.012181	0.620595
-31.046329	13.862100	0.625600
-31.068734	10.172655	0.630605
-31.744140	17.858434	0.635610
-31.743545	16.004072	0.640614
-31.824091	13.323366	0.645619
-32.534660	12.405733	0.650624
-32.564483	3.688009	0.655629
-33.157511	16.393948	0.660634
-33.116560	13.045020	0.665638
-33.348111	16.508579	0.670643
-33.585637	15.946638	0.675648
-33.643748	12.130720	0.680653
-34.580578	13.372178	0.685658
-34.700313	12.334631	0.690662
-34.950146	18.939546	0.695667
-35.118788	13.533968	0.700672
-34.868802	9.895345	0.705677
-35.410349	11.598362	0.710682
-35.149580	9.802576	0.715686
-35.671419	8.759645	0.720691
-36.424612	23.007697	0.725696
-36.376502	11.042795	0.730701
-36.705319	9.733353	0.735706
-36.683496	3.785630	0.740710
-37.472849	12.222634	0.745715
-37.893703	8.739523	0.750720
-38.083476	10.476023	0.755725
-38.397867	19.849141	0.760730
-38.242434	18.477557	0.765734
-38.336300	19.077881	0.770739
-38.464757	19.457618	0.775744
-38.435169	13.545698	0.780749
-38.950888	19.513236	0.785754
-39.598702	15.424558	0.790758
-39.881690	11.670094	0.795763
-39.996999	20.200480	0.800768
-40.007180	15.854068	0.805773
-40.106023	26.547799	0.810778
-40.274554	16.517011	0.815782
-40.764163	18.657951	0.820787
-40.921610	10.973142	0.825792
-40.932725	16.015195	0.830797
-42.249047	18.162921	0.835802
-42.615474	23.777290	0.840806
-42.198806	13.816565	0.845811
-42.645089	22.087031	0.850816
-42.705501	20.167233	0.855821
-42.931310	19.735358	0.860826
-42.980879	17.972212	0.865830
-43.172373	20.411489	0.870835
-43.807459	17.794545	0.875840
-44.155050	14.969977	0.880845
-44.440943	26.793132	0.885850
-44.325297	14.885277	0.890854
-44.303204	24.476556	0.895859
-44.221163	27.123145	0.900864
-44.909645	16.744464	0.905869
-45.941702	27.443545	0.910874
-45.591341	13.634483	0.915878
-45.807642	22.085954	0.920883
-46.104810	9.213707	0.925888
-46.340612	8.619908	0.930893
-47.127114	18.228377	0.935898
-47.480278	15.564571	0.940902
-47.581676	18.016499	0.945907
-47.726778	21.299538	0.950912
-47.571289	20.785931	0.955917
-47.677807	20.150317	0.960922
-47.835878	15.015099	0.965926
-47.870053	18.317586	0.970931
-48.701646	13.328857	0.975936
-49.182901	22.305456	0.980941
-49.418302	16.006223	0.985946
-49.257665	19.173323	0.990950
-49.583307	22.023045	0.995955
-50.134367	29.918642	1.000960
-50.264139	18.908580	1.005965
-50.978983	25.226525	1.010970
-50.789158	15.104796	1.015974
-50.945546	18.587632	1.020979
-51.070296	23.252932	1.025984
-51.083365	12.119877	1.030989
-51.332438	19.523848	1.035994
-51.692581	16.924151	1.040998
-52.129841	14.750479	1.046003
-52.084273	20.346485	1.051008
-52.530931	8.175138	1.056013
-53.459662	18.993787	1.061018
-53.755648	17.747165	1.066022
-53.938003	17.200721	1.071027
-54.049671	15.125858	1.076032
-53.867447	14.602676	1.081037
-54.301469	22.523411	1.086042
-54.357653	11.969975	1.091046
-54.485966	5.133577	1.096051
-54.499530	18.035638	1.101056
-55.195717	12.058873	1.106061
-55.371541	23.308643	1.111066
-55.705743	12.354076	1.116070
-55.869580	20.750254	1.121075
-56.012526	15.356390	1.126080
-57.123780	13.794589	1.131085
-57.345529	17.446349	1.136090
-56.431362	12.403634	1.141094
-57.231189	11.656339	1.146099
-57.354082	16.065392	1.151104
-57.396135	6.749625	1.156109
-57.933387	18.640011	1.161114
-58.378395	19.302256	1.166118
-58.829064	22.482765	1.171123
-59.016580	14.137957	1.176128
-58.592436	14.475169	1.181133
-58.959122	14.157286	1.186138
-59.064292	13.086142	1.191142
-59.796427	15.679025	1.196147
-60.222495	12.528099	1.201152
-60.194746	12.268376	1.206157
-60.868249	17.885442	1.211162
-60.597759	19.798213	1.216166
-60.540574	16.081725	1.221171
-61.193701	20.808413	1.226176
-61.716793	6.478764	1.231181
-62.275423	14.422774	1.236186
-62.222149	8.020308	1.241190
-62.336894	10.614556	1.246195
-62.176030	4.169936	1.251200
-62.132596	11.080106	1.256205
-63.116845	9.142990	1.261210
-63.335049	13.177373	1.266214
-63.814278	17.552916	1.271219
-63.927607	20.555401	1.276224
-63.574649	12.322619	1.281229
-64.039138	14.777085	1.286234
-64.323207	14.639049	1.291238
-64.960166	8.285017	1.296243
-65.656787	8.135838	1.301248
-65.404443	6.914296	1.306253
-65.551667	14.393289	1.311258
-65.400745	3.872130	1.316262
-65.603419	5.428048	1.321267
-65.837232	17.809463	1.326272
-66.118520	5.488288	1.331277
-66.800873	16.577564	1.336282
-66.910096	13.041866	1.341286
-66.935513	17.432941	1.346291
-67.793135	12.160049	1.351296
-68.001342	18.277352	1.356301
-68.624018	10.078290	1.361306
-68.515791	8.112504	1.366310
-68.646292	18.639814	1.371315
-68.938587	20.451570	1.376320
-68.570289	11.286229	1.381325
-68.854998	21.696506	1.386330
-69.297206	14.652205	1.391334
-70.001433	18.400744	1.396339
-70.232569	20.355066	1.401344
-69.987974	13.324468	1.406349
-70.259605	16.360172	1.411354
-70.508043	10.088764	1.416358
-71.204614	14.363095	1.421363
-71.888748	21.804657	1.426368
-71.397595	13.367755	1.431373
-71.610133	22.864836	1.436378
-71.873321	12.156376	1.441382
-71.660329	12.503429	1.446387
-72.687917	13.171549	1.451392
-72.715882	12.494068	1.456397
-73.498694	13.829120	1.461402
-73.357900	6.524127	1.466406
-73.392818	17.976608	1.471411
-73.689089	21.360748	1.476416
-73.508209	7.532705	1.481421
-74.446282	22.795570	1.486426
-74.959693	19.055535	1.491430
-75.095530	9.612097	1.496435
-75.285174	13.448942	1.501440
-74.822968	8.036181	1.506445
-75.036811	17.604909	1.511450
-75.561436	10.128743	1.516454
-76.200718	24.899925	1.521459
-76.551109	22.912302	1.526464
-76.374140	17.238922	1.531469
-76.665387	10.468483	1.536474
-76.587957	19.758313	1.541478
-77.512380	13.728525	1.546483
-78.084645	13.072854	1.551488
-78.130591	11.257605	1.556493
-78.358863	14.312347	1.561498
-78.046531	15.608612	1.566502
-78.315473	9.168741	1.571507
-78.383289	14.659668	1.576512
-78.213689	10.901605	1.581517
-79.201939	21.228938	1.586522
-79.692174	10.458573	1.591526
-79.611633	4.829643	1.596531
-79.733056	13.413924	1.601536
-80.616316	5.949822	1.606541
-81.251516	17.755063	1.611546
-81.566109	10.334361	1.616550
-80.594270	5.088082	1.621555
-81.038178	2.898354	1.626560
-81.258723	4.136979	1.631565
-81.494769	9.408815	1.636570
-81.983629	7.727773	1.641574
-82.347300	15.355816	1.646579
-82.961514	10.680036	1.651584
-82.910612	7.860861	1.656589
-83.276448	7.931577	1.661594
-83.202991	11.118887	1.666598
-82.947909	6.027671	1.671603
-83.773064	15.148062	1.676608
-83.878626	0.981668	1.681613
-84.544448	7.222790	1.686618
-84.604775	4.240169	1.691622
-84.614627	6.734891	1.696627
-84.913106	14.770828	1.701632
-84.909817	5.327156	1.706637
-85.523069	9.412409	1.711642
-85.861924	3.049874	1.716646
-86.153535	2.277301	1.721651
-86.041477	16.810903	1.726656
-86.522778	-0.767197	1.731661
-87.432054	8.920681	1.736666
-87.506553	5.410391	1.741670
-87.586703	1.533024	1.746675
-87.917478	13.866618	1.751680
-87.592623	4.771845	1.756685
-88.023024	12.757883	1.761690
-88.008423	12.323736	1.766694
-87.949842	13.812547	1.771699
-88.541057	11.630336	1.776704
-88.984243	8.378861	1.781709
-89.141176	14.335300	1.786714
-89.447301	7.500838	1.791718
-89.511174	-1.266667	1.796723
-90.604552	11.242437	1.801728
-90.620647	2.469553	1.806733
-90.758187	3.279595	1.811738
-91.053699	11.619317	1.816742
-90.679061	6.805008	1.821747
-91.086994	8.184499	1.826752
-91.105794	3.191301	1.831757
-91.634555	10.352083	1.836762
-92.006846	10.664614	1.841766
-91.753000	11.252916	1.846771
-92.894023	11.471440	1.851776
-93.020713	4.772512	1.856781
-93.488407	12.527166	1.861786
-93.713896	9.163530	1.866790
-93.763872	12.505542	1.871795
-94.137390	8.307346	1.876800
-93.655279	3.587649	1.881805
-93.850438	10.071586	1.886810
-94.011182	11.925211	1.891814
-94.742101	3.979369	1.896819
-95.577853	15.532216	1.901824
-95.279453	6.639958	1.906829
-95.662580	14.455736	1.911834
-95.611100	11.073881	1.916838
-95.615933	11.067024	1.921843
-96.798191	14.494062	1.926848
-97.050306	12.578113	1.931853
-97.418725	16.290763	1.936858
-97.302266	10.752157	1.941862
-97.158342	19.083556	1.946867
-97.457424	20.412197	1.951872
-97.153723	11.774201	1.956877
-97.726395	14.387941	1.961882
-98.398044	15.511728	1.966886
-98.588622	14.107090	1.971891
-98.975835	19.833840	1.976896
-98.886167	7.376809	1.981901
-99.079740	17.207572	1.986906
-99.642807	12.611893	1.991910
-100.029684	23.254835	1.996915
-100.491870	16.751004	2.006912
-99.606913	20.981771	2.016909
-99.156150	13.903045	2.026906
-99.298018	12.398409	2.036902
-98.206986	20.481540	2.046899
-97.795555	13.617604	2.056896
-97.464594	11.508207	2.066893
-96.601911	14.710906	2.076890
-96.365378	15.836793	2.086886
-95.856552	22.007506	2.096883
-94.930962	13.878339	2.106880
-94.681934	16.189613	2.116877
-94.679387	18.722451	2.126874
-93.774341	14.273491	2.136870
-93.330054	9.368843	2.146867
-92.944879	11.334833	2.156864
-92.192595	9.433197	2.166861
-92.077830	4.454111	2.176858
-91.294742	5.373951	2.186854
-90.653908	7.277091	2.196851
-90.438121	13.985529	2.206848
-89.356946	8.355986	2.216845
-89.076860	13.749502	2.226842
-88.941850	16.732143	2.236838
-88.443326	12.045302	2.246835
-87.761560	13.251093	2.256832
-87.555505	13.956852	2.266829
-86.680515	10.086272	2.276826
-86.188155	7.723618	2.286822
-85.620014	7.087476	2.296819
-85.538478	9.356847	2.306816
-84.681368	14.392054	2.316813
-84.414859	11.313764	2.326810
-83.758964	8.637234	2.336806
-83.188896	12.755566	2.346803
-82.969857	9.124036	2.356800
-82.094431	5.266821	2.366797
-81.528277	11.493402	2.376794
-81.606540	11.938989	2.386790
-80.806486	-0.000006	2.396787
-80.404943	5.947488	2.406784
-79.665881	16.820299	2.416781
-78.908295	7.932889	2.426778
-78.675517	14.785505	2.436774
-78.598736	14.365795	2.446771
-77.881290	11.703337	2.456768
-77.184183	10.803128	2.466765
-76.917075	8.751767	2.476762
-76.035774	9.451380	2.486758
-75.371269	10.064927	2.496755
-75.690597	8.864625	2.506752
-74.895420	14.256886	2.516749
-74.001506	9.273150	2.526746
-73.850571	7.304722	2.536742
-73.184974	3.402566	2.546739
-72.619483	7.167396	2.556736
-72.356093	5.650518	2.566733
-71.628216	7.658531	2.576730
-70.768849	7.467935	2.586726
-70.997161	6.938109	2.596723
-70.501484	2.493981	2.606720
-69.398394	10.475137	2.616717
-69.171213	6.349487	2.626714
-68.819495	3.210603	2.636710
-68.160351	4.645597	2.646707
-67.575295	2.742127	2.656704
-67.470527	6.227305	2.666701
-66.998031	4.989624	2.676698
-65.923000	4.745989	2.686694
-65.741173	5.159603	2.696691
-65.158727	2.433246	2.706688
-64.541461	9.860333	2.716685
-64.625248	3.017077	2.726682
-63.696183	1.060178	2.736678
-63.081198	6.204592	2.746675
-62.816753	4.708285	2.756672
-61.820011	7.844450	2.766669
-61.411634	7.019506	2.776666
-61.324334	6.003131	2.786662
-61.325255	8.682754	2.796659
-60.333414	10.315746	2.806656
-59.637480	10.027448	2.816653
-58.718843	10.820836	2.826650
-58.491354	10.721051	2.836646
-58.383315	7.981481	2.846643
-57.941180	9.033480	2.856640
-56.598933	14.688676	2.866637
-56.568014	5.531246	2.876634
-56.720598	9.987638	2.886630
-55.821199	6.103128	2.896627
-55.379264	3.634856	2.906624
-54.923981	5.535257	2.916621
-54.000905	7.307318	2.926618
-53.792479	5.441758	2.936614
-52.888712	2.945124	2.946611
-52.237049	1.439183	2.956608
-52.041392	3.915222	2.966605
-51.969051	5.450329	2.976602
-51.545372	6.707523	2.986598
-50.555377	9.309368	2.996595
-50.291739	7.788893	3.006592
-49.184154	13.633063	3.016589
-49.175539	11.445266	3.026586
-48.871359	5.985591	3.036582
-48.480481	6.494069	3.046579
-47.459436	4.553892	3.056576
-47.300600	13.644358	3.066573
-46.278345	9.563186	3.076570
-46.078528	10.535929	3.086566
-45.813504	13.633688	3.096563
-45.412067	13.163767	3.106560
-44.325082	13.223020	3.116557
-43.963006	11.395935	3.126554
-43.849119	9.073079	3.136550
-43.420277	13.077377	3.146547
-43.073703	15.578914	3.156544
-42.022183	15.740087	3.166541
-41.416451	14.904271	3.176538
-41.227181	10.149303	3.186534
-40.639442	8.794271	3.196531
-39.900933	10.554536	3.206528
-39.591058	11.501477	3.216525
-38.983944	11.460105	3.226522
-38.745907	9.152770	3.236518
-37.856638	12.457760	3.246515
-37.335917	11.416760	3.256512
-37.042284	13.026521	3.266509
-37.135721	10.880780	3.276506
-36.099682	8.685209	3.286502
-35.889594	7.528887	3.296499
-34.653017	12.266504	3.306496
-34.290443	10.355761	3.316493
-34.129146	13.820482	3.326490
-34.176669	10.455342	3.336486
-33.617171	8.170643	3.346483
-32.786180	4.318256	3.356480
-32.051595	6.007057	3.366477
-31.703269	10.680117	3.376474
-31.082114	3.142349	3.386470
-29.803600	3.161077	3.396467
-30.300490	4.164864	3.406464
-30.014680	7.745218	3.416461
-29.145335	8.091382	3.426458
-28.360118	9.425606	3.436454
-28.174511	9.284773	3.446451
-27.782985	9.523645	3.456448
-26.882424	7.945117	3.466445
-26.549946	5.345274	3.476442
-26.506962	6.342506	3.486438
-25.341336	5.934849	3.496435
-24.948580	10.707416	3.506432
-24.901908	12.504438	3.516429
-24.084054	9.138111	3.526426
-23.347623	9.366086	3.536422
-23.337328	9.105021	3.546419
-22.352659	3.421001	3.556416
-21.784864	10.664669	3.566413
-21.587399	13.010007	3.576410
-21.475931	15.971869	3.586406
-20.951503	12.905045	3.596403
-20.015221	12.838797	3.606400
-19.160155	14.773718	3.616397
-18.624955	11.687520	3.626394
-18.406289	8.429088	3.636390
-18.317420	17.206761	3.646387
-18.271097	11.229604	3.656384
-17.536456	11.014307	3.666381
-16.297615	9.013634	3.676378
-16.063845	10.025587	3.686374
-15.561624	10.924951	3.696371
-15.424679	10.427669	3.706368
-14.551353	12.523548	3.716365
-14.082316	15.155488	3.726362
-13.464043	16.873111	3.736358
-12.575489	8.368784	3.746355
-12.647020	14.535999	3.756352
-12.364409	15.662137	3.766349
-11.161801	17.189970	3.776346
-11.077686	8.259999	3.786342
-11.128563	9.645866	3.796339
-9.594575	9.655924	3.806336
-9.410864	11.460201	3.816333
-9.522052	10.950815	3.826330
-8.315621	7.674216	3.836326
-7.852843	6.398443	3.846323
-8.019804	10.851496	3.856320
-6.657996	12.074279	3.866317
-6.243382	13.503498	3.876314
-6.148732	11.934254	3.886310
-5.854563	7.385513	3.896307
-5.054597	13.372112	3.906304
-4.716490	18.282592	3.916301
-4.190031	19.564794	3.926298
-3.264113	9.468666	3.936294
-3.135900	18.383839	3.946291
-3.229957	24.494737	3.956288
-2.293782	36.560621	3.966285
-1.989022	53.989909	3.976282
-1.457644	64.444638	3.986278
-1.101764	88.117758	3.996275
-0.542663	101.935500	4.006272
0.000000	97.973035	4.011277
0.410861	118.664492	4.016282
0.539073	126.046257	4.021286
0.468093	131.500065	4.026291
0.615529	133.047134	4.031296
0.738159	139.634987	4.036301
0.598084	127.900770	4.041306
0.527234	138.581444	4.046310
0.387354	134.208208	4.051315
0.681431	134.674200	4.056320
0.566483	144.530263	4.061325
0.645333	133.223380	4.066330
0.628611	138.781638	4.071334
0.775516	132.837739	4.076339
0.593365	135.082688	4.081344
0.330959	129.074217	4.086349
0.755126	144.282255	4.091354
0.820566	157.440072	4.096358
0.829089	167.183276	4.101363
1.061700	169.531168	4.106368
0.954549	171.083852	4.111373
1.054340	175.585784	4.116378
0.882768	159.249102	4.121382
0.956649	150.365662	4.126387
0.835913	136.767791	4.131392
0.770701	151.667843	4.136397
0.740578	159.027595	4.141402
0.901815	168.696875	4.146406
0.933493	164.413711	4.151411
0.904455	162.152229	4.156416
1.014480	163.272378	4.161421
1.171216	164.767783	4.166426
1.235204	166.407065	4.171430
1.145706	163.865162	4.176435
1.245778	160.284771	4.181440
1.064422	170.576150	4.186445
1.126566	169.905785	4.191450
1.160520	169.830321	4.196454
1.073126	167.291817	4.201459
1.270659	164.401473	4.206464
1.083927	156.996730	4.211469
0.829475	153.292144	4.216474
0.996735	162.769008	4.221478
0.800751	170.339456	4.226483
1.224678	173.789216	4.231488
1.004975	166.888208	4.236493
1.239603	173.836336	4.241498
1.130562	168.680875	4.246502
1.199205	170.924993	4.251507
1.507169	165.665295	4.256512
0.839484	174.854511	4.261517
0.749817	165.868994	4.266522
1.006266	167.831483	4.271526
0.993307	169.922616	4.276531
1.285952	169.048773	4.281536
1.315388	167.206372	4.286541
1.324426	166.278832	4.291546
1.127916	172.092335	4.296550
1.552615	185.860403	4.301555
1.519548	171.198129	4.306560
1.299074	178.863621	4.311565
0.961819	168.848931	4.316570
1.115140	180.303601	4.321574
1.422328	181.325270	4.326579
1.297841	192.871313	4.331584
1.421960	188.910214	4.336589
1.715341	192.345959	4.341594
1.487311	187.531327	4.346598
1.600888	196.669832	4.351603
1.734374	186.811515	4.356608
1.496328	194.300562	4.361613
1.579331	191.695646	4.366618
1.730233	197.564092	4.371622
1.645237	200.643203	4.376627
1.611465	186.093313	4.381632
1.404361	187.539478	4.386637
1.528520	184.792946	4.391642
1.405946	196.950006	4.396646
1.383745	190.392077	4.401651
1.524674	188.716830	4.406656
1.463717	192.702626	4.411661
1.784104	190.955915	4.416666
1.757568	196.707235	4.421670
1.726662	196.957493	4.426675
1.830220	194.158341	4.431680
1.749250	199.751176	4.436685
1.945241	203.666642	4.441690
1.744628	201.020263	4.446694
1.981690	198.220233	4.451699
1.750762	191.734094	4.456704
1.685379	199.234700	4.461709
1.978647	194.548512	4.466714
1.841969	187.236468	4.471718
1.289710	184.252694	4.476723
1.508261	185.888981	4.481728
1.758233	186.500634	4.486733
2.144141	182.153261	4.491738
1.754953	193.392841	4.496742
1.828373	193.504202	4.501747
2.026740	186.799504	4.506752
1.841211	194.160436	4.511757
1.814994	194.962836	4.516762
1.710193	193.272982	4.521766
1.777552	189.805370	4.526771
1.970787	187.366638	4.531776
1.783172	184.808085	4.536781
2.181374	196.290145	4.541786
1.974396	193.396977	4.546790
1.884595	190.994040	4.551795
1.983682	187.949561	4.556800
1.529710	196.846739	4.561805
1.737874	192.526735	4.566810
1.692410	196.967371	4.571814
1.539603	199.737089	4.576819
1.970216	205.501624	4.581824
1.983690	225.929534	4.586829
2.407359	222.755127	4.591834
2.236959	233.994088	4.596838
2.147007	207.891071	4.601843
2.271253	199.269575	4.606848
1.987295	199.111583	4.611853
1.951734	198.756413	4.616858
2.145660	214.732914	4.621862
2.023320	223.984449	4.626867
2.392659	230.384718	4.631872
2.218507	232.312029	4.636877
2.107095	231.704449	4.641882
2.298725	237.442217	4.646886
2.102877	235.233116	4.651891
2.712304	218.613235	4.656896
2.243559	219.579764	4.661901
2.028347	203.957327	4.666906
2.449247	203.063547	4.671910
2.705531	221.552965	4.676915
2.134552	203.536239	4.681920
1.721558	212.240925	4.686925
2.143233	216.872097	4.691930
2.321551	229.378372	4.696934
2.316577	225.751886	4.701939
2.456507	229.740216	4.706944
2.413515	234.582417	4.711949
2.709787	233.003099	4.716954
2.659537	227.785554	4.721958
2.067580	237.086539	4.726963
2.154808	228.082437	4.731968
2.006403	240.452206	4.736973
2.077209	230.804966	4.741978
1.777614	238.705636	4.746982
1.882822	239.786336	4.751987
2.351061	245.655138	4.756992
2.464283	254.694281	4.761997
2.581242	264.772945	4.767002
2.676469	263.749181	4.772006
2.119497	265.666914	4.777011
2.677230	257.499424	4.782016
2.266750	266.221877	4.787021
2.166012	263.798449	4.792026
2.467227	262.386828	4.797030
2.302412	267.715583	4.802035
2.622420	260.482504	4.807040
2.320440	263.699910	4.812045
2.702833	269.465577	4.817050
2.785914	256.534450	4.822054
2.847217	260.328067	4.827059
2.927082	261.522500	4.832064
2.617455	268.029913	4.837069
2.803595	261.985909	4.842074
2.951500	266.972015	4.847078
2.494253	268.065297	4.852083
2.870530	257.573203	4.857088
2.743868	262.842532	4.862093
3.018621	262.920036	4.867098
2.923782	263.363650	4.872102
2.731852	266.384772	4.877107
2.878706	261.478207	4.882112
2.280161	267.678641	4.887117
2.969164	264.173598	4.892122
2.818562	262.643689	4.897126
2.614724	266.476640	4.902131
2.721940	255.902384	4.907136
2.263019	259.851730	4.912141
2.617270	279.541290	4.917146
2.990084	280.678942	4.922150
3.086344	289.575096	4.927155
2.973765	285.312522	4.932160
2.869468	293.704677	4.937165
3.123211	294.988217	4.942170
3.041358	294.261466	4.947174
2.900296	295.823745	4.952179
2.897474	293.403968	4.957184
3.000553	298.349386	4.962189
3.132422	280.413082	4.967194
3.020907	296.233828	4.972198
2.779268	301.825186	4.977203
3.032494	291.766538	4.982208
2.409285	298.644973	4.987213
2.803705	298.951622	4.992218
2.779964	293.767931	4.997222
2.759408	296.521605	5.002227
3.110304	295.772851	5.007232
3.124720	292.757422	5.012237
2.972735	294.599361	5.017242
3.269606	300.727743	5.022246
3.569169	305.650965	5.027251
3.329972	299.565754	5.032256
2.986395	293.062184	5.037261
3.179999	293.895146	5.042266
3.166393	294.094380	5.047270
2.974479	304.748129	5.052275
3.464722	297.381165	5.057280
3.122895	305.454451	5.062285
3.223105	292.414677	5.067290
3.373119	298.992522	5.072294
3.062626	297.876745	5.077299
3.408129	305.937811	5.082304
3.377984	313.648103	5.087309
3.894605	310.346933	5.092314
3.674832	300.355255	5.097318
3.142362	298.645106	5.102323
3.021908	300.569815	5.107328
3.370209	297.053116	5.112333
3.255871	290.986819	5.117338
3.361548	307.950539	5.122342
3.254450	317.715423	5.127347
3.476929	314.361318	5.132352
3.759663	330.425594	5.137357
3.467071	319.097236	5.142362
3.229034	312.849619	5.147366
3.213486	313.119427	5.152371
3.731070	315.377155	5.157376
3.427595	329.152322	5.162381
3.160632	318.873462	5.167386
2.957682	329.018364	5.172390
3.221032	332.016909	5.177395
3.608317	325.269305	5.182400
3.465120	331.023293	5.187405
3.691880	327.565071	5.192410
3.481820	325.190192	5.197414
3.067036	331.496859	5.202419
3.562847	326.542338	5.207424
3.573643	325.184508	5.212429
4.011950	329.510241	5.217434
3.781754	324.463271	5.222438
3.425358	325.575905	5.227443
3.757905	321.680375	5.232448
3.590941	332.815631	5.237453
3.645089	327.671079	5.242458
3.969769	322.614763	5.247462
3.756658	325.820568	5.252467
3.761019	323.044788	5.257472
3.492746	329.745843	5.262477
3.504506	321.823183	5.267482
3.780675	327.095435	5.272486
3.447637	357.267000	5.277491
4.316456	348.371299	5.282496
4.098712	352.533958	5.287501
3.897558	332.836296	5.292506
3.750257	325.663690	5.297510
3.524836	326.781985	5.302515
4.088735	351.713471	5.307520
4.023629	349.540639	5.312525
4.011287	337.297422	5.317530
3.705854	334.894389	5.322534
3.687284	345.166917	5.327539
4.352391	351.076051	5.332544
4.004734	348.518220	5.337549
4.194424	337.096467	5.342554
4.119994	335.650978	5.347558
3.888892	320.809542	5.352563
4.231419	321.576116	5.357568
4.058617	327.199652	5.362573
4.124682	321.226099	5.367578
4.138233	325.266639	5.372582
3.875715	329.627950	5.377587
4.372381	321.467024	5.382592
4.117538	331.747438	5.387597
4.081255	321.638026	5.392602
3.847960	328.304852	5.397606
3.993280	321.576944	5.402611
4.152879	316.503865	5.407616
3.896224	322.511928	5.412621
4.096319	325.315759	5.417626
4.182664	319.245300	5.422630
3.965006	325.512098	5.427635
4.016183	334.757157	5.432640
3.760467	348.275763	5.437645
4.391328	356.300477	5.442650
4.302694	356.594471	5.447654
4.175080	366.176514	5.452659
4.459350	353.115371	5.457664
4.156217	355.839457	5.462669
3.928399	359.313324	5.467674
4.126238	356.284564	5.472678
4.061231	355.876268	5.477683
4.448881	360.063811	5.482688
4.249220	359.479182	5.487693
4.097061	361.901712	5.492698
3.955638	358.586375	5.497702
4.270592	351.676734	5.502707
4.688416	356.411399	5.507712
4.413215	354.144233	5.512717
4.103077	363.017401	5.517722
4.724198	358.043621	5.522726
4.466555	364.589005	5.527731
4.693725	351.578597	5.532736
4.170888	359.516433	5.537741
4.577200	357.123758	5.542746
4.382755	357.571302	5.547750
4.448659	355.990203	5.552755
4.604388	360.291478	5.557760
4.419205	368.719614	5.562765
4.555925	356.197638	5.567770
4.831202	357.719140	5.572774
4.461199	367.002057	5.577779
4.463354	354.488044	5.582784
4.415251	356.225108	5.587789
4.334087	349.349141	5.592794
4.417293	361.435028	5.597798
4.178672	360.536997	5.602803
4.683109	367.086154	5.607808
4.966768	372.499060	5.612813
4.621780	377.700327	5.617818
4.777674	368.670522	5.622822
4.714742	363.522330	5.627827
4.640557	355.324054	5.632832
4.449275	362.145132	5.637837
4.655288	380.232840	5.642842
4.823198	375.011940	5.647846
4.578238	385.631542	5.652851
4.680765	389.502008	5.657856
4.542168	387.647451	5.662861
4.660656	387.753888	5.667866
4.918551	387.534446	5.672870
4.422225	389.443298	5.677875
4.627881	386.056256	5.682880
4.602331	385.528724	5.687885
4.470243	386.893372	5.692890
4.583400	390.291036	5.697894
4.425650	389.378180	5.702899
4.946411	381.723918	5.707904
4.638772	392.552065	5.712909
4.927372	413.450917	5.717914
5.294203	413.131475	5.722918
4.800786	409.991453	5.727923
4.980152	396.985794	5.732928
4.773133	396.702137	5.737933
4.954082	410.969720	5.742938
5.059530	420.943247	5.747942
5.152759	416.886387	5.752947
5.219916	397.773344	5.757952
4.802817	397.371867	5.762957
4.666747	391.049846	5.767962
5.032798	397.973863	5.772966
5.250793	422.156058	5.777971
4.812993	419.618723	5.782976
5.357842	423.327669	5.787981
5.480028	416.873913	5.792986
5.221607	406.091754	5.797990
5.110694	399.301025	5.802995
4.996221	386.100310	5.808000
4.811096	392.206030	5.813005
4.877151	404.754787	5.818010
5.169442	421.019047	5.823014
5.294387	422.191594	5.828019
5.380522	418.992145	5.833024
5.661467	430.752969	5.838029
5.353655	401.958084	5.843034
4.891764	401.462227	5.848038
5.173587	402.000713	5.853043
5.256414	396.476042	5.858048
5.259473	417.369671	5.863053
5.068248	418.359941	5.868058
5.480213	423.997220	5.873062
5.226868	419.881141	5.878067
5.459504	425.391939	5.883072
4.983743	438.891944	5.888077
4.912108	420.767497	5.893082
5.304324	424.740192	5.898086
5.181621	430.708272	5.903091
5.274603	416.177354	5.908096
5.203414	421.625774	5.913101
5.013747	424.403829	5.918106
5.299584	425.880169	5.923110
5.261441	427.203158	5.928115
5.362279	419.912700	5.933120
5.220977	433.642258	5.938125
5.255518	417.683473	5.943130
5.697435	435.051826	5.948134
5.335916	434.030163	5.953139
5.387980	440.018138	5.958144
5.417266	444.147064	5.963149
5.579593	447.386792	5.968154
5.628815	450.024506	5.973158
5.548477	452.104774	5.978163
5.959690	444.525916	5.983168
5.486918	445.837476	5.988173
5.540361	435.699066	5.993178
5.678094	440.467089	5.998182
5.423695	440.819420	6.003187
5.961242	426.561121	6.008192
5.382708	434.970410	6.013197
5.501347	440.911207	6.018202
5.921816	451.213447	6.023206
5.588850	448.086413	6.028211
5.683084	430.064233	6.033216
5.462921	433.102708	6.038221
5.367259	438.619927	6.043226
5.586292	444.958639	6.048230
5.620635	458.335199	6.053235
5.735763	460.024424	6.058240
5.613854	448.835731	6.063245
5.471223	457.559356	6.068250
5.475482	454.620373	6.073254
5.136924	448.800259	6.078259
5.222356	449.538333	6.083264
5.094283	459.494656	6.088269
5.897059	454.002250	6.093274
5.698162	464.063489	6.098278
5.620616	455.215107	6.103283
5.831587	461.006180	6.108288
5.472023	461.488275	6.113293
5.775042	466.604559	6.118298
5.336082	457.526756	6.123302
5.586713	465.762529	6.128307
5.755050	458.620280	6.133312
5.393102	456.333773	6.138317
5.438591	456.013473	6.143322
5.610036	451.180511	6.148326
5.628793	457.542254	6.153331
5.498496	450.130555	6.158336
5.539891	468.774979	6.163341
5.541958	482.238227	6.168346
5.551597	494.757164	6.173350
5.580795	488.171621	6.178355
6.029780	497.703493	6.183360
5.516974	488.202625	6.188365
5.699454	485.475158	6.193370
5.795186	467.735071	6.198374
5.859608	472.867532	6.203379
5.731295	458.300737	6.208384
5.841961	462.603610	6.213389
5.805491	453.733207	6.218394
5.721724	465.477124	6.223398
5.590670	463.358256	6.228403
6.140316	456.613407	6.233408
5.697325	458.107683	6.238413
5.661107	463.214836	6.243418
5.704610	456.011048	6.248422
5.456850	465.447558	6.253427
5.409348	461.169776	6.258432
5.604776	465.943413	6.263437
5.645793	468.889349	6.268442
5.733461	463.687281	6.273446
5.463774	462.954446	6.278451
6.047060	449.586790	6.283456
5.565567	462.517670	6.288461
5.618352	457.203593	6.293466
5.439404	452.353883	6.298470
5.465504	460.991449	6.303475
5.734273	460.570693	6.308480
5.568924	468.299390	6.313485
5.456439	465.804276	6.318490
5.724543	462.881428	6.323494
5.554915	469.116817	6.328499
6.057830	460.110188	6.333504
5.615437	465.166451	6.338509
5.518046	466.923165	6.343514
5.687443	461.364546	6.348518
5.725611	462.564741	6.353523
6.078437	463.048409	6.358528
5.483700	452.613580	6.363533
5.762447	467.705211	6.368538
5.700593	464.114565	6.373542
5.401061	461.379995	6.378547
5.789609	459.744667	6.383552
5.760786	467.365818	6.388557
5.552578	465.371860	6.393562
5.774918	459.363203	6.398566
5.278303	469.362829	6.403571
5.549825	447.221994	6.408576
5.517278	469.737977	6.413581
5.674029	461.644724	6.418586
5.925001	458.517128	6.423590
5.479354	462.123523	6.428595
5.931733	460.449564	6.433600
5.360049	461.350927	6.438605
5.400041	464.572906	6.443610
5.473579	466.103481	6.448614
5.593391	472.181440	6.453619
5.905097	457.754632	6.458624
5.920608	460.420842	6.463629
5.512318	462.302638	6.468634
5.475227	466.817933	6.473638
5.166830	474.643620	6.478643
5.484898	457.278034	6.483648
5.398958	457.317612	6.488653
5.594258	466.752114	6.493658
5.637884	464.787340	6.498662
5.158921	462.081014	6.503667
5.675294	473.520749	6.508672
5.638572	492.792291	6.513677
5.800297	495.029273	6.518682
5.810003	480.008538	6.523686
5.586294	476.932998	6.528691
5.929507	456.884019	6.533696
5.333096	468.451084	6.538701
6.004061	462.622816	6.543706
6.016484	464.862112	6.548710
5.785135	472.085948	6.553715
5.583105	462.644936	6.558720
5.496070	461.473260	6.563725
5.355994	466.643260	6.568730
5.287450	462.022851	6.573734
5.460803	466.742338	6.578739
5.415046	465.562222	6.583744
5.874174	485.570279	6.588749
6.017732	479.917676	6.593754
6.069815	471.519961	6.598758
5.712012	467.737756	6.603763
5.679395	455.583853	6.608768
5.470160	466.632300	6.613773
5.521843	463.307340	6.618778
5.700325	454.194403	6.623782
5.359905	461.086094	6.628787
5.547776	462.632988	6.633792
5.440052	463.134792	6.638797
5.807666	455.887988	6.643802
5.845557	460.060086	6.648806
5.503673	465.659679	6.653811
5.944991	465.431061	6.658816
5.354072	465.804989	6.663821
5.617784	463.792583	6.668826
5.917198	457.142211	6.673830
5.596531	464.097319	6.678835
5.955508	455.897640	6.683840
5.380912	465.998237	6.688845
5.651606	462.659964	6.693850
5.487361	462.653357	6.698854
5.661116	464.531554	6.703859
5.710614	451.436336	6.708864
5.297418	461.391308	6.713869
5.359934	464.944421	6.718874
5.459478	457.700139	6.723878
5.485569	493.789344	6.728883
5.903358	481.670672	6.733888
5.893769	482.165244	6.738893
5.616972	474.655535	6.743898
5.751824	462.094515	6.748902
5.689632	461.247863	6.753907
5.850488	459.698332	6.758912
5.733504	460.509912	6.763917
5.590244	461.252846	6.768922
5.865756	455.400916	6.773926
5.471688	466.365630	6.778931
5.624566	458.078253	6.783936
5.534493	459.912289	6.788941
5.179275	464.978137	6.793946
5.280323	463.112352	6.798950
5.225890	488.798826	6.803955
5.786503	489.364584	6.808960
5.869695	505.621062	6.813965
5.790786	501.069064	6.818970
5.616346	502.790043	6.823974
5.771299	502.207247	6.828979
6.151271	486.766012	6.833984
5.979164	470.273590	6.838989
5.466569	466.196839	6.843994
5.496637	463.079516	6.848998
5.478134	469.421409	6.854003
5.808748	463.676942	6.859008
5.694035	468.067005	6.864013
5.492340	460.034711	6.869018
5.369895	463.696314	6.874022
5.568586	471.503430	6.879027
5.620629	464.124762	6.884032
5.597479	479.421687	6.889037
5.829499	471.188638	6.894042
6.118989	454.370277	6.899046
5.766935	472.825737	6.904051
5.706543	459.680894	6.909056
5.828991	458.894525	6.914061
5.513504	470.761813	6.919066
5.888270	457.145831	6.924070
5.464535	461.371963	6.929075
5.556163	466.122399	6.934080
5.679381	467.040280	6.939085
5.553993	462.398929	6.944090
5.977413	459.297136	6.949094
5.415314	458.438655	6.954099
5.751997	459.768809	6.959104
5.878253	466.932021	6.964109
5.756171	464.300566	6.969114
5.893639	465.005128	6.974118
5.652885	460.954433	6.979123
5.633642	459.484368	6.984128
5.812091	467.650048	6.989133
5.487373	471.490511	6.994138
5.811964	461.150728	6.999142
5.244177	464.763413	7.004147
5.663615	464.184019	7.009152
5.508383	465.517394	7.014157
5.947702	468.954204	7.019162
5.915664	454.327998	7.024166
5.707740	462.750492	7.029171
6.033047	456.433061	7.034176
5.839207	462.660434	7.039181
5.901601	448.850500	7.044186
5.725831	440.461863	7.049190
5.471330	437.777828	7.054195
5.413124	431.849752	7.059200
5.592427	442.869519	7.064205
5.815788	437.865131	7.069210
5.753813	439.243783	7.074214
5.311818	442.421942	7.079219
5.423127	441.600919	7.084224
5.760811	450.348308	7.089229
5.689500	464.596300	7.094234
5.732633	455.721743	7.099238
5.408977	462.418641	7.104243
5.672178	452.885115	7.109248
5.727838	469.698274	7.114253
5.631533	455.451566	7.119258
5.571996	455.369737	7.124262
5.537074	469.040205	7.129267
5.733646	458.042673	7.134272
5.649699	465.592275	7.139277
5.837302	466.588453	7.144282
6.111370	448.249240	7.149286
5.697781	441.887484	7.154291
5.706305	435.996267	7.159296
5.742660	443.453047	7.164301
5.276252	436.719020	7.169306
5.381907	431.064446	7.174310
5.385967	434.487752	7.179315
5.613462	436.301168	7.184320
5.812815	444.063167	7.189325
5.360142	449.700310	7.194330
5.766482	453.331841	7.199334
5.417662	471.675268	7.204339
5.788523	461.423304	7.209344
5.699690	467.759717	7.214349
5.639532	466.703553	7.219354
5.908331	457.942644	7.224358
5.368984	455.475264	7.229363
5.436760	448.506023	7.234368
5.823637	458.017607	7.239373
5.568035	464.021207	7.244378
5.870730	461.013676	7.249382
5.535774	450.691565	7.254387
5.663775	447.234734	7.259392
5.684685	453.842785	7.264397
5.611209	449.994383	7.269402
5.562652	448.908862	7.274406
5.544009	466.950342	7.279411
5.938748	461.997975	7.284416
5.606220	448.955007	7.289421
5.662483	443.476767	7.294426
5.810415	425.773044	7.299430
5.751905	437.215951	7.304435
5.386905	431.895941	7.309440
5.802662	442.956722	7.314445
5.657892	440.881577	7.319450
5.821127	435.406872	7.324454
5.414556	431.813540	7.329459
5.542285	434.192324	7.334464
5.458864	434.563005	7.339469
5.512626	440.850448	7.344474
5.685014	439.057071	7.349478
5.533954	450.979106	7.354483
5.858304	455.682175	7.359488
5.578953	452.680614	7.364493
5.568828	448.562976	7.369498
6.068644	448.718515	7.374502
5.630272	445.768249	7.379507
5.557632	437.780426	7.384512
5.243502	432.597791	7.389517
5.341380	448.617731	7.394522
5.829334	448.876868	7.399526
5.818550	470.006908	7.404531
5.579380	450.155573	7.409536
5.513065	463.853553	7.414541
5.896453	463.336391	7.419546
5.911444	459.451180	7.424550
5.515311	440.999395	7.429555
5.691856	431.630061	7.434560
5.576677	438.961064	7.439565
5.537824	439.126017	7.444570
5.368548	434.618460	7.449574
5.080886	456.015909	7.454579
5.545876	459.163894	7.459584
5.671947	462.138513	7.464589
5.585303	464.522149	7.469594
6.088004	469.878159	7.474598
5.944449	470.109453	7.479603
6.048636	466.679270	7.484608
5.649407	448.451569	7.489613
5.328078	444.924184	7.494618
5.283183	447.224706	7.499622
5.375037	464.394939	7.504627
5.481237	476.737970	7.509632
5.454852	472.371230	7.514637
5.384169	472.585677	7.519642
5.488080	469.573296	7.524646
5.400198	468.088589	7.529651
5.690028	466.706076	7.534656
5.667972	472.370124	7.539661
5.353196	467.208502	7.544666
5.811718	468.032962	7.549670
5.423217	485.239249	7.554675
5.565345	471.861624	7.559680
5.449941	475.066217	7.564685
5.375584	477.018806	7.569690
6.046076	465.526320	7.574694
5.546561	471.622955	7.579699
5.769593	478.922825	7.584704
5.700969	475.060191	7.589709
5.555642	474.147831	7.594714
5.838881	463.927992	7.599718
5.624861	470.421769	7.604723
5.544558	467.663389	7.609728
5.712121	474.136962	7.614733
5.634438	473.151790	7.619738
6.457566	466.181315	7.624742
5.689550	474.207716	7.629747
5.831400	466.996655	7.634752
5.629683	475.267953	7.639757
5.850935	472.501878	7.644762
5.997673	471.923408	7.649766
5.752742	478.348918	7.654771
5.850223	463.383270	7.659776
5.641629	455.911568	7.664781
5.759438	445.562158	7.669786
5.693370	445.803662	7.674790
5.370109	445.520773	7.679795
5.545969	442.294764	7.684800
5.592946	453.439145	7.689805
5.715706	463.664384	7.694810
5.515743	456.198944	7.699814
5.564372	473.773013	7.704819
5.586639	474.179014	7.709824
5.778337	462.908586	7.714829
5.704547	466.554605	7.719834
5.841272	454.026432	7.724838
5.209797	459.693889	7.729843
5.679642	463.142595	7.734848
5.934675	466.943924	7.739853
5.432606	465.742760	7.744858
5.734667	460.187351	7.749862
6.003579	464.017157	7.754867
5.973884	453.497095	7.759872
6.159133	440.193237	7.764877
5.688361	453.788528	7.769882
5.674080	448.310960	7.774886
5.290362	451.251909	7.779891
5.531948	439.372125	7.784896
5.575249	439.175917	7.789901
5.229424	440.537022	7.794906
5.336714	434.001078	7.799910
5.030304	443.284324	7.804915
5.815425	461.669360	7.809920
5.613096	462.574059	7.814925
5.790229	479.753222	7.819930
5.880734	464.828988	7.824934
5.668180	471.014877	7.829939
5.490576	446.581466	7.834944
5.889242	454.182865	7.839949
5.740697	449.212661	7.844954
6.028605	442.447780	7.849958
5.520136	443.925310	7.854963
5.622466	429.908066	7.859968
5.717875	438.502329	7.864973
5.411579	438.358308	7.869978
5.760096	445.051222	7.874982
5.329241	449.855343	7.879987
5.491470	437.609079	7.884992
5.350681	454.708645	7.889997
5.540552	471.093581	7.895002
5.624559	468.246323	7.900006
5.360687	472.103708	7.905011
5.916525	469.695044	7.910016
5.762189	470.946180	7.915021
5.736601	480.685977	7.920026
6.021318	470.141469	7.925030
5.336388	454.381755	7.930035
5.144806	457.828309	7.935040
5.432341	464.069210	7.940045
5.169663	476.966495	7.945050
5.663150	471.075370	7.950054
5.683383	473.605425	7.955059
5.847513	474.752519	7.960064
5.807004	469.131500	7.965069
5.644862	474.553220	7.970074
5.914609	469.141116	7.975078
5.588775	469.247996	7.980083
5.748421	466.977408	7.985088
5.902402	463.081329	7.990093
5.776636	478.156929	7.995098
5.804370	457.515890	8.000102
5.702008	450.213410	8.005107
5.529314	436.525638	8.010112
5.521218	441.785313	8.015130
5.111259	458.274506	8.020147
5.464287	459.950538	8.025165
5.600467	462.073398	8.030182
5.761928	467.583065	8.035200
6.059110	466.358230	8.040218
5.792665	479.580405	8.045235
6.069026	473.623269	8.050253
5.596293	464.608471	8.055270
5.251967	447.530412	8.060288
5.494046	456.597779	8.065306
5.703199	473.226385	8.070323
5.819997	463.979954	8.075341
5.657945	469.244602	8.080358
5.865871	466.728037	8.085376
5.821145	471.487799	8.090394
5.602043	471.534881	8.095411
5.969270	465.384709	8.100429
5.698348	473.295544	8.105446
5.897522	473.538039	8.110464
5.897816	457.186669	8.115482
5.604381	453.382901	8.120499
5.596129	447.432927	8.125517
5.713383	460.409833	8.130534
5.667525	460.519843	8.135552
6.000829	465.349436	8.140570
5.659310	471.706015	8.145587
5.718980	459.908307	8.150605
5.595503	470.691988	8.155622
5.532735	467.782268	8.160640
5.894910	466.737951	8.165658
5.664353	475.550257	8.170675
5.647429	460.462843	8.175693
5.362531	470.456899	8.180710
5.394449	478.749643	8.185728
5.650083	465.051037	8.190746
5.584892	469.311493	8.195763
6.138261	470.731415	8.200781
5.659574	474.874988	8.205798
5.777215	472.307489	8.210816
6.095283	478.264706	8.215834
5.528807	478.893095	8.220851
5.584800	476.804498	8.225869
5.522144	481.361949	8.230886
5.614393	490.218239	8.235904
5.929425	500.455873	8.240922
5.726137	508.367491	8.245939
6.043383	494.564927	8.250957
6.054445	502.314549	8.255974
5.908770	507.269037	8.260992
5.998052	512.345877	8.266010
5.558940	500.125970	8.271027
6.184269	505.493793	8.276045
6.133643	512.826549	8.281062
5.985769	499.472118	8.286080
5.985437	480.249448	8.291098
5.749382	478.933338	8.296115
6.189443	486.861231	8.301133
5.838783	480.334554	8.306150
5.701248	468.180875	8.311168
5.884503	491.906817	8.316186
5.828362	492.957422	8.321203
5.905662	493.274500	8.326221
5.877422	501.061556	8.331238
5.749213	506.285556	8.336256
5.792668	497.734104	8.341274
5.630074	511.138435	8.346291
5.940893	501.027332	8.351309
6.212840	507.486667	8.356326
6.149596	497.976467	8.361344
6.278655	499.114193	8.366362
6.431816	507.334838	8.371379
6.300520	497.821383	8.376397
6.073508	508.262491	8.381414
6.101821	497.830860	8.386432
5.847205	475.308064	8.391450
5.843189	488.400220	8.396467
5.976178	500.769288	8.401485
6.253576	504.379169	8.406502
6.093657	508.637666	8.411520
6.367146	491.756449	8.416538
5.950161	497.566974	8.421555
5.772851	476.619364	8.426573
5.903606	490.463062	8.431590
5.621915	502.281430	8.436608
6.343761	502.076063	8.441626
5.955565	507.228325	8.446643
6.051645	496.276622	8.451661
5.824840	504.812954	8.456678
6.064369	501.832709	8.461696
5.884242	512.522499	8.466714
5.815474	503.745034	8.471731
5.816814	507.130746	8.476749
5.829601	510.675957	8.481766
6.020638	505.744706	8.486784
5.752491	502.767943	8.491802
5.881701	519.272104	8.496819
6.184652	525.855809	8.501837
6.353681	529.127245	8.506854
6.348677	537.987719	8.511872
