Fri Jun 17 18:20:27 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.168410	86.117663	0.000000
-0.034717	95.974552	0.005005
0.356475	94.750652	0.010010
0.080773	94.941357	0.015014
0.239274	85.158860	0.020019
-0.122908	76.972881	0.025024
-0.486960	72.895425	0.030029
-0.257024	70.678529	0.035034
-0.934936	64.271670	0.040038
-0.763821	54.198600	0.045043
-0.911973	49.986600	0.050048
-1.592918	40.842309	0.055053
-1.429222	25.738988	0.060058
-1.934271	25.074109	0.065062
-2.408467	13.710839	0.070067
-2.726970	3.791207	0.075072
-2.836477	11.848432	0.080077
-2.627585	9.292085	0.085082
-3.325709	9.599373	0.090086
-3.609761	-14.235685	0.095091
-3.900474	-1.817773	0.100096
-4.513125	-9.467964	0.105101
-4.932679	-6.314730	0.110106
-5.299817	-2.509551	0.115110
-5.196567	-6.101875	0.120115
-5.368524	-16.028289	0.125120
-5.582723	-6.930721	0.130125
-5.198232	-9.823098	0.135130
-5.842727	-3.988469	0.140134
-6.664094	-15.664200	0.145139
-6.408899	-7.678457	0.150144
-6.811188	-8.347391	0.155149
-6.721840	-12.250563	0.160154
-7.928462	3.151451	0.165158
-7.995481	-10.416549	0.170163
-8.464911	6.434464	0.175168
-8.553530	2.307695	0.180173
-7.950535	-0.864111	0.185178
-8.614202	-2.329629	0.190182
-8.444446	-11.631860	0.195187
-8.452996	-2.459744	0.200192
-9.619838	3.088561	0.205197
-9.799957	0.751580	0.210202
-10.301962	-9.911464	0.215206
-10.596610	0.829809	0.220211
-10.459584	-0.673090	0.225216
-10.389288	-0.593568	0.230221
-10.213494	-5.648712	0.235226
-10.739043	-6.475542	0.240230
-11.506820	-10.314589	0.245235
-11.653233	-3.110210	0.250240
-11.939433	-8.993906	0.255245
-11.777676	-12.560829	0.260250
-12.658993	1.886902	0.265254
-13.277691	-11.544212	0.270259
-13.083921	-0.139008	0.275264
-13.571565	-1.924251	0.280269
-13.228314	-15.088033	0.285274
-13.401766	0.550130	0.290278
-13.213042	-4.325226	0.295283
-13.859800	-5.539788	0.300288
-14.659930	-2.124782	0.305293
-14.340352	-23.443180	0.310298
-14.649212	-1.685849	0.315302
-14.626668	-0.390738	0.320307
-15.463139	-10.806778	0.325312
-16.348995	-16.566725	0.330317
-16.119916	-13.689231	0.335322
-16.654711	-3.667760	0.340326
-16.401786	-5.981212	0.345331
-16.166032	-9.391127	0.350336
-16.414930	-9.261313	0.355341
-16.866181	-11.626632	0.360346
-17.619204	-7.154079	0.365350
-17.959867	-11.523301	0.370355
-17.517070	-5.833087	0.375360
-17.726421	-12.350746	0.380365
-18.145185	-15.767305	0.385370
-19.040067	-6.233768	0.390374
-18.963883	-12.211440	0.395379
-18.886484	-14.286744	0.400384
-19.449803	-16.535953	0.405389
-19.647668	-13.021162	0.410394
-20.399560	-10.881420	0.415398
-20.296587	-6.094529	0.420403
-20.858447	-20.115818	0.425408
-20.731889	-12.787311	0.430413
-20.802741	-11.926389	0.435418
-20.950295	-3.619346	0.440422
-20.991991	-6.425099	0.445427
-21.449153	0.184089	0.450432
-22.305736	-7.456927	0.455437
-22.341355	-15.960962	0.460442
-22.248973	-5.336119	0.465446
-22.308921	-10.788765	0.470451
-22.612667	-5.051027	0.475456
-23.540608	-1.850189	0.480461
-23.897867	-0.829577	0.485466
-23.948723	-6.980109	0.490470
-24.013477	5.057094	0.495475
-23.821984	-2.753989	0.500480
-24.121177	-2.316270	0.505485
-24.227544	-11.755725	0.510490
-24.999881	-0.297681	0.515494
-25.320919	-3.757323	0.520499
-25.136423	-6.710980	0.525504
-25.468151	-1.629048	0.530509
-25.739109	-4.733929	0.535514
-26.498408	-3.770217	0.540518
-26.872058	-4.061485	0.545523
-26.809588	0.847182	0.550528
-27.180896	-7.456417	0.555533
-27.097844	-14.913615	0.560538
-27.053093	-2.613822	0.565542
-26.934502	-1.720651	0.570547
-27.737425	-7.694080	0.575552
-28.768678	-1.332819	0.580557
-28.316391	-10.065952	0.585562
-28.167897	1.336317	0.590566
-28.792667	-5.038887	0.595571
-29.414709	-3.423914	0.600576
-30.204022	-5.120926	0.605581
-30.434799	-10.087965	0.610586
-29.995658	-3.693076	0.615590
-29.994079	-0.617930	0.620595
-30.099084	-7.011647	0.625600
-30.487207	-1.946389	0.630605
-30.229806	-13.944292	0.635610
-31.093135	-6.191560	0.640614
-31.500127	-1.558868	0.645619
-31.584670	-5.782607	0.650624
-32.017740	-4.374075	0.655629
-32.039841	-9.435591	0.660634
-32.723782	-4.597029	0.665638
-33.009521	-4.425965	0.670643
-33.139151	-11.778550	0.675648
-33.347990	-4.688706	0.680653
-33.500709	-8.953206	0.685658
-33.562313	-0.726751	0.690662
-33.562312	-1.321855	0.695667
-34.056063	-14.493323	0.700672
-34.965519	-8.903737	0.705677
-34.829930	-18.782600	0.710682
-35.042615	-4.586906	0.715686
-34.922081	-5.053062	0.720691
-35.027551	0.746439	0.725696
-35.607475	-6.560505	0.730701
-36.099632	-10.336434	0.735706
-36.396721	-10.820193	0.740710
-36.351363	-2.634211	0.745715
-36.376346	-4.603306	0.750720
-36.855184	-1.766004	0.755725
-37.362203	-10.766107	0.760730
-38.028865	1.414356	0.765734
-38.299071	-13.005277	0.770739
-37.953828	-4.387268	0.775744
-38.216350	-7.486445	0.780749
-38.041873	-7.400364	0.785754
-37.900784	-8.075750	0.790758
-38.605836	0.401315	0.795763
-39.328569	-12.169310	0.800768
-39.668830	1.100022	0.805773
-39.411775	-10.393255	0.810778
-39.808989	-1.727409	0.815782
-40.299204	-7.789911	0.820787
-40.823329	-0.743164	0.825792
-41.103215	-4.634492	0.830797
-41.222673	-11.762431	0.835802
-41.536481	-3.805047	0.840806
-41.444356	-3.330747	0.845811
-41.423608	-3.785842	0.850816
-41.493875	-0.290875	0.855821
-41.881834	-5.639666	0.860826
-42.679752	1.644001	0.865830
-42.933984	-12.090596	0.870835
-42.924750	-12.960140	0.875840
-43.281205	2.212357	0.880845
-43.108426	-6.618170	0.885850
-43.876704	1.372138	0.890854
-44.270867	3.198264	0.895859
-44.299414	-10.591411	0.900864
-44.558481	2.777496	0.905869
-44.448251	-8.556996	0.910874
-44.369716	-5.993490	0.915878
-45.076544	-3.394946	0.920883
-45.710362	-6.170944	0.925888
-46.232679	2.627586	0.930893
-46.121340	-3.371915	0.935898
-46.113646	6.702649	0.940902
-46.295783	-7.187393	0.945907
-46.505850	-1.720963	0.950912
-47.104268	-1.993022	0.955917
-47.544248	-6.957451	0.960922
-47.725653	0.050285	0.965926
-47.760438	1.454576	0.970931
-47.566276	1.996568	0.975936
-48.021667	3.163139	0.980941
-48.362392	-3.887176	0.985946
-48.749011	4.065740	0.990950
-49.011574	-1.816358	0.995955
-49.028940	-0.014188	1.000960
-49.459829	5.172830	1.005965
-49.629699	-5.610732	1.010970
-50.669141	-2.584933	1.015974
-50.837828	-6.867696	1.020979
-50.509986	-10.831626	1.025984
-50.908776	-2.926811	1.030989
-50.838035	-6.418619	1.035994
-50.998914	-4.671328	1.040998
-51.050500	-7.469516	1.046003
-50.795062	-6.333884	1.051008
-52.045954	-5.656470	1.056013
-52.270288	-9.497634	1.061018
-52.098904	-5.703827	1.066022
-52.571710	-17.039864	1.071027
-53.377789	-6.561672	1.076032
-54.011141	-9.676361	1.081037
-53.854125	-4.207016	1.086042
-53.979203	-6.632468	1.091046
-54.006028	-8.356963	1.096051
-53.838229	-3.280910	1.101056
-54.089239	-3.692410	1.106061
-54.086094	-6.179825	1.111066
-55.146334	-2.214441	1.116070
-55.497536	3.443180	1.121075
-55.392509	-9.904382	1.126080
-55.858217	-2.003638	1.131085
-55.600294	-11.660125	1.136090
-56.482368	-2.734706	1.141094
-56.871724	-5.275472	1.146099
-57.296939	-3.233042	1.151104
-57.172239	-0.467844	1.156109
-57.131729	-7.587250	1.161114
-57.346547	-8.934578	1.166118
-57.275686	-3.363692	1.171123
-57.830205	-8.224031	1.176128
-58.532387	-2.375267	1.181133
-58.657206	-11.564989	1.186138
-58.868539	-0.968200	1.191142
-59.117711	-5.748072	1.196147
-58.999966	-3.926725	1.201152
-59.620620	-1.374865	1.206157
-59.867660	-10.020364	1.211162
-60.423668	1.737973	1.216166
-60.575596	-1.772074	1.221171
-60.531755	-4.373404	1.226176
-60.654195	-11.106583	1.231181
-60.575865	-5.374933	1.236186
-60.566510	-2.920693	1.241190
-61.493050	-3.118079	1.246195
-61.800027	-3.857115	1.251200
-62.083927	-4.484352	1.256205
-62.134834	-8.624092	1.261210
-62.280078	4.208498	1.266214
-63.049701	-5.720781	1.271219
-63.179020	-2.985186	1.276224
-63.597844	-6.455404	1.281229
-63.444782	-5.533235	1.286234
-63.695430	-10.617536	1.291238
-64.017209	-2.317447	1.296243
-63.627337	-1.129375	1.301248
-64.687381	6.456766	1.306253
-64.790307	-8.471957	1.311258
-64.817698	-0.728332	1.316262
-65.127754	0.017253	1.321267
-65.421755	-2.515684	1.326272
-66.522198	1.565510	1.331277
-66.748368	-0.738356	1.336282
-66.274046	0.676616	1.341286
-66.409355	-6.322990	1.346291
-66.784946	-4.174357	1.351296
-66.825198	-5.642658	1.356301
-66.901340	-1.839672	1.361306
-67.380378	-0.479339	1.366310
-67.940388	0.797960	1.371315
-67.795878	-6.374647	1.376320
-68.502230	-2.115854	1.381325
-68.446198	-9.479763	1.386330
-68.690103	-3.722767	1.391334
-69.157341	-9.072778	1.396339
-69.616162	-11.548914	1.401344
-69.963751	-7.493612	1.406349
-69.777311	-14.423170	1.411354
-69.928978	-7.792740	1.416358
-70.102763	-5.597341	1.421363
-70.246261	-17.722176	1.426368
-70.389860	-10.241419	1.431373
-71.017403	-14.405673	1.436378
-71.326859	-18.378509	1.441382
-71.799829	-13.438068	1.446387
-71.242330	-12.434936	1.451392
-72.025473	-11.062333	1.456397
-72.832871	-6.416359	1.461402
-73.168729	-8.964239	1.466406
-73.042559	-4.935793	1.471411
-73.305376	-21.214882	1.476416
-73.510961	-8.139622	1.481421
-73.328180	-21.011709	1.486426
-73.356085	-8.978873	1.491430
-73.378730	-1.725610	1.496435
-73.981231	-2.362833	1.501440
-74.763319	-1.612187	1.506445
-74.692834	-5.687452	1.511450
-75.279475	-8.663287	1.516454
-75.125467	-9.510327	1.521459
-75.587109	-8.962524	1.526464
-76.010870	-11.281887	1.531469
-76.088778	-10.217530	1.536474
-76.341116	-10.799299	1.541478
-76.782982	-3.541468	1.546483
-76.431897	-8.359553	1.551488
-76.901772	1.477877	1.556493
-77.471311	-13.686630	1.561498
-77.768823	-2.576670	1.566502
-78.459490	-8.628141	1.571507
-78.272995	-7.683510	1.576512
-78.169900	-1.861259	1.581517
-78.364898	-13.427186	1.586522
-78.550279	4.438822	1.591526
-78.790935	0.512165	1.596531
-79.086708	-5.994871	1.601536
-79.708461	-3.257731	1.606541
-79.653247	-9.388594	1.611546
-79.908168	-9.235279	1.616550
-80.615057	-11.419371	1.621555
-80.916440	-13.247996	1.626560
-80.944509	-2.240841	1.631565
-81.270821	-10.937488	1.636570
-81.794121	-4.627899	1.641574
-81.473417	-9.347005	1.646579
-81.377134	-8.829986	1.651584
-81.544347	-5.094938	1.656589
-81.894914	-7.650042	1.661594
-82.719614	1.920780	1.666598
-82.914101	-9.135336	1.671603
-82.623336	-8.351891	1.676608
-83.177256	-6.658253	1.681613
-83.946194	-13.650200	1.686618
-84.463626	-5.378958	1.691622
-84.405439	-7.725355	1.696627
-84.324092	-2.436027	1.701632
-84.741710	-9.885573	1.706637
-84.604541	-10.100335	1.711642
-84.893167	-10.204062	1.716646
-84.886835	-6.041442	1.721651
-85.645032	-4.107637	1.726656
-86.284231	-6.465382	1.731661
-86.141781	-7.351742	1.736666
-86.055319	-12.046511	1.741670
-86.595874	-6.034388	1.746675
-86.108410	-11.544679	1.751680
-87.176397	0.321656	1.756685
-87.415053	-2.789969	1.761690
-87.674428	-4.479752	1.766694
-88.234487	4.627559	1.771699
-87.479050	-8.675389	1.776704
-88.171481	1.081430	1.781709
-88.601253	-7.067599	1.786714
-89.030186	-6.283505	1.791718
-89.582638	-11.883767	1.796723
-89.360206	-10.567424	1.801728
-89.359723	-4.239927	1.806733
-89.292989	-8.378305	1.811738
-89.975738	-8.817288	1.816742
-90.076720	-4.666033	1.821747
-90.551156	-9.860138	1.826752
-90.748551	-10.119133	1.831757
-90.828654	-9.226087	1.836762
-91.883838	-3.639888	1.841766
-92.301379	-7.350069	1.846771
-92.051208	-15.547993	1.851776
-91.847627	-6.718194	1.856781
-92.110918	-5.332749	1.861786
-92.217465	-6.458318	1.866790
-92.587029	-9.209565	1.871795
-93.079041	-13.587161	1.876800
-93.908160	1.805785	1.881805
-94.008266	-12.264623	1.886810
-94.059219	-4.523400	1.891814
-94.091830	-0.022003	1.896819
-93.972971	-7.259015	1.901824
-94.165778	-2.667845	1.906829
-94.642872	1.285462	1.911834
-95.251572	-8.014834	1.916838
-95.731326	-3.853102	1.921843
-95.912283	-8.604054	1.926848
-95.786709	-0.829818	1.931853
-95.755719	-11.392600	1.936858
-95.988432	-12.650914	1.941862
-97.122075	-6.740683	1.946867
-97.396495	-16.538361	1.951872
-97.488894	-1.791401	1.956877
-97.501800	-12.480870	1.961882
-97.981035	-14.195668	1.966886
-98.057646	-2.647462	1.971891
-97.595040	0.123916	1.976896
-97.967963	-1.982494	1.981901
-98.283463	-5.011292	1.986906
-98.646293	-6.785894	1.991910
-99.487486	-8.765719	1.996915
-99.471285	-7.998950	2.006912
-99.145895	-6.439119	2.016909
-98.368943	-4.952378	2.026906
-97.845699	-4.368098	2.036902
-97.872476	-8.399163	2.046899
-97.046294	-9.986671	2.056896
-96.638888	-5.951742	2.066893
-96.349776	-11.028164	2.076890
-95.669792	-8.173059	2.086886
-95.235647	-3.783371	2.096883
-94.169758	-3.334939	2.106880
-93.856724	-5.703932	2.116877
-93.708133	-6.007933	2.126874
-93.238749	-8.393828	2.136870
-92.379314	-8.293790	2.146867
-91.813206	-5.903827	2.156864
-91.621424	-11.308453	2.166861
-91.568246	-12.620064	2.176858
-90.495836	-9.246933	2.186854
-90.330931	-3.616132	2.196851
-89.229254	-6.265004	2.206848
-88.998890	-5.315510	2.216845
-88.921375	-3.275052	2.226842
-87.892572	-11.061763	2.236838
-87.663316	-15.455075	2.246835
-87.257398	-9.129537	2.256832
-86.369290	-3.899918	2.266829
-86.306507	-6.033285	2.276826
-85.530694	-11.032352	2.286822
-85.165271	-7.193753	2.296819
-84.726570	-10.302830	2.306816
-83.826003	-13.076135	2.316813
-83.764804	-7.699573	2.326810
-83.006870	-9.215669	2.336806
-82.104053	-4.847972	2.346803
-82.104630	-12.503871	2.356800
-81.774297	-10.081035	2.366797
-81.092109	-4.728076	2.376794
-80.499040	-9.926550	2.386790
-80.148252	-6.245953	2.396787
-79.393229	-9.073701	2.406784
-78.694281	-14.413856	2.416781
-78.581228	-13.531006	2.426778
-78.420902	-14.673911	2.436774
-77.496040	-13.337614	2.446771
-76.909126	-9.191251	2.456768
-76.633101	-11.310868	2.466765
-75.526738	-9.747292	2.476762
-75.388666	-6.222396	2.486758
-75.212280	-11.578822	2.496755
-74.778192	-13.726689	2.506752
-73.906526	-9.344329	2.516749
-73.878634	-3.305863	2.526746
-72.984456	-4.609681	2.536742
-72.565962	-2.916940	2.546739
-72.141915	-9.635367	2.556736
-71.165135	-6.452014	2.566733
-70.663650	-9.487951	2.576730
-70.622981	-6.523405	2.586726
-70.620898	-9.270841	2.596723
-69.351069	-9.791454	2.606720
-69.125450	-4.485689	2.616717
-67.858439	-6.146668	2.626714
-67.908233	-9.477434	2.636710
-67.625769	-8.239240	2.646707
-67.318182	-1.322783	2.656704
-66.501118	-7.704068	2.666701
-66.202015	-6.768765	2.676698
-65.418378	-4.002604	2.686694
-64.748948	-1.567572	2.696691
-64.633860	-5.351733	2.706688
-64.300023	-14.570964	2.716685
-63.407302	-14.229278	2.726682
-63.087778	-7.825951	2.736678
-62.215968	-12.190533	2.746675
-61.576624	-1.510570	2.756672
-61.407395	-10.689993	2.766669
-61.400196	-5.863014	2.776666
-60.635822	0.579585	2.786662
-59.900991	-5.685486	2.796659
-59.777255	-2.770904	2.806656
-58.645250	-4.765875	2.816653
-58.411374	-0.771641	2.826650
-58.285404	-2.197502	2.836646
-57.210492	-5.801569	2.846643
-56.832144	0.898829	2.856640
-56.643439	-3.615777	2.866637
-56.181979	-0.543155	2.876634
-55.286012	-1.861690	2.886630
-55.081747	-6.640085	2.896627
-54.257636	-2.851843	2.906624
-53.928215	-6.947652	2.916621
-53.399120	-8.949886	2.926618
-53.257711	-5.981339	2.936614
-52.233730	-5.492142	2.946611
-52.011608	-3.793825	2.956608
-51.850626	-4.933282	2.966605
-50.812232	-6.791573	2.976602
-50.932252	-9.421701	2.986598
-49.974167	-6.143754	2.996595
-49.650600	2.156874	3.006592
-48.717441	-7.240819	3.016589
-48.003282	-10.846561	3.026586
-47.932674	-10.125784	3.036582
-47.870368	-12.792146	3.046579
-47.092172	-13.468523	3.056576
-46.607335	-12.564488	3.066573
-45.786542	-10.393687	3.076570
-44.900496	-9.049347	3.086566
-44.795120	-8.633685	3.096563
-44.580498	-10.564875	3.106560
-44.365359	-12.958689	3.116557
-43.371679	-13.099874	3.126554
-42.926176	-9.745219	3.136550
-42.669981	-10.155621	3.146547
-41.997488	-17.652121	3.156544
-41.528495	-14.116040	3.166541
-40.438865	-12.075280	3.176538
-40.050813	-20.019241	3.186534
-39.992974	-11.443081	3.196531
-40.110682	-8.008836	3.206528
-38.932127	-8.799180	3.216525
-38.583288	-15.764130	3.226522
-37.409798	-7.267114	3.236518
-37.074548	-12.480224	3.246515
-36.810856	-12.419455	3.256512
-36.904274	-11.302332	3.266509
-36.312482	-8.261646	3.276506
-35.690619	-14.055076	3.286502
-34.699522	-12.760402	3.296499
-34.054933	-6.032733	3.306496
-33.738138	-12.014529	3.316493
-33.709733	-8.976814	3.326490
-32.865234	-11.968402	3.336486
-32.428883	-16.739927	3.346483
-32.143124	-14.336351	3.356480
-30.956741	-13.808743	3.366477
-30.596390	-11.045519	3.376474
-30.458393	-16.929625	3.386470
-30.307459	-12.714935	3.396467
-29.114882	-14.525347	3.406464
-28.794248	-14.174311	3.416461
-28.864774	-9.743603	3.426458
-28.049368	-11.095370	3.436454
-27.587838	-13.118576	3.446451
-26.491320	-9.559753	3.456448
-26.167274	-8.941561	3.466445
-25.839482	-18.468408	3.476442
-25.698494	-13.229384	3.486438
-24.862955	-15.360595	3.496435
-24.390068	-15.734699	3.506432
-24.085609	-11.622188	3.516429
-22.956004	-6.420639	3.526426
-22.580310	-6.120049	3.536422
-22.476541	-12.511192	3.546419
-22.332630	-8.182908	3.556416
-21.327653	-13.426725	3.566413
-21.135607	-12.085376	3.576410
-19.932244	-4.590509	3.586406
-19.582245	-8.143227	3.596403
-19.571271	-4.561043	3.606400
-19.509385	-9.130242	3.616397
-18.399122	-13.222864	3.626394
-17.774787	-9.566784	3.636390
-17.153588	-5.307558	3.646387
-16.684174	-11.885533	3.656384
-16.514631	-15.085604	3.666381
-16.391919	-11.209025	3.676378
-15.248673	-10.627810	3.686374
-14.976642	-13.887791	3.696371
-14.045916	-10.364041	3.706368
-13.435298	-11.132292	3.716365
-13.437604	-8.827437	3.726362
-13.179563	-6.537009	3.736358
-12.286684	-6.659653	3.746355
-12.070076	-9.619583	3.756352
-11.515898	-11.098439	3.766349
-10.532959	-7.445256	3.776346
-10.275895	-5.264915	3.786342
-10.199720	-8.164754	3.796339
-9.131272	-11.090424	3.806336
-8.926010	-7.713021	3.816333
-8.530308	-9.570775	3.826330
-7.786829	-11.665541	3.836326
-7.409168	-10.779842	3.846323
-6.829244	-7.485855	3.856320
-5.749331	-1.559214	3.866317
-5.450904	-3.266049	3.876314
-5.306758	-7.895749	3.886310
-5.388509	-7.873387	3.896307
-4.758788	6.541102	3.906304
-4.483797	10.640540	3.916301
-3.489477	19.151361	3.926298
-3.045822	32.174806	3.936294
-2.578798	50.679455	3.946291
-1.906523	62.281852	3.956288
-1.659556	69.560321	3.966285
-1.269228	78.105376	3.976282
-0.894321	93.409140	3.986278
-0.671550	115.629503	3.996275
0.000000	126.573856	4.001280
-0.072177	146.017429	4.006285
0.446894	144.996833	4.011290
0.551199	157.355924	4.016294
0.810174	165.693563	4.021299
0.648572	169.097585	4.026304
0.813062	177.359373	4.031309
0.778609	169.951017	4.036314
0.667109	178.472585	4.041318
0.845770	180.893782	4.046323
0.602962	171.757100	4.051328
0.657514	175.918862	4.056333
0.823923	176.487578	4.061338
0.737412	179.366455	4.066342
1.173297	182.844428	4.071347
1.155011	190.817715	4.076352
0.877024	191.915143	4.081357
1.362923	177.356824	4.086362
0.945079	193.848217	4.091366
0.802616	182.290171	4.096371
1.021136	185.887942	4.101376
1.164633	196.288353	4.106381
1.297393	188.822990	4.111386
1.316361	195.539600	4.116390
1.300409	187.854067	4.121395
1.176036	183.021221	4.126400
1.038579	185.890216	4.131405
1.151163	175.817324	4.136410
0.824239	186.622106	4.141414
1.204581	187.166709	4.146419
1.479441	192.492421	4.151424
1.045521	194.101202	4.156429
1.602709	196.901706	4.161434
1.194797	199.618916	4.166438
1.141867	194.685590	4.171443
1.552815	199.580999	4.176448
1.166094	200.177716	4.181453
1.206633	193.989416	4.186458
1.271310	207.694422	4.191462
1.368452	194.858879	4.196467
1.355590	200.035874	4.201472
1.157422	204.292533	4.206477
1.257710	194.346387	4.211482
1.175453	210.878317	4.216486
1.055198	203.634770	4.221491
1.190364	204.007994	4.226496
1.046788	202.112455	4.231501
1.142265	203.284166	4.236506
1.025106	199.963056	4.241510
1.094791	206.397739	4.246515
1.350969	220.570570	4.251520
1.656052	229.870663	4.256525
1.474753	229.302724	4.261530
1.469050	234.478541	4.266534
1.858716	231.744309	4.271539
2.104609	223.220583	4.276544
1.359089	214.599785	4.281549
1.658172	208.427114	4.286554
1.356368	210.199429	4.291558
1.814187	203.415485	4.296563
1.629394	203.675539	4.301568
1.499408	204.476051	4.306573
1.699936	193.226446	4.311578
1.295879	200.311537	4.316582
1.651561	210.465743	4.321587
1.636816	216.263269	4.326592
1.887317	220.535935	4.331597
1.749167	210.098981	4.336602
1.485528	218.486020	4.341606
1.883097	213.028091	4.346611
1.795601	218.995773	4.351616
1.535893	217.917346	4.356621
1.722511	209.241076	4.361626
2.120283	221.980243	4.366630
1.643650	212.059331	4.371635
1.502405	205.673520	4.376640
1.741514	220.506302	4.381645
2.102786	220.598832	4.386650
1.919581	230.892743	4.391654
1.992982	211.600885	4.396659
2.054230	204.660857	4.401664
1.575861	206.303272	4.406669
1.555170	203.244957	4.411674
1.576196	228.216182	4.416678
1.950990	225.366420	4.421683
2.143190	227.054655	4.426688
2.154793	225.151475	4.431693
2.292693	216.916440	4.436698
1.894382	207.956344	4.441702
1.857461	209.072313	4.446707
1.871159	210.692733	4.451712
1.774296	227.343732	4.456717
2.393603	223.757143	4.461722
1.614194	209.697205	4.466726
1.911734	225.003544	4.471731
1.878600	219.743691	4.476736
1.769752	234.135663	4.481741
2.311957	229.654161	4.486746
1.898040	227.750075	4.491750
1.986322	237.909870	4.496755
2.117104	233.122214	4.501760
1.716005	238.275346	4.506765
2.131451	231.255124	4.511770
2.337055	232.094183	4.516774
2.453919	234.678198	4.521779
2.124070	230.451554	4.526784
2.261329	230.206387	4.531789
1.949392	231.061020	4.536794
1.587598	236.317335	4.541798
1.854538	237.056020	4.546803
1.953544	231.924171	4.551808
1.673418	230.518803	4.556813
2.208312	250.195097	4.561818
2.232542	260.742259	4.566822
2.218851	259.519537	4.571827
2.406990	261.619099	4.576832
2.191595	261.029396	4.581837
2.487581	254.765462	4.586842
2.437076	271.996854	4.591846
2.613914	264.103022	4.596851
2.314473	256.551400	4.601856
2.234069	261.661893	4.606861
2.539507	252.242824	4.611866
2.558368	260.396451	4.616870
2.377573	243.112825	4.621875
2.268801	238.567249	4.626880
2.164200	251.310218	4.631885
2.680177	250.201528	4.636890
2.277130	265.003348	4.641894
2.752944	264.135763	4.646899
2.568093	253.317207	4.651904
2.255610	245.426571	4.656909
2.429133	254.359406	4.661914
2.600337	262.658801	4.666918
2.684553	259.201002	4.671923
2.481862	255.633026	4.676928
2.305393	264.971738	4.681933
2.803623	264.595337	4.686938
2.627228	265.845787	4.691942
2.616628	261.215413	4.696947
3.077214	261.091539	4.701952
2.453519	248.762730	4.706957
2.377607	237.177795	4.711962
2.312709	237.933549	4.716966
2.447463	260.306797	4.721971
2.730179	262.985201	4.726976
2.703512	265.791199	4.731981
2.596727	267.166831	4.736986
2.565449	259.413362	4.741990
2.586282	269.366336	4.746995
3.165284	264.644080	4.752000
2.663261	266.709369	4.757005
2.805273	264.050236	4.762010
2.646116	273.955972	4.767014
2.690763	272.071172	4.772019
2.773816	268.143124	4.777024
2.697084	266.731179	4.782029
2.676050	267.382754	4.787034
2.462254	279.364828	4.792038
2.429837	276.207413	4.797043
2.768417	268.892505	4.802048
2.703022	272.636547	4.807053
2.614732	263.216017	4.812058
2.475545	273.170529	4.817062
2.786403	288.399535	4.822067
2.861718	299.065512	4.827072
2.971002	296.545999	4.832077
3.087618	306.525109	4.837082
2.783609	303.340605	4.842086
2.915331	307.978172	4.847091
3.084438	309.565076	4.852096
2.523694	309.044415	4.857101
2.870303	301.368816	4.862106
3.028685	306.127454	4.867110
2.998242	305.402818	4.872115
3.157743	303.360593	4.877120
2.939165	305.041731	4.882125
3.124527	303.055790	4.887130
2.900281	305.666715	4.892134
3.068013	306.785972	4.897139
3.113923	295.012815	4.902144
2.859647	303.246791	4.907149
2.979234	284.797669	4.912154
2.860510	307.453467	4.917158
3.086322	302.558826	4.922163
3.121349	302.809183	4.927168
2.948858	312.500883	4.932173
3.442697	291.982082	4.937178
3.515153	308.576609	4.942182
3.051331	305.079256	4.947187
3.463237	304.701415	4.952192
2.828672	304.693657	4.957197
3.280429	301.677761	4.962202
2.966362	302.246816	4.967206
2.922729	303.323849	4.972211
3.251716	314.692606	4.977216
2.873259	325.411921	4.982221
3.605210	323.429454	4.987226
3.359803	342.469117	4.992230
3.245809	340.731444	4.997235
3.426696	327.341968	5.002240
3.251309	339.825048	5.007245
3.604522	332.035658	5.012250
3.411809	333.125237	5.017254
3.555818	338.288045	5.022259
3.396190	326.574680	5.027264
3.247885	346.197114	5.032269
3.259419	329.404160	5.037274
3.311580	327.619335	5.042278
3.444538	332.936517	5.047283
3.545702	324.218540	5.052288
3.460011	337.337711	5.057293
3.823155	335.555464	5.062298
3.592913	335.129250	5.067302
3.635773	334.995478	5.072307
3.835221	331.446682	5.077312
3.494566	333.379387	5.082317
3.381505	328.951714	5.087322
3.396132	333.632036	5.092326
3.464778	325.691430	5.097331
3.726242	334.093472	5.102336
3.486703	343.924799	5.107341
3.748670	328.913777	5.112346
3.779842	333.410593	5.117350
3.527658	330.498275	5.122355
3.612641	333.216858	5.127360
3.228374	335.192728	5.132365
3.716276	327.498958	5.137370
3.626747	336.544235	5.142374
3.504460	331.100052	5.147379
4.049402	329.498341	5.152384
3.790092	342.806608	5.157389
4.094265	332.436752	5.162394
3.860242	341.246752	5.167398
3.912805	331.834737	5.172403
3.675982	330.850178	5.177408
3.542428	329.717426	5.182413
3.820928	327.939382	5.187418
3.645286	341.446072	5.192422
3.534291	333.568472	5.197427
3.701085	321.435592	5.202432
3.608560	329.277237	5.207437
3.795261	329.411019	5.212442
3.278900	328.633748	5.217446
3.303589	338.486670	5.222451
3.399638	348.682345	5.227456
3.681294	355.839816	5.232461
4.046988	356.576301	5.237466
3.744075	368.955294	5.242470
3.875613	365.257936	5.247475
4.331423	355.148798	5.252480
3.698383	371.007778	5.257485
3.674882	359.446798	5.262490
3.691404	368.912546	5.267494
3.994700	368.485663	5.272499
4.058356	367.468327	5.277504
3.965622	362.228198	5.282509
4.177334	365.619942	5.287514
4.156298	361.169859	5.292518
4.544465	367.735590	5.297523
4.141242	359.508132	5.302528
4.225575	374.058749	5.307533
4.220466	359.833273	5.312538
4.082045	367.986657	5.317542
4.376100	370.716476	5.322547
4.320002	359.415079	5.327552
3.903380	373.085972	5.332557
3.879694	363.718382	5.337562
3.689990	374.285787	5.342566
3.614793	365.443772	5.347571
4.180981	378.548560	5.352576
4.156227	394.406509	5.357581
4.303639	388.670615	5.362586
3.931988	399.602168	5.367590
4.177099	383.654783	5.372595
4.648461	395.282516	5.377600
4.480340	390.374785	5.382605
4.672474	386.426012	5.387610
4.693426	395.241813	5.392614
4.415277	385.091056	5.397619
4.694159	369.337182	5.402624
3.904471	371.792079	5.407629
4.316765	364.132171	5.412634
4.170992	371.621567	5.417638
4.463470	392.690859	5.422643
4.672843	396.118914	5.427648
4.356635	381.105864	5.432653
4.327572	379.567191	5.437658
4.412515	386.812231	5.442662
4.561000	390.298159	5.447667
4.493081	391.164338	5.452672
4.465023	400.224694	5.457677
4.549445	391.033098	5.462682
4.613648	399.397514	5.467686
4.550827	395.410602	5.472691
4.531740	387.050610	5.477696
4.487695	396.725552	5.482701
4.593336	386.329458	5.487706
4.749440	398.049651	5.492710
4.426720	387.161958	5.497715
4.438623	403.945240	5.502720
4.547639	395.134355	5.507725
4.733945	393.954551	5.512730
4.621183	399.278852	5.517734
4.592357	394.829068	5.522739
4.421861	402.451250	5.527744
4.205712	404.596716	5.532749
4.285422	400.310043	5.537754
4.181259	394.840724	5.542758
4.542334	395.877334	5.547763
4.625288	389.867203	5.552768
4.218236	402.436396	5.557773
4.703423	410.345847	5.562778
4.833423	427.801774	5.567782
4.707964	426.524207	5.572787
4.913210	430.464446	5.577792
4.872050	426.835640	5.582797
5.015128	435.963081	5.587802
4.935715	429.679776	5.592806
4.950233	426.549259	5.597811
4.785267	401.867724	5.602816
4.798414	419.956969	5.607821
5.130228	423.537939	5.612826
4.550309	409.631338	5.617830
4.934167	423.044118	5.622835
5.499224	420.961112	5.627840
4.869776	419.887489	5.632845
4.853882	404.455290	5.637850
4.773034	414.383423	5.642854
4.822408	412.356528	5.647859
5.471521	419.774609	5.652864
4.843976	417.092989	5.657869
4.900392	404.396453	5.662874
4.784471	406.852440	5.667878
4.923367	421.996495	5.672883
5.143203	433.816630	5.677888
5.025468	434.555128	5.682893
5.050359	426.874725	5.687898
5.172504	433.263882	5.692902
4.837353	431.637944	5.697907
4.871265	435.492208	5.702912
4.593750	442.246165	5.707917
5.197836	427.921938	5.712922
5.011319	430.149704	5.717926
4.598182	433.432988	5.722931
4.992043	435.200012	5.727936
4.599654	429.378984	5.732941
4.830109	438.509072	5.737946
5.390750	462.896073	5.742950
5.272353	460.807073	5.747955
5.387242	467.343872	5.752960
5.394324	477.077067	5.757965
5.430144	446.137948	5.762970
5.085727	440.367354	5.767974
5.263538	442.169499	5.772979
5.302236	448.023350	5.777984
5.209945	462.208935	5.782989
5.393234	456.668137	5.787994
5.328221	464.296892	5.792998
5.300340	466.708853	5.798003
5.255076	459.727411	5.803008
5.175200	459.250548	5.808013
5.196783	459.771911	5.813018
5.287342	456.595203	5.818022
5.247121	463.348801	5.823027
5.276722	456.507853	5.828032
5.398897	458.384564	5.833037
5.221722	458.900088	5.838042
5.547641	463.758013	5.843046
5.502327	457.491524	5.848051
5.863594	463.983820	5.853056
5.648914	461.028342	5.858061
5.513656	461.835861	5.863066
5.595937	452.061263	5.868070
5.607727	460.083365	5.873075
5.633905	463.851305	5.878080
5.376541	462.403454	5.883085
5.604145	463.732405	5.888090
5.417125	453.003263	5.893094
5.263407	459.449333	5.898099
5.406309	458.316601	5.903104
5.342480	469.893829	5.908109
5.591506	458.543223	5.913114
5.446643	466.886974	5.918118
5.159406	471.142723	5.923123
5.584089	471.832113	5.928128
5.436538	495.094255	5.933133
5.564646	493.086232	5.938138
5.305115	495.879471	5.943142
5.185368	496.474054	5.948147
5.799428	497.348446	5.953152
5.339966	501.590599	5.958157
5.736158	497.915725	5.963162
5.802220	502.825338	5.968166
5.617733	502.613319	5.973171
5.978651	499.426397	5.978176
5.715119	497.114846	5.983181
6.004625	489.831080	5.988186
5.621266	493.613223	5.993190
5.760642	494.632027	5.998195
5.635914	497.669658	6.003200
5.451056	494.512671	6.008205
5.962508	503.784549	6.013210
5.979014	510.722917	6.018214
6.022898	507.445028	6.023219
5.837184	499.840244	6.028224
5.429034	500.988336	6.033229
5.843773	508.131257	6.038234
5.833694	512.921117	6.043238
6.008059	525.687012	6.048243
6.585279	515.071356	6.053248
5.894225	504.289004	6.058253
5.860591	495.636946	6.063258
6.042005	495.810483	6.068262
5.601850	492.811173	6.073267
5.895034	485.060101	6.078272
5.978165	494.733108	6.083277
6.324073	483.982462	6.088282
6.065854	487.018203	6.093286
5.954512	495.295223	6.098291
5.981278	491.153881	6.103296
5.759038	488.807446	6.108301
6.101636	487.537327	6.113306
6.203881	492.176691	6.118310
6.154140	488.150680	6.123315
6.116376	478.418909	6.128320
5.760092	466.061463	6.133325
5.786484	456.744496	6.138330
5.708210	460.539662	6.143334
5.625763	472.252596	6.148339
5.951372	488.747027	6.153344
5.939766	492.021206	6.158349
6.115271	484.557280	6.163354
6.457110	469.125745	6.168358
6.319540	463.865603	6.173363
5.903641	459.206629	6.178368
5.902856	470.648664	6.183373
5.876631	462.576150	6.188378
6.021857	464.940197	6.193382
5.696109	458.636255	6.198387
5.856772	455.476311	6.203392
5.770124	463.025781	6.208397
6.098786	459.263077	6.213402
5.659046	456.591873	6.218406
5.644910	462.742027	6.223411
5.996839	464.561806	6.228416
5.557745	465.698264	6.233421
5.726751	459.147709	6.238426
6.047711	473.754404	6.243430
5.527040	467.055034	6.248435
5.878521	457.429866	6.253440
5.666070	465.133645	6.258445
6.064125	445.876335	6.263450
5.852727	468.254927	6.268454
5.559315	464.318558	6.273459
5.629198	453.548493	6.278464
5.643687	465.457642	6.283469
5.742042	460.359570	6.288474
5.831167	478.816126	6.293478
5.912981	476.128482	6.298483
6.060272	474.407750	6.303488
5.652725	468.260467	6.308493
6.012643	471.054739	6.313498
5.538877	474.318508	6.318502
5.725182	486.222006	6.323507
6.245672	491.690715	6.328512
5.736578	481.486717	6.333517
5.770979	480.134425	6.338522
5.672906	486.172641	6.343526
5.362131	497.698582	6.348531
5.871221	491.408211	6.353536
5.829457	505.921894	6.358541
6.034676	486.933585	6.363546
6.057241	501.281270	6.368550
5.968813	496.534703	6.373555
6.085651	494.057909	6.378560
5.678515	493.029027	6.383565
5.801616	489.038619	6.388570
5.580774	492.548660	6.393574
5.561298	487.010571	6.398579
6.044672	491.291770	6.403584
5.780583	494.289810	6.408589
6.048620	488.910543	6.413594
6.094738	480.651156	6.418598
6.184096	482.803872	6.423603
6.099820	476.232062	6.428608
6.000720	464.046966	6.433613
5.695960	466.138496	6.438618
5.875729	457.000081	6.443622
5.796865	460.412121	6.448627
5.770011	450.420835	6.453632
5.780969	453.004335	6.458637
5.441207	459.639589	6.463642
6.165465	468.691567	6.468646
6.071327	482.166086	6.473651
5.985480	463.299000	6.478656
5.833892	467.155095	6.483661
5.778075	459.256025	6.488666
5.720940	458.137991	6.493670
5.559518	457.115632	6.498675
5.921422	465.833364	6.503680
5.777611	486.618715	6.508685
6.014440	478.117668	6.513690
6.014054	468.539137	6.518694
5.627347	470.375518	6.523699
6.062997	466.254233	6.528704
5.987821	471.414839	6.533709
5.874469	466.149487	6.538714
6.143616	465.468190	6.543718
5.740831	454.338406	6.548723
5.751779	459.808322	6.553728
5.615950	458.929908	6.558733
5.974136	461.477205	6.563738
6.101076	457.092682	6.568742
5.762795	463.715457	6.573747
5.797993	458.603611	6.578752
5.664220	463.541690	6.583757
5.691287	464.048723	6.588762
5.760348	466.010435	6.593766
5.771383	479.324008	6.598771
5.871392	484.479181	6.603776
5.737494	501.729819	6.608781
6.130646	490.219864	6.613786
5.791720	491.759407	6.618790
5.812603	489.512473	6.623795
6.047241	484.652027	6.628800
5.790074	472.057481	6.633805
5.694169	477.999625	6.638810
5.778722	482.647255	6.643814
6.005717	496.065451	6.648819
6.200033	477.646896	6.653824
5.651143	462.979099	6.658829
5.534848	458.343935	6.663834
5.739404	474.176876	6.668838
5.766744	488.945658	6.673843
6.034651	489.823118	6.678848
6.260218	483.074697	6.683853
5.833277	484.298332	6.688858
5.916023	468.714697	6.693862
5.757929	463.606363	6.698867
5.845451	451.952662	6.703872
5.429549	463.569064	6.708877
5.644304	468.734760	6.713882
6.083494	480.942348	6.718886
5.820532	485.103687	6.723891
5.839272	486.424927	6.728896
5.823058	491.575542	6.733901
5.951298	486.817042	6.738906
5.850503	485.175036	6.743910
5.757230	487.131567	6.748915
6.072028	488.105032	6.753920
6.220549	492.176076	6.758925
6.154556	472.578104	6.763930
5.930150	462.664638	6.768934
5.538219	455.826855	6.773939
5.875236	454.399207	6.778944
5.462576	464.294510	6.783949
5.836560	466.512594	6.788954
5.984452	475.683067	6.793958
5.891134	473.560494	6.798963
5.805808	460.922201	6.803968
5.812351	465.728228	6.808973
5.985919	469.493970	6.813978
5.901431	457.500628	6.818982
5.687324	456.229307	6.823987
5.615894	462.415230	6.828992
5.915092	467.564719	6.833997
6.064654	485.372268	6.839002
6.066192	472.878184	6.844006
5.882650	462.621668	6.849011
5.954082	461.946987	6.854016
5.916319	463.698138	6.859021
5.626551	452.328555	6.864026
5.824760	465.016832	6.869030
5.861325	458.470924	6.874035
5.971184	457.315859	6.879040
5.674497	470.146386	6.884045
5.854480	456.217041	6.889050
5.595157	466.668997	6.894054
5.846736	480.482696	6.899059
6.036601	477.421693	6.904064
5.738751	473.509543	6.909069
5.850629	483.332870	6.914074
5.829398	482.687996	6.919078
5.902049	496.755622	6.924083
5.811367	493.189890	6.929088
5.902804	495.063822	6.934093
5.971132	489.839701	6.939098
5.848479	465.807761	6.944102
5.638804	482.704522	6.949107
6.113366	478.963149	6.954112
5.973907	474.013134	6.959117
5.612056	462.753008	6.964122
5.916684	473.393621	6.969126
5.673610	476.132814	6.974131
5.976357	473.352604	6.979136
5.866931	492.764126	6.984141
5.951737	480.758414	6.989146
5.814468	469.937716	6.994150
5.834941	469.270322	6.999155
5.597145	468.161200	7.004160
5.762238	485.405736	7.009165
6.012639	482.820509	7.014170
5.975965	498.236542	7.019174
5.813488	495.940162	7.024179
6.183194	488.690230	7.029184
6.102651	476.461783	7.034189
5.586888	471.577669	7.039194
5.550025	463.991379	7.044198
5.958039	476.858113	7.049203
5.922815	469.978204	7.054208
5.742707	469.192398	7.059213
5.678772	476.144910	7.064218
5.846839	479.631946	7.069222
6.028255	489.372679	7.074227
6.233591	474.993915	7.079232
5.804822	473.564291	7.084237
5.731729	460.895548	7.089242
5.821965	453.741416	7.094246
5.810422	456.920463	7.099251
5.838647	447.379222	7.104256
5.666326	469.251274	7.109261
5.824472	473.413264	7.114266
6.309495	483.172598	7.119270
5.926756	481.866747	7.124275
5.985063	466.944104	7.129280
5.606576	468.128900	7.134285
5.738044	465.497534	7.139290
5.744664	465.402740	7.144294
5.510636	469.750680	7.149299
6.078310	474.551061	7.154304
5.777396	488.042785	7.159309
6.030911	483.930456	7.164314
6.190571	469.529294	7.169318
5.801305	478.112191	7.174323
5.602933	463.528216	7.179328
5.364168	470.586745	7.184333
5.683699	487.358453	7.189338
5.781475	487.283633	7.194342
5.766638	494.815460	7.199347
6.238861	494.300507	7.204352
6.280090	502.699187	7.209357
5.709249	486.516127	7.214362
5.780238	485.555976	7.219366
5.573093	504.043057	7.224371
6.072535	495.464607	7.229376
5.693681	503.585800	7.234381
6.100627	497.336084	7.239386
5.962445	501.615808	7.244390
5.612101	488.553659	7.249395
5.985278	486.252316	7.254400
5.732040	495.460267	7.259405
6.149347	490.100392	7.264410
6.010344	485.097411	7.269414
5.803791	478.442127	7.274419
5.710873	461.675072	7.279424
5.558296	473.092215	7.284429
5.867806	493.242982	7.289434
5.985232	493.703029	7.294438
6.123073	491.943807	7.299443
5.979123	467.956647	7.304448
5.374311	473.896745	7.309453
5.855707	479.260651	7.314458
6.132662	485.890896	7.319462
5.895031	488.359627	7.324467
5.576198	466.791658	7.329472
5.875348	481.903019	7.334477
5.923347	497.273404	7.339482
6.114467	482.421221	7.344486
5.800545	485.633363	7.349491
5.787224	463.432285	7.354496
5.696220	468.649590	7.359501
5.763645	479.469345	7.364506
6.225444	488.686912	7.369510
5.811310	472.101108	7.374515
5.803257	467.440846	7.379520
5.560842	472.053031	7.384525
6.049985	481.950998	7.389530
5.953393	475.216659	7.394534
5.733910	471.562622	7.399539
5.799540	461.494783	7.404544
5.790796	474.150963	7.409549
5.880998	487.147884	7.414554
6.060742	474.217670	7.419558
5.990376	478.472303	7.424563
6.358280	461.510649	7.429568
6.118632	471.501720	7.434573
5.887360	467.526014	7.439578
5.912755	460.038900	7.444582
5.925064	474.292557	7.449587
5.985368	467.509450	7.454592
5.620180	473.109376	7.459597
6.008544	471.085726	7.464602
5.772806	468.454218	7.469606
5.550066	474.200966	7.474611
5.649682	464.002367	7.479616
5.495062	467.029568	7.484621
5.748664	457.679572	7.489626
5.875158	456.523519	7.494630
5.679051	464.666216	7.499635
5.733967	470.193948	7.504640
5.611923	468.845163	7.509645
5.950293	489.932417	7.514650
5.870482	494.459763	7.519654
5.907026	493.369767	7.524659
6.014837	491.808332	7.529664
5.805764	490.886244	7.534669
5.916709	486.490557	7.539674
5.830044	475.244279	7.544678
5.775230	476.989582	7.549683
5.850960	466.294510	7.554688
5.945803	477.363085	7.559693
5.944291	482.571441	7.564698
6.255367	470.681261	7.569702
5.850984	474.732901	7.574707
5.830905	464.365741	7.579712
5.815497	465.745344	7.584717
6.098342	462.492670	7.589722
5.983045	469.743996	7.594726
5.715086	473.501823	7.599731
5.699899	469.121383	7.604736
5.645944	468.928714	7.609741
6.064360	466.991633	7.614746
5.870409	461.979638	7.619750
5.736030	467.515941	7.624755
6.107413	471.124484	7.629760
6.253715	471.219990	7.634765
5.650104	465.768143	7.639770
6.190170	472.522385	7.644774
5.682246	474.901062	7.649779
5.716704	479.203788	7.654784
5.970492	470.848322	7.659789
5.966276	461.649907	7.664794
6.417148	467.964116	7.669798
5.915468	464.391123	7.674803
5.934834	461.571977	7.679808
6.114482	471.758180	7.684813
6.142654	459.107142	7.689818
6.091014	466.889964	7.694822
5.806522	459.648138	7.699827
5.869405	457.251161	7.704832
5.644779	446.077563	7.709837
5.881385	458.970008	7.714842
6.024316	458.111961	7.719846
5.541285	459.142846	7.724851
5.589577	458.117796	7.729856
5.757706	471.081623	7.734861
6.062644	467.852902	7.739866
6.165233	459.210586	7.744870
5.938413	467.948223	7.749875
5.913379	459.665943	7.754880
5.943612	444.530130	7.759885
5.864937	444.466286	7.764890
5.774825	438.441290	7.769894
5.478242	447.924397	7.774899
6.132762	446.516005	7.779904
5.947280	467.591432	7.784909
5.541879	462.978862	7.789914
5.772282	460.067216	7.794918
5.841937	465.593878	7.799923
5.879072	466.159424	7.804928
5.778801	464.363018	7.809933
5.619185	474.640540	7.814938
6.115127	461.794535	7.819942
5.611530	464.955120	7.824947
5.890820	475.065169	7.829952
5.982894	472.145136	7.834957
5.816367	463.225694	7.839962
6.147008	463.164464	7.844966
5.811581	476.629551	7.849971
6.269415	463.779222	7.854976
5.860030	457.227318	7.859981
5.776686	448.285179	7.864986
5.877270	436.619846	7.869990
5.560753	445.041054	7.874995
5.459604	446.807474	7.880000
5.714118	463.511029	7.885005
5.674889	465.251767	7.890010
6.055354	466.263650	7.895014