6.454791	527.427991	8.516890
6.030759	513.681103	8.521907
6.151574	512.352717	8.526925
5.915334	511.315151	8.531942
6.122163	525.419242	8.536960
6.232077	519.921799	8.541978
6.252311	533.824846	8.546995
6.292208	531.301162	8.552013
6.424627	528.303876	8.557030
6.127980	529.046459	8.562048
6.219099	519.564915	8.567066
6.467201	538.284952	8.572083
6.354549	521.528113	8.577101
6.283467	507.344060	8.582119
6.066646	510.937276	8.587136
6.391267	508.237544	8.592154
6.073897	516.511600	8.597171
6.093392	506.710109	8.602189
6.139233	520.958265	8.607207
6.140983	528.815148	8.612224
6.593029	533.862799	8.617242
6.187699	533.469224	8.622259
6.702540	537.573455	8.627277
6.412127	524.733396	8.632295
6.041245	506.198602	8.637312
6.376141	508.936017	8.642330
6.034245	516.816943	8.647347
6.376513	524.614076	8.652365
6.650228	538.898776	8.657383
6.410184	523.574199	8.662400
6.163661	511.384472	8.667418
6.024424	519.631873	8.672435
6.551170	527.975458	8.677453
6.315630	539.561204	8.682471
6.426287	539.940251	8.687488
6.269914	524.504728	8.692506
5.929920	534.912471	8.697523
5.852899	536.094491	8.702541
6.353191	540.918398	8.707559
6.161558	540.081074	8.712576
6.437089	534.428355	8.717594
6.381448	542.358359	8.722611
6.409151	532.851130	8.727629
6.345763	537.244758	8.732647
6.378663	537.048398	8.737664
6.565528	547.031408	8.742682
6.312587	538.517387	8.747699
6.209825	538.282951	8.752717
6.619613	537.662171	8.757735
6.754989	536.231176	8.762752
6.611079	537.872893	8.767770
6.312591	535.994964	8.772787
6.677490	537.510581	8.777805
6.595461	530.366256	8.782823
6.334179	539.900961	8.787840
6.548017	529.702228	8.792858
6.464168	531.042848	8.797875
6.763461	538.715451	8.802893
6.832336	532.067058	8.807911
6.227123	543.330034	8.812928
6.461656	540.282902	8.817946
6.499251	542.201511	8.822963
6.233620	529.047712	8.827981
6.557734	535.710573	8.832999
6.386277	533.899514	8.838016
6.723033	537.638697	8.843034
6.312361	539.293260	8.848051
6.288983	541.939456	8.853069
6.403045	538.750748	8.858087
6.538075	539.753639	8.863104
6.181360	537.943256	8.868122
6.705810	538.308837	8.873139
6.355319	542.344120	8.878157
6.392134	536.851932	8.883175
6.046801	542.620646	8.888192
6.643903	559.888540	8.893210
6.454393	567.290661	8.898227
6.738699	575.075015	8.903245
6.644216	570.569117	8.908263
6.961423	576.241108	8.913280
6.646110	552.116623	8.918298
6.603368	551.961179	8.923315
6.838640	546.521033	8.928333
6.470781	539.635609	8.933351
6.211130	543.199341	8.938368
6.945920	551.073754	8.943386
6.668723	571.036348	8.948403
6.770635	571.299538	8.953421
6.918668	562.465928	8.958439
6.806898	556.465407	8.963456
6.693539	546.188775	8.968474
6.505391	532.433173	8.973491
6.737046	538.202629	8.978509
6.794083	534.532895	8.983527
6.421144	536.617760	8.988544
6.330772	556.436105	8.993562
6.524916	573.529082	8.998579
6.784141	572.533560	9.003597
7.114014	575.246036	9.008615
6.707790	573.340934	9.013632
6.827532	574.274327	9.018650
6.868856	576.590316	9.023667
6.694654	575.756588	9.028685
6.896785	572.793569	9.033703
6.816117	580.135483	9.038720
7.096994	563.201390	9.043738
6.838775	552.818528	9.048755
6.368002	544.967226	9.053773
6.730966	544.004655	9.058791
6.727957	571.484169	9.063808
6.760601	564.673689	9.068826
6.807263	566.539814	9.073843
6.520290	568.217516	9.078861
6.859716	560.273667	9.083879
6.753100	562.377059	9.088896
6.935339	559.001245	9.093914
7.094919	561.634159	9.098931
6.621144	565.332295	9.103949
6.970139	557.848625	9.108967
6.844916	564.274400	9.113984
6.816495	552.921144	9.119002
7.091508	562.057700	9.124019
6.743231	565.282262	9.129037
6.612986	560.224094	9.134055
6.478936	566.022261	9.139072
6.858722	558.348254	9.144090
6.836575	563.904612	9.149107
6.686210	563.233837	9.154125
7.139855	567.450995	9.159143
6.736572	576.048782	9.164160
6.678606	564.905921	9.169178
6.667869	566.221992	9.174195
6.563359	568.634455	9.179213
6.644539	569.438443	9.184231
7.030317	585.149312	9.189248
7.157100	590.054998	9.194266
7.146236	603.657005	9.199283
7.195670	581.910019	9.204301
6.958688	573.083709	9.209319
7.090625	572.091234	9.214336
6.905244	566.235018	9.219354
6.949888	560.020720	9.224371
7.125771	572.322682	9.229389
7.072762	559.715355	9.234407
6.489104	573.006867	9.239424
7.212492	578.745194	9.244442
7.081684	590.769436	9.249459
6.724528	579.760537	9.254477
7.321359	595.533179	9.259495
7.073555	595.464962	9.264512
6.936601	602.162757	9.269530
7.174889	591.835718	9.274547
7.034007	593.663339	9.279565
7.296901	595.065022	9.284583
7.683617	585.487264	9.289600
7.283858	575.375330	9.294618
7.395434	569.906921	9.299635
6.613623	566.772237	9.304653
7.025170	566.669227	9.309671
6.711517	564.853652	9.314688
6.711146	570.512486	9.319706
7.225003	582.794106	9.324723
6.924615	586.339424	9.329741
7.226114	587.804959	9.334759
6.969667	591.286484	9.339776
7.245146	593.352158	9.344794
7.215923	598.489270	9.349811
7.410578	596.034333	9.354829
7.504891	595.717932	9.359847
7.119239	592.874452	9.364864
7.341400	587.252630	9.369882
7.215997	572.628766	9.374899
6.990420	571.345548	9.379917
7.296586	571.151009	9.384935
7.506092	589.795247	9.389952
7.053173	574.620360	9.394970
7.346734	566.792388	9.399987
6.759439	576.364375	9.405005
7.251358	583.059203	9.410023
7.164933	598.169299	9.415040
7.367038	581.879521	9.420058
7.629901	589.694807	9.425075
6.935179	591.450912	9.430093
7.094495	585.890909	9.435111
7.317524	588.819160	9.440128
6.972164	591.760198	9.445146
7.223807	600.342836	9.450163
6.967345	604.802035	9.455181
7.098311	597.323485	9.460199
7.361614	593.650356	9.465216
7.080501	602.042238	9.470234
7.059129	590.192749	9.475251
6.910681	609.213210	9.480269
7.055133	591.484511	9.485287
6.886053	605.804093	9.490304
7.013864	627.928775	9.495322
7.390863	620.024316	9.500339
7.331257	632.052304	9.505357
7.831988	615.851821	9.510375
7.773478	632.903007	9.515392
7.553529	637.731311	9.520410
7.900736	625.002691	9.525427
7.423101	616.086445	9.530445
7.572017	603.689396	9.535463
7.483880	593.069004	9.540480
7.419976	600.470538	9.545498
7.662596	587.399324	9.550515
7.544596	601.022679	9.555533
7.577102	586.465068	9.560551
7.389108	593.160517	9.565568
7.405092	589.953065	9.570586
7.708189	597.591800	9.575603
7.348370	598.890310	9.580621
7.781273	594.757731	9.585639
7.462306	589.851973	9.590656
7.248264	592.730637	9.595674
7.822915	591.511639	9.600691
7.303436	595.394922	9.605709
7.730746	599.416877	9.610727
7.624000	583.257362	9.615744
7.617911	593.125635	9.620762
7.804885	581.303722	9.625779
7.650057	597.579414	9.630797
7.684499	590.909359	9.635815
7.656353	590.914466	9.640832
7.412405	590.733021	9.645850
7.559056	585.904388	9.650867
7.560705	587.867359	9.655885
7.289095	598.409239	9.660903
7.449268	593.459863	9.665920
7.636435	594.075976	9.670938
7.890622	586.712765	9.675955
7.680876	596.449157	9.680973
7.543828	585.466853	9.685991
7.561881	594.081030	9.691008
7.417982	593.479054	9.696026
7.830893	590.676650	9.701043
7.656979	595.451033	9.706061
7.683064	587.439772	9.711079
7.417060	584.078617	9.716096
7.618699	593.636405	9.721114
7.473002	587.802520	9.726131
7.187375	591.576073	9.731149
7.318577	597.743513	9.736167
7.487060	589.751887	9.741184
7.688791	613.492856	9.746202
7.877178	612.897063	9.751219
7.778656	612.919379	9.756237
7.882843	603.052574	9.761255
7.301413	597.369447	9.766272
7.583987	616.691079	9.771290
7.622988	621.253720	9.776307
7.654886	631.168848	9.781325
7.888139	624.335235	9.786343
7.816439	630.819655	9.791360
7.770671	629.836242	9.796378
7.900226	629.270697	9.801395
7.695079	640.950081	9.806413
7.867659	635.980127	9.811431
7.996436	633.410948	9.816448
7.460337	640.834099	9.821466
7.883247	644.523165	9.826483
7.748711	631.961019	9.831501
7.492006	627.556667	9.836519
7.530500	625.250702	9.841536
7.312783	636.880798	9.846554
7.570160	633.276356	9.851571
7.435214	638.521794	9.856589
7.698951	633.873668	9.861607
8.150809	648.122956	9.866624
7.970863	642.305372	9.871642
8.101408	635.465204	9.876659
7.891973	627.864099	9.881677
7.863132	634.013866	9.886695
8.032651	626.362373	9.891712
7.626954	632.885183	9.896730
7.846830	623.724074	9.901747
8.018993	635.616308	9.906765
7.959764	640.071867	9.911783
8.033462	631.527715	9.916800
7.576208	642.014660	9.921818
8.032025	651.219634	9.926835
8.299576	666.255412	9.931853
8.225891	649.649819	9.936871
8.223241	637.121059	9.941888
8.075494	635.664677	9.946906
7.868683	633.951993	9.951923
7.932902	632.450146	9.956941
8.024988	635.508035	9.961959
7.992923	622.992836	9.966976
7.803045	636.360672	9.971994
7.682223	633.889273	9.977011
7.909174	639.786704	9.982029
7.673065	659.871115	9.987047
8.297188	646.709083	9.992064
8.145888	661.137170	9.997082
8.009829	658.520477	10.002099
8.059210	657.541718	10.007117
8.357646	653.787152	10.012135
8.482708	660.983503	10.017152
8.166367	658.143056	10.022170
8.439413	642.893106	10.027187
8.340200	636.324767	10.032205
8.012054	630.684955	10.037223
8.329833	630.719961	10.042240
7.958128	636.021283	10.047258
8.116607	620.274103	10.052275
7.851942	639.068466	10.057293
7.975914	634.232565	10.062311
8.246945	642.402000	10.067328
8.175000	662.305402	10.072346
8.428213	647.507918	10.077363
8.656664	637.130914	10.082381
8.194883	631.241880	10.087399
8.387303	630.583216	10.092416
8.335031	616.223117	10.097434
8.226317	622.459377	10.102451
8.064756	620.291576	10.107469
8.179555	618.532526	10.112487
8.160283	608.911808	10.117504
8.295254	628.783532	10.122522
8.114671	630.613032	10.127539
8.339357	628.168452	10.132557
8.273343	626.353634	10.137575
8.436432	627.810292	10.142592
8.255424	622.963673	10.147610
8.196441	629.592620	10.152627
8.446116	628.748471	10.157645
8.110520	629.305030	10.162663
8.095399	630.897598	10.167680
8.101229	642.120102	10.172698
8.138058	647.428126	10.177715
8.516260	655.845678	10.182733
8.442836	664.623117	10.187751
8.497066	654.067595	10.192768
8.401984	663.198210	10.197786
8.421867	656.947243	10.202803
8.199749	648.512087	10.207821
8.484502	653.077588	10.212839
8.189789	656.294447	10.217856
8.491858	663.903270	10.222874
8.490584	661.064388	10.227891
8.599758	667.192214	10.232909
8.336769	666.898194	10.237927
8.708414	657.881314	10.242944
8.422782	655.294402	10.247962
8.281562	657.633264	10.252979
8.548551	651.878978	10.257997
8.431761	663.665926	10.263015
8.420201	657.636900	10.268032
8.430598	660.347378	10.273050
8.312388	656.465622	10.278067
8.328184	653.542415	10.283085
8.244857	657.909866	10.288103
8.384600	658.139606	10.293120
8.129602	666.742912	10.298138
7.878926	663.704952	10.303155
8.344388	666.254566	10.308173
8.393182	669.346230	10.313191
8.398036	674.091318	10.318208
8.497891	692.747016	10.323226
8.836362	702.168752	10.328243
8.889899	689.800282	10.333261
8.496596	681.360688	10.338279
8.550686	668.471517	10.343296
8.528251	671.600215	10.348314
8.677720	675.551057	10.353331
8.688658	674.897558	10.358349
8.675522	673.482376	10.363367
8.634123	663.333851	10.368384
8.358272	673.616075	10.373402
8.499998	690.572828	10.378419
8.671954	697.370883	10.383437
8.717353	690.011817	10.388455
8.599908	681.151601	10.393472
8.953288	692.488803	10.398490
8.961813	688.807806	10.403507
8.661307	683.295850	10.408525
8.793574	686.579138	10.413543
8.716530	682.064207	10.418560
8.863601	673.100784	10.423578
8.868166	665.552273	10.428595
8.816251	651.287743	10.433613
8.683920	654.797664	10.438631
8.768680	661.635390	10.443648
8.648404	651.971203	10.448666
8.507087	659.549594	10.453683
8.907876	673.844202	10.458701
8.780927	686.066874	10.463719
9.031225	687.462590	10.468736
8.746682	666.038493	10.473754
8.712994	667.440073	10.478771
8.561396	664.179757	10.483789
8.551949	690.591745	10.488807
8.848961	688.996086	10.493824
8.707846	694.040419	10.498842
8.800587	695.151522	10.503859
8.868000	694.538238	10.508877
8.429602	697.456376	10.513895
8.510710	687.867937	10.518912
8.636530	692.007935	10.523930
9.039409	691.362120	10.528947
9.134319	694.278814	10.533965
8.832155	689.050770	10.538983
8.956161	694.984031	10.544000
9.241232	688.886006	10.549018
9.142822	695.738839	10.554035
9.139621	685.955574	10.559053
9.000899	691.508915	10.564071
8.758647	693.846268	10.569088
8.639311	695.170755	10.574106
8.769131	698.659553	10.579123
8.758169	681.857688	10.584141
9.020238	699.471361	10.589159
9.078918	688.540894	10.594176
8.778044	690.906690	10.599194
8.908255	696.667085	10.604211
8.915808	690.958070	10.609229
8.745911	692.190771	10.614247
9.429096	699.980343	10.619264
9.230720	711.264395	10.624282
9.171244	694.770949	10.629299
9.316887	688.289045	10.634317
8.989153	693.478953	10.639335
9.169808	690.279737	10.644352
9.343202	693.626461	10.649370
9.062818	697.407829	10.654387
9.159486	691.933982	10.659405
9.020320	695.296635	10.664423
9.206712	692.634019	10.669440
9.186792	680.811578	10.674458
9.254891	686.161265	10.679475
9.291517	693.369377	10.684493
9.269702	698.739327	10.689511
9.223937	690.114416	10.694528
9.286212	691.557524	10.699546
9.161125	692.047799	10.704563
9.098049	692.783455	10.709581
9.080415	695.956828	10.714599
9.234787	693.117462	10.719616
9.541688	689.905727	10.724634
9.213217	696.849157	10.729651
9.490169	698.596713	10.734669
8.914189	695.468141	10.739687
8.892452	690.537356	10.744704
8.934406	695.719359	10.749722
9.082884	690.988019	10.754739
8.885541	709.937209	10.759757
9.001743	710.508434	10.764775
9.447065	717.162448	10.769792
9.493046	715.287867	10.774810
9.206600	717.434751	10.779827
9.399734	709.648200	10.784845
9.446074	718.688025	10.789863
9.350796	717.611662	10.794880
9.859124	711.869206	10.799898
9.446959	707.178884	10.804915
9.383369	690.235376	10.809933
9.501099	709.179437	10.814951
9.327961	712.457984	10.819968
9.345656	704.747245	10.824986
9.436606	713.027745	10.830003
9.576918	706.667773	10.835021
9.273163	701.623242	10.840039
9.190907	711.050940	10.845056
9.437825	715.659753	10.850074
9.258808	720.526158	10.855091
9.509347	714.555506	10.860109
9.256940	708.091530	10.865127
9.276766	714.975502	10.870144
9.240912	705.335436	10.875162
9.549605	715.640404	10.880179
9.393559	712.436127	10.885197
9.463639	715.739008	10.890215
9.367402	713.570768	10.895232
9.218705	714.505680	10.900250
9.209110	725.867216	10.905267
9.249125	713.618287	10.910285
9.206063	731.131542	10.915303
9.503946	749.541223	10.920320
9.571716	745.205535	10.925338
9.637998	752.989211	10.930355
9.418286	748.543836	10.935373
9.609124	753.785948	10.940391
9.513220	756.203703	10.945408
9.465435	747.456271	10.950426
9.452278	744.802011	10.955443
9.648177	739.828936	10.960461
9.832768	743.715301	10.965479
9.899572	747.844652	10.970496
9.850434	747.512528	10.975514
9.713315	746.818285	10.980531
9.867120	748.338893	10.985549
9.916489	747.059761	10.990567
9.756528	752.968004	10.995584
9.710474	742.870197	11.000602
9.773117	750.439927	11.005619
9.898369	750.350253	11.010637
9.712535	754.086394	11.015655
9.638190	754.392661	11.020672
10.085947	752.904805	11.025690
9.744459	749.971284	11.030707
9.911848	745.868231	11.035725
9.882751	748.268188	11.040743
9.956850	737.845320	11.045760
9.680009	722.252667	11.050778
9.564353	732.322099	11.055795
9.938761	735.034879	11.060813
10.129802	745.698764	11.065831
9.717806	735.024040	11.070848
9.938701	730.369228	11.075866
9.771350	734.426676	11.080883
9.650666	730.789978	11.085901
9.996484	740.540608	11.090919
9.890815	745.342274	11.095936
10.161049	742.314167	11.100954
9.737223	739.697656	11.105971
9.622304	741.646756	11.110989
9.749231	747.929524	11.116007
9.524745	747.216537	11.121024
9.627235	750.106000	11.126042
9.837537	757.045334	11.131059
9.935067	744.217969	11.136077
9.620684	756.229547	11.141095
9.943621	753.547572	11.146112
10.183877	751.064758	11.151130
9.823210	754.913416	11.156147
9.930837	750.019964	11.161165
9.802417	751.739241	11.166183
9.825490	755.613088	11.171200
9.766363	748.454817	11.176218
9.846701	765.813557	11.181235
10.047750	763.223093	11.186253
10.236648	767.585680	11.191271
9.983530	773.017917	11.196288
10.440763	774.040690	11.201306
9.916414	775.742122	11.206323
10.319822	766.661046	11.211341
10.302145	773.719178	11.216359
10.006787	762.631575	11.221376
10.274884	752.020560	11.226394
9.905353	775.980537	11.231411
10.282935	763.702429	11.236429
10.228388	769.656145	11.241447
10.299654	783.573964	11.246464
10.222789	755.235836	11.251482
9.691509	758.847126	11.256499
10.234314	761.336071	11.261517
10.487938	764.060467	11.266535
10.260433	769.511279	11.271552
10.402919	763.678244	11.276570
10.312349	761.833439	11.281587
9.966626	758.949829	11.286605
10.340564	772.561250	11.291623
9.970430	766.564615	11.296640
10.233819	767.224362	11.301658
10.175673	772.900943	11.306675
10.108723	777.279090	11.311693
10.150481	776.393120	11.316711
10.184240	780.943491	11.321728
10.722993	769.842040	11.326746
10.367546	771.825414	11.331763
10.188433	762.513232	11.336781
10.460370	769.634832	11.341799
10.587164	772.300592	11.346816
10.752589	762.582157	11.351834
10.434352	763.562966	11.356851
10.567137	763.198439	11.361869
10.721096	765.441606	11.366887
10.514622	766.397147	11.371904
10.623911	760.259418	11.376922
10.481628	751.793614	11.381939
10.288897	751.338713	11.386957
10.106184	731.251431	11.391975
9.960353	755.532434	11.396992
10.242875	761.254350	11.402010
10.470299	775.987677	11.407027
10.535778	769.076579	11.412045
10.478008	771.002209	11.417063
10.167383	776.045020	11.422080
10.602055	774.335535	11.427098
10.296145	774.144112	11.432115
10.704612	772.675578	11.437133
10.892635	770.726599	11.442151
10.952127	773.841306	11.447168
10.725255	775.150211	11.452186
10.603729	769.605523	11.457203
10.267808	768.419363	11.462221
10.504378	760.703120	11.467239
10.557975	770.202952	11.472256
10.475201	760.047856	11.477274
10.506410	772.281512	11.482291
10.320063	765.018600	11.487309
10.820391	756.442444	11.492327
10.320153	766.485077	11.497344
10.186648	766.043166	11.502362
10.474588	772.150375	11.507379
10.715225	784.049845	11.512397
11.127385	789.717353	11.517415
10.594369	790.544900	11.522432
10.866337	778.843149	11.527450
10.435740	773.116777	11.532467
10.914154	790.741836	11.537485
10.940643	786.894063	11.542503
10.548703	790.066090	11.547520
10.938350	785.605835	11.552538
10.923715	791.872980	11.557555
10.490353	781.106900	11.562573
10.990675	779.541806	11.567591
10.909263	786.416655	11.572608
11.067011	772.417733	11.577626
10.812260	777.139668	11.582643
10.620928	772.974586	11.587661
10.919439	778.342303	11.592679
10.995046	787.592641	11.597696
11.146462	780.005297	11.602714
10.756667	779.925643	11.607731
10.932141	769.303241	11.612749
11.124593	778.467032	11.617767
10.919230	771.691296	11.622784
10.972041	763.287343	11.627802
11.140953	775.974258	11.632819
10.766815	770.949669	11.637837
10.975927	777.466605	11.642855
10.542541	775.646496	11.647872
10.761633	778.818530	11.652890
10.650498	794.129168	11.657907
10.907865	798.821893	11.662925
11.205341	804.167352	11.667943
10.901841	807.005810	11.672960
10.776322	813.876389	11.677978
10.815129	801.231755	11.682995
10.561657	806.242441	11.688013
11.380891	805.864796	11.693031
10.876831	805.146112	11.698048
11.053685	799.116815	11.703066
11.120666	810.298768	11.708083
11.103078	798.125287	11.713101
11.596675	790.521416	11.718119
10.977361	803.710003	11.723136
10.749993	802.587287	11.728154
10.851956	794.500321	11.733171
11.021424	795.205795	11.738189
11.148479	804.796187	11.743207
10.762073	810.084855	11.748224
11.365402	814.444120	11.753242
11.502132	824.652949	11.758259
11.474179	818.317946	11.763277
11.208144	802.899189	11.768295
10.907380	807.320537	11.773312
11.458990	798.384286	11.778330
11.243708	801.225401	11.783347
11.181626	795.680666	11.788365
11.320406	798.964077	11.793383
11.565253	798.122493	11.798400
11.263344	790.273115	11.803418
11.351875	799.038474	11.808435
11.193061	807.025720	11.813453
11.286614	795.770508	11.818471
10.925608	806.493122	11.823488
11.009920	812.738515	11.828506
11.376864	824.537698	11.833523
11.394822	828.842697	11.838541
11.766017	840.249482	11.843559
11.241513	831.995183	11.848576
11.317828	831.581776	11.853594
11.659924	825.971231	11.858611
11.501721	827.303960	11.863629
11.687902	821.145948	11.868647
11.221438	821.066635	11.873664
11.495355	823.600282	11.878682
11.625569	822.039616	11.883699
11.360833	823.111529	11.888717
11.792430	820.655165	11.893735
11.343735	817.522143	11.898752
11.429139	820.521538	11.903770
11.452114	822.634920	11.908787
11.322589	824.754753	11.913805
11.805982	820.199975	11.918823
11.768336	822.823986	11.923840
11.541139	830.032313	11.928858
11.634501	827.976431	11.933875
11.529034	837.245675	11.938893
11.757715	822.070634	11.943911
11.677489	820.147141	11.948928
11.812855	822.874866	11.953946
11.912746	807.109087	11.958963
11.643689	793.404098	11.963981
11.635059	789.298796	11.968999
11.732770	793.066160	11.974016
11.454521	789.788681	11.979034
11.486214	796.514037	11.984051
11.401346	812.763564	11.989069
11.785083	824.899498	11.994087
11.482485	822.867896	11.999104
11.639602	827.966633	12.004122
11.685080	813.487946	12.009139
11.513082	818.854751	12.014157
11.890629	821.274134	12.019175
11.465363	825.925023	12.024192
11.394719	827.623682	12.029210
11.853384	809.297274	12.034227
11.686187	826.802925	12.039245
11.981713	817.601572	12.044263
11.904238	820.419590	12.049280
11.788353	819.694847	12.054298
12.033280	834.644793	12.059315
11.373799	812.257690	12.064333
11.769846	821.337081	12.069351
11.508449	826.578404	12.074368
11.903756	842.189336	12.079386
12.197673	849.747248	12.084403
11.948538	860.596964	12.089421
12.241659	845.173609	12.094439
11.982708	841.299058	12.099456
11.731625	833.776815	12.104474
11.740623	829.377845	12.109491
11.801319	851.674817	12.114509
12.316365	852.314196	12.119527
12.348901	868.582847	12.124544
12.211327	850.434028	12.129562
11.803739	832.436400	12.134579
11.550864	839.087624	12.139597
12.187003	850.069897	12.144615
12.329211	851.660746	12.149632
12.056822	851.277936	12.154650
11.903764	843.541969	12.159667
11.879695	858.055187	12.164685
12.281029	858.170985	12.169703
12.151889	861.297575	12.174720
11.956516	857.523862	12.179738
12.270339	866.746857	12.184755
12.175564	875.091578	12.189773
12.085852	855.077450	12.194791
12.105381	862.093418	12.199808
11.959071	866.728858	12.204826
11.985168	859.019598	12.209843
11.856376	861.936500	12.214861
11.818893	858.266653	12.219879
11.909123	858.092057	12.224896
12.221717	859.312487	12.229914
12.353225	858.656065	12.234931
12.056101	861.060039	12.239949
12.218757	862.223112	12.244967
12.435926	856.853185	12.249984
11.851433	867.562596	12.255002
12.613448	874.643338	12.260019
12.314025	881.485375	12.265037
12.152112	874.751974	12.270055
12.245696	883.500795	12.275072
12.222235	890.727450	12.280090
12.616837	891.814968	12.285107
12.594656	894.557278	12.290125
12.451347	882.551073	12.295143
12.819334	879.089793	12.300160
12.110362	880.444585	12.305178
12.341828	874.418779	12.310195
12.698965	886.441278	12.315213
12.515790	885.826528	12.320231
12.746590	863.623836	12.325248
12.363636	862.722827	12.330266
12.420660	858.120999	12.335283
12.047972	860.124373	12.340301
12.720975	883.680941	12.345319
12.585211	886.022079	12.350336
12.585851	898.424879	12.355354
12.812365	887.171910	12.360371
12.622015	885.334029	12.365389
12.844488	872.247226	12.370407
12.478059	871.449565	12.375424
12.120469	868.398627	12.380442
12.730357	866.647216	12.385459
12.414110	888.794112	12.390477
12.422575	880.111857	12.395495
12.574131	888.863249	12.400512
12.538322	900.159983	12.405530
12.718899	885.308995	12.410547
12.811065	886.339701	12.415565
12.899022	888.019093	12.420583
13.012676	892.774116	12.425600
12.769835	887.720777	12.430618
12.627944	886.296860	12.435635
12.628482	884.850057	12.440653
12.673925	881.246337	12.445671
12.774633	880.473782	12.450688
12.836436	892.182405	12.455706
13.094668	884.430417	12.460723
12.685860	887.691679	12.465741
12.539493	889.229714	12.470759
12.639361	891.957447	12.475776
12.471227	898.469227	12.480794
13.151203	889.186020	12.485811
12.972083	890.700368	12.490829
12.657918	885.505352	12.495847
12.688754	886.211236	12.500864
12.957084	885.436409	12.505882
12.771559	888.382233	12.510899
12.460185	884.686844	12.515917
12.578763	885.163986	12.520935
12.817308	883.371545	12.525952
12.483532	906.298883	12.530970
12.751004	908.414747	12.535987
13.113813	923.939437	12.541005
13.626435	921.255826	12.546023
13.177736	919.075671	12.551040
13.034223	924.882630	12.556058
13.221840	902.229414	12.561075
13.304998	902.587255	12.566093
13.069038	890.608844	12.571111
13.234135	883.935843	12.576128
12.752396	885.352664	12.581146
12.982460	890.044640	12.586163
13.006200	907.865867	12.591181
13.136924	923.358467	12.596199
13.062327	924.362566	12.601216
13.000881	928.991005	12.606234
13.177377	920.961462	12.611251
13.134670	921.385496	12.616269
13.187267	920.944929	12.621287
13.429083	918.653352	12.626304
13.494082	923.610946	12.631322
13.278024	911.074721	12.636339
13.470025	922.516862	12.641357
13.336417	903.450258	12.646375
13.192712	895.861125	12.651392
13.266912	900.881352	12.656410
13.338180	905.570004	12.661427
13.277823	907.593711	12.666445
13.365544	910.905316	12.671463
13.459783	909.114220	12.676480
13.337766	909.083358	12.681498
13.767370	899.788219	12.686515
13.821938	891.906507	12.691533
13.714368	887.810340	12.696551
13.632647	883.376830	12.701568
13.318528	889.566438	12.706586
13.557103	869.271169	12.711603
13.366650	883.182582	12.716621
13.109347	884.127288	12.721639
13.749896	877.933888	12.726656
13.057115	881.485440	12.731674
13.381791	874.904809	12.736691
13.411808	885.125903	12.741709
13.200234	885.527614	12.746727
13.420642	878.435609	12.751744
13.503528	911.032188	12.756762
13.518774	911.170231	12.761779
13.388126	911.170330	12.766797
13.573820	910.526551	12.771815
13.564674	901.475583	12.776832
13.645208	920.767204	12.781850
13.979973	904.631996	12.786867
13.691688	910.188621	12.791885
13.571219	914.178485	12.796903
13.626614	906.634793	12.801920
13.490861	917.550344	12.806938
13.786174	904.221108	12.811955
13.638266	904.592159	12.816973
13.630219	907.878345	12.821991
13.657683	907.645879	12.827008
13.613254	916.408602	12.832026
13.316041	916.397608	12.837043
13.719276	906.318516	12.842061
13.884508	909.626686	12.847079
13.783135	904.415585	12.852096
13.460294	916.499946	12.857114
13.440447	911.887062	12.862131
13.613947	909.351346	12.867149
13.448449	919.188649	12.872167
13.812197	906.557634	12.877184
13.654963	923.606061	12.882202
13.947933	928.465928	12.887219
14.151089	945.604667	12.892237
13.814731	942.523809	12.897255
14.078888	925.797008	12.902272
13.563747	936.445139	12.907290
13.730466	934.636088	12.912307
13.736131	940.379679	12.917325
13.876860	945.488462	12.922343
14.250740	932.148703	12.927360
13.802598	952.353767	12.932378
13.958561	937.562132	12.937395
14.171024	949.192809	12.942413
14.114344	946.282774	12.947431
13.824396	945.447989	12.952448
14.140923	948.351124	12.957466
13.996594	943.936664	12.962483
14.270606	949.514011	12.967501
14.145616	943.803903	12.972519
14.582044	937.858566	12.977536
14.311255	947.139606	12.982554
14.357117	943.537179	12.987571
14.317989	943.949006	12.992589
14.285895	941.341164	12.997607
14.366917	929.024427	13.002624
14.245598	923.480634	13.007642
14.207663	912.536148	13.012659
13.908277	911.361816	13.017677
13.915400	926.671629	13.022695
13.873899	934.817383	13.027712
14.173271	941.753807	13.032730
14.252354	942.240074	13.037747
14.223508	934.393265	13.042765
14.294574	941.297954	13.047783
14.338074	933.636155	13.052800
14.221318	938.365516	13.057818
14.174258	948.567969	13.062835
14.036363	940.768216	13.067853
14.081492	946.870580	13.072871
14.350600	932.827416	13.077888
14.174940	938.008663	13.082906
14.156465	961.551153	13.087923
14.685125	962.896692	13.092941
14.294540	967.502687	13.097959
14.431785	963.568750	13.102976
14.730602	968.483757	13.107994
14.514957	971.550146	13.113011
14.783643	966.740086	13.118029
14.482453	957.158332	13.123047
14.501957	957.527936	13.128064
14.335970	964.604113	13.133082
14.667758	965.391861	13.138099
14.885159	965.405760	13.143117
14.783852	956.910397	13.148135
14.798584	934.594902	13.153152
14.763244	941.679864	13.158170
14.272545	937.887701	13.163187
14.272008	936.159989	13.168205
14.489896	963.760363	13.173223
14.741443	962.002954	13.178240
14.501627	972.413433	13.183258
14.430447	976.195527	13.188275
14.690456	966.708866	13.193293
14.597170	975.023867	13.198311
14.840232	970.845977	13.203328
14.774706	968.289354	13.208346
14.760054	979.675340	13.213363
14.689447	970.495186	13.218381
14.655767	980.156494	13.223399
14.874699	965.436447	13.228416
14.687268	966.492372	13.233434
14.682951	972.402976	13.238451
14.727834	965.829050	13.243469
14.555935	975.496794	13.248487
14.782290	974.991915	13.253504
14.405378	978.612634	13.258522
14.718022	984.538275	13.263539
15.341383	990.393378	13.268557
15.336914	992.714481	13.273575
15.412923	981.309304	13.278592
14.962980	977.822935	13.283610
14.719348	974.600683	13.288627
15.115085	966.974412	13.293645
14.837538	978.855637	13.298663
14.783658	969.155414	13.303680
14.952576	979.612129	13.308698
15.250561	986.107099	13.313715
15.276861	984.137929	13.318733
14.952599	984.368225	13.323751
14.923541	976.524776	13.328768
15.338591	988.650321	13.333786
15.025605	993.118631	13.338803
15.104694	979.593000	13.343821
15.260794	993.875624	13.348839
15.503632	993.858919	13.353856
15.359173	979.135482	13.358874
15.340609	974.487329	13.363891
15.229105	965.528528	13.368909
15.030422	966.446174	13.373927
14.900564	964.291951	13.378944
15.101204	973.151367	13.383962
15.226226	992.510875	13.388979
15.336776	987.967628	13.393997
15.323403	990.730340	13.399015
15.543175	988.743578	13.404032
15.410669	997.921355	13.409050
15.510740	995.888350	13.414067
15.668094	993.630878	13.419085
15.443802	982.108301	13.424103
15.459063	967.266996	13.429120
15.630445	970.171427	13.434138
15.117744	969.794108	13.439155
15.238020	962.291177	13.444173
15.192929	969.191170	13.449191
15.363169	979.236274	13.454208
15.236649	991.118784	13.459226
15.183303	988.248342	13.464243
15.775628	982.251488	13.469261
15.295811	991.247237	13.474279
15.554053	979.031509	13.479296
15.590929	991.591146	13.484314
15.369001	994.309000	13.489331
15.563146	988.185029	13.494349
15.546530	995.544839	13.499367
15.437483	994.320557	13.504384
15.436483	1001.887997	13.509402
15.418719	997.618814	13.514419
15.800160	989.059928	13.519437
15.453129	998.962293	13.524455
15.675689	992.432836	13.529472
15.692985	995.512872	13.534490
15.422917	998.288724	13.539507
16.155901	1000.367975	13.544525
15.643194	996.816054	13.549543
15.520247	995.645655	13.554560
15.764007	1004.099128	13.559578
15.825992	1019.989839	13.564595
16.321073	1018.434058	13.569613
15.758583	1004.696949	13.574631
15.761268	999.997228	13.579648
15.851452	992.576050	13.584666
15.644375	998.572724	13.589683
15.711846	1013.788544	13.594701
15.742418	1018.078113	13.599719
16.247389	1018.723308	13.604736
16.652889	1016.680479	13.609754
15.917179	1005.053133	13.614771
16.101813	985.333572	13.619789
15.921696	986.763454	13.624807
16.125445	983.911302	13.629824
16.071972	985.370920	13.634842
15.576856	995.585672	13.639859
15.961079	1001.271090	13.644877
16.177015	1017.191720	13.649895
16.120052	1017.573247	13.654912
15.795551	1005.113036	13.659930
15.982724	1012.736208	13.664947
16.069548	1010.725875	13.669965
16.174794	1019.948789	13.674983
16.429577	1014.246986	13.680000
16.601621	1020.606614	13.685018
16.171992	1014.026893	13.690035
16.317882	1001.768407	13.695053
16.255412	997.764512	13.700071
16.286954	1004.720677	13.705088
16.163135	1001.053335	13.710106
16.167966	1011.879842	13.715123
16.541427	1003.320307	13.720141
16.045037	1006.551073	13.725159
16.365371	1006.557312	13.730176
16.394752	1006.286339	13.735194
16.240352	1019.353745	13.740211
16.685980	1011.253047	13.745229
16.110872	1009.311789	13.750247
16.347898	1014.918927	13.755264
16.177330	1008.564639	13.760282
16.002546	1012.416321	13.765299
16.315105	1000.650968	13.770317
16.564761	1015.768404	13.775335
16.555892	1011.388690	13.780352
16.471377	998.774037	13.785370
16.281114	1012.074155	13.790387
16.398324	1006.670400	13.795405
16.735457	1012.733705	13.800423
16.232389	1002.213293	13.805440
16.564406	1005.843346	13.810458
16.349813	1009.222540	13.815475
16.528806	1012.372155	13.820493
16.637891	1014.187804	13.825511
16.382060	1008.755899	13.830528
16.480176	1007.140908	13.835546
16.392870	1012.757860	13.840563
16.802199	1018.599732	13.845581
17.144652	1028.697343	13.850599
17.208045	1012.220143	13.855616
17.029850	1010.417626	13.860634
16.773191	1017.379181	13.865651
16.946301	998.890182	13.870669
17.189089	1006.591504	13.875687
16.874452	1004.008172	13.880704
16.981370	1005.288387	13.885722
17.032953	1006.386079	13.890739
17.113762	1000.122289	13.895757
17.104188	1001.265970	13.900775
16.959806	993.107843	13.905792
17.161062	993.080728	13.910810
17.054401	983.466035	13.915827
16.977921	973.634928	13.920845
16.637908	959.851039	13.925863
16.837098	981.413416	13.930880
17.103362	973.595289	13.935898
17.303745	993.032031	13.940915
16.971029	977.739529	13.945933
17.193281	972.317540	13.950951
16.968234	971.165293	13.955968
16.670795	957.166668	13.960986
16.830368	982.739108	13.966003
17.412054	981.730711	13.971021
17.397596	997.277435	13.976039
17.163675	991.428534	13.981056
17.296998	967.979178	13.986074
17.035425	969.017899	13.991091
17.131918	973.045335	13.996109
17.177445	968.996728	14.001127
17.276948	972.600856	14.006144
17.366105	968.009993	14.011162
17.201167	972.854452	14.016179
17.409295	979.602134	14.021197
16.985886	977.916751	14.026215
17.054223	981.956742	14.031232
17.595278	988.088500	14.036250
17.152700	993.166894	14.041267
17.432778	1000.701789	14.046285
17.491634	995.555359	14.051303
17.076069	995.670918	14.056320
17.217766	995.496625	14.061338
16.994019	1000.968545	14.066355
17.297347	994.598879	14.071373
17.563859	985.133566	14.076391
17.475563	991.931702	14.081408
17.453369	988.327782	14.086426
17.507017	991.707268	14.091443
17.498459	990.039147	14.096461
17.336323	992.866346	14.101479
17.173391	993.399729	14.106496
17.451001	992.898141	14.111514
17.361379	992.794576	14.116531
17.484358	991.063257	14.121549
17.735022	986.514044	14.126567
17.390881	1000.943988	14.131584
17.509581	1005.378739	14.136602
17.540296	1029.819794	14.141619
17.465623	1015.341007	14.146637
17.730662	1015.745783	14.151655
17.387453	1022.398123	14.156672
17.833727	1009.821217	14.161690
17.763457	1031.000917	14.166707
17.713348	1023.223537	14.171725
17.752024	1017.462776	14.176743
17.343130	1023.382773	14.181760
17.737447	1018.236875	14.186778
17.696280	1026.827870	14.191795
17.686119	1021.224427	14.196813
17.829100	1027.699118	14.201831
17.835596	1024.544724	14.206848
17.574694	1022.656746	14.211866
17.751204	1026.707115	14.216883
17.617905	1026.897799	14.221901
18.093413	1036.547736	14.226919
17.975045	1052.944019	14.231936
18.368141	1041.693564	14.236954
18.088520	1022.335352	14.241971
17.978617	1015.722174	14.246989
18.202414	1007.324117	14.252007
18.086152	1023.075570	14.257024
18.004385	1011.070256	14.262042
17.887361	1024.794011	14.267059
17.967085	1014.763305	14.272077
17.871188	1016.846474	14.277095
18.155117	1047.192347	14.282112
18.477043	1047.021167	14.287130
18.006783	1053.938717	14.292147
17.795663	1039.958148	14.297165
18.290064	1042.941968	14.302183
18.309150	1050.312798	14.307200
18.250121	1047.139764	14.312218
18.487686	1052.254731	14.317235
18.147874	1059.167137	14.322253
18.398766	1046.635272	14.327271
18.066831	1050.525681	14.332288
18.102574	1040.932950	14.337306
17.994781	1047.991817	14.342323
18.208150	1044.571553	14.347341
18.265522	1036.263342	14.352359
18.039715	1049.627270	14.357376
18.507844	1036.084563	14.362394
18.457415	1036.431543	14.367411
18.283892	1040.914873	14.372429
18.716892	1041.135050	14.377447
18.519465	1053.191981	14.382464
18.516452	1039.938588	14.387482
18.247103	1050.848486	14.392499
18.306802	1059.701064	14.397517
18.625467	1065.744627	14.402535
18.380900	1063.292544	14.407552
18.773349	1067.028310	14.412570
18.670710	1069.140951	14.417587
18.872920	1068.625910	14.422605
19.339136	1059.895424	14.427623
19.009688	1048.556012	14.432640
18.886460	1031.259466	14.437658
19.117311	1032.862765	14.442675
18.631505	1029.275658	14.447693
18.930521	1030.717243	14.452711
18.531145	1027.941311	14.457728
18.931301	1031.775387	14.462746
19.092206	1030.190901	14.467763
18.653392	1031.470883	14.472781
18.873744	1028.610845	14.477799
18.687794	1028.689815	14.482816
18.760436	1026.844031	14.487834
19.012506	1030.988529	14.492851
18.419801	1031.189431	14.497869
19.215854	1028.755331	14.502887
18.830369	1041.531262	14.507904
19.104408	1030.213207	14.512922
19.122037	1028.652140	14.517939
19.027287	1033.451883	14.522957
19.242281	1022.797938	14.527975
19.014821	1027.843345	14.532992
19.003635	1024.110036	14.538010
19.109163	1030.681105	14.543027
18.880993	1021.527108	14.548045
18.892535	1020.593786	14.553063
18.814040	1042.777169	14.558080
19.008007	1049.022936	14.563098
19.002777	1048.042403	14.568115
18.955637	1067.592815	14.573133
19.480415	1061.794942	14.578151
19.276025	1063.713090	14.583168
18.940467	1064.815685	14.588186
19.228476	1058.746948	14.593203
19.082368	1065.294504	14.598221
19.287976	1057.723017	14.603239
19.211402	1064.263740	14.608256
19.389449	1058.349098	14.613274
19.191529	1058.740275	14.618291
19.030800	1066.435076	14.623309
19.205790	1054.330364	14.628327
19.515936	1069.145690	14.633344
19.170907	1061.362981	14.638362
19.481746	1055.714835	14.643379
19.232781	1063.426268	14.648397
19.454832	1062.131204	14.653415
19.408972	1093.111080	14.658432
20.011070	1088.879784	14.663450
19.949200	1076.323505	14.668467
19.567370	1069.238601	14.673485
19.686128	1049.716116	14.678503
19.757175	1058.245173	14.683520
19.767000	1059.596645	14.688538
19.885036	1055.491871	14.693555
19.723771	1050.630419	14.698573
20.020802	1052.537269	14.703591
19.716028	1059.827687	14.708608
19.959032	1049.383622	14.713626
19.754464	1044.887221	14.718643
19.737084	1047.038048	14.723661
19.982724	1050.741914	14.728679
19.726804	1059.124146	14.733696
19.802078	1056.155547	14.738714
19.705335	1057.290887	14.743731
19.486709	1060.727451	14.748749
19.893589	1047.692523	14.753767
19.592975	1048.680261	14.758784
19.556156	1053.549118	14.763802
19.941954	1050.497021	14.768819
19.464528	1058.080291	14.773837
19.883539	1070.587503	14.778855
20.020730	1087.109841	14.783872
19.936257	1079.520418	14.788890
19.915962	1084.495980	14.793907
19.764658	1078.865191	14.798925
20.372828	1075.300961	14.803943
20.434670	1082.500536	14.808960
20.075831	1081.316190	14.813978
20.219234	1072.196069	14.818995
20.111826	1084.715200	14.824013
20.447981	1084.951868	14.829031
20.319989	1072.962061	14.834048
20.044338	1077.183259	14.839066
20.629042	1081.803951	14.844083
20.310639	1085.235452	14.849101
20.596123	1068.992916	14.854119
20.250366	1053.080102	14.859136
19.953121	1047.370043	14.864154
20.365012	1063.347516	14.869171
20.098641	1076.741043	14.874189
20.669794	1082.480064	14.879207
20.401284	1076.836080	14.884224
20.522289	1080.644916	14.889242
20.378120	1080.435462	14.894259
20.252633	1077.697853	14.899277
20.324448	1074.242058	14.904295
20.556448	1072.834716	14.909312
20.225777	1082.760005	14.914330
20.484598	1073.495904	14.919347
20.500496	1081.558971	14.924365
20.470481	1075.800549	14.929383
20.437457	1082.556470	14.934400
20.295495	1075.820256	14.939418
20.570532	1080.816412	14.944435
20.796814	1080.433977	14.949453
20.589083	1076.908115	14.954471
20.284012	1079.555555	14.959488
20.079830	1079.565512	14.964506
20.678207	1078.428752	14.969523
20.584893	1100.466658	14.974541
20.847352	1089.192215	14.979559
20.970333	1098.920468	14.984576
21.055459	1094.393225	14.989594
21.347942	1098.738100	14.994611
20.772590	1084.729056	14.999629
20.870949	1076.702183	15.004647
20.714893	1074.768821	15.009664
20.589125	1081.368118	15.014682
21.044005	1078.681678	15.019699
20.739925	1093.192445	15.024717
21.161624	1096.539521	15.029735
21.250500	1096.197638	15.034752
21.073970	1094.410581	15.039770
21.053658	1089.227675	15.044787
21.108939	1086.634813	15.049805
20.879407	1076.674756	15.054823
21.416588	1095.695828	15.059840
21.044259	1095.534531	15.064858
21.559409	1089.374490	15.069875
20.916954	1086.964126	15.074893
20.869280	1076.451039	15.079911
21.140607	1093.753800	15.084928
21.018850	1096.505019	15.089946
21.196106	1092.746278	15.094963
21.045222	1095.070080	15.099981
21.226400	1088.869882	15.104999
21.238141	1093.046468	15.110016
20.970420	1091.933979	15.115034
21.142882	1091.938026	15.120051
20.929596	1091.736910	15.125069
20.832900	1088.980341	15.130087
21.459080	1100.783498	15.135104
21.311060	1114.045188	15.140122
21.439803	1119.182201	15.145139
21.462019	1118.309695	15.150157
21.758232	1118.913612	15.155175
21.774744	1114.906401	15.160192
21.319993	1114.543460	15.165210
21.805455	1104.033078	15.170227
21.385654	1115.006213	15.175245
21.385489	1107.305919	15.180263
21.551649	1109.855753	15.185280
21.636666	1109.631433	15.190298
21.910553	1109.690666	15.195315
21.998214	1116.599762	15.200333
22.148491	1093.565091	15.205351
21.775065	1087.742096	15.210368
21.584881	1083.727517	15.215386
21.687411	1070.973061	15.220403
21.529617	1072.625606	15.225421
21.893970	1079.157615	15.230439
21.827409	1076.254709	15.235456
21.538048	1075.145818	15.240474
22.042126	1091.493410	15.245491
21.909285	1105.944234	15.250509
21.956582	1107.809532	15.255527
22.058191	1096.768892	15.260544
21.997673	1101.579501	15.265562
22.010819	1088.350546	15.270579
22.094643	1080.385138	15.275597
21.976172	1080.384393	15.280615
21.986404	1079.528053	15.285632
21.823293	1101.013420	15.290650
21.930729	1091.965010	15.295667
22.007813	1105.669567	15.300685
21.906149	1096.754327	15.305703
22.159450	1104.133496	15.310720
22.167043	1108.548163	15.315738
22.245930	1094.696105	15.320755
22.280257	1095.525427	15.325773
22.084819	1105.200314	15.330791
22.607205	1095.402265	15.335808
22.408017	1098.343902	15.340826
22.476406	1101.035174	15.345843
22.314482	1106.398042	15.350861
22.427624	1105.892293	15.355879
22.257211	1100.565835	15.360896
21.999490	1097.030168	15.365914
22.474964	1096.246099	15.370931
22.577510	1104.474688	15.375949
22.297777	1102.143004	15.380967
22.335877	1102.984691	15.385984
22.183361	1102.369166	15.391002
22.434804	1106.517333	15.396019
22.370846	1092.031575	15.401037
22.403144	1106.438025	15.406055
22.416761	1090.268209	15.411072
22.149545	1101.754921	15.416090
22.436420	1108.552954	15.421107
22.737882	1124.758676	15.426125
22.539666	1131.639313	15.431143
22.591109	1123.721783	15.436160
22.281069	1134.210573	15.441178
22.360226	1126.633692	15.446195
22.837944	1125.315420	15.451213
22.813789	1125.636382	15.456231
23.081479	1129.994441	15.461248
22.832812	1127.697351	15.466266
23.015328	1130.294073	15.471283
22.878685	1123.451448	15.476301
22.970817	1125.497869	15.481319
23.036741	1124.603531	15.486336
23.024935	1134.539238	15.491354
23.173918	1134.473569	15.496371
23.212214	1132.153192	15.501389
22.742694	1120.423251	15.506407
23.259758	1125.694533	15.511424
22.972570	1129.565320	15.516442
23.019677	1129.808693	15.521459
23.186929	1122.432515	15.526477
22.939434	1130.136257	15.531495
22.895490	1128.612578	15.536512
22.766589	1126.589267	15.541530
23.152470	1138.381214	15.546547
22.973752	1127.495800	15.551565
23.025419	1132.925534	15.556583
23.091473	1129.287230	15.561600
23.128744	1134.568184	15.566618
23.413083	1144.573962	15.571635
23.391922	1149.270570	15.576653
23.034536	1155.105288	15.581671
23.807463	1154.324926	15.586688
23.503195	1146.515715	15.591706
23.346271	1128.706577	15.596723
23.357925	1122.829801	15.601741
23.265660	1146.141937	15.606759
23.445467	1144.568470	15.611776
23.613338	1153.440916	15.616794
23.822989	1138.479348	15.621811
23.665274	1126.959769	15.626829
23.443141	1118.833000	15.631847
23.620756	1119.626304	15.636864
23.716979	1150.485836	15.641882
23.841521	1137.482011	15.646899
23.596025	1121.467034	15.651917
23.368566	1127.139998	15.656935
23.860796	1133.757463	15.661952
23.625884	1146.902134	15.666970
23.834766	1148.700819	15.671987
23.882155	1144.061336	15.677005
23.767114	1151.910782	15.682023
24.085089	1154.240913	15.687040
23.956825	1151.571071	15.692058
24.154983	1144.473983	15.697075
23.919423	1130.273389	15.702093
23.916318	1114.294113	15.707111
23.857713	1110.475756	15.712128
23.751870	1124.758734	15.717146
23.954229	1125.937669	15.722163
24.188352	1130.550899	15.727181
23.729785	1148.371862	15.732199
23.963495	1143.424655	15.737216
24.144271	1143.885563	15.742234
24.268536	1146.262061	15.747251
24.278070	1147.736417	15.752269
24.149723	1147.101127	15.757287
24.061186	1141.845688	15.762304
24.301730	1142.778527	15.767322
24.041519	1147.466049	15.772339
24.318244	1144.822593	15.777357
24.273691	1145.174897	15.782375
24.253517	1140.736399	15.787392
24.300394	1139.101959	15.792410
24.041589	1138.795816	15.797427
24.413721	1138.958398	15.802445
24.017993	1153.552167	15.807463
24.268763	1146.628608	15.812480
24.196019	1155.638679	15.817498
24.208876	1150.486064	15.822515
24.448841	1142.747416	15.827533
24.413625	1148.368358	15.832551
24.624062	1153.223315	15.837568
24.312881	1165.116178	15.842586
24.517603	1173.855353	15.847603
24.939745	1176.546108	15.852621
24.604175	1180.195038	15.857639
24.653426	1171.462536	15.862656
24.578479	1167.577987	15.867674
24.638008	1174.463833	15.872691
24.974932	1171.957210	15.877709
24.756598	1168.575995	15.882727
24.629729	1161.244352	15.887744
24.711346	1174.130936	15.892762
24.646116	1170.164461	15.897779
25.032428	1169.852271	15.902797
24.675782	1175.197135	15.907815
24.909947	1169.245960	15.912832
25.033581	1176.079422	15.917850
24.660694	1171.975901	15.922867
24.898762	1169.976628	15.927885
25.017603	1170.706085	15.932903
25.148934	1168.741874	15.937920
25.016073	1168.578175	15.942938
25.167170	1174.542156	15.947955
25.168476	1166.840407	15.952973
24.749311	1172.063384	15.957991
24.760450	1172.379269	15.963008
24.761171	1177.020283	15.968026
24.851100	1170.630111	15.973043
24.792680	1180.216133	15.978061
24.978602	1189.114733	15.983079
25.220678	1191.228756	15.988096
25.343080	1196.746750	15.993114
25.658335	1199.383231	15.998131
25.693510	1191.927008	16.003149
25.931098	1188.110975	16.008167
25.874468	1173.658961	16.013184
25.949288	1164.061627	16.018202
25.336800	1169.692306	16.023219
25.619861	1159.678888	16.028237
25.309565	1156.861750	16.033255
25.383522	1152.072975	16.038272
25.674986	1147.468906	16.043290
25.603347	1155.123748	16.048307
26.338212	1150.918793	16.053325
25.622748	1158.840477	16.058343
25.828372	1154.757338	16.063360
25.896921	1157.526542	16.068378
25.734965	1152.111658	16.073395
25.878349	1156.077021	16.078413
25.716121	1155.847734	16.083431
25.734131	1157.210846	16.088448
25.736003	1164.247601	16.093466
25.439012	1163.231306	16.098483
25.830248	1157.053252	16.103501
25.495454	1150.611639	16.108519
25.277761	1151.032088	16.113536
25.469961	1160.603607	16.118554
25.667560	1177.272293	16.123571
26.143406	1175.303575	16.128589
25.559472	1193.687129	16.133607
25.888923	1187.229191	16.138624
25.560063	1193.439871	16.143642
25.548919	1185.185879	16.148659
25.954232	1188.553414	16.153677
25.667705	1189.823844	16.158695
26.135339	1206.344929	16.163712
26.675727	1203.346634	16.168730
26.700517	1190.618780	16.173747
26.560661	1179.727263	16.178765
26.270816	1180.294736	16.183783
26.629796	1176.521913	16.188800
26.492512	1174.464559	16.193818
26.100411	1173.687287	16.198835
26.435341	1166.885943	16.203853
26.185566	1177.082083	16.208871
26.012004	1168.882652	16.213888
26.131336	1179.052484	16.218906
25.948271	1178.885318	16.223923
26.374831	1186.662875	16.228941
26.433467	1204.452268	16.233959
26.606092	1199.761641	16.238976
26.668896	1200.731898	16.243994
26.615466	1200.847501	16.249011
26.856329	1198.437938	16.254029
26.858975	1199.208361	16.259047
26.821047	1193.660256	16.264064
26.847749	1174.533602	16.269082
26.216447	1179.064712	16.274099
26.750306	1185.322544	16.279117
26.719746	1198.211258	16.284135
26.946956	1200.254922	16.289152
26.826323	1202.887475	16.294170
26.380897	1201.741918	16.299187
26.601395	1197.085459	16.304205
26.612289	1204.138055	16.309223
26.819291	1202.742730	16.314240
26.977838	1207.288235	16.319258
26.498883	1203.152336	16.324275
27.018139	1197.482097	16.329293
27.249921	1206.284506	16.334311
26.681971	1200.444194	16.339328
27.082225	1196.838907	16.344346
26.781918	1207.846181	16.349363
26.967187	1223.783932	16.354381
27.290446	1233.714405	16.359399
27.026420	1230.488794	16.364416
27.613091	1229.938589	16.369434
27.236308	1242.551829	16.374451
27.450793	1227.591733	16.379469
26.986021	1236.977624	16.384487
27.214094	1232.621455	16.389504
27.615640	1233.743672	16.394522
27.498688	1235.892177	16.399539
27.617650	1230.073900	16.404557
27.408791	1227.926077	16.409575
26.857793	1227.592514	16.414592
27.343057	1232.684876	16.419610
27.196353	1235.033592	16.424627
27.650878	1233.866011	16.429645
27.699515	1228.610183	16.434663
27.327288	1235.274917	16.439680
27.686476	1233.100001	16.444698
27.504284	1230.333601	16.449715
27.655995	1230.278896	16.454733
27.534902	1228.833774	16.459751
27.637987	1237.203676	16.464768
27.632248	1226.808708	16.469786
27.627367	1235.163877	16.474803
28.051185	1240.101108	16.479821
27.963151	1233.444046	16.484839
27.943321	1229.439696	16.489856
28.021675	1229.766456	16.494874
27.845139	1236.571886	16.499891
27.875224	1228.552345	16.504909
27.748515	1227.022728	16.509927
27.755466	1245.779374	16.514944
28.304197	1246.379908	16.519962
28.034230	1249.609309	16.524979
28.360190	1241.126433	16.529997
28.383951	1254.465986	16.535015
28.163468	1237.781014	16.540032
28.166348	1229.285308	16.545050
28.224082	1219.478586	16.550067
28.411935	1218.453354	16.555085
28.541926	1218.206205	16.560103
28.405062	1216.466082	16.565120
28.400617	1214.612616	16.570138
28.290313	1218.781569	16.575155
28.577344	1218.993335	16.580173
28.434794	1220.137480	16.585191
28.094203	1228.201609	16.590208
28.776250	1223.195610	16.595226
28.381260	1220.422062	16.600243
28.412778	1219.461394	16.605261
28.564395	1224.641882	16.610279
28.186449	1219.597502	16.615296
28.505999	1213.825022	16.620314
28.390471	1228.455752	16.625331
28.600107	1240.260536	16.630349
28.607485	1239.591267	16.635367
28.603934	1249.115459	16.640384
28.804394	1250.315190	16.645402
28.319492	1257.092356	16.650419
28.938001	1243.321730	16.655437
28.776157	1243.143162	16.660455
28.700167	1250.385802	16.665472
28.573482	1244.362296	16.670490
28.653846	1245.464276	16.675507
28.512939	1237.117262	16.680525
28.465063	1252.370204	16.685543
28.408883	1255.378256	16.690560
28.978780	1267.837718	16.695578
29.078182	1276.697995	16.700595
29.223100	1277.069596	16.705613
29.358019	1274.131198	16.710631
29.063754	1273.111292	16.715648
29.546037	1261.405325	16.720666
29.369774	1272.888068	16.725683
29.440885	1263.501910	16.730701
29.311842	1238.450944	16.735719
29.107832	1242.003617	16.740736
29.392070	1243.266586	16.745754
29.400629	1264.360672	16.750771
29.519094	1263.435942	16.755789
29.461435	1253.724751	16.760807
29.400056	1246.149123	16.765824
29.782000	1241.649668	16.770842
29.335127	1236.637209	16.775859
29.585064	1234.489505	16.780877
29.502511	1226.209960	16.785895
29.247691	1231.949316	16.790912
29.581377	1254.414481	16.795930
29.578232	1261.413927	16.800947
29.914533	1260.503778	16.805965
29.488159	1262.625764	16.810983
29.385120	1265.653417	16.816000
29.740926	1259.059971	16.821018
29.720213	1259.894120	16.826035
29.484858	1262.557954	16.831053
29.420397	1262.833652	16.836071
29.355601	1271.575159	16.841088
29.660039	1255.282430	16.846106
29.886492	1264.208981	16.851123
29.897378	1278.594742	16.856141
30.307378	1279.968302	16.861159
29.956584	1271.019174	16.866176
30.189078	1257.107190	16.871194
30.256128	1262.149785	16.876211
30.118164	1255.707301	16.881229
30.227109	1255.201851	16.886247
29.758270	1255.141626	16.891264
30.275552	1250.885017	16.896282
29.994974	1252.997337	16.901299
30.057397	1274.917092	16.906317
30.442251	1277.788858	16.911335
30.542444	1282.905869	16.916352
30.669549	1268.253945	16.921370
30.206131	1264.115446	16.926387
30.337556	1248.329017	16.931405
30.747918	1245.654672	16.936423
30.467725	1247.182309	16.941440
30.733834	1245.361429	16.946458
30.610054	1247.347299	16.951475
30.656755	1242.799235	16.956493
30.747766	1252.279368	16.961511
30.367839	1248.955305	16.966528
30.642776	1252.219333	16.971546
30.309177	1250.000117	16.976563
30.520836	1253.014438	16.981581
30.616428	1247.595689	16.986599
30.473734	1268.054714	16.991616
30.882598	1268.604484	16.996634
30.971990	1282.129995	17.001651
30.965860	1279.328419	17.006669
31.032633	1273.969173	17.011687
30.768974	1273.680761	17.016704
31.134639	1267.752179	17.021722
30.972083	1259.418986	17.026739
30.830639	1246.789970	17.031757
30.977654	1264.993858	17.036775
30.905419	1284.687686	17.041792
31.130987	1278.087140	17.046810
31.103906	1286.341308	17.051827
30.473543	1291.015593	17.056845
30.674457	1275.617569	17.061863
30.520112	1282.216583	17.066880
30.683198	1283.073332	17.071898
31.217476	1303.359656	17.076915
30.908678	1307.486035	17.081933
30.997885	1304.741047	17.086951
31.360015	1305.441099	17.091968
31.415096	1313.659579	17.096986
31.493896	1306.629496	17.102003
31.508135	1310.842732	17.107021
31.709058	1309.118895	17.112039
31.319378	1309.747452	17.117056
31.667618	1309.532135	17.122074
31.653881	1302.659948	17.127091
31.815140	1316.471170	17.132109
32.127413	1301.364047	17.137127
31.727621	1310.627769	17.142144
32.009673	1294.838697	17.147162
31.639476	1298.413099	17.152179
31.131876	1297.553839	17.157197
31.710710	1299.033586	17.162215
31.539164	1299.545577	17.167232
31.936683	1292.144433	17.172250
31.969061	1301.659930	17.177267
31.663664	1308.906081	17.182285
31.933996	1299.416714	17.187303
31.601708	1299.981403	17.192320
31.742059	1300.273059	17.197338
31.757121	1301.966580	17.202355
32.029454	1326.366372	17.207373
32.413577	1322.395250	17.212391
31.877556	1325.125601	17.217408
32.345073	1331.983865	17.222426
32.453098	1321.734091	17.227443
32.381617	1334.236823	17.232461
32.343052	1319.785606	17.237479
32.035896	1323.966045	17.242496
32.023534	1318.830163	17.247514
32.490297	1315.692516	17.252531
32.277081	1325.229161	17.257549
32.673349	1319.408461	17.262567
32.722527	1322.248234	17.267584
32.677816	1312.014403	17.272602
32.644707	1317.942130	17.277619
32.238344	1309.787221	17.282637
32.628984	1313.766646	17.287655
32.501400	1315.465373	17.292672
32.657906	1325.021276	17.297690
32.697146	1317.136382	17.302707
32.549001	1323.571398	17.307725
32.689072	1317.922407	17.312743
32.524975	1317.970581	17.317760
32.688393	1317.370646	17.322778
32.868676	1322.413338	17.327795
32.862079	1319.683090	17.332813
33.124560	1313.814945	17.337831
32.992473	1314.696739	17.342848
32.933530	1316.478937	17.347866
33.138666	1310.602215	17.352883
32.809773	1325.434632	17.357901
32.756217	1313.961378	17.362919
32.941657	1317.237538	17.367936
32.859721	1317.570470	17.372954
32.574761	1308.173782	17.377971
32.802474	1333.340417	17.382989
33.241837	1330.976580	17.388007
32.949414	1336.706872	17.393024
33.017082	1350.045509	17.398042
33.067084	1353.228444	17.403059
32.870826	1357.441246	17.408077
33.381622	1349.975974	17.413095
33.218181	1351.257454	17.418112
33.460214	1350.588942	17.423130
33.847457	1352.398951	17.428147
33.523011	1349.988442	17.433165
33.075124	1337.585080	17.438183
33.599933	1358.224610	17.443200
33.772910	1370.518245	17.448218
34.008103	1365.254987	17.453235
33.851363	1357.973488	17.458253
33.900663	1342.804919	17.463271
33.685363	1345.629206	17.468288
33.730710	1341.860441	17.473306
33.860945	1334.246624	17.478323
33.632590	1347.303370	17.483341
34.084871	1359.430896	17.488359
34.435305	1365.766530	17.493376
33.968663	1349.308561	17.498394
34.114477	1339.417048	17.503411
33.941865	1341.223258	17.508429
34.030396	1328.044557	17.513447
33.986073	1345.233141	17.518464
34.126356	1350.724204	17.523482
34.553283	1350.658008	17.528499
34.135683	1349.336167	17.533517
34.172171	1341.165904	17.538535
34.035312	1344.502723	17.543552
34.157539	1357.616560	17.548570
34.506543	1358.163291	17.553587
34.421234	1362.650556	17.558605
34.446863	1362.020766	17.563623
34.313267	1360.094658	17.568640
34.456547	1363.911279	17.573658
34.593437	1350.670193	17.578675
34.281892	1364.998210	17.583693
34.352463	1356.751411	17.588711
34.581475	1358.625906	17.593728
34.638554	1370.184896	17.598746
34.746131	1360.617035	17.603763
34.624743	1374.570557	17.608781
34.616432	1361.386270	17.613799
34.364414	1360.321149	17.618816
34.308017	1356.015769	17.623834
34.597400	1354.590598	17.628851
34.517797	1359.344226	17.633869
34.465630	1367.091208	17.638887
34.775966	1380.073411	17.643904
34.731490	1387.944712	17.648922
35.179129	1389.282894	17.653939
34.867838	1400.040170	17.658957
35.200646	1381.839121	17.663975
35.382369	1385.658413	17.668992
35.259665	1386.326455	17.674010
35.226610	1381.349892	17.679027
35.032498	1388.355151	17.684045
35.295232	1388.475293	17.689063
35.112928	1385.548654	17.694080
35.427018	1385.839781	17.699098
35.475126	1376.296754	17.704115
35.442713	1393.901112	17.709133
35.327595	1384.986760	17.714151
35.554543	1387.126159	17.719168
35.303302	1394.749555	17.724186
35.876678	1387.331343	17.729203
35.689475	1388.324266	17.734221
35.744865	1379.526455	17.739239
35.223805	1379.942606	17.744256
34.964606	1380.525857	17.749274
35.646031	1377.141899	17.754291
35.291160	1385.493904	17.759309
35.520847	1393.350348	17.764327
35.717455	1399.445825	17.769344
35.724247	1410.167958	17.774362
36.220655	1401.598401	17.779379
36.082920	1408.170693	17.784397
35.809541	1408.272462	17.789415
36.055178	1411.381557	17.794432
35.666562	1406.881781	17.799450
35.929840	1402.677189	17.804467
35.808577	1403.072168	17.809485
35.851102	1396.577582	17.814503
36.087685	1396.214687	17.819520
36.072421	1401.841853	17.824538
36.217843	1390.954346	17.829555
36.142609	1396.091890	17.834573
36.256652	1395.506457	17.839591
36.382063	1410.165422	17.844608
36.155925	1422.086471	17.849626
36.843497	1425.311876	17.854643
36.815215	1421.696662	17.859661
36.677871	1408.894004	17.864679
36.663630	1401.829737	17.869696
36.780538	1399.769867	17.874714
36.838313	1386.722208	17.879731
36.603047	1398.784121	17.884749
36.480243	1396.739289	17.889767
36.465215	1399.779898	17.894784
36.466058	1407.738555	17.899802
36.720381	1402.143770	17.904819
36.789213	1425.818122	17.909837
37.051665	1422.548668	17.914855
37.008411	1415.836055	17.919872
36.606012	1411.525963	17.924890
37.034497	1413.245664	17.929907
36.921058	1420.883176	17.934925
36.902015	1422.367426	17.939943
37.074496	1424.278096	17.944960
37.004882	1426.945512	17.949978
37.164142	1412.918793	17.954995
36.728965	1426.124149	17.960013
36.999637	1420.585694	17.965031
37.246439	1422.568260	17.970048
37.072251	1430.895377	17.975066
37.416815	1423.855322	17.980083
37.223777	1428.910885	17.985101
37.417374	1427.157545	17.990119
37.566656	1421.882957	17.995136
37.418761	1426.339305	18.000154
37.318757	1421.896671	18.005171
37.235528	1434.371122	18.010189
37.229760	1421.471785	18.015207
37.657931	1436.084786	18.020224
37.247087	1447.113750	18.025242
37.616720	1446.015380	18.030259
37.807679	1454.943610	18.035277
37.787734	1453.656059	18.040295
37.777130	1457.314034	18.045312
37.241402	1451.935968	18.050330
37.296623	1452.942540	18.055347
37.512056	1449.615937	18.060365
37.492286	1456.339898	18.065383
38.422956	1467.164813	18.070400
37.858936	1485.868619	18.075418
38.526194	1461.314453	18.080435
39.080564	1452.153365	18.085453
38.985146	1438.850029	18.090471
38.872537	1426.447562	18.095488
39.079158	1423.106682	18.100506
38.650364	1393.527886	18.105523
38.512594	1387.099488	18.110541
38.530975	1394.268245	18.115559
38.845471	1375.493890	18.120576
38.651758	1386.026505	18.125594
38.664515	1381.345465	18.130611
38.754650	1380.064821	18.135629
38.303354	1382.034671	18.140647
38.641827	1381.361153	18.145664
38.562526	1389.475242	18.150682
38.724672	1381.263207	18.155699
38.731514	1386.817405	18.160717
38.559973	1397.497519	18.165735
38.984407	1377.671857	18.170752
39.071121	1379.982194	18.175770
38.800882	1383.278594	18.180787
38.644038	1380.602044	18.185805
38.637253	1384.523136	18.190823
38.877219	1378.404782	18.195840
38.543948	1379.800707	18.200858
38.647082	1385.244416	18.205875
38.546894	1393.492682	18.210893
38.586286	1412.117372	18.215911
38.922002	1412.119483	18.220928
39.034635	1420.996148	18.225946
38.890975	1422.854246	18.230963
38.937749	1418.517923	18.235981
39.003755	1423.874906	18.240999
38.808292	1430.056423	18.246016
39.268355	1453.649653	18.251034
39.093791	1455.858943	18.256051
39.403743	1459.249869	18.261069
39.627703	1457.012362	18.266087
39.608958	1452.633377	18.271104
39.416011	1460.095546	18.276122
39.280402	1457.393408	18.281139
39.233180	1458.282758	18.286157
39.095885	1458.137114	18.291175
39.546216	1451.914086	18.296192
39.566040	1462.308904	18.301210
39.443771	1476.955555	18.306227
39.677487	1465.984819	18.311245
39.727684	1475.560845	18.316263
40.446134	1456.850353	18.321280
40.113822	1472.068505	18.326298
40.498308	1458.662164	18.331315
40.749648	1453.776889	18.336333
40.457164	1445.254960	18.341351
40.272091	1431.234272	18.346368
40.256048	1432.629445	18.351386
40.550955	1424.440203	18.356403
40.708888	1426.434391	18.361421
40.358561	1432.023558	18.366439
40.397584	1424.469737	18.371456
40.159569	1429.231211	18.376474
40.307073	1433.657362	18.381491
40.393289	1428.130270	18.386509
40.413125	1429.275000	18.391527
40.571458	1431.300617	18.396544
40.607321	1434.581979	18.401562
40.603049	1428.965205	18.406579
40.350933	1432.809371	18.411597
40.273509	1436.805206	18.416615
40.612917	1424.534694	18.421632
40.248990	1424.309398	18.426650
40.356273	1444.795218	18.431667
40.619292	1455.954704	18.436685
40.784068	1453.309725	18.441703
40.483989	1463.298672	18.446720
40.444834	1465.015395	18.451738
40.840012	1459.283011	18.456755
40.662807	1467.719307	18.461773
41.011743	1479.210975	18.466791
41.196902	1479.744786	18.471808
41.198782	1494.090514	18.476826
41.297832	1488.853384	18.481843
41.332560	1485.896560	18.486861
41.025701	1491.513562	18.491879
41.441467	1487.694615	18.496896
41.311511	1480.882607	18.501914
41.297685	1483.373838	18.506931
41.527526	1473.503312	18.511949
41.171738	1481.316167	18.516967
41.497964	1475.651928	18.521984
41.340733	1483.426272	18.527002
41.023222	1483.219638	18.532019
41.123168	1484.582152	18.537037
41.219642	1509.349247	18.542055
41.594785	1505.964593	18.547072
42.124822	1518.088771	18.552090
41.954672	1513.287701	18.557107
42.123735	1509.879818	18.562125
42.007846	1524.406953	18.567143
41.896697	1510.743582	18.572160
41.856826	1517.681927	18.577178
41.955181	1511.907126	18.582195
42.099332	1500.088679	18.587213
42.033774	1509.978051	18.592231
41.947835	1508.093608	18.597248
41.970949	1506.183560	18.602266
41.909574	1504.323774	18.607283
41.872986	1505.014515	18.612301
41.885864	1518.612791	18.617319
42.205697	1522.319009	18.622336
42.301071	1536.976787	18.627354
42.067742	1540.682428	18.632371
42.285459	1532.313050	18.637389
42.177981	1543.963298	18.642407
42.551397	1532.375613	18.647424
42.497388	1533.360187	18.652442
42.506453	1545.415070	18.657459
42.624144	1538.355585	18.662477
42.138296	1544.276755	18.667495
42.586789	1537.031980	18.672512
42.734132	1545.525006	18.677530
42.787559	1557.846533	18.682547
43.355190	1560.445857	18.687565
43.174959	1560.412463	18.692583
43.005316	1550.066565	18.697600
43.109256	1537.420543	18.702618
43.158414	1539.978085	18.707635
43.169112	1521.228455	18.712653
43.295142	1531.774561	18.717671
43.241639	1532.629134	18.722688
43.533423	1528.224895	18.727706
42.935812	1529.360443	18.732723
42.984157	1521.053472	18.737741
43.175722	1547.535089	18.742759
43.332596	1547.954709	18.747776
43.141332	1549.358542	18.752794
43.259399	1554.143154	18.757811
43.273601	1547.910291	18.762829
43.153631	1554.295840	18.767847
43.344508	1550.306386	18.772864
43.598254	1567.565359	18.777882
43.520956	1569.776215	18.782899
43.602173	1582.012043	18.787917
43.641631	1590.670264	18.792935
44.106809	1583.934492	18.797952
44.037665	1590.025001	18.802970
43.746443	1588.813233	18.807987
44.212460	1573.484630	18.813005
44.231115	1575.783080	18.818023
44.086873	1569.604494	18.823040
44.395189	1573.259490	18.828058
44.167507	1575.407942	18.833075
44.336163	1571.664689	18.838093
44.329665	1566.554127	18.843111
44.401901	1566.931911	18.848128
44.704375	1566.069098	18.853146
44.395650	1578.642953	18.858163
44.792145	1561.379903	18.863181
44.620257	1560.479791	18.868199
44.316456	1543.310709	18.873216
44.410734	1556.765179	18.878234
44.278084	1567.400364	18.883251
44.621764	1564.267771	18.888269
44.621116	1578.305737	18.893287
44.561448	1569.402534	18.898304
44.606558	1576.500794	18.903322
44.691871	1579.347207	18.908339
44.783637	1572.098713	18.913357
44.680797	1564.305809	18.918375
44.847209	1568.419417	18.923392
44.897829	1571.626703	18.928410
44.684253	1574.046818	18.933427
45.008760	1576.091686	18.938445
44.931158	1587.356696	18.943463
45.081292	1592.896601	18.948480
45.295592	1588.437902	18.953498
45.177332	1596.049924	18.958515
45.714905	1599.001881	18.963533
45.753226	1597.923920	18.968551
45.370711	1576.505389	18.973568
45.100322	1569.827309	18.978586
44.947053	1581.144259	18.983603
45.476518	1588.739963	18.988621
45.293858	1594.292266	18.993639
45.320079	1594.996194	18.998656
45.526023	1594.921059	19.003674
45.132240	1594.714500	19.008691
45.587829	1583.732789	19.013709
45.347518	1595.144528	19.018727
45.390832	1617.699033	19.023744
45.806134	1611.733333	19.028762
45.926075	1619.730965	19.033779
46.223491	1613.803360	19.038797
45.840209	1626.013668	19.043815
45.987598	1620.118082	19.048832
45.801708	1624.515841	19.053850
45.910047	1621.125113	19.058867
45.894082	1616.352321	19.063885
45.872331	1627.031319	19.068903
46.061659	1637.170923	19.073920
46.648695	1646.038162	19.078938
46.730331	1642.042825	19.083955
47.340552	1613.873962	19.088973
47.051463	1607.511958	19.093991
47.416911	1596.870802	19.099008
47.420293	1590.798378	19.104026
46.966957	1584.045581	19.109043
47.100059	1565.099575	19.114061
46.900127	1565.623377	19.119079
46.944901	1559.862974	19.124096
47.048268	1564.961048	19.129114
47.070330	1571.011589	19.134131
46.932074	1555.122821	19.139149
47.043431	1553.844934	19.144167
46.656466	1560.810278	19.149184
47.024845	1557.187374	19.154202
47.066990	1562.412548	19.159219
47.070458	1551.752059	19.164237
47.169630	1556.521703	19.169255
46.968365	1557.155172	19.174272
47.206164	1562.297437	19.179290
47.000541	1559.665576	19.184307
47.314813	1572.448474	19.189325
47.308447	1588.148775	19.194343
47.311403	1585.267682	19.199360
47.580539	1590.041372	19.204378
47.585603	1594.788874	19.209395
47.446628	1599.724485	19.214413
47.745007	1590.431850	19.219431
47.256033	1587.378978	19.224448
47.435009	1591.879077	19.229466
47.332941	1593.736582	19.234483
47.313718	1590.398556	19.239501
47.679151	1598.882530	19.244519
47.302484	1617.936843	19.249536
47.266731	1617.042448	19.254554
47.656251	1621.499296	19.259571
47.503999	1627.769770	19.264589
47.853932	1641.275916	19.269607
48.136415	1651.294144	19.274624
48.490149	1649.811011	19.279642
48.218195	1648.360606	19.284659
48.307675	1640.757350	19.289677
48.486301	1650.564497	19.294695
48.263003	1642.879367	19.299712
48.379335	1649.979602	19.304730
48.344273	1655.997545	19.309747
48.641186	1639.060402	19.314765
48.551505	1647.296820	19.319783
48.590636	1645.312047	19.324800
48.591728	1655.441217	19.329818
48.414953	1649.525874	19.334835
48.661742	1651.236038	19.339853
48.319639	1642.428551	19.344871
48.476100	1652.713389	19.349888
49.026171	1666.985885	19.354906
48.489852	1671.041906	19.359923
48.893619	1675.563330	19.364941
49.191927	1678.478691	19.369959
48.986889	1676.230564	19.374976
49.399311	1665.729190	19.379994
49.492393	1674.634446	19.385011
49.204211	1671.030479	19.390029
49.096459	1666.218991	19.395047
48.966955	1673.991972	19.400064
49.316595	1669.802089	19.405082
49.402727	1669.501201	19.410099
49.599620	1663.091869	19.415117
49.388295	1671.642999	19.420135
49.211199	1665.893841	19.425152
49.654282	1682.153779	19.430170
49.401306	1700.649851	19.435187
49.716597	1683.564726	19.440205
49.792013	1685.175819	19.445223
49.822893	1686.462431	19.450240
50.340249	1672.001167	19.455258
50.154541	1686.938082	19.460275
50.368589	1685.099034	19.465293
50.686282	1670.744575	19.470311
50.412509	1672.044023	19.475328
50.457571	1645.793797	19.480346
50.385461	1648.415211	19.485363
50.310812	1640.878601	19.490381
50.336140	1635.933590	19.495399
50.283411	1643.889067	19.500416
50.551131	1639.673045	19.505434
50.501379	1639.615996	19.510451
50.471616	1640.787882	19.515469
50.783268	1633.676039	19.520487
50.490041	1641.213622	19.525504
50.189149	1643.175828	19.530522
50.609459	1671.342439	19.535539
50.623961	1672.295558	19.540557
50.730990	1677.260780	19.545575
50.434134	1684.567101	19.550592
50.621522	1677.599116	19.555610
51.015141	1679.358896	19.560627
50.805328	1678.293429	19.565645
50.754362	1678.803106	19.570663
50.691291	1690.966940	19.575680
51.381146	1686.685471	19.580698
51.429304	1690.762074	19.585715
51.134171	1694.500856	19.590733
51.377157	1684.470141	19.595751
51.523112	1686.164785	19.600768
51.466361	1690.981250	19.605786
51.635531	1693.474777	19.610803
51.465212	1691.779135	19.615821
51.692547	1690.183149	19.620839
51.596672	1686.155099	19.625856
51.585381	1693.081293	19.630874
51.387812	1689.380768	19.635891
51.593917	1692.574837	19.640909
51.827994	1681.718453	19.645927
51.418749	1696.322457	19.650944
52.228219	1687.168047	19.655962
51.874901	1688.338593	19.660979
51.673830	1688.986995	19.665997
51.949475	1690.595914	19.671015
51.612868	1692.868387	19.676032
51.898656	1704.256548	19.681050
51.762276	1723.400188	19.686067
52.092407	1720.127299	19.691085
51.936478	1720.503244	19.696103
51.813318	1726.300820	19.701120
52.049259	1721.215267	19.706138
52.153627	1735.624893	19.711155
52.265704	1755.544590	19.716173
52.775667	1746.566693	19.721191
52.613683	1753.886851	19.726208
52.928947	1735.578462	19.731226
52.814993	1736.659231	19.736243
53.075719	1735.725791	19.741261
53.346938	1732.582768	19.746279
53.389077	1737.819813	19.751296
53.418602	1723.970672	19.756314
53.392617	1709.228815	19.761331
53.194603	1700.151682	19.766349
53.188374	1700.044093	19.771367
53.057320	1703.476479	19.776384
53.053819	1692.552095	19.781402
52.964447	1688.537923	19.786419
53.171873	1711.061747	19.791437
53.358489	1720.868005	19.796455
53.652541	1718.146773	19.801472
53.249636	1727.912825	19.806490
54.066998	1717.637419	19.811507
53.784824	1728.793620	19.816525
53.758137	1720.210040	19.821543
53.498953	1728.684905	19.826560
53.795565	1728.134471	19.831578
53.814340	1724.522783	19.836595
53.719614	1732.441586	19.841613
54.304296	1724.860710	19.846631
54.087353	1728.224700	19.851648
54.160590	1729.958206	19.856666
54.076235	1718.341740	19.861683
53.709429	1729.119493	19.866701
53.932136	1727.854976	19.871719
53.869839	1723.564646	19.876736
53.653024	1725.464071	19.881754
53.913443	1736.774979	19.886771
53.624685	1756.952236	19.891789
54.006550	1750.428663	19.896807
53.892926	1760.557676	19.901824
54.447457	1758.232117	19.906842
54.611268	1784.447103	19.911859
54.611579	1778.569601	19.916877
54.476447	1770.352438	19.921895
54.647268	1777.351158	19.926912
54.768769	1779.175071	19.931930
54.862199	1778.962731	19.936947
54.501066	1776.048020	19.941965
54.908323	1776.577608	19.946983
54.659259	1780.857566	19.952000
54.866030	1794.508898	19.957018
55.186660	1793.544240	19.962035
55.175819	1797.878704	19.967053
55.515254	1801.847872	19.972071
55.530981	1805.083447	19.977088
55.267611	1800.796987	19.982106
55.581664	1796.427948	19.987123
55.358724	1796.461492	19.992141
55.429652	1794.689524	19.997159
55.421471	1801.996741	20.002176
55.745677	1806.438121	20.007194
55.820965	1796.150956	20.012211
55.687713	1796.862106	20.017229
55.778210	1795.681760	20.022247
55.681584	1794.062441	20.027264
55.964906	1795.826786	20.032282
56.052672	1788.917434	20.037299
55.920229	1802.727511	20.042317
56.127645	1789.936529	20.047335
55.915691	1790.513516	20.052352
56.256773	1777.664109	20.057370
56.143059	1781.560160	20.062387
55.926026	1795.881133	20.067405
56.196460	1795.209066	20.072423
56.447290	1820.419111	20.077440
56.567727	1820.992038	20.082458
56.513501	1821.343602	20.087475
56.123366	1822.573425	20.092493
56.122120	1823.830349	20.097511
56.370661	1819.401326	20.102528
56.005538	1819.662829	20.107546
56.645253	1832.490281	20.112563
56.881449	1843.902142	20.117581
57.330217	1843.302795	20.122599
57.001592	1853.203036	20.127616
57.145721	1858.945609	20.132634
57.562102	1837.702601	20.137651
57.130723	1847.937629	20.142669
57.461990	1842.959422	20.147687
57.291562	1844.920837	20.152704
57.477696	1847.506451	20.157722
57.309122	1842.839267	20.162739
57.232861	1845.698409	20.167757
57.470961	1851.041901	20.172775
57.604581	1838.963925	20.177792
57.400291	1840.022706	20.182810
57.726767	1833.391376	20.187827
57.700759	1842.878328	20.192845
57.694297	1834.211797	20.197863
57.668150	1844.227114	20.202880
57.844727	1828.821563	20.207898
58.271903	1833.563551	20.212915
58.085731	1844.417661	20.217933
58.170404	1838.693437	20.222951
58.114249	1843.241349	20.227968
58.058823	1837.769935	20.232986
58.276574	1835.427896	20.238003
58.076282	1848.574493	20.243021
58.117835	1850.563276	20.248039
58.350655	1866.775284	20.253056
58.229789	1869.726882	20.258074
58.247995	1863.794800	20.263091
57.957788	1869.284760	20.268109
58.290922	1861.162165	20.273127
58.206849	1885.724437	20.278144
58.377275	1891.736273	20.283162
58.917447	1891.452048	20.288179
59.002318	1897.845032	20.293197
59.316205	1890.236247	20.298215
59.166415	1890.213933	20.303232
58.737747	1895.698568	20.308250
58.988161	1887.801123	20.313267
58.903470	1887.513661	20.318285
59.207042	1888.211271	20.323303
59.016412	1892.766192	20.328320
58.962031	1886.347742	20.333338
59.521952	1886.385823	20.338355
59.314891	1907.877250	20.343373
59.368659	1909.186848	20.348391
59.401172	1904.179927	20.353408
59.456873	1907.335652	20.358426
59.640419	1905.250862	20.363443
59.720289	1909.671069	20.368461
59.928088	1905.219659	20.373479
60.117013	1907.718600	20.378496
59.987049	1900.576882	20.383514
60.044715	1901.393314	20.388531
60.096379	1907.800876	20.393549
60.020586	1908.674922	20.398567
60.124678	1904.409645	20.403584
59.937729	1901.793125	20.408602
60.229865	1894.034805	20.413619
60.016111	1902.426229	20.418637
60.322586	1911.461905	20.423655
60.336015	1925.820680	20.428672
59.972449	1934.214578	20.433690
60.223246	1925.739099	20.438707
60.417408	1931.765116	20.443725
60.873594	1937.131841	20.448743
60.474948	1930.867438	20.453760
60.298450	1936.610177	20.458778
60.660981	1939.664915	20.463795
60.647824	1965.336391	20.468813
60.759894	1953.759151	20.473831
60.970591	1956.697789	20.478848
60.914927	1954.451172	20.483866
61.316779	1949.823012	20.488883
61.089771	1953.461163	20.493901
61.269874	1977.606843	20.498919
61.627186	1978.065999	20.503936
61.398727	1984.539439	20.508954
61.952755	1978.557238	20.513971
62.012374	1976.414294	20.518989
61.735442	1955.095012	20.524007
61.949944	1952.270426	20.529024
61.586048	1949.700235	20.534042
61.792658	1949.919476	20.539059
61.580733	1968.270068	20.544077
61.985489	1974.205983	20.549095
62.367004	1971.741826	20.554112
62.202976	1973.550224	20.559130
62.944096	1967.753864	20.564147
62.479441	1969.810255	20.569165
62.252621	1947.373994	20.574183
62.406030	1943.520195	20.579200
62.111565	1944.944363	20.584218
62.387862	1946.546114	20.589235
62.263423	1957.771933	20.594253
62.296952	1965.871901	20.599271
62.404220	1976.215918	20.604288
62.268633	1978.864078	20.609306
62.708868	1966.703155	20.614323
62.442902	1969.834006	20.619341
62.482697	1965.892390	20.624359
62.701979	1981.296926	20.629376
62.649809	1996.040291	20.634394
62.776127	1997.258705	20.639411
62.834562	2013.784494	20.644429
62.748348	2002.111825	20.649447
63.314776	1998.679530	20.654464
63.046921	1999.894949	20.659482
63.438264	2005.147672	20.664499
63.596240	2020.480545	20.669517
64.028085	2015.306829	20.674535
63.909524	1997.887162	20.679552
63.707405	1997.873545	20.684570
63.696799	1989.116277	20.689587
63.891700	1988.616204	20.694605
64.031039	1986.345443	20.699623
63.995408	1980.486436	20.704640
63.772290	1991.914112	20.709658
63.835286	1979.244614	20.714675
63.632275	1987.586267	20.719693
63.942984	1997.540976	20.724711
64.406918	2013.467090	20.729728
64.286327	2021.726954	20.734746
64.880936	2021.127380	20.739763
64.455864	2021.461053	20.744781
64.328299	2021.820479	20.749799
64.308720	2014.244219	20.754816
64.571982	2005.356388	20.759834
65.159085	2003.080107	20.764851
64.885181	2012.500880	20.769869
65.072068	2000.587155	20.774887
65.333034	1994.225307	20.779904
65.106728	1979.918453	20.784922
65.415579	1965.630547	20.789939
65.066771	1962.154302	20.794957
64.731982	1962.906827	20.799975
65.170979	1964.727210	20.804992
64.727054	1982.481337	20.810010
65.136780	1986.311706	20.815027
65.346441	1995.922971	20.820045
65.267451	1998.453067	20.825063
65.238626	1994.698439	20.830080
65.341357	1996.320380	20.835098
65.153433	1991.989043	20.840115
65.518856	1990.359842	20.845133
65.505527	1999.418404	20.850151
66.212462	2002.141115	20.855168
65.751747	2010.629940	20.860186
65.878270	1996.578607	20.865203
66.039935	2002.187217	20.870221
65.958025	2007.231977	20.875239
66.165292	2013.150336	20.880256
66.121278	2015.216747	20.885274
66.317297	2002.202287	20.890291
66.132462	2006.241316	20.895309
66.054733	1999.538509	20.900327
66.082024	2009.450564	20.905344
65.822190	2030.978885	20.910362
66.586272	2027.982634	20.915379
66.684746	2038.922645	20.920397
66.737180	2038.754517	20.925415
66.604534	2029.619081	20.930432
66.352001	2036.264654	20.935450
66.562376	2053.393190	20.940467
66.901124	2048.569189	20.945485
67.009395	2065.995418	20.950503
67.120707	2058.438329	20.955520
66.825162	2062.122935	20.960538
67.126224	2067.282021	20.965555
67.245689	2059.150739	20.970573
67.040433	2062.929789	20.975591
67.316398	2069.184786	20.980608
67.638640	2088.417224	20.985626
67.469588	2086.050455	20.990643
67.572216	2091.014574	20.995661
67.550957	2090.758298	21.000679
67.576646	2079.857530	21.005696
67.540358	2090.910919	21.010714
67.768264	2077.021800	21.015731
67.618744	2090.586543	21.020749
67.465483	2090.399843	21.025767
67.764661	2100.325826	21.030784
67.995829	2111.739508	21.035802
67.962302	2116.380197	21.040819
68.275840	2115.692292	21.045837
67.991207	2122.898360	21.050855
68.247406	2109.757666	21.055872
68.508223	2118.273488	21.060890
68.521290	2120.448931	21.065907
68.901299	2128.567387	21.070925
68.807239	2144.695821	21.075943
68.970004	2133.361994	21.080960
69.235629	2145.738095	21.085978
69.113166	2129.448076	21.090995
69.044394	2120.314570	21.096013
68.852523	2133.418275	21.101031
68.961924	2127.802828	21.106048
69.131484	2136.099966	21.111066
69.270553	2135.517041	21.116083
69.266052	2141.386784	21.121101
69.260719	2141.832592	21.126119
69.381383	2127.748650	21.131136
69.592925	2136.428972	21.136154
69.392361	2135.959184	21.141171
69.540960	2138.765656	21.146189
69.686634	2144.412803	21.151207
69.964092	2158.601929	21.156224
69.910917	2162.766757	21.161242
70.285769	2161.512748	21.166259
70.676585	2144.985046	21.171277
70.748107	2132.452983	21.176295
71.215065	2118.041023	21.181312
71.108645	2105.776353	21.186330
70.839965	2100.582808	21.191347
71.064901	2098.521822	21.196365
70.594231	2098.514252	21.201383
70.472356	2075.919810	21.206400
70.635841	2074.958024	21.211418
70.865361	2083.780999	21.216435
70.858106	2102.101672	21.221453
70.938495	2097.783588	21.226471
71.151230	2096.063217	21.231488
71.007288	2104.355745	21.236506
70.923800	2106.058253	21.241523
71.511533	2094.900679	21.246541
71.428269	2103.902814	21.251559
71.531740	2100.270663	21.256576
71.167336	2108.625030	21.261594
70.775758	2101.164095	21.266611
71.074439	2099.436920	21.271629
71.002134	2109.662837	21.276647
71.092323	2098.774958	21.281664
71.057195	2109.342731	21.286682
71.035840	2128.970121	21.291699
71.510967	2132.107368	21.296717
71.077170	2139.266579	21.301735
71.660704	2154.530437	21.306752
71.902449	2162.342751	21.311770
71.735819	2161.075582	21.316787
72.090053	2164.322299	21.321805
71.813688	2158.354018	21.326823
72.042099	2179.047456	21.331840
72.192690	2189.028899	21.336858
72.117951	2194.346941	21.341875
72.379365	2189.870005	21.346893
72.227649	2198.159545	21.351911
72.658140	2189.975717	21.356928
72.631749	2193.992399	21.361946
72.338253	2195.830213	21.366963
72.641462	2204.756760	21.371981
72.655048	2214.423188	21.376999
73.193348	2221.183871	21.382016
73.012287	2228.407420	21.387034
72.860603	2227.097603	21.392051
73.219190	2218.977679	21.397069
72.909731	2228.445830	21.402087
73.377342	2222.602706	21.407104
73.129020	2226.991324	21.412122
73.277557	2240.086578	21.417139