5.887422	469.043633	7.900019
5.968702	468.761196	7.905024
6.118168	476.504481	7.910029
5.991797	473.099002	7.915034
6.251077	469.502341	7.920038
5.620521	455.746393	7.925043
5.392917	454.189799	7.930048
5.571587	460.752502	7.935053
5.251255	465.384542	7.940058
5.598538	464.670327	7.945062
5.644855	472.699524	7.950067
6.114435	467.892583	7.955072
6.186579	465.501169	7.960077
5.985106	472.203824	7.965082
6.126425	464.536414	7.970086
5.857523	465.894411	7.975091
5.959668	469.409371	7.980096
6.049822	467.166320	7.985101
6.035277	457.347427	7.990106
6.015284	464.715717	7.995110
5.417593	465.289491	8.000115
5.952558	476.079201	8.005133
5.861414	468.484296	8.010150
5.864780	479.023905	8.015168
6.027412	468.768566	8.020186
5.519587	475.185473	8.025203
5.897667	472.612481	8.030221
6.079840	474.116543	8.035238
6.024300	466.990085	8.040256
6.313107	466.350447	8.045274
6.202436	465.112310	8.050291
6.070719	444.212264	8.055309
5.727164	441.981835	8.060326
5.494090	438.142255	8.065344
6.016238	448.938497	8.070362
5.755068	455.529930	8.075379
5.917046	468.858447	8.080397
5.868736	474.641945	8.085414
5.738396	479.340956	8.090432
5.991027	469.234422	8.095450
5.788672	471.672982	8.100467
5.888835	470.152188	8.105485
5.879114	464.563242	8.110502
5.843620	473.203192	8.115520
6.240942	452.613983	8.120538
5.937658	470.190686	8.125555
6.137293	469.104103	8.130573
5.796322	477.594651	8.135590
5.920690	472.811288	8.140608
6.026017	468.239733	8.145626
5.590948	475.791680	8.150643
5.872945	471.150804	8.155661
5.919045	474.855029	8.160678
5.782595	470.672838	8.165696
6.004901	463.874574	8.170714
5.905908	471.354126	8.175731
5.978148	462.818573	8.180749
5.927044	466.470849	8.185766
6.053286	467.758048	8.190784
6.115805	457.086131	8.195802
5.977284	467.179676	8.200819
5.808734	464.219633	8.205837
5.958223	461.150240	8.210854
6.098549	462.100681	8.215872
6.002668	460.727028	8.220890
5.729659	473.164752	8.225907
5.735861	480.678789	8.230925
6.176745	491.140372	8.235942
6.110082	497.683157	8.240960
5.993531	490.716223	8.245978
6.347136	496.270738	8.250995
6.035239	500.804478	8.256013
6.274587	501.597335	8.261030
6.196863	504.533837	8.266048
6.380814	497.299651	8.271066
5.974303	494.993860	8.276083
5.990094	492.753102	8.281101
5.954165	493.461409	8.286118
5.991208	492.749847	8.291136
6.371887	490.059306	8.296154
6.162428	496.895877	8.301171
6.158999	491.319456	8.306189
6.343207	492.287013	8.311206
6.130536	502.082698	8.316224
6.503056	491.388167	8.321242
6.024773	489.000023	8.326259
5.950322	492.069627	8.331277
6.258853	500.684299	8.336294
5.830051	496.831965	8.341312
6.277381	494.662774	8.346330
5.924173	506.420416	8.351347
5.963773	504.381782	8.356365
6.279665	499.934457	8.361382
6.249393	500.026528	8.366400
6.438476	491.698092	8.371418
6.283426	501.695597	8.376435
6.110585	501.101589	8.381453
6.113768	507.780392	8.386470
6.516080	506.997883	8.391488
6.619689	496.755879	8.396506
6.351008	506.451832	8.401523
6.289705	502.329379	8.406541
6.048976	496.085379	8.411558
6.132636	506.204810	8.416576
6.146709	496.702619	8.421594
6.434699	488.391404	8.426611
6.189868	504.274535	8.431629
5.907465	497.214113	8.436646
6.087879	498.520064	8.441664
6.085524	505.635769	8.446682
6.089745	507.878598	8.451699
6.295859	499.202280	8.456717
6.604069	497.804567	8.461734
5.996550	500.939154	8.466752
6.370806	501.616093	8.471770
6.121538	504.492139	8.476787
6.244316	511.982681	8.481805
6.242798	500.327967	8.486822
6.168350	512.939590	8.491840
6.259963	518.327836	8.496858
6.148374	534.708095	8.501875
6.670715	524.214800	8.506893
6.810635	524.506909	8.511910
6.478998	518.216991	8.516928
6.257608	496.036624	8.521946
6.263207	501.921004	8.526963
6.369417	526.876253	8.531981
6.460949	519.978255	8.536998
6.502613	533.267382	8.542016
6.555117	505.631348	8.547034
6.310965	508.710659	8.552051
6.293403	522.637711	8.557069
6.312614	520.307412	8.562087
6.355833	529.650189	8.567104
6.483242	532.352029	8.572122
6.511155	522.881968	8.577139
6.288206	525.656408	8.582157
6.953968	529.515504	8.587175
6.550447	529.677289	8.592192
6.424436	524.632797	8.597210
6.062481	521.004364	8.602227
6.033941	531.517819	8.607245
6.609587	518.538732	8.612263
6.207908	532.775283	8.617280
6.693544	525.709032	8.622298
6.669715	532.903312	8.627315
6.414861	535.014418	8.632333
6.740758	523.683382	8.637351
6.439621	538.960413	8.642368
6.401466	523.948497	8.647386
6.643836	524.300343	8.652403
6.536645	524.789415	8.657421
6.908576	522.943944	8.662439
6.734587	533.315252	8.667456
6.611930	524.461697	8.672474
6.572050	520.337450	8.677491
6.126580	524.553863	8.682509
6.466357	529.423154	8.687527
6.604306	540.339218	8.692544
6.595406	531.595479	8.697562
6.628278	524.157870	8.702579
6.389469	529.960848	8.707597
6.470836	527.644231	8.712615
6.238134	536.922646	8.717632
6.391242	528.052189	8.722650
6.694234	533.606272	8.727667
6.376682	534.614122	8.732685
6.628379	519.879989	8.737703
6.423661	536.717026	8.742720
6.712805	523.794805	8.747738
6.576136	523.442792	8.752755
6.334606	528.595298	8.757773
6.789488	532.486492	8.762791
6.715149	548.751136	8.767808
6.854230	543.951134	8.772826
6.671317	534.113585	8.777843
6.710397	524.907587	8.782861
6.731601	533.558026	8.787879
6.741060	531.684226	8.792896
6.599405	530.613423	8.797914
6.764816	532.696799	8.802931
6.507224	539.272910	8.807949
7.090379	537.829298	8.812967
6.874548	533.318189	8.817984
6.601927	535.936532	8.823002
6.594799	522.281344	8.828019
6.484184	533.368035	8.833037
6.922571	541.888515	8.838055
6.718052	554.286380	8.843072
6.993478	551.329489	8.848090
7.026657	539.290470	8.853107
6.503098	538.993707	8.858125
6.672522	532.769308	8.863143
6.929992	540.154610	8.868160
6.770830	534.742432	8.873178
6.765870	526.394068	8.878195
6.686394	533.259046	8.883213
7.004617	537.374708	8.888231
6.770019	550.161195	8.893248
6.932919	544.593130	8.898266
6.990136	534.636740	8.903283
6.472195	534.419351	8.908301
7.097365	542.822771	8.913319
6.791458	541.778677	8.918336
7.056437	542.559796	8.923354
7.227552	529.954601	8.928371
6.659920	532.155485	8.933389
6.842461	520.057406	8.938407
7.094468	530.628355	8.943424
6.901183	520.914575	8.948442
7.051685	514.719506	8.953459
6.835497	528.251664	8.958477
6.977327	514.831345	8.963495
6.952043	526.139260	8.968512
6.623396	513.728550	8.973530
7.108642	519.664699	8.978547
6.785786	529.345853	8.983565
6.768785	524.921176	8.988583
6.746217	534.342403	8.993600
6.818762	540.301293	8.998618
6.900282	548.571277	9.003635
6.968170	559.676740	9.008653
7.177527	561.044808	9.013671
7.180863	567.810612	9.018688
7.187396	550.959518	9.023706
6.953783	534.250513	9.028723
6.698660	537.404481	9.033741
6.922886	542.654169	9.038759
7.199087	551.252393	9.043776
7.292055	549.178901	9.048794
7.162834	534.360442	9.053811
7.289522	542.292237	9.058829
7.209775	528.883146	9.063847
7.123519	525.018158	9.068864
6.856015	523.382697	9.073882
6.934453	522.641225	9.078899
6.839577	534.382523	9.083917
6.968672	523.711305	9.088935
6.980781	526.412428	9.093952
6.866228	528.827546	9.098970
7.079053	528.759735	9.103987
6.870330	546.890637	9.109005
7.433328	548.623313	9.114023
7.248649	550.371214	9.119040
7.167867	531.529325	9.124058
7.360140	525.688890	9.129075
7.025862	528.808379	9.134093
7.529760	516.350621	9.139111
7.144227	521.076116	9.144128
7.169149	522.184903	9.149146
7.057969	525.216528	9.154163
6.657812	531.736614	9.159181
7.230348	530.155410	9.164199
7.288218	526.209385	9.169216
6.887695	526.600966	9.174234
7.279480	514.403552	9.179251
6.987932	520.878026	9.184269
7.100633	515.635215	9.189287
7.301942	528.242549	9.194304
7.465591	529.495979	9.199322
7.346040	516.891472	9.204339
7.054275	527.513039	9.209357
6.691464	523.587924	9.214375
6.966450	538.163939	9.219392
7.203391	552.470332	9.224410
7.531973	546.618847	9.229427
7.134842	559.372125	9.234445
7.317250	548.748716	9.239463
7.355312	555.087128	9.244480
7.556135	560.475542	9.249498
7.460188	543.926895	9.254515
7.135533	534.694741	9.259533
7.226856	535.748992	9.264551
7.350914	536.209668	9.269568
6.859553	549.814350	9.274586
7.434272	547.471434	9.279603
7.268598	548.425697	9.284621
7.018351	556.602417	9.289639
7.320279	551.040373	9.294656
7.129116	564.522148	9.299674
7.448203	557.146390	9.304691
7.179300	554.449051	9.309709
7.213317	558.642071	9.314727
7.048786	552.773930	9.319744
7.121732	561.944478	9.324762
7.380333	558.705762	9.329779
7.430085	555.924163	9.334797
7.647659	563.297802	9.339815
7.410104	554.470216	9.344832
7.152580	558.715433	9.349850
7.485177	550.600099	9.354867
7.301509	562.271932	9.359885
7.271749	555.541505	9.364903
7.281766	558.548859	9.369920
7.316453	556.635827	9.374938
7.359515	557.306207	9.379955
7.255518	553.592178	9.384973
7.287095	549.708386	9.389991
7.440454	566.233798	9.395008
7.296707	562.604910	9.400026
7.293055	573.913004	9.405043
7.362270	582.052977	9.410061
7.903139	590.268878	9.415079
7.566808	581.224250	9.420096
7.409615	570.918861	9.425114
7.710639	575.003340	9.430131
7.296487	562.948897	9.435149
7.514352	575.292124	9.440167
7.660049	573.833037	9.445184
7.292754	573.201471	9.450202
7.742964	573.355402	9.455219
7.449492	573.515823	9.460237
7.542277	585.084250	9.465255
7.804783	577.840514	9.470272
7.520003	570.241328	9.475290
7.871095	557.332599	9.480307
7.598383	561.996446	9.485325
7.277794	554.876405	9.490343
7.755183	557.127989	9.495360
7.627785	565.320315	9.500378
7.730898	568.560404	9.505395
7.499713	557.080815	9.510413
7.696521	558.689334	9.515431
7.813187	555.076608	9.520448
7.681232	569.219548	9.525466
7.830696	563.327361	9.530483
7.450984	570.050936	9.535501
7.435677	565.606677	9.540519
7.835407	552.829619	9.545536
7.335762	559.891205	9.550554
7.635683	556.416706	9.555571
7.585128	562.737962	9.560589
7.497296	572.716074	9.565607
7.622224	576.631611	9.570624
7.440193	600.460977	9.575642
7.690153	594.405828	9.580659
8.043576	585.603019	9.585677
7.901687	590.932864	9.590695
8.353449	585.874795	9.595712
7.901046	577.040980	9.600730
7.636421	563.724590	9.605747
7.658484	562.481508	9.610765
7.367504	557.594335	9.615783
7.865313	555.317936	9.620800
7.359183	567.113244	9.625818
7.759085	570.304792	9.630835
8.050886	585.817933	9.635853
8.004866	580.811502	9.640871
7.906950	570.428354	9.645888
7.929148	568.027676	9.650906
7.954187	553.365432	9.655923
7.784673	563.001437	9.660941
7.807107	561.196336	9.665959
7.984059	566.479281	9.670976
7.492973	566.298172	9.675994
7.427515	558.605458	9.681011
7.682876	573.006044	9.686029
8.145548	584.511417	9.691047
8.002200	579.004476	9.696064
7.595023	580.565170	9.701082
8.108216	573.754530	9.706099
7.834914	580.903297	9.711117
8.085101	591.370072	9.716135
7.783637	574.363272	9.721152
7.712159	568.153704	9.726170
7.785285	570.051655	9.731187
8.022090	579.156005	9.736205
7.797670	586.382468	9.741223
7.750732	593.270015	9.746240
7.762881	594.001042	9.751258
8.103589	583.144427	9.756275
7.962631	589.290777	9.761293
7.644157	589.465787	9.766311
7.819849	579.472354	9.771328
7.656448	581.436585	9.776346
7.711416	594.936133	9.781363
8.185379	586.151474	9.786381
7.639232	591.115872	9.791399
7.941724	589.157537	9.796416
7.666640	589.459771	9.801434
7.712814	585.733766	9.806451
8.216555	585.608942	9.811469
7.866487	594.194167	9.816487
8.068494	592.698556	9.821504
7.825468	600.750684	9.826522
8.034551	609.218181	9.831539
8.409368	610.006636	9.836557
8.020201	602.415730	9.841575
8.160531	587.768737	9.846592
8.023009	597.619309	9.851610
7.993253	592.473568	9.856627
8.419810	601.420419	9.861645
8.264500	598.444569	9.866663
8.022732	584.224638	9.871680
8.173487	592.605765	9.876698
7.958131	579.735660	9.881715
8.425828	577.900444	9.886733
7.652997	588.384313	9.891751
7.964270	595.394983	9.896768
8.112642	608.340483	9.901786
8.144002	618.150401	9.906803
8.257070	611.080490	9.911821
8.204326	621.035283	9.916839
8.368357	614.073425	9.921856
8.329885	622.134475	9.926874
8.223233	611.304562	9.931891
8.531629	598.810931	9.936909
7.912698	595.359038	9.941927
8.237415	596.002486	9.946944
8.435036	617.382176	9.951962
8.267636	595.811930	9.956979
7.980300	580.628205	9.961997
8.213621	605.194967	9.967015
8.321144	609.707842	9.972032
8.242716	616.892340	9.977050
7.969903	620.434861	9.982067
8.073235	610.932922	9.987085
7.950985	619.917462	9.992103
8.187406	611.147076	9.997120
8.115346	622.049485	10.002138
7.853183	628.548841	10.007155
8.226860	619.288946	10.012173
8.240100	617.731211	10.017191
8.266126	611.757366	10.022208
7.995880	616.503096	10.027226
8.006488	618.296689	10.032243
8.393727	630.811201	10.037261
8.332329	644.969449	10.042279
8.635720	643.558745	10.047296
8.659766	653.950954	10.052314
8.253488	637.916937	10.057331
8.248110	625.111294	10.062349
8.263661	635.963525	10.067367
8.469828	637.393149	10.072384
8.616679	650.417080	10.077402
8.400229	634.429462	10.082419
8.631867	621.770238	10.087437
8.483844	623.345141	10.092455
8.467960	606.410121	10.097472
8.385099	614.583261	10.102490
8.120289	625.729896	10.107507
8.883089	617.494011	10.112525
8.805986	629.990040	10.117543
8.738414	621.680375	10.122560
8.694536	616.294082	10.127578
8.593865	614.538173	10.132595
8.905844	616.664517	10.137613
8.233484	618.429315	10.142631
8.707113	609.199856	10.147648
8.583873	618.728016	10.152666
8.304555	624.807424	10.157683
8.591530	608.812530	10.162701
8.497681	625.041917	10.167719
8.775257	615.333470	10.172736
8.546378	616.269112	10.177754
8.334807	617.709706	10.182771
8.439597	614.908516	10.187789
8.309502	623.369605	10.192807
8.414105	606.213002	10.197824
8.553612	625.908613	10.202842
8.492397	612.104672	10.207859
8.363961	623.461295	10.212877
8.548921	638.566300	10.217895
8.660889	634.753764	10.222912
8.621587	650.436166	10.227930
8.648426	662.005375	10.232947
8.831634	655.900672	10.237965
8.633464	645.946897	10.242983
8.470081	644.383480	10.248000
8.816237	656.458029	10.253018
8.574318	646.921530	10.258035
8.756102	638.838105	10.263053
8.445052	650.672700	10.268071
8.558291	643.342925	10.273088
8.690787	642.476921	10.278106
8.400359	647.886588	10.283123
8.437013	642.038907	10.288141
8.422557	646.487821	10.293159
8.720387	641.728918	10.298176
8.627376	635.051485	10.303194
8.690175	651.958938	10.308211
8.827409	642.640501	10.313229
8.814743	642.149382	10.318247
8.994284	648.602100	10.323264
9.021198	643.510304	10.328282
8.775531	649.197940	10.333299
8.898024	651.077263	10.338317
8.857958	656.461067	10.343335
8.832687	647.065512	10.348352
8.807427	651.654008	10.353370
8.687002	650.872557	10.358387
8.812490	649.169008	10.363405
8.433363	650.230403	10.368423
8.796322	654.030223	10.373440
9.139341	671.178499	10.378458
9.277896	676.087777	10.383475
9.138320	646.407802	10.388493
8.694696	645.272427	10.393511
8.414440	646.090243	10.398528
8.927315	643.266689	10.403546
9.222454	666.771788	10.408563
9.365651	648.100977	10.413581
9.156172	646.371614	10.418599
9.333415	648.032405	10.423616
9.398376	644.480807	10.428634
9.065608	638.625046	10.433651
9.221227	645.682082	10.438669
9.153819	643.489183	10.443687
9.065205	641.603129	10.448704
8.719916	644.219002	10.453722
8.758836	640.028088	10.458739
9.016079	644.898339	10.463757
8.686581	646.817159	10.468775
8.919502	648.760995	10.473792
8.953449	645.423983	10.478810
8.694390	654.218898	10.483827
8.803520	644.205978	10.488845
8.731419	650.395823	10.493863
8.903581	671.845759	10.498880
9.511632	666.424511	10.503898
9.262093	672.249992	10.508915
9.126590	665.036741	10.513933
8.670494	657.659868	10.518951
9.018425	668.637374	10.523968
9.239772	666.480919	10.528986
9.296657	676.120503	10.534003
9.184514	672.335759	10.539021
9.159767	666.602005	10.544039
9.277945	668.019291	10.549056
9.422032	658.819380	10.554074
9.101595	659.100220	10.559091
9.275847	651.608541	10.564109
8.993876	649.614479	10.569127
9.107159	659.401948	10.574144
9.150252	664.163126	10.579162
9.145562	678.318278	10.584179
9.350430	670.262887	10.589197
9.569885	679.245387	10.594215
9.296734	658.795098	10.599232
9.055688	648.252041	10.604250
9.108575	667.132251	10.609267
9.442486	672.941657	10.614285
9.429642	675.903035	10.619303
9.277127	671.553985	10.624320
9.702504	664.156771	10.629338
9.030542	655.767243	10.634355
9.316679	646.770875	10.639373
9.363459	646.584022	10.644391
9.269400	662.494810	10.649408
9.452550	655.206358	10.654426
9.064417	656.864672	10.659443
9.601342	666.290223	10.664461
9.335273	675.841568	10.669479
9.695635	673.714561	10.674496
9.541889	645.454936	10.679514
8.900110	655.614927	10.684531
9.169932	661.154296	10.689549
9.607433	664.344338	10.694567
9.469138	667.407858	10.699584
9.296189	668.563124	10.704602
9.017065	681.665755	10.709619
9.340426	669.410505	10.714637
9.408998	677.573271	10.719655
9.201463	684.990265	10.724672
9.337995	672.281656	10.729690
9.042790	679.517566	10.734707
9.465094	683.140417	10.739725
9.298712	676.572201	10.744743
9.604702	682.364403	10.749760
9.967199	678.913332	10.754778
9.580996	678.600822	10.759795
9.591653	683.503015	10.764813
9.449550	677.698023	10.769831
9.343350	675.091719	10.774848
9.371153	674.697997	10.779866
9.643058	673.584036	10.784883
9.545408	675.842639	10.789901
9.399823	667.994304	10.794919
9.382071	676.482809	10.799936
9.737344	669.656646	10.804954
9.759071	673.059878	10.809971
9.734116	665.093865	10.814989
9.824707	676.170836	10.820007
9.384524	674.909897	10.825024
9.479959	669.737221	10.830042
9.502202	679.041452	10.835059
9.543138	673.387519	10.840077
9.935373	675.793618	10.845095
9.478531	679.088613	10.850112
9.801326	680.421895	10.855130
9.722458	675.226027	10.860147
9.876238	681.889323	10.865165
9.916140	674.619750	10.870183
9.443209	679.699752	10.875200
9.827648	679.279232	10.880218
9.794390	673.393950	10.885235
9.605158	675.353431	10.890253
9.833970	675.887244	10.895271
9.589446	685.251170	10.900288
9.964821	675.652207	10.905306
9.620142	679.567877	10.910323
9.556517	672.914676	10.915341
9.836980	679.517942	10.920359
9.919397	697.250462	10.925376
10.128694	688.532372	10.930394
9.662205	691.805943	10.935411
9.841893	686.899353	10.940429
9.694705	679.889596	10.945447
9.747938	691.244812	10.950464
10.010063	694.128603	10.955482
10.052086	707.195397	10.960499
9.929986	702.266724	10.965517
9.678510	700.206173	10.970535
9.428645	704.615695	10.975552
10.269779	697.034608	10.980570
10.227525	700.959462	10.985587
10.037538	698.652294	10.990605
10.163925	690.495773	10.995623
9.741982	691.192073	11.000640
9.803226	678.953218	11.005658
9.887967	693.165953	11.010675
9.894773	692.447598	11.015693
10.161342	692.417504	11.020711
9.699177	701.868201	11.025728
10.079647	698.233444	11.030746
10.256613	704.134100	11.035763
9.837586	691.501870	11.040781
9.958625	698.448545	11.045799
10.201873	700.978812	11.050816
10.406703	691.073568	11.055834
10.201056	705.491653	11.060851
10.032999	693.824516	11.065869
10.283819	699.836310	11.070887
10.049352	699.052750	11.075904
10.061503	695.963424	11.080922
10.230229	693.346656	11.085939
10.068499	688.003152	11.090957
9.989890	676.687272	11.095975
9.969763	691.636275	11.100992
10.141265	700.405909	11.106010
10.061593	697.063953	11.111027
10.051079	695.858359	11.116045
10.512433	702.050892	11.121063
10.315438	696.677816	11.126080
10.127100	704.601036	11.131098
10.165246	692.675236	11.136115
10.028851	701.132297	11.141133
10.170991	691.065438	11.146151
9.966759	700.477397	11.151168
10.008193	694.386795	11.156186
9.822063	697.055548	11.161203
9.945607	705.299932	11.166221
10.233952	687.868822	11.171239
9.880246	701.960754	11.176256
10.213951	695.992426	11.181274
9.914502	697.883819	11.186291
10.131613	718.693920	11.191309
10.459692	718.705567	11.196327
10.225605	729.437754	11.201344
10.385269	730.049592	11.206362
10.355452	728.497231	11.211379
10.338543	727.750535	11.216397
10.641323	736.501520	11.221415
10.409322	723.069539	11.226432
10.473090	710.508021	11.231450
10.428644	709.798971	11.236467
10.440013	707.894126	11.241485
10.320678	713.415131	11.246503
10.322874	718.408695	11.251520
10.423760	716.433070	11.256538
10.274727	718.899810	11.261555
10.566253	728.470705	11.266573
10.471721	719.641299	11.271591
10.414695	723.672936	11.276608
10.373007	719.740063	11.281626
10.862484	724.691416	11.286643
10.548371	724.933412	11.291661
10.865835	719.072688	11.296679
10.386715	700.430844	11.301696
10.550678	694.848968	11.306714
10.582825	689.783056	11.311731
10.195118	695.884246	11.316749
10.633354	704.645964	11.321767
10.450160	714.957511	11.326784
10.509649	722.881672	11.331802
10.649454	719.534726	11.336819
10.626769	722.130258	11.341837
10.603617	720.025850	11.346855
10.442171	728.888632	11.351872
10.640399	719.122842	11.356890
10.716905	715.264215	11.361907
10.468310	725.701590	11.366925
10.654980	712.763963	11.371943
10.932494	722.565315	11.376960
10.911236	722.044521	11.381978
10.862244	727.587301	11.386995
10.690845	727.664447	11.392013
10.853567	717.915188	11.397031
10.798783	715.368634	11.402048
10.548969	700.923573	11.407066
10.959458	697.950111	11.412083
10.539939	711.517602	11.417101
10.608799	705.560221	11.422119
10.765202	728.934354	11.427136
10.778453	729.587257	11.432154
11.158080	720.233013	11.437171
10.569085	715.005196	11.442189
10.878994	715.500730	11.447207
10.778762	728.990170	11.452224
10.884565	726.883421	11.457242
10.818058	721.413063	11.462259
10.613529	726.182939	11.467277
11.092243	712.757831	11.472295
10.620461	727.547900	11.477312
10.720706	725.906999	11.482330
10.997214	720.685511	11.487347
10.870721	725.276682	11.492365
10.921458	722.911784	11.497383
10.662145	726.358983	11.502400
10.809847	723.776410	11.507418
11.238099	729.529807	11.512435
10.922668	724.130347	11.517453
11.059970	720.439159	11.522471
10.579243	721.415485	11.527488
10.679676	724.581451	11.532506
11.011707	729.426111	11.537523
11.031566	725.478283	11.542541
11.415979	719.692448	11.547559
11.106038	723.475003	11.552576
11.098145	719.570959	11.557594
11.208797	725.392298	11.562611
11.042079	734.924016	11.567629
10.906978	722.007384	11.572647
11.136957	728.733030	11.577664
10.906192	732.203239	11.582682
10.986454	734.746232	11.587699
10.942218	731.172216	11.592717
11.207585	724.374357	11.597735
11.011520	720.456514	11.602752
10.925884	730.605411	11.607770
11.397418	724.559444	11.612787
10.981451	734.016850	11.617805
11.039569	722.695533	11.622823
11.003487	720.769441	11.627840
11.273536	725.017167	11.632858
11.190718	715.621294	11.637875
11.197593	730.391647	11.642893
11.398773	726.653623	11.647911
11.291589	724.582669	11.652928
10.843424	733.500587	11.657946
11.230846	729.201729	11.662963
10.945912	728.825933	11.667981
10.908483	720.349801	11.672999
11.181499	729.010461	11.678016
11.422937	736.194995	11.683034
11.387593	725.194304	11.688051
10.998519	731.453400	11.693069
11.188513	739.256084	11.698087
11.309350	748.419963	11.703104
11.320507	757.020823	11.708122
11.391023	754.600275	11.713139
11.497372	752.620981	11.718157
11.362149	748.482602	11.723175
11.368097	750.654514	11.728192
11.227799	751.659489	11.733210
11.586269	744.768398	11.738227
11.173355	760.735826	11.743245
11.222003	744.990033	11.748263
11.381605	754.607476	11.753280
11.418336	748.643412	11.758298
11.753474	749.419180	11.763315
11.387161	746.649027	11.768333
11.594670	750.506989	11.773351
11.754925	742.271196	11.778368
11.405691	751.808852	11.783386
11.883253	750.633540	11.788403
11.674835	745.701288	11.793421
11.720376	740.709112	11.798439
11.816197	722.222646	11.803456
11.750772	723.069320	11.808474
11.838392	719.236992	11.813491
11.292704	727.943576	11.818509
11.464466	721.683873	11.823527
11.514047	711.206633	11.828544
11.642406	720.112573	11.833562
11.539143	718.463374	11.838579
11.287399	719.352039	11.843597
11.380605	723.922047	11.848615
11.546978	735.690740	11.853632
11.134693	751.978304	11.858650
11.905009	750.515771	11.863667
11.751784	757.740323	11.868685
11.555959	744.865455	11.873703
11.856996	752.122368	11.878720
11.684486	744.016285	11.883738
11.870187	744.959203	11.888755
11.580270	752.451137	11.893773
11.787578	746.749055	11.898791
11.865775	752.102213	11.903808
11.961285	744.272424	11.908826
11.857230	748.914593	11.913843
11.783959	760.376115	11.918861
11.814476	754.598107	11.923879
11.503036	750.787220	11.928896
11.777946	751.488360	11.933914
11.871993	745.237825	11.938931
11.474730	746.083753	11.943949
11.574342	757.176408	11.948967
11.524073	751.287822	11.953984
11.314958	748.684636	11.959002
11.436356	751.588679	11.964019
11.242321	765.278963	11.969037
11.811428	783.234603	11.974055
11.902197	791.815362	11.979072
11.660895	781.018929	11.984090
11.939436	786.401591	11.989107
12.281860	780.276479	11.994125
12.185163	784.272602	11.999143
12.278870	778.855117	12.004160
11.887829	785.227151	12.009178
12.069270	775.123000	12.014195
12.152855	778.041994	12.019213
11.984141	778.184634	12.024231
12.495590	776.266343	12.029248
12.225608	779.964126	12.034266
12.409658	749.040098	12.039283
12.088010	749.875231	12.044301
11.949382	746.121442	12.049319
12.100243	743.208840	12.054336
11.528503	749.380596	12.059354
11.663078	760.006257	12.064371
12.211705	780.037381	12.069389
12.269220	783.950594	12.074407
12.109856	772.792150	12.079424
12.323342	772.051250	12.084442
12.458133	771.211626	12.089459
12.356860	775.139616	12.094477
12.123292	774.898577	12.099495
12.224480	773.420887	12.104512
11.900730	770.121451	12.109530
12.222970	775.165966	12.114547
12.247504	775.272156	12.119565
12.027347	778.577633	12.124583
12.350342	771.024367	12.129600
12.367243	778.875720	12.134618
12.307453	781.049706	12.139635
12.441625	776.374257	12.144653
12.146265	768.245277	12.149671
12.265273	775.090757	12.154688
12.172125	776.572899	12.159706
12.483849	767.001978	12.164723
12.689100	772.692660	12.169741
12.520980	771.935664	12.174759
12.501020	768.811900	12.179776
11.986799	773.116768	12.184794
12.316787	765.467861	12.189811
12.294901	774.808812	12.194829
12.143582	768.643337	12.199847
12.195345	769.180007	12.204864
12.213015	772.368203	12.209882
12.305452	773.330364	12.214899
12.303833	771.375114	12.219917
11.928172	774.809971	12.224935
12.115279	777.758999	12.229952
12.464274	790.000492	12.234970
12.981226	800.429960	12.239987
12.515241	790.198778	12.245005
11.839408	787.339718	12.250023
12.784217	794.850451	12.255040
12.294249	798.364937	12.260058
12.937843	797.343509	12.265075
12.753213	796.142439	12.270093
12.620398	805.218796	12.275111
12.784757	791.720483	12.280128
12.623218	804.859182	12.285146
12.704291	787.717903	12.290163
12.804759	790.832306	12.295181
12.364999	784.464391	12.300199
12.663963	789.136430	12.305216
12.502056	796.786033	12.310234
12.643263	793.863412	12.315251
12.871408	789.687066	12.320269
12.707088	803.537786	12.325287
12.873768	800.525898	12.330304
12.538367	805.012652	12.335322
12.818092	806.695204	12.340339
13.229506	791.190622	12.345357
12.664877	797.084464	12.350375
12.722679	782.106738	12.355392
12.890213	794.029602	12.360410
12.915659	790.844551	12.365427
12.794219	780.458282	12.370445
12.492734	801.019872	12.375463
12.522619	796.519416	12.380480
12.624331	812.705277	12.385498
12.614872	798.761474	12.390515
12.835168	804.568949	12.395533
12.648729	804.519471	12.400551
13.124357	796.415273	12.405568
12.601871	806.238235	12.410586
12.790470	796.426756	12.415603
12.762584	791.946533	12.420621
12.752384	799.173512	12.425639
12.985890	798.968612	12.430656
12.877375	803.683777	12.435674
12.946490	809.116215	12.440691
12.928145	794.316870	12.445709
12.990028	818.980768	12.450727
13.192162	809.664041	12.455744
12.984919	811.859193	12.460762
12.820765	808.275171	12.465779
13.124099	811.100171	12.470797
13.091646	826.905030	12.475815
13.555891	818.866093	12.480832
13.243869	798.428574	12.485850
13.063285	794.280203	12.490867
13.092006	789.951780	12.495885
12.891723	794.966229	12.500903
13.152607	784.783518	12.505920
12.866199	789.819169	12.510938
13.198384	819.894226	12.515955
13.404098	816.929189	12.520973
13.236862	826.606118	12.525991
13.367032	812.721766	12.531008
12.888091	808.754466	12.536026
13.179429	816.708049	12.541043
13.417847	823.062872	12.546061
13.300086	823.331286	12.551079
13.599048	814.325408	12.556096
13.223650	813.220802	12.561114
13.012760	804.394152	12.566131
13.407775	810.236955	12.571149
13.136127	819.321239	12.576167
13.389932	820.818352	12.581184
13.051134	833.314342	12.586202
13.120868	821.896934	12.591219
13.396361	817.582603	12.596237
13.245549	827.195192	12.601255
13.271997	824.402459	12.606272
13.363743	825.457644	12.611290
13.245161	828.560238	12.616307
13.475351	816.832327	12.621325
13.470098	818.155190	12.626343
13.431068	819.423041	12.631360
13.405707	821.937151	12.636378
12.876177	821.427412	12.641395
13.240903	813.337111	12.646413
13.411555	825.946044	12.651431
13.473775	840.551606	12.656448
13.980283	851.535955	12.661466
13.281198	842.210742	12.666483
13.653384	832.682680	12.671501
13.563332	830.108506	12.676519
13.463770	821.578477	12.681536
13.622463	840.850339	12.686554
13.520680	849.050170	12.691571
13.943166	842.866257	12.696589
13.774091	843.873462	12.701607
13.918087	822.087573	12.706624
13.795195	827.266518	12.711642
13.487095	823.798143	12.716659
13.814307	821.951213	12.721677
13.619914	827.587088	12.726695
13.377577	824.400084	12.731712
13.634226	832.726540	12.736730
13.716830	847.952101	12.741747
13.988396	841.315945	12.746765
13.850404	850.278827	12.751783
13.789450	837.030310	12.756800
13.537937	832.471307	12.761818
13.746182	850.174231	12.766835
13.901595	850.551561	12.771853
13.597306	847.354772	12.776871
13.872904	844.791667	12.781888
13.807283	854.524947	12.786906
14.117415	848.645119	12.791923
14.290487	848.359325	12.796941
14.126972	854.306984	12.801959
13.829292	842.050693	12.806976
13.824061	825.838216	12.811994
13.660752	840.384617	12.817011
14.150384	843.844162	12.822029
14.040846	854.881498	12.827047
14.127649	851.335081	12.832064
14.164046	847.150828	12.837082
13.805354	831.871046	12.842099
14.296707	830.813900	12.847117
13.997150	832.857284	12.852135
14.082007	825.576429	12.857152
14.128441	822.095778	12.862170
14.103548	814.671371	12.867187
14.176754	806.905292	12.872205
13.772306	813.536042	12.877223
13.948088	828.873845	12.882240
14.061044	831.208088	12.887258
14.086530	850.556822	12.892275
14.330613	848.010568	12.897293
14.404053	844.663603	12.902311
14.243834	837.341789	12.907328
13.982466	843.895625	12.912346
14.178677	851.829410	12.917363
14.242763	849.925430	12.922381
13.954790	850.964798	12.927399
14.004925	851.104920	12.932416
14.235003	848.140748	12.937434
14.116603	857.331070	12.942451
14.498425	850.072297	12.947469
14.329532	850.484239	12.952487
14.250597	853.022809	12.957504
14.546965	848.586110	12.962522
14.314114	862.847654	12.967539
14.420792	854.008742	12.972557
14.211137	854.445371	12.977575
14.558258	860.622902	12.982592
14.417045	857.598992	12.987610
14.435262	856.775590	12.992627
14.337853	844.663557	12.997645
14.082314	856.067852	13.002663
14.125306	853.348342	13.007680
13.975527	847.711478	13.012698
14.063993	855.646835	13.017715
14.258580	851.085527	13.022733
14.160422	877.976355	13.027751
14.353129	878.173090	13.032768
14.569546	882.859468	13.037786
14.775677	889.766301	13.042803
15.021251	884.326294	13.047821
14.696355	895.802968	13.052839
14.523812	882.968207	13.057856
14.566171	870.386891	13.062874
14.629538	884.212044	13.067891
14.930251	883.375544	13.072909
14.495252	858.647269	13.077927
14.417008	869.050128	13.082944
14.642803	869.391747	13.087962
14.267943	886.563130	13.092979
14.580333	889.355933	13.097997
14.696591	886.367958	13.103015
14.831073	893.319770	13.108032
15.141597	885.574440	13.113050
14.939327	896.460105	13.118067
14.908180	883.554798	13.123085
14.905101	882.856973	13.128103
14.792716	888.979796	13.133120
14.932150	871.563585	13.138138
14.607914	867.400883	13.143155
15.186419	867.634276	13.148173
14.667281	866.329360	13.153191
14.788173	869.367162	13.158208
14.833245	872.405756	13.163226
14.865502	882.451109	13.168243
14.848242	872.371259	13.173261
14.940679	883.518737	13.178279
14.742963	881.140193	13.183296
14.763826	877.899393	13.188314
14.538750	882.607382	13.193331
14.771764	885.058678	13.198349
14.843197	882.842668	13.203367
14.886283	875.843516	13.208384
15.064922	884.627619	13.213402
15.073377	888.411228	13.218419
15.220148	884.380459	13.223437
15.206240	876.541626	13.228455
15.101284	888.592523	13.233472
15.299509	882.658452	13.238490
15.119331	885.527612	13.243507
14.986377	889.720917	13.248525
15.085989	885.223806	13.253543
14.732417	881.594877	13.258560
15.026892	879.710472	13.263578
14.734804	888.573406	13.268595
14.434161	885.579335	13.273613
15.006213	900.999958	13.278631
15.007579	906.932042	13.283648
15.414374	906.707788	13.288666
15.195160	910.806979	13.293683
15.320487	899.807410	13.298701
15.764395	901.270376	13.303719
15.668582	914.742314	13.308736
15.793548	898.880144	13.313754
15.214873	886.264643	13.318771
15.135459	875.526664	13.323789
15.286938	883.456483	13.328807
15.351472	904.423681	13.333824
15.492983	902.953647	13.338842
15.524995	910.187046	13.343859
15.251143	896.191633	13.348877
15.395705	904.418655	13.353895
15.231350	904.318068	13.358912
15.643295	894.382994	13.363930
15.616930	905.100067	13.368947
15.501133	904.617813	13.373965
15.836061	906.041809	13.378983
15.707297	888.610907	13.384000
15.486160	873.982386	13.389018
15.449780	883.645278	13.394035
15.379982	886.658482	13.399053
15.483351	893.335957	13.404071
15.243422	899.862042	13.409088
15.698539	892.934155	13.414106
15.704631	910.481784	13.419123
15.319938	902.768537	13.424141
15.832553	892.096703	13.429159
15.782889	906.611482	13.434176
15.706115	896.009262	13.439194
15.521169	894.647420	13.444211
16.063596	900.226010	13.449229
15.900366	894.918704	13.454247
15.655486	902.898270	13.459264
15.655058	895.639234	13.464282
15.745230	905.445070	13.469299
15.643686	902.461602	13.474317
15.730623	903.486098	13.479335
15.477963	899.705559	13.484352
15.579139	898.886476	13.489370
15.525949	909.514710	13.494387
15.510861	907.918941	13.499405
15.836943	899.833443	13.504423
15.762564	901.833898	13.509440
15.797811	887.936517	13.514458
15.697810	897.570428	13.519475
15.810723	891.061007	13.524493
16.025488	903.981351	13.529511
15.989650	904.229260	13.534528
16.092043	899.020905	13.539546
15.821173	904.374066	13.544563
15.956359	903.894779	13.549581
16.325174	907.439770	13.554599
16.024779	896.745197	13.559616
15.942860	896.803141	13.564634
15.920228	911.411457	13.569651
16.162645	913.940323	13.574669
16.121846	924.887746	13.579687
16.400448	915.551948	13.584704
16.007808	893.781730	13.589722
16.124222	905.198251	13.594739
15.814601	902.755041	13.599757
16.138349	911.255413	13.604775
16.088909	924.158077	13.609792
16.661708	929.544438	13.614810
16.337303	922.769522	13.619827
16.253561	920.178734	13.624845
16.273214	909.223886	13.629863
16.146678	921.511845	13.634880
16.533347	919.963072	13.639898
16.285149	916.739427	13.644915
16.164170	918.380528	13.649933
16.339887	916.319216	13.654951
16.371581	925.943066	13.659968
16.357094	922.482360	13.664986
16.436726	916.119592	13.670003
16.515648	927.061094	13.675021
16.757406	912.131206	13.680039
16.033263	903.522473	13.685056
16.284645	905.516223	13.690074
16.544369	915.236803	13.695091
16.249212	922.063790	13.700109
16.377357	915.069772	13.705127
16.403892	933.147655	13.710144
16.239047	924.240060	13.715162
16.522113	918.961120	13.720179
16.236378	920.741015	13.725197
16.447568	910.757020	13.730215
16.634335	922.502388	13.735232
16.446368	916.169138	13.740250
16.484385	930.534336	13.745267
16.137555	921.776863	13.750285
16.421135	924.311487	13.755303
16.693741	948.564019	13.760320
16.578956	940.500794	13.765338
17.048339	946.330896	13.770355
16.928575	937.218962	13.775373
17.132465	916.975441	13.780391
16.827529	919.205938	13.785408
16.919546	912.852529	13.790426
16.730922	912.924468	13.795443
16.458739	909.445970	13.800461
16.882873	913.187463	13.805479
16.802518	913.421710	13.810496
16.970673	920.590757	13.815514
16.831520	913.169939	13.820531
16.672392	914.693964	13.825549
16.608642	914.591024	13.830567
16.855807	920.110436	13.835584
17.065578	920.869455	13.840602
16.755879	920.451512	13.845619
16.523314	933.000984	13.850637
17.163142	929.118554	13.855655
17.069479	942.514771	13.860672
17.069605	945.234887	13.865690
17.072079	948.215423	13.870707
17.191545	955.963604	13.875725
17.307192	932.265074	13.880743
16.925823	926.510974	13.885760
17.065337	920.112466	13.890778
16.874611	924.641542	13.895795
16.842829	933.065200	13.900813
17.363486	936.310373	13.905831
17.179129	943.282329	13.910848
17.062642	946.070248	13.915866
17.229282	940.897458	13.920883
17.008622	944.638063	13.925901
17.290279	947.541096	13.930919
17.482273	944.686183	13.935936
17.319363	940.483657	13.940954
17.486852	939.434076	13.945971
17.168860	937.258769	13.950989
17.375090	932.563818	13.956007
16.994602	941.386360	13.961024
17.402384	939.038853	13.966042
17.198558	948.776660	13.971059
17.233820	943.130068	13.976077
17.205608	933.733843	13.981095
17.050140	945.941400	13.986112
17.079644	950.929123	13.991130
17.146409	946.239632	13.996147
17.025375	946.371986	14.001165
17.503372	944.561985	14.006183
17.220032	948.439182	14.011200
17.533209	948.456063	14.016218
17.569906	941.909488	14.021235
17.049401	956.347463	14.026253
17.542096	965.682722	14.031271
17.497578	976.216653	14.036288
17.294174	972.905044	14.041306
17.274481	977.013214	14.046323
17.910297	980.805362	14.051341
17.797166	978.826300	14.056359
17.414683	984.305316	14.061376
17.638491	986.392434	14.066394
18.015046	989.035623	14.071411
17.482983	977.703951	14.076429
18.035834	967.497395	14.081447
18.108676	984.788164	14.086464
17.923254	975.868803	14.091482
17.980980	981.694705	14.096499
17.868634	971.843179	14.101517
17.858905	950.034828	14.106535
17.747915	952.768493	14.111552
17.446719	954.103943	14.116570
18.174029	959.927596	14.121587
18.099310	959.258209	14.126605
18.175310	948.533716	14.131623
17.823031	951.845638	14.136640
17.279032	943.006560	14.141658
17.967045	956.178978	14.146675
17.966628	965.450536	14.151693
18.206295	965.149735	14.156711
18.247978	966.641570	14.161728
17.736648	954.445106	14.166746
17.886697	962.317334	14.171763
18.192694	971.306486	14.176781
18.467775	960.627237	14.181799
17.990192	946.305623	14.186816
18.267366	950.275868	14.191834
18.232307	936.295844	14.196851
17.450786	948.104733	14.201869
18.074071	961.972712	14.206887
18.203068	966.419135	14.211904
18.000071	976.808945	14.216922
18.486150	972.304462	14.221939
18.023766	982.053573	14.226957
18.341814	971.509686	14.231975
18.376655	973.185324	14.236992
18.449118	973.865796	14.242010
18.226508	949.053259	14.247027
17.748380	957.834956	14.252045
18.271619	959.719163	14.257063
18.104343	975.814084	14.262080
18.198669	975.828760	14.267098
18.236441	974.334821	14.272115
17.802180	974.570020	14.277133
18.029828	979.113428	14.282151
18.033770	987.507164	14.287168
17.997385	988.583657	14.292186
18.591261	991.006487	14.297203
18.641238	1000.935002	14.302221
18.501290	1002.672763	14.307239
18.818802	1008.854292	14.312256
18.459410	999.074122	14.317274
18.688553	976.531981	14.322291
18.274068	986.579019	14.327309
18.594564	990.148792	14.332327
18.420473	997.474555	14.337344
18.182182	1005.650310	14.342362
18.677570	1001.362762	14.347379
18.668425	1004.763718	14.352397
18.750964	1002.907634	14.357415
18.730112	1002.407234	14.362432
18.418445	997.965653	14.367450
19.115774	995.757403	14.372467
18.446601	996.132427	14.377485
18.630370	1001.287034	14.382503
18.859006	994.469574	14.387520
18.753391	1006.242738	14.392538
18.789812	1001.387418	14.397555
18.735980	1002.167224	14.402573
18.992880	991.350040	14.407591
18.765600	991.113857	14.412608
18.781678	993.851210	14.417626
18.979692	990.469730	14.422643
18.569579	1008.530122	14.427661
18.796204	990.758165	14.432679
18.929610	997.435220	14.437696
18.761673	991.935958	14.442714
19.033187	986.345944	14.447731
18.698396	994.981011	14.452749
18.911992	997.585937	14.457767
19.393384	1015.463521	14.462784
18.933607	1005.663813	14.467802
19.500668	991.436625	14.472819
19.278242	998.803098	14.477837
18.842828	992.187734	14.482855
19.029071	988.503112	14.487872
18.636913	996.224938	14.492890
19.158699	1010.815693	14.497907
19.497294	1026.427006	14.502925
19.473217	1023.174552	14.507943
19.627065	1009.700630	14.512960
19.339634	992.401881	14.517978
19.318701	986.932121	14.522995
19.117524	999.018781	14.528013
18.984894	991.259068	14.533031
19.325719	990.123788	14.538048
18.977676	992.424054	14.543066
19.427270	1005.016692	14.548083
19.521078	1024.592856	14.553101
19.293482	1022.606830	14.558119
19.617561	1025.843359	14.563136
19.572429	1023.305778	14.568154
19.583771	1000.439588	14.573171
19.492684	994.654734	14.578189
19.253799	992.907976	14.583207
19.434626	999.975550	14.588224
19.374946	1014.388953	14.593242
20.057631	1027.054671	14.598259
19.820905	1002.305021	14.603277
19.484527	1006.341432	14.608295
19.477845	999.328450	14.613312
19.244721	1001.263969	14.618330
19.651406	1015.859686	14.623347
19.615069	1028.637826	14.628365
19.630022	1022.895176	14.633383
19.454237	1025.467980	14.638400
19.543007	1026.900816	14.643418
19.792237	1019.432324	14.648435
19.787527	1025.660722	14.653453
19.853886	1031.454501	14.658471
19.837648	1026.827204	14.663488
19.746743	1033.496283	14.668506
20.051057	1021.171682	14.673523
20.012289	1027.131742	14.678541
19.863259	1023.216239	14.683559
19.642334	1015.896752	14.688576
19.557368	1021.840868	14.693594
19.546653	1023.165837	14.698611
19.943082	1020.206463	14.703629
19.901897	1023.145848	14.708647
19.836527	1020.403770	14.713664
19.783745	1025.637463	14.718682
19.880701	1021.987357	14.723699
19.943743	1019.440065	14.728717
19.909388	1028.260636	14.733735
20.273099	1033.505418	14.738752
19.936767	1033.014541	14.743770
20.468241	1039.616398	14.748787
20.302848	1028.033600	14.753805
19.799315	1025.653305	14.758823
19.909446	1023.044646	14.763840
20.008587	1040.587390	14.768858
20.177319	1052.298063	14.773875
20.173781	1050.386205	14.778893
20.126481	1048.905611	14.783911
20.447562	1042.365662	14.788928
20.285763	1049.839791	14.793946
20.108333	1037.399982	14.798963
20.488241	1045.473010	14.803981
20.144968	1040.224119	14.808999
20.558728	1036.466240	14.814016
20.478380	1044.643322	14.819034
20.364470	1046.070479	14.824051
20.797873	1052.650062	14.829069
20.586753	1041.292163	14.834087
20.575813	1040.411397	14.839104
20.295641	1051.255396	14.844122
20.411550	1038.299929	14.849139
20.342081	1050.360014	14.854157
20.451364	1049.672639	14.859175
20.570531	1038.784225	14.864192
20.487769	1039.479476	14.869210
20.583368	1036.294919	14.874227
20.480189	1041.511404	14.879245
20.123600	1036.706828	14.884263
20.855025	1023.901418	14.889280
20.455484	1035.803373	14.894298
20.554906	1030.008888	14.899315
20.655230	1036.530838	14.904333
20.716336	1033.098880	14.909351
20.634621	1033.799074	14.914368
20.642377	1044.052726	14.919386
20.842541	1038.054104	14.924403
21.094538	1043.263524	14.929421
20.607195	1046.901045	14.934439
20.645531	1054.738347	14.939456
20.744818	1064.741774	14.944474
21.024895	1073.867176	14.949491
21.020699	1064.041708	14.954509
20.924904	1077.164002	14.959527
21.274803	1061.332387	14.964544
21.107585	1060.786631	14.969562
21.064617	1046.059637	14.974579
21.200896	1028.018811	14.979597
21.034090	1037.987712	14.984615
21.192336	1034.399065	14.989632
21.112755	1035.685878	14.994650
20.960429	1032.624805	14.999667
21.344843	1033.236110	15.004685
21.252639	1040.281764	15.009703
20.986874	1030.249019	15.014720
21.157663	1039.163445	15.019738
21.156216	1033.764836	15.024755
21.128937	1041.410686	15.029773
21.106749	1053.753449	15.034791
21.803852	1063.998441	15.039808
21.127298	1050.399130	15.044826
20.839651	1054.745545	15.049843
21.205040	1061.270298	15.054861
20.969706	1077.370337	15.059879
21.035734	1071.890425	15.064896
21.155655	1071.634721	15.069914
21.228774	1070.050257	15.074931
21.591842	1065.454389	15.079949
21.128265	1075.086833	15.084967
21.334169	1071.530018	15.089984
21.393362	1078.316681	15.095002
21.271634	1072.812073	15.100019
21.468424	1074.791101	15.105037
21.360581	1077.526232	15.110055
21.846652	1087.369725	15.115072
21.708483	1085.134589	15.120090
21.741609	1085.590908	15.125107
21.806276	1080.265148	15.130125
21.663493	1080.566069	15.135143
21.908832	1054.812643	15.140160
21.745505	1054.098140	15.145178
21.608096	1061.215486	15.150195
21.721351	1058.647245	15.155213
21.616209	1058.882070	15.160231
21.906277	1060.191694	15.165248
21.794049	1069.889354	15.170266
21.745890	1082.119928	15.175283
22.001435	1081.000785	15.180301
21.810143	1080.333052	15.185319
22.080705	1085.102811	15.190336
22.162508	1069.725171	15.195354
22.130797	1068.491577	15.200371
21.927025	1062.864001	15.205389
21.699388	1061.890517	15.210407
21.661972	1062.299902	15.215424
21.728303	1067.818912	15.220442
21.906103	1083.932179	15.225459
22.091698	1077.733219	15.230477
21.916508	1085.763890	15.235495
22.075248	1077.928936	15.240512
22.377248	1081.210482	15.245530
22.231142	1086.227042	15.250547
22.387370	1084.743325	15.255565
22.224607	1087.311612	15.260583
22.625608	1077.753416	15.265600
22.192997	1084.699377	15.270618
22.254335	1093.965472	15.275635
22.622990	1075.814712	15.280653
22.319179	1076.325063	15.285671
22.207410	1063.368443	15.290688
22.198156	1070.752665	15.295706
21.974044	1082.895955	15.300723
22.240669	1065.307017	15.305741
22.238304	1085.487004	15.310759
22.338659	1081.780023	15.315776
22.198093	1081.267629	15.320794
22.282762	1078.095903	15.325811
22.419116	1075.218325	15.330829
22.095220	1082.611937	15.335847
21.980933	1083.654143	15.340864
22.322619	1094.589293	15.345882
22.643219	1098.331899	15.350899
23.084199	1101.077781	15.355917
22.566785	1095.212574	15.360935
22.936395	1095.665722	15.365952
22.707491	1078.470528	15.370970
22.704229	1072.003370	15.375987
23.077364	1067.114900	15.381005
22.679763	1075.115606	15.386023
22.232360	1087.288531	15.391040
22.823233	1084.417294	15.396058
23.023763	1100.143750	15.401075
23.322317	1087.964140	15.406093
22.653815	1079.022258	15.411111
22.590232	1065.614739	15.416128
22.897380	1072.234999	15.421146
22.941011	1093.054952	15.426163
23.407436	1089.072571	15.431181
22.771395	1075.501541	15.436199
22.775699	1064.889666	15.441216
23.052631	1083.877234	15.446234
22.944940	1086.700526	15.451251
23.124675	1085.880974	15.456269
22.943001	1097.687319	15.461287
23.039045	1095.421522	15.466304
22.445125	1096.636747	15.471322
22.650556	1102.710966	15.476339
23.030577	1089.297803	15.481357
23.297141	1093.127337	15.486375
23.185695	1094.637155	15.491392
23.108008	1101.007626	15.496410
23.259299	1102.867850	15.501427
23.203966	1091.917068	15.506445
23.037761	1096.835403	15.511463
23.093034	1095.559004	15.516480
22.965314	1097.540399	15.521498
23.148880	1115.421145	15.526515
23.084732	1127.374113	15.531533
23.392432	1124.886135	15.536551
23.450696	1123.851744	15.541568
23.648299	1120.147487	15.546586
23.885803	1120.589916	15.551603
24.255462	1116.198832	15.556621
23.942512	1099.682113	15.561639
23.790128	1090.023376	15.566656
23.975532	1080.297874	15.571674
23.545242	1090.723176	15.576691
23.519735	1082.635393	15.581709
23.574880	1089.509343	15.586727
23.621978	1087.572530	15.591744
23.990260	1091.632781	15.596762
23.605814	1083.515684	15.601779
23.851093	1079.179532	15.606797
23.647955	1093.273170	15.611815
23.474621	1081.942424	15.616832
23.758933	1079.885088	15.621850
23.977206	1088.142868	15.626867
24.083086	1082.750418	15.631885
23.870275	1079.675375	15.636903
23.708163	1093.029558	15.641920
23.503976	1087.710293	15.646938
23.630940	1086.968799	15.651955
23.585430	1083.729736	15.656973
23.623581	1094.075608	15.661991
23.741007	1113.833383	15.667008
23.818037	1107.598128	15.672026
23.879116	1121.712441	15.677043
23.920460	1120.219863	15.682061
23.707526	1115.103606	15.687079
23.794700	1120.231397	15.692096
23.970902	1111.082177	15.697114
23.626385	1118.207988	15.702131
24.216864	1135.991996	15.707149
24.384032	1147.850237	15.712167
24.628537	1134.822532	15.717184
24.415702	1119.690652	15.722202
24.089146	1113.605145	15.727219
24.367917	1116.124853	15.732237
24.334713	1118.108257	15.737255
24.210287	1131.327477	15.742272
24.596906	1130.201111	15.747290
24.645943	1137.737874	15.752307
24.434856	1112.638528	15.757325
24.498281	1117.470281	15.762343
23.994318	1117.632818	15.767360
24.747957	1115.749035	15.772378
24.504792	1136.706472	15.777395
24.537990	1137.689918	15.782413
24.509389	1142.246439	15.787431
24.589625	1151.520844	15.792448
25.016270	1149.262687	15.797466
24.577791	1131.356242	15.802483
24.662849	1116.458304	15.807501
24.815113	1127.032069	15.812519
24.782324	1115.020101	15.817536
24.992312	1111.010261	15.822554
24.735727	1107.109069	15.827571
24.752185	1111.816351	15.832589
24.701612	1102.563890	15.837607
24.474324	1116.330085	15.842624
24.982564	1128.878434	15.847642
24.966400	1139.731762	15.852659
24.918422	1144.368271	15.857677
25.265886	1142.104773	15.862695
25.053258	1117.109213	15.867712
25.134948	1107.633596	15.872730
25.104100	1111.457844	15.877747
24.953188	1108.158346	15.882765
25.234639	1098.982980	15.887783
24.748077	1110.966774	15.892800
24.989862	1103.651045	15.897818
24.568615	1103.871877	15.902835
25.122470	1129.733567	15.907853
25.209781	1130.198991	15.912871
24.992410	1137.531226	15.917888
25.084498	1138.397804	15.922906
24.951674	1140.790660	15.927923
25.121681	1138.483431	15.932941
25.362981	1134.449484	15.937959
25.158118	1138.743583	15.942976
25.412288	1132.715084	15.947994
25.236476	1135.636316	15.953011
24.902723	1140.453385	15.958029
25.233629	1139.407535	15.963047
25.247399	1135.139765	15.968064
25.564779	1130.084567	15.973082
25.180176	1145.432363	15.978099
25.320780	1157.441082	15.983117
25.744012	1170.222086	15.988135
25.646531	1170.301710	15.993152
25.947870	1162.501277	15.998170
25.529496	1157.092789	16.003187
25.462043	1134.269810	16.008205
25.673831	1142.174779	16.013223
25.676361	1159.391608	16.018240
25.900819	1154.463651	16.023258
25.891895	1171.214705	16.028275
25.890255	1155.925254	16.033293
25.721956	1140.778865	16.038311
25.464908	1133.758618	16.043328
26.098928	1149.865809	16.048346
25.935928	1153.743133	16.053363
25.888890	1160.137274	16.058381
26.098307	1160.814282	16.063399
25.850043	1155.123205	16.068416
26.018248	1154.274859	16.073434
26.165792	1157.360844	16.078451
25.661061	1144.994243	16.083469
25.691205	1146.151023	16.088487
25.716774	1155.831346	16.093504
25.870857	1149.010462	16.098522
26.017613	1161.883078	16.103539
25.876629	1154.678972	16.108557
25.987580	1156.879747	16.113575
25.832763	1171.272496	16.118592
26.029494	1157.117337	16.123610
25.900425	1167.504042	16.128627
26.254595	1187.861507	16.133645
26.340033	1183.846760	16.138663
26.156250	1195.661404	16.143680
26.216430	1188.862015	16.148698
26.291472	1193.914686	16.153715
26.529217	1192.088686	16.158733
26.547094	1187.962338	16.163751
26.737831	1187.028754	16.168768
26.608356	1174.796993	16.173786
26.599883	1188.637115	16.178803
26.336113	1178.751966	16.183821
26.476680	1184.453945	16.188839
26.254597	1186.193567	16.193856
26.840017	1184.605438	16.198874
26.756518	1182.911961	16.203891
26.757962	1180.453224	16.208909
26.747770	1180.984852	16.213927
26.810938	1187.161485	16.218944
27.231886	1171.266770	16.223962
26.618012	1165.457330	16.228979
26.432143	1165.157570	16.233997
26.448621	1166.015064	16.239015
26.763690	1180.377359	16.244032
26.981211	1170.050036	16.249050
26.819784	1180.135057	16.254067
26.789334	1177.626112	16.259085
27.032743	1168.491671	16.264103
26.637441	1189.542966	16.269120
27.048054	1183.895512	16.274138
26.804523	1175.804155	16.279155
26.635745	1183.023615	16.284173
26.861832	1179.766556	16.289191
26.889922	1186.263569	16.294208
27.136850	1174.344034	16.299226
26.931765	1189.472676	16.304243
26.618281	1194.443078	16.309261
27.453602	1209.803131	16.314279
27.062597	1216.385559	16.319296
27.400849	1204.852772	16.324314
27.509638	1212.558765	16.329331
27.012384	1202.224241	16.334349
27.502157	1204.256555	16.339367
27.542154	1203.850361	16.344384
27.903502	1195.833254	16.349402
27.702763	1190.055529	16.354419
27.302604	1181.546915	16.359437
27.276073	1176.282734	16.364455
27.321599	1176.728334	16.369472
27.493905	1198.947838	16.374490
27.674202	1198.556906	16.379507
27.624749	1207.337177	16.384525
27.769796	1200.842559	16.389543
27.747628	1204.880338	16.394560
27.542345	1196.122409	16.399578
27.396772	1190.776832	16.404595
27.508264	1210.936484	16.409613
27.624250	1204.237257	16.414631
27.535887	1212.140576	16.419648
27.218493	1206.803079	16.424666
27.572055	1199.444319	16.429683
27.377356	1204.564265	16.434701
27.925461	1203.506720	16.439719
27.593554	1218.567496	16.444736
27.886617	1230.630457	16.449754
28.052096	1233.915830	16.454771
27.910085	1234.948874	16.459789
28.229490	1224.923071	16.464807
27.969435	1231.364062	16.469824
28.283184	1226.725952	16.474842
28.295942	1232.903501	16.479859
28.317545	1225.995946	16.484877
28.028920	1194.889561	16.489895
27.737008	1204.406550	16.494912
28.209229	1214.260300	16.499930
28.130045	1224.804887	16.504947
28.062630	1231.201262	16.509965
28.274971	1219.177604	16.514983
28.169167	1228.364871	16.520000
28.115709	1229.845380	16.525018
28.631648	1219.607790	16.530035
28.209946	1231.005332	16.535053
28.246336	1228.746281	16.540071
27.817393	1229.794732	16.545088
28.486944	1230.588960	16.550106
28.312538	1226.283152	16.555123
28.285088	1223.048539	16.560141
28.544730	1226.875714	16.565159
28.451779	1231.546494	16.570176
28.903153	1235.116619	16.575194
28.934165	1227.637841	16.580211
28.687517	1227.130476	16.585229
28.528184	1232.129991	16.590247
28.317698	1223.296537	16.595264
28.795569	1239.548667	16.600282
29.088067	1247.380043	16.605299
28.621408	1248.922142	16.610317
29.250636	1238.255100	16.615335
29.174115	1232.034292	16.620352
28.796077	1230.102769	16.625370
28.575337	1217.393253	16.630387
28.666462	1226.403702	16.635405
28.743025	1236.472825	16.640423
29.103429	1243.257528	16.645440
29.163109	1237.217615	16.650458
29.407091	1242.176871	16.655475
29.065068	1237.552479	16.660493
29.409321	1240.166045	16.665511
29.057763	1227.073951	16.670528
29.203474	1225.621889	16.675546
29.534287	1225.366956	16.680563
28.994551	1224.013463	16.685581
29.299768	1220.848357	16.690599
29.219870	1228.019210	16.695616
29.396897	1241.495887	16.700634
29.342583	1234.089553	16.705651
29.320292	1249.452033	16.710669
29.437136	1239.545315	16.715687
29.775825	1245.498234	16.720704
29.470234	1231.819784	16.725722
29.502092	1227.515519	16.730739
29.245644	1238.035642	16.735757
29.179288	1243.145686	16.740775
29.364655	1249.397304	16.745792
29.269934	1234.790144	16.750810
29.372465	1248.160710	16.755827
29.345286	1241.013630	16.760845
29.517691	1240.489763	16.765863
29.446789	1240.712995	16.770880
29.261705	1247.493090	16.775898
29.777158	1245.315038	16.780915
29.786347	1261.355337	16.785933
29.957931	1267.805702	16.790951
30.081257	1271.947657	16.795968
30.033694	1283.273213	16.800986
30.283513	1268.253262	16.806003
29.750175	1265.476324	16.811021
30.152106	1263.446265	16.816039
30.224508	1254.361848	16.821056
29.912292	1253.583502	16.826074
30.106225	1247.494108	16.831091
30.112153	1264.338459	16.836109
30.485380	1261.245896	16.841127
30.216616	1251.278462	16.846144
29.752394	1248.804987	16.851162
29.901931	1248.241222	16.856179
29.803208	1261.655090	16.861197
30.366225	1268.887604	16.866215
30.021632	1271.017659	16.871232
30.154820	1264.036032	16.876250
30.430738	1256.890928	16.881267
30.444141	1264.955305	16.886285
30.657296	1261.250005	16.891303
30.490935	1268.621853	16.896320
30.330447	1270.913032	16.901338
30.563406	1255.978175	16.906355
30.237487	1262.275407	16.911373
30.044650	1268.071805	16.916391
30.223307	1266.350102	16.921408
30.312235	1273.281902	16.926426
30.744153	1276.421431	16.931443
30.719131	1294.331148	16.936461
30.797144	1292.021471	16.941479
30.885137	1288.594436	16.946496
30.741366	1295.153522	16.951514
30.958873	1282.309700	16.956531
30.586655	1287.466657	16.961549
30.835402	1297.940648	16.966567
30.949012	1284.660569	16.971584
30.970621	1294.612885	16.976602
30.960931	1288.336854	16.981619
30.888313	1285.748289	16.986637
30.791979	1286.949722	16.991655
30.886708	1278.408801	16.996672
30.690831	1283.716755	17.001690
30.701735	1276.153110	17.006707
30.672677	1280.128277	17.011725
30.907424	1277.124472	17.016743
31.335129	1290.151672	17.021760
31.423403	1304.120693	17.026778
31.823299	1293.405513	17.031795
31.731485	1275.664108	17.036813
31.929767	1267.444549	17.041831
31.912866	1264.774290	17.046848
32.075461	1275.298017	17.051866
31.993665	1257.971878	17.056883
31.834917	1244.258380	17.061901
31.801906	1232.898689	17.066919
31.563899	1234.249642	17.071936
31.291058	1241.596657	17.076954
31.450897	1232.746134	17.081971
31.245794	1236.755273	17.086989
31.573981	1236.985006	17.092007
31.764440	1231.069416	17.097024
31.214333	1243.828010	17.102042
31.766917	1246.505372	17.107059
31.558580	1255.096733	17.112077
31.801285	1265.816578	17.117095
31.900331	1249.461922	17.122112
31.733872	1255.706667	17.127130
31.965950	1253.248954	17.132147
31.561800	1258.410027	17.137165
31.478046	1260.599873	17.142183
32.066197	1255.537426	17.147200
31.708286	1265.428396	17.152218
32.031437	1257.377058	17.157235
31.933172	1262.776257	17.162253
31.900317	1257.544987	17.167271
31.814715	1252.031160	17.172288
31.984500	1280.943022	17.177306
32.353814	1281.875339	17.182323
32.457944	1292.508396	17.187341
32.214199	1286.957457	17.192359
32.567573	1284.035898	17.197376
32.085286	1295.556545	17.202394
32.024952	1281.675483	17.207411
32.451783	1293.484775	17.212429
32.188211	1282.011012	17.217447
32.534566	1290.679879	17.222464
32.319355	1283.586863	17.227482
32.600490	1287.958096	17.232499
32.406205	1287.032201	17.237517
32.257383	1293.922426	17.242535
32.257055	1288.737705	17.247552
32.272172	1287.839996	17.252570
32.325049	1298.155606	17.257587
32.573143	1286.708999	17.262605
32.488911	1306.490695	17.267623
32.579959	1315.621281	17.272640
32.538759	1313.168429	17.277658
32.685695	1314.956965	17.282675
32.787618	1319.704434	17.287693
32.885165	1322.490508	17.292711
32.924010	1326.378420	17.297728
32.692916	1326.164123	17.302746
32.902339	1323.980232	17.307763
32.895217	1311.584726	17.312781
33.042817	1331.146828	17.317799
33.451771	1322.307211	17.322816
32.878868	1324.085076	17.327834
33.534123	1317.610333	17.332851
33.759205	1321.936957	17.337869
33.473869	1317.337762	17.342887
33.300552	1310.101951	17.347904
33.309679	1320.189817	17.352922
33.845218	1305.739639	17.357939
33.461439	1315.673129	17.362957
33.847939	1311.258326	17.367975
33.838603	1291.396590	17.372992
33.431131	1291.399395	17.378010
33.358324	1276.683439	17.383027
33.533283	1279.933784	17.388045
33.286539	1275.741949	17.393063
33.849077	1290.401786	17.398080
33.409342	1284.546428	17.403098
33.557230	1302.716774	17.408115
33.999350	1308.236010	17.413133
33.744247	1294.747529	17.418151
33.636035	1295.165930	17.423168
33.394489	1301.875515	17.428186
33.846811	1298.300528	17.433203
33.786387	1307.787767	17.438221
33.682444	1314.469370	17.443239
33.555346	1308.493542	17.448256
33.233493	1316.260137	17.453274
33.699408	1306.091826	17.458291
33.635167	1312.769585	17.463309
33.566640	1333.579371	17.468327
33.953323	1333.980873	17.473344
34.029921	1334.453596	17.478362
34.116908	1340.191309	17.483379
34.527851	1330.569892	17.488397
34.743015	1342.606126	17.493415
34.770676	1320.792612	17.498432
34.262384	1314.736441	17.503450
34.296656	1298.184240	17.508467
34.183310	1293.650164	17.513485
34.587059	1317.526576	17.518503
34.835913	1317.344711	17.523520
34.446046	1303.717602	17.528538
34.512518	1294.073148	17.533555
34.637159	1290.498689	17.538573
34.468383	1296.111972	17.543591
34.440843	1291.421122	17.548608
34.286285	1292.996783	17.553626
34.395310	1310.218914	17.558643
34.174494	1309.704890	17.563661
34.386003	1325.687222	17.568679
34.533040	1331.463375	17.573696
34.471703	1322.919235	17.578714
34.656057	1326.895557	17.583731
34.593572	1321.363691	17.588749
34.155606	1332.876211	17.593767
34.529292	1334.194009	17.598784
34.686767	1353.752923	17.603802
34.817498	1357.183463	17.608819
35.303150	1348.944839	17.613837
34.976521	1370.307787	17.618855
35.054000	1352.578313	17.623872
35.105622	1354.294115	17.628890
34.930077	1352.977321	17.633907
35.225572	1342.281033	17.638925
34.930534	1357.152752	17.643943
35.114012	1345.271977	17.648960
35.040794	1339.452529	17.653978
35.066847	1350.946601	17.658995
35.170764	1342.491516	17.664013
35.539020	1365.088124	17.669031
35.689487	1364.713958	17.674048
35.530853	1370.553920	17.679066
35.718853	1373.145449	17.684083
35.933101	1348.380917	17.689101
35.604726	1342.469629	17.694119
35.684552	1334.234291	17.699136
35.507723	1343.136199	17.704154
35.328593	1341.840473	17.709171
35.565465	1355.677762	17.714189
35.287866	1366.086530	17.719207
35.758305	1366.260341	17.724224
36.003211	1375.564597	17.729242
35.721818	1382.807985	17.734259
36.058281	1363.509921	17.739277
35.683343	1376.589497	17.744295
36.026381	1364.833363	17.749312
36.076806	1365.180914	17.754330
35.811075	1366.836868	17.759347
36.045518	1359.848999	17.764365
35.764111	1370.933574	17.769383
36.322920	1361.658021	17.774400
35.965211	1368.683780	17.779418
36.143851	1366.998288	17.784435
36.215852	1367.754048	17.789453
36.153193	1371.077762	17.794471
36.394394	1367.856339	17.799488
36.396672	1368.588650	17.804506
36.129711	1371.152254	17.809523
36.192397	1358.651805	17.814541
36.330600	1387.680530	17.819559
36.640134	1385.952022	17.824576
36.596740	1390.958302	17.829594
36.736582	1388.225357	17.834611
36.783826	1387.982121	17.839629
36.871319	1387.862899	17.844647
36.751229	1380.494984	17.849664
36.703377	1369.340407	17.854682
36.530057	1388.838601	17.859699
36.948570	1373.804289	17.864717
36.887928	1390.939359	17.869735
36.693901	1381.339721	17.874752
36.626109	1380.347128	17.879770
36.912725	1390.428684	17.884787
36.702047	1377.731929	17.889805
36.826668	1382.147705	17.894823
37.141452	1384.241411	17.899840
36.992208	1385.718170	17.904858
37.293879	1388.266401	17.909875
37.251098	1385.659868	17.914893
36.944957	1394.115991	17.919911
37.002610	1392.105342	17.924928
37.039602	1387.664358	17.929946
36.888806	1390.538174	17.934963
37.250610	1378.677734	17.939981
36.862954	1386.835995	17.944999
36.844008	1398.402145	17.950016
37.086170	1414.411757	17.955034
37.108787	1417.428011	17.960051
37.621772	1414.572024	17.965069
37.497785	1421.701870	17.970087
37.158362	1419.476906	17.975104
37.429693	1418.344487	17.980122
37.087425	1417.249091	17.985139
37.493110	1418.787555	17.990157
37.723500	1451.363551	17.995175
37.924324	1444.712323	18.000192
38.239986	1437.840837	18.005210
37.731649	1435.973854	18.010227
37.977959	1426.288012	18.015245
37.884207	1439.802386	18.020263
38.251368	1431.286966	18.025280
38.139767	1417.738701	18.030298
37.710872	1420.903223	18.035315
38.217944	1427.008537	18.040333
38.347539	1430.573135	18.045351
38.022227	1416.195459	18.050368
38.047702	1426.339337	18.055386
37.845244	1436.514018	18.060403
38.145918	1447.576706	18.065421
37.956951	1449.086450	18.070439
38.316304	1447.307924	18.075456
38.371349	1443.839089	18.080474
38.456645	1450.869207	18.085491
38.518406	1445.499711	18.090509
38.286434	1444.376533	18.095527
38.862981	1436.245194	18.100544
38.590349	1432.754051	18.105562
38.323514	1445.942091	18.110579
38.432435	1437.865244	18.115597
38.633540	1434.927627	18.120615
38.633481	1424.560710	18.125632
38.577053	1430.855345	18.130650
38.490543	1435.307407	18.135667
38.469987	1443.265320	18.140685
38.748400	1461.960993	18.145703
38.783593	1461.836684	18.150720
39.188582	1469.210121	18.155738
38.963610	1472.756890	18.160755
38.756050	1460.742204	18.165773
38.693844	1468.152740	18.170791
38.936084	1469.091228	18.175808
38.873946	1453.801302	18.180826
38.951696	1464.945145	18.185843
39.165038	1458.107585	18.190861
39.292618	1461.224508	18.195879
39.019430	1467.805963	18.200896
38.917299	1458.050851	18.205914
38.970573	1484.955360	18.210931
39.154622	1490.991948	18.215949
39.260844	1492.416023	18.220967
39.465419	1486.450353	18.225984
39.642246	1480.197575	18.231002
39.764523	1491.668672	18.236019
39.737687	1479.860542	18.241037
39.661795	1486.682828	18.246055
39.640921	1485.257641	18.251072
39.792833	1482.380947	18.256090
39.761491	1482.493279	18.261107
39.836949	1479.605670	18.266125
39.826929	1487.195331	18.271143
39.971933	1483.647363	18.276160
39.975846	1484.766797	18.281178
39.850433	1489.280063	18.286195
40.124985	1482.638218	18.291213
40.326129	1481.554467	18.296231
40.119630	1480.343197	18.301248
40.200297	1487.067811	18.306266
40.346164	1486.986523	18.311283
40.404798	1477.125154	18.316301
40.373187	1482.101160	18.321319
39.950769	1480.536417	18.326336
40.323940	1482.971997	18.331354
40.600567	1491.330135	18.336371
40.356289	1482.430890	18.341389
40.415030	1479.409056	18.346407
39.799863	1482.806117	18.351424
39.887017	1467.289008	18.356442
39.715673	1476.786125	18.361459
39.991406	1484.904652	18.366477
40.225782	1502.852598	18.371495
39.845812	1523.543933	18.376512
40.488214	1514.941779	18.381530
40.108411	1527.420731	18.386547
40.596431	1527.712487	18.391565
40.518839	1543.474990	18.396583
40.819886	1540.294372	18.401600
40.928382	1538.274073	18.406618
40.954867	1548.797380	18.411635
41.215677	1541.018848	18.416653
41.108587	1544.185027	18.421671
41.053641	1550.142859	18.426688
41.250566	1527.763141	18.431706
41.030512	1542.631630	18.436723
41.487075	1541.574713	18.441741
41.433219	1536.332272	18.446759
41.095230	1538.606142	18.451776
41.212705	1528.710946	18.456794
41.351369	1528.086382	18.461811
41.430001	1526.436785	18.466829
41.629299	1535.473529	18.471847
41.630032	1530.589724	18.476864
41.563309	1529.883944	18.481882
41.632258	1539.088019	18.486899
41.563068	1538.936177	18.491917
42.201579	1531.783834	18.496935
41.654183	1523.195172	18.501952
41.874515	1528.371046	18.506970
41.681405	1531.058225	18.511987
41.638804	1528.496519	18.517005
42.022938	1531.514520	18.522023
41.957715	1532.673400	18.527040
41.778068	1530.876182	18.532058
41.732606	1531.057395	18.537075
41.758926	1529.418067	18.542093
42.093001	1528.714571	18.547111
41.655137	1523.493438	18.552128
42.056374	1520.331211	18.557146
41.981298	1539.281784	18.562163
42.278560	1529.109470	18.567181
42.139450	1528.593275	18.572199
41.841751	1533.793831	18.577216
42.008420	1521.929493	18.582234
41.999530	1544.039062	18.587251
41.953154	1555.471309	18.592269
42.405495	1557.950828	18.597287
42.203033	1562.075356	18.602304
42.181114	1556.185492	18.607322
42.317914	1562.842150	18.612339
42.473617	1554.544086	18.617357
42.325136	1555.175874	18.622375
42.274758	1563.124239	18.627392
42.585969	1573.511661	18.632410
42.884909	1574.166725	18.637427
42.986888	1577.566267	18.642445
43.115362	1584.107785	18.647463
43.066907	1577.045580	18.652480
43.119709	1573.477090	18.657498
42.694912	1574.550462	18.662515
43.192104	1579.098069	18.667533
43.189462	1583.784654	18.672551
42.840385	1589.804378	18.677568
43.457385	1578.012000	18.682586
43.374325	1578.505754	18.687603
42.886120	1583.350202	18.692621
43.474820	1579.108802	18.697639
43.064733	1584.628439	18.702656
43.344533	1579.274233	18.707674
43.232779	1580.912098	18.712691
43.060749	1584.439856	18.717709
43.426935	1581.556664	18.722727
43.478962	1588.392773	18.727744
43.597700	1579.131178	18.732762
43.784232	1585.552815	18.737779
43.263419	1579.963961	18.742797
43.668379	1578.806961	18.747815
43.278809	1578.383176	18.752832
43.331078	1591.854124	18.757850
43.643769	1605.412900	18.762867
43.310168	1612.490666	18.767885
43.658063	1607.721182	18.772903
43.520486	1611.564079	18.777920
43.729029	1622.509924	18.782938
44.035694	1625.148308	18.787955
44.262881	1632.674601	18.792973
44.519857	1623.073476	18.797991
44.218558	1624.172782	18.803008
44.422576	1612.694679	18.808026
44.145238	1615.365163	18.813043
44.349739	1620.979122	18.818061
44.496879	1619.293327	18.823079
44.200693	1631.105330	18.828096
44.469994	1625.747340	18.833114
44.300843	1630.004536	18.838131
44.329843	1634.171715	18.843149
44.498188	1628.684444	18.848167
44.313708	1631.022575	18.853184
44.485095	1625.381653	18.858202
44.596600	1625.488749	18.863219
44.625494	1635.546764	18.868237
44.739328	1631.488601	18.873255
45.009581	1629.781162	18.878272
44.730005	1615.472469	18.883290
44.784490	1633.861086	18.888307
44.795712	1655.417482	18.893325
45.096826	1650.873866	18.898343
45.078765	1663.327057	18.903360
45.606579	1651.407717	18.908378
45.590254	1643.405121	18.913395
45.254999	1625.928965	18.918413
45.424327	1625.954405	18.923431
45.380425	1622.496463	18.928448
45.361663	1623.599204	18.933466
45.261398	1618.330197	18.938483
45.293714	1622.248008	18.943501
45.526432	1619.804699	18.948519
45.269118	1615.367288	18.953536
45.235782	1627.729685	18.958554
45.262353	1641.944301	18.963571
45.392617	1652.141776	18.968589
45.636840	1654.227562	18.973607
45.457716	1656.725434	18.978624
45.540956	1657.645479	18.983642
45.758953	1650.135027	18.988659
45.788074	1657.939522	18.993677
45.698757	1652.632858	18.998695
45.629721	1659.884780	19.003712
45.919097	1656.897020	19.008730
46.141342	1674.777892	19.013747
46.272427	1670.046391	19.018765
46.422321	1674.693086	19.023783
46.097172	1653.041282	19.028800
46.019364	1643.346575	19.033818
46.464555	1650.947273	19.038835
46.376461	1671.478881	19.043853
46.483726	1670.691029	19.048871
46.289549	1675.625218	19.053888
46.471313	1675.588357	19.058906
46.443193	1666.998349	19.063923
46.377677	1671.461950	19.068941
46.313371	1658.815045	19.073959
46.039009	1672.887188	19.078976
46.267923	1666.659929	19.083994
46.299507	1679.007640	19.089011
46.162600	1686.923993	19.094029
46.580885	1697.416142	19.099047
46.912935	1710.298577	19.104064
46.722998	1699.576425	19.109082
47.007330	1704.869278	19.114099
46.805921	1695.615153	19.119117
47.116829	1703.292524	19.124135
46.961409	1702.655807	19.129152
47.075852	1697.040071	19.134170
47.326996	1697.236950	19.139187
47.004247	1702.183461	19.144205
47.297763	1701.837480	19.149223
46.887281	1709.534356	19.154240
46.943944	1732.899814	19.159258
47.639690	1725.315436	19.164275
47.586970	1735.535110	19.169293
47.852954	1726.935559	19.174311
47.560251	1724.550031	19.179328
47.935777	1718.033035	19.184346
48.126896	1716.557240	19.189363
47.996115	1714.553457	19.194381
47.977453	1700.862334	19.199399
47.805665	1690.329688	19.204416
47.877755	1699.871520	19.209434
48.142611	1692.662310	19.214451
47.854237	1704.405748	19.219469
48.003345	1686.373835	19.224487
47.998571	1694.927275	19.229504
47.680262	1715.425550	19.234522
48.158528	1711.749704	19.239539
47.810785	1724.325845	19.244557
47.905580	1717.288980	19.249575
48.065877	1716.043894	19.254592
48.177826	1713.572218	19.259610
48.167561	1712.938541	19.264627
48.261525	1727.851079	19.269645
48.644966	1710.935293	19.274663
48.569184	1716.311621	19.279680
48.184730	1721.169970	19.284698
48.520705	1739.251303	19.289715
48.407671	1742.186230	19.294733
48.791634	1749.625108	19.299751
48.607766	1740.526700	19.304768
48.575454	1756.429136	19.309786
49.029174	1746.660986	19.314803
48.672197	1758.901687	19.319821
48.737185	1753.103995	19.324839
48.771890	1742.582664	19.329856
48.449002	1756.646412	19.334874
48.886603	1750.293887	19.339891
49.035763	1763.059520	19.344909
49.343870	1759.072183	19.349927
49.408025	1760.584376	19.354944
49.283052	1765.694491	19.359962
49.723881	1759.545360	19.364979
49.554960	1748.168115	19.369997
49.462282	1740.313196	19.375015
49.473103	1734.467821	19.380032
49.691108	1739.366204	19.385050
49.929830	1724.014590	19.390067
49.412864	1734.212996	19.395085
49.492963	1728.119105	19.400103
49.732036	1736.425352	19.405120
49.824643	1756.895544	19.410138
50.036435	1746.061712	19.415155
49.659012	1750.766541	19.420173
49.831603	1746.808817	19.425191
49.971513	1757.994509	19.430208
50.208541	1760.487800	19.435226
50.086670	1751.666479	19.440243
50.035564	1752.119495	19.445261
50.035838	1750.478567	19.450279
50.369376	1751.886540	19.455296
50.028376	1752.330256	19.460314
50.309518	1745.276580	19.465331
50.145650	1750.751024	19.470349
50.134577	1748.160026	19.475367
50.156866	1757.723163	19.480384
49.981293	1754.195343	19.485402
50.194024	1770.267695	19.490419
50.123286	1781.368729	19.495437
50.174253	1777.719396	19.500455
50.561747	1777.904246	19.505472
50.677576	1781.016101	19.510490
50.664083	1784.637239	19.515507
50.664738	1797.378763	19.520525
50.728028	1811.660660	19.525543
51.073439	1806.540745	19.530560
50.976187	1812.298230	19.535578
51.143142	1794.602199	19.540595
51.039287	1808.455184	19.545613
50.975180	1810.144602	19.550631
51.011421	1812.575209	19.555648
50.878449	1814.523315	19.560666
51.281337	1793.615269	19.565683
51.130627	1794.112005	19.570701
51.596495	1802.870747	19.575719
51.232685	1801.902127	19.580736
51.532242	1827.745838	19.585754
51.642176	1829.286650	19.590771
51.465978	1834.342309	19.595789
51.515938	1829.354166	19.600807
51.856779	1825.113738	19.605824
51.422252	1823.708055	19.610842
51.760005	1830.193244	19.615859
51.934589	1825.448167	19.620877
51.719542	1831.117757	19.625895
51.899656	1827.225298	19.630912
51.844967	1833.742640	19.635930
51.848018	1813.252984	19.640947
51.996097	1821.611407	19.645965
51.667363	1822.880638	19.650983
52.359442	1830.747477	19.656000
52.213484	1849.188954	19.661018
52.324995	1848.976368	19.666035
52.226550	1851.129762	19.671053
52.339086	1854.776034	19.676071
52.381592	1845.802538	19.681088
52.287697	1852.520497	19.686106
52.432016	1851.935926	19.691123
52.388362	1849.055053	19.696141
52.259574	1850.711131	19.701159
52.717432	1855.058668	19.706176
52.705450	1864.984650	19.711194
53.043219	1871.449381	19.716211
53.081175	1884.331627	19.721229
52.935593	1883.102718	19.726247
53.046140	1881.487938	19.731264
52.745099	1884.401775	19.736282
53.050932	1876.548665	19.741299
53.219515	1870.076629	19.746317
52.953485	1878.827133	19.751335
53.302332	1874.874335	19.756352
53.227394	1877.695869	19.761370
53.568128	1869.484602	19.766387
53.471002	1874.730676	19.771405
53.353399	1875.034117	19.776423
53.808121	1861.222053	19.781440
53.353280	1877.218064	19.786458
53.370070	1871.242906	19.791475
53.679659	1872.661564	19.796493
53.425556	1874.480596	19.801511
53.926107	1881.945044	19.806528
53.456364	1898.875439	19.811546
53.861887	1902.950586	19.816563
53.905707	1895.489043	19.821581
54.075403	1907.384062	19.826599
53.991537	1897.949257	19.831616
53.826133	1907.336987	19.836634
54.020654	1902.625976	19.841651
54.152407	1897.210833	19.846669
54.020044	1908.419050	19.851687
54.410474	1900.350688	19.856704
54.224460	1896.084022	19.861722
54.433678	1918.443308	19.866739
54.390511	1935.830799	19.871757
54.413026	1940.597562	19.876775
54.549367	1932.050153	19.881792
54.648748	1942.579330	19.886810
54.512878	1933.001178	19.891827
54.490186	1943.238832	19.896845
54.715486	1934.865614	19.901863
54.779134	1940.013729	19.906880
54.816539	1939.089050	19.911898
55.034036	1926.624226	19.916915
54.777163	1930.727578	19.921933
54.527609	1953.980088	19.926951
54.595657	1962.966455	19.931968
54.857946	1967.620149	19.936986
55.120584	1957.740712	19.942003
55.442018	1957.769221	19.947021
55.204009	1957.798974	19.952039
55.177074	1954.412154	19.957056
55.057378	1964.252558	19.962074
55.643965	1977.283070	19.967091
55.949102	1976.859169	19.972109
55.810643	1981.068052	19.977127
56.029977	1956.591470	19.982144
55.943422	1947.091728	19.987162
56.054951	1943.035835	19.992179
56.172489	1937.198632	19.997197
56.135068	1942.377719	20.002215
56.114822	1933.949247	20.007232
55.886631	1943.610819	20.012250
55.772586	1938.203836	20.017267
56.253478	1926.447204	20.022285
56.069564	1939.685660	20.027303
56.010439	1929.368379	20.032320
56.127503	1950.030824	20.037338
56.479091	1961.032270	20.042355
56.648634	1965.842716	20.047373
56.584364	1972.552260	20.052391
56.713056	1971.140754	20.057408
56.473423	1979.038501	20.062426
56.531310	1973.182852	20.067443
56.849605	1973.515032	20.072461
56.514325	1966.544019	20.077479
56.553290	1970.895853	20.082496
56.758985	1962.629027	20.087514
56.377977	1960.326641	20.092531
56.685341	1970.855523	20.097549
56.534464	1979.236551	20.102567
56.639164	1994.760161	20.107584
56.457170	2002.860939	20.112602
56.568266	2001.053141	20.117619
56.749604	2013.458119	20.122637
56.681468	2020.294704	20.127655
57.060339	2032.295214	20.132672
57.261813	2025.967648	20.137690
57.790242	2020.813704	20.142707
57.795545	2023.012084	20.147725
57.668130	2030.220731	20.152743
57.714544	2013.736222	20.157760
57.645248	2025.513177	20.162778
57.778676	2024.884740	20.167795
57.684636	2015.903525	20.172813
57.923767	2021.275653	20.177831
57.994564	2012.729251	20.182848
58.187294	2019.015786	20.187866
57.752734	2011.269123	20.192883
58.080182	2020.973439	20.197901
58.596490	2042.145641	20.202919
58.872239	2042.967968	20.207936
58.530784	2022.109306	20.212954
58.406480	2019.511097	20.217971
58.838325	2019.054326	20.222989
58.681354	2005.472141	20.228007
58.603346	2011.349731	20.233024
58.906976	2011.944193	20.238042
58.875839	2012.376968	20.243059
58.822782	2014.190557	20.248077
58.665264	2013.851814	20.253095
58.392113	2004.730292	20.258112
58.514925	2009.365841	20.263130
58.591482	2022.332731	20.268147
58.818310	2032.660078	20.273165
58.741437	2039.683558	20.278183
58.998073	2039.224802	20.283200
59.037989	2046.910769	20.288218
58.871901	2038.865535	20.293235
59.001790	2029.277014	20.298253
59.131425	2047.448513	20.303271
59.186591	2025.345184	20.308288
59.312485	2041.226343	20.313306
59.447522	2061.398546	20.318323
59.732802	2052.238519	20.323341
59.593102	2060.233085	20.328359
59.909104	2059.592809	20.333376
59.740020	2060.541034	20.338394
59.586650	2057.735050	20.343411
59.965007	2058.429694	20.348429
59.759159	2054.920616	20.353447
59.815046	2055.597986	20.358464
59.882991	2056.784773	20.363482
59.981571	2060.258609	20.368499
60.125297	2051.350456	20.373517
60.152466	2056.387743	20.378535
60.056119	2048.671073	20.383552
60.082905	2052.695819	20.388570
59.973726	2059.646329	20.393587
60.562239	2061.190698	20.398605
60.322972	2076.166040	20.403623
60.761313	2072.558559	20.408640
60.770291	2079.375267	20.413658
60.541381	2085.979150	20.418675
60.822257	2080.310813	20.423693
61.092687	2081.876157	20.428711
60.832269	2081.468293	20.433728
61.085211	2081.201884	20.438746
60.408448	2083.589219	20.443763
60.894429	2081.647848	20.448781
61.182155	2076.425621	20.453799
60.832877	2077.917184	20.458816
60.829560	2081.398904	20.463834
61.120608	2109.021679	20.468851
61.323844	2103.533167	20.473869
61.217150	2114.992780	20.478887
61.503726	2113.423524	20.483904
61.809302	2109.168408	20.488922
61.740717	2108.723543	20.493939
62.084993	2105.676968	20.498957
61.860251	2103.098193	20.503975
62.007919	2101.270919	20.508992
62.109796	2107.390305	20.514010
61.981537	2108.232535	20.519027
62.267042	2101.602388	20.524045
62.082992	2104.533830	20.529063
62.055347	2102.538446	20.534080
62.118349	2095.301180	20.539098
62.171019	2106.583513	20.544115
62.411999	2101.843066	20.549133
62.336604	2104.078098	20.554151
62.190548	2106.420937	20.559168
62.043635	2105.286721	20.564186
62.212224	2104.229993	20.569203
62.310331	2096.962876	20.574221
62.180164	2106.743298	20.579239
62.482229	2114.813294	20.584256
62.787369	2116.313425	20.589274
62.593031	2130.056929	20.594291
62.590419	2121.328177	20.599309
62.894972	2125.630010	20.604327
62.632468	2127.105582	20.609344
62.846528	2141.189888	20.614362
62.739195	2149.796451	20.619379
63.090416	2145.779018	20.624397
63.025399	2154.570285	20.629415
63.181720	2150.458075	20.634432
63.185144	2143.725182	20.639450
63.159628	2150.601198	20.644467
63.061632	2148.562775	20.649485
63.406674	2168.232100	20.654503
63.116881	2170.626790	20.659520
63.377582	2175.479633	20.664538
63.282283	2177.631367	20.669555
63.738013	2187.478644	20.674573
63.440496	2184.386745	20.679591
63.771729	2195.376781	20.684608
64.323341	2198.100938	20.689626
64.128636	2212.397340	20.694643
64.392288	2209.916122	20.699661
64.114340	2207.731217	20.704679
64.221711	2206.801981	20.709696
64.676885	2201.260541	20.714714
64.449023	2209.451334	20.719731
64.708026	2199.373527	20.724749
64.680695	2206.451054	20.729767
64.478710	2209.176437	20.734784
64.889162	2194.045825	20.739802
64.549902	2203.903973	20.744819
64.782025	2196.035000	20.749837
64.797119	2196.449861	20.754855
64.469767	2208.637170	20.759872
64.790413	2200.974747	20.764890
64.865593	2206.801360	20.769907
64.863236	2199.276872	20.774925
64.994929	2205.743709	20.779943
65.117041	2226.407652	20.784960
65.415668	2218.366983	20.789978
65.437314	2225.088342	20.794995
65.041319	2226.683747	20.800013
65.149824	2232.630424	20.805031
64.961832	2245.348548	20.810048
65.117233	2233.082385	20.815066
65.213523	2257.220014	20.820083
65.880874	2243.751022	20.825101
66.039664	2248.315307	20.830119
66.015495	2258.879405	20.835136
66.103408	2246.369325	20.840154
66.113840	2252.894131	20.845171
66.465908	2245.374498	20.850189
66.543535	2248.130979	20.855207
66.339390	2250.943738	20.860224
66.428876	2242.735055	20.865242
66.765690	2250.370599	20.870259
66.738797	2230.364512	20.875277
67.028178	2232.518073	20.880295
66.669693	2222.475155	20.885312
66.987731	2201.899173	20.890330
66.955105	2195.990371	20.895347
66.915533	2190.419739	20.900365
66.722686	2197.440516	20.905383
66.400153	2188.951118	20.910400
66.925922	2204.105349	20.915418
67.025948	2220.672892	20.920435
66.638119	2228.033966	20.925453
67.122533	2222.128598	20.930471
66.798487	2227.709752	20.935488
67.320869	2218.393293	20.940506
67.106357	2233.409947	20.945523
66.803027	2228.610314	20.950541
66.964648	2247.668086	20.955559
67.026369	2255.744240	20.960576
67.376479	2249.604091	20.965594
67.193787	2260.973290	20.970611
67.408475	2268.068105	20.975629
67.543633	2289.022883	20.980647
67.431901	2293.468358	20.985664
67.839517	2293.467979	20.990682
67.495161	2284.615612	20.995699
67.751014	2282.181743	21.000717
68.070563	2284.148010	21.005735
67.884127	2297.687195	21.010752
68.409280	2306.462358	21.015770
68.576305	2305.875178	21.020787
68.868276	2303.788855	21.025805