73.646058	2242.734868	21.422157
73.501615	2250.829129	21.427175
73.123462	2245.941135	21.432192
73.720008	2248.186953	21.437210
73.452218	2248.960640	21.442227
73.602461	2267.112022	21.447245
73.668882	2283.641103	21.452263
74.387472	2276.719613	21.457280
74.182085	2280.045973	21.462298
74.278568	2285.413151	21.467315
74.560747	2267.308460	21.472333
74.305232	2277.180676	21.477351
74.452240	2276.673200	21.482368
74.371185	2270.865728	21.487386
74.358137	2270.263983	21.492403
74.761343	2281.781487	21.497421
74.695473	2300.403084	21.502439
75.367608	2285.871043	21.507456
75.727149	2277.904477	21.512474
75.449597	2259.079415	21.517491
76.032230	2240.391348	21.522509
75.608854	2242.250358	21.527527
76.010887	2235.171649	21.532544
75.933404	2231.909310	21.537562
75.824160	2227.740031	21.542579
75.917884	2213.727417	21.547597
75.641973	2206.106655	21.552615
75.653285	2212.532467	21.557632
75.631977	2201.841788	21.562650
75.685716	2213.391335	21.567667
75.853364	2220.775830	21.572685
75.500119	2229.718179	21.577703
75.672335	2229.862038	21.582720
75.652476	2233.850085	21.587738
75.465857	2237.073709	21.592755
76.051981	2241.113415	21.597773
75.654937	2268.980725	21.602791
75.961909	2263.936344	21.607808
76.127023	2262.743169	21.612826
76.159611	2283.734650	21.617843
76.748129	2290.837419	21.622861
76.510042	2296.903524	21.627879
76.593888	2296.266384	21.632896
77.015781	2299.854255	21.637914
76.771664	2301.046459	21.642931
76.943923	2289.666451	21.647949
76.512161	2293.720606	21.652967
76.873990	2298.210604	21.657984
76.934421	2317.452191	21.663002
76.962321	2324.852479	21.668019
77.535286	2317.635875	21.673037
77.317696	2330.214086	21.678055
77.536270	2323.479220	21.683072
77.661480	2318.753617	21.688090
77.582005	2326.468608	21.693107
77.789929	2308.489204	21.698125
77.951402	2321.094178	21.703143
77.993738	2311.715318	21.708160
78.128834	2319.073772	21.713178
77.821001	2323.199467	21.718195
77.887470	2320.238390	21.723213
78.106017	2323.734468	21.728231
78.148328	2337.954570	21.733248
78.217037	2340.833806	21.738266
78.183425	2343.052866	21.743283
78.450347	2338.204491	21.748301
78.501889	2341.941325	21.753319
78.502581	2348.858340	21.758336
78.735954	2339.442990	21.763354
78.606465	2354.483016	21.768371
78.882291	2344.103498	21.773389
78.991970	2347.946816	21.778407
78.786751	2359.925737	21.783424
78.952534	2357.723758	21.788442
78.861178	2362.106013	21.793459
79.384750	2350.141185	21.798477
79.693493	2345.289402	21.803495
79.662885	2340.728668	21.808512
79.686467	2346.395392	21.813530
79.902057	2346.733623	21.818547
79.907294	2339.122765	21.823565
80.229328	2346.927737	21.828583
80.022201	2349.378394	21.833600
80.145593	2347.410239	21.838618
79.905933	2353.624662	21.843635
80.282267	2345.382036	21.848653
79.976973	2341.197275	21.853671
80.099030	2343.479836	21.858688
80.257536	2339.568792	21.863706
80.170217	2365.215853	21.868723
79.818962	2373.358327	21.873741
80.177750	2376.100383	21.878759
80.227144	2372.266915	21.883776
80.446339	2388.158104	21.888794
80.652411	2387.954991	21.893811
80.905906	2399.317931	21.898829
80.916021	2395.459881	21.903847
80.739601	2385.131478	21.908864
80.799692	2394.701704	21.913882
80.894270	2413.467250	21.918899
81.160147	2414.985743	21.923917
81.211708	2429.201242	21.928935
81.493347	2425.621692	21.933952
81.668485	2419.437719	21.938970
81.738261	2424.203462	21.943987
81.860769	2419.756633	21.949005
81.686285	2412.224427	21.954023
81.851854	2417.992387	21.959040
82.024408	2412.539970	21.964058
81.831121	2410.572858	21.969075
82.175461	2436.486498	21.974093
82.502999	2433.730840	21.979111
82.446226	2439.520797	21.984128
82.948391	2436.445951	21.989146
82.389864	2421.769871	21.994163
82.303189	2427.016746	21.999181
82.567457	2432.567122	22.004199
82.640345	2441.216326	22.009216
83.108545	2437.388440	22.014234
82.779873	2443.463750	22.019251
82.569660	2433.073212	22.024269
82.858560	2437.918294	22.029287
82.958483	2442.219964	22.034304
83.094023	2436.494941	22.039322
82.853782	2442.309090	22.044339
82.779354	2445.238119	22.049357
83.265197	2461.164993	22.054375
82.995800	2471.991637	22.059392
83.447596	2458.633098	22.064410
83.902828	2453.760874	22.069427
84.248867	2438.263170	22.074445
84.422127	2448.618977	22.079463
84.869279	2430.521720	22.084480
84.951794	2432.864018	22.089498
84.669188	2426.766351	22.094515
84.849615	2399.518702	22.099533
84.774505	2406.026281	22.104551
84.547014	2397.295378	22.109568
84.770003	2404.581391	22.114586
84.655765	2395.233226	22.119603
84.954178	2394.903346	22.124621
84.514130	2386.646367	22.129639
84.835169	2401.067063	22.134656
84.596064	2390.509697	22.139674
84.561427	2396.828651	22.144691
84.874796	2398.354605	22.149709
85.155539	2414.928133	22.154727
84.968774	2418.357728	22.159744
85.610716	2429.256912	22.164762
85.344800	2426.525074	22.169779
85.307130	2427.887315	22.174797
84.887466	2432.045402	22.179815
85.168130	2432.500385	22.184832
85.554223	2454.384558	22.189850
85.561859	2457.466097	22.194867
85.309277	2457.456138	22.199885
85.658269	2457.228092	22.204903
85.539236	2465.333202	22.209920
85.641094	2478.167116	22.214938
85.668822	2492.198832	22.219955
85.707260	2496.371359	22.224973
86.055809	2506.049234	22.229991
86.238403	2516.594094	22.235008
86.712378	2516.449610	22.240026
86.647846	2520.301843	22.245043
86.254557	2514.741451	22.250061
86.602659	2513.635569	22.255079
86.540209	2541.717849	22.260096
86.985774	2535.266440	22.265114
87.296817	2546.054944	22.270131
87.071678	2537.894063	22.275149
87.312965	2540.704497	22.280167
87.429112	2546.218111	22.285184
87.714269	2536.689308	22.290202
87.319841	2534.442604	22.295219
87.558069	2534.882988	22.300237
87.852459	2530.150073	22.305255
87.587218	2532.439544	22.310272
88.015471	2543.308571	22.315290
87.849211	2556.420580	22.320307
87.584201	2563.136562	22.325325
88.238267	2560.776240	22.330343
87.936854	2572.020494	22.335360
87.846628	2561.630403	22.340378
87.909959	2571.070667	22.345395
88.037294	2593.385061	22.350413
88.197849	2594.023795	22.355431
88.099809	2601.521526	22.360448
88.226783	2595.408877	22.365466
88.537067	2613.081294	22.370483
88.737961	2612.779036	22.375501
89.362979	2618.776635	22.380519
89.299664	2622.057013	22.385536
89.121101	2618.147583	22.390554
89.006188	2620.960139	22.395571
89.114116	2614.731351	22.400589
89.559372	2603.346299	22.405607
89.191516	2609.548268	22.410624
89.459491	2615.549688	22.415642
89.873696	2629.561397	22.420659
89.734791	2634.337474	22.425677
89.950904	2624.670480	22.430695
89.719874	2637.208650	22.435712
90.312653	2620.098434	22.440730
90.519557	2625.021772	22.445747
90.580591	2627.436963	22.450765
90.580587	2620.761523	22.455783
90.565838	2629.423034	22.460800
90.555962	2620.510951	22.465818
90.701831	2626.847248	22.470835
90.674623	2623.817426	22.475853
90.892612	2622.771744	22.480871
90.963288	2631.274565	22.485888
90.780239	2625.244135	22.490906
91.010655	2617.468155	22.495923
90.890773	2630.037457	22.500941
91.112892	2638.973402	22.505959
91.065326	2659.466878	22.510976
91.007444	2650.375740	22.515994
91.242666	2654.424659	22.521011
90.895028	2670.105993	22.526029
91.416944	2671.215410	22.531047
91.140077	2692.066341	22.536064
91.442567	2681.756582	22.541082
91.698054	2697.769229	22.546099
91.617334	2707.359505	22.551117
92.237754	2699.961606	22.556135
92.343568	2712.859232	22.561152
92.630237	2705.189613	22.566170
92.279300	2697.209798	22.571187
92.342433	2706.952948	22.576205
92.304085	2722.077400	22.581223
92.421922	2724.080390	22.586240
92.673593	2729.000653	22.591258
92.927804	2722.113230	22.596275
93.258226	2720.433473	22.601293
93.372553	2726.164786	22.606311
93.227397	2727.989032	22.611328
92.969423	2726.898419	22.616346
92.973525	2728.330520	22.621363
93.497820	2750.681144	22.626381
93.940330	2754.618865	22.631399
93.670374	2754.486196	22.636416
93.953116	2749.267331	22.641434
93.999618	2750.777431	22.646451
94.013407	2755.682508	22.651469
94.388662	2748.486360	22.656487
93.976316	2759.352707	22.661504
94.354773	2747.942429	22.666522
94.424759	2750.488836	22.671539
94.199558	2752.594904	22.676557
94.200875	2752.514401	22.681575
93.895529	2758.239482	22.686592
94.313935	2768.132695	22.691610
94.240502	2783.239807	22.696627
94.088146	2779.414961	22.701645
94.508805	2792.263087	22.706663
94.627853	2801.669822	22.711680
94.827331	2798.429450	22.716698
95.319757	2791.061834	22.721715
95.376624	2794.700249	22.726733
95.639134	2781.611882	22.731751
95.791440	2792.848613	22.736768
95.837020	2785.884803	22.741786
95.744528	2785.607675	22.746803
95.597281	2791.872271	22.751821
96.319847	2791.167551	22.756839
96.219166	2786.738810	22.761856
96.357019	2783.893742	22.766874
96.610213	2778.555756	22.771891
96.214600	2788.898056	22.776909
96.259308	2785.165664	22.781927
96.309879	2811.716577	22.786944
96.335602	2820.512027	22.791962
96.425760	2815.740129	22.796979
96.173475	2822.577735	22.801997
96.247126	2814.796605	22.807015
96.564043	2842.504555	22.812032
96.722874	2854.363903	22.817050
96.855276	2856.594819	22.822067
96.895084	2846.276633	22.827085
97.379077	2868.572705	22.832103
97.616648	2883.723905	22.837120
97.512307	2874.649806	22.842138
97.611585	2872.300531	22.847155
97.703914	2874.112100	22.852173
97.788231	2876.917972	22.857191
97.740239	2874.808538	22.862208
97.581737	2878.380395	22.867226
98.137429	2887.891795	22.872243
98.259051	2900.724347	22.877261
98.622388	2894.406150	22.882279
98.526738	2895.726489	22.887296
98.262943	2894.208460	22.892314
99.043330	2883.290771	22.897331
98.858015	2889.913723	22.902349
98.950505	2894.984515	22.907367
99.050818	2906.671333	22.912384
99.040646	2898.524935	22.917402
99.533476	2906.167547	22.922419
99.005445	2900.603814	22.927437
99.303722	2904.341515	22.932455
99.660397	2919.264282	22.937472
99.712710	2927.256506	22.942490
99.945050	2924.864244	22.947507
99.799883	2932.429024	22.952525
100.053759	2935.936301	22.957543
100.183507	2926.270480	22.962560
100.037012	2931.390056	22.967578
100.316989	2927.829568	22.972595
99.723331	2932.856909	22.977613
99.876877	2919.930244	22.982631
99.843526	2931.619214	22.987648
100.372229	2944.141225	22.992666
100.865824	2949.676120	22.997683
100.807211	2960.473978	23.002701
100.761157	2956.701900	23.007719
100.510812	2952.948811	23.012736
100.269090	2958.421643	23.017754
100.977997	2965.070048	23.022771
101.248589	2976.369150	23.027789
101.462947	2968.745280	23.032807
101.725895	2970.293059	23.037824
101.470359	2981.726057	23.042842
101.584772	2971.415078	23.047859
101.731521	2964.014664	23.052877
101.883972	2971.218567	23.057895
101.823277	2977.210963	23.062912
101.566830	2969.326729	23.067930
101.870334	2983.619771	23.072947
102.022980	2994.351441	23.077965
102.019342	3000.824554	23.082983
101.721214	3004.824788	23.088000
101.567779	3010.585349	23.093018
102.159821	3019.810455	23.098035
102.475990	3027.335626	23.103053
102.334335	3031.168909	23.108071
102.403729	3036.845202	23.113088
102.824083	3054.965611	23.118106
103.261937	3047.845151	23.123123
103.425181	3061.308759	23.128141
103.750060	3057.231296	23.133159
103.749314	3054.864362	23.138176
103.501917	3053.326267	23.143194
103.895187	3051.983300	23.148211
104.067606	3053.137836	23.153229
103.893490	3054.246802	23.158247
104.199017	3043.828813	23.163264
103.971442	3040.596364	23.168282
104.296909	3037.859058	23.173299
104.067710	3046.639909	23.178317
104.154678	3054.987094	23.183335
104.790384	3065.575934	23.188352
104.726683	3076.120763	23.193370
104.643343	3067.382062	23.198387
104.707268	3078.162788	23.203405
104.750016	3083.455703	23.208423
104.856514	3072.401824	23.213440
104.867345	3078.287091	23.218458
105.113221	3084.373867	23.223475
105.183350	3096.582023	23.228493
105.321257	3089.208613	23.233511
105.680399	3087.994158	23.238528
105.295755	3088.054177	23.243546
105.214701	3090.817486	23.248563
105.447383	3105.751589	23.253581
105.513268	3116.109937	23.258599
106.267916	3113.992292	23.263616
105.320534	3127.280654	23.268634
105.864006	3131.781660	23.273651
106.018519	3140.007816	23.278669
106.233722	3145.125231	23.283687
106.550305	3152.671262	23.288704
106.554588	3169.433281	23.293722
106.925557	3171.639559	23.298739
106.931187	3174.579043	23.303757
107.438867	3175.043573	23.308775
107.548820	3155.254138	23.313792
107.457263	3163.740507	23.318810
107.506321	3155.651853	23.323827
107.670406	3160.523025	23.328845
107.615593	3153.141056	23.333863
107.612112	3155.553664	23.338880
107.694212	3159.497837	23.343898
107.719468	3148.940907	23.348915
107.936085	3157.332355	23.353933
107.757070	3176.367140	23.358951
108.073056	3180.999673	23.363968
108.044553	3181.521020	23.368986
108.340996	3176.597793	23.374003
108.336993	3180.757083	23.379021
108.353970	3178.605312	23.384039
108.791096	3198.085413	23.389056
108.859118	3206.163759	23.394074
109.328039	3204.222729	23.399091
109.186243	3209.534149	23.404109
108.887714	3209.664509	23.409127
109.206705	3197.010933	23.414144
109.348446	3215.040418	23.419162
109.428900	3211.926837	23.424179
109.421776	3208.396280	23.429197
109.384255	3204.427826	23.434215
109.513216	3225.262031	23.439232
109.360501	3229.284617	23.444250
109.641892	3234.433192	23.449267
109.722921	3244.459555	23.454285
109.802869	3263.447867	23.459303
110.237338	3270.082165	23.464320
110.660015	3273.568162	23.469338
110.487500	3268.099951	23.474355
110.596147	3265.260044	23.479373
110.392506	3272.879985	23.484391
111.014384	3285.352140	23.489408
110.822414	3301.083045	23.494426
110.780755	3293.511800	23.499443
111.112853	3293.168041	23.504461
111.092634	3303.427427	23.509479
111.297909	3307.037756	23.514496
111.431569	3319.163081	23.519514
111.569303	3322.567690	23.524531
111.313376	3320.559684	23.529549
111.389594	3328.959201	23.534567
111.758753	3341.249757	23.539584
111.657228	3357.510618	23.544602
112.063730	3343.155224	23.549619
112.196598	3363.805877	23.554637
112.423787	3367.651576	23.559655
112.323299	3377.563688	23.564672
112.413794	3389.172571	23.569690
113.064027	3381.940677	23.574707
113.037459	3382.076636	23.579725
113.142890	3372.328353	23.584743
113.721382	3370.939619	23.589760
113.472617	3371.449934	23.594778
113.661904	3363.939498	23.599795
114.213098	3373.023955	23.604813
114.015530	3364.429278	23.609831
113.961128	3360.242310	23.614848
113.756384	3360.611833	23.619866
114.031213	3363.931065	23.624883
114.233304	3378.739400	23.629901
114.202737	3389.392330	23.634919
114.390415	3375.722542	23.639936
114.497758	3386.327746	23.644954
114.657004	3386.758053	23.649971
114.903455	3382.441943	23.654989
114.870845	3379.949534	23.660007
114.803243	3376.654206	23.665024
114.670856	3386.809835	23.670042
114.731968	3393.897605	23.675059
115.063127	3410.593751	23.680077
114.969286	3415.527946	23.685095
115.327807	3411.147137	23.690112
115.144200	3418.020050	23.695130
115.314372	3442.659861	23.700147
115.451511	3440.602663	23.705165
115.798528	3455.245636	23.710183
115.890122	3443.854569	23.715200
115.953367	3449.622594	23.720218
116.802377	3445.681970	23.725235
116.817572	3423.301003	23.730253
116.918900	3422.958973	23.735271
117.114425	3416.830281	23.740288
116.772246	3419.066909	23.745306
116.879038	3412.992338	23.750323
117.191683	3415.071324	23.755341
117.120154	3408.171585	23.760359
117.355813	3414.481864	23.765376
117.235063	3419.739852	23.770394
117.215152	3444.181706	23.775411
116.964469	3454.915751	23.780429
117.134759	3451.673010	23.785447
117.457237	3442.040204	23.790464
117.545810	3461.341527	23.795482
117.589442	3459.566820	23.800499
118.049578	3473.839010	23.805517
118.017807	3469.754168	23.810535
118.361221	3461.204196	23.815552
117.933036	3478.784156	23.820570
118.184048	3494.634573	23.825587
118.354931	3493.999066	23.830605
118.573123	3494.293190	23.835623
118.923755	3503.469721	23.840640
118.538433	3522.979805	23.845658
118.984366	3518.966762	23.850675
119.331046	3522.668221	23.855693
119.016167	3515.698626	23.860711
119.661102	3532.455371	23.865728
119.644179	3541.542595	23.870746
119.644775	3545.422056	23.875763
119.994429	3536.338276	23.880781
120.024039	3549.122474	23.885799
120.349151	3534.550487	23.890816
120.166647	3548.980331	23.895834
120.534457	3563.025402	23.900851
120.584726	3573.807165	23.905869
120.226857	3577.512715	23.910887
120.605161	3568.971061	23.915904
120.590389	3576.707810	23.920922
120.456769	3578.216030	23.925939
121.016091	3590.305480	23.930957
120.877044	3597.169097	23.935975
121.179678	3600.098286	23.940992
121.291637	3598.938259	23.946010
121.167048	3617.015617	23.951027
121.764430	3614.435805	23.956045
121.619319	3622.843123	23.961063
122.046625	3611.398115	23.966080
121.962276	3623.600462	23.971098
122.108575	3631.875886	23.976115
122.674715	3649.566815	23.981133
122.208551	3651.107072	23.986151
122.301439	3654.959412	23.991168
122.432534	3656.653202	23.996186
122.415049	3647.483108	24.001203
122.841674	3662.231563	24.006221
122.633788	3681.674952	24.011239
122.756204	3676.456439	24.016256
122.949705	3682.321815	24.021274
123.154395	3698.306135	24.026291
123.632851	3694.716432	24.031309
123.528055	3716.242965	24.036327
123.900670	3713.465423	24.041344
123.911302	3712.011955	24.046362
123.723883	3711.906899	24.051379
123.812329	3719.943531	24.056397
123.931195	3729.976124	24.061415
123.875539	3734.691845	24.066432
123.821525	3742.968722	24.071450
124.449948	3763.118215	24.076467
124.685529	3762.872779	24.081485
124.586468	3776.345945	24.086503
124.910452	3768.591647	24.091520
125.268995	3764.528491	24.096538
125.143366	3766.344097	24.101555
125.921615	3762.998295	24.106573
125.968842	3764.378831	24.111591
126.056525	3752.234167	24.116608
126.078195	3763.355890	24.121626
125.995276	3754.598622	24.126643
126.174033	3746.822400	24.131661
126.095597	3770.127113	24.136679
126.597776	3768.824660	24.141696
126.739590	3773.710751	24.146714
126.761319	3778.373463	24.151731
126.925126	3770.637513	24.156749
126.873571	3775.824667	24.161767
126.937531	3771.280085	24.166784
127.003782	3774.093454	24.171802
126.921366	3767.438699	24.176819
127.008190	3763.285248	24.181837
127.239510	3776.826755	24.186855
127.485532	3788.475847	24.191872
127.616520	3792.568769	24.196890
127.554758	3795.386088	24.201907
127.656630	3791.999904	24.206925
127.739632	3819.114532	24.211943
127.950312	3816.795823	24.216960
128.197414	3827.129648	24.221978
127.984132	3830.534818	24.226995
128.405567	3852.214672	24.232013
128.334846	3864.783883	24.237031
128.290836	3868.092420	24.242048
128.689572	3867.794277	24.247066
128.479471	3881.029655	24.252083
128.797229	3885.904655	24.257101
128.818710	3900.817525	24.262119
128.845700	3909.612984	24.267136
128.954269	3909.456378	24.272154
129.235841	3925.847106	24.277171
129.875436	3924.005206	24.282189
129.797544	3931.195463	24.287207
130.123115	3937.614258	24.292224
130.509769	3930.786592	24.297242
130.565452	3927.001310	24.302259
130.610670	3922.190869	24.307277
130.785912	3936.627377	24.312295
130.835631	3947.930028	24.317312
130.818299	3948.397963	24.322330
131.038815	3953.795902	24.327347
131.369098	3946.708665	24.332365
131.412549	3962.412531	24.337383
131.262102	3955.005125	24.342400
131.560910	3958.982790	24.347418
131.684088	3970.772526	24.352435
132.085564	3969.200929	24.357453
131.868941	3977.660877	24.362471
131.942561	3975.998466	24.367488
132.177241	3966.944570	24.372506
132.335631	3969.971825	24.377523
132.338540	3977.035669	24.382541
132.955478	3987.245537	24.387559
132.549148	3992.357841	24.392576
132.887618	3990.068665	24.397594
132.854009	3992.904967	24.402611
132.922005	3991.803011	24.407629
133.312222	3985.955959	24.412647
133.341800	3989.875602	24.417664
133.907572	4000.223132	24.422682
134.111866	4012.050608	24.427699
134.167131	3980.872850	24.432717
133.930630	3987.278361	24.437735
133.840456	3994.921139	24.442752
134.080457	4004.243533	24.447770
134.242092	4008.090048	24.452787
134.438044	4008.035078	24.457805
134.505810	4015.880785	24.462823
134.423664	4009.768079	24.467840
134.829448	4031.936280	24.472858
134.657612	4047.059783	24.477875
134.996233	4047.732780	24.482893
134.661783	4042.661333	24.487911
134.771989	4057.229249	24.492928
135.127065	4065.139851	24.497946
135.077528	4080.324964	24.502963
135.723859	4081.687086	24.507981
135.877955	4090.271343	24.512999
135.731510	4097.496692	24.518016
136.174800	4095.010925	24.523034
136.116014	4110.195242	24.528051
136.271130	4114.685474	24.533069
136.778002	4117.466242	24.538087
136.830760	4115.567093	24.543104
137.439360	4101.490855	24.548122
137.242119	4121.341737	24.553139
137.067676	4109.515983	24.558157
137.210300	4124.653456	24.563175
137.586212	4134.445537	24.568192
137.819484	4145.052776	24.573210
137.665658	4151.674962	24.578227
137.621164	4143.929736	24.583245
138.089685	4145.583653	24.588263
137.788773	4141.920970	24.593280
138.278958	4154.385788	24.598298
138.290315	4165.212225	24.603315
138.720102	4161.219031	24.608333
138.791546	4177.191334	24.613351
138.602937	4169.628727	24.618368
138.819966	4180.324134	24.623386
138.467249	4202.918269	24.628403
138.569170	4192.779059	24.633421
139.229982	4203.753149	24.638439
139.359633	4218.484150	24.643456
139.307200	4221.174386	24.648474
139.377516	4230.893670	24.653491
139.865292	4247.972622	24.658509
140.132096	4257.465936	24.663527
140.055339	4252.101562	24.668544
140.353737	4250.034395	24.673562
140.613283	4261.289804	24.678579
140.508049	4267.857894	24.683597
140.724237	4265.181460	24.688615
140.621975	4278.076763	24.693632
140.594395	4266.997072	24.698650
140.720608	4288.851018	24.703667
141.245103	4291.069751	24.708685
141.363021	4296.826641	24.713703
141.316814	4311.104202	24.718720
141.618126	4311.632995	24.723738
141.810684	4322.146711	24.728755
142.029823	4324.238211	24.733773
142.065989	4327.733552	24.738791
142.171764	4330.231351	24.743808
142.576740	4330.402709	24.748826
142.467641	4339.322221	24.753843
143.007206	4341.328977	24.758861
143.337935	4347.617538	24.763879
143.395023	4346.485869	24.768896
143.867750	4340.200109	24.773914
143.977810	4340.665394	24.778931
143.887848	4321.543629	24.783949
143.706620	4305.336699	24.788967
143.533128	4326.776652	24.793984
143.838395	4334.379873	24.799002
144.168716	4335.873285	24.804019
143.804214	4332.350671	24.809037
144.059314	4333.788855	24.814055
144.150007	4342.576728	24.819072
144.835672	4362.113065	24.824090
144.301992	4365.206180	24.829107
144.277451	4363.855756	24.834125
144.830391	4382.871571	24.839143
144.682666	4396.165924	24.844160
145.131872	4381.248861	24.849178
145.123088	4403.801095	24.854195
145.276006	4409.723891	24.859213
145.443873	4416.567185	24.864231
145.194090	4417.592346	24.869248
145.900961	4430.167463	24.874266
146.108379	4448.114612	24.879283
146.427904	4440.810798	24.884301
146.895742	4441.307987	24.889319
146.884236	4450.783088	24.894336
147.144837	4467.781116	24.899354
146.984421	4465.264882	24.904371
146.971859	4472.200397	24.909389
147.128333	4469.551964	24.914407
147.232722	4466.829497	24.919424
147.542803	4481.481148	24.924442
147.927833	4478.767959	24.929459
148.346417	4477.454144	24.934477
148.562230	4476.952102	24.939495
148.492091	4483.213615	24.944512
148.717338	4475.427733	24.949530
148.809510	4476.882767	24.954547
149.113911	4477.848131	24.959565
149.171543	4460.925649	24.964583
149.013684	4472.687649	24.969600
149.168785	4467.027152	24.974618
149.002069	4471.822582	24.979635
149.603070	4468.689193	24.984653
149.367136	4473.884377	24.989671
149.385107	4478.832614	24.994688
149.607575	4490.865340	24.999706
149.647901	4491.245352	25.004723
149.698624	4506.769393	25.009741
149.844260	4509.718152	25.014759
149.941400	4529.765948	25.019776
150.163957	4523.509874	25.024794
150.235038	4544.499967	25.029811
150.334670	4557.587185	25.034829
150.640182	4565.155827	25.039847
150.599861	4583.571140	25.044864
151.910438	4572.076714	25.049882
151.788269	4571.484350	25.054899
152.042126	4569.408793	25.059917
151.994939	4573.063733	25.064935
151.855721	4580.147922	25.069952
152.110900	4563.966649	25.074970
152.156062	4565.301922	25.079987
152.418549	4588.055842	25.085005
152.567751	4595.159839	25.090023
152.488791	4602.679770	25.095040
152.587091	4599.314088	25.100058
152.539114	4590.786017	25.105075
152.778536	4606.761559	25.110093
153.013316	4622.444926	25.115111
152.894513	4630.448736	25.120128
153.245094	4631.532443	25.125146
153.262015	4633.293747	25.130163
153.296507	4641.240588	25.135181
153.871392	4661.136713	25.140199
153.298318	4665.582331	25.145216
153.786053	4684.378601	25.150234
153.795066	4691.433483	25.155251
153.973709	4705.214905	25.160269
154.460473	4703.825953	25.165287
154.838313	4710.436812	25.170304
155.371803	4723.303230	25.175322
155.295764	4739.454971	25.180339
155.415617	4740.703032	25.185357
155.688409	4731.288364	25.190375
155.378168	4750.312605	25.195392
155.885830	4731.598998	25.200410
156.132685	4745.239176	25.205427
155.850865	4761.333779	25.210445
156.353830	4755.154663	25.215463
156.186324	4761.456092	25.220480
156.346549	4773.204837	25.225498
156.641960	4787.813537	25.230515
156.370790	4785.541680	25.235533
156.862947	4801.792804	25.240551
156.970328	4817.162042	25.245568
156.959116	4817.591577	25.250586
157.256624	4829.661710	25.255603
157.653095	4846.598195	25.260621
157.968872	4850.419700	25.265639
157.420039	4851.242564	25.270656
158.015218	4865.577861	25.275674
158.167702	4879.503966	25.280691
158.583834	4878.122012	25.285709
158.300838	4875.605603	25.290727
158.516293	4897.646394	25.295744
158.446058	4907.869463	25.300762
159.184606	4914.902452	25.305779
159.144236	4923.197372	25.310797
159.485442	4924.491359	25.315815
159.664949	4933.469569	25.320832
160.119740	4927.670903	25.325850
159.823556	4927.294878	25.330867
160.168715	4949.678037	25.335885
160.768725	4952.566342	25.340903
160.389071	4966.532119	25.345920
160.879273	4955.821109	25.350938
160.905178	4957.350203	25.355955
160.758099	4956.265018	25.360973
161.149572	4961.675065	25.365991
161.044194	4978.317058	25.371008
161.070107	4980.790430	25.376026
161.505238	4990.768917	25.381043
161.495002	5006.920236	25.386061
161.631017	5016.498749	25.391079
161.829447	5018.151967	25.396096
161.826690	5024.563947	25.401114
162.336249	5037.409399	25.406131
162.187740	5053.143498	25.411149
162.450590	5035.874426	25.416167
162.582841	5060.392745	25.421184
162.656952	5071.706329	25.426202
162.879030	5084.358596	25.431219
163.012219	5087.389077	25.436237
163.118096	5092.619022	25.441255
163.061688	5102.913950	25.446272
163.360851	5108.351988	25.451290
163.548389	5119.186036	25.456307
163.389694	5133.468859	25.461325
163.727592	5136.283407	25.466343
164.183177	5151.915649	25.471360
164.085720	5163.561806	25.476378
164.264128	5162.109071	25.481395
164.015310	5192.529116	25.486413
164.464448	5193.083784	25.491431
165.175843	5212.630301	25.496448
165.549721	5208.081455	25.501466
165.858997	5202.026497	25.506483
166.354654	5206.328542	25.511501
166.289610	5201.037503	25.516519
166.232495	5210.171749	25.521536
166.854491	5209.725840	25.526554
167.159558	5208.778936	25.531571
167.296633	5199.555081	25.536589
167.374974	5183.437997	25.541607
167.303904	5183.133242	25.546624
167.413179	5201.060546	25.551642
167.538741	5205.457953	25.556659
167.174788	5213.131063	25.561677
167.788405	5215.512329	25.566695
168.009522	5213.384638	25.571712
167.687633	5208.610389	25.576730
167.760265	5223.122627	25.581747
168.026407	5243.564599	25.586765
168.292561	5237.548296	25.591783
168.389823	5261.571851	25.596800
168.433664	5273.199336	25.601818
168.491096	5283.346305	25.606835
168.717987	5300.505201	25.611853
169.115327	5306.930359	25.616871
169.038725	5313.413794	25.621888
169.441447	5340.674818	25.626906
169.451112	5338.460173	25.631923
169.575022	5349.186028	25.636941
169.620536	5373.569610	25.641959
169.766923	5384.325620	25.646976
170.183357	5383.804393	25.651994
170.593161	5406.072714	25.657011
170.562585	5408.125524	25.662029
170.774432	5413.041052	25.667047
171.055697	5431.283422	25.672064
171.001173	5432.667624	25.677082
171.609931	5436.379161	25.682100
171.489640	5461.909575	25.687117
171.852719	5457.179736	25.692135
171.803555	5461.272315	25.697152
171.640721	5479.902777	25.702170
172.425306	5486.403065	25.707188
172.348882	5495.482404	25.712205
172.541906	5515.859696	25.717223
172.891874	5518.255679	25.722240
172.955751	5530.427392	25.727258
173.376037	5524.401909	25.732276
173.194845	5537.713811	25.737293
173.582081	5531.111006	25.742311
173.238246	5531.855732	25.747328
173.400444	5551.156845	25.752346
174.152261	5548.063562	25.757364
175.167835	5535.594404	25.762381
175.373545	5534.524589	25.767399
175.730390	5529.695742	25.772416
175.333464	5528.046382	25.777434
175.837628	5514.086270	25.782452
175.228898	5502.673829	25.787469
176.104356	5491.614915	25.792487
175.995634	5492.923070	25.797504
175.720903	5495.679602	25.802522
176.220172	5511.438046	25.807540
175.995278	5518.645578	25.812557
176.198319	5527.037408	25.817575
176.016331	5528.809024	25.822592
175.957386	5528.288025	25.827610
176.332295	5540.052865	25.832628
176.259421	5552.033883	25.837645
176.228931	5575.936594	25.842663
176.673110	5585.329572	25.847680
176.920437	5604.674887	25.852698
177.056448	5619.376218	25.857716
177.198516	5632.546277	25.862733
178.276282	5630.048576	25.867751
178.613794	5627.441541	25.872768
178.723119	5630.012204	25.877786
179.059116	5631.933250	25.882804
178.907867	5623.124071	25.887821
179.072529	5639.973919	25.892839
178.878785	5636.296617	25.897856
179.092766	5651.694638	25.902874
179.524688	5647.174616	25.907892
179.261528	5666.160631	25.912909
179.225655	5688.023767	25.917927
179.554510	5681.970099	25.922944
179.573848	5704.284823	25.927962
180.119982	5705.125830	25.932980
180.150662	5722.361894	25.937997
180.457516	5729.576464	25.943015
180.729941	5743.079371	25.948032
180.620920	5762.676263	25.953050
180.992975	5765.401766	25.958068
181.170833	5790.296415	25.963085
181.235575	5786.190207	25.968103
181.361051	5797.744657	25.973120
181.537668	5819.740425	25.978138
182.040034	5816.179755	25.983156
182.155909	5837.503584	25.988173
182.236202	5832.774154	25.993191
182.703827	5842.030288	25.998208
182.508050	5859.586090	26.003226
183.090018	5859.351596	26.008244
183.197251	5870.831946	26.013261
183.441315	5877.295410	26.018279
183.706673	5885.584141	26.023296
183.575871	5904.728021	26.028314
183.885988	5896.175184	26.033332
183.984510	5906.517352	26.038349
184.509279	5922.228655	26.043367
184.689751	5927.558323	26.048384
184.511240	5928.826128	26.053402
184.676301	5929.150794	26.058420
184.959915	5941.960500	26.063437
184.980301	5951.858084	26.068455
185.144390	5961.302555	26.073472
185.162704	5981.985141	26.078490
185.607237	5979.090907	26.083508
185.554100	5996.844476	26.088525
185.885450	6013.154296	26.093543
186.457718	6009.475643	26.098560
186.592367	6008.092324	26.103578
186.797182	6021.463361	26.108596
186.796441	6041.070172	26.113613
186.818411	6043.152138	26.118631
187.089551	6034.087458	26.123648
187.174817	6048.588906	26.128666
187.323851	6064.280084	26.133684
187.214366	6073.103762	26.138701
187.165081	6071.320967	26.143719
187.590227	6090.482174	26.148736
187.951289	6110.844130	26.153754
188.087501	6118.246329	26.158772
188.353335	6125.507277	26.163789
188.616391	6149.403822	26.168807
189.237408	6156.942078	26.173824
189.036586	6155.686949	26.178842
189.498590	6155.010846	26.183860
189.459247	6180.219439	26.188877
189.435171	6180.064377	26.193895
190.120687	6184.824258	26.198912
189.892325	6212.551592	26.203930
190.300267	6202.671745	26.208948
190.694622	6219.751835	26.213965
190.699499	6234.988266	26.218983
191.162346	6241.963708	26.224000
191.282967	6241.451442	26.229018
191.610110	6240.895408	26.234036
191.612270	6261.204564	26.239053
191.691262	6272.153532	26.244071
191.614341	6268.591353	26.249088
191.959748	6286.561780	26.254106
192.062360	6286.573120	26.259124
192.272053	6294.794918	26.264141
192.024845	6320.485639	26.269159
192.576882	6338.252454	26.274176
192.740313	6348.068235	26.279194
193.058371	6360.325161	26.284212
193.313834	6384.906193	26.289229
193.587511	6390.174061	26.294247
194.129136	6378.162638	26.299264
193.887992	6391.794755	26.304282
194.206530	6392.496406	26.309300
194.508251	6404.978191	26.314317
194.279915	6411.627485	26.319335
194.974544	6425.871291	26.324352
194.820293	6437.836571	26.329370
195.146223	6445.182985	26.334388
195.405705	6465.591419	26.339405
195.379517	6468.635260	26.344423
196.025350	6484.174998	26.349440
196.300790	6497.610315	26.354458
196.156793	6500.093254	26.359476
196.394980	6511.666517	26.364493
196.570277	6518.485078	26.369511
196.836096	6530.251459	26.374528
196.521847	6543.127124	26.379546
196.807958	6558.558153	26.384564
197.250397	6559.840188	26.389581
197.328827	6584.389510	26.394599
197.825137	6584.660728	26.399616
197.169545	6599.518918	26.404634
198.041630	6616.688615	26.409652
198.331133	6636.859930	26.414669
198.360869	6650.436232	26.419687
198.810364	6652.823733	26.424704
198.736364	6661.399249	26.429722
198.960908	6671.347639	26.434740
199.111934	6691.048184	26.439757
199.292188	6694.821775	26.444775
199.472390	6698.672564	26.449792
199.731260	6706.955718	26.454810
200.132071	6710.148408	26.459828
200.705774	6712.653905	26.464845
200.749982	6730.112509	26.469863
200.957057	6734.988288	26.474880
201.065663	6738.990396	26.479898
201.060682	6738.258753	26.484916
201.633844	6732.985606	26.489933
201.564048	6750.166234	26.494951
202.193540	6746.213261	26.499968
201.916240	6755.026607	26.504986
202.268298	6766.458266	26.510004
202.689668	6758.900964	26.515021
202.166015	6786.983182	26.520039
202.774918	6786.508703	26.525056
202.768142	6803.790763	26.530074
202.842640	6810.085875	26.535092
203.405932	6815.316005	26.540109
203.636051	6833.396003	26.545127
203.855537	6846.239153	26.550144
204.306696	6852.500053	26.555162
203.853108	6854.071982	26.560180
204.543751	6861.035057	26.565197
204.439357	6874.236075	26.570215
204.789911	6875.847678	26.575232
204.832800	6887.658455	26.580250
205.090491	6893.916860	26.585268
205.247240	6902.088699	26.590285
205.492009	6920.278995	26.595303
205.609307	6928.003715	26.600320
205.677708	6948.955708	26.605338
205.888486	6958.747461	26.610356
206.333750	6972.993027	26.615373
205.989698	6997.540722	26.620391
206.563271	7009.514676	26.625408
206.738399	7031.262691	26.630426
206.898688	7032.479801	26.635444
207.293222	7044.889961	26.640461
207.742848	7049.983101	26.645479
208.183594	7059.292468	26.650496
208.492625	7071.255288	26.655514
208.693897	7079.203214	26.660532
209.095697	7075.514052	26.665549
208.905778	7084.466654	26.670567
208.913766	7077.467024	26.675584
209.131194	7100.768455	26.680602
209.415949	7107.135872	26.685620
209.727102	7116.523517	26.690637
209.656620	7142.384693	26.695655
209.959643	7144.654829	26.700672
210.303130	7142.652271	26.705690
210.043979	7169.193083	26.710708
210.554613	7166.938266	26.715725
210.606654	7184.323604	26.720743
210.782327	7195.055504	26.725760
211.014287	7207.176951	26.730778
211.042847	7228.593565	26.735796
211.614380	7230.939613	26.740813
211.842086	7257.155503	26.745831
212.150049	7256.407285	26.750848
212.154352	7269.011636	26.755866
212.822207	7273.272258	26.760884
213.216251	7278.481043	26.765901
213.260517	7281.837065	26.770919
213.362543	7283.393908	26.775936
213.591415	7295.738058	26.780954
214.135953	7302.036397	26.785972
215.104726	7282.142806	26.790989
215.157646	7293.418968	26.796007
215.256309	7257.373917	26.801024
215.180919	7252.750274	26.806042
215.304743	7250.597524	26.811060
215.653959	7249.810158	26.816077
215.434345	7243.200357	26.821095
215.668148	7245.847487	26.826112
215.734544	7271.119011	26.831130
215.577958	7283.090828	26.836148
215.789635	7282.935968	26.841165
215.537409	7292.918281	26.846183
215.854511	7307.010582	26.851200
216.036961	7318.000583	26.856218
215.960261	7335.116827	26.861236
216.060214	7350.971033	26.866253
216.603084	7371.598209	26.871271
216.861881	7398.196701	26.876288
217.242340	7415.399335	26.881306
217.105417	7431.672637	26.886324
217.936090	7440.687442	26.891341
217.585242	7469.125747	26.896359
217.887716	7484.039032	26.901376
217.977037	7502.300723	26.906394
218.489616	7517.213001	26.911412
218.838983	7537.556684	26.916429
218.859603	7553.480198	26.921447
219.446486	7564.475640	26.926464
220.272049	7576.153737	26.931482
220.741616	7577.855916	26.936500
221.258594	7554.885537	26.941517
221.486007	7568.820471	26.946535
221.605215	7558.690806	26.951552
222.093509	7555.286484	26.956570
222.098070	7542.963281	26.961588
222.419498	7550.203836	26.966605
222.132435	7547.946025	26.971623
222.297016	7549.693361	26.976640
222.480413	7554.159796	26.981658
222.220862	7570.763961	26.986676
222.774193	7576.210254	26.991693
222.722556	7583.072494	26.996711
223.161800	7613.201693	27.001728
223.348099	7610.723440	27.006746
223.082420	7623.545433	27.011764
223.511935	7637.187700	27.016781
223.613869	7651.322359	27.021799
223.779727	7669.937013	27.026816
223.881018	7677.716746	27.031834
224.010741	7705.194203	27.036852
224.078210	7718.012906	27.041869
224.167589	7747.345845	27.046887
224.963967	7746.557417	27.051904
225.258147	7759.080911	27.056922
225.562172	7778.358814	27.061940
225.866580	7783.036003	27.066957
226.320910	7794.463230	27.071975
226.336868	7802.155589	27.076992
226.805903	7825.084662	27.082010
226.660446	7832.606931	27.087028
226.716068	7839.156862	27.092045
226.684636	7862.885944	27.097063
227.320292	7885.431381	27.102080
227.493939	7895.437835	27.107098
227.475129	7902.272703	27.112116
228.134238	7915.100392	27.117133
227.915601	7928.336232	27.122151
228.324395	7946.306679	27.127168
228.751544	7964.192177	27.132186
228.748700	7969.780640	27.137204
229.020255	7977.398321	27.142221
229.421146	7987.270978	27.147239
229.528714	7998.610241	27.152256
229.962792	8017.157106	27.157274
230.370368	8017.221758	27.162292
230.550104	8017.370740	27.167309
230.776325	8034.724129	27.172327
230.917052	8044.583332	27.177344
231.336973	8047.936180	27.182362
231.107344	8066.029377	27.187380
231.055968	8075.043012	27.192397
231.150199	8098.943766	27.197415
231.687863	8112.240788	27.202432
232.078915	8119.820566	27.207450
232.591561	8132.148940	27.212468
233.071868	8138.982904	27.217485
233.280749	8157.120717	27.222503
233.216709	8159.505553	27.227520
233.397737	8161.207689	27.232538
233.660869	8177.137221	27.237556
234.383975	8183.225074	27.242573
234.480967	8189.243660	27.247591
234.411851	8197.407218	27.252608
235.774000	8183.035195	27.257626
236.173460	8183.307578	27.262644
236.256003	8180.306107	27.267661
236.816928	8177.187345	27.272679
236.915962	8153.024421	27.277696
237.184526	8136.830985	27.282714
236.753139	8141.277635	27.287732
236.929113	8131.840026	27.292749
237.119354	8136.797020	27.297767
236.830739	8148.644120	27.302784
237.236408	8162.141925	27.307802
237.508838	8169.409811	27.312820
237.481317	8175.738957	27.317837
237.368742	8182.504450	27.322855
237.283427	8205.332399	27.327872
237.913339	8219.432619	27.332890
238.111046	8250.367240	27.337908
238.246336	8258.913570	27.342925
238.575194	8276.614884	27.347943
238.660637	8293.760358	27.352960
238.542484	8317.262695	27.357978
238.886497	8341.323182	27.362996
239.266823	8357.851785	27.368013
239.865753	8385.762115	27.373031
239.686871	8398.656956	27.378048
240.337477	8413.606228	27.383066
240.704749	8419.960465	27.388084
241.317078	8433.951154	27.393101
241.356680	8441.837613	27.398119
241.558573	8456.875655	27.403136
241.688224	8475.243618	27.408154
241.896241	8486.739840	27.413172
242.098274	8498.699461	27.418189
242.532890	8504.051583	27.423207
242.259159	8521.698891	27.428224
243.153086	8545.977112	27.433242
243.121629	8564.004863	27.438260
243.297817	8569.870219	27.443277
243.651988	8583.655007	27.448295
243.778739	8609.607105	27.453312
244.048052	8611.736540	27.458330
244.255635	8619.114660	27.463348
245.170375	8622.394087	27.468365
245.626000	8612.181078	27.473383
245.992338	8611.044993	27.478400
246.530436	8599.535860	27.483418
246.604559	8605.475691	27.488436
246.687800	8606.523761	27.493453
247.015064	8593.838915	27.498471
246.919984	8600.541023	27.503488
247.033275	8588.567607	27.508506
246.820648	8599.354730	27.513524
247.101667	8622.317769	27.518541
247.345884	8629.970241	27.523559
247.461650	8641.656779	27.528576
247.777903	8654.263964	27.533594
247.774765	8666.354690	27.538612
248.129557	8679.851149	27.543629
248.300900	8702.625350	27.548647
248.273774	8718.234200	27.553664
248.627121	8738.065156	27.558682
248.593828	8759.509859	27.563700
248.581887	8781.752177	27.568717
249.017517	8809.817210	27.573735