68.784658	2297.787306	21.030823
68.497293	2281.846182	21.035840
68.700622	2276.867448	21.040858
68.518773	2292.687409	21.045875
68.691884	2292.747264	21.050893
69.066651	2302.732482	21.055911
68.996408	2309.252608	21.060928
69.016737	2297.915162	21.065946
69.128588	2305.801117	21.070963
69.233547	2305.028973	21.075981
69.139976	2304.556757	21.080999
68.990443	2305.155283	21.086016
69.019318	2302.516215	21.091034
69.277747	2303.185920	21.096051
69.315657	2300.544956	21.101069
69.541961	2313.917921	21.106087
69.358633	2310.013301	21.111104
69.534076	2308.450685	21.116122
69.525985	2319.165698	21.121139
69.404998	2329.672705	21.126157
69.511371	2333.125228	21.131175
69.408878	2332.801742	21.136192
69.885806	2326.790884	21.141210
69.692218	2340.977767	21.146227
69.908354	2352.249648	21.151245
70.511643	2362.655994	21.156263
70.297521	2367.206303	21.161280
70.270754	2354.648657	21.166298
70.522104	2358.724747	21.171315
70.269770	2353.049648	21.176333
71.066856	2349.959665	21.181351
71.043478	2348.820254	21.186368
70.509508	2356.032443	21.191386
70.509387	2347.985844	21.196403
70.682976	2358.467143	21.201421
71.035446	2351.308819	21.206439
70.937198	2360.467152	21.211456
70.747408	2352.344589	21.216474
70.863267	2348.428820	21.221491
70.841922	2357.896032	21.226509
71.174287	2365.283941	21.231527
71.112283	2384.149906	21.236544
71.105082	2382.692442	21.241562
70.973376	2374.104690	21.246579
70.843652	2380.976866	21.251597
71.184555	2384.658542	21.256615
71.291320	2405.982773	21.261632
71.577574	2404.926550	21.266650
71.515619	2414.486768	21.271667
71.722137	2417.733685	21.276685
71.822799	2409.148243	21.281703
71.911737	2423.740623	21.286720
72.051433	2427.321492	21.291738
72.314000	2446.876133	21.296755
71.933320	2446.251228	21.301773
72.408257	2437.856726	21.306791
71.972103	2444.246769	21.311808
72.653928	2440.084552	21.316826
72.204446	2441.201056	21.321843
72.120602	2441.268576	21.326861
72.793924	2440.122432	21.331879
72.875648	2441.770359	21.336896
72.749450	2432.156037	21.341914
72.827477	2454.365453	21.346931
73.173911	2459.862033	21.351949
73.760410	2448.294160	21.356967
72.949770	2438.250258	21.361984
73.129554	2432.663557	21.367002
73.412216	2428.778317	21.372019
72.995712	2444.547269	21.377037
73.589462	2438.545695	21.382055
73.328052	2450.752943	21.387072
73.612023	2445.839889	21.392090
73.610047	2456.201608	21.397107
73.449212	2444.312254	21.402125
73.520840	2452.981371	21.407143
73.243332	2456.153614	21.412160
73.422034	2452.207690	21.417178
73.727262	2466.656681	21.422195
73.815419	2481.796901	21.427213
73.991178	2479.444819	21.432231
74.041042	2484.797776	21.437248
74.178728	2481.876805	21.442266
74.082213	2483.950434	21.447283
74.076665	2488.583442	21.452301
74.510423	2494.204110	21.457319
74.361656	2503.502816	21.462336
74.382763	2500.220495	21.467354
74.369818	2500.462064	21.472371
74.665424	2496.068733	21.477389
74.805558	2492.940259	21.482407
74.977438	2494.557067	21.487424
75.003306	2486.925382	21.492442
74.974931	2493.036645	21.497459
75.030664	2508.599223	21.502477
75.349197	2516.583226	21.507495
75.400219	2524.002612	21.512512
75.543474	2521.559466	21.517530
75.502067	2516.537073	21.522547
75.480703	2535.583088	21.527565
75.950026	2518.202533	21.532583
75.780102	2513.713723	21.537600
75.761032	2521.007350	21.542618
75.928507	2514.974618	21.547635
75.680461	2519.980626	21.552653
75.654045	2515.802229	21.557671
75.875047	2526.080085	21.562688
75.808576	2514.465163	21.567706
75.995307	2534.012439	21.572723
76.149131	2547.071654	21.577741
76.442838	2540.784067	21.582759
76.208054	2547.660390	21.587776
76.183224	2546.171587	21.592794
76.405901	2546.591330	21.597811
76.477227	2543.940441	21.602829
76.632044	2555.177383	21.607847
76.647916	2575.107450	21.612864
76.624026	2572.194416	21.617882
77.062076	2569.412495	21.622899
76.885761	2581.927764	21.627917
77.194141	2571.237156	21.632935
77.107062	2581.933193	21.637952
77.059655	2565.309354	21.642970
77.468966	2569.461614	21.647987
77.468698	2576.281652	21.653005
77.574500	2570.420572	21.658023
77.212410	2585.542409	21.663040
77.277801	2594.430367	21.668058
77.739613	2600.533833	21.673075
77.574988	2595.017698	21.678093
77.790685	2601.876662	21.683111
78.154727	2595.990766	21.688128
77.706461	2587.918516	21.693146
78.146726	2593.882247	21.698163
77.975679	2600.641698	21.703181
78.342662	2595.075406	21.708199
78.259270	2590.632824	21.713216
78.197609	2606.748103	21.718234
78.340521	2616.287391	21.723251
78.207730	2627.480053	21.728269
78.197647	2621.793337	21.733287
78.169838	2622.908676	21.738304
78.199147	2630.755756	21.743322
78.667203	2641.728883	21.748339
78.667924	2643.548962	21.753357
79.004523	2648.046807	21.758375
79.161187	2645.983713	21.763392
79.395171	2643.602638	21.768410
79.421076	2634.643652	21.773427
79.272413	2648.871776	21.778445
79.329568	2640.952127	21.783463
79.312136	2649.583397	21.788480
79.834486	2663.933494	21.793498
80.241673	2670.678772	21.798515
80.119713	2667.050096	21.803533
80.027900	2640.665399	21.808551
79.691889	2650.964645	21.813568
79.581341	2664.428541	21.818586
80.018485	2660.164405	21.823603
79.987785	2674.572563	21.828621
80.089633	2660.060531	21.833639
80.371393	2665.836843	21.838656
80.341211	2671.183087	21.843674
80.517786	2660.920641	21.848691
80.406969	2671.287992	21.853709
80.662906	2670.665944	21.858727
80.832777	2688.070842	21.863744
80.906268	2686.279846	21.868762
80.804635	2694.830247	21.873779
80.887289	2690.298228	21.878797
81.144089	2684.551388	21.883815
81.253969	2681.427905	21.888832
81.042619	2693.218736	21.893850
81.431236	2682.579288	21.898867
81.150000	2685.014760	21.903885
81.344005	2699.915938	21.908903
81.280663	2690.880409	21.913920
81.012550	2706.858833	21.918938
82.015026	2714.187122	21.923955
81.454545	2717.582437	21.928973
81.942280	2714.351268	21.933991
81.685355	2719.106833	21.939008
81.562889	2722.610860	21.944026
81.873964	2718.993281	21.949043
81.919134	2742.604306	21.954061
81.813399	2743.360932	21.959079
81.994577	2753.822732	21.964096
82.134492	2752.308892	21.969114
82.347058	2748.959265	21.974131
82.282697	2764.386538	21.979149
82.647603	2772.170042	21.984167
82.599815	2774.265535	21.989184
82.679908	2775.207826	21.994202
82.731624	2779.669191	21.999219
82.737968	2782.202169	22.004237
83.072443	2779.108274	22.009255
83.072639	2774.400948	22.014272
82.950709	2787.278228	22.019290
83.342410	2789.800711	22.024307
83.339994	2800.194230	22.029325
83.624952	2799.223241	22.034343
84.042789	2783.797904	22.039360
83.726683	2795.443614	22.044378
83.925600	2796.859493	22.049395
83.723987	2798.030895	22.054413
83.781237	2790.924191	22.059431
83.700138	2793.190978	22.064448
83.726628	2791.304232	22.069466
84.103849	2798.579378	22.074483
84.004354	2798.473899	22.079501
83.883087	2788.697504	22.084519
84.083334	2798.922295	22.089536
84.202019	2819.072608	22.094554
84.452592	2825.632553	22.099571
84.372959	2823.449248	22.104589
84.579542	2824.392570	22.109607
84.953818	2819.896306	22.114624
84.855587	2827.744602	22.119642
84.935008	2836.073642	22.124659
84.918240	2844.334416	22.129677
84.861970	2848.776343	22.134695
85.086168	2843.725453	22.139712
85.274341	2848.687812	22.144730
85.258940	2836.412944	22.149747
85.265825	2840.990839	22.154765
85.532434	2869.100945	22.159783
86.146625	2866.260172	22.164800
85.731364	2878.505921	22.169818
85.938958	2875.374035	22.174835
85.704697	2877.934414	22.179853
85.971270	2873.308782	22.184871
86.082111	2881.151101	22.189888
85.799706	2890.438386	22.194906
86.223389	2879.534301	22.199923
86.505865	2875.009574	22.204941
86.225671	2872.985979	22.209959
86.421217	2885.244404	22.214976
86.581094	2897.426479	22.219994
86.739685	2888.633102	22.225011
86.908580	2895.746840	22.230029
86.750322	2895.214486	22.235047
86.674687	2886.015915	22.240064
86.789790	2892.176329	22.245082
86.759507	2890.033242	22.250099
86.770448	2911.389052	22.255117
86.840677	2913.272025	22.260135
87.472889	2918.153920	22.265152
86.893428	2921.943794	22.270170
87.467985	2916.127919	22.275187
87.782027	2940.504059	22.280205
87.726684	2948.315758	22.285223
88.040371	2945.215443	22.290240
88.250139	2939.111736	22.295258
88.564798	2943.771985	22.300275
88.311532	2932.781926	22.305293
88.236332	2929.608832	22.310311
88.615004	2929.288839	22.315328
88.671427	2938.400939	22.320346
88.643684	2931.453973	22.325363
88.645684	2926.241939	22.330381
88.530907	2938.781127	22.335399
88.907653	2924.507040	22.340416
88.648935	2944.379663	22.345434
88.925281	2928.773353	22.350451
88.953202	2929.176259	22.355469
88.913009	2924.855938	22.360487
89.335074	2918.962249	22.365504
89.139094	2924.642451	22.370522
89.161545	2923.464278	22.375539
88.998835	2929.037372	22.380557
88.711465	2922.281203	22.385575
89.141002	2938.811682	22.390592
89.335814	2953.460985	22.395610
89.403795	2949.201426	22.400627
89.392071	2966.056068	22.405645
89.503683	2967.958157	22.410663
89.807124	2972.426960	22.415680
89.376349	2988.107878	22.420698
89.902430	2976.478001	22.425715
89.819026	2992.739034	22.430733
90.329510	3007.607992	22.435751
90.770590	3006.657507	22.440768
90.543073	3010.132990	22.445786
90.788964	3002.470395	22.450803
90.931280	3009.429536	22.455821
90.647456	3008.755829	22.460839
91.219622	3006.581903	22.465856
90.992617	3013.101207	22.470874
91.050243	3007.339708	22.475891
91.405625	3016.209244	22.480909
91.093821	3004.124063	22.485927
91.252008	2997.860784	22.490944
91.660418	3017.441124	22.495962
91.640567	3032.920324	22.500979
91.831079	3027.982461	22.505997
91.547246	3029.549066	22.511015
91.897733	3031.512259	22.516032
91.695522	3030.708838	22.521050
91.865310	3024.697574	22.526067
92.164502	3032.427954	22.531085
91.894163	3032.969806	22.536103
91.774505	3040.485131	22.541120
91.822808	3049.485645	22.546138
92.012536	3057.516138	22.551155
92.587288	3061.937123	22.556173
92.505325	3055.635772	22.561191
93.010831	3075.195324	22.566208
93.049118	3079.315282	22.571226
92.967073	3076.004702	22.576243
93.290473	3069.981674	22.581261
93.372119	3082.269814	22.586279
93.534339	3077.220094	22.591296
93.482127	3079.011222	22.596314
93.437681	3076.357040	22.601331
93.579749	3077.964296	22.606349
93.627181	3076.504775	22.611367
93.951734	3067.782937	22.616384
94.111307	3077.252413	22.621402
93.662264	3072.520040	22.626419
93.505583	3076.592471	22.631437
93.486841	3076.064485	22.636455
93.635566	3087.641432	22.641472
94.046078	3101.181328	22.646490
94.152336	3116.611699	22.651507
93.897884	3113.135655	22.656525
94.004423	3117.315545	22.661543
93.895293	3128.934193	22.666560
94.159231	3140.099876	22.671578
94.234407	3138.950330	22.676595
94.586105	3161.053457	22.681613
94.612509	3168.214230	22.686631
94.741525	3165.720197	22.691648
94.810464	3170.836344	22.696666
94.953780	3176.285040	22.701683
95.397856	3190.870306	22.706701
95.166830	3199.016862	22.711719
95.181233	3196.980095	22.716736
95.384602	3197.721597	22.721754
95.073490	3204.633334	22.726771
95.460927	3197.105795	22.731789
95.567469	3212.108227	22.736807
95.880296	3215.427024	22.741824
95.984980	3217.644099	22.746842
96.065580	3213.371346	22.751859
96.436433	3213.781448	22.756877
96.046250	3221.739093	22.761895
96.616706	3225.687180	22.766912
97.049570	3239.118749	22.771930
96.987645	3230.153543	22.776947
97.732039	3223.360043	22.781965
97.158042	3214.042507	22.786983
97.313162	3198.424577	22.792000
97.296637	3194.855033	22.797018
96.962791	3205.324373	22.802035
97.386091	3204.276037	22.807053
97.398090	3215.115897	22.812071
97.240645	3220.659870	22.817088
97.290675	3224.180622	22.822106
97.603445	3223.770388	22.827123
97.641718	3215.814606	22.832141
97.549661	3234.673207	22.837159
97.880484	3243.525300	22.842176
98.299252	3246.483162	22.847194
98.240127	3260.972970	22.852211
98.628250	3256.238830	22.857229
98.444395	3265.180404	22.862247
98.261084	3252.602770	22.867264
98.565034	3259.828494	22.872282
98.665172	3258.429888	22.877299
99.254688	3249.748963	22.882317
98.747903	3262.118890	22.887335
99.100222	3247.638316	22.892352
98.813474	3252.329307	22.897370
98.658483	3260.202607	22.902387
99.121461	3267.177872	22.907405
98.935950	3278.310070	22.912423
98.900837	3282.207220	22.917440
98.962633	3291.462740	22.922458
99.068365	3295.597139	22.927475
99.329297	3301.142485	22.932493
99.426492	3310.252752	22.937511
99.324982	3313.186449	22.942528
99.721561	3333.530637	22.947546
99.743237	3340.533600	22.952563
99.781633	3339.714982	22.957581
99.792524	3350.642136	22.962599
100.246873	3361.781455	22.967616
100.536316	3360.110020	22.972634
100.258429	3364.425522	22.977651
100.780986	3354.683918	22.982669
100.688719	3372.905262	22.987687
100.850698	3382.877718	22.992704
101.182993	3388.553769	22.997722
101.174898	3391.951923	23.002739
101.251432	3372.510700	23.007757
101.797186	3392.897505	23.012775
101.893050	3384.923798	23.017792
102.104018	3376.391941	23.022810
101.991746	3379.708970	23.027827
102.065057	3367.062217	23.032845
102.044599	3357.352185	23.037863
101.652423	3349.843098	23.042880
102.048378	3361.271674	23.047898
102.142575	3372.060184	23.052915
102.182491	3364.482435	23.057933
102.586842	3372.424270	23.062951
102.160115	3369.504797	23.067968
102.394952	3366.836439	23.072986
102.132814	3380.398591	23.078003
102.186504	3376.785050	23.083021
102.195145	3398.762045	23.088039
102.493435	3402.793207	23.093056
102.548430	3407.390834	23.098074
102.330716	3429.739772	23.103091
102.772412	3441.593916	23.108109
102.889125	3442.467165	23.113127
102.927356	3458.137153	23.118144
103.455985	3456.084589	23.123162
103.913795	3454.673382	23.128179
104.048636	3452.598061	23.133197
104.468088	3451.675558	23.138215
104.202125	3451.287471	23.143232
104.637938	3450.731183	23.148250
104.432183	3449.862573	23.153267
104.593401	3436.795211	23.158285
104.653096	3440.003746	23.163303
104.522208	3440.641738	23.168320
105.029779	3444.074692	23.173338
104.790145	3458.876204	23.178355
105.039867	3439.709689	23.183373
104.829237	3442.405221	23.188391
104.690183	3449.045929	23.193408
105.020245	3438.694863	23.198426
105.033509	3453.987071	23.203443
105.463809	3465.289925	23.208461
104.956895	3461.908123	23.213479
104.946427	3473.676001	23.218496
105.118196	3471.051181	23.223514
104.941202	3489.009942	23.228531
105.269435	3497.032214	23.233549
105.377587	3504.192549	23.238567
105.042174	3526.882083	23.243584
105.604743	3535.503686	23.248602
106.153184	3546.110519	23.253619
106.277649	3553.390620	23.258637
106.276598	3557.577877	23.263655
106.571160	3554.214848	23.268672
107.314941	3548.096185	23.273690
106.775748	3557.633645	23.278707
106.969219	3543.781226	23.283725
107.176177	3545.155678	23.288743
106.918783	3548.016102	23.293760
107.533526	3561.653971	23.298778
107.512029	3577.714359	23.303795
107.859597	3571.414655	23.308813
107.852181	3571.554525	23.313831
107.662550	3574.267064	23.318848
108.056682	3574.470138	23.323866
107.681118	3577.749459	23.328883
107.986513	3578.673258	23.333901
107.800977	3579.639268	23.338919
107.788501	3577.575025	23.343936
108.196819	3573.160303	23.348954
108.190268	3593.003261	23.353971
107.929260	3601.654272	23.358989
108.211156	3601.885842	23.364007
108.410469	3601.472799	23.369024
108.704930	3606.228742	23.374042
108.521128	3629.082619	23.379059
108.814424	3632.101964	23.384077
109.103310	3643.076442	23.389095
109.223534	3631.631652	23.394112
109.193262	3633.606226	23.399130
108.866743	3645.355093	23.404147
109.241840	3652.115585	23.409165
109.311017	3668.661446	23.414183
109.548868	3667.173376	23.419200
109.539987	3664.119834	23.424218
109.668073	3683.429846	23.429235
109.773875	3691.289161	23.434253
110.228328	3693.080422	23.439271
110.351718	3692.760318	23.444288
110.604196	3679.937852	23.449306
110.066568	3702.689594	23.454323
109.994644	3713.004315	23.459341
110.115111	3716.476067	23.464359
109.986848	3726.820635	23.469376
110.894518	3740.193423	23.474394
110.890866	3745.454907	23.479411
111.074651	3749.786717	23.484429
111.491039	3752.899029	23.489447
111.501053	3770.569918	23.494464
111.891473	3775.137900	23.499482
111.796887	3772.345852	23.504499
112.131384	3770.898017	23.509517
112.280735	3767.225571	23.514535
112.152077	3780.077617	23.519552
112.343455	3763.674267	23.524570
112.320578	3767.496268	23.529587
112.632608	3772.390304	23.534605
112.552937	3762.919414	23.539623
112.288553	3763.621733	23.544640
112.599412	3761.692339	23.549658
112.726405	3764.195189	23.554675
112.595395	3776.787356	23.559693
112.547852	3797.604821	23.564711
112.703244	3802.611128	23.569728
112.697412	3797.802908	23.574746
112.874171	3822.336723	23.579763
113.129116	3823.613058	23.584781
113.898745	3828.048739	23.589799
113.695260	3821.174682	23.594816
113.826323	3816.556331	23.599834
114.093912	3828.609017	23.604851
113.990786	3847.670219	23.609869
114.133966	3844.752415	23.614887
113.798321	3854.076678	23.619904
114.539726	3843.011636	23.624922
114.471428	3832.227632	23.629939
114.612504	3844.917570	23.634957
114.953498	3857.516021	23.639975
114.991860	3866.624970	23.644992
115.256255	3861.548570	23.650010
115.425515	3875.796638	23.655027
115.616714	3870.814692	23.660045
115.763842	3861.599395	23.665063
115.833130	3859.832589	23.670080
115.746981	3855.398373	23.675098
115.915540	3857.017453	23.680115
115.785525	3863.960414	23.685133
116.134900	3856.223114	23.690151
115.731838	3858.150203	23.695168
115.834488	3852.643541	23.700186
115.919050	3861.486511	23.705203
115.551028	3866.046683	23.710221
116.152640	3869.699175	23.715239
115.782662	3889.323341	23.720256
115.951258	3884.518002	23.725274
116.207553	3909.866792	23.730291
116.215137	3921.985595	23.735309
116.649946	3922.043317	23.740327
116.679324	3940.943619	23.745344
116.736991	3949.461145	23.750362
116.599299	3956.253435	23.755379
116.822134	3978.168874	23.760397
117.157017	3974.560442	23.765415
117.093611	3990.115947	23.770432
117.337487	3999.256971	23.775450
117.371710	3998.080305	23.780467
117.735334	3999.326389	23.785485
118.275880	4016.227807	23.790503
118.536711	4041.395324	23.795520
118.608731	4033.581177	23.800538
118.888684	4040.604139	23.805555
118.753155	4037.110485	23.810573
118.920918	4028.795326	23.815591
118.705591	4033.166763	23.820608
119.072437	4032.402204	23.825626
118.995546	4028.905108	23.830643
118.957055	4037.914708	23.835661
119.556724	4042.618493	23.840679
119.682879	4052.129946	23.845696
120.267708	4045.570124	23.850714
120.044033	4048.258082	23.855731
120.305000	4045.840422	23.860749
120.673011	4042.997439	23.865767
120.373680	4043.769759	23.870784
120.440069	4031.750475	23.875802
120.866790	4038.666753	23.880819
120.688425	4030.019296	23.885837
120.633070	4035.604078	23.890855
120.675643	4032.921885	23.895872
120.774418	4020.232967	23.900890
121.050205	4036.122754	23.905907
120.920380	4034.809938	23.910925
120.973114	4030.106103	23.915943
121.041648	4043.496144	23.920960
120.994611	4057.175123	23.925978
121.233804	4059.729464	23.930995
121.185307	4067.977257	23.936013
121.614375	4079.301633	23.941031
121.865910	4080.987667	23.946048
121.761842	4086.821540	23.951066
121.746652	4088.231383	23.956083
121.556900	4105.751964	23.961101
122.195615	4108.625801	23.966119
121.960526	4118.415466	23.971136
122.063007	4126.861459	23.976154
122.414002	4141.209115	23.981171
122.493690	4141.202213	23.986189
122.935082	4158.376992	23.991207
123.066211	4179.781895	23.996224
123.337928	4180.506970	24.001242
123.344058	4176.042365	24.006259
123.000028	4180.210396	24.011277
123.341155	4176.713102	24.016295
123.872550	4206.552342	24.021312
123.772593	4205.200292	24.026330
124.178935	4206.705081	24.031347
124.222453	4208.323714	24.036365
124.400274	4193.374346	24.041383
124.589214	4191.830962	24.046400
124.539368	4187.474095	24.051418
124.779305	4191.137547	24.056435
124.483510	4186.859746	24.061453
124.661011	4183.541632	24.066471
124.795298	4206.531706	24.071488
125.108825	4209.512759	24.076506
125.370208	4216.984621	24.081523
125.230800	4218.404880	24.086541
125.501097	4213.964880	24.091559
125.287996	4222.592520	24.096576
125.420459	4214.275253	24.101594
125.961628	4235.683364	24.106611
125.957561	4245.395735	24.111629
126.110264	4234.433369	24.116647
126.230541	4243.625003	24.121664
126.006514	4235.370509	24.126682
126.132510	4240.035335	24.131699
126.113278	4269.540544	24.136717
126.882355	4265.033395	24.141735
126.465185	4261.867635	24.146752
127.262993	4265.418319	24.151770
127.283462	4254.195195	24.156787
127.462075	4254.291557	24.161805
127.631645	4260.765163	24.166823
127.560597	4260.828198	24.171840
127.583909	4283.190668	24.176858
127.832752	4283.239133	24.181875
127.945350	4280.502735	24.186893
127.833551	4286.262365	24.191911
127.944193	4282.667897	24.196928
127.894993	4288.794347	24.201946
128.079517	4304.773993	24.206963
127.950756	4321.266416	24.211981
127.897114	4319.794044	24.216999
127.697371	4332.698517	24.222016
128.515336	4330.238657	24.227034
129.013965	4347.652203	24.232051
129.292320	4361.581358	24.237069
129.138309	4368.563968	24.242087
129.327028	4371.821344	24.247104
129.558965	4369.147002	24.252122
129.666119	4364.470250	24.257139
129.811218	4381.275550	24.262157
130.127923	4389.326582	24.267175
130.316503	4388.655815	24.272192
130.418794	4396.125062	24.277210
130.575546	4398.141893	24.282227
130.575476	4389.059427	24.287245
130.649179	4384.752064	24.292263
130.825214	4387.168113	24.297280
130.566131	4387.754597	24.302298
131.088869	4398.901018	24.307315
130.734922	4408.199116	24.312333
131.072780	4428.467471	24.317351
131.166309	4416.413063	24.322368
130.963450	4422.886410	24.327386
131.399147	4439.809650	24.332403
131.609676	4453.653293	24.337421
131.299596	4450.620116	24.342439
131.268479	4475.204856	24.347456
131.761382	4485.701860	24.352474
132.096124	4482.671778	24.357491
132.122265	4488.012433	24.362509
132.760122	4500.211623	24.367527
132.911480	4497.347467	24.372544
132.764103	4497.776000	24.377562
132.830459	4498.232806	24.382579
132.849219	4493.102912	24.387597
133.027555	4499.678327	24.392615
133.524954	4512.288331	24.397632
133.507794	4525.279177	24.402650
133.448845	4526.749095	24.407667
133.528010	4527.225037	24.412685
133.736833	4524.868735	24.417703
134.219747	4528.538749	24.422720
133.607219	4538.872182	24.427738
134.191013	4543.190114	24.432755
134.377489	4553.037968	24.437773
134.374811	4552.365900	24.442791
134.226268	4555.195814	24.447808
134.341185	4553.092160	24.452826
134.946969	4575.685081	24.457843
134.870817	4591.755590	24.462861
135.165985	4586.595485	24.467879
135.411134	4577.926568	24.472896
135.032862	4593.494434	24.477914
135.462914	4598.606563	24.482931
135.130902	4611.595460	24.487949
135.420518	4612.301045	24.492967
135.867807	4622.824622	24.497984
135.753765	4639.618134	24.503002
136.061756	4632.228730	24.508019
136.006291	4639.565225	24.513037
136.388410	4652.340194	24.518055
136.371048	4659.903479	24.523072
136.522571	4661.890499	24.528090
136.843447	4670.011861	24.533107
136.615960	4688.313511	24.538125
137.065095	4692.223865	24.543143
137.065229	4701.621591	24.548160
137.152273	4707.995690	24.553178
137.482602	4718.674225	24.558195
137.807949	4719.386479	24.563213
137.926873	4717.266386	24.568231
137.956523	4717.928546	24.573248
138.116057	4732.301473	24.578266
138.374509	4745.201811	24.583283
138.499596	4748.711616	24.588301
139.025537	4738.483871	24.593319
139.524968	4739.126245	24.598336
139.101947	4747.005844	24.603354
139.313294	4734.785131	24.608371
139.241311	4739.758644	24.613389
139.321448	4737.491424	24.618407
139.463293	4740.133721	24.623424
139.534803	4751.894056	24.628442
139.967787	4750.988138	24.633459
139.784719	4764.083142	24.638477
140.283741	4752.611606	24.643495
140.609029	4747.051097	24.648512
140.647818	4758.390026	24.653530
140.725227	4747.519357	24.658547
140.881883	4750.333242	24.663565
140.638768	4744.536419	24.668583
140.887314	4754.298482	24.673600
140.752244	4786.388150	24.678618
141.090897	4788.604767	24.683635
141.163373	4779.795112	24.688653
141.403282	4780.990154	24.693671
141.356903	4780.289112	24.698688
141.296077	4811.349774	24.703706
141.557890	4820.439473	24.708723
141.714673	4819.558973	24.713741
141.586069	4822.423423	24.718759
141.994252	4841.270133	24.723776
142.305320	4845.158579	24.728794
142.573523	4840.429723	24.733811
142.327236	4844.849449	24.738829
142.162778	4861.590934	24.743847
142.571708	4866.249096	24.748864
142.307657	4878.794555	24.753882
142.812358	4886.435794	24.758899
143.111407	4895.798929	24.763917
143.106048	4906.195516	24.768935
143.591964	4912.684554	24.773952
143.473369	4922.036774	24.778970
143.771764	4924.749958	24.783987
144.129707	4918.768924	24.789005
143.969089	4932.875490	24.794023
144.199305	4945.896456	24.799040
144.117631	4956.951550	24.804058
144.062505	4964.725232	24.809075
144.624987	4962.854297	24.814093
144.757116	4978.313314	24.819111
144.873869	4982.675115	24.824128
145.045306	4981.889828	24.829146
145.256290	4987.428327	24.834163
145.112844	5006.724450	24.839181
145.207831	5016.676005	24.844199
145.528039	4999.401370	24.849216
145.476669	5036.197453	24.854234
145.988142	5041.555305	24.859251
146.131559	5039.275951	24.864269
145.905947	5058.222727	24.869287
146.564147	5062.292962	24.874304
146.500143	5070.141414	24.879322
146.753996	5067.737385	24.884339
147.167179	5072.020025	24.889357
147.246042	5086.340527	24.894375
147.645805	5091.531883	24.899392
147.448806	5095.785189	24.904410
147.582219	5092.104059	24.909427
147.738994	5086.149302	24.914445
147.901515	5085.181991	24.919463
147.991779	5096.240902	24.924480
148.281058	5110.868262	24.929498
148.278934	5124.324915	24.934515
148.189239	5113.451834	24.939533
148.234013	5134.197450	24.944551
148.284496	5131.961878	24.949568
148.222770	5144.318777	24.954586
148.920121	5158.512944	24.959603
149.275061	5174.616372	24.964621
149.148883	5177.299343	24.969639
149.726922	5177.680594	24.974656
149.446914	5177.759453	24.979674
149.955225	5183.785734	24.984691
149.753584	5184.877766	24.989709
149.769050	5199.390046	24.994727
150.050976	5195.225063	24.999744
150.166059	5223.460666	25.004762
150.253322	5234.609956	25.009779
150.366493	5225.932688	25.014797
150.761196	5245.809110	25.019815
151.131515	5246.896675	25.024832
151.007864	5257.850271	25.029850
151.209631	5257.619891	25.034867
151.279764	5259.371641	25.039885
151.481863	5284.436324	25.044903
151.793614	5285.406825	25.049920
151.442103	5289.673256	25.054938
151.658349	5291.392855	25.059955
151.838915	5311.501836	25.064973
151.981473	5317.855932	25.069991
152.095122	5322.151399	25.075008
152.369849	5342.276275	25.080026
152.145584	5348.340869	25.085043
152.778279	5344.594042	25.090061
152.699096	5365.244787	25.095079
153.118457	5366.561270	25.100096
153.284210	5376.630456	25.105114
153.312300	5374.883716	25.110131
154.088402	5378.716287	25.115149
154.205415	5403.077030	25.120167
154.193573	5386.987318	25.125184
154.555702	5402.725138	25.130202
154.701395	5388.090675	25.135219
154.796910	5388.969528	25.140237
154.595331	5395.691932	25.145255
155.012568	5394.499560	25.150272
154.744413	5393.167479	25.155290
155.118322	5390.104729	25.160307
155.055060	5400.008791	25.165325
155.020050	5413.288437	25.170343
155.162048	5426.867101	25.175360
155.585945	5435.015060	25.180378
155.595369	5443.077531	25.185395
155.927038	5441.908825	25.190413
155.775507	5447.644765	25.195431
156.148393	5456.008344	25.200448
156.016850	5471.907812	25.205466
156.071819	5481.669416	25.210483
156.632610	5495.480979	25.215501
156.533988	5514.052789	25.220519
156.726951	5505.513324	25.225536
156.829102	5529.463253	25.230554
156.979690	5542.450690	25.235571
157.334023	5557.908007	25.240589
157.480125	5565.588692	25.245607
157.956885	5571.364402	25.250624
158.161502	5571.288700	25.255642
158.373870	5592.272485	25.260659
158.888804	5576.840889	25.265677
159.163453	5585.317734	25.270695
159.127076	5570.092741	25.275712
159.054639	5585.933672	25.280730
159.045008	5591.653960	25.285747
159.781009	5579.846319	25.290765
159.481916	5583.017252	25.295783
159.389011	5571.902600	25.300800
159.545269	5589.042848	25.305818
159.641003	5601.059695	25.310835
159.951095	5604.887063	25.315853
159.785850	5610.693073	25.320871
160.193055	5624.084497	25.325888
160.291599	5637.259443	25.330906
160.213896	5649.931278	25.335923
160.644353	5653.893024	25.340941
160.207315	5679.425254	25.345959
160.597137	5674.883078	25.350976
160.883295	5691.725409	25.355994
161.098766	5706.422296	25.361011
161.457423	5699.416197	25.366029
161.175472	5727.571398	25.371047
161.488302	5729.801895	25.376064
161.772143	5749.839144	25.381082
162.137173	5766.940957	25.386099
162.514391	5759.207162	25.391117
162.442231	5771.123659	25.396135
162.457274	5775.451387	25.401152
162.613562	5796.691281	25.406170
162.608177	5804.579188	25.411187
162.793870	5803.880492	25.416205
163.070911	5815.113646	25.421223
163.237205	5814.185832	25.426240
163.598577	5809.443571	25.431258
163.316246	5814.917844	25.436275
163.723140	5842.171190	25.441293
163.806751	5854.724235	25.446311
163.731306	5849.957672	25.451328
164.250015	5866.098391	25.456346
164.239285	5871.891422	25.461363
164.848032	5870.736503	25.466381
165.437582	5885.931381	25.471399
165.456220	5889.908062	25.476416
165.508374	5891.200549	25.481434
165.716007	5887.841632	25.486451
166.202446	5890.137029	25.491469
166.092634	5898.580266	25.496487
165.751875	5904.984194	25.501504
166.106333	5886.199373	25.506522
166.029008	5904.664927	25.511539
166.774068	5914.215256	25.516557
166.447258	5924.006706	25.521575
166.577550	5919.663531	25.526592
166.621821	5923.025571	25.531610
166.802055	5938.568111	25.536627
166.922308	5949.116998	25.541645
166.912228	5969.850775	25.546663
167.692012	5967.245806	25.551680
168.320102	5955.596800	25.556698
168.122051	5956.629216	25.561715
168.495683	5970.275398	25.566733
168.699715	5985.119365	25.571751
168.749797	5994.011797	25.576768
169.005284	5993.960720	25.581786
168.733737	5988.814783	25.586803
169.028400	5987.378102	25.591821
169.025172	5991.360017	25.596839
169.382749	6017.232528	25.601856
169.540245	6013.399901	25.606874
169.551765	6017.014711	25.611891
169.659640	6025.298977	25.616909
169.746370	6050.969240	25.621927
169.767443	6056.991762	25.626944
169.688413	6065.934042	25.631962
169.863655	6081.401155	25.636979
170.036952	6089.621814	25.641997
170.094608	6124.942879	25.647015
170.378469	6133.506703	25.652032
170.779423	6145.579575	25.657050
170.639323	6161.050333	25.662067
171.451984	6180.009441	25.667085
171.455525	6187.113169	25.672103
171.220271	6203.099913	25.677120
172.078588	6209.905670	25.682138
172.091365	6219.579441	25.687156
172.072183	6229.258527	25.692173
172.699948	6255.075506	25.697191
172.572892	6262.246650	25.702208
172.872349	6249.417053	25.707226
172.911716	6259.892949	25.712244
173.421925	6262.837389	25.717261
173.773840	6267.996921	25.722279
173.684602	6267.240711	25.727296
174.175011	6266.422841	25.732314
174.160935	6269.640276	25.737332
174.426233	6278.309654	25.742349
174.475450	6292.655868	25.747367
174.788182	6296.348286	25.752384
174.929194	6299.980236	25.757402
174.964172	6296.720808	25.762420
174.704440	6290.222041	25.767437
174.977796	6297.514120	25.772455
175.060813	6312.251696	25.777472
175.090142	6313.410178	25.782490
174.979425	6324.810518	25.787508
175.687907	6342.699431	25.792525
176.247793	6342.059829	25.797543
176.748113	6345.030344	25.802560
177.024397	6333.556089	25.807578
176.800150	6340.500042	25.812596
177.029366	6334.403611	25.817613
176.834039	6333.840666	25.822631
177.002625	6344.433769	25.827648
177.271755	6358.133094	25.832666
177.115113	6372.857778	25.837684
177.216176	6370.767214	25.842701
177.631394	6386.418437	25.847719
177.550471	6390.259775	25.852736
178.015920	6395.424902	25.857754
178.209688	6418.831672	25.862772
178.395424	6420.960519	25.867789
178.229077	6421.082715	25.872807
178.375847	6443.389930	25.877824
178.563138	6447.623060	25.882842
178.995791	6474.769255	25.887860
179.261415	6474.356548	25.892877
179.767413	6471.924591	25.897895
179.954157	6479.537534	25.902912
179.803157	6484.434935	25.907930
180.382276	6508.509515	25.912948
180.218559	6504.962495	25.917965
180.555925	6505.431039	25.922983
180.532486	6515.825388	25.928000
180.925601	6524.206657	25.933018
181.038697	6530.006921	25.938036
181.011967	6530.098042	25.943053
180.978609	6549.788110	25.948071
181.303481	6576.834244	25.953088
181.474940	6572.569903	25.958106
181.636890	6596.409908	25.963124
181.883397	6600.440271	25.968141
182.135116	6616.960871	25.973159
181.829920	6633.777235	25.978176
182.744286	6631.238806	25.983194
183.017693	6652.171327	25.988212
183.049353	6652.986825	25.993229
183.424898	6658.690756	25.998247
183.274521	6662.957998	26.003264
183.573394	6671.428255	26.008282
183.446991	6683.651390	26.013300
183.958265	6693.632501	26.018317
184.283701	6697.852984	26.023335
184.173744	6707.456080	26.028352
184.521093	6710.013369	26.033370
184.451262	6713.608774	26.038388
184.391183	6720.585475	26.043405
184.717844	6733.784080	26.048423
184.930185	6744.352065	26.053440
185.013599	6762.638320	26.058458
185.259548	6775.166698	26.063476
185.224670	6785.372515	26.068493
185.895449	6798.656559	26.073511
185.815664	6813.510657	26.078528
186.265932	6821.006726	26.083546
186.291606	6833.441001	26.088564
186.126545	6839.246640	26.093581
186.483169	6853.880184	26.098599
186.337942	6869.772300	26.103616
186.848098	6876.682674	26.108634
186.970127	6891.572625	26.113652
187.598838	6893.427082	26.118669
188.025527	6876.447771	26.123687
187.842413	6914.702848	26.128704
188.342551	6918.321741	26.133722
188.473455	6915.944169	26.138740
188.651939	6916.337521	26.143757
188.999649	6923.458430	26.148775
189.109283	6933.875838	26.153792
189.700861	6934.663690	26.158810
189.670676	6929.474975	26.163828
189.774093	6932.111428	26.168845
190.134424	6926.486055	26.173863
189.960550	6938.631420	26.178880
190.104300	6930.807467	26.183898
190.341906	6953.121574	26.188916
190.049341	6968.935875	26.193933
190.555848	6965.783060	26.198951
190.495094	6986.203649	26.203968
190.854273	6995.705339	26.208986
190.763467	7005.911927	26.214004
190.660379	7017.204375	26.219021
191.095658	7030.228437	26.224039
190.975740	7050.457299	26.229056
191.688560	7056.147081	26.234074
191.909609	7083.481498	26.239092
191.927722	7083.161890	26.244109
192.578334	7104.744377	26.249127
192.485798	7125.853328	26.254144
192.936068	7116.488887	26.259162
192.893008	7136.541255	26.264180
193.020428	7155.375952	26.269197
193.525359	7153.988513	26.274215
193.676220	7170.437444	26.279232
194.025126	7183.728824	26.284250
193.979193	7174.045877	26.289268
194.029321	7187.659436	26.294285
194.252570	7206.249848	26.299303
194.403998	7211.329582	26.304320
194.682821	7233.963329	26.309338
195.176257	7231.522322	26.314356
195.620103	7225.849886	26.319373
196.395942	7221.147043	26.324391
196.539972	7207.172818	26.329408
196.805320	7200.530504	26.334426
196.880426	7199.555539	26.339444
196.677894	7209.238120	26.344461
196.766379	7210.929540	26.349479
197.248844	7226.394774	26.354496
197.316202	7234.611578	26.359514
197.445361	7230.428132	26.364532
197.427994	7251.053735	26.369549
197.456193	7237.683178	26.374567
197.200518	7251.425582	26.379584
197.492017	7259.319233	26.384602
197.648474	7268.252994	26.389620
197.710391	7297.138357	26.394637
198.148893	7304.352265	26.399655
198.154456	7336.748255	26.404672
198.049485	7335.596046	26.409690
198.636413	7355.902404	26.414708
198.550933	7368.865192	26.419725
198.905415	7386.784969	26.424743
198.970399	7406.882740	26.429760
199.274085	7421.484647	26.434778
199.373167	7424.325910	26.439796
199.439774	7451.523574	26.444813
200.245167	7465.785378	26.449831
200.412205	7463.787683	26.454848
200.519198	7488.732245	26.459866
200.760085	7495.268590	26.464884
200.714733	7501.906059	26.469901
200.822286	7515.489878	26.474919
201.150968	7531.409460	26.479936
201.273204	7546.322834	26.484954
201.420143	7551.204139	26.489972
201.562049	7578.684890	26.494989
202.056164	7585.123271	26.500007
201.994728	7600.837568	26.505024
202.280988	7625.923487	26.510042
202.565897	7636.806900	26.515060
202.372968	7651.681367	26.520077
202.687842	7658.898649	26.525095
203.447583	7682.779594	26.530112
203.492044	7677.586110	26.535130
203.958592	7699.039304	26.540148
203.977854	7701.759184	26.545165
204.182521	7716.667686	26.550183
204.470603	7737.404643	26.555200
204.579355	7742.166322	26.560218
205.145384	7751.165422	26.565236
205.083697	7766.622348	26.570253
205.510157	7777.775361	26.575271
205.418387	7782.738936	26.580288
205.467225	7805.321913	26.585306
205.873589	7813.791465	26.590324
205.665756	7840.727405	26.595341
206.054880	7850.150590	26.600359
205.915965	7865.375471	26.605376
206.235977	7874.059478	26.610394
207.071817	7898.951324	26.615412
206.956959	7912.770149	26.620429
207.739014	7917.208905	26.625447
207.869768	7923.683381	26.630464
207.939465	7928.364958	26.635482
208.369881	7938.314608	26.640500
208.318800	7955.858938	26.645517
208.237186	7953.716599	26.650535
209.074106	7974.758101	26.655552
209.133378	7986.950597	26.660570
209.529017	7987.470164	26.665588
209.757841	7988.408149	26.670605
209.942455	7989.425160	26.675623
209.999208	8007.347845	26.680640
210.081848	8016.313196	26.685658
210.402252	8014.538078	26.690676
210.468726	8025.377706	26.695693
210.835796	8043.701014	26.700711
210.933871	8042.980550	26.705728
211.052654	8049.436585	26.710746
210.867493	8062.084873	26.715764
211.188056	8081.417915	26.720781
211.594572	8095.094343	26.725799
211.978493	8103.819847	26.730816
211.646171	8102.075976	26.735834
212.436778	8114.937129	26.740852
212.435244	8129.096507	26.745869
212.779263	8128.507684	26.750887
212.916690	8154.189467	26.755904
213.009784	8157.832959	26.760922
213.303392	8170.222186	26.765940
213.583875	8190.709717	26.770957
213.413750	8180.890037	26.775975
213.381091	8200.788412	26.780992
213.785728	8227.835923	26.786010
214.310944	8232.131545	26.791028
214.215387	8242.189259	26.796045
214.504599	8248.816350	26.801063
214.746010	8269.882357	26.806080
215.159170	8286.570076	26.811098
215.109584	8286.235698	26.816116
214.907872	8311.847260	26.821133
215.230411	8317.684275	26.826151
215.606137	8348.078301	26.831168
215.379129	8371.870589	26.836186
215.882719	8393.009779	26.841204
216.192713	8411.804601	26.846221
216.940457	8409.353466	26.851239
217.580888	8429.628680	26.856256
217.904932	8433.194476	26.861274
218.194450	8427.579560	26.866292
218.657084	8430.812754	26.871309
218.609195	8429.817189	26.876327
218.713066	8429.244625	26.881344
218.837193	8431.754213	26.886362
219.201929	8451.093757	26.891380
219.314145	8458.269456	26.896397
219.400276	8460.679020	26.901415
219.458786	8456.508567	26.906432
219.748773	8482.367977	26.911450
219.696385	8486.595791	26.916468
219.782343	8500.738599	26.921485
219.928100	8519.545081	26.926503
220.189276	8527.245896	26.931520
220.308198	8559.309656	26.936538
220.485679	8556.814608	26.941556
220.846279	8588.798097	26.946573
221.143205	8592.359771	26.951591
221.533456	8600.130553	26.956608
221.800338	8606.199850	26.961626
222.179041	8624.460452	26.966644
222.249413	8640.554041	26.971661
222.581732	8645.933454	26.976679
222.872395	8644.969064	26.981696
223.169662	8664.268874	26.986714
223.193922	8668.978699	26.991732
223.360557	8674.955971	26.996749
223.564644	8690.780832	27.001767
223.798449	8695.354232	27.006784
223.754548	8714.759627	27.011802
224.337637	8721.271919	27.016820
224.529992	8742.767355	27.021837
224.896106	8748.566567	27.026855
224.843044	8753.494865	27.031872
225.043417	8768.896616	27.036890
225.558395	8785.254421	27.041908
225.807233	8789.676467	27.046925
226.369537	8815.902374	27.051943
226.259230	8818.028744	27.056960
226.236593	8824.971785	27.061978
226.493163	8837.436219	27.066996
226.645165	8859.853089	27.072013
226.765747	8856.910557	27.077031
226.933974	8884.378944	27.082048
227.068881	8889.683318	27.087066
227.528674	8911.279491	27.092084
227.399301	8922.218439	27.097101
227.575267	8947.520127	27.102119
228.167855	8952.086768	27.107136
228.349712	8972.288407	27.112154
228.530996	8986.030595	27.117172
228.785056	8993.700521	27.122189
228.902813	9007.785715	27.127207
229.332644	9015.520978	27.132224
228.874122	9047.207429	27.137242
229.053267	9052.721140	27.142260
229.672141	9075.779175	27.147277
229.688504	9096.918327	27.152295
230.180773	9110.425405	27.157312
230.023484	9127.014209	27.162330
231.059546	9132.957486	27.167348
231.501555	9127.984224	27.172365
231.841436	9149.338319	27.177383
232.724373	9143.222803	27.182400
232.696142	9152.586126	27.187418
232.686785	9144.504512	27.192436
232.839585	9144.054562	27.197453
232.759191	9154.066214	27.202471
233.448895	9171.476194	27.207488
233.293197	9168.444013	27.212506
233.747610	9174.001836	27.217524
233.896036	9186.553047	27.222541
233.864632	9208.689712	27.227559
234.474927	9202.075916	27.232576
234.514045	9209.451586	27.237594
234.480473	9236.784737	27.242612
234.617217	9246.643781	27.247629
234.707259	9269.269248	27.252647
234.991401	9279.491404	27.257664
235.081281	9299.814299	27.262682
235.616086	9301.794949	27.267700
236.075582	9329.613531	27.272717
235.605811	9344.541078	27.277735
235.962490	9348.423859	27.282752
236.373941	9377.024096	27.287770
236.227932	9395.951773	27.292788
236.543860	9422.385831	27.297805
237.035939	9437.487674	27.302823
237.435892	9435.397471	27.307840
237.547998	9474.624280	27.312858
237.877495	9480.822158	27.317876
238.304390	9500.370073	27.322893
238.326525	9510.535072	27.327911
238.486074	9520.261300	27.332928
238.569119	9549.988576	27.337946
239.599196	9541.500882	27.342964
240.600037	9548.640508	27.347981
240.957970	9556.693640	27.352999
241.391965	9539.685092	27.358016
241.306419	9543.156910	27.363034
241.653293	9533.234744	27.368052
241.496790	9533.638920	27.373069
241.232820	9538.496937	27.378087
241.439546	9556.095509	27.383104
241.670417	9564.833855	27.388122
241.820667	9566.985570	27.393140
242.035692	9582.845737	27.398157
242.311363	9588.714641	27.403175
242.567319	9596.413691	27.408192
242.474683	9618.910871	27.413210
242.763231	9625.983747	27.418228
242.740513	9642.287604	27.423245
242.818961	9673.246392	27.428263
243.149978	9680.344535	27.433280
243.055709	9714.239030	27.438298
243.256901	9730.346642	27.443316
243.590640	9752.123242	27.448333
243.936477	9783.931960	27.453351
244.452079	9790.513417	27.458368
244.666053	9829.322395	27.463386
244.523512	9837.566747	27.468404
245.222778	9844.390289	27.473421
245.228250	9864.507340	27.478439
245.524736	9880.274699	27.483456
245.533680	9908.196716	27.488474
246.066264	9924.110812	27.493492
246.505822	9949.044138	27.498509
246.242766	9965.888507	27.503527
246.957813	9980.682028	27.508544
247.182681	10013.505504	27.513562
247.580109	10026.432751	27.518580
247.617013	10040.035181	27.523597
247.572013	10058.549014	27.528615
248.131773	10078.230759	27.533632
248.324413	10084.680862	27.538650
248.519832	10115.599796	27.543668
248.770115	10127.766128	27.548685
249.280613	10148.796994	27.553703
249.547660	10167.434001	27.558720
249.536742	10177.648243	27.563738
249.912538	10194.678988	27.568756
250.771257	10200.547363	27.573773
250.693180	10228.068428	27.578791
251.081347	10238.787569	27.583808
251.510795	10239.860953	27.588826
251.337565	10263.365068	27.593844
252.005876	10265.190523	27.598861
251.933399	10299.841296	27.603879
252.380242	10297.508427	27.608896
252.373241	10311.667489	27.613914
252.246227	10331.432923	27.618932
252.815972	10350.350735	27.623949
252.763877	10372.921014	27.628967
252.945804	10390.193736	27.633984
253.424137	10411.857397	27.639002
253.824045	10436.347435	27.644020
254.173465	10445.552653	27.649037
254.644662	10461.463302	27.654055
254.970683	10470.748841	27.659072
255.134065	10494.453411	27.664090
255.896674	10499.067102	27.669108
256.399342	10517.655128	27.674125
255.981616	10524.707085	27.679143
256.030345	10534.420040	27.684160
256.760170	10552.063575	27.689178
256.991223	10567.890539	27.694196
257.046519	10566.059929	27.699213
256.794699	10589.120634	27.704231
257.403751	10599.818289	27.709248
257.473101	10623.541034	27.714266
257.645478	10632.664690	27.719284
257.787037	10650.874829	27.724301
257.953685	10681.745271	27.729319
258.179270	10691.837036	27.734336
258.408599	10711.234900	27.739354
258.956090	10734.265433	27.744372
259.365461	10748.582601	27.749389
259.430065	10771.212045	27.754407
259.616405	10783.402890	27.759424
259.943627	10811.283047	27.764442
260.452192	10819.999577	27.769460
261.060117	10843.259731	27.774477
261.167373	10851.303166	27.779495
261.889112	10833.746750	27.784512
262.394946	10852.347244	27.789530
262.513718	10860.472282	27.794548
262.654194	10868.538570	27.799565
262.933744	10875.277085	27.804583
262.955356	10872.854850	27.809600
263.035807	10874.982887	27.814618
262.962509	10889.838109	27.819636
263.275370	10894.867776	27.824653
263.328851	10911.406853	27.829671
263.705301	10928.451662	27.834688
264.098755	10941.724598	27.839706
263.882344	10962.112298	27.844724
264.387827	10971.055536	27.849741
264.372188	11001.171388	27.854759
264.587468	11020.198517	27.859776
264.605565	11039.356122	27.864794
264.800705	11074.556561	27.869812
265.495454	11084.851891	27.874829
265.714105	11113.751974	27.879847
265.684113	11134.381517	27.884864
266.201595	11147.780559	27.889882
266.405748	11178.889170	27.894900
266.929007	11207.124282	27.899917
266.863514	11233.418269	27.904935
267.225049	11248.532480	27.909952
267.576544	11267.387576	27.914970
267.983902	11297.536127	27.919988
268.508531	11317.010143	27.925005
268.689123	11333.463929	27.930023
268.775670	11354.088573	27.935040
269.604285	11363.013013	27.940058
269.539264	11397.195331	27.945076
269.776229	11402.499340	27.950093
270.089765	11439.992518	27.955111
270.337321	11440.725120	27.960128
270.731880	11456.174401	27.965146
270.911207	11486.022403	27.970164
271.313604	11491.828409	27.975181
271.706382	11509.023968	27.980199
272.148668	11522.601269	27.985216
272.724426	11520.086875	27.990234
273.033476	11546.856478	27.995252
273.424066	11547.292718	28.000269
273.320769	11554.686031	28.005287
273.451634	11559.798144	28.010304
273.632363	11578.286459	28.015322
273.826348	11603.779999	28.020340
273.759715	11623.828495	28.025357
274.150798	11641.051265	28.030375
274.430953	11657.739387	28.035392
274.568947	11675.957579	28.040410
275.008922	11694.962355	28.045428
275.240763	11714.097854	28.050445
275.268428	11738.524078	28.055463
275.498672	11749.880291	28.060480
276.025175	11778.345927	28.065498
275.997873	11798.085555	28.070516
276.524613	11825.556919	28.075533
276.621276	11850.622646	28.080551
276.766160	11880.396732	28.085568
277.229346	11904.084291	28.090586
277.493565	11930.902948	28.095604
277.966356	11943.545820	28.100621
278.229617	11966.718309	28.105639
278.116135	11995.913091	28.110656
279.182193	11993.210018	28.115674
279.720754	12012.030179	28.120692
280.234119	12015.161140	28.125709
280.570596	12033.228575	28.130727
280.532799	12034.763422	28.135744
281.118190	12028.534763	28.140762
281.357008	12044.443827	28.145780
281.448212	12058.343067	28.150797
281.805756	12066.167461	28.155815
281.993084	12072.121291	28.160832
282.132446	12074.570618	28.165850
282.055606	12104.344133	28.170868
282.396242	12103.684047	28.175885
282.786718	12121.539330	28.180903
282.796911	12131.003576	28.185920
283.216332	12139.429141	28.190938
283.347340	12163.462217	28.195956
283.511741	12181.525312	28.200973
283.737319	12198.057599	28.205991
284.194739	12231.149508	28.211008
283.999538	12239.445589	28.216026
284.444759	12262.652881	28.221044
284.531420	12287.899014	28.226061
284.663425	12315.843353	28.231079
284.979614	12352.231971	28.236096
285.370878	12371.135327	28.241114
285.851954	12409.828918	28.246132
286.273308	12417.250498	28.251149
286.453675	12445.552620	28.256167
286.961446	12474.405524	28.261184
287.542177	12490.891715	28.266202
287.518054	12508.680780	28.271220
287.661287	12521.848458	28.276237
288.120842	12543.117052	28.281255
288.543212	12567.176385	28.286272
289.089909	12591.568092	28.291290
289.463568	12604.008907	28.296308
289.983639	12616.471108	28.301325
290.156299	12642.431552	28.306343
290.313122	12647.125245	28.311360
290.631850	12653.545977	28.316378
290.806355	12667.788044	28.321396
291.039310	12680.171924	28.326413
291.867610	12696.759024	28.331431
292.008998	12709.539498	28.336448
292.278042	12719.841995	28.341466
292.443722	12729.606964	28.346484
292.845422	12737.187969	28.351501
293.130382	12755.572063	28.356519
293.447093	12765.694900	28.361536
293.931506	12769.407592	28.366554
294.151831	12793.283357	28.371572
294.634016	12793.680783	28.376589
294.822204	12798.035223	28.381607
294.748754	12812.781919	28.386624
295.190372	12829.063064	28.391642
295.266704	12847.975173	28.396660
295.351072	12860.131734	28.401677
295.864082	12873.438404	28.406695
295.270989	12901.231582	28.411712
295.952650	12931.236751	28.416730
296.139043	12953.933320	28.421748
296.666409	12973.545984	28.426765
297.152542	12985.185188	28.431783
297.815495	13001.789041	28.436800
297.960088	13015.141273	28.441818
298.272087	13040.069054	28.446836
298.465399	13058.980885	28.451853
298.918142	13070.214387	28.456871
298.788069	13096.159661	28.461888
299.293734	13108.816896	28.466906
299.274147	13137.903574	28.471924
299.435461	13158.119385	28.476941
299.918164	13181.982075	28.481959
300.039473	13194.276157	28.486976
300.521919	13206.417274	28.491994
300.556718	13237.576880	28.497012
300.811452	13257.468415	28.502029
301.135756	13276.831514	28.507047
301.261415	13309.632458	28.512064
301.694256	13327.762547	28.517082
301.958600	13355.730814	28.522100
302.197659	13369.092858	28.527117
302.796220	13394.988477	28.532135
302.888110	13416.793653	28.537152
303.312787	13432.955296	28.542170
303.541012	13468.472197	28.547188
304.115419	13491.443883	28.552205
304.770675	13512.421207	28.557223
304.700014	13542.382284	28.562240
305.304089	13546.549640	28.567258
305.256902	13572.503963	28.572276
305.346950	13589.132676	28.577293
305.962730	13609.360226	28.582311
306.323998	13642.228286	28.587328
306.751315	13657.592279	28.592346
307.198697	13683.042260	28.597364
307.162648	13682.558165	28.602381
307.645258	13712.016314	28.607399
307.621626	13734.479371	28.612416
308.008084	13750.866739	28.617434
308.731960	13775.013308	28.622452
308.570007	13788.360365	28.627469
308.904676	13811.488952	28.632487
309.261563	13842.399208	28.637504
309.647113	13865.905534	28.642522
309.931892	13887.799070	28.647540
310.657736	13909.934559	28.652557
311.318591	13915.135882	28.657575
311.749561	13943.476200	28.662592
312.195480	13956.180271	28.667610
312.282890	13957.046768	28.672628
312.656889	13979.574913	28.677645
313.150120	13987.866256	28.682663
313.353143	13981.572732	28.687680
313.969435	14002.026053	28.692698
313.953664	14005.883592	28.697716
313.857652	14027.706615	28.702733
314.633628	14042.135222	28.707751
314.602265	14044.430396	28.712768
315.004541	14056.960557	28.717786
315.166211	14089.096741	28.722804
315.284942	14103.401339	28.727821
315.596231	14120.849609	28.732839
315.627492	14154.189589	28.737856
315.840258	14173.945798	28.742874
315.858239	14196.482953	28.747892
316.100869	14219.449319	28.752909
316.566951	14249.762234	28.757927
316.736100	14283.640633	28.762944
316.768107	14312.980873	28.767962
317.770339	14343.603629	28.772980
317.626393	14376.519271	28.777997
317.995823	14399.294615	28.783015
318.257714	14438.037319	28.788032
319.122057	14463.988200	28.793050
319.408864	14485.704108	28.798068
319.644843	14513.337069	28.803085
320.203499	14535.394014	28.808103
320.498990	14563.084942	28.813120
320.847042	14575.540980	28.818138
321.150721	14587.320392	28.823156
321.536486	14613.095694	28.828173
321.995341	14626.646056	28.833191
322.338640	14646.627016	28.838208
322.562702	14664.266875	28.843226
322.523121	14691.126363	28.848244
322.694802	14715.121769	28.853261
322.963969	14730.098543	28.858279
323.089415	14749.542131	28.863296
323.479592	14772.785792	28.868314
324.035281	14801.589156	28.873332
324.300384	14829.422702	28.878349
324.739162	14847.261924	28.883367
324.992470	14883.085065	28.888384
325.493179	14895.725605	28.893402
326.136760	14929.742449	28.898420
325.666028	14954.986008	28.903437
326.336824	14975.827094	28.908455
326.524467	15004.975652	28.913472
327.084879	15032.060701	28.918490
326.998954	15066.328253	28.923508
327.489198	15093.240656	28.928525
327.625596	15119.371823	28.933543
328.250057	15150.489125	28.938560
329.156427	15162.264975	28.943578
329.962757	15180.234212	28.948596
330.177195	15194.298480	28.953613
331.191565	15195.498075	28.958631
331.847805	15190.920837	28.963648
332.703767	15194.928575	28.968666
333.420117	15188.241978	28.973684
332.921649	15178.956446	28.978701
333.367337	15165.955234	28.983719
333.589534	15178.153668	28.988736
333.721801	15171.653942	28.993754
334.316605	15161.334135	28.998772
334.430759	15176.857183	29.003789
334.853103	15164.157734	29.008807
334.953949	15171.786706	29.013824
334.862445	15167.313200	29.018842
334.959811	15186.273379	29.023860
335.175870	15214.790300	29.028877
335.475858	15213.072983	29.033895
335.170010	15243.850108	29.038912
335.356542	15262.901163	29.043930
335.550598	15291.278446	29.048948
335.675154	15330.898754	29.053965
335.753137	15361.372766	29.058983
336.029991	15399.171158	29.064000
336.420664	15440.523818	29.069018
336.558852	15468.417358	29.074036
337.076905	15514.460108	29.079053
337.296106	15560.221641	29.084071
337.649962	15603.156968	29.089088
337.622905	15646.431510	29.094106
338.185271	15676.354371	29.099124
338.468750	15725.166575	29.104141
339.272922	15740.737876	29.109159
340.022438	15785.239277	29.114176
340.246041	15803.613354	29.119194
340.406475	15845.317358	29.124212
341.030355	15873.245962	29.129229
341.779010	15901.529016	29.134247
342.216339	15926.418311	29.139264
341.875810	15953.285718	29.144282
342.497100	15972.074655	29.149300
342.937140	16000.831563	29.154317
343.306622	16015.647839	29.159335
343.510800	16049.749455	29.164352
343.614151	16083.563686	29.169370
343.847165	16110.326616	29.174388
344.122967	16146.872246	29.179405
344.203336	16169.275645	29.184423
344.921342	16206.711010	29.189440
345.381242	16233.129090	29.194458
345.705202	16259.530389	29.199476
346.155257	16282.055371	29.204493
347.102170	16294.096418	29.209511
347.544902	16314.330848	29.214528
347.751362	16342.752015	29.219546
348.053953	16354.343734	29.224564
348.214507	16381.530534	29.229581
348.909402	16395.337906	29.234599
349.098157	16423.164765	29.239616
348.917219	16447.679955	29.244634
349.175404	16476.494698	29.249652
349.458977	16507.978564	29.254669
350.080826	16527.559314	29.259687
350.541361	16549.211263	29.264704
350.778346	16590.701099	29.269722
351.123570	16614.875359	29.274740
351.230794	16637.410488	29.279757
351.503470	16676.162977	29.284775
352.160792	16703.871490	29.289792
352.382580	16746.387229	29.294810
352.870625	16755.705412	29.299828
353.163848	16795.537656	29.304845
353.678405	16822.407870	29.309863
353.920298	16847.857493	29.314880
354.486811	16878.283103	29.319898
355.107745	16905.975933	29.324916
355.523609	16933.789569	29.329933
355.577813	16952.795202	29.334951
355.955673	16976.646162	29.339968
356.435997	17001.824704	29.344986
357.243963	17013.378650	29.350004
357.152893	17050.959788	29.355021
357.299071	17075.070056	29.360039
357.457573	17097.089729	29.365056
357.569981	17135.694948	29.370074
358.346879	17155.424082	29.375092
358.810184	17194.283256	29.380109
358.789907	17217.398364	29.385127
359.340731	17249.297951	29.390144
359.637118	17291.690780	29.395162
360.352310	17314.363862	29.400180
360.413089	17352.749598	29.405197
360.885488	17381.664321	29.410215
361.061706	17415.754482	29.415232
361.652317	17444.146832	29.420250
361.954035	17464.756040	29.425268
362.232719	17501.132365	29.430285
362.907997	17524.663583	29.435303
363.353609	17548.255054	29.440320
362.957033	17576.425411	29.445338
363.700833	17609.671354	29.450356
363.935647	17647.146112	29.455373
364.220625	17672.397532	29.460391
364.862395	17712.270239	29.465408
364.770807	17742.020157	29.470426
365.470602	17774.025271	29.475444
365.550566	17809.497350	29.480461
366.407825	17844.339107	29.485479
366.819754	17861.257583	29.490496
367.215990	17902.911837	29.495514
367.484387	17917.896368	29.500532
367.798987	17943.561016	29.505549
368.307294	17969.768904	29.510567
368.770978	17991.833653	29.515584
368.831355	18023.819352	29.520602
369.219873	18030.932101	29.525620
369.533488	18060.008374	29.530637
369.883771	18087.106553	29.535655
370.282788	18106.380964	29.540672
370.696565	18140.924984	29.545690
371.200328	18160.956066	29.550708
371.503391	18188.804734	29.555725
371.470563	18222.325939	29.560743
371.778835	18254.081735	29.565760
372.251939	18292.506768	29.570778
372.096830	18330.793474	29.575796
372.620581	18363.281395	29.580813
373.361353	18406.604272	29.585831
373.677930	18432.162150	29.590848
373.742872	18473.500829	29.595866
374.755842	18509.445259	29.600884
374.981248	18537.602200	29.605901
375.238132	18579.298635	29.610919
376.109809	18603.219670	29.615936
375.776664	18640.483602	29.620954
376.417681	18664.026860	29.625972
376.941399	18696.587954	29.630989
377.678718	18720.935045	29.636007
378.576924	18732.746363	29.641024
378.963225	18759.680433	29.646042
380.318013	18751.547982	29.651060
380.969782	18771.427525	29.656077
380.852227	18774.650433	29.661095
381.177526	18788.770287	29.666112
381.326025	18798.396684	29.671130
382.303191	18803.983726	29.676148
382.762791	18809.494366	29.681165
383.010674	18811.745391	29.686183
383.974491	18806.476059	29.691200
383.600323	18804.928694	29.696218
383.809782	18813.890748	29.701236
383.833443	18837.090663	29.706253
383.807113	18844.818125	29.711271
384.871316	18864.151607	29.716288
384.875342	18886.483072	29.721306
384.905719	18902.059788	29.726324
385.712974	18927.186950	29.731341
385.716084	18938.467641	29.736359
386.120546	18954.336972	29.741376
386.078137	18979.728311	29.746394
386.413238	19008.673403	29.751412
387.156133	19039.469377	29.756429
387.193081	19072.679594	29.761447
387.724313	19101.245444	29.766464
387.691745	19130.064217	29.771482
388.420589	19159.831729	29.776500
388.639366	19193.278408	29.781517
388.722238	19228.513398	29.786535
389.121232	19240.877796	29.791552
389.327299	19287.523592	29.796570
390.006795	19330.991480	29.801588
390.411275	19359.290327	29.806605
390.640138	19408.398324	29.811623
390.980724	19442.764867	29.816640
391.230239	19483.708061	29.821658
391.922046	19510.769170	29.826676
392.313353	19555.683882	29.831693
392.646563	19590.865440	29.836711
393.172733	19614.211560	29.841728
393.604245	19645.739858	29.846746
394.239498	19676.690471	29.851764
394.869390	19685.625725	29.856781
394.883351	19716.190883	29.861799
395.601623	19741.931564	29.866816
395.957256	19769.783599	29.871834
395.760320	19801.083926	29.876852
396.005297	19822.600957	29.881869
396.329513	19858.662708	29.886887
396.890326	19893.330978	29.891904
396.807846	19932.066482	29.896922
397.381615	19969.753441	29.901940
398.123460	20011.787533	29.906957
398.053962	20050.787593	29.911975
398.727454	20085.708715	29.916992
399.212000	20119.679088	29.922010
399.496411	20160.083679	29.927028
399.663600	20196.281022	29.932045
400.568053	20233.580989	29.937063
401.377955	20262.950741	29.942080
401.494526	20300.886234	29.947098
401.730355	20332.290668	29.952116
402.197875	20363.046534	29.957133
402.697944	20393.770248	29.962151
402.932793	20427.937227	29.967168
403.891858	20463.380857	29.972186
404.373774	20481.904819	29.977204
405.157357	20516.252010	29.982221
405.320086	20540.558460	29.987239
405.667873	20572.356243	29.992256
405.912560	20608.372903	29.997274
406.321102	20636.638548	30.002292
406.759537	20660.924603	30.007309
406.881823	20702.967162	30.012327
407.359917	20732.717637	30.017344
407.613646	20762.215330	30.022362
408.300920	20784.450024	30.027380
408.718021	20817.463381	30.032397
408.981737	20860.859249	30.037415
409.658470	20873.555544	30.042432
409.772811	20916.954294	30.047450
410.333053	20947.298514	30.052468
410.725744	20987.158929	30.057485
410.580786	21024.850965	30.062503
411.380360	21051.604985	30.067520
411.523227	21098.837060	30.072538
412.071532	21125.424813	30.077556
412.484702	21176.691051	30.082573
412.669272	21219.593300	30.087591
413.271339	21255.006452	30.092608
413.381642	21297.670543	30.097626
414.053112	21331.289098	30.102644
415.700546	21335.097551	30.107661
416.202314	21358.686659	30.112679
416.782888	21384.734965	30.117696
417.246258	21395.847833	30.122714
417.776481	21435.826792	30.127732
418.253123	21425.079733	30.132749
418.341163	21458.574712	30.137767
418.540879	21466.737266	30.142784
418.677985	21488.734744	30.147802
418.910246	21512.346758	30.152820
419.517509	21538.807120	30.157837
419.147714	21583.623468	30.162855
419.219187	21615.264143	30.167872
419.909320	21652.385277	30.172890
419.949168	21695.096762	30.177908
420.700758	21730.503424	30.182925
420.674992	21774.214612	30.187943
421.489377	21810.027268	30.192960
422.001742	21836.570082	30.197978
421.960684	21884.470326	30.202996
422.515324	21919.219485	30.208013
422.771685	21958.166676	30.213031
423.582495	22000.689386	30.218048
423.677675	22038.205039	30.223066
423.684975	22076.001843	30.228084
424.216419	22119.586684	30.233101
424.557120	22178.936288	30.238119
424.828497	22218.425568	30.243136
425.413877	22279.513482	30.248154
425.581527	22329.255103	30.253172
426.498068	22369.202064	30.258189
426.515226	22433.057558	30.263207
427.222069	22468.358094	30.268224
427.711453	22524.325642	30.273242
428.413666	22561.703785	30.278260
429.531656	22601.285131	30.283277
429.467560	22652.187299	30.288295
429.809344	22683.912793	30.293312
430.408733	22726.994369	30.298330
430.835487	22765.092014	30.303348
431.255734	22807.787269	30.308365
431.700830	22848.885908	30.313383
432.254095	22896.141557	30.318400
432.320983	22934.420768	30.323418
433.002452	22986.830555	30.328436
433.620267	23019.240907	30.333453
433.591404	23068.284098	30.338471
434.321178	23113.235642	30.343488
435.093627	23143.304151	30.348506
435.264014	23192.905928	30.353524
435.949800	23219.652330	30.358541
436.072669	23264.522159	30.363559
436.387107	23310.426253	30.368576
436.976573	23355.499508	30.373594
437.389865	23406.526481	30.378612
437.662392	23441.119045	30.383629
438.235877	23497.492127	30.388647
438.910612	23531.909268	30.393664
439.354806	23565.633090	30.398682
439.621486	23621.693278	30.403700
440.321516	23656.718308	30.408717
440.623057	23697.768726	30.413735
441.195717	23734.671091	30.418752
441.653180	23769.198913	30.423770
441.844183	23813.101682	30.428788
442.762979	23848.819310	30.433805
443.302031	23880.818619	30.438823
443.665126	23923.694897	30.443840
443.996870	23959.354143	30.448858
444.307774	23999.471766	30.453876
445.126558	24031.517937	30.458893
445.582493	24070.134047	30.463911
445.544267	24109.592406	30.468928
446.490956	24137.221011	30.473946
446.454726	24184.822572	30.478964
447.226273	24214.432657	30.483981
447.729629	24259.380680	30.488999
448.098042	24287.834128	30.494016
448.657432	24333.716063	30.499034
449.087293	24361.121784	30.504052
449.537756	24403.581053	30.509069
449.882402	24433.271883	30.514087
450.436124	24472.437220	30.519104
451.251864	24498.135861	30.524122
451.229049	24535.302865	30.529140
452.158023	24555.999517	30.534157
452.687572	24570.060334	30.539175
452.909043	24598.772099	30.544192
453.588845	24615.236564	30.549210
454.068891	24652.459081	30.554228
454.490304	24667.957234	30.559245
454.500658	24694.594203	30.564263
454.950395	24719.350995	30.569280
455.494543	24742.893619	30.574298
456.131638	24782.282370	30.579316
456.319677	24801.509602	30.584333
456.826603	24838.860529	30.589351
457.078795	24879.906213	30.594368
457.948025	24904.382282	30.599386
458.112430	24934.214309	30.604404
458.276783	24967.156289	30.609421
458.315654	25011.054281	30.614439
459.053474	25041.437842	30.619456
460.226592	25071.209815	30.624474
460.025652	25116.447382	30.629492
460.526849	25154.519078	30.634509
460.566884	25199.048175	30.639527
461.543628	25251.631937	30.644544
462.432382	25270.017875	30.649562
463.096288	25313.500577	30.654580
463.310992	25330.790504	30.659597
463.868455	25370.900357	30.664615
463.881376	25406.732274	30.669632
464.899252	25443.457149	30.674650
465.168017	25490.207374	30.679668
465.456557	25521.196300	30.684685
465.840795	25561.316443	30.689703
466.014585	25595.608040	30.694720
466.461057	25638.285515	30.699738
466.619578	25686.300480	30.704756
467.306146	25739.829720	30.709773
467.600803	25801.445347	30.714791
467.833513	25845.871571	30.719808
468.648500	25887.526428	30.724826
468.922037	25939.661330	30.729844
469.381511	25983.394168	30.734861
470.162269	26030.650670	30.739879
470.734691	26079.086895	30.744896
471.969456	26099.513840	30.749914
472.538641	26134.355923	30.754932
473.238244	26170.728316	30.759949
473.556120	26203.404288	30.764967
473.968637	26228.790833	30.769984
474.461271	26254.375448	30.775002
474.357762	26300.997289	30.780020
475.010581	26336.305343	30.785037
475.379480	26370.502993	30.790055
475.822819	26420.201259	30.795072
476.124178	26463.551515	30.800090
476.781125	26511.284122	30.805108
477.156985	26550.739244	30.810125
477.248897	26584.809831	30.815143
477.874113	26636.427898	30.820160
478.391254	26681.225411	30.825178
478.813449	26728.508680	30.830196
479.648113	26768.998442	30.835213
480.151977	26807.912420	30.840231
480.358239	26843.295676	30.845248
481.127871	26879.408739	30.850266
481.294709	26933.198340	30.855284
481.523392	26973.388612	30.860301
481.842212	27029.872378	30.865319
482.552652	27075.260232	30.870336
483.549212	27119.250586	30.875354
483.404138	27157.516058	30.880372
483.952747	27191.843211	30.885389
484.996076	27222.271373	30.890407
485.395442	27251.194604	30.895424
486.362144	27275.825062	30.900442
486.862380	27309.737784	30.905460
486.926780	27326.622513	30.910477
487.404379	27373.611287	30.915495
487.772855	27408.495585	30.920512
488.235409	27441.742917	30.925530
488.375965	27494.516567	30.930548
488.935104	27527.596607	30.935565
489.546666	27587.367898	30.940583
489.916735	27628.943129	30.945600
490.236046	27677.848581	30.950618
490.239134	27725.876096	30.955636
490.543428	27782.058734	30.960653
490.957610	27824.778522	30.965671
491.597997	27883.975071	30.970688
492.515300	27933.242500	30.975706
492.654507	27993.333384	30.980724
493.317622	28034.700033	30.985741
493.638983	28104.448853	30.990759
494.087779	28163.037783	30.995776
494.831233	28212.905866	31.000794
495.214972	28264.587817	31.005812
496.155598	28320.840024	31.010829
496.722271	28370.154306	31.015847
497.244832	28421.996641	31.020864
497.889605	28469.799762	31.025882
499.121942	28501.883393	31.030900
500.209708	28533.757646	31.035917
500.844506	28552.485823	31.040935
500.756835	28601.903121	31.045952
501.367658	28623.449358	31.050970
502.008042	28662.288043	31.055988
502.229918	28692.732181	31.061005
502.828011	28728.467477	31.066023
502.981686	28771.122437	31.071040
503.528511	28801.553813	31.076058
503.991316	28844.227019	31.081076
504.213174	28880.447845	31.086093
504.751101	28934.901298	31.091111
504.836351	28985.798945	31.096128
505.507139	29022.002297	31.101146
505.834337	29071.617027	31.106164
506.198639	29123.746426	31.111181
506.956055	29184.625249	31.116199
507.252863	29234.967943	31.121216
508.329612	29258.560789	31.126234
509.380643	29307.087449	31.131252
509.777032	29342.851192	31.136269
510.570555	29381.287466	31.141287
511.035315	29423.425440	31.146304
511.656080	29454.385158	31.151322
512.261379	29484.044538	31.156340
512.884702	29507.306045	31.161357
513.767895	29527.527293	31.166375
514.088846	29567.004695	31.171392
514.633523	29574.574343	31.176410
514.953947	29615.171926	31.181428
515.177529	29648.327501	31.186445
515.418310	29673.138716	31.191463
515.642557	29709.916127	31.196480
516.276741	29761.428415	31.201498
516.801407	29791.669595	31.206516
516.829348	29833.171240	31.211533
517.242957	29872.719126	31.216551
517.457609	29924.995653	31.221568
517.547533	29970.740201	31.226586
517.738997	30016.335497	31.231604
518.216007	30089.262375	31.236621
518.442952	30140.632023	31.241639
518.801265	30205.871462	31.246656
519.617704	30271.104475	31.251674
519.886338	30335.444335	31.256692
520.276396	30405.739902	31.261709
521.045857	30458.209833	31.266727
521.439756	30539.768811	31.271744
522.328534	30603.154800	31.276762
522.965551	30657.281646	31.281780
523.494801	30711.256182	31.286797
524.795429	30755.886740	31.291815
525.163351	30811.699401	31.296832
526.115516	30860.638025	31.301850
526.880510	30908.907429	31.306868
527.133697	30965.228675	31.311885
527.510272	31015.919763	31.316903
527.887860	31073.217721	31.321920
528.514218	31121.024836	31.326938
529.344253	31178.664483	31.331956
529.512657	31231.769762	31.336973
530.613129	31270.723989	31.341991
531.011092	31327.170643	31.347008
531.295036	31371.539339	31.352026
532.063984	31421.358700	31.357044
532.524697	31482.496704	31.362061
532.940998	31517.870323	31.367079
533.038910	31575.471930	31.372096
534.365681	31610.779731	31.377114
535.095188	31668.822617	31.382132
535.353595	31713.906348	31.387149
535.983287	31759.420761	31.392167
536.456560	31818.626813	31.397184
536.794212	31867.670285	31.402202
537.505873	31919.090834	31.407220
537.527622	31969.666886	31.412237
538.315318	32031.831609	31.417255
538.330654	32101.382086	31.422272
538.841174	32153.808564	31.427290
539.415731	32208.976034	31.432308
539.682017	32271.663624	31.437325
540.348633	32331.975219	31.442343
540.976578	32397.727022	31.447360
541.222553	32472.835163	31.452378
542.186409	32532.782540	31.457396
542.586018	32583.909745	31.462413
543.623366	32657.189633	31.467431
543.997617	32723.117300	31.472448
544.312094	32772.025126	31.477466
544.718838	32826.556583	31.482484
545.053750	32910.591245	31.487501
545.824393	32968.003617	31.492519
546.554926	33038.944168	31.497536
547.072759	33105.234379	31.502554
547.846290	33164.193109	31.507572
548.297556	33218.169313	31.512589
548.869239	33274.394521	31.517607
549.854329	33334.009748	31.522624
551.263361	33374.517248	31.527642
552.138693	33402.185095	31.532660
552.358786	33442.148624	31.537677
553.268918	33480.473510	31.542695
554.179879	33504.938997	31.547712
554.996618	33524.027259	31.552730
555.310712	33543.217943	31.557748
555.690351	33577.560416	31.562765
556.561511	33594.503376	31.567783
556.766029	33633.810401	31.572800
557.185638	33648.786717	31.577818
557.644858	33676.224308	31.582836
557.673672	33707.166731	31.587853
557.897596	33743.892632	31.592871
558.339029	33789.983132	31.597888
558.965316	33836.967659	31.602906
559.682085	33878.727301	31.607924
559.709177	33932.712994	31.612941
560.187080	33979.908722	31.617959
560.264735	34028.805680	31.622976
560.763488	34096.298752	31.627994
561.667248	34149.779776	31.633012
561.938897	34226.276399	31.638029
562.320942	34279.191212	31.643047
562.626296	34354.272176	31.648064
563.273232	34417.093452	31.653082
563.769571	34484.746178	31.658100
564.418006	34558.395116	31.663117
565.039466	34625.024059	31.668135
565.751241	34692.594459	31.673152
566.140389	34752.802539	31.678170
566.821245	34826.996308	31.683188
567.257633	34899.290143	31.688205
568.127224	34973.787698	31.693223
568.592944	35035.012816	31.698240
569.079627	35107.744114	31.703258
569.738148	35177.641593	31.708276
570.236402	35241.948466	31.713293
571.329201	35315.312125	31.718311
571.963955	35365.354177	31.723328
572.833939	35421.574479	31.728346
573.732180	35474.583835	31.733364
574.236629	35539.263145	31.738381
574.714201	35592.778223	31.743399
575.372976	35648.276877	31.748416
575.912518	35708.330637	31.753434
576.518728	35756.784752	31.758452
576.780391	35821.634786	31.763469
577.417918	35872.618277	31.768487
577.832713	35939.677759	31.773504
578.405181	35995.999756	31.778522
579.102275	36061.639945	31.783540
579.141445	36117.934104	31.788557
579.954826	36191.003726	31.793575
580.311332	36257.935203	31.798592
580.688748	36329.591268	31.803610
581.710423	36397.627904	31.808628
581.595173	36473.301997	31.813645
582.581308	36546.656827	31.818663
583.243627	36612.964425	31.823680
583.880858	36681.523607	31.828698
584.729674	36752.673838	31.833716
585.309752	36821.615468	31.838733
585.620245	36881.483920	31.843751
586.277770	36950.125967	31.848768
586.976144	37013.244448	31.853786
587.958016	37076.344482	31.858804
588.029763	37147.155019	31.863821
589.061143	37217.645520	31.868839
589.576853	37263.906185	31.873856
589.842212	37334.849430	31.878874
590.544712	37389.664425	31.883892
590.808888	37454.100109	31.888909
591.291968	37518.831085	31.893927
592.144783	37586.540416	31.898944
592.988152	37645.417048	31.903962
594.377412	37684.050121	31.908980
595.235148	37718.939756	31.913997
596.228561	37758.244732	31.919015
597.302679	37789.771801	31.924032
597.805137	37820.702608	31.929050
598.477482	37857.068898	31.934068
598.878515	37887.584240	31.939085
599.192320	37926.030269	31.944103
599.607433	37974.178016	31.949120
599.904886	38010.894093	31.954138
600.533808	38053.025216	31.959156
600.470829	38105.059291	31.964173
601.271028	38166.176353	31.969191
601.596632	38214.058677	31.974208
601.923779	38279.247525	31.979226
602.737077	38339.690676	31.984244
602.878140	38406.416495	31.989261
603.324055	38474.019936	31.994279
603.838097	38542.521379	31.999296
604.434010	38611.056833	32.004314
604.979519	38679.474653	32.009332
605.362000	38760.640511	32.014349
606.078970	38830.687593	32.019367
606.927916	38900.391064	32.024384
607.322713	38981.110786	32.029402
608.427565	39052.738874	32.034420
608.981014	39112.501724	32.039437
609.714637	39177.304316	32.044455
610.579689	39252.498902	32.049472
611.180781	39315.303770	32.054490
612.165584	39387.609679	32.059508
612.834017	39445.807785	32.064525
613.256016	39506.736447	32.069543
614.075268	39568.151765	32.074560
614.640281	39629.268583	32.079578
615.125149	39686.137415	32.084596
615.550550	39751.981254	32.089613
616.051181	39824.097804	32.094631
616.787562	39884.773494	32.099648
617.211097	39952.335606	32.104666
618.029653	40011.164021	32.109684
619.030344	40073.359026	32.114701
619.732748	40129.959516	32.119719
620.454212	40195.534816	32.124736
620.592339	40265.942353	32.129754
621.102505	40325.713188	32.134772
621.598922	40394.821115	32.139789
622.350642	40461.841306	32.144807
622.972991	40541.381035	32.149824
623.242162	40609.681474	32.154842
624.112751	40674.845434	32.159860
624.147537	40752.826294	32.164877
624.616768	40833.753308	32.169895
625.007675	40907.186634	32.174912
625.527532	40994.940582	32.179930
626.197969	41079.898184	32.184948
626.850570	41166.011413	32.189965
627.328740	41263.594733	32.194983
628.261672	41336.712471	32.200000
628.745974	41432.837156	32.205018
629.375146	41514.059447	32.210036
630.042438	41599.016800	32.215053
630.589846	41688.019631	32.220071
631.890020	41764.386629	32.225088
632.610483	41844.026172	32.230106
632.530852	41902.435175	32.235124
633.483358	41974.213597	32.240141
634.635076	42034.694807	32.245159
636.775766	42070.011142	32.250176
637.747113	42124.461018	32.255194
639.519291	42147.175640	32.260212
639.863116	42163.267092	32.265229
640.586619	42196.668997	32.270247
641.216284	42221.792844	32.275264
641.222657	42264.412696	32.280282
641.730875	42297.054936	32.285300
642.237857	42340.674735	32.290317
642.308580	42380.673233	32.295335
642.871228	42437.547104	32.300352
642.656871	42493.874527	32.305370
643.543710	42549.438371	32.310388
643.920761	42616.468598	32.315405
644.316489	42688.266459	32.320423
644.375751	42748.186289	32.325440
644.811572	42836.228113	32.330458
645.400483	42912.904215	32.335476
645.932205	42999.244934	32.340493
646.404842	43090.612723	32.345511
646.738867	43170.293699	32.350528
647.575621	43266.798745	32.355546
648.135246	43367.259029	32.360564
648.797241	43455.897683	32.365581
649.045351	43550.115003	32.370599
649.987871	43647.561125	32.375616
650.575566	43737.773178	32.380634
652.204553	43827.828567	32.385652
652.673308	43908.977443	32.390669
653.794585	43992.632659	32.395687
654.577534	44064.494660	32.400704
655.257903	44153.291440	32.405722
656.552132	44216.774587	32.410740
657.588493	44279.135666	32.415757
658.186738	44343.663087	32.420775
659.384710	44407.020777	32.425792
660.263073	44452.408872	32.430810
660.825699	44510.217361	32.435828
661.379305	44565.242615	32.440845
661.855698	44625.916994	32.445863
662.440439	44688.565972	32.450880
663.200756	44744.624673	32.455898
663.924366	44801.990540	32.460916
664.821233	44860.916061	32.465933
665.013414	44917.871622	32.470951
665.781056	44974.832855	32.475968
666.079834	45043.608803	32.480986
666.955180	45103.211221	32.486004
667.452446	45161.679871	32.491021
667.843424	45221.123103	32.496039
668.424571	45293.566426	32.501056
668.590596	45368.434538	32.506074
669.535406	45455.725276	32.511092
669.997581	45533.986707	32.516109
670.592509	45609.845541	32.521127
671.536365	45688.217103	32.526144
671.882058	45769.959671	32.531162
672.570182	45851.440490	32.536180
673.361586	45921.820911	32.541197
673.791804	45997.718123	32.546215
674.645714	46075.648355	32.551232
675.041659	46162.900862	32.556250
675.418427	46242.786710	32.561268
676.261809	46328.854161	32.566285
677.180023	46428.396561	32.571303
677.849331	46499.920425	32.576320
678.093371	46574.347737	32.581338
678.769062	46650.266808	32.586356
679.263356	46726.080511	32.591373
679.669559	46821.137405	32.596391
680.716200	46898.991660	32.601408
681.139686	46994.229709	32.606426
681.558031	47081.760619	32.611444
682.337098	47166.910967	32.616461
682.789437	47263.655064	32.621479
683.529430	47353.855973	32.626496
684.398077	47446.767599	32.631514
684.961068	47533.079698	32.636532
685.862125	47638.568309	32.641549
686.431905	47728.183440	32.646567
687.272969	47816.099142	32.651584
687.928531	47898.933165	32.656602
689.204757	47997.296922	32.661620
690.191176	48067.435018	32.666637
690.795791	48172.997907	32.671655
691.558352	48254.151393	32.676672
692.237489	48326.220528	32.681690
693.144369	48414.484929	32.686708
694.010099	48490.010285	32.691725
694.697007	48576.524442	32.696743
695.451151	48642.979743	32.701760
696.253990	48727.053017	32.706778
696.823259	48804.081597	32.711796
698.198170	48879.899786	32.716813
698.493939	48965.324730	32.721831
698.995940	49045.062570	32.726848
699.763171	49126.073699	32.731866
700.204985	49204.334656	32.736884
700.777361	49283.070106	32.741901
701.175108	49372.339345	32.746919
702.148087	49465.515075	32.751936
702.436201	49562.231735	32.756954
702.914282	49655.702155	32.761972
703.885659	49740.298280	32.766989
704.349809	49833.790827	32.772007
705.292892	49929.952111	32.777024
705.746494	50016.584130	32.782042
706.849023	50130.833363	32.787060
707.595292	50214.584586	32.792077
708.325775	50310.274555	32.797095
709.426807	50387.511773	32.802112
710.491576	50483.431365	32.807130
710.747652	50556.330818	32.812148
712.574510	50613.922700	32.817165
713.191146	50700.135910	32.822183
714.240785	50766.764275	32.827200
714.739453	50841.886032	32.832218
715.040158	50907.742192	32.837236
715.980286	50984.509462	32.842253
716.631724	51051.413379	32.847271
717.460362	51121.497225	32.852288
718.343269	51195.337354	32.857306
718.719051	51273.696630	32.862324
719.187485	51354.220286	32.867341
719.538125	51431.365146	32.872359
720.000400	51510.677559	32.877376
720.895489	51596.924340	32.882394
721.395692	51689.251165	32.887412
722.445431	51764.442945	32.892429
723.014740	51859.462938	32.897447
723.725028	51937.124983	32.902464
724.553385	52022.557149	32.907482
724.987754	52116.368895	32.912500
726.275168	52170.441377	32.917517
726.913844	52253.871814	32.922535
727.467873	52331.637183	32.927552
728.078616	52405.457601	32.932570
728.901361	52483.766502	32.937588
729.917452	52564.311648	32.942605
730.232109	52637.044923	32.947623
730.566947	52718.196573	32.952640
731.344623	52804.082815	32.957658
731.958701	52896.529125	32.962676
732.637362	52964.161641	32.967693
733.359858	53061.752338	32.972711
733.856471	53156.228430	32.977728
735.064095	53248.040855	32.982746
735.595227	53332.896313	32.987764
736.502853	53416.748272	32.992781
737.304943	53509.482160	32.997799
738.382070	53593.685814	33.002816
739.155842	53687.625657	33.007834
739.818647	53765.587163	33.012852
740.670178	53839.215068	33.017869
741.537526	53940.349464	33.022887
742.206685	54029.955164	33.027904
742.983076	54117.559581	33.032922
743.101921	54213.398687	33.037940
743.932619	54304.236132	33.042957
744.313217	54402.572615	33.047975
744.962210	54506.930551	33.052992
745.406704	54609.471730	33.058010
745.778180	54719.399035	33.063028
746.436093	54818.563483	33.068045
747.080555	54939.870273	33.073063
747.748393	55069.078278	33.078080
748.861323	55167.398094	33.083098
749.644741	55277.974107	33.088116
750.821635	55394.001496	33.093133
751.750688	55490.123000	33.098151
752.714291	55601.675561	33.103168
753.498260	55693.228516	33.108186
754.141248	55808.664552	33.113204
755.392756	55908.077128	33.118221
756.126068	56004.953953	33.123239
757.048594	56099.506133	33.128256
758.359347	56190.708549	33.133274
758.895138	56283.019444	33.138292
759.658612	56366.351811	33.143309
760.696927	56466.763040	33.148327
761.237357	56544.067061	33.153344
762.055761	56645.052800	33.158362
762.351686	56741.803614	33.163380
763.612127	56821.706344	33.168397
764.292203	56923.537925	33.173415
764.565330	57019.352334	33.178432
765.238460	57115.890688	33.183450
765.574156	57231.518683	33.188468
766.167423	57326.782213	33.193485
766.917223	57440.800806	33.198503
767.266546	57547.777409	33.203520
768.248235	57650.782234	33.208538
768.668372	57776.434322	33.213556
769.752224	57892.030407	33.218573
770.968718	58000.887664	33.223591
771.870511	58106.372643	33.228608
773.283357	58187.911219	33.233626
774.083887	58299.935661	33.238644
774.952709	58391.139338	33.243661
775.530858	58491.144199	33.248679
776.300950	58582.643192	33.253696
777.083685	58660.427046	33.258714
777.386257	58762.343269	33.263732
778.021377	58859.332375	33.268749
779.041664	58949.843562	33.273767
779.409187	59050.233741	33.278784
780.405331	59144.408908	33.283802
781.180975	59234.247853	33.288820