248.848746	8833.511471	27.578752
249.526422	8854.352141	27.583770
249.618272	8888.573154	27.588788
250.158957	8917.782849	27.593805
250.506312	8931.400493	27.598823
250.831113	8962.299623	27.603840
251.145182	8977.907969	27.608858
251.335471	8999.710511	27.613876
251.296849	9028.911097	27.618893
252.005851	9040.551358	27.623911
252.081804	9061.252005	27.628928
252.502022	9071.568785	27.633946
253.063580	9098.808317	27.638964
253.497576	9105.783527	27.643981
253.593932	9114.693639	27.648999
253.882879	9141.919454	27.654016
254.345071	9155.897124	27.659034
254.652750	9149.963050	27.664052
255.575997	9147.132889	27.669069
255.674976	9153.984171	27.674087
255.901179	9153.252608	27.679104
256.254858	9155.713928	27.684122
256.119963	9160.581101	27.689140
256.249554	9171.091967	27.694157
256.265431	9186.244316	27.699175
256.583860	9196.856957	27.704192
256.763776	9208.249657	27.709210
256.669959	9218.447904	27.714228
256.817932	9249.235958	27.719245
257.138620	9259.932556	27.724263
256.977232	9286.772594	27.729280
257.463794	9304.317292	27.734298
257.905823	9324.317792	27.739316
257.946452	9342.129622	27.744333
258.488324	9367.033208	27.749351
259.007550	9383.224691	27.754368
259.317441	9383.513559	27.759386
259.661444	9403.195641	27.764404
259.564645	9422.690229	27.769421
260.204502	9434.924433	27.774439
260.063133	9456.607025	27.779456
260.504075	9459.141338	27.784474
260.512768	9484.861594	27.789492
260.805238	9501.350049	27.794509
261.171934	9512.473238	27.799527
261.382565	9535.984972	27.804544
261.775823	9544.793215	27.809562
262.075661	9552.673224	27.814580
262.072739	9577.503792	27.819597
262.402082	9585.303288	27.824615
262.301222	9615.091937	27.829632
262.734414	9612.166654	27.834650
262.936804	9645.618586	27.839668
263.169843	9655.900670	27.844685
263.471907	9676.347905	27.849703
263.589289	9702.816180	27.854720
264.192514	9712.564913	27.859738
264.315173	9719.245492	27.864756
264.602038	9739.136791	27.869773
265.199331	9760.429225	27.874791
265.280430	9773.344211	27.879808
265.767926	9790.786876	27.884826
265.959915	9808.767086	27.889844
266.554319	9823.926336	27.894861
266.670525	9834.329570	27.899879
266.589617	9849.823196	27.904896
267.132586	9855.580034	27.909914
267.044459	9878.822849	27.914932
267.412622	9900.812922	27.919949
267.788671	9911.812728	27.924967
268.028096	9930.279930	27.929984
268.419894	9951.206557	27.935002
268.786091	9960.879803	27.940020
268.686900	9979.211096	27.945037
269.205431	9977.060947	27.950055
269.590797	10010.925197	27.955072
270.113032	10014.004647	27.960090
270.242773	10029.405153	27.965108
270.190372	10052.704520	27.970125
270.913392	10059.168904	27.975143
271.371156	10050.605085	27.980160
271.804100	10062.434554	27.985178
272.007367	10072.900683	27.990196
272.239694	10084.918696	27.995213
272.530249	10091.910293	28.000231
272.314937	10099.067081	28.005248
272.661083	10114.588489	28.010266
272.900669	10125.492942	28.015284
272.924334	10147.975458	28.020301
273.453261	10141.250332	28.025319
273.485913	10174.661452	28.030336
273.663771	10193.664655	28.035354
273.644862	10206.700596	28.040372
274.277262	10227.766445	28.045389
274.937939	10242.331314	28.050407
275.240089	10252.163487	28.055424
275.372062	10266.102454	28.060442
276.205338	10281.505280	28.065460
276.115833	10300.456127	28.070477
276.668040	10289.394083	28.075495
276.962560	10302.185015	28.080512
276.843136	10324.388241	28.085530
277.230679	10333.625656	28.090548
277.452765	10342.682580	28.095565
277.879555	10352.386964	28.100583
277.746067	10363.701776	28.105600
278.076038	10382.711445	28.110618
278.209599	10399.347761	28.115636
278.267965	10421.533400	28.120653
278.930558	10425.250597	28.125671
278.859978	10451.863992	28.130688
279.157650	10475.504450	28.135706
279.801927	10486.259195	28.140724
279.345356	10504.466893	28.145741
279.950937	10521.254174	28.150759
280.109626	10542.217937	28.155776
280.496927	10562.034484	28.160794
280.756831	10577.874771	28.165812
280.744813	10588.119382	28.170829
281.728796	10610.480031	28.175847
281.890594	10615.258959	28.180864
282.307505	10645.367653	28.185882
282.541697	10635.775520	28.190900
282.617384	10664.874213	28.195917
283.055939	10674.623321	28.200935
283.374692	10697.895837	28.205952
283.451620	10720.013413	28.210970
283.840075	10736.818872	28.215988
283.555154	10757.929094	28.221005
283.812536	10769.947397	28.226023
283.999790	10794.816790	28.231040
283.974350	10820.297468	28.236058
284.948800	10845.656192	28.241076
285.930440	10872.561876	28.246093
286.479500	10866.955786	28.251111
287.700212	10855.855568	28.256128
287.700328	10852.496220	28.261146
288.178827	10846.695445	28.266164
288.022864	10847.422572	28.271181
288.198478	10853.912047	28.276199
288.231104	10872.704615	28.281216
288.330903	10884.083455	28.286234
288.839393	10884.169189	28.291252
288.889451	10905.560364	28.296269
289.073960	10911.645007	28.301287
289.089614	10925.869375	28.306304
288.828167	10949.018834	28.311322
289.429800	10973.116901	28.316340
288.937651	10996.734921	28.321357
289.387920	11020.322466	28.326375
289.660247	11050.516603	28.331392
290.070104	11078.273962	28.336410
290.854402	11099.141608	28.341428
290.978092	11113.535702	28.346445
291.594792	11128.525461	28.351463
291.932994	11154.235399	28.356480
291.838468	11175.999184	28.361498
292.396112	11202.049338	28.366516
292.386271	11219.196434	28.371533
292.614187	11232.843760	28.376551
293.025147	11255.114572	28.381568
293.245560	11290.651615	28.386586
293.801192	11313.380646	28.391604
293.996068	11334.690028	28.396621
294.456256	11359.212408	28.401639
294.960704	11382.348701	28.406656
295.065540	11391.521028	28.411674
295.602032	11407.873207	28.416692
295.711617	11430.892382	28.421709
295.960418	11447.651664	28.426727
296.785636	11454.066554	28.431744
296.531426	11483.129346	28.436762
297.112892	11488.412388	28.441780
297.220009	11528.563659	28.446797
298.100247	11532.919387	28.451815
298.478815	11539.573968	28.456832
298.460278	11558.100076	28.461850
298.972446	11564.139988	28.466868
299.195136	11581.575019	28.471885
299.526985	11589.516897	28.476903
299.652603	11595.261765	28.481920
299.808115	11623.940015	28.486938
300.304172	11618.369265	28.491956
300.998913	11618.148308	28.496973
301.884244	11619.280784	28.501991
302.376173	11609.454592	28.507008
302.554343	11612.414246	28.512026
302.793664	11604.019843	28.517044
302.791201	11597.235067	28.522061
302.866659	11598.960629	28.527079
302.820299	11609.588988	28.532096
303.060678	11611.389578	28.537114
303.328168	11612.602633	28.542132
303.622530	11634.315037	28.547149
303.542380	11633.969114	28.552167
303.701150	11656.441529	28.557184
303.636253	11670.287568	28.562202
304.109307	11694.805171	28.567220
304.296425	11718.643882	28.572237
304.467767	11742.792525	28.577255
304.628521	11769.273536	28.582272
304.643802	11809.571551	28.587290
304.968908	11839.544089	28.592308
305.350621	11874.296092	28.597325
306.107805	11902.242993	28.602343
306.396578	11926.693862	28.607360
306.849938	11953.643424	28.612378
307.062073	11981.030205	28.617396
307.096795	12006.219901	28.622413
307.456824	12034.619079	28.627431
307.897940	12067.053078	28.632448
308.268888	12086.562997	28.637466
309.294974	12105.644215	28.642484
310.051921	12117.719993	28.647501
310.484532	12118.414004	28.652519
311.315199	12115.408072	28.657536
311.006994	12119.121489	28.662554
311.625814	12134.841438	28.667572
311.479751	12155.286691	28.672589
311.839705	12159.900793	28.677607
312.255314	12157.668193	28.682624
312.471770	12182.345774	28.687642
312.461664	12183.315039	28.692660
312.558778	12214.727049	28.697677
312.522717	12230.152473	28.702695
312.733025	12248.841483	28.707712
312.810520	12283.515685	28.712730
313.022480	12303.208284	28.717748
313.495323	12337.016404	28.722765
313.772284	12364.399367	28.727783
313.951289	12392.257217	28.732800
313.904047	12437.058311	28.737818
314.746420	12460.023400	28.742836
314.762899	12493.409692	28.747853
315.670086	12516.701326	28.752871
315.893549	12544.797885	28.757888
316.140150	12574.186001	28.762906
317.016453	12591.037632	28.767924
317.420827	12613.818838	28.772941
317.076149	12624.631366	28.777959
317.608763	12642.186247	28.782976
318.193031	12672.353652	28.787994
318.679244	12684.652905	28.793012
318.989367	12710.269126	28.798029
319.242147	12728.708949	28.803047
319.470785	12750.247815	28.808064
319.373364	12769.681929	28.813082
319.955591	12783.820109	28.818100
320.065650	12818.902923	28.823117
320.587758	12844.421105	28.828135
321.414504	12849.028775	28.833152
321.121400	12887.864697	28.838170
322.194305	12883.322876	28.843188
322.744989	12891.381905	28.848205
322.892422	12908.104384	28.853223
323.163546	12900.354873	28.858240
323.124289	12916.156539	28.863258
323.226858	12933.575160	28.868276
323.606486	12951.466242	28.873293
323.739038	12969.373174	28.878311
324.060835	12987.521317	28.883328
324.531743	13007.729621	28.888346
324.810948	13022.495127	28.893364
325.346367	13045.088125	28.898381
325.724340	13056.884020	28.903399
326.511071	13070.503103	28.908416
326.344577	13084.260061	28.913434
326.985582	13083.992870	28.918452
327.159378	13112.752662	28.923469
327.638228	13123.493326	28.928487
327.884317	13143.163940	28.933504
328.198175	13146.249472	28.938522
328.329765	13169.445537	28.943540
328.504712	13184.666614	28.948557
328.936728	13207.700937	28.953575
329.289830	13219.567271	28.958592
329.356997	13245.672257	28.963610
329.942809	13270.376809	28.968628
330.311783	13283.387823	28.973645
330.441957	13301.719440	28.978663
330.751777	13324.003600	28.983680
330.922260	13351.412219	28.988698
331.228284	13377.536046	28.993716
331.127640	13401.844230	28.998733
331.658185	13439.826015	29.003751
331.923755	13463.151531	29.008768
332.069257	13501.309313	29.013786
332.592527	13526.719636	29.018804
332.864512	13558.505479	29.023821
333.100263	13590.344682	29.028839
333.782196	13604.318879	29.033856
334.280090	13646.821678	29.038874
334.862791	13664.470209	29.043892
335.141884	13688.361146	29.048909
335.293086	13711.827366	29.053927
335.768296	13716.640253	29.058944
336.513119	13738.343682	29.063962
336.956017	13765.652585	29.068980
337.376504	13774.939301	29.073997
337.479225	13802.347327	29.079015
337.632486	13816.321274	29.084032
337.991570	13834.777788	29.089050
338.244733	13858.104355	29.094068
338.430259	13881.867705	29.099085
338.776897	13910.574976	29.104103
339.148015	13921.007837	29.109120
339.310412	13959.408162	29.114138
339.728462	13983.238624	29.119156
340.195287	14006.515726	29.124173
340.108827	14027.503443	29.129191
340.693085	14048.564161	29.134208
341.005364	14083.417527	29.139226
341.428499	14116.771109	29.144244
341.519482	14127.529590	29.149261
342.780674	14133.844779	29.154279
342.991405	14159.925802	29.159296
343.292431	14187.919326	29.164314
343.459689	14202.378266	29.169332
343.853760	14219.507131	29.174349
343.882554	14246.362392	29.179367
344.218519	14247.888938	29.184384
344.181896	14272.131043	29.189402
344.616965	14301.766771	29.194420
344.885709	14321.594221	29.199437
344.937646	14347.188137	29.204455
345.783711	14366.719585	29.209472
346.231989	14398.033338	29.214490
346.162221	14429.442663	29.219508
346.876661	14440.490217	29.224525
346.956535	14469.359410	29.229543
347.664029	14498.589329	29.234560
347.767688	14527.457825	29.239578
347.926497	14550.262047	29.244596
348.770927	14573.888580	29.249613
348.973654	14586.917222	29.254631
349.864637	14614.324901	29.259648
350.009444	14638.255295	29.264666
350.297985	14664.456585	29.269684
350.912991	14674.066117	29.274701
350.868852	14704.592272	29.279719
351.399313	14717.289189	29.284736
351.550466	14741.172974	29.289754
351.867281	14763.128540	29.294772
352.110682	14782.465875	29.299789
352.508763	14819.063869	29.304807
352.904891	14837.255313	29.309824
353.277296	14867.474590	29.314842
353.867133	14885.257227	29.319860
354.441368	14916.478550	29.324877
354.140842	14935.860713	29.329895
354.876076	14955.001498	29.334912
355.332976	14980.308480	29.339930
355.288799	15005.468628	29.344948
355.952951	15025.797066	29.349965
356.065092	15057.131667	29.354983
356.440780	15079.835979	29.360000
356.354241	15108.267415	29.365018
357.079234	15147.086148	29.370036
357.513547	15166.759455	29.375053
357.919306	15199.081053	29.380071
358.499680	15215.919958	29.385088
358.988389	15242.481373	29.390106
359.343464	15261.983552	29.395124
359.913834	15277.084154	29.400141
359.630700	15304.227802	29.405159
360.100747	15325.263433	29.410176
360.860845	15347.116201	29.415194
360.725896	15380.163151	29.420212
360.889844	15401.419948	29.425229
361.458488	15432.379970	29.430247
361.830689	15460.069109	29.435264
362.277418	15482.956043	29.440282
362.267043	15519.412246	29.445300
362.749503	15551.313578	29.450317
363.170216	15581.411087	29.455335
363.498606	15611.378981	29.460352
363.681907	15640.315011	29.465370
363.969183	15681.868258	29.470388
364.389898	15707.820716	29.475405
364.704795	15735.273957	29.480423
364.912889	15772.733119	29.485440
365.331512	15806.484930	29.490458
365.929435	15829.944599	29.495476
366.919462	15852.231122	29.500493
367.307251	15870.992520	29.505511
368.098433	15891.570458	29.510528
368.605831	15897.833461	29.515546
368.648720	15909.244178	29.520564
369.132210	15926.538086	29.525581
369.047145	15944.115595	29.530599
369.494694	15952.874193	29.535616
370.177850	15974.797323	29.540634
370.256091	16005.524650	29.545652
370.658620	16014.565016	29.550669
370.508303	16048.240026	29.555687
370.859068	16069.846515	29.560704
371.035106	16096.086115	29.565722
371.284557	16119.856274	29.570740
372.031363	16148.854062	29.575757
372.148858	16184.217104	29.580775
372.489821	16210.793593	29.585792
372.895822	16243.126661	29.590810
372.959083	16272.153093	29.595828
373.534519	16305.487403	29.600845
373.966172	16340.423457	29.605863
374.194883	16364.687617	29.610880
374.700890	16399.561006	29.615898
375.013474	16434.537528	29.620916
375.597677	16467.358437	29.625933
375.904328	16500.321664	29.630951
376.139277	16525.185568	29.635968
376.874926	16554.376648	29.640986
377.574361	16582.144147	29.646004
378.830348	16588.636148	29.651021
379.007291	16610.169764	29.656039
379.659210	16626.214844	29.661056
379.996919	16640.841496	29.666074
379.901122	16645.007696	29.671092
380.342591	16661.749791	29.676109
380.482609	16684.208589	29.681127
380.923514	16717.596029	29.686144
381.218571	16735.766960	29.691162
381.348050	16763.511219	29.696180
381.850013	16781.422427	29.701197
381.760149	16814.395399	29.706215
382.412015	16834.844766	29.711232
383.304716	16861.207709	29.716250
383.647412	16884.397602	29.721268
383.951089	16902.912487	29.726285
384.114081	16935.066599	29.731303
384.558204	16952.588804	29.736320
384.684634	16972.994789	29.741338
384.986045	17011.852029	29.746356
385.416614	17023.120307	29.751373
385.634668	17062.759161	29.756391
386.108891	17105.654732	29.761408
386.486336	17128.199222	29.766426
386.482761	17166.156980	29.771444
386.963280	17199.995940	29.776461
387.481099	17241.916775	29.781479
387.688439	17281.365623	29.786496
388.286872	17314.389196	29.791514
388.640725	17350.516235	29.796532
389.213224	17384.718609	29.801549
389.142695	17420.451279	29.806567
389.385605	17447.957157	29.811584
391.994287	17419.969810	29.816602
393.046542	17417.435315	29.821620
393.411406	17409.302421	29.826637
393.948019	17426.606422	29.831655
394.191473	17421.400422	29.836672
394.267631	17421.491844	29.841690
394.250449	17432.377643	29.846708
394.616308	17445.070917	29.851725
394.548671	17454.886907	29.856743
394.757507	17459.705751	29.861760
394.918662	17468.662483	29.866778
394.800830	17495.995067	29.871796
395.265056	17522.020394	29.876813
395.461119	17544.598733	29.881831
395.444798	17573.479880	29.886848
395.655333	17606.350934	29.891866
396.130795	17640.398135	29.896884
396.998586	17659.638288	29.901901
397.331236	17699.051554	29.906919
397.636534	17728.070285	29.911936
398.191909	17750.146268	29.916954
398.415057	17795.175569	29.921972
398.903434	17811.581582	29.926989
399.916125	17843.697207	29.932007
400.191991	17873.931726	29.937024
400.556718	17901.760196	29.942042
400.664927	17934.322588	29.947060
400.933283	17955.043551	29.952077
400.989657	17991.495687	29.957095
401.072728	18024.502239	29.962112
401.655935	18055.469497	29.967130
401.782633	18106.436541	29.972148
402.396720	18136.079388	29.977165
403.208595	18179.798125	29.982183
403.627428	18219.768964	29.987200
404.048945	18251.047195	29.992218
404.456638	18291.630122	29.997236
404.857718	18329.313661	30.002253
405.276532	18362.938242	30.007271
405.938180	18389.447625	30.012288
407.406057	18396.961366	30.017306
408.761794	18398.301592	30.022324
409.165825	18428.020838	30.027341
409.489881	18435.034115	30.032359
409.591513	18450.295889	30.037376
409.540376	18439.250591	30.042394
409.716122	18469.351487	30.047412
410.279327	18469.098757	30.052429
410.750033	18485.694392	30.057447
410.766750	18507.747352	30.062464
411.206091	18530.233024	30.067482
411.063059	18561.914590	30.072500
411.366493	18585.026682	30.077517
411.855872	18618.157672	30.082535
411.881775	18652.612670	30.087552
412.248335	18686.796761	30.092570
412.250413	18720.661540	30.097588
412.860112	18767.382269	30.102605
413.372961	18809.467111	30.107623
413.353025	18862.169693	30.112640
414.005360	18897.736595	30.117658
414.178282	18944.087382	30.122676
414.777802	18981.676379	30.127693
415.155344	19029.062258	30.132711
415.708284	19073.106965	30.137728
416.190411	19113.260188	30.142746
416.592688	19153.961198	30.147764
416.793197	19184.361954	30.152781
417.669999	19218.355184	30.157799
418.044956	19262.171408	30.162816
418.846240	19298.928326	30.167834
419.263198	19324.735736	30.172852
419.564730	19365.587997	30.177869
420.045281	19402.086268	30.182887
420.358761	19440.311844	30.187904
421.182779	19472.154542	30.192922
421.279475	19498.097393	30.197940
421.806144	19517.052687	30.202957
422.523235	19538.626503	30.207975
422.806465	19571.645434	30.212992
423.073439	19597.869156	30.218010
423.616066	19621.048580	30.223028
423.893875	19648.883369	30.228045
424.800859	19662.251503	30.233063
426.165043	19654.361444	30.238080
426.996858	19641.412446	30.243098
427.367423	19655.703655	30.248116
428.055227	19661.865618	30.253133
428.106659	19669.930525	30.258151
428.215456	19679.620773	30.263168
428.499965	19677.374291	30.268186
428.552127	19704.275508	30.273204
428.573529	19717.957890	30.278221
428.744402	19729.472943	30.283239
428.964655	19777.044723	30.288256
429.658500	19803.577815	30.293274
429.448079	19835.400682	30.298292
429.666856	19876.595858	30.303309
429.917448	19917.926165	30.308327
430.323569	19961.472607	30.313344
431.175787	20000.440830	30.318362
431.083090	20048.205670	30.323380
431.480866	20097.700663	30.328397
431.527227	20150.464078	30.333415
431.449302	20200.892888	30.338432
432.294133	20250.585251	30.343450
433.077414	20310.261497	30.348468
433.487493	20366.331201	30.353485
433.792713	20413.126020	30.358503
433.915499	20463.847061	30.363520
434.985230	20513.895425	30.368538
435.698062	20562.275246	30.373556
435.834179	20613.699272	30.378573
436.303352	20663.204567	30.383591
436.607054	20718.850083	30.388608
438.172509	20727.952141	30.393626
438.799014	20771.700575	30.398644
439.304534	20801.247943	30.403661
440.113762	20838.896151	30.408679
440.334143	20863.645971	30.413696
440.759398	20888.454823	30.418714
441.118341	20920.085844	30.423732
441.381806	20956.300342	30.428749
441.638231	20992.333195	30.433767
441.995721	21031.753345	30.438784
442.460345	21059.620935	30.443802
442.681165	21108.121885	30.448820
443.271822	21156.593083	30.453837
443.678297	21180.672332	30.458855
443.933795	21236.144669	30.463872
444.006309	21266.682398	30.468890
444.774197	21315.947645	30.473908
445.034486	21350.443353	30.478925
445.737903	21394.650486	30.483943
445.833772	21437.348833	30.488960
446.625762	21468.298778	30.493978
446.891238	21510.895036	30.498996
447.556621	21554.347357	30.504013
448.258119	21593.979726	30.509031
448.549962	21638.911768	30.514048
448.782482	21683.740258	30.519066
449.638614	21713.738700	30.524084
450.081587	21765.351779	30.529101
450.720849	21781.227356	30.534119
450.786016	21823.062999	30.539136
451.359604	21848.619650	30.544154
451.509462	21888.662832	30.549172
451.990136	21923.050577	30.554189
453.242954	21944.629971	30.559207
453.514079	21970.547661	30.564224
453.986323	22005.111992	30.569242
454.475253	22034.661126	30.574260
454.624898	22059.394490	30.579277
455.001136	22079.069863	30.584295
455.259814	22125.448285	30.589312
456.452116	22150.839566	30.594330
457.120848	22175.236182	30.599348
457.345063	22197.565410	30.604365
457.811305	22233.422578	30.609383
457.996076	22261.266103	30.614400
458.217203	22290.349288	30.619418
458.966060	22318.133909	30.624436
459.372062	22354.160592	30.629453
460.083711	22377.057160	30.634471
460.097937	22429.066713	30.639488
460.478238	22455.370672	30.644506
460.838544	22487.080089	30.649524
461.024271	22528.001830	30.654541
461.763054	22557.027881	30.659559
461.697570	22607.423960	30.664576
462.256999	22647.632703	30.669594
463.113643	22704.411796	30.674612
463.860394	22731.114175	30.679629
464.693742	22766.236624	30.684647
464.510428	22802.403132	30.689664
465.281363	22837.630704	30.694682
465.815114	22873.522166	30.699700
466.046821	22915.315498	30.704717
466.868803	22947.092592	30.709735
467.266388	22993.510237	30.714752
468.037221	23025.083098	30.719770
467.951216	23064.122780	30.724788
468.349376	23092.439973	30.729805
468.886818	23130.573647	30.734823
469.136629	23170.157004	30.739840
469.821816	23219.969783	30.744858
470.055866	23267.637404	30.749876
470.570670	23312.953146	30.754893
471.302965	23352.835245	30.759911
471.668116	23389.369203	30.764928
472.215724	23431.904509	30.769946
473.011270	23456.868514	30.774964
473.534444	23490.793509	30.779981
474.150578	23525.737574	30.784999
474.358800	23566.590272	30.790016
474.892594	23607.888873	30.795034
475.370624	23622.615021	30.800052
476.293588	23653.540912	30.805069
477.057298	23675.545950	30.810087
477.478210	23708.043918	30.815104
477.921275	23734.107631	30.820122
478.326966	23759.031174	30.825140
478.804243	23793.106318	30.830157
479.165185	23813.704012	30.835175
479.308181	23851.900082	30.840192
480.110113	23882.083262	30.845210
480.335504	23919.119376	30.850228
480.239317	23956.823980	30.855245
480.790996	23987.810566	30.860263
480.891746	24034.165230	30.865280
481.431654	24075.968572	30.870298
481.626049	24130.448118	30.875316
481.725794	24165.878225	30.880333
482.398299	24217.115283	30.885351
482.730184	24274.410971	30.890368
482.738633	24316.672174	30.895386
483.536837	24366.892164	30.900404
483.873967	24420.235588	30.905421
484.421921	24476.035790	30.910439
484.937898	24535.765020	30.915456
485.264800	24583.064496	30.920474
486.307072	24635.029892	30.925492
486.655248	24684.253199	30.930509
487.772451	24732.339650	30.935527
488.098569	24784.985850	30.940544
488.452403	24833.622001	30.945562
489.060411	24872.987385	30.950580
489.175059	24918.881647	30.955597
489.401529	24961.325859	30.960615
490.272924	25032.847549	30.965632
490.708369	25082.322448	30.970650
490.993071	25125.911784	30.975668
491.198208	25184.404881	30.980685
492.000693	25234.270295	30.985703
493.321758	25282.832248	30.990720
493.955134	25324.806057	30.995738
494.607305	25367.672617	31.000756
495.373222	25414.557678	31.005773
496.257332	25418.984374	31.010791
497.031853	25446.940175	31.015808
497.558485	25474.151808	31.020826
498.219400	25497.407966	31.025844
498.286024	25536.278114	31.030861
498.599819	25559.431142	31.035879
499.354801	25594.184480	31.040896
499.126815	25629.195759	31.045914
499.737748	25670.896576	31.050932
499.500543	25719.235965	31.055949
500.059772	25757.081702	31.060967
500.592706	25819.928930	31.065984
501.474970	25860.074282	31.071002
502.281285	25895.437931	31.076020
502.666676	25938.448003	31.081037
503.231490	25972.795252	31.086055
503.611159	26014.582623	31.091072
503.724834	26044.415521	31.096090
504.542125	26091.416916	31.101108
505.053869	26140.106243	31.106125
505.444156	26179.059723	31.111143
505.648564	26226.879289	31.116160
506.027773	26283.896247	31.121178
506.920355	26331.280079	31.126196
507.385891	26380.403589	31.131213
507.861272	26430.733707	31.136231
508.398194	26474.331888	31.141248
508.816608	26537.878932	31.146266
509.228952	26587.800450	31.151284
510.113505	26616.250887	31.156301
510.893161	26648.339991	31.161319
511.219889	26688.169469	31.166336
511.732985	26734.526023	31.171354
512.360620	26769.668795	31.176372
512.796163	26808.237655	31.181389
513.766974	26857.978887	31.186407
514.134489	26887.894108	31.191424
514.151087	26934.898290	31.196442
514.358024	26974.275160	31.201460
514.772960	27026.197413	31.206477
515.675171	27066.089913	31.211495
516.494091	27106.248694	31.216512
516.581997	27158.698818	31.221530
517.159737	27191.576379	31.226548
517.372040	27238.312299	31.231565
517.970695	27277.015995	31.236583
518.568610	27312.533880	31.241600
518.689518	27363.988640	31.246618
519.401018	27406.348860	31.251636
519.646381	27461.420371	31.256653
519.715730	27507.672882	31.261671
520.414995	27565.066772	31.266688
520.781936	27622.374087	31.271706
521.395200	27682.060218	31.276724
521.831258	27745.747565	31.281741
522.526620	27796.458371	31.286759
523.542655	27848.646040	31.291776
523.803099	27899.236942	31.296794
524.427806	27952.458366	31.301812
524.997296	28010.969927	31.306829
525.254336	28067.839544	31.311847
525.710068	28124.241013	31.316864
525.920754	28187.336480	31.321882
527.018620	28235.133092	31.326900
527.635419	28292.694505	31.331917
528.630233	28343.243613	31.336935
529.993225	28384.772462	31.341952
530.346128	28414.856788	31.346970
531.296380	28440.838679	31.351988
532.142742	28486.475784	31.357005
532.736131	28506.264444	31.362023
533.350559	28528.182208	31.367040
533.799689	28555.673412	31.372058
534.492787	28586.269387	31.377076
534.697028	28620.836358	31.382093
534.646934	28658.906359	31.387111
535.221258	28696.901144	31.392128
535.158006	28733.036489	31.397146
536.033685	28783.612973	31.402164
536.527600	28820.684422	31.407181
537.543720	28867.609868	31.412199
537.821348	28899.546756	31.417216
538.205136	28936.819716	31.422234
539.053414	28969.232982	31.427252
539.426500	29011.870999	31.432269
539.679550	29056.147462	31.437287
540.283852	29087.860088	31.442304
540.455835	29144.974491	31.447322
541.251700	29186.735097	31.452340
541.810783	29241.791692	31.457357
542.130687	29298.446666	31.462375
542.726947	29341.720408	31.467392
542.817381	29395.640696	31.472410
543.404045	29450.743846	31.477428
543.869593	29501.295873	31.482445
544.163615	29563.808292	31.487463
545.024786	29616.645343	31.492480
545.523765	29677.379476	31.497498
546.217104	29711.838991	31.502516
547.074300	29772.633857	31.507533
547.116317	29824.881934	31.512551
547.966416	29874.882167	31.517568
548.397173	29936.821096	31.522586
549.003984	29985.858774	31.527604
549.309848	30052.475569	31.532621
549.559736	30112.425972	31.537639
550.082656	30165.484909	31.542656
550.690932	30226.682354	31.547674
551.731225	30271.925947	31.552692
552.454511	30321.563603	31.557709
553.192783	30368.775851	31.562727
553.905802	30406.517850	31.567744
553.906256	30457.083611	31.572762
554.525486	30508.890817	31.577780
555.421648	30537.058654	31.582797
555.577355	30592.678667	31.587815
556.544553	30615.726782	31.592832
556.844926	30678.873132	31.597850
557.986232	30715.301574	31.602868
558.450088	30757.149459	31.607885
558.889852	30803.730945	31.612903
559.364141	30847.337861	31.617920
559.506729	30894.423272	31.622938
559.998024	30943.880354	31.627956
560.931804	30985.029186	31.632973
561.517177	31033.253014	31.637991
562.084280	31073.557417	31.643008
562.386261	31129.016006	31.648026
562.853145	31169.012287	31.653044
563.487782	31228.344137	31.658061
564.223122	31277.045404	31.663079
565.034160	31319.628928	31.668096
565.608432	31372.083492	31.673114
566.664364	31409.587704	31.678132
567.223037	31453.431371	31.683149
567.520344	31494.112835	31.688167
568.108220	31534.910215	31.693184
568.537406	31584.786435	31.698202
569.038333	31626.399897	31.703220
569.625032	31676.493175	31.708237
569.618562	31735.639751	31.713255
570.362139	31786.912605	31.718272
570.521318	31846.558977	31.723290
571.217189	31909.284353	31.728308
571.755130	31971.793218	31.733325
572.065591	32034.712406	31.738343
572.782402	32105.481081	31.743360
573.066944	32168.395581	31.748378
573.846476	32214.716120	31.753396
574.981107	32267.190731	31.758413
575.495150	32329.840509	31.763431
576.225444	32381.322393	31.768448
576.522751	32454.127927	31.773466
577.522066	32507.427192	31.778484
578.164377	32563.527958	31.783501
578.314680	32626.737740	31.788519
578.962347	32682.074377	31.793536
579.370992	32735.816354	31.798554
580.016076	32792.677846	31.803572
580.863717	32847.953396	31.808589
581.274830	32917.763170	31.813607
581.699797	32964.349652	31.818624
582.482204	33027.298124	31.823642
583.800526	33075.727679	31.828660
584.951123	33101.247770	31.833677
585.410670	33152.622231	31.838695
586.039769	33191.425450	31.843712
586.114467	33236.660287	31.848730
586.585037	33285.553049	31.853748
587.446881	33330.698442	31.858765
587.448390	33385.904744	31.863783
588.284585	33430.956828	31.868800
588.337191	33491.462646	31.873818
588.680320	33542.788141	31.878836
589.694563	33607.918554	31.883853
590.052483	33661.270989	31.888871
590.549662	33727.831989	31.893888
590.732419	33788.841037	31.898906
591.368722	33834.328099	31.903924
592.001345	33889.705705	31.908941
592.278655	33959.005315	31.913959
593.539087	33992.586962	31.918976
594.232901	34052.041506	31.923994
595.466995	34089.300924	31.929012
595.976639	34135.406212	31.934029
596.859366	34176.299561	31.939047
597.357863	34230.517107	31.944064
597.876839	34274.311222	31.949082
597.863695	34321.857602	31.954100
598.401627	34369.511417	31.959117
598.982979	34424.362719	31.964135
599.582576	34483.035940	31.969152
599.970134	34545.815502	31.974170
600.142755	34606.870048	31.979188
601.003352	34662.164858	31.984205
601.426062	34730.938389	31.989223
602.100660	34795.605672	31.994240
602.496889	34861.228287	31.999258
603.367799	34926.469363	32.004276
604.274162	34983.357576	32.009293
604.791203	35051.359270	32.014311
605.497971	35111.705138	32.019328
606.138522	35174.643714	32.024346
606.854298	35235.086334	32.029364
607.710914	35282.733845	32.034381
608.239295	35334.049498	32.039399
608.774518	35399.278604	32.044416
609.290595	35464.293367	32.049434
610.131207	35527.105282	32.054452
610.944182	35591.711430	32.059469
611.158686	35647.624668	32.064487
611.669214	35698.859116	32.069504
612.658574	35750.172004	32.074522
613.503196	35812.526633	32.079540
614.057148	35869.211067	32.084557
614.356506	35919.386074	32.089575
614.999193	35992.240188	32.094592
615.261053	36051.798336	32.099610
615.673969	36114.711722	32.104628
616.785338	36176.376332	32.109645
617.372792	36243.651261	32.114663
618.024926	36309.239823	32.119680
618.455619	36370.465803	32.124698
618.946480	36440.834692	32.129716
619.824954	36483.734983	32.134733
620.023092	36562.548200	32.139751
620.676328	36630.798359	32.144768
621.079080	36705.620433	32.149786
621.851175	36764.051525	32.154804
622.811769	36846.589895	32.159821
623.015682	36914.903106	32.164839
624.213661	36973.680779	32.169856
625.021853	37041.654264	32.174874
626.050862	37100.106909	32.179892
626.530609	37159.080188	32.184909
626.890741	37224.868899	32.189927
627.456022	37274.365953	32.194944
627.728796	37347.132292	32.199962
628.426378	37411.972430	32.204980
628.770885	37477.322772	32.209997
629.127259	37551.849880	32.215015
629.673889	37630.098555	32.220032
630.252556	37697.825386	32.225050
630.466733	37772.168691	32.230068
631.650774	37839.852352	32.235085
632.440509	37918.598483	32.240103
633.176087	37981.171236	32.245120
633.958815	38051.857744	32.250138
634.188540	38109.041762	32.255156
635.385948	38170.092859	32.260173
636.227634	38226.222406	32.265191
637.612155	38266.400987	32.270208
639.409807	38275.514994	32.275226
640.205282	38317.669562	32.280244
641.047019	38345.805140	32.285261
641.251376	38374.191783	32.290279
642.054432	38399.123769	32.295296
642.793794	38428.873633	32.300314
642.909276	38469.080295	32.305332
643.101904	38499.268259	32.310349
643.306971	38560.608534	32.315367
643.846063	38600.195926	32.320384
644.693188	38651.029317	32.325402
645.055499	38692.975748	32.330420
645.700171	38747.526648	32.335437
645.977032	38809.840669	32.340455
646.500386	38865.460027	32.345472
647.334589	38927.107424	32.350490
647.698129	38995.477700	32.355508
648.139356	39058.125123	32.360525
648.563106	39126.170234	32.365543
648.902083	39209.397040	32.370560
649.222817	39274.098046	32.375578
649.992630	39355.849302	32.380596
651.423491	39424.403824	32.385613
652.312725	39486.261778	32.390631
652.712428	39556.411639	32.395648
653.022974	39627.457277	32.400666
653.624564	39704.200000	32.405684
654.959189	39756.464416	32.410701
655.685240	39830.118714	32.415719
656.417539	39886.962847	32.420736
657.386295	39956.663053	32.425754
657.993746	40027.108520	32.430772
658.682013	40084.863400	32.435789
659.105539	40156.327956	32.440807
659.248520	40215.439633	32.445824
659.752018	40281.243964	32.450842
660.399370	40373.045976	32.455860
661.007482	40440.112003	32.460877
661.480210	40523.470927	32.465895
661.962941	40606.692825	32.470912
663.263114	40673.720566	32.475930
664.019270	40752.787532	32.480948
664.650203	40823.961382	32.485965
665.084428	40906.722316	32.490983
665.628436	40981.794160	32.496000
666.085286	41052.167533	32.501018
666.358122	41142.848564	32.506036
667.154357	41223.363072	32.511053
667.749706	41316.520108	32.516071
668.071940	41409.050524	32.521088
669.418211	41485.077211	32.526106
669.595680	41595.961980	32.531124
670.300327	41672.597926	32.536141
670.923922	41765.635723	32.541159
671.311772	41856.698939	32.546176
671.977684	41944.104771	32.551194
672.770556	42047.815123	32.556212
673.469745	42142.648104	32.561229
673.969462	42233.909279	32.566247
674.672628	42328.158484	32.571264
675.864230	42415.731830	32.576282
676.305485	42498.119850	32.581300
677.049649	42574.045759	32.586317
678.013941	42652.625340	32.591335
679.099937	42726.727107	32.596352
680.559710	42787.352200	32.601370
681.555378	42854.855158	32.606388
682.669246	42900.983347	32.611405
683.608586	42936.570259	32.616423
684.050085	42988.423827	32.621440
684.876315	43040.889315	32.626458
685.515198	43094.238510	32.631476
686.253882	43132.836393	32.636493
686.906253	43185.413241	32.641511
687.832187	43225.849329	32.646528
688.573875	43266.783369	32.651546
689.024317	43320.767538	32.656564
689.446964	43377.879040	32.661581
689.926482	43436.389431	32.666599
690.186947	43500.827918	32.671616
690.249016	43560.986661	32.676634
690.990338	43643.718281	32.681652
692.059597	43703.685011	32.686669
692.700017	43781.117020	32.691687
693.510348	43857.261349	32.696704
694.101320	43924.453330	32.701722
694.118653	43998.867031	32.706740
694.691576	44076.311467	32.711757
695.118144	44164.260011	32.716775
695.716340	44260.465597	32.721792
696.127502	44344.597041	32.726810
696.645243	44449.253674	32.731828
697.595329	44539.156789	32.736845
699.212768	44615.075480	32.741863
699.875688	44695.696609	32.746880
701.018592	44769.617064	32.751898
701.721695	44861.119387	32.756916
702.347961	44935.290457	32.761933
703.051434	45011.858226	32.766951
703.680608	45088.182878	32.771968
704.554325	45164.899831	32.776986
704.711055	45254.556012	32.782004
705.256752	45333.042687	32.787021
706.009577	45423.709036	32.792039
706.568337	45519.646583	32.797056
707.512001	45591.247738	32.802074
708.317312	45670.324251	32.807092
709.262846	45753.811215	32.812109
710.098673	45836.846263	32.817127
710.522286	45937.172318	32.822144
711.251472	46014.952458	32.827162
711.978161	46102.433937	32.832180
712.906186	46180.680674	32.837197
713.655747	46267.720192	32.842215
714.281490	46345.796751	32.847232
715.865982	46408.288606	32.852250
716.548381	46479.964926	32.857268
718.129417	46535.741112	32.862285
719.146159	46603.323542	32.867303
719.428295	46658.024169	32.872320
719.911117	46718.865237	32.877338
720.182251	46791.037320	32.882356
720.716736	46862.307015	32.887373
721.065560	46939.670945	32.892391
721.552903	47012.850080	32.897408
722.387149	47094.068798	32.902426
722.950845	47171.754846	32.907444
723.824720	47250.157098	32.912461
724.925820	47313.205885	32.917479
725.317899	47393.772960	32.922496
726.035403	47458.354362	32.927514
726.584814	47534.051580	32.932532
727.802852	47596.721884	32.937549
728.985159	47656.483487	32.942567
729.463648	47718.503253	32.947584
730.036384	47778.698026	32.952602
730.894555	47846.431212	32.957620
731.255747	47919.000009	32.962637
731.755329	47989.828121	32.967655
731.840258	48069.893224	32.972672
732.354946	48143.091112	32.977690
732.971692	48243.387805	32.982708
733.641661	48335.452443	32.987725
734.499281	48434.740610	32.992743
735.121173	48516.547003	32.997760
736.122503	48600.138282	33.002778
736.768774	48692.167514	33.007796
737.480085	48790.989143	33.012813
738.286152	48886.103602	33.017831
739.174031	48965.480150	33.022848
739.769725	49062.073714	33.027866
740.269284	49158.876376	33.032884
741.237337	49248.663033	33.037901
742.203327	49350.215067	33.042919
742.857388	49449.823373	33.047936
743.404848	49525.854100	33.052954
744.488607	49624.820325	33.057972
744.997539	49715.917132	33.062989
745.970169	49815.278628	33.068007
746.325619	49920.582936	33.073024
746.721017	50014.274080	33.078042
747.801508	50127.339356	33.083060
748.667935	50223.476896	33.088077
749.516358	50326.121145	33.093095
749.815759	50437.716570	33.098112
750.938192	50520.515961	33.103130
752.042763	50622.718138	33.108148
752.628898	50719.808008	33.113165
753.873431	50816.656412	33.118183
754.570830	50908.548777	33.123200
755.041609	51005.874012	33.128218
755.787642	51102.895040	33.133236
756.458705	51199.695264	33.138253
757.088697	51301.019593	33.143271
757.945405	51404.612611	33.148288
758.601964	51499.104624	33.153306
759.550532	51598.450854	33.158324
760.070101	51703.086928	33.163341
761.069597	51796.102057	33.168359
762.081891	51905.224888	33.173376
763.024870	52005.717578	33.178394
764.145981	52072.281691	33.183412
765.880905	52142.452504	33.188429
768.236124	52180.699348	33.193447
769.359651	52234.704441	33.198464
770.196064	52279.944390	33.203482
771.382651	52325.713849	33.208500
771.629668	52366.155741	33.213517
772.308305	52411.618031	33.218535
772.514501	52454.600229	33.223552
773.257849	52509.136695	33.228570
774.035167	52566.725404	33.233588
773.937102	52627.542601	33.238605
774.395793	52703.632125	33.243623
774.774728	52773.783921	33.248640
775.281873	52851.603342	33.253658
775.993975	52932.080408	33.258676
776.496217	53019.251566	33.263693
777.316923	53080.833736	33.268711
777.808182	53166.427926	33.273728
778.636831	53236.449870	33.278746
779.088468	53307.261201	33.283764
779.592695	53404.712906	33.288781
780.251845	53487.109047	33.293799
780.820655	53581.682576	33.298816
781.675382	53662.101059	33.303834
782.390344	53778.580979	33.308852
782.719950	53872.184731	33.313869
783.422735	53976.265531	33.318887
784.067153	54081.329559	33.323904
784.627516	54182.168626	33.328922
785.307028	54297.703464	33.333940
786.262083	54420.888829	33.338957
787.360540	54527.945930	33.343975
788.147196	54642.965865	33.348992
788.976439	54751.667395	33.354010
789.993670	54859.188378	33.359028
791.434920	54951.039460	33.364045
792.946041	55032.340256	33.369063
793.817367	55127.205868	33.374080
794.932691	55205.590772	33.379098
795.672174	55296.688002	33.384116
796.347332	55370.767906	33.389133
797.325148	55465.010885	33.394151
797.891184	55555.253498	33.399168
798.657034	55636.484614	33.404186
799.510746	55716.033360	33.409204
800.145098	55814.391575	33.414221
801.151991	55896.114512	33.419239
801.850246	55981.926676	33.424256
802.518404	56075.130818	33.429274
803.393917	56165.173186	33.434292
803.874980	56267.950639	33.439309
804.869706	56353.595140	33.444327
806.158874	56453.332752	33.449344
806.611531	56535.839075	33.454362
807.462943	56632.212770	33.459380
808.111844	56725.688551	33.464397
808.731906	56821.766659	33.469415
809.114089	56925.353788	33.474432
809.870614	57035.672296	33.479450
811.131194	57123.620349	33.484468
812.747822	57211.819327	33.489485
813.967279	57294.624891	33.494503
814.777148	57383.963284	33.499520
815.393784	57469.763808	33.504538
815.879525	57556.079326	33.509556
816.482007	57648.138987	33.514573
817.414003	57748.195132	33.519591