781.738715	59329.722687	33.293837
783.108793	59424.721860	33.298855
783.849381	59520.856104	33.303872
785.184121	59612.512516	33.308890
785.774231	59708.204960	33.313908
786.641524	59803.586409	33.318925
787.147916	59892.480746	33.323943
787.744175	60002.210167	33.328960
788.662236	60090.872722	33.333978
789.030504	60194.491659	33.338996
790.015744	60282.101092	33.344013
790.917370	60384.494853	33.349031
791.416746	60499.709933	33.354048
792.175879	60590.992310	33.359066
792.881238	60687.972198	33.364084
794.203001	60790.936609	33.369101
794.895106	60881.314982	33.374119
795.630350	60992.189605	33.379136
796.597023	61095.366185	33.384154
796.548728	61210.473942	33.389172
797.820942	61317.254096	33.394189
798.481932	61422.025243	33.399207
798.937050	61538.947417	33.404224
800.087145	61655.552644	33.409242
800.735521	61766.022415	33.414260
801.577935	61881.005060	33.419277
802.446757	61998.834558	33.424295
802.789277	62116.739451	33.429312
803.805487	62228.711859	33.434330
803.906497	62359.672502	33.439348
804.783482	62486.099613	33.444365
805.784493	62609.770014	33.449383
806.244922	62738.669722	33.454400
807.239001	62866.622020	33.459418
807.990476	62992.655901	33.464436
808.580986	63131.055759	33.469453
809.746952	63252.989669	33.474471
810.682818	63387.313777	33.479488
811.605306	63504.340224	33.484506
812.568522	63637.378243	33.489524
813.502623	63766.888433	33.494541
814.506944	63882.594964	33.499559
815.604471	64007.237511	33.504576
816.384431	64114.802929	33.509594
816.987001	64247.936343	33.514612
817.806954	64368.632084	33.519629
818.694061	64490.404655	33.524647
819.274722	64613.575263	33.529664
820.097352	64719.840849	33.534682
820.577099	64861.760092	33.539700
821.378865	64985.578924	33.544717
822.426284	65113.302366	33.549735
823.546107	65249.826875	33.554752
824.552485	65360.762180	33.559770
825.408814	65482.216942	33.564788
826.141529	65589.804155	33.569805
826.977367	65724.570903	33.574823
827.723289	65850.698932	33.579840
828.406560	65961.899681	33.584858
829.118169	66088.376216	33.589876
829.642791	66224.879454	33.594893
830.696639	66324.881458	33.599911
831.543322	66445.654327	33.604928
832.825152	66557.504880	33.609946
833.653239	66667.452549	33.614964
834.339576	66783.645225	33.619981
835.287634	66887.903252	33.624999
835.717197	67011.429174	33.630016
836.511320	67124.564901	33.635034
837.530065	67241.204383	33.640052
838.429114	67360.418558	33.645069
839.099501	67470.586267	33.650087
839.603270	67608.518136	33.655104
840.512128	67719.924672	33.660122
841.511502	67841.647528	33.665140
842.459660	67969.493358	33.670157
843.368336	68090.638396	33.675175
844.275287	68221.603235	33.680192
845.179279	68350.982420	33.685210
845.816944	68469.354760	33.690228
846.896165	68591.220419	33.695245
847.760146	68715.354391	33.700263
848.609453	68831.183538	33.705280
849.672148	68950.449063	33.710298
850.716841	69069.813088	33.715316
851.383521	69190.163648	33.720333
852.703349	69300.675679	33.725351
853.356499	69424.905694	33.730368
854.415380	69534.488532	33.735386
855.655465	69647.026273	33.740404
856.330909	69769.326106	33.745421
856.989787	69873.387592	33.750439
857.906611	69997.197797	33.755456
858.877215	70105.748601	33.760474
859.857795	70230.384219	33.765492
860.754220	70332.827744	33.770509
861.648902	70446.236383	33.775527
862.915539	70553.981552	33.780544
863.581533	70658.823427	33.785562
864.291127	70768.944809	33.790580
864.563090	70890.995530	33.795597
865.883578	71007.877504	33.800615
866.602045	71126.965706	33.805632
867.392032	71251.581980	33.810650
868.525325	71380.049872	33.815668
868.989380	71491.145246	33.820685
870.160124	71612.633542	33.825703
870.555874	71738.133791	33.830720
871.000010	71863.424385	33.835738
871.926154	71993.561792	33.840756
872.578576	72127.666068	33.845773
873.464808	72254.308372	33.850791
874.234884	72391.075992	33.855808
875.298758	72521.630054	33.860826
876.515815	72660.203345	33.865844
877.255796	72794.923275	33.870861
878.165953	72935.427439	33.875879
878.723176	73070.331182	33.880896
879.669230	73206.688978	33.885914
880.393279	73335.660106	33.890932
881.127193	73493.202343	33.895949
882.490452	73626.925971	33.900967
883.094874	73768.567671	33.905984
883.807320	73904.589158	33.911002
884.744929	74046.114119	33.916020
885.125389	74188.288996	33.921037
886.194947	74327.789098	33.926055
887.288710	74472.699690	33.931072
889.530131	74573.510770	33.936090
890.559656	74694.046812	33.941108
891.279046	74806.805359	33.946125
892.413009	74901.901071	33.951143
893.132129	75030.440304	33.956160
894.084075	75138.494493	33.961178
894.877789	75251.932361	33.966196
895.448935	75358.324228	33.971213
896.501024	75471.290276	33.976231
897.219840	75596.961498	33.981248
898.161755	75704.254848	33.986266
899.494347	75818.124825	33.991284
900.205176	75934.002325	33.996301
901.072753	76048.526216	34.001319
901.358478	76166.486763	34.006336
902.499573	76299.207310	34.011354
903.444265	76424.421990	34.016372
904.360082	76546.840233	34.021389
905.192362	76660.006966	34.026407
905.944361	76791.783048	34.031424
907.794609	76906.350696	34.036442
908.893484	77013.997528	34.041460
909.699154	77127.841520	34.046477
910.867154	77236.211668	34.051495
911.623506	77355.997968	34.056512
912.337757	77473.179601	34.061530
913.336929	77587.303765	34.066548
913.500863	77720.719971	34.071565
914.614346	77843.416164	34.076583
915.289549	77968.424931	34.081600
915.825572	78107.676895	34.086618
916.695471	78248.424039	34.091636
917.178301	78383.638293	34.096653
918.240808	78523.292528	34.101671
919.169783	78676.955512	34.106688
919.869755	78823.990410	34.111706
920.876158	78969.798856	34.116724
921.815742	79114.132812	34.121741
922.414626	79272.586230	34.126759
923.607281	79418.316070	34.131776
926.274170	79529.877134	34.136794
927.281578	79648.305622	34.141812
928.075156	79786.544755	34.146829
929.048379	79905.423074	34.151847
929.379702	80042.399402	34.156864
930.202549	80179.193775	34.161882
930.743737	80316.149583	34.166900
931.570663	80464.217897	34.171917
932.261462	80602.042575	34.176935
933.275892	80745.419304	34.181952
934.383232	80902.933097	34.186970
935.476640	81049.404777	34.191988
936.074354	81187.956989	34.197005
937.104394	81326.925423	34.202023
938.065069	81477.230293	34.207040
939.108714	81627.610954	34.212058
940.072450	81777.297313	34.217076
940.730619	81923.018081	34.222093
941.998017	82066.785024	34.227111
943.073644	82212.919176	34.232128
943.713369	82359.721293	34.237146
944.983545	82488.275088	34.242164
945.557342	82647.926627	34.247181
946.735322	82793.130134	34.252199
947.388073	82938.307839	34.257216
948.293509	83085.032541	34.262234
949.243186	83244.752385	34.267252
950.347544	83405.048717	34.272269
951.220921	83532.680892	34.277287
952.225623	83667.473017	34.282304
953.244972	83805.047352	34.287322
954.193441	83940.400847	34.292340
954.668728	84089.810038	34.297357
955.584352	84236.211367	34.302375
956.079390	84379.709677	34.307392
957.362369	84535.276847	34.312410
958.297840	84667.960371	34.317428
958.868428	84835.599813	34.322445
959.637126	84987.478003	34.327463
961.389690	85130.525512	34.332480
962.749685	85264.540329	34.337498
964.336815	85405.579580	34.342516
965.088774	85552.933835	34.347533
966.210012	85691.837534	34.352551
967.841733	85820.425795	34.357568
968.255872	85946.198582	34.362586
969.554679	86084.505673	34.367604
970.177688	86234.093940	34.372621
971.028931	86366.952973	34.377639
971.620658	86508.088127	34.382656
972.210441	86656.975904	34.387674
973.470929	86802.336339	34.392692
973.957873	86969.562018	34.397709
974.873296	87136.141949	34.402727
975.833619	87295.204403	34.407744
976.777625	87460.592241	34.412762
977.423483	87622.189631	34.417780
978.564489	87790.989511	34.422797
979.733422	87950.622926	34.427815
980.822795	88121.490354	34.432832
981.423837	88284.593136	34.437850
982.408065	88448.639637	34.442868
983.069360	88640.192776	34.447885
984.348497	88805.300247	34.452903
985.254952	88978.849423	34.457920
986.178105	89163.762869	34.462938
987.203606	89329.675470	34.467956
988.179431	89511.798364	34.472973
989.024881	89686.894303	34.477991
990.215813	89868.231125	34.483008
992.332469	90021.076169	34.488026
993.377533	90180.143868	34.493044
994.569365	90343.042444	34.498061
995.313110	90497.485338	34.503079
996.409012	90674.167087	34.508096
997.279979	90828.445434	34.513114
998.069005	90991.143100	34.518132
999.189213	91168.330750	34.523149
1000.382589	91336.166016	34.528167
1001.503385	91489.116027	34.533184
1002.279648	91657.421464	34.538202
1003.451688	91823.523169	34.543220
1004.349865	91984.665114	34.548237
1005.910620	92144.723496	34.553255
1006.571887	92298.552344	34.558272
1007.389845	92464.881752	34.563290
1008.654811	92622.485980	34.568308
1009.255804	92795.777897	34.573325
1010.257041	92960.440980	34.578343
1011.390838	93125.507249	34.583360
1011.933032	93299.053013	34.588378
1013.049383	93464.637156	34.593396
1013.875230	93640.524501	34.598413
1014.201552	93801.912594	34.603431
1015.236887	93983.008543	34.608448
1016.106243	94175.767344	34.613466
1017.602810	94350.655999	34.618484
1018.573822	94533.665600	34.623501
1019.196750	94693.003782	34.628519
1020.396787	94870.850725	34.633536
1021.479848	95047.268808	34.638554
1022.456615	95209.912801	34.643572
1023.192711	95382.257381	34.648589
1024.726456	95545.596084	34.653607
1026.957227	95702.236923	34.658624
1027.708225	95866.929329	34.663642
1028.808204	96025.962723	34.668660
1030.126543	96166.065240	34.673677
1031.022496	96325.710453	34.678695
1032.767430	96461.243048	34.683712
1033.667797	96622.231448	34.688730
1034.974624	96767.511131	34.693748
1035.740844	96929.859478	34.698765
1036.145642	97081.317190	34.703783
1037.559404	97226.493173	34.708800
1038.490979	97395.805946	34.713818
1039.403573	97553.215237	34.718836
1040.267421	97717.236413	34.723853
1041.114208	97877.013633	34.728871
1042.262808	98036.191022	34.733888
1043.218821	98211.918214	34.738906
1044.653283	98364.263717	34.743924
1045.935767	98528.480279	34.748941
1047.006630	98687.320153	34.753959
1048.062805	98841.522929	34.758976
1048.665894	99011.907676	34.763994
1049.687268	99194.677172	34.769012
1050.721570	99364.916772	34.774029
1051.192481	99537.979672	34.779047
1052.665418	99702.127926	34.784064
1053.128619	99885.602786	34.789082
1054.440789	100068.849472	34.794100
1055.151635	100248.322532	34.799117
1055.997970	100435.181962	34.804135
1057.398883	100608.762608	34.809152
1058.453477	100796.546153	34.814170
1059.722013	100971.189564	34.819188
1060.960616	101150.847308	34.824205
1061.864386	101344.104931	34.829223
1062.979961	101523.621074	34.834240
1064.115896	101705.294161	34.839258
1064.891264	101892.460892	34.844276
1066.139482	102076.194737	34.849293
1067.436337	102252.716322	34.854311
1069.282454	102414.793879	34.859328
1070.229133	102600.455681	34.864346
1071.450617	102757.497592	34.869364
1072.875838	102944.918699	34.874381
1073.632110	103110.803268	34.879399
1074.818984	103281.569055	34.884416
1075.655116	103461.968157	34.889434
1076.115049	103632.742875	34.894452
1077.404003	103813.841793	34.899469
1077.961279	104004.510919	34.904487
1078.917839	104185.540916	34.909504
1080.239841	104373.464326	34.914522
1081.181762	104564.846245	34.919540
1082.478449	104752.877890	34.924557
1083.201359	104936.396107	34.929575
1084.964538	105109.269202	34.934592
1086.484003	105272.305241	34.939610
1087.689530	105454.531167	34.944628
1089.029506	105627.034597	34.949645
1089.825932	105805.733936	34.954663
1091.071710	105968.021772	34.959680
1091.886290	106139.577160	34.964698
1093.172467	106285.369998	34.969716
1094.542845	106446.322889	34.974733
1096.487493	106573.503831	34.979751
1098.292743	106694.236398	34.984768
1099.291388	106829.808143	34.989786
1100.109705	106977.189609	34.994804
1101.360621	107106.831354	34.999821
1102.106092	107239.496059	35.004839
1102.924095	107397.949846	35.009856
1103.683082	107550.676669	35.014874
1104.622344	107694.419551	35.019892
1105.296423	107855.344469	35.024909
1105.819077	108018.714719	35.029927
1106.956532	108181.451980	35.034944
1108.537800	108342.013981	35.039962
1109.374739	108503.713741	35.044980
1110.840090	108681.510690	35.049997
1111.466355	108848.605406	35.055015
1112.651693	109009.186400	35.060032
1113.550504	109190.918693	35.065050
1114.844114	109381.162162	35.070068
1115.911368	109539.511194	35.075085
1116.387192	109733.528209	35.080103
1117.732777	109922.918162	35.085120
1118.575998	110106.261857	35.090138
1119.617701	110302.405804	35.095156
1121.016090	110481.847073	35.100173
1122.267524	110669.446400	35.105191
1123.556813	110849.212199	35.110208
1124.547998	111052.742412	35.115226
1125.600823	111243.317506	35.120244
1126.528819	111439.273110	35.125261
1127.331168	111645.372600	35.130279
1128.640660	111837.214021	35.135296
1129.846812	112045.377733	35.140314
1130.673641	112256.874331	35.145332
1131.671920	112463.352804	35.150349
1132.855902	112662.771067	35.155367
1133.894768	112873.147713	35.160384
1134.991521	113089.559250	35.165402
1135.539911	113307.203617	35.170420
1136.602768	113526.284587	35.175437
1137.380363	113757.804739	35.180455
1138.424363	113982.086643	35.185472
1139.860869	114214.768164	35.190490
1140.753566	114446.249574	35.195508
1142.119091	114672.751444	35.200525
1143.292651	114919.177905	35.205543
1144.333699	115145.598044	35.210560
1145.538468	115376.173801	35.215578
1146.584121	115607.018559	35.220596
1147.783278	115846.607231	35.225613
1148.554938	116086.420883	35.230631
1149.603000	116327.432365	35.235648
1150.550744	116571.110584	35.240666
1151.704267	116815.960420	35.245684
1153.059996	117062.273910	35.250701
1154.479103	117322.187069	35.255719
1155.878131	117554.534777	35.260736
1157.433617	117796.462770	35.265754
1159.229233	118034.336332	35.270772
1160.704391	118257.490789	35.275789
1162.712049	118451.060656	35.280807
1164.832253	118641.128620	35.285824
1166.267276	118841.524416	35.290842
1167.071839	119026.199850	35.295860
1168.611923	119219.687701	35.300877
1169.551374	119401.770876	35.305895
1170.371318	119583.203430	35.310912
1171.297079	119772.425217	35.315930
1172.087533	119955.765708	35.320948
1173.490471	120148.953022	35.325965
1174.246378	120332.732445	35.330983
1175.428805	120529.595647	35.336000
1176.289089	120721.596898	35.341018
1177.177147	120924.733501	35.346036
1177.939234	121128.348598	35.351053
1178.944169	121347.055424	35.356071
1179.905588	121565.036095	35.361088
1181.021555	121792.953237	35.366106
1182.128492	122002.992751	35.371124
1183.593495	122214.000835	35.376141
1184.686239	122444.131861	35.381159
1186.090702	122668.852378	35.386176
1187.679134	122887.321699	35.391194
1188.445338	123108.349544	35.396212
1189.563515	123335.745872	35.401229
1190.546360	123563.369146	35.406247
1191.681112	123783.149558	35.411264
1192.965278	124036.212327	35.416282
1193.990599	124275.810262	35.421300
1194.930911	124502.129653	35.426317
1195.675290	124757.734004	35.431335
1197.028405	125007.206830	35.436352
1198.289050	125251.665527	35.441370
1198.984650	125509.958487	35.446388
1200.446383	125756.719896	35.451405
1201.596483	126018.046916	35.456423
1202.796595	126283.677130	35.461440
1203.959123	126540.709971	35.466458
1204.990552	126799.312999	35.471476
1206.245292	127075.270716	35.476493
1207.283764	127338.858228	35.481511
1208.576910	127602.342372	35.486528
1209.989380	127874.364547	35.491546
1211.615539	128123.361138	35.496564
1213.793722	128374.765164	35.501581
1215.314290	128621.742566	35.506599
1216.825885	128855.249530	35.511616
1218.970259	129079.603027	35.516634
1219.885720	129323.238631	35.521652
1221.644175	129537.392250	35.526669
1222.905676	129764.939244	35.531687
1223.829197	129991.834100	35.536704
1225.401414	130211.055489	35.541722
1226.396663	130437.028986	35.546740
1227.733917	130655.671310	35.551757
1228.806462	130875.575961	35.556775
1230.417624	131094.226584	35.561792
1231.459809	131326.333931	35.566810
1232.735069	131544.548988	35.571828
1233.643892	131762.953081	35.576845
1234.451871	131992.594174	35.581863
1235.572130	132226.457159	35.586880
1237.040128	132462.533314	35.591898
1238.380698	132678.628245	35.596916
1239.782022	132892.394670	35.601933
1240.797434	133132.227120	35.606951
1242.264469	133354.289167	35.611968
1243.579898	133582.336176	35.616986
1244.241566	133807.361929	35.622004
1245.692215	134041.880519	35.627021
1246.781659	134281.683834	35.632039
1248.105872	134506.667916	35.637056
1249.709704	134728.412400	35.642074
1250.573225	134946.680695	35.647092
1251.867411	135162.457548	35.652109
1253.469709	135374.241884	35.657127
1254.741776	135584.446896	35.662144
1256.263134	135787.512182	35.667162
1257.200625	136007.613568	35.672180
1258.506256	136216.321015	35.677197
1259.512273	136419.526370	35.682215
1260.030250	136653.774555	35.687232
1261.392768	136881.519714	35.692250
1262.381878	137125.607655	35.697268
1263.633491	137348.404394	35.702285
1264.882069	137595.698473	35.707303
1265.739998	137833.892359	35.712320
1266.766803	138078.564221	35.717338
1267.440693	138338.891608	35.722356
1268.760101	138588.767767	35.727373
1270.063289	138863.157415	35.732391
1270.782463	139130.190698	35.737408
1272.195348	139402.613899	35.742426
1274.181470	139653.718670	35.747444
1276.178021	139899.244530	35.752461
1277.317473	140152.167104	35.757479
1278.571609	140417.448020	35.762496
1280.302478	140675.513131	35.767514
1280.916276	140933.182168	35.772532
1282.323751	141183.886925	35.777549
1283.563741	141464.495810	35.782567
1284.637226	141722.360774	35.787584
1286.051276	142003.896179	35.792602
1287.598380	142268.851071	35.797620
1288.814284	142530.134815	35.802637
1290.302096	142784.413724	35.807655
1291.513829	143056.785006	35.812672
1293.112847	143313.179678	35.817690
1294.312508	143585.595103	35.822708
1295.766573	143848.269427	35.827725
1296.918567	144121.812827	35.832743
1298.305165	144385.466096	35.837760
1299.785567	144651.122099	35.842778
1301.084569	144909.442253	35.847796
1302.685455	145165.735893	35.852813
1304.356334	145424.112230	35.857831
1305.938776	145680.095572	35.862848
1307.346074	145919.496630	35.867866
1308.760684	146172.860820	35.872884
1309.909822	146428.921348	35.877901
1311.614983	146665.957161	35.882919
1313.196197	146911.410658	35.887936
1315.150668	147143.703174	35.892954
1316.430476	147381.752688	35.897972
1317.532698	147607.214232	35.902989
1318.978811	147846.925956	35.908007
1319.608493	148089.881872	35.913024
1321.194322	148325.667330	35.918042
1322.066723	148578.174292	35.923060
1322.587937	148817.627202	35.928077
1323.868148	149079.632795	35.933095
1324.756975	149345.218333	35.938112
1327.150990	149602.286788	35.943130
1328.222784	149863.393927	35.948148
1329.215476	150119.797843	35.953165
1330.462909	150390.011473	35.958183
1331.175974	150658.717555	35.963200
1332.501565	150908.717260	35.968218
1333.588929	151198.115350	35.973236
1334.806452	151460.287531	35.978253
1336.058383	151733.630236	35.983271
1337.164947	152003.929517	35.988288
1338.631647	152273.879262	35.993306
1340.633544	152525.718121	35.998324
1342.115841	152767.357976	36.003341
1343.686946	153013.880732	36.008359
1344.999324	153277.901570	36.013376
1346.613955	153532.804758	36.018394
1347.764803	153796.297818	36.023412
1349.036414	154044.893663	36.028429
1350.375968	154294.367757	36.033447
1351.059418	154554.848426	36.038464
1352.677941	154820.084786	36.043482
1354.176880	155090.607006	36.048500
1355.163681	155349.089185	36.053517
1356.470014	155622.513815	36.058535
1357.753073	155906.269916	36.063552
1358.678354	156184.759581	36.068570
1359.983891	156470.431470	36.073588
1360.782515	156765.716229	36.078605
1362.200726	157072.685280	36.083623
1363.781764	157349.983397	36.088640
1365.708972	157640.660187	36.093658
1366.764984	157925.901800	36.098676
1368.063329	158227.000661	36.103693
1369.720405	158526.545330	36.108711
1370.446568	158835.114150	36.113728
1372.022424	159129.551558	36.118746
1373.387803	159432.982496	36.123764
1375.208755	159732.648407	36.128781
1377.758337	160007.837706	36.133799
1379.353567	160303.371372	36.138816
1380.984827	160571.701066	36.143834
1382.115633	160860.223908	36.148852
1383.438072	161141.244456	36.153869
1384.951473	161426.942066	36.158887
1385.853816	161727.155350	36.163904
1387.091188	162012.750488	36.168922
1388.238341	162317.507424	36.173940
1389.424627	162620.598045	36.178957
1391.269300	162916.248389	36.183975
1392.509237	163210.630832	36.188992
1393.893357	163510.929153	36.194010
1395.117134	163809.289597	36.199028
1396.300458	164104.042840	36.204045
1398.410739	164416.432646	36.209063
1399.414775	164716.459861	36.214080
1400.990460	165018.551318	36.219098
1402.309598	165316.487680	36.224116
1403.989977	165613.033929	36.229133
1405.506311	165911.157356	36.234151
1406.682812	166228.422357	36.239168
1408.112370	166527.021136	36.244186
1409.312051	166829.745741	36.249204
1411.267912	167122.158122	36.254221
1412.726930	167422.978562	36.259239
1414.110277	167719.702435	36.264256
1416.277243	168005.830079	36.269274
1418.020781	168290.075674	36.274292
1418.878562	168582.476675	36.279309
1420.528016	168875.535022	36.284327
1421.479956	169179.471309	36.289344
1423.174058	169472.665695	36.294362
1425.345889	169742.155290	36.299380
1426.548723	170014.408468	36.304397
1428.293155	170292.753218	36.309415
1429.709019	170578.805916	36.314432
1431.061407	170844.757901	36.319450
1432.490465	171129.162172	36.324468
1433.837104	171395.676618	36.329485
1435.028177	171651.025965	36.334503
1435.708436	171936.143055	36.339520
1437.209420	172198.728005	36.344538
1438.300901	172468.488741	36.349556
1439.439168	172755.666786	36.354573
1440.646664	173051.705538	36.359591
1441.933271	173342.758433	36.364608
1442.985411	173622.659099	36.369626
1444.437980	173921.314903	36.374644
1445.665792	174241.063383	36.379661
1447.209177	174545.202999	36.384679
1448.681032	174860.219602	36.389696
1450.668690	175165.951936	36.394714
1451.391813	175465.563133	36.399732
1452.722598	175788.007886	36.404749
1454.165226	176108.062999	36.409767
1455.145726	176443.273816	36.414784
1456.348275	176774.718886	36.419802
1457.917208	177103.909836	36.424820
1459.324537	177455.136531	36.429837
1461.227594	177789.416594	36.434855
1462.411312	178126.838729	36.439872
1463.842177	178470.974069	36.444890
1465.665381	178806.238671	36.449908
1467.277859	179148.368590	36.454925
1469.252518	179480.376116	36.459943
1470.724186	179824.856508	36.464960
1472.219147	180156.947936	36.469978
1473.634229	180490.552405	36.474996
1475.240078	180844.714097	36.480013
1477.182115	181149.563795	36.485031
1479.016281	181489.755908	36.490048
1480.173424	181805.781880	36.495066
1482.383205	182125.849124	36.500084
1484.383642	182438.705554	36.505101
1486.443507	182758.230296	36.510119
1487.423895	183075.917776	36.515136
1488.886201	183386.863520	36.520154
1490.377343	183704.723883	36.525172
1491.556055	184043.860500	36.530189
1493.051211	184351.430007	36.535207
1494.443330	184683.858696	36.540224
1495.604425	185015.134540	36.545242
1497.131329	185348.941145	36.550260
1498.342861	185678.029360	36.555277
1499.783239	186014.989562	36.560295
1501.038283	186356.476007	36.565312
1501.985415	186688.990465	36.570330
1503.314531	187039.290782	36.575348
1505.497327	187379.829906	36.580365
1507.659825	187712.707393	36.585383
1509.365251	188043.796597	36.590400
1510.818574	188370.232752	36.595418
1512.638635	188695.924475	36.600436
1514.094649	189033.191892	36.605453
1515.617536	189359.583993	36.610471
1516.905793	189697.873197	36.615488
1518.459068	190032.718340	36.620506
1519.840011	190356.295976	36.625524
1521.081283	190706.328308	36.630541
1522.962515	191026.995787	36.635559
1524.547426	191364.686729	36.640576
1525.795387	191699.833021	36.645594
1527.125717	192032.187369	36.650612
1528.808314	192381.280310	36.655629
1530.516894	192720.189667	36.660647
1531.738247	193042.005448	36.665664
1533.323126	193372.750678	36.670682
1534.749123	193684.595698	36.675700
1536.106204	193999.360877	36.680717
1538.153211	194311.715432	36.685735
1539.755141	194627.496858	36.690752
1540.668374	194946.669413	36.695770
1542.625898	195274.303287	36.700788
1543.934693	195600.903794	36.705805
1546.096937	195904.766511	36.710823
1547.932203	196225.620716	36.715840
1549.629923	196545.432875	36.720858
1551.226501	196851.450478	36.725876
1552.252918	197177.331273	36.730893
1554.185164	197494.024107	36.735911
1555.341979	197815.950731	36.740928
1556.404399	198141.792199	36.745946
1558.156007	198472.408950	36.750964
1559.101051	198817.240933	36.755981
1560.511223	199160.854912	36.760999
1562.189190	199507.778014	36.766016
1563.389810	199870.601507	36.771034
1564.553047	200228.951307	36.776052
1565.814498	200595.475827	36.781069
1567.506331	200964.063923	36.786087
1569.241277	201328.495047	36.791104
1570.636621	201696.907579	36.796122
1572.270559	202073.294036	36.801140
1573.683431	202460.587486	36.806157
1575.121537	202841.403477	36.811175
1576.542821	203211.660485	36.816192
1578.061317	203604.643391	36.821210
1579.918161	203994.106030	36.826228
1581.468747	204391.227000	36.831245
1583.063223	204770.643048	36.836263
1584.896088	205156.370068	36.841280
1586.434198	205554.083302	36.846298
1588.080574	205943.489325	36.851316
1589.902859	206336.550390	36.856333
1591.279108	206717.713715	36.861351
1593.045441	207122.622015	36.866368
1594.744207	207528.864141	36.871386
1596.591653	207910.932841	36.876404
1598.571971	208303.634687	36.881421
1599.981001	208688.458968	36.886439
1601.836383	209081.147203	36.891456
1603.417851	209464.765666	36.896474
1604.974340	209849.901105	36.901492
1606.391740	210252.317924	36.906509
1608.194593	210632.603602	36.911527
1609.904316	211017.350759	36.916544
1612.100047	211395.974777	36.921562
1614.878843	211741.259940	36.926580
1617.310199	212102.857828	36.931597
1619.408497	212445.896720	36.936615
1620.939530	212793.373816	36.941632
1622.476756	213143.746483	36.946650
1624.284266	213493.821756	36.951668
1625.702010	213834.185159	36.956685
1627.492001	214160.037201	36.961703
1629.031147	214498.732159	36.966720
1630.418102	214844.996581	36.971738
1631.882841	215175.731617	36.976756
1633.478298	215527.830811	36.981773
1634.916101	215871.017518	36.986791
1636.160576	216223.736228	36.991808
1637.242916	216582.476977	36.996826
1638.833366	216926.505692	37.001844
1639.951119	217294.513414	37.006861
1641.453611	217649.658147	37.011879
1642.618193	218004.936357	37.016896
1644.135082	218357.643016	37.021914
1645.887239	218713.893073	37.026932
1648.511700	219107.005227	37.031949
1650.388501	219442.181916	37.036967
1652.707291	219769.844660	37.041984
1654.342542	220112.048147	37.047002
1656.327312	220440.885895	37.052020
1657.424826	220777.491356	37.057037
1658.743013	221118.633095	37.062055
1660.184451	221464.835271	37.067072
1661.532730	221821.873972	37.072090
1662.934521	222175.222090	37.077108
1664.223059	222544.007411	37.082125
1665.663647	222909.873224	37.087143
1667.049383	223290.988923	37.092160
1668.580875	223673.504099	37.097178
1670.428773	224057.822262	37.102196
1671.575192	224457.446917	37.107213
1673.106567	224846.569840	37.112231
1676.391439	225202.205897	37.117248
1679.112501	225566.115198	37.122266
1681.068042	225924.488277	37.127284
1682.465542	226296.137480	37.132301
1684.482736	226648.431827	37.137319
1686.732978	226999.621725	37.142336
1688.258900	227358.146294	37.147354
1690.192483	227704.234357	37.152372
1691.912282	228062.423931	37.157389
1693.444716	228427.529040	37.162407
1695.163712	228778.837163	37.167424
1696.375713	229142.574889	37.172442
1697.596844	229509.461742	37.177460
1699.005727	229881.449384	37.182477
1700.039525	230267.699194	37.187495
1701.719189	230652.598367	37.192512
1703.084737	231043.316626	37.197530
1704.934705	231425.471723	37.202548
1706.750527	231824.906156	37.207565
1708.574136	232231.554266	37.212583
1710.416109	232617.650880	37.217600
1711.949742	233013.782232	37.222618
1713.808356	233415.017181	37.227636
1715.362118	233811.121783	37.232653
1717.158918	234214.096253	37.237671
1718.732747	234624.703696	37.242688
1719.924806	235038.448997	37.247706
1721.318907	235452.771452	37.252724
1723.377210	235867.899275	37.257741
1724.914212	236294.773849	37.262759
1726.626563	236713.999841	37.267776
1728.393574	237130.855360	37.272794
1730.761362	237528.230607	37.277812
1732.703655	237949.300994	37.282829
1734.330566	238366.004612	37.287847
1736.477145	238792.783798	37.292864
1737.866657	239196.954472	37.297882
1739.367299	239624.528292	37.302900
1740.837743	240038.492404	37.307917
1742.611847	240466.352815	37.312935
1744.237490	240880.496016	37.317952
1746.223896	241317.010452	37.322970
1747.897600	241742.121054	37.327988
1749.340011	242161.910833	37.333005
1750.958607	242594.093946	37.338023
1752.991650	243023.872091	37.343040
1754.364180	243456.935734	37.348058
1756.364248	243880.090688	37.353076
1757.770424	244287.925321	37.358093
1759.229105	244702.331139	37.363111
1761.197981	245115.306663	37.368128
1762.845350	245535.804449	37.373146
1764.234274	245957.819002	37.378164
1766.145140	246390.670835	37.383181
1767.627799	246828.166715	37.388199
1769.998877	247247.175060	37.393216
1771.132358	247682.596047	37.398234
1773.049142	248106.989892	37.403252
1775.041798	248560.127796	37.408269
1777.423769	248973.319007	37.413287
1780.039915	249403.872896	37.418304
1781.443571	249824.111281	37.423322
1783.288123	250249.103580	37.428340
1785.064457	250681.144221	37.433357
1786.626977	251113.576312	37.438375
1788.240787	251543.358335	37.443392
1789.701590	251988.179306	37.448410
1791.655401	252429.667312	37.453428
1793.851228	252857.829657	37.458445
1796.390644	253283.903084	37.463463
1798.933210	253701.389954	37.468480
1800.555850	254130.765773	37.473498
1802.503274	254554.524681	37.478516
1804.638717	254966.262291	37.483533
1806.300488	255387.579373	37.488551
1808.030162	255803.195025	37.493568
1809.514396	256235.109573	37.498586
1811.485462	256663.387115	37.503604
1813.185725	257090.033013	37.508621
1814.623537	257530.821307	37.513639
1816.078009	257958.422596	37.518656
1817.737068	258413.273167	37.523674
1819.145040	258852.745567	37.528692
1821.044365	259306.997480	37.533709
1822.490952	259765.642951	37.538727
1824.963401	260215.227242	37.543744
1826.669112	260663.007865	37.548762
1827.943109	261122.240607	37.553780
1830.047921	261588.829535	37.558797
1832.058983	262055.306839	37.563815
1833.637774	262511.618088	37.568832
1835.307328	262992.402842	37.573850
1837.212002	263470.277842	37.578868
1838.944632	263941.525450	37.583885
1840.522649	264422.172184	37.588903
1842.653888	264892.489456	37.593920
1844.155163	265367.381743	37.598938
1845.999469	265849.863182	37.603956
1848.116415	266338.929267	37.608973
1849.645318	266829.235489	37.613991
1851.880606	267308.627896	37.619008
1853.900154	267797.124465	37.624026
1855.836938	268269.020651	37.629044
1857.894154	268749.203152	37.634061
1859.795467	269231.062121	37.639079
1862.311725	269702.530426	37.644096
1864.397225	270172.037283	37.649114
1865.988061	270640.888809	37.654132
1867.933394	271114.177268	37.659149
1869.802053	271581.965356	37.664167
1871.829296	272046.728963	37.669184
1873.283569	272513.542818	37.674202
1874.822024	272994.211861	37.679220
1876.658750	273475.033910	37.684237
1878.360916	273943.353950	37.689255
1880.388262	274404.836826	37.694272
1882.069202	274866.350884	37.699290
1883.608830	275326.947632	37.704308
1885.829702	275765.406768	37.709325
1887.853544	276239.308648	37.714343
1889.768679	276691.635622	37.719360
1891.578721	277149.643821	37.724378
1893.440865	277600.352017	37.729396
1895.583291	278061.326121	37.734413
1897.633010	278529.706599	37.739431
1901.223491	278934.427252	37.744448
1904.411715	279344.954598	37.749466
1906.580611	279774.066388	37.754484
1909.114903	280177.918029	37.759501
1911.192489	280585.578555	37.764519
1913.104669	280985.137033	37.769536
1914.631049	281387.603558	37.774554
1916.394631	281803.238759	37.779572
1918.076012	282191.783096	37.784589
1919.321278	282625.791391	37.789607
1921.113636	283040.860055	37.794624
1922.653493	283473.648921	37.799642
1923.917488	283909.124103	37.804660
1925.217036	284366.005513	37.809677
1927.008721	284812.364194	37.814695
1928.924280	285272.138288	37.819712
1931.190853	285719.838165	37.824730
1933.414647	286170.363322	37.829748
1935.823194	286619.307062	37.834765
1937.087623	287077.253063	37.839783
1939.203468	287519.892320	37.844800
1941.142072	287985.851979	37.849818
1942.718962	288451.616010	37.854836
1944.587075	288922.130918	37.859853
1946.064363	289408.914403	37.864871
1947.829762	289886.809080	37.869888
1949.466371	290376.229658	37.874906
1950.833190	290880.806154	37.879924
1952.872438	291385.574060	37.884941
1954.518603	291902.978014	37.889959
1956.326285	292415.628685	37.894976
1957.666947	292939.378033	37.899994
1959.397762	293473.499689	37.905012
1961.870738	293998.783968	37.910029
1963.816190	294530.884091	37.915047
1965.513582	295061.752877	37.920064
1967.469928	295597.452898	37.925082
1969.656504	296138.826972	37.930100
1971.998743	296680.147188	37.935117
1974.255009	297216.856366	37.940135
1976.489142	297738.911513	37.945152
1978.138288	298274.699956	37.950170
1980.608680	298807.809753	37.955188
1983.300171	299327.215909	37.960205
1985.312602	299864.967703	37.965223
1987.774459	300378.437908	37.970240
1989.879658	300886.605577	37.975258
1992.133598	301409.984558	37.980276
1994.597664	301900.232883	37.985293
1996.767242	302400.737218	37.990311
1999.400251	302885.415804	37.995328
2001.911343	303373.413684	38.000346
2003.592421	303850.676539	38.005364
2006.063191	304329.202904	38.010381
2007.983786	304808.579758	38.015399
2009.824842	305285.097387	38.020416
2011.252387	305760.436506	38.025434
2012.783943	306247.742868	38.030452
2014.629437	306707.185652	38.035469
2016.114796	307191.218201	38.040487
2017.868379	307660.829470	38.045504
2019.599723	308139.076346	38.050522
2021.082223	308632.040344	38.055540
2022.854497	309126.705669	38.060557
2024.529269	309634.411920	38.065575
2026.099783	310142.310003	38.070592
2027.804398	310663.337228	38.075610
2029.469023	311189.979884	38.080628
2031.502670	311725.903083	38.085645
2033.088856	312267.915166	38.090663
2034.477733	312823.288074	38.095680
2036.401728	313389.868632	38.100698
2038.169477	313963.377917	38.105716
2040.009221	314533.772813	38.110733
2041.797146	315121.083909	38.115751
2043.366303	315719.574131	38.120768
2045.243086	316317.805270	38.125786
2047.271605	316941.805351	38.130804
2049.641708	317549.238130	38.135821
2051.625260	318176.104013	38.140839
2054.106453	318782.821971	38.145856
2056.515640	319404.527684	38.150874
2058.658898	320020.685544	38.155892
2061.409863	320619.597835	38.160909
2063.903295	321230.303489	38.165927
2066.463751	321820.273305	38.170944
2068.543539	322438.450314	38.175962
2070.274837	323036.468256	38.180980
2072.218254	323646.531209	38.185997
2074.163572	324263.570195	38.191015
2076.415507	324876.566107	38.196032
2078.397504	325492.164992	38.201050
2080.674240	326113.853074	38.206068
2083.008281	326719.758735	38.211085
2085.391797	327330.956345	38.216103
2087.715546	327947.946159	38.221120
2090.189112	328548.707040	38.226138
2092.100951	329163.442002	38.231156
2095.091660	329751.867847	38.236173
2097.518334	330349.038205	38.241191
2099.813438	330933.733627	38.246208
2101.998899	331531.667742	38.251226
2103.998774	332114.013454	38.256244
2106.447706	332697.954207	38.261261
2108.882613	333267.903376	38.266279
2111.091003	333846.312231	38.271296
2113.226197	334421.655410	38.276314
2114.801654	335015.844885	38.281332
2116.893408	335598.290551	38.286349
2118.758902	336179.828075	38.291367
2120.895347	336770.757330	38.296384
2122.931697	337364.742592	38.301402
2124.728690	337961.603699	38.306420
2126.705301	338548.122426	38.311437
2128.879563	339144.348879	38.316455
2130.916892	339744.093863	38.321472
2133.205789	340347.648219	38.326490
2135.057184	340950.100166	38.331508
2137.204065	341549.602321	38.336525
2139.662311	342152.675215	38.341543
2141.487850	342748.484849	38.346560
2143.944602	343353.979761	38.351578
2145.984530	343956.591934	38.356596
2148.507937	344556.882982	38.361613
2150.715239	345151.279850	38.366631
2152.418212	345742.986361	38.371648
2154.784834	346324.601358	38.376666
2156.311784	346897.084743	38.381684
2158.686870	347478.277833	38.386701
2161.005316	348050.159025	38.391719
2162.780054	348632.198271	38.396736
2165.085760	349197.646475	38.401754
2166.832049	349780.741543	38.406772
2169.025199	350369.464917	38.411789
2171.357213	350961.862548	38.416807
2173.786755	351538.401104	38.421824
2176.121150	352121.951708	38.426842
2178.221218	352718.348168	38.431860
2180.453723	353297.078483	38.436877
2182.390078	353903.077704	38.441895
2184.452814	354495.421132	38.446912
2186.786399	355095.882070	38.451930
2188.380919	355708.154365	38.456948
2190.744504	356315.849990	38.461965
2192.615322	356928.591573	38.466983
2194.756158	357555.361438	38.472000
2197.499953	358173.547484	38.477018
2199.598060	358813.879623	38.482036
2201.556151	359441.741943	38.487053
2204.011112	360056.040010	38.492071
2205.994692	360688.978387	38.497088
2208.442327	361324.138642	38.502106
2210.615858	361944.873091	38.507124
2213.246293	362582.240872	38.512141
2216.014227	363208.615942	38.517159
2217.680767	363848.126917	38.522176
2220.006553	364472.855131	38.527194
2221.803280	365135.738499	38.532212
2224.082392	365765.349503	38.537229
2226.240702	366413.691206	38.542247
2228.299849	367062.165065	38.547264
2231.163008	367704.939367	38.552282
2233.387308	368363.991934	38.557300
2235.232086	369011.275310	38.562317
2237.362366	369670.700709	38.567335
2239.151820	370336.993806	38.572352
2241.185135	371003.056826	38.577370
2242.743277	371684.531365	38.582388
2244.984022	372381.782763	38.587405
2247.195241	373072.557999	38.592423
2249.093216	373779.654278	38.597440
2251.023583	374479.832694	38.602458
2253.497723	375182.798333	38.607476
2255.646762	375901.121550	38.612493
2258.207425	376606.174485	38.617511
2260.022206	377332.587937	38.622528
2263.079416	378031.671414	38.627546
2265.345274	378745.351374	38.632564
2267.827834	379464.812808	38.637581
2270.319197	380151.723727	38.642599
2272.858782	380870.461012	38.647616
2275.870237	381570.873382	38.652634
2278.119921	382258.516268	38.657652
2280.636688	382950.842056	38.662669
2282.945086	383656.372256	38.667687
2285.755187	384337.869643	38.672704
2288.266498	385001.274204	38.677722
2291.076023	385698.335600	38.682740
2293.476637	386361.020548	38.687757
2296.240641	387022.135785	38.692775
2298.552369	387687.520510	38.697792
2301.268450	388344.002066	38.702810
2303.511242	388994.033150	38.707828
2306.136149	389637.878077	38.712845
2308.592119	390239.454520	38.717863
2310.632708	390859.871731	38.722880
2312.632842	391467.862336	38.727898
2314.368290	392078.774391	38.732916
2317.038083	392703.840911	38.737933
2318.717966	393327.841799	38.742951
2320.363724	393956.119025	38.747968
2322.420525	394592.856684	38.752986
2324.234408	395237.934330	38.758004
2326.234331	395895.158107	38.763021
2328.256742	396561.462211	38.768039
2329.789127	397250.717790	38.773056
2331.971664	397928.774615	38.778074
2334.288584	398626.560638	38.783092
2336.228432	399326.774482	38.788109
2338.743878	400027.332233	38.793127
2341.058622	400748.457445	38.798144
2343.645168	401443.064506	38.803162
2345.791770	402163.649691	38.808180
2348.492360	402878.068886	38.813197
2351.096730	403598.364360	38.818215
2353.154239	404329.956375	38.823232
2355.292900	405046.668429	38.828250
2358.722353	405763.300326	38.833268
2361.245365	406472.817751	38.838285
2364.158342	407190.562147	38.843303
2366.479283	407902.330868	38.848320
2369.160520	408621.748070	38.853338
2371.960117	409329.296154	38.858356
2374.341803	410036.438887	38.863373
2376.740692	410747.942504	38.868391
2378.834197	411471.079254	38.873408
2380.825985	412188.260607	38.878426
2383.821603	412905.864266	38.883444
2386.199371	413624.437165	38.888461
2388.850896	414343.603587	38.893479
2390.988807	415063.392421	38.898496
2393.570424	415770.399207	38.903514
2396.162885	416502.964090	38.908532
2398.145716	417217.248246	38.913549
2401.116938	417931.931342	38.918567
2403.335545	418659.380903	38.923584
2405.291986	419381.839050	38.928602
2407.962312	420112.185562	38.933620
2410.188690	420855.903528	38.938637
2412.698990	421575.421622	38.943655
2414.839320	422313.387928	38.948672
2417.266367	423047.157769	38.953690
2419.846551	423785.539089	38.958708
2421.824274	424527.188011	38.963725
2424.447350	425272.201396	38.968743
2426.511494	426020.170579	38.973760
2429.478560	426750.094473	38.978778
2432.359324	427493.832446	38.983796
2434.766244	428230.234157	38.988813
2437.807973	428967.014396	38.993831
2440.603605	429692.016992	38.998848
2443.392487	430411.176865	39.003866
2445.830869	431141.408403	39.008884
2448.040596	431864.973253	39.013901
2450.539866	432573.687181	39.018919
2452.601367	433314.340798	39.023936
2454.480422	434053.735610	39.028954
2456.865394	434785.228515	39.033972