817.933072	57844.952125	33.524608
818.592412	57938.671980	33.529626
819.597391	58035.633611	33.534644
820.065285	58142.454645	33.539661
820.767287	58237.116722	33.544679
821.077070	58350.341409	33.549696
821.629835	58455.715501	33.554714
822.432334	58568.758522	33.559732
823.232634	58686.738126	33.564749
823.992945	58801.186079	33.569767
824.996170	58923.569752	33.574784
825.915347	59039.610519	33.579802
826.771924	59145.279053	33.584820
827.312515	59271.849441	33.589837
828.330406	59375.084577	33.594855
829.550595	59474.083987	33.599872
830.517855	59576.968330	33.604890
831.962360	59680.772525	33.609908
832.167312	59771.511183	33.614925
833.256924	59869.763176	33.619943
834.094883	59973.315630	33.624960
834.750503	60067.185035	33.629978
835.737236	60156.449497	33.634996
836.045527	60267.511081	33.640013
837.014569	60366.961029	33.645031
837.999837	60463.425672	33.650048
838.386668	60574.488538	33.655066
839.436868	60681.024092	33.660084
839.878224	60800.484997	33.665101
840.813434	60889.015443	33.670119
841.571816	61002.686124	33.675136
842.422254	61119.710894	33.680154
843.531141	61216.860148	33.685172
844.865569	61331.208135	33.690189
846.036110	61433.334979	33.695207
846.850082	61540.072245	33.700224
847.863933	61630.274100	33.705242
848.614295	61734.077592	33.710260
849.645160	61833.707736	33.715277
850.228967	61929.323152	33.720295
851.726257	62036.922967	33.725312
852.599740	62137.674179	33.730330
853.401959	62226.763435	33.735348
854.067476	62325.280966	33.740365
854.685156	62424.464265	33.745383
855.416677	62526.795850	33.750400
855.792671	62642.037128	33.755418
856.740016	62748.480439	33.760436
857.418400	62874.392958	33.765453
857.877191	62978.883228	33.770471
858.640068	63109.549121	33.775488
859.509202	63229.269235	33.780506
860.566408	63351.645260	33.785524
861.240158	63477.568554	33.790541
862.032943	63598.460235	33.795559
862.970738	63728.070675	33.800576
863.507736	63844.941765	33.805594
864.285753	63981.988722	33.810612
865.128813	64112.470656	33.815629
865.859790	64242.422063	33.820647
867.266868	64375.283666	33.825664
867.859583	64522.137721	33.830682
868.876940	64644.034938	33.835700
869.718987	64787.770963	33.840717
870.410860	64927.095217	33.845735
871.325355	65047.298746	33.850752
872.498504	65185.299511	33.855770
873.792924	65294.422914	33.860788
875.604760	65418.512843	33.865805
876.725231	65523.114734	33.870823
878.209740	65622.637297	33.875840
879.267774	65718.204173	33.880858
880.814046	65803.373341	33.885876
881.839176	65879.709313	33.890893
882.584702	65964.063768	33.895911
883.656711	66045.860932	33.900928
885.094517	66109.694215	33.905946
886.631027	66175.983164	33.910964
887.718286	66223.513977	33.915981
889.117145	66277.618536	33.920999
890.139633	66331.159831	33.926016
890.736463	66389.367954	33.931034
891.018305	66435.427148	33.936052
891.318222	66504.337356	33.941069
891.970897	66567.695436	33.946087
892.545531	66621.627901	33.951104
892.686611	66697.778516	33.956122
893.548241	66776.850730	33.961140
893.902534	66856.816666	33.966157
894.363385	66959.164438	33.971175
894.911400	67040.002982	33.976192
895.433012	67146.450967	33.981210
896.134327	67254.374348	33.986228
896.275795	67364.022331	33.991245
897.262762	67478.815975	33.996263
898.366300	67592.832222	34.001280
899.165882	67716.206005	34.006298
899.787786	67832.478363	34.011316
900.582767	67964.756259	34.016333
901.186396	68094.487181	34.021351
902.003381	68228.476458	34.026368
902.718965	68370.671085	34.031386
903.660037	68497.465399	34.036404
904.829739	68642.349447	34.041421
905.694720	68785.091094	34.046439
906.913269	68919.511261	34.051456
907.371602	69049.740017	34.056474
908.241933	69201.360689	34.061492
909.444778	69353.685996	34.066509
910.138467	69484.788840	34.071527
911.416577	69617.825151	34.076544
912.274363	69767.529772	34.081562
913.096673	69901.067130	34.086580
913.886603	70058.872152	34.091597
915.227049	70183.435107	34.096615
916.794478	70313.417959	34.101632
918.788854	70413.719484	34.106650
920.247732	70527.085488	34.111668
920.835398	70643.846802	34.116685
921.664346	70752.196744	34.121703
922.788409	70872.031900	34.126720
923.271969	70988.123127	34.131738
923.959991	71112.711235	34.136756
924.756979	71240.228675	34.141773
925.395296	71368.127314	34.146791
926.116535	71506.573121	34.151808
926.414000	71645.083820	34.156826
927.408206	71790.498909	34.161844
928.040282	71929.632522	34.166861
928.902282	72072.782315	34.171879
930.069754	72221.668516	34.176896
930.696964	72364.992005	34.181914
932.515685	72489.583805	34.186932
933.777286	72625.999396	34.191949
934.838471	72760.425482	34.196967
936.027684	72882.360501	34.201984
936.890613	73010.731164	34.207002
938.260179	73127.970600	34.212020
939.420084	73258.184297	34.217037
940.193871	73377.452760	34.222055
941.092294	73500.413402	34.227072
941.801370	73626.359503	34.232090
942.653381	73754.679449	34.237108
943.947166	73879.429585	34.242125
944.560929	74002.250572	34.247143
945.568979	74120.794888	34.252160
946.702257	74262.630271	34.257178
947.222615	74381.990548	34.262196
948.137179	74517.691370	34.267213
948.897423	74641.705909	34.272231
950.422598	74766.612440	34.277248
951.455804	74892.075658	34.282266
952.107031	75014.681074	34.287284
952.928175	75130.320989	34.292301
954.014175	75252.804988	34.297319
954.759175	75360.268466	34.302336
956.880678	75452.116287	34.307354
957.654767	75553.940666	34.312372
958.668774	75661.670884	34.317389
959.273843	75771.031688	34.322407
961.109271	75846.648881	34.327424
961.757323	75954.921939	34.332442
962.648749	76052.187983	34.337460
963.651382	76163.116549	34.342477
964.384553	76265.526561	34.347495
965.280516	76372.748554	34.352512
966.164053	76476.715808	34.357530
966.798231	76597.081188	34.362548
967.517058	76713.726746	34.367565
968.163669	76844.875469	34.372583
968.969724	76961.741881	34.377600
969.796095	77101.458010	34.382618
970.836943	77234.112228	34.387636
971.676770	77360.178167	34.392653
972.292379	77507.756027	34.397671
973.393068	77641.009959	34.402688
974.107834	77784.986797	34.407706
975.127837	77924.619030	34.412724
975.724179	78078.522842	34.417741
976.490073	78239.015938	34.422759
977.768547	78380.999131	34.427776
978.418415	78538.818994	34.432794
979.679783	78692.819090	34.437812
981.109776	78839.625398	34.442829
982.233950	78990.702593	34.447847
983.525679	79128.684216	34.452864
984.970243	79271.398239	34.457882
985.616094	79398.216324	34.462900
986.550767	79555.199027	34.467917
987.634523	79702.422668	34.472935
988.691458	79835.867704	34.477952
989.592711	79992.928583	34.482970
990.162300	80138.633612	34.487988
991.108689	80285.434707	34.493005
991.681131	80447.158606	34.498023
992.566155	80600.342221	34.503040
993.540117	80769.105951	34.508058
994.174850	80930.601546	34.513076
995.425412	81099.416725	34.518093
996.592568	81274.870575	34.523111
998.303152	81407.431949	34.528128
999.117932	81563.524822	34.533146
999.976056	81722.793734	34.538164
1001.283798	81887.018649	34.543181
1001.971223	82035.974386	34.548199
1003.135423	82194.531521	34.553216
1003.842527	82359.473165	34.558234
1004.818784	82525.997269	34.563252
1006.816848	82658.771274	34.568269
1008.194857	82800.677087	34.573287
1009.920084	82929.341315	34.578304
1010.741467	83065.121979	34.583322
1011.779981	83196.147641	34.588340
1012.756381	83340.439028	34.593357
1013.205623	83476.340808	34.598375
1014.706741	83612.094158	34.603392
1015.101507	83756.092389	34.608410
1016.293953	83892.664167	34.613428
1017.195063	84036.434608	34.618445
1018.043894	84185.130731	34.623463
1019.291028	84317.494787	34.628480
1020.110720	84455.599623	34.633498
1020.705414	84590.199407	34.638516
1022.046754	84728.453417	34.643533
1022.340312	84872.595596	34.648551
1022.938500	85009.924269	34.653568
1023.944160	85178.848007	34.658586
1024.547289	85327.914909	34.663604
1025.558377	85479.667491	34.668621
1026.333758	85659.503392	34.673639
1026.948815	85819.176253	34.678656
1028.269473	85982.289200	34.683674
1029.620564	86140.620916	34.688692
1031.038664	86298.645187	34.693709
1031.846266	86469.420819	34.698727
1033.309278	86632.609593	34.703744
1034.594530	86792.924558	34.708762
1035.398844	86941.171053	34.713780
1037.066751	87097.900028	34.718797
1039.376048	87227.345418	34.723815
1041.493690	87340.718814	34.728832
1042.733660	87463.413882	34.733850
1043.189174	87583.879415	34.738868
1044.222614	87712.526693	34.743885
1044.978322	87838.411107	34.748903
1045.758557	87978.226526	34.753920
1046.461040	88129.838608	34.758938
1047.408876	88271.317554	34.763956
1047.748880	88416.764716	34.768973
1048.691615	88564.384597	34.773991
1049.832493	88725.685873	34.779008
1050.774295	88873.459707	34.784026
1051.098965	89049.200580	34.789044
1052.231514	89206.817068	34.794061
1053.071801	89387.189535	34.799079
1053.871719	89564.994367	34.804096
1054.758417	89731.597270	34.809114
1055.766304	89921.508378	34.814132
1056.751274	90100.507901	34.819149
1057.594796	90297.803134	34.824167
1058.504654	90481.241709	34.829184
1059.853400	90673.013488	34.834202
1060.843906	90860.485668	34.839220
1061.907817	91041.814443	34.844237
1063.003260	91236.721231	34.849255
1064.002405	91435.803711	34.854272
1065.027651	91625.301342	34.859290
1065.766459	91825.170716	34.864308
1067.415609	92007.150135	34.869325
1069.822578	92180.220290	34.874343
1071.514057	92338.492419	34.879360
1073.077329	92491.793068	34.884378
1074.227563	92654.264744	34.889396
1075.427652	92803.361665	34.894413
1077.061563	92944.836577	34.899431
1078.319679	93089.178590	34.904448
1079.921092	93226.919849	34.909466
1080.819682	93354.765249	34.914484
1082.387541	93480.595096	34.919501
1083.211248	93607.871929	34.924519
1084.150978	93739.408971	34.929536
1084.936568	93879.764129	34.934554
1085.542493	94015.067187	34.939572
1086.520260	94159.316444	34.944589
1087.361185	94306.994644	34.949607
1088.907617	94433.674795	34.954624
1090.343599	94568.336804	34.959642
1091.420766	94705.078296	34.964660
1092.428071	94842.756298	34.969677
1093.141492	94979.110238	34.974695
1093.778683	95113.388698	34.979712
1094.922907	95241.317099	34.984730
1096.227523	95365.250644	34.989748
1097.984499	95471.183121	34.994765
1099.286276	95592.567276	34.999783
1100.418050	95706.580360	35.004800
1101.431132	95818.296838	35.009818
1102.220064	95948.281825	35.014836
1103.100882	96070.896578	35.019853
1103.964655	96210.055608	35.024871
1104.509083	96347.983355	35.029888
1105.664074	96490.798836	35.034906
1105.977548	96649.928721	35.039924
1107.004374	96807.523270	35.044941
1107.725766	96972.601383	35.049959
1108.818212	97127.395353	35.054976
1109.791245	97305.006179	35.059994
1110.607754	97470.818793	35.065012
1111.571174	97641.223119	35.070029
1112.285467	97829.110791	35.075047
1112.970121	98011.123592	35.080064
1114.783111	98197.977103	35.085082
1115.482537	98388.549308	35.090100
1117.103018	98574.253693	35.095117
1118.262562	98754.623033	35.100135
1119.204976	98948.121986	35.105152
1120.782373	99128.671576	35.110170
1122.057993	99330.202791	35.115188
1123.227077	99494.495084	35.120205
1124.302540	99690.737962	35.125223
1125.922460	99859.332603	35.130240
1127.109829	100035.382270	35.135258
1128.347128	100219.592140	35.140276
1129.644447	100384.020850	35.145293
1130.878337	100560.610910	35.150311
1132.057734	100728.929829	35.155328
1133.258133	100912.872238	35.160346
1134.337023	101081.444407	35.165364
1135.200031	101265.147736	35.170381
1136.041799	101439.700520	35.175399
1136.749173	101637.462979	35.180416
1137.933559	101818.647631	35.185434
1138.561846	102023.447929	35.190452
1140.012158	102216.754388	35.195469
1141.341615	102414.527237	35.200487
1142.421182	102613.894345	35.205504
1143.624936	102798.812086	35.210522
1145.399104	102976.785405	35.215540
1147.529810	103145.633461	35.220557
1148.729121	103316.834324	35.225575
1150.028858	103482.035894	35.230592
1151.803303	103632.456724	35.235610
1152.857896	103805.679404	35.240628
1153.919751	103973.038467	35.245645
1154.814484	104131.130688	35.250663
1155.639371	104302.913037	35.255680
1156.990200	104459.221878	35.260698
1157.819126	104618.974344	35.265716
1159.085773	104802.540738	35.270733
1160.586488	104972.986885	35.275751
1161.662301	105138.995941	35.280768
1162.614411	105297.085660	35.285786
1163.592873	105469.268093	35.290804
1164.587966	105656.646988	35.295821
1165.314985	105836.890526	35.300839
1166.222318	106015.104268	35.305856
1166.899774	106196.574338	35.310874
1167.973925	106379.436366	35.315892
1169.145576	106545.362351	35.320909
1170.887553	106708.294344	35.325927
1171.789205	106891.644469	35.330944
1173.045109	107061.701372	35.335962
1173.864400	107246.131519	35.340980
1175.040866	107419.256344	35.345997
1176.535129	107596.357363	35.351015
1177.230775	107782.559625	35.356032
1178.464798	107965.646653	35.361050
1179.529608	108157.984044	35.366068
1180.675642	108355.008557	35.371085
1181.797382	108539.650749	35.376103
1182.660873	108733.482286	35.381120
1184.638130	108916.832491	35.386138
1185.891417	109114.022089	35.391156
1186.843530	109307.374372	35.396173
1188.211585	109494.274919	35.401191
1189.301174	109706.480927	35.406208
1190.402968	109893.555060	35.411226
1191.500708	110092.474959	35.416244
1192.432732	110282.822725	35.421261
1193.620519	110491.117039	35.426279
1195.323941	110684.924513	35.431296
1197.366279	110870.582586	35.436314
1198.722930	111058.078456	35.441332
1200.046266	111248.621385	35.446349
1201.078783	111430.979809	35.451367
1202.093438	111634.801801	35.456384
1203.038638	111822.282461	35.461402
1203.876393	112030.139799	35.466420
1204.888447	112232.003083	35.471437
1206.081521	112432.203609	35.476455
1206.846114	112643.776823	35.481472
1207.992725	112856.529791	35.486490
1208.898084	113081.270846	35.491508
1209.673056	113311.850255	35.496525
1210.892447	113541.331684	35.501543
1212.037165	113768.065574	35.506560
1214.077802	113987.748109	35.511578
1216.245020	114168.542723	35.516596
1218.349001	114356.861789	35.521613
1219.710821	114571.049077	35.526631
1221.240261	114758.135868	35.531648
1222.608768	114945.960084	35.536666
1224.211295	115136.103259	35.541684
1225.530683	115317.185266	35.546701
1226.270975	115502.494792	35.551719
1227.032810	115687.877976	35.556736
1228.357880	115874.017826	35.561754
1229.225322	116065.505480	35.566772
1230.102251	116271.487310	35.571789
1231.252417	116471.039591	35.576807
1231.918813	116691.401906	35.581824
1233.291855	116889.741824	35.586842
1234.645702	117103.797538	35.591860
1235.608709	117320.263715	35.596877
1236.801553	117537.871764	35.601895
1237.500624	117764.166730	35.606912
1238.298092	117979.030815	35.611930
1239.325994	118205.680173	35.616948
1240.261683	118450.922209	35.621965
1241.807071	118678.870580	35.626983
1242.890340	118926.613708	35.632000
1244.374461	119164.054086	35.637018
1245.616814	119412.991420	35.642036
1246.953099	119648.382170	35.647053
1248.089678	119873.860763	35.652071
1249.392096	120103.115091	35.657088
1250.344854	120311.216683	35.662106
1252.137223	120537.529333	35.667124
1253.861933	120746.684462	35.672141
1255.621420	120954.010541	35.677159
1256.996557	121149.996923	35.682176
1258.894149	121333.580575	35.687194
1260.439118	121528.945717	35.692212
1261.127261	121733.020783	35.697229
1262.975773	121926.741491	35.702247
1264.066972	122119.980792	35.707264
1265.363290	122315.557109	35.712282
1266.443985	122519.445752	35.717300
1267.470781	122724.510627	35.722317
1268.869459	122920.517491	35.727335
1269.699884	123132.232979	35.732352
1270.768915	123349.435842	35.737370
1271.789881	123575.810939	35.742388
1273.061996	123774.163572	35.747405
1275.042572	123980.346185	35.752423
1276.212866	124200.947538	35.757440
1277.551729	124410.648679	35.762458
1278.556718	124624.259424	35.767476
1279.676880	124857.433419	35.772493
1281.130991	125086.624948	35.777511
1281.686321	125324.255995	35.782528
1282.504315	125541.693706	35.787546
1284.108890	125784.730874	35.792564
1285.483084	126018.720806	35.797581
1286.405680	126255.892624	35.802599
1287.930636	126494.930903	35.807616
1289.181170	126729.567821	35.812634
1291.201955	126964.649138	35.817652
1293.320329	127186.078138	35.822669
1295.113285	127401.542198	35.827687
1296.894917	127606.527558	35.832704
1298.243149	127814.032416	35.837722
1300.091906	128020.023377	35.842740
1300.543927	128229.771027	35.847757
1301.962593	128442.807420	35.852775
1303.154067	128668.545531	35.857792
1303.985712	128880.972461	35.862810
1305.174927	129098.931399	35.867828
1305.631965	129332.946418	35.872845
1306.643637	129553.498419	35.877863
1307.728215	129798.820892	35.882880
1309.295430	130044.990568	35.887898
1310.292871	130291.155254	35.892916
1311.747809	130532.796703	35.897933
1313.141544	130771.826195	35.902951
1314.325260	131018.447336	35.907968
1315.741087	131284.198472	35.912986
1317.050895	131520.433374	35.918004
1318.031455	131779.187391	35.923021
1319.326352	132028.181090	35.928039
1320.346528	132288.618645	35.933056
1321.447563	132543.340337	35.938074
1322.874353	132798.846698	35.943092
1324.287534	133065.690591	35.948109
1325.990478	133303.166473	35.953127
1328.019345	133556.284425	35.958144
1330.140972	133788.496780	35.963162
1331.700259	134016.886746	35.968180
1332.944083	134253.609023	35.973197
1334.306448	134484.570422	35.978215
1335.886789	134716.663650	35.983232
1337.410280	134938.575046	35.988250
1338.919455	135154.366929	35.993268
1339.806305	135372.203156	35.998285
1340.953771	135580.070738	36.003303
1341.872750	135799.945622	36.008320
1343.382961	136012.953785	36.013338
1344.873585	136222.771654	36.018356
1346.501107	136435.053101	36.023373
1348.264971	136626.419302	36.028391
1350.018951	136829.503148	36.033408
1351.368001	137025.606117	36.038426
1352.748143	137227.727426	36.043444
1353.731046	137444.889378	36.048461
1354.767429	137653.637837	36.053479
1355.614247	137873.956796	36.058496
1356.537451	138094.797048	36.063514
1358.114568	138324.114012	36.068532
1358.833371	138554.462412	36.073549
1360.063474	138793.400170	36.078567
1360.883157	139039.558799	36.083584
1361.609558	139314.339404	36.088602
1363.049087	139569.363421	36.093620
1363.968223	139829.420686	36.098637
1365.705957	140094.872528	36.103655
1366.654697	140364.261206	36.108672
1368.025673	140636.498355	36.113690
1369.936933	140914.151182	36.118708
1371.426472	141201.284814	36.123725
1372.728624	141464.258084	36.128743
1375.415490	141702.759014	36.133760
1377.077260	141945.425895	36.138778
1379.541468	142181.988908	36.143796
1381.599802	142423.502846	36.148813
1383.230344	142638.320588	36.153831
1384.266503	142869.241265	36.158848
1384.900993	143105.264344	36.163866
1386.097669	143340.866081	36.168884
1387.176145	143599.340097	36.173901
1388.393735	143850.387199	36.178919
1389.684445	144108.943881	36.183936
1390.221284	144375.084034	36.188954
1391.375904	144641.897297	36.193972
1392.163487	144919.413152	36.198989
1393.576428	145199.541315	36.204007
1394.696717	145488.001312	36.209024
1395.808493	145786.889436	36.214042
1396.882775	146068.691124	36.219060
1398.177747	146385.752295	36.224077
1399.657577	146676.977589	36.229095
1400.836047	146990.195343	36.234112
1402.056500	147297.841312	36.239130
1403.687162	147606.246211	36.244148
1405.017944	147915.857546	36.249165
1407.004997	148214.962943	36.254183
1409.051135	148509.013265	36.259200
1410.831276	148796.350112	36.264218
1412.582310	149085.444261	36.269236
1413.885312	149379.168153	36.274253
1415.575971	149665.093400	36.279271
1417.302778	149950.532887	36.284288
1418.927026	150231.197282	36.289306
1420.398625	150510.823689	36.294324
1421.856523	150794.297544	36.299341
1423.108786	151069.119388	36.304359
1424.721852	151345.557649	36.309376
1425.787116	151625.640215	36.314394
1428.193626	151886.235694	36.319412
1430.013198	152147.894263	36.324429
1431.508536	152409.303975	36.329447
1433.360006	152648.941252	36.334464
1435.368011	152887.425183	36.339482
1437.195873	153092.428693	36.344500
1438.269175	153312.234158	36.349517
1439.504481	153530.288938	36.354535
1441.339753	153749.907133	36.359552
1442.219267	153983.955146	36.364570
1443.495025	154194.472351	36.369588
1444.801852	154426.245056	36.374605
1445.740437	154665.627627	36.379623
1446.738247	154914.020761	36.384640
1447.845692	155163.602359	36.389658
1449.038183	155414.465313	36.394676
1450.034569	155675.649982	36.399693
1451.399306	155943.637979	36.404711
1452.497942	156213.447849	36.409728
1453.454480	156508.717228	36.414746
1454.610421	156791.752344	36.419764
1455.975535	157087.896995	36.424781
1456.906756	157384.635891	36.429799
1458.479459	157690.214054	36.434816
1459.545172	158002.208823	36.439834
1462.247649	158280.266211	36.444852
1464.066128	158572.566226	36.449869
1465.910528	158863.519325	36.454887
1467.497960	159150.381417	36.459904
1469.044379	159452.526594	36.464922
1470.981847	159734.310986	36.469940
1472.425698	160029.499927	36.474957
1474.192158	160291.779368	36.479975
1475.836919	160578.629253	36.484992
1477.410670	160861.496587	36.490010
1479.174799	161129.325813	36.495028
1480.750711	161409.938274	36.500045
1483.014522	161674.668684	36.505063
1485.165429	161923.192778	36.510080
1487.145902	162162.218592	36.515098
1488.667470	162403.973468	36.520116
1490.380699	162649.960869	36.525133
1492.261978	162880.557498	36.530151
1493.538620	163128.383600	36.535168
1494.803011	163366.925957	36.540186
1496.124006	163605.802827	36.545204
1497.449635	163860.159142	36.550221
1498.804330	164107.432422	36.555239
1500.010906	164349.491642	36.560256
1500.900583	164614.404784	36.565274
1502.120933	164870.954148	36.570292
1503.949097	165132.707837	36.575309
1505.300164	165398.259804	36.580327
1505.973167	165673.441910	36.585344
1507.292357	165950.624859	36.590362
1508.577385	166240.960304	36.595380
1509.669965	166530.834726	36.600397
1511.051797	166825.586222	36.605415
1512.892226	167106.192049	36.610432
1514.290905	167413.049540	36.615450
1515.806967	167701.567170	36.620468
1516.802330	168004.232184	36.625485
1517.731467	168308.470955	36.630503
1519.522331	168618.126690	36.635520
1520.719235	168936.790748	36.640538
1522.970622	169219.181591	36.645556
1525.546115	169520.376654	36.650573
1526.848705	169811.988590	36.655591
1529.618981	170072.676125	36.660608
1531.508281	170363.356808	36.665626
1533.997669	170608.815848	36.670644
1535.466093	170859.470539	36.675661
1536.646320	171108.029811	36.680679
1538.295722	171344.508145	36.685696
1539.211579	171589.738354	36.690714
1540.382672	171844.153071	36.695732
1541.399676	172097.033855	36.700749
1542.545144	172370.224095	36.705767
1543.927103	172629.607976	36.710784
1544.824789	172925.481618	36.715802
1545.956867	173203.018928	36.720820
1547.333197	173499.095979	36.725837
1548.338954	173782.190582	36.730855
1550.117642	174083.077657	36.735872
1551.296194	174392.441870	36.740890
1552.888403	174696.714002	36.745908
1554.231972	175017.311447	36.750925
1555.456905	175336.864649	36.755943
1557.334587	175656.667078	36.760960
1558.304711	175993.945213	36.765978
1560.029979	176322.381725	36.770996
1561.701543	176654.458990	36.776013
1563.009838	176996.421707	36.781031
1564.865675	177314.207905	36.786048
1566.482503	177669.779938	36.791066
1568.037487	178006.454437	36.796084
1569.763869	178352.583370	36.801101
1571.096088	178694.566386	36.806119
1574.485330	179002.234938	36.811136
1576.672854	179315.143209	36.816154
1578.710376	179611.946881	36.821172
1581.585369	179904.095105	36.826189
1583.333491	180189.730403	36.831207
1585.105120	180474.005327	36.836224
1586.658778	180766.555152	36.841242
1588.166570	181032.092465	36.846260
1589.938580	181326.043449	36.851277
1591.086727	181629.568003	36.856295
1592.855526	181916.224703	36.861312
1593.909118	182209.830084	36.866330
1595.170500	182502.171462	36.871348
1596.468253	182799.001609	36.876365
1597.093493	183118.284071	36.881383
1598.766420	183435.858926	36.886400
1600.239914	183750.866669	36.891418
1601.618978	184073.380733	36.896436
1603.529094	184381.833660	36.901453
1605.322215	184708.369992	36.906471
1608.018700	184990.840170	36.911488
1610.067037	185294.896177	36.916506
1612.004054	185587.383327	36.921524
1613.716194	185887.550698	36.926541
1615.104447	186173.239393	36.931559
1616.805061	186472.002841	36.936576
1618.034397	186772.711949	36.941594
1619.352123	187070.056885	36.946612
1620.875830	187371.507382	36.951629
1621.871088	187689.460110	36.956647
1623.663054	187996.835511	36.961664
1624.689295	188299.338084	36.966682
1626.304298	188618.856123	36.971700
1628.137560	188949.777077	36.976717
1629.397362	189282.394425	36.981735
1631.093578	189606.525075	36.986752
1632.309339	189936.195681	36.991770
1634.093214	190252.051388	36.996788
1636.055842	190577.387247	37.001805
1637.632452	190914.848608	37.006823
1638.885345	191243.961741	37.011840
1640.701370	191577.375663	37.016858
1641.914685	191891.151104	37.021876
1643.341817	192215.124681	37.026893
1644.827359	192536.538636	37.031911
1646.063595	192863.746373	37.036928
1647.584581	193196.443639	37.041946
1648.741777	193541.009347	37.046964
1650.177606	193884.426300	37.051981
1651.202976	194240.925698	37.056999
1653.434339	194587.413808	37.062016
1654.975463	194946.751598	37.067034
1656.135347	195325.362695	37.072052
1657.598751	195688.005631	37.077069
1658.716145	196072.556935	37.082087
1660.635791	196452.000872	37.087104
1662.469323	196835.600074	37.092122
1664.190654	197211.069448	37.097140
1666.433461	197587.228966	37.102157
1668.936952	197953.990543	37.107175
1670.869454	198323.286392	37.112192
1672.598089	198694.154276	37.117210
1674.348748	199064.804706	37.122228
1675.969278	199437.510105	37.127245
1677.710847	199806.642524	37.132263
1679.225134	200181.248600	37.137280
1680.923460	200556.956169	37.142298
1682.603090	200938.674267	37.147316
1684.764949	201304.304227	37.152333
1686.442338	201684.744384	37.157351
1688.594442	202061.984520	37.162368
1690.398722	202425.457587	37.167386
1691.814901	202799.027247	37.172404
1693.800597	203171.653747	37.177421
1694.894596	203554.295416	37.182439
1696.307106	203921.154753	37.187456
1697.748377	204311.272074	37.192474
1699.537189	204704.914407	37.197492
1701.384524	205079.630345	37.202509
1702.795978	205480.957554	37.207527
1705.421176	205860.170203	37.212544
1707.428930	206240.071134	37.217562
1709.053253	206615.860031	37.222580
1710.901715	206998.101993	37.227597
1712.711753	207379.882375	37.232615
1714.764710	207746.247561	37.237632
1717.206300	208107.991568	37.242650
1719.129968	208459.829954	37.247668
1721.071798	208815.349210	37.252685
1723.687385	209167.520414	37.257703
1725.463136	209498.906245	37.262720
1727.518397	209837.726153	37.267738
1729.073619	210177.316003	37.272756
1730.801217	210501.869612	37.277773
1732.618508	210844.593230	37.282791
1734.491097	211170.395181	37.287808
1736.090984	211508.129047	37.292826
1737.287153	211844.991478	37.297844
1738.805679	212170.500343	37.302861
1740.670405	212500.778403	37.307879
1743.155188	212821.050230	37.312896
1745.437714	213150.829742	37.317914
1746.758438	213483.868289	37.322932
1748.103421	213812.662754	37.327949
1749.595597	214147.910273	37.332967
1751.200661	214484.613353	37.337984
1752.416133	214824.963246	37.343002
1753.878221	215178.886503	37.348020
1755.831564	215515.941973	37.353037
1757.094144	215861.748291	37.358055
1758.306342	216203.881561	37.363072
1760.079800	216535.535373	37.368090
1761.081763	216886.264949	37.373108
1762.680149	217239.563731	37.378125
1763.728457	217605.806334	37.383143
1765.264653	217972.020236	37.388160
1766.940650	218357.972108	37.393178
1768.475289	218741.561446	37.398196
1770.441350	219122.032930	37.403213
1772.237297	219505.912014	37.408231
1774.214355	219940.585062	37.413248
1776.501008	220314.124780	37.418266
1778.428630	220702.126415	37.423284
1780.557740	221086.133848	37.428301
1782.217969	221464.581783	37.433319
1784.439467	221826.200058	37.438336
1786.598127	222200.199304	37.443354
1788.196220	222583.182423	37.448372
1790.145089	222949.167395	37.453389
1792.022194	223324.512406	37.458407
1793.620109	223702.851246	37.463424
1795.342803	224083.507401	37.468442
1797.041439	224467.140533	37.473460
1799.511356	224849.351713	37.478477
1800.989081	225226.800972	37.483495
1802.768491	225604.988809	37.488512
1804.463307	225994.647202	37.493530
1805.363636	226399.119681	37.498548
1806.981112	226798.039003	37.503565
1808.224406	227209.213666	37.508583
1809.939996	227636.110341	37.513600
1811.932508	228039.772010	37.518618
1814.127002	228449.980149	37.523636
1816.812146	228849.795640	37.528653
1818.809960	229257.092369	37.533671
1820.533792	229680.590513	37.538688
1822.185249	230077.558180	37.543706
1823.729817	230503.704780	37.548724
1825.567085	230915.427250	37.553741
1827.385135	231332.869278	37.558759
1828.600322	231769.082122	37.563776
1830.189928	232198.375893	37.568794
1832.324844	232639.900072	37.573812
1834.273071	233070.584714	37.578829
1836.017951	233498.078260	37.583847
1838.378948	233904.082907	37.588864
1840.811213	234321.583599	37.593882
1842.489737	234772.968814	37.598900
1844.145666	235191.667174	37.603917
1845.777792	235630.971206	37.608935
1847.633955	236058.630648	37.613952
1849.525495	236482.500392	37.618970
1851.843526	236915.292691	37.623988
1853.656976	237339.304358	37.629005
1855.520405	237767.703225	37.634023
1856.969578	238201.328280	37.639040
1859.003311	238628.608532	37.644058
1860.419473	239072.350956	37.649076
1862.324060	239508.468974	37.654093
1864.524937	239944.919834	37.659111
1866.073032	240388.414550	37.664128
1867.744997	240826.072510	37.669146
1869.379585	241268.640160	37.674164
1871.207253	241719.534048	37.679181
1872.821766	242169.422609	37.684199
1874.352562	242632.052511	37.689216
1876.206536	243079.794644	37.694234
1877.638198	243556.337829	37.699252
1880.228041	243985.771348	37.704269
1884.125965	244361.567050	37.709287
1887.220409	244754.516176	37.714304
1890.702454	245111.964840	37.719322
1893.196247	245464.928976	37.724340
1894.745195	245815.814625	37.729357
1896.688585	246181.699174	37.734375
1898.600874	246531.814139	37.739392
1900.160599	246886.687417	37.744410
1901.639928	247245.130788	37.749428
1903.930674	247580.425061	37.754445
1905.935641	247949.248049	37.759463
1907.527110	248301.018323	37.764480
1909.285446	248648.950826	37.769498
1910.550773	249038.804047	37.774516
1911.972079	249405.134000	37.779533
1913.344355	249796.494382	37.784551
1914.949508	250180.475038	37.789568
1916.734292	250580.277772	37.794586
1918.033417	250986.588279	37.799604
1919.908349	251387.799292	37.804621
1921.601893	251805.527293	37.809639
1923.170422	252235.876275	37.814656
1924.880632	252665.414588	37.819674
1926.035493	253110.668154	37.824692
1927.940382	253542.511861	37.829709
1929.890047	254007.194763	37.834727
1931.422815	254473.598202	37.839744
1933.235268	254935.738600	37.844762
1934.560185	255418.333392	37.849780
1936.160061	255899.942908	37.854797
1938.052148	256391.259041	37.859815
1939.653720	256890.600083	37.864832
1942.116174	257380.018358	37.869850
1943.703898	257897.779296	37.874868
1945.624969	258398.287041	37.879885
1947.721496	258901.128256	37.884903
1949.499293	259419.365866	37.889920
1951.498069	259942.698297	37.894938
1953.214984	260457.389429	37.899956
1955.159761	260984.058463	37.904973
1957.217319	261512.563110	37.909991
1959.115189	262046.936784	37.915008
1961.232659	262577.691999	37.920026
1962.824888	263112.573090	37.925044
1964.960954	263658.871452	37.930061
1967.317095	264186.537859	37.935079
1969.933856	264717.209113	37.940096
1972.426974	265228.416217	37.945114
1974.863567	265748.167739	37.950132
1977.459192	266250.364305	37.955149
1979.766621	266765.741565	37.960167
1981.442295	267273.348015	37.965184
1983.635663	267776.244821	37.970202
1985.528443	268291.079487	37.975220
1988.055346	268783.936519	37.980237
1990.601520	269253.088808	37.985255
1992.777230	269742.421031	37.990272
1995.104457	270223.242951	37.995290
1997.583676	270698.043976	38.000308
1999.941589	271154.599812	38.005325
2002.808568	271603.145022	38.010343
2004.460257	272062.712498	38.015360
2006.575382	272498.146149	38.020378
2008.179016	272963.994700	38.025396
2009.969664	273416.906984	38.030413
2011.589284	273869.973882	38.035431
2013.358732	274331.855298	38.040448
2014.909276	274779.521361	38.045466
2016.788241	275216.132973	38.050484
2018.833865	275658.126933	38.055501
2021.186364	276088.307957	38.060519
2022.956874	276522.242543	38.065536
2025.143897	276969.849957	38.070554
2026.791188	277421.813464	38.075572
2028.388700	277873.758888	38.080589
2030.154440	278327.733069	38.085607
2031.521933	278808.419002	38.090624
2033.505692	279269.264371	38.095642
2035.021434	279760.287509	38.100660
2036.834174	280247.500741	38.105677
2038.795123	280737.888811	38.110695
2040.263260	281261.735116	38.115712
2041.956716	281766.770763	38.120730
2043.903273	282280.348797	38.125748
2045.876132	282812.997504	38.130765
2048.209871	283331.613982	38.135783
2049.810796	283886.978992	38.140800
2051.801776	284413.980492	38.145818
2053.515860	284962.363117	38.150836
2055.815634	285514.126760	38.155853
2057.997911	286054.528231	38.160871
2059.873695	286620.049224	38.165888
2061.837896	287180.600243	38.170906
2063.950989	287745.569548	38.175924
2066.092337	288305.756604	38.180941
2069.341261	288844.599326	38.185959
2071.498365	289396.854372	38.190976
2073.825563	289949.993378	38.195994
2076.106061	290496.584543	38.201012
2077.942332	291063.287639	38.206029
2080.200396	291617.497759	38.211047
2082.091127	292184.643985	38.216064
2084.204265	292733.564542	38.221082
2085.833902	293302.120391	38.226100
2087.887966	293869.409441	38.231117
2090.925483	294423.426772	38.236135
2093.653136	294973.022487	38.241152
2096.723036	295515.675685	38.246170
2099.220605	296045.492943	38.251188
2101.438307	296575.100011	38.256205
2104.121051	297087.610300	38.261223
2106.546630	297602.929176	38.266240
2108.734495	298120.265990	38.271258
2110.943479	298622.179914	38.276276
2113.132590	299138.216112	38.281293
2115.448203	299627.967064	38.286311
2117.716231	300131.108256	38.291328
2119.908520	300628.544911	38.296346
2121.858184	301126.933540	38.301364
2123.623680	301630.962975	38.306381
2125.970624	302130.499688	38.311399
2128.489791	302619.871691	38.316416
2130.574995	303100.881126	38.321434
2132.807536	303598.219375	38.326452
2134.549867	304092.334501	38.331469
2136.953338	304586.718379	38.336487
2138.942754	305087.644245	38.341504
2140.870770	305579.536281	38.346522
2143.261776	306070.231430	38.351540
2145.021984	306569.231249	38.356557
2147.016432	307054.043748	38.361575
2148.897196	307569.728361	38.366592
2150.859207	308071.200110	38.371610
2153.217012	308573.796876	38.376628
2154.723699	309082.347083	38.381645
2156.782250	309563.578946	38.386663
2158.899796	310060.695533	38.391680
2160.669764	310547.073710	38.396698
2162.792785	311040.500980	38.401716
2164.457956	311543.498573	38.406733
2166.471351	312041.076992	38.411751
2169.557502	312525.498018	38.416768
2171.913568	313011.204999	38.421786
2173.947335	313519.283571	38.426804
2175.977280	314027.917986	38.431821
2177.520909	314540.565461	38.436839
2178.871045	315081.986821	38.441856
2180.809828	315606.724843	38.446874
2182.716591	316148.046041	38.451892
2184.003872	316716.966231	38.456909
2185.864759	317273.471389	38.461927
2187.558552	317857.499854	38.466944
2189.654919	318430.817364	38.471962
2191.708976	319024.298377	38.476980
2193.646815	319627.975570	38.481997
2195.712165	320228.756974	38.487015
2197.808583	320855.020736	38.492032
2199.525814	321479.310047	38.497050
2201.455308	322108.636405	38.502068
2202.994513	322762.548595	38.507085
2205.211786	323416.595711	38.512103
2207.635436	324075.476784	38.517120
2209.597888	324734.985870	38.522138
2212.764274	325398.757132	38.527156
2214.638566	326057.174925	38.532173
2217.270787	326733.917869	38.537191
2219.467410	327408.567291	38.542208
2222.191554	328061.566952	38.547226
2225.627962	328701.468098	38.552244
2227.915903	329361.304165	38.557261
2230.694507	329998.228038	38.562279
2233.395613	330633.989857	38.567296
2236.403174	331250.653563	38.572314
2239.760208	331856.234809	38.577332
2241.881121	332470.924827	38.582349
2244.505253	333081.285212	38.587367
2247.282727	333691.816515	38.592384
2249.174410	334299.542925	38.597402
2251.411108	334887.963297	38.602420
2253.539520	335489.392295	38.607437
2256.000040	336089.642578	38.612455
2258.042382	336697.824471	38.617472
2259.610829	337298.970207	38.622490
2261.793569	337905.667886	38.627508
2263.709368	338532.607961	38.632525
2265.918906	339145.886294	38.637543
2268.288345	339769.055485	38.642560
2270.040866	340399.527792	38.647578
2272.053290	341033.807231	38.652596
2274.071049	341671.631162	38.657613
2276.398411	342316.451670	38.662631
2278.466774	342960.012109	38.667648
2280.706054	343605.058567	38.672666
2283.078511	344249.312909	38.677684
2285.079500	344893.518547	38.682701
2287.316000	345548.234493	38.687719
2290.081927	346196.178836	38.692736
2292.522675	346831.833716	38.697754
2295.699744	347459.312854	38.702772
2298.133376	348100.331779	38.707789
2301.047095	348721.391096	38.712807
2303.651459	349345.259317	38.717824
2306.368357	349944.534843	38.722842
2308.885394	350521.934932	38.727860
2311.371499	351099.459531	38.732877
2313.708660	351655.583455	38.737895
2316.124512	352218.208995	38.742912
2318.297264	352776.655137	38.747930
2320.927680	353345.879056	38.752948
2322.530472	353902.095866	38.757965
2324.801830	354476.845311	38.762983
2326.865006	355046.546567	38.768000
2329.438263	355603.011877	38.773018
2332.065235	356185.519897	38.778036
2333.955189	356760.504411	38.783053
2336.181776	357340.652119	38.788071
2338.143636	357929.233915	38.793088
2340.140393	358539.900886	38.798106
2342.297592	359135.004489	38.803124
2344.475356	359747.678532	38.808141
2346.830387	360350.393767	38.813159
2349.069066	360956.214465	38.818176
2351.168301	361582.928973	38.823194
2353.056236	362198.201278	38.828212
2355.710013	362827.239787	38.833229
2358.018649	363464.215182	38.838247
2360.172984	364105.670624	38.843264
2362.433649	364749.888361	38.848282
2365.105792	365392.226060	38.853300
2367.906206	366036.003050	38.858317
2370.276771	366682.808253	38.863335
2372.992326	367320.235681	38.868352
2375.208677	367969.504888	38.873370
2377.683095	368614.661544	38.878388
2379.718213	369269.442463	38.883405
2382.557319	369905.587612	38.888423
2385.534930	370545.782481	38.893440
2387.705666	371206.340200	38.898458
2389.726147	371859.225587	38.903476
2391.975997	372514.927209	38.908493
2394.625931	373172.883962	38.913511
2397.143207	373828.821544	38.918528
2399.419284	374490.518653	38.923546
2401.619450	375152.215893	38.928564
2403.564571	375826.496420	38.933581
2405.701904	376508.720547	38.938599
2407.798106	377198.723475	38.943616
2409.617772	377900.017839	38.948634
2411.909622	378601.625396	38.953652
2414.120065	379314.541695	38.958669
2416.214902	380022.491992	38.963687
2418.286984	380749.144674	38.968704
2420.934003	381472.719653	38.973722
2423.430688	382188.798369	38.978740
2426.055042	382930.956501	38.983757
2428.036502	383661.642447	38.988775
2430.635362	384400.728856	38.993792
2433.025658	385151.064619	38.998810
2435.534434	385896.825087	39.003828
2437.861580	386637.324931	39.008845
2441.340147	387358.121321	39.013863
2445.840240	388023.491541	39.018880
2449.599915	388717.540662	39.023898
2453.173104	389379.156892	39.028916
2456.054774	390050.430391	39.033933
2458.919839	390693.148880	39.038951
2461.668620	391329.485347	39.043968
2463.917172	391971.290582	39.048986
2466.260741	392609.517934	39.054004
2468.529480	393233.296414	39.059021
2471.009269	393850.665103	39.064039
2473.340654	394462.697673	39.069056
2475.536209	395061.078964	39.074074
2477.553338	395651.924959	39.079092
2479.257957	396272.996306	39.084109
2481.330214	396879.699733	39.089127
2483.796031	397486.756358	39.094144
2485.647905	398120.689548	39.099162
2487.921001	398753.550894	39.104180
2489.811486	399407.368802	39.109197
2491.616382	400063.162711	39.114215
2494.544579	400710.241281	39.119232
2496.671718	401382.347139	39.124250
2498.768502	402044.661130	39.129268
2501.283296	402736.207576	39.134285
2503.046990	403423.401869	39.139303
2505.498079	404124.806689	39.144320
2507.878717	404828.131186	39.149338
2509.962821	405542.660315	39.154356
2512.310789	406264.981397	39.159373
2515.940231	406966.752753	39.164391
2520.339880	407632.935839	39.169408
2522.639266	408351.789838	39.174426
2524.864825	409058.831817	39.179444
2527.355408	409776.881707	39.184461
2529.246551	410497.570148	39.189479
2531.710589	411210.545059	39.194496