2458.900237	435529.915310	39.038989
2461.497009	436271.701329	39.044007
2463.509077	437019.177613	39.049024
2465.720379	437760.776513	39.054042
2467.958692	438493.743698	39.059060
2469.746620	439227.267638	39.064077
2472.052590	439963.110780	39.069095
2474.308294	440697.369403	39.074112
2477.031071	441428.237571	39.079130
2479.755467	442167.480525	39.084148
2482.188479	442915.044629	39.089165
2484.761737	443662.610700	39.094183
2486.997832	444422.146789	39.099200
2489.482042	445173.065597	39.104218
2491.528346	445943.608690	39.109236
2493.748487	446720.064796	39.114253
2496.150723	447497.525055	39.119271
2498.733428	448278.872738	39.124288
2500.653634	449077.954308	39.129306
2503.251191	449858.432319	39.134324
2505.730839	450675.165052	39.139341
2507.857154	451472.453102	39.144359
2510.761733	452295.728547	39.149376
2513.434844	453112.840158	39.154394
2515.847364	453936.941402	39.159412
2518.061411	454768.374999	39.164429
2520.881264	455584.100697	39.169447
2523.543510	456425.910784	39.174464
2526.507642	457237.956795	39.179482
2529.157717	458067.667596	39.184500
2531.864902	458907.598111	39.189517
2534.624746	459730.953471	39.194535
2537.306315	460566.623011	39.199552
2539.658002	461400.239690	39.204570
2542.369991	462226.027934	39.209588
2545.209511	463055.501187	39.214605
2548.176248	463892.298098	39.219623
2550.668298	464722.668583	39.224640
2553.066589	465558.073455	39.229658
2555.898293	466396.908536	39.234676
2558.102363	467245.413123	39.239693
2560.898460	468083.473707	39.244711
2563.297539	468928.890644	39.249728
2565.993646	469759.112981	39.254746
2568.887380	470602.454146	39.259764
2570.896841	471459.647058	39.264781
2573.607396	472294.657428	39.269799
2576.318645	473132.257844	39.274816
2578.979659	473987.763196	39.279834
2582.185853	474825.357762	39.284852
2584.712681	475686.263348	39.289869
2587.895475	476511.814296	39.294887
2590.429397	477353.649168	39.299904
2592.761500	478188.913180	39.304922
2596.057084	479006.707330	39.309940
2599.201828	479836.862899	39.314957
2601.957659	480644.017151	39.319975
2604.610807	481461.201539	39.324992
2607.007680	482280.714221	39.330010
2609.237850	483098.550981	39.335028
2611.679276	483925.252392	39.340045
2614.509875	484743.571143	39.345063
2616.882488	485584.192411	39.350080
2618.900433	486404.891596	39.355098
2621.675476	487233.706361	39.360116
2623.572087	488078.074028	39.365133
2626.704497	488912.050871	39.370151
2629.402998	489756.962129	39.375168
2632.020762	490592.861868	39.380186
2634.847836	491444.685425	39.385204
2637.122607	492278.188602	39.390221
2639.968258	493100.253045	39.395239
2642.677739	493915.841561	39.400256
2645.414315	494703.886344	39.405274
2648.248645	495503.735953	39.410292
2651.065609	496305.720337	39.415309
2653.379895	497089.738435	39.420327
2656.136041	497890.850447	39.425344
2658.179575	498704.805438	39.430362
2660.883319	499510.641344	39.435380
2663.321557	500323.594713	39.440397
2665.825333	501141.995509	39.445415
2668.339996	501967.112768	39.450432
2670.947088	502797.065748	39.455450
2673.708716	503625.942683	39.460468
2675.929072	504470.702329	39.465485
2678.796259	505313.092516	39.470503
2681.633345	506152.317800	39.475520
2683.652020	507005.299518	39.480538
2686.105626	507873.290144	39.485556
2688.236898	508752.227793	39.490573
2691.007726	509634.389269	39.495591
2693.748270	510519.481389	39.500608
2696.402369	511412.654417	39.505626
2699.316352	512296.157207	39.510644
2701.764520	513211.038161	39.515661
2704.158710	514111.813490	39.520679
2706.658626	515035.500601	39.525696
2709.133766	515962.009760	39.530714
2711.918226	516884.079110	39.535732
2714.706040	517838.542846	39.540749
2717.914488	518758.969336	39.545767
2721.118255	519701.005734	39.550784
2723.525121	520626.995108	39.555802
2726.523676	521563.258296	39.560820
2729.280559	522509.225841	39.565837
2731.847835	523445.394252	39.570855
2734.557742	524391.655117	39.575872
2737.309303	525347.569753	39.580890
2740.163142	526290.564956	39.585908
2742.949156	527249.172837	39.590925
2745.654147	528194.338566	39.595943
2748.926936	529154.555945	39.600960
2751.409116	530121.840032	39.605978
2754.660354	531065.876187	39.610996
2756.837687	532033.689242	39.616013
2759.586506	532998.373931	39.621031
2762.438559	533955.025067	39.626048
2764.959637	534941.815750	39.631066
2767.629279	535907.578730	39.636084
2770.328976	536890.382031	39.641101
2772.983722	537877.755013	39.646119
2775.627064	538856.910572	39.651136
2778.161448	539840.142640	39.656154
2781.681146	540821.584131	39.661172
2784.724111	541815.009294	39.666189
2787.550092	542792.907300	39.671207
2790.526483	543780.218921	39.676224
2793.552726	544758.651047	39.681242
2796.758007	545736.984990	39.686260
2799.312533	546708.317424	39.691277
2802.545835	547676.955283	39.696295
2806.224093	548631.423133	39.701312
2809.288799	549582.406842	39.706330
2812.626047	550529.458694	39.711348
2815.110205	551474.122788	39.716365
2817.859147	552424.810220	39.721383
2821.056205	553369.526366	39.726400
2823.574414	554305.443035	39.731418
2826.191782	555239.871180	39.736436
2828.905857	556153.212448	39.741453
2832.554918	557015.332903	39.746471
2836.189486	557885.138140	39.751488
2839.488673	558754.489842	39.756506
2842.618433	559601.103963	39.761524
2846.264247	560449.236403	39.766541
2848.873555	561285.278908	39.771559
2852.236201	562123.404083	39.776576
2854.296894	562972.188653	39.781594
2856.734372	563819.198446	39.786612
2859.162400	564684.485506	39.791629
2861.804964	565533.057458	39.796647
2864.433629	566414.918549	39.801664
2866.622997	567293.578664	39.806682
2869.501525	568175.278188	39.811700
2871.812374	569072.674771	39.816717
2874.310227	569981.322880	39.821735
2876.851087	570893.413025	39.826752
2879.158086	571825.202450	39.831770
2881.629917	572759.405703	39.836788
2884.134047	573693.835771	39.841805
2886.630520	574655.496881	39.846823
2889.791956	575625.906161	39.851840
2892.454946	576590.301848	39.856858
2895.342384	577569.386197	39.861876
2898.466601	578552.919536	39.866893
2901.128476	579555.412733	39.871911
2904.000557	580544.447864	39.876928
2906.979352	581538.953127	39.881946
2910.419240	582539.169211	39.886964
2913.299713	583550.478393	39.891981
2916.066645	584563.928829	39.896999
2919.017322	585574.557053	39.902016
2921.204787	586611.346769	39.907034
2924.132553	587635.643543	39.912052
2926.942881	588689.045236	39.917069
2928.875196	589735.533029	39.922087
2931.790671	590802.063648	39.927104
2934.413455	591872.155321	39.932122
2937.324399	592948.015604	39.937140
2940.149554	594037.269845	39.942157
2942.836530	595137.117199	39.947175
2945.847157	596246.526195	39.952192
2948.648964	597356.866492	39.957210
2952.343379	598446.719995	39.962228
2955.690666	599553.555567	39.967245
2958.658658	600656.542651	39.972263
2961.634426	601759.523355	39.977280
2964.660609	602871.651996	39.982298
2968.592018	603954.538845	39.987316
2971.872520	605064.960864	39.992333
2974.927570	606161.598417	39.997351
2977.995500	607249.370161	40.002368
2980.898901	608350.175150	40.007386
2983.862323	609443.958016	40.012404
2987.010431	610524.546082	40.017421
2990.005589	611627.366686	40.022439
2993.068807	612719.262775	40.027456
2996.169274	613809.145076	40.032474
2999.647819	614897.007461	40.037492
3002.469482	615979.570897	40.042509
3005.732093	617069.605307	40.047527
3009.178425	618153.151762	40.052544
3011.430829	619226.040424	40.057562
3014.566410	620313.173651	40.062580
3017.494998	621400.932289	40.067597
3020.133643	622492.228125	40.072615
3023.654977	623563.579310	40.077632
3026.312505	624610.733274	40.082650
3029.095385	625658.913621	40.087668
3032.003699	626698.278275	40.092685
3034.635614	627767.808230	40.097703
3037.582640	628815.851509	40.102720
3040.465918	629880.632204	40.107738
3043.439483	630935.053862	40.112756
3046.531570	631985.805413	40.117773
3049.444054	633071.679922	40.122791
3052.183810	634149.483152	40.127808
3055.205865	635229.624403	40.132826
3058.396741	636315.864661	40.137844
3061.801327	637382.542661	40.142861
3064.914399	638481.644287	40.147879
3068.167649	639577.063175	40.152896
3071.660262	640658.356714	40.157914
3074.929220	641738.176505	40.162932
3078.508853	642829.502716	40.167949
3081.510083	643914.872752	40.172967
3084.955033	644998.507620	40.177984
3088.447824	646070.949026	40.183002
3091.477111	647149.685226	40.188020
3095.003465	648236.100470	40.193037
3097.856658	649319.867580	40.198055
3100.963443	650399.139218	40.203072
3103.552764	651503.597024	40.208090
3106.537172	652601.388938	40.213108
3109.178602	653714.362686	40.218125
3112.062327	654833.647732	40.223143
3114.700134	655942.883590	40.228160
3117.373495	657091.635914	40.233178
3120.477894	658231.068487	40.238196
3123.401221	659380.805612	40.243213
3126.116492	660548.615019	40.248231
3129.454684	661697.461928	40.253248
3132.622803	662874.674022	40.258266
3135.708077	664044.787993	40.263284
3139.124964	665220.826050	40.268301
3142.208095	666403.840977	40.273319
3145.404735	667592.362658	40.278336
3148.667259	668773.362436	40.283354
3151.643053	669960.480445	40.288372
3155.363762	671149.912654	40.293389
3158.263142	672333.760999	40.298407
3162.814462	673489.541179	40.303424
3167.188234	674641.877139	40.308442
3171.762107	675785.338491	40.313460
3175.313603	676917.098151	40.318477
3178.582097	678034.503133	40.323495
3181.746693	679161.579998	40.328512
3185.055166	680267.676740	40.333530
3188.484150	681372.627078	40.338548
3191.870213	682496.477025	40.343565
3194.900575	683590.744523	40.348583
3198.342849	684689.580403	40.353600
3201.343882	685786.469610	40.358618
3204.913824	686878.167125	40.363636
3208.101386	687960.214680	40.368653
3210.689160	689061.144132	40.373671
3214.617391	690144.991043	40.378688
3217.700842	691228.300793	40.383706
3220.642122	692320.285831	40.388724
3223.893936	693397.945695	40.393741
3226.754261	694492.654844	40.398759
3229.850260	695583.370615	40.403776
3232.298350	696685.218306	40.408794
3235.329932	697801.808278	40.413812
3238.458368	698894.192335	40.418829
3241.337364	699970.368826	40.423847
3245.133565	701016.419048	40.428864
3248.543531	702057.550258	40.433882
3251.725682	703132.840654	40.438900
3254.501871	704197.311793	40.443917
3257.315555	705278.145314	40.448935
3260.634907	706338.002059	40.453952
3263.433298	707425.158083	40.458970
3266.421789	708506.152077	40.463988
3269.985003	709596.720200	40.469005
3273.424157	710711.036536	40.474023
3276.271588	711818.026973	40.479040
3279.341144	712926.717612	40.484058
3281.892212	714049.604016	40.489076
3285.117790	715181.335949	40.494093
3287.933249	716325.799918	40.499111
3290.713751	717487.430667	40.504128
3294.086531	718643.855499	40.509146
3297.308849	719826.311025	40.514164
3300.793651	720999.257629	40.519181
3303.747249	722194.378379	40.524199
3306.576601	723401.114336	40.529216
3309.755858	724618.590562	40.534234
3313.019630	725833.549747	40.539252
3316.768520	727038.167341	40.544269
3320.349800	728257.755534	40.549287
3323.489608	729482.718393	40.554304
3327.082256	730721.105106	40.559322
3330.213405	731967.725947	40.564340
3333.775008	733212.651459	40.569357
3337.339264	734457.927480	40.574375
3341.081279	735688.467392	40.579392
3344.042006	736940.023981	40.584410
3346.776228	738211.853578	40.589428
3350.403426	739471.342174	40.594445
3353.203502	740746.308570	40.599463
3356.837630	742024.335563	40.604480
3360.010877	743302.873067	40.609498
3362.930026	744600.082022	40.614516
3366.531668	745890.209278	40.619533
3369.847570	747194.959661	40.624551
3372.891676	748509.591324	40.629568
3376.224408	749829.078095	40.634586
3379.281356	751150.011849	40.639604
3382.774018	752473.505089	40.644621
3385.880653	753807.818305	40.649639
3389.396398	755136.760008	40.654656
3392.878050	756484.186448	40.659674
3395.966293	757847.242061	40.664692
3399.457308	759195.713722	40.669709
3402.573561	760561.772343	40.674727
3405.939330	761917.260110	40.679744
3409.819608	763286.586436	40.684762
3413.210677	764659.629591	40.689780
3417.261807	766015.888039	40.694797
3420.556088	767391.199590	40.699815
3423.845618	768748.807652	40.704832
3427.221936	770105.759945	40.709850
3430.797458	771485.525263	40.714868
3434.752199	772846.890589	40.719885
3438.458271	774205.736396	40.724903
3442.029508	775565.482200	40.729920
3445.578596	776921.541655	40.734938
3448.633695	778284.794231	40.739956
3452.258125	779639.500129	40.744973
3455.773640	781004.914086	40.749991
3459.388057	782367.943767	40.755008
3462.931861	783697.083128	40.760013
3466.276538	785004.372858	40.765018
3469.632878	786229.565395	40.770023
3472.957235	787408.789551	40.775028
3476.182007	788504.579211	40.780032
3479.765708	789539.255682	40.785037
3482.501851	790512.160262	40.790042
3485.439888	791417.298583	40.795047
3487.814764	792247.405486	40.800052
3490.203657	793008.404125	40.805056
3492.889842	793705.131989	40.810061
3495.260655	794333.535206	40.815066
3497.958751	794896.913983	40.820071
3500.515400	795397.472667	40.825076
3502.616193	795821.087744	40.830080
3504.869454	796193.103410	40.835085
3506.223273	796527.545567	40.840090
3508.481344	796787.009772	40.845095
3509.518428	797015.004227	40.850100
3511.143741	797190.911101	40.855104
3512.585896	797331.256537	40.860109
3513.548448	797411.303574	40.865114
3514.773131	797451.645695	40.870119
3515.772389	797472.832623	40.875124
3516.938308	797451.877029	40.880128
3518.184168	797407.003590	40.885133
3518.275375	797333.752682	40.890138
3518.886128	797221.833075	40.895143
3519.344929	797097.812150	40.900148
3520.177494	796952.815530	40.905152
3520.544347	796787.422434	40.910157
3520.825991	796613.497665	40.915162
3521.365294	796410.561501	40.920167
3521.659429	796200.099492	40.925172
3521.943382	795967.883527	40.930176
3522.299356	795720.476899	40.935181
3522.257896	795481.965016	40.940186
3523.051705	795205.548484	40.945191
3522.854982	794934.833341	40.950196
3522.656032	794644.662610	40.955200
3523.178345	794353.967833	40.960205
3522.647558	794059.408095	40.965210
3523.095442	793763.741168	40.970215
3523.496900	793454.268684	40.975220
3523.760628	793144.412416	40.980224
3523.575128	792817.229114	40.985229
3523.660168	792489.789417	40.990234
3523.646589	792156.849109	40.995239
3523.533366	791819.635703	41.000244
3523.415943	791483.242027	41.005248
3523.702711	791153.152333	41.010253
3523.494441	790803.722046	41.015258
3523.266329	790460.222985	41.020263
3523.536350	790121.587710	41.025268
3523.161184	789761.176084	41.030272
3523.334240	789419.427517	41.035277
3523.034824	789070.467295	41.040282
3523.138073	788711.200983	41.045287
3523.310991	788376.184375	41.050292
3522.951297	788024.627001	41.055296
3523.068598	787668.205556	41.060301
3523.014192	787322.117357	41.065306
3522.641644	786955.467625	41.070311
3522.609945	786611.504129	41.075316
3522.258552	786251.943022	41.080320
3522.401267	785903.983565	41.085325
3522.376837	785569.555952	41.090330
3522.461001	785210.509657	41.095335
3521.985815	784861.421495	41.100340
3521.930761	784511.755143	41.105344
3521.859235	784156.714111	41.110349
3521.366953	783816.577363	41.115354
3521.147069	783462.264186	41.120359
3521.109111	783134.315610	41.125364
3521.153407	782791.975938	41.130368
3521.507958	782455.717364	41.135373
3520.879402	782120.835329	41.140378
3520.794252	781778.616452	41.145383
3520.896687	781444.074128	41.150388
3520.537999	781107.329371	41.155392
3520.879176	780766.222011	41.160397
3520.400306	780439.699731	41.165402
3520.436700	780114.553719	41.170407
3519.963731	779781.702512	41.175412
3520.178539	779443.555348	41.180416
3520.206606	779127.765468	41.185421
3519.773849	778792.696885	41.190426
3519.627809	778472.625644	41.195431
3519.663078	778155.709540	41.200436
3519.263418	777829.204262	41.205440
3519.139199	777515.535179	41.210445
3518.969774	777198.611214	41.215450
3519.222894	776878.403887	41.220455
3518.871654	776565.617514	41.225460
3518.515660	776259.710886	41.230464
3518.715264	775950.794871	41.235469
3518.498608	775648.039765	41.240474
3518.298606	775336.357403	41.245479
3518.189323	775031.047908	41.250484
3517.954299	774743.079456	41.255488
3518.289887	774429.349571	41.260493
3517.747529	774137.419382	41.265498
3518.004079	773832.885949	41.270503
3517.755486	773544.281699	41.275508
3517.310506	773245.700525	41.280512
3517.327293	772956.142800	41.285517
3516.962322	772665.159102	41.290522
3517.070127	772371.081083	41.295527
3517.304772	772093.866278	41.300532
3516.936559	771810.730822	41.305536
3516.706641	771525.147758	41.310541
3516.319393	771242.486266	41.315546
3516.559042	770971.386569	41.320551
3516.222703	770682.684710	41.325556
3516.280357	770414.698594	41.330560
3516.438179	770153.436503	41.335565
3516.218450	769871.335446	41.340570
3516.328387	769603.705533	41.345575
3515.873059	769332.562104	41.350580
3515.798746	769064.943193	41.355584
3515.703647	768803.379641	41.360589
3515.691766	768539.328985	41.365594
3515.789552	768269.238105	41.370599
3514.932462	768021.129045	41.375604
3514.712103	767767.386241	41.380608
3515.148394	767509.780269	41.385613
3514.964035	767256.605587	41.390618
3515.012116	767008.017435	41.395623
3515.050396	766749.169333	41.400628
3514.837951	766502.677766	41.405632
3514.547642	766247.958168	41.410637
3514.262074	766001.708636	41.415642
3514.068262	765762.535199	41.420647
3514.107854	765515.722915	41.425652
3513.893997	765277.572642	41.430656
3514.027293	765038.469921	41.435661
3513.758881	764818.409321	41.440666
3513.575920	764575.843270	41.445671
3513.744271	764345.588268	41.450676
3513.276550	764122.926729	41.455680
3513.338721	763889.519313	41.460685
3512.764494	763662.571441	41.465690
3512.795245	763437.637350	41.470695
3513.019072	763230.616336	41.475700
3512.683643	763019.489908	41.480704
3512.877230	762789.478968	41.485709
3512.858329	762594.120238	41.490714
3512.305538	762369.595904	41.495719
3512.602172	762150.744855	41.500724
3512.631782	761946.778791	41.505728
3512.725758	761736.926596	41.510733
3511.945699	761518.580419	41.515738
3512.393822	761307.276548	41.520743
3512.181168	761104.166370	41.525748
3511.694366	760902.280026	41.530752
3511.992067	760699.419971	41.535757
3511.897718	760499.678075	41.540762
3511.820018	760285.472409	41.545767
3511.697820	760095.641201	41.550772
3511.414909	759902.131325	41.555776
3511.285863	759697.242683	41.560781
3511.024860	759528.587424	41.565786
3511.021871	759321.842155	41.570791
3510.884435	759140.427255	41.575796
3510.980314	758960.301799	41.580800
3510.947659	758778.614213	41.585805
3510.563367	758594.907770	41.590810
3510.683081	758405.734531	41.595815
3510.366378	758230.496187	41.600820
3510.469355	758051.680493	41.605824
3510.744705	757874.855579	41.610829
3510.407517	757700.003226	41.615834
3510.598057	757513.411865	41.620839
3510.500032	757335.550322	41.625844
3510.319677	757170.580501	41.630848
3509.980681	756994.231533	41.635853
3509.889738	756830.424182	41.640858
3509.757495	756655.168481	41.645863
3509.756668	756493.412153	41.650868
3509.730855	756329.731384	41.655872
3509.544589	756167.850718	41.660877
3509.199488	756005.647317	41.665882
3509.532497	755845.154957	41.670887
3509.555585	755692.164844	41.675892
3508.968798	755541.691475	41.680896
3509.237492	755378.534098	41.685901
3509.186035	755215.228671	41.690906
3509.192274	755066.573396	41.695911
3508.852125	754924.588300	41.700916
3508.801895	754762.359200	41.705920
3509.131638	754598.335794	41.710925
3508.688725	754467.270834	41.715930
3508.804281	754312.114779	41.720935
3509.005112	754165.039278	41.725940
3508.844253	754021.082142	41.730944
3508.977425	753862.062633	41.735949
3508.624761	753713.934252	41.740954
3508.755509	753569.673576	41.745959
3508.792115	753428.487400	41.750964
3508.501394	753297.377327	41.755968
3508.518900	753140.781750	41.760973
3508.124702	753001.782413	41.765978
3508.074343	752859.316179	41.770983
3508.421259	752721.769645	41.775988
3507.879458	752587.281337	41.780992
3508.190213	752463.762017	41.785997
3508.012998	752316.219782	41.791002
3507.783244	752180.783822	41.796007
3507.584020	752057.786779	41.801012
3507.837889	751927.847553	41.806016
3508.039926	751795.247547	41.811021
3507.480224	751670.278829	41.816026
3507.543668	751539.623650	41.821031
3507.168753	751428.154288	41.826036
3507.561004	751311.913421	41.831040
3507.791320	751165.813106	41.836045
3507.547906	751051.402222	41.841050
3507.146526	750924.271219	41.846055
3507.382158	750803.701624	41.851060
3506.852402	750678.366128	41.856064
3507.265061	750554.354866	41.861069
3506.686482	750440.385530	41.866074
3506.829502	750331.334201	41.871079
3506.887706	750212.859581	41.876084
3507.190395	750098.294968	41.881088
3506.783328	749988.588677	41.886093
3506.684321	749885.598287	41.891098
3506.901388	749781.417990	41.896103
3506.840166	749662.263029	41.901108
3506.440025	749559.021631	41.906112
3506.822482	749435.442131	41.911117
3506.519923	749333.367372	41.916122
3506.654592	749229.143876	41.921127
3506.547765	749118.436910	41.926132
3506.396828	749017.172893	41.931136
3506.604993	748904.632085	41.936141
3506.399363	748797.543827	41.941146
3506.314632	748682.380010	41.946151
3506.333272	748594.176556	41.951156
3505.861914	748487.325584	41.956160
3506.221079	748392.837543	41.961165
3505.699730	748285.102610	41.966170
3505.762863	748187.201995	41.971175
3506.121443	748096.861308	41.976180
3506.081817	748006.288881	41.981184
3506.250105	747911.777133	41.986189
3505.852284	747820.026316	41.991194
3505.931246	747711.838332	41.996199
3506.040580	747615.998458	42.001204
3505.697458	747523.543252	42.006208
3505.985703	747414.229337	42.011213
3505.465142	747336.281207	42.016218
3505.656102	747230.242528	42.021223
3505.431740	747142.408744	42.026228
3505.216300	747064.209789	42.031232
3505.807711	746976.189910	42.036237
3505.697099	746890.459664	42.041242
3505.237733	746793.814056	42.046247
3505.624302	746703.452620	42.051252
3505.131853	746623.021505	42.056256
3504.959407	746539.027486	42.061261
3505.264461	746451.197295	42.066266
3505.219857	746371.430973	42.071271
3505.306832	746297.079047	42.076276
3505.239526	746211.927323	42.081280
3505.486209	746126.129653	42.086285
3504.987528	746052.860742	42.091290
3505.236823	745954.950804	42.096295
3505.141139	745881.168830	42.101300
3505.051601	745802.639872	42.106304
3505.255577	745719.266869	42.111309
3505.028696	745638.188572	42.116314
3504.953971	745542.106534	42.121319
3505.025312	745480.354483	42.126324
3504.914341	745410.821754	42.131328
3505.144534	745326.204429	42.136333
3504.802810	745252.506624	42.141338
3504.619785	745179.325674	42.146343
3504.955506	745099.483550	42.151348
3504.543378	745024.855985	42.156352
3504.639981	744948.957196	42.161357
3504.372111	744877.814301	42.166362
3504.384142	744803.213408	42.171367
3504.313164	744730.800738	42.176372
3504.540488	744667.483976	42.181376
3504.628082	744601.322418	42.186381
3504.329078	744544.419639	42.191386
3504.313441	744460.871804	42.196391
3504.498841	744398.795766	42.201396
3504.347544	744346.019998	42.206400
3504.476706	744263.830437	42.211405
3504.595951	744207.103297	42.216410
3504.635235	744132.293770	42.221415
3504.290177	744068.869010	42.226420
3504.017606	743995.395175	42.231424
3504.165012	743928.278684	42.236429
3503.971004	743861.959672	42.241434
3504.037042	743805.633966	42.246439
3504.116833	743753.903771	42.251444
3503.829590	743691.900258	42.256448
3504.051475	743623.779998	42.261453
3503.914787	743566.151100	42.266458
3503.843508	743501.044865	42.271463
3504.097270	743450.816708	42.276468
3504.016573	743387.589992	42.281472
3503.813748	743325.174078	42.286477
3503.999251	743275.005526	42.291482
3504.131343	743214.461779	42.296487
3504.031629	743150.049589	42.301492
3503.670547	743098.190154	42.306496
3503.693628	743029.998720	42.311501
3503.697930	742987.324834	42.316506
3504.198151	742928.547623	42.321511
3504.230062	742873.061507	42.326516
3503.525793	742812.949573	42.331520
3504.099710	742749.461218	42.336525
3503.678951	742701.614414	42.341530
3503.762801	742642.755531	42.346535
3503.844485	742575.440581	42.351540
3503.511658	742527.726542	42.356544
3503.636922	742472.963943	42.361549
3503.461616	742417.113256	42.366554
3503.671552	742359.269900	42.371559
3503.714559	742305.558217	42.376564
3503.391764	742259.275002	42.381568
3503.721677	742206.158111	42.386573
3503.396786	742164.028697	42.391578
3503.157381	742112.043761	42.396583
3503.334584	742062.709580	42.401588
3503.407052	742030.552835	42.406592
3503.351075	741966.717200	42.411597
3503.496995	741923.371257	42.416602
3503.505548	741869.365577	42.421607
3503.382865	741815.628489	42.426612
3503.140525	741775.263738	42.431616
3503.407982	741716.021424	42.436621
3503.199393	741676.689160	42.441626
3503.234700	741624.210516	42.446631
3503.389800	741578.042161	42.451636
3503.376591	741542.336721	42.456640
3503.320280	741484.877164	42.461645
3503.425907	741443.562991	42.466650
3502.976234	741401.054467	42.471655
3503.363051	741344.213068	42.476660
3503.044637	741298.467535	42.481664
3503.509497	741260.654037	42.486669
3503.321642	741223.492265	42.491674
3503.028087	741174.972222	42.496679
3503.167437	741128.210338	42.501684
3502.828202	741097.057559	42.506688
3502.904986	741043.034964	42.511693
3502.868538	741011.238294	42.516698
3503.152742	740966.726682	42.521703
3503.052489	740926.284657	42.526708
3502.630763	740888.714813	42.531712
3502.950455	740841.624673	42.536717
3502.997487	740804.966193	42.541722
3502.839367	740769.380136	42.546727
3503.269818	740730.877339	42.551732
3502.971372	740683.245402	42.556736
3502.998235	740624.974467	42.561741
3502.641047	740603.418417	42.566746
3502.646542	740547.524647	42.571751
3502.796303	740526.725485	42.576756
3502.781103	740497.297468	42.581760
3502.667798	740452.502416	42.586765
3502.514700	740419.090350	42.591770
3502.620520	740401.612191	42.596775
3502.154387	740349.158497	42.601780
3502.014895	740331.325007	42.606784
3502.494344	740302.704885	42.611789
3502.506217	740273.667280	42.616794
3502.663726	740236.888989	42.621799
3502.625824	740190.991772	42.626804
3502.428119	740171.040540	42.631808
3502.593924	740134.408799	42.636813
3502.657336	740103.581297	42.641818
3502.463669	740065.771999	42.646823
3502.561433	740034.740689	42.651828
3502.606133	740005.202017	42.656832
3502.993896	739960.618185	42.661837
3502.649349	739930.995158	42.666842
3502.720331	739895.218919	42.671847
3502.780576	739862.016587	42.676852
3502.547604	739829.307777	42.681856
3502.929412	739786.900521	42.686861
3502.764833	739757.840720	42.691866
3502.335045	739712.599110	42.696871
3502.599980	739691.086176	42.701876
3502.522021	739661.863305	42.706880
3502.629017	739619.451100	42.711885
3502.400583	739590.302300	42.716890
3502.416968	739563.883205	42.721895
3502.708450	739525.298596	42.726900
3502.801316	739487.340256	42.731904
3502.752628	739458.111799	42.736909
3502.388866	739425.323998	42.741914
3502.401889	739396.827166	42.746919
3502.638472	739369.035344	42.751924
3502.065989	739334.253375	42.756928
3502.547529	739300.830671	42.761933
3502.075591	739271.523056	42.766938
3502.242647	739239.190949	42.771943
3502.735468	739209.872096	42.776948
3502.326373	739183.818875	42.781952
3502.186251	739144.116427	42.786957
3502.050947	739120.590281	42.791962
3502.115553	739098.713077	42.796967
3502.140681	739077.633889	42.801972
3502.157702	739049.926708	42.806977
3502.591465	739027.592528	42.811981
3502.185000	739008.316010	42.816986
3502.341693	738976.034019	42.821991
3502.522615	738944.539460	42.826996
3501.853899	738913.729381	42.832001
3502.168863	738900.863833	42.837005
3502.167939	738869.695867	42.842010
3502.035476	738849.037903	42.847015
3502.019581	738828.162727	42.852020
3502.123795	738806.921334	42.857025
3502.250935	738763.660185	42.862029
3502.057276	738758.447978	42.867034
3502.083916	738725.295929	42.872039
3501.945033	738708.497652	42.877044
3502.229190	738678.073417	42.882049
3502.422169	738656.025360	42.887053
3502.242404	738627.805006	42.892058
3502.027149	738603.795795	42.897063
3501.952293	738565.959727	42.902068
3502.157656	738551.231668	42.907073
3502.250630	738533.652578	42.912077
3502.309632	738514.396894	42.917082
3502.160164	738477.116965	42.922087
3502.328285	738457.843112	42.927092
3502.018724	738426.081225	42.932097
3501.909931	738399.233664	42.937101
3501.821199	738371.986886	42.942106
3501.608798	738352.132465	42.947111
3501.913869	738343.819499	42.952116
3501.878588	738321.016610	42.957121
3502.174177	738291.529070	42.962125
3502.143860	738281.094476	42.967130
3502.130900	738260.662622	42.972135
3502.306768	738230.304051	42.977140
3502.045504	738209.814144	42.982145
3501.931122	738183.609988	42.987149
3501.735445	738155.044244	42.992154
3502.166261	738145.324915	42.997159
3502.148618	738112.425025	43.002164
3501.885819	738095.893322	43.007169
3502.144634	738064.085546	43.012173
3501.953958	738044.573116	43.017178
3502.120435	738026.485977	43.022183
3502.116116	738000.460945	43.027188
3502.025989	737987.067123	43.032193
3501.988711	737959.464081	43.037197
3501.827674	737942.321495	43.042202
3501.802492	737910.411599	43.047207
3501.882946	737903.322798	43.052212
3501.881703	737887.638070	43.057217
3501.927548	737852.450560	43.062221
3501.662841	737846.309380	43.067226
3501.857219	737821.487923	43.072231
3502.173134	737789.570658	43.077236
3501.844858	737783.885255	43.082241
3501.939784	737751.608516	43.087245
3502.085500	737735.305440	43.092250
3501.756168	737715.567715	43.097255
3502.040005	737693.452506	43.102260
3501.784350	737675.879656	43.107265
3501.728068	737659.461363	43.112269
3502.004239	737646.352805	43.117274
3501.809291	737621.248694	43.122279
3502.099126	737601.457851	43.127284
3501.658431	737589.704692	43.132289
3501.534322	737555.088250	43.137293
3501.555294	737550.087189	43.142298
3501.831636	737528.566541	43.147303
3501.828676	737502.440698	43.152308
3501.661329	737495.837821	43.157313
3501.914758	737483.277055	43.162317
3501.837388	737463.596033	43.167322
3501.888790	737447.703813	43.172327
3501.871471	737419.204924	43.177332
3501.733688	737406.609720	43.182337
3502.305762	737379.151389	43.187341
3501.920404	737362.786865	43.192346
3501.722052	737343.818298	43.197351
3501.905051	737323.846492	43.202356
3501.580215	737297.624719	43.207361
3501.913678	737287.376126	43.212365
3501.820362	737274.575433	43.217370
3501.892550	737252.296046	43.222375
3502.087866	737241.377456	43.227380
3501.599092	737218.349454	43.232385
3501.625975	737206.023624	43.237389
3501.529732	737191.788254	43.242394
3501.761214	737185.416116	43.247399
3501.888550	737152.290376	43.252404
3501.748766	737145.336266	43.257409
3501.922206	737117.349103	43.262413
3501.783765	737099.557677	43.267418
3501.529977	737086.981138	43.272423
3501.857789	737061.491975	43.277428
3501.451786	737061.410652	43.282433
3502.009133	737033.112332	43.287437
3501.495476	737011.918781	43.292442
3501.577206	736995.723741	43.297447
3501.960343	736988.138747	43.302452
3501.643558	736971.564147	43.307457
3502.051941	736952.791300	43.312461
3501.833005	736942.188183	43.317466
3502.106109	736906.662043	43.322471
3501.900847	736897.838086	43.327476
3501.791937	736879.645405	43.332481
3502.067754	736856.638468	43.337485
3501.924793	736838.847208	43.342490
3502.107293	736822.239278	43.347495
3501.946134	736794.850626	43.352500
3501.531268	736764.831540	43.357505
3501.963907	736757.238148	43.362509
3501.855825	736733.551999	43.367514
3501.701150	736716.554188	43.372519
3501.693885	736697.601996	43.377524
3501.674898	736704.236405	43.382529
3501.868589	736659.913641	43.387533
3501.654675	736655.396219	43.392538
3501.874280	736637.346648	43.397543
3501.783779	736604.304125	43.402548
3501.853252	736596.572646	43.407553
3501.750289	736585.999378	43.412557
3501.987975	736566.313572	43.417562
3501.739490	736548.638079	43.422567
3501.979291	736521.182232	43.427572
3501.540344	736506.457905	43.432577
3501.725571	736494.847134	43.437581
3501.681389	736474.118942	43.442586
3501.637602	736460.615924	43.447591
3501.913853	736439.884181	43.452596
3501.592045	736426.031141	43.457601
3502.031518	736396.017956	43.462605
3501.772042	736402.494401	43.467610
3501.596912	736377.036684	43.472615
3501.697649	736359.105108	43.477620
3501.621209	736355.950488	43.482625
3501.955891	736334.070569	43.487629
3501.535519	736319.243850	43.492634
3501.453605	736305.796361	43.497639
3501.545151	736283.857505	43.502644
3501.643741	736273.745412	43.507649
3501.844484	736256.885849	43.512653
3501.564272	736255.002101	43.517658
3501.666779	736223.955185	43.522663
3501.649336	736214.555048	43.527668
3501.537425	736215.909806	43.532673
3501.524688	736186.663422	43.537677
3501.616319	736170.465078	43.542682
3501.647397	736156.998668	43.547687
3501.467481	736147.922242	43.552692
3501.163074	736123.029473	43.557697
3501.519899	736105.747877	43.562701
3501.312003	736109.395076	43.567706
3501.429810	736117.442590	43.572711
3501.791130	736099.219920	43.577716
3501.453954	736082.894297	43.582721
3501.796321	736053.935183	43.587725
3501.572953	736052.982317	43.592730
3501.307803	736026.647527	43.597735
3501.743968	736002.621824	43.602740
3501.498288	735996.674034	43.607745
3501.704606	735986.692251	43.612749
3501.620725	735971.660807	43.617754
3501.617922	735953.448486	43.622759
3502.213405	735935.186749	43.627764
3501.777764	735927.191653	43.632769
3501.977600	735905.184375	43.637773
3501.946287	735888.758321	43.642778
3501.733652	735873.500510	43.647783
3501.629613	735857.383360	43.652788
3501.605083	735831.008164	43.657793
3501.803906	735816.078188	43.662797
3501.440070	735804.606643	43.667802
3501.391926	735781.402696	43.672807
3501.415247	735759.473679	43.677812
3501.148755	735755.063419	43.682817
3501.579764	735750.587388	43.687821
3501.708044	735754.179195	43.692826
3501.614445	735724.202097	43.697831
3501.644970	735715.486347	43.702836
3501.597076	735707.228984	43.707841
3501.678727	735682.023583	43.712845
3501.936752	735681.733519	43.717850
3501.857005	735662.394910	43.722855
3501.654797	735637.533235	43.727860
3501.269375	735630.073969	43.732865
3501.620489	735616.553766	43.737869
3501.506797	735613.108047	43.742874
3501.346802	735580.369745	43.747879
3501.628136	735568.890235	43.752884
3501.214614	735581.183568	43.757889
3501.357214	735569.924960	43.762893
3501.712225	735558.977693	43.767898
3501.525160	735535.301051	43.772903
3501.655670	735517.907110	43.777908
3501.164988	735519.621540	43.782913
3501.452330	735511.754024	43.787917
3501.549473	735495.355431	43.792922
3501.216899	735476.949051	43.797927
3501.651479	735464.454181	43.802932
3501.564189	735464.369657	43.807937
3501.343761	735438.421497	43.812941
3501.311345	735424.320920	43.817946
3501.501708	735426.120805	43.822951
3501.858176	735418.835713	43.827956
3501.329855	735404.866543	43.832961
3501.436195	735382.031871	43.837965
3501.360136	735376.995992	43.842970
3501.491654	735377.964199	43.847975
3501.657157	735358.089379	43.852980
3501.519032	735340.145503	43.857985
3501.410585	735319.622926	43.862989
3501.180891	735309.019418	43.867994
3501.449197	735316.300437	43.872999
3501.488784	735289.615894	43.878004
3501.490735	735277.241721	43.883009
3501.736306	735274.627410	43.888013
3501.515737	735268.130474	43.893018
3501.498311	735245.662336	43.898023
3501.609057	735230.498349	43.903028
3501.304815	735227.529415	43.908033
3501.680201	735221.577408	43.913037
3501.650442	735199.210169	43.918042
3501.528075	735180.867364	43.923047
3501.419039	735166.778995	43.928052
3501.516302	735174.979341	43.933057
3501.766967	735140.191532	43.938061
3501.637133	735131.204669	43.943066
3501.385214	735119.713646	43.948071
3501.308784	735108.391594	43.953076
3501.364117	735096.651779	43.958081
3501.316994	735087.552206	43.963085
3501.234054	735077.617095	43.968090
3501.269314	735079.987156	43.973095
3501.609933	735072.258899	43.978100
3501.651040	735050.770480	43.983105
3501.302964	735033.355582	43.988109
3501.627378	735024.095547	43.993114
3501.424235	735018.585472	43.998119
3501.731454	734976.363028	44.003124
3501.350380	734977.316993	44.008129
3501.440156	734974.035366	44.013133
3501.428029	734970.275601	44.018138
3501.720319	734954.586119	44.023143
3501.707921	734933.304218	44.028148
3501.368906	734944.546756	44.033153
3501.586147	734930.404055	44.038157
3501.786507	734907.601996	44.043162
3501.561336	734899.274100	44.048167
3501.766347	734891.271092	44.053172
3501.705392	734866.284689	44.058177
3501.482790	734848.848655	44.063181
3501.759321	734850.188949	44.068186
3501.349123	734822.884207	44.073191
3501.733787	734808.416636	44.078196
3501.403362	734793.275229	44.083201
3501.574322	734800.671801	44.088205
3501.896070	734776.215859	44.093210
3501.309188	734744.683160	44.098215
3501.615865	734738.494658	44.103220
3501.650262	734742.498425	44.108225
3501.472765	734720.302764	44.113229
3501.750279	734707.436686	44.118234
3501.397644	734700.515622	44.123239
3501.529658	734680.842660	44.128244
3501.524836	734666.340198	44.133249
3501.472500	734659.270474	44.138253
3501.742819	734652.741420	44.143258
3501.627516	734639.346153	44.148263
3501.406779	734611.910386	44.153268
3501.433015	734617.846052	44.158273
3501.614116	734600.095268	44.163277
3501.279322	734570.054717	44.168282
3501.148103	734569.036942	44.173287
3501.439735	734557.603791	44.178292
3501.332848	734552.324989	44.183297
3501.691836	734547.414699	44.188301
3501.819628	734529.573569	44.193306
3501.582737	734521.395717	44.198311
3501.730603	734498.898177	44.203316
3501.404220	734485.785037	44.208321
3501.232410	734464.429236	44.213325
3501.237836	734459.181314	44.218330
3501.467770	734463.301410	44.223335
3501.494462	734444.090779	44.228340
3501.322987	734440.159096	44.233345
3501.416730	734421.085833	44.238349
3501.187377	734405.728989	44.243354
3501.294075	734404.523373	44.248359
3501.130195	734407.669055	44.253364
3501.425331	734414.401951	44.258369
3501.712587	734383.515396	44.263373
3501.892877	734367.645276	44.268378
3501.324472	734362.244609	44.273383
3501.596429	734344.428747	44.278388
3501.689026	734334.265705	44.283393
3501.593928	734316.015421	44.288397
3501.587092	734311.412948	44.293402
3501.545009	734284.243550	44.298407
3501.511667	734270.240103	44.303412
3501.333389	734262.596821	44.308417
3501.501608	734255.886311	44.313421
3501.386388	734244.321942	44.318426
3501.207760	734215.689816	44.323431
3501.610324	734207.356473	44.328436
3501.442675	734220.452782	44.333441
3501.740694	734206.839987	44.338445
3501.163106	734192.530323	44.343450
3501.377941	734162.793443	44.348455
3501.714386	734160.411270	44.353460
3501.437897	734165.605254	44.358465
3501.443270	734146.743954	44.363469
3501.600717	734133.203767	44.368474
3501.391539	734130.317717	44.373479
3501.624719	734130.823753	44.378484
3501.099264	734108.931416	44.383489
3501.409429	734088.980056	44.388493
3501.408250	734082.000377	44.393498
3501.263745	734072.420718	44.398503
3501.228858	734063.367466	44.403508
3501.083155	734081.361177	44.408513
3501.587425	734054.892767	44.413517
3501.837841	734027.327644	44.418522
3501.619737	734022.314388	44.423527
3501.752460	733994.719099	44.428532
3501.357777	733989.883513	44.433537
3501.570829	733986.977142	44.438541
3501.278398	733975.243655	44.443546
3501.322590	733974.840363	44.448551
3501.369380	733948.001668	44.453556
3501.105821	733941.758279	44.458561
3501.600696	733933.112377	44.463565
3501.417639	733943.142441	44.468570
3501.350753	733926.817261	44.473575
3501.396528	733903.146834	44.478580
3501.238585	733886.539595	44.483585
3501.274740	733887.226718	44.488589
3501.352712	733883.897095	44.493594
3501.300029	733888.113694	44.498599
3501.180417	733883.529612	44.503604
3501.257720	733858.715249	44.508609
3501.248243	733849.311027	44.513613
3501.325649	733830.536093	44.518618
3501.093385	733836.218025	44.523623
3501.340307	733836.771315	44.528628
3501.067035	733836.767008	44.533633
3501.634824	733807.960583	44.538637
3501.359087	733798.649806	44.543642
3501.338337	733791.326576	44.548647
3501.313507	733777.469380	44.553652
3501.014670	733786.528675	44.558657
3501.183744	733779.174067	44.563661
3501.497917	733776.300415	44.568666
3501.621324	733760.537510	44.573671
3501.574786	733744.357112	44.578676
3501.363858	733747.708844	44.583681
3501.356320	733717.759544	44.588685
3501.352112	733693.849236	44.593690
3501.244245	733686.144265	44.598695
3501.491867	733679.766693	44.603700
3501.389898	733693.447069	44.608705
3501.508765	733673.476789	44.613709
3501.194295	733659.271209	44.618714
3501.234253	733640.502020	44.623719
3500.900194	733639.022587	44.628724
3500.783847	733636.665580	44.633729
3500.902903	733630.754767	44.638733
3501.151024	733645.466497	44.643738
3500.898418	733642.191402	44.648743
3501.273255	733630.545168	44.653748
3501.386739	733627.209571	44.658753
3501.243119	733614.658874	44.663757
3501.290467	733594.799229	44.668762
3501.477414	733599.817981	44.673767
3501.634062	733579.989745	44.678772
3501.469345	733585.710196	44.683777
3501.495119	733571.151199	44.688781
3501.518526	733551.047872	44.693786
3501.054495	733548.253232	44.698791