2533.962328	411945.320144	39.199514
2536.025602	412675.470736	39.204532
2538.310651	413435.705861	39.209549
2540.293583	414192.802955	39.214567
2542.932840	414950.503987	39.219584
2545.220831	415719.562112	39.224602
2547.780561	416491.211628	39.229620
2550.002561	417285.053439	39.234637
2552.127300	418086.965221	39.239655
2554.583880	418882.947103	39.244672
2556.208721	419696.539685	39.249690
2558.397009	420524.876760	39.254708
2560.935980	421360.876709	39.259725
2562.863141	422221.459891	39.264743
2565.204373	423065.613746	39.269760
2567.585384	423947.380722	39.274778
2570.325585	424819.435939	39.279796
2573.058038	425687.714449	39.284813
2575.466822	426575.812401	39.289831
2578.566689	427446.701188	39.294848
2581.343788	428317.611845	39.299866
2584.476184	429200.379705	39.304884
2587.121668	430080.816063	39.309901
2589.996151	430955.562717	39.314919
2593.486609	431815.039477	39.319936
2596.478198	432684.134135	39.324954
2598.755186	433550.480119	39.329972
2602.058357	434406.855299	39.334989
2604.720882	435250.449065	39.340007
2607.892983	436102.430147	39.345024
2610.339499	436953.436743	39.350042
2613.317402	437786.914701	39.355060
2616.271691	438621.580396	39.360077
2618.308898	439467.651480	39.365095
2621.108020	440321.508984	39.370112
2624.195791	441150.138068	39.375130
2627.340005	441965.166705	39.380148
2630.116415	442793.229279	39.385165
2632.423015	443627.106139	39.390183
2635.078222	444453.203590	39.395200
2637.314504	445280.856766	39.400218
2639.611462	446102.853063	39.405236
2642.030354	446915.591225	39.410253
2644.318969	447711.779164	39.415271
2647.031544	448516.516956	39.420288
2649.238564	449315.390115	39.425306
2651.766912	450127.886862	39.430324
2654.395855	450945.848598	39.435341
2656.883760	451764.611086	39.440359
2659.184875	452591.362987	39.445376
2661.484499	453416.312412	39.450394
2664.081524	454258.423788	39.455412
2667.102975	455091.733204	39.460429
2670.207385	455929.849371	39.465447
2673.226787	456752.877728	39.470464
2675.942254	457603.074148	39.475482
2678.731790	458434.162282	39.480500
2681.513250	459266.734320	39.485517
2684.677469	460102.747427	39.490535
2687.865978	460926.336440	39.495552
2690.455509	461765.863307	39.500570
2693.616026	462611.679858	39.505588
2696.100438	463451.102338	39.510605
2698.417996	464285.310748	39.515623
2701.495319	465128.657649	39.520640
2703.665453	465979.901336	39.525658
2706.130444	466826.712890	39.530676
2708.928101	467675.908659	39.535693
2711.201752	468540.263022	39.540711
2714.178626	469416.336806	39.545728
2716.747780	470292.387469	39.550746
2719.353800	471158.943547	39.555764
2722.453739	472033.007394	39.560781
2725.112588	472904.173631	39.565799
2727.993289	473775.111334	39.570816
2731.166077	474648.182997	39.575834
2734.720744	475498.722537	39.580852
2738.150956	476359.598655	39.585869
2740.568423	477221.460997	39.590887
2743.294948	478068.332457	39.595904
2745.975791	478932.546020	39.600922
2748.772037	479794.376613	39.605940
2751.179954	480667.290165	39.610957
2753.330098	481540.406416	39.615975
2755.959231	482428.246761	39.620992
2758.003846	483321.037821	39.626010
2760.421991	484208.673701	39.631028
2763.396185	485113.793549	39.636045
2765.817420	486032.842120	39.641063
2768.582561	486934.521308	39.646080
2771.559517	487853.383355	39.651098
2774.212092	488760.994723	39.656116
2777.254640	489680.557846	39.661133
2781.151341	490558.342634	39.666151
2786.286968	491415.185765	39.671168
2789.464289	492295.928748	39.676186
2792.439329	493153.295370	39.681204
2795.655247	494000.386106	39.686221
2798.887697	494835.977956	39.691239
2802.213782	495654.004908	39.696256
2805.368156	496483.928033	39.701274
2807.960851	497313.096140	39.706292
2810.858735	498126.533731	39.711309
2812.831778	498955.370300	39.716327
2815.298656	499768.446430	39.721344
2818.281376	500598.194716	39.726362
2821.268690	501418.166044	39.731380
2824.177014	502223.180556	39.736397
2826.917385	503048.105151	39.741415
2829.408679	503859.564298	39.746432
2831.832491	504644.266894	39.751450
2834.231580	505426.817966	39.756468
2837.141163	506213.180104	39.761485
2839.849453	506988.646270	39.766503
2842.574121	507784.240427	39.771520
2845.811197	508553.594465	39.776538
2848.939388	509340.322785	39.781556
2851.397062	510133.374509	39.786573
2854.035216	510936.489357	39.791591
2856.572099	511721.433844	39.796608
2859.666301	512543.345151	39.801626
2861.955929	513355.468029	39.806644
2864.246387	514164.776961	39.811661
2866.703661	515011.511813	39.816679
2869.517076	515843.225335	39.821696
2872.645858	516689.002315	39.826714
2875.160748	517540.528739	39.831732
2878.107007	518389.115418	39.836749
2880.874145	519250.482374	39.841767
2883.596004	520129.995832	39.846784
2886.573484	520994.253033	39.851802
2889.132520	521881.199033	39.856820
2891.661317	522754.095143	39.861837
2894.467969	523678.019059	39.866855
2896.876595	524585.231093	39.871872
2899.694157	525502.191885	39.876890
2902.429619	526420.016729	39.881908
2905.233390	527338.126469	39.886925
2907.688508	528293.649555	39.891943
2910.669012	529233.214500	39.896960
2914.067217	530186.999442	39.901978
2916.651821	531136.980835	39.906996
2919.507163	532109.962028	39.912013
2922.433111	533074.259333	39.917031
2925.589484	534042.783421	39.922048
2928.352210	535003.255290	39.927066
2931.021558	536001.423701	39.932084
2934.760736	536979.166613	39.937101
2937.075898	537964.324523	39.942119
2940.264955	538960.188693	39.947136
2943.061027	539952.778023	39.952154
2946.140002	540954.558394	39.957172
2948.548665	541957.686693	39.962189
2951.217685	542991.032542	39.967207
2953.389385	544007.484549	39.972224
2956.205673	545058.056880	39.977242
2958.191511	546112.006602	39.982260
2960.981951	547170.470264	39.987277
2963.454476	548252.990975	39.992295
2966.321246	549334.406200	39.997312
2969.593221	550422.456340	40.002330
2972.410135	551531.156435	40.007348
2975.848607	552610.157031	40.012365
2978.755942	553719.367489	40.017383
2981.323877	554822.411544	40.022400
2984.603116	555925.649649	40.027418
2987.405088	557045.508729	40.032436
2990.916831	558143.299589	40.037453
2994.737853	559243.410581	40.042471
2998.546490	560329.215057	40.047488
3002.100812	561407.839135	40.052506
3005.426407	562493.344263	40.057524
3009.885497	563530.857956	40.062541
3013.892457	564566.656434	40.067559
3017.804604	565583.657005	40.072576
3021.019486	566607.572362	40.077594
3023.849704	567620.976394	40.082612
3027.311576	568602.968270	40.087629
3030.379015	569560.702677	40.092647
3033.152577	570503.454886	40.097664
3036.520831	571439.061999	40.102682
3039.542576	572371.646080	40.107700
3043.127536	573294.231675	40.112717
3046.185400	574211.718305	40.117735
3048.965121	575140.123305	40.122752
3051.653644	576059.543357	40.127770
3054.361151	576992.288791	40.132788
3056.968287	577925.884128	40.137805
3059.166494	578891.080905	40.142823
3061.404602	579845.511675	40.147840
3064.690881	580824.322532	40.152858
3067.252999	581799.363729	40.157876
3070.876886	582772.095825	40.162893
3074.402825	583736.693440	40.167911
3077.724173	584720.101663	40.172928
3081.289483	585686.945079	40.177946
3084.617001	586652.497373	40.182964
3088.519550	587609.706398	40.187981
3091.673285	588562.903042	40.192999
3096.055423	589497.777296	40.198016
3099.692474	590436.761235	40.203034
3102.853203	591375.850297	40.208052
3105.984061	592315.371298	40.213069
3108.624006	593261.312577	40.218087
3111.094944	594216.975943	40.223104
3113.992245	595166.078947	40.228122
3116.261932	596136.097992	40.233140
3119.262344	597109.071582	40.238157
3122.330249	598084.857937	40.243175
3125.083590	599066.524101	40.248192
3128.170752	600045.948913	40.253210
3131.213681	601061.350064	40.258228
3133.988898	602063.538401	40.263245
3136.785539	603101.180769	40.268263
3139.318850	604116.346579	40.273280
3142.243957	605162.841545	40.278298
3144.848540	606222.556533	40.283316
3147.671098	607276.631732	40.288333
3150.254037	608346.110823	40.293351
3153.229401	609419.076289	40.298368
3156.354467	610511.176395	40.303386
3159.217312	611611.867905	40.308404
3162.831107	612718.479381	40.313421
3166.297757	613805.399121	40.318439
3169.468595	614920.967458	40.323456
3172.804994	616029.895223	40.328474
3175.784417	617147.970582	40.333492
3178.751898	618263.634390	40.338509
3182.070861	619393.173729	40.343527
3184.729326	620521.505754	40.348544
3188.299538	621650.569639	40.353562
3191.657030	622793.194198	40.358580
3195.366841	623905.158365	40.363597
3198.770827	625038.642839	40.368615
3202.315804	626168.687032	40.373632
3205.423853	627284.297441	40.378650
3208.252796	628414.971676	40.383668
3211.637874	629554.073861	40.388685
3215.016112	630679.971016	40.393703
3217.938620	631812.065009	40.398720
3221.263719	632946.966303	40.403738
3224.745192	634082.417864	40.408756
3227.772232	635216.872832	40.413773
3231.594640	636341.589787	40.418791
3234.579434	637477.302593	40.423808
3237.957136	638582.985748	40.428826
3240.967500	639678.881724	40.433844
3244.143830	640760.963858	40.438861
3246.553824	641862.812624	40.443879
3249.400990	642937.885056	40.448896
3252.593827	644055.678117	40.453914
3255.997660	645153.815009	40.458932
3259.321491	646257.031783	40.463949
3262.579929	647360.886707	40.468967
3266.103493	648461.336422	40.473984
3270.393867	649542.696870	40.479002
3273.747567	650653.650812	40.484020
3277.184972	651746.227530	40.489037
3281.149255	652826.189511	40.494055
3284.469469	653934.689611	40.499072
3287.823820	655020.990097	40.504090
3290.510048	656137.766926	40.509108
3293.007466	657248.520969	40.514125
3296.927974	658355.875934	40.519143
3300.177308	659471.183633	40.524160
3303.876444	660572.347897	40.529178
3307.606441	661676.120284	40.534196
3311.789769	662779.144256	40.539213
3315.650822	663882.841967	40.544231
3318.871184	664970.443952	40.549248
3322.191365	666053.775851	40.554266
3325.444204	667169.735872	40.559284
3328.248339	668275.739093	40.564301
3331.435528	669378.167690	40.569319
3334.200358	670494.862691	40.574336
3337.491995	671625.114709	40.579354
3340.221350	672774.966210	40.584372
3343.207243	673928.413344	40.589389
3346.346831	675079.803849	40.594407
3348.816435	676261.037854	40.599424
3351.976842	677430.327796	40.604442
3354.823626	678639.477565	40.609460
3357.486423	679851.928225	40.614477
3361.264913	681067.612188	40.619495
3364.522536	682273.037828	40.624512
3368.275981	683493.173391	40.629530
3372.421764	684713.428697	40.634548
3376.324874	685920.004379	40.639565
3380.790378	687119.177108	40.644583
3384.404366	688319.225128	40.649600
3388.054019	689510.073719	40.654618
3391.458505	690707.852501	40.659636
3394.892299	691912.066231	40.664653
3398.562452	693097.968575	40.669671
3401.822314	694300.102467	40.674688
3405.190016	695486.381208	40.679706
3408.452647	696679.858636	40.684724
3411.544872	697894.675187	40.689741
3414.918231	699095.196041	40.694759
3418.485961	700283.523050	40.699776
3422.053801	701484.180045	40.704794
3425.790346	702684.247316	40.709812
3429.597035	703866.297251	40.714829
3433.807183	705039.646390	40.719847
3437.573482	706232.181456	40.724864
3441.044488	707405.727260	40.729882
3444.699967	708580.171878	40.734900
3448.488293	709735.565640	40.739917
3452.266907	710881.446289	40.744935
3455.386296	712040.748016	40.749952
3458.523270	713197.908501	40.754970
3461.895793	714354.030510	40.759988
3464.788214	715515.814185	40.765005
3468.259005	716660.705834	40.770010
3471.282600	717766.591061	40.775015
3474.137340	718818.696223	40.780020
3476.991318	719824.451877	40.785024
3480.145326	720759.132106	40.790029
3483.332009	721634.306983	40.795034
3486.340827	722448.790561	40.800039
3489.009772	723193.704903	40.805044
3491.497645	723886.984992	40.810048
3493.435421	724519.734147	40.815053
3495.747267	725073.229353	40.820058
3497.741325	725588.186300	40.825063
3499.986401	726043.062212	40.830068
3501.742907	726452.061335	40.835072
3503.410958	726797.832364	40.840077
3505.160580	727097.646637	40.845082
3506.558536	727363.570446	40.850087
3507.978717	727572.359337	40.855092
3509.604549	727754.257375	40.860096
3510.471090	727901.251587	40.865101
3511.743012	727998.190287	40.870106
3512.586712	728065.672952	40.875111
3513.118515	728107.446096	40.880116
3513.903927	728118.462725	40.885120
3514.381509	728097.280015	40.890125
3515.647064	728059.767544	40.895130
3515.868263	727996.914332	40.900135
3516.446159	727906.902966	40.905140
3517.157225	727807.852092	40.910144
3517.258913	727682.148040	40.915149
3517.502751	727540.317128	40.920154
3517.958588	727404.691243	40.925159
3518.636013	727233.998405	40.930164
3519.241000	727059.251225	40.935168
3519.166862	726869.599819	40.940173
3519.740734	726648.076524	40.945178
3519.695402	726436.955894	40.950183
3520.047836	726203.961684	40.955188
3520.309066	725974.147290	40.960192
3520.592753	725730.199914	40.965197
3520.865477	725473.511378	40.970202
3520.782662	725206.020601	40.975207
3521.041838	724935.292861	40.980212
3521.323271	724670.301534	40.985216
3521.048933	724387.105184	40.990221
3521.342903	724092.355979	40.995226
3521.336244	723794.919822	41.000231
3520.926269	723505.916465	41.005236
3521.211024	723213.714914	41.010240
3521.232017	722919.712508	41.015245
3521.180868	722606.526986	41.020250
3521.341299	722296.269125	41.025255
3521.554700	721987.279881	41.030260
3521.343460	721670.119312	41.035264
3521.022904	721362.384904	41.040269
3521.093400	721038.708242	41.045274
3520.843184	720739.516819	41.050279
3520.995046	720420.066834	41.055284
3521.131541	720095.202082	41.060288
3520.852393	719785.716507	41.065293
3520.873931	719472.301630	41.070298
3520.909839	719146.573484	41.075303
3520.994984	718825.486443	41.080308
3520.656707	718502.869929	41.085312
3520.295793	718200.530675	41.090317
3520.463364	717867.390290	41.095322
3520.458451	717550.683680	41.100327
3520.116159	717230.895765	41.105332
3520.133205	716914.508733	41.110336
3519.809150	716608.831935	41.115341
3520.096811	716274.070578	41.120346
3519.950494	715969.432581	41.125351
3519.763319	715651.047254	41.130356
3519.806896	715338.813734	41.135360
3519.420197	715019.792514	41.140365
3519.401372	714699.060990	41.145370
3519.367788	714401.344032	41.150375
3519.545168	714078.125060	41.155380
3519.205835	713771.802009	41.160384
3518.871489	713462.489433	41.165389
3518.749835	713155.711095	41.170394
3518.424008	712854.365101	41.175399
3518.441577	712548.931446	41.180404
3518.347889	712257.501945	41.185408
3518.312384	711963.025057	41.190413
3517.994947	711656.473046	41.195418
3517.685700	711359.687538	41.200423
3517.723114	711069.188418	41.205428
3517.672660	710775.516792	41.210432
3517.699464	710492.942578	41.215437
3517.527058	710191.327916	41.220442
3517.260122	709916.527911	41.225447
3517.104059	709622.436870	41.230452
3517.026816	709350.119411	41.235456
3516.752616	709070.675884	41.240461
3516.086347	708785.279882	41.245466
3516.284302	708525.453178	41.250471
3516.365502	708250.790416	41.255476
3516.318959	707981.850724	41.260480
3516.286897	707725.861536	41.265485
3516.282249	707438.771919	41.270490
3515.999310	707189.860199	41.275495
3515.923086	706908.177990	41.280500
3515.889706	706639.839773	41.285504
3515.925428	706379.627328	41.290509
3515.634051	706118.070335	41.295514
3515.354871	705859.881017	41.300519
3515.245836	705609.653116	41.305524
3515.653377	705339.115320	41.310528
3515.272923	705104.266871	41.315533
3515.291668	704838.149072	41.320538
3515.032478	704584.240208	41.325543
3514.847930	704335.279535	41.330548
3514.603135	704075.540843	41.335552
3514.546372	703827.637452	41.340557
3514.634585	703585.068895	41.345562
3514.624673	703337.590917	41.350567
3514.275714	703101.987378	41.355572
3514.221242	702867.570987	41.360576
3514.168805	702632.352907	41.365581
3513.887398	702381.463994	41.370586
3513.841013	702159.251133	41.375591
3513.998482	701922.289645	41.380596
3513.904308	701681.834963	41.385600
3513.597406	701454.578305	41.390605
3513.947133	701221.740491	41.395610
3513.392037	700982.833637	41.400615
3513.413930	700759.231956	41.405620
3513.422411	700529.215286	41.410624
3512.959312	700313.634583	41.415629
3512.742465	700093.733334	41.420634
3512.540007	699881.379367	41.425639
3512.592400	699676.782028	41.430644
3512.755760	699453.720093	41.435648
3512.357825	699239.841949	41.440653
3512.131230	699030.801851	41.445658
3512.265400	698822.293692	41.450663
3512.347310	698606.232945	41.455668
3512.454517	698405.971612	41.460672
3512.041793	698207.332790	41.465677
3512.332703	697988.935467	41.470682
3511.829535	697789.407270	41.475687
3511.682935	697592.202093	41.480692
3511.684264	697386.068315	41.485696
3511.723450	697195.287055	41.490701
3511.447313	696990.234003	41.495706
3511.340538	696800.512477	41.500711
3511.513489	696615.414668	41.505716
3511.195612	696413.935223	41.510720
3511.364357	696219.232933	41.515725
3510.936283	696030.492757	41.520730
3511.165209	695840.794605	41.525735
3511.027072	695652.943292	41.530740
3511.210569	695456.431538	41.535744
3510.701124	695283.055456	41.540749
3510.864701	695085.096558	41.545754
3510.764140	694914.331231	41.550759
3510.444678	694728.628813	41.555764
3510.694266	694550.338488	41.560768
3510.587853	694374.092861	41.565773
3510.521573	694191.818907	41.570778
3510.144271	694022.673752	41.575783
3510.216812	693842.657652	41.580788
3510.326300	693670.242044	41.585792
3510.100637	693500.564499	41.590797
3509.918247	693321.077387	41.595802
3510.204159	693151.656849	41.600807
3509.895288	692980.888807	41.605812
3510.003868	692815.719425	41.610816
3509.962622	692647.686488	41.615821
3510.047460	692463.710576	41.620826
3509.957066	692307.867331	41.625831
3509.878593	692145.701325	41.630836
3509.577507	691969.987534	41.635840
3509.199592	691812.541424	41.640845
3509.485187	691654.684386	41.645850
3509.435443	691504.094048	41.650855
3509.171921	691335.376634	41.655860
3509.105405	691180.853132	41.660864
3508.520011	691023.128890	41.665869
3509.268326	690869.112172	41.670874
3509.111463	690715.839474	41.675879
3509.007584	690569.670706	41.680884
3508.904761	690413.099916	41.685888
3508.602476	690264.968641	41.690893
3508.683169	690110.750685	41.695898
3508.316011	689966.357195	41.700903
3508.161957	689828.395162	41.705908
3508.666178	689678.379283	41.710912
3508.434483	689543.610497	41.715917
3508.460918	689402.477029	41.720922
3508.181900	689259.202182	41.725927
3507.981913	689121.386187	41.730932
3508.129066	688978.633632	41.735936
3508.057285	688843.827940	41.740941
3507.977063	688705.836494	41.745946
3507.959500	688576.591823	41.750951
3507.999068	688450.122929	41.755956
3507.843684	688314.178443	41.760960
3507.624172	688182.473005	41.765965
3507.869290	688049.096181	41.770970
3507.827066	687913.525130	41.775975
3507.625775	687782.905837	41.780980
3507.814859	687665.957618	41.785984
3507.383270	687538.010832	41.790989
3507.376254	687400.285975	41.795994
3507.476914	687282.003481	41.800999
3507.646231	687151.313818	41.806004
3507.675193	687020.048139	41.811008
3507.427615	686900.872450	41.816013
3507.507622	686763.671079	41.821018
3507.331637	686645.575324	41.826023
3507.311478	686522.872546	41.831028
3507.232201	686403.015358	41.836032
3507.068794	686276.947859	41.841037
3507.072244	686147.167183	41.846042
3506.572190	686046.341650	41.851047
3506.722750	685923.204289	41.856052
3507.115944	685807.393143	41.861056
3506.493791	685698.220264	41.866061
3506.750692	685569.484700	41.871066
3506.413404	685467.231857	41.876071
3506.581639	685365.242824	41.881076
3506.660435	685261.176391	41.886080
3506.669869	685154.282359	41.891085
3506.651772	685030.413968	41.896090
3506.668121	684922.171794	41.901095
3506.509109	684808.032411	41.906100
3506.762428	684689.939857	41.911104
3506.362103	684590.276638	41.916109
3506.686700	684476.999203	41.921114
3506.362856	684379.810587	41.926119
3506.100279	684258.262501	41.931124
3506.545364	684158.703813	41.936128
3506.229723	684052.348497	41.941133
3506.037463	683948.809797	41.946138
3506.035857	683853.753248	41.951143
3505.906363	683751.297409	41.956148
3505.953610	683649.060191	41.961152
3505.575080	683559.092198	41.966157
3505.743774	683446.624475	41.971162
3505.631032	683363.781333	41.976167
3505.629473	683270.610992	41.981172
3505.811143	683163.914154	41.986176
3505.348809	683086.155872	41.991181
3505.713486	682988.440269	41.996186
3505.404527	682895.765099	42.001191
3505.292137	682802.608306	42.006196
3505.606849	682710.824200	42.011200
3505.170307	682625.288848	42.016205
3505.051347	682535.566692	42.021210
3505.030226	682452.799762	42.026215
3504.929879	682381.499721	42.031220
3505.187347	682286.135052	42.036224
3504.847796	682220.251991	42.041229
3504.990083	682129.536425	42.046234
3505.148677	682056.497738	42.051239
3505.097799	681971.540001	42.056244
3504.994061	681882.556004	42.061248
3504.746953	681795.288225	42.066253
3505.128562	681723.754006	42.071258
3504.866719	681639.575146	42.076263
3504.948217	681562.062693	42.081268
3504.884936	681482.531415	42.086272
3504.690486	681408.400349	42.091277
3504.805843	681317.731019	42.096282
3504.607906	681248.231389	42.101287
3504.679156	681170.269047	42.106292
3504.565244	681092.137406	42.111296
3504.275953	681017.271716	42.116301
3504.257696	680946.793728	42.121306
3504.450152	680881.460668	42.126311
3504.400828	680808.496230	42.131316
3504.492785	680729.480702	42.136320
3504.310708	680680.944691	42.141325
3503.941381	680602.801289	42.146330
3504.319577	680537.086407	42.151335
3504.214014	680477.279084	42.156340
3504.248343	680400.810704	42.161344
3503.863492	680337.711151	42.166349
3503.929928	680273.889008	42.171354
3504.094165	680212.839851	42.176359
3504.027105	680144.904307	42.181364
3504.062657	680082.231674	42.186368
3504.001213	680018.827417	42.191373
3504.199858	679948.355758	42.196378
3504.184249	679872.887561	42.201383
3503.876220	679825.762702	42.206388
3503.967360	679758.744677	42.211392
3503.738550	679701.792229	42.216397
3503.978997	679620.799801	42.221402
3504.134872	679576.984582	42.226407
3503.944175	679513.797484	42.231412
3503.844480	679443.470909	42.236416
3503.932499	679392.591836	42.241421
3504.019594	679327.464452	42.246426
3503.891413	679268.998138	42.251431
3503.529647	679206.136119	42.256436
3503.957952	679146.331578	42.261440
3503.696027	679083.800965	42.266445
3504.227541	679029.658113	42.271450
3503.985045	678972.902713	42.276455
3504.005548	678901.406270	42.281460
3503.816418	678839.758757	42.286464
3503.696084	678791.900099	42.291469
3503.781087	678721.138930	42.296474
3503.682755	678658.528584	42.301479
3503.781200	678606.198610	42.306484
3503.650949	678543.044706	42.311488
3503.660509	678485.846077	42.316493
3504.152623	678431.407300	42.321498
3503.946159	678372.549664	42.326503
3503.501696	678317.617281	42.331508
3503.458154	678253.500411	42.336512
3503.302867	678199.914631	42.341517
3503.514885	678149.606131	42.346522
3503.453376	678087.932519	42.351527
3503.400112	678041.155057	42.356532
3503.655081	677992.931292	42.361536
3503.204174	677932.765953	42.366541
3503.201907	677888.271305	42.371546
3503.101050	677841.550527	42.376551
3503.150058	677802.179157	42.381556
3503.453527	677737.851893	42.386560
3503.100874	677693.464041	42.391565
3503.532284	677635.144067	42.396570
3503.676632	677592.816203	42.401575
3503.125167	677534.060082	42.406580
3503.390611	677484.636061	42.411584
3503.150695	677433.102813	42.416589
3503.124552	677386.965348	42.421594
3503.453465	677341.466591	42.426599
3503.188453	677297.311507	42.431604
3503.380345	677239.676420	42.436608
3503.068274	677200.312339	42.441613
3502.796973	677152.320669	42.446618
3503.000031	677096.676072	42.451623
3503.016600	677051.028188	42.456628
3503.153206	677002.171035	42.461632
3502.562291	676960.808932	42.466637
3502.807813	676917.115817	42.471642
3502.972815	676877.073544	42.476647
3502.788947	676827.670450	42.481652
3503.100521	676787.902564	42.486656
3502.943145	676750.853141	42.491661
3503.008764	676704.896455	42.496666
3502.830692	676659.428312	42.501671
3502.675047	676620.733588	42.506676
3502.622742	676580.327281	42.511680
3502.351655	676554.508426	42.516685
3502.782543	676509.038581	42.521690
3502.556135	676463.776805	42.526695
3502.369998	676424.986636	42.531700
3502.820638	676384.147522	42.536704
3502.740096	676367.615739	42.541709
3502.379924	676308.870083	42.546714
3502.690374	676277.322989	42.551719
3502.668227	676251.212976	42.556724
3502.493255	676202.353279	42.561728
3502.508543	676162.233001	42.566733
3502.446139	676132.889977	42.571738
3502.505536	676090.818497	42.576743
3502.386056	676061.883371	42.581748
3502.726451	676018.220199	42.586752
3502.653087	675980.705294	42.591757
3502.159976	675954.173910	42.596762
3502.289898	675917.073687	42.601767
3502.296593	675888.017496	42.606772
3502.024799	675858.708211	42.611776
3501.865783	675836.207951	42.616781
3501.975104	675793.478990	42.621786
3502.472183	675777.149730	42.626791
3502.382780	675743.723231	42.631796
3502.490196	675723.770252	42.636800
3502.213242	675695.757100	42.641805
3502.337273	675659.105370	42.646810
3502.319996	675625.616690	42.651815
3502.538608	675590.743257	42.656820
3502.605490	675556.891550	42.661824
3502.517709	675527.201938	42.666829
3502.189911	675493.415224	42.671834
3502.476731	675455.938364	42.676839
3502.371081	675424.307632	42.681844
3502.558013	675382.660440	42.686848
3502.361396	675362.358212	42.691853
3502.329451	675328.272807	42.696858
3502.384706	675288.889772	42.701863
3502.439858	675252.596713	42.706868
3502.410898	675212.031093	42.711872
3502.218663	675202.044861	42.716877
3502.220121	675147.667968	42.721882
3502.236380	675137.049116	42.726887
3501.965702	675096.921673	42.731892
3502.233018	675062.586476	42.736896
3502.152060	675045.055581	42.741901
3501.833780	675006.630237	42.746906
3502.078297	674986.952080	42.751911
3501.867602	674956.682860	42.756916
3501.981093	674932.739802	42.761920
3501.783925	674906.754633	42.766925
3502.015058	674885.184455	42.771930
3501.870003	674855.552015	42.776935
3502.088862	674832.039872	42.781940
3502.103506	674803.327892	42.786945
3502.079138	674783.843272	42.791949
3501.884593	674747.689203	42.796954
3501.660213	674730.330948	42.801959
3501.429922	674704.649751	42.806964
3501.893166	674685.134188	42.811969
3501.736530	674668.811342	42.816973
3501.810318	674647.316463	42.821978
3501.680117	674626.802282	42.826983
3501.572664	674614.857491	42.831988
3501.968160	674580.947942	42.836993
3501.730636	674567.529257	42.841997
3501.970154	674531.950598	42.847002
3501.879048	674518.059043	42.852007
3501.921556	674489.839942	42.857012
3502.040289	674468.387069	42.862017
3502.088357	674443.805588	42.867021
3501.755248	674417.741834	42.872026
3501.990380	674398.263371	42.877031
3501.807656	674370.280512	42.882036
3501.861679	674344.501495	42.887041
3501.511337	674325.967011	42.892045
3501.739009	674304.096993	42.897050
3501.884784	674280.794927	42.902055
3501.588231	674259.659435	42.907060
3501.931013	674236.175163	42.912065
3501.777772	674232.312522	42.917069
3501.931410	674204.921582	42.922074
3502.158872	674180.110377	42.927079
3502.084202	674149.467139	42.932084
3501.881390	674127.468463	42.937089
3501.918368	674106.975361	42.942093
3501.847376	674077.278368	42.947098
3501.386124	674050.736296	42.952103
3501.824017	674041.591784	42.957108
3501.932347	674014.058232	42.962113
3501.691061	673995.255832	42.967117
3501.488963	673969.567957	42.972122
3501.497864	673952.817724	42.977127
3501.618559	673937.195484	42.982132
3501.858975	673918.512717	42.987137
3501.729849	673901.585811	42.992141
3501.825285	673874.353067	42.997146
3501.634957	673860.825870	43.002151
3501.390071	673852.043248	43.007156
3501.718370	673832.897153	43.012161
3501.676170	673800.004231	43.017165
3501.819136	673786.172605	43.022170
3501.782844	673756.718104	43.027175
3501.721002	673749.998782	43.032180
3501.994168	673708.429588	43.037185
3501.200140	673699.338780	43.042189
3501.492646	673679.649949	43.047194
3501.546073	673669.771027	43.052199
3501.452603	673652.289437	43.057204
3501.521718	673637.223564	43.062209
3501.671082	673621.197266	43.067213
3501.653317	673592.686327	43.072218
3501.829460	673575.209887	43.077223
3501.438241	673550.798358	43.082228
3501.599570	673533.922487	43.087233
3501.415291	673517.751750	43.092237
3501.481837	673489.625364	43.097242
3501.432459	673482.604690	43.102247
3501.178784	673490.074317	43.107252
3501.737294	673462.165649	43.112257
3501.328670	673444.237250	43.117261
3501.768017	673426.368085	43.122266
3501.658327	673397.273537	43.127271
3501.478687	673386.136716	43.132276
3501.872860	673368.574011	43.137281
3501.553514	673351.328591	43.142285
3501.672790	673340.790379	43.147290
3501.677968	673312.075392	43.152295
3501.347541	673293.037057	43.157300
3501.264433	673287.567196	43.162305
3501.020274	673286.161896	43.167309
3501.228904	673254.671295	43.172314
3501.430356	673249.054684	43.177319
3501.567225	673246.090868	43.182324
3501.534327	673220.622234	43.187329
3501.240723	673191.108776	43.192333
3501.393683	673180.066300	43.197338
3501.264531	673176.548203	43.202343
3501.241583	673171.865962	43.207348
3501.677548	673144.774233	43.212353
3501.752720	673145.310217	43.217357
3501.432821	673118.143916	43.222362
3501.541503	673087.466905	43.227367
3501.254753	673094.842606	43.232372
3501.381632	673069.197601	43.237377
3501.289220	673047.178143	43.242381
3501.244293	673035.370560	43.247386
3501.723993	673028.411670	43.252391
3501.321284	673007.390596	43.257396
3501.346319	672988.691721	43.262401
3501.140457	672985.335787	43.267405
3500.917813	672986.868200	43.272410
3501.473183	672976.756040	43.277415
3500.903309	672958.304976	43.282420
3501.234865	672938.458582	43.287425
3501.303458	672933.312416	43.292429
3501.213787	672938.113164	43.297434
3501.531168	672912.685515	43.302439
3500.947363	672904.257130	43.307444
3501.107656	672880.799631	43.312449
3501.275565	672886.554905	43.317453
3501.351435	672867.448561	43.322458
3501.637347	672846.014205	43.327463
3501.282980	672842.383640	43.332468
3501.538022	672821.751987	43.337473
3501.351934	672808.322276	43.342477
3501.496744	672787.459496	43.347482
3501.381061	672786.680987	43.352487
3501.073093	672774.368153	43.357492
3501.150355	672751.522300	43.362497
3500.968684	672741.182712	43.367501
3500.848215	672752.220404	43.372506
3501.301045	672736.740697	43.377511
3500.893874	672737.805102	43.382516
3501.077133	672715.739310	43.387521
3501.022895	672705.976875	43.392525
3501.186354	672687.503797	43.397530
3501.084851	672689.365218	43.402535
3500.854281	672687.259619	43.407540
3501.135489	672677.840555	43.412545
3501.083542	672669.822608	43.417549
3500.910537	672653.199826	43.422554
3500.860015	672637.155029	43.427559
3500.843252	672635.163649	43.432564
3500.832406	672622.253112	43.437569
3501.045724	672624.411503	43.442573
3501.151425	672622.050899	43.447578
3500.979345	672621.630679	43.452583
3500.920531	672622.388254	43.457588
3501.212552	672589.086873	43.462593
3501.339910	672583.581821	43.467597
3501.273214	672583.892008	43.472602
3501.105093	672575.843325	43.477607
3500.798350	672579.932303	43.482612
3501.191895	672575.380356	43.487617
3500.845220	672565.965233	43.492621
3501.198217	672542.973595	43.497626
3501.243123	672533.942425	43.502631
3500.697581	672547.742782	43.507636
3501.124142	672541.091447	43.512641
3500.939275	672542.767253	43.517645
3500.966750	672517.436301	43.522650
3500.705199	672488.264321	43.527655
3500.888441	672482.849686	43.532660
3501.029961	672471.210005	43.537665
3500.964724	672484.631947	43.542669
3501.016307	672485.371289	43.547674
3501.213586	672483.793204	43.552679
3501.062788	672477.536370	43.557684
3501.501713	672458.020209	43.562689
3501.253202	672452.776618	43.567693
3501.329377	672443.640482	43.572698
3501.187492	672435.288209	43.577703
3501.184202	672411.906429	43.582708
3501.490474	672390.268249	43.587713
3501.180604	672386.380872	43.592717
3500.996794	672379.281876	43.597722
3501.418879	672370.936057	43.602727
3501.121765	672348.699511	43.607732
3501.263449	672349.523686	43.612737
3501.309717	672341.688654	43.617741
3501.062780	672328.517593	43.622746
3501.211858	672298.579177	43.627751
3500.870648	672302.075694	43.632756
3501.003015	672290.935866	43.637761
3501.197274	672295.889445	43.642765
3500.789947	672286.434207	43.647770
3501.109736	672279.850191	43.652775
3500.521389	672293.957131	43.657780
3501.152746	672264.886181	43.662785
3501.176203	672265.530476	43.667789
3501.286500	672245.120907	43.672794
3501.350675	672244.711483	43.677799
3501.055513	672251.141954	43.682804
3501.273140	672225.579366	43.687809
3501.125327	672216.430169	43.692813
3500.945588	672209.031230	43.697818
3501.104488	672201.376895	43.702823
3500.647589	672218.453642	43.707828
3501.081562	672198.289623	43.712833
3501.013263	672199.397798	43.717837
3500.840483	672172.653160	43.722842
3501.365843	672167.580664	43.727847
3501.329612	672165.093830	43.732852
3501.201976	672142.978360	43.737857
3501.186349	672160.131860	43.742861
3500.821963	672121.802013	43.747866
3501.195980	672101.847126	43.752871
3500.914585	672111.217008	43.757876
3501.214642	672104.536416	43.762881
3501.050376	672104.015165	43.767885
3501.207914	672099.402278	43.772890
3501.193913	672079.860470	43.777895
3500.786581	672077.584513	43.782900
3501.006761	672061.194852	43.787905
3501.258680	672058.660371	43.792909
3500.874317	672062.662683	43.797914
3500.868882	672066.004081	43.802919
3500.964400	672067.334488	43.807924
3501.061413	672040.644604	43.812929
3501.035584	672031.524925	43.817933
3501.176144	672015.796496	43.822938
3501.292283	672011.639129	43.827943
3500.883514	672022.625602	43.832948
3501.250781	672003.768497	43.837953
3501.107846	671980.707872	43.842957
3501.152842	671973.820048	43.847962
3501.342781	671962.171737	43.852967
3500.914718	671962.292371	43.857972
3501.259308	671960.839430	43.862977
3501.077876	671939.380529	43.867981
3501.320611	671925.330247	43.872986
3501.422284	671921.574098	43.877991
3501.224072	671914.128121	43.882996
3501.394311	671898.095440	43.888001
3501.315958	671885.095331	43.893005
3501.267843	671883.009255	43.898010
3501.257846	671875.332709	43.903015
3501.065585	671857.564952	43.908020
3501.050589	671829.098064	43.913025
3501.057025	671828.797882	43.918029
3501.249445	671820.888405	43.923034
3501.335307	671816.636238	43.928039
3500.983890	671825.818538	43.933044
3501.236964	671793.168947	43.938049
3501.108681	671791.594691	43.943053
3501.190444	671784.750512	43.948058
3500.779303	671785.965252	43.953063
3500.927932	671788.982133	43.958068
3501.208206	671765.003436	43.963073
3501.032508	671745.288218	43.968077
3500.827419	671740.435926	43.973082
3501.005287	671732.080045	43.978087
3500.548618	671736.094443	43.983092
3501.097679	671726.081713	43.988097
3501.065613	671738.801203	43.993101
3500.997669	671728.940300	43.998106
3501.110871	671718.800154	44.003111
3500.969961	671692.996216	44.008116
3501.302551	671683.318372	44.013121
3501.257393	671688.162259	44.018125
3501.160808	671685.834851	44.023130
3500.918298	671661.393828	44.028135
3500.952763	671657.748401	44.033140
3501.267547	671641.142938	44.038145
3501.257838	671639.549060	44.043149
3501.160331	671647.094055	44.048154
3501.075283	671627.612910	44.053159
3500.857677	671613.688099	44.058164
3501.208407	671603.259275	44.063169
3500.967847	671607.487313	44.068173
3500.967161	671589.288510	44.073178
3500.916446	671591.141753	44.078183
3500.979304	671588.488810	44.083188
3501.073557	671596.301317	44.088193
3500.967986	671577.920384	44.093197
3500.885325	671563.624176	44.098202
3501.162315	671542.337914	44.103207
3501.014320	671558.567035	44.108212
3500.865224	671542.885685	44.113217
3501.016605	671538.472984	44.118221
3501.109510	671540.501945	44.123226
3500.989658	671531.696483	44.128231
3500.855684	671513.968305	44.133236
3500.939333	671502.636156	44.138241
3500.918993	671495.958223	44.143245
3500.928789	671499.696190	44.148250
3500.978326	671502.230933	44.153255
3500.465076	671501.667598	44.158260
3501.175489	671496.913190	44.163265
3500.982801	671496.745626	44.168269
3500.856372	671494.971570	44.173274
3500.777121	671472.248199	44.178279
3500.760501	671459.935353	44.183284
3500.926120	671460.356767	44.188289
3501.022200	671457.249549	44.193293
3500.837356	671452.044737	44.198298
3501.189528	671450.839771	44.203303
3500.802389	671455.790154	44.208308
3500.879789	671442.514390	44.213313
3500.983632	671443.295040	44.218317
3501.096446	671439.935747	44.223322
3500.929433	671414.235081	44.228327
3500.730642	671415.165468	44.233332
3501.017835	671408.087623	44.238337
3500.965431	671409.891319	44.243341
3500.809264	671410.465635	44.248346
3501.058076	671400.901070	44.253351
3500.859710	671409.011396	44.258356
3500.867938	671397.192973	44.263361
3500.863782	671410.008016	44.268365
3500.926395	671382.623899	44.273370
3501.331109	671360.169309	44.278375
3500.879354	671359.346495	44.283380
3501.223718	671363.777147	44.288385
3501.472318	671354.860769	44.293389
3501.157664	671342.247992	44.298394
3501.022756	671331.151201	44.303399
3501.202074	671325.487245	44.308404
3501.264247	671312.463123	44.313409
3501.311363	671318.339045	44.318413
3501.220489	671294.968968	44.323418
3501.005619	671273.314627	44.328423
3501.038491	671281.536434	44.333428
3501.086412	671264.675240	44.338433
3501.286785	671266.885948	44.343437
3500.829739	671263.321594	44.348442
3500.827509	671239.637559	44.353447
3500.900353	671242.068796	44.358452
3501.044981	671225.390999	44.363457
3500.824457	671231.211481	44.368461
3501.052669	671219.605792	44.373466
3500.871827	671222.029095	44.378471
3500.955902	671234.829796	44.383476
3501.086163	671226.880233	44.388481
3500.791457	671205.887138	44.393485
3500.839859	671197.751629	44.398490
3501.293709	671176.485178	44.403495
3501.006433	671180.421952	44.408500
3500.913656	671173.955211	44.413505
3501.039051	671178.920762	44.418509
3500.622024	671181.881730	44.423514
3500.758685	671168.147026	44.428519
3500.725424	671180.069668	44.433524
3500.765910	671170.888335	44.438529
3500.770576	671175.225627	44.443533
3500.666639	671176.539261	44.448538
3501.204674	671166.278452	44.453543
3500.850963	671147.638512	44.458548
3501.367321	671139.575208	44.463553
3500.992866	671128.567629	44.468557
3500.773864	671134.038880	44.473562
3500.822967	671140.163898	44.478567
3500.777227	671135.783586	44.483572
3501.027173	671124.174188	44.488577
3500.992929	671117.697735	44.493581
3501.062077	671106.168057	44.498586
3501.023451	671100.789297	44.503591
3500.900523	671088.493534	44.508596
3500.896043	671081.912413	44.513601
3501.066229	671086.172530	44.518605
3500.726600	671083.037468	44.523610
3500.918058	671066.152200	44.528615
3501.200342	671077.923099	44.533620
3500.948757	671052.235422	44.538625
3500.962312	671052.233217	44.543629
3500.871142	671063.218179	44.548634
3500.953478	671041.813369	44.553639
3500.687117	671051.879897	44.558644
3500.868010	671046.764008	44.563649
3501.253976	671047.498068	44.568653
3500.825364	671046.820989	44.573658
3501.256927	671032.588586	44.578663
3500.842774	671029.565548	44.583668
3501.121063	671005.984159	44.588673
3500.844401	671001.990988	44.593677
3500.929123	670998.486591	44.598682
3501.448411	670990.223224	44.603687
3501.152776	670994.111592	44.608692
3501.051533	670968.847614	44.613697
3501.297301	670964.219594	44.618701
3501.039144	670959.575122	44.623706
3501.327891	670952.097772	44.628711
3501.079865	670947.750801	44.633716
3501.550387	670922.741256	44.638721
3501.461430	670906.899318	44.643725
3500.876927	670913.228920	44.648730
3501.302203	670900.044496	44.653735
3501.291108	670882.294824	44.658740
3501.135422	670878.879976	44.663745
3501.195091	670868.997084	44.668749
3501.038076	670868.574291	44.673754
3501.035978	670853.166685	44.678759
3500.834846	670835.149145	44.683764
3501.071857	670821.945861	44.688769
3500.951081	670826.603229	44.693773
3501.329857	670825.842569	44.698778
3501.395435	670811.570589	44.703783
3501.406608	670803.440893	44.708788
3501.369396	670782.553896	44.713793
3501.223065	670775.397629	44.718797
3501.242365	670771.255721	44.723802
3501.214910	670752.212031	44.728807
3500.863840	670748.480372	44.733812
3500.692124	670734.796001	44.738817
3500.897038	670730.124754	44.743821
3500.700987	670733.099206	44.748826
3500.921202	670730.021101	44.753831
3501.058681	670730.696523	44.758836
3500.785804	670725.206667	44.763841
3501.112509	670722.160826	44.768845
3500.909422	670716.559702	44.773850
3500.755781	670689.508502	44.778855
3500.831589	670683.861269	44.783860
3500.903871	670686.492203	44.788865
3500.906444	670684.547079	44.793869
3500.840001	670694.580948	44.798874
3501.017998	670672.660844	44.803879
3500.881984	670687.692720	44.808884
3500.759064	670681.579677	44.813889
3500.992118	670685.131477	44.818893
3500.929744	670681.501676	44.823898
3501.029714	670656.851856	44.828903
3501.098320	670646.468604	44.833908
3501.482012	670641.518443	44.838913
3501.310356	670647.630398	44.843917
3500.947195	670633.528730	44.848922
3501.332384	670617.508220	44.853927
3501.200667	670600.924856	44.858932
3501.103007	670594.358794	44.863937
3501.164169	670593.949798	44.868941
3500.993956	670592.332402	44.873946
3501.199165	670552.655404	44.878951
3501.120706	670545.687210	44.883956
3501.266387	670544.366662	44.888961
3500.978907	670542.419577	44.893965
3500.880439	670549.466948	44.898970
3501.013988	670540.120026	44.903975
3501.173276	670529.921123	44.908980
3501.144132	670502.350155	44.913985
3501.364776	670502.862253	44.918989
3500.993058	670493.249722	44.923994
3501.162859	670492.224377	44.928999
3501.122090	670471.835940	44.934004
3501.014493	670464.024777	44.939009
3501.130910	670450.641440	44.944013
3500.913708	670463.492976	44.949018
3501.370894	670457.383653	44.954023
3501.031673	670456.891219	44.959028
3501.193684	670423.005291	44.964033
3501.135538	670416.881372	44.969037
3501.057202	670424.723372	44.974042
3501.007090	670411.317633	44.979047
3500.973305	670411.971515	44.984052
3501.183753	670408.695455	44.989057
3501.077570	670372.659544	44.994061
3500.719780	670364.440846	44.999066
3501.247046	670364.952146	45.004071
3500.880401	670370.149036	45.009076
3500.869351	670364.067167	45.014081
3501.134877	670357.540654	45.019085
3501.121150	670361.382692	45.024090
3501.149688	670331.507827	45.029095
3501.177062	670326.217453	45.034100
3500.998536	670315.026941	45.039105
3501.277413	670323.807330	45.044109
3501.448020	670325.474645	45.049114
3501.685899	670296.612278	45.054119
3501.283833	670289.946708	45.059124
3501.260588	670276.586206	45.064129
3501.549240	670257.190077	45.069133
3501.226773	670239.789858	45.074138
3501.147989	670234.616711	45.079143
3501.064498	670236.575370	45.084148
3501.174901	670213.069618	45.089153
3501.442431	670197.965458	45.094157
3501.168744	670192.724762	45.099162
3501.180531	670184.644301	45.104167
3501.283887	670179.640494	45.109172
3501.155235	670154.827677	45.114177
3501.250423	670160.895846	45.119181
3500.823223	670152.538830	45.124186
3501.025073	670156.095987	45.129191
3500.975105	670149.970544	45.134196
3500.816304	670141.170219	45.139201
3501.049086	670121.334235	45.144205
3500.824468	670104.017331	45.149210
3500.897680	670090.241681	45.154215
3500.984168	670102.644573	45.159220
3501.116996	670099.281498	45.164225
3501.260237	670091.877387	45.169229
3500.629832	670106.792414	45.174234
3501.067637	670093.205856	45.179239
3501.057264	670082.186752	45.184244
3500.912993	670063.759398	45.189249
3500.957178	670056.471365	45.194253
3500.948647	670055.375708	45.199258
3501.297537	670053.273486	45.204263
3500.909640	670041.768172	45.209268
3501.014308	670037.711573	45.214273
3501.274858	670015.576832	45.219277
3501.115891	670019.742222	45.224282
3501.243076	670004.062525	45.229287
3500.694635	670007.594124	45.234292
3501.000407	670002.357299	45.239297
3501.005564	670009.537553	45.244301
3500.858144	669990.013467	45.249306
3501.031868	669971.633119	45.254311
3501.139642	669966.129783	45.259316
3501.157986	669958.546732	45.264321
3500.993739	669949.846867	45.269325
3500.917623	669953.998594	45.274330
3501.054765	669953.227934	45.279335
3501.119653	669927.285421	45.284340
3501.074121	669920.959621	45.289345
3501.194368	669904.383264	45.294349
3501.159592	669914.362857	45.299354
3501.193821	669892.165492	45.304359
3501.268811	669889.061247	45.309364
3501.054731	669869.797275	45.314369
3500.965507	669861.533754	45.319373
3500.713316	669858.284091	45.324378
3501.227278	669860.692656	45.329383
3501.152869	669860.954335	45.334388
3501.043477	669855.536691	45.339393
3501.504738	669828.580888	45.344397
3501.485822	669825.940967	45.349402
3501.644497	669815.691528	45.354407
3501.243581	669784.788778	45.359412
3501.555849	669776.558572	45.364417
3501.290003	669769.870121	45.369421
3501.414775	669767.954485	45.374426
3501.527867	669728.638348	45.379431
3500.997684	669732.216899	45.384436
3500.866234	669720.120243	45.389441
3501.212507	669726.546158	45.394445
3500.858834	669703.614535	45.399450
3501.134910	669685.665550	45.404455
3500.979306	669690.279360	45.409460
3501.013011	669669.527796	45.414465
3501.206901	669673.734766	45.419469
3500.963189	669680.457693	45.424474
3501.415241	669665.172582	45.429479
3501.351060	669643.090637	45.434484
3501.122431	669641.632341	45.439489
3501.165644	669631.252173	45.444493
3501.259412	669629.690726	45.449498
3501.363827	669620.148231	45.454503
3501.411802	669612.659748	45.459508
3501.504123	669604.814837	45.464513
3501.162862	669585.571304	45.469517
3501.096645	669567.878146	45.474522
3501.171756	669557.093658	45.479527
3501.515815	669560.029089	45.484532
3501.288141	669552.885338	45.489537
3501.567872	669525.160738	45.494541
3501.527471	669513.996323	45.499546
3501.380142	669496.615663	45.504551
3501.428547	669475.761503	45.509556
3501.164909	669474.857551	45.514561
3501.360297	669463.753853	45.519565
3500.979185	669464.465198	45.524570
3501.075498	669435.573734	45.529575
3501.096222	669426.992434	45.534580
3501.422704	669417.762138	45.539585
3501.539599	669420.934640	45.544589
3501.672981	669406.300236	45.549594
3501.652307	669385.457293	45.554599
3501.316674	669388.006385	45.559604
3501.436494	669350.233593	45.564609
3501.475523	669332.173498	45.569613
3501.283605	669324.973793	45.574618
3501.234909	669317.900031	45.579623
3501.278362	669296.397957	45.584628
3501.286101	669285.973401	45.589633
3501.409718	669271.789254	45.594637
3501.430206	669266.499427	45.599642
3501.777872	669238.214166	45.604647
3501.222021	669248.081082	45.609652
3501.469273	669224.251028	45.614657
3501.486421	669206.742911	45.619661
3501.541022	669196.061148	45.624666
3501.316767	669182.433084	45.629671
3500.868485	669162.009426	45.634676
3500.945967	669156.759992	45.639681
3501.211815	669143.549609	45.644685
3501.104879	669135.388127	45.649690
3501.500411	669131.731932	45.654695
3501.093862	669120.777181	45.659700
3500.924903	669108.785688	45.664705
3501.354249	669095.298853	45.669709
3501.217479	669094.523517	45.674714
3501.106629	669092.945924	45.679719
3501.095217	669069.806583	45.684724
3500.825135	669067.257830	45.689729
3501.339733	669045.228466	45.694733
3501.022826	669044.183653	45.699738
3501.180991	669039.269936	45.704743
3500.996249	669047.280279	45.709748
3500.868226	669030.643678	45.714753
3501.103004	669004.520945	45.719757
3501.090655	669004.971886	45.724762
3501.271234	669000.004570	45.729767
3501.168558	669002.016527	45.734772
3500.962302	668998.609353	45.739777
3501.102663	668969.160578	45.744781
3501.130981	668972.547365	45.749786
3501.551120	668958.014503	45.754791
3501.243003	668957.018102	45.759796
3500.972722	668941.402334	45.764801
3501.487704	668915.532297	45.769805
3501.198825	668915.380574	45.774810
3500.791971	668888.914691	45.779815
3501.365091	668815.055458	45.784820
3501.101118	668697.294089	45.789825
3500.992572	668522.696589	45.794829
3500.285646	668292.332075	45.799834
3500.535765	668013.122024	45.804839
3500.365530	667669.876623	45.809844
3500.159787	667278.388119	45.814849
3499.994546	666817.386921	45.819853
3499.573346	666316.146327	45.824858
3499.543066	665742.922369	45.829863
3499.045438	665123.739089	45.834868
3498.651525	664440.330533	45.839873
3498.560249	663716.004099	45.844877
3498.087438	662923.615363	45.849882
3497.689244	662054.038584	45.854887
3497.196421	661141.372887	45.859892
3496.854890	660187.262934	45.864897
3496.370116	659157.447107	45.869901
3495.517912	658073.758364	45.874906
3495.059458	656935.953452	45.879911
3494.645553	655736.530383	45.884916
3494.034407	654465.966844	45.889921
3493.483698	653139.379800	45.894925
3492.464652	651767.426809	45.899930
3491.941849	650317.100385	45.904935
3490.973505	648835.451419	45.909940
3490.380031	647262.099771	45.914945
3489.746776	645648.314848	45.919949
3488.687767	643985.642089	45.924954
3487.782764	642249.058213	45.929959
3486.909877	640457.654108	45.934964
3486.044990	638600.050461	45.939969
3485.131896	636691.984093	45.944973
3483.967257	634730.259748	45.949978
3483.122710	632703.742522	45.954983
3482.090024	630629.853929	45.959988
3480.692762	628495.628106	45.964993
3479.781197	626293.728518	45.969997
3478.453128	624054.122903	45.975002
3477.376949	621741.906081	45.980007
3476.121384	619401.360393	45.985012
3474.772100	616986.789678	45.990017
3473.720167	614513.828337	45.995021
3471.985670	612005.472438	46.000026
3470.935645	609416.981963	46.005031
3469.333806	606802.297963	46.010036
3468.100340	604135.509534	46.015041
3466.811864	601395.873305	46.020045
3465.318121	598625.795498	46.025050
3463.921775	595787.091313	46.030055
3462.296714	592885.548015	46.035060
3460.387634	589947.464686	46.040065
3459.052868	586965.542499	46.045069
3456.897584	583930.334457	46.050074
3455.680485	580848.356241	46.055079
3454.221664	577707.804893	46.060084
3452.202018	574523.639258	46.065089
3450.678356	571280.663771	46.070093
3448.862522	567987.177647	46.075098
3447.058044	564642.396488	46.080103
3445.352046	561255.391846	46.085108
3443.005631	557825.910969	46.090113
3441.634260	554340.865989	46.095117
3439.785370	550835.494268	46.100122
3437.804525	547249.035375	46.105127
3435.832754	543636.431631	46.110132
3433.713879	539965.065954	46.115137
3431.880822	536254.157984	46.120141
3429.421559	532497.987197	46.125146
3427.746587	528689.232115	46.130151
3425.611326	524832.566283	46.135156
3423.417096	520960.528240	46.140161
3421.540717	517016.831894	46.145165
3419.318802	513029.593192	46.150170
3417.289742	508990.215013	46.155175
3415.082476	504925.278849	46.160180
3412.431488	500794.977866	46.165185
3409.912592	496626.298252	46.170189
3407.519994	492445.591144	46.175194
3405.553382	488193.151366	46.180199
3403.088622	483924.173040	46.185204
3400.535693	479600.774820	46.190209
3398.111974	475245.135074	46.195213
3395.327279	470840.414434	46.200218
3393.380641	466407.428988	46.205223
3390.484611	461928.790337	46.210228
3387.988106	457409.995158	46.215233
3385.522369	452850.999576	46.220237
3382.947590	448265.516453	46.225242
3380.456769	443624.203263	46.230247
3377.886002	438964.264373	46.235252
3374.898451	434263.949421	46.240257
3372.336821	429511.243811	46.245261
3369.257593	424749.854738	46.250266
3366.766597	419937.199512	46.255271
3364.120497	415099.222936	46.260276
3361.264878	410229.852884	46.265281
3358.451262	405314.377443	46.270285
3355.531999	400386.259712	46.275290
3352.646363	395403.090716	46.280295
3349.714292	390393.096201	46.285300
3346.821635	385360.296112	46.290305
3343.739568	380285.428245	46.295309
3340.342159	375196.774637	46.300314
3337.632825	370072.962222	46.305319
3334.933984	364930.932598	46.310324
3331.201429	359739.470580	46.315329
3328.257333	354550.720993	46.320333
3325.165825	349319.637098	46.325338
3321.777603	344066.340270	46.330343
3319.039149	338788.717227	46.335348
3315.712167	333481.554664	46.340353
3312.363581	328154.942520	46.345357
3309.164791	322808.476832	46.350362
3305.813281	317415.611393	46.355367
3302.377066	312008.975681	46.360372
3298.810518	306609.898437	46.365377
3295.463515	301165.628768	46.370381
3292.254212	295721.919469	46.375386
3288.649691	290247.525171	46.380391
3284.835827	284770.845818	46.385396
3281.234669	279264.856574	46.390401
3277.953614	273762.099822	46.395405
3274.103832	268237.830360	46.400410
3270.616169	262707.597351	46.405415
3267.258622	257151.334938	46.410420
3263.598797	251593.172851	46.415425
3260.001837	245999.195099	46.420429
3255.959873	240422.756431	46.425434
3252.123094	234825.590854	46.430439
3248.417526	229231.310922	46.435444
3244.513231	223613.938104	46.440449
3241.024270	217999.873478	46.445453
3236.720335	212375.461256	46.450458
3233.330354	206744.419978	46.455463
3229.173589	201049.283120	46.460468
3224.857750	195420.292948	46.465473
3221.285816	189777.263350	46.470477
3217.178932	184155.054373	46.475482
3212.740085	178524.900705	46.480487
3208.777428	172881.600627	46.485492
3204.745449	167262.387907	46.490497
3200.690068	161637.017513	46.495501
3196.220739	156034.088083	46.500506
3191.712285	150413.949159	46.505511
3187.384551	144810.841724	46.510516
3182.937599	139225.766411	46.515521
3179.025252	133651.570300	46.520525
3174.354771	128095.748057	46.525530
3169.974415	122539.139638	46.530535
3165.410695	117010.397133	46.535540
3160.888398	111492.186474	46.540545
3156.106244	105996.453059	46.545549
3151.101103	100508.797053	46.550554
3146.884752	95055.474974	46.555559
3141.847493	89611.100537	46.560564
3137.120994	84205.544263	46.565569
3132.101224	78821.555307	46.570573
3126.714439	73469.276615	46.575578
3121.521961	68149.410986	46.580583
3116.437077	62874.775367	46.585588
3110.655102	57646.285360	46.590593
3104.810729	52442.390568	46.595597
3098.309092	47320.927114	46.600602
3091.173557	42277.634649	46.605607
3077.843965	37463.383883	46.610612
3062.670540	32817.718834	46.615617
3048.183453	28354.150268	46.620621
3033.690577	24084.952718	46.625626
3020.298578	20026.089188	46.630631
3007.082832	16205.970696	46.635636
2993.959377	12618.990847	46.640641
2981.808037	9252.734803	46.645645
2969.238508	6126.937382	46.650650
2956.813250	3248.595532	46.655655
2937.725307	793.891756	46.660660
2859.268321	259.449538	46.665665
2790.325421	256.444145	46.670669
2760.703926	249.463695	46.675674
2763.245513	231.509011	46.680679
2783.717725	228.585307	46.685684
2806.902419	233.700844	46.690689
2825.668372	240.239689	46.695693
2835.827728	237.424227	46.700698
2838.562632	235.807735	46.705703
2836.499551	224.271853	46.710708
2831.855658	238.551183	46.715713
2827.216967	229.722008	46.720717
2822.484795	238.474915	46.725722
2819.230716	230.089511	46.730727
2816.447433	229.499964	46.735732
2813.513449	224.580515	46.740737
2811.264457	221.336564	46.745741
2808.159493	238.100257	46.750746
2805.323788	226.754626	46.755751
2802.906277	228.370774	46.760756
2799.651607	219.931025	46.765761
2797.019215	210.653011	46.770765
2793.769812	208.406033	46.775770
2790.753753	216.321592	46.780775
2787.134035	216.432718	46.785780
2783.492008	216.423612	46.790785
2780.739874	204.352587	46.795789
2777.693333	215.181159	46.800794
2774.380587	206.113850	46.805799
2771.247659	204.265374	46.810804
2767.358672	214.100675	46.815809
2764.295027	201.669579	46.820813
2760.990354	210.215660	46.825818
2757.810416	209.291409	46.830823
2754.532916	203.408439	46.835828
2750.937872	214.169353	46.840833
2748.037714	210.491924	46.845837
2743.997181	215.673661	46.850842
2740.679755	205.036154	46.855847
2737.677454	204.565597	46.860852
2734.627404	205.720123	46.865857
2731.272083	209.415576	46.870861
2727.308884	217.437036	46.875866
2723.671974	208.180505	46.880871
2720.494143	200.641984	46.885876
2716.939187	205.503798	46.890881
2713.909869	193.167317	46.895885
2710.343675	200.340429	46.900890
2706.604648	194.615794	46.905895
2703.251456	198.431288	46.910900
2700.437241	208.019070	46.915905
2696.669267	193.973191	46.920909
2692.956588	203.643395	46.925914
2689.760507	193.445650	46.930919
2686.362618	186.808322	46.935924
2682.601206	195.640416	46.940929
2679.627965	196.023505	46.945933
2676.176628	195.663633	46.950938
2673.018132	195.266141	46.955943
2669.381202	197.023441	46.960948
2665.834690	196.946724	46.965953
2662.929601	199.970553	46.970957
2659.148386	198.464508	46.975962
2655.464532	191.650171	46.980967
2651.640849	195.126419	46.985972
2648.114973	197.402898	46.990977
2644.914796	186.066057	46.995981
2641.587384	186.082148	47.000986
2638.169551	191.066756	47.005991
2634.906134	180.115733	47.010996
2630.814354	198.858540	47.016001
2627.934769	186.159507	47.021005
2624.181002	196.830941	47.026010
2620.781349	191.587157	47.031015
2617.646129	190.603907	47.036020
2613.671375	192.632474	47.041025
2610.350668	184.623574	47.046029
2606.842124	192.570446	47.051034
2603.073450	192.145557	47.056039
2600.472971	188.298252	47.061044
2596.237584	193.788052	47.066049
2593.037303	175.613567	47.071053
2589.341223	184.190412	47.076058
2585.836283	180.877665	47.081063
2582.594203	175.074825	47.086068
2579.187827	184.234797	47.091073
2575.943692	179.049176	47.096077
2572.303833	182.020067	47.101082
2568.891187	183.563897	47.106087
2565.056062	184.063713	47.111092
2561.434826	186.085301	47.116097
2558.050902	183.819540	47.121101
2554.858994	183.244343	47.126106
2551.146189	188.763695	47.131111
2547.915991	179.057771	47.136116
2544.002293	188.484302	47.141121
2541.140263	178.318609	47.146125
2537.540788	171.291112	47.151130
2533.658393	181.678031	47.156135
2530.380324	171.981433	47.161140
2526.796819	171.816237	47.166145
2523.247827	170.435658	47.171149
2520.005041	170.421256	47.176154
2516.280693	171.865182	47.181159
2513.077931	171.258070	47.186164
2509.173519	179.488019	47.191169
2506.324390	170.365711	47.196173
2502.045395	180.025623	47.201178
2498.722932	163.724263	47.206183
2495.484499	167.304229	47.211188
2492.067330	176.609113	47.216193
2488.834668	168.424525	47.221197
2485.220027	179.513471	47.226202
2481.695900	174.051251	47.231207
2478.361836	172.480016	47.236212
2474.552711	175.184194	47.241217
2471.432295	171.454842	47.246221
2467.663525	171.099751	47.251226
2463.830017	173.305952	47.256231
2460.307553	165.652851	47.261236
2457.092527	170.889750	47.266241
2453.862388	171.002757	47.271245
2450.156112	162.104918	47.276250
2446.500137	169.747352	47.281255
2443.234408	159.365027	47.286260
2439.625599	172.739173	47.291265
2436.194666	165.143162	47.296269
2432.687332	165.926853	47.301274
2429.027984	166.665074	47.306279
2425.882515	160.809272	47.311284
2421.912865	166.410131	47.316289
2419.047467	159.418465	47.321293
2415.378247	165.007664	47.326298
2411.763525	164.910882	47.331303
2408.424544	157.484380	47.336308
2404.803967	170.140419	47.341313
2401.291572	165.541452	47.346317
2397.561950	155.846549	47.351322
2393.991577	161.804199	47.356327
2390.892557	157.657557	47.361332
2387.111744	159.746367	47.366337
2383.851591	163.113730	47.371341
2380.019692	169.980220	47.376346
2376.786140	166.619555	47.381351
2373.022413	158.575512	47.386356
2369.457958	160.160031	47.391361
2366.336075	164.556308	47.396365
2363.023438	157.295191	47.401370
2359.735925	159.306669	47.406375
2355.735360	153.017506	47.411380
2352.209520	158.919269	47.416385
2348.828531	162.000602	47.421389
2345.401783	168.064156	47.426394
2341.524041	162.580117	47.431399
2338.286669	157.900337	47.436404
2334.743444	164.053243	47.441409
2331.172528	165.467379	47.446413
2328.056392	158.939015	47.451418
2324.503025	162.408265	47.456423
2320.865943	160.518918	47.461428
2317.128270	164.059350	47.466433
2313.550235	159.922838	47.471437
2310.278027	157.891965	47.476442
2306.705810	169.183777	47.481447
2303.381666	157.821021	47.486452
2300.133342	163.431377	47.491457
2296.821483	155.492539	47.496461
2292.810568	158.701532	47.501466
2289.178683	161.698567	47.506471
2285.672442	156.709343	47.511476
2282.232184	166.465554	47.516481
2278.859606	155.139853	47.521485
2275.296573	162.725387	47.526490
2271.974782	161.802902	47.531495
2268.120118	161.879188	47.536500
2264.679611	158.367202	47.541505
2261.493801	164.149569	47.546509
2258.048708	162.501590	47.551514
2254.099981	159.750654	47.556519
2250.681756	157.429856	47.561524
2247.428569	160.782747	47.566529
2244.253982	157.826435	47.571533
2240.520069	156.074166	47.576538
2236.806342	162.424506	47.581543
2233.334041	152.633469	47.586548
2229.752299	158.833881	47.591553
2226.285093	154.833210	47.596557
2222.846689	156.988978	47.601562
2219.338217	152.926082	47.606567
2215.939006	153.688490	47.611572
2212.146331	159.873338	47.616577
2208.845323	160.380906	47.621581
2205.666066	159.288442	47.626586
2201.854907	153.595587	47.631591
2198.407057	150.521975	47.636596
2195.050478	161.418007	47.641601
2191.378910	148.950014	47.646605
2187.844114	152.587583	47.651610
2184.033853	160.610587	47.656615
2181.149009	157.259610	47.661620
2177.337911	155.493939	47.666625
2174.045149	154.586459	47.671629
2170.626971	153.374351	47.676634
2166.902523	161.716848	47.681639
2163.413799	158.083880	47.686644
2159.579589	164.903378	47.691649
2156.164334	148.494799	47.696653
2152.676030	157.989103	47.701658
2149.152006	158.310280	47.706663
2146.332690	147.814215	47.711668
2142.621550	160.071628	47.716673
2139.101696	151.297535	47.721677
2135.376893	155.359716	47.726682
2131.791101	149.384111	47.731687
2128.404143	152.276372	47.736692
2124.791538	159.355188	47.741697
2121.463832	156.648316	47.746701
2117.834966	151.954052	47.751706
2114.022670	149.861262	47.756711
2110.819918	147.608488	47.761716
2107.553547	155.624524	47.766721
2103.706376	157.558026	47.771725
2100.265575	149.568107	47.776730
2096.824001	148.700933	47.781735
2093.481913	146.370814	47.786740
2089.598351	159.134976	47.791745
2086.583132	148.781527	47.796749
2082.938628	167.315639	47.801754
2079.064045	161.733064	47.806759
2076.012858	154.705348	47.811764
2072.223453	153.015906	47.816769
2068.869203	147.925724	47.821773
2065.182587	148.162022	47.826778
2061.489148	158.725798	47.831783
2058.675580	157.988447	47.836788
2054.683460	153.450135	47.841793
2051.087055	154.809727	47.846797
2047.722000	148.336653	47.851802
2044.464547	154.122160	47.856807
2041.192715	155.172829	47.861812
2037.394590	159.658490	47.866817
2033.702421	150.122523	47.871821
2030.293774	160.073773	47.876826
2026.932007	160.535706	47.881831
2023.357489	159.676413	47.886836
2019.879472	159.136603	47.891841
2016.470755	152.498319	47.896845
2012.666481	151.208040	47.901850
2008.985472	155.797259	47.906855
2006.028238	151.034240	47.911860
2002.350432	153.817122	47.916865
1998.723276	153.345061	47.921869
1995.497359	144.638633	47.926874
1991.675491	157.270105	47.931879
1988.519709	151.455644	47.936884
1984.501077	154.126295	47.941889
1981.348595	136.079502	47.946893
1977.712018	154.971310	47.951898
1974.065757	148.795513	47.956903
1970.952165	142.924351	47.961908
1967.294637	144.930350	47.966913
1964.082427	148.844985	47.971917
1960.338687	149.316988	47.976922
1956.724771	150.477097	47.981927
1953.358147	143.009408	47.986932
1949.754272	153.342345	47.991937
1946.567048	150.295225	47.996941
1942.988315	142.276018	48.001946
1939.357916	143.686529	48.006951
1935.719728	148.137287	48.011956
1932.099857	145.248899	48.016961
1929.087383	150.324139	48.021965
1925.157825	145.583193	48.026970
1921.596781	143.799415	48.031975
1918.443261	146.135350	48.036980
1914.736207	155.262729	48.041985
1910.854455	144.217714	48.046989
1907.613481	142.217317	48.051994
1904.137902	146.244512	48.056999
1901.075925	139.556769	48.062004
1897.295748	148.011328	48.067009
1893.715154	139.020014	48.072013
1890.568382	144.684279	48.077018
1886.685589	146.843516	48.082023
1883.397320	144.105249	48.087028
1879.360895	145.822073	48.092033
1875.855329	139.583986	48.097037
1872.831858	143.482011	48.102042
1869.705657	151.016378	48.107047
1866.112412	139.806581	48.112052
1862.156453	149.254873	48.117057
1858.649897	146.955760	48.122061
1855.088055	144.929058	48.127066
1851.773928	141.809710	48.132071
1848.223653	137.757039	48.137076
1844.649511	145.809465	48.142081
1841.488708	136.413753	48.147085
1838.114286	139.623253	48.152090
1834.315183	147.702119	48.157095
1831.089866	137.952434	48.162100
1826.980950	148.616624	48.167105
1823.407892	144.173476	48.172109
1820.167774	154.402416	48.177114
1816.212644	150.408782	48.182119
1813.409914	141.887135	48.187124
1809.430092	146.796790	48.192129
1806.313239	147.701978	48.197133
1802.920933	146.156740	48.202138
1799.006292	144.125614	48.207143
1795.708059	148.215065	48.212148
1792.243324	146.550219	48.217153
1788.643087	151.971617	48.222157
1785.196940	145.758099	48.227162
1781.866258	157.369211	48.232167
1778.242765	149.870055	48.237172
1774.577151	147.679078	48.242177
1771.320898	134.442548	48.247181
1767.841010	139.846972	48.252186
1764.108906	136.145185	48.257191
1761.066968	135.796560	48.262196
1756.826199	153.657350	48.267201
1753.420797	142.907101	48.272205
1750.277377	138.797145	48.277210
1746.540093	135.357702	48.282215
1743.320394	140.133131	48.287220
1739.789353	145.388585	48.292225
1736.725619	140.979691	48.297229
1732.496560	141.719619	48.302234
1728.733093	143.183748	48.307239
1725.503690	129.350221	48.312244
1722.000796	145.571417	48.317249
1718.772390	144.587730	48.322253
1715.333213	138.814955	48.327258
1711.414572	140.321596	48.332263
1707.976046	139.011234	48.337268
1704.339906	141.525605	48.342273
1701.412154	134.247852	48.347277
1697.750105	132.804451	48.352282
1694.084597	138.566686	48.357287
1690.796285	133.502022	48.362292
1687.124250	130.440767	48.367297
1683.461094	137.235269	48.372301
1679.953496	134.757509	48.377306
1676.217732	136.055477	48.382311
1673.495752	135.040365	48.387316
1670.123354	136.667243	48.392321
1666.028372	133.000451	48.397325
1662.342897	138.827591	48.402330
1658.903067	134.712978	48.407335
1655.620411	133.729062	48.412340
1651.987666	138.094106	48.417345
1648.596280	133.429789	48.422349
1645.201775	143.733377	48.427354
1641.241640	141.696334	48.432359
1638.259887	136.270288	48.437364
1634.382977	142.669096	48.442369
1630.774570	138.101552	48.447373
1627.400945	142.479110	48.452378
1624.038490	139.929383	48.457383
1621.104828	136.303154	48.462388
1617.148764	148.466203	48.467393
1613.542148	138.810713	48.472397
1610.265936	146.225482	48.477402
1606.560685	133.591221	48.482407
1603.165998	125.567493	48.487412
1599.472986	137.117035	48.492417
1596.131934	136.742548	48.497421
1592.787046	132.855961	48.502426
1589.218651	142.102887	48.507431
1585.582262	130.354906	48.512436
1581.819509	141.708434	48.517441
1578.362671	137.044177	48.522445
1574.665716	136.907107	48.527450
1571.364525	135.431816	48.532455
1568.280604	134.123166	48.537460
1564.145011	139.731389	48.542465
1561.096511	124.783284	48.547469
1557.254368	130.120066	48.552474
1553.852576	139.589613	48.557479
1550.762681	128.956569	48.562484
1547.246393	135.846417	48.567489
1543.722014	126.045947	48.572493
1540.213790	135.169661	48.577498
1536.328137	129.855293	48.582503
1532.843843	133.519363	48.587508
1529.094664	131.773648	48.592513
1526.329187	125.528223	48.597517
1522.509699	130.177914	48.602522
1518.910522	135.315196	48.607527
1515.801307	136.847649	48.612532
1511.710891	134.898448	48.617537
1508.337195	127.083658	48.622541
1505.007470	127.086644	48.627546
1501.360636	135.852520	48.632551
1498.181517	130.803269	48.637556
1494.289018	131.292475	48.642561
1490.708244	131.692895	48.647565
1487.544143	128.954505	48.652570
1483.776732	136.160340	48.657575
1480.616722	128.215223	48.662580
1477.068502	134.247681	48.667585
1473.508701	134.927220	48.672589
1469.836878	122.195417	48.677594
1466.386863	131.548899	48.682599
1463.085284	121.463517	48.687604
1459.206221	129.941150	48.692609
1455.854428	135.168492	48.697613
1452.508013	134.352001	48.702618
1449.096590	135.367682	48.707623
1445.478790	120.931458	48.712628
1441.760471	131.507730	48.717633
1438.267930	126.895111	48.722637
1434.918010	131.970210	48.727642
1431.100376	133.552327	48.732647
1428.034641	126.612232	48.737652
1424.340769	126.432758	48.742657
1420.647913	123.222081	48.747661
1417.497374	122.648812	48.752666
1413.826510	127.425899	48.757671
1410.840359	122.346499	48.762676
1406.780864	134.769789	48.767681
1403.133375	123.360692	48.772685
1399.375366	123.122023	48.777690
1396.248314	127.817028	48.782695
1393.217430	119.078216	48.787700
1389.832604	123.648242	48.792705
1386.171592	121.275325	48.797709
1382.375802	123.666680	48.802714
1378.605206	124.106576	48.807719
1375.390267	123.506528	48.812724
1371.734052	125.653139	48.817729
1368.206349	131.938224	48.822733
1364.786316	123.764808	48.827738
1360.772778	122.732455	48.832743
1358.094044	121.747293	48.837748
1354.439972	126.249919	48.842753
1350.680205	130.073099	48.847757
1347.637060	118.340448	48.852762
1343.733990	131.870933	48.857767
1340.452156	117.025284	48.862772
1337.028316	128.613858	48.867777
1333.697153	131.787779	48.872781
1329.869886	114.923511	48.877786
1325.967641	127.715057	48.882791
1322.599469	130.853685	48.887796
1318.995540	129.850918	48.892801
1315.676963	120.576376	48.897805
1312.267691	127.612843	48.902810
1308.602860	130.315644	48.907815
1305.453315	123.451519	48.912820
1301.585280	127.332168	48.917825
1297.878298	126.568119	48.922829
1294.691735	131.881252	48.927834
1291.193060	135.477660	48.932839
1287.922107	121.775969	48.937844
1284.338269	138.331952	48.942849
1280.700061	126.082382	48.947853
1277.567884	120.653564	48.952858
1273.424493	132.698984	48.957863
1270.501565	125.965425	48.962868
1266.785899	123.918209	48.967873
1263.359353	129.785817	48.972877
1259.578873	118.101950	48.977882
1256.275773	133.587814	48.982887
1252.712492	125.748473	48.987892
1248.893316	128.289860	48.992897
1245.861337	137.885957	48.997901
1242.181343	129.653559	49.002906
1238.740878	123.670891	49.007911
1235.557828	120.130145	49.012916
1231.631772	128.197430	49.017921
1228.024418	125.230472	49.022925
1224.364918	117.037324	49.027930
1220.776589	128.687213	49.032935
1217.798489	122.283715	49.037940
1214.160573	131.831955	49.042945
1210.820356	127.565659	49.047949
1207.570597	119.512937	49.052954
1203.778961	117.788988	49.057959
1200.512045	115.529259	49.062964
1196.378477	127.229758	49.067969
1192.752538	119.941962	49.072973
1189.761711	120.849608	49.077978
1185.483551	118.296489	49.082983
1182.849163	112.928436	49.087988
1179.650590	121.827601	49.092993
1175.506428	120.604978	49.097997
1172.272889	123.658049	49.103002
1168.414733	124.935748	49.108007
1165.274099	113.177605	49.113012
1161.758891	128.602617	49.118017
1158.129752	122.585024	49.123021
1155.026204	123.170209	49.128026
1150.927770	128.057735	49.133031
1147.825737	114.976204	49.138036
1144.021411	122.544246	49.143041
1140.450103	124.046108	49.148045
1137.268820	120.679594	49.153050
1133.559628	127.367351	49.158055
1130.073990	117.089247	49.163060
1126.532775	121.276166	49.168065
1123.245751	121.948650	49.173069
1119.592985	111.348024	49.178074
1116.387473	112.831247	49.183079
1112.977309	118.931476	49.188084
1108.948638	123.321042	49.193089
1105.268772	125.655537	49.198093
1101.901100	121.164793	49.203098
1098.723443	124.118471	49.208103
1095.288026	117.946059	49.213108
1091.411555	127.377692	49.218113
1088.115282	117.853594	49.223117
1084.842103	111.962311	49.228122
1081.030253	122.398307	49.233127
1077.777635	122.957179	49.238132
1073.940531	120.199776	49.243137
1070.228209	116.155982	49.248141
1067.154117	119.569254	49.253146
1063.667762	118.317719	49.258151
1060.254614	118.772214	49.263156
1056.683798	122.911023	49.268161
1052.967143	124.541668	49.273165
1049.435005	125.835833	49.278170
1045.780138	117.862520	49.283175
1042.615892	116.000486	49.288180
1039.044614	120.259957	49.293185
1035.435911	117.778451	49.298189
1032.020826	120.396845	49.303194
1027.886967	127.135232	49.308199
1025.266438	107.562789	49.313204
1021.440038	123.549248	49.318209
1018.212521	116.636553	49.323213
1014.968799	118.321952	49.328218
1010.685453	125.905079	49.333223
1007.411548	103.731114	49.338228
1004.011439	118.824954	49.343233
1000.576486	109.471562	49.348237
997.337392	111.539230	49.353242
993.362748	113.024290	49.358247
989.724645	115.443324	49.363252
986.146898	117.341255	49.368257
982.561174	128.225844	49.373261
979.672800	112.328998	49.378266
975.789138	114.224623	49.383271
972.610940	114.725057	49.388276
969.331928	110.518486	49.393281
965.655010	118.762324	49.398285
962.532430	114.682335	49.403290
958.342675	114.912775	49.408295
954.751446	105.966414	49.413300
951.341476	110.601550	49.418305
947.897109	116.281351	49.423309
944.379624	113.025264	49.428314
940.621488	110.545367	49.433319
937.372742	101.973161	49.438324
933.865451	113.909171	49.443329
930.464636	109.782051	49.448333
926.973162	114.642471	49.453338
923.539041	116.112486	49.458343
919.860629	114.128494	49.463348
916.465290	114.145831	49.468353
912.657223	118.946922	49.473357
909.352233	106.414937	49.478362
905.785771	118.247525	49.483367
902.553107	117.085061	49.488372
899.171066	117.351015	49.493377
895.452248	115.949568	49.498381
891.933422	119.215972	49.503386
887.853043	120.982523	49.508391
884.602800	120.663034	49.513396
881.419680	118.310938	49.518401
877.807820	120.902727	49.523405
874.880966	115.919895	49.528410
870.717760	115.515942	49.533415
867.497181	103.284341	49.538420
863.723432	120.240755	49.543425
860.357293	118.078696	49.548429
856.813749	113.539427	49.553434
853.140500	115.809910	49.558439
849.919856	114.431983	49.563444
846.009465	114.875469	49.568449
842.992595	108.102414	49.573453
839.705820	111.664626	49.578458
835.746900	112.405269	49.583463
832.115576	108.254540	49.588468
828.784631	101.946255	49.593473
825.193830	106.026817	49.598477
821.926592	104.702431	49.603482
818.097804	110.693604	49.608487
814.795047	109.208768	49.613492
811.333409	115.977665	49.618497
807.736587	117.386187	49.623501
804.924796	119.209627	49.628506
801.065668	117.885238	49.633511
797.346736	120.159805	49.638516
793.585027	115.727851	49.643521
790.008249	128.191542	49.648525
786.755995	118.950898	49.653530
783.235442	116.951293	49.658535
779.900478	114.472545	49.663540
776.514811	113.756301	49.668545
773.193748	112.045043	49.673549
769.574087	107.432065	49.678554
765.598942	120.440431	49.683559
762.289669	118.809908	49.688564
758.658828	113.216675	49.693569
754.809837	110.273518	49.698573
751.912445	113.151736	49.703578
748.000801	121.887410	49.708583
744.841858	109.454477	49.713588
741.252937	111.077629	49.718593
737.455375	115.073211	49.723597
734.281028	110.091920	49.728602
730.684447	113.399594	49.733607
727.261881	108.529571	49.738612
723.950656	113.691955	49.743617
720.064256	111.250940	49.748621
716.596371	106.321556	49.753626
713.161927	113.304859	49.758631
709.470927	113.122829	49.763636
706.189753	112.194927	49.768641
702.453262	117.572184	49.773645
699.658964	108.296642	49.778650
695.829507	113.790767	49.783655
692.153960	102.128992	49.788660
688.739207	108.363724	49.793665
685.267153	114.230478	49.798669
681.872605	108.957237	49.803674
678.030594	105.880198	49.808679
674.587592	101.366647	49.813684
671.112613	103.447896	49.818689
667.622221	106.887572	49.823693
664.215814	101.531862	49.828698
660.641142	110.208505	49.833703
657.335929	109.638453	49.838708
653.876059	107.769002	49.843713
649.793576	108.408008	49.848717
646.436636	93.650144	49.853722
642.781191	108.696648	49.858727
639.615732	110.344303	49.863732
636.509011	111.629379	49.868737
632.712348	111.990264	49.873741
629.341024	108.325612	49.878746
625.822435	110.778417	49.883751
622.110699	103.700816	49.888756
618.493776	109.191888	49.893761
615.024883	114.332985	49.898765
611.577315	113.525343	49.903770
608.094462	115.534353	49.908775
604.523857	112.448040	49.913780
601.207037	109.326103	49.918785
597.438420	113.358649	49.923789
593.947100	104.457247	49.928794
590.595932	116.388128	49.933799
587.734634	113.418084	49.938804
583.965912	106.051818	49.943809
580.159708	109.822251	49.948813
576.510158	109.421533	49.953818
573.323711	113.343814	49.958823
569.458960	109.822722	49.963828
565.741552	110.306474	49.968833
562.402308	108.044911	49.973837
559.135341	107.444520	49.978842
555.384410	105.924426	49.983847
551.735770	101.742914	49.988852
548.624158	103.404789	49.993857
544.840391	101.732491	49.998861
541.879520	104.516818	50.003866
537.950672	117.731607	50.008871
534.795033	107.267500	50.013876
531.226440	106.005056	50.018881
527.429645	111.532395	50.023885
524.183369	95.155136	50.028890
519.962750	109.424185	50.033895
516.938493	102.811495	50.038900
513.266967	107.667048	50.043905
509.568118	105.397175	50.048909
506.596104	108.869304	50.053914
502.812396	111.714145	50.058919
499.354112	112.162624	50.063924
496.226047	103.395760	50.068929
492.796874	109.853864	50.073933
489.423326	114.208460	50.078938
485.517131	110.597648	50.083943
482.220606	113.171963	50.088948
478.380795	109.535137	50.093953
474.439973	118.460417	50.098957
471.449743	102.945245	50.103962
468.272490	112.694451	50.108967
464.808466	103.701428	50.113972
460.979187	100.855158	50.118977
457.096488	109.658515	50.123981
454.106088	102.219557	50.128986
450.580042	111.182130	50.133991
447.115434	104.739134	50.138996
443.532200	109.560157	50.144001
439.852844	110.272142	50.149005
436.231022	114.775171	50.154010
432.832838	106.170050	50.159015
429.363993	108.933461	50.164020
425.992639	105.942693	50.169025
422.435946	120.478669	50.174029
418.715237	102.818137	50.179034
415.285494	109.776240	50.184039
411.923254	101.715726	50.189044
408.290609	108.963672	50.194049
404.899772	104.303189	50.199053
401.486178	99.687931	50.204058
397.749928	106.269935	50.209063
394.481446	104.098793	50.214068
390.860035	111.198075	50.219073
387.138142	114.447355	50.224077
384.353342	108.015817	50.229082
380.136858	108.932521	50.234087
377.003142	103.253751	50.239092
373.270156	114.177306	50.244097
369.713477	109.891706	50.249101
366.418559	106.706357	50.254106
362.733200	108.006080	50.259111
359.329634	101.308737	50.264116
356.014432	108.539912	50.269121
352.761385	109.617267	50.274125
349.223192	96.196154	50.279130
345.198815	101.485207	50.284135
341.926436	101.155460	50.289140
338.028539	104.962475	50.294145
334.307999	106.793955	50.299149
331.092368	108.071916	50.304154
327.812009	114.810514	50.309159
324.410916	99.354467	50.314164
320.714774	110.700745	50.319169
317.179239	107.053208	50.324173
314.082040	106.779236	50.329178
310.164165	114.336909	50.334183
306.705865	102.032481	50.339188
303.459129	103.927357	50.344193
300.112580	106.928873	50.349197
296.673671	101.352777	50.354202
293.003086	108.128997	50.359207
289.140731	109.005125	50.364212
285.644536	99.799583	50.369217
281.761885	108.032417	50.374221
279.121806	102.897658	50.379226
275.183640	118.132729	50.384231
271.598041	99.746247	50.389236
268.409932	103.945311	50.394241
264.919368	106.670644	50.399245
261.393967	106.368600	50.404250
257.604099	102.674185	50.409255
254.222329	100.022351	50.414260
250.976317	103.301820	50.419265
247.056317	103.505594	50.424269
243.848006	101.950326	50.429274
240.108052	103.739344	50.434279
236.606294	98.429687	50.439284
233.269212	101.867761	50.444289
229.579300	108.380066	50.449293
226.340161	100.365389	50.454298
222.731074	96.456669	50.459303
219.216178	94.349321	50.464308
216.034317	96.006168	50.469313
211.731056	105.368420	50.474317
208.666333	99.699653	50.479322
205.464028	102.926512	50.484327
201.833481	97.711302	50.489332
198.370362	108.528404	50.494337
194.570097	105.162365	50.499341
191.175948	106.888645	50.504346
187.939484	103.284881	50.509351
184.212949	103.225502	50.514356
180.743938	102.755315	50.519361
177.056240	102.859391	50.524365
173.905013	98.907793	50.529370
170.194036	97.463150	50.534375
166.375946	98.113999	50.539380
163.014145	91.606851	50.544385
159.425195	111.934310	50.549389
156.224124	103.849240	50.554394
152.695396	109.470921	50.559399
149.208597	109.473760	50.564404
145.766290	106.996265	50.569409
142.235713	107.129322	50.574413
138.763496	107.079034	50.579418
135.025354	101.666682	50.584423
131.509904	94.546733	50.589428
128.208843	104.985515	50.594433
124.666812	105.789640	50.599437
121.247462	102.175481	50.604442
117.346895	100.489096	50.609447
113.708368	99.707734	50.614452
110.710472	97.333033	50.619457
107.190224	104.001167	50.624461
103.808290	102.974515	50.629466
100.328859	100.371418	50.634471
96.997538	96.930120	50.639476
93.165218	102.504428	50.644481
89.449842	103.717452	50.649485
86.223096	99.526097	50.654490
82.183539	96.754050	50.659495
78.965450	93.702030	50.664500
75.632992	100.286886	50.669505
71.897376	108.495881	50.674509
69.029363	99.731194	50.679514
64.892154	104.152290	50.684519
61.335505	101.359604	50.689524
58.004922	105.952513	50.694529
54.364992	103.500058	50.699533
51.074319	102.085335	50.704538
47.671015	98.131937	50.709543
44.278918	98.044152	50.714548
40.739061	94.725575	50.719553
36.600648	105.219535	50.724557
33.388531	99.549571	50.729562
30.122593	112.977081	50.734567
26.752990	104.235411	50.739572
23.241699	93.296351	50.744577
19.193291	112.295883	50.749581
15.797206	103.171464	50.754586
12.381927	108.237678	50.759591
9.110351	104.662212	50.764596
5.478609	98.753002	50.769601
2.162479	106.736448	50.774605