3501.496976	733551.497069	44.703796
3501.017535	733552.813991	44.708801
3501.225520	733544.215084	44.713805
3501.262040	733516.634056	44.718810
3501.681386	733507.653638	44.723815
3501.450447	733498.285603	44.728820
3501.413061	733504.430629	44.733825
3501.573049	733474.650769	44.738829
3501.406049	733452.202340	44.743834
3501.216858	733451.639561	44.748839
3501.558021	733445.691910	44.753844
3501.247962	733449.258173	44.758849
3501.262095	733424.947982	44.763853
3501.629533	733411.470898	44.768858
3501.387130	733410.669374	44.773863
3501.584246	733395.388647	44.778868
3501.320338	733405.977318	44.783873
3501.238480	733379.405525	44.788877
3501.123842	733367.938814	44.793882
3500.917574	733377.923908	44.798887
3501.218614	733359.407966	44.803892
3501.346493	733368.496228	44.808897
3501.184697	733369.463644	44.813901
3500.939160	733362.325692	44.818906
3501.165069	733375.803903	44.823911
3501.111998	733335.612692	44.828916
3500.908766	733325.348741	44.833921
3501.164662	733320.454748	44.838925
3501.420430	733308.580190	44.843930
3501.320702	733319.191351	44.848935
3501.338172	733311.019740	44.853940
3501.079478	733310.121882	44.858945
3501.211306	733303.119550	44.863949
3501.319917	733285.971947	44.868954
3501.238025	733274.450184	44.873959
3501.480831	733270.152418	44.878964
3501.268023	733261.028650	44.883969
3501.370058	733254.823327	44.888973
3501.700694	733254.719222	44.893978
3501.023553	733231.809890	44.898983
3501.255924	733217.562672	44.903988
3501.198770	733219.750520	44.908993
3500.983430	733206.963498	44.913997
3501.106623	733214.022868	44.919002
3501.055641	733214.031332	44.924007
3501.117281	733202.188697	44.929012
3501.077130	733217.740981	44.934017
3501.545269	733196.127539	44.939021
3501.609911	733169.629863	44.944026
3501.194030	733167.569759	44.949031
3501.371491	733155.658408	44.954036
3501.397576	733161.496155	44.959041
3501.326466	733144.724511	44.964045
3501.451480	733127.177790	44.969050
3501.315337	733117.645121	44.974055
3501.630535	733108.978526	44.979060
3501.361046	733094.764514	44.984065
3501.447722	733075.639729	44.989069
3501.321197	733085.116915	44.994074
3501.054912	733079.417904	44.999079
3501.358670	733066.891443	45.004084
3501.227728	733072.953239	45.009089
3501.101593	733056.735105	45.014093
3501.021238	733037.340775	45.019098
3501.061064	733029.858316	45.024103
3501.297210	733021.303709	45.029108
3501.147869	733028.507296	45.034113
3501.021000	733019.270034	45.039117
3501.107406	733014.898960	45.044122
3501.247986	733026.262947	45.049127
3501.221314	733009.978774	45.054132
3501.429204	733009.350346	45.059137
3501.359858	732989.904573	45.064141
3501.278265	732974.669107	45.069146
3501.265599	732979.226135	45.074151
3501.343438	732964.360382	45.079156
3501.133313	732976.277491	45.084161
3501.266547	732948.232951	45.089165
3501.348901	732936.634054	45.094170
3501.024752	732928.617528	45.099175
3501.197707	732916.359999	45.104180
3501.233798	732921.057534	45.109185
3501.237377	732916.650584	45.114189
3501.310974	732926.144397	45.119194
3500.851400	732917.902688	45.124199
3501.417341	732882.112346	45.129204
3501.352625	732877.172047	45.134209
3501.277146	732877.778684	45.139213
3501.268436	732870.799201	45.144218
3500.805276	732880.381766	45.149223
3501.208419	732876.057298	45.154228
3500.765450	732877.219765	45.159233
3500.712487	732875.990798	45.164237
3501.155621	732872.699437	45.169242
3501.038501	732882.274327	45.174247
3500.759615	732868.606083	45.179252
3500.777809	732869.444793	45.184257
3500.736350	732873.610556	45.189261
3501.108330	732870.528993	45.194266
3501.093654	732876.175641	45.199271
3501.207414	732857.095372	45.204276
3500.925905	732844.467241	45.209281
3500.909362	732837.290981	45.214285
3501.283520	732821.781872	45.219290
3500.911967	732834.072441	45.224295
3501.002243	732823.511795	45.229300
3501.102277	732821.316834	45.234305
3501.191660	732824.173723	45.239309
3501.384851	732822.012879	45.244314
3501.208895	732824.220465	45.249319
3501.174638	732799.866878	45.254324
3501.026452	732793.256952	45.259329
3501.038523	732788.699996	45.264333
3501.134096	732785.763100	45.269338
3501.132893	732773.930222	45.274343
3501.490503	732768.821046	45.279348
3500.780410	732777.256273	45.284353
3500.948941	732779.852544	45.289357
3501.184907	732769.614329	45.294362
3501.000211	732777.566647	45.299367
3501.003825	732771.476239	45.304372
3501.069578	732766.118224	45.309377
3501.225589	732754.754450	45.314381
3500.961577	732738.112859	45.319386
3500.912368	732734.457201	45.324391
3501.252617	732724.350230	45.329396
3500.964286	732734.448701	45.334401
3501.088666	732727.645147	45.339405
3501.229174	732721.185501	45.344410
3500.891732	732732.331827	45.349415
3501.223442	732714.948100	45.354420
3501.095461	732716.850720	45.359425
3501.542154	732719.252510	45.364429
3501.380687	732687.443393	45.369434
3501.128123	732696.496259	45.374439
3501.439842	732689.513180	45.379444
3501.097632	732687.341752	45.384449
3501.325708	732685.472176	45.389453
3501.234205	732659.493745	45.394458
3501.027061	732648.635438	45.399463
3501.113403	732634.906443	45.404468
3500.983174	732644.780852	45.409473
3501.130186	732645.746834	45.414477
3501.428252	732635.646723	45.419482
3500.845253	732632.475322	45.424487
3501.110797	732634.808049	45.429492
3501.034773	732633.632367	45.434497
3501.070797	732621.149460	45.439501
3501.395863	732629.809876	45.444506
3500.935689	732617.260424	45.449511
3500.848910	732603.361936	45.454516
3501.347024	732603.824295	45.459521
3501.217955	732604.439808	45.464525
3501.089036	732601.242869	45.469530
3500.859482	732596.626710	45.474535
3501.318767	732590.708427	45.479540
3501.157207	732609.252670	45.484545
3501.057639	732590.603121	45.489549
3500.948774	732601.365270	45.494554
3501.177585	732583.057536	45.499559
3501.078230	732556.584950	45.504564
3501.020746	732570.358900	45.509569
3500.809607	732562.620407	45.514573
3501.354869	732547.726158	45.519578
3500.859995	732556.126049	45.524583
3501.334831	732548.818821	45.529588
3501.656108	732561.589461	45.534593
3501.528782	732556.956385	45.539597
3501.340482	732531.241099	45.544602
3501.139784	732515.182736	45.549607
3501.331479	732514.309384	45.554612
3501.129191	732519.244595	45.559617
3501.110105	732503.205709	45.564621
3500.986595	732503.226159	45.569626
3500.857663	732517.655670	45.574631
3501.010819	732509.312288	45.579636
3500.859315	732519.140853	45.584641
3500.898197	732488.634683	45.589645
3501.034489	732465.737287	45.594650
3501.072938	732480.881898	45.599655
3501.056974	732462.069698	45.604660
3501.117665	732457.207444	45.609665
3500.745358	732464.448377	45.614669
3500.901400	732462.491629	45.619674
3500.843359	732459.827563	45.624679
3501.008891	732465.989360	45.629684
3501.065034	732463.454965	45.634689
3500.808961	732472.607686	45.639693
3501.118998	732464.584924	45.644698
3500.720940	732469.106900	45.649703
3501.360313	732457.365756	45.654708
3501.084094	732466.719864	45.659713
3500.981873	732460.894276	45.664717
3501.182935	732463.435761	45.669722
3500.965883	732463.026052	45.674727
3501.171890	732438.186055	45.679732
3501.455504	732424.226052	45.684737
3501.221481	732419.858095	45.689741
3501.186079	732429.519043	45.694746
3501.018167	732425.734321	45.699751
3501.076934	732416.614231	45.704756
3501.098003	732435.920903	45.709761
3500.819451	732426.311922	45.714765
3501.148406	732432.991383	45.719770
3501.133523	732432.102647	45.724775
3500.993355	732393.456044	45.729780
3501.340811	732387.754148	45.734785
3501.272972	732377.763696	45.739789
3501.505306	732376.289453	45.744794
3501.368625	732373.440301	45.749799
3501.416940	732367.441229	45.754804
3501.307987	732358.447816	45.759809
3501.261269	732346.126698	45.764813
3501.706357	732318.028440	45.769818
3501.161741	732252.462947	45.774823
3501.348948	732130.576747	45.779828
3501.036466	731964.355611	45.784833
3501.076863	731715.379007	45.789837
3500.733782	731439.668307	45.794842
3500.496718	731098.860070	45.799847
3500.492321	730694.410886	45.804852
3500.138942	730241.612019	45.809857
3500.097231	729729.697379	45.814861
3499.428332	729143.951073	45.819866
3499.187152	728527.032401	45.824871
3498.856928	727850.385132	45.829876
3498.537218	727118.684877	45.834881
3497.826234	726325.789609	45.839885
3497.754205	725467.596583	45.844890
3497.183763	724565.782934	45.849895
3497.256653	723603.441919	45.854900
3496.543164	722577.021403	45.859905
3495.714249	721498.583424	45.864909
3495.407999	720338.994787	45.869914
3494.442028	719130.157216	45.874919
3494.063242	717870.206903	45.879924
3493.198960	716545.805135	45.884929
3492.784382	715164.061179	45.889933
3491.832996	713706.947818	45.894938
3490.776493	712208.305387	45.899943
3490.127187	710654.773506	45.904948
3489.246489	709031.632364	45.909953
3488.069161	707361.450696	45.914957
3487.360497	705620.829344	45.919962
3486.248338	703822.639826	45.924967
3485.684614	701974.939725	45.929972
3484.831893	700065.063899	45.934977
3483.426485	698100.723060	45.939981
3482.737270	696071.628401	45.944986
3481.217224	693999.430686	45.949991
3480.375881	691842.659698	45.954996
3479.194179	689652.034062	45.960001
3478.003145	687396.716556	45.965005
3476.764733	685095.239095	45.970010
3475.800106	682731.680584	45.975015
3474.486518	680318.005086	45.980020
3473.037457	677839.443023	45.985025
3471.928037	675307.231771	45.990029
3470.582019	672730.700456	45.995034
3469.199845	670105.046929	46.000039
3467.943953	667405.467120	46.005044
3466.224446	664672.467332	46.010049
3464.667918	661878.071065	46.015053
3463.504170	659012.058449	46.020058
3461.682912	656118.993587	46.025063
3459.809132	653161.892514	46.030068
3458.384935	650177.950042	46.035073
3456.784550	647124.565686	46.040077
3455.692254	644019.371459	46.045082
3453.211436	640883.248504	46.050087
3451.897721	637677.380335	46.055092
3449.788267	634426.108677	46.060097
3448.124180	631129.896397	46.065101
3446.571066	627789.317562	46.070106
3444.478025	624394.629847	46.075111
3442.724867	620952.362191	46.080116
3440.433367	617460.971700	46.085121
3438.099211	613934.832505	46.090125
3436.717938	610359.263213	46.095130
3434.799665	606750.983036	46.100135
3432.753504	603063.429243	46.105140
3430.724357	599358.069063	46.110145
3428.565525	595591.329988	46.115149
3426.494195	591769.712900	46.120154
3424.202581	587923.183307	46.125159
3422.320324	584030.916786	46.130164
3419.669199	580096.499853	46.135169
3417.692416	576127.416811	46.140173
3415.384319	572086.530716	46.145178
3413.182544	568037.997413	46.150183
3410.818681	563931.822228	46.155188
3408.807534	559792.866486	46.160193
3406.204720	555608.275540	46.165197
3404.297481	551358.661497	46.170202
3401.641867	547091.965765	46.175207
3399.195875	542776.414740	46.180212
3396.373797	538430.040305	46.185217
3393.906011	534039.998915	46.190221
3391.739593	529600.628570	46.195226
3389.002846	525138.206653	46.200231
3386.432886	520630.593031	46.205236
3383.847072	516092.857319	46.210241
3381.361576	511516.841989	46.215245
3379.006996	506905.667923	46.220250
3375.842700	502255.794705	46.225255
3373.486311	497560.423286	46.230260
3370.701300	492843.525758	46.235265
3367.719478	488096.267428	46.240269
3365.348577	483298.927231	46.245274
3362.037112	478480.662059	46.250279
3359.509139	473622.813832	46.255284
3356.827820	468734.857566	46.260289
3353.832199	463803.854156	46.265293
3351.377277	458840.507100	46.270298
3348.135525	453856.602352	46.275303
3345.069677	448832.067908	46.280308
3342.143516	443793.440862	46.285313
3338.657470	438721.732738	46.290317
3336.070704	433617.169349	46.295322
3332.530337	428491.590501	46.300327
3329.512265	423346.143087	46.305332
3326.380188	418160.922204	46.310337
3323.354873	412964.774744	46.315341
3320.588790	407733.956132	46.320346
3316.749296	402486.256320	46.325351
3313.901224	397203.142576	46.330356
3310.659090	391901.151122	46.335361
3307.328254	386578.225212	46.340365
3304.291272	381235.980825	46.345370
3300.825015	375869.252025	46.350375
3297.234884	370472.624058	46.355380
3294.151174	365073.409424	46.360385
3290.633055	359635.122151	46.365389
3287.343436	354187.364492	46.370394
3283.905713	348738.631140	46.375399
3280.434932	343247.669248	46.380404
3276.967310	337755.725810	46.385409
3273.397613	332230.840823	46.390413
3270.077398	326692.128741	46.395418
3266.212351	321143.322559	46.400423
3263.089950	315580.964529	46.405428
3259.034989	310015.223663	46.410433
3255.576223	304428.676524	46.415437
3251.882285	298827.992325	46.420442
3247.997405	293231.385968	46.425447
3243.948918	287609.509099	46.430452
3240.543859	281991.529527	46.435457
3236.717057	276364.984487	46.440461
3233.059822	270740.260827	46.445466
3228.949032	265104.210844	46.450471
3225.566941	259454.874104	46.455476
3221.364344	253800.853308	46.460481
3217.575205	248149.043225	46.465485
3213.935202	242489.166366	46.470490
3209.390120	236829.412950	46.475495
3205.809170	231170.180290	46.480500
3202.086131	225506.297043	46.485505
3197.829175	219850.706698	46.490509
3193.529618	214179.080190	46.495514
3189.587894	208507.667967	46.500519
3185.644474	202778.846834	46.505524
3181.588873	197127.855044	46.510529
3177.444972	191486.191170	46.515533
3173.030268	185840.730258	46.520538
3168.585744	180211.404428	46.525543
3164.677863	174582.369407	46.530548
3160.593110	168966.915690	46.535553
3155.815397	163371.094936	46.540557
3151.610762	157761.882202	46.545562
3147.223505	152174.052970	46.550567
3143.110063	146611.507309	46.555572
3138.794435	141055.171941	46.560577
3134.326759	135516.161770	46.565581
3129.814381	129982.394404	46.570586
3125.013346	124476.655408	46.575591
3120.621186	118974.515699	46.580596
3115.766879	113513.564178	46.585601
3111.084990	108072.010766	46.590605
3106.508122	102632.926959	46.595610
3100.982910	97247.407720	46.600615
3096.427272	91864.118104	46.605620
3091.671616	86538.633979	46.610625
3086.756385	81223.017813	46.615629
3081.942344	75946.990708	46.620634
3076.281659	70713.267308	46.625639
3071.587989	65492.151909	46.630644
3066.745539	60326.734036	46.635649
3061.168043	55195.521587	46.640653
3056.096208	50096.243667	46.645658
3050.745314	45059.122904	46.650663
3044.989426	40047.191861	46.655668
3039.251801	35097.158466	46.660673
3032.531148	30200.951462	46.665677
3025.679898	25379.935227	46.670682
3015.540075	20717.595271	46.675687
2999.380976	16334.906710	46.680692
2982.900182	12129.955373	46.685697
2960.698426	8310.844248	46.690701
2929.222215	5037.137070	46.695706
2897.427861	2219.370150	46.700711
2850.448984	364.256049	46.705716
2765.356392	254.124282	46.710721
2717.004540	262.492546	46.715725
2709.638280	254.875916	46.720730
2727.815070	247.924768	46.725735
2755.470122	235.784093	46.730740
2780.358742	229.137933	46.735745
2795.703400	239.349027	46.740749
2802.213119	232.552005	46.745754
2801.235598	235.413809	46.750759
2797.375713	231.843679	46.755764
2792.441108	220.332171	46.760769
2787.165527	231.630535	46.765773
2783.101493	217.496389	46.770778
2779.363705	223.753414	46.775783
2777.237025	223.421676	46.780788
2775.477819	210.881017	46.785793
2772.556205	221.106393	46.790797
2770.349259	209.576213	46.795802
2767.219694	218.758943	46.800807
2763.835085	214.133362	46.805812
2760.782833	219.254329	46.810817
2757.939563	215.851841	46.815821
2755.131899	204.979372	46.820826
2751.870890	215.986148	46.825831
2748.740964	217.024635	46.830836
2745.177385	215.247067	46.835841
2741.646585	212.340438	46.840845
2738.927521	207.629384	46.845850
2735.529755	216.581635	46.850855
2732.563961	203.972149	46.855860
2729.211393	210.215964	46.860865
2725.658300	208.659077	46.865869
2722.063865	215.502189	46.870874
2718.852214	208.546669	46.875879
2715.705851	205.114659	46.880884
2712.737092	205.003448	46.885889
2709.203574	201.629016	46.890893
2705.732724	200.172397	46.895898
2702.460690	214.192395	46.900903
2699.094705	218.416932	46.905908
2695.923568	199.254942	46.910913
2692.321464	209.021314	46.915917
2688.862913	193.692041	46.920922
2685.172927	202.814449	46.925927
2682.192823	200.785047	46.930932
2678.779825	196.308890	46.935937
2674.991279	202.850666	46.940941
2671.973731	199.504126	46.945946
2668.711961	201.369433	46.950951
2665.195384	206.855042	46.955956
2661.831303	196.735248	46.960961
2658.199722	200.500568	46.965965
2655.026837	191.269119	46.970970
2651.299857	202.073857	46.975975
2647.888183	198.546303	46.980980
2644.407612	195.560996	46.985985
2640.786907	195.419625	46.990989
2637.257424	192.513463	46.995994
2633.646630	196.181232	47.000999
2630.093888	194.236997	47.006004
2627.428609	183.730021	47.011009
2623.776738	190.268152	47.016013
2620.265957	185.006654	47.021018
2617.196803	192.790804	47.026023
2614.074440	184.629475	47.031028
2610.192078	191.142232	47.036033
2606.534164	192.127530	47.041037
2602.680260	190.802889	47.046042
2599.106864	187.616116	47.051047
2596.079800	187.344534	47.056052
2593.161888	186.051821	47.061057
2588.938722	191.573161	47.066061
2586.270424	183.454886	47.071066
2582.364412	185.805803	47.076071
2579.234808	184.398763	47.081076
2575.395896	182.734023	47.086081
2571.434085	185.410518	47.091085
2567.648141	186.514530	47.096090
2564.823489	185.062143	47.101095
2561.544283	183.718958	47.106100
2558.139756	183.488981	47.111105
2554.377399	187.938297	47.116109
2551.315960	180.808872	47.121114
2547.570180	185.026341	47.126119
2544.231231	183.153937	47.131124
2540.958072	180.801181	47.136129
2537.394341	187.814179	47.141133
2533.851048	176.017817	47.146138
2530.102384	193.668481	47.151143
2527.074080	186.004725	47.156148
2523.289185	183.884516	47.161153
2519.521872	188.734091	47.166157
2516.287022	178.905229	47.171162
2512.733307	176.065154	47.176167
2509.214866	178.610868	47.181172
2506.241926	179.549139	47.186177
2502.149011	182.682531	47.191181
2499.047462	173.278386	47.196186
2495.367115	173.808882	47.201191
2491.635869	176.306373	47.206196
2488.124027	167.838260	47.211201
2484.667644	175.653649	47.216205
2481.548572	176.457870	47.221210
2478.297892	180.047977	47.226215
2474.631272	177.951446	47.231220
2471.086106	170.517975	47.236225
2467.358710	170.748047	47.241229
2464.035749	165.467039	47.246234
2460.184942	168.712130	47.251239
2457.275510	171.695570	47.256244
2453.824338	165.687897	47.261249
2450.139020	170.169532	47.266253
2447.062765	171.709067	47.271258
2443.056928	173.729918	47.276263
2439.426012	169.206191	47.281268
2436.098863	169.692459	47.286273
2432.326663	169.289033	47.291277
2429.470601	160.069661	47.296282
2425.731062	178.019017	47.301287
2422.144135	173.296407	47.306292
2418.723986	170.309580	47.311297
2414.975359	175.715395	47.316301
2411.536812	167.493529	47.321306
2408.162155	171.591439	47.326311
2404.664302	176.937186	47.331316
2401.321706	155.483843	47.336321
2397.657182	171.265683	47.341325
2394.262019	167.524073	47.346330
2390.883734	164.780757	47.351335
2387.360813	163.734214	47.356340
2384.075555	162.707912	47.361345
2380.276804	169.332120	47.366349
2377.101696	167.637161	47.371354
2373.206658	169.046139	47.376359
2369.411979	159.975351	47.381364
2366.118899	155.358055	47.386369
2362.713852	159.990285	47.391373
2359.328253	157.720433	47.396378
2355.958891	164.606650	47.401383
2352.114429	162.111662	47.406388
2349.147995	159.944476	47.411393
2345.403664	167.229852	47.416397
2342.100673	168.901339	47.421402
2337.867056	161.080386	47.426407
2334.253651	160.984247	47.431412
2330.984238	150.912252	47.436417
2327.703064	160.565527	47.441421
2325.001498	155.153704	47.446426
2321.376896	163.352470	47.451431
2317.576372	161.514667	47.456436
2314.250550	157.135299	47.461441
2309.844740	155.468006	47.466445
2307.024783	163.654283	47.471450
2303.457287	159.190432	47.476455
2299.389387	162.410839	47.481460
2296.157702	158.205732	47.486465
2292.959019	156.317803	47.491469
2289.427344	154.247241	47.496474
2285.979927	157.321082	47.501479
2282.245361	160.973912	47.506484
2279.191952	160.975102	47.511489
2275.366003	160.577958	47.516493
2272.079507	156.336956	47.521498
2268.487134	159.767134	47.526503
2264.725743	158.268040	47.531508
2261.339348	154.245666	47.536513
2257.461852	161.340440	47.541517
2254.035744	165.322272	47.546522
2251.111760	157.826771	47.551527
2247.563020	162.972085	47.556532
2244.372719	150.205863	47.561537
2240.674851	164.896736	47.566541
2237.271545	155.845518	47.571546
2233.260270	159.278018	47.576551
2229.638728	166.834417	47.581556
2226.503084	157.340451	47.586561
2222.841326	168.260196	47.591565
2219.222513	154.706957	47.596570
2215.777462	159.654361	47.601575
2212.470519	153.496327	47.606580
2209.430995	152.480372	47.611585
2205.519878	169.706841	47.616589
2202.404037	155.502567	47.621594
2198.181628	157.641809	47.626599
2194.916215	164.484086	47.631604
2191.664664	159.213782	47.636609
2187.502303	158.380883	47.641613
2183.892246	149.138215	47.646618
2181.120850	153.105182	47.651623
2177.595403	157.114973	47.656628
2174.197379	145.340504	47.661633
2170.543387	155.442815	47.666637
2166.989574	155.442721	47.671642
2163.537219	156.828483	47.676647
2160.047955	164.265144	47.681652
2156.724730	149.072680	47.686657
2152.880546	152.704311	47.691661
2149.290278	151.567108	47.696666
2145.853058	150.010277	47.701671
2142.378891	160.623916	47.706676
2138.956525	149.376054	47.711681
2135.253164	157.742917	47.716685
2132.362547	150.531279	47.721690
2128.007070	155.759226	47.726695
2124.477369	147.731914	47.731700
2121.285853	145.010575	47.736705
2117.584297	160.494643	47.741709
2114.795868	148.580361	47.746714
2111.337051	153.396726	47.751719
2107.259206	162.583818	47.756724
2104.410943	157.576127	47.761729
2100.573679	158.192363	47.766733
2097.300222	145.371974	47.771738
2093.270569	154.193321	47.776743
2089.680585	156.107913	47.781748
2086.665295	153.955921	47.786753
2082.919061	154.048361	47.791757
2079.524046	147.759402	47.796762
2075.981591	150.842840	47.801767
2072.379696	152.422963	47.806772
2069.127877	134.728398	47.811777
2065.514019	151.975955	47.816781
2062.082190	136.813627	47.821786
2058.260015	148.813240	47.826791
2054.750864	145.563626	47.831796
2051.566838	144.067146	47.836801
2048.232546	140.278260	47.841805
2044.555442	139.476404	47.846810
2040.458663	149.306050	47.851815
2037.312340	152.240610	47.856820
2034.189289	145.377379	47.861825
2030.193196	156.926510	47.866829
2027.158450	140.657279	47.871834
2023.390127	149.418809	47.876839
2020.012114	156.238228	47.881844
2016.479740	139.105832	47.886849
2012.581448	147.023788	47.891853
2009.628135	142.581184	47.896858
2005.985186	138.804207	47.901863
2002.372917	142.217968	47.906868
1999.135068	133.223435	47.911873
1995.321163	137.566709	47.916877
1992.122182	144.870536	47.921882
1988.698105	137.176718	47.926887
1984.724668	141.393898	47.931892
1981.293367	142.596350	47.936897
1977.820117	140.166507	47.941901
1974.249760	141.152838	47.946906
1970.994143	136.022326	47.951911
1967.595680	139.239465	47.956916
1964.022893	140.441697	47.961921
1960.332760	149.247154	47.966925
1957.173497	139.843974	47.971930
1953.230711	144.893002	47.976935
1949.748805	141.951152	47.981940
1946.676021	141.114560	47.986945
1943.314919	142.283310	47.991949
1939.593763	131.956002	47.996954
1935.897843	138.786520	48.001959
1931.990732	145.900092	48.006964
1929.085839	130.996509	48.011969
1925.589479	137.935257	48.016973
1922.035596	132.102963	48.021978
1918.285977	137.581969	48.026983
1914.869743	142.243231	48.031988
1911.453306	137.230194	48.036993
1907.653255	137.128458	48.041997
1904.701185	132.818735	48.047002
1900.988047	138.268425	48.052007
1897.079835	137.299577	48.057012
1893.788455	133.463655	48.062017
1890.091236	135.649564	48.067021
1887.196010	129.408988	48.072026
1883.414529	132.131015	48.077031
1880.052149	138.336401	48.082036
1876.398229	127.904284	48.087041
1872.625549	141.292374	48.092045
1869.462181	133.447321	48.097050
1865.786897	144.925656	48.102055
1862.243429	134.034003	48.107060
1858.678689	131.820315	48.112065
1855.444090	144.812192	48.117069
1851.762915	127.943220	48.122074
1848.652372	130.847319	48.127079
1844.726366	144.763654	48.132084
1841.865237	133.942060	48.137089
1838.159748	133.697041	48.142093
1834.548620	140.183648	48.147098
1830.285415	144.382692	48.152103
1827.004846	144.296954	48.157108
1824.123828	136.310816	48.162113
1820.229501	139.900734	48.167117
1816.810620	138.028963	48.172122
1813.529646	143.157276	48.177127
1809.913033	139.800386	48.182132
1806.161622	139.896897	48.187137
1802.399840	151.068559	48.192141
1799.305556	141.097672	48.197146
1796.001759	142.003468	48.202151
1792.501097	142.298192	48.207156
1788.905990	144.178369	48.212161
1785.477244	141.068802	48.217165
1781.989121	145.715248	48.222170
1778.418977	141.030319	48.227175
1774.834871	141.693697	48.232180
1771.456825	138.548310	48.237185
1767.801120	139.058195	48.242189
1764.233918	135.859709	48.247194
1760.896909	136.134438	48.252199
1757.071242	145.266615	48.257204
1753.651474	145.983876	48.262209
1750.407726	134.468212	48.267213
1747.102927	132.124118	48.272218
1743.392027	132.667644	48.277223
1739.851056	135.083334	48.282228
1736.529457	128.722928	48.287233
1732.353703	139.646538	48.292237
1729.450335	121.295457	48.297242
1725.939025	128.198158	48.302247
1722.295464	130.068861	48.307252
1718.706296	125.752018	48.312257
1715.308009	137.269205	48.317261
1711.637787	133.388492	48.322266
1708.213352	132.131249	48.327271
1704.655448	130.242169	48.332276
1701.426330	133.574909	48.337281
1697.717025	137.715615	48.342285
1694.459671	135.859403	48.347290
1691.024401	131.945090	48.352295
1687.237704	140.041174	48.357300
1683.818210	138.766161	48.362305
1680.311227	134.457829	48.367309
1676.695246	133.625456	48.372314
1673.364653	127.036308	48.377319
1669.942606	145.086468	48.382324
1666.557646	130.633886	48.387329
1662.485673	137.018247	48.392333
1659.143441	136.465320	48.397338
1655.527150	131.029410	48.402343
1651.901360	138.326285	48.407348
1648.734338	134.352541	48.412353
1645.280899	129.742522	48.417357
1641.855841	133.596194	48.422362
1638.301899	134.373486	48.427367
1634.486971	126.382691	48.432372
1631.206560	134.871249	48.437377
1627.620480	140.705434	48.442381
1623.737182	127.890312	48.447386
1620.793374	137.211077	48.452391
1617.139096	130.368985	48.457396
1613.789995	134.095238	48.462401
1609.840351	134.999728	48.467405
1606.760404	140.361466	48.472410
1603.364493	128.936488	48.477415
1599.913315	128.019241	48.482420
1596.378889	129.702451	48.487425
1592.579274	137.288675	48.492429
1589.202957	136.345014	48.497434
1585.814206	127.614450	48.502439
1582.110957	127.882561	48.507444
1579.112039	127.008155	48.512449
1575.075992	127.752758	48.517453
1571.782079	121.885588	48.522458
1568.180479	126.959103	48.527463
1564.203344	130.317306	48.532468
1561.046444	121.966280	48.537473
1557.680501	130.828218	48.542477
1554.297870	122.825031	48.547482
1550.514170	121.971052	48.552487
1546.965070	134.569889	48.557492
1544.077917	126.500934	48.562497
1540.431823	127.333453	48.567501
1536.566264	120.038472	48.572506
1533.112239	126.029422	48.577511
1529.390934	124.570748	48.582516
1526.265202	121.339342	48.587521
1522.458647	128.255641	48.592525
1519.028787	121.054983	48.597530
1515.523330	130.743629	48.602535
1511.988956	117.251353	48.607540
1508.879902	121.795100	48.612545
1505.008230	123.189569	48.617549
1501.620727	123.676534	48.622554
1497.898587	114.501497	48.627559
1494.513619	128.888621	48.632564
1491.303983	113.900998	48.637569
1487.642899	125.563348	48.642573
1484.125871	119.366411	48.647578
1480.759024	126.964041	48.652583
1477.237056	130.630071	48.657588
1473.896153	122.120194	48.662593
1470.121791	131.252784	48.667597
1466.607680	118.668283	48.672602
1462.816315	120.337976	48.677607
1458.932795	123.342327	48.682612
1456.062212	110.825570	48.687617
1452.475079	121.879538	48.692621
1449.004180	123.085252	48.697626
1445.479003	122.027478	48.702631
1441.998551	124.806544	48.707636
1438.843793	115.842949	48.712641
1434.897960	127.281230	48.717645
1431.417107	115.137818	48.722650
1428.040562	120.036982	48.727655
1424.194832	122.657008	48.732660
1421.175910	108.023618	48.737665
1417.497806	126.181507	48.742669
1414.214085	120.296606	48.747674
1410.364959	120.392722	48.752679
1406.766327	115.766551	48.757684
1403.701488	118.811202	48.762689
1400.010917	122.957151	48.767693
1396.645812	124.530560	48.772698
1392.963180	117.272685	48.777703
1389.476427	118.529624	48.782708
1385.996522	118.118161	48.787713
1382.523288	125.227942	48.792717
1379.187728	123.860737	48.797722
1375.397737	121.366354	48.802727
1371.648133	125.087196	48.807732
1368.682581	111.412328	48.812737
1365.039285	115.288999	48.817741
1361.632613	111.877787	48.822746
1357.954369	108.155238	48.827751
1354.250464	121.404050	48.832756
1351.062598	106.129195	48.837761
1347.429457	114.377691	48.842765
1343.764306	115.859026	48.847770
1340.538454	113.497255	48.852775
1337.069625	120.583647	48.857780
1333.414166	118.312672	48.862785
1329.847926	124.438231	48.867789
1326.265613	124.884840	48.872794
1323.093438	116.257336	48.877799
1320.088953	117.962407	48.882804
1315.966106	117.666134	48.887809
1312.483041	119.084736	48.892813
1308.852210	117.554237	48.897818
1305.482385	124.961872	48.902823
1301.819315	131.997043	48.907828
1298.522115	123.503563	48.912833
1294.800703	129.236348	48.917837
1291.553110	121.312242	48.922842
1288.083926	126.128416	48.927847
1284.242125	120.477493	48.932852
1280.891665	127.776165	48.937857
1277.071677	121.370185	48.942861
1273.486846	123.393360	48.947866
1270.275859	112.501039	48.952871
1266.728806	129.962228	48.957876
1263.982888	116.617859	48.962881
1260.360623	125.792489	48.967885
1256.332336	122.510926	48.972890
1252.728243	122.062166	48.977895
1249.356327	124.374262	48.982900
1245.910474	108.671072	48.987905
1242.453654	117.076689	48.992909
1238.901083	124.624999	48.997914
1235.539917	114.904126	49.002919
1231.643804	108.693559	49.007924
1228.374512	115.004766	49.012929
1224.588079	115.385084	49.017933
1221.286294	116.989970	49.022938
1217.937838	111.330883	49.027943
1214.241848	116.857252	49.032948
1211.006627	123.596956	49.037953
1207.455607	114.171440	49.042957
1204.100808	122.216018	49.047962
1200.232001	115.440525	49.052967
1196.583062	115.129102	49.057972
1193.694192	119.106320	49.062977
1189.668248	118.117054	49.067981
1186.359857	117.871885	49.072986
1182.827123	110.724334	49.077991
1179.561288	122.965846	49.082996
1175.931314	112.876017	49.088001
1171.913055	120.289309	49.093005
1168.523813	110.723134	49.098010
1164.881533	111.435386	49.103015
1161.432700	112.390825	49.108020
1158.717329	111.299403	49.113025
1155.118858	120.291386	49.118029
1151.401457	108.064966	49.123034
1148.157606	108.912607	49.128039
1144.093557	109.912905	49.133044
1140.595021	103.138012	49.138049
1137.263930	113.797899	49.143053
1133.799356	108.919071	49.148058
1130.242994	111.075585	49.153063
1126.570416	119.397510	49.158068
1123.334262	109.921025	49.163073
1119.790451	112.326079	49.168077
1116.068716	106.517677	49.173082
1112.905467	106.956914	49.178087
1109.128157	112.689464	49.183092
1105.685633	99.163247	49.188097
1102.255809	102.937439	49.193101
1098.891654	107.164075	49.198106
1095.681484	107.731484	49.203111
1091.875678	112.414232	49.208116
1088.512144	107.975113	49.213121
1084.743907	103.965845	49.218125
1081.103221	107.462468	49.223130
1077.607818	105.389550	49.228135
1074.101396	116.746154	49.233140
1070.721612	106.309061	49.238145
1067.176944	104.239394	49.243149
1063.615428	110.311899	49.248154
1060.012609	101.074314	49.253159
1056.648457	110.857078	49.258164
1053.167172	107.229819	49.263169
1049.652757	112.180382	49.268173
1046.275215	108.208344	49.273178
1042.784170	112.140351	49.278183
1039.013946	107.657465	49.283188
1035.576672	110.412940	49.288193
1031.934971	110.095143	49.293197
1028.479867	115.043381	49.298202
1025.171247	104.184271	49.303207
1021.460402	110.115043	49.308212
1018.313425	100.842114	49.313217
1014.562372	114.485000	49.318221
1010.855951	109.399952	49.323226
1007.680826	109.212544	49.328231
1004.280947	109.347382	49.333236
1001.023947	106.005198	49.338241
997.578730	101.872165	49.343245
993.895039	101.879275	49.348250
990.165499	107.782393	49.353255
986.189680	107.386295	49.358260
982.945230	110.245580	49.363265
979.827064	102.650359	49.368269
976.327399	108.016091	49.373274
972.826703	102.378749	49.378279
968.998713	109.589567	49.383284
965.450410	108.293154	49.388289
961.907364	112.936561	49.393293
958.445576	111.663092	49.398298
955.100703	105.295825	49.403303
951.576574	109.663585	49.408308
948.208190	99.503753	49.413313
944.308526	113.481171	49.418317
941.298498	110.530997	49.423322
937.681990	108.059371	49.428327
933.823833	107.616765	49.433332
930.749763	110.719542	49.438337
927.145988	102.277303	49.443341
923.392067	105.587045	49.448346
919.935147	101.946989	49.453351
916.006604	111.084325	49.458356
913.102835	99.737028	49.463361
909.826144	99.305684	49.468365
906.077382	108.031944	49.473370
902.818438	103.680618	49.478375
899.112360	117.071444	49.483380
895.653041	104.648948	49.488385
892.064472	109.544465	49.493389
888.501725	108.137647	49.498394
884.979662	103.399825	49.503399
881.390776	107.187581	49.508404
878.048650	100.507555	49.513409
874.620658	103.622942	49.518413
870.992654	110.410136	49.523418
867.757652	99.155745	49.528423
864.005973	110.148293	49.533428
860.585450	104.770465	49.538433
857.016233	102.763284	49.543437
853.321724	105.231475	49.548442
850.282531	101.728755	49.553447
846.289558	104.592811	49.558452
843.136684	109.058289	49.563457
839.159550	101.637346	49.568461
836.101013	103.617363	49.573466
832.673255	102.182272	49.578471
828.466121	104.134110	49.583476
825.423284	96.395893	49.588481
821.761350	106.622532	49.593485
818.232750	94.932281	49.598490
815.130197	99.894397	49.603495
811.421046	115.801194	49.608500
808.374635	100.950751	49.613505
804.859486	110.800014	49.618509
801.315671	96.402543	49.623514
797.520981	99.095600	49.628519
793.851486	105.646832	49.633524
790.518771	107.299046	49.638529
787.023732	102.289449	49.643533
783.403070	105.852873	49.648538
779.859450	103.203740	49.653543
775.993069	107.396405	49.658548
772.941056	95.892298	49.663553
769.606138	111.745485	49.668557
765.763988	107.129980	49.673562
762.639092	103.788573	49.678567
758.866252	99.974183	49.683572
755.706023	104.215398	49.688577
752.016294	101.431301	49.693581
748.342071	93.858157	49.698586
744.963983	103.265579	49.703591
741.010106	110.645702	49.708596
737.900364	103.444752	49.713601
734.257181	108.407491	49.718605
730.718251	96.495271	49.723610
727.537341	92.964285	49.728615
723.702441	107.615285	49.733620
720.450664	92.959657	49.738625
716.835795	100.911426	49.743629
713.308239	103.221595	49.748634
710.501451	95.528354	49.753639
706.768238	100.991893	49.758644
702.958934	91.012664	49.763649
699.059530	104.762721	49.768653
695.780821	101.990162	49.773658
692.135959	92.586688	49.778663
688.713348	95.205644	49.783668
685.336066	100.031531	49.788673
681.660987	102.955651	49.793677
678.376050	109.000327	49.798682
675.024060	102.876830	49.803687
671.393454	97.359625	49.808692
667.854579	90.526387	49.813697
664.356669	102.600573	49.818701
660.718154	108.447438	49.823706
657.188271	100.971779	49.828711
653.802920	97.986285	49.833716
650.591439	100.976327	49.838721
646.834255	99.573608	49.843725
643.053747	105.454128	49.848730
639.811724	94.024517	49.853735
636.116053	106.884581	49.858740
632.720734	91.133022	49.863745
629.276109	90.472485	49.868749
625.824317	102.375654	49.873754
622.458450	98.020235	49.878759
619.037023	106.867232	49.883764
615.283960	89.539019	49.888769
611.660240	102.875549	49.893773
608.036171	96.847418	49.898778
604.711053	103.471479	49.903783
600.500983	113.005134	49.908788
597.648458	101.210346	49.913793
594.253119	105.690823	49.918797
590.805824	104.482380	49.923802
587.712020	100.938432	49.928807
584.023832	102.875401	49.933812
580.459260	99.774893	49.938817
576.511724	104.864878	49.943821
573.037080	96.340987	49.948826
569.831028	96.112510	49.953831
566.239697	103.915859	49.958836
562.880083	103.059326	49.963841
559.297320	103.861916	49.968845
555.684781	104.766344	49.973850
552.300073	93.757347	49.978855
548.729677	102.399641	49.983860
545.223960	92.846924	49.988865
541.574463	98.351966	49.993869
538.071927	100.682805	49.998874
534.714401	100.380057	50.003879
531.165250	101.869330	50.008884
527.731078	93.262202	50.013889
524.316810	99.720771	50.018893
520.652896	97.344844	50.023898
517.339003	100.727328	50.028903
513.804812	102.013644	50.033908
510.372338	98.561329	50.038913
506.732739	102.833611	50.043917
503.000138	95.195829	50.048922
499.650585	95.374855	50.053927
495.844865	92.856945	50.058932
492.460172	97.541160	50.063937
488.769821	89.866977	50.068941
485.580487	95.333927	50.073946
482.648916	90.243087	50.078951
479.130761	99.192492	50.083956
475.373637	98.115336	50.088961
471.593621	89.302071	50.093965
467.860531	103.402992	50.098970
464.795603	89.227091	50.103975
461.003029	105.074411	50.108980
457.686756	91.902447	50.113985
453.808601	96.756663	50.118989
450.329864	107.013577	50.123994
447.149693	88.969214	50.128999
443.444538	104.252856	50.134004
440.557308	91.768387	50.139009
436.935857	96.863153	50.144013
432.984450	96.203697	50.149018
429.575175	94.446627	50.154023
425.924184	103.076563	50.159028
422.466573	105.691701	50.164033
419.217570	104.303076	50.169037
415.739092	105.003233	50.174042
412.111892	102.498182	50.179047
408.375093	94.928489	50.184052
405.125451	104.510796	50.189057
401.437421	101.943637	50.194061
397.942626	103.933514	50.199066
394.467652	89.270108	50.204071
390.687716	96.168797	50.209076
387.538930	85.022319	50.214081
384.174075	100.311837	50.219085
380.560176	94.182009	50.224090
377.310134	93.822478	50.229095
373.427775	108.457391	50.234100
370.211507	92.939609	50.239105
366.480332	107.338665	50.244109
362.742139	95.729494	50.249114
359.336536	98.532590	50.254119
355.898526	98.433600	50.259124
352.660646	104.017846	50.264129
349.073764	96.009905	50.269133
345.700765	95.861053	50.274138
341.926355	88.996037	50.279143
338.271250	105.107346	50.284148
334.902381	94.551380	50.289153
331.551434	99.133435	50.294157
327.869969	98.309468	50.299162
325.052801	88.286220	50.304167
321.315523	91.379469	50.309172
317.376732	87.022235	50.314177
314.047100	94.349974	50.319181
310.229175	101.752523	50.324186
307.232609	87.226209	50.329191
303.509947	94.014826	50.334196
300.102953	82.510354	50.339201
296.629752	93.451204	50.344205
292.699192	89.316994	50.349210
289.670980	80.070610	50.354215
285.650718	91.303826	50.359220
282.107570	83.731309	50.364225
278.602745	85.628044	50.369229
275.529566	95.688465	50.374234
272.206597	93.525700	50.379239
268.375896	95.193022	50.384244
265.058501	92.148257	50.389249
261.241925	94.384117	50.394253
257.868061	88.289919	50.399258
254.333646	93.289091	50.404263
250.859734	92.987191	50.409268
247.325715	91.218063	50.414273
244.049792	84.745310	50.419277
240.440586	90.090605	50.424282
236.892152	83.338330	50.429287
233.010717	97.601632	50.434292
230.019486	93.361939	50.439297
226.617192	104.456237	50.444301
222.867982	90.268171	50.449306
219.968850	93.691710	50.454311
215.851109	90.627630	50.459316
212.321918	86.486416	50.464321
208.600316	93.553970	50.469325
205.003388	93.900260	50.474330
201.862832	88.299750	50.479335
198.380808	101.605972	50.484340
194.755654	95.226413	50.489345
191.271168	96.195950	50.494349
188.024475	95.947915	50.499354
184.596725	93.240052	50.504359
180.884831	100.256295	50.509364
177.609119	93.502764	50.514369
173.876901	93.863277	50.519373
170.133835	99.928052	50.524378
166.718061	92.399604	50.529383
163.240098	94.583638	50.534388
159.764724	95.826374	50.539393
156.180162	100.409512	50.544397
152.721851	97.093256	50.549402
149.464834	92.220561	50.554407
145.656956	102.161633	50.559412
142.478426	91.919565	50.564417
138.874922	89.681789	50.569421
135.114786	98.843966	50.574426
132.148445	95.922531	50.579431
128.488760	95.179800	50.584436
124.919919	94.828872	50.589441
121.486578	92.005574	50.594445
117.925591	96.259628	50.599450
114.315293	83.087754	50.604455
110.655366	97.345336	50.609460
107.300185	85.072140	50.614465
103.594810	101.388531	50.619469
99.962923	103.518877	50.624474
96.908369	80.067295	50.629479
93.567259	99.875690	50.634484
89.851174	90.107803	50.639489
86.496940	87.562456	50.644493
82.439122	88.658751	50.649498
79.374974	83.420978	50.654503
75.776572	91.781215	50.659508
72.035847	86.434682	50.664513
68.331176	91.372334	50.669517
65.103145	91.018301	50.674522
61.605877	96.914457	50.679527
58.196120	92.552665	50.684532
54.996732	85.472422	50.689537
51.475289	81.091511	50.694541
47.535794	98.842769	50.699546
44.057882	79.477671	50.704551
40.281073	95.736127	50.709556
37.088618	80.266644	50.714561
34.169135	81.722771	50.719565
30.208550	79.717709	50.724570
27.060045	81.543222	50.729575
23.354491	87.091997	50.734580
19.882323	85.310446	50.739585
15.916328	87.229612	50.744589
12.246122	87.127899	50.749594
9.211414	85.170840	50.754599
5.702684	84.360717	50.759604
2.106663	75.238182	50.764